Tue Jun 21 12:33:28 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.646049	120.263310	0.000000
0.630443	115.102134	0.005005
0.902020	113.075226	0.010010
0.644042	121.852878	0.015014
0.443233	123.229491	0.020019
0.446483	108.984238	0.025024
0.339291	97.248637	0.030029
0.341806	90.504212	0.035034
-0.037441	89.450204	0.040038
-0.043519	64.421814	0.045043
-0.052401	59.294668	0.050048
-0.297695	48.536875	0.055053
-0.397132	35.593339	0.060058
-1.142111	17.223487	0.065062
-1.024892	6.621965	0.070067
-1.145643	-8.524981	0.075072
-2.013777	-7.989603	0.080077
-2.524037	-29.975527	0.085082
-3.159582	-18.014011	0.090086
-3.132410	-17.397208	0.095091
-3.530621	-17.495935	0.100096
-3.914452	-19.576295	0.105101
-4.751926	-19.158079	0.110106
-5.056787	-10.882054	0.115110
-4.284264	-16.181601	0.120115
-4.715643	-13.936043	0.125120
-5.027616	-13.410087	0.130125
-4.792381	-17.564724	0.135130
-4.958990	-12.736707	0.140134
-6.058954	-22.813003	0.145139
-6.108051	-8.852136	0.150144
-6.630649	-16.277965	0.155149
-6.513383	-26.956431	0.160154
-6.937533	-10.101722	0.165158
-6.934166	-12.386116	0.170163
-7.214436	-14.852443	0.175168
-8.055683	-16.676293	0.180173
-8.039637	-10.702419	0.185178
-8.337373	-1.714801	0.190182
-8.358390	-4.106454	0.195187
-8.316575	-7.471499	0.200192
-8.471084	-2.764079	0.205197
-8.739915	-16.169298	0.210202
-9.415564	-6.013242	0.215206
-9.863136	-7.318775	0.220211
-9.776798	-12.984204	0.225216
-10.232726	-5.780528	0.230221
-10.017855	-11.032321	0.235226
-10.425087	-15.643945	0.240230
-10.970295	-14.664371	0.245235
-11.261695	-15.268199	0.250240
-11.652109	-7.029705	0.255245
-11.332910	-4.902726	0.260250
-11.536997	-6.202802	0.265254
-11.518875	-3.374959	0.270259
-12.408860	-9.576666	0.275264
-13.019649	-5.681682	0.280269
-12.826561	-4.443722	0.285274
-12.877424	-10.162995	0.290278
-13.009750	-15.743073	0.295283
-13.746300	0.473704	0.300288
-14.273849	-11.870628	0.305293
-14.219727	-9.609372	0.310298
-14.212983	-7.748157	0.315302
-14.400705	-4.772362	0.320307
-13.981557	-13.874016	0.325312
-14.658332	-14.756000	0.330317
-15.222177	-12.666694	0.335322
-15.485951	-7.526189	0.340326
-15.758754	-18.091122	0.345331
-16.535695	-12.201408	0.350336
-17.117672	-3.709582	0.355341
-16.595088	-14.315470	0.360346
-17.162407	0.074786	0.365350
-17.600786	-9.699642	0.370355
-17.592208	-18.603453	0.375360
-17.954843	-3.563339	0.380365
-17.598544	-15.187159	0.385370
-17.832269	-9.259142	0.390374
-17.707936	-2.549386	0.395379
-18.234112	-7.372587	0.400384
-18.612706	-12.865902	0.405389
-18.918531	-14.271474	0.410394
-19.145522	-5.128039	0.415398
-19.626878	-4.075764	0.420403
-20.128693	-8.750657	0.425408
-20.770946	-7.923927	0.430413
-20.617102	-5.688460	0.435418
-20.627222	-13.090430	0.440422
-20.714454	-8.415467	0.445427
-21.105458	-6.275259	0.450432
-21.352029	-0.039441	0.455437
-20.971734	-11.620865	0.460442
-22.012836	-9.797850	0.465446
-22.253869	-14.185595	0.470451
-22.269057	-9.117834	0.475456
-22.455848	-5.302540	0.480461
-22.310082	-1.369853	0.485466
-23.240071	0.429630	0.490470
-23.663523	-16.288069	0.495475
-23.393953	-10.862145	0.500480
-24.067577	-4.962702	0.505485
-23.986574	-6.705644	0.510490
-24.414352	-5.047943	0.515494
-24.715620	-1.205205	0.520499
-24.775629	-1.045787	0.525504
-25.422768	-3.967381	0.530509
-25.040212	-10.685506	0.535514
-25.473671	-6.483436	0.540518
-25.692682	0.800986	0.545523
-26.060949	-10.412759	0.550528
-26.882201	-3.744524	0.555533
-26.985913	-7.630501	0.560538
-27.245794	-4.847982	0.565542
-27.221939	-3.363547	0.570547
-27.213034	-8.610041	0.575552
-27.634544	-3.342376	0.580557
-27.310903	-8.631524	0.585562
-28.273005	-9.553669	0.590566
-28.770204	-16.393477	0.595571
-28.703305	-13.696850	0.600576
-28.590677	-11.940393	0.605581
-28.580160	-18.672280	0.610586
-28.798481	-7.315810	0.615590
-29.573074	-14.474744	0.620595
-30.041004	-11.363152	0.625600
-30.509506	-8.978637	0.630605
-30.322505	-11.004153	0.635610
-30.523929	-8.639007	0.640614
-30.537883	-7.356497	0.645619
-31.424626	-8.415442	0.650624
-31.953542	-2.635275	0.655629
-31.987634	-8.844541	0.660634
-31.880118	-14.356991	0.665638
-32.157253	-9.372732	0.670643
-31.974025	-6.643077	0.675648
-32.367009	-8.809930	0.680653
-32.447394	-12.264649	0.685658
-33.261219	2.039746	0.690662
-33.094980	0.807000	0.695667
-33.147797	-8.648454	0.700672
-34.166728	0.895107	0.705677
-34.759424	-12.284200	0.710682
-34.987947	-4.302015	0.715686
-34.635525	-18.408036	0.720691
-34.869435	-19.188920	0.725696
-35.068838	-8.381408	0.730701
-34.926465	-12.417462	0.735706
-35.432790	0.029222	0.740710
-35.613022	-3.519075	0.745715
-36.083182	-10.414668	0.750720
-36.989946	-10.156847	0.755725
-36.595057	-13.564973	0.760730
-36.840918	-8.050923	0.765734
-37.138465	-4.063958	0.770739
-36.845902	-9.556737	0.775744
-37.643668	-9.971916	0.780749
-38.112523	-10.852812	0.785754
-38.276455	-6.837065	0.790758
-38.432052	-10.659589	0.795763
-38.122263	-4.572353	0.800768
-38.891366	-7.849073	0.805773
-39.196294	-11.196155	0.810778
-39.432316	-2.380770	0.815782
-39.390526	-9.231109	0.820787
-39.163430	-8.469423	0.825792
-39.990252	-0.611725	0.830797
-40.820259	-10.913878	0.835802
-41.183314	-3.468456	0.840806
-41.259045	-3.110088	0.845811
-41.252183	0.486654	0.850816
-41.255218	1.194498	0.855821
-41.120630	-6.383190	0.860826
-41.917275	-2.717111	0.865830
-42.314716	-6.398744	0.870835
-42.588851	-6.572876	0.875840
-42.731765	-5.974868	0.880845
-42.196591	-2.881407	0.885850
-42.652914	-5.806579	0.890854
-43.920766	-12.457182	0.895859
-43.962248	-1.718051	0.900864
-44.376987	-8.242166	0.905869
-43.940569	-4.980797	0.910874
-44.323753	-6.306068	0.915878
-44.190996	-3.767163	0.920883
-44.588878	-8.049208	0.925888
-45.457928	-5.466929	0.930893
-45.639422	-9.640757	0.935898
-45.793932	0.548776	0.940902
-46.093656	-10.663292	0.945907
-45.924290	-8.670158	0.950912
-45.921278	-17.442410	0.955917
-46.777834	-5.997207	0.960922
-47.209992	-0.169127	0.965926
-47.620500	-7.664823	0.970931
-47.041253	-11.016064	0.975936
-47.661650	3.154275	0.980941
-47.434009	-6.826951	0.985946
-48.382895	-3.968009	0.990950
-48.737823	-5.617638	0.995955
-48.574108	-15.182752	1.000960
-48.943024	-5.217403	1.005965
-48.862223	-16.891101	1.010970
-49.199241	-13.422902	1.015974
-50.057944	-5.085339	1.020979
-50.123752	-14.646578	1.025984
-50.779508	-5.960196	1.030989
-50.846577	-13.929931	1.035994
-51.007835	-4.048702	1.040998
-50.896658	-3.947630	1.046003
-50.737189	-12.832426	1.051008
-51.052856	-0.513224	1.056013
-50.941677	-6.803775	1.061018
-51.728429	-8.157912	1.066022
-52.344970	-4.592109	1.071027
-52.108190	-8.630973	1.076032
-52.547771	0.160900	1.081037
-53.051732	-12.610213	1.086042
-53.683105	-14.346663	1.091046
-53.875372	-7.292030	1.096051
-53.649448	-11.491106	1.101056
-54.122605	-5.787069	1.106061
-54.134302	-16.222771	1.111066
-54.063902	-9.586180	1.116070
-54.241340	-14.461211	1.121075
-54.536711	-9.254695	1.126080
-55.381958	-13.281886	1.131085
-55.236952	-13.988576	1.136090
-55.405013	-14.868178	1.141094
-56.573796	-7.346143	1.146099
-56.796944	-19.917684	1.151104
-56.954656	-15.399573	1.156109
-56.323053	-19.574668	1.161114
-56.748802	-16.076776	1.166118
-56.960546	-8.565052	1.171123
-56.927639	-14.096520	1.176128
-57.743799	-5.974781	1.181133
-58.204222	-19.227882	1.186138
-58.551299	-11.027351	1.191142
-58.668830	-19.170271	1.196147
-58.760724	-14.746730	1.201152
-59.091331	-9.466496	1.206157
-58.698680	-16.266802	1.211162
-59.236918	-10.601913	1.216166
-59.811003	-8.098085	1.221171
-60.199682	-19.561810	1.226176
-60.354808	-11.294997	1.231181
-60.401570	-14.581234	1.236186
-60.420481	-13.448470	1.241190
-60.747037	-13.661475	1.246195
-61.610178	-20.224586	1.251200
-61.867668	-7.892135	1.256205
-61.931795	-15.522153	1.261210
-62.217958	-14.667962	1.266214
-62.217918	-10.954061	1.271219
-62.069855	-19.814073	1.276224
-62.225311	-14.875424	1.281229
-62.465282	-19.826923	1.286234
-63.140537	-18.245250	1.291238
-63.702539	-15.189312	1.296243
-63.728011	-27.743068	1.301248
-63.896404	-16.610562	1.306253
-63.862128	-16.236275	1.311258
-64.718409	-17.202380	1.316262
-64.692743	-17.513188	1.321267
-64.584717	-16.802428	1.326272
-64.900638	-14.598089	1.331277
-64.841773	-19.868441	1.336282
-66.196308	-14.346791	1.341286
-66.689523	-10.766288	1.346291
-66.797210	-20.405438	1.351296
-66.745700	-14.532558	1.356301
-66.689278	-19.932943	1.361306
-66.892255	-14.830136	1.366310
-66.676577	-10.874698	1.371315
-67.076175	-25.246285	1.376320
-67.726845	-15.546459	1.381325
-68.056024	-25.495043	1.386330
-68.188749	-15.076080	1.391334
-68.279123	-13.905825	1.396339
-67.930605	-26.670707	1.401344
-69.206204	-15.227145	1.406349
-69.597109	-12.748920	1.411354
-69.712983	-7.425119	1.416358
-69.940761	-16.145134	1.421363
-69.807555	-17.193229	1.426368
-69.977214	-14.991211	1.431373
-70.309221	-20.646151	1.436378
-71.262614	-18.106534	1.441382
-71.196197	-11.194007	1.446387
-71.263421	-20.192014	1.451392
-71.717526	-16.778421	1.456397
-71.433842	-20.403350	1.461402
-71.377434	-14.928710	1.466406
-72.333305	-18.524358	1.471411
-72.635520	-27.804106	1.476416
-72.977150	-14.083302	1.481421
-72.995888	-24.703718	1.486426
-73.003021	-15.550135	1.491430
-73.383857	-5.643394	1.496435
-73.551579	-18.822821	1.501440
-74.161721	-10.784143	1.506445
-74.586696	-18.927448	1.511450
-74.651242	-20.167552	1.516454
-74.616627	-13.603379	1.521459
-74.904441	-17.558314	1.526464
-74.840058	-16.185970	1.531469
-75.241064	-14.665899	1.536474
-75.961733	-13.801704	1.541478
-76.516007	-11.215118	1.546483
-76.257220	-20.872143	1.551488
-76.447446	-10.167388	1.556493
-76.181135	-8.873084	1.561498
-77.060578	-5.621698	1.566502
-77.940084	-10.568702	1.571507
-77.770851	-8.741702	1.576512
-78.001267	-2.592823	1.581517
-78.290347	-13.878869	1.586522
-78.169896	-8.062792	1.591526
-78.096844	-20.465531	1.596531
-77.935337	-13.637427	1.601536
-78.904120	-7.828607	1.606541
-79.336545	-19.672447	1.611546
-79.613060	-17.745573	1.616550
-79.727008	-16.287452	1.621555
-80.092309	-27.981577	1.626560
-79.938176	-18.603107	1.631565
-80.531018	-23.651261	1.636570
-80.955416	-15.403590	1.641574
-81.356902	-16.645115	1.646579
-81.057274	-20.187831	1.651584
-81.370883	-18.884699	1.656589
-81.220409	-20.567121	1.661594
-82.027473	-22.218621	1.666598
-82.544971	-16.258010	1.671603
-82.539299	-14.373137	1.676608
-82.892682	-18.572757	1.681613
-83.064533	-15.264324	1.686618
-83.228359	-10.705733	1.691622
-83.210088	-6.838564	1.696627
-84.148627	-20.946839	1.701632
-84.426309	-15.005426	1.706637
-84.470065	-19.006308	1.711642
-84.681031	-14.856678	1.716646
-84.803243	-18.432139	1.721651
-84.407575	-23.826748	1.726656
-85.014345	-31.054698	1.731661
-85.781112	-18.707170	1.736666
-85.841619	-20.950592	1.741670
-86.538986	-19.886213	1.746675
-85.945726	-27.430929	1.751680
-86.165363	-8.864296	1.756685
-86.496386	-16.920350	1.761690
-86.755600	-17.244357	1.766694
-87.592773	-11.227640	1.771699
-87.696387	-26.058698	1.776704
-87.972162	-13.100245	1.781709
-87.846313	-15.154310	1.786714
-87.966724	-23.051265	1.791718
-88.357508	-18.135209	1.796723
-89.091705	-14.566888	1.801728
-89.561246	-11.318667	1.806733
-89.704593	-26.923595	1.811738
-89.705215	-19.333773	1.816742
-89.439835	-15.384795	1.821747
-89.675267	-21.086709	1.826752
-90.111201	-14.480713	1.831757
-91.096131	-11.237309	1.836762
-91.138834	-16.510966	1.841766
-91.567247	-1.819503	1.846771
-91.404220	-19.662423	1.851776
-91.887707	-8.362679	1.856781
-92.058142	-17.721088	1.861786
-91.825690	-15.605207	1.866790
-92.067749	-11.580863	1.871795
-92.046215	-14.574913	1.876800
-92.394920	-7.634082	1.881805
-93.086353	-14.240822	1.886810
-93.363348	-15.384367	1.891814
-93.766615	-5.263160	1.896819
-93.323268	-15.568803	1.901824
-94.048997	-5.324330	1.906829
-94.086513	-13.347895	1.911834
-95.035739	-7.019576	1.916838
-95.416099	-8.614865	1.921843
-95.078644	-17.470528	1.926848
-95.331382	-10.027791	1.931853
-95.375007	-12.945140	1.936858
-95.429863	-9.699891	1.941862
-95.764123	-3.564596	1.946867
-96.353944	-17.573749	1.951872
-96.700610	-15.624598	1.956877
-97.214431	-17.081946	1.961882
-97.013177	-6.655545	1.966886
-97.165343	-10.804429	1.971891
-97.077590	-11.015015	1.976896
-97.928928	-8.678972	1.981901
-98.045834	-8.147628	1.986906
-98.238564	-9.894565	1.991910
-98.729650	-3.332117	1.996915
-98.597455	-10.586960	2.006912
-98.744028	-5.989167	2.016909
-98.429309	-11.791238	2.026906
-97.640534	-12.484411	2.036902
-96.908534	-16.651419	2.046899
-96.112080	-16.502371	2.056896
-95.995812	-8.664240	2.066893
-95.958682	-6.225268	2.076890
-95.133885	-7.777978	2.086886
-94.292408	-6.146986	2.096883
-94.207782	-13.656615	2.106880
-93.072997	-11.456552	2.116877
-92.714818	-8.928098	2.126874
-92.819572	-7.604312	2.136870
-91.794035	-15.038609	2.146867
-91.078775	-12.985020	2.156864
-90.774421	-20.320809	2.166861
-90.537131	-15.233358	2.176858
-90.662433	-14.104742	2.186854
-89.582891	-16.394158	2.196851
-89.038361	-11.380317	2.206848
-87.899354	-9.130171	2.216845
-87.687071	-19.211971	2.226842
-87.830969	-9.730898	2.236838
-87.480731	-15.933033	2.246835
-86.361378	-12.658905	2.256832
-85.971785	-11.672870	2.266829
-85.366771	-13.889815	2.276826
-84.832396	-15.526013	2.286822
-84.641454	-12.766742	2.296819
-84.170311	-17.374034	2.306816
-83.204057	-14.826756	2.316813
-83.195206	-13.972084	2.326810
-82.547388	-10.057327	2.336806
-81.395452	-15.502518	2.346803
-81.369052	-14.384013	2.356800
-81.404309	-14.471632	2.366797
-80.442469	-13.203977	2.376794
-79.990301	-9.183708	2.386790
-79.658523	-9.449880	2.396787
-78.440606	-13.175938	2.406784
-78.412926	-15.273747	2.416781
-78.305062	-15.143424	2.426778
-77.890730	-14.529391	2.436774
-77.117030	-16.532033	2.446771
-75.968237	-16.840462	2.456768
-75.393106	-15.924081	2.466765
-75.630361	-13.026512	2.476762
-75.401125	-18.081576	2.486758
-74.508284	-9.405870	2.496755
-73.728461	-12.990015	2.506752
-73.678844	-16.675304	2.516749
-72.621825	-15.366902	2.526746
-72.290343	-15.482661	2.536742
-72.189986	-20.277498	2.546739
-71.722546	-18.263080	2.556736
-71.036653	-16.981925	2.566733
-70.477096	-7.470949	2.576730
-69.302823	-16.902375	2.586726
-69.108191	-17.788775	2.596723
-69.260368	-16.249078	2.606720
-68.700728	-20.280244	2.616717
-67.788453	-18.617702	2.626714
-67.188144	-15.843838	2.636710
-67.368643	-19.030837	2.646707
-66.507211	-21.208249	2.656704
-66.212810	-23.949509	2.666701
-65.379742	-21.188906	2.676698
-64.859001	-22.214674	2.686694
-64.779962	-18.041519	2.696691
-63.760813	-19.695764	2.706688
-63.068409	-16.081607	2.716685
-63.190650	-16.105424	2.726682
-62.427011	-15.552997	2.736678
-61.501113	-12.098038	2.746675
-61.525479	-18.462191	2.756672
-61.105098	-17.359541	2.766669
-60.232725	-13.365397	2.776666
-60.484131	-17.833851	2.786662
-59.095871	-11.515592	2.796659
-58.607729	-16.194853	2.806656
-58.486920	-12.317682	2.816653
-58.278839	-18.216885	2.826650
-57.291066	-21.191140	2.836646
-56.767375	-14.180203	2.846643
-56.519148	-16.636208	2.856640
-55.381157	-6.759469	2.866637
-55.285581	-12.927529	2.876634
-54.974576	-12.341825	2.886630
-54.655730	-10.525670	2.896627
-53.765422	-13.511643	2.906624
-53.368133	-11.282287	2.916621
-53.099637	-5.115054	2.926618
-52.331893	-4.957686	2.936614
-51.977382	-9.850537	2.946611
-51.417838	-11.093159	2.956608
-50.510552	-10.360810	2.966605
-50.445568	-6.624754	2.976602
-50.140867	-5.745183	2.986598
-49.298330	-2.503439	2.996595
-48.917501	-5.375394	3.006592
-48.648852	-5.504455	3.016589
-47.737494	2.509645	3.026586
-47.456983	-5.996258	3.036582
-46.773185	0.525623	3.046579
-45.977381	-4.056802	3.056576
-45.835231	-4.683576	3.066573
-45.562633	0.402977	3.076570
-45.073628	1.831149	3.086566
-44.228736	-4.531159	3.096563
-43.985962	-10.529767	3.106560
-43.298221	-7.721179	3.116557
-42.393895	-3.079497	3.126554
-42.406953	-5.158112	3.136550
-42.070959	-7.864177	3.146547
-41.391109	-14.192626	3.156544
-41.062094	-12.716619	3.166541
-40.395013	-15.360348	3.176538
-39.805441	-8.001697	3.186534
-39.427980	-8.936950	3.196531
-39.194481	-10.145133	3.206528
-38.264501	-13.960223	3.216525
-37.894863	-16.787446	3.226522
-37.022251	-7.218253	3.236518
-36.699938	-5.487039	3.246515
-36.807558	-5.948560	3.256512
-35.820553	-10.447258	3.266509
-34.883794	-12.035888	3.276506
-34.877843	-7.423245	3.286502
-35.022687	-8.085473	3.296499
-33.596063	-2.976653	3.306496
-33.361132	-5.063541	3.316493
-32.686083	-7.902224	3.326490
-31.914053	-6.422725	3.336486
-32.290220	-3.557671	3.346483
-31.720584	-6.562651	3.356480
-30.193396	-9.879741	3.366477
-29.906064	-5.652953	3.376474
-30.075287	-5.519615	3.386470
-29.778310	-6.632998	3.396467
-28.834668	-8.046323	3.406464
-28.513159	-10.189239	3.416461
-27.701494	-6.696580	3.426458
-27.133937	-7.806762	3.436454
-27.100318	-10.258641	3.446451
-26.232733	-10.254928	3.456448
-25.572650	-9.882337	3.466445
-25.322202	-9.559666	3.476442
-25.169993	-2.376150	3.486438
-24.249709	-3.217546	3.496435
-23.648438	-6.143791	3.506432
-23.376749	-4.422172	3.516429
-22.500570	-6.539188	3.526426
-22.435769	-5.386733	3.536422
-22.129460	-3.350561	3.546419
-20.968117	-4.516797	3.556416
-20.786302	-4.768403	3.566413
-20.628078	-7.651503	3.576410
-19.668339	-3.636448	3.586406
-19.177620	-2.453959	3.596403
-19.062777	-6.764941	3.606400
-18.134478	-9.146264	3.616397
-17.577818	-7.128436	3.626394
-17.352793	-10.163279	3.636390
-16.944408	-7.987129	3.646387
-16.247306	-7.362817	3.656384
-15.929274	-15.076288	3.666381
-15.256380	-5.270103	3.676378
-14.670342	-13.531804	3.686374
-14.153939	-5.188906	3.696371
-14.138740	-7.870689	3.706368
-13.100974	-10.726366	3.716365
-13.036636	-9.508236	3.726362
-12.117505	0.773664	3.736358
-11.393477	-0.032264	3.746355
-11.089271	-3.093658	3.756352
-11.127828	-3.961591	3.766349
-10.732001	-0.324384	3.776346
-9.899001	-6.960350	3.786342
-9.118456	-2.873529	3.796339
-8.337740	-5.437084	3.806336
-8.094643	-6.411136	3.816333
-7.823601	-9.428112	3.826330
-7.789453	-15.553002	3.836326
-6.759587	-11.498384	3.846323
-6.497626	-12.585813	3.856320
-5.287562	-16.728841	3.866317
-4.681951	-14.935079	3.876314
-4.945871	-13.044142	3.886310
-4.541413	-13.509064	3.896307
-3.996717	-3.851568	3.906304
-3.266833	-6.760581	3.916301
-3.156664	-2.693342	3.926298
-2.566572	8.552547	3.936294
-2.634638	27.764659	3.946291
-1.597133	41.402946	3.956288
-1.441168	64.038336	3.966285
-0.869247	82.674667	3.976282
-0.585258	108.354088	3.986278
0.000000	129.107230	3.991283
-0.156982	143.620288	3.996288
0.106642	150.125495	4.001293
0.439990	172.373436	4.006298
0.503025	186.371361	4.011302
0.324706	194.561418	4.016307
0.515945	194.149974	4.021312
1.026093	184.260762	4.026317
0.505496	189.422156	4.031322
0.867216	195.515282	4.036326
0.735355	212.852265	4.041331
0.916735	208.853108	4.046336
1.281888	211.661605	4.051341
1.331017	211.274485	4.056346
1.269942	212.715385	4.061350
1.265673	213.056200	4.066355
1.073134	212.445264	4.071360
1.450090	209.509722	4.076365
0.828915	201.915404	4.081370
1.042225	202.562564	4.086374
1.190771	214.133133	4.091379
1.242983	218.017631	4.096384
1.383719	214.270690	4.101389
1.097979	210.808290	4.106394
1.168391	211.714340	4.111398
1.086701	213.086034	4.116403
1.006746	221.412553	4.121408
1.217490	218.921902	4.126413
1.283656	223.385443	4.131418
1.176350	223.640510	4.136422
1.391629	218.430802	4.141427
1.261991	208.760405	4.146432
1.403465	225.935708	4.151437
1.392760	223.251438	4.156442
1.468487	220.895431	4.161446
1.713115	215.938781	4.166451
1.252572	216.352397	4.171456
1.593940	207.285794	4.176461
1.254453	216.900679	4.181466
1.394208	207.292033	4.186470
1.412013	219.227227	4.191475
1.588245	220.473326	4.196480
1.446482	218.952943	4.201485
1.336177	221.515170	4.206490
1.338417	213.910944	4.211494
1.243759	215.446009	4.216499
0.974779	219.492827	4.221504
1.481984	220.771929	4.226509
1.327473	221.954795	4.231514
1.228790	220.965019	4.236518
1.136655	224.107365	4.241523
1.176843	219.697448	4.246528
1.583457	225.810383	4.251533
1.286994	225.817348	4.256538
1.449689	245.018959	4.261542
1.584337	252.093967	4.266547
1.336416	252.660434	4.271552
1.690186	256.107235	4.276557
1.607698	263.800154	4.281562
1.819906	248.550059	4.286566
1.679952	259.939924	4.291571
1.484101	257.956268	4.296576
1.661003	257.548776	4.301581
1.936848	263.750872	4.306586
1.737692	259.746443	4.311590
1.652181	260.199185	4.316595
1.671905	258.367100	4.321600
1.878929	266.943110	4.326605
1.388333	270.407202	4.331610
1.678261	262.936266	4.336614
1.549540	262.098478	4.341619
1.697981	264.245881	4.346624
1.821427	267.529348	4.351629
1.484329	272.245184	4.356634
1.673783	268.152715	4.361638
1.602753	276.691699	4.366643
1.774847	266.000004	4.371648
1.766852	261.765594	4.376653
1.478469	273.486908	4.381658
1.630714	267.954320	4.386662
1.828515	285.393278	4.391667
1.665193	290.663866	4.396672
2.085796	289.637027	4.401677
1.727172	292.469695	4.406682
1.839595	294.886710	4.411686
1.832746	292.746835	4.416691
1.667332	300.227751	4.421696
1.845030	297.657508	4.426701
1.684487	303.826906	4.431706
1.520995	302.006609	4.436710
1.685526	297.344009	4.441715
2.176928	314.266095	4.446720
2.335883	311.982922	4.451725
1.743147	317.514472	4.456730
1.948791	326.584876	4.461734
2.106369	329.583274	4.466739
2.088180	336.640217	4.471744
1.984936	335.850895	4.476749
2.050981	330.276713	4.481754
2.650868	329.449290	4.486758
2.191879	331.018851	4.491763
2.173298	338.989534	4.496768
2.233405	334.106227	4.501773
2.370736	332.644794	4.506778
2.113156	310.151217	4.511782
1.977576	314.913417	4.516787
1.919355	323.849716	4.521792
2.578047	326.557525	4.526797
2.174966	336.373841	4.531802
2.261662	334.967957	4.536806
1.949430	342.254558	4.541811
1.913950	334.623564	4.546816
2.377773	330.722841	4.551821
2.118275	334.134072	4.556826
2.596044	330.506326	4.561830
2.117101	335.158054	4.566835
2.419803	340.916657	4.571840
2.664724	331.365703	4.576845
2.604177	333.284084	4.581850
2.506477	334.955630	4.586854
2.510953	336.101913	4.591859
2.159080	340.841529	4.596864
2.298143	337.712897	4.601869
1.957686	345.280644	4.606874
2.097418	339.541714	4.611878
2.392399	339.429024	4.616883
2.340734	338.112753	4.621888
2.309077	335.868642	4.626893
2.188076	343.137190	4.631898
2.427702	358.219603	4.636902
2.521235	357.633510	4.641907
2.465458	367.338258	4.646912
2.620354	367.693765	4.651917
2.530421	365.263146	4.656922
2.268641	371.173261	4.661926
2.381693	356.985373	4.666931
2.524894	357.810901	4.671936
2.503048	356.033248	4.676941
2.509938	365.660325	4.681946
2.578403	363.767270	4.686950
2.265754	366.574379	4.691955
2.229790	361.911810	4.696960
2.612026	363.119069	4.701965
2.329153	371.281344	4.706970
2.457741	379.872773	4.711974
2.609399	392.798871	4.716979
2.858482	401.539082	4.721984
3.058420	399.451775	4.726989
2.721865	407.813588	4.731994
2.847780	396.496981	4.736998
2.894347	401.907097	4.742003
2.875510	391.420199	4.747008
2.784625	373.182154	4.752013
2.479933	380.223219	4.757018
2.733023	396.946281	4.762022
2.698176	401.451664	4.767027
2.882514	405.432337	4.772032
3.004576	401.232592	4.777037
2.754432	410.274924	4.782042
3.242876	398.141682	4.787046
3.101629	412.765855	4.792051
3.056001	406.773825	4.797056
3.145048	389.348795	4.802061
2.803199	387.523096	4.807066
2.725128	381.175517	4.812070
2.794767	396.669349	4.817075
2.824877	399.863515	4.822080
3.040526	398.567104	4.827085
2.902207	405.562671	4.832090
2.706776	404.217514	4.837094
2.952386	405.441877	4.842099
2.845931	407.921601	4.847104
3.181301	402.517496	4.852109
2.933825	403.683408	4.857114
3.157989	404.820547	4.862118
3.088828	408.929242	4.867123
3.079326	407.934354	4.872128
3.178636	403.388889	4.877133
3.136953	409.627053	4.882138
2.962709	403.651982	4.887142
2.861902	407.475435	4.892147
2.819831	403.440810	4.897152
3.159718	400.137613	4.902157
3.085146	402.543185	4.907162
2.967315	407.882452	4.912166
3.015274	412.463322	4.917171
3.031282	427.440357	4.922176
3.436871	431.919184	4.927181
3.628993	435.605923	4.932186
3.504262	429.997191	4.937190
3.187365	416.558508	4.942195
3.222221	431.727989	4.947200
3.405256	434.169247	4.952205
3.312208	426.875521	4.957210
3.287134	419.129490	4.962214
3.136910	426.591375	4.967219
3.299353	432.123606	4.972224
3.396977	434.283791	4.977229
3.520636	446.831535	4.982234
3.145695	443.074822	4.987238
3.346008	436.588368	4.992243
2.889738	444.575743	4.997248
3.292009	439.707174	5.002253
3.019530	448.410845	5.007258
3.080179	444.623040	5.012262
3.255437	448.626541	5.017267
3.325194	459.150629	5.022272
3.396521	446.213202	5.027277
3.362200	457.907775	5.032282
3.398325	468.598272	5.037286
3.356799	469.806846	5.042291
3.639047	471.421800	5.047296
3.745048	475.585571	5.052301
3.315943	476.592516	5.057306
3.583272	476.535515	5.062310
3.468127	472.693540	5.067315
3.251833	473.891195	5.072320
3.633420	472.891527	5.077325
3.522325	484.315653	5.082330
3.340765	479.522644	5.087334
3.609489	473.517404	5.092339
3.404026	484.178259	5.097344
3.659884	475.307807	5.102349
3.220732	484.830431	5.107354
3.182731	480.378528	5.112358
3.530542	493.498771	5.117363
3.618028	500.480270	5.122368
3.837129	511.206208	5.127373
3.709687	511.622091	5.132378
3.573795	514.617818	5.137382
4.026999	504.773947	5.142387
3.742115	521.728715	5.147392
4.070349	512.445063	5.152397
3.705994	518.203495	5.157402
3.882025	510.495353	5.162406
4.005395	511.980329	5.167411
3.919062	514.954428	5.172416
3.828987	506.668934	5.177421
3.347328	521.818465	5.182426
3.889022	512.380071	5.187430
3.957080	513.340600	5.192435
3.932221	516.447394	5.197440
4.053839	505.573658	5.202445
3.872054	506.870388	5.207450
3.858292	512.012285	5.212454
3.364793	504.213542	5.217459
3.734613	512.098086	5.222464
4.151290	504.252016	5.227469
4.043860	515.234504	5.232474
4.251796	517.641261	5.237478
4.172282	512.200249	5.242483
4.237122	512.925096	5.247488
3.736912	512.737677	5.252493
3.840908	523.453874	5.257498
3.900109	512.597179	5.262502
3.718434	520.436501	5.267507
4.023405	537.135532	5.272512
4.463634	537.368603	5.277517
4.024232	532.892384	5.282522
3.929099	526.519153	5.287526
4.290485	536.324634	5.292531
4.244459	545.947759	5.297536
4.132196	542.211852	5.302541
4.198928	547.736295	5.307546
4.495850	541.494682	5.312550
4.188652	522.941610	5.317555
3.928638	533.199881	5.322560
4.243870	548.089392	5.327565
4.237507	554.158564	5.332570
4.286111	552.650628	5.337574
4.437708	539.797711	5.342579
4.077173	560.530302	5.347584
4.808392	547.596386	5.352589
4.256142	556.297508	5.357594
4.441305	539.864801	5.362598
4.173199	533.954362	5.367603
4.401848	558.962634	5.372608
4.561448	546.762372	5.377613
4.519928	545.726600	5.382618
4.434627	534.678325	5.387622
4.404997	519.780207	5.392627
4.351284	521.565261	5.397632
4.643713	522.131645	5.402637
4.220020	523.240313	5.407642
4.434011	537.556929	5.412646
4.261829	538.678412	5.417651
3.987225	554.431685	5.422656
4.568580	546.234881	5.427661
4.515658	552.572055	5.432666
4.782963	549.359191	5.437670
4.679059	546.373371	5.442675
4.827528	559.982539	5.447680
4.720742	557.530211	5.452685
4.528220	561.038740	5.457690
4.583096	550.667009	5.462694
4.774317	550.291673	5.467699
4.599943	543.872159	5.472704
4.684869	535.565561	5.477709
4.825956	539.915551	5.482714
4.304806	531.843320	5.487718
4.470881	539.539613	5.492723
4.417681	549.491710	5.497728
5.120363	547.214365	5.502733
4.583342	553.283995	5.507738
4.578795	553.727876	5.512742
4.789707	551.626102	5.517747
4.575092	559.541152	5.522752
4.823612	540.389060	5.527757
4.506507	551.218231	5.532762
4.679466	552.957461	5.537766
4.808511	552.872250	5.542771
4.630672	554.897701	5.547776
4.556559	546.064291	5.552781
4.622100	552.755214	5.557786
4.583887	560.762810	5.562790
4.620685	544.561087	5.567795
4.319623	561.749269	5.572800
4.772485	567.119390	5.577805
4.631554	573.917335	5.582810
4.349279	585.959933	5.587814
4.875025	580.565285	5.592819
4.637373	587.925098	5.597824
4.957699	580.084488	5.602829
4.410501	593.908156	5.607834
4.574012	593.671599	5.612838
4.907002	592.835871	5.617843
4.821691	590.108638	5.622848
4.996936	601.162185	5.627853
5.117650	616.575552	5.632858
4.968780	612.401279	5.637862
4.988195	607.204538	5.642867
5.255530	628.543076	5.647872
5.320834	606.524865	5.652877
5.066417	598.079064	5.657882
4.749365	587.105245	5.662886
4.914306	590.452359	5.667891
4.931604	615.934216	5.672896
4.998259	615.505702	5.677901
5.129411	622.451411	5.682906
5.334303	618.931347	5.687910
5.305302	619.690091	5.692915
4.865802	623.983710	5.697920
5.045356	616.688757	5.702925
5.094646	628.835337	5.707930
5.147000	629.951612	5.712934
5.634275	632.057951	5.717939
5.152744	626.243602	5.722944
5.386885	627.600918	5.727949
5.167096	626.422187	5.732954
5.246054	617.577002	5.737958
5.386964	621.237337	5.742963
5.282996	624.736148	5.747968
5.251352	616.721933	5.752973
5.348571	621.734186	5.757978
4.995555	624.363709	5.762982
5.324301	622.932711	5.767987
5.138092	627.416852	5.772992
5.303979	621.664607	5.777997
5.204067	635.628945	5.783002
4.941956	625.104030	5.788006
5.514004	622.389489	5.793011
5.130950	630.919757	5.798016
5.385298	621.146438	5.803021
5.447875	635.841657	5.808026
5.511724	643.180180	5.813030
5.483373	642.315092	5.818035
5.464134	656.074272	5.823040
5.318470	651.194947	5.828045
5.782104	651.746995	5.833050
5.546940	651.503445	5.838054
5.675418	648.444784	5.843059
5.284235	644.376148	5.848064
5.500461	646.363584	5.853069
5.439650	652.194542	5.858074
5.199241	651.912392	5.863078
5.751443	662.337777	5.868083
5.667095	659.110308	5.873088
5.795645	657.540380	5.878093
5.860141	652.398518	5.883098
5.731289	656.864880	5.888102
5.872753	658.728532	5.893107
5.853208	656.339691	5.898112
5.661391	643.126379	5.903117
5.819696	640.235651	5.908122
5.681983	641.197112	5.913126
5.774123	632.824145	5.918131
5.376455	636.023883	5.923136
5.602403	646.601169	5.928141
5.812174	647.827935	5.933146
5.803924	658.352843	5.938150
5.820809	656.669977	5.943155
5.881803	653.959156	5.948160
6.059847	653.106459	5.953165
5.854102	661.314525	5.958170
5.863299	653.709918	5.963174
5.883215	651.267575	5.968179
5.666468	664.327334	5.973184
6.113035	652.086964	5.978189
5.819291	656.906642	5.983194
5.953863	651.324154	5.988198
5.970328	649.319692	5.993203
5.553352	657.815335	5.998208
5.689476	655.630420	6.003213
5.789754	647.702878	6.008218
5.875998	655.609989	6.013222
5.786434	649.742164	6.018227
5.666362	663.266636	6.023232
5.867397	655.050468	6.028237
5.829281	651.091495	6.033242
5.919536	656.753773	6.038246
5.838035	648.891462	6.043251
5.510336	663.632001	6.048256
5.860554	652.988294	6.053261
5.344163	651.755274	6.058266
5.381165	664.951802	6.063270
5.661523	680.296958	6.068275
5.856761	681.821752	6.073280
6.014720	686.164845	6.078285
5.979745	690.225721	6.083290
5.919345	693.835344	6.088294
6.010746	687.219605	6.093299
5.597429	696.241961	6.098304
5.678354	690.484026	6.103309
5.748056	696.301280	6.108314
5.658783	695.424571	6.113318
5.918345	690.529829	6.118323
5.893184	700.482905	6.123328
6.038374	690.313200	6.128333
6.047078	691.442233	6.133338
5.668223	696.802132	6.138342
5.835242	696.362126	6.143347
5.659032	702.626238	6.148352
5.882526	693.283453	6.153357
5.636464	699.967630	6.158362
5.782499	703.210348	6.163366
5.795175	690.016413	6.168371
5.715401	698.703308	6.173376
6.032378	696.898908	6.178381
5.994571	697.902635	6.183386
6.108601	701.722156	6.188390
5.960079	690.630563	6.193395
5.879180	697.509594	6.198400
5.802034	701.577063	6.203405
6.066943	700.719846	6.208410
5.737017	697.431604	6.213414
6.070422	689.902350	6.218419
5.856120	696.061072	6.223424
5.984276	695.408846	6.228429
5.853740	695.079688	6.233434
6.050470	698.815654	6.238438
6.385582	688.701328	6.243443
6.084118	694.995258	6.248448
6.037967	688.516362	6.253453
6.198604	686.566561	6.258458
5.906629	697.649993	6.263462
6.173718	693.490090	6.268467
6.108897	698.049267	6.273472
6.336707	694.306735	6.278477
5.942414	695.585786	6.283482
5.910216	695.437684	6.288486
6.012096	691.791393	6.293491
6.261492	700.384307	6.298496
6.006400	680.501012	6.303501
5.912434	665.969019	6.308506
5.556783	662.048421	6.313510
5.488009	658.860604	6.318515
5.770523	687.870148	6.323520
6.075245	684.508777	6.328525
6.203570	693.821512	6.333530
5.874389	697.708511	6.338534
5.882084	698.769037	6.343539
5.918488	706.164627	6.348544
5.870739	696.356433	6.353549
6.557326	691.323086	6.358554
6.387332	678.584093	6.363558
6.364158	666.041029	6.368563
5.917215	668.829779	6.373568
5.857975	657.905768	6.378573
5.607478	660.448854	6.383578
5.630869	657.214200	6.388582
5.895466	653.953809	6.393587
5.680707	660.806841	6.398592
5.801697	656.955315	6.403597
5.883067	660.107694	6.408602
5.826934	659.489542	6.413606
6.283907	649.692120	6.418611
5.741567	657.746745	6.423616
6.039739	660.157131	6.428621
5.680195	660.536072	6.433626
5.887639	662.414058	6.438630
5.839857	654.573788	6.443635
5.615187	663.345834	6.448640
6.255301	674.418553	6.453645
6.001722	668.853373	6.458650
5.717099	661.771041	6.463654
5.820049	658.420198	6.468659
5.925753	671.979910	6.473664
6.223818	670.400457	6.478669
6.044091	662.825159	6.483674
5.626985	662.893149	6.488678
5.985702	652.149760	6.493683
5.888603	658.338787	6.498688
6.148307	652.910421	6.503693
5.992989	661.698215	6.508698
5.689305	660.177370	6.513702
6.102828	651.046660	6.518707
5.892556	657.489266	6.523712
6.069429	652.980416	6.528717
5.878757	653.683842	6.533722
5.887400	654.584360	6.538726
5.936682	647.578167	6.543731
6.030735	653.874860	6.548736
5.845586	650.681847	6.553741
5.858520	656.902776	6.558746
5.967314	655.558327	6.563750
6.221089	652.404714	6.568755
5.302358	655.118851	6.573760
5.686088	665.253234	6.578765
5.678056	668.420816	6.583770
6.091932	695.171947	6.588774
6.344258	677.921237	6.593779
5.933556	673.715713	6.598784
6.190858	660.746124	6.603789
6.091000	658.337824	6.608794
5.762883	659.334765	6.613798
6.247465	647.956012	6.618803
5.811687	665.772852	6.623808
6.293346	660.738326	6.628813
6.089774	656.071062	6.633818
5.681948	661.563230	6.638822
6.263033	656.340552	6.643827
6.270934	662.838596	6.648832
6.139803	662.132614	6.653837
5.820175	658.253807	6.658842
5.530972	657.791869	6.663846
6.163533	657.308314	6.668851
6.115123	674.377817	6.673856
6.272275	656.624277	6.678861
5.960199	660.150851	6.683866
6.055131	660.643186	6.688870
6.228077	646.749810	6.693875
5.968895	638.174926	6.698880
5.743207	631.239537	6.703885
5.779545	629.789868	6.708890
5.770863	643.525581	6.713894
5.896983	644.360072	6.718899
5.542960	658.415059	6.723904
5.873330	658.678955	6.728909
5.852377	659.062604	6.733914
5.481869	667.109695	6.738918
5.742407	657.861440	6.743923
5.702855	665.341817	6.748928
5.852146	658.221176	6.753933
5.975077	657.817283	6.758938
5.952795	660.534916	6.763942
6.029057	658.967726	6.768947
5.710374	654.298213	6.773952
5.716843	660.089615	6.778957
5.823497	661.668545	6.783962
5.326076	659.804047	6.788966
5.959069	651.957996	6.793971
5.976612	653.749025	6.798976
5.958415	666.567906	6.803981
5.847741	660.102470	6.808986
5.886540	659.077070	6.813990
6.310102	655.819560	6.818995
5.966161	665.459534	6.824000
5.945247	664.505988	6.829005
6.087232	656.955168	6.834010
5.969444	655.199487	6.839014
6.036755	654.097928	6.844019
5.791731	657.612608	6.849024
5.685683	653.082726	6.854029
6.020705	652.048133	6.859034
5.837831	663.935598	6.864038
6.257205	656.162811	6.869043
6.003660	659.490639	6.874048
6.019975	658.671040	6.879053
5.956823	654.313241	6.884058
5.399735	659.159559	6.889062
6.008577	657.557848	6.894067
5.607225	659.951467	6.899072
5.804476	658.745110	6.904077
5.839349	663.028854	6.909082
5.891598	660.152529	6.914086
6.215762	650.013993	6.919091
6.050212	656.735337	6.924096
6.086866	657.043534	6.929101
5.947275	652.544861	6.934106
5.936505	663.375280	6.939110
6.169131	652.974044	6.944115
6.113987	658.842745	6.949120
6.189762	657.375096	6.954125
5.972207	663.992177	6.959130
5.723582	654.434746	6.964134
6.100501	653.808027	6.969139
6.029755	661.595106	6.974144
5.671184	662.735625	6.979149
6.141520	659.204351	6.984154
5.798046	669.096058	6.989158
6.287875	662.863102	6.994163
6.170288	658.885713	6.999168
6.222867	657.745547	7.004173
5.949244	642.300429	7.009178
5.449540	643.894524	7.014182
5.651167	641.169493	7.019187
5.922906	657.754569	7.024192
6.040130	654.818544	7.029197
5.937874	657.000020	7.034202
5.767904	669.143081	7.039206
6.010881	662.862991	7.044211
6.058661	660.049371	7.049216
5.887367	661.738666	7.054221
5.872523	657.338133	7.059226
5.451462	657.969597	7.064230
5.993049	658.285739	7.069235
5.727110	665.698621	7.074240
5.360291	666.240982	7.079245
5.857262	669.948531	7.084250
5.608156	669.746364	7.089254
5.835486	664.493464	7.094259
5.633266	665.764385	7.099264
5.711615	662.951227	7.104269
5.682611	658.922463	7.109274
6.038312	681.179866	7.114278
6.095207	680.208697	7.119283
5.961362	665.086941	7.124288
5.915174	661.220080	7.129293
5.724601	662.093598	7.134298
5.658070	674.354909	7.139302
6.214144	681.470637	7.144307
5.993700	691.187267	7.149312
5.929534	673.990949	7.154317
5.959761	667.744511	7.159322
5.906778	670.339747	7.164326
6.044807	656.963260	7.169331
6.204964	659.254022	7.174336
5.955592	654.661440	7.179341
6.050823	650.867858	7.184346
6.014539	660.105611	7.189350
6.213866	649.046823	7.194355
5.955109	652.924912	7.199360
5.894128	657.097046	7.204365
6.276535	657.418236	7.209370
6.064402	661.888130	7.214374
6.104474	653.184347	7.219379
6.211428	657.502330	7.224384
6.121697	662.430309	7.229389
6.359969	659.766302	7.234394
6.227909	660.468705	7.239398
6.168660	629.432443	7.244403
5.714654	636.853961	7.249408
5.757014	627.877876	7.254413
6.090753	628.147924	7.259418
5.821620	627.940785	7.264422
5.949950	623.830324	7.269427
6.037664	628.869808	7.274432
6.017321	624.176946	7.279437
6.035539	632.612344	7.284442
5.957532	624.248615	7.289446
5.956005	617.559491	7.294451
5.865400	624.769657	7.299456
5.683752	624.258728	7.304461
6.017026	623.954589	7.309466
6.093092	626.837877	7.314470
6.015045	627.159937	7.319475
6.072713	622.140779	7.324480
5.564479	631.548634	7.329485
6.017711	619.112212	7.334490
5.945247	632.696265	7.339494
5.936379	627.228318	7.344499
5.714573	631.660336	7.349504
5.986988	632.527433	7.354509
6.026381	629.005173	7.359514
5.430311	632.540488	7.364518
5.480812	626.880366	7.369523
5.832459	629.405033	7.374528
5.660019	652.317017	7.379533
5.974380	649.684616	7.384538
5.870663	663.024430	7.389542
5.932654	662.636550	7.394547
5.937703	661.318359	7.399552
6.081951	665.351916	7.404557
5.793646	657.457937	7.409562
5.621894	663.357397	7.414566
5.930471	660.861722	7.419571
5.771557	663.280710	7.424576
6.106686	659.207430	7.429581
5.968939	661.498587	7.434586
5.662558	666.299836	7.439590
5.983240	658.561153	7.444595
5.871016	666.584021	7.449600
5.824412	666.222018	7.454605
5.686663	659.251925	7.459610
6.018669	670.771928	7.464614
6.127683	650.567883	7.469619
5.751906	659.251282	7.474624
5.986219	663.862344	7.479629
6.205637	657.182791	7.484634
6.029779	657.800881	7.489638
5.961606	654.023308	7.494643
6.104598	651.016315	7.499648
5.661936	656.902618	7.504653
5.954027	661.497796	7.509658
6.133702	659.132401	7.514662
6.080562	655.257615	7.519667
6.093893	654.166968	7.524672
5.868362	645.715174	7.529677
6.112764	631.846683	7.534682
5.639627	631.839885	7.539686
5.930697	622.967859	7.544691
5.788736	632.922079	7.549696
5.657214	638.879201	7.554701
6.357488	651.757877	7.559706
6.192402	652.666248	7.564710
6.110860	633.366427	7.569715
5.729670	628.529666	7.574720
5.789735	625.628372	7.579725
5.883872	628.603391	7.584730
5.472559	622.770706	7.589734
5.590922	638.870442	7.594739
6.071132	654.558214	7.599744
6.410002	658.554408	7.604749
6.151173	644.333120	7.609754
6.109761	637.062911	7.614758
5.952754	632.438462	7.619763
5.662079	634.525630	7.624768
5.977469	639.916175	7.629773
6.004884	633.459457	7.634778
5.601952	630.259889	7.639782
5.716274	628.526158	7.644787
6.083775	631.946103	7.649792
5.748481	634.234844	7.654797
6.052805	646.489972	7.659802
5.954913	643.338950	7.664806
6.199173	637.350723	7.669811
5.943527	630.765644	7.674816
5.832406	620.825511	7.679821
5.845863	622.738381	7.684826
5.639860	631.018306	7.689830
5.821636	622.593400	7.694835
5.808452	651.455689	7.699840
5.864169	651.949387	7.704845
6.014596	660.995188	7.709850
5.724714	668.269557	7.714854
6.170661	660.802589	7.719859
6.069220	668.779072	7.724864
6.056339	657.571104	7.729869
5.948867	638.586976	7.734874
5.771887	643.142609	7.739878
6.049314	633.541094	7.744883
6.032960	627.274759	7.749888
5.736496	628.550233	7.754893
5.899191	624.758115	7.759898
5.964249	626.750848	7.764902
5.791801	619.647985	7.769907
5.372940	642.182006	7.774912
5.914789	650.726066	7.779917
6.170251	654.279028	7.784922
5.878120	663.681900	7.789926
6.203760	652.265132	7.794931
6.184833	652.134567	7.799936
6.037534	648.454957	7.804941
5.847368	634.976151	7.809946
5.762255	633.545411	7.814950
6.022453	625.450495	7.819955
6.018056	629.498004	7.824960
5.937444	631.789561	7.829965
5.928867	624.921627	7.834970
5.931581	634.486808	7.839974
5.857621	626.060836	7.844979
5.801967	627.592443	7.849984
5.928612	623.477524	7.854989
6.141057	628.001814	7.859994
5.915487	625.040865	7.864998
5.705235	623.786354	7.870003
5.748703	627.185365	7.875008
5.782032	624.864341	7.880013
6.059341	635.885025	7.885018
5.640528	633.429696	7.890022
5.924815	630.363391	7.895027
6.075367	650.400296	7.900032
5.645334	652.486075	7.905037
6.080091	651.752290	7.910042
5.804103	659.057506	7.915046
6.010772	654.443472	7.920051
5.848728	666.075681	7.925056
6.136901	665.428137	7.930061
6.021626	642.615286	7.935066
5.772079	642.760907	7.940070
5.921068	634.181183	7.945075
5.906499	635.432866	7.950080
5.919470	638.722077	7.955085
5.878937	644.174331	7.960090
5.976098	650.873874	7.965094
6.004307	650.240175	7.970099
5.958877	640.114307	7.975104
5.787227	640.106916	7.980109
6.032800	641.713752	7.985114
5.569467	638.672192	7.990118
6.016101	654.682039	7.995136
5.967415	660.209153	8.000154
5.770470	667.654015	8.005171
6.092037	658.314811	8.010189
6.011271	662.104826	8.015206
6.107094	653.874599	8.020224
5.777828	646.732427	8.025242
5.618428	650.818121	8.030259
5.965768	656.914649	8.035277
5.919206	663.684644	8.040294
5.988585	664.294868	8.045312
6.046357	660.506103	8.050330
6.095009	667.668573	8.055347
6.008246	664.295451	8.060365
5.853820	672.316309	8.065382
5.938360	661.107024	8.070400
5.924139	660.934685	8.075418
5.706742	668.458913	8.080435
6.103097	666.246259	8.085453
5.768358	667.077730	8.090470
5.689758	664.399670	8.095488
5.840001	665.160273	8.100506
5.815211	662.519756	8.105523
6.215198	662.132767	8.110541
5.968329	662.693403	8.115558
5.433668	655.142749	8.120576
5.867066	666.262516	8.125594
5.864478	665.669772	8.130611
6.429747	666.250233	8.135629
5.806172	666.600829	8.140646
5.927115	667.148187	8.145664
6.245740	668.639913	8.150682
6.155785	664.368162	8.155699
6.248519	664.002924	8.160717
5.846753	658.376205	8.165734
6.264945	661.312376	8.170752
6.214223	660.366603	8.175770
5.827587	657.623423	8.180787
6.066096	655.601467	8.185805
6.003083	662.444653	8.190822
6.379835	668.904403	8.195840
6.120896	659.395604	8.200858
6.022206	666.128959	8.205875
6.222713	654.775679	8.210893
6.159233	661.050473	8.215910
6.087081	666.128747	8.220928
6.098292	660.239946	8.225946
5.876519	683.953689	8.230963
6.056009	689.787100	8.235981
5.859854	689.979122	8.240998
5.973546	692.590158	8.246016
6.156543	691.835978	8.251034
6.207123	704.679308	8.256051
6.510631	695.940676	8.261069
6.378864	702.446074	8.266086
6.580484	698.646862	8.271104
6.535506	690.271045	8.276122
6.204272	678.463320	8.281139
6.264493	664.910170	8.286157
6.445584	660.352996	8.291174
6.373809	662.309350	8.296192
6.371072	656.206339	8.301210
6.017822	673.295791	8.306227
6.066445	667.119313	8.311245
6.110606	659.101563	8.316262
5.803865	663.075056	8.321280
6.321014	687.177818	8.326298
6.083712	693.316854	8.331315
6.217410	690.150903	8.336333
6.231981	700.838510	8.341350
6.410093	697.926997	8.346368
6.477069	697.717197	8.351386
6.268873	699.265071	8.356403
6.578708	684.126169	8.361421
6.369892	673.231977	8.366438
6.229594	668.448120	8.371456
6.451559	663.455068	8.376474
6.081893	665.588308	8.381491
6.060977	680.337830	8.386509
6.200855	690.749182	8.391526
6.555867	698.286104	8.396544
6.681657	698.180730	8.401562
6.157582	690.834986	8.406579
6.546297	673.116648	8.411597
6.511426	678.421809	8.416614
6.120306	672.594909	8.421632
6.290887	673.128535	8.426650
6.147142	698.102528	8.431667
6.476204	693.340141	8.436685
6.320134	697.159564	8.441702
6.396953	705.933434	8.446720
6.252659	699.239318	8.451738
6.579924	707.713461	8.456755
6.613391	697.736946	8.461773
6.621085	703.868876	8.466790
6.208995	689.987647	8.471808
6.460293	689.617408	8.476826
6.210432	700.765711	8.481843
6.534307	707.368085	8.486861
6.471605	704.181509	8.491878
6.343730	705.427910	8.496896
6.566876	695.778232	8.501914
6.197743	701.244262	8.506931
6.452291	701.049852	8.511949
6.372371	701.964708	8.516966
6.482735	706.432882	8.521984
6.823135	703.611022	8.527002
6.373351	708.922704	8.532019
6.456162	710.210982	8.537037
6.417695	701.848647	8.542054
6.185386	705.520076	8.547072
6.394749	697.635962	8.552090
6.166256	708.270526	8.557107
6.256232	700.614437	8.562125
6.531420	696.868393	8.567143
6.078235	703.829753	8.572160
6.459271	696.151841	8.577178
6.238742	706.508723	8.582195
6.241777	702.813653	8.587213
6.509360	714.412462	8.592231
6.350697	740.002738	8.597248
6.914720	736.420256	8.602266
6.482703	732.337016	8.607283
6.388278	734.201073	8.612301
6.440776	733.942491	8.617319
6.333814	735.046857	8.622336
6.556965	732.079850	8.627354
6.944873	738.845639	8.632371
6.698061	742.185639	8.637389
6.662123	739.550892	8.642407
6.230144	742.420405	8.647424
6.423099	731.357279	8.652442
6.724921	737.599165	8.657459
6.767737	741.814377	8.662477
6.574323	725.744660	8.667495
6.315530	732.582900	8.672512
6.341839	728.035986	8.677530
6.588782	736.495102	8.682547
6.555866	735.972335	8.687565
6.588125	735.153751	8.692583
6.451348	740.010088	8.697600
6.375896	735.750087	8.702618
6.071337	740.877110	8.707635
6.431395	760.523576	8.712653
6.759253	759.497385	8.717671
6.860108	775.505502	8.722688
6.835539	769.345435	8.727706
6.818667	775.101167	8.732723
6.580478	753.588342	8.737741
6.753332	758.324120	8.742759
6.446705	767.541034	8.747776
6.762441	765.445254	8.752794
6.841377	772.924788	8.757811
6.774577	768.936165	8.762829
6.776590	772.523532	8.767847
6.705299	773.747576	8.772864
6.808186	775.842333	8.777882
6.709570	774.178539	8.782899
6.554930	775.830538	8.787917
6.814429	772.595707	8.792935
6.451675	776.045068	8.797952
6.889046	776.369170	8.802970
6.850276	771.014561	8.807987
6.701729	769.807437	8.813005
6.829874	770.275658	8.818023
6.394915	784.988736	8.823040
6.772503	774.569770	8.828058
6.489242	782.476201	8.833075
6.575271	776.976913	8.838093
6.553058	778.079450	8.843111
6.737577	780.755539	8.848128
6.834332	776.211117	8.853146
6.633432	778.175091	8.858163
6.775840	780.928623	8.863181
6.856211	778.904889	8.868199
6.612435	793.895746	8.873216
6.621946	800.780524	8.878234
6.396064	807.140143	8.883251
6.583085	803.793693	8.888269
6.681908	801.851542	8.893287
6.321160	809.907032	8.898304
6.681906	803.022545	8.903322
6.795929	795.893108	8.908339
7.038589	808.930686	8.913357
7.066683	802.953607	8.918375
7.216618	812.146509	8.923392
7.054026	801.312679	8.928410
7.061608	802.517365	8.933427
7.139395	798.990985	8.938445
7.055916	800.200121	8.943463
7.062099	803.523826	8.948480
7.028904	803.741222	8.953498
7.158556	799.059069	8.958515
7.050099	802.747410	8.963533
7.088947	794.493868	8.968551
6.695365	807.371077	8.973568
7.289181	798.796898	8.978586
7.086286	809.199745	8.983603
6.865057	803.410798	8.988621
7.046040	801.247177	8.993639
6.603586	799.913930	8.998656
6.843837	807.362435	9.003674
7.021421	805.251342	9.008691
7.014026	804.613722	9.013709
7.005538	798.621050	9.018727
6.942736	809.605389	9.023744
7.156031	811.377552	9.028762
6.973844	808.247355	9.033779
7.057346	807.852543	9.038797
7.400901	803.437704	9.043815
6.599451	810.106017	9.048832
6.867285	805.075798	9.053850
6.973651	805.723995	9.058867
6.957834	831.228956	9.063885
7.338900	844.537330	9.068903
7.117861	846.106636	9.073920
7.018308	838.215738	9.078938
7.177612	838.629590	9.083955
7.010091	847.690450	9.088973
7.590074	833.311349	9.093991
7.160076	826.167273	9.099008
6.965328	816.896946	9.104026
7.483800	818.289847	9.109043
6.984288	803.675393	9.114061
7.118696	808.037258	9.119079
6.908996	811.864015	9.124096
7.038436	827.257247	9.129114
7.175848	842.042904	9.134131
7.091727	843.587961	9.139149
7.431873	832.548810	9.144167
7.180867	841.925840	9.149184
7.253372	837.481080	9.154202
7.152231	841.872121	9.159219
7.300540	843.971569	9.164237
7.177865	833.833433	9.169255
7.209469	834.007029	9.174272
7.102904	842.475930	9.179290
7.133090	841.930899	9.184307
7.028032	836.326234	9.189325
7.456056	836.795973	9.194343
7.158519	840.521148	9.199360
7.231813	838.704474	9.204378
7.276206	836.070580	9.209395
6.659915	843.543241	9.214413
6.914906	836.942381	9.219431
7.079763	840.094942	9.224448
7.144970	838.424875	9.229466
7.342942	832.825930	9.234483
7.229612	843.258453	9.239501
7.756075	841.148237	9.244519
7.237732	843.594296	9.249536
7.093501	844.450129	9.254554
7.328674	838.882422	9.259571
7.206134	855.304764	9.264589
7.393014	860.457127	9.269607
7.673985	859.421372	9.274624
7.175317	856.910873	9.279642
7.352339	853.103099	9.284659
7.184521	862.931302	9.289677
7.246244	866.221020	9.294695
7.232424	865.121098	9.299712
6.912728	860.682625	9.304730
7.096620	859.210213	9.309747
7.316516	868.824219	9.314765
7.185149	864.845871	9.319783
7.365063	860.798258	9.324800
7.062192	865.277041	9.329818
7.330655	867.260142	9.334835
7.111832	872.164358	9.339853
7.380798	890.272998	9.344871
7.502421	895.525152	9.349888
7.350956	900.332005	9.354906
7.506100	895.260973	9.359923
7.400952	907.636189	9.364941
7.580511	899.665967	9.369959
7.301510	906.850922	9.374976
7.172832	912.817732	9.379994
7.727233	890.999450	9.385011
7.300885	901.583451	9.390029
7.328772	894.963093	9.395047
7.109125	903.982226	9.400064
7.329674	903.685182	9.405082
7.541682	906.134310	9.410099
7.185809	904.888285	9.415117
7.496746	905.925423	9.420135
7.511800	912.057791	9.425152
7.295990	909.846486	9.430170
7.539319	908.490206	9.435187
7.625696	934.964982	9.440205
7.873865	935.517658	9.445223
7.704436	933.129778	9.450240
7.377886	920.592778	9.455258
7.511253	918.884645	9.460275
7.455421	937.469945	9.465293
7.725016	929.772974	9.470311
7.887253	938.808409	9.475328
7.662130	939.555995	9.480346
7.728898	931.059973	9.485363
7.645998	923.743807	9.490381
7.552070	928.039587	9.495399
7.816881	928.866659	9.500416
7.470939	934.878513	9.505434
7.718061	930.643775	9.510451
7.825633	940.935453	9.515469
7.579073	929.874111	9.520487
7.867298	935.372298	9.525504
7.645539	935.482741	9.530522
7.893771	925.743336	9.535539
7.754207	927.492849	9.540557
8.081184	925.893197	9.545575
7.931207	912.513218	9.550592
7.559677	906.313316	9.555610
7.986914	905.746620	9.560627
7.669643	896.993364	9.565645
7.720556	904.554371	9.570663
7.731523	903.815285	9.575680
7.378439	910.771970	9.580698
7.562656	916.773574	9.585715
8.068525	933.123030	9.590733
7.705263	931.282189	9.595751
7.863277	925.686679	9.600768
7.794749	926.865398	9.605786
8.141575	929.286691	9.610803
7.722562	923.656432	9.615821
7.847938	914.302718	9.620839
8.055185	920.778441	9.625856
7.808143	917.775099	9.630874
8.235756	902.619629	9.635891
7.916429	909.407344	9.640909
7.847188	909.755115	9.645927
7.976715	907.811409	9.650944
8.009703	903.658595	9.655962
8.092901	900.856853	9.660979
8.064685	902.452891	9.665997
8.017432	905.170141	9.671015
8.007060	899.484027	9.676032
7.668409	902.414093	9.681050
7.990459	903.181687	9.686067
8.100015	909.194865	9.691085
8.101372	906.765715	9.696103
7.819291	906.508211	9.701120
7.619537	905.777646	9.706138
8.043423	900.093235	9.711155
7.776819	909.522885	9.716173
7.966561	911.296598	9.721191
7.820408	904.867255	9.726208
7.806818	908.517077	9.731226
7.828588	902.561872	9.736243
7.973385	907.434619	9.741261
7.668565	907.854473	9.746279
7.980111	914.023169	9.751296
8.165243	935.527879	9.756314
8.145631	931.096379	9.761331
7.798952	921.335819	9.766349
7.881073	927.813370	9.771367
8.192901	930.050310	9.776384
8.086577	934.965834	9.781402
8.203749	933.261562	9.786419
8.059332	938.858957	9.791437
8.380434	936.285122	9.796455
8.154767	921.286245	9.801472
7.671252	927.357885	9.806490
8.293702	926.384467	9.811507
8.502816	930.670218	9.816525
8.495462	923.597042	9.821543
8.302439	912.348507	9.826560
8.176964	915.054698	9.831578
8.112540	906.510733	9.836595
7.940430	906.591301	9.841613
7.800195	910.950254	9.846631
8.057940	902.728905	9.851648
7.670584	912.860414	9.856666
8.196570	922.945786	9.861683
8.075249	930.827835	9.866701
7.998721	939.667389	9.871719
8.055501	935.470077	9.876736
8.578080	940.205078	9.881754
8.445329	934.498669	9.886771
8.234075	937.808807	9.891789
7.995089	940.122795	9.896807
8.105408	942.748998	9.901824
7.939795	943.818605	9.906842
8.257890	931.781504	9.911859
8.229838	934.720372	9.916877
8.054196	937.922649	9.921895
8.379049	929.984254	9.926912
8.228872	934.749567	9.931930
8.342973	938.336913	9.936947
8.367755	942.157152	9.941965
8.195529	941.775160	9.946983
8.659392	942.753119	9.952000
8.012260	943.097778	9.957018
8.298348	938.133388	9.962035
8.375082	927.920830	9.967053
8.068362	938.228363	9.972071
8.663327	933.337226	9.977088
8.472732	934.977480	9.982106
8.515388	927.010626	9.987123
8.660331	941.219960	9.992141
8.405703	943.018057	9.997159
8.831850	931.998844	10.002176
8.358646	946.978634	10.007194
8.026515	940.028918	10.012211
8.349463	934.020281	10.017229
8.168087	938.582503	10.022247
8.560363	940.007731	10.027264
8.377247	939.239371	10.032282
8.225663	937.533152	10.037299
8.759378	933.680066	10.042317
8.341314	942.541538	10.047335
8.556703	938.276622	10.052352
8.180410	940.884203	10.057370
8.487570	944.141166	10.062387
8.330216	940.981240	10.067405
8.174261	941.757133	10.072423
8.435671	938.815640	10.077440
8.265951	954.393181	10.082458
8.413270	943.017004	10.087475
8.365751	941.676999	10.092493
8.108576	943.830227	10.097511
8.537711	960.782552	10.102528
8.303678	973.116568	10.107546
8.655209	974.145020	10.112563
8.559628	974.571561	10.117581
8.250672	976.795964	10.122599
8.778197	978.817277	10.127616
9.009057	976.282788	10.132634
9.012573	968.990478	10.137651
8.830109	953.531678	10.142669
8.584530	948.310465	10.147687
8.266900	945.515255	10.152704
8.212094	955.853519	10.157722
8.143938	966.027472	10.162739
8.409419	976.673716	10.167757
8.163845	979.410043	10.172775
8.634662	975.904358	10.177792
8.517802	985.950568	10.182810
8.124899	983.136323	10.187827
8.273324	973.590575	10.192845
8.292549	984.874433	10.197863
8.709511	996.691620	10.202880
8.755616	1016.317178	10.207898
8.583998	1013.421400	10.212915
9.080005	1001.384309	10.217933
9.081345	1018.736665	10.222951
9.002748	998.527335	10.227968
8.807371	988.296417	10.232986
8.666535	988.785175	10.238003
8.824377	984.089243	10.243021
8.727759	985.450564	10.248039
8.830416	976.424971	10.253056
8.619724	979.201976	10.258074
8.749369	972.939915	10.263091
9.147334	983.910667	10.268109
8.932625	984.807312	10.273127
9.178112	973.175101	10.278144
8.685071	985.709494	10.283162
8.629847	977.882048	10.288179
8.699863	979.759451	10.293197
8.564120	976.355397	10.298215
8.972322	975.001727	10.303232
8.931438	974.761362	10.308250
8.760710	978.799807	10.313267
9.006787	975.833289	10.318285
9.046450	978.134993	10.323303
8.847972	978.018754	10.328320
8.688001	978.505956	10.333338
8.279564	981.702702	10.338355
9.024559	994.520638	10.343373
8.689348	1011.990923	10.348391
8.653611	1004.906664	10.353408
8.917801	1014.325243	10.358426
8.880018	1014.482774	10.363443
8.849656	1011.044726	10.368461
8.403429	1013.191084	10.373479
8.838316	1017.605999	10.378496
8.877235	1017.848461	10.383514
8.816496	1019.333366	10.388531
8.879697	1007.957687	10.393549
8.930654	1015.452207	10.398567
9.061445	1012.869326	10.403584
9.113912	1013.934317	10.408602
9.015796	1015.334469	10.413619
9.065829	1019.131649	10.418637
8.855191	1016.409255	10.423655
8.924348	1015.126690	10.428672
8.906957	1015.295804	10.433690
9.057300	1017.182349	10.438707
8.925604	1011.152128	10.443725
8.497156	1027.462326	10.448743
8.874739	1043.186711	10.453760
8.753817	1044.410334	10.458778
8.803649	1046.599738	10.463795
8.932810	1049.354331	10.468813
9.285903	1053.115896	10.473831
9.350441	1045.451646	10.478848
9.141177	1053.391233	10.483866
8.962636	1048.557689	10.488883
9.240000	1043.113625	10.493901
9.455624	1046.778667	10.498919
9.331449	1050.062204	10.503936
9.233011	1048.444806	10.508954
9.258825	1052.612920	10.513971
9.386088	1052.508481	10.518989
9.366954	1061.690162	10.524007
9.232032	1047.802079	10.529024
9.154590	1046.872517	10.534042
8.917337	1056.437154	10.539059
9.461728	1054.254259	10.544077
9.331242	1058.815569	10.549095
8.940634	1057.939443	10.554112
9.064371	1053.299137	10.559130
9.082220	1058.383499	10.564147
9.122511	1054.000310	10.569165
9.114096	1054.907282	10.574183
9.144610	1061.195016	10.579200
9.196191	1052.130990	10.584218
9.211104	1056.566256	10.589235
9.372366	1040.952417	10.594253
9.519283	1052.492332	10.599271
9.221391	1049.421797	10.604288
9.332998	1042.450516	10.609306
9.342248	1043.676597	10.614323
9.328699	1045.988698	10.619341
9.372023	1055.172629	10.624359
9.450590	1047.598178	10.629376
9.156252	1049.020593	10.634394
9.184387	1058.912528	10.639411
9.479689	1065.162713	10.644429
9.605276	1080.026144	10.649447
9.214688	1064.460366	10.654464
9.589019	1064.084310	10.659482
9.438248	1071.659507	10.664499
9.357043	1076.431157	10.669517
9.367107	1079.610583	10.674535
9.284173	1081.904259	10.679552
9.557013	1074.394075	10.684570
9.567037	1085.598430	10.689587
9.567235	1082.695445	10.694605
9.294524	1090.542018	10.699623
9.637267	1080.673483	10.704640
9.676621	1079.621037	10.709658
9.596237	1084.742148	10.714675
9.668459	1082.003214	10.719693
9.574996	1079.219280	10.724711
9.421977	1079.049450	10.729728
9.661454	1080.347246	10.734746
9.452295	1084.623571	10.739763
9.628558	1077.827780	10.744781
9.878978	1088.993508	10.749799
9.443095	1070.681380	10.754816
9.812861	1066.071583	10.759834
9.574588	1061.247927	10.764851
9.554833	1052.571685	10.769869
9.650410	1056.187322	10.774887
9.661754	1068.259919	10.779904
9.777580	1059.357290	10.784922
9.321514	1066.528335	10.789939
9.636038	1073.607201	10.794957
9.634480	1081.331308	10.799975
9.538120	1081.025328	10.804992
9.773412	1083.886363	10.810010
9.338763	1092.381781	10.815027
9.404133	1086.324406	10.820045
9.769672	1096.720706	10.825063
9.728136	1091.094013	10.830080
10.006254	1080.366524	10.835098
9.380893	1079.899340	10.840115
9.585187	1088.304690	10.845133
9.578579	1090.616829	10.850151
9.750639	1087.001546	10.855168
9.909379	1088.594200	10.860186
9.535179	1095.991457	10.865203
9.716644	1083.225317	10.870221
9.856912	1094.962421	10.875239
9.551674	1090.275432	10.880256
9.639703	1077.606263	10.885274
9.444024	1093.321308	10.890291
9.799582	1103.546437	10.895309
10.039571	1112.673818	10.900327
9.800242	1115.504013	10.905344
9.707267	1096.048882	10.910362
9.394199	1113.423885	10.915379
9.864743	1119.257681	10.920397
9.814486	1119.835376	10.925415
9.609582	1128.817159	10.930432
9.779623	1130.492588	10.935450
9.892816	1121.755316	10.940467
9.647469	1120.321683	10.945485
9.787070	1126.695312	10.950503
9.711015	1127.170196	10.955520
9.900458	1121.752083	10.960538
9.545609	1128.188700	10.965555
9.904471	1134.682710	10.970573
9.725986	1146.332487	10.975591
9.908796	1150.646276	10.980608
10.170290	1155.229705	10.985626
10.170470	1161.594943	10.990643
9.982949	1158.894286	10.995661
10.172229	1158.822882	11.000679
10.214792	1162.148513	11.005696
10.389250	1146.616632	11.010714
9.914092	1132.050983	11.015731
10.345825	1125.637260	11.020749
9.993688	1119.360441	11.025767
9.867908	1127.305924	11.030784
10.263075	1130.094036	11.035802
9.966442	1122.564361	11.040819
9.806790	1131.487866	11.045837
10.340635	1140.827615	11.050855
10.347782	1156.711097	11.055872
10.427783	1145.690005	11.060890
10.201191	1127.628181	11.065907
10.090505	1128.954050	11.070925
10.151784	1129.732558	11.075943
9.980096	1131.081915	11.080960
10.075808	1127.802091	11.085978
9.903762	1140.528323	11.090995
10.570623	1155.759261	11.096013
10.310978	1150.815891	11.101031
10.229889	1135.975141	11.106048
10.057361	1130.950030	11.111066
10.112779	1141.563855	11.116083
10.157568	1145.021786	11.121101
10.585208	1150.228073	11.126119
10.228920	1168.401609	11.131136
10.563329	1153.319597	11.136154
10.049266	1140.344982	11.141171
10.427615	1146.629083	11.146189
10.461108	1136.614882	11.151207
10.171692	1140.453346	11.156224
10.213791	1144.482965	11.161242
10.573603	1158.779745	11.166259
10.491828	1147.846071	11.171277
10.276012	1135.123240	11.176295
10.143702	1129.065910	11.181312
10.244587	1152.679295	11.186330
10.265927	1155.022248	11.191347
10.129477	1161.610894	11.196365
10.490696	1147.647250	11.201383
10.289373	1158.849258	11.206400
10.298346	1167.185425	11.211418
10.430910	1155.545009	11.216435
10.229247	1151.649880	11.221453
10.267784	1150.879839	11.226471
10.106247	1158.196633	11.231488
10.997164	1156.407899	11.236506
10.281184	1148.577984	11.241523
10.361019	1160.432623	11.246541
10.655587	1152.503855	11.251559
10.335637	1160.864964	11.256576
10.221511	1143.824230	11.261594
10.456973	1155.987729	11.266611
10.383272	1160.223532	11.271629
10.638222	1157.516526	11.276647
10.350677	1165.530943	11.281664
10.324255	1159.628501	11.286682
10.582931	1173.262141	11.291699
10.415495	1184.418399	11.296717
10.568855	1185.241502	11.301735
10.416138	1193.215495	11.306752
10.419784	1189.230846	11.311770
10.756144	1191.585412	11.316787
10.599964	1202.257154	11.321805
10.769378	1195.642757	11.326823
10.523359	1192.038814	11.331840
10.715559	1192.324398	11.336858
11.030962	1195.206830	11.341875
10.572769	1197.948092	11.346893
10.605065	1204.085200	11.351911
10.675815	1205.807001	11.356928
10.593782	1200.044065	11.361946
10.761964	1195.934530	11.366963
10.723231	1193.388749	11.371981
11.040216	1201.840851	11.376999
10.435474	1205.494549	11.382016
10.716502	1192.271686	11.387034
10.999780	1189.342666	11.392051
10.506655	1191.163359	11.397069
10.282148	1190.653014	11.402087
10.468456	1200.819231	11.407104
10.920212	1191.791211	11.412122
10.974546	1201.180093	11.417139
10.624967	1193.255619	11.422157
10.886548	1191.973849	11.427175
10.714866	1202.872169	11.432192
10.851593	1195.122270	11.437210
10.920861	1199.409209	11.442227
10.607198	1190.279214	11.447245
10.826256	1195.114951	11.452263
10.259422	1206.972391	11.457280
10.755267	1214.306325	11.462298
10.884494	1213.138595	11.467315
10.718668	1232.371187	11.472333
11.216765	1222.911077	11.477351
10.563111	1224.201679	11.482368
10.929463	1229.866556	11.487386
11.134436	1227.048920	11.492403
10.675054	1238.283485	11.497421
10.859004	1226.533327	11.502439
10.836342	1226.084434	11.507456
10.900355	1229.092361	11.512474
11.031088	1230.742422	11.517491
10.652854	1225.449779	11.522509
10.847488	1228.101043	11.527527
10.804433	1226.049662	11.532544
10.963852	1230.438211	11.537562
11.123207	1248.625264	11.542579
11.009039	1257.775949	11.547597
11.083925	1254.824343	11.552615
11.283505	1258.267295	11.557632
11.129522	1256.367741	11.562650
11.304084	1256.612940	11.567667
11.171127	1251.214710	11.572685
11.010938	1253.302313	11.577703
10.883711	1258.342264	11.582720
10.990310	1258.003456	11.587738
11.140034	1249.997841	11.592755
11.002056	1266.228295	11.597773
10.895511	1254.588034	11.602791
11.000659	1268.875122	11.607808
10.885109	1261.001225	11.612826
11.306551	1260.624845	11.617843
11.389512	1258.822268	11.622861
11.190969	1257.525356	11.627879
11.098726	1260.538694	11.632896
11.016897	1260.201565	11.637914
11.181910	1252.290264	11.642931
11.104589	1261.373433	11.647949
11.487728	1258.809351	11.652967
11.467712	1261.999306	11.657984
11.292589	1267.277502	11.663002
11.572146	1262.658178	11.668019
11.604464	1270.993291	11.673037
11.458007	1261.514705	11.678055
11.337736	1259.199735	11.683072
11.152575	1263.755198	11.688090
11.338921	1257.298204	11.693107
11.126167	1265.425480	11.698125
11.268035	1261.037221	11.703143
11.530195	1258.879386	11.708160
10.878763	1271.778026	11.713178
11.547808	1280.200607	11.718195
11.416955	1301.565636	11.723213
11.782650	1290.066823	11.728231
11.548539	1299.961790	11.733248
11.329441	1294.759696	11.738266
11.768066	1286.830231	11.743283
12.016632	1285.197073	11.748301
11.444373	1266.712421	11.753319
11.464860	1271.943264	11.758336
11.319661	1256.416574	11.763354
11.492636	1258.747029	11.768371
11.148752	1277.879246	11.773389
11.495568	1284.786723	11.778407
11.662075	1290.226456	11.783424
11.562622	1296.198808	11.788442
11.748666	1287.330483	11.793459
11.451280	1289.223887	11.798477
11.429412	1292.988159	11.803495
11.523611	1288.816445	11.808512
11.473117	1290.389834	11.813530
11.660540	1294.088738	11.818547
11.698025	1295.551497	11.823565
11.755654	1289.432728	11.828583
11.439981	1297.366046	11.833600
11.227957	1290.685252	11.838618
11.631815	1290.187376	11.843635
11.477441	1290.792162	11.848653
11.452888	1291.296710	11.853671
11.973422	1298.508882	11.858688
11.466538	1299.185825	11.863706
11.848869	1290.200348	11.868723
11.756561	1300.322614	11.873741
11.814063	1295.991230	11.878759
11.857024	1299.670360	11.883776
11.515457	1297.765253	11.888794
11.886001	1296.124885	11.893811
11.583993	1321.270573	11.898829
11.659030	1322.234211	11.903847
11.643749	1325.895828	11.908864
11.876831	1335.615024	11.913882
11.941703	1329.993850	11.918899
11.665783	1338.553665	11.923917
11.944523	1325.295241	11.928935
12.292493	1325.995968	11.933952
11.710638	1331.926965	11.938970
12.418497	1328.067779	11.943987
12.071854	1327.161129	11.949005
12.057584	1321.962899	11.954023
12.247502	1327.620418	11.959040
11.995079	1306.631615	11.964058
12.066327	1302.501491	11.969075
11.907350	1308.488430	11.974093
12.151433	1294.847985	11.979111
12.083746	1298.890707	11.984128
11.934018	1301.697436	11.989146
11.975011	1288.602035	11.994163
11.738604	1296.561201	11.999181
11.994962	1318.489676	12.004199
12.109570	1326.729302	12.009216
12.059315	1327.620778	12.014234
12.184592	1326.387554	12.019251
12.079911	1332.950933	12.024269
12.253175	1333.888462	12.029287
12.133928	1336.076774	12.034304
11.972211	1345.895216	12.039322
12.166747	1342.004504	12.044339
12.182592	1344.710199	12.049357
11.862565	1338.845289	12.054375
12.041497	1335.974467	12.059392
11.732643	1347.594804	12.064410
12.012043	1337.798013	12.069427
11.854720	1343.189820	12.074445
12.015435	1334.462669	12.079463
12.507414	1343.518534	12.084480
12.004600	1346.630984	12.089498
11.918608	1340.172600	12.094515
11.783649	1339.082076	12.099533
11.937527	1349.000615	12.104551
12.089197	1355.571156	12.109568
12.432553	1358.802528	12.114586
12.211750	1361.278523	12.119603
11.871978	1366.850157	12.124621
12.143081	1371.537175	12.129639
12.953474	1364.952775	12.134656
12.170824	1373.685501	12.139674
12.326514	1365.563879	12.144691
12.316864	1366.111236	12.149709
12.193070	1370.408541	12.154727
12.270867	1359.860883	12.159744
11.971045	1366.717612	12.164762
12.124521	1363.543132	12.169779
12.206688	1376.963667	12.174797
12.302492	1384.698178	12.179815
12.524505	1389.521676	12.184832
12.222800	1394.451198	12.189850
12.244462	1398.220098	12.194867
12.262332	1403.910073	12.199885
12.363584	1402.116262	12.204903
12.677631	1399.410058	12.209920
12.278849	1410.906754	12.214938
12.608967	1397.870073	12.219955
12.836528	1403.529653	12.224973
12.598657	1404.780939	12.229991
12.829220	1401.112195	12.235008
12.524378	1406.013894	12.240026
12.648076	1397.932986	12.245043
12.468096	1398.140053	12.250061
12.652558	1413.657430	12.255079
12.453213	1406.563075	12.260096
12.814383	1400.649109	12.265114
12.610294	1398.510988	12.270131
12.673761	1402.666662	12.275149
12.630047	1404.162562	12.280167
12.778121	1409.811686	12.285184
12.526213	1400.787875	12.290202
12.506704	1397.473139	12.295219
12.630698	1408.698222	12.300237
12.408816	1405.481172	12.305255
12.975770	1400.992950	12.310272
12.966979	1408.204645	12.315290
12.961613	1406.722581	12.320307
12.789359	1401.596944	12.325325
12.708044	1403.028600	12.330343
12.784313	1398.302352	12.335360
12.762178	1405.339092	12.340378
12.892539	1399.588939	12.345395
12.887857	1405.992877	12.350413
12.434012	1402.139841	12.355431
12.868809	1411.804421	12.360448
12.779402	1424.859321	12.365466
12.788822	1429.970398	12.370483
12.867681	1432.470793	12.375501
12.723737	1437.983251	12.380519
13.056140	1429.134308	12.385536
12.747329	1441.642493	12.390554
12.730445	1437.856059	12.395571
12.829984	1437.064485	12.400589
12.561642	1440.830635	12.405607
12.879232	1437.536836	12.410624
12.821702	1445.947158	12.415642
12.710854	1437.320039	12.420659
12.979211	1437.247350	12.425677
12.614903	1446.853739	12.430695
13.194566	1453.061713	12.435712
12.991278	1457.995035	12.440730
13.164571	1470.362381	12.445747
13.529935	1464.467775	12.450765
12.837134	1454.956321	12.455783
13.356775	1454.288087	12.460800
13.097212	1456.859492	12.465818
13.074970	1439.205192	12.470835
13.266793	1448.669484	12.475853
13.025305	1450.621366	12.480871
13.208511	1461.031965	12.485888
13.107609	1467.605010	12.490906
13.114894	1467.666500	12.495923
13.364597	1471.004743	12.500941
13.057526	1471.633642	12.505959
13.167045	1466.873521	12.510976
13.315918	1472.587102	12.515994
13.046811	1473.370343	12.521011
13.061461	1472.149129	12.526029
13.128482	1475.700695	12.531047
13.375884	1470.734276	12.536064
12.955959	1469.016137	12.541082
13.098017	1470.398603	12.546099
13.407348	1469.423074	12.551117
13.047641	1473.330739	12.556135
13.021867	1467.401301	12.561152
13.289371	1461.929592	12.566170
13.393920	1469.480416	12.571187
13.283536	1474.806621	12.576205
13.293419	1498.015920	12.581223
13.768290	1496.035816	12.586240
13.703437	1484.632964	12.591258
13.477527	1478.275647	12.596275
13.344325	1469.422686	12.601293
13.326158	1468.536038	12.606311
13.541933	1495.877734	12.611328
13.545232	1494.331235	12.616346
13.608084	1476.794689	12.621363
13.623968	1481.990144	12.626381
13.400253	1482.503665	12.631399
13.932673	1487.328938	12.636416
13.506487	1474.700903	12.641434
13.691342	1468.594459	12.646451
13.736285	1465.448562	12.651469
13.763523	1474.470445	12.656487
14.174668	1471.862715	12.661504
13.896349	1474.810454	12.666522
13.529417	1469.908371	12.671539
13.712170	1466.030996	12.676557
13.661948	1476.750732	12.681575
13.832082	1469.050283	12.686592
13.704269	1462.547200	12.691610
13.722467	1466.466295	12.696627
13.883753	1464.524741	12.701645
13.840272	1471.403237	12.706663
13.723111	1471.384550	12.711680
13.770184	1475.526028	12.716698
13.636785	1470.794324	12.721715
13.693836	1465.553133	12.726733
13.363281	1479.459818	12.731751
13.617417	1466.203775	12.736768
13.697675	1473.277919	12.741786
13.645969	1478.279057	12.746803
13.922743	1483.936816	12.751821
13.529290	1494.046088	12.756839
13.652817	1500.882372	12.761856
13.781767	1495.040292	12.766874
13.571999	1495.770400	12.771891
13.923905	1497.841339	12.776909
13.854933	1494.909181	12.781927
14.045188	1494.322658	12.786944
13.932865	1498.444478	12.791962
14.033844	1495.152287	12.796979
13.828022	1491.815631	12.801997
13.903414	1505.306295	12.807015
13.809364	1502.134590	12.812032
13.865109	1508.112423	12.817050
13.629658	1498.048829	12.822067
14.049609	1496.436085	12.827085
13.781224	1503.134126	12.832103
13.676775	1508.389675	12.837120
14.155780	1526.277268	12.842138
14.049300	1533.653623	12.847155
14.101410	1533.986822	12.852173
14.064046	1536.695457	12.857191
14.478885	1533.271361	12.862208
14.408904	1541.107815	12.867226
14.156975	1530.200081	12.872243
14.303047	1532.510623	12.877261
14.251756	1536.245969	12.882279
14.344572	1524.611072	12.887296
14.171800	1505.610767	12.892314
13.787898	1513.356282	12.897331
14.030815	1524.747580	12.902349
13.912174	1529.201160	12.907367
13.794729	1532.799036	12.912384
14.155810	1531.164149	12.917402
13.922271	1530.311195	12.922419
14.338815	1520.479768	12.927437
14.063403	1529.219916	12.932455
14.143206	1526.786733	12.937472
14.182825	1540.628626	12.942490
14.147112	1559.955035	12.947507
14.151603	1561.699266	12.952525
14.005003	1574.101954	12.957543
14.204392	1569.554871	12.962560
14.191764	1559.957090	12.967578
13.967756	1574.614322	12.972595
14.471189	1565.686979	12.977613
14.656616	1567.000461	12.982631
14.469792	1568.652753	12.987648
14.486496	1565.914661	12.992666
14.436920	1565.775726	12.997683
14.365531	1562.364035	13.002701
14.273474	1566.686846	13.007719
14.114197	1589.056186	13.012736
14.839556	1598.844812	13.017754
14.618523	1599.435057	13.022771
14.731465	1605.740070	13.027789
14.770942	1609.601347	13.032807
14.535493	1602.401070	13.037824
14.962123	1589.078561	13.042842
14.508858	1585.294281	13.047859
14.725029	1571.571602	13.052877
14.502849	1588.555704	13.057895
14.795236	1599.556582	13.062912
14.984110	1594.372651	13.067930
14.080899	1592.344770	13.072947
14.674388	1595.456422	13.077965
14.951194	1601.386659	13.082983
14.802173	1600.567736	13.088000
15.025108	1593.166750	13.093018
15.102810	1607.618537	13.098035
14.979620	1593.472511	13.103053
14.660320	1576.302289	13.108071
14.704081	1568.892797	13.113088
15.013341	1566.436963	13.118106
14.689672	1575.003239	13.123123
14.939358	1572.316325	13.128141
14.871393	1575.823734	13.133159
14.871016	1586.219937	13.138176
15.110957	1585.234633	13.143194
14.788371	1583.238551	13.148211
14.979409	1585.291261	13.153229
15.151489	1591.213247	13.158247
14.642450	1577.615779	13.163264
14.839878	1582.733172	13.168282
14.737072	1598.243188	13.173299
14.802554	1597.434806	13.178317
14.969271	1593.320291	13.183335
14.723788	1606.738986	13.188352
14.970833	1610.603290	13.193370
14.996262	1607.389335	13.198387
15.066531	1605.701026	13.203405
15.281586	1604.504487	13.208423
14.996948	1612.244635	13.213440
15.063231	1604.487302	13.218458
15.141825	1604.205094	13.223475
14.996188	1592.841919	13.228493
15.484076	1598.869482	13.233511
14.889306	1601.410990	13.238528
15.161641	1595.315206	13.243546
15.156637	1601.888962	13.248563
15.363020	1601.085198	13.253581
15.179789	1601.753829	13.258599
15.079502	1605.799668	13.263616
15.160952	1605.970530	13.268634
14.948840	1611.204967	13.273651
15.077399	1598.310553	13.278669
15.167583	1612.969727	13.283687
15.146759	1624.074853	13.288704
15.203035	1628.611306	13.293722
15.367122	1641.228344	13.298739
15.554130	1635.049037	13.303757
15.266774	1628.744747	13.308775
15.305834	1640.884458	13.313792
15.331589	1627.618855	13.318810
15.551022	1632.534195	13.323827
15.935726	1634.307202	13.328845
15.413116	1635.213140	13.333863
15.023409	1642.827001	13.338880
15.729247	1638.864139	13.343898
15.606710	1642.528238	13.348915
15.468868	1642.933842	13.353933
15.494779	1632.935933	13.358951
15.302464	1639.083637	13.363968
15.594328	1635.582246	13.368986
15.360643	1645.463188	13.374003
15.186556	1639.925177	13.379021
15.305285	1639.693014	13.384039
15.498239	1635.019025	13.389056
15.200035	1630.175588	13.394074
15.230046	1649.972327	13.399091
15.639894	1658.894341	13.404109
16.039589	1666.632211	13.409127
15.980585	1664.527900	13.414144
16.051666	1646.951217	13.419162
15.881981	1638.884519	13.424179
15.888653	1631.272084	13.429197
15.878742	1632.214376	13.434215
15.730481	1630.561466	13.439232
16.012733	1624.418753	13.444250
15.676790	1639.791041	13.449267
15.618422	1628.757483	13.454285
15.808128	1627.730495	13.459303
15.545556	1631.670932	13.464320
15.743154	1633.663113	13.469338
15.681549	1635.499401	13.474355
15.632071	1649.871107	13.479373
16.177715	1656.337949	13.484391
15.943153	1657.666659	13.489408
16.109794	1658.767905	13.494426
16.086820	1647.639495	13.499443
16.124177	1632.726687	13.504461
16.083628	1627.513810	13.509479
15.873404	1626.382186	13.514496
15.929623	1635.147395	13.519514
15.646927	1632.934463	13.524531
15.886461	1663.157169	13.529549
16.120216	1662.942572	13.534567
15.963531	1662.581215	13.539584
15.986688	1665.360559	13.544602
15.938236	1667.979715	13.549619
16.284327	1663.893351	13.554637
16.379135	1667.403745	13.559655
15.942172	1670.140784	13.564672
16.172876	1663.396354	13.569690
16.053244	1665.845406	13.574707
15.891720	1666.125011	13.579725
15.965899	1669.028190	13.584743
16.014438	1673.179321	13.589760
16.154210	1659.546383	13.594778
16.249821	1667.259413	13.599795
16.284427	1664.480543	13.604813
16.361423	1652.601320	13.609831
16.270546	1669.154316	13.614848
16.565632	1656.951963	13.619866
16.381391	1667.114889	13.624883
16.118958	1665.424584	13.629901
16.547808	1663.722161	13.634919
16.478058	1667.702328	13.639936
16.392081	1659.944198	13.644954
16.162451	1664.634308	13.649971
16.178329	1668.245176	13.654989
16.139220	1658.303293	13.660007
16.177293	1669.389643	13.665024
16.278468	1676.956875	13.670042
16.498198	1692.894282	13.675059
16.215176	1693.404639	13.680077
17.032025	1685.352889	13.685095
16.627207	1693.232271	13.690112
16.781551	1684.607554	13.695130
16.698264	1676.915112	13.700147
16.246705	1663.208837	13.705165
16.669035	1674.253210	13.710183
16.600727	1683.696157	13.715200
16.775837	1695.864956	13.720218
16.741916	1687.939135	13.725235
16.860297	1677.084147	13.730253
16.973295	1661.001694	13.735271
16.310160	1662.921459	13.740288
16.648068	1661.673469	13.745306
16.617600	1668.271943	13.750323
16.413689	1684.340522	13.755341
16.671776	1689.002627	13.760359
16.566947	1698.655570	13.765376
16.669675	1693.353588	13.770394
16.670395	1695.076805	13.775411
16.706837	1697.483480	13.780429
16.749267	1686.993427	13.785447
16.423818	1699.845914	13.790464
16.822220	1691.700464	13.795482
16.898024	1692.142343	13.800499
16.634958	1699.377777	13.805517
16.986310	1693.055483	13.810535
16.737029	1696.929561	13.815552
16.662753	1696.296682	13.820570
16.927904	1696.311532	13.825587
16.793367	1713.374563	13.830605
16.842864	1721.173604	13.835623
16.823918	1726.565462	13.840640
16.523070	1719.988563	13.845658
17.501058	1726.211787	13.850675
17.171005	1735.840240	13.855693
17.309733	1733.031515	13.860711
16.921222	1733.729029	13.865728
17.027256	1737.121044	13.870746
17.420609	1717.191288	13.875763
17.377951	1729.511924	13.880781
17.390936	1719.981457	13.885799
17.025798	1712.350241	13.890816
17.106694	1719.733842	13.895834
17.443739	1719.796236	13.900851
17.285994	1714.666911	13.905869
17.607156	1688.130600	13.910887
17.320636	1692.662817	13.915904
17.190521	1688.686805	13.920922
17.385328	1686.626286	13.925939
17.155087	1691.603908	13.930957
17.595488	1693.434234	13.935975
17.246337	1691.531120	13.940992
17.010480	1694.184071	13.946010
17.392452	1701.693396	13.951027
17.239690	1717.693696	13.956045
17.461545	1719.898408	13.961063
17.110625	1732.147262	13.966080
17.473764	1728.681291	13.971098
17.606660	1714.315974	13.976115
17.504750	1727.192882	13.981133
17.608674	1729.639174	13.986151
17.540234	1733.546306	13.991168
17.733571	1724.152899	13.996186
17.641437	1729.228136	14.001203
17.437245	1714.811554	14.006221
17.585511	1719.537524	14.011239
17.722557	1723.420861	14.016256
17.467708	1717.883991	14.021274
17.524422	1719.528646	14.026291
17.495420	1730.278901	14.031309
17.886878	1722.143247	14.036327
17.472229	1723.566747	14.041344
17.502247	1721.685483	14.046362
17.485231	1725.426616	14.051379
17.517071	1729.389187	14.056397
17.548904	1720.297728	14.061415
17.658513	1728.469498	14.066432
17.790264	1729.860781	14.071450
17.635720	1720.836800	14.076467
17.478503	1721.597979	14.081485
17.550554	1729.957073	14.086503
17.784061	1732.989785	14.091520
17.564110	1732.254256	14.096538
17.840648	1740.827919	14.101555
17.552927	1754.508068	14.106573
17.900254	1750.782110	14.111591
18.000006	1750.310567	14.116608
17.747838	1761.741902	14.121626
17.866944	1759.668319	14.126643
17.750992	1759.086433	14.131661
18.000179	1757.481471	14.136679
18.066486	1762.434809	14.141696
18.359251	1753.752879	14.146714
18.487377	1753.308134	14.151731
17.854213	1748.045716	14.156749
18.346697	1752.220201	14.161767
18.409644	1750.475214	14.166784
18.255431	1747.640983	14.171802
18.047666	1732.900170	14.176819
18.202374	1746.348774	14.181837
18.337155	1730.403195	14.186855
18.414357	1727.453872	14.191872
18.206270	1722.760444	14.196890
18.573746	1713.681909	14.201907
18.317089	1715.981219	14.206925
18.234434	1715.615082	14.211943
18.411063	1718.475319	14.216960
18.230642	1717.748992	14.221978
18.359726	1710.115853	14.226995
18.039480	1713.169005	14.232013
18.090229	1714.291809	14.237031
18.643838	1720.173103	14.242048
18.237895	1717.963246	14.247066
18.497130	1711.649507	14.252083
18.260521	1722.131379	14.257101
18.283156	1712.636720	14.262119
18.253773	1717.590143	14.267136
18.307029	1741.998930	14.272154
18.734607	1743.506973	14.277171
18.446099	1747.861186	14.282189
18.720415	1749.289492	14.287207
18.846264	1753.249887	14.292224
18.768797	1735.463844	14.297242
18.425900	1710.379604	14.302259
18.361441	1722.594396	14.307277
18.668825	1709.924608	14.312295
18.634114	1720.402572	14.317312
18.436604	1733.459491	14.322330
18.591804	1738.197312	14.327347
18.458408	1743.652224	14.332365
18.717389	1739.955467	14.337383
18.894530	1742.995940	14.342400
18.294653	1737.643762	14.347418
18.507983	1747.987359	14.352435
18.595605	1744.863865	14.357453
18.252639	1747.289285	14.362471
18.924106	1750.811682	14.367488
18.540258	1750.174161	14.372506
18.450785	1735.602733	14.377523
18.360733	1756.003353	14.382541
18.698507	1766.755099	14.387559
18.916697	1775.471910	14.392576
18.646751	1785.478238	14.397594
18.756336	1776.799859	14.402611
18.918728	1783.387703	14.407629
18.841281	1775.767474	14.412647
18.892021	1782.001363	14.417664
18.433359	1778.093910	14.422682
18.653902	1780.696097	14.427699
18.938790	1778.215133	14.432717
18.873415	1770.148021	14.437735
18.975753	1775.954460	14.442752
19.129546	1805.129819	14.447770
19.202672	1803.258730	14.452787
19.088433	1793.707947	14.457805
19.409693	1808.769988	14.462823
19.579807	1795.374035	14.467840
19.296146	1788.557644	14.472858
19.627903	1774.014849	14.477875
19.402965	1772.226589	14.482893
19.199758	1756.951528	14.487911
19.395635	1772.391781	14.492928
19.421514	1769.773394	14.497946
19.679456	1764.147650	14.502963
19.281494	1775.969678	14.507981
19.097305	1774.896330	14.512999
19.236655	1766.687442	14.518016
19.152784	1771.667622	14.523034
19.335519	1770.374847	14.528051
19.388569	1771.835861	14.533069
19.458962	1774.423542	14.538087
19.673727	1764.432461	14.543104
19.598659	1774.557693	14.548122
19.212471	1767.585060	14.553139
19.199888	1773.212890	14.558157
18.964970	1776.031842	14.563175
19.360926	1763.316634	14.568192
19.072250	1789.593163	14.573210
19.288019	1796.242646	14.578227
19.774109	1800.552456	14.583245
19.570352	1802.998532	14.588263
19.331044	1804.501271	14.593280
19.353612	1804.667714	14.598298
19.725549	1798.393150	14.603315
19.809914	1796.380828	14.608333
19.615129	1806.900714	14.613351
20.077362	1790.320917	14.618368
19.969973	1797.475891	14.623386
19.450563	1795.426548	14.628403
19.747712	1793.488832	14.633421
19.747253	1802.097378	14.638439
20.021797	1791.074321	14.643456
20.031057	1789.737044	14.648474
20.002898	1796.340702	14.653491
19.861147	1790.872479	14.658509
19.760219	1795.886988	14.663527
20.002561	1786.812203	14.668544
19.770858	1790.812135	14.673562
20.107102	1790.821512	14.678579
20.025897	1790.807105	14.683597
19.944574	1788.421431	14.688615
20.009955	1783.627185	14.693632
19.940831	1792.073472	14.698650
19.956959	1792.756734	14.703667
20.087954	1794.976504	14.708685
19.845660	1798.454958	14.713703
19.909426	1802.798092	14.718720
19.751269	1798.927485	14.723738
20.046674	1798.677086	14.728755
20.028587	1804.358989	14.733773
19.992889	1807.727246	14.738791
20.192391	1814.809358	14.743808
20.002101	1831.582929	14.748826
19.929716	1825.215005	14.753843
20.084350	1830.173817	14.758861
20.117496	1835.981895	14.763879
20.036830	1827.820827	14.768896
20.008851	1832.877599	14.773914
20.056839	1822.570789	14.778931
20.204227	1821.940565	14.783949
20.284792	1822.499771	14.788967
20.452812	1829.802067	14.793984
20.530435	1823.029769	14.799002
20.425676	1834.165087	14.804019
20.509413	1824.183069	14.809037
20.285333	1829.060501	14.814055
20.653699	1824.056615	14.819072
20.785486	1833.361791	14.824090
20.366257	1831.836017	14.829107
20.440282	1825.415894	14.834125
20.163034	1826.407588	14.839143
20.621359	1836.143342	14.844160
20.509126	1850.638226	14.849178
20.597098	1845.391394	14.854195
20.776909	1844.071144	14.859213
20.583842	1852.304915	14.864231
20.833869	1852.301404	14.869248
20.909641	1840.365940	14.874266
20.943752	1837.383969	14.879283
20.903878	1825.091678	14.884301
20.406304	1827.873821	14.889319
20.978385	1834.139900	14.894336
20.867501	1835.755628	14.899354
20.618840	1831.670076	14.904371
20.985159	1830.726427	14.909389
20.905961	1845.195757	14.914407
21.218423	1832.487233	14.919424
20.752044	1827.516464	14.924442
20.470803	1828.501732	14.929459
21.042623	1833.252479	14.934477
20.717334	1850.949228	14.939495
21.122332	1841.109275	14.944512
20.738544	1858.218073	14.949530
20.883659	1854.659045	14.954547
20.917443	1848.028250	14.959565
20.766152	1865.936756	14.964583
20.800477	1849.565164	14.969600
20.948509	1850.827775	14.974618
21.091770	1856.768809	14.979635
21.159011	1848.519062	14.984653
20.564441	1853.595653	14.989671
21.268677	1862.610374	14.994688
21.179789	1871.685972	14.999706
21.230512	1867.112634	15.004723
21.507552	1861.234082	15.009741
21.258823	1854.700858	15.014759
21.395845	1844.285980	15.019776
21.548995	1847.035562	15.024794
21.408207	1838.831688	15.029811
21.150580	1837.815774	15.034829
21.033897	1849.492062	15.039847
21.455906	1862.952802	15.044864
21.543840	1861.588316	15.049882
21.486386	1866.054695	15.054899
21.705935	1858.059646	15.059917
21.505759	1851.571533	15.064935
21.642807	1843.028728	15.069952
21.355787	1848.307539	15.074970
21.685363	1845.041593	15.079987
21.615015	1845.463977	15.085005
21.411243	1841.236734	15.090023
21.819104	1850.961957	15.095040
21.443255	1850.940832	15.100058
21.514373	1860.078509	15.105075
21.410598	1864.625000	15.110093
21.452014	1873.516812	15.115111
21.645714	1866.129987	15.120128
21.641843	1868.755573	15.125146
21.719074	1868.950759	15.130163
21.675666	1861.694148	15.135181
21.675427	1868.058170	15.140199
21.764094	1875.143310	15.145216
21.528478	1877.101751	15.150234
21.585722	1882.406241	15.155251
21.904126	1869.938045	15.160269
21.616484	1871.060600	15.165287
21.597183	1868.066995	15.170304
21.708550	1877.403532	15.175322
21.661782	1893.402208	15.180339
22.150664	1894.447350	15.185357
22.059582	1900.473273	15.190375
22.443138	1891.898280	15.195392
22.552532	1886.062049	15.200410
22.141710	1872.110255	15.205427
22.453246	1858.259719	15.210445
22.364493	1866.492758	15.215463
22.433492	1865.140069	15.220480
22.412132	1860.486150	15.225498
22.216623	1855.846504	15.230515
22.507214	1858.754038	15.235533
22.157361	1862.998361	15.240551
22.342786	1861.140164	15.245568
22.686796	1857.995056	15.250586
21.915754	1861.818570	15.255603
21.946036	1856.352543	15.260621
21.948111	1861.439781	15.265639
21.883463	1854.181179	15.270656
22.371318	1852.322507	15.275674
22.166782	1860.086520	15.280691
22.445442	1850.798594	15.285709
21.916592	1863.680175	15.290727
22.318243	1879.628200	15.295744
22.706240	1883.127492	15.300762
22.206740	1891.686444	15.305779
22.473423	1883.339082	15.310797
22.650779	1893.070220	15.315815
22.410991	1896.568753	15.320832
22.469047	1885.665341	15.325850
22.209315	1894.846411	15.330867
22.456591	1895.190606	15.335885
22.470475	1896.407325	15.340903
22.620589	1899.614513	15.345920
22.682802	1894.522720	15.350938
22.567833	1902.326253	15.355955
22.894130	1894.152875	15.360973
22.510553	1890.542020	15.365991
22.524536	1890.014597	15.371008
22.875618	1891.769186	15.376026
22.691944	1892.140653	15.381043
22.732328	1887.301694	15.386061
22.601949	1887.224957	15.391079
22.704787	1912.034862	15.396096
22.878442	1919.407135	15.401114
22.768212	1918.755002	15.406131
23.127769	1918.184523	15.411149
23.049621	1909.391881	15.416167
23.270556	1920.650888	15.421184
23.080233	1918.349387	15.426202
23.148512	1929.559664	15.431219
23.275618	1919.193230	15.436237
23.116069	1905.317513	15.441255
22.734037	1900.958354	15.446272
23.216728	1909.795615	15.451290
23.089073	1915.787835	15.456307
23.323963	1921.834982	15.461325
23.084799	1925.343654	15.466343
23.278716	1919.542233	15.471360
23.273279	1923.583863	15.476378
23.018948	1919.480722	15.481395
23.308166	1917.779349	15.486413
23.577538	1915.237940	15.491431
23.192213	1923.514217	15.496448
23.413280	1916.091339	15.501466
23.125685	1928.290882	15.506483
23.535312	1917.182767	15.511501
23.580096	1921.929086	15.516519
23.358274	1920.828889	15.521536
23.506252	1918.989879	15.526554
23.298716	1916.319569	15.531571
23.335272	1921.742461	15.536589
23.250737	1912.112669	15.541607
23.481537	1929.454813	15.546624
23.684067	1926.538242	15.551642
23.087724	1924.409100	15.556659
23.118436	1919.248104	15.561677
23.229677	1928.457918	15.566695
23.668824	1943.365526	15.571712
23.717229	1944.217470	15.576730
23.803373	1943.655653	15.581747
24.041018	1941.706514	15.586765
23.942894	1933.227409	15.591783
23.501229	1931.905344	15.596800
24.072671	1926.727635	15.601818
23.517637	1932.749692	15.606835
23.546359	1936.020693	15.611853
23.951757	1937.056041	15.616871
23.877628	1946.392629	15.621888
24.157941	1941.296593	15.626906
23.954275	1947.739218	15.631923
24.322505	1945.822391	15.636941
24.063243	1940.903114	15.641959
23.927988	1948.211987	15.646976
24.184051	1937.158817	15.651994
24.498512	1934.813879	15.657011
23.999759	1921.841189	15.662029
23.704753	1913.402573	15.667047
23.543713	1928.551688	15.672064
24.342297	1932.294027	15.677082
24.239571	1942.259377	15.682099
24.139891	1943.785071	15.687117
24.262991	1939.170198	15.692135
24.398645	1938.797431	15.697152
24.472431	1934.972238	15.702170
24.493873	1943.856375	15.707187
24.323282	1942.567373	15.712205
24.348591	1945.592085	15.717223
24.168874	1943.470718	15.722240
24.392037	1936.698285	15.727258
24.243900	1941.537978	15.732275
24.212118	1945.664688	15.737293
24.532162	1947.606711	15.742311
24.218475	1947.078036	15.747328
24.346935	1933.068377	15.752346
24.173491	1934.826762	15.757363
24.231901	1940.595655	15.762381
23.979494	1945.366394	15.767399
24.155201	1954.410820	15.772416
24.734584	1970.664159	15.777434
24.873295	1980.955307	15.782451
24.786664	1981.510710	15.787469
24.662331	1973.545384	15.792487
24.473273	1978.884789	15.797504
24.909759	1969.786804	15.802522
24.832642	1974.409623	15.807539
24.756805	1978.047168	15.812557
24.806490	1976.643337	15.817575
24.806880	1971.217654	15.822592
24.729549	1972.977843	15.827610
24.762711	1978.444232	15.832627
24.631526	1974.488797	15.837645
25.090827	1968.743017	15.842663
24.694212	1980.735846	15.847680
24.919796	1972.844860	15.852698
24.832312	1972.142501	15.857715
24.958752	1974.259112	15.862733
25.180236	1973.537083	15.867751
24.847997	1958.732808	15.872768
25.069491	1965.005423	15.877786
25.051880	1972.515697	15.882803
24.901018	1967.781614	15.887821
25.129391	1970.960503	15.892839
24.947440	1998.671318	15.897856
25.063154	1991.865867	15.902874
24.817473	1999.189114	15.907891
24.695941	1999.090044	15.912909
24.917154	2000.051566	15.917927
25.029319	1995.118007	15.922944
24.883659	1991.105121	15.927962
25.060671	2009.645660	15.932979
25.164751	2014.731410	15.937997
25.611168	2012.895331	15.943015
25.505078	2033.372594	15.948032
25.925611	2032.516416	15.953050
26.202437	2022.511744	15.958067
26.030924	1996.167524	15.963085
26.135016	1987.532851	15.968103
25.821531	1991.472360	15.973120
25.957775	1984.153657	15.978138
25.680190	1985.322586	15.983155
25.785862	1977.161684	15.988173
26.008731	1981.990739	15.993191
25.960730	1986.791421	15.998208
26.054171	1978.361672	16.003226
25.935626	1968.317388	16.008243
25.533461	1963.542244	16.013261
25.904850	1946.965514	16.018279
25.689640	1963.883908	16.023296
26.041539	1959.949660	16.028314
25.848925	1956.652842	16.033331
25.891121	1965.639462	16.038349
26.191528	1969.935581	16.043367
25.573444	1961.220906	16.048384
25.967299	1967.007883	16.053402
26.107624	1981.547287	16.058419
25.816524	1981.524725	16.063437
26.206831	1978.667208	16.068455
26.155920	1984.689267	16.073472
26.272668	1981.735709	16.078490
26.289230	1990.365556	16.083507
26.247373	1985.857517	16.088525
26.271263	1976.692024	16.093543
25.862361	1973.520393	16.098560
26.080285	1979.149496	16.103578
26.569022	1985.532592	16.108595
26.203433	1990.662253	16.113613
26.416253	1992.553927	16.118631
26.321756	1991.005069	16.123648
26.635070	1975.746226	16.128666
26.095835	1976.618713	16.133683
26.042021	1990.225686	16.138701
26.223013	1977.563620	16.143719
26.069619	1987.179507	16.148736
25.984584	1988.183081	16.153754
25.985257	1986.154673	16.158771
26.382767	1992.141058	16.163789
26.715716	2005.448557	16.168807
26.479991	2021.902290	16.173824
26.552680	2020.058807	16.178842
26.734697	2021.778021	16.183859
26.343739	2025.513039	16.188877
26.462569	2022.591808	16.193895
26.317028	2031.780033	16.198912
26.328238	2027.489183	16.203930
26.613882	2024.837972	16.208947
26.523420	2021.953762	16.213965
26.750612	2024.695445	16.218983
26.620101	2023.220660	16.224000
26.575952	2023.776509	16.229018
26.694872	2027.730249	16.234035
26.813821	2044.066213	16.239053
27.124584	2038.409576	16.244071
27.117753	2046.793715	16.249088
27.119686	2037.757417	16.254106
26.954084	2026.354709	16.259123
26.955211	2042.119616	16.264141
27.133597	2050.617184	16.269159
27.275122	2052.186410	16.274176
27.241033	2042.917091	16.279194
27.280386	2033.586795	16.284211
26.666776	2030.832920	16.289229
27.040676	2034.992080	16.294247
26.880203	2039.399976	16.299264
26.851087	2043.947541	16.304282
27.388945	2034.860684	16.309299
27.055201	2040.494945	16.314317
27.267393	2039.514602	16.319335
27.086707	2037.263851	16.324352
27.113759	2048.164497	16.329370
27.166361	2036.286658	16.334387
26.932323	2058.469047	16.339405
27.336267	2069.049805	16.344423
27.160880	2076.616573	16.349440
27.463675	2076.022811	16.354458
27.813671	2075.933059	16.359475
27.605180	2078.844148	16.364493
27.482328	2070.544265	16.369511
27.660212	2073.428772	16.374528
27.906722	2076.857048	16.379546
27.636295	2071.001362	16.384563
27.431556	2074.601219	16.389581
27.798897	2060.340069	16.394599
28.218442	2064.175134	16.399616
27.678649	2073.533006	16.404634
27.741791	2071.817086	16.409651
27.622180	2075.495369	16.414669
28.046148	2070.397549	16.419687
27.730825	2079.985977	16.424704
27.551699	2074.733692	16.429722
28.032205	2061.408553	16.434739
27.692265	2072.605036	16.439757
28.175516	2067.230857	16.444775
27.824598	2073.708943	16.449792
27.674885	2085.712147	16.454810
28.079982	2094.867885	16.459827
28.036117	2102.003424	16.464845
28.245182	2097.478996	16.469863
27.986210	2102.627653	16.474880
28.250024	2096.727975	16.479898
28.374974	2105.247807	16.484915
28.095128	2100.596463	16.489933
28.243343	2095.216731	16.494951
28.795558	2100.075930	16.499968
28.548694	2096.436480	16.504986
28.523204	2094.851774	16.510003
28.256696	2105.045144	16.515021
28.552201	2088.731233	16.520039
28.765900	2094.394543	16.525056
28.738771	2090.831308	16.530074
28.810286	2070.375246	16.535091
28.390339	2070.543317	16.540109
28.435921	2056.236633	16.545127
28.572767	2061.711078	16.550144
28.296664	2061.584848	16.555162
28.779562	2076.824720	16.560179
28.605458	2093.916374	16.565197
28.822652	2085.042439	16.570215
28.778022	2092.062348	16.575232
28.773560	2091.122211	16.580250
28.725881	2087.148194	16.585267
28.928698	2092.727083	16.590285
28.931108	2096.351304	16.595303
29.020126	2085.065448	16.600320
28.832644	2089.284911	16.605338
28.958920	2084.007245	16.610355
29.190555	2092.130651	16.615373
29.051753	2079.314762	16.620391
29.248686	2063.537688	16.625408
28.777220	2063.371761	16.630426
29.141343	2053.032919	16.635443
28.834292	2065.062950	16.640461
29.063164	2085.975772	16.645479
29.269772	2087.406661	16.650496
29.072315	2087.618992	16.655514
29.026497	2086.561292	16.660531
28.917549	2090.333484	16.665549
29.270504	2093.093330	16.670567
29.425000	2087.441686	16.675584
29.223662	2092.895766	16.680602
29.301870	2086.835090	16.685619
28.569050	2094.205193	16.690637
28.683507	2081.339881	16.695655
29.408639	2095.391984	16.700672
29.579193	2111.934835	16.705690
29.737137	2109.981551	16.710707
29.393831	2117.030460	16.715725
29.448564	2107.023141	16.720743
29.724400	2117.009773	16.725760
29.392411	2122.525658	16.730778
29.588328	2113.068597	16.735795
29.306980	2122.161250	16.740813
29.338089	2118.949399	16.745831
29.703579	2108.772898	16.750848
29.473651	2116.437696	16.755866
29.843079	2108.262183	16.760883
29.437961	2116.870196	16.765901
29.759438	2118.888384	16.770919
29.628081	2116.779064	16.775936
29.746026	2128.904912	16.780954
29.909600	2126.388076	16.785971
29.727578	2132.210636	16.790989
30.088143	2138.102800	16.796007
30.549044	2143.657473	16.801024
30.014604	2133.103196	16.806042
30.091289	2123.296569	16.811059
30.072702	2120.813050	16.816077
30.033088	2120.869710	16.821095
30.171633	2124.089886	16.826112
30.099998	2130.918609	16.831130
30.964694	2133.326778	16.836147
30.502106	2120.020756	16.841165
30.317447	2108.488463	16.846183
30.426797	2105.912891	16.851200
30.130722	2111.186990	16.856218
30.337330	2096.365792	16.861235
30.399469	2103.181405	16.866253
30.338755	2096.330319	16.871271
30.517771	2100.691461	16.876288
30.600608	2105.463426	16.881306
30.493325	2099.701581	16.886323
30.643395	2103.943891	16.891341
30.357736	2111.917533	16.896359
30.814609	2100.632955	16.901376
30.442658	2101.048597	16.906394
30.669516	2105.578595	16.911411
30.367309	2100.067147	16.916429
30.612123	2120.411609	16.921447
30.812065	2120.471907	16.926464
30.826729	2136.121672	16.931482
30.853358	2129.181695	16.936499
30.759569	2131.336767	16.941517
30.828729	2124.645663	16.946535
31.019395	2118.366345	16.951552
30.780596	2124.173107	16.956570
31.017101	2126.514433	16.961587
30.844477	2137.854915	16.966605
30.428484	2120.554033	16.971623
30.833524	2121.838282	16.976640
30.745041	2122.008550	16.981658
30.851746	2128.221105	16.986675
30.791148	2132.029397	16.991693
30.826435	2148.937219	16.996711
30.905726	2154.939750	17.001728
31.072181	2165.903616	17.006746
31.638623	2151.769654	17.011763
31.259053	2158.946244	17.016781
31.571085	2164.126351	17.021799
31.547441	2152.733508	17.026816
31.146706	2162.980247	17.031834
31.442055	2155.834335	17.036851
31.565314	2161.185077	17.041869
31.515241	2154.462129	17.046887
31.692673	2145.610492	17.051904
31.458516	2158.403354	17.056922
31.531267	2152.964837	17.061939
31.558979	2153.625724	17.066957
31.708280	2143.736585	17.071975
31.806322	2146.504401	17.076992
31.644354	2153.807952	17.082010
31.786794	2153.997462	17.087027
32.208140	2152.569863	17.092045
31.762445	2149.992497	17.097063
31.850183	2144.152668	17.102080
31.880495	2158.400998	17.107098
31.768154	2144.687728	17.112115
31.862324	2144.398206	17.117133
31.589605	2154.114668	17.122151
32.230571	2144.021663	17.127168
31.743812	2145.662659	17.132186
31.752414	2143.729377	17.137203
32.106686	2153.108141	17.142221
32.113975	2145.197311	17.147239
32.048803	2139.363121	17.152256
32.055083	2143.817055	17.157274
31.948616	2144.145426	17.162291
32.346202	2139.841350	17.167309
32.060817	2143.571905	17.172327
32.390845	2150.805791	17.177344
31.767493	2151.631190	17.182362
32.083870	2166.481782	17.187379
32.375330	2170.328636	17.192397
32.278966	2180.206073	17.197415
32.609483	2172.997635	17.202432
32.481821	2168.474223	17.207450
32.237610	2172.279859	17.212467
32.509546	2174.479494	17.217485
32.383525	2172.568503	17.222503
32.531919	2165.330383	17.227520
32.585192	2174.744045	17.232538
32.587619	2170.375867	17.237555
32.589558	2170.571715	17.242573
32.910763	2166.636593	17.247591
32.958075	2168.194267	17.252608
32.649416	2168.626989	17.257626
32.630944	2160.551907	17.262643
32.806053	2177.527160	17.267661
32.988073	2171.285868	17.272679
33.060177	2166.191167	17.277696
32.474311	2168.213551	17.282714
32.834037	2172.198712	17.287731
32.920215	2179.876551	17.292749
32.855986	2199.064770	17.297767
33.171170	2197.561044	17.302784
32.827982	2203.465440	17.307802
33.069125	2198.784878	17.312819
33.106595	2200.594982	17.317837
33.023283	2197.708374	17.322855
33.240965	2184.597528	17.327872
33.244583	2194.676142	17.332890
33.251192	2188.752878	17.337907
33.399444	2192.565183	17.342925
33.484150	2193.552473	17.347943
33.669287	2182.589224	17.352960
33.591685	2187.620863	17.357978
33.333028	2192.599018	17.362995
33.515324	2182.752423	17.368013
33.453087	2184.261702	17.373031
33.656166	2188.816529	17.378048
33.569377	2191.516533	17.383066
33.449706	2189.861190	17.388083
33.702310	2184.069638	17.393101
33.811255	2184.659592	17.398119
33.740717	2189.505409	17.403136
33.509776	2185.312099	17.408154
33.489199	2189.666947	17.413171
33.816485	2183.850823	17.418189
33.674330	2197.460401	17.423207
33.466173	2202.406181	17.428224
34.017609	2205.602094	17.433242
33.840471	2214.535412	17.438259
33.908064	2211.176550	17.443277
33.742789	2221.575682	17.448295
34.019770	2212.310656	17.453312
33.931569	2212.050153	17.458330
33.489671	2219.328041	17.463347
34.132098	2210.854499	17.468365
34.160947	2213.299915	17.473383
33.923233	2202.159030	17.478400
33.966126	2222.520922	17.483418
34.452194	2230.752667	17.488435
34.554393	2237.740846	17.493453
34.326620	2240.217345	17.498471
34.809490	2228.119282	17.503488
34.742755	2229.434028	17.508506
34.730386	2222.307547	17.513523
34.795753	2206.387936	17.518541
34.566231	2204.504711	17.523559
34.480216	2195.195866	17.528576
34.507286	2195.873397	17.533594
34.675688	2198.477204	17.538611
34.758602	2186.882824	17.543629
34.708744	2198.954622	17.548647
34.779883	2201.695800	17.553664
34.680112	2202.075033	17.558682
34.584541	2200.234195	17.563699
34.708980	2209.536877	17.568717
34.833211	2229.670734	17.573735
34.671625	2226.511638	17.578752
35.020195	2227.328851	17.583770
35.131835	2229.574331	17.588787
34.952781	2233.441636	17.593805
34.866333	2227.338091	17.598823
35.029977	2228.865088	17.603840
34.974651	2239.023968	17.608858
34.963116	2230.315391	17.613875
35.062164	2230.924703	17.618893
34.818522	2236.412611	17.623911
35.083782	2228.974392	17.628928
35.183643	2228.671722	17.633946
35.120562	2231.458755	17.638963
35.425487	2225.109683	17.643981
35.257057	2229.133895	17.648999
35.034204	2235.627062	17.654016
35.429074	2245.008608	17.659034
35.212457	2248.747092	17.664051
35.354986	2247.530626	17.669069
35.516338	2259.860420	17.674087
35.770717	2253.295288	17.679104
35.325644	2248.804730	17.684122
35.435627	2256.747967	17.689139
35.564188	2252.795117	17.694157
35.439018	2257.557873	17.699175
35.550100	2252.999624	17.704192
35.622330	2263.012194	17.709210
35.842276	2260.816330	17.714227
35.899898	2268.742259	17.719245
36.139681	2283.974956	17.724263
35.899424	2270.628048	17.729280
35.967908	2272.931471	17.734298
35.710925	2282.697770	17.739315
36.352181	2276.968207	17.744333
36.173784	2282.706755	17.749351
36.396121	2278.164329	17.754368
36.333952	2266.184844	17.759386
35.919120	2269.410858	17.764403
36.329425	2270.705273	17.769421
36.186804	2285.656007	17.774439
36.037285	2293.531208	17.779456
36.678350	2289.685612	17.784474
36.496989	2290.355142	17.789491
36.513065	2285.701195	17.794509
36.329120	2288.373209	17.799527
36.629333	2286.299882	17.804544
36.842350	2278.989588	17.809562
36.308405	2281.358128	17.814579
36.497157	2272.251384	17.819597
37.000278	2275.050178	17.824615
36.795691	2275.853874	17.829632
36.936409	2272.285637	17.834650
36.575229	2272.613669	17.839667
36.781067	2267.894836	17.844685
36.784402	2273.305242	17.849703
36.826796	2269.885971	17.854720
36.969722	2263.609381	17.859738
36.697758	2285.553482	17.864755
36.615093	2276.266476	17.869773
36.439361	2277.648490	17.874791
36.260250	2281.281554	17.879808
36.843137	2281.453641	17.884826
36.610277	2288.448508	17.889843
36.689967	2298.630739	17.894861
36.739834	2306.835149	17.899879
37.096764	2298.816731	17.904896
37.316400	2294.225533	17.909914
37.054734	2303.115811	17.914931
37.428877	2303.754377	17.919949
37.079035	2298.375554	17.924967
37.018677	2305.003264	17.929984
37.236811	2297.271230	17.935002
37.173649	2298.906269	17.940019
37.336132	2317.811017	17.945037
37.513105	2327.509025	17.950055
37.657402	2334.451692	17.955072
37.733579	2321.594883	17.960090
37.654682	2326.356690	17.965107
37.695574	2330.312404	17.970125
37.726423	2330.683002	17.975143
38.028704	2325.161925	17.980160
37.962293	2320.883061	17.985178
37.690841	2324.202671	17.990195
37.779679	2318.613395	17.995213
37.849481	2325.614853	18.000231
37.928219	2332.141978	18.005248
38.071586	2325.197937	18.010266
37.965133	2322.631294	18.015283
38.172722	2322.592685	18.020301
38.105140	2318.493945	18.025319
37.891472	2329.868923	18.030336
38.298392	2316.221881	18.035354
37.964757	2319.746678	18.040371
37.993571	2316.189876	18.045389
38.028767	2316.984969	18.050407
38.019311	2314.369193	18.055424
37.989968	2313.202444	18.060442
38.023925	2325.753790	18.065459
38.367879	2335.806846	18.070477
38.457301	2347.817504	18.075495
38.399675	2351.580867	18.080512
38.520904	2343.760915	18.085530
38.374784	2353.175025	18.090547
38.578479	2347.244656	18.095565
38.588910	2353.375601	18.100583
38.608790	2350.608103	18.105600
38.934220	2342.201554	18.110618
38.742061	2352.216230	18.115635
38.674919	2350.319482	18.120653
38.867632	2345.094902	18.125671
38.702470	2345.754271	18.130688
38.817011	2349.661966	18.135706
38.844417	2344.415152	18.140723
38.777387	2346.491015	18.145741
38.645175	2332.282421	18.150759
38.557380	2358.810120	18.155776
39.082848	2363.454138	18.160794
38.905769	2373.564366	18.165811
39.045651	2372.539676	18.170829
39.306517	2363.483539	18.175847
39.294714	2367.290895	18.180864
39.657517	2369.184945	18.185882
39.762795	2373.107173	18.190899
39.753859	2372.571323	18.195917
39.484451	2366.098002	18.200935
39.383635	2371.242210	18.205952
39.603487	2357.405234	18.210970
39.380496	2363.143715	18.215987
39.692798	2364.751232	18.221005
39.985033	2357.246672	18.226023
39.779703	2359.489541	18.231040
40.109139	2347.565227	18.236058
39.753509	2337.562722	18.241075
40.081020	2330.148794	18.246093
39.926310	2321.663886	18.251111
40.168788	2318.798504	18.256128
40.044198	2322.359554	18.261146
39.847731	2323.921785	18.266163
39.658974	2324.317725	18.271181
39.804013	2316.117449	18.276199
39.622204	2326.383555	18.281216
39.921811	2318.862831	18.286234
40.050361	2343.931779	18.291251
40.336515	2351.378153	18.296269
40.322628	2356.111879	18.301287
40.313242	2362.950081	18.306304
40.222449	2347.808979	18.311322
40.542998	2348.077270	18.316339
40.178113	2339.666134	18.321357
40.603539	2341.011597	18.326375
40.242712	2354.498462	18.331392
40.385688	2361.215758	18.336410
40.116244	2356.388589	18.341427
40.269443	2352.397774	18.346445
40.426626	2357.984317	18.351463
40.421187	2358.842050	18.356480
40.275926	2351.018191	18.361498
40.362287	2351.415031	18.366515
40.599720	2353.646392	18.371533
40.732658	2359.956669	18.376551
40.612943	2378.758216	18.381568
40.937372	2384.302111	18.386586
40.853826	2391.642788	18.391603
40.652719	2388.441776	18.396621
40.977263	2378.834113	18.401639
40.565525	2385.003091	18.406656
40.863687	2382.861978	18.411674
40.874146	2386.720379	18.416691
40.488056	2383.348416	18.421709
40.942841	2394.708420	18.426727
41.020181	2407.179415	18.431744
41.304141	2413.172958	18.436762
41.486712	2414.076729	18.441779
41.243626	2419.025998	18.446797
41.598687	2413.535522	18.451815
41.171884	2421.813811	18.456832
41.454177	2408.024326	18.461850
41.520548	2415.444918	18.466867
41.448747	2413.276086	18.471885
41.864309	2413.319185	18.476903
41.349712	2411.205568	18.481920
41.652156	2399.709329	18.486938
41.837889	2407.934209	18.491955
41.680276	2407.031227	18.496973
42.213986	2403.981769	18.501991
42.066467	2404.993355	18.507008
41.976891	2400.117487	18.512026
42.129544	2399.504088	18.517043
42.044805	2404.191291	18.522061
42.171710	2395.105348	18.527079
41.905154	2402.788951	18.532096
41.617798	2398.008832	18.537114
41.473330	2396.311508	18.542131
41.767597	2408.678468	18.547149
41.967355	2424.334093	18.552167
41.896808	2436.518562	18.557184
41.795695	2432.232028	18.562202
42.103409	2434.423414	18.567219
42.044636	2432.592597	18.572237
42.571729	2433.834614	18.577255
42.457443	2439.626385	18.582272
42.686252	2433.895378	18.587290
42.643614	2434.067900	18.592307
42.240946	2438.599878	18.597325
42.366792	2436.855816	18.602343
42.850416	2450.100556	18.607360
42.564826	2453.796570	18.612378
43.003836	2452.098290	18.617395
42.699836	2440.027215	18.622413
43.022120	2451.695832	18.627431
42.646725	2449.959573	18.632448
42.885828	2454.764433	18.637466
43.200290	2461.076583	18.642483
42.940485	2456.298183	18.647501
43.275551	2454.018658	18.652519
43.211787	2461.660834	18.657536
42.991796	2455.198584	18.662554
43.052751	2448.835489	18.667571
43.097117	2462.510479	18.672589
43.120254	2456.401296	18.677607
43.049276	2456.170615	18.682624
43.216400	2453.712985	18.687642
43.513790	2450.515635	18.692659
43.384446	2454.901562	18.697677
43.597585	2444.233115	18.702695
43.223305	2456.739172	18.707712
43.247963	2459.481006	18.712730
43.663991	2450.219587	18.717747
43.443657	2452.881117	18.722765
43.703703	2447.627242	18.727783
43.537142	2451.355910	18.732800
43.397997	2460.393713	18.737818
43.739730	2466.817497	18.742835
43.108166	2481.295813	18.747853
43.528856	2480.904968	18.752871
43.986334	2472.899734	18.757888
43.779554	2476.694914	18.762906
44.111434	2472.552032	18.767923
44.100352	2481.004042	18.772941
44.201710	2473.659783	18.777959
43.992782	2476.246589	18.782976
44.244495	2481.389152	18.787994
44.498134	2473.415705	18.793011
44.038074	2470.244959	18.798029
44.547054	2488.741729	18.803047
44.600256	2484.883982	18.808064
44.402545	2480.674851	18.813082
44.459934	2481.309970	18.818099
44.786874	2478.598693	18.823117
44.573000	2474.975738	18.828135
44.478922	2476.599379	18.833152
44.258139	2485.038083	18.838170
44.643028	2497.783831	18.843187
44.578163	2505.819146	18.848205
44.827750	2504.303813	18.853223
44.896919	2497.290088	18.858240
44.933900	2498.569175	18.863258
44.862136	2496.024320	18.868275
44.578792	2499.498306	18.873293
45.067910	2494.232074	18.878311
45.032417	2503.018078	18.883328
44.962300	2500.526495	18.888346
45.580168	2496.185058	18.893363
45.240218	2487.266141	18.898381
45.371478	2492.619609	18.903399
45.354319	2491.474059	18.908416
45.195613	2496.047548	18.913434
45.546891	2489.607618	18.918451
45.399022	2490.508631	18.923469
45.534978	2481.736904	18.928487
45.549823	2488.192388	18.933504
45.390684	2495.332234	18.938522
45.765443	2489.330173	18.943539
45.658207	2499.097402	18.948557
45.324164	2488.557335	18.953575
45.301346	2487.382799	18.958592
45.517000	2495.851604	18.963610
45.580691	2492.038971	18.968627
45.604113	2494.741250	18.973645
45.764473	2509.227041	18.978663
45.821774	2511.270919	18.983680
46.012526	2520.183256	18.988698
46.080196	2515.122249	18.993715
46.355712	2517.987128	18.998733
46.294876	2512.904879	19.003751
46.233593	2512.324541	19.008768
46.194082	2513.813551	19.013786
46.289761	2508.701842	19.018803
46.228596	2505.074458	19.023821
46.102988	2509.214492	19.028839
46.603688	2510.627825	19.033856
46.310913	2512.452100	19.038874
46.633351	2509.875823	19.043891
46.272475	2508.437171	19.048909
46.590912	2505.548547	19.053927
46.718485	2503.423462	19.058944
46.259775	2511.264930	19.063962
46.414523	2504.935102	19.068979
46.651320	2505.911400	19.073997
46.583373	2505.229404	19.079015
46.619444	2509.802139	19.084032
46.753429	2521.226778	19.089050
46.782008	2534.918620	19.094067
46.659446	2540.179878	19.099085
47.256926	2535.824483	19.104103
47.147074	2532.982760	19.109120
46.807917	2544.846813	19.114138
47.428754	2540.478886	19.119155
46.973828	2545.134122	19.124173
47.265684	2541.090768	19.129191
47.174756	2541.764232	19.134208
47.110444	2538.442498	19.139226
47.525053	2533.576803	19.144243
47.349006	2538.287435	19.149261
47.420917	2531.581921	19.154279
47.801673	2534.346300	19.159296
47.518673	2539.523095	19.164314
47.313213	2533.663166	19.169331
47.837159	2545.752818	19.174349
47.422565	2546.663355	19.179367
47.525125	2550.885702	19.184384
47.619745	2558.534376	19.189402
47.954652	2545.993220	19.194419
47.735035	2555.525929	19.199437
47.730937	2552.757641	19.204455
47.745676	2549.494079	19.209472
47.841932	2552.432746	19.214490
48.059121	2558.581900	19.219507
47.732597	2551.622259	19.224525
47.889714	2578.354278	19.229543
48.172280	2583.609096	19.234560
48.281646	2579.113640	19.239578
48.625016	2580.203405	19.244595
48.302134	2581.427124	19.249613
48.615696	2574.458332	19.254631
48.935808	2578.917906	19.259648
48.758788	2575.539627	19.264666
48.956547	2567.147012	19.269683
48.990271	2553.604087	19.274701
48.751996	2542.006722	19.279719
49.153426	2530.342805	19.284736
48.836035	2537.268311	19.289754
48.644625	2526.372689	19.294771
48.578505	2537.262727	19.299789
48.887026	2543.668420	19.304807
48.939302	2533.886051	19.309824
48.966721	2537.545606	19.314842
48.774431	2534.674619	19.319859
49.178726	2551.815097	19.324877
49.088238	2555.007932	19.329895
49.357943	2561.266114	19.334912
49.171379	2576.809085	19.339930
49.176467	2565.541505	19.344947
49.259270	2571.016418	19.349965
49.243106	2573.144521	19.354983
49.574744	2561.417725	19.360000
49.364669	2571.469368	19.365018
49.056574	2567.815927	19.370035
49.311850	2567.889902	19.375053
49.153619	2569.187935	19.380071
49.262616	2573.538364	19.385088
49.353894	2589.438906	19.390106
49.495080	2592.188240	19.395123
49.447831	2603.807135	19.400141
49.441004	2607.403476	19.405159
49.703546	2595.832199	19.410176
49.778788	2614.358030	19.415194
49.966901	2620.583287	19.420211
50.136559	2628.319576	19.425229
49.956165	2626.544312	19.430247
50.430185	2632.383624	19.435264
50.528117	2623.225176	19.440282
50.701910	2618.959212	19.445299
50.223244	2622.600225	19.450317
50.526553	2619.696762	19.455335
50.943742	2617.307152	19.460352
50.469392	2611.539756	19.465370
50.606949	2591.742588	19.470387
50.838664	2604.889404	19.475405
50.734313	2596.577513	19.480423
50.503352	2586.960525	19.485440
50.574417	2602.892383	19.490458
50.511571	2609.777344	19.495475
50.618153	2614.920362	19.500493
50.458985	2627.834662	19.505511
50.759770	2610.270826	19.510528
50.392049	2617.597246	19.515546
50.601425	2624.434379	19.520563
50.931332	2631.588584	19.525581
50.957668	2641.349926	19.530599
51.188976	2644.917471	19.535616
51.006259	2650.165891	19.540634
50.841426	2653.178131	19.545651
51.368866	2648.835485	19.550669
51.255247	2649.465856	19.555687
51.229227	2637.523408	19.560704
51.628119	2639.275682	19.565722
51.235975	2648.546447	19.570739
51.427001	2658.009643	19.575757
51.488077	2666.128916	19.580775
51.476602	2673.581028	19.585792
51.553023	2675.342609	19.590810
52.000399	2677.577443	19.595827
51.991007	2677.411369	19.600845
51.903300	2678.937906	19.605863
51.999559	2660.521994	19.610880
52.251676	2666.026781	19.615898
52.310026	2665.209288	19.620915
52.313100	2664.960830	19.625933
52.076923	2672.486374	19.630951
52.444996	2662.931963	19.635968
52.132211	2674.023190	19.640986
52.407281	2666.424075	19.646003
52.529277	2665.744084	19.651021
52.120836	2665.918913	19.656039
52.342846	2664.135279	19.661056
52.532981	2660.607593	19.666074
52.466480	2659.963541	19.671091
52.553221	2650.551008	19.676109
52.461706	2658.801459	19.681127
52.551196	2656.698015	19.686144
52.502300	2664.755966	19.691162
52.397896	2659.391100	19.696179
52.625394	2650.884060	19.701197
52.357340	2671.968550	19.706215
52.657193	2687.694093	19.711232
52.940785	2689.810765	19.716250
52.999021	2693.948752	19.721267
52.745350	2686.863986	19.726285
52.637409	2682.396217	19.731303
52.740220	2693.574159	19.736320
52.947577	2708.255123	19.741338
52.734300	2716.140701	19.746355
53.402517	2712.047580	19.751373
53.197805	2718.110352	19.756391
53.196161	2710.985415	19.761408
53.358269	2720.604629	19.766426
53.799842	2735.143283	19.771443
54.012923	2737.648043	19.776461
54.138729	2743.308036	19.781479
54.528833	2717.909036	19.786496
54.139940	2715.230819	19.791514
54.273644	2707.969683	19.796531
54.382152	2698.086554	19.801549
54.150854	2711.920018	19.806567
54.258999	2698.444964	19.811584
54.269939	2699.663021	19.816602
53.996928	2705.625280	19.821619
54.145224	2697.288034	19.826637
54.278084	2710.107978	19.831655
54.474192	2699.447689	19.836672
54.392515	2704.265981	19.841690
53.922667	2706.641684	19.846707
54.082398	2699.782569	19.851725
54.178292	2708.693399	19.856743
54.427778	2698.110499	19.861760
54.809813	2713.303525	19.866778
54.391887	2723.698368	19.871795
54.566601	2726.011829	19.876813
54.371595	2732.983694	19.881831
54.510876	2727.469389	19.886848
54.731482	2736.103659	19.891866
54.464776	2732.192520	19.896883
54.585894	2731.889077	19.901901
54.798422	2743.837526	19.906919
54.972356	2756.256583	19.911936
55.214931	2760.290434	19.916954
55.066107	2760.393923	19.921971
55.265048	2750.541853	19.926989
55.289302	2752.622339	19.932007
55.487278	2742.321188	19.937024
55.438338	2749.806708	19.942042
55.285269	2743.274195	19.947059
55.409158	2739.409405	19.952077
55.425759	2738.744895	19.957095
55.541061	2743.110471	19.962112
55.469203	2737.831140	19.967130
55.143965	2752.804688	19.972147
55.654843	2759.233658	19.977165
55.403903	2774.778037	19.982183
55.686400	2775.375892	19.987200
55.664116	2768.926837	19.992218
55.742018	2774.183719	19.997235
55.798833	2769.638639	20.002253
55.913573	2789.837002	20.007271
56.450230	2795.457327	20.012288
56.404514	2800.607908	20.017306
56.633031	2801.402119	20.022323
56.471964	2797.106906	20.027341
56.506282	2788.720764	20.032359
56.276169	2798.203780	20.037376
56.838736	2795.166795	20.042394
56.353145	2800.349663	20.047411
56.868647	2792.447660	20.052429
56.874393	2797.073931	20.057447
56.656810	2793.947615	20.062464
56.715490	2784.665247	20.067482
56.776984	2796.297383	20.072499
56.622073	2783.311126	20.077517
56.904728	2788.134077	20.082535
57.120108	2782.061834	20.087552
57.298874	2786.844109	20.092570
57.253328	2790.462653	20.097587
57.079055	2787.688249	20.102605
56.913456	2790.258088	20.107623
56.985155	2789.298211	20.112640
57.411732	2793.107098	20.117658
57.087113	2804.905943	20.122675
57.401669	2806.016246	20.127693
57.060078	2812.931313	20.132711
57.236311	2804.341333	20.137728
57.470619	2816.762253	20.142746
57.368757	2812.640710	20.147763
57.363011	2821.929094	20.152781
57.790580	2839.855075	20.157799
57.768055	2843.652117	20.162816
57.997699	2838.916572	20.167834
57.704909	2839.141153	20.172851
58.288207	2835.934179	20.177869
58.384259	2840.465975	20.182887
58.434419	2839.313582	20.187904
58.755209	2833.850685	20.192922
58.624968	2843.721159	20.197939
58.316269	2825.020116	20.202957
58.308561	2836.964553	20.207975
58.205480	2836.281666	20.212992
58.646779	2832.770229	20.218010
58.301400	2843.190542	20.223027
58.487419	2834.755630	20.228045
58.317964	2839.022706	20.233063
58.744077	2837.165881	20.238080
58.983682	2831.045904	20.243098
58.622702	2835.779768	20.248115
58.838503	2846.922573	20.253133
59.324365	2855.893724	20.258151
59.280183	2863.498992	20.263168
59.146954	2840.924470	20.268186
59.166025	2843.847626	20.273203
59.429581	2837.774077	20.278221
59.474505	2837.224568	20.283239
59.188666	2831.373899	20.288256
59.414520	2835.253834	20.293274
59.382497	2843.559890	20.298291
59.444517	2848.979283	20.303309
59.580417	2849.870336	20.308327
59.644338	2853.046718	20.313344
59.454706	2850.591406	20.318362
59.494409	2858.270190	20.323379
59.695122	2854.027659	20.328397
59.925049	2851.736748	20.333415
59.884163	2851.479029	20.338432
60.030710	2846.118609	20.343450
59.664464	2849.904455	20.348467
59.740790	2852.771672	20.353485
59.678984	2851.702391	20.358503
60.127914	2874.243354	20.363520
60.065026	2878.956217	20.368538
59.785369	2884.774356	20.373555
60.038665	2882.773295	20.378573
60.003249	2885.065666	20.383591
59.851294	2884.170380	20.388608
60.657716	2888.090421	20.393626
60.464801	2903.995428	20.398643
60.461028	2909.657252	20.403661
60.466335	2903.793780	20.408679
60.692674	2908.215824	20.413696
60.768223	2906.843456	20.418714
61.044310	2900.272885	20.423731
61.227889	2898.088469	20.428749
61.201045	2897.591003	20.433767
60.874411	2897.770004	20.438784
61.427525	2889.317585	20.443802
61.082587	2894.916992	20.448819
60.994911	2912.008223	20.453837
61.196120	2918.490903	20.458855
61.224862	2934.809274	20.463872
61.665123	2935.432197	20.468890
60.938694	2928.125186	20.473907
61.397405	2931.707902	20.478925
61.259630	2938.649121	20.483943
61.159755	2936.931358	20.488960
61.851328	2952.641126	20.493978
61.865352	2956.837690	20.498995
61.852236	2956.576158	20.504013
62.021768	2946.352817	20.509031
62.148201	2967.327494	20.514048
62.061776	2945.549077	20.519066
62.102200	2955.641775	20.524083
62.003610	2950.382942	20.529101
62.258022	2947.652098	20.534119
62.470323	2948.804938	20.539136
62.456577	2938.980882	20.544154
62.462577	2946.409756	20.549171
62.630912	2942.464715	20.554189
62.724529	2929.334416	20.559207
62.637535	2939.014702	20.564224
62.609658	2937.851994	20.569242
62.477741	2942.927125	20.574259
62.709381	2955.258038	20.579277
63.195516	2960.007581	20.584295
62.894910	2967.917590	20.589312
63.201039	2966.831078	20.594330
63.303058	2968.382530	20.599347
63.274012	2968.353184	20.604365
63.664869	2960.648525	20.609383
63.506103	2957.637249	20.614400
63.806376	2953.950696	20.619418
63.584006	2939.258008	20.624435
63.212472	2925.545627	20.629453
63.622960	2920.927762	20.634471
63.476654	2915.930406	20.639488
63.566352	2928.181251	20.644506
63.120038	2942.032806	20.649523
63.295763	2952.708268	20.654541
63.517731	2951.647112	20.659559
63.400983	2961.467390	20.664576
63.675608	2952.338551	20.669594
63.589162	2969.475708	20.674611
64.034524	2980.227809	20.679629
64.099787	2980.735650	20.684647
64.051019	2992.419265	20.689664
64.114920	2977.780719	20.694682
64.140397	2977.373021	20.699699
64.332485	2977.282250	20.704717
64.678039	2974.474886	20.709735
64.540703	2983.933595	20.714752
64.881803	2977.677058	20.719770
64.538685	2982.740321	20.724787
64.634647	2975.620755	20.729805
64.558289	2973.328965	20.734823
64.485749	2984.376297	20.739840
64.738292	2995.957653	20.744858
64.964801	3001.723910	20.749875
65.168270	3009.252410	20.754893
64.946837	3008.436738	20.759911
64.849741	3011.429166	20.764928
64.899072	3006.115896	20.769946
65.103435	3002.088882	20.774963
64.891158	3010.348492	20.779981
65.325581	3023.338068	20.784999
65.005406	3046.229887	20.790016
65.393097	3040.779071	20.795034
65.517549	3031.610874	20.800051
65.499125	3040.985353	20.805069
65.711963	3041.330951	20.810087
65.398687	3044.843874	20.815104
65.958232	3060.135810	20.820122
65.856104	3066.290007	20.825139
65.556594	3062.331454	20.830157
66.172139	3066.723743	20.835175
66.143031	3069.975028	20.840192
66.327112	3060.663069	20.845210
66.242240	3062.664021	20.850227
66.232353	3061.015997	20.855245
66.367123	3063.626701	20.860263
66.389282	3063.466029	20.865280
66.278100	3063.256958	20.870298
66.693702	3068.113499	20.875315
66.865174	3085.239179	20.880333
67.190527	3089.142076	20.885351
66.758802	3082.150398	20.890368
66.930437	3063.648294	20.895386
67.379523	3073.553308	20.900403
66.776283	3072.076379	20.905421
66.929419	3067.259332	20.910439
67.311703	3074.470825	20.915456
67.298387	3083.754712	20.920474
67.181168	3075.799453	20.925491
67.301890	3080.572139	20.930509
67.461742	3071.635874	20.935527
67.138580	3082.472784	20.940544
67.322613	3078.016400	20.945562
67.733464	3074.137870	20.950579
67.121949	3084.879605	20.955597
67.477749	3078.032743	20.960615
67.432251	3098.466328	20.965632
67.913239	3095.098276	20.970650
68.219652	3109.214739	20.975667
68.012315	3102.015406	20.980685
68.435910	3094.767116	20.985703
68.112464	3098.063210	20.990720
68.190362	3094.092158	20.995738
68.406556	3093.182752	21.000755
68.388207	3095.430984	21.005773
68.606715	3097.391941	21.010791
68.689833	3096.985324	21.015808
68.571849	3087.317819	21.020826
68.652384	3093.376812	21.025843
68.698638	3092.089995	21.030861
68.720239	3091.819563	21.035879
68.947572	3089.332571	21.040896
68.391611	3085.700364	21.045914
69.143845	3087.956045	21.050931
68.448790	3093.624523	21.055949
69.110926	3083.219512	21.060967
68.801779	3087.160148	21.065984
68.837290	3093.545524	21.071002
68.968286	3107.296508	21.076019
68.968991	3119.561058	21.081037
69.478214	3112.306849	21.086055
69.175874	3122.506814	21.091072
69.032110	3124.169854	21.096090
69.467866	3127.824535	21.101107
69.748707	3150.091341	21.106125
69.442509	3152.749094	21.111143
69.417290	3147.238257	21.116160
69.668304	3154.134877	21.121178
69.661980	3151.551121	21.126195
69.718432	3161.905892	21.131213
70.164644	3173.308051	21.136231
70.158114	3176.136287	21.141248
70.419647	3175.065021	21.146266
70.634946	3177.429709	21.151283
70.373292	3173.794026	21.156301
70.540755	3168.949770	21.161319
70.370596	3175.220797	21.166336
70.649417	3172.182299	21.171354
70.755291	3168.855480	21.176371
70.433095	3166.106683	21.181389
70.755203	3160.913167	21.186407
71.005557	3170.725942	21.191424
70.570052	3159.245036	21.196442
71.047191	3158.535353	21.201459
70.959841	3176.081588	21.206477
71.384252	3184.820957	21.211495
70.972472	3193.172365	21.216512
70.913146	3200.451138	21.221530
71.362176	3188.144929	21.226547
71.212470	3198.806331	21.231565
71.502779	3195.895861	21.236583
71.484799	3192.802165	21.241600
71.357793	3199.352306	21.246618
71.607275	3198.056634	21.251635
71.444368	3223.301258	21.256653
72.088216	3217.355161	21.261671
71.870522	3221.059797	21.266688
72.006490	3219.949867	21.271706
72.052993	3220.518702	21.276723
72.075962	3225.505671	21.281741
72.154567	3216.642233	21.286759
72.572290	3215.755752	21.291776
71.884642	3220.061491	21.296794
72.119213	3209.164936	21.301811
72.426003	3232.603668	21.306829
72.652444	3239.446121	21.311847
72.690944	3243.534761	21.316864
72.755329	3242.826881	21.321882
73.153294	3246.381144	21.326899
73.332871	3244.861586	21.331917
73.085069	3229.474731	21.336935
73.133732	3207.327085	21.341952
72.707486	3215.915965	21.346970
73.421070	3223.848731	21.351987
73.090078	3239.839549	21.357005
73.098427	3227.135368	21.362023
73.280529	3234.858874	21.367040
73.201066	3243.321045	21.372058
73.483661	3233.295747	21.377075
73.472357	3227.101011	21.382093
73.274084	3227.514690	21.387111
73.091112	3234.708037	21.392128
73.136693	3247.192445	21.397146
73.778833	3248.626137	21.402163
73.529827	3250.681854	21.407181
73.250090	3261.049443	21.412199
73.531781	3279.807260	21.417216
73.888317	3285.572173	21.422234
73.503446	3280.555930	21.427251
74.106173	3297.720680	21.432269
74.632550	3302.111659	21.437287
74.583444	3302.190763	21.442304
74.782550	3314.753752	21.447322
75.107205	3308.263561	21.452339
74.921321	3307.753437	21.457357
75.105714	3308.821153	21.462375
75.134498	3284.598117	21.467392
74.908814	3279.046405	21.472410
75.017033	3281.096521	21.477427
75.015133	3284.877262	21.482445
75.069187	3292.175101	21.487463
75.183769	3298.610074	21.492480
75.226363	3294.582212	21.497498
75.398749	3302.368390	21.502515
75.100582	3293.480675	21.507533
75.011393	3296.596665	21.512551
75.597369	3295.479936	21.517568
75.475307	3317.483741	21.522586
75.790146	3315.348013	21.527603
75.840732	3320.569835	21.532621
75.916929	3321.412922	21.537639
76.102632	3308.702537	21.542656
75.901186	3326.669847	21.547674
76.154872	3313.914732	21.552691
75.821281	3314.071262	21.557709
75.795456	3326.052148	21.562727
76.328211	3326.523931	21.567744
76.191993	3345.432141	21.572762
76.154517	3346.377133	21.577779
76.295508	3352.644350	21.582797
76.330728	3353.415475	21.587815
76.733265	3353.241031	21.592832
76.478923	3341.380739	21.597850
76.879750	3355.594009	21.602867
77.119858	3368.513678	21.607885
77.076030	3368.563165	21.612903
77.171192	3369.359408	21.617920
76.912558	3377.708392	21.622938
77.357589	3370.210336	21.627955
77.212993	3368.977543	21.632973
77.356435	3371.532133	21.637991
77.702442	3368.717145	21.643008
77.315105	3376.349561	21.648026
77.690054	3366.340779	21.653043
77.719822	3369.317386	21.658061
77.806850	3377.657562	21.663079
77.987878	3364.702602	21.668096
77.399304	3360.391400	21.673114
78.012196	3375.563385	21.678131
78.248980	3399.260445	21.683149
77.978707	3399.420271	21.688167
78.499626	3393.611408	21.693184
78.211674	3394.739627	21.698202
78.432198	3397.170815	21.703219
78.232881	3399.794373	21.708237
78.302187	3393.548029	21.713255
78.650712	3391.064941	21.718272
78.383691	3394.584850	21.723290
78.445090	3394.262541	21.728307
78.457622	3417.935339	21.733325
78.545397	3421.318541	21.738343
79.469120	3419.142217	21.743360
78.874837	3430.166797	21.748378
79.127618	3412.732073	21.753395
79.291061	3424.510806	21.758413
79.317627	3420.226875	21.763431
79.051638	3422.819740	21.768448
79.388009	3432.059710	21.773466
79.395694	3442.994070	21.778483
79.584729	3447.873286	21.783501
79.477819	3453.928809	21.788519
79.708792	3441.168295	21.793536
79.326175	3448.017983	21.798554
79.894553	3469.124902	21.803571
79.881205	3477.819982	21.808589
79.708499	3484.112028	21.813607
80.079692	3484.582615	21.818624
79.916332	3477.032084	21.823642
79.977495	3475.155295	21.828659
80.250787	3491.673546	21.833677
80.199876	3503.092905	21.838695
80.709265	3503.925300	21.843712
80.805442	3499.682189	21.848730
80.930167	3497.129044	21.853747
81.251396	3500.947286	21.858765
81.107343	3501.755585	21.863783
81.205956	3502.109478	21.868800
81.025031	3499.494333	21.873818
81.445602	3494.964801	21.878835
81.423741	3484.999208	21.883853
81.237147	3495.755907	21.888871
81.614390	3489.934182	21.893888
81.513656	3502.568235	21.898906
81.423239	3496.064799	21.903923
81.772367	3490.763933	21.908941
81.571017	3493.594561	21.913959
81.887578	3505.442895	21.918976
81.682338	3525.004167	21.923994
81.888509	3519.863988	21.929011
81.696841	3518.542116	21.934029
81.725692	3527.372379	21.939047
82.383544	3515.887741	21.944064
82.291644	3522.468034	21.949082
82.497670	3534.441399	21.954099
82.629076	3542.488846	21.959117
82.544786	3546.463629	21.964135
82.847916	3549.976180	21.969152
82.919291	3543.147078	21.974170
82.784999	3548.610247	21.979187
82.988418	3549.233830	21.984205
82.687685	3543.894869	21.989223
82.911018	3536.978000	21.994240
82.812284	3544.987564	21.999258
83.212920	3540.386114	22.004275
82.937561	3538.995804	22.009293
82.899518	3546.536207	22.014311
82.837746	3548.588914	22.019328
83.369650	3573.337506	22.024346
83.119887	3573.969194	22.029363
83.514722	3577.519329	22.034381
83.314696	3574.196221	22.039399
83.413419	3591.597923	22.044416
83.708665	3601.002304	22.049434
83.610720	3598.570277	22.054451
84.100964	3597.824939	22.059469
83.960072	3602.447774	22.064487
84.596001	3613.992093	22.069504
84.783156	3623.960914	22.074522
84.826673	3611.845555	22.079539
84.908527	3596.791594	22.084557
84.795036	3592.091381	22.089575
84.607824	3590.390370	22.094592
84.420003	3600.448831	22.099610
84.761625	3615.457676	22.104627
84.769489	3615.920705	22.109645
84.882638	3629.317971	22.114663
85.187633	3616.941960	22.119680
85.005278	3628.918678	22.124698
84.948977	3630.969308	22.129715
85.329165	3624.522949	22.134733
85.544598	3640.101997	22.139751
85.519152	3640.030709	22.144768
85.594444	3645.757277	22.149786
85.477937	3641.802921	22.154803
85.554336	3643.301589	22.159821
85.488823	3640.502328	22.164839
85.875747	3631.821489	22.169856
85.905089	3652.020935	22.174874
86.282309	3668.246144	22.179891
86.477086	3663.163324	22.184909
86.336175	3679.924794	22.189927
86.499020	3666.162253	22.194944
86.300858	3660.646797	22.199962
86.255657	3670.105232	22.204979
86.859453	3676.158131	22.209997
86.365281	3670.302659	22.215015
86.826713	3671.463521	22.220032
86.699080	3685.959115	22.225050
86.654944	3697.310555	22.230067
87.123155	3691.069701	22.235085
86.941050	3701.709641	22.240103
87.009302	3695.151105	22.245120
87.351604	3693.836086	22.250138
87.369195	3716.539864	22.255155
87.903641	3723.114177	22.260173
87.780142	3724.013191	22.265191
87.796563	3730.000359	22.270208
87.855327	3728.574787	22.275226
88.150502	3726.621025	22.280243
88.253095	3720.632461	22.285261
87.947645	3722.106165	22.290279
88.156877	3723.813586	22.295296
88.240483	3718.539286	22.300314
88.035485	3721.146512	22.305331
88.196925	3715.572278	22.310349
88.113791	3711.735624	22.315367
88.417719	3726.804762	22.320384
88.593760	3741.505668	22.325402
88.248589	3744.507420	22.330419
88.639965	3739.929497	22.335437
88.572491	3742.330071	22.340455
88.899225	3746.436871	22.345472
88.956467	3748.592749	22.350490
88.945689	3764.230641	22.355507
89.342403	3770.376931	22.360525
89.389527	3783.717930	22.365543
89.479169	3774.718472	22.370560
89.722203	3771.438114	22.375578
89.622923	3769.748904	22.380595
90.051083	3765.868129	22.385613
89.919422	3769.248761	22.390631
89.719240	3765.829956	22.395648
90.126866	3764.052084	22.400666
89.854627	3765.249390	22.405683
89.806046	3760.383238	22.410701
89.652678	3771.786683	22.415719
90.067926	3793.207233	22.420736
90.047547	3790.240212	22.425754
89.963616	3792.071786	22.430771
90.113533	3795.671583	22.435789
90.113067	3824.376592	22.440807
90.133966	3827.723312	22.445824
90.510127	3833.135130	22.450842
90.458139	3846.818232	22.455859
90.669045	3845.038275	22.460877
91.094568	3847.387944	22.465895
91.373429	3850.078874	22.470912
91.755604	3842.237803	22.475930
91.610855	3852.057369	22.480947
91.924813	3840.783400	22.485965
92.031794	3837.074311	22.490983
91.856342	3834.118785	22.496000
92.061849	3838.928065	22.501018
92.082432	3835.104525	22.506035
92.010994	3826.931824	22.511053
92.070294	3836.809731	22.516071
91.720561	3849.580190	22.521088
92.253692	3843.823086	22.526106
92.518362	3868.654986	22.531123
92.204418	3861.309151	22.536141
92.390805	3858.428763	22.541159
92.275551	3859.580392	22.546176
92.200349	3867.631900	22.551194
92.377635	3883.960134	22.556211
92.835037	3889.657776	22.561229
92.892492	3898.188193	22.566247
92.609576	3901.211166	22.571264
93.298097	3894.329334	22.576282
92.732072	3910.283755	22.581299
93.005405	3915.615765	22.586317
93.371002	3922.378382	22.591335
93.316286	3926.486573	22.596352
93.388817	3925.881660	22.601370
93.131724	3930.582502	22.606387
94.057920	3937.214497	22.611405
94.338682	3938.625803	22.616423
94.519914	3940.371748	22.621440
94.880449	3932.813391	22.626458
94.490687	3937.047154	22.631475
94.604361	3931.806392	22.636493
94.652447	3917.553897	22.641511
94.625037	3915.674003	22.646528
94.532044	3919.438086	22.651546
94.499116	3928.468597	22.656563
94.909132	3929.144220	22.661581
94.706578	3931.223832	22.666599
94.737050	3935.050164	22.671616
95.035125	3931.909894	22.676634
95.213304	3934.775408	22.681651
95.127004	3939.236916	22.686669
94.895847	3933.328736	22.691687
95.033924	3946.585118	22.696704
95.282824	3960.569730	22.701722
95.384992	3960.011884	22.706739
95.416018	3963.956259	22.711757
95.252844	3965.026842	22.716775
95.432189	3975.689411	22.721792
95.780794	3986.528716	22.726810
95.744554	3994.839231	22.731827
95.835733	3994.992762	22.736845
96.112964	4000.165075	22.741863
96.000645	4008.024345	22.746880
96.368700	4017.129476	22.751898
96.358337	4035.009647	22.756915
96.441990	4035.088822	22.761933
96.633264	4027.041832	22.766951
96.377696	4030.700558	22.771968
96.837737	4026.360040	22.776986
96.737244	4044.354374	22.782003
97.291441	4047.189934	22.787021
97.392074	4037.164723	22.792039
97.300813	4038.621103	22.797056
97.525753	4037.587736	22.802074
97.199055	4044.769026	22.807091
97.524493	4028.868679	22.812109
97.776772	4039.015200	22.817127
97.596679	4058.383572	22.822144
98.124258	4060.747089	22.827162
97.764493	4070.846134	22.832179
98.036505	4063.528394	22.837197
98.375210	4062.915627	22.842215
98.293654	4063.055234	22.847232
98.223072	4060.276031	22.852250
97.986640	4070.961048	22.857267
98.147406	4079.493357	22.862285
98.507950	4081.496286	22.867303
98.505793	4090.130394	22.872320
98.886961	4074.594848	22.877338
98.940132	4095.995048	22.882355
99.184824	4106.800454	22.887373
99.437841	4118.702303	22.892391
99.099391	4128.700202	22.897408
99.334078	4119.597776	22.902426
99.447220	4117.400837	22.907443
99.528146	4119.701293	22.912461
99.558037	4113.252101	22.917479
99.470373	4128.065945	22.922496
99.729645	4130.809388	22.927514
99.887014	4140.345605	22.932531
100.053302	4144.659030	22.937549
100.168263	4145.762322	22.942567
100.288120	4142.637346	22.947584
100.551163	4126.917338	22.952602
100.419366	4135.591839	22.957619
100.647421	4135.265152	22.962637
101.064601	4143.598320	22.967655
100.816827	4161.261212	22.972672
100.834447	4156.188275	22.977690
100.848499	4169.911912	22.982707
101.008073	4163.038798	22.987725
101.010606	4162.653375	22.992743
100.891784	4152.944002	22.997760
101.339879	4158.752752	23.002778
101.394708	4177.960305	23.007795
101.547497	4181.368740	23.012813
101.505483	4191.412884	23.017831
101.478443	4186.419785	23.022848
101.996841	4177.527082	23.027866
101.678042	4183.886519	23.032883
101.941110	4185.346455	23.037901
102.054186	4180.701083	23.042919
101.772164	4195.418019	23.047936
102.122045	4204.661725	23.052954
102.229434	4222.343054	23.057971
102.437761	4214.927897	23.062989
102.490723	4210.824843	23.068007
102.112684	4222.774562	23.073024
102.587494	4234.655524	23.078042
102.620030	4241.415153	23.083059
102.765760	4238.623726	23.088077
102.995108	4240.805907	23.093095
102.994665	4261.188265	23.098112
103.233204	4269.212440	23.103130
103.388009	4277.537148	23.108147
103.413065	4279.053043	23.113165
103.265427	4274.743777	23.118183
103.271281	4297.062477	23.123200
103.858954	4302.133085	23.128218
104.162284	4294.243813	23.133235
104.193548	4306.436898	23.138253
104.234235	4300.846620	23.143271
104.533449	4301.106675	23.148288
104.424079	4294.289062	23.153306
104.607160	4297.394030	23.158323
104.753904	4323.036471	23.163341
104.934838	4324.611613	23.168359
104.603249	4334.081642	23.173376
104.545373	4329.581877	23.178394
104.893809	4328.591834	23.183411
105.175666	4317.850491	23.188429
105.454185	4317.587899	23.193447
105.672085	4335.846436	23.198464
105.835466	4342.660047	23.203482
105.861736	4336.277516	23.208499
105.910695	4341.428676	23.213517
106.210543	4333.080826	23.218535
106.047024	4341.990654	23.223552
106.196400	4353.764149	23.228570
106.170349	4336.750621	23.233587
106.261070	4336.012737	23.238605
106.509731	4330.620335	23.243623
106.535396	4336.950359	23.248640
106.431267	4345.143144	23.253658
106.427778	4346.232200	23.258675
106.621165	4339.463666	23.263693
107.029917	4336.041165	23.268711
106.848936	4364.073780	23.273728
107.034739	4367.842208	23.278746
107.387964	4370.123602	23.283763
107.155418	4375.858489	23.288781
107.046534	4371.169485	23.293799
107.209529	4369.641542	23.298816
107.336850	4378.170102	23.303834
107.502289	4393.662887	23.308851
107.426045	4406.152641	23.313869
108.019256	4397.115121	23.318887
107.780697	4397.610708	23.323904
107.731130	4407.301060	23.328922
108.295504	4427.291630	23.333939
108.139677	4433.789565	23.338957
108.173944	4435.377191	23.343975
108.123835	4442.700297	23.348992
108.265045	4446.126458	23.354010
108.478280	4448.502710	23.359027
108.221926	4455.237812	23.364045
108.792041	4457.287207	23.369063
108.863792	4469.352433	23.374080
109.139914	4472.731059	23.379098
109.454776	4479.265269	23.384115
109.574549	4484.566198	23.389133
109.688739	4488.441806	23.394151
109.224370	4486.108116	23.399168
109.437962	4485.075814	23.404186
109.820604	4483.604421	23.409203
109.596225	4491.305288	23.414221
109.687013	4494.932758	23.419239
109.920322	4512.169864	23.424256
110.176372	4512.167730	23.429274
110.301930	4504.240848	23.434291
110.212090	4520.111522	23.439309
110.081150	4526.520319	23.444327
110.364481	4530.775881	23.449344
110.361781	4540.871230	23.454362
110.568859	4550.030105	23.459379
110.985700	4569.756256	23.464397
111.234304	4557.764113	23.469415
111.221048	4555.478574	23.474432
111.427776	4556.880145	23.479450
111.711645	4558.092533	23.484467
111.735418	4561.553128	23.489485
111.764596	4562.243802	23.494503
111.610261	4581.461281	23.499520
111.562600	4586.348940	23.504538
111.675945	4588.000668	23.509555
111.808405	4594.167415	23.514573
112.054495	4597.783369	23.519591
111.977525	4606.586871	23.524608
112.395472	4602.006665	23.529626
112.665523	4601.201273	23.534643
112.720760	4617.248061	23.539661
112.846762	4631.288275	23.544679
112.736045	4636.384853	23.549696
112.934194	4637.078267	23.554714
113.402736	4634.592443	23.559731
113.478383	4638.527237	23.564749
113.699465	4633.806357	23.569767
113.716407	4643.792987	23.574784
113.602417	4645.557181	23.579802
113.558266	4650.865620	23.584819
113.681249	4665.017409	23.589837
113.738593	4660.336234	23.594855
113.992022	4667.821824	23.599872
113.945771	4669.615757	23.604890
114.068562	4672.898533	23.609907
114.082799	4691.128202	23.614925
114.273471	4700.920715	23.619943
114.756362	4705.713473	23.624960
114.545220	4699.088949	23.629978
114.895617	4695.476783	23.634995
114.804848	4716.259014	23.640013
114.705943	4713.021301	23.645031
115.138169	4719.656675	23.650048
115.376106	4714.908566	23.655066
115.490135	4720.311333	23.660083
115.864962	4740.265959	23.665101
115.965936	4736.754151	23.670119
116.286486	4741.384787	23.675136
116.292917	4746.252513	23.680154
116.620458	4735.510410	23.685171
116.400570	4745.639490	23.690189
116.433258	4741.651488	23.695207
116.657235	4734.145290	23.700224
116.568225	4736.319614	23.705242
117.037554	4734.251839	23.710259
116.486617	4738.702301	23.715277
116.389825	4745.972636	23.720295
116.519573	4740.313113	23.725312
116.650897	4740.555299	23.730330
117.097605	4745.340673	23.735347
116.914083	4754.253257	23.740365
117.145540	4755.182155	23.745383
117.282415	4758.174369	23.750400
117.273862	4768.527577	23.755418
117.744449	4772.845920	23.760435
117.579258	4790.329667	23.765453
117.645402	4800.375192	23.770471
117.774715	4793.143748	23.775488
117.814269	4815.100838	23.780506
118.217837	4812.880129	23.785523
117.967398	4828.165770	23.790541
118.133995	4821.196699	23.795559
118.470820	4844.219009	23.800576
118.220764	4860.836389	23.805594
118.898732	4853.524309	23.810611
118.806006	4858.138353	23.815629
119.227233	4868.699262	23.820647
119.326731	4870.934536	23.825664
119.114573	4879.231331	23.830682
119.470841	4878.536085	23.835699
119.019213	4877.898217	23.840717
119.811586	4888.871800	23.845735
120.018844	4893.632287	23.850752
119.686033	4898.212853	23.855770
120.118407	4895.715652	23.860787
120.441635	4894.706124	23.865805
119.871591	4900.352171	23.870823
120.363250	4909.739784	23.875840
120.635595	4920.464780	23.880858
120.711393	4930.232353	23.885875
120.636371	4928.746131	23.890893
120.955044	4930.814386	23.895911
121.192426	4942.543035	23.900928
121.052908	4953.008620	23.905946
121.370430	4951.082515	23.910963
121.361249	4961.113050	23.915981
121.249654	4951.909182	23.920999
121.545225	4957.415858	23.926016
121.424901	4975.465732	23.931034
121.618557	4978.837647	23.936051
121.927727	4976.815263	23.941069
121.757022	5002.009692	23.946087
122.083130	5009.395991	23.951104
122.247360	5009.527986	23.956122
122.209463	5006.949546	23.961139
122.697087	5027.244206	23.966157
122.744890	5038.299439	23.971175
122.988716	5038.993184	23.976192
123.095671	5039.180343	23.981210
123.273831	5027.453895	23.986227
123.607300	5038.677623	23.991245
123.470270	5039.310781	23.996263
123.851588	5032.560450	24.001280
123.707513	5048.970674	24.006298
124.094276	5050.551189	24.011315
123.884924	5054.586044	24.016333
124.227361	5064.341054	24.021351
124.507535	5060.663252	24.026368
124.520785	5069.548158	24.031386
124.569826	5061.191836	24.036403
124.393667	5060.530400	24.041421
124.649070	5064.092153	24.046439
124.854348	5057.832480	24.051456
124.542292	5062.517553	24.056474
124.678579	5059.713370	24.061491
124.936691	5075.115087	24.066509
124.816581	5084.229216	24.071527
125.003752	5083.083902	24.076544
125.126420	5104.422775	24.081562
125.361291	5111.675377	24.086579
125.387810	5114.485888	24.091597
125.499267	5119.970340	24.096615
126.100381	5129.026505	24.101632
125.917506	5142.045637	24.106650
125.922527	5144.587210	24.111667
126.069200	5152.831821	24.116685
126.259351	5151.320572	24.121703
126.583203	5169.152994	24.126720
126.313270	5182.389769	24.131738
126.816045	5174.326847	24.136755
126.764345	5181.183524	24.141773
126.863436	5191.056088	24.146791
127.053942	5197.297733	24.151808
127.050760	5203.658872	24.156826
127.457662	5196.419873	24.161843
127.614241	5208.469258	24.166861
127.820089	5224.946163	24.171879
128.243580	5229.882021	24.176896
128.078912	5235.079085	24.181914
128.020375	5236.988529	24.186931
128.084384	5225.405274	24.191949
128.172404	5228.458436	24.196967
128.466497	5238.774443	24.201984
128.178357	5241.649678	24.207002
128.434239	5251.830256	24.212019
128.652228	5259.160542	24.217037
128.584894	5273.123079	24.222055
128.795317	5281.394218	24.227072
129.321156	5282.079872	24.232090
129.387457	5291.257764	24.237107
129.776969	5301.765936	24.242125
129.710154	5312.071654	24.247143
130.110320	5289.539569	24.252160
130.248801	5313.071897	24.257178
130.306094	5299.866481	24.262195
130.038079	5300.305538	24.267213
130.201490	5317.950471	24.272231
130.635294	5318.747450	24.277248
130.591223	5332.536857	24.282266
130.785321	5332.066918	24.287283
130.954210	5330.572562	24.292301
131.103599	5331.519809	24.297319
131.039809	5320.341988	24.302336
131.115260	5337.658119	24.307354
131.421178	5350.792598	24.312371
131.757111	5347.785975	24.317389
131.318218	5357.775288	24.322407
131.678082	5348.801860	24.327424
131.619183	5364.330384	24.332442
131.766127	5381.418925	24.337459
131.875816	5372.370343	24.342477
131.582097	5391.022768	24.347495
132.181229	5411.727125	24.352512
132.265394	5413.927999	24.357530
132.474457	5413.744626	24.362547
132.882418	5424.690090	24.367565
132.795146	5440.480143	24.372583
132.995737	5444.844167	24.377600
133.274393	5434.560190	24.382618
133.043321	5444.384406	24.387635
133.573951	5440.381513	24.392653
133.270936	5465.144934	24.397671
133.497129	5466.430740	24.402688
133.507220	5473.408053	24.407706
133.741767	5462.038967	24.412723
133.623124	5473.064570	24.417741
133.837727	5493.507427	24.422759
134.687416	5498.103445	24.427776
134.211439	5497.306546	24.432794
134.739025	5500.473640	24.437811
134.931792	5518.290358	24.442829
134.621752	5524.993847	24.447847
135.392660	5524.600093	24.452864
135.325667	5519.867579	24.457882
135.199441	5518.466964	24.462899
135.421352	5524.012815	24.467917
135.523687	5544.284516	24.472935
135.844101	5543.758214	24.477952
135.530750	5556.114865	24.482970
135.620422	5558.265229	24.487987
136.175755	5567.229205	24.493005
135.859939	5575.985371	24.498023
136.467271	5568.344420	24.503040
136.535454	5582.009919	24.508058
136.242681	5592.839183	24.513075
136.963042	5600.166784	24.518093
136.836066	5614.569528	24.523111
136.712525	5609.736874	24.528128
136.926881	5617.167168	24.533146
137.106136	5631.226234	24.538163
137.716292	5638.446084	24.543181
137.419790	5643.443005	24.548199
137.570180	5633.317181	24.553216
137.784922	5651.643929	24.558234
138.135986	5658.894873	24.563251
138.572477	5655.014629	24.568269
138.433830	5652.659118	24.573287
138.805754	5649.351128	24.578304
138.757114	5661.132398	24.583322
138.826834	5680.121939	24.588339
139.312521	5673.133528	24.593357
139.214159	5681.488298	24.598375
139.229068	5679.253065	24.603392
139.508450	5680.000811	24.608410
139.501264	5684.457588	24.613427
139.442977	5676.733833	24.618445
139.696725	5705.480516	24.623463
139.835499	5708.173308	24.628480
139.657113	5715.326854	24.633498
139.735249	5718.377811	24.638515
140.352582	5716.650071	24.643533
140.129526	5736.955418	24.648551
140.466913	5728.263524	24.653568
140.741241	5729.339755	24.658586
140.496302	5756.651380	24.663603
140.982304	5756.207921	24.668621
140.695775	5756.928080	24.673639
140.854017	5774.450725	24.678656
141.183816	5781.723362	24.683674
141.585598	5786.120329	24.688691
141.923709	5783.032929	24.693709
141.707674	5791.420629	24.698727
141.719182	5810.920887	24.703744
142.045813	5811.516684	24.708762
141.751749	5819.825169	24.713779
142.403029	5819.290545	24.718797
142.360097	5837.089154	24.723815
142.517736	5833.206206	24.728832
142.660638	5836.346489	24.733850
142.829500	5846.709622	24.738867
143.144670	5831.509355	24.743885
142.823307	5855.346251	24.748903
143.192390	5866.562312	24.753920
143.645869	5862.154654	24.758938
143.178845	5874.220376	24.763955
143.631816	5881.743605	24.768973
143.889566	5895.508732	24.773991
144.212759	5893.347655	24.779008
144.111898	5893.685014	24.784026
144.150270	5907.239950	24.789043
144.441487	5906.970510	24.794061
144.458510	5931.827379	24.799079
144.711058	5932.428359	24.804096
144.809377	5926.906724	24.809114
144.985081	5937.430246	24.814131
145.372894	5934.944205	24.819149
145.276309	5943.468944	24.824167
145.701917	5946.540386	24.829184
145.850805	5943.803272	24.834202
146.127201	5953.875366	24.839219
146.271064	5962.579262	24.844237
146.071724	5975.958596	24.849255
146.009587	5973.108344	24.854272
146.522595	5973.228283	24.859290
146.090383	5977.182128	24.864307
146.801527	5981.638195	24.869325
146.988671	5995.559234	24.874343
147.354307	5992.879163	24.879360
147.166962	5992.865387	24.884378
147.079463	6003.568003	24.889395
147.515719	6017.936929	24.894413
147.118370	6035.712531	24.899431
147.249883	6047.185440	24.904448
147.614883	6039.409538	24.909466
147.767236	6061.082680	24.914483
147.978598	6060.634279	24.919501
148.191638	6068.167395	24.924519
148.308697	6087.190543	24.929536
148.813925	6084.440874	24.934554
149.030586	6087.446125	24.939571
149.313629	6081.077083	24.944589
149.201007	6086.791942	24.949607
149.294584	6097.070039	24.954624
149.560969	6110.201460	24.959642
149.533209	6108.519056	24.964659
149.616136	6103.679632	24.969677
150.008674	6108.082159	24.974695
149.750748	6112.638069	24.979712
150.107953	6127.205276	24.984730
149.948287	6138.505140	24.989747
150.327600	6136.158311	24.994765
150.894479	6146.837741	24.999783
150.810234	6161.855347	25.004800
151.092428	6161.879608	25.009818
150.973862	6168.946266	25.014835
151.122434	6160.635895	25.019853
151.242615	6164.407747	25.024871
150.971746	6180.280131	25.029888
151.468998	6185.800319	25.034906
151.386286	6196.262045	25.039923
151.637148	6209.958488	25.044941
151.603831	6215.419246	25.049959
152.031727	6228.759526	25.054976
152.076353	6229.016880	25.059994
152.225493	6251.100384	25.065011
152.226607	6247.763091	25.070029
152.647766	6253.456579	25.075047
152.821501	6273.035301	25.080064
153.256558	6272.661702	25.085082
153.080015	6285.290843	25.090099
153.519787	6271.395905	25.095117
153.457792	6271.514962	25.100135
153.490508	6299.705446	25.105152
154.011160	6292.104497	25.110170
153.887706	6301.152142	25.115187
154.025341	6300.486740	25.120205
154.267791	6311.626419	25.125223
154.211895	6329.293041	25.130240
154.590771	6325.071678	25.135258
154.584337	6332.534140	25.140275
154.784211	6339.938030	25.145293
155.244265	6364.203957	25.150311
155.001206	6364.398677	25.155328
155.276742	6361.447550	25.160346
155.479642	6381.808431	25.165363
155.558244	6394.051214	25.170381
155.628031	6393.180441	25.175399
155.475501	6401.951769	25.180416
155.904718	6411.393945	25.185434
155.979384	6427.049473	25.190451
156.587228	6436.920497	25.195469
156.856458	6439.701297	25.200487
156.717077	6459.163537	25.205504
157.047948	6449.552360	25.210522
157.317573	6451.736063	25.215539
157.297661	6477.386759	25.220557
157.350039	6482.482919	25.225575
157.710004	6486.516027	25.230592
158.015195	6480.099051	25.235610
158.177401	6485.582665	25.240627
158.436055	6485.574594	25.245645
158.830809	6492.391787	25.250663
158.321126	6499.505233	25.255680
158.760754	6507.535068	25.260698
158.854858	6504.903021	25.265715
158.585819	6501.400890	25.270733
158.926983	6516.384628	25.275751
159.170850	6530.171511	25.280768
159.807966	6536.531141	25.285786
159.337924	6540.983667	25.290803
159.386173	6544.046033	25.295821
159.623037	6550.905146	25.300839
159.630229	6567.380900	25.305856
160.062937	6561.664267	25.310874
159.959254	6595.602502	25.315891
160.212777	6591.572745	25.320909
160.322479	6600.708768	25.325927
160.578942	6603.388529	25.330944
160.808009	6618.237331	25.335962
160.885080	6624.191927	25.340979
161.318217	6643.661996	25.345997
161.937055	6638.819532	25.351015
161.268277	6641.084593	25.356032
161.735724	6642.696814	25.361050
162.191976	6657.764026	25.366067
162.116540	6669.951399	25.371085
162.139680	6670.555736	25.376103
162.144543	6675.570820	25.381120
162.664385	6693.158274	25.386138
162.553425	6702.719993	25.391155
162.679853	6723.829646	25.396173
162.764990	6718.840802	25.401191
163.113336	6727.100893	25.406208
163.393268	6734.412947	25.411226
163.529728	6738.091660	25.416243
163.905165	6734.966393	25.421261
164.210404	6739.018867	25.426279
163.822121	6744.592928	25.431296
164.020453	6754.350794	25.436314
164.479940	6768.672450	25.441331
164.351689	6768.711899	25.446349
164.453933	6767.782959	25.451367
164.652665	6782.358106	25.456384
164.864186	6796.052906	25.461402
164.978254	6796.984039	25.466419
165.000165	6804.873669	25.471437
165.269439	6815.580774	25.476455
165.339456	6822.978036	25.481472
165.309779	6827.066293	25.486490
165.857412	6841.152087	25.491507
165.760402	6852.536604	25.496525
166.271462	6853.468961	25.501543
166.232234	6881.594412	25.506560
166.517863	6876.135956	25.511578
166.591908	6886.681668	25.516595
166.815144	6903.041659	25.521613
166.840279	6916.253076	25.526631
166.884283	6919.691148	25.531648
167.117413	6931.266812	25.536666
167.075696	6943.072305	25.541683
167.647080	6948.608058	25.546701
168.082646	6954.538080	25.551719
168.405494	6965.408916	25.556736
168.405859	6969.107853	25.561754
168.917715	6963.900986	25.566771
168.487860	6976.156726	25.571789
169.033042	6990.302923	25.576807
169.249881	6992.122085	25.581824
169.394946	6986.597858	25.586842
169.514206	6993.381327	25.591859
169.471275	7013.563173	25.596877
169.782163	7012.739880	25.601895
169.851204	7028.156693	25.606912
170.145760	7027.520418	25.611930
170.527217	7030.448154	25.616947
170.209922	7061.599731	25.621965
170.857831	7056.296267	25.626983
170.377016	7055.495353	25.632000
170.915516	7059.682578	25.637018
171.111302	7078.255147	25.642035
170.794462	7089.738456	25.647053
171.637388	7080.947948	25.652071
171.393506	7090.647696	25.657088
171.646381	7104.530473	25.662106
171.765135	7106.181572	25.667123
171.797226	7112.840893	25.672141
172.135425	7131.720770	25.677159
171.967998	7142.468894	25.682176
172.459872	7151.130002	25.687194
172.414420	7158.066842	25.692212
172.440187	7182.919496	25.697229
172.992722	7184.510599	25.702247
172.878047	7200.967804	25.707264
173.213189	7208.375699	25.712282
173.492183	7216.337970	25.717300
173.767557	7234.568293	25.722317
174.043807	7228.349581	25.727335
173.786583	7242.311420	25.732352
174.143079	7257.873057	25.737370
174.457278	7250.132548	25.742388
174.557857	7263.377449	25.747405
174.898650	7271.478388	25.752423
175.051483	7287.999305	25.757440
175.023422	7284.852519	25.762458
175.210747	7283.879530	25.767476
175.273882	7302.986320	25.772493
175.414673	7313.673288	25.777511
175.868026	7321.869044	25.782528
175.953214	7322.234704	25.787546
176.335155	7323.490943	25.792564
176.499890	7344.627374	25.797581
176.540544	7349.955758	25.802599
176.313333	7353.680648	25.807616
176.698220	7365.784462	25.812634
177.220774	7364.343217	25.817652
177.433803	7379.764888	25.822669
177.396088	7370.034592	25.827687
177.575470	7386.840298	25.832704
177.469168	7402.567711	25.837722
177.819465	7400.104202	25.842740
178.180471	7415.864534	25.847757
178.432606	7422.910544	25.852775
178.459906	7440.020329	25.857792
178.211785	7433.162103	25.862810
178.853829	7452.738788	25.867828
178.829498	7456.219010	25.872845
179.095847	7454.648459	25.877863
179.413508	7475.005920	25.882880
179.399713	7488.677184	25.887898
179.610454	7483.649187	25.892916
179.816548	7505.757303	25.897933
180.238898	7516.130761	25.902951
180.588943	7518.205989	25.907968
180.599919	7528.632599	25.912986
180.955956	7524.179972	25.918004
180.880035	7536.453158	25.923021
181.447140	7536.583858	25.928039
181.297458	7537.497262	25.933056
181.319375	7553.195718	25.938074
181.564641	7554.390321	25.943092
181.472161	7561.929047	25.948109
181.587433	7572.216324	25.953127
181.982807	7582.484802	25.958144
182.007902	7594.642846	25.963162
182.355637	7602.296180	25.968180
182.404337	7619.676736	25.973197
182.555153	7623.476947	25.978215
182.943040	7634.087774	25.983232
183.002637	7636.553756	25.988250
183.755813	7640.083310	25.993268
183.400165	7663.921499	25.998285
183.885158	7678.116875	26.003303
183.835236	7683.368993	26.008320
183.858940	7693.969262	26.013338
184.204774	7702.594989	26.018356
184.510680	7718.769625	26.023373
184.718212	7715.423843	26.028391
185.035871	7737.396441	26.033408
184.851383	7747.183641	26.038426
185.385160	7735.793325	26.043444
185.465033	7749.003461	26.048461
185.736102	7770.599417	26.053479
185.964475	7768.533352	26.058496
185.714701	7777.398731	26.063514
186.194924	7782.404779	26.068532
186.425751	7786.826678	26.073549
186.249889	7804.275335	26.078567
186.524832	7798.632436	26.083584
186.658961	7817.354714	26.088602
187.000051	7825.681175	26.093620
187.137675	7832.728997	26.098637
187.103665	7835.083686	26.103655
187.382154	7848.631246	26.108672
187.559766	7868.614604	26.113690
187.874701	7862.348281	26.118708
188.358330	7875.119872	26.123725
188.548721	7888.343334	26.128743
188.662638	7882.510444	26.133760
188.474701	7892.095073	26.138778
188.554787	7899.244614	26.143796
188.703803	7914.552155	26.148813
189.015530	7935.795008	26.153831
189.445496	7942.321847	26.158848
188.805856	7952.422420	26.163866
189.166675	7961.166327	26.168884
189.521688	7982.695108	26.173901
190.095860	7996.564855	26.178919
190.492503	8003.346944	26.183936
190.594382	8019.901476	26.188954
191.268237	8015.278725	26.193972
191.144762	8019.213457	26.198989
191.182516	8026.069941	26.204007
191.838720	8031.607792	26.209024
191.816676	8054.267248	26.214042
191.669716	8049.765418	26.219060
191.964427	8056.449398	26.224077
192.100632	8076.340619	26.229095
192.316425	8074.527095	26.234112
191.935121	8092.396065	26.239130
192.728302	8108.419528	26.244148
192.668008	8112.159495	26.249165
192.736574	8135.969901	26.254183
193.296825	8141.123510	26.259200
193.325975	8154.798475	26.264218
193.458909	8164.175747	26.269236
193.697270	8183.514532	26.274253
193.956961	8188.877828	26.279271
194.457170	8202.873435	26.284288
193.826272	8208.470837	26.289306
194.529773	8221.949137	26.294324
195.136757	8239.241087	26.299341
195.501318	8226.546385	26.304359
195.525024	8238.741385	26.309376
195.749363	8244.242105	26.314394
196.286583	8261.020999	26.319412
196.475552	8258.230380	26.324429
196.270531	8249.984554	26.329447
196.752436	8252.009691	26.334464
196.390025	8263.406857	26.339482
196.773122	8277.816574	26.344500
196.671408	8283.226346	26.349517
196.755659	8296.192800	26.354535
197.043054	8310.625482	26.359552
197.142095	8315.857084	26.364570
197.427141	8323.960703	26.369588
197.543550	8355.990645	26.374605
197.296246	8378.313679	26.379623
198.185967	8383.516015	26.384640
197.913982	8397.937406	26.389658
198.384965	8409.978924	26.394676
198.627046	8419.067292	26.399693
198.753721	8442.083155	26.404711
199.011313	8447.608374	26.409728
199.415686	8456.745518	26.414746
199.376547	8461.604598	26.419764
199.753245	8470.408389	26.424781
200.024155	8476.969661	26.429799
200.226623	8486.270227	26.434816
199.983542	8499.796772	26.439834
200.674218	8502.920945	26.444852
200.797342	8511.222409	26.449869
200.904055	8522.057624	26.454887
201.276117	8528.322520	26.459904
201.107556	8527.667549	26.464922
201.443590	8550.558316	26.469940
201.783540	8554.758336	26.474957
201.840150	8563.833380	26.479975
202.242048	8569.713658	26.484992
201.894575	8589.721833	26.490010
201.742420	8584.464470	26.495028
202.418599	8614.668416	26.500045
202.607671	8641.079685	26.505063
203.381057	8639.325820	26.510080
203.408460	8649.429038	26.515098
203.744374	8661.185885	26.520116
203.783394	8680.325101	26.525133
203.842580	8687.411496	26.530151
204.350211	8689.887754	26.535168
204.243299	8700.136132	26.540186
204.543640	8699.918714	26.545204
204.635268	8710.646270	26.550221
204.813900	8736.931021	26.555239
205.304017	8735.323302	26.560256
205.506363	8763.639736	26.565274
205.720153	8764.729359	26.570292
205.931728	8766.781202	26.575309
206.066402	8791.881442	26.580327
206.248441	8790.835192	26.585344
206.322182	8810.483222	26.590362
206.590764	8825.533938	26.595380
206.879940	8825.012716	26.600397
207.074542	8838.111015	26.605415
207.314393	8854.744403	26.610432
207.665021	8864.157732	26.615450
207.680832	8859.765794	26.620468
207.889128	8881.943201	26.625485
207.869587	8890.122745	26.630503
208.599049	8913.803622	26.635520
208.558477	8922.106404	26.640538
208.747009	8923.348320	26.645556
209.027410	8935.012150	26.650573
209.257006	8947.411510	26.655591
209.582658	8944.587115	26.660608
209.826872	8962.432268	26.665626
209.626627	8975.477096	26.670644
210.443666	8978.292122	26.675661
210.415145	8987.316904	26.680679
210.680957	8991.899567	26.685696
210.587005	9004.037428	26.690714
210.607462	9021.477753	26.695732
211.026888	9029.705222	26.700749
211.174136	9049.957414	26.705767
210.976403	9052.173167	26.710784
211.228561	9067.237859	26.715802
211.638740	9084.532589	26.720820
211.970794	9098.175542	26.725837
211.881064	9117.951848	26.730855
212.409482	9124.861492	26.735872
212.638783	9137.873150	26.740890
212.630094	9161.191331	26.745908
212.815831	9171.461671	26.750925
213.311309	9185.693685	26.755943
213.824312	9194.272853	26.760960
214.031641	9203.412326	26.765978
214.098686	9205.136805	26.770996
214.297514	9216.789925	26.776013
214.355862	9227.704526	26.781031
214.247978	9219.635910	26.786048
214.549047	9240.355239	26.791066
214.649418	9260.496502	26.796084
215.192278	9273.290924	26.801101
214.912688	9292.493860	26.806119
215.304259	9301.309830	26.811136
215.611667	9324.869760	26.816154
215.850101	9324.849291	26.821172
216.427260	9342.628718	26.826189
216.157941	9361.897785	26.831207
216.660440	9366.146739	26.836224
216.684142	9374.844037	26.841242
216.912529	9403.447197	26.846260
217.379199	9405.995740	26.851277
217.538954	9423.896355	26.856295
217.590587	9430.153209	26.861312
218.043107	9436.596578	26.866330
217.868322	9462.574707	26.871348
218.508451	9463.756081	26.876365
218.707463	9480.083339	26.881383
219.046179	9501.679891	26.886400
219.117448	9496.051213	26.891418
219.244707	9518.206678	26.896436
219.719120	9537.906647	26.901453
219.740658	9541.270224	26.906471
219.942625	9558.544792	26.911488
220.136745	9567.930089	26.916506
220.238951	9581.149858	26.921524
220.754416	9590.975130	26.926541
220.725163	9603.179937	26.931559
221.152632	9615.371376	26.936576
221.510463	9621.732021	26.941594
221.465411	9642.081396	26.946612
222.166731	9645.645209	26.951629
222.067368	9651.456831	26.956647
222.394087	9668.270483	26.961664
222.751333	9675.202403	26.966682
222.717210	9693.668760	26.971700
223.241897	9701.338717	26.976717
223.134152	9704.693794	26.981735
223.338967	9724.521346	26.986752
223.692714	9738.990026	26.991770
223.501753	9746.717824	26.996788
223.761598	9771.061486	27.001805
224.226577	9780.987408	27.006823
224.258504	9802.587887	27.011840
224.427409	9817.004519	27.016858
224.791353	9838.043516	27.021876
225.272303	9832.389438	27.026893
225.240982	9853.628610	27.031911
225.594964	9866.313760	27.036928
226.143040	9879.077080	27.041946
225.884891	9904.371720	27.046964
226.413136	9906.665141	27.051981
226.851801	9917.069768	27.056999
227.129775	9923.844753	27.062016
227.268049	9932.832998	27.067034
227.356882	9936.011408	27.072052
227.645619	9947.058524	27.077069
227.799080	9957.124365	27.082087
227.808662	9961.214800	27.087104
228.256565	9971.986633	27.092122
228.340422	9981.269891	27.097140
228.630422	9995.829715	27.102157
228.697268	10014.935189	27.107175
229.083252	10011.048096	27.112192
229.080856	10026.587558	27.117210
229.282053	10052.227080	27.122228
229.350070	10047.384995	27.127245
229.864013	10061.792781	27.132263
229.722064	10074.532626	27.137280
229.807274	10087.829680	27.142298
230.141121	10114.765369	27.147316
230.412200	10127.848122	27.152333
230.825290	10141.284744	27.157351
231.016323	10157.919689	27.162368
231.546375	10159.094922	27.167386
231.540721	10186.112147	27.172404
232.214194	10199.867324	27.177421
232.151239	10203.629487	27.182439
231.988033	10231.663961	27.187456
232.712202	10232.421814	27.192474
232.926870	10249.144329	27.197492
233.359991	10269.888821	27.202509
233.338126	10267.069736	27.207527
233.518847	10291.835383	27.212544
234.013350	10293.282800	27.217562
233.769635	10315.993964	27.222580
234.544997	10327.896729	27.227597
234.559042	10335.117378	27.232615
234.816913	10351.313663	27.237632
235.213365	10367.003290	27.242650
235.216188	10387.399254	27.247668
235.571417	10392.165265	27.252685
235.766992	10395.066897	27.257703
236.125099	10405.684503	27.262720
236.597201	10415.082576	27.267738
236.496493	10428.821943	27.272756
236.613507	10438.923269	27.277773
236.721316	10452.604501	27.282791
236.833716	10477.833966	27.287808
237.193286	10486.237546	27.292826
237.561604	10514.572134	27.297844
237.245087	10515.647255	27.302861
238.015949	10541.093189	27.307879
238.150871	10559.002330	27.312896
238.399321	10566.668015	27.317914
238.762859	10582.944733	27.322932
239.165186	10601.873247	27.327949
239.412521	10612.985190	27.332967
239.490842	10630.985718	27.337984
239.948362	10630.264036	27.343002
240.058006	10651.856726	27.348020
240.366213	10662.314163	27.353037
240.631093	10675.563049	27.358055
241.060628	10688.691721	27.363072
241.217959	10689.244057	27.368090
241.119603	10709.147437	27.373108
241.477431	10718.928595	27.378125
242.166266	10719.202281	27.383143
241.820737	10745.076017	27.388160
242.484704	10750.166044	27.393178
242.833078	10764.066131	27.398196
243.055180	10784.701257	27.403213
243.377239	10781.677815	27.408231
243.497904	10787.373057	27.413248
243.785776	10801.848875	27.418266
243.791654	10820.329595	27.423284
243.997639	10821.193753	27.428301
244.238962	10826.268684	27.433319
244.244280	10844.002634	27.438336
244.942614	10855.427708	27.443354
244.992575	10875.877150	27.448372
245.358260	10883.180070	27.453389
245.572143	10879.898767	27.458407
245.361438	10884.478138	27.463424
245.776004	10894.459583	27.468442
245.814880	10914.474432	27.473460
246.390955	10926.241246	27.478477
246.478264	10933.977904	27.483495
246.340518	10959.634800	27.488512
246.456088	10972.095571	27.493530
246.623002	10995.628422	27.498548
247.176672	11016.297194	27.503565
247.808522	11037.852797	27.508583
247.660577	11048.009399	27.513600
247.798597	11067.459667	27.518618
247.890963	11087.957508	27.523636
248.469778	11099.411997	27.528653
248.846344	11119.916405	27.533671
248.782639	11132.145404	27.538688
249.162724	11154.656777	27.543706
249.389180	11167.113523	27.548724
250.061689	11192.970711	27.553741
250.263014	11196.760263	27.558759
250.601375	11214.847604	27.563776
250.782169	11231.557050	27.568794
251.189218	11239.707346	27.573812
251.315938	11251.553516	27.578829
252.095460	11260.789315	27.583847
251.743741	11271.441489	27.588864
252.279096	11285.585256	27.593882
252.456856	11309.127798	27.598900
252.675152	11303.959488	27.603917
253.210167	11321.812696	27.608935
253.006831	11339.304395	27.613952
253.331402	11347.980526	27.618970
253.576895	11366.863418	27.623988
253.714779	11372.806564	27.629005
254.127682	11391.083462	27.634023
254.102115	11402.962833	27.639040
254.442137	11426.683535	27.644058
254.579094	11435.627139	27.649076
255.375935	11454.385767	27.654093
255.419440	11464.041353	27.659111
255.789550	11485.576279	27.664128
255.775588	11506.356984	27.669146
256.141981	11513.742016	27.674164
256.533070	11526.149723	27.679181
256.929220	11541.898851	27.684199
256.914735	11563.472337	27.689216
257.443392	11569.281529	27.694234
257.225685	11590.190619	27.699252
257.553431	11596.302541	27.704269
258.136998	11617.841702	27.709287
258.085036	11634.610582	27.714304
258.522525	11644.851856	27.719322
258.641310	11662.826349	27.724340
258.818674	11675.811629	27.729357
259.524586	11676.328339	27.734375
259.444699	11702.537817	27.739392
259.627880	11713.253005	27.744410
260.265541	11726.875966	27.749428
260.104513	11749.977280	27.754445
260.217229	11760.715196	27.759463
260.688660	11778.413976	27.764480
261.130475	11788.972940	27.769498
261.213389	11806.253869	27.774516
261.512775	11825.350565	27.779533
262.009377	11842.574079	27.784551
261.873103	11847.473896	27.789568
262.369720	11870.100920	27.794586
262.573829	11877.352250	27.799604
262.573301	11889.744702	27.804621
262.795471	11902.820448	27.809639
263.050911	11922.929909	27.814656
263.582190	11927.508078	27.819674
263.681702	11938.150596	27.824692
263.874963	11965.033857	27.829709
264.313568	11975.842457	27.834727
264.246500	11998.581886	27.839744
264.526024	12012.519662	27.844762
265.099529	12029.396567	27.849780
265.242683	12055.453079	27.854797
265.577310	12069.035097	27.859815
265.348368	12100.887764	27.864832
265.699380	12112.621793	27.869850
266.045002	12129.172508	27.874868
266.270195	12155.864848	27.879885
266.747430	12172.296116	27.884903
267.068327	12200.622602	27.889920
267.191384	12218.357474	27.894938
267.647618	12232.147996	27.899956
267.947016	12260.500207	27.904973
268.299506	12272.396421	27.909991
268.529555	12295.247817	27.915008
269.134659	12305.595712	27.920026
269.104639	12320.708587	27.925044
269.233640	12335.982678	27.930061
269.836165	12353.274299	27.935079
270.066034	12366.349144	27.940096
270.071658	12388.090590	27.945114
270.669050	12406.303426	27.950132
270.932890	12420.564051	27.955149
271.390518	12418.215982	27.960167
271.294098	12440.907308	27.965184
271.713725	12456.724356	27.970202
272.304165	12476.864145	27.975220
272.032410	12491.714627	27.980237
272.801090	12496.783156	27.985255
272.849293	12510.020565	27.990272
273.045404	12523.506127	27.995290
273.473438	12547.815890	28.000308
273.590051	12562.717184	28.005325
274.141961	12568.641083	28.010343
274.284530	12583.627926	28.015360
274.488268	12606.785110	28.020378
275.098061	12617.401908	28.025396
274.844263	12640.783017	28.030413
275.248882	12649.514361	28.035431
275.404725	12661.944551	28.040448
275.761692	12685.112726	28.045466
276.429857	12698.409976	28.050484
276.166594	12714.426997	28.055501
276.352786	12727.469967	28.060519
276.646324	12758.822963	28.065536
276.926251	12770.266663	28.070554
277.319152	12786.707789	28.075572
277.204134	12802.307954	28.080589
277.961058	12830.651609	28.085607
278.209783	12849.003034	28.090624
278.420988	12873.300325	28.095642
278.829340	12887.080421	28.100660
279.010040	12908.609196	28.105677
279.421825	12919.104532	28.110695
279.711162	12947.097144	28.115712
279.876155	12960.990082	28.120730
280.586627	12962.073424	28.125748
280.742851	12977.764384	28.130765
280.795250	12995.340024	28.135783
281.171300	13003.655515	28.140800
281.238726	13015.536428	28.145818
281.325752	13025.488316	28.150836
281.878790	13052.881153	28.155853
281.569501	13063.938788	28.160871
282.375625	13088.141067	28.165888
282.234877	13105.699945	28.170906
282.527971	13114.921209	28.175924
282.835689	13153.052318	28.180941
283.185743	13163.581670	28.185959
283.450911	13178.736303	28.190976
283.704223	13204.831578	28.195994
284.541451	13222.775541	28.201012
284.263765	13247.062915	28.206029
284.902946	13258.688610	28.211047
284.868620	13294.205427	28.216064
285.137456	13310.667621	28.221082
286.126750	13318.602813	28.226100
285.564317	13350.473725	28.231117
286.023970	13365.385157	28.236135
286.270875	13387.950047	28.241152
286.345107	13421.917331	28.246170
287.099377	13432.644707	28.251188
287.236719	13451.581023	28.256205
287.266591	13474.407325	28.261223
287.762474	13496.669538	28.266240
287.989753	13520.889486	28.271258
288.419904	13536.625469	28.276276
288.424989	13563.974339	28.281293
288.976348	13590.277777	28.286311
289.295758	13609.915396	28.291328
289.335880	13633.170467	28.296346
289.973026	13649.028316	28.301364
290.484712	13683.426469	28.306381
290.851742	13692.197694	28.311399
291.222161	13713.708734	28.316416
291.264229	13730.186827	28.321434
291.957477	13743.877937	28.326452
292.210706	13761.503107	28.331469
292.419939	13780.517737	28.336487
292.692756	13782.349696	28.341504
292.853341	13813.794498	28.346522
293.403530	13810.455366	28.351540
293.604409	13845.961238	28.356557
293.665728	13861.678215	28.361575
294.111898	13869.445123	28.366592
293.999710	13898.933705	28.371610
294.379603	13918.869007	28.376628
294.803374	13938.871142	28.381645
294.902107	13956.310911	28.386663
295.083786	13976.066331	28.391680
295.406865	14001.494128	28.396698
295.813426	14014.701804	28.401716
296.239720	14041.422256	28.406733
296.520062	14060.110233	28.411751
297.105267	14082.413621	28.416768
297.163712	14098.656120	28.421786
297.139568	14111.723984	28.426804
297.681692	14142.490027	28.431821
298.106423	14156.424517	28.436839
298.537577	14176.108937	28.441856
298.869135	14208.968275	28.446874
299.051627	14220.796344	28.451892
299.481932	14245.122449	28.456909
300.023441	14255.765812	28.461927
300.458330	14270.117947	28.466944
300.167250	14289.442940	28.471962
300.587891	14284.208677	28.476980
300.746669	14304.997449	28.481997
300.918912	14321.025900	28.487015
301.413151	14342.651237	28.492032
301.200049	14354.905806	28.497050
301.933897	14372.738918	28.502068
302.196775	14389.494759	28.507085
302.363250	14414.744233	28.512103
302.354102	14424.240073	28.517120
302.435622	14462.022391	28.522138
303.250077	14482.538938	28.527156
303.797943	14502.242256	28.532173
304.028683	14527.796482	28.537191
304.383337	14536.852330	28.542208
304.439223	14551.232777	28.547226
304.962923	14569.573716	28.552244
305.161008	14589.864605	28.557261
305.612539	14607.751013	28.562279
306.135502	14620.988770	28.567296
305.959032	14647.795807	28.572314
306.745478	14666.247818	28.577332
306.834080	14683.407917	28.582349
307.191814	14711.267719	28.587367
307.561414	14724.023444	28.592384
307.556954	14744.770447	28.597402
307.937886	14761.904303	28.602420
308.347361	14783.033598	28.607437
308.250170	14820.909368	28.612455
308.863095	14837.188477	28.617472
309.094133	14864.697551	28.622490
309.336802	14884.478645	28.627508
309.300808	14904.805519	28.632525
309.763229	14941.480924	28.637543
310.084246	14964.492794	28.642560
310.473086	14998.702848	28.647578
311.038248	15015.540108	28.652596
311.146008	15029.693305	28.657613
311.411757	15056.645310	28.662631
311.742256	15083.810451	28.667648
311.791422	15103.748355	28.672666
312.406602	15128.281589	28.677684
312.956042	15157.139629	28.682701
313.348009	15181.355261	28.687719
313.930535	15204.139770	28.692736
314.101615	15227.378574	28.697754
314.651146	15239.029986	28.702772
314.875611	15254.005719	28.707789
314.950769	15287.393538	28.712807
315.468813	15297.277034	28.717824
315.707814	15316.247538	28.722842
315.990078	15338.140974	28.727860
316.129053	15361.825029	28.732877
316.333778	15386.283163	28.737895
316.927039	15400.001677	28.742912
316.984829	15425.390483	28.747930
317.486828	15444.591852	28.752948
317.591386	15461.048728	28.757965
317.563656	15488.803430	28.762983
318.241546	15505.824284	28.768000
318.724173	15544.964398	28.773018
318.965406	15561.836927	28.778036
319.525652	15581.060338	28.783053
319.383399	15602.130703	28.788071
320.258443	15614.773508	28.793088
320.493847	15641.758290	28.798106
320.575690	15658.956777	28.803124
321.072388	15693.708393	28.808141
320.810865	15710.495644	28.813159
321.250123	15721.984392	28.818176
321.393249	15752.316699	28.823194
321.924448	15775.499818	28.828212
322.546378	15786.673082	28.833229
322.267462	15815.603198	28.838247
323.162084	15828.933304	28.843264
323.274261	15864.499202	28.848282
323.689077	15880.309333	28.853300
324.211209	15896.492615	28.858317
324.603720	15923.436090	28.863335
324.524976	15929.520788	28.868352
324.895274	15959.157015	28.873370
325.337337	15976.787985	28.878388
325.860607	16000.830196	28.883405
325.854973	16027.508741	28.888423
326.179419	16043.299311	28.893440
326.417275	16071.212785	28.898458
326.836044	16090.304164	28.903476
327.320121	16116.115252	28.908493
327.597502	16141.766719	28.913511
327.880867	16161.865740	28.918528
328.236188	16188.027686	28.923546
328.264888	16207.218447	28.928564
328.805117	16230.961854	28.933581
329.152535	16265.588066	28.938599
329.530287	16283.308822	28.943616
329.669052	16313.077009	28.948634
329.615834	16340.818445	28.953652
330.570549	16362.925063	28.958669
330.380998	16405.364092	28.963687
331.130190	16427.126515	28.968704
332.001511	16452.528829	28.973722
332.076497	16465.921045	28.978740
332.671037	16496.944484	28.983757
332.834161	16516.307232	28.988775
333.495290	16523.861708	28.993792
333.580811	16548.907176	28.998810
333.838714	16571.045875	29.003828
334.727072	16591.887005	29.008845
334.425133	16608.101785	29.013863
334.783755	16634.872336	29.018880
335.176322	16645.967509	29.023898
335.345861	16659.126704	29.028916
335.353626	16680.509356	29.033933
335.741760	16706.464928	29.038951
336.380957	16745.192631	29.043968
336.864388	16774.102264	29.048986
336.924734	16797.866022	29.054004
337.440919	16810.832397	29.059021
337.268977	16841.108513	29.064039
337.829502	16868.465506	29.069056
338.333738	16895.551281	29.074074
338.292526	16915.635587	29.079092
338.753679	16937.441635	29.084109
339.370291	16975.607722	29.089127
339.713273	17003.264191	29.094144
339.906871	17025.633250	29.099162
340.138736	17055.790897	29.104180
340.335412	17083.233694	29.109197
340.293024	17114.838195	29.114215
340.992936	17144.450360	29.119232
341.434630	17181.386390	29.124250
341.431239	17211.052037	29.129268
342.146386	17231.637332	29.134285
342.662836	17260.670032	29.139303
343.417084	17287.949939	29.144320
343.573686	17316.733340	29.149338
343.644079	17337.092882	29.154356
344.101913	17350.383032	29.159373
344.105766	17379.770345	29.164391
344.574110	17400.923204	29.169408
344.972796	17424.973924	29.174426
345.012819	17453.355971	29.179444
345.759722	17483.161162	29.184461
346.262441	17504.759303	29.189479
346.398283	17526.689334	29.194496
347.012921	17554.640676	29.199514
347.143802	17568.442267	29.204532
347.642414	17595.473368	29.209549
347.742756	17624.097941	29.214567
347.829275	17650.040285	29.219584
348.255933	17670.514666	29.224602
348.530850	17694.368723	29.229620
349.294340	17717.424690	29.234637
349.316955	17753.666816	29.239655
349.790059	17782.638245	29.244672
350.125127	17810.666245	29.249690
350.143618	17842.460675	29.254708
350.782100	17871.663413	29.259725
351.080795	17901.644435	29.264743
351.089001	17940.241339	29.269760
351.418758	17956.524695	29.274778
352.001324	17991.911674	29.279796
352.664600	18027.621145	29.284813
352.603034	18066.728036	29.289831
353.116869	18084.768702	29.294848
354.011358	18122.183621	29.299866
354.210068	18152.799602	29.304884
354.721383	18164.607600	29.309901
355.159281	18195.699560	29.314919
355.660020	18223.216869	29.319936
356.062089	18234.361982	29.324954
356.554848	18264.076648	29.329972
357.289357	18281.450429	29.334989
357.333166	18305.539094	29.340007
357.472972	18308.066726	29.345024
358.007014	18313.713507	29.350042
358.013636	18354.394106	29.355060
358.588117	18365.666837	29.360077
358.885867	18395.346228	29.365095
358.894399	18424.192311	29.370112
359.378772	18447.628125	29.375130
359.319831	18475.730345	29.380148
359.485991	18499.955107	29.385165
359.654126	18531.566859	29.390183
360.305716	18570.342487	29.395200
361.032075	18598.174623	29.400218
361.077333	18639.547893	29.405236
361.887967	18657.361915	29.410253
362.295363	18684.885979	29.415271
362.402824	18713.277926	29.420288
363.347990	18741.204931	29.425306
363.482879	18770.349144	29.430324
363.900050	18793.925840	29.435341
364.069146	18812.114218	29.440359
364.364312	18841.892574	29.445376
364.818931	18865.731176	29.450394
364.976613	18882.534209	29.455412
365.211924	18922.218253	29.460429
365.842366	18948.048937	29.465447
365.858698	18976.254622	29.470464
366.448900	19003.823050	29.475482
366.630206	19044.389705	29.480500
367.358397	19062.304515	29.485517
367.291301	19094.298368	29.490535
367.619878	19124.074849	29.495552
368.176507	19147.599008	29.500570
368.095667	19178.702989	29.505588
368.674020	19203.960956	29.510605
369.175702	19232.670050	29.515623
369.491486	19265.392271	29.520640
369.911883	19285.541758	29.525658
370.279245	19324.897476	29.530676
370.720900	19352.437465	29.535693
371.208858	19383.110299	29.540711
371.113983	19408.494197	29.545728
372.155675	19440.011947	29.550746
371.891662	19463.167889	29.555764
372.472703	19497.465770	29.560781
372.952593	19527.438641	29.565799
373.055963	19561.880356	29.570816
373.968219	19585.160236	29.575834
373.894357	19614.628980	29.580852
374.349392	19643.786361	29.585869
374.963578	19669.233018	29.590887
375.025860	19700.150313	29.595904
375.642962	19726.291840	29.600922
375.923903	19762.489254	29.605940
376.308165	19788.715139	29.610957
376.784450	19815.225383	29.615975
377.121663	19848.074474	29.620992
377.432813	19872.833758	29.626010
377.760598	19912.785473	29.631028
378.301502	19943.423768	29.636045
378.392800	19972.053858	29.641063
378.620641	20012.071225	29.646080
379.362138	20047.429950	29.651098
379.557896	20086.882077	29.656116
380.006978	20102.889215	29.661133
380.766513	20135.996902	29.666151
380.897991	20169.695781	29.671168
381.423715	20194.927694	29.676186
381.857453	20228.923518	29.681204
382.224399	20263.684091	29.686221
382.560378	20294.270232	29.691239
382.847083	20325.266624	29.696256
383.619632	20350.492603	29.701274
383.700228	20384.004831	29.706292
384.253128	20414.701914	29.711309
385.152074	20433.015627	29.716327
385.379175	20464.269673	29.721344
385.634594	20482.636348	29.726362
385.720586	20504.463439	29.731380
386.163893	20544.416454	29.736397
386.564987	20557.633422	29.741415
386.440818	20583.638833	29.746432
386.763512	20617.761035	29.751450
387.088483	20656.576638	29.756468
387.860578	20696.254862	29.761485
388.099840	20733.200718	29.766503
388.021335	20769.537050	29.771520
388.811063	20802.306801	29.776538
389.324173	20839.664799	29.781556
389.598906	20875.884556	29.786573
390.312533	20908.359657	29.791591
390.703235	20950.271119	29.796608
391.154599	20972.609101	29.801626
391.485518	21000.671511	29.806644
391.730120	21030.654475	29.811661
392.236973	21071.120106	29.816679
392.656836	21100.473464	29.821696
393.233862	21124.684465	29.826714
393.933373	21161.965025	29.831732
394.015868	21169.455009	29.836749
394.391681	21190.665827	29.841767
394.787617	21227.858029	29.846784
395.164772	21245.120610	29.851802
395.402256	21265.137196	29.856820
395.834432	21297.885103	29.861837
396.019348	21314.033300	29.866855
396.349206	21349.787702	29.871872
397.004681	21379.873568	29.876890
397.273148	21414.430497	29.881908
397.573592	21443.015853	29.886925
397.813130	21469.187899	29.891943
397.939957	21510.116396	29.896960
398.079295	21539.595786	29.901978
399.069469	21584.602501	29.906996
399.341270	21633.116669	29.912013
399.844303	21658.808637	29.917031
399.956009	21698.377779	29.922048
400.484597	21724.797232	29.927066
400.966875	21761.500137	29.932084
401.176441	21794.765187	29.937101
401.882840	21829.327741	29.942119
401.982400	21874.526786	29.947136
402.666641	21900.029876	29.952154
403.131267	21942.887089	29.957172
403.693264	21982.421785	29.962189
404.399304	22013.711380	29.967207
404.612946	22046.079059	29.972224
404.898366	22080.521013	29.977242
405.505000	22113.757236	29.982260
405.899448	22146.058914	29.987277
406.429324	22168.000747	29.992295
406.240209	22211.422536	29.997312
406.859159	22235.587196	30.002330
407.581271	22269.376992	30.007348
407.458187	22306.652738	30.012365
408.265454	22328.961993	30.017383
408.691200	22368.791354	30.022400
409.110557	22399.298128	30.027418
409.441178	22436.174240	30.032436
409.768157	22467.551065	30.037453
410.122266	22498.546596	30.042471
410.621087	22539.773948	30.047488
411.108235	22579.527414	30.052506
411.611179	22615.311030	30.057524
411.650776	22658.429619	30.062541
412.555731	22678.887722	30.067559
412.797721	22718.948577	30.072576
413.585945	22744.279623	30.077594
414.147699	22776.253632	30.082612
414.331174	22808.992012	30.087629
414.674090	22831.090219	30.092647
414.969453	22865.828571	30.097664
415.143684	22891.654097	30.102682
415.894968	22929.691611	30.107700
415.917062	22957.966066	30.112717
416.577137	22999.092155	30.117735
416.837436	23028.191429	30.122752
417.224519	23068.661157	30.127770
417.754066	23091.957206	30.132788
417.896790	23131.347940	30.137805
418.577143	23179.773678	30.142823
418.885434	23211.385195	30.147840
419.299159	23242.481021	30.152858
419.856758	23279.982116	30.157876
420.203685	23314.867386	30.162893
420.928912	23352.334590	30.167911
421.126611	23384.297459	30.172928
421.038172	23420.175916	30.177946
421.718512	23445.483289	30.182964
421.870989	23484.636687	30.187981
422.618866	23512.392977	30.192999
422.373390	23557.655175	30.198016
423.048266	23595.722596	30.203034
423.515236	23626.657348	30.208052
423.858587	23669.050138	30.213069
424.578725	23711.218247	30.218087
424.773904	23748.124348	30.223104
425.139643	23787.105949	30.228122
425.584994	23827.487411	30.233140
425.826211	23866.515034	30.238157
426.694194	23907.974761	30.243175
426.923263	23954.870470	30.248192
427.226313	23997.004237	30.253210
427.891597	24025.837910	30.258228
428.293839	24072.771513	30.263245
428.966869	24116.228923	30.268263
429.451226	24144.165478	30.273280
429.585276	24182.501917	30.278298
430.368402	24228.940817	30.283316
430.229754	24268.215156	30.288333
431.055368	24304.907728	30.293351
431.374537	24346.270113	30.298368
432.191145	24386.235049	30.303386
432.538430	24414.869689	30.308404
432.578661	24457.199479	30.313421
433.472904	24493.748631	30.318439
433.850976	24536.915293	30.323456
434.339526	24572.736941	30.328474
434.974242	24610.395360	30.333492
435.643652	24645.644732	30.338509
435.826471	24666.320950	30.343527
436.201625	24700.341741	30.348544
436.526795	24734.225786	30.353562
437.155072	24764.561861	30.358580
437.374850	24799.204684	30.363597
437.784689	24833.387166	30.368615
438.137998	24875.275064	30.373632
438.499735	24918.133133	30.378650
439.180318	24947.817439	30.383668
439.720397	24995.039860	30.388685
440.209420	25029.373641	30.393703
440.317832	25069.993584	30.398720
440.865650	25120.031707	30.403738
441.620773	25149.243521	30.408756
441.696545	25189.481188	30.413773
442.175151	25220.760702	30.418791
442.588954	25265.569754	30.423808
442.524359	25302.686212	30.428826
443.133627	25338.060512	30.433844
443.324060	25393.697323	30.438861
444.264595	25437.189513	30.443879
444.754730	25478.009041	30.448896
444.814919	25524.608952	30.453914
445.691173	25565.834763	30.458932
445.972111	25620.924265	30.463949
446.725358	25655.890575	30.468967
447.035624	25693.860564	30.473984
447.608395	25736.957013	30.479002
448.216586	25772.395470	30.484020
448.493699	25808.207376	30.489037
449.086137	25834.772464	30.494055
449.588617	25865.535053	30.499072
449.528795	25908.515827	30.504090
450.309209	25948.351607	30.509108
450.886426	25988.883512	30.514125
451.043919	26020.006285	30.519143
451.852922	26053.276622	30.524160
452.108200	26090.073718	30.529178
452.360525	26116.011042	30.534196
452.850330	26148.741379	30.539213
453.624013	26188.736546	30.544231
453.840290	26214.023882	30.549248
454.226032	26263.536989	30.554266
454.904334	26285.596770	30.559284
454.969849	26332.283147	30.564301
455.212462	26369.748505	30.569319
455.704205	26404.986730	30.574336
455.948905	26456.703407	30.579354
456.644148	26493.841774	30.584372
457.069745	26541.607857	30.589389
457.077787	26587.036364	30.594407
457.813432	26626.707629	30.599424
458.065924	26681.798914	30.604442
458.600567	26728.572750	30.609460
458.954674	26787.536973	30.614477
459.459755	26833.416967	30.619495
459.860809	26877.166110	30.624512
460.644063	26928.271425	30.629530
461.377555	26975.224367	30.634548
461.835107	27019.803613	30.639565
462.112582	27061.176263	30.644583
462.793791	27089.107108	30.649600
463.097997	27141.421645	30.654618
463.667853	27184.550580	30.659636
464.251022	27236.588957	30.664653
464.759046	27280.592705	30.669671
465.420303	27318.801547	30.674688
465.770655	27358.557184	30.679706
466.665850	27394.585539	30.684724
466.762470	27443.039464	30.689741
467.224232	27478.868433	30.694759
467.498317	27520.280594	30.699776
467.760895	27569.861982	30.704794
468.430271	27615.757867	30.709812
469.064550	27652.050760	30.714829
469.439970	27694.257297	30.719847
470.169217	27740.354962	30.724864
470.390289	27788.287668	30.729882
470.802678	27815.065415	30.734900
471.385473	27868.030054	30.739917
471.475864	27921.773523	30.744935
472.222427	27960.821418	30.749952
472.560995	28015.101405	30.754970
473.188645	28052.516139	30.759988
473.533107	28094.514254	30.765005
473.997797	28149.742275	30.770023
474.608010	28198.088067	30.775040
475.009442	28244.361199	30.780058
475.947726	28283.721954	30.785076
476.382355	28331.623967	30.790093
476.542152	28367.126174	30.795111
477.364318	28398.225236	30.800128
478.264848	28436.015216	30.805146
478.741077	28465.793027	30.810164
479.405145	28500.470686	30.815181
479.810685	28535.904175	30.820199
479.861206	28565.547549	30.825216
480.364314	28610.845778	30.830234
480.951580	28641.753853	30.835252
481.085432	28683.021628	30.840269
481.474795	28719.805262	30.845287
482.032136	28756.116348	30.850304
482.221544	28813.546759	30.855322
482.765734	28844.862984	30.860340
483.223528	28878.947724	30.865357
483.538986	28924.981349	30.870375
484.174544	28965.340196	30.875392
484.342816	29012.780230	30.880410
484.677036	29057.072776	30.885428
485.135732	29103.859262	30.890445
485.487416	29157.004878	30.895463
486.486325	29197.913022	30.900480
486.601013	29256.082874	30.905498
487.097043	29291.528159	30.910516
487.332908	29335.941800	30.915533
488.146535	29394.920831	30.920551
488.486307	29441.680577	30.925568
488.874088	29499.424296	30.930586
489.122842	29542.687931	30.935604
489.975096	29595.723643	30.940621
490.445484	29658.054136	30.945639
491.365737	29702.342825	30.950656
491.741028	29754.416811	30.955674
492.056989	29810.741078	30.960692
492.836913	29858.189447	30.965709
493.534079	29906.882093	30.970727
494.051338	29953.976659	30.975744
494.105761	30005.041247	30.980762
494.878271	30043.764544	30.985780
495.349808	30094.470101	30.990797
495.559312	30144.010784	30.995815
496.425645	30189.189887	31.000832
496.961314	30247.394316	31.005850
497.584507	30290.591517	31.010868
497.943131	30331.829129	31.015885
498.634434	30388.481208	31.020903
499.010736	30428.343655	31.025920
499.319816	30483.453346	31.030938
499.715975	30518.639990	31.035956
500.496996	30575.189480	31.040973
500.857021	30631.572187	31.045991
501.122760	30670.702556	31.051008
501.369699	30730.010181	31.056026
501.804272	30784.980152	31.061044
502.839178	30839.254618	31.066061
503.445310	30898.430798	31.071079
503.847465	30950.115790	31.076096
504.481471	30997.105482	31.081114
504.867788	31056.012513	31.086132
505.495334	31090.745520	31.091149
505.486706	31147.225589	31.096167
506.537027	31197.198028	31.101184
506.972170	31252.923465	31.106202
507.425093	31306.481627	31.111220
508.169031	31357.593789	31.116237
508.414391	31408.766519	31.121255
509.062645	31451.135737	31.126272
509.766391	31508.505608	31.131290
510.016712	31552.165175	31.136308
510.651552	31607.038303	31.141325
511.191815	31668.903671	31.146343
511.450447	31711.479981	31.151360
511.916962	31769.072964	31.156378
512.550895	31812.868478	31.161396
513.350332	31856.955405	31.166413
513.509915	31918.092646	31.171431
513.987639	31961.109759	31.176448
514.717554	32018.495885	31.181466
514.867685	32062.476207	31.186484
515.709842	32110.248506	31.191501
516.310035	32170.830928	31.196519
516.729134	32202.647150	31.201536
517.045073	32251.257900	31.206554
517.494446	32303.686868	31.211572
518.010162	32343.492698	31.216589
518.654743	32393.724994	31.221607
519.212062	32442.577159	31.226624
519.315039	32489.292660	31.231642
520.026479	32550.097782	31.236660
520.725459	32588.397071	31.241677
520.687626	32653.334008	31.246695
521.315479	32693.450239	31.251712
521.624885	32749.257987	31.256730
522.202998	32818.079012	31.261748
523.034702	32865.129304	31.266765
523.590047	32925.305190	31.271783
523.815025	32980.231458	31.276800
524.596463	33032.976825	31.281818
525.093370	33101.957543	31.286836
525.955025	33149.997640	31.291853
526.188626	33205.128287	31.296871
526.884199	33258.538585	31.301888
527.289277	33316.118350	31.306906
527.719736	33374.397805	31.311924
528.431800	33424.729137	31.316941
528.574314	33490.182045	31.321959
529.126327	33541.373283	31.326976
529.967743	33604.290566	31.331994
530.055196	33671.823368	31.337012
531.025943	33729.298235	31.342029
531.388840	33793.589203	31.347047
532.027503	33853.511444	31.352064
532.764282	33911.016147	31.357082
533.191450	33962.958224	31.362100
533.652097	34015.800610	31.367117
534.247785	34085.712347	31.372135
535.051970	34128.526044	31.377152
535.604102	34192.998569	31.382170
536.087371	34258.404210	31.387188
537.196042	34300.350586	31.392205
537.648053	34357.345272	31.397223
538.082224	34401.255955	31.402240
538.719330	34450.154066	31.407258
538.871571	34500.407499	31.412276
539.632454	34543.655393	31.417293
540.073210	34602.050754	31.422311
540.453124	34661.371570	31.427328
540.767579	34720.138515	31.432346
541.258944	34778.576569	31.437364
542.024177	34838.427512	31.442381
542.413109	34893.521875	31.447399
542.859857	34955.158496	31.452416
543.571449	35005.510135	31.457434
544.145852	35070.969931	31.462452
544.960625	35127.547259	31.467469
545.263870	35189.088503	31.472487
545.869190	35233.925997	31.477504
546.306416	35296.739379	31.482522
546.452320	35362.681419	31.487540
547.033967	35419.740080	31.492557
547.537860	35492.314046	31.497575
548.365448	35556.354540	31.502592
549.200343	35607.893060	31.507610
549.918016	35674.009885	31.512628
550.289214	35720.679960	31.517645
550.795872	35781.728785	31.522663
551.486899	35838.199427	31.527680
552.341910	35882.141927	31.532698
552.370951	35946.136052	31.537716
552.959265	35988.491251	31.542733
553.576969	36045.940439	31.547751
553.732389	36089.005038	31.552768
554.500203	36139.763997	31.557786
554.985606	36207.145784	31.562804
555.539057	36256.782247	31.567821
556.050535	36312.952692	31.572839
556.750200	36363.404787	31.577856
557.367073	36421.338198	31.582874
557.368109	36481.412586	31.587892
558.275575	36530.962816	31.592909
558.695311	36606.585119	31.597927
559.381754	36659.025473	31.602944
560.215319	36719.540473	31.607962
560.572392	36782.536409	31.612980
561.194698	36837.534966	31.617997
561.416301	36891.432185	31.623015
562.194910	36957.382656	31.628032
562.960218	37004.328548	31.633050
563.125801	37063.023597	31.638068
564.018469	37126.254039	31.643085
564.342315	37190.213243	31.648103
565.114800	37251.557608	31.653120
565.925889	37309.726852	31.658138
566.139541	37377.599842	31.663156
566.590295	37438.070115	31.668173
567.431821	37503.368266	31.673191
567.942552	37558.333813	31.678208
568.641706	37622.589102	31.683226
568.859096	37687.524050	31.688244
569.658955	37741.157660	31.693261
570.093254	37804.194861	31.698279
570.570892	37871.748247	31.703296
571.197313	37934.002881	31.708314
571.849362	38007.307322	31.713332
572.554210	38065.360838	31.718349
573.044347	38139.405958	31.723367
573.589604	38207.312392	31.728384
574.495000	38270.854045	31.733402
574.821891	38328.475372	31.738420
575.384234	38392.405645	31.743437
576.134842	38463.160938	31.748455
576.563261	38529.222403	31.753472
577.598551	38576.149777	31.758490
578.061053	38646.530478	31.763508
578.876637	38702.787407	31.768525
579.325110	38758.139346	31.773543
580.036840	38825.802731	31.778560
580.891992	38879.837742	31.783578
581.015931	38937.554545	31.788596
581.892709	38992.722686	31.793613
582.206446	39042.643166	31.798631
582.451644	39111.679016	31.803648
582.793513	39164.859126	31.808666
583.211883	39241.859414	31.813684
584.054745	39313.423461	31.818701
584.691568	39387.338878	31.823719
584.893250	39455.167901	31.828736
585.633764	39520.025951	31.833754
586.631913	39588.465501	31.838772
586.877396	39661.878571	31.843789
587.433583	39723.052378	31.848807
588.140293	39786.707936	31.853824
588.546742	39854.772874	31.858842
589.106881	39921.480478	31.863860
589.828576	39995.857816	31.868877
590.594611	40066.209524	31.873895
590.691156	40136.189288	31.878912
591.349843	40204.999828	31.883930
591.602636	40266.070959	31.888948
592.491415	40329.688799	31.893965
593.159569	40394.558751	31.898983
593.624052	40468.248169	31.904000
594.304146	40532.302160	31.909018
594.764784	40606.706220	31.914036
595.333102	40665.532431	31.919053
596.225814	40725.621583	31.924071
596.545111	40814.009694	31.929088
597.311788	40878.805066	31.934106
597.734548	40947.297524	31.939124
598.229514	41018.310164	31.944141
599.031459	41090.759213	31.949159
599.880548	41159.096675	31.954176
600.709237	41231.327175	31.959194
601.118359	41301.632157	31.964212
601.902854	41365.046676	31.969229
602.444621	41426.888338	31.974247
603.259386	41502.809605	31.979264
603.734017	41561.651013	31.984282
604.442911	41629.625094	31.989300
604.613482	41697.789523	31.994317
605.627922	41767.955074	31.999335
605.927415	41839.533596	32.004352
606.768639	41906.893264	32.009370
607.111582	41973.082249	32.014388
607.917710	42053.654476	32.019405
608.589014	42122.650022	32.024423
608.876808	42198.213015	32.029440
609.501787	42260.492002	32.034458
609.829298	42333.444312	32.039476
610.665940	42405.861189	32.044493
611.490358	42480.654585	32.049511
611.868650	42567.977312	32.054528
612.353295	42633.112789	32.059546
612.980358	42725.516115	32.064564
613.441861	42802.855604	32.069581
614.424448	42873.081116	32.074599
614.770338	42950.023584	32.079616
615.756647	43026.295251	32.084634
616.414124	43107.338655	32.089652
616.664224	43175.277476	32.094669
617.506016	43256.417323	32.099687
618.047998	43335.927420	32.104704
619.089931	43410.145492	32.109722
619.453190	43485.574918	32.114740
620.113524	43564.712780	32.119757
620.915265	43637.165472	32.124775
621.355547	43716.311968	32.129792
621.992124	43784.444805	32.134810
622.545068	43870.718558	32.139828
623.117186	43945.534310	32.144845
624.132732	44018.685630	32.149863
624.567492	44110.691889	32.154880
625.140005	44169.569536	32.159898
625.939264	44248.860963	32.164916
626.589681	44325.477679	32.169933
627.168582	44400.912996	32.174951
627.525373	44471.301731	32.179968
628.380287	44549.123278	32.184986
629.072189	44625.908020	32.190004
629.616314	44706.074030	32.195021
630.415043	44764.935059	32.200039
630.680154	44846.309823	32.205056
631.568100	44917.768026	32.210074
631.958896	44990.543388	32.215092
632.457341	45067.014599	32.220109
633.532033	45131.565385	32.225127
633.627733	45214.397023	32.230144
634.350805	45268.778795	32.235162
635.103024	45343.772400	32.240180
635.324221	45425.968453	32.245197
636.431843	45495.829443	32.250215
636.979735	45575.925900	32.255232
637.525391	45631.907461	32.260250
637.921839	45714.375756	32.265268
638.358755	45785.747671	32.270285
639.102683	45870.135908	32.275303
639.646488	45961.078459	32.280320
640.539166	46027.045535	32.285338
640.960392	46108.608318	32.290356
641.219867	46204.790523	32.295373
642.252956	46275.693021	32.300391
643.126698	46359.338815	32.305408
643.888313	46439.994084	32.310426
644.584648	46515.446840	32.315444
644.894513	46603.263826	32.320461
645.805290	46675.760689	32.325479
646.447057	46776.328868	32.330496
647.141327	46852.051726	32.335514
647.980997	46931.385626	32.340532
648.627483	47004.347478	32.345549
649.104299	47075.929227	32.350567
649.666947	47164.449102	32.355584
650.466876	47256.195503	32.360602
651.486618	47331.740101	32.365620
651.713582	47422.994712	32.370637
652.528147	47501.059297	32.375655
653.263240	47579.266830	32.380672
653.936066	47657.298661	32.385690
654.566977	47725.746659	32.390708
655.125255	47821.240186	32.395725
656.076036	47891.274905	32.400743
656.416416	47981.360710	32.405760
656.811092	48062.756244	32.410778
657.920867	48149.740583	32.415796
658.302884	48237.846864	32.420813
659.091468	48315.982241	32.425831
659.626926	48405.131368	32.430848
660.324780	48486.551180	32.435866
661.125746	48565.137148	32.440884
661.831294	48658.102860	32.445901
662.224450	48744.703150	32.450919
662.966070	48830.687165	32.455936
663.953503	48911.643981	32.460954
664.540786	48991.874613	32.465972
665.178208	49078.199121	32.470989
665.878326	49155.108184	32.476007
666.144044	49240.468467	32.481024
666.368457	49330.188156	32.486042
667.570690	49429.309992	32.491060
668.099559	49522.729178	32.496077
668.954511	49612.996488	32.501095
669.699682	49695.891721	32.506112
670.183836	49790.210271	32.511130
670.641601	49876.208020	32.516148
671.564440	49978.009878	32.521165
672.488064	50050.476344	32.526183
673.211078	50145.054004	32.531200
673.979286	50219.309246	32.536218
674.363512	50312.933062	32.541236
675.195131	50393.817658	32.546253
676.166596	50475.412234	32.551271
676.988504	50562.066616	32.556288
677.269197	50645.886104	32.561306
678.165668	50721.954019	32.566324
678.275655	50789.921091	32.571341
678.993824	50873.485986	32.576359
679.506304	50955.329085	32.581376
679.991817	51045.079862	32.586394
680.684518	51117.815953	32.591412
680.793837	51213.353192	32.596429
681.919878	51290.674086	32.601447
682.738895	51389.594573	32.606464
683.412977	51487.200256	32.611482
684.038822	51579.829966	32.616500
684.320806	51676.433825	32.621517
685.188357	51764.709608	32.626535
685.656244	51862.319697	32.631552
686.237308	51961.863671	32.636570
687.262499	52054.309534	32.641588
687.880370	52162.086554	32.646605
688.752578	52251.974764	32.651623
689.554571	52350.991396	32.656640
690.108713	52452.475531	32.661658
691.005478	52541.331224	32.666676
691.596777	52645.078276	32.671693
692.723224	52722.543780	32.676711
693.156952	52824.112942	32.681728
693.825574	52920.305185	32.686746
694.571069	53015.215287	32.691764
695.169737	53114.699038	32.696781
696.082376	53209.146491	32.701799
696.862075	53306.484753	32.706816
697.294089	53400.431388	32.711834
698.496590	53490.877172	32.716852
698.627932	53597.870694	32.721869
699.558674	53680.439455	32.726887
700.227833	53780.502498	32.731904
700.878244	53884.657001	32.736922
701.906618	53969.390588	32.741940
702.629341	54071.986162	32.746957
703.397193	54167.327770	32.751975
704.192045	54258.084618	32.756992
704.681923	54358.628855	32.762010
705.695067	54441.837963	32.767028
706.181084	54541.360199	32.772045
706.624673	54634.451503	32.777063
707.676510	54716.972983	32.782080
708.474694	54827.034698	32.787098
709.279239	54905.705706	32.792116
709.518764	55010.723937	32.797133
710.016324	55103.176665	32.802151
711.010262	55197.620200	32.807168
711.813627	55294.098712	32.812186
712.445019	55390.189114	32.817204
713.278153	55493.576266	32.822221
713.866197	55581.593184	32.827239
714.396385	55685.113596	32.832256
715.100982	55793.667026	32.837274
715.936578	55886.465561	32.842292
716.521505	55997.782262	32.847309
717.388076	56097.584247	32.852327
718.132973	56190.380249	32.857344
718.849526	56295.086229	32.862362
719.711402	56385.860689	32.867380
720.158955	56497.013336	32.872397
720.990719	56600.141068	32.877415
721.949323	56689.826675	32.882432
722.212804	56792.347998	32.887450
723.140308	56888.523026	32.892468
724.009044	56989.902577	32.897485
724.415949	57091.618132	32.902503
725.175439	57181.718039	32.907520
725.899419	57269.302850	32.912538
726.652886	57371.101515	32.917556
726.996504	57462.788109	32.922573
727.504642	57558.827198	32.927591
728.611943	57651.620586	32.932608
728.975104	57754.509502	32.937626
730.032780	57850.819282	32.942644
730.975346	57950.649542	32.947661
731.774394	58054.794970	32.952679
732.728978	58156.753933	32.957696
733.003488	58255.400724	32.962714
733.563059	58340.913001	32.967732
734.610277	58448.956508	32.972749
735.374102	58552.731163	32.977767
736.364859	58648.246920	32.982784
736.722478	58759.401695	32.987802
737.467535	58850.023366	32.992820
738.366631	58957.537966	32.997837
738.904319	59061.674956	33.002855
739.415473	59165.052172	33.007872
739.881562	59278.940986	33.012890
741.037789	59378.875691	33.017908
741.638380	59491.580589	33.022925
742.053814	59603.337148	33.027943
743.197080	59706.132239	33.032960
743.899706	59823.644262	33.037978
744.997810	59930.233662	33.042996
745.883188	60046.440089	33.048013
746.460989	60151.776863	33.053031
747.469265	60253.345670	33.058048
747.938016	60361.002109	33.063066
749.238712	60458.187907	33.068084
749.901996	60558.854636	33.073101
750.518667	60674.938459	33.078119
751.279615	60770.875136	33.083136
752.100036	60874.329975	33.088154
752.804167	60984.346185	33.093172
753.704565	61081.866637	33.098189
754.372119	61187.617385	33.103207
754.850257	61293.570669	33.108224
755.685094	61408.181497	33.113242
756.573817	61523.738458	33.118260
757.393706	61633.005823	33.123277
757.658831	61737.789409	33.128295
758.439012	61838.569517	33.133312
759.395547	61950.634985	33.138330
760.307132	62061.836241	33.143348
761.047961	62179.848525	33.148365
761.572129	62285.394790	33.153383
762.688308	62387.360887	33.158400
763.067211	62500.466713	33.163418
764.060304	62610.804140	33.168436
765.010300	62720.188506	33.173453
765.617320	62838.030752	33.178471
766.323966	62941.293608	33.183488
766.781258	63074.092172	33.188506
767.853814	63174.027686	33.193524
768.632903	63281.825110	33.198541
769.163721	63405.188879	33.203559
770.502799	63515.240029	33.208576
771.229604	63625.449940	33.213594
772.096515	63731.781305	33.218612
772.693732	63830.749302	33.223629
773.141521	63946.765754	33.228647
774.323821	64051.118589	33.233664
775.392478	64165.364727	33.238682
775.845127	64259.946370	33.243700
776.965645	64365.581608	33.248717
777.410978	64460.690053	33.253735
778.315369	64545.343113	33.258752
778.878099	64650.503136	33.263770
779.644261	64742.601328	33.268788
780.276942	64847.908816	33.273805
781.054908	64957.188060	33.278823
781.926572	65047.120799	33.283840
782.380637	65152.073750	33.288858
783.029849	65262.444254	33.293876
783.925840	65372.041199	33.298893
784.577449	65486.635412	33.303911
785.233159	65591.658363	33.308928
785.936861	65709.930794	33.313946
786.626422	65828.825776	33.318964
787.642144	65945.132393	33.323981
788.339217	66070.905745	33.328999
789.269278	66175.032775	33.334016
790.011086	66306.192786	33.339034
790.317559	66419.344551	33.344052
791.472210	66536.497588	33.349069
792.100643	66669.290751	33.354087
793.189126	66780.424784	33.359104
793.886277	66909.642398	33.364122
794.853237	67020.987470	33.369140
795.697796	67147.147486	33.374157
796.432764	67273.674111	33.379175
797.346088	67389.468262	33.384192
798.167185	67512.618586	33.389210
798.786343	67636.776684	33.394228
799.699047	67744.088199	33.399245
800.119580	67872.560834	33.404263
801.362624	68010.065856	33.409280
801.901002	68126.646833	33.414298
802.827074	68252.155057	33.419316
803.705996	68365.222552	33.424333
804.690604	68501.793504	33.429351
805.759206	68615.652906	33.434368
806.479224	68739.775487	33.439386
807.083770	68858.752180	33.444404
808.072002	68983.944628	33.449421
808.905182	69104.566745	33.454439
809.623143	69222.224200	33.459456
810.352865	69339.355555	33.464474
811.149882	69471.885476	33.469492
812.170774	69583.816797	33.474509
812.930297	69716.974093	33.479527
814.267669	69823.631495	33.484544
814.744020	69952.455213	33.489562
815.674161	70069.197000	33.494580
816.476383	70188.761749	33.499597
817.240940	70311.924977	33.504615
818.212269	70415.598090	33.509632
818.880236	70536.704563	33.514650
819.498227	70665.970735	33.519668
820.256375	70783.819824	33.524685
821.138908	70913.827823	33.529703
822.150638	71038.623705	33.534720
822.794043	71145.737614	33.539738
823.913850	71279.717646	33.544756
824.828030	71390.790757	33.549773
825.316216	71517.750130	33.554791
826.498409	71638.252882	33.559808
827.099762	71753.230674	33.564826
827.858383	71877.466207	33.569844
828.982499	71994.888281	33.574861
829.286892	72125.422895	33.579879
830.051939	72238.339942	33.584896
830.926794	72355.413127	33.589914
831.801729	72465.328342	33.594932
832.373342	72578.165324	33.599949
833.106085	72706.906165	33.604967
834.192877	72817.692440	33.609984
835.175408	72943.149181	33.615002
835.719610	73051.743441	33.620020
836.510465	73165.799361	33.625037
837.145111	73305.336140	33.630055
837.961266	73428.148106	33.635072
838.757300	73557.433704	33.640090
839.248596	73681.837600	33.645108
840.345119	73811.093969	33.650125
840.918485	73949.190423	33.655143
841.784231	74078.081787	33.660160
842.712739	74220.137143	33.665178
843.441215	74351.260017	33.670196
844.672368	74485.551284	33.675213
845.751476	74627.963837	33.680231
846.527112	74764.039758	33.685248
847.308564	74893.392570	33.690266
848.061851	75030.517386	33.695284
849.364593	75151.038595	33.700301
850.212126	75291.748156	33.705319
850.957202	75413.792415	33.710336
852.054372	75551.167176	33.715354
852.741783	75689.173472	33.720372
853.907514	75803.238021	33.725389
854.791613	75944.635097	33.730407
855.300025	76070.257714	33.735424
856.046382	76207.055763	33.740442
857.079651	76350.505331	33.745460
857.705828	76484.118213	33.750477
858.523538	76624.126455	33.755495
859.663407	76752.463132	33.760512
860.335872	76885.305437	33.765530
861.382518	77032.874847	33.770548
862.568842	77155.557806	33.775565
863.182104	77291.480042	33.780583
864.015447	77421.142646	33.785600
864.883877	77558.346282	33.790618
865.684105	77700.881655	33.795636
866.639996	77825.061239	33.800653
867.725867	77962.275670	33.805671
868.413652	78099.189908	33.810688
869.561327	78227.824755	33.815706
870.180225	78379.117291	33.820724
871.221001	78502.375715	33.825741
871.740219	78646.791673	33.830759
872.847378	78786.082424	33.835776
873.888004	78917.123697	33.840794
874.550200	79056.337901	33.845812
875.746805	79190.188890	33.850829
876.635715	79334.269779	33.855847
877.415323	79464.901954	33.860864
877.871780	79595.854018	33.865882
878.632657	79735.176280	33.870900
879.933913	79863.636930	33.875917
880.579234	80002.195532	33.880935
881.215672	80152.295127	33.885952
882.533232	80295.969641	33.890970
883.198912	80431.408747	33.895988
884.207842	80564.293061	33.901005
885.230842	80702.780824	33.906023
886.275567	80840.557301	33.911040
887.380655	80979.785995	33.916058
887.769267	81117.641035	33.921076
888.980517	81243.239591	33.926093
889.755590	81370.751953	33.931111
890.384656	81493.803757	33.936128
891.068263	81619.915524	33.941146
891.795333	81758.028447	33.946164
892.807923	81879.051358	33.951181
893.532941	82028.294583	33.956199
894.645446	82155.249388	33.961216
895.743889	82298.074391	33.966234
896.269664	82429.334960	33.971252
897.048140	82566.969755	33.976269
897.724597	82698.358779	33.981287
898.662353	82846.325770	33.986304
899.540356	82983.117787	33.991322
900.506121	83138.965236	33.996340
901.211275	83288.251560	34.001357
902.250975	83437.337999	34.006375
903.099651	83584.476651	34.011392
904.029686	83733.943779	34.016410
904.635051	83894.923877	34.021428
905.818613	84033.367231	34.026445
906.985830	84190.820845	34.031463
907.558371	84345.165999	34.036480
908.576894	84495.009358	34.041498
909.217386	84663.512050	34.046516
910.358780	84815.918683	34.051533
911.496437	84969.516475	34.056551
912.279165	85113.170370	34.061568
913.249636	85262.817815	34.066586
914.264848	85429.593627	34.071604
915.299595	85587.287403	34.076621
916.081710	85738.310480	34.081639
916.972880	85889.436719	34.086656
918.147653	86039.903246	34.091674
918.702803	86195.997287	34.096692
919.450846	86361.185048	34.101709
920.780393	86530.947695	34.106727
921.798199	86687.626572	34.111744
922.769795	86835.986671	34.116762
923.362030	87001.286955	34.121780
924.237949	87167.098339	34.126797
925.313884	87329.144292	34.131815
926.045768	87481.218327	34.136832
927.068493	87644.199133	34.141850
928.029278	87808.672084	34.146868
928.749732	87972.318965	34.151885
929.793400	88137.482915	34.156903
930.882602	88304.323798	34.161920
931.831597	88462.506622	34.166938
932.641217	88638.648053	34.171956
933.535928	88803.151472	34.176973
934.523081	88964.432225	34.181991
935.211172	89135.186619	34.187008
936.168859	89288.095539	34.192026
936.934412	89472.559746	34.197044
937.833203	89643.422150	34.202061
938.987561	89806.009933	34.207079
939.545221	89986.152036	34.212096
940.693240	90158.685639	34.217114
941.787848	90340.374412	34.222132
942.855398	90511.158120	34.227149
943.819482	90677.846380	34.232167
944.695768	90850.986826	34.237184
945.618996	91025.918176	34.242202
946.539451	91197.370294	34.247220
947.642307	91359.420130	34.252237
948.698278	91530.187643	34.257255
949.358901	91710.300269	34.262272
950.614549	91873.227010	34.267290
952.031538	92036.242090	34.272308
952.387310	92186.332171	34.277325
953.431376	92340.898098	34.282343
954.511321	92497.199645	34.287360
955.451997	92654.284752	34.292378
956.243688	92815.174181	34.297396
957.185293	92970.229420	34.302413
958.055144	93132.734688	34.307431
958.573265	93302.078159	34.312448
959.736044	93462.252199	34.317466
960.852852	93636.486697	34.322484
961.471031	93803.918190	34.327501
962.767420	93971.618448	34.332519
963.330841	94142.865473	34.337536
964.628969	94310.200624	34.342554
965.414543	94490.211772	34.347572
966.414000	94653.376624	34.352589
967.404887	94824.728595	34.357607
968.520220	95003.372318	34.362624
969.739566	95183.088896	34.367642
970.561744	95358.327456	34.372660
971.625582	95518.873039	34.377677
973.001998	95687.736453	34.382695
973.765408	95856.689728	34.387712
975.444659	96025.739574	34.392730
976.755150	96195.978345	34.397748
977.540732	96338.419941	34.402765
978.344338	96509.491654	34.407783
979.363100	96677.199157	34.412800
980.255010	96839.503554	34.417818
981.124912	97008.396366	34.422836
982.340524	97170.851954	34.427853
983.175846	97327.408072	34.432871
983.721490	97504.885146	34.437888
984.973672	97679.119279	34.442906
986.198686	97847.091701	34.447924
986.654191	98026.530886	34.452941
987.890294	98188.622474	34.457959
988.768794	98362.511622	34.462976
990.145672	98533.160436	34.467994
990.870574	98710.913897	34.473012
992.092008	98877.013471	34.478029
992.748238	99062.181658	34.483047
993.544520	99231.740955	34.488064
994.690208	99403.567117	34.493082
995.847268	99583.502759	34.498100
996.831106	99760.954833	34.503117
997.796860	99930.313481	34.508135
998.635694	100115.509775	34.513152
999.711524	100293.621452	34.518170
1000.803137	100462.741217	34.523188
1001.741175	100651.774455	34.528205
1002.654375	100826.757356	34.533223
1003.770233	101003.094534	34.538240
1005.023487	101183.500378	34.543258
1006.120142	101361.470395	34.548276
1006.632379	101541.621390	34.553293
1008.331722	101708.762026	34.558311
1008.762619	101897.635005	34.563328
1010.057711	102062.805968	34.568346
1011.298041	102238.428180	34.573364
1012.231247	102424.309306	34.578381
1013.191320	102593.458464	34.583399
1014.411084	102767.340056	34.588416
1015.690167	102928.947972	34.593434
1016.244141	103109.558857	34.598452
1017.229377	103287.110946	34.603469
1018.496454	103446.026598	34.608487
1019.664816	103615.217599	34.613504
1020.531645	103768.375832	34.618522
1021.297043	103925.173758	34.623540
1022.115798	104090.107072	34.628557
1023.583784	104256.327169	34.633575
1023.955440	104419.854731	34.638592
1024.978678	104579.184851	34.643610
1026.501373	104744.879738	34.648628
1027.084228	104926.207587	34.653645
1028.109074	105099.889931	34.658663
1029.496851	105268.130749	34.663680
1029.913702	105435.912596	34.668698
1031.067497	105608.956368	34.673716
1031.971081	105792.782833	34.678733
1032.886725	105979.749597	34.683751
1033.821333	106153.542428	34.688768
1035.097932	106333.118672	34.693786
1035.877567	106520.732342	34.698804
1036.554613	106717.572298	34.703821
1038.097000	106893.853270	34.708839
1039.418627	107079.494033	34.713856
1040.427998	107270.824095	34.718874
1041.543711	107448.065894	34.723892
1042.157854	107637.804668	34.728909
1043.441275	107826.395477	34.733927
1044.544627	108014.384065	34.738944
1045.536872	108211.195527	34.743962
1046.478948	108398.250809	34.748980
1047.526903	108599.020517	34.753997
1048.876368	108771.875051	34.759015
1049.789985	108987.173256	34.764032
1050.815786	109173.764049	34.769050
1051.936725	109362.050437	34.774068
1052.834042	109561.028129	34.779085
1054.002354	109744.584507	34.784103
1055.008222	109960.381852	34.789120
1056.376742	110153.294331	34.794138
1057.227011	110338.136025	34.799156
1058.120046	110537.400226	34.804173
1059.435352	110735.379959	34.809191
1060.414354	110939.028534	34.814208
1061.337776	111142.231766	34.819226
1062.439479	111345.356348	34.824244
1063.410254	111550.277597	34.829261
1064.383314	111751.665589	34.834279
1065.428112	111955.095434	34.839296
1066.423280	112165.743239	34.844314
1067.742974	112367.293756	34.849332
1068.358752	112575.347042	34.854349
1069.742076	112778.574931	34.859367
1070.657919	112992.155891	34.864384
1071.770986	113198.218636	34.869402
1073.240574	113417.526255	34.874420
1073.717439	113626.015752	34.879437
1075.057438	113823.202653	34.884455
1076.088149	114041.282814	34.889472
1077.420915	114243.528855	34.894490
1078.589005	114453.063103	34.899508
1079.275327	114663.362719	34.904525
1080.650080	114873.322022	34.909543
1081.614385	115082.704601	34.914560
1082.493546	115298.501010	34.919578
1083.832184	115501.882704	34.924596
1084.673801	115717.891229	34.929613
1085.710880	115931.081680	34.934631
1086.740516	116147.543840	34.939648
1087.888530	116365.723886	34.944666
1089.408400	116567.233384	34.949684
1090.001833	116780.592230	34.954701
1091.091890	116981.896969	34.959719
1092.247997	117176.882270	34.964736
1092.969469	117378.618181	34.969754
1094.342157	117586.773254	34.974772
1095.472579	117800.025545	34.979789
1096.284951	118000.711777	34.984807
1096.931951	118211.626896	34.989824
1098.358111	118438.823788	34.994842
1099.500387	118636.089369	34.999860
1100.507075	118863.016820	35.004877
1101.617803	119071.377948	35.009895
1103.280198	119291.978689	35.014912
1103.955829	119514.581630	35.019930
1104.985049	119715.598662	35.024948
1106.038558	119944.947078	35.029965
1107.229115	120171.246059	35.034983
1108.192235	120388.802734	35.040000
1109.210919	120623.877261	35.045018
1110.599023	120845.802265	35.050036
1111.370770	121077.702518	35.055053
1112.616495	121303.253419	35.060071
1114.032352	121532.744381	35.065088
1114.729844	121769.870705	35.070106
1116.330927	121989.918891	35.075124
1117.401723	122223.121960	35.080141
1118.561371	122441.941184	35.085159
1119.874066	122676.400432	35.090176
1120.571947	122912.585317	35.095194
1122.514067	123128.048576	35.100212
1123.288294	123362.792325	35.105229
1124.297720	123593.456236	35.110247
1125.680494	123812.451353	35.115264
1126.559178	124054.026858	35.120282
1127.743942	124275.732184	35.125300
1128.947231	124519.196798	35.130317
1130.330948	124757.525998	35.135335
1131.346707	124977.147877	35.140352
1132.690811	125209.276968	35.145370
1133.979044	125433.191591	35.150388
1135.124908	125664.761245	35.155405
1135.993495	125890.206130	35.160423
1137.466943	126111.560249	35.165440
1138.504229	126347.576369	35.170458
1139.652370	126565.565445	35.175476
1140.867212	126806.359382	35.180493
1141.732576	127035.057907	35.185511
1142.663215	127270.350919	35.190528
1143.755976	127499.382852	35.195546
1145.445594	127738.990166	35.200564
1146.315677	127978.874250	35.205581
1147.754435	128209.552684	35.210599
1149.115437	128440.942823	35.215616
1150.001884	128677.888909	35.220634
1151.452761	128905.262200	35.225652
1152.194710	129137.989366	35.230669
1153.651308	129368.039617	35.235687
1154.927852	129601.771943	35.240704
1155.952147	129833.443512	35.245722
1157.371215	130053.909345	35.250740
1158.065546	130288.719063	35.255757
1159.103149	130524.411802	35.260775
1160.486615	130755.143406	35.265792
1161.503982	130992.642991	35.270810
1162.585797	131221.957397	35.275828
1163.891759	131456.408411	35.280845
1164.765842	131692.580505	35.285863
1166.147838	131932.042372	35.290880
1166.972131	132156.386073	35.295898
1168.192494	132373.452713	35.300916
1169.409988	132598.330302	35.305933
1169.971542	132827.260466	35.310951
1171.218233	133065.130464	35.315968
1172.151480	133297.260530	35.320986
1173.346250	133534.077665	35.326004
1174.633532	133766.013100	35.331021
1175.808549	134004.307504	35.336039
1177.206538	134253.000460	35.341056
1177.987784	134489.715415	35.346074
1179.298158	134724.278122	35.351092
1180.241063	134981.977015	35.356109
1181.365173	135220.770444	35.361127
1182.885743	135465.395365	35.366144
1183.688242	135725.164451	35.371162
1184.839733	135974.025274	35.376180
1186.269981	136237.688254	35.381197
1187.088290	136488.218166	35.386215
1188.502167	136737.802039	35.391232
1189.643040	137005.221077	35.396250
1191.000378	137262.032376	35.401268
1192.050589	137521.850592	35.406285
1193.438422	137788.905404	35.411303
1194.657276	138047.203681	35.416320
1195.936846	138305.164240	35.421338
1197.124353	138566.616102	35.426356
1198.511846	138828.163714	35.431373
1199.749475	139090.422805	35.436391
1201.010719	139344.362232	35.441408
1202.121136	139612.022496	35.446426
1203.272502	139870.776907	35.451444
1204.642553	140126.745597	35.456461
1205.936569	140400.353869	35.461479
1207.120233	140652.832267	35.466496
1208.230035	140921.580642	35.471514
1209.996078	141180.243284	35.476532
1211.159326	141445.651995	35.481549
1212.093532	141703.149979	35.486567
1213.582617	141966.606741	35.491584
1214.484505	142224.063194	35.496602
1215.873808	142496.530996	35.501620
1217.258790	142754.621609	35.506637
1218.381461	143018.844308	35.511655
1220.009992	143288.374784	35.516672
1220.668548	143543.953626	35.521690
1221.978527	143802.913948	35.526708
1223.440453	144063.296708	35.531725
1224.485079	144330.915327	35.536743
1225.900367	144589.927384	35.541760
1227.243990	144858.020472	35.546778
1228.417311	145127.411885	35.551796
1229.991841	145379.491843	35.556813
1231.063701	145646.697305	35.561831
1232.158226	145909.513058	35.566848
1233.335988	146183.236173	35.571866
1234.547533	146429.866804	35.576884
1236.062809	146694.051777	35.581901
1237.006819	146969.709112	35.586919
1238.242165	147223.189623	35.591936
1239.442363	147481.699957	35.596954
1240.861952	147760.911827	35.601972
1242.444104	148025.171466	35.606989
1243.063086	148281.893797	35.612007
1244.373550	148550.070347	35.617024
1245.398265	148822.899978	35.622042
1246.891784	149086.674546	35.627060
1248.341273	149345.423073	35.632077
1249.208867	149602.138811	35.637095
1250.617349	149845.753864	35.642112
1251.851701	150105.418367	35.647130
1253.068218	150358.809309	35.652148
1254.246305	150609.113530	35.657165
1255.082390	150870.764365	35.662183
1256.768762	151130.602206	35.667200
1257.816018	151390.293802	35.672218
1258.695579	151642.861189	35.677236
1260.496664	151907.733570	35.682253
1261.257914	152181.518990	35.687271
1262.243448	152442.141206	35.692288
1263.398251	152716.524968	35.697306
1264.607253	152995.265135	35.702324
1266.060997	153271.125553	35.707341
1267.115578	153552.343360	35.712359
1268.616787	153832.994679	35.717376
1269.629320	154121.834320	35.722394
1271.096236	154400.618068	35.727412
1272.679885	154681.426773	35.732429
1273.619351	154974.242471	35.737447
1275.158169	155254.136684	35.742464
1276.408338	155548.617779	35.747482
1277.515722	155837.949090	35.752500
1278.779974	156125.899252	35.757517
1280.341591	156427.857804	35.762535
1281.511466	156696.418988	35.767552
1282.576372	157011.073462	35.772570
1284.251287	157294.625694	35.777588
1285.804125	157598.738414	35.782605
1286.460577	157887.258401	35.787623
1288.360442	158171.769120	35.792640
1289.167243	158472.180558	35.797658
1290.486106	158768.843270	35.802676
1291.882287	159066.649808	35.807693
1293.165600	159374.258349	35.812711
1294.518766	159672.964447	35.817728
1295.866694	159972.320592	35.822746
1297.298501	160272.197880	35.827764
1299.023727	160563.135448	35.832781
1300.016747	160865.753766	35.837799
1301.461936	161158.670182	35.842816
1302.670228	161450.079994	35.847834
1303.950736	161752.619149	35.852852
1305.587371	162052.158193	35.857869
1306.933068	162354.576711	35.862887
1307.906707	162642.887118	35.867904
1309.351681	162941.715584	35.872922
1310.595254	163239.843559	35.877940
1312.143086	163536.730689	35.882957
1312.704559	163851.647195	35.887975
1314.297406	164144.128450	35.892992
1316.174847	164460.126045	35.898010
1317.162766	164761.516860	35.903028
1318.674463	165058.014418	35.908045
1320.513836	165358.697675	35.913063
1321.362668	165657.174025	35.918080
1322.890375	165949.157973	35.923098
1324.284499	166249.375336	35.928116
1325.601809	166549.708946	35.933133
1326.541810	166853.697823	35.938151
1328.146788	167139.040737	35.943168
1329.583910	167442.215527	35.948186
1330.818550	167746.047593	35.953204
1332.343011	168033.147892	35.958221
1333.553634	168335.820536	35.963239
1334.958358	168622.792115	35.968256
1336.263148	168915.745933	35.973274
1337.830837	169195.347176	35.978292
1339.081894	169475.383148	35.983309
1340.179215	169756.169540	35.988327
1341.638257	170037.887643	35.993344
1342.857704	170314.786975	35.998362
1344.063357	170599.913124	36.003380
1345.393821	170880.604382	36.008397
1346.423149	171169.227460	36.013415
1347.505472	171462.627642	36.018432
1348.958774	171754.204448	36.023450
1350.289752	172052.262501	36.028468
1351.619277	172349.167882	36.033485
1352.820571	172649.611501	36.038503
1353.993461	172948.043966	36.043520
1355.702908	173255.907376	36.048538
1357.060385	173556.648165	36.053556
1358.456151	173865.747552	36.058573
1360.103345	174168.969703	36.063591
1361.176721	174474.649060	36.068608
1362.594817	174780.501803	36.073626
1363.745045	175095.246245	36.078644
1365.612165	175401.206344	36.083661
1367.049284	175706.503345	36.088679
1368.341659	176020.900273	36.093696
1369.750657	176324.022886	36.098714
1371.089658	176642.845269	36.103732
1372.703339	176946.217058	36.108749
1374.202847	177257.516289	36.113767
1375.519172	177555.331330	36.118784
1376.971428	177869.180452	36.123802
1378.248228	178186.271500	36.128820
1380.208781	178485.038954	36.133837
1381.146126	178803.052989	36.138855
1382.733262	179107.051351	36.143872
1384.165807	179420.189861	36.148890
1385.447194	179733.647172	36.153908
1386.952055	180040.418805	36.158925
1388.612567	180347.306141	36.163943
1389.929660	180662.806597	36.168960
1391.318746	180959.753615	36.173978
1392.433060	181278.388208	36.178996
1394.007989	181582.555368	36.184013
1395.504709	181899.391640	36.189031
1396.526672	182205.265707	36.194048
1398.343919	182522.281178	36.199066
1399.365999	182836.929469	36.204084
1401.316447	183157.391793	36.209101
1402.710486	183469.304116	36.214119
1403.657645	183780.530507	36.219136
1405.418965	184092.106457	36.224154
1406.391462	184411.938134	36.229172
1407.826922	184724.409273	36.234189
1409.765258	185044.275398	36.239207
1410.567443	185366.717480	36.244224
1412.108714	185667.270108	36.249242
1413.347803	186000.978850	36.254260
1414.669985	186317.971138	36.259277
1416.415898	186656.436244	36.264295
1417.553823	186967.420461	36.269312
1418.797356	187288.848578	36.274330
1420.306526	187626.926988	36.279348
1421.716975	187941.793857	36.284365
1423.510576	188271.984217	36.289383
1424.633401	188615.743001	36.294400
1426.376553	188938.087866	36.299418
1427.317457	189272.194964	36.304436
1428.853542	189599.007950	36.309453
1430.598703	189920.558128	36.314471
1431.772567	190228.024816	36.319488
1433.428984	190534.207369	36.324506
1434.597423	190853.547491	36.329524
1435.731248	191158.562830	36.334541
1437.540159	191472.176678	36.339559
1438.789861	191797.195557	36.344576
1440.047669	192097.333037	36.349594
1441.485192	192424.088781	36.354612
1442.754241	192741.911483	36.359629
1444.330513	193072.633931	36.364647
1445.257614	193399.885410	36.369664
1446.898031	193722.958281	36.374682
1447.961164	194069.093803	36.379700
1449.545014	194395.619864	36.384717
1450.618951	194737.034612	36.389735
1452.153561	195091.755998	36.394752
1453.875759	195422.618963	36.399770
1454.782726	195786.068107	36.404788
1456.427292	196134.937106	36.409805
1457.832063	196489.636817	36.414823
1458.863858	196853.731443	36.419840
1460.530015	197209.991499	36.424858
1461.930452	197568.912724	36.429876
1463.318433	197943.111150	36.434893
1464.835041	198313.430814	36.439911
1466.083703	198691.097028	36.444928
1467.941897	199045.303692	36.449946
1469.229292	199425.862287	36.454964
1470.764277	199809.556139	36.459981
1472.503506	200177.144771	36.464999
1473.547067	200566.764324	36.470016
1475.348479	200944.935526	36.475034
1476.697622	201326.141784	36.480052
1478.355299	201699.198646	36.485069
1479.945102	202080.826237	36.490087
1481.405463	202475.516810	36.495104
1483.101887	202840.396447	36.500122
1484.455992	203229.560142	36.505140
1485.759058	203608.208544	36.510157
1487.718548	203984.274485	36.515175
1488.870894	204374.671041	36.520192
1490.932849	204765.147861	36.525210
1491.897312	205144.240879	36.530228
1493.679895	205532.977496	36.535245
1495.013298	205931.122851	36.540263
1496.596485	206312.100167	36.545280
1497.971351	206685.698441	36.550298
1499.636554	207081.674356	36.555316
1500.884807	207470.839050	36.560333
1502.773183	207863.239348	36.565351
1503.862436	208252.675364	36.570368
1505.600317	208637.942780	36.575386
1507.089200	209040.141284	36.580404
1508.732024	209432.043711	36.585421
1510.415816	209818.189041	36.590439
1511.864181	210215.041390	36.595456
1513.404375	210599.969633	36.600474
1514.848635	210994.007335	36.605492
1516.271234	211386.755209	36.610509
1518.215216	211769.564871	36.615527
1519.728547	212168.548828	36.620544
1521.286928	212552.492286	36.625562
1522.403750	212951.138947	36.630580
1523.929541	213337.910223	36.635597
1525.535273	213727.260448	36.640615
1526.582952	214128.158672	36.645632
1528.465691	214514.723584	36.650650
1530.169341	214904.646759	36.655668
1531.427553	215289.946627	36.660685
1533.097386	215676.399138	36.665703
1534.755562	216045.965681	36.670720
1535.972600	216425.562470	36.675738
1537.901378	216803.925636	36.680756
1539.067577	217197.223296	36.685773
1540.276484	217573.600341	36.690791
1541.831762	217961.122175	36.695808
1543.201832	218343.063084	36.700826
1544.495190	218740.206335	36.705844
1546.050093	219142.565393	36.710861
1547.892587	219530.274316	36.715879
1549.077261	219937.904330	36.720896
1550.752498	220333.390446	36.725914
1552.611614	220747.363413	36.730932
1553.563183	221144.191232	36.735949
1555.379876	221544.001633	36.740967
1557.114333	221958.863363	36.745984
1558.635031	222377.038457	36.751002
1560.156589	222791.201865	36.756020
1561.688370	223210.775163	36.761037
1563.413964	223604.562858	36.766055
1564.547807	224069.924132	36.771072
1566.207056	224524.354749	36.776090
1567.691840	224958.013478	36.781108
1569.212604	225390.956614	36.786125
1570.807282	225806.286878	36.791143
1572.391120	226242.092763	36.796160
1573.907984	226665.744548	36.801178
1576.188713	227110.633121	36.806196
1577.270473	227542.411550	36.811213
1578.832103	227976.067940	36.816231
1580.321578	228408.188231	36.821248
1582.095839	228847.578210	36.826266
1583.734512	229280.870441	36.831284
1585.520741	229725.442961	36.836301
1587.314936	230164.859198	36.841319
1588.839803	230601.704986	36.846336
1590.235334	231036.642978	36.851354
1591.896128	231484.137327	36.856372
1593.031855	231932.303980	36.861389
1594.830640	232373.046855	36.866407
1596.370061	232824.502351	36.871424
1598.139503	233269.545398	36.876442
1599.299544	233719.338809	36.881460
1600.910614	234173.681998	36.886477
1602.885084	234618.440808	36.891495
1603.970479	235084.634202	36.896512
1605.919716	235538.086901	36.901530
1607.474893	235996.381389	36.906548
1609.014148	236468.371232	36.911565
1611.007475	236922.353553	36.916583
1612.363269	237393.004344	36.921600
1614.134572	237845.450625	36.926618
1615.612787	238299.673706	36.931636
1617.310315	238766.689631	36.936653
1619.129694	239225.608600	36.941671
1620.545930	239690.386872	36.946688
1622.081353	240155.806910	36.951706
1623.796841	240617.464037	36.956724
1625.760320	241078.903313	36.961741
1627.760247	241533.783659	36.966759
1628.952560	241999.416520	36.971776
1630.544955	242445.576653	36.976794
1632.526448	242914.052930	36.981812
1633.582468	243375.468610	36.986829
1635.502916	243830.747248	36.991847
1637.149889	244286.554467	36.996864
1638.716335	244718.166931	37.001882
1640.427693	245167.156969	37.006900
1642.167115	245608.725419	37.011917
1643.735214	246038.586690	37.016935
1645.081692	246484.615951	37.021952
1646.834485	246924.024731	37.026970
1648.212190	247372.183825	37.031988
1649.665007	247819.670584	37.037005
1651.424271	248268.199572	37.042023
1653.174882	248729.431999	37.047040
1654.390925	249180.083978	37.052058
1656.079521	249632.563585	37.057076
1657.677098	250105.177918	37.062093
1659.702767	250566.163579	37.067111
1661.210338	251044.229941	37.072128
1662.797010	251505.695398	37.077146
1664.754061	251966.896811	37.082164
1666.226611	252444.792294	37.087181
1668.201512	252915.847878	37.092199
1669.909017	253395.864474	37.097216
1671.371819	253865.379444	37.102234
1672.981070	254337.232976	37.107252
1674.579448	254817.420805	37.112269
1676.712354	255296.936267	37.117287
1678.216709	255780.239226	37.122304
1679.808079	256258.828360	37.127322
1681.884209	256738.302868	37.132340
1683.360779	257229.968496	37.137357
1685.308526	257703.951878	37.142375
1686.851011	258186.486958	37.147392
1688.476243	258679.093504	37.152410
1690.405600	259160.980415	37.157428
1691.884379	259650.435700	37.162445
1693.751564	260132.027946	37.167463
1695.480521	260612.169548	37.172480
1697.147529	261118.334232	37.177498
1698.859971	261591.848040	37.182516
1700.409865	262092.849466	37.187533
1702.475697	262581.749708	37.192551
1704.476079	263075.842788	37.197568
1705.816536	263568.622032	37.202586
1708.300991	264050.644265	37.207604
1709.445229	264551.736748	37.212621
1711.284473	265036.278201	37.217639
1712.974371	265521.936288	37.222656
1714.510947	266009.118086	37.227674
1716.860658	266498.807055	37.232692
1718.495989	266992.042983	37.237709
1720.367131	267479.041110	37.242727
1721.647071	267966.136378	37.247744
1723.453446	268463.356147	37.252762
1725.153312	268945.147906	37.257780
1726.894811	269448.981948	37.262797
1728.831623	269938.760650	37.267815
1730.291842	270433.088314	37.272832
1731.898671	270935.265929	37.277850
1733.788555	271433.763425	37.282868
1735.498085	271930.257710	37.287885
1737.488414	272425.053630	37.292903
1739.147069	272920.233742	37.297920
1740.599499	273428.808834	37.302938
1742.471249	273925.704747	37.307956
1743.857550	274428.344681	37.312973
1745.523579	274939.117025	37.317991
1747.084995	275445.510986	37.323008
1749.066527	275952.215528	37.328026
1750.867226	276457.170685	37.333044
1752.515171	276961.667316	37.338061
1753.770822	277450.122607	37.343079
1755.571285	277940.214150	37.348096
1757.077400	278439.345510	37.353114
1759.051007	278930.930247	37.358132
1760.528828	279435.322049	37.363149
1762.199695	279931.602866	37.368167
1763.907621	280440.424772	37.373184
1765.386504	280946.869959	37.378202
1767.574925	281450.275349	37.383220
1769.304664	281973.009498	37.388237
1770.861652	282485.051173	37.393255
1772.844242	283002.761741	37.398272
1774.162756	283523.857171	37.403290
1776.055992	284044.271785	37.408308
1777.679191	284571.409828	37.413325
1779.440495	285092.960447	37.418343
1781.302508	285634.229266	37.423360
1783.209448	286167.182617	37.428378
1785.292848	286699.088869	37.433396
1786.716628	287236.995096	37.438413
1788.686479	287774.783698	37.443431
1790.543969	288310.810752	37.448448
1792.326859	288859.751467	37.453466
1794.017448	289397.884643	37.458484
1795.764349	289944.667817	37.463501
1797.753174	290488.944922	37.468519
1799.845300	291035.488654	37.473536
1801.685381	291582.909838	37.478554
1803.677214	292136.501088	37.483572
1805.422407	292686.473001	37.488589
1807.013352	293235.477281	37.493607
1809.176121	293780.422243	37.498624
1810.933059	294331.806906	37.503642
1812.673767	294874.505060	37.508660
1814.114473	295438.051992	37.513677
1816.239566	295993.812540	37.518695
1818.622153	296547.368829	37.523712
1820.518223	297107.326897	37.528730
1822.430954	297654.046607	37.533748
1824.250391	298211.420804	37.538765
1825.893473	298761.252424	37.543783
1827.830056	299312.581882	37.548800
1829.544521	299871.259617	37.553818
1831.564685	300427.851878	37.558836
1833.216155	300991.587818	37.563853
1835.221948	301539.744027	37.568871
1837.251048	302095.258475	37.573888
1838.982597	302652.596586	37.578906
1841.194044	303206.042518	37.583924
1843.082961	303763.982838	37.588941
1844.541901	304320.847870	37.593959
1846.846931	304870.737995	37.598976
1848.869116	305425.496736	37.603994
1850.628733	305977.273148	37.609012
1852.229166	306533.516642	37.614029
1853.933827	307086.031474	37.619047
1856.150128	307639.550200	37.624064
1857.764857	308203.856164	37.629082
1859.523721	308765.925046	37.634100
1861.549553	309321.520944	37.639117
1862.960293	309881.836501	37.644135
1864.750065	310434.517823	37.649152
1866.481538	311013.615442	37.654170
1868.448623	311579.769402	37.659188
1870.339881	312151.975586	37.664205
1872.092722	312718.054938	37.669223
1874.096702	313289.548275	37.674240
1875.645241	313849.659844	37.679258
1877.892587	314398.021484	37.684276
1879.952530	314946.333780	37.689293
1881.162894	315499.860876	37.694311
1883.369707	316028.613286	37.699328
1884.776217	316588.727128	37.704346
1886.723511	317141.764228	37.709364
1888.571131	317699.409431	37.714381
1890.053268	318259.929025	37.719399
1892.399533	318824.567178	37.724416
1893.926505	319398.476975	37.729434
1895.734324	319969.872500	37.734452
1897.556392	320529.149078	37.739469
1899.378580	321113.151867	37.744487
1901.238269	321700.951875	37.749504
1902.931422	322292.557251	37.754522
1904.774066	322876.236048	37.759540
1906.733371	323469.893956	37.764557
1908.949229	324080.083539	37.769575
1910.898213	324667.105014	37.774592
1912.793412	325276.167856	37.779610
1914.641554	325865.758872	37.784628
1917.048016	326470.891563	37.789645
1918.387362	327076.803712	37.794663
1920.633503	327684.260978	37.799680
1922.522453	328285.880919	37.804698
1924.426092	328894.270828	37.809716
1926.572207	329509.646698	37.814733
1928.437227	330121.736656	37.819751
1930.493986	330728.888667	37.824768
1932.226600	331343.018293	37.829786
1934.265206	331953.054201	37.834804
1936.587794	332560.675595	37.839821
1937.821127	333193.221511	37.844839
1940.355859	333808.359089	37.849856
1942.645888	334424.393198	37.854874
1944.622582	335041.842789	37.859892
1946.547588	335655.892201	37.864909
1948.452562	336283.163136	37.869927
1950.539598	336899.633600	37.874944
1952.655180	337517.818159	37.879962
1954.631692	338132.794565	37.884980
1956.668139	338741.839384	37.889997
1958.453253	339363.660686	37.895015
1960.761292	339982.519735	37.900032
1962.547734	340599.553589	37.905050
1964.449103	341226.561341	37.910068
1966.873353	341840.428570	37.915085
1968.949367	342462.112321	37.920103
1971.178033	343079.575033	37.925120
1972.895596	343699.093939	37.930138
1974.669677	344315.600609	37.935156
1977.015409	344921.573666	37.940173
1978.608251	345546.545826	37.945191
1980.785643	346159.078723	37.950208
1982.738991	346777.426991	37.955226
1984.853934	347403.303178	37.960244
1986.883929	348008.729845	37.965261
1989.126812	348625.761861	37.970279
1991.212734	349238.218013	37.975296
1992.895398	349861.467044	37.980314
1994.701738	350481.387942	37.985332
1997.168750	351093.045171	37.990349
1998.823279	351713.633648	37.995367
2000.798685	352320.837959	38.000384
2002.963321	352951.804867	38.005402
2004.923248	353562.673794	38.010420
2006.741163	354184.392544	38.015437
2008.458339	354805.078505	38.020455
2010.691576	355390.501601	38.025472
2012.516688	355993.415737	38.030490
2014.212135	356590.354464	38.035508
2016.428831	357195.622410	38.040525
2018.348918	357796.338007	38.045543
2020.090812	358396.998122	38.050560
2021.863381	359010.913854	38.055578
2023.768018	359630.887661	38.060596
2025.645188	360234.517446	38.065613
2027.184328	360872.875787	38.070631
2029.175886	361497.779024	38.075648
2031.279152	362138.992198	38.080666
2032.988398	362787.617138	38.085684
2035.027231	363423.644559	38.090701
2036.803979	364081.978547	38.095719
2038.767284	364734.588021	38.100736
2040.885336	365403.218668	38.105754
2042.906410	366061.503717	38.110772
2045.302880	366732.069038	38.115789
2046.831272	367413.115258	38.120807
2049.265281	368078.957524	38.125824
2051.156680	368753.222719	38.130842
2053.071713	369436.222663	38.135860
2055.315303	370119.916598	38.140877
2057.123035	370810.340454	38.145895
2059.311525	371500.003488	38.150912
2061.103828	372186.700526	38.155930
2063.272926	372894.068849	38.160948
2065.689777	373581.371480	38.165965
2067.365327	374289.807967	38.170983
2069.766255	374989.005780	38.176000
2071.806924	375695.451508	38.181018
2073.910841	376405.017088	38.186036
2076.037532	377110.633596	38.191053
2078.104528	377819.592856	38.196071
2080.394014	378541.509584	38.201088
2082.325052	379254.087670	38.206106
2084.400126	379979.939581	38.211124
2086.541335	380700.389193	38.216141
2088.476254	381428.540258	38.221159
2090.568951	382147.216913	38.226176
2093.034566	382865.486696	38.231194
2094.938103	383606.475234	38.236212
2096.864458	384330.531953	38.241229
2098.750638	385068.853132	38.246247
2100.985245	385796.679783	38.251264
2103.004514	386526.198671	38.256282
2104.940793	387281.421212	38.261300
2107.481484	388025.599574	38.266317
2109.322496	388777.962645	38.271335
2111.392106	389510.116647	38.276352
2113.536857	390262.469765	38.281370
2115.232371	391027.324935	38.286388
2117.467117	391773.390493	38.291405
2119.526503	392532.546058	38.296423
2121.917208	393289.042562	38.301440
2124.346823	394038.720898	38.306458
2126.032917	394799.275111	38.311476
2128.537598	395567.734484	38.316493
2130.272543	396335.819484	38.321511
2132.488650	397102.461849	38.326528
2135.007606	397855.298321	38.331546
2136.937151	398626.585811	38.336564
2139.146902	399381.562586	38.341581
2141.245377	400149.943329	38.346599
2143.324766	400914.759018	38.351616
2146.038716	401678.714613	38.356634
2147.649110	402438.980314	38.361652
2149.745549	403170.538472	38.366669
2151.917272	403910.730598	38.371687
2153.882131	404643.538899	38.376704
2156.448191	405377.242092	38.381722
2158.115009	406119.739025	38.386740
2160.117665	406857.118857	38.391757
2162.273628	407608.463325	38.396775
2164.243288	408353.307128	38.401792
2166.542703	409110.438422	38.406810
2168.460265	409866.572882	38.411828
2170.825962	410622.637394	38.416845
2172.865107	411390.563795	38.421863
2174.778035	412160.008625	38.426880
2176.748463	412929.674856	38.431898
2178.623102	413723.472313	38.436916
2180.881926	414500.516708	38.441933
2183.151115	415285.336861	38.446951
2185.293320	416080.588529	38.451968
2187.677611	416882.537538	38.456986
2189.448882	417677.345168	38.462004
2191.895816	418480.044108	38.467021
2194.101078	419297.419488	38.472039
2196.219205	420097.057343	38.477056
2198.449102	420908.805489	38.482074
2200.423537	421741.154925	38.487092
2202.966872	422555.456337	38.492109
2205.428051	423381.720255	38.497127
2207.230437	424199.254549	38.502144
2209.332342	425029.876960	38.507162
2211.239517	425858.680428	38.512180
2213.828885	426694.684383	38.517197
2216.177845	427542.191768	38.522215
2218.417267	428382.953905	38.527232
2220.911958	429214.886129	38.532250
2222.829965	430070.373670	38.537268
2224.928990	430910.057055	38.542285
2227.209944	431769.725853	38.547303
2229.509044	432610.530210	38.552320
2231.726099	433461.238494	38.557338
2233.961502	434331.145898	38.562356
2236.295554	435178.886626	38.567373
2238.958605	436039.194318	38.572391
2240.788108	436909.981897	38.577408
2243.634887	437760.123142	38.582426
2245.516346	438619.601779	38.587444
2247.866443	439486.510023	38.592461
2250.263500	440351.251705	38.597479
2252.452461	441216.904936	38.602496
2255.019758	442073.101510	38.607514
2256.915681	442945.768377	38.612532
2259.513130	443810.797038	38.617549
2261.502419	444684.239302	38.622567
2263.812134	445556.885355	38.627584
2266.079457	446421.105824	38.632602
2268.302495	447293.341886	38.637620
2270.860187	448172.265291	38.642637
2273.098379	449046.400072	38.647655
2275.138903	449907.937470	38.652672
2277.626970	450776.851192	38.657690
2279.733756	451658.030925	38.662708
2282.067908	452526.745890	38.667725
2284.571521	453413.450173	38.672743
2286.683997	454286.679509	38.677760
2289.337433	455159.630950	38.682778
2291.620373	456040.191004	38.687796
2293.826097	456910.360840	38.692813
2296.548134	457772.622180	38.697831
2298.087592	458647.832978	38.702848
2300.869355	459486.097966	38.707866
2303.029435	460338.635947	38.712884
2305.020068	461177.618017	38.717901
2307.348161	462021.816686	38.722919
2309.783957	462864.546380	38.727936
2311.852893	463703.307699	38.732954
2314.129955	464568.280795	38.737972
2316.085382	465423.464085	38.742989
2318.341998	466296.501034	38.748007
2320.396911	467158.515363	38.753024
2322.914121	468032.593458	38.758042
2325.241959	468908.330666	38.763060
2327.733141	469778.341764	38.768077
2329.973710	470656.135620	38.773095
2332.160175	471545.316268	38.778112
2334.541623	472428.613047	38.783130
2336.685105	473317.161708	38.788148
2338.868296	474217.634209	38.793165
2341.463434	475140.019512	38.798183
2343.546975	476038.652598	38.803200
2346.297324	476953.193994	38.808218
2348.323333	477866.849995	38.813236
2350.770619	478779.583002	38.818253
2352.804061	479686.783617	38.823271
2355.323896	480611.735478	38.828288
2357.883687	481538.804950	38.833306
2359.755207	482478.159952	38.838324
2362.318018	483405.890343	38.843341
2364.958520	484343.657587	38.848359
2366.660533	485290.819813	38.853376
2369.483720	486236.232031	38.858394
2371.751271	487189.711798	38.863412
2374.092188	488132.527520	38.868429
2376.640004	489083.839166	38.873447
2379.005638	490044.415942	38.878464
2381.459282	491000.938046	38.883482
2383.643351	491959.066727	38.888500
2386.383486	492929.010328	38.893517
2388.808624	493874.931682	38.898535
2391.170054	494849.118247	38.903552
2393.497949	495814.828574	38.908570
2396.065355	496780.343461	38.913588
2398.441876	497751.131820	38.918605
2401.166379	498716.711593	38.923623
2403.296419	499694.742901	38.928640
2406.025887	500663.639480	38.933658
2408.116205	501635.913870	38.938676
2410.630800	502616.483678	38.943693
2412.979987	503594.349499	38.948711
2415.506575	504567.337001	38.953728
2417.972052	505553.488144	38.958746
2420.338463	506541.310201	38.963764
2422.833384	507519.723186	38.968781
2425.607419	508504.584903	38.973799
2427.841317	509497.339845	38.978816
2430.433379	510474.246086	38.983834
2433.146240	511454.500181	38.988852
2435.093310	512447.017856	38.993869
2437.523221	513422.307646	38.998887
2440.083591	514416.969011	39.003904
2442.182885	515401.816422	39.008922
2444.794769	516393.975066	39.013940
2447.431849	517386.066260	39.018957
2449.714898	518376.338479	39.023975
2451.987423	519375.667960	39.028992
2454.575174	520369.439592	39.034010
2457.094271	521356.961902	39.039028
2459.715795	522343.093689	39.044045
2462.415436	523304.316842	39.049063
2464.874758	524265.820775	39.054080
2467.071350	525207.010745	39.059098
2469.338184	526159.964537	39.064116
2471.884059	527112.559822	39.069133
2474.138705	528075.867398	39.074151
2476.207634	529049.565455	39.079168
2478.903659	530015.040616	39.084186
2480.920446	530996.825303	39.089204
2483.506197	531966.570414	39.094221
2486.210167	532955.208403	39.099239
2488.795522	533948.379167	39.104256
2490.991978	534931.882995	39.109274
2493.255882	535930.758814	39.114292
2495.906504	536933.225446	39.119309
2498.306041	537930.027840	39.124327
2500.572631	538954.506301	39.129344
2502.860364	539962.556436	39.134362
2505.217848	540990.596314	39.139380
2507.811704	542011.328988	39.144397
2510.290079	543042.821374	39.149415
2512.649784	544084.719267	39.154432
2514.944111	545131.378447	39.159450
2517.462115	546181.241174	39.164468
2519.829814	547254.633076	39.169485
2522.683995	548306.190099	39.174503
2525.439942	549362.610225	39.179520
2527.980816	550441.456792	39.184538
2530.438827	551511.082785	39.189556
2532.820136	552582.547487	39.194573
2535.279672	553659.895771	39.199591
2538.265898	554742.800617	39.204608
2540.569744	555825.831397	39.209626
2543.047796	556922.162565	39.214644
2545.491199	558006.149572	39.219661
2548.099867	559093.035466	39.224679
2550.817484	560203.074027	39.229696
2553.235073	561290.313248	39.234714
2556.145522	562386.372222	39.239732
2558.298056	563499.239509	39.244749
2560.989862	564599.518555	39.249767
2563.660304	565708.294934	39.254784
2566.021584	566827.822891	39.259802
2569.466951	567927.242996	39.264820
2571.558087	569050.940074	39.269837
2574.543362	570148.137208	39.274855
2577.148308	571268.191273	39.279872
2579.975226	572380.430971	39.284890
2582.385959	573492.741987	39.289908
2585.019356	574601.857151	39.294925
2587.722187	575713.070738	39.299943
2590.066348	576832.723941	39.304960
2593.125496	577939.014809	39.309978
2595.692762	579056.374365	39.314996
2597.696974	580173.073917	39.320013
2600.638475	581285.906694	39.325031
2603.004860	582417.639899	39.330048
2605.825209	583541.571633	39.335066
2608.544363	584657.444240	39.340084
2610.951522	585789.359378	39.345101
2613.963639	586910.691867	39.350119
2616.472012	588040.875576	39.355136
2618.695830	589157.316849	39.360154
2621.772941	590279.928279	39.365172
2624.330520	591399.312657	39.370189
2626.746620	592531.141855	39.375207
2629.444292	593651.292949	39.380224
2632.044465	594760.182069	39.385242
2635.142107	595853.005117	39.390260
2637.626707	596950.886376	39.395277
2640.351759	598031.546265	39.400295
2642.977066	599101.255150	39.405312
2645.533133	600187.501627	39.410330
2648.335709	601264.542806	39.415348
2650.841152	602351.194953	39.420365
2653.371224	603431.232423	39.425383
2656.239700	604532.485973	39.430400
2658.567579	605618.006480	39.435418
2661.375687	606731.520073	39.440436
2663.461023	607831.782634	39.445453
2666.371481	608925.047065	39.450471
2668.900886	610035.929243	39.455488
2671.646961	611160.673069	39.460506
2674.130832	612278.494117	39.465524
2676.710857	613408.541195	39.470541
2679.226439	614535.683316	39.475559
2681.754352	615681.010809	39.480576
2684.117165	616819.396530	39.485594
2686.994112	617978.127726	39.490612
2689.322421	619138.326563	39.495629
2692.253191	620297.702929	39.500647
2694.761869	621467.421096	39.505664
2697.370734	622648.140758	39.510682
2700.296988	623825.031338	39.515700
2702.452577	625011.363404	39.520717
2705.411276	626199.580023	39.525735
2708.177957	627403.630910	39.530752
2710.823404	628609.613517	39.535770
2713.556035	629812.448326	39.540788
2716.043301	631018.882029	39.545805
2718.713684	632227.394288	39.550823
2721.299323	633451.906735	39.555840
2724.077856	634677.641828	39.560858
2727.314811	635905.602948	39.565876
2729.534139	637138.327867	39.570893
2732.209740	638374.423617	39.575911
2735.361196	639617.327855	39.580928
2738.015214	640865.252456	39.585946
2740.791870	642095.895522	39.590964
2743.544360	643354.174917	39.595981
2746.390075	644599.865914	39.600999
2749.367036	645850.917049	39.606016
2751.701568	647113.884910	39.611034
2754.735228	648363.219098	39.616052
2757.050155	649630.609792	39.621069
2760.185637	650895.312299	39.626087
2763.318750	652145.403440	39.631104
2765.989553	653409.414388	39.636122
2768.910882	654675.464403	39.641140
2771.517986	655932.088699	39.646157
2774.148635	657199.505795	39.651175
2777.357872	658475.079585	39.656192
2779.820822	659744.634494	39.661210
2782.621617	661004.110153	39.666228
2785.435405	662277.408237	39.671245
2788.216505	663547.308529	39.676263
2791.149679	664827.069125	39.681280
2794.034901	666102.238169	39.686298
2796.940251	667364.695780	39.691316
2799.528794	668656.090671	39.696333
2802.541728	669924.906440	39.701351
2805.170041	671196.947608	39.706368
2807.767975	672471.159330	39.711386
2810.817307	673755.863386	39.716404
2813.562869	675038.204161	39.721421
2816.452283	676296.187573	39.726439
2819.090784	677554.091908	39.731456
2821.707236	678784.994812	39.736474
2824.930047	680023.782365	39.741492
2827.612740	681263.684663	39.746509
2830.235665	682503.727387	39.751527
2833.142578	683740.525572	39.756544
2835.693787	684982.031692	39.761562
2839.020666	686210.678148	39.766580
2841.760535	687466.808466	39.771597
2844.592131	688720.813045	39.776615
2847.604507	689975.506536	39.781632
2849.872044	691237.343108	39.786650
2852.801035	692495.121635	39.791668
2855.078313	693762.157131	39.796685
2858.081691	695037.870642	39.801703
2861.136833	696329.858092	39.806720
2863.680750	697623.922729	39.811738
2866.458537	698917.758531	39.816756
2869.647957	700210.740715	39.821773
2872.103640	701512.872246	39.826791
2875.161046	702822.590072	39.831808
2878.152103	704147.928631	39.836826
2880.658317	705460.757967	39.841844
2883.194434	706791.166592	39.846861
2886.107260	708126.309797	39.851879
2889.352909	709456.931245	39.856896
2892.100841	710816.739902	39.861914
2895.157993	712154.250101	39.866932
2897.956634	713502.679760	39.871949
2901.080052	714859.947138	39.876967
2904.315266	716216.086834	39.881984
2906.984166	717579.175833	39.887002
2910.039251	718930.305171	39.892020
2913.133767	720300.201278	39.897037
2915.942600	721659.336500	39.902055
2919.363605	723018.790696	39.907072
2921.786864	724392.323816	39.912090
2924.976176	725761.250937	39.917108
2928.248566	727137.694555	39.922125
2930.788792	728502.465539	39.927143
2933.801366	729872.364301	39.932160
2936.439336	731267.629768	39.937178
2939.578725	732643.164349	39.942196
2942.653008	734028.350358	39.947213
2945.294310	735425.217327	39.952231
2948.690834	736812.980046	39.957248
2951.553287	738202.267726	39.962266
2953.986607	739586.153716	39.967284
2956.907662	741000.501543	39.972301
2960.240839	742404.713258	39.977319
2963.132953	743804.703861	39.982336
2966.038912	745218.248529	39.987354
2969.316096	746621.962647	39.992372
2972.171976	748034.661493	39.997389
2975.278898	749442.824540	40.002407
2978.068663	750847.138272	40.007424
2980.911412	752257.986296	40.012442
2984.125002	753674.572943	40.017460
2987.334202	755087.550539	40.022477
2990.214951	756507.263517	40.027495
2993.080700	757923.023000	40.032512
2996.047940	759342.636370	40.037530
2999.092636	760753.163208	40.042548
3002.280509	762166.600990	40.047565
3004.911994	763597.376187	40.052583
3008.097381	765008.165178	40.057600
3010.873234	766443.881230	40.062618
3013.829799	767850.975117	40.067636
3016.931913	769234.825368	40.072653
3019.718584	770619.402937	40.077671
3022.560475	771991.232337	40.082688
3025.722121	773389.673031	40.087706
3028.851869	774768.354466	40.092724
3031.927809	776151.695544	40.097741
3034.644174	777543.130738	40.102759
3037.795485	778935.307974	40.107776
3040.825720	780335.139171	40.112794
3043.653724	781736.597175	40.117812
3046.878151	783138.894658	40.122829
3049.418391	784545.935946	40.127847
3052.267259	785965.007477	40.132864
3055.440748	787392.372351	40.137882
3058.213473	788829.565705	40.142900
3061.452486	790260.412028	40.147917
3064.050833	791704.695934	40.152935
3067.692445	793145.768614	40.157952
3070.332297	794605.861249	40.162970
3073.221553	796069.819641	40.167988
3076.273780	797540.591978	40.173005
3079.558850	799019.727653	40.178023
3082.683710	800497.693460	40.183040
3085.635552	801980.068760	40.188058
3088.434603	803478.439247	40.193076
3091.746771	804976.838490	40.198093
3094.815761	806479.350363	40.203111
3097.938122	807989.197316	40.208128
3101.242889	809513.682852	40.213146
3104.040365	811034.049213	40.218164
3107.422408	812547.187034	40.223181
3110.261666	814081.514799	40.228199
3113.760272	815605.861828	40.233216
3116.346385	817151.979564	40.238234
3119.655104	818688.834880	40.243252
3122.975105	820224.015616	40.248269
3126.032812	821783.421613	40.253287
3129.118464	823321.093064	40.258304
3132.354393	824880.858817	40.263322
3135.661156	826433.563618	40.268340
3138.636526	827994.385796	40.273357
3141.808284	829561.087366	40.278375
3145.154079	831124.313524	40.283392
3148.161818	832693.695271	40.288410
3151.064412	834259.304501	40.293428
3154.559194	835842.348391	40.298445
3157.466098	837421.837729	40.303463
3160.682113	838993.490446	40.308480
3163.853503	840584.121930	40.313498
3167.021952	842168.617144	40.318516
3170.377529	843757.157485	40.323533
3173.380004	845351.480059	40.328551
3176.745550	846947.962404	40.333568
3180.387105	848527.669626	40.338586
3183.652026	850121.803785	40.343604
3186.699508	851702.455638	40.348621
3189.829218	853298.807375	40.353639
3193.367001	854897.494486	40.358656
3196.203785	856482.976796	40.363674
3199.286702	858088.187405	40.368692
3202.660803	859677.411742	40.373709
3205.804542	861282.452360	40.378727
3209.084187	862874.251909	40.383744
3212.063686	864485.452233	40.388762
3215.296964	866085.330457	40.393780
3218.568573	867697.853036	40.398797
3221.256001	869302.776599	40.403815
3224.615322	870900.092394	40.408832
3227.621651	872484.941382	40.413850
3230.984617	874046.765827	40.418868
3234.345618	875609.436534	40.423885
3237.207351	877186.378217	40.428903
3240.447834	878759.838396	40.433920
3243.758592	880334.315101	40.438938
3246.290276	881918.835409	40.443956
3249.772453	883493.785277	40.448973
3252.721853	885091.090664	40.453991
3255.600285	886697.139418	40.459008
3258.311476	888314.641066	40.464026
3261.547354	889951.961467	40.469044
3264.915268	891584.259532	40.474061
3267.852414	893220.599057	40.479079
3270.670290	894881.265413	40.484096
3273.998052	896543.579494	40.489114
3276.977346	898215.676523	40.494132
3280.048553	899895.065506	40.499149
3282.974205	901597.280246	40.504167
3286.369807	903295.339515	40.509184
3289.869814	905017.597938	40.514202
3292.534479	906735.228930	40.519220
3296.169979	908468.903079	40.524237
3299.226571	910224.627145	40.529255
3302.501857	911967.742511	40.534272
3305.720265	913734.046816	40.539290
3308.904502	915479.040553	40.544308
3312.522958	917249.426521	40.549325
3315.893871	919033.771572	40.554343
3318.953157	920803.187491	40.559360
3322.169073	922588.977116	40.564378
3325.181078	924394.825267	40.569396
3329.110287	926185.056419	40.574413
3332.176565	928001.087499	40.579431
3335.690737	929801.386239	40.584448
3339.033850	931619.489489	40.589466
3342.216044	933450.109787	40.594484
3345.729388	935268.748075	40.599501
3349.238751	937098.141727	40.604519
3352.387669	938928.199051	40.609536
3356.091335	940760.104476	40.614554
3359.073895	942597.695082	40.619572
3362.645034	944431.480392	40.624589
3366.136149	946277.615060	40.629607
3369.677362	948114.106083	40.634624
3373.037329	949951.877926	40.639642
3376.172498	951800.568397	40.644660
3379.856900	953666.435174	40.649677
3383.492520	955573.505695	40.654695
3386.618569	957463.505128	40.659712
3390.659258	959358.306195	40.664730
3393.497547	961261.281323	40.669748
3397.169111	963152.354195	40.674765
3400.672767	965060.605714	40.679783
3403.835105	966947.193991	40.684800
3407.511429	968838.737873	40.689818
3410.847749	970756.444307	40.694836
3414.649649	972645.345909	40.699853
3417.633457	974556.182146	40.704871
3420.864941	976450.161492	40.709888
3424.601135	978349.568099	40.714906
3427.848896	980258.942048	40.719924
3431.635533	982160.773188	40.724941
3435.069087	984069.425103	40.729959
3438.575332	985970.712210	40.734976
3442.172358	987873.391814	40.739994
3445.438898	989777.920062	40.745012
3448.881325	991651.395475	40.750016
3452.233372	993494.827755	40.755021
3455.537719	995265.020018	40.760026
3458.903901	996977.599086	40.765031
3462.042744	998622.250236	40.770036
3465.069522	1000190.548061	40.775040
3467.769314	1001688.330232	40.780045
3470.919650	1003103.951578	40.785050
3474.058134	1004443.577739	40.790055
3476.456635	1005705.341181	40.795060
3479.090024	1006902.350506	40.800064
3481.962407	1008024.152195	40.805069
3484.411390	1009070.511510	40.810074
3486.775793	1010031.118722	40.815079
3489.039802	1010935.154852	40.820084
3490.982878	1011772.099452	40.825088
3493.285821	1012539.831419	40.830093
3494.961148	1013252.326405	40.835098
3497.017459	1013898.568084	40.840103
3498.459505	1014484.663520	40.845108
3500.567029	1015009.935482	40.850112
3502.166229	1015482.454348	40.855117
3503.478907	1015918.982956	40.860122
3505.166619	1016287.500340	40.865127
3506.576686	1016627.807424	40.870132
3507.875357	1016903.308537	40.875136
3509.295849	1017149.770789	40.880141
3510.477172	1017337.477167	40.885146
3511.485044	1017493.292321	40.890151
3512.432697	1017612.932268	40.895156
3513.544745	1017699.466267	40.900160
3514.207073	1017752.512038	40.905165
3515.054056	1017780.307760	40.910170
3516.159935	1017774.596844	40.915175
3516.948502	1017740.614991	40.920180
3517.931559	1017674.979417	40.925184
3518.341989	1017584.314414	40.930189
3519.220412	1017469.417348	40.935194
3519.905189	1017330.007721	40.940199
3520.162571	1017165.734187	40.945204
3520.622844	1016986.482813	40.950208
3521.646236	1016792.774908	40.955213
3521.956006	1016576.572831	40.960218
3522.282219	1016338.723912	40.965223
3522.620142	1016089.996083	40.970228
3523.074781	1015832.699335	40.975232
3523.332722	1015561.062019	40.980237
3523.661193	1015266.207368	40.985242
3524.408613	1014966.221861	40.990247
3524.502443	1014670.404149	40.995252
3524.615927	1014334.677596	41.000256
3524.786708	1013998.727422	41.005261
3525.317617	1013652.991032	41.010266
3526.080734	1013299.817492	41.015271
3526.071429	1012948.205238	41.020276
3526.559085	1012560.178698	41.025280
3526.644735	1012181.998079	41.030285
3526.626842	1011780.990529	41.035290
3527.009628	1011372.799539	41.040295
3527.271207	1010965.278715	41.045300
3527.104602	1010564.791675	41.050304
3527.231350	1010138.391605	41.055309
3527.452767	1009731.273707	41.060314
3527.809147	1009301.664102	41.065319
3527.884174	1008860.507147	41.070324
3527.955780	1008416.692929	41.075328
3528.294730	1007971.342216	41.080333
3528.170781	1007530.405398	41.085338
3528.439102	1007077.707681	41.090343
3528.221069	1006615.626367	41.095348
3528.633632	1006161.665075	41.100352
3528.694247	1005701.504101	41.105357
3528.719801	1005242.186288	41.110362
3528.680624	1004764.953035	41.115367
3528.364079	1004296.281325	41.120372
3528.740376	1003812.968133	41.125376
3528.885329	1003346.572497	41.130381
3528.722261	1002867.546073	41.135386
3529.133003	1002381.381595	41.140391
3528.909136	1001895.474387	41.145396
3528.820773	1001398.996906	41.150400
3528.986881	1000918.194513	41.155405
3528.549114	1000432.585925	41.160410
3528.745266	999936.322307	41.165415
3528.811336	999463.002425	41.170420
3528.845705	998966.485766	41.175424
3528.773415	998484.542560	41.180429
3528.773069	997990.963254	41.185434
3529.086522	997491.448427	41.190439
3528.681690	996999.406871	41.195444
3528.878680	996500.894779	41.200448
3528.613669	995995.988373	41.205453
3528.422218	995502.807938	41.210458
3528.778549	995005.306600	41.215463
3528.699120	994519.813328	41.220468
3528.692807	994008.161580	41.225472
3528.576668	993512.944917	41.230477
3528.497873	993024.206237	41.235482
3528.763616	992509.744101	41.240487
3528.270523	992026.638827	41.245492
3528.398762	991525.459469	41.250496
3528.827039	991017.949158	41.255501
3528.241861	990517.870456	41.260506
3528.200683	990012.004546	41.265511
3528.146025	989515.454249	41.270516
3528.366891	989020.960003	41.275520
3528.466011	988510.647708	41.280525
3527.952269	988011.799187	41.285530
3528.087704	987508.216608	41.290535
3528.219364	987014.927885	41.295540
3528.061318	986516.572317	41.300544
3527.979657	986022.062262	41.305549
3528.080672	985515.090053	41.310554
3527.914938	985005.189831	41.315559
3527.448900	984520.661461	41.320564
3527.667130	984013.829016	41.325568
3528.008379	983529.376077	41.330573
3527.678172	983032.793280	41.335578
3527.640639	982520.112067	41.340583
3527.391181	982027.625352	41.345588
3527.576162	981532.291164	41.350592
3527.264017	981035.140927	41.355597
3527.530752	980550.544829	41.360602
3527.722219	980044.730910	41.365607
3527.095784	979549.065321	41.370612
3527.337200	979055.459949	41.375616
3527.154854	978558.658592	41.380621
3526.927518	978065.337903	41.385626
3526.928168	977576.821453	41.390631
3526.994082	977079.264430	41.395636
3527.066325	976583.226338	41.400640
3526.845192	976092.274642	41.405645
3526.657343	975601.861641	41.410650
3527.084242	975103.291442	41.415655
3526.625384	974628.183241	41.420660
3526.554543	974136.256999	41.425664
3526.779740	973648.931950	41.430669
3526.615399	973165.051321	41.435674
3526.453599	972674.383144	41.440679
3526.193894	972192.880378	41.445684
3526.203415	971699.753776	41.450688
3526.033785	971222.261708	41.455693
3525.952349	970737.575589	41.460698
3526.061194	970259.272797	41.465703
3525.925650	969779.796524	41.470708
3525.555336	969297.970942	41.475712
3526.105050	968828.280817	41.480717
3525.740962	968350.092421	41.485722
3525.496629	967852.175844	41.490727
3525.488956	967402.423041	41.495732
3525.802891	966923.416919	41.500736
3525.642412	966441.219044	41.505741
3525.307318	965966.155143	41.510746
3525.498501	965485.287386	41.515751
3525.433756	965023.022995	41.520756
3525.386434	964553.962764	41.525760
3525.294516	964074.394369	41.530765
3525.117813	963594.897874	41.535770
3525.294898	963118.730825	41.540775
3525.173722	962663.239369	41.545780
3525.037982	962175.586555	41.550784
3525.316199	961714.762849	41.555789
3524.873795	961253.335225	41.560794
3524.820640	960769.272391	41.565799
3524.680917	960307.915085	41.570804
3524.594352	959845.728148	41.575808
3524.441288	959382.045119	41.580813
3524.262092	958919.407151	41.585818
3524.598876	958460.665605	41.590823
3524.190961	958011.028235	41.595828
3524.242207	957530.498946	41.600832
3524.183608	957079.849155	41.605837
3524.092731	956625.835953	41.610842
3524.194009	956172.735896	41.615847
3523.666155	955719.605862	41.620852
3523.640453	955260.277294	41.625856
3523.724654	954820.313083	41.630861
3523.532328	954378.889669	41.635866
3523.527512	953912.094194	41.640871
3523.353433	953471.775549	41.645876
3523.636069	953023.205302	41.650880
3523.557309	952572.403175	41.655885
3523.207636	952159.009714	41.660890
3523.149822	951714.042990	41.665895
3522.989558	951289.713487	41.670900
3522.855459	950856.448691	41.675904
3523.109245	950420.883009	41.680909
3523.052971	950008.865722	41.685914
3523.123501	949570.674719	41.690919
3522.618047	949146.032600	41.695924
3522.421113	948723.696725	41.700928
3522.570138	948298.876530	41.705933
3522.472267	947883.249798	41.710938
3522.531051	947456.651989	41.715943
3522.444119	947045.358556	41.720948
3522.476873	946619.652784	41.725952
3522.283356	946203.905957	41.730957
3521.800876	945794.779699	41.735962
3521.936300	945380.444151	41.740967
3521.887190	944974.245502	41.745972
3521.585587	944565.470698	41.750976
3521.604382	944155.365640	41.755981
3521.498637	943741.225595	41.760986
3521.693971	943344.245430	41.765991
3521.577138	942945.274465	41.770996
3521.367672	942533.449871	41.776000
3521.601272	942116.058110	41.781005
3521.475516	941720.156229	41.786010
3521.218341	941310.063009	41.791015
3521.173018	940916.099020	41.796020
3520.756712	940515.840573	41.801024
3521.004080	940131.161676	41.806029
3520.854546	939728.498305	41.811034
3521.098279	939330.053019	41.816039
3520.991714	938931.539145	41.821044
3520.892168	938539.705354	41.826048
3520.811944	938146.688333	41.831053
3520.263199	937760.911097	41.836058
3520.913132	937365.701297	41.841063
3520.337028	936977.281438	41.846068
3520.267200	936587.790196	41.851072
3520.516668	936197.641875	41.856077
3520.127095	935821.575728	41.861082
3520.137732	935439.852330	41.866087
3519.957408	935049.881431	41.871092
3519.949751	934678.563733	41.876096
3520.136033	934283.869985	41.881101
3519.721400	933918.994998	41.886106
3519.728668	933537.805948	41.891111
3519.435677	933169.595994	41.896116
3519.553072	932791.406205	41.901120
3519.770725	932419.412345	41.906125
3519.243756	932047.706993	41.911130
3519.538062	931676.512241	41.916135
3519.566411	931312.056176	41.921140
3518.862087	930939.918186	41.926144
3519.340742	930572.936612	41.931149
3518.896373	930218.181841	41.936154
3518.915591	929841.430065	41.941159
3518.711624	929485.338210	41.946164
3518.715838	929122.176387	41.951168
3518.888485	928762.516198	41.956173
3518.463873	928411.479916	41.961178
3518.293493	928049.906812	41.966183
3518.388480	927703.061469	41.971188
3518.065836	927356.934972	41.976192
3518.260173	927004.262793	41.981197
3517.990611	926667.211420	41.986202
3518.160463	926307.866654	41.991207
3518.306484	925965.032469	41.996212
3518.075894	925616.952035	42.001216
3518.183049	925264.083367	42.006221
3517.970801	924924.798127	42.011226
3518.109162	924570.052214	42.016231
3517.926076	924229.372308	42.021236
3517.929863	923881.236725	42.026240
3517.847889	923539.246487	42.031245
3517.631426	923203.410809	42.036250
3517.747689	922856.344245	42.041255
3517.386926	922523.567192	42.046260
3517.716258	922178.345254	42.051264
3517.092714	921832.488748	42.056269
3516.893056	921524.438638	42.061274
3517.408745	921169.598781	42.066279
3517.216038	920846.117634	42.071284
3517.135212	920514.805970	42.076288
3517.353368	920179.287617	42.081293
3517.289355	919854.186541	42.086298
3517.093562	919525.912267	42.091303
3517.081601	919199.031266	42.096308
3516.930162	918868.881526	42.101312
3516.929183	918543.980193	42.106317
3516.558536	918221.622753	42.111322
3516.157125	917887.412126	42.116327
3516.225294	917579.574753	42.121332
3516.323039	917252.077192	42.126336
3516.481939	916942.648615	42.131341
3516.218156	916628.554610	42.136346
3516.018297	916311.350976	42.141351
3515.924246	916010.865297	42.146356
3515.807365	915694.671278	42.151360
3515.622885	915387.810927	42.156365
3515.701833	915084.549436	42.161370
3515.842034	914765.562809	42.166375
3515.782456	914474.906701	42.171380
3515.433079	914161.166418	42.176384
3515.262166	913860.864152	42.181389
3515.416600	913573.881597	42.186394
3515.526918	913268.491419	42.191399
3515.166760	912967.497053	42.196404
3514.798299	912684.311365	42.201408
3515.090007	912376.818449	42.206413
3514.904567	912093.957573	42.211418
3514.750663	911799.899159	42.216423
3514.601856	911511.509746	42.221428
3514.627616	911228.087721	42.226432
3514.830836	910942.308865	42.231437
3515.085398	910652.555139	42.236442
3515.116263	910356.172446	42.241447
3514.868797	910076.495266	42.246452
3514.649992	909778.869626	42.251456
3515.000061	909501.185558	42.256461
3514.672466	909225.334492	42.261466
3514.668652	908926.952707	42.266471
3514.401816	908643.638997	42.271476
3514.477762	908362.568395	42.276480
3514.508271	908079.466086	42.281485
3514.369399	907796.280793	42.286490
3514.613123	907517.068271	42.291495
3514.210802	907240.455582	42.296500
3514.279987	906963.751416	42.301504
3514.508993	906678.423124	42.306509
3514.005945	906406.800877	42.311514
3514.111556	906124.551023	42.316519
3513.946124	905849.276920	42.321524
3513.926217	905585.734403	42.326528
3513.948121	905311.753416	42.331533
3513.898607	905052.242413	42.336538
3513.832822	904760.882762	42.341543
3513.702319	904500.298105	42.346548
3513.639772	904222.321520	42.351552
3513.403801	903957.579738	42.356557
3513.217752	903701.791795	42.361562
3513.365518	903432.426350	42.366567
3513.118377	903166.973414	42.371572
3513.011928	902915.672382	42.376576
3513.233726	902658.900916	42.381581
3512.971206	902400.749625	42.386586
3512.942030	902143.416744	42.391591
3513.054156	901894.736685	42.396596
3512.747438	901644.763100	42.401600
3512.931003	901387.457024	42.406605
3512.743286	901146.613036	42.411610
3512.754261	900892.788361	42.416615
3512.613698	900639.942730	42.421620
3512.491927	900401.083555	42.426624
3512.507840	900156.108138	42.431629
3512.334887	899917.719688	42.436634
3512.319998	899658.339296	42.441639
3512.427400	899410.612396	42.446644
3512.015582	899185.656222	42.451648
3512.005524	898939.859566	42.456653
3511.739778	898712.735632	42.461658
3512.113198	898467.917696	42.466663
3512.232323	898238.682867	42.471668
3511.789066	897995.717736	42.476672
3511.862804	897759.805615	42.481677
3511.682145	897535.711637	42.486682
3511.853456	897298.604923	42.491687
3511.942084	897073.772007	42.496692
3511.676392	896825.993240	42.501696
3511.592109	896595.662543	42.506701
3511.589800	896365.888742	42.511706
3511.390364	896137.587573	42.516711
3511.754445	895921.940141	42.521716
3511.670182	895705.295370	42.526720
3511.639815	895464.472925	42.531725
3511.371148	895246.681334	42.536730
3511.415780	895020.904491	42.541735
3511.668371	894805.329702	42.546740
3511.311573	894575.735186	42.551744
3511.185797	894351.119725	42.556749
3511.285746	894127.424860	42.561754
3511.149012	893903.083527	42.566759
3511.121054	893689.639437	42.571764
3511.404314	893462.214706	42.576768
3511.192401	893249.557864	42.581773
3511.063367	893030.208271	42.586778
3510.901642	892809.115262	42.591783
3510.815625	892609.176534	42.596788
3510.715156	892397.823268	42.601792
3510.838625	892180.623412	42.606797
3510.818321	891969.627901	42.611802
3510.729973	891759.506164	42.616807
3510.674318	891550.144995	42.621812
3510.315323	891342.180118	42.626816
3510.817374	891143.157087	42.631821
3510.458886	890940.303457	42.636826
3510.423467	890730.328676	42.641831
3510.244852	890530.912929	42.646836
3510.146641	890325.286327	42.651840
3510.531056	890118.992441	42.656845
3509.896726	889918.663173	42.661850
3509.946072	889723.631680	42.666855
3510.068190	889527.420664	42.671860
3509.969773	889330.271828	42.676864
3510.310483	889135.656113	42.681869
3509.783933	888944.466299	42.686874
3510.127143	888756.513276	42.691879
3510.216962	888543.922299	42.696884
3509.770253	888360.440667	42.701888
3509.779043	888157.621777	42.706893
3509.655348	887973.300467	42.711898
3509.970945	887775.256018	42.716903
3509.754133	887593.550763	42.721908
3509.378171	887391.058632	42.726912
3509.639471	887205.391230	42.731917
3509.621890	887022.280218	42.736922
3509.479698	886837.248175	42.741927
3509.636482	886654.483930	42.746932
3509.609517	886468.937157	42.751936
3509.751891	886275.999937	42.756941
3509.268238	886086.450649	42.761946
3509.480670	885902.975891	42.766951
3509.477823	885725.629606	42.771956
3509.347141	885536.875422	42.776960
3509.772747	885343.279601	42.781965
3509.306493	885164.927564	42.786970
3509.161170	884987.582167	42.791975
3509.270391	884804.380095	42.796980
3509.108266	884633.223232	42.801985
3509.163887	884439.464564	42.806989
3508.926433	884268.793507	42.811994
3509.258619	884092.310386	42.816999
3508.854155	883922.237667	42.822004
3508.643408	883755.517430	42.827009
3508.985716	883570.882299	42.832013
3508.592384	883403.213620	42.837018
3508.670557	883234.397090	42.842023
3509.013899	883059.624068	42.847028
3509.046285	882887.027823	42.852033
3508.903988	882721.428925	42.857037
3508.918313	882537.008769	42.862042
3509.483652	882355.397872	42.867047
3508.919550	882187.819195	42.872052
3508.319413	882011.814092	42.877057
3509.140932	881843.416007	42.882061
3508.661134	881679.393063	42.887066
3508.373511	881508.649351	42.892071
3508.786391	881337.591469	42.897076
3508.383004	881171.119664	42.902081
3508.936848	881008.554569	42.907085
3508.771641	880844.359454	42.912090
3508.810407	880665.689422	42.917095
3508.436344	880498.224716	42.922100
3508.219782	880349.139525	42.927105
3508.610710	880171.171541	42.932109
3508.588451	880020.301782	42.937114
3508.185506	879845.652457	42.942119
3508.159338	879681.111088	42.947124
3508.102479	879528.780770	42.952129
3508.047834	879369.177722	42.957133
3507.907680	879221.892586	42.962138
3508.103080	879060.301646	42.967143
3508.233532	878901.430717	42.972148
3508.300278	878747.315187	42.977153
3508.164438	878592.841294	42.982157
3507.852321	878436.356905	42.987162
3508.391965	878274.396846	42.992167
3508.217634	878113.907028	42.997172
3508.040252	877951.183815	43.002177
3508.161586	877801.881281	43.007181
3507.949613	877648.461435	43.012186
3507.835052	877488.526350	43.017191
3508.023903	877347.635220	43.022196
3508.177484	877193.561617	43.027201
3507.678225	877028.345276	43.032205
3507.406724	876880.538369	43.037210
3507.751003	876739.607096	43.042215
3507.988151	876586.279496	43.047220
3507.635759	876438.571796	43.052225
3507.839459	876285.629738	43.057229
3507.540484	876137.323916	43.062234
3507.527905	875982.567300	43.067239
3507.656149	875836.510761	43.072244
3507.420108	875695.068351	43.077249
3507.843215	875541.489040	43.082253
3507.523074	875397.822942	43.087258
3507.284043	875253.073209	43.092263
3507.581941	875109.589216	43.097268
3507.697639	874964.580012	43.102273
3507.600537	874812.813224	43.107277
3507.344286	874679.787730	43.112282
3507.358943	874538.955287	43.117287
3507.358010	874403.456727	43.122292
3507.139797	874251.986501	43.127297
3507.226800	874107.349023	43.132301
3507.056553	873978.561548	43.137306
3507.149583	873831.976344	43.142311
3507.005929	873701.432413	43.147316
3506.774488	873562.169396	43.152321
3507.287710	873435.003645	43.157325
3506.764255	873305.483676	43.162330
3506.828694	873165.968589	43.167335
3506.981789	873028.958042	43.172340
3506.742643	872909.860347	43.177345
3506.886495	872769.546722	43.182349
3506.786591	872648.480435	43.187354
3506.853029	872499.732235	43.192359
3506.993676	872373.090284	43.197364
3506.642844	872248.176111	43.202369
3506.918290	872108.989571	43.207373
3506.732910	871998.888673	43.212378
3506.431440	871856.006983	43.217383
3506.923218	871719.201576	43.222388
3506.706096	871602.985212	43.227393
3506.876559	871468.070734	43.232397
3506.497278	871331.399948	43.237402
3506.862732	871202.464055	43.242407
3506.799699	871086.600416	43.247412
3506.483427	870956.024659	43.252417
3506.542802	870824.510679	43.257421
3506.263033	870718.963135	43.262426
3506.301752	870589.679623	43.267431
3506.506812	870455.901229	43.272436
3506.088463	870346.099362	43.277441
3506.595811	870217.701185	43.282445
3506.510275	870099.686731	43.287450
3506.306173	869976.156724	43.292455
3505.978334	869861.477732	43.297460
3506.215849	869742.529387	43.302465
3506.452811	869610.377002	43.307469
3506.111863	869487.150654	43.312474
3506.080424	869376.976006	43.317479
3506.231264	869260.362177	43.322484
3506.198535	869157.367439	43.327489
3506.026558	869032.841863	43.332493
3505.932865	868932.086163	43.337498
3506.153253	868805.452469	43.342503
3506.002831	868687.129590	43.347508
3505.724122	868573.777039	43.352513
3506.041874	868460.615338	43.357517
3506.159192	868348.746730	43.362522
3506.019636	868236.821266	43.367527
3506.081180	868126.511210	43.372532
3506.058382	868005.532261	43.377537
3506.181287	867882.584868	43.382541
3505.892532	867785.434737	43.387546
3505.946043	867664.436340	43.392551
3506.005020	867552.465402	43.397556
3505.975062	867444.294205	43.402561
3506.181282	867331.615142	43.407565
3505.828124	867230.485180	43.412570
3506.187764	867104.472435	43.417575
3506.190443	866984.731193	43.422580
3505.920181	866870.665285	43.427585
3506.043421	866750.802405	43.432589
3505.782730	866654.891905	43.437594
3505.754936	866531.358988	43.442599
3505.921560	866431.975266	43.447604
3505.750914	866318.173839	43.452609
3505.705468	866209.303109	43.457613
3505.549954	866098.700229	43.462618
3505.653294	865991.355104	43.467623
3505.793610	865889.052847	43.472628
3505.221731	865792.111421	43.477633
3505.404408	865671.343065	43.482637
3505.730781	865574.832955	43.487642
3505.733621	865468.563592	43.492647
3505.868239	865367.710515	43.497652
3505.155263	865285.355241	43.502657
3505.476132	865163.873968	43.507661
3505.249045	865068.321246	43.512666
3505.478298	864956.662569	43.517671
3505.330110	864862.065054	43.522676
3505.269414	864763.565634	43.527681
3505.292386	864659.124559	43.532685
3505.484541	864569.712589	43.537690
3505.199645	864465.416046	43.542695
3504.993467	864372.472054	43.547700
3505.352111	864282.251150	43.552705
3505.338194	864167.411749	43.557709
3505.207271	864082.903803	43.562714
3504.836446	863979.487484	43.567719
3505.041236	863881.707255	43.572724
3504.848108	863800.995030	43.577729
3505.186885	863691.238258	43.582733
3504.979736	863600.420246	43.587738
3505.116784	863510.904543	43.592743
3505.168170	863424.802644	43.597748
3505.246756	863321.981243	43.602753
3504.930189	863221.263882	43.607757
3504.728064	863133.936344	43.612762
3504.910336	863051.986165	43.617767
3505.010736	862960.524818	43.622772
3504.530750	862872.947765	43.627777
3504.965577	862773.751230	43.632781
3504.781058	862684.567857	43.637786
3504.850905	862602.824502	43.642791
3504.729079	862519.556649	43.647796
3504.321083	862426.421665	43.652801
3504.788290	862339.555529	43.657805
3504.521500	862266.610127	43.662810
3504.453863	862166.222985	43.667815
3504.713594	862085.121717	43.672820
3504.671296	862011.650296	43.677825
3504.820998	861919.290390	43.682829
3504.619836	861840.302908	43.687834
3504.466461	861748.670725	43.692839
3504.934362	861653.241192	43.697844
3504.500174	861586.730407	43.702849
3504.675264	861505.538154	43.707853
3504.506208	861423.623892	43.712858
3504.317339	861328.297477	43.717863
3504.592500	861236.878589	43.722868
3504.225019	861151.591120	43.727873
3504.381198	861089.254772	43.732877
3504.330579	861001.288341	43.737882
3504.530110	860922.903394	43.742887
3504.659438	860836.265894	43.747892
3504.374331	860761.361180	43.752897
3504.366142	860674.744041	43.757901
3504.556251	860595.287059	43.762906
3504.204078	860518.154411	43.767911
3504.333976	860436.858138	43.772916
3504.247690	860365.707357	43.777921
3504.481231	860285.753082	43.782925
3504.416083	860212.944262	43.787930
3504.566744	860127.945972	43.792935
3504.766346	860036.715981	43.797940
3504.494712	859964.910481	43.802945
3504.746868	859874.058308	43.807949
3504.615506	859787.935009	43.812954
3504.634158	859713.550743	43.817959
3504.506746	859628.299620	43.822964
3504.285308	859546.077044	43.827969
3504.401263	859463.700532	43.832973
3504.146503	859394.413647	43.837978
3504.085846	859317.412247	43.842983
3504.359656	859236.854177	43.847988
3504.341404	859160.913443	43.852993
3504.653786	859086.570385	43.857997
3504.372142	859002.502830	43.863002
3504.053775	858923.788569	43.868007
3504.284972	858855.874158	43.873012
3504.343330	858784.681115	43.878017
3504.604408	858700.228242	43.883021
3504.052687	858624.368742	43.888026
3503.797504	858559.643129	43.893031
3504.253913	858475.738470	43.898036
3504.243116	858406.789191	43.903041
3504.458122	858328.465642	43.908045
3504.273449	858246.705791	43.913050
3503.506902	858184.491824	43.918055
3503.567200	858107.747027	43.923060
3503.861304	858036.603696	43.928065
3504.136863	857968.088582	43.933069
3503.816985	857909.299533	43.938074
3504.221999	857835.995885	43.943079
3504.455886	857756.494784	43.948084
3504.071832	857695.671752	43.953089
3503.632013	857620.073146	43.958093
3504.013934	857558.247163	43.963098
3503.624264	857485.362059	43.968103
3504.278505	857419.112813	43.973108
3503.915916	857361.687290	43.978113
3504.013230	857271.308330	43.983117
3504.407559	857207.336832	43.988122
3504.133336	857143.377553	43.993127
3504.052980	857043.978228	43.998132
3503.842050	856986.329653	44.003137
3504.075310	856905.163960	44.008141
3503.725760	856846.272326	44.013146
3503.470747	856778.025899	44.018151
3503.991056	856707.997226	44.023156
3503.940970	856646.330524	44.028161
3503.271282	856588.559241	44.033165
3503.397043	856519.079828	44.038170
3503.709721	856453.751994	44.043175
3504.231606	856383.622086	44.048180
3503.619079	856325.449771	44.053185
3503.724094	856267.158675	44.058189
3503.699712	856193.322460	44.063194
3503.676523	856125.517020	44.068199
3503.732295	856064.118897	44.073204
3503.257264	856010.201651	44.078209
3503.758544	855949.410007	44.083213
3503.826789	855876.624926	44.088218
3503.657904	855810.785860	44.093223
3503.740830	855762.125616	44.098228
3503.826819	855690.211050	44.103233
3503.697518	855621.541885	44.108237
3503.816520	855561.976957	44.113242
3503.450556	855512.610328	44.118247
3503.824273	855435.780496	44.123252
3503.699691	855375.962007	44.128257
3503.691133	855305.907228	44.133261
3503.853985	855242.926456	44.138266
3503.479158	855177.601059	44.143271
3503.827867	855113.518008	44.148276
3503.718854	855045.130983	44.153281
3503.788415	854980.800633	44.158285
3503.562471	854926.638232	44.163290
3503.511660	854859.212623	44.168295
3503.707474	854796.903020	44.173300
3503.404031	854749.466147	44.178305
3503.513105	854675.881672	44.183309
3503.695553	854608.025640	44.188314
3503.486603	854565.340064	44.193319
3503.462884	854486.909583	44.198324
3503.190596	854436.351121	44.203329
3503.333232	854377.549372	44.208333
3503.770707	854328.527445	44.213338
3503.190467	854265.853767	44.218343
3503.345783	854198.289652	44.223348
3503.532966	854147.750437	44.228353
3503.606128	854082.534254	44.233357
3503.873040	854016.993495	44.238362
3503.148887	853964.364549	44.243367
3503.889897	853897.576542	44.248372
3503.439208	853836.823620	44.253377
3503.343297	853785.160195	44.258381
3503.174621	853743.824848	44.263386
3503.272075	853687.846420	44.268391
3503.342571	853623.404442	44.273396
3503.158253	853583.238527	44.278401
3503.216955	853517.726781	44.283405
3503.060065	853469.963932	44.288410
3502.972802	853414.013461	44.293415
3503.430429	853358.946019	44.298420
3503.442477	853310.570112	44.303425
3503.576086	853240.955131	44.308429
3503.426378	853183.942198	44.313434
3503.136943	853123.447691	44.318439
3503.152482	853064.557058	44.323444
3503.342657	853021.892383	44.328449
3503.232139	852970.808580	44.333453
3503.049434	852903.383350	44.338458
3502.764113	852856.902330	44.343463
3503.076509	852811.587900	44.348468
3502.956948	852762.450671	44.353473
3503.007505	852701.117284	44.358477
3502.780799	852661.828445	44.363482
3502.707448	852611.903666	44.368487
3503.229286	852572.198891	44.373492
3503.260491	852521.574749	44.378497
3503.075927	852462.516671	44.383501
3503.057827	852414.430766	44.388506
3502.899986	852364.517915	44.393511
3503.178288	852309.470696	44.398516
3503.016666	852257.123899	44.403521
3502.911110	852206.032968	44.408525
3503.123199	852155.960134	44.413530
3502.894530	852105.278059	44.418535
3503.132069	852059.094303	44.423540
3502.894047	852013.767384	44.428545
3503.054833	851957.178758	44.433549
3503.202123	851909.937872	44.438554
3502.939215	851861.498597	44.443559
3502.995544	851813.298410	44.448564
3503.125050	851786.796297	44.453569
3503.155689	851723.314679	44.458573
3503.058059	851675.236145	44.463578
3503.069827	851619.447859	44.468583
3503.011284	851578.761415	44.473588
3502.758742	851524.086777	44.478593
3502.924559	851479.468295	44.483597
3503.114001	851430.074866	44.488602
3503.119113	851380.127240	44.493607
3503.190852	851325.884238	44.498612
3503.210407	851292.582678	44.503617
3503.078147	851224.157225	44.508621
3502.813441	851183.015331	44.513626
3503.030455	851134.296569	44.518631
3502.932708	851088.355573	44.523636
3503.035158	851043.744403	44.528641
3502.906797	850990.310386	44.533645
3503.340555	850941.359662	44.538650
3503.178400	850888.514555	44.543655
3502.808702	850840.571756	44.548660
3502.956799	850805.493725	44.553665
3502.914934	850751.946034	44.558669
3502.807975	850708.535434	44.563674
3502.599942	850657.935510	44.568679
3503.113569	850616.953742	44.573684
3502.967408	850574.814539	44.578689
3502.899790	850521.755985	44.583693
3502.989718	850471.300199	44.588698
3502.738221	850433.656734	44.593703
3503.122548	850387.436372	44.598708
3502.575384	850345.848581	44.603713
3502.698132	850293.340986	44.608717
3502.835453	850247.160282	44.613722
3502.660061	850214.371971	44.618727
3502.981353	850153.942621	44.623732
3502.891246	850114.712522	44.628737
3502.703792	850072.771486	44.633741
3502.813352	850009.551509	44.638746
3502.821009	849974.686706	44.643751
3502.809419	849939.922264	44.648756
3502.849039	849882.750410	44.653761
3502.592989	849853.966321	44.658765
3503.082122	849810.256463	44.663770
3502.811517	849780.013621	44.668775
3502.791390	849716.714654	44.673780
3502.769712	849676.009683	44.678785
3502.807538	849639.190243	44.683789
3503.033766	849591.529180	44.688794
3503.068496	849539.808864	44.693799
3503.040209	849489.851564	44.698804
3502.632635	849443.462509	44.703809
3502.777965	849399.514243	44.708813
3502.899013	849346.317193	44.713818
3502.420762	849310.360000	44.718823
3502.516475	849260.283033	44.723828
3502.447869	849228.640686	44.728833
3502.563085	849189.176133	44.733837
3502.641861	849151.373095	44.738842
3502.510610	849105.909972	44.743847
3502.927596	849076.816598	44.748852
3502.892502	849032.603280	44.753857
3502.622602	848982.681727	44.758861
3502.904051	848945.720652	44.763866
3502.703852	848906.111479	44.768871
3502.698559	848865.398517	44.773876
3502.656889	848820.697771	44.778881
3502.556255	848771.623263	44.783885
3503.051558	848728.684049	44.788890
3502.865982	848696.960874	44.793895
3502.571014	848646.164115	44.798900
3502.514552	848610.815224	44.803905
3502.550038	848575.256169	44.808909
3502.866816	848538.968713	44.813914
3502.596579	848490.212160	44.818919
3502.587193	848449.497161	44.823924
3502.482032	848417.077452	44.828929
3502.398124	848367.802196	44.833933
3503.011573	848321.528786	44.838938
3502.811224	848292.923128	44.843943
3502.884736	848235.340950	44.848948
3502.696054	848196.894320	44.853953
3502.773557	848151.876914	44.858957
3503.231292	848108.062914	44.863962
3502.649825	848071.433681	44.868967
3502.854386	848014.802023	44.873972
3502.621332	847977.627754	44.878977
3502.632128	847938.659588	44.883981
3502.678145	847894.327431	44.888986
3502.397706	847865.927848	44.893991
3502.464535	847825.001388	44.898996
3502.334605	847790.926400	44.904001
3502.325277	847753.713936	44.909005
3502.635584	847721.027321	44.914010
3502.583236	847684.016371	44.919015
3502.723083	847641.517952	44.924020
3502.387636	847606.014503	44.929025
3502.470688	847563.037800	44.934029
3502.293146	847528.287271	44.939034
3502.373214	847488.525503	44.944039
3502.528994	847453.232518	44.949044
3502.413900	847420.517005	44.954049
3502.389620	847378.530967	44.959053
3502.672956	847343.606048	44.964058
3502.516309	847311.481366	44.969063
3502.448494	847258.395090	44.974068
3502.364419	847226.355441	44.979073
3502.020911	847196.209508	44.984077
3501.948989	847163.388109	44.989082
3502.141227	847136.855901	44.994087
3502.092736	847098.574276	44.999092
3502.169081	847084.044768	45.004097
3501.874833	847044.244427	45.009101
3502.443378	847019.306034	45.014106
3502.215024	846987.094072	45.019111
3502.275710	846951.229340	45.024116
3502.215459	846915.092032	45.029121
3501.992409	846889.211798	45.034125
3502.154347	846863.852622	45.039130
3502.151948	846834.428206	45.044135
3502.253533	846801.576324	45.049140
3502.226916	846780.437548	45.054145
3502.294382	846747.688439	45.059149
3502.620974	846711.875960	45.064154
3502.041048	846675.530591	45.069159
3501.906893	846639.696180	45.074164
3502.092443	846623.296314	45.079169
3502.063023	846595.629095	45.084173
3502.001418	846566.115739	45.089178
3501.870075	846533.203392	45.094183
3502.315710	846498.247025	45.099188
3502.075342	846475.096222	45.104193
3502.225033	846441.844772	45.109197
3502.525499	846411.004310	45.114202
3502.138015	846377.938471	45.119207
3502.163773	846350.261079	45.124212
3502.256729	846308.930646	45.129217
3501.980444	846283.056679	45.134221
3502.493880	846233.861084	45.139226
3502.565092	846217.966214	45.144231
3502.591369	846178.399888	45.149236
3502.204855	846132.762321	45.154241
3502.388994	846112.950794	45.159245
3502.095609	846072.169685	45.164250
3501.857724	846056.032999	45.169255
3502.382559	846018.624771	45.174260
3502.417273	845987.826020	45.179265
3502.364254	845947.589177	45.184269
3502.471864	845917.362755	45.189274
3502.229334	845885.732154	45.194279
3502.345493	845847.123415	45.199284
3502.217094	845816.935397	45.204289
3502.245144	845797.538392	45.209293
3502.284099	845764.886304	45.214298
3502.105847	845734.803555	45.219303
3502.335441	845689.548501	45.224308
3502.236909	845663.740140	45.229313
3502.232123	845634.992657	45.234317
3502.403650	845601.635710	45.239322
3502.183696	845578.575685	45.244327
3502.346611	845541.614069	45.249332
3502.264270	845510.539905	45.254337
3502.423454	845479.230882	45.259341
3502.205275	845445.644955	45.264346
3501.968677	845421.027809	45.269351
3502.180412	845378.014935	45.274356
3502.618143	845350.460169	45.279361
3502.304402	845312.113893	45.284365
3502.440152	845278.761129	45.289370
3502.369247	845251.582113	45.294375
3502.903494	845198.281745	45.299380
3502.437264	845179.061734	45.304385
3501.964304	845145.223803	45.309389
3502.221000	845115.066419	45.314394
3502.225500	845084.658064	45.319399
3502.164575	845050.849194	45.324404
3502.141748	845021.029801	45.329409
3501.795780	844993.310219	45.334413
3501.902945	844958.206145	45.339418
3501.696199	844946.154908	45.344423
3502.549522	844912.584507	45.349428
3502.304433	844887.771742	45.354433
3502.174960	844864.109401	45.359437
3502.176273	844821.224859	45.364442
3501.684645	844798.694057	45.369447
3501.948757	844768.728725	45.374452
3501.747515	844746.052422	45.379457
3502.022175	844718.716698	45.384461
3502.297048	844690.406151	45.389466
3501.584622	844678.827589	45.394471
3502.291595	844644.305206	45.399476
3502.144417	844610.898054	45.404481
3501.675286	844586.608357	45.409485
3502.019318	844557.018724	45.414490
3501.742130	844542.639062	45.419495
3501.693248	844506.583491	45.424500
3502.094448	844479.518289	45.429505
3501.857664	844456.164506	45.434509
3502.023143	844424.459318	45.439514
3501.901489	844405.277630	45.444519
3502.302819	844378.017030	45.449524
3502.122868	844347.245617	45.454529
3501.937535	844324.955064	45.459533
3502.124964	844289.054255	45.464538
3502.078196	844272.978966	45.469543
3502.164222	844232.025921	45.474548
3502.337264	844219.228393	45.479553
3502.136793	844187.874737	45.484557
3502.383240	844153.328078	45.489562
3501.956367	844132.928673	45.494567
3502.147077	844098.585849	45.499572
3502.063673	844063.898097	45.504577
3502.037259	844036.901457	45.509581
3501.915988	844022.689869	45.514586
3501.925925	843992.860209	45.519591
3502.027380	843963.795154	45.524596
3502.044800	843928.505176	45.529601
3501.937240	843908.539822	45.534605
3502.092424	843878.393252	45.539610
3502.218218	843844.449659	45.544615
3502.260372	843826.214017	45.549620
3502.220789	843805.457294	45.554625
3501.870959	843781.632230	45.559629
3502.209394	843739.952034	45.564634
3502.212393	843717.043407	45.569639
3502.130424	843686.057655	45.574644
3502.193306	843658.947202	45.579649
3501.875615	843615.814570	45.584653
3502.487845	843589.003234	45.589658
3502.195791	843562.535753	45.594663
3501.900173	843546.694583	45.599668
3501.777157	843525.658233	45.604673
3501.956014	843497.845583	45.609677
3501.999345	843463.133644	45.614682
3501.592854	843439.609080	45.619687
3501.647127	843416.398454	45.624692
3501.632514	843398.950824	45.629697
3501.912490	843381.844555	45.634701
3502.166454	843338.518347	45.639706
3501.674151	843332.360336	45.644711
3502.005604	843311.053410	45.649716
3501.877864	843281.828004	45.654721
3501.712939	843264.209791	45.659725
3501.841705	843228.702574	45.664730
3501.912850	843217.479641	45.669735
3502.233200	843188.179969	45.674740
3502.038435	843167.446716	45.679745
3501.810021	843151.983442	45.684749
3502.107741	843116.155282	45.689754
3502.096870	843095.976442	45.694759
3502.127977	843066.723866	45.699764
3502.173203	843037.956291	45.704769
3502.147240	843009.297808	45.709773
3502.395652	842975.036861	45.714778
3502.074022	842946.036834	45.719783
3501.766257	842912.354657	45.724788
3501.820302	842898.306636	45.729793
3501.610792	842882.937081	45.734797
3501.773787	842841.279867	45.739802
3501.887260	842829.269306	45.744807
3501.880796	842812.208696	45.749812
3502.017459	842785.959803	45.754817
3501.625480	842742.735944	45.759821
3501.745513	842657.113273	45.764826
3501.523111	842522.503330	45.769831
3501.872047	842327.442032	45.774836
3501.897642	842070.462342	45.779841
3501.654520	841759.251188	45.784845
3501.883196	841380.367364	45.789850
3501.535096	840953.281442	45.794855
3501.244334	840457.933900	45.799860
3501.339408	839902.057942	45.804865
3501.197169	839289.105918	45.809869
3500.982469	838604.400166	45.814874
3500.740056	837868.302841	45.819879
3500.668550	837055.782040	45.824884
3500.516366	836188.858542	45.829889
3500.036779	835245.295660	45.834893
3500.254486	834239.144573	45.839898
3499.661968	833166.963073	45.844903
3499.554010	832017.225393	45.849908
3499.365325	830801.412283	45.854913
3498.816225	829512.303520	45.859917
3498.739564	828139.507261	45.864922
3497.907103	826698.910138	45.869927
3497.813287	825177.121678	45.874932
3497.497628	823589.548522	45.879937
3496.710766	821928.751729	45.884941
3496.590893	820192.141825	45.889946
3496.301224	818372.605859	45.894951
3495.280336	816488.573896	45.899956
3495.082806	814513.151866	45.904961
3494.656659	812469.502321	45.909965
3494.020006	810340.318237	45.914970
3493.234629	808136.146207	45.919975
3492.709015	805862.290986	45.924980
3491.877361	803507.942314	45.929985
3490.998095	801088.333832	45.934989
3490.849403	798584.968434	45.939994
3490.049412	796017.576431	45.944999
3489.328320	793368.881468	45.950004
3488.743606	790650.382794	45.955009
3487.919238	787850.419768	45.960013
3487.592522	784956.882507	45.965018
3486.521530	782020.142017	45.970023
3485.898394	778994.437539	45.975028
3485.061020	775899.714314	45.980033
3483.864625	772736.656560	45.985037
3483.215289	769485.770488	45.990042
3482.226360	766171.400499	45.995047
3481.042717	762791.772703	46.000052
3480.266830	759325.149880	46.005057
3479.381690	755798.266202	46.010061
3478.740370	752198.400042	46.015066
3477.326358	748529.732219	46.020071
3476.338204	744784.814945	46.025076
3475.708690	740972.122560	46.030081
3474.098701	737086.005448	46.035085
3472.943948	733131.335732	46.040090
3472.108402	729108.252041	46.045095
3471.112388	725005.304395	46.050100
3469.771598	720848.851120	46.055105
3468.444061	716613.376237	46.060109
3467.260094	712307.347623	46.065114
3465.891869	707945.483867	46.070119
3464.601556	703498.666822	46.075124
3463.304619	698983.706503	46.080129
3462.205329	694421.976310	46.085133
3461.086399	689769.729321	46.090138
3459.452523	685065.470053	46.095143
3458.244296	680277.661604	46.100148
3456.926244	675419.849655	46.105153
3455.061624	670509.731675	46.110157
3453.815076	665521.724171	46.115162
3452.188187	660454.707653	46.120167
3450.566194	655328.259253	46.125172
3449.036235	650148.356472	46.130177
3447.446082	644911.081270	46.135181
3445.724316	639592.537294	46.140186
3444.168403	634229.726308	46.145191
3442.589893	628787.503910	46.150196
3441.046900	623284.169288	46.155201
3438.770958	617733.285309	46.160205
3437.269179	612110.206256	46.165210
3435.465874	606410.583813	46.170215
3433.207734	600678.554562	46.175220
3431.639087	594876.315176	46.180225
3429.714875	589016.851271	46.185229
3427.981088	583087.625836	46.190234
3425.842417	577114.645890	46.195239
3423.674172	571067.399013	46.200244
3421.838897	564977.043986	46.205249
3419.565664	558819.429524	46.210253
3417.454894	552612.264340	46.215258
3415.053262	546348.510035	46.220263
3413.173780	540028.878368	46.225268
3411.149880	533667.499578	46.230273
3408.590147	527236.028882	46.235277
3406.156606	520752.921670	46.240282
3403.833645	514229.756565	46.245287
3401.476523	507640.345655	46.250292
3399.137961	501020.222305	46.255297
3396.621668	494351.245614	46.260301
3394.318157	487622.641394	46.265306
3391.835197	480846.836838	46.270311
3389.263964	474034.023350	46.275316
3386.756943	467165.369166	46.280321
3384.061649	460266.533005	46.285325
3381.098294	453305.589189	46.290330
3378.447043	446305.641694	46.295335
3375.613206	439279.503708	46.300340
3373.111261	432200.307678	46.305345
3369.945519	425090.035600	46.310349
3367.235781	417939.552657	46.315354
3364.155411	410749.230308	46.320359
3361.355370	403527.582187	46.325364
3358.056099	396259.815053	46.330369
3354.903435	388992.774118	46.335373
3351.751341	381664.756227	46.340378
3348.415880	374309.969992	46.345383
3345.272809	366932.783689	46.350388
3341.918711	359517.019555	46.355393
3338.657796	352100.816697	46.360397
3335.274376	344645.176715	46.365402
3331.822214	337179.897819	46.370407
3328.309380	329686.903750	46.375412
3325.138118	322173.093212	46.380417
3320.907116	314643.656252	46.385421
3317.603248	307092.330587	46.390426
3314.286943	299538.722228	46.395431
3310.681697	291954.537638	46.400436
3306.794346	284354.391820	46.405441
3302.559721	276755.361429	46.410445
3299.179389	269136.421172	46.415450
3295.148909	261519.573603	46.420455
3291.234947	253895.122478	46.425460
3287.360992	246259.827006	46.430465
3283.138042	238634.234277	46.435469
3279.216509	231001.638921	46.440474
3274.981070	223271.445726	46.445479
3270.453919	215635.005374	46.450484
3266.454792	208000.995736	46.455489
3261.893158	200386.608954	46.460493
3257.924183	192772.322049	46.465498
3253.309422	185167.241025	46.470503
3248.750366	177577.067818	46.475508
3244.230772	169985.405824	46.480513
3239.211489	162439.821035	46.485517
3234.928249	154893.124704	46.490522
3230.122482	147380.292104	46.495527
3225.230982	139881.149006	46.500532
3220.591742	132402.446153	46.505537
3215.255878	124966.208973	46.510541
3210.113404	117544.657148	46.515546
3205.101383	110176.995081	46.520551
3199.983084	102828.340733	46.525556
3194.614410	95525.983359	46.530561
3188.501123	88280.302688	46.535565
3182.456192	81053.915773	46.540570
3176.476132	73905.734429	46.545575
3169.965987	66822.069336	46.550580
3163.402491	59809.160626	46.555585
3154.853103	52907.387613	46.560589
3138.741285	46318.802448	46.565594
3117.734037	40003.127324	46.570599
3098.173254	33949.690900	46.575604
3079.485633	28192.596158	46.580609
3060.312307	22777.037978	46.585613
3040.159165	17768.611594	46.590618
3017.100519	13242.219818	46.595623
2990.199052	9249.730975	46.600628
2962.532432	5778.678395	46.605633
2936.051931	2837.830380	46.610637
2903.411873	637.215354	46.615642
2825.621500	300.347884	46.620647
2772.154021	292.442802	46.625652
2759.828431	290.608843	46.630657
2774.489104	288.119904	46.635661
2801.769471	287.600925	46.640666
2828.173590	283.076154	46.645671
2845.589868	268.099171	46.650676
2854.203130	267.378295	46.655681
2854.654103	271.054288	46.660685
2850.829686	262.909165	46.665690
2845.562287	271.300279	46.670695
2840.161802	271.112762	46.675700
2836.368392	258.448517	46.680705
2833.447049	265.416892	46.685709
2831.121263	266.024923	46.690714
2828.893947	258.633010	46.695719
2826.315369	270.641802	46.700724
2824.201697	261.825663	46.705729
2820.988531	259.880074	46.710733
2818.696651	253.149659	46.715738
2815.576888	254.376929	46.720743
2812.439808	258.719152	46.725748
2809.548293	250.084262	46.730753
2806.091919	258.975031	46.735757
2803.145132	253.282959	46.740762
2800.172568	243.239797	46.745767
2796.640632	252.510093	46.750772
2793.646717	250.153000	46.755777
2790.330713	263.189677	46.760781
2787.465187	251.696148	46.765786
2784.218924	250.225326	46.770791
2780.727807	246.108685	46.775796
2777.584008	239.601361	46.780801
2773.737883	252.087701	46.785805
2770.366360	241.662031	46.790810
2767.073730	243.575400	46.795815
2763.799862	250.639075	46.800820
2760.964265	236.169845	46.805825
2757.620133	243.053298	46.810829
2753.945421	242.787126	46.815834
2750.589387	246.889232	46.820839
2747.055998	248.154802	46.825844
2744.394185	241.098291	46.830849
2741.077813	242.038749	46.835853
2737.198544	238.558091	46.840858
2734.098197	238.492772	46.845863
2730.277210	239.109984	46.850868
2727.557848	230.660670	46.855873
2723.638444	230.599483	46.860877
2720.303101	234.563209	46.865882
2716.872580	229.105745	46.870887
2713.273058	236.176609	46.875892
2710.445105	235.752186	46.880897
2706.511948	240.037571	46.885901
2702.688846	225.321673	46.890906
2699.928061	229.160204	46.895911
2696.483874	232.807215	46.900916
2693.031724	217.806725	46.905921
2689.136395	236.253848	46.910925
2685.775968	223.773278	46.915930
2682.712660	230.627003	46.920935
2679.366803	234.181230	46.925940
2676.227084	226.055893	46.930945
2672.577614	233.858481	46.935949
2668.360071	221.012209	46.940954
2665.154633	228.280135	46.945959
2662.143692	225.268000	46.950964
2658.912166	222.619859	46.955969
2654.578243	226.901560	46.960973
2651.149916	222.026338	46.965978
2648.006431	213.669576	46.970983
2643.938579	223.249021	46.975988
2641.035329	218.611976	46.980993
2637.924307	212.786101	46.985997
2634.624772	214.612282	46.991002
2631.341149	226.941132	46.996007
2627.778128	223.056710	47.001012
2624.497205	211.941708	47.006017
2620.473225	218.774430	47.011021
2616.608476	214.124401	47.016026
2613.569807	224.797392	47.021031
2610.584465	214.303000	47.026036
2606.576888	220.471141	47.031041
2603.180817	213.820084	47.036045
2599.859766	217.077803	47.041050
2596.309473	217.249835	47.046055
2592.839950	218.623770	47.051060
2589.150541	216.528815	47.056065
2585.411674	224.422778	47.061069
2582.580628	222.174317	47.066074
2578.744562	217.932423	47.071079
2575.465390	216.312854	47.076084
2572.258785	209.498332	47.081089
2568.691278	204.536822	47.086093
2564.840005	208.533696	47.091098
2561.579726	211.218984	47.096103
2557.863298	210.970895	47.101108
2554.612581	201.861090	47.106113
2550.905120	205.081971	47.111117
2547.425550	207.226042	47.116122
2543.942648	207.547624	47.121127
2540.093005	205.059609	47.126132
2537.259747	203.060193	47.131137
2533.747179	207.064728	47.136141
2529.932972	199.312515	47.141146
2527.225680	196.131948	47.146151
2523.108373	197.503524	47.151156
2519.856597	195.199831	47.156161
2516.472772	201.999974	47.161165
2512.554674	197.501718	47.166170
2509.028894	194.522964	47.171175
2505.334417	198.782511	47.176180
2502.679711	196.960063	47.181185
2498.842170	202.759995	47.186189
2495.533003	191.517750	47.191194
2492.022240	199.712552	47.196199
2488.258287	205.121056	47.201204
2484.767930	188.918167	47.206209
2481.431754	195.329596	47.211213
2477.675479	201.085342	47.216218
2474.247537	192.070376	47.221223
2470.729879	201.758031	47.226228
2467.820342	192.950745	47.231233
2463.741722	193.700477	47.236237
2460.565088	197.065870	47.241242
2457.005501	195.291780	47.246247
2453.113113	207.391048	47.251252
2449.774120	193.173909	47.256257
2446.343743	199.144263	47.261261
2443.184100	193.401941	47.266266
2439.905633	185.624721	47.271271
2435.919740	196.400470	47.276276
2432.928309	189.523699	47.281281
2429.030935	192.770293	47.286285
2425.441377	199.022297	47.291290
2422.477842	192.062781	47.296295
2418.587773	194.121171	47.301300
2415.347223	186.368693	47.306305
2411.107788	189.345168	47.311309
2407.616212	194.164889	47.316314
2404.424288	185.546748	47.321319
2400.795053	191.031937	47.326324
2397.567666	182.255273	47.331329
2394.049170	194.898485	47.336333
2390.556670	189.943286	47.341338
2387.328704	186.842838	47.346343
2383.808885	193.443699	47.351348
2380.525257	189.151034	47.356353
2376.654563	190.849070	47.361357
2373.048907	191.122759	47.366362
2369.845103	180.761720	47.371367
2365.968530	192.671542	47.376372
2362.595098	180.390759	47.381377
2359.091577	188.491495	47.386381
2355.475071	190.098643	47.391386
2352.403961	191.878413	47.396391
2348.687171	182.011168	47.401396
2345.606275	182.603184	47.406401
2341.681102	187.914868	47.411405
2337.940477	191.666301	47.416410
2334.768724	184.953957	47.421415
2331.057339	182.639840	47.426420
2327.693140	185.238431	47.431425
2324.101165	183.605362	47.436429
2320.692430	177.456688	47.441434
2317.279907	170.871536	47.446439
2313.527872	190.831466	47.451444
2310.583994	179.021507	47.456449
2306.722853	181.704130	47.461453
2303.309761	175.356284	47.466458
2300.186701	180.174234	47.471463
2296.427948	181.909895	47.476468
2292.245920	180.934126	47.481473
2289.089614	172.863935	47.486477
2286.035753	170.949249	47.491482
2282.905667	163.593057	47.496487
2279.011593	183.917256	47.501492
2275.440246	170.123265	47.506497
2271.303730	175.153752	47.511501
2267.722550	179.798317	47.516506
2264.731356	177.528937	47.521511
2261.016576	187.159668	47.526516
2257.816399	168.233547	47.531521
2254.344131	179.224562	47.536525
2251.047948	175.322630	47.541530
2247.417510	169.260944	47.546535
2243.526848	182.784253	47.551540
2240.093172	179.942449	47.556545
2236.714068	173.599502	47.561549
2233.551772	176.477008	47.566554
2230.146097	169.574654	47.571559
2226.136095	176.897116	47.576564
2223.023137	172.002325	47.581569
2219.188248	179.296470	47.586573
2215.920885	168.493157	47.591578
2212.529125	170.632624	47.596583
2208.653455	177.460485	47.601588
2205.144242	172.762763	47.606593
2201.675636	176.132121	47.611597
2198.488378	176.900454	47.616602
2195.171244	165.251289	47.621607
2191.265704	177.863993	47.626612
2187.761568	166.334515	47.631617
2184.326441	165.795954	47.636621
2180.791592	171.288988	47.641626
2177.501611	170.435387	47.646631
2173.541556	173.523797	47.651636
2170.164030	164.320791	47.656641
2166.957305	169.818260	47.661645
2163.451486	172.771283	47.666650
2160.064228	174.187185	47.671655
2156.141937	174.981017	47.676660
2152.949301	174.290345	47.681665
2149.339851	168.836436	47.686669
2145.655536	167.114360	47.691674
2141.945574	163.868124	47.696679
2138.762828	172.365363	47.701684
2135.475420	160.860728	47.706689
2132.105451	169.751007	47.711693
2128.493195	175.064058	47.716698
2124.802043	164.365339	47.721703
2121.028266	174.186266	47.726708
2117.808962	160.589644	47.731713
2114.339931	168.367705	47.736717
2110.786533	175.174188	47.741722
2107.739411	166.637155	47.746727
2103.755433	166.611204	47.751732
2099.957361	161.082911	47.756737
2096.852841	162.187727	47.761741
2093.347991	168.346623	47.766746
2089.875549	154.230008	47.771751
2086.324029	164.739471	47.776756
2082.811462	155.440636	47.781761
2079.190166	157.401814	47.786765
2075.774008	157.671069	47.791770
2072.615850	159.883152	47.796775
2068.858385	159.647938	47.801780
2065.491505	164.963724	47.806785
2061.903509	165.137043	47.811789
2057.936362	166.815932	47.816794
2054.747926	156.409003	47.821799
2051.041495	167.558986	47.826804
2048.037000	167.366380	47.831809
2044.531040	161.723387	47.836813
2040.866591	159.559229	47.841818
2037.633233	157.238231	47.846823
2033.775319	169.475524	47.851828
2030.298638	157.644657	47.856833
2026.828499	158.114873	47.861837
2023.224427	164.277374	47.866842
2019.778942	148.695664	47.871847
2016.371142	165.813033	47.876852
2012.981862	159.002868	47.881857
2009.399168	155.636262	47.886861
2005.380520	162.285410	47.891866
2002.275687	156.701116	47.896871
1998.424548	150.665043	47.901876
1995.223306	162.473418	47.906881
1992.217607	159.788844	47.911885
1988.385679	158.499372	47.916890
1984.899915	157.622001	47.921895
1981.204734	166.831112	47.926900
1977.905195	162.467372	47.931905
1974.785844	163.470915	47.936909
1970.430649	165.646735	47.941914
1967.139587	164.305438	47.946919
1963.561173	157.523001	47.951924
1959.976541	148.972252	47.956929
1956.814479	161.616617	47.961933
1953.691450	168.765148	47.966938
1950.029238	150.759260	47.971943
1946.159729	164.443443	47.976948
1942.780146	150.956331	47.981953
1939.379168	161.109291	47.986957
1936.052040	159.699379	47.991962
1932.535484	160.707187	47.996967
1928.597230	164.979778	48.001972
1925.266548	169.104455	48.006977
1921.395903	159.590597	48.011981
1918.236506	158.940575	48.016986
1914.646839	158.275390	48.021991
1911.019145	161.881588	48.026996
1907.640225	155.576959	48.032001
1904.342318	154.228945	48.037005
1900.723454	164.859370	48.042010
1897.402001	156.901813	48.047015
1893.745975	164.953828	48.052020
1890.278527	154.379597	48.057025
1886.994266	160.077711	48.062029
1883.348339	152.734211	48.067034
1880.092779	154.993094	48.072039
1876.224256	159.817412	48.077044
1872.571979	157.496269	48.082049
1869.065334	157.969867	48.087053
1865.582852	157.900739	48.092058
1862.590801	153.135818	48.097063
1858.800933	152.843764	48.102068
1855.274196	155.822558	48.107073
1851.701393	157.685710	48.112077
1847.944187	152.955438	48.117082
1845.164808	157.711550	48.122087
1841.252140	160.000471	48.127092
1837.648983	148.816432	48.132097
1834.439563	150.945570	48.137101
1831.008932	154.205106	48.142106
1827.558409	149.777621	48.147111
1823.650419	153.415978	48.152116
1819.985600	151.122209	48.157121
1816.665813	152.236718	48.162125
1813.108189	160.422311	48.167130
1809.712081	145.300526	48.172135
1805.914514	152.000525	48.177140
1802.704245	150.875307	48.182145
1799.217545	147.532675	48.187149
1795.632608	153.687828	48.192154
1792.325548	150.885437	48.197159
1788.508512	152.942515	48.202164
1784.996470	149.847005	48.207169
1781.641030	146.646493	48.212173
1778.494510	147.872119	48.217178
1775.295631	143.709964	48.222183
1771.143586	152.340511	48.227188
1767.862693	153.840939	48.232193
1764.234547	153.819435	48.237197
1760.521892	153.520821	48.242202
1757.381768	149.761410	48.247207
1753.570575	153.427244	48.252212
1749.958067	148.129283	48.257217
1746.915570	149.585206	48.262221
1742.914197	155.016093	48.267226
1739.765061	148.574965	48.272231
1736.071371	154.349699	48.277236
1732.378800	152.475195	48.282241
1728.897306	153.867696	48.287245
1725.646732	157.415666	48.292250
1722.392906	151.604583	48.297255
1718.762773	155.865897	48.302260
1715.577229	147.019320	48.307265
1711.835951	154.013596	48.312269
1707.747868	150.107932	48.317274
1704.449627	148.214869	48.322279
1700.995458	145.240896	48.327284
1697.518604	146.256722	48.332289
1694.795296	142.938410	48.337293
1690.783585	151.696402	48.342298
1687.384739	146.968822	48.347303
1683.577597	149.337327	48.352308
1679.953860	151.689739	48.357313
1676.464671	147.052874	48.362317
1672.647395	146.780893	48.367322
1669.606509	146.968697	48.372327
1665.940109	144.247287	48.377332
1662.760733	154.668881	48.382337
1659.340387	149.291486	48.387341
1655.691453	147.386351	48.392346
1652.125774	147.299753	48.397351
1648.606165	143.192464	48.402356
1645.135485	146.209112	48.407361
1641.862419	137.960985	48.412365
1637.811088	151.208112	48.417370
1634.609119	133.935588	48.422375
1630.855226	144.753464	48.427380
1627.448853	147.126831	48.432385
1624.020771	143.560735	48.437389
1620.206848	139.476450	48.442394
1617.383891	145.598165	48.447399
1613.740415	132.471886	48.452404
1610.573468	140.395905	48.457409
1606.884392	142.007111	48.462413
1602.924477	146.749451	48.467418
1599.274880	144.708505	48.472423
1595.723143	155.560497	48.477428
1592.624903	156.683150	48.482433
1589.014307	151.788958	48.487437
1585.279031	152.146426	48.492442
1582.230684	150.305103	48.497447
1578.993453	149.720074	48.502452
1575.381451	152.727368	48.507457
1571.433495	155.260724	48.512461
1567.654579	157.466589	48.517466
1564.449060	149.957241	48.522471
1561.156946	151.592671	48.527476
1557.557049	147.556148	48.532481
1554.176299	152.351018	48.537485
1550.616015	148.527986	48.542490
1547.273517	136.690968	48.547495
1543.448820	153.519109	48.552500
1539.867559	143.854385	48.557505
1536.590340	150.265133	48.562509
1532.680540	141.422557	48.567514
1529.767599	141.794145	48.572519
1525.751025	151.564624	48.577524
1522.310021	147.178038	48.582529
1519.153380	142.110214	48.587533
1515.620818	148.802151	48.592538
1512.271406	149.151360	48.597543
1508.443392	147.960112	48.602548
1505.046232	147.074182	48.607553
1501.499639	147.897630	48.612557
1497.750448	151.984009	48.617562
1494.407220	148.861222	48.622567
1491.407875	150.084421	48.627572
1487.590065	141.755551	48.632577
1483.967996	147.362734	48.637581
1480.240127	153.520418	48.642586
1476.983688	139.789782	48.647591
1473.439788	149.208470	48.652596
1470.120868	146.661662	48.657601
1466.628802	143.782740	48.662605
1462.790337	144.596045	48.667610
1459.495456	141.678618	48.672615
1455.786414	148.421867	48.677620
1452.618948	147.431510	48.682625
1449.166750	137.000192	48.687629
1445.093801	149.675593	48.692634
1441.902931	144.493107	48.697639
1438.273736	147.152477	48.702644
1435.047707	148.807659	48.707649
1431.834366	143.161203	48.712653
1427.778410	145.819485	48.717658
1424.557124	134.292685	48.722663
1420.883899	138.337752	48.727668
1417.362628	143.803012	48.732673
1414.040650	148.746922	48.737677
1410.281989	144.983435	48.742682
1407.037054	140.462510	48.747687
1403.670720	147.615263	48.752692
1399.739413	144.544959	48.757697
1396.531846	140.929962	48.762701
1392.652891	138.466707	48.767706
1389.304848	137.632539	48.772711
1385.962877	144.597751	48.777716
1382.151729	144.141275	48.782721
1379.421750	141.153028	48.787725
1375.374063	142.573665	48.792730
1371.804237	131.927029	48.797735
1368.051100	151.721481	48.802740
1364.515046	141.475187	48.807745
1361.308248	140.868903	48.812749
1357.916249	139.917503	48.817754
1354.766295	136.257889	48.822759
1351.095157	131.657880	48.827764
1347.537089	132.580432	48.832769
1344.222072	132.235368	48.837773
1339.822393	138.108148	48.842778
1336.800757	140.319847	48.847783
1333.423891	136.294991	48.852788
1330.007899	138.620430	48.857793
1326.391762	136.671266	48.862797
1322.635737	142.081269	48.867802
1319.466620	128.486123	48.872807
1315.471637	136.268165	48.877812
1312.393537	133.653054	48.882817
1309.061256	124.406395	48.887821
1305.283068	140.615834	48.892826
1301.809611	134.195897	48.897831
1298.431823	136.111289	48.902836
1294.820827	138.683694	48.907841
1291.436588	135.287822	48.912845
1287.748432	147.664501	48.917850
1284.126077	130.608015	48.922855
1280.228802	140.126293	48.927860
1277.612282	141.992810	48.932865
1274.136956	131.258809	48.937869
1270.436121	136.437918	48.942874
1266.837935	131.962873	48.947879
1263.032041	137.364390	48.952884
1259.664345	136.360897	48.957889
1256.307871	132.043238	48.962893
1252.579833	140.713422	48.967898
1249.443666	133.375993	48.972903
1245.767101	135.293852	48.977908
1241.888156	141.068395	48.982913
1238.459196	134.649442	48.987917
1234.968119	146.123906	48.992922
1231.844677	138.473181	48.997927
1228.293937	139.450264	49.002932
1225.123070	137.566492	49.007937
1221.867906	132.728109	49.012941
1217.757677	137.974944	49.017946
1214.164646	134.296927	49.022951
1210.502033	142.875615	49.027956
1206.816191	148.246478	49.032961
1203.748865	129.655766	49.037965
1200.006000	140.020413	49.042970
1196.846276	130.943244	49.047975
1193.410957	142.068500	49.052980
1189.599277	140.600721	49.057985
1186.400290	131.955512	49.062989
1182.498319	146.033734	49.067994
1179.757004	124.648323	49.072999
1175.996166	135.915223	49.078004
1172.066422	138.070958	49.083009
1169.024192	140.172898	49.088013
1165.150925	133.123369	49.093018
1161.673222	124.739168	49.098023
1158.086724	134.667920	49.103028
1154.300275	140.494334	49.108033
1151.196963	132.307929	49.113037
1147.703642	142.054536	49.118042
1144.480691	133.002465	49.123047
1141.012436	132.057919	49.128052
1137.411854	137.432297	49.133057
1133.681369	131.634581	49.138061
1129.887515	139.423181	49.143066
1126.741024	131.478373	49.148071
1122.850799	130.143622	49.153076
1119.383944	132.542745	49.158081
1116.269994	132.561051	49.163085
1112.686664	131.039597	49.168090
1109.057442	124.659593	49.173095
1105.570039	140.278206	49.178100
1102.122167	138.536036	49.183105
1098.705907	136.091251	49.188109
1095.288849	143.234045	49.193114
1091.655217	130.657005	49.198119
1088.173469	137.017399	49.203124
1084.439060	146.372735	49.208129
1081.326946	138.513641	49.213133
1077.515510	137.673453	49.218138
1074.287089	131.936824	49.223143
1070.430837	126.190749	49.228148
1067.038390	135.357721	49.233153
1063.718728	131.563188	49.238157
1059.950484	132.703651	49.243162
1056.517743	136.300148	49.248167
1053.302979	131.500998	49.253172
1049.302955	131.863415	49.258177
1046.037670	133.916676	49.263181
1042.571975	141.334743	49.268186
1038.870994	134.194877	49.273191
1035.691719	129.294163	49.278196
1031.993481	127.213777	49.283201
1028.861536	129.515352	49.288205
1025.033878	136.572566	49.293210
1021.785304	133.425612	49.298215
1017.814615	121.268083	49.303220
1014.366011	132.224554	49.308225
1011.297401	133.176733	49.313229
1007.473059	144.140495	49.318234
1004.221839	133.925765	49.323239
1000.518983	131.488989	49.328244
996.936877	131.266695	49.333249
993.642790	122.365838	49.338253
990.063400	126.433011	49.343258
986.538556	131.490482	49.348263
982.970938	131.832753	49.353268
979.414530	128.872512	49.358273
975.580319	119.054582	49.363277
972.501136	127.573845	49.368282
969.335288	128.074249	49.373287
965.680249	126.410655	49.378292
961.897396	119.533840	49.383297
958.516142	121.802693	49.388301
954.748123	131.868168	49.393306
951.391776	132.258995	49.398311
948.328586	127.944974	49.403316
944.541637	129.284582	49.408321
941.277225	123.638868	49.413325
937.149242	136.900368	49.418330
933.856593	133.298213	49.423335
930.769101	128.051860	49.428340
926.798161	126.775034	49.433345
923.533867	123.377970	49.438349
919.886522	130.606921	49.443354
916.643429	123.217385	49.448359
912.979764	125.044771	49.453364
909.097524	129.828110	49.458369
905.878035	119.569152	49.463373
902.416528	130.433107	49.468378
899.105334	129.587490	49.473383
895.542622	129.758915	49.478388
891.637878	127.643343	49.483393
888.825194	117.316718	49.488397
884.975958	137.436376	49.493402
881.332307	118.929253	49.498407
877.686897	126.961075	49.503412
874.633089	131.410274	49.508417
871.223843	122.130934	49.513421
867.148369	130.394731	49.518426
863.896668	123.082045	49.523431
860.313617	126.261907	49.528436
856.679443	132.536774	49.533441
853.620418	126.504712	49.538445
849.830373	128.406137	49.543450
846.940545	128.609957	49.548455
843.116248	122.604245	49.553460
839.093718	127.871628	49.558465
835.973121	121.389577	49.563469
832.639264	136.402784	49.568474
828.725318	124.514502	49.573479
825.348273	128.783752	49.578484
821.605307	131.372039	49.583489
818.318410	131.649455	49.588493
814.699613	132.153065	49.593498
811.582108	129.028400	49.598503
807.935875	131.356197	49.603508
803.888977	122.781710	49.608513
800.893627	119.710455	49.613517
797.154973	126.986766	49.618522
793.820754	127.460880	49.623527
790.418540	135.265858	49.628532
786.848925	136.090118	49.633537
783.698127	125.279586	49.638541
779.924118	126.358286	49.643546
776.434299	129.815638	49.648551
772.995545	119.058677	49.653556
768.933129	118.379864	49.658561
766.009938	127.363629	49.663565
762.064931	127.905856	49.668570
758.847967	114.557894	49.673575
755.611450	124.029613	49.678580
751.613351	129.496484	49.683585
748.044611	118.487739	49.688589
744.505364	120.968581	49.693594
741.518587	118.964527	49.698599
737.786996	122.276409	49.703604
734.496381	125.445483	49.708609
731.281205	123.152827	49.713613
727.336596	122.680118	49.718618
723.668984	124.139291	49.723623
720.217795	128.669922	49.728628
716.559634	125.660430	49.733633
713.634335	118.156522	49.738637
709.482077	136.862784	49.743642
706.227319	125.482638	49.748647
702.778771	123.969613	49.753652
699.082919	129.712128	49.758657
695.848838	116.162611	49.763661
691.919767	128.000562	49.768666
688.558713	133.376495	49.773671
685.079380	123.074278	49.778676
681.537550	132.530652	49.783681
678.819689	121.403883	49.788685
675.231035	125.997350	49.793690
671.171771	117.262047	49.798695
667.646697	120.356491	49.803700
664.103429	112.808051	49.808705
660.838628	119.537982	49.813709
657.271784	125.956767	49.818714
653.602568	119.258971	49.823719
650.109594	119.788074	49.828724
646.666174	124.696359	49.833729
643.148271	119.602548	49.838733
639.398147	117.158713	49.843738
636.362275	117.092805	49.848743
632.769602	111.310440	49.853748
629.214619	127.721573	49.858753
625.947589	117.180634	49.863757
622.133716	125.011806	49.868762
618.647530	117.497175	49.873767
615.222189	120.963121	49.878772
611.649773	122.657054	49.883777
608.583047	122.313488	49.888781
604.550086	131.865983	49.893786
601.064825	121.083127	49.898791
597.743979	116.118959	49.903796
594.211169	120.693183	49.908801
590.714677	116.826266	49.913805
586.834708	121.486160	49.918810
583.327850	107.429348	49.923815
580.347222	112.165784	49.928820
576.413899	121.578869	49.933825
573.531241	113.945664	49.938829
569.685763	118.687678	49.943834
566.112310	117.928340	49.948839
562.636612	113.379368	49.953844
559.062041	123.668672	49.958849
555.815493	123.199005	49.963853
552.162215	119.485544	49.968858
548.641056	113.263397	49.973863
545.251093	121.460788	49.978868
541.351168	123.775330	49.983873
538.118169	112.894945	49.988877
534.651266	122.469064	49.993882
531.282964	122.292084	49.998887
527.645641	123.065992	50.003892
523.838911	124.632812	50.008897
520.755190	122.439135	50.013901
517.119803	124.620724	50.018906
513.805100	127.371446	50.023911
510.296735	114.002466	50.028916
506.557852	124.357481	50.033921
502.790484	121.290473	50.038925
499.523593	130.342915	50.043930
495.938884	116.321164	50.048935
492.776777	117.847042	50.053940
488.663390	126.011066	50.058945
485.338516	116.651209	50.063949
482.063941	121.989490	50.068954
478.636484	113.539563	50.073959
475.571112	116.160444	50.078964
471.396266	115.407375	50.083969
468.154732	120.570686	50.088973
464.313379	120.535395	50.093978
460.697229	114.428305	50.098983
457.598760	115.314569	50.103988
454.089980	118.725377	50.108993
450.570971	114.363442	50.113997
446.888207	120.111683	50.119002
443.614876	119.547470	50.124007
440.310773	123.429792	50.129012
436.753781	123.886385	50.134017
433.414381	114.360060	50.139021
429.507521	121.565432	50.144026
425.785126	115.995938	50.149031
422.429999	119.574137	50.154036
418.672635	113.585574	50.159041
415.438773	116.152094	50.164045
411.854255	116.027769	50.169050
408.375673	115.280487	50.174055
405.143251	108.754141	50.179060
401.505783	116.183717	50.184065
398.213811	113.636442	50.189069
394.574538	110.735407	50.194074
390.873359	121.549782	50.199079
387.321274	113.400386	50.204084
383.998628	116.442798	50.209089
380.468411	109.149583	50.214093
377.058640	108.347721	50.219098
373.433613	113.672846	50.224103
369.872572	108.276008	50.229108
366.156684	117.855342	50.234113
362.927537	116.055859	50.239117
359.485283	114.103790	50.244122
356.006898	112.105213	50.249127
352.718477	111.584023	50.254132
348.674360	117.004785	50.259137
345.317649	107.502127	50.264141
341.750526	112.045518	50.269146
338.281623	114.309018	50.274151
335.224362	108.433161	50.279156
331.472390	112.212883	50.284161
328.037409	106.919142	50.289165
324.705472	108.818985	50.294170
320.975074	111.462044	50.299175
317.598272	106.821729	50.304180
313.806941	112.581335	50.309185
309.959340	103.563522	50.314189
306.621771	119.648782	50.319194
303.385986	110.089240	50.324199
299.794352	104.136703	50.329204
296.419258	102.823395	50.334209
292.996466	102.048819	50.339213
289.277916	113.703828	50.344218
285.505389	112.398895	50.349223
282.521875	108.677417	50.354228
278.716703	115.948171	50.359233
275.489237	108.823777	50.364237
272.104050	109.933069	50.369242
268.148549	113.702335	50.374247
264.615379	118.506373	50.379252
261.072108	120.969714	50.384257
257.580462	119.063202	50.389261
254.318822	119.858420	50.394266
251.038455	107.375874	50.399271
247.570213	112.384665	50.404276
243.734046	101.901193	50.409281
240.090480	113.043382	50.414285
236.447798	113.686799	50.419290
233.097282	117.012969	50.424295
230.103787	113.011386	50.429300
226.458473	114.128062	50.434305
222.937427	108.265732	50.439309
219.739782	112.411790	50.444314
215.668244	120.326990	50.449319
212.107201	110.800655	50.454324
208.603136	114.359862	50.459329
205.296859	110.171702	50.464333
201.491155	116.537628	50.469338
198.362829	110.122486	50.474343
194.895016	109.387805	50.479348
191.182561	111.684838	50.484353
188.177822	102.813538	50.489357
184.306253	111.066840	50.494362
180.386814	117.638689	50.499367
177.469250	108.232193	50.504372
173.516814	112.599552	50.509377
170.439368	108.689862	50.514381
166.799466	114.733348	50.519386
163.400611	105.610400	50.524391
160.101753	105.900557	50.529396
156.176072	104.872505	50.534401
152.742034	101.424831	50.539405
148.850006	105.930407	50.544410
145.646992	103.694999	50.549415
142.185853	104.867881	50.554420
138.675290	105.907460	50.559425
135.367490	104.811062	50.564429
131.504993	107.371962	50.569434
128.030063	108.459522	50.574439
124.832260	100.202775	50.579444
121.387089	112.345842	50.584449
118.186825	104.810765	50.589453
114.287220	106.015423	50.594458
110.490801	101.238354	50.599463
107.186630	101.227904	50.604468
103.421058	108.122632	50.609473
100.317079	105.750881	50.614477
96.721370	106.077020	50.619482
92.845650	110.190604	50.624487
89.763104	107.597058	50.629492
85.934511	107.660044	50.634497
82.449321	96.306984	50.639501
79.193635	105.473082	50.644506
75.599299	111.107912	50.649511
72.319546	104.210799	50.654516
68.804593	101.952119	50.659521
65.087173	101.727353	50.664525
61.531888	100.092621	50.669530
58.078895	111.016312	50.674535
55.020002	106.775077	50.679540
50.732637	107.234538	50.684545
47.806712	101.739329	50.689549
44.297453	113.351773	50.694554
40.579044	110.329772	50.699559
37.137258	109.712273	50.704564
33.302575	111.860763	50.709569
29.933452	102.325320	50.714573
26.706181	109.581089	50.719578
23.141943	118.901338	50.724583
19.869503	108.536277	50.729588
15.938414	115.513350	50.734593
12.726666	109.236495	50.739597
8.991995	108.589181	50.744602
5.492308	113.943768	50.749607
2.153558	103.312058	50.754612