Tue Jun 21 12:39:39 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
1.097960	110.743725	0.000000
0.564387	117.445284	0.005005
0.682454	92.489876	0.010010
0.710083	90.775328	0.015014
0.268865	96.581868	0.020019
0.421453	80.689467	0.025024
-0.080622	83.138571	0.030029
0.255163	70.942109	0.035034
-0.306417	59.992610	0.040038
-0.784171	55.320637	0.045043
-0.717891	43.946121	0.050048
-1.465988	40.091874	0.055053
-1.878234	28.858373	0.060058
-1.423005	28.411145	0.065062
-1.921307	21.955729	0.070067
-2.607613	14.299692	0.075072
-2.918129	27.600995	0.080077
-2.838324	9.795731	0.085082
-3.734766	24.889344	0.090086
-4.259250	24.234739	0.095091
-4.065798	20.251821	0.100096
-4.453980	26.262673	0.105101
-4.267915	26.760645	0.110106
-4.293477	26.373297	0.115110
-4.491403	26.657403	0.120115
-5.126406	15.435540	0.125120
-5.684494	24.153129	0.130125
-6.207793	24.270495	0.135130
-6.133655	23.358898	0.140134
-6.211781	25.907499	0.145139
-5.808099	28.115641	0.150144
-6.578755	33.546917	0.155149
-6.839573	18.860862	0.160154
-7.125243	25.849300	0.165158
-7.221886	24.493764	0.170163
-7.964575	19.201449	0.175168
-8.446434	19.503563	0.180173
-8.754554	24.715770	0.185178
-8.735560	21.060503	0.190182
-8.856104	20.123522	0.195187
-8.623290	17.538706	0.200192
-9.293450	29.245909	0.205197
-9.363469	25.586436	0.210202
-9.225008	24.054625	0.215206
-9.945651	26.601284	0.220211
-10.478477	19.119731	0.225216
-10.491824	23.876423	0.230221
-10.485375	23.887913	0.235226
-10.487241	17.640376	0.240230
-11.629945	25.273930	0.245235
-11.909546	21.481824	0.250240
-12.065532	24.071931	0.255245
-12.184073	17.867987	0.260250
-11.718258	18.277800	0.265254
-12.280814	21.973007	0.270259
-12.316771	25.511554	0.275264
-13.274551	28.469455	0.280269
-13.391403	17.469238	0.285274
-13.280495	19.966210	0.290278
-13.774328	26.608659	0.295283
-13.578684	19.608346	0.300288
-14.402310	20.656735	0.305293
-14.929206	17.635516	0.310298
-15.096097	15.659358	0.315302
-15.192658	33.042596	0.320307
-14.993323	21.405911	0.325312
-15.246179	23.120704	0.330317
-15.496311	24.544176	0.335322
-15.945439	23.224709	0.340326
-16.758764	32.652938	0.345331
-17.018488	20.808701	0.350336
-17.008959	26.060661	0.355341
-16.989151	19.892217	0.360346
-16.679278	22.936995	0.365350
-17.114359	31.339207	0.370355
-17.232495	16.536783	0.375360
-17.769906	16.996492	0.380365
-18.360845	18.983940	0.385370
-18.263376	14.354469	0.390374
-19.170191	20.039563	0.395379
-19.311299	16.715491	0.400384
-19.990556	14.466214	0.405389
-19.315096	21.898742	0.410394
-19.428930	26.467044	0.415398
-19.978037	25.803495	0.420403
-19.670745	25.720373	0.425408
-20.359724	12.637127	0.430413
-20.864454	13.449585	0.435418
-21.221862	10.922644	0.440422
-21.682418	18.631494	0.445427
-21.392429	13.441488	0.450432
-21.854382	18.155838	0.455437
-21.802149	22.300394	0.460442
-22.021837	19.475169	0.465446
-22.843368	23.165113	0.470451
-22.428338	16.428814	0.475456
-22.649973	18.793584	0.480461
-22.855418	20.914925	0.485466
-23.882768	19.756725	0.490470
-24.554198	25.489275	0.495475
-24.170054	21.442219	0.500480
-24.866610	18.589401	0.505485
-24.646994	22.544623	0.510490
-24.354795	20.709706	0.515494
-24.783983	21.491303	0.520499
-24.557745	21.805811	0.525504
-25.939963	17.622646	0.530509
-26.249483	17.654490	0.535514
-26.462353	19.208347	0.540518
-26.451402	22.304794	0.545523
-26.092750	22.680058	0.550528
-26.261187	23.702242	0.555533
-26.776515	22.703948	0.560538
-27.108445	19.622227	0.565542
-27.806144	28.105419	0.570547
-27.783008	17.213644	0.575552
-27.698854	26.677956	0.580557
-28.115396	21.095034	0.585562
-28.705978	19.081095	0.590566
-29.208239	16.511048	0.595571
-29.259580	19.076327	0.600576
-29.400063	29.199440	0.605581
-29.557985	31.871763	0.610586
-29.540265	27.586817	0.615590
-29.685746	33.138543	0.620595
-30.337916	22.188688	0.625600
-30.843656	24.896702	0.630605
-31.292985	22.985665	0.635610
-31.391191	22.420512	0.640614
-31.555613	27.913805	0.645619
-31.292368	25.511020	0.650624
-30.880405	16.999030	0.655629
-31.482438	15.732119	0.660634
-31.963957	16.579609	0.665638
-32.657184	25.668069	0.670643
-32.365890	20.389439	0.675648
-33.188166	21.768141	0.680653
-33.884401	20.403165	0.685658
-33.684856	22.156509	0.690662
-34.322803	26.747863	0.695667
-34.262033	22.425993	0.700672
-34.071741	19.984772	0.705677
-34.219306	19.113045	0.710682
-34.276609	13.139514	0.715686
-35.477728	25.160388	0.720691
-35.580247	21.867814	0.725696
-35.759445	26.426812	0.730701
-35.810650	27.831946	0.735706
-35.724521	27.267644	0.740710
-35.957627	27.224873	0.745715
-36.394004	21.049092	0.750720
-36.991254	22.791513	0.755725
-37.040185	28.739282	0.760730
-37.433963	23.531471	0.765734
-37.791658	22.771897	0.770739
-37.464747	20.074409	0.775744
-38.066399	23.699331	0.780749
-38.740095	24.961867	0.785754
-38.565350	24.339871	0.790758
-39.341602	24.734942	0.795763
-39.199995	19.676459	0.800768
-39.350702	22.934850	0.805773
-39.304706	31.727248	0.810778
-39.269686	22.959574	0.815782
-40.186752	21.658992	0.820787
-40.701047	22.993404	0.825792
-40.925272	29.957855	0.830797
-41.427722	25.172574	0.835802
-41.431057	16.679234	0.840806
-41.437186	21.367042	0.845811
-41.251527	25.294537	0.850816
-41.739399	27.820021	0.855821
-41.569625	29.612237	0.860826
-42.208398	20.482147	0.865830
-42.779042	26.999579	0.870835
-43.405026	22.464452	0.875840
-42.957916	25.840715	0.880845
-43.039816	31.576483	0.885850
-43.013795	28.453839	0.890854
-43.695232	29.652143	0.895859
-43.999616	22.590777	0.900864
-44.251758	23.289383	0.905869
-44.304796	28.113623	0.910874
-44.673968	22.396762	0.915878
-45.488299	31.641047	0.920883
-45.540986	26.986316	0.925888
-45.743963	24.773216	0.930893
-45.801254	20.704145	0.935898
-46.040047	22.270978	0.940902
-46.006788	16.488070	0.945907
-46.166447	20.217399	0.950912
-47.091052	22.407118	0.955917
-46.882317	27.787507	0.960922
-47.189719	24.348499	0.965926
-47.284381	32.807806	0.970931
-47.683189	29.826750	0.975936
-48.211505	23.682574	0.980941
-48.600917	18.289735	0.985946
-48.339365	17.133983	0.990950
-48.955702	23.895780	0.995955
-48.456544	17.088125	1.000960
-49.394133	22.356027	1.005965
-50.182491	19.440667	1.010970
-50.459605	12.936006	1.015974
-50.374312	24.810158	1.020979
-50.641473	24.633907	1.025984
-50.864970	19.970957	1.030989
-50.889118	17.770474	1.035994
-50.474859	21.685370	1.040998
-50.587996	22.032594	1.046003
-51.654819	24.062346	1.051008
-51.824023	25.008093	1.056013
-52.016362	22.983067	1.061018
-52.022512	18.436664	1.066022
-52.621235	25.370383	1.071027
-53.230194	14.266370	1.076032
-53.397955	15.583456	1.081037
-53.620597	16.978894	1.086042
-53.633125	8.036767	1.091046
-53.781605	29.347434	1.096051
-53.528386	23.550397	1.101056
-54.304605	20.166334	1.106061
-54.675353	26.136412	1.111066
-54.860580	25.801750	1.116070
-55.208872	35.453316	1.121075
-55.018165	18.607670	1.126080
-55.169842	21.438205	1.131085
-56.419871	24.396164	1.136090
-56.316751	29.385563	1.141094
-57.014233	32.289909	1.146099
-56.769654	22.003980	1.151104
-56.952716	29.255641	1.156109
-57.148153	28.099395	1.161114
-57.036911	23.975577	1.166118
-57.114918	25.740942	1.171123
-57.463686	15.990370	1.176128
-58.293230	20.899389	1.181133
-58.463426	21.121086	1.186138
-58.244784	14.982867	1.191142
-58.567161	15.733952	1.196147
-59.342604	15.042770	1.201152
-59.689895	27.344548	1.206157
-59.917137	23.261195	1.211162
-60.069161	24.067937	1.216166
-60.393380	33.045962	1.221171
-59.795912	14.623557	1.226176
-60.189488	21.012011	1.231181
-60.933450	24.074224	1.236186
-61.079605	13.753355	1.241190
-61.550024	23.470918	1.246195
-61.397036	13.922798	1.251200
-61.682875	19.069352	1.256205
-61.988400	22.411988	1.261210
-62.554768	18.078535	1.266214
-62.957467	19.769402	1.271219
-63.019431	17.357721	1.276224
-62.787999	23.463889	1.281229
-63.214096	18.432919	1.286234
-63.326539	10.394549	1.291238
-64.276706	18.230065	1.296243
-64.185883	17.560201	1.301248
-64.566667	26.628496	1.306253
-64.585010	15.317750	1.311258
-64.679241	18.025896	1.316262
-64.851360	16.378377	1.321267
-65.337860	14.373256	1.326272
-65.788257	15.816673	1.331277
-66.522258	14.367579	1.336282
-66.254140	23.349724	1.341286
-66.663223	22.584454	1.346291
-66.474006	20.757906	1.351296
-66.194932	21.767155	1.356301
-66.934018	24.191176	1.361306
-67.301333	17.334216	1.366310
-67.711807	24.111848	1.371315
-67.641151	15.337293	1.376320
-67.812301	11.905720	1.381325
-68.456869	18.737115	1.386330
-68.836778	16.909900	1.391334
-69.171011	25.110901	1.396339
-69.176905	16.024804	1.401344
-69.542989	13.061620	1.406349
-69.272141	14.065916	1.411354
-69.356738	13.043263	1.416358
-70.087705	20.759008	1.421363
-70.630838	17.044493	1.426368
-70.917100	19.021551	1.431373
-70.667760	14.909399	1.436378
-71.064959	16.283820	1.441382
-71.542203	25.840702	1.446387
-71.936366	13.990723	1.451392
-72.423184	14.096333	1.456397
-72.563840	23.254705	1.461402
-72.686019	12.725824	1.466406
-72.863297	13.476561	1.471411
-72.626412	5.548472	1.476416
-72.605465	11.705279	1.481421
-73.045627	22.590385	1.486426
-73.327319	20.205225	1.491430
-74.204191	30.168295	1.496435
-73.875489	23.693547	1.501440
-74.046805	15.093843	1.506445
-74.604850	18.976761	1.511450
-75.138108	27.797593	1.516454
-75.476168	22.327580	1.521459
-75.611117	15.175805	1.526464
-75.540733	24.380530	1.531469
-75.750725	20.390226	1.536474
-75.962690	20.667780	1.541478
-76.414621	26.076471	1.546483
-76.857594	17.595557	1.551488
-77.162497	27.065685	1.556493
-77.566607	20.085763	1.561498
-77.329698	22.015845	1.566502
-77.756019	33.992289	1.571507
-77.637402	17.077680	1.576512
-77.360139	14.092216	1.581517
-78.216520	14.764793	1.586522
-78.717150	19.851211	1.591526
-78.909446	26.114969	1.596531
-79.035631	27.411950	1.601536
-79.306789	27.611691	1.606541
-80.135086	24.084113	1.611546
-80.161216	19.783148	1.616550
-80.500121	24.234406	1.621555
-80.614173	21.526668	1.626560
-80.864607	29.944280	1.631565
-81.010376	27.053340	1.636570
-80.680131	18.220600	1.641574
-81.063820	16.092881	1.646579
-81.846895	14.662178	1.651584
-82.093625	18.107952	1.656589
-82.413545	24.788696	1.661594
-82.120517	12.601930	1.666598
-82.223861	20.186901	1.671603
-82.751965	12.610061	1.676608
-83.400406	13.574789	1.681613
-83.967366	26.219994	1.686618
-83.757899	20.518215	1.691622
-83.904770	16.426095	1.696627
-83.908901	15.213108	1.701632
-83.994269	21.760484	1.706637
-85.036891	17.471176	1.711642
-85.409965	9.815976	1.716646
-85.813623	15.598313	1.721651
-85.496663	16.018758	1.726656
-85.465997	18.628274	1.731661
-85.807734	17.163357	1.736666
-85.685348	10.503742	1.741670
-85.914562	10.739556	1.746675
-86.395235	9.901094	1.751680
-86.901944	11.137758	1.756685
-87.069137	16.436342	1.761690
-87.038496	6.304650	1.766694
-88.494445	13.984564	1.771699
-88.658059	13.544501	1.776704
-88.056390	12.566853	1.781709
-88.459494	14.004018	1.786714
-88.552140	8.262095	1.791718
-88.999645	21.391107	1.796723
-88.747864	18.333100	1.801728
-89.376287	17.434056	1.806733
-89.926318	13.724239	1.811738
-89.955397	3.990791	1.816742
-90.137895	8.525466	1.821747
-90.145498	13.531614	1.826752
-90.488377	12.534370	1.831757
-90.971083	17.672087	1.836762
-91.302173	14.786779	1.841766
-91.866475	23.445609	1.846771
-91.704456	13.590721	1.851776
-91.933433	14.119338	1.856781
-92.223962	20.059751	1.861786
-91.959784	18.016944	1.866790
-92.755552	14.812346	1.871795
-93.307175	18.322822	1.876800
-93.234172	19.074537	1.881805
-93.527785	18.831235	1.886810
-93.740371	18.806184	1.891814
-93.929872	16.706494	1.896819
-93.982652	7.107999	1.901824
-94.734659	18.431717	1.906829
-95.266819	23.767855	1.911834
-95.351494	9.787132	1.916838
-95.439573	16.298053	1.921843
-95.399029	10.326082	1.926848
-95.450542	14.140901	1.931853
-95.458471	16.766083	1.936858
-95.493301	8.402288	1.941862
-96.472093	26.021793	1.946867
-96.796903	15.235011	1.951872
-97.148824	18.376158	1.956877
-97.143298	5.726708	1.961882
-97.342177	12.091796	1.966886
-98.041826	16.939644	1.971891
-98.260847	15.174390	1.976896
-98.545953	13.873355	1.981901
-98.439205	20.671100	1.986906
-98.257563	10.782969	1.991910
-98.865205	19.020564	1.996915
-98.676170	16.778013	2.006912
-99.117915	14.800086	2.016909
-98.940284	15.355972	2.026906
-98.083415	25.939677	2.036902
-97.236687	19.270869	2.046899
-96.974452	16.382059	2.056896
-96.172964	18.775317	2.066893
-95.931981	18.981457	2.076890
-95.828894	15.741812	2.086886
-95.025687	18.417729	2.096883
-94.388847	22.404716	2.106880
-93.941383	21.623703	2.116877
-93.180795	16.278565	2.126874
-92.916549	22.507618	2.136870
-92.698221	23.462211	2.146867
-91.626477	20.707068	2.156864
-91.315391	20.580323	2.166861
-91.178181	22.259265	2.176858
-90.347891	20.716387	2.186854
-89.848128	15.557694	2.196851
-89.507715	20.258648	2.206848
-88.699097	13.182608	2.216845
-88.300561	21.303238	2.226842
-88.213132	22.923047	2.236838
-87.320827	25.320038	2.246835
-86.714606	27.444714	2.256832
-86.673373	28.688857	2.266829
-85.808614	29.970691	2.276826
-85.197259	26.243203	2.286822
-84.935598	26.171472	2.296819
-84.761008	27.198118	2.306816
-84.052787	23.532240	2.316813
-83.369152	24.493750	2.326810
-82.278624	28.552413	2.336806
-81.983262	21.249183	2.346803
-82.003188	20.475827	2.356800
-81.850900	26.510031	2.366797
-81.127919	18.410054	2.376794
-80.521159	22.630237	2.386790
-79.675946	23.506899	2.396787
-79.042884	19.871845	2.406784
-79.097155	20.275071	2.416781
-78.650157	19.940089	2.426778
-77.744767	27.218056	2.436774
-77.705494	21.838847	2.446771
-76.470441	23.539099	2.456768
-76.036564	18.463435	2.466765
-75.993136	19.905196	2.476762
-75.793629	27.976794	2.486758
-74.799479	20.112482	2.496755
-74.703705	19.335772	2.506752
-73.720801	21.482437	2.516749
-73.129304	25.515665	2.526746
-73.047002	17.640143	2.536742
-72.373219	18.882277	2.546739
-71.529206	22.597659	2.556736
-71.487553	20.971598	2.566733
-70.999829	21.980570	2.576730
-69.983501	22.142680	2.586726
-69.841105	20.787028	2.596723
-69.576076	24.924903	2.606720
-68.724914	21.988752	2.616717
-68.314170	26.401444	2.626714
-67.946264	21.823360	2.636710
-67.208973	19.322776	2.646707
-66.949185	24.050127	2.656704
-66.589395	26.015263	2.666701
-65.624546	15.921504	2.676698
-65.274340	20.575198	2.686694
-65.273972	14.643068	2.696691
-63.803247	18.021317	2.706688
-63.652930	23.868339	2.716685
-63.693433	22.918192	2.726682
-63.279234	22.112855	2.736678
-62.128983	21.296275	2.746675
-61.852019	23.684131	2.756672
-61.079780	24.898700	2.766669
-60.782378	20.316090	2.776666
-60.673599	19.680674	2.786662
-59.477522	19.518617	2.796659
-59.067895	23.098472	2.806656
-59.330078	23.709608	2.816653
-58.440427	30.037627	2.826650
-57.519723	23.555146	2.836646
-57.309832	25.204863	2.846643
-57.008449	24.838672	2.856640
-56.190304	23.075922	2.866637
-56.123086	29.748392	2.876634
-55.288673	27.017938	2.886630
-54.752999	27.109087	2.896627
-54.694923	27.800362	2.906624
-53.526900	27.017197	2.916621
-52.898723	19.412265	2.926618
-52.831835	22.430039	2.936614
-52.759254	24.818745	2.946611
-51.306462	23.538124	2.956608
-51.096974	21.012519	2.966605
-51.030855	21.675393	2.976602
-50.428929	24.424169	2.986598
-49.902419	24.667002	2.996595
-49.527814	22.797110	3.006592
-48.356969	18.751728	3.016589
-48.237002	21.334124	3.026586
-48.186375	23.075222	3.036582
-47.130055	19.159256	3.046579
-46.391143	22.337820	3.056576
-46.360131	22.766045	3.066573
-46.111404	22.544119	3.076570
-45.127260	22.424275	3.086566
-44.882836	20.726304	3.096563
-44.538439	19.209956	3.106560
-43.580129	13.451136	3.116557
-43.301540	11.823381	3.126554
-42.619479	13.819323	3.136550
-42.119394	15.102871	3.146547
-41.630870	17.266209	3.156544
-41.690705	21.281833	3.166541
-40.559409	22.209723	3.176538
-40.416973	12.512775	3.186534
-40.016715	18.839640	3.196531
-38.986923	16.798419	3.206528
-38.634942	14.367969	3.216525
-38.407574	12.289902	3.226522
-37.713058	18.160814	3.236518
-36.762337	15.320412	3.246515
-36.767944	15.242163	3.256512
-36.675794	16.466809	3.266509
-35.826584	19.298327	3.276506
-35.468500	22.667202	3.286502
-34.427910	19.347195	3.296499
-33.718931	15.808249	3.306496
-33.721653	15.836613	3.316493
-33.648502	13.215036	3.326490
-33.065901	22.619538	3.336486
-32.234964	21.806644	3.346483
-31.796513	21.489482	3.356480
-30.679013	16.862156	3.366477
-30.816795	18.665474	3.376474
-30.290492	16.753668	3.386470
-30.176048	21.642216	3.396467
-29.078974	19.182829	3.406464
-28.936493	18.389098	3.416461
-28.027692	18.342986	3.426458
-27.501611	23.179967	3.436454
-27.247911	18.665254	3.446451
-27.062818	17.307867	3.456448
-26.079988	14.224059	3.466445
-25.802157	19.867596	3.476442
-25.498914	13.247305	3.486438
-24.595586	18.641247	3.496435
-24.410616	17.794444	3.506432
-23.972006	18.866286	3.516429
-23.057870	22.616896	3.526426
-23.085408	22.806253	3.536422
-21.835145	20.303124	3.546419
-21.508484	17.250124	3.556416
-21.466502	13.542638	3.566413
-20.750061	22.459271	3.576410
-19.584466	27.308117	3.586406
-19.489228	21.309887	3.596403
-19.584984	18.940538	3.606400
-18.986695	11.049716	3.616397
-18.536157	17.111198	3.626394
-17.716003	26.022515	3.636390
-16.719825	18.796672	3.646387
-16.507151	21.746443	3.656384
-16.511729	21.386660	3.666381
-15.818377	25.637370	3.676378
-14.941127	16.221814	3.686374
-15.075468	20.151576	3.696371
-14.105557	15.626148	3.706368
-13.168728	14.834845	3.716365
-12.992346	20.297202	3.726362
-12.895116	17.686455	3.736358
-12.569038	17.302545	3.746355
-11.543483	18.093638	3.756352
-11.228955	15.211979	3.766349
-10.894468	14.412932	3.776346
-10.151529	12.369032	3.786342
-9.611143	13.857723	3.796339
-9.201767	21.518964	3.806336
-8.466971	21.264763	3.816333
-8.276002	17.114315	3.826330
-7.743414	18.904827	3.836326
-7.049046	19.430475	3.846323
-6.580723	16.194171	3.856320
-6.506374	23.613325	3.866317
-5.412649	21.339043	3.876314
-5.150075	22.309038	3.886310
-4.920466	26.822864	3.896307
-4.005416	30.302834	3.906304
-3.423095	23.007014	3.916301
-3.422896	29.169946	3.926298
-3.007499	27.732536	3.936294
-2.489415	39.682771	3.946291
-2.273481	46.360858	3.956288
-1.886143	52.558487	3.966285
-1.140096	72.106932	3.976282
-0.659183	93.021952	3.986278
-0.128604	113.255003	3.996275
0.000000	117.074222	4.001280
0.234509	134.631270	4.006285
0.713882	137.561573	4.011290
0.748857	151.245040	4.016294
0.880457	153.726965	4.021299
1.132478	148.268313	4.026304
0.874244	161.612380	4.031309
1.145778	150.559792	4.036314
1.010213	159.588349	4.041318
0.920950	158.869958	4.046323
1.285603	155.353573	4.051328
0.962220	164.168538	4.056333
0.784183	158.600927	4.061338
0.825676	158.573265	4.066342
1.294257	177.857950	4.071347
1.445114	168.424538	4.076352
1.021228	162.033701	4.081357
1.183532	152.835206	4.086362
0.969918	156.743998	4.091366
1.217865	180.150455	4.096371
1.367088	179.264502	4.101376
1.511198	181.331535	4.106381
1.556330	163.006726	4.111386
1.259647	162.370041	4.116390
0.923888	162.449445	4.121395
1.353588	166.492662	4.126400
1.192975	169.363775	4.131405
1.377978	176.592645	4.136410
1.403397	179.824469	4.141414
1.251794	173.837479	4.146419
1.294816	181.721335	4.151424
1.060014	180.018264	4.156429
1.257055	180.192964	4.161434
1.530705	178.721042	4.166438
1.321750	183.881361	4.171443
1.852852	177.796912	4.176448
1.263983	186.456541	4.181453
1.559975	185.012097	4.186458
1.749915	174.853316	4.191462
1.502650	182.443061	4.196467
1.822159	183.084112	4.201472
1.575278	167.077998	4.206477
1.273411	163.429848	4.211482
1.506355	168.337414	4.216486
1.716363	176.036735	4.221491
1.523629	167.484685	4.226496
1.271014	175.190358	4.231501
1.502363	170.689633	4.236506
1.803697	174.896387	4.241510
1.580962	188.789506	4.246515
1.822275	182.615497	4.251520
1.533369	185.536866	4.256525
1.614364	180.313922	4.261530
1.892341	188.587291	4.266534
1.507338	188.485209	4.271539
1.654364	185.814522	4.276544
1.568825	188.084161	4.281549
1.231068	193.426639	4.286554
1.339865	192.744913	4.291558
1.161299	203.320426	4.296563
1.666203	186.428879	4.301568
1.643072	200.254818	4.306573
1.456550	190.283475	4.311578
1.866893	180.507138	4.316582
1.579213	196.274458	4.321587
1.871236	184.544156	4.326592
1.682012	197.522412	4.331597
1.634373	187.754812	4.336602
1.878066	192.358288	4.341606
1.862032	201.823712	4.346611
2.135171	202.086059	4.351616
1.930510	189.871841	4.356621
1.640098	193.157150	4.361626
1.976479	195.722983	4.366630
1.894231	203.871302	4.371635
1.891192	211.228415	4.376640
2.273706	215.811082	4.381645
2.141569	202.383464	4.386650
1.899671	195.448024	4.391654
1.833368	197.338751	4.396659
1.857348	193.162441	4.401664
1.792296	195.392773	4.406669
2.224062	218.683009	4.411674
2.247735	207.300825	4.416678
1.981103	196.608457	4.421683
1.995368	182.221243	4.426688
1.824660	205.820594	4.431693
2.200038	215.142673	4.436698
2.204295	210.166861	4.441702
2.459376	219.891300	4.446707
2.221289	199.190060	4.451712
2.047084	194.846467	4.456717
2.013925	198.935355	4.461722
2.214615	186.552588	4.466726
1.829771	195.797283	4.471731
2.124327	202.603881	4.476736
2.385550	214.528581	4.481741
2.259129	218.009729	4.486746
2.164707	212.642560	4.491750
2.106948	203.504549	4.496755
2.095536	213.957867	4.501760
2.274411	221.842731	4.506765
2.472232	219.880549	4.511770
2.510871	218.425041	4.516774
1.689358	220.632832	4.521779
2.144193	213.123998	4.526784
2.191373	222.698157	4.531789
2.111524	220.181460	4.536794
2.469706	219.760954	4.541798
2.297780	221.232075	4.546803
2.209647	217.843143	4.551808
2.078262	231.083779	4.556813
2.086303	222.929829	4.561818
2.228762	222.066307	4.566822
2.260914	221.807926	4.571827
2.564221	218.873171	4.576832
2.161034	222.028960	4.581837
2.200450	222.911164	4.586842
2.451970	230.359928	4.591846
2.313162	251.331666	4.596851
2.635976	243.770084	4.601856
2.575003	260.277237	4.606861
2.857950	247.597820	4.611866
2.630834	234.884867	4.616870
2.260955	234.878357	4.621875
2.360167	231.780256	4.626880
2.594410	248.465646	4.631885
2.639684	255.494897	4.636890
2.648066	248.423663	4.641894
2.563600	255.778296	4.646899
2.565427	253.843630	4.651904
2.363865	258.027908	4.656909
2.416929	254.851207	4.661914
2.720938	245.419226	4.666918
2.766827	253.435057	4.671923
3.060171	250.892868	4.676928
2.787297	253.493291	4.681933
2.797818	248.294031	4.686938
2.776202	248.638339	4.691942
2.448339	251.771992	4.696947
2.925729	242.693741	4.701952
2.531212	258.921046	4.706957
2.949531	253.684253	4.711962
3.111859	252.442697	4.716966
2.437205	247.879637	4.721971
2.595047	247.680760	4.726976
2.786448	251.609537	4.731981
2.821246	255.653639	4.736986
3.112724	248.908297	4.741990
2.778249	256.625986	4.746995
3.032276	251.007716	4.752000
2.817598	248.534849	4.757005
2.777116	252.852295	4.762010
3.041884	247.900823	4.767014
3.091006	251.976494	4.772019
2.981393	252.685646	4.777024
2.842832	252.186366	4.782029
2.874565	250.966829	4.787034
3.008001	250.669576	4.792038
2.607632	255.626586	4.797043
2.745778	246.275943	4.802048
2.701445	253.551901	4.807053
3.043700	251.694462	4.812058
3.037303	253.590472	4.817062
2.798165	253.658218	4.822067
2.785081	251.303919	4.827072
2.876741	256.131503	4.832077
2.712946	251.355583	4.837082
2.965129	252.687017	4.842086
2.825265	269.185141	4.847091
3.097501	273.374836	4.852096
3.328388	284.599726	4.857101
3.322025	278.774339	4.862106
3.347022	269.540889	4.867110
3.226298	264.709879	4.872115
3.084066	247.079244	4.877120
3.240737	262.399692	4.882125
2.979885	258.610144	4.887130
3.327481	273.273234	4.892134
3.258676	280.549902	4.897139
3.232910	279.830069	4.902144
3.350760	278.858333	4.907149
3.286139	275.961008	4.912154
3.470616	264.812245	4.917158
2.922472	264.177530	4.922163
3.254000	271.541630	4.927168
3.535880	287.330370	4.932173
3.334332	272.313191	4.937178
3.475688	268.966563	4.942182
3.334767	272.043217	4.947187
3.411636	262.844595	4.952192
3.238629	270.747296	4.957197
3.466048	277.958732	4.962202
3.778491	273.649779	4.967206
3.233981	268.465457	4.972211
3.488480	255.421330	4.977216
2.968270	267.118286	4.982221
3.353661	277.255127	4.987226
3.524816	271.588213	4.992230
3.471287	291.199851	4.997235
3.557784	283.074912	5.002240
3.594160	282.170540	5.007245
3.770262	288.187314	5.012250
3.871368	281.901110	5.017254
3.256108	274.600421	5.022259
3.450558	271.674998	5.027264
3.862260	287.334101	5.032269
3.744347	282.399018	5.037274
3.644579	259.878830	5.042278
3.294909	266.964999	5.047283
3.709189	272.326836	5.052288
3.695464	284.686462	5.057293
3.779276	282.228102	5.062298
3.725496	259.389099	5.067302
3.436402	255.559434	5.072307
3.897118	272.706808	5.077312
3.603875	261.738385	5.082317
3.582432	273.327300	5.087322
3.544558	267.939894	5.092326
3.502976	288.946695	5.097331
3.808991	291.499812	5.102336
3.996051	286.985863	5.107341
4.028066	284.380381	5.112346
4.027979	278.953562	5.117350
3.657883	276.393944	5.122355
3.618270	268.207605	5.127360
3.711456	282.551113	5.132365
3.645743	292.174991	5.137370
3.939249	288.111105	5.142374
3.795135	283.239956	5.147379
4.011898	288.059071	5.152384
3.662827	293.597834	5.157389
3.446517	284.966544	5.162394
3.731613	285.014381	5.167398
3.363990	295.330388	5.172403
3.810963	292.069509	5.177408
3.709914	290.668107	5.182413
3.561785	282.611027	5.187418
3.814305	293.342354	5.192422
3.778618	316.603777	5.197427
4.015583	305.836627	5.202432
4.165787	317.850831	5.207437
3.896718	321.713987	5.212442
4.346497	318.678787	5.217446
4.100119	320.444833	5.222451
4.118637	317.192734	5.227456
4.109988	310.035293	5.232461
3.941078	312.688763	5.237466
4.294724	306.361520	5.242470
3.984351	305.685063	5.247475
3.882000	310.410601	5.252480
4.340425	310.256870	5.257485
3.917911	309.128333	5.262490
3.935353	308.785559	5.267494
4.247840	320.391440	5.272499
4.427285	313.992595	5.277504
4.309014	328.776096	5.282509
4.018157	311.954611	5.287514
4.461989	311.856775	5.292518
4.319335	316.279563	5.297523
4.208819	315.158170	5.302528
4.277147	308.353452	5.307533
4.204553	318.814603	5.312538
4.587306	315.052461	5.317542
4.330854	319.935340	5.322547
4.362482	307.048451	5.327552
4.435910	299.867360	5.332557
4.143157	297.744663	5.337562
4.294579	302.479879	5.342566
4.265528	313.769540	5.347571
4.426786	318.945168	5.352576
4.319112	316.394187	5.357581
4.238300	318.210765	5.362586
4.624835	310.316545	5.367590
4.191620	313.255123	5.372595
4.432999	317.535782	5.377600
4.303614	329.021644	5.382605
4.106656	322.071404	5.387610
4.147814	314.562149	5.392614
4.391644	320.882672	5.397619
4.329463	320.040598	5.402624
4.170643	320.190950	5.407629
4.398521	323.191745	5.412634
4.681937	311.724245	5.417638
4.299061	322.453651	5.422643
4.310441	314.994517	5.427648
4.518725	319.876220	5.432653
4.575094	335.984938	5.437658
4.923476	333.162087	5.442662
4.502339	339.853805	5.447667
4.662612	320.630407	5.452672
4.673014	320.727480	5.457677
4.321139	320.603137	5.462682
4.867648	315.162166	5.467686
4.537294	330.054196	5.472691
4.773580	334.381287	5.477696
4.866643	344.436532	5.482701
4.733209	337.764668	5.487706
4.716189	320.917169	5.492710
4.241322	328.792528	5.497715
4.745758	337.873280	5.502720
4.884148	345.096332	5.507725
4.463394	355.362764	5.512730
5.013784	357.145672	5.517734
4.692475	361.529777	5.522739
5.001012	358.986437	5.527744
4.997819	350.274631	5.532749
4.941558	355.806372	5.537754
5.031836	353.779888	5.542758
4.657268	349.683343	5.547763
4.525730	355.482509	5.552768
4.735308	353.929221	5.557773
4.404588	354.674002	5.562778
4.804692	356.266303	5.567782
4.456793	358.428051	5.572787
4.812055	356.685862	5.577792
4.809353	348.189666	5.582797
4.517731	357.456515	5.587802
4.799845	352.116539	5.592806
5.059793	366.298913	5.597811
4.890835	371.262043	5.602816
5.109078	378.953392	5.607821
4.812556	381.580642	5.612826
5.457247	375.369759	5.617830
5.041330	380.543495	5.622835
4.997204	361.934461	5.627840
5.216062	366.776736	5.632845
4.856720	378.285124	5.637850
5.177371	358.666298	5.642854
5.040822	378.450256	5.647859
4.939507	379.688286	5.652864
5.288299	378.480965	5.657869
5.228379	383.163584	5.662874
5.457011	373.837545	5.667878
5.279034	366.892627	5.672883
4.939289	345.830911	5.677888
5.107134	357.647847	5.682893
5.359893	373.134242	5.687898
5.266882	364.348498	5.692902
5.101223	365.909173	5.697907
5.119923	370.053653	5.702912
5.297188	378.784260	5.707917
5.018162	383.667345	5.712922
5.333389	382.816449	5.717926
5.026554	379.972038	5.722931
5.214060	379.898491	5.727936
5.087771	379.022825	5.732941
5.155577	380.041433	5.737946
5.328044	376.224308	5.742950
5.164180	379.221505	5.747955
5.057202	382.326896	5.752960
5.140762	373.540129	5.757965
5.049026	389.671059	5.762970
5.598277	382.634132	5.767974
5.409836	379.398727	5.772979
5.282959	386.126200	5.777984
5.324025	391.220717	5.782989
5.578055	401.906088	5.787994
5.780676	385.964438	5.792998
5.199932	390.603255	5.798003
5.585297	392.156756	5.803008
5.236783	400.041816	5.808013
5.491734	407.093250	5.813018
5.911791	404.029013	5.818022
5.554358	402.414107	5.823027
5.555437	390.426939	5.828032
5.475743	393.425791	5.833037
5.691223	406.583289	5.838042
5.785444	403.698513	5.843046
5.550340	398.288071	5.848051
5.248672	394.965441	5.853056
5.599355	399.525609	5.858061
5.865875	405.669739	5.863066
5.933056	413.068996	5.868070
5.607285	404.074902	5.873075
5.771954	398.329685	5.878080
5.829485	397.018642	5.883085
5.470542	393.536180	5.888090
5.672637	393.094352	5.893094
5.811114	413.290638	5.898099
5.850976	402.311358	5.903104
5.791468	402.852967	5.908109
5.606594	405.399770	5.913114
5.982934	395.697208	5.918118
5.590616	410.180231	5.923123
5.526612	405.067655	5.928128
6.025763	405.861311	5.933133
5.325366	417.913233	5.938138
5.799834	411.675464	5.943142
5.730734	424.512853	5.948147
5.768055	410.990689	5.953152
5.855042	403.084256	5.958157
5.595222	407.633232	5.963162
5.856983	405.008039	5.968166
5.439148	413.084951	5.973171
5.725345	412.429490	5.978176
5.762220	409.491850	5.983181
5.541143	417.028432	5.988186
5.914392	429.588728	5.993190
6.111850	433.935498	5.998195
6.626021	428.915438	6.003200
6.440237	423.251134	6.008205
5.878091	414.410828	6.013210
5.999807	405.345200	6.018214
5.861544	404.072102	6.023219
6.123561	414.162959	6.028224
5.796158	414.672953	6.033229
5.849152	415.759336	6.038234
6.127203	402.835509	6.043238
5.729320	417.439442	6.048243
5.910997	413.094876	6.053248
6.018811	407.832880	6.058253
5.851780	429.691044	6.063258
6.160682	434.269389	6.068262
6.020945	428.835054	6.073267
5.992563	419.293427	6.078272
6.387310	409.191947	6.083277
5.836381	407.648351	6.088282
6.229949	402.208797	6.093286
6.314761	409.744257	6.098291
6.076370	412.508311	6.103296
6.090588	409.060949	6.108301
5.904444	408.097115	6.113306
5.968118	406.426489	6.118310
6.143688	410.376280	6.123315
5.907295	405.639566	6.128320
6.402871	400.344149	6.133325
5.833091	409.463104	6.138330
6.145570	400.950605	6.143334
5.908217	412.691608	6.148339
6.256218	411.087371	6.153344
6.209601	411.913777	6.158349
5.842115	412.425474	6.163354
6.241173	399.625670	6.168358
5.984309	403.850916	6.173363
6.031855	410.317052	6.178368
6.229960	406.971260	6.183373
6.145857	409.298513	6.188378
6.137252	411.982091	6.193382
5.994770	419.658400	6.198387
6.091409	406.397166	6.203392
6.226015	406.249693	6.208397
5.893895	412.627734	6.213402
6.130309	406.534370	6.218406
6.166037	410.128822	6.223411
5.887079	389.017316	6.228416
5.898121	385.906354	6.233421
5.650123	400.670950	6.238426
6.257870	404.094115	6.243430
6.089205	414.683722	6.248435
5.907341	408.513786	6.253440
6.319180	405.116026	6.258445
5.661246	402.370005	6.263450
6.128440	400.123628	6.268454
5.996381	408.308128	6.273459
5.988953	403.775634	6.278464
6.115012	391.965503	6.283469
5.863882	393.576446	6.288474
6.035063	394.905519	6.293478
5.992304	407.467193	6.298483
5.985937	408.679439	6.303488
6.035543	397.639348	6.308493
5.969173	396.431308	6.313498
6.275737	395.282089	6.318502
5.946497	377.799095	6.323507
5.538051	372.930050	6.328512
6.099492	389.617260	6.333517
5.993693	408.197531	6.338522
6.279441	402.468969	6.343526
6.066007	389.795261	6.348531
5.876619	385.756253	6.353536
6.040013	375.551021	6.358541
5.862948	389.918657	6.363546
6.022508	388.079812	6.368550
6.067357	398.631093	6.373555
6.039651	391.900850	6.378560
5.943494	378.929879	6.383565
5.752712	393.623819	6.388570
6.016340	398.396924	6.393574
6.076341	407.087368	6.398579
5.668012	402.678289	6.403584
5.815944	405.352719	6.408589
5.809567	412.332379	6.413594
5.958806	403.118533	6.418598
5.742730	400.200481	6.423603
6.085929	411.305434	6.428608
5.959785	408.610677	6.433613
5.767567	408.539818	6.438618
6.217759	401.050212	6.443622
6.345475	409.744048	6.448627
6.302299	402.159715	6.453632
6.387017	401.207272	6.458637
6.219443	396.080275	6.463642
5.575433	385.661810	6.468646
5.768411	391.043757	6.473651
5.774429	399.698734	6.478656
5.904065	398.450542	6.483661
5.702345	414.695222	6.488666
6.044933	397.319611	6.493670
6.081352	403.703127	6.498675
5.647495	411.125949	6.503680
6.044821	405.104808	6.508685
6.070657	409.624046	6.513690
6.061491	400.373875	6.518694
6.041138	414.465558	6.523699
5.871486	412.805742	6.528704
6.122813	417.039591	6.533709
6.032932	417.892104	6.538714
6.401535	404.890923	6.543718
5.673591	403.061686	6.548723
5.950371	406.446314	6.553728
6.202027	407.304041	6.558733
5.829298	420.554806	6.563738
6.197046	409.486694	6.568742
5.513292	415.817386	6.573747
5.688725	402.713213	6.578752
5.951186	407.336932	6.583757
5.673504	413.699052	6.588762
5.674211	405.791316	6.593766
5.723912	410.268319	6.598771
5.842353	408.403127	6.603776
5.812354	420.488691	6.608781
6.170894	433.921097	6.613786
6.242206	429.947445	6.618790
6.017928	421.238660	6.623795
6.112239	415.340508	6.628800
6.318744	406.938302	6.633805
6.164947	407.147025	6.638810
6.152648	414.149177	6.643814
6.324253	415.476998	6.648819
6.277216	408.948076	6.653824
6.314544	403.087583	6.658829
6.172889	414.304200	6.663834
6.190759	399.888560	6.668838
6.122868	399.387835	6.673843
5.873057	400.597569	6.678848
6.177520	405.829041	6.683853
5.896586	409.766015	6.688858
6.471075	398.055678	6.693862
6.164563	393.761565	6.698867
5.834418	382.762658	6.703872
5.809403	370.676421	6.708877
5.599153	388.339570	6.713882
5.999754	395.895353	6.718886
5.694831	399.421886	6.723891
5.696279	407.969878	6.728896
6.268072	408.974301	6.733901
5.983812	405.805275	6.738906
6.340326	404.407624	6.743910
5.760996	409.457859	6.748915
5.776859	405.755066	6.753920
6.074490	404.395976	6.758925
5.825273	410.779826	6.763930
5.978508	397.108236	6.768934
6.057388	408.197556	6.773939
6.359557	408.594816	6.778944
6.061384	407.007196	6.783949
6.077765	409.230981	6.788954
6.370509	404.090513	6.793958
6.235510	409.697670	6.798963
5.667217	399.944318	6.803968
5.982154	401.450083	6.808973
5.913631	406.700889	6.813978
6.058823	398.504996	6.818982
5.974257	413.998940	6.823987
5.794453	414.937385	6.828992
5.963950	411.466678	6.833997
5.942521	414.403197	6.839002
6.255284	403.542519	6.844006
5.825482	416.965141	6.849011
6.370121	412.765705	6.854016
6.315972	405.506429	6.859021
5.932344	407.142668	6.864026
6.102266	386.088265	6.869030
6.037216	387.674315	6.874035
5.576555	375.617389	6.879040
6.219619	387.217719	6.884045
6.079592	395.969300	6.889050
5.852705	386.737823	6.894054
5.741667	385.767869	6.899059
5.971580	405.185897	6.904064
6.263010	402.354506	6.909069
5.873730	408.718922	6.914074
6.434684	403.452344	6.919078
5.822489	393.414008	6.924083
5.873560	379.514454	6.929088
6.032150	388.094234	6.934093
5.612154	398.168362	6.939098
5.812371	402.170114	6.944102
6.173809	407.055888	6.949107
6.082578	410.594598	6.954112
6.285445	409.941686	6.959117
5.737580	413.345449	6.964122
6.076241	409.591178	6.969126
6.304688	415.570524	6.974131
5.769252	403.338288	6.979136
6.230791	399.431258	6.984141
6.086816	389.233104	6.989146
5.948003	379.522710	6.994150
5.679871	384.200733	6.999155
5.864377	399.541375	7.004160
6.255169	405.019631	7.009165
5.939238	410.521965	7.014170
6.023208	410.383864	7.019174
6.229458	401.409225	7.024179
6.009320	392.500065	7.029184
6.136060	387.968251	7.034189
5.844722	375.066899	7.039194
6.212829	371.126605	7.044198
6.072969	371.315062	7.049203
6.172326	372.792584	7.054208
6.182718	370.027074	7.059213
5.601001	381.573075	7.064218
6.159573	375.439008	7.069222
5.815397	382.505572	7.074227
5.811492	379.666452	7.079232
5.954564	376.919426	7.084237
6.149018	384.537755	7.089242
6.267038	379.794854	7.094246
5.993667	385.057668	7.099251
5.954777	380.889349	7.104256
6.186036	376.534807	7.109261
6.021966	372.170739	7.114266
6.131493	376.139745	7.119270
5.915484	368.646209	7.124275
5.664926	365.555283	7.129280
5.963982	376.100174	7.134285
5.614432	380.761090	7.139290
5.947480	371.127281	7.144294
6.124991	393.870237	7.149299
5.961223	382.656507	7.154304
5.975145	379.976845	7.159309
6.256272	394.355444	7.164314
5.745330	377.294452	7.169318
5.639363	388.457385	7.174323
5.955981	399.562193	7.179328
6.105772	405.493779	7.184333
5.950092	413.988067	7.189338
5.996585	405.108159	7.194342
6.154366	410.758795	7.199347
6.006375	410.480709	7.204352
6.478246	406.901917	7.209357
6.022143	384.421805	7.214362
5.941706	378.318559	7.219366
5.722107	384.574749	7.224371
5.477430	394.628329	7.229376
6.317145	394.022705	7.234381
5.991284	407.219324	7.239386
6.028353	410.060510	7.244390
6.245318	412.340280	7.249395
5.942495	401.178768	7.254400
6.076023	379.969964	7.259405
5.746480	388.516906	7.264410
6.042089	400.768965	7.269414
6.047338	405.476517	7.274419
5.813698	412.550248	7.279424
6.175995	401.430947	7.284429
6.048266	404.334350	7.289434
6.063915	399.676674	7.294438
6.013969	393.719929	7.299443
6.094284	392.407876	7.304448
5.820580	376.760405	7.309453
5.915880	384.386272	7.314458
6.228992	399.844545	7.319462
5.776154	389.999461	7.324467
5.718047	388.738351	7.329472
6.096900	395.364325	7.334477
5.918428	410.265027	7.339482
6.361171	411.504536	7.344486
6.229375	402.030168	7.349491
5.781772	380.096466	7.354496
5.797570	386.400507	7.359501
5.635564	399.685627	7.364506
6.137705	407.455685	7.369510
6.140420	402.577749	7.374515
6.170916	411.543040	7.379520
6.547195	405.450394	7.384525
6.118990	395.037630	7.389530
5.768318	383.499442	7.394534
5.927962	378.656111	7.399539
5.723540	381.413746	7.404544
6.257697	377.113835	7.409549
5.887890	384.337778	7.414554
6.008163	381.294967	7.419558
6.102827	386.688653	7.424563
5.853146	388.340796	7.429568
6.066101	374.641577	7.434573
5.955641	378.547158	7.439578
6.415575	378.351538	7.444582
6.183962	376.280868	7.449587
6.035763	380.472523	7.454592
6.231938	376.215158	7.459597
5.811331	376.666977	7.464602
5.951273	373.547698	7.469606
6.098137	373.364451	7.474611
6.170466	379.676099	7.479616
6.092577	379.620646	7.484621
5.741033	388.261415	7.489626
5.880276	374.374695	7.494630
5.763216	383.806835	7.499635
5.795641	382.817664	7.504640
5.830925	375.258045	7.509645
5.707746	382.773663	7.514650
6.052421	390.684046	7.519654
6.128871	407.692336	7.524659
6.075910	397.994553	7.529664
5.966369	384.206643	7.534669
5.859349	385.458248	7.539674
5.870186	390.009763	7.544678
5.747877	393.331018	7.549683
5.952964	405.934926	7.554688
6.257294	409.448394	7.559693
6.227416	420.712813	7.564698
6.170589	400.251248	7.569702
5.768659	380.395454	7.574707
5.949147	380.408319	7.579712
6.263467	390.201202	7.584717
5.623579	389.200218	7.589722
6.230710	398.029958	7.594726
6.341309	383.754283	7.599731
5.548474	385.315604	7.604736
5.898787	389.795711	7.609741
6.108825	396.177312	7.614746
6.147525	397.826304	7.619750
6.099876	384.235350	7.624755
6.121620	376.096417	7.629760
6.057114	376.538605	7.634765
5.691401	375.643383	7.639770
6.059281	377.799488	7.644774
6.189776	385.798418	7.649779
5.744950	377.237476	7.654784
5.849725	382.013397	7.659789
5.898953	394.560420	7.664794
6.067188	403.869947	7.669798
6.053004	413.728095	7.674803
6.304667	406.905013	7.679808
6.557338	387.048367	7.684813
5.601922	394.899335	7.689818
6.255958	387.956550	7.694822
6.070183	382.599121	7.699827
5.982861	393.319301	7.704832
5.967897	380.069070	7.709837
5.770359	394.452336	7.714842
5.535536	381.583851	7.719846
5.724598	381.710541	7.724851
6.137413	401.445200	7.729856
6.292847	405.538039	7.734861
5.871737	391.089323	7.739866
6.120429	378.218726	7.744870
6.162834	385.121229	7.749875
5.913658	384.410559	7.754880
5.763914	380.397352	7.759885
5.781576	389.310289	7.764890
6.085694	396.660833	7.769894
6.069359	413.933929	7.774899
5.940167	410.422891	7.779904
6.500848	400.454969	7.784909
5.915029	398.078661	7.789914
6.068163	382.641910	7.794918
5.944861	372.125984	7.799923
5.917260	375.783406	7.804928
6.260101	370.172093	7.809933
5.908723	385.591590	7.814938
5.716890	381.421955	7.819942
5.771435	381.437322	7.824947
6.233066	401.682699	7.829952
6.167739	390.264402	7.834957
5.798503	386.077767	7.839962
6.146282	383.529702	7.844966
6.008369	379.808964	7.849971
5.763675	384.453308	7.854976
6.139287	380.967619	7.859981
5.879079	381.950161	7.864986
5.973340	382.199901	7.869990
6.007734	393.250597	7.874995
6.226378	391.067676	7.880000
5.991917	385.640753	7.885005
5.714095	399.568048	7.890010
6.046239	391.942885	7.895014
5.950309	390.773682	7.900019
6.062330	393.841826	7.905024
6.035130	394.974244	7.910029
6.048595	387.552225	7.915034
5.996640	381.124969	7.920038
5.975110	386.452447	7.925043
5.933121	384.421615	7.930048
5.890518	381.085296	7.935053
6.198846	392.924385	7.940058
6.063681	391.751813	7.945062
6.013896	378.200291	7.950067
5.876204	381.496463	7.955072
6.177859	376.598044	7.960077
5.968308	379.775871	7.965082
6.032688	383.748606	7.970086
5.893610	376.996948	7.975091
5.937795	390.153393	7.980096
5.834806	379.543718	7.985101
6.189866	388.978396	7.990106
5.690763	383.066823	7.995110
6.189936	391.818727	8.000115
6.049111	403.421978	8.005133
6.191304	386.801840	8.010150
5.945878	384.886265	8.015168
5.909922	384.728775	8.020186
6.160948	385.253629	8.025203
6.063365	386.969778	8.030221
6.320106	380.747767	8.035238
6.026530	386.749574	8.040256
5.984614	381.274794	8.045274
6.118633	384.371772	8.050291
6.046899	382.948654	8.055309
6.249626	379.818806	8.060326
5.949859	389.142239	8.065344
6.124369	388.275741	8.070362
6.124560	380.535508	8.075379
6.068965	380.484018	8.080397
6.223772	380.139442	8.085414
5.973051	385.928657	8.090432
5.889697	375.331623	8.095450
5.927217	377.663538	8.100467
6.053621	388.472184	8.105485
6.054264	375.581895	8.110502
5.955747	382.857596	8.115520
5.853487	382.414849	8.120538
6.089364	402.067271	8.125555
5.957486	404.733908	8.130573
6.314774	407.808879	8.135590
6.450000	407.163828	8.140608
6.579882	407.283775	8.145626
6.650034	394.605566	8.150643
6.051764	386.588669	8.155661
6.077447	377.205961	8.160678
6.079445	387.450214	8.165696
6.411812	387.476401	8.170714
6.422915	384.881194	8.175731
5.924318	383.022698	8.180749
5.887201	376.652709	8.185766
5.956423	388.339651	8.190784
5.929917	371.950006	8.195802
6.105870	390.895268	8.200819
5.994486	388.335302	8.205837
6.299166	400.341505	8.210854
6.245696	404.721795	8.215872
6.339631	405.107517	8.220890
6.476355	397.728889	8.225907
5.941244	390.300501	8.230925
6.088036	395.086176	8.235942
6.363388	407.212978	8.240960
6.308262	412.826913	8.245978
6.275014	402.189283	8.250995
6.347397	410.362216	8.256013
6.622100	396.054589	8.261030
6.166190	386.585689	8.266048
5.998824	384.041884	8.271066
6.318326	385.705701	8.276083
5.997265	398.281620	8.281101
6.170318	407.593105	8.286118
6.494431	417.255932	8.291136
6.135989	423.661180	8.296154
6.440574	423.059142	8.301171
6.429075	427.929498	8.306189
6.388117	413.670975	8.311206
6.506517	413.014341	8.316224
6.023885	404.500174	8.321242
6.325281	409.049246	8.326259
6.290031	418.341888	8.331277
6.589186	414.171342	8.336294
6.274142	404.877318	8.341312
6.116305	419.139478	8.346330
6.705204	410.192189	8.351347
6.175971	413.622799	8.356365
6.362023	411.846978	8.361382
6.460457	404.140068	8.366400
6.577056	412.269462	8.371418
6.511046	391.334922	8.376435
6.018349	392.013238	8.381453
6.030319	394.481069	8.386470
6.143277	412.271329	8.391488
6.133402	425.520488	8.396506
6.492864	414.781014	8.401523
6.395380	420.172259	8.406541
6.074518	409.810381	8.411558
6.052141	409.483333	8.416576
6.105098	411.700304	8.421594
6.514281	410.111141	8.426611
6.271995	421.292843	8.431629
6.510883	407.052156	8.436646
6.767742	410.216586	8.441664
6.726381	414.422250	8.446682
7.018341	407.445242	8.451699
6.297107	412.618337	8.456717
6.541929	416.804170	8.461734
6.584284	418.824684	8.466752
6.426603	414.358947	8.471770
6.517099	407.840265	8.476787
6.352704	410.040868	8.481805
6.471538	416.059627	8.486822
6.630893	416.475851	8.491840
6.322289	420.696440	8.496858
6.387570	420.181662	8.501875
6.290231	423.440372	8.506893
6.448800	419.947777	8.511910
6.646095	414.846140	8.516928
6.443956	418.121021	8.521946
6.268379	415.903348	8.526963
6.090023	428.417475	8.531981
5.991438	424.955650	8.536998
6.650813	432.607808	8.542016
6.202777	447.235935	8.547034
6.964230	440.823839	8.552051
6.881486	439.504303	8.557069
6.886815	432.267880	8.562087
6.596662	424.792221	8.567104
6.491448	430.099126	8.572122
6.624137	415.444356	8.577139
6.615206	431.088651	8.582157
6.491192	430.449127	8.587175
6.862387	427.438015	8.592192
6.469570	433.322031	8.597210
6.724830	428.068872	8.602227
6.588498	434.615679	8.607245
6.588535	435.716306	8.612263
6.652906	425.740593	8.617280
6.220937	440.253071	8.622298
6.773011	444.379964	8.627315
6.577610	444.779348	8.632333
6.629038	448.674797	8.637351
6.707107	444.406216	8.642368
6.460685	446.868813	8.647386
6.703856	444.631596	8.652403
6.395745	447.467570	8.657421
6.735055	441.118485	8.662439
6.772740	447.345363	8.667456
6.768580	442.372146	8.672474
6.903600	438.214009	8.677491
6.744073	441.007072	8.682509
6.764674	446.975972	8.687527
6.809590	441.928492	8.692544
6.469136	446.266164	8.697562
6.627666	447.295078	8.702579
6.717885	453.629393	8.707597
6.675648	450.872548	8.712615
6.824902	445.553085	8.717632
6.656946	453.147970	8.722650
6.642486	438.592342	8.727667
6.625297	447.301347	8.732685
6.569311	445.610085	8.737703
6.826159	436.357948	8.742720
6.608925	444.968984	8.747738
6.761242	449.673649	8.752755
6.696057	446.616297	8.757773
6.789287	444.563345	8.762791
6.813261	436.814028	8.767808
6.644240	442.516513	8.772826
6.754148	428.583362	8.777843
7.020115	439.310277	8.782861
6.840427	442.682029	8.787879
6.956375	440.958755	8.792896
6.695999	441.927122	8.797914
6.835858	440.958099	8.802931
6.641765	445.114657	8.807949
6.757345	444.267361	8.812967
6.877313	456.539018	8.817984
6.774152	471.806663	8.823002
7.245399	471.830719	8.828019
7.071808	465.325823	8.833037
6.802991	457.405309	8.838055
6.940700	449.171834	8.843072
6.912688	449.411227	8.848090
6.915876	447.331455	8.853107
6.965778	445.887994	8.858125
6.687254	453.950564	8.863143
7.049676	456.580633	8.868160
6.913906	462.912611	8.873178
6.828089	462.104174	8.878195
6.896033	468.713029	8.883213
6.933810	480.539096	8.888231
7.288007	477.461504	8.893248
7.082316	476.871720	8.898266
6.941484	458.671915	8.903283
6.871068	464.178960	8.908301
6.994301	466.720891	8.913319
7.223557	458.786402	8.918336
6.542930	468.745739	8.923354
6.989791	459.169038	8.928371
7.285838	469.593771	8.933389
6.985377	471.358483	8.938407
7.147837	471.853323	8.943424
7.103862	474.599505	8.948442
7.070369	462.102170	8.953459
7.246822	463.712129	8.958477
6.909400	450.383108	8.963495
6.900826	439.662633	8.968512
7.048883	459.748142	8.973530
6.925457	466.505604	8.978547
7.125404	464.082643	8.983565
7.364849	469.403351	8.988583
7.275631	465.458703	8.993600
7.124530	453.253663	8.998618
6.867724	447.857354	9.003635
7.104193	453.223034	9.008653
7.155607	466.066440	9.013671
7.307754	453.812958	9.018688
7.077360	453.031414	9.023706
7.091959	447.053197	9.028723
7.056555	445.739600	9.033741
7.039595	458.883868	9.038759
7.115828	457.716536	9.043776
6.829051	466.167064	9.048794
6.624340	466.324700	9.053811
7.282911	473.923866	9.058829
6.835944	469.713676	9.063847
7.029559	474.651846	9.068864
6.896664	475.670361	9.073882
7.004763	481.057505	9.078899
7.498897	462.664765	9.083917
7.106541	466.253810	9.088935
7.102081	460.457666	9.093952
7.107290	471.894661	9.098970
7.215835	470.867440	9.103987
7.077137	474.621752	9.109005
6.761709	467.820877	9.114023
7.438050	470.174773	9.119040
7.222315	481.615685	9.124058
7.493326	484.700234	9.129075
7.713119	467.193602	9.134093
7.444408	475.688187	9.139111
7.412708	462.066819	9.144128
7.557163	465.931712	9.149146
7.479508	462.001684	9.154163
7.622578	470.834154	9.159181
7.426741	475.399837	9.164199
7.577232	471.075362	9.169216
7.339405	468.802837	9.174234
7.576009	463.763763	9.179251
7.459032	463.936988	9.184269
7.303118	469.545587	9.189287
7.486898	470.896085	9.194304
7.418797	454.084335	9.199322
7.147461	466.557201	9.204339
7.231222	465.461058	9.209357
7.049178	473.677531	9.214375
7.269933	470.332688	9.219392
7.308280	474.283258	9.224410
7.093259	473.163759	9.229427
7.248643	470.352142	9.234445
7.324382	480.135263	9.239463
7.067396	472.460009	9.244480
7.274996	471.512441	9.249498
7.260875	473.979290	9.254515
6.893141	467.680544	9.259533
7.313716	480.079792	9.264551
7.653068	497.580121	9.269568
7.200907	477.644967	9.274586
7.190879	498.458423	9.279603
7.532333	497.154068	9.284621
7.557007	504.602523	9.289639
7.692332	500.302991	9.294656
7.632257	503.211675	9.299674
7.431885	489.462515	9.304691
7.691589	479.392223	9.309709
7.503038	471.323776	9.314727
7.469693	470.079123	9.319744
7.406243	474.913414	9.324762
7.211611	475.740395	9.329779
7.756646	490.537368	9.334797
7.615098	493.826443	9.339815
7.605219	483.808071	9.344832
7.402465	477.811111	9.349850
7.748639	485.614756	9.354867
7.650802	469.222253	9.359885
7.460655	479.513146	9.364903
7.796172	469.032109	9.369920
7.681368	470.377131	9.374938
7.602097	482.284978	9.379955
7.769639	477.950789	9.384973
7.571531	478.305742	9.389991
7.449684	471.191926	9.395008
7.894976	471.648004	9.400026
7.201986	475.787976	9.405043
7.682690	468.177960	9.410061
7.376656	474.560575	9.415079
7.590284	465.756293	9.420096
7.697392	474.877376	9.425114
7.484210	475.754079	9.430131
7.782754	476.975346	9.435149
7.944517	473.745577	9.440167
7.713985	479.866892	9.445184
7.722625	476.859904	9.450202
7.511674	478.820015	9.455219
7.892037	464.790478	9.460237
7.405405	466.794662	9.465255
7.680526	472.899957	9.470272
7.616499	471.912727	9.475290
7.347222	474.889903	9.480307
7.907044	487.368454	9.485325
7.901235	491.267682	9.490343
8.127887	495.251246	9.495360
8.032571	475.357983	9.500378
8.001338	476.013233	9.505395
7.697364	470.347188	9.510413
7.509579	472.276299	9.515431
7.691865	467.282043	9.520448
7.941001	472.268496	9.525466
7.482810	472.626361	9.530483
7.373423	466.402544	9.535501
7.335383	477.690811	9.540519
7.863945	491.942128	9.545536
8.189848	498.896442	9.550554
7.896753	506.395745	9.555571
8.088718	485.779947	9.560589
7.703533	482.646648	9.565607
7.579648	477.983775	9.570624
7.349314	479.981346	9.575642
7.607522	495.769449	9.580659
7.813807	492.352199	9.585677
8.079707	503.820848	9.590695
8.070201	491.005367	9.595712
8.074835	497.255060	9.600730
7.720997	505.926934	9.605747
8.215890	504.878254	9.610765
8.098335	502.420071	9.615783
8.061798	495.171261	9.620800
7.766687	487.235402	9.625818
7.879044	499.242821	9.630835
8.126684	496.611578	9.635853
8.149170	503.232699	9.640871
7.849199	483.529996	9.645888
7.892207	475.954069	9.650906
7.616380	476.738987	9.655923
8.012623	489.979612	9.660941
8.077422	496.891143	9.665959
7.871567	502.287764	9.670976
8.157303	514.626695	9.675994
8.343121	506.194686	9.681011
8.221067	484.409913	9.686029
7.813001	478.642605	9.691047
7.944092	472.785628	9.696064
7.985233	473.140333	9.701082
7.642581	482.717362	9.706099
7.899848	486.223054	9.711117
8.130526	497.814058	9.716135
8.096248	504.996901	9.721152
8.369267	494.201416	9.726170
8.054315	490.502195	9.731187
7.844275	487.893003	9.736205
8.281322	494.784032	9.741223
7.868607	504.669505	9.746240
8.038126	500.845772	9.751258
7.978325	508.759760	9.756275
7.860424	495.030992	9.761293
7.685632	493.853062	9.766311
7.969511	509.004297	9.771328
7.973305	507.601140	9.776346
7.812956	505.900383	9.781363
8.123620	496.411167	9.786381
8.382788	508.196069	9.791399
7.894060	502.534818	9.796416
8.247001	503.275264	9.801434
8.085146	512.463738	9.806451
8.429169	499.297606	9.811469
8.156483	502.335582	9.816487
8.034376	495.935132	9.821504
8.240915	490.220763	9.826522
8.071321	511.136046	9.831539
8.134785	500.940569	9.836557
8.231582	497.310559	9.841575
8.071395	491.537434	9.846592
8.771432	504.544710	9.851610
8.122546	506.893066	9.856627
8.327817	503.100812	9.861645
8.347957	502.116571	9.866663
8.215210	499.085356	9.871680
8.158760	498.095296	9.876698
8.236106	506.720181	9.881715
8.338304	500.325891	9.886733
8.382322	504.610546	9.891751
8.223828	503.924369	9.896768
8.314540	493.571640	9.901786
8.127596	510.487330	9.906803
8.370679	508.066274	9.911821
7.990213	510.534346	9.916839
8.094676	510.910650	9.921856
8.321133	499.567399	9.926874
7.916444	512.274769	9.931891
8.395998	522.352639	9.936909
8.241156	532.710944	9.941927
8.225319	540.647391	9.946944
8.530435	536.695101	9.951962
8.577648	538.369379	9.956979
8.529105	530.182842	9.961997
8.820831	540.780964	9.967015
8.511763	526.888757	9.972032
8.506697	514.998046	9.977050
8.413727	511.635068	9.982067
7.992136	507.230522	9.987085
8.624057	516.319054	9.992103
8.187372	520.435690	9.997120
8.733199	522.239986	10.002138
8.576249	520.490440	10.007155
8.472938	507.290506	10.012173
8.561966	501.721566	10.017191
8.190819	504.415637	10.022208
8.355398	504.570978	10.027226
8.204059	527.476620	10.032243
8.819628	528.185587	10.037261
8.662245	533.148238	10.042279
8.373019	539.247998	10.047296
8.760554	527.426905	10.052314
8.735705	522.873790	10.057331
8.292928	507.208199	10.062349
8.435139	516.067213	10.067367
8.592744	522.325835	10.072384
8.813661	525.434434	10.077402
8.467311	520.208427	10.082419
8.615831	512.175869	10.087437
8.532857	502.594361	10.092455
8.326657	520.628131	10.097472
8.871910	524.897899	10.102490
8.684365	533.475722	10.107507
8.400998	526.235094	10.112525
8.771179	529.548292	10.117543
8.699805	527.579077	10.122560
8.617063	512.545744	10.127578
8.460247	520.794874	10.132595
8.720365	519.025476	10.137613
8.645553	523.859893	10.142631
8.789849	535.298508	10.147648
8.877949	524.123021	10.152666
8.503363	529.476532	10.157683
8.816921	523.255882	10.162701
8.989870	520.613579	10.167719
8.615391	510.182564	10.172736
8.369943	508.296109	10.177754
8.580993	520.935188	10.182771
8.731025	533.567255	10.187789
8.635908	533.138281	10.192807
8.409845	540.139330	10.197824
8.828792	533.330595	10.202842
8.786714	534.795658	10.207859
8.806339	544.475520	10.212877
8.708697	537.352155	10.217895
8.298526	541.466768	10.222912
8.622375	544.520927	10.227930
8.757964	536.633796	10.232947
8.429078	544.798839	10.237965
8.809911	537.393110	10.242983
8.624795	544.523788	10.248000
8.766655	534.148390	10.253018
8.401335	542.042517	10.258035
8.979429	551.070696	10.263053
9.104848	551.897241	10.268071
8.848046	556.691334	10.273088
8.670601	544.228399	10.278106
8.722705	550.608431	10.283123
9.058673	556.024597	10.288141
9.041240	562.233878	10.293159
8.950074	556.137314	10.298176
8.894950	549.312787	10.303194
8.793129	551.708743	10.308211
9.202574	551.965458	10.313229
9.295612	554.987765	10.318247
8.776057	544.380960	10.323264
8.892087	538.709117	10.328282
8.919792	547.305436	10.333299
8.789872	543.814917	10.338317
9.210152	540.406707	10.343335
8.821206	546.156275	10.348352
9.032759	536.034279	10.353370
9.153609	541.552394	10.358387
8.886996	535.707315	10.363405
9.618556	529.331232	10.368423
8.804752	534.784047	10.373440
8.847945	536.173773	10.378458
9.078457	531.439996	10.383475
8.929860	538.394164	10.388493
9.158337	536.106222	10.393511
8.917992	533.183164	10.398528
8.813622	543.904747	10.403546
9.205728	545.882127	10.408563
9.151801	551.592167	10.413581
9.586699	546.759389	10.418599
9.020629	550.197309	10.423616
9.161240	538.208447	10.428634
9.204732	536.275916	10.433651
9.016474	528.079446	10.438669
9.096461	525.689527	10.443687
8.971229	533.587592	10.448704
9.257204	536.320485	10.453722
9.187896	532.814421	10.458739
9.013253	532.046081	10.463757
9.377244	536.133676	10.468775
8.764426	531.654102	10.473792
9.411679	543.978467	10.478810
9.566617	544.713909	10.483827
8.918411	542.840995	10.488845
9.333288	536.460068	10.493863
9.096253	538.085554	10.498880
9.131742	541.902766	10.503898
9.312508	545.271739	10.508915
9.130508	561.070208	10.513933
9.516979	552.457518	10.518951
9.131657	556.222374	10.523968
9.355075	560.961950	10.528986
9.335935	552.860290	10.534003
9.355861	563.996905	10.539021
9.337482	556.973587	10.544039
9.046352	547.465295	10.549056
9.112783	552.859954	10.554074
9.297828	553.890587	10.559091
9.052444	562.745111	10.564109
9.387501	558.384736	10.569127
9.154328	562.767074	10.574144
9.212863	569.605073	10.579162
9.379516	561.836399	10.584179
8.958844	566.557440	10.589197
9.307755	560.014407	10.594215
9.040790	560.121727	10.599232
9.170191	562.886457	10.604250
9.318701	555.507180	10.609267
9.401462	557.202344	10.614285
9.771995	560.943217	10.619303
9.292421	559.898421	10.624320
9.435710	561.068047	10.629338
9.675309	555.958374	10.634355
9.337934	558.491754	10.639373
9.261703	555.272835	10.644391
9.100646	567.714924	10.649408
9.477501	574.309284	10.654426
9.534169	576.961068	10.659443
9.655069	585.273491	10.664461
9.709533	577.556060	10.669479
9.648915	579.374370	10.674496
9.357240	566.865374	10.679514
9.364112	575.782657	10.684531
9.510357	584.269807	10.689549
9.839030	587.670004	10.694567
9.481995	590.978837	10.699584
9.895711	590.503595	10.704602
10.285697	566.365173	10.709619
10.012010	563.264572	10.714637
9.835807	557.207284	10.719655
9.567428	549.890742	10.724672
9.560598	556.295102	10.729690
9.501786	555.057612	10.734707
9.507339	558.002679	10.739725
9.770254	553.274750	10.744743
9.739980	563.317194	10.749760
9.517450	554.759677	10.754778
9.741947	554.997021	10.759795
9.771191	545.002050	10.764813
9.904477	553.357480	10.769831
9.478609	554.790629	10.774848
9.511791	551.261881	10.779866
9.589176	547.074679	10.784883
9.362611	557.386416	10.789901
9.618748	548.898255	10.794919
9.678882	552.038404	10.799936
9.715184	556.535949	10.804954
9.717884	558.383730	10.809971
9.415705	561.470890	10.814989
9.720621	570.577975	10.820007
9.675093	586.198173	10.825024
9.415746	583.688855	10.830042
9.927277	586.450939	10.835059
9.393448	587.904133	10.840077
9.641000	582.222110	10.845095
9.825030	594.673019	10.850112
9.842902	588.837305	10.855130
10.069948	584.256242	10.860147
10.164912	589.461555	10.865165
10.312819	585.548079	10.870183
9.724691	593.710015	10.875200
10.005023	591.286321	10.880218
10.219987	590.026525	10.885235
9.852855	593.009887	10.890253
10.275349	584.975624	10.895271
9.691804	574.078823	10.900288
9.794941	575.188961	10.905306
10.097542	576.646360	10.910323
9.750450	584.017839	10.915341
9.666707	579.745702	10.920359
10.255017	583.822149	10.925376
10.077502	583.259779	10.930394
10.237298	577.911559	10.935411
9.746565	578.469289	10.940429
10.354231	578.725070	10.945447
10.487554	572.041365	10.950464
9.810964	562.475639	10.955482
10.185140	547.307168	10.960499
10.112689	553.663539	10.965517
9.816054	555.363457	10.970535
9.722134	555.670257	10.975552
9.880564	570.883662	10.980570
9.927264	578.437750	10.985587
10.045402	584.558454	10.990605
10.047454	575.272446	10.995623
10.183606	580.880752	11.000640
9.982604	579.557756	11.005658
10.161429	581.405311	11.010675
10.222057	584.115885	11.015693
10.084453	579.514107	11.020711
10.270518	576.130106	11.025728
10.144243	589.432536	11.030746
10.620494	588.902651	11.035763
9.961729	585.804002	11.040781
9.905292	589.577790	11.045799
10.397308	588.433721	11.050816
10.230927	592.361926	11.055834
10.281959	580.917357	11.060851
10.298935	576.758259	11.065869
10.288899	585.467731	11.070887
9.982359	581.452352	11.075904
9.995791	579.791704	11.080922
10.186770	581.078229	11.085939
10.324471	585.613911	11.090957
10.228780	578.720896	11.095975
10.414639	580.751132	11.100992
10.247188	580.881341	11.106010
10.339095	574.458806	11.111027
10.173013	573.790024	11.116045
10.095717	577.284604	11.121063
10.066960	581.521492	11.126080
9.739893	591.072386	11.131098
10.417072	582.290093	11.136115
10.196183	585.274236	11.141133
10.083810	582.933482	11.146151
10.267072	579.333424	11.151168
10.236716	590.456731	11.156186
10.467584	591.881328	11.161203
10.253810	594.287955	11.166221
10.271671	606.959880	11.171239
10.492837	613.201912	11.176256
10.664051	625.943730	11.181274
10.449631	609.561132	11.186291
10.292349	615.644782	11.191309
10.439646	615.206765	11.196327
10.645410	614.496486	11.201344
10.211061	618.892664	11.206362
10.400700	605.311680	11.211379
10.329958	614.497922	11.216397
10.373229	612.581952	11.221415
10.383409	606.603420	11.226432
10.428346	606.945689	11.231450
10.785072	608.971847	11.236467
10.574388	613.072343	11.241485
10.625012	609.579274	11.246503
10.705480	608.374815	11.251520
10.414326	621.535688	11.256538
10.573046	612.079828	11.261555
10.714904	616.693565	11.266573
10.761522	612.256732	11.271591
10.686598	609.288750	11.276608
10.512952	617.528908	11.281626
10.725864	610.770200	11.286643
10.511045	613.484463	11.291661
10.654398	619.978934	11.296679
10.853525	614.022455	11.301696
10.699484	617.106946	11.306714
10.697113	611.015734	11.311731
10.764541	613.944662	11.316749
10.543430	619.177915	11.321767
10.586013	605.232920	11.326784
10.702040	618.058667	11.331802
10.882667	607.294149	11.336819
10.547431	620.292253	11.341837
10.546200	614.386272	11.346855
10.736677	606.869716	11.351872
10.403783	623.971300	11.356890
10.594217	618.432768	11.361907
10.819592	617.341314	11.366925
10.589850	621.304425	11.371943
10.527334	603.680026	11.376960
10.802188	622.310789	11.381978
10.646853	613.009287	11.386995
10.802268	621.951997	11.392013
10.883281	636.818466	11.397031
10.906802	633.262955	11.402048
10.795459	629.360508	11.407066
11.039459	639.584540	11.412083
11.030046	627.584233	11.417101
10.699675	618.544767	11.422119
10.812791	626.536277	11.427136
10.878399	637.644122	11.432154
11.169092	636.740657	11.437171
11.252769	629.717138	11.442189
10.640183	628.063693	11.447207
10.821528	621.949143	11.452224
10.921338	637.029809	11.457242
10.933422	639.643516	11.462259
11.126990	645.298240	11.467277
11.083140	642.115277	11.472295
10.796457	622.038173	11.477312
10.919293	640.171525	11.482330
10.712693	638.721310	11.487347
10.836806	645.991370	11.492365
10.553844	649.291296	11.497383
10.893819	642.903242	11.502400
10.830974	645.225046	11.507418
11.098222	639.673000	11.512435
10.885943	646.827119	11.517453
10.900323	648.194070	11.522471
11.189145	634.504320	11.527488
10.684416	649.887844	11.532506
10.854162	657.840074	11.537523
11.424919	658.230307	11.542541
10.956302	669.590010	11.547559
11.136624	672.676229	11.552576
11.194934	678.900572	11.557594
11.598088	673.392147	11.562611
11.513704	668.177433	11.567629
11.053267	659.809834	11.572647
11.198945	646.523280	11.577664
10.940447	647.187430	11.582682
11.069037	658.195497	11.587699
11.471856	660.848045	11.592717
11.215652	669.513292	11.597735
11.371737	661.181786	11.602752
11.307460	662.166117	11.607770
11.215980	663.876956	11.612787
11.469253	668.341559	11.617805
11.301402	664.611049	11.622823
11.493959	649.798713	11.627840
10.990985	660.290532	11.632858
11.223907	661.155183	11.637875
11.667738	667.665270	11.642893
11.534618	667.426038	11.647911
11.407377	653.496129	11.652928
11.293330	645.083385	11.657946
11.359683	647.409385	11.662963
11.383564	650.323878	11.667981
11.231076	665.082985	11.672999
11.497778	652.387372	11.678016
11.126043	674.776020	11.683034
11.302339	680.456056	11.688051
11.591091	674.524476	11.693069
11.683465	676.960732	11.698087
11.841400	670.927593	11.703104
11.683802	657.401108	11.708122
10.860456	654.023220	11.713139
11.623804	656.566072	11.718157
11.388563	664.396401	11.723175
11.686376	654.938348	11.728192
11.585156	666.304532	11.733210
11.490982	671.141610	11.738227
11.571429	664.228840	11.743245
11.335498	674.059951	11.748263
11.935567	670.532579	11.753280
11.749607	666.820813	11.758298
11.647677	669.699059	11.763315
11.688249	666.132450	11.768333
11.770891	660.040134	11.773351
11.556184	637.395344	11.778368
11.161601	648.171550	11.783386
11.542741	667.728213	11.788403
11.754500	667.183070	11.793421
11.559510	665.994299	11.798439
11.865064	660.749663	11.803456
11.684223	664.267314	11.808474
11.584956	673.631335	11.813491
11.825908	676.996867	11.818509
11.437483	676.210182	11.823527
11.738864	671.229997	11.828544
11.836049	675.621635	11.833562
11.542385	676.323892	11.838579
11.756599	665.043961	11.843597
11.217503	668.412679	11.848615
11.449429	667.916950	11.853632
11.598528	674.951798	11.858650
11.443253	677.992806	11.863667
11.772940	669.340441	11.868685
11.787901	690.871430	11.873703
12.037080	695.799684	11.878720
11.945808	695.601156	11.883738
11.686446	682.269049	11.888755
11.822448	676.947371	11.893773
11.837958	692.543987	11.898791
12.032727	699.887013	11.903808
12.098931	707.860351	11.908826
11.820717	693.761322	11.913843
11.974118	685.032633	11.918861
11.933309	685.530432	11.923879
12.111255	691.899921	11.928896
11.735370	694.111766	11.933914
11.819059	695.678255	11.938931
12.041883	700.685280	11.943949
12.056113	707.700745	11.948967
12.181822	704.902661	11.953984
12.225508	707.778454	11.959002
11.898556	693.236341	11.964019
11.824878	695.074149	11.969037
12.138103	701.162990	11.974055
12.440092	694.626096	11.979072
12.172556	693.997334	11.984090
11.890565	684.344736	11.989107
12.131844	685.620579	11.994125
12.137034	692.941847	11.999143
12.149260	688.009143	12.004160
12.196695	689.985941	12.009178
12.224926	698.105317	12.014195
12.072081	680.247181	12.019213
12.354784	693.366238	12.024231
12.017603	690.814479	12.029248
12.151807	686.623342	12.034266
12.019190	699.650162	12.039283
12.287456	699.890890	12.044301
12.525522	706.037844	12.049319
12.529940	696.036257	12.054336
12.481497	678.769067	12.059354
12.146960	676.993990	12.064371
12.180763	673.800525	12.069389
12.201352	670.225019	12.074407
11.910261	672.445654	12.079424
12.295263	674.675984	12.084442
12.083154	700.382522	12.089459
12.283353	705.555490	12.094477
12.235324	704.239631	12.099495
12.054687	699.796312	12.104512
12.160249	704.568045	12.109530
12.012432	706.510251	12.114547
12.347226	704.470018	12.119565
12.326273	711.547213	12.124583
12.370861	713.694555	12.129600
12.605311	705.870097	12.134618
12.023803	706.541675	12.139635
12.213745	703.662880	12.144653
12.201924	712.209343	12.149671
12.034116	707.776100	12.154688
12.421224	716.698215	12.159706
12.452362	731.573034	12.164723
12.601565	726.016883	12.169741
12.660472	742.815349	12.174759
12.762677	731.312199	12.179776
12.853025	715.138458	12.184794
12.240282	724.556433	12.189811
12.491775	714.183627	12.194829
12.383072	712.019203	12.199847
12.219350	733.915252	12.204864
12.602127	737.923024	12.209882
12.338243	742.920501	12.214899
12.679771	738.010021	12.219917
12.283213	741.890949	12.224935
12.620650	740.627395	12.229952
12.766853	737.705446	12.234970
12.489781	747.061160	12.239987
12.861883	741.418885	12.245005
12.977826	740.665602	12.250023
12.685155	747.192564	12.255040
12.899809	741.943662	12.260058
12.846548	746.961380	12.265075
12.725827	736.542324	12.270093
12.701903	747.484375	12.275111
13.010862	741.548242	12.280128
12.910312	738.188044	12.285146
12.691764	747.823028	12.290163
12.796312	737.554061	12.295181
13.021110	744.673251	12.300199
13.200298	736.410316	12.305216
12.733963	720.074825	12.310234
12.675379	725.505205	12.315251
12.872846	727.805176	12.320269
12.358047	738.671424	12.325287
12.590620	744.532706	12.330304
12.777513	740.854848	12.335322
12.818382	741.302512	12.340339
13.027973	741.175025	12.345357
13.102558	736.770138	12.350375
12.896693	732.607348	12.355392
12.549156	734.906231	12.360410
12.715067	746.440040	12.365427
13.106708	737.019942	12.370445
12.817225	744.454984	12.375463
12.968577	737.238331	12.380480
13.296157	735.927988	12.385498
12.702486	741.314699	12.390515
12.894407	739.582355	12.395533
12.977975	738.783649	12.400551
13.012426	741.942458	12.405568
13.045638	731.355799	12.410586
12.807698	734.026276	12.415603
12.958896	741.389922	12.420621
13.246990	741.878928	12.425639
13.236037	751.022085	12.430656
13.284670	732.694331	12.435674
12.930096	737.045050	12.440691
13.040931	743.711483	12.445709
12.938169	743.066458	12.450727
12.987257	756.249841	12.455744
13.171580	771.132402	12.460762
13.316180	773.827727	12.465779
13.460487	769.634896	12.470797
13.454612	771.083553	12.475815
13.200240	748.276281	12.480832
13.387420	737.149585	12.485850
13.392676	735.124547	12.490867
13.189164	729.311069	12.495885
13.173561	743.267314	12.500903
13.036465	732.152980	12.505920
13.276267	740.133414	12.510938
13.311728	761.210344	12.515955
13.534077	768.216965	12.520973
13.358457	755.850795	12.525991
13.298738	759.492891	12.531008
13.365600	763.599828	12.536026
13.349705	769.391244	12.541043
13.376876	772.740624	12.546061
13.905198	765.063134	12.551079
13.572501	751.888771	12.556096
13.644822	743.262053	12.561114
12.963431	736.488390	12.566131
13.033776	735.317486	12.571149
13.319856	753.206236	12.576167
13.241382	769.644037	12.581184
13.503123	759.368711	12.586202
13.500392	774.546406	12.591219
13.270164	767.443314	12.596237
13.375565	769.272736	12.601255
13.287742	771.817581	12.606272
13.548407	766.680337	12.611290
13.709853	774.460389	12.616307
13.718890	769.575428	12.621325
13.606528	769.127256	12.626343
13.723146	770.222185	12.631360
13.643657	762.052066	12.636378
13.286416	772.993818	12.641395
13.355983	769.815276	12.646413
13.857326	764.756283	12.651431
13.599377	770.321259	12.656448
13.452170	758.584205	12.661466
13.198547	770.350877	12.666483
13.575199	783.323753	12.671501
13.804219	786.280284	12.676519
13.773539	791.198219	12.681536
13.672903	793.388515	12.686554
13.888683	788.029575	12.691571
13.676649	793.213354	12.696589
13.845141	793.187549	12.701607
13.884352	789.133761	12.706624
14.029439	787.903629	12.711642
13.655515	778.848054	12.716659
13.650420	790.911759	12.721677
13.524189	788.840380	12.726695
13.663322	794.399453	12.731712
14.014294	790.487733	12.736730
14.155823	789.229057	12.741747
13.960163	796.385611	12.746765
14.121749	788.967643	12.751783
14.000938	790.800276	12.756800
14.297966	791.784234	12.761818
14.191753	783.613805	12.766835
14.196080	774.706218	12.771853
14.201888	758.773189	12.776871
13.887458	761.600423	12.781888
13.885805	757.290827	12.786906
13.805930	760.546125	12.791923
13.658244	762.286752	12.796941
14.044542	765.110943	12.801959
14.055318	781.822151	12.806976
14.471696	782.751703	12.811994
13.870765	776.494593	12.817011
13.889755	782.673523	12.822029
14.241438	780.874565	12.827047
14.011901	795.679623	12.832064
14.295245	788.064733	12.837082
14.296469	790.554287	12.842099
14.162901	790.990681	12.847117
14.496427	789.601400	12.852135
13.991013	773.169180	12.857152
14.388879	757.828284	12.862170
14.109776	765.474204	12.867187
13.876529	761.988345	12.872205
14.158417	763.274792	12.877223
14.190472	791.426740	12.882240
14.149542	790.513221	12.887258
14.153537	790.078851	12.892275
14.545609	787.981094	12.897293
14.492051	787.390909	12.902311
14.407037	796.518011	12.907328
14.410924	800.394060	12.912346
14.832967	791.146838	12.917363
14.221017	780.541390	12.922381
14.248604	768.274625	12.927399
14.099498	784.920190	12.932416
14.153160	782.246614	12.937434
14.037504	789.658406	12.942451
14.151635	795.797180	12.947469
14.288708	788.856081	12.952487
14.142582	801.304939	12.957504
14.292893	792.797949	12.962522
14.224065	793.662183	12.967539
14.068379	801.786871	12.972557
14.379948	805.288369	12.977575
14.378767	818.437611	12.982592
14.602723	822.372103	12.987610
14.525563	824.063659	12.992627
14.353822	830.050186	12.997645
14.658718	825.809883	13.002663
14.739959	833.956771	13.007680
14.537122	823.610305	13.012698
15.003122	822.049881	13.017715
14.819022	823.486325	13.022733
14.704459	820.951616	13.027751
14.574856	823.351032	13.032768
14.567366	829.160763	13.037786
14.637915	824.493934	13.042803
14.405117	833.718360	13.047821
14.527208	822.056345	13.052839
14.589717	816.818438	13.057856
14.758362	817.200068	13.062874
14.568411	826.226459	13.067891
14.408077	829.275420	13.072909
14.771029	828.576110	13.077927
14.639484	828.498811	13.082944
14.722285	823.441391	13.087962
14.770372	820.926203	13.092979
14.780622	826.956212	13.097997
14.769782	822.857163	13.103015
14.390708	837.861029	13.108032
14.732390	846.114003	13.113050
15.249262	846.227746	13.118067
14.909796	862.115583	13.123085
15.016107	848.858209	13.128103
15.012666	867.342641	13.133120
15.021090	855.736429	13.138138
15.104609	849.910809	13.143155
15.150064	843.730095	13.148173
14.957845	832.917322	13.153191
14.729020	832.294741	13.158208
14.842724	833.660222	13.163226
15.177751	846.259354	13.168243
15.090082	858.453708	13.173261
15.370078	850.494083	13.178279
15.445774	836.435923	13.183296
15.025198	827.279388	13.188314
15.064894	818.984785	13.193331
14.981644	820.974972	13.198349
15.379849	826.485647	13.203367
14.837716	826.468461	13.208384
14.939487	826.784002	13.213402
15.225469	841.957262	13.218419
15.031574	850.261916	13.223437
15.134014	851.796971	13.228455
15.377659	853.959007	13.233472
15.160095	856.041908	13.238490
15.436037	848.167203	13.243507
14.964681	858.559041	13.248525
15.086097	843.777198	13.253543
14.833721	852.374593	13.258560
14.939692	860.036714	13.263578
15.325426	854.153571	13.268595
14.865524	856.756890	13.273613
15.105641	847.047658	13.278631
15.138903	852.007384	13.283648
15.087301	868.220378	13.288666
15.422953	880.828883	13.293683
15.177709	891.691546	13.298701
15.528176	887.594067	13.303719
15.352855	893.581999	13.308736
15.116170	891.158046	13.313754
15.513858	895.858634	13.318771
15.281027	893.333260	13.323789
15.448518	892.274992	13.328807
15.318396	884.619468	13.333824
15.424487	890.186803	13.338842
15.508148	890.205358	13.343859
15.413850	904.152732	13.348877
15.557351	882.053755	13.353895
15.786985	892.373636	13.358912
15.841728	887.744049	13.363930
15.869636	882.005574	13.368947
15.564248	888.343765	13.373965
15.626384	891.961384	13.378983
15.879850	891.360512	13.384000
15.519451	885.081244	13.389018
15.693871	889.146784	13.394035
15.879896	891.252227	13.399053
15.887556	877.614331	13.404071
15.824710	885.356779	13.409088
15.783752	880.977675	13.414106
16.059046	885.245398	13.419123
15.593653	888.832263	13.424141
15.799752	882.522575	13.429159
16.177613	885.064341	13.434176
15.716633	886.108075	13.439194
15.790652	882.242585	13.444211
15.505026	894.348886	13.449229
15.855667	882.973376	13.454247
15.948920	888.864474	13.459264
15.841761	886.269082	13.464282
15.939851	881.961044	13.469299
15.688295	889.313895	13.474317
15.862486	888.945036	13.479335
15.696509	883.007968	13.484352
15.489085	883.753824	13.489370
15.843319	888.296651	13.494387
15.487976	887.747378	13.499405
15.763714	898.674166	13.504423
15.766289	912.189384	13.509440
15.960716	909.217688	13.514458
16.409530	911.064669	13.519475
16.098087	913.822541	13.524493
16.129355	914.791068	13.529511
16.184137	913.609736	13.534528
15.951546	919.647315	13.539546
16.171073	911.803966	13.544563
15.852196	922.000134	13.549581
16.263868	914.123393	13.554599
16.294486	914.164510	13.559616
16.182927	918.554564	13.564634
16.253069	902.708762	13.569651
15.830449	910.994237	13.574669
16.071578	911.550078	13.579687
16.166071	914.604103	13.584704
16.019850	917.310996	13.589722
16.276031	904.946039	13.594739
15.957630	913.783130	13.599757
16.036221	923.395398	13.604775
16.283720	927.691749	13.609792
16.381318	935.926530	13.614810
16.419995	949.262581	13.619827
16.325526	950.397199	13.624845
16.318795	948.359946	13.629863
16.604017	939.819120	13.634880
16.321016	944.119464	13.639898
16.436126	939.531045	13.644915
16.512823	945.317037	13.649933
16.530133	946.391416	13.654951
16.562363	942.075763	13.659968
16.425004	946.021691	13.664986
16.760618	940.838123	13.670003
16.211622	949.616965	13.675021
16.353032	947.265824	13.680039
16.643138	939.932405	13.685056
16.476507	947.738917	13.690074
16.613053	946.699155	13.695091
16.588301	954.432180	13.700109
16.585609	948.508204	13.705127
16.444866	949.928819	13.710144
16.493023	955.915201	13.715162
16.678496	943.874900	13.720179
16.665567	944.852321	13.725197
16.453529	946.849283	13.730215
16.801064	940.182704	13.735232
16.602016	953.742760	13.740250
16.561962	942.254742	13.745267
16.785294	951.603307	13.750285
16.759918	943.063912	13.755303
16.789740	943.353182	13.760320
16.817851	946.235929	13.765338
17.155489	938.942670	13.770355
16.835491	940.314228	13.775373
16.637710	943.026514	13.780391
16.909569	948.036523	13.785408
16.886517	947.773549	13.790426
17.035502	940.321771	13.795443
16.682417	946.232469	13.800461
16.862969	941.008438	13.805479
16.775516	939.164859	13.810496
16.525599	957.105197	13.815514
17.130766	969.791583	13.820531
17.168872	979.529482	13.825549
16.808174	978.480718	13.830567
17.337819	975.510193	13.835584
17.032389	987.648978	13.840602
17.230022	980.777684	13.845619
17.226677	975.524251	13.850637
17.292475	977.100818	13.855655
17.115222	949.985382	13.860672
16.840679	947.847205	13.865690
17.059805	957.829120	13.870707
16.971518	981.161783	13.875725
17.071112	980.633629	13.880743
16.941184	973.319353	13.885760
17.055643	985.340186	13.890778
17.307312	978.538289	13.895795
17.208278	974.791584	13.900813
16.909962	980.294818	13.905831
17.248031	974.899423	13.910848
17.126073	977.828678	13.915866
17.129945	977.901388	13.920883
17.089932	980.060807	13.925901
17.215812	976.052853	13.930919
17.373067	982.216055	13.935936
17.152204	985.786072	13.940954
17.600228	998.399687	13.945971
17.454201	999.536153	13.950989
17.131530	990.289691	13.956007
17.564709	993.831329	13.961024
17.618443	1013.049351	13.966042
17.812048	1004.311464	13.971059
17.605764	996.312211	13.976077
17.329106	988.768298	13.981095
17.710289	978.628949	13.986112
17.268494	981.527309	13.991130
17.489866	985.239051	13.996147
17.828737	1004.136631	14.001165
17.577623	1001.889059	14.006183
17.450216	1000.319794	14.011200
17.724736	1021.069316	14.016218
17.707734	1016.101190	14.021235
17.745931	1012.629380	14.026253
17.459348	1013.428111	14.031271
17.716271	1008.548878	14.036288
17.699911	1023.971978	14.041306
17.829308	1013.360145	14.046323
17.658636	1010.387468	14.051341
17.337479	1013.194602	14.056359
18.005745	1012.860067	14.061376
17.827030	1013.146469	14.066394
17.779218	1016.600834	14.071411
17.647995	1018.263570	14.076429
17.919649	1017.529371	14.081447
18.079984	1012.650776	14.086464
17.444055	1017.315473	14.091482
17.690793	1019.897476	14.096499
17.917428	1021.693075	14.101517
17.654331	1020.702554	14.106535
17.360280	1013.685504	14.111552
17.599124	1023.445307	14.116570
17.778149	1023.726014	14.121587
18.005297	1033.991285	14.126605
17.903744	1030.872125	14.131623
18.033308	1037.544639	14.136640
17.804944	1035.260619	14.141658
17.785713	1040.366888	14.146675
18.101538	1031.692209	14.151693
18.084884	1035.762262	14.156711
17.957700	1034.492945	14.161728
17.876877	1037.587835	14.166746
18.155539	1038.032352	14.171763
18.324181	1039.060026	14.176781
18.007507	1045.913122	14.181799
18.127282	1043.503741	14.186816
18.181693	1033.639716	14.191834
18.251465	1033.022013	14.196851
18.010919	1027.832248	14.201869
18.057489	1034.949589	14.206887
18.094315	1030.366232	14.211904
18.129627	1055.179664	14.216922
18.130685	1071.630992	14.221939
18.691050	1070.585609	14.226957
18.412747	1070.951098	14.231975
18.418886	1063.442996	14.236992
18.352339	1076.791856	14.242010
18.425731	1063.675178	14.247027
18.696936	1063.941409	14.252045
18.363523	1066.821839	14.257063
18.560701	1058.091992	14.262080
18.344866	1064.881944	14.267098
18.453132	1063.330733	14.272115
18.384606	1063.734712	14.277133
18.264919	1065.453415	14.282151
18.425888	1057.383477	14.287168
18.326439	1065.105304	14.292186
18.297386	1061.498954	14.297203
18.575881	1062.517101	14.302221
18.352193	1071.957867	14.307239
18.316593	1061.691027	14.312256
18.449967	1062.272197	14.317274
18.240268	1065.184895	14.322291
18.721408	1074.815637	14.327309
18.944850	1090.060912	14.332327
18.716031	1089.101323	14.337344
18.814113	1096.605819	14.342362
18.931197	1098.592789	14.347379
19.000259	1099.689317	14.352397
18.869275	1093.016477	14.357415
18.917048	1081.731522	14.362432
18.917854	1078.797759	14.367450
18.542005	1076.786570	14.372467
18.874314	1083.312151	14.377485
19.053254	1100.939919	14.382503
18.872728	1093.129258	14.387520
18.975265	1105.360025	14.392538
19.086869	1097.158481	14.397555
18.948986	1094.242956	14.402573
18.925178	1094.805667	14.407591
19.101528	1089.895263	14.412608
18.985232	1093.171228	14.417626
18.947449	1098.647504	14.422643
19.128045	1089.216078	14.427661
18.935319	1090.323670	14.432679
19.025818	1094.331115	14.437696
18.786515	1078.330474	14.442714
18.994085	1089.245851	14.447731
19.199135	1088.039230	14.452749
18.702741	1092.034409	14.457767
18.812976	1092.920976	14.462784
18.872500	1095.714301	14.467802
18.572891	1101.898870	14.472819
19.276766	1108.516474	14.477837
18.915339	1123.870437	14.482855
19.124309	1123.737933	14.487872
19.324746	1126.012670	14.492890
19.297063	1133.723042	14.497907
19.648885	1116.743800	14.502925
19.231884	1128.616532	14.507943
19.340208	1117.414830	14.512960
19.308042	1122.350831	14.517978
19.419831	1129.811342	14.522995
19.473728	1116.261641	14.528013
19.620821	1125.708759	14.533031
19.767033	1119.274645	14.538048
19.679454	1124.952083	14.543066
19.278123	1127.432365	14.548083
19.743143	1115.897594	14.553101
19.482681	1124.620489	14.558119
19.545741	1123.969249	14.563136
19.669292	1125.088251	14.568154
19.636982	1129.285720	14.573171
19.762405	1124.059339	14.578189
19.689522	1132.340562	14.583207
19.945027	1124.832083	14.588224
19.480547	1112.352833	14.593242
19.284085	1131.555739	14.598259
19.753778	1124.099981	14.603277
19.377482	1127.228066	14.608295
19.385915	1128.998393	14.613312
19.604823	1119.229907	14.618330
19.718306	1129.862082	14.623347
19.561119	1127.180054	14.628365
19.449784	1128.677703	14.633383
19.635307	1125.174779	14.638400
19.534979	1126.256051	14.643418
19.504175	1145.707126	14.648435
20.060724	1147.262685	14.653453
20.029534	1155.502372	14.658471
19.986533	1158.042613	14.663488
20.029160	1153.279919	14.668506
19.761535	1154.043629	14.673523
19.972239	1159.574841	14.678541
19.870825	1153.693905	14.683559
19.961685	1158.429238	14.688576
19.890965	1149.723227	14.693594
19.784312	1162.937074	14.698611
20.103104	1154.237428	14.703629
20.015608	1157.876343	14.708647
20.244886	1157.584182	14.713664
20.185418	1151.278991	14.718682
20.194366	1154.182272	14.723699
20.199586	1144.240498	14.728717
20.186015	1151.930432	14.733735
20.271896	1149.863251	14.738752
20.338656	1149.027939	14.743770
20.259614	1157.712151	14.748787
20.194612	1135.876465	14.753805
20.201270	1146.075567	14.758823
20.113318	1148.173264	14.763840
20.240615	1146.805109	14.768858
20.136850	1148.947155	14.773875
20.323948	1156.131044	14.778893
20.060309	1154.680381	14.783911
20.218316	1172.781762	14.788928
20.248247	1182.791213	14.793946
20.279275	1188.906108	14.798963
20.542802	1182.955678	14.803981
20.491541	1184.620939	14.808999
20.305013	1183.030737	14.814016
20.595078	1181.828536	14.819034
20.568452	1184.746374	14.824051
20.627535	1175.138172	14.829069
21.006654	1182.804042	14.834087
20.846883	1179.252773	14.839104
20.785166	1174.440028	14.844122
20.629606	1182.683001	14.849139
21.013107	1173.825783	14.854157
20.775884	1171.884932	14.859175
20.442354	1155.169520	14.864192
20.426557	1159.854012	14.869210
20.325019	1175.203573	14.874227
20.759967	1171.613278	14.879245
20.642559	1183.266763	14.884263
20.546593	1174.550746	14.889280
20.982357	1177.695948	14.894298
20.555785	1180.152859	14.899315
20.686309	1175.489774	14.904333
20.691773	1183.033268	14.909351
20.855016	1173.114521	14.914368
20.865532	1176.512809	14.919386
20.970039	1176.833022	14.924403
20.955857	1181.941651	14.929421
20.894862	1179.860598	14.934439
20.516316	1179.060437	14.939456
21.056021	1187.009553	14.944474
21.102678	1204.199119	14.949491
20.994151	1202.717257	14.954509
21.111032	1203.738946	14.959527
21.082887	1207.682997	14.964544
21.101820	1199.603435	14.969562
21.102749	1216.569490	14.974579
21.493032	1206.046608	14.979597
21.355015	1200.462652	14.984615
21.118273	1207.358487	14.989632
21.467523	1207.672427	14.994650
21.399903	1212.441892	14.999667
21.257348	1191.414224	15.004685
21.525209	1176.666081	15.009703
21.486045	1180.089130	15.014720
21.464085	1173.068291	15.019738
21.041674	1178.785049	15.024755
21.296099	1167.815017	15.029773
21.281080	1174.509955	15.034791
21.387203	1188.644471	15.039808
21.825161	1199.308791	15.044826
21.472019	1194.449022	15.049843
21.178806	1176.268684	15.054861
21.406807	1187.479951	15.059879
21.599660	1198.699409	15.064896
21.609578	1206.827988	15.069914
21.662684	1207.870474	15.074931
21.773976	1200.463001	15.079949
21.847465	1196.766808	15.084967
21.610293	1193.791328	15.089984
21.683449	1181.033634	15.095002
21.641908	1176.578562	15.100019
21.633289	1165.286742	15.105037
21.686611	1179.073309	15.110055
21.663056	1190.412450	15.115072
22.003048	1195.826995	15.120090
21.677530	1186.098616	15.125107
21.943012	1188.349207	15.130125
21.664287	1176.591882	15.135143
21.319446	1196.461151	15.140160
21.773022	1196.852696	15.145178
21.712211	1198.638433	15.150195
22.015178	1195.427457	15.155213
21.788984	1198.137405	15.160231
21.577760	1204.949094	15.165248
21.733563	1200.564485	15.170266
21.914660	1202.814091	15.175283
21.859406	1203.832000	15.180301
21.769407	1196.594864	15.185319
21.750352	1204.941226	15.190336
21.813342	1187.818399	15.195354
22.102549	1208.962973	15.200371
22.214432	1217.559702	15.205389
22.330537	1211.787210	15.210407
22.002039	1206.253690	15.215424
21.819275	1207.248226	15.220442
21.819817	1220.656572	15.225459
22.066577	1226.084990	15.230477
22.574895	1235.047177	15.235495
22.416355	1229.946911	15.240512
22.422768	1233.184084	15.245530
22.442614	1236.156047	15.250547
22.178999	1231.155461	15.255565
22.438959	1227.744123	15.260583
22.066229	1233.112527	15.265600
22.352200	1227.594967	15.270618
22.093088	1232.034343	15.275635
22.335846	1234.918216	15.280653
22.477307	1229.946617	15.285671
22.119164	1233.617766	15.290688
22.511730	1224.740909	15.295706
22.598398	1233.917791	15.300723
22.489294	1233.946612	15.305741
22.424018	1224.321964	15.310759
22.492388	1241.774112	15.315776
22.474746	1228.848348	15.320794
22.374653	1241.049390	15.325811
22.501861	1233.759341	15.330829
22.843257	1227.485379	15.335847
22.262640	1236.636929	15.340864
22.502335	1233.959243	15.345882
22.465129	1246.212867	15.350899
22.761887	1254.005400	15.355917
22.741700	1250.036129	15.360935
22.798932	1260.132052	15.365952
23.025036	1252.221303	15.370970
22.807194	1253.433062	15.375987
22.834360	1257.430171	15.381005
23.099059	1255.449506	15.386023
22.775811	1258.538124	15.391040
23.118078	1250.945141	15.396058
22.973322	1265.453937	15.401075
22.903699	1256.676032	15.406093
23.245435	1257.222708	15.411111
22.806835	1263.866172	15.416128
22.856514	1255.434253	15.421146
23.082008	1258.330831	15.426163
22.907794	1256.253161	15.431181
23.291210	1247.532920	15.436199
23.004586	1255.711415	15.441216
22.983922	1256.929895	15.446234
23.067935	1248.768272	15.451251
22.970315	1253.395476	15.456269
23.134792	1246.392945	15.461287
23.009738	1257.195017	15.466304
23.138882	1246.972427	15.471322
23.034551	1241.680116	15.476339
22.944728	1250.755920	15.481357
23.260122	1259.328422	15.486375
23.270286	1272.825375	15.491392
23.432479	1279.805576	15.496410
23.253202	1284.441585	15.501427
23.302743	1288.972387	15.506445
23.489794	1283.478273	15.511463
23.344175	1296.423889	15.516480
23.760088	1290.757628	15.521498
23.727312	1290.560036	15.526515
23.637545	1280.418554	15.531533
23.574740	1276.295706	15.536551
23.652027	1284.702141	15.541568
23.748618	1274.062886	15.546586
23.664959	1261.681478	15.551603
23.192224	1255.636796	15.556621
23.477521	1267.722865	15.561639
23.555472	1275.760297	15.566656
23.357016	1282.035272	15.571674
23.885116	1276.016196	15.576691
23.737795	1283.251187	15.581709
23.855295	1276.322954	15.586727
23.565230	1289.076738	15.591744
23.325940	1282.929613	15.596762
23.350002	1276.644397	15.601779
23.367365	1283.376933	15.606797
23.605861	1279.647886	15.611815
23.891648	1301.197474	15.616832
23.933100	1306.186698	15.621850
23.921258	1304.560865	15.626867
24.251173	1304.844939	15.631885
24.455811	1300.764020	15.636903
24.096025	1291.934143	15.641920
24.204351	1285.514895	15.646938
24.096703	1270.898918	15.651955
23.949836	1275.531921	15.656973
24.260504	1283.615860	15.661991
24.375919	1275.065174	15.667008
24.074115	1277.544747	15.672026
24.110849	1270.552334	15.677043
24.003089	1280.020486	15.682061
24.469626	1278.004035	15.687079
24.359755	1295.134583	15.692096
24.449594	1278.145003	15.697114
24.225049	1276.120545	15.702131
24.141076	1275.374750	15.707149
24.551829	1281.993723	15.712167
24.509746	1298.446530	15.717184
24.815872	1293.006710	15.722202
24.337195	1275.872297	15.727219
24.354106	1279.465607	15.732237
24.281132	1269.387097	15.737255
24.360021	1277.917670	15.742272
24.425047	1289.596145	15.747290
25.101557	1293.711723	15.752307
24.448376	1281.113191	15.757325
24.538653	1275.257947	15.762343
24.828637	1279.608385	15.767360
24.528959	1284.924947	15.772378
24.559586	1282.402734	15.777395
24.348905	1297.314593	15.782413
24.718650	1300.384533	15.787431
24.862576	1299.969498	15.792448
24.832800	1294.588447	15.797466
24.894711	1295.682235	15.802483
24.477133	1295.975516	15.807501
24.769350	1298.537438	15.812519
24.903564	1298.491720	15.817536
24.864298	1306.212756	15.822554
24.902961	1304.905720	15.827571
24.512466	1307.210223	15.832589
24.970390	1294.013143	15.837607
25.080248	1297.389496	15.842624
24.514758	1311.988867	15.847642
24.743517	1296.232539	15.852659
24.899309	1307.173178	15.857677
24.939522	1298.098722	15.862695
24.848852	1309.093558	15.867712
24.639290	1311.786598	15.872730
24.973121	1319.213584	15.877747
25.024036	1324.850840	15.882765
25.385271	1332.845725	15.887783
24.893742	1332.950468	15.892800
25.239167	1329.825345	15.897818
25.034274	1318.747013	15.902835
25.303012	1330.420527	15.907853
25.207933	1322.586546	15.912871
25.447375	1334.965295	15.917888
25.514615	1326.072958	15.922906
25.822166	1337.927055	15.927923
25.356725	1331.981133	15.932941
25.451899	1332.736352	15.937959
25.234276	1336.483074	15.942976
25.389604	1336.330712	15.947994
25.230873	1327.690354	15.953011
25.234028	1336.501604	15.958029
25.353584	1326.140789	15.963047
25.341921	1326.475124	15.968064
25.406122	1331.114138	15.973082
25.597350	1325.671286	15.978099
25.511815	1341.640004	15.983117
25.761185	1353.005724	15.988135
26.121810	1355.869709	15.993152
25.648696	1345.285762	15.998170
25.688554	1326.545382	16.003187
25.732032	1329.103615	16.008205
26.276487	1334.665452	16.013223
26.077855	1324.940778	16.018240
25.803647	1327.373270	16.023258
25.978086	1322.498936	16.028275
25.723440	1321.758565	16.033293
25.785633	1317.961853	16.038311
25.814004	1325.235094	16.043328
26.089377	1328.450979	16.048346
26.206116	1337.026891	16.053363
25.717745	1337.762989	16.058381
25.979481	1342.510241	16.063399
26.131299	1344.487949	16.068416
26.002471	1351.120707	16.073434
26.123967	1340.054062	16.078451
25.804132	1350.718770	16.083469
25.740550	1346.178323	16.088487
26.509533	1352.399434	16.093504
25.993145	1352.539788	16.098522
26.041833	1342.421401	16.103539
26.045724	1350.436489	16.108557
26.046920	1344.359360	16.113575
26.089518	1346.019332	16.118592
26.133007	1357.489223	16.123610
26.405585	1365.898799	16.128627
26.147692	1377.090660	16.133645
26.748069	1375.724072	16.138663
26.949548	1368.461820	16.143680
26.610087	1354.973499	16.148698
26.532442	1344.319740	16.153715
26.423594	1341.085980	16.158733
26.611420	1337.610974	16.163751
26.561053	1339.830817	16.168768
26.340252	1346.477621	16.173786
27.186951	1354.203161	16.178803
26.811606	1362.560966	16.183821
26.429600	1347.532085	16.188839
26.524274	1350.640496	16.193856
26.473585	1364.190124	16.198874
27.126313	1365.770331	16.203891
26.787423	1371.185933	16.208909
26.894459	1371.188021	16.213927
27.177941	1358.930780	16.218944
26.780700	1360.926177	16.223962
26.691833	1351.012841	16.228979
26.826723	1357.277926	16.233997
26.836842	1371.800152	16.239015
26.723632	1376.769339	16.244032
26.655156	1371.352543	16.249050
26.924225	1370.093570	16.254067
26.923627	1370.561110	16.259085
26.834646	1369.111033	16.264103
27.015113	1377.105165	16.269120
26.872477	1370.541613	16.274138
27.297672	1370.593380	16.279155
27.357294	1376.113861	16.284173
26.875295	1371.654106	16.289191
27.281458	1364.829609	16.294208
27.323532	1373.979707	16.299226
27.241606	1365.347870	16.304243
27.177085	1377.216362	16.309261
27.051349	1366.089456	16.314279
27.112371	1377.458823	16.319296
26.924884	1392.935427	16.324314
27.296252	1402.164086	16.329331
27.543695	1396.366630	16.334349
27.312691	1403.163964	16.339367
27.735816	1393.918964	16.344384
27.668907	1400.477319	16.349402
27.788806	1397.252126	16.354419
27.865024	1396.121145	16.359437
27.788515	1396.179608	16.364455
28.100181	1391.282530	16.369472
27.216968	1389.531684	16.374490
27.659671	1387.929397	16.379507
27.717142	1396.389173	16.384525
27.647502	1392.417818	16.389543
27.939538	1382.827213	16.394560
27.868651	1392.223187	16.399578
27.992722	1391.605928	16.404595
28.124088	1397.152725	16.409613
27.999949	1389.664462	16.414631
27.753133	1371.633296	16.419648
27.864014	1395.145804	16.424666
28.142988	1394.505258	16.429683
27.847005	1393.576061	16.434701
27.550311	1392.449347	16.439719
27.949634	1387.383428	16.444736
27.804255	1391.350875	16.449754
27.871074	1388.199039	16.454771
28.002733	1387.880913	16.459789
28.033982	1390.475826	16.464807
27.990145	1393.961900	16.469824
27.872178	1396.570892	16.474842
28.258675	1389.575627	16.479859
28.275776	1385.866679	16.484877
27.798899	1399.151084	16.489895
28.397167	1415.017282	16.494912
27.986619	1418.677860	16.499930
28.571331	1416.503243	16.504947
28.135943	1422.723413	16.509965
28.408630	1415.666668	16.514983
28.723202	1414.978495	16.520000
28.631517	1418.261083	16.525018
28.496808	1407.336418	16.530035
28.919014	1407.459939	16.535053
28.628613	1408.911281	16.540071
28.811328	1414.779105	16.545088
28.780130	1414.100548	16.550106
28.868554	1411.057333	16.555123
29.059267	1388.225026	16.560141
28.789944	1384.844208	16.565159
28.987724	1371.074794	16.570176
28.737365	1373.396653	16.575194
28.942088	1381.630468	16.580211
28.518336	1377.553974	16.585229
28.779087	1380.291590	16.590247
28.898875	1371.178325	16.595264
28.664149	1371.814945	16.600282
28.584365	1374.285330	16.605299
28.861836	1367.951818	16.610317
29.142050	1397.639735	16.615335
29.321524	1390.560641	16.620352
28.866942	1385.366432	16.625370
29.026336	1369.174672	16.630387
29.161004	1378.647230	16.635405
28.617447	1389.330898	16.640423
29.072065	1389.447871	16.645440
29.135211	1409.717567	16.650458
29.057097	1410.294793	16.655475
29.331179	1405.590546	16.660493
28.803596	1408.011462	16.665511
29.476898	1408.086321	16.670528
29.189816	1408.971766	16.675546
29.352255	1403.472631	16.680563
29.215523	1408.046909	16.685581
29.321625	1407.553489	16.690599
29.528007	1396.694398	16.695616
29.414479	1404.374631	16.700634
29.233163	1406.670890	16.705651
29.610506	1402.390091	16.710669
29.194144	1404.331180	16.715687
29.381475	1396.829134	16.720704
29.213383	1415.119044	16.725722
29.260971	1421.974587	16.730739
29.300728	1426.026347	16.735757
29.903035	1431.637302	16.740775
29.735821	1430.741111	16.745792
29.530180	1430.035533	16.750810
29.365968	1424.911339	16.755827
29.534411	1429.764222	16.760845
29.560960	1434.697294	16.765863
29.750198	1422.710723	16.770880
29.676397	1437.159505	16.775898
29.590483	1452.104002	16.780915
30.180914	1444.461961	16.785933
29.892522	1458.173075	16.790951
29.948731	1462.170152	16.795968
30.055604	1457.638456	16.800986
29.846701	1460.599126	16.806003
30.359470	1452.967578	16.811021
30.116853	1457.905856	16.816039
30.101828	1453.767963	16.821056
30.385726	1455.556889	16.826074
30.463946	1456.175946	16.831091
30.560512	1446.855854	16.836109
30.064817	1455.799772	16.841127
30.414576	1448.993633	16.846144
30.471773	1452.450786	16.851162
30.658494	1454.482965	16.856179
30.501678	1440.700550	16.861197
30.544655	1453.266648	16.866215
30.561210	1442.412973	16.871232
30.430146	1430.746751	16.876250
30.560652	1427.714676	16.881267
30.523022	1418.606188	16.886285
30.003128	1429.142266	16.891303
30.795395	1438.696131	16.896320
30.895807	1440.447721	16.901338
30.581624	1447.956084	16.906355
30.858420	1449.665477	16.911373
30.893800	1453.334901	16.916391
30.689404	1434.798218	16.921408
30.743006	1431.585177	16.926426
30.700539	1443.197315	16.931443
30.851367	1441.581541	16.936461
30.561614	1448.104374	16.941479
30.537994	1435.625092	16.946496
30.585709	1441.012529	16.951514
30.721429	1443.474800	16.956531
30.683620	1440.376498	16.961549
30.481696	1451.893394	16.966567
30.564850	1453.328555	16.971584
30.751068	1465.370556	16.976602
30.603463	1474.939124	16.981619
31.169117	1479.014055	16.986637
30.858978	1482.625738	16.991655
30.997760	1487.463866	16.996672
30.931450	1479.081345	17.001690
30.740102	1484.777671	17.006707
30.982209	1496.319895	17.011725
30.791418	1503.721634	17.016743
31.269653	1506.329168	17.021760
31.744403	1509.436488	17.026778
31.778617	1508.495917	17.031795
31.808986	1501.902875	17.036813
31.932857	1502.867129	17.041831
31.836164	1480.893292	17.046848
31.808318	1476.410275	17.051866
31.621086	1471.085155	17.056883
32.083164	1458.956136	17.061901
31.830927	1466.030239	17.066919
31.917137	1463.473203	17.071936
31.825785	1461.147141	17.076954
31.487779	1471.268095	17.081971
31.884232	1465.461688	17.086989
32.089661	1463.066012	17.092007
31.730964	1460.851146	17.097024
32.304757	1459.295648	17.102042
31.966896	1463.136324	17.107059
32.087556	1457.806291	17.112077
31.899309	1455.295488	17.117095
32.055845	1454.597261	17.122112
32.070548	1458.985064	17.127130
31.812807	1462.282164	17.132147
31.753937	1459.846394	17.137165
31.545415	1459.037750	17.142183
31.877639	1466.369011	17.147200
31.994538	1463.548629	17.152218
31.647394	1461.366888	17.157235
32.186680	1474.468927	17.162253
32.071448	1498.120606	17.167271
31.697313	1494.106336	17.172288
32.216199	1495.071718	17.177306
32.083358	1490.560413	17.182323
32.345807	1488.183245	17.187341
31.948545	1498.162847	17.192359
32.287647	1501.451681	17.197376
32.246196	1487.608784	17.202394
32.253806	1499.236688	17.207411
32.674894	1506.488688	17.212429
32.782637	1511.483931	17.217447
32.479087	1503.512724	17.222464
32.622677	1491.500588	17.227482
32.439863	1500.208080	17.232499
32.982708	1509.196994	17.237517
32.573220	1510.914517	17.242535
32.613495	1518.647686	17.247552
32.874073	1525.802651	17.252570
32.612634	1527.367711	17.257587
32.607905	1514.006109	17.262605
32.775782	1520.997682	17.267623
32.934498	1516.040852	17.272640
33.096797	1517.773542	17.277658
32.678664	1518.240932	17.282675
32.975762	1520.123742	17.287693
33.067583	1520.864959	17.292711
32.950840	1518.744666	17.297728
33.408387	1515.080079	17.302746
33.213848	1525.287941	17.307763
33.295014	1514.432180	17.312781
33.337381	1514.530408	17.317799
33.204861	1519.415830	17.322816
33.073267	1510.462217	17.327834
33.142544	1520.168916	17.332851
33.171640	1524.432308	17.337869
33.263052	1521.647631	17.342887
33.313080	1517.155251	17.347904
33.287117	1518.747461	17.352922
33.154974	1514.132885	17.357939
33.454318	1509.425998	17.362957
33.319720	1513.632634	17.367975
33.108582	1540.700627	17.372992
33.578871	1539.095332	17.378010
33.749936	1545.403322	17.383027
33.463596	1549.299661	17.388045
33.865871	1544.882806	17.393063
34.046712	1548.176988	17.398080
33.980619	1544.566028	17.403098
33.874056	1549.660547	17.408115
33.934091	1541.805102	17.413133
33.890875	1538.607676	17.418151
33.972416	1535.154162	17.423168
34.134919	1528.606946	17.428186
34.012403	1527.581302	17.433203
34.213258	1525.422593	17.438221
33.992911	1508.408138	17.443239
33.710563	1514.545524	17.448256
34.268254	1526.238664	17.453274
34.324058	1535.952723	17.458291
34.207360	1521.009269	17.463309
34.321024	1512.251264	17.468327
34.194818	1517.133671	17.473344
34.414438	1505.038463	17.478362
33.929060	1504.392980	17.483379
34.465709	1520.545079	17.488397
34.525867	1525.895053	17.493415
34.344475	1527.660637	17.498432
34.876360	1528.712451	17.503450
34.325248	1521.478285	17.508467
34.284045	1504.709760	17.513485
34.616030	1514.641459	17.518503
34.311314	1526.290390	17.523520
34.696428	1521.092923	17.528538
34.511906	1529.514102	17.533555
34.226721	1525.280766	17.538573
34.575532	1529.171538	17.543591
34.257743	1531.291201	17.548608
34.544553	1525.808043	17.553626
34.050878	1526.254477	17.558643
34.562004	1539.944696	17.563661
34.714259	1548.287681	17.568679
34.703006	1559.159702	17.573696
34.937381	1556.914730	17.578714
34.875324	1557.392846	17.583731
35.024948	1554.417423	17.588749
34.702560	1556.807141	17.593767
34.746527	1555.121254	17.598784
34.868868	1553.305068	17.603802
34.816672	1561.163805	17.608819
35.237735	1555.069433	17.613837
35.285858	1554.420255	17.618855
34.979689	1565.398987	17.623872
34.906733	1561.664357	17.628890
35.059682	1564.491509	17.633907
35.244079	1579.618929	17.638925
35.177133	1582.082890	17.643943
35.193842	1585.026699	17.648960
35.598048	1578.647315	17.653978
35.407784	1587.476955	17.658995
35.720924	1577.177620	17.664013
35.966531	1569.078442	17.669031
35.779011	1579.807617	17.674048
35.700889	1573.376209	17.679066
35.877720	1579.879715	17.684083
35.824697	1573.684701	17.689101
36.028689	1562.311719	17.694119
35.867279	1555.163798	17.699136
35.536699	1538.077011	17.704154
35.613761	1550.339907	17.709171
35.722333	1563.648773	17.714189
36.166780	1566.768997	17.719207
35.537420	1572.222134	17.724224
36.001280	1573.670253	17.729242
35.665965	1573.324327	17.734259
35.659261	1571.883442	17.739277
35.901399	1574.779293	17.744295
35.691653	1577.412173	17.749312
35.939312	1570.666194	17.754330
35.861979	1569.736609	17.759347
35.988736	1586.421606	17.764365
36.420288	1585.167208	17.769383
36.381935	1598.197676	17.774400
36.167830	1598.186797	17.779418
36.569415	1601.522000	17.784435
36.596946	1604.330950	17.789453
36.633493	1598.262040	17.794471
36.523956	1597.338967	17.799488
36.268371	1578.544051	17.804506
36.275347	1572.958000	17.809523
36.233746	1588.996469	17.814541
36.670593	1589.604182	17.819559
36.518639	1593.957414	17.824576
36.562482	1590.546350	17.829594
36.742859	1587.851261	17.834611
36.783642	1589.713922	17.839629
36.923945	1591.616404	17.844647
36.600801	1594.509007	17.849664
36.810241	1591.145720	17.854682
36.706505	1589.722475	17.859699
36.520788	1599.951366	17.864717
37.109411	1581.691072	17.869735
36.713257	1596.035504	17.874752
36.772484	1603.115578	17.879770
36.633174	1618.284824	17.884787
36.897578	1622.202981	17.889805
37.092189	1615.161830	17.894823
37.057070	1620.103597	17.899840
37.597548	1613.568170	17.904858
37.632585	1617.760525	17.909875
37.466256	1625.397247	17.914893
37.707350	1616.485800	17.919911
37.658859	1611.394352	17.924928
37.560807	1591.154046	17.929946
37.530937	1588.142589	17.934963
37.595339	1582.600175	17.939981
37.724131	1583.449840	17.944999
37.766098	1585.112699	17.950016
37.520854	1578.071560	17.955034
37.601015	1579.263529	17.960051
37.374138	1580.107518	17.965069
37.532912	1587.504959	17.970087
37.404703	1582.983018	17.975104
37.714498	1582.860982	17.980122
37.630805	1594.754863	17.985139
37.863449	1607.256216	17.990157
37.965827	1609.862224	17.995175
37.799700	1618.467806	18.000192
37.928157	1618.229733	18.005210
37.949152	1611.172449	18.010227
37.843652	1617.523506	18.015245
38.089572	1608.954178	18.020263
38.014628	1605.039945	18.025280
38.029239	1605.742376	18.030298
38.234874	1615.480494	18.035315
38.240329	1608.690745	18.040333
38.172823	1605.944177	18.045351
37.952343	1606.021755	18.050368
38.388371	1604.370946	18.055386
38.393692	1600.653660	18.060403
38.405652	1602.821882	18.065421
38.088161	1606.073000	18.070439
38.091444	1604.487151	18.075456
38.289091	1611.342341	18.080474
38.335338	1625.017091	18.085491
38.437689	1622.879797	18.090509
38.949756	1634.208134	18.095527
38.623114	1642.077315	18.100544
38.970166	1635.889654	18.105562
39.180659	1633.169099	18.110579
38.374777	1626.726674	18.115597
38.646179	1622.916113	18.120615
38.605407	1642.480091	18.125632
38.740638	1627.834978	18.130650
38.933400	1628.062636	18.135667
39.030671	1637.449813	18.140685
38.871805	1633.140414	18.145703
39.026477	1633.363355	18.150720
39.022382	1633.070852	18.155738
39.221397	1623.824636	18.160755
38.863583	1635.873386	18.165773
39.030925	1630.292650	18.170791
39.026651	1626.125372	18.175808
38.582424	1633.900238	18.180826
39.080510	1645.685229	18.185843
38.853719	1651.180004	18.190861
39.391362	1654.369855	18.195879
39.298206	1668.164575	18.200896
39.328253	1656.958515	18.205914
39.494959	1658.719232	18.210931
39.514041	1663.488258	18.215949
39.537135	1663.136135	18.220967
39.862738	1656.606741	18.225984
39.465514	1655.979724	18.231002
39.761804	1648.264635	18.236019
39.606462	1659.977909	18.241037
39.670444	1652.521361	18.246055
39.697145	1661.371811	18.251072
39.307638	1655.751379	18.256090
39.737607	1663.922458	18.261107
39.982299	1686.554589	18.266125
39.930125	1676.838513	18.271143
40.073105	1685.211848	18.276160
39.945436	1686.564615	18.281178
40.415437	1680.322327	18.286195
39.921026	1695.568162	18.291213
40.164217	1684.122459	18.296231
39.996131	1680.387016	18.301248
40.062890	1674.144177	18.306266
40.232775	1671.726796	18.311283
40.256926	1678.383576	18.316301
40.138001	1668.400604	18.321319
40.436181	1674.404528	18.326336
40.351886	1673.816247	18.331354
40.555362	1670.568105	18.336371
40.523983	1663.145846	18.341389
40.627344	1671.280063	18.346407
40.565076	1671.755068	18.351424
40.428452	1674.558928	18.356442
40.885426	1672.430627	18.361459
40.704504	1669.646528	18.366477
40.514191	1678.541188	18.371495
40.680508	1674.197225	18.376512
40.620280	1669.987625	18.381530
40.556772	1676.805377	18.386547
40.636439	1699.793986	18.391565
40.929277	1697.948766	18.396583
40.984879	1704.465310	18.401600
40.881466	1705.737290	18.406618
40.957255	1703.032727	18.411635
41.149398	1705.158925	18.416653
41.074401	1689.205249	18.421671
41.085685	1693.035414	18.426688
41.071512	1690.792995	18.431706
41.558018	1694.624002	18.436723
41.320222	1699.567857	18.441741
41.487474	1694.126484	18.446759
41.829418	1695.687716	18.451776
41.269104	1697.259759	18.456794
41.718461	1693.283101	18.461811
41.517419	1694.516915	18.466829
41.334968	1698.194513	18.471847
41.325171	1692.511195	18.476864
41.625409	1695.717923	18.481882
41.772834	1692.256615	18.486899
41.546717	1697.361922	18.491917
41.159101	1693.652589	18.496935
41.731886	1711.529622	18.501952
41.807877	1725.739697	18.506970
42.066535	1716.692606	18.511987
41.895197	1730.636549	18.517005
42.115341	1728.284066	18.522023
42.155878	1722.230983	18.527040
42.215382	1722.198816	18.532058
42.228929	1719.091561	18.537075
42.505230	1715.521507	18.542093
42.624948	1704.932458	18.547111
42.496971	1689.211572	18.552128
42.356233	1681.664103	18.557146
42.683279	1679.972277	18.562163
42.298197	1682.941293	18.567181
42.255206	1686.735168	18.572199
42.248561	1675.319421	18.577216
42.095561	1679.016548	18.582234
42.380365	1680.738815	18.587251
42.429553	1695.060387	18.592269
42.362416	1700.041733	18.597287
42.555633	1711.385519	18.602304
41.934311	1712.275929	18.607322
42.523889	1706.627221	18.612339
42.627751	1715.598392	18.617357
42.653734	1714.697360	18.622375
42.686483	1712.152285	18.627392
42.611215	1722.438954	18.632410
42.677103	1712.732441	18.637427
42.714258	1717.863454	18.642445
42.856840	1727.799486	18.647463
43.461803	1736.792029	18.652480
43.206938	1743.359603	18.657498
43.233940	1734.854012	18.662515
43.160141	1722.824148	18.667533
43.200520	1723.387671	18.672551
43.382631	1732.426998	18.677568
43.299170	1736.311838	18.682586
43.562959	1721.087079	18.687603
43.309963	1714.617244	18.692621
43.342051	1717.858534	18.697639
43.476226	1726.183349	18.702656
43.548384	1727.068778	18.707674
43.552394	1738.093516	18.712691
43.511044	1732.065406	18.717709
43.552780	1727.384573	18.722727
43.782605	1729.820285	18.727744
43.587224	1733.953185	18.732762
43.717877	1735.815156	18.737779
43.864787	1736.325214	18.742797
43.654918	1734.666770	18.747815
43.915790	1736.617811	18.752832
43.685971	1734.891804	18.757850
43.880127	1725.361684	18.762867
44.018045	1727.698439	18.767885
43.646488	1728.666786	18.772903
43.943967	1728.088126	18.777920
43.900614	1742.952627	18.782938
44.023580	1739.880794	18.787955
44.271390	1740.897377	18.792973
44.166652	1754.697636	18.797991
44.449659	1740.333069	18.803008
43.956051	1747.329941	18.808026
44.131984	1751.699399	18.813043
44.337384	1738.209109	18.818061
44.006025	1736.625899	18.823079
44.227447	1747.649292	18.828096
44.446439	1769.370044	18.833114
44.450852	1768.941089	18.838131
44.574393	1775.523187	18.843149
44.528276	1780.544386	18.848167
44.675145	1771.550419	18.853184
44.639895	1783.385242	18.858202
44.954348	1767.933542	18.863219
44.795873	1770.356388	18.868237
45.068012	1776.606398	18.873255
45.202142	1769.375189	18.878272
44.927297	1775.278361	18.883290
45.244722	1772.863701	18.888307
45.274896	1766.568614	18.893325
45.213739	1769.822598	18.898343
45.413250	1764.618381	18.903360
45.198642	1765.991456	18.908378
45.520691	1762.949254	18.913395
45.526661	1767.177171	18.918413
45.254859	1763.686049	18.923431
45.536259	1758.455676	18.928448
45.024000	1759.268187	18.933466
45.359189	1764.378215	18.938483
45.416740	1755.825428	18.943501
45.112507	1764.163011	18.948519
45.474684	1771.751667	18.953536
45.603688	1782.811647	18.958554
45.722474	1787.988223	18.963571
45.991720	1789.056379	18.968589
45.637685	1795.997485	18.973607
45.865231	1792.642575	18.978624
45.323034	1794.488008	18.983642
45.536021	1796.609586	18.988659
45.792411	1793.238482	18.993677
45.538227	1801.638665	18.998695
46.060625	1805.637382	19.003712
46.038888	1825.378362	19.008730
46.332144	1815.261299	19.013747
46.320323	1821.891026	19.018765
46.014270	1828.199390	19.023783
46.286272	1816.163773	19.028800
46.339770	1821.725585	19.033818
46.623031	1826.114695	19.038835
46.867417	1816.060054	19.043853
46.153761	1814.603522	19.048871
46.604282	1824.826035	19.053888
46.486996	1820.326625	19.058906
46.156597	1824.936635	19.063923
46.445034	1819.568855	19.068941
46.554818	1808.729015	19.073959
46.642087	1816.378566	19.078976
46.651268	1820.205568	19.083994
47.086382	1828.264464	19.089011
47.115030	1839.906464	19.094029
46.954728	1826.917994	19.099047
47.159328	1816.876633	19.104064
47.276921	1816.208856	19.109082
47.023537	1812.550103	19.114099
47.567635	1815.566871	19.119117
47.347701	1810.017124	19.124135
47.401622	1798.992837	19.129152
47.126942	1808.468083	19.134170
47.188956	1797.619231	19.139187
47.572397	1806.798496	19.144205
47.521932	1816.812220	19.149223
47.457649	1810.769765	19.154240
47.483720	1824.084641	19.159258
47.424911	1826.968952	19.164275
48.072704	1813.506923	19.169293
47.566335	1824.835131	19.174311
48.061064	1818.467040	19.179328
47.734527	1824.555563	19.184346
47.539152	1825.483326	19.189363
47.955738	1817.290749	19.194381
47.594852	1831.416562	19.199399
47.763624	1826.869391	19.204416
48.042620	1831.347793	19.209434
47.508301	1830.174955	19.214451
47.811255	1820.035417	19.219469
47.813163	1827.230597	19.224487
47.746900	1827.695638	19.229504
48.140913	1843.500823	19.234522
48.039200	1851.120264	19.239539
48.493714	1851.474668	19.244557
48.099616	1855.649164	19.249575
48.614158	1851.472695	19.254592
48.522978	1850.466643	19.259610
48.255681	1853.535482	19.264627
48.385644	1850.708536	19.269645
48.458202	1850.671845	19.274663
48.513335	1845.146226	19.279680
48.646076	1839.387678	19.284698
48.499951	1847.967240	19.289715
48.679949	1849.691526	19.294733
48.760560	1858.501666	19.299751
48.759453	1867.074550	19.304768
49.095196	1873.908173	19.309786
49.127627	1878.225047	19.314803
49.085001	1869.025782	19.319821
49.212705	1871.217792	19.324839
49.317165	1865.897388	19.329856
49.028550	1862.039729	19.334874
49.462550	1870.200409	19.339891
50.014541	1863.819669	19.344909
49.461401	1849.060763	19.349927
49.504202	1843.086786	19.354944
49.847631	1838.278013	19.359962
49.534701	1842.878837	19.364979
49.545329	1828.569918	19.369997
49.306172	1836.834165	19.375015
49.653233	1835.131134	19.380032
49.397006	1831.629543	19.385050
49.294311	1841.372005	19.390067
49.559951	1851.101912	19.395085
49.127603	1871.769614	19.400103
49.266999	1869.322605	19.405120
49.759292	1864.101767	19.410138
49.758292	1868.048578	19.415155
49.623488	1873.185281	19.420173
49.835869	1903.021229	19.425191
49.925581	1895.490618	19.430208
49.998079	1905.749792	19.435226
49.924020	1896.660047	19.440243
50.332740	1899.438220	19.445261
50.203102	1899.298785	19.450279
50.628366	1896.463094	19.455296
50.674815	1892.297582	19.460314
50.510549	1892.326088	19.465331
50.767868	1882.775571	19.470349
50.417116	1898.757672	19.475367
50.479094	1890.516289	19.480384
50.727808	1902.933330	19.485402
50.423731	1896.988027	19.490419
50.682360	1894.701590	19.495437
50.416506	1912.479917	19.500455
50.483104	1917.967152	19.505472
50.634809	1917.280336	19.510490
50.451799	1920.195465	19.515507
50.585571	1918.297816	19.520525
50.718897	1921.858613	19.525543
50.464435	1937.366140	19.530560
51.152061	1944.567130	19.535578
51.467517	1946.110333	19.540595
51.557388	1933.555951	19.545613
51.497832	1936.932149	19.550631
51.587782	1947.857766	19.555648
51.899265	1937.882096	19.560666
51.961442	1937.949095	19.565683
51.695764	1914.639208	19.570701
51.376953	1911.244025	19.575719
51.774031	1909.981532	19.580736
51.967891	1905.058919	19.585754
51.527879	1904.803548	19.590771
51.559078	1912.262820	19.595789
51.821123	1926.489124	19.600807
51.663185	1931.915115	19.605824
51.732870	1943.248029	19.610842
51.816703	1941.118876	19.615859
52.247307	1932.430994	19.620877
51.980125	1945.841775	19.625895
52.039459	1930.763659	19.630912
52.158350	1931.642543	19.635930
51.645448	1938.182449	19.640947
51.954865	1937.077778	19.645965
52.501526	1933.045579	19.650983
52.123596	1930.566498	19.656000
52.239783	1931.397404	19.661018
51.877730	1943.132125	19.666035
52.472281	1959.658177	19.671053
52.259249	1964.049578	19.676071
52.522180	1962.264005	19.681088
52.848243	1967.513017	19.686106
52.531546	1967.606920	19.691123
52.824500	1960.833588	19.696141
52.694583	1962.708416	19.701159
52.673081	1971.569387	19.706176
52.700426	1960.633246	19.711194
52.522411	1968.414988	19.716211
52.864800	1983.366640	19.721229
53.136990	1985.732779	19.726247
53.342050	1989.036432	19.731264
53.644475	1984.498977	19.736282
53.343135	1989.066821	19.741299
53.619387	1986.235708	19.746317
53.598189	1991.446554	19.751335
53.431436	1986.627719	19.756352
53.814294	1981.086373	19.761370
53.648725	1962.035136	19.766387
53.457101	1948.977338	19.771405
53.497012	1960.458899	19.776423
53.457587	1972.239043	19.781440
53.757127	1978.132622	19.786458
53.621542	1982.853732	19.791475
53.782983	1980.175885	19.796493
54.024699	1975.777621	19.801511
53.852218	1979.954433	19.806528
54.108315	1977.047523	19.811546
54.301826	1977.123092	19.816563
54.283241	1986.665888	19.821581
53.992316	1976.090315	19.826599
54.038942	1975.166559	19.831616
54.276706	1971.334711	19.836634
54.419062	1972.062465	19.841651
54.136379	1972.278692	19.846669
54.158646	1967.441558	19.851687
54.295309	1975.837751	19.856704
54.854568	1989.403470	19.861722
54.875719	2005.072522	19.866739
54.815964	1990.571166	19.871757
54.640360	1975.243317	19.876775
54.444948	1980.678285	19.881792
55.273802	1982.169558	19.886810
54.676415	1994.242503	19.891827
54.716259	1994.983294	19.896845
54.832558	1996.285456	19.901863
54.715892	1998.489598	19.906880
55.274291	1982.745713	19.911898
55.058340	1997.614232	19.916915
55.159683	1994.788062	19.921933
55.085350	1998.547831	19.926951
54.731942	1995.899320	19.931968
55.006314	1988.583765	19.936986
54.837033	2005.771785	19.942003
55.153285	2023.019986	19.947021
55.558467	2025.119617	19.952039
55.568936	2025.401875	19.957056
55.467664	2023.097843	19.962074
55.365643	2028.625635	19.967091
55.663641	2031.438307	19.972109
55.743881	2017.216117	19.977127
55.819298	2028.159158	19.982144
56.356835	2024.256403	19.987162
55.884349	2028.857714	19.992179
55.717146	2030.138707	19.997197
55.973761	2023.261520	20.002215
55.669205	2028.551580	20.007232
56.021838	2038.197514	20.012250
56.293228	2050.393197	20.017267
56.460806	2049.900997	20.022285
56.360206	2046.897224	20.027303
56.206786	2055.358026	20.032320
56.448609	2052.715678	20.037338
56.509740	2052.776157	20.042355
56.421646	2047.087956	20.047373
56.746507	2037.266312	20.052391
56.434570	2044.489147	20.057408
56.658611	2033.071951	20.062426
56.514931	2039.850378	20.067443
56.692147	2045.164614	20.072461
56.881204	2047.847686	20.077479
56.448281	2051.182181	20.082496
57.056677	2061.425564	20.087514
56.901326	2067.708678	20.092531
57.232902	2068.442903	20.097549
57.258034	2069.790482	20.102567
56.658326	2078.672051	20.107584
57.162768	2066.875715	20.112602
57.185677	2066.807873	20.117619
56.828365	2066.877791	20.122637
57.447171	2082.080237	20.127655
57.563662	2085.007227	20.132672
57.579649	2082.351083	20.137690
57.430791	2085.492879	20.142707
57.651622	2085.000916	20.147725
58.198060	2087.074804	20.152743
57.843983	2084.153546	20.157760
58.215490	2087.215876	20.162778
58.191061	2082.651407	20.167795
58.156661	2086.177807	20.172813
58.223635	2081.531666	20.177831
57.925987	2079.857796	20.182848
58.684367	2077.490162	20.187866
58.209113	2078.301677	20.192883
58.395314	2076.385091	20.197901
58.442499	2080.994076	20.202919
58.281861	2087.313114	20.207936
58.242456	2070.677541	20.212954
58.442217	2077.235730	20.217971
58.367477	2074.274128	20.222989
58.626570	2080.231926	20.228007
58.440782	2078.095033	20.233024
58.781931	2071.982985	20.238042
58.761578	2068.897809	20.243059
58.560115	2068.505690	20.248077
58.727294	2072.767630	20.253095
58.673563	2076.881497	20.258112
58.534483	2083.384371	20.263130
58.722821	2103.424003	20.268147
58.661224	2107.337600	20.273165
58.677318	2106.433459	20.278183
58.867016	2109.742438	20.283200
58.903096	2120.653080	20.288218
58.721869	2125.955037	20.293235
58.915221	2131.382383	20.298253
59.342074	2126.172689	20.303271
59.152607	2135.030854	20.308288
59.148171	2137.487702	20.313306
59.490579	2159.129509	20.318323
59.577923	2157.425745	20.323341
59.849432	2155.098948	20.328359
59.873764	2164.674118	20.333376
60.112545	2161.546018	20.338394
60.150994	2153.560369	20.343411
60.344520	2164.784748	20.348429
60.525097	2159.274470	20.353447
60.131817	2158.977496	20.358464
60.498220	2148.093749	20.363482
60.493636	2140.886911	20.368499
60.678878	2136.599925	20.373517
60.439703	2115.209034	20.378535
60.388027	2122.268336	20.383552
60.373371	2124.900896	20.388570
60.310661	2128.585541	20.393587
60.238669	2148.248636	20.398605
60.578361	2147.220438	20.403623
60.555774	2155.172607	20.408640
60.597127	2159.370363	20.413658
60.912017	2152.548039	20.418675
60.675732	2157.394934	20.423693
60.775024	2154.810422	20.428711
60.649298	2155.747932	20.433728
60.910924	2152.770781	20.438746
60.870469	2163.876415	20.443763
60.880525	2180.093562	20.448781
60.997393	2183.408710	20.453799
60.912347	2185.218653	20.458816
61.236103	2183.141872	20.463834
61.397529	2182.731005	20.468851
61.255452	2192.494774	20.473869
61.842526	2203.179200	20.478887
61.605412	2212.149632	20.483904
61.645980	2214.029334	20.488922
62.350024	2200.889169	20.493939
61.771528	2194.507279	20.498957
61.799752	2180.645534	20.503975
61.954414	2187.293129	20.508992
62.115649	2198.971715	20.514010
62.304302	2198.129945	20.519027
62.183606	2200.055245	20.524045
62.485879	2192.581032	20.529063
62.169138	2201.008322	20.534080
62.365523	2203.759501	20.539098
62.825541	2193.279924	20.544115
62.251157	2192.145974	20.549133
62.582598	2184.490945	20.554151
62.438008	2191.683777	20.559168
62.366597	2191.966603	20.564186
62.658981	2188.952856	20.569203
62.455731	2191.262309	20.574221
62.881591	2188.526472	20.579239
62.833833	2190.605842	20.584256
62.807731	2185.703418	20.589274
63.015929	2176.936867	20.594291
62.766072	2187.033057	20.599309
62.653700	2184.637922	20.604327
62.731176	2207.775685	20.609344
62.872074	2213.272770	20.614362
63.117909	2217.961114	20.619379
63.178256	2217.938650	20.624397
63.291277	2209.863456	20.629415
63.459825	2216.841848	20.634432
63.395700	2218.203825	20.639450
63.567775	2206.125395	20.644467
63.453028	2222.636096	20.649485
63.454345	2235.510918	20.654503
64.117016	2246.159234	20.659520
64.051956	2249.895480	20.664538
64.009136	2245.447792	20.669555
63.821673	2247.435335	20.674573
64.057651	2246.648328	20.679591
64.409748	2245.653505	20.684608
63.932566	2247.768155	20.689626
64.260432	2240.112115	20.694643
63.945272	2238.482861	20.699661
64.259831	2236.318222	20.704679
64.045307	2243.904956	20.709696
64.323441	2243.031833	20.714714
64.557576	2229.732037	20.719731
64.333422	2231.816602	20.724749
64.482256	2241.558615	20.729767
64.441660	2258.936245	20.734784
64.450888	2260.462466	20.739802
65.160939	2254.822753	20.744819
64.997463	2267.982772	20.749837
64.903474	2261.652134	20.754855
64.927753	2260.784425	20.759872
64.973971	2263.990812	20.764890
65.386822	2248.764874	20.769907
65.016221	2256.505808	20.774925
65.279048	2252.994953	20.779943
65.312560	2249.620103	20.784960
65.069614	2269.970345	20.789978
65.496422	2283.987801	20.794995
65.404269	2286.993470	20.800013
65.472559	2289.288294	20.805031
65.736931	2283.756618	20.810048
65.537996	2286.857136	20.815066
65.721285	2287.769081	20.820083
65.628226	2289.276018	20.825101
65.688110	2277.199180	20.830119
65.853764	2293.988346	20.835136
65.789352	2305.351208	20.840154
66.074380	2307.751494	20.845171
66.066320	2313.465413	20.850189
66.291731	2314.980649	20.855207
66.431414	2307.972692	20.860224
66.428257	2315.825658	20.865242
66.440391	2306.889127	20.870259
66.400915	2319.061686	20.875277
66.341311	2310.383497	20.880295
66.146232	2323.268074	20.885312
66.300807	2339.941796	20.890330
66.732644	2343.473345	20.895347
66.723277	2344.789651	20.900365
66.852072	2335.461328	20.905383
67.028786	2328.159422	20.910400
67.005569	2337.383500	20.915418
67.303103	2340.930199	20.920435
67.476650	2348.634234	20.925453
67.537381	2333.040512	20.930471
67.238368	2327.986764	20.935488
67.415031	2348.510164	20.940506
67.795939	2354.900676	20.945523
67.706598	2357.790140	20.950541
67.617367	2339.781755	20.955559
67.859283	2338.618547	20.960576
67.935571	2344.105510	20.965594
68.204931	2349.199860	20.970611
68.166532	2335.501771	20.975629
67.776862	2328.113712	20.980647
68.170309	2318.057692	20.985664
67.659463	2334.165962	20.990682
67.978169	2337.848925	20.995699
67.858454	2353.270379	21.000717
68.061180	2349.294628	21.005735
68.192068	2352.425987	21.010752
68.138882	2347.097661	21.015770
68.242593	2340.696067	21.020787
68.257949	2352.392229	21.025805
68.051767	2356.901114	21.030823
68.558039	2366.143451	21.035840
68.522236	2378.489472	21.040858
68.811834	2377.002997	21.045875
68.557989	2375.268294	21.050893
68.254591	2376.217911	21.055911
68.655292	2376.701720	21.060928
69.028082	2395.875716	21.065946
68.933321	2400.916193	21.070963
69.097233	2404.402743	21.075981
69.386853	2396.823436	21.080999
69.136111	2394.692922	21.086016
69.101846	2394.982201	21.091034
69.560434	2392.597622	21.096051
69.582471	2398.317613	21.101069
69.943717	2393.684077	21.106087
69.995836	2379.977654	21.111104
69.937205	2393.424765	21.116122
70.038832	2389.384637	21.121139
70.367509	2391.997799	21.126157
70.132528	2390.224537	21.131175
70.375936	2387.762589	21.136192
70.036516	2389.385132	21.141210
70.102733	2391.155485	21.146227
70.483275	2388.064502	21.151245
70.536031	2384.077745	21.156263
70.266227	2383.716224	21.161280
69.887704	2387.817411	21.166298
69.973244	2402.728921	21.171315
70.349043	2412.722847	21.176333
70.054460	2421.999387	21.181351
70.928221	2416.802222	21.186368
70.672535	2430.291834	21.191386
71.010307	2428.854073	21.196403
71.229006	2434.809640	21.201421
71.285845	2437.553650	21.206439
71.329478	2437.502455	21.211456
71.158658	2436.108742	21.216474
71.579019	2426.747839	21.221491
71.557474	2430.409204	21.226509
71.329257	2435.128463	21.231527
71.604561	2423.889905	21.236544
71.890642	2427.579472	21.241562
71.886815	2420.659402	21.246579
72.281274	2412.115043	21.251597
71.858163	2413.280555	21.256615
71.667201	2394.403079	21.261632
71.888197	2404.692329	21.266650
72.067259	2402.611523	21.271667
72.000500	2410.670354	21.276685
71.946447	2422.762333	21.281703
72.376778	2414.085649	21.286720
72.133036	2419.043707	21.291738
72.196570	2422.807918	21.296755
72.302072	2414.332661	21.301773
72.304435	2422.274536	21.306791
72.180032	2421.672787	21.311808
71.866453	2424.004478	21.316826
72.416142	2442.750798	21.321843
72.578759	2448.524701	21.326861
72.509813	2446.660947	21.331879
72.691630	2450.931592	21.336896
72.781684	2449.916361	21.341914
73.065363	2448.637169	21.346931
73.112319	2449.770921	21.351949
73.015316	2448.637440	21.356967
73.007500	2445.210726	21.361984
72.964706	2462.249953	21.367002
73.107008	2468.503237	21.372019
73.355367	2470.507630	21.377037
73.630077	2472.771060	21.382055
73.676689	2468.845932	21.387072
73.920085	2476.616424	21.392090
73.518257	2472.958073	21.397107
73.750801	2470.378613	21.402125
73.816157	2479.835368	21.407143
74.169452	2467.963752	21.412160
73.917760	2463.754533	21.417178
73.783195	2464.195466	21.422195
74.072311	2485.618195	21.427213
74.191725	2496.253083	21.432231
74.199138	2493.193149	21.437248
74.302158	2501.399517	21.442266
74.375103	2495.051381	21.447283
74.688118	2493.341714	21.452301
74.488775	2501.828866	21.457319
74.882106	2494.205568	21.462336
74.850246	2497.387132	21.467354
75.152794	2499.258928	21.472371
75.168923	2491.604772	21.477389
74.737941	2498.147880	21.482407
74.911967	2488.869854	21.487424
74.993951	2494.343328	21.492442
75.043174	2508.788093	21.497459
75.111075	2520.927282	21.502477
74.937724	2510.603545	21.507495
75.352257	2508.332943	21.512512
75.160861	2510.520000	21.517530
75.456080	2512.332771	21.522547
75.765445	2524.768224	21.527565
75.581722	2546.106323	21.532583
75.719040	2541.735030	21.537600
75.919666	2542.231104	21.542618
76.077184	2548.079121	21.547635
76.199496	2538.060372	21.552653
75.850947	2541.537701	21.557671
76.262109	2544.217946	21.562688
76.265580	2535.491784	21.567706
76.166970	2537.426854	21.572723
76.125734	2533.924153	21.577741
76.232093	2552.859763	21.582759
76.949462	2560.605368	21.587776
76.716753	2559.521515	21.592794
77.092910	2559.428651	21.597811
77.118795	2546.880825	21.602829
76.960958	2562.803316	21.607847
77.142977	2549.552431	21.612864
77.491631	2548.551073	21.617882
77.360809	2554.001138	21.622899
77.669112	2545.564678	21.627917
77.485740	2528.094527	21.632935
77.544099	2516.737482	21.637952
77.211918	2521.405078	21.642970
76.668939	2524.921683	21.647987
77.356433	2534.080571	21.653005
77.444098	2540.037794	21.658023
77.215171	2543.587449	21.663040
77.271882	2552.429896	21.668058
77.445306	2573.570702	21.673075
77.749461	2578.915683	21.678093
77.520433	2586.445532	21.683111
77.932492	2592.080151	21.688128
78.167526	2587.171375	21.693146
78.042622	2591.628284	21.698163
78.024566	2585.217221	21.703181
77.948296	2604.494963	21.708199
78.106750	2606.695373	21.713216
78.178381	2608.242400	21.718234
78.273832	2616.277236	21.723251
78.505316	2605.904913	21.728269
78.903316	2628.219317	21.733287
79.039228	2628.056380	21.738304
79.225104	2636.234533	21.743322
79.418004	2632.016621	21.748339
79.599278	2614.634828	21.753357
79.246679	2603.824926	21.758375
79.538525	2601.510447	21.763392
79.287406	2588.924587	21.768410
79.205811	2603.510397	21.773427
79.671764	2614.089566	21.778445
79.743227	2620.197150	21.783463
79.618240	2622.546073	21.788480
79.770461	2616.809212	21.793498
79.731881	2617.573255	21.798515
80.005401	2622.454002	21.803533
79.728817	2625.166236	21.808551
79.778433	2624.665596	21.813568
80.003313	2627.652307	21.818586
79.808426	2629.217870	21.823603
80.208640	2641.964382	21.828621
80.328025	2651.693416	21.833639
79.795757	2655.231899	21.838656
80.061206	2657.828802	21.843674
80.203718	2663.297039	21.848691
80.569699	2675.124380	21.853709
81.041468	2684.552162	21.858727
80.895332	2678.594973	21.863744
80.903382	2678.876463	21.868762
80.847034	2683.597264	21.873779
81.124442	2685.618924	21.878797
81.023965	2677.302835	21.883815
80.927579	2675.545177	21.888832
81.377346	2683.067416	21.893850
81.218702	2693.828011	21.898867
81.645795	2691.847844	21.903885
81.636569	2702.038392	21.908903
81.863463	2691.131302	21.913920
81.878196	2700.425695	21.918938
81.541511	2696.275762	21.923955
82.089933	2691.313885	21.928973
81.915044	2704.041878	21.933991
82.134715	2702.963436	21.939008
82.089402	2693.195190	21.944026
81.916802	2701.816615	21.949043
82.430229	2708.734978	21.954061
82.321328	2720.038181	21.959079
82.447643	2719.428769	21.964096
82.641226	2718.646791	21.969114
82.549483	2724.525121	21.974131
82.679543	2714.574665	21.979149
82.723310	2724.692277	21.984167
82.727155	2724.487815	21.989184
83.153745	2715.460773	21.994202
82.700815	2715.994977	21.999219
83.221520	2711.091230	22.004237
83.253220	2718.600022	22.009255
83.077064	2717.297725	22.014272
83.553143	2727.382346	22.019290
83.540917	2740.204706	22.024307
83.495268	2735.730178	22.029325
83.898438	2741.139537	22.034343
83.957465	2740.735374	22.039360
84.420715	2727.680312	22.044378
83.795899	2719.916794	22.049395
84.274719	2708.467552	22.054413
84.159415	2711.130655	22.059431
83.710981	2706.124751	22.064448
84.155395	2713.314798	22.069466
84.089775	2720.120756	22.074483
84.302303	2728.593385	22.079501
84.231295	2730.963310	22.084519
84.528648	2726.538302	22.089536
84.387717	2734.219395	22.094554
84.295988	2734.493389	22.099571
84.759553	2749.988360	22.104589
84.659806	2764.643079	22.109607
84.562550	2758.620282	22.114624
85.207618	2759.544784	22.119642
84.699129	2764.829875	22.124659
84.913023	2756.561700	22.129677
85.017013	2763.306916	22.134695
85.070652	2772.979584	22.139712
85.282257	2774.879465	22.144730
85.135617	2782.917065	22.149747
85.427840	2774.304392	22.154765
85.603041	2790.374745	22.159783
85.533414	2804.366984	22.164800
85.973001	2801.654759	22.169818
85.769665	2802.296077	22.174835
86.061572	2799.746896	22.179853
86.160371	2793.786120	22.184871
85.975932	2799.127422	22.189888
86.241127	2792.395733	22.194906
86.468263	2809.361119	22.199923
86.518143	2818.989159	22.204941
86.476686	2821.238055	22.209959
86.404319	2825.507185	22.214976
86.764657	2817.995894	22.219994
86.533028	2820.677094	22.225011
86.578482	2817.873810	22.230029
87.366787	2814.536479	22.235047
87.241104	2822.076892	22.240064
87.390200	2815.026595	22.245082
87.375252	2824.477956	22.250099
87.350367	2828.091931	22.255117
87.429489	2835.199591	22.260135
87.413227	2850.150828	22.265152
87.856120	2842.914069	22.270170
87.768174	2848.298471	22.275187
87.564441	2847.147589	22.280205
88.319353	2840.825783	22.285223
87.843066	2846.904845	22.290240
88.134787	2836.188512	22.295258
88.044135	2834.669275	22.300275
88.093050	2834.755798	22.305293
88.287136	2842.631497	22.310311
88.049359	2849.679811	22.315328
88.604131	2856.979616	22.320346
88.448338	2857.668581	22.325363
88.424751	2865.536233	22.330381
88.468799	2863.747034	22.335399
88.531241	2867.900541	22.340416
88.706022	2860.210093	22.345434
89.105926	2872.659972	22.350451
89.175930	2885.770042	22.355469
89.346098	2894.799821	22.360487
88.982172	2897.450964	22.365504
89.065406	2895.618657	22.370522
89.211135	2894.469366	22.375539
89.199527	2895.989256	22.380557
89.409619	2895.243909	22.385575
89.073575	2902.219927	22.390592
89.672150	2907.588724	22.395610
89.517535	2914.466592	22.400627
89.579572	2912.694096	22.405645
89.945628	2911.042145	22.410663
89.786132	2918.297627	22.415680
89.801015	2937.094506	22.420698
89.947337	2941.426287	22.425715
90.343642	2941.951007	22.430733
90.817368	2940.321387	22.435751
90.545531	2943.788858	22.440768
90.601520	2937.144900	22.445786
90.661814	2949.337656	22.450803
90.823793	2963.281061	22.455821
91.262907	2964.655460	22.460839
91.024863	2960.459594	22.465856
91.466086	2959.436193	22.470874
91.389582	2962.314981	22.475891
91.549842	2966.583039	22.480909
91.647150	2956.665020	22.485927
91.533493	2957.623021	22.490944
91.718585	2953.931558	22.495962
91.496573	2951.760379	22.500979
91.722862	2958.058229	22.505997
91.839277	2959.221466	22.511015
91.944522	2955.460538	22.516032
92.012572	2957.018824	22.521050
92.069892	2972.442290	22.526067
92.128109	2979.968473	22.531085
92.445147	2984.332637	22.536103
92.221325	2991.122776	22.541120
92.458679	2988.470776	22.546138
92.784292	2987.820090	22.551155
92.294083	2988.817206	22.556173
92.637356	2984.693212	22.561191
92.677443	3005.015269	22.566208
92.864759	3010.716783	22.571226
93.036140	3011.056677	22.576243
93.149245	3012.611840	22.581261
93.050253	3007.614916	22.586279
92.780952	3016.645473	22.591296
93.062415	3026.269160	22.596314
93.179679	3031.890146	22.601331
93.146670	3043.825564	22.606349
93.601643	3037.607676	22.611367
93.365314	3052.179756	22.616384
93.735261	3061.710856	22.621402
93.901457	3073.097519	22.626419
93.884144	3067.312571	22.631437
94.147908	3056.387705	22.636455
94.363259	3064.749804	22.641472
94.590337	3054.865360	22.646490
94.419456	3062.618115	22.651507
94.592781	3077.717725	22.656525
94.970996	3082.540336	22.661543
94.975459	3083.952454	22.666560
94.984189	3084.640570	22.671578
95.109579	3087.998995	22.676595
95.195657	3083.775418	22.681613
95.288968	3082.309959	22.686631
95.072631	3089.713920	22.691648
95.573961	3073.713407	22.696666
95.687180	3084.508400	22.701683
95.192209	3078.354852	22.706701
95.669364	3076.812849	22.711719
95.342659	3084.931603	22.716736
95.307734	3085.256439	22.721754
95.453052	3083.462261	22.726771
95.807278	3108.047020	22.731789
95.975907	3108.413753	22.736807
95.613437	3108.839281	22.741824
95.843533	3108.579243	22.746842
96.060498	3113.701816	22.751859
96.014757	3132.167990	22.756877
96.341989	3137.367599	22.761895
96.639462	3150.974141	22.766912
96.441719	3143.759839	22.771930
96.978197	3140.221200	22.776947
96.758702	3133.269585	22.781965
97.146162	3140.519660	22.786983
96.948507	3153.109254	22.792000
97.078844	3161.095284	22.797018
96.995740	3154.830991	22.802035
96.470328	3160.661587	22.807053
97.344937	3171.132530	22.812071
97.550820	3190.496970	22.817088
97.257018	3194.850111	22.822106
97.876048	3196.384134	22.827123
97.452150	3190.670394	22.832141
97.953486	3188.227042	22.837159
97.747929	3210.395336	22.842176
98.091064	3219.894748	22.847194
98.286895	3224.506630	22.852211
98.034097	3227.018944	22.857229
98.467055	3218.769775	22.862247
98.379481	3222.306022	22.867264
98.522879	3234.429724	22.872282
98.979486	3236.124909	22.877299
99.105609	3253.051590	22.882317
99.183870	3237.706451	22.887335
99.354279	3247.184472	22.892352
99.061110	3247.543799	22.897370
99.299863	3241.831364	22.902387
99.234142	3239.051529	22.907405
99.453642	3240.977723	22.912423
99.348818	3232.531728	22.917440
99.150655	3243.971360	22.922458
99.710242	3251.049273	22.927475
99.473345	3258.335444	22.932493
99.770064	3266.234920	22.937511
99.565483	3270.013802	22.942528
100.156451	3279.628535	22.947546
100.293956	3279.947664	22.952563
100.243178	3293.126110	22.957581
100.189840	3291.201789	22.962599
100.225573	3285.269380	22.967616
100.110341	3295.622370	22.972634
100.627882	3313.616718	22.977651
100.610518	3325.610791	22.982669
101.095480	3314.656210	22.987687
101.252156	3324.370041	22.992704
101.103015	3325.489074	22.997722
101.076081	3316.255643	23.002739
101.369084	3331.864090	23.007757
101.636286	3340.310282	23.012775
101.613135	3344.645035	23.017792
101.682142	3361.665158	23.022810
102.006088	3351.286091	23.027827
101.826920	3353.400759	23.032845
101.966279	3348.361507	23.037863
101.992128	3351.503372	23.042880
101.838706	3353.047179	23.047898
101.955585	3350.009508	23.052915
101.721067	3350.178398	23.057933
102.139017	3363.087151	23.062951
102.354197	3368.055756	23.067968
102.288327	3387.192567	23.072986
102.487726	3375.079968	23.078003
102.508002	3385.070386	23.083021
103.173797	3395.687484	23.088039
103.428058	3402.531733	23.093056
103.043260	3402.949152	23.098074
103.437802	3393.749056	23.103091
103.239482	3398.243549	23.108109
103.370734	3394.962912	23.113127
103.250191	3390.550601	23.118144
103.429996	3398.559276	23.123162
103.568987	3406.041579	23.128179
103.660287	3421.984332	23.133197
103.651441	3424.261777	23.138215
103.899997	3419.017394	23.143232
103.684433	3429.381965	23.148250
104.308140	3446.354048	23.153267
104.276750	3456.631445	23.158285
104.470728	3458.798927	23.163303
104.310587	3446.276060	23.168320
104.312942	3451.998909	23.173338
104.598090	3477.123702	23.178355
104.621773	3478.284613	23.183373
104.933962	3481.897663	23.188391
105.255357	3481.933172	23.193408
104.707646	3483.070560	23.198426
105.232111	3484.695870	23.203443
105.435374	3497.517824	23.208461
105.714903	3500.535032	23.213479
105.786011	3499.702027	23.218496
105.681367	3499.749009	23.223514
105.804982	3488.423767	23.228531
105.853035	3497.958817	23.233549
106.199898	3514.753949	23.238567
106.437152	3535.731536	23.243584
106.310569	3535.523064	23.248602
106.604526	3528.645338	23.253619
106.395509	3530.519272	23.258637
106.494421	3530.784553	23.263655
106.813546	3524.373585	23.268672
106.651876	3532.825132	23.273690
106.617748	3529.704935	23.278707
106.918412	3545.204045	23.283725
107.128525	3551.958413	23.288743
107.427578	3550.918748	23.293760
107.286571	3554.380835	23.298778
107.680827	3545.789041	23.303795
107.720638	3549.310965	23.308813
107.732046	3553.279773	23.313831
108.217433	3543.147901	23.318848
107.831490	3548.313736	23.323866
108.093317	3545.938336	23.328883
108.359137	3563.194237	23.333901
107.997394	3566.305422	23.338919
108.328722	3564.696562	23.343936
108.371985	3564.583214	23.348954
108.790970	3565.261309	23.353971
108.399076	3571.625925	23.358989
108.474605	3562.500597	23.364007
108.479457	3569.385425	23.369024
108.344739	3591.866979	23.374042
108.799004	3596.992555	23.379059
108.870363	3599.448897	23.384077
108.659852	3600.871454	23.389095
109.086789	3611.833403	23.394112
108.684853	3626.712210	23.399130
109.423320	3621.046055	23.404147
109.398543	3625.609924	23.409165
109.337847	3652.694472	23.414183
109.878160	3661.112947	23.419200
109.911377	3660.589789	23.424218
110.173801	3655.401308	23.429235
110.346166	3654.595630	23.434253
110.189110	3660.677275	23.439271
110.554167	3656.460513	23.444288
110.513296	3674.880845	23.449306
110.815246	3673.609166	23.454323
110.750705	3676.053763	23.459341
110.946844	3675.914315	23.464359
110.924624	3665.118275	23.469376
111.005428	3669.535132	23.474394
111.436471	3670.456939	23.479411
111.425871	3695.011280	23.484429
111.532244	3693.706222	23.489447
111.788373	3696.783650	23.494464
111.734860	3696.714673	23.499482
111.615975	3694.407007	23.504499
111.808993	3695.965940	23.509517
111.562602	3695.440642	23.514535
112.154413	3710.860214	23.519552
112.041891	3725.549054	23.524570
112.188194	3723.719990	23.529587
112.324976	3725.788304	23.534605
112.089173	3724.052821	23.539623
112.734037	3732.625703	23.544640
112.927092	3754.867766	23.549658
112.615662	3753.032187	23.554675
112.930518	3756.455858	23.559693
112.844088	3758.566644	23.564711
113.042143	3751.700368	23.569728
113.465332	3778.088793	23.574746
113.483888	3777.448357	23.579763
113.489996	3777.166331	23.584781
113.562956	3777.518996	23.589799
113.878503	3782.451034	23.594816
113.342132	3787.739110	23.599834
113.837139	3810.110812	23.604851
114.125732	3812.177629	23.609869
114.190008	3810.216052	23.614887
114.389532	3815.961123	23.619904
114.348128	3843.800393	23.624922
114.128647	3843.011936	23.629939
114.759753	3845.963917	23.634957
114.775856	3846.009810	23.639975
114.583954	3840.281832	23.644992
114.681289	3859.531195	23.650010
115.207318	3866.490127	23.655027
115.446292	3869.727145	23.660045
115.408558	3871.270354	23.665063
115.678385	3857.590775	23.670080
115.572191	3867.313421	23.675098
115.610791	3872.513814	23.680115
115.882049	3891.598181	23.685133
115.859065	3890.731120	23.690151
116.034413	3888.764139	23.695168
116.194252	3891.952443	23.700186
116.346877	3884.217912	23.705203
116.435550	3887.723160	23.710221
116.105411	3905.610862	23.715239
116.634689	3915.787072	23.720256
116.676085	3918.665021	23.725274
116.799355	3920.156773	23.730291
117.059435	3919.813009	23.735309
117.066715	3928.123393	23.740327
116.935046	3918.539964	23.745344
116.943339	3939.831632	23.750362
117.288261	3948.757881	23.755379
117.438669	3940.555509	23.760397
117.552965	3952.933049	23.765415
117.883241	3961.879843	23.770432
117.877462	3977.693543	23.775450
118.185539	3971.784300	23.780467
118.296569	3974.754684	23.785485
118.368016	3981.550310	23.790503
118.489200	3969.136376	23.795520
118.672499	3972.512968	23.800538
118.208178	3971.178731	23.805555
118.747375	3973.675017	23.810573
118.779371	3990.636981	23.815591
119.083417	3982.861189	23.820608
118.778656	3989.726190	23.825626
119.029200	3990.276265	23.830643
119.424471	3998.372034	23.835661
119.224758	4016.433967	23.840679
119.316931	4022.772566	23.845696
119.592437	4022.829458	23.850714
119.412134	4016.745109	23.855731
119.816075	4039.462189	23.860749
119.795131	4049.541364	23.865767
119.683778	4045.063951	23.870784
120.133822	4052.803383	23.875802
120.397954	4072.647144	23.880819
120.248378	4074.080916	23.885837
120.677937	4072.662469	23.890855
120.924931	4070.618239	23.895872
121.052365	4074.578996	23.900890
121.190194	4091.183336	23.905907
121.040487	4098.238496	23.910925
121.217535	4104.073235	23.915943
121.439404	4108.354639	23.920960
121.880258	4099.079526	23.925978
121.772720	4102.379080	23.930995
122.092437	4096.230819	23.936013
121.831549	4095.314930	23.941031
122.213905	4111.025916	23.946048
121.935725	4117.167560	23.951066
122.081090	4129.214847	23.956083
122.475898	4126.219217	23.961101
122.497519	4136.250449	23.966119
122.474329	4133.620919	23.971136
122.457120	4137.243376	23.976154
122.707755	4152.498182	23.981171
123.104409	4156.438800	23.986189
122.806210	4161.964778	23.991207
122.838112	4160.885432	23.996224
123.355078	4177.626339	24.001242
123.058750	4190.843829	24.006259
123.420021	4186.503125	24.011277
123.506057	4193.053080	24.016295
123.776866	4199.917385	24.021312
123.818956	4206.691192	24.026330
123.606180	4210.719334	24.031347
124.169796	4205.116574	24.036365
123.872990	4231.338698	24.041383
124.229453	4235.083595	24.046400
124.556612	4244.306704	24.051418
124.475314	4256.819245	24.056435
124.593627	4241.583049	24.061453
124.650189	4259.291756	24.066471
124.668319	4272.697451	24.071488
124.823630	4272.230845	24.076506
124.956471	4275.181925	24.081523
125.291524	4292.386217	24.086541
125.501358	4297.843095	24.091559
125.824821	4300.547623	24.096576
126.259084	4306.060277	24.101594
125.926179	4301.150099	24.106611
125.991916	4300.810939	24.111629
126.136326	4301.548705	24.116647
126.264794	4312.722402	24.121664
126.135687	4320.461771	24.126682
126.379481	4336.200649	24.131699
126.517288	4323.494657	24.136717
126.743777	4326.211307	24.141735
127.083977	4348.225091	24.146752
127.198557	4358.268639	24.151770
126.772964	4362.984922	24.156787
127.051172	4360.720489	24.161805
127.357200	4365.757458	24.166823
127.546456	4379.425516	24.171840
127.709940	4383.329192	24.176858
127.610304	4387.412675	24.181875
127.685611	4378.475921	24.186893
127.919521	4394.996947	24.191911
128.120380	4405.443638	24.196928
128.308400	4399.290286	24.201946
128.042816	4411.378261	24.206963
128.288753	4410.474524	24.211981
128.825519	4423.084121	24.216999
129.064029	4425.458579	24.222016
129.441647	4429.870221	24.227034
129.071767	4427.054688	24.232051
129.432784	4422.639145	24.237069
129.159584	4421.537052	24.242087
129.394581	4422.535467	24.247104
129.797507	4439.809801	24.252122
129.617206	4443.914530	24.257139
129.980257	4443.918341	24.262157
130.032236	4450.387412	24.267175
130.030061	4453.883020	24.272192
130.037895	4462.790555	24.277210
130.032488	4474.851255	24.282227
130.477419	4474.905302	24.287245
130.366842	4489.980037	24.292263
130.550128	4499.618527	24.297280
130.859365	4507.939080	24.302298
130.967160	4510.080027	24.307315
131.058004	4507.756026	24.312333
131.302098	4526.720839	24.317351
130.999692	4538.756729	24.322368
131.448581	4538.880213	24.327386
131.555274	4543.330440	24.332403
131.676816	4548.572847	24.337421
131.764626	4568.553534	24.342439
131.885507	4570.012667	24.347456
132.056431	4571.742307	24.352474
132.139569	4579.498643	24.357491
132.504712	4592.930642	24.362509
132.497413	4595.256041	24.367527
132.550284	4599.578160	24.372544
132.964791	4596.924130	24.377562
133.024334	4615.066685	24.382579
133.022685	4624.145205	24.387597
133.299902	4621.962017	24.392615
133.180177	4632.069732	24.397632
133.386125	4627.797151	24.402650
133.367469	4625.633020	24.407667
133.512705	4648.419016	24.412685
133.888580	4655.645729	24.417703
133.674763	4656.447545	24.422720
133.925880	4649.780402	24.427738
134.043337	4670.947880	24.432755
134.398621	4683.051408	24.437773
134.424717	4689.656384	24.442791
134.099860	4692.628976	24.447808
134.546616	4702.218459	24.452826
134.614668	4711.935223	24.457843
134.870169	4711.073203	24.462861
135.139794	4734.755447	24.467879
135.243589	4747.587411	24.472896
135.621454	4735.853358	24.477914
135.338747	4743.875107	24.482931
135.978959	4741.445944	24.487949
136.127275	4762.602137	24.492967
136.198010	4774.476410	24.497984
136.699966	4756.433917	24.503002
136.477049	4770.537555	24.508019
136.897172	4768.322814	24.513037
136.950756	4764.069121	24.518055
136.545349	4763.529156	24.523072
136.759921	4766.455772	24.528090
137.297141	4789.586608	24.533107
137.023373	4785.495787	24.538125
137.289645	4791.610559	24.543143
137.194818	4803.554005	24.548160
137.612746	4787.599038	24.553178
137.336222	4818.951317	24.558195
137.495759	4829.807576	24.563213
137.799604	4824.939088	24.568231
137.609790	4845.040119	24.573248
138.169136	4852.201108	24.578266
138.468283	4866.258568	24.583283
138.653421	4862.256354	24.588301
138.562337	4865.815602	24.593319
138.647865	4880.805477	24.598336
139.016344	4878.994628	24.603354
139.128927	4880.590626	24.608371
139.342832	4881.661081	24.613389
139.042450	4889.970930	24.618407
139.408440	4900.867877	24.623424
139.660373	4906.538518	24.628442
139.505050	4911.388995	24.633459
139.717423	4918.930361	24.638477
139.851777	4932.689109	24.643495
139.448244	4940.944393	24.648512
140.458918	4949.803525	24.653530
140.478218	4964.471302	24.658547
140.698499	4960.670376	24.663565
140.624086	4956.837907	24.668583
140.854360	4965.174927	24.673600
141.335738	4977.055402	24.678618
141.579757	4977.013554	24.683635
141.767738	4979.717005	24.688653
141.751265	4985.571510	24.693671
141.821428	4980.289596	24.698688
141.934612	4979.382605	24.703706
141.856069	4986.591769	24.708723
141.979628	4990.225770	24.713741
142.198628	5004.801456	24.718759
142.094605	5016.794627	24.723776
142.335956	5001.812190	24.728794
142.644021	5009.228285	24.733811
142.605258	5011.683391	24.738829
142.811104	5020.185149	24.743847
142.776562	5038.739130	24.748864
142.743268	5042.959076	24.753882
142.893442	5053.809951	24.758899
142.710244	5078.237905	24.763917
143.095874	5082.202639	24.768935
143.133880	5088.312788	24.773952
143.434448	5104.857392	24.778970
143.748341	5113.817797	24.783987
143.923129	5119.124825	24.789005
144.370735	5129.860355	24.794023
144.492897	5138.326415	24.799040
144.220856	5128.090530	24.804058
144.501380	5137.198238	24.809075
144.838464	5151.386711	24.814093
145.093229	5163.629326	24.819111
145.050565	5156.997219	24.824128
145.278996	5161.755100	24.829146
145.204709	5185.327992	24.834163
145.308960	5187.908301	24.839181
145.819489	5191.377474	24.844199
145.587163	5200.733940	24.849216
146.006309	5213.435318	24.854234
146.458307	5220.715060	24.859251
146.135001	5221.622451	24.864269
146.446833	5219.512998	24.869287
146.374892	5234.425318	24.874304
146.639861	5247.802793	24.879322
146.693361	5257.401016	24.884339
147.219553	5257.245509	24.889357
147.320022	5269.546830	24.894375
147.392950	5279.861703	24.899392
147.577859	5283.082371	24.904410
147.700477	5288.787160	24.909427
147.843219	5288.570697	24.914445
148.301857	5283.723698	24.919463
147.934022	5297.050035	24.924480
148.260797	5307.245717	24.929498
148.424878	5315.062261	24.934515
148.192575	5317.039886	24.939533
148.690255	5323.237844	24.944551
148.295283	5343.857840	24.949568
148.634434	5342.163635	24.954586
148.793559	5347.118917	24.959603
148.938765	5374.281813	24.964621
149.589098	5369.520405	24.969639
149.484836	5371.977746	24.974656
149.583020	5381.041749	24.979674
149.920671	5394.387626	24.984691
149.746459	5395.138027	24.989709
149.953745	5400.832778	24.994727
150.211881	5416.594780	24.999744
150.173420	5421.620601	25.004762
150.345286	5430.566896	25.009779
150.731886	5446.491958	25.014797
150.893542	5448.572136	25.019815
151.054014	5450.853346	25.024832
151.316633	5456.314492	25.029850
151.746384	5475.147327	25.034867
151.581996	5485.259830	25.039885
151.782605	5478.739319	25.044903
151.665447	5480.630956	25.049920
152.014742	5482.403628	25.054938
151.997289	5485.434950	25.059955
152.262591	5515.711265	25.064973
152.314661	5512.321615	25.069991
152.242404	5511.276748	25.075008
152.600322	5523.119007	25.080026
152.784750	5537.607973	25.085043
152.870165	5552.779653	25.090061
153.173732	5532.579596	25.095079
153.007307	5546.574549	25.100096
153.379648	5560.500797	25.105114
153.852208	5571.278181	25.110131
153.610234	5573.857589	25.115149
153.865731	5564.587895	25.120167
153.900646	5580.651649	25.125184
153.848448	5589.098773	25.130202
154.415152	5601.946160	25.135219
154.478910	5598.718378	25.140237
154.548364	5611.590598	25.145255
154.766656	5626.465478	25.150272
154.919892	5630.939812	25.155290
155.089234	5634.305686	25.160307
155.396904	5646.187860	25.165325
155.675983	5653.205018	25.170343
155.478706	5659.535489	25.175360
156.073440	5665.182733	25.180378
156.079002	5666.527956	25.185395
155.609131	5677.273195	25.190413
156.073385	5680.381540	25.195431
155.881432	5688.058734	25.200448
156.021424	5717.706406	25.205466
156.292866	5725.607769	25.210483
156.266555	5739.506448	25.215501
156.520292	5747.269771	25.220519
156.610642	5759.913396	25.225536
156.662353	5782.598373	25.230554
156.733117	5791.891620	25.235571
156.850760	5807.218094	25.240589
157.322427	5811.705923	25.245607
157.621425	5838.010075	25.250624
157.839596	5841.907425	25.255642
158.199288	5857.463240	25.260659
158.150123	5873.599495	25.265677
158.516737	5871.968424	25.270695
158.611400	5880.950597	25.275712
159.085614	5895.149331	25.280730
159.329675	5895.242161	25.285747
159.402423	5895.946974	25.290765
159.400898	5890.638032	25.295783
159.524399	5903.793748	25.300800
159.780469	5920.315858	25.305818
159.800764	5923.590690	25.310835
160.013955	5929.293318	25.315853
160.344724	5941.611382	25.320871
160.762016	5943.457127	25.325888
160.495892	5953.414282	25.330906
160.740724	5947.237537	25.335923
160.591385	5950.809822	25.340941
161.126454	5969.662043	25.345959
161.313298	5977.153798	25.350976
161.233644	5975.980955	25.355994
161.495024	5981.908761	25.361011
161.468937	6005.837201	25.366029
161.723637	6014.068343	25.371047
161.754001	6022.031031	25.376064
161.742349	6035.896826	25.381082
162.230598	6044.639082	25.386099
161.875477	6052.697107	25.391117
162.257612	6059.791114	25.396135
162.975362	6067.363572	25.401152
162.633674	6073.894543	25.406170
163.167732	6078.652515	25.411187
162.979532	6104.722716	25.416205
163.361830	6102.000525	25.421223
163.546422	6105.888536	25.426240
163.642475	6110.535512	25.431258
164.361143	6112.418811	25.436275
164.110715	6136.878431	25.441293
164.192167	6136.045939	25.446311
164.411682	6136.005787	25.451328
164.220693	6131.994636	25.456346
164.608407	6146.600944	25.461363
164.888312	6152.869942	25.466381
164.920762	6155.598557	25.471399
165.284509	6164.875026	25.476416
165.491940	6178.997675	25.481434
165.847399	6181.526322	25.486451
165.843253	6187.528881	25.491469
165.596814	6185.677916	25.496487
166.020730	6189.794909	25.501504
165.806208	6206.279443	25.506522
166.073627	6212.801786	25.511539
166.131696	6225.859121	25.516557
166.650363	6246.613372	25.521575
166.702067	6247.135804	25.526592
166.910369	6251.483841	25.531610
167.289360	6263.200298	25.536627
166.966189	6278.678968	25.541645
167.162375	6280.961477	25.546663
167.326223	6292.671039	25.551680
167.563994	6306.461123	25.556698
168.085604	6319.092874	25.561715
168.311981	6333.874141	25.566733
168.045353	6333.247339	25.571751
168.339285	6345.397749	25.576768
168.363432	6367.409970	25.581786
168.618762	6369.916630	25.586803
168.796523	6378.896356	25.591821
168.962079	6395.519013	25.596839
169.294736	6394.154221	25.601856
169.222840	6410.580699	25.606874
169.690456	6418.227819	25.611891
169.579827	6424.728557	25.616909
169.921251	6450.292622	25.621927
170.471096	6449.833893	25.626944
170.621797	6460.564352	25.631962
170.560695	6450.584115	25.636979
170.749035	6475.452081	25.641997
170.774451	6494.743743	25.647015
171.245181	6497.519583	25.652032
171.334551	6496.663708	25.657050
171.297097	6513.559541	25.662067
171.301970	6523.448560	25.667085
171.406365	6532.219190	25.672103
171.746167	6546.841678	25.677120
171.672015	6556.951739	25.682138
172.043075	6557.724558	25.687156
172.389968	6584.742722	25.692173
172.288278	6592.377054	25.697191
173.038982	6597.954709	25.702208
172.509854	6604.267240	25.707226
172.875175	6615.174940	25.712244
173.128974	6626.234223	25.717261
173.183603	6633.975809	25.722279
173.411011	6643.056163	25.727296
173.567577	6669.957902	25.732314
174.032885	6674.577784	25.737332
173.973788	6669.056781	25.742349
174.365248	6698.127479	25.747367
174.567513	6696.957533	25.752384
174.576100	6713.346582	25.757402
174.675786	6711.381543	25.762420
174.994929	6720.616101	25.767437
174.864896	6728.747475	25.772455
175.624549	6738.656606	25.777472
175.263456	6731.305436	25.782490
175.764045	6735.294883	25.787508
175.841354	6754.790938	25.792525
175.773600	6760.789277	25.797543
176.330401	6750.618342	25.802560
176.364514	6781.308702	25.807578
176.408386	6785.246169	25.812596
177.012297	6775.985043	25.817613
177.150552	6786.275906	25.822631
177.109969	6799.932914	25.827648
177.211530	6812.363643	25.832666
177.408759	6813.882025	25.837684
177.803911	6829.074543	25.842701
177.609810	6845.872998	25.847719
178.034804	6852.710579	25.852736
178.040886	6854.385847	25.857754
178.142874	6857.394508	25.862772
178.419501	6875.686458	25.867789
178.725872	6887.687145	25.872807
178.814384	6890.370373	25.877824
179.000223	6913.139523	25.882842
179.155808	6907.226872	25.887860
179.333117	6925.846450	25.892877
179.575225	6933.730433	25.897895
180.075857	6941.663780	25.902912
179.852463	6959.596721	25.907930
180.305026	6953.555335	25.912948
180.626734	6971.366544	25.917965
180.348209	6974.055411	25.922983
180.892554	6976.558433	25.928000
181.160889	6995.771893	25.933018
180.972324	6996.516866	25.938036
181.582650	7001.178215	25.943053
181.497134	7005.202533	25.948071
181.552839	7020.893312	25.953088
181.827245	7030.271724	25.958106
181.947956	7026.618334	25.963124
182.051113	7041.104016	25.968141
181.948266	7054.791242	25.973159
182.272138	7069.967434	25.978176
182.368642	7086.714885	25.983194
182.728472	7089.537548	25.988212
183.017524	7108.963539	25.993229
182.980725	7126.301013	25.998247
183.018560	7132.206396	26.003264
183.479154	7147.360817	26.008282
183.688664	7148.953604	26.013300
183.965092	7158.465663	26.018317
183.864211	7180.342960	26.023335
184.472390	7171.996185	26.028352
184.658735	7196.720679	26.033370
184.789580	7213.620902	26.038388
184.918452	7211.647031	26.043405
184.994654	7219.104130	26.048423
185.391113	7217.503433	26.053440
185.415756	7233.023910	26.058458
185.855101	7236.659716	26.063476
186.002703	7241.417431	26.068493
185.962696	7256.751713	26.073511
186.417417	7255.284726	26.078528
186.512220	7267.272676	26.083546
186.571920	7271.966971	26.088564
186.662995	7283.539653	26.093581
186.922763	7306.811487	26.098599
187.457865	7295.744263	26.103616
187.330700	7291.377243	26.108634
187.542141	7298.507944	26.113652
187.631417	7312.807127	26.118669
187.875576	7322.390792	26.123687
188.253972	7313.698380	26.128704
188.273751	7332.281498	26.133722
188.231116	7344.258388	26.138740
188.655561	7347.182253	26.143757
188.574567	7357.115937	26.148775
189.043118	7368.536396	26.153792
188.666718	7381.939934	26.158810
189.113898	7386.643373	26.163828
189.519725	7405.013795	26.168845
189.444372	7421.081913	26.173863
189.491631	7427.552197	26.178880
189.622867	7452.960476	26.183898
189.963265	7458.600853	26.188916
189.736001	7465.781410	26.193933
189.949337	7486.325532	26.198951
190.546331	7499.108803	26.203968
190.913726	7513.796146	26.208986
190.822504	7538.586025	26.214004
191.618136	7540.691502	26.219021
191.451334	7555.361764	26.224039
191.842675	7567.922346	26.229056
192.163762	7579.847865	26.234074
192.283859	7586.869361	26.239092
192.606897	7591.531185	26.244109
192.473277	7606.193637	26.249127
192.498038	7609.729594	26.254144
192.965103	7631.078679	26.259162
193.193772	7629.672712	26.264180
193.524898	7635.329653	26.269197
193.756588	7663.020155	26.274215
193.940536	7663.465603	26.279232
194.330899	7659.642973	26.284250
194.182192	7668.756245	26.289268
194.552847	7695.592772	26.294285
194.300924	7700.070172	26.299303
194.476069	7705.875842	26.304320
194.657325	7720.775363	26.309338
194.916510	7720.374177	26.314356
195.288947	7732.225143	26.319373
195.198747	7749.878554	26.324391
195.509848	7755.560122	26.329408
195.880262	7770.478001	26.334426
195.746908	7782.181148	26.339444
195.907064	7798.888878	26.344461
196.089084	7818.219236	26.349479
196.291906	7837.310648	26.354496
196.776922	7848.074927	26.359514
197.027619	7867.082829	26.364532
197.407161	7874.879938	26.369549
197.530037	7887.111837	26.374567
197.380532	7894.558565	26.379584
197.925607	7905.135704	26.384602
197.570818	7915.449051	26.389620
198.244529	7935.240893	26.394637
198.418198	7945.683400	26.399655
198.658897	7946.488903	26.404672
198.612491	7961.622478	26.409690
198.954836	7972.159964	26.414708
199.140485	7982.006572	26.419725
198.957201	8002.169591	26.424743
199.485059	8009.955605	26.429760
199.874649	8028.229395	26.434778
199.835149	8033.057707	26.439796
200.528277	8029.828440	26.444813
200.623738	8059.184582	26.449831
200.822155	8050.647602	26.454848
200.871827	8056.657710	26.459866
200.789833	8061.714416	26.464884
201.644045	8072.008114	26.469901
201.585713	8089.889003	26.474919
201.516644	8090.043929	26.479936
201.970474	8085.522222	26.484954
201.953916	8111.447557	26.489972
202.219381	8118.625613	26.494989
202.331868	8116.283325	26.500007
202.606959	8136.487218	26.505024
202.799824	8137.800856	26.510042
203.047535	8155.761132	26.515060
203.347612	8168.272703	26.520077
203.371570	8179.891019	26.525095
203.475147	8183.388061	26.530112
203.662352	8194.875383	26.535130
203.718220	8203.470640	26.540148
204.099838	8219.315033	26.545165
204.451050	8236.863614	26.550183
204.374521	8235.074865	26.555200
204.556540	8249.153937	26.560218
204.868355	8266.069432	26.565236
205.201462	8279.451583	26.570253
205.157004	8300.568000	26.575271
205.526785	8303.072567	26.580288
205.511024	8312.309141	26.585306
205.543472	8334.364456	26.590324
206.469800	8354.330056	26.595341
206.513675	8361.307006	26.600359
206.548316	8377.966011	26.605376
206.961161	8382.576179	26.610394
207.051072	8393.536211	26.615412
207.567319	8410.655128	26.620429
207.583706	8420.019571	26.625447
207.891907	8432.525278	26.630464
208.284704	8434.638488	26.635482
208.350971	8453.973811	26.640500
208.509304	8448.406745	26.645517
208.671554	8462.761837	26.650535
208.789370	8478.364994	26.655552
209.118783	8482.354869	26.660570
209.390002	8505.250804	26.665588
209.473400	8511.717908	26.670605
209.522898	8514.964807	26.675623
209.659148	8537.432540	26.680640
209.691517	8546.363513	26.685658
209.858297	8565.824915	26.690676
210.200077	8579.649385	26.695693
210.606312	8587.266758	26.700711
210.982063	8605.322932	26.705728
211.324210	8603.431750	26.710746
211.262559	8622.028273	26.715764
211.551443	8627.900529	26.720781
211.703376	8636.982702	26.725799
211.894404	8663.600088	26.730816
212.100368	8660.565568	26.735834
212.381873	8676.343487	26.740852
212.675833	8695.118341	26.745869
212.588973	8697.004552	26.750887
212.778846	8710.850343	26.755904
213.147125	8722.997358	26.760922
213.056920	8739.847562	26.765940
213.270478	8754.036871	26.770957
213.672821	8769.638114	26.775975
213.666374	8782.797243	26.780992
214.030950	8788.907536	26.786010
214.414432	8803.561898	26.791028
214.552880	8824.621944	26.796045
214.536555	8830.721257	26.801063
214.632030	8849.058855	26.806080
215.245304	8851.358562	26.811098
215.437055	8866.672567	26.816116
215.333961	8879.267191	26.821133
215.653401	8893.599012	26.826151
215.702175	8915.343622	26.831168
216.115742	8926.875140	26.836186
216.516588	8944.435977	26.841204
216.533329	8948.956691	26.846221
217.149793	8957.925913	26.851239
216.986006	8973.576169	26.856256
217.445831	8994.192505	26.861274
217.823384	9008.105957	26.866292
217.696247	9012.597725	26.871309
218.147753	9025.550475	26.876327
218.249193	9043.313023	26.881344
218.690690	9049.406746	26.886362
218.812139	9075.957558	26.891380
218.925209	9069.555640	26.896397
219.018253	9093.017597	26.901415
219.395112	9109.585265	26.906432
219.845905	9116.123355	26.911450
219.809135	9138.196749	26.916468
220.227363	9136.936526	26.921485
220.714699	9153.071580	26.926503
220.712237	9173.121846	26.931520
221.271564	9166.691709	26.936538
221.104687	9188.776469	26.941556
221.434974	9185.254118	26.946573
221.799242	9187.387122	26.951591
221.270908	9197.370789	26.956608
221.765916	9212.900407	26.961626
222.100161	9230.995670	26.966644
222.093045	9250.596192	26.971661
222.371505	9258.884172	26.976679
222.675851	9275.675929	26.981696
223.005874	9299.692161	26.986714
222.870481	9304.716344	26.991732
223.252655	9325.853296	26.996749
223.364717	9329.283798	27.001767
223.564069	9360.388981	27.006784
224.073457	9375.370440	27.011802
224.190179	9387.542272	27.016820
224.233992	9396.855477	27.021837
225.038165	9408.768575	27.026855
224.853869	9427.231925	27.031872
225.247825	9443.133788	27.036890
225.567972	9458.019816	27.041908
225.744427	9462.689915	27.046925
225.893044	9473.466078	27.051943
226.257088	9488.563875	27.056960
226.520316	9499.988345	27.061978
226.691805	9519.526543	27.066996
227.005924	9516.416451	27.072013
227.027419	9537.518063	27.077031
227.278990	9546.177757	27.082048
227.423528	9564.092095	27.087066
227.957146	9578.932657	27.092084
228.264479	9580.839588	27.097101
228.558354	9599.308277	27.102119
228.439735	9608.598862	27.107136
228.991463	9613.722893	27.112154
228.737262	9619.498706	27.117172
228.926873	9624.510943	27.122189
229.309304	9633.149810	27.127207
229.359063	9651.811801	27.132224
229.607569	9673.101325	27.137242
229.902132	9684.305670	27.142260
230.250731	9698.876031	27.147277
230.362954	9689.138445	27.152295
230.088499	9700.857680	27.157312
230.455042	9723.837267	27.162330
230.464602	9738.761576	27.167348
230.928998	9760.809588	27.172365
231.264661	9777.105095	27.177383
231.324228	9793.996999	27.182400
231.712653	9818.143783	27.187418
232.002505	9834.097143	27.192436
231.925168	9847.559580	27.197453
232.345235	9863.033696	27.202471
232.919865	9895.729049	27.207488
233.172437	9893.466520	27.212506
233.583806	9909.993853	27.217524
233.618805	9914.787551	27.222541
234.091607	9931.775062	27.227559
234.356942	9951.042210	27.232576
234.452386	9947.098486	27.237594
234.986590	9967.788849	27.242612
234.543906	9986.491778	27.247629
235.047412	9989.206100	27.252647
234.977147	10011.585608	27.257664
235.552959	10020.317149	27.262682
235.579839	10044.596600	27.267700
235.807855	10059.433837	27.272717
236.435076	10061.310722	27.277735
236.402346	10085.399995	27.282752
236.705114	10100.154779	27.287770
236.624393	10111.078841	27.292788
237.273899	10125.966118	27.297805
237.662543	10147.727828	27.302823
237.746114	10165.129811	27.307840
237.818756	10173.389309	27.312858
238.025836	10195.210287	27.317876
237.929750	10218.877729	27.322893
238.064899	10224.055947	27.327911
238.518172	10246.868299	27.332928
239.248852	10262.490706	27.337946
239.489351	10273.267954	27.342964
239.173811	10301.081963	27.347981
239.966153	10308.044587	27.352999
239.798093	10331.416065	27.358016
239.984402	10339.854579	27.363034
240.467657	10361.784483	27.368052
240.721725	10377.866422	27.373069
241.063367	10392.795454	27.378087
241.199426	10408.572369	27.383104
241.204181	10425.032818	27.388122
241.920370	10427.989331	27.393140
241.909349	10455.262375	27.398157
242.043718	10469.768841	27.403175
242.464882	10484.579225	27.408192
242.331395	10505.846420	27.413210
242.816939	10526.874090	27.418228
242.900043	10537.803624	27.423245
243.368187	10563.008224	27.428263
243.633232	10575.393545	27.433280
243.511354	10598.387476	27.438298
243.993695	10606.712525	27.443316
244.082064	10625.948322	27.448333
244.595056	10630.778138	27.453351
244.609881	10664.067215	27.458368
245.137286	10671.006098	27.463386
245.632066	10685.713879	27.468404
245.453544	10707.368538	27.473421
246.176710	10706.166449	27.478439
245.899318	10714.634645	27.483456
246.314385	10731.673529	27.488474
246.658012	10738.984791	27.493492
246.782160	10760.683964	27.498509
247.321379	10759.471351	27.503527
247.104029	10770.031637	27.508544
246.975457	10787.199960	27.513562
247.786593	10802.142262	27.518580
247.748183	10825.735653	27.523597
248.192816	10838.373503	27.528615
248.788446	10851.630838	27.533632
248.496078	10866.339871	27.538650
249.041137	10876.881175	27.543668
249.314833	10905.388124	27.548685
249.892017	10918.662749	27.553703
249.529995	10926.358776	27.558720
249.651905	10944.268941	27.563738
250.187310	10966.409276	27.568756
250.272249	10982.387452	27.573773
250.690511	11002.104840	27.578791
251.145097	11024.578507	27.583808
251.294465	11034.411726	27.588826
251.562416	11044.809921	27.593844
251.892391	11069.469343	27.598861
252.039047	11083.412575	27.603879
251.763554	11093.459549	27.608896
252.132870	11113.747716	27.613914
252.986691	11135.575579	27.618932
252.726158	11152.165771	27.623949
253.564171	11173.364427	27.628967
253.629241	11194.065479	27.633984
253.547383	11220.110631	27.639002
254.047995	11231.448980	27.644020
254.066545	11236.587733	27.649037
254.673260	11254.794600	27.654055
254.907585	11281.506061	27.659072
255.149046	11291.499101	27.664090
255.325942	11315.824965	27.669108
255.359892	11330.357493	27.674125
255.464298	11353.403283	27.679143
255.914417	11366.540158	27.684160
256.104524	11381.067369	27.689178
256.285888	11403.095148	27.694196
256.531906	11433.485933	27.699213
257.291390	11445.660867	27.704231
257.190967	11463.113613	27.709248
257.646747	11483.805515	27.714266
258.262304	11489.113411	27.719284
258.129866	11517.874609	27.724301
258.323506	11526.414958	27.729319
258.709272	11543.673857	27.734336
258.550148	11562.579849	27.739354
258.988946	11572.608159	27.744372
259.351328	11606.462505	27.749389
259.908883	11619.358041	27.754407
260.272231	11635.147381	27.759424
260.484864	11640.777301	27.764442
260.921183	11660.796635	27.769460
261.040083	11685.674728	27.774477
261.059649	11690.233563	27.779495
262.001778	11705.892501	27.784512
261.905584	11715.177430	27.789530
262.355362	11722.154834	27.794548
262.175020	11746.860365	27.799565
262.457720	11750.584605	27.804583
262.982355	11751.270037	27.809600
262.675571	11763.676860	27.814618
262.963844	11772.529443	27.819636
263.020334	11787.399026	27.824653
262.947507	11800.392748	27.829671
263.542062	11827.015541	27.834688
263.796342	11854.006714	27.839706
263.950768	11872.638976	27.844724
264.111028	11897.439637	27.849741
264.771879	11916.219768	27.854759
265.041826	11931.290523	27.859776
265.201521	11956.149673	27.864794
265.470873	11963.023101	27.869812
266.000207	11995.560023	27.874829
265.972503	12006.600288	27.879847
266.422945	12027.117277	27.884864
266.738827	12038.530895	27.889882
266.713579	12061.019244	27.894900
266.934576	12078.255561	27.899917
267.635837	12085.320715	27.904935
267.930435	12107.592299	27.909952
268.228056	12130.394472	27.914970
268.755534	12139.573259	27.919988
269.015859	12150.873237	27.925005
269.065807	12158.574140	27.930023
269.598124	12183.416084	27.935040
269.627088	12190.181269	27.940058
270.076968	12209.170006	27.945076
270.279719	12221.010626	27.950093
270.220977	12239.801510	27.955111
270.628565	12253.099007	27.960128
270.773022	12272.316444	27.965146
271.323660	12282.340867	27.970164
271.565188	12304.244875	27.975181
271.312828	12323.417745	27.980199
271.611009	12333.885832	27.985216
271.914628	12372.997561	27.990234
272.406305	12372.572764	27.995252
272.572760	12403.807444	28.000269
273.142947	12423.017627	28.005287
273.273275	12435.546440	28.010304
273.711623	12463.240941	28.015322
274.480253	12469.820776	28.020340
274.350492	12484.929841	28.025357
274.348924	12513.529308	28.030375
274.846803	12523.676077	28.035392
274.882032	12544.582353	28.040410
275.296816	12560.086726	28.045428
275.713967	12582.384377	28.050445
275.839982	12590.912843	28.055463
276.164087	12618.158479	28.060480
275.892506	12636.427184	28.065498
276.732824	12656.068851	28.070516
276.988802	12676.369858	28.075533
277.137220	12696.939263	28.080551
277.071757	12706.591582	28.085568
277.269427	12731.732446	28.090586
278.261223	12748.600777	28.095604
278.091694	12776.699003	28.100621
278.464095	12795.119742	28.105639
278.908687	12802.040165	28.110656
279.141324	12821.944937	28.115674
279.457305	12834.843610	28.120692
279.756597	12860.576155	28.125709
279.951796	12876.531642	28.130727
280.047578	12888.560653	28.135744
280.363059	12910.363409	28.140762
281.022782	12925.684181	28.145780
280.919383	12947.466493	28.150797
281.236710	12958.330523	28.155815
281.606769	12964.185421	28.160832
281.501079	12991.354684	28.165850
281.775374	13015.528291	28.170868
282.098763	13029.984488	28.175885
281.826194	13060.115874	28.180903
282.516871	13067.983790	28.185920
282.800565	13095.323590	28.190938
283.158656	13120.753689	28.195956
283.513818	13144.395618	28.200973
283.835884	13166.769695	28.205991
284.450671	13180.898852	28.211008
284.733351	13202.274043	28.216026
284.891458	13215.520643	28.221044
285.353768	13234.103504	28.226061
285.748780	13258.049464	28.231079
286.407094	13273.782122	28.236096
286.434463	13286.960591	28.241114
286.358136	13296.143845	28.246132
286.977763	13311.096541	28.251149
287.014441	13329.811424	28.256167
287.609601	13342.238781	28.261184
287.390840	13364.918555	28.266202
287.699478	13381.144162	28.271220
288.551084	13401.820276	28.276237
288.428461	13427.814244	28.281255
288.656818	13429.155547	28.286272
289.010640	13456.602543	28.291290
289.347931	13475.885618	28.296308
289.889864	13489.771796	28.301325
290.121762	13520.561239	28.306343
290.213097	13527.841457	28.311360
290.647018	13543.791181	28.316378
290.988140	13560.786973	28.321396
291.235338	13581.172513	28.326413
291.383794	13607.774356	28.331431
291.991268	13617.216542	28.336448
292.000153	13636.209023	28.341466
292.025278	13650.075287	28.346484
292.391496	13670.888821	28.351501
292.350059	13699.219589	28.356519
293.086771	13712.613526	28.361536
293.303061	13734.165884	28.366554
293.635792	13759.572809	28.371572
294.204608	13774.266422	28.376589
294.442178	13790.244159	28.381607
294.793587	13807.315730	28.386624
294.923258	13827.254532	28.391642
295.344373	13848.095453	28.396660
295.891012	13862.067851	28.401677
295.916933	13885.588837	28.406695
296.249389	13891.459751	28.411712
296.405121	13920.458017	28.416730
296.965026	13929.506375	28.421748
297.279062	13943.808906	28.426765
297.423965	13963.346620	28.431783
297.739193	13976.641905	28.436800
298.064488	13993.208938	28.441818
298.120584	14008.537659	28.446836
298.234275	14025.385608	28.451853
298.780073	14048.313298	28.456871
299.176273	14064.441563	28.461888
299.218125	14090.333709	28.466906
299.687586	14113.792641	28.471924
299.905418	14115.934795	28.476941
300.163635	14142.320759	28.481959
300.582160	14152.733852	28.486976
300.901568	14176.313848	28.491994
300.976641	14184.129753	28.497012
301.553139	14206.704278	28.502029
301.541145	14224.436908	28.507047
301.881181	14239.121527	28.512064
302.074957	14257.275612	28.517082
302.294638	14281.532632	28.522100
302.860865	14304.028613	28.527117
302.840119	14325.758100	28.532135
303.244298	14347.220276	28.537152
303.600884	14363.662725	28.542170
303.812783	14389.653283	28.547188
304.109136	14395.795134	28.552205
304.021054	14435.231960	28.557223
304.325037	14460.315335	28.562240
305.108684	14488.435251	28.567258
305.204365	14511.819502	28.572276
305.783402	14536.638393	28.577293
306.303082	14564.363981	28.582311
306.623227	14583.011313	28.587328
306.834465	14608.412873	28.592346
306.783561	14621.220806	28.597364
307.383234	14639.695850	28.602381
307.162429	14669.588361	28.607399
307.719604	14695.924159	28.612416
308.105791	14722.947108	28.617434
308.408803	14757.178754	28.622452
308.430235	14780.797907	28.627469
308.925528	14803.645178	28.632487
309.451446	14823.850590	28.637504
310.036892	14848.725634	28.642522
310.050787	14876.897970	28.647540
310.817355	14894.204575	28.652557
310.949584	14930.729721	28.657575
311.376598	14942.377588	28.662592
311.886582	14954.319072	28.667610
311.944387	14963.232031	28.672628
312.098399	14981.767040	28.677645
312.483765	15008.292541	28.682663
312.970782	15024.214435	28.687680
313.243089	15050.525451	28.692698
313.411716	15072.949600	28.697716
313.952281	15083.120853	28.702733
314.096128	15111.629864	28.707751
314.378669	15136.651624	28.712768
314.863341	15154.058751	28.717786
314.679523	15176.765186	28.722804
315.159532	15194.371721	28.727821
315.508265	15224.829801	28.732839
315.628882	15243.980599	28.737856
316.218684	15269.315795	28.742874
316.031017	15292.582559	28.747892
316.334070	15312.721435	28.752909
317.250813	15350.558269	28.757927
317.098824	15377.259993	28.762944
317.741790	15395.835905	28.767962
317.668841	15422.877680	28.772980
318.564146	15452.801240	28.777997
318.964653	15471.742057	28.783015
319.164998	15497.383218	28.788032
319.480612	15519.581898	28.793050
319.881787	15529.529042	28.798068
320.195653	15548.627720	28.803085
320.345294	15570.283363	28.808103
320.358963	15597.843837	28.813120
321.058322	15626.022214	28.818138
321.144711	15638.108389	28.823156
321.659568	15661.877261	28.828173
321.839806	15680.296807	28.833191
322.042504	15691.678129	28.838208
322.687139	15714.623319	28.843226
322.671379	15747.005748	28.848244
323.310820	15764.088430	28.853261
323.304575	15783.490977	28.858279
323.377546	15807.604302	28.863296
324.090154	15817.645087	28.868314
324.459055	15853.190539	28.873332
324.412660	15871.778634	28.878349
324.724683	15897.516997	28.883367
325.070460	15927.374754	28.888384
325.725819	15945.908256	28.893402
325.812995	15979.643833	28.898420
326.179347	16002.447913	28.903437
326.686903	16022.131383	28.908455
326.666871	16040.701118	28.913472
327.147788	16070.722762	28.918490
327.204215	16104.731641	28.923508
327.860616	16126.811686	28.928525
328.229676	16159.574152	28.933543
328.493979	16183.199251	28.938560
329.180932	16211.861437	28.943578
329.153350	16238.039565	28.948596
329.500046	16249.589742	28.953613
329.716164	16280.101669	28.958631
330.341138	16307.808044	28.963648
330.767119	16327.166488	28.968666
330.602337	16359.499121	28.973684
331.212708	16382.980534	28.978701
331.845789	16413.266071	28.983719
332.120259	16432.835714	28.988736
332.413705	16458.634772	28.993754
332.335142	16492.895348	28.998772
333.008266	16510.592704	29.003789
333.350361	16542.223904	29.008807
333.460418	16566.533960	29.013824
334.365071	16590.573828	29.018842
334.274738	16607.049932	29.023860
334.543151	16636.124180	29.028877
335.279285	16663.781230	29.033895
335.501942	16683.920901	29.038912
335.809545	16706.965815	29.043930
336.024466	16729.721878	29.048948
336.222256	16751.123623	29.053965
336.857991	16784.125346	29.058983
337.082935	16803.996815	29.064000
337.766556	16830.256782	29.069018
337.793001	16851.560912	29.074036
338.124264	16876.779014	29.079053
338.543126	16898.171158	29.084071
338.817905	16922.243248	29.089088
339.333319	16948.608481	29.094106
339.511994	16975.018455	29.099124
339.637528	16997.609981	29.104141
340.172648	17021.115791	29.109159
340.169656	17051.723729	29.114176
340.607927	17080.133812	29.119194
340.684675	17103.969391	29.124212
341.321409	17134.685982	29.129229
341.836411	17154.180413	29.134247
342.018414	17189.769130	29.139264
342.520574	17199.174078	29.144282
342.785227	17232.529734	29.149300
342.993755	17256.042642	29.154317
343.474128	17276.900174	29.159335
343.355014	17311.739786	29.164352
343.808345	17331.881475	29.169370
344.317048	17357.896946	29.174388
344.797656	17380.321458	29.179405
345.185728	17414.208774	29.184423
345.149902	17438.339326	29.189440
345.558956	17454.973226	29.194458
345.700868	17491.891787	29.199476
346.202305	17523.016122	29.204493
346.508357	17548.603559	29.209511
346.900510	17577.751984	29.214528
347.428154	17603.835643	29.219546
347.596797	17631.244586	29.224564
348.221728	17657.364248	29.229581
348.191026	17684.591884	29.234599
348.563306	17714.306605	29.239616
349.150588	17734.858542	29.244634
349.190939	17778.386977	29.249652
349.627888	17804.686163	29.254669
350.333550	17830.537362	29.259687
350.384599	17866.961043	29.264704
351.296717	17887.341179	29.269722
351.483782	17920.069462	29.274740
351.601212	17944.093409	29.279757
351.973057	17966.651792	29.284775
352.246849	17995.609301	29.289792
352.659772	18025.417165	29.294810
352.655339	18064.758935	29.299828
353.585771	18096.546377	29.304845
353.695608	18119.777321	29.309863
354.165051	18159.321489	29.314880
354.769602	18183.451179	29.319898
355.026962	18212.233648	29.324916
355.368527	18231.482177	29.329933
355.954106	18255.771178	29.334951
356.178988	18294.468612	29.339968
356.643248	18310.406907	29.344986
356.624829	18335.636229	29.350004
356.929350	18366.129477	29.355021
357.474264	18388.621954	29.360039
357.813261	18425.987629	29.365056
358.359554	18453.743723	29.370074
358.590709	18483.580914	29.375092
359.155841	18500.847411	29.380109
359.506894	18529.056857	29.385127
359.643996	18560.025881	29.390144
360.168159	18587.295581	29.395162
360.411448	18606.259704	29.400180
360.398868	18639.895803	29.405197
361.270730	18667.041877	29.410215
361.233108	18699.960218	29.415232
361.757985	18733.504402	29.420250
362.086842	18765.001719	29.425268
362.038761	18797.152660	29.430285
362.932755	18812.984057	29.435303
362.919907	18852.456769	29.440320
363.697110	18875.915684	29.445338
363.888560	18907.615731	29.450356
363.892353	18946.318159	29.455373
364.414818	18970.429469	29.460391
364.822830	19009.484493	29.465408
365.171562	19035.319390	29.470426
365.487615	19070.412255	29.475444
365.859260	19104.825977	29.480461
366.494528	19133.282636	29.485479
366.543654	19178.862734	29.490496
367.060154	19195.572032	29.495514
367.312935	19228.766536	29.500532
367.859510	19253.429202	29.505549
368.642999	19277.464650	29.510567
368.806266	19300.753030	29.515584
369.045527	19324.084044	29.520602
369.721372	19351.309395	29.525620
369.578514	19370.499099	29.530637
370.369309	19396.578277	29.535655
370.447796	19427.708379	29.540672
370.949739	19445.722559	29.545690
371.242054	19474.145119	29.550708
371.554314	19512.766273	29.555725
371.923273	19536.093459	29.560743
371.841911	19560.677621	29.565760
372.386545	19601.084593	29.570778
373.091537	19621.072316	29.575796
373.131916	19654.348537	29.580813
373.733785	19676.261033	29.585831
374.043074	19721.307660	29.590848
374.309991	19750.037592	29.595866
374.883455	19787.195658	29.600884
375.228673	19826.056448	29.605901
375.739946	19838.745403	29.610919
375.969246	19882.457725	29.615936
376.329033	19905.479511	29.620954
376.983575	19938.187981	29.625972
377.135244	19973.311519	29.630989
378.022907	19990.873034	29.636007
378.278298	20024.773420	29.641024
378.553595	20051.681512	29.646042
378.717865	20080.816841	29.651060
378.879167	20119.880598	29.656077
379.325590	20145.210715	29.661095
379.594497	20185.477111	29.666112
380.029232	20221.328437	29.671130
380.522617	20259.546099	29.676148
380.882999	20282.320773	29.681165
381.544884	20318.311296	29.686183
381.829701	20354.288621	29.691200
382.218001	20382.219115	29.696218
382.689955	20412.816088	29.701236
383.155587	20440.852129	29.706253
383.635443	20473.699341	29.711271
383.921589	20499.042328	29.716288
384.371305	20520.041432	29.721306
384.910646	20551.439477	29.726324
384.853679	20577.876800	29.731341
385.359251	20601.964878	29.736359
385.524274	20643.551876	29.741376
385.937651	20675.201189	29.746394
386.688747	20707.548316	29.751412
386.755721	20743.674468	29.756429
387.124193	20763.320354	29.761447
387.284576	20813.058327	29.766464
387.824082	20838.150197	29.771482
388.222909	20867.728956	29.776500
388.515006	20906.914792	29.781517
389.219069	20944.714434	29.786535
389.523598	20982.643350	29.791552
389.722003	21017.915847	29.796570
390.245911	21042.367313	29.801588
390.635059	21086.300693	29.806605
391.313503	21114.039328	29.811623
391.602390	21147.873364	29.816640
391.684725	21175.428523	29.821658
391.963145	21201.795550	29.826676
392.381256	21240.518252	29.831693
393.161455	21267.801975	29.836711
393.185929	21312.884228	29.841728
393.665266	21337.936346	29.846746
394.278940	21358.535681	29.851764
394.210923	21404.109653	29.856781
394.651626	21431.779363	29.861799
394.815074	21461.229406	29.866816
395.081759	21509.058181	29.871834
395.630454	21531.451769	29.876852
396.070784	21583.819828	29.881869
396.305343	21625.684703	29.886887
396.449103	21663.875112	29.891904
397.087468	21703.484823	29.896922
397.860644	21742.561447	29.901940
397.858361	21784.886905	29.906957
398.416881	21813.658819	29.911975
398.875585	21855.457209	29.916992
399.023074	21900.145395	29.922010
399.458941	21930.689601	29.927028
399.769546	21975.421946	29.932045
400.421690	22012.070485	29.937063
400.846075	22057.780744	29.942080
400.983741	22095.465409	29.947098
401.655354	22141.611170	29.952116
402.004068	22196.039810	29.957133
402.706884	22226.871500	29.962151
403.187189	22269.517233	29.967168
403.470685	22300.527251	29.972186
403.764389	22325.499600	29.977204
404.280605	22377.974239	29.982221
404.997271	22403.816490	29.987239
405.353215	22436.755832	29.992256
405.467278	22484.801835	29.997274
405.970089	22519.405813	30.002292
406.267567	22552.889601	30.007309
406.623180	22602.633633	30.012327
406.966122	22646.331143	30.017344
407.260036	22689.850811	30.022362
407.830432	22719.216769	30.027380
408.352931	22771.300526	30.032397
409.009938	22803.031768	30.037415
409.773733	22840.910916	30.042432
409.789510	22869.936860	30.047450
410.521940	22905.328324	30.052468
410.859369	22949.562083	30.057485
410.893499	22986.095818	30.062503
411.548564	23012.155762	30.067520
411.886715	23058.974184	30.072538
412.450612	23085.747887	30.077556
412.565316	23132.193499	30.082573
413.146007	23158.292782	30.087591
413.750440	23188.533824	30.092608
413.942517	23238.716771	30.097626
414.435361	23267.369563	30.102644
414.487219	23303.730740	30.107661
414.958372	23346.874261	30.112679
415.563773	23380.772330	30.117696
415.804887	23428.252781	30.122714
416.581226	23465.552519	30.127732
416.842393	23499.750637	30.132749
417.065680	23537.011170	30.137767
417.715889	23578.457261	30.142784
417.911141	23621.281288	30.147802
418.558275	23651.732126	30.152820
419.121676	23691.597000	30.157837
419.540039	23724.776085	30.162855
419.814417	23763.416365	30.167872
419.905423	23801.191372	30.172890
420.552856	23835.515475	30.177908
420.538847	23881.549187	30.182925
420.937976	23912.555620	30.187943
421.497435	23959.365121	30.192960
421.834506	23992.353173	30.197978
422.378064	24027.303560	30.202996
422.773196	24080.833244	30.208013
423.038702	24119.819578	30.213031
423.669534	24143.199674	30.218048
424.096529	24188.088883	30.223066
424.593743	24220.237150	30.228084
424.783300	24261.636549	30.233101
425.389237	24299.094046	30.238119
425.905862	24340.032646	30.243136
426.166763	24382.808290	30.248154
426.598673	24416.585736	30.253172
427.232961	24463.996113	30.258189
427.431307	24499.755250	30.263207
427.985639	24540.625009	30.268224
428.322691	24585.170585	30.273242
428.875891	24626.321445	30.278260
429.529709	24664.771653	30.283277
429.485235	24711.418213	30.288295
430.354062	24741.973088	30.293312
430.098490	24791.711093	30.298330
431.001564	24825.998034	30.303348
431.543399	24873.516313	30.308365
431.812296	24915.698993	30.313383
432.542788	24955.780452	30.318400
432.621295	24996.045597	30.323418
432.940548	25038.488346	30.328436
433.226398	25089.348797	30.333453
433.962680	25133.293526	30.338471
434.626680	25177.124163	30.343488
434.623164	25233.152109	30.348506
435.269625	25265.523664	30.353524
436.216912	25321.886606	30.358541
436.535064	25350.984997	30.363559
436.801000	25383.763552	30.368576
437.415897	25423.218624	30.373594
438.346275	25455.515167	30.378612
438.494649	25492.533703	30.383629
438.756641	25527.937485	30.388647
439.479938	25563.624582	30.393664
439.738613	25601.019376	30.398682
440.370828	25631.034617	30.403700
440.857244	25671.309541	30.408717
441.066062	25710.728383	30.413735
441.413552	25747.175140	30.418752
441.983382	25786.534414	30.423770
442.385515	25828.094819	30.428788
442.567323	25865.767866	30.433805
442.931297	25911.766545	30.438823
443.641783	25944.677630	30.443840
443.940011	25990.081774	30.448858
444.392748	26022.105142	30.453876
444.444530	26072.827436	30.458893
444.981335	26113.173913	30.463911
445.661835	26154.452466	30.468928
446.351210	26210.577111	30.473946
447.001313	26245.176872	30.478964
447.230775	26291.530028	30.483981
447.365122	26324.723287	30.488999
448.208778	26361.915679	30.494016
448.414750	26410.777608	30.499034
448.831217	26456.699656	30.504052
449.248337	26493.802042	30.509069
449.716224	26534.542590	30.514087
450.164123	26575.201372	30.519104
450.505154	26616.190221	30.524122
451.211297	26638.469833	30.529140
451.750411	26686.861031	30.534157
451.718932	26726.123225	30.539175
452.643119	26755.618946	30.544192
452.842681	26790.546711	30.549210
453.149344	26830.390383	30.554228
453.715925	26861.790816	30.559245
454.034235	26900.295232	30.564263
454.594854	26942.011896	30.569280
454.879375	26989.676380	30.574298
455.403363	27025.680237	30.579316
456.008259	27064.415189	30.584333
455.969484	27111.054668	30.589351
457.078927	27147.450845	30.594368
457.560059	27191.496674	30.599386
457.827635	27225.202725	30.604404
458.684662	27264.757588	30.609421
458.802240	27298.599012	30.614439
459.453654	27335.604497	30.619456
459.723467	27380.152645	30.624474
460.247439	27415.725142	30.629492
460.660658	27460.543140	30.634509
460.328121	27509.184975	30.639527
461.543034	27553.343736	30.644544
461.783582	27596.521884	30.649562
462.116531	27646.918343	30.654580
462.762379	27690.619567	30.659597
463.274384	27749.295930	30.664615
463.235721	27776.583607	30.669632
464.033275	27830.045720	30.674650
464.414492	27880.687239	30.679668
465.603126	27926.983840	30.684685
465.621054	27972.430097	30.689703
466.237603	28016.427217	30.694720
466.776897	28061.427801	30.699738
467.129154	28117.273705	30.704756
467.472301	28153.196258	30.709773
467.760573	28198.251352	30.714791
468.434585	28246.791777	30.719808
469.119101	28302.599067	30.724826
469.260878	28347.745038	30.729844
469.710490	28396.764676	30.734861
470.320098	28440.751399	30.739879
470.908722	28482.167429	30.744896
471.222385	28524.250544	30.749914
471.874764	28576.016475	30.754932
472.232574	28619.471147	30.759949
472.592299	28674.093546	30.764967
473.374195	28718.102936	30.769984
473.731090	28763.908440	30.775002
474.105798	28815.497038	30.780020
474.636483	28852.642459	30.785037
474.743990	28900.805225	30.790055
475.514145	28949.350626	30.795072
475.668139	29000.935281	30.800090
475.906492	29053.869024	30.805108
477.286925	29097.761401	30.810125
477.170175	29148.242921	30.815143
478.027939	29197.711513	30.820160
478.656131	29248.760973	30.825178
478.894647	29303.212945	30.830196
479.484976	29338.737377	30.835213
479.675701	29393.184917	30.840231
480.553290	29429.422334	30.845248
481.061691	29483.738716	30.850266
481.249197	29538.430169	30.855284
481.725431	29566.351609	30.860301
482.615453	29619.258101	30.865319
483.211277	29656.069490	30.870336
483.316289	29698.590637	30.875354
483.658357	29736.523184	30.880372
484.641848	29768.686482	30.885389
484.708040	29807.999391	30.890407
484.706563	29860.312707	30.895424
485.588107	29899.872659	30.900442
485.936500	29951.090355	30.905460
486.348937	29992.081640	30.910477
486.487638	30049.748482	30.915495
487.238709	30088.289288	30.920512
487.606485	30143.558563	30.925530
488.149727	30205.711713	30.930548
488.861437	30248.266310	30.935565
489.156009	30295.190403	30.940583
489.573764	30340.289530	30.945600
490.087871	30394.478427	30.950618
490.635285	30455.600054	30.955636
491.030395	30502.880367	30.960653
491.128755	30566.360985	30.965671
492.064056	30608.459825	30.970688
492.667256	30675.078690	30.975706
492.782639	30729.236784	30.980724
493.283654	30780.097192	30.985741
493.868450	30833.840332	30.990759
494.678292	30896.421927	30.995776
495.119868	30939.344725	31.000794
495.656888	30997.857454	31.005812
496.366397	31050.353245	31.010829
496.881543	31105.721051	31.015847
497.483932	31151.375419	31.020864
498.144531	31201.406053	31.025882
498.377878	31257.505651	31.030900
498.952979	31297.027955	31.035917
499.564613	31349.951016	31.040935
499.876795	31396.606928	31.045952
500.775175	31453.313352	31.050970
501.038631	31502.811051	31.055988
501.722638	31538.504283	31.061005
502.048570	31590.714913	31.066023
502.694925	31631.339999	31.071040
503.255655	31680.028573	31.076058
503.858274	31724.892400	31.081076
504.391224	31770.430489	31.086093
504.872480	31824.903730	31.091111
504.925502	31874.115442	31.096128
505.612620	31920.149041	31.101146
505.728829	31974.992371	31.106164
506.632237	32020.135335	31.111181
507.397191	32073.921856	31.116199
507.958656	32123.602323	31.121216
508.194881	32168.010413	31.126234
508.569261	32211.272425	31.131252
509.249285	32271.595848	31.136269
509.423333	32315.399286	31.141287
509.843769	32374.106252	31.146304
510.447261	32429.517225	31.151322
510.908353	32483.872763	31.156340
511.170126	32534.509588	31.161357
511.912076	32601.598693	31.166375
512.318771	32653.635002	31.171392
512.694229	32704.553273	31.176410
513.228712	32765.883819	31.181428
513.755651	32811.785306	31.186445
514.481766	32885.937014	31.191463
514.937896	32936.795267	31.196480
515.406759	32997.944983	31.201498
515.766234	33055.503040	31.206516
516.215354	33089.805636	31.211533
516.992765	33147.335859	31.216551
517.106200	33208.156970	31.221568
517.958442	33249.853000	31.226586
518.427543	33316.093755	31.231604
518.943204	33362.320400	31.236621
519.431951	33413.988769	31.241639
519.477248	33466.920338	31.246656
520.498090	33513.344638	31.251674
520.885612	33582.313737	31.256692
521.434167	33627.484792	31.261709
521.729997	33696.106600	31.266727
522.468213	33764.614449	31.271744
522.985552	33810.397025	31.276762
523.224429	33878.167448	31.281780
523.548507	33928.782144	31.286797
524.357954	33997.954426	31.291815
525.126665	34064.889980	31.296832
525.837195	34111.086321	31.301850
525.990238	34171.553866	31.306868
526.783211	34228.286591	31.311885
527.002254	34292.218130	31.316903
527.627061	34357.332455	31.321920
528.114681	34414.270928	31.326938
528.743934	34474.894231	31.331956
529.275831	34543.107838	31.336973
530.066134	34597.835068	31.341991
530.468751	34666.679613	31.347008
531.287778	34725.868011	31.352026
531.426893	34784.421162	31.357044
532.152066	34842.536699	31.362061
532.601499	34896.267176	31.367079
533.208839	34957.337561	31.372096
533.769885	35017.712045	31.377114
534.422067	35077.052289	31.382132
535.066356	35137.482832	31.387149
535.600524	35208.526307	31.392167
536.192840	35270.149376	31.397184
536.722068	35320.058677	31.402202
537.343273	35371.660281	31.407220
537.739396	35428.465620	31.412237
538.060502	35483.790766	31.417255
538.863464	35550.429533	31.422272
539.393497	35608.087496	31.427290
539.656507	35661.087347	31.432308
540.173764	35729.951707	31.437325
541.063759	35787.721113	31.442343
541.223937	35857.714943	31.447360
541.791418	35910.942883	31.452378
542.178457	35968.095437	31.457396
542.553759	36039.354681	31.462413
543.446712	36097.942019	31.467431
543.744989	36169.643751	31.472448
544.583332	36235.976210	31.477466
545.037011	36307.479189	31.482484
545.796097	36356.210805	31.487501
546.302403	36422.507358	31.492519
546.726035	36496.203273	31.497536
547.478246	36547.846533	31.502554
548.249812	36618.149294	31.507572
548.530038	36667.317629	31.512589
549.211903	36718.243932	31.517607
549.629003	36788.255663	31.522624
550.307764	36837.494237	31.527642
550.865338	36910.421648	31.532660
551.309396	36967.902487	31.537677
551.916166	37026.590686	31.542695
552.235269	37092.355694	31.547712
553.174775	37138.708141	31.552730
553.361014	37203.785372	31.557748
553.625155	37258.468860	31.562765
553.902701	37309.634162	31.567783
554.150908	37379.824465	31.572800
555.105511	37431.149531	31.577818
555.576520	37503.153058	31.582836
556.208955	37566.645872	31.587853
557.194046	37634.650980	31.592871
557.531670	37709.638067	31.597888
557.975225	37759.754501	31.602906
558.508208	37833.516660	31.607924
559.244752	37894.269416	31.612941
560.040865	37945.543248	31.617959
560.158765	38014.536022	31.622976
561.090869	38068.495922	31.627994
561.248093	38149.082632	31.633012
561.948923	38210.227439	31.638029
562.591496	38273.272821	31.643047
562.982175	38348.825081	31.648064
563.769166	38407.551047	31.653082
564.571824	38486.211154	31.658100
564.765044	38552.892398	31.663117
565.405640	38614.313674	31.668135
566.268044	38684.675683	31.673152
566.798295	38744.389020	31.678170
567.483557	38805.645720	31.683188
567.946386	38867.229833	31.688205
568.125150	38936.787357	31.693223
568.869966	39006.191516	31.698240
569.380853	39070.145284	31.703258
570.216364	39142.738921	31.708276
570.775048	39226.733090	31.713293
571.548321	39280.391405	31.718311
571.767630	39352.027187	31.723328
572.406670	39403.214305	31.728346
572.962145	39480.565370	31.733364
573.609778	39556.329477	31.738381
573.962627	39618.224725	31.743399
574.563656	39698.066128	31.748416
575.615538	39769.022830	31.753434
576.170349	39825.645181	31.758452
576.687721	39901.564846	31.763469
577.463795	39958.542437	31.768487
577.823787	40021.785802	31.773504
578.463726	40092.123731	31.778522
579.084639	40148.262619	31.783540
579.597205	40223.322601	31.788557
580.118359	40281.852327	31.793575
580.325914	40355.801600	31.798592
581.273626	40418.769151	31.803610
581.755427	40489.905033	31.808628
582.408488	40556.542724	31.813645
583.061109	40628.970453	31.818663
583.686211	40690.947382	31.823680
584.370702	40757.167044	31.828698
584.616077	40832.210571	31.833716
585.476371	40897.135726	31.838733
586.054786	40955.800179	31.843751
586.629560	41037.902629	31.848768
587.169637	41106.032137	31.853786
587.735536	41170.552356	31.858804
588.074500	41247.618334	31.863821
588.730054	41307.161410	31.868839
589.426620	41380.074147	31.873856
589.882183	41446.053179	31.878874
590.481902	41517.577605	31.883892
590.848804	41580.477890	31.888909
591.776449	41648.191682	31.893927
591.745795	41720.269485	31.898944
592.253358	41783.939612	31.903962
593.102872	41850.063271	31.908980
593.569914	41927.622333	31.913997
594.132879	41995.186201	31.919015
594.735756	42065.471471	31.924032
595.362225	42136.488716	31.929050
596.186498	42210.488589	31.934068
596.614017	42289.713206	31.939085
597.326836	42356.132800	31.944103
597.671268	42431.188506	31.949120
598.394590	42506.980601	31.954138
598.957519	42574.625510	31.959156
599.429098	42646.778512	31.964173
600.048306	42730.908038	31.969191
600.568755	42809.172318	31.974208
601.202894	42878.685116	31.979226
601.943387	42960.162451	31.984244
602.374459	43047.469181	31.989261
603.517416	43120.867422	31.994279
603.820553	43200.438532	31.999296
604.267893	43279.904032	32.004314
604.947869	43346.705155	32.009332
605.447696	43435.603098	32.014349
606.357386	43504.415907	32.019367
606.873434	43590.662868	32.024384
607.578054	43670.857866	32.029402
608.210022	43741.305666	32.034420
609.066053	43823.288622	32.039437
609.742637	43897.341723	32.044455
610.001919	43971.224189	32.049472
610.655680	44050.905092	32.054490
611.461429	44119.977328	32.059508
611.878518	44203.234406	32.064525
612.857489	44278.489350	32.069543
613.275658	44363.316237	32.074560
613.516388	44440.039066	32.079578
614.233199	44518.290633	32.084596
614.962453	44600.414788	32.089613
615.467983	44672.244750	32.094631
615.916027	44753.096232	32.099648
616.770297	44830.293827	32.104666
617.816154	44914.015237	32.109684
618.188274	45001.754462	32.114701
618.946474	45069.489751	32.119719
619.902769	45145.250824	32.124736
620.108429	45222.326824	32.129754
621.218695	45299.054548	32.134772
621.378234	45371.932769	32.139789
622.172687	45443.645245	32.144807
623.154733	45524.102235	32.149824
623.482438	45598.355531	32.154842
624.417914	45672.581198	32.159860
624.651248	45755.900797	32.164877
625.277353	45824.298514	32.169895
625.980892	45898.582387	32.174912
626.613209	45981.098051	32.179930
627.277237	46044.213629	32.184948
627.670487	46117.097106	32.189965
628.099768	46198.914696	32.194983
629.213106	46277.155326	32.200000
629.618846	46360.243799	32.205018
630.357273	46427.781968	32.210036
631.034938	46509.461913	32.215053
631.811736	46583.038460	32.220071
632.339572	46663.401752	32.225088
632.554037	46740.447734	32.230106
633.600628	46803.537287	32.235124
633.841232	46861.464536	32.240141
634.477352	46934.907822	32.245159
635.061339	47016.618077	32.250176
635.640290	47085.798686	32.255194
636.367388	47159.824646	32.260212
637.182634	47243.995583	32.265229
637.669109	47309.926938	32.270247
638.186288	47379.106200	32.275264
638.851387	47457.956397	32.280282
639.766535	47525.519760	32.285300
640.122753	47594.874861	32.290317
640.726006	47669.030662	32.295335
641.660839	47744.549874	32.300352
642.147313	47826.507114	32.305370
643.000678	47902.416241	32.310388
643.366860	47979.890582	32.315405
644.074578	48057.892989	32.320423
644.523043	48130.879258	32.325440
644.940336	48213.973902	32.330458
646.011217	48293.515219	32.335476
646.656118	48380.937524	32.340493
646.961002	48462.646451	32.345511
647.799007	48548.906942	32.350528
648.718171	48628.228408	32.355546
649.620851	48701.328045	32.360564
649.824636	48791.718143	32.365581
650.835044	48863.717296	32.370599
651.475842	48937.543341	32.375616
651.948048	49028.044901	32.380634
652.755651	49101.518678	32.385652
653.448123	49194.043794	32.390669
654.099001	49266.697700	32.395687
654.512460	49355.482913	32.400704
655.321410	49435.416557	32.405722
655.886337	49516.202604	32.410740
656.322906	49608.389882	32.415757
657.020159	49690.977159	32.420775
657.980550	49770.653421	32.425792
658.308990	49856.078662	32.430810
659.251937	49951.954973	32.435828
659.877174	50039.489142	32.440845
660.304148	50122.707293	32.445863
660.931225	50211.622188	32.450880
661.734222	50293.907130	32.455898
662.081931	50376.078229	32.460916
662.673042	50472.125873	32.465933
663.331373	50561.555205	32.470951
664.127991	50651.764346	32.475968
664.768570	50750.496277	32.480986
665.685884	50828.134114	32.486004
666.440396	50929.343390	32.491021
666.900956	51013.077821	32.496039
667.846803	51099.840423	32.501056
668.524566	51198.113639	32.506074
669.524251	51286.864435	32.511092
670.276744	51358.031140	32.516109
671.049882	51454.742128	32.521127
671.711964	51519.177427	32.526144
672.032589	51597.927835	32.531162
673.316383	51688.553963	32.536180
673.653717	51765.520764	32.541197
673.916640	51848.154340	32.546215
674.501125	51923.583633	32.551232
675.218999	52017.469989	32.556250
675.954574	52097.505729	32.561268
676.566041	52184.404296	32.566285
676.878771	52260.568466	32.571303
678.090991	52341.897285	32.576320
678.416277	52433.614136	32.581338
679.147910	52505.401300	32.586356
679.758926	52596.364064	32.591373
680.274552	52674.840166	32.596391
681.065325	52750.832399	32.601408
680.979325	52844.836757	32.606426
682.316854	52921.225678	32.611444
683.036193	53011.989236	32.616461
683.276215	53101.019266	32.621479
684.088385	53188.792554	32.626496
684.648493	53286.811440	32.631514
685.403211	53379.049247	32.636532
686.119888	53472.588976	32.641549
686.949732	53577.306023	32.646567
687.846766	53658.660865	32.651584
688.143795	53759.612992	32.656602
689.376305	53848.589637	32.661620
689.751999	53942.567096	32.666637
690.179111	54031.633571	32.671655
691.250200	54127.664023	32.676672
691.809507	54231.740618	32.681690
692.521833	54318.151763	32.686708
692.972878	54405.705897	32.691725
694.073679	54496.767032	32.696743
695.014432	54595.664582	32.701760
695.397313	54694.623320	32.706778
696.369518	54784.298047	32.711796
697.326986	54869.097760	32.716813
697.756725	54972.466747	32.721831
698.582510	55063.102099	32.726848
699.396251	55152.141262	32.731866
699.826856	55227.153755	32.736884
700.748349	55319.910132	32.741901
701.569560	55424.543629	32.746919
702.446740	55510.016508	32.751936
702.952460	55598.660003	32.756954
703.815203	55686.808843	32.761972
704.755705	55770.010263	32.766989
704.950718	55866.143526	32.772007
705.483933	55957.804456	32.777024
706.138745	56052.693580	32.782042
707.349108	56146.309629	32.787060
707.861629	56236.199659	32.792077
708.449225	56327.929124	32.797095
709.481885	56409.538241	32.802112
709.958354	56509.078200	32.807130
710.671650	56594.791378	32.812148
711.691414	56696.763692	32.817165
712.262538	56787.537499	32.822183
712.984720	56865.086119	32.827200
713.781044	56968.626005	32.832218
714.571619	57055.908163	32.837236
715.408421	57148.080429	32.842253
716.131045	57239.551616	32.847271
716.889344	57313.797369	32.852288
717.439550	57405.076659	32.857306
717.978664	57493.312295	32.862324
718.589855	57583.293171	32.867341
719.596924	57678.643615	32.872359
720.107004	57768.616770	32.877376
720.582968	57867.215657	32.882394
721.313092	57952.002909	32.887412
722.361653	58037.989100	32.892429
723.282093	58128.224598	32.897447
723.778383	58225.501105	32.902464
724.370322	58320.512495	32.907482
724.996472	58409.483466	32.912500
726.014534	58494.806780	32.917517
726.301314	58577.312785	32.922535
727.342987	58648.009196	32.927552
727.867153	58735.254248	32.932570
728.456518	58817.698545	32.937588
729.236733	58916.631425	32.942605
729.878993	59000.116797	32.947623
730.487204	59092.285233	32.952640
731.458749	59182.978347	32.957658
732.143957	59268.973018	32.962676
733.066029	59362.108265	32.967693
733.110001	59450.990527	32.972711
733.838220	59544.360915	32.977728
734.831915	59644.917872	32.982746
735.463960	59745.838509	32.987764
736.098915	59844.755715	32.992781
736.435341	59956.470364	32.997799
737.252466	60053.822677	33.002816
738.164170	60167.358320	33.007834
738.813912	60273.992059	33.012852
739.563668	60372.241866	33.017869
740.092107	60492.788624	33.022887
740.997226	60592.789783	33.027904
742.251207	60705.917881	33.032922
742.977116	60814.545389	33.037940
744.123860	60897.228279	33.042957
744.281516	61015.469321	33.047975
745.208453	61108.712896	33.052992
746.026379	61214.211339	33.058010
746.810670	61326.162796	33.063028
747.817038	61425.740460	33.068045
748.061133	61528.636576	33.073063
749.097255	61631.825681	33.078080
749.841437	61733.635135	33.083098
750.617045	61836.994778	33.088116
751.282769	61940.474248	33.093133
751.969329	62049.380291	33.098151
752.758675	62152.119819	33.103168
753.548856	62258.563701	33.108186
754.348979	62366.605657	33.113204
755.494734	62474.293931	33.118221
755.911234	62581.818953	33.123239
756.615957	62676.528616	33.128256
757.283889	62791.598240	33.133274
757.884061	62901.724065	33.138292
758.880347	62999.395773	33.143309
759.452281	63116.284575	33.148327
760.266105	63220.751033	33.153344
761.345338	63332.411792	33.158362
761.740471	63449.919589	33.163380
762.797649	63552.255171	33.168397
763.530231	63660.213937	33.173415
764.537826	63767.710575	33.178432
765.322429	63867.008032	33.183450
766.134304	63977.357421	33.188468
766.735933	64080.207133	33.193485
767.333935	64184.714154	33.198503
768.069920	64295.077785	33.203520
768.656275	64399.783779	33.208538
769.712512	64505.379764	33.213556
770.469333	64622.467733	33.218573
771.240748	64737.309799	33.223591
772.220477	64844.184468	33.228608
772.943521	64956.096211	33.233626
773.886661	65050.360067	33.238644
774.603751	65153.689077	33.243661
775.309897	65266.717895	33.248679
776.067613	65359.591436	33.253696
776.963136	65461.969487	33.258714
777.058114	65564.101143	33.263732
778.396913	65645.582808	33.268749
778.906152	65755.561793	33.273767
779.585086	65856.839668	33.278784
780.388410	65944.227195	33.283802
781.180809	66058.586270	33.288820
781.843167	66159.849385	33.293837
782.506553	66272.372305	33.298855
783.572453	66374.043860	33.303872
784.255530	66480.609284	33.308890
784.704102	66592.366546	33.313908
785.518098	66696.300382	33.318925
786.006772	66812.332262	33.323943
786.999138	66927.914784	33.328960
787.930929	67036.623047	33.333978
788.379440	67159.384016	33.338996
789.300804	67267.406066	33.344013
789.848990	67391.953758	33.349031
790.375745	67504.126518	33.354048
791.776593	67625.354404	33.359066
792.600094	67745.698499	33.364084
793.392715	67864.145320	33.369101
794.086659	67983.627049	33.374119
795.063131	68100.148027	33.379136
796.177748	68222.324479	33.384154
796.764411	68336.666712	33.389172
797.762998	68449.980386	33.394189
798.184375	68573.696118	33.399207
798.977422	68691.382442	33.404224
799.997882	68807.937967	33.409242
800.848370	68932.153859	33.414260
801.981561	69045.796201	33.419277
802.708558	69164.596240	33.424295
803.293749	69276.724441	33.429312
803.997567	69391.248973	33.434330
805.148636	69512.117959	33.439348
805.943114	69625.610755	33.444365
806.740637	69751.958389	33.449383
807.904435	69867.509605	33.454400
808.876377	69971.325875	33.459418
809.418129	70095.485784	33.464436
810.284461	70196.418290	33.469453
811.104254	70320.615718	33.474471
811.701390	70427.992926	33.479488
813.062492	70549.345217	33.484506
813.342214	70661.727217	33.489524
814.211765	70770.793670	33.494541
814.867828	70887.427124	33.499559
816.134801	71008.386557	33.504576
816.686168	71118.019592	33.509594
817.601660	71243.053862	33.514612
818.515158	71353.975105	33.519629
819.363675	71473.488717	33.524647
819.844747	71592.248021	33.529664
821.005292	71690.931951	33.534682
821.698633	71811.206635	33.539700
822.360329	71931.853995	33.544717
823.387588	72042.993938	33.549735
823.760321	72158.669325	33.554752
824.861901	72275.129087	33.559770
825.586325	72411.458049	33.564788
826.420848	72523.720031	33.569805
827.030732	72639.434645	33.574823
828.498340	72754.223852	33.579840
829.109628	72874.391525	33.584858
829.861906	72997.869287	33.589876
830.896415	73105.952664	33.594893
831.607063	73214.494880	33.599911
832.182366	73316.950955	33.604928
833.091183	73423.886743	33.609946
833.477989	73537.505472	33.614964
834.524643	73643.407676	33.619981
835.191454	73758.555966	33.624999
836.040361	73882.111291	33.630016
837.429209	73985.624913	33.635034
837.672133	74105.297425	33.640052
838.553607	74231.119762	33.645069
839.558396	74347.954453	33.650087
840.370429	74474.384163	33.655104
841.358063	74580.699102	33.660122
841.942924	74702.057540	33.665140
843.171414	74822.703048	33.670157
843.676565	74940.192730	33.675175
844.019421	75063.889001	33.680192
844.967562	75190.502706	33.685210
845.782206	75319.751301	33.690228
846.380156	75447.904371	33.695245
847.500025	75591.220806	33.700263
848.106904	75716.591074	33.705280
849.159568	75847.188519	33.710298
849.665935	75990.267465	33.715316
850.903587	76125.649173	33.720333
851.985873	76242.000400	33.725351
852.570095	76388.750149	33.730368
853.327747	76518.850073	33.735386
854.512833	76653.003996	33.740404
855.400940	76788.959891	33.745421
856.433805	76918.067876	33.750439
857.340161	77049.784520	33.755456
858.587806	77173.165828	33.760474
858.952259	77305.220285	33.765492
859.872165	77436.462583	33.770509
861.127382	77566.669778	33.775527
861.772285	77694.606665	33.780544
862.634707	77818.909174	33.785562
863.601318	77946.882856	33.790580
864.755268	78072.890703	33.795597
865.438906	78206.902865	33.800615
866.122143	78338.322432	33.805632
867.058061	78461.395529	33.810650
868.070615	78596.241199	33.815668
868.882620	78724.877451	33.820685
869.978538	78850.254049	33.825703
870.520508	78983.895761	33.830720
871.713585	79105.987331	33.835738
872.433645	79242.877857	33.840756
873.097156	79367.538125	33.845773
874.491243	79489.263263	33.850791
874.941779	79622.847972	33.855808
876.209597	79749.535907	33.860826
877.104574	79883.295365	33.865844
878.113818	80009.957938	33.870861
878.895872	80135.178501	33.875879
879.753807	80267.232002	33.880896
880.601065	80389.027114	33.885914
881.081518	80520.423340	33.890932
881.819120	80650.038105	33.895949
883.266441	80771.198307	33.900967
884.119371	80905.584390	33.905984
884.969212	81028.793255	33.911002
885.488491	81169.018281	33.916020
886.249060	81292.395166	33.921037
887.426252	81431.209775	33.926055
887.941242	81567.370095	33.931072
889.250485	81687.393947	33.936090
889.915157	81804.001173	33.941108
890.701941	81931.286941	33.946125
891.569439	82051.841269	33.951143
892.161562	82187.834361	33.956160
893.121285	82313.233634	33.961178
894.331811	82431.917493	33.966196
894.764141	82564.978369	33.971213
896.073947	82695.136451	33.976231
896.603269	82822.931594	33.981248
897.808703	82950.976265	33.986266
898.303911	83090.881709	33.991284
899.190640	83225.800946	33.996301
900.509192	83360.396484	34.001319
901.110814	83485.260309	34.006336
901.923507	83626.033901	34.011354
902.930443	83762.619374	34.016372
903.667667	83901.471054	34.021389
904.821659	84041.665589	34.026407
905.471082	84185.734368	34.031424
906.659168	84317.408606	34.036442
907.454382	84459.468243	34.041460
907.979499	84611.013674	34.046477
909.352636	84754.466447	34.051495
910.002108	84895.287388	34.056512
911.234959	85035.088912	34.061530
911.961555	85178.727146	34.066548
912.635105	85330.531116	34.071565
913.749322	85480.523140	34.076583
914.554136	85615.950703	34.081600
915.637797	85759.925770	34.086618
917.096720	85908.395542	34.091636
917.745437	86049.533617	34.096653
918.996890	86190.421004	34.101671
920.122507	86331.950163	34.106688
920.925932	86469.534313	34.111706
921.696635	86615.028094	34.116724
922.511723	86758.920821	34.121741
923.655132	86893.249343	34.126759
924.552558	87038.965247	34.131776
925.402597	87172.166881	34.136794
926.453073	87311.316063	34.141812
927.363401	87466.764912	34.146829
928.440561	87606.303757	34.151847
929.147357	87749.935669	34.156864
930.120458	87878.912749	34.161882
931.345137	88029.263459	34.166900
932.111921	88171.641356	34.171917
933.133912	88318.350724	34.176935
933.514960	88461.888933	34.181952
934.367135	88611.172161	34.186970
935.654010	88755.593868	34.191988
936.279710	88908.086919	34.197005
937.271624	89055.204491	34.202023
938.265059	89207.961399	34.207040
939.189733	89353.971789	34.212058
939.798590	89510.287569	34.217076
940.947071	89655.167945	34.222093
942.074977	89808.229208	34.227111
942.960029	89961.723986	34.232128
943.693509	90112.732305	34.237146
944.818758	90263.278077	34.242164
945.819289	90423.319638	34.247181
946.683977	90566.980355	34.252199
947.598134	90722.994059	34.257216
948.433345	90869.648688	34.262234
949.237808	91024.498971	34.267252
950.077613	91184.407606	34.272269
951.294495	91333.274051	34.277287
952.533531	91483.220021	34.282304
953.460236	91625.648936	34.287322
954.222660	91764.390638	34.292340
954.981816	91901.677958	34.297357
956.047855	92047.548379	34.302375
956.873995	92191.345369	34.307392
957.922040	92332.030472	34.312410
959.150003	92485.528875	34.317428
959.653246	92622.179008	34.322445
960.941915	92774.713458	34.327463
961.863730	92920.543332	34.332480
962.892907	93066.622162	34.337498
963.977692	93213.838315	34.342516
964.727749	93365.630017	34.347533
965.462474	93503.778555	34.352551
966.454865	93658.089158	34.357568
967.409395	93823.914366	34.362586
968.516619	93968.612123	34.367604
969.275174	94133.541354	34.372621
970.409375	94286.212030	34.377639
971.330985	94451.445577	34.382656
972.328248	94612.945745	34.387674
973.248149	94767.477843	34.392692
974.162309	94935.127563	34.397709
975.390315	95092.452905	34.402727
976.175564	95253.954335	34.407744
976.899285	95415.599921	34.412762
978.069265	95579.495932	34.417780
978.584672	95750.337855	34.422797
979.899608	95917.845653	34.427815
981.005994	96087.528694	34.432832
981.884014	96259.497911	34.437850
982.954223	96427.328133	34.442868
983.432806	96598.105988	34.447885
984.664356	96778.724621	34.452903
985.894978	96951.703812	34.457920
986.964083	97119.488217	34.462938
987.901759	97291.492645	34.467956
988.629851	97467.375589	34.472973
989.990342	97645.700123	34.477991
990.823187	97813.471250	34.483008
991.678051	97990.147215	34.488026
992.993716	98164.424824	34.493044
993.788204	98339.581165	34.498061
994.934856	98510.881963	34.503079
995.825754	98685.841165	34.508096
997.030789	98864.693825	34.513114
997.927960	99038.267940	34.518132
998.727345	99213.986643	34.523149
1000.193264	99393.895168	34.528167
1001.131387	99564.952660	34.533184
1002.196525	99739.561088	34.538202
1003.440352	99906.467719	34.543220
1003.834576	100087.615655	34.548237
1005.001650	100257.766219	34.553255
1006.399379	100433.147465	34.558272
1007.117345	100613.454172	34.563290
1008.179432	100776.711654	34.568308
1009.210929	100958.824058	34.573325
1010.131604	101120.720512	34.578343
1011.202899	101305.507025	34.583360
1011.832608	101477.628668	34.588378
1013.294996	101647.125441	34.593396
1014.356723	101818.456117	34.598413
1015.415000	101999.355758	34.603431
1016.687842	102167.943858	34.608448
1017.504277	102347.423275	34.613466
1018.274416	102507.073849	34.618484
1019.057988	102667.869257	34.623501
1020.096648	102830.826999	34.628519
1021.468722	103001.746926	34.633536
1022.410166	103161.968402	34.638554
1023.646977	103305.678668	34.643572
1024.208851	103479.692759	34.648589
1025.039152	103648.496599	34.653607
1026.324264	103813.376362	34.658624
1027.110365	103995.753285	34.663642
1028.350157	104162.757704	34.668660
1029.065831	104340.374138	34.673677
1030.171666	104513.785905	34.678695
1031.184412	104693.027343	34.683712
1032.015153	104870.210389	34.688730
1033.354608	105046.765922	34.693748
1034.079968	105230.921875	34.698765
1035.190591	105407.403668	34.703783
1036.199885	105590.324655	34.708800
1037.019257	105777.077898	34.713818
1038.247525	105964.157475	34.718836
1039.389976	106152.620432	34.723853
1040.152360	106335.511383	34.728871
1041.463906	106517.489525	34.733888
1042.353237	106708.100762	34.738906
1043.481654	106893.493502	34.743924
1044.453307	107085.968367	34.748941
1045.651985	107273.619326	34.753959
1046.974371	107470.852055	34.758976
1047.604155	107658.751761	34.763994
1049.308530	107843.878524	34.769012
1050.322067	108027.258826	34.774029
1051.164368	108218.141898	34.779047
1052.503783	108398.392896	34.784064
1053.210103	108602.968376	34.789082
1054.495139	108784.700273	34.794100
1055.499911	108969.785765	34.799117
1056.724864	109163.006269	34.804135
1057.583234	109355.832744	34.809152
1058.862304	109550.351756	34.814170
1059.906461	109733.168531	34.819188
1060.623556	109930.620617	34.824205
1061.733117	110119.851472	34.829223
1063.252643	110303.796875	34.834240
1063.893820	110501.987685	34.839258
1065.345269	110688.594443	34.844276
1066.263353	110880.395735	34.849293
1067.211889	111071.952643	34.854311
1068.520886	111270.114593	34.859328
1069.349996	111467.432548	34.864346
1070.808591	111650.915670	34.869364
1071.591246	111851.651758	34.874381
1072.722886	112044.540641	34.879399
1073.922633	112232.770336	34.884416
1074.866900	112434.484727	34.889434
1076.054756	112624.631977	34.894452
1077.015360	112819.746178	34.899469
1078.214007	113021.891513	34.904487
1079.361113	113208.755635	34.909504
1080.400452	113401.985918	34.914522
1081.436457	113595.547481	34.919540
1082.386691	113791.506339	34.924557
1083.618043	113987.331408	34.929575
1084.867762	114176.845545	34.934592
1085.361092	114376.798810	34.939610
1086.611100	114570.471080	34.944628
1087.839816	114772.269328	34.949645
1089.227453	114968.784880	34.954663
1090.248153	115155.302769	34.959680
1090.947924	115344.826990	34.964698
1092.302955	115530.531895	34.969716
1093.208299	115703.629804	34.974733
1093.683023	115899.808617	34.979751
1094.856760	116088.955367	34.984768
1095.920070	116285.597013	34.989786
1096.779879	116477.573003	34.994804
1097.932626	116671.440412	34.999821
1098.835756	116872.179748	35.004839
1099.893324	117080.776005	35.009856
1100.829712	117290.040012	35.014874
1101.806323	117501.440238	35.019892
1102.707289	117713.120609	35.024909
1103.631829	117934.428497	35.029927
1104.920327	118148.100673	35.034944
1106.032896	118364.907924	35.039962
1107.161843	118591.660947	35.044980
1108.625331	118817.891600	35.049997
1109.475477	119041.881213	35.055015
1110.452436	119252.445193	35.060032
1111.711613	119485.519382	35.065050
1113.122073	119706.380300	35.070068
1114.270128	119931.873437	35.075085
1115.286893	120155.844051	35.080103
1116.680541	120369.730573	35.085120
1117.783549	120600.203692	35.090138
1118.677922	120822.514241	35.095156
1119.966100	121035.751419	35.100173
1121.133457	121271.566824	35.105191
1122.285568	121491.013872	35.110208
1123.463107	121724.752929	35.115226
1124.551888	121946.368145	35.120244
1125.688320	122170.030112	35.125261
1126.658156	122405.925203	35.130279
1128.376330	122625.211011	35.135296
1129.185919	122852.733999	35.140314
1130.317494	123078.114427	35.145332
1131.488599	123311.752930	35.150349
1132.479956	123549.453069	35.155367
1133.572328	123765.010669	35.160384
1134.841105	124005.520057	35.165402
1136.090219	124239.000778	35.170420
1137.333611	124464.956090	35.175437
1138.177499	124705.604655	35.180455
1139.694400	124939.109875	35.185472
1140.449381	125172.185190	35.190490
1141.670480	125399.228426	35.195508
1143.159428	125628.992039	35.200525
1144.422889	125866.690712	35.205543
1145.789136	126092.903958	35.210560
1146.722823	126323.829224	35.215578
1147.921883	126550.555110	35.220596
1149.159370	126778.873318	35.225613
1150.110984	127001.853719	35.230631
1151.734925	127228.121437	35.235648
1152.653686	127462.378500	35.240666
1153.750449	127685.567984	35.245684
1155.175297	127910.377949	35.250701
1155.966528	128148.463797	35.255719
1157.082991	128368.093196	35.260736
1158.608011	128607.899166	35.265754
1159.354276	128831.066070	35.270772
1160.737060	129058.527758	35.275789
1161.477305	129300.306715	35.280807
1163.295474	129514.960713	35.285824
1164.118504	129734.800305	35.290842
1165.765843	129964.062807	35.295860
1166.893148	130173.080625	35.300877
1168.033699	130402.341349	35.305895
1169.456315	130600.082153	35.310912
1170.156014	130800.935287	35.315930
1171.488713	131015.654371	35.320948
1172.681743	131224.782337	35.325965
1173.800231	131441.783429	35.330983
1175.095754	131646.650585	35.336000
1175.965598	131849.535800	35.341018
1176.401738	132077.758759	35.346036
1177.750727	132292.610491	35.351053
1178.942567	132524.654200	35.356071
1180.392135	132749.076115	35.361088
1181.275510	132986.904152	35.366106
1182.406107	133211.432713	35.371124
1183.607655	133439.183810	35.376141
1184.584281	133685.964405	35.381159
1185.886987	133914.297946	35.386176
1186.999155	134154.682917	35.391194
1187.754874	134395.559618	35.396212
1189.370810	134639.008936	35.401229
1190.074054	134872.062960	35.406247
1191.538745	135124.643577	35.411264
1192.720892	135374.521701	35.416282
1193.775013	135621.849219	35.421300
1195.105123	135869.487957	35.426317
1196.248054	136124.715768	35.431335
1197.369116	136378.808098	35.436352
1198.831848	136624.997888	35.441370
1200.360251	136884.275649	35.446388
1201.622425	137124.378504	35.451405
1202.572672	137382.018710	35.456423
1203.765895	137628.184363	35.461440
1205.085815	137886.185733	35.466458
1205.944240	138132.676676	35.471476
1207.430677	138386.280063	35.476493
1208.324683	138646.652579	35.481511
1209.801502	138910.772609	35.486528
1210.933783	139164.414999	35.491546
1211.960157	139425.811321	35.496564
1213.515231	139687.451925	35.501581
1214.373879	139952.316188	35.506599
1216.032018	140208.960595	35.511616
1217.555099	140461.165900	35.516634
1218.716897	140725.669017	35.521652
1220.178657	140983.137820	35.526669
1221.297672	141245.927492	35.531687
1222.340288	141487.010376	35.536704
1223.503277	141744.470817	35.541722
1225.146251	142008.029237	35.546740
1226.410992	142269.635951	35.551757
1227.734129	142517.463723	35.556775
1228.846458	142769.436669	35.561792
1230.376247	143017.145049	35.566810
1231.448676	143275.316487	35.571828
1233.024220	143524.009985	35.576845
1234.139701	143773.440696	35.581863
1235.299519	144029.992694	35.586880
1236.646243	144274.975637	35.591898
1237.681248	144532.984886	35.596916
1239.410838	144769.715749	35.601933
1240.394764	145022.106386	35.606951
1241.629512	145269.612937	35.611968
1243.234647	145522.551184	35.616986
1244.011670	145765.533323	35.622004
1245.173021	146001.897009	35.627021
1246.170449	146259.595145	35.632039
1247.804266	146513.245787	35.637056
1249.371868	146750.067176	35.642074
1250.094560	146994.867413	35.647092
1251.406449	147224.733531	35.652109
1252.500054	147458.619464	35.657127
1253.691456	147701.926531	35.662144
1255.312211	147945.214977	35.667162
1256.093004	148178.979648	35.672180
1257.356742	148415.862038	35.677197
1258.758847	148664.962042	35.682215
1259.670875	148906.420808	35.687232
1260.895213	149150.036372	35.692250
1262.003130	149404.922699	35.697268
1263.516923	149652.742556	35.702285
1264.727386	149905.383109	35.707303
1265.712446	150154.003943	35.712320
1266.899863	150416.050126	35.717338
1268.088934	150676.969024	35.722356
1269.666576	150939.398276	35.727373
1270.465461	151210.139066	35.732391
1271.676444	151472.125263	35.737408
1273.397835	151744.543862	35.742426
1274.220189	152024.342881	35.747444
1275.873747	152284.232075	35.752461
1277.159787	152558.605682	35.757479
1278.331428	152829.118772	35.762496
1280.067463	153090.636067	35.767514
1281.053887	153365.876747	35.772532
1282.892712	153630.437658	35.777549
1284.206710	153911.310742	35.782567
1285.101883	154173.748088	35.787584
1286.736162	154427.046160	35.792602
1287.834348	154714.823170	35.797620
1289.269020	154978.419870	35.802637
1290.597261	155252.183971	35.807655
1291.613052	155523.375790	35.812672
1293.174504	155797.231980	35.817690
1294.288910	156078.508748	35.822708
1295.438042	156346.068845	35.827725
1297.220013	156622.735814	35.832743
1298.560559	156905.084682	35.837760
1299.702750	157162.528307	35.842778
1300.828507	157449.102773	35.847796
1302.157060	157722.198772	35.852813
1303.527948	157996.088836	35.857831
1305.336029	158281.110245	35.862848
1306.607244	158542.562812	35.867866
1307.741032	158821.876539	35.872884
1309.123970	159087.513264	35.877901
1310.569448	159363.988204	35.882919
1311.427960	159646.968665	35.887936
1313.103397	159927.545170	35.892954
1314.273616	160206.621254	35.897972
1315.666974	160478.824214	35.902989
1317.226158	160755.391178	35.908007
1318.237843	161029.170547	35.913024
1319.572786	161312.159755	35.918042
1320.650977	161597.692654	35.923060
1321.974578	161866.845933	35.928077
1323.375845	162154.460653	35.933095
1324.569675	162442.733291	35.938112
1326.142254	162721.011086	35.943130
1327.487159	163016.824329	35.948148
1328.975419	163287.545355	35.953165
1330.378881	163573.025123	35.958183
1331.698726	163851.745378	35.963200
1332.968159	164123.573616	35.968218
1334.202006	164402.007138	35.973236
1335.770864	164682.264903	35.978253
1337.144586	164952.076418	35.983271
1337.753454	165217.993881	35.988288
1339.477595	165474.225203	35.993306
1340.243204	165745.969224	35.998324
1341.455152	166023.046394	36.003341
1342.869742	166299.571595	36.008359
1343.900430	166578.001805	36.013376
1345.485109	166854.984533	36.018394
1346.472562	167138.437393	36.023412
1348.058363	167417.542446	36.028429
1349.581133	167701.278387	36.033447
1350.499628	167996.675573	36.038464
1352.238302	168275.481549	36.043482
1353.176389	168573.531276	36.048500
1354.789764	168868.755889	36.053517
1355.992792	169157.210744	36.058535
1356.861643	169455.239629	36.063552
1358.466003	169751.448528	36.068570
1359.838094	170063.090056	36.073588
1361.151199	170368.842796	36.078605
1362.599252	170663.928650	36.083623
1363.690432	170975.432410	36.088640
1365.506865	171288.493458	36.093658
1367.047425	171601.665646	36.098676
1368.017888	171900.251836	36.103693
1369.345301	172207.232512	36.108711
1370.469802	172529.261155	36.113728
1371.828191	172836.405769	36.118746
1373.100958	173156.510633	36.123764
1374.792422	173484.035787	36.128781
1376.220675	173801.378149	36.133799
1377.402702	174133.154399	36.138816
1378.919700	174450.676732	36.143834
1380.267609	174785.843833	36.148852
1381.901637	175113.148412	36.153869
1383.249838	175441.086202	36.158887
1384.538294	175764.873411	36.163904
1385.794482	176092.272349	36.168922
1387.091713	176425.390388	36.173940
1388.854941	176747.696861	36.178957
1389.936720	177082.212868	36.183975
1391.427310	177418.935317	36.188992
1392.722781	177748.331199	36.194010
1393.943865	178085.102641	36.199028
1395.701018	178422.612696	36.204045
1397.292444	178750.950859	36.209063
1398.886924	179099.851398	36.214080
1400.293538	179428.173679	36.219098
1401.534210	179763.467997	36.224116
1402.714684	180092.352244	36.229133
1404.304959	180432.403416	36.234151
1405.638176	180770.278140	36.239168
1406.923619	181104.101393	36.244186
1408.533388	181448.217481	36.249204
1409.740342	181795.803960	36.254221
1411.575240	182130.951770	36.259239
1412.644460	182479.276256	36.264256
1414.120321	182813.002631	36.269274
1415.535757	183153.684028	36.274292
1416.638815	183501.844533	36.279309
1418.536840	183842.869385	36.284327
1419.756403	184184.757370	36.289344
1421.325568	184534.459460	36.294362
1422.411583	184872.134284	36.299380
1424.133809	185214.504102	36.304397
1426.034964	185559.943644	36.309415
1426.867724	185917.074824	36.314432
1428.559177	186254.632595	36.319450
1429.863266	186593.183028	36.324468
1430.987655	186923.158866	36.329485
1432.586807	187246.800149	36.334503
1433.931571	187581.998595	36.339520
1435.226325	187911.050721	36.344538
1436.722532	188242.102470	36.349556
1437.991042	188568.661962	36.354573
1439.681115	188897.400484	36.359591
1441.038094	189239.245509	36.364608
1442.544390	189577.703872	36.369626
1443.844464	189913.938658	36.374644
1445.033428	190258.635482	36.379661
1446.542204	190589.863394	36.384679
1447.808085	190943.386803	36.389696
1449.251015	191280.621225	36.394714
1450.697696	191641.024710	36.399732
1452.432327	191997.942465	36.404749
1453.672260	192342.693524	36.409767
1454.904307	192697.641827	36.414784
1456.409289	193046.605814	36.419802
1458.004969	193404.341748	36.424820
1459.319350	193774.338918	36.429837
1460.771203	194126.910428	36.434855
1462.192685	194499.585535	36.439872
1463.686019	194868.531214	36.444890
1465.351060	195238.847143	36.449908
1466.736397	195600.692743	36.454925
1468.451673	195966.611906	36.459943
1470.019877	196342.625062	36.464960
1471.510118	196712.127664	36.469978
1473.140016	197078.003661	36.474996
1474.513285	197449.408684	36.480013
1476.454273	197809.892353	36.485031
1477.732304	198175.438932	36.490048
1479.096586	198540.985934	36.495066
1480.700263	198908.120450	36.500084
1481.966448	199281.825847	36.505101
1483.742387	199649.304058	36.510119
1485.512812	200028.186431	36.515136
1486.924709	200401.061227	36.520154
1488.211215	200760.678225	36.525172
1489.195752	201141.626326	36.530189
1491.288176	201508.960420	36.535207
1492.573856	201887.209160	36.540224
1494.264533	202260.682487	36.545242
1496.194227	202633.826222	36.550260
1496.861783	203003.117409	36.555277
1498.787636	203379.160461	36.560295
1500.085888	203766.165044	36.565312
1501.466645	204136.740721	36.570330
1503.325904	204521.751970	36.575348
1504.359584	204906.292122	36.580365
1506.272224	205280.531202	36.585383
1507.481460	205663.687560	36.590400
1509.103257	206042.511342	36.595418
1510.536656	206433.849671	36.600436
1511.988009	206824.818763	36.605453
1513.630339	207200.127551	36.610471
1515.267498	207593.558461	36.615488
1516.518233	207975.652637	36.620506
1518.135795	208357.776900	36.625524
1519.393030	208748.025592	36.630541
1521.515385	209144.672606	36.635559
1522.828734	209536.922032	36.640576
1524.144438	209923.128680	36.645594
1525.532056	210302.214326	36.650612
1526.859796	210702.974508	36.655629
1528.584104	211096.356918	36.660647
1530.202440	211483.663497	36.665664
1531.371579	211858.576327	36.670682
1532.719097	212230.566078	36.675700
1534.002555	212621.488556	36.680717
1535.877095	212994.816667	36.685735
1537.300658	213377.058984	36.690752
1538.538997	213768.882818	36.695770
1540.316801	214153.914355	36.700788
1541.665548	214541.278749	36.705805
1542.987906	214927.430048	36.710823
1544.817596	215328.382054	36.715840
1546.164976	215716.157899	36.720858
1548.102074	216119.940039	36.725876
1549.050786	216526.071380	36.730893
1550.863533	216920.531017	36.735911
1552.215648	217326.776829	36.740928
1553.638341	217733.114241	36.745946
1555.407280	218136.703889	36.750964
1556.946455	218557.730966	36.755981
1558.459631	218975.284490	36.760999
1560.187710	219391.407281	36.766016
1561.471967	219803.439682	36.771034
1563.334339	220219.391185	36.776052
1564.556154	220632.707065	36.781069
1566.393297	221055.803060	36.786087
1567.861002	221483.787550	36.791104
1569.513467	221910.498623	36.796122
1571.354643	222340.177264	36.801140
1573.244859	222762.915427	36.806157
1574.871734	223178.561429	36.811175
1576.257564	223604.764145	36.816192
1577.619165	224038.566900	36.821210
1579.409836	224449.847036	36.826228
1581.184835	224956.558166	36.831245
1582.374208	225389.911670	36.836263
1584.129152	225810.346278	36.841280
1585.502620	226260.461796	36.846298
1587.134044	226680.691126	36.851316
1588.682742	227120.569881	36.856333
1590.248079	227554.605305	36.861351
1592.039477	227990.814648	36.866368
1593.466481	228449.412642	36.871386
1595.226769	228878.975079	36.876404
1596.839918	229321.822303	36.881421
1598.536056	229763.082377	36.886439
1600.138679	230210.226859	36.891456
1601.845971	230655.297968	36.896474
1603.498889	231083.995795	36.901492
1605.034198	231529.199559	36.906509
1606.548764	231973.188808	36.911527
1608.107968	232414.403239	36.916544
1609.774677	232866.066473	36.921562
1611.548717	233299.779927	36.926580
1612.998135	233762.581962	36.931597
1614.674382	234207.084175	36.936615
1616.352307	234653.924231	36.941632
1617.770833	235108.377983	36.946650
1619.697851	235549.159034	36.951668
1621.175429	236005.510476	36.956685
1622.926415	236454.781610	36.961703
1624.589055	236900.867798	36.966720
1626.164700	237351.059120	36.971738
1627.739564	237787.305946	36.976756
1629.284245	238244.667806	36.981773
1630.965846	238686.843049	36.986791
1632.968014	239132.116154	36.991808
1634.496427	239589.255077	36.996826
1636.311355	240039.793865	37.001844
1637.900719	240474.443600	37.006861
1639.485094	240901.906135	37.011879
1641.350143	241320.940311	37.016896
1642.805317	241744.208934	37.021914
1644.211487	242164.793728	37.026932
1646.097576	242596.248440	37.031949
1647.316111	243021.641331	37.036967
1649.163275	243451.859173	37.041984
1650.686875	243888.303989	37.047002
1652.391637	244327.945706	37.052020
1653.744363	244767.061985	37.057037
1655.200774	245205.425110	37.062055
1656.840909	245640.862597	37.067072
1658.198546	246095.323258	37.072090
1660.070668	246545.076244	37.077108
1661.426773	247005.533473	37.082125
1662.943740	247460.909548	37.087143
1664.745091	247926.756036	37.092160
1666.087668	248395.320781	37.097178
1668.125511	248851.781006	37.102196
1669.879771	249335.622241	37.107213
1671.856323	249803.474162	37.112231
1673.125303	250272.611973	37.117248
1674.436415	250742.530768	37.122266
1676.580418	251220.797057	37.127284
1678.480661	251710.281414	37.132301
1679.905089	252180.944803	37.137319
1681.803160	252656.153685	37.142336
1683.309372	253137.981651	37.147354
1684.798595	253610.159505	37.152372
1686.411609	254106.653489	37.157389
1688.111235	254589.618905	37.162407
1690.431195	255070.754662	37.167424
1691.773509	255572.806580	37.172442
1693.355441	256058.484791	37.177460
1695.409140	256558.819134	37.182477
1697.113507	257045.671343	37.187495
1698.711904	257533.836714	37.192512
1700.476994	258032.516984	37.197530
1702.295329	258520.442894	37.202548
1704.317500	259019.055335	37.207565
1705.907467	259504.199177	37.212583
1707.689767	259995.103150	37.217600
1709.453757	260495.028234	37.222618
1711.203763	260976.131674	37.227636
1713.055839	261473.222186	37.232653
1714.491127	261964.868854	37.237671
1716.394507	262452.094050	37.242688
1717.985631	262955.577868	37.247706
1719.860011	263446.922691	37.252724
1721.658502	263948.161612	37.257741
1723.388659	264444.661092	37.262759
1725.193487	264938.505953	37.267776
1726.880945	265439.330287	37.272794
1728.637363	265925.027944	37.277812
1730.638645	266424.986686	37.282829
1732.196088	266925.246884	37.287847
1734.280080	267416.909576	37.292864
1735.865996	267912.362854	37.297882
1737.728249	268408.989275	37.302900
1739.684689	268900.315728	37.307917
1740.933963	269399.176028	37.312935
1742.725325	269874.067402	37.317952
1744.158059	270388.544257	37.322970
1746.231702	270885.996204	37.327988
1747.736274	271383.338173	37.333005
1749.072024	271886.219648	37.338023
1751.031667	272385.034433	37.343040
1752.953620	272893.075771	37.348058
1754.595638	273371.136538	37.353076
1756.028134	273854.311598	37.358093
1757.155129	274342.210309	37.363111
1759.274404	274826.489478	37.368128
1761.046934	275322.738725	37.373146
1762.659655	275813.958283	37.378164
1764.360236	276311.614503	37.383181
1765.850927	276814.359366	37.388199
1767.961217	277313.749286	37.393216
1769.393288	277824.833457	37.398234
1771.000899	278335.658788	37.403252
1772.879565	278847.174749	37.408269
1774.670440	279366.375305	37.413287
1776.152258	279880.189525	37.418304
1777.672264	280407.611441	37.423322
1779.551625	280927.428201	37.428340
1781.528657	281456.448162	37.433357
1783.284545	281990.761210	37.438375
1785.137522	282530.162293	37.443392
1786.679549	283074.794919	37.448410
1788.430747	283606.690543	37.453428
1790.566161	284148.402075	37.458445
1791.655193	284696.406268	37.463463
1793.505789	285241.412444	37.468480
1795.324940	285806.539469	37.473498
1797.081988	286364.105152	37.478516
1798.671132	286912.450556	37.483533
1800.746368	287485.809498	37.488551
1802.664871	288049.590570	37.493568
1804.631917	288617.704818	37.498586
1806.684347	289180.239905	37.503604
1808.429229	289745.896847	37.508621
1809.862006	290312.212495	37.513639
1811.930935	290872.324579	37.518656
1813.689104	291443.915481	37.523674
1815.796185	292016.360527	37.528692
1817.723725	292589.518332	37.533709
1819.508521	293165.744927	37.538727
1821.443129	293739.683417	37.543744
1823.576721	294317.573907	37.548762
1824.975568	294885.829518	37.553780
1827.460448	295443.006702	37.558797
1829.183485	296035.179654	37.563815
1830.888999	296596.137147	37.568832
1832.887650	297167.863139	37.573850
1834.589395	297735.291924	37.578868
1836.802417	298305.782592	37.583885
1838.662555	298882.093774	37.588903
1840.324527	299449.799045	37.593920
1842.505765	300029.047609	37.598938
1844.208447	300596.460219	37.603956
1846.581494	301159.669790	37.608973
1848.180305	301743.855270	37.613991
1849.756227	302297.970449	37.619008
1851.400510	302875.284102	37.624026
1853.290040	303454.712390	37.629044
1855.291908	304031.197796	37.634061
1857.066984	304611.297891	37.639079
1859.154997	305185.348931	37.644096
1860.915111	305758.688465	37.649114
1862.892571	306332.420046	37.654132
1864.927306	306906.620844	37.659149
1866.331091	307478.636303	37.664167
1868.202763	308064.690587	37.669184
1870.508150	308632.282736	37.674202
1871.841653	309224.360156	37.679220
1874.082459	309795.027666	37.684237
1875.471879	310375.380188	37.689255
1877.681538	310925.474780	37.694272
1879.220513	311491.014583	37.699290
1880.738440	312056.985423	37.704308
1882.696710	312612.874028	37.709325
1884.401018	313185.662122	37.714343
1886.029401	313738.524198	37.719360
1888.208201	314311.326848	37.724378
1889.623673	314896.084412	37.729396
1891.874463	315476.357081	37.734413
1894.109709	316056.932341	37.739431
1895.666141	316629.235311	37.744448
1897.311452	317213.123375	37.749466
1898.900368	317805.953981	37.754484
1900.943625	318388.826906	37.759501
1902.954723	318997.447613	37.764519
1904.947152	319593.954066	37.769536
1906.861655	320189.528581	37.774554
1908.379377	320797.376462	37.779572
1910.460434	321404.465526	37.784589
1912.566496	322012.636593	37.789607
1914.473516	322629.924595	37.794624
1916.193835	323245.688638	37.799642
1918.281747	323873.877883	37.804660
1920.468792	324478.355762	37.809677
1922.448713	325093.779450	37.814695
1923.639790	325716.563166	37.819712
1925.844577	326347.373778	37.824730
1927.415457	326974.017139	37.829748
1929.706648	327600.255711	37.834765
1931.439479	328245.138633	37.839783
1933.529364	328875.433599	37.844800
1935.544440	329500.301112	37.849818
1937.088980	330149.941459	37.854836
1939.272507	330795.000770	37.859853
1941.348974	331448.321103	37.864871
1943.090364	332090.366759	37.869888
1945.469709	332728.390177	37.874906
1947.091196	333384.910729	37.879924
1949.327312	334024.770482	37.884941
1951.362234	334687.756507	37.889959
1953.265737	335334.738106	37.894976
1955.453501	335981.741049	37.899994
1957.246511	336638.294978	37.905012
1959.245270	337278.890892	37.910029
1961.321046	337932.462643	37.915047
1963.538810	338589.607084	37.920064
1965.408938	339234.667341	37.925082
1967.352642	339897.754358	37.930100
1969.858100	340541.398460	37.935117
1971.674171	341197.458369	37.940135
1973.675300	341849.087964	37.945152
1975.813432	342492.614981	37.950170
1977.729843	343155.256648	37.955188
1979.720232	343799.298309	37.960205
1981.744425	344453.173307	37.965223
1983.365638	345102.207490	37.970240
1985.569674	345752.202457	37.975258
1987.335148	346412.361768	37.980276
1989.511399	347070.261282	37.985293
1991.942717	347722.652891	37.990311
1993.790918	348382.491154	37.995328
1995.578588	349036.112245	38.000346
1997.779733	349691.406641	38.005364
1999.473087	350334.035959	38.010381
2001.429584	350997.421476	38.015399
2003.229686	351655.214660	38.020416
2005.775640	352316.097577	38.025434
2007.505353	352973.857131	38.030452
2009.643387	353598.855971	38.035469
2011.760537	354222.377410	38.040487
2013.624643	354861.790553	38.045504
2015.869898	355481.390063	38.050522
2017.430895	356114.110133	38.055540
2019.689311	356743.812923	38.060557
2021.670419	357383.701121	38.065575
2023.270611	358015.345455	38.070592
2025.010803	358659.617649	38.075610
2027.251585	359304.050722	38.080628
2029.204954	359950.550687	38.085645
2030.991145	360595.723193	38.090663
2033.333452	361253.580211	38.095680
2035.203411	361905.516959	38.100698
2037.003849	362574.680415	38.105716
2039.043378	363238.186369	38.110733
2041.127961	363902.257057	38.115751
2042.940875	364576.381697	38.120768
2045.329186	365241.393910	38.125786
2047.155959	365923.432716	38.130804
2049.374192	366599.382657	38.135821
2051.120244	367281.993736	38.140839
2053.218210	367974.122663	38.145856
2055.562295	368659.603033	38.150874
2057.480665	369354.627543	38.155892
2059.671000	370045.586400	38.160909
2061.528187	370747.747423	38.165927
2063.690536	371445.608753	38.170944
2065.684094	372137.676277	38.175962
2067.852467	372856.230962	38.180980
2070.175771	373553.415986	38.185997
2072.055429	374259.232768	38.191015
2074.262042	374966.198758	38.196032
2076.757054	375666.864126	38.201050
2078.974321	376386.150205	38.206068
2080.927535	377081.170390	38.211085
2082.934291	377788.618993	38.216103
2084.962612	378496.226887	38.221120
2087.212927	379208.778917	38.226138
2089.574331	379911.103841	38.231156
2091.090219	380627.576037	38.236173
2093.381610	381340.963479	38.241191
2095.700328	382058.311926	38.246208
2097.965499	382769.314766	38.251226
2099.599892	383496.176964	38.256244
2101.990225	384215.342607	38.261261
2103.870089	384942.740411	38.266279
2105.950698	385668.389989	38.271296
2108.207529	386391.661598	38.276314
2109.895618	387123.554244	38.281332
2112.165692	387852.469195	38.286349
2113.974972	388584.967073	38.291367
2116.155163	389329.275781	38.296384
2118.687213	390061.061986	38.301402
2120.401815	390808.656784	38.306420
2122.639089	391537.237309	38.311437
2125.163952	392283.901947	38.316455
2126.915178	393021.297541	38.321472
2129.069018	393765.325505	38.326490
2131.001513	394496.648000	38.331508
2133.425703	395248.603817	38.336525
2135.812945	395987.950482	38.341543
2137.739765	396735.946252	38.346560
2140.074056	397478.178856	38.351578
2141.802283	398219.732393	38.356596
2144.043407	398963.893968	38.361613
2146.216620	399714.560340	38.366631
2148.138651	400455.441769	38.371648
2150.441328	401179.542135	38.376666
2152.398939	401906.037617	38.381684
2154.601092	402626.646209	38.386701
2156.762162	403344.608010	38.391719
2158.500831	404079.673249	38.396736
2161.093637	404793.700666	38.401754
2162.965926	405530.884508	38.406772
2164.820557	406264.732665	38.411789
2167.195355	406999.184756	38.416807
2169.160442	407744.730405	38.421824
2171.393591	408477.798047	38.426842
2173.259914	409233.553800	38.431860
2175.282932	409987.945240	38.436877
2177.695455	410745.442902	38.441895
2179.556249	411508.430851	38.446912
2181.489669	412265.736344	38.451930
2183.598026	413048.674896	38.456948
2185.972864	413818.020839	38.461965
2188.259588	414591.411091	38.466983
2190.140595	415389.716197	38.472000
2192.635219	416170.395152	38.477018
2194.502877	416971.414084	38.482036
2196.673685	417760.835331	38.487053
2199.162079	418557.371622	38.492071
2201.018620	419353.328787	38.497088
2203.261624	420147.804351	38.502106
2205.556763	420964.604800	38.507124
2207.836246	421776.342370	38.512141
2210.387857	422593.477534	38.517159
2212.353933	423413.897809	38.522176
2214.814833	424224.031281	38.527194
2216.973900	425046.086755	38.532212
2219.319619	425863.577404	38.537229
2221.553543	426672.147941	38.542247
2224.079583	427497.249441	38.547264
2226.343438	428319.277586	38.552282
2228.440118	429143.380668	38.557300
2230.847413	429968.365756	38.562317
2233.358351	430787.129086	38.567335
2235.364945	431614.704444	38.572352
2237.887131	432431.434380	38.577370
2240.610884	433252.657915	38.582388
2242.511469	434077.025110	38.587405
2244.788794	434897.099818	38.592423
2246.796806	435721.036147	38.597440
2249.908441	436537.270471	38.602458
2252.163037	437378.566438	38.607476
2254.417760	438191.036557	38.612493
2256.972636	439005.047181	38.617511
2259.150520	439822.430223	38.622528
2261.519373	440629.024619	38.627546
2264.045168	441449.478378	38.632564
2266.100206	442266.994230	38.637581
2268.433865	443077.148166	38.642599
2270.462444	443892.988904	38.647616
2273.234060	444704.831646	38.652634
2275.352488	445519.433073	38.657652
2277.453099	446337.800805	38.662669
2279.679030	447143.976374	38.667687
2282.508665	447971.621004	38.672704
2284.319247	448784.834367	38.677722
2286.843326	449594.105450	38.682740
2288.981190	450410.743039	38.687757
2291.476016	451216.770422	38.692775
2293.564078	452036.943949	38.697792
2295.906773	452845.260143	38.702810
2298.199092	453672.314499	38.707828
2300.031244	454483.938172	38.712845
2302.524413	455263.210659	38.717863
2304.608078	456062.594891	38.722880
2307.091565	456852.224667	38.727898
2309.368795	457634.122268	38.732916
2311.206717	458421.573031	38.737933
2313.548811	459207.443816	38.742951
2316.081006	460012.412401	38.747968
2318.204220	460809.479558	38.752986
2320.570105	461613.197962	38.758004
2322.389764	462425.263828	38.763021
2324.862112	463234.560344	38.768039
2327.077618	464050.537775	38.773056
2329.497252	464878.779706	38.778074
2331.856233	465698.051172	38.783092
2333.404577	466528.388495	38.788109
2336.120503	467359.205125	38.793127
2338.178777	468202.778254	38.798144
2340.585314	469051.107870	38.803162
2343.002674	469898.236020	38.808180
2344.858670	470763.507473	38.813197
2347.332517	471607.518761	38.818215
2349.785116	472487.113437	38.823232
2351.712670	473363.116366	38.828250
2354.441475	474240.613266	38.833268
2356.762940	475121.167050	38.838285
2359.276428	475994.777914	38.843303
2361.629764	476878.627451	38.848320
2363.834222	477770.994926	38.853338
2366.301063	478658.225363	38.858356
2368.446045	479551.526169	38.863373
2370.883102	480453.117951	38.868391
2373.339313	481344.208939	38.873408
2375.152462	482254.095595	38.878426
2378.150952	483177.373520	38.883444
2380.500996	484073.396193	38.888461
2382.707021	484972.325920	38.893479
2384.888432	485902.464010	38.898496
2386.820211	486830.625680	38.903514
2389.541087	487762.798063	38.908532
2391.860494	488695.542460	38.913549
2394.317575	489620.744337	38.918567
2396.625375	490567.169902	38.923584
2399.001333	491505.710055	38.928602
2401.560346	492447.096003	38.933620
2404.033824	493403.583290	38.938637
2406.534859	494332.310282	38.943655
2408.627813	495284.011948	38.948672
2410.671037	496238.292132	38.953690
2413.307983	497197.919723	38.958708
2415.852204	498161.039343	38.963725
2418.587819	499121.045384	38.968743
2420.976041	500078.884567	38.973760
2423.733161	501030.756769	38.978778
2426.588770	501994.864605	38.983796
2429.004328	502948.750689	38.988813
2431.761456	503889.060042	38.993831
2434.091448	504837.101349	38.998848
2436.778730	505774.792328	39.003866
2439.768643	506718.934126	39.008884
2441.836972	507667.559350	39.013901
2444.391584	508603.847807	39.018919
2446.818416	509546.202750	39.023936
2449.624480	510478.357547	39.028954
2452.456337	511414.586947	39.033972
2454.427276	512354.078629	39.038989
2457.174431	513277.963610	39.044007
2459.451549	514210.691668	39.049024
2461.649706	515124.378237	39.054042
2464.513504	516028.327008	39.059060
2466.437954	516934.948161	39.064077
2468.912479	517834.522632	39.069095
2471.603829	518730.431751	39.074112
2474.030834	519623.309535	39.079130
2476.439311	520522.637197	39.084148
2478.660771	521434.838819	39.089165
2481.108395	522337.327517	39.094183
2483.721681	523252.327477	39.099200
2485.437002	524168.477943	39.104218
2487.990487	525085.492102	39.109236
2490.563606	526023.195217	39.114253
2492.548142	526953.584664	39.119271
2495.193661	527892.820281	39.124288
2497.576941	528834.355911	39.129306
2500.104835	529782.101182	39.134324
2502.289347	530731.352536	39.139341
2504.973162	531692.390890	39.144359
2507.275358	532655.694310	39.149376
2509.233453	533632.732003	39.154394
2511.809420	534611.816651	39.159412
2514.349814	535590.790667	39.164429
2516.717467	536587.994159	39.169447
2519.705525	537580.396721	39.174464
2521.697124	538580.844896	39.179482
2524.100807	539586.035312	39.184500
2526.782609	540590.203222	39.189517
2529.407157	541600.547292	39.194535
2532.001712	542610.421561	39.199552
2533.997714	543643.559885	39.204570
2537.026349	544663.224179	39.209588
2539.656076	545695.050175	39.214605
2541.926543	546726.557132	39.219623
2544.774537	547756.986898	39.224640
2547.507947	548804.001178	39.229658
2549.962753	549824.687401	39.234676
2552.134618	550873.546875	39.239693
2554.853382	551914.494213	39.244711
2558.286395	552969.569338	39.249728
2560.561907	554020.380534	39.254746
2563.021155	555055.801613	39.259764
2565.622430	556104.536957	39.264781
2568.250407	557148.864387	39.269799
2570.930687	558199.733752	39.274816
2573.805386	559251.794232	39.279834
2576.573759	560300.121397	39.284852
2578.985562	561352.191552	39.289869
2581.627187	562404.792590	39.294887
2584.326866	563447.455437	39.299904
2587.018868	564500.381716	39.304922
2589.678564	565540.774362	39.309940
2592.268617	566596.359582	39.314957
2594.889227	567642.514700	39.319975
2597.779798	568705.559486	39.324992
2600.009977	569758.484620	39.330010
2602.986856	570802.917455	39.335028
2605.480209	571860.093081	39.340045
2607.774267	572915.306332	39.345063
2610.433571	573978.049313	39.350080
2612.810173	575033.774323	39.355098
2615.632984	576092.196895	39.360116
2618.571060	577159.039884	39.365133
2620.602770	578209.085094	39.370151
2623.374958	579272.362853	39.375168
2626.011971	580351.571883	39.380186
2628.342942	581419.051175	39.385204
2631.071979	582482.661032	39.390221
2633.502999	583544.572864	39.395239
2636.298226	584591.540776	39.400256
2638.417993	585635.722320	39.405274
2641.105572	586664.430030	39.410292
2643.505530	587710.341435	39.415309
2646.261337	588748.334173	39.420327
2648.902533	589799.437246	39.425344
2651.395781	590856.285578	39.430362
2654.358703	591899.583351	39.435380
2656.927382	592950.921475	39.440397
2659.589348	594014.024772	39.445415
2662.295234	595073.568352	39.450432
2664.676178	596136.776838	39.455450
2667.338420	597209.609498	39.460468
2669.936842	598279.849979	39.465485
2672.892359	599354.490253	39.470503
2675.578604	600438.889766	39.475520
2677.885390	601526.504604	39.480538
2680.896110	602616.203614	39.485556
2683.520847	603710.568417	39.490573
2686.292517	604805.004537	39.495591
2688.812825	605892.720472	39.500608
2691.163882	607010.937594	39.505626
2693.921474	608108.811229	39.510644
2696.515117	609233.373813	39.515661
2699.210212	610354.455249	39.520679
2701.691751	611490.467251	39.525696
2704.044985	612633.187589	39.530714
2706.652162	613757.043318	39.535732
2709.786544	614916.655078	39.540749
2712.354536	616062.287459	39.545767
2715.166282	617215.710371	39.550784
2717.681494	618377.759932	39.555802
2720.530985	619536.781631	39.560820
2723.492980	620704.808478	39.565837
2725.701512	621876.082583	39.570855
2728.713252	623050.345749	39.575872
2731.490755	624228.017434	39.580890
2734.539796	625393.824437	39.585908
2736.855674	626585.402715	39.590925
2739.588473	627771.734339	39.595943
2742.645053	628959.678335	39.600960
2745.130921	630149.730759	39.605978
2747.717905	631349.019988	39.610996
2750.787431	632548.642291	39.616013
2753.324474	633750.312008	39.621031
2756.459495	634951.645231	39.626048
2758.958546	636158.834285	39.631066
2761.882551	637360.872423	39.636084
2764.534504	638573.244673	39.641101
2766.891585	639788.815997	39.646119
2769.832949	641007.838878	39.651136
2772.984927	642227.928989	39.656154
2775.729265	643438.115122	39.661172
2778.873475	644659.660986	39.666189
2781.307592	645885.664438	39.671207
2784.532682	647098.126755	39.676224
2787.142730	648317.174672	39.681242
2790.033977	649534.682331	39.686260
2792.917432	650743.171745	39.691277
2795.681174	651961.002610	39.696295
2798.704753	653179.837174	39.701312
2801.263421	654405.822318	39.706330
2804.670408	655621.104065	39.711348
2807.086367	656827.582980	39.716365
2809.526855	658063.342334	39.721383
2812.220399	659280.379659	39.726400
2814.905587	660506.278118	39.731418
2817.660116	661718.568817	39.736436
2820.567243	662919.631904	39.741453
2823.135999	664122.144031	39.746471
2825.836735	665307.663471	39.751488
2828.630393	666495.459011	39.756506
2831.360049	667693.664795	39.761524
2834.446702	668893.600935	39.766541
2836.817905	670099.223300	39.771559
2839.590807	671298.409054	39.776576
2842.122654	672518.367268	39.781594
2844.888511	673737.830157	39.786612
2847.338420	674962.008578	39.791629
2850.332562	676205.024305	39.796647
2853.294087	677455.533202	39.801664
2855.663798	678696.479501	39.806682
2858.433196	679951.155380	39.811700
2861.427677	681213.721145	39.816717
2863.768478	682504.087833	39.821735
2866.530665	683766.737593	39.826752
2869.591387	685057.816844	39.831770
2872.140498	686346.612357	39.836788
2875.314841	687638.646258	39.841805
2878.038928	688959.111389	39.846823
2880.872514	690265.071047	39.851840
2883.599119	691583.710655	39.856858
2886.564956	692912.237963	39.861876
2889.254662	694235.850214	39.866893
2892.216691	695574.100594	39.871911
2895.200522	696911.252256	39.876928
2897.917598	698261.732535	39.881946
2900.652776	699613.787099	39.886964
2903.716786	700961.464315	39.891981
2906.503479	702324.492378	39.896999
2909.571923	703689.391247	39.902016
2912.567817	705060.577840	39.907034
2915.416588	706429.738044	39.912052
2918.509484	707797.401929	39.917069
2921.148782	709187.653919	39.922087
2924.224315	710569.190257	39.927104
2927.324848	711970.945035	39.932122
2929.861938	713355.929486	39.937140
2933.164256	714740.759040	39.942157
2936.085292	716133.885605	39.947175
2939.036691	717529.843638	39.952192
2942.092792	718935.692346	39.957210
2944.983352	720343.507673	39.962228
2948.194869	721738.570424	39.967245
2950.775239	723155.503851	39.972263
2954.082580	724554.723412	39.977280
2957.438494	725963.483171	39.982298
2960.114035	727374.929874	39.987316
2963.805555	728772.328950	39.992333
2966.832985	730186.541679	39.997351
2969.967755	731569.325048	40.002368
2972.959025	732970.019017	40.007386
2976.199415	734365.046986	40.012404
2979.482371	735761.504256	40.017421
2982.297192	737153.748097	40.022439
2985.150386	738535.231853	40.027456
2988.470287	739929.375087	40.032474
2991.215583	741319.421611	40.037492
2994.598353	742697.034876	40.042509
2997.312899	744092.467459	40.047527
3000.218665	745477.069546	40.052544
3003.670514	746861.533962	40.057562
3006.503395	748253.149260	40.062580
3009.606114	749640.923133	40.067597
3012.162690	751033.662659	40.072615
3015.232563	752395.229655	40.077632
3018.421285	753748.754657	40.082650
3021.101268	755098.136287	40.087668
3024.526495	756434.799409	40.092685
3027.223927	757771.446851	40.097703
3030.296454	759117.395024	40.102720
3033.126842	760470.230295	40.107738
3035.861861	761819.788902	40.112756
3039.116953	763166.708226	40.117773
3041.506458	764533.595029	40.122791
3044.404810	765906.737756	40.127808
3047.666081	767276.667538	40.132826
3050.352112	768655.631981	40.137844
3053.459301	770045.869138	40.142861
3056.218377	771436.590344	40.147879
3059.069865	772839.364927	40.152896
3062.456231	774244.828975	40.157914
3064.987874	775664.012792	40.162932
3068.118883	777080.514517	40.167949
3070.921988	778513.484915	40.172967
3073.786477	779955.634554	40.177984
3076.871708	781411.297844	40.183002
3079.608939	782863.781131	40.188020
3083.231897	784322.937083	40.193037
3086.144133	785795.300673	40.198055
3088.970826	787266.688423	40.203072
3092.528545	788738.631931	40.208090
3095.542132	790235.648132	40.213108
3098.572590	791713.725382	40.218125
3101.738194	793202.737624	40.223143
3104.602651	794689.035054	40.228160
3107.828381	796192.879402	40.233178
3111.095539	797696.197075	40.238196
3114.417068	799205.397029	40.243213
3117.497081	800721.012390	40.248231
3120.339949	802235.747373	40.253248
3124.085945	803745.793868	40.258266
3126.809390	805272.939384	40.263284
3129.899491	806791.665446	40.268301
3133.263007	808322.619516	40.273319
3136.488644	809848.950980	40.278336
3139.726321	811384.170916	40.283354
3142.481800	812924.836484	40.288372
3146.206890	814451.022424	40.293389
3149.489422	815989.921592	40.298407
3152.849851	817529.332405	40.303424
3156.016435	819060.415950	40.308442
3158.916103	820603.437250	40.313460
3162.306980	822142.018068	40.318477
3165.237302	823680.803773	40.323495
3168.359491	825240.309744	40.328512
3171.904902	826782.314105	40.333530
3174.748419	828329.382278	40.338548
3177.728276	829875.914397	40.343565
3181.019765	831433.181545	40.348583
3184.026737	832989.633842	40.353600
3187.622601	834541.475103	40.358618
3190.558401	836105.170724	40.363636
3193.990963	837663.001277	40.368653
3197.115729	839232.811446	40.373671
3200.167995	840800.349550	40.378688
3203.616061	842360.821865	40.383706
3206.673718	843928.265844	40.388724
3209.994928	845495.762731	40.393741
3213.250957	847061.615979	40.398759
3216.074503	848643.471615	40.403776
3219.616526	850211.986466	40.408794
3222.601328	851794.472788	40.413812
3225.933410	853349.120418	40.418829
3229.033666	854888.079841	40.423847
3232.027730	856414.931136	40.428864
3235.141856	857939.637008	40.433882
3238.188383	859477.067819	40.438900
3241.407802	861011.077158	40.443917
3244.768224	862542.156230	40.448935
3247.490524	864088.557290	40.453952
3250.831308	865638.918011	40.458970
3253.963538	867201.409927	40.463988
3256.882133	868758.979438	40.469005
3260.166243	870333.123022	40.474023
3263.086092	871918.332701	40.479040
3266.385857	873508.089325	40.484058
3269.406086	875096.402031	40.489076
3272.378685	876705.572276	40.494093
3275.741876	878322.360397	40.499111
3278.352359	879939.407713	40.504128
3281.685476	881569.804301	40.509146
3285.181108	883209.668901	40.514164
3288.291067	884850.969903	40.519181
3291.696328	886506.626186	40.524199
3294.937361	888169.363946	40.529216
3298.432258	889833.413465	40.534234
3301.423574	891515.681298	40.539252
3304.587813	893200.126481	40.544269
3308.309784	894892.080604	40.549287
3311.316543	896580.661406	40.554304
3314.402457	898272.194651	40.559322
3318.108655	899987.873319	40.564340
3321.379620	901685.864837	40.569357
3324.627439	903398.555555	40.574375
3327.498183	905112.516013	40.579392
3331.376082	906836.365629	40.584410
3334.826650	908580.331292	40.589428
3337.874378	910304.008791	40.594445
3341.693319	912037.592918	40.599463
3345.134676	913767.329777	40.604480
3348.476298	915507.967023	40.609498
3351.891506	917239.203531	40.614516
3355.087089	918985.475761	40.619533
3358.597744	920731.997525	40.624551
3361.959037	922480.569651	40.629568
3365.457930	924238.716533	40.634586
3368.837565	925997.266004	40.639604
3372.183676	927745.851492	40.644621
3375.833601	929488.352936	40.649639
3379.277441	931263.453323	40.654656
3382.575270	933010.410550	40.659674
3385.544846	934771.103951	40.664692
3389.077088	936536.186198	40.669709
3392.726752	938302.376485	40.674727
3395.498214	940084.463625	40.679744
3399.185560	941847.630733	40.684762
3402.754803	943633.530954	40.689780
3405.837194	945414.405849	40.694797
3409.269408	947185.060248	40.699815
3412.131352	948969.515071	40.704832
3415.628640	950761.448778	40.709850
3418.954095	952559.744128	40.714868
3422.209443	954408.369411	40.719885
3425.733205	956257.121750	40.724903
3428.768650	958113.379367	40.729920
3432.127223	959968.008759	40.734938
3435.496820	961842.264590	40.739956
3438.705696	963706.657448	40.744973
3442.443539	965580.220729	40.749991
3445.448744	967448.803629	40.755008
3448.749722	969301.859559	40.760013
3452.066132	971124.372318	40.765018
3455.211551	972866.945973	40.770023
3458.706786	974558.009464	40.775028
3461.904643	976194.294541	40.780032
3464.956245	977736.651063	40.785037
3467.861668	979214.355153	40.790042
3471.066650	980623.575385	40.795047
3474.134091	981951.451550	40.800052
3476.565137	983205.441783	40.805056
3479.186127	984388.385692	40.810061
3482.107736	985490.456251	40.815066
3484.374108	986512.150300	40.820071
3486.228014	987462.735376	40.825076
3488.435877	988368.934324	40.830080
3490.982925	989197.916881	40.835085
3492.905626	989950.947712	40.840090
3494.809795	990647.450119	40.845095
3496.903213	991287.020816	40.850100
3498.311448	991872.161694	40.855104
3500.006933	992390.452661	40.860109
3501.896190	992874.370422	40.865114
3503.182047	993285.477228	40.870119
3504.160943	993665.530251	40.875124
3505.446000	993999.434095	40.880128
3506.920817	994285.755048	40.885133
3508.016111	994539.495944	40.890138
3508.975375	994742.116204	40.895143
3510.386383	994913.684492	40.900148
3511.334002	995050.945770	40.905152
3512.274054	995159.475892	40.910157
3513.427640	995214.796260	40.915162
3514.011233	995267.872742	40.920167
3514.667220	995270.102045	40.925172
3515.282885	995268.053048	40.930176
3516.126599	995216.299869	40.935181
3516.859076	995152.001630	40.940186
3517.444314	995067.275372	40.945191
3518.238287	994959.821560	40.950196
3517.945774	994834.429723	40.955200
3518.941680	994688.077765	40.960205
3519.659259	994532.612513	40.965210
3519.924231	994347.705185	40.970215
3520.425418	994146.486423	40.975220
3520.798187	993935.540898	40.980224
3521.210120	993713.963213	40.985229
3521.810859	993469.453079	40.990234
3521.663653	993219.015578	40.995239
3522.287414	992955.969663	41.000244
3522.294917	992693.402801	41.005248
3522.785407	992408.042117	41.010253
3523.323505	992102.197018	41.015258
3523.247045	991795.559688	41.020263
3523.455591	991486.617498	41.025268
3523.708795	991168.197980	41.030272
3523.880595	990832.231039	41.035277
3524.118485	990493.211867	41.040282
3524.064205	990161.141166	41.045287
3524.313672	989796.735581	41.050292
3524.311347	989451.650150	41.055296
3524.496818	989090.719304	41.060301
3524.823290	988730.912286	41.065306
3524.541815	988353.437011	41.070311
3524.957363	987976.016872	41.075316
3524.645375	987611.758762	41.080320
3524.702273	987229.569881	41.085325
3525.003784	986836.976896	41.090330
3525.056800	986451.517925	41.095335
3525.085161	986075.303480	41.100340
3525.145761	985683.255873	41.105344
3525.136914	985287.583136	41.110349
3525.149506	984890.806183	41.115354
3525.229010	984489.404785	41.120359
3525.203343	984079.991132	41.125364
3525.207906	983678.057039	41.130368
3525.137504	983267.128600	41.135373
3525.164600	982862.107942	41.140378
3524.892710	982469.796361	41.145383
3525.372398	982049.124269	41.150388
3525.025195	981654.231085	41.155392
3524.993772	981228.701770	41.160397
3524.922024	980825.700538	41.165402
3525.241890	980412.158897	41.170407
3524.935041	979999.276423	41.175412
3524.952185	979598.224461	41.180416
3525.050085	979173.204164	41.185421
3524.914804	978743.893253	41.190426
3524.789768	978329.785751	41.195431
3524.993090	977923.506405	41.200436
3524.752984	977507.893058	41.205440
3524.863522	977082.031280	41.210445
3524.591814	976669.195353	41.215450
3525.008327	976248.790217	41.220455
3524.645257	975832.195895	41.225460
3524.881163	975423.290551	41.230464
3524.604112	975006.133268	41.235469
3524.368870	974587.081634	41.240474
3524.453679	974168.826305	41.245479
3524.607852	973750.724497	41.250484
3524.349073	973333.344513	41.255488
3524.307401	972924.013056	41.260493
3524.105095	972501.479218	41.265498
3523.949555	972085.555681	41.270503
3524.217370	971673.737134	41.275508
3523.572467	971273.970457	41.280512
3523.681768	970850.970176	41.285517
3523.799472	970447.597124	41.290522
3523.493258	970025.289049	41.295527
3523.621902	969611.878062	41.300532
3523.570154	969211.282872	41.305536
3523.222455	968792.999795	41.310541
3523.661664	968394.419136	41.315546
3523.480717	967992.488161	41.320551
3523.449440	967580.816373	41.325556
3523.294309	967175.398879	41.330560
3523.008333	966776.042411	41.335565
3523.122397	966361.518840	41.340570
3523.091341	965960.301830	41.345575
3523.123719	965545.341288	41.350580
3522.822461	965147.244611	41.355584
3522.707042	964746.054623	41.360589
3522.673946	964341.396087	41.365594
3522.833844	963950.582023	41.370599
3522.851203	963543.998577	41.375604
3522.336868	963150.401316	41.380608
3522.325279	962756.302531	41.385613
3522.478407	962362.345517	41.390618
3522.223644	961963.433060	41.395623
3522.428323	961560.988624	41.400628
3522.413015	961174.814986	41.405632
3522.058703	960781.617136	41.410637
3522.112317	960395.281897	41.415642
3521.893355	960000.636694	41.420647
3521.750959	959612.223489	41.425652
3521.857309	959223.449120	41.430656
3521.595704	958818.243838	41.435661
3521.379518	958439.662553	41.440666
3521.178475	958072.130250	41.445671
3521.229515	957685.123643	41.450676
3521.058145	957295.186695	41.455680
3521.409271	956926.117925	41.460685
3521.152244	956545.360168	41.465690
3520.990204	956164.169422	41.470695
3521.077141	955800.563165	41.475700
3520.814449	955419.241744	41.480704
3520.956390	955034.395949	41.485709
3521.144751	954664.522892	41.490714
3520.622599	954290.329384	41.495719
3520.786226	953917.077656	41.500724
3520.271334	953551.172808	41.505728
3520.204219	953182.718424	41.510733
3520.341184	952812.931502	41.515738
3520.138002	952456.500191	41.520743
3520.136704	952100.102494	41.525748
3520.027541	951750.583408	41.530752
3519.677646	951396.489159	41.535757
3519.790390	951050.328618	41.540762
3519.303349	950700.417177	41.545767
3519.680313	950355.600821	41.550772
3519.423849	950010.291536	41.555776
3519.680984	949673.485050	41.560781
3519.203934	949323.477648	41.565786
3519.166388	948991.937316	41.570791
3519.309947	948648.766729	41.575796
3519.272853	948313.928852	41.580800
3518.832831	947980.379673	41.585805
3518.973971	947627.474783	41.590810
3518.832054	947297.852080	41.595815
3518.703503	946963.994111	41.600820
3518.700701	946636.029099	41.605824
3518.529240	946298.880148	41.610829
3518.435873	945960.738807	41.615834
3518.303505	945639.529471	41.620839
3518.148547	945311.696670	41.625844
3518.321950	944998.153240	41.630848
3518.411824	944667.366304	41.635853
3518.377960	944341.367272	41.640858
3518.153828	944016.049477	41.645863
3518.077497	943691.644720	41.650868
3518.270117	943379.053524	41.655872
3517.454935	943057.700288	41.660877
3517.537226	942731.868075	41.665882
3517.745073	942424.965023	41.670887
3517.877382	942102.438352	41.675892
3517.597120	941783.409176	41.680896
3517.677969	941476.758435	41.685901
3517.646497	941155.637341	41.690906
3517.381359	940841.147783	41.695911
3517.299444	940524.883820	41.700916
3517.312304	940219.607813	41.705920
3517.064651	939910.330881	41.710925
3516.887193	939605.817102	41.715930
3517.061569	939304.199454	41.720935
3516.893466	938994.663359	41.725940
3516.735718	938700.160093	41.730944
3516.692824	938392.101698	41.735949
3516.752716	938093.021811	41.740954
3516.220402	937801.310378	41.745959
3516.503312	937496.693657	41.750964
3516.331978	937217.549023	41.755968
3516.308927	936927.143548	41.760973
3516.107287	936630.516861	41.765978
3515.939165	936347.488703	41.770983
3515.864429	936041.599352	41.775988
3515.983839	935764.439843	41.780992
3515.857414	935476.081572	41.785997
3516.264461	935189.922211	41.791002
3515.823049	934904.942484	41.796007
3515.680387	934614.716644	41.801012
3515.572459	934340.494068	41.806016
3515.291157	934056.401589	41.811021
3515.663271	933784.278128	41.816026
3515.452181	933507.534030	41.821031
3515.533288	933224.680651	41.826036
3515.156869	932950.717948	41.831040
3514.837313	932668.380682	41.836045
3514.976758	932400.735676	41.841050
3514.544892	932125.491394	41.846055
3515.123382	931853.426442	41.851060
3514.934353	931594.243009	41.856064
3514.575428	931318.944750	41.861069
3514.711980	931058.625323	41.866074
3514.399866	930813.058406	41.871079
3514.902336	930534.600812	41.876084
3514.605025	930274.122298	41.881088
3514.396838	930013.904424	41.886093
3514.526329	929757.747933	41.891098
3514.208095	929495.313837	41.896103
3514.316446	929231.643898	41.901108
3514.101776	928978.964398	41.906112
3514.351950	928734.073205	41.911117
3514.373582	928461.926172	41.916122
3514.095200	928206.434631	41.921127
3513.951632	927945.048132	41.926132
3513.629799	927703.758546	41.931136
3513.753022	927460.366991	41.936141
3513.698822	927203.445301	41.941146
3513.772536	926960.231276	41.946151
3514.055582	926702.461200	41.951156
3513.862376	926448.312883	41.956160
3513.558531	926195.131763	41.961165
3513.749685	925953.390271	41.966170
3513.581322	925709.967042	41.971175
3513.470626	925459.891077	41.976180
3513.350483	925225.761375	41.981184
3513.461347	924968.416772	41.986189
3513.357232	924733.205520	41.991194
3512.674104	924490.003941	41.996199
3512.859167	924247.032864	42.001204
3512.914973	924026.377574	42.006208
3512.898108	923795.245045	42.011213
3512.816960	923546.805709	42.016218
3512.583564	923319.246036	42.021223
3512.568343	923090.198378	42.026228
3512.717166	922862.267927	42.031232
3512.756747	922633.191799	42.036237
3512.727319	922409.983856	42.041242
3512.370824	922188.551736	42.046247
3512.664665	921958.539452	42.051252
3512.370051	921739.098481	42.056256
3512.194418	921508.663437	42.061261
3512.042856	921286.198619	42.066266
3511.995856	921060.532907	42.071271
3512.065410	920850.423121	42.076276
3512.009408	920633.495328	42.081280
3511.875824	920413.204314	42.086285
3511.782221	920184.623463	42.091290
3511.730721	919979.502845	42.096295
3511.891335	919761.157365	42.101300
3511.379786	919544.934527	42.106304
3511.151553	919341.262213	42.111309
3511.816581	919126.272251	42.116314
3511.405452	918926.848684	42.121319
3511.310124	918717.549420	42.126324
3511.440192	918513.787007	42.131328
3511.213092	918307.092168	42.136333
3511.240701	918102.368742	42.141338
3510.671298	917906.494993	42.146343
3510.823698	917696.345541	42.151348
3510.743568	917510.098828	42.156352
3510.876368	917319.190017	42.161357
3510.961609	917112.109497	42.166362
3510.734771	916920.379546	42.171367
3510.566984	916722.182762	42.176372
3510.505891	916529.641559	42.181376
3510.506270	916341.993747	42.186381
3510.689321	916148.147202	42.191386
3510.352763	915960.252912	42.196391
3510.469005	915766.981558	42.201396
3510.199465	915587.344394	42.206400
3510.212574	915394.462022	42.211405
3510.507788	915216.934475	42.216410
3510.214436	915034.490335	42.221415
3510.162942	914838.517264	42.226420
3510.053013	914660.171622	42.231424
3509.870459	914474.223358	42.236429
3510.289611	914291.251787	42.241434
3509.783561	914121.622361	42.246439
3510.166161	913933.250941	42.251444
3510.071441	913753.428406	42.256448
3510.110768	913578.009040	42.261453
3510.299997	913384.930497	42.266458
3509.897058	913214.292662	42.271463
3510.264404	913033.021678	42.276468
3509.995736	912846.839699	42.281472
3509.626102	912677.046746	42.286477
3509.996816	912498.840622	42.291482
3509.664789	912325.658417	42.296487
3509.981111	912143.595682	42.301492
3509.641103	911960.286040	42.306496
3509.391432	911788.133265	42.311501
3509.840969	911616.630820	42.316506
3509.460003	911449.307261	42.321511
3509.805256	911268.174464	42.326516
3509.577800	911098.309329	42.331520
3509.655837	910926.653860	42.336525
3509.760910	910757.494442	42.341530
3509.385154	910581.951466	42.346535
3509.494789	910399.672366	42.351540
3509.633626	910235.888949	42.356544
3509.500192	910068.000722	42.361549
3509.792021	909899.844540	42.366554
3509.199578	909735.973978	42.371559
3509.386156	909554.425468	42.376564
3509.016334	909382.313743	42.381568
3508.786012	909232.154161	42.386573
3509.048886	909059.831754	42.391578
3508.673101	908905.252467	42.396583
3508.796917	908742.005711	42.401588
3508.972719	908590.508419	42.406592
3508.802501	908428.361440	42.411597
3508.695442	908274.105928	42.416602
3508.455378	908114.853938	42.421607
3508.652301	907958.803918	42.426612
3507.995190	907804.047370	42.431616
3508.270509	907662.537055	42.436621
3508.587539	907524.487927	42.441626
3508.292873	907380.653447	42.446631
3508.192027	907220.581331	42.451636
3508.450966	907071.536288	42.456640
3508.389899	906923.407976	42.461645
3508.415147	906770.631979	42.466650
3508.680204	906624.081580	42.471655
3508.488814	906461.012515	42.476660
3508.454710	906306.015091	42.481664
3507.905131	906158.911444	42.486669
3507.949395	906002.156379	42.491674
3507.843639	905868.476538	42.496679
3507.834138	905727.832055	42.501684
3508.017767	905593.229733	42.506688
3507.869054	905445.558837	42.511693
3507.707438	905309.270048	42.516698
3507.580244	905168.534357	42.521703
3507.556419	905032.602004	42.526708
3507.612127	904889.224211	42.531712
3507.665193	904762.920696	42.536717
3507.714106	904629.185636	42.541722
3507.620671	904493.830532	42.546727
3507.412195	904360.903348	42.551732
3507.827792	904223.817506	42.556736
3507.586373	904089.827878	42.561741
3507.428027	903958.716258	42.566746
3507.471140	903825.927884	42.571751
3507.527974	903691.300564	42.576756
3507.759022	903556.737805	42.581760
3507.601985	903432.465396	42.586765
3507.686235	903287.015139	42.591770
3507.241712	903160.467841	42.596775
3507.693076	903020.161745	42.601780
3507.661211	902904.253618	42.606784
3507.455293	902759.609580	42.611789
3507.420109	902616.381478	42.616794
3507.414574	902501.425876	42.621799
3507.129793	902363.541142	42.626804
3507.286906	902233.495410	42.631808
3507.110518	902117.305227	42.636813
3507.166012	901977.520891	42.641818
3507.524532	901855.348756	42.646823
3507.413007	901726.493925	42.651828
3507.428444	901594.139861	42.656832
3507.079616	901474.875572	42.661837
3507.216443	901331.779399	42.666842
3506.918506	901221.672848	42.671847
3506.917618	901086.606273	42.676852
3507.061730	900965.801761	42.681856
3506.886401	900841.474908	42.686861
3506.949689	900719.616363	42.691866
3506.670811	900603.508282	42.696871
3506.735161	900483.961770	42.701876
3506.995868	900366.214985	42.706880
3506.854733	900252.490934	42.711885
3506.889442	900127.534328	42.716890
3506.827336	899998.631730	42.721895
3506.952683	899882.731872	42.726900
3506.749737	899766.594008	42.731904
3506.581911	899650.834247	42.736909
3506.429974	899529.951114	42.741914
3506.476939	899424.001759	42.746919
3506.563913	899304.812787	42.751924
3506.481256	899198.880556	42.756928
3506.227730	899077.038658	42.761933
3506.515729	898960.416973	42.766938
3506.316565	898852.276019	42.771943
3506.098949	898749.544879	42.776948
3506.512565	898641.588694	42.781952
3506.206432	898531.817219	42.786957
3506.517881	898408.418950	42.791962
3506.222995	898301.538914	42.796967
3506.134571	898197.810508	42.801972
3506.418041	898084.455745	42.806977
3506.061614	897985.211090	42.811981
3506.366486	897876.678614	42.816986
3506.157666	897765.523793	42.821991
3506.235377	897660.695523	42.826996
3506.385554	897546.385886	42.832001
3506.315508	897439.645722	42.837005
3506.345727	897329.988702	42.842010
3506.124225	897215.830234	42.847015
3505.971199	897112.285784	42.852020
3506.198102	897004.908813	42.857025
3506.122046	896920.671410	42.862029
3506.455449	896794.722271	42.867034
3506.131187	896692.164551	42.872039
3506.131379	896587.812298	42.877044
3506.110979	896477.084249	42.882049
3506.038884	896368.874861	42.887053
3506.392020	896257.791110	42.892058
3506.180944	896169.989519	42.897063
3506.104511	896052.015107	42.902068
3506.089286	895954.031478	42.907073
3506.093740	895845.509593	42.912077
3506.256046	895740.921782	42.917082
3506.006259	895634.660423	42.922087
3506.074704	895520.999889	42.927092
3506.142858	895417.581335	42.932097
3505.815884	895329.592548	42.937101
3505.481463	895217.925219	42.942106
3505.818542	895136.396013	42.947111
3505.711901	895029.229910	42.952116
3505.869322	894934.003092	42.957121
3505.728567	894834.087795	42.962125
3505.683909	894732.995051	42.967130
3505.752780	894640.580905	42.972135
3505.534781	894529.944102	42.977140
3505.655143	894435.971615	42.982145
3505.374639	894331.817477	42.987149
3505.524017	894238.320256	42.992154
3505.492985	894152.197758	42.997159
3505.406463	894052.453132	43.002164
3505.420829	893965.837004	43.007169
3505.220128	893865.914586	43.012173
3505.356005	893774.248700	43.017178
3505.366295	893682.698704	43.022183
3505.168826	893584.414255	43.027188
3505.460830	893499.292089	43.032193
3505.409727	893424.956359	43.037197
3505.031286	893319.543043	43.042202
3505.169339	893234.055568	43.047207
3505.224568	893143.359635	43.052212
3505.111927	893058.684291	43.057217
3504.939078	892970.150215	43.062221
3505.131813	892885.131932	43.067226
3505.427288	892796.711384	43.072231
3505.231797	892710.787588	43.077236
3505.262357	892619.894027	43.082241
3504.747536	892538.468022	43.087245
3505.099393	892459.702184	43.092250
3504.997950	892374.724772	43.097255
3505.077141	892280.723565	43.102260
3505.103110	892196.786179	43.107265
3505.115663	892117.491341	43.112269
3505.249888	892024.733951	43.117274
3505.146856	891944.778855	43.122279
3504.830537	891854.703894	43.127284
3505.150649	891777.964681	43.132289
3504.594914	891704.946870	43.137293
3504.737050	891611.311118	43.142298
3504.875942	891547.750933	43.147303
3504.951115	891451.996011	43.152308
3505.070303	891367.644264	43.157313
3504.749166	891287.812633	43.162317
3504.778338	891201.635718	43.167322
3504.914993	891121.532919	43.172327
3504.667932	891042.846263	43.177332
3504.765515	890956.267517	43.182337
3504.539179	890882.121026	43.187341
3504.780649	890806.252241	43.192346
3504.553345	890727.364554	43.197351
3504.516813	890666.241564	43.202356
3504.685416	890571.713952	43.207361
3504.469024	890502.107001	43.212365
3504.644882	890423.051980	43.217370
3504.566771	890339.975082	43.222375
3504.390483	890261.556229	43.227380
3504.375319	890194.524120	43.232385
3504.490522	890133.854118	43.237389
3504.585499	890056.451833	43.242394
3504.681431	889987.077381	43.247399
3504.494821	889914.169390	43.252404
3504.567377	889835.123295	43.257409
3504.207807	889763.209260	43.262413
3504.528136	889689.731207	43.267418
3504.783546	889596.334124	43.272423
3504.535524	889529.235873	43.277428
3504.664135	889452.497112	43.282433
3504.598077	889382.851822	43.287437
3504.838031	889299.804224	43.292442
3504.511207	889225.652886	43.297447
3504.483013	889154.837619	43.302452
3504.643983	889088.537585	43.307457
3504.436550	889018.427420	43.312461
3504.322638	888941.238038	43.317466
3504.636378	888875.781161	43.322471
3504.256723	888792.151039	43.327476
3504.410073	888719.752422	43.332481
3504.029556	888653.439830	43.337485
3504.418977	888570.357085	43.342490
3504.334534	888511.251005	43.347495
3503.930085	888438.069903	43.352500
3503.999497	888378.163019	43.357505
3504.032683	888314.003892	43.362509
3504.072688	888237.553824	43.367514
3503.962564	888193.834284	43.372519
3503.753534	888122.552284	43.377524
3504.118507	888062.786962	43.382529
3503.942149	887996.239629	43.387533
3504.131476	887928.470043	43.392538
3503.905468	887863.961530	43.397543
3503.741830	887799.054931	43.402548
3503.763672	887741.955662	43.407553
3503.564656	887676.085777	43.412557
3504.020988	887616.107232	43.417562
3504.035402	887555.233109	43.422567
3503.607162	887495.882928	43.427572
3503.549773	887431.728908	43.432577
3503.463918	887378.031018	43.437581
3503.566263	887317.236677	43.442586
3503.574683	887271.651792	43.447591
3503.498198	887211.272921	43.452596
3503.632225	887158.020669	43.457601
3503.557173	887111.480444	43.462605
3503.779640	887047.082477	43.467610
3503.593868	886988.267834	43.472615
3503.701673	886937.824656	43.477620
3503.924731	886869.262791	43.482625
3503.338087	886827.740730	43.487629
3503.665467	886764.483791	43.492634
3503.473947	886716.991681	43.497639
3503.594516	886653.090064	43.502644
3503.791883	886601.564494	43.507649
3503.624821	886546.420370	43.512653
3503.657390	886478.949983	43.517658
3503.312729	886424.317924	43.522663
3503.276206	886378.539808	43.527668
3503.617106	886327.472129	43.532673
3503.272031	886272.161123	43.537677
3503.566211	886228.166489	43.542682
3503.464916	886171.071982	43.547687
3503.317588	886123.277315	43.552692
3503.449464	886062.174512	43.557697
3503.264602	886008.189801	43.562701
3503.214766	885953.504720	43.567706
3503.482852	885914.739363	43.572711
3503.641968	885866.601679	43.577716
3503.619386	885800.681342	43.582721
3503.366893	885746.898947	43.587725
3503.347204	885686.397988	43.592730
3503.196125	885638.406320	43.597735
3503.271436	885590.473765	43.602740
3503.543676	885545.412664	43.607745
3503.274299	885496.955264	43.612749
3503.469571	885444.354827	43.617754
3503.077111	885403.661837	43.622759
3503.177752	885349.043069	43.627764
3503.474923	885295.940433	43.632769
3503.562800	885257.394000	43.637773
3503.041771	885199.778179	43.642778
3503.179708	885156.285231	43.647783
3503.382904	885102.131324	43.652788
3503.489881	885046.734129	43.657793
3503.451537	885004.043627	43.662797
3503.468949	884938.300529	43.667802
3503.304470	884889.046202	43.672807
3503.041919	884851.813477	43.677812
3503.718823	884796.126352	43.682817
3503.488551	884742.330969	43.687821
3503.359268	884695.296132	43.692826
3503.358084	884649.885830	43.697831
3503.302089	884600.611181	43.702836
3503.360065	884542.021998	43.707841
3503.272878	884497.205629	43.712845
3503.501167	884454.370328	43.717850
3503.595591	884401.002427	43.722855
3503.106974	884352.765238	43.727860
3503.529416	884292.176895	43.732865
3503.300024	884250.771126	43.737869
3503.521214	884202.028417	43.742874
3503.351518	884144.344222	43.747879
3503.287842	884094.291877	43.752884
3503.179947	884040.663496	43.757889
3503.307959	884006.653385	43.762893
3503.514559	883943.095067	43.767898
3503.239567	883905.761482	43.772903
3503.396106	883854.992936	43.777908
3503.410532	883784.298527	43.782913
3503.608724	883747.854362	43.787917
3503.532519	883694.895448	43.792922
3503.491833	883652.485918	43.797927
3503.064464	883600.649254	43.802932
3503.307992	883542.891009	43.807937
3503.030145	883498.776252	43.812941
3503.298355	883444.789879	43.817946
3503.173973	883408.299887	43.822951
3503.130832	883352.620737	43.827956
3503.452765	883311.989063	43.832961
3503.154119	883264.098916	43.837965
3503.142594	883208.219480	43.842970
3503.184687	883163.565226	43.847975
3503.056884	883114.289806	43.852980
3502.979563	883066.942675	43.857985
3503.390279	883028.037714	43.862989
3503.055366	882972.693554	43.867994
3503.125840	882930.454153	43.872999
3502.869098	882892.917348	43.878004
3502.759303	882835.307150	43.883009
3503.081301	882797.190106	43.888013
3503.183630	882757.656160	43.893018
3503.314156	882716.567590	43.898023
3502.973938	882671.875695	43.903028
3502.947284	882627.809806	43.908033
3502.666239	882582.332607	43.913037
3502.987001	882540.533441	43.918042
3502.977431	882502.275376	43.923047
3502.881576	882472.555048	43.928052
3503.275347	882425.996844	43.933057
3503.401269	882375.220444	43.938061
3503.186916	882325.080844	43.943066
3503.409739	882271.575401	43.948071
3503.306756	882229.456362	43.953076
3503.009852	882177.294924	43.958081
3503.149265	882133.197938	43.963085
3503.556114	882084.794393	43.968090
3503.434194	882039.674213	43.973095
3502.962175	881996.355003	43.978100
3503.133405	881947.504794	43.983105
3502.963803	881894.254284	43.988109
3502.973188	881863.544808	43.993114
3503.322552	881813.695422	43.998119
3503.268103	881775.149366	44.003124
3503.210969	881721.394387	44.008129
3503.002840	881677.835586	44.013133
3503.217373	881645.056805	44.018138
3502.990559	881589.294194	44.023143
3502.962886	881552.001637	44.028148
3502.811068	881497.291431	44.033153
3502.912726	881470.536648	44.038157
3503.139383	881424.288628	44.043162
3502.918196	881381.892310	44.048167
3502.989163	881343.807140	44.053172
3502.849845	881293.355670	44.058177
3503.152860	881256.878673	44.063181
3503.261814	881208.613834	44.068186
3503.242755	881150.100107	44.073191
3503.158858	881112.717126	44.078196
3503.099085	881057.406334	44.083201
3502.895811	881024.789794	44.088205
3502.913422	880986.517318	44.093210
3503.025503	880949.197889	44.098215
3502.950865	880909.874360	44.103220
3502.810380	880867.073462	44.108225
3502.860338	880836.642566	44.113229
3502.747821	880787.732525	44.118234
3502.927792	880758.636249	44.123239
3502.758959	880717.292265	44.128244
3502.908733	880667.950449	44.133249
3502.839324	880638.022641	44.138253
3502.932541	880581.907015	44.143258
3502.891248	880539.765626	44.148263
3503.101032	880520.061870	44.153268
3503.120601	880469.674007	44.158273
3502.984960	880425.415666	44.163277
3502.732378	880385.827245	44.168282
3503.017108	880329.677650	44.173287
3502.823222	880297.539988	44.178292
3502.784001	880252.586174	44.183297
3503.099261	880220.751800	44.188301
3503.053161	880178.705501	44.193306
3503.129129	880134.022497	44.198311
3503.022533	880088.884728	44.203316
3502.915590	880049.173134	44.208321
3502.627141	880003.483259	44.213325
3502.279760	879972.919533	44.218330
3502.583382	879942.054587	44.223335
3502.312132	879920.296203	44.228340
3502.789174	879875.642055	44.233345
3502.810173	879842.691260	44.238349
3502.882341	879808.665894	44.243354
3502.744337	879767.988460	44.248359
3502.529162	879732.168779	44.253364
3502.510141	879691.568118	44.258369
3502.430652	879654.368908	44.263373
3502.126484	879625.637493	44.268378
3502.367418	879598.269761	44.273383
3502.610605	879569.447894	44.278388
3502.493427	879527.602451	44.283393
3502.491797	879496.591634	44.288397
3502.491332	879456.955395	44.293402
3502.988173	879429.350893	44.298407
3502.358661	879393.015932	44.303412
3502.568664	879347.820293	44.308417
3502.689625	879332.003691	44.313421
3502.381730	879289.315751	44.318426
3502.682203	879263.874926	44.323431
3502.730011	879230.819363	44.328436
3502.818262	879172.752769	44.333441
3502.862294	879148.032101	44.338445
3502.716584	879108.902020	44.343450
3502.876576	879078.056198	44.348455
3502.482853	879038.966510	44.353460
3502.592020	878997.564583	44.358465
3502.822688	878975.623078	44.363469
3502.703714	878935.518246	44.368474
3502.906924	878898.655346	44.373479
3502.442417	878867.814387	44.378484
3502.385202	878829.540148	44.383489
3502.454229	878793.086378	44.388493
3502.650018	878767.466808	44.393498
3503.187652	878720.855457	44.398503
3502.525773	878690.433773	44.403508
3502.792505	878648.809583	44.408513
3502.631448	878616.269593	44.413517
3502.889533	878580.558756	44.418522
3502.683141	878544.827300	44.423527
3502.425737	878505.033111	44.428532
3502.634376	878473.012979	44.433537
3502.617594	878436.861919	44.438541
3502.619410	878407.492554	44.443546
3502.648983	878366.777795	44.448551
3502.370662	878335.806432	44.453556
3502.763776	878300.362437	44.458561
3502.689856	878268.775465	44.463565
3502.445510	878241.869092	44.468570
3502.802237	878202.747125	44.473575
3502.778008	878171.345307	44.478580
3502.235641	878133.340326	44.483585
3502.426900	878101.514901	44.488589
3502.657723	878077.049754	44.493594
3502.757756	878036.418033	44.498599
3502.203579	877996.378488	44.503604
3502.633568	877974.982024	44.508609
3502.414342	877941.381589	44.513613
3502.192223	877910.204851	44.518618
3502.480955	877877.392792	44.523623
3502.075058	877856.424421	44.528628
3502.496603	877818.743285	44.533633
3502.816278	877796.879661	44.538637
3502.385181	877756.915144	44.543642
3502.733091	877718.082228	44.548647
3502.487733	877699.898099	44.553652
3502.661532	877651.399428	44.558657
3502.661262	877616.694716	44.563661
3502.616886	877590.334061	44.568666
3503.057453	877549.642878	44.573671
3502.451287	877519.108991	44.578676
3502.698708	877478.643025	44.583681
3502.595316	877439.107075	44.588685
3502.524680	877410.714113	44.593690
3502.508163	877368.933651	44.598695
3502.574115	877329.950741	44.603700
3502.593275	877300.766886	44.608705
3502.652563	877273.515215	44.613709
3502.461546	877245.529077	44.618714
3502.666433	877207.104149	44.623719
3502.603011	877186.076962	44.628724
3502.641297	877144.576725	44.633729
3502.372155	877117.669290	44.638733
3502.399395	877084.411152	44.643738
3502.710305	877049.360980	44.648743
3502.422860	877017.511617	44.653748
3502.650705	876977.627145	44.658753
3502.661993	876945.340368	44.663757
3502.456555	876915.028178	44.668762
3502.709458	876874.751071	44.673767
3502.664785	876851.780531	44.678772
3502.532335	876807.591341	44.683777
3502.590276	876778.786331	44.688781
3502.340480	876751.970992	44.693786
3502.711977	876708.764547	44.698791
3502.567076	876687.361178	44.703796
3502.433086	876641.910564	44.708801
3502.341176	876611.772024	44.713805
3502.473503	876583.632511	44.718810
3502.542410	876556.182024	44.723815
3502.519768	876525.643797	44.728820
3502.423041	876479.604038	44.733825
3502.866340	876458.296851	44.738829
3502.611685	876427.408499	44.743834
3502.799792	876397.416652	44.748839
3502.379204	876368.979364	44.753844
3502.668817	876323.068657	44.758849
3502.499189	876284.893352	44.763853
3502.215420	876247.803206	44.768858
3502.506735	876231.659323	44.773863
3502.509646	876215.659875	44.778868
3502.459091	876175.137098	44.783873
3502.393370	876139.949650	44.788877
3502.609302	876107.333676	44.793882
3502.786012	876069.778682	44.798887
3502.718481	876031.778853	44.803892
3502.644315	875985.537587	44.808897
3502.223316	875968.831565	44.813901
3502.155524	875936.455328	44.818906
3502.669446	875902.237625	44.823911
3502.296049	875874.178051	44.828916
3502.604628	875841.351406	44.833921
3502.471602	875803.263926	44.838925
3502.393485	875783.591754	44.843930
3502.402375	875750.038204	44.848935
3502.145282	875724.480028	44.853940
3502.178654	875697.613239	44.858945
3502.443861	875664.501840	44.863949
3502.185847	875627.597498	44.868954
3502.456254	875594.775774	44.873959
3502.430914	875572.572866	44.878964
3502.241117	875545.354253	44.883969
3502.351472	875526.329000	44.888973
3502.472188	875499.446921	44.893978
3502.639287	875465.671741	44.898983
3502.202976	875436.553707	44.903988
3502.427351	875405.193172	44.908993
3502.646863	875372.378601	44.913997
3502.071728	875345.804422	44.919002
3502.302821	875313.084591	44.924007
3502.500698	875291.813645	44.929012
3502.093597	875263.853700	44.934017
3502.147589	875227.962237	44.939021
3502.394747	875207.167770	44.944026
3502.454232	875167.201836	44.949031
3502.242630	875154.726191	44.954036
3502.406406	875108.341879	44.959041
3502.143318	875088.600884	44.964045
3501.943035	875069.431375	44.969050
3502.569371	875036.741885	44.974055
3502.503818	875018.616835	44.979060
3502.401972	874979.355100	44.984065
3502.443636	874947.440336	44.989069
3502.060310	874917.438144	44.994074
3502.478672	874882.939344	44.999079
3502.290894	874866.385743	45.004084
3502.250018	874833.417111	45.009089
3502.245581	874805.679618	45.014093
3502.191014	874779.405072	45.019098
3502.255386	874747.388500	45.024103
3502.288539	874719.547422	45.029108
3502.021126	874704.073364	45.034113
3502.640279	874667.891417	45.039117
3502.122372	874645.766181	45.044122
3502.280015	874619.455963	45.049127
3502.043088	874605.819444	45.054132
3502.550748	874573.243946	45.059137
3502.385483	874534.668648	45.064141
3502.066015	874513.771118	45.069146
3502.647350	874481.958919	45.074151
3502.266088	874444.582532	45.079156
3502.515647	874421.457073	45.084161
3502.405444	874398.778773	45.089165
3502.448852	874384.804576	45.094170
3502.707095	874329.572110	45.099175
3502.149194	874315.114844	45.104180
3502.394878	874274.336244	45.109185
3502.621184	874247.237094	45.114189
3502.394905	874214.198564	45.119194
3502.611317	874178.564975	45.124199
3502.452668	874157.736689	45.129204
3502.648731	874126.471052	45.134209
3502.471954	874091.289712	45.139213
3502.236184	874060.870866	45.144218
3502.406650	874026.892930	45.149223
3502.363043	874007.209164	45.154228
3502.404438	873963.940074	45.159233
3502.348373	873942.221118	45.164237
3502.027081	873919.187752	45.169242
3502.451582	873883.227101	45.174247
3502.206511	873879.969514	45.179252
3502.273796	873835.046173	45.184257
3502.512711	873810.077024	45.189261
3502.558079	873783.005565	45.194266
3502.688356	873740.981259	45.199271
3502.327164	873720.572825	45.204276
3502.515292	873686.299014	45.209281
3502.637963	873663.967558	45.214285
3502.275152	873624.448817	45.219290
3502.559758	873592.001696	45.224295
3502.081379	873568.798832	45.229300
3502.413797	873530.232008	45.234305
3502.022428	873505.559436	45.239309
3501.747173	873490.859564	45.244314
3501.694864	873469.332275	45.249319
3501.772346	873433.135045	45.254324
3502.172664	873424.338318	45.259329
3502.133356	873399.122250	45.264333
3501.995427	873374.019332	45.269338
3502.211763	873348.954955	45.274343
3502.165294	873326.747108	45.279348
3502.174815	873305.306050	45.284353
3501.988786	873269.442272	45.289357
3501.920507	873261.983672	45.294362
3502.152775	873233.035671	45.299367
3502.083845	873199.771536	45.304372
3502.307760	873175.966359	45.309377
3502.225121	873156.286201	45.314381
3502.034511	873134.877499	45.319386
3501.943914	873105.691026	45.324391
3502.131436	873077.234715	45.329396
3502.331757	873053.238903	45.334401
3502.114442	873034.065607	45.339405
3502.066092	873020.588398	45.344410
3502.521541	872971.713909	45.349415
3502.155450	872966.244350	45.354420
3502.191443	872933.446525	45.359425
3501.829244	872904.109772	45.364429
3501.930718	872881.875888	45.369434
3502.243045	872847.285720	45.374439
3502.217529	872829.923535	45.379444
3502.452708	872794.278553	45.384449
3502.294384	872772.960246	45.389453
3502.073759	872745.733841	45.394458
3502.284294	872717.369039	45.399463
3501.708992	872705.433254	45.404468
3501.841981	872674.655478	45.409473
3502.333215	872658.468948	45.414477
3502.314919	872630.820591	45.419482
3502.435246	872596.357621	45.424487
3502.379421	872577.544339	45.429492
3501.941769	872552.099231	45.434497
3502.443459	872519.416447	45.439501
3502.090438	872501.331061	45.444506
3502.293627	872477.235429	45.449511
3502.167867	872446.110999	45.454516
3502.187227	872421.851377	45.459521
3502.184920	872385.660915	45.464525
3502.075829	872376.655493	45.469530
3502.123809	872330.268548	45.474535
3502.073599	872322.223623	45.479540
3501.957718	872297.694691	45.484545
3502.606803	872273.330717	45.489549
3501.947214	872253.839650	45.494554
3502.358483	872218.647356	45.499559
3501.864748	872197.479274	45.504564
3502.160888	872167.157145	45.509569
3502.346263	872139.667012	45.514573
3502.077351	872121.566611	45.519578
3502.290320	872095.721261	45.524583
3502.112590	872068.193588	45.529588
3501.574757	872047.517397	45.534593
3502.135692	872028.309668	45.539597
3502.056653	872001.541690	45.544602
3502.066713	871979.610596	45.549607
3502.044746	871966.999954	45.554612
3502.042289	871930.709716	45.559617
3502.094075	871914.496537	45.564621
3501.964989	871892.005837	45.569626
3502.132153	871859.762693	45.574631
3501.957329	871853.969482	45.579636
3501.871701	871822.155925	45.584641
3502.382243	871794.028409	45.589645
3501.841231	871778.494744	45.594650
3502.180530	871752.044870	45.599655
3501.971753	871735.291907	45.604660
3502.125199	871705.864281	45.609665
3502.084918	871692.576808	45.614669
3501.727308	871664.785789	45.619674
3502.024852	871641.156427	45.624679
3501.997671	871632.524539	45.629684
3501.881159	871609.933662	45.634689
3502.135142	871580.100693	45.639693
3502.233109	871565.140477	45.644698
3502.312059	871524.758657	45.649703
3502.130437	871514.890510	45.654708
3502.142711	871478.498049	45.659713
3502.083523	871456.285312	45.664717
3502.121831	871427.166406	45.669722
3502.247401	871408.610672	45.674727
3502.302290	871385.408447	45.679732
3502.128658	871354.286193	45.684737
3502.543075	871334.906291	45.689741
3502.151197	871313.621230	45.694746
3502.451629	871273.201217	45.699751
3502.206386	871249.950867	45.704756
3502.301264	871224.315289	45.709761
3502.337333	871202.182957	45.714765
3502.239524	871177.064153	45.719770
3502.160753	871134.861789	45.724775
3502.148716	871126.808959	45.729780
3501.993241	871085.492310	45.734785
3502.121309	871082.753986	45.739789
3501.952201	871050.658918	45.744794
3502.423251	871015.061484	45.749799
3502.258872	871006.839492	45.754804
3502.240177	870986.656372	45.759809
3502.467489	870954.107275	45.764813
3502.366026	870907.733877	45.769818
3502.393463	870808.833605	45.774823
3502.658492	870676.991051	45.779828
3502.224145	870465.867673	45.784833
3502.402706	870202.028175	45.789837
3502.209095	869895.043447	45.794842
3501.934202	869508.650494	45.799847
3501.819294	869080.461648	45.804852
3501.626229	868593.613809	45.809857
3501.709184	868033.566825	45.814861
3501.345680	867427.609463	45.819866
3500.840843	866748.290265	45.824871
3500.616076	866031.453266	45.829876
3500.490676	865223.200833	45.834881
3499.988591	864367.878509	45.839885
3499.896579	863446.971476	45.844890
3499.424372	862454.263123	45.849895
3499.029117	861410.639331	45.854900
3498.899369	860296.015520	45.859905
3498.785241	859102.517881	45.864909
3497.997166	857857.933752	45.869914
3498.100909	856533.957536	45.874919
3497.210101	855149.726485	45.879924
3496.519764	853682.618761	45.884929
3496.093523	852151.549359	45.889933
3495.648484	850555.544970	45.894938
3494.832418	848883.705983	45.899943
3494.487939	847163.796259	45.904948
3493.726127	845367.662070	45.909953
3493.360252	843493.351212	45.914957
3492.357956	841549.742779	45.919962
3492.074547	839533.869530	45.924967
3490.894801	837443.345916	45.929972
3490.640815	835301.276911	45.934977
3489.766826	833080.430903	45.939981
3488.856810	830797.923093	45.944986
3487.882066	828440.407823	45.949991
3487.326642	826029.037949	45.954996
3486.243819	823535.507339	45.960001
3485.537437	820975.671070	45.965005
3484.737508	818350.856423	45.970010
3483.979480	815660.970144	45.975015
3482.889912	812908.401362	45.980020
3481.748167	810077.846250	45.985025
3480.730035	807180.262527	45.990029
3479.808162	804232.592260	45.995034
3478.883056	801213.456300	46.000039
3477.632070	798133.571086	46.005044
3476.162473	794987.201113	46.010049
3475.376955	791769.844348	46.015053
3473.804926	788500.921776	46.020058
3472.963471	785153.572431	46.025063
3472.049712	781752.229772	46.030068
3470.565404	778284.706696	46.035073
3469.191438	774739.582839	46.040077
3467.741986	771168.516715	46.045082
3466.639927	767510.742996	46.050087
3465.377128	763784.429119	46.055092
3463.771619	760017.789179	46.060097
3462.525078	756164.856684	46.065101
3461.148297	752268.714227	46.070106
3459.907713	748304.120213	46.075111
3458.373678	744283.716109	46.080116
3456.830024	740187.901040	46.085121
3455.600756	736037.063730	46.090125
3453.759787	731818.667018	46.095130
3452.567539	727553.227424	46.100135
3450.615337	723216.689108	46.105140
3448.861319	718826.858575	46.110145
3447.558770	714374.406465	46.115149
3445.868569	709875.136326	46.120154
3444.425936	705300.931319	46.125159
3442.469905	700662.859337	46.130164
3440.463017	695981.905156	46.135169
3438.563634	691241.736244	46.140173
3436.751846	686440.849606	46.145178
3434.963070	681578.843191	46.150183
3432.973176	676673.480131	46.155188
3431.282488	671702.407229	46.160193
3429.308476	666673.833035	46.165197
3427.151628	661604.606442	46.170202
3425.168755	656462.932454	46.175207
3423.283470	651263.038043	46.180212
3421.279372	646026.353166	46.185217
3419.146899	640709.950024	46.190221
3417.136924	635365.148028	46.195226
3415.143324	629959.871358	46.200231
3412.935302	624506.081718	46.205236
3410.519765	618995.630305	46.210241
3408.459993	613435.204525	46.215245
3406.181274	607842.631477	46.220250
3403.832810	602188.624622	46.225255
3401.500776	596482.921204	46.230260
3399.313177	590725.374908	46.235265
3396.762610	584921.676204	46.240269
3394.599546	579066.508393	46.245274
3392.127814	573171.036785	46.250279
3389.572027	567229.031651	46.255284
3387.087444	561254.157603	46.260289
3384.814162	555199.194337	46.265293
3381.901803	549136.565986	46.270298
3379.077473	543014.311132	46.275303
3376.803288	536859.579501	46.280308
3373.630051	530661.980381	46.285313
3371.215363	524415.845998	46.290317
3368.276951	518144.981310	46.295322
3365.796560	511814.491239	46.300327
3363.043672	505466.754138	46.305332
3360.308371	499064.040418	46.310337
3357.327954	492626.786941	46.315341
3354.133798	486167.165408	46.320346
3351.350544	479659.245717	46.325351
3348.416532	473121.575200	46.330356
3345.343693	466558.600226	46.335361
3342.558070	459948.503506	46.340365
3339.044060	453314.749980	46.345370
3336.028749	446648.922146	46.350375
3332.553890	439958.071694	46.355380
3329.964545	433239.340428	46.360385
3326.448922	426486.632651	46.365389
3322.902544	419715.817724	46.370394
3319.966057	412917.076704	46.375399
3316.542923	406101.594713	46.380404
3312.716237	399268.382969	46.385409
3309.489872	392395.767858	46.390413
3305.787622	385522.335992	46.395418
3302.373735	378605.178206	46.400423
3299.092645	371684.602393	46.405428
3295.079751	364747.351825	46.410433
3291.637999	357802.544239	46.415437
3287.802683	350833.702434	46.420442
3283.922979	343858.703316	46.425447
3280.285466	336884.782591	46.430452
3276.144250	329883.106114	46.435457
3272.469658	322882.555747	46.440461
3268.548022	315885.981482	46.445466
3264.736279	308875.740311	46.450471
3260.924795	301850.505097	46.455476
3256.932350	294837.811909	46.460481
3252.988313	287805.266815	46.465485
3249.130877	280780.321970	46.470490
3245.120867	273745.300812	46.475495
3240.936076	266720.207172	46.480500
3236.702598	259691.327285	46.485505
3232.603755	252664.522452	46.490509
3228.222985	245645.931056	46.495514
3224.228330	238627.530415	46.500519
3220.077044	231615.377165	46.505524
3215.679651	224546.646265	46.510529
3211.293268	217524.694359	46.515533
3207.052418	210544.100884	46.520538
3202.547867	203560.021268	46.525543
3197.780953	196603.036502	46.530548
3193.231939	189653.122687	46.535553
3188.603612	182725.895508	46.540557
3183.740290	175828.133878	46.545562
3179.257416	168939.590499	46.550567
3174.460912	162085.603191	46.555572
3169.478684	155253.852659	46.560577
3164.714625	148436.011417	46.565581
3160.104481	141650.645633	46.570586
3155.188564	134898.436702	46.575591
3150.491924	128168.642086	46.580596
3145.103974	121484.113878	46.585601
3140.211402	114820.579939	46.590605
3134.665837	108196.423188	46.595610
3129.102086	101609.691824	46.600615
3123.813873	95068.110945	46.605620
3118.240803	88580.424365	46.610625
3112.942145	82137.102128	46.615629
3107.323046	75742.756430	46.620634
3101.437206	69396.249355	46.625639
3095.703381	63111.077886	46.630644
3089.402316	56890.447968	46.635649
3083.213430	50717.726135	46.640653
3076.071331	44646.496159	46.645658
3068.816261	38650.358070	46.650663
3060.908964	32753.490907	46.655668
3048.739335	27075.025955	46.660673
3021.461817	21953.557146	46.665677
2989.005756	17283.072146	46.670682
2956.730395	13050.604988	46.675687
2926.789518	9298.654845	46.680692
2899.694468	6053.000436	46.685697
2875.318648	3336.682435	46.690701
2852.424645	1163.264876	46.695706
2801.448085	317.449431	46.700711
2746.526899	308.362685	46.705716
2725.973166	310.362118	46.710721
2732.931432	303.224369	46.715725
2753.533608	306.881753	46.720730
2775.849839	297.672646	46.725735
2792.936684	296.946623	46.730740
2801.413483	293.875894	46.735745
2803.368679	289.876151	46.740749
2801.018840	301.377928	46.745754
2796.638080	302.390130	46.750759
2792.353238	293.096655	46.755764
2788.214564	289.858021	46.760769
2784.818743	286.239888	46.765773
2782.347203	288.053664	46.770778
2780.028087	292.993858	46.775783
2777.961817	287.652218	46.780788
2774.788787	281.216775	46.785793
2772.367121	275.008242	46.790797
2769.428666	272.262300	46.795802
2766.766116	282.720814	46.800807
2763.575072	267.511346	46.805812
2760.273777	277.602417	46.810817
2757.359321	270.256414	46.815821
2754.366985	277.449648	46.820826
2751.191403	275.149762	46.825831
2747.983750	264.243146	46.830836
2744.569195	279.706419	46.835841
2741.079171	269.581298	46.840845
2738.143336	275.275676	46.845850
2735.087664	270.178618	46.850855
2731.957603	261.371172	46.855860
2728.474855	271.235256	46.860865
2725.279697	263.879548	46.865869
2721.710595	274.650269	46.870874
2718.307307	267.908699	46.875879
2715.395035	257.250176	46.880884
2711.612168	265.776076	46.885889
2708.791208	266.658462	46.890893
2705.388588	258.769447	46.895898
2701.615878	268.913070	46.900903
2698.505891	260.696731	46.905908
2694.779909	266.593736	46.910913
2691.618417	261.802685	46.915917
2688.223503	266.059223	46.920922
2685.198062	261.949844	46.925927
2681.794017	257.830715	46.930932
2677.845100	262.996855	46.935937
2674.672888	263.844864	46.940941
2671.285677	253.805462	46.945946
2667.897886	266.713107	46.950951
2664.625043	257.441442	46.955956
2661.319228	265.450556	46.960961
2658.007376	263.068233	46.965965
2654.455606	263.183598	46.970970
2650.526394	261.244951	46.975975
2647.486054	256.938347	46.980980
2644.198186	258.152386	46.985985
2640.593361	249.445459	46.990989
2637.346793	253.211030	46.995994
2633.702691	252.236925	47.000999
2630.435811	253.632617	47.006004
2627.026460	249.224707	47.011009
2623.561703	246.726347	47.016013
2620.327795	243.506302	47.021018
2616.319492	251.315219	47.026023
2612.584555	245.161292	47.031028
2609.436849	253.653875	47.036033
2606.082854	239.718653	47.041037
2602.200205	247.461849	47.046042
2598.739487	253.472617	47.051047
2595.975699	245.977149	47.056052
2592.218076	252.507776	47.061057
2589.054174	244.545519	47.066061
2585.808610	242.286109	47.071066
2581.903291	239.772866	47.076071
2578.606214	240.443803	47.081076
2575.066133	240.901459	47.086081
2571.762152	238.918900	47.091085
2567.962143	244.660459	47.096090
2564.483929	246.026736	47.101095
2561.333413	244.907289	47.106100
2557.629166	241.063162	47.111105
2554.205571	240.683824	47.116109
2550.978328	238.151056	47.121114
2547.196784	234.618866	47.126119
2543.917292	241.004306	47.131124
2540.252739	240.747629	47.136129
2536.670163	238.436912	47.141133
2533.515342	240.406590	47.146138
2529.421352	239.810719	47.151143
2526.521297	239.907814	47.156148
2522.684711	246.606234	47.161153
2519.257119	236.061329	47.166157
2516.360127	234.994004	47.171162
2512.366237	236.196774	47.176167
2509.561082	224.736898	47.181172
2505.741336	230.831443	47.186177
2502.060420	225.532659	47.191181
2498.825311	219.005854	47.196186
2495.060627	241.903627	47.201191
2492.150609	231.074402	47.206196
2488.551079	232.984102	47.211201
2484.464400	231.775304	47.216205
2480.883902	221.678382	47.221210
2477.414864	233.031834	47.226215
2474.203443	223.010560	47.231220
2470.857980	234.211796	47.236225
2467.504188	227.013115	47.241229
2463.970024	220.515960	47.246234
2460.026040	233.971746	47.251239
2456.902517	223.102013	47.256244
2453.043683	238.023811	47.261249
2450.035333	231.275686	47.266253
2446.770399	226.494389	47.271258
2443.242655	239.532587	47.276263
2439.736870	217.372917	47.281268
2435.862759	221.304150	47.286273
2432.476050	226.287675	47.291277
2428.983387	226.101774	47.296282
2425.393968	234.276225	47.301287
2421.911717	227.665151	47.306292
2418.260839	233.431926	47.311297
2414.852945	233.412412	47.316301
2411.370709	227.640045	47.321306
2408.166491	230.116042	47.326311
2404.730523	223.346180	47.331316
2401.148399	227.564723	47.336321
2397.425570	220.350247	47.341325
2394.529995	216.726801	47.346330
2390.257866	225.150720	47.351335
2387.346320	215.122841	47.356340
2383.523679	218.574366	47.361345
2379.778656	208.591130	47.366349
2376.473687	213.600465	47.371354
2373.129239	215.114503	47.376359
2369.744618	213.619213	47.381364
2366.127182	221.904096	47.386369
2362.678047	214.144608	47.391373
2359.071116	218.215517	47.396378
2355.362996	220.499831	47.401383
2352.351823	217.967054	47.406388
2348.576724	213.366548	47.411393
2345.355797	219.057459	47.416397
2341.823025	218.700042	47.421402
2337.892352	218.441663	47.426407
2334.803829	219.221800	47.431412
2331.037151	224.011965	47.436417
2327.460929	220.033617	47.441421
2324.307279	214.109986	47.446426
2320.704378	229.946121	47.451431
2317.507693	217.598452	47.456436
2314.080442	221.746294	47.461441
2309.968827	214.351769	47.466445
2306.739151	213.577682	47.471450
2303.136943	212.038239	47.476455
2299.834020	216.957889	47.481460
2296.123165	216.497883	47.486465
2292.453309	222.256822	47.491469
2289.022730	207.616608	47.496474
2285.506611	216.250091	47.501479
2282.404794	205.295417	47.506484
2278.647435	211.072754	47.511489
2275.373719	208.082916	47.516493
2272.429475	209.998451	47.521498
2268.324241	212.852593	47.526503
2265.205597	206.300618	47.531508
2261.365885	212.028020	47.536513
2257.764654	204.177891	47.541517
2254.265610	211.941063	47.546522
2250.648703	215.102966	47.551527
2247.289197	204.309859	47.556532
2243.586739	211.233191	47.561537
2240.173972	208.589579	47.566541
2236.851629	202.539545	47.571546
2233.270915	206.474387	47.576551
2230.155690	216.825281	47.581556
2226.400676	203.240589	47.586561
2222.374467	214.751288	47.591565
2219.097759	213.579095	47.596570
2215.393359	209.401767	47.601575
2212.171569	207.323008	47.606580
2208.715939	207.875124	47.611585
2205.398054	204.453348	47.616589
2202.386128	202.707394	47.621594
2198.876133	213.180119	47.626599
2195.204346	203.313227	47.631604
2191.594467	204.028962	47.636609
2187.421137	211.146311	47.641613
2184.179556	204.517009	47.646618
2180.527244	214.600407	47.651623
2177.706319	197.788352	47.656628
2174.152147	207.509016	47.661633
2170.247154	211.041785	47.666637
2166.616404	203.104053	47.671642
2163.055036	208.961200	47.676647
2159.832442	200.774924	47.681652
2156.264884	208.079404	47.686657
2152.821121	198.690750	47.691661
2149.641785	201.170493	47.696666
2145.884117	202.883156	47.701671
2142.385854	201.917707	47.706676
2139.016529	200.872163	47.711681
2135.075390	199.068924	47.716685
2131.985716	200.718266	47.721690
2128.446651	210.458568	47.726695
2125.036784	197.110429	47.731700
2121.176094	197.663579	47.736705
2117.429835	202.244102	47.741709
2114.087511	190.607013	47.746714
2110.716827	207.840353	47.751719
2107.565333	198.898601	47.756724
2103.760391	193.397241	47.761729
2100.156463	203.464998	47.766733
2096.894798	194.397588	47.771738
2093.397466	195.843124	47.776743
2089.886212	192.973554	47.781748
2086.338195	201.400676	47.786753
2082.845091	194.841404	47.791757
2079.775149	201.135669	47.796762
2076.209181	199.621595	47.801767
2072.696088	190.370955	47.806772
2068.621615	198.178741	47.811777
2064.625896	204.172998	47.816781
2061.671820	193.848679	47.821786
2058.113527	203.787563	47.826791
2054.873314	187.506629	47.831796
2052.082033	190.311307	47.836801
2048.309137	202.077088	47.841805
2044.396227	199.376891	47.846810
2040.881616	203.362322	47.851815
2037.281969	194.361626	47.856820
2033.647408	199.206156	47.861825
2030.235772	194.616938	47.866829
2026.820685	199.552908	47.871834
2023.020264	205.388844	47.876839
2020.286775	190.537261	47.881844
2016.435396	197.534475	47.886849
2012.879268	200.535344	47.891853
2009.300618	194.406252	47.896858
2005.476073	202.953688	47.901863
2002.197557	191.761811	47.906868
1998.901710	198.675187	47.911873
1995.530815	194.517164	47.916877
1992.010048	182.849857	47.921882
1988.304577	195.737267	47.926887
1984.674062	193.442787	47.931892
1981.319394	193.251785	47.936897
1977.716957	197.041398	47.941901
1974.340257	186.246826	47.946906
1971.196738	195.543198	47.951911
1967.708407	193.929752	47.956916
1963.973813	198.738163	47.961921
1960.343089	196.979711	47.966925
1957.174028	201.526592	47.971930
1953.180262	202.727620	47.976935
1949.826092	196.507823	47.981940
1946.049262	186.665809	47.986945
1942.619605	192.966081	47.991949
1939.398976	188.357227	47.996954
1935.889077	197.976791	48.001959
1932.343298	185.379851	48.006964
1928.927080	196.199558	48.011969
1925.509845	196.275076	48.016973
1921.915048	186.846835	48.021978
1918.659506	188.147575	48.026983
1914.856242	183.846322	48.031988
1911.237402	190.019593	48.036993
1907.772435	187.273353	48.041997
1904.326942	188.800843	48.047002
1900.975884	196.879807	48.052007
1897.305693	188.633475	48.057012
1893.687146	186.524168	48.062017
1890.174375	196.884653	48.067021
1887.222500	192.644477	48.072026
1883.499057	196.509399	48.077031
1879.580220	185.332612	48.082036
1875.970812	187.489870	48.087041
1872.027934	198.911264	48.092045
1869.594101	187.543074	48.097050
1866.159122	194.409061	48.102055
1862.736543	184.401257	48.107060
1859.382917	192.056192	48.112065
1855.711267	198.218098	48.117069
1852.068390	185.595037	48.122074
1848.013070	191.228302	48.127079
1844.858269	191.878399	48.132084
1841.105874	190.829051	48.137089
1837.513140	189.807404	48.142093
1834.578595	184.045087	48.147098
1830.765691	195.106404	48.152103
1827.383712	189.084494	48.157108
1824.155946	195.872471	48.162113
1820.243287	195.237779	48.167117
1816.859682	185.383222	48.172122
1813.295105	186.490774	48.177127
1809.927701	188.556205	48.182132
1806.189788	195.121205	48.187137
1802.060643	198.851524	48.192141
1798.816388	187.019708	48.197146
1795.651925	195.083700	48.202151
1792.605165	194.834863	48.207156
1789.185729	197.985392	48.212161
1785.165755	198.447904	48.217165
1782.212326	186.085170	48.222170
1778.078079	189.373915	48.227175
1774.661920	187.121548	48.232180
1771.194618	192.825278	48.237185
1767.546328	190.070355	48.242189
1764.469873	189.792303	48.247194
1760.760231	188.900340	48.252199
1757.580174	185.207874	48.257204
1753.977115	186.561792	48.262209
1750.433993	187.654203	48.267213
1746.829888	184.712025	48.272218
1742.782419	189.446380	48.277223
1739.805994	188.351410	48.282228
1736.318650	182.369083	48.287233
1732.778466	194.031895	48.292237
1729.140328	182.422490	48.297242
1725.988040	180.818439	48.302247
1722.221816	184.760404	48.307252
1718.848952	181.814186	48.312257
1714.888255	184.684765	48.317261
1711.759320	185.991960	48.322266
1708.081346	185.372267	48.327271
1704.727544	185.843193	48.332276
1701.365585	189.448032	48.337281
1697.709739	180.426331	48.342285
1694.374424	174.917205	48.347290
1690.451145	186.980780	48.352295
1687.048570	184.495940	48.357300
1683.725529	187.348222	48.362305
1680.144689	186.885372	48.367309
1677.025402	181.070605	48.372314
1673.472880	192.755621	48.377319
1669.808320	186.129106	48.382324
1665.920575	187.257007	48.387329
1662.290905	176.354517	48.392333
1659.170040	182.487917	48.397338
1655.486455	187.681026	48.402343
1652.250283	182.320327	48.407348
1648.901588	175.276767	48.412353
1645.434496	178.060519	48.417357
1641.985287	181.070035	48.422362
1638.382140	181.030248	48.427367
1634.837531	183.194344	48.432372
1631.390593	182.239149	48.437377
1627.706464	176.908675	48.442381
1624.208495	169.669176	48.447386
1620.368530	187.978230	48.452391
1617.276325	175.442602	48.457396
1613.702226	178.176962	48.462401
1609.989931	172.600734	48.467405
1606.677425	168.391925	48.472410
1602.990422	176.520456	48.477415
1599.483484	173.309157	48.482420
1596.316651	175.047362	48.487425
1592.590268	179.704905	48.492429
1589.216864	180.681576	48.497434
1585.433183	172.597741	48.502439
1581.959580	176.032647	48.507444
1578.727395	177.155703	48.512449
1574.870620	184.855866	48.517453
1571.681119	170.717584	48.522458
1567.839899	179.301624	48.527463
1564.781449	176.112941	48.532468
1561.220181	177.333407	48.537473
1557.640780	181.628055	48.542477
1554.274031	170.966388	48.547482
1550.609546	176.190159	48.552487
1546.925863	176.858581	48.557492
1543.555142	180.334730	48.562497
1540.315938	172.372313	48.567501
1536.965103	176.092642	48.572506
1533.289891	171.196303	48.577511
1529.556249	174.464051	48.582516
1526.311283	182.945056	48.587521
1522.355585	183.757313	48.592525
1518.737892	165.786083	48.597530
1515.378704	178.172551	48.602535
1512.253893	177.940939	48.607540
1508.569875	171.714040	48.612545
1505.169734	178.456491	48.617549
1501.906409	173.952504	48.622554
1498.220391	173.049548	48.627559
1494.414910	182.462085	48.632564
1491.107264	175.496920	48.637569
1487.483478	173.588904	48.642573
1484.022116	171.108015	48.647578
1480.402725	178.228308	48.652583
1477.060616	168.955057	48.657588
1473.408528	172.927288	48.662593
1469.877779	174.219148	48.667597
1466.353141	166.074064	48.672602
1463.211351	173.716138	48.677607
1459.539746	169.816219	48.682612
1456.185779	167.250311	48.687617
1452.445132	171.211144	48.692621
1449.144053	166.135828	48.697626
1445.147175	168.693705	48.702631
1442.026332	168.679939	48.707636
1438.592443	169.275393	48.712641
1435.293803	167.615810	48.717645
1431.929973	172.096729	48.722650
1428.529164	167.088035	48.727655
1424.463615	174.977917	48.732660
1421.321371	168.741477	48.737665
1417.011581	177.487134	48.742669
1414.134296	167.433011	48.747674
1410.201005	176.030606	48.752679
1406.894822	176.477890	48.757684
1403.539255	167.830909	48.762689
1400.096174	171.905012	48.767693
1396.808498	170.890125	48.772698
1392.724515	167.399814	48.777703
1389.025141	167.640164	48.782708
1385.988722	165.734612	48.787713
1382.312021	172.501737	48.792717
1379.240984	169.662777	48.797722
1375.390426	172.444386	48.802727
1371.955411	180.250621	48.807732
1368.664230	175.257794	48.812737
1364.747786	174.810007	48.817741
1361.567049	179.597176	48.822746
1357.924428	172.280965	48.827751
1354.549916	173.231150	48.832756
1351.129901	175.016496	48.837761
1347.188352	180.573931	48.842765
1343.929977	182.121019	48.847770
1340.318499	171.399537	48.852775
1336.688409	168.779111	48.857780
1333.421203	171.997738	48.862785
1329.864849	176.140935	48.867789
1326.929635	179.164188	48.872794
1323.354300	173.616878	48.877799
1319.261827	170.141456	48.882804
1315.802567	175.246228	48.887809
1311.890785	178.737968	48.892813
1309.152479	180.919992	48.897818
1305.612568	174.401659	48.902823
1301.521995	167.695515	48.907828
1298.640102	171.693899	48.912833
1295.119822	176.156371	48.917837
1291.411977	172.549908	48.922842
1287.844083	180.225424	48.927847
1284.797390	169.188828	48.932852
1281.183000	161.787904	48.937857
1277.207683	165.697280	48.942861
1274.035300	165.565063	48.947866
1270.012614	164.701170	48.952871
1266.588109	166.956588	48.957876
1263.379449	167.265703	48.962881
1260.032042	177.886173	48.967885
1256.535649	165.571778	48.972890
1252.630771	166.597277	48.977895
1249.087169	165.753665	48.982900
1246.155878	158.961123	48.987905
1241.946400	173.361440	48.992909
1238.964440	170.287822	48.997914
1235.343764	161.662311	49.002919
1232.092824	170.712022	49.007924
1228.831774	167.005507	49.012929
1225.233759	165.555808	49.017933
1221.509151	157.757959	49.022938
1217.644489	166.031966	49.027943
1214.017058	170.227648	49.032948
1210.517382	155.563748	49.037953
1206.846039	164.479120	49.042957
1203.473086	156.269722	49.047962
1200.242813	168.351682	49.052967
1196.529393	170.942238	49.057972
1193.504629	160.819321	49.062977
1189.730662	163.486197	49.067981
1186.550987	162.270677	49.072986
1183.334158	158.708641	49.077991
1179.282982	164.603622	49.082996
1176.038429	170.184692	49.088001
1171.990655	172.140848	49.093005
1168.864208	159.854573	49.098010
1165.360911	164.087390	49.103015
1161.601656	159.763337	49.108020
1158.146679	167.736405	49.113025
1154.381474	167.508889	49.118029
1151.159443	166.273954	49.123034
1147.841112	164.489372	49.128039
1144.156644	159.611475	49.133044
1141.207309	159.525948	49.138049
1137.199116	167.934453	49.143053
1133.363784	161.954708	49.148058
1130.061264	164.464357	49.153063
1126.537376	164.618085	49.158068
1123.424065	162.271155	49.163073
1119.849042	162.417162	49.168077
1116.581945	150.475457	49.173082
1113.294635	160.566284	49.178087
1109.324012	166.717569	49.183092
1105.856904	161.876387	49.188097
1102.001871	164.740261	49.193101
1098.723185	167.719207	49.198106
1095.319369	164.024756	49.203111
1091.798852	159.954535	49.208116
1088.279744	164.788350	49.213121
1084.766550	168.245946	49.218125
1080.964412	167.877581	49.223130
1077.299980	159.099998	49.228135
1074.671875	158.703876	49.233140
1071.091265	155.454469	49.238145
1067.435072	154.843730	49.243149
1063.753323	169.512722	49.248154
1060.277570	156.447585	49.253159
1056.346428	158.996104	49.258164
1053.232694	154.971927	49.263169
1049.712398	163.084926	49.268173
1046.117346	162.705832	49.273178
1042.102635	158.589493	49.278183
1038.929564	157.393116	49.283188
1035.959700	155.769650	49.288193
1032.078452	160.218785	49.293197
1028.745876	159.273163	49.298202
1025.277642	155.308413	49.303207
1021.515881	158.786435	49.308212
1018.370213	159.949644	49.313217
1014.734744	162.135541	49.318221
1011.171526	153.175325	49.323226
1007.880397	154.320758	49.328231
1004.074694	160.965826	49.333236
1000.966703	158.311047	49.338241
997.053128	161.066680	49.343245
993.579125	153.281670	49.348250
990.137365	160.635392	49.353255
986.476187	156.283831	49.358260
983.111417	153.666989	49.363265
979.070146	159.333757	49.368269
976.191604	155.698769	49.373274
972.516265	154.600101	49.378279
968.922256	160.799530	49.383284
965.943301	152.873478	49.388289
962.340487	161.126084	49.393293
958.500481	159.040739	49.398298
955.119048	155.802299	49.403303
951.059005	158.261913	49.408308
947.968023	153.501536	49.413313
944.464876	153.900227	49.418317
940.716442	152.319541	49.423322
937.759895	153.662680	49.428327
933.875861	150.008113	49.433332
930.861204	157.308805	49.438337
927.165522	166.049616	49.443341
923.500213	155.235208	49.448346
920.113113	161.922017	49.453351
916.921290	160.722514	49.458356
913.126018	151.152906	49.463361
909.318503	159.773888	49.468365
905.924759	152.841794	49.473370
902.972667	159.562247	49.478375
899.010095	163.779256	49.483380
895.700549	147.161164	49.488385
891.654074	161.650819	49.493389
888.191745	153.619271	49.498394
884.889334	155.411557	49.503399
881.239943	157.551316	49.508404
878.308283	147.432004	49.513409
874.671776	158.606489	49.518413
871.149470	153.457512	49.523418
867.568644	155.976669	49.528423
863.774016	158.124677	49.533428
860.475081	157.913434	49.538433
856.873920	160.093387	49.543437
853.816981	146.887545	49.548442
850.343670	155.983342	49.553447
846.327612	162.737523	49.558452
843.308030	160.975986	49.563457
839.474962	164.992445	49.568461
835.865617	149.231100	49.573466
832.538449	152.284948	49.578471
828.547937	160.931721	49.583476
825.027291	156.435496	49.588481
821.603745	157.945148	49.593485
818.670129	152.940584	49.598490
815.199844	157.536427	49.603495
811.690617	155.572921	49.608500
808.384056	147.363337	49.613505
804.301013	151.418406	49.618509
800.718325	149.347474	49.623514
797.535100	150.925139	49.628519
794.249585	154.899609	49.633524
790.295533	151.681028	49.638529
786.628637	156.748685	49.643533
783.545999	151.750049	49.648538
779.886165	148.740337	49.653543
776.090624	160.115446	49.658548
773.098074	147.639822	49.663553
769.133369	152.135536	49.668557
766.018281	153.592629	49.673562
762.880402	152.584613	49.678567
759.046939	165.316189	49.683572
755.398545	147.190776	49.688577
751.674197	150.850887	49.693581
748.090291	149.046211	49.698586
744.844078	142.701793	49.703591
741.419975	152.240832	49.708596
738.237234	151.986977	49.713601
734.302146	152.604497	49.718605
730.834278	144.672084	49.723610
727.170411	154.736441	49.728615
723.702600	152.227623	49.733620
720.282067	147.834909	49.738625
716.628485	149.872878	49.743629
713.521799	153.332768	49.748634
710.378252	142.442519	49.753639
706.521105	145.780676	49.758644
702.785250	149.515744	49.763649
699.310530	149.063351	49.768653
695.977311	147.238757	49.773658
692.337115	145.325826	49.778663
688.511313	148.304398	49.783668
685.458187	150.947944	49.788673
681.687105	153.870898	49.793677
678.058965	150.025835	49.798682
674.738051	152.151872	49.803687
671.430260	143.792633	49.808692
667.924735	144.276198	49.813697
664.348559	149.562388	49.818701
660.582607	147.006449	49.823706
657.547269	147.662260	49.828711
653.822171	152.566781	49.833716
650.636761	141.128993	49.838721
646.947254	161.467832	49.843725
643.390886	152.470701	49.848730
639.856769	150.933359	49.853735
636.335306	152.465666	49.858740
632.703018	146.070756	49.863745
628.939808	152.586144	49.868749
625.632038	154.978421	49.873754
622.405901	149.414993	49.878759
618.755391	163.051579	49.883764
615.640629	146.742518	49.888769
611.921808	150.068921	49.893773
608.087852	152.836575	49.898778
604.770869	148.779266	49.903783
600.982894	147.386967	49.908788
597.888480	144.189340	49.913793
594.168282	147.931970	49.918797
590.619879	147.263536	49.923802
587.716649	146.834684	49.928807
583.690094	144.299435	49.933812
580.389505	138.235684	49.938817
576.476713	151.992647	49.943821
573.183083	147.136629	49.948826
569.848573	148.037759	49.953831
566.153312	147.291818	49.958836
562.865136	137.835989	49.963841
558.886272	144.879465	49.968845
555.507065	146.743897	49.973850
552.134543	138.577811	49.978855
548.884692	144.240878	49.983860
545.285047	139.892551	49.988865
541.503871	146.995291	49.993869
538.168848	150.395990	49.998874
534.937430	140.068037	50.003879
530.948981	150.901388	50.008884
527.633824	133.165882	50.013889
524.320401	145.758680	50.018893
520.548274	147.216126	50.023898
517.166956	138.982458	50.028903
513.571497	139.869581	50.033908
510.507696	134.002327	50.038913
506.926112	137.315182	50.043917
503.265323	145.350375	50.048922
499.587617	134.578693	50.053927
496.060190	141.919301	50.058932
492.545530	140.763075	50.063937
488.880079	146.225197	50.068941
485.807836	145.157780	50.073946
482.218523	131.467886	50.078951
478.521291	142.947311	50.083956
475.364201	135.626552	50.088961
471.653376	141.001868	50.093965
467.697653	140.987026	50.098970
464.430858	138.985466	50.103975
461.180048	140.578894	50.108980
457.877380	132.710164	50.113985
454.498033	137.128419	50.118989
450.369319	137.849276	50.123994
447.155496	135.232747	50.128999
443.491909	139.966425	50.134004
440.213783	127.308453	50.139009
436.615746	139.167938	50.144013
433.276130	138.488171	50.149018
429.537797	132.599603	50.154023
425.928539	138.888585	50.159028
422.368657	131.034233	50.164033
418.770168	141.576985	50.169037
415.475457	135.056750	50.174042
412.379597	133.305384	50.179047
408.670802	135.249730	50.184052
405.615075	139.190389	50.189057
402.026669	135.946001	50.194061
397.732431	135.321436	50.199066
394.430113	132.607704	50.204071
390.708555	141.019293	50.209076
387.332441	136.442300	50.214081
384.012425	148.673774	50.219085
380.419812	133.265531	50.224090
376.930072	130.108043	50.229095
373.542646	138.276086	50.234100
370.065035	130.884337	50.239105
366.553702	129.212422	50.244109
363.162840	139.371566	50.249114
359.461796	135.019464	50.254119
356.335668	139.337669	50.259124
352.696136	127.838552	50.264129
349.095310	138.037586	50.269133
345.512506	140.258321	50.274138
341.811588	138.211884	50.279143
338.188869	144.457578	50.284148
334.847183	132.511745	50.289153
331.463890	137.751265	50.294157
327.875324	139.652889	50.299162
324.817673	134.268628	50.304167
320.950326	136.420445	50.309172
317.443409	136.460910	50.314177
314.198118	138.210020	50.319181
310.246704	140.341029	50.324186
307.029622	133.336207	50.329191
303.759450	142.826381	50.334196
300.059831	141.773942	50.339201
296.542636	139.623727	50.344205
292.865958	134.784378	50.349210
289.355353	134.237613	50.354215
285.822754	146.476314	50.359220
282.266233	141.125323	50.364225
278.754736	136.977143	50.369229
275.080726	133.314673	50.374234
271.570492	132.117642	50.379239
268.543680	134.828350	50.384244
264.933682	129.899648	50.389249
261.519497	140.177374	50.394253
257.928298	134.837673	50.399258
254.816951	141.483243	50.404263
251.050050	143.948440	50.409268
247.643760	132.118560	50.414273
243.693807	133.397292	50.419277
240.724991	141.478179	50.424282
236.828077	125.046758	50.429287
233.298947	131.583696	50.434292
230.015847	131.264935	50.439297
226.386649	127.055182	50.444301
222.965059	128.592202	50.449306
219.234241	138.091194	50.454311
215.848192	132.077415	50.459316
212.247736	124.455529	50.464321
208.954953	127.899005	50.469325
205.154215	134.202093	50.474330
202.217836	117.345702	50.479335
198.612472	127.356346	50.484340
195.010714	126.258595	50.489345
191.246512	130.788508	50.494349
187.460634	128.450208	50.499354
184.387801	119.793401	50.504359
181.044335	137.332655	50.509364
177.704386	130.284345	50.514369
173.647333	133.274798	50.519373
170.126673	137.430718	50.524378
166.677426	128.350396	50.529383
163.145822	137.788035	50.534388
159.752193	136.945546	50.539393
156.322883	127.727548	50.544397
152.900089	130.654851	50.549402
149.639584	128.509429	50.554407
145.660943	128.861578	50.559412
142.033697	133.847792	50.564417
138.878882	133.735587	50.569421
135.121234	129.087983	50.574426
131.870402	125.916804	50.579431
128.447493	132.318625	50.584436
124.718706	123.633316	50.589441
121.268786	131.679665	50.594445
117.589402	134.572319	50.599450
114.183175	126.207368	50.604455
110.670255	126.090734	50.609460
107.293986	123.714489	50.614465
103.808738	127.138206	50.619469
100.359285	133.358750	50.624474
97.230630	135.551460	50.629479
93.211675	143.037685	50.634484
90.057105	137.847647	50.639489
86.135417	127.563139	50.644493
82.201291	131.305100	50.649498
79.243024	120.934302	50.654503
75.896980	133.502190	50.659508
72.134748	127.834984	50.664513
68.882310	127.481671	50.669517
65.210928	133.394440	50.674522
61.979262	122.550128	50.679527
58.002311	126.801615	50.684532
54.904090	130.102483	50.689537
51.530138	130.209360	50.694541
47.653896	129.623683	50.699546
44.004979	120.734013	50.704551
40.315809	133.312956	50.709556
37.132334	131.369963	50.714561
33.488444	121.600342	50.719565
30.136620	129.422522	50.724570
27.004666	119.073424	50.729575
23.261498	131.556140	50.734580
19.862345	122.533374	50.739585
15.939902	124.960984	50.744589
12.638492	132.996043	50.749594
8.908460	126.693081	50.754599
5.552365	131.174714	50.759604
2.289578	121.906395	50.764609