Tue Jun 21 12:36:36 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
-0.144605	91.015434	0.000000
0.131382	83.952827	0.005005
0.030849	92.795960	0.010010
0.382896	82.684570	0.015014
-0.120237	88.136475	0.020019
0.129052	87.003651	0.025024
0.100989	84.493379	0.030029
-0.172314	65.195440	0.035034
0.050822	58.297687	0.040038
-0.679199	58.792823	0.045043
-0.982309	49.179674	0.050048
-1.180542	27.695718	0.055053
-1.666179	31.897163	0.060058
-1.672015	13.290266	0.065062
-2.632642	8.083549	0.070067
-2.673894	-8.004415	0.075072
-2.668168	-5.451762	0.080077
-3.297003	13.072364	0.085082
-3.721146	-1.734262	0.090086
-4.181470	7.595034	0.095091
-4.216542	2.919609	0.100096
-4.280986	5.672140	0.105101
-4.493960	3.012927	0.110106
-4.741237	-0.410009	0.115110
-5.442382	5.908390	0.120115
-5.495047	5.835129	0.125120
-5.579856	7.480439	0.130125
-5.902765	4.545600	0.135130
-5.797759	8.816378	0.140134
-5.780535	9.609283	0.145139
-6.694096	10.476000	0.150144
-6.966340	8.767487	0.155149
-7.627626	7.126946	0.160154
-7.248811	0.542262	0.165158
-7.443238	7.504915	0.170163
-7.818726	4.014014	0.175168
-8.282654	3.798101	0.180173
-8.967700	14.191338	0.185178
-8.907396	3.727721	0.190182
-9.156711	14.907799	0.195187
-8.950348	10.074980	0.200192
-8.987805	12.851460	0.205197
-8.972826	5.537291	0.210202
-9.868714	6.502906	0.215206
-10.505625	9.176578	0.220211
-10.607229	10.064541	0.225216
-10.371028	9.560029	0.230221
-10.907072	18.900488	0.235226
-11.064356	-0.364876	0.240230
-11.852619	9.182511	0.245235
-11.877260	9.801789	0.250240
-12.298948	6.968554	0.255245
-12.277095	15.449201	0.260250
-12.097952	8.383523	0.265254
-12.275724	5.460566	0.270259
-12.844068	2.702530	0.275264
-13.668065	1.523462	0.280269
-13.880040	-0.713425	0.285274
-13.661463	2.466432	0.290278
-13.755133	6.358075	0.295283
-14.300882	4.848575	0.300288
-14.065921	10.370041	0.305293
-14.145276	11.748246	0.310298
-14.419459	2.770094	0.315302
-15.157883	7.142250	0.320307
-15.283138	13.505398	0.325312
-15.504004	4.607216	0.330317
-16.365523	15.235494	0.335322
-16.463959	6.852996	0.340326
-16.526699	12.462239	0.345331
-16.821066	5.626128	0.350336
-16.545296	1.087489	0.355341
-16.936863	17.197226	0.360346
-16.856916	1.255932	0.365350
-17.787560	3.168386	0.370355
-17.607875	0.387520	0.375360
-17.721564	5.208365	0.380365
-18.240051	7.797899	0.385370
-19.018106	-2.225363	0.390374
-19.717589	6.137331	0.395379
-19.877953	5.296518	0.400384
-19.105937	6.644843	0.405389
-19.391051	11.044748	0.410394
-19.694716	6.477933	0.415398
-19.927013	9.795795	0.420403
-20.297307	6.787897	0.425408
-20.911183	13.612020	0.430413
-21.320013	13.384616	0.435418
-21.405127	2.080761	0.440422
-21.736080	10.101825	0.445427
-21.651810	13.495929	0.450432
-21.547105	2.546822	0.455437
-21.943364	7.564827	0.460442
-22.108146	0.315752	0.465446
-22.905144	6.237992	0.470451
-22.918806	8.760903	0.475456
-23.076379	0.498314	0.480461
-23.514351	6.720447	0.485466
-23.374126	2.994967	0.490470
-23.904280	6.349522	0.495475
-24.576875	13.633683	0.500480
-24.707994	11.953306	0.505485
-25.061389	14.356650	0.510490
-24.717952	17.532607	0.515494
-25.004373	14.338745	0.520499
-25.154802	12.833837	0.525504
-25.649106	7.899188	0.530509
-26.445513	10.393848	0.535514
-26.402247	8.478381	0.540518
-26.735290	11.690580	0.545523
-26.502239	3.141502	0.550528
-26.046782	1.175936	0.555533
-27.161803	9.592642	0.560538
-27.650317	7.080290	0.565542
-27.976190	5.824857	0.570547
-28.180441	19.077763	0.575552
-27.742234	17.993382	0.580557
-28.173533	17.639460	0.585562
-28.470966	11.005728	0.590566
-29.532579	20.020792	0.595571
-29.689810	12.528135	0.600576
-29.607199	5.327287	0.605581
-29.809020	14.261738	0.610586
-29.425099	13.928518	0.615590
-29.877473	13.234923	0.620595
-30.129590	13.685656	0.625600
-30.136138	7.667784	0.630605
-30.856066	17.996353	0.635610
-31.123908	10.956542	0.640614
-31.672108	8.452495	0.645619
-32.449981	11.351778	0.650624
-32.041492	3.825831	0.655629
-32.463233	9.778878	0.660634
-32.557155	9.592866	0.665638
-32.662426	6.147600	0.670643
-32.606050	6.098513	0.675648
-32.681766	-6.014183	0.680653
-33.670574	3.943713	0.685658
-33.821017	3.428633	0.690662
-34.003607	3.367612	0.695667
-34.031288	10.514590	0.700672
-34.011857	4.761581	0.705677
-34.598172	11.766633	0.710682
-35.176667	9.482301	0.715686
-35.296439	2.766072	0.720691
-35.627940	5.586111	0.725696
-35.695802	12.894058	0.730701
-36.220074	10.270411	0.735706
-35.918104	9.769411	0.740710
-36.223611	3.884717	0.745715
-37.150078	3.784276	0.750720
-37.060105	1.082003	0.755725
-37.553154	13.473021	0.760730
-37.274949	3.917564	0.765734
-37.276608	2.955750	0.770739
-37.921818	5.897593	0.775744
-38.382205	-0.197068	0.780749
-38.962396	1.705507	0.785754
-39.019416	6.011005	0.790758
-38.968041	-1.804294	0.795763
-39.286044	-3.766692	0.800768
-39.106133	1.384610	0.805773
-39.251702	-1.073826	0.810778
-39.367010	1.108545	0.815782
-40.270739	7.166467	0.820787
-40.250124	0.578741	0.825792
-40.296796	0.709913	0.830797
-41.523403	2.580016	0.835802
-41.741962	1.744302	0.840806
-41.926174	5.111822	0.845811
-42.319838	5.949088	0.850816
-42.209522	2.779516	0.855821
-42.411102	8.175343	0.860826
-42.228867	-0.745381	0.865830
-42.178409	9.445151	0.870835
-42.386459	16.974240	0.875840
-42.930763	4.149406	0.880845
-43.741136	5.239789	0.885850
-43.372676	3.997843	0.890854
-43.579259	0.040898	0.895859
-44.641365	14.099685	0.900864
-44.904624	4.624025	0.905869
-45.645973	5.000867	0.910874
-44.400789	7.933958	0.915878
-44.987285	6.639396	0.920883
-45.396264	11.838688	0.925888
-45.193982	11.525087	0.930893
-46.169244	8.418460	0.935898
-46.530881	2.925494	0.940902
-46.908180	13.177194	0.945907
-47.199901	18.390618	0.950912
-47.047780	6.837712	0.955917
-46.933194	8.696670	0.960922
-47.022448	2.727426	0.965926
-47.203559	10.991261	0.970931
-48.197385	1.198898	0.975936
-48.396487	7.644127	0.980941
-49.153843	15.362450	0.985946
-48.585674	3.900885	0.990950
-48.718467	0.631662	0.995955
-49.017491	1.896664	1.000960
-49.632112	-3.734176	1.005965
-50.368297	5.467542	1.010970
-50.376570	4.620883	1.015974
-50.414690	5.859849	1.020979
-50.789950	13.673355	1.025984
-50.560133	11.253198	1.030989
-50.598995	1.154302	1.035994
-50.665942	3.569017	1.040998
-51.309535	3.500077	1.046003
-51.893160	5.879783	1.051008
-52.036066	8.670368	1.056013
-52.338630	6.360474	1.061018
-52.275942	5.044250	1.066022
-52.730566	0.502834	1.071027
-53.353759	6.283816	1.076032
-53.119872	-1.988142	1.081037
-53.722207	1.588922	1.086042
-53.674668	3.095099	1.091046
-53.716570	12.300250	1.096051
-54.396626	5.824014	1.101056
-54.617621	11.261733	1.106061
-55.311911	14.216049	1.111066
-55.112558	1.386670	1.116070
-55.123273	2.963076	1.121075
-55.399574	5.605057	1.126080
-55.264590	3.709330	1.131085
-55.779810	13.025619	1.136090
-56.034722	2.113770	1.141094
-56.458014	11.145869	1.146099
-56.685042	14.544162	1.151104
-56.604218	7.795109	1.156109
-58.006072	15.589968	1.161114
-58.150111	9.240851	1.166118
-57.878196	7.247461	1.171123
-58.150991	11.932447	1.176128
-58.273405	4.772065	1.181133
-58.569973	10.649131	1.186138
-58.283358	6.193350	1.191142
-58.396669	8.564831	1.196147
-59.110439	6.868463	1.201152
-59.299210	5.029507	1.206157
-59.970854	10.444766	1.211162
-59.891600	7.350193	1.216166
-60.115480	7.903601	1.221171
-61.028830	-1.328632	1.226176
-61.318115	-0.407615	1.231181
-61.284333	6.281826	1.236186
-61.856138	1.667661	1.241190
-61.632766	5.476806	1.246195
-61.853341	1.664654	1.251200
-61.379365	-5.178310	1.256205
-61.804616	9.078115	1.261210
-62.430951	3.054943	1.266214
-62.887675	5.571501	1.271219
-63.172399	11.407337	1.276224
-62.951324	9.109001	1.281229
-62.955187	7.013478	1.286234
-63.830531	4.124545	1.291238
-64.328367	6.311458	1.296243
-64.629714	9.539326	1.301248
-64.470177	5.259694	1.306253
-64.841938	2.707293	1.311258
-64.625130	9.105551	1.316262
-65.121006	14.078291	1.321267
-65.988097	13.718001	1.326272
-65.692859	9.597639	1.331277
-66.043761	13.466168	1.336282
-66.309169	6.019850	1.341286
-66.174052	9.022506	1.346291
-66.757467	6.049709	1.351296
-66.993315	7.497243	1.356301
-67.576999	9.409281	1.361306
-67.780829	2.603375	1.366310
-68.087730	4.031693	1.371315
-68.302063	5.792384	1.376320
-67.780204	-2.376895	1.381325
-68.252909	5.524969	1.386330
-68.998293	-1.248085	1.391334
-69.186729	2.812972	1.396339
-69.456690	11.218997	1.401344
-69.040144	-2.577759	1.406349
-69.678573	8.165916	1.411354
-69.891308	3.673837	1.416358
-70.410808	-2.823850	1.421363
-70.628110	3.760156	1.426368
-70.522228	-2.624028	1.431373
-70.993614	8.081329	1.436378
-71.220663	7.068041	1.441382
-71.931670	9.254737	1.446387
-72.635149	-3.154977	1.451392
-72.016524	0.515303	1.456397
-72.283575	5.157501	1.461402
-72.495552	-2.714429	1.466406
-72.371298	2.362221	1.471411
-72.883598	5.416442	1.476416
-72.771947	-4.599826	1.481421
-73.676781	7.876941	1.486426
-74.084066	7.418210	1.491430
-74.182210	5.038551	1.496435
-74.116468	7.709138	1.501440
-74.213672	-2.804752	1.506445
-75.118578	4.360408	1.511450
-75.567270	4.662348	1.516454
-75.567352	8.022662	1.521459
-75.864244	11.240518	1.526464
-75.756295	2.679008	1.531469
-75.969696	9.431683	1.536474
-75.991969	1.684426	1.541478
-75.921744	5.230825	1.546483
-76.980583	10.491363	1.551488
-76.865266	3.224718	1.556493
-77.590338	5.351781	1.561498
-77.548385	8.282052	1.566502
-77.670340	10.031589	1.571507
-78.168412	1.775271	1.576512
-78.578679	-2.133732	1.581517
-79.266614	15.620912	1.586522
-78.918672	3.178366	1.591526
-79.183774	-0.228191	1.596531
-79.360002	10.592667	1.601536
-79.122727	0.329842	1.606541
-79.075324	3.627828	1.611546
-79.885578	0.647016	1.616550
-80.289154	6.732623	1.621555
-80.581370	4.476667	1.626560
-80.505121	3.365002	1.631565
-81.595459	13.585206	1.636570
-81.733586	5.657235	1.641574
-82.046359	7.714837	1.646579
-82.371356	17.751072	1.651584
-81.700592	3.391055	1.656589
-81.881285	5.006660	1.661594
-82.124511	8.398754	1.666598
-82.282360	0.321711	1.671603
-83.131961	12.892147	1.676608
-83.461918	8.402313	1.681613
-83.872288	8.502744	1.686618
-83.933217	0.222184	1.691622
-84.038815	1.476271	1.696627
-84.451387	6.832051	1.701632
-84.081246	6.103087	1.706637
-84.980866	0.546485	1.711642
-85.020855	2.711647	1.716646
-85.135632	6.054645	1.721651
-85.455713	2.900110	1.726656
-85.599211	-4.232108	1.731661
-86.543427	4.760752	1.736666
-86.888939	-0.749874	1.741670
-86.811925	1.448008	1.746675
-87.264539	7.100697	1.751680
-86.940746	-8.074063	1.756685
-87.055287	-0.933627	1.761690
-87.057770	6.383022	1.766694
-88.087704	-2.014513	1.771699
-88.697865	-2.684338	1.776704
-88.410271	-5.186089	1.781709
-88.626002	12.148964	1.786714
-88.492215	4.041186	1.791718
-88.701116	-1.750570	1.796723
-89.239318	2.925087	1.801728
-89.505079	0.863466	1.806733
-90.031307	0.818311	1.811738
-89.969029	1.381557	1.816742
-90.334619	-0.533292	1.821747
-90.472665	2.609319	1.826752
-90.569752	4.073143	1.831757
-91.976197	5.513848	1.836762
-91.799919	3.624110	1.841766
-91.682590	7.351555	1.846771
-92.191971	3.194540	1.851776
-91.852253	-8.328245	1.856781
-92.187856	5.346588	1.861786
-92.099350	8.977180	1.866790
-92.487435	-0.057476	1.871795
-93.415720	-2.366946	1.876800
-93.429238	-2.290401	1.881805
-93.808281	-2.337829	1.886810
-93.838916	6.422041	1.891814
-93.587148	-0.593497	1.896819
-94.517550	3.189651	1.901824
-94.821623	-3.426587	1.906829
-95.192773	3.419697	1.911834
-95.377001	4.022779	1.916838
-95.016312	1.926874	1.921843
-95.123728	2.432185	1.926848
-95.359929	-4.470375	1.931853
-96.329726	2.790782	1.936858
-96.898807	2.537237	1.941862
-96.598570	0.025696	1.946867
-96.503220	-2.244122	1.951872
-96.770813	0.403522	1.956877
-97.571631	-5.564498	1.961882
-98.081631	-1.407762	1.966886
-98.347022	3.338353	1.971891
-98.367733	10.160545	1.976896
-97.943967	-1.902254	1.981901
-98.426427	7.807615	1.986906
-98.360929	-3.859989	1.991910
-99.390299	-7.257584	1.996915
-99.710991	-0.540369	2.006912
-98.811718	-1.346249	2.016909
-98.566046	7.136941	2.026906
-98.353694	4.691048	2.036902
-97.341626	-0.353550	2.046899
-97.249700	4.060134	2.056896
-96.717636	6.281621	2.066893
-95.680845	3.456362	2.076890
-95.459019	1.055927	2.086886
-95.477044	2.532725	2.096883
-94.216244	-2.225269	2.106880
-94.085587	-0.515047	2.116877
-94.075435	2.092611	2.126874
-93.185285	-0.198788	2.136870
-92.558763	0.308214	2.146867
-91.959424	5.860331	2.156864
-91.341339	1.883530	2.166861
-90.914194	3.481425	2.176858
-90.953412	2.521548	2.186854
-90.042501	6.545705	2.196851
-89.422994	8.423338	2.206848
-89.392968	8.107583	2.216845
-88.673624	7.784962	2.226842
-88.097816	3.907633	2.236838
-87.284131	8.438498	2.246835
-86.663101	6.424424	2.256832
-86.540519	6.623069	2.266829
-86.335078	7.634890	2.276826
-85.746760	7.844530	2.286822
-84.931431	4.784070	2.296819
-84.855352	5.709827	2.306816
-83.729377	9.257557	2.316813
-83.517440	2.990026	2.326810
-83.376733	10.918591	2.336806
-82.361237	3.693263	2.346803
-82.247465	-2.267953	2.356800
-81.412058	-1.813917	2.366797
-80.576295	5.143204	2.376794
-80.329258	-4.076143	2.386790
-80.410677	0.359727	2.396787
-80.079745	0.943344	2.406784
-78.902961	3.692711	2.416781
-78.782943	-2.132019	2.426778
-77.698820	-2.928594	2.436774
-77.359700	-0.026873	2.446771
-77.367234	-3.892360	2.456768
-76.155419	-1.726140	2.466765
-75.787711	4.890798	2.476762
-75.524836	0.796576	2.486758
-75.707132	4.836001	2.496755
-74.585553	4.900626	2.506752
-73.996220	4.275102	2.516749
-73.223440	3.705740	2.526746
-72.674227	-2.026267	2.536742
-72.523202	-8.757517	2.546739
-72.326171	-6.495760	2.556736
-71.846400	0.856606	2.566733
-71.048329	-1.548366	2.576730
-69.974389	-0.278876	2.586726
-69.868782	-1.214723	2.596723
-69.697301	-4.704607	2.606720
-69.407526	-0.274685	2.616717
-68.318980	-0.006410	2.626714
-67.838199	1.673495	2.636710
-67.714909	-0.778789	2.646707
-66.872682	8.324433	2.656704
-66.488687	9.810925	2.666701
-66.303975	11.233603	2.676698
-65.135803	5.741706	2.686694
-64.906743	7.476931	2.696691
-64.830701	7.190109	2.706688
-63.945426	4.520157	2.716685
-63.536285	5.668368	2.726682
-63.297387	-0.461958	2.736678
-62.441671	4.554930	2.746675
-62.046768	7.124758	2.756672
-61.196268	4.375603	2.766669
-60.725854	3.877260	2.776666
-60.367485	4.220418	2.786662
-60.083660	3.930801	2.796659
-59.792426	-1.822898	2.806656
-58.837594	2.775291	2.816653
-58.621164	0.303434	2.826650
-58.110685	0.540194	2.836646
-57.489820	-1.064055	2.846643
-57.092716	5.548017	2.856640
-56.340455	6.109483	2.866637
-56.197694	3.602997	2.876634
-55.551448	-0.293106	2.886630
-54.736381	0.142766	2.896627
-54.549228	1.725677	2.906624
-54.151430	4.736829	2.916621
-52.847516	-3.451274	2.926618
-52.737803	-6.752113	2.936614
-52.661233	1.768567	2.946611
-52.418938	3.312313	2.956608
-51.381041	3.699431	2.966605
-51.134824	5.064107	2.976602
-50.035040	3.201933	2.986598
-49.640695	-0.698493	2.996595
-49.911247	2.320197	3.006592
-49.269351	-0.706004	3.016589
-48.296028	1.561761	3.026586
-47.667363	0.672470	3.036582
-47.603964	-4.122551	3.046579
-46.806611	0.811928	3.056576
-46.350091	-0.012302	3.066573
-46.364295	2.385602	3.076570
-45.184150	2.957619	3.086566
-44.718266	-1.169033	3.096563
-44.615966	-8.590089	3.106560
-44.347596	0.500084	3.116557
-43.378220	-3.368120	3.126554
-43.075517	3.619588	3.136550
-41.813803	1.265483	3.146547
-41.847589	2.936155	3.156544
-41.715857	5.958372	3.166541
-41.057820	3.800260	3.176538
-40.138518	3.515863	3.186534
-39.818316	4.797751	3.196531
-39.744269	3.391145	3.206528
-38.898647	0.522275	3.216525
-38.609068	-3.630505	3.226522
-38.014777	1.220039	3.236518
-36.854237	-0.413509	3.246515
-36.874690	1.212870	3.256512
-36.635848	-1.577057	3.266509
-35.800084	1.235117	3.276506
-35.180066	1.037822	3.286502
-34.846043	-3.567874	3.296499
-34.786741	7.450786	3.306496
-33.563730	5.913590	3.316493
-33.244125	0.437938	3.326490
-33.400303	-6.043870	3.336486
-32.345169	-1.518398	3.346483
-31.976019	-1.101151	3.356480
-31.705658	-2.038001	3.366477
-30.988855	-2.620412	3.376474
-30.548134	-2.160878	3.386470
-29.602382	-4.996337	3.396467
-29.103589	4.119109	3.406464
-29.232433	3.575369	3.416461
-28.400224	4.468388	3.426458
-27.678564	11.268175	3.436454
-27.250019	0.747695	3.446451
-27.338260	1.082022	3.456448
-26.405039	-2.899337	3.466445
-25.961924	-6.049698	3.476442
-25.430325	1.055213	3.486438
-24.536248	7.118892	3.496435
-24.172647	4.128502	3.506432
-24.265974	10.247411	3.516429
-23.151128	-1.053171	3.526426
-22.454062	3.203012	3.536422
-22.381652	6.528073	3.546419
-22.584386	3.048387	3.556416
-21.478890	-0.148432	3.566413
-21.036027	1.902502	3.576410
-20.162782	-1.077043	3.586406
-19.345600	3.450295	3.596403
-19.508077	-2.467550	3.606400
-19.317953	-5.648137	3.616397
-18.244947	1.373249	3.626394
-17.797125	2.962592	3.636390
-17.521824	0.335564	3.646387
-16.621699	9.139948	3.656384
-16.300020	3.129086	3.666381
-16.182449	2.037931	3.676378
-14.966795	7.049171	3.686374
-14.285516	3.432387	3.696371
-14.634665	1.604857	3.706368
-14.315991	5.913623	3.716365
-13.024476	-5.427866	3.726362
-12.904617	-5.503807	3.736358
-12.711581	-0.923304	3.746355
-11.885675	-1.558752	3.756352
-11.391629	4.906474	3.766349
-10.604308	5.779070	3.776346
-9.988041	1.163388	3.786342
-9.764444	2.647006	3.796339
-9.690313	7.212821	3.806336
-9.034302	6.070839	3.816333
-8.109979	4.841946	3.826330
-7.978655	5.323078	3.836326
-7.589138	-1.996958	3.846323
-6.920511	-3.359163	3.856320
-6.623073	6.904807	3.866317
-5.943066	0.785807	3.876314
-5.552781	4.471978	3.886310
-4.275012	5.096799	3.896307
-4.005182	4.071124	3.906304
-3.621998	3.800624	3.916301
-3.614263	1.437420	3.926298
-3.137695	5.296616	3.936294
-2.676899	13.853071	3.946291
-2.178777	23.465378	3.956288
-1.836446	39.972779	3.966285
-1.316561	59.180064	3.976282
-0.936436	74.436053	3.986278
-0.367730	91.367391	3.996275
0.023237	117.402384	4.006272
0.000000	133.838664	4.011277
0.587037	136.546490	4.016282
0.759020	152.495366	4.021286
1.043740	171.198354	4.026291
0.656003	170.257044	4.031296
0.625551	182.874705	4.036301
1.080693	176.379331	4.041306
1.633808	188.616203	4.046310
1.573253	187.390820	4.051315
1.521323	168.940752	4.056320
1.279541	172.841372	4.061325
1.496383	184.432986	4.066330
1.362086	192.971161	4.071334
1.632915	195.962239	4.076339
1.920654	198.265763	4.081344
1.600061	191.481665	4.086349
1.589730	172.014346	4.091354
1.528068	169.269072	4.096358
1.235120	177.814564	4.101363
1.298521	175.768066	4.106368
1.280650	199.049650	4.111373
1.743402	198.288773	4.116378
1.722327	210.121480	4.121382
1.652783	206.213024	4.126387
1.630327	204.478124	4.131392
1.396338	221.502879	4.136397
1.763310	209.557656	4.141402
1.502952	214.434229	4.146406
1.580302	218.422323	4.151411
1.832698	213.542944	4.156416
1.421209	210.869599	4.161421
1.715164	205.670958	4.166426
1.484157	212.104585	4.171430
1.655392	218.002343	4.176435
1.620038	206.720683	4.181440
1.647708	208.947884	4.186445
1.863624	203.722895	4.191450
1.488749	214.615867	4.196454
1.451682	212.004845	4.201459
1.586886	212.081629	4.206464
1.511975	212.787581	4.211469
1.674944	227.693331	4.216474
1.987659	241.699704	4.221478
1.694262	244.532024	4.226483
2.085416	247.410835	4.231488
2.188792	251.920925	4.236493
1.913655	228.045865	4.241498
1.960291	226.468442	4.246502
2.137471	224.637138	4.251507
1.406366	211.101857	4.256512
2.003735	236.200123	4.261517
2.133397	245.952047	4.266522
2.148207	250.403589	4.271526
2.111211	240.651140	4.276531
2.041037	216.919761	4.281536
1.816634	221.337694	4.286541
2.086078	225.150123	4.291546
1.937542	234.804247	4.296550
1.934751	244.826549	4.301555
2.239630	243.855403	4.306560
2.341727	250.623825	4.311565
2.300455	234.244541	4.316570
2.104291	225.923491	4.321574
2.040813	218.577221	4.326579
1.972281	216.331744	4.331584
1.916777	222.474844	4.336589
2.317843	243.259889	4.341594
2.009122	250.770439	4.346598
2.024572	247.539564	4.351603
2.181874	240.984156	4.356608
2.216200	246.871246	4.361613
2.103711	247.936852	4.366618
2.100385	250.459868	4.371622
2.203095	250.864086	4.376627
2.281759	245.190374	4.381632
2.252092	252.461327	4.386637
2.361868	243.759662	4.391642
2.133080	249.067329	4.396646
1.892495	243.801686	4.401651
2.033966	237.259755	4.406656
2.193205	251.424950	4.411661
2.368500	240.623038	4.416666
2.192933	240.728391	4.421670
2.346993	248.676173	4.426675
2.314948	244.208167	4.431680
2.277015	247.702678	4.436685
2.576968	237.893844	4.441690
2.433363	241.994308	4.446694
2.356988	248.434708	4.451699
2.394764	243.659925	4.456704
2.145440	243.004129	4.461709
2.563540	240.538553	4.466714
2.500669	242.181045	4.471718
2.603542	252.568491	4.476723
2.647170	249.475427	4.481728
2.362592	247.574552	4.486733
2.479572	246.816858	4.491738
2.673531	246.413463	4.496742
2.549786	246.313489	4.501747
2.452088	244.787197	4.506752
2.435280	252.073386	4.511757
2.940444	257.699388	4.516762
2.611375	256.401638	4.521766
2.188775	256.495798	4.526771
2.611655	261.491122	4.531776
2.809736	274.980541	4.536781
2.553744	274.197973	4.541786
2.603194	275.390295	4.546790
2.601248	282.214242	4.551795
2.793739	284.034880	4.556800
2.799536	282.004616	4.561805
2.395130	279.143603	4.566810
2.873040	279.714210	4.571814
2.849222	281.959024	4.576819
2.632546	279.462192	4.581824
2.440554	281.119754	4.586829
2.823741	284.566446	4.591834
2.800108	283.334349	4.596838
2.400343	290.702518	4.601843
2.668190	287.666844	4.606848
2.820973	283.804239	4.611853
2.741829	281.015663	4.616858
2.605944	277.254139	4.621862
2.732180	281.970616	4.626867
2.794312	278.010541	4.631872
2.855132	276.999292	4.636877
2.865756	282.996685	4.641882
2.791374	290.253353	4.646886
2.518771	284.273901	4.651891
3.224037	296.450934	4.656896
3.029432	301.108653	4.661901
2.779646	285.168382	4.666906
3.297045	294.631959	4.671910
2.832280	288.287282	4.676915
3.197251	283.533692	4.681920
2.719211	284.517944	4.686925
3.405631	293.925708	4.691930
3.278150	285.741651	4.696934
3.119547	286.034033	4.701939
3.155366	280.070016	4.706944
2.900241	277.972645	4.711949
3.076121	273.638135	4.716954
2.780023	271.610698	4.721958
2.552902	283.661694	4.726963
3.337026	299.101663	4.731968
3.035787	305.501767	4.736973
3.352025	310.978114	4.741978
3.143832	311.929526	4.746982
3.253052	319.732426	4.751987
3.250704	309.904140	4.756992
3.107716	312.430361	4.761997
3.179533	310.098286	4.767002
3.237562	311.076854	4.772006
3.369911	313.563601	4.777011
3.448707	307.050371	4.782016
3.255454	319.568607	4.787021
3.537126	312.847927	4.792026
3.358219	309.062933	4.797030
3.360592	314.138166	4.802035
3.164809	293.729712	4.807040
3.693062	306.567148	4.812045
3.411780	294.235660	4.817050
2.973260	295.753284	4.822054
3.118812	304.127568	4.827059
3.156534	314.138667	4.832064
3.312752	314.341821	4.837069
3.356275	315.244448	4.842074
3.596816	313.627805	4.847078
3.454210	317.490331	4.852083
3.601752	304.950087	4.857088
3.499382	322.646799	4.862093
3.524573	321.597045	4.867098
3.498669	313.577705	4.872102
3.362229	318.968378	4.877107
3.528507	302.971233	4.882112
3.243991	312.481172	4.887117
3.137166	319.028864	4.892122
3.574750	316.134196	4.897126
3.441226	319.343019	4.902131
3.418246	314.563869	4.907136
3.211488	321.652238	4.912141
3.778325	318.542382	4.917146
3.390859	321.018311	4.922150
3.298252	314.014265	4.927155
4.035447	307.545937	4.932160
3.760862	317.032922	4.937165
4.030546	312.495003	4.942170
4.196421	314.689270	4.947174
3.728720	322.699393	4.952179
3.693538	310.518362	4.957184
3.616081	325.949073	4.962189
3.440189	327.504515	4.967194
3.556680	317.899075	4.972198
3.364863	322.486679	4.977203
3.480384	320.103359	4.982208
3.525200	320.006061	4.987213
3.736255	334.616037	4.992218
3.997248	343.246908	4.997222
3.909106	333.313425	5.002227
3.674601	325.544901	5.007232
3.442121	334.844952	5.012237
3.794443	344.463571	5.017242
4.190465	342.212589	5.022246
4.156701	355.371841	5.027251
4.055408	333.717682	5.032256
3.817389	326.158128	5.037261
3.617304	321.217477	5.042266
3.797160	329.718508	5.047270
3.979077	345.326321	5.052275
4.317178	347.404457	5.057280
4.101172	342.931757	5.062285
3.725375	333.159375	5.067290
4.035533	331.546791	5.072294
4.149002	343.142026	5.077299
3.967043	326.719041	5.082304
4.025611	333.594758	5.087309
3.701034	336.356479	5.092314
4.061277	341.645578	5.097318
3.861066	359.910093	5.102323
4.162873	350.172910	5.107328
4.332697	356.614424	5.112333
3.940937	348.971780	5.117338
4.146209	360.518279	5.122342
4.023369	356.168285	5.127347
4.123542	351.149292	5.132352
4.055749	356.414551	5.137357
4.210130	348.214376	5.142362
4.403610	353.974511	5.147366
4.062212	353.452950	5.152371
4.218259	341.771463	5.157376
4.114462	353.319799	5.162381
3.997647	358.380642	5.167386
4.088184	355.496269	5.172390
4.048040	356.585227	5.177395
4.182162	356.387102	5.182400
4.028411	363.071642	5.187405
4.014848	359.688467	5.192410
4.045165	352.151957	5.197414
3.910129	357.330865	5.202419
4.502394	356.613264	5.207424
3.991052	368.092733	5.212429
4.242287	377.763829	5.217434
4.651130	381.340880	5.222438
4.166676	387.240910	5.227443
4.382120	383.376588	5.232448
4.390954	393.045601	5.237453
4.521323	386.068539	5.242458
4.634983	388.424202	5.247462
4.244380	392.132841	5.252467
4.207195	384.584010	5.257472
4.280401	391.336558	5.262477
4.300336	386.103506	5.267482
4.634338	384.806262	5.272486
4.427831	395.666152	5.277491
4.360667	385.592801	5.282496
4.249090	386.873956	5.287501
4.728374	385.369724	5.292506
4.644906	386.892897	5.297510
4.527489	394.784670	5.302515
4.795125	387.278508	5.307520
4.172916	399.560975	5.312525
4.324725	397.497441	5.317530
4.441423	387.257875	5.322534
4.325131	390.887348	5.327539
4.561379	377.557211	5.332544
4.666333	382.875178	5.337549
4.697958	394.133530	5.342554
4.793153	389.945156	5.347558
4.405188	396.050626	5.352563
4.847570	388.766542	5.357568
4.539337	384.342649	5.362573
4.434677	397.518807	5.367578
4.707645	394.720057	5.372582
4.815448	410.744160	5.377587
4.973838	399.029089	5.382592
4.741185	395.484845	5.387597
4.399028	390.038830	5.392602
4.708862	399.467575	5.397606
4.459041	401.157616	5.402611
5.019644	402.067180	5.407616
4.692656	414.232496	5.412621
4.706465	414.766093	5.417626
5.166947	411.385321	5.422630
4.983872	419.345996	5.427635
4.833285	403.017195	5.432640
4.966899	414.456604	5.437645
4.973512	416.942875	5.442650
4.913949	405.261718	5.447654
4.756383	419.643119	5.452659
4.937737	408.296617	5.457664
4.922398	407.922744	5.462669
4.987611	408.246741	5.467674
4.884566	413.540944	5.472678
4.366149	417.838300	5.477683
4.923799	414.269950	5.482688
4.799537	421.663406	5.487693
5.199205	421.883083	5.492698
5.084859	419.047226	5.497702
4.605786	421.588068	5.502707
4.584835	414.693870	5.507712
5.133524	425.343482	5.512717
4.903367	439.433809	5.517722
5.320497	438.127730	5.522726
5.047955	442.277026	5.527731
5.443034	442.417344	5.532736
4.905218	454.368164	5.537741
5.266955	451.964381	5.542746
5.384529	453.506172	5.547750
5.349032	441.800677	5.552755
5.161340	425.751113	5.557760
5.193584	422.007497	5.562765
5.036897	417.476211	5.567770
5.266921	425.404204	5.572774
5.192947	441.951589	5.577779
5.349488	434.316584	5.582784
5.272572	446.689954	5.587789
5.115933	449.118801	5.592794
5.334799	441.987936	5.597798
5.182139	447.658206	5.602803
5.469693	445.455561	5.607808
5.194586	455.410015	5.612813
5.356672	444.807093	5.617818
5.501129	439.499333	5.622822
5.325726	455.334952	5.627827
5.563126	441.859327	5.632832
5.346821	445.827036	5.637837
5.815112	445.960559	5.642842
5.777057	439.409986	5.647846
5.260358	428.314036	5.652851
5.498793	418.065145	5.657856
5.296338	419.588685	5.662861
5.349431	432.842749	5.667866
5.589291	429.064359	5.672870
5.376381	440.356329	5.677875
5.613929	435.287131	5.682880
5.429933	450.077284	5.687885
5.375645	446.065007	5.692890
5.484751	436.143000	5.697894
5.175396	454.195996	5.702899
5.840599	446.859005	5.707904
5.359133	445.990228	5.712909
5.338996	449.370736	5.717914
5.431302	443.486499	5.722918
5.032989	448.966165	5.727923
5.109563	443.263126	5.732928
5.379441	448.983216	5.737933
5.655584	462.472700	5.742938
5.531390	462.091985	5.747942
5.239352	478.520013	5.752947
5.480947	472.432257	5.757952
5.278403	478.566060	5.762957
5.630433	476.166841	5.767962
5.911032	477.152178	5.772966
5.677286	484.530245	5.777971
5.550922	477.846668	5.782976
5.471613	481.060362	5.787981
5.734446	475.399090	5.792986
5.985254	472.935920	5.797990
5.658949	477.031571	5.802995
5.959081	473.353701	5.808000
6.028652	475.386134	5.813005
5.922916	473.888382	5.818010
5.934440	477.564398	5.823014
5.603314	480.334925	5.828019
6.084706	477.880935	5.833024
6.057034	474.776346	5.838029
5.935494	475.168762	5.843034
6.096276	481.247537	5.848038
6.096248	474.296368	5.853043
6.234417	478.516594	5.858048
6.052134	476.327212	5.863053
5.662389	479.050019	5.868058
6.113924	480.918169	5.873062
5.940366	470.622415	5.878067
5.829609	477.371124	5.883072
5.972058	477.024601	5.888077
6.115549	480.852227	5.893082
6.245833	466.013929	5.898086
5.939427	486.948616	5.903091
6.215287	476.893789	5.908096
5.953860	474.110694	5.913101
5.437708	480.725443	5.918106
5.620755	484.073497	5.923110
5.968162	504.024153	5.928115
6.235734	511.641873	5.933120
6.059043	516.002456	5.938125
6.247528	515.268233	5.943130
6.443470	511.867502	5.948134
6.084493	525.507989	5.953139
6.335679	512.883714	5.958144
6.171730	510.083879	5.963149
6.147126	514.798171	5.968154
6.102633	506.493495	5.973158
6.028917	516.895163	5.978163
6.366699	516.587535	5.983168
6.157291	514.260160	5.988173
6.357819	511.581131	5.993178
6.500786	509.492208	5.998182
6.010211	516.987017	6.003187
6.161530	515.988198	6.008192
6.299263	514.794880	6.013197
6.116800	517.672818	6.018202
6.312290	518.152062	6.023206
5.987239	514.912982	6.028211
6.148392	519.151121	6.033216
6.398852	520.412202	6.038221
6.309102	517.069038	6.043226
6.562664	507.875918	6.048230
6.291602	512.657462	6.053235
6.488904	513.268624	6.058240
6.228540	512.069196	6.063245
6.310631	510.475612	6.068250
6.244473	507.186956	6.073254
6.156770	510.651285	6.078259
6.751578	502.895329	6.083264
6.725667	511.508876	6.088269
6.333671	502.936329	6.093274
6.523281	508.490351	6.098278
6.124779	509.776203	6.103283
6.443032	506.772200	6.108288
6.221917	511.954757	6.113293
6.023403	510.382179	6.118298
6.367300	509.759966	6.123302
6.209474	517.501212	6.128307
6.171719	504.102275	6.133312
6.352724	510.546541	6.138317
5.894158	517.813253	6.143322
5.865035	514.350330	6.148326
5.854872	524.354496	6.153331
6.198576	532.973554	6.158336
6.453196	548.709645	6.163341
6.466428	542.445955	6.168346
6.391197	536.922338	6.173350
6.339910	551.058137	6.178355
6.519840	542.509467	6.183360
6.685219	544.821464	6.188365
6.217351	543.483128	6.193370
6.594958	533.341362	6.198374
6.232150	531.370324	6.203379
6.344330	521.265412	6.208384
6.244582	524.440465	6.213389
5.944408	526.342118	6.218394
6.342896	533.466528	6.223398
5.827062	539.918838	6.228403
6.233634	537.031239	6.233408
6.205689	545.210006	6.238413
6.039349	551.787583	6.243418
6.117179	536.191828	6.248422
6.277980	549.593528	6.253427
6.166921	544.013481	6.258432
6.404977	544.570337	6.263437
6.177014	548.300628	6.268442
6.389824	542.355354	6.273446
6.317409	545.351042	6.278451
6.425506	544.311819	6.283456
6.340020	548.891946	6.288461
6.316986	550.906965	6.293466
6.458119	543.604215	6.298470
6.105173	548.108449	6.303475
6.231131	551.650090	6.308480
6.065920	551.402463	6.313485
6.119829	554.790663	6.318490
6.627179	544.652271	6.323494
6.303764	553.317866	6.328499
6.579684	537.420729	6.333504
6.619027	545.296094	6.338509
6.324916	555.272900	6.343514
6.616320	552.674725	6.348518
6.490253	550.014839	6.353523
6.324024	552.907264	6.358528
6.513105	557.025344	6.363533
6.180098	561.365646	6.368538
6.631610	550.804123	6.373542
6.597228	559.144796	6.378547
6.762464	548.566936	6.383552
6.594318	552.446380	6.388557
6.634561	552.245050	6.393562
6.306308	531.162002	6.398566
6.048261	523.256770	6.403571
6.615671	546.464459	6.408576
6.690062	526.170019	6.413581
6.222904	526.633085	6.418586
6.196390	524.013751	6.423590
6.222311	525.374766	6.428595
6.296328	522.588610	6.433600
6.437788	528.534438	6.438605
6.161729	537.690861	6.443610
6.452032	533.883768	6.448614
6.322319	545.698803	6.453619
6.398283	545.398020	6.458624
6.446960	527.942826	6.463629
6.151871	533.008381	6.468634
6.407049	526.801529	6.473638
6.032560	533.259046	6.478643
6.540814	533.259458	6.483648
6.813194	542.223441	6.488653
6.497816	527.204507	6.493658
6.565317	521.504915	6.498662
6.113783	521.312593	6.503667
6.310589	517.560650	6.508672
6.192250	523.331236	6.513677
6.247014	526.381246	6.518682
6.479785	520.560156	6.523686
6.294291	524.513311	6.528691
6.381632	512.087655	6.533696
6.308895	519.727589	6.538701
6.219849	523.948153	6.543706
6.281288	528.391660	6.548710
6.066725	517.573595	6.553715
6.350090	527.153819	6.558720
6.227020	540.411885	6.563725
6.304229	561.238355	6.568730
6.379263	546.682840	6.573734
6.162092	555.158368	6.578739
6.176615	547.258707	6.583744
6.346616	549.598554	6.588749
6.331859	548.022778	6.593754
6.397015	550.671457	6.598758
6.092828	556.096501	6.603763
6.311708	553.422123	6.608768
6.566368	558.547622	6.613773
6.161119	561.745838	6.618778
6.435642	550.202054	6.623782
6.589346	548.465969	6.628787
6.608497	545.700932	6.633792
6.602305	543.294712	6.638797
6.674626	533.808739	6.643802
6.524098	529.853422	6.648806
5.826748	528.756938	6.653811
5.986274	521.074628	6.658816
6.255874	538.086202	6.663821
6.369519	544.942433	6.668826
6.524231	551.268521	6.673830
6.313939	552.516897	6.678835
6.470444	551.971692	6.683840
6.361353	537.654867	6.688845
6.070541	531.765756	6.693850
6.449832	538.250216	6.698854
6.362602	549.307340	6.703859
6.410706	542.312058	6.708864
6.365598	538.455911	6.713869
6.761001	532.355096	6.718874
6.458148	523.611088	6.723878
5.972795	521.596997	6.728883
6.067427	524.336106	6.733888
6.657423	532.820251	6.738893
6.094067	526.566790	6.743898
6.102417	520.986121	6.748902
5.947065	538.087005	6.753907
6.426503	539.552309	6.758912
6.230179	548.726518	6.763917
6.387754	553.910519	6.768922
6.447177	543.509240	6.773926
6.292604	546.962153	6.778931
6.014192	549.774286	6.783936
6.177719	546.259919	6.788941
6.205460	547.420532	6.793946
6.122752	545.874953	6.798950
6.242309	554.001476	6.803955
6.533555	545.568761	6.808960
6.606338	555.200449	6.813965
6.543837	550.526637	6.818970
6.657235	543.053439	6.823974
6.386284	557.895389	6.828979
6.409419	548.774146	6.833984
6.579053	552.627852	6.838989
6.378169	561.359202	6.843994
6.218530	545.318091	6.848998
6.407084	557.265738	6.854003
6.600493	543.957550	6.859008
6.668214	538.564384	6.864013
6.014665	528.957062	6.869018
6.368198	526.521079	6.874022
6.134330	527.051289	6.879027
6.070298	536.205165	6.884032
6.343127	545.127634	6.889037
6.167299	555.532619	6.894042
6.577757	546.438809	6.899046
6.276668	559.316887	6.904051
6.735880	552.751022	6.909056
6.391826	543.462062	6.914061
6.104206	535.933510	6.919066
6.732678	545.576584	6.924070
6.354999	542.162095	6.929075
6.612923	535.311258	6.934080
6.458877	532.530698	6.939085
6.349210	523.562887	6.944090
6.720169	522.214322	6.949094
6.579393	521.703740	6.954099
6.405334	515.363523	6.959104
6.273557	520.077407	6.964109
6.301564	526.908737	6.969114
5.911055	519.602069	6.974118
6.044454	526.253735	6.979123
6.256356	526.480034	6.984128
6.259239	520.234446	6.989133
6.227589	526.354377	6.994138
6.477690	516.650912	6.999142
6.197280	520.573209	7.004147
6.370609	523.623912	7.009152
6.109267	517.514036	7.014157
6.382368	528.901424	7.019162
6.461697	519.026527	7.024166
6.113779	524.541881	7.029171
6.309659	534.340843	7.034176
6.333276	526.406139	7.039181
6.518498	546.599792	7.044186
6.439307	520.543983	7.049190
6.236538	529.254710	7.054195
5.972677	520.569370	7.059200
6.239529	528.639126	7.064205
6.364746	547.368585	7.069210
6.713513	543.204292	7.074214
6.377644	538.455175	7.079219
6.663738	531.755574	7.084224
6.311464	513.823313	7.089229
6.586979	519.316739	7.094234
6.372427	517.749382	7.099238
6.519939	529.230582	7.104243
6.527372	529.196702	7.109248
6.580202	530.063464	7.114253
6.207122	529.910643	7.119258
6.194265	528.654641	7.124262
6.365507	523.679869	7.129267
6.237179	523.806606	7.134272
6.381333	521.516593	7.139277
6.151392	529.202888	7.144282
6.453626	523.620326	7.149286
6.316137	532.193750	7.154291
5.970745	525.253173	7.159296
6.174891	526.041795	7.164301
5.819330	526.198068	7.169306
6.440990	532.416044	7.174310
6.302650	548.991961	7.179315
6.432599	550.003827	7.184320
6.238326	541.686241	7.189325
6.534970	554.163606	7.194330
6.445978	537.843211	7.199334
6.261935	526.812682	7.204339
6.218840	521.184685	7.209344
6.694875	523.012077	7.214349
6.288134	524.635168	7.219354
6.273610	524.944743	7.224358
6.366250	518.875121	7.229363
6.414592	523.345462	7.234368
6.415872	519.847507	7.239373
6.425335	524.407761	7.244378
6.409300	511.984028	7.249382
6.082514	526.397889	7.254387
6.127965	524.698478	7.259392
6.237568	519.458822	7.264397
6.460615	536.680968	7.269402
6.450290	521.998315	7.274406
6.267676	513.277029	7.279411
6.343518	521.789666	7.284416
6.450037	514.191125	7.289421
6.188226	523.815245	7.294426
6.201371	522.478567	7.299430
6.430130	537.439436	7.304435
6.243476	542.831002	7.309440
6.410974	540.651973	7.314445
6.178053	544.862621	7.319450
6.637277	537.638434	7.324454
6.301138	538.093619	7.329459
6.245706	539.331547	7.334464
6.577602	535.475335	7.339469
6.305189	539.427493	7.344474
6.213330	516.264823	7.349478
6.323457	529.088600	7.354483
6.442139	541.099704	7.359488
6.500075	531.991850	7.364493
6.117923	527.365449	7.369498
6.479034	517.921457	7.374502
6.169370	526.849985	7.379507
6.345779	526.512638	7.384512
6.578952	523.599288	7.389517
6.440674	530.492491	7.394522
6.375659	524.832206	7.399526
6.455404	532.546555	7.404531
6.361411	530.837672	7.409536
6.640437	527.494223	7.414541
6.329756	520.702023	7.419546
6.422038	519.329942	7.424550
6.495156	523.659819	7.429555
6.469749	519.682208	7.434560
6.385559	529.649696	7.439565
6.188363	526.720185	7.444570
6.496004	512.945344	7.449574
6.643925	525.723983	7.454579
6.577933	533.691773	7.459584
6.360664	531.128494	7.464589
6.562956	531.211735	7.469594
6.736674	523.764473	7.474598
6.782383	531.903805	7.479603
6.021795	511.866244	7.484608
6.270103	505.199750	7.489613
5.983553	534.407053	7.494618
6.276132	523.954551	7.499622
6.338825	514.990569	7.504627
6.378110	526.790236	7.509632
6.449860	531.593958	7.514637
6.445760	533.690894	7.519642
6.391388	528.208030	7.524646
6.325464	531.597715	7.529651
6.575227	531.677240	7.534656
6.599560	509.552492	7.539661
6.462033	508.914285	7.544666
6.498484	501.673092	7.549670
6.388398	497.816072	7.554675
6.077266	501.617549	7.559680
6.341213	495.228297	7.564685
6.103973	501.828051	7.569690
6.391168	496.335410	7.574694
5.990889	501.594399	7.579699
5.877875	524.549249	7.584704
6.238705	521.602921	7.589709
6.009311	531.019009	7.594714
6.195591	523.077699	7.599718
6.079588	530.103378	7.604723
6.278982	531.700500	7.609728
6.374087	527.328381	7.614733
6.241665	539.094130	7.619738
6.079953	522.996946	7.624742
6.261205	527.787074	7.629747
6.528271	523.706765	7.634752
6.364704	527.360082	7.639757
6.197530	530.727262	7.644762
6.377004	527.983437	7.649766
6.530319	530.671191	7.654771
6.321994	517.752789	7.659776
6.341349	525.866683	7.664781
6.094711	525.607280	7.669786
6.221709	519.263586	7.674790
6.481802	528.623881	7.679795
6.268472	522.968421	7.684800
6.304000	518.725363	7.689805
6.426937	524.287470	7.694810
6.511276	520.885681	7.699814
6.405165	522.512273	7.704819
6.289870	526.228837	7.709824
6.380610	523.356437	7.714829
6.180198	527.856918	7.719834
6.597601	526.461786	7.724838
6.439211	521.632571	7.729843
6.356572	519.022136	7.734848
6.683084	525.241817	7.739853
6.442128	532.356467	7.744858
6.272411	519.117506	7.749862
6.343711	523.004458	7.754867
6.571572	523.344546	7.759872
6.560191	531.997929	7.764877
6.278758	522.445623	7.769882
6.333266	531.637096	7.774886
6.081434	532.856038	7.779891
5.999185	527.737542	7.784896
6.268527	527.878157	7.789901
6.195245	525.794649	7.794906
6.696220	519.562098	7.799910
6.108078	520.174848	7.804915
6.629633	525.913285	7.809920
6.408506	525.679456	7.814925
6.113695	534.160527	7.819930
6.431743	521.876833	7.824934
6.243468	531.323213	7.829939
6.296026	527.166530	7.834944
6.565248	525.572151	7.839949
6.183468	527.415090	7.844954
6.468155	531.476681	7.849958
6.238084	530.728683	7.854963
6.428488	524.530386	7.859968
6.567984	529.937604	7.864973
5.945311	529.808549	7.869978
6.445004	528.074970	7.874982
6.561321	524.808587	7.879987
6.232108	530.753219	7.884992
6.585548	522.063544	7.889997
6.560833	518.954312	7.895002
6.784901	518.969220	7.900006
6.499947	528.495741	7.905011
6.286981	519.093919	7.910016
6.416940	512.418009	7.915021
6.135493	526.542561	7.920026
6.224640	520.329853	7.925030
6.050597	530.587903	7.930035
6.583108	530.274277	7.935040
6.677460	521.930025	7.940045
6.497498	520.698339	7.945050
6.686010	492.752923	7.950054
6.470749	491.942286	7.955059
6.232453	488.633789	7.960064
6.405923	485.397617	7.965069
6.330119	492.568575	7.970074
6.183051	480.495134	7.975078
6.080861	488.648079	7.980083
5.888078	491.179416	7.985088
6.232499	502.548266	7.990093
6.126914	515.205673	7.995098
6.469018	520.176173	8.000102
6.495578	519.930340	8.005107
6.157997	528.324162	8.010112
6.486020	517.280125	8.015130
6.319418	523.929010	8.020147
6.326164	522.680452	8.025165
6.422634	523.223604	8.030182
6.342314	523.488373	8.035200
7.001981	521.996869	8.040218
6.542031	508.248129	8.045235
6.312995	497.902061	8.050253
6.135653	492.447481	8.055270
6.193997	495.278670	8.060288
6.559441	503.730257	8.065306
6.233840	508.332777	8.070323
6.231595	509.866614	8.075341
6.286869	503.959171	8.080358
6.439571	522.285455	8.085376
6.644420	509.747210	8.090394
6.365162	518.421888	8.095411
6.185244	514.638869	8.100429
6.646650	513.835069	8.105446
6.366933	520.337537	8.110464
6.583902	517.810950	8.115482
6.295140	517.611647	8.120499
6.373602	521.526441	8.125517
6.426427	522.198858	8.130534
6.457888	524.951439	8.135552
6.325376	517.253560	8.140570
6.502352	519.845440	8.145587
6.519614	515.734713	8.150605
6.342477	524.636365	8.155622
6.260318	525.136659	8.160640
6.554427	516.049726	8.165658
6.324840	520.885152	8.170675
6.652915	516.130481	8.175693
6.426190	515.354016	8.180710
6.529122	523.642010	8.185728
6.561250	516.456989	8.190746
6.479399	524.143538	8.195763
6.554366	521.237933	8.200781
6.513720	527.071137	8.205798
6.538292	522.087998	8.210816
6.833223	513.030851	8.215834
6.097743	516.931808	8.220851
6.246758	515.338850	8.225869
6.555636	523.727575	8.230886
6.203596	526.303911	8.235904
6.438060	522.457196	8.240922
6.451685	532.148271	8.245939
6.279568	519.734245	8.250957
6.447259	527.465493	8.255974
6.297274	552.298964	8.260992
6.613938	553.674495	8.266010
6.503338	558.688051	8.271027
6.339829	555.231810	8.276045
6.597402	553.675199	8.281062
6.698453	551.423098	8.286080
6.676944	563.013188	8.291098
6.814118	555.449362	8.296115
6.417169	551.142269	8.301133
6.691796	545.746089	8.306150
6.603617	546.759157	8.311168
6.681572	550.487047	8.316186
6.604361	556.562521	8.321203
6.773772	557.864016	8.326221
6.819253	551.807793	8.331238
6.734708	557.837241	8.336256
6.691239	541.803124	8.341274
6.472139	550.835747	8.346291
6.506200	555.069692	8.351309
6.482709	546.707726	8.356326
6.442831	550.739754	8.361344
6.551950	558.899980	8.366362
6.709666	553.050353	8.371379
6.596941	552.037702	8.376397
6.720441	552.436625	8.381414
6.581036	558.371227	8.386432
6.588710	549.976542	8.391450
6.780414	568.832804	8.396467
6.628597	560.413345	8.401485
7.004409	554.112869	8.406502
6.698086	560.751837	8.411520
6.569127	555.002825	8.416538
6.749091	566.139703	8.421555
6.400889	560.030956	8.426573
7.017489	553.967953	8.431590
6.848330	568.315971	8.436608
7.056816	556.325673	8.441626
7.177926	554.607418	8.446643
7.040223	554.135481	8.451661
7.206084	549.975731	8.456678
6.886278	558.869926	8.461696
6.900175	557.306423	8.466714
7.062782	556.482811	8.471731
6.733998	552.515785	8.476749
6.971202	546.752008	8.481766
6.896667	554.193283	8.486784
7.031208	556.993954	8.491802
7.200420	555.408473	8.496819
6.813052	540.728654	8.501837
6.936921	527.815839	8.506854
6.724222	532.888219	8.511872
6.767173	526.522604	8.516890
6.820954	539.775290	8.521907
6.689832	547.507409	8.526925
7.000796	551.460872	8.531942
7.018962	554.270774	8.536960
7.023752	552.160785	8.541978
6.854150	539.122551	8.546995
6.880609	547.222053	8.552013
6.902986	539.506585	8.557030
6.808616	552.451159	8.562048
6.853126	551.694343	8.567066
6.964625	556.247727	8.572083
6.991297	556.692602	8.577101
7.421267	544.536513	8.582119
7.052846	545.466465	8.587136
6.935955	535.142941	8.592154
6.751062	526.462460	8.597171
6.393326	526.508420	8.602189
6.929494	533.907023	8.607207
6.799619	547.400742	8.612224
6.882093	550.977304	8.617242
6.871447	544.195782	8.622259
7.000353	551.070728	8.627277
6.891522	555.636778	8.632295
6.594963	561.510598	8.637312
6.934184	552.622263	8.642330
7.035027	554.511450	8.647347
6.835387	553.188410	8.652365
6.697267	551.755190	8.657383
6.882092	561.265977	8.662400
6.968316	558.203393	8.667418
6.885050	549.859984	8.672435
6.741447	561.833848	8.677453
7.283228	558.179725	8.682471
6.742058	572.158076	8.687488
7.278967	576.841404	8.692506
6.950747	575.845144	8.697523
7.106782	580.834044	8.702541
7.280671	580.132964	8.707559
7.208117	567.036119	8.712576
7.068780	561.069153	8.717594
6.822241	560.980764	8.722611
6.900076	577.642851	8.727629
7.394919	571.454934	8.732647
7.419973	585.510591	8.737664
6.915837	569.201763	8.742682
7.729100	558.816916	8.747699
7.442354	554.922647	8.752717
7.397826	547.825496	8.757735
7.105962	549.773803	8.762752
7.196393	555.322930	8.767770
6.954534	551.012990	8.772787
6.951714	557.880619	8.777805
7.068779	554.002157	8.782823
7.077684	562.873026	8.787840
7.301850	552.631197	8.792858
7.259339	554.594905	8.797875
6.837735	555.121094	8.802893
7.173515	546.027047	8.807911
7.154221	550.116489	8.812928
7.408941	544.277180	8.817946
7.457917	539.302986	8.822963
7.003166	552.109609	8.827981
7.415181	551.855287	8.832999
7.176000	552.095185	8.838016
7.191652	549.787348	8.843034
7.163729	550.053283	8.848051
7.132086	550.534781	8.853069
7.010627	550.638855	8.858087
6.955635	558.759330	8.863104
7.165065	571.802227	8.868122
7.502279	581.578523	8.873139
7.318632	580.893734	8.878157
7.032772	574.701435	8.883175
7.123965	581.327538	8.888192
7.158251	585.219547	8.893210
7.574442	581.508857	8.898227
7.224815	584.888686	8.903245
7.427323	582.913069	8.908263
7.313409	589.439880	8.913280
7.225356	585.478453	8.918298
7.318338	578.873051	8.923315
7.249151	585.545003	8.928333
7.494045	582.477203	8.933351
7.235084	584.947788	8.938368
7.105268	588.149695	8.943386
7.269885	582.047947	8.948403
7.439005	588.891253	8.953421
7.401692	580.428218	8.958439
7.567115	589.047413	8.963456
7.568153	596.446866	8.968474
7.738147	579.010524	8.973491
7.501440	596.864404	8.978509
7.427826	582.184951	8.983527
7.703231	589.960990	8.988544
7.721390	582.260765	8.993562
7.706906	555.149934	8.998579
7.253078	554.122509	9.003597
7.257586	543.511179	9.008615
7.405329	555.323418	9.013632
6.986800	563.944416	9.018650
7.351121	569.634798	9.023667
7.345073	582.350023	9.028685
7.502729	585.200805	9.033703
7.891878	588.348077	9.038720
7.029407	587.610544	9.043738
7.293448	589.966972	9.048755
7.429312	592.676885	9.053773
7.460447	582.851226	9.058791
7.358395	587.348056	9.063808
7.509529	585.414801	9.068826
7.602371	586.992543	9.073843
7.455782	588.824089	9.078861
7.404725	580.141495	9.083879
7.649607	583.468943	9.088896
7.369592	592.970899	9.093914
7.852655	589.329640	9.098931
7.460379	595.154759	9.103949
7.773026	582.852724	9.108967
7.459201	583.957287	9.113984
7.211668	593.025743	9.119002
7.547559	584.083811	9.124019
7.539283	590.610452	9.129037
7.564102	589.078599	9.134055
7.508873	585.760710	9.139072
7.242446	593.167050	9.144090
7.398750	577.342321	9.149107
7.519384	583.361425	9.154125
7.526941	577.375444	9.159143
7.461219	581.986524	9.164160
7.598701	592.128554	9.169178
7.889455	597.693735	9.174195
7.409142	593.111870	9.179213
7.873505	592.296751	9.184231
7.815588	586.674734	9.189248
7.536944	594.098647	9.194266
7.746417	578.382428	9.199283
7.788196	590.052407	9.204301
7.680102	580.427745	9.209319
7.806238	581.297460	9.214336
7.406760	585.283536	9.219354
7.624171	585.276778	9.224371
7.860319	592.911887	9.229389
8.091662	593.478965	9.234407
7.337696	591.902062	9.239424
7.476120	596.473241	9.244442
8.065969	600.658080	9.249459
7.594295	598.610445	9.254477
7.916954	601.427019	9.259495
7.967237	582.676133	9.264512
7.436387	594.406881	9.269530
7.501470	595.955954	9.274547
7.967150	606.536530	9.279565
7.987486	607.015525	9.284583
8.032321	595.564268	9.289600
7.747216	598.110046	9.294618
7.714586	588.928167	9.299635
7.488353	595.375160	9.304653
7.445802	598.036669	9.309671
7.852031	602.723929	9.314688
7.817228	618.833489	9.319706
7.938843	619.539793	9.324723
8.021049	625.116880	9.329741
7.740876	618.595295	9.334759
7.939525	622.787046	9.339776
7.854458	618.446007	9.344794
8.118973	621.042699	9.349811
8.128956	628.917822	9.354829
7.821516	621.622453	9.359847
7.793844	602.697653	9.364864
7.754384	623.630905	9.369882
7.862919	615.460807	9.374899
8.011454	617.464932	9.379917
7.975750	621.230950	9.384935
7.829060	630.229583	9.389952
8.138623	630.890594	9.394970
8.156361	610.116649	9.399987
7.917214	604.245715	9.405005
7.744819	602.134351	9.410023
8.062873	600.770070	9.415040
7.602072	612.219762	9.420058
7.719575	606.401969	9.425075
7.776656	611.149014	9.430093
7.926191	619.289981	9.435111
8.005697	609.827137	9.440128
7.821273	620.521668	9.445146
8.335098	621.924791	9.450163
8.267205	626.954722	9.455181
7.704475	626.725196	9.460199
7.824132	617.324986	9.465216
8.053458	626.050345	9.470234
8.088657	618.356926	9.475251
8.193536	626.885189	9.480269
8.042525	626.489464	9.485287
8.186837	626.284193	9.490304
8.012309	626.765929	9.495322
8.310737	619.747381	9.500339
8.119729	619.053968	9.505357
7.989537	627.288499	9.510375
8.463047	616.123113	9.515392
7.978119	627.779947	9.520410
8.300821	621.605357	9.525427
8.270879	616.639088	9.530445
8.017820	616.862585	9.535463
8.270339	614.996982	9.540480
7.809151	612.364969	9.545498
8.558016	618.892228	9.550515
8.204935	607.098019	9.555533
7.896901	600.703882	9.560551
8.210689	610.585643	9.565568
7.927043	620.166755	9.570586
7.922578	619.323563	9.575603
8.374470	619.870066	9.580621
8.177234	625.744196	9.585639
8.069032	626.166133	9.590656
8.216483	631.408817	9.595674
7.873846	625.471946	9.600691
8.174292	624.322376	9.605709
8.139492	629.588151	9.610727
8.244889	623.940457	9.615744
7.885601	628.247033	9.620762
8.096482	627.295353	9.625779
7.861359	623.298430	9.630797
7.722581	629.874648	9.635815
7.903669	630.702592	9.640832
7.826429	645.111440	9.645850
8.040076	655.272787	9.650867
8.533677	656.391484	9.655885
8.579830	665.260968	9.660903
8.572722	653.120084	9.665920
8.372056	656.537858	9.670938
8.420511	644.064573	9.675955
8.408861	637.528830	9.680973
8.145186	631.835952	9.685991
8.521189	624.612444	9.691008
8.295752	627.939043	9.696026
8.028580	625.313089	9.701043
8.306553	640.997677	9.706061
8.227328	652.036992	9.711079
8.299115	658.094920	9.716096
8.224853	655.557089	9.721114
8.348664	657.718847	9.726131
8.517968	655.039904	9.731149
8.232902	661.669884	9.736167
8.449995	653.858145	9.741184
8.386139	662.017147	9.746202
8.560371	659.204325	9.751219
8.744240	645.296892	9.756237
8.870818	660.166069	9.761255
8.375753	642.223282	9.766272
8.300197	631.442484	9.771290
8.446877	641.360595	9.776307
8.412743	645.296427	9.781325
8.230676	659.114022	9.786343
8.085050	649.284127	9.791360
8.419871	657.906608	9.796378
8.544906	665.228479	9.801395
8.625871	652.599419	9.806413
8.550147	665.986051	9.811431
8.406673	647.792925	9.816448
8.350497	657.068694	9.821466
8.528612	658.256165	9.826483
8.446011	660.701299	9.831501
8.412918	660.829322	9.836519
8.476713	657.315933	9.841536
8.284345	660.915000	9.846554
8.494038	658.575410	9.851571
8.600371	658.205966	9.856589
8.454537	648.370594	9.861607
8.600519	658.071523	9.866624
8.468557	662.610136	9.871642
8.314533	651.154958	9.876659
8.346674	657.023400	9.881677
8.524122	659.539246	9.886695
8.518982	663.228170	9.891712
8.339302	671.834283	9.896730
8.654008	673.311717	9.901747
8.742354	688.397082	9.906765
8.498376	702.280870	9.911783
8.304419	683.735846	9.916800
8.724603	685.776096	9.921818
8.712149	696.081595	9.926835
8.725644	689.389314	9.931853
8.620153	689.530506	9.936871
8.917626	676.944311	9.941888
9.062697	686.112763	9.946906
8.763688	686.766678	9.951923
9.326297	679.940173	9.956941
8.842271	673.327130	9.961959
8.703320	663.904364	9.966976
8.569639	653.829195	9.971994
8.807744	657.225100	9.977011
8.370786	655.501216	9.982029
8.348834	660.430643	9.987047
8.918719	666.810010	9.992064
9.022598	685.781541	9.997082
8.661170	681.212246	10.002099
8.998154	677.312298	10.007117
8.495625	673.866303	10.012135
8.817675	672.825744	10.017152
9.191020	680.154535	10.022170
8.809082	667.762338	10.027187
8.676647	659.625031	10.032205
8.718851	668.100706	10.037223
8.771519	673.477202	10.042240
9.039311	687.369931	10.047258
8.950111	681.958362	10.052275
8.777826	660.228078	10.057293
8.338069	662.427646	10.062311
8.618369	679.050807	10.067328
8.949351	681.375102	10.072346
8.832021	695.627260	10.077363
9.231256	682.858472	10.082381
9.082097	685.076456	10.087399
9.181372	695.080400	10.092416
9.000274	678.733123	10.097434
8.444920	675.296268	10.102451
9.123493	682.156434	10.107469
8.925011	688.960659	10.112487
8.852341	697.082165	10.117504
9.174198	682.306231	10.122522
8.764793	694.313186	10.127539
8.933903	689.696982	10.132557
8.861124	687.779729	10.137575
8.988654	694.511472	10.142592
8.903828	691.398253	10.147610
8.834752	692.480997	10.152627
9.101078	689.147044	10.157645
8.820676	690.623027	10.162663
8.858065	684.075995	10.167680
9.235194	687.583131	10.172698
8.824518	688.442533	10.177715
8.882333	684.107342	10.182733
9.282267	691.003414	10.187751
9.228887	684.565501	10.192768
8.705671	688.548471	10.197786
8.682703	694.378417	10.202803
8.815208	693.572380	10.207821
8.991569	693.272043	10.212839
9.237437	689.052555	10.217856
9.351003	695.896840	10.222874
8.951160	691.820881	10.227891
8.794637	693.718058	10.232909
8.832642	705.049398	10.237927
9.057955	703.913839	10.242944
9.356569	712.556911	10.247962
9.080958	714.107295	10.252979
9.229353	714.731220	10.257997
9.501067	704.828248	10.263015
9.295176	704.365235	10.268032
9.478422	686.939569	10.273050
8.967075	692.706296	10.278067
9.022340	689.046289	10.283085
9.205812	694.552699	10.288103
8.980411	687.620859	10.293120
9.598961	696.471561	10.298138
9.445546	705.136331	10.303155
9.186710	688.282655	10.308173
9.254271	688.948309	10.313191
8.984031	689.692731	10.318208
8.956290	697.335172	10.323226
9.122638	721.772854	10.328243
9.360487	711.847140	10.333261
9.324587	717.821354	10.338279
9.235103	719.534214	10.343296
9.660286	720.061524	10.348314
9.246320	716.020179	10.353331
9.572789	721.040743	10.358349
9.491663	709.132925	10.363367
8.993312	701.905349	10.368384
9.427579	709.391772	10.373402
9.337518	716.442608	10.378419
9.514860	718.484887	10.383437
9.458741	713.963448	10.388455
9.448919	710.398067	10.393472
9.685895	702.751505	10.398490
9.306355	698.202919	10.403507
9.340225	684.232892	10.408525
9.199874	684.263721	10.413543
9.129227	703.987752	10.418560
9.608506	712.143849	10.423578
9.631720	715.277729	10.428595
9.600789	703.838742	10.433613
9.322795	697.838780	10.438631
9.190732	708.906175	10.443648
9.747715	710.925352	10.448666
9.462170	712.538400	10.453683
9.753314	714.328778	10.458701
9.601331	697.866430	10.463719
9.238339	685.143936	10.468736
9.357434	690.944846	10.473754
9.403400	714.764299	10.478771
9.700636	714.657321	10.483789
9.759510	718.920270	10.488807
9.701489	709.627768	10.493824
9.570068	696.766138	10.498842
9.218865	701.571761	10.503859
9.855113	708.478314	10.508877
9.669357	695.361525	10.513895
9.188965	694.081811	10.518912
9.665397	703.683172	10.523930
9.434841	712.850455	10.528947
9.677217	722.211466	10.533965
9.679765	718.076351	10.538983
9.650470	729.986537	10.544000
9.851282	715.917189	10.549018
9.382751	718.983684	10.554035
9.683209	715.907051	10.559053
9.839812	718.444075	10.564071
9.401860	711.209643	10.569088
9.538944	716.537138	10.574106
9.718502	717.771616	10.579123
9.784278	724.650204	10.584141
9.847953	720.044363	10.589159
9.492267	724.946399	10.594176
9.965589	717.579968	10.599194
9.457063	726.404726	10.604211
9.435375	728.700029	10.609229
9.486660	724.056084	10.614247
9.747331	730.247715	10.619264
9.706465	729.718007	10.624282
9.321001	715.014677	10.629299
9.677452	726.896419	10.634317
9.543194	720.245912	10.639335
9.072376	729.649040	10.644352
9.637808	734.807195	10.649370
9.622718	753.571750	10.654387
9.709427	743.717102	10.659405
9.895230	745.056054	10.664423
9.837735	748.996962	10.669440
10.033591	752.959302	10.674458
10.078593	754.326293	10.679475
9.897973	762.760574	10.684493
10.177799	750.453212	10.689511
9.849315	750.805727	10.694528
9.804963	749.499080	10.699546
9.747776	753.930462	10.704563
9.799217	752.556775	10.709581
9.989866	745.595779	10.714599
9.817514	742.778129	10.719616
10.204193	753.181346	10.724634
10.216573	746.903769	10.729651
10.079159	749.816235	10.734669
10.122469	735.573747	10.739687
10.028364	730.259819	10.744704
10.115485	717.869043	10.749722
9.773084	726.873762	10.754739
9.580749	720.216731	10.759757
9.888563	726.402130	10.764775
9.889269	744.825888	10.769792
10.212479	736.930005	10.774810
10.395756	746.561038	10.779827
9.968297	744.787148	10.784845
10.202097	746.417742	10.789863
10.156320	740.575758	10.794880
10.203226	719.927144	10.799898
9.814772	729.839832	10.804915
9.940722	740.877519	10.809933
10.264266	743.955376	10.814951
9.873567	750.891451	10.819968
10.635787	748.675701	10.824986
10.314680	736.575328	10.830003
10.136161	731.940694	10.835021
10.057988	721.298448	10.840039
9.917710	718.667606	10.845056
9.749846	713.832799	10.850074
10.075052	731.926842	10.855091
9.882744	741.809028	10.860109
10.194123	741.635932	10.865127
10.003432	746.199253	10.870144
9.854569	739.675952	10.875162
10.101257	740.590673	10.880179
10.199863	743.003059	10.885197
10.198049	743.245581	10.890215
9.934035	752.090493	10.895232
10.192898	748.907362	10.900250
10.570082	746.597109	10.905267
10.493879	750.504896	10.910285
10.389403	747.830722	10.915303
10.386821	746.686047	10.920320
10.455666	742.218312	10.925338
10.176509	745.312507	10.930355
10.153709	747.380056	10.935373
10.527921	745.108877	10.940391
10.134751	739.527160	10.945408
10.166676	744.765784	10.950426
10.274581	751.261838	10.955443
10.327074	742.554920	10.960461
10.128306	747.877412	10.965479
10.041094	750.929982	10.970496
10.139254	747.958884	10.975514
10.333848	747.456325	10.980531
10.234798	755.373187	10.985549
10.509898	752.459005	10.990567
10.473017	766.614840	10.995584
10.256947	754.470291	11.000602
10.096075	752.751071	11.005619
10.518020	769.346544	11.010637
10.692731	778.245197	11.015655
10.562349	775.286740	11.020672
10.653496	773.694283	11.025690
10.527114	758.298440	11.030707
10.252097	760.538062	11.035725
10.723101	757.005252	11.040743
10.524495	758.893658	11.045760
10.646519	762.809174	11.050778
10.454373	747.255737	11.055795
10.609398	754.416787	11.060813
10.781800	752.785682	11.065831
10.605748	758.442980	11.070848
10.365101	755.796863	11.075866
10.483124	748.556175	11.080883
10.480825	739.330802	11.085901
10.658472	736.128839	11.090919
10.633571	748.713865	11.095936
10.437178	749.798798	11.100954
10.900457	751.276047	11.105971
10.542432	757.806343	11.110989
10.858809	748.786844	11.116007
10.474094	741.871517	11.121024
10.212247	744.563655	11.126042
10.522314	762.959437	11.131059
10.489692	777.359445	11.136077
10.788554	777.022682	11.141095
10.714869	782.855154	11.146112
10.643287	782.949789	11.151130
10.841235	776.729657	11.156147
10.813626	788.952978	11.161165
10.854688	779.391678	11.166183
10.990215	778.471757	11.171200
10.863464	773.836805	11.176218
10.836744	752.511399	11.181235
10.728258	751.767310	11.186253
10.807758	750.605106	11.191271
10.607136	756.503072	11.196288
10.863275	762.231713	11.201306
11.013678	763.642273	11.206323
11.003506	756.460208	11.211341
10.807376	748.856601	11.216359
10.558834	739.360207	11.221376
10.532322	742.589723	11.226394
10.893230	762.389999	11.231411
10.890713	780.596236	11.236429
11.213595	776.388379	11.241447
10.909712	771.985897	11.246464
10.542908	767.585567	11.251482
10.676036	769.025758	11.256499
10.884891	780.395002	11.261517
11.316299	778.828876	11.266535
10.883158	777.370473	11.271552
11.189043	774.365367	11.276570
11.067642	773.740338	11.281587
10.677196	770.725343	11.286605
10.668284	773.750387	11.291623
11.152598	782.893824	11.296640
10.886019	779.681555	11.301658
11.319392	776.414801	11.306675
11.009222	777.711478	11.311693
11.096778	775.821600	11.316711
11.084614	779.310938	11.321728
10.888920	779.974520	11.326746
11.105169	775.358359	11.331763
10.910324	776.330445	11.336781
11.044946	771.041618	11.341799
11.167200	784.174322	11.346816
11.044261	778.546665	11.351834
11.413614	770.886811	11.356851
11.217022	792.677368	11.361869
11.001664	776.582498	11.366887
11.225531	771.585570	11.371904
11.201549	781.182442	11.376922
11.052134	765.611282	11.381939
10.833241	771.772108	11.386957
10.985901	774.227121	11.391975
11.059191	774.183207	11.396992
10.908107	772.299774	11.402010
11.155649	778.619971	11.407027
10.728074	780.525820	11.412045
10.783065	775.049401	11.417063
10.852976	777.257106	11.422080
10.798951	777.214589	11.427098
11.303786	789.382817	11.432115
11.019602	802.641101	11.437133
11.376236	802.135331	11.442151
11.047403	806.521554	11.447168
10.987834	802.445125	11.452186
11.335858	807.013746	11.457203
11.041055	811.809669	11.462221
11.197822	807.086031	11.467239
11.458635	808.603898	11.472256
11.179657	813.017693	11.477274
11.540646	802.406605	11.482291
11.464385	807.996218	11.487309
11.368068	803.481408	11.492327
11.462702	805.853520	11.497344
11.374435	809.866857	11.502362
11.671295	799.173088	11.507379
11.489318	810.617305	11.512397
11.228032	801.935540	11.517415
10.915837	804.070306	11.522432
11.336240	801.003322	11.527450
11.981642	797.879398	11.532467
11.617760	801.482489	11.537485
11.726368	807.233607	11.542503
11.936079	799.133663	11.547520
11.495505	798.413458	11.552538
11.715039	784.357483	11.557555
11.245839	778.865896	11.562573
11.369788	789.431926	11.567591
11.512908	800.601845	11.572608
11.271192	804.037077	11.577626
11.804149	798.468515	11.582643
11.691943	803.360178	11.587661
11.792673	793.944493	11.592679
11.620974	788.859523	11.597696
11.408408	784.158466	11.602714
11.754402	785.745686	11.607731
11.659395	800.607597	11.612749
11.460149	794.854386	11.617767
12.002215	801.949797	11.622784
11.612711	786.343964	11.627802
11.608423	773.755693	11.632819
11.465606	777.200920	11.637837
11.731047	800.721186	11.642855
11.793882	799.939277	11.647872
11.257153	794.415168	11.652890
11.435570	800.569663	11.657907
11.679263	804.750855	11.662925
11.852754	805.297011	11.667943
11.843413	801.321708	11.672960
11.731505	804.166579	11.677978
12.052714	802.495869	11.682995
11.711056	811.325719	11.688013
12.100499	801.287844	11.693031
11.599567	800.829195	11.698048
11.446655	799.162980	11.703066
11.868364	804.324092	11.708083
11.825745	803.578541	11.713101
11.546025	797.319785	11.718119
11.708833	803.210344	11.723136
11.646587	807.333933	11.728154
11.955505	797.822753	11.733171
11.813856	792.482818	11.738189
11.649755	806.494804	11.743207
11.986752	798.758409	11.748224
11.529278	808.340074	11.753242
11.650732	797.177345	11.758259
11.583952	799.882072	11.763277
11.699611	797.499768	11.768295
11.892440	799.356038	11.773312
12.008291	830.480253	11.778330
12.059118	826.530412	11.783347
11.821800	813.735824	11.788365
11.893691	826.973356	11.793383
12.018095	828.240597	11.798400
11.977919	837.185494	11.803418
12.329235	828.479833	11.808435
12.061535	823.455627	11.813453
12.062479	813.143507	11.818471
11.962874	801.173327	11.823488
11.796279	811.311916	11.828506
12.556792	817.753872	11.833523
12.214135	818.849249	11.838541
12.201012	808.167827	11.843559
12.149839	795.514470	11.848576
12.102258	807.069889	11.853594
12.281114	797.575520	11.858611
12.290871	793.677762	11.863629
12.147131	796.926700	11.868647
12.241871	792.762521	11.873664
12.090495	804.392995	11.878682
12.435320	790.217061	11.883699
12.397455	799.167459	11.888717
12.069265	796.518115	11.893735
12.370384	801.055526	11.898752
12.153001	795.679315	11.903770
12.156685	792.055776	11.908787
12.285138	795.798198	11.913805
12.204435	798.233985	11.918823
12.106982	799.583626	11.923840
12.122962	798.054791	11.928858
12.016308	803.141981	11.933875
11.764763	801.063380	11.938893
12.097442	818.362628	11.943911
12.445884	819.432543	11.948928
12.219039	838.594843	11.953946
12.029530	834.348986	11.958963
12.169246	828.996306	11.963981
12.283080	833.844252	11.968999
12.594447	825.405430	11.974016
12.060858	840.946270	11.979034
12.427581	828.983494	11.984051
12.492389	829.996443	11.989069
12.189002	838.868395	11.994087
12.379303	827.019081	11.999104
12.252995	839.884739	12.004122
12.442223	833.805785	12.009139
12.297078	829.299446	12.014157
12.385888	834.439316	12.019175
12.333712	830.957295	12.024192
12.089942	836.226641	12.029210
12.353441	844.835447	12.034227
12.511676	854.788395	12.039245
12.411045	862.548099	12.044263
12.507609	855.938837	12.049280
12.941524	861.738861	12.054298
12.806831	861.801823	12.059315
12.902558	847.533231	12.064333
12.450677	837.158287	12.069351
12.683816	830.868136	12.074368
12.470275	836.568676	12.079386
12.695187	828.396518	12.084403
12.787794	830.970533	12.089421
12.400456	832.168580	12.094439
12.490485	830.678266	12.099456
12.504321	846.107995	12.104474
12.506645	854.747848	12.109491
13.009678	856.261437	12.114509
12.881204	860.611744	12.119527
12.844166	839.932777	12.124544
12.852497	828.629709	12.129562
12.728991	835.018454	12.134579
12.910971	827.486838	12.139597
12.665348	826.955207	12.144615
12.978465	826.069653	12.149632
12.816021	825.453386	12.154650
12.573883	825.061721	12.159667
12.885385	822.476521	12.164685
12.684050	830.409176	12.169703
13.033675	818.846070	12.174720
12.956201	826.911749	12.179738
12.813404	830.005428	12.184755
12.821283	827.678365	12.189773
12.911527	833.195538	12.194791
12.964009	821.636751	12.199808
12.610843	833.871891	12.204826
12.745817	836.980598	12.209843
12.883790	832.356910	12.214861
12.947468	846.239880	12.219879
12.995480	850.064136	12.224896
12.643299	850.283969	12.229914
12.463847	864.595778	12.234931
13.104426	861.132894	12.239949
12.876354	871.950173	12.244967
13.081006	861.633817	12.249984
12.966003	863.109985	12.255002
13.099791	868.971912	12.260019
12.924812	861.202550	12.265037
12.785018	870.269468	12.270055
12.867387	863.486578	12.275072
12.969568	864.308704	12.280090
12.816828	867.482379	12.285107
12.819140	862.430773	12.290125
12.521825	864.653236	12.295143
12.885381	870.881823	12.300160
13.214378	889.617912	12.305178
13.440762	890.695445	12.310195
13.412122	895.553617	12.315213
13.264910	876.959678	12.320231
13.277382	858.425536	12.325248
13.566169	853.591839	12.330266
13.169387	867.821139	12.335283
13.243806	850.445592	12.340301
12.963030	847.694692	12.345319
13.359601	850.774652	12.350336
13.399209	854.257797	12.355354
13.200549	852.396405	12.360371
13.360215	851.890966	12.365389
13.210720	851.742215	12.370407
13.256294	853.200455	12.375424
13.137127	851.102290	12.380442
12.889941	855.807275	12.385459
13.393613	861.774086	12.390477
13.865777	876.583886	12.395495
13.452919	869.893623	12.400512
12.919356	857.969272	12.405530
13.323915	867.119667	12.410547
13.636722	884.241579	12.415565
13.326950	881.104548	12.420583
13.594282	877.211754	12.425600
13.334476	870.747710	12.430618
13.454220	868.235198	12.435635
13.543693	868.226397	12.440653
13.282763	871.434916	12.445671
13.596350	887.376049	12.450688
13.466538	892.158456	12.455706
13.468813	884.929785	12.460723
13.650661	875.686830	12.465741
13.468882	870.886166	12.470759
13.381217	873.346344	12.475776
13.569138	882.323574	12.480794
13.390577	895.603422	12.485811
13.470593	886.328506	12.490829
13.355739	894.592921	12.495847
13.383964	887.901658	12.500864
13.429955	885.540719	12.505882
13.449365	890.293299	12.510899
13.707833	879.425131	12.515917
13.756837	893.224751	12.520935
13.661970	884.597663	12.525952
13.569724	880.288840	12.530970
13.612410	881.978258	12.535987
13.897066	884.042158	12.541005
13.638859	886.951031	12.546023
13.599430	884.242441	12.551040
13.929468	879.403087	12.556058
13.725725	886.198427	12.561075
13.682209	879.161190	12.566093
13.767209	886.885445	12.571111
13.613281	885.480794	12.576128
13.914190	880.138019	12.581146
13.691366	885.872396	12.586163
13.764928	883.186433	12.591181
13.821862	889.433911	12.596199
13.860687	885.177396	12.601216
14.200389	884.188623	12.606234
13.674196	891.067277	12.611251
14.120310	875.200949	12.616269
13.992996	885.762984	12.621287
13.791769	876.949190	12.626304
13.960487	883.136031	12.631322
13.882833	887.646427	12.636339
13.944631	879.191816	12.641357
13.665470	884.833557	12.646375
13.749318	888.564491	12.651392
13.985995	885.843252	12.656410
13.763840	883.868823	12.661427
14.103456	878.864898	12.666445
13.989848	888.429436	12.671463
14.077391	882.736574	12.676480
14.206425	885.281733	12.681498
13.691877	889.819198	12.686515
14.069791	893.110120	12.691533
14.175899	908.390780	12.696551
14.166800	905.642521	12.701568
14.173712	906.054459	12.706586
14.168583	901.754826	12.711603
14.613151	898.436195	12.716621
14.283774	895.664595	12.721639
14.351498	894.173638	12.726656
14.437342	879.894449	12.731674
13.970214	886.237755	12.736691
14.215730	883.517809	12.741709
14.133526	881.530048	12.746727
14.021787	884.755990	12.751744
14.166999	883.832097	12.756762
14.289073	881.298331	12.761779
14.420664	873.273486	12.766797
14.277442	878.924210	12.771815
13.909982	881.882666	12.776832
14.074042	887.156937	12.781850
14.317578	901.465273	12.786867
14.529604	897.834770	12.791885
14.493595	905.567261	12.796903
14.353965	905.137756	12.801920
14.582621	905.642892	12.806938
14.362588	890.566742	12.811955
14.432063	887.379117	12.816973
14.148020	887.344373	12.821991
13.864931	894.472525	12.827008
14.379834	887.253848	12.832026
14.083807	898.680402	12.837043
14.217634	896.514356	12.842061
14.224810	905.135718	12.847079
14.161352	904.718008	12.852096
14.057013	901.832770	12.857114
14.286924	908.089013	12.862131
14.581451	918.794203	12.867149
14.610284	930.951206	12.872167
14.725288	934.348266	12.877184
14.737440	912.155218	12.882202
14.691868	914.926529	12.887219
14.600780	906.630677	12.892237
14.217167	907.599384	12.897255
14.402885	920.552018	12.902272
14.404363	928.241701	12.907290
14.684030	937.229361	12.912307
14.893292	931.729310	12.917325
15.094196	927.413664	12.922343
14.518163	924.669515	12.927360
14.537079	927.938002	12.932378
14.645302	933.956542	12.937395
14.719037	924.314549	12.942413
14.600490	936.897912	12.947431
14.480264	928.748206	12.952448
14.651361	932.289120	12.957466
14.614455	940.424515	12.962483
14.939644	927.630389	12.967501
14.804652	926.230472	12.972519
14.997703	930.305128	12.977536
14.984705	923.897435	12.982554
14.748479	929.848998	12.987571
14.929598	930.639160	12.992589
14.847536	919.828532	12.997607
14.928662	933.741367	13.002624
15.095922	920.139575	13.007642
15.145412	919.172871	13.012659
14.862326	931.396090	13.017677
14.992177	927.283932	13.022695
14.917571	934.827956	13.027712
15.123974	931.107435	13.032730
14.824138	936.187682	13.037747
14.792191	936.172216	13.042765
14.876282	922.317275	13.047783
14.566513	928.098739	13.052800
15.053069	928.440706	13.057818
15.038820	926.161779	13.062835
14.949472	927.345923	13.067853
15.192105	924.531569	13.072871
15.075144	928.970930	13.077888
15.095033	920.245296	13.082906
15.295520	936.330793	13.087923
15.069278	927.789998	13.092941
15.046831	924.859701	13.097959
15.030509	924.445603	13.102976
15.246551	923.339120	13.107994
15.201102	929.750804	13.113011
15.265494	931.076414	13.118029
15.495710	918.060629	13.123047
14.933363	931.245796	13.128064
15.265090	919.705656	13.133082
15.094281	932.398846	13.138099
15.108813	935.614913	13.143117
15.306498	944.466946	13.148135
15.277146	952.315676	13.153152
15.281938	948.607275	13.158170
15.327993	948.382839	13.163187
15.548493	953.914311	13.168205
16.145941	942.162447	13.173223
15.864123	930.141633	13.178240
15.490382	925.714061	13.183258
15.520449	920.697996	13.188275
15.408263	917.903421	13.193293
15.447227	911.841444	13.198311
15.123518	916.742181	13.203328
15.483146	914.582442	13.208346
15.261963	907.624608	13.213363
15.410454	910.342920	13.218381
15.376443	908.670784	13.223399
15.174828	923.719355	13.228416
15.516442	917.287591	13.233434
15.216105	923.443853	13.238451
15.350031	941.535170	13.243469
15.824651	940.834277	13.248487
15.898558	952.613378	13.253504
15.769654	941.988041	13.258522
15.583374	938.264827	13.263539
15.697095	939.460227	13.268557
15.584046	931.277442	13.273575
15.701389	948.031021	13.278592
15.788676	937.623816	13.283610
15.445245	929.998055	13.288627
15.917807	946.445974	13.293645
16.111611	939.496967	13.298663
15.681279	923.563125	13.303680
15.478660	921.318932	13.308698
15.615923	927.020470	13.313715
15.925249	936.668544	13.318733
16.164555	934.752338	13.323751
15.797046	934.911328	13.328768
15.648025	915.228319	13.333786
15.735255	921.169625	13.338803
15.881573	933.877625	13.343821
15.763620	944.603497	13.348839
15.886164	948.693376	13.353856
16.033400	942.473307	13.358874
16.096876	942.318031	13.363891
15.980907	937.283230	13.368909
15.913309	930.062563	13.373927
15.874130	942.279261	13.378944
15.960165	939.829009	13.383962
15.969700	941.368811	13.388979
16.037481	954.459108	13.393997
15.993622	949.852896	13.399015
16.063032	948.040014	13.404032
16.131660	940.396016	13.409050
16.098279	947.017117	13.414067
16.284858	942.087329	13.419085
16.472026	936.266933	13.424103
15.788124	935.295686	13.429120
15.855008	925.510738	13.434138
15.962751	930.983318	13.439155
16.247068	938.349807	13.444173
16.259830	939.465078	13.449191
15.958995	941.590501	13.454208
16.006770	938.122219	13.459226
16.046551	947.401957	13.464243
15.934985	941.755428	13.469261
16.206242	937.023423	13.474279
16.336155	947.486217	13.479296
16.167054	941.007912	13.484314
16.137614	943.570266	13.489331
15.914176	945.449027	13.494349
16.095348	938.508017	13.499367
15.661258	951.862900	13.504384
16.012411	953.936271	13.509402
16.589590	963.331751	13.514419
16.258815	971.920136	13.519437
16.352057	968.752968	13.524455
16.780452	968.584903	13.529472
16.636353	972.690988	13.534490
16.160308	965.433216	13.539507
16.506494	969.295133	13.544525
16.718215	967.724422	13.549543
16.346569	964.901543	13.554560
16.628836	961.346792	13.559578
16.468902	957.559370	13.564595
16.346241	958.517940	13.569613
16.558186	963.622110	13.574631
16.859384	969.646899	13.579648
16.732482	948.971249	13.584666
16.658082	937.390081	13.589683
16.396744	937.385040	13.594701
16.837582	931.116361	13.599719
16.376458	948.441687	13.604736
16.743145	951.851405	13.609754
16.865876	949.601759	13.614771
16.523667	949.049109	13.619789
16.447893	951.027430	13.624807
16.700739	963.990639	13.629824
16.719103	968.734361	13.634842
16.849431	967.090123	13.639859
16.444761	959.141430	13.644877
16.881696	957.831054	13.649895
16.738033	963.827537	13.654912
16.486616	971.746116	13.659930
16.990056	965.008809	13.664947
16.909079	974.233365	13.669965
16.788842	972.475897	13.674983
16.844751	969.436952	13.680000
17.005740	967.251045	13.685018
17.076249	967.918585	13.690035
17.015440	976.876428	13.695053
17.004565	968.847171	13.700071
17.022097	967.517267	13.705088
17.211919	972.981783	13.710106
17.042345	976.467309	13.715123
16.835464	979.720441	13.720141
16.792019	959.501019	13.725159
16.909190	970.457649	13.730176
16.866183	971.573889	13.735194
17.297603	972.562756	13.740211
16.924730	966.178022	13.745229
16.868914	958.324315	13.750247
16.953858	967.092277	13.755264
16.858449	973.312260	13.760282
17.249640	960.322933	13.765299
16.902207	969.917577	13.770317
16.782723	976.265165	13.775335
17.159401	967.091072	13.780352
16.846818	966.926413	13.785370
17.370879	960.512845	13.790387
17.096026	969.503370	13.795405
17.023704	972.630287	13.800423
17.292448	980.637538	13.805440
17.394969	988.282962	13.810458
17.345556	979.973872	13.815475
17.047493	997.665937	13.820493
17.340994	984.423879	13.825511
17.727130	990.256272	13.830528
17.403030	987.771565	13.835546
17.560005	972.537637	13.840563
17.441238	971.740516	13.845581
17.352259	969.173969	13.850599
17.392477	959.937487	13.855616
17.281800	965.376563	13.860634
17.249216	965.049798	13.865651
17.175272	986.575841	13.870669
17.509517	996.736735	13.875687
17.616982	988.281196	13.880704
17.675246	996.022925	13.885722
17.614755	987.281430	13.890739
17.802168	996.714698	13.895757
17.736224	973.915226	13.900775
17.496609	965.544727	13.905792
17.488765	963.126945	13.910810
17.806923	955.890815	13.915827
17.509848	965.389720	13.920845
17.651382	962.390927	13.925863
17.706533	961.138256	13.930880
17.373746	973.091402	13.935898
17.850661	977.212765	13.940915
17.540444	995.143839	13.945933
17.780257	990.230417	13.950951
17.942707	987.745852	13.955968
17.566221	990.020811	13.960986
17.729464	990.160813	13.966003
17.486346	989.649231	13.971021
17.539130	990.070111	13.976039
17.579425	993.150827	13.981056
17.797293	990.558664	13.986074
17.996489	989.474258	13.991091
17.635348	999.746753	13.996109
17.849744	991.893167	14.001127
18.095158	989.335418	14.006144
17.622089	992.229889	14.011162
18.020203	984.058890	14.016179
17.834290	993.485865	14.021197
17.962975	991.781662	14.026215
18.129091	982.466449	14.031232
17.873670	992.624195	14.036250
17.872464	997.046770	14.041267
17.581195	994.558988	14.046285
17.458601	1011.677942	14.051303
17.979133	1007.743978	14.056320
18.155210	1022.237998	14.061338
18.502856	1024.212751	14.066355
18.504824	1027.014791	14.071373
18.477296	1012.649925	14.076391
18.504424	1007.623296	14.081408
18.278015	1001.880410	14.086426
18.639585	991.367913	14.091443
18.268124	989.215445	14.096461
18.186435	990.271558	14.101479
18.237803	989.969080	14.106496
17.721392	995.080482	14.111514
17.882028	986.734639	14.116531
18.344773	989.369829	14.121549
18.236331	998.754453	14.126567
18.531745	1003.023982	14.131584
18.485340	1007.695373	14.136602
18.321327	992.548826	14.141619
18.385178	1001.072278	14.146637
18.073877	990.354280	14.151655
18.377647	1002.688248	14.156672
18.046000	1025.985295	14.161690
18.251765	1010.483418	14.166707
18.413691	1014.532937	14.171725
18.010777	1022.731736	14.176743
18.092775	1015.557910	14.181760
18.217652	1025.361379	14.186778
18.660064	1015.759067	14.191795
18.153820	1017.262632	14.196813
18.037961	1018.436212	14.201831
18.675269	1030.162239	14.206848
18.638412	1046.511945	14.211866
18.942651	1042.832677	14.216883
19.173039	1042.318277	14.221901
18.860132	1021.594593	14.226919
18.807797	1002.726928	14.231936
18.713647	1021.705678	14.236954
18.923270	1005.142971	14.241971
18.951449	1014.147516	14.246989
18.684371	1011.990752	14.252007
19.040564	1015.366002	14.257024
19.018027	1014.483657	14.262042
18.950960	1008.371091	14.267059
18.760291	1003.319505	14.272077
19.224654	1009.246035	14.277095
18.877579	1008.087125	14.282112
18.997633	1005.431631	14.287130
19.053443	1000.949446	14.292147
19.135477	1009.026996	14.297165
18.738764	1008.145586	14.302183
18.787936	1000.648081	14.307200
19.010644	1008.262198	14.312218
18.890010	1007.422473	14.317235
18.926699	1011.503751	14.322253
18.800301	1007.920204	14.327271
19.272731	1000.029006	14.332288
19.205632	1008.632018	14.337306
18.769875	1011.746289	14.342323
18.855551	1009.522061	14.347341
18.943108	1011.143830	14.352359
19.185393	1012.054573	14.357376
18.627781	1001.785209	14.362394
18.771030	1006.712194	14.367411
18.986258	1014.818084	14.372429
18.858634	1026.163699	14.377447
19.261406	1028.796229	14.382464
19.164659	1034.172001	14.387482
19.522610	1029.464982	14.392499
19.672180	1031.510721	14.397517
18.879755	1020.851107	14.402535
19.366942	1018.980064	14.407552
19.239592	1029.272921	14.412570
19.161736	1027.389930	14.417587
19.275599	1031.563155	14.422605
19.170280	1041.318927	14.427623
19.666085	1030.856221	14.432640
19.418223	1038.164819	14.437658
19.468964	1027.971078	14.442675
19.769548	1019.946520	14.447693
19.761282	1028.370122	14.452711
19.551816	1025.014885	14.457728
19.431238	1026.322706	14.462746
19.661679	1024.452051	14.467763
19.475461	1017.758840	14.472781
19.432156	1017.412196	14.477799
19.885252	1017.136502	14.482816
19.238436	1024.680831	14.487834
19.642135	1029.735557	14.492851
19.687420	1029.403378	14.497869
19.488705	1034.629505	14.502887
19.773802	1025.517785	14.507904
19.713090	1032.413910	14.512922
19.780188	1031.236024	14.517939
19.774419	1025.355419	14.522957
19.548463	1027.214527	14.527975
19.824002	1026.525730	14.532992
19.722883	1032.786838	14.538010
19.541688	1033.787386	14.543027
19.408582	1025.378747	14.548045
19.421619	1029.585596	14.553063
19.666822	1030.219882	14.558080
19.510353	1032.338735	14.563098
19.396241	1030.227110	14.568115
19.655233	1032.289769	14.573133
19.470525	1044.352698	14.578151
19.838169	1047.278832	14.583168
19.901956	1062.917034	14.588186
19.921371	1056.183851	14.593203
20.017678	1057.940786	14.598221
19.986207	1065.173804	14.603239
20.177652	1056.705504	14.608256
20.040518	1061.733261	14.613274
20.116075	1064.638080	14.618291
20.413571	1054.279452	14.623309
20.001219	1056.682402	14.628327
20.375820	1054.809131	14.633344
20.341549	1057.357345	14.638362
20.250232	1050.677932	14.643379
20.397921	1047.285598	14.648397
20.202480	1046.592898	14.653415
20.392839	1039.769609	14.658432
20.171694	1032.425506	14.663450
20.144419	1040.314880	14.668467
20.517973	1039.710243	14.673485
20.517396	1044.137058	14.678503
20.140647	1026.713975	14.683520
20.384763	1029.635757	14.688538
20.655371	1028.767468	14.693555
20.274774	1014.623260	14.698573
20.107997	1019.925193	14.703591
20.606265	1028.691678	14.708608
20.475109	1030.719729	14.713626
20.449060	1030.374165	14.718643
20.335946	1025.474290	14.723661
20.373558	1050.796374	14.728679
20.813062	1053.580301	14.733696
20.452371	1044.668410	14.738714
20.560006	1050.627647	14.743731
20.721197	1051.648666	14.748749
20.207740	1052.592031	14.753767
20.410078	1044.199884	14.758784
20.533476	1046.043666	14.763802
20.679687	1043.615323	14.768819
20.982140	1037.544706	14.773837
20.798272	1040.998757	14.778855
20.815306	1045.525802	14.783872
20.984160	1044.503107	14.788890
20.673487	1042.391351	14.793907
21.153047	1035.184363	14.798925
20.419978	1032.472101	14.803943
20.493886	1033.093020	14.808960
21.082890	1043.725916	14.813978
20.708129	1043.058972	14.818995
20.906801	1041.177827	14.824013
21.013999	1048.436300	14.829031
21.174230	1048.042569	14.834048
21.239700	1046.462997	14.839066
20.818967	1032.864375	14.844083
20.983125	1015.678894	14.849101
20.726057	1016.527050	14.854119
20.688894	1026.644742	14.859136
21.238248	1035.494501	14.864154
20.928479	1043.172394	14.869171
20.748500	1041.372056	14.874189
20.952531	1048.908973	14.879207
21.443740	1042.866547	14.884224
21.161949	1042.590493	14.889242
21.089024	1041.206271	14.894259
21.451377	1036.531591	14.899277
21.353602	1053.029968	14.904295
21.253373	1038.807820	14.909312
21.196287	1038.935094	14.914330
20.844070	1044.923622	14.919347
21.140784	1041.809359	14.924365
20.872239	1046.336054	14.929383
20.873028	1048.054475	14.934400
20.838572	1044.824186	14.939418
20.569495	1046.649494	14.944435
21.031440	1051.145390	14.949453
21.277371	1069.173431	14.954471
21.348253	1069.916108	14.959488
21.812593	1072.699076	14.964506
21.517797	1077.458465	14.969523
21.827660	1069.729579	14.974541
21.587417	1061.982733	14.979559
21.391289	1052.126692	14.984576
21.748386	1049.994913	14.989594
21.742156	1040.984570	14.994611
21.457292	1038.348481	14.999629
21.142918	1045.351178	15.004647
21.658393	1052.922746	15.009664
21.696096	1058.658534	15.014682
21.466911	1063.492486	15.019699
21.811971	1059.191515	15.024717
21.630389	1068.428061	15.029735
21.981925	1064.520097	15.034752
21.812898	1053.457642	15.039770
21.498031	1055.146837	15.044787
22.066876	1053.601627	15.049805
21.700858	1045.103989	15.054823
21.821161	1046.537275	15.059840
21.934708	1040.032206	15.064858
21.790673	1032.236768	15.069875
21.640017	1050.416671	15.074893
21.910700	1059.643284	15.079911
21.934435	1065.815230	15.084928
22.133976	1065.490578	15.089946
22.005622	1063.589173	15.094963
22.190703	1053.606627	15.099981
21.900712	1049.172237	15.104999
22.086126	1050.480573	15.110016
22.439478	1033.938130	15.115034
22.154528	1034.937749	15.120051
22.141406	1030.949234	15.125069
22.103253	1031.087939	15.130087
21.775952	1026.106605	15.135104
21.839536	1015.586347	15.140122
21.964255	1053.376219	15.145139
22.462859	1046.017653	15.150157
22.275675	1050.028928	15.155175
22.308656	1053.353378	15.160192
21.891572	1045.063401	15.165210
22.027247	1046.164233	15.170227
22.131631	1050.672486	15.175245
22.216093	1056.667844	15.180263
22.107460	1056.773733	15.185280
22.545098	1055.694721	15.190298
22.116633	1059.864449	15.195315
22.315000	1059.405350	15.200333
22.540698	1059.943658	15.205351
22.318656	1054.273650	15.210368
22.422107	1060.515463	15.215386
22.130544	1061.650031	15.220403
22.495745	1060.315700	15.225421
22.372598	1064.236457	15.230439
22.227962	1066.279342	15.235456
22.053117	1054.148202	15.240474
22.175594	1067.593304	15.245491
22.377895	1076.797393	15.250509
22.280427	1081.350888	15.255527
22.374232	1087.538405	15.260544
22.592026	1088.574464	15.265562
22.626319	1089.592089	15.270579
22.579214	1084.161204	15.275597
22.898821	1089.094446	15.280615
22.747843	1096.599621	15.285632
22.782255	1093.292567	15.290650
22.522955	1089.545580	15.295667
22.619260	1086.207807	15.300685
22.698700	1084.506631	15.305703
22.672085	1087.888199	15.310720
22.714594	1088.255667	15.315738
22.515153	1088.518320	15.320755
23.123902	1101.449878	15.325773
23.295647	1102.108929	15.330791
23.227850	1092.315075	15.335808
23.327769	1070.109236	15.340826
23.403926	1080.716844	15.345843
23.638982	1074.732173	15.350861
23.794116	1065.804148	15.355879
23.568779	1074.051126	15.360896
23.550124	1053.574728	15.365914
23.301494	1050.240536	15.370931
22.892934	1041.149178	15.375949
22.967916	1037.593695	15.380967
22.845814	1031.003243	15.385984
23.091436	1046.953434	15.391002
22.944747	1064.222887	15.396019
23.310097	1069.361533	15.401037
23.052038	1077.445827	15.406055
23.191438	1067.163760	15.411072
23.556307	1065.061400	15.416090
23.608748	1068.555854	15.421107
23.450172	1071.629359	15.426125
23.490433	1069.343747	15.431143
23.487093	1062.013563	15.436160
23.502770	1052.016943	15.441178
23.347826	1067.444526	15.446195
23.644270	1062.832718	15.451213
23.744961	1065.922345	15.456231
23.597087	1061.391194	15.461248
23.781472	1045.768417	15.466266
22.919713	1046.385609	15.471283
23.401712	1054.623720	15.476301
23.673880	1060.647053	15.481319
22.945141	1063.155932	15.486336
23.402477	1056.468738	15.491354
23.391915	1065.500986	15.496371
23.290469	1063.007351	15.501389
23.329768	1064.730027	15.506407
23.182782	1072.883326	15.511424
23.727854	1090.146924	15.516442
23.745637	1095.135262	15.521459
24.106949	1098.741960	15.526477
24.041840	1097.948939	15.531495
23.891448	1102.652537	15.536512
24.309860	1087.025613	15.541530
23.642909	1079.775382	15.546547
23.972895	1082.058568	15.551565
24.048821	1085.363316	15.556583
23.639145	1077.639792	15.561600
23.814106	1086.819281	15.566618
23.937800	1091.406629	15.571635
24.132975	1095.787267	15.576653
24.445074	1094.243622	15.581671
23.990983	1103.751288	15.586688
24.063357	1095.539288	15.591706
24.299855	1095.661650	15.596723
24.182887	1092.770200	15.601741
23.991209	1087.007359	15.606759
24.177914	1092.422829	15.611776
24.522928	1093.940168	15.616794
24.155196	1097.597111	15.621811
24.304487	1100.072025	15.626829
24.479495	1092.918588	15.631847
23.963421	1085.056384	15.636864
24.112647	1098.151820	15.641882
24.308711	1100.229632	15.646899
24.190544	1103.936195	15.651917
24.358875	1099.566055	15.656935
24.158721	1098.034790	15.661952
24.384327	1099.992754	15.666970
24.153982	1094.464258	15.671987
24.186674	1099.183208	15.677005
24.502321	1092.900943	15.682023
24.322940	1103.261911	15.687040
24.352685	1096.183705	15.692058
24.198688	1093.594045	15.697075
24.410616	1117.870875	15.702093
24.613670	1117.011405	15.707111
24.589953	1125.249041	15.712128
24.698796	1122.365076	15.717146
24.611359	1134.995021	15.722163
24.800963	1130.280415	15.727181
25.183715	1120.856416	15.732199
24.684088	1123.146271	15.737216
25.073629	1118.103690	15.742234
24.931400	1126.700310	15.747251
24.694654	1130.229276	15.752269
24.941004	1126.268243	15.757287
24.886809	1127.753265	15.762304
24.873474	1119.940865	15.767322
25.023963	1128.573661	15.772339
24.985810	1130.942613	15.777357
25.089232	1122.562472	15.782375
24.752670	1130.648375	15.787392
25.126468	1123.311620	15.792410
25.300427	1118.066553	15.797427
25.220501	1119.634966	15.802445
25.226396	1118.720742	15.807463
25.031906	1122.636792	15.812480
25.117157	1120.742529	15.817498
25.269300	1126.869223	15.822515
25.154113	1128.930468	15.827533
25.138905	1118.856245	15.832551
24.671561	1129.947567	15.837568
25.019918	1123.211463	15.842586
25.058701	1115.195560	15.847603
24.694661	1124.736358	15.852621
24.994350	1112.660452	15.857639
24.843039	1125.451749	15.862656
25.280352	1138.586917	15.867674
25.412569	1142.062273	15.872691
25.417974	1151.135627	15.877709
25.629654	1141.991115	15.882727
25.498362	1149.002519	15.887744
25.394016	1143.565737	15.892762
25.851253	1143.415730	15.897779
25.650223	1149.907202	15.902797
25.689231	1134.533203	15.907815
25.729623	1142.255131	15.912832
25.661204	1146.795174	15.917850
25.899603	1142.766559	15.922867
25.572144	1132.911740	15.927885
25.826678	1128.669833	15.932903
25.532887	1123.286867	15.937920
25.836025	1127.033122	15.942938
25.839341	1139.272465	15.947955
25.617447	1145.487870	15.952973
25.782465	1143.268989	15.957991
25.394457	1152.452760	15.963008
25.339090	1138.174668	15.968026
25.753486	1136.609750	15.973043
25.747139	1144.358315	15.978061
26.093143	1137.363547	15.983079
25.933290	1143.645448	15.988096
25.882140	1145.617748	15.993114
26.115175	1141.106177	15.998131
25.876279	1142.470212	16.003149
26.008476	1134.177029	16.008167
26.095700	1145.237952	16.013184
26.007031	1139.006868	16.018202
26.255533	1144.541647	16.023219
26.125563	1139.345717	16.028237
26.083993	1136.688618	16.033255
25.851751	1135.622884	16.038272
26.000993	1152.204872	16.043290
26.459601	1165.605033	16.048307
26.072745	1170.171827	16.053325
26.235787	1168.715452	16.058343
26.141521	1171.921238	16.063360
26.163212	1180.234847	16.068378
26.514888	1176.766584	16.073395
26.234053	1178.854476	16.078413
26.306205	1166.516213	16.083431
26.158829	1171.749633	16.088448
26.279132	1170.317264	16.093466
26.584221	1163.775703	16.098483
26.043025	1167.818854	16.103501
26.748127	1176.998802	16.108519
26.395181	1194.277749	16.113536
26.897054	1188.682702	16.118554
26.892238	1196.023964	16.123571
26.878527	1174.432837	16.128589
26.813910	1163.008930	16.133607
26.802493	1165.683294	16.138624
26.728258	1153.207080	16.143642
26.866362	1158.605818	16.148659
26.521589	1158.400424	16.153677
26.623541	1158.945053	16.158695
26.962892	1175.426299	16.163712
26.687138	1185.122589	16.168730
27.304208	1191.208939	16.173747
26.955949	1179.702855	16.178765
27.076548	1163.474790	16.183783
26.659701	1167.881199	16.188800
26.787846	1180.077465	16.193818
27.335435	1187.805195	16.198835
27.368775	1193.455931	16.203853
27.371414	1177.386356	16.208871
27.194878	1166.531356	16.213888
26.898782	1158.261047	16.218906
26.973221	1152.021847	16.223923
26.832069	1170.464483	16.228941
27.180990	1181.376198	16.233959
27.233859	1191.238545	16.238976
27.205482	1188.680037	16.243994
27.312764	1184.018414	16.249011
27.166300	1192.331921	16.254029
27.307889	1192.450708	16.259047
27.103813	1184.421047	16.264064
26.884095	1182.555227	16.269082
27.397037	1180.597620	16.274099
27.496836	1180.897732	16.279117
27.181492	1180.424874	16.284135
27.378806	1183.801667	16.289152
27.154328	1184.682229	16.294170
27.391961	1188.512965	16.299187
27.495419	1209.734755	16.304205
27.441994	1213.877857	16.309223
27.979137	1210.650130	16.314240
27.680733	1219.904928	16.319258
27.901901	1202.446421	16.324275
27.745481	1203.204301	16.329293
27.826873	1200.143376	16.334311
28.069993	1191.197954	16.339328
27.546816	1183.237665	16.344346
27.809954	1175.210960	16.349363
27.884472	1204.886514	16.354381
27.911386	1209.752120	16.359399
27.988712	1195.952384	16.364416
28.113360	1200.375044	16.369434
28.076809	1187.242187	16.374451
27.679700	1190.437098	16.379469
27.731072	1193.001861	16.384487
28.214374	1204.070077	16.389504
27.956882	1220.850978	16.394522
28.104611	1212.304794	16.399539
28.408952	1214.873736	16.404557
28.214833	1218.860218	16.409575
28.248431	1214.873369	16.414592
28.062135	1218.806589	16.419610
28.556075	1208.017704	16.424627
28.107420	1210.230629	16.429645
28.236417	1209.339323	16.434663
28.631273	1209.011461	16.439680
28.490643	1210.716702	16.444698
28.256818	1184.621573	16.449715
27.861420	1191.920421	16.454733
28.435969	1194.837521	16.459751
28.246713	1206.124578	16.464768
28.078079	1212.952041	16.469786
28.492457	1205.684904	16.474803
28.195354	1208.183751	16.479821
28.180177	1212.090604	16.484839
28.371421	1207.129253	16.489856
28.371161	1213.625695	16.494874
28.517357	1202.619991	16.499891
28.474570	1206.906601	16.504909
28.503640	1220.942486	16.509927
29.244866	1223.235945	16.514944
28.922551	1235.233227	16.519962
29.237362	1219.387896	16.524979
28.664067	1212.105559	16.529997
28.787191	1210.228636	16.535015
29.170431	1201.354100	16.540032
29.015828	1208.605211	16.545050
28.910969	1197.565491	16.550067
28.927674	1200.997390	16.555085
28.603647	1198.052411	16.560103
29.018474	1199.033806	16.565120
28.664750	1194.527252	16.570138
28.891309	1196.964192	16.575155
28.935494	1212.650672	16.580173
28.927321	1216.150471	16.585191
28.827172	1229.224713	16.590208
28.700106	1226.321524	16.595226
29.006161	1218.960509	16.600243
28.769131	1226.100083	16.605261
28.729892	1225.330330	16.610279
29.218483	1216.590700	16.615296
28.786946	1234.318915	16.620314
29.172807	1236.779089	16.625331
29.426433	1245.718881	16.630349
29.240511	1251.633891	16.635367
29.494509	1245.660978	16.640384
29.340451	1249.215648	16.645402
29.634110	1242.142889	16.650419
29.275572	1251.624586	16.655437
29.405654	1251.003958	16.660455
29.842854	1252.211568	16.665472
29.821790	1246.861746	16.670490
29.965745	1248.819469	16.675507
29.894624	1251.074610	16.680525
29.468684	1248.202401	16.685543
29.912797	1247.863626	16.690560
30.057575	1246.023664	16.695578
29.757185	1241.062212	16.700595
29.548772	1230.033710	16.705613
29.759414	1238.411731	16.710631
30.129650	1232.981375	16.715648
29.778577	1240.078422	16.720666
30.013514	1242.898225	16.725683
29.830145	1242.073598	16.730701
29.773723	1253.307987	16.735719
29.877112	1244.981720	16.740736
29.950608	1244.318888	16.745754
30.018009	1242.369694	16.750771
29.601955	1244.606752	16.755789
29.878045	1243.108425	16.760807
30.125164	1245.645903	16.765824
30.093389	1244.089893	16.770842
30.318442	1238.287914	16.775859
30.650030	1237.843759	16.780877
30.322667	1243.454634	16.785895
30.326482	1243.458836	16.790912
30.292067	1243.031977	16.795930
30.180005	1245.774987	16.800947
30.087617	1231.145073	16.805965
30.038381	1236.592180	16.810983
29.931632	1232.242354	16.816000
30.083408	1244.991044	16.821018
30.039931	1255.743774	16.826035
30.527544	1261.883871	16.831053
30.232117	1268.534720	16.836071
30.697518	1269.427827	16.841088
30.487298	1271.976469	16.846106
30.531834	1268.956671	16.851123
30.796957	1276.104853	16.856141
30.513308	1273.518520	16.861159
30.762740	1265.218060	16.866176
30.471966	1272.151992	16.871194
30.910091	1267.815871	16.876211
30.658012	1269.055724	16.881229
30.439378	1280.207150	16.886247
30.715557	1261.037143	16.891264
30.639775	1263.338332	16.896282
30.771646	1266.067727	16.901299
31.077473	1284.249090	16.906317
31.052802	1295.206604	16.911335
30.949586	1273.066391	16.916352
30.972475	1280.203897	16.921370
31.060818	1289.892327	16.926387
31.424900	1295.065117	16.931405
31.318035	1285.786654	16.936423
31.409402	1258.686000	16.941440
31.041386	1262.433577	16.946458
30.866332	1257.299795	16.951475
31.220015	1262.922711	16.956493
31.347479	1268.184669	16.961511
31.418604	1264.100651	16.966528
31.278264	1257.072187	16.971546
31.361200	1253.268492	16.976563
31.468801	1256.100327	16.981581
31.532159	1257.406845	16.986599
31.531322	1257.763778	16.991616
31.629581	1255.616170	16.996634
31.529554	1245.543703	17.001651
31.895789	1240.123062	17.006669
31.514662	1247.151469	17.011687
31.584523	1244.663690	17.016704
31.402613	1248.323757	17.021722
31.588642	1250.948121	17.026739
31.301711	1256.203495	17.031757
31.154329	1267.816333	17.036775
31.869161	1272.808600	17.041792
31.849165	1277.640263	17.046810
31.597999	1277.811879	17.051827
32.082486	1274.983795	17.056845
32.115788	1283.245144	17.061863
32.074278	1278.900250	17.066880
31.860896	1284.961155	17.071898
32.021095	1289.414962	17.076915
31.881881	1284.506334	17.081933
31.891602	1281.620642	17.086951
32.307683	1274.656728	17.091968
32.344510	1284.274552	17.096986
32.298966	1282.213742	17.102003
32.614575	1277.925069	17.107021
32.282159	1281.300228	17.112039
32.231965	1281.183848	17.117056
32.388583	1281.496994	17.122074
32.286838	1277.534507	17.127091
32.503679	1280.990764	17.132109
32.458249	1267.277824	17.137127
32.305336	1251.554787	17.142144
32.170567	1252.347666	17.147162
32.254324	1267.070978	17.152179
32.312035	1280.443134	17.157197
32.178151	1280.851230	17.162215
32.656251	1278.136012	17.167232
32.400639	1278.664262	17.172250
32.458677	1273.364323	17.177267
32.786468	1275.172716	17.182285
32.377458	1277.887736	17.187303
32.468207	1275.959475	17.192320
32.380288	1278.472120	17.197338
32.122458	1282.681762	17.202355
32.607009	1286.455497	17.207373
32.779811	1295.730741	17.212391
32.763854	1306.559263	17.217408
32.671202	1303.488160	17.222426
32.569580	1308.906172	17.227443
32.936329	1303.984233	17.232461
32.875724	1305.290415	17.237479
32.946028	1307.553642	17.242496
33.015474	1296.768056	17.247514
33.201023	1299.166528	17.252531
33.066576	1302.978194	17.257549
33.011484	1311.556944	17.262567
33.438463	1303.072739	17.267584
33.385709	1297.267919	17.272602
33.039351	1300.718617	17.277619
33.206974	1304.767663	17.282637
32.861238	1309.191076	17.287655
32.805476	1305.391831	17.292672
33.165141	1306.421343	17.297690
33.049620	1307.068127	17.302707
33.215595	1321.266864	17.307725
33.584027	1331.973884	17.312743
33.546274	1333.413684	17.317760
33.541847	1326.772913	17.322778
33.427718	1333.281567	17.327795
33.800243	1318.655298	17.332813
33.588895	1326.734349	17.337831
33.503972	1328.852419	17.342848
33.872872	1318.122744	17.347866
33.624011	1331.699640	17.352883
34.083423	1331.794938	17.357901
33.746180	1327.173805	17.362919
33.819021	1327.826409	17.367936
33.808436	1334.660433	17.372954
33.290231	1326.476021	17.377971
33.926367	1330.816389	17.382989
33.643271	1333.123963	17.388007
33.963004	1317.489132	17.393024
33.674079	1320.656314	17.398042
33.706933	1320.987592	17.403059
34.156821	1315.105050	17.408077
33.881125	1322.781769	17.413095
34.069341	1314.763461	17.418112
34.066051	1319.473476	17.423130
34.271713	1344.017442	17.428147
34.508356	1342.027615	17.433165
34.057240	1330.726240	17.438183
34.253177	1346.724731	17.443200
34.716664	1346.389047	17.448218
34.329247	1329.774459	17.453235
34.283296	1333.750611	17.458253
34.226841	1346.627169	17.463271
34.331109	1345.263974	17.468288
34.427122	1337.273913	17.473306
34.273411	1347.312688	17.478323
34.721329	1345.054417	17.483341
34.864168	1341.693531	17.488359
34.907049	1339.269259	17.493376
34.701774	1348.349660	17.498394
34.895143	1350.062999	17.503411
35.028158	1337.034218	17.508429
34.813554	1341.434353	17.513447
34.816180	1341.645835	17.518464
34.672321	1334.204146	17.523482
34.699987	1342.076703	17.528499
34.908918	1337.432849	17.533517
34.950520	1332.163170	17.538535
34.740221	1348.536008	17.543552
34.965436	1339.628505	17.548570
34.869356	1342.386209	17.553587
34.970559	1330.360322	17.558605
34.822908	1345.247613	17.563623
35.090188	1329.365553	17.568640
35.062987	1333.313797	17.573658
34.805198	1340.006081	17.578675
35.022029	1339.017943	17.583693
34.965851	1341.906832	17.588711
34.980731	1364.369464	17.593728
35.600805	1362.443703	17.598746
35.265477	1370.861017	17.603763
34.829194	1372.478223	17.608781
34.956661	1369.449005	17.613799
35.422090	1362.346569	17.618816
35.473695	1369.982896	17.623834
35.268508	1373.825584	17.628851
35.448455	1370.685315	17.633869
35.370563	1372.991594	17.638887
35.172338	1371.069830	17.643904
35.671365	1379.392305	17.648922
35.211109	1397.558918	17.653939
35.529254	1386.565557	17.658957
35.658773	1392.864998	17.663975
35.875666	1402.307413	17.668992
36.171029	1388.841871	17.674010
36.066168	1389.916809	17.679027
36.080060	1387.089461	17.684045
36.166854	1385.735061	17.689063
35.838927	1386.444970	17.694080
36.271980	1377.697911	17.699098
36.159893	1380.790156	17.704115
36.533516	1387.150357	17.709133
36.412162	1382.599366	17.714151
36.402096	1368.557257	17.719168
36.470162	1359.226164	17.724186
36.260625	1349.887105	17.729203
36.403621	1351.074147	17.734221
36.442677	1352.213834	17.739239
36.183655	1352.479269	17.744256
36.791104	1348.641459	17.749274
36.416089	1352.133527	17.754291
36.365939	1339.511444	17.759309
36.159977	1353.136766	17.764327
36.203866	1347.272619	17.769344
36.382221	1354.836378	17.774362
36.307092	1381.656389	17.779379
36.657302	1376.293077	17.784397
36.630616	1378.186160	17.789415
36.413837	1380.776850	17.794432
36.693057	1376.146149	17.799450
36.538314	1381.686366	17.804467
36.531359	1376.643213	17.809485
36.689917	1381.355975	17.814503
36.337962	1373.506998	17.819520
36.523177	1375.142163	17.824538
36.439090	1399.908600	17.829555
36.762617	1406.274741	17.834573
37.302638	1400.325670	17.839591
36.745391	1405.039640	17.844608
36.938514	1399.795243	17.849626
36.995996	1401.079912	17.854643
37.153757	1402.219238	17.859661
37.280254	1391.732009	17.864679
37.082416	1396.556149	17.869696
37.185710	1392.525824	17.874714
37.314038	1395.528660	17.879731
37.311708	1390.173717	17.884749
37.395161	1393.245399	17.889767
37.107531	1402.733557	17.894784
37.756012	1403.697932	17.899802
37.628505	1405.918338	17.904819
37.416530	1400.271337	17.909837
37.387262	1392.680726	17.914855
37.503297	1402.510703	17.919872
38.022055	1408.692553	17.924890
37.822836	1405.720175	17.929907
37.605032	1405.716585	17.934925
37.887666	1398.148736	17.939943
37.249598	1402.223733	17.944960
37.897113	1406.247284	17.949978
38.001646	1418.835832	17.954995
37.970583	1415.559629	17.960013
37.860531	1406.958384	17.965031
37.910905	1404.662388	17.970048
37.835106	1413.361551	17.975066
37.782082	1418.806593	17.980083
38.040663	1424.722084	17.985101
38.225185	1430.280159	17.990119
38.051547	1432.876313	17.995136
38.388020	1438.447025	18.000154
38.057780	1435.957748	18.005171
38.131349	1425.943034	18.010189
38.277246	1427.519362	18.015207
37.640807	1426.254000	18.020224
37.927995	1422.628648	18.025242
37.906906	1425.926304	18.030259
38.104912	1441.347786	18.035277
38.470342	1440.356690	18.040295
38.104861	1456.184082	18.045312
38.395387	1457.707332	18.050330
38.382964	1455.208342	18.055347
38.314164	1453.623008	18.060365
38.344461	1449.857115	18.065383
38.489638	1462.730699	18.070400
38.360580	1451.991651	18.075418
38.876743	1465.616008	18.080435
39.010779	1466.032109	18.085453
39.321602	1469.650405	18.090471
39.025818	1463.425137	18.095488
38.930000	1448.244016	18.100506
38.813725	1457.042818	18.105523
38.936308	1452.487242	18.110541
39.062465	1437.097726	18.115559
38.588601	1448.763969	18.120576
39.170331	1458.076325	18.125594
39.329819	1465.210590	18.130611
39.186937	1467.445361	18.135629
39.546462	1465.836349	18.140647
39.629187	1470.651065	18.145664
39.374025	1453.261303	18.150682
39.043406	1442.414692	18.155699
39.214713	1452.052479	18.160717
39.659450	1457.184805	18.165735
39.418526	1466.695977	18.170752
39.616384	1463.210207	18.175770
39.574986	1466.983279	18.180787
39.625939	1461.897833	18.185805
39.565909	1461.692530	18.190823
39.727421	1465.442633	18.195840
39.656821	1453.827377	18.200858
39.619465	1459.767473	18.205875
39.857388	1465.417505	18.210893
39.674618	1458.566839	18.215911
39.494255	1459.549953	18.220928
39.756142	1463.650755	18.225946
39.954116	1465.092874	18.230963
39.839702	1463.098561	18.235981
40.054197	1458.005722	18.240999
39.981504	1458.809593	18.246016
39.794311	1450.050626	18.251034
40.294537	1452.111195	18.256051
39.892596	1461.310052	18.261069
39.913375	1458.252813	18.266087
39.733066	1461.067790	18.271104
40.214447	1474.779015	18.276122
40.377654	1470.223007	18.281139
40.557106	1479.001596	18.286157
40.446913	1475.075495	18.291175
40.600494	1476.493470	18.296192
40.609216	1475.122856	18.301210
40.200440	1458.958906	18.306227
40.332415	1466.325677	18.311245
40.794853	1473.025536	18.316263
40.281941	1481.024678	18.321280
40.591584	1468.257091	18.326298
40.613205	1478.275581	18.331315
40.517379	1480.643506	18.336333
40.920475	1479.034759	18.341351
40.829722	1484.560087	18.346368
40.790274	1478.362054	18.351386
40.818533	1474.177598	18.356403
40.794459	1488.693781	18.361421
40.889024	1481.308999	18.366439
40.751481	1478.639779	18.371456
40.765109	1485.142303	18.376474
41.457813	1470.467209	18.381491
40.834000	1475.246157	18.386509
40.945591	1474.912044	18.391527
41.285887	1486.178945	18.396544
41.383276	1498.753387	18.401562
41.498902	1494.856820	18.406579
41.151955	1494.073437	18.411597
41.427501	1489.919292	18.416615
41.370193	1503.128008	18.421632
41.456488	1499.026062	18.426650
41.760482	1501.838023	18.431667
41.524942	1507.970005	18.436685
41.388891	1507.185166	18.441703
41.380988	1509.637750	18.446720
41.508715	1503.031714	18.451738
41.566267	1504.212444	18.456755
41.478893	1509.399821	18.461773
41.474540	1503.603051	18.466791
41.494924	1511.987921	18.471808
41.428671	1502.075836	18.476826
41.922873	1511.995627	18.481843
41.990941	1524.987542	18.486861
41.933085	1526.270452	18.491879
41.915195	1533.969155	18.496896
42.112146	1532.181151	18.501914
42.267689	1525.845302	18.506931
41.956572	1532.001618	18.511949
42.175947	1524.620560	18.516967
42.097731	1528.370215	18.521984
42.014777	1530.368301	18.527002
42.252137	1523.801978	18.532019
42.187823	1522.431641	18.537037
42.259466	1524.904127	18.542055
42.283355	1522.237697	18.547072
42.447425	1523.711026	18.552090
42.550764	1519.617669	18.557107
42.438720	1523.915441	18.562125
42.613258	1515.587091	18.567143
42.422569	1520.092764	18.572160
42.278823	1532.561492	18.577178
42.813135	1539.434124	18.582195
42.774947	1548.866108	18.587213
42.857469	1540.914791	18.592231
42.842097	1548.305211	18.597248
42.697500	1547.074149	18.602266
43.136920	1542.736557	18.607283
42.909291	1556.014071	18.612301
43.164421	1546.762128	18.617319
43.009846	1545.978385	18.622336
43.135264	1538.090045	18.627354
43.221258	1545.606593	18.632371
42.963327	1545.160829	18.637389
43.120491	1545.299876	18.642407
42.817941	1547.720543	18.647424
42.985419	1556.469663	18.652442
42.894630	1541.636041	18.657459
42.524394	1553.813155	18.662477
43.016365	1567.436489	18.667495
42.927909	1567.566205	18.672512
43.281334	1571.384951	18.677530
43.740793	1577.507398	18.682547
43.558453	1569.999526	18.687565
43.742552	1563.451847	18.692583
43.959406	1572.968782	18.697600
43.694897	1571.326078	18.702618
43.928930	1569.803582	18.707635
43.770396	1568.001599	18.712653
43.658529	1565.971811	18.717671
43.956082	1563.878170	18.722688
43.536015	1566.403731	18.727706
43.867518	1565.809584	18.732723
43.875874	1596.883454	18.737741
44.223203	1592.083145	18.742759
44.321145	1586.281611	18.747776
44.517815	1586.838527	18.752794
44.507032	1563.038502	18.757811
44.101853	1557.036426	18.762829
44.490387	1554.543472	18.767847
44.481606	1552.903309	18.772864
44.431215	1559.457016	18.777882
44.432020	1549.672379	18.782899
44.466282	1553.932155	18.787917
44.521122	1557.628290	18.792935
44.789727	1547.416638	18.797952
44.639243	1555.739272	18.802970
44.585166	1546.511361	18.807987
44.403101	1552.617971	18.813005
44.885509	1563.837383	18.818023
44.724655	1556.938949	18.823040
44.769852	1577.159476	18.828058
44.934419	1572.461481	18.833075
45.021283	1577.067670	18.838093
45.051007	1585.652214	18.843111
45.086329	1581.928764	18.848128
44.966963	1581.052970	18.853146
45.341107	1573.578153	18.858163
44.759377	1567.511211	18.863181
44.803536	1575.910288	18.868199
44.963878	1586.543674	18.873216
44.990039	1583.944967	18.878234
44.992702	1579.634800	18.883251
44.884690	1581.648853	18.888269
44.799605	1579.539039	18.893287
45.184004	1583.631006	18.898304
45.243061	1616.018960	18.903322
45.720098	1604.127089	18.908339
45.571073	1618.849909	18.913357
45.915941	1606.940551	18.918375
45.645605	1609.657075	18.923392
45.574029	1616.099746	18.928410
45.482739	1603.937410	18.933427
45.702769	1603.224316	18.938445
45.623923	1612.709135	18.943463
45.838537	1597.242215	18.948480
45.454704	1605.772804	18.953498
45.949241	1599.576072	18.958515
45.968074	1602.020700	18.963533
45.946967	1608.850681	18.968551
46.186441	1607.380824	18.973568
45.891581	1604.839598	18.978586
45.941136	1610.804731	18.983603
45.893389	1619.091490	18.988621
46.220623	1626.247662	18.993639
46.119921	1631.535318	18.998656
46.277435	1635.930615	19.003674
46.411889	1641.143118	19.008691
46.195105	1634.155880	19.013709
46.269232	1632.548043	19.018727
46.635387	1624.743815	19.023744
46.476150	1632.933688	19.028762
46.680280	1625.378728	19.033779
46.808854	1626.426447	19.038797
46.563244	1630.584158	19.043815
46.765097	1623.928790	19.048832
46.653299	1621.471424	19.053850
46.455455	1622.459804	19.058867
46.928580	1632.128439	19.063885
46.900720	1646.639097	19.068903
46.909278	1649.344096	19.073920
46.972927	1662.018352	19.078938
47.403487	1655.495575	19.083955
47.283924	1653.640279	19.088973
47.275928	1656.233452	19.093991
47.553710	1642.646586	19.099008
47.428811	1633.887830	19.104026
47.654571	1617.162744	19.109043
47.455565	1614.488716	19.114061
47.371176	1612.279569	19.119079
47.528152	1610.475734	19.124096
47.556414	1614.898724	19.129114
47.591561	1607.294981	19.134131
47.590065	1614.070143	19.139149
47.180884	1622.093913	19.144167
47.925607	1629.418363	19.149184
47.523845	1637.041699	19.154202
47.417636	1648.121231	19.159219
47.752534	1644.307612	19.164237
47.592466	1638.765315	19.169255
47.752713	1640.936140	19.174272
47.455044	1648.386341	19.179290
47.775014	1629.560205	19.184307
48.003061	1647.319836	19.189325
47.872107	1663.999948	19.194343
48.197292	1659.914311	19.199360
48.045125	1661.536077	19.204378
48.537768	1663.641633	19.209395
48.725577	1657.539759	19.214413
48.676854	1664.435755	19.219431
48.909129	1651.872561	19.224448
48.727101	1638.143721	19.229466
48.566514	1622.862128	19.234483
48.662795	1625.640394	19.239501
48.665315	1633.665688	19.244519
48.817199	1623.634730	19.249536
48.735914	1632.348704	19.254554
48.865951	1624.483177	19.259571
48.682882	1631.466363	19.264589
48.617741	1626.880795	19.269607
48.825645	1615.525604	19.274624
48.542100	1623.260069	19.279642
48.732399	1634.114906	19.284659
48.668853	1642.420042	19.289677
48.867471	1648.643186	19.294695
49.069918	1647.151898	19.299712
49.007108	1665.504592	19.304730
48.783634	1657.804274	19.309747
49.008300	1656.134108	19.314765
49.045200	1662.776949	19.319783
49.167237	1649.811929	19.324800
49.112370	1665.378261	19.329818
49.218519	1675.529340	19.334835
49.376443	1682.498610	19.339853
49.201214	1690.995099	19.344871
49.231140	1687.794961	19.349888
49.463292	1688.176319	19.354906
49.487965	1689.745186	19.359923
49.738724	1677.882458	19.364941
49.338001	1690.622996	19.369959
49.699329	1680.574645	19.374976
49.769589	1690.249785	19.379994
49.837113	1701.837993	19.385011
50.043329	1707.713444	19.390029
50.340030	1705.014017	19.395047
50.477496	1701.203941	19.400064
50.217631	1686.448963	19.405082
50.084903	1668.820181	19.410099
50.558047	1667.630922	19.415117
49.666299	1670.427117	19.420135
50.084024	1683.680563	19.425152
50.190874	1692.770116	19.430170
50.447868	1694.103665	19.435187
50.412143	1695.018750	19.440205
50.335687	1697.690196	19.445223
50.528036	1698.424209	19.450240
50.803739	1698.838909	19.455258
50.494885	1700.585836	19.460275
50.513437	1694.527326	19.465293
50.608932	1699.774253	19.470311
50.480272	1689.693640	19.475328
50.566210	1701.765810	19.480346
50.655298	1711.617767	19.485363
51.034432	1719.881538	19.490381
50.850370	1726.132249	19.495399
51.430117	1720.653256	19.500416
51.303625	1725.465684	19.505434
50.931224	1729.732604	19.510451
51.544774	1711.627056	19.515469
50.840014	1724.186858	19.520487
50.959928	1727.197057	19.525504
51.138228	1723.388089	19.530522
51.449523	1721.541367	19.535539
51.790368	1722.122841	19.540557
51.513919	1719.736422	19.545575
51.529410	1716.082365	19.550592
51.382838	1717.514628	19.555610
51.173963	1719.900913	19.560627
51.378578	1730.117615	19.565645
51.789523	1750.460094	19.570663
51.678457	1744.975788	19.575680
51.769417	1749.440011	19.580698
51.682374	1750.292335	19.585715
51.934526	1744.294736	19.590733
51.547826	1758.425145	19.595751
51.792340	1749.649647	19.600768
51.918565	1745.650081	19.605786
52.053699	1766.422897	19.610803
52.251616	1772.758020	19.615821
52.183529	1778.055681	19.620839
52.440362	1776.448288	19.625856
52.592601	1778.959045	19.630874
52.568310	1772.754054	19.635891
52.587035	1760.692671	19.640909
52.377687	1752.630908	19.645927
52.622027	1757.196904	19.650944
52.969626	1763.494642	19.655962
52.458663	1753.815872	19.660979
52.252255	1745.764649	19.665997
52.322778	1763.654433	19.671015
52.528051	1759.163424	19.676032
52.728183	1762.780040	19.681050
52.598968	1764.381874	19.686067
52.835745	1765.735314	19.691085
52.491124	1773.194136	19.696103
52.859498	1783.414862	19.701120
53.146780	1787.339891	19.706138
53.077106	1797.912293	19.711155
53.319801	1803.058110	19.716173
53.425805	1796.848859	19.721191
53.535736	1794.257901	19.726208
53.385132	1790.632903	19.731226
53.323587	1795.905470	19.736243
53.603007	1786.548181	19.741261
53.487753	1791.553652	19.746279
53.572590	1797.961052	19.751296
53.719700	1790.067418	19.756314
53.715292	1794.876583	19.761331
53.697876	1783.676688	19.766349
53.533842	1787.642979	19.771367
53.757751	1786.809549	19.776384
53.747703	1793.148011	19.781402
53.588108	1796.767502	19.786419
54.340349	1810.602293	19.791437
54.122791	1812.743964	19.796455
54.145010	1815.480982	19.801472
54.165125	1820.768778	19.806490
54.112163	1817.180363	19.811507
54.381314	1811.585440	19.816525
54.437549	1816.681425	19.821543
54.383610	1815.212493	19.826560
54.439018	1815.182168	19.831578
54.289720	1814.042021	19.836595
54.606141	1812.731061	19.841613
54.419899	1822.278672	19.846631
54.637081	1808.039482	19.851648
54.637357	1805.113524	19.856666
54.363114	1819.788368	19.861683
54.511675	1806.507798	19.866701
54.926126	1829.842754	19.871719
54.895474	1832.955857	19.876736
55.212232	1834.004717	19.881754
54.879515	1832.667769	19.886771
55.246439	1821.173499	19.891789
55.253918	1829.660285	19.896807
55.404165	1827.539031	19.901824
55.516016	1830.014358	19.906842
55.360742	1832.824468	19.911859
55.820442	1827.469648	19.916877
55.118260	1829.399038	19.921895
55.556820	1829.921818	19.926912
55.739183	1832.400824	19.931930
55.490313	1834.144133	19.936947
55.621553	1821.274298	19.941965
55.554231	1828.281322	19.946983
55.728428	1831.971934	19.952000
55.836541	1828.311177	19.957018
55.835845	1823.988506	19.962035
55.951128	1827.642020	19.967053
55.665620	1826.213397	19.972071
55.795407	1824.157737	19.977088
55.698141	1827.099582	19.982106
55.205728	1830.443080	19.987123
55.847786	1853.045099	19.992141
56.216152	1859.142978	19.997159
55.886666	1859.924424	20.002176
56.266499	1861.725454	20.007194
56.373725	1849.520606	20.012211
56.280010	1851.866584	20.017229
56.324798	1862.507087	20.022247
56.256495	1862.708273	20.027264
56.312988	1867.414067	20.032282
56.534579	1880.942288	20.037299
56.859769	1871.134055	20.042317
56.919548	1868.629736	20.047335
57.143205	1869.460939	20.052352
57.029569	1865.311683	20.057370
57.100373	1866.513869	20.062387
57.018584	1870.244513	20.067405
56.711861	1870.659980	20.072423
57.049562	1869.643136	20.077440
57.049887	1863.772620	20.082458
56.675391	1868.962381	20.087475
56.954360	1862.529580	20.092493
56.958715	1871.922827	20.097511
57.117667	1887.550830	20.102528
57.595862	1889.581645	20.107546
57.436406	1900.000474	20.112563
57.544668	1896.754252	20.117581
57.676296	1897.013281	20.122599
57.893385	1887.704441	20.127616
57.629172	1888.769575	20.132634
57.442848	1904.176806	20.137651
57.730713	1884.268255	20.142669
58.112817	1889.969770	20.147687
58.174955	1893.618320	20.152704
58.189136	1889.397893	20.157722
57.934315	1887.235824	20.162739
57.789879	1885.102722	20.167757
57.781634	1903.380913	20.172775
57.981012	1906.554765	20.177792
58.296382	1910.354308	20.182810
58.175619	1920.351382	20.187827
58.464900	1914.085754	20.192845
58.861113	1911.807620	20.197863
58.593292	1916.742721	20.202880
59.006107	1914.506326	20.207898
58.859629	1918.017766	20.212915
58.951379	1918.420015	20.217933
58.937891	1914.982132	20.222951
58.989662	1915.202020	20.227968
59.124184	1909.483288	20.232986
59.171437	1911.606717	20.238003
59.486570	1906.199821	20.243021
59.409091	1898.454737	20.248039
58.552368	1885.906305	20.253056
58.950900	1899.568634	20.258074
58.630122	1902.616400	20.263091
59.116082	1902.615578	20.268109
58.822413	1907.485663	20.273127
59.156170	1909.101804	20.278144
59.389631	1923.308818	20.283162
59.441260	1927.253216	20.288179
59.500001	1949.284621	20.293197
59.324441	1943.915649	20.298215
59.437649	1945.455316	20.303232
59.652230	1940.588296	20.308250
59.511847	1938.371837	20.313267
59.501216	1932.198380	20.318285
59.570533	1938.366670	20.323303
59.715440	1963.796107	20.328320
59.895651	1962.208075	20.333338
59.658280	1968.525585	20.338355
59.894860	1961.263916	20.343373
60.022436	1964.794558	20.348391
60.040867	1966.573547	20.353408
60.651532	1963.413028	20.358426
60.495364	1958.800306	20.363443
60.374833	1954.730122	20.368461
60.896532	1955.605292	20.373479
60.614597	1959.752962	20.378496
60.901710	1955.821588	20.383514
60.825677	1966.137277	20.388531
60.858760	1964.535022	20.393549
60.564500	1954.188340	20.398567
60.362608	1962.401984	20.403584
60.632387	1971.658035	20.408602
60.793381	1984.675107	20.413619
60.663202	1987.090136	20.418637
61.366960	1984.970525	20.423655
61.325149	1991.435196	20.428672
61.206463	1984.409114	20.433690
61.055050	1996.191670	20.438707
61.381524	1995.932995	20.443725
61.114435	1988.429108	20.448743
61.113596	1984.802102	20.453760
61.333001	2001.492679	20.458778
61.477417	2012.997914	20.463795
61.485242	2010.117126	20.468813
61.574165	2006.353596	20.473831
61.735516	2018.195410	20.478848
62.059780	2007.572263	20.483866
61.954941	2010.979976	20.488883
61.671308	2013.871216	20.493901
61.740178	2003.814387	20.498919
62.112041	2017.232805	20.503936
62.507668	2007.561647	20.508954
62.387498	2012.032556	20.513971
62.067949	2013.527344	20.518989
62.155626	2015.479917	20.524007
62.078254	2028.300659	20.529024
62.514681	2041.013507	20.534042
62.621639	2038.152127	20.539059
62.695084	2027.860660	20.544077
63.103790	2015.438833	20.549095
63.230275	2021.423671	20.554112
63.071152	2006.613911	20.559130
63.000497	1999.051116	20.564147
62.997293	1997.413132	20.569165
63.198239	1981.476429	20.574183
63.049826	1986.957543	20.579200
63.155629	1983.293982	20.584218
63.107188	1984.813173	20.589235
62.915114	2006.691301	20.594253
63.272706	2012.552829	20.599271
63.403537	2012.431274	20.604288
63.568615	2018.627838	20.609306
63.660844	2008.582886	20.614323
63.454830	2019.208328	20.619341
63.738596	2023.864336	20.624359
63.286517	2018.206466	20.629376
63.466975	2012.582849	20.634394
63.596437	2017.246292	20.639411
63.191343	2019.658417	20.644429
63.750353	2015.202863	20.649447
63.448704	2026.570542	20.654464
63.924212	2043.064425	20.659482
63.954623	2047.105677	20.664499
63.963215	2041.947131	20.669517
64.152808	2038.907892	20.674535
64.043382	2048.944511	20.679552
64.104774	2041.128724	20.684570
64.210080	2038.698732	20.689587
64.079710	2038.049936	20.694605
64.169935	2037.579976	20.699623
64.304000	2062.540491	20.704640
63.907089	2065.148518	20.709658
64.312075	2074.792887	20.714675
64.609561	2073.494097	20.719693
64.811597	2070.261053	20.724711
64.737015	2079.333233	20.729728
65.021352	2088.707027	20.734746
65.201153	2093.649175	20.739763
65.149265	2098.635198	20.744781
65.392183	2095.018203	20.749799
65.324848	2099.488263	20.754816
65.446879	2088.302857	20.759834
65.129032	2070.145589	20.764851
65.303549	2083.572723	20.769869
65.755459	2085.277592	20.774887
65.412756	2080.221294	20.779904
65.792787	2083.667644	20.784922
65.810882	2083.565542	20.789939
65.648525	2089.437595	20.794957
65.795521	2083.325777	20.799975
66.043996	2094.094924	20.804992
66.178719	2085.847668	20.810010
66.014482	2086.115923	20.815027
65.780296	2084.884295	20.820045
66.194363	2083.966609	20.825063
66.062792	2080.988804	20.830080
66.320927	2077.599615	20.835098
66.187294	2073.919770	20.840115
66.193968	2073.739635	20.845133
66.227119	2071.716479	20.850151
66.253629	2081.508952	20.855168
66.473077	2097.028723	20.860186
66.699943	2101.628425	20.865203
66.600007	2116.103028	20.870221
66.606181	2104.400161	20.875239
66.675387	2113.132402	20.880256
66.623515	2107.409024	20.885274
66.664790	2106.951498	20.890291
66.541093	2116.601535	20.895309
67.075340	2125.762708	20.900327
66.831029	2133.968110	20.905344
66.841517	2135.505512	20.910362
67.271837	2135.640679	20.915379
67.015495	2134.645400	20.920397
67.185890	2121.627885	20.925415
67.215757	2136.382601	20.930432
67.396928	2159.186580	20.935450
68.040142	2154.273329	20.940467
67.867960	2162.271915	20.945485
67.984376	2165.974930	20.950503
68.183754	2154.177436	20.955520
68.007007	2155.377717	20.960538
68.018954	2153.108446	20.965555
67.893768	2158.475534	20.970573
68.160859	2153.162337	20.975591
68.095635	2161.290857	20.980608
67.923651	2162.769493	20.985626
68.348646	2165.236335	20.990643
68.291097	2160.458006	20.995661
68.406930	2155.637192	21.000679
68.433628	2163.550879	21.005696
68.356005	2157.294720	21.010714
68.457010	2158.673431	21.015731
68.496841	2162.954894	21.020749
68.317285	2157.407762	21.025767
68.448699	2170.123578	21.030784
68.615123	2178.912990	21.035802
68.896613	2181.927236	21.040819
68.959659	2192.019647	21.045837
68.879723	2183.206677	21.050855
69.019583	2188.389336	21.055872
68.925667	2193.262658	21.060890
69.138848	2188.141846	21.065907
69.317032	2201.918882	21.070925
69.333402	2211.607600	21.075943
69.429247	2210.918980	21.080960
69.392669	2210.567258	21.085978
69.830874	2209.292011	21.090995
69.649854	2215.208148	21.096013
69.691478	2211.353184	21.101031
70.006441	2210.378669	21.106048
69.763686	2211.596576	21.111066
69.966523	2201.737132	21.116083
69.662812	2212.861970	21.121101
69.876171	2200.775501	21.126119
70.101257	2214.297529	21.131136
70.049515	2222.091157	21.136154
70.485289	2219.557995	21.141171
70.076613	2219.078897	21.146189
69.882576	2219.998963	21.151207
70.145844	2216.178169	21.156224
70.135492	2233.979913	21.161242
70.559060	2235.748156	21.166259
70.832625	2243.119416	21.171277
71.128474	2244.476505	21.176295
71.249214	2248.171737	21.181312
70.879885	2251.703612	21.186330
71.321862	2241.210036	21.191347
71.006472	2241.161572	21.196365
71.497209	2248.649640	21.201383
71.699719	2233.866405	21.206400
71.539936	2241.573202	21.211418
71.572054	2239.840364	21.216435
71.379895	2246.365075	21.221453
71.545586	2232.826177	21.226471
71.967803	2234.572596	21.231488
71.794604	2235.175420	21.236506
71.662314	2233.120577	21.241523
71.732816	2239.732904	21.246541
71.808054	2237.894104	21.251559
71.959544	2233.593762	21.256576
71.550278	2237.192091	21.261594
71.718259	2234.378055	21.266611
71.562786	2254.690959	21.271629
71.827742	2259.479292	21.276647
71.593009	2267.995002	21.281664
72.113274	2269.818502	21.286682
72.326712	2277.391473	21.291699
72.231457	2295.454206	21.296717
72.522377	2292.003242	21.301735
72.650069	2297.605293	21.306752
72.325510	2302.674324	21.311770
72.566273	2293.247539	21.316787
72.743461	2298.492561	21.321805
72.672625	2299.810756	21.326823
72.990677	2297.513224	21.331840
72.803771	2318.404276	21.336858
73.006017	2317.579525	21.341875
73.015450	2327.254109	21.346893
73.145977	2329.039383	21.351911
73.412746	2322.632432	21.356928
73.210400	2320.508464	21.361946
73.327505	2323.493259	21.366963
73.479151	2320.712229	21.371981
73.440041	2313.988584	21.376999
73.614726	2322.231016	21.382016
73.642333	2343.919695	21.387034
74.345301	2345.310967	21.392051
74.222006	2354.184669	21.397069
74.005992	2344.060609	21.402087
74.072269	2345.115150	21.407104
74.368869	2351.084943	21.412122
74.936242	2338.002702	21.417139
74.535224	2320.959750	21.422157
74.363517	2310.845306	21.427175
74.510716	2304.118379	21.432192
74.199953	2322.407385	21.437210
74.762943	2327.925957	21.442227
74.672379	2339.516406	21.447245
74.733950	2341.322943	21.452263
75.201364	2330.580202	21.457280
74.754459	2337.927480	21.462298
74.856662	2339.093007	21.467315
74.757598	2339.641039	21.472333
74.793900	2336.035363	21.477351
75.151793	2327.762447	21.482368
74.997330	2338.247675	21.487386
75.339480	2347.451416	21.492403
75.436534	2365.189069	21.497421
75.449559	2369.580150	21.502439
75.805424	2359.918115	21.507456
75.565707	2367.364180	21.512474
75.556858	2364.867995	21.517491
75.349951	2363.749550	21.522509
75.175647	2367.933839	21.527527
75.877613	2378.508804	21.532544
75.639404	2387.976383	21.537562
75.946455	2384.334530	21.542579
76.129821	2392.505873	21.547597
76.178522	2385.105421	21.552615
76.609692	2385.903478	21.557632
76.506031	2390.224510	21.562650
76.682186	2382.368683	21.567667
76.757193	2384.710429	21.572685
76.726013	2390.851048	21.577703
76.605658	2387.133495	21.582720
76.328416	2391.308454	21.587738
76.512017	2386.525564	21.592755
76.772046	2410.751968	21.597773
77.043938	2406.639528	21.602791
77.203260	2409.935478	21.607808
76.796161	2412.942905	21.612826
77.196580	2410.256898	21.617843
77.267132	2405.474214	21.622861
77.084921	2402.020061	21.627879
77.394464	2409.279532	21.632896
77.384885	2426.550239	21.637914
77.667221	2435.959222	21.642931
77.786882	2427.739478	21.647949
77.651304	2427.469893	21.652967
77.871868	2431.434484	21.657984
77.995189	2440.635927	21.663002
77.713575	2430.060049	21.668019
78.034383	2422.487355	21.673037
78.084499	2427.934966	21.678055
78.270793	2425.293070	21.683072
78.246275	2432.024366	21.688090
78.350609	2426.933705	21.693107
78.438204	2425.992491	21.698125
78.139996	2424.771041	21.703143
78.326780	2434.463968	21.708160
78.462567	2450.933427	21.713178
78.478400	2447.721292	21.718195
78.567436	2456.719355	21.723213
78.704174	2460.264737	21.728231
78.979738	2444.054170	21.733248
78.949677	2449.455611	21.738266
78.803218	2459.450986	21.743283
79.137601	2471.980286	21.748301
79.066035	2476.632267	21.753319
79.470125	2477.644273	21.758336
79.230757	2477.057601	21.763354
79.452569	2480.568428	21.768371
79.421891	2476.857661	21.773389
79.396623	2482.810319	21.778407
79.750693	2488.957669	21.783424
79.754458	2497.172978	21.788442
79.627027	2509.117708	21.793459
79.591991	2507.383753	21.798477
79.781929	2510.069502	21.803495
79.907010	2508.153516	21.808512
79.958249	2509.190085	21.813530
80.612233	2522.957925	21.818547
80.846942	2518.414185	21.823565
80.457504	2530.374356	21.828583
80.850590	2524.618495	21.833600
80.810823	2517.453507	21.838618
81.006164	2518.173287	21.843635
81.073710	2519.383151	21.848653
80.922540	2527.900916	21.853671
81.432221	2511.515288	21.858688
80.909996	2501.383159	21.863706
80.722461	2521.299727	21.868723
81.368141	2514.959497	21.873741
81.001537	2516.882618	21.878759
81.274005	2507.281153	21.883776
81.600323	2514.176458	21.888794
81.335530	2513.990868	21.893811
81.731101	2513.563652	21.898829
81.692530	2514.472956	21.903847
81.733281	2506.042994	21.908864
81.900239	2519.784767	21.913882
81.878190	2536.171388	21.918899
82.231003	2536.576497	21.923917
81.960452	2540.647232	21.928935
81.910724	2541.875727	21.933952
81.991326	2538.295742	21.938970
82.246422	2540.026951	21.943987
82.443599	2538.606142	21.949005
82.376323	2532.609157	21.954023
82.635887	2528.050275	21.959040
82.658618	2545.327182	21.964058
82.627676	2563.865041	21.969075
83.183395	2564.175923	21.974093
82.812867	2565.178382	21.979111
83.096171	2560.057258	21.984128
83.598213	2555.414518	21.989146
83.232095	2565.046304	21.994163
83.120875	2563.748999	21.999181
83.302618	2563.066615	22.004199
83.488713	2552.602204	22.009216
83.499194	2560.210098	22.014234
83.635828	2564.876851	22.019251
83.365134	2550.660275	22.024269
83.452904	2557.753373	22.029287
83.823552	2555.700655	22.034304
83.681441	2553.679287	22.039322
83.762420	2552.879327	22.044339
83.864006	2563.280577	22.049357
84.122125	2577.341975	22.054375
84.120262	2581.962367	22.059392
84.078166	2578.006206	22.064410
84.034871	2579.532870	22.069427
83.991992	2570.064685	22.074445
84.330583	2574.001110	22.079463
84.333952	2595.416575	22.084480
84.394525	2599.697087	22.089498
84.662412	2604.860263	22.094515
84.608193	2603.640530	22.099533
84.759370	2601.903689	22.104551
84.377855	2600.251501	22.109568
84.964434	2614.100666	22.114586
85.008515	2625.027260	22.119603
85.410620	2621.412531	22.124621
85.196448	2630.485306	22.129639
85.182162	2624.583063	22.134656
85.319243	2628.414272	22.139674
85.379620	2646.709536	22.144691
86.219371	2646.194996	22.149709
85.922741	2647.823850	22.154727
86.625983	2643.933259	22.159744
86.591287	2642.159860	22.164762
86.465266	2628.037773	22.169779
86.402270	2617.787012	22.174797
86.364861	2618.848108	22.179815
86.265007	2609.737780	22.184832
86.355046	2609.565098	22.189850
86.369121	2627.201033	22.194867
86.701402	2630.498711	22.199885
86.796454	2650.802938	22.204903
86.546163	2641.549771	22.209920
86.561829	2641.941407	22.214938
86.441057	2644.586884	22.219955
86.982686	2641.224660	22.224973
86.647508	2653.250749	22.229991
86.851532	2660.919962	22.235008
87.360792	2668.804014	22.240026
87.299227	2671.217631	22.245043
87.478360	2664.447464	22.250061
87.256952	2664.542897	22.255079
87.664654	2676.858636	22.260096
87.899897	2669.128718	22.265114
87.582910	2670.813705	22.270131
87.523069	2684.809331	22.275149
87.726970	2692.827816	22.280167
88.204206	2692.137058	22.285184
88.266535	2693.122194	22.290202
88.171041	2690.001674	22.295219
88.253158	2692.585219	22.300237
88.388741	2686.089596	22.305255
88.580927	2690.327474	22.310272
88.518860	2686.004094	22.315290
88.190719	2701.718288	22.320307
88.758120	2709.874645	22.325325
88.977809	2716.463262	22.330343
88.714689	2718.190520	22.335360
88.614454	2715.555461	22.340378
88.719522	2724.673474	22.345395
88.594865	2712.468152	22.350413
88.923864	2729.517378	22.355431
89.006770	2747.333405	22.360448
89.293473	2748.721585	22.365466
89.360434	2750.343799	22.370483
89.448521	2747.868907	22.375501
89.774541	2745.030583	22.380519
89.594045	2745.338156	22.385536
89.703116	2751.102127	22.390554
89.615520	2764.405518	22.395571
89.889185	2767.845617	22.400589
90.384137	2776.208113	22.405607
90.189181	2757.750539	22.410624
90.146960	2766.740196	22.415642
90.086202	2772.873263	22.420659
90.297510	2760.741816	22.425677
90.889867	2783.412881	22.430695
90.782836	2790.116651	22.435712
90.907608	2794.581484	22.440730
90.673180	2799.245563	22.445747
91.334100	2788.852392	22.450765
91.044151	2793.902069	22.455783
91.304235	2793.040157	22.460800
91.402860	2784.808747	22.465818
91.063331	2793.205468	22.470835
91.596623	2788.301956	22.475853
91.482325	2793.095368	22.480871
91.443207	2788.610667	22.485888
91.528475	2786.101982	22.490906
91.544941	2791.502532	22.495923
91.666358	2802.327857	22.500941
91.676789	2812.247477	22.505959
91.980048	2811.843413	22.510976
92.064335	2816.403545	22.515994
92.042733	2812.812464	22.521011
92.241649	2812.921777	22.526029
92.166874	2830.881337	22.531047
92.313038	2832.602267	22.536064
92.657557	2836.516122	22.541082
92.305468	2845.277971	22.546099
92.612228	2841.484868	22.551117
92.746664	2841.518630	22.556135
92.716581	2846.151647	22.561152
93.000838	2848.544259	22.566170
92.992962	2871.685725	22.571187
93.044097	2867.782958	22.576205
92.994169	2863.087410	22.581223
93.353852	2869.547000	22.586240
93.144909	2859.037544	22.591258
93.275230	2882.532948	22.596275
93.462828	2885.436491	22.601293
93.756340	2893.107933	22.606311
93.339401	2902.190418	22.611328
93.709166	2897.681694	22.616346
93.831029	2914.852039	22.621363
94.177520	2913.708471	22.626381
94.581772	2912.296262	22.631399
94.477455	2914.565013	22.636416
94.667015	2907.160679	22.641434
94.631969	2911.338200	22.646451
94.828061	2912.061419	22.651469
94.558328	2909.121684	22.656487
94.633984	2907.940666	22.661504
94.816628	2909.898104	22.666522
94.524566	2920.213967	22.671539
94.752984	2935.759472	22.676557
94.995920	2940.631197	22.681575
95.096086	2941.711668	22.686592
95.553066	2933.302728	22.691610
95.637996	2934.021516	22.696627
95.522078	2935.842546	22.701645
95.775514	2940.917275	22.706663
95.732265	2938.542057	22.711680
96.169009	2928.896994	22.716698
95.799095	2936.902726	22.721715
95.899700	2927.429468	22.726733
96.251651	2938.275780	22.731751
96.104698	2953.462941	22.736768
96.899018	2954.555268	22.741786
96.369001	2954.878976	22.746803
96.461154	2946.248911	22.751821
96.769320	2951.183469	22.756839
96.769945	2947.570171	22.761856
96.815845	2950.961794	22.766874
96.602372	2940.451457	22.771891
96.951516	2950.607632	22.776909
96.939116	2941.208198	22.781927
96.717025	2946.306929	22.786944
97.030806	2957.250133	22.791962
97.201696	2973.353279	22.796979
97.234898	2975.727234	22.801997
97.154549	2971.824161	22.807015
96.965470	2976.829634	22.812032
97.127023	2992.564628	22.817050
97.364731	3002.492020	22.822067
97.145015	3005.268123	22.827085
98.024079	3020.564244	22.832103
98.008551	3031.853781	22.837120
98.466613	3025.645996	22.842138
98.452493	3024.434159	22.847155
98.578129	3015.797331	22.852173
98.730137	3012.182579	22.857191
98.588885	3017.772326	22.862208
99.143843	3012.775387	22.867226
99.056729	3016.250075	22.872243
99.179556	3015.378197	22.877261
99.204907	3013.537329	22.882279
98.981792	3015.399740	22.887296
99.221530	3015.874377	22.892314
99.296434	3033.700718	22.897331
98.979528	3044.003845	22.902349
99.287683	3039.551742	22.907367
99.274979	3046.563657	22.912384
99.721022	3038.473037	22.917402
99.740429	3054.732068	22.922419
99.766979	3064.793288	22.927437
99.990725	3059.194416	22.932455
99.899364	3067.827387	22.937472
100.335631	3068.013166	22.942490
100.257256	3067.497068	22.947507
100.250141	3066.678199	22.952525
100.547415	3059.254779	22.957543
100.489776	3089.528309	22.962560
100.863468	3084.834612	22.967578
100.826856	3092.181246	22.972595
100.700895	3097.727935	22.977613
100.830695	3095.863858	22.982631
100.844477	3098.313495	22.987648
101.004963	3087.279684	22.992666
101.409082	3106.350939	22.997683
101.216572	3116.866218	23.002701
101.487100	3118.547296	23.007719
101.547034	3127.156433	23.012736
101.939242	3117.380426	23.017754
101.997899	3118.035061	23.022771
101.913622	3121.036028	23.027789
102.377152	3112.301468	23.032807
102.142404	3115.991190	23.037824
102.174392	3109.359378	23.042842
102.044832	3113.022629	23.047859
101.970583	3107.688451	23.052877
102.451011	3128.541368	23.057895
102.469062	3137.444480	23.062912
102.597357	3144.879201	23.067930
102.659322	3142.595599	23.072947
102.509544	3149.773969	23.077965
102.812542	3143.733951	23.082983
102.521826	3151.990091	23.088000
102.990335	3151.505900	23.093018
102.935773	3161.164035	23.098035
102.890130	3165.922569	23.103053
103.178564	3173.656415	23.108071
103.290380	3196.490328	23.113088
103.612297	3190.977529	23.118106
103.705529	3188.215861	23.123123
103.644893	3205.163172	23.128141
103.989504	3200.198244	23.133159
103.792437	3222.558871	23.138176
104.237572	3217.139060	23.143194
104.342485	3228.261539	23.148211
104.566904	3221.014689	23.153229
104.708357	3212.983465	23.158247
104.635744	3220.960593	23.163264
104.736648	3209.446352	23.168282
105.034346	3212.399846	23.173299
104.971525	3218.779912	23.178317
105.311561	3228.088476	23.183335
105.077433	3242.317808	23.188352
105.383811	3237.064286	23.193370
105.525697	3236.193965	23.198387
105.588711	3237.586545	23.203405
105.720453	3238.367289	23.208423
105.713927	3237.612494	23.213440
105.597721	3232.680538	23.218458
105.878929	3229.516836	23.223475
106.074236	3233.362968	23.228493
106.163677	3238.260988	23.233511
106.399232	3251.310483	23.238528
106.503628	3252.851347	23.243546
106.716324	3259.702405	23.248563
106.599532	3264.590479	23.253581
107.122733	3246.656801	23.258599
106.861216	3250.697873	23.263616
106.725083	3247.085492	23.268634
107.163873	3242.359316	23.273651
107.122804	3240.505399	23.278669
106.935175	3247.123879	23.283687
106.752789	3248.830739	23.288704
107.295943	3264.311471	23.293722
107.463869	3273.119367	23.298739
107.231851	3286.858181	23.303757
107.744288	3273.750398	23.308775
107.821635	3280.704197	23.313792
107.635331	3282.284530	23.318810
107.563679	3294.227712	23.323827
107.962451	3297.497595	23.328845
108.381072	3298.928954	23.333863
108.275212	3315.325543	23.338880
108.319120	3302.917422	23.343898
108.638345	3305.485832	23.348915
108.536013	3319.568991	23.353933
108.867624	3325.384137	23.358951
109.205526	3325.176318	23.363968
109.251960	3319.629547	23.368986
109.059094	3317.271954	23.374003
109.027117	3324.930169	23.379021
109.499470	3319.447543	23.384039
109.068128	3320.465233	23.389056
109.346759	3321.054715	23.394074
109.366461	3329.850959	23.399091
109.299058	3351.784353	23.404109
109.547533	3348.456737	23.409127
109.653416	3345.991011	23.414144
109.501198	3351.114923	23.419162
109.599298	3359.007553	23.424179
109.751002	3379.476204	23.429197
110.005860	3376.206980	23.434215
110.248243	3393.756370	23.439232
110.332557	3411.051996	23.444250
110.584841	3408.814020	23.449267
110.789106	3410.739987	23.454285
111.041627	3408.942181	23.459303
110.904231	3410.269125	23.464320
110.976514	3409.105953	23.469338
111.344508	3415.791589	23.474355
111.248189	3430.651108	23.479373
111.437736	3423.296145	23.484391
111.547267	3430.618349	23.489408
111.828466	3431.470433	23.494426
111.978454	3421.203963	23.499443
111.887513	3422.969333	23.504461
111.993954	3437.527542	23.509479
112.001035	3455.237231	23.514496
112.259308	3452.382831	23.519514
112.890204	3449.482489	23.524531
112.459607	3450.795373	23.529549
112.503320	3443.787812	23.534567
112.934484	3448.565143	23.539584
112.710639	3452.940620	23.544602
113.049369	3447.024114	23.549619
112.828873	3462.117633	23.554637
113.059339	3475.235489	23.559655
113.149182	3474.904938	23.564672
113.429148	3475.236695	23.569690
113.414782	3473.916189	23.574707
113.564452	3470.833673	23.579725
113.661245	3478.316294	23.584743
113.948398	3500.461702	23.589760
114.236158	3499.513667	23.594778
114.312098	3497.596248	23.599795
114.139619	3504.061128	23.604813
114.353315	3504.148315	23.609831
114.483457	3502.258540	23.614848
114.520549	3496.352186	23.619866
114.966702	3496.770222	23.624883
114.845465	3509.820730	23.629901
114.790325	3498.336837	23.634919
114.766461	3513.481719	23.639936
114.976854	3518.413746	23.644954
115.248436	3515.183069	23.649971
115.271115	3523.297349	23.654989
115.529839	3522.478939	23.660007
115.507705	3526.228843	23.665024
115.652158	3532.010871	23.670042
116.039823	3545.119299	23.675059
115.514558	3561.921057	23.680077
115.821839	3553.732266	23.685095
116.114261	3553.224063	23.690112
116.022314	3549.014065	23.695130
116.293409	3547.319874	23.700147
116.429600	3566.736876	23.705165
116.897857	3564.300110	23.710183
116.972599	3569.463693	23.715200
117.107416	3574.054663	23.720218
117.238760	3563.647862	23.725235
117.295097	3568.462085	23.730253
117.284467	3560.524768	23.735271
117.297762	3565.311073	23.740288
117.134192	3569.597066	23.745306
117.207765	3559.304175	23.750323
117.538386	3558.032073	23.755341
117.407542	3565.057085	23.760359
117.538538	3576.234556	23.765376
117.558774	3592.837360	23.770394
117.905389	3594.290907	23.775411
117.497728	3594.012401	23.780429
117.617016	3609.370714	23.785447
117.872235	3618.334847	23.790464
117.930451	3617.592153	23.795482
118.319351	3639.206673	23.800499
118.581175	3653.798815	23.805517
118.766952	3644.031459	23.810535
119.037299	3642.679947	23.815552
118.996266	3663.578963	23.820570
119.328575	3666.773304	23.825587
119.541581	3672.221945	23.830605
119.739165	3669.929988	23.835623
120.061573	3670.261418	23.840640
119.924614	3664.534623	23.845658
120.087928	3662.481836	23.850675
120.138570	3661.729763	23.855693
119.934718	3657.972964	23.860711
120.103040	3661.253517	23.865728
120.071255	3665.906352	23.870746
120.355574	3683.111285	23.875763
120.247016	3688.430862	23.880781
120.422474	3697.011736	23.885799
121.160373	3689.485147	23.890816
120.742476	3695.132354	23.895834
121.123522	3694.518911	23.900851
121.133480	3710.743175	23.905869
121.208061	3716.473052	23.910887
121.192042	3718.134699	23.915904
121.237346	3713.825939	23.920922
121.569364	3722.093861	23.925939
121.597228	3734.317005	23.930957
121.528675	3739.802047	23.935975
121.982155	3737.123180	23.940992
121.310645	3744.965836	23.946010
121.944414	3755.949553	23.951027
121.822439	3754.797254	23.956045
122.056092	3767.252926	23.961063
122.381658	3789.765665	23.966080
122.447612	3798.518289	23.971098
122.761764	3801.953887	23.976115
122.968688	3800.831003	23.981133
123.163699	3812.654830	23.986151
123.302873	3819.424987	23.991168
123.537955	3817.596159	23.996186
123.439633	3814.103782	24.001203
123.595969	3820.077678	24.006221
123.756020	3820.102084	24.011239
124.363315	3811.708745	24.016256
123.882577	3820.030950	24.021274
124.064972	3826.723866	24.026291
124.395452	3836.691952	24.031309
124.197030	3840.012783	24.036327
124.446468	3840.683116	24.041344
124.427037	3852.939777	24.046362
124.543082	3832.379541	24.051379
124.806036	3839.850183	24.056397
124.422906	3867.785454	24.061415
124.962780	3858.971693	24.066432
124.493282	3878.816177	24.071450
125.224044	3874.790406	24.076467
125.185429	3877.028335	24.081485
125.494836	3891.808914	24.086503
125.767503	3901.316465	24.091520
125.320972	3904.227926	24.096538
125.841515	3895.991839	24.101555
126.084057	3905.038957	24.106573
125.935268	3919.622544	24.111591
126.335623	3923.751483	24.116608
126.093618	3920.039920	24.121626
126.321155	3928.371319	24.126643
126.678129	3926.919997	24.131661
126.860727	3941.285725	24.136679
127.382492	3942.053124	24.141696
127.202181	3950.473320	24.146714
127.290865	3950.313056	24.151731
127.263721	3945.221619	24.156749
127.028506	3952.596416	24.161767
127.828399	3948.177628	24.166784
127.494766	3942.106857	24.171802
127.737170	3952.803092	24.176819
128.060423	3973.573303	24.181837
128.071826	3965.912884	24.186855
128.341709	3967.200798	24.191872
128.579753	3974.774463	24.196890
128.585013	3962.062328	24.201907
128.607293	3971.901970	24.206925
128.393395	3979.042508	24.211943
128.935345	3982.416414	24.216960
128.744093	4000.072139	24.221978
129.114484	4002.390034	24.226995
128.994968	4004.522853	24.232013
128.942622	4010.653043	24.237031
129.242526	4015.753115	24.242048
129.605333	4023.340011	24.247066
129.614935	4022.555733	24.252083
130.028991	4028.274017	24.257101
129.864931	4042.379069	24.262119
130.459206	4047.364265	24.267136
130.397616	4044.686749	24.272154
130.830939	4037.327369	24.277171
130.768335	4035.388720	24.282189
130.554695	4046.600745	24.287207
131.046431	4037.205393	24.292224
130.973310	4047.054577	24.297242
130.978326	4041.412817	24.302259
130.992909	4055.574934	24.307277
130.851825	4078.261029	24.312295
131.240039	4074.957772	24.317312
131.303148	4075.901128	24.322330
131.335816	4091.219521	24.327347
131.667809	4103.863545	24.332365
131.457981	4112.169797	24.337383
131.945128	4114.039963	24.342400
132.237352	4123.605840	24.347418
131.685112	4122.174295	24.352435
131.877190	4130.480171	24.357453
132.074833	4151.891987	24.362471
132.185541	4149.956133	24.367488
132.560938	4157.940289	24.372506
132.987934	4180.916011	24.377523
133.244604	4182.773153	24.382541
133.221947	4185.398707	24.387559
133.190597	4169.765210	24.392576
133.442113	4178.794463	24.397594
133.383984	4179.325542	24.402611
134.166457	4183.797656	24.407629
134.231254	4204.681053	24.412647
134.308388	4199.212367	24.417664
134.372664	4215.778613	24.422682
134.352013	4206.589269	24.427699
134.414741	4202.847664	24.432717
134.771793	4198.272163	24.437735
134.894664	4195.937374	24.442752
134.780419	4199.012022	24.447770
134.869106	4207.309068	24.452787
135.066554	4206.845708	24.457805
134.999528	4230.270281	24.462823
135.074065	4222.676463	24.467840
134.891479	4231.499615	24.472858
135.223583	4247.975090	24.477875
135.611160	4250.278365	24.482893
135.423908	4262.980129	24.487911
135.581403	4265.938925	24.492928
135.870190	4276.893102	24.497946
135.863119	4287.012652	24.502963
136.401449	4296.387471	24.507981
136.399686	4311.387314	24.512999
136.548354	4311.606947	24.518016
136.779435	4323.844160	24.523034
137.031092	4313.682739	24.528051
137.146440	4317.005276	24.533069
137.068755	4333.284858	24.538087
137.643129	4337.511106	24.543104
137.546724	4341.312090	24.548122
137.156151	4338.364522	24.553139
137.438328	4350.882323	24.558157
137.855427	4372.280160	24.563175
138.185906	4356.766134	24.568192
138.670989	4360.357450	24.573210
138.613913	4358.174496	24.578227
138.852291	4345.480948	24.583245
138.539936	4363.136654	24.588263
139.039070	4382.932455	24.593280
139.242426	4389.957635	24.598298
139.313191	4381.380725	24.603315
139.407187	4388.020000	24.608333
139.256599	4385.687927	24.613351
139.320278	4375.561524	24.618368
139.795800	4386.144646	24.623386
139.624491	4404.996951	24.628403
140.043271	4409.816796	24.633421
140.046101	4406.370149	24.638439
140.005602	4406.672292	24.643456
140.241531	4412.688760	24.648474
140.305424	4438.136430	24.653491
140.410051	4436.644935	24.658509
140.121731	4439.259383	24.663527
140.548780	4455.483883	24.668544
140.690094	4471.000448	24.673562
140.950822	4467.046440	24.678579
141.064742	4470.940218	24.683597
141.025989	4491.569436	24.688615
141.305511	4504.770603	24.693632
141.618301	4511.439863	24.698650
141.696161	4519.554580	24.703667
141.952240	4528.710076	24.708685
142.063079	4542.219568	24.713703
142.318360	4534.714598	24.718720
142.112389	4536.199472	24.723738
142.527967	4542.051578	24.728755
142.953672	4545.644892	24.733773
142.820534	4550.851483	24.738791
142.922316	4556.865801	24.743808
143.083787	4548.863659	24.748826
143.057688	4541.864409	24.753843
143.022896	4549.472496	24.758861
143.220269	4579.610997	24.763879
143.346092	4576.002979	24.768896
143.704554	4576.819502	24.773914
143.628976	4593.414024	24.778931
144.164312	4596.831690	24.783949
144.252993	4606.582770	24.788967
144.110100	4604.710108	24.793984
144.414343	4604.555106	24.799002
145.115497	4611.377478	24.804019
145.364293	4611.790817	24.809037
145.644450	4617.817369	24.814055
145.619538	4621.942870	24.819072
145.752861	4608.408857	24.824090
145.762742	4613.744577	24.829107
145.928524	4595.705123	24.834125
146.171492	4597.292880	24.839143
146.241310	4602.917156	24.844160
146.076667	4601.448960	24.849178
145.985932	4607.023425	24.854195
146.194276	4598.366917	24.859213
146.102635	4604.835403	24.864231
146.286417	4628.768759	24.869248
146.494701	4635.521528	24.874266
146.230737	4638.391082	24.879283
146.676096	4656.893518	24.884301
146.889805	4658.139600	24.889319
146.976059	4668.060444	24.894336
147.296742	4685.762133	24.899354
147.273552	4692.861182	24.904371
147.207227	4699.742134	24.909389
147.729785	4714.241304	24.914407
147.980278	4719.907379	24.919424
148.117930	4725.826042	24.924442
147.913326	4730.015972	24.929459
148.577874	4741.586356	24.934477
148.598924	4752.337110	24.939495
148.764002	4753.238424	24.944512
149.212618	4747.190622	24.949530
149.245609	4747.028546	24.954547
149.129854	4746.472900	24.959565
149.357385	4770.977298	24.964583
149.652609	4778.917554	24.969600
149.985860	4769.607863	24.974618
149.478729	4779.037916	24.979635
149.979120	4775.919137	24.984653
150.011162	4789.640353	24.989671
149.827167	4802.488498	24.994688
150.523458	4800.918709	24.999706
150.153290	4804.023241	25.004723
150.610453	4824.920475	25.009741
150.541342	4833.147892	25.014759
150.550084	4835.105227	25.019776
151.075232	4849.206373	25.024794
151.493600	4862.512442	25.029811
151.584119	4865.016989	25.034829
151.516451	4867.706812	25.039847
151.577777	4872.321356	25.044864
151.889897	4880.673914	25.049882
151.644755	4896.177695	25.054899
152.200564	4884.571561	25.059917
151.953084	4900.745952	25.064935
152.069825	4903.887244	25.069952
152.776585	4905.136779	25.074970
152.833231	4909.025184	25.079987
153.178175	4908.334196	25.085005
153.590978	4924.496173	25.090023
153.092832	4943.272492	25.095040
153.791343	4939.315987	25.100058
153.502444	4950.910483	25.105075
153.731873	4952.284723	25.110093
154.206237	4937.561443	25.115111
154.082613	4951.635412	25.120128
154.109656	4932.245020	25.125146
154.287831	4946.180026	25.130163
154.306990	4956.286213	25.135181
154.933538	4966.436766	25.140199
154.553453	4965.086896	25.145216
154.846881	4960.761920	25.150234
154.821710	4972.936529	25.155251
154.792344	4986.838985	25.160269
155.184361	4996.844880	25.165287
155.354351	5000.684616	25.170304
155.533196	5008.500130	25.175322
155.700506	5011.614957	25.180339
155.382596	5018.334503	25.185357
156.036902	5037.651802	25.190375
155.706609	5051.643513	25.195392
156.358640	5049.039854	25.200410
156.753103	5061.408898	25.205427
157.153847	5059.795079	25.210445
157.430869	5067.091108	25.215463
157.308916	5069.535565	25.220480
157.409310	5056.444512	25.225498
157.563094	5067.768914	25.230515
157.724360	5074.140594	25.235533
158.078205	5081.360118	25.240551
158.044853	5103.056408	25.245568
157.889823	5096.898125	25.250586
158.080070	5087.601682	25.255603
158.113994	5102.942118	25.260621
158.372522	5113.530942	25.265639
158.359884	5122.671415	25.270656
158.721482	5121.655542	25.275674
158.886019	5142.060576	25.280691
159.380838	5146.947609	25.285709
159.535079	5149.125833	25.290727
159.335163	5152.894530	25.295744
159.997203	5159.399927	25.300762
159.970588	5176.313803	25.305779
160.359778	5172.909351	25.310797
160.402119	5171.349341	25.315815
160.466374	5171.371104	25.320832
160.457728	5168.718497	25.325850
160.541518	5174.085489	25.330867
160.839430	5194.737076	25.335885
160.646587	5201.666757	25.340903
160.808307	5201.610953	25.345920
161.062929	5204.879908	25.350938
161.144236	5214.967308	25.355955
161.168719	5226.582584	25.360973
161.383575	5236.491948	25.365991
161.637458	5252.210384	25.371008
162.110180	5254.369765	25.376026
162.124761	5255.138506	25.381043
162.301523	5275.375508	25.386061
162.696169	5283.180636	25.391079
162.362264	5290.341631	25.396096
162.849533	5274.291181	25.401114
162.883892	5289.293852	25.406131
162.770268	5309.588422	25.411149
163.683387	5310.194239	25.416167
163.342648	5308.397562	25.421184
163.775531	5306.779187	25.426202
163.823827	5318.058225	25.431219
163.785624	5333.860539	25.436237
164.184238	5338.052366	25.441255
164.130996	5337.386326	25.446272
164.202638	5337.387964	25.451290
164.589976	5353.080470	25.456307
164.723308	5365.246468	25.461325
164.972973	5370.609695	25.466343
164.945240	5371.345280	25.471360
164.864463	5385.591325	25.476378
165.236848	5390.115147	25.481395
164.930054	5390.816596	25.486413
165.335161	5406.716501	25.491431
165.306867	5412.769221	25.496448
165.768016	5422.266185	25.501466
165.938793	5446.790483	25.506483
166.092157	5445.360922	25.511501
166.626559	5449.984743	25.516519
166.502462	5468.752529	25.521536
166.750551	5472.677901	25.526554
167.517794	5473.654418	25.531571
167.246622	5475.588075	25.536589
167.692596	5483.351727	25.541607
167.734734	5506.516757	25.546624
168.171972	5498.476359	25.551642
168.042596	5491.411874	25.556659
168.100287	5488.137844	25.561677
168.515207	5494.448013	25.566695
168.570147	5504.918011	25.571712
168.627739	5520.783412	25.576730
168.716198	5525.307021	25.581747
168.885606	5525.741406	25.586765
169.190919	5536.158950	25.591783
169.006674	5549.675627	25.596800
169.488909	5554.846047	25.601818
169.593825	5555.177694	25.606835
169.655616	5574.735513	25.611853
169.993804	5580.185757	25.616871
170.300931	5582.113478	25.621888
170.191929	5578.485038	25.626906
170.593842	5598.126773	25.631923
170.385432	5613.307770	25.636941
170.680916	5595.378809	25.641959
170.722314	5612.804074	25.646976
170.718296	5624.840215	25.651994
171.250481	5635.877129	25.657011
171.208600	5650.228813	25.662029
171.721690	5663.711271	25.667047
171.274744	5664.353234	25.672064
171.805840	5673.852161	25.677082
172.123890	5688.119091	25.682100
171.994454	5697.415488	25.687117
172.399823	5703.689518	25.692135
172.679817	5723.278345	25.697152
173.009806	5717.702691	25.702170
173.168587	5722.436820	25.707188
173.065248	5732.085704	25.712205
173.478194	5744.117494	25.717223
173.851058	5750.338641	25.722240
173.951331	5738.721449	25.727258
174.111949	5745.459746	25.732276
173.715034	5762.203206	25.737293
174.296230	5767.933845	25.742311
174.478308	5779.977890	25.747328
174.528195	5771.936895	25.752346
174.761801	5779.791771	25.757364
174.603089	5799.773088	25.762381
175.123142	5810.382885	25.767399
175.129658	5811.724008	25.772416
175.116541	5816.481896	25.777434
175.544041	5821.949733	25.782452
175.514770	5838.576491	25.787469
175.506150	5839.393208	25.792487
175.697373	5857.531146	25.797504
175.558047	5859.787997	25.802522
176.048037	5857.704086	25.807540
176.376009	5892.057698	25.812557
176.662804	5889.702613	25.817575
176.607413	5904.574228	25.822592
176.821014	5920.403966	25.827610
177.270023	5912.119613	25.832628
177.060407	5927.679955	25.837645
177.318025	5941.128544	25.842663
177.797162	5953.423628	25.847680
177.639064	5963.054939	25.852698
178.226505	5972.269840	25.857716
178.028534	5978.643073	25.862733
178.387786	5994.492092	25.867751
178.577841	6000.041830	25.872768
178.655902	6009.636436	25.877786
179.260487	6026.872048	25.882804
179.241644	6037.432587	25.887821
179.507478	6038.119605	25.892839
179.686791	6046.382927	25.897856
179.620176	6066.929027	25.902874
180.164739	6064.202805	25.907892
180.039831	6070.779788	25.912909
180.355408	6077.327961	25.917927
180.347934	6099.708146	25.922944
180.726771	6098.178192	25.927962
181.385684	6109.551256	25.932980
181.098518	6128.501981	25.937997
181.261902	6124.358109	25.943015
181.325247	6131.037062	25.948032
181.410560	6149.592196	25.953050
181.884764	6153.739439	25.958068
182.129657	6153.447754	25.963085
182.108572	6165.968374	25.968103
182.198350	6176.164467	25.973120
182.282276	6185.013898	25.978138
182.690830	6190.968606	25.983156
182.667944	6211.166608	25.988173
182.776496	6217.333242	25.993191
183.252219	6227.164602	25.998208
183.183240	6246.343205	26.003226
183.830077	6250.493401	26.008244
183.700476	6257.954177	26.013261
183.554133	6282.162079	26.018279
183.932578	6280.120998	26.023296
183.808545	6299.571062	26.028314
184.528104	6304.453551	26.033332
184.225698	6312.176887	26.038349
184.499221	6326.599843	26.043367
185.064683	6337.236348	26.048384
184.966526	6354.342907	26.053402
185.360659	6361.891101	26.058420
185.650713	6383.186684	26.063437
185.722018	6388.659338	26.068455
185.853918	6399.351905	26.073472
186.166240	6407.017631	26.078490
186.532110	6421.963346	26.083508
186.604554	6434.488386	26.088525
186.720658	6432.728582	26.093543
187.052107	6428.174802	26.098560
187.098401	6435.954682	26.103578
187.543537	6454.166268	26.108596
187.395909	6461.326092	26.113613
187.214178	6459.992872	26.118631
187.636284	6471.765355	26.123648
187.846835	6487.132241	26.128666
188.284066	6484.449711	26.133684
188.148882	6501.479856	26.138701
188.530180	6513.006290	26.143719
188.668695	6524.050712	26.148736
188.581203	6530.901307	26.153754
188.966916	6540.687114	26.158772
189.017295	6556.961963	26.163789
189.405895	6566.363723	26.168807
189.549583	6576.913469	26.173824
189.839439	6588.467699	26.178842
190.501734	6586.472534	26.183860
190.562018	6600.667176	26.188877
190.269188	6604.079035	26.193895
190.828124	6610.269722	26.198912
190.795507	6612.813048	26.203930
191.035239	6632.169432	26.208948
191.336953	6652.892400	26.213965
191.506522	6639.871292	26.218983
191.558622	6654.337502	26.224000
191.401470	6660.601066	26.229018
191.905065	6672.607533	26.234036
191.794157	6690.516036	26.239053
191.917545	6700.866010	26.244071
192.422212	6715.238454	26.249088
192.568491	6737.347548	26.254106
192.921958	6732.167787	26.259124
192.776724	6763.302910	26.264141
193.064818	6760.938033	26.269159
193.095213	6769.828946	26.274176
193.516791	6791.042656	26.279194
193.611639	6802.344190	26.284212
194.035790	6812.958726	26.289229
194.177327	6820.229951	26.294247
194.760830	6831.671947	26.299264
194.270227	6845.220748	26.304282
194.767685	6852.173927	26.309300
195.051861	6873.625526	26.314317
194.661200	6886.085805	26.319335
195.326524	6901.714144	26.324352
195.683905	6911.359154	26.329370
195.884263	6917.290316	26.334388
196.080717	6934.083285	26.339405
195.970675	6942.854975	26.344423
196.362993	6961.651675	26.349440
196.803599	6975.433969	26.354458
196.906413	6976.904181	26.359476
196.663418	6993.527357	26.364493
197.224060	7009.295221	26.369511
197.462923	7011.629834	26.374528
197.730137	7029.740783	26.379546
198.004650	7036.474956	26.384564
197.988748	7036.353245	26.389581
198.064674	7047.920381	26.394599
198.055720	7065.520201	26.399616
198.203218	7079.885938	26.404634
198.465653	7100.292258	26.409652
198.943652	7104.668341	26.414669
198.881014	7125.723202	26.419687
199.456151	7134.543836	26.424704
199.727324	7133.893331	26.429722
199.771963	7152.008181	26.434740
199.854030	7164.964640	26.439757
200.330764	7160.252698	26.444775
200.434241	7163.273760	26.449792
200.779819	7186.988863	26.454810
200.925162	7186.907411	26.459828
200.874383	7191.110329	26.464845
200.738229	7200.180288	26.469863
201.184151	7219.812029	26.474880
201.403754	7233.141980	26.479898
201.523774	7246.530963	26.484916
201.820156	7253.815351	26.489933
201.636716	7265.581542	26.494951
201.941569	7273.437971	26.499968
202.055210	7284.202685	26.504986
202.134750	7302.108706	26.510004
202.624205	7310.211073	26.515021
203.004445	7341.107528	26.520039
203.230100	7335.855785	26.525056
203.279041	7359.423327	26.530074
203.524414	7375.529678	26.535092
203.695040	7380.396251	26.540109
203.862749	7398.461865	26.545127
204.065815	7408.284747	26.550144
204.342191	7435.193953	26.555162
204.474930	7446.075345	26.560180
205.038421	7457.088665	26.565197
205.269076	7467.407203	26.570215
205.850055	7458.313301	26.575232
206.140052	7477.837264	26.580250
206.282212	7491.203883	26.585268
206.378467	7489.852126	26.590285
206.505560	7485.348419	26.595303
207.156397	7481.660713	26.600320
206.796451	7497.657863	26.605338
206.885535	7509.085309	26.610356
207.130048	7520.437410	26.615373
206.932441	7534.187203	26.620391
207.422018	7543.245149	26.625408
207.811177	7549.632092	26.630426
207.831167	7570.143741	26.635444
208.250877	7574.453986	26.640461
208.120124	7595.601877	26.645479
208.411375	7607.646569	26.650496
208.334905	7618.691107	26.655514
208.558218	7623.382041	26.660532
208.678190	7651.376175	26.665549
209.240410	7674.712705	26.670567
209.580379	7668.968519	26.675584
209.492665	7694.014856	26.680602
209.885751	7709.463778	26.685620
210.163212	7706.813798	26.690637
210.352060	7736.913250	26.695655
211.016295	7733.539929	26.700672
211.217088	7740.275578	26.705690
211.076243	7753.088242	26.710708
211.560236	7751.791223	26.715725
211.420084	7767.543515	26.720743
211.799231	7769.642338	26.725760
211.757457	7785.255480	26.730778
211.917770	7803.685913	26.735796
211.822027	7813.923220	26.740813
212.307494	7830.824475	26.745831
212.789102	7848.629107	26.750848
212.901726	7862.063943	26.755866
213.388031	7864.932755	26.760884
213.314644	7877.687090	26.765901
213.648998	7887.646080	26.770919
214.076491	7889.443886	26.775936
214.118934	7902.594193	26.780954
214.435280	7912.066220	26.785972
214.761706	7911.215125	26.790989
214.564119	7911.195165	26.796007
215.052430	7920.608009	26.801024
215.138089	7943.138427	26.806042
215.175835	7946.965327	26.811060
215.683145	7934.139326	26.816077
215.301538	7963.456118	26.821095
216.083869	7974.313840	26.826112
216.106579	7974.106170	26.831130
216.040114	7998.557891	26.836148
216.497303	8006.609242	26.841165
216.484849	8020.734480	26.846183
216.708798	8029.745300	26.851200
216.826716	8041.867853	26.856218
217.109998	8067.447308	26.861236
217.559366	8069.475468	26.866253
217.555806	8096.302156	26.871271
217.740752	8107.907156	26.876288
217.801566	8112.377001	26.881306
218.100877	8129.633932	26.886324
218.501332	8145.121444	26.891341
218.473769	8166.815446	26.896359
219.055837	8180.242163	26.901376
219.258762	8202.119412	26.906394
219.241696	8204.396526	26.911412
219.629133	8218.543182	26.916429
219.725936	8236.324509	26.921447
220.045062	8253.413658	26.926464
220.749091	8254.930199	26.931482
220.639905	8275.950169	26.936500
220.986860	8281.522789	26.941517
221.243593	8291.472036	26.946535
221.578962	8307.100456	26.951552
221.688503	8310.211322	26.956570
221.830243	8325.673303	26.961588
222.060382	8332.341326	26.966605
222.242690	8348.588290	26.971623
222.596467	8364.422469	26.976640
222.864043	8369.598635	26.981658
223.218438	8372.526401	26.986676
223.575197	8380.493737	26.991693
223.540868	8409.564801	26.996711
223.685283	8404.374997	27.001728
223.591302	8407.143031	27.006746
223.970241	8427.955574	27.011764
224.068887	8441.831197	27.016781
224.091861	8470.755031	27.021799
224.583605	8477.564144	27.026816
225.098391	8491.285849	27.031834
224.858991	8507.510615	27.036852
225.466063	8518.364638	27.041869
225.569333	8539.282827	27.046887
225.428116	8544.499935	27.051904
226.188440	8564.672105	27.056922
226.222852	8574.830060	27.061940
226.441496	8589.187745	27.066957
226.471096	8599.613560	27.071975
226.651237	8604.944496	27.076992
227.080835	8617.652396	27.082010
226.999048	8636.102596	27.087028
227.553857	8654.003147	27.092045
227.760505	8670.734817	27.097063
227.819635	8688.617413	27.102080
227.958800	8698.409919	27.107098
228.131027	8714.938577	27.112116
228.740537	8725.788400	27.117133
229.019840	8749.765733	27.122151
229.411474	8751.363185	27.127168
229.659027	8751.775277	27.132186
229.774976	8775.675705	27.137204
229.740868	8774.082309	27.142221
229.964167	8789.852643	27.147239
229.910195	8796.805795	27.152256
230.226355	8812.194471	27.157274
230.540080	8831.112740	27.162292
231.226016	8838.559462	27.167309
231.015766	8861.207903	27.172327
231.402220	8876.247843	27.177344
231.666814	8881.174160	27.182362
231.611807	8903.742608	27.187380
232.213666	8904.015705	27.192397
232.469906	8926.390866	27.197415
232.652829	8931.349624	27.202432
233.066200	8936.260785	27.207450
233.365104	8959.286716	27.212468
233.508247	8959.548303	27.217485
233.794302	8976.022939	27.222503
233.905594	8983.039408	27.227520
234.322580	8984.234864	27.232538
233.949978	8998.407976	27.237556
234.647194	9010.336902	27.242573
235.105725	9021.382078	27.247591
235.054598	9031.045582	27.252608
235.330517	9044.522919	27.257626
235.368421	9052.426782	27.262644
235.626512	9068.973104	27.267661
235.853756	9080.056606	27.272679
235.882354	9095.196165	27.277696
236.394156	9101.520108	27.282714
236.387141	9126.560055	27.287732
236.793333	9147.471436	27.292749
236.721942	9159.901896	27.297767
236.954724	9174.089181	27.302784
237.964803	9187.723200	27.307802
238.423416	9201.370524	27.312820
239.025539	9200.005002	27.317837
238.904876	9203.755225	27.322855
239.017407	9200.598977	27.327872
239.196371	9202.468014	27.332890
239.435282	9217.751702	27.337908
239.390162	9221.026209	27.342925
239.610052	9239.588662	27.347943
239.470682	9256.197817	27.352960
240.141895	9256.155359	27.357978
240.274762	9279.180086	27.362996
240.562162	9283.736434	27.368013
240.927886	9304.837486	27.373031
241.037704	9317.127782	27.378048
241.557139	9320.530227	27.383066
241.022384	9348.248905	27.388084
241.513801	9354.193460	27.393101
241.655677	9377.618609	27.398119
242.078409	9384.345002	27.403136
242.522888	9400.429106	27.408154
242.381053	9417.097920	27.413172
242.731236	9437.647114	27.418189
242.812548	9451.781727	27.423207
243.065538	9467.294933	27.428224
243.489881	9473.182885	27.433242
243.242280	9507.382752	27.438260
243.863489	9512.883623	27.443277
244.331716	9534.021580	27.448295
244.108201	9545.614094	27.453312
244.596475	9564.316842	27.458330
244.613313	9582.591092	27.463348
245.016748	9593.503194	27.468365
245.563089	9611.874964	27.473383
245.737694	9628.820130	27.478400
245.980691	9641.759050	27.483418
246.088052	9655.063913	27.488436
246.382044	9668.007805	27.493453
246.269176	9673.032300	27.498471
246.425680	9704.312270	27.503488
247.141626	9710.452196	27.508506
247.280773	9729.238136	27.513524
247.267269	9744.793360	27.518541
247.699041	9754.608980	27.523559
247.915554	9774.473281	27.528576
248.451302	9782.409329	27.533594
248.518131	9789.756513	27.538612
248.755389	9818.582706	27.543629
249.029234	9829.969411	27.548647
249.453495	9856.920453	27.553664
249.663297	9853.430489	27.558682
249.664150	9880.598977	27.563700
250.142282	9889.947712	27.568717
250.608438	9902.596227	27.573735
250.338359	9926.615838	27.578752
250.994138	9939.807313	27.583770
251.154475	9958.582924	27.588788
251.251547	9972.794955	27.593805
251.374496	9991.064711	27.598823
251.481135	10002.116030	27.603840
252.370585	10014.258116	27.608858
252.015730	10033.571300	27.613876
252.508785	10057.839003	27.618893
252.815621	10079.279343	27.623911
253.368507	10094.638735	27.628928
253.749051	10103.866668	27.633946
254.153329	10112.897660	27.638964
254.328374	10115.779809	27.643981
254.653892	10141.487940	27.648999
254.495082	10148.579566	27.654016
255.199598	10158.360531	27.659034
255.175778	10177.411106	27.664052
255.413517	10174.230793	27.669069
255.623830	10197.599327	27.674087
255.992785	10221.999692	27.679104
256.082721	10214.936986	27.684122
256.123683	10227.954726	27.689140
256.298961	10255.551916	27.694157
256.949778	10260.971729	27.699175
256.601038	10281.384011	27.704192
257.312472	10290.116094	27.709210
257.342367	10308.566270	27.714228
257.669508	10334.220868	27.719245
258.300422	10338.830956	27.724263
258.129294	10367.932932	27.729280
258.732849	10379.991839	27.734298
259.084363	10393.947835	27.739316
259.134130	10402.407400	27.744333
259.391258	10424.461489	27.749351
259.539094	10433.612318	27.754368
259.823299	10452.002443	27.759386
259.849406	10472.680662	27.764404
259.823662	10493.688930	27.769421
260.325981	10507.148931	27.774439
260.842839	10527.161408	27.779456
261.071140	10541.646874	27.784474
261.608614	10561.082430	27.789492
261.700611	10581.077060	27.794509
262.313475	10587.672434	27.799527
262.321579	10608.487741	27.804544
262.561303	10620.037437	27.809562
262.841889	10618.054568	27.814580
262.775598	10634.875220	27.819597
263.200683	10643.868403	27.824615
263.336982	10662.521181	27.829632
263.968787	10673.158288	27.834650
263.790701	10689.644544	27.839668
264.114678	10719.154458	27.844685
264.363406	10713.713442	27.849703
264.368201	10738.424617	27.854720
264.826417	10746.400766	27.859738
265.236466	10760.300120	27.864756
265.356693	10782.233181	27.869773
265.793740	10796.262032	27.874791
266.168744	10817.759041	27.879808
266.362424	10832.023596	27.884826
266.575973	10846.678805	27.889844
266.802269	10859.103845	27.894861
267.125728	10874.399538	27.899879
267.212523	10897.173423	27.904896
267.924085	10911.689533	27.909914
268.061537	10923.811031	27.914932
268.406363	10936.435538	27.919949
268.556312	10954.372589	27.924967
269.034462	10972.080428	27.929984
268.861276	10988.638661	27.935002
269.468760	11003.105899	27.940020
269.455796	11030.456668	27.945037
270.146471	11028.254601	27.950055
270.061830	11062.177091	27.955072
270.263090	11074.861711	27.960090
271.010576	11089.414581	27.965108
270.773049	11106.057643	27.970125
270.995881	11117.514372	27.975143
271.222309	11138.691312	27.980160
271.568511	11155.147987	27.985178
271.991979	11180.995989	27.990196
272.382815	11196.570775	27.995213
272.826511	11209.016827	28.000231
273.009459	11229.334417	28.005248
272.721529	11242.824990	28.010266
273.059928	11261.049492	28.015284
273.510122	11275.949559	28.020301
274.022403	11295.456354	28.025319
274.216507	11322.982919	28.030336
274.220142	11343.544637	28.035354
274.483127	11353.089780	28.040372
274.779208	11380.672050	28.045389
275.195064	11396.829076	28.050407
275.443973	11420.038565	28.055424
275.721034	11443.867437	28.060442
275.907808	11454.400663	28.065460
276.020722	11474.812094	28.070477
276.605581	11496.456487	28.075495
276.862652	11521.194858	28.080512
277.134192	11547.005561	28.085530
277.776458	11557.042724	28.090548
277.784064	11576.538846	28.095565
278.410400	11587.722691	28.100583
278.811858	11610.220158	28.105600
278.497481	11620.655226	28.110618
279.203679	11629.800983	28.115636
279.218696	11645.413195	28.120653
279.759128	11671.794152	28.125671
279.862292	11680.954658	28.130688
280.262501	11694.333281	28.135706
280.359266	11712.391857	28.140724
280.149798	11733.287169	28.145741
280.767808	11752.149845	28.150759
280.790961	11766.933527	28.155776
281.033425	11789.862544	28.160794
281.645658	11800.716375	28.165812
281.977849	11809.534914	28.170829
282.158399	11828.870345	28.175847
282.582718	11841.015961	28.180864
282.825279	11866.995855	28.185882
282.922474	11876.901248	28.190900
283.266164	11895.604640	28.195917
283.883668	11903.276081	28.200935
283.717290	11918.598688	28.205952
283.912294	11946.537454	28.210970
284.522214	11959.955650	28.215988
284.337561	11986.039539	28.221005
284.666473	12002.867109	28.226023
284.909448	12027.427365	28.231040
285.246136	12044.611406	28.236058
286.009682	12065.913396	28.241076
286.451703	12087.661016	28.246093
286.591698	12098.509693	28.251111
286.721181	12120.655774	28.256128
286.935316	12134.145928	28.261146
287.256403	12150.223267	28.266164
287.749373	12171.269193	28.271181
288.137124	12190.138977	28.276199
288.467276	12201.107530	28.281216
288.614788	12227.557580	28.286234
289.053507	12242.501411	28.291252
289.181578	12263.436086	28.296269
289.214802	12272.064832	28.301287
289.566300	12284.708200	28.306304
289.947058	12303.640731	28.311322
290.514657	12326.121149	28.316340
290.409128	12342.656955	28.321357
290.771428	12362.412061	28.326375
290.892834	12384.665421	28.331392
290.903516	12404.612726	28.336410
291.529374	12426.817319	28.341428
291.902801	12457.343384	28.346445
292.224391	12477.144765	28.351463
292.692604	12492.927042	28.356480
292.472062	12509.980032	28.361498
293.367352	12528.939551	28.366516
293.932793	12552.314167	28.371533
293.837352	12560.428560	28.376551
294.188705	12585.124583	28.381568
294.534953	12595.038045	28.386586
294.936388	12612.363257	28.391604
295.106967	12633.255127	28.396621
295.351674	12661.443767	28.401639
295.641324	12669.924696	28.406656
295.925830	12690.031895	28.411674
296.312806	12698.287135	28.416692
296.246524	12728.971588	28.421709
296.591801	12740.844149	28.426727
296.870230	12767.925834	28.431744
297.197528	12786.120797	28.436762
297.623434	12798.955543	28.441780
298.130651	12819.224605	28.446797
298.260575	12836.724221	28.451815
298.723871	12852.159385	28.456832
299.106539	12880.527287	28.461850
299.303250	12893.133713	28.466868
299.384615	12909.311367	28.471885
299.874046	12924.278952	28.476903
300.494104	12933.124528	28.481920
299.986881	12950.469695	28.486938
300.416461	12963.497803	28.491956
300.885911	12989.260707	28.496973
301.177643	12999.870546	28.501991
301.780245	13026.549149	28.507008
301.396739	13028.752851	28.512026
301.768747	13044.696575	28.517044
301.803332	13075.700659	28.522061
302.391188	13099.014043	28.527079
302.704997	13120.735416	28.532096
302.576609	13151.134665	28.537114
303.015036	13168.175405	28.542132
303.563755	13188.031464	28.547149
304.038780	13211.589046	28.552167
304.616390	13230.157551	28.557184
304.336827	13260.274714	28.562202
304.420354	13271.105152	28.567220
304.620801	13304.572230	28.572237
305.243677	13326.584706	28.577255
305.747236	13341.411653	28.582272
305.824449	13375.545419	28.587290
306.408214	13388.630298	28.592308
306.651283	13414.696108	28.597325
307.414155	13437.331710	28.602343
308.063391	13452.957306	28.607360
308.402323	13471.447393	28.612378
308.674428	13476.362063	28.617396
308.905446	13498.173288	28.622413
308.768795	13505.150810	28.627431
309.628146	13513.219540	28.632448
309.718308	13537.318815	28.637466
309.951911	13552.341931	28.642484
310.045358	13566.991109	28.647501
310.196523	13595.605027	28.652519
310.663544	13607.524264	28.657536
310.865635	13630.207248	28.662554
311.332880	13649.295664	28.667572
311.538290	13669.825347	28.672589
311.861523	13693.746013	28.677607
312.548596	13698.067261	28.682624
312.631917	13729.020390	28.687642
313.108388	13750.907952	28.692660
313.685545	13771.328955	28.697677
313.532685	13782.897028	28.702695
314.040507	13794.338423	28.707712
314.233622	13819.289454	28.712730
314.820477	13840.993386	28.717748
315.303810	13844.826736	28.722765
315.335303	13866.148240	28.727783
315.436642	13874.437173	28.732800
315.587170	13903.065919	28.737818
316.059237	13916.305250	28.742836
316.504337	13945.492083	28.747853
316.411741	13963.012399	28.752871
317.151370	13978.130245	28.757888
317.639741	13998.777415	28.762906
317.839550	14023.174463	28.767924
318.180527	14039.234619	28.772941
318.250911	14065.040058	28.777959
318.253129	14068.908962	28.782976
318.916233	14100.803865	28.787994
319.252580	14114.619009	28.793012
319.670830	14134.508850	28.798029
319.405648	14157.974395	28.803047
320.304559	14171.512081	28.808064
320.296188	14195.898137	28.813082
320.540153	14227.826410	28.818100
321.151785	14238.218625	28.823117
321.407143	14263.587140	28.828135
321.933480	14276.562462	28.833152
321.598455	14298.354965	28.838170
322.455580	14308.299971	28.843188
322.800287	14334.695582	28.848205
322.919570	14354.614684	28.853223
323.201144	14366.781091	28.858240
323.502354	14388.167383	28.863258
323.887483	14397.883231	28.868276
324.285374	14413.500918	28.873293
324.374471	14433.797064	28.878311
325.071594	14451.719908	28.883328
324.813855	14480.027944	28.888346
325.397322	14493.985334	28.893364
325.651876	14522.021101	28.898381
325.569009	14557.537675	28.903399
326.616403	14567.528578	28.908416
326.626727	14595.852338	28.913434
326.685617	14617.835393	28.918452
326.939709	14643.220466	28.923469
327.886667	14672.349176	28.928487
328.115743	14687.881586	28.933504
328.263834	14719.743152	28.938522
328.650159	14741.560277	28.943540
329.009782	14758.473875	28.948557
329.561395	14779.190370	28.953575
329.870473	14802.092109	28.958592
330.361351	14817.560823	28.963610
330.708481	14839.193856	28.968628
330.817860	14864.384144	28.973645
331.207162	14876.269891	28.978663
331.900549	14904.529990	28.983680
331.958738	14917.036393	28.988698
332.648434	14930.766952	28.993716
333.265700	14949.781624	28.998733
333.046916	14963.134571	29.003751
333.616758	14970.946184	29.008768
333.404725	14995.951875	29.013786
333.974070	15015.222006	29.018804
334.248888	15039.250372	29.023821
334.495183	15050.270978	29.028839
334.822335	15076.470521	29.033856
335.113155	15106.605419	29.038874
335.480882	15127.075389	29.043892
335.986709	15152.665464	29.048909
336.119001	15189.788552	29.053927
336.490061	15200.101412	29.058944
336.631474	15225.800774	29.063962
336.887201	15262.150198	29.068980
337.593308	15274.049999	29.073997
337.757539	15299.041161	29.079015
338.195025	15328.833808	29.084032
338.523038	15351.025487	29.089050
339.070919	15372.972753	29.094068
339.738755	15380.894438	29.099085
339.632779	15404.773580	29.104103
340.080611	15420.016716	29.109120
340.691731	15440.079548	29.114138
341.058517	15446.500144	29.119156
341.168470	15464.284855	29.124173
341.309889	15492.377255	29.129191
341.651923	15506.912944	29.134208
342.033326	15538.791072	29.139226
342.170183	15556.546211	29.144244
342.689361	15575.677144	29.149261
342.797023	15607.316999	29.154279
342.938846	15619.146521	29.159296
343.564872	15644.755298	29.164314
343.911419	15677.219499	29.169332
344.291710	15690.823797	29.174349
344.551378	15721.701057	29.179367
344.954933	15733.446362	29.184384
345.105202	15758.678537	29.189402
344.939417	15777.806431	29.194420
345.963550	15808.372916	29.199437
345.838162	15826.195391	29.204455
346.506061	15849.398579	29.209472
346.511687	15882.130818	29.214490
346.837142	15907.904814	29.219508
347.171370	15932.526764	29.224525
347.655183	15964.210654	29.229543
348.357529	15976.926494	29.234560
348.631094	15999.378677	29.239578
349.266326	16025.449932	29.244596
349.377716	16042.503662	29.249613
349.756323	16066.986065	29.254631
350.090618	16091.356045	29.259648
350.562850	16113.923669	29.264666
350.535304	16148.194020	29.269684
351.238961	16164.694324	29.274701
351.701232	16188.140085	29.279719
351.508629	16208.754577	29.284736
352.383637	16238.008317	29.289754
352.605435	16254.238534	29.294772
353.276136	16280.747248	29.299789
353.310127	16312.038108	29.304807
353.788832	16324.493321	29.309824
353.924438	16351.508414	29.314842
354.360331	16374.835858	29.319860
355.245935	16400.199515	29.324877
355.222271	16429.386379	29.329895
355.733125	16446.495787	29.334912
355.873662	16466.841093	29.339930
356.099700	16488.955030	29.344948
356.536027	16504.765380	29.349965
356.970775	16531.116514	29.354983
357.482761	16548.596263	29.360000
357.968835	16568.276068	29.365018
358.185420	16600.722612	29.370036
358.313972	16619.262101	29.375053
358.884946	16645.620822	29.380071
359.116729	16657.918542	29.385088
359.423535	16691.698052	29.390106
359.641069	16721.113481	29.395124
360.263644	16741.185464	29.400141
360.156312	16776.208022	29.405159
360.702165	16793.989804	29.410176
361.085437	16829.019552	29.415194
361.432417	16858.968658	29.420212
361.930109	16884.387803	29.425229
362.172915	16915.137674	29.430247
362.325842	16937.327361	29.435264
362.868970	16969.313897	29.440282
363.181944	17002.227626	29.445300
363.760610	17028.620363	29.450317
363.911268	17050.416499	29.455335
364.139410	17080.384097	29.460352
364.726333	17106.093044	29.465370
364.836839	17138.882920	29.470388
365.410857	17162.261127	29.475405
365.460366	17204.396250	29.480423
366.127675	17223.504582	29.485440
366.452378	17251.916430	29.490458
366.764892	17287.133829	29.495476
367.158004	17305.838379	29.500493
367.511754	17339.450654	29.505511
367.901340	17372.127020	29.510528
368.584466	17384.380534	29.515546
368.489812	17406.258721	29.520564
369.147447	17427.101301	29.525581
369.386525	17458.724520	29.530599
369.893519	17479.193279	29.535616
370.461145	17507.333636	29.540634
370.494849	17528.363151	29.545652
371.015894	17547.358921	29.550669
371.273134	17574.954895	29.555687
371.913913	17603.141635	29.560704
372.309655	17617.879954	29.565722
372.294838	17647.081681	29.570740
372.925864	17654.104150	29.575757
373.227105	17687.251330	29.580775
373.286590	17719.547930	29.585792
373.765473	17745.881082	29.590810
373.608824	17781.162986	29.595828
374.398933	17808.860328	29.600845
374.595196	17851.844546	29.605863
375.041307	17874.954872	29.610880
375.505675	17908.430184	29.615898
375.499654	17947.313231	29.620916
376.225137	17980.914151	29.625933
376.709956	18013.765187	29.630951
377.024741	18047.651756	29.635968
377.354557	18069.150011	29.640986
378.217515	18116.873631	29.646004
378.481560	18137.050784	29.651021
379.008386	18167.618820	29.656039
379.168505	18184.050306	29.661056
379.592409	18214.304412	29.666074
379.672261	18247.062133	29.671092
380.426705	18271.804035	29.676109
380.774290	18304.895906	29.681127
380.891418	18330.066537	29.686144
381.479047	18361.670047	29.691162
381.773807	18403.223741	29.696180
382.264178	18433.281224	29.701197
382.322638	18457.071328	29.706215
382.911723	18491.589702	29.711232
383.609054	18517.407106	29.716250
383.639036	18555.426441	29.721268
384.182979	18568.873604	29.726285
384.752983	18600.675965	29.731303
385.084311	18637.483761	29.736320
385.343673	18661.739073	29.741338
385.706354	18700.895491	29.746356
386.160888	18714.007591	29.751373
386.391647	18745.172722	29.756391
386.589672	18783.913594	29.761408
387.057435	18809.580265	29.766426
387.890109	18852.936262	29.771444
388.177856	18880.847801	29.776461
388.520860	18907.805923	29.781479
388.488422	18942.456465	29.786496
389.462813	18961.724081	29.791514
389.711915	18999.618302	29.796532
390.060159	19025.032350	29.801549
390.899822	19051.112374	29.806567
391.104967	19073.321491	29.811584
391.476196	19104.341077	29.816602
391.630420	19125.250184	29.821620
392.272911	19157.837751	29.826637
392.642978	19189.023221	29.831655
392.971327	19211.834857	29.836672
393.233106	19235.962904	29.841690
393.666364	19261.689583	29.846708
393.914290	19286.676050	29.851725
394.396784	19304.915593	29.856743
394.728142	19333.719294	29.861760
395.010545	19350.253083	29.866778
395.147669	19381.896821	29.871796
395.559897	19417.601982	29.876813
396.085349	19439.312415	29.881831
396.109481	19473.738707	29.886848
396.970526	19504.859278	29.891866
397.182079	19537.665522	29.896884
397.531255	19564.888542	29.901901
397.686499	19604.235907	29.906919
397.922466	19638.882883	29.911936
398.543706	19663.119173	29.916954
398.865181	19707.870537	29.921972
399.254581	19739.988739	29.926989
399.836028	19771.633779	29.932007
400.059912	19813.087614	29.937024
400.532559	19841.641779	29.942042
401.066016	19875.216810	29.947060
401.404528	19911.259998	29.952077
402.086740	19941.409844	29.957095
402.377418	19982.019025	29.962112
402.880666	20009.759619	29.967130
403.121420	20052.984926	29.972148
403.919242	20083.918386	29.977165
404.202511	20115.782118	29.982183
404.625387	20153.609198	29.987200
405.167114	20172.916711	29.992218
405.608115	20202.301296	29.997236
406.228002	20238.060552	30.002253
406.791485	20268.676819	30.007271
406.816455	20291.451840	30.012288
407.418959	20310.728959	30.017306
407.451511	20341.510476	30.022324
408.170839	20375.869290	30.027341
408.557058	20399.259473	30.032359
408.918536	20428.015923	30.037376
409.869543	20454.612618	30.042394
409.579550	20478.229911	30.047412
409.763630	20501.871264	30.052429
410.464496	20540.886147	30.057447
410.648185	20576.467623	30.062464
410.924789	20600.711851	30.067482
411.427849	20653.229077	30.072500
412.033492	20680.561247	30.077517
412.979543	20701.271906	30.082535
412.970938	20736.406237	30.087552
413.538836	20762.287948	30.092570
414.128419	20791.112907	30.097588
414.133928	20819.563146	30.102605
414.618154	20849.014236	30.107623
414.715433	20891.198028	30.112640
415.216768	20918.060652	30.117658
415.612482	20952.020114	30.122676
416.233634	20993.594009	30.127693
416.770746	21009.885467	30.132711
416.990432	21045.272772	30.137728
417.351726	21083.768039	30.142746
417.836559	21115.669682	30.147764
418.370483	21142.552499	30.152781
418.824523	21178.606087	30.157799
419.219922	21218.010506	30.162816
419.384813	21246.931753	30.167834
419.538292	21281.797581	30.172852
420.030974	21321.154607	30.177869
420.631254	21358.420527	30.182887
421.128791	21397.778505	30.187904
421.596539	21420.265765	30.192922
421.799890	21450.849176	30.197940
422.014692	21477.507832	30.202957
422.662176	21511.984920	30.207975
422.742422	21553.294941	30.212992
423.185155	21577.252919	30.218010
423.974828	21613.012228	30.223028
423.989209	21648.160415	30.228045
424.846113	21669.159802	30.233063
425.010577	21716.318649	30.238080
425.625832	21743.069130	30.243098
425.880123	21777.187680	30.248116
426.260109	21820.156383	30.253133
427.022190	21843.565210	30.258151
426.955529	21878.922807	30.263168
427.738721	21909.185613	30.268186
428.474480	21947.395400	30.273204
428.342092	21989.960522	30.278221
429.041922	22016.924498	30.283239
429.776197	22052.916233	30.288256
430.160617	22083.267418	30.293274
430.702297	22114.921869	30.298292
431.227788	22146.017720	30.303309
431.643143	22175.851492	30.308327
431.692903	22204.865961	30.313344
432.228631	22237.395175	30.318362
432.484485	22272.518888	30.323380
432.644838	22307.540217	30.328397
433.266954	22348.393530	30.333415
433.615402	22384.033538	30.338432
434.343456	22428.363743	30.343450
434.585017	22464.210826	30.348468
434.783083	22504.907626	30.353485
435.565423	22540.195485	30.358503
435.786852	22581.776360	30.363520
436.466625	22615.044074	30.368538
437.085189	22645.638196	30.373556
437.117242	22697.489137	30.378573
437.799931	22739.295245	30.383591
437.795776	22768.647583	30.388608
438.558477	22806.862735	30.393626
439.370946	22845.118620	30.398644
439.595354	22883.952849	30.403661
440.072601	22920.898812	30.408679
440.507625	22951.654739	30.413696
440.604779	22998.531832	30.418714
441.119824	23030.958763	30.423732
441.624931	23078.446626	30.428749
442.031303	23107.547118	30.433767
442.702544	23154.742786	30.438784
443.248595	23198.061218	30.443802
443.890012	23229.554594	30.448820
444.371936	23268.225664	30.453837
444.772168	23290.496353	30.458855
444.938640	23324.738196	30.463872
445.503835	23355.847039	30.468890
446.262133	23390.079385	30.473908
446.505354	23431.433230	30.478925
446.962340	23449.239950	30.483943
447.539230	23495.245833	30.488960
447.745847	23524.610324	30.493978
448.459097	23554.706300	30.498996
448.839847	23599.319380	30.504013
449.493974	23626.293481	30.509031
449.243875	23660.813086	30.514048
449.760787	23692.531348	30.519066
450.563901	23727.785122	30.524084
450.479094	23772.404731	30.529101
451.310564	23798.107123	30.534119
451.655660	23837.609526	30.539136
451.826538	23876.696146	30.544154
452.374177	23906.627760	30.549172
452.826097	23944.923706	30.554189
453.699169	23971.868432	30.559207
453.791988	23997.835284	30.564224
454.007496	24038.677940	30.569242
454.635563	24067.445338	30.574260
454.747186	24117.833455	30.579277
455.216148	24146.302456	30.584295
455.572160	24185.583079	30.589312
456.053550	24238.225376	30.594330
456.340607	24276.804818	30.599348
456.945949	24323.393290	30.604365
457.677348	24361.539840	30.609383
458.251291	24405.676764	30.614400
458.582031	24451.289124	30.619418
459.051049	24491.999445	30.624436
459.137084	24527.452382	30.629453
460.090827	24562.660878	30.634471
460.489761	24605.821139	30.639488
460.798687	24644.687964	30.644506
461.592052	24697.992866	30.649524
461.886429	24734.928862	30.654541
462.233922	24778.189537	30.659559
462.671564	24818.498949	30.664576
463.074316	24864.996254	30.669594
463.690420	24895.959123	30.674612
464.085595	24951.863449	30.679629
464.652657	24981.203911	30.684647
465.048490	25034.197147	30.689664
465.323315	25068.156446	30.694682
466.195817	25106.139371	30.699700
466.737462	25153.541791	30.704717
467.264827	25195.086284	30.709735
467.830396	25237.097679	30.714752
467.913122	25272.458077	30.719770
468.644141	25312.054571	30.724788
468.902770	25362.090824	30.729805
469.603679	25402.395894	30.734823
469.846415	25452.056535	30.739840
470.446446	25501.815907	30.744858
471.172738	25542.038248	30.749876
471.181043	25585.609420	30.754893
471.776863	25630.726840	30.759911
472.323524	25675.833588	30.764928
472.381741	25711.883413	30.769946
472.951482	25752.876555	30.774964
473.213274	25805.326579	30.779981
474.019296	25858.254477	30.784999
474.573837	25902.464699	30.790016
474.827673	25948.428112	30.795034
475.783826	25981.405887	30.800052
476.054834	26035.407001	30.805069
476.603755	26079.350491	30.810087
477.045323	26117.769708	30.815104
477.344922	26170.820217	30.820122
477.837962	26213.748137	30.825140
478.053064	26265.011788	30.830157
478.773472	26307.489099	30.835175
479.147959	26352.272818	30.840192
479.628143	26404.937720	30.845210
480.193077	26453.254633	30.850228
479.971714	26503.802618	30.855245
480.746529	26554.826255	30.860263
481.385022	26602.809665	30.865280
481.616666	26667.067954	30.870298
482.341982	26710.286733	30.875316
482.874058	26753.887739	30.880333
483.321219	26804.644578	30.885351
483.864244	26855.641213	30.890368
484.234516	26891.323260	30.895386
484.802696	26929.631853	30.900404
485.220806	26976.611791	30.905421
485.531484	27022.492944	30.910439
486.261661	27066.528823	30.915456
486.617256	27118.061965	30.920474
487.303807	27156.897203	30.925492
487.836508	27217.962669	30.930509
488.313099	27264.441605	30.935527
489.119519	27310.168935	30.940544
489.023690	27349.244473	30.945562
489.689898	27398.455777	30.950580
490.333433	27448.128384	30.955597
490.678943	27493.052339	30.960615
491.220054	27540.912506	30.965632
491.359424	27590.877148	30.970650
491.721160	27639.839830	30.975668
492.297968	27699.492739	30.980685
492.696415	27747.036383	30.985703
493.146332	27798.937647	30.990720
493.573181	27862.928309	30.995738
494.454467	27916.777517	31.000756
495.062529	27977.218025	31.005773
495.180304	28032.247584	31.010791
495.791151	28075.201634	31.015808
496.068981	28148.663117	31.020826
496.947173	28194.750001	31.025844
497.629871	28248.446969	31.030861
497.827705	28307.211946	31.035879
498.802796	28351.358832	31.040896
499.136803	28419.975963	31.045914
499.502541	28470.738522	31.050932
500.076820	28523.075650	31.055949
500.654466	28573.670945	31.060967
501.115871	28616.357663	31.065984
501.451866	28677.814135	31.071002
502.275961	28729.482743	31.076020
502.860937	28778.099360	31.081037
503.031474	28829.627177	31.086055
503.963481	28877.221275	31.091072
504.402566	28936.472151	31.096090
505.052228	28983.188889	31.101108
505.756335	29032.483723	31.106125
506.152334	29082.511127	31.111143
506.788233	29123.870411	31.116160
506.964361	29171.091912	31.121178
507.396602	29225.694611	31.126196
507.756727	29277.315416	31.131213
508.340717	29331.454806	31.136231
508.748819	29376.906435	31.141248
508.719927	29431.437795	31.146266
509.944401	29491.989779	31.151284
510.131429	29544.129026	31.156301
510.556107	29585.420237	31.161319
511.702241	29647.001614	31.166336
511.997693	29702.764220	31.171354
512.295014	29743.064129	31.176372
513.170797	29802.053222	31.181389
513.470973	29855.780563	31.186407
514.032786	29901.179723	31.191424
514.592000	29957.076174	31.196442
515.420986	30007.514138	31.201460
515.771436	30047.279065	31.206477
516.109251	30098.035187	31.211495
516.798016	30139.627906	31.216512
516.975506	30189.603127	31.221530
517.558772	30236.258473	31.226548
518.424584	30279.216769	31.231565
518.484959	30328.501870	31.236583
519.215490	30364.396438	31.241600
519.735192	30417.183661	31.246618
520.126910	30453.443672	31.251636
520.826442	30508.813844	31.256653
520.948371	30552.949703	31.261671
521.452569	30603.168622	31.266688
521.578968	30657.163799	31.271706
522.017294	30709.167110	31.276724
522.717471	30756.056903	31.281741
523.087186	30810.154272	31.286759
523.877297	30876.866079	31.291776
524.214180	30947.291071	31.296794
524.968286	30987.486698	31.301812
525.671253	31058.794968	31.306829
525.737041	31123.712340	31.311847
526.811374	31164.555848	31.316864
527.280667	31232.830286	31.321882
527.748464	31289.459179	31.326900
528.598689	31336.928345	31.331917
528.733377	31393.887197	31.336935
529.565338	31445.688716	31.341952
529.995022	31509.701678	31.346970
530.817729	31562.420106	31.351988
531.044530	31613.192646	31.357005
531.341201	31680.762188	31.362023
532.150106	31729.296280	31.367040
532.557748	31790.732841	31.372058
532.774980	31839.535521	31.377076
533.673564	31894.697252	31.382093
534.068304	31959.856710	31.387111
534.715519	32012.548720	31.392128
535.398700	32068.484993	31.397146
535.822680	32134.927657	31.402164
536.223484	32183.552607	31.407181
536.900700	32256.371943	31.412199
537.592826	32309.644315	31.417216
537.910012	32369.819896	31.422234
538.388502	32431.089181	31.427252
539.146752	32486.380104	31.432269
539.718347	32550.843509	31.437287
540.318183	32600.029898	31.442304
540.591890	32664.678690	31.447322
540.868304	32725.228258	31.452340
541.753676	32780.006802	31.457357
542.100328	32847.209627	31.462375
542.802561	32911.911480	31.467392
543.677548	32975.404807	31.472410
544.093461	33035.714616	31.477428
544.756906	33093.146810	31.482445
545.026277	33154.623587	31.487463
545.773829	33202.499722	31.492480
546.156259	33263.970792	31.497498
546.796995	33312.641176	31.502516
547.412716	33364.670262	31.507533
547.738398	33431.039360	31.512551
548.241626	33492.939333	31.517568
548.546944	33554.020237	31.522586
549.303056	33616.623533	31.527604
550.000368	33672.837059	31.532621
550.351315	33739.001158	31.537639
551.217765	33801.738320	31.542656
551.988447	33854.440605	31.547674
552.426858	33912.846762	31.552692
553.477150	33956.162151	31.557709
553.543925	34013.535087	31.562727
554.268520	34056.431246	31.567744
554.649167	34104.799691	31.572762
555.156581	34158.953900	31.577780
555.559445	34202.774633	31.582797
555.931209	34261.249758	31.587815
556.634603	34311.493546	31.592832
557.064202	34365.197351	31.597850
557.138741	34427.922568	31.602868
558.096012	34485.547312	31.607885
558.353752	34548.368872	31.612903
559.096913	34597.877887	31.617920
559.764136	34666.000197	31.622938
559.723626	34728.859111	31.627956
560.646723	34794.140321	31.632973
560.964191	34866.281884	31.637991
561.731389	34929.774745	31.643008
562.147475	34999.495730	31.648026
562.868086	35071.681874	31.653044
563.508382	35127.202471	31.658061
563.756513	35205.719234	31.663079
564.307457	35262.744641	31.668096
565.390946	35326.101361	31.673114
565.616026	35399.879362	31.678132
566.346635	35464.140756	31.683149
566.755640	35539.971855	31.688167
567.199788	35604.145435	31.693184
568.144819	35671.291409	31.698202
568.624175	35747.231670	31.703220
569.401678	35803.485947	31.708237
569.898887	35881.014468	31.713255
570.366111	35942.392314	31.718272
571.123311	36005.748602	31.723290
571.629576	36084.759861	31.728308
572.542857	36141.825940	31.733325
573.016425	36211.520010	31.738343
573.545502	36276.773949	31.743360
574.059341	36336.005560	31.748378
574.514272	36405.151133	31.753396
575.244038	36454.276108	31.758413
575.611660	36531.579522	31.763431
576.384592	36596.734302	31.768448
576.972039	36653.549757	31.773466
577.384121	36731.802998	31.778484
578.092561	36797.903412	31.783501
578.575566	36876.682102	31.788519
579.428192	36938.687625	31.793536
579.810538	37003.457146	31.798554
580.390156	37080.153384	31.803572
581.107969	37130.475245	31.808589
581.809315	37207.189756	31.813607
582.136739	37274.077736	31.818624
582.842692	37331.822602	31.823642
583.183220	37409.254177	31.828660
583.829967	37475.446175	31.833677
584.430796	37539.865826	31.838695
584.951785	37609.756273	31.843712
585.519076	37679.083805	31.848730
586.016641	37756.636070	31.853748
586.599453	37821.649945	31.858765
587.138183	37890.588458	31.863783
587.596490	37955.639192	31.868800
588.649688	38033.782498	31.873818
589.086525	38104.013878	31.878836
589.992996	38167.873839	31.883853
590.260495	38240.955640	31.888871
590.783486	38307.363682	31.893888
591.725802	38369.242457	31.898906
592.164194	38433.932037	31.903924
592.702658	38485.546768	31.908941
593.007635	38557.045374	31.913959
593.722525	38612.684261	31.918976
594.482293	38677.602467	31.923994
594.933437	38743.462114	31.929012
595.512578	38815.370916	31.934029
595.851802	38883.626486	31.939047
596.243597	38947.741624	31.944064
596.860603	39012.523652	31.949082
597.546105	39086.158369	31.954100
598.286352	39157.325307	31.959117
598.929812	39228.754753	31.964135
599.088242	39304.889228	31.969152
599.890121	39375.800599	31.974170
600.422129	39452.915583	31.979188
601.056203	39527.220328	31.984205
601.677878	39606.717058	31.989223
602.049244	39683.250342	31.994240
603.065209	39760.677986	31.999258
603.255252	39838.520393	32.004276
604.096166	39909.998741	32.009293
604.779249	39993.268787	32.014311
605.512906	40074.633611	32.019328
606.075753	40147.933005	32.024346
606.614744	40233.062078	32.029364
607.456905	40314.198503	32.034381
608.015904	40388.219247	32.039399
608.216799	40471.230288	32.044416
608.884180	40542.799783	32.049434
609.669481	40622.586360	32.054452
610.038011	40703.929133	32.059469
610.539091	40785.240863	32.064487
611.451479	40878.727473	32.069504
612.131728	40953.541756	32.074522
612.504965	41043.443716	32.079540
612.924071	41115.208037	32.084557
613.840922	41194.274473	32.089575
614.600700	41280.770392	32.094592
615.411757	41361.259908	32.099610
615.760428	41441.993593	32.104628
616.427636	41521.876200	32.109645
617.856714	41599.950401	32.114663
617.845073	41684.672125	32.119680
618.577379	41760.661801	32.124698
618.953567	41834.276584	32.129716
619.831625	41916.490671	32.134733
620.499311	41997.117166	32.139751
620.738215	42078.572660	32.144768
621.307269	42148.475564	32.149786
622.154313	42238.497514	32.154804
622.859324	42329.471608	32.159821
623.623877	42400.962750	32.164839
624.030533	42483.639353	32.169856
624.611529	42555.628722	32.174874
625.084882	42639.504196	32.179892
625.656242	42719.859293	32.184909
626.262937	42803.966026	32.189927
626.783090	42894.869274	32.194944
627.782842	42985.908316	32.199962
628.030006	43071.190255	32.204980
628.942632	43152.314813	32.209997
629.631480	43230.063673	32.215015
630.076278	43327.624512	32.220032
630.979222	43399.914342	32.225050
631.161231	43493.032915	32.230068
631.924776	43579.235786	32.235085
632.670109	43655.913032	32.240103
632.976508	43729.711027	32.245120
634.244653	43799.813890	32.250138
634.399776	43881.508968	32.255156
635.308685	43951.681303	32.260173
635.961007	44032.966413	32.265191
636.195779	44104.242287	32.270208
637.286250	44177.782876	32.275226
637.698837	44267.374966	32.280244
638.004229	44347.995765	32.285261
638.887546	44435.692054	32.290279
639.485144	44511.421561	32.295296
640.497160	44584.806218	32.300314
640.747174	44672.046333	32.305332
641.680788	44749.331572	32.310349
642.295154	44830.717982	32.315367
642.628328	44924.311225	32.320384
643.805800	45002.769687	32.325402
644.359988	45077.567681	32.330420
644.454405	45175.404485	32.335437
645.177044	45243.029497	32.340455
645.433133	45330.682150	32.345472
646.401380	45423.392860	32.350490
647.144902	45517.966360	32.355508
647.752579	45607.920946	32.360525
648.601251	45697.463479	32.365543
649.155429	45784.465794	32.370560
649.963587	45869.307629	32.375578
650.509851	45958.386708	32.380596
651.231475	46058.802123	32.385613
652.020168	46137.784343	32.390631
652.688362	46225.701379	32.395648
653.443776	46314.627536	32.400666
653.829430	46405.727887	32.405684
654.208535	46489.307701	32.410701
655.456200	46573.899985	32.415719
655.647489	46677.021136	32.420736
656.462541	46756.753155	32.425754
656.877490	46845.251800	32.430772
657.449732	46950.225118	32.435789
658.142892	47040.364992	32.440807
658.692401	47145.219986	32.445824
659.667486	47238.421614	32.450842
660.106289	47335.126227	32.455860
660.820060	47443.511612	32.460877
661.674875	47527.219401	32.465895
661.966457	47628.364803	32.470912
663.141782	47723.266295	32.475930
664.063833	47806.275726	32.480948
664.318376	47906.089694	32.485965
664.996817	47981.604940	32.490983
665.997651	48090.113887	32.496000
666.220245	48170.638302	32.501018
667.300695	48265.766623	32.506036
667.881540	48362.089745	32.511053
668.832490	48446.013045	32.516071
669.453786	48553.883129	32.521088
670.059788	48634.671364	32.526106
670.764399	48724.517257	32.531124
670.895168	48812.771988	32.536141
671.899421	48902.714427	32.541159
672.211780	49006.027079	32.546176
672.963371	49097.534521	32.551194
674.135312	49197.370837	32.556212
674.509430	49286.989782	32.561229
675.356031	49373.656886	32.566247
675.722125	49466.474244	32.571264
676.563815	49560.912582	32.576282
677.310784	49647.771113	32.581300
677.517132	49733.250806	32.586317
678.762658	49822.971290	32.591335
678.882182	49910.190628	32.596352
679.890285	49998.381460	32.601370
680.789036	50085.633769	32.606388
681.167596	50164.387777	32.611405
681.968607	50251.195865	32.616423
682.545262	50340.511409	32.621440
683.163650	50441.191145	32.626458
684.007274	50529.882232	32.631476
684.315387	50616.779813	32.636493
685.163726	50714.504429	32.641511
685.242909	50811.952473	32.646528
686.315502	50893.418412	32.651546
687.202579	51000.177968	32.656564
687.257195	51102.356821	32.661581
688.242394	51194.280919	32.666599
688.597385	51303.972945	32.671616
689.539876	51404.591431	32.676634
690.836791	51484.310739	32.681652
691.281197	51579.238433	32.686669
692.542518	51663.285478	32.691687
693.431902	51761.962509	32.696704
694.362664	51858.144098	32.701722
695.506951	51939.457264	32.706740
695.684501	52031.474697	32.711757
696.602852	52107.582361	32.716775
697.104176	52194.739322	32.721792
697.724225	52268.502582	32.726810
698.423400	52361.818849	32.731828
699.034441	52459.326141	32.736845
699.816953	52548.371383	32.741863
700.434313	52637.273769	32.746880
701.254617	52725.902913	32.751898
702.020059	52820.177027	32.756916
702.543292	52905.545589	32.761933
703.118092	52994.911524	32.766951
703.449773	53086.030235	32.771968
703.890094	53186.886289	32.776986
705.012352	53285.033373	32.782004
705.514854	53392.703606	32.787021
706.262339	53486.522680	32.792039
707.098361	53582.924280	32.797056
707.919883	53692.015490	32.802074
708.873928	53778.832929	32.807092
709.009474	53883.931893	32.812109
709.965294	53979.917578	32.817127
710.593897	54076.823455	32.822144
711.286156	54177.030043	32.827162
712.391767	54271.343307	32.832180
712.887199	54368.790746	32.837197
713.385149	54468.190619	32.842215
714.027947	54570.669356	32.847232
714.553422	54678.323858	32.852250
715.478580	54779.992446	32.857268
716.205052	54882.831748	32.862285
716.846919	54979.695631	32.867303
717.944107	55086.512200	32.872320
718.460979	55184.326585	32.877338
719.501766	55282.313854	32.882356
720.135591	55391.224348	32.887373
721.050319	55474.965933	32.892391
721.451307	55572.415962	32.897408
722.130015	55678.180213	32.902426
722.901781	55772.644319	32.907444
723.665284	55876.430464	32.912461
724.382793	55976.578793	32.917479
725.143999	56072.328793	32.922496
725.451226	56164.394608	32.927514
726.105448	56259.253282	32.932532
726.136235	56352.907509	32.937549
727.419816	56441.767373	32.942567
728.379546	56546.895770	32.947584
729.108833	56639.001385	32.952602
729.704443	56742.630241	32.957620
730.320931	56853.858063	32.962637
731.221039	56946.233837	32.967655
731.922804	57053.960505	32.972672
732.514049	57150.129258	32.977690
733.437724	57246.527852	32.982708
734.047527	57362.625414	32.987725
734.969032	57455.120065	32.992743
735.623150	57556.443233	32.997760
736.398089	57667.662004	33.002778
736.902714	57768.442227	33.007796
737.765045	57880.323896	33.012813
738.879110	57976.852495	33.017831
739.466099	58087.839263	33.022848
740.170541	58190.288494	33.027866
740.868581	58289.472094	33.032884
741.216334	58404.418305	33.037901
742.507734	58517.490145	33.042919
742.894203	58614.135832	33.047936
743.639798	58723.753782	33.052954
744.977849	58829.267625	33.057972
745.604441	58941.939912	33.062989
746.112527	59046.972838	33.068007
747.305943	59150.673225	33.073024
747.628278	59259.959625	33.078042
748.369247	59360.929910	33.083060
749.124425	59466.480293	33.088077
750.386902	59567.908864	33.093095
751.148467	59672.283752	33.098112
751.331405	59784.288351	33.103130
752.088069	59888.090037	33.108148
753.050146	60003.834848	33.113165
753.761095	60112.536995	33.118183
754.697370	60211.501011	33.123200
755.414867	60329.512827	33.128218
756.704119	60432.729908	33.133236
757.366196	60534.313180	33.138253
757.958055	60640.117886	33.143271
758.813025	60740.437824	33.148288
759.293690	60835.201376	33.153306
760.154065	60937.752475	33.158324
760.916385	61047.146355	33.163341
761.665679	61158.186292	33.168359
762.488593	61267.230024	33.173376
763.085180	61375.351054	33.178394
764.011929	61477.786436	33.183412
764.679142	61588.134383	33.188429
765.577529	61702.325546	33.193447
766.040744	61804.504240	33.198464
766.551174	61918.748135	33.203482
767.656896	62022.471342	33.208500
768.266881	62140.435548	33.213517
768.978417	62242.916672	33.218535
769.886161	62340.087974	33.223552
771.173441	62456.406011	33.228570
772.127080	62560.776535	33.233588
772.503185	62662.518800	33.238605
773.506789	62765.352436	33.243623
774.312810	62872.542814	33.248640
775.551017	62984.150184	33.253658
776.101602	63068.356399	33.258676
776.663473	63172.946528	33.263693
777.443128	63251.559384	33.268711
778.430790	63353.930832	33.273728
778.922369	63437.863863	33.278746
779.505293	63531.232286	33.283764
780.399707	63632.678682	33.288781
781.030394	63726.887130	33.293799
781.726189	63821.274874	33.298816
782.140067	63924.768096	33.303834
782.978521	64023.893106	33.308852
783.636202	64135.040109	33.313869
784.685051	64234.782429	33.318887
785.549787	64346.003779	33.323904
786.011342	64456.723479	33.328922
786.546596	64559.573963	33.333940
787.251122	64668.004150	33.338957
788.293900	64790.438102	33.343975
788.984058	64900.787311	33.348992
789.758971	65016.635545	33.354010
790.546803	65129.574321	33.359028
791.176552	65247.053547	33.364045
791.947446	65361.159570	33.369063
792.647998	65481.896743	33.374080
793.395890	65609.081349	33.379098
794.134884	65723.163014	33.384116
794.979630	65845.054297	33.389133
795.720489	65975.384265	33.394151
796.982544	66097.416619	33.399168
797.495069	66227.077858	33.404186
798.410590	66347.006857	33.409204
799.116625	66471.497788	33.414221
799.742368	66602.634627	33.419239
801.183950	66714.297910	33.424256
801.678610	66840.615153	33.429274
802.350033	66960.866201	33.434292
803.199215	67082.194929	33.439309
803.823444	67213.089251	33.444327
804.811514	67338.973824	33.449344
805.211794	67464.456897	33.454362
806.419245	67592.449980	33.459380
807.629626	67724.186240	33.464397
808.396042	67861.389827	33.469415
809.648113	67975.481034	33.474432
810.194882	68089.373378	33.479450
811.169480	68201.292477	33.484468
812.137415	68330.044088	33.489485
812.705943	68444.465840	33.494503
813.850916	68555.871787	33.499520
814.505743	68686.934547	33.504538
815.197350	68798.802437	33.509556
816.075929	68912.549475	33.514573
816.505807	69035.052581	33.519591
817.280608	69163.626204	33.524608
818.411119	69292.350429	33.529626
819.144554	69420.173692	33.534644
820.052154	69535.164874	33.539661
820.742214	69653.581790	33.544679
821.768251	69772.418024	33.549696
822.497922	69898.600778	33.554714
822.829125	70022.605467	33.559732
823.731050	70154.559545	33.564749
824.454373	70280.442085	33.569767
825.544318	70395.091570	33.574784
826.143571	70536.740993	33.579802
826.834209	70661.777532	33.584820
827.992372	70795.337233	33.589837
828.989533	70930.764499	33.594855
829.680132	71053.236023	33.599872
830.574646	71179.980798	33.604890
830.988293	71293.178703	33.609908
832.092959	71412.352479	33.614925
832.543633	71534.505974	33.619943
833.776462	71648.733799	33.624960
834.425949	71777.773811	33.629978
835.036872	71890.423680	33.634996
835.728324	72017.415634	33.640013
836.554458	72147.200126	33.645031
837.858082	72269.577159	33.650048
838.183816	72407.375993	33.655066
839.066966	72532.189158	33.660084
839.908712	72651.166609	33.665101
840.735685	72798.143207	33.670119
841.797080	72922.581320	33.675136
842.773873	73056.482209	33.680154
843.716348	73180.220525	33.685172
844.751339	73305.759256	33.690189
845.365180	73442.416602	33.695207
846.366992	73567.930709	33.700224
847.205999	73700.574536	33.705242
848.006448	73823.226929	33.710260
849.073871	73953.190983	33.715277
849.961879	74090.932762	33.720295
850.857750	74205.552291	33.725312
851.811500	74332.957068	33.730330
852.468664	74457.540348	33.735348
853.183025	74584.239893	33.740365
854.391198	74719.896199	33.745383
855.247029	74847.630057	33.750400
855.865396	74977.339245	33.755418
856.741349	75111.294680	33.760436
857.506011	75240.013556	33.765453
858.172570	75372.677034	33.770471
859.185502	75502.785763	33.775488
860.218598	75637.287629	33.780506
860.901256	75776.825883	33.785524
862.304504	75900.332568	33.790541
862.750529	76036.572084	33.795559
863.721616	76162.662677	33.800576
864.568282	76296.193721	33.805594
865.617583	76434.404171	33.810612
866.922557	76560.561985	33.815629
867.945738	76691.738613	33.820647
868.508264	76816.875832	33.825664
869.399653	76946.469185	33.830682
870.292814	77072.584159	33.835700
871.355095	77187.824164	33.840717
871.766414	77324.127914	33.845735
872.592939	77455.872887	33.850752
873.344161	77587.934706	33.855770
874.077008	77730.373917	33.860788
875.041321	77855.943898	33.865805
875.504862	78001.446580	33.870823
876.383784	78128.037952	33.875840
877.639698	78280.110072	33.880858
878.199064	78431.248374	33.885876
879.134117	78555.195122	33.890893
880.043001	78710.306897	33.895911
880.952700	78844.639791	33.900928
881.787440	78981.807146	33.905946
882.578394	79133.557092	33.910964
883.527059	79269.777476	33.915981
884.127000	79421.662161	33.920999
885.145349	79562.104765	33.926016
886.257676	79710.825964	33.931034
886.881003	79849.412604	33.936052
888.079800	79985.102514	33.941069
888.986644	80133.613761	33.946087
890.046489	80261.401799	33.951104
890.615026	80400.165346	33.956122
891.525511	80525.872982	33.961140
892.887437	80652.151929	33.966157
893.140412	80784.523643	33.971175
894.007356	80915.959529	33.976192
895.008208	81047.513208	33.981210
895.340955	81185.890354	33.986228
896.639480	81318.041653	33.991245
897.454838	81473.333326	33.996263
898.392724	81605.033488	34.001280
899.401688	81742.454439	34.006298
900.433503	81894.549943	34.011316
901.236426	82025.597910	34.016333
902.086984	82168.469468	34.021351
903.066322	82314.509240	34.026368
903.988417	82464.178264	34.031386
904.725236	82611.019229	34.036404
905.542165	82748.370411	34.041421
906.430928	82903.925360	34.046439
907.039565	83050.239893	34.051456
908.273498	83199.381293	34.056474
909.229228	83357.129979	34.061492
910.238430	83495.744511	34.066509
910.780030	83647.875735	34.071527
911.848927	83806.507207	34.076544
912.920832	83951.295619	34.081562
913.452272	84115.472027	34.086580
914.970458	84264.263262	34.091597
915.746293	84431.666309	34.096615
916.539640	84587.691265	34.101632
917.577200	84733.350742	34.106650
918.515368	84888.385691	34.111668
919.589372	85034.154916	34.116685
920.408027	85185.130447	34.121703
921.163420	85344.596206	34.126720
922.225964	85494.533670	34.131738
923.052627	85658.488636	34.136756
924.428201	85818.544775	34.141773
925.011411	85974.088557	34.146791
925.951591	86131.036033	34.151808
926.898677	86289.875402	34.156826
927.576314	86448.570570	34.161844
928.711511	86600.401419	34.166861
929.806934	86762.807315	34.171879
930.586643	86924.545158	34.176896
931.949392	87071.114586	34.181914
932.854866	87230.694895	34.186932
933.868412	87363.054326	34.191949
935.024381	87519.798191	34.196967
935.863355	87679.481119	34.201984
936.702049	87828.052982	34.207002
937.412673	87984.778645	34.212020
938.948962	88135.768349	34.217037
939.519712	88287.918538	34.222055
940.141811	88440.270042	34.227072
941.559718	88589.655837	34.232090
942.393348	88751.080816	34.237108
943.317413	88895.259674	34.242125
944.454409	89049.036089	34.247143
945.393846	89203.453699	34.252160
946.217412	89351.221196	34.257178
947.003358	89505.090239	34.262196
947.803252	89667.412986	34.267213
948.771486	89822.405731	34.272231
949.526469	89975.669034	34.277248
950.364038	90129.514560	34.282266
951.371789	90292.402064	34.287284
952.361660	90432.364329	34.292301
953.342751	90586.201701	34.297319
953.935519	90729.535017	34.302336
955.120611	90873.258568	34.307354
955.672166	91037.758145	34.312372
956.948431	91188.474669	34.317389
957.693974	91337.425478	34.322407
958.766693	91501.772414	34.327424
959.919828	91651.240032	34.332442
960.595158	91812.553510	34.337460
961.219442	91970.237202	34.342477
962.201001	92136.926334	34.347495
963.044342	92307.475021	34.352512
964.274425	92467.485886	34.357530
965.192272	92641.904481	34.362548
966.303973	92809.969164	34.367565
966.980525	92983.670567	34.372583
967.578623	93147.961519	34.377600
968.953380	93321.587847	34.382618
969.605673	93508.411844	34.387636
970.955087	93669.151408	34.392653
971.944327	93840.579140	34.397671
972.576025	94017.498108	34.402688
973.902678	94199.373597	34.407706
974.687585	94373.250476	34.412724
975.551728	94551.362829	34.417741
976.428833	94722.834231	34.422759
977.403092	94911.406998	34.427776
978.812992	95085.248844	34.432794
979.434349	95274.996815	34.437812
980.526598	95463.079516	34.442829
981.927055	95647.745033	34.447847
982.928316	95827.458077	34.452864
984.223452	96008.795012	34.457882
984.650521	96190.492031	34.462900
985.467163	96362.326585	34.467917
986.444348	96545.036702	34.472935
987.548352	96739.046004	34.477952
988.756009	96928.937516	34.482970
989.593937	97113.542301	34.487988
990.762576	97293.776307	34.493005
991.894129	97485.387540	34.498023
992.656193	97668.369313	34.503040
993.887335	97843.032262	34.508058
994.698211	98035.713620	34.513076
995.849881	98226.162299	34.518093
996.873806	98411.619497	34.523111
997.625004	98589.374123	34.528128
998.827001	98765.757615	34.533146
999.600272	98971.994215	34.538164
1000.702873	99161.546378	34.543181
1001.832808	99347.068861	34.548199
1002.614673	99534.777509	34.553216
1004.048139	99726.691338	34.558234
1004.712544	99910.661451	34.563252
1006.035784	100100.798250	34.568269
1007.346619	100275.585057	34.573287
1008.026845	100467.046509	34.578304
1008.781045	100646.119245	34.583322
1009.902627	100838.377896	34.588340
1010.756956	101020.703722	34.593357
1012.144030	101200.182199	34.598375
1013.364949	101382.082743	34.603392
1014.731805	101563.998430	34.608410
1015.741239	101747.798022	34.613428
1016.949676	101922.429336	34.618445
1017.793861	102086.984897	34.623463
1018.493809	102274.549815	34.628480
1019.570414	102433.370516	34.633498
1020.644228	102608.142684	34.638516
1021.214296	102777.648831	34.643533
1022.464830	102939.255246	34.648551
1023.404377	103113.850388	34.653568
1024.425882	103287.394690	34.658586
1025.218504	103457.394020	34.663604
1025.978261	103634.365245	34.668621
1027.314132	103803.010575	34.673639
1027.824677	103997.375641	34.678656
1029.290853	104172.346698	34.683674
1030.400742	104359.865155	34.688692
1030.959727	104538.205458	34.693709
1032.350663	104716.371423	34.698727
1033.328884	104904.738743	34.703744
1034.445584	105088.563114	34.708762
1035.525542	105265.745677	34.713780
1036.456757	105461.837769	34.718797
1038.067217	105648.940667	34.723815
1038.507755	105841.152468	34.728832
1039.574481	106022.547174	34.733850
1040.853699	106218.979953	34.738868
1041.706476	106405.466187	34.743885
1042.902236	106588.882583	34.748903
1043.475998	106794.808860	34.753920
1044.607290	106980.949088	34.758938
1045.470814	107179.585536	34.763956
1046.335367	107382.124435	34.768973
1047.770996	107575.260814	34.773991
1048.686470	107785.140712	34.779008
1049.829752	107986.067465	34.784026
1051.014993	108183.758836	34.789044
1052.139096	108386.819712	34.794061
1053.339334	108591.820190	34.799079
1054.298843	108792.073997	34.804096
1054.913348	108986.724252	34.809114
1056.315593	109193.266572	34.814132
1057.238437	109399.205705	34.819149
1058.701941	109591.743876	34.824167
1059.671084	109799.198434	34.829184
1060.854241	110004.744427	34.834202
1061.658188	110209.885968	34.839220
1062.953586	110416.759248	34.844237
1063.869976	110613.930045	34.849255
1065.055436	110830.882689	34.854272
1066.241291	111022.298747	34.859290
1067.245511	111223.538423	34.864308
1068.179634	111425.095189	34.869325
1069.856922	111619.297110	34.874343
1070.516063	111834.520479	34.879360
1071.695014	112031.734029	34.884378
1072.830075	112231.515242	34.889396
1073.574420	112433.680810	34.894413
1075.117566	112636.095842	34.899431
1075.972161	112833.546076	34.904448
1076.991908	113044.500567	34.909466
1078.471744	113251.668634	34.914484
1079.089302	113441.143018	34.919501
1080.713612	113635.887226	34.924519
1081.576858	113846.518915	34.929536
1082.488054	114040.674367	34.934554
1083.593224	114238.536516	34.939572
1084.825773	114445.450235	34.944589
1086.133482	114635.350694	34.949607
1086.577260	114847.706252	34.954624
1087.974391	115043.524005	34.959642
1089.391287	115249.614960	34.964660
1090.123866	115447.597865	34.969677
1091.313097	115637.182558	34.974695
1092.311706	115835.960401	34.979712
1092.976007	116028.611926	34.984730
1094.116113	116213.546011	34.989748
1094.964754	116413.214245	34.994765
1096.283690	116604.456403	34.999783
1097.217957	116802.960209	35.004800
1098.209135	117006.562179	35.009818
1099.485927	117207.216820	35.014836
1099.915296	117411.548069	35.019853
1101.506566	117620.833002	35.024871
1102.586233	117831.800560	35.029888
1103.591573	118039.360800	35.034906
1104.970489	118242.641326	35.039924
1106.129188	118454.677403	35.044941
1107.289978	118656.336981	35.049959
1108.196136	118882.292892	35.054976
1109.298805	119087.779132	35.059994
1110.391204	119299.528227	35.065012
1111.314889	119514.930818	35.070029
1112.619814	119724.658428	35.075047
1113.653648	119954.238304	35.080064
1114.705576	120173.831570	35.085082
1116.252130	120386.425829	35.090100
1117.382481	120607.606039	35.095117
1118.443428	120806.673852	35.100135
1119.393024	121032.094276	35.105152
1120.549477	121253.008897	35.110170
1121.973267	121466.873133	35.115188
1123.183010	121698.972010	35.120205
1124.137508	121911.155555	35.125223
1125.527950	122118.858454	35.130240
1126.418815	122340.319312	35.135258
1127.960043	122550.737617	35.140276
1128.555613	122771.147950	35.145293
1130.077592	122992.547334	35.150311
1131.262089	123215.486903	35.155328
1132.369719	123431.546594	35.160346
1133.651608	123652.787769	35.165364
1134.335418	123872.215753	35.170381
1136.089391	124095.359193	35.175399
1137.556145	124316.916868	35.180416
1138.078267	124525.553065	35.185434
1139.753792	124741.287456	35.190452
1140.803047	124958.242211	35.195469
1141.854273	125163.956381	35.200487
1142.796209	125387.661814	35.205504
1144.089256	125607.470578	35.210522
1145.235563	125824.960448	35.215540
1146.401052	126044.704723	35.220557
1147.545147	126268.623995	35.225575
1148.639030	126493.744604	35.230592
1149.799965	126709.032958	35.235610
1151.374583	126912.340226	35.240628
1152.540728	127133.815933	35.245645
1153.390365	127350.820621	35.250663
1154.878155	127564.692025	35.255680
1156.164231	127774.998538	35.260698
1157.116166	127991.889401	35.265716
1157.814902	128199.481999	35.270733
1159.901380	128419.369771	35.275751
1160.766156	128632.451560	35.280768
1161.862010	128839.729261	35.285786
1162.883938	129050.975328	35.290804
1164.040847	129266.117278	35.295821
1165.229938	129469.200765	35.300839
1166.517176	129694.261870	35.305856
1167.725468	129903.847680	35.310874
1168.654824	130098.472629	35.315892
1169.716913	130305.220498	35.320909
1171.008787	130511.919055	35.325927
1172.002787	130702.962361	35.330944
1172.954028	130917.617152	35.335962
1174.206065	131109.976613	35.340980
1175.113648	131324.730099	35.345997
1176.126338	131526.436162	35.351015
1177.598038	131742.797864	35.356032
1178.205012	131971.486296	35.361050
1179.623829	132176.640771	35.366068
1180.577774	132410.561199	35.371085
1181.747208	132623.403914	35.376103
1183.035710	132838.827149	35.381120
1184.150177	133075.248596	35.386138
1185.187225	133294.342095	35.391156
1186.266275	133532.103838	35.396173
1187.608890	133763.713234	35.401191
1188.815931	133985.420197	35.406208
1189.983366	134230.297188	35.411226
1191.374925	134463.196576	35.416244
1192.632404	134701.266964	35.421261
1194.063900	134934.556112	35.426279
1194.982860	135159.247230	35.431296
1196.122274	135399.928498	35.436314
1197.507460	135633.179537	35.441332
1198.601202	135872.350419	35.446349
1199.675431	136113.719603	35.451367
1200.873057	136351.051086	35.456384
1201.767604	136591.603987	35.461402
1203.406605	136831.097353	35.466420
1204.705522	137085.799692	35.471437
1205.949393	137311.022206	35.476455
1206.896481	137557.456327	35.481472
1208.051692	137797.315506	35.486490
1209.591079	138046.596828	35.491508
1210.789146	138286.439726	35.496525
1211.780321	138534.382521	35.501543
1213.558004	138780.739003	35.506560
1214.214712	139025.558161	35.511578
1215.720623	139269.528659	35.516596
1216.706177	139525.962215	35.521613
1217.882308	139772.311188	35.526631
1219.361296	140017.863767	35.531648
1220.389729	140265.825675	35.536666
1221.729490	140514.612831	35.541684
1222.939518	140762.028420	35.546701
1224.433019	141015.865808	35.551719
1225.578306	141255.078885	35.556736
1226.869306	141510.119951	35.561754
1228.063102	141753.284710	35.566772
1229.583096	142007.137653	35.571789
1231.201269	142248.143435	35.576807
1232.006704	142490.299671	35.581824
1233.175827	142745.534762	35.586842
1234.658967	142976.841713	35.591860
1235.762988	143223.290509	35.596877
1237.295154	143463.240969	35.601895
1238.597045	143702.584382	35.606912
1239.595919	143945.111760	35.611930
1240.917373	144185.127303	35.616948
1242.022952	144438.203938	35.621965
1242.984006	144679.119353	35.626983
1244.552617	144926.213348	35.632000
1245.619992	145183.245544	35.637018
1247.138327	145419.571843	35.642036
1248.401894	145666.518450	35.647053
1249.611080	145906.640185	35.652071
1250.798567	146131.383842	35.657088
1251.888500	146367.482793	35.662106
1253.295855	146593.423139	35.667124
1254.273087	146821.832924	35.672141
1255.460950	147057.070461	35.677159
1256.912438	147282.462450	35.682176
1257.813684	147519.931713	35.687194
1258.877640	147769.931357	35.692212
1260.149578	148014.153087	35.697229
1261.136431	148259.387444	35.702247
1262.327956	148500.328177	35.707264
1263.623621	148760.138107	35.712282
1264.832624	149018.810029	35.717300
1265.821421	149270.950314	35.722317
1267.159391	149541.577383	35.727335
1268.137710	149797.971825	35.732352
1269.270347	150063.322326	35.737370
1270.722380	150331.640573	35.742388
1271.932669	150594.001382	35.747405
1272.760343	150873.689656	35.752423
1274.285570	151142.585024	35.757440
1276.090727	151424.627189	35.762458
1277.194773	151700.699057	35.767476
1278.576681	151971.678775	35.772493
1279.668964	152244.877261	35.777511
1281.400002	152510.945099	35.782528
1282.309028	152804.840371	35.787546
1283.719768	153081.137873	35.792564
1285.053795	153359.606387	35.797581
1286.330608	153633.355031	35.802599
1287.746997	153913.044311	35.807616
1289.011869	154195.081947	35.812634
1290.565006	154467.788703	35.817652
1292.013549	154744.497704	35.822669
1293.336460	155028.599397	35.827687
1294.639877	155305.260226	35.832704
1295.908315	155583.235350	35.837722
1297.526877	155862.017160	35.842740
1298.588056	156129.666525	35.847757
1299.946546	156404.347022	35.852775
1301.230886	156681.883222	35.857792
1302.123391	156972.095599	35.862810
1303.841022	157241.610198	35.867828
1305.375462	157530.236292	35.872845
1306.248144	157817.502262	35.877863
1308.055586	158095.925902	35.882880
1308.942331	158372.397736	35.887898
1310.428988	158649.216318	35.892916
1311.744123	158924.555468	35.897933
1312.954562	159219.653667	35.902951
1314.491790	159498.258412	35.907968
1315.747459	159775.325770	35.912986
1317.143221	160055.378552	35.918004
1318.681767	160335.993221	35.923021
1319.959059	160615.752208	35.928039
1321.377295	160888.816517	35.933056
1322.674411	161172.407389	35.938074
1323.845490	161451.390261	35.943092
1325.365071	161729.188245	35.948109
1326.462050	162020.189116	35.953127
1327.876713	162297.120084	35.958144
1329.189955	162589.116801	35.963162
1330.362797	162868.565498	35.968180
1332.101246	163148.556931	35.973197
1332.910769	163434.831821	35.978215
1334.327795	163709.525889	35.983232
1335.781576	163986.816627	35.988250
1336.648168	164267.505028	35.993268
1338.472905	164544.814177	35.998285
1339.467136	164825.015647	36.003303
1340.737351	165090.353647	36.008320
1342.175466	165357.403791	36.013338
1343.163329	165629.656019	36.018356
1344.654937	165907.193842	36.023373
1345.545101	166196.138166	36.028391
1346.697722	166466.414335	36.033408
1348.203085	166770.106255	36.038426
1349.741268	167057.248845	36.043444
1351.122221	167335.016933	36.048461
1352.099914	167628.765140	36.053479
1353.699447	167918.821556	36.058496
1355.106338	168218.352269	36.063514
1356.231929	168513.629871	36.068532
1357.818964	168804.569596	36.073549
1358.794723	169106.588372	36.078567
1360.351509	169408.398927	36.083584
1362.099393	169708.124217	36.088602
1363.144343	169998.755081	36.093620
1364.192014	170306.898900	36.098637
1365.481480	170621.095840	36.103655
1367.200912	170925.846156	36.108672
1368.542049	171231.929966	36.113690
1369.783930	171556.635554	36.118708
1371.179338	171852.994011	36.123725
1372.486706	172167.337993	36.128743
1374.257484	172484.691193	36.133760
1375.610403	172791.595383	36.138778
1376.980779	173107.280358	36.143796
1378.351644	173419.109465	36.148813
1379.978210	173738.715677	36.153831
1381.311717	174052.166764	36.158848
1382.616869	174368.568801	36.163866
1383.625850	174682.267963	36.168884
1385.369762	174997.129473	36.173901
1386.740479	175323.819134	36.178919
1388.245176	175632.391519	36.183936
1389.580892	175955.360027	36.188954
1390.699132	176285.727442	36.193972
1392.054697	176609.610705	36.198989
1393.577065	176937.923158	36.204007
1394.875570	177262.403893	36.209024
1396.478992	177581.150566	36.214042
1397.918107	177919.826748	36.219060
1399.766390	178238.575189	36.224077
1400.710850	178559.264517	36.229095
1402.469476	178891.586610	36.234112
1403.664729	179210.233281	36.239130
1405.238743	179535.419151	36.244148
1406.843777	179849.813725	36.249165
1408.121295	180177.540267	36.254183
1409.638875	180500.710787	36.259200
1411.177245	180814.677985	36.264218
1412.264733	181143.190831	36.269236
1414.371614	181455.303680	36.274253
1415.660340	181782.759169	36.279271
1417.190343	182093.904938	36.284288
1418.262794	182407.082796	36.289306
1419.720993	182725.009282	36.294324
1421.484508	183038.343180	36.299341
1422.581644	183363.060273	36.304359
1424.301153	183678.715254	36.309376
1425.610437	183991.850477	36.314394
1427.154242	184320.967414	36.319412
1428.589874	184621.341499	36.324429
1429.750547	184954.295401	36.329447
1431.136286	185259.783880	36.334464
1432.686978	185580.047253	36.339482
1434.176663	185894.826282	36.344500
1435.894803	186183.738025	36.349517
1437.050084	186479.040270	36.354535
1438.651718	186782.127669	36.359552
1439.801781	187079.096770	36.364570
1441.114231	187381.105401	36.369588
1442.927808	187678.298017	36.374605
1444.033794	187991.844602	36.379623
1445.433880	188300.419027	36.384640
1447.234858	188602.670685	36.389658
1447.918259	188923.311935	36.394676
1449.548546	189239.266657	36.399693
1451.279981	189552.667513	36.404711
1452.340747	189862.613745	36.409728
1453.861550	190189.432588	36.414746
1454.940096	190515.577323	36.419764
1456.384524	190839.251418	36.424781
1457.738529	191178.226486	36.429799
1458.892454	191512.057087	36.434816
1460.375372	191846.000192	36.439834
1461.729836	192200.747745	36.444852
1463.256354	192533.824146	36.449869
1464.495448	192881.688669	36.454887
1465.930823	193237.609436	36.459904
1467.695714	193583.270932	36.464922
1468.873325	193951.603370	36.469940
1470.693404	194295.863192	36.474957
1472.107202	194656.505480	36.479975
1473.802500	195005.334678	36.484992
1475.437902	195349.630700	36.490010
1476.578966	195700.446862	36.495028
1478.207764	196056.808476	36.500045
1479.780396	196404.992622	36.505063
1481.006906	196764.877777	36.510080
1482.756496	197119.168495	36.515098
1484.296361	197490.774817	36.520116
1485.682866	197840.939734	36.525133
1487.637986	198197.512873	36.530151
1488.722270	198568.375189	36.535168
1490.557072	198916.783033	36.540186
1491.765979	199278.170004	36.545204
1493.518208	199646.566312	36.550221
1495.099997	200003.464476	36.555239
1496.628619	200366.010450	36.560256
1498.305523	200729.244802	36.565274
1499.551719	201095.078794	36.570292
1501.136805	201451.894889	36.575309
1502.741634	201817.660642	36.580327
1503.841219	202173.659083	36.585344
1505.904210	202531.011016	36.590362
1507.311705	202896.852919	36.595380
1509.056259	203253.080192	36.600397
1510.711712	203619.557658	36.605415
1512.134630	203976.006612	36.610432
1513.616889	204324.308631	36.615450
1515.258370	204694.298071	36.620468
1516.857802	205035.765647	36.625485
1518.560410	205395.565248	36.630503
1519.626895	205751.167242	36.635520
1521.241282	206103.442519	36.640538
1522.508715	206461.503256	36.645556
1524.068537	206823.948748	36.650573
1525.821958	207167.381082	36.655591
1527.150725	207545.727294	36.660608
1529.025950	207893.713775	36.665626
1530.276087	208251.963209	36.670644
1531.596782	208596.260410	36.675661
1533.442579	208950.402011	36.680679
1534.836426	209294.690060	36.685696
1536.578514	209626.287563	36.690714
1537.758607	209976.226237	36.695732
1539.295598	210312.571296	36.700749
1540.558883	210666.918009	36.705767
1542.131605	211013.367622	36.710784
1543.741598	211362.860041	36.715802
1544.951542	211733.854603	36.720820
1546.134256	212085.045897	36.725837
1548.155353	212438.766738	36.730855
1548.876795	212803.268779	36.735872
1551.059425	213169.537260	36.740890
1552.024774	213547.487789	36.745908
1553.807237	213921.063580	36.750925
1555.363254	214302.729227	36.755943
1556.485784	214680.607676	36.760960
1558.196113	215055.342858	36.765978
1559.749764	215443.286740	36.770996
1560.940295	215838.327346	36.776013
1562.505592	216226.018520	36.781031
1564.025900	216611.255095	36.786048
1566.191158	217015.003336	36.791066
1567.778685	217426.950659	36.796084
1569.013410	217816.531409	36.801101
1570.789850	218215.904098	36.806119
1571.993371	218614.534867	36.811136
1573.822793	219011.641476	36.816154
1575.382036	219426.598629	36.821172
1577.303402	219837.027446	36.826189
1579.005189	220229.283238	36.831207
1580.032098	220636.510285	36.836224
1581.882655	221051.679665	36.841242
1583.645177	221458.508891	36.846260
1584.937243	221872.071912	36.851277
1587.092710	222281.607754	36.856295
1588.403893	222689.963801	36.861312
1590.167527	223096.443209	36.866330
1591.894990	223509.584695	36.871348
1593.286065	223913.563171	36.876365
1595.154062	224327.954305	36.881383
1596.421313	224737.874167	36.886400
1598.267470	225136.117461	36.891418
1599.991571	225620.208568	36.896436
1601.422808	226050.324087	36.901453
1603.527872	226453.507252	36.906471
1604.877215	226876.222280	36.911488
1606.859139	227274.272135	36.916506
1608.287970	227685.978358	36.921524
1609.796369	228096.174093	36.926541
1611.990625	228506.308584	36.931559
1613.456094	228906.099669	36.936576
1614.828076	229312.994139	36.941594
1616.759405	229724.547329	36.946612
1618.368313	230124.750021	36.951629
1620.024846	230527.917862	36.956647
1621.629340	230949.942911	36.961664
1623.202277	231346.293958	36.966682
1624.547413	231752.564700	36.971700
1625.967780	232171.778681	36.976717
1628.187421	232580.421867	36.981735
1629.514873	232988.324453	36.986752
1631.452920	233388.303605	36.991770
1632.906020	233811.148908	36.996788
1634.432176	234216.989647	37.001805
1636.255165	234627.329206	37.006823
1637.561018	235045.680474	37.011840
1639.142802	235451.032328	37.016858
1640.941684	235832.852674	37.021876
1642.396014	236239.675273	37.026893
1644.061444	236628.962057	37.031911
1645.630783	237025.911489	37.036928
1647.405867	237417.671176	37.041946
1648.804267	237816.962061	37.046964
1649.933036	238212.360981	37.051981
1652.012543	238614.233572	37.056999
1653.114936	239030.493545	37.062016
1654.666386	239434.334714	37.067034
1656.423856	239848.481319	37.072052
1657.935562	240269.324699	37.077069
1659.910699	240686.358182	37.082087
1661.220292	241113.079053	37.087104
1662.867663	241535.502705	37.092122
1664.574480	241967.112968	37.097140
1666.194858	242394.318233	37.102157
1667.991353	242823.451124	37.107175
1669.085619	243265.706841	37.112192
1670.868634	243690.829766	37.117210
1672.911282	244140.246211	37.122228
1674.357277	244587.983736	37.127245
1676.137612	245028.909592	37.132263
1677.611625	245483.934425	37.137280
1679.303595	245930.109143	37.142298
1680.996499	246391.221196	37.147316
1682.829279	246842.683088	37.152333
1684.551647	247287.279612	37.157351
1686.009182	247750.591590	37.162368
1687.926976	248210.373307	37.167386
1689.473289	248675.703969	37.172404
1691.039247	249135.875095	37.177421
1693.055671	249587.030428	37.182439
1694.809940	250055.783040	37.187456
1696.486650	250525.158594	37.192474
1698.339999	250990.720339	37.197492
1700.002935	251453.011529	37.202509
1702.146670	251913.928114	37.207527
1704.034544	252386.471160	37.212544
1705.463209	252837.319847	37.217562
1707.233356	253303.074911	37.222580
1708.685752	253759.051687	37.227597
1710.174562	254223.481974	37.232615
1712.205381	254700.651612	37.237632
1713.879132	255170.081639	37.242650
1715.641860	255643.714097	37.247668
1717.209335	256117.505982	37.252685
1719.313569	256580.031896	37.257703
1720.477207	257057.548798	37.262720
1722.052257	257535.582108	37.267738
1724.238881	258016.588262	37.272756
1725.864086	258500.329120	37.277773
1728.129713	258964.124224	37.282791
1729.698911	259445.461000	37.287808
1731.340542	259918.656707	37.292826
1733.177264	260398.577394	37.297844
1734.851600	260865.086458	37.302861
1736.691681	261346.276525	37.307879
1738.605833	261828.698960	37.312896
1739.892308	262289.936946	37.317914
1741.888425	262774.657150	37.322932
1743.534043	263253.058790	37.327949
1745.371569	263729.599439	37.332967
1746.764901	264198.566799	37.337984
1748.829246	264679.032289	37.343002
1750.539731	265157.142576	37.348020
1752.167449	265640.067359	37.353037
1754.231163	266108.338334	37.358055
1755.891897	266561.814643	37.363072
1757.417209	267020.368130	37.368090
1759.553096	267465.204300	37.373108
1760.818779	267935.180345	37.378125
1762.545904	268382.572610	37.383143
1764.462066	268852.897464	37.388160
1766.017132	269310.376703	37.393178
1767.799911	269772.263293	37.398196
1769.645227	270244.858986	37.403213
1771.413432	270704.943172	37.408231
1773.050720	271166.648728	37.413248
1774.358027	271645.910636	37.418266
1776.507041	272121.603427	37.423284
1778.322537	272612.261930	37.428301
1779.920074	273082.887509	37.433319
1781.798024	273565.201994	37.438336
1783.262536	274055.687322	37.443354
1785.148673	274541.707471	37.448372
1786.627621	275035.262268	37.453389
1788.400823	275530.088412	37.458407
1790.342231	276031.871407	37.463424
1792.304448	276534.005522	37.468442
1794.502115	277030.003105	37.473460
1796.378333	277525.951054	37.478477
1797.947223	278019.941848	37.483495
1800.052217	278526.721792	37.488512
1801.719303	279028.670213	37.493530
1803.626436	279526.615027	37.498548
1804.963321	280048.352690	37.503565
1806.972405	280549.402451	37.508583
1809.030195	281060.247886	37.513600
1810.568148	281559.670780	37.518618
1812.354912	282070.304085	37.523636
1814.264570	282588.434441	37.528653
1815.914106	283111.788068	37.533671
1818.021702	283626.859766	37.538688
1819.520779	284145.688113	37.543706
1821.619224	284653.188468	37.548724
1823.135876	285195.150949	37.553741
1825.299347	285715.540844	37.558759
1826.983581	286235.830274	37.563776
1828.930080	286767.428732	37.568794
1830.674070	287286.536117	37.573812
1832.206117	287828.232380	37.578829
1834.320300	288348.747955	37.583847
1836.364750	288882.659106	37.588864
1837.908016	289418.708334	37.593882
1840.088737	289947.868258	37.598900
1842.027531	290481.434806	37.603917
1843.726526	291016.816732	37.608935
1845.486186	291538.038605	37.613952
1847.421935	292082.749434	37.618970
1849.427932	292607.177268	37.623988
1851.037727	293151.149720	37.629005
1853.117593	293680.005556	37.634023
1854.971189	294216.439959	37.639040
1856.650423	294765.168474	37.644058
1858.716694	295291.250598	37.649076
1860.541001	295841.905613	37.654093
1862.435869	296370.677790	37.659111
1864.338497	296896.804629	37.664128
1865.956870	297449.796739	37.669146
1868.167847	297979.321485	37.674164
1869.999998	298521.478260	37.679181
1871.590308	299052.547681	37.684199
1873.611254	299590.680053	37.689216
1875.670319	300134.568551	37.694234
1877.913344	300666.054936	37.699252
1879.521563	301184.411055	37.704269
1881.192748	301693.966430	37.709287
1883.153600	302200.347351	37.714304
1884.429450	302719.689652	37.719322
1886.703449	303230.838731	37.724340
1888.629004	303755.579068	37.729357
1890.126824	304274.063182	37.734375
1892.175764	304792.021540	37.739392
1893.766658	305317.823827	37.744410
1895.655756	305849.567248	37.749428
1897.278600	306389.249577	37.754445
1899.083856	306932.326838	37.759463
1900.913000	307467.193796	37.764480
1902.764178	308010.815206	37.769498
1904.668626	308568.214017	37.774516
1906.313495	309120.471232	37.779533
1908.057648	309684.694804	37.784551
1910.295245	310234.459339	37.789568
1911.904035	310814.188190	37.794586
1913.937643	311377.945554	37.799604
1915.619733	311948.359406	37.804621
1917.521960	312521.627600	37.809639
1919.917823	313100.726757	37.814656
1921.624094	313688.746967	37.819674
1923.939602	314261.044813	37.824692
1925.708343	314841.452804	37.829709
1927.906392	315410.967738	37.834727
1929.917758	315996.252672	37.839744
1931.516674	316579.544069	37.844762
1933.993640	317155.931210	37.849780
1935.638663	317746.442172	37.854797
1937.546214	318325.478241	37.859815
1939.809417	318908.665747	37.864832
1941.688320	319503.972765	37.869850
1943.674818	320078.892714	37.874868
1945.568200	320688.812285	37.879885
1947.203754	321281.959875	37.884903
1948.925937	321872.447107	37.889920
1950.672989	322481.079110	37.894938
1952.974627	323086.770022	37.899956
1955.233120	323688.628350	37.904973
1956.659502	324296.051720	37.909991
1959.039271	324890.185298	37.915008
1960.355885	325517.266359	37.920026
1962.754369	326122.962435	37.925044
1964.663744	326741.275288	37.930061
1966.533084	327357.151060	37.935079
1968.640228	327970.696224	37.940096
1970.478556	328592.657428	37.945114
1972.590221	329209.616245	37.950132
1974.675908	329829.111513	37.955149
1976.373323	330463.744201	37.960167
1978.856775	331078.158934	37.965184
1980.281722	331713.152607	37.970202
1982.436672	332325.373870	37.975220
1984.676680	332949.023447	37.980237
1986.688829	333584.888739	37.985255
1989.010005	334203.204958	37.990272
1990.682267	334825.200540	37.995290
1992.878095	335437.075402	38.000308
1995.124052	336068.201868	38.005325
1996.403292	336686.585133	38.010343
1998.852505	337304.412538	38.015360
2000.654877	337935.513516	38.020378
2002.581169	338564.682530	38.025396
2004.863040	339192.008258	38.030413
2006.647118	339819.078414	38.035431
2008.299491	340428.953171	38.040448
2010.315502	341050.207779	38.045466
2012.390377	341646.646808	38.050484
2014.862716	342257.404296	38.055501
2016.412080	342871.936018	38.060519
2018.432451	343464.173898	38.065536
2020.085922	344084.002967	38.070554
2021.947795	344691.277118	38.075572
2024.152048	345309.019616	38.080589
2025.791599	345938.674103	38.085607
2028.026826	346560.278056	38.090624
2029.308633	347198.400450	38.095642
2031.536049	347832.982537	38.100660
2033.657386	348472.953490	38.105677
2035.391816	349128.967303	38.110695
2037.327868	349765.296136	38.115712
2039.102368	350434.378999	38.120730
2041.232136	351083.726195	38.125748
2042.986653	351756.370466	38.130765
2045.029755	352429.515021	38.135783
2047.684239	353091.205354	38.140800
2049.464001	353774.015162	38.145818
2051.130850	354450.818914	38.150836
2053.339718	355127.877651	38.155853
2055.348953	355819.243985	38.160871
2057.638530	356512.506390	38.165888
2059.773241	357202.382820	38.170906
2061.909551	357890.293774	38.175924
2064.265906	358580.085153	38.180941
2066.023142	359271.308460	38.185959
2068.830910	359967.268573	38.190976
2070.671675	360664.771661	38.195994
2073.038837	361346.826542	38.201012
2074.971536	362033.837818	38.206029
2076.800934	362742.646610	38.211047
2079.296537	363429.870323	38.216064
2081.352119	364124.232368	38.221082
2082.927313	364828.326501	38.226100
2085.529495	365526.403594	38.231117
2087.364768	366239.307491	38.236135
2089.605584	366955.225753	38.241152
2091.255417	367667.930315	38.246170
2093.357524	368372.125168	38.251188
2096.062504	369085.237181	38.256205
2098.034317	369807.283373	38.261223
2099.739380	370509.245455	38.266240
2101.741724	371236.001466	38.271258
2103.669492	371959.102856	38.276276
2106.098892	372686.925810	38.281293
2108.205605	373413.189358	38.286311
2110.342021	374133.752089	38.291328
2112.593959	374868.889081	38.296346
2114.845449	375589.986240	38.301364
2117.054248	376313.636874	38.306381
2119.077682	377047.548251	38.311399
2121.424190	377764.501461	38.316416
2123.959855	378492.312573	38.321434
2125.470813	379211.959792	38.326452
2127.822135	379940.454847	38.331469
2129.900115	380660.966403	38.336487
2132.029900	381387.285798	38.341504
2134.505326	382115.890306	38.346522
2136.433475	382845.811436	38.351540
2138.553519	383562.500179	38.356557
2140.883284	384302.210776	38.361575
2142.824976	385018.871440	38.366592
2144.787082	385747.301906	38.371610
2147.081240	386471.984875	38.376628
2149.339581	387207.457115	38.381645
2151.350173	387902.162998	38.386663
2153.404469	388600.015156	38.391680
2155.786310	389315.441358	38.396698
2157.530434	390012.527255	38.401716
2160.176665	390712.034138	38.406733
2162.001428	391410.722816	38.411751
2164.224418	392116.376505	38.416768
2166.287383	392825.081916	38.421786
2168.555778	393543.976863	38.426804
2170.528937	394244.882369	38.431821
2172.392004	394974.480655	38.436839
2174.504391	395691.727708	38.441856
2176.744578	396413.751704	38.446874
2178.546624	397139.961333	38.451892
2180.480232	397879.056151	38.456909
2182.707501	398628.651495	38.461927
2185.043305	399371.747451	38.466944
2187.248432	400118.165503	38.471962
2189.296837	400878.755228	38.476980
2191.200477	401633.292422	38.481997
2193.243174	402406.106653	38.487015
2195.506301	403158.846163	38.492032
2197.834605	403931.926129	38.497050
2199.871339	404702.144431	38.502068
2202.111895	405482.796905	38.507085
2204.466464	406265.156659	38.512103
2206.057121	407051.977800	38.517120
2208.797558	407829.567654	38.522138
2210.999543	408631.164037	38.527156
2213.325031	409411.690347	38.532173
2215.618688	410208.183595	38.537191
2218.236714	410999.482757	38.542208
2220.309079	411801.411160	38.547226
2222.440873	412596.998451	38.552244
2224.796158	413386.445955	38.557261
2226.658500	414188.311063	38.562279
2229.075182	414995.100127	38.567296
2231.492959	415804.016657	38.572314
2233.517729	416621.254142	38.577332
2236.101505	417419.253186	38.582349
2238.084990	418230.697407	38.587367
2240.327859	419039.034134	38.592384
2242.539841	419857.048555	38.597402
2245.030475	420671.318768	38.602420
2247.459944	421479.799467	38.607437
2249.947652	422301.638485	38.612455
2252.189626	423121.921012	38.617472
2254.735996	423926.884476	38.622490
2256.810956	424745.621297	38.627508
2258.978605	425555.100158	38.632525
2261.493031	426376.494401	38.637543
2263.938187	427187.796876	38.642560
2265.888208	428004.874625	38.647578
2268.385159	428819.404156	38.652596
2270.655384	429626.248336	38.657613
2273.108088	430443.361932	38.662631
2274.826935	431259.150936	38.667648
2277.678319	432082.266917	38.672666
2279.729675	432909.788374	38.677684
2282.183986	433708.160581	38.682701
2284.556599	434538.051063	38.687719
2286.877417	435351.724371	38.692736
2289.503030	436156.208662	38.697754
2291.542435	436966.480053	38.702772
2293.783196	437776.638688	38.707789
2296.329195	438594.662838	38.712807
2298.227535	439412.966526	38.717824
2300.770878	440209.679042	38.722842
2303.072493	440998.964881	38.727860
2305.385868	441776.482098	38.732877
2307.604231	442551.002486	38.737895
2309.406837	443341.653065	38.742912
2312.024964	444120.251398	38.747930
2313.689447	444920.935457	38.752948
2316.012101	445714.044899	38.757965
2318.359108	446515.366821	38.762983
2320.402245	447306.642724	38.768000
2323.063960	448105.829991	38.773018
2325.134656	448934.320543	38.778036
2327.661415	449743.787066	38.783053
2329.732992	450554.966763	38.788071
2331.920740	451385.263936	38.793088
2334.109834	452204.199691	38.798106
2336.311008	453044.846812	38.803124
2338.696843	453877.692439	38.808141
2341.013512	454716.078311	38.813159
2343.094188	455558.059111	38.818176
2345.217670	456403.992745	38.823194
2347.671972	457265.611634	38.828212
2349.808227	458127.094825	38.833229
2352.414939	458998.979415	38.838247
2354.727827	459865.566608	38.843264
2357.284358	460730.559623	38.848282
2359.109458	461608.879874	38.853300
2361.572141	462489.684604	38.858317
2364.152052	463373.665698	38.863335
2366.236418	464274.974555	38.868352
2368.743235	465157.725059	38.873370
2370.959501	466062.366650	38.878388
2373.444136	466955.248131	38.883405
2376.004109	467861.720052	38.888423
2377.972784	468765.012942	38.893440
2380.808017	469662.006380	38.898458
2382.670943	470579.530779	38.903476
2385.117536	471509.697166	38.908493
2387.381982	472440.504716	38.913511
2389.967023	473373.840411	38.918528
2392.358273	474289.531496	38.923546
2395.002927	475221.704454	38.928564
2397.339856	476142.819526	38.933581
2400.075102	477076.904863	38.938599
2402.172523	478007.613727	38.943616
2404.838926	478930.454500	38.948634
2406.997139	479870.654431	38.953652
2409.973259	480806.832989	38.958669
2412.236175	481748.433440	38.963687
2414.322351	482677.895575	38.968704
2417.032000	483614.426941	38.973722
2419.331658	484561.579414	38.978740
2421.912983	485501.718603	38.983757
2424.491816	486440.697778	38.988775
2426.529161	487383.451911	38.993792
2429.382354	488315.420721	38.998810
2431.727412	489269.733512	39.003828
2434.022097	490208.659023	39.008845
2436.474176	491168.654321	39.013863
2439.036854	492116.062501	39.018880
2441.222413	493062.067828	39.023898
2443.525795	494027.428875	39.028916
2446.157836	494968.713738	39.033933
2448.707823	495926.105637	39.038951
2450.882298	496881.890926	39.043968
2453.766776	497837.555386	39.048986
2456.182011	498787.441580	39.054004
2458.345689	499746.193409	39.059021
2461.453734	500676.487558	39.064039
2463.203393	501615.578534	39.069056
2466.100940	502533.899783	39.074074
2468.037515	503461.406146	39.079092
2470.230231	504392.196577	39.084109
2472.883442	505304.855793	39.089127
2475.212768	506236.526954	39.094144
2477.632031	507172.213815	39.099162
2480.035740	508121.663478	39.104180
2482.327220	509057.614901	39.109197
2484.986880	510005.096033	39.114215
2487.037207	510955.847610	39.119232
2489.541114	511910.348753	39.124250
2491.744064	512880.315628	39.129268
2494.386815	513854.535069	39.134285
2497.034887	514813.977486	39.139303
2498.761970	515805.764713	39.144320
2501.581144	516786.424449	39.149338
2504.064671	517776.953438	39.154356
2506.597221	518778.142601	39.159373
2509.193745	519770.741875	39.164391
2511.748308	520767.565906	39.169408
2514.249708	521784.936528	39.174426
2516.754681	522787.580807	39.179444
2519.349790	523788.481802	39.184461
2521.894801	524806.095814	39.189479
2523.834684	525829.935115	39.194496
2526.698454	526840.257871	39.199514
2529.186418	527882.347147	39.204532
2531.825355	528916.534252	39.209549
2534.439655	529947.481363	39.214567
2536.870561	530990.418547	39.219584
2539.334145	532028.141698	39.224602
2542.050604	533070.581730	39.229620
2544.589699	534124.452105	39.234637
2547.243977	535175.106603	39.239655
2549.602771	536224.676664	39.244672
2552.597487	537281.462480	39.249690
2554.923521	538332.393617	39.254708
2557.352799	539388.966143	39.259725
2560.189717	540440.663858	39.264743
2562.618939	541509.957855	39.269760
2565.184332	542569.037679	39.274778
2568.193465	543640.840903	39.279796
2570.509878	544704.226908	39.284813
2573.124847	545764.917802	39.289831
2575.762065	546851.120017	39.294848
2578.534381	547920.822540	39.299866
2581.326348	548983.852303	39.304884
2583.858380	550068.159262	39.309901
2586.758175	551131.809075	39.314919
2589.144903	552205.714997	39.319936
2591.609584	553279.221553	39.324954
2594.547124	554356.284087	39.329972
2597.181520	555441.803626	39.334989
2599.781625	556501.261278	39.340007
2602.155723	557577.203542	39.345024
2604.833457	558653.059074	39.350042
2607.338942	559724.384548	39.355060
2609.957817	560810.674944	39.360077
2612.816916	561891.059614	39.365095
2615.068895	562967.035547	39.370112
2617.790831	564047.013872	39.375130
2620.664199	565137.172386	39.380148
2623.102831	566219.377223	39.385165
2626.179430	567295.310868	39.390183
2628.365074	568382.397005	39.395200
2631.058481	569460.672699	39.400218
2634.086079	570523.140856	39.405236
2636.453627	571578.451681	39.410253
2639.043892	572623.148596	39.415271
2641.312199	573667.862522	39.420288
2643.950671	574714.887659	39.425306
2646.732865	575758.038594	39.430324
2648.469512	576818.634580	39.435341
2651.434867	577874.422644	39.440359
2653.934934	578949.611025	39.445376
2656.143561	580023.750961	39.450394
2658.838889	581090.494867	39.455412
2661.169451	582179.423002	39.460429
2663.919337	583263.371222	39.465447
2666.283578	584365.137145	39.470464
2668.873881	585470.576419	39.475482
2671.514544	586583.777341	39.480500
2673.522278	587698.233260	39.485517
2676.443679	588828.023515	39.490535
2679.108526	589959.152950	39.495552
2681.557513	591093.819071	39.500570
2684.375247	592249.161366	39.505588
2686.593776	593412.957451	39.510605
2689.353643	594558.714564	39.515623
2691.525258	595737.318665	39.520640
2694.433448	596918.437762	39.525658
2697.313528	598093.932946	39.530676
2700.174886	599289.143598	39.535693
2702.871792	600474.343733	39.540711
2705.771962	601669.001882	39.545728
2708.132958	602867.630035	39.550746
2711.003217	604056.237683	39.555764
2713.512514	605271.959691	39.560781
2716.377238	606473.530185	39.565799
2719.212565	607703.852294	39.570816
2721.848013	608915.209802	39.575834
2724.759067	610136.247613	39.580852
2727.124350	611365.796856	39.585869
2729.918511	612594.339801	39.590887
2732.897092	613828.518433	39.595904
2735.928243	615052.899408	39.600922
2738.573931	616293.109298	39.605940
2741.369903	617540.404347	39.610957
2744.254963	618766.196407	39.615975
2746.727437	620004.915435	39.620992
2749.618406	621263.316747	39.626010
2752.636058	622499.062632	39.631028
2755.205323	623753.129727	39.636045
2757.954638	624999.376760	39.641063
2760.792062	626245.564428	39.646080
2763.383225	627513.126521	39.651098
2766.286302	628759.159644	39.656116
2769.081808	630026.338436	39.661133
2772.249685	631283.267314	39.666151
2774.818961	632545.936517	39.671168
2777.939420	633795.283486	39.676186
2780.593244	635042.311941	39.681204
2783.115898	636317.012433	39.686221
2786.159490	637584.184634	39.691239
2788.864572	638846.317596	39.696256
2791.858996	640110.493406	39.701274
2794.834936	641370.176652	39.706292
2797.347540	642630.728940	39.711309
2800.435654	643900.606068	39.716327
2803.191491	645168.284879	39.721344
2805.894971	646431.824785	39.726362
2808.710221	647689.355095	39.731380
2811.365916	648969.185870	39.736397
2814.112262	650231.194367	39.741415
2816.802427	651504.913306	39.746432
2819.308293	652735.198398	39.751450
2821.948599	653965.208991	39.756468
2824.662983	655207.707582	39.761485
2827.626832	656446.073236	39.766503
2830.219715	657679.413179	39.771520
2832.925102	658939.569225	39.776538
2835.940462	660181.835411	39.781556
2838.487826	661446.124203	39.786573
2841.135195	662698.234854	39.791591
2843.896719	663963.801553	39.796608
2846.448181	665240.333848	39.801626
2849.392379	666513.197963	39.806644
2852.124160	667800.106590	39.811661
2854.653375	669091.799277	39.816679
2857.445215	670383.670588	39.821696
2860.051040	671693.547798	39.826714
2862.920388	673011.354089	39.831732
2865.613754	674340.240364	39.836749
2868.394907	675673.546308	39.841767
2871.310234	677006.092579	39.846784
2873.815842	678352.231134	39.851802
2877.004594	679697.663666	39.856820
2879.732870	681063.941145	39.861837
2882.683148	682426.600982	39.866855
2885.445321	683789.784272	39.871872
2888.316642	685167.742752	39.876890
2891.646028	686533.996974	39.881908
2894.318700	687925.471578	39.886925
2896.921132	689300.561844	39.891943
2900.436760	690693.008563	39.896960
2902.890426	692079.062468	39.901978
2905.931785	693476.413689	39.906996
2908.718411	694887.030332	39.912013
2911.794034	696295.539716	39.917031
2914.910702	697701.090260	39.922048
2917.792348	699116.817496	39.927066
2920.919260	700523.005510	39.932084
2924.007076	701938.539705	39.937101
2926.732951	703361.981195	39.942119
2929.983794	704778.562094	39.947136
2932.813917	706200.825987	39.952154
2935.664004	707614.876973	39.957172
2938.637376	709052.396832	39.962189
2941.586383	710471.407638	39.967207
2944.789997	711898.457478	39.972224
2947.627591	713340.177638	39.977242
2950.546503	714762.584706	39.982260
2953.468395	716204.791773	39.987277
2956.580864	717635.786076	39.992295
2959.528585	719070.767510	39.997312
2962.552854	720515.281993	40.002330
2965.690479	721948.005284	40.007348
2968.997795	723382.677593	40.012365
2971.537674	724828.546834	40.017383
2974.490393	726270.189521	40.022400
2977.973220	727712.232488	40.027418
2980.701064	729156.615587	40.032436
2983.943909	730597.990113	40.037453
2986.897754	732041.823095	40.042471
2989.951600	733480.147577	40.047488
2992.878060	734928.505206	40.052506
2996.276636	736368.231076	40.057524
2999.228433	737807.524744	40.062541
3001.997296	739235.387856	40.067559
3004.935894	740676.385375	40.072576
3007.977353	742115.032079	40.077594
3010.991937	743554.062088	40.082612
3013.853058	744982.647513	40.087629
3017.003196	746395.593164	40.092647
3020.089279	747795.872882	40.097664
3022.833377	749186.150317	40.102682
3025.977196	750585.474531	40.107700
3029.017163	751984.809087	40.112717
3031.825338	753382.007031	40.117735
3034.910122	754767.135844	40.122752
3037.655250	756187.274068	40.127770
3040.985750	757582.093684	40.132788
3043.503340	759004.452159	40.137805
3046.357402	760425.307559	40.142823
3049.428223	761851.518212	40.147840
3052.240118	763298.456591	40.152858
3055.003366	764724.616116	40.157876
3058.098374	766189.786130	40.162893
3061.309994	767639.310999	40.167911
3064.292072	769102.894373	40.172928
3066.784122	770579.881903	40.177946
3070.224789	772047.819795	40.182964
3073.181827	773526.941147	40.187981
3075.979598	775016.988287	40.192999
3079.018986	776513.320919	40.198016
3082.705891	778018.370844	40.203034
3085.407023	779524.498544	40.208052
3088.715734	781036.150549	40.213069
3091.863110	782546.580380	40.218087
3095.253143	784051.698922	40.223104
3098.294723	785576.371271	40.228122
3100.976220	787101.120845	40.233140
3104.587848	788623.380858	40.238157
3107.620666	790154.231333	40.243175
3110.920337	791679.561680	40.248192
3113.880245	793212.847892	40.253210
3117.297692	794741.463073	40.258228
3120.312999	796283.423405	40.263245
3123.416919	797837.267242	40.268263
3127.007670	799370.078097	40.273280
3129.821458	800919.853681	40.278298
3133.317340	802471.810991	40.283316
3136.778189	804015.207081	40.288333
3139.527283	805571.331910	40.293351
3142.943654	807118.974847	40.298368
3146.221959	808668.439730	40.303386
3149.341970	810216.208979	40.308404
3152.686694	811771.355418	40.313421
3155.641955	813325.377253	40.318439
3159.157117	814886.370359	40.323456
3162.091990	816444.215048	40.328474
3165.288005	818003.703457	40.333492
3168.851461	819562.229239	40.338509
3171.982768	821107.482704	40.343527
3175.421661	822664.079490	40.348544
3178.294284	824215.379283	40.353562
3181.717277	825781.384300	40.358580
3185.154111	827332.097706	40.363597
3188.062946	828905.042807	40.368615
3191.487075	830443.079135	40.373632
3194.501133	832017.250567	40.378650
3197.722179	833563.930396	40.383668
3201.243859	835117.929900	40.388685
3204.025864	836679.657231	40.393703
3207.257104	838253.921424	40.398720
3210.536445	839810.762758	40.403738
3213.536491	841385.458433	40.408756
3216.881614	842946.383322	40.413773
3219.908231	844513.294416	40.418791
3223.443956	846072.733471	40.423808
3226.871618	847636.272821	40.428826
3229.819268	849160.835031	40.433844
3233.047027	850679.636462	40.438861
3236.056203	852212.765277	40.443879
3239.346786	853716.053749	40.448896
3242.525805	855232.291290	40.453914
3245.658463	856750.880043	40.458932
3248.701086	858287.539248	40.463949
3251.925436	859818.157750	40.468967
3255.170380	861346.352757	40.473984
3258.372068	862890.746488	40.479002
3261.184842	864434.714015	40.484020
3264.660899	865983.893988	40.489037
3267.548750	867560.183436	40.494055
3270.256555	869126.502442	40.499072
3273.786529	870716.478018	40.504090
3276.682823	872300.521064	40.509108
3279.949154	873896.659549	40.514125
3283.005616	875506.525405	40.519143
3286.147285	877108.202530	40.524160
3289.595639	878743.133643	40.529178
3292.499073	880383.401612	40.534196
3296.154638	882016.902196	40.539213
3299.124688	883663.291765	40.544231
3302.301056	885311.402232	40.549248
3305.621198	886967.129644	40.554266
3309.018283	888640.899999	40.559284
3312.570103	890313.193404	40.564301
3315.854613	891991.120135	40.569319
3318.907324	893678.813993	40.574336
3322.460960	895359.563353	40.579354
3325.622356	897048.938790	40.584372
3328.967298	898742.693310	40.589389
3332.446179	900459.995229	40.594407
3335.754286	902165.247085	40.599424
3339.280569	903867.056638	40.604442
3342.458832	905587.938387	40.609460
3346.112258	907296.089615	40.614477
3349.289321	909019.083501	40.619495
3352.915549	910730.988041	40.624512
3356.596691	912445.523241	40.629530
3359.717815	914176.524510	40.634548
3363.320828	915895.758130	40.639565
3366.641095	917621.409558	40.644583
3370.175848	919346.670054	40.649600
3373.666184	921070.333233	40.654618
3376.993020	922802.777699	40.659636
3380.671569	924527.606796	40.664653
3384.003326	926272.452419	40.669671
3387.852726	927995.465568	40.674688
3391.501271	929713.164952	40.679706
3394.806520	931425.672964	40.684724
3398.149341	933147.864591	40.689741
3401.646175	934875.019673	40.694759
3405.295151	936594.024482	40.699776
3408.646137	938313.758071	40.704794
3411.653207	940036.328693	40.709812
3415.596549	941750.338039	40.714829
3418.844017	943476.508134	40.719847
3422.523944	945207.761974	40.724864
3425.852464	946922.547047	40.729882
3429.084383	948644.698367	40.734900
3432.698820	950364.871988	40.739917
3436.373571	952090.942464	40.744935
3439.809955	953835.509321	40.749952
3443.183315	955594.575825	40.754970
3446.312816	957353.048616	40.759988
3450.225196	959110.172008	40.765005
3453.534670	960853.300603	40.770010
3456.681424	962545.511851	40.775015
3460.011850	964185.691254	40.780020
3462.808147	965760.198617	40.785024
3466.346344	967271.128185	40.790029
3469.765768	968698.125146	40.795034
3472.702353	970052.267224	40.800039
3475.311594	971325.365409	40.805044
3478.055360	972537.538909	40.810048
3481.023283	973665.741306	40.815053
3483.537955	974724.207762	40.820058
3485.993945	975708.905350	40.825063
3488.626737	976620.908017	40.830068
3490.636412	977474.058811	40.835072
3492.908205	978238.642259	40.840077
3494.945111	978949.642080	40.845082
3496.925945	979603.142668	40.850087
3498.750271	980195.079270	40.855092
3500.240223	980729.210424	40.860096
3502.124867	981188.640566	40.865101
3504.018876	981625.091763	40.870106
3505.475145	982003.112170	40.875111
3506.794377	982317.490717	40.880116
3508.011033	982601.319448	40.885120
3509.217886	982828.431398	40.890125
3510.375364	983034.266829	40.895130
3511.414926	983193.563091	40.900135
3512.800718	983309.760867	40.905140
3513.517413	983388.202250	40.910144
3514.486099	983453.231574	40.915149
3515.277276	983469.496017	40.920154
3516.281257	983456.546801	40.925159
3516.961779	983406.762606	40.930164
3517.746365	983369.940170	40.935168
3518.542278	983257.776042	40.940173
3519.041766	983149.855028	40.945178
3519.459954	983020.962515	40.950183
3519.959390	982860.822568	40.955188
3520.595773	982692.261934	40.960192
3521.390854	982495.072329	40.965197
3521.361008	982295.474019	40.970202
3521.989766	982063.939063	40.975207
3522.544945	981829.478381	40.980212
3522.517691	981582.803980	40.985216
3523.291856	981308.456952	40.990221
3523.564919	981031.055169	40.995226
3523.618668	980733.563471	41.000231
3523.945913	980428.004805	41.005236
3524.018600	980128.623316	41.010240
3524.590810	979808.539772	41.015245
3524.333883	979492.090468	41.020250
3524.666696	979155.213029	41.025255
3525.107050	978806.089658	41.030260
3525.317504	978468.605892	41.035264
3525.288298	978108.187188	41.040269
3525.547232	977742.032548	41.045274
3525.652231	977367.869115	41.050279
3525.738636	976989.190148	41.055284
3525.731000	976608.840616	41.060288
3526.186594	976228.780317	41.065293
3526.403033	975842.675681	41.070298
3526.111480	975445.976726	41.075303
3526.575927	975036.811583	41.080308
3526.316388	974639.660520	41.085312
3526.376452	974237.151014	41.090317
3526.241246	973825.847698	41.095322
3526.409095	973409.088158	41.100327
3526.594927	972997.770235	41.105332
3526.252467	972594.527198	41.110336
3526.369214	972164.975044	41.115341
3526.106519	971760.193427	41.120346
3525.986223	971341.668554	41.125351
3526.268325	970908.376577	41.130356
3526.101758	970496.545943	41.135360
3526.262580	970077.686864	41.140365
3526.187166	969649.347263	41.145370
3526.185021	969231.920620	41.150375
3526.281226	968804.076618	41.155380
3525.976172	968388.301741	41.160384
3526.097933	967952.464611	41.165389
3526.347743	967528.218585	41.170394
3525.993298	967094.449819	41.175399
3525.886912	966658.454184	41.180404
3525.796048	966246.012333	41.185408
3525.954288	965803.937489	41.190413
3525.721651	965377.164839	41.195418
3525.660971	964945.143287	41.200423
3525.584586	964515.343800	41.205428
3525.344049	964105.122807	41.210432
3525.727741	963666.959023	41.215437
3525.718912	963239.403251	41.220442
3525.165315	962812.884843	41.225447
3525.515398	962383.149581	41.230452
3525.202331	961959.270789	41.235456
3525.284078	961532.748738	41.240461
3525.092550	961112.999952	41.245466
3524.874548	960692.833024	41.250471
3525.421072	960258.987831	41.255476
3524.476256	959847.011531	41.260480
3524.801559	959402.849341	41.265485
3524.946915	958994.356392	41.270490
3524.546966	958577.593333	41.275495
3524.553582	958149.853057	41.280500
3524.483480	957740.620638	41.285504
3524.330719	957320.981293	41.290509
3524.550433	956892.328386	41.295514
3524.604556	956478.574150	41.300519
3524.815315	956052.703732	41.305524
3524.344897	955640.740828	41.310528
3524.530497	955213.439778	41.315533
3524.190480	954797.080149	41.320538
3523.922844	954398.529666	41.325543
3523.897630	953971.956152	41.330548
3523.982447	953549.943587	41.335552
3523.845300	953127.250039	41.340557
3523.710302	952722.872049	41.345562
3523.604229	952315.202501	41.350567
3523.902962	951914.564351	41.355572
3523.623046	951515.998458	41.360576
3523.420458	951114.997463	41.365581
3523.275049	950705.155243	41.370586
3523.312742	950314.669487	41.375591
3523.128631	949912.805696	41.380596
3522.778052	949532.082441	41.385600
3522.777746	949137.398895	41.390605
3522.587241	948744.247329	41.395610
3522.748472	948359.429175	41.400615
3522.666540	947978.928984	41.405620
3522.155506	947592.919890	41.410624
3522.042943	947204.901710	41.415629
3522.237592	946820.441277	41.420634
3522.122800	946452.469469	41.425639
3521.820136	946064.205059	41.430644
3521.716516	945697.613577	41.435648
3522.217670	945317.777867	41.440653
3521.903427	944949.348516	41.445658
3521.687748	944581.930083	41.450663
3521.574283	944192.344317	41.455668
3521.571527	943829.817697	41.460672
3521.247851	943465.881681	41.465677
3521.002246	943087.920854	41.470682
3520.887488	942737.885590	41.475687
3520.842083	942356.964345	41.480692
3520.617443	942005.748022	41.485696
3520.995081	941651.917295	41.490701
3520.620095	941290.232552	41.495706
3520.713665	940931.128872	41.500711
3520.548309	940575.397575	41.505716
3520.086328	940225.250119	41.510720
3520.351680	939862.114528	41.515725
3520.715336	939520.314902	41.520730
3520.459543	939167.282358	41.525735
3520.395832	938805.277823	41.530740
3520.247655	938456.206243	41.535744
3519.888853	938103.022820	41.540749
3520.038115	937759.225464	41.545754
3519.609664	937422.021990	41.550759
3519.697606	937058.049360	41.555764
3519.692835	936727.349005	41.560768
3519.552414	936366.531136	41.565773
3519.518380	936033.106046	41.570778
3519.216281	935700.567334	41.575783
3519.923006	935360.262193	41.580788
3519.579105	935035.171497	41.585792
3519.083108	934683.315388	41.590797
3519.280545	934356.078564	41.595802
3518.836977	934014.340568	41.600807
3519.009668	933672.958728	41.605812
3518.635995	933360.629473	41.610816
3519.000526	933033.187031	41.615821
3518.812983	932699.000130	41.620826
3518.695660	932369.868176	41.625831
3519.140601	932032.367142	41.630836
3518.480002	931708.659507	41.635840
3518.557523	931376.169437	41.640845
3518.521320	931047.998020	41.645850
3518.138319	930740.988519	41.650855
3518.203215	930406.711296	41.655860
3518.216339	930094.989750	41.660864
3517.876122	929777.737771	41.665869
3517.863420	929462.333810	41.670874
3517.828683	929162.667245	41.675879
3517.991715	928832.981362	41.680884
3517.649627	928526.413453	41.685888
3517.496108	928217.491180	41.690893
3517.297311	927906.252675	41.695898
3517.225172	927599.202645	41.700903
3517.316870	927298.833917	41.705908
3517.252977	926988.768769	41.710912
3517.243968	926692.610526	41.715917
3517.010705	926388.496396	41.720922
3516.727192	926094.176151	41.725927
3516.897521	925794.286553	41.730932
3516.878952	925510.655127	41.735936
3516.535806	925209.952344	41.740941
3516.490483	924919.469317	41.745946
3516.318504	924624.473163	41.750951
3516.324494	924338.276202	41.755956
3516.152104	924056.323682	41.760960
3515.960221	923769.263704	41.765965
3516.041667	923488.681806	41.770970
3515.843432	923210.919942	41.775975
3516.107057	922922.297336	41.780980
3516.035293	922645.735597	41.785984
3515.916375	922358.588331	41.790989
3516.085008	922078.591800	41.795994
3516.110689	921803.413465	41.800999
3515.871074	921517.106926	41.806004
3515.714226	921239.717578	41.811008
3515.441613	920958.966104	41.816013
3515.783653	920682.908961	41.821018
3514.795188	920408.307629	41.826023
3515.514219	920132.641341	41.831028
3515.107482	919870.135932	41.836032
3515.100125	919606.782217	41.841037
3515.031826	919330.531263	41.846042
3514.837013	919071.127731	41.851047
3514.856208	918800.224346	41.856052
3514.593024	918547.351142	41.861056
3514.248894	918278.887628	41.866061
3514.636331	918020.974169	41.871066
3514.434795	917777.968811	41.876071
3514.571457	917509.484337	41.881076
3514.046593	917265.835541	41.886080
3514.080603	917010.724071	41.891085
3513.792435	916777.411420	41.896090
3513.606922	916527.127102	41.901095
3513.883068	916278.680866	41.906100
3513.660724	916047.925745	41.911104
3513.725024	915802.477579	41.916109
3513.807363	915556.822818	41.921114
3513.534439	915324.601033	41.926119
3513.970055	915077.999858	41.931124
3513.778305	914844.684976	41.936128
3513.445444	914595.106805	41.941133
3513.518707	914350.458751	41.946138
3513.204841	914122.430536	41.951143
3513.282639	913884.310635	41.956148
3513.430718	913643.953266	41.961152
3513.401289	913410.454187	41.966157
3513.265275	913179.949147	41.971162
3512.882849	912942.731198	41.976167
3512.845122	912713.635480	41.981172
3512.886203	912482.782952	41.986176
3512.765121	912263.317014	41.991181
3512.798537	912032.639544	41.996186
3512.620188	911814.321391	42.001191
3512.612029	911587.486503	42.006196
3512.889368	911364.353585	42.011200
3512.708396	911147.069442	42.016205
3512.749293	910922.704753	42.021210
3512.385321	910706.879030	42.026215
3512.410800	910476.137654	42.031220
3512.139616	910269.725106	42.036224
3512.058756	910049.778762	42.041229
3512.278630	909832.665952	42.046234
3511.895718	909617.764683	42.051239
3512.229536	909400.230515	42.056244
3512.127774	909193.653426	42.061248
3511.971241	908980.521792	42.066253
3512.342983	908765.655889	42.071258
3512.160039	908548.751853	42.076263
3512.108339	908337.892209	42.081268
3512.023531	908124.908654	42.086272
3511.803433	907917.242748	42.091277
3512.088491	907706.592887	42.096282
3511.883046	907504.502148	42.101287
3511.650736	907283.313555	42.106292
3511.532348	907085.918741	42.111296
3511.395885	906882.250894	42.116301
3511.314417	906685.125089	42.121306
3511.104703	906480.682989	42.126311
3511.961470	906289.079301	42.131316
3511.452763	906083.417918	42.136320
3511.196622	905890.826343	42.141325
3511.450742	905680.972950	42.146330
3510.958773	905481.653376	42.151335
3511.084544	905278.365941	42.156340
3511.065032	905102.398071	42.161344
3510.803192	904905.045966	42.166349
3510.677760	904701.007017	42.171354
3510.535324	904520.120340	42.176359
3510.879361	904344.937061	42.181364
3510.507361	904164.173157	42.186368
3510.667398	903965.174413	42.191373
3510.792180	903775.148888	42.196378
3510.486520	903606.611482	42.201383
3510.230520	903417.408548	42.206388
3510.403532	903240.578226	42.211392
3510.405195	903053.443732	42.216397
3510.712701	902865.963048	42.221402
3510.197048	902696.660691	42.226407
3510.214132	902516.551557	42.231412
3510.165212	902338.088427	42.236416
3509.874847	902143.442704	42.241421
3510.340071	901970.578323	42.246426
3510.103832	901801.106336	42.251431
3510.210368	901619.119491	42.256436
3509.853768	901457.186828	42.261440
3510.156686	901275.349566	42.266445
3509.837874	901097.663781	42.271450
3509.787754	900936.051780	42.276455
3509.857297	900754.236103	42.281460
3509.771991	900587.116404	42.286464
3509.716724	900423.173192	42.291469
3509.644631	900252.372180	42.296474
3509.467561	900085.735505	42.301479
3509.387004	899921.878417	42.306484
3509.368222	899759.841194	42.311488
3509.333101	899594.132274	42.316493
3509.681767	899429.900448	42.321498
3509.352656	899264.230261	42.326503
3509.592380	899086.968422	42.331508
3509.389767	898943.674610	42.336512
3509.038309	898794.220209	42.341517
3509.474734	898612.371535	42.346522
3509.158374	898471.499187	42.351527
3509.120900	898307.394900	42.356532
3509.210410	898147.611774	42.361536
3508.820116	897975.635050	42.366541
3509.284618	897817.906015	42.371546
3508.982634	897681.068878	42.376551
3509.189880	897523.277407	42.381556
3508.976822	897374.245669	42.386560
3509.049859	897213.279543	42.391565
3509.228949	897058.281513	42.396570
3508.786884	896912.463644	42.401575
3508.896261	896756.889146	42.406580
3508.485832	896600.719652	42.411584
3508.657467	896454.402393	42.416589
3508.698245	896303.754658	42.421594
3508.507358	896163.287293	42.426599
3508.568688	896000.452668	42.431604
3508.682898	895863.696316	42.436608
3508.341177	895722.373164	42.441613
3508.844666	895568.633909	42.446618
3508.452644	895419.870185	42.451623
3508.351969	895276.370072	42.456628
3508.307064	895131.697371	42.461632
3508.437773	894977.133701	42.466637
3508.229924	894842.435489	42.471642
3508.189183	894706.160072	42.476647
3508.252939	894553.045738	42.481652
3507.919663	894412.655197	42.486656
3507.774814	894269.426933	42.491661
3508.080561	894139.170601	42.496666
3507.809972	894014.902930	42.501671
3508.015554	893884.463944	42.506676
3508.067318	893745.926914	42.511680
3507.958501	893619.013825	42.516685
3507.872179	893473.049034	42.521690
3507.741427	893343.426491	42.526695
3507.921055	893211.139493	42.531700
3507.890661	893083.041391	42.536704
3507.746615	892954.282342	42.541709
3507.790732	892815.240546	42.546714
3507.519349	892691.524286	42.551719
3507.541677	892551.512765	42.556724
3507.382108	892420.133551	42.561728
3507.583624	892300.101970	42.566733
3507.260660	892186.246249	42.571738
3507.520531	892050.341328	42.576743
3507.564068	891926.556624	42.581748
3507.366926	891798.844010	42.586752
3507.339396	891679.804193	42.591757
3507.363658	891561.043494	42.596762
3507.303790	891436.104715	42.601767
3507.336902	891310.470903	42.606772
3507.203890	891189.504015	42.611776
3507.279767	891062.793863	42.616781
3507.322411	890943.630467	42.621786
3506.954483	890828.304349	42.626791
3506.940934	890700.827162	42.631796
3507.436113	890592.995231	42.636800
3506.961282	890478.550212	42.641805
3506.674086	890352.657997	42.646810
3506.809199	890247.297114	42.651815
3506.971820	890120.842054	42.656820
3506.991339	890009.595150	42.661824
3506.573993	889894.645337	42.666829
3506.821496	889780.744551	42.671834
3506.814196	889672.881392	42.676839
3506.607249	889561.663122	42.681844
3506.538155	889441.229293	42.686848
3506.759471	889331.387176	42.691853
3506.921381	889225.616162	42.696858
3506.883900	889101.396840	42.701863
3507.000248	888981.987094	42.706868
3506.635545	888884.326971	42.711872
3506.449451	888773.864056	42.716877
3506.767177	888657.800849	42.721882
3506.296725	888552.411915	42.726887
3506.785440	888445.218093	42.731892
3506.915288	888322.018758	42.736896
3506.495239	888215.744490	42.741901
3506.676991	888115.852475	42.746906
3506.541651	888009.527498	42.751911
3506.471417	887901.931822	42.756916
3506.541148	887789.762798	42.761920
3506.596696	887688.626141	42.766925
3506.626297	887582.362888	42.771930
3506.410895	887472.847614	42.776935
3506.421982	887365.228531	42.781940
3506.088596	887257.373849	42.786945
3505.875082	887166.240790	42.791949
3506.510671	887066.546193	42.796954
3506.073171	886965.478095	42.801959
3506.208875	886861.506954	42.806964
3506.211864	886769.751245	42.811969
3506.016325	886661.185195	42.816973
3506.323071	886559.793803	42.821978
3506.245541	886467.175425	42.826983
3506.192007	886357.805929	42.831988
3505.941308	886265.503237	42.836993
3505.967989	886168.894213	42.841997
3506.065782	886072.368661	42.847002
3506.105359	885983.014463	42.852007
3506.077322	885883.699230	42.857012
3506.228567	885769.251069	42.862017
3506.246523	885688.802022	42.867021
3506.254469	885587.249212	42.872026
3506.358404	885481.419143	42.877031
3506.310570	885371.255586	42.882036
3506.380045	885273.850083	42.887041
3505.747631	885177.623551	42.892045
3506.111773	885071.936769	42.897050
3505.668388	884983.711719	42.902055
3506.070899	884882.952938	42.907060
3506.047780	884782.068887	42.912065
3505.856453	884689.344004	42.917069
3505.669665	884587.127993	42.922074
3505.466086	884504.472022	42.927079
3505.713916	884417.189573	42.932084
3505.501577	884325.914769	42.937089
3505.198244	884240.172911	42.942093
3505.956621	884155.707363	42.947098
3505.539999	884076.275875	42.952103
3505.660047	883973.804849	42.957108
3505.814693	883879.363823	42.962113
3505.572632	883803.385988	42.967117
3505.880103	883705.140248	42.972122
3505.644821	883613.664354	42.977127
3505.351616	883528.588217	42.982132
3505.542875	883443.043643	42.987137
3505.327679	883346.621160	42.992141
3505.313171	883260.139335	42.997146
3505.194951	883180.162197	43.002151
3505.744133	883091.454322	43.007156
3505.538499	883014.201118	43.012161
3505.448418	882927.533099	43.017165
3505.495799	882836.482683	43.022170
3505.492240	882748.441779	43.027175
3505.217959	882671.292191	43.032180
3505.301630	882594.857479	43.037185
3504.925367	882511.136173	43.042189
3505.148118	882419.372327	43.047194
3505.205050	882356.983823	43.052199
3505.121202	882258.584430	43.057204
3505.324141	882178.540631	43.062209
3505.227603	882100.676146	43.067213
3505.474727	882016.748170	43.072218
3505.579022	881934.876783	43.077223
3505.557920	881852.831165	43.082228
3505.289984	881772.278145	43.087233
3505.007934	881690.563852	43.092237
3505.290977	881604.492811	43.097242
3504.980368	881530.434115	43.102247
3505.067893	881449.139938	43.107252
3505.421213	881374.873011	43.112257
3504.795894	881288.171929	43.117261
3505.039019	881213.242940	43.122266
3505.100398	881139.214879	43.127271
3504.972473	881051.071971	43.132276
3505.147873	880983.998830	43.137281
3504.707149	880915.282467	43.142285
3505.156203	880823.068714	43.147290
3504.923033	880760.420284	43.152295
3504.902736	880672.253933	43.157300
3504.989140	880595.598822	43.162305
3504.858010	880521.788447	43.167309
3504.724316	880448.268245	43.172314
3504.682155	880382.774365	43.177319
3504.669231	880302.062165	43.182324
3504.755236	880229.278191	43.187329
3504.507298	880158.292515	43.192333
3504.995941	880092.029640	43.197338
3504.582553	880023.395191	43.202343
3504.072659	879961.462103	43.207348
3504.573919	879900.912228	43.212353
3504.556727	879831.241219	43.217357
3504.698613	879757.763851	43.222362
3504.489767	879684.730972	43.227367
3504.470382	879624.264018	43.232372
3504.668461	879557.461528	43.237377
3504.367534	879477.560690	43.242381
3504.844986	879416.815924	43.247386
3504.257306	879346.942412	43.252391
3504.431120	879279.656194	43.257396
3504.532102	879207.050889	43.262401
3504.231443	879150.598899	43.267405
3504.272793	879092.539351	43.272410
3504.525955	879024.946392	43.277415
3504.663367	878960.860806	43.282420
3504.487303	878886.843400	43.287425
3504.370957	878826.578039	43.292429
3504.405226	878755.722725	43.297434
3504.306517	878697.488501	43.302439
3504.460561	878624.867257	43.307444
3504.381748	878559.359046	43.312449
3504.432768	878501.679768	43.317453
3504.260845	878429.885228	43.322458
3504.739450	878361.181289	43.327463
3504.386444	878303.663558	43.332468
3504.528938	878243.640363	43.337473
3504.298776	878182.320905	43.342477
3504.467772	878106.976710	43.347482
3504.455804	878044.747473	43.352487
3504.418597	877990.373470	43.357492
3504.352780	877922.820391	43.362497
3504.008020	877857.057360	43.367501
3504.413919	877790.685232	43.372506
3504.352555	877738.930216	43.377511
3504.465652	877675.416260	43.382516
3504.329600	877606.126194	43.387521
3504.054936	877542.965516	43.392525
3504.406326	877469.328072	43.397530
3504.066817	877422.075492	43.402535
3504.030434	877361.878886	43.407540
3504.345539	877301.720703	43.412545
3504.541148	877245.847272	43.417549
3504.270487	877184.136292	43.422554
3504.360247	877120.038503	43.427559
3504.173296	877047.163121	43.432564
3504.059741	876989.205281	43.437569
3504.073177	876934.231471	43.442573
3504.330500	876864.577015	43.447578
3503.963843	876811.409842	43.452583
3504.257675	876746.886559	43.457588
3504.009154	876692.147560	43.462593
3503.930657	876638.252656	43.467597
3504.048021	876573.174803	43.472602
3504.114092	876534.186682	43.477607
3503.672866	876476.374742	43.482612
3504.201236	876419.178180	43.487617
3504.276778	876368.455138	43.492621
3504.264903	876305.431819	43.497626
3504.007280	876250.108440	43.502631
3503.682672	876192.371465	43.507636
3503.679946	876129.538689	43.512641
3503.915261	876081.792793	43.517645
3503.948113	876026.807329	43.522650
3503.939460	875979.488669	43.527655
3503.572954	875925.440767	43.532660
3504.038679	875866.115860	43.537665
3503.691283	875818.075955	43.542669
3504.194127	875752.828584	43.547674
3504.009904	875709.803443	43.552679
3503.795053	875660.576750	43.557684
3503.817926	875603.067682	43.562689
3503.857750	875545.361312	43.567693
3503.993896	875484.826204	43.572698
3503.737474	875445.981007	43.577703
3503.555130	875381.812196	43.582708
3503.811716	875337.451008	43.587713
3503.488808	875302.301002	43.592717
3503.551498	875241.969468	43.597722
3503.549565	875189.697389	43.602727
3503.586873	875147.892411	43.607732
3503.606021	875087.857424	43.612737
3503.304559	875041.452337	43.617741
3503.742232	874991.627652	43.622746
3503.486614	874944.050438	43.627751
3503.269872	874891.811117	43.632756
3503.843657	874857.286622	43.637761
3503.081163	874806.591257	43.642765
3503.404525	874746.987629	43.647770
3503.662494	874724.055975	43.652775
3503.569621	874685.081843	43.657780
3503.266378	874627.326050	43.662785
3503.276137	874593.280902	43.667789
3503.269803	874537.221147	43.672794
3503.416555	874496.557439	43.677799
3503.330009	874458.453704	43.682804
3503.437619	874405.865678	43.687809
3503.425787	874365.324190	43.692813
3503.508181	874318.268223	43.697818
3503.700892	874274.297580	43.702823
3503.478617	874216.718433	43.707828
3503.849196	874179.022575	43.712833
3503.522428	874130.771562	43.717837
3503.473397	874078.303436	43.722842
3503.433566	874039.995315	43.727847
3503.419145	873989.654697	43.732852
3503.484644	873938.136468	43.737857
3503.271747	873895.102851	43.742861
3503.569462	873849.850734	43.747866
3503.548497	873807.463880	43.752871
3503.515859	873767.406749	43.757876
3503.819648	873720.794589	43.762881
3503.334535	873669.364739	43.767885
3503.447713	873625.984430	43.772890
3503.462538	873575.441465	43.777895
3503.260712	873539.484977	43.782900
3503.213478	873490.503641	43.787905
3503.172703	873449.378606	43.792909
3503.384666	873406.950516	43.797914
3503.385035	873361.646658	43.802919
3503.302009	873329.646770	43.807924
3503.223294	873281.639011	43.812929
3503.257190	873241.082304	43.817933
3503.326994	873187.616594	43.822938
3503.372205	873155.400613	43.827943
3502.999179	873112.872771	43.832948
3503.076400	873068.427149	43.837953
3503.191126	873033.482615	43.842957
3503.137184	872996.625326	43.847962
3503.006901	872954.541442	43.852967
3502.997474	872924.079523	43.857972
3503.009888	872892.546646	43.862977
3503.029695	872863.534878	43.867981
3503.280804	872801.983246	43.872986
3503.423067	872766.159423	43.877991
3503.163898	872720.699395	43.882996
3502.840920	872682.720227	43.888001
3503.106163	872647.457560	43.893005
3503.050425	872599.925619	43.898010
3502.865267	872569.102739	43.903015
3502.877736	872539.120358	43.908020
3503.016896	872500.481742	43.913025
3502.793197	872475.777295	43.918029
3503.071702	872433.816426	43.923034
3503.353394	872403.691984	43.928039
3502.993460	872363.873361	43.933044
3503.406611	872309.372916	43.938049
3503.241813	872275.149175	43.943053
3503.212747	872239.156349	43.948058
3503.430968	872202.928506	43.953063
3503.048078	872158.357827	43.958068
3503.070302	872122.743969	43.963073
3502.800487	872084.267061	43.968077
3503.347903	872037.407509	43.973082
3503.089876	872000.674703	43.978087
3503.015073	871975.167379	43.983092
3503.234626	871925.158855	43.988097
3502.878358	871903.967106	43.993101
3502.767366	871849.645843	43.998106
3503.074872	871816.020897	44.003111
3503.092044	871789.042082	44.008116
3503.210682	871748.170125	44.013121
3503.230551	871711.874938	44.018125
3503.268133	871663.446802	44.023130
3502.812609	871622.086342	44.028135
3502.731975	871601.818496	44.033140
3503.032332	871553.540254	44.038145
3502.867491	871528.531053	44.043149
3503.168960	871494.905292	44.048154
3503.229526	871455.108348	44.053159
3503.002855	871417.590440	44.058164
3503.264138	871373.295921	44.063169
3503.366665	871338.537535	44.068173
3503.313366	871293.517901	44.073178
3503.553587	871253.690014	44.078183
3503.128171	871212.127654	44.083188
3503.085940	871174.189643	44.088193
3502.855325	871136.767662	44.093197
3503.172600	871099.449277	44.098202
3503.207933	871075.666817	44.103207
3503.299974	871030.330106	44.108212
3503.488106	870986.432964	44.113217
3503.230537	870956.195956	44.118221
3503.132630	870900.019929	44.123226
3503.190038	870868.274818	44.128231
3503.271130	870827.111581	44.133236
3503.315210	870788.768690	44.138241
3503.157200	870749.488313	44.143245
3503.228399	870705.996588	44.148250
3503.427348	870676.750547	44.153255
3502.959340	870628.494358	44.158260
3503.134296	870597.698996	44.163265
3503.415834	870556.694984	44.168269
3503.010587	870508.427482	44.173274
3502.820544	870471.285813	44.178279
3502.877195	870448.856154	44.183284
3503.376303	870404.612328	44.188289
3503.295660	870372.596149	44.193293
3503.123630	870335.935967	44.198298
3503.154977	870289.438909	44.203303
3503.012669	870253.161566	44.208308
3503.359742	870210.882585	44.213313
3502.841848	870184.955290	44.218317
3502.640707	870155.481426	44.223322
3502.888495	870111.373900	44.228327
3502.944656	870086.419302	44.233332
3503.194274	870051.629193	44.238337
3503.289663	870012.981675	44.243341
3503.173118	869971.650975	44.248346
3503.122160	869943.995579	44.253351
3503.082012	869897.021914	44.258356
3503.079171	869856.254086	44.263361
3502.897676	869829.687415	44.268365
3503.280363	869794.873891	44.273370
3503.297683	869759.829150	44.278375
3502.810409	869719.528478	44.283380
3502.900688	869670.978426	44.288385
3503.286488	869633.736678	44.293389
3503.236801	869605.788294	44.298394
3503.345109	869566.844550	44.303399
3503.022353	869530.495476	44.308404
3503.145512	869490.286834	44.313409
3503.126136	869460.197151	44.318413
3503.032002	869425.751261	44.323418
3503.055862	869387.985166	44.328423
3503.005016	869343.824109	44.333428
3503.259411	869310.290897	44.338433
3503.058967	869281.395067	44.343437
3503.138831	869242.745133	44.348442
3503.157378	869197.018314	44.353447
3502.906824	869169.877617	44.358452
3502.867004	869116.199305	44.363457
3502.856424	869098.920898	44.368461
3503.123988	869053.928603	44.373466
3503.203489	869022.364214	44.378471
3502.700228	868990.604422	44.383476
3502.763408	868942.926669	44.388481
3502.785807	868922.729836	44.393485
3502.950590	868892.315709	44.398490
3502.923330	868863.389328	44.403495
3502.753092	868829.243796	44.408500
3503.042363	868782.401279	44.413505
3503.336072	868754.974861	44.418509
3503.113738	868729.186716	44.423514
3503.209020	868669.462794	44.428519
3502.957519	868645.717925	44.433524
3503.314513	868602.455086	44.438529
3502.984213	868566.101393	44.443533
3503.133789	868531.610208	44.448538
3503.183001	868488.105984	44.453543
3502.841142	868448.355324	44.458548
3503.128604	868425.491695	44.463553
3502.965625	868393.090121	44.468557
3502.901130	868358.827395	44.473562
3502.981472	868326.967930	44.478567
3503.135654	868294.319384	44.483572
3503.016349	868255.210430	44.488577
3502.767786	868228.647698	44.493581
3503.024867	868179.281325	44.498586
3502.996847	868156.080266	44.503591
3502.744122	868122.429773	44.508596
3502.804590	868078.532340	44.513601
3502.734578	868048.055520	44.518605
3502.469726	868023.630702	44.523610
3502.864274	867991.426398	44.528615
3503.053650	867954.789181	44.533620
3502.816250	867923.077019	44.538625
3503.142084	867897.292081	44.543629
3503.178611	867863.204080	44.548634
3503.009267	867823.129550	44.553639
3502.902073	867792.463356	44.558644
3503.246556	867751.818190	44.563649
3502.861609	867715.274133	44.568653
3502.686025	867680.734528	44.573658
3502.921877	867647.195081	44.578663
3502.551359	867617.542412	44.583668
3503.066809	867577.936051	44.588673
3502.770359	867553.028997	44.593677
3502.960047	867517.554327	44.598682
3502.646455	867493.135378	44.603687
3502.619768	867475.757842	44.608692
3502.946281	867434.239532	44.613697
3503.141585	867414.106243	44.618701
3502.713548	867377.178794	44.623706
3502.893721	867334.227281	44.628711
3502.766869	867308.514401	44.633716
3503.183336	867277.079537	44.638721
3502.651545	867233.661943	44.643725
3502.751040	867211.989996	44.648730
3502.855803	867184.296209	44.653735
3502.793688	867164.398717	44.658740
3502.903903	867111.454641	44.663745
3502.885698	867098.541786	44.668749
3502.608775	867057.120290	44.673754
3502.901256	867022.402671	44.678759
3502.736621	866989.896679	44.683764
3502.372594	866955.966637	44.688769
3502.383299	866934.211202	44.693773
3502.426070	866922.356190	44.698778
3502.611502	866871.437034	44.703783
3502.333798	866864.199169	44.708788
3502.907439	866832.153391	44.713793
3502.355830	866809.616095	44.718797
3502.346082	866786.503853	44.723802
3502.136405	866758.859912	44.728807
3502.309519	866742.612756	44.733812
3502.558424	866705.958125	44.738817
3502.412387	866688.403738	44.743821
3502.619432	866680.211715	44.748826
3502.354239	866630.821555	44.753831
3502.292731	866611.310613	44.758836
3502.596255	866594.167488	44.763841
3503.028070	866568.553642	44.768845
3503.019971	866529.220885	44.773850
3502.818128	866509.635612	44.778855
3502.671951	866486.738940	44.783860
3502.873414	866436.687570	44.788865
3502.809826	866408.240963	44.793869
3502.592036	866387.006813	44.798874
3502.701877	866342.797200	44.803879
3502.623770	866324.259310	44.808884
3502.685302	866280.057196	44.813889
3503.140598	866263.956513	44.818893
3502.602962	866237.238340	44.823898
3502.922910	866200.763186	44.828903
3502.474399	866175.584089	44.833908
3502.755819	866140.960343	44.838913
3502.556303	866117.196900	44.843917
3502.392640	866087.793982	44.848922
3502.963649	866065.943099	44.853927
3502.692287	866030.147108	44.858932
3503.004559	865997.460052	44.863937
3502.878790	865964.553595	44.868941
3502.650620	865931.275302	44.873946
3502.889234	865900.736749	44.878951
3502.612866	865878.733401	44.883956
3502.414872	865846.129592	44.888961
3502.191221	865825.282956	44.893965
3502.041281	865793.059475	44.898970
3502.183568	865778.757476	44.903975
3502.157327	865756.129666	44.908980
3502.586468	865730.318439	44.913985
3502.446238	865717.034185	44.918989
3502.548808	865693.316434	44.923994
3502.879518	865667.326884	44.928999
3502.833599	865653.929818	44.934004
3502.965565	865608.545545	44.939009
3502.625850	865571.106763	44.944013
3502.362155	865565.516352	44.949018
3502.370293	865532.294060	44.954023
3502.262461	865508.804524	44.959028
3502.441756	865487.113226	44.964033
3502.778551	865461.704621	44.969037
3502.609161	865440.653436	44.974042
3502.804183	865398.074232	44.979047
3502.902003	865387.761373	44.984052
3503.113282	865344.401991	44.989057
3502.859596	865321.032895	44.994061
3503.040378	865284.672276	44.999066
3503.018575	865235.716284	45.004071
3502.909864	865209.311446	45.009076
3502.928413	865182.205523	45.014081
3502.790179	865138.125094	45.019085
3502.697638	865110.745719	45.024090
3502.751306	865074.210486	45.029095
3502.619594	865060.437654	45.034100
3503.129110	865030.141505	45.039105
3502.898339	864990.349663	45.044109
3502.649522	864962.218188	45.049114
3502.933854	864923.506806	45.054119
3502.826443	864901.666347	45.059124
3502.700895	864861.564876	45.064129
3502.755380	864831.634146	45.069133
3502.680971	864817.948469	45.074138
3503.046161	864787.091986	45.079143
3502.513609	864758.229106	45.084148
3502.805880	864737.876611	45.089153
3502.923480	864702.494405	45.094157
3502.189283	864670.069727	45.099162
3502.439076	864618.343735	45.104167
3502.131270	864618.491707	45.109172
3502.590086	864599.665751	45.114177
3502.377699	864582.990533	45.119181
3502.311435	864553.369778	45.124186
3502.398225	864519.254572	45.129191
3502.702881	864500.065088	45.134196
3502.829143	864474.104095	45.139201
3502.763160	864437.196104	45.144205
3502.402915	864417.144344	45.149210
3502.532202	864388.559278	45.154215
3502.899898	864365.667044	45.159220
3502.875399	864330.597543	45.164225
3502.565470	864299.655488	45.169229
3502.614318	864279.244398	45.174234
3502.867499	864238.396289	45.179239
3502.534007	864223.877521	45.184244
3502.920370	864180.869586	45.189249
3502.594374	864168.389801	45.194253
3502.259716	864127.540630	45.199258
3502.543844	864108.741931	45.204263
3502.230634	864080.811277	45.209268
3502.421647	864059.987382	45.214273
3502.340659	864049.410216	45.219277
3502.045829	864014.869229	45.224282
3502.315526	863988.202385	45.229287
3502.012022	863986.406404	45.234292
3502.224994	863955.182110	45.239297
3502.250319	863935.453880	45.244301
3502.139791	863922.257942	45.249306
3502.614082	863905.467722	45.254311
3502.691865	863887.285316	45.259316
3502.626642	863858.049640	45.264321
3502.719944	863827.135897	45.269325
3502.650027	863806.645616	45.274330
3502.947521	863783.276921	45.279335
3502.445816	863750.808993	45.284340
3502.718486	863727.152673	45.289345
3502.978621	863691.449572	45.294349
3502.493303	863676.954501	45.299354
3502.778096	863631.335871	45.304359
3502.932133	863608.378811	45.309364
3502.509904	863576.382696	45.314369
3503.052308	863549.183147	45.319373
3502.686130	863513.290673	45.324378
3502.747270	863481.117248	45.329383
3502.747806	863459.739648	45.334388
3502.682382	863421.659315	45.339393
3503.012021	863407.418018	45.344397
3502.358846	863373.126747	45.349402
3502.485357	863341.233327	45.354407
3502.651739	863319.827910	45.359412
3502.679304	863273.180056	45.364417
3502.873223	863269.844294	45.369421
3502.572030	863238.409495	45.374426
3502.996389	863216.572513	45.379431
3502.931215	863184.321148	45.384436
3502.639279	863149.969096	45.389441
3502.886882	863121.164206	45.394445
3502.906887	863079.763644	45.399450
3502.614711	863052.310660	45.404455
3502.309891	863031.273388	45.409460
3502.323255	863016.597392	45.414465
3502.431507	862997.338336	45.419469
3502.007317	862968.643399	45.424474
3502.546648	862943.482406	45.429479
3502.258783	862926.815052	45.434484
3502.640599	862898.861612	45.439489
3502.623003	862878.165209	45.444493
3502.225811	862852.672230	45.449498
3502.833329	862822.543274	45.454503
3502.849856	862795.232628	45.459508
3502.657815	862764.068929	45.464513
3502.467642	862723.866752	45.469517
3502.252913	862719.237453	45.474522
3502.687978	862680.195358	45.479527
3502.676097	862670.770600	45.484532
3502.522273	862628.423758	45.489537
3502.812264	862616.422385	45.494541
3502.511955	862584.303752	45.499546
3502.712629	862562.890016	45.504551
3502.601897	862539.875349	45.509556
3502.573214	862507.225627	45.514561
3502.597234	862477.385468	45.519565
3502.285131	862453.334592	45.524570
3502.427531	862427.750926	45.529575
3502.549128	862403.628400	45.534580
3502.539507	862381.957109	45.539585
3502.874873	862343.026463	45.544589
3502.539723	862335.598225	45.549594
3502.519088	862292.060821	45.554599
3502.879224	862278.006238	45.559604
3502.601858	862245.104506	45.564609
3503.121798	862222.859449	45.569613
3502.763298	862182.195459	45.574618
3502.763667	862164.992562	45.579623
3502.713561	862142.257974	45.584628
3502.491706	862101.376545	45.589633
3502.748017	862078.980010	45.594637
3502.630362	862055.673067	45.599642
3502.597805	862020.397135	45.604647
3502.633475	862014.073739	45.609652
3502.846648	861975.355260	45.614657
3502.626885	861953.522671	45.619661
3502.553703	861930.791094	45.624666
3502.820964	861899.644478	45.629671
3502.916846	861862.208153	45.634676
3502.554793	861837.385488	45.639681
3502.909187	861795.435090	45.644685
3502.454440	861770.238631	45.649690
3502.786911	861745.495564	45.654695
3502.436948	861730.779119	45.659700
3502.811309	861695.823060	45.664705
3502.610054	861659.017633	45.669709
3502.433059	861645.244484	45.674714
3502.690410	861619.638480	45.679719
3502.512374	861573.789045	45.684724
3502.780988	861556.929039	45.689729
3502.767808	861523.007851	45.694733
3502.560324	861494.659039	45.699738
3502.478507	861469.983107	45.704743
3502.714230	861464.403805	45.709748
3502.607182	861420.777192	45.714753
3502.722028	861392.180390	45.719757
3502.761544	861375.454830	45.724762
3502.977520	861343.925003	45.729767
3502.907774	861318.274417	45.734772
3502.690173	861289.245875	45.739777
3502.741864	861262.894606	45.744781
3502.501937	861225.218066	45.749786
3502.440325	861196.066173	45.754791
3502.076516	861169.005292	45.759796
3502.622276	861147.821348	45.764801
3502.584376	861128.483242	45.769805
3502.741527	861102.113903	45.774810
3502.478629	861044.026120	45.779815
3502.581006	860963.421875	45.784820
3502.516441	860820.141740	45.789825
3502.479770	860622.509821	45.794829
3502.503432	860382.473608	45.799834
3502.274467	860057.008877	45.804839
3502.134049	859692.133600	45.809844
3501.792425	859256.383325	45.814849
3501.631941	858771.949296	45.819853
3501.264636	858223.517670	45.824858
3501.298820	857612.721830	45.829863
3501.020225	856953.084853	45.834868
3501.079975	856226.777696	45.839873
3500.639773	855427.785142	45.844877
3500.431123	854582.135596	45.849882
3500.222011	853647.997790	45.854887
3499.700556	852671.231713	45.859892
3499.197482	851622.847454	45.864897
3498.939113	850501.992788	45.869901
3498.408856	849328.193128	45.874906
3497.910443	848087.536240	45.879911
3497.871933	846767.538218	45.884916
3496.992003	845383.274954	45.889921
3496.737828	843937.582369	45.894925
3495.977243	842421.538129	45.899930
3495.603677	840825.826804	45.904935
3494.923192	839189.768677	45.909940
3494.481783	837451.867705	45.914945
3493.764429	835655.122803	45.919949
3492.879961	833796.685924	45.924954
3492.422393	831855.312673	45.929959
3492.036134	829851.651584	45.934964
3491.234025	827787.829016	45.939969
3490.444702	825644.559847	45.944973
3489.528366	823437.340881	45.949978
3488.743819	821160.492762	45.954983
3487.673729	818831.239173	45.959988
3487.081083	816419.203580	45.964993
3486.303290	813945.073191	45.969997
3485.170662	811413.465670	45.975002
3484.427154	808801.903292	45.980007
3483.285049	806129.939845	45.985012
3482.105067	803393.920256	45.990017
3481.280532	800593.023015	45.995021
3480.178799	797721.587337	46.000026
3479.397149	794799.321149	46.005031
3478.075150	791807.103967	46.010036
3477.301947	788747.722640	46.015041
3476.215303	785622.126638	46.020045
3475.056646	782439.151029	46.025050
3473.740566	779174.385554	46.030055
3472.397929	775857.198906	46.035060
3471.281436	772471.137233	46.040065
3470.090611	769020.454421	46.045069
3468.279034	765532.968771	46.050074
3467.475439	761963.735772	46.055079
3466.141112	758333.337128	46.060084
3464.636927	754643.319203	46.065089
3463.575650	750881.556853	46.070093
3461.928992	747076.844314	46.075098
3460.284911	743206.640737	46.080103
3459.018493	739268.183745	46.085108
3457.462079	735279.120395	46.090113
3455.970845	731220.816254	46.095117
3454.018708	727113.933916	46.100122
3452.795244	722940.777143	46.105127
3451.002582	718724.145903	46.110132
3449.170848	714427.786976	46.115137
3447.763314	710078.482935	46.120141
3446.184939	705684.222849	46.125146
3444.425872	701217.185246	46.130151
3442.832403	696692.342810	46.135156
3440.937779	692111.103897	46.140161
3439.152650	687486.233383	46.145165
3437.393738	682797.987138	46.150170
3435.801028	678040.893726	46.155175
3433.714312	673241.556975	46.160180
3431.682213	668375.015864	46.165185
3429.783134	663453.363251	46.170189
3427.893793	658483.209527	46.175194
3425.481839	653462.705415	46.180199
3423.628665	648370.291715	46.185204
3421.879150	643228.722869	46.190209
3419.529249	638046.683895	46.195213
3417.294450	632811.571971	46.200218
3415.263341	627515.771536	46.205223
3413.341933	622187.457351	46.210228
3411.175508	616801.167102	46.215233
3408.947989	611351.060979	46.220237
3406.287530	605863.143367	46.225242
3404.162385	600324.042583	46.230247
3401.840603	594744.450060	46.235252
3399.418611	589121.525945	46.240257
3397.087435	583438.284304	46.245261
3394.635469	577708.003661	46.250266
3391.993180	571942.103828	46.255271
3389.821981	566122.053735	46.260276
3386.913716	560265.206717	46.265281
3384.815494	554355.390196	46.270285
3381.673355	548413.512443	46.275290
3379.155394	542427.864907	46.280295
3376.688780	536410.399271	46.285300
3374.181273	530339.091693	46.290305
3371.573084	524230.506061	46.295309
3368.281485	518093.845413	46.300314
3365.255861	511889.209829	46.305319
3362.897578	505667.523949	46.310324
3359.904136	499418.122043	46.315329
3357.419606	493117.069428	46.320333
3354.304975	486794.421346	46.325338
3351.345748	480417.688143	46.330343
3348.115372	474022.097598	46.335348
3344.799237	467594.494527	46.340353
3342.121152	461131.095740	46.345357
3338.807781	454637.214581	46.350362
3335.547705	448119.421324	46.355367
3332.147023	441575.817808	46.360372
3329.105486	435002.919035	46.365377
3326.291596	428414.750932	46.370381
3322.813279	421793.852030	46.375386
3319.768810	415138.970418	46.380391
3316.428828	408467.468172	46.385396
3312.471843	401770.441722	46.390401
3309.388793	395050.852748	46.395405
3305.731253	388322.851739	46.400410
3302.074613	381562.213420	46.405415
3298.555403	374787.583428	46.410420
3295.010458	368004.855752	46.415425
3291.375460	361190.764174	46.420429
3287.607507	354378.397890	46.425434
3284.113468	347542.681542	46.430439
3280.358023	340703.594674	46.435444
3276.500330	333854.774882	46.440449
3272.916767	326988.268341	46.445453
3268.758023	320148.225957	46.450458
3264.954589	313256.270097	46.455463
3261.129380	306372.106902	46.460468
3256.852526	299496.423969	46.465473
3253.471815	292605.958750	46.470477
3249.459724	285719.783303	46.475482
3245.106084	278814.780922	46.480487
3241.163732	271921.135885	46.485492
3236.940757	265031.835864	46.490497
3232.792736	258139.949544	46.495501
3228.560061	251269.777926	46.500506
3224.558586	244385.922252	46.505511
3220.250415	237510.020290	46.510516
3216.032595	230643.358655	46.515521
3212.181255	223717.852155	46.520525
3207.736643	216838.351255	46.525530
3203.076033	209978.945330	46.530535
3198.420174	203152.541933	46.535540
3194.070206	196333.997249	46.540545
3189.931361	189529.803914	46.545549
3185.467371	182743.304312	46.550554
3180.788234	175962.819638	46.555559
3176.145773	169197.707781	46.560564
3171.352572	162477.274114	46.565569
3166.869558	155747.332139	46.570573
3162.309183	149056.471913	46.575578
3157.497630	142393.435658	46.580583
3152.255721	135747.494048	46.585588
3147.109373	129141.307322	46.590593
3142.817843	122551.927850	46.595597
3137.355405	115999.172287	46.600602
3132.217182	109480.973010	46.605607
3127.096196	103010.052395	46.610612
3121.990303	96571.593161	46.615617
3116.847606	90171.198344	46.620621
3111.364377	83809.817060	46.625626
3105.742407	77501.477162	46.630631
3100.014497	71231.788858	46.635636
3094.133649	65026.781213	46.640641
3088.771936	58872.668153	46.645645
3082.249918	52781.224127	46.650650
3075.746073	46742.443795	46.655655
3068.961203	40794.294769	46.660660
3061.263806	34957.336680	46.665665
3050.350259	29277.837706	46.670669
3030.556626	23961.869103	46.675674
3006.571403	18999.837640	46.680679
2979.417496	14452.267054	46.685684
2949.805254	10385.310618	46.690689
2921.329380	6809.624457	46.695693
2893.380895	3757.570973	46.700698
2866.567219	1253.542773	46.705703
2804.981293	292.457070	46.710708
2739.220190	301.989715	46.715713
2714.379479	304.961711	46.720717
2721.195768	300.039452	46.725722
2744.570759	303.289827	46.730727
2771.499416	288.918547	46.735732
2791.523639	278.924160	46.740737
2802.829108	274.180974	46.745741
2805.262490	283.437966	46.750746
2802.133944	283.479036	46.755751
2797.628415	279.974885	46.760756
2792.511497	293.067109	46.765761
2788.764652	281.233850	46.770765
2785.308416	272.444622	46.775770
2782.519271	273.067519	46.780775
2780.327318	269.188777	46.785780
2777.750365	282.101512	46.790785
2775.313721	270.089599	46.795789
2772.571484	265.425846	46.800794
2770.257880	264.111322	46.805799
2767.258452	260.235173	46.810804
2763.397835	273.366411	46.815809
2760.608026	262.009153	46.820813
2757.387335	261.909554	46.825818
2754.444685	266.595028	46.830823
2751.139063	260.484972	46.835828
2748.594003	261.692006	46.840833
2745.338866	267.680985	46.845837
2741.495321	264.699950	46.850842
2737.908425	254.292017	46.855847
2735.432437	250.414777	46.860852
2732.149369	254.603080	46.865857
2729.141027	253.293485	46.870861
2725.757755	253.543979	46.875866
2722.336463	245.130317	46.880871
2718.774768	248.516818	46.885876
2715.389647	249.900369	46.890881
2712.288540	255.045766	46.895885
2708.871941	249.783289	46.900890
2705.529201	251.625976	46.905895
2702.465111	243.432037	46.910900
2698.524106	252.339626	46.915905
2695.604404	244.391042	46.920909
2692.236022	241.797769	46.925914
2688.265252	251.186660	46.930919
2685.157829	242.884241	46.935924
2681.540583	244.379527	46.940929
2678.937319	243.040223	46.945933
2675.150141	249.623408	46.950938
2672.072619	244.354345	46.955943
2668.756718	239.433658	46.960948
2664.525909	237.408974	46.965953
2661.605021	237.886725	46.970957
2658.213517	237.498445	46.975962
2654.363779	234.961343	46.980967
2651.152074	233.688908	46.985972
2648.076630	240.212285	46.990977
2645.060378	230.188243	46.995981
2641.228894	242.076207	47.000986
2637.598029	235.058463	47.005991
2634.038153	233.542745	47.010996
2630.269551	235.061859	47.016001
2627.363169	232.437388	47.021005
2623.676388	234.891430	47.026010
2620.093553	241.069137	47.031015
2616.786671	233.988869	47.036020
2613.663648	239.902436	47.041025
2609.709143	231.500686	47.046029
2606.413464	232.206478	47.051034
2602.603314	231.916924	47.056039
2599.163947	227.405035	47.061044
2595.553435	233.085679	47.066049
2592.831073	229.382187	47.071053
2589.563119	227.435878	47.076058
2586.431438	238.387051	47.081063
2582.317093	229.586235	47.086068
2578.456912	231.901974	47.091073
2575.531201	222.231679	47.096077
2572.152147	223.948223	47.101082
2568.106735	227.979441	47.106087
2565.001795	220.104942	47.111092
2561.990435	230.120600	47.116097
2558.207098	225.164260	47.121101
2554.767272	230.591397	47.126106
2550.780870	221.882773	47.131111
2547.355387	219.074060	47.136116
2544.204036	221.652132	47.141121
2540.886553	223.155273	47.146125
2537.388450	221.397358	47.151130
2533.698334	234.789477	47.156135
2530.374436	219.221265	47.161140
2526.759083	225.868541	47.166145
2523.426110	215.241297	47.171149
2520.333325	217.776169	47.176154
2516.161866	214.297283	47.181159
2512.985621	211.701637	47.186164
2509.235627	222.777778	47.191169
2506.063492	219.315917	47.196173
2502.244184	225.013714	47.201178
2498.605706	223.350037	47.206183
2495.438348	219.320235	47.211188
2491.992168	222.648350	47.216193
2488.498814	224.055043	47.221197
2485.618437	221.130751	47.226202
2481.743358	220.559547	47.231207
2478.195771	214.572527	47.236212
2474.921039	224.593805	47.241217
2471.156999	213.208128	47.246221
2467.387279	212.972391	47.251226
2463.797240	220.919165	47.256231
2460.534472	215.132220	47.261236
2457.184562	223.106856	47.266241
2453.632363	213.384155	47.271245
2450.289391	217.835105	47.276250
2446.619762	211.095466	47.281255
2443.091917	206.410828	47.286260
2439.721361	216.325980	47.291265
2436.484603	210.237960	47.296269
2432.838432	209.915156	47.301274
2429.828369	214.015157	47.306279
2426.057529	206.762974	47.311284
2422.404115	213.184916	47.316289
2418.677418	207.473002	47.321293
2415.280671	203.705302	47.326298
2411.376597	208.919456	47.331303
2408.290156	199.836073	47.336308
2404.587536	208.523335	47.341313
2401.464965	205.193479	47.346317
2398.230750	206.613503	47.351322
2394.663583	216.717626	47.356327
2391.016168	201.445877	47.361332
2387.208013	208.746292	47.366337
2383.892839	202.741905	47.371341
2380.338451	204.908248	47.376346
2376.730181	212.534048	47.381351
2373.665678	205.164920	47.386356
2369.851586	207.172852	47.391361
2366.557224	205.322623	47.396365
2363.171580	208.343632	47.401370
2359.671053	207.873700	47.406375
2356.342045	204.861728	47.411380
2352.475201	207.656693	47.416385
2348.911001	202.836439	47.421389
2345.466062	200.237111	47.426394
2341.781131	201.478385	47.431399
2338.330321	194.694629	47.436404
2334.574761	206.983265	47.441409
2331.518735	198.740326	47.446413
2328.357483	206.795187	47.451418
2324.641876	203.049602	47.456423
2321.269904	201.069342	47.461428
2317.741848	200.749030	47.466433
2314.091257	205.021140	47.471437
2310.329497	203.474262	47.476442
2306.754113	201.754731	47.481447
2303.637687	197.483599	47.486452
2300.330613	200.786307	47.491457
2296.531769	197.889436	47.496461
2293.385532	197.278181	47.501466
2289.644600	198.150239	47.506471
2286.531768	197.281469	47.511476
2282.522152	194.782316	47.516481
2279.037281	194.396688	47.521485
2275.520824	193.890768	47.526490
2272.052534	198.606427	47.531495
2268.708732	193.576193	47.536500
2264.952109	198.733942	47.541505
2262.086994	197.127680	47.546509
2258.573404	194.216900	47.551514
2254.317797	200.203970	47.556519
2250.824737	192.870955	47.561524
2247.513026	196.195577	47.566529
2244.351756	194.198545	47.571533
2240.374442	190.409210	47.576538
2237.136895	200.188644	47.581543
2233.645260	196.602115	47.586548
2230.251744	199.078074	47.591553
2226.975345	194.923590	47.596557
2223.352057	184.370783	47.601562
2219.414970	186.494251	47.606567
2216.341875	183.822577	47.611572
2212.388429	195.421095	47.616577
2208.827326	195.122501	47.621581
2205.960192	189.907643	47.626586
2202.115430	192.780181	47.631591
2199.016600	193.935252	47.636596
2194.903735	194.418064	47.641601
2191.823323	190.014963	47.646605
2188.166205	181.154048	47.651610
2184.341301	187.498287	47.656615
2181.238531	194.180340	47.661620
2177.526428	199.742059	47.666625
2174.192821	194.647259	47.671629
2170.993716	191.390584	47.676634
2167.377292	193.804521	47.681639
2164.055345	190.408485	47.686644
2160.234245	194.203069	47.691649
2156.783553	188.350688	47.696653
2153.269021	191.322071	47.701658
2149.568524	190.453923	47.706663
2146.308844	186.042171	47.711668
2142.706941	192.453421	47.716673
2138.933576	196.562989	47.721677
2135.696757	188.810640	47.726682
2131.529614	198.920639	47.731687
2128.855229	177.735028	47.736692
2125.761006	185.803987	47.741697
2122.093160	193.827753	47.746701
2118.368219	184.638077	47.751706
2114.382977	196.848735	47.756711
2110.968902	184.390297	47.761716
2107.925549	184.119361	47.766721
2104.304234	188.236406	47.771725
2100.940568	179.610293	47.776730
2097.203002	183.400207	47.781735
2093.913978	184.087083	47.786740
2089.683022	187.755609	47.791745
2086.388243	186.166135	47.796749
2083.217393	176.100374	47.801754
2079.680833	192.115089	47.806759
2076.354229	186.665180	47.811764
2072.852888	185.491481	47.816769
2069.206037	186.164052	47.821773
2065.822456	185.675021	47.826778
2062.530918	187.173797	47.831783
2059.039500	177.705845	47.836788
2054.971443	194.078897	47.841793
2051.779122	185.669423	47.846797
2048.395829	187.449769	47.851802
2044.600960	186.703061	47.856807
2041.368166	174.493595	47.861812
2037.794385	184.695512	47.866817
2033.983490	182.128827	47.871821
2030.592096	180.224803	47.876826
2027.145091	192.235728	47.881831
2023.626612	178.871650	47.886836
2020.457205	189.017457	47.891841
2016.814667	180.874966	47.896845
2013.294904	177.391925	47.901850
2009.239572	186.910074	47.906855
2005.947211	186.204735	47.911860
2002.576694	190.097501	47.916865
1998.949572	187.577654	47.921869
1996.132672	179.036763	47.926874
1992.260102	190.362966	47.931879
1988.893117	187.542637	47.936884
1985.079028	189.136643	47.941889
1981.551113	185.344357	47.946893
1978.542535	182.222118	47.951898
1974.800525	191.326629	47.956903
1971.410672	182.285989	47.961908
1967.894532	175.248491	47.966913
1964.192317	179.305584	47.971917
1960.465234	176.331228	47.976922
1956.830952	166.195682	47.981927
1953.748452	162.818475	47.986932
1950.326343	177.283582	47.991937
1946.664911	168.817483	47.996941
1943.384337	166.260775	48.001946
1939.574556	175.150343	48.006951
1936.614762	168.625835	48.011956
1932.923853	169.609688	48.016961
1929.497597	177.287010	48.021965
1925.855140	173.738261	48.026970
1921.850616	185.895987	48.031975
1918.657818	172.323108	48.036980
1915.196345	174.914497	48.041985
1911.826346	168.692394	48.046989
1908.203367	169.540525	48.051994
1904.622424	174.634384	48.056999
1901.045104	170.486233	48.062004
1897.543162	168.906640	48.067009
1894.272100	171.756289	48.072013
1890.795950	169.818612	48.077018
1886.979671	176.808516	48.082023
1884.015855	169.865756	48.087028
1880.281660	176.285018	48.092033
1876.578603	174.768457	48.097037
1873.059973	175.959918	48.102042
1869.220146	183.066013	48.107047
1866.298208	167.281061	48.112052
1862.525255	166.850965	48.117057
1859.175583	166.217950	48.122061
1855.892823	163.094907	48.127066
1852.209422	168.715452	48.132071
1848.623541	153.413759	48.137076
1845.319056	166.909891	48.142081
1841.403476	168.189044	48.147085
1838.059365	166.010747	48.152090
1834.454967	172.623897	48.157095
1831.462825	178.645334	48.162100
1827.860532	166.965960	48.167105
1824.540441	170.246256	48.172109
1821.122710	168.297995	48.177114
1816.999251	171.209363	48.182119
1813.676294	167.882231	48.187124
1810.282966	160.812544	48.192129
1806.423393	173.296282	48.197133
1802.941200	166.545772	48.202138
1799.714762	164.935741	48.207143
1796.322870	168.953534	48.212148
1792.307340	173.854627	48.217153
1788.704770	167.245574	48.222157
1785.632168	159.185368	48.227162
1782.205789	161.172720	48.232167
1778.907960	163.089504	48.237172
1775.184138	170.866990	48.242177
1771.708467	172.594111	48.247181
1768.155156	165.055562	48.252186
1764.733632	168.579002	48.257191
1761.085875	170.630568	48.262196
1757.491463	171.442321	48.267201
1753.873698	175.594153	48.272205
1750.738018	163.125371	48.277210
1747.224811	161.625900	48.282215
1743.614480	161.579895	48.287220
1740.114616	165.735346	48.292225
1736.534675	174.367054	48.297229
1733.153536	165.138100	48.302234
1729.549742	171.402327	48.307239
1725.954207	172.745921	48.312244
1722.932169	169.965108	48.317249
1719.103630	178.315249	48.322253
1715.863816	168.103890	48.327258
1711.778166	172.220566	48.332263
1708.531068	165.275593	48.337268
1705.200634	171.506911	48.342273
1701.394160	176.518782	48.347277
1698.121128	164.850644	48.352282
1694.438697	172.788299	48.357287
1691.271590	169.640150	48.362292
1687.762815	170.235930	48.367297
1684.082697	168.108126	48.372301
1680.684016	151.715359	48.377306
1676.824055	164.786128	48.382311
1673.318755	165.922646	48.387316
1670.067014	165.475859	48.392321
1666.392151	160.080255	48.397325
1663.457522	157.961126	48.402330
1659.423566	157.643186	48.407335
1655.949795	161.506862	48.412340
1652.893974	164.844253	48.417345
1648.673200	158.892574	48.422349
1645.763745	153.101755	48.427354
1642.090895	160.179631	48.432359
1638.465071	152.837886	48.437364
1635.146528	167.239874	48.442369
1631.291380	167.095083	48.447373
1627.853337	153.041609	48.452378
1624.369445	164.783956	48.457383
1621.105819	159.048314	48.462388
1617.508876	156.647521	48.467393
1613.936721	161.856360	48.472397
1610.667429	159.708494	48.477402
1606.954028	171.780050	48.482407
1603.722817	156.917865	48.487412
1599.834016	158.613910	48.492417
1596.341243	158.757971	48.497421
1593.149509	156.739781	48.502426
1589.531376	156.802536	48.507431
1586.024576	164.872271	48.512436
1582.658770	163.775611	48.517441
1578.807874	157.622774	48.522445
1575.560985	156.270059	48.527450
1571.746744	160.719510	48.532455
1568.334924	160.849031	48.537460
1565.163992	163.733067	48.542465
1561.549701	167.202657	48.547469
1558.531827	163.856089	48.552474
1554.351486	157.924659	48.557479
1550.713850	161.016066	48.562484
1547.361058	157.516262	48.567489
1543.704640	159.651711	48.572493
1540.631911	151.718403	48.577498
1537.054125	163.392844	48.582503
1533.435724	160.676960	48.587508
1529.931302	159.406103	48.592513
1526.350032	165.494077	48.597517
1523.032370	156.443270	48.602522
1519.150745	156.652828	48.607527
1516.093172	157.378026	48.612532
1512.956791	147.378271	48.617537
1508.840347	153.986269	48.622541
1505.453930	153.403982	48.627546
1501.872913	155.931744	48.632551
1498.580777	154.258782	48.637556
1494.826391	150.254878	48.642561
1490.886427	159.423205	48.647565
1487.919153	155.052032	48.652570
1484.451769	170.277134	48.657575
1481.017414	148.772863	48.662580
1477.408300	148.470323	48.667585
1473.771603	149.776309	48.672589
1470.718786	148.405018	48.677594
1466.965862	155.913817	48.682599
1463.572895	150.528636	48.687604
1460.425873	149.814072	48.692609
1456.426825	155.929100	48.697613
1452.843820	145.292389	48.702618
1449.125098	155.807327	48.707623
1445.504371	158.753737	48.712628
1442.346967	148.425784	48.717633
1438.741277	141.323023	48.722637
1435.580711	147.123469	48.727642
1431.896757	146.623365	48.732647
1428.166460	141.290215	48.737652
1424.785385	145.737257	48.742657
1421.310102	153.170011	48.747661
1417.984508	150.681513	48.752666
1414.280289	148.362352	48.757671
1410.936656	155.841241	48.762676
1407.735757	146.480557	48.767681
1404.255508	157.503333	48.772685
1400.477967	149.947299	48.777690
1396.725075	155.387448	48.782695
1393.203453	145.407451	48.787700
1389.819456	147.220338	48.792705
1385.930222	150.967566	48.797709
1382.744159	144.526833	48.802714
1379.134670	146.517698	48.807719
1375.488773	147.325227	48.812724
1372.496011	143.774935	48.817729
1368.735871	149.079742	48.822733
1365.407141	146.490568	48.827738
1361.598871	143.122629	48.832743
1358.290673	138.455453	48.837748
1355.203355	142.188368	48.842753
1351.363526	155.557362	48.847757
1347.817164	141.125403	48.852762
1343.721433	149.665997	48.857767
1340.510544	150.166426	48.862772
1337.335515	144.089966	48.867777
1333.699609	148.273909	48.872781
1330.949391	151.329114	48.877786
1326.924447	149.655841	48.882791
1322.954030	148.352448	48.887796
1319.859899	150.846836	48.892801
1316.041640	155.459163	48.897805
1313.072738	145.759267	48.902810
1309.361130	154.846568	48.907815
1305.742009	146.208283	48.912820
1302.611828	144.761288	48.917825
1298.915998	152.408578	48.922829
1295.226719	148.956497	48.927834
1291.479218	146.250707	48.932839
1288.154406	143.677520	48.937844
1284.958003	148.366262	48.942849
1281.279292	155.741567	48.947853
1277.920129	143.439382	48.952858
1273.933868	149.271629	48.957863
1270.337259	148.256767	48.962868
1267.449912	139.607278	48.967873
1263.699511	148.934669	48.972877
1260.188485	145.246540	48.977882
1256.753518	149.081387	48.982887
1253.142556	152.065597	48.987892
1249.851917	148.369857	48.992897
1245.956237	149.648579	48.997901
1243.055892	146.964607	49.002906
1239.247890	146.719207	49.007911
1235.529526	154.351126	49.012916
1232.395864	138.389373	49.017921
1228.641402	145.242646	49.022925
1225.181924	139.653556	49.027930
1221.602853	139.460904	49.032935
1218.059570	137.215750	49.037940
1214.701515	140.405640	49.042945
1210.960274	151.365118	49.047949
1207.355854	141.893108	49.052954
1204.425170	137.285993	49.057959
1201.042254	129.852779	49.062964
1197.615432	138.594105	49.067969
1193.819701	146.083735	49.072973
1189.866891	143.247787	49.077978
1186.453387	148.707369	49.082983
1182.964923	146.680117	49.087988
1179.727456	136.863107	49.092993
1176.064222	145.861790	49.097997
1172.857557	138.397484	49.103002
1169.234595	139.845098	49.108007
1165.647211	138.821297	49.113012
1162.260787	133.233011	49.118017
1158.443483	148.241639	49.123021
1154.877394	133.059101	49.128026
1151.531634	137.596595	49.133031
1148.207462	146.763221	49.138036
1144.918143	137.400400	49.143041
1141.006656	132.633626	49.148045
1137.375796	138.823210	49.153050
1134.024500	144.766676	49.158055
1130.729929	139.013250	49.163060
1127.268731	137.377789	49.168065
1123.382478	132.041093	49.173069
1120.012938	138.439090	49.178074
1116.488473	134.461835	49.183079
1112.840184	141.437947	49.188084
1109.842174	133.671999	49.193089
1106.097233	138.363140	49.198093
1102.609888	140.078471	49.203098
1099.140622	142.088400	49.208103
1095.726295	143.140055	49.213108
1092.563428	134.954013	49.218113
1088.390710	144.259986	49.223117
1084.948470	130.505893	49.228122
1081.537373	136.484932	49.233127
1077.989961	141.736435	49.238132
1074.929133	134.200734	49.243137
1070.749905	137.032960	49.248141
1067.481539	135.963990	49.253146
1064.236843	132.648172	49.258151
1060.261575	135.153045	49.263156
1056.838126	133.550076	49.268161
1053.233091	136.091026	49.273165
1050.438553	137.742952	49.278170
1046.863951	132.877147	49.283175
1043.342017	134.740126	49.288180
1039.327503	132.784975	49.293185
1035.959794	134.477810	49.298189
1032.252338	127.333232	49.303194
1028.545457	138.727014	49.308199
1025.307579	141.754294	49.313204
1022.093139	135.964420	49.318209
1018.476419	139.193668	49.323213
1015.106707	135.116116	49.328218
1011.285149	138.354377	49.333223
1007.940689	145.734597	49.338228
1004.875304	137.854164	49.343233
1000.883044	140.952726	49.348237
997.480636	126.646886	49.353242
994.359323	131.851471	49.358247
990.500868	136.701582	49.363252
986.903773	138.013438	49.368257
983.257675	141.840373	49.373261
980.175742	136.696408	49.378266
976.621210	142.062435	49.383271
972.759093	143.965146	49.388276
969.459926	131.310939	49.393281
965.483871	144.009673	49.398285
962.660170	128.866571	49.403290
959.327860	139.957512	49.408295
955.416439	127.948034	49.413300
952.257130	136.244493	49.418305
948.269306	133.133746	49.423309
944.828865	133.640840	49.428314
941.384755	133.219480	49.433319
937.841244	134.554679	49.438324
934.501629	126.571061	49.443329
930.819823	134.236816	49.448333
927.453560	132.928588	49.453338
924.080245	133.083796	49.458343
920.152220	143.479985	49.463348
917.115557	134.233245	49.468353
913.452481	129.011587	49.473357
909.796297	137.399716	49.478362
906.168752	135.443640	49.483367
902.592062	136.230626	49.488372
899.313341	133.222486	49.493377
895.702066	132.162796	49.498381
892.504042	126.920092	49.503386
888.771900	142.301398	49.508391
885.928055	139.063278	49.513396
882.191098	128.859267	49.518401
878.319581	132.951881	49.523405
875.013774	128.460715	49.528410
871.130189	136.541536	49.533415
867.669834	137.535063	49.538420
864.241243	137.244597	49.543425
860.853674	136.896040	49.548429
857.402398	130.382562	49.553434
853.921454	132.626279	49.558439
850.207751	133.510167	49.563444
846.822229	127.738861	49.568449
843.264869	141.212051	49.573453
839.892120	129.619764	49.578458
836.358021	133.915511	49.583463
832.973354	135.925461	49.588468
829.526975	130.529702	49.593473
825.473005	133.090024	49.598477
822.320520	130.955395	49.603482
819.041883	136.508169	49.608487
815.327721	143.699048	49.613492
811.653232	140.994816	49.618497
807.954381	139.994478	49.623501
804.748143	130.187022	49.628506
801.630721	131.684512	49.633511
797.773411	132.028404	49.638516
794.352794	125.091360	49.643521
790.558017	137.855550	49.648525
787.438232	130.471708	49.653530
783.977638	124.851009	49.658535
780.331068	136.867848	49.663540
777.167839	123.823889	49.668545
773.368405	133.450813	49.673549
769.428828	134.811006	49.678554
766.445414	131.181648	49.683559
762.534849	130.556971	49.688564
759.226568	132.632486	49.693569
755.655303	136.467938	49.698573
752.184693	138.465326	49.703578
748.850617	128.879361	49.708583
745.176090	139.256839	49.713588
741.874912	131.067514	49.718593
738.291230	126.324049	49.723597
734.878309	126.980674	49.728602
731.637600	131.787220	49.733607
727.638479	139.245332	49.738612
724.424878	128.859386	49.743617
720.382715	127.318182	49.748621
716.855283	129.488193	49.753626
713.594794	123.527199	49.758631
709.829661	144.567381	49.763636
706.419843	126.599873	49.768641
703.208460	133.183536	49.773645
699.913135	130.164878	49.778650
696.371304	125.572790	49.783655
692.478764	131.939589	49.788660
689.300884	131.630477	49.793665
685.602350	140.000125	49.798669
682.122155	133.594785	49.803674
678.828531	130.205659	49.808679
674.912842	134.534463	49.813684
671.971648	135.319314	49.818689
668.302702	135.831665	49.823693
664.457443	132.952754	49.828698
661.319078	135.151192	49.833703
657.682917	134.938047	49.838708
654.126618	128.700431	49.843713
650.200162	133.658566	49.848717
647.143124	130.607829	49.853722
643.601024	127.244052	49.858727
640.035520	131.216774	49.863732
636.997478	126.924618	49.868737
632.927079	134.657647	49.873741
629.384805	130.230662	49.878746
626.243396	128.533221	49.883751
622.714977	124.652545	49.888756
619.495063	115.054325	49.893761
615.929465	119.596789	49.898765
612.248107	118.087952	49.903770
608.585964	124.311124	49.908775
604.964807	129.653911	49.913780
601.342376	133.834603	49.918785
597.905966	139.494342	49.923789
594.585727	127.363345	49.928794
591.103648	122.398561	49.933799
587.641527	131.398922	49.938804
584.008857	126.783281	49.943809
580.545392	133.703552	49.948813
577.236889	125.781590	49.953818
573.998037	122.903862	49.958823
569.952215	136.194997	49.963828
566.491390	126.391384	49.968833
562.833780	134.578326	49.973837
559.503104	128.214859	49.978842
556.254535	122.923949	49.983847
552.390542	125.564181	49.988852
549.146131	123.794052	49.993857
545.532285	125.544948	49.998861
541.817972	129.572757	50.003866
538.483235	127.568346	50.008871
535.290726	121.778785	50.013876
531.811387	124.884051	50.018881
528.054897	129.137697	50.023885
524.428001	130.485637	50.028890
521.088249	131.136043	50.033895
517.196269	136.169494	50.038900
513.942545	130.753174	50.043905
510.460859	129.567575	50.048909
507.107773	125.343432	50.053914
503.722411	124.759562	50.058919
500.085270	128.938030	50.063924
496.298846	126.373761	50.068929
492.800506	131.405440	50.073933
489.317188	127.084064	50.078938
486.171259	120.366064	50.083943
482.743411	135.092057	50.088948
479.028173	135.345230	50.093953
475.261395	134.642948	50.098957
471.554998	126.551495	50.103962
468.505594	132.401256	50.108967
465.150735	132.735507	50.113972
461.484204	125.302489	50.118977
457.847318	121.623426	50.123981
454.040982	132.523368	50.128986
450.947408	132.216858	50.133991
447.763307	136.163122	50.138996
444.166066	127.171144	50.144001
440.315073	134.246026	50.149005
436.471159	136.172824	50.154010
433.517013	129.046607	50.159015
430.221660	128.207545	50.164020
426.411043	126.806493	50.169025
422.941059	135.391499	50.174029
419.166751	131.287257	50.179034
416.055108	121.655105	50.184039
412.131674	130.662271	50.189044
409.291500	117.287719	50.194049
405.282238	129.055811	50.199053
401.803515	130.377160	50.204058
398.687492	125.934889	50.209063
395.063934	136.262744	50.214068
391.384796	126.160936	50.219073
387.930010	125.436106	50.224077
384.344082	123.459378	50.229082
381.182064	115.187148	50.234087
377.253567	125.696113	50.239092
373.900824	121.505571	50.244097
370.458531	126.408084	50.249101
366.683948	130.867126	50.254106
363.465128	125.548161	50.259111
359.765294	127.328239	50.264116
356.550000	118.143879	50.269121
352.777351	124.297724	50.274125
349.116523	116.969445	50.279130
345.776975	120.839284	50.284135
342.156830	122.715314	50.289140
338.681164	121.335471	50.294145
335.599294	120.360114	50.299149
332.119094	124.288171	50.304154
328.660578	121.729378	50.309159
324.698171	131.310801	50.314164
321.096714	127.798069	50.319169
317.742979	119.723777	50.324173
314.201770	129.218128	50.329178
310.732469	127.215844	50.334183
307.422959	123.525550	50.339188
303.981779	120.428734	50.344193
300.277804	120.333280	50.349197
296.615269	128.011518	50.354202
293.654550	113.831757	50.359207
289.726504	126.840760	50.364212
286.508069	119.439511	50.369217
282.827947	124.594972	50.374221
279.248023	125.965138	50.379226
276.112472	123.740892	50.384231
271.989292	135.123807	50.389236
268.930338	121.729139	50.394241
265.129090	118.262554	50.399245
261.389405	130.327530	50.404250
258.180482	116.684390	50.409255
254.389027	126.430762	50.414260
251.131249	118.669406	50.419265
248.329597	125.867341	50.424269
244.390011	124.159633	50.429274
240.672212	118.792927	50.434279
237.041568	130.167550	50.439284
233.749436	119.424630	50.444289
230.262555	128.281535	50.449293
226.680630	127.943742	50.454298
223.133171	117.744330	50.459303
219.739065	118.695626	50.464308
216.430131	123.515004	50.469313
212.876529	123.746188	50.474317
209.251743	119.777233	50.479322
206.085068	110.169172	50.484327
202.334082	122.744590	50.489332
198.830093	118.008931	50.494337
194.931930	117.024751	50.499341
191.153925	124.349812	50.504346
188.226282	106.339918	50.509351
184.751340	114.028424	50.514356
181.617474	114.593108	50.519361
178.192665	116.437725	50.524365
174.401669	113.129172	50.529370
170.288511	111.271287	50.534375
166.490456	126.284512	50.539380
163.173573	116.232086	50.544385
159.970018	123.968830	50.549389
156.675924	129.647756	50.554394
153.918316	119.960567	50.559399
149.920579	128.877436	50.564404
146.275305	117.986250	50.569409
142.686917	125.470190	50.574413
139.171974	120.471966	50.579418
135.827005	111.877000	50.584423
132.025139	121.985917	50.589428
128.613762	120.179425	50.594433
125.091208	126.034923	50.599437
121.435177	127.129314	50.604442
118.051555	118.933653	50.609447
114.168683	124.122422	50.614452
110.838829	123.114284	50.619457
107.925130	118.536722	50.624461
104.203957	118.145323	50.629466
100.748486	122.586088	50.634471
96.933067	130.107850	50.639476
93.516206	120.565374	50.644481
90.085283	122.679844	50.649485
86.344660	117.971029	50.654490
83.574917	121.041841	50.659495
79.722261	131.684323	50.664500
76.239671	120.248066	50.669505
72.681250	120.851155	50.674509
69.202975	121.961152	50.679514
65.644452	123.901406	50.684519
61.710609	117.159495	50.689524
58.638835	127.309800	50.694529
55.072396	119.516637	50.699533
51.256089	123.700265	50.704538
48.304973	120.612112	50.709543
44.368128	123.504413	50.714548
41.244993	117.473474	50.719553
37.795644	120.170016	50.724557
33.827843	117.264818	50.729562
30.601409	113.313933	50.734567
27.004128	130.767415	50.739572
23.529637	113.814358	50.744577
20.160026	116.436142	50.749581
16.549574	136.916963	50.754586
12.857486	121.698797	50.759591
9.198002	131.039695	50.764596
6.028843	116.774118	50.769601
2.597916	122.367474	50.774605