Tue Jun 21 12:30:25 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.098592	74.054046	0.000000
-0.162277	75.704054	0.005005
-0.015309	69.769077	0.010010
-0.179110	91.153423	0.015014
-0.152834	81.144525	0.020019
-0.141664	71.016381	0.025024
-0.451268	59.267571	0.030029
-0.266559	56.225978	0.035034
-0.735777	36.425944	0.040038
-1.158682	39.448202	0.045043
-0.949132	26.247308	0.050048
-1.559822	13.412538	0.055053
-1.841801	2.314345	0.060058
-2.119501	-6.319856	0.065062
-2.889462	-2.792190	0.070067
-2.839712	-0.114607	0.075072
-3.389410	1.697476	0.080077
-3.527792	-1.685272	0.085082
-4.325920	-5.638781	0.090086
-4.933157	-1.956712	0.095091
-4.830571	-9.355034	0.100096
-5.131024	5.308156	0.105101
-5.083911	0.155986	0.110106
-4.917716	-10.632005	0.115110
-5.199942	3.576667	0.120115
-5.009988	8.236731	0.125120
-5.935090	3.035194	0.130125
-6.532477	3.304924	0.135130
-6.414228	-2.582448	0.140134
-6.866796	-2.846214	0.145139
-7.086256	-3.847338	0.150144
-6.936036	-3.535843	0.155149
-6.928948	-6.520385	0.160154
-7.384195	-1.445841	0.165158
-7.998627	-0.905112	0.170163
-7.805811	-0.266783	0.175168
-8.214686	8.046417	0.180173
-8.885851	4.121018	0.185178
-9.064820	0.249289	0.190182
-9.336919	2.637992	0.195187
-9.211654	-8.450274	0.200192
-9.744790	8.881705	0.205197
-9.659498	6.592441	0.210202
-9.476463	-6.711186	0.215206
-10.363023	3.541176	0.220211
-10.417116	-8.358621	0.225216
-10.822339	-5.889267	0.230221
-11.297196	-6.233603	0.235226
-12.015356	-9.232827	0.240230
-12.105166	-1.204136	0.245235
-11.819380	-1.801511	0.250240
-12.368640	0.032404	0.255245
-12.380247	-7.540396	0.260250
-12.331998	-4.829611	0.265254
-12.417665	0.756001	0.270259
-12.962710	-6.351559	0.275264
-13.596705	-1.381405	0.280269
-13.985741	-1.059152	0.285274
-14.038878	-2.583124	0.290278
-14.143381	-5.522547	0.295283
-14.053944	-5.467782	0.300288
-14.887874	2.085028	0.305293
-15.672200	-2.249842	0.310298
-15.639582	-5.253412	0.315302
-16.102106	4.811518	0.320307
-15.122043	-3.838955	0.325312
-15.639224	8.837460	0.330317
-15.809520	-5.607641	0.335322
-15.795125	-6.563820	0.340326
-16.970580	-3.319469	0.345331
-17.187977	-10.301710	0.350336
-17.154678	-2.835678	0.355341
-17.359066	-9.080469	0.360346
-17.283529	-10.652979	0.365350
-17.968392	-0.160120	0.370355
-18.450328	-5.085362	0.375360
-18.682475	3.892394	0.380365
-18.832618	6.205649	0.385370
-18.618264	-6.316986	0.390374
-18.797270	-3.407348	0.395379
-18.936535	-17.894872	0.400384
-20.013999	-1.411876	0.405389
-20.097941	-9.297902	0.410394
-20.025164	-7.010512	0.415398
-20.442897	-0.889209	0.420403
-20.190162	-2.552435	0.425408
-21.296978	-8.683110	0.430413
-21.508707	-14.020331	0.435418
-21.621458	-10.526508	0.440422
-21.841708	-13.815973	0.445427
-21.934194	-10.033650	0.450432
-21.990022	1.470569	0.455437
-22.040109	-10.100342	0.460442
-22.308285	-13.623800	0.465446
-23.326734	-10.481027	0.470451
-23.595004	-10.983299	0.475456
-23.438371	-4.114694	0.480461
-23.597393	-5.276390	0.485466
-23.629973	-6.310827	0.490470
-24.805876	-1.664150	0.495475
-25.017384	-4.773714	0.500480
-25.094447	-1.032226	0.505485
-24.955513	-2.814740	0.510490
-25.000924	-4.216658	0.515494
-25.401813	2.922071	0.520499
-25.077006	-13.059159	0.525504
-25.840915	-7.039781	0.530509
-26.267046	-1.590585	0.535514
-26.647978	-3.598600	0.540518
-27.156096	-3.643400	0.545523
-26.974972	-12.160976	0.550528
-26.832830	-3.149301	0.555533
-27.030065	-4.238957	0.560538
-27.617090	-8.371669	0.565542
-28.131396	-4.467397	0.570547
-28.387490	-11.905185	0.575552
-28.472087	-4.093440	0.580557
-28.347100	-3.599181	0.585562
-29.073815	-7.265155	0.590566
-29.748002	-5.845868	0.595571
-29.877195	-13.214093	0.600576
-29.946968	-9.652796	0.605581
-29.870230	-15.290568	0.610586
-30.010971	-7.079005	0.615590
-30.430784	-0.963277	0.620595
-30.102776	-2.957069	0.625600
-30.809379	-10.247044	0.630605
-31.180528	-4.377163	0.635610
-31.223755	-2.375640	0.640614
-31.865828	-4.553136	0.645619
-31.547564	-7.763057	0.650624
-32.483104	-3.316614	0.655629
-33.170802	-8.243101	0.660634
-33.142221	-5.136564	0.665638
-33.406766	-9.342410	0.670643
-33.171351	-6.836472	0.675648
-33.110322	-6.567435	0.680653
-33.318543	-5.694963	0.685658
-33.350177	-5.602783	0.690662
-34.430377	-2.408538	0.695667
-34.351724	-11.271054	0.700672
-34.610023	-0.016087	0.705677
-34.835964	-9.992430	0.710682
-35.403320	-12.257283	0.715686
-35.629114	2.145293	0.720691
-35.610535	-4.514116	0.725696
-35.758747	-2.228019	0.730701
-35.789131	2.359205	0.735706
-36.232998	-3.299709	0.740710
-37.314221	5.306771	0.745715
-37.148011	-8.425238	0.750720
-37.680096	-2.459046	0.755725
-37.526521	-11.424940	0.760730
-37.172137	-6.119206	0.765734
-37.737465	-5.055187	0.770739
-38.333456	-4.813903	0.775744
-38.855378	-4.336244	0.780749
-39.256553	-1.825921	0.785754
-38.693808	-8.398631	0.790758
-39.164431	1.573707	0.795763
-39.172124	-1.701427	0.800768
-39.371812	-2.244457	0.805773
-40.157672	-9.193337	0.810778
-40.710661	-3.486729	0.815782
-41.096589	-12.252182	0.820787
-40.893317	-12.498060	0.825792
-41.183397	-10.901238	0.830797
-41.094668	-6.600536	0.835802
-40.890541	-5.904487	0.840806
-41.565138	-0.279761	0.845811
-42.160179	-7.845728	0.850816
-42.547450	-5.944704	0.855821
-42.517752	-4.851152	0.860826
-43.045138	-1.506717	0.865830
-43.129228	7.144010	0.870835
-42.586788	-3.505404	0.875840
-43.359050	0.275433	0.880845
-44.135638	4.865265	0.885850
-44.112829	-6.607211	0.890854
-44.941309	0.258374	0.895859
-44.517372	-5.279821	0.900864
-44.273967	-1.486027	0.905869
-44.792636	-5.909480	0.910874
-44.942847	-14.640163	0.915878
-45.438498	5.165882	0.920883
-45.720812	-5.630914	0.925888
-46.056627	2.338862	0.930893
-45.953172	-2.897819	0.935898
-46.613117	-2.510375	0.940902
-47.462068	-3.583667	0.945907
-47.188562	-0.998394	0.950912
-47.123438	1.045570	0.955917
-47.517458	-2.144276	0.960922
-47.279658	-10.311696	0.965926
-48.101210	3.651016	0.970931
-48.652035	-0.271609	0.975936
-48.986853	6.515780	0.980941
-49.035186	1.883802	0.985946
-48.825223	-0.208843	0.990950
-48.969484	8.886969	0.995955
-49.043931	-2.820016	1.000960
-49.266977	-3.095541	1.005965
-50.255380	0.451533	1.010970
-50.457901	-8.239312	1.015974
-50.479509	-10.875740	1.020979
-50.267779	-13.410307	1.025984
-50.485452	-9.686582	1.030989
-51.794670	-4.343337	1.035994
-51.947341	-6.461373	1.040998
-52.353714	-5.611931	1.046003
-52.222837	-3.526169	1.051008
-52.417463	-11.077733	1.056013
-52.534546	-5.780752	1.061018
-52.245331	-17.745480	1.066022
-52.737935	-6.677071	1.071027
-53.146735	-13.969390	1.076032
-53.811298	-3.027210	1.081037
-53.710167	-1.874052	1.086042
-53.683795	-5.009984	1.091046
-54.008572	-2.559671	1.096051
-54.858906	-9.467876	1.101056
-54.980055	3.590502	1.106061
-55.649800	-1.564902	1.111066
-55.427983	-0.545789	1.116070
-55.572884	2.818779	1.121075
-55.394983	-6.290265	1.126080
-55.338221	-3.081441	1.131085
-56.349906	0.975452	1.136090
-56.477446	-1.838005	1.141094
-57.026332	3.800835	1.146099
-56.986762	-4.637457	1.151104
-56.989594	-5.052260	1.156109
-57.500083	-0.087557	1.161114
-57.901450	1.820539	1.166118
-58.435776	3.934766	1.171123
-58.764131	-2.555301	1.176128
-58.406990	-7.246135	1.181133
-58.598020	-7.777180	1.186138
-58.509222	-4.873214	1.191142
-59.226953	2.325287	1.196147
-59.971989	-14.585807	1.201152
-60.148433	-3.992243	1.206157
-60.445014	-2.717378	1.211162
-60.250426	-3.576314	1.216166
-60.250622	2.874656	1.221171
-60.381241	-11.559834	1.226176
-61.109000	-0.975017	1.231181
-61.620972	11.047167	1.236186
-61.717251	2.081598	1.241190
-61.607939	1.693610	1.246195
-61.658457	-0.899749	1.251200
-61.847477	-3.192918	1.256205
-62.661066	3.603507	1.261210
-62.718633	-0.128285	1.266214
-63.233249	-2.300440	1.271219
-63.165227	-0.504018	1.276224
-63.265482	-0.567419	1.281229
-64.227406	1.954864	1.286234
-64.274525	-10.579322	1.291238
-65.166673	4.101535	1.296243
-64.692733	-3.806232	1.301248
-64.839817	-1.274641	1.306253
-65.229830	3.581312	1.311258
-65.219015	-1.219904	1.316262
-65.342556	1.098023	1.321267
-65.288212	-7.686270	1.326272
-65.864196	0.403198	1.331277
-66.435596	-3.881280	1.336282
-66.328967	-3.723198	1.341286
-66.955995	-1.021550	1.346291
-66.915831	0.497891	1.351296
-67.243963	0.722250	1.356301
-68.151785	-1.073396	1.361306
-68.385474	-5.627709	1.366310
-68.747466	2.781719	1.371315
-68.276366	-6.588013	1.376320
-68.194871	-3.806368	1.381325
-68.537776	-3.873984	1.386330
-68.840202	-3.303221	1.391334
-68.833569	-1.448089	1.396339
-69.466695	-10.575752	1.401344
-70.068112	4.447876	1.406349
-70.280436	0.425388	1.411354
-70.031940	-9.302144	1.416358
-70.383709	1.831551	1.421363
-70.950355	-2.923959	1.426368
-71.308918	4.450481	1.431373
-71.787035	3.553567	1.436378
-71.700746	0.985899	1.441382
-71.746291	-2.749263	1.446387
-71.580331	-5.290461	1.451392
-71.978183	-5.780742	1.456397
-72.856790	-1.973607	1.461402
-72.945087	-8.967749	1.466406
-73.351084	0.331241	1.471411
-73.200611	-10.050003	1.476416
-73.081560	-2.847606	1.481421
-73.508323	-2.649735	1.486426
-74.065421	-3.010438	1.491430
-74.635564	-2.129728	1.496435
-74.708384	-2.548136	1.501440
-74.878534	1.407482	1.506445
-74.649199	4.731781	1.511450
-75.031636	-7.606373	1.516454
-76.359093	2.025187	1.521459
-76.309698	1.053741	1.526464
-76.342576	-0.151932	1.531469
-76.626678	5.256974	1.536474
-76.673914	1.210698	1.541478
-76.661103	5.523185	1.546483
-76.502954	-4.994309	1.551488
-76.844930	-2.610608	1.556493
-77.570996	10.627280	1.561498
-77.661997	-3.764837	1.566502
-78.297054	-4.485194	1.571507
-78.154815	0.796470	1.576512
-78.555190	-5.111570	1.581517
-79.311487	-6.745629	1.586522
-79.525079	-0.842638	1.591526
-79.704671	1.135687	1.596531
-79.858114	-6.162217	1.601536
-79.475823	0.163248	1.606541
-79.774896	-0.165002	1.611546
-79.878264	0.669585	1.616550
-80.626063	6.610531	1.621555
-80.947522	-2.595980	1.626560
-80.873259	5.384818	1.631565
-81.392901	-0.587141	1.636570
-81.338185	-4.830858	1.641574
-82.304562	-4.988410	1.646579
-83.013200	-12.052679	1.651584
-82.205417	-10.987346	1.656589
-82.455056	-2.525093	1.661594
-83.018773	-9.739854	1.666598
-83.021107	1.866007	1.671603
-83.060596	-5.608240	1.676608
-83.198901	-10.286288	1.681613
-83.736697	-0.877855	1.686618
-83.859227	-11.888962	1.691622
-84.577008	-7.645913	1.696627
-84.471386	-7.577056	1.701632
-84.382238	-7.778975	1.706637
-85.483109	-3.112150	1.711642
-85.547452	-2.952393	1.716646
-85.861039	0.202521	1.721651
-86.081988	-7.328303	1.726656
-85.802581	-16.655232	1.731661
-86.750448	-2.976484	1.736666
-86.404758	-16.916593	1.741670
-86.485761	-4.608228	1.746675
-87.332449	-0.501102	1.751680
-87.517093	-3.630502	1.756685
-87.601055	-0.573606	1.761690
-87.668778	-9.663477	1.766694
-87.850394	-8.118162	1.771699
-88.740892	-5.332426	1.776704
-88.933142	-4.281050	1.781709
-89.615883	-0.397224	1.786714
-89.365540	-6.577209	1.791718
-89.235010	-4.329579	1.796723
-89.250845	-5.482228	1.801728
-89.203561	-1.664444	1.806733
-89.829235	-4.398559	1.811738
-90.458049	-8.439683	1.816742
-90.837068	-0.987857	1.821747
-90.667177	-7.597531	1.826752
-91.041760	-0.798428	1.831757
-91.251168	-0.894071	1.836762
-91.348176	-6.811304	1.841766
-92.409819	-5.299819	1.846771
-92.519984	0.414956	1.851776
-92.214796	-12.537703	1.856781
-92.712916	7.702092	1.861786
-92.452564	0.083861	1.866790
-92.940081	1.702926	1.871795
-93.567598	-7.798029	1.876800
-93.743755	-0.142802	1.881805
-94.006419	2.529290	1.886810
-93.920487	-0.792526	1.891814
-94.285059	1.070012	1.896819
-94.225431	-1.361224	1.901824
-94.742035	-0.695197	1.906829
-95.721230	0.162881	1.911834
-95.511445	3.683210	1.916838
-95.456904	-2.858424	1.921843
-95.869480	-3.631016	1.926848
-95.994611	-3.020547	1.931853
-96.966842	-0.567592	1.936858
-96.928539	-7.098444	1.941862
-97.619063	4.794057	1.946867
-97.065014	-3.266295	1.951872
-97.200799	-2.802456	1.956877
-97.635474	-5.214778	1.961882
-97.618764	-9.368925	1.966886
-97.955841	5.458386	1.971891
-98.165002	0.530802	1.976896
-98.434962	-6.491664	1.981901
-98.459600	-6.122600	1.986906
-98.713978	-6.411285	1.991910
-99.608476	0.605741	1.996915
-100.035201	-0.012912	2.006912
-99.433300	-5.895308	2.016909
-99.266081	-0.073444	2.026906
-98.412530	0.969754	2.036902
-97.756681	1.295658	2.046899
-97.380249	-10.874908	2.056896
-96.784849	-10.730651	2.066893
-96.255281	-4.533714	2.076890
-96.180114	-3.774362	2.086886
-94.954866	-8.502160	2.096883
-94.474332	-6.669675	2.106880
-94.452654	-6.091543	2.116877
-94.232592	1.218481	2.126874
-93.261212	-1.944283	2.136870
-93.049155	-8.405059	2.146867
-92.149793	-0.936054	2.156864
-91.806677	-6.740026	2.166861
-91.509303	-1.439609	2.176858
-90.801894	-0.204851	2.186854
-90.215327	0.565834	2.196851
-90.013324	-1.210297	2.206848
-89.375170	1.031565	2.216845
-88.335282	4.440030	2.226842
-88.436398	1.751262	2.236838
-88.172124	3.487182	2.246835
-87.592629	-7.399118	2.256832
-86.683188	-9.718798	2.266829
-86.146107	-9.101147	2.276826
-85.908278	-8.865267	2.286822
-85.723063	-5.664197	2.296819
-84.868204	1.176153	2.306816
-84.182886	-0.534794	2.316813
-84.002690	-4.757575	2.326810
-82.922199	-2.374390	2.336806
-82.647030	-5.621413	2.346803
-82.399068	-4.421016	2.356800
-82.141114	-2.690768	2.366797
-81.338676	-4.984823	2.376794
-81.201484	-5.448524	2.386790
-80.235117	-10.177112	2.396787
-79.853099	-3.250750	2.406784
-79.029931	-7.513030	2.416781
-78.413348	-1.949140	2.426778
-78.414455	-7.461176	2.436774
-78.154956	-2.304650	2.446771
-77.137005	-1.052756	2.456768
-76.564614	2.079256	2.466765
-76.318868	5.689384	2.476762
-76.152625	-1.366248	2.486758
-75.055931	-11.944013	2.496755
-74.799558	-1.403349	2.506752
-74.744591	-0.407303	2.516749
-73.917163	2.663704	2.526746
-73.467431	3.922762	2.536742
-72.314562	-0.271617	2.546739
-71.862992	0.448123	2.556736
-71.964224	-0.481321	2.566733
-71.594549	0.547965	2.576730
-70.600145	-0.841519	2.586726
-70.216961	-8.122363	2.596723
-70.232154	-1.887959	2.606720
-69.125214	1.492216	2.616717
-68.695664	-1.511855	2.626714
-68.300830	4.267182	2.636710
-67.222470	-2.123077	2.646707
-67.025457	-1.414726	2.656704
-66.873427	-4.833410	2.666701
-66.888432	2.076510	2.676698
-65.995518	-1.262146	2.686694
-65.307410	-2.607426	2.696691
-64.159265	-10.754513	2.706688
-63.847788	-4.358050	2.716685
-64.026266	-4.678980	2.726682
-63.812069	-3.773913	2.736678
-62.606562	-6.702972	2.746675
-62.250992	-10.817274	2.756672
-62.184183	-0.890333	2.766669
-61.057383	-5.131566	2.776666
-60.830398	-3.127273	2.786662
-60.270117	3.724130	2.796659
-59.560541	-0.366012	2.806656
-59.399872	-2.151499	2.816653
-59.065921	-4.206144	2.826650
-57.914014	1.522405	2.836646
-57.722918	0.976670	2.846643
-57.246893	3.723941	2.856640
-56.442563	5.459144	2.866637
-56.277768	2.544165	2.876634
-56.123704	-0.102691	2.886630
-55.247885	0.796345	2.896627
-54.692447	4.138437	2.906624
-54.384482	-0.751808	2.916621
-53.294308	-0.598196	2.926618
-53.068585	2.374676	2.936614
-52.910569	1.420279	2.946611
-52.804705	-6.877849	2.956608
-51.739738	0.774766	2.966605
-51.213533	2.047244	2.976602
-50.365987	-2.797602	2.986598
-49.981041	3.633923	2.996595
-49.864548	-4.453365	3.006592
-49.676837	-4.974433	3.016589
-48.623635	-0.577467	3.026586
-48.333577	-5.187334	3.036582
-47.363271	-5.046077	3.046579
-46.901747	-7.151880	3.056576
-46.711731	-12.120196	3.066573
-46.852058	2.339488	3.076570
-45.539617	-0.891207	3.086566
-45.121914	-6.968343	3.096563
-44.783769	-3.499576	3.106560
-43.752927	-2.603092	3.116557
-43.836115	-9.465472	3.126554
-43.394899	-8.297470	3.136550
-42.774105	-9.875222	3.146547
-41.814113	-8.773174	3.156544
-41.611088	-4.332630	3.166541
-41.700335	2.461551	3.176538
-40.696307	-4.928230	3.186534
-40.334347	-2.981853	3.196531
-39.700780	4.893558	3.206528
-38.837481	-2.618737	3.216525
-38.794123	-0.971302	3.226522
-38.661812	-1.985657	3.236518
-37.771402	-7.383133	3.246515
-37.362371	-10.208741	3.256512
-36.356982	-7.146649	3.266509
-36.025912	-3.487817	3.276506
-35.668525	1.564777	3.286502
-35.551198	-5.853030	3.296499
-34.630359	-4.867790	3.306496
-34.100473	-9.733530	3.316493
-33.892415	-4.907143	3.326490
-32.924253	-2.992391	3.336486
-32.715800	-3.882032	3.346483
-32.412838	-8.169599	3.356480
-31.532557	-7.447742	3.366477
-31.408645	-4.365144	3.376474
-30.797081	-4.687289	3.386470
-30.003694	-5.056535	3.396467
-29.610542	-6.828159	3.406464
-29.344537	-2.778000	3.416461
-28.331674	-8.089649	3.426458
-27.954996	-4.089629	3.436454
-27.818913	-7.286944	3.446451
-27.421593	-10.247539	3.456448
-26.452699	-6.506226	3.466445
-26.105541	-1.280236	3.476442
-25.965313	-10.115956	3.486438
-24.872582	-7.162178	3.496435
-24.760276	-18.159997	3.506432
-24.298117	-14.098460	3.516429
-23.314764	-7.602823	3.526426
-22.960879	-12.880823	3.536422
-22.906096	-5.501733	3.546419
-22.554108	-6.304692	3.556416
-21.579075	-10.542122	3.566413
-21.276094	-7.150713	3.576410
-20.181750	-4.675950	3.586406
-19.642309	-9.233259	3.596403
-19.663808	-8.486548	3.606400
-19.541157	-6.999445	3.616397
-18.867108	-4.673021	3.626394
-18.267199	-5.504389	3.636390
-17.380438	-6.811623	3.646387
-17.055519	-8.813792	3.656384
-16.775434	-4.951695	3.666381
-16.181577	0.198867	3.676378
-15.640595	-3.795578	3.686374
-14.751049	0.936338	3.696371
-14.853991	-1.293138	3.706368
-14.231864	-0.574368	3.716365
-13.246272	-5.061320	3.726362
-13.142729	-8.209382	3.736358
-13.006179	-12.096744	3.746355
-12.257830	-6.808955	3.756352
-11.778817	-5.516407	3.766349
-11.152712	-6.967591	3.776346
-10.601183	-6.122333	3.786342
-10.243480	-5.625924	3.796339
-9.314328	-9.668640	3.806336
-8.822177	-6.192572	3.816333
-8.809770	-9.788486	3.826330
-8.519130	-3.981915	3.836326
-7.555121	-6.432131	3.846323
-7.184620	-7.401558	3.856320
-6.710937	-3.450002	3.866317
-6.127569	-2.510432	3.876314
-5.739135	-3.769921	3.886310
-5.020194	2.291155	3.896307
-4.413655	6.525786	3.906304
-4.159413	0.942810	3.916301
-4.068873	10.786209	3.926298
-3.395481	14.839453	3.936294
-2.830553	25.178098	3.946291
-2.306090	30.598607	3.956288
-2.033230	37.126169	3.966285
-1.731351	57.599536	3.976282
-1.278428	74.789708	3.986278
-0.883462	95.647430	3.996275
-0.329484	122.269745	4.006272
0.000000	135.514740	4.011277
0.309658	150.866379	4.016282
0.255687	173.287803	4.021286
0.505833	164.409219	4.026291
0.860473	189.258311	4.031296
0.649540	195.135283	4.036301
1.218565	196.182168	4.041306
0.944646	205.140910	4.046310
0.584255	199.398827	4.051315
1.005623	198.881806	4.056320
0.828739	201.102429	4.061325
1.034593	206.286413	4.066330
0.912695	211.794628	4.071334
1.422436	226.293082	4.076339
1.282615	233.393224	4.081344
1.418593	232.605945	4.086349
1.639469	212.474738	4.091354
0.937757	215.470380	4.096358
1.062398	200.223999	4.101363
1.295410	213.152872	4.106368
1.160599	224.485040	4.111373
1.449797	227.699234	4.116378
1.117550	231.402718	4.121382
1.574012	228.523098	4.126387
1.347109	234.309982	4.131392
1.073429	230.761722	4.136397
1.326807	229.449625	4.141402
1.262360	238.984654	4.146406
1.697207	239.457410	4.151411
1.583099	236.036451	4.156416
1.527591	235.222469	4.161421
1.668753	231.055539	4.166426
1.535245	234.021427	4.171430
1.322333	219.249276	4.176435
1.271441	225.181850	4.181440
1.340424	238.343926	4.186445
1.583843	239.660420	4.191450
1.158134	249.479252	4.196454
1.472472	237.930887	4.201459
1.630299	242.705272	4.206464
1.384676	242.342703	4.211469
1.706267	240.896370	4.216474
1.463876	248.419227	4.221478
1.221094	241.195784	4.226483
2.020063	245.678508	4.231488
1.099638	240.365998	4.236493
1.336834	244.079977	4.241498
1.018237	248.831430	4.246502
1.255100	250.813049	4.251507
1.583086	269.394539	4.256512
1.930637	274.950546	4.261517
2.078591	274.554378	4.266522
1.642358	265.803996	4.271526
1.829658	249.252860	4.276531
1.443957	242.231080	4.281536
1.630718	267.398181	4.286541
2.079097	269.099685	4.291546
1.820220	267.726972	4.296550
1.450633	256.104374	4.301555
1.624505	263.091805	4.306560
1.669660	282.319260	4.311565
1.775183	283.258590	4.316570
1.418623	288.007658	4.321574
1.777735	272.212264	4.326579
1.630572	271.262495	4.331584
1.654296	282.375655	4.336589
1.993797	271.050035	4.341594
1.801262	280.045862	4.346598
1.807737	282.463071	4.351603
1.787967	289.175917	4.356608
1.867854	284.218524	4.361613
1.723736	270.665525	4.366618
1.587988	280.860835	4.371622
1.973255	267.937498	4.376627
1.938832	274.801162	4.381632
2.038893	287.851966	4.386637
2.212239	279.979032	4.391642
1.669618	285.746976	4.396646
1.866973	291.028697	4.401651
2.415533	302.957189	4.406656
2.300436	306.786155	4.411661
2.249699	280.209810	4.416666
2.244093	285.911720	4.421670
2.186025	277.791956	4.426675
1.839474	284.631532	4.431680
1.959594	281.348591	4.436685
1.950805	276.855220	4.441690
2.085633	285.161416	4.446694
2.240365	296.225858	4.451699
2.392040	294.345887	4.456704
1.826414	295.981655	4.461709
2.286867	291.532532	4.466714
2.212147	298.736379	4.471718
2.164429	300.818804	4.476723
2.105829	300.853486	4.481728
2.350140	304.973408	4.486733
2.699971	292.698054	4.491738
2.061274	298.314372	4.496742
1.845416	286.724706	4.501747
2.120905	295.693561	4.506752
1.968570	306.413787	4.511757
2.140253	293.710899	4.516762
2.226679	304.731797	4.521766
2.136493	305.649663	4.526771
2.328175	308.343067	4.531776
2.108210	307.130460	4.536781
2.199965	305.282512	4.541786
2.328509	304.256499	4.546790
2.107545	308.712768	4.551795
1.922066	313.408058	4.556800
2.373069	338.617362	4.561805
2.551515	329.088488	4.566810
2.507199	338.480134	4.571814
2.718223	337.751860	4.576819
2.959978	338.715405	4.581824
2.414608	321.480968	4.586829
2.878438	303.929264	4.591834
2.496338	310.622788	4.596838
2.489187	313.234465	4.601843
2.378512	309.085930	4.606848
2.377778	315.395633	4.611853
2.442763	298.825822	4.616858
2.522534	322.487287	4.621862
2.806894	325.685332	4.626867
2.637825	310.628772	4.631872
2.320488	314.106223	4.636877
2.985322	318.912120	4.641882
2.400372	325.857298	4.646886
2.698183	329.445818	4.651891
3.124020	330.473207	4.656896
2.893589	329.777974	4.661901
3.093522	303.353668	4.666906
2.776525	306.635106	4.671910
2.673028	307.908608	4.676915
2.865914	311.653621	4.681920
2.536327	311.641216	4.686925
2.998672	298.256938	4.691930
2.520419	310.031241	4.696934
2.527705	318.569331	4.701939
2.927222	308.026649	4.706944
2.598538	311.119987	4.711949
2.923491	301.386109	4.716954
2.694688	307.171953	4.721958
2.736032	298.301227	4.726963
2.765064	302.651963	4.731968
2.883881	307.416647	4.736973
2.873222	313.745950	4.741978
2.902739	333.339158	4.746982
2.885397	328.063758	4.751987
3.178616	323.273100	4.756992
2.589359	327.475804	4.761997
2.880613	331.093432	4.767002
2.894829	337.440333	4.772006
3.039061	329.263560	4.777011
3.114475	333.321077	4.782016
2.966201	343.958960	4.787021
3.054508	333.915355	4.792026
3.036402	340.023305	4.797030
3.068240	328.617557	4.802035
3.235469	328.417507	4.807040
3.120243	328.607595	4.812045
2.943135	316.144785	4.817050
3.030086	331.163474	4.822054
3.241284	332.409929	4.827059
2.967819	335.243509	4.832064
2.931957	342.049621	4.837069
3.163719	335.145980	4.842074
2.948667	338.951248	4.847078
3.107781	344.016328	4.852083
3.387609	337.146167	4.857088
2.861047	342.223356	4.862093
3.032732	336.548814	4.867098
2.990136	342.374879	4.872102
3.190368	340.102843	4.877107
3.330061	341.359165	4.882112
2.922867	344.209761	4.887117
3.134611	341.433002	4.892122
2.777391	333.117849	4.897126
2.829175	341.342316	4.902131
2.846887	345.589363	4.907136
3.391939	367.631262	4.912141
3.702805	369.337984	4.917146
3.385726	366.988210	4.922150
3.351644	367.263728	4.927155
3.457678	365.193179	4.932160
3.067317	369.382693	4.937165
3.552442	364.945646	4.942170
3.187676	371.577322	4.947174
3.760798	376.975440	4.952179
3.527661	365.358976	4.957184
3.283380	346.341237	4.962189
3.339330	347.296871	4.967194
3.373922	364.952803	4.972198
3.284448	361.596016	4.977203
3.263830	372.467740	4.982208
3.508018	371.344428	4.987213
3.505425	367.370187	4.992218
3.309614	373.337866	4.997222
3.515923	372.724236	5.002227
3.397501	378.077023	5.007232
3.234000	370.881240	5.012237
3.706803	374.888554	5.017242
3.318399	376.750537	5.022246
3.442751	378.881836	5.027251
3.672830	372.292619	5.032256
3.248035	372.090550	5.037261
3.433186	368.702692	5.042266
3.659599	382.367687	5.047270
3.579077	371.838145	5.052275
3.732836	382.461562	5.057280
3.575967	381.513985	5.062285
3.935540	380.365645	5.067290
3.525922	381.774106	5.072294
3.649627	389.359548	5.077299
3.767486	387.587979	5.082304
3.693882	403.645868	5.087309
3.793415	394.168700	5.092314
3.730394	408.252641	5.097318
3.917034	409.639925	5.102323
3.850242	406.747064	5.107328
3.805457	405.343624	5.112333
3.814375	405.976902	5.117338
3.719243	403.843160	5.122342
3.836711	406.178663	5.127347
3.980730	404.076955	5.132352
3.669529	410.077569	5.137357
3.893569	407.206802	5.142362
3.643162	410.572352	5.147366
3.771956	409.168387	5.152371
4.001135	410.973892	5.157376
3.627170	411.409098	5.162381
4.079135	406.407024	5.167386
3.922971	413.659537	5.172390
3.921175	405.280162	5.177395
3.818639	407.972771	5.182400
3.893425	414.261721	5.187405
3.966757	408.373540	5.192410
4.087657	414.456528	5.197414
4.150201	404.462532	5.202419
4.101163	410.780667	5.207424
3.858160	415.071694	5.212429
3.827002	407.400890	5.217434
4.147157	409.734011	5.222438
4.104098	410.828196	5.227443
4.243152	398.354209	5.232448
4.156166	414.234944	5.237453
4.525340	410.365884	5.242458
4.134867	416.957237	5.247462
4.227625	412.634088	5.252467
3.796772	414.259392	5.257472
3.834503	422.046163	5.262477
4.128810	413.053364	5.267482
3.819744	415.179080	5.272486
4.129659	414.173546	5.277491
4.417287	411.466696	5.282496
3.980225	414.829608	5.287501
4.205836	422.360302	5.292506
4.439071	436.236157	5.297510
4.282005	442.937665	5.302515
4.176698	425.221159	5.307520
3.853244	436.365080	5.312525
4.396705	440.370776	5.317530
4.203544	442.641884	5.322534
4.243679	443.590473	5.327539
4.467115	436.523979	5.332544
4.315487	449.364200	5.337549
4.582771	440.412762	5.342554
4.451729	443.473991	5.347558
4.641675	444.006646	5.352563
4.942270	440.188600	5.357568
4.343197	437.205084	5.362573
4.408594	434.072862	5.367578
4.389841	429.975380	5.372582
4.678800	442.189102	5.377587
4.830829	432.106465	5.382592
4.521937	419.267164	5.387597
4.344510	411.758912	5.392602
4.706636	411.856736	5.397606
4.546567	413.200394	5.402611
4.696083	405.967760	5.407616
4.385078	418.379086	5.412621
4.542813	421.381441	5.417626
4.546436	415.018163	5.422630
4.184768	412.478821	5.427635
4.665306	424.583252	5.432640
4.829034	436.080844	5.437645
4.832655	441.863575	5.442650
4.731022	429.126503	5.447654
4.517570	419.639577	5.452659
4.713823	413.492655	5.457664
4.228940	426.037171	5.462669
4.766950	435.109061	5.467674
4.744142	445.783861	5.472678
4.612580	442.601369	5.477683
4.698975	441.848339	5.482688
4.700771	451.354373	5.487693
4.648140	441.707008	5.492698
4.937999	440.732420	5.497702
4.647244	441.955242	5.502707
4.861644	439.312216	5.507712
4.602896	451.159406	5.512717
4.622149	442.205821	5.517722
4.778193	450.326055	5.522726
4.740920	446.488768	5.527731
4.824746	445.152238	5.532736
4.540035	447.125131	5.537741
4.747835	438.502839	5.542746
4.923989	449.069114	5.547750
4.581665	448.217759	5.552755
4.734990	445.756925	5.557760
4.467913	452.647944	5.562765
5.207908	468.216164	5.567770
5.046062	471.293155	5.572774
4.827820	469.701358	5.577779
4.928422	468.193520	5.582784
5.160953	477.704777	5.587789
5.272938	475.886415	5.592794
4.896834	466.457178	5.597798
4.832276	478.075880	5.602803
5.300117	470.753011	5.607808
5.270632	480.359952	5.612813
5.227095	460.767726	5.617818
4.857757	451.951893	5.622822
4.771521	463.820058	5.627827
5.237944	473.345470	5.632832
4.940808	478.483776	5.637837
5.001055	475.804898	5.642842
5.412481	479.502319	5.647846
5.193266	479.384018	5.652851
5.290749	483.880750	5.657856
5.098587	482.398892	5.662861
5.131431	484.489314	5.667866
5.051694	492.582701	5.672870
4.936791	490.683306	5.677875
5.209913	482.153776	5.682880
4.971605	490.513780	5.687885
5.166407	486.566222	5.692890
4.934179	490.187294	5.697894
4.677062	490.936065	5.702899
5.112893	482.899779	5.707904
4.929314	483.753395	5.712909
5.274851	499.083061	5.717914
5.053371	507.509948	5.722918
5.410541	517.036507	5.727923
5.574889	505.546130	5.732928
5.631041	513.226294	5.737933
5.933810	505.797340	5.742938
5.346273	498.112058	5.747942
5.414103	493.850046	5.752947
5.452831	484.788622	5.757952
5.354526	495.130612	5.762957
5.496548	490.943342	5.767962
5.351672	486.842456	5.772966
5.182482	494.654056	5.777971
5.724904	495.447643	5.782976
5.127179	511.828056	5.787981
5.785982	508.530857	5.792986
5.969313	513.017723	5.797990
5.312365	503.447496	5.802995
5.586837	492.553804	5.808000
5.733548	510.023597	5.813005
5.731572	493.289626	5.818010
5.420311	491.386632	5.823014
5.415946	489.776980	5.828019
5.706790	498.816426	5.833024
5.718208	511.321257	5.838029
5.704990	505.869284	5.843034
5.602362	486.329633	5.848038
5.644899	499.938153	5.853043
5.945376	484.156595	5.858048
5.803325	487.919421	5.863053
5.481543	481.824113	5.868058
5.567531	488.079072	5.873062
5.509200	500.488486	5.878067
5.903245	504.636949	5.883072
5.615725	515.655784	5.888077
5.771020	503.501477	5.893082
5.623716	509.150563	5.898086
5.764164	520.450786	5.903091
5.803639	515.051259	5.908096
5.503744	527.245534	5.913101
5.419498	511.810245	5.918106
5.711278	513.040806	5.923110
5.482705	518.153563	5.928115
5.636456	512.174077	5.933120
5.552876	511.708495	5.938125
5.454605	512.410835	5.943130
5.866955	526.853079	5.948134
5.705731	558.386845	5.953139
5.912009	545.681969	5.958144
5.571936	550.683745	5.963149
6.181947	545.579086	5.968154
6.348223	546.507583	5.973158
5.954649	549.802936	5.978163
6.163471	544.428047	5.983168
6.161346	554.124437	5.988173
5.905475	542.116332	5.993178
6.216074	548.709068	5.998182
6.024684	537.428145	6.003187
5.979027	544.693599	6.008192
6.007394	545.579810	6.013197
6.286383	539.667589	6.018202
6.318679	541.949529	6.023206
5.839736	533.664094	6.028211
6.099366	531.199457	6.033216
6.034203	543.413486	6.038221
6.069759	538.519397	6.043226
6.265955	540.771039	6.048230
5.980899	529.201333	6.053235
6.339106	510.316488	6.058240
5.916489	510.959658	6.063245
5.847420	505.444904	6.068250
5.998394	515.497179	6.073254
6.304934	525.043375	6.078259
6.276393	501.903203	6.083264
5.795771	521.406871	6.088269
5.918091	512.239234	6.093274
6.234108	519.569507	6.098278
5.992953	529.683566	6.103283
6.351195	509.788730	6.108288
5.958862	506.729525	6.113293
6.136861	511.945655	6.118298
5.873117	506.113846	6.123302
6.056356	514.255264	6.128307
6.032050	505.789576	6.133312
6.211941	511.334358	6.138317
6.152458	506.954299	6.143322
6.238493	511.220271	6.148326
5.648322	512.956821	6.153331
6.064777	508.397111	6.158336
5.972594	522.565316	6.163341
6.035484	528.025283	6.168346
5.888629	524.685066	6.173350
5.924174	536.105683	6.178355
6.166524	546.080882	6.183360
6.211297	540.323678	6.188365
6.271100	535.441165	6.193370
6.352707	525.645615	6.198374
6.341149	517.038093	6.203379
6.225531	506.314957	6.208384
6.091939	517.391384	6.213389
6.123905	513.143594	6.218394
6.189510	512.893274	6.223398
6.112053	512.736304	6.228403
6.541038	516.037133	6.233408
5.603941	507.508478	6.238413
5.974820	515.439642	6.243418
6.289968	508.428182	6.248422
5.793299	511.660478	6.253427
5.939236	511.769434	6.258432
5.891692	522.852534	6.263437
5.780554	511.094986	6.268442
5.806598	512.303639	6.273446
5.938248	513.606499	6.278451
6.151831	519.552225	6.283456
6.037802	521.121524	6.288461
6.013651	515.615905	6.293466
6.118053	528.803739	6.298470
6.145803	529.665779	6.303475
6.202707	516.712542	6.308480
5.945214	514.192046	6.313485
6.037230	507.479602	6.318490
6.083168	519.770136	6.323494
6.010452	521.697673	6.328499
6.064715	510.509888	6.333504
5.941816	517.529211	6.338509
6.016805	526.068440	6.343514
6.395375	542.161318	6.348518
5.765412	525.256208	6.353523
6.251098	525.093410	6.358528
6.260041	526.648859	6.363533
6.090150	518.584388	6.368538
6.056831	516.104719	6.373542
6.035515	517.489743	6.378547
6.327986	507.448924	6.383552
5.751500	515.294429	6.388557
5.650758	511.112621	6.393562
6.086313	520.434783	6.398566
5.840990	536.545320	6.403571
6.071085	540.162468	6.408576
6.152428	548.021807	6.413581
5.887922	552.613430	6.418586
6.670128	544.818333	6.423590
6.213268	536.945232	6.428595
6.257437	514.527304	6.433600
6.043843	513.241990	6.438605
5.761420	515.899875	6.443610
5.742284	519.412257	6.448614
5.937592	534.833733	6.453619
5.998491	535.959850	6.458624
6.235391	543.008212	6.463629
6.187217	544.501486	6.468634
6.191712	543.527968	6.473638
5.985809	529.630748	6.478643
5.767812	525.429476	6.483648
5.695117	537.551405	6.488653
5.559929	546.254904	6.493658
6.139028	543.246777	6.498662
5.791818	549.794120	6.503667
6.151891	541.184248	6.508672
6.254349	547.730146	6.513677
5.946640	545.558766	6.518682
5.977395	547.617967	6.523686
6.039734	557.110094	6.528691
6.301759	548.779114	6.533696
6.123145	554.570553	6.538701
5.983725	548.593618	6.543706
6.390427	551.143515	6.548710
6.260463	555.445266	6.553715
6.230215	546.076326	6.558720
6.097386	551.203235	6.563725
6.018338	545.149012	6.568730
6.293433	545.138306	6.573734
6.379292	558.938426	6.578739
6.275936	539.222801	6.583744
6.205993	527.361328	6.588749
6.167726	522.793042	6.593754
5.951239	525.570452	6.598758
5.671211	521.723021	6.603763
6.072419	517.256610	6.608768
5.670499	530.002573	6.613773
5.950454	546.273209	6.618778
6.198588	550.042285	6.623782
5.863606	556.916967	6.628787
5.971264	553.985522	6.633792
6.246139	549.833269	6.638797
5.993346	552.016189	6.643802
6.104302	549.520716	6.648806
6.134043	559.508830	6.653811
6.454886	552.816889	6.658816
6.058261	556.900531	6.663821
6.267129	548.260438	6.668826
6.348886	520.021448	6.673830
6.311835	530.226824	6.678835
6.250621	524.952898	6.683840
5.877126	517.319388	6.688845
6.198646	517.271393	6.693850
6.389530	514.789331	6.698854
6.205162	516.197407	6.703859
6.469332	515.162736	6.708864
6.010387	515.883162	6.713869
6.290139	515.524957	6.718874
6.484918	520.243975	6.723878
6.069896	523.759948	6.728883
6.044642	515.452086	6.733888
6.231857	522.042548	6.738893
5.872539	516.896726	6.743898
5.885907	512.385409	6.748902
6.026960	519.573363	6.753907
6.319086	519.322239	6.758912
6.354419	515.724717	6.763917
6.302102	517.104613	6.768922
6.208237	491.957274	6.773926
5.978325	495.581713	6.778931
6.393734	484.619695	6.783936
6.198767	495.694429	6.788941
6.108620	492.716223	6.793946
6.406524	490.102776	6.798950
5.918955	497.761272	6.803955
5.918576	479.247245	6.808960
6.052743	486.322261	6.813965
6.167644	484.242335	6.818970
6.236644	486.515820	6.823974
6.268004	492.774104	6.828979
5.953454	496.172593	6.833984
5.967838	488.844090	6.838989
6.054020	487.134984	6.843994
6.263852	488.858450	6.848998
5.660167	496.372184	6.854003
6.034994	494.167714	6.859008
6.074274	490.022717	6.864013
6.225203	489.597239	6.869018
6.210771	481.829103	6.874022
5.990740	490.296985	6.879027
5.984054	487.089859	6.884032
6.019666	486.585201	6.889037
5.605740	501.544517	6.894042
5.993392	485.978620	6.899046
5.647260	506.232781	6.904051
6.018024	496.762340	6.909056
5.984885	503.278575	6.914061
6.090682	513.073302	6.919066
6.349926	520.141041	6.924070
6.147138	514.626325	6.929075
6.384251	496.105907	6.934080
6.036484	499.981539	6.939085
5.867307	481.889547	6.944090
6.257276	483.905637	6.949094
6.238253	492.042450	6.954099
6.072802	490.353106	6.959104
5.732383	494.282183	6.964109
5.798991	501.458380	6.969114
6.023924	493.722434	6.974118
5.978724	498.380342	6.979123
6.245620	513.985704	6.984128
5.796057	502.729599	6.989133
5.712234	509.342439	6.994138
6.400455	519.317793	6.999142
5.839120	527.214867	7.004147
5.917449	523.344012	7.009152
6.071074	518.513853	7.014157
5.995874	525.803136	7.019162
6.166995	523.545761	7.024166
6.170391	521.680054	7.029171
6.070442	511.822419	7.034176
6.343042	521.662744	7.039181
6.043454	522.205422	7.044186
6.260984	511.945924	7.049190
6.219984	514.711837	7.054195
6.108076	487.182443	7.059200
6.182246	489.613143	7.064205
5.908016	491.042017	7.069210
6.186632	490.488043	7.074214
5.931118	489.123436	7.079219
5.945631	480.961748	7.084224
5.901315	502.173937	7.089229
5.940295	500.720504	7.094234
6.577583	495.513266	7.099238
6.047517	498.535003	7.104243
6.323313	487.874350	7.109248
5.972076	484.864390	7.114253
5.840350	495.031940	7.119258
5.906543	485.261071	7.124262
5.844041	496.001285	7.129267
6.239991	505.573513	7.134272
6.106488	500.857211	7.139277
6.131958	500.697998	7.144282
6.352727	486.809100	7.149286
5.897989	495.536080	7.154291
5.847280	494.798845	7.159296
6.105677	503.150214	7.164301
5.876755	494.729859	7.169306
6.154810	504.612488	7.174310
6.148271	511.409674	7.179315
6.321063	506.300859	7.184320
6.231815	497.805671	7.189325
5.791196	493.768555	7.194330
5.884699	485.759550	7.199334
5.834947	499.871176	7.204339
6.133485	508.119007	7.209344
6.135757	516.904515	7.214349
6.277676	515.430680	7.219354
6.555874	497.615855	7.224358
5.564756	507.024469	7.229363
5.618191	499.648251	7.234368
6.071963	505.335350	7.239373
5.955743	518.852363	7.244378
6.071509	522.172301	7.249382
6.100176	526.757008	7.254387
6.077189	525.878818	7.259392
6.277922	529.246258	7.264397
5.974520	522.144810	7.269402
6.164362	530.508138	7.274406
6.099583	527.761743	7.279411
6.090830	519.377933	7.284416
6.068962	525.113409	7.289421
5.829279	517.978521	7.294426
6.270735	514.846174	7.299430
6.242508	522.226938	7.304435
6.047124	511.885639	7.309440
6.455034	496.944706	7.314445
5.879521	494.689014	7.319450
6.337234	489.612355	7.324454
5.862612	491.397654	7.329459
6.014157	495.471024	7.334464
5.922104	493.462465	7.339469
6.217107	498.120282	7.344474
6.007153	486.206246	7.349478
5.921712	493.672842	7.354483
5.801130	485.678172	7.359488
5.877670	498.578531	7.364493
6.275031	515.919207	7.369498
6.320722	511.646450	7.374502
6.261577	501.321277	7.379507
6.192450	492.698436	7.384512
6.182324	484.158579	7.389517
5.704877	499.811403	7.394522
6.003829	491.134323	7.399526
5.676714	492.161488	7.404531
6.053114	505.148956	7.409536
6.602481	507.566291	7.414541
6.228251	503.282358	7.419546
6.180135	498.297152	7.424550
5.951487	491.059213	7.429555
6.082576	480.428646	7.434560
5.974969	498.791663	7.439565
5.979898	496.202456	7.444570
6.221805	485.757781	7.449574
5.834302	485.607356	7.454579
5.723962	495.968311	7.459584
6.104291	498.848571	7.464589
5.949684	509.810858	7.469594
6.212819	515.776203	7.474598
6.052741	516.173232	7.479603
6.029427	512.276190	7.484608
5.976481	514.927059	7.489613
6.155239	521.229817	7.494618
6.298172	515.024391	7.499622
5.902514	501.664597	7.504627
5.878231	503.709225	7.509632
6.029487	512.375930	7.514637
5.910425	523.488634	7.519642
5.940748	517.575169	7.524646
6.305729	513.991342	7.529651
6.390682	515.742002	7.534656
6.272453	503.861310	7.539661
5.927453	494.279098	7.544666
6.098803	486.878625	7.549670
5.668777	503.862747	7.554675
6.004363	514.137836	7.559680
6.175098	512.463666	7.564685
5.946928	511.214315	7.569690
6.285044	516.377687	7.574694
5.941489	528.252200	7.579699
5.983039	522.586116	7.584704
6.013372	519.852192	7.589709
5.919066	528.609099	7.594714
6.343093	517.369356	7.599718
6.134834	524.937410	7.604723
5.977702	522.468771	7.609728
6.524159	521.624954	7.614733
6.035368	508.447130	7.619738
6.013243	500.191053	7.624742
6.086661	496.729906	7.629747
6.029102	494.867192	7.634752
6.204941	490.573877	7.639757
5.693175	494.630984	7.644762
6.167982	504.240475	7.649766
6.231034	508.816128	7.654771
5.905731	503.581007	7.659776
5.842658	503.361862	7.664781
6.099541	526.789472	7.669786
6.421022	511.461251	7.674790
5.837691	510.503768	7.679795
6.260845	514.009809	7.684800
6.287104	504.027677	7.689805
5.932096	502.577322	7.694810
6.047561	490.693464	7.699814
5.937030	495.591696	7.704819
5.665218	500.067490	7.709824
6.063627	508.469680	7.714829
5.934428	520.880189	7.719834
6.303649	518.862538	7.724838
6.134872	522.852793	7.729843
6.027869	520.167856	7.734848
5.929314	519.701399	7.739853
5.993735	522.203379	7.744858
6.433894	510.489721	7.749862
6.274685	517.239372	7.754867
6.129918	499.231924	7.759872
6.035334	488.275614	7.764877
6.141426	491.872041	7.769882
6.300180	493.011355	7.774886
5.736787	496.360274	7.779891
5.902072	491.438205	7.784896
6.165687	488.048577	7.789901
5.694501	488.463770	7.794906
6.138322	506.992029	7.799910
6.373416	514.220453	7.804915
5.963923	510.637981	7.809920
6.187929	503.986762	7.814925
6.047931	508.153208	7.819930
5.974010	497.846665	7.824934
6.029051	501.777356	7.829939
5.677410	498.740621	7.834944
6.056418	506.179650	7.839949
5.758149	515.270084	7.844954
6.083031	511.725458	7.849958
6.017903	533.473361	7.854963
6.149450	524.705973	7.859968
6.178380	524.738791	7.864973
6.284312	524.742874	7.869978
6.242327	513.023012	7.874982
6.076290	531.396928	7.879987
6.010668	523.535419	7.884992
6.126480	521.671819	7.889997
5.847572	521.878752	7.895002
6.018893	522.193079	7.900006
6.081622	530.134230	7.905011
5.937096	530.934809	7.910016
6.060321	526.468841	7.915021
6.119718	533.705449	7.920026
6.594084	520.974750	7.925030
6.121949	502.373837	7.930035
5.889244	500.644518	7.935040
6.200860	500.581980	7.940045
6.221400	500.863060	7.945050
5.922897	494.009857	7.950054
6.144929	494.184556	7.955059
5.803694	490.401734	7.960064
5.736632	489.195960	7.965069
5.751566	507.878121	7.970074
5.906116	520.180666	7.975078
5.899652	532.616446	7.980083
5.928827	532.277435	7.985088
6.109626	531.653222	7.990093
5.843090	535.484429	7.995098
6.214416	522.607000	8.000102
6.066967	528.474374	8.005107
6.174803	529.109038	8.010112
6.001761	522.163677	8.015130
6.113672	531.510355	8.020147
6.248558	517.203109	8.025165
6.121449	524.051548	8.030182
6.231290	521.552545	8.035200
6.328092	520.005045	8.040218
6.110685	527.243215	8.045235
6.411657	526.172696	8.050253
6.183122	530.189707	8.055270
6.173914	521.280354	8.060288
5.992188	509.839321	8.065306
5.904007	528.148422	8.070323
6.411822	532.109836	8.075341
6.462116	530.585192	8.080358
6.177874	507.444632	8.085376
6.451036	506.435015	8.090394
6.132542	495.665019	8.095411
5.714776	496.654127	8.100429
6.129540	501.032487	8.105446
6.137152	497.238502	8.110464
6.183336	496.841233	8.115482
5.831797	508.728242	8.120499
6.250655	507.222289	8.125517
6.216277	521.150146	8.130534
6.322495	527.967430	8.135552
6.442628	513.381154	8.140570
6.193151	514.066628	8.145587
5.988964	492.669009	8.150605
5.926827	512.637636	8.155622
6.117808	513.423981	8.160640
6.360795	515.739993	8.165658
6.195723	526.558417	8.170675
6.801946	515.930539	8.175693
5.954411	510.499932	8.180710
6.024952	516.547584	8.185728
6.240298	514.205706	8.190746
6.031456	521.855024	8.195763
6.396933	514.530170	8.200781
6.139165	522.676729	8.205798
6.453300	527.480392	8.210816
6.401325	514.839606	8.215834
6.188709	524.380756	8.220851
6.123758	526.619620	8.225869
6.523800	522.385673	8.230886
6.426684	523.952547	8.235904
6.578665	519.762433	8.240922
6.173366	508.235006	8.245939
6.326285	509.955147	8.250957
5.904018	505.649904	8.255974
6.113751	516.594040	8.260992
6.366608	527.861335	8.266010
6.464758	525.865413	8.271027
6.431852	526.087300	8.276045
6.576122	525.292909	8.281062
6.367313	529.703279	8.286080
6.305257	523.411550	8.291098
6.024278	527.203402	8.296115
6.324576	525.877895	8.301133
6.353917	524.224448	8.306150
6.213442	529.011664	8.311168
6.068413	524.123144	8.316186
6.132245	531.410605	8.321203
6.229913	523.132524	8.326221
6.248698	526.953670	8.331238
6.322490	534.769368	8.336256
6.539651	528.402664	8.341274
6.322907	524.118300	8.346291
6.204411	531.940249	8.351309
6.119749	524.837555	8.356326
6.507251	526.217300	8.361344
6.393375	530.546798	8.366362
5.997097	522.563880	8.371379
6.230925	529.831262	8.376397
6.661028	541.250896	8.381414
6.317712	554.385706	8.386432
6.558210	547.722629	8.391450
6.645029	544.725697	8.396467
6.532274	527.274431	8.401485
6.497624	525.040085	8.406502
6.282029	533.676679	8.411520
6.352618	524.669274	8.416538
6.409733	545.959441	8.421555
6.654093	558.308209	8.426573
6.735716	539.276815	8.431590
6.633057	532.666828	8.436608
6.555653	521.899015	8.441626
6.132513	525.927384	8.446643
6.201582	538.030379	8.451661
6.546142	544.867452	8.456678
6.279566	559.346552	8.461696
6.580311	550.013245	8.466714
6.557004	555.774307	8.471731
6.330661	558.382593	8.476749
6.539963	551.811486	8.481766
6.469417	556.470997	8.486784
6.651779	557.886486	8.491802
6.712104	555.506693	8.496819
6.713386	555.884916	8.501837
6.798805	563.297943	8.506854
6.645479	557.592534	8.511872
6.805762	559.630338	8.516890
6.490727	565.932788	8.521907
6.293979	565.456263	8.526925
6.228709	563.396853	8.531942
6.434821	559.109384	8.536960
6.858416	551.703240	8.541978
6.605676	562.431686	8.546995
6.688473	559.152562	8.552013
6.789981	553.981493	8.557030
6.423360	560.668441	8.562048
6.508244	549.446403	8.567066
6.503296	558.628209	8.572083
6.206757	557.624939	8.577101
6.538885	553.334714	8.582119
6.754137	556.874533	8.587136
7.076232	555.356844	8.592154
7.073947	556.677326	8.597171
6.509747	565.332492	8.602189
6.972121	551.127275	8.607207
7.015056	557.882222	8.612224
7.037538	553.554104	8.617242
7.026459	550.348791	8.622259
6.674656	543.508419	8.627277
6.661003	535.915845	8.632295
6.552070	539.130824	8.637312
6.683684	554.643908	8.642330
6.737800	549.560211	8.647347
6.251039	554.677986	8.652365
6.618797	553.140532	8.657383
6.672571	565.148646	8.662400
6.802090	551.005829	8.667418
6.489069	551.706157	8.672435
6.581421	557.219343	8.677453
6.870790	554.604393	8.682471
6.254096	556.413595	8.687488
6.477850	548.346300	8.692506
6.776830	548.062867	8.697523
6.470700	552.665331	8.702541
7.052271	551.660151	8.707559
6.712827	555.738050	8.712576
6.945196	550.873637	8.717594
7.126791	550.902732	8.722611
6.777422	552.487169	8.727629
6.779372	549.305485	8.732647
6.791319	559.980651	8.737664
6.753636	560.429102	8.742682
6.734242	554.841468	8.747699
6.774901	553.570959	8.752717
6.942883	555.737006	8.757735
6.624296	563.276770	8.762752
6.905914	574.638149	8.767770
6.827609	569.696639	8.772787
6.858406	582.730353	8.777805
7.335512	571.706129	8.782823
7.042599	572.857822	8.787840
7.009358	566.256009	8.792858
6.977754	560.362148	8.797875
6.782636	556.459011	8.802893
6.926573	555.213918	8.807911
6.806931	556.485530	8.812928
6.738125	555.001076	8.817946
7.040623	554.488140	8.822963
6.730691	564.214118	8.827981
7.192813	560.591296	8.832999
6.997025	556.429036	8.838016
6.801682	562.109933	8.843034
7.019079	561.125688	8.848051
7.387218	571.445642	8.853069
7.328213	560.210613	8.858087
7.136124	560.961384	8.863104
6.933482	552.521219	8.868122
7.199850	554.794194	8.873139
7.132717	560.338318	8.878157
6.993121	549.130027	8.883175
6.930582	563.013965	8.888192
6.934061	560.701849	8.893210
7.213346	556.154053	8.898227
7.200768	552.987961	8.903245
7.364875	547.320538	8.908263
6.971649	560.211075	8.913280
6.565048	555.435933	8.918298
6.914552	550.319659	8.923315
6.610935	558.127593	8.928333
6.784305	556.274516	8.933351
6.791505	559.800168	8.938368
6.875636	572.987630	8.943386
7.173320	578.812076	8.948403
7.427954	582.290462	8.953421
7.396898	576.841356	8.958439
6.866446	564.641547	8.963456
6.873071	565.531449	8.968474
7.349387	573.872599	8.973491
6.865771	578.047011	8.978509
6.993645	586.476966	8.983527
6.850328	586.644701	8.988544
6.867029	591.711204	8.993562
7.230873	583.038251	8.998579
6.874317	590.730369	9.003597
7.297177	587.309305	9.008615
7.293782	590.311950	9.013632
6.995771	585.799507	9.018650
6.740328	580.860556	9.023667
6.721895	584.654220	9.028685
6.982436	582.686516	9.033703
7.301097	589.242089	9.038720
6.860471	590.437533	9.043738
7.241105	599.036455	9.048755
7.461575	604.553638	9.053773
7.271698	589.202142	9.058791
7.283744	588.572350	9.063808
7.129126	588.330959	9.068826
7.501425	586.291209	9.073843
7.250818	592.829638	9.078861
7.087800	586.191240	9.083879
7.404439	590.709685	9.088896
6.958702	594.867396	9.093914
7.094083	581.404638	9.098931
7.081192	594.014325	9.103949
7.523827	601.112133	9.108967
7.282279	608.906468	9.113984
7.378897	615.606688	9.119002
7.612418	601.030095	9.124019
7.294184	598.788960	9.129037
7.445165	583.683763	9.134055
7.513867	588.375341	9.139072
7.155048	582.919487	9.144090
7.534684	583.151207	9.149107
7.653813	582.839094	9.154125
7.431380	584.621004	9.159143
7.456802	578.704899	9.164160
7.313952	587.090320	9.169178
7.539129	584.836167	9.174195
7.217845	592.317538	9.179213
7.283819	580.103595	9.184231
7.313273	584.973706	9.189248
7.418192	584.515531	9.194266
7.514030	582.197172	9.199283
7.165889	585.107699	9.204301
7.616916	591.284095	9.209319
7.531379	574.349888	9.214336
7.219648	580.425237	9.219354
7.411775	573.741617	9.224371
7.299234	588.796379	9.229389
7.290208	578.974621	9.234407
7.674213	591.074716	9.239424
7.169395	580.197925	9.244442
7.613134	582.435432	9.249459
7.306252	596.464381	9.254477
7.235009	588.791953	9.259495
7.277764	591.676530	9.264512
7.659318	612.590646	9.269530
7.591593	603.093140	9.274547
7.414149	609.704101	9.279565
7.643430	605.695246	9.284583
7.624221	596.002320	9.289600
7.295967	587.268980	9.294618
7.508573	603.743638	9.299635
7.566938	618.996099	9.304653
7.450857	613.914974	9.309671
7.838152	611.469220	9.314688
7.450108	603.755745	9.319706
7.572009	607.848794	9.324723
7.606245	609.934837	9.329741
7.657755	618.681372	9.334759
7.849474	601.459114	9.339776
7.323569	593.843862	9.344794
7.521803	588.106407	9.349811
7.198346	607.167308	9.354829
7.585189	622.936210	9.359847
7.645796	618.216352	9.364864
7.348111	627.871842	9.369882
7.988054	621.941162	9.374899
7.806988	625.434425	9.379917
7.311979	623.281216	9.384935
7.929266	620.439525	9.389952
8.033597	618.005195	9.394970
7.825767	609.134782	9.399987
7.667372	595.171284	9.405005
7.679771	594.644971	9.410023
7.586618	586.699615	9.415040
7.163169	594.380766	9.420058
7.845357	607.955021	9.425075
7.985485	618.537550	9.430093
7.601802	612.503557	9.435111
7.690126	609.139655	9.440128
7.919022	614.322004	9.445146
7.710133	603.869982	9.450163
7.591088	598.179550	9.455181
7.479777	609.778055	9.460199
7.587854	612.503010	9.465216
7.489515	614.329134	9.470234
7.837581	612.350870	9.475251
7.823132	615.844492	9.480269
7.632774	617.160691	9.485287
7.758885	612.324877	9.490304
7.549921	616.011721	9.495322
7.740130	609.046926	9.500339
7.578472	616.602066	9.505357
7.626295	619.459039	9.510375
7.598090	610.646672	9.515392
7.687086	617.101320	9.520410
7.705440	619.026619	9.525427
7.859873	617.817378	9.530445
7.609228	613.894289	9.535463
7.698735	616.705386	9.540480
7.738781	618.595598	9.545498
7.857962	621.391152	9.550515
7.976579	625.998103	9.555533
7.772843	630.051779	9.560551
8.373954	620.164787	9.565568
7.895434	620.121312	9.570586
7.884147	619.781585	9.575603
7.985262	613.931077	9.580621
7.996811	621.066618	9.585639
8.058328	611.781155	9.590656
7.730268	623.152192	9.595674
7.744772	612.423031	9.600691
7.679534	614.457834	9.605709
7.600134	622.011953	9.610727
8.006466	635.347480	9.615744
7.863461	643.009380	9.620762
8.098979	644.214512	9.625779
8.370447	646.731327	9.630797
8.288473	636.511401	9.635815
7.967734	617.344188	9.640832
8.081894	614.360628	9.645850
8.188313	608.762377	9.650867
8.296649	618.427002	9.655885
7.945745	617.552998	9.660903
8.319911	606.312739	9.665920
8.160210	619.508138	9.670938
8.289093	605.374038	9.675955
8.308535	608.200278	9.680973
7.955023	615.739945	9.685991
8.124924	615.320219	9.691008
8.150130	618.657284	9.696026
7.648882	618.943142	9.701043
7.646175	605.922494	9.706061
7.524419	613.584797	9.711079
8.000665	598.126336	9.716096
7.730456	617.471524	9.721114
8.225138	627.632774	9.726131
8.154197	624.919611	9.731149
7.917733	636.484533	9.736167
8.117605	626.036065	9.741184
8.307378	649.375340	9.746202
8.378335	637.900245	9.751219
8.248388	614.301719	9.756237
7.848958	614.595125	9.761255
8.104729	606.150671	9.766272
8.239713	615.922686	9.771290
8.135226	625.150539	9.776307
8.268959	618.329729	9.781325
8.283006	625.823497	9.786343
8.173477	611.134026	9.791360
8.022480	610.505248	9.796378
8.124965	633.815649	9.801395
8.214019	633.808891	9.806413
8.197484	636.638731	9.811431
8.721765	628.730475	9.816448
8.435006	610.036355	9.821466
7.903322	610.535507	9.826483
8.339921	607.339118	9.831501
8.077536	611.320616	9.836519
8.342745	618.539735	9.841536
7.921161	626.581593	9.846554
8.269022	633.520515	9.851571
8.417666	637.257591	9.856589
8.390409	636.890195	9.861607
8.640622	627.624654	9.866624
8.034984	621.599459	9.871642
8.271807	626.245494	9.876659
8.458532	636.354208	9.881677
8.280704	633.026892	9.886695
8.567901	639.445187	9.891712
8.493083	625.394402	9.896730
8.104154	615.193824	9.901747
8.322683	621.102255	9.906765
8.222831	637.013963	9.911783
8.499768	633.794009	9.916800
8.406968	637.427374	9.921818
8.300467	645.560759	9.926835
8.339087	633.674118	9.931853
8.314587	645.385432	9.936871
8.135101	647.439552	9.941888
8.216535	649.734306	9.946906
8.265231	649.355514	9.951923
8.320977	639.252537	9.956941
8.293116	651.592325	9.961959
8.483228	638.719631	9.966976
8.227404	639.136099	9.971994
8.285923	639.810732	9.977011
8.522181	637.663983	9.982029
8.289595	644.627770	9.987047
8.317149	646.958610	9.992064
8.019939	648.880657	9.997082
8.261258	663.608803	10.002099
8.385576	668.183722	10.007117
8.363495	678.142404	10.012135
8.679075	670.243491	10.017152
8.891453	668.259343	10.022170
8.309405	678.765840	10.027187
8.823517	674.471628	10.032205
8.729216	674.002741	10.037223
8.755388	664.401071	10.042240
8.651960	647.478801	10.047258
8.726878	642.115267	10.052275
8.850973	631.729734	10.057293
8.781680	644.050788	10.062311
8.687804	635.287468	10.067328
8.820081	638.641845	10.072346
8.615237	641.503656	10.077363
8.839415	641.085177	10.082381
8.657320	642.311432	10.087399
8.599982	639.069669	10.092416
8.653844	640.426921	10.097434
8.680426	640.722221	10.102451
8.747318	643.693357	10.107469
8.792876	649.983569	10.112487
8.600063	643.221937	10.117504
8.601495	635.723464	10.122522
8.284828	642.899979	10.127539
8.336602	646.464527	10.132557
8.161329	646.279504	10.137575
8.309002	652.443366	10.142592
8.681062	662.245834	10.147610
8.742143	673.383583	10.152627
8.683089	670.829851	10.157645
8.638283	677.925934	10.162663
8.790646	670.290648	10.167680
8.985481	679.587072	10.172698
8.589633	669.670264	10.177715
8.842989	659.468020	10.182733
9.068836	667.039329	10.187751
9.068770	671.691535	10.192768
9.180649	662.602414	10.197786
8.781281	651.004807	10.202803
8.975566	647.109603	10.207821
8.769676	640.080864	10.212839
8.831690	639.923868	10.217856
8.872848	635.986311	10.222874
8.901729	645.548763	10.227891
9.101553	638.042239	10.232909
8.797570	647.993648	10.237927
8.435018	643.409990	10.242944
8.884845	634.834181	10.247962
8.746832	641.625623	10.252979
8.570356	661.431299	10.257997
8.973308	673.516314	10.263015
8.896694	675.255389	10.268032
9.131992	672.014372	10.273050
8.851453	675.131621	10.278067
8.986558	675.794755	10.283085
9.452642	672.552922	10.288103
9.056344	655.984631	10.293120
8.773548	648.178121	10.298138
8.664219	653.902679	10.303155
8.777846	661.290217	10.308173
8.975321	673.598616	10.313191
8.898880	678.263864	10.318208
9.105437	671.074694	10.323226
9.338223	676.103279	10.328243
9.365811	664.674319	10.333261
9.218192	650.318656	10.338279
8.803995	648.757536	10.343296
9.051212	635.745082	10.348314
8.668202	642.395608	10.353331
9.102219	657.137899	10.358349
8.819842	665.589377	10.363367
9.039432	664.155183	10.368384
9.427895	660.580163	10.373402
8.870599	674.063873	10.378419
9.341747	666.973009	10.383437
9.041937	669.326172	10.388455
9.233259	671.513763	10.393472
9.403144	660.282884	10.398490
9.107461	652.238362	10.403507
9.077437	639.486365	10.408525
8.837444	639.503780	10.413543
9.015243	660.268444	10.418560
9.322744	662.379712	10.423578
9.142438	673.644042	10.428595
9.386863	666.774568	10.433613
9.093132	663.741224	10.438631
9.091917	662.484923	10.443648
9.528263	660.313306	10.448666
9.006116	654.965175	10.453683
9.248917	654.061752	10.458701
9.266305	655.856908	10.463719
9.377592	656.909395	10.468736
9.122490	654.954630	10.473754
9.139489	658.613122	10.478771
9.426936	657.641679	10.483789
9.560164	652.544061	10.488807
8.933396	643.465851	10.493824
9.370094	645.221887	10.498842
9.093822	651.436264	10.503859
9.248161	665.671760	10.508877
9.483267	658.897527	10.513895
9.317467	665.394387	10.518912
9.660943	660.175735	10.523930
9.286822	644.749778	10.528947
9.446948	640.015796	10.533965
9.293551	634.415679	10.538983
8.939017	637.443999	10.544000
9.087632	645.051706	10.549018
9.266000	656.030267	10.554035
9.107466	664.906879	10.559053
9.420693	665.993246	10.564071
9.030681	668.906982	10.569088
9.408444	661.782768	10.574106
9.370355	673.362897	10.579123
9.251957	673.704644	10.584141
9.151332	667.835162	10.589159
9.265831	666.250270	10.594176
9.461490	668.561545	10.599194
9.281173	672.511359	10.604211
9.233187	671.356104	10.609229
9.403302	670.932797	10.614247
9.197604	680.186103	10.619264
9.562749	677.199158	10.624282
9.617876	691.940840	10.629299
9.409179	692.988445	10.634317
9.940378	690.222017	10.639335
9.781124	683.614644	10.644352
9.593986	666.659366	10.649370
9.553900	667.878643	10.654387
8.916177	675.399264	10.659405
9.265899	675.697746	10.664423
9.218078	694.693232	10.669440
9.651645	687.487329	10.674458
9.400017	691.744608	10.679475
9.893775	695.023787	10.684493
10.079361	687.735332	10.689511
9.691838	698.669841	10.694528
9.903679	684.433354	10.699546
9.605641	674.217293	10.704563
9.462189	660.879373	10.709581
9.530699	660.763031	10.714599
9.689000	690.670172	10.719616
9.711625	685.486926	10.724634
9.767087	689.840197	10.729651
9.594175	692.131801	10.734669
9.571557	682.503162	10.739687
9.628773	696.947277	10.744704
9.851906	697.795430	10.749722
9.525391	697.576793	10.754739
9.783208	698.786505	10.759757
9.754489	687.564084	10.764775
9.760982	700.766282	10.769792
9.685264	698.916445	10.774810
9.909509	692.660108	10.779827
9.906878	693.549582	10.784845
9.908921	690.225145	10.789863
9.565250	683.169204	10.794880
9.737038	685.947792	10.799898
9.485207	689.556324	10.804915
9.507038	697.051200	10.809933
9.806420	693.296053	10.814951
9.739592	695.189800	10.819968
9.981982	688.854480	10.824986
9.768825	700.166391	10.830003
9.796237	699.842694	10.835021
9.874788	696.624477	10.840039
9.806342	694.911224	10.845056
10.071698	694.262316	10.850074
9.857303	695.018362	10.855091
9.803463	691.575233	10.860109
10.349445	688.088683	10.865127
9.950953	694.285129	10.870144
9.836309	695.949406	10.875162
10.123778	689.208613	10.880179
9.955031	690.927121	10.885197
10.053827	683.810510	10.890215
9.966993	697.526161	10.895232
9.824408	685.743891	10.900250
10.144248	688.607012	10.905267
9.921664	688.701461	10.910285
10.475710	691.802162	10.915303
9.942906	691.440923	10.920320
9.884163	695.426908	10.925338
9.860350	689.203381	10.930355
10.017824	692.633514	10.935373
9.944236	695.523990	10.940391
9.572262	690.549776	10.945408
9.990432	694.561901	10.950426
9.935962	691.435787	10.955443
9.989165	695.704792	10.960461
10.233183	687.541358	10.965479
9.590377	690.646948	10.970496
9.846250	692.571506	10.975514
9.939086	699.584969	10.980531
9.745189	697.652344	10.985549
9.908042	691.019582	10.990567
10.178998	710.573683	10.995584
10.398677	714.423811	11.000602
10.386757	697.831195	11.005619
9.931811	697.761376	11.010637
9.964876	693.973167	11.015655
10.025264	713.493245	11.020672
10.235307	718.875196	11.025690
10.292727	723.129338	11.030707
10.353584	724.727552	11.035725
10.449362	709.433550	11.040743
10.574216	698.535671	11.045760
10.312838	690.787006	11.050778
10.568477	691.155789	11.055795
10.318217	698.118589	11.060813
10.720060	695.951499	11.065831
9.981625	693.493333	11.070848
9.999450	690.802466	11.075866
10.136176	690.604753	11.080883
10.046180	683.930009	11.085901
10.085296	679.262114	11.090919
10.252296	706.509344	11.095936
10.515229	711.443190	11.100954
10.724490	701.754490	11.105971
10.162931	693.002836	11.110989
10.470877	681.374693	11.116007
10.488593	688.728522	11.121024
10.183658	688.962584	11.126042
10.219003	680.762845	11.131059
10.226734	697.190627	11.136077
10.566957	706.784234	11.141095
10.420832	717.577214	11.146112
10.523458	705.614175	11.151130
10.557496	696.527689	11.156147
10.247204	689.894932	11.161165
10.094316	695.316107	11.166183
10.182839	708.865732	11.171200
10.608873	718.177830	11.176218
10.700707	729.260530	11.181235
10.402382	724.896121	11.186253
10.210245	719.020908	11.191271
10.399048	727.897518	11.196288
10.178365	724.154469	11.201306
10.755683	715.902760	11.206323
10.568574	718.028225	11.211341
10.647203	714.055311	11.216359
10.641637	719.072595	11.221376
10.515659	722.927208	11.226394
10.794433	725.536521	11.231411
10.674255	735.585890	11.236429
10.654735	717.119027	11.241447
10.649518	725.751401	11.246464
10.575844	722.715857	11.251482
10.957913	717.996673	11.256499
10.707885	720.145155	11.261517
10.775718	718.185329	11.266535
10.955292	720.007177	11.271552
10.665561	710.272366	11.276570
10.511328	690.318480	11.281587
10.646213	705.342621	11.286605
10.804377	712.189768	11.291623
10.914786	704.053961	11.296640
10.620407	708.692712	11.301658
10.708834	691.149682	11.306675
10.217576	706.890068	11.311693
10.582641	716.139036	11.316711
10.068935	720.310200	11.321728
10.355023	722.356523	11.326746
10.995026	718.581185	11.331763
10.507856	729.402696	11.336781
10.652601	717.055136	11.341799
10.717677	720.547423	11.346816
10.558243	718.992532	11.351834
11.073883	713.667013	11.356851
10.713198	715.174013	11.361869
10.832421	717.271587	11.366887
10.852063	720.114348	11.371904
10.441837	719.224178	11.376922
10.961993	726.500339	11.381939
10.813778	739.504185	11.386957
10.803321	750.337712	11.391975
11.087585	755.786515	11.396992
11.085106	752.301405	11.402010
10.999873	731.396723	11.407027
10.623486	729.280152	11.412045
10.873865	740.168900	11.417063
11.313525	745.731724	11.422080
11.034620	733.936165	11.427098
11.308763	714.557341	11.432115
10.988502	721.115625	11.437133
11.163709	718.717178	11.442151
11.100617	719.728469	11.447168
11.143415	722.232771	11.452186
11.090703	711.342240	11.457203
11.019976	725.836306	11.462221
10.693984	716.853516	11.467239
10.788929	712.703107	11.472256
10.988763	726.860263	11.477274
11.125538	710.970135	11.482291
11.081239	724.628376	11.487309
10.670707	715.915083	11.492327
11.418553	718.004228	11.497344
10.955411	718.873507	11.502362
11.274282	719.701478	11.507379
10.801746	727.154615	11.512397
11.030267	747.254735	11.517415
11.481960	747.655619	11.522432
11.201448	744.032701	11.527450
10.966819	729.223683	11.532467
10.863546	738.841144	11.537485
10.949808	748.803584	11.542503
11.189705	739.872737	11.547520
11.386380	753.079707	11.552538
11.133711	750.622192	11.557555
11.238433	754.928743	11.562573
11.139921	750.636745	11.567591
11.418265	750.074263	11.572608
11.150796	757.609986	11.577626
11.058244	747.794472	11.582643
10.917787	746.174629	11.587661
10.932065	753.000741	11.592679
11.099173	748.210062	11.597696
10.913781	757.932466	11.602714
11.108079	749.878015	11.607731
11.267504	755.772270	11.612749
11.367893	763.775008	11.617767
11.575659	764.320214	11.622784
11.382350	771.694460	11.627802
11.122285	755.260977	11.632819
11.339629	771.257693	11.637837
11.626098	783.568371	11.642855
11.265477	768.717188	11.647872
11.049519	771.839116	11.652890
11.694411	771.498993	11.657907
11.822493	780.256561	11.662925
11.261254	767.827055	11.667943
11.533722	775.211966	11.672960
11.558153	782.593073	11.677978
11.560299	766.042934	11.682995
11.440331	756.009920	11.688013
11.194916	760.092576	11.693031
11.797016	769.444051	11.698048
11.645118	776.232340	11.703066
11.370906	765.613475	11.708083
11.666821	771.579618	11.713101
11.634186	766.928302	11.718119
11.592133	753.276284	11.723136
11.074626	753.956546	11.728154
11.411732	766.045845	11.733171
11.767895	786.555172	11.738189
11.519441	790.141515	11.743207
11.729654	773.274647	11.748224
11.679370	789.944405	11.753242
11.714924	780.790692	11.758259
11.601712	783.153916	11.763277
11.535168	784.296091	11.768295
11.781028	777.488139	11.773312
11.361083	781.120986	11.778330
11.613561	778.948699	11.783347
11.842068	778.990105	11.788365
11.674587	783.250010	11.793383
11.682518	780.567064	11.798400
11.557287	776.276728	11.803418
11.308219	774.418974	11.808435
11.435269	779.001347	11.813453
11.522256	784.997367	11.818471
11.952443	780.691041	11.823488
11.626900	776.125623	11.828506
11.674811	778.212967	11.833523
11.517731	783.607310	11.838541
11.526172	778.239777	11.843559
11.876596	781.945050	11.848576
11.976726	788.429027	11.853594
11.966506	783.603137	11.858611
11.897702	774.461984	11.863629
11.877932	781.557118	11.868647
12.007103	774.320875	11.873664
11.826224	774.016707	11.878682
11.976545	772.986079	11.883699
12.008394	776.778353	11.888717
11.952935	787.582745	11.893735
12.099970	772.406172	11.898752
11.984763	770.458146	11.903770
12.075287	768.865010	11.908787
11.802295	770.103177	11.913805
11.598431	771.792865	11.918823
12.091730	770.996767	11.923840
11.851088	766.890102	11.928858
12.043516	773.145809	11.933875
12.072395	779.525051	11.938893
11.783882	788.660252	11.943911
12.609928	785.751683	11.948928
12.004420	789.071182	11.953946
11.763273	781.267943	11.958963
12.278046	780.130905	11.963981
11.705612	787.210869	11.968999
12.126427	788.498317	11.974016
12.254644	798.646351	11.979034
12.338448	807.552204	11.984051
12.397962	800.347955	11.989069
12.081625	783.106479	11.994087
12.200845	780.748000	11.999104
11.974570	774.636700	12.004122
12.113210	784.292080	12.009139
12.278003	785.241233	12.014157
12.065362	795.766556	12.019175
12.256689	803.370812	12.024192
12.401988	796.243299	12.029210
12.240353	795.470614	12.034227
12.197555	783.584348	12.039245
12.216213	798.438071	12.044263
12.343765	801.305103	12.049280
12.187834	794.121965	12.054298
12.001343	801.684063	12.059315
12.226484	802.361820	12.064333
11.823032	801.086291	12.069351
12.103167	798.767302	12.074368
12.216774	804.275089	12.079386
12.001004	803.285789	12.084403
12.326579	803.521741	12.089421
12.185837	796.274673	12.094439
12.239410	799.346858	12.099456
12.206061	804.701429	12.104474
12.082926	797.233740	12.109491
12.345762	809.651496	12.114509
12.644601	821.390894	12.119527
12.554143	808.401534	12.124544
12.635369	797.945433	12.129562
12.291370	798.389497	12.134579
12.354495	798.783862	12.139597
12.466659	804.884377	12.144615
12.787325	811.603879	12.149632
12.632578	807.725487	12.154650
12.463244	809.054362	12.159667
12.694450	797.357347	12.164685
12.451110	802.436470	12.169703
12.592883	804.158293	12.174720
12.825932	806.245298	12.179738
12.494640	799.548258	12.184755
12.381657	799.012780	12.189773
12.271795	802.036441	12.194791
12.835319	806.408366	12.199808
12.338244	802.583905	12.204826
12.294431	820.605310	12.209843
12.860420	832.079625	12.214861
12.845661	822.655886	12.219879
12.927097	817.937242	12.224896
12.576835	808.107674	12.229914
12.394028	816.781710	12.234931
12.964110	820.461643	12.239949
12.561057	832.284992	12.244967
12.780298	829.791446	12.249984
12.658424	829.657418	12.255002
12.358615	835.505312	12.260019
12.789309	825.333828	12.265037
12.625133	838.928559	12.270055
12.703179	831.696425	12.275072
13.012751	836.419055	12.280090
12.870017	843.664888	12.285107
12.793545	833.391168	12.290125
12.570931	837.032689	12.295143
12.920162	828.841523	12.300160
13.134492	833.788575	12.305178
12.818569	830.900992	12.310195
12.822565	829.079670	12.315213
12.572967	836.629007	12.320231
12.889573	827.506283	12.325248
12.788599	835.550668	12.330266
12.909750	824.209636	12.335283
13.150823	829.758526	12.340301
12.660352	832.820416	12.345319
12.750605	832.912273	12.350336
13.040900	828.909398	12.355354
13.076473	828.653241	12.360371
13.099310	827.930319	12.365389
12.703063	823.065981	12.370407
12.970268	827.909398	12.375424
12.853199	825.276275	12.380442
12.757326	836.747596	12.385459
13.008274	831.478465	12.390477
13.031157	831.961380	12.395495
13.289639	844.603103	12.400512
13.234288	840.898786	12.405530
12.837049	834.986235	12.410547
13.321184	840.748412	12.415565
13.073906	834.580726	12.420583
12.897609	836.576471	12.425600
13.214074	837.230840	12.430618
13.426161	849.084226	12.435635
13.261965	844.858194	12.440653
13.155217	839.337676	12.445671
13.110683	838.688898	12.450688
13.322184	836.129706	12.455706
13.025305	836.899416	12.460723
13.142701	833.480261	12.465741
13.642429	845.262787	12.470759
13.528224	832.232459	12.475776
13.157257	830.183870	12.480794
13.095741	828.807626	12.485811
13.252604	813.722688	12.490829
13.342368	827.307248	12.495847
13.025906	831.927645	12.500864
13.525304	841.979995	12.505882
13.588562	850.140886	12.510899
13.508219	832.981531	12.515917
13.296560	828.629906	12.520935
13.239575	817.518759	12.525952
13.579269	829.199432	12.530970
13.290531	834.847078	12.535987
13.240472	831.412740	12.541005
13.410679	843.923417	12.546023
13.235426	858.044383	12.551040
13.758267	845.328223	12.556058
13.278622	856.848147	12.561075
13.704861	849.285920	12.566093
13.557270	856.239270	12.571111
13.419315	852.736021	12.576128
13.605204	858.382638	12.581146
13.713251	852.233663	12.586163
13.782084	849.398895	12.591181
13.619544	844.257280	12.596199
13.346571	833.349989	12.601216
13.499090	838.873391	12.606234
13.382888	851.182300	12.611251
13.675651	854.916823	12.616269
13.638407	853.740878	12.621287
13.441587	853.681068	12.626304
13.963432	854.267968	12.631322
13.568826	851.058780	12.636339
13.730656	855.224413	12.641357
13.514921	854.497689	12.646375
13.517507	862.782014	12.651392
13.565256	854.595877	12.656410
13.104785	857.467379	12.661427
13.626374	853.659259	12.666445
13.690330	854.387723	12.671463
13.611735	852.749357	12.676480
13.655870	849.720657	12.681498
13.399880	864.083727	12.686515
13.371969	857.373826	12.691533
13.671113	873.116956	12.696551
13.580860	886.273130	12.701568
13.945039	889.545464	12.706586
14.235852	879.340811	12.711603
13.926509	884.012011	12.716621
14.104053	879.989606	12.721639
13.771621	885.535455	12.726656
14.308718	873.853870	12.731674
13.858660	871.462483	12.736691
13.829227	861.321500	12.741709
13.988432	872.652190	12.746727
13.842802	886.516320	12.751744
14.029509	882.636091	12.756762
13.893047	883.564271	12.761779
13.993571	883.714661	12.766797
13.965387	880.924692	12.771815
14.226420	883.327924	12.776832
14.545653	874.373628	12.781850
14.193061	865.518772	12.786867
13.970344	854.011440	12.791885
14.442594	858.022528	12.796903
13.969663	849.804900	12.801920
14.416623	854.200864	12.806938
13.797080	848.494402	12.811955
14.017247	845.556233	12.816973
13.976100	849.018503	12.821991
13.884321	851.099462	12.827008
14.504898	855.101735	12.832026
13.974379	852.215826	12.837043
13.772603	848.507408	12.842061
14.291507	859.289968	12.847079
14.166058	875.726607	12.852096
14.557049	875.671820	12.857114
14.244713	876.587786	12.862131
13.948701	881.462280	12.867149
14.386091	874.857598	12.872167
14.307082	884.684114	12.877184
14.465555	884.055260	12.882202
14.316231	882.477025	12.887219
14.218776	876.901414	12.892237
14.474340	882.810505	12.897255
14.210332	880.948913	12.902272
14.398925	885.688049	12.907290
14.595555	884.942251	12.912307
14.520135	886.144169	12.917325
14.314629	887.129449	12.922343
14.530102	889.073713	12.927360
14.309641	874.146861	12.932378
14.093986	879.034818	12.937395
14.321879	884.154829	12.942413
14.574308	879.833030	12.947431
14.311951	885.033038	12.952448
14.420040	887.747805	12.957466
14.410330	889.799826	12.962483
14.354613	878.041605	12.967501
14.615304	879.051652	12.972519
14.362426	890.292724	12.977536
14.553598	882.197385	12.982554
14.577875	887.261747	12.987571
14.293108	885.296904	12.992589
14.216067	893.098784	12.997607
14.353788	885.342200	13.002624
14.303328	877.095152	13.007642
14.493713	889.637169	13.012659
14.607651	900.064787	13.017677
14.873685	902.224292	13.022695
14.755844	909.366432	13.027712
14.975045	912.674193	13.032730
15.020579	905.295447	13.037747
14.605394	893.734920	13.042765
14.929684	885.088427	13.047783
14.908040	889.283663	13.052800
15.003827	887.049122	13.057818
14.724224	880.446239	13.062835
14.226776	882.597525	13.067853
15.279890	884.074361	13.072871
14.927437	888.077536	13.077888
14.650763	884.049637	13.082906
14.546417	886.682263	13.087923
14.837027	913.445237	13.092941
14.627754	907.706642	13.097959
14.653991	909.802317	13.102976
15.120807	906.747708	13.107994
15.251214	909.118640	13.113011
14.781435	907.915105	13.118029
14.821308	906.882679	13.123047
15.250099	918.090420	13.128064
15.219199	908.258296	13.133082
15.286764	901.926643	13.138099
15.190893	896.180691	13.143117
15.506555	877.655772	13.148135
15.264735	875.327143	13.153152
15.125153	874.925981	13.158170
15.399034	872.209611	13.163187
15.114922	877.219528	13.168205
15.396108	874.592495	13.173223
14.955679	873.227024	13.178240
15.178442	871.458838	13.183258
15.156688	869.126445	13.188275
14.704058	874.453621	13.193293
15.178747	873.816105	13.198311
15.211239	877.273274	13.203328
15.032042	878.241600	13.208346
14.761996	878.197064	13.213363
14.858183	878.862321	13.218381
15.342344	865.787212	13.223399
15.048029	879.560607	13.228416
15.193420	873.572361	13.233434
15.646476	884.038692	13.238451
15.037649	876.114013	13.243469
15.177498	882.667039	13.248487
15.221211	893.347608	13.253504
15.308756	898.182216	13.258522
15.260189	903.324390	13.263539
15.519529	908.932880	13.268557
15.787503	895.085313	13.273575
15.241739	885.009340	13.278592
15.134486	885.989374	13.283610
15.455430	896.757892	13.288627
15.370006	907.059084	13.293645
15.647927	904.278263	13.298663
15.355577	902.643399	13.303680
15.658921	900.871315	13.308698
15.496183	901.446383	13.313715
15.110411	912.896869	13.318733
15.688033	906.759877	13.323751
15.487640	908.921424	13.328768
15.545182	908.850989	13.333786
15.473683	909.210959	13.338803
15.442743	909.640193	13.343821
15.485398	906.623144	13.348839
15.550741	906.207732	13.353856
15.246606	909.359248	13.358874
15.416500	904.497591	13.363891
15.684697	908.162576	13.368909
15.599653	900.674357	13.373927
15.265308	901.147138	13.378944
15.323481	908.089273	13.383962
15.730779	917.756548	13.388979
15.723511	926.946042	13.393997
15.801737	927.730412	13.399015
15.478471	927.991920	13.404032
15.851904	934.779506	13.409050
15.861029	934.750945	13.414067
15.572650	937.299884	13.419085
15.895675	938.859826	13.424103
16.025965	941.088663	13.429120
16.079087	941.976399	13.434138
16.074184	923.676547	13.439155
15.946597	921.675043	13.444173
15.805485	904.783533	13.449191
16.030367	897.574296	13.454208
15.959208	906.662158	13.459226
15.983169	905.193804	13.464243
15.848953	906.224365	13.469261
16.059930	903.189287	13.474279
16.179557	907.230039	13.479296
15.842223	912.866469	13.484314
16.308706	899.802525	13.489331
16.026091	911.787086	13.494349
15.994744	906.137527	13.499367
15.672893	895.966599	13.504384
15.899561	909.320303	13.509402
16.156661	917.050726	13.514419
16.169370	930.398934	13.519437
16.062731	918.015284	13.524455
16.140677	913.486552	13.529472
16.344684	909.218430	13.534490
16.330793	907.403210	13.539507
15.951992	909.246677	13.544525
16.062181	901.766679	13.549543
16.011162	917.636338	13.554560
15.766201	928.672592	13.559578
16.212481	927.730736	13.564595
16.248997	932.740727	13.569613
16.263327	928.333149	13.574631
16.470330	934.824686	13.579648
16.306860	929.495409	13.584666
16.516035	931.103729	13.589683
16.380091	926.462778	13.594701
16.310505	924.561901	13.599719
16.219637	930.998040	13.604736
16.435049	930.168031	13.609754
16.712481	937.694319	13.614771
16.439883	930.356428	13.619789
16.236119	936.350260	13.624807
16.432880	932.540792	13.629824
16.430549	938.394188	13.634842
16.587073	930.201810	13.639859
16.148509	939.395408	13.644877
16.111995	929.780333	13.649895
16.253230	931.047162	13.654912
16.300912	935.715555	13.659930
16.679126	935.262508	13.664947
16.021803	938.013478	13.669965
16.131682	927.178940	13.674983
16.458791	932.115222	13.680000
16.180639	951.362932	13.685018
16.704110	953.005034	13.690035
16.729547	962.050557	13.695053
16.437013	959.734643	13.700071
16.873643	965.767321	13.705088
16.647301	960.703946	13.710106
16.697534	961.825223	13.715123
16.388197	966.481092	13.720141
16.658788	959.508342	13.725159
16.923323	949.916630	13.730176
16.638012	963.115010	13.735194
16.648705	951.467386	13.740211
16.650773	960.217971	13.745229
16.734944	957.095617	13.750247
17.101579	954.743779	13.755264
16.754443	958.333509	13.760282
16.859306	960.518924	13.765299
16.969842	962.079015	13.770317
17.188018	956.106637	13.775335
17.143609	948.890394	13.780352
17.053744	952.212729	13.785370
17.093329	952.573596	13.790387
16.951135	957.402172	13.795405
16.871278	953.212143	13.800423
16.920740	948.807009	13.805440
16.633804	949.803415	13.810458
16.790397	952.665273	13.815475
16.827233	959.421208	13.820493
16.787350	952.362082	13.825511
16.916911	956.015391	13.830528
16.716251	959.855659	13.835546
16.800318	955.615652	13.840563
16.871915	964.532278	13.845581
16.995012	970.011782	13.850599
17.340744	982.118326	13.855616
17.350322	984.590770	13.860634
17.566425	988.135272	13.865651
17.580080	970.085826	13.870669
17.157215	959.314678	13.875687
17.205140	955.326315	13.880704
16.809205	955.393565	13.885722
17.297378	957.605268	13.890739
17.543238	968.341783	13.895757
17.019767	968.788011	13.900775
17.424296	962.575332	13.905792
17.258759	964.838591	13.910810
17.273943	971.249706	13.915827
17.537123	975.508034	13.920845
17.301837	977.300580	13.925863
17.607316	976.122205	13.930880
17.580743	968.021933	13.935898
17.407500	950.083769	13.940915
17.660977	949.278951	13.945933
17.425462	947.594515	13.950951
17.416280	952.351460	13.955968
17.210826	955.803167	13.960986
17.317522	950.750000	13.966003
17.408548	964.974602	13.971021
17.677881	977.442204	13.976039
17.672203	979.441996	13.981056
17.657851	984.701362	13.986074
17.973150	974.065444	13.991091
17.735955	953.885988	13.996109
17.249348	954.898529	14.001127
17.175182	953.242097	14.006144
17.285008	980.422114	14.011162
17.583858	976.219762	14.016179
17.705598	974.191925	14.021197
17.716089	981.656535	14.026215
17.775513	977.459577	14.031232
17.564804	992.699484	14.036250
17.806233	978.273584	14.041267
18.035226	976.314598	14.046285
17.659752	982.354203	14.051303
18.133545	977.667782	14.056320
17.754272	983.725732	14.061338
18.001728	984.713570	14.066355
17.862903	981.886787	14.071373
17.833396	987.156930	14.076391
18.189008	985.252171	14.081408
18.061096	986.929698	14.086426
17.984067	984.828479	14.091443
18.045694	980.800047	14.096461
18.019333	985.446859	14.101479
17.812281	974.743110	14.106496
18.011756	981.488266	14.111514
18.017259	984.396800	14.116531
18.129981	979.457188	14.121549
18.065129	973.251365	14.126567
18.106160	973.653330	14.131584
18.275306	980.766091	14.136602
17.968612	982.050404	14.141619
18.256372	971.381648	14.146637
18.206805	983.775294	14.151655
18.085604	969.227960	14.156672
18.067763	979.454627	14.161690
18.086613	974.253800	14.166707
18.292772	975.015414	14.171725
18.065867	981.003252	14.176743
18.357201	976.714747	14.181760
18.074675	976.445908	14.186778
17.918323	974.035004	14.191795
18.011372	964.794894	14.196813
18.106090	983.945076	14.201831
18.408560	972.028659	14.206848
18.142807	963.559744	14.211866
18.021899	965.143593	14.216883
18.658888	965.977956	14.221901
18.363136	972.996835	14.226919
18.135620	967.476583	14.231936
18.084436	968.932357	14.236954
18.164104	979.329091	14.241971
18.172479	975.655133	14.246989
17.638821	982.927181	14.252007
18.223421	991.412040	14.257024
18.287341	1003.993594	14.262042
18.316049	998.519878	14.267059
18.933291	995.167126	14.272077
18.825684	993.811097	14.277095
19.005913	995.609642	14.282112
18.900079	998.581102	14.287130
18.827446	992.367898	14.292147
19.134637	987.644891	14.297165
19.085570	986.848832	14.302183
19.075253	971.649302	14.307200
18.774099	961.030039	14.312218
18.862932	955.310172	14.317235
19.028224	950.094552	14.322253
18.563075	965.767886	14.327271
18.712571	963.127212	14.332288
18.723236	956.303011	14.337306
18.661674	961.687504	14.342323
18.851083	954.040039	14.347341
18.287082	959.147506	14.352359
18.510683	951.015267	14.357376
18.801216	964.199002	14.362394
18.830595	983.848567	14.367411
18.852218	989.109850	14.372429
18.411124	990.970728	14.377447
18.687951	990.493525	14.382464
18.982715	986.109964	14.387482
18.809075	991.722466	14.392499
19.077353	990.809294	14.397517
18.919693	993.248018	14.402535
19.053696	980.929978	14.407552
18.867075	984.533685	14.412570
18.709947	982.342584	14.417587
19.328049	979.919183	14.422605
19.098805	991.362312	14.427623
19.012348	990.794088	14.432640
19.306826	986.525531	14.437658
18.988440	985.120156	14.442675
19.136657	977.723584	14.447693
18.624729	988.408040	14.452711
19.032098	985.228226	14.457728
19.048645	997.225124	14.462746
19.269115	1015.514005	14.467763
19.614207	1014.571578	14.472781
19.378059	1005.232810	14.477799
19.076497	991.406238	14.482816
19.322249	995.617066	14.487834
19.523709	1007.644374	14.492851
19.767846	988.481979	14.497869
19.320552	994.952362	14.502887
19.230357	990.803403	14.507904
19.538901	984.668025	14.512922
19.316273	977.160032	14.517939
19.491870	976.732268	14.522957
19.438125	987.167632	14.527975
19.383720	982.665126	14.532992
19.599192	978.243518	14.538010
19.493840	981.758179	14.543027
19.567222	980.321791	14.548045
19.494759	981.822033	14.553063
19.184356	983.941179	14.558080
19.579235	1000.643746	14.563098
19.393317	1012.426158	14.568115
19.711683	1012.449537	14.573133
19.670101	1012.105763	14.578151
19.826394	1011.600488	14.583168
20.011344	1015.173383	14.588186
19.638296	1015.619112	14.593203
19.908392	1011.953381	14.598221
20.224800	1011.757014	14.603239
19.683145	998.940627	14.608256
19.549679	989.265981	14.613274
19.802143	987.132642	14.618291
19.942394	979.693690	14.623309
19.696515	987.649948	14.628327
19.988784	978.442193	14.633344
20.010161	972.600029	14.638362
19.458111	983.504108	14.643379
19.699240	989.938445	14.648397
19.715703	998.554784	14.653415
19.825891	1003.194345	14.658432
19.883101	1000.759490	14.663450
19.605477	1006.766760	14.668467
20.055562	1006.449837	14.673485
19.990725	1013.289558	14.678503
19.878650	1009.776476	14.683520
19.977437	1006.507603	14.688538
19.820144	1014.126383	14.693555
19.814367	1014.681764	14.698573
19.745702	1011.382745	14.703591
20.099751	1020.458531	14.708608
20.252172	1025.502507	14.713626
19.785380	1034.415807	14.718643
20.260331	1034.040043	14.723661
20.831714	1044.395949	14.728679
20.360857	1024.719249	14.733696
20.370063	1009.267639	14.738714
19.947278	1011.115252	14.743731
20.275016	999.809172	14.748749
19.891644	1010.795571	14.753767
20.264672	1027.137232	14.758784
20.655620	1030.036674	14.763802
20.574612	1032.050521	14.768819
20.543941	1022.506465	14.773837
20.508385	1032.477842	14.778855
20.212098	1021.813639	14.783872
20.672221	1027.330267	14.788890
20.715762	1021.378119	14.793907
20.419976	1007.404519	14.798925
20.672406	1004.048790	14.803943
20.489868	1006.245582	14.808960
20.650634	1004.382533	14.813978
20.327681	1007.662376	14.818995
20.503421	998.731769	14.824013
20.540095	1004.779905	14.829031
20.333049	1025.938693	14.834048
20.634282	1027.059750	14.839066
20.650646	1029.132274	14.844083
20.732879	1028.631782	14.849101
20.804306	1034.938732	14.854119
20.634173	1032.685213	14.859136
20.939855	1032.165831	14.864154
20.920311	1038.915783	14.869171
20.970070	1033.107478	14.874189
20.812646	1023.391503	14.879207
20.798913	1017.192945	14.884224
20.657725	1017.942789	14.889242
20.665891	1026.699094	14.894259
20.596223	1027.788657	14.899277
20.927797	1032.984853	14.904295
20.834627	1030.155619	14.909312
21.299277	1030.727195	14.914330
20.792515	1023.373312	14.919347
20.768980	1035.532382	14.924365
21.192069	1030.220113	14.929383
21.201441	1034.599616	14.934400
21.196085	1018.896874	14.939418
21.159487	1037.778722	14.944435
21.092120	1021.992548	14.949453
21.199023	1024.597697	14.954471
21.124410	1031.584315	14.959488
21.266994	1019.974640	14.964506
21.026964	1031.178647	14.969523
21.195657	1024.638867	14.974541
21.154510	1022.359660	14.979559
21.018973	1031.442509	14.984576
21.607377	1015.055648	14.989594
21.229754	1019.558673	14.994611
21.110268	1028.867594	14.999629
21.240491	1023.872316	15.004647
20.979917	1023.169936	15.009664
21.139386	1023.910151	15.014682
21.153553	1025.486994	15.019699
20.939619	1023.611581	15.024717
21.220043	1019.920517	15.029735
21.271005	1026.315889	15.034752
21.262375	1020.036173	15.039770
20.903396	1029.125311	15.044787
21.069324	1046.856746	15.049805
21.440237	1051.425985	15.054823
21.312942	1062.684180	15.059840
21.764207	1057.398338	15.064858
21.398469	1053.457187	15.069875
21.313372	1049.551454	15.074893
21.472377	1043.026656	15.079911
21.504205	1055.778521	15.084928
21.689591	1045.304613	15.089946
21.597289	1051.039883	15.094963
21.482519	1056.709588	15.099981
21.820179	1045.993937	15.104999
21.925670	1044.363256	15.110016
21.925720	1038.639949	15.115034
21.984023	1052.081890	15.120051
21.848871	1046.554977	15.125069
21.799738	1050.639064	15.130087
21.847046	1053.962722	15.135104
22.200656	1051.278394	15.140122
21.919985	1044.362636	15.145139
22.192309	1043.704294	15.150157
22.213331	1039.993975	15.155175
21.979861	1051.777993	15.160192
21.979904	1040.963925	15.165210
22.078205	1048.952590	15.170227
22.100532	1048.685237	15.175245
22.305174	1046.970818	15.180263
21.699123	1055.207607	15.185280
21.951502	1046.193813	15.190298
21.895090	1052.380605	15.195315
21.850405	1047.812692	15.200333
21.942696	1038.448652	15.205351
21.937712	1041.309330	15.210368
21.876312	1047.720953	15.215386
21.962173	1040.768126	15.220403
22.150245	1053.638994	15.225421
22.255886	1042.537764	15.230439
21.950221	1048.627250	15.235456
22.412312	1061.687782	15.240474
22.619405	1064.229893	15.245491
22.146197	1052.572165	15.250509
22.230903	1059.800515	15.255527
22.248349	1064.380257	15.260544
22.278014	1065.107717	15.265562
22.542823	1072.966071	15.270579
22.259458	1073.000902	15.275597
22.166698	1075.605657	15.280615
22.365834	1080.959228	15.285632
22.478512	1076.090850	15.290650
22.556067	1076.939903	15.295667
22.070927	1075.390878	15.300685
22.639227	1074.807143	15.305703
22.530282	1075.474488	15.310720
22.750867	1073.194847	15.315738
22.698059	1079.977095	15.320755
22.462757	1073.814022	15.325773
22.768701	1067.801872	15.330791
22.538793	1077.693653	15.335808
22.597475	1075.261299	15.340826
22.912704	1071.438086	15.345843
22.564614	1069.762828	15.350861
22.745371	1063.115920	15.355879
22.974075	1075.950159	15.360896
23.124212	1071.069280	15.365914
22.657770	1064.458674	15.370931
22.709867	1069.453137	15.375949
22.716354	1072.146573	15.380967
22.644438	1067.396556	15.385984
22.528780	1065.165112	15.391002
22.835246	1078.445516	15.396019
23.049446	1093.172658	15.401037
23.315129	1089.825739	15.406055
23.189182	1082.463492	15.411072
23.080845	1072.964941	15.416090
23.192349	1064.774829	15.421107
22.951967	1062.482151	15.426125
23.406623	1059.078752	15.431143
23.088960	1058.797620	15.436160
23.068061	1059.631875	15.441178
23.282387	1059.504377	15.446195
22.937141	1051.924923	15.451213
23.104598	1060.967459	15.456231
23.213072	1077.770288	15.461248
23.405415	1085.130035	15.466266
23.223169	1082.735605	15.471283
23.388134	1089.177871	15.476301
23.590455	1077.593694	15.481319
23.521283	1069.641363	15.486336
23.402193	1052.527154	15.491354
23.506388	1051.267934	15.496371
22.914610	1058.273272	15.501389
23.354645	1065.227048	15.506407
23.229675	1076.147872	15.511424
23.471395	1077.232726	15.516442
23.539972	1084.035033	15.521459
23.203656	1082.051141	15.526477
23.597723	1079.278222	15.531495
23.672277	1082.444230	15.536512
23.775987	1087.658098	15.541530
23.642728	1074.158296	15.546547
23.738621	1086.435027	15.551565
23.840669	1076.632749	15.556583
23.882413	1081.694283	15.561600
24.004497	1080.745473	15.566618
24.097064	1062.358453	15.571635
23.639453	1057.984498	15.576653
23.317516	1055.890359	15.581671
23.555028	1055.061803	15.586688
23.581754	1071.719112	15.591706
23.678361	1083.231970	15.596723
23.790620	1092.389173	15.601741
23.884667	1090.885181	15.606759
23.609367	1087.940823	15.611776
23.899075	1085.174554	15.616794
24.041757	1075.013198	15.621811
24.033940	1085.033951	15.626829
24.044022	1086.105982	15.631847
24.154624	1088.210152	15.636864
23.810046	1091.410525	15.641882
23.504285	1088.715691	15.646899
23.944099	1083.892745	15.651917
24.014162	1076.968107	15.656935
23.893713	1078.807001	15.661952
23.711119	1105.310881	15.666970
23.975418	1101.512235	15.671987
23.987013	1106.030755	15.677005
23.963511	1108.576805	15.682023
24.365072	1109.752907	15.687040
24.664374	1106.159481	15.692058
24.611917	1097.426440	15.697075
24.380756	1103.793758	15.702093
24.759327	1099.000239	15.707111
24.781005	1104.180847	15.712128
24.359377	1097.564774	15.717146
24.625638	1083.781494	15.722163
24.544719	1077.687340	15.727181
24.268623	1067.341798	15.732199
24.342181	1080.624944	15.737216
24.542197	1089.749505	15.742234
24.752018	1097.406747	15.747251
24.679249	1099.047204	15.752269
24.459032	1092.020237	15.757287
24.740815	1092.654378	15.762304
25.024137	1101.160053	15.767322
24.930164	1076.271049	15.772339
24.527999	1077.781800	15.777357
24.543177	1066.351056	15.782375
24.621140	1074.873005	15.787392
24.574654	1079.088940	15.792410
24.655959	1097.211205	15.797427
24.564638	1097.313446	15.802445
25.059517	1092.266426	15.807463
25.179678	1095.508346	15.812480
24.983315	1107.167762	15.817498
24.925571	1099.750907	15.822515
25.128722	1092.331406	15.827533
24.200389	1084.863445	15.832551
24.519137	1096.434409	15.837568
24.658770	1100.775038	15.842586
25.219163	1094.969949	15.847603
24.694603	1099.900464	15.852621
24.762480	1097.244150	15.857639
24.889315	1093.561179	15.862656
24.823345	1103.708499	15.867674
25.062510	1101.335622	15.872691
25.090506	1119.894286	15.877709
25.351548	1116.571358	15.882727
25.413088	1106.623017	15.887744
24.811432	1099.895026	15.892762
25.027472	1103.867504	15.897779
25.283668	1121.913596	15.902797
25.520882	1125.685337	15.907815
25.827118	1122.106900	15.912832
25.537421	1118.657456	15.917850
25.798547	1095.125719	15.922867
25.483403	1089.109321	15.927885
25.784716	1091.396078	15.932903
25.598609	1084.965021	15.937920
25.329635	1085.503357	15.942938
25.389570	1076.072607	15.947955
25.144743	1081.466228	15.952973
25.217613	1077.621730	15.957991
25.678656	1079.532049	15.963008
25.419724	1082.389116	15.968026
25.658744	1087.567193	15.973043
25.491043	1099.154142	15.978061
25.404848	1111.255540	15.983079
25.944821	1112.802018	15.988096
25.917466	1114.808960	15.993114
25.884044	1113.576065	15.998131
26.031795	1118.690134	16.003149
25.482931	1100.510065	16.008167
25.807588	1094.523545	16.013184
25.449109	1110.493524	16.018202
26.039921	1101.637430	16.023219
25.982014	1112.319230	16.028237
25.518700	1128.054625	16.033255
25.921786	1113.218773	16.038272
25.963812	1119.447165	16.043290
25.910918	1116.795098	16.048307
25.740677	1112.465272	16.053325
25.898044	1111.615339	16.058343
25.991678	1117.753297	16.063360
25.743267	1119.968886	16.068378
26.008793	1114.954718	16.073395
26.064948	1113.801082	16.078413
26.110491	1120.439508	16.083431
26.213485	1116.538832	16.088448
25.983399	1120.317478	16.093466
25.922231	1126.375958	16.098483
26.335827	1130.365730	16.103501
26.309359	1138.042434	16.108519
26.790163	1133.926443	16.113536
26.378266	1140.293389	16.118554
26.511615	1139.812775	16.123571
26.619395	1137.906124	16.128589
26.516399	1129.237731	16.133607
26.392357	1118.346913	16.138624
26.183952	1122.110160	16.143642
26.372850	1125.448182	16.148659
26.480117	1130.376838	16.153677
26.671154	1137.488803	16.158695
26.566725	1125.252648	16.163712
26.575752	1135.894247	16.168730
26.655382	1123.400852	16.173747
26.643099	1133.812915	16.178765
26.468089	1126.506407	16.183783
26.669392	1129.222317	16.188800
26.314133	1136.484186	16.193818
26.426630	1132.211865	16.198835
26.570351	1130.361466	16.203853
26.715151	1138.035400	16.208871
26.535481	1137.788502	16.213888
26.758660	1140.830702	16.218906
26.911972	1129.230980	16.223923
26.737826	1144.205933	16.228941
26.966025	1152.713678	16.233959
27.085776	1164.866446	16.238976
26.949300	1171.539365	16.243994
27.031612	1167.416123	16.249011
26.917093	1163.455786	16.254029
26.975642	1167.920487	16.259047
27.093764	1166.284947	16.264064
26.980233	1167.201866	16.269082
27.266576	1169.222618	16.274099
27.542524	1163.722864	16.279117
27.281316	1161.733611	16.284135
27.432086	1155.899086	16.289152
27.077318	1143.924441	16.294170
27.070552	1143.426871	16.299187
27.347033	1158.478005	16.304205
26.840712	1157.441518	16.309223
27.440560	1154.985683	16.314240
27.060994	1162.732283	16.319258
27.251565	1159.394244	16.324275
27.577538	1146.637605	16.329293
27.451837	1157.705454	16.334311
27.336176	1151.011136	16.339328
27.415992	1159.277320	16.344346
27.588222	1164.920801	16.349363
27.467193	1162.215049	16.354381
27.524285	1160.281356	16.359399
27.747126	1152.042841	16.364416
27.606993	1162.662703	16.369434
27.347013	1160.406325	16.374451
27.401146	1154.986216	16.379469
27.627775	1155.034234	16.384487
27.925706	1164.365454	16.389504
27.582904	1166.456919	16.394522
27.795200	1177.064889	16.399539
28.072156	1188.846773	16.404557
27.709479	1184.390922	16.409575
28.285897	1181.735030	16.414592
28.316160	1167.850993	16.419610
27.664869	1158.846613	16.424627
28.053315	1153.129028	16.429645
27.468433	1158.589613	16.434663
27.993674	1161.745576	16.439680
28.014644	1173.418265	16.444698
28.299573	1178.541135	16.449715
28.358093	1176.674524	16.454733
28.137574	1182.211395	16.459751
28.142132	1180.177346	16.464768
28.105509	1180.925630	16.469786
27.862759	1171.370930	16.474803
27.703476	1166.375514	16.479821
28.121539	1178.903689	16.484839
28.338741	1178.891853	16.489856
28.400459	1180.469106	16.494874
28.381630	1179.121194	16.499891
28.318300	1173.154008	16.504909
27.777485	1178.470693	16.509927
28.120580	1174.202696	16.514944
28.365087	1184.782897	16.519962
28.229978	1202.134055	16.524979
28.687337	1201.988361	16.529997
28.720234	1210.892641	16.535015
28.889318	1211.101760	16.540032
28.529375	1210.470941	16.545050
28.364989	1206.830259	16.550067
28.786974	1200.667745	16.555085
28.835364	1205.862073	16.560103
28.974907	1205.563892	16.565120
28.973876	1186.174927	16.570138
28.711209	1176.192038	16.575155
28.666222	1171.122972	16.580173
28.565526	1175.225866	16.585191
28.816022	1175.776218	16.590208
28.959670	1192.848538	16.595226
28.657785	1201.481483	16.600243
29.223175	1198.643562	16.605261
29.023566	1201.188867	16.610279
29.140056	1206.170350	16.615296
29.116940	1208.768714	16.620314
29.240333	1195.959360	16.625331
29.132828	1173.718432	16.630349
28.752125	1177.762183	16.635367
28.715133	1188.951188	16.640384
28.958558	1198.302083	16.645402
28.900736	1206.622579	16.650419
29.191384	1199.892851	16.655437
28.744564	1206.565205	16.660455
29.223468	1198.643311	16.665472
29.018987	1207.612878	16.670490
29.285528	1206.168500	16.675507
29.700606	1198.042221	16.680525
29.039584	1201.859173	16.685543
29.197572	1203.900002	16.690560
29.364985	1196.760377	16.695578
29.478636	1218.796617	16.700595
29.629776	1220.691736	16.705613
29.583470	1234.516503	16.710631
29.572419	1232.541723	16.715648
29.799408	1225.672922	16.720666
29.434868	1214.470293	16.725683
29.340832	1211.670302	16.730701
29.857943	1223.646299	16.735719
29.840140	1225.845371	16.740736
30.088373	1229.188551	16.745754
29.776857	1210.330877	16.750771
29.705746	1195.110486	16.755789
29.885915	1203.712824	16.760807
29.652653	1216.121325	16.765824
29.953674	1224.281233	16.770842
29.870330	1227.914743	16.775859
30.065889	1217.979966	16.780877
29.787067	1232.152672	16.785895
29.887854	1215.660914	16.790912
30.307648	1210.273149	16.795930
29.962592	1224.698936	16.800947
30.290032	1211.003441	16.805965
30.068055	1216.194905	16.810983
29.766307	1215.053675	16.816000
29.754058	1211.387407	16.821018
30.067938	1211.541842	16.826035
30.134613	1211.665558	16.831053
30.164551	1217.084594	16.836071
30.072709	1219.565208	16.841088
30.248719	1211.834798	16.846106
30.006780	1218.262607	16.851123
30.144696	1211.503441	16.856141
30.427634	1223.792617	16.861159
30.218736	1238.176973	16.866176
30.559253	1240.691509	16.871194
30.692040	1239.154711	16.876211
30.952963	1237.619137	16.881229
30.437465	1227.198563	16.886247
30.589486	1219.154806	16.891264
30.717689	1217.868370	16.896282
30.582741	1214.251551	16.901299
30.596103	1204.934730	16.906317
30.499911	1216.558350	16.911335
30.720324	1220.930125	16.916352
31.087427	1242.141773	16.921370
30.655395	1231.819579	16.926387
30.502631	1223.955023	16.931405
30.582509	1225.434394	16.936423
30.666581	1238.732077	16.941440
30.745700	1241.362335	16.946458
30.793162	1241.268372	16.951475
30.901704	1238.529712	16.956493
30.819948	1245.177066	16.961511
30.687541	1237.710305	16.966528
30.878787	1235.267786	16.971546
30.778951	1246.036146	16.976563
31.132944	1248.217751	16.981581
30.857534	1242.873830	16.986599
30.675711	1264.373247	16.991616
31.083680	1270.211191	16.996634
31.084981	1272.155142	17.001651
31.342802	1270.857081	17.006669
31.442929	1265.886000	17.011687
31.699886	1250.913981	17.016704
31.609286	1252.151116	17.021722
31.326785	1264.880794	17.026739
31.436872	1259.801769	17.031757
31.810020	1256.235450	17.036775
31.635600	1265.561483	17.041792
31.815810	1246.687301	17.046810
31.667270	1242.621949	17.051827
31.583200	1232.371662	17.056845
31.316865	1225.708166	17.061863
31.593242	1230.724992	17.066880
31.515707	1244.046289	17.071898
31.500972	1262.955106	17.076915
32.002661	1253.358190	17.081933
32.311283	1263.079816	17.086951
31.998832	1247.863115	17.091968
31.779112	1231.461418	17.096986
31.541403	1235.938582	17.102003
31.857788	1235.490254	17.107021
32.089300	1253.333900	17.112039
31.643213	1257.608177	17.117056
32.046089	1254.906602	17.122074
31.737770	1259.573413	17.127091
32.078747	1253.425473	17.132109
31.909111	1259.327165	17.137127
31.971949	1262.397121	17.142144
31.917072	1256.053315	17.147162
31.759444	1264.482492	17.152179
31.561356	1260.893046	17.157197
31.786096	1261.898443	17.162215
31.995563	1283.496478	17.167232
32.282971	1279.133345	17.172250
32.134762	1295.288770	17.177267
32.379506	1292.766913	17.182285
32.530212	1285.122938	17.187303
32.467046	1285.279572	17.192320
32.584236	1279.959999	17.197338
32.326465	1278.490623	17.202355
32.771025	1279.581274	17.207373
33.097450	1278.589169	17.212391
32.848812	1284.321673	17.217408
32.740444	1256.050975	17.222426
32.775461	1252.180418	17.227443
32.776654	1247.593432	17.232461
32.955013	1243.319624	17.237479
32.602643	1248.735834	17.242496
32.670947	1237.149713	17.247514
32.415848	1250.120505	17.252531
32.180030	1244.719636	17.257549
32.675242	1265.979394	17.262567
32.888306	1277.664841	17.267584
32.973501	1280.655116	17.272602
32.937729	1280.749341	17.277619
32.821682	1281.965890	17.282637
32.956319	1277.947338	17.287655
32.764871	1288.523421	17.292672
33.086578	1276.189027	17.297690
32.827911	1285.001867	17.302707
32.901295	1284.209531	17.307725
33.349377	1276.140737	17.312743
32.814676	1279.183657	17.317760
32.752235	1279.517726	17.322778
32.993283	1289.609606	17.327795
32.913813	1297.571537	17.332813
33.398590	1303.723148	17.337831
33.078750	1312.770537	17.342848
33.204207	1304.808298	17.347866
33.330781	1305.355947	17.352883
33.062438	1304.599723	17.357901
33.628409	1303.454962	17.362919
33.600157	1311.920614	17.367936
33.763345	1302.580502	17.372954
33.624559	1302.543755	17.377971
33.721785	1295.913335	17.382989
34.064877	1292.624421	17.388007
33.674692	1299.859865	17.393024
33.764168	1301.465211	17.398042
33.907596	1290.822497	17.403059
34.008291	1298.382951	17.408077
34.082450	1292.908691	17.413095
33.585908	1290.734377	17.418112
33.718156	1297.987644	17.423130
33.956654	1299.192730	17.428147
33.948656	1298.650086	17.433165
34.204449	1295.330352	17.438183
34.023341	1296.931289	17.443200
34.000158	1292.297934	17.448218
33.961760	1299.557804	17.453235
33.935873	1293.282803	17.458253
34.213730	1292.238110	17.463271
34.140848	1297.232476	17.468288
34.148193	1288.743750	17.473306
34.148006	1295.492971	17.478323
34.049363	1290.741799	17.483341
33.891495	1303.039462	17.488359
34.174082	1317.783447	17.493376
34.610392	1321.817933	17.498394
34.442564	1320.513578	17.503411
34.230411	1325.796363	17.508429
34.452406	1318.533867	17.513447
34.282181	1322.455403	17.518464
34.156225	1316.686717	17.523482
34.539554	1314.600956	17.528499
34.359260	1324.214211	17.533517
34.624584	1321.437371	17.538535
34.531416	1322.100539	17.543552
34.603178	1318.983710	17.548570
34.500827	1321.763319	17.553587
34.382253	1336.052890	17.558605
34.732529	1349.934925	17.563623
34.627742	1350.985838	17.568640
35.200691	1342.145953	17.573658
35.167671	1345.401480	17.578675
34.988398	1335.614125	17.583693
35.318454	1331.357693	17.588711
35.456286	1333.979426	17.593728
35.464263	1317.519069	17.598746
35.507136	1304.933977	17.603763
35.565313	1310.286560	17.608781
35.434615	1300.543938	17.613799
35.430464	1304.691903	17.618816
35.570106	1306.483033	17.623834
35.329585	1310.112274	17.628851
35.202766	1312.027053	17.633869
35.599239	1308.200566	17.638887
35.150918	1313.614577	17.643904
35.186361	1310.054559	17.648922
35.425704	1303.606899	17.653939
35.212637	1311.867331	17.658957
35.385421	1298.510355	17.663975
35.415794	1292.113048	17.668992
35.300946	1298.205286	17.674010
35.181499	1298.514543	17.679027
35.345956	1305.744370	17.684045
35.411868	1307.666211	17.689063
35.390445	1318.537777	17.694080
35.319423	1335.696193	17.699098
35.675808	1326.935482	17.704115
35.666659	1336.743237	17.709133
35.824713	1336.142781	17.714151
35.573172	1332.239733	17.719168
35.502561	1340.805327	17.724186
35.562588	1341.123056	17.729203
35.388548	1356.561574	17.734221
35.705797	1357.047338	17.739239
35.707297	1361.877442	17.744256
35.947937	1370.363957	17.749274
36.130959	1363.812607	17.754291
36.016736	1365.770187	17.759309
36.078131	1359.232285	17.764327
36.115738	1363.234377	17.769344
36.183743	1365.811379	17.774362
36.524740	1372.717916	17.779379
36.224077	1378.522847	17.784397
36.606287	1369.849568	17.789415
36.697911	1371.071106	17.794432
36.801188	1363.244398	17.799450
36.769808	1349.988898	17.804467
36.455516	1356.996058	17.809485
36.839517	1347.204796	17.814503
36.681882	1348.943188	17.819520
36.759445	1349.472576	17.824538
36.938002	1350.324606	17.829555
36.741872	1355.237037	17.834573
36.563767	1351.009626	17.839591
36.540551	1348.655749	17.844608
36.330040	1347.621841	17.849626
36.410940	1349.470339	17.854643
36.543170	1369.187614	17.859661
37.139677	1373.758178	17.864679
37.464637	1373.085991	17.869696
37.341929	1374.187903	17.874714
37.438618	1350.202306	17.879731
37.052605	1355.886718	17.884749
37.033845	1347.101894	17.889767
36.753509	1347.930697	17.894784
37.090407	1359.773653	17.899802
37.778797	1367.956109	17.904819
37.219110	1353.682589	17.909837
36.969396	1350.833942	17.914855
36.983197	1360.938694	17.919872
36.868171	1374.631266	17.924890
37.161684	1379.202791	17.929907
37.578136	1378.269394	17.934925
37.987773	1376.503674	17.939943
37.462422	1369.502300	17.944960
37.446109	1372.310979	17.949978
37.676094	1375.264699	17.954995
37.647887	1372.504171	17.960013
37.573449	1377.621653	17.965031
37.686657	1369.413775	17.970048
37.450563	1371.432480	17.975066
37.660555	1371.841124	17.980083
37.315414	1372.666092	17.985101
37.655822	1374.410995	17.990119
37.609290	1377.097121	17.995136
37.248782	1368.049980	18.000154
37.910885	1383.224093	18.005171
37.779370	1392.251762	18.010189
37.871107	1396.809458	18.015207
38.272370	1399.124989	18.020224
38.145653	1402.156675	18.025242
38.180243	1389.051634	18.030259
38.533222	1401.082507	18.035277
38.697036	1387.295055	18.040295
38.230667	1377.639461	18.045312
38.186481	1367.845071	18.050330
38.482123	1369.831634	18.055347
38.078646	1383.165683	18.060365
38.334671	1381.735629	18.065383
38.431916	1387.193973	18.070400
38.591275	1387.806667	18.075418
38.907949	1390.128329	18.080435
38.315957	1387.176115	18.085453
38.411990	1387.457175	18.090471
38.771731	1394.664157	18.095488
38.824898	1395.175933	18.100506
39.099669	1384.153539	18.105523
38.788580	1379.287518	18.110541
38.797335	1365.794654	18.115559
38.558012	1361.544699	18.120576
38.474592	1371.663195	18.125594
38.879987	1376.009897	18.130611
38.819682	1392.868574	18.135629
38.804213	1389.936251	18.140647
39.096598	1386.339183	18.145664
39.058230	1389.089706	18.150682
39.406727	1386.871516	18.155699
39.018873	1389.282669	18.160717
38.875497	1379.936186	18.165735
38.622760	1381.663951	18.170752
39.000333	1387.356976	18.175770
39.214283	1385.916959	18.180787
38.994510	1389.346330	18.185805
38.926639	1380.367653	18.190823
39.434095	1400.324014	18.195840
39.478885	1410.977598	18.200858
39.574205	1408.513535	18.205875
39.650675	1407.193524	18.210893
39.793681	1413.458069	18.215911
40.119012	1401.708795	18.220928
39.560030	1394.643688	18.225946
39.537780	1377.118208	18.230963
39.653729	1380.699071	18.235981
39.749743	1380.692342	18.240999
39.862410	1380.956867	18.246016
39.707919	1379.204636	18.251034
39.947286	1396.002280	18.256051
39.970212	1386.861717	18.261069
39.709816	1381.063299	18.266087
40.114765	1374.930703	18.271104
39.930792	1395.530278	18.276122
39.527720	1386.564581	18.281139
39.744646	1400.064418	18.286157
39.741766	1401.967346	18.291175
39.748304	1403.628955	18.296192
39.590259	1409.492171	18.301210
39.859941	1404.906744	18.306227
40.284033	1427.157229	18.311245
40.244545	1429.690625	18.316263
40.253860	1430.651391	18.321280
40.191364	1438.716095	18.326298
40.272535	1429.954441	18.331315
40.493913	1434.796584	18.336333
40.631494	1434.296364	18.341351
40.842066	1433.195482	18.346368
40.671366	1434.320699	18.351386
40.719337	1430.590471	18.356403
40.716179	1431.958022	18.361421
40.675299	1426.079933	18.366439
40.756839	1425.049629	18.371456
40.372286	1427.237015	18.376474
40.712788	1425.659901	18.381491
40.656759	1428.707840	18.386509
40.514694	1429.805481	18.391527
40.802249	1416.314833	18.396544
40.721536	1422.967996	18.401562
40.778441	1416.540655	18.406579
41.061693	1429.337811	18.411597
40.968767	1440.466575	18.416615
41.195327	1450.211751	18.421632
40.986424	1449.282292	18.426650
41.093194	1447.324984	18.431667
41.558243	1452.477963	18.436685
41.409594	1446.652357	18.441703
41.562072	1442.711910	18.446720
41.092558	1448.648761	18.451738
41.568663	1438.962268	18.456755
41.836566	1429.745684	18.461773
41.738043	1435.645117	18.466791
41.825372	1421.379753	18.471808
41.981619	1417.148929	18.476826
41.953547	1409.080169	18.481843
41.910049	1404.299753	18.486861
41.722068	1405.143974	18.491879
41.749988	1395.132512	18.496896
41.750634	1399.663167	18.501914
42.314623	1394.869565	18.506931
42.166124	1399.655622	18.511949
41.944315	1397.874771	18.516967
41.721032	1393.544987	18.521984
41.916412	1398.885512	18.527002
41.684027	1393.682050	18.532019
41.778744	1392.453111	18.537037
41.911552	1395.998510	18.542055
42.309465	1411.056162	18.547072
42.132549	1419.364208	18.552090
42.443557	1419.121883	18.557107
42.311497	1414.304553	18.562125
42.043625	1423.971347	18.567143
42.134598	1420.126916	18.572160
42.113946	1427.278397	18.577178
42.180960	1417.969888	18.582195
42.234860	1422.791728	18.587213
42.120829	1426.045331	18.592231
42.316794	1424.124437	18.597248
42.295513	1437.967289	18.602266
42.103121	1449.001507	18.607283
42.188016	1451.814307	18.612301
42.597775	1456.894948	18.617319
42.701657	1443.056348	18.622336
42.548698	1463.207181	18.627354
42.242301	1455.049051	18.632371
42.946196	1461.769163	18.637389
43.114279	1471.488603	18.642407
43.476666	1467.366938	18.647424
43.262751	1457.767522	18.652442
43.204827	1448.062757	18.657459
43.278315	1444.249167	18.662477
43.001515	1454.052102	18.667495
43.133533	1441.261196	18.672512
43.495032	1441.674677	18.677530
42.887596	1446.795397	18.682547
43.311029	1440.723887	18.687565
43.248174	1442.316282	18.692583
43.364374	1450.303766	18.697600
43.463553	1452.199250	18.702618
43.492435	1473.886508	18.707635
43.638414	1459.709823	18.712653
43.899319	1464.287953	18.717671
43.992048	1453.001167	18.722688
43.763840	1441.464383	18.727706
43.717810	1447.851187	18.732723
43.482419	1437.314798	18.737741
43.502898	1443.997671	18.742759
43.634117	1456.010189	18.747776
43.993556	1464.965270	18.752794
43.545430	1465.267929	18.757811
44.218410	1471.651829	18.762829
43.924837	1475.941462	18.767847
43.442994	1467.073013	18.772864
44.032384	1471.623920	18.777882
43.943043	1461.379077	18.782899
43.945829	1461.072828	18.787917
43.911178	1473.493923	18.792935
44.185924	1476.231198	18.797952
44.172625	1493.601489	18.802970
43.834834	1495.065793	18.807987
44.246207	1491.011994	18.813005
44.423715	1506.537727	18.818023
44.697107	1496.343823	18.823040
44.555607	1494.985487	18.828058
44.749421	1501.747163	18.833075
44.558656	1489.907295	18.838093
44.391296	1499.675209	18.843111
44.780356	1489.259796	18.848128
44.881793	1491.879315	18.853146
44.657140	1498.546501	18.858163
45.029235	1491.837020	18.863181
44.734894	1491.229183	18.868199
45.084055	1487.067971	18.873216
44.844586	1487.809307	18.878234
44.844936	1490.238085	18.883251
44.823131	1491.164244	18.888269
44.826263	1496.074040	18.893287
45.001433	1499.520322	18.898304
45.160122	1509.447639	18.903322
45.324647	1520.098008	18.908339
45.566088	1519.738855	18.913357
45.427296	1515.233630	18.918375
45.586569	1500.363765	18.923392
45.841980	1504.982975	18.928410
45.555775	1499.696656	18.933427
45.916798	1479.797377	18.938445
45.532488	1481.280011	18.943463
45.643770	1461.331557	18.948480
45.871883	1459.486831	18.953498
45.516191	1470.214248	18.958515
45.707276	1470.591380	18.963533
45.424208	1473.626135	18.968551
45.696709	1474.985447	18.973568
45.737237	1486.680725	18.978586
45.614303	1494.493263	18.983603
46.045564	1491.555848	18.988621
45.603162	1519.204234	18.993639
45.553933	1509.077126	18.998656
46.117330	1502.330453	19.003674
45.936789	1498.271907	19.008691
46.087922	1497.968258	19.013709
45.491081	1499.455377	19.018727
45.875042	1513.985522	19.023744
46.115407	1531.517396	19.028762
45.794105	1536.049825	19.033779
45.912392	1531.632342	19.038797
46.220560	1534.427874	19.043815
46.104548	1535.259004	19.048832
46.635886	1531.177458	19.053850
46.588884	1549.239609	19.058867
46.848869	1545.972672	19.063885
46.771070	1535.453035	19.068903
46.790965	1530.905388	19.073920
46.975509	1528.122991	19.078938
46.838128	1523.391153	19.083955
47.146828	1523.788969	19.088973
46.839285	1519.905776	19.093991
47.007925	1529.104690	19.099008
47.097271	1518.164478	19.104026
46.908459	1522.171818	19.109043
46.886869	1525.323916	19.114061
47.220742	1536.361607	19.119079
47.144037	1545.546038	19.124096
47.247475	1549.599482	19.129114
47.376069	1555.391670	19.134131
47.374349	1550.435786	19.139149
47.362621	1558.093723	19.144167
47.553959	1550.757062	19.149184
47.685894	1546.067237	19.154202
47.343365	1543.222110	19.159219
47.345049	1546.817207	19.164237
47.581279	1543.199087	19.169255
47.433815	1542.584251	19.174272
47.800734	1548.827524	19.179290
47.357531	1545.163636	19.184307
47.202811	1540.238995	19.189325
47.333071	1548.927349	19.194343
47.866556	1569.017809	19.199360
47.871283	1562.263614	19.204378
47.845172	1571.945981	19.209395
48.224796	1578.071414	19.214413
47.965484	1573.480616	19.219431
48.031617	1580.176066	19.224448
48.539452	1565.164567	19.229466
48.182588	1581.167831	19.234483
48.416931	1573.395693	19.239501
48.287605	1564.745982	19.244519
48.289568	1574.933936	19.249536
48.722766	1572.579650	19.254554
48.299311	1575.654991	19.259571
48.683945	1566.219392	19.264589
48.741123	1575.962773	19.269607
48.712366	1574.350329	19.274624
48.770614	1568.761678	19.279642
48.435632	1570.419223	19.284659
48.677054	1578.704543	19.289677
48.852645	1563.027587	19.294695
48.603074	1565.037917	19.299712
48.682962	1558.863010	19.304730
48.620117	1566.814453	19.309747
48.797622	1565.454471	19.314765
48.784910	1572.370847	19.319783
48.651793	1565.001288	19.324800
48.794566	1568.122636	19.329818
48.948621	1582.526742	19.334835
48.627247	1585.882426	19.339853
49.140887	1581.209310	19.344871
49.069065	1585.863436	19.349888
48.834251	1569.020966	19.354906
48.697665	1575.835020	19.359923
49.209952	1592.023122	19.364941
49.226546	1604.910246	19.369959
49.453143	1606.327171	19.374976
49.542256	1593.509780	19.379994
49.574672	1601.554916	19.385011
49.837018	1600.456867	19.390029
49.917936	1595.273507	19.395047
49.719863	1594.178466	19.400064
50.196912	1593.300773	19.405082
50.088920	1598.874277	19.410099
50.234498	1591.370764	19.415117
50.271451	1590.311218	19.420135
50.484486	1596.017392	19.425152
50.723190	1590.250428	19.430170
50.036846	1572.691379	19.435187
49.937818	1579.667719	19.440205
50.215226	1586.677009	19.445223
50.345632	1593.872059	19.450240
50.569651	1592.819727	19.455258
50.344007	1600.339876	19.460275
50.512207	1597.457417	19.465293
50.713724	1593.515505	19.470311
50.149206	1591.278385	19.475328
50.660992	1587.826046	19.480346
50.571613	1602.820870	19.485363
50.344683	1606.868796	19.490381
50.495582	1594.173456	19.495399
50.359998	1600.742867	19.500416
50.837364	1592.691110	19.505434
50.902431	1597.815093	19.510451
50.592898	1599.486931	19.515469
50.976434	1607.982594	19.520487
50.972527	1628.021166	19.525504
51.065439	1617.736987	19.530522
50.865969	1620.033518	19.535539
51.228369	1624.525206	19.540557
51.411421	1624.012333	19.545575
51.317346	1626.033932	19.550592
51.505905	1622.915420	19.555610
51.134946	1618.497031	19.560627
50.951639	1624.998370	19.565645
51.312919	1617.159523	19.570663
51.177716	1622.832029	19.575680
51.241191	1623.990926	19.580698
51.091696	1645.579613	19.585715
51.233671	1654.376323	19.590733
51.520110	1655.357359	19.595751
51.759010	1662.049436	19.600768
51.870528	1654.821612	19.605786
51.874192	1657.649082	19.610803
51.633552	1667.801283	19.615821
52.084602	1655.947930	19.620839
51.752736	1658.613239	19.625856
52.031766	1656.473445	19.630874
51.859096	1673.957334	19.635891
52.073896	1686.557376	19.640909
52.242179	1678.452027	19.645927
52.047912	1684.339455	19.650944
52.208506	1677.362157	19.655962
52.501212	1677.457901	19.660979
52.543008	1681.494815	19.665997
52.537103	1667.895453	19.671015
52.697290	1674.607261	19.676032
53.181255	1668.683122	19.681050
52.690934	1674.213659	19.686067
52.955690	1666.921480	19.691085
53.084855	1663.565155	19.696103
52.970346	1673.591357	19.701120
52.855035	1673.352689	19.706138
53.297871	1669.486156	19.711155
53.161406	1663.676560	19.716173
52.766660	1642.685672	19.721191
52.813945	1659.449266	19.726208
53.253801	1662.647821	19.731226
52.947892	1669.662788	19.736243
53.083474	1662.960505	19.741261
53.423612	1668.031879	19.746279
53.021223	1662.765135	19.751296
53.359259	1667.513627	19.756314
53.329595	1670.462366	19.761331
53.518235	1668.180449	19.766349
53.421063	1664.052542	19.771367
53.329816	1677.092623	19.776384
53.294388	1666.137533	19.781402
53.313920	1680.314790	19.786419
53.715483	1688.289006	19.791437
53.679587	1690.158854	19.796455
53.470716	1695.215628	19.801472
53.774759	1688.977963	19.806490
53.704772	1699.775554	19.811507
53.846141	1701.523926	19.816525
53.854634	1680.136690	19.821543
54.072591	1703.900060	19.826560
54.055701	1708.536859	19.831578
54.292731	1714.241860	19.836595
54.385911	1722.048650	19.841613
54.603501	1707.788621	19.846631
54.474684	1707.606913	19.851648
54.439461	1709.413659	19.856666
54.463072	1721.235932	19.861683
54.333625	1713.718449	19.866701
54.636458	1710.911709	19.871719
54.859692	1710.101234	19.876736
54.736967	1713.761457	19.881754
54.598742	1708.704109	19.886771
54.623215	1707.741897	19.891789
55.060049	1707.236608	19.896807
54.922669	1711.739027	19.901824
54.665255	1698.836798	19.906842
54.673859	1700.555971	19.911859
54.823590	1718.969212	19.916877
55.417216	1737.249526	19.921895
55.306088	1748.207508	19.926912
55.257611	1738.848243	19.931930
55.191841	1740.706113	19.936947
55.329483	1743.957876	19.941965
55.431172	1725.162650	19.946983
55.423601	1736.085760	19.952000
55.497314	1738.314633	19.957018
56.013589	1735.737904	19.962035
55.392861	1731.278948	19.967053
55.767278	1727.463494	19.972071
55.695324	1737.732693	19.977088
55.833817	1729.811386	19.982106
55.759875	1730.978083	19.987123
55.685383	1739.991788	19.992141
55.852714	1735.885028	19.997159
55.904905	1726.085476	20.002176
56.023210	1726.752228	20.007194
56.176821	1725.897374	20.012211
55.863146	1739.249141	20.017229
56.214728	1728.584260	20.022247
56.045875	1728.800130	20.027264
55.787848	1726.708699	20.032282
56.182868	1737.271052	20.037299
56.144743	1751.126028	20.042317
56.271148	1754.824933	20.047335
56.563315	1757.343231	20.052352
56.224255	1750.808085	20.057370
56.579444	1750.939547	20.062387
56.497522	1753.994200	20.067405
57.119118	1761.151306	20.072423
57.248110	1762.205663	20.077440
57.002464	1753.787313	20.082458
56.975340	1744.915852	20.087475
56.669948	1745.396457	20.092493
56.841597	1756.111164	20.097511
57.061818	1769.435186	20.102528
56.642094	1777.028894	20.107546
56.991187	1768.862458	20.112563
56.848000	1772.914670	20.117581
56.868834	1769.176650	20.122599
57.315691	1782.189532	20.127616
57.273773	1789.675414	20.132634
57.497631	1784.098241	20.137651
57.371546	1791.889008	20.142669
58.037037	1788.660785	20.147687
57.857697	1784.038965	20.152704
57.934570	1791.047299	20.157722
57.978763	1787.629426	20.162739
58.122911	1788.997421	20.167757
58.064835	1782.064945	20.172775
58.102071	1790.781043	20.177792
57.737120	1789.992756	20.182810
58.214942	1787.339708	20.187827
58.190902	1785.272519	20.192845
58.190375	1783.610103	20.197863
57.963118	1785.269912	20.202880
58.102519	1787.454057	20.207898
57.771518	1780.182121	20.212915
58.022556	1812.497366	20.217933
58.466380	1821.502070	20.222951
58.553004	1809.273503	20.227968
58.705474	1813.020469	20.232986
58.878527	1810.768278	20.238003
58.819233	1810.145131	20.243021
58.576945	1809.707404	20.248039
59.087554	1804.250856	20.253056
58.970683	1817.211438	20.258074
58.977439	1809.935139	20.263091
59.193787	1815.421552	20.268109
59.210833	1811.683755	20.273127
58.984683	1815.807983	20.278144
58.952061	1811.121704	20.283162
59.375991	1803.082624	20.288179
59.331598	1815.592222	20.293197
59.100122	1801.004094	20.298215
59.222466	1803.524534	20.303232
59.046447	1806.303829	20.308250
59.317553	1813.956400	20.313267
59.351427	1832.549591	20.318285
59.308236	1836.223840	20.323303
59.456394	1841.084536	20.328320
59.536836	1843.006006	20.333338
59.690892	1831.915880	20.338355
59.547349	1838.416236	20.343373
59.752461	1849.449487	20.348391
59.619228	1853.401251	20.353408
60.039489	1858.258238	20.358426
60.313893	1852.944329	20.363443
60.167959	1860.197857	20.368461
60.315408	1861.670039	20.373479
60.665498	1851.047449	20.378496
60.487112	1851.670416	20.383514
60.538731	1851.030477	20.388531
60.807925	1861.583829	20.393549
60.676332	1853.484340	20.398567
60.839368	1848.238873	20.403584
60.475980	1847.623948	20.408602
60.890372	1847.664506	20.413619
60.634359	1845.697530	20.418637
60.836390	1848.008717	20.423655
60.962997	1837.378258	20.428672
60.728975	1850.237396	20.433690
60.986063	1845.973223	20.438707
60.885931	1842.497738	20.443725
60.635585	1839.597133	20.448743
60.970004	1846.341585	20.453760
60.908417	1858.119407	20.458778
61.133966	1863.698410	20.463795
61.128855	1874.081830	20.468813
61.334424	1876.454642	20.473831
61.466118	1869.595038	20.478848
61.088347	1868.449807	20.483866
61.290178	1873.616592	20.488883
61.883353	1883.686386	20.493901
61.706665	1895.764795	20.498919
61.918384	1895.516071	20.503936
62.020901	1894.603131	20.508954
61.992165	1897.417898	20.513971
62.234021	1895.190525	20.518989
62.262904	1904.129333	20.524007
62.336419	1892.315084	20.529024
62.516419	1896.444134	20.534042
62.210174	1899.478476	20.539059
62.583247	1897.082916	20.544077
62.484351	1889.819742	20.549095
62.435293	1888.033852	20.554112
62.099762	1893.352218	20.559130
62.487154	1895.727605	20.564147
62.495964	1899.368849	20.569165
62.329683	1901.735516	20.574183
62.781504	1903.742749	20.579200
62.489887	1902.149384	20.584218
62.699212	1894.050121	20.589235
62.913881	1896.030083	20.594253
62.874872	1901.656841	20.599271
62.695464	1898.723613	20.604288
62.756983	1927.085756	20.609306
62.868741	1921.100315	20.614323
62.976429	1915.541148	20.619341
63.045428	1920.772070	20.624359
63.229974	1916.420281	20.629376
63.028659	1934.243071	20.634394
63.432158	1943.465551	20.639411
63.540984	1946.066995	20.644429
63.343456	1949.543198	20.649447
63.644897	1939.939649	20.654464
63.642658	1949.799799	20.659482
63.733668	1935.074682	20.664499
63.888778	1942.161078	20.669517
63.661961	1947.925251	20.674535
64.013047	1933.253139	20.679552
64.139827	1945.319923	20.684570
64.039982	1941.407350	20.689587
64.041911	1933.153031	20.694605
63.977479	1942.225819	20.699623
64.103594	1940.951481	20.704640
63.717695	1960.722228	20.709658
64.400380	1968.148458	20.714675
64.306362	1962.101794	20.719693
64.464770	1972.482615	20.724711
64.996349	1966.210316	20.729728
64.778271	1969.253696	20.734746
64.807708	1963.004696	20.739763
64.916094	1960.852957	20.744781
64.834292	1970.734562	20.749799
65.155216	1959.357655	20.754816
65.088927	1964.226337	20.759834
64.958928	1958.809268	20.764851
65.070083	1958.201988	20.769869
64.812483	1967.240237	20.774887
64.835494	1960.204883	20.779904
64.991153	1967.737667	20.784922
65.387861	1985.660715	20.789939
65.389875	1990.352737	20.794957
65.274309	1993.357100	20.799975
65.930005	1985.566568	20.804992
65.598124	1993.952548	20.810010
65.967373	1983.971594	20.815027
65.932727	1989.682703	20.820045
65.644981	1987.955221	20.825063
66.002755	1983.881431	20.830080
66.371329	1986.722165	20.835098
66.023715	1984.508913	20.840115
66.093908	1992.397994	20.845133
66.023221	1987.987656	20.850151
66.001720	1986.536964	20.855168
66.028735	1992.886699	20.860186
66.061578	2002.522564	20.865203
66.552652	2006.611161	20.870221
66.355612	2009.661301	20.875239
66.566904	2004.646775	20.880256
66.846960	2007.365551	20.885274
66.570323	2003.153485	20.890291
66.715440	1997.007763	20.895309
66.480097	2000.378425	20.900327
66.913007	1990.558190	20.905344
66.768299	1994.352043	20.910362
66.893333	2001.415492	20.915379
67.069898	2001.189910	20.920397
66.935471	2023.843584	20.925415
67.552646	2019.900462	20.930432
67.805120	2022.003712	20.935450
67.296812	2017.417393	20.940467
67.584053	2013.717882	20.945485
67.467427	2017.051568	20.950503
67.694118	2023.145020	20.955520
67.844461	2016.414945	20.960538
67.488637	2016.751541	20.965555
67.789636	2019.627879	20.970573
67.902617	2015.938717	20.975591
68.151385	2015.367313	20.980608
67.869510	2025.465942	20.985626
67.804274	2024.274069	20.990643
68.308910	2026.634002	20.995661
68.107877	2021.701520	21.000679
68.202670	2012.726253	21.005696
68.337650	2015.563936	21.010714
67.764806	2016.604593	21.015731
68.379869	2012.359846	21.020749
68.192503	2016.373372	21.025767
68.136860	2014.677142	21.030784
68.197252	2009.996269	21.035802
68.371870	2037.275293	21.040819
68.424244	2036.769871	21.045837
68.314134	2053.506406	21.050855
68.790886	2045.186009	21.055872
68.825206	2049.396309	21.060890
68.960499	2061.007036	21.065907
69.310061	2065.879339	21.070925
69.039705	2073.507908	21.075943
69.150243	2073.839731	21.080960
69.002153	2070.956797	21.085978
69.475713	2067.792977	21.090995
69.675552	2058.137279	21.096013
69.614353	2062.944123	21.101031
69.530452	2063.885716	21.106048
69.762741	2055.442793	21.111066
69.682362	2064.440337	21.116083
69.894574	2053.255383	21.121101
69.418622	2070.424568	21.126119
69.893424	2058.046886	21.131136
70.041127	2060.422221	21.136154
69.881963	2051.995687	21.141171
70.056380	2058.536404	21.146189
70.102533	2072.241881	21.151207
70.127407	2071.950467	21.156224
70.277818	2072.774522	21.161242
70.355690	2075.090947	21.166259
70.499788	2078.145248	21.171277
70.521163	2083.156150	21.176295
70.723016	2072.044553	21.181312
70.647092	2082.581181	21.186330
70.586612	2092.676268	21.191347
70.733454	2079.137477	21.196365
70.776740	2076.460658	21.201383
70.861393	2091.141303	21.206400
71.350527	2099.465420	21.211418
70.925860	2102.698547	21.216435
71.017692	2111.284915	21.221453
70.901504	2107.894314	21.226471
71.020565	2108.386936	21.231488
71.087123	2103.930612	21.236506
71.005779	2106.417502	21.241523
71.103499	2114.374137	21.246541
71.259807	2119.337511	21.251559
71.667562	2127.880636	21.256576
72.003259	2133.360788	21.261594
71.345237	2134.616743	21.266611
71.568205	2124.676062	21.271629
71.896159	2132.002439	21.276647
72.195121	2138.933606	21.281664
71.972755	2158.662566	21.286682
72.305979	2160.237487	21.291699
72.558051	2154.671653	21.296717
72.266440	2163.566428	21.301735
72.530655	2160.965224	21.306752
72.848870	2153.076151	21.311770
72.698472	2148.264384	21.316787
72.741408	2153.769787	21.321805
72.607382	2150.936480	21.326823
72.354017	2165.977111	21.331840
72.986668	2158.385592	21.336858
72.701794	2166.318984	21.341875
73.064674	2157.082308	21.346893
72.833631	2162.533862	21.351911
72.830775	2159.299295	21.356928
73.029344	2147.107835	21.361946
73.076732	2142.680264	21.366963
73.062875	2145.907982	21.371981
72.975594	2145.590252	21.376999
72.989174	2165.600638	21.382016
73.269925	2177.169651	21.387034
73.134790	2174.420779	21.392051
73.306592	2168.667436	21.397069
73.330600	2192.011289	21.402087
73.749852	2202.592392	21.407104
73.611733	2205.322960	21.412122
73.887527	2213.241106	21.417139
74.203771	2202.285286	21.422157
73.980870	2213.573924	21.427175
74.229563	2202.926151	21.432192
74.505078	2206.168176	21.437210
74.045549	2210.869752	21.442227
74.426612	2198.640949	21.447245
74.280282	2206.157706	21.452263
73.902284	2204.355374	21.457280
74.559483	2220.805195	21.462298
74.739967	2232.509753	21.467315
74.751066	2230.132344	21.472333
74.908782	2237.113321	21.477351
74.804689	2236.757033	21.482368
74.968950	2234.459779	21.487386
74.781770	2230.845856	21.492403
74.919381	2221.732272	21.497421
74.913585	2227.734372	21.502439
74.982533	2253.141038	21.507456
75.248418	2258.220966	21.512474
75.347089	2260.595001	21.517491
75.555900	2249.471496	21.522509
75.766729	2255.060952	21.527527
75.545270	2255.553265	21.532544
75.985772	2244.788269	21.537562
75.926420	2246.157715	21.542579
75.735269	2248.558474	21.547597
76.098153	2244.746381	21.552615
76.073562	2239.685399	21.557632
76.081892	2250.112122	21.562650
76.266442	2263.631855	21.567667
76.681245	2272.675489	21.572685
76.399354	2277.992976	21.577703
76.570844	2278.137932	21.582720
76.504144	2269.911728	21.587738
76.347452	2272.079217	21.592755
76.338647	2272.118192	21.597773
76.312533	2268.087418	21.602791
76.349051	2270.245752	21.607808
76.575627	2267.921640	21.612826
76.619919	2297.842103	21.617843
76.613059	2300.035577	21.622861
76.874258	2293.722874	21.627879
76.831176	2302.328142	21.632896
76.995119	2301.471941	21.637914
77.067209	2316.698604	21.642931
77.059724	2326.215357	21.647949
77.580105	2326.445467	21.652967
77.495227	2323.439810	21.657984
77.732134	2323.004224	21.663002
77.723546	2323.031352	21.668019
77.877430	2317.009649	21.673037
77.678580	2323.739058	21.678055
77.436940	2321.320407	21.683072
78.130974	2318.013729	21.688090
78.013761	2335.300588	21.693107
78.453147	2338.991515	21.698125
78.316269	2343.024325	21.703143
78.102970	2341.669532	21.708160
78.713626	2340.332260	21.713178
78.416543	2341.876122	21.718195
78.499753	2345.039775	21.723213
78.495215	2344.031931	21.728231
78.663312	2343.899484	21.733248
78.999740	2329.798746	21.738266
78.674423	2336.810924	21.743283
78.799534	2336.757251	21.748301
79.019367	2330.942350	21.753319
78.653738	2339.403396	21.758336
79.114526	2350.849419	21.763354
78.808234	2359.649882	21.768371
78.909583	2364.985444	21.773389
79.202397	2363.711033	21.778407
79.223519	2371.658827	21.783424
79.449281	2361.965577	21.788442
79.538577	2368.342951	21.793459
79.681317	2382.077987	21.798477
79.806972	2385.345650	21.803495
79.986156	2397.436394	21.808512
80.315933	2392.778130	21.813530
80.201897	2391.536432	21.818547
80.296295	2393.054852	21.823565
80.513793	2389.506179	21.828583
80.149236	2387.409065	21.833600
80.616192	2381.543385	21.838618
80.562499	2382.626065	21.843635
80.537125	2374.922911	21.848653
80.352479	2373.519274	21.853671
80.457047	2381.950920	21.858688
80.761046	2374.258195	21.863706
80.518127	2387.166101	21.868723
80.951368	2390.292282	21.873741
80.998278	2398.072032	21.878759
80.957273	2407.035694	21.883776
81.166303	2403.562834	21.888794
81.605675	2407.926649	21.893811
81.323229	2410.883128	21.898829
81.489466	2405.919243	21.903847
81.324583	2413.794307	21.908864
81.645624	2406.113706	21.913882
81.568483	2404.774161	21.918899
81.632631	2404.931773	21.923917
81.821901	2408.439709	21.928935
81.662618	2418.033622	21.933952
82.038814	2422.453180	21.938970
82.071368	2434.446178	21.943987
81.981479	2434.563936	21.949005
82.241035	2441.277737	21.954023
82.447341	2435.874901	21.959040
82.375819	2426.341862	21.964058
82.581761	2434.884318	21.969075
82.637724	2432.137225	21.974093
82.686549	2421.709020	21.979111
82.586909	2422.570558	21.984128
82.711723	2420.419580	21.989146
82.403262	2423.567386	21.994163
82.679979	2437.124768	21.999181
83.273681	2431.205800	22.004199
82.893108	2444.116858	22.009216
83.086043	2446.219789	22.014234
83.162128	2449.019269	22.019251
83.052714	2443.004890	22.024269
83.408456	2438.557285	22.029287
83.251884	2443.085534	22.034304
83.608057	2460.626060	22.039322
83.234348	2472.066238	22.044339
83.065447	2471.675791	22.049357
83.616935	2460.838330	22.054375
83.663786	2469.346513	22.059392
83.724952	2468.282898	22.064410
83.737948	2485.035343	22.069427
83.820719	2502.579055	22.074445
84.015609	2500.127077	22.079463
84.272864	2503.315492	22.084480
84.503394	2493.103625	22.089498
84.223833	2497.741234	22.094515
84.642876	2517.612101	22.099533
84.904580	2512.466617	22.104551
84.703467	2521.018246	22.109568
85.120323	2516.777443	22.114586
85.629633	2518.832332	22.119603
85.174613	2511.873121	22.124621
85.302293	2514.948733	22.129639
85.014819	2508.294872	22.134656
85.203988	2517.381915	22.139674
85.373725	2513.181241	22.144691
85.234149	2513.638348	22.149709
85.529826	2508.363612	22.154727
85.173870	2518.409860	22.159744
85.508790	2510.758408	22.164762
85.643552	2514.266337	22.169779
85.470437	2532.375315	22.174797
86.082907	2530.880239	22.179815
85.871686	2540.074928	22.184832
85.787171	2536.194707	22.189850
86.212998	2535.586884	22.194867
85.854646	2537.143664	22.199885
86.090815	2554.107279	22.204903
86.417355	2556.922007	22.209920
86.232622	2566.164298	22.214938
86.569974	2559.933767	22.219955
86.411803	2563.689827	22.224973
86.982438	2560.531493	22.229991
86.819648	2561.399557	22.235008
87.372780	2581.574703	22.240026
87.239448	2577.352139	22.245043
87.624585	2591.204322	22.250061
87.312377	2576.098089	22.255079
87.353292	2578.293929	22.260096
87.430077	2589.284778	22.265114
87.966664	2580.636062	22.270131
87.631706	2583.095723	22.275149
87.693395	2579.966530	22.280167
87.821883	2589.794416	22.285184
87.920241	2580.535931	22.290202
87.950148	2575.174853	22.295219
87.782253	2586.965708	22.300237
87.965905	2569.020122	22.305255
88.107730	2575.860173	22.310272
87.897376	2585.332716	22.315290
88.142376	2602.314607	22.320307
88.300605	2604.711907	22.325325
88.222858	2603.329135	22.330343
88.524111	2611.298392	22.335360
88.337638	2610.737216	22.340378
88.368988	2621.367083	22.345395
88.417864	2638.290141	22.350413
88.915812	2635.570234	22.355431
89.097933	2639.717244	22.360448
89.254842	2632.633824	22.365466
89.143558	2642.202210	22.370483
89.002617	2635.156686	22.375501
89.048761	2632.620647	22.380519
89.644009	2654.369334	22.385536
89.400709	2663.369393	22.390554
89.686228	2662.972604	22.395571
89.931189	2668.217560	22.400589
89.882432	2654.163375	22.405607
89.979836	2655.282872	22.410624
90.125259	2662.733037	22.415642
90.219241	2656.600248	22.420659
89.863394	2656.262008	22.425677
90.008946	2651.079015	22.430695
90.076102	2663.267654	22.435712
90.260958	2680.493463	22.440730
90.649375	2682.051427	22.445747
90.247953	2684.112631	22.450765
90.356653	2678.960141	22.455783
90.670979	2693.276927	22.460800
90.781329	2711.137590	22.465818
91.129013	2697.238216	22.470835
91.075972	2708.807771	22.475853
91.347431	2702.291616	22.480871
91.595133	2693.183940	22.485888
91.443072	2688.632140	22.490906
91.816783	2689.514540	22.495923
91.571084	2695.448660	22.500941
91.998502	2689.582326	22.505959
91.798427	2689.531309	22.510976
91.871094	2694.326814	22.515994
92.344553	2689.819489	22.521011
91.988460	2699.733976	22.526029
91.977496	2689.009564	22.531047
92.176370	2687.231354	22.536064
92.041038	2698.153062	22.541082
92.404321	2699.211217	22.546099
92.048910	2710.323320	22.551117
92.223092	2714.386225	22.556135
92.237238	2712.177541	22.561152
92.478472	2737.745856	22.566170
92.861239	2741.812425	22.571187
92.845574	2751.924143	22.576205
92.994819	2746.892092	22.581223
93.304129	2743.941963	22.586240
93.085108	2748.996425	22.591258
93.140634	2741.494277	22.596275
93.680323	2753.366150	22.601293
93.729785	2760.473956	22.606311
93.932602	2762.930833	22.611328
93.958460	2770.084681	22.616346
93.967125	2761.190965	22.621363
93.814219	2765.571838	22.626381
93.893024	2760.749885	22.631399
94.209817	2768.788309	22.636416
93.995528	2761.887559	22.641434
94.556447	2759.456834	22.646451
94.349342	2764.950306	22.651469
94.673097	2757.340744	22.656487
94.669231	2758.822710	22.661504
94.222849	2761.062246	22.666522
94.562109	2756.109764	22.671539
94.552621	2773.126890	22.676557
95.013156	2784.385074	22.681575
95.053715	2793.822105	22.686592
94.817923	2791.754012	22.691610
94.970947	2782.591876	22.696627
95.000814	2793.239036	22.701645
95.015202	2791.300793	22.706663
95.390442	2794.024426	22.711680
95.144053	2809.606687	22.716698
95.464591	2808.467032	22.721715
95.840867	2813.450514	22.726733
95.356528	2814.833676	22.731751
95.825807	2810.295511	22.736768
95.864206	2817.902063	22.741786
95.643061	2824.893667	22.746803
96.024236	2835.530332	22.751821
96.252140	2831.553425	22.756839
96.465007	2840.154412	22.761856
96.042254	2854.741821	22.766874
96.664710	2838.495069	22.771891
96.734898	2843.859974	22.776909
96.980167	2851.206290	22.781927
97.360774	2854.416091	22.786944
96.955451	2857.261490	22.791962
97.175317	2853.983996	22.796979
97.122669	2857.939995	22.801997
97.006614	2852.724258	22.807015
97.747789	2849.552595	22.812032
97.646199	2858.137933	22.817050
97.673613	2851.453051	22.822067
97.504962	2854.490385	22.827085
97.434766	2850.909314	22.832103
97.719433	2855.012629	22.837120
97.666774	2869.510034	22.842138
97.985665	2874.380192	22.847155
97.934472	2885.381415	22.852173
97.674944	2886.422219	22.857191
97.950034	2884.305357	22.862208
98.137154	2915.974765	22.867226
98.274973	2916.780084	22.872243
98.093326	2909.208059	22.877261
98.499068	2916.755809	22.882279
98.890721	2926.195426	22.887296
98.569304	2937.448136	22.892314
99.039256	2937.325949	22.897331
98.980730	2936.793188	22.902349
98.908664	2943.697951	22.907367
99.234131	2950.091585	22.912384
99.550170	2962.796780	22.917402
99.680791	2959.520260	22.922419
99.576142	2959.982227	22.927437
99.863889	2964.207120	22.932455
100.307278	2965.111075	22.937472
100.096687	2964.713341	22.942490
100.331098	2960.454198	22.947507
100.421747	2961.929197	22.952525
100.291205	2971.004866	22.957543
100.404597	2963.217023	22.962560
100.265421	2961.774304	22.967578
100.580133	2955.762739	22.972595
100.476833	2963.110122	22.977613
100.456420	2964.149927	22.982631
100.753491	2982.953695	22.987648
100.692815	2984.082852	22.992666
101.041180	2989.593499	22.997683
101.017367	2989.723551	23.002701
100.946586	3001.697870	23.007719
101.396802	2989.710175	23.012736
101.285824	3001.354112	23.017754
101.435291	3010.348401	23.022771
101.740589	3015.414572	23.027789
101.647762	3011.675385	23.032807
102.105084	3012.523882	23.037824
101.952357	3014.069893	23.042842
101.854392	3011.739164	23.047859
102.012609	3007.155979	23.052877
102.085069	3007.489009	23.057895
102.319472	3006.115549	23.062912
102.181198	3006.492525	23.067930
102.144868	3031.329256	23.072947
102.615511	3026.667958	23.077965
102.231151	3030.581667	23.082983
102.592596	3023.614221	23.088000
102.529310	3043.047855	23.093018
102.643941	3056.347549	23.098035
102.863394	3064.869609	23.103053
102.801736	3067.803828	23.108071
103.137001	3056.811190	23.113088
103.184032	3074.943802	23.118106
103.374337	3080.428678	23.123123
103.504090	3085.328249	23.128141
103.660298	3088.097255	23.133159
103.944096	3076.789471	23.138176
103.847310	3079.527127	23.143194
104.093208	3079.556614	23.148211
104.185328	3085.186107	23.153229
104.244746	3103.366312	23.158247
104.561012	3108.407074	23.163264
104.437869	3108.820134	23.168282
104.232661	3112.538045	23.173299
104.252096	3102.475309	23.178317
104.242877	3116.214497	23.183335
104.511474	3129.693900	23.188352
104.649333	3134.751609	23.193370
105.216866	3132.559522	23.198387
105.560366	3128.391732	23.203405
105.478525	3142.290619	23.208423
105.360136	3137.413001	23.213440
105.443024	3145.069440	23.218458
105.694439	3157.794550	23.223475
105.980091	3163.616461	23.228493
106.142246	3164.715431	23.233511
106.050983	3159.080878	23.238528
105.832925	3158.823759	23.243546
106.279856	3152.311047	23.248563
106.143042	3159.242375	23.253581
106.053831	3154.326847	23.258599
106.479327	3169.448190	23.263616
106.373953	3186.151293	23.268634
106.508108	3186.936759	23.273651
107.293116	3185.508740	23.278669
106.716638	3184.838079	23.283687
106.490402	3178.790783	23.288704
107.158586	3191.071289	23.293722
107.364708	3196.039362	23.298739
107.303605	3202.595145	23.303757
107.468455	3204.395712	23.308775
107.781836	3206.322885	23.313792
107.736189	3206.204560	23.318810
107.765353	3204.366586	23.323827
107.697706	3206.484416	23.328845
107.594931	3209.362471	23.333863
107.819323	3213.919608	23.338880
108.138114	3227.742791	23.343898
107.920844	3228.679365	23.348915
108.480422	3236.482933	23.353933
108.503217	3242.380680	23.358951
108.473833	3235.643220	23.363968
108.616975	3240.037027	23.368986
108.537340	3257.926228	23.374003
108.885914	3260.592936	23.379021
108.607787	3270.492511	23.384039
108.615377	3258.922813	23.389056
108.760847	3263.936386	23.394074
109.440324	3286.229554	23.399091
109.587333	3286.040744	23.404109
109.518293	3291.705262	23.409127
109.589485	3293.644982	23.414144
109.677478	3285.118191	23.419162
109.794150	3283.692144	23.424179
110.054685	3278.143806	23.429197
109.743383	3284.882007	23.434215
109.969296	3299.099411	23.439232
110.694971	3296.374766	23.444250
110.397847	3302.840126	23.449267
110.673452	3305.237002	23.454285
110.817857	3307.561496	23.459303
110.728055	3298.753469	23.464320
111.066690	3299.262933	23.469338
111.115500	3297.162220	23.474355
111.493581	3295.476333	23.479373
111.108130	3300.852258	23.484391
111.535755	3305.750619	23.489408
111.793279	3312.901797	23.494426
111.495183	3321.792788	23.499443
111.867237	3324.296941	23.504461
112.075907	3319.832097	23.509479
112.317047	3311.461452	23.514496
112.224489	3310.975654	23.519514
111.955815	3316.431475	23.524531
112.286977	3311.202965	23.529549
112.355698	3324.542775	23.534567
112.639450	3313.326966	23.539584
112.430113	3311.643834	23.544602
112.232930	3314.351691	23.549619
112.691554	3338.468310	23.554637
112.589447	3338.256171	23.559655
112.800547	3349.567089	23.564672
112.975696	3339.278792	23.569690
112.257319	3352.481195	23.574707
112.711892	3358.494527	23.579725
112.825470	3380.258619	23.584743
113.113114	3396.317677	23.589760
113.710287	3395.825175	23.594778
113.497841	3408.419391	23.599795
113.902018	3396.547290	23.604813
114.007797	3408.121385	23.609831
114.179630	3416.414488	23.614848
114.429827	3425.584488	23.619866
114.194007	3435.317301	23.624883
114.353025	3428.582033	23.629901
114.627270	3428.745035	23.634919
114.659599	3424.026647	23.639936
114.629059	3430.041182	23.644954
114.679538	3443.114397	23.649971
114.989247	3446.956215	23.654989
114.960464	3442.334170	23.660007
115.184725	3444.712794	23.665024
115.398067	3456.779414	23.670042
115.380729	3473.409974	23.675059
115.752357	3477.848313	23.680077
115.571964	3480.626655	23.685095
115.630459	3481.873142	23.690112
115.732728	3482.501284	23.695130
115.894446	3486.666861	23.700147
116.151426	3494.493097	23.705165
116.292121	3504.996788	23.710183
116.491290	3501.699750	23.715200
116.718771	3496.970293	23.720218
116.609854	3499.257614	23.725235
116.730353	3501.130528	23.730253
116.856057	3507.397210	23.735271
116.612208	3502.497725	23.740288
117.366499	3494.735021	23.745306
117.044364	3516.272190	23.750323
116.960816	3522.542023	23.755341
117.609544	3526.248982	23.760359
117.430674	3526.876028	23.765376
117.836927	3520.006076	23.770394
117.343643	3521.290370	23.775411
117.548953	3528.466042	23.780429
118.147382	3546.826454	23.785447
118.267981	3549.984950	23.790464
118.305505	3548.399915	23.795482
118.304214	3553.954480	23.800499
118.400839	3557.554797	23.805517
118.269081	3552.025638	23.810535
118.370101	3572.090288	23.815552
118.680319	3576.448260	23.820570
119.038644	3590.527851	23.825587
119.070419	3579.792208	23.830605
118.876417	3583.089817	23.835623
119.206410	3591.934853	23.840640
119.615038	3596.303313	23.845658
119.527334	3604.084690	23.850675
119.665037	3598.872365	23.855693
119.874263	3602.509963	23.860711
119.648579	3600.862581	23.865728
119.902691	3613.043059	23.870746
119.960738	3627.411012	23.875763
120.050828	3623.369704	23.880781
120.079379	3626.289880	23.885799
120.341968	3637.110924	23.890816
120.974540	3646.816645	23.895834
120.322198	3657.994326	23.900851
120.588835	3656.940714	23.905869
121.006930	3647.608580	23.910887
121.178785	3659.229410	23.915904
121.645258	3671.333037	23.920922
121.338689	3675.971918	23.925939
121.636849	3678.830535	23.930957
121.864058	3678.988334	23.935975
121.654623	3678.873103	23.940992
121.919273	3676.846067	23.946010
121.885070	3680.433816	23.951027
122.018051	3674.404422	23.956045
122.145532	3688.990100	23.961063
122.230154	3691.481658	23.966080
122.617467	3701.681229	23.971098
122.492308	3705.448238	23.976115
122.589218	3695.859762	23.981133
122.457213	3692.614364	23.986151
123.183513	3717.094000	23.991168
123.346813	3714.568709	23.996186
123.008278	3724.574252	24.001203
123.128008	3723.153566	24.006221
123.334218	3730.252400	24.011239
123.102177	3733.923316	24.016256
123.628480	3741.027042	24.021274
123.784572	3742.406231	24.026291
124.027544	3743.724572	24.031309
124.068049	3739.698532	24.036327
124.155522	3750.151742	24.041344
124.437857	3747.651232	24.046362
124.435487	3773.978212	24.051379
124.576135	3782.969289	24.056397
124.681634	3782.858223	24.061415
124.893404	3780.577687	24.066432
125.011185	3772.383936	24.071450
125.102461	3781.381610	24.076467
124.966890	3782.739789	24.081485
125.335315	3762.717078	24.086503
125.101521	3768.561821	24.091520
125.439611	3791.950176	24.096538
125.424998	3799.986909	24.101555
125.437203	3797.692160	24.106573
125.542863	3799.570324	24.111591
125.754066	3817.288372	24.116608
125.977054	3823.531594	24.121626
125.893940	3832.647553	24.126643
126.452450	3831.156576	24.131661
126.414424	3831.764646	24.136679
126.374147	3849.499954	24.141696
127.035500	3855.983650	24.146714
127.012058	3864.158905	24.151731
127.184010	3858.896329	24.156749
127.471597	3852.113607	24.161767
127.285343	3853.705412	24.166784
127.360011	3850.070596	24.171802
127.435750	3858.690124	24.176819
127.227865	3871.844667	24.181837
127.310458	3876.615661	24.186855
127.601130	3872.655665	24.191872
127.860513	3890.265412	24.196890
127.966877	3910.696594	24.201907
128.158606	3909.282084	24.206925
128.476807	3910.183989	24.211943
127.879921	3916.081419	24.216960
128.606737	3932.160460	24.221978
128.538636	3934.475342	24.226995
128.597651	3939.567236	24.232013
128.781699	3941.020566	24.237031
129.095931	3962.769572	24.242048
129.156881	3957.911620	24.247066
129.513426	3969.300104	24.252083
129.317597	3966.736971	24.257101
129.335559	3983.311432	24.262119
129.612442	3997.218232	24.267136
130.016024	3990.291424	24.272154
129.952994	3998.957630	24.277171
129.659579	4009.798532	24.282189
130.525381	4004.462379	24.287207
130.457182	4010.911784	24.292224
130.703050	4009.930890	24.297242
130.939093	4010.280174	24.302259
130.733087	4029.991455	24.307277
130.859539	4030.356521	24.312295
131.034642	4042.654762	24.317312
131.200751	4035.724724	24.322330
131.259067	4035.178092	24.327347
131.213520	4041.916718	24.332365
132.036505	4048.832075	24.337383
131.828347	4054.098969	24.342400
132.270315	4053.614035	24.347418
132.312347	4061.472206	24.352435
132.179900	4061.117024	24.357453
132.884668	4054.807358	24.362471
132.683497	4053.153899	24.367488
132.492151	4068.034485	24.372506
132.710508	4071.898277	24.377523
132.810109	4084.079897	24.382541
132.630890	4090.794998	24.387559
132.892783	4084.358611	24.392576
133.121988	4089.808265	24.397594
133.335139	4100.604739	24.402611
133.150654	4114.339168	24.407629
133.828242	4107.589816	24.412647
133.646587	4114.164362	24.417664
133.939728	4105.203491	24.422682
134.165369	4107.284698	24.427699
134.131186	4112.594472	24.432717
134.367772	4110.372390	24.437735
134.258956	4138.169018	24.442752
134.330602	4130.505638	24.447770
134.594452	4136.578808	24.452787
134.256398	4145.821422	24.457805
134.684462	4152.697468	24.462823
134.555723	4159.162469	24.467840
134.821463	4157.906578	24.472858
135.162938	4176.038182	24.477875
134.899732	4194.526653	24.482893
135.658713	4189.031718	24.487911
135.467413	4202.720888	24.492928
135.574642	4212.599387	24.497946
136.057429	4214.719940	24.502963
136.019577	4223.513619	24.507981
136.341458	4220.297708	24.512999
136.574239	4235.809927	24.518016
136.502633	4238.645207	24.523034
136.835917	4247.023852	24.528051
136.904500	4237.303098	24.533069
137.629105	4233.664545	24.538087
137.464506	4239.592117	24.543104
137.503057	4238.849504	24.548122
137.572581	4233.764025	24.553139
137.575869	4234.614132	24.558157
138.062805	4239.866812	24.563175
137.954665	4258.821108	24.568192
138.217275	4258.328062	24.573210
138.299157	4258.763515	24.578227
138.194372	4266.891019	24.583245
138.232550	4253.635316	24.588263
138.467789	4258.568983	24.593280
138.395106	4278.825528	24.598298
138.560550	4281.367984	24.603315
138.295566	4292.972221	24.608333
138.826138	4299.901452	24.613351
138.774412	4314.882800	24.618368
138.865873	4329.036379	24.623386
139.575024	4336.224300	24.628403
139.384367	4360.099537	24.633421
139.856939	4348.843068	24.638439
139.824716	4348.470498	24.643456
139.831609	4342.740906	24.648474
140.483267	4352.033210	24.653491
140.530576	4374.866533	24.658509
140.902180	4365.709027	24.663527
140.595517	4370.117376	24.668544
140.557845	4373.534567	24.673562
140.904215	4372.303901	24.678579
140.838465	4381.258220	24.683597
141.153281	4385.411687	24.688615
141.294173	4395.969102	24.693632
141.384084	4401.308832	24.698650
141.699327	4402.742849	24.703667
141.559443	4397.056439	24.708685
141.670205	4404.936480	24.713703
141.861308	4421.242538	24.718720
142.024895	4410.653827	24.723738
142.028565	4411.243991	24.728755
142.198630	4434.384695	24.733773
142.768539	4441.702825	24.738791
142.502331	4439.521411	24.743808
142.665729	4451.868377	24.748826
143.002716	4440.139712	24.753843
142.534247	4456.190370	24.758861
143.131329	4467.161374	24.763879
143.299012	4482.108919	24.768896
143.252066	4477.085171	24.773914
143.227938	4481.991757	24.778931
143.206438	4499.344304	24.783949
143.672547	4502.204016	24.788967
143.940836	4510.985761	24.793984
144.149037	4519.891654	24.799002
144.326453	4531.896929	24.804019
144.546141	4537.755479	24.809037
144.417631	4528.709816	24.814055
144.723593	4547.724272	24.819072
145.004399	4563.382437	24.824090
145.208213	4558.521124	24.829107
144.973099	4565.207877	24.834125
145.323589	4552.007324	24.839143
145.625048	4559.025794	24.844160
145.815579	4575.087966	24.849178
146.013701	4572.472900	24.854195
145.964012	4582.929685	24.859213
146.384708	4584.425803	24.864231
146.360383	4578.782412	24.869248
146.471225	4592.607761	24.874266
146.849035	4605.809285	24.879283
146.682226	4606.777354	24.884301
146.663263	4611.672887	24.889319
146.966722	4605.613733	24.894336
146.876048	4619.470892	24.899354
147.633414	4626.074479	24.904371
147.480115	4635.443514	24.909389
147.425387	4631.521218	24.914407
147.622148	4630.811461	24.919424
147.578581	4654.162695	24.924442
147.783811	4657.847668	24.929459
147.760102	4665.787118	24.934477
148.129672	4675.366521	24.939495
148.538770	4689.499340	24.944512
148.482462	4694.351465	24.949530
148.769596	4686.714356	24.954547
148.662155	4717.040624	24.959565
148.963921	4715.468429	24.964583
149.153389	4715.920737	24.969600
149.286479	4720.127219	24.974618
149.532332	4724.952955	24.979635
149.813329	4738.739237	24.984653
149.830396	4741.203162	24.989671
149.927386	4738.055883	24.994688
150.137936	4743.734884	24.999706
150.507981	4758.345979	25.004723
150.494169	4767.239940	25.009741
150.563878	4770.495316	25.014759
150.844495	4770.823852	25.019776
150.667961	4775.195017	25.024794
150.933039	4794.761534	25.029811
151.154629	4796.634802	25.034829
151.294761	4798.786964	25.039847
151.387432	4795.167063	25.044864
151.749707	4804.486283	25.049882
152.203302	4817.410818	25.054899
152.007792	4827.083079	25.059917
152.002635	4826.850928	25.064935
152.512854	4824.167613	25.069952
152.149096	4822.055848	25.074970
152.600390	4815.339726	25.079987
152.855883	4830.291180	25.085005
153.083811	4835.644436	25.090023
153.232188	4835.355364	25.095040
153.396846	4837.676736	25.100058
153.733811	4838.295219	25.105075
153.366559	4843.387096	25.110093
153.304762	4842.038104	25.115111
153.547814	4838.515370	25.120128
153.612960	4860.809327	25.125146
153.812154	4859.932982	25.130163
153.743323	4860.309922	25.135181
153.994218	4870.266647	25.140199
153.946541	4885.966915	25.145216
154.094036	4896.905544	25.150234
154.472969	4907.475088	25.155251
154.521780	4912.567411	25.160269
154.971388	4920.059260	25.165287
154.776424	4931.930386	25.170304
154.907500	4950.200103	25.175322
155.311036	4949.497054	25.180339
155.561832	4962.000855	25.185357
155.495133	4980.679808	25.190375
156.161600	4974.645475	25.195392
155.933502	4981.046141	25.200410
156.492279	4998.604023	25.205427
156.483848	5005.725977	25.210445
156.781506	5003.857520	25.215463
157.024399	5000.104806	25.220480
157.010560	5021.959213	25.225498
157.465804	5027.143378	25.230515
157.672564	5037.621014	25.235533
157.489851	5027.097884	25.240551
157.724795	5037.303866	25.245568
157.711668	5028.409716	25.250586
158.187253	5041.060658	25.255603
158.131877	5051.196577	25.260621
158.180822	5050.505761	25.265639
158.358138	5050.562366	25.270656
158.416233	5064.402375	25.275674
158.781622	5073.813387	25.280691
158.962901	5080.150257	25.285709
158.889247	5081.609343	25.290727
159.034631	5084.107997	25.295744
159.274965	5105.932255	25.300762
159.368841	5118.838622	25.305779
159.538554	5113.985935	25.310797
159.676574	5125.091683	25.315815
159.744758	5130.665232	25.320832
159.915429	5147.811836	25.325850
159.996398	5140.713479	25.330867
160.385179	5160.947529	25.335885
160.673771	5166.286918	25.340903
160.901523	5160.757528	25.345920
160.925185	5176.680974	25.350938
161.262476	5181.454698	25.355955
161.463980	5187.300751	25.360973
161.554344	5190.215710	25.365991
162.083947	5186.601355	25.371008
162.044804	5191.761886	25.376026
162.029617	5187.743121	25.381043
162.418676	5207.723585	25.386061
162.236695	5221.127777	25.391079
162.390827	5215.320725	25.396096
162.654924	5221.089483	25.401114
162.345078	5229.621595	25.406131
162.671665	5239.770795	25.411149
162.795914	5248.135754	25.416167
163.096490	5244.895602	25.421184
163.240268	5265.147507	25.426202
163.188345	5263.189616	25.431219
163.471490	5276.628690	25.436237
163.219574	5280.019327	25.441255
163.533457	5286.608408	25.446272
163.955313	5302.844101	25.451290
164.253382	5303.245370	25.456307
164.538857	5317.145619	25.461325
164.403245	5329.204901	25.466343
164.803817	5324.412380	25.471360
164.635335	5334.587682	25.476378
165.122051	5346.995239	25.481395
165.507817	5353.948916	25.486413
165.249253	5362.942014	25.491431
165.814838	5353.482470	25.496448
165.428069	5365.294313	25.501466
166.035850	5376.291754	25.506483
166.123665	5376.052866	25.511501
165.965227	5380.900057	25.516519
166.486345	5395.427667	25.521536
166.428055	5402.317051	25.526554
166.718575	5419.267689	25.531571
167.063338	5409.547747	25.536589
166.801826	5422.046155	25.541607
167.196954	5427.265609	25.546624
167.337628	5437.070821	25.551642
167.595520	5446.669186	25.556659
167.903257	5460.347712	25.561677
168.140156	5468.093991	25.566695
168.708013	5460.631351	25.571712
168.522456	5462.533512	25.576730
168.602702	5458.609930	25.581747
168.887811	5467.333509	25.586765
169.124936	5482.396524	25.591783
169.168950	5484.236266	25.596800
169.285185	5493.903004	25.601818
169.300869	5486.819238	25.606835
169.835721	5503.207341	25.611853
169.610045	5513.887626	25.616871
169.918833	5510.027008	25.621888
170.090240	5519.854750	25.626906
169.914325	5518.951471	25.631923
170.312126	5530.340564	25.636941
170.253102	5553.975287	25.641959
170.364928	5542.246853	25.646976
170.505183	5557.956058	25.651994
170.506779	5574.930279	25.657011
171.139349	5584.610044	25.662029
171.057179	5598.963632	25.667047
171.121867	5600.428216	25.672064
171.330966	5623.023124	25.677082
171.502165	5633.487355	25.682100
171.612946	5638.817750	25.687117
171.720485	5663.736422	25.692135
172.364169	5667.114343	25.697152
172.317709	5681.760596	25.702170
172.821113	5697.793384	25.707188
172.856465	5699.677116	25.712205
173.171979	5709.883587	25.717223
173.361242	5704.945572	25.722240
173.523009	5709.283829	25.727258
173.594099	5710.143268	25.732276
173.941482	5702.855635	25.737293
174.299442	5721.341507	25.742311
174.186440	5726.890129	25.747328
174.229252	5739.167494	25.752346
174.302945	5737.201350	25.757364
174.655979	5743.528957	25.762381
174.403315	5751.059494	25.767399
174.818175	5762.144277	25.772416
174.999173	5763.669958	25.777434
174.984569	5773.282130	25.782452
175.643453	5793.054057	25.787469
175.491925	5805.284098	25.792487
175.527687	5800.166687	25.797504
175.933805	5819.077101	25.802522
175.928528	5830.351990	25.807540
176.466690	5831.706709	25.812557
175.983201	5842.616560	25.817575
176.336894	5855.131604	25.822592
176.689247	5860.424445	25.827610
176.413762	5880.191279	25.832628
176.835327	5889.580880	25.837645
176.982932	5895.917353	25.842663
177.335475	5913.687616	25.847680
177.785770	5910.501307	25.852698
177.508315	5918.732280	25.857716
178.187157	5938.433352	25.862733
178.389305	5946.685758	25.867751
178.560868	5951.982568	25.872768
179.027733	5949.061298	25.877786
179.022722	5974.451974	25.882804
179.105843	5976.549940	25.887821
179.235787	5972.635332	25.892839
179.684221	5969.085438	25.897856
179.813765	5967.054886	25.902874
179.717830	5984.389883	25.907892
180.330442	5986.552205	25.912909
180.215580	5996.508761	25.917927
180.462361	6004.944413	25.922944
180.135939	6006.156371	25.927962
179.881947	6018.557913	25.932980
180.368063	6032.260965	25.937997
180.618155	6048.443163	25.943015
180.835168	6053.801794	25.948032
180.865799	6076.561580	25.953050
181.223445	6091.876957	25.958068
182.027709	6099.933674	25.963085
181.779290	6119.682148	25.968103
181.927710	6130.215853	25.973120
182.314892	6122.799357	25.978138
181.995454	6132.410228	25.983156
182.167191	6148.935517	25.988173
183.088659	6166.400796	25.993191
183.269712	6171.366880	25.998208
183.505708	6172.856717	26.003226
183.603527	6177.896442	26.008244
184.215787	6165.776739	26.013261
183.884805	6178.195088	26.018279
184.203066	6183.952084	26.023296
184.304374	6197.267671	26.028314
184.128005	6198.784032	26.033332
184.517692	6205.130175	26.038349
184.678619	6215.064840	26.043367
184.795411	6229.169462	26.048384
185.120978	6216.202430	26.053402
185.140300	6225.786419	26.058420
185.420374	6247.765568	26.063437
185.648170	6254.344892	26.068455
185.521079	6262.881957	26.073472
185.835042	6261.754974	26.078490
185.768144	6286.623954	26.083508
185.971547	6281.024169	26.088525
186.349184	6297.817193	26.093543
186.560234	6305.361015	26.098560
186.804197	6306.113893	26.103578
186.840019	6321.649749	26.108596
187.178864	6334.519707	26.113613
187.277859	6337.461805	26.118631
187.568325	6340.669935	26.123648
187.500762	6352.186285	26.128666
187.850995	6365.353686	26.133684
188.056408	6364.370688	26.138701
187.625497	6386.347221	26.143719
188.412405	6393.785516	26.148736
188.706738	6393.689646	26.153754
188.871059	6413.326838	26.158772
189.205508	6426.960037	26.163789
188.909974	6428.732440	26.168807
189.264592	6439.887535	26.173824
189.466609	6453.784488	26.178842
189.557674	6457.736107	26.183860
189.809005	6481.157004	26.188877
190.034142	6486.827921	26.193895
190.143587	6492.447104	26.198912
190.672675	6512.246937	26.203930
190.664346	6526.710438	26.208948
190.992392	6520.694535	26.213965
191.192762	6535.016375	26.218983
191.559143	6551.172748	26.224000
191.571339	6544.110353	26.229018
191.702542	6553.620883	26.234036
191.818326	6570.377992	26.239053
191.966548	6574.365075	26.244071
191.869697	6588.771610	26.249088
192.464349	6600.184027	26.254106
192.302277	6616.880851	26.259124
192.793282	6622.435340	26.264141
192.912162	6636.258786	26.269159
192.988917	6642.269385	26.274176
193.755212	6657.522387	26.279194
193.572825	6678.990315	26.284212
193.700836	6673.394997	26.289229
194.036964	6691.042828	26.294247
193.878596	6697.019119	26.299264
194.428157	6704.963935	26.304282
194.447632	6724.687716	26.309300
195.065359	6722.373824	26.314317
195.532156	6718.029919	26.319335
195.301896	6735.763686	26.324352
195.512951	6734.223646	26.329370
195.748839	6748.349185	26.334388
195.860945	6746.112691	26.339405
196.018221	6770.052900	26.344423
196.245370	6781.304166	26.349440
196.422235	6783.064568	26.354458
196.476394	6799.220896	26.359476
196.643204	6811.269835	26.364493
196.955614	6812.686435	26.369511
197.041017	6839.104030	26.374528
197.761072	6839.403981	26.379546
197.756611	6840.188559	26.384564
197.816767	6849.173054	26.389581
198.408918	6863.610708	26.394599
198.139710	6874.455070	26.399616
198.470163	6861.143283	26.404634
198.431472	6885.550898	26.409652
198.971575	6898.594368	26.414669
199.067089	6898.046207	26.419687
199.103496	6904.243173	26.424704
199.272605	6914.248601	26.429722
199.381519	6927.861281	26.434740
199.367352	6932.661429	26.439757
199.973676	6951.801564	26.444775
199.622424	6969.675347	26.449792
200.118826	6962.936683	26.454810
200.516943	6984.649198	26.459828
200.403595	6984.792529	26.464845
200.338259	6996.757162	26.469863
200.561345	7024.705562	26.474880
201.060272	7032.973996	26.479898
201.177332	7047.328994	26.484916
201.316978	7057.621377	26.489933
201.766848	7073.046891	26.494951
201.766193	7082.745766	26.499968
202.211036	7087.120247	26.504986
202.336803	7102.326907	26.510004
202.555083	7111.074275	26.515021
203.236188	7122.078922	26.520039
202.939585	7129.421249	26.525056
202.903622	7142.195588	26.530074
203.488039	7158.166041	26.535092
203.652973	7162.058347	26.540109
203.932440	7166.019914	26.545127
203.979120	7196.065479	26.550144
204.203313	7200.963306	26.555162
204.522293	7200.426191	26.560180
204.699025	7221.548685	26.565197
204.968509	7226.757247	26.570215
205.074529	7234.708803	26.575232
205.478737	7248.328800	26.580250
205.631807	7246.265048	26.585268
205.707906	7263.330354	26.590285
205.716283	7275.619335	26.595303
205.950092	7289.566109	26.600320
206.403018	7299.583085	26.605338
206.439508	7304.062248	26.610356
207.070864	7317.706142	26.615373
207.651360	7326.396818	26.620391
207.455469	7341.816068	26.625408
207.763290	7330.910088	26.630426
208.133952	7338.722578	26.635444
207.631947	7365.899947	26.640461
208.230206	7362.679409	26.645479
208.342685	7367.390194	26.650496
208.700542	7377.213433	26.655514
208.593244	7399.456016	26.660532
209.010984	7393.065752	26.665549
209.406160	7397.407583	26.670567
209.493963	7419.560395	26.675584
209.733245	7417.405944	26.680602
209.605489	7421.816231	26.685620
209.910323	7442.888668	26.690637
210.350963	7440.739478	26.695655
209.877876	7460.155801	26.700672
210.446815	7476.159071	26.705690
210.854975	7496.258211	26.710708
210.539552	7513.905328	26.715725
211.136990	7515.614308	26.720743
211.478965	7547.116154	26.725760
212.343263	7542.146961	26.730778
212.193166	7537.321274	26.735796
211.990831	7548.615038	26.740813
212.520941	7555.804164	26.745831
212.471532	7557.831331	26.750848
212.628747	7563.060164	26.755866
213.206035	7579.036162	26.760884
212.981447	7593.564789	26.765901
213.484429	7597.182261	26.770919
213.425577	7608.411355	26.775936
213.846552	7624.901650	26.780954
213.913176	7621.065651	26.785972
213.958164	7633.255111	26.790989
214.289841	7651.965786	26.796007
214.346817	7659.236432	26.801024
214.679495	7675.154557	26.806042
214.592536	7683.810196	26.811060
214.686297	7695.025902	26.816077
215.378244	7711.539961	26.821095
215.067250	7720.070440	26.826112
215.483954	7733.944003	26.831130
215.956450	7755.518440	26.836148
215.679311	7762.539599	26.841165
216.685715	7777.343543	26.846183
216.493451	7793.476294	26.851200
216.865499	7808.790949	26.856218
217.020768	7810.433735	26.861236
216.958240	7838.241006	26.866253
217.303076	7840.532998	26.871271
217.906262	7854.794073	26.876288
218.159854	7867.995265	26.881306
218.361512	7873.237325	26.886324
218.277239	7885.638215	26.891341
218.638821	7892.882176	26.896359
218.703600	7908.599114	26.901376
218.927636	7929.243661	26.906394
219.230739	7930.305858	26.911412
219.565053	7953.493841	26.916429
219.715296	7959.883482	26.921447
219.975818	7974.079292	26.926464
220.146217	7988.546831	26.931482
220.164198	7996.817403	26.936500
220.749528	8009.105968	26.941517
220.859517	8018.560233	26.946535
221.129373	8029.946318	26.951552
221.733396	8038.013556	26.956570
221.708968	8041.602644	26.961588
221.711880	8060.419424	26.966605
222.181570	8072.230916	26.971623
222.109477	8087.718616	26.976640
222.147473	8092.632576	26.981658
222.670477	8105.372660	26.986676
222.624708	8113.051234	26.991693
222.806628	8123.152193	26.996711
223.119275	8144.073022	27.001728
223.289488	8164.414056	27.006746
223.661750	8172.407871	27.011764
224.031615	8206.854879	27.016781
224.280102	8202.592406	27.021799
224.545527	8216.073936	27.026816
224.892613	8225.512707	27.031834
224.969135	8224.399692	27.036852
224.809264	8241.705979	27.041869
225.398815	8256.879506	27.046887
225.224495	8271.342922	27.051904
225.599263	8296.133261	27.056922
226.006630	8300.734853	27.061940
226.069605	8320.147766	27.066957
226.170116	8330.244214	27.071975
226.322855	8342.435285	27.076992
226.714009	8355.487284	27.082010
227.268379	8378.334603	27.087028
227.190031	8398.349993	27.092045
227.253297	8395.619566	27.097063
227.431955	8406.999748	27.102080
228.006070	8432.968847	27.107098
228.416575	8445.114176	27.112116
228.479670	8458.601833	27.117133
228.732447	8466.681746	27.122151
229.306229	8479.916306	27.127168
229.698137	8478.750278	27.132186
229.724377	8477.063426	27.137204
229.729002	8480.996773	27.142221
229.985669	8486.855399	27.147239
229.844769	8498.072703	27.152256
230.346887	8510.417183	27.157274
230.849319	8522.449673	27.162292
230.985358	8538.884102	27.167309
231.029043	8531.991281	27.172327
231.122128	8542.970584	27.177344
231.644804	8553.217072	27.182362
231.873493	8556.787219	27.187380
231.621114	8572.532104	27.192397
232.031791	8582.036972	27.197415
231.992036	8601.664958	27.202432
232.054745	8624.677519	27.207450
232.607609	8642.333393	27.212468
232.446651	8652.339410	27.217485
232.971603	8672.072516	27.222503
233.138386	8682.624568	27.227520
233.382335	8712.867206	27.232538
233.488207	8718.677619	27.237556
233.547845	8749.854393	27.242573
233.865982	8759.936359	27.247591
234.503143	8777.074262	27.252608
234.535833	8806.790375	27.257626
235.486344	8815.487584	27.262644
235.719841	8829.654757	27.267661
235.964771	8840.064783	27.272679
236.013967	8848.761535	27.277696
236.267205	8860.629137	27.282714
236.681071	8866.755718	27.287732
236.793360	8876.731610	27.292749
237.133592	8885.583448	27.297767
237.158135	8902.269885	27.302784
237.072540	8913.149825	27.307802
237.771627	8918.190936	27.312820
238.049571	8937.315352	27.317837
238.208481	8949.750072	27.322855
238.580837	8954.780683	27.327872
238.913728	8968.695983	27.332890
239.053635	8974.652894	27.337908
238.763553	8993.405833	27.342925
238.956961	9000.811272	27.347943
239.401877	9013.207364	27.352960
239.931675	9030.260115	27.357978
240.487302	9038.344543	27.362996
240.678660	9049.977532	27.368013
240.504771	9055.943878	27.373031
240.723693	9063.956435	27.378048
241.195314	9089.362981	27.383066
240.890560	9087.727704	27.388084
241.325237	9108.305033	27.393101
241.563727	9123.856550	27.398119
242.029077	9135.467880	27.403136
242.006576	9149.858114	27.408154
242.334547	9154.801602	27.413172
242.354612	9189.284998	27.418189
242.494206	9194.603941	27.423207
243.157703	9216.896344	27.428224
243.233333	9235.021824	27.433242
243.280325	9255.520929	27.438260
243.531623	9267.472660	27.443277
243.610447	9282.833333	27.448295
244.019350	9302.253984	27.453312
244.037924	9315.377110	27.458330
244.767695	9342.920342	27.463348
245.008738	9351.420174	27.468365
244.998074	9355.376749	27.473383
245.468219	9371.229696	27.478400
245.451214	9384.474573	27.483418
245.839050	9389.376713	27.488436
246.343052	9416.179108	27.493453
246.203089	9419.892404	27.498471
246.353626	9434.331452	27.503488
246.600731	9455.515366	27.508506
246.884455	9469.896161	27.513524
247.378208	9484.620344	27.518541
247.982562	9509.091743	27.523559
248.340111	9509.457294	27.528576
248.175157	9513.524529	27.533594
248.574930	9520.461187	27.538612
248.670232	9535.757926	27.543629
248.798724	9545.935592	27.548647
248.934510	9561.819654	27.553664
249.280408	9573.937148	27.558682
249.513950	9582.160251	27.563700
249.614304	9611.031586	27.568717
249.987153	9619.982423	27.573735
250.637311	9630.132088	27.578752
250.726469	9655.379107	27.583770
250.674906	9657.620389	27.588788
251.131229	9679.596372	27.593805
251.247417	9698.044963	27.598823
251.564207	9710.538436	27.603840
251.916534	9728.085326	27.608858
252.218940	9747.851087	27.613876
252.240564	9762.581200	27.618893
252.319198	9772.170892	27.623911
252.759630	9791.098476	27.628928
252.857511	9815.261063	27.633946
253.210600	9835.008300	27.638964
253.735490	9850.309071	27.643981
253.799002	9874.832740	27.648999
253.998198	9872.857133	27.654016
254.688773	9899.842951	27.659034
254.676180	9904.647669	27.664052
255.157292	9927.388008	27.669069
255.274652	9936.244233	27.674087
255.606003	9942.810310	27.679104
255.800123	9965.926729	27.684122
256.196996	9977.763506	27.689140
256.627843	9992.713645	27.694157
256.664741	10009.041516	27.699175
257.034975	10013.041558	27.704192
257.015341	10024.522679	27.709210
257.077251	10034.398124	27.714228
257.402433	10042.015429	27.719245
257.536914	10075.211816	27.724263
257.751589	10088.257418	27.729280
257.908349	10122.813938	27.734298
258.489383	10121.544802	27.739316
258.798815	10152.551384	27.744333
258.930464	10167.535455	27.749351
259.396253	10179.832095	27.754368
259.771436	10195.495956	27.759386
259.750599	10216.781162	27.764404
260.476111	10227.421371	27.769421
260.631209	10234.812452	27.774439
260.858599	10252.063101	27.779456
260.923389	10269.068880	27.784474
261.269288	10274.358760	27.789492
261.251996	10291.708253	27.794509
261.139601	10318.596855	27.799527
261.797859	10331.384875	27.804544
262.053011	10352.704935	27.809562
262.107056	10363.006527	27.814580
262.758401	10382.445081	27.819597
262.903592	10392.079274	27.824615
263.240168	10413.096800	27.829632
263.497035	10418.732358	27.834650
263.879733	10435.474549	27.839668
263.948746	10455.661916	27.844685
263.948644	10474.102284	27.849703
264.164317	10483.733532	27.854720
264.542735	10509.517012	27.859738
264.816852	10515.037087	27.864756
265.087510	10536.812562	27.869773
265.307200	10544.828098	27.874791
265.631820	10574.392795	27.879808
265.857187	10583.864928	27.884826
266.063632	10599.660322	27.889844
266.735539	10614.784646	27.894861
266.609489	10627.718485	27.899879
266.894576	10645.834519	27.904896
267.396011	10664.017182	27.909914
267.592221	10692.130068	27.914932
267.528936	10704.301966	27.919949
267.915506	10724.610433	27.924967
268.209131	10743.520897	27.929984
268.366912	10768.087046	27.935002
268.606355	10780.979418	27.940020
269.536335	10804.642551	27.945037
269.427330	10831.495203	27.950055
269.645253	10837.888186	27.955072
269.751982	10858.558287	27.960090
270.345198	10888.060191	27.965108
270.772249	10900.838090	27.970125
271.089051	10920.234976	27.975143
271.267347	10933.517341	27.980160
271.395625	10954.421934	27.985178
271.714867	10962.942767	27.990196
272.336021	10986.041175	27.995213
272.104723	10996.892275	28.000231
272.609039	11020.950787	28.005248
272.846999	11030.512492	28.010266
273.162863	11049.102910	28.015284
273.613858	11057.061505	28.020301
274.056240	11082.539075	28.025319
274.276818	11089.229534	28.030336
274.560878	11100.301093	28.035354
274.845144	11117.606283	28.040372
275.410402	11133.626442	28.045389
275.178904	11159.141617	28.050407
275.612638	11154.309591	28.055424
276.062968	11177.811579	28.060442
275.581730	11183.119703	28.065460
275.926463	11198.524066	28.070477
276.725540	11219.291179	28.075495
276.742290	11239.656783	28.080512
276.889744	11246.838442	28.085530
277.178222	11287.620394	28.090548
277.381209	11297.823080	28.095565
277.471577	11321.740983	28.100583
278.090469	11336.646277	28.105600
278.192682	11360.976705	28.110618
278.510742	11377.212935	28.115636
279.407911	11384.587290	28.120653
279.303081	11411.170754	28.125671
279.493323	11415.625616	28.130688
279.942298	11438.322985	28.135706
280.036216	11444.732008	28.140724
280.049818	11469.707578	28.145741
280.315032	11488.757560	28.150759
280.844976	11510.420521	28.155776
281.148899	11516.478078	28.160794
281.348038	11542.095910	28.165812
281.799430	11546.134120	28.170829
281.675428	11558.184343	28.175847
282.251467	11569.398565	28.180864
282.418007	11585.823967	28.185882
282.345328	11603.921506	28.190900
282.953458	11625.105244	28.195917
283.303515	11640.926735	28.200935
283.318322	11657.374173	28.205952
283.914871	11673.599271	28.210970
284.019452	11693.868966	28.215988
284.223718	11708.372069	28.221005
284.586722	11733.477733	28.226023
284.878327	11750.066970	28.231040
285.504561	11763.469698	28.236058
285.467648	11793.625941	28.241076
285.648912	11803.870362	28.246093
285.972216	11828.628186	28.251111
286.675087	11853.794391	28.256128
287.127645	11843.156881	28.261146
287.632236	11863.037533	28.266164
288.250635	11868.212713	28.271181
288.270693	11874.786986	28.276199
288.818806	11888.918173	28.281216
289.169334	11900.852286	28.286234
288.801660	11911.241214	28.291252
289.217456	11909.377640	28.296269
289.568446	11930.193051	28.301287
289.529362	11935.858431	28.306304
289.657497	11956.045763	28.311322
290.130428	11973.142573	28.316340
290.274872	11990.331594	28.321357
290.381382	12014.868726	28.326375
290.732400	12036.443821	28.331392
290.706257	12051.877295	28.336410
290.993305	12073.790802	28.341428
291.691280	12089.805704	28.346445
291.681614	12123.057731	28.351463
291.914519	12138.884919	28.356480
292.250364	12163.020294	28.361498
292.528220	12191.842434	28.366516
292.990687	12213.629392	28.371533
293.285925	12247.887029	28.376551
293.411703	12263.667460	28.381568
294.030729	12296.343022	28.386586
294.095539	12313.662179	28.391604
294.539391	12333.805602	28.396621
294.929794	12359.421433	28.401639
295.068276	12379.424778	28.406656
295.534362	12400.689775	28.411674
295.729781	12418.721783	28.416692
296.245164	12436.820616	28.421709
296.737484	12450.272872	28.426727
296.767719	12472.242033	28.431744
297.151561	12487.371676	28.436762
297.398286	12513.882995	28.441780
297.754753	12536.803659	28.446797
297.721664	12553.021972	28.451815
298.158733	12562.384584	28.456832
298.564810	12579.910711	28.461850
298.867581	12605.005632	28.466868
299.361637	12624.621063	28.471885
299.651464	12628.777692	28.476903
299.964806	12650.791636	28.481920
300.343273	12664.496148	28.486938
300.331828	12674.421590	28.491956
300.614127	12696.054639	28.496973
300.978748	12709.826093	28.501991
300.880294	12726.892202	28.507008
301.261073	12744.761515	28.512026
301.427940	12769.822452	28.517044
301.466318	12785.364134	28.522061
301.646597	12811.338519	28.527079
301.984411	12842.739537	28.532096
302.308646	12857.676099	28.537114
302.651408	12898.825030	28.542132
303.302218	12916.607287	28.547149
303.483752	12941.002597	28.552167
303.855909	12956.777589	28.557184
304.016015	12980.591836	28.562202
304.212311	13006.092678	28.567220
304.907662	13026.647626	28.572237
305.227501	13064.059504	28.577255
305.515872	13077.144175	28.582272
306.169778	13100.629442	28.587290
306.549631	13126.785624	28.592308
306.751926	13130.908017	28.597325
307.271722	13152.592191	28.602343
307.499303	13171.410834	28.607360
307.750060	13181.619407	28.612378
307.670535	13206.882546	28.617396
308.334943	13218.620690	28.622413
308.419478	13234.960472	28.627431
308.690779	13266.573462	28.632448
308.999991	13285.930310	28.637466
309.025640	13310.383493	28.642484
309.756433	13322.615033	28.647501
309.870162	13354.757006	28.652519
310.007157	13381.984477	28.657536
310.683069	13398.978276	28.662554
310.630067	13424.927636	28.667572
311.171099	13446.228877	28.672589
311.496124	13466.700688	28.677607
311.740209	13494.533132	28.682624
312.288495	13512.033575	28.687642
312.543851	13541.630907	28.692660
312.871340	13570.667910	28.697677
313.259613	13589.840251	28.702695
313.678561	13601.335623	28.707712
313.983227	13619.292566	28.712730
314.026398	13644.980502	28.717748
314.558823	13666.567135	28.722765
314.944848	13673.023248	28.727783
315.049344	13692.975518	28.732800
315.546713	13708.443685	28.737818
315.497202	13731.017162	28.742836
316.018004	13759.683665	28.747853
316.381734	13776.614483	28.752871
316.218356	13802.940463	28.757888
316.856167	13824.374326	28.762906
317.260923	13855.949032	28.767924
317.666639	13879.044676	28.772941
318.073456	13906.382809	28.777959
317.842913	13928.450676	28.782976
318.596373	13943.760053	28.787994
318.789336	13969.868144	28.793012
319.209729	13994.684116	28.798029
319.528586	14010.795190	28.803047
319.629581	14044.519807	28.808064
320.313846	14066.483726	28.813082
320.349852	14086.266568	28.818100
320.528390	14105.493142	28.823117
321.196248	14126.293589	28.828135
321.295625	14140.756333	28.833152
321.779760	14146.126265	28.838170
321.942544	14167.190031	28.843188
322.151167	14190.014560	28.848205
322.665912	14198.191108	28.853223
322.671619	14222.046904	28.858240
323.379264	14231.598952	28.863258
323.563609	14274.287425	28.868276
323.516135	14288.183585	28.873293
324.277153	14312.839642	28.878311
324.153218	14346.458688	28.883328
324.369848	14360.350597	28.888346
324.996209	14392.953503	28.893364
325.100706	14424.731882	28.898381
325.609096	14437.759164	28.903399
325.739187	14463.173944	28.908416
326.132312	14479.353568	28.913434
326.517508	14513.295313	28.918452
326.765061	14545.010846	28.923469
327.301403	14575.416199	28.928487
327.598095	14601.022693	28.933504
328.038901	14625.445375	28.938522
328.120024	14649.845668	28.943540
328.429432	14682.217914	28.948557
328.925905	14703.737793	28.953575
329.066603	14735.441433	28.958592
329.451493	14753.570748	28.963610
330.160883	14779.046169	28.968628
330.073592	14808.398315	28.973645
330.493321	14830.752214	28.978663
330.884051	14855.207168	28.983680
331.722740	14880.401289	28.988698
331.732320	14899.029466	28.993716
332.215210	14927.092758	28.998733
332.520665	14945.344184	29.003751
332.743456	14975.948756	29.008768
333.376643	14996.981437	29.013786
333.494571	15029.178011	29.018804
333.538401	15039.827060	29.023821
334.172194	15067.131140	29.028839
334.673546	15100.128111	29.033856
334.767253	15112.655583	29.038874
335.306673	15140.035298	29.043892
335.603624	15158.726535	29.048909
335.855518	15182.130029	29.053927
336.137694	15206.759511	29.058944
336.532036	15239.178690	29.063962
336.534650	15259.260057	29.068980
336.774043	15289.949154	29.073997
337.499903	15306.329860	29.079015
337.515446	15342.752319	29.084032
337.688950	15359.574405	29.089050
338.430759	15403.696113	29.094068
338.372844	15425.581373	29.099085
338.948198	15453.469492	29.104103
339.411780	15484.949334	29.109120
339.766095	15504.249328	29.114138
340.008349	15540.511759	29.119156
340.411795	15570.649360	29.124173
340.837709	15593.096268	29.129191
340.764218	15623.729015	29.134208
341.414774	15649.633216	29.139226
341.936878	15676.453993	29.144244
341.950009	15706.312834	29.149261
343.002169	15722.435047	29.154279
343.240166	15749.186327	29.159296
343.483250	15763.279950	29.164314
343.973044	15798.822640	29.169332
343.873094	15805.984209	29.174349
344.179000	15820.713727	29.179367
344.614880	15853.147731	29.184384
344.962923	15863.601952	29.189402
345.275650	15883.330120	29.194420
345.244728	15903.759859	29.199437
345.875717	15923.246256	29.204455
346.242660	15955.375052	29.209472
346.411628	15976.209984	29.214490
346.803507	16008.568038	29.219508
346.751176	16033.487400	29.224525
347.625312	16059.716199	29.229543
347.609423	16083.877747	29.234560
348.052567	16116.979388	29.239578
348.698673	16145.837386	29.244596
348.507669	16178.843926	29.249613
349.095588	16202.281523	29.254631
349.705896	16221.346112	29.259648
350.038031	16255.760497	29.264666
350.636569	16276.371815	29.269684
350.893134	16306.788847	29.274701
351.201187	16329.625108	29.279719
351.555243	16350.474014	29.284736
351.840997	16382.982771	29.289754
352.327496	16407.107354	29.294772
352.380828	16442.496687	29.299789
353.042812	16453.392693	29.304807
353.338696	16485.887365	29.309824
353.520359	16510.339974	29.314842
353.877151	16537.112275	29.319860
354.391457	16572.297914	29.324877
354.671504	16586.950430	29.329895
354.702108	16613.335484	29.334912
355.043460	16648.174754	29.339930
355.740322	16682.903242	29.344948
355.918315	16720.425739	29.349965
356.235965	16738.317741	29.354983
356.449995	16775.859620	29.360000
356.833402	16807.196049	29.365018
357.435974	16831.796998	29.370036
357.799184	16869.621778	29.375053
358.407648	16892.967108	29.380071
358.604076	16929.713062	29.385088
359.319953	16949.869167	29.390106
359.643057	16968.450938	29.395124
360.012603	17004.031886	29.400141
360.476285	17017.566735	29.405159
360.679067	17045.648469	29.410176
361.144693	17070.455293	29.415194
361.205515	17079.168699	29.420212
361.547050	17107.044720	29.425229
361.965465	17126.564570	29.430247
362.427035	17158.959054	29.435264
362.232788	17186.157786	29.440282
362.904992	17212.614155	29.445300
363.193880	17255.259933	29.450317
363.711877	17277.232025	29.455335
363.942208	17314.050461	29.460352
364.301422	17339.906228	29.465370
365.030683	17360.583966	29.470388
365.050225	17391.915515	29.475405
365.512270	17418.813694	29.480423
365.804328	17446.761528	29.485440
366.523595	17482.432224	29.490458
366.841340	17500.052323	29.495476
366.986270	17534.185075	29.500493
367.258591	17550.354609	29.505511
367.772857	17573.847329	29.510528
367.950275	17608.589639	29.515546
368.749644	17626.407604	29.520564
368.535471	17651.841704	29.525581
369.162314	17670.400792	29.530599
369.624269	17699.370800	29.535616
369.646520	17720.210139	29.540634
370.075719	17749.936014	29.545652
370.345352	17775.137322	29.550669
370.875085	17807.953722	29.555687
371.011634	17836.263719	29.560704
371.459931	17874.434548	29.565722
371.746006	17893.416007	29.570740
372.069329	17925.440768	29.575757
372.834065	17957.589585	29.580775
372.941312	17988.450584	29.585792
373.171482	18037.194595	29.590810
373.965738	18057.369031	29.595828
373.919979	18088.454165	29.600845
374.594394	18115.149648	29.605863
375.038692	18142.783396	29.610880
375.103581	18184.477059	29.615898
375.859385	18198.874127	29.620916
376.163515	18231.881614	29.625933
376.858625	18256.305416	29.630951
377.186388	18282.098492	29.635968
377.118894	18319.441372	29.640986
377.916099	18337.411800	29.646004
378.072155	18381.698300	29.651021
378.412422	18402.446448	29.656039
378.551073	18426.782880	29.661056
378.691905	18472.413698	29.666074
379.089520	18505.306938	29.671092
379.443543	18546.587916	29.676109
380.091297	18585.761522	29.681127
380.337486	18620.633289	29.686144
380.751504	18651.042743	29.691162
381.474673	18674.195035	29.696180
382.247699	18716.534266	29.701197
382.227342	18741.397215	29.706215
382.894756	18763.099038	29.711232
383.379296	18802.156705	29.716250
384.060597	18825.188441	29.721268
384.043330	18850.159818	29.726285
384.366484	18872.736957	29.731303
384.874003	18906.055792	29.736320
385.057181	18937.214971	29.741338
385.609403	18957.916120	29.746356
385.907957	18994.447936	29.751373
386.494244	19017.531922	29.756391
386.947978	19040.344648	29.761408
387.113627	19069.471704	29.766426
387.687534	19097.262153	29.771444
388.028562	19127.911574	29.776461
388.363330	19154.308643	29.781479
389.028711	19177.371878	29.786496
389.222562	19204.667317	29.791514
389.718186	19225.523206	29.796532
389.885157	19251.054309	29.801549
390.198943	19278.099846	29.806567
390.781014	19302.961673	29.811584
390.824707	19341.798749	29.816602
391.625665	19359.139049	29.821620
391.834943	19384.469440	29.826637
391.733247	19425.864270	29.831655
392.235827	19456.638905	29.836672
392.558583	19492.303856	29.841690
392.867459	19516.891175	29.846708
393.521950	19553.928135	29.851725
393.706754	19587.751055	29.856743
394.106282	19605.342505	29.861760
394.553900	19640.331258	29.866778
395.191509	19665.414611	29.871796
395.257219	19703.006546	29.876813
395.943252	19730.126792	29.881831
396.451585	19755.718836	29.886848
396.647880	19779.166390	29.891866
397.442268	19807.142252	29.896884
397.516709	19834.221991	29.901901
397.670651	19858.740858	29.906919
398.223315	19891.617472	29.911936
398.599507	19920.941345	29.916954
398.864246	19951.076740	29.921972
399.371684	19982.832178	29.926989
399.497039	20016.161290	29.932007
400.069256	20050.573740	29.937024
400.070050	20083.966168	29.942042
400.940106	20119.210790	29.947060
401.193624	20156.928742	29.952077
401.389344	20198.668829	29.957095
402.020500	20230.695935	29.962112
402.251011	20269.408063	29.967130
402.792833	20294.134552	29.972148
403.079114	20338.130336	29.977165
403.517839	20378.804269	29.982183
404.152865	20406.738135	29.987200
404.687223	20443.421703	29.992218
405.040308	20470.237198	29.997236
405.434003	20505.337583	30.002253
405.805812	20547.240167	30.007271
406.351617	20575.856002	30.012288
406.258799	20610.017027	30.017306
407.018535	20655.422071	30.022324
407.656912	20682.613235	30.027341
407.615534	20728.300838	30.032359
408.320806	20768.368731	30.037376
408.501891	20799.706722	30.042394
409.062114	20834.928442	30.047412
409.413411	20876.929840	30.052429
409.603224	20911.979673	30.057447
410.406469	20941.491651	30.062464
410.551340	20986.485344	30.067482
410.896690	21020.246734	30.072500
411.626157	21049.719081	30.077517
411.907496	21095.638074	30.082535
412.449255	21130.734179	30.087552
412.800664	21168.742499	30.092570
413.428872	21197.158126	30.097588
414.078088	21224.581726	30.102605
414.178955	21262.440938	30.107623
414.393886	21292.995346	30.112640
414.659584	21332.263826	30.117658
415.363178	21363.257809	30.122676
415.466140	21405.295313	30.127693
415.943780	21454.001983	30.132711
416.497619	21486.632396	30.137728
417.145417	21522.295159	30.142746
417.443554	21559.873266	30.147764
418.074820	21586.557780	30.152781
418.025163	21627.214635	30.157799
418.884091	21653.744901	30.162816
418.845075	21700.965763	30.167834
419.301449	21728.865166	30.172852
419.660639	21772.843163	30.177869
420.130769	21819.686819	30.182887
420.309334	21855.664454	30.187904
420.716835	21893.392340	30.192922
420.987370	21933.337849	30.197940
421.442026	21961.933278	30.202957
421.874254	22012.210082	30.207975
422.387097	22043.079203	30.212992
422.758834	22087.390219	30.218010
423.333665	22117.650036	30.223028
424.467625	22150.277182	30.228045
424.378568	22181.444840	30.233063
425.019719	22204.699156	30.238080
425.471811	22244.705231	30.243098
425.749863	22275.033366	30.248116
426.489516	22310.264736	30.253133
426.762599	22343.170326	30.258151
427.083317	22365.577531	30.263168
427.912262	22388.078839	30.268186
428.398635	22424.889762	30.273204
429.117758	22450.023700	30.278221
429.277979	22488.407217	30.283239
429.992150	22499.319062	30.288256
429.910855	22531.345449	30.293274
430.577963	22553.651428	30.298292
430.890854	22586.011624	30.303309
430.962508	22624.372260	30.308327
431.439220	22659.058132	30.313344
431.838738	22688.154311	30.318362
432.239073	22727.998215	30.323380
432.599364	22764.281995	30.328397
433.036268	22800.810201	30.333415
433.376393	22838.410999	30.338432
433.521545	22870.711191	30.343450
433.803984	22917.741896	30.348468
434.177594	22961.974464	30.353485
434.459044	23012.263412	30.358503
435.199160	23059.958326	30.363520
435.659999	23107.209179	30.368538
436.093208	23157.657937	30.373556
436.038263	23202.327888	30.378573
436.738376	23249.285658	30.383591
437.356492	23296.331242	30.388608
437.979461	23344.495757	30.393626
438.331723	23387.053555	30.398644
438.989066	23431.718192	30.403661
439.652054	23479.020200	30.408679
440.074156	23513.718428	30.413696
440.700350	23546.785526	30.418714
441.059683	23599.731477	30.423732
441.666150	23632.015117	30.428749
441.991270	23677.839232	30.433767
442.403938	23715.015224	30.438784
442.991615	23745.895557	30.443802
443.574347	23778.836258	30.448820
443.968556	23814.425958	30.453837
444.340655	23847.562497	30.458855
445.059502	23880.572333	30.463872
445.456421	23909.185327	30.468890
445.490539	23946.105920	30.473908
446.169686	23979.832152	30.478925
446.719381	24017.304674	30.483943
446.924170	24053.547544	30.488960
447.101906	24091.469717	30.493978
447.542575	24140.412557	30.498996
448.058182	24171.535827	30.504013
448.037100	24211.396163	30.509031
449.005010	24254.578080	30.514048
449.592252	24301.973753	30.519066
449.805618	24342.804875	30.524084
450.310353	24378.746478	30.529101
450.702795	24430.940448	30.534119
451.291304	24469.076188	30.539136
451.596518	24491.078732	30.544154
451.891804	24533.398068	30.549172
452.341632	24553.143704	30.554189
452.436094	24596.758045	30.559207
453.148554	24636.305583	30.564224
453.811331	24671.552988	30.569242
454.093323	24723.315095	30.574260
454.696836	24749.920861	30.579277
454.991134	24796.464315	30.584295
455.396039	24841.939279	30.589312
456.229714	24877.950506	30.594330
456.525166	24921.311623	30.599348
457.066721	24951.835893	30.604365
457.396027	24992.807081	30.609383
457.927178	25024.556999	30.614400
458.662521	25054.721355	30.619418
458.678166	25107.812427	30.624436
459.338468	25148.603048	30.629453
459.786435	25188.299716	30.634471
460.255950	25230.349069	30.639488
460.443503	25272.438875	30.644506
460.637783	25322.715918	30.649524
461.277358	25360.403606	30.654541
461.757002	25415.879110	30.659559
462.309069	25461.028558	30.664576
463.164703	25507.932099	30.669594
463.272292	25547.490361	30.674612
463.709204	25589.410356	30.679629
464.165480	25644.824226	30.684647
464.571708	25692.168529	30.689664
465.087826	25737.463438	30.694682
465.437179	25788.359645	30.699700
465.995832	25821.951731	30.704717
466.535045	25874.292972	30.709735
467.086963	25916.497543	30.714752
467.668287	25967.210795	30.719770
468.032092	26015.238025	30.724788
468.329930	26056.456679	30.729805
469.451695	26096.375146	30.734823
469.826111	26141.435911	30.739840
470.359363	26183.331945	30.744858
470.561357	26223.219956	30.749876
471.610235	26261.081617	30.754893
471.855541	26298.798752	30.759911
472.575028	26340.298444	30.764928
473.031733	26371.448068	30.769946
473.229234	26413.835524	30.774964
473.598378	26447.239383	30.779981
474.231569	26490.684200	30.784999
474.698756	26535.367887	30.790016
474.895394	26571.872917	30.795034
475.281202	26619.513349	30.800052
475.808358	26654.850354	30.805069
476.159275	26710.606831	30.810087
476.614471	26750.293283	30.815104
477.354767	26794.020811	30.820122
477.766840	26848.543687	30.825140
478.221892	26872.313059	30.830157
478.588506	26920.436974	30.835175
478.947461	26963.865271	30.840192
479.565974	27004.809154	30.845210
480.148499	27057.768248	30.850228
480.433965	27097.470964	30.855245
481.033717	27138.399341	30.860263
481.415583	27190.597109	30.865280
482.390907	27233.722199	30.870298
482.393417	27282.591901	30.875316
482.787570	27312.182611	30.880333
483.324411	27353.342724	30.885351
483.572127	27405.178481	30.890368
483.932425	27443.872766	30.895386
484.348019	27489.731486	30.900404
485.184895	27532.791903	30.905421
484.925723	27577.122129	30.910439
485.523331	27631.395942	30.915456
486.489822	27674.517283	30.920474
486.712231	27724.105789	30.925492
487.071041	27775.776000	30.930509
487.572681	27829.854954	30.935527
487.999285	27876.788604	30.940544
488.618085	27929.820068	30.945562
489.077670	27983.849676	30.950580
489.799878	28028.059666	30.955597
490.253046	28089.740743	30.960615
490.587114	28139.589568	30.965632
491.013740	28182.987631	30.970650
491.604647	28245.211158	30.975668
491.955102	28297.089355	30.980685
492.522602	28352.266340	30.985703
493.371121	28404.923683	30.990720
493.883639	28450.544911	30.995738
494.263037	28510.047133	31.000756
494.956222	28547.117718	31.005773
495.261087	28602.067643	31.010791
495.953820	28653.735679	31.015808
496.870818	28696.176848	31.020826
497.275465	28748.924453	31.025844
497.883179	28790.196121	31.030861
498.252489	28826.156768	31.035879
498.837604	28876.417295	31.040896
499.330517	28916.604070	31.045914
499.488093	28977.816651	31.050932
499.881115	29025.490874	31.055949
500.673379	29073.767993	31.060967
500.905774	29128.242561	31.065984
501.486798	29176.564383	31.071002
501.784513	29226.703110	31.076020
502.267991	29283.436526	31.081037
503.196395	29340.781119	31.086055
503.477599	29381.732777	31.091072
504.147552	29430.725204	31.096090
504.342380	29489.535666	31.101108
505.116076	29543.761054	31.106125
505.581232	29591.503756	31.111143
505.751516	29655.694877	31.116160
506.437211	29689.642559	31.121178
507.245278	29757.347270	31.126196
507.546476	29803.344578	31.131213
508.063965	29852.855591	31.136231
508.696871	29906.695249	31.141248
509.211958	29959.850998	31.146266
509.344168	30009.479840	31.151284
510.006922	30050.076507	31.156301
510.680466	30108.377589	31.161319
510.793970	30165.569458	31.166336
511.648822	30212.618355	31.171354
512.062823	30273.316609	31.176372
512.458815	30323.413811	31.181389
512.851241	30385.150889	31.186407
512.935554	30447.727942	31.191424
514.182744	30498.713362	31.196442
514.313451	30559.740284	31.201460
514.855713	30607.880001	31.206477
515.768116	30650.733685	31.211495
516.026301	30714.929901	31.216512
516.804529	30752.783031	31.221530
517.157271	30803.844770	31.226548
517.568199	30849.397553	31.231565
518.244483	30901.040229	31.236583
518.854384	30952.709817	31.241600
519.482008	30996.554869	31.246618
519.996673	31043.211086	31.251636
520.244938	31094.631717	31.256653
520.961989	31141.756386	31.261671
521.027566	31186.527891	31.266688
521.603175	31240.292764	31.271706
522.317375	31294.624901	31.276724
522.590578	31339.920920	31.281741
523.229306	31385.349046	31.286759
523.653746	31451.063357	31.291776
524.545772	31491.455027	31.296794
525.010685	31559.321264	31.301812
525.129717	31612.632725	31.306829
526.124661	31668.648672	31.311847
526.335661	31724.106649	31.316864
526.898930	31768.939267	31.321882
527.392507	31830.317572	31.326900
528.036562	31890.409046	31.331917
528.751698	31946.244985	31.336935
528.868749	31992.811729	31.341952
529.575139	32051.034914	31.346970
530.335234	32106.232840	31.351988
530.648451	32173.580645	31.357005
531.514729	32221.068461	31.362023
531.668629	32288.070721	31.367040
532.313697	32337.700127	31.372058
532.704967	32390.236816	31.377076
533.289650	32454.461047	31.382093
533.841705	32509.129822	31.387111
534.242526	32577.098911	31.392128
535.099097	32632.929387	31.397146
535.736283	32689.086645	31.402164
535.901419	32748.345171	31.407181
536.533800	32797.239570	31.412199
537.139606	32860.978980	31.417216
537.735246	32926.216029	31.422234
538.268395	32978.854048	31.427252
538.689738	33042.451073	31.432269
539.289323	33094.683996	31.437287
539.917796	33164.069225	31.442304
540.757550	33205.454843	31.447322
541.494654	33268.867896	31.452340
541.767698	33321.013510	31.457357
542.432554	33374.303052	31.462375
542.572211	33422.132046	31.467392
543.407098	33475.390601	31.472410
544.371715	33541.234693	31.477428
544.478593	33589.325166	31.482445
545.374562	33647.746265	31.487463
545.685866	33710.208901	31.492480
546.463521	33757.147463	31.497498
547.150881	33805.470663	31.502516
547.316869	33861.381388	31.507533
548.030044	33906.573280	31.512551
548.639964	33959.671694	31.517568
548.626424	34008.095634	31.522586
549.507182	34068.492964	31.527604
549.826453	34122.734998	31.532621
550.459209	34173.703288	31.537639
550.821137	34245.506802	31.542656
551.442122	34288.092459	31.547674
552.246205	34352.116811	31.552692
552.480344	34403.277941	31.557709
553.186689	34448.620656	31.562727
553.408691	34508.898095	31.567744
554.265788	34551.457935	31.572762
555.277595	34606.508352	31.577780
555.293364	34655.459371	31.582797
555.737186	34708.574865	31.587815
555.957880	34765.883717	31.592832
556.722622	34825.109876	31.597850
557.429122	34875.521994	31.602868
557.564095	34941.186609	31.607885
558.505234	34997.322926	31.612903
558.951480	35064.050525	31.617920
559.162963	35119.812470	31.622938
559.706527	35176.933506	31.627956
560.302146	35244.094670	31.632973
560.682340	35300.252157	31.637991
561.044378	35367.768026	31.643008
561.846608	35434.996709	31.648026
562.810834	35508.962150	31.653044
563.125288	35580.782010	31.658061
563.852984	35642.140988	31.663079
564.178320	35703.232208	31.668096
564.840295	35765.189502	31.673114
565.557904	35835.608664	31.678132
566.459570	35911.006333	31.683149
566.976462	35964.441675	31.688167
567.438482	36029.696350	31.693184
568.054047	36082.834824	31.698202
568.908237	36145.111948	31.703220
569.399506	36222.510362	31.708237
570.036007	36273.364054	31.713255
570.870828	36340.698031	31.718272
571.243953	36385.857741	31.723290
571.829389	36439.570358	31.728308
572.297905	36491.967418	31.733325
573.193867	36555.277426	31.738343
573.373855	36627.126847	31.743360
573.758554	36679.547786	31.748378
574.536437	36733.709179	31.753396
574.816953	36806.773603	31.758413
575.690281	36875.293097	31.763431
576.199454	36947.029352	31.768448
576.904196	37006.316791	31.773466
577.671596	37065.351024	31.778484
578.272865	37129.655524	31.783501
578.978447	37188.485759	31.788519
579.352075	37247.626768	31.793536
579.946296	37307.908777	31.798554
580.305097	37370.006949	31.803572
580.736560	37437.162387	31.808589
581.483535	37495.346032	31.813607
582.313858	37563.190311	31.818624
582.814915	37629.343849	31.823642
583.333251	37681.635098	31.828660
583.744504	37751.916703	31.833677
584.436778	37802.800179	31.838695
584.713001	37875.042629	31.843712
585.286975	37946.519594	31.848730
586.265465	38004.373015	31.853748
586.678401	38073.396164	31.858765
587.407492	38140.328192	31.863783
587.891486	38209.649432	31.868800
588.765044	38263.218767	31.873818
589.336534	38318.492238	31.878836
589.716396	38391.578152	31.883853
590.073857	38460.062709	31.888871
590.490824	38514.358566	31.893888
591.275533	38593.650321	31.898906
592.149916	38643.120294	31.903924
592.246592	38711.049194	31.908941
592.907732	38766.138732	31.913959
593.560541	38829.856742	31.918976
593.919284	38895.132476	31.923994
594.709017	38951.804846	31.929012
595.590977	39024.690268	31.934029
595.880556	39075.770184	31.939047
596.301672	39141.718308	31.944064
597.075884	39205.291273	31.949082
597.741311	39263.992802	31.954100
598.282489	39339.811570	31.959117
598.625309	39400.441970	31.964135
599.239411	39466.381428	31.969152
599.283930	39549.366841	31.974170
600.451017	39610.306656	31.979188
600.823733	39693.465704	31.984205
601.692268	39758.754869	31.989223
602.418906	39833.509582	31.994240
602.590434	39911.841507	31.999258
603.748860	39972.345168	32.004276
604.433659	40047.325491	32.009293
604.942158	40121.991195	32.014311
605.449895	40192.534531	32.019328
605.961647	40258.436942	32.024346
606.871199	40322.565927	32.029364
607.441187	40389.014773	32.034381
608.009326	40463.706721	32.039399
608.146700	40528.535567	32.044416
608.842405	40611.335948	32.049434
609.822947	40684.378960	32.054452
610.240399	40764.416426	32.059469
610.921880	40842.869978	32.064487
611.294720	40916.285945	32.069504
611.886886	40981.628327	32.074522
612.812913	41060.837897	32.079540
613.057727	41142.045222	32.084557
613.825814	41215.185466	32.089575
615.015410	41291.135447	32.094592
615.295867	41376.729291	32.099610
616.206230	41438.592128	32.104628
616.268099	41529.217254	32.109645
617.072052	41595.710657	32.114663
617.738217	41662.223937	32.119680
617.927030	41751.190629	32.124698
618.903983	41820.961679	32.129716
619.465175	41908.484711	32.134733
620.297359	41979.581037	32.139751
620.973443	42062.760539	32.144768
621.402025	42141.820244	32.149786
621.878523	42217.390013	32.154804
622.888879	42293.058040	32.159821
623.191497	42362.696431	32.164839
624.150214	42443.191472	32.169856
624.810607	42520.736869	32.174874
625.499715	42591.732918	32.179892
625.792181	42663.164256	32.184909
626.485515	42733.364524	32.189927
627.248321	42811.250955	32.194944
627.867042	42887.327175	32.199962
628.752613	42958.869902	32.204980
629.475560	43026.455302	32.209997
630.240110	43090.043230	32.215015
630.693886	43168.727405	32.220032
631.158900	43234.225040	32.225050
631.867579	43308.248459	32.230068
632.585777	43374.572969	32.235085
633.220583	43437.188978	32.240103
634.062126	43500.936067	32.245120
634.842874	43568.971688	32.250138
635.357322	43618.464026	32.255156
635.997003	43684.909978	32.260173
636.250914	43740.558478	32.265191
636.944045	43803.137648	32.270208
637.508179	43872.069026	32.275226
638.251374	43939.436516	32.280244
638.605087	44008.662119	32.285261
638.872057	44073.008248	32.290279
639.449932	44145.130560	32.295296
639.660076	44224.225742	32.300314
640.213250	44303.539210	32.305332
641.398890	44385.628041	32.310349
642.082319	44465.662663	32.315367
642.985517	44532.380619	32.320384
643.544802	44616.212847	32.325402
644.199015	44698.611993	32.330420
644.815551	44774.743604	32.335437
645.388831	44851.141602	32.340455
646.121435	44927.093590	32.345472
646.645573	45008.678844	32.350490
647.264790	45087.643669	32.355508
647.965272	45167.640563	32.360525
648.425728	45263.326910	32.365543
649.083344	45339.962393	32.370560
649.605309	45433.015390	32.375578
650.545631	45521.471474	32.380596
651.344602	45596.104727	32.385613
651.818422	45677.319110	32.390631
652.652914	45753.181782	32.395648
653.053605	45847.283150	32.400666
653.514667	45917.435862	32.405684
654.814881	45995.524482	32.410701
655.390678	46087.207625	32.415719
656.086513	46169.663147	32.420736
656.641585	46251.314961	32.425754
657.518913	46333.516964	32.430772
657.821519	46414.488099	32.435789
658.144931	46487.615135	32.440807
659.236921	46586.680513	32.445824
660.120569	46664.291332	32.450842
660.713477	46752.962223	32.455860
661.442720	46833.479298	32.460877
662.088248	46914.913736	32.465895
662.428426	46995.776919	32.470912
663.259271	47073.893946	32.475930
664.097116	47160.293530	32.480948
664.906465	47246.672956	32.485965
665.061410	47321.138477	32.490983
665.973497	47405.474184	32.496000
666.836724	47493.282717	32.501018
667.353191	47572.202251	32.506036
668.075600	47653.200789	32.511053
668.557132	47744.414857	32.516071
669.336763	47816.650422	32.521088
669.812867	47904.414355	32.526106
670.868734	47989.369953	32.531124
671.426761	48073.189246	32.536141
671.898916	48163.105710	32.541159
673.034254	48228.004450	32.546176
673.567443	48317.305174	32.551194
674.035937	48395.178053	32.556212
674.813900	48470.782995	32.561229
675.692456	48550.963639	32.566247
676.494848	48634.536522	32.571264
676.695557	48717.615555	32.576282
677.585717	48789.353297	32.581300
678.235201	48864.099892	32.586317
678.549832	48939.562252	32.591335
679.868518	49020.224747	32.596352
680.073359	49095.611134	32.601370
680.594239	49165.674304	32.606388
680.979149	49241.078846	32.611405
681.695570	49328.370532	32.616423
682.728705	49405.964602	32.621440
683.622197	49475.746177	32.626458
684.599741	49552.610977	32.631476
685.169201	49633.267337	32.636493
685.381286	49708.253806	32.641511
686.185209	49785.903118	32.646528
686.745704	49870.551034	32.651546
687.276833	49956.167505	32.656564
687.978099	50044.860976	32.661581
688.614223	50134.317348	32.666599
689.260604	50221.839442	32.671616
689.545403	50315.492389	32.676634
690.615327	50407.840942	32.681652
691.139635	50492.611275	32.686669
691.792358	50589.906487	32.691687
692.899553	50681.662692	32.696704
693.136927	50772.925188	32.701722
693.573610	50874.123665	32.706740
693.938896	50969.232044	32.711757
694.944651	51075.953444	32.716775
695.531072	51165.062714	32.721792
696.708071	51267.448453	32.726810
697.234865	51374.572909	32.731828
697.867664	51469.607897	32.736845
698.668287	51582.765526	32.741863
699.631174	51679.263114	32.746880
700.550150	51776.362289	32.751898
701.316674	51879.589886	32.756916
702.212139	51968.152627	32.761933
702.776140	52067.908487	32.766951
703.541609	52153.385326	32.771968
703.863539	52251.324790	32.776986
704.861084	52344.016721	32.782004
705.765298	52432.801242	32.787021
706.314429	52534.141366	32.792039
707.043977	52616.770563	32.797056
707.744742	52707.005161	32.802074
708.412073	52803.405574	32.807092
709.476832	52900.580993	32.812109
710.178956	52997.576801	32.817127
710.817026	53089.510406	32.822144
711.404114	53181.547645	32.827162
712.176092	53269.713408	32.832180
712.880294	53353.335507	32.837197
713.481433	53454.185299	32.842215
714.674869	53541.480177	32.847232
715.157162	53633.378917	32.852250
715.407139	53728.816749	32.857268
716.424024	53826.093125	32.862285
716.992806	53918.528567	32.867303
717.651174	54004.884152	32.872320
718.505003	54111.539849	32.877338
719.123017	54203.185022	32.882356
719.842204	54306.730189	32.887373
720.713232	54406.554559	32.892391
721.243118	54490.880069	32.897408
722.133321	54594.158357	32.902426
722.700320	54687.728690	32.907444
723.635709	54779.861106	32.912461
724.144158	54874.914208	32.917479
724.575759	54975.155337	32.922496
725.523212	55059.591118	32.927514
725.976058	55161.586229	32.932532
726.995483	55248.399329	32.937549
727.553296	55350.953043	32.942567
728.340287	55439.069153	32.947584
728.908644	55520.694618	32.952602
729.536632	55607.858382	32.957620
730.352154	55700.943761	32.962637
731.023342	55808.624541	32.967655
731.457299	55910.771957	32.972672
732.728525	56006.077112	32.977690
733.228176	56105.864055	32.982708
733.878285	56198.599993	32.987725
734.588893	56300.684690	32.992743
735.322196	56409.211500	32.997760
736.224553	56508.447284	33.002778
736.542663	56619.817957	33.007796
737.493717	56723.084616	33.012813
738.430159	56820.483785	33.017831
738.756384	56917.965411	33.022848
739.803693	57025.413611	33.027866
740.325087	57141.922639	33.032884
741.144031	57244.961078	33.037901
741.398228	57360.656160	33.042919
741.958545	57467.346824	33.047936
742.977214	57584.123728	33.052954
743.909422	57704.479741	33.057972
744.989612	57818.195574	33.062989
745.495044	57929.940665	33.068007
746.245797	58045.570195	33.073024
747.041371	58153.009202	33.078042
747.676074	58265.177138	33.083060
748.799178	58375.230005	33.088077
749.521782	58493.830652	33.093095
750.373822	58598.671653	33.098112
751.455020	58697.642224	33.103130
751.598560	58819.171785	33.108148
752.606031	58925.157922	33.113165
753.510394	59034.801869	33.118183
754.494341	59142.347706	33.123200
755.068494	59262.254025	33.128218
755.597748	59378.307023	33.133236
756.772258	59476.204232	33.138253
757.363365	59591.249671	33.143271
758.171410	59696.855721	33.148288
759.050580	59795.890367	33.153306
759.746883	59905.586085	33.158324
760.789616	60006.098877	33.163341
761.007188	60117.467588	33.168359
761.568922	60228.691500	33.173376
762.779901	60343.291058	33.178394
763.605667	60455.875623	33.183412
764.378773	60557.149925	33.188429
764.679697	60668.406737	33.193447
765.908636	60781.609007	33.198464
766.648524	60878.314478	33.203482
767.126625	60996.363446	33.208500
768.074916	61106.352613	33.213517
768.966153	61223.057828	33.218535
769.308981	61323.035559	33.223552
770.601913	61431.243974	33.228570
771.152877	61559.005121	33.233588
772.148294	61665.039141	33.238605
773.065149	61774.190139	33.243623
773.607873	61878.422911	33.248640
774.363028	61984.719550	33.253658
774.944630	62096.664581	33.258676
776.012014	62196.975502	33.263693
776.661969	62298.556909	33.268711
777.366436	62400.654431	33.273728
778.229454	62507.839815	33.278746
778.952267	62602.647348	33.283764
779.377928	62690.368147	33.288781
780.346595	62791.058587	33.293799
780.660754	62912.261921	33.298816
782.089513	63012.415910	33.303834
782.379457	63117.632281	33.308852
783.015201	63222.374799	33.313869
784.068192	63337.693597	33.318887
784.795883	63449.173014	33.323904
785.751063	63558.181747	33.328922
785.905379	63682.671446	33.333940
786.745832	63792.414687	33.338957
787.784361	63913.832783	33.343975
788.523611	64031.046835	33.348992
789.680943	64143.343910	33.354010
790.077164	64272.038770	33.359028
791.018637	64372.880482	33.364045
791.998904	64500.468726	33.369063
792.699089	64625.019180	33.374080
793.506970	64731.485587	33.379098
794.090212	64853.395380	33.384116
795.007781	64964.712455	33.389133
795.531983	65090.249361	33.394151
796.632679	65215.735923	33.399168
797.809879	65340.622665	33.404186
798.046267	65454.811294	33.409204
798.687210	65579.807127	33.414221
799.671936	65699.114089	33.419239
800.515593	65831.986518	33.424256
801.672241	65948.984272	33.429274
802.188031	66078.176242	33.434292
802.851295	66188.277504	33.439309
803.700975	66323.263593	33.444327
804.581386	66453.655649	33.449344
805.465354	66574.982032	33.454362
806.676477	66700.465548	33.459380
806.972058	66824.451154	33.464397
808.087125	66944.786799	33.469415
808.626125	67072.963165	33.474432
809.631887	67195.410984	33.479450
810.181769	67320.400621	33.484468
810.988801	67452.163972	33.489485
811.718274	67582.448886	33.494503
812.573582	67718.435599	33.499520
813.805447	67843.492561	33.504538
814.358860	67967.480164	33.509556
815.246246	68106.941451	33.514573
816.471742	68221.499934	33.519591
816.945478	68358.597093	33.524608
818.024092	68483.506146	33.529626
818.749685	68602.265424	33.534644
819.388086	68720.843781	33.539661
820.598457	68847.478259	33.544679
821.259050	68973.445682	33.549696
822.124393	69097.837210	33.554714
822.944873	69222.300112	33.559732
824.032570	69350.810479	33.564749
824.830219	69457.504790	33.569767
825.429992	69595.727198	33.574784
826.387593	69706.107897	33.579802
827.074219	69841.206595	33.584820
827.725979	69956.577490	33.589837
828.739986	70080.185055	33.594855
829.388865	70208.260978	33.599872
830.296987	70328.295921	33.604890
831.067456	70448.031816	33.609908
831.951985	70571.954500	33.614925
832.901318	70678.427461	33.619943
833.210056	70807.878466	33.624960
834.168586	70916.286032	33.629978
834.964558	71038.259476	33.634996
835.423170	71166.815218	33.640013
836.342952	71285.418150	33.645031
837.200347	71422.787654	33.650048
838.250538	71550.937990	33.655066
838.843637	71674.693893	33.660084
839.728217	71801.172053	33.665101
840.893810	71918.529992	33.670119
841.383108	72057.488416	33.675136
842.647234	72187.845744	33.680154
843.149746	72315.123652	33.685172
844.136053	72438.730356	33.690189
845.131677	72569.855304	33.695207
845.682585	72706.157991	33.700224
846.791942	72844.234736	33.705242
847.560423	72972.402128	33.710260
848.440259	73102.303612	33.715277
849.308041	73226.446643	33.720295
849.711111	73367.141519	33.725312
850.874433	73498.952631	33.730330
851.885115	73638.891057	33.735348
852.396858	73779.146894	33.740365
853.566827	73914.855137	33.745383
854.365095	74056.899403	33.750400
855.218794	74196.026225	33.755418
856.374655	74336.963325	33.760436
857.102615	74475.657361	33.765453
858.042494	74603.907162	33.770471
858.781698	74737.433909	33.775488
859.449370	74873.933179	33.780506
860.425934	75009.262761	33.785524
861.089514	75153.575295	33.790541
862.570618	75292.991102	33.795559
863.112813	75432.348031	33.800576
863.750687	75574.453926	33.805594
864.773928	75727.381948	33.810612
865.326297	75867.517887	33.815629
866.404574	76009.490494	33.820647
867.206221	76155.336329	33.825664
867.784990	76295.382060	33.830682
868.707573	76441.690473	33.835700
869.680835	76593.652369	33.840717
870.755522	76741.594761	33.845735
871.532414	76882.205983	33.850752
872.402434	77024.156273	33.855770
873.185747	77177.323725	33.860788
874.159879	77332.819984	33.865805
874.953251	77476.689730	33.870823
875.788665	77624.639606	33.875840
876.856956	77762.633783	33.880858
877.463947	77913.975792	33.885876
878.399228	78075.347293	33.890893
879.577657	78207.841838	33.895911
880.356610	78370.879622	33.900928
881.240542	78508.655864	33.905946
881.969649	78658.787171	33.910964
882.814438	78813.745802	33.915981
883.984124	78960.662412	33.920999
885.016751	79113.846153	33.926016
885.899294	79253.449000	33.931034
886.416790	79398.964465	33.936052
887.201227	79545.259083	33.941069
888.135518	79683.230285	33.946087
889.034421	79832.044516	33.951104
889.712753	79973.121571	33.956122
890.799707	80112.474512	33.961140
891.665700	80250.447814	33.966157
892.387143	80391.602584	33.971175
893.662661	80543.009837	33.976192
894.545272	80675.700651	33.981210
895.278329	80814.983583	33.986228
896.205243	80968.216333	33.991245
897.376021	81098.736337	33.996263
897.844163	81249.389804	34.001280
898.814334	81395.115238	34.006298
899.753164	81539.783948	34.011316
900.629614	81695.326418	34.016333
901.557084	81838.474220	34.021351
902.217454	81990.992409	34.026368
903.295953	82144.739414	34.031386
904.077576	82294.316687	34.036404
905.086472	82456.751098	34.041421
905.696519	82608.459245	34.046439
906.850161	82757.364321	34.051456
907.644807	82920.413173	34.056474
908.632538	83077.775053	34.061492
909.431573	83234.669389	34.066509
910.744713	83393.561332	34.071527
911.307689	83552.363307	34.076544
912.077875	83716.453124	34.081562
913.409698	83868.708208	34.086580
914.175823	84029.352669	34.091597
915.115670	84184.009347	34.096615
915.970632	84347.412608	34.101632
916.379983	84511.599359	34.106650
917.632389	84677.185381	34.111668
918.537711	84845.082506	34.116685
919.697679	85010.198980	34.121703
920.453035	85179.198963	34.126720
921.395305	85330.408094	34.131738
922.427094	85492.638551	34.136756
923.182093	85667.811438	34.141773
924.357297	85830.735536	34.146791
925.387073	85993.482333	34.151808
926.486423	86152.441133	34.156826
927.577089	86309.181417	34.161844
928.188908	86470.538936	34.166861
929.677649	86634.169770	34.171879
930.461658	86791.413254	34.176896
931.260888	86951.566099	34.181914
932.244632	87110.404948	34.186932
933.098030	87282.264085	34.191949
933.959394	87437.575378	34.196967
935.060143	87595.872917	34.201984
935.994165	87773.347938	34.207002
936.749413	87923.731386	34.212020
937.550710	88087.378390	34.217037
938.607594	88249.269304	34.222055
939.706886	88423.532426	34.227072
940.718289	88579.421242	34.232090
941.573150	88737.842999	34.237108
942.835434	88899.527178	34.242125
943.566826	89060.547158	34.247143
944.675316	89227.423007	34.252160
945.671645	89389.534194	34.257178
946.612750	89537.466937	34.262196
947.120307	89707.211092	34.267213
948.251683	89869.429768	34.272231
949.144486	90032.866132	34.277248
950.122306	90199.745046	34.282266
951.332075	90347.094082	34.287284
951.936377	90498.923691	34.292301
952.957250	90643.559065	34.297319
953.610908	90797.483577	34.302336
954.117144	90960.774978	34.307354
955.230309	91110.511683	34.312372
956.293724	91269.194134	34.317389
957.669108	91436.604465	34.322407
958.668343	91597.894605	34.327424
958.987849	91764.804587	34.332442
960.234451	91909.840591	34.337460
960.999668	92085.153870	34.342477
961.843140	92247.550052	34.347495
962.877120	92416.036278	34.352512
963.629477	92577.753502	34.357530
964.736504	92743.793105	34.362548
965.912328	92922.316816	34.367565
966.804190	93099.451987	34.372583
968.230553	93262.714295	34.377600
968.759436	93433.379808	34.382618
969.935071	93601.496324	34.387636
970.958573	93778.171558	34.392653
971.643135	93947.764176	34.397671
972.886524	94119.151829	34.402688
973.494895	94297.266665	34.407706
974.736679	94458.364665	34.412724
975.827073	94634.503274	34.417741
976.926114	94806.451284	34.422759
978.077276	94974.233068	34.427776
978.942875	95144.462292	34.432794
980.026667	95317.024053	34.437812
980.748268	95498.464764	34.442829
981.596232	95673.954537	34.447847
982.693021	95839.440653	34.452864
983.678409	96028.469515	34.457882
984.940829	96200.438147	34.462900
985.899187	96379.377311	34.467917
986.820625	96557.266686	34.472935
987.371754	96729.293270	34.477952
988.442841	96913.104709	34.482970
989.308927	97086.461711	34.487988
990.411041	97288.382408	34.493005
991.524672	97467.335322	34.498023
992.797078	97640.470696	34.503040
993.583035	97832.977371	34.508058
994.848258	98013.656379	34.513076
995.567249	98202.619062	34.518093
996.354879	98381.309497	34.523111
997.776203	98569.316786	34.528128
998.113737	98755.250860	34.533146
999.506174	98934.376992	34.538164
1000.785257	99132.218678	34.543181
1001.464768	99309.850926	34.548199
1002.611634	99485.881336	34.553216
1003.827249	99682.914753	34.558234
1004.743264	99874.972240	34.563252
1005.864891	100041.577141	34.568269
1006.865056	100229.868943	34.573287
1007.704931	100408.153437	34.578304
1008.480163	100610.464861	34.583322
1009.525874	100790.952966	34.588340
1010.742615	100970.654282	34.593357
1011.520018	101153.506624	34.598375
1012.752381	101354.064126	34.603392
1013.259683	101546.955163	34.608410
1014.297470	101725.792243	34.613428
1015.591614	101924.748382	34.618445
1016.328632	102122.645785	34.623463
1017.798858	102307.094985	34.628480
1018.594749	102488.054164	34.633498
1019.562185	102664.091675	34.638516
1020.571892	102844.809032	34.643533
1021.477605	103020.086660	34.648551
1022.682109	103199.558528	34.653568
1023.502100	103390.233337	34.658586
1024.435141	103560.539393	34.663604
1025.377262	103755.667154	34.668621
1026.580447	103943.281188	34.673639
1027.630861	104122.056660	34.678656
1028.356467	104323.873321	34.683674
1029.278961	104512.614326	34.688692
1030.509641	104710.981635	34.693709
1031.572385	104897.663178	34.698727
1032.294607	105086.998665	34.703744
1033.398285	105284.492071	34.708762
1034.420201	105484.470179	34.713780
1035.714749	105686.456493	34.718797
1036.708676	105881.553431	34.723815
1037.618495	106083.327739	34.728832
1038.719885	106290.366105	34.733850
1039.862533	106489.597217	34.738868
1040.784010	106689.056372	34.743885
1041.618294	106906.276280	34.748903
1042.770666	107107.650924	34.753920
1043.407218	107318.776557	34.758938
1044.740416	107528.648715	34.763956
1046.009988	107735.417139	34.768973
1046.680185	107955.015924	34.773991
1047.981109	108155.930547	34.779008
1049.017270	108378.436220	34.784026
1050.165888	108585.991162	34.789044
1051.539381	108781.502455	34.794061
1052.454059	108998.839959	34.799079
1053.857552	109202.342101	34.804096
1054.699659	109416.173541	34.809114
1055.290158	109628.110190	34.814132
1056.986837	109847.719276	34.819149
1057.680266	110057.146799	34.824167
1059.165476	110261.390717	34.829184
1060.047865	110477.199930	34.834202
1061.202976	110684.516453	34.839220
1062.492759	110899.463574	34.844237
1063.354535	111114.533812	34.849255
1064.685009	111314.618113	34.854272
1065.545726	111532.757425	34.859290
1066.476780	111745.718246	34.864308
1067.452588	111941.571247	34.869325
1068.437471	112169.322880	34.874343
1069.831104	112375.649893	34.879360
1070.930834	112596.975846	34.884378
1071.658662	112814.551803	34.889396
1073.213457	113026.279159	34.894413
1074.303627	113247.130451	34.899431
1075.568220	113451.092372	34.904448
1076.467821	113662.641495	34.909466
1077.441743	113878.221360	34.914484
1078.849208	114078.401516	34.919501
1079.618840	114294.309743	34.924519
1080.543297	114501.046757	34.929536
1081.665199	114722.436533	34.934554
1082.753552	114927.451870	34.939572
1084.287834	115131.774158	34.944589
1085.017038	115350.585827	34.949607
1086.136002	115567.016167	34.954624
1087.065671	115779.399739	34.959642
1088.596512	115992.052937	34.964660
1089.468038	116190.195422	34.969677
1090.645429	116394.040985	34.974695
1091.760042	116589.295259	34.979712
1092.865641	116785.946099	34.984730
1093.862661	116989.889082	34.989748
1095.286441	117174.655781	34.994765
1096.154014	117383.184357	34.999783
1097.257483	117568.994857	35.004800
1098.067663	117779.943232	35.009818
1098.884510	117985.773005	35.014836
1100.019028	118180.008458	35.019853
1100.875112	118404.144298	35.024871
1102.029968	118607.058946	35.029888
1103.358676	118824.720962	35.034906
1103.917589	119045.945813	35.039924
1105.215738	119263.806240	35.044941
1106.311240	119491.560264	35.049959
1107.508611	119698.961229	35.054976
1108.451432	119932.471516	35.059994
1109.388615	120151.589382	35.065012
1110.559965	120375.510852	35.070029
1111.375341	120603.661977	35.075047
1112.944203	120833.312335	35.080064
1113.963274	121058.860867	35.085082
1115.264589	121294.527668	35.090100
1116.446292	121511.904464	35.095117
1117.578436	121749.262941	35.100135
1118.980846	121974.222827	35.105152
1119.818945	122197.148692	35.110170
1120.938563	122437.480149	35.115188
1122.172914	122661.573241	35.120205
1123.187928	122894.334595	35.125223
1124.452663	123133.722531	35.130240
1125.978104	123365.668123	35.135258
1127.203545	123592.012807	35.140276
1128.368454	123813.642024	35.145293
1129.735780	124038.078270	35.150311
1130.859224	124274.418982	35.155328
1132.144346	124492.408661	35.160346
1132.994608	124722.144348	35.165364
1134.185223	124928.568955	35.170381
1135.381010	125169.137753	35.175399
1136.577068	125388.289245	35.180416
1137.695305	125617.036833	35.185434
1138.696439	125845.805492	35.190452
1140.117355	126064.303622	35.195469
1140.895071	126295.140465	35.200487
1142.337854	126521.787899	35.205504
1143.612569	126741.176884	35.210522
1144.402347	126980.572240	35.215540
1145.948205	127205.014936	35.220557
1147.027981	127423.857958	35.225575
1148.131480	127649.543096	35.230592
1149.621747	127882.276658	35.235610
1150.443203	128111.205897	35.240628
1151.690344	128330.674074	35.245645
1152.714547	128550.003195	35.250663
1154.002679	128782.029047	35.255680
1155.374102	129015.475186	35.260698
1156.329335	129223.057524	35.265716
1157.325405	129446.301663	35.270733
1158.448249	129691.354171	35.275751
1159.629267	129906.623264	35.280768
1161.229126	130129.265392	35.285786
1161.751623	130364.002700	35.290804
1163.187074	130585.141406	35.295821
1164.168754	130816.218796	35.300839
1165.309547	131056.309804	35.305856
1166.667519	131272.420906	35.310874
1167.282464	131506.771067	35.315892
1168.632781	131713.962141	35.320909
1170.025238	131934.293331	35.325927
1170.671448	132150.350547	35.330944
1171.938426	132370.211076	35.335962
1172.984874	132594.026743	35.340980
1174.316966	132807.642425	35.345997
1175.443280	133045.798445	35.351015
1176.544414	133263.689484	35.356032
1177.970604	133488.247231	35.361050
1179.333724	133728.283392	35.366068
1180.692597	133945.236300	35.371085
1181.593565	134167.958579	35.376103
1182.778080	134398.609758	35.381120
1183.914486	134618.849398	35.386138
1185.045615	134856.891081	35.391156
1186.172798	135083.106627	35.396173
1186.958286	135321.120060	35.401191
1188.365647	135556.382685	35.406208
1189.311720	135798.658218	35.411226
1190.405132	136054.743195	35.416244
1191.860134	136298.066619	35.421261
1192.901609	136544.896052	35.426279
1193.855459	136785.871613	35.431296
1195.538308	137031.609699	35.436314
1196.620605	137272.580216	35.441332
1197.699997	137518.446985	35.446349
1198.940634	137769.753529	35.451367
1200.441004	138032.290693	35.456384
1201.792150	138273.857897	35.461402
1202.697716	138521.776704	35.466420
1204.221931	138771.687153	35.471437
1205.662175	139021.930308	35.476455
1206.836853	139263.457657	35.481472
1208.032396	139518.664565	35.486490
1209.021987	139761.443275	35.491508
1210.358873	140008.604227	35.496525
1211.362182	140260.247378	35.501543
1212.653709	140512.022250	35.506560
1214.292644	140757.591703	35.511578
1215.372882	141022.858783	35.516596
1216.573107	141260.084698	35.521613
1217.907739	141521.927923	35.526631
1219.020520	141766.031818	35.531648
1220.577619	142013.589166	35.536666
1221.642049	142251.338829	35.541684
1223.078470	142497.524689	35.546701
1224.092839	142752.303532	35.551719
1225.548713	142999.161780	35.556736
1227.061632	143247.445279	35.561754
1228.089342	143494.339727	35.566772
1229.091303	143743.243775	35.571789
1230.311062	143991.758497	35.576807
1231.594050	144246.135962	35.581824
1233.279617	144480.069670	35.586842
1234.443960	144728.294343	35.591860
1235.428150	144972.720680	35.596877
1236.737410	145225.743854	35.601895
1238.083097	145466.068348	35.606912
1239.074735	145715.710716	35.611930
1240.111248	145968.353014	35.616948
1241.519103	146215.304881	35.621965
1242.487293	146469.838913	35.626983
1244.021066	146723.494949	35.632000
1245.435520	146969.499693	35.637018
1246.332496	147223.251783	35.642036
1247.361386	147473.876628	35.647053
1249.041457	147723.964349	35.652071
1250.361301	147973.187484	35.657088
1251.696700	148194.685324	35.662106
1252.828235	148434.392628	35.667124
1254.140515	148665.497990	35.672141
1255.406659	148906.619270	35.677159
1256.395194	149135.777169	35.682176
1258.010275	149363.551927	35.687194
1259.117540	149602.205407	35.692212
1259.999952	149832.146120	35.697229
1261.442021	150087.222925	35.702247
1262.208853	150323.020097	35.707264
1263.514330	150569.624857	35.712282
1264.752845	150826.072089	35.717300
1266.183518	151077.288990	35.722317
1267.482192	151324.457885	35.727335
1268.609421	151582.526790	35.732352
1269.939185	151832.014995	35.737370
1270.814966	152093.312589	35.742388
1272.158573	152347.558384	35.747405
1273.741810	152619.270451	35.752423
1274.792152	152878.984393	35.757440
1276.367951	153136.951586	35.762458
1277.414019	153404.216972	35.767476
1278.765114	153670.583924	35.772493
1280.103666	153928.024799	35.777511
1281.432981	154199.320612	35.782528
1282.774622	154459.428279	35.787546
1283.859836	154734.040831	35.792564
1285.339765	155004.809944	35.797581
1286.465436	155264.578100	35.802599
1288.164693	155544.917272	35.807616
1289.543125	155810.101858	35.812634
1290.853932	156088.048146	35.817652
1291.754960	156349.535016	35.822669
1293.460596	156619.339157	35.827687
1294.342958	156896.042604	35.832704
1295.629316	157155.758513	35.837722
1297.079391	157423.111234	35.842740
1298.505405	157710.475270	35.847757
1299.695920	157985.016744	35.852775
1300.672092	158261.181257	35.857792
1302.294753	158526.977750	35.862810
1303.615171	158802.835326	35.867828
1305.127080	159095.269442	35.872845
1306.230916	159362.501870	35.877863
1307.665990	159643.750551	35.882880
1308.758792	159932.872623	35.887898
1309.848531	160206.164330	35.892916
1311.236119	160493.706523	35.897933
1313.033846	160768.610319	35.902951
1314.399608	161052.315888	35.907968
1315.706767	161328.433585	35.912986
1316.987046	161610.672697	35.918004
1318.397778	161892.016733	35.923021
1319.988959	162168.296005	35.928039
1321.082164	162436.793266	35.933056
1322.389377	162716.700867	35.938074
1323.587380	162999.571849	35.943092
1324.989595	163275.762689	35.948109
1326.269934	163547.839294	35.953127
1327.623388	163824.599990	35.958144
1329.277880	164098.749784	35.963162
1330.367585	164381.660474	35.968180
1331.593286	164661.315111	35.973197
1333.111706	164938.474386	35.978215
1334.234750	165227.120067	35.983232
1335.569398	165495.495022	35.988250
1337.068437	165777.217888	35.993268
1338.178785	166043.488951	35.998285
1339.349540	166305.907049	36.003303
1340.688850	166573.678772	36.008320
1342.315129	166839.742487	36.013338
1343.582700	167102.238124	36.018356
1344.642509	167370.238484	36.023373
1346.186636	167637.386395	36.028391
1347.403705	167904.539195	36.033408
1348.813201	168171.103468	36.038426
1349.860390	168449.809148	36.043444
1350.667717	168726.716266	36.048461
1352.375352	169003.793516	36.053479
1353.225404	169297.307196	36.058496
1355.024965	169582.278186	36.063514
1356.353658	169874.599808	36.068532
1357.641188	170176.434534	36.073549
1359.264046	170459.143368	36.078567
1360.290508	170753.626983	36.083584
1361.640065	171047.843346	36.088602
1363.072136	171339.763764	36.093620
1364.102695	171637.488197	36.098637
1365.427207	171937.602420	36.103655
1366.630480	172250.707846	36.108672
1368.529633	172557.050706	36.113690
1369.748350	172866.325229	36.118708
1371.239231	173173.335979	36.123725
1372.625616	173472.789806	36.128743
1373.840437	173785.852670	36.133760
1375.390022	174093.430690	36.138778
1376.939962	174401.581691	36.143796
1378.268249	174710.228150	36.148813
1380.098321	175020.050035	36.153831
1381.354784	175330.235190	36.158848
1382.778503	175641.828749	36.163866
1383.984560	175950.185963	36.168884
1385.208547	176250.762483	36.173901
1386.815038	176561.481342	36.178919
1388.110539	176880.084056	36.183936
1389.450258	177193.274978	36.188954
1390.732449	177511.185888	36.193972
1392.354861	177827.456146	36.198989
1393.719033	178137.577560	36.204007
1395.219109	178477.541937	36.209024
1396.316223	178783.269335	36.214042
1397.809976	179094.479350	36.219060
1399.168860	179419.446193	36.224077
1400.489950	179737.275738	36.229095
1401.842513	180068.124105	36.234112
1403.369816	180389.718506	36.239130
1404.755337	180720.387882	36.244148
1405.920997	181055.969528	36.249165
1407.411924	181375.075604	36.254183
1408.709313	181707.796535	36.259200
1410.469414	182038.704211	36.264218
1411.845359	182364.219593	36.269236
1412.656923	182699.641680	36.274253
1414.607009	183019.976392	36.279271
1416.015229	183352.841551	36.284288
1417.656509	183689.401966	36.289306
1419.064480	184020.963887	36.294324
1420.397205	184346.980677	36.299341
1421.726348	184674.827810	36.304359
1423.169052	185003.990915	36.309376
1424.152870	185337.471372	36.314394
1425.969685	185667.515895	36.319412
1427.231889	186013.863575	36.324429
1428.770249	186350.203318	36.329447
1430.487822	186686.439290	36.334464
1431.990660	187003.938761	36.339482
1432.997643	187311.506558	36.344500
1434.375404	187624.003414	36.349517
1436.305981	187942.389449	36.354535
1437.704034	188262.337736	36.359552
1438.694633	188573.570840	36.364570
1439.962746	188891.652650	36.369588
1441.397035	189213.999361	36.374605
1443.000941	189544.126776	36.379623
1443.949882	189867.204665	36.384640
1445.388963	190194.735218	36.389658
1446.737848	190523.996225	36.394676
1448.424336	190868.068550	36.399693
1450.030024	191202.292486	36.404711
1450.839220	191545.421896	36.409728
1452.579658	191881.277612	36.414746
1454.326507	192233.421561	36.419764
1455.581434	192570.097574	36.424781
1457.091401	192920.989714	36.429799
1458.256361	193269.046377	36.434816
1459.724615	193624.608447	36.439834
1460.964391	193975.995486	36.444852
1462.469775	194343.171560	36.449869
1464.238240	194687.962530	36.454887
1465.574790	195045.445941	36.459904
1466.973095	195406.920206	36.464922
1468.524029	195766.657378	36.469940
1469.817020	196135.643470	36.474957
1471.512551	196488.555896	36.479975
1472.879466	196869.137742	36.484992
1474.323587	197235.210406	36.490010
1476.105482	197595.909700	36.495028
1477.324511	197978.401317	36.500045
1479.244963	198338.027942	36.505063
1480.215320	198707.310134	36.510080
1481.605492	199088.014981	36.515098
1483.272975	199463.178653	36.520116
1484.917488	199843.337804	36.525133
1486.316422	200219.045099	36.530151
1487.889861	200591.945060	36.535168
1489.563710	200970.366080	36.540186
1491.390233	201341.755392	36.545204
1492.737294	201721.123163	36.550221
1494.416200	202086.179718	36.555239
1495.868526	202466.752907	36.560256
1497.038566	202851.006023	36.565274
1499.264745	203215.228707	36.570292
1500.400432	203588.038755	36.575309
1502.209464	203962.339246	36.580327
1503.421796	204336.689414	36.585344
1504.822579	204700.357401	36.590362
1506.801127	205076.933612	36.595380
1508.088251	205450.553184	36.600397
1509.601217	205825.737121	36.605415
1511.153224	206199.989518	36.610432
1512.403122	206582.458090	36.615450
1514.272986	206944.941784	36.620468
1516.095334	207324.195787	36.625485
1517.063741	207691.034728	36.630503
1518.860920	208064.239631	36.635520
1520.458813	208455.116361	36.640538
1522.208498	208814.720576	36.645556
1523.653509	209188.293565	36.650573
1525.114074	209549.523294	36.655591
1526.463070	209923.001174	36.660608
1528.504322	210305.991452	36.665626
1530.067992	210661.329742	36.670644
1531.470997	211023.299093	36.675661
1532.910498	211364.464298	36.680679
1534.624119	211716.480652	36.685696
1536.039934	212062.249278	36.690714
1537.390113	212409.604705	36.695732
1538.621964	212763.101672	36.700749
1539.888546	213101.864108	36.705767
1541.641108	213462.769891	36.710784
1543.007044	213837.099859	36.715802
1544.430321	214193.720046	36.720820
1545.984239	214567.107641	36.725837
1547.347830	214929.150151	36.730855
1549.053883	215299.925014	36.735872
1550.453608	215671.971028	36.740890
1552.241853	216037.604886	36.745908
1553.785779	216417.960422	36.750925
1555.132232	216799.289799	36.755943
1556.609688	217182.732450	36.760960
1557.916067	217568.363694	36.765978
1559.799117	217943.030735	36.770996
1561.225718	218339.820290	36.776013
1562.629929	218733.262508	36.781031
1564.777196	219106.163105	36.786048
1566.408081	219501.882072	36.791066
1568.152417	219890.243582	36.796084
1569.302705	220283.327236	36.801101
1571.129110	220671.855840	36.806119
1572.758720	221052.544687	36.811136
1574.270231	221450.805104	36.816154
1576.133996	221830.543610	36.821172
1577.559400	222227.982880	36.826189
1579.115213	222621.363525	36.831207
1580.759821	223024.052435	36.836224
1582.192369	223416.897397	36.841242
1583.721134	223826.415299	36.846260
1584.648618	224279.645163	36.851277
1586.595787	224686.429956	36.856295
1588.623373	225087.030680	36.861312
1589.812450	225496.102416	36.866330
1591.652410	225892.672781	36.871348
1593.213285	226304.886156	36.876365
1594.492183	226715.445647	36.881383
1596.083930	227123.084541	36.886400
1597.848820	227546.368107	36.891418
1599.459298	227955.606723	36.896436
1601.602221	228374.791821	36.901453
1602.996222	228788.894828	36.906471
1604.503712	229198.535227	36.911488
1606.001389	229608.381660	36.916506
1607.878545	230014.559683	36.921524
1609.474500	230433.206330	36.926541
1611.032107	230848.736205	36.931559
1612.436879	231267.924842	36.936576
1613.828873	231689.072647	36.941594
1615.613122	232098.446897	36.946612
1617.317071	232525.692541	36.951629
1618.805656	232949.875973	36.956647
1620.694550	233363.808468	36.961664
1622.417557	233792.197419	36.966682
1624.085518	234213.026941	36.971700
1625.693382	234637.931691	36.976717
1627.202463	235055.512758	36.981735
1628.856777	235468.092113	36.986752
1630.164266	235902.092563	36.991770
1632.213233	236323.346890	36.996788
1633.505939	236741.018446	37.001805
1634.565864	237176.256688	37.006823
1636.877926	237592.339230	37.011840
1638.103481	238023.640125	37.016858
1639.823143	238427.883357	37.021876
1641.480967	238827.158799	37.026893
1643.035472	239255.715352	37.031911
1645.143691	239655.680039	37.036928
1646.257972	240065.437107	37.041946
1647.920317	240466.162794	37.046964
1649.401990	240894.582182	37.051981
1650.744885	241316.776301	37.056999
1652.636357	241719.752528	37.062016
1654.062576	242153.416253	37.067034
1655.580211	242574.288170	37.072052
1657.308454	243005.718855	37.077069
1658.898260	243448.578883	37.082087
1660.753222	243881.361794	37.087104
1662.018232	244329.865478	37.092122
1663.715204	244768.797892	37.097140
1665.489168	245205.330381	37.102157
1667.143850	245662.230830	37.107175
1668.853491	246096.793778	37.112192
1670.314371	246551.415845	37.117210
1672.138279	247001.787077	37.122228
1674.040312	247455.676985	37.127245
1675.496555	247915.534575	37.132263
1677.220526	248360.259121	37.137280
1678.775532	248811.616853	37.142298
1680.344444	249282.355293	37.147316
1682.142603	249739.059281	37.152333
1683.835932	250211.276920	37.157351
1685.595558	250685.287685	37.162368
1687.340966	251144.160963	37.167386
1689.130014	251622.562442	37.172404
1690.955830	252079.746586	37.177421
1692.541299	252556.277189	37.182439
1694.529918	253018.541140	37.187456
1695.782289	253491.570944	37.192474
1697.974477	253964.369580	37.197492
1699.834088	254422.921371	37.202509
1701.222321	254904.033125	37.207527
1703.390702	255365.887559	37.212544
1704.965255	255829.237426	37.217562
1706.936231	256318.382508	37.222580
1708.500348	256779.498879	37.227597
1709.927062	257249.783226	37.232615
1711.949717	257717.378074	37.237632
1713.567232	258202.187117	37.242650
1715.632869	258669.139849	37.247668
1717.271811	259146.146553	37.252685
1718.822338	259616.181921	37.257703
1720.982374	260090.054069	37.262720
1722.853394	260563.948468	37.267738
1724.271768	261039.187685	37.272756
1726.243975	261499.804613	37.277773
1727.913630	261980.768575	37.282791
1729.827964	262444.366907	37.287808
1731.439438	262917.490469	37.292826
1733.277082	263386.435710	37.297844
1735.147627	263857.331305	37.302861
1736.250814	264330.588838	37.307879
1738.132551	264795.867879	37.312896
1739.918333	265271.349108	37.317914
1741.437442	265755.028422	37.322932
1743.698590	266224.130387	37.327949
1745.380308	266704.835246	37.332967
1746.885716	267169.869665	37.337984
1748.585512	267649.859322	37.343002
1750.668413	268122.545330	37.348020
1752.307546	268594.186378	37.353037
1753.862209	269068.152501	37.358055
1755.462098	269516.097976	37.363072
1757.260373	269973.485429	37.368090
1758.937138	270435.160048	37.373108
1760.749851	270895.516050	37.378125
1762.268188	271357.342589	37.383143
1763.811141	271808.546041	37.388160
1765.333547	272273.850737	37.393178
1767.431088	272744.622904	37.398196
1769.017130	273209.407551	37.403213
1770.584658	273692.865389	37.408231
1772.237560	274169.220949	37.413248
1774.167085	274654.344624	37.418266
1775.513510	275134.508589	37.423284
1777.536834	275626.702171	37.428301
1778.829535	276115.865518	37.433319
1780.872295	276617.986140	37.438336
1782.638368	277108.085283	37.443354
1784.396770	277612.460626	37.448372
1786.031239	278106.897622	37.453389
1787.838285	278627.926301	37.458407
1789.545383	279129.182004	37.463424
1791.473667	279643.862932	37.468442
1792.862363	280156.751871	37.473460
1794.877359	280670.806074	37.478477
1796.597638	281208.556515	37.483495
1798.256614	281720.126391	37.488512
1800.195692	282255.068763	37.493530
1801.726961	282783.624851	37.498548
1803.681492	283319.831406	37.503565
1805.629456	283859.060060	37.508583
1807.124493	284390.131716	37.513600
1809.208073	284936.751495	37.518618
1810.843273	285478.667998	37.523636
1812.601303	286019.927257	37.528653
1814.289298	286580.500772	37.533671
1816.419880	287111.000730	37.538688
1818.061841	287664.897237	37.543706
1819.815603	288230.482757	37.548724
1822.062617	288775.613321	37.553741
1823.638491	289327.558220	37.558759
1825.298889	289891.602788	37.563776
1827.383223	290445.999050	37.568794
1829.156514	291008.445292	37.573812
1831.035521	291573.462354	37.578829
1832.914624	292140.712003	37.583847
1835.012398	292689.939919	37.588864
1837.080937	293251.514332	37.593882
1838.852174	293816.005301	37.598900
1840.243789	294371.158464	37.603917
1842.208513	294946.254245	37.608935
1844.158427	295505.627506	37.613952
1846.365870	296069.984397	37.618970
1847.827653	296638.372917	37.623988
1849.980085	297200.243909	37.629005
1851.679894	297768.256909	37.634023
1853.331538	298331.169689	37.639040
1855.633366	298889.832099	37.644058
1857.303449	299467.771323	37.649076
1859.262650	300026.636387	37.654093
1861.100058	300594.179047	37.659111
1862.785649	301162.759370	37.664128
1864.921374	301748.176729	37.669146
1866.761518	302306.337120	37.674164
1868.716030	302866.837228	37.679181
1870.682259	303449.376628	37.684199
1872.537088	304008.870325	37.689216
1874.800680	304571.950167	37.694234
1876.269006	305133.837140	37.699252
1878.302441	305670.230791	37.704269
1880.383139	306215.121061	37.709287
1881.943862	306752.932035	37.714304
1883.775523	307288.028283	37.719322
1885.697007	307833.569335	37.724340
1887.610058	308363.870833	37.729357
1889.306819	308906.826144	37.734375
1891.261149	309456.058707	37.739392
1893.190331	310001.228450	37.744410
1894.787382	310545.839816	37.749428
1896.578267	311110.375652	37.754445
1898.602401	311671.897710	37.759463
1900.105525	312233.577882	37.764480
1901.934014	312797.333290	37.769498
1903.491928	313372.099351	37.774516
1905.259156	313942.306323	37.779533
1907.086697	314528.496875	37.784551
1908.623550	315116.000386	37.789568
1911.245163	315698.977764	37.794586
1912.754780	316294.398796	37.799604
1914.410952	316896.418118	37.804621
1916.781676	317493.819798	37.809639
1918.519498	318100.715979	37.814656
1920.704882	318685.898846	37.819674
1922.418675	319307.185563	37.824692
1924.758726	319906.881831	37.829709
1926.330641	320517.160776	37.834727
1928.535149	321132.560188	37.839744
1930.550374	321735.391165	37.844762
1932.245330	322356.753798	37.849780
1934.608515	322969.367321	37.854797
1936.194555	323574.486193	37.859815
1938.215260	324197.224234	37.864832
1940.400861	324808.706581	37.869850
1942.472219	325435.333808	37.874868
1944.644780	326047.161408	37.879885
1946.717322	326656.206554	37.884903
1948.133505	327280.003125	37.889920
1950.556400	327904.413961	37.894938
1952.063665	328530.670356	37.899956
1954.106900	329151.068497	37.904973
1956.432124	329782.507774	37.909991
1958.304680	330407.921891	37.915008
1960.098389	331033.697558	37.920026
1962.005914	331668.002793	37.925044
1963.915075	332293.821490	37.930061
1966.028312	332928.154535	37.935079
1968.062185	333550.206612	37.940096
1970.596999	334172.143481	37.945114
1972.255599	334812.952154	37.950132
1974.571184	335433.184426	37.955149
1976.466816	336056.068019	37.960167
1978.593675	336690.684393	37.965184
1980.592595	337311.657574	37.970202
1982.309639	337946.732429	37.975220
1984.604116	338562.666545	37.980237
1987.021584	339190.299904	37.985255
1988.527257	339811.908002	37.990272
1990.779854	340437.040158	37.995290
1992.848561	341070.037911	38.000308
1994.704002	341681.209023	38.005325
1996.797874	342297.231787	38.010343
1998.632852	342931.386283	38.015360
2001.043824	343541.655509	38.020378
2002.966859	344175.093807	38.025396
2004.677067	344794.929663	38.030413
2007.147408	345409.657445	38.035431
2008.706835	346027.014762	38.040448
2010.730556	346621.166809	38.045466
2012.988402	347230.652169	38.050484
2014.639262	347815.942411	38.055501
2016.842054	348410.574724	38.060519
2018.762602	349014.331118	38.065536
2020.637528	349607.403017	38.070554
2022.530414	350210.386577	38.075572
2024.764019	350803.078843	38.080589
2026.779666	351424.728352	38.085607
2028.489335	352031.143140	38.090624
2030.516123	352632.371232	38.095642
2032.191816	353265.647357	38.100660
2033.818596	353881.388083	38.105677
2036.065031	354517.317386	38.110695
2037.546499	355159.529411	38.115712
2039.612164	355790.445324	38.120730
2041.547866	356436.648054	38.125748
2043.449862	357086.347812	38.130765
2045.602489	357744.648084	38.135783
2047.317060	358402.705659	38.140800
2049.418623	359052.595102	38.145818
2051.161013	359735.414865	38.150836
2053.135241	360411.334598	38.155853
2055.286355	361085.412394	38.160871
2057.332293	361770.785851	38.165888
2059.597100	362453.193755	38.170906
2061.497079	363145.594775	38.175924
2063.423183	363829.049343	38.180941
2065.846909	364522.201889	38.185959
2067.888224	365225.171718	38.190976
2070.049550	365923.060671	38.195994
2071.996943	366614.579622	38.201012
2074.075494	367326.509649	38.206029
2076.214355	368026.468784	38.211047
2078.266314	368725.515937	38.216064
2080.661317	369435.806062	38.221082
2082.608698	370139.460096	38.226100
2084.860256	370857.634700	38.231117
2086.788897	371556.521335	38.236135
2088.973123	372284.950947	38.241152
2091.491999	372988.784891	38.246170
2093.417193	373706.854950	38.251188
2095.401871	374423.252107	38.256205
2098.050338	375126.793840	38.261223
2100.342168	375840.879527	38.266240
2102.138650	376546.511333	38.271258
2104.377605	377261.210438	38.276276
2106.569050	377971.895775	38.281293
2109.112902	378682.000951	38.286311
2110.908446	379400.633587	38.291328
2113.057569	380111.661393	38.296346
2115.208986	380829.925765	38.301364
2117.054115	381542.849671	38.306381
2119.451059	382248.947863	38.311399
2121.381238	382971.994484	38.316416
2123.668267	383685.914625	38.321434
2125.655513	384402.784289	38.326452
2127.722953	385119.650174	38.331469
2129.717028	385834.103656	38.336487
2132.026180	386564.638595	38.341504
2134.277926	387280.056572	38.346522
2136.461419	388001.148281	38.351540
2138.148231	388724.992591	38.356557
2140.450110	389450.949406	38.361575
2142.451201	390180.361079	38.366592
2144.863219	390906.899333	38.371610
2146.938914	391628.456976	38.376628
2148.830973	392355.477629	38.381645
2151.306849	393055.871551	38.386663
2153.160119	393756.554785	38.391680
2155.567232	394449.475829	38.396698
2157.471165	395159.191744	38.401716
2159.488529	395860.888448	38.406733
2161.819314	396558.816557	38.411751
2164.051268	397268.833259	38.416768
2165.851700	397968.766855	38.421786
2168.095770	398673.780232	38.426804
2170.265453	399388.570603	38.431821
2172.646632	400108.097797	38.436839
2174.383728	400823.810859	38.441856
2176.556679	401543.184320	38.446874
2178.867744	402273.235181	38.451892
2180.776819	403002.117299	38.456909
2182.654821	403732.885986	38.461927
2184.719591	404481.315355	38.466944
2186.776427	405225.824115	38.471962
2189.251173	405967.076922	38.476980
2190.887832	406727.398684	38.481997
2193.309148	407484.529735	38.487015
2195.658814	408257.383730	38.492032
2197.833238	409021.454136	38.497050
2200.037121	409784.738083	38.502068
2201.958010	410565.703020	38.507085
2204.585504	411324.972113	38.512103
2206.020577	412110.126194	38.517120
2208.623509	412888.073358	38.522138
2211.149821	413676.344145	38.527156
2213.006742	414464.245769	38.532173
2215.848892	415237.980502	38.537191
2217.825898	416027.866342	38.542208
2219.661677	416830.667198	38.547226
2221.941672	417627.570287	38.552244
2224.114044	418429.708255	38.557261
2227.151294	419231.348927	38.562279
2229.138747	420032.352420	38.567296
2231.496535	420831.243549	38.572314
2233.663750	421632.318162	38.577332
2235.958531	422435.244897	38.582349
2238.467481	423236.743016	38.587367
2240.677460	424041.251919	38.592384
2242.546680	424849.436327	38.597402
2245.411384	425643.151224	38.602420
2247.681946	426455.621076	38.607437
2249.901599	427257.844865	38.612455
2252.124487	428070.420008	38.617472
2254.248798	428871.744852	38.622490
2256.852019	429689.365923	38.627508
2258.845081	430496.023769	38.632525
2261.360874	431303.681395	38.637543
2263.765627	432124.389233	38.642560
2266.098275	432934.551743	38.647578
2268.593783	433743.494970	38.652596
2270.270516	434548.394705	38.657613
2272.736282	435355.970347	38.662631
2274.983631	436171.954845	38.667648
2276.894078	436979.919028	38.672666
2279.956330	437796.216863	38.677684
2281.884331	438613.026620	38.682701
2284.465123	439422.159164	38.687719
2286.791945	440237.123485	38.692736
2288.662062	441051.829778	38.697754
2291.022927	441860.201703	38.702772
2293.341680	442683.375435	38.707789
2295.756301	443499.115872	38.712807
2298.136370	444313.920954	38.717824
2300.175621	445125.514064	38.722842
2302.501638	445912.797903	38.727860
2304.148909	446701.632049	38.732877
2306.392540	447491.451699	38.737895
2308.742616	448292.099839	38.742912
2311.043010	449083.115838	38.747930
2313.371131	449883.606544	38.752948
2315.654938	450698.185105	38.757965
2317.671965	451503.065846	38.762983
2319.762855	452313.163044	38.768000
2321.974996	453133.980337	38.773018
2324.318321	453948.776457	38.778036
2326.357650	454777.901014	38.783053
2328.817795	455610.613974	38.788071
2330.905308	456457.410995	38.793088
2333.095528	457301.880741	38.798106
2335.551001	458142.682006	38.803124
2337.904119	458998.985986	38.808141
2340.143647	459851.177460	38.813159
2342.177806	460719.189367	38.818176
2344.580639	461579.773038	38.823194
2347.256113	462448.665367	38.828212
2349.381301	463321.350731	38.833229
2351.529707	464196.520798	38.838247
2354.032294	465077.607760	38.843264
2356.658920	465969.298142	38.848282
2358.944549	466845.085078	38.853300
2361.370460	467745.116036	38.858317
2364.178377	468632.004875	38.863335
2366.219046	469521.101592	38.868352
2368.406396	470421.753927	38.873370
2371.103559	471313.387270	38.878388
2373.268152	472236.440662	38.883405
2375.536403	473140.082892	38.888423
2378.459478	474041.350883	38.893440
2380.308730	474965.484202	38.898458
2383.112537	475857.541093	38.903476
2385.316122	476774.100792	38.908493
2387.796131	477690.266371	38.913511
2390.451069	478599.185812	38.918528
2392.808390	479531.037185	38.923546
2395.589802	480445.550664	38.928564
2397.818918	481355.160523	38.933581
2400.414428	482269.663124	38.938599
2403.203643	483178.432241	38.943616
2405.309408	484101.051639	38.948634
2407.884318	485013.347672	38.953652
2410.043341	485919.960831	38.958669
2412.482010	486846.118728	38.963687
2414.853340	487761.436648	38.968704
2417.436612	488685.959512	38.973722
2420.192329	489594.758281	38.978740
2422.319233	490528.041274	38.983757
2424.952383	491450.693177	38.988775
2427.368884	492376.258550	38.993792
2429.380915	493305.776968	38.998810
2432.246783	494221.883592	39.003828
2434.824321	495154.185386	39.008845
2437.293230	496087.059427	39.013863
2439.707571	497005.260087	39.018880
2441.861663	497937.528942	39.023898
2444.731243	498861.707966	39.028916
2447.007525	499793.802976	39.033933
2449.423256	500724.107863	39.038951
2452.043600	501636.118842	39.043968
2454.211885	502566.966305	39.048986
2456.399908	503497.102280	39.054004
2459.099566	504428.361827	39.059021
2461.297171	505342.657462	39.064039
2463.741095	506251.717903	39.069056
2466.099790	507161.951531	39.074074
2468.618873	508051.486503	39.079092
2471.385408	508962.912436	39.084109
2473.423841	509855.350871	39.089127
2476.035839	510758.432422	39.094144
2478.240942	511674.786751	39.099162
2480.812964	512585.331980	39.104180
2483.060925	513496.130183	39.109197
2485.379263	514412.710194	39.114215
2487.713358	515340.774410	39.119232
2490.436887	516273.153703	39.124250
2492.759178	517209.372856	39.129268
2495.006494	518143.179715	39.134285
2497.583429	519083.072787	39.139303
2500.138574	520029.511744	39.144320
2502.589232	520987.496049	39.149338
2505.066735	521942.443810	39.154356
2507.659813	522896.405897	39.159373
2509.902336	523861.698292	39.164391
2512.295469	524827.155946	39.169408
2514.756880	525808.403848	39.174426
2517.322003	526774.916506	39.179444
2519.890552	527757.529552	39.184461
2522.277667	528750.379064	39.189479
2524.954477	529739.791346	39.194496
2527.349855	530729.989214	39.199514
2529.747284	531732.050664	39.204532
2532.346025	532732.147884	39.209549
2534.998087	533734.936077	39.214567
2537.890436	534740.534561	39.219584
2540.028692	535751.471850	39.224602
2542.856822	536757.544474	39.229620
2545.322866	537774.173401	39.234637
2547.751713	538788.773957	39.239655
2550.795359	539813.212982	39.244672
2553.265381	540847.382245	39.249690
2555.734684	541858.587457	39.254708
2558.517429	542892.505087	39.259725
2560.777192	543920.749286	39.264743
2563.741886	544933.612974	39.269760
2566.503242	545972.838808	39.274778
2569.238103	546998.363701	39.279796
2572.415899	548013.733305	39.284813
2574.423102	549035.807720	39.289831
2577.479521	550063.414624	39.294848
2579.789263	551088.403144	39.299866
2582.637073	552110.410870	39.304884
2584.961346	553141.073393	39.309901
2587.798690	554171.019934	39.314919
2590.585461	555194.262357	39.319936
2593.154219	556222.789523	39.324954
2595.686150	557249.686039	39.329972
2598.575179	558266.496202	39.334989
2601.230523	559303.413545	39.340007
2603.769355	560324.645341	39.345024
2606.268993	561354.796207	39.350042
2608.929609	562373.287195	39.355060
2611.603028	563401.792075	39.360077
2613.737670	564431.911859	39.365095
2616.656542	565458.255317	39.370112
2618.900137	566503.609342	39.375130
2621.388656	567522.729795	39.380148
2624.210888	568570.682678	39.385165
2626.723289	569603.691431	39.390183
2629.484170	570635.571763	39.395200
2631.776836	571694.449283	39.400218
2634.294481	572720.077045	39.405236
2637.018753	573745.135882	39.410253
2639.174275	574749.029072	39.415271
2641.697795	575765.827161	39.420288
2644.417475	576784.968734	39.425306
2646.945115	577799.092078	39.430324
2649.559944	578830.123897	39.435341
2651.995524	579849.061143	39.440359
2654.356275	580881.619139	39.445376
2657.090451	581920.548587	39.450394
2659.886646	582967.704209	39.455412
2661.977169	584008.969661	39.460429
2664.366236	585070.402943	39.465447
2667.299585	586131.402978	39.470464
2669.818425	587189.571059	39.475482
2672.170828	588269.678668	39.480500
2674.921475	589340.501538	39.485517
2677.203894	590429.548129	39.490535
2680.372127	591523.661038	39.495552
2682.784545	592630.675363	39.500570
2685.351177	593744.174299	39.505588
2688.103686	594839.051615	39.510605
2690.337877	595970.279814	39.515623
2693.497648	597093.933385	39.520640
2696.082332	598219.176358	39.525658
2698.314871	599356.387378	39.530676
2701.202084	600498.085807	39.535693
2703.642091	601647.605903	39.540711
2706.337794	602782.500828	39.545728
2709.080733	603946.109234	39.550746
2711.733150	605108.512982	39.555764
2714.284832	606278.371978	39.560781
2717.026940	607449.680377	39.565799
2719.637425	608629.845900	39.570816
2722.662303	609807.267854	39.575834
2724.998866	611005.090858	39.580852
2728.376992	612191.158924	39.585869
2730.663414	613389.084661	39.590887
2733.471129	614580.743943	39.595904
2735.972848	615792.327542	39.600922
2738.503104	617000.973339	39.605940
2741.784344	618199.163487	39.610957
2744.674699	619424.280934	39.615975
2747.713481	620626.993771	39.620992
2750.082553	621837.480487	39.626010
2752.816596	623061.514052	39.631028
2755.786121	624268.281431	39.636045
2758.776599	625506.984717	39.641063
2761.552817	626712.509920	39.646080
2764.349222	627935.228089	39.651098
2766.831041	629159.006296	39.656116
2769.929129	630379.595258	39.661133
2772.752155	631614.668655	39.666151
2775.576471	632825.183007	39.671168
2778.768475	634063.901682	39.676186
2781.497881	635289.971364	39.681204
2784.462546	636512.963190	39.686221
2787.285728	637733.887991	39.691239
2789.896532	638950.662011	39.696256
2792.341566	640183.484331	39.701274
2795.032606	641407.338345	39.706292
2798.018385	642629.999801	39.711309
2800.767152	643872.353258	39.716327
2803.801621	645098.350883	39.721344
2806.641932	646329.068572	39.726362
2809.426325	647572.258597	39.731380
2812.349672	648800.666428	39.736397
2814.791573	650041.563337	39.741415
2817.564044	651247.465916	39.746432
2820.942289	652450.182515	39.751450
2823.343304	653646.387452	39.756468
2826.170451	654837.893774	39.761485
2828.753309	656030.840493	39.766503
2831.089476	657234.690157	39.771520
2833.911365	658422.276123	39.776538
2836.657630	659634.328195	39.781556
2839.255740	660866.019308	39.786573
2842.079662	662077.106391	39.791591
2844.774361	663302.348387	39.796608
2847.755865	664536.942760	39.801626
2850.244771	665785.343161	39.806644
2852.733282	667020.146692	39.811661
2855.283825	668275.127460	39.816679
2858.168374	669540.184089	39.821696
2860.891453	670814.199974	39.826714
2863.439276	672096.626152	39.831732
2866.557458	673384.352305	39.836749
2868.858328	674677.604401	39.841767
2871.826470	675974.593812	39.846784
2875.311434	677286.824117	39.851802
2877.615948	678601.448733	39.856820
2880.665461	679910.198608	39.861837
2883.866348	681234.635233	39.866855
2886.263712	682558.665552	39.871872
2889.108432	683888.638727	39.876890
2891.732647	685240.353594	39.881908
2894.942978	686589.735032	39.886925
2897.547771	687950.631754	39.891943
2900.718321	689305.174327	39.896960
2903.424002	690673.634301	39.901978
2905.830944	692049.873830	39.906996
2908.794531	693425.809432	39.912013
2912.063414	694802.771606	39.917031
2914.713194	696181.506657	39.922048
2917.614603	697578.779602	39.927066
2920.840093	698985.495359	39.932084
2923.764737	700379.294563	39.937101
2926.635994	701774.218565	39.942119
2929.605124	703174.552629	39.947136
2932.715727	704569.285988	39.952154
2935.804245	705989.163568	39.957172
2939.209207	707401.225863	39.962189
2942.064294	708799.477476	39.967207
2945.128417	710201.972247	39.972224
2948.202068	711617.107218	39.977242
2950.770333	713035.554903	39.982260
2953.946013	714433.224274	39.987277
2956.828588	715848.524936	39.992295
2959.776860	717269.464231	39.997312
2963.131771	718690.689138	40.002330
2965.818205	720108.122336	40.007348
2968.987328	721529.338956	40.012365
2971.857321	722959.409274	40.017383
2974.633933	724376.790156	40.022400
2977.965230	725796.109217	40.027418
2980.770527	727230.835810	40.032436
2983.694986	728648.838158	40.037453
2986.873832	730077.666764	40.042471
2989.706111	731519.439092	40.047488
2992.852411	732936.755045	40.052506
2995.535277	734367.179800	40.057524
2998.689037	735799.098909	40.062541
3001.748870	737235.713136	40.067559
3004.443404	738681.110197	40.072576
3007.484263	740103.985620	40.077594
3010.612800	741549.923863	40.082612
3013.455013	742971.379371	40.087629
3016.613936	744383.058424	40.092647
3019.318712	745778.880356	40.097664
3022.181852	747173.835674	40.102682
3025.148335	748586.316211	40.107700
3027.804116	749985.040500	40.112717
3030.622913	751390.481305	40.117735
3033.892616	752811.305224	40.122752
3036.831861	754220.347906	40.127770
3039.513838	755653.892448	40.132788
3042.311215	757089.955352	40.137805
3045.257444	758528.233397	40.142823
3048.261043	759984.831593	40.147840
3050.853806	761434.378189	40.152858
3053.715505	762903.574140	40.157876
3056.707904	764374.723926	40.162893
3059.162872	765854.770549	40.167911
3062.325676	767350.385308	40.172928
3065.474811	768859.366424	40.177946
3068.182402	770377.696300	40.182964
3071.055815	771887.678362	40.187981
3074.248374	773421.270343	40.192999
3077.061972	774959.712172	40.198016
3080.366504	776505.605971	40.203034
3083.052811	778070.076013	40.208052
3086.429393	779617.751467	40.213069
3089.269419	781186.677430	40.218087
3092.233955	782767.310436	40.223104
3095.636832	784337.321551	40.228122
3098.537468	785924.332830	40.233140
3101.841665	787506.953651	40.238157
3105.004028	789107.283759	40.243175
3108.258693	790697.289382	40.248192
3111.381217	792300.383293	40.253210
3114.088092	793908.176913	40.258228
3117.357203	795521.239066	40.263245
3120.663477	797135.685421	40.268263
3123.567752	798767.934871	40.273280
3126.776024	800376.700943	40.278298
3129.927056	802019.007819	40.283316
3132.973476	803652.820848	40.288333
3136.352361	805293.868057	40.293351
3139.564738	806939.242639	40.298368
3142.961775	808575.196042	40.303386
3146.086471	810220.378348	40.308404
3149.512064	811867.993741	40.313421
3152.902229	813504.076334	40.318439
3156.022931	815148.252965	40.323456
3159.204268	816787.524700	40.328474
3162.091227	818433.909919	40.333492
3165.525207	820075.405968	40.338509
3169.099347	821726.180235	40.343527
3171.889020	823374.330236	40.348544
3175.001677	825025.329952	40.353562
3178.276092	826674.668813	40.358580
3181.619455	828325.724436	40.363597
3184.803054	829975.364741	40.368615
3187.651261	831645.391168	40.373632
3191.132493	833297.789673	40.378650
3194.299711	834959.650500	40.383668
3197.358284	836610.926979	40.388685
3200.776515	838278.554188	40.393703
3204.199631	839938.934190	40.398720
3207.645472	841591.387232	40.403738
3210.514659	843261.445283	40.408756
3213.611165	844924.899557	40.413773
3217.343102	846585.476760	40.418791
3220.434991	848256.213305	40.423808
3223.459831	849893.972937	40.428826
3226.689527	851521.459700	40.433844
3229.696926	853137.099998	40.438861
3233.186119	854745.541628	40.443879
3236.260801	856363.626713	40.448896
3239.732206	857959.295784	40.453914
3242.475625	859590.165931	40.458932
3245.573504	861214.821371	40.463949
3249.092528	862831.509671	40.468967
3252.171260	864466.252010	40.473984
3255.369299	866098.691796	40.479002
3258.377079	867747.476510	40.484020
3261.594412	869396.839037	40.489037
3264.719051	871048.472666	40.494055
3267.809943	872717.848101	40.499072
3271.155182	874372.684408	40.504090
3273.979421	876053.839085	40.509108
3277.200282	877748.663515	40.514125
3280.431285	879425.985159	40.519143
3283.538254	881139.376132	40.524160
3287.134827	882844.745293	40.529178
3290.307918	884571.511855	40.534196
3293.564757	886299.778477	40.539213
3296.939893	888022.779660	40.544231
3300.361301	889742.556400	40.549248
3303.859671	891485.535705	40.554266
3307.121923	893226.383862	40.559284
3310.543451	894982.581354	40.564301
3313.791906	896722.170279	40.569319
3317.171305	898481.628704	40.574336
3320.199378	900231.157871	40.579354
3323.724793	901986.512236	40.584372
3327.357809	903758.721445	40.589389
3330.152039	905533.489724	40.594407
3333.705209	907301.314796	40.599424
3337.067978	909084.282524	40.604442
3340.841255	910869.299416	40.609460
3344.074752	912655.364603	40.614477
3347.332498	914428.932364	40.619495
3350.787150	916231.568493	40.624512
3354.432850	918014.856166	40.629530
3357.580915	919809.829348	40.634548
3361.107192	921595.606436	40.639565
3365.021924	923395.786538	40.644583
3368.065660	925186.782613	40.649600
3371.534066	926985.832248	40.654618
3375.174127	928774.762023	40.659636
3378.652770	930585.338395	40.664653
3381.987384	932364.489314	40.669671
3385.196069	934170.437083	40.674688
3388.797415	935963.644889	40.679706
3392.266298	937760.661881	40.684724
3395.424019	939562.849923	40.689741
3399.279283	941362.388381	40.694759
3402.681408	943166.251284	40.699776
3405.959220	944954.700862	40.704794
3409.851425	946758.088928	40.709812
3413.137689	948563.044267	40.714829
3416.756789	950352.519275	40.719847
3420.177394	952155.898416	40.724864
3423.896868	953977.374919	40.729882
3427.563325	955806.382178	40.734900
3430.836425	957644.456830	40.739917
3434.427548	959473.584755	40.744935
3437.653686	961304.928163	40.749952
3441.389182	963130.037076	40.754970
3444.771489	964958.042929	40.759988
3447.916288	966775.256110	40.765005
3451.436318	968585.023716	40.770010
3455.145130	970358.985379	40.775015
3458.492341	972055.698985	40.780020
3461.852562	973694.624075	40.785024
3465.112225	975258.335234	40.790029
3468.614589	976725.635705	40.795034
3471.466612	978133.571365	40.800039
3474.227084	979463.050934	40.805044
3477.385951	980725.178533	40.810048
3480.272299	981895.510372	40.815053
3483.041258	982983.056032	40.820058
3485.475178	984006.828776	40.825063
3488.030356	984942.689941	40.830068
3490.244093	985824.120122	40.835072
3492.278841	986626.832078	40.840077
3494.610648	987355.949241	40.845082
3496.695523	988020.072774	40.850087
3498.746687	988626.502720	40.855092
3500.610724	989183.179430	40.860096
3502.130728	989670.647206	40.865101
3504.428176	990099.461215	40.870106
3505.651866	990481.050923	40.875111
3507.035536	990797.387187	40.880116
3508.734545	991072.234841	40.885120
3509.720021	991304.015246	40.890125
3511.060095	991501.815438	40.895130
3512.210349	991645.069916	40.900135
3513.309849	991749.546058	40.905140
3514.797202	991823.261607	40.910144
3515.508691	991866.604359	40.915149
3516.242020	991869.017190	40.920154
3517.096999	991845.295157	40.925159
3518.015526	991788.041724	40.930164
3518.745171	991694.081742	40.935168
3519.418798	991589.897410	40.940173
3520.365320	991458.867470	40.945178
3520.871551	991301.107557	40.950183
3521.559984	991120.898413	40.955188
3522.159128	990906.684941	40.960192
3522.636897	990699.890603	40.965197
3523.161496	990446.979057	40.970202
3523.495299	990195.549770	40.975207
3524.380407	989923.256077	40.980212
3524.659812	989630.383076	40.985216
3524.991137	989328.127716	40.990221
3525.478114	989012.279253	40.995226
3525.764561	988684.551570	41.000231
3525.949176	988339.856161	41.005236
3526.412606	987981.247552	41.010240
3526.532770	987619.162315	41.015245
3526.872143	987230.199240	41.020250
3527.411752	986841.469186	41.025255
3527.575349	986448.873090	41.030260
3527.587987	986052.958331	41.035264
3527.630135	985651.548392	41.040269
3528.044183	985226.245023	41.045274
3528.103571	984813.749240	41.050279
3528.100493	984384.451611	41.055284
3528.526699	983943.341447	41.060288
3528.567439	983508.115838	41.065293
3528.614495	983078.028431	41.070298
3528.774818	982622.415952	41.075303
3529.262076	982165.932338	41.080308
3529.128152	981710.685937	41.085312
3529.030339	981253.347126	41.090317
3529.421024	980774.216640	41.095322
3529.793672	980308.035207	41.100327
3529.196305	979824.203326	41.105332
3529.638184	979340.061566	41.110336
3529.515939	978862.222329	41.115341
3529.930001	978369.896651	41.120346
3529.531868	977888.798182	41.125351
3529.762668	977398.958793	41.130356
3529.639811	976898.193354	41.135360
3529.423909	976411.273906	41.140365
3529.545212	975914.778965	41.145370
3529.583523	975423.434012	41.150375
3529.219583	974932.699525	41.155380
3529.784718	974437.957970	41.160384
3529.408637	973941.764718	41.165389
3529.975686	973437.259119	41.170394
3529.674252	972936.469544	41.175399
3529.802317	972429.405544	41.180404
3529.718604	971915.095498	41.185408
3529.467171	971421.890249	41.190413
3529.574915	970899.536280	41.195418
3529.760107	970400.694325	41.200423
3529.344992	969895.353997	41.205428
3529.700145	969368.417939	41.210432
3529.199502	968867.501228	41.215437
3529.231971	968348.742954	41.220442
3529.251925	967853.522688	41.225447
3529.240233	967352.980348	41.230452
3529.533318	966836.097570	41.235456
3529.370728	966336.078689	41.240461
3529.832365	965814.475882	41.245466
3529.438895	965299.232045	41.250471
3529.020972	964780.519319	41.255476
3529.225187	964267.238444	41.260480
3528.658056	963750.415650	41.265485
3528.546489	963243.362531	41.270490
3528.743971	962748.456422	41.275495
3528.970030	962236.068054	41.280500
3528.996345	961720.434359	41.285504
3528.824303	961208.607874	41.290509
3528.871865	960697.385543	41.295514
3528.888632	960183.477331	41.300519
3528.554209	959673.892830	41.305524
3528.530272	959177.540335	41.310528
3528.577310	958670.058261	41.315533
3528.298028	958156.018009	41.320538
3528.376016	957653.930460	41.325543
3528.494673	957137.283160	41.330548
3528.227780	956628.006482	41.335552
3528.164719	956127.868297	41.340557
3528.195847	955610.510398	41.345562
3528.276808	955112.417877	41.350567
3528.038401	954609.332969	41.355572
3528.193974	954098.194219	41.360576
3527.652170	953598.602419	41.365581
3527.914832	953095.793632	41.370586
3528.024224	952585.019168	41.375591
3527.611160	952091.352685	41.380596
3527.776749	951605.888465	41.385600
3527.829228	951125.465947	41.390605
3527.562366	950627.928271	41.395610
3527.437353	950137.685008	41.400615
3527.374436	949653.029301	41.405620
3527.124025	949171.420444	41.410624
3527.115973	948691.544510	41.415629
3527.078116	948196.699036	41.420634
3526.940516	947726.515720	41.425639
3526.928868	947253.396995	41.430644
3526.886997	946774.113056	41.435648
3526.598301	946287.453314	41.440653
3526.660663	945808.732441	41.445658
3526.642800	945329.022751	41.450663
3526.437923	944856.864629	41.455668
3526.426252	944373.330253	41.460672
3526.410197	943906.896328	41.465677
3526.135162	943437.780859	41.470682
3526.295151	942967.018408	41.475687
3526.200519	942502.003603	41.480692
3525.839377	942024.151574	41.485696
3526.203297	941559.743292	41.490701
3525.812046	941083.726167	41.495706
3526.029730	940613.124010	41.500711
3525.335348	940157.869900	41.505716
3525.488455	939686.427803	41.510720
3525.102463	939241.012167	41.515725
3525.082119	938769.324006	41.520730
3525.235646	938326.330097	41.525735
3525.002144	937875.019719	41.530740
3525.049772	937409.814279	41.535744
3524.454115	936958.580421	41.540749
3524.921596	936512.408039	41.545754
3524.793761	936059.485028	41.550759
3524.496624	935607.222366	41.555764
3524.546980	935157.166142	41.560768
3524.267086	934713.746417	41.565773
3524.005530	934274.892327	41.570778
3523.929982	933830.980746	41.575783
3523.783252	933409.309656	41.580788
3523.787153	932967.231774	41.585792
3523.441027	932534.965581	41.590797
3524.240928	932094.219364	41.595802
3523.885107	931663.899519	41.600807
3523.751754	931224.578719	41.605812
3523.957987	930798.128522	41.610816
3523.089754	930360.297472	41.615821
3523.402271	929922.139720	41.620826
3523.444730	929498.109025	41.625831
3523.250580	929073.795327	41.630836
3523.123514	928633.778800	41.635840
3522.800206	928214.989446	41.640845
3522.961803	927796.375517	41.645850
3523.146079	927375.418989	41.650855
3522.652767	926954.444803	41.655860
3522.778017	926523.917828	41.660864
3522.863882	926109.604699	41.665869
3522.606912	925692.913123	41.670874
3522.579386	925272.979307	41.675879
3522.350194	924865.830959	41.680884
3522.370530	924442.651972	41.685888
3522.003941	924038.155267	41.690893
3522.253511	923618.911635	41.695898
3522.295031	923212.650994	41.700903
3521.881302	922800.183908	41.705908
3521.798890	922385.322481	41.710912
3521.447196	921993.556769	41.715917
3521.601946	921577.151380	41.720922
3521.605510	921190.174371	41.725927
3521.385926	920789.064782	41.730932
3521.348935	920394.918582	41.735936
3520.895682	920003.794927	41.740941
3521.127440	919604.351234	41.745946
3521.478535	919207.071726	41.750951
3521.152352	918810.644592	41.755956
3520.864883	918416.010746	41.760960
3520.475778	918031.278781	41.765965
3520.779508	917650.544499	41.770970
3520.603202	917260.332507	41.775975
3520.383969	916871.447405	41.780980
3520.555316	916491.327756	41.785984
3520.261940	916114.146702	41.790989
3520.302498	915734.188397	41.795994
3520.282786	915353.732090	41.800999
3519.937739	914979.370071	41.806004
3520.201407	914596.599372	41.811008
3520.013812	914220.233225	41.816013
3520.142128	913843.885485	41.821018
3520.143197	913471.482436	41.826023
3519.663824	913105.587857	41.831028
3520.014549	912719.974281	41.836032
3519.765341	912354.955187	41.841037
3519.599894	911982.285835	41.846042
3519.468943	911610.934635	41.851047
3519.601275	911247.128235	41.856052
3519.441984	910886.044388	41.861056
3518.985794	910528.166418	41.866061
3519.267438	910152.793647	41.871066
3518.995232	909807.272780	41.876071
3518.686770	909456.241395	41.881076
3519.184432	909092.714741	41.886080
3518.829969	908732.968317	41.891085
3518.565600	908376.558363	41.896090
3518.423726	908028.301518	41.901095
3518.382254	907673.641715	41.906100
3518.402569	907323.385222	41.911104
3518.285738	906983.255882	41.916109
3517.965156	906638.509663	41.921114
3518.318632	906300.672308	41.926119
3518.024966	905959.255493	41.931124
3518.299806	905610.199555	41.936128
3518.155431	905269.005211	41.941133
3517.976864	904929.628725	41.946138
3518.049896	904591.637416	41.951143
3517.811813	904241.808409	41.956148
3518.029981	903892.364804	41.961152
3517.628075	903570.215531	41.966157
3517.643041	903225.781904	41.971162
3517.323348	902892.770999	41.976167
3517.567193	902574.994230	41.981172
3517.681761	902238.108548	41.986176
3517.265915	901916.831664	41.991181
3516.976130	901573.794638	41.996186
3517.192646	901256.913057	42.001191
3517.268888	900937.912640	42.006196
3516.848592	900599.858153	42.011200
3516.671726	900285.690147	42.016205
3516.590556	899964.729256	42.021210
3516.512113	899647.805597	42.026215
3516.387152	899338.308144	42.031220
3516.601908	899018.210340	42.036224
3516.765680	898709.693221	42.041229
3516.724812	898384.192702	42.046234
3516.622157	898079.452150	42.051239
3516.349007	897767.091618	42.056244
3516.480119	897455.130268	42.061248
3516.360540	897142.709956	42.066253
3516.099926	896836.189396	42.071258
3516.462241	896520.563568	42.076263
3515.711986	896204.813579	42.081268
3516.515156	895906.667540	42.086272
3515.982853	895603.410677	42.091277
3515.831378	895290.313707	42.096282
3515.990417	894993.868857	42.101287
3515.745779	894696.798472	42.106292
3516.142782	894383.174571	42.111296
3515.485773	894090.490200	42.116301
3515.538353	893785.783379	42.121306
3515.417159	893496.073656	42.126311
3514.969714	893198.861869	42.131316
3515.328104	892894.733825	42.136320
3515.162044	892602.762362	42.141325
3515.023327	892311.835124	42.146330
3514.874629	892022.635335	42.151335
3514.814472	891736.500911	42.156340
3515.082846	891450.491477	42.161344
3514.913543	891166.377458	42.166349
3514.958274	890891.209032	42.171354
3514.774724	890603.200645	42.176359
3514.569686	890322.919690	42.181364
3514.768132	890034.723103	42.186368
3514.685738	889757.780046	42.191373
3514.280084	889484.166175	42.196378
3514.341816	889203.496407	42.201383
3514.191841	888926.040669	42.206388
3514.244567	888649.215461	42.211392
3514.209977	888389.034402	42.216397
3513.975191	888106.134457	42.221402
3514.051140	887843.781703	42.226407
3513.420060	887573.597906	42.231412
3513.762251	887312.628768	42.236416
3513.893103	887057.586499	42.241421
3513.830192	886790.659895	42.246426
3514.082898	886519.894031	42.251431
3513.467955	886268.714755	42.256436
3513.289205	886009.708567	42.261440
3513.431556	885761.092937	42.266445
3513.587349	885496.684357	42.271450
3513.718773	885236.527577	42.276455
3513.097108	884978.225938	42.281460
3513.029254	884721.080252	42.286464
3513.134831	884469.704251	42.291469
3513.393273	884222.262282	42.296474
3513.158814	883965.013729	42.301479
3512.693735	883721.349393	42.306484
3512.802486	883474.965513	42.311488
3512.813285	883232.267567	42.316493
3512.637059	882991.333653	42.321498
3513.013131	882738.482320	42.326503
3512.908384	882495.094698	42.331508
3512.755405	882251.607994	42.336512
3512.531160	882007.638522	42.341517
3512.399436	881769.843441	42.346522
3512.674878	881519.183900	42.351527
3512.696794	881276.305826	42.356532
3512.321780	881035.033207	42.361536
3512.686067	880813.103398	42.366541
3512.203750	880561.268075	42.371546
3512.597419	880322.261720	42.376551
3512.363259	880094.298776	42.381556
3512.151105	879861.090518	42.386560
3511.848794	879621.394999	42.391565
3512.068344	879397.594149	42.396570
3511.880977	879171.913495	42.401575
3511.593924	878942.751494	42.406580
3511.751195	878701.585804	42.411584
3511.685547	878483.903264	42.416589
3511.292455	878259.578408	42.421594
3511.224153	878048.859179	42.426599
3511.409889	877831.207988	42.431604
3511.112582	877607.133273	42.436608
3511.228245	877407.121218	42.441613
3510.893631	877196.124497	42.446618
3511.453115	876970.817984	42.451623
3511.359783	876759.475022	42.456628
3511.431214	876543.831159	42.461632
3511.197995	876324.254152	42.466637
3510.670699	876116.741184	42.471642
3511.147097	875908.861620	42.476647
3510.927572	875705.453163	42.481652
3510.725567	875475.172455	42.486656
3510.745072	875276.461685	42.491661
3511.004107	875080.711242	42.496666
3511.087314	874868.786623	42.501671
3510.608239	874665.967085	42.506676
3511.022523	874454.846010	42.511680
3510.756550	874252.559162	42.516685
3510.800484	874046.237364	42.521690
3510.734220	873844.194674	42.526695
3510.894705	873639.973607	42.531700
3510.395830	873438.085365	42.536704
3509.927261	873230.461495	42.541709
3510.394845	873030.049369	42.546714
3510.450243	872834.452353	42.551719
3510.137953	872645.507013	42.556724
3510.201618	872449.798956	42.561728
3510.236296	872259.134738	42.566733
3510.266651	872072.734528	42.571738
3510.419062	871864.087335	42.576743
3510.167037	871677.915359	42.581748
3510.464439	871464.863571	42.586752
3510.249338	871281.875514	42.591757
3510.193873	871088.956661	42.596762
3510.083462	870898.272794	42.601767
3510.154104	870698.526965	42.606772
3509.859209	870504.464008	42.611776
3509.778588	870320.259609	42.616781
3509.326449	870133.490025	42.621786
3509.598688	869942.227265	42.626791
3509.353251	869771.234129	42.631796
3509.319960	869580.980845	42.636800
3509.213144	869411.313593	42.641805
3509.440005	869236.538503	42.646810
3509.587467	869063.810092	42.651815
3509.227786	868885.917737	42.656820
3509.723752	868702.927711	42.661824
3509.419827	868522.879485	42.666829
3509.179191	868349.514799	42.671834
3509.380930	868167.722028	42.676839
3508.794867	867990.811355	42.681844
3509.038392	867811.039956	42.686848
3509.257633	867647.483520	42.691853
3509.157376	867479.314164	42.696858
3509.274042	867303.918281	42.701863
3508.963882	867129.073161	42.706868
3509.217279	866956.557979	42.711872
3509.200523	866787.967066	42.716877
3508.598570	866620.439044	42.721882
3508.717070	866449.776844	42.726887
3508.834595	866281.246736	42.731892
3509.054142	866110.364021	42.736896
3508.785244	865940.625378	42.741901
3508.638777	865777.466890	42.746906
3508.773779	865616.103207	42.751911
3508.478100	865455.583276	42.756916
3508.646813	865298.673944	42.761920
3508.787653	865127.484923	42.766925
3508.577626	864970.143730	42.771930
3508.533977	864808.982195	42.776935
3508.372675	864653.276259	42.781940
3508.548693	864493.138781	42.786945
3508.330467	864336.462514	42.791949
3508.201938	864175.200906	42.796954
3508.408070	864015.823106	42.801959
3508.290842	863853.773770	42.806964
3508.482956	863700.608526	42.811969
3508.392387	863542.919003	42.816973
3508.189341	863387.090179	42.821978
3508.640713	863227.554059	42.826983
3508.299431	863082.235047	42.831988
3508.133115	862910.936731	42.836993
3508.223870	862763.692483	42.841997
3507.946695	862605.523402	42.847002
3508.634278	862447.094061	42.852007
3507.937397	862292.095953	42.857012
3507.734276	862145.857031	42.862017
3507.983475	861993.416806	42.867021
3507.889479	861850.068623	42.872026
3507.810173	861703.409863	42.877031
3507.886406	861550.403831	42.882036
3507.615310	861399.686869	42.887041
3507.778607	861253.268895	42.892045
3507.508588	861113.334569	42.897050
3507.783948	860966.988455	42.902055
3507.162644	860834.688052	42.907060
3507.064563	860685.771950	42.912065
3507.461503	860557.089160	42.917069
3507.074848	860421.727377	42.922074
3507.343283	860284.893550	42.927079
3507.471836	860154.204815	42.932084
3507.590160	860013.208993	42.937089
3507.604781	859877.769020	42.942093
3507.385947	859741.294967	42.947098
3507.809151	859593.724771	42.952103
3507.299108	859457.486816	42.957108
3507.617411	859313.038645	42.962113
3507.516353	859179.741469	42.967117
3507.214053	859041.029006	42.972122
3507.365635	858898.640587	42.977127
3507.346931	858766.001527	42.982132
3507.234488	858626.762152	42.987137
3506.898971	858492.321634	42.992141
3507.079828	858368.296358	42.997146
3507.572996	858229.045410	43.002151
3507.008241	858103.192513	43.007156
3506.822130	857959.281768	43.012161
3507.196733	857836.672690	43.017165
3506.936788	857707.940883	43.022170
3506.904582	857575.180984	43.027175
3506.624595	857451.991205	43.032180
3507.018428	857318.863765	43.037185
3507.018494	857196.984491	43.042189
3506.795767	857057.922165	43.047194
3507.093984	856934.432184	43.052199
3506.639439	856810.480078	43.057204
3506.841259	856683.109838	43.062209
3506.851624	856562.286336	43.067213
3506.715428	856448.586259	43.072218
3506.862544	856306.430210	43.077223
3506.733924	856184.843905	43.082228
3506.445063	856063.670751	43.087233
3506.949654	855939.445756	43.092237
3506.919571	855816.863032	43.097242
3506.789833	855690.110606	43.102247
3506.813029	855566.833059	43.107252
3506.707857	855440.752528	43.112257
3506.528777	855319.838532	43.117261
3506.410356	855195.214666	43.122266
3506.582731	855078.811259	43.127271
3506.317314	854960.337043	43.132276
3506.603917	854837.779959	43.137281
3506.554369	854736.197496	43.142285
3506.231590	854619.380445	43.147290
3506.481828	854488.550908	43.152295
3506.612511	854371.946402	43.157300
3506.403999	854247.610171	43.162305
3506.294602	854131.527266	43.167309
3506.172241	854018.753237	43.172314
3506.456089	853903.963762	43.177319
3506.008998	853796.494618	43.182324
3506.251488	853675.770906	43.187329
3506.322865	853578.139853	43.192333
3505.858500	853459.280278	43.197338
3505.980540	853340.419134	43.202343
3505.996427	853238.995922	43.207348
3506.093706	853117.798575	43.212353
3505.966214	853011.820494	43.217357
3505.387429	852906.596321	43.222362
3505.951951	852791.837305	43.227367
3505.676069	852712.744487	43.232372
3505.438898	852596.556466	43.237377
3505.765847	852497.795482	43.242381
3505.559430	852407.200573	43.247386
3505.715250	852293.667828	43.252391
3505.494548	852194.992247	43.257396
3505.757257	852083.482392	43.262401
3505.763154	851977.269927	43.267405
3505.680107	851879.734889	43.272410
3505.728558	851766.210179	43.277415
3505.242366	851694.148681	43.282420
3505.379079	851588.005356	43.287425
3505.487928	851474.757442	43.292429
3505.514684	851384.303892	43.297434
3505.533918	851284.016484	43.302439
3505.552968	851185.966900	43.307444
3505.816292	851079.404562	43.312449
3505.610792	850982.849280	43.317453
3505.708187	850892.182189	43.322458
3505.583459	850780.712773	43.327463
3505.676373	850690.627715	43.332468
3505.591757	850585.672216	43.337473
3505.487563	850480.328665	43.342477
3505.290484	850390.287033	43.347482
3505.765053	850294.874938	43.352487
3505.333964	850191.917473	43.357492
3505.248563	850098.931785	43.362497
3505.246920	850004.470144	43.367501
3505.202953	849914.688558	43.372506
3505.190919	849809.513239	43.377511
3504.992794	849725.305395	43.382516
3505.021220	849632.975715	43.387521
3505.461022	849538.629061	43.392525
3504.915875	849459.539157	43.397530
3505.324433	849358.961792	43.402535
3505.307707	849275.594534	43.407540
3505.259890	849170.414326	43.412545
3505.188800	849073.709882	43.417549
3505.089348	848995.806844	43.422554
3505.285270	848914.932132	43.427559
3505.074876	848812.402508	43.432564
3505.283011	848712.042547	43.437569
3505.324975	848632.845423	43.442573
3505.142437	848540.047297	43.447578
3505.458190	848435.379246	43.452583
3504.855824	848348.589376	43.457588
3505.096546	848249.482948	43.462593
3505.257140	848169.870763	43.467597
3504.780477	848088.609102	43.472602
3505.029562	847993.491219	43.477607
3504.999065	847914.004675	43.482612
3504.735244	847824.813742	43.487617
3504.953242	847741.192492	43.492621
3504.949093	847655.755728	43.497626
3505.135168	847562.687518	43.502631
3505.055070	847479.306728	43.507636
3504.664711	847389.448468	43.512641
3504.995717	847301.516023	43.517645
3504.897242	847221.155041	43.522650
3504.838032	847129.971937	43.527655
3505.003722	847061.256861	43.532660
3504.670628	846964.660383	43.537665
3504.933748	846877.999793	43.542669
3504.817719	846795.492715	43.547674
3504.934284	846712.361616	43.552679
3504.831787	846621.762863	43.557684
3504.502181	846539.482477	43.562689
3504.609439	846457.713671	43.567693
3504.832441	846377.288902	43.572698
3504.939989	846297.369335	43.577703
3504.371626	846215.903574	43.582708
3504.697900	846140.038585	43.587713
3505.043901	846046.044511	43.592717
3504.604976	845966.405657	43.597722
3504.665249	845882.006019	43.602727
3504.797617	845807.923039	43.607732
3505.202597	845721.905265	43.612737
3504.864441	845628.407467	43.617741
3504.406072	845560.266037	43.622746
3504.928456	845475.687353	43.627751
3505.008068	845383.871272	43.632756
3504.212595	845319.875932	43.637761
3504.840992	845228.844286	43.642765
3504.769191	845150.206637	43.647770
3504.618717	845071.873351	43.652775
3504.605129	844998.779495	43.657780
3504.315160	844908.381833	43.662785
3504.736646	844823.811015	43.667789
3504.432920	844750.664614	43.672794
3504.525063	844670.239567	43.677799
3504.414589	844604.467135	43.682804
3504.627250	844522.070974	43.687809
3504.900765	844448.728491	43.692813
3504.351721	844367.722926	43.697818
3504.339099	844285.653206	43.702823
3504.485244	844226.950092	43.707828
3504.122931	844137.722969	43.712833
3504.487631	844052.956214	43.717837
3504.658595	843994.539279	43.722842
3504.477315	843908.008453	43.727847
3504.276700	843828.888130	43.732852
3504.254045	843762.020151	43.737857
3504.389579	843688.691563	43.742861
3504.037291	843610.080895	43.747866
3504.215289	843533.819001	43.752871
3504.299441	843471.707103	43.757876
3504.341354	843402.387530	43.762881
3504.343740	843324.689740	43.767885
3504.221441	843259.197683	43.772890
3504.369306	843184.496360	43.777895
3504.603021	843114.947051	43.782900
3504.310631	843035.734411	43.787905
3504.370164	842954.415426	43.792909
3504.349344	842892.607610	43.797914
3504.402674	842806.315509	43.802919
3504.641643	842734.031253	43.807924
3504.456656	842657.038604	43.812929
3504.531912	842582.927125	43.817933
3503.927006	842521.894412	43.822938
3503.764135	842449.283106	43.827943
3504.212617	842379.982834	43.832948
3503.979715	842312.549134	43.837953
3503.844111	842244.026132	43.842957
3503.789771	842182.704423	43.847962
3504.180181	842109.608039	43.852967
3504.094617	842053.458080	43.857972
3503.920648	841981.330770	43.862977
3504.165908	841902.454135	43.867981
3503.865812	841843.412358	43.872986
3503.877243	841771.934692	43.877991
3504.360312	841719.149759	43.882996
3504.038085	841646.604254	43.888001
3503.958286	841571.921401	43.893005
3503.808914	841517.727506	43.898010
3503.837370	841449.851489	43.903015
3504.154431	841384.999013	43.908020
3503.966940	841333.686604	43.913025
3504.114270	841252.282526	43.918029
3504.118785	841197.816742	43.923034
3504.310434	841116.549902	43.928039
3504.066610	841052.274046	43.933044
3503.967380	840991.679627	43.938049
3504.001791	840920.334859	43.943053
3504.073119	840861.320259	43.948058
3503.942826	840777.566444	43.953063
3503.588509	840723.594581	43.958068
3503.748906	840658.321616	43.963073
3503.796494	840598.040601	43.968077
3503.526191	840534.690396	43.973082
3503.896560	840478.890261	43.978087
3503.755457	840415.761413	43.983092
3503.322893	840359.165953	43.988097
3503.453776	840300.721533	43.993101
3503.369043	840251.480432	43.998106
3503.700309	840183.394678	44.003111
3503.470157	840138.907178	44.008116
3503.270568	840076.857505	44.013121
3503.549699	840018.190987	44.018125
3503.556107	839974.248593	44.023130
3503.645137	839913.564098	44.028135
3503.820027	839855.400957	44.033140
3503.362167	839791.732847	44.038145
3503.789752	839719.139303	44.043149
3503.567664	839677.134601	44.048154
3503.422699	839614.632467	44.053159
3503.283222	839559.493541	44.058164
3503.466581	839510.056209	44.063169
3503.833630	839445.565895	44.068173
3503.423412	839400.517607	44.073178
3503.480120	839341.442530	44.078183
3503.824694	839295.000996	44.083188
3503.426597	839225.708241	44.088193
3503.362650	839160.651970	44.093197
3503.399171	839112.894133	44.098202
3503.406221	839058.507148	44.103207
3503.583808	839003.116057	44.108212
3503.587607	838946.143453	44.113217
3503.647390	838883.063848	44.118221
3503.512230	838835.429774	44.123226
3503.647562	838769.263546	44.128231
3503.532809	838717.820463	44.133236
3503.441327	838676.519329	44.138241
3503.599292	838615.908671	44.143245
3503.150851	838562.470542	44.148250
3503.465887	838515.052583	44.153255
3503.394510	838454.722084	44.158260
3502.976838	838398.106711	44.163265
3503.350452	838354.043855	44.168269
3503.314914	838299.511065	44.173274
3503.333889	838251.554536	44.178279
3503.372487	838201.301596	44.183284
3503.409787	838149.097122	44.188289
3503.191416	838095.909876	44.193293
3503.104393	838048.505912	44.198298
3503.307216	837983.296105	44.203303
3503.491168	837939.164067	44.208308
3503.493668	837878.279306	44.213313
3503.309942	837819.961536	44.218317
3503.094197	837783.700080	44.223322
3503.197790	837725.773190	44.228327
3503.068438	837678.812538	44.233332
3502.817894	837641.385110	44.238337
3503.201502	837601.120855	44.243341
3502.674766	837564.079994	44.248346
3502.863070	837502.575580	44.253351
3503.068320	837464.388977	44.258356
3503.025128	837419.168625	44.263361
3502.997438	837358.625411	44.268365
3502.725485	837336.324550	44.273370
3503.030116	837274.945152	44.278375
3502.894201	837231.397623	44.283380
3502.854775	837191.249279	44.288385
3503.399975	837138.708914	44.293389
3503.234224	837100.190931	44.298394
3503.505889	837057.404527	44.303399
3503.614487	836994.834938	44.308404
3503.154958	836958.852927	44.313409
3503.646338	836899.342082	44.318413
3503.124938	836837.557857	44.323418
3503.427033	836789.494917	44.328423
3503.210641	836743.761589	44.333428
3503.167537	836697.755410	44.338433
3503.207069	836638.902129	44.343437
3503.173453	836605.629289	44.348442
3503.025402	836553.686302	44.353447
3503.233793	836503.880003	44.358452
3503.149622	836455.097453	44.363457
3503.328671	836405.002440	44.368461
3503.203620	836351.199731	44.373466
3503.474001	836302.845582	44.378471
3502.862415	836262.736883	44.383476
3502.930124	836206.266095	44.388481
3503.285875	836159.214360	44.393485
3502.928126	836123.845265	44.398490
3502.558518	836075.741243	44.403495
3502.865718	836029.086950	44.408500
3502.896758	835986.040239	44.413505
3503.107338	835943.695667	44.418509
3502.722073	835905.597065	44.423514
3502.906331	835855.448099	44.428519
3502.849743	835816.806803	44.433524
3502.731104	835769.293551	44.438529
3503.042001	835738.594752	44.443533
3502.717647	835710.440588	44.448538
3502.743496	835656.314368	44.453543
3502.809904	835624.679249	44.458548
3502.616514	835583.618935	44.463553
3503.367498	835531.861165	44.468557
3503.040773	835499.460537	44.473562
3503.037888	835454.902928	44.478567
3503.235383	835403.967386	44.483572
3502.858593	835365.766567	44.488577
3503.043411	835301.703741	44.493581
3503.283630	835268.671678	44.498586
3503.143435	835221.157919	44.503591
3503.074266	835168.263391	44.508596
3503.110293	835130.725255	44.513601
3503.264385	835073.693393	44.518605
3503.132404	835025.493530	44.523610
3502.709625	834985.443333	44.528615
3503.067298	834938.089491	44.533620
3502.908923	834896.238077	44.538625
3503.251661	834842.443256	44.543629
3503.182409	834811.558619	44.548634
3502.801355	834773.940687	44.553639
3502.702745	834728.417619	44.558644
3502.809170	834683.836651	44.563649
3503.303597	834636.360437	44.568653
3502.659822	834595.709680	44.573658
3502.635498	834550.319544	44.578663
3503.011410	834511.257455	44.583668
3502.552508	834478.580577	44.588673
3502.668488	834430.628269	44.593677
3502.620511	834406.376623	44.598682
3502.175481	834372.281361	44.603687
3502.723761	834332.701665	44.608692
3502.666421	834292.586935	44.613697
3502.960938	834262.860057	44.618701
3502.856077	834225.827983	44.623706
3502.741173	834172.005331	44.628711
3502.818165	834129.231491	44.633716
3502.792434	834094.138197	44.638721
3502.921169	834037.638288	44.643725
3502.853497	834012.851437	44.648730
3502.998191	833962.547778	44.653735
3503.055744	833931.589206	44.658740
3502.787010	833876.324950	44.663745
3503.177673	833833.204566	44.668749
3502.903746	833796.588410	44.673754
3502.680271	833756.692980	44.678759
3503.134391	833716.392758	44.683764
3502.896994	833674.399958	44.688769
3503.257032	833626.401451	44.693773
3502.622390	833588.574268	44.698778
3502.820489	833547.826990	44.703783
3502.673266	833500.838681	44.708788
3502.579232	833459.162590	44.713793
3502.773284	833420.953789	44.718797
3502.771830	833394.152036	44.723802
3502.795952	833352.114047	44.728807
3503.070484	833312.817300	44.733812
3502.816659	833278.733555	44.738817
3503.034376	833237.004665	44.743821
3502.564059	833192.557218	44.748826
3502.732334	833148.004251	44.753831
3502.803128	833117.234874	44.758836
3502.856887	833085.491711	44.763841
3503.006720	833032.299430	44.768845
3502.924562	832997.453574	44.773850
3503.176868	832944.146038	44.778855
3503.005122	832905.896810	44.783860
3502.622936	832868.365561	44.788865
3502.948607	832819.194940	44.793869
3502.938117	832790.732141	44.798874
3502.707701	832744.044970	44.803879
3502.920787	832708.025933	44.808884
3502.915934	832664.816435	44.813889
3502.580556	832618.096820	44.818893
3502.662970	832591.277913	44.823898
3502.831640	832558.536705	44.828903
3503.122680	832509.906526	44.833908
3502.433370	832472.277092	44.838913
3502.793717	832430.665974	44.843917
3502.879567	832392.761881	44.848922
3502.728161	832347.865443	44.853927
3502.746571	832313.829400	44.858932
3502.724089	832277.407322	44.863937
3502.746522	832224.864151	44.868941
3502.791468	832189.162899	44.873946
3502.997349	832150.016880	44.878951
3502.750218	832113.630892	44.883956
3502.608100	832080.791980	44.888961
3502.761832	832038.675254	44.893965
3502.819694	831998.429608	44.898970
3502.715441	831953.620323	44.903975
3502.557138	831918.195216	44.908980
3502.538772	831885.334922	44.913985
3502.803317	831846.470389	44.918989
3502.514817	831826.057532	44.923994
3502.512826	831788.310863	44.928999
3503.160397	831750.163959	44.934004
3502.742397	831723.130904	44.939009
3502.877579	831670.906484	44.944013
3502.395014	831635.875085	44.949018
3502.609858	831598.824084	44.954023
3502.743851	831565.058057	44.959028
3502.716322	831526.483893	44.964033
3502.529415	831482.466306	44.969037
3502.529477	831461.858252	44.974042
3502.901586	831414.183174	44.979047
3502.846691	831377.224182	44.984052
3502.801266	831337.675138	44.989057
3502.791196	831286.692437	44.994061
3502.586529	831249.659721	44.999066
3502.477201	831214.173852	45.004071
3502.428041	831177.017426	45.009076
3502.262289	831149.940411	45.014081
3502.526842	831103.550528	45.019085
3502.456720	831083.783068	45.024090
3502.004377	831049.671421	45.029095
3502.692893	831018.399580	45.034100
3502.307047	830993.604716	45.039105
3502.229275	830964.851936	45.044109
3502.250700	830937.352486	45.049114
3502.581515	830895.736374	45.054119
3502.472743	830867.574335	45.059124
3502.512331	830844.564691	45.064129
3502.439895	830805.114522	45.069133
3502.250505	830778.577083	45.074138
3502.298491	830750.681747	45.079143
3502.744452	830707.384898	45.084148
3502.643568	830672.822636	45.089153
3502.510130	830648.717472	45.094157
3502.340390	830610.698532	45.099162
3502.350791	830578.999051	45.104167
3502.834378	830538.136936	45.109172
3502.529141	830512.057065	45.114177
3502.555482	830468.290499	45.119181
3502.413155	830440.669395	45.124186
3502.536405	830406.850264	45.129191
3502.729986	830365.106833	45.134196
3502.327291	830349.836624	45.139201
3502.688138	830307.137245	45.144205
3502.569426	830272.478099	45.149210
3502.405241	830235.188695	45.154215
3502.957615	830205.400691	45.159220
3502.898921	830168.972718	45.164225
3503.032917	830123.769606	45.169229
3502.651515	830093.548802	45.174234
3502.483061	830050.641876	45.179239
3502.859235	830006.277259	45.184244
3502.581400	829974.280395	45.189249
3502.605520	829928.654415	45.194253
3502.657904	829905.199716	45.199258
3502.401468	829878.669638	45.204263
3502.460416	829843.637005	45.209268
3502.642370	829819.183712	45.214273
3502.810425	829776.268376	45.219277
3502.286692	829741.233498	45.224282
3502.453292	829703.788844	45.229287
3502.612803	829673.818897	45.234292
3502.467214	829647.220761	45.239297
3502.250390	829607.054372	45.244301
3502.367194	829583.978689	45.249306
3502.485311	829547.811191	45.254311
3502.595317	829515.113126	45.259316
3501.984660	829480.481952	45.264321
3502.457733	829442.154857	45.269325
3502.994699	829421.012211	45.274330
3502.345612	829391.369586	45.279335
3502.803410	829346.791622	45.284340
3502.689192	829320.675485	45.289345
3502.728390	829283.884464	45.294349
3502.715854	829251.009856	45.299354
3502.398636	829213.690946	45.304359
3502.058389	829180.234904	45.309364
3502.345114	829151.853700	45.314369
3502.403142	829125.073322	45.319373
3502.294540	829098.613402	45.324378
3502.392864	829061.078594	45.329383
3502.457352	829024.184231	45.334388
3502.294714	828998.270188	45.339393
3502.581911	828957.088529	45.344397
3502.539458	828932.962001	45.349402
3502.094690	828914.812973	45.354407
3502.479735	828874.640601	45.359412
3502.517532	828854.018048	45.364417
3502.525571	828824.264562	45.369421
3502.429675	828789.984580	45.374426
3502.359634	828752.133747	45.379431
3502.330295	828719.894338	45.384436
3502.112064	828691.985169	45.389441
3502.342772	828659.311773	45.394445
3502.468434	828633.593054	45.399450
3502.482527	828601.199335	45.404455
3502.749891	828560.018435	45.409460
3502.514991	828535.482433	45.414465
3502.540616	828490.188109	45.419469
3502.465445	828470.560092	45.424474
3502.351140	828430.858114	45.429479
3502.458091	828405.727868	45.434484
3502.464772	828363.660384	45.439489
3502.660714	828341.202410	45.444493
3502.385669	828303.675894	45.449498
3502.454885	828274.642692	45.454503
3502.616923	828245.740644	45.459508
3502.115662	828209.325747	45.464513
3502.448475	828177.414858	45.469517
3502.757809	828150.051615	45.474522
3502.104502	828119.622120	45.479527
3502.492675	828091.366166	45.484532
3502.056238	828058.311077	45.489537
3502.607576	828027.145213	45.494541
3501.989693	827997.588797	45.499546
3502.098328	827979.052810	45.504551
3502.475523	827948.159564	45.509556
3502.358164	827923.210998	45.514561
3502.149883	827888.065284	45.519565
3502.211377	827868.119766	45.524570
3501.987818	827843.383838	45.529575
3502.409164	827817.124566	45.534580
3502.303763	827787.775933	45.539585
3502.489949	827752.662221	45.544589
3502.541514	827732.082712	45.549594
3502.557645	827704.765911	45.554599
3502.504342	827657.231113	45.559604
3502.262782	827632.008717	45.564609
3502.430658	827599.486956	45.569613
3502.331756	827581.521533	45.574618
3501.962976	827543.615171	45.579623
3502.268055	827517.471580	45.584628
3502.273889	827500.856876	45.589633
3502.465645	827457.629174	45.594637
3502.654711	827435.462406	45.599642
3502.485734	827406.415720	45.604647
3502.437147	827367.087356	45.609652
3502.211709	827351.732010	45.614657
3502.453979	827308.397268	45.619661
3502.440639	827273.802513	45.624666
3502.228305	827243.491727	45.629671
3502.638511	827213.860096	45.634676
3502.304523	827191.827546	45.639681
3502.593125	827149.168247	45.644685
3502.576754	827126.350141	45.649690
3502.355205	827090.078367	45.654695
3502.352417	827041.455679	45.659700
3502.404600	827022.877412	45.664705
3502.390334	826988.379034	45.669709
3502.450395	826967.991190	45.674714
3502.523595	826940.759527	45.679719
3502.601530	826902.433757	45.684724
3502.615108	826867.881287	45.689729
3502.402002	826845.925389	45.694733
3502.402129	826805.950319	45.699738
3502.490537	826770.700832	45.704743
3502.436682	826744.906510	45.709748
3502.119350	826729.320489	45.714753
3502.471867	826681.271894	45.719757
3502.350786	826665.555645	45.724762
3502.584004	826622.217847	45.729767
3502.692908	826595.760799	45.734772
3502.044399	826574.071207	45.739777
3502.463672	826537.886270	45.744781
3502.637065	826502.230362	45.749786
3502.180220	826470.050269	45.754791
3502.549526	826437.391797	45.759796
3502.223617	826417.163572	45.764801
3502.347491	826375.210582	45.769805
3502.275932	826346.192001	45.774810
3502.334353	826304.444834	45.779815
3502.353853	826210.946464	45.784820
3502.380896	826074.337902	45.789825
3502.387870	825875.705824	45.794829
3502.360804	825612.700724	45.799834
3502.480136	825297.065412	45.804839
3502.524343	824905.169117	45.809844
3502.048115	824468.945943	45.814849
3502.018444	823954.150945	45.819853
3501.809595	823398.273548	45.824858
3501.709804	822776.121581	45.829863
3501.950163	822082.454385	45.834868
3501.095503	821346.929961	45.839873
3501.071961	820527.931917	45.844877
3501.139083	819646.686136	45.849882
3500.853863	818705.198212	45.854887
3500.706021	817677.719070	45.859892
3500.040321	816596.816860	45.864897
3499.664803	815440.744381	45.869901
3499.460213	814220.352527	45.874906
3499.322371	812930.188095	45.879911
3498.478689	811550.403338	45.884916
3498.124283	810121.361837	45.889921
3497.658120	808610.839423	45.894925
3497.336238	807028.690592	45.899930
3496.921780	805368.336230	45.904935
3496.731281	803633.199478	45.909940
3495.796462	801824.022546	45.914945
3495.563820	799932.660171	45.919949
3495.140676	797977.255406	45.924954
3494.226815	795950.589330	45.929959
3493.894979	793835.336116	45.934964
3493.090797	791663.129644	45.939969
3492.496813	789398.133165	45.944973
3491.729871	787059.200108	45.949978
3491.020065	784672.923978	45.954983
3490.444772	782184.108752	45.959988
3489.809572	779632.295909	45.964993
3488.739749	777003.998504	45.969997
3488.110717	774313.619999	45.975002
3487.415536	771539.999745	45.980007
3486.440863	768692.596544	45.985012
3485.496039	765801.008820	45.990017
3484.475740	762811.601427	45.995021
3483.687450	759753.818303	46.000026
3482.750363	756636.829015	46.005031
3482.166755	753450.908103	46.010036
3480.967232	750190.014054	46.015041
3479.827801	746850.887192	46.020045
3479.146816	743448.007916	46.025050
3478.154120	739972.578494	46.030055
3476.946924	736424.252864	46.035060
3476.042389	732811.823427	46.040065
3474.840483	729149.235608	46.045069
3473.697802	725391.135388	46.050074
3472.336968	721582.369825	46.055079
3471.574179	717692.197874	46.060084
3470.003208	713741.746052	46.065089
3468.728915	709715.028115	46.070093
3467.601851	705633.139780	46.075098
3466.076777	701482.297953	46.080103
3465.036684	697263.970074	46.085108
3463.332721	692977.723580	46.090113
3462.245124	688635.116761	46.095117
3460.996911	684217.748103	46.100122
3459.283224	679748.548712	46.105127
3458.362896	675198.903288	46.110132
3456.535160	670587.201942	46.115137
3455.051920	665907.039322	46.120141
3453.721326	661170.355101	46.125146
3451.946643	656356.071749	46.130151
3450.563151	651472.062873	46.135156
3448.753615	646550.385082	46.140161
3447.226272	641546.590574	46.145165
3445.798836	636481.989400	46.150170
3443.499278	631363.547534	46.155175
3442.275312	626189.099883	46.160180
3440.313619	620949.432302	46.165185
3438.705145	615645.964747	46.170189
3436.858417	610278.543385	46.175194
3434.441624	604873.920396	46.180199
3433.476121	599382.200531	46.185204
3431.089022	593857.373533	46.190209
3429.334886	588266.385753	46.195213
3427.389961	582608.121463	46.200218
3425.075504	576906.810023	46.205223
3422.864663	571131.969703	46.210228
3420.921858	565319.572040	46.215233
3419.031868	559449.910679	46.220237
3416.880094	553517.875389	46.225242
3414.533417	547541.223864	46.230247
3412.768142	541503.940129	46.235252
3410.266065	535420.853847	46.240257
3407.766996	529277.761338	46.245261
3405.568217	523091.263670	46.250266
3403.173925	516850.387899	46.255271
3400.924893	510562.908911	46.260276
3398.526463	504231.109212	46.265281
3396.028775	497837.090233	46.270285
3393.394166	491404.027684	46.275290
3390.763413	484934.504698	46.280295
3388.397043	478408.102694	46.285300
3385.431061	471837.181285	46.290305
3382.928651	465239.173203	46.295309
3380.624010	458588.673074	46.300314
3377.686187	451904.194730	46.305319
3375.016090	445155.150736	46.310324
3372.012651	438385.085481	46.315329
3369.403896	431577.140314	46.320333
3366.579743	424729.228366	46.325338
3363.301489	417843.212838	46.330343
3360.619004	410928.824720	46.335348
3357.481492	403975.171560	46.340353
3354.614742	396992.071688	46.345357
3351.515642	389967.752337	46.350362
3347.945927	382921.248174	46.355367
3344.706979	375835.210226	46.360372
3341.590445	368730.690855	46.365377
3338.348127	361591.403290	46.370381
3334.617774	354455.331768	46.375386
3331.809934	347277.478132	46.380391
3328.398377	340065.697344	46.385396
3324.840085	332850.812248	46.390401
3321.241527	325607.060436	46.395405
3317.561897	318342.041001	46.400410
3314.206695	311088.489615	46.405415
3310.551580	303791.965188	46.410420
3306.994891	296500.765194	46.415425
3303.336656	289169.996053	46.420429
3299.584134	281836.239214	46.425434
3295.409282	274518.439791	46.430439
3291.741686	267153.075706	46.435444
3287.954632	259805.136028	46.440449
3283.977773	252449.669123	46.445453
3280.348256	245073.898976	46.450458
3276.028700	237708.095813	46.455463
3272.065063	230325.928698	46.460468
3267.914274	222910.806657	46.465473
3263.589973	215499.244358	46.470477
3259.724971	208125.086034	46.475482
3254.913931	200774.510283	46.480487
3250.984239	193425.873110	46.485492
3246.125313	186078.589821	46.490497
3241.600052	178753.124347	46.495501
3237.225504	171440.345412	46.500506
3232.378573	164142.583377	46.505511
3228.192535	156860.553924	46.510516
3223.459117	149599.655064	46.515521
3219.143024	142353.581136	46.520525
3214.058331	135130.544384	46.525530
3208.943202	127939.079742	46.530535
3204.028033	120768.485081	46.535540
3199.033598	113624.523005	46.540545
3193.613965	106516.667730	46.545549
3187.998523	99449.773685	46.550554
3182.600300	92438.105804	46.555559
3177.459775	85447.434935	46.560564
3171.890423	78517.369324	46.565569
3165.955664	71641.353507	46.570573
3160.348232	64793.535622	46.575578
3153.988274	58046.020995	46.580583
3147.427720	51328.559622	46.585588
3140.297084	44709.031172	46.590593
3132.196874	38184.987487	46.595597
3120.118861	31871.708806	46.600602
3099.556297	25910.805172	46.605607
3079.795832	20184.435875	46.610612
3059.680786	14769.527892	46.615617
3036.461389	9777.891175	46.620621
3005.944697	5399.052416	46.625626
2970.430799	1666.123908	46.630631
2871.681093	304.773781	46.635636
2765.513300	306.918636	46.640641
2720.044454	312.675053	46.645645
2727.187080	298.634965	46.650650
2762.647427	300.176578	46.655655
2805.082300	276.900765	46.660660
2837.832074	273.183345	46.665665
2856.195691	280.125953	46.670669
2861.685218	283.612481	46.675674
2858.605801	290.650714	46.680679
2852.441086	281.492077	46.685684
2846.488826	275.850180	46.690689
2840.422979	276.222705	46.695693
2836.721315	267.982305	46.700698
2833.250228	277.625361	46.705703
2831.188976	274.497048	46.710708
2829.488471	268.365259	46.715713
2827.377838	263.349028	46.720717
2825.190262	259.067768	46.725722
2821.780597	267.011438	46.730727
2818.693593	264.604927	46.735732
2815.843174	261.500260	46.740737
2812.795394	263.263448	46.745741
2809.745364	257.798742	46.750746
2806.578980	253.596889	46.755751
2803.666582	254.608762	46.760756
2800.715185	260.412234	46.765761
2797.074096	254.213848	46.770765
2793.731965	248.216768	46.775770
2790.272438	255.639800	46.780775
2787.903567	253.432546	46.785780
2784.281635	245.351918	46.790785
2780.830683	247.342281	46.795789
2777.860450	248.630911	46.800794
2774.312865	253.615515	46.805799
2771.216437	243.121131	46.810804
2768.357836	245.372534	46.815809
2764.565901	241.840299	46.820813
2761.368321	240.448652	46.825818
2757.234306	248.427404	46.830823
2754.255998	250.013789	46.835828
2751.113369	237.820035	46.840833
2747.794630	255.028170	46.845837
2744.319287	250.357933	46.850842
2740.914422	235.362570	46.855847
2737.466506	246.755423	46.860852
2734.282023	235.291652	46.865857
2730.353837	242.130158	46.870861
2727.524616	238.911934	46.875866
2723.892745	241.300032	46.880871
2720.834643	237.562284	46.885876
2717.179977	232.832069	46.890881
2713.316129	240.529854	46.895885
2710.313629	231.471673	46.900890
2706.862840	234.753068	46.905895
2703.099984	232.561564	46.910900
2700.124129	237.629478	46.915905
2696.747780	238.366303	46.920909
2693.629203	230.092187	46.925914
2690.310713	240.485678	46.930919
2686.856267	231.933874	46.935924
2682.938351	233.284608	46.940929
2678.757354	236.040022	46.945933
2675.733417	235.313632	46.950938
2672.693479	238.308993	46.955943
2669.421601	230.765886	46.960948
2665.898359	233.131755	46.965953
2661.867365	234.739159	46.970957
2658.261636	219.357873	46.975962
2654.967499	232.214527	46.980967
2651.867597	227.573189	46.985972
2648.260402	227.590741	46.990977
2644.489560	227.417436	46.995981
2641.803371	224.417604	47.000986
2638.614487	229.184038	47.005991
2634.829225	224.882754	47.010996
2631.147252	222.601786	47.016001
2627.670194	229.997802	47.021005
2624.660870	226.925005	47.026010
2620.367853	219.928954	47.031015
2617.224464	226.100463	47.036020
2613.828687	224.617691	47.041025
2610.154837	224.182517	47.046029
2606.867159	218.460771	47.051034
2603.223298	225.477803	47.056039
2599.859725	223.726472	47.061044
2596.797757	218.898148	47.066049
2592.986202	221.819998	47.071053
2589.749361	221.545188	47.076058
2585.562648	225.850356	47.081063
2582.152891	216.096561	47.086068
2579.373390	214.230699	47.091073
2575.348752	223.899316	47.096077
2572.629424	217.161029	47.101082
2568.762533	219.487374	47.106087
2565.369055	216.807577	47.111092
2561.230395	212.734393	47.116097
2557.992856	217.012388	47.121101
2555.129595	214.720292	47.126106
2551.417333	217.890222	47.131111
2547.710192	213.249716	47.136116
2544.640791	208.967714	47.141121
2541.043907	218.084242	47.146125
2537.353501	215.700937	47.151130
2533.772424	211.852289	47.156135
2530.131465	211.412536	47.161140
2526.808367	213.498788	47.166145
2522.943646	212.818509	47.171149
2520.145891	206.952427	47.176154
2516.437469	213.282367	47.181159
2512.782512	214.060166	47.186164
2509.641049	209.722984	47.191169
2505.739585	210.075352	47.196173
2502.709218	208.281331	47.201178
2499.015842	200.270769	47.206183
2495.478058	211.317037	47.211188
2492.288270	210.564458	47.216193
2488.094965	204.223435	47.221197
2484.778162	203.723110	47.226202
2481.333241	213.390038	47.231207
2478.188087	212.197924	47.236212
2474.721449	213.155823	47.241217
2470.985494	212.899138	47.246221
2467.740616	200.991285	47.251226
2464.629949	208.717258	47.256231
2460.600916	199.174322	47.261236
2457.290610	200.980650	47.266241
2453.286157	200.112927	47.271245
2450.174043	192.331884	47.276250
2446.868656	206.723823	47.281255
2443.301269	198.987143	47.286260
2439.785461	201.475865	47.291265
2436.128587	217.852478	47.296269
2432.761655	203.907710	47.301274
2429.141796	192.426080	47.306279
2425.787994	202.747770	47.311284
2422.219368	200.814323	47.316289
2418.543123	204.300856	47.321293
2415.520022	197.668072	47.326298
2411.816231	201.226252	47.331303
2407.921445	208.695886	47.336308
2405.104390	196.521703	47.341313
2400.816086	193.745229	47.346317
2397.989734	196.224368	47.351322
2394.364772	191.951294	47.356327
2390.717205	198.555044	47.361332
2387.719786	193.765154	47.366337
2383.981473	200.748181	47.371341
2380.445529	190.976318	47.376346
2376.858443	189.252176	47.381351
2373.106495	190.747041	47.386356
2369.825237	193.373515	47.391361
2366.158283	185.223729	47.396365
2362.888689	185.902106	47.401370
2359.092581	186.974069	47.406375
2355.803742	198.057069	47.411380
2352.559323	193.486174	47.416385
2348.745562	186.816025	47.421389
2345.556807	188.182024	47.426394
2342.212837	197.597919	47.431399
2338.482458	192.553717	47.436404
2334.911348	197.300141	47.441409
2331.116795	190.964681	47.446413
2327.797728	186.832583	47.451418
2324.496631	198.458930	47.456423
2321.177515	196.602971	47.461428
2317.542835	189.474462	47.466433
2313.368284	196.150263	47.471437
2310.590580	190.279825	47.476442
2307.117724	186.479798	47.481447
2303.109602	193.668252	47.486452
2299.929067	190.472576	47.491457
2296.492184	184.420487	47.496461
2292.866437	193.046993	47.501466
2289.781339	192.626755	47.506471
2286.076926	189.877525	47.511476
2282.764573	189.163080	47.516481
2279.011590	187.714259	47.521485
2275.357812	191.018786	47.526490
2272.004925	187.924797	47.531495
2268.064000	188.457528	47.536500
2265.076888	181.621572	47.541505
2261.435060	181.391740	47.546509
2258.176658	178.237565	47.551514
2254.494996	184.035567	47.556519
2250.917205	181.546475	47.561524
2247.561303	188.176167	47.566529
2243.850462	185.511311	47.571533
2240.548581	189.075679	47.576538
2236.860668	188.205604	47.581543
2233.323241	185.135600	47.586548
2230.271107	183.257729	47.591553
2226.565183	185.393171	47.596557
2223.067123	181.619866	47.601562
2219.508856	185.406750	47.606567
2215.362555	178.958769	47.611572
2212.138037	178.138305	47.616577
2208.915246	176.644036	47.621581
2205.730835	178.555446	47.626586
2202.360756	182.780150	47.631591
2198.686209	176.875128	47.636596
2194.863366	173.798801	47.641601
2191.458633	180.317393	47.646605
2188.155267	174.028246	47.651610
2184.581708	182.622716	47.656615
2180.936320	188.831958	47.661620
2177.413206	181.574636	47.666625
2173.961072	184.337591	47.671629
2170.665392	179.408834	47.676634
2167.008328	173.193101	47.681639
2163.223112	183.109191	47.686644
2159.915184	176.243991	47.691649
2155.985763	185.005580	47.696653
2153.022204	179.977792	47.701658
2149.771517	190.886072	47.706663
2146.007330	187.986781	47.711668
2142.655255	178.614964	47.716673
2138.831387	181.866763	47.721677
2135.761066	173.142280	47.726682
2132.155100	185.910157	47.731687
2128.498931	183.124473	47.736692
2125.258871	173.041514	47.741697
2121.186497	191.689204	47.746701
2118.109422	174.480612	47.751706
2114.572269	181.083084	47.756711
2110.689808	181.826518	47.761716
2107.756829	175.738732	47.766721
2103.733212	180.064707	47.771725
2100.649250	180.439091	47.776730
2097.159535	179.328202	47.781735
2093.647174	176.051894	47.786740
2090.289251	177.054072	47.791745
2086.335139	177.561498	47.796749
2083.223644	174.340563	47.801754
2079.502493	177.509532	47.806759
2076.091347	177.824886	47.811764
2072.412798	179.503025	47.816769
2068.702932	184.410284	47.821773
2065.374190	175.990593	47.826778
2062.065167	183.570743	47.831783
2058.519474	178.261047	47.836788
2055.266759	180.034446	47.841793
2051.508703	190.712007	47.846797
2047.758056	178.357970	47.851802
2044.197528	178.080538	47.856807
2040.986024	177.837431	47.861812
2037.737640	170.565248	47.866817
2034.010393	180.755822	47.871821
2030.601754	177.471905	47.876826
2026.683582	176.218895	47.881831
2023.222626	176.934626	47.886836
2019.942217	170.177277	47.891841
2016.384591	180.434377	47.896845
2013.216791	169.000820	47.901850
2009.689833	172.073041	47.906855
2005.983793	171.489717	47.911860
2002.445447	172.593781	47.916865
1998.712951	168.405486	47.921869
1995.453340	164.544434	47.926874
1991.922663	163.202003	47.931879
1988.602918	170.210690	47.936884
1985.152555	173.569052	47.941889
1981.627783	172.766757	47.946893
1977.894091	167.775110	47.951898
1974.649877	173.698989	47.956903
1970.854374	175.349947	47.961908
1967.710286	172.717021	47.966913
1964.184152	171.413328	47.971917
1960.909479	170.579610	47.976922
1957.132057	172.726270	47.981927
1953.234930	176.196725	47.986932
1950.062757	167.622605	47.991937
1946.200423	169.508403	47.996941
1942.629238	173.643152	48.001946
1938.994756	167.496106	48.006951
1935.756805	180.654239	48.011956
1932.892825	167.391942	48.016961
1929.222698	176.737614	48.021965
1925.454745	166.632481	48.026970
1922.016554	169.427443	48.031975
1918.521957	171.522684	48.036980
1915.188835	166.990641	48.041985
1911.258649	175.023949	48.046989
1907.785879	165.525443	48.051994
1904.333030	169.357884	48.056999
1900.821575	169.231510	48.062004
1897.761045	165.221018	48.067009
1894.192166	166.587535	48.072013
1890.394952	163.156754	48.077018
1887.004803	165.672068	48.082023
1883.046311	173.600351	48.087028
1880.044265	172.452882	48.092033
1876.079081	172.055732	48.097037
1872.954058	164.949588	48.102042
1869.448081	165.595114	48.107047
1866.078216	171.428119	48.112052
1862.885379	165.218449	48.117057
1859.484191	165.442917	48.122061
1855.185906	166.101711	48.127066
1852.070257	166.850316	48.132071
1847.802297	161.890394	48.137076
1844.885144	154.663900	48.142081
1841.217194	167.146368	48.147085
1837.928310	169.213211	48.152090
1834.531466	167.269994	48.157095
1830.540587	162.725501	48.162100
1827.514686	163.547902	48.167105
1823.745232	161.865557	48.172109
1820.604677	170.070422	48.177114
1817.316133	166.108110	48.182119
1813.431294	174.291476	48.187124
1809.976559	161.146202	48.192129
1806.312966	162.912254	48.197133
1802.761152	171.843588	48.202138
1799.571225	161.857791	48.207143
1795.703224	162.417735	48.212148
1792.232579	159.916234	48.217153
1788.888368	167.601026	48.222157
1785.093306	160.388167	48.227162
1781.893519	163.923136	48.232167
1778.608044	171.282687	48.237172
1775.191031	160.597559	48.242177
1771.290336	163.412985	48.247181
1767.751054	161.877371	48.252186
1764.152005	164.704739	48.257191
1760.843652	172.311794	48.262196
1757.580620	156.384583	48.267201
1754.131396	162.746021	48.272205
1750.333511	159.760666	48.277210
1746.936932	164.058321	48.282215
1743.087305	168.166588	48.287220
1740.016756	161.594031	48.292225
1736.108755	157.998946	48.297229
1732.800543	155.188265	48.302234
1729.493785	157.749309	48.307239
1725.577258	161.382397	48.312244
1722.502551	162.505779	48.317249
1719.066064	163.779905	48.322253
1715.578073	158.686714	48.327258
1711.822051	153.156302	48.332263
1708.127592	158.283079	48.337268
1705.015379	153.073350	48.342273
1701.511852	168.640583	48.347277
1697.581955	159.139435	48.352282
1694.448519	154.096420	48.357287
1690.573732	160.757120	48.362292
1687.021560	159.467806	48.367297
1683.484035	165.689166	48.372301
1680.532749	156.126603	48.377306
1676.895466	150.004519	48.382311
1673.522224	162.124631	48.387316
1670.283722	154.309013	48.392321
1666.372424	162.086980	48.397325
1662.674225	155.263169	48.402330
1659.161562	159.892845	48.407335
1655.659625	164.544827	48.412340
1652.224713	158.989629	48.417345
1648.845608	153.891922	48.422349
1645.545506	153.450202	48.427354
1641.989116	154.076201	48.432359
1637.984836	152.303946	48.437364
1634.936597	150.939699	48.442369
1631.392751	163.554535	48.447373
1627.781383	156.383100	48.452378
1624.179284	147.009618	48.457383
1620.760933	149.917741	48.462388
1617.305112	150.599172	48.467393
1613.811264	151.429169	48.472397
1609.844160	146.958109	48.477402
1606.554134	151.833030	48.482407
1603.112160	163.463893	48.487412
1599.904564	142.871464	48.492417
1596.205091	145.710612	48.497421
1592.607271	145.072239	48.502426
1589.398514	152.600380	48.507431
1585.568428	160.012343	48.512436
1582.040461	146.759005	48.517441
1578.668857	145.333377	48.522445
1575.190726	145.563462	48.527450
1571.261160	147.964472	48.532455
1568.372121	149.059048	48.537460
1565.000917	148.541516	48.542465
1560.981628	157.573336	48.547469
1557.667553	150.376718	48.552474
1554.436728	141.216644	48.557479
1550.956145	158.399128	48.562484
1547.778706	153.640356	48.567489
1543.827496	154.717272	48.572493
1539.735552	155.268845	48.577498
1536.697131	152.247764	48.582503
1532.834947	150.969148	48.587508
1529.375464	148.050017	48.592513
1526.197715	153.925493	48.597517
1522.944226	146.554706	48.602522
1519.391261	150.263844	48.607527
1515.299204	154.442342	48.612532
1512.065323	149.971566	48.617537
1508.510461	152.930942	48.622541
1505.147373	158.966121	48.627546
1501.865384	142.736009	48.632551
1498.705756	146.542570	48.637556
1494.820712	145.677241	48.642561
1491.264838	156.524810	48.647565
1487.249011	147.038069	48.652570
1484.230507	148.772354	48.657575
1480.356637	142.727031	48.662580
1477.270655	150.321383	48.667585
1473.521482	144.646386	48.672589
1470.168136	146.734785	48.677594
1466.735253	148.793509	48.682599
1463.098757	149.067610	48.687604
1459.501160	149.359359	48.692609
1456.059447	150.280908	48.697613
1452.506013	145.294063	48.702618
1449.207095	146.180572	48.707623
1445.534123	153.160943	48.712628
1442.402444	149.217983	48.717633
1439.050529	142.725504	48.722637
1435.330365	154.025919	48.727642
1431.586795	153.789070	48.732647
1427.931546	153.950262	48.737652
1424.384249	147.632759	48.742657
1420.694737	151.446234	48.747661
1417.464907	150.051759	48.752666
1414.379917	147.864321	48.757671
1410.619775	148.591069	48.762676
1407.130007	149.607622	48.767681
1403.545635	147.661387	48.772685
1400.149293	151.396428	48.777690
1396.591797	145.982273	48.782695
1393.155601	147.571933	48.787700
1389.697815	151.534998	48.792705
1386.037332	151.654858	48.797709
1382.595136	150.966260	48.802714
1379.042449	144.508196	48.807719
1375.639802	146.017335	48.812724
1372.065385	142.981555	48.817729
1368.359294	152.525155	48.822733
1365.293980	146.116001	48.827738
1361.883898	145.194975	48.832743
1357.476515	146.994123	48.837748
1354.347020	139.327888	48.842753
1351.151328	140.667463	48.847757
1347.345385	147.099180	48.852762
1344.103137	146.229164	48.857767
1340.744094	142.729390	48.862772
1337.128592	138.515416	48.867777
1333.834847	137.464871	48.872781
1330.039389	146.516700	48.877786
1326.263927	143.103725	48.882791
1322.627186	147.525035	48.887796
1319.684855	146.167965	48.892801
1316.043259	146.396254	48.897805
1312.303712	148.333109	48.902810
1308.666265	141.777620	48.907815
1305.477594	146.427594	48.912820
1302.350575	144.755328	48.917825
1298.613802	143.728310	48.922829
1295.019884	146.488080	48.927834
1291.808886	143.646859	48.932839
1287.912812	155.192933	48.937844
1284.542322	140.051363	48.942849
1281.005905	147.295418	48.947853
1277.268830	140.398849	48.952858
1274.121916	141.533471	48.957863
1270.148863	145.808536	48.962868
1266.827355	142.095410	48.967873
1263.489268	131.731785	48.972877
1260.204622	144.694523	48.977882
1256.269938	139.581618	48.982887
1252.930989	148.122516	48.987892
1249.593122	142.968382	48.992897
1245.732251	143.842750	48.997901
1242.425220	143.905677	49.002906
1239.296324	137.254143	49.007911
1235.381569	148.020500	49.012916
1232.192517	137.443407	49.017921
1228.614260	146.977021	49.022925
1224.876451	140.518907	49.027930
1221.537749	137.585578	49.032935
1217.602786	151.403370	49.037940
1214.148520	137.943418	49.042945
1210.627883	143.819137	49.047949
1207.099618	148.967551	49.052954
1203.736430	135.374151	49.057959
1200.220032	144.388228	49.062964
1197.258995	136.136195	49.067969
1193.580889	143.497272	49.072973
1189.955800	141.506041	49.077978
1186.819027	134.268179	49.082983
1183.056525	148.215351	49.087988
1179.407964	144.872890	49.092993
1175.747533	134.937964	49.097997
1172.707050	139.340533	49.103002
1169.132889	136.267975	49.108007
1165.410052	142.714901	49.113012
1161.470326	137.149830	49.118017
1157.751846	141.016641	49.123021
1154.478888	144.759674	49.128026
1151.476841	140.208614	49.133031
1147.619440	140.248542	49.138036
1144.503636	144.188196	49.143041
1141.120466	135.002140	49.148045
1137.332312	133.709453	49.153050
1134.093701	131.895321	49.158055
1129.989343	142.676919	49.163060
1126.974721	133.121899	49.168065
1123.250623	132.601866	49.173069
1119.645550	135.258234	49.178074
1116.414682	135.062383	49.183079
1112.630365	143.870592	49.188084
1109.451533	138.831570	49.193089
1105.781437	132.538988	49.198093
1102.280663	135.599835	49.203098
1098.983096	130.419625	49.208103
1095.017212	145.979774	49.213108
1091.497913	136.511381	49.218113
1088.426296	135.762722	49.223117
1085.238044	133.756973	49.228122
1081.885073	132.859279	49.233127
1077.793046	132.811172	49.238132
1074.341966	135.445271	49.243137
1070.630556	136.182788	49.248141
1066.966937	135.360742	49.253146
1064.173492	133.836746	49.258151
1060.320443	139.557964	49.263156
1056.548323	129.845270	49.268161
1053.181730	129.833724	49.273165
1049.610249	136.953492	49.278170
1046.488199	129.811975	49.283175
1042.151468	136.575204	49.288180
1039.121333	133.821877	49.293185
1035.991445	133.130646	49.298189
1032.384587	141.657965	49.303194
1028.969668	139.702169	49.308199
1025.324756	142.296131	49.313204
1021.894247	137.006931	49.318209
1018.353885	133.931080	49.323213
1014.680994	135.134106	49.328218
1011.203127	125.012464	49.333223
1007.777561	135.307954	49.338228
1004.016002	132.746249	49.343233
1000.713712	130.826712	49.348237
996.947234	133.776467	49.353242
993.839759	130.386921	49.358247
990.332497	130.555763	49.363252
986.685547	124.670515	49.368257
983.065809	130.854248	49.373261
979.457069	137.680276	49.378266
976.442389	132.258611	49.383271
972.621625	139.513394	49.388276
969.149372	120.293817	49.393281
965.796575	136.441961	49.398285
962.240871	133.974716	49.403290
958.604604	129.330948	49.408295
954.999540	136.804440	49.413300
951.467566	136.626731	49.418305
948.390204	132.762181	49.423309
944.642711	125.664976	49.428314
941.200735	124.863213	49.433319
937.292802	137.316679	49.438324
934.067163	128.295576	49.443329
930.863904	128.505754	49.448333
927.292694	128.593263	49.453338
923.952551	128.696631	49.458343
920.141006	137.355955	49.463348
916.317761	135.357071	49.468353
912.871016	134.429034	49.473357
909.559773	138.700522	49.478362
906.479212	130.834733	49.483367
902.573601	126.479468	49.488372
899.030777	130.681121	49.493377
895.554165	129.585170	49.498381
891.891889	131.584373	49.503386
888.804726	130.014543	49.508391
885.049274	127.745570	49.513396
881.432828	132.098140	49.518401
878.194120	125.483402	49.523405
874.359372	130.170062	49.528410
871.281051	125.466454	49.533415
867.541398	129.372118	49.538420
864.328216	131.195833	49.543425
860.661215	127.208840	49.548429
857.174374	134.732706	49.553434
853.597320	134.699680	49.558439
849.892366	138.943580	49.563444
846.581520	124.018116	49.568449
843.132991	132.198509	49.573453
839.214206	140.623438	49.578458
836.188009	129.642037	49.583463
832.582472	138.414963	49.588468
829.279523	128.716252	49.593473
825.915142	128.872839	49.598477
821.857450	138.205417	49.603482
818.391901	130.204657	49.608487
815.035583	139.008402	49.613492
811.212947	132.728287	49.618497
808.155194	126.630495	49.623501
804.750754	134.481766	49.628506
801.220287	121.021195	49.633511
797.343549	128.471259	49.638516
793.710072	132.472100	49.643521
790.480638	135.607293	49.648525
786.755811	123.828420	49.653530
783.565941	118.893503	49.658535
779.758866	128.758312	49.663540
776.592147	131.470311	49.668545
773.467512	134.219160	49.673549
769.397170	131.335376	49.678554
766.210368	130.415368	49.683559
762.269946	139.561847	49.688564
758.984610	128.298757	49.693569
755.814320	128.003161	49.698573
751.737443	130.346344	49.703578
748.466617	128.849423	49.708583
744.700652	131.978678	49.713588
741.659891	130.298859	49.718593
738.138646	123.730775	49.723597
734.403283	126.720392	49.728602
730.635452	115.805923	49.733607
727.229741	135.726557	49.738612
724.115444	123.344725	49.743617
720.315872	123.316254	49.748621
716.955137	137.324952	49.753626
713.498796	118.043009	49.758631
709.698641	123.098819	49.763636
706.314578	122.385540	49.768641
702.885365	117.508830	49.773645
699.362176	131.756940	49.778650
695.931139	120.705878	49.783655
692.507466	127.315015	49.788660
688.961069	129.240746	49.793665
685.587429	128.423143	49.798669
681.742442	121.961947	49.803674
678.507741	125.141896	49.808679
675.129680	132.292294	49.813684
671.300843	127.214131	49.818689
667.811674	126.648511	49.823693
664.400003	128.097507	49.828698
661.233149	124.718228	49.833703
657.549048	129.834212	49.838708
653.685263	137.558129	49.843713
650.432051	124.507083	49.848717
646.399917	131.906807	49.853722
643.128511	133.959946	49.858727
640.147227	124.229100	49.863732
636.370569	126.412011	49.868737
632.898310	130.150882	49.873741
629.362880	124.032009	49.878746
626.060833	123.285686	49.883751
622.242334	135.129226	49.888756
618.630249	130.031826	49.893761
615.411459	125.630289	49.898765
611.727831	134.546337	49.903770
608.435504	130.002851	49.908775
604.867935	135.333639	49.913780
601.168715	125.563145	49.918785
597.841413	128.299863	49.923789
594.665166	123.192339	49.928794
591.045947	114.062992	49.933799
587.034283	132.931517	49.938804
583.690204	122.381609	49.943809
580.299502	124.538400	49.948813
576.809948	135.497354	49.953818
573.731673	124.082555	49.958823
569.882196	128.173379	49.963828
566.064581	124.353648	49.968833
562.732519	128.750579	49.973837
559.034567	131.404401	49.978842
555.730384	136.240535	49.983847
552.219484	140.698838	49.988852
549.058463	131.098243	49.993857
545.387666	125.266469	49.998861
541.490076	129.641747	50.003866
538.483096	123.188053	50.008871
534.815527	134.120645	50.013876
531.343826	125.985389	50.018881
528.001883	121.041103	50.023885
524.361998	131.391714	50.028890
521.017699	118.362175	50.033895
517.196437	125.866234	50.038900
513.703498	121.601114	50.043905
510.266056	123.414038	50.048909
505.970828	131.193479	50.053914
503.196361	122.868479	50.058919
499.780495	120.669948	50.063924
496.301507	121.277128	50.068929
493.110904	126.162392	50.073933
488.809512	130.945531	50.078938
485.706420	112.880355	50.083943
482.160922	127.367914	50.088948
478.799672	115.307378	50.093953
475.316369	120.207147	50.098957
471.520589	126.998196	50.103962
468.385380	119.937854	50.108967
464.871523	128.834992	50.113972
461.325872	124.815837	50.118977
458.027425	111.130328	50.123981
453.865418	122.310949	50.128986
450.642102	118.355285	50.133991
447.257141	127.292871	50.138996
443.445241	117.792981	50.144001
440.009248	116.484656	50.149005
436.162732	122.355663	50.154010
433.258041	110.418333	50.159015
429.571343	121.675618	50.164020
426.369722	115.329213	50.169025
423.108547	110.091828	50.174029
419.245247	127.069316	50.179034
415.985294	122.908197	50.184039
412.235360	118.745094	50.189044
408.474532	124.166620	50.194049
404.828791	116.769510	50.199053
401.313111	122.059893	50.204058
398.256261	119.439719	50.209063
394.599978	120.014754	50.214068
391.128061	120.487054	50.219073
387.658592	121.037689	50.224077
384.059870	128.256974	50.229082
380.821031	114.892598	50.234087
377.156484	121.986421	50.239092
373.567703	122.643642	50.244097
370.198781	122.377255	50.249101
366.484791	125.150910	50.254106
363.094507	121.436861	50.259111
359.548500	128.016557	50.264116
355.881666	119.728656	50.269121
352.901821	116.610720	50.274125
348.841158	122.328787	50.279130
345.422140	118.173530	50.284135
342.125928	108.474926	50.289140
338.504665	111.429406	50.294145
335.263873	111.772525	50.299149
331.419711	118.099269	50.304154
328.170504	120.828982	50.309159
324.662810	115.430998	50.314164
320.688789	113.661060	50.319169
317.734295	110.834366	50.324173
313.950355	115.826443	50.329178
310.683263	117.185673	50.334183
306.960090	114.692235	50.339188
303.743735	117.486582	50.344193
300.189161	111.210739	50.349197
296.502084	112.151288	50.354202
292.656836	116.155803	50.359207
289.581969	113.835880	50.364212
285.777986	114.767175	50.369217
282.742886	114.156111	50.374221
279.202758	118.981172	50.379226
275.695694	119.907729	50.384231
271.871374	126.195918	50.389236
268.320881	114.420476	50.394241
265.303746	119.063072	50.399245
261.252205	112.979442	50.404250
257.853808	117.030197	50.409255
254.387499	123.114490	50.414260
250.734774	115.260270	50.419265
247.540941	109.689040	50.424269
243.951539	118.752759	50.429274
240.903925	102.066694	50.434279
237.017329	107.732558	50.439284
233.432262	110.882808	50.444289
229.792730	116.517057	50.449293
225.579115	121.459765	50.454298
223.020560	113.781620	50.459303
219.937092	114.711312	50.464308
216.276400	113.647371	50.469313
213.246670	110.127141	50.474317
208.912673	110.763019	50.479322
205.435849	110.445164	50.484327
202.018681	114.865321	50.489332
198.377654	108.099889	50.494337
194.969957	105.422114	50.499341
191.048887	113.719270	50.504346
188.063512	111.970298	50.509351
184.327487	112.041496	50.514356
180.857708	111.884704	50.519361
177.548746	108.880189	50.524365
173.842929	114.710358	50.529370
170.401018	115.514523	50.534375
166.477173	122.953162	50.539380
163.204269	121.071642	50.544385
159.861407	107.420994	50.549389
156.374932	119.563137	50.554394
153.107604	105.050070	50.559399
149.455275	120.032490	50.564404
145.657862	112.056691	50.569409
142.499014	109.388672	50.574413
138.635149	117.743891	50.579418
135.391405	105.431762	50.584423
131.885907	111.017256	50.589428
128.328653	106.390156	50.594433
125.053972	106.874614	50.599437
121.439491	118.182723	50.604442
117.810208	102.631053	50.609447
114.509188	115.669399	50.614452
111.027176	109.184182	50.619457
107.528104	109.630028	50.624461
103.978979	113.443398	50.629466
100.194591	111.731862	50.634471
96.328499	109.568739	50.639476
93.233416	114.305852	50.644481
89.961908	112.123815	50.649485
86.347033	116.845368	50.654490
82.858014	101.710964	50.659495
79.317092	103.625816	50.664500
75.431730	117.634541	50.669505
72.206871	110.825972	50.674509
68.390088	120.591109	50.679514
65.234015	107.582535	50.684519
62.297508	110.416362	50.689524
58.438331	108.034667	50.694529
54.803803	101.355123	50.699533
51.193232	114.433910	50.704538
47.881333	111.072020	50.709543
44.197989	117.012437	50.714548
40.774767	113.450930	50.719553
37.598721	114.545661	50.724557
33.420031	118.358549	50.729562
30.402384	110.414378	50.734567
26.620746	115.651009	50.739572
23.238028	121.566726	50.744577
20.001651	105.913784	50.749581
16.168954	120.155966	50.754586
12.874029	103.618406	50.759591
9.523102	107.479740	50.764596
6.008619	117.989140	50.769601
2.434308	110.292472	50.774605