Tue Jun 21 12:42:42 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
-0.171651	99.240378	0.000000
-0.155111	107.398517	0.005005
-0.072833	106.720767	0.010010
0.060450	100.036977	0.015014
-0.251354	94.949921	0.020019
-0.166398	87.337984	0.025024
-0.227797	84.782905	0.030029
-0.758344	67.545103	0.035034
-1.074307	55.656638	0.040038
-1.320568	53.858958	0.045043
-1.565440	40.687507	0.050048
-2.034431	33.422872	0.055053
-2.684686	35.211145	0.060058
-2.373454	16.505756	0.065062
-2.958786	23.479466	0.070067
-3.216827	6.294288	0.075072
-3.275586	8.050522	0.080077
-3.798322	6.478004	0.085082
-4.075837	-4.208902	0.090086
-4.455708	10.750013	0.095091
-4.476534	-5.016927	0.100096
-4.787302	-6.868841	0.105101
-5.064216	7.423401	0.110106
-5.586481	-8.915648	0.115110
-5.875108	-6.277950	0.120115
-6.306638	-4.765463	0.125120
-6.276588	-8.131317	0.130125
-6.507233	5.093187	0.135130
-6.267037	-7.623968	0.140134
-6.834361	-6.821101	0.145139
-7.468273	-4.518920	0.150144
-7.898990	0.240554	0.155149
-8.191130	-5.534866	0.160154
-8.063721	-15.473040	0.165158
-8.285138	-4.402188	0.170163
-8.298168	-10.249675	0.175168
-7.928203	-3.543291	0.180173
-8.830614	0.655720	0.185178
-9.293851	-7.945202	0.190182
-9.166056	-2.489671	0.195187
-9.295933	-9.627708	0.200192
-10.291064	-16.417236	0.205197
-11.012308	-7.053628	0.210202
-10.538110	-9.676069	0.215206
-10.832778	-10.336979	0.220211
-11.064707	-14.014058	0.225216
-10.378921	-15.078465	0.230221
-11.288778	-15.556006	0.235226
-11.742242	-13.068021	0.240230
-12.144472	-6.392031	0.245235
-12.393514	-6.189665	0.250240
-12.499177	-9.743403	0.255245
-12.960345	-5.164974	0.260250
-12.740243	-19.408519	0.265254
-12.447985	-14.506710	0.270259
-13.465120	-9.019851	0.275264
-13.522319	-13.457970	0.280269
-14.209373	-9.217662	0.285274
-13.934677	-18.936122	0.290278
-14.582365	-8.503309	0.295283
-15.164001	-6.427245	0.300288
-15.299370	-3.319223	0.305293
-15.539363	-7.552829	0.310298
-15.329901	-10.153533	0.315302
-15.399529	-7.583673	0.320307
-15.485792	-14.961584	0.325312
-16.304901	-11.321601	0.330317
-17.244956	-8.818948	0.335322
-16.992293	-17.758634	0.340326
-16.981249	-10.544479	0.345331
-17.333236	-11.266740	0.350336
-17.228202	-16.713061	0.355341
-17.639981	-1.940486	0.360346
-17.415866	-11.407262	0.365350
-18.184208	-10.850727	0.370355
-18.380471	-7.513386	0.375360
-18.372445	-7.231834	0.380365
-19.203937	-10.374509	0.385370
-19.524781	-11.936251	0.390374
-19.865725	-13.722388	0.395379
-20.280209	-11.778392	0.400384
-20.124081	-6.122723	0.405389
-20.114404	-15.693502	0.410394
-20.378763	-14.315848	0.415398
-20.415244	-10.832694	0.420403
-20.858275	-11.332679	0.425408
-21.523538	-14.179253	0.430413
-22.073610	-10.358070	0.435418
-21.900721	-8.688545	0.440422
-22.221647	-6.283679	0.445427
-22.477806	-7.419237	0.450432
-22.087343	-6.253223	0.455437
-22.205341	-9.963771	0.460442
-22.309148	-14.082779	0.465446
-23.240780	-3.520260	0.470451
-23.706955	-7.290171	0.475456
-23.470593	-9.441069	0.480461
-24.104769	1.024836	0.485466
-24.740570	-11.287958	0.490470
-24.775439	-7.371332	0.495475
-24.923819	-5.629070	0.500480
-24.861937	-9.934370	0.505485
-25.233047	0.767396	0.510490
-25.073301	-16.320385	0.515494
-25.096457	-2.668884	0.520499
-25.860915	-8.581970	0.525504
-26.231444	-15.374285	0.530509
-26.674758	-6.155365	0.535514
-26.657195	-9.779038	0.540518
-26.854047	-12.244576	0.545523
-27.734781	-1.749487	0.550528
-28.338777	-13.660051	0.555533
-28.150455	-3.107957	0.560538
-27.550848	-9.196803	0.565542
-28.277672	-7.884449	0.570547
-28.328753	-3.689068	0.575552
-27.955395	-8.581905	0.580557
-28.778866	-3.353847	0.585562
-29.301854	-15.288677	0.590566
-29.647256	-0.383830	0.595571
-29.533423	-3.196225	0.600576
-30.133965	-12.980306	0.605581
-30.961194	0.514861	0.610586
-30.988282	-2.243612	0.615590
-30.798827	-5.876017	0.620595
-31.237464	-4.364324	0.625600
-31.134563	-15.219589	0.630605
-31.351171	-4.361076	0.635610
-31.611386	-12.750720	0.640614
-31.942031	-3.901512	0.645619
-32.189734	-6.960299	0.650624
-32.523257	-7.169590	0.655629
-32.989621	-6.139929	0.660634
-33.261950	-7.995048	0.665638
-33.028376	-4.023024	0.670643
-33.136908	-1.612481	0.675648
-33.901849	-11.213839	0.680653
-34.519672	2.014785	0.685658
-34.579806	-9.149347	0.690662
-35.304256	-8.511870	0.695667
-35.195595	-4.132388	0.700672
-35.066702	-13.152812	0.705677
-35.244044	-2.985153	0.710682
-34.954614	-3.123555	0.715686
-34.723311	-11.371804	0.720691
-35.902001	-6.630746	0.725696
-35.941877	-11.102319	0.730701
-36.168658	-11.342508	0.735706
-36.945347	-1.524332	0.740710
-37.868798	-1.638497	0.745715
-37.853904	-9.526691	0.750720
-37.921759	-16.339723	0.755725
-38.107856	-3.446233	0.760730
-38.060612	-17.533280	0.765734
-37.637317	-1.620472	0.770739
-37.788334	-10.884033	0.775744
-38.321484	-18.882550	0.780749
-38.958714	-8.178753	0.785754
-39.140345	-9.080183	0.790758
-39.562031	-7.018171	0.795763
-39.784866	-8.435908	0.800768
-40.006552	-12.554734	0.805773
-40.407339	-11.158828	0.810778
-40.717166	-14.014728	0.815782
-40.761392	-7.099654	0.820787
-40.740457	0.781628	0.825792
-41.007942	-14.144657	0.830797
-41.791265	-8.300859	0.835802
-42.299733	-10.220473	0.840806
-42.257198	-15.575536	0.845811
-42.422070	-21.732943	0.850816
-42.282263	-18.220180	0.855821
-42.478735	-11.329427	0.860826
-43.144067	-13.301800	0.865830
-43.709998	-8.670896	0.870835
-43.963796	-2.789675	0.875840
-43.967832	-5.002983	0.880845
-44.215902	-6.201053	0.885850
-43.882102	-20.229780	0.890854
-44.131534	-7.542872	0.895859
-44.463328	-11.932556	0.900864
-44.964564	-20.964264	0.905869
-45.306199	-13.317368	0.910874
-45.583519	-12.371700	0.915878
-45.522775	-10.489824	0.920883
-46.043967	-9.727743	0.925888
-46.633576	-16.176330	0.930893
-47.086788	-8.814847	0.935898
-46.968947	-10.049240	0.940902
-47.087917	-3.632486	0.945907
-47.277867	-6.933294	0.950912
-46.967317	0.518583	0.955917
-47.690503	-1.637596	0.960922
-48.534137	-7.572296	0.965926
-48.541425	-5.816892	0.970931
-49.027076	-8.727542	0.975936
-49.043340	-13.182501	0.980941
-48.780582	0.536302	0.985946
-49.098718	-15.587496	0.990950
-48.917491	-12.215580	0.995955
-49.664582	-8.493191	1.000960
-50.005793	-9.782001	1.005965
-50.503907	-4.347340	1.010970
-50.356929	1.070873	1.015974
-50.548132	-10.231785	1.020979
-51.645933	-4.871863	1.025984
-51.589134	-9.794763	1.030989
-52.129492	-6.805168	1.035994
-52.123621	-8.373258	1.040998
-52.070892	-12.563377	1.046003
-51.893929	-10.403958	1.051008
-51.826685	-13.261521	1.056013
-52.313237	-8.082941	1.061018
-53.060899	-12.738433	1.066022
-53.293895	-9.916560	1.071027
-53.633666	-14.654398	1.076032
-53.662210	-13.922002	1.081037
-54.685012	-9.060927	1.086042
-54.537830	-15.139969	1.091046
-54.840252	-23.105452	1.096051
-55.005951	-17.447999	1.101056
-54.730843	-12.871915	1.106061
-54.905327	-9.878382	1.111066
-55.453278	-12.940526	1.116070
-55.783806	-4.518565	1.121075
-56.652241	-12.431760	1.126080
-56.386327	-15.016554	1.131085
-57.049311	-10.557636	1.136090
-57.029223	-9.385347	1.141094
-56.807720	-4.747103	1.146099
-57.195640	-10.006611	1.151104
-57.190529	-9.145601	1.156109
-58.074030	-4.124270	1.161114
-58.589950	-8.736443	1.166118
-58.688950	-5.087240	1.171123
-58.974582	-11.004230	1.176128
-58.597018	-15.024760	1.181133
-58.790042	-11.412281	1.186138
-58.857530	-17.487938	1.191142
-59.571300	-13.066194	1.196147
-59.852267	2.705524	1.201152
-59.589635	-13.125113	1.206157
-60.329032	-9.805570	1.211162
-60.606226	-19.556952	1.216166
-61.366056	-20.736771	1.221171
-61.637857	-13.737050	1.226176
-61.873232	-16.877201	1.231181
-61.812812	-10.999870	1.236186
-61.877439	-6.712462	1.241190
-61.824038	-11.605000	1.246195
-61.749272	-7.014681	1.251200
-61.646298	-18.327569	1.256205
-62.906351	-13.987038	1.261210
-63.181959	-13.675289	1.266214
-63.088448	-14.164271	1.271219
-63.925801	-5.535835	1.276224
-64.067693	-23.157756	1.281229
-64.547762	-11.454448	1.286234
-64.962791	-7.240830	1.291238
-64.886206	-0.936775	1.296243
-64.987656	-9.545305	1.301248
-64.984519	-10.804707	1.306253
-65.040174	-18.512294	1.311258
-64.985509	-16.376432	1.316262
-65.329678	-11.538940	1.321267
-66.281008	-14.223679	1.326272
-66.001742	-12.779959	1.331277
-66.176294	-5.193486	1.336282
-67.001197	-17.961176	1.341286
-67.453273	-9.682283	1.346291
-67.960306	-12.700684	1.351296
-67.692407	-13.526583	1.356301
-67.989734	-2.659637	1.361306
-67.986299	-13.955057	1.366310
-67.674823	-12.758405	1.371315
-68.632203	-8.812341	1.376320
-69.286868	-11.455040	1.381325
-69.855686	-11.901826	1.386330
-69.638875	-9.446101	1.391334
-69.778204	-19.121844	1.396339
-70.070393	-7.726703	1.401344
-69.721554	-13.945504	1.406349
-70.043110	-9.810710	1.411354
-70.461680	-0.850642	1.416358
-71.068807	-12.574394	1.421363
-71.522295	-9.168209	1.426368
-71.457071	-17.602069	1.431373
-71.792523	-4.228207	1.436378
-71.371209	-17.712382	1.441382
-71.599996	-11.006705	1.446387
-72.633600	-13.256313	1.451392
-72.597440	-15.991512	1.456397
-73.214464	-8.233296	1.461402
-73.184886	-4.830543	1.466406
-73.114305	-7.006282	1.471411
-73.411634	-6.024344	1.476416
-73.878909	-13.666133	1.481421
-74.909019	-7.131248	1.486426
-75.017445	-11.549632	1.491430
-74.460925	-15.539416	1.496435
-75.062508	-8.485867	1.501440
-74.638191	-12.155587	1.506445
-74.947402	-18.084652	1.511450
-75.034510	-13.272563	1.516454
-75.681628	-14.534785	1.521459
-75.861937	-16.100457	1.526464
-76.238945	-17.380573	1.531469
-77.322936	-15.121064	1.536474
-77.274285	-16.018793	1.541478
-77.625712	-13.882377	1.546483
-77.805531	-5.008027	1.551488
-77.087947	-18.561196	1.556493
-77.685764	-13.365768	1.561498
-77.905963	-12.951109	1.566502
-77.963466	-17.213743	1.571507
-78.781923	-6.115852	1.576512
-78.844010	-1.514314	1.581517
-79.108901	-9.413792	1.586522
-79.272045	-8.870843	1.591526
-79.328092	-9.907127	1.596531
-80.687717	-7.520865	1.601536
-80.456749	-12.159833	1.606541
-80.479383	-11.749476	1.611546
-81.113157	-10.835152	1.616550
-81.185016	-11.871975	1.621555
-81.445405	-6.461092	1.626560
-81.208688	-12.145497	1.631565
-81.553792	-1.689972	1.636570
-81.132843	-2.198451	1.641574
-81.528310	-12.228417	1.646579
-82.438691	-13.566228	1.651584
-82.752519	-17.270584	1.656589
-82.831443	-13.032906	1.661594
-83.320170	-10.173614	1.666598
-83.635426	-17.782165	1.671603
-84.401541	-9.919535	1.676608
-84.122233	-25.835601	1.681613
-84.208855	-15.044209	1.686618
-84.616151	-17.043323	1.691622
-84.533692	-9.431534	1.696627
-84.767494	-12.031449	1.701632
-84.564709	-22.535023	1.706637
-85.275320	-11.234772	1.711642
-86.003109	-19.263993	1.716646
-86.253896	-22.002384	1.721651
-86.509058	-9.166532	1.726656
-86.154988	-24.320053	1.731661
-86.134067	-19.942427	1.736666
-86.396268	-16.886022	1.741670
-87.213951	-19.357667	1.746675
-87.610391	-9.684555	1.751680
-87.509095	-16.239661	1.756685
-87.679833	-6.733969	1.761690
-88.098040	-9.438913	1.766694
-88.944853	-12.482735	1.771699
-89.121022	-8.481933	1.776704
-89.218669	-18.036704	1.781709
-89.752509	-14.518151	1.786714
-89.947012	-11.167485	1.791718
-89.527486	-14.662167	1.796723
-89.736578	-8.372768	1.801728
-89.412840	-14.315093	1.806733
-89.448048	-16.254468	1.811738
-90.653707	-19.585574	1.816742
-90.834000	-21.791593	1.821747
-91.395134	-13.326315	1.826752
-91.129623	-17.937851	1.831757
-91.893594	0.142728	1.836762
-92.167002	-4.722920	1.841766
-92.065314	-4.210214	1.846771
-92.606655	-9.755700	1.851776
-92.396096	-14.802530	1.856781
-92.630278	-13.935043	1.861786
-93.268504	-11.317194	1.866790
-93.390052	-9.889977	1.871795
-94.179358	-5.474661	1.876800
-93.742719	-8.721566	1.881805
-94.041532	-18.214211	1.886810
-94.270220	-1.391086	1.891814
-94.986519	-7.285886	1.896819
-95.856345	-3.838768	1.901824
-95.054723	-10.996876	1.906829
-95.190450	-8.847835	1.911834
-95.832464	-11.017447	1.916838
-95.470469	-26.069072	1.921843
-95.955250	-9.329837	1.926848
-96.388014	-14.543629	1.931853
-97.114149	-16.701084	1.936858
-97.351437	-7.284419	1.941862
-97.287704	-15.390261	1.946867
-97.542681	-18.781130	1.951872
-97.363072	-25.494043	1.956877
-97.334750	-15.722759	1.961882
-97.926364	-10.553615	1.966886
-98.429124	-20.225207	1.971891
-98.943038	-14.911066	1.976896
-98.905448	-21.418125	1.981901
-99.160008	-8.828250	1.986906
-99.457818	-9.922568	1.991910
-100.027493	-22.332518	1.996915
-100.332403	-19.227278	2.006912
-99.423137	-8.249241	2.016909
-99.200758	-11.010769	2.026906
-98.672975	-14.669333	2.036902
-97.844028	-12.474309	2.046899
-97.590294	-9.649553	2.056896
-97.758481	-15.851963	2.066893
-96.614348	-14.329754	2.076890
-96.160995	-18.105409	2.086886
-95.522893	-11.709919	2.096883
-94.778642	-7.500509	2.106880
-94.546628	-14.297345	2.116877
-94.461391	-12.037638	2.126874
-94.096899	-10.702053	2.136870
-93.311590	-6.323393	2.146867
-92.355496	-7.708536	2.156864
-92.193190	-12.511252	2.166861
-91.890806	-6.942579	2.176858
-91.033413	-8.456008	2.186854
-90.267076	-11.453637	2.196851
-90.580668	-11.335505	2.206848
-89.698230	-6.966607	2.216845
-89.397232	-11.765224	2.226842
-88.799340	-9.973932	2.236838
-87.527717	-3.859403	2.246835
-87.356908	-9.705004	2.256832
-87.280983	-13.800679	2.266829
-87.145096	-10.552936	2.276826
-86.097745	-8.137019	2.286822
-85.657033	-13.188763	2.296819
-84.536361	-10.860269	2.306816
-84.972797	-12.066957	2.316813
-84.305204	-16.384701	2.326810
-83.628162	-13.905482	2.336806
-83.166684	-12.665584	2.346803
-82.736959	-10.654190	2.356800
-81.581100	-8.193805	2.366797
-81.573918	-6.648681	2.376794
-80.917761	-10.891426	2.386790
-81.006054	-7.026444	2.396787
-80.171668	-9.104317	2.406784
-79.461665	-7.918814	2.416781
-79.361132	-5.472550	2.426778
-78.779451	-8.495119	2.436774
-78.259423	-6.064780	2.446771
-77.526435	-12.185260	2.456768
-76.711269	0.489829	2.466765
-76.544163	-6.445439	2.476762
-76.130192	-5.169022	2.486758
-75.959110	0.745047	2.496755
-75.098762	-7.683978	2.506752
-74.637521	-2.212343	2.516749
-74.045717	-3.593268	2.526746
-73.836062	-4.940346	2.536742
-72.771819	-8.801758	2.546739
-72.170653	-6.765010	2.556736
-71.930812	-3.303502	2.566733
-71.790490	-4.197494	2.576730
-71.456461	-5.574258	2.586726
-70.551604	-9.752282	2.596723
-70.153823	-5.994865	2.606720
-69.621454	-6.868820	2.616717
-68.668311	-2.940189	2.626714
-68.506068	-5.054940	2.636710
-68.417017	-4.396307	2.646707
-67.798812	-5.440768	2.656704
-67.312427	-8.925910	2.666701
-66.349389	-5.894771	2.676698
-65.694150	-7.378077	2.686694
-66.000300	-5.808725	2.696691
-64.891664	-13.518158	2.706688
-64.174140	-0.600265	2.716685
-64.056017	-3.357767	2.726682
-63.977698	-6.908109	2.736678
-63.084276	-7.455773	2.746675
-62.321360	-10.516652	2.756672
-62.294999	-8.918985	2.766669
-61.387010	-9.770576	2.776666
-60.783778	-10.483575	2.786662
-60.719862	-12.042238	2.796659
-60.296790	-12.659803	2.806656
-59.398228	-9.769929	2.816653
-59.105722	-10.257003	2.826650
-58.825120	-8.064422	2.836646
-57.873857	-8.553299	2.846643
-57.856168	-7.569872	2.856640
-56.750387	-6.714870	2.866637
-56.144704	-4.718582	2.876634
-56.050841	-6.541042	2.886630
-55.886471	-14.739612	2.896627
-55.540288	-4.732704	2.906624
-54.616332	-9.887592	2.916621
-53.575842	-7.649543	2.926618
-53.196897	-4.724396	2.936614
-52.916024	-7.406500	2.946611
-53.211272	-7.033164	2.956608
-52.192243	-10.975403	2.966605
-51.404542	-7.367122	2.976602
-51.084793	-7.522613	2.986598
-50.057334	-7.582699	2.996595
-49.923456	-3.164318	3.006592
-50.106151	-7.294820	3.016589
-48.884475	-8.881212	3.026586
-48.468850	-7.129477	3.036582
-48.198109	-6.924556	3.046579
-47.317617	-7.590603	3.056576
-46.819289	-6.368065	3.066573
-46.662800	-8.372004	3.076570
-46.233592	-12.154723	3.086566
-45.266310	-16.012518	3.096563
-45.310214	-10.647110	3.106560
-44.263404	-7.659476	3.116557
-43.724059	-3.303103	3.126554
-43.593666	-5.755588	3.136550
-43.446227	-7.799522	3.146547
-42.719373	-6.958626	3.156544
-42.209676	-11.423305	3.166541
-41.487451	-4.841576	3.176538
-40.669968	-15.888028	3.186534
-40.789629	-6.759697	3.196531
-40.008898	-6.907551	3.206528
-39.579610	-4.067403	3.216525
-39.189649	-5.309585	3.226522
-38.051661	-5.396073	3.236518
-37.615101	-7.488873	3.246515
-37.484869	-2.969710	3.256512
-37.325789	-5.367868	3.266509
-36.542697	-11.948717	3.276506
-35.824699	-7.883334	3.286502
-35.806276	-11.848962	3.296499
-34.773996	-3.395670	3.306496
-34.551246	-2.432370	3.316493
-34.260668	-4.414255	3.326490
-33.513630	-15.218458	3.336486
-32.772895	-8.789367	3.346483
-32.712185	-12.832733	3.356480
-31.598559	-3.459911	3.366477
-31.226453	-4.815711	3.376474
-31.021687	-6.995000	3.386470
-30.695396	-8.364750	3.396467
-30.037983	-17.733862	3.406464
-29.463576	-13.959060	3.416461
-29.226896	-10.735710	3.426458
-28.065258	-10.397942	3.436454
-27.950764	-12.100919	3.446451
-27.822679	-10.078295	3.456448
-26.603602	-2.685157	3.466445
-26.141535	-6.903660	3.476442
-26.048174	-10.499567	3.486438
-25.976483	-7.821498	3.496435
-24.762904	-5.836561	3.506432
-24.481037	-3.553494	3.516429
-24.096638	-4.955786	3.526426
-23.246423	-6.274973	3.536422
-22.907757	-9.412992	3.546419
-22.702072	-9.129722	3.556416
-21.888272	-9.339559	3.566413
-21.462170	-8.642886	3.576410
-21.174158	-10.222455	3.586406
-20.300674	-9.658154	3.596403
-20.119956	-5.138460	3.606400
-19.317701	-4.798083	3.616397
-18.613143	-5.216460	3.626394
-18.185131	-2.921831	3.636390
-18.003195	-8.242907	3.646387
-17.909323	-8.768611	3.656384
-17.018391	-4.216358	3.666381
-16.676501	-5.502741	3.676378
-15.690270	-1.977710	3.686374
-15.222690	-5.864983	3.696371
-15.069297	2.945866	3.706368
-14.634311	-3.072509	3.716365
-13.822532	-7.522203	3.726362
-13.347731	-8.262930	3.736358
-13.100018	-4.121246	3.746355
-12.304563	-1.426493	3.756352
-11.956440	-5.101931	3.766349
-11.830535	-7.757779	3.776346
-10.536663	-9.515963	3.786342
-10.386445	-7.408089	3.796339
-10.080846	-2.647469	3.806336
-9.060562	0.539191	3.816333
-8.728987	-1.412138	3.826330
-8.603957	-2.739274	3.836326
-8.417766	-0.732394	3.846323
-7.512774	-2.047410	3.856320
-6.814581	-3.948602	3.866317
-6.164562	-3.897176	3.876314
-5.712723	-7.734223	3.886310
-5.596168	-1.977684	3.896307
-5.428216	-1.771151	3.906304
-4.788524	5.935284	3.916301
-3.900812	11.951204	3.926298
-3.501071	23.215601	3.936294
-3.077029	26.463063	3.946291
-2.836719	38.963694	3.956288
-2.393319	52.566236	3.966285
-1.784990	58.208961	3.976282
-1.212840	70.668105	3.986278
-1.051668	85.313051	3.996275
-0.431276	106.287157	4.006272
0.000000	137.788955	4.011277
-0.221244	133.242191	4.016282
0.380232	135.335680	4.021286
0.241793	151.705955	4.026291
0.573317	169.380168	4.031296
0.768915	168.317790	4.036301
0.757562	167.279815	4.041306
0.988482	160.640808	4.046310
0.656169	170.326304	4.051315
0.781313	159.673841	4.056320
0.731220	173.547227	4.061325
0.756748	165.209228	4.066330
0.774883	169.990924	4.071334
0.576667	181.369068	4.076339
1.117188	170.352009	4.081344
0.746669	170.806163	4.086349
1.020320	168.140337	4.091354
0.824683	177.527330	4.096358
0.749034	174.188805	4.101363
1.191219	171.537300	4.106368
0.949518	179.126499	4.111373
0.893542	184.653969	4.116378
1.027007	180.570407	4.121382
0.880480	174.997742	4.126387
1.048083	182.153306	4.131392
0.905796	186.775879	4.136397
1.119327	194.977419	4.141402
1.182611	193.037690	4.146406
1.114455	205.192341	4.151411
1.357402	195.673183	4.156416
1.411348	196.694840	4.161421
1.286074	189.921611	4.166426
0.885978	183.092857	4.171430
0.918184	189.886435	4.176435
1.204270	184.359348	4.181440
0.947499	183.140796	4.186445
1.116710	189.458802	4.191450
1.112794	193.771340	4.196454
1.039073	194.864261	4.201459
1.323191	196.473754	4.206464
1.339319	199.502660	4.211469
0.985122	203.670737	4.216474
1.309470	197.702184	4.221478
1.179741	196.400828	4.226483
1.281590	195.155847	4.231488
1.412683	202.019292	4.236493
1.440103	205.517962	4.241498
1.808542	205.296818	4.246502
1.244171	196.473158	4.251507
1.447833	201.731296	4.256512
1.316920	203.821157	4.261517
1.097483	212.832833	4.266522
1.345374	206.369783	4.271526
0.951338	206.978992	4.276531
1.364223	204.934997	4.281536
1.471062	210.832358	4.286541
1.444197	204.532615	4.291546
1.531664	199.189966	4.296550
1.782059	204.275591	4.301555
1.483633	204.483373	4.306560
0.976430	211.317341	4.311565
1.257993	209.767513	4.316570
1.060125	201.440834	4.321574
1.293174	212.991495	4.326579
1.451222	213.851465	4.331584
1.597293	230.300414	4.336589
1.473325	231.455530	4.341594
1.725817	234.643035	4.346598
1.817225	238.350949	4.351603
1.935534	227.189851	4.356608
1.412715	218.051454	4.361613
1.201767	218.035574	4.366618
1.960714	226.048148	4.371622
1.818586	229.149837	4.376627
1.754350	211.076294	4.381632
1.658327	217.511640	4.386637
1.600144	219.990842	4.391642
1.650750	217.123953	4.396646
1.669984	232.386407	4.401651
1.865171	228.432721	4.406656
2.104718	233.015169	4.411661
1.764951	225.545521	4.416666
1.809893	214.000725	4.421670
1.639527	207.790851	4.426675
1.687895	211.829714	4.431680
1.808646	217.743916	4.436685
1.921877	224.822267	4.441690
1.721321	223.125138	4.446694
1.456256	232.553064	4.451699
1.742538	232.484844	4.456704
1.480720	235.075123	4.461709
1.736706	245.113177	4.466714
2.014267	238.123048	4.471718
1.765662	246.262019	4.476723
2.041612	240.753956	4.481728
1.742336	244.485716	4.486733
1.733613	244.897526	4.491738
1.837214	231.729580	4.496742
1.598611	245.809875	4.501747
2.115753	236.339813	4.506752
1.859879	242.708299	4.511757
1.965895	234.512831	4.516762
2.005640	228.924892	4.521766
2.046418	234.556535	4.526771
2.220088	233.481208	4.531776
1.766742	235.416866	4.536781
1.644067	251.232883	4.541786
2.340546	250.981494	4.546790
2.171854	264.606814	4.551795
2.258398	258.108102	4.556800
2.197625	259.076535	4.561805
2.159984	255.359917	4.566810
2.077001	239.481461	4.571814
1.934575	248.468565	4.576819
2.501742	249.181857	4.581824
2.217105	248.310688	4.586829
2.025203	252.356393	4.591834
2.349195	260.035285	4.596838
1.969620	273.246395	4.601843
2.276317	264.620046	4.606848
2.401495	263.826847	4.611853
2.296908	262.783386	4.616858
2.694154	262.705869	4.621862
2.328374	248.303739	4.626867
2.375921	249.113336	4.631872
1.777124	253.134262	4.636877
2.024084	259.269910	4.641882
2.432031	265.989660	4.646886
2.205693	278.744812	4.651891
2.332418	268.894186	4.656896
2.360038	274.967295	4.661901
2.470395	271.059614	4.666906
2.579689	270.682071	4.671910
2.201980	279.467994	4.676915
2.624460	273.118287	4.681920
2.452465	271.932854	4.686925
2.379756	269.891114	4.691930
2.546931	270.027718	4.696934
2.537779	265.974460	4.701939
2.785404	270.464609	4.706944
2.705589	263.530292	4.711949
2.396313	262.914411	4.716954
2.494447	270.815810	4.721958
2.363632	266.684226	4.726963
2.665758	268.179842	4.731968
2.706549	268.359870	4.736973
2.865532	265.247892	4.741978
2.808933	258.932133	4.746982
2.261709	252.248678	4.751987
2.596668	257.373796	4.756992
2.516543	277.755479	4.761997
2.317440	270.338294	4.767002
2.703550	267.958319	4.772006
2.379220	272.573370	4.777011
2.649113	270.171790	4.782016
2.363076	272.061002	4.787021
2.447307	270.025836	4.792026
2.514714	266.951912	4.797030
2.195093	268.269474	4.802035
2.661722	275.569943	4.807040
2.555012	280.939492	4.812045
2.734226	288.403989	4.817050
2.970113	298.214915	4.822054
2.773519	291.789911	4.827059
2.860185	273.599744	4.832064
2.918025	276.712533	4.837069
2.247793	284.450691	4.842074
2.825839	293.931448	4.847078
2.576970	299.273038	4.852083
2.743824	303.411892	4.857088
3.055530	302.859932	4.862093
2.959074	311.869259	4.867098
2.836686	299.123091	4.872102
3.022821	311.762607	4.877107
3.173080	309.724396	4.882112
3.303127	303.152551	4.887117
2.972840	311.998326	4.892122
3.229811	301.050822	4.897126
2.703678	298.524315	4.902131
2.829329	300.211367	4.907136
3.115310	303.797882	4.912141
3.172941	306.906765	4.917146
3.143925	300.350801	4.922150
2.999770	309.398414	4.927155
3.276312	298.201592	4.932160
2.918330	292.117472	4.937165
2.830054	300.559672	4.942170
3.087760	301.282375	4.947174
3.115323	303.605703	4.952179
3.233452	298.471265	4.957184
3.185596	305.118307	4.962189
3.457788	306.265452	4.967194
3.304722	288.543186	4.972198
3.012345	287.891946	4.977203
2.610715	284.339195	4.982208
2.934188	295.680963	4.987213
3.150556	299.270124	4.992218
3.286997	295.155847	4.997222
3.159392	313.006302	5.002227
2.970492	305.790077	5.007232
3.210471	309.401181	5.012237
2.984092	306.555672	5.017242
2.947249	309.620208	5.022246
3.082333	305.005114	5.027251
2.985268	296.398443	5.032256
3.381987	298.081853	5.037261
2.972364	309.514633	5.042266
3.462952	317.912297	5.047270
3.650238	321.139428	5.052275
3.629439	321.948112	5.057280
3.462942	300.922850	5.062285
3.413426	311.683073	5.067290
3.350638	303.238854	5.072294
2.965751	314.269512	5.077299
3.364438	314.888160	5.082304
3.281004	316.951032	5.087309
3.413118	327.383803	5.092314
3.825352	328.252998	5.097318
3.584972	331.596927	5.102323
3.385666	318.093666	5.107328
3.726280	329.036761	5.112333
3.576796	328.259439	5.117338
3.320892	305.585026	5.122342
3.291334	322.541500	5.127347
3.380286	329.333834	5.132352
3.712132	329.909283	5.137357
3.330497	348.156261	5.142362
3.659336	323.883648	5.147366
3.551209	340.027294	5.152371
3.728200	338.717762	5.157376
3.905076	334.064955	5.162381
3.593868	333.818610	5.167386
3.982540	332.672942	5.172390
3.848961	335.284234	5.177395
3.654771	328.731731	5.182400
3.800700	326.861576	5.187405
3.270042	330.869660	5.192410
3.880925	325.440099	5.197414
3.668919	336.612251	5.202419
3.484647	327.497650	5.207424
3.822266	328.596864	5.212429
3.501898	337.113826	5.217434
3.770599	335.242482	5.222438
3.279143	328.754201	5.227443
3.261218	332.559572	5.232448
3.594081	334.151141	5.237453
3.592006	331.520287	5.242458
3.634506	333.905281	5.247462
3.590069	344.959509	5.252467
3.981939	349.837245	5.257472
4.058482	361.047673	5.262477
4.031853	370.370487	5.267482
4.093473	345.063637	5.272486
3.938857	348.226421	5.277491
3.660045	338.845472	5.282496
3.802798	348.500761	5.287501
3.444619	358.055875	5.292506
3.973115	367.508572	5.297510
3.977305	366.252319	5.302515
4.239260	373.964037	5.307520
4.132683	367.943439	5.312525
3.888540	363.244501	5.317530
4.088800	361.197411	5.322534
4.157818	370.386773	5.327539
4.070470	371.667658	5.332544
4.191457	364.761220	5.337549
3.893908	360.436597	5.342554
3.906765	365.226134	5.347558
3.959568	368.938894	5.352563
3.783623	373.096246	5.357568
4.039146	370.736104	5.362573
4.118809	377.220373	5.367578
4.163337	361.190829	5.372582
4.375647	369.332279	5.377587
4.020724	369.797077	5.382592
4.131651	372.378741	5.387597
4.050962	373.798830	5.392602
4.378970	364.210032	5.397606
4.098019	367.018995	5.402611
3.991773	376.478529	5.407616
4.318078	370.429072	5.412621
3.945199	369.654206	5.417626
3.994671	376.496906	5.422630
4.035254	389.136513	5.427635
4.180489	384.483799	5.432640
4.448944	390.658368	5.437645
3.894238	405.210297	5.442650
4.316748	398.820869	5.447654
4.355342	404.566800	5.452659
4.378232	389.999734	5.457664
4.499440	388.511174	5.462669
4.201076	392.772869	5.467674
4.558125	399.911175	5.472678
4.539888	400.354756	5.477683
4.482884	400.085656	5.482688
4.632932	406.039085	5.487693
4.547079	416.241996	5.492698
4.764893	397.186541	5.497702
4.611969	394.907843	5.502707
4.548578	398.884155	5.507712
4.138020	389.996236	5.512717
4.530910	401.639171	5.517722
4.765604	394.722574	5.522726
4.464829	406.791973	5.527731
4.566801	400.889766	5.532736
4.483588	396.544046	5.537741
4.484540	402.112093	5.542746
4.649076	400.177477	5.547750
4.465363	402.358989	5.552755
4.615021	402.831603	5.557760
4.775699	396.194655	5.562765
4.510919	402.307944	5.567770
4.509826	398.827571	5.572774
4.661166	399.947966	5.577779
4.401800	396.579035	5.582784
4.605782	397.522580	5.587789
4.453674	400.719493	5.592794
4.695883	392.006465	5.597798
4.270023	398.311795	5.602803
4.389391	403.447402	5.607808
4.463203	406.330830	5.612813
4.539788	418.438591	5.617818
4.931608	423.393716	5.622822
4.519190	424.355265	5.627827
4.906968	427.763135	5.632832
4.933167	428.637846	5.637837
4.740735	440.515278	5.642842
4.792726	433.632272	5.647846
5.014984	439.166844	5.652851
5.217214	439.891044	5.657856
5.147909	437.164939	5.662861
4.713113	425.685019	5.667866
5.191230	422.942864	5.672870
4.879109	426.951687	5.677875
4.733544	410.006344	5.682880
4.877083	417.513120	5.687885
4.634957	427.335398	5.692890
4.906303	424.974600	5.697894
5.046958	435.572189	5.702899
4.614385	436.705604	5.707904
5.240555	429.217402	5.712909
4.693683	432.856015	5.717914
5.040080	436.957083	5.722918
4.871091	430.574023	5.727923
4.653200	433.721055	5.732928
5.024771	425.249838	5.737933
4.857872	438.712013	5.742938
4.703640	435.858084	5.747942
4.802661	444.334470	5.752947
5.150433	460.097663	5.757952
5.679532	456.499094	5.762957
5.241489	454.731741	5.767962
5.314227	438.149435	5.772966
5.378187	434.868054	5.777971
5.133481	431.339606	5.782976
5.155494	428.648308	5.787981
4.760338	436.054061	5.792986
5.223441	432.407618	5.797990
5.177747	439.613619	5.802995
5.310828	444.106998	5.808000
5.402999	437.714631	5.813005
5.074440	435.305363	5.818010
5.122321	431.774840	5.823014
5.193658	451.514593	5.828019
5.508954	457.354836	5.833024
5.484453	454.823187	5.838029
4.891144	453.708490	5.843034
5.419584	459.417533	5.848038
5.752751	466.309204	5.853043
5.285318	466.242650	5.858048
5.266441	458.385461	5.863053
5.366842	467.009635	5.868058
5.599832	461.398691	5.873062
5.602092	468.820547	5.878067
5.379277	455.455249	5.883072
5.572001	458.435822	5.888077
5.539731	452.654099	5.893082
5.543204	440.018401	5.898086
5.386712	440.268397	5.903091
4.812192	457.989566	5.908096
5.497102	462.821971	5.913101
5.160033	466.275281	5.918106
5.657499	467.457954	5.923110
5.616228	476.591048	5.928115
5.411445	464.671031	5.933120
5.516257	464.693245	5.938125
5.215037	468.166669	5.943130
5.546133	463.171556	5.948134
5.419908	468.381991	5.953139
5.072035	472.223877	5.958144
5.364925	476.854990	5.963149
5.435791	493.153669	5.968154
5.595802	497.756074	5.973158
5.687787	505.069552	5.978163
5.856683	502.923245	5.983168
5.833720	494.864045	5.988173
5.778036	500.266663	5.993178
5.921193	492.052082	5.998182
5.529748	480.727352	6.003187
5.792075	485.961665	6.008192
5.854778	492.575088	6.013197
5.532028	489.034093	6.018202
5.735735	494.232727	6.023206
6.039227	495.906337	6.028211
5.761121	493.441343	6.033216
5.584388	484.406311	6.038221
5.383139	498.134515	6.043226
5.922136	486.251363	6.048230
5.752751	491.013493	6.053235
5.592410	497.734302	6.058240
5.885121	494.328200	6.063245
5.795006	506.191897	6.068250
5.977306	505.470532	6.073254
6.114468	497.390934	6.078259
5.661474	485.033848	6.083264
5.902869	474.359551	6.088269
5.746023	472.588653	6.093274
5.854103	475.650932	6.098278
5.519193	476.152084	6.103283
5.625489	472.328302	6.108288
5.915159	481.201168	6.113293
5.708046	476.006663	6.118298
5.872865	465.972985	6.123302
5.650404	474.125901	6.128307
5.310492	472.617979	6.133312
5.984653	492.460433	6.138317
5.940404	498.755105	6.143322
5.994769	487.317082	6.148326
5.849068	483.042664	6.153331
5.519012	476.188959	6.158336
5.910182	468.070276	6.163341
5.791047	472.764089	6.168346
5.804081	465.779772	6.173350
5.774499	470.626099	6.178355
5.700414	476.740992	6.183360
6.139742	456.703332	6.188365
6.138193	469.896018	6.193370
6.114272	463.928594	6.198374
6.138116	467.731818	6.203379
5.660436	469.447159	6.208384
5.896097	462.345860	6.213389
5.501502	481.045468	6.218394
5.612590	471.559224	6.223398
5.899198	476.441209	6.228403
5.573928	476.398673	6.233408
5.981786	460.574087	6.238413
5.703057	475.993078	6.243418
5.870458	470.678739	6.248422
5.782878	471.031583	6.253427
5.656031	481.018726	6.258432
6.004776	473.256553	6.263437
5.390191	472.413168	6.268442
5.604886	466.396364	6.273446
5.756003	461.461642	6.278451
5.318696	474.240836	6.283456
5.927861	471.426257	6.288461
5.837761	474.958656	6.293466
5.891694	468.649966	6.298470
5.731379	461.587200	6.303475
5.630527	468.945617	6.308480
5.943951	474.746906	6.313485
5.811251	461.321096	6.318490
5.725526	470.049897	6.323494
5.877240	468.047142	6.328499
5.984714	470.429884	6.333504
5.552620	464.761330	6.338509
5.601672	476.396727	6.343514
5.326825	471.870776	6.348518
5.594334	468.294602	6.353523
5.615913	467.858761	6.358528
5.780198	463.109922	6.363533
5.732485	464.744396	6.368538
5.676775	466.350593	6.373542
5.674143	472.234409	6.378547
5.556559	471.383518	6.383552
5.716238	475.531302	6.388557
5.804547	476.268645	6.393562
5.893859	479.959204	6.398566
5.764624	468.955551	6.403571
5.615648	472.518419	6.408576
5.605249	470.993232	6.413581
5.772901	496.300811	6.418586
6.150912	482.871324	6.423590
5.889073	478.451359	6.428595
5.701928	473.367018	6.433600
5.787259	460.397269	6.438605
5.693117	467.496257	6.443610
5.836679	468.895404	6.448614
5.698462	472.778549	6.453619
5.547492	476.167695	6.458624
5.907326	466.945351	6.463629
6.074684	476.718404	6.468634
5.823203	460.759480	6.473638
5.746502	466.044400	6.478643
5.732906	470.960700	6.483648
5.870478	465.455344	6.488653
5.587202	471.464369	6.493658
5.601524	464.124629	6.498662
5.916583	470.965624	6.503667
5.644338	474.642247	6.508672
6.122675	473.167163	6.513677
5.580545	469.296829	6.518682
5.566926	467.855650	6.523686
5.947375	474.062818	6.528691
5.675649	471.840091	6.533696
5.820145	464.793354	6.538701
5.713662	464.701763	6.543706
5.714862	471.172029	6.548710
6.091552	459.741828	6.553715
5.877257	472.460412	6.558720
5.870234	468.378332	6.563725
5.584818	473.153947	6.568730
5.405366	470.475873	6.573734
5.508576	474.205571	6.578739
5.449826	482.654229	6.583744
5.835509	483.808052	6.588749
5.803557	494.482611	6.593754
5.902075	484.865828	6.598758
5.714240	478.907780	6.603763
5.521673	480.440338	6.608768
5.662199	487.078959	6.613773
5.727269	496.816470	6.618778
5.933512	497.853384	6.623782
6.114009	501.142655	6.628787
5.715373	493.362145	6.633792
5.827459	479.487095	6.638797
5.480803	486.279600	6.643802
5.525674	487.309884	6.648806
5.859764	490.564050	6.653811
5.741789	497.976032	6.658816
5.748849	500.362184	6.663821
5.710817	498.834662	6.668826
5.844885	497.359750	6.673830
6.071074	502.374295	6.678835
5.679226	492.619659	6.683840
5.743844	471.720280	6.688845
5.372525	482.002078	6.693850
5.284181	495.977796	6.698854
6.031993	502.669592	6.703859
5.963346	510.773178	6.708864
6.141365	496.721430	6.713869
6.120886	487.456670	6.718874
6.061357	476.950802	6.723878
5.729609	466.587108	6.728883
5.352130	473.097977	6.733888
5.842938	471.903221	6.738893
5.934735	476.943367	6.743898
5.633400	468.763130	6.748902
5.775899	471.134547	6.753907
5.804427	467.520391	6.758912
5.797083	465.841958	6.763917
5.290483	473.980353	6.768922
5.475041	483.900935	6.773926
5.759968	494.525390	6.778931
5.776782	508.659537	6.783936
5.784058	507.522941	6.788941
6.448016	505.110933	6.793946
5.918454	493.063121	6.798950
6.001463	482.014249	6.803955
5.757317	481.792120	6.808960
5.687668	474.153892	6.813965
5.557272	482.806030	6.818970
5.525826	467.145352	6.823974
5.757893	468.366447	6.828979
5.957473	475.343786	6.833984
6.105502	470.933311	6.838989
5.921747	468.702726	6.843994
5.906786	472.810952	6.848998
5.877359	472.629836	6.854003
5.573853	475.408807	6.859008
6.105236	471.549171	6.864013
5.767439	479.620347	6.869018
5.771805	476.818887	6.874022
5.707552	474.109503	6.879027
5.565054	477.127037	6.884032
5.790127	466.891371	6.889037
5.663490	476.881239	6.894042
5.776938	472.768355	6.899046
5.703185	468.791455	6.904051
5.792997	473.003695	6.909056
5.878915	475.766136	6.914061
5.903210	472.813570	6.919066
5.677998	471.709356	6.924070
5.928410	464.633044	6.929075
5.829264	471.641691	6.934080
5.886913	467.374848	6.939085
5.610936	475.428681	6.944090
5.748511	466.721491	6.949094
5.944647	469.007853	6.954099
5.644917	473.417603	6.959104
5.632298	470.462665	6.964109
5.636683	470.828106	6.969114
5.431899	483.521049	6.974118
5.998400	471.515936	6.979123
5.793850	476.501945	6.984128
5.573426	465.586212	6.989133
5.447402	479.760758	6.994138
5.513200	478.807077	6.999142
5.604246	472.200374	7.004147
5.700194	481.179123	7.009152
5.796375	468.072197	7.014157
5.934514	481.523761	7.019162
5.771682	473.800122	7.024166
5.790982	469.466021	7.029171
5.514686	472.888944	7.034176
5.676402	477.146507	7.039181
5.644656	475.364168	7.044186
5.556020	474.760486	7.049190
5.580468	492.351135	7.054195
5.615261	514.402932	7.059200
5.778326	505.430617	7.064205
6.008517	504.699940	7.069210
6.139749	496.015887	7.074214
6.193619	477.978520	7.079219
5.988216	477.223474	7.084224
6.085628	476.314091	7.089229
5.980206	470.459619	7.094234
6.393058	478.392287	7.099238
6.115252	462.687552	7.104243
5.738765	476.961587	7.109248
5.959735	471.665018	7.114253
5.997442	473.002560	7.119258
5.931209	469.137885	7.124262
5.926048	451.366273	7.129267
5.993909	451.122871	7.134272
6.118217	443.339859	7.139277
5.850037	447.251031	7.144282
6.038137	441.256795	7.149286
5.997568	442.295896	7.154291
5.677023	444.684386	7.159296
5.934823	444.950241	7.164301
5.719067	449.336410	7.169306
5.491917	447.973215	7.174310
5.874957	445.459335	7.179315
5.491107	440.847247	7.184320
6.088188	444.834977	7.189325
5.711976	447.187692	7.194330
5.847482	438.419686	7.199334
5.734496	445.304316	7.204339
5.647660	442.292604	7.209344
6.199868	436.283663	7.214349
5.862210	432.318503	7.219354
5.923519	439.125724	7.224358
6.009162	435.590921	7.229363
5.989126	443.235306	7.234368
6.003050	434.901254	7.239373
5.475802	417.432022	7.244378
5.555179	417.958110	7.249382
5.681822	432.526498	7.254387
5.176193	451.340758	7.259392
5.558769	446.013885	7.264397
5.641410	444.791601	7.269402
5.861938	450.072093	7.274406
5.529297	441.382394	7.279411
5.392240	441.270607	7.284416
5.599131	437.488984	7.289421
5.663370	448.166330	7.294426
5.495492	432.427636	7.299430
5.805338	437.896001	7.304435
5.421405	450.669495	7.309440
5.757588	447.236274	7.314445
5.646008	447.516524	7.319450
5.327246	456.792054	7.324454
5.640408	458.834464	7.329459
5.704005	471.444673	7.334464
5.571610	465.867195	7.339469
5.893303	470.325798	7.344474
5.764308	472.380448	7.349478
6.042753	463.101528	7.354483
5.860010	469.564955	7.359488
5.647361	463.170362	7.364493
5.624407	464.047689	7.369498
5.766342	470.789673	7.374502
6.051793	473.268452	7.379507
6.068677	474.513141	7.384512
5.855343	451.257208	7.389517
5.691104	453.975028	7.394522
5.756822	443.875287	7.399526
5.604807	438.619178	7.404531
5.745099	457.119282	7.409536
6.045841	461.679627	7.414541
5.961518	445.272313	7.419546
5.465689	442.204988	7.424550
5.884305	440.763082	7.429555
5.710068	437.534365	7.434560
6.008253	441.174540	7.439565
5.863493	442.826660	7.444570
5.573869	440.234128	7.449574
5.955403	434.569192	7.454579
5.811841	440.157630	7.459584
5.659217	442.856751	7.464589
5.853090	443.777701	7.469594
5.427114	448.977577	7.474598
5.898718	447.474799	7.479603
5.572832	450.284112	7.484608
5.876684	443.100883	7.489613
5.885544	438.284052	7.494618
5.864004	444.371288	7.499622
5.785401	444.865519	7.504627
5.721871	447.452994	7.509632
5.857377	435.808970	7.514637
6.068767	437.356530	7.519642
5.909706	440.859492	7.524646
5.940801	443.903333	7.529651
5.964280	444.424667	7.534656
5.744450	436.125769	7.539661
5.830468	438.735249	7.544666
5.828745	445.798992	7.549670
6.176451	444.405336	7.554675
5.931010	450.618254	7.559680
6.133634	439.878372	7.564685
6.042001	443.814774	7.569690
5.818384	430.705974	7.574694
5.822712	418.374449	7.579699
5.367814	421.369503	7.584704
5.473280	427.433136	7.589709
5.793001	440.952279	7.594714
5.350101	452.937107	7.599718
5.462560	444.888662	7.604723
5.669068	453.513414	7.609728
5.764807	444.271272	7.614733
5.911620	446.497715	7.619738
6.042176	440.116950	7.624742
5.749830	438.771458	7.629747
5.861027	447.338579	7.634752
5.901471	435.260364	7.639757
6.103095	447.449073	7.644762
5.658662	440.980979	7.649766
5.888132	444.538206	7.654771
5.841384	456.217276	7.659776
5.554399	442.596602	7.664781
5.580624	443.112153	7.669786
5.688378	452.741334	7.674790
6.022095	444.735187	7.679795
5.688843	446.239730	7.684800
5.866554	447.036862	7.689805
6.060810	444.820255	7.694810
5.998659	445.638160	7.699814
5.996374	418.396009	7.704819
5.844195	422.977072	7.709824
5.591572	408.112044	7.714829
5.709911	413.208356	7.719834
5.532773	416.293580	7.724838
5.694720	412.850342	7.729843
5.445526	421.235187	7.734848
5.684080	435.320117	7.739853
5.850076	448.433536	7.744858
5.660061	451.852626	7.749862
5.878330	438.183418	7.754867
5.866667	447.523139	7.759872
5.761769	443.430631	7.764877
5.898968	445.522700	7.769882
5.537882	432.946980	7.774886
5.849005	436.481607	7.779891
5.871692	447.471709	7.784896
5.579990	431.727470	7.789901
5.887872	435.058980	7.794906
5.710668	435.367068	7.799910
5.810910	434.644493	7.804915
5.688578	435.554061	7.809920
6.040500	438.318033	7.814925
5.855493	423.282541	7.819930
5.555293	425.528339	7.824934
5.640166	421.242792	7.829939
5.345327	426.553952	7.834944
5.526051	441.962740	7.839949
5.870310	434.283818	7.844954
5.556215	445.757911	7.849958
5.909605	448.535258	7.854963
5.933683	445.910711	7.859968
5.866035	443.871465	7.864973
5.871792	446.313869	7.869978
5.602829	445.977644	7.874982
6.051017	446.074428	7.879987
5.582489	447.347987	7.884992
5.470528	433.182298	7.889997
5.965479	448.723178	7.895002
5.442051	450.078055	7.900006
5.767508	449.152224	7.905011
5.795689	450.220988	7.910016
5.740545	445.535130	7.915021
5.705822	445.068355	7.920026
5.337163	446.844577	7.925030
5.644935	440.753168	7.930035
5.817372	452.417254	7.935040
5.654948	438.643148	7.940045
5.789167	451.002077	7.945050
5.415953	439.544115	7.950054
5.795144	440.624021	7.955059
5.891158	443.749861	7.960064
5.627918	444.330512	7.965069
5.661822	442.160981	7.970074
6.039864	438.590389	7.975078
6.162331	446.383456	7.980083
5.624541	448.722078	7.985088
5.974714	448.703269	7.990093
6.011017	446.095445	7.995098
5.884821	446.785620	8.000102
5.915873	437.751138	8.005107
5.872008	449.535696	8.010112
5.858482	445.831248	8.015130
5.853790	453.880739	8.020147
5.566336	451.682742	8.025165
5.962662	451.160559	8.030182
5.851890	452.883405	8.035200
5.496862	453.284002	8.040218
5.917580	443.222471	8.045235
5.636713	447.621314	8.050253
5.737767	440.823303	8.055270
5.463877	450.910919	8.060288
5.595948	453.864914	8.065306
5.685506	449.500512	8.070323
5.556557	449.435359	8.075341
5.993513	446.011980	8.080358
5.722428	446.429975	8.085376
5.459693	450.773655	8.090394
5.840229	443.252446	8.095411
5.584966	445.200383	8.100429
5.981387	448.360586	8.105446
5.998036	449.260423	8.110464
5.918490	449.579384	8.115482
6.402200	442.586719	8.120499
5.637446	451.997997	8.125517
5.923553	452.695943	8.130534
6.068564	457.722642	8.135552
5.684433	453.441794	8.140570
5.827020	449.707736	8.145587
5.881093	447.463422	8.150605
5.435010	445.553878	8.155622
5.401507	456.129212	8.160640
5.564691	456.573911	8.165658
5.895155	463.708918	8.170675
5.932636	481.821763	8.175693
6.047756	480.811143	8.180710
6.058807	485.409672	8.185728
6.048543	482.454603	8.190746
6.065061	468.887016	8.195763
5.748278	459.161753	8.200781
5.733850	464.745722	8.205798
5.883633	474.974797	8.210816
5.811892	477.177170	8.215834
5.936198	474.998382	8.220851
5.883181	485.812383	8.225869
5.981814	485.552077	8.230886
5.915834	482.530057	8.235904
6.052573	480.961763	8.240922
6.257778	477.356100	8.245939
5.733661	479.865648	8.250957
5.761319	477.792424	8.255974
5.841684	477.793391	8.260992
6.015913	483.183541	8.266010
6.038158	479.749107	8.271027
5.767423	487.286804	8.276045
5.678026	480.215019	8.281062
6.117400	486.519266	8.286080
5.859144	481.525490	8.291098
6.007781	478.188032	8.296115
5.626790	487.640895	8.301133
5.938574	483.547537	8.306150
5.762070	490.817288	8.311168
6.070390	505.360960	8.316186
6.330829	501.276100	8.321203
6.304352	503.118841	8.326221
6.264702	499.098829	8.331238
5.575808	486.344048	8.336256
5.947182	500.992031	8.341274
6.281318	507.665460	8.346291
6.069633	520.100133	8.351309
6.295279	511.664251	8.356326
6.369783	519.908718	8.361344
6.091122	502.792989	8.366362
6.194118	487.952298	8.371379
5.882902	491.469826	8.376397
6.171277	503.716572	8.381414
6.134921	508.095218	8.386432
6.209544	517.114413	8.391450
6.224686	498.937511	8.396467
6.130022	497.932495	8.401485
6.304181	496.096212	8.406502
6.241816	489.830125	8.411520
6.043492	491.902094	8.416538
6.253514	485.142708	8.421555
5.766399	492.798121	8.426573
6.046372	495.778221	8.431590
6.340387	500.435600	8.436608
6.113769	512.223574	8.441626
6.497758	505.529067	8.446643
6.174937	505.588333	8.451661
6.077391	501.936149	8.456678
6.379645	507.500763	8.461696
6.345916	506.304568	8.466714
6.290088	501.291635	8.471731
5.885682	503.819551	8.476749
6.300817	499.666361	8.481766
6.544177	504.243553	8.486784
6.558764	505.078582	8.491802
6.419124	475.940131	8.496819
6.251970	483.707506	8.501837
6.005330	484.067324	8.506854
5.917059	474.969912	8.511872
5.710126	496.783215	8.516890
6.466787	502.468828	8.521907
6.306025	504.377504	8.526925
6.453641	511.514072	8.531942
6.779045	507.189335	8.536960
6.290092	512.846582	8.541978
6.502342	503.985787	8.546995
6.493114	508.386908	8.552013
6.072482	491.503937	8.557030
6.358459	499.414776	8.562048
6.223351	501.346563	8.567066
6.155172	506.120608	8.572083
6.250215	496.634783	8.577101
6.433316	507.074292	8.582119
6.650844	499.781411	8.587136
6.497548	505.998582	8.592154
6.381221	503.384276	8.597171
6.398177	508.601673	8.602189
6.203931	517.566380	8.607207
5.930197	501.274976	8.612224
6.186566	512.600520	8.617242
6.487371	504.101019	8.622259
6.604089	511.508629	8.627277
6.366733	511.828921	8.632295
6.619195	512.816674	8.637312
6.345398	512.878648	8.642330
6.718504	506.733936	8.647347
6.469086	512.576896	8.652365
6.381523	512.609410	8.657383
6.723463	509.052549	8.662400
6.343810	515.519986	8.667418
6.603589	509.883964	8.672435
6.561128	507.571971	8.677453
6.447186	501.981891	8.682471
6.798779	505.160946	8.687488
6.775409	499.746013	8.692506
6.565167	479.387126	8.697523
6.267733	482.106364	8.702541
6.332405	473.049174	8.707559
6.540573	481.212633	8.712576
6.109780	487.058652	8.717594
6.462983	496.404118	8.722611
6.906871	502.885762	8.727629
6.638392	493.932343	8.732647
6.564452	477.785426	8.737664
6.202706	490.276418	8.742682
6.671995	494.934101	8.747699
6.403879	505.833927	8.752717
6.532929	503.483693	8.757735
6.808621	495.416671	8.762752
6.643602	513.338100	8.767770
6.480520	497.719470	8.772787
6.594521	495.215440	8.777805
6.557177	503.959684	8.782823
6.558823	503.999472	8.787840
6.496172	510.918711	8.792858
6.620824	505.348960	8.797875
6.436505	511.387031	8.802893
6.441353	516.457430	8.807911
6.899197	505.300023	8.812928
6.580959	517.543299	8.817946
6.334671	512.586898	8.822963
6.363922	512.565426	8.827981
6.455153	512.680137	8.832999
6.594790	505.446212	8.838016
6.534706	516.446824	8.843034
6.630959	502.895728	8.848051
6.604938	499.584628	8.853069
6.674740	502.839474	8.858087
6.585100	508.886668	8.863104
6.663629	519.640724	8.868122
6.548707	516.492363	8.873139
6.748592	508.513472	8.878157
6.396124	509.178589	8.883175
6.831780	510.278516	8.888192
6.485269	510.525748	8.893210
6.825682	506.094989	8.898227
6.369202	511.965151	8.903245
6.640848	529.793428	8.908263
6.946097	523.808359	8.913280
6.530729	521.582521	8.918298
6.711067	538.757864	8.923315
6.713976	542.304879	8.928333
6.716936	539.396817	8.933351
7.094866	534.870475	8.938368
7.058002	540.655810	8.943386
6.904852	521.466073	8.948403
6.856431	515.430523	8.953421
6.524066	509.546318	8.958439
6.550191	505.014660	8.963456
6.352960	521.053181	8.968474
7.065052	524.773290	8.973491
7.084220	530.143860	8.978509
6.902118	529.315515	8.983527
6.718940	536.493879	8.988544
6.907641	549.288231	8.993562
6.802634	544.825123	8.998579
6.788686	537.886871	9.003597
6.823529	537.999307	9.008615
6.781331	534.013760	9.013632
6.649465	540.916718	9.018650
6.754039	530.379367	9.023667
7.126267	533.856564	9.028685
6.900547	541.411634	9.033703
7.027902	529.515092	9.038720
6.838739	539.066331	9.043738
6.964316	536.876104	9.048755
6.808326	541.436567	9.053773
6.912428	544.686530	9.058791
6.805828	527.334423	9.063808
6.784289	536.680357	9.068826
6.432921	543.966884	9.073843
6.785792	539.789350	9.078861
6.914758	538.203048	9.083879
6.887578	532.184053	9.088896
6.896934	533.613413	9.093914
6.723470	542.651853	9.098931
7.061769	541.106473	9.103949
6.823921	531.013197	9.108967
7.055116	536.806896	9.113984
6.967990	539.364557	9.119002
6.731225	541.339165	9.124019
7.065827	542.844581	9.129037
6.684275	536.884067	9.134055
7.200882	535.523123	9.139072
7.248109	543.014888	9.144090
7.050105	536.949773	9.149107
7.276036	530.954216	9.154125
6.705553	540.267437	9.159143
7.114638	536.676028	9.164160
7.217441	539.662837	9.169178
6.928318	542.540738	9.174195
7.287728	538.021792	9.179213
6.811268	552.163802	9.184231
7.170845	536.871157	9.189248
7.122767	544.025185	9.194266
6.812624	540.495197	9.199283
7.111160	530.335345	9.204301
7.077124	540.443534	9.209319
7.218553	531.770029	9.214336
7.361607	541.995539	9.219354
7.008966	544.195816	9.224371
7.292957	533.437428	9.229389
6.885185	540.424259	9.234407
7.120065	542.867975	9.239424
7.224746	533.763773	9.244442
7.325008	537.730265	9.249459
7.032481	532.056959	9.254477
7.070223	542.123147	9.259495
7.467969	539.455205	9.264512
7.209710	542.752573	9.269530
6.977335	538.393819	9.274547
7.229659	529.708645	9.279565
7.018462	545.864850	9.284583
7.289773	554.320431	9.289600
7.266202	568.019180	9.294618
7.479298	562.979609	9.299635
7.210126	540.411061	9.304653
7.024639	545.666913	9.309671
7.160310	547.631619	9.314688
7.546000	548.883317	9.319706
6.926106	539.969560	9.324723
7.445215	540.875565	9.329741
7.424767	550.480364	9.334759
7.282230	539.120204	9.339776
7.312302	527.652146	9.344794
7.329463	526.819150	9.349811
7.376603	522.966046	9.354829
7.152341	527.355736	9.359847
7.253140	531.784507	9.364864
7.324187	535.065137	9.369882
7.180841	551.709881	9.374899
7.574441	545.759975	9.379917
7.249937	542.626825	9.384935
7.416192	548.623198	9.389952
7.211850	541.003922	9.394970
7.264710	560.044562	9.399987
7.612692	553.712666	9.405005
7.462180	551.247704	9.410023
7.278402	542.436914	9.415040
7.320793	540.358880	9.420058
7.087612	548.059667	9.425075
7.588419	555.337364	9.430093
7.523124	555.741363	9.435111
7.485128	549.214344	9.440128
7.249355	551.597619	9.445146
7.589066	557.478664	9.450163
7.542919	542.577977	9.455181
7.337609	544.075559	9.460199
7.281109	545.818560	9.465216
7.530821	552.888245	9.470234
7.384378	564.342335	9.475251
7.411607	568.978168	9.480269
7.499719	572.545330	9.485287
7.883520	558.807406	9.490304
7.854387	549.371243	9.495322
7.786689	536.838142	9.500339
7.662992	524.030485	9.505357
7.040436	530.307654	9.510375
7.107938	537.046505	9.515392
7.403744	531.660988	9.520410
7.352022	544.018015	9.525427
7.850857	559.066375	9.530445
7.680522	544.232704	9.535463
7.373660	531.585677	9.540480
7.727841	540.409982	9.545498
7.433415	530.280999	9.550515
7.416648	537.177692	9.555533
7.336856	531.810868	9.560551
7.480386	557.253763	9.565568
7.354776	562.966407	9.570586
7.058498	568.714595	9.575603
7.598056	559.680090	9.580621
7.570809	565.558324	9.585639
7.449595	567.798428	9.590656
7.494338	563.112893	9.595674
7.125052	564.389615	9.600691
7.793845	560.711694	9.605709
7.596543	564.740852	9.610727
7.693767	562.472645	9.615744
7.588695	562.889726	9.620762
7.161909	568.397535	9.625779
7.174717	565.233918	9.630797
7.618896	581.479459	9.635815
7.961715	585.840023	9.640832
8.226509	579.942336	9.645850
7.633758	569.431652	9.650867
7.671033	565.859680	9.655885
7.693379	573.430379	9.660903
7.604826	574.641718	9.665920
7.798368	566.712073	9.670938
7.595831	570.065176	9.675955
7.866024	570.331934	9.680973
7.879853	561.796069	9.685991
7.595837	565.541574	9.691008
7.734634	562.132898	9.696026
7.766436	572.272329	9.701043
7.711233	566.950434	9.706061
7.965280	574.464656	9.711079
7.747086	580.180433	9.716096
7.985105	567.029006	9.721114
7.909785	573.377377	9.726131
7.608851	572.469106	9.731149
7.843504	569.519131	9.736167
7.292862	571.722083	9.741184
8.107917	577.252987	9.746202
8.098929	589.897049	9.751219
7.688618	586.062989	9.756237
8.017455	572.076888	9.761255
8.039199	574.502755	9.766272
7.774957	557.213920	9.771290
7.626016	569.265631	9.776307
7.839156	581.694374	9.781325
7.933370	575.379097	9.786343
8.017381	585.797865	9.791360
7.937995	567.062755	9.796378
7.841694	570.130174	9.801395
8.011782	572.870825	9.806413
7.852390	575.570174	9.811431
7.660530	568.164551	9.816448
7.833731	580.215089	9.821466
7.778158	596.174722	9.826483
7.870950	593.609036	9.831501
8.177533	590.387124	9.836519
8.375845	593.083540	9.841536
8.476099	585.587612	9.846554
7.865805	568.180291	9.851571
7.835072	566.588937	9.856589
7.786651	559.279441	9.861607
7.925172	566.489976	9.866624
8.314801	581.543057	9.871642
7.386450	578.988795	9.876659
7.955773	579.691028	9.881677
8.149996	587.627735	9.886695
8.165435	592.273007	9.891712
8.281195	582.642763	9.896730
8.217659	591.858292	9.901747
7.843863	577.011630	9.906765
8.049513	583.893560	9.911783
8.117678	598.236354	9.916800
8.425707	588.361488	9.921818
7.924067	588.048226	9.926835
7.871854	589.353346	9.931853
7.904084	581.628345	9.936871
7.911407	590.281979	9.941888
7.988281	592.067660	9.946906
7.926284	594.169624	9.951923
8.113166	599.200065	9.956941
8.244299	595.607427	9.961959
8.155806	603.742521	9.966976
8.397803	593.171545	9.971994
8.570762	596.026087	9.977011
8.082124	591.951665	9.982029
8.446061	590.778782	9.987047
8.378825	597.948999	9.992064
8.453196	582.165775	9.997082
8.241894	576.481365	10.002099
8.198647	566.751484	10.007117
8.014185	559.296613	10.012135
7.740432	575.865936	10.017152
8.383957	574.769781	10.022170
8.454524	590.255008	10.027187
8.613748	593.835202	10.032205
8.218305	573.529100	10.037223
8.187358	571.944079	10.042240
8.059257	562.619958	10.047258
8.193163	577.460672	10.052275
7.774328	584.310191	10.057293
8.414900	589.600324	10.062311
8.467747	599.098338	10.067328
8.230969	592.163103	10.072346
8.282813	586.282566	10.077363
7.921154	591.941203	10.082381
8.283634	590.105219	10.087399
8.531430	590.515244	10.092416
8.462523	595.435885	10.097434
8.432245	592.197709	10.102451
7.788475	592.994524	10.107469
8.160799	588.676758	10.112487
8.064801	588.097717	10.117504
8.243182	594.849727	10.122522
8.157166	591.899307	10.127539
8.248686	591.897640	10.132557
8.204700	599.545668	10.137575
8.477018	590.538076	10.142592
8.310075	596.706562	10.147610
8.036423	596.227209	10.152627
8.548031	625.400162	10.157645
8.855156	620.401691	10.162663
8.562732	616.163088	10.167680
8.471166	598.666098	10.172698
8.557632	595.164512	10.177715
8.399193	601.519375	10.182733
8.565078	589.586291	10.187751
8.389658	592.659139	10.192768
8.168725	587.858938	10.197786
8.500008	601.092095	10.202803
8.395778	618.406374	10.207821
8.809065	615.148482	10.212839
8.790053	619.389257	10.217856
8.582960	608.603480	10.222874
8.729924	602.385160	10.227891
8.520772	593.760814	10.232909
8.582472	584.424147	10.237927
8.542353	598.010121	10.242944
8.309370	588.831886	10.247962
8.524185	594.898380	10.252979
8.226296	592.245624	10.257997
8.727734	609.411377	10.263015
8.716794	619.593741	10.268032
8.696438	626.508980	10.273050
8.923605	627.570610	10.278067
8.633181	614.880244	10.283085
8.481627	601.559453	10.288103
8.124583	607.556876	10.293120
8.515860	616.288473	10.298138
8.767026	613.823912	10.303155
8.736074	629.461216	10.308173
9.052211	627.706716	10.313191
8.680786	630.626016	10.318208
8.748665	625.317969	10.323226
8.823111	622.173660	10.328243
8.710675	622.588812	10.333261
8.832852	621.728186	10.338279
8.636002	621.562866	10.343296
8.993635	614.959285	10.348314
8.535270	606.460642	10.353331
8.709848	606.542460	10.358349
8.994539	618.959188	10.363367
8.217264	610.981824	10.368384
8.621184	619.046411	10.373402
9.036460	615.009499	10.378419
8.584129	627.335691	10.383437
8.746331	619.708237	10.388455
8.698808	612.632016	10.393472
8.722597	623.436544	10.398490
8.704308	624.350641	10.403507
8.947989	627.489326	10.408525
8.801440	616.147489	10.413543
8.567834	620.346245	10.418560
8.721185	627.085879	10.423578
9.122525	615.470260	10.428595
8.925209	622.706513	10.433613
8.786965	622.374018	10.438631
8.625026	629.887863	10.443648
8.662137	617.318446	10.448666
8.801442	618.879632	10.453683
8.613169	626.124231	10.458701
8.708862	623.305910	10.463719
8.780115	624.362650	10.468736
9.082670	623.740643	10.473754
8.940465	614.105461	10.478771
9.057029	630.038397	10.483789
9.161992	613.175734	10.488807
9.063379	622.932882	10.493824
8.687554	631.563179	10.498842
8.865579	627.060069	10.503859
8.771073	628.683987	10.508877
8.834017	616.506331	10.513895
9.171517	633.711264	10.518912
9.157306	645.024430	10.523930
9.361547	629.176743	10.528947
9.190481	633.302945	10.533965
8.888188	630.625717	10.538983
9.039814	631.690407	10.544000
8.852218	621.966679	10.549018
8.803869	614.547703	10.554035
8.648974	627.329729	10.559053
9.089404	638.102282	10.564071
9.173892	645.886334	10.569088
9.182081	661.517582	10.574106
9.443414	649.069269	10.579123
8.989183	650.883455	10.584141
9.440781	643.779687	10.589159
9.422976	636.946157	10.594176
9.225272	634.250034	10.599194
9.449253	624.836475	10.604211
8.803137	621.530004	10.609229
8.958332	615.274885	10.614247
9.100017	622.156204	10.619264
8.749279	635.494254	10.624282
9.201074	640.205859	10.629299
9.138285	644.781823	10.634317
9.508902	641.779794	10.639335
9.443683	649.081188	10.644352
9.234426	647.310935	10.649370
9.346697	637.866263	10.654387
8.968426	640.637494	10.659405
9.887578	639.892127	10.664423
9.483175	632.200231	10.669440
8.947178	634.204716	10.674458
9.166734	615.873167	10.679475
8.875909	622.281650	10.684493
8.984920	647.426295	10.689511
9.483437	644.791253	10.694528
9.066338	655.700696	10.699546
9.144831	651.208156	10.704563
9.230853	652.841551	10.709581
9.308507	648.345608	10.714599
8.920358	646.952987	10.719616
8.931391	646.479638	10.724634
9.247159	649.748114	10.729651
9.509746	652.935639	10.734669
9.193852	652.373520	10.739687
9.236044	649.641214	10.744704
9.016487	654.231723	10.749722
9.315501	661.205110	10.754739
9.285750	674.385718	10.759757
9.604647	678.971319	10.764775
10.099014	684.540010	10.769792
9.520320	673.760999	10.774810
9.525190	651.063648	10.779827
9.455201	657.302122	10.784845
9.350012	653.113209	10.789863
9.682873	645.786596	10.794880
9.594281	650.245188	10.799898
9.797527	644.193505	10.804915
9.562090	642.236654	10.809933
9.488278	653.950223	10.814951
9.421963	644.740617	10.819968
9.085717	646.959649	10.824986
9.286674	648.202382	10.830003
9.281871	652.273894	10.835021
9.469811	669.412693	10.840039
9.786849	673.627363	10.845056
9.377484	678.874861	10.850074
9.894732	669.541446	10.855091
9.472134	661.682087	10.860109
9.286043	662.748374	10.865127
9.892093	668.387931	10.870144
9.413163	679.886729	10.875162
9.609701	667.738876	10.880179
9.431668	679.552394	10.885197
9.555606	682.716823	10.890215
9.651857	680.968020	10.895232
9.589798	689.857792	10.900250
9.477429	682.519065	10.905267
9.655478	686.590622	10.910285
9.550365	686.111702	10.915303
9.876764	679.649872	10.920320
9.667673	689.741085	10.925338
10.059964	682.593974	10.930355
9.715867	690.650185	10.935373
9.645882	680.625072	10.940391
9.849437	680.162361	10.945408
9.596354	680.713789	10.950426
9.723873	677.815783	10.955443
9.737241	677.948310	10.960461
9.508089	678.583959	10.965479
9.905248	678.408068	10.970496
9.538108	688.858502	10.975514
9.645802	686.669641	10.980531
9.921112	680.463106	10.985549
9.794031	677.880471	10.990567
10.322833	677.822537	10.995584
9.910938	686.901723	11.000602
9.889500	677.601601	11.005619
9.584703	683.818734	11.010637
9.834542	683.048376	11.015655
9.965044	681.689154	11.020672
9.755855	684.596165	11.025690
10.273724	669.540155	11.030707
9.967342	680.069493	11.035725
9.992927	682.414038	11.040743
9.931266	670.934490	11.045760
9.959664	690.377939	11.050778
10.270007	689.753459	11.055795
9.884714	679.886850	11.060813
9.856174	683.898920	11.065831
10.018099	673.505115	11.070848
9.976516	682.613919	11.075866
9.776749	689.736837	11.080883
10.084802	686.523913	11.085901
10.027406	692.174524	11.090919
10.387937	683.415050	11.095936
9.856665	681.761890	11.100954
9.683535	678.494007	11.105971
9.829666	680.553646	11.110989
9.656516	687.836319	11.116007
10.032825	683.544440	11.121024
9.832667	686.475939	11.126042
9.905707	678.449858	11.131059
10.215463	674.570160	11.136077
10.055049	690.930102	11.141095
10.236813	675.982099	11.146112
10.127361	684.947428	11.151130
9.807984	683.923314	11.156147
10.172708	672.955016	11.161165
9.863704	676.616698	11.166183
10.614252	687.129286	11.171200
10.065506	689.952769	11.176218
10.131745	687.768016	11.181235
10.281520	675.060612	11.186253
10.032220	681.356738	11.191271
10.287757	686.618935	11.196288
10.337467	691.625076	11.201306
10.102834	680.160779	11.206323
10.390609	685.356617	11.211341
10.092225	685.680522	11.216359
10.271347	683.981772	11.221376
10.181425	687.265074	11.226394
10.590518	691.962902	11.231411
10.438898	686.071533	11.236429
10.297742	682.178313	11.241447
10.334495	679.398874	11.246464
10.399433	675.677817	11.251482
10.061902	677.291591	11.256499
10.237039	664.096166	11.261517
10.349087	681.770349	11.266535
10.422453	695.248841	11.271552
10.182770	691.754195	11.276570
10.349287	685.561736	11.281587
10.440104	697.466175	11.286605
10.259763	697.471338	11.291623
10.546728	695.606313	11.296640
10.192931	699.229357	11.301658
10.570527	691.713043	11.306675
10.742701	697.672866	11.311693
10.242505	704.088101	11.316711
10.102041	692.133820	11.321728
10.546708	701.274710	11.326746
10.519717	702.939815	11.331763
10.594353	698.871891	11.336781
10.038390	703.703147	11.341799
10.173629	700.268850	11.346816
10.242930	713.847632	11.351834
10.091237	698.502882	11.356851
10.494160	702.984818	11.361869
10.097045	703.378218	11.366887
10.413331	699.169498	11.371904
10.415715	700.322682	11.376922
10.579506	707.187386	11.381939
10.512418	703.929891	11.386957
10.470797	716.922748	11.391975
10.837840	720.615401	11.396992
10.809884	712.263920	11.402010
10.448595	712.254167	11.407027
10.740178	696.377382	11.412045
10.431253	702.151532	11.417063
10.746693	707.833320	11.422080
10.765617	727.285076	11.427098
10.721532	712.128388	11.432115
10.946250	699.050701	11.437133
10.727898	704.043363	11.442151
10.801739	692.891341	11.447168
10.639425	699.376602	11.452186
10.270680	700.143235	11.457203
10.811262	693.715220	11.462221
10.418446	703.216035	11.467239
10.383115	708.590573	11.472256
10.851301	720.672685	11.477274
10.732416	724.801294	11.482291
10.769130	728.456527	11.487309
10.838303	730.433645	11.492327
11.066948	727.028756	11.497344
10.924213	725.207716	11.502362
10.860238	728.072974	11.507379
11.116323	719.437069	11.512397
10.752785	711.993076	11.517415
10.610872	704.145875	11.522432
10.533074	707.232697	11.527450
10.770716	718.568776	11.532467
11.062933	712.892076	11.537485
10.963498	727.719212	11.542503
10.831977	723.892493	11.547520
10.868598	714.937439	11.552538
10.826959	726.361499	11.557555
11.448569	716.402936	11.562573
11.026719	729.083982	11.567591
10.910598	713.719941	11.572608
10.745562	721.460708	11.577626
10.394723	722.832216	11.582643
11.109082	726.329966	11.587661
11.265822	732.720680	11.592679
10.993734	727.312602	11.597696
10.996594	722.005841	11.602714
10.964987	728.752132	11.607731
11.032862	718.669129	11.612749
11.281844	734.185387	11.617767
11.138336	729.073322	11.622784
11.244743	725.646157	11.627802
11.083463	726.419379	11.632819
11.146650	722.801744	11.637837
11.153373	724.076252	11.642855
11.246818	717.014434	11.647872
11.050924	713.166095	11.652890
10.824281	717.331049	11.657907
11.056956	709.413551	11.662925
11.065710	721.957151	11.667943
11.197365	720.126895	11.672960
10.956348	723.753316	11.677978
11.084450	729.538570	11.682995
11.040484	720.259474	11.688013
10.761713	724.976730	11.693031
11.471742	721.647634	11.698048
11.091936	724.505350	11.703066
10.945072	729.259817	11.708083
11.142312	728.484388	11.713101
10.906941	725.788188	11.718119
10.956937	718.564282	11.723136
11.165302	718.149196	11.728154
11.119804	730.958859	11.733171
11.484814	729.444272	11.738189
11.273311	737.129752	11.743207
11.080484	731.503049	11.748224
11.464994	738.062730	11.753242
11.453577	748.331473	11.758259
11.511907	739.958211	11.763277
11.273990	728.046415	11.768295
11.608741	734.440722	11.773312
11.362858	724.077799	11.778330
10.893402	731.417823	11.783347
11.331612	735.361279	11.788365
11.290097	747.234915	11.793383
11.397682	756.371028	11.798400
11.880651	742.552943	11.803418
11.515261	750.665857	11.808435
11.740720	725.626093	11.813453
11.562612	722.246828	11.818471
11.257198	718.552835	11.823488
11.559442	715.858161	11.828506
11.235533	720.101421	11.833523
11.434569	709.910884	11.838541
11.365868	720.574111	11.843559
11.538495	741.152731	11.848576
11.778613	741.405576	11.853594
11.665477	751.169147	11.858611
11.849313	732.126879	11.863629
11.787849	723.216800	11.868647
11.548901	728.807728	11.873664
11.885190	718.207472	11.878682
11.683969	721.472599	11.883699
11.903289	717.849976	11.888717
12.031451	717.487538	11.893735
12.088423	714.361064	11.898752
12.198069	710.490871	11.903770
11.707709	726.863755	11.908787
11.881657	714.516469	11.913805
11.568226	695.551075	11.918823
11.565131	696.716189	11.923840
11.924224	704.487868	11.928858
11.546968	705.392123	11.933875
11.787678	699.967248	11.938893
12.012434	694.485573	11.943911
11.711647	700.359943	11.948928
11.955402	690.001393	11.953946
11.629057	696.980322	11.958963
11.528624	684.945406	11.963981
11.502086	696.443711	11.968999
11.787816	723.870500	11.974016
11.837163	716.355774	11.979034
11.688025	719.453624	11.984051
11.919887	716.595811	11.989069
11.612283	718.452257	11.994087
11.684550	729.769668	11.999104
11.517070	716.981699	12.004122
11.673841	726.515139	12.009139
11.694306	720.357479	12.014157
11.971176	724.227260	12.019175
11.942255	725.308862	12.024192
11.854921	720.844548	12.029210
11.854292	727.519571	12.034227
12.059698	722.343828	12.039245
11.850966	716.584732	12.044263
11.493305	721.913048	12.049280
12.006880	713.689994	12.054298
11.590255	720.365397	12.059315
11.581429	729.576673	12.064333
11.900244	744.176704	12.069351
11.475582	750.594804	12.074368
11.698098	740.536571	12.079386
12.062130	752.302509	12.084403
11.942982	754.276171	12.089421
12.403240	756.060982	12.094439
12.035057	752.144317	12.099456
11.807672	746.591831	12.104474
11.819832	750.786144	12.109491
12.213659	744.826085	12.114509
12.234185	752.286549	12.119527
11.926935	747.547636	12.124544
12.350587	740.075244	12.129562
12.124572	749.025267	12.134579
12.002630	737.059617	12.139597
11.943005	748.316996	12.144615
11.458338	742.995292	12.149632
12.204544	760.734232	12.154650
12.289817	776.257561	12.159667
12.428011	774.086471	12.164685
12.557680	766.021837	12.169703
12.279847	748.592132	12.174720
12.437662	747.616943	12.179738
12.229647	740.452679	12.184755
12.091496	742.524756	12.189773
12.336083	736.008737	12.194791
12.063821	743.933008	12.199808
12.492617	746.522590	12.204826
12.767428	758.932406	12.209843
12.441057	747.137992	12.214861
12.306098	742.460704	12.219879
12.087995	739.741564	12.224896
12.438389	730.088124	12.229914
12.363392	745.508441	12.234931
11.903442	744.179666	12.239949
12.483339	753.430865	12.244967
12.304421	772.638289	12.249984
12.466689	770.016780	12.255002
12.616305	774.450923	12.260019
12.766410	777.188227	12.265037
12.803659	758.991415	12.270055
12.255574	748.688752	12.275072
12.191146	754.152371	12.280090
12.617643	765.326118	12.285107
12.761784	766.259387	12.290125
12.807531	760.373889	12.295143
12.528374	746.862696	12.300160
12.726567	743.371118	12.305178
12.647540	744.492512	12.310195
12.370442	742.526800	12.315213
12.803245	736.176454	12.320231
12.550313	747.331204	12.325248
12.408966	741.494015	12.330266
12.303834	739.448255	12.335283
12.554629	752.219503	12.340301
12.899911	763.702350	12.345319
12.836598	771.302288	12.350336
12.461589	748.396847	12.355354
12.490384	750.660560	12.360371
12.469308	765.041710	12.365389
12.855179	772.732222	12.370407
12.876876	767.259343	12.375424
12.968384	770.149254	12.380442
12.929410	771.477786	12.385459
12.748784	755.014209	12.390477
12.937862	738.870906	12.395495
12.504248	739.402232	12.400512
12.572163	747.752040	12.405530
12.864112	761.613664	12.410547
12.766509	771.114059	12.415565
13.038828	776.780573	12.420583
12.836620	774.206031	12.425600
13.023778	769.580509	12.430618
13.041226	764.488629	12.435635
12.963220	758.323245	12.440653
12.826503	742.920068	12.445671
12.541628	756.883107	12.450688
12.750858	763.130504	12.455706
12.854288	762.302501	12.460723
12.419182	769.558513	12.465741
12.732255	766.717949	12.470759
12.713101	761.289630	12.475776
12.691582	773.791831	12.480794
12.729148	771.374032	12.485811
12.463226	771.286679	12.490829
13.087381	769.594933	12.495847
12.917615	768.876730	12.500864
12.960940	785.151857	12.505882
12.995960	789.780167	12.510899
13.064815	792.560060	12.515917
13.217717	794.248927	12.520935
13.304752	797.219501	12.525952
12.874624	776.527360	12.530970
13.244592	783.446537	12.535987
13.129920	792.347441	12.541005
13.425142	787.224518	12.546023
13.055150	780.625610	12.551040
13.185628	773.886357	12.556058
12.932005	770.145983	12.561075
13.035214	776.985713	12.566093
13.515386	787.817142	12.571111
13.322956	779.034617	12.576128
13.144690	764.733515	12.581146
13.217780	774.167067	12.586163
13.161455	776.280321	12.591181
13.815122	776.744595	12.596199
13.428514	773.641169	12.601216
13.277642	771.712422	12.606234
13.044846	767.660349	12.611251
12.852851	764.278256	12.616269
13.112926	781.162727	12.621287
13.103050	790.370670	12.626304
13.613833	788.615810	12.631322
13.713910	790.956697	12.636339
13.467911	802.763453	12.641357
13.381350	788.837675	12.646375
13.143311	791.454617	12.651392
13.100166	795.914779	12.656410
13.329589	785.596726	12.661427
13.382983	796.498436	12.666445
13.334107	793.383174	12.671463
13.367906	795.078378	12.676480
13.558250	797.742884	12.681498
13.662951	799.135025	12.686515
13.486944	798.307624	12.691533
13.553248	795.069357	12.696551
13.341440	793.649491	12.701568
13.381170	793.054463	12.706586
13.511514	790.980728	12.711603
13.266293	798.741110	12.716621
13.656966	799.158781	12.721639
13.718139	795.724917	12.726656
13.305460	797.051556	12.731674
13.589093	797.373965	12.736691
13.599559	797.440441	12.741709
13.716778	791.661988	12.746727
13.581321	795.708324	12.751744
13.473570	798.904843	12.756762
13.967205	788.700116	12.761779
13.328942	804.076760	12.766797
13.410735	798.094732	12.771815
14.000815	802.446107	12.776832
13.620529	804.746859	12.781850
13.529714	799.179612	12.786867
13.590158	814.384668	12.791885
13.630884	820.570624	12.796903
13.949513	827.487693	12.801920
13.853037	824.440145	12.806938
13.930769	823.016031	12.811955
14.063141	829.348225	12.816973
14.032946	811.956180	12.821991
13.932231	811.185992	12.827008
13.585201	801.038574	12.832026
13.748294	793.023900	12.837043
14.006342	800.867869	12.842061
13.866379	796.756324	12.847079
14.147906	807.922612	12.852096
13.828390	799.764631	12.857114
14.221712	799.040191	12.862131
13.808679	796.758021	12.867149
13.792889	790.696097	12.872167
13.767560	793.987228	12.877184
13.735956	814.755661	12.882202
14.081604	818.992011	12.887219
13.699325	827.183348	12.892237
13.801867	827.700697	12.897255
13.721540	829.515978	12.902272
13.864624	829.820718	12.907290
14.198063	818.762621	12.912307
14.275453	832.203954	12.917325
13.961119	827.672084	12.922343
13.962497	822.060431	12.927360
14.070082	822.908424	12.932378
14.256099	822.245867	12.937395
14.286163	825.138482	12.942413
14.052127	829.020452	12.947431
14.096818	821.228508	12.952448
13.898677	823.967189	12.957466
14.247343	814.704907	12.962483
14.097609	826.993748	12.967501
14.410753	827.556140	12.972519
14.136959	824.087584	12.977536
14.071023	828.966076	12.982554
14.167085	815.392298	12.987571
13.864627	830.168115	12.992589
14.397982	843.634739	12.997607
14.650779	851.144974	13.002624
14.508546	847.603842	13.007642
14.469110	828.271278	13.012659
14.367096	828.194577	13.017677
14.228116	814.305013	13.022695
14.470684	821.691343	13.027712
14.388305	830.441260	13.032730
14.487518	814.962726	13.037747
14.281854	821.767011	13.042765
14.495743	824.784692	13.047783
14.670846	831.412158	13.052800
14.477789	826.767298	13.057818
14.295286	818.563392	13.062835
14.224352	838.984450	13.067853
14.566263	855.581451	13.072871
14.670217	847.585202	13.077888
14.413335	854.518449	13.082906
15.119153	848.345281	13.087923
14.893388	837.143558	13.092941
14.449197	825.000109	13.097959
14.620410	822.537732	13.102976
14.696395	826.312856	13.107994
14.521731	815.159378	13.113011
14.194120	819.902860	13.118029
14.230602	826.460762	13.123047
14.752906	836.906135	13.128064
14.658084	846.017158	13.133082
15.017743	850.708261	13.138099
15.332978	848.742873	13.143117
14.684590	822.065060	13.148135
14.674385	820.294108	13.153152
14.240586	822.694270	13.158170
14.719397	826.346396	13.163187
14.989440	835.783985	13.168205
15.172319	840.834262	13.173223
14.850731	824.653781	13.178240
14.550939	819.129399	13.183258
15.193262	815.109955	13.188275
14.527923	809.971286	13.193293
14.539680	817.326938	13.198311
15.025771	827.486584	13.203328
15.307727	838.960682	13.208346
14.922412	826.878345	13.213363
14.789536	819.999224	13.218381
14.995664	815.009936	13.223399
14.903346	811.718408	13.228416
14.733397	818.606931	13.233434
15.040848	832.580613	13.238451
15.074796	842.340357	13.243469
15.075634	842.329298	13.248487
15.039263	826.960993	13.253504
14.983185	837.625360	13.258522
14.874715	843.184488	13.263539
15.174621	845.953296	13.268557
15.088317	842.476916	13.273575
15.043173	843.270282	13.278592
15.163352	847.354614	13.283610
15.324168	840.242216	13.288627
15.109285	838.058326	13.293645
15.001430	838.859320	13.298663
14.983896	842.772762	13.303680
15.302273	843.062255	13.308698
15.537978	840.763991	13.313715
15.057472	833.905028	13.318733
15.069330	841.107533	13.323751
15.269404	848.799323	13.328768
14.767149	845.880771	13.333786
14.714638	855.284779	13.338803
14.951532	851.184829	13.343821
14.948819	845.714783	13.348839
15.143438	847.960894	13.353856
15.141878	855.409317	13.358874
15.422975	839.172330	13.363891
15.134632	838.935153	13.368909
15.119252	853.613853	13.373927
15.683279	862.697282	13.378944
15.524504	877.204089	13.383962
15.359575	868.197284	13.388979
15.510965	850.498763	13.393997
15.515947	863.656065	13.399015
15.300710	847.661483	13.404032
15.170225	853.418739	13.409050
15.697732	866.504874	13.414067
15.740431	872.253538	13.419085
15.682645	861.912129	13.424103
15.850263	841.944110	13.429120
15.696782	846.516647	13.434138
15.383630	843.058934	13.439155
15.599367	834.670184	13.444173
15.668705	842.140718	13.449191
15.915252	833.618527	13.454208
15.844428	836.337309	13.459226
15.236673	839.911497	13.464243
15.241580	832.141095	13.469261
15.269156	839.760268	13.474279
15.617633	855.656216	13.479296
15.492999	871.677369	13.484314
15.586539	874.041398	13.489331
15.970251	863.015888	13.494349
15.682966	866.912195	13.499367
15.731165	865.601229	13.504384
15.605144	875.116629	13.509402
15.766444	866.314062	13.514419
15.944711	869.745899	13.519437
15.735252	877.514964	13.524455
15.819490	872.291916	13.529472
16.112855	871.264354	13.534490
15.651751	872.307692	13.539507
15.806902	866.764650	13.544525
15.989583	872.435413	13.549543
16.114306	863.579852	13.554560
16.273419	860.323449	13.559578
15.984328	857.072761	13.564595
15.833971	849.579229	13.569613
15.958534	864.557192	13.574631
16.173064	870.115205	13.579648
16.244357	864.738405	13.584666
15.912340	842.676844	13.589683
16.184646	836.575071	13.594701
15.407119	832.755299	13.599719
15.862024	846.809690	13.604736
16.067108	865.084001	13.609754
16.031206	867.495839	13.614771
15.998532	868.206043	13.619789
16.094695	865.320281	13.624807
16.271094	857.871847	13.629824
16.293051	872.092435	13.634842
16.162278	867.125453	13.639859
16.146011	862.424538	13.644877
16.188533	870.990812	13.649895
16.027224	863.192014	13.654912
15.972342	866.625450	13.659930
16.007015	863.809710	13.664947
16.254927	863.422322	13.669965
16.072680	864.074226	13.674983
16.685132	865.150024	13.680000
16.365220	862.048920	13.685018
16.403772	864.515749	13.690035
16.323614	869.580458	13.695053
16.056613	869.205895	13.700071
16.662574	853.972923	13.705088
16.399561	862.858275	13.710106
16.164948	865.697879	13.715123
16.408488	855.038089	13.720141
16.170460	865.282625	13.725159
15.838207	861.751696	13.730176
16.186280	869.335135	13.735194
16.502238	886.364399	13.740211
16.741272	887.633521	13.745229
16.589779	890.786517	13.750247
16.094926	880.792652	13.755264
16.401137	880.387736	13.760282
16.377633	887.927206	13.765299
16.746954	877.346174	13.770317
16.623648	892.949038	13.775335
16.424713	880.626751	13.780352
16.478303	890.595468	13.785370
16.299976	888.815734	13.790387
16.446869	892.279541	13.795405
16.426982	895.931194	13.800423
16.588039	884.630740	13.805440
16.789229	888.082800	13.810458
16.801767	889.473281	13.815475
16.724133	892.625464	13.820493
16.753159	898.048070	13.825511
16.817959	887.206446	13.830528
16.862391	886.821650	13.835546
16.430531	900.303275	13.840563
16.622222	890.728374	13.845581
16.289920	891.097266	13.850599
16.730634	898.280358	13.855616
16.692081	921.288171	13.860634
16.845236	910.481111	13.865651
17.231124	914.654134	13.870669
17.330684	900.883648	13.875687
17.070619	893.185830	13.880704
17.001225	891.505376	13.885722
16.944077	881.154400	13.890739
17.120565	883.457059	13.895757
16.679434	890.897975	13.900775
16.742168	880.317710	13.905792
17.014975	890.354453	13.910810
16.911033	913.601024	13.915827
17.458904	907.638624	13.920845
17.151325	901.152552	13.925863
16.966186	882.590863	13.930880
17.095865	883.443861	13.935898
17.060189	886.788692	13.940915
17.324638	895.143437	13.945933
17.211359	898.740873	13.950951
17.233788	887.376368	13.955968
17.239968	881.502887	13.960986
17.206187	878.789026	13.966003
17.565373	872.407904	13.971021
17.111963	880.598056	13.976039
17.264822	880.124443	13.981056
17.048337	876.538516	13.986074
16.912982	880.106928	13.991091
17.395949	889.588817	13.996109
17.301293	912.155927	14.001127
17.401340	910.718661	14.006144
17.060642	912.966418	14.011162
17.201591	908.858720	14.016179
17.691373	911.203990	14.021197
17.482073	918.729360	14.026215
17.262928	920.446778	14.031232
17.273439	913.113184	14.036250
17.283696	911.264820	14.041267
17.300086	906.819496	14.046285
17.412763	909.201226	14.051303
17.465872	907.784724	14.056320
17.681569	909.025431	14.061338
17.612219	909.828320	14.066355
17.552645	900.282815	14.071373
17.470672	917.024083	14.076391
17.501629	915.375039	14.081408
17.371592	910.250054	14.086426
17.286420	913.026734	14.091443
17.404842	911.168728	14.096461
17.265084	914.076095	14.101479
17.301766	929.259215	14.106496
18.052920	921.684872	14.111514
17.893003	940.469691	14.116531
17.975583	921.501042	14.121549
18.128848	910.210127	14.126567
17.924143	911.410215	14.131584
17.555914	905.633366	14.136602
17.382097	910.407705	14.141619
17.471945	900.192999	14.146637
17.580678	915.566528	14.151655
18.029080	926.409614	14.156672
18.330920	915.735011	14.161690
17.749970	923.956934	14.166707
17.922593	903.421891	14.171725
17.876734	901.471408	14.176743
17.711540	900.513476	14.181760
18.119169	910.964109	14.186778
17.784847	930.967506	14.191795
18.027602	926.282733	14.196813
18.008779	933.106127	14.201831
17.912790	938.881323	14.206848
18.258595	928.864756	14.211866
18.268709	939.029671	14.216883
18.166335	926.421685	14.221901
17.765776	906.820487	14.226919
18.102327	925.809682	14.231936
18.393406	924.106541	14.236954
17.824714	915.349235	14.241971
18.274912	925.704250	14.246989
18.405389	928.855443	14.252007
18.114410	921.126905	14.257024
18.412452	906.005891	14.262042
17.998308	910.492087	14.267059
18.099537	922.568982	14.272077
18.210069	934.578996	14.277095
18.321157	933.311939	14.282112
18.463623	928.500865	14.287130
18.152828	928.798090	14.292147
18.158447	933.019912	14.297165
18.466569	929.087668	14.302183
18.046186	933.144214	14.307200
18.294800	925.321207	14.312218
18.527815	933.163877	14.317235
18.336994	923.528677	14.322253
18.221690	926.687104	14.327271
18.133910	927.038342	14.332288
18.564366	921.396153	14.337306
18.417730	937.274173	14.342323
18.594978	931.412109	14.347341
18.645350	931.911722	14.352359
18.485222	933.161121	14.357376
18.468152	922.980639	14.362394
18.495525	928.994842	14.367411
18.812912	927.285376	14.372429
18.793518	924.133317	14.377447
18.402987	931.419423	14.382464
18.451077	934.420487	14.387482
18.408410	933.372582	14.392499
18.445562	927.119956	14.397517
18.643718	927.520298	14.402535
18.506118	925.244074	14.407552
18.604637	927.080144	14.412570
18.708789	947.801080	14.417587
18.722461	952.575095	14.422605
18.531294	965.143728	14.427623
18.583089	966.356857	14.432640
18.763297	957.286159	14.437658
18.882406	958.851511	14.442675
18.859052	960.742410	14.447693
19.124146	962.704439	14.452711
18.688035	957.749406	14.457728
18.964521	952.653546	14.462746
19.150839	957.281656	14.467763
19.045281	957.468128	14.472781
19.184994	948.858058	14.477799
19.194493	959.955726	14.482816
19.295338	952.209534	14.487834
19.176074	946.381602	14.492851
19.016007	941.480074	14.497869
19.276088	924.573672	14.502887
18.726791	928.192528	14.507904
18.830360	925.884637	14.512922
18.760723	942.743176	14.517939
19.019153	950.975724	14.522957
19.412067	950.887932	14.527975
18.968179	959.627313	14.532992
19.426640	951.410899	14.538010
19.368935	950.509178	14.543027
19.162484	953.077217	14.548045
19.242162	948.389128	14.553063
19.059815	958.115865	14.558080
19.359136	953.174485	14.563098
19.172420	957.084475	14.568115
19.378671	958.931449	14.573133
19.355226	951.396382	14.578151
19.225503	955.994543	14.583168
19.416911	952.273737	14.588186
19.549234	951.991310	14.593203
19.212422	959.503169	14.598221
19.439572	947.220113	14.603239
19.347647	961.502946	14.608256
19.490748	947.121691	14.613274
19.406707	955.516851	14.618291
19.437784	947.949136	14.623309
19.786020	946.049922	14.628327
19.487448	956.837198	14.633344
19.433311	950.211899	14.638362
19.611981	950.167851	14.643379
19.147463	957.007577	14.648397
19.447238	949.783541	14.653415
19.592349	954.994828	14.658432
19.471449	952.601666	14.663450
19.599655	953.137602	14.668467
19.452517	968.499618	14.673485
19.895859	975.220913	14.678503
19.402263	986.581425	14.683520
19.922937	981.665979	14.688538
19.906129	978.739062	14.693555
19.988755	984.252425	14.698573
19.879736	975.015049	14.703591
19.643599	981.431553	14.708608
20.021863	971.659967	14.713626
20.036815	980.551720	14.718643
19.808158	977.548076	14.723661
19.717897	969.860683	14.728679
19.584048	981.985606	14.733696
20.090950	978.488919	14.738714
20.090536	977.824157	14.743731
20.183524	976.245146	14.748749
20.168482	974.786776	14.753767
20.046842	976.064843	14.758784
19.914820	971.712182	14.763802
20.329094	981.985786	14.768819
19.998573	986.020773	14.773837
20.421737	977.724760	14.778855
20.365335	983.458380	14.783872
20.171626	959.385248	14.788890
20.007027	943.813266	14.793907
20.110927	951.206873	14.798925
20.297007	956.834586	14.803943
20.224957	968.422515	14.808960
20.340932	969.317550	14.813978
20.025318	966.389722	14.818995
19.861685	978.048726	14.824013
20.203198	964.338903	14.829031
19.981682	981.760013	14.834048
20.272094	975.333546	14.839066
20.468237	975.918075	14.844083
20.245193	982.263910	14.849101
20.331485	975.526768	14.854119
20.026869	983.354161	14.859136
20.148672	971.592446	14.864154
20.244312	972.690840	14.869171
20.270021	982.502034	14.874189
20.314973	966.983122	14.879207
20.208469	987.094531	14.884224
20.652621	1000.562285	14.889242
20.700669	1003.307867	14.894259
20.738724	1013.542611	14.899277
20.944978	1002.633785	14.904295
20.524545	985.714020	14.909312
20.323558	976.493840	14.914330
20.776298	986.196140	14.919347
20.567173	1003.015246	14.924365
20.477196	1006.375393	14.929383
20.636668	1002.581520	14.934400
20.473793	1006.714732	14.939418
20.721104	1005.017255	14.944435
20.609103	1008.905832	14.949453
20.835681	998.767629	14.954471
20.982131	1000.995362	14.959488
20.946727	1001.376903	14.964506
21.216506	997.200607	14.969523
20.824236	1009.346295	14.974541
21.010836	1000.159163	14.979559
20.731530	1006.939110	14.984576
20.826039	998.911671	14.989594
21.082567	997.595725	14.994611
20.885015	1001.663420	14.999629
20.853782	993.173754	15.004647
21.064420	994.114530	15.009664
20.761818	1002.395911	15.014682
21.390350	991.248673	15.019699
21.115604	999.408910	15.024717
20.977492	993.121894	15.029735
21.174956	999.039852	15.034752
20.899339	1003.418494	15.039770
20.942884	997.045494	15.044787
21.066407	1006.910978	15.049805
21.143888	990.567396	15.054823
21.331725	1008.521911	15.059840
20.817453	1005.610829	15.064858
20.871000	1005.444590	15.069875
20.854729	1015.415114	15.074893
21.381236	1019.521970	15.079911
21.667011	1030.328281	15.084928
21.719873	1021.954590	15.089946
21.554802	1000.081294	15.094963
21.318223	1003.975538	15.099981
21.739069	986.760963	15.104999
21.553280	999.466918	15.110016
21.497873	992.532375	15.115034
21.353007	993.609967	15.120051
21.598479	992.786777	15.125069
21.589412	985.464657	15.130087
21.377661	990.957479	15.135104
21.545646	991.483681	15.140122
21.635172	993.237786	15.145139
21.537876	995.251165	15.150157
21.502670	983.854009	15.155175
21.704238	991.844036	15.160192
21.430459	989.291544	15.165210
21.421799	1003.672041	15.170227
21.659685	1012.428870	15.175245
21.814491	1017.300790	15.180263
22.158893	1017.074974	15.185280
22.072369	1012.969876	15.190298
21.910869	996.206429	15.195315
21.830948	989.748368	15.200333
21.549039	983.253287	15.205351
21.474687	988.445415	15.210368
21.456124	1014.640480	15.215386
21.667733	1013.793764	15.220403
21.858435	1014.015823	15.225421
22.009818	1015.147508	15.230439
22.133320	1020.899775	15.235456
22.185342	1019.857051	15.240474
22.385380	1012.312506	15.245491
22.234383	1019.170422	15.250509
22.136102	1006.415241	15.255527
21.901328	989.719444	15.260544
21.730802	1004.166900	15.265562
22.241268	1005.801702	15.270579
22.387137	1013.055716	15.275597
22.177796	1002.780252	15.280615
22.235913	996.646562	15.285632
21.984691	998.176787	15.290650
22.281413	1008.976547	15.295667
22.188410	1012.774581	15.300685
22.258377	1009.411652	15.305703
22.454790	1019.474515	15.310720
22.245876	1021.942190	15.315738
22.446086	1009.354502	15.320755
22.394137	1022.048549	15.325773
22.211686	1004.508277	15.330791
22.143653	1006.500670	15.335808
22.525421	1012.789675	15.340826
22.616413	1011.686170	15.345843
22.029167	1016.671907	15.350861
22.406333	1015.903284	15.355879
22.503353	1010.768621	15.360896
22.478357	1010.364217	15.365914
22.627051	1007.599253	15.370931
22.504520	1010.862433	15.375949
22.575096	1019.967430	15.380967
22.743195	1008.844847	15.385984
22.331167	1021.907954	15.391002
22.424184	1013.271329	15.396019
22.426819	1021.059282	15.401037
22.279038	1017.305258	15.406055
22.375712	1015.882320	15.411072
22.343215	1013.133185	15.416090
22.377403	1026.040916	15.421107
22.537011	1046.594147	15.426125
22.433032	1050.442431	15.431143
22.820232	1045.632134	15.436160
22.781769	1049.690428	15.441178
22.544427	1047.086225	15.446195
22.757596	1042.921653	15.451213
22.750250	1052.758837	15.456231
22.916075	1043.807394	15.461248
22.614685	1047.377747	15.466266
22.980060	1042.157301	15.471283
22.948050	1059.395549	15.476301
22.966647	1067.548192	15.481319
23.289298	1055.325218	15.486336
23.453156	1056.050131	15.491354
23.451171	1039.272428	15.496371
23.053115	1038.495560	15.501389
23.116808	1039.218947	15.506407
23.544487	1030.470601	15.511424
23.210014	1037.296309	15.516442
23.147550	1038.821266	15.521459
23.037489	1032.435892	15.526477
23.141264	1030.775566	15.531495
23.252349	1037.488915	15.536512
23.128166	1036.877714	15.541530
23.617184	1029.566009	15.546547
23.527779	1034.925993	15.551565
23.406922	1033.101294	15.556583
23.483796	1035.215754	15.561600
23.458263	1038.174306	15.566618
23.165510	1030.888903	15.571635
23.357242	1036.887350	15.576653
23.192267	1034.633358	15.581671
23.546264	1033.264263	15.586688
23.184341	1038.637484	15.591706
23.234208	1038.309263	15.596723
23.528527	1047.015430	15.601741
23.436118	1056.608050	15.606759
23.749344	1049.420322	15.611776
23.565194	1057.726606	15.616794
23.788319	1041.346650	15.621811
23.753561	1049.676222	15.626829
23.712605	1053.048340	15.631847
23.746884	1049.875164	15.636864
24.064046	1052.028970	15.641882
23.693071	1047.203668	15.646899
24.031253	1050.667725	15.651917
24.022601	1051.005468	15.656935
24.049029	1039.642552	15.661952
23.870867	1036.962019	15.666970
23.771694	1027.150561	15.671987
23.978805	1031.209524	15.677005
23.531107	1023.387203	15.682023
23.719666	1030.047959	15.687040
23.859757	1048.928503	15.692058
23.909547	1044.253601	15.697075
24.273976	1043.022536	15.702093
23.997021	1055.160976	15.707111
23.797174	1044.526050	15.712128
24.175439	1045.286323	15.717146
23.957093	1039.723966	15.722163
23.756611	1052.369013	15.727181
23.756480	1054.782437	15.732199
24.087968	1035.868886	15.737216
24.021710	1051.749855	15.742234
24.103176	1044.356813	15.747251
23.972989	1052.203781	15.752269
24.296284	1063.877101	15.757287
24.451979	1076.651767	15.762304
24.595601	1075.836383	15.767322
24.149755	1068.073573	15.772339
24.672063	1068.993848	15.777357
24.481294	1069.472374	15.782375
24.674433	1054.209930	15.787392
24.511662	1047.977367	15.792410
24.587881	1043.751222	15.797427
24.522596	1042.216522	15.802445
24.523932	1052.291630	15.807463
24.689170	1039.130596	15.812480
24.389890	1042.049441	15.817498
24.444185	1045.215634	15.822515
24.714673	1051.133332	15.827533
24.418863	1057.403454	15.832551
24.484942	1064.397092	15.837568
24.466471	1075.468373	15.842586
24.495138	1076.972339	15.847603
24.571332	1073.103659	15.852621
24.714426	1081.695914	15.857639
24.781110	1066.729190	15.862656
24.480840	1075.612959	15.867674
24.783591	1084.618135	15.872691
25.224363	1075.804606	15.877709
25.117208	1077.130674	15.882727
25.111283	1071.424474	15.887744
25.099548	1071.332429	15.892762
25.061741	1072.801339	15.897779
25.142711	1063.291515	15.902797
24.770481	1073.754072	15.907815
24.905619	1067.619411	15.912832
24.935366	1064.618630	15.917850
24.973128	1067.008853	15.922867
24.702852	1061.692480	15.927885
24.343898	1079.143149	15.932903
24.739906	1061.950713	15.937920
25.012486	1076.815400	15.942938
25.053966	1095.891851	15.947955
25.450684	1095.798705	15.952973
25.463485	1099.661916	15.957991
25.677616	1087.029735	15.963008
25.403995	1070.199343	15.968026
24.937317	1069.447615	15.973043
25.356554	1070.945961	15.978061
25.642960	1091.645179	15.983079
25.550661	1083.533279	15.988096
25.471222	1073.155158	15.993114
24.990630	1070.208565	15.998131
25.482780	1067.724897	16.003149
25.380266	1095.814645	16.008167
25.370943	1099.083900	16.013184
25.446949	1092.631079	16.018202
25.678998	1097.806759	16.023219
25.654280	1096.979879	16.028237
25.244394	1094.032204	16.033255
25.552726	1089.163696	16.038272
25.841174	1093.380068	16.043290
25.595714	1097.010853	16.048307
25.797789	1087.022315	16.053325
25.453806	1099.004570	16.058343
25.870440	1086.273507	16.063360
26.022086	1094.026193	16.068378
25.382539	1093.427887	16.073395
25.819007	1084.122956	16.078413
25.730071	1093.553218	16.083431
25.567943	1089.851944	16.088448
25.532080	1092.202001	16.093466
25.559413	1097.959592	16.098483
25.924962	1110.660169	16.103501
25.909257	1125.511222	16.108519
26.284306	1124.775622	16.113536
26.161045	1114.473625	16.118554
25.976105	1118.872323	16.123571
26.486946	1113.579342	16.128589
26.372503	1121.163904	16.133607
26.250846	1103.329997	16.138624
26.156015	1091.402494	16.143642
25.812782	1095.231746	16.148659
26.421983	1101.285497	16.153677
26.276165	1114.319956	16.158695
26.519277	1118.041101	16.163712
26.335475	1108.597925	16.168730
26.698873	1113.400298	16.173747
26.493317	1091.641839	16.178765
26.383569	1084.778062	16.183783
26.539288	1078.070717	16.188800
26.546922	1081.473770	16.193818
26.067284	1083.134735	16.198835
26.300481	1078.602283	16.203853
26.185674	1098.215228	16.208871
26.142927	1106.851262	16.213888
26.298036	1112.864463	16.218906
26.435473	1111.219420	16.223923
26.435779	1112.970991	16.228941
26.451609	1104.273476	16.233959
26.774576	1121.233731	16.238976
26.876098	1115.975457	16.243994
26.411590	1117.030396	16.249011
26.811730	1111.758896	16.254029
26.689407	1118.527858	16.259047
26.620668	1113.936339	16.264064
26.581189	1113.155996	16.269082
26.431269	1117.739046	16.274099
26.825972	1116.240373	16.279117
26.991727	1135.139213	16.284135
26.849835	1133.296726	16.289152
27.213850	1131.746442	16.294170
26.880445	1123.551219	16.299187
27.029634	1124.507296	16.304205
27.095576	1129.796316	16.309223
26.679523	1135.230894	16.314240
27.550069	1133.663663	16.319258
27.225846	1134.194209	16.324275
26.609367	1120.955465	16.329293
27.184291	1131.122256	16.334311
27.456329	1149.363770	16.339328
27.463448	1138.561049	16.344346
27.146934	1136.020726	16.349363
27.319400	1136.461942	16.354381
27.411353	1140.282136	16.359399
27.218688	1139.484244	16.364416
27.311920	1142.641649	16.369434
27.154371	1140.609239	16.374451
27.429129	1130.179911	16.379469
27.221759	1143.052937	16.384487
27.301319	1135.042863	16.389504
27.266574	1123.900244	16.394522
27.551436	1135.148893	16.399539
27.673295	1137.019705	16.404557
27.626387	1139.206643	16.409575
27.337510	1140.384466	16.414592
27.780557	1130.685910	16.419610
27.486907	1138.139135	16.424627
27.663756	1124.924532	16.429645
27.870812	1131.305900	16.434663
27.988087	1129.283102	16.439680
28.013276	1122.347753	16.444698
27.565711	1135.670375	16.449715
27.947612	1128.703122	16.454733
27.821014	1126.005374	16.459751
27.455768	1134.487350	16.464768
27.948242	1124.189687	16.469786
27.560633	1131.162812	16.474803
27.527407	1121.545880	16.479821
27.823889	1128.898629	16.484839
27.845856	1142.469091	16.489856
28.164625	1151.444883	16.494874
27.906812	1158.803603	16.499891
28.160632	1153.636236	16.504909
28.454710	1160.168950	16.509927
27.942340	1149.878604	16.514944
28.425085	1147.629545	16.519962
28.177320	1144.544782	16.524979
28.235725	1135.108333	16.529997
28.035723	1138.730026	16.535015
28.049850	1153.019491	16.540032
28.296504	1152.013425	16.545050
28.177627	1154.835886	16.550067
28.335237	1152.280044	16.555085
28.349146	1157.334389	16.560103
28.081893	1157.312211	16.565120
28.271680	1153.192424	16.570138
27.860099	1155.673993	16.575155
28.199091	1157.923016	16.580173
28.344261	1153.490941	16.585191
28.126132	1160.026580	16.590208
28.357625	1175.615861	16.595226
28.396079	1185.567590	16.600243
28.538532	1180.788723	16.605261
28.625092	1184.173219	16.610279
28.497401	1188.871503	16.615296
28.593504	1182.260203	16.620314
28.576497	1185.373273	16.625331
28.634839	1187.193193	16.630349
28.719242	1177.265812	16.635367
28.809171	1180.647387	16.640384
29.071631	1172.275522	16.645402
29.249582	1173.973670	16.650419
29.034128	1173.585051	16.655437
28.955233	1178.958698	16.660455
28.872632	1166.672035	16.665472
29.315657	1172.634831	16.670490
29.198390	1175.885757	16.675507
28.976810	1180.634624	16.680525
28.969267	1177.059696	16.685543
28.956363	1183.521994	16.690560
28.969986	1177.850705	16.695578
28.906791	1176.335330	16.700595
29.102775	1167.928413	16.705613
29.415125	1164.635156	16.710631
29.261155	1175.031327	16.715648
29.134653	1175.376777	16.720666
29.220095	1178.861454	16.725683
29.029705	1180.989087	16.730701
29.295470	1181.002268	16.735719
29.429077	1195.684181	16.740736
29.627027	1195.778275	16.745754
30.062746	1190.814235	16.750771
29.828610	1176.641684	16.755789
29.582769	1168.725630	16.760807
29.514340	1174.183760	16.765824
29.578952	1167.780037	16.770842
29.260368	1170.600530	16.775859
28.809446	1171.467008	16.780877
29.319785	1188.630163	16.785895
29.528323	1204.247683	16.790912
30.064675	1205.276269	16.795930
29.647129	1203.079034	16.800947
29.557361	1214.723229	16.805965
29.990682	1208.928499	16.810983
29.664990	1213.270216	16.816000
29.644692	1201.921217	16.821018
29.779914	1204.909874	16.826035
30.148518	1201.835635	16.831053
30.104194	1197.873496	16.836071
29.762768	1205.011444	16.841088
29.972735	1204.436636	16.846106
29.942747	1201.390209	16.851123
30.222339	1204.687630	16.856141
30.019311	1196.947145	16.861159
29.735837	1212.890624	16.866176
30.256473	1196.281325	16.871194
30.326500	1186.775206	16.876211
30.121237	1190.391877	16.881229
30.540100	1198.533822	16.886247
30.319551	1193.745375	16.891264
30.337686	1190.483506	16.896282
30.533366	1204.222891	16.901299
30.350738	1207.341737	16.906317
30.551725	1191.995970	16.911335
30.057102	1198.808503	16.916352
30.468177	1194.835918	16.921370
30.200894	1200.913977	16.926387
30.250120	1191.356576	16.931405
30.292454	1194.475176	16.936423
30.485201	1218.715570	16.941440
30.655516	1219.550442	16.946458
30.577731	1216.227682	16.951475
30.792532	1228.096252	16.956493
31.142652	1226.886441	16.961511
30.594730	1208.595054	16.966528
30.712442	1197.303519	16.971546
31.178525	1205.962045	16.976563
31.085660	1202.209906	16.981581
31.059026	1182.604313	16.986599
30.774627	1187.191935	16.991616
31.110037	1180.528806	16.996634
31.299325	1189.606373	17.001651
30.804703	1184.934962	17.006669
31.073802	1184.363749	17.011687
30.776194	1186.646928	17.016704
30.869144	1180.669992	17.021722
30.826143	1190.325377	17.026739
30.982719	1184.877260	17.031757
31.251271	1189.917403	17.036775
30.869966	1204.546006	17.041792
30.845865	1209.160216	17.046810
31.297861	1210.147654	17.051827
31.030496	1211.246331	17.056845
31.260810	1207.264699	17.061863
31.282623	1215.329881	17.066880
31.313805	1212.068998	17.071898
31.271665	1210.535960	17.076915
31.269870	1211.963882	17.081933
31.605236	1209.832523	17.086951
31.473543	1217.401484	17.091968
31.330289	1224.633396	17.096986
31.715093	1213.916899	17.102003
31.299430	1211.729586	17.107021
31.324946	1206.850785	17.112039
30.899836	1221.848853	17.117056
31.290281	1223.309858	17.122074
31.775075	1239.969046	17.127091
31.656874	1236.343138	17.132109
31.956743	1240.168692	17.137127
31.516463	1246.582493	17.142144
31.809747	1248.268639	17.147162
32.023310	1246.074768	17.152179
31.804491	1246.314642	17.157197
31.789690	1242.259416	17.162215
31.890658	1236.888597	17.167232
32.007940	1244.742716	17.172250
32.330498	1241.933174	17.177267
32.304386	1243.217098	17.182285
32.523037	1235.865027	17.187303
32.042393	1234.243182	17.192320
32.140890	1232.617566	17.197338
32.080082	1234.179274	17.202355
32.085776	1238.928321	17.207373
32.128255	1231.623140	17.212391
32.080585	1239.106153	17.217408
31.889212	1243.995309	17.222426
32.109444	1230.739182	17.227443
31.709764	1237.813170	17.232461
31.906193	1253.289441	17.237479
31.967701	1267.212118	17.242496
32.615100	1263.252352	17.247514
32.899871	1263.491516	17.252531
32.458032	1263.336438	17.257549
32.962549	1260.958565	17.262567
32.778766	1269.332222	17.267584
32.518381	1271.648618	17.272602
33.000465	1256.070815	17.277619
32.604940	1255.569886	17.282637
32.134810	1246.945672	17.287655
32.399288	1252.423508	17.292672
32.447012	1254.070789	17.297690
32.772025	1258.064228	17.302707
32.487422	1264.232185	17.307725
32.750319	1251.379990	17.312743
32.716890	1263.113710	17.317760
32.701681	1266.689874	17.322778
32.899514	1251.981958	17.327795
32.465603	1257.669922	17.332813
33.048380	1264.577308	17.337831
32.978103	1283.674071	17.342848
32.917720	1286.506160	17.347866
33.263811	1287.899320	17.352883
33.186774	1290.773538	17.357901
32.923245	1280.952520	17.362919
33.009734	1284.129573	17.367936
33.075413	1289.820651	17.372954
33.621062	1290.809910	17.377971
33.368252	1289.618828	17.382989
33.911268	1278.654440	17.388007
33.641682	1283.749075	17.393024
33.746718	1280.825941	17.398042
33.692122	1276.802099	17.403059
33.433020	1281.955232	17.408077
33.561046	1275.126406	17.413095
33.764973	1272.230599	17.418112
33.351505	1282.652094	17.423130
33.720947	1275.769121	17.428147
33.599223	1278.116495	17.433165
33.271849	1269.692247	17.438183
33.958187	1274.019553	17.443200
33.771214	1270.644783	17.448218
33.891441	1262.879873	17.453235
33.853315	1276.308438	17.458253
34.177365	1267.735776	17.463271
34.253203	1270.469718	17.468288
33.811578	1279.550233	17.473306
34.022347	1267.563725	17.478323
33.903405	1280.362382	17.483341
34.592860	1267.854101	17.488359
34.124517	1250.773870	17.493376
33.865985	1252.193521	17.498394
34.286706	1247.329582	17.503411
33.875687	1257.547116	17.508429
34.139135	1264.588872	17.513447
34.156519	1268.842302	17.518464
33.829687	1263.102949	17.523482
34.105255	1263.898349	17.528499
34.083158	1266.751260	17.533517
34.226117	1266.951702	17.538535
34.235117	1265.734200	17.543552
34.046671	1262.357313	17.548570
34.182677	1264.483273	17.553587
33.889565	1273.337230	17.558605
34.220603	1282.555550	17.563623
34.526935	1283.610025	17.568640
34.661976	1297.402446	17.573658
34.718282	1293.064179	17.578675
34.514234	1297.383021	17.583693
34.282047	1299.379011	17.588711
34.755229	1303.993191	17.593728
34.615465	1301.148775	17.598746
34.685409	1301.973107	17.603763
34.510555	1305.743034	17.608781
34.591840	1292.891350	17.613799
34.767714	1296.469738	17.618816
34.536447	1299.941531	17.623834
34.720428	1314.194358	17.628851
34.773585	1323.554382	17.633869
35.017350	1324.390090	17.638887
35.058894	1332.533167	17.643904
34.938840	1318.318368	17.648922
35.275839	1321.696465	17.653939
35.210971	1328.132388	17.658957
35.014131	1323.762801	17.663975
35.381583	1318.305704	17.668992
35.481994	1322.391467	17.674010
35.565186	1310.477624	17.679027
35.493205	1318.443826	17.684045
35.314289	1319.438496	17.689063
35.278878	1311.854841	17.694080
35.241773	1331.070183	17.699098
35.735153	1314.969199	17.704115
35.466589	1316.916491	17.709133
35.458743	1328.150364	17.714151
35.571999	1316.918927	17.719168
35.720373	1306.684420	17.724186
36.108680	1313.953551	17.729203
35.803851	1316.321013	17.734221
35.667532	1306.343091	17.739239
35.914789	1314.324934	17.744256
35.687261	1317.231555	17.749274
35.928474	1308.223777	17.754291
35.750202	1313.025354	17.759309
35.797457	1315.704589	17.764327
35.828274	1315.549199	17.769344
35.772271	1323.221030	17.774362
35.946440	1316.949496	17.779379
35.702021	1321.532505	17.784397
35.407383	1317.390134	17.789415
35.685865	1329.716340	17.794432
35.575969	1341.243099	17.799450
35.991691	1343.004256	17.804467
35.901342	1349.465667	17.809485
35.853404	1346.831625	17.814503
36.302234	1347.534956	17.819520
36.586321	1344.037684	17.824538
36.255487	1343.715801	17.829555
36.382523	1348.275501	17.834573
36.370859	1347.437391	17.839591
36.887719	1348.377879	17.844608
36.562394	1350.232213	17.849626
36.504873	1340.116421	17.854643
36.529738	1338.775028	17.859661
36.723013	1337.036858	17.864679
36.762154	1333.197082	17.869696
36.493300	1343.234048	17.874714
36.670696	1338.133999	17.879731
36.382327	1348.722222	17.884749
36.666252	1359.181046	17.889767
37.138088	1359.467976	17.894784
36.931784	1366.243865	17.899802
36.696528	1362.043224	17.904819
36.808027	1360.171745	17.909837
37.258928	1362.523526	17.914855
37.615977	1362.951509	17.919872
37.163412	1355.432574	17.924890
37.062776	1332.202491	17.929907
37.235339	1329.641782	17.934925
36.781091	1335.516603	17.939943
37.301059	1338.445517	17.944960
37.006868	1349.563042	17.949978
37.453200	1348.953817	17.954995
37.478752	1351.354767	17.960013
37.135807	1362.048097	17.965031
37.349399	1356.950709	17.970048
37.111110	1359.257554	17.975066
37.330428	1361.744924	17.980083
37.593250	1357.626770	17.985101
37.237618	1362.671506	17.990119
37.590087	1362.385298	17.995136
37.660949	1365.966524	18.000154
37.472686	1357.842810	18.005171
37.467032	1363.522893	18.010189
37.619021	1358.654993	18.015207
37.742324	1355.161900	18.020224
37.442162	1358.107720	18.025242
37.511649	1364.409603	18.030259
37.853567	1367.993979	18.035277
37.673243	1367.929847	18.040295
37.428504	1370.443664	18.045312
37.336125	1385.400968	18.050330
37.578690	1391.248225	18.055347
37.937908	1387.114889	18.060365
38.102474	1381.687033	18.065383
38.161846	1380.356852	18.070400
37.952591	1380.441996	18.075418
37.932449	1385.114658	18.080435
38.099409	1394.872411	18.085453
38.047685	1406.582497	18.090471
38.476985	1402.128896	18.095488
38.538289	1398.509841	18.100506
38.494709	1405.851315	18.105523
39.097911	1397.148897	18.110541
38.521613	1392.794878	18.115559
38.511023	1374.705263	18.120576
38.460995	1380.656475	18.125594
38.350309	1374.883652	18.130611
38.590437	1378.367957	18.135629
38.560503	1403.298259	18.140647
38.599006	1398.832204	18.145664
38.975745	1402.273422	18.150682
38.702118	1408.695521	18.155699
39.064489	1396.919241	18.160717
38.752257	1390.727428	18.165735
38.897248	1392.638536	18.170752
38.792158	1394.966244	18.175770
38.959329	1398.347281	18.180787
39.098287	1396.962189	18.185805
38.730710	1394.272405	18.190823
38.974820	1392.999822	18.195840
39.050076	1400.764523	18.200858
38.920605	1400.815198	18.205875
38.710990	1395.067015	18.210893
38.695679	1404.217956	18.215911
38.841430	1399.875872	18.220928
39.167738	1416.912277	18.225946
38.893363	1421.917199	18.230963
39.105865	1413.052303	18.235981
38.992043	1423.510495	18.240999
39.312568	1421.249677	18.246016
39.361235	1422.427534	18.251034
39.318172	1426.753614	18.256051
39.432162	1434.503258	18.261069
39.593595	1450.085520	18.266087
39.860828	1451.406714	18.271104
39.860955	1453.747324	18.276122
39.692348	1437.521971	18.281139
40.044266	1421.497844	18.286157
39.392065	1425.004323	18.291175
39.749633	1433.899447	18.296192
39.921001	1443.995475	18.301210
40.157644	1446.386290	18.306227
40.273789	1441.942011	18.311245
40.153727	1429.009381	18.316263
40.140388	1418.592524	18.321280
39.994136	1409.947266	18.326298
39.995259	1404.082691	18.331315
40.146405	1401.770789	18.336333
39.981430	1420.218842	18.341351
40.193929	1440.060304	18.346368
40.168642	1430.526904	18.351386
40.161260	1442.013536	18.356403
40.758535	1435.603786	18.361421
40.542786	1433.407354	18.366439
40.442935	1438.000711	18.371456
40.683495	1436.370054	18.376474
40.469621	1435.159915	18.381491
40.593658	1435.657978	18.386509
40.597196	1435.702376	18.391527
40.541658	1437.884879	18.396544
40.537282	1441.627004	18.401562
40.577697	1437.133850	18.406579
40.567270	1433.784141	18.411597
40.804666	1436.310655	18.416615
40.786840	1429.183869	18.421632
40.450316	1431.732184	18.426650
40.636966	1439.082008	18.431667
40.947073	1435.073327	18.436685
40.520791	1437.462098	18.441703
40.761431	1445.595103	18.446720
40.961831	1457.303244	18.451738
40.597680	1458.025447	18.456755
40.965022	1464.551671	18.461773
41.295956	1462.468257	18.466791
41.104966	1461.339758	18.471808
41.332484	1456.195151	18.476826
41.207333	1454.160090	18.481843
41.101707	1460.168176	18.486861
40.682210	1462.799526	18.491879
41.450798	1477.113970	18.496896
41.649441	1487.977157	18.501914
41.550473	1483.896829	18.506931
41.777606	1474.234205	18.511949
41.629744	1481.100072	18.516967
41.912644	1477.819107	18.521984
42.041647	1475.897866	18.527002
41.528389	1473.906593	18.532019
41.768285	1463.718639	18.537037
41.805071	1475.884984	18.542055
42.053259	1481.513630	18.547072
42.191527	1477.990080	18.552090
42.172319	1474.552053	18.557107
41.991409	1457.192505	18.562125
41.961346	1452.982273	18.567143
41.889256	1447.398699	18.572160
42.179040	1465.895522	18.577178
42.029947	1468.567532	18.582195
42.454709	1475.467714	18.587213
42.262427	1477.890973	18.592231
41.867681	1481.916642	18.597248
42.333016	1474.216923	18.602266
42.054325	1474.911591	18.607283
42.417502	1469.577589	18.612301
41.986981	1480.616207	18.617319
42.240983	1476.160509	18.622336
42.476699	1472.944444	18.627354
42.077114	1474.098889	18.632371
42.389093	1465.024580	18.637389
42.535809	1466.240142	18.642407
42.267066	1483.749161	18.647424
42.391269	1488.142837	18.652442
42.239454	1497.809739	18.657459
42.574458	1495.302814	18.662477
42.778718	1502.441093	18.667495
42.851357	1506.201978	18.672512
42.719654	1501.656595	18.677530
42.966961	1506.390126	18.682547
42.936718	1501.815346	18.687565
42.926392	1501.181336	18.692583
43.233658	1491.278270	18.697600
43.364257	1503.522016	18.702618
43.178045	1500.570688	18.707635
43.498649	1492.143356	18.712653
43.479059	1501.400967	18.717671
43.243525	1488.361030	18.722688
43.345018	1496.235214	18.727706
43.455664	1496.618962	18.732723
43.593313	1487.339254	18.737741
43.607273	1495.507457	18.742759
43.267242	1498.259119	18.747776
43.603572	1488.325652	18.752794
43.431207	1499.152247	18.757811
43.727988	1519.486545	18.762829
43.709733	1519.705024	18.767847
43.694034	1517.965610	18.772864
43.770989	1517.739192	18.777882
43.885930	1524.689515	18.782899
43.844291	1516.333961	18.787917
43.869263	1520.252741	18.792935
43.812767	1533.132998	18.797952
44.146545	1515.907059	18.802970
43.792896	1525.897947	18.807987
43.838176	1516.903987	18.813005
43.910465	1518.325971	18.818023
43.948674	1524.192943	18.823040
44.030429	1517.011832	18.828058
44.148860	1526.328494	18.833075
44.489881	1528.103617	18.838093
44.217254	1537.779917	18.843111
44.019876	1549.195726	18.848128
44.508247	1545.506317	18.853146
44.439117	1550.742256	18.858163
44.514320	1547.749603	18.863181
44.885367	1545.804811	18.868199
44.721644	1543.853684	18.873216
44.924650	1535.039109	18.878234
44.885965	1546.442025	18.883251
45.143926	1542.054157	18.888269
45.268558	1533.684448	18.893287
44.883705	1514.739714	18.898304
45.091172	1502.354361	18.903322
45.022327	1516.725222	18.908339
44.733427	1513.748375	18.913357
45.054187	1509.234371	18.918375
44.967411	1515.058255	18.923392
44.984500	1510.513429	18.928410
44.960045	1527.142290	18.933427
45.035928	1530.773117	18.938445
45.074728	1529.047119	18.943463
45.080469	1531.173426	18.948480
45.366867	1526.108416	18.953498
45.016265	1541.683821	18.958515
44.993869	1538.291583	18.963533
45.201828	1539.510396	18.968551
44.980396	1541.769989	18.973568
45.332262	1550.395260	18.978586
45.230495	1571.279080	18.983603
45.306635	1569.100439	18.988621
45.571114	1573.650046	18.993639
45.447167	1572.656107	18.998656
45.665078	1568.044943	19.003674
45.800410	1566.423822	19.008691
45.560629	1563.959304	19.013709
46.051788	1569.124918	19.018727
45.585726	1580.108861	19.023744
45.886570	1579.305214	19.028762
45.839115	1591.878905	19.033779
46.268544	1594.594515	19.038797
46.542242	1595.381582	19.043815
45.908675	1590.388957	19.048832
46.000854	1593.563557	19.053850
46.028950	1590.198775	19.058867
46.283865	1585.006282	19.063885
46.832213	1580.056542	19.068903
46.608961	1593.681388	19.073920
46.563044	1587.661148	19.078938
46.236211	1594.642131	19.083955
45.969629	1590.690709	19.088973
46.344639	1585.935416	19.093991
46.365007	1586.308130	19.099008
46.671216	1582.800450	19.104026
46.828976	1583.550414	19.109043
46.665228	1581.954010	19.114061
46.804177	1588.564955	19.119079
46.558594	1609.237206	19.124096
47.417152	1601.753025	19.129114
47.323840	1613.015035	19.134131
46.989205	1598.651649	19.139149
47.105110	1594.258548	19.144167
47.142024	1604.319462	19.149184
47.201048	1595.548772	19.154202
47.002468	1603.998287	19.159219
46.818077	1620.923021	19.164237
47.293005	1610.827158	19.169255
47.184106	1615.729939	19.174272
47.248109	1608.662749	19.179290
47.478891	1614.210468	19.184307
47.265462	1616.776226	19.189325
47.334861	1616.201452	19.194343
47.041527	1617.385952	19.199360
47.469908	1616.910399	19.204378
47.822236	1627.712411	19.209395
47.706561	1636.504515	19.214413
47.779135	1634.946142	19.219431
47.729913	1643.181183	19.224448
47.979083	1637.449859	19.229466
47.779746	1640.028249	19.234483
47.971756	1643.414676	19.239501
48.093885	1629.594531	19.244519
47.911836	1640.737396	19.249536
48.179970	1632.740330	19.254554
48.090573	1634.241852	19.259571
47.985127	1635.507054	19.264589
48.332939	1624.136164	19.269607
48.169191	1627.957479	19.274624
48.199681	1624.155678	19.279642
48.166931	1632.304522	19.284659
47.919906	1632.518361	19.289677
48.140500	1623.528383	19.294695
48.094728	1637.378211	19.299712
48.541048	1645.759550	19.304730
48.857233	1665.089250	19.309747
48.757052	1660.289781	19.314765
48.879977	1658.337634	19.319783
49.006593	1655.895110	19.324800
49.216740	1648.704491	19.329818
49.334103	1624.884721	19.334835
48.971827	1621.782994	19.339853
49.132016	1614.072710	19.344871
49.182651	1618.014431	19.349888
49.049074	1615.024444	19.354906
49.142464	1610.308294	19.359923
48.768742	1613.707680	19.364941
48.992965	1617.397036	19.369959
48.974970	1627.425325	19.374976
48.930769	1631.239839	19.379994
48.982879	1647.932923	19.385011
49.174524	1655.382811	19.390029
49.110113	1648.684111	19.395047
49.241847	1655.387224	19.400064
49.685760	1648.606718	19.405082
49.598944	1652.893649	19.410099
49.233347	1639.515276	19.415117
49.940357	1651.842833	19.420135
49.744886	1655.894998	19.425152
50.013101	1658.303061	19.430170
50.078230	1647.936443	19.435187
49.737672	1646.365765	19.440205
49.760604	1646.041991	19.445223
49.995673	1660.405970	19.450240
50.057965	1678.573391	19.455258
50.406394	1679.028403	19.460275
50.242152	1671.797400	19.465293
50.299140	1666.750645	19.470311
50.097296	1659.410914	19.475328
50.015355	1670.342735	19.480346
50.086444	1670.397996	19.485363
50.046050	1669.082735	19.490381
50.510354	1674.459919	19.495399
50.261386	1669.959100	19.500416
50.118956	1665.395367	19.505434
50.511814	1665.499713	19.510451
50.545084	1667.371479	19.515469
50.452152	1664.980661	19.520487
50.769914	1692.767648	19.525504
50.673769	1697.477398	19.530522
50.934039	1700.763166	19.535539
50.829703	1703.852610	19.540557
51.076087	1696.290219	19.545575
51.317267	1705.224064	19.550592
51.373903	1701.029723	19.555610
51.193369	1688.187205	19.560627
50.797076	1681.771002	19.565645
51.360911	1684.310830	19.570663
51.088321	1695.828570	19.575680
50.734979	1701.824615	19.580698
50.700028	1694.812747	19.585715
51.028515	1694.871452	19.590733
51.154117	1697.156677	19.595751
51.320598	1702.876099	19.600768
51.562385	1711.846855	19.605786
52.054081	1708.891903	19.610803
51.929248	1716.248946	19.615821
51.626649	1702.440399	19.620839
51.466533	1696.289811	19.625856
51.780214	1705.389999	19.630874
51.819738	1700.657151	19.635891
51.936616	1716.160837	19.640909
52.060306	1710.182545	19.645927
52.109901	1709.960655	19.650944
52.166934	1705.166637	19.655962
51.964500	1700.312039	19.660979
51.845019	1708.170557	19.665997
52.053787	1699.884860	19.671015
51.801535	1711.837042	19.676032
51.787660	1717.217038	19.681050
51.925319	1707.612787	19.686067
51.767756	1718.004010	19.691085
52.030923	1726.470837	19.696103
52.146556	1733.337675	19.701120
52.103436	1731.050017	19.706138
52.288984	1733.072563	19.711155
52.366116	1734.498489	19.716173
52.572012	1741.407866	19.721191
52.619417	1752.795104	19.726208
52.780000	1750.233161	19.731226
53.270442	1755.561164	19.736243
53.227341	1756.112896	19.741261
53.277057	1753.476396	19.746279
53.503485	1746.498786	19.751296
53.196324	1731.944505	19.756314
53.234424	1722.990198	19.761331
52.874999	1724.803763	19.766349
52.946927	1720.082472	19.771367
53.276830	1736.178864	19.776384
53.417234	1743.145543	19.781402
53.540277	1748.672173	19.786419
53.398263	1749.214298	19.791437
53.519764	1753.570308	19.796455
53.365404	1757.191673	19.801472
53.659486	1751.029245	19.806490
53.723970	1750.252128	19.811507
53.582543	1758.832816	19.816525
53.726043	1748.990167	19.821543
53.831366	1754.261857	19.826560
53.717792	1752.529567	19.831578
53.501298	1747.609959	19.836595
53.841700	1760.555790	19.841613
53.923082	1760.644781	19.846631
53.635330	1773.444629	19.851648
54.001131	1775.651511	19.856666
54.175183	1776.920841	19.861683
54.161006	1782.439100	19.866701
54.279687	1774.166311	19.871719
54.288080	1780.248162	19.876736
54.094274	1777.623632	19.881754
54.377730	1771.619650	19.886771
54.210517	1783.234181	19.891789
54.511022	1784.562101	19.896807
54.588543	1804.214567	19.901824
54.447086	1810.607071	19.906842
54.715402	1803.624468	19.911859
54.818754	1806.142530	19.916877
54.557629	1798.047971	19.921895
54.924931	1803.087321	19.926912
54.691955	1807.512276	19.931930
54.759942	1799.834095	19.936947
54.892139	1796.595340	19.941965
54.987064	1798.168721	19.946983
54.994763	1798.923464	19.952000
55.290399	1820.068594	19.957018
55.596221	1816.213283	19.962035
55.225822	1808.816349	19.967053
55.365687	1802.888887	19.972071
55.702349	1814.492059	19.977088
55.661610	1814.972929	19.982106
55.614524	1795.412862	19.987123
55.383367	1797.718195	19.992141
55.550292	1812.656992	19.997159
55.560784	1813.325445	20.002176
55.811862	1818.433651	20.007194
55.747377	1812.159701	20.012211
55.833279	1817.838964	20.017229
55.547873	1827.717168	20.022247
56.173880	1818.356403	20.027264
55.854231	1811.234927	20.032282
56.010252	1807.298121	20.037299
55.808378	1810.199404	20.042317
56.212329	1815.520095	20.047335
56.530040	1812.149831	20.052352
56.140358	1818.021227	20.057370
56.414064	1809.572748	20.062387
56.565166	1810.858873	20.067405
56.366201	1811.262791	20.072423
56.374862	1816.938307	20.077440
56.457587	1832.214297	20.082458
56.446851	1838.259179	20.087475
56.650876	1840.995620	20.092493
56.731853	1835.960587	20.097511
56.792241	1836.607393	20.102528
56.853968	1836.183096	20.107546
56.656351	1836.778526	20.112563
56.766845	1838.681229	20.117581
57.186164	1831.882669	20.122599
56.942509	1833.029824	20.127616
56.949919	1835.498028	20.132634
57.168016	1850.398072	20.137651
56.996773	1864.607073	20.142669
57.111645	1859.557758	20.147687
57.160232	1866.286935	20.152704
57.286636	1873.741825	20.157722
57.458902	1864.647110	20.162739
57.355739	1864.675711	20.167757
57.329987	1866.685623	20.172775
57.563314	1858.510344	20.177792
57.335394	1875.679968	20.182810
57.783307	1887.424620	20.187827
57.683923	1880.133568	20.192845
57.765926	1888.850957	20.197863
58.290940	1885.189657	20.202880
58.202196	1894.942426	20.207898
58.097587	1889.508568	20.212915
58.181301	1885.110872	20.217933
58.239788	1887.364324	20.222951
58.389388	1878.170596	20.227968
58.358547	1883.106207	20.232986
58.636490	1880.044094	20.238003
58.510909	1884.381602	20.243021
58.560958	1875.820905	20.248039
58.682447	1882.751407	20.253056
58.614711	1890.651451	20.258074
58.728021	1885.100014	20.263091
58.435901	1878.036942	20.268109
58.594923	1881.038327	20.273127
58.875876	1878.835967	20.278144
58.473371	1884.355567	20.283162
58.614182	1882.740201	20.288179
58.725008	1905.827499	20.293197
58.678718	1901.960389	20.298215
58.933270	1912.654378	20.303232
58.777168	1917.314278	20.308250
59.075643	1914.715304	20.313267
59.191174	1913.772243	20.318285
59.007336	1917.721760	20.323303
59.109102	1917.863284	20.328320
59.339350	1941.463943	20.333338
59.622395	1941.516396	20.338355
59.747110	1935.907540	20.343373
59.618787	1947.267323	20.348391
60.011483	1932.025308	20.353408
60.113094	1939.737097	20.358426
60.094273	1938.258788	20.363443
59.930854	1931.040914	20.368461
59.713833	1938.070405	20.373479
60.072781	1932.502297	20.378496
60.082819	1935.135438	20.383514
60.418742	1932.564907	20.388531
60.287762	1937.108446	20.393549
60.258043	1936.835904	20.398567
60.495546	1927.124039	20.403584
60.093279	1927.493509	20.408602
60.203418	1924.515472	20.413619
60.347207	1928.595001	20.418637
59.979784	1938.676229	20.423655
60.477964	1930.078705	20.428672
60.323122	1932.188742	20.433690
60.429080	1947.345248	20.438707
60.969629	1946.947181	20.443725
60.894941	1957.086253	20.448743
61.110621	1960.669624	20.453760
60.909103	1957.599479	20.458778
61.091827	1957.219713	20.463795
61.243047	1949.084361	20.468813
61.070590	1960.979819	20.473831
61.171262	1955.765104	20.478848
60.900281	1954.616741	20.483866
61.200789	1953.408006	20.488883
61.353247	1944.352745	20.493901
61.231280	1953.735453	20.498919
61.284500	1950.257376	20.503936
61.589376	1958.057568	20.508954
61.835772	1968.677748	20.513971
61.812818	1965.809144	20.518989
61.794298	1982.690271	20.524007
62.041547	1981.813983	20.529024
62.074405	1982.081486	20.534042
61.910149	1975.172399	20.539059
62.011187	1965.576020	20.544077
61.695155	1976.237754	20.549095
62.277909	1972.171588	20.554112
62.066796	1975.346878	20.559130
62.179181	1975.665388	20.564147
62.436873	1976.826002	20.569165
61.967254	1977.185758	20.574183
62.239271	1973.863184	20.579200
62.212568	1976.036264	20.584218
62.141098	1976.196629	20.589235
62.362436	1988.749365	20.594253
62.520149	1999.477953	20.599271
62.505095	2003.136546	20.604288
62.817065	2003.699971	20.609306
62.859464	2002.904844	20.614323
62.887005	1997.514030	20.619341
63.108666	2005.751264	20.624359
62.948544	1998.636752	20.629376
62.849511	2001.651753	20.634394
62.777006	1997.958255	20.639411
63.090490	2008.348058	20.644429
63.079704	2027.224462	20.649447
63.117788	2032.329815	20.654464
63.536924	2029.339574	20.659482
63.438322	2028.831185	20.664499
63.640050	2030.914479	20.669517
63.178586	2030.076003	20.674535
63.486763	2019.803545	20.679552
63.672675	2014.599106	20.684570
63.451593	2016.610670	20.689587
63.398687	2023.723658	20.694605
63.754062	2042.397324	20.699623
64.161060	2045.682888	20.704640
64.279083	2046.390635	20.709658
64.054377	2046.876775	20.714675
64.266767	2036.314645	20.719693
64.398319	2042.674640	20.724711
64.230840	2045.430109	20.729728
64.552958	2049.437622	20.734746
64.500305	2051.701625	20.739763
64.592012	2036.154610	20.744781
64.566725	2048.619092	20.749799
64.624882	2037.981314	20.754816
64.574148	2038.294943	20.759834
64.514673	2042.921952	20.764851
64.722366	2038.202889	20.769869
64.854032	2037.055570	20.774887
64.966510	2036.279941	20.779904
64.857585	2033.232247	20.784922
65.021017	2042.636653	20.789939
65.387881	2051.243188	20.794957
65.172069	2061.531682	20.799975
65.243470	2056.341072	20.804992
65.390908	2063.189798	20.810010
65.302699	2065.428981	20.815027
65.574848	2052.665148	20.820045
65.723772	2055.987540	20.825063
65.683723	2054.780852	20.830080
65.594426	2050.696410	20.835098
65.599705	2051.291719	20.840115
65.751818	2045.316073	20.845133
65.436738	2052.612251	20.850151
65.477073	2050.161905	20.855168
65.847080	2058.473033	20.860186
65.552718	2075.836954	20.865203
65.969868	2075.227026	20.870221
66.045957	2075.371622	20.875239
65.992253	2080.822121	20.880256
66.242550	2080.439432	20.885274
66.396418	2080.734934	20.890291
66.425979	2079.621053	20.895309
66.104289	2080.027973	20.900327
66.379783	2097.277880	20.905344
66.733625	2089.263241	20.910362
66.380352	2103.398658	20.915379
66.632382	2097.201717	20.920397
66.831477	2098.496456	20.925415
66.800395	2106.984259	20.930432
66.931261	2096.209989	20.935450
67.064031	2099.451991	20.940467
67.405300	2095.819098	20.945485
67.117749	2103.178067	20.950503
67.182691	2092.146990	20.955520
67.386229	2109.993489	20.960538
67.458464	2125.864437	20.965555
67.715288	2121.973857	20.970573
67.341189	2130.027900	20.975591
67.444642	2131.446749	20.980608
67.564270	2122.709823	20.985626
67.881500	2118.826566	20.990643
67.983899	2118.335289	20.995661
68.046611	2124.715377	21.000679
67.938157	2116.487889	21.005696
68.052474	2115.161146	21.010714
67.912972	2121.763304	21.015731
68.327018	2122.038170	21.020749
68.445529	2116.908639	21.025767
68.283694	2117.483981	21.030784
68.582739	2111.495005	21.035802
68.331055	2108.198876	21.040819
68.552627	2106.057500	21.045837
68.388799	2117.626049	21.050855
68.049112	2119.143860	21.055872
68.268932	2109.131650	21.060890
68.071758	2113.180672	21.065907
68.494482	2117.849521	21.070925
68.394729	2132.156380	21.075943
68.672115	2138.254465	21.080960
68.920129	2131.768796	21.085978
68.572078	2145.000206	21.090995
69.007656	2138.805143	21.096013
68.800207	2153.318443	21.101031
69.288517	2165.137330	21.106048
69.425274	2160.427614	21.111066
69.097113	2165.846417	21.116083
69.318067	2160.178237	21.121101
69.533720	2159.352842	21.126119
69.349810	2160.843290	21.131136
69.644831	2160.636272	21.136154
69.815170	2165.002029	21.141171
69.775964	2168.577255	21.146189
69.534553	2168.530318	21.151207
69.792787	2184.832358	21.156224
70.498556	2183.224604	21.161242
70.160588	2187.872963	21.166259
70.127260	2187.643142	21.171277
70.616783	2187.424392	21.176295
70.487642	2185.660771	21.181312
70.865536	2175.340839	21.186330
70.655633	2178.899054	21.191347
70.455218	2181.157619	21.196365
70.714500	2181.521893	21.201383
70.649374	2183.546633	21.206400
70.616035	2180.464346	21.211418
70.292378	2179.054992	21.216435
70.509035	2179.260963	21.221453
70.828505	2185.067048	21.226471
70.837687	2186.445997	21.231488
71.215030	2186.850175	21.236506
71.346771	2209.517518	21.241523
71.268806	2206.117012	21.246541
71.190451	2206.180090	21.251559
71.092258	2210.466301	21.256576
71.373965	2207.473583	21.261594
70.812763	2211.652197	21.266611
71.116842	2195.810401	21.271629
71.403551	2212.028225	21.276647
71.306633	2227.778066	21.281664
71.666785	2223.294346	21.286682
71.594209	2230.865035	21.291699
71.906898	2232.915024	21.296717
72.047039	2233.606125	21.301735
72.015139	2232.808327	21.306752
72.173077	2220.567225	21.311770
72.136063	2226.559915	21.316787
71.991597	2228.561182	21.321805
72.040973	2245.901057	21.326823
72.164482	2257.441426	21.331840
72.268625	2257.182543	21.336858
72.235292	2267.483875	21.341875
72.367284	2267.766861	21.346893
72.456699	2265.902867	21.351911
72.646941	2267.226647	21.356928
72.944174	2267.822839	21.361946
72.933888	2282.433541	21.366963
73.010714	2282.422498	21.371981
73.114175	2297.230532	21.376999
73.028997	2287.217524	21.382016
73.442662	2295.424302	21.387034
73.543826	2286.921848	21.392051
73.723001	2278.864770	21.397069
73.592074	2285.863232	21.402087
73.471939	2289.905449	21.407104
73.536224	2272.857948	21.412122
73.285138	2272.153135	21.417139
73.699968	2280.828237	21.422157
73.838198	2279.952266	21.427175
73.783434	2286.686532	21.432192
73.789246	2271.165710	21.437210
73.549510	2284.836410	21.442227
73.963177	2288.895760	21.447245
74.223831	2292.293802	21.452263
74.129379	2308.131510	21.457280
74.317087	2299.584403	21.462298
74.230691	2302.898564	21.467315
74.380455	2299.536713	21.472333
74.289639	2299.978643	21.477351
74.046579	2301.145024	21.482368
74.561204	2314.416034	21.487386
74.308292	2328.435032	21.492403
74.821163	2334.479638	21.497421
74.931435	2326.689467	21.502439
74.847423	2326.390867	21.507456
74.802829	2324.572678	21.512474
75.117448	2321.474879	21.517491
74.961281	2321.107513	21.522509
75.293559	2336.384021	21.527527
75.379154	2345.094773	21.532544
75.802924	2344.856199	21.537562
76.158927	2349.703104	21.542579
76.227625	2339.842939	21.547597
76.001606	2314.068637	21.552615
75.687605	2321.934080	21.557632
75.978315	2315.516466	21.562650
75.752689	2308.601641	21.567667
75.647085	2313.748989	21.572685
76.189761	2326.785040	21.577703
75.993564	2334.282936	21.582720
76.176486	2333.787769	21.587738
76.350658	2340.968822	21.592755
76.177003	2337.595548	21.597773
76.374179	2330.013438	21.602791
76.110859	2344.809014	21.607808
76.536925	2344.922439	21.612826
76.502634	2334.987987	21.617843
76.536838	2351.558015	21.622861
77.085516	2367.624354	21.627879
76.821940	2371.642308	21.632896
76.845138	2369.806590	21.637914
77.206092	2370.982029	21.642931
77.094166	2366.091762	21.647949
77.102988	2367.218412	21.652967
76.961856	2371.178295	21.657984
76.635915	2369.702368	21.663002
76.733224	2379.482119	21.668019
77.080953	2398.941772	21.673037
77.535189	2390.981620	21.678055
77.842978	2397.603541	21.683072
78.007033	2388.381921	21.688090
77.772196	2399.883692	21.693107
77.567216	2391.662983	21.698125
78.111169	2385.552248	21.703143
77.732450	2393.713495	21.708160
77.658836	2391.212273	21.713178
77.952187	2391.962271	21.718195
77.912412	2402.297043	21.723213
78.138425	2398.388267	21.728231
78.400985	2408.317456	21.733248
78.374798	2408.588444	21.738266
78.628789	2408.537437	21.743283
78.101269	2410.284810	21.748301
78.149541	2413.514490	21.753319
78.392452	2429.293706	21.758336
78.865016	2431.522381	21.763354
78.792466	2421.986355	21.768371
78.741721	2436.502320	21.773389
79.232543	2433.077278	21.778407
79.212081	2431.690143	21.783424
78.744334	2428.984473	21.788442
79.598141	2441.702557	21.793459
79.486708	2458.866134	21.798477
79.733543	2456.263811	21.803495
79.702898	2462.970930	21.808512
80.155126	2466.675106	21.813530
80.092428	2462.782224	21.818547
80.045524	2458.879642	21.823565
80.760414	2457.870386	21.828583
80.488816	2427.789033	21.833600
80.117621	2427.413564	21.838618
80.321873	2421.077942	21.843635
80.144010	2415.143403	21.848653
80.410906	2421.537447	21.853671
80.093831	2423.044061	21.858688
80.322009	2432.604529	21.863706
80.571326	2448.729181	21.868723
80.329679	2452.524615	21.873741
80.692323	2448.599110	21.878759
80.686255	2449.323485	21.883776
80.356374	2454.285560	21.888794
80.799678	2458.596756	21.893811
80.295481	2476.984109	21.898829
81.057807	2479.373488	21.903847
80.990187	2490.433836	21.908864
81.170195	2480.009847	21.913882
81.249085	2484.212085	21.918899
80.930527	2495.777003	21.923917
81.389514	2502.482209	21.928935
81.515066	2508.705586	21.933952
81.667207	2505.898054	21.938970
81.900922	2502.767943	21.943987
81.811601	2506.359813	21.949005
81.846252	2503.119346	21.954023
81.934174	2497.146675	21.959040
81.562113	2501.905500	21.964058
82.022162	2506.684831	21.969075
82.013062	2522.368458	21.974093
82.142000	2530.000421	21.979111
82.263756	2530.972550	21.984128
83.018929	2532.094149	21.989146
83.204047	2525.412026	21.994163
82.741468	2515.336940	21.999181
82.722635	2519.614427	22.004199
82.866515	2515.930651	22.009216
82.862308	2520.214378	22.014234
83.317109	2516.364155	22.019251
83.150014	2530.629771	22.024269
82.924102	2518.072834	22.029287
82.869481	2521.875116	22.034304
82.849608	2517.204219	22.039322
83.143188	2526.709426	22.044339
83.042192	2539.538825	22.049357
83.220590	2536.819072	22.054375
83.441795	2546.108307	22.059392
83.375642	2553.827704	22.064410
83.533782	2555.648981	22.069427
83.785895	2571.530762	22.074445
84.243232	2575.644774	22.079463
84.081608	2571.093399	22.084480
84.387707	2569.448628	22.089498
84.540229	2575.319119	22.094515
84.301638	2579.577493	22.099533
84.683000	2565.644694	22.104551
84.574290	2569.588629	22.109568
84.747671	2568.411923	22.114586
84.784727	2567.109747	22.119603
84.710764	2566.088567	22.124621
84.674211	2559.897884	22.129639
84.779611	2560.456161	22.134656
84.561122	2562.804392	22.139674
84.907784	2558.867333	22.144691
84.986559	2564.363392	22.149709
84.785606	2579.690630	22.154727
84.897271	2582.717711	22.159744
85.251644	2590.542708	22.164762
85.489960	2582.520960	22.169779
85.256586	2594.023812	22.174797
85.631612	2588.578410	22.179815
85.686869	2597.812470	22.184832
85.533983	2610.001658	22.189850
85.877590	2607.825442	22.194867
85.923390	2605.714283	22.199885
86.427062	2602.625682	22.204903
86.429783	2601.355961	22.209920
86.493301	2600.626998	22.214938
86.468208	2596.845580	22.219955
86.213633	2598.846619	22.224973
86.505075	2599.639860	22.229991
86.451671	2600.320108	22.235008
86.566585	2603.370672	22.240026
86.866323	2612.168961	22.245043
86.708172	2632.491850	22.250061
87.006226	2626.458352	22.255079
87.400196	2625.965245	22.260096
86.999068	2634.080323	22.265114
87.120940	2625.791200	22.270131
87.221784	2624.803676	22.275149
87.293506	2624.242261	22.280167
87.148640	2623.480077	22.285184
87.568700	2629.067301	22.290202
87.794020	2640.422190	22.295219
87.423365	2650.049655	22.300237
87.420998	2655.372555	22.305255
87.736745	2652.834779	22.310272
87.540827	2660.208366	22.315290
87.621172	2660.618030	22.320307
87.899912	2671.091596	22.325325
88.257055	2684.137800	22.330343
88.464114	2692.064804	22.335360
88.395435	2679.686835	22.340378
88.536438	2678.614701	22.345395
88.539989	2688.686567	22.350413
88.694259	2689.361176	22.355431
88.783198	2680.736507	22.360448
88.552160	2679.603128	22.365466
88.886418	2680.597173	22.370483
88.787148	2696.388825	22.375501
89.093487	2704.919520	22.380519
89.202470	2710.739787	22.385536
89.131597	2721.620116	22.390554
89.393677	2706.147775	22.395571
89.101264	2701.838898	22.400589
89.226323	2713.123032	22.405607
89.548629	2719.152094	22.410624
89.580942	2736.200438	22.415642
89.511860	2735.435938	22.420659
89.543377	2739.656327	22.425677
89.580753	2732.448931	22.430695
89.791034	2735.815252	22.435712
89.675434	2750.511157	22.440730
90.171561	2760.466866	22.445747
89.891712	2763.592271	22.450765
89.930785	2757.481121	22.455783
90.584418	2766.578805	22.460800
90.601167	2779.458596	22.465818
90.823938	2777.937451	22.470835
90.730235	2778.752735	22.475853
90.987131	2776.880245	22.480871
91.192559	2772.132202	22.485888
91.092971	2783.619735	22.490906
91.474458	2768.403175	22.495923
91.307932	2772.543361	22.500941
91.098971	2773.360797	22.505959
91.530664	2771.863334	22.510976
91.271640	2778.837946	22.515994
91.365373	2794.689087	22.521011
91.810744	2798.941766	22.526029
92.075604	2801.432069	22.531047
92.285077	2793.109454	22.536064
92.019701	2799.978426	22.541082
92.082084	2798.738578	22.546099
92.284909	2797.618008	22.551117
92.468475	2801.914428	22.556135
92.141249	2793.408604	22.561152
92.263400	2795.228781	22.566170
92.429291	2799.033600	22.571187
92.350600	2808.999860	22.576205
92.584662	2819.717950	22.581223
92.795797	2824.188172	22.586240
92.518493	2825.526808	22.591258
92.931789	2825.433677	22.596275
92.950589	2828.510436	22.601293
92.843201	2840.967883	22.606311
93.623502	2844.280012	22.611328
93.328994	2853.819791	22.616346
93.351441	2846.903420	22.621363
93.468988	2841.347006	22.626381
93.613853	2846.071139	22.631399
93.785905	2841.022278	22.636416
93.763798	2852.811232	22.641434
94.088035	2862.306844	22.646451
94.054528	2861.065544	22.651469
93.989914	2863.895470	22.656487
94.519252	2861.029754	22.661504
94.068827	2868.374312	22.666522
94.326588	2861.531581	22.671539
94.622471	2863.591527	22.676557
94.711548	2864.490341	22.681575
94.991638	2866.877338	22.686592
94.968192	2861.715551	22.691610
94.744789	2861.280950	22.696627
94.674740	2861.979320	22.701645
94.991960	2872.700215	22.706663
95.178904	2884.960922	22.711680
95.212429	2892.679733	22.716698
95.468595	2897.982747	22.721715
95.496045	2905.017474	22.726733
95.220803	2901.629397	22.731751
95.371669	2904.600046	22.736768
95.423016	2903.178538	22.741786
95.600192	2894.675767	22.746803
95.778613	2914.906681	22.751821
95.954536	2911.810076	22.756839
96.062941	2915.641767	22.761856
95.796704	2925.721442	22.766874
96.212341	2922.732797	22.771891
96.200861	2922.246570	22.776909
96.019519	2926.499889	22.781927
96.029470	2933.096543	22.786944
96.512254	2950.218582	22.791962
96.426827	2951.248664	22.796979
96.656007	2949.437835	22.801997
96.653095	2964.996462	22.807015
96.854716	2969.854950	22.812032
97.071659	2971.435023	22.817050
97.288041	2975.300430	22.822067
97.497788	2964.179008	22.827085
97.190068	2974.110845	22.832103
97.947726	2958.969626	22.837120
97.814251	2968.046161	22.842138
97.546017	2970.620029	22.847155
97.934093	2975.267317	22.852173
98.188796	2982.794421	22.857191
98.002740	2982.864308	22.862208
98.285064	2993.037865	22.867226
98.370605	2988.451745	22.872243
98.372573	2984.336590	22.877261
98.398073	2990.339697	22.882279
98.581168	2979.731383	22.887296
98.415241	2978.168266	22.892314
98.481189	3000.079476	22.897331
98.761377	2997.382952	22.902349
98.763405	3007.372197	22.907367
98.972601	3008.412170	22.912384
98.703425	3009.699865	22.917402
99.013967	3009.657214	22.922419
99.410498	3015.214220	22.927437
99.558005	3032.370599	22.932455
99.900666	3035.660338	22.937472
99.873213	3041.512374	22.942490
99.991436	3039.562411	22.947507
99.991756	3029.172531	22.952525
99.849475	3033.089066	22.957543
100.140128	3025.385623	22.962560
100.523486	3036.073238	22.967578
100.279203	3030.421138	22.972595
100.578721	3031.775716	22.977613
100.342765	3038.228072	22.982631
100.514508	3026.958159	22.987648
100.560458	3030.366320	22.992666
100.249211	3044.357819	22.997683
100.737519	3048.344380	23.002701
100.687054	3053.656479	23.007719
100.745853	3060.723097	23.012736
100.944340	3052.952608	23.017754
100.796991	3061.197558	23.022771
101.158642	3082.606339	23.027789
101.223997	3086.599151	23.032807
101.293153	3091.209898	23.037824
101.385249	3087.381003	23.042842
101.087627	3090.933078	23.047859
101.465576	3091.476962	23.052877
101.555491	3116.311812	23.057895
101.856407	3109.969752	23.062912
101.874527	3115.831595	23.067930
101.959229	3117.144181	23.072947
101.993982	3115.987631	23.077965
102.164718	3145.800182	23.082983
102.532293	3135.591970	23.088000
102.641742	3139.760978	23.093018
102.755864	3143.868183	23.098035
103.095826	3142.804027	23.103053
102.816806	3140.813510	23.108071
103.027464	3136.776373	23.113088
102.865147	3132.608056	23.118106
103.209013	3156.090953	23.123123
103.635082	3153.433248	23.128141
103.446542	3154.864706	23.133159
103.448479	3151.913407	23.138176
103.631037	3155.045016	23.143194
103.494405	3162.518876	23.148211
103.986072	3151.382539	23.153229
104.009073	3155.431992	23.158247
104.040268	3141.164100	23.163264
104.231011	3157.732692	23.168282
104.334392	3176.522288	23.173299
104.762217	3172.961836	23.178317
104.738207	3178.540098	23.183335
104.728878	3171.604826	23.188352
105.016445	3170.025668	23.193370
104.851150	3177.862191	23.198387
104.961340	3171.342214	23.203405
105.040830	3170.028238	23.208423
104.947306	3178.217877	23.213440
105.207909	3170.600842	23.218458
105.293162	3171.560943	23.223475
105.041828	3187.107767	23.228493
105.199669	3206.799105	23.233511
105.321699	3194.460814	23.238528
105.344873	3194.420855	23.243546
105.225169	3216.118593	23.248563
105.942147	3218.646326	23.253581
105.761748	3221.775042	23.258599
106.213299	3227.569498	23.263616
106.445743	3224.022878	23.268634
106.203851	3230.684978	23.273651
106.429608	3230.571711	23.278669
106.533783	3247.520518	23.283687
106.464555	3249.837837	23.288704
106.729397	3243.298919	23.293722
106.715866	3244.644317	23.298739
107.053935	3247.097373	23.303757
107.117304	3266.381941	23.308775
107.416476	3268.278782	23.313792
107.704916	3256.450743	23.318810
107.931441	3265.545020	23.323827
107.949495	3252.686439	23.328845
107.444907	3262.933366	23.333863
107.825068	3266.846148	23.338880
108.025410	3254.044796	23.343898
108.414383	3253.701729	23.348915
108.406868	3247.046467	23.353933
108.378382	3256.536147	23.358951
108.261148	3255.507517	23.363968
108.375847	3256.195003	23.368986
107.967066	3251.108303	23.374003
108.501277	3256.396907	23.379021
108.845136	3283.576058	23.384039
108.771622	3286.166563	23.389056
108.768523	3275.213245	23.394074
109.013224	3285.319594	23.399091
108.927725	3277.677911	23.404109
109.087301	3279.752607	23.409127
109.064391	3277.762194	23.414144
109.388096	3295.445655	23.419162
109.227245	3305.317161	23.424179
109.645044	3306.758886	23.429197
109.676618	3297.979577	23.434215
109.581153	3308.467099	23.439232
109.653868	3309.606075	23.444250
109.869106	3333.252284	23.449267
110.319441	3341.544111	23.454285
110.058935	3336.844297	23.459303
110.086210	3341.277385	23.464320
110.513815	3347.324304	23.469338
110.004199	3368.207969	23.474355
110.327290	3353.808082	23.479373
111.196231	3361.705381	23.484391
110.931805	3369.802928	23.489408
111.163614	3377.595855	23.494426
110.849165	3394.813366	23.499443
111.447317	3380.593137	23.504461
111.284073	3393.448504	23.509479
111.249150	3388.924736	23.514496
111.743944	3389.352426	23.519514
111.712430	3403.429442	23.524531
111.795527	3416.433435	23.529549
111.653910	3416.936962	23.534567
112.162575	3420.913557	23.539584
112.584179	3414.048579	23.544602
112.650862	3421.457796	23.549619
112.614698	3415.145041	23.554637
112.725782	3415.094465	23.559655
112.620552	3415.173414	23.564672
113.024211	3421.144396	23.569690
112.984908	3434.262381	23.574707
113.387407	3433.857616	23.579725
113.213393	3440.539279	23.584743
113.641730	3438.629666	23.589760
113.552521	3433.254141	23.594778
113.483602	3431.750516	23.599795
113.762831	3428.630801	23.604813
114.027100	3428.240653	23.609831
113.675709	3428.689924	23.614848
114.152803	3421.972861	23.619866
113.942073	3437.547860	23.624883
114.217033	3436.112513	23.629901
114.728916	3448.464372	23.634919
114.314410	3452.667055	23.639936
114.872135	3449.792206	23.644954
114.344496	3456.014251	23.649971
114.626332	3449.266111	23.654989
114.706002	3453.588182	23.660007
114.510620	3460.900632	23.665024
114.787900	3463.607517	23.670042
114.699617	3477.564455	23.675059
114.896626	3479.715274	23.680077
115.293583	3498.879538	23.685095
114.855130	3512.885032	23.690112
115.246741	3512.873849	23.695130
115.392917	3522.819477	23.700147
115.627090	3526.721058	23.705165
115.947515	3540.303261	23.710183
115.992747	3538.904364	23.715200
116.228575	3534.079790	23.720218
116.252157	3536.453054	23.725235
116.340080	3521.094582	23.730253
116.410773	3540.772420	23.735271
116.058582	3560.132452	23.740288
116.816262	3556.569673	23.745306
116.995977	3566.103426	23.750323
117.235915	3552.341218	23.755341
117.295283	3544.040302	23.760359
117.483071	3559.368317	23.765376
118.081789	3549.111333	23.770394
117.908651	3552.225131	23.775411
117.698155	3553.083021	23.780429
117.880914	3549.552823	23.785447
117.707085	3554.033836	23.790464
117.924356	3549.733655	23.795482
118.081079	3570.818331	23.800499
118.620095	3568.237541	23.805517
118.631864	3563.307516	23.810535
118.690149	3571.481676	23.815552
118.644950	3565.458581	23.820570
118.768732	3576.478952	23.825587
118.561960	3572.651777	23.830605
119.005380	3566.731667	23.835623
118.721930	3574.443443	23.840640
119.095605	3571.475014	23.845658
119.244519	3588.761710	23.850675
119.231251	3596.884729	23.855693
119.294491	3588.300434	23.860711
118.881122	3593.473562	23.865728
119.237433	3609.158814	23.870746
119.446725	3615.196307	23.875763
119.270542	3625.633223	23.880781
119.786070	3642.057602	23.885799
119.899930	3655.511879	23.890816
119.943597	3650.903360	23.895834
120.269992	3661.194879	23.900851
120.373931	3670.860155	23.905869
120.732986	3670.907125	23.910887
121.019949	3674.591709	23.915904
121.560445	3671.855519	23.920922
121.048454	3672.521173	23.925939
121.204072	3671.357959	23.930957
121.852387	3668.121966	23.935975
121.540160	3671.415922	23.940992
121.656508	3682.059596	23.946010
121.978139	3691.599067	23.951027
122.186495	3692.202161	23.956045
122.257452	3697.926324	23.961063
121.998941	3692.728366	23.966080
122.499274	3694.703390	23.971098
122.766020	3696.482409	23.976115
122.640840	3691.845919	23.981133
122.866323	3682.449961	23.986151
122.577781	3683.672795	23.991168
122.768357	3681.227245	23.996186
122.638906	3687.209810	24.001203
122.896774	3695.581731	24.006221
122.765395	3711.343891	24.011239
122.401962	3718.525994	24.016256
122.692972	3716.401257	24.021274
122.784996	3741.569474	24.026291
122.808098	3750.255527	24.031309
123.524756	3770.769751	24.036327
123.216326	3781.067618	24.041344
123.474989	3779.782598	24.046362
123.787051	3789.628481	24.051379
124.169836	3804.616930	24.056397
124.609952	3797.823536	24.061415
124.591051	3807.621454	24.066432
125.135596	3803.873800	24.071450
124.990712	3797.823413	24.076467
124.659059	3793.695159	24.081485
125.208831	3792.555670	24.086503
125.297482	3798.590763	24.091520
125.393546	3796.106111	24.096538
125.355045	3787.586196	24.101555
125.372848	3808.608353	24.106573
125.689040	3808.374979	24.111591
125.645344	3820.807698	24.116608
125.400961	3815.091539	24.121626
125.682186	3812.805788	24.126643
125.752988	3818.767850	24.131661
126.244756	3834.373414	24.136679
126.143428	3847.830014	24.141696
126.347656	3841.135900	24.146714
126.688755	3837.940498	24.151731
126.532909	3846.744433	24.156749
126.762999	3862.120475	24.161767
126.786624	3873.682516	24.166784
126.953981	3870.693458	24.171802
127.405222	3867.473909	24.176819
127.353205	3872.572732	24.181837
127.419126	3883.220166	24.186855
127.563329	3899.202676	24.191872
127.941408	3898.364480	24.196890
127.914072	3890.793194	24.201907
127.807283	3901.036099	24.206925
128.111373	3895.377946	24.211943
128.221603	3895.199933	24.216960
128.791649	3910.575654	24.221978
128.863248	3905.601753	24.226995
128.649989	3914.136056	24.232013
128.714184	3911.128237	24.237031
128.929688	3913.514279	24.242048
128.827173	3908.508564	24.247066
129.178229	3911.450990	24.252083
129.134625	3936.503765	24.257101
129.374596	3939.944973	24.262119
129.232014	3940.931030	24.267136
129.518468	3939.025950	24.272154
129.497774	3960.632724	24.277171
129.682285	3974.407518	24.282189
129.681318	3963.571494	24.287207
129.887604	3978.331812	24.292224
130.239691	3990.084085	24.297242
130.367083	4006.816847	24.302259
130.132605	4014.477416	24.307277
130.722735	4008.207213	24.312295
130.754271	4022.301122	24.317312
130.659456	4026.203351	24.322330
131.119645	4026.988028	24.327347
130.970710	4030.418042	24.332365
131.254963	4044.455955	24.337383
131.418288	4056.515951	24.342400
131.222044	4059.841974	24.347418
131.512999	4054.153651	24.352435
131.829821	4064.787233	24.357453
132.019779	4074.939383	24.362471
132.245633	4085.898326	24.367488
132.426386	4090.377094	24.372506
132.642862	4082.046339	24.377523
132.460197	4089.681828	24.382541
132.544882	4083.864626	24.387559
132.998827	4100.020506	24.392576
132.960130	4105.833456	24.397594
132.907012	4107.653666	24.402611
133.190341	4113.523559	24.407629
133.240601	4116.796971	24.412647
133.376114	4119.633366	24.417664
133.234771	4111.876878	24.422682
133.470705	4118.412205	24.427699
133.909320	4133.710677	24.432717
133.861670	4135.859960	24.437735
133.967828	4140.581051	24.442752
133.736387	4142.037024	24.447770
134.146343	4150.030409	24.452787
134.146019	4156.885227	24.457805
134.571955	4153.909614	24.462823
134.914205	4160.641566	24.467840
134.426305	4186.478649	24.472858
135.350929	4184.057581	24.477875
135.002554	4183.538100	24.482893
135.317319	4186.929967	24.487911
135.485097	4184.112855	24.492928
135.687999	4200.979803	24.497946
135.715510	4214.954059	24.502963
135.897529	4223.581382	24.507981
136.042626	4213.176198	24.512999
136.020216	4218.717944	24.518016
135.886245	4222.120320	24.523034
136.417475	4232.060929	24.528051
136.423130	4245.171755	24.533069
136.626777	4238.897719	24.538087
136.590779	4242.054707	24.543104
136.645811	4262.187694	24.548122
136.968582	4270.523191	24.553139
137.081264	4278.443790	24.558157
137.117181	4269.790800	24.563175
137.199346	4285.822564	24.568192
137.478972	4297.954058	24.573210
137.737578	4296.627660	24.578227
137.980663	4303.028000	24.583245
138.009355	4315.531029	24.588263
138.296735	4324.689878	24.593280
138.281191	4320.306752	24.598298
138.709107	4314.186929	24.603315
138.693607	4323.933810	24.608333
138.803511	4320.273352	24.613351
139.035141	4322.972590	24.618368
138.742951	4340.367401	24.623386
139.431181	4328.603496	24.628403
139.585813	4332.948840	24.633421
139.588003	4334.398440	24.638439
139.666165	4333.525609	24.643456
140.000707	4334.084607	24.648474
140.175587	4346.357911	24.653491
140.438817	4353.825990	24.658509
140.416607	4361.457885	24.663527
140.457770	4353.311157	24.668544
140.169358	4351.898121	24.673562
140.255794	4351.409814	24.678579
140.628309	4364.469454	24.683597
140.610473	4379.512181	24.688615
140.957972	4375.758034	24.693632
141.040449	4379.355359	24.698650
141.433609	4377.568807	24.703667
141.324886	4398.388252	24.708685
141.260560	4410.325550	24.713703
141.615624	4410.585037	24.718720
141.680274	4419.657960	24.723738
141.875585	4414.219243	24.728755
141.712126	4439.162718	24.733773
142.110002	4439.007957	24.738791
142.353956	4441.705964	24.743808
141.914541	4436.006114	24.748826
142.261038	4448.769290	24.753843
142.363775	4467.456586	24.758861
142.542773	4471.739656	24.763879
142.803080	4482.048172	24.768896
142.661701	4490.605537	24.773914
143.213783	4484.777748	24.778931
143.411904	4507.788684	24.783949
143.744990	4513.117320	24.788967
144.169704	4516.176826	24.793984
144.579257	4519.715309	24.799002
144.855887	4510.241874	24.804019
144.698440	4507.726626	24.809037
144.888336	4511.455044	24.814055
145.116885	4507.987538	24.819072
144.935050	4508.761190	24.824090
145.175891	4509.164022	24.829107
145.169140	4511.238856	24.834125
145.223095	4512.108929	24.839143
145.211415	4503.625138	24.844160
145.239347	4507.232310	24.849178
145.642860	4514.501619	24.854195
145.554704	4525.691629	24.859213
145.505775	4535.835588	24.864231
145.560690	4542.271903	24.869248
145.425197	4544.301114	24.874266
145.911393	4559.344836	24.879283
146.071013	4570.500157	24.884301
146.104134	4588.261149	24.889319
146.461554	4589.752769	24.894336
146.584072	4601.923897	24.899354
146.892200	4612.852262	24.904371
146.947831	4626.022074	24.909389
146.829456	4630.670228	24.914407
147.650451	4631.095150	24.919424
147.668242	4649.429725	24.924442
147.800385	4653.240981	24.929459
147.699340	4655.400750	24.934477
147.729044	4657.760176	24.939495
147.996607	4660.755159	24.944512
148.245371	4673.569351	24.949530
148.427446	4670.965577	24.954547
148.801702	4679.342385	24.959565
148.581839	4695.451347	24.964583
148.958343	4706.323566	24.969600
148.888194	4704.745991	24.974618
149.286148	4704.338411	24.979635
149.330418	4706.325280	24.984653
149.189415	4728.982366	24.989671
149.565956	4736.771308	24.994688
149.528538	4742.874103	24.999706
150.041461	4749.508749	25.004723
150.030594	4760.212806	25.009741
150.088432	4767.326819	25.014759
150.436271	4756.386037	25.019776
150.392285	4771.483871	25.024794
150.926975	4774.337782	25.029811
150.842412	4788.216118	25.034829
150.749085	4786.815635	25.039847
151.294925	4785.381004	25.044864
151.236214	4803.963118	25.049882
151.163143	4802.503363	25.054899
151.568982	4806.430796	25.059917
151.409539	4815.384321	25.064935
152.193373	4819.022361	25.069952
152.268070	4846.222011	25.074970
152.618464	4839.394200	25.079987
152.588745	4837.341317	25.085005
152.435008	4829.351831	25.090023
152.739287	4827.623261	25.095040
152.729888	4836.262134	25.100058
152.636382	4840.874731	25.105075
153.183756	4860.896261	25.110093
153.006985	4861.961278	25.115111
153.382372	4851.728615	25.120128
153.087347	4863.172056	25.125146
153.760812	4883.918566	25.130163
153.759184	4886.846324	25.135181
153.647703	4890.612913	25.140199
153.977627	4895.340503	25.145216
154.244990	4917.480553	25.150234
154.372717	4919.375664	25.155251
154.651170	4916.417240	25.160269
154.857361	4932.328323	25.165287
154.995963	4936.253564	25.170304
155.202485	4944.003813	25.175322
155.574704	4941.609512	25.180339
155.385648	4936.236612	25.185357
155.465595	4945.275016	25.190375
155.918685	4959.151912	25.195392
155.905752	4964.371023	25.200410
156.328239	4956.492421	25.205427
156.387245	4970.615710	25.210445
156.276456	4973.332373	25.215463
156.511200	4975.019969	25.220480
156.843854	4985.193191	25.225498
157.014910	4987.492249	25.230515
157.157604	4989.209262	25.235533
156.871815	4992.871634	25.240551
157.325301	4996.422643	25.245568
157.349146	5018.350339	25.250586
157.342362	5021.590854	25.255603
157.637023	5020.726249	25.260621
157.693128	5041.161697	25.265639
157.957973	5051.649404	25.270656
157.818993	5056.234938	25.275674
158.070557	5068.019628	25.280691
158.433328	5074.365817	25.285709
158.595270	5077.713874	25.290727
158.702533	5092.432567	25.295744
158.947309	5108.122431	25.300762
158.867955	5103.892202	25.305779
159.303821	5110.216854	25.310797
159.637963	5127.874277	25.315815
160.242660	5124.738154	25.320832
159.949605	5125.679887	25.325850
159.715299	5123.923888	25.330867
160.459752	5130.967712	25.335885
160.307886	5155.073991	25.340903
160.684350	5156.795639	25.345920
160.359338	5161.801066	25.350938
160.698656	5158.697057	25.355955
161.184604	5174.027304	25.360973
161.216678	5172.639104	25.365991
161.703987	5175.537951	25.371008
161.498577	5178.019863	25.376026
161.659585	5171.299658	25.381043
161.812577	5179.119529	25.386061
161.703473	5200.337037	25.391079
162.154613	5199.166138	25.396096
162.065150	5203.867955	25.401114
162.209985	5225.323049	25.406131
162.494667	5227.465505	25.411149
162.725818	5233.972163	25.416167
162.863753	5225.038706	25.421184
163.378705	5234.246261	25.426202
163.390134	5242.440074	25.431219
163.845223	5252.363226	25.436237
163.648032	5259.779585	25.441255
163.810854	5250.953043	25.446272
163.965517	5250.339215	25.451290
163.901691	5246.989260	25.456307
164.105617	5241.619716	25.461325
164.313083	5263.752842	25.466343
164.167474	5270.395922	25.471360
164.710082	5274.882858	25.476378
164.429016	5284.930264	25.481395
164.821190	5292.219141	25.486413
164.743823	5310.661600	25.491431
165.350469	5302.367209	25.496448
165.173639	5323.127479	25.501466
165.544785	5332.922813	25.506483
165.797722	5336.262950	25.511501
165.498405	5350.507332	25.516519
165.955261	5368.931513	25.521536
166.025435	5377.468513	25.526554
165.868132	5389.222683	25.531571
166.443048	5401.726721	25.536589
166.447563	5398.378021	25.541607
166.655623	5424.243675	25.546624
166.979292	5435.934007	25.551642
166.915467	5434.495503	25.556659
167.488535	5446.454867	25.561677
167.753824	5455.336077	25.566695
168.164177	5449.135243	25.571712
168.112490	5455.950299	25.576730
168.123662	5480.489251	25.581747
168.912404	5478.564633	25.586765
168.557024	5482.011021	25.591783
168.710933	5474.569637	25.596800
168.687606	5485.164410	25.601818
168.762015	5506.752048	25.606835
169.024036	5506.389009	25.611853
169.212921	5506.425575	25.616871
169.368930	5531.224163	25.621888
169.701598	5541.414284	25.626906
169.606895	5540.167542	25.631923
170.235734	5543.588837	25.636941
170.265291	5557.982161	25.641959
170.295743	5559.533520	25.646976
170.735388	5559.220622	25.651994
170.770596	5573.030988	25.657011
171.265686	5587.637895	25.662029
171.064713	5595.666217	25.667047
171.438755	5599.018653	25.672064
171.588038	5590.771475	25.677082
171.737124	5601.969441	25.682100
171.853289	5604.651002	25.687117
171.791595	5614.500053	25.692135
171.791092	5609.819515	25.697152
171.748869	5613.143991	25.702170
171.680122	5638.306023	25.707188
172.258945	5650.665482	25.712205
172.508754	5666.579537	25.717223
172.513222	5684.044067	25.722240
172.492341	5687.741501	25.727258
173.030974	5701.164622	25.732276
173.263967	5721.496844	25.737293
173.516255	5719.616115	25.742311
173.606130	5734.368215	25.747328
173.576158	5732.691734	25.752346
174.046334	5749.957160	25.757364
174.619976	5747.999600	25.762381
174.433079	5750.970003	25.767399
174.811874	5750.961742	25.772416
175.215467	5773.059965	25.777434
174.708902	5785.677975	25.782452
175.260978	5780.178942	25.787469
175.323552	5784.120920	25.792487
175.650022	5778.670262	25.797504
175.641398	5786.771589	25.802522
175.816380	5806.449569	25.807540
175.811779	5810.531055	25.812557
175.841968	5814.235817	25.817575
176.412629	5819.517696	25.822592
176.643097	5825.971155	25.827610
176.512497	5833.314537	25.832628
177.067449	5841.178460	25.837645
177.521665	5856.311422	25.842663
177.651121	5855.295336	25.847680
177.700926	5849.545480	25.852698
177.941843	5856.765147	25.857716
177.883227	5848.225393	25.862733
178.287340	5853.111118	25.867751
178.158690	5865.795010	25.872768
178.725285	5869.908758	25.877786
178.724230	5885.212419	25.882804
178.534568	5879.599860	25.887821
178.945396	5889.153475	25.892839
179.246230	5897.502135	25.897856
179.509005	5898.414904	25.902874
179.203360	5901.149018	25.907892
179.747941	5920.112230	25.912909
179.965159	5927.022381	25.917927
180.028630	5935.193761	25.922944
180.203450	5934.858539	25.927962
180.273377	5946.172245	25.932980
180.444219	5959.842352	25.937997
180.552096	5966.473688	25.943015
180.661724	5976.674236	25.948032
181.261149	5982.119959	25.953050
180.875146	6000.489871	25.958068
181.293954	6003.705815	25.963085
181.561218	6011.385101	25.968103
181.680908	6020.224574	25.973120
182.144571	6023.617400	25.978138
182.213726	6033.389129	25.983156
182.763294	6035.716259	25.988173
182.760221	6041.950916	25.993191
183.058430	6038.330563	25.998208
183.404195	6028.241459	26.003226
183.184543	6043.166382	26.008244
183.615258	6054.040803	26.013261
183.571857	6058.985712	26.018279
183.629956	6067.320301	26.023296
183.882367	6055.543000	26.028314
183.619686	6071.994403	26.033332
184.097284	6090.983088	26.038349
184.265409	6098.564623	26.043367
184.548048	6115.826842	26.048384
184.752750	6118.573384	26.053402
185.072234	6128.839318	26.058420
185.196029	6120.293636	26.063437
185.450947	6127.698566	26.068455
185.564730	6148.523651	26.073472
185.931756	6137.504706	26.078490
185.686220	6148.717980	26.083508
186.214720	6162.878032	26.088525
186.454457	6180.362446	26.093543
186.075195	6179.724342	26.098560
186.786146	6173.879097	26.103578
186.508668	6183.063232	26.108596
186.795411	6196.986090	26.113613
186.976133	6205.591876	26.118631
187.085718	6210.438257	26.123648
187.234674	6211.324992	26.128666
187.615594	6229.683203	26.133684
187.788404	6233.363665	26.138701
187.864322	6235.285629	26.143719
187.784369	6264.813217	26.148736
188.266120	6264.761923	26.153754
188.334417	6272.008783	26.158772
188.462428	6285.960360	26.163789
188.845493	6286.553149	26.168807
188.882475	6300.396150	26.173824
189.470963	6324.850291	26.178842
189.130384	6321.922413	26.183860
189.479992	6337.943497	26.188877
189.888317	6357.076294	26.193895
189.460542	6364.984233	26.198912
190.248867	6366.236142	26.203930
190.457584	6379.665626	26.208948
190.386049	6393.246271	26.213965
190.945487	6405.713504	26.218983
191.033875	6421.138351	26.224000
191.112065	6410.524622	26.229018
191.160078	6434.782492	26.234036
191.409156	6438.285760	26.239053
191.735653	6446.722618	26.244071
191.668822	6474.079251	26.249088
192.259399	6474.959843	26.254106
192.494678	6471.924004	26.259124
192.690027	6489.015984	26.264141
193.104642	6490.013136	26.269159
193.088344	6491.710164	26.274176
193.478502	6494.177963	26.279194
193.481903	6517.252423	26.284212
193.508266	6519.578812	26.289229
193.579262	6524.814474	26.294247
193.675681	6536.053328	26.299264
194.189472	6542.057691	26.304282
194.321147	6551.422414	26.309300
194.393992	6567.900701	26.314317
194.883834	6568.704245	26.319335
194.973963	6579.580276	26.324352
195.259494	6589.617412	26.329370
195.387765	6603.184064	26.334388
195.710793	6603.005454	26.339405
196.553490	6601.871250	26.344423
196.150420	6617.005872	26.349440
196.588467	6621.131650	26.354458
196.306441	6615.798770	26.359476
196.643017	6616.161398	26.364493
197.032124	6615.606379	26.369511
197.174029	6634.848205	26.374528
197.440992	6641.266815	26.379546
197.453642	6643.626999	26.384564
197.445683	6644.816202	26.389581
197.936452	6659.708378	26.394599
197.068404	6674.630959	26.399616
197.753725	6679.124612	26.404634
197.971873	6693.598808	26.409652
198.006678	6716.168984	26.414669
198.444469	6720.530340	26.419687
198.592283	6741.034720	26.424704
198.743795	6745.085090	26.429722
198.824383	6770.739327	26.434740
198.947554	6786.931466	26.439757
199.403102	6795.989881	26.444775
199.492950	6803.465776	26.449792
199.831469	6817.011196	26.454810
200.463849	6824.016848	26.459828
200.538727	6834.545856	26.464845
200.798872	6825.451064	26.469863
200.583503	6849.333344	26.474880
201.451950	6848.001097	26.479898
201.557043	6851.370759	26.484916
201.517500	6854.932927	26.489933
201.874617	6852.914989	26.494951
201.753418	6872.155761	26.499968
201.959530	6873.755362	26.504986
202.126096	6871.279038	26.510004
202.294375	6897.965772	26.515021
202.657040	6905.098815	26.520039
202.733974	6905.969944	26.525056
202.640663	6918.226636	26.530074
203.064779	6920.345459	26.535092
202.955079	6935.568873	26.540109
203.675664	6949.864821	26.545127
203.692169	6960.109775	26.550144
204.122031	6978.262261	26.555162
204.477719	6983.524988	26.560180
204.328791	6998.016907	26.565197
204.547307	7002.851800	26.570215
204.674074	7029.559805	26.575232
204.885595	7026.480535	26.580250
205.291131	7045.429525	26.585268
205.486514	7051.322958	26.590285
205.785169	7057.780601	26.595303
206.082896	7073.625128	26.600320
206.472368	7079.732985	26.605338
206.502405	7073.303832	26.610356
206.537179	7090.979142	26.615373
206.743732	7103.569147	26.620391
206.779032	7111.828504	26.625408
206.833981	7129.416236	26.630426
207.352178	7129.286446	26.635444
207.641116	7138.662504	26.640461
208.043477	7157.006428	26.645479
207.754022	7172.474861	26.650496
207.848885	7171.561304	26.655514
207.947491	7190.670764	26.660532
208.249588	7201.337267	26.665549
208.777306	7223.973863	26.670567
208.926642	7225.749101	26.675584
209.218376	7247.171591	26.680602
209.942719	7255.018426	26.685620
209.455491	7259.246344	26.690637
209.984298	7270.823737	26.695655
209.838127	7284.642776	26.700672
210.544004	7290.629021	26.705690
210.686527	7307.197364	26.710708
210.655935	7316.983246	26.715725
211.269540	7320.420066	26.720743
211.496372	7331.500049	26.725760
211.613878	7341.607225	26.730778
211.868959	7347.232524	26.735796
212.086468	7347.064288	26.740813
212.073545	7338.057732	26.745831
212.188518	7371.315534	26.750848
212.454200	7371.413440	26.755866
212.870847	7369.086263	26.760884
212.423347	7390.354052	26.765901
213.144016	7386.870627	26.770919
213.070265	7404.913198	26.775936
213.166480	7415.042849	26.780954
213.645617	7418.105742	26.785972
213.920129	7435.629896	26.790989
214.185320	7439.986944	26.796007
214.323573	7452.178144	26.801024
214.222347	7459.181067	26.806042
214.775750	7464.634931	26.811060
214.633872	7485.511182	26.816077
214.741859	7488.658372	26.821095
214.853562	7504.050478	26.826112
215.055503	7514.707778	26.831130
215.739568	7529.195407	26.836148
216.025266	7545.578820	26.841165
216.500205	7536.978977	26.846183
216.195661	7561.882189	26.851200
216.447905	7563.198531	26.856218
216.862693	7573.918310	26.861236
216.745375	7593.808375	26.866253
217.015692	7591.043798	26.871271
217.250813	7619.104669	26.876288
217.311423	7624.450329	26.881306
217.553358	7640.591382	26.886324
217.870085	7652.100185	26.891341
218.288778	7675.582564	26.896359
218.405160	7687.399466	26.901376
218.654701	7699.041520	26.906394
219.402450	7707.077696	26.911412
219.223633	7712.732415	26.916429
219.674755	7724.433280	26.921447
219.626068	7737.374034	26.926464
220.213229	7744.377345	26.931482
220.446036	7757.436148	26.936500
220.477800	7778.559737	26.941517
220.711391	7776.705499	26.946535
220.848952	7790.912037	26.951552
220.621290	7805.771404	26.956570
220.906353	7812.436412	26.961588
221.003444	7846.303128	26.966605
221.228288	7853.234916	26.971623
221.683477	7862.610665	26.976640
221.708561	7883.162041	26.981658
222.532171	7894.548514	26.986676
222.502857	7908.142367	26.991693
222.831926	7911.979318	26.996711
223.394991	7928.854435	27.001728
223.458402	7925.650633	27.006746
224.172881	7931.617584	27.011764
224.552760	7945.302063	27.016781
224.671981	7946.760979	27.021799
224.771507	7945.339316	27.026816
224.612673	7946.087262	27.031834
224.814088	7947.503425	27.036852
224.800190	7968.383541	27.041869
225.048952	7965.099423	27.046887
225.492883	7978.143152	27.051904
225.529360	7999.948419	27.056922
226.002682	8002.139596	27.061940
226.009026	8023.634007	27.066957
226.189689	8034.947412	27.071975
226.634694	8035.834085	27.076992
226.405099	8057.762248	27.082010
226.685900	8066.429676	27.087028
226.882957	8086.584979	27.092045
227.262646	8092.585355	27.097063
227.380572	8108.777345	27.102080
227.240455	8126.970358	27.107098
227.702936	8139.210817	27.112116
228.014054	8162.120926	27.117133
228.459497	8165.223417	27.122151
228.664335	8174.071265	27.127168
228.645238	8181.759624	27.132186
229.505035	8187.210287	27.137204
229.362744	8198.480378	27.142221
229.628705	8213.838182	27.147239
230.123328	8222.400192	27.152256
230.051217	8222.943951	27.157274
230.432808	8228.149242	27.162292
230.286741	8248.968103	27.167309
230.382925	8256.606694	27.172327
230.886342	8270.043349	27.177344
231.121817	8289.138559	27.182362
231.413436	8294.038157	27.187380
231.385901	8317.543360	27.192397
231.899928	8312.833570	27.197415
231.985207	8329.335254	27.202432
231.842408	8338.657453	27.207450
232.714647	8342.361271	27.212468
232.972747	8356.868969	27.217485
233.003710	8357.343679	27.222503
233.509477	8376.649480	27.227520
233.763115	8393.291150	27.232538
233.723787	8380.076327	27.237556
233.816630	8405.549201	27.242573
234.072809	8418.979643	27.247591
234.305439	8426.750914	27.252608
234.269757	8453.341677	27.257626
234.824957	8464.795839	27.262644
234.436420	8486.344422	27.267661
234.886151	8502.929326	27.272679
235.436888	8516.358356	27.277696
235.377706	8547.908882	27.282714
235.584762	8547.662018	27.287732
236.157308	8576.576992	27.292749
236.297225	8592.820187	27.297767
236.861639	8599.741781	27.302784
237.096257	8610.412524	27.307802
237.647053	8618.974904	27.312820
237.917669	8634.485167	27.317837
237.753692	8633.109426	27.322855
237.802252	8651.776751	27.327872
238.197380	8674.008825	27.332890
238.663952	8677.703464	27.337908
238.999618	8690.908284	27.342925
238.929386	8695.622125	27.347943
239.290073	8713.216136	27.352960
239.188310	8724.681553	27.357978
239.542485	8740.809869	27.362996
239.685056	8760.380284	27.368013
240.193743	8780.721207	27.373031
240.410719	8788.598442	27.378048
240.601684	8797.098379	27.383066
240.868602	8806.246679	27.388084
241.308494	8816.217135	27.393101
241.432863	8831.283080	27.398119
241.685607	8843.711627	27.403136
241.957205	8859.978987	27.408154
242.094285	8865.524313	27.413172
242.559350	8873.433786	27.418189
242.521223	8891.117642	27.423207
243.021863	8901.475917	27.428224
242.957020	8915.581465	27.433242
243.072168	8931.053154	27.438260
243.549569	8934.642076	27.443277
243.875258	8957.869961	27.448295
244.143367	8964.104199	27.453312
244.234572	8975.788364	27.458330
244.668647	8986.444461	27.463348
244.857973	8997.754752	27.468365
244.636757	9001.044178	27.473383
244.989414	9020.449366	27.478400
245.247067	9033.748524	27.483418
245.537855	9047.926090	27.488436
245.779659	9061.936103	27.493453
245.818335	9073.235935	27.498471
246.337213	9082.474245	27.503488
246.298912	9103.293708	27.508506
246.448798	9117.855460	27.513524
246.890519	9134.016161	27.518541
247.136165	9156.414662	27.523559
247.696555	9165.338916	27.528576
247.880549	9177.070890	27.533594
247.945375	9182.591261	27.538612
248.744946	9201.386213	27.543629
248.668059	9207.557912	27.548647
249.290350	9222.310984	27.553664
249.363008	9240.229764	27.558682
249.427133	9239.790699	27.563700
250.221627	9255.912035	27.568717
250.200543	9274.430906	27.573735
250.661410	9275.166139	27.578752
250.421485	9281.089917	27.583770
250.961415	9285.751773	27.588788
251.065759	9299.243540	27.593805
251.098309	9307.057026	27.598823
251.468948	9322.064548	27.603840
251.573886	9339.287207	27.608858
251.701253	9357.965156	27.613876
251.725262	9362.116868	27.618893
252.235326	9387.612048	27.623911
252.811781	9397.602016	27.628928
252.678687	9423.323460	27.633946
253.038731	9431.402639	27.638964
253.462294	9446.526777	27.643981
253.453991	9458.291576	27.648999
253.781225	9477.931563	27.654016
254.125921	9495.701610	27.659034
254.172498	9516.743109	27.664052
254.773965	9527.000807	27.669069
255.104976	9553.694193	27.674087
255.081531	9546.895545	27.679104
255.237889	9574.172484	27.684122
255.550850	9589.583704	27.689140
255.903729	9605.494887	27.694157
256.411605	9629.535748	27.699175
256.620901	9649.881643	27.704192
256.878966	9654.762795	27.709210
256.832716	9672.619021	27.714228
256.920409	9687.080506	27.719245
257.120265	9706.243965	27.724263
257.319588	9725.418564	27.729280
257.401904	9756.010552	27.734298
257.917822	9777.930314	27.739316
258.687853	9786.480670	27.744333
258.351503	9807.738770	27.749351
258.770712	9817.350096	27.754368
259.132369	9838.970110	27.759386
259.450855	9851.928211	27.764404
260.038026	9860.088183	27.769421
260.153120	9881.567871	27.774439
260.653136	9886.407469	27.779456
261.035855	9904.858649	27.784474
261.272499	9923.208768	27.789492
261.926082	9925.105676	27.794509
261.998149	9928.605146	27.799527
262.425697	9920.805215	27.804544
262.247758	9932.882842	27.809562
261.857759	9949.048898	27.814580
262.507531	9952.893137	27.819597
262.595526	9975.203856	27.824615
262.662109	9984.617612	27.829632
263.149288	9998.541347	27.834650
263.365664	10021.902315	27.839668
263.478392	10022.225672	27.844685
263.494680	10047.018178	27.849703
263.729996	10065.950092	27.854720
264.215542	10081.715312	27.859738
263.832910	10123.431038	27.864756
264.860644	10130.944688	27.869773
264.864023	10153.107368	27.874791
265.600135	10174.304239	27.879808
265.758044	10179.292730	27.884826
266.051937	10198.080385	27.889844
266.432767	10199.935815	27.894861
266.526660	10223.850710	27.899879
266.723405	10231.623286	27.904896
267.436282	10258.022223	27.909914
267.258639	10280.021234	27.914932
267.851451	10278.241187	27.919949
268.197342	10293.766596	27.924967
268.330280	10300.352259	27.929984
268.711349	10318.136892	27.935002
268.813951	10329.338000	27.940020
269.426732	10344.726317	27.945037
269.395504	10361.688201	27.950055
269.434981	10378.968504	27.955072
269.802738	10391.064868	27.960090
270.035559	10415.865431	27.965108
270.575147	10419.226169	27.970125
270.642845	10449.786442	27.975143
270.990851	10455.729143	27.980160
271.318694	10462.528417	27.985178
271.398642	10478.998529	27.990196
272.213421	10502.224903	27.995213
272.045378	10530.746017	28.000231
272.407791	10536.897507	28.005248
272.817592	10552.674940	28.010266
272.758045	10574.227791	28.015284
273.067928	10583.655986	28.020301
273.190577	10605.678216	28.025319
273.376355	10627.045566	28.030336
273.709517	10642.875166	28.035354
273.993664	10659.529109	28.040372
274.343174	10678.691803	28.045389
274.703966	10705.986456	28.050407
275.287878	10717.890504	28.055424
275.756472	10729.218031	28.060442
275.497191	10747.011438	28.065460
275.963501	10763.236681	28.070477
276.001774	10791.125333	28.075495
276.162849	10797.239342	28.080512
276.427579	10804.043693	28.085530
276.746498	10841.623916	28.090548
277.337890	10852.743693	28.095565
277.367564	10881.845655	28.100583
277.695438	10891.171782	28.105600
278.460543	10906.367610	28.110618
278.467349	10920.784501	28.115636
278.821551	10933.331812	28.120653
278.946355	10948.263369	28.125671
279.367003	10970.941124	28.130688
279.399281	10977.738328	28.135706
279.687030	11006.194290	28.140724
280.316507	11017.583632	28.145741
280.566574	11040.228266	28.150759
280.599484	11041.757693	28.155776
280.990199	11052.794221	28.160794
281.020941	11074.693639	28.165812
281.161750	11089.487162	28.170829
281.460865	11098.490415	28.175847
281.795629	11116.070869	28.180864
282.168654	11142.259636	28.185882
281.864478	11162.599465	28.190900
282.364445	11180.546583	28.195917
282.611842	11207.879763	28.200935
283.124077	11227.520418	28.205952
283.241797	11246.006758	28.210970
283.297322	11275.380907	28.215988
283.809776	11292.457837	28.221005
283.945673	11325.075879	28.226023
284.440625	11333.865635	28.231040
284.758599	11357.734876	28.236058
285.128858	11381.100706	28.241076
285.386247	11397.611717	28.246093
285.661491	11412.458922	28.251111
285.672123	11440.400540	28.256128
286.225233	11465.502675	28.261146
286.302255	11483.545349	28.266164
286.970857	11504.670060	28.271181
287.261263	11528.482661	28.276199
287.752558	11542.030441	28.281216
288.208424	11556.409812	28.286234
288.487596	11570.900383	28.291252
289.198229	11584.399288	28.296269
288.813839	11603.311093	28.301287
289.289065	11633.708448	28.306304
289.620404	11641.493306	28.311322
289.833102	11660.583689	28.316340
290.079815	11669.491931	28.321357
290.268311	11689.806025	28.326375
290.256874	11711.587220	28.331392
290.725393	11733.790108	28.336410
290.943677	11757.353400	28.341428
291.398436	11779.011821	28.346445
291.924410	11805.021916	28.351463
291.976269	11814.729914	28.356480
292.738106	11827.632768	28.361498
292.629919	11849.103968	28.366516
292.608583	11857.462598	28.371533
292.978140	11882.078893	28.376551
293.373605	11906.722453	28.381568
293.576209	11926.583822	28.386586
293.621320	11947.793404	28.391604
294.228154	11971.217054	28.396621
294.338783	11997.586159	28.401639
294.701545	12022.763213	28.406656
294.990642	12035.008567	28.411674
295.210160	12066.771187	28.416692
295.572136	12082.283837	28.421709
295.968635	12109.682107	28.426727
296.151444	12128.563673	28.431744
296.653533	12154.381302	28.436762
296.772860	12178.272026	28.441780
297.199782	12194.229455	28.446797
297.389716	12216.849443	28.451815
297.668188	12241.047999	28.456832
298.364011	12259.323195	28.461850
298.347643	12282.667648	28.466868
298.929277	12295.118492	28.471885
299.132665	12317.315637	28.476903
299.649922	12326.073879	28.481920
299.880285	12350.195464	28.486938
299.988526	12365.179920	28.491956
300.158086	12379.711420	28.496973
300.633606	12393.587157	28.501991
300.511712	12412.346140	28.507008
300.993353	12422.857974	28.512026
301.358464	12451.525868	28.517044
301.716467	12457.590577	28.522061
302.187307	12479.362313	28.527079
301.978568	12507.066297	28.532096
302.475284	12517.897178	28.537114
302.474063	12558.533280	28.542132
302.697107	12564.369800	28.547149
303.350658	12585.566180	28.552167
303.629177	12622.804221	28.557184
303.868928	12633.669833	28.562202
304.181927	12667.370688	28.567220
304.620839	12684.034194	28.572237
305.085577	12699.415386	28.577255
305.057933	12725.313724	28.582272
305.591684	12743.600534	28.587290
305.815742	12776.172229	28.592308
306.199132	12792.172123	28.597325
306.495378	12819.006672	28.602343
306.900796	12831.975631	28.607360
307.345903	12854.273757	28.612378
307.453822	12877.418836	28.617396
307.747447	12902.958552	28.622413
308.313102	12915.716673	28.627431
308.342707	12944.619048	28.632448
309.023789	12959.268119	28.637466
309.381718	12986.551331	28.642484
309.726410	12991.572026	28.647501
309.985361	13008.172672	28.652519
310.152665	13033.166166	28.657536
310.677216	13046.095090	28.662554
310.975600	13070.182845	28.667572
311.194943	13085.636540	28.672589
311.286604	13099.883725	28.677607
311.352815	13129.535244	28.682624
311.736371	13146.581886	28.687642
311.728932	13176.198401	28.692660
312.296568	13200.029030	28.697677
312.781092	13227.784964	28.702695
312.624220	13259.125240	28.707712
313.085457	13273.139627	28.712730
313.528406	13302.087688	28.717748
314.071169	13332.793815	28.722765
314.694819	13346.984683	28.727783
314.848235	13380.092496	28.732800
314.968681	13394.005796	28.737818
314.985399	13421.196493	28.742836
315.420684	13433.659830	28.747853
316.323462	13463.784969	28.752871
316.422396	13480.113146	28.757888
316.759239	13494.493451	28.762906
317.300922	13523.498060	28.767924
317.191154	13532.491545	28.772941
317.449838	13557.661412	28.777959
317.677126	13581.372421	28.782976
318.241719	13601.541550	28.787994
318.539935	13625.266099	28.793012
318.645017	13652.882258	28.798029
319.023990	13671.148451	28.803047
319.031235	13703.910754	28.808064
319.390634	13728.522071	28.813082
319.748858	13753.954716	28.818100
320.242041	13775.651994	28.823117
320.698831	13796.116583	28.828135
320.602652	13827.157915	28.833152
321.338664	13832.760269	28.838170
321.570276	13863.982243	28.843188
321.896081	13891.111531	28.848205
322.240859	13910.255188	28.853223
322.311473	13923.184295	28.858240
322.731198	13947.114572	28.863258
322.684895	13969.500288	28.868276
322.986386	13994.504564	28.873293
323.629848	14017.376647	28.878311
323.972253	14051.302442	28.883328
324.403036	14072.378454	28.888346
324.874009	14098.202743	28.893364
325.062227	14120.600283	28.898381
325.535994	14140.116871	28.903399
325.496427	14169.225135	28.908416
326.104740	14186.757335	28.913434
326.190079	14220.018383	28.918452
326.654330	14248.050489	28.923469
326.946244	14271.126110	28.928487
327.012852	14300.987724	28.933504
327.664491	14322.995204	28.938522
327.879668	14345.115931	28.943540
328.440948	14381.218972	28.948557
329.065171	14395.264087	28.953575
329.323064	14415.592158	28.958592
329.622014	14433.286151	28.963610
330.064671	14454.442647	28.968628
330.041431	14488.677309	28.973645
330.530853	14503.822864	28.978663
330.385502	14536.052579	28.983680
330.724279	14547.068566	28.988698
331.332519	14577.517175	28.993716
331.738416	14609.977318	28.998733
332.144198	14632.393135	29.003751
332.408936	14660.405382	29.008768
332.793291	14678.553604	29.013786
333.168501	14705.767478	29.018804
333.103129	14732.447521	29.023821
333.768111	14760.946904	29.028839
333.812124	14789.112534	29.033856
334.197815	14820.414850	29.038874
334.660893	14850.099940	29.043892
334.866877	14874.025969	29.048909
335.784630	14889.134087	29.053927
336.230325	14923.602536	29.058944
336.608390	14922.225584	29.063962
336.929103	14950.728691	29.068980
337.001763	14969.192035	29.073997
337.544870	14995.664619	29.079015
337.546084	15017.125019	29.084032
337.818469	15045.864827	29.089050
338.210739	15059.865371	29.094068
338.519797	15093.894986	29.099085
338.827118	15105.320045	29.104103
339.075617	15141.662512	29.109120
339.460862	15170.306628	29.114138
339.961558	15184.224711	29.119156
340.112476	15222.916197	29.124173
340.615279	15225.979066	29.129191
340.618051	15263.606050	29.134208
340.979068	15283.763666	29.139226
341.732638	15308.581639	29.144244
341.726496	15346.620089	29.149261
342.185850	15362.334103	29.154279
342.567616	15394.662666	29.159296
342.935178	15421.521204	29.164314
343.388550	15445.824804	29.169332
343.312849	15468.663481	29.174349
343.710907	15492.763523	29.179367
344.271852	15517.320526	29.184384
344.288701	15542.246600	29.189402
344.473972	15563.075149	29.194420
344.710270	15594.438341	29.199437
345.478592	15620.092872	29.204455
345.726600	15653.043030	29.209472
346.052495	15665.896581	29.214490
346.480348	15687.988644	29.219508
346.911416	15719.587791	29.224525
347.315230	15755.904332	29.229543
347.334287	15774.290759	29.234560
347.774829	15796.171234	29.239578
348.213664	15829.104346	29.244596
348.571069	15855.079446	29.249613
349.095890	15878.810732	29.254631
349.259599	15907.558997	29.259648
349.492875	15938.721590	29.264666
350.191990	15960.012541	29.269684
349.922472	15995.383410	29.274701
350.535169	16030.053512	29.279719
351.042180	16051.866581	29.284736
351.245465	16083.269267	29.289754
351.759332	16114.984719	29.294772
351.956368	16147.072644	29.299789
352.863471	16174.629652	29.304807
353.241975	16196.766819	29.309824
353.532595	16221.399562	29.314842
353.454306	16238.089245	29.319860
354.022927	16272.951573	29.324877
354.390736	16294.844748	29.329895
354.830589	16318.756236	29.334912
355.006221	16350.055245	29.339930
355.734855	16375.216276	29.344948
355.764691	16398.837930	29.349965
356.227538	16418.905999	29.354983
356.242416	16459.279544	29.360000
356.853874	16487.875901	29.365018
357.463547	16513.750389	29.370036
357.603656	16543.127867	29.375053
357.955306	16566.513652	29.380071
358.222353	16602.116994	29.385088
358.293895	16628.200521	29.390106
359.003181	16659.060282	29.395124
359.346131	16698.027662	29.400141
359.503250	16718.089947	29.405159
360.236830	16745.053996	29.410176
360.633994	16770.412356	29.415194
361.283690	16796.848129	29.420212
361.359763	16825.973466	29.425229
361.567846	16845.335476	29.430247
362.153256	16873.653078	29.435264
362.196117	16901.983284	29.440282
362.609254	16925.353095	29.445300
363.088651	16969.256015	29.450317
363.419188	16994.457081	29.455335
363.910494	17012.013246	29.460352
364.182319	17052.214875	29.465370
364.792508	17073.834096	29.470388
364.871858	17105.505139	29.475405
365.234019	17124.012828	29.480423
365.603548	17158.832735	29.485440
365.904122	17177.205654	29.490458
366.342869	17210.828814	29.495476
366.523908	17237.629748	29.500493
367.197730	17266.045310	29.505511
367.230263	17295.650002	29.510528
367.217990	17329.562429	29.515546
368.033115	17334.785624	29.520564
368.246841	17365.739754	29.525581
369.072257	17388.127704	29.530599
369.307463	17417.850400	29.535616
369.519213	17445.251907	29.540634
370.320585	17454.237025	29.545652
370.319978	17486.768531	29.550669
370.812544	17510.433412	29.555687
371.290807	17526.379665	29.560704
371.358197	17556.368413	29.565722
372.257744	17576.050339	29.570740
372.332331	17609.034668	29.575757
372.620043	17624.388308	29.580775
373.139823	17644.692780	29.585792
373.277764	17666.994686	29.590810
373.437805	17694.791374	29.595828
374.104749	17733.193666	29.600845
374.188057	17760.952720	29.605863
374.571143	17788.205054	29.610880
374.996835	17827.427803	29.615898
375.430788	17855.253517	29.620916
375.807784	17885.347682	29.625933
375.935018	17908.539195	29.630951
376.565302	17933.007920	29.635968
376.616222	17970.223215	29.640986
377.251745	17998.580163	29.646004
377.544794	18039.250436	29.651021
377.897350	18063.727484	29.656039
378.679843	18086.681534	29.661056
378.755402	18135.132972	29.666074
379.229903	18155.536996	29.671092
379.882309	18192.517669	29.676109
380.074518	18220.633078	29.681127
380.425041	18254.109002	29.686144
380.530255	18285.429618	29.691162
381.109581	18305.816477	29.696180
381.615986	18352.817860	29.701197
381.980971	18381.163482	29.706215
382.432265	18405.910029	29.711232
382.921804	18441.887214	29.716250
383.014530	18479.348957	29.721268
383.391817	18506.154138	29.726285
383.624353	18542.511435	29.731303
384.190743	18573.409446	29.736320
384.454455	18603.432221	29.741338
385.036807	18643.860608	29.746356
385.358693	18666.743503	29.751373
385.682617	18702.994589	29.756391
386.347698	18731.037329	29.761408
386.021600	18770.892767	29.766426
387.048482	18799.870505	29.771444
387.429301	18841.469368	29.776461
387.810426	18863.593897	29.781479
388.200823	18900.428748	29.786496
388.810963	18919.863788	29.791514
389.142044	18948.318458	29.796532
389.478714	18983.964246	29.801549
389.436430	19016.377933	29.806567
390.202463	19044.224771	29.811584
390.071325	19078.657023	29.816602
390.845430	19110.097078	29.821620
391.327934	19142.553432	29.826637
391.844377	19175.675829	29.831655
392.054789	19199.880107	29.836672
392.156717	19242.421588	29.841690
392.964508	19267.893948	29.846708
393.033513	19308.235482	29.851725
393.796225	19338.744547	29.856743
394.211787	19347.379924	29.861760
394.653042	19392.022328	29.866778
394.796490	19404.253136	29.871796
395.259056	19434.503046	29.876813
395.396814	19464.463079	29.881831
396.103416	19495.642290	29.886848
396.252925	19535.121287	29.891866
396.992523	19552.741524	29.896884
397.129253	19580.747007	29.901901
397.419701	19606.562481	29.906919
397.606403	19635.546712	29.911936
397.822061	19671.625474	29.916954
398.512597	19700.800758	29.921972
399.092411	19734.128187	29.926989
399.250975	19772.034401	29.932007
399.835849	19799.138382	29.937024
399.965361	19839.840099	29.942042
400.121070	19875.044757	29.947060
400.808688	19909.773621	29.952077
400.939748	19956.920458	29.957095
401.469842	19997.529461	29.962112
401.949510	20042.640218	29.967130
402.444962	20067.515929	29.972148
402.763187	20113.575907	29.977165
403.064585	20149.340374	29.982183
403.654145	20183.745485	29.987200
404.148229	20217.411268	29.992218
404.611064	20253.686866	29.997236
405.002362	20280.593474	30.002253
404.988722	20325.048769	30.007271
406.112137	20360.542057	30.012288
406.444252	20393.079327	30.017306
407.045195	20433.423821	30.022324
407.490575	20460.208249	30.027341
407.447382	20498.469547	30.032359
408.231268	20522.407396	30.037376
408.289499	20572.535256	30.042394
408.606136	20596.252549	30.047412
409.344059	20634.553589	30.052429
409.632440	20677.597601	30.057447
410.192101	20701.095084	30.062464
410.570393	20738.140940	30.067482
410.607502	20775.851934	30.072500
411.550089	20806.232999	30.077517
411.394144	20846.911863	30.082535
412.177436	20876.731317	30.087552
412.603248	20921.840731	30.092570
413.098420	20954.859794	30.097588
413.516916	20980.377114	30.102605
413.957362	21024.252986	30.107623
414.222762	21058.986302	30.112640
414.506471	21093.942127	30.117658
414.140733	21124.909231	30.122676
415.466310	21171.226372	30.127693
415.529143	21213.588523	30.132711
416.285474	21253.608115	30.137728
416.746874	21297.545876	30.142746
417.128222	21333.662270	30.147764
417.340251	21347.158709	30.152781
417.628567	21393.361155	30.157799
418.448832	21421.059488	30.162816
419.136627	21474.338630	30.167834
419.146549	21502.431362	30.172852
419.979754	21530.031552	30.177869
420.353041	21562.392401	30.182887
420.931440	21599.903706	30.187904
420.878610	21626.556423	30.192922
421.306995	21654.220657	30.197940
421.887203	21673.974469	30.202957
422.178116	21709.863814	30.207975
422.773176	21741.475610	30.212992
422.998539	21760.509328	30.218010
423.220903	21800.227546	30.223028
423.876188	21831.044315	30.228045
424.031783	21868.058549	30.233063
424.895562	21888.204027	30.238080
424.908631	21924.953422	30.243098
425.330878	21951.867037	30.248116
425.788458	21985.812023	30.253133
426.131948	22025.788238	30.258151
426.823132	22059.600106	30.263168
427.078969	22097.511213	30.268186
427.392457	22126.216994	30.273204
427.831301	22161.553012	30.278221
428.287400	22203.187147	30.283239
428.690077	22240.109270	30.288256
429.093800	22282.958524	30.293274
429.087658	22316.856345	30.298292
430.140072	22362.698464	30.303309
430.159438	22411.324457	30.308327
430.889013	22447.402945	30.313344
431.294844	22494.738452	30.318362
431.601627	22524.507223	30.323380
432.465656	22555.363302	30.328397
432.520925	22598.173252	30.333415
433.362363	22640.731794	30.338432
433.854605	22683.881203	30.343450
433.951318	22712.802034	30.348468
434.382845	22748.224057	30.353485
434.742655	22791.629030	30.358503
435.212655	22827.413836	30.363520
435.758703	22874.230485	30.368538
435.771740	22921.900250	30.373556
436.459358	22959.580986	30.378573
436.799134	23003.781404	30.383591
437.491788	23045.824715	30.388608
438.121516	23085.089035	30.393626
438.558639	23121.799225	30.398644
439.288622	23156.199769	30.403661
439.362499	23188.400387	30.408679
439.976332	23224.909676	30.413696
440.232467	23265.918786	30.418714
440.505184	23315.845799	30.423732
441.366585	23348.838887	30.428749
441.681048	23394.011152	30.433767
441.695865	23426.040647	30.438784
442.572814	23470.645381	30.443802
442.857532	23506.232046	30.448820
443.630537	23541.323250	30.453837
443.813145	23578.994314	30.458855
444.327785	23621.822278	30.463872
444.835191	23655.634623	30.468890
445.320063	23697.221923	30.473908
445.778637	23719.201237	30.478925
445.917352	23761.210250	30.483943
446.495480	23799.273662	30.488960
447.130199	23837.901805	30.493978
447.815638	23886.150542	30.498996
448.340917	23909.522555	30.504013
448.446794	23948.386697	30.509031
448.523642	23988.880006	30.514048
449.032530	24022.066777	30.519066
449.776367	24056.485772	30.524084
450.173638	24097.367866	30.529101
450.190800	24128.724920	30.534119
450.689408	24173.179633	30.539136
451.173811	24205.594936	30.544154
451.534380	24249.347275	30.549172
452.048290	24290.762477	30.554189
452.395379	24331.448425	30.559207
452.708463	24367.238776	30.564224
453.427186	24404.412920	30.569242
454.114602	24446.351738	30.574260
454.399182	24477.384469	30.579277
454.652361	24519.234469	30.584295
455.202592	24559.657099	30.589312
455.626442	24601.365511	30.594330
456.136178	24647.207394	30.599348
456.820888	24674.405173	30.604365
456.992787	24726.248576	30.609383
457.324245	24767.619426	30.614400
458.180082	24810.297707	30.619418
458.479378	24857.884490	30.624436
458.860310	24888.712776	30.629453
459.048781	24947.900004	30.634471
459.533579	24974.320735	30.639488
460.256963	25012.952632	30.644506
460.258301	25069.086513	30.649524
460.860427	25117.062326	30.654541
461.363070	25172.558461	30.659559
462.042084	25214.014809	30.664576
462.751290	25264.553418	30.669594
462.995146	25308.403472	30.674612
463.595196	25342.918242	30.679629
463.878542	25385.598064	30.684647
464.407720	25441.503875	30.689664
465.099312	25470.953880	30.694682
465.516906	25520.106332	30.699700
466.218424	25551.948883	30.704717
466.288939	25590.226444	30.709735
467.122048	25638.641779	30.714752
467.593592	25684.704085	30.719770
468.110708	25716.227334	30.724788
468.551764	25751.422165	30.729805
469.330761	25803.679343	30.734823
469.632754	25841.619502	30.739840
470.343088	25875.476775	30.744858
470.512155	25918.530108	30.749876
471.128728	25963.219125	30.754893
471.384932	25994.934311	30.759911
471.426212	26048.099727	30.764928
471.960551	26080.560777	30.769946
472.706527	26128.685942	30.774964
473.084752	26173.099511	30.779981
473.600686	26226.101763	30.784999
474.144816	26266.917403	30.790016
474.604185	26299.968520	30.795034
474.789307	26345.878109	30.800052
475.660522	26385.860778	30.805069
476.096522	26437.861199	30.810087
476.382255	26479.038692	30.815104
477.186989	26516.976004	30.820122
477.430695	26569.242066	30.825140
477.847804	26611.666206	30.830157
478.078318	26665.698060	30.835175
478.896959	26708.475533	30.840192
479.465008	26741.052117	30.845210
479.653117	26790.119982	30.850228
480.308902	26823.729480	30.855245
480.895629	26869.577158	30.860263
480.990700	26926.452325	30.865280
481.640938	26967.195281	30.870298
482.064948	27005.736083	30.875316
482.664652	27047.597969	30.880333
483.351528	27086.073371	30.885351
483.822512	27127.303769	30.890368
484.002261	27157.872880	30.895386
484.323252	27198.885371	30.900404
484.856544	27240.992149	30.905421
485.167636	27281.659474	30.910439
485.655570	27333.026238	30.915456
486.096018	27379.129751	30.920474
486.637532	27419.017950	30.925492
487.138929	27462.622651	30.930509
487.599955	27505.369788	30.935527
487.983806	27562.098305	30.940544
488.644985	27606.449802	30.945562
489.018118	27663.275061	30.950580
489.396723	27707.175146	30.955597
490.206453	27756.508817	30.960615
490.492766	27808.358304	30.965632
491.137320	27850.258872	30.970650
491.722281	27909.236048	30.975668
492.030050	27943.129286	30.980685
492.475300	27997.972045	30.985703
492.967319	28053.255201	30.990720
493.604906	28099.652936	30.995738
493.854690	28143.550201	31.000756
494.112906	28204.569900	31.005773
495.242294	28251.782597	31.010791
495.389921	28307.543125	31.015808
496.263958	28354.293599	31.020826
496.840253	28406.286166	31.025844
497.113815	28458.291126	31.030861
497.393175	28502.310589	31.035879
497.768049	28559.088006	31.040896
498.796789	28597.683702	31.045914
499.529545	28657.080622	31.050932
499.911092	28703.916682	31.055949
500.214513	28747.140929	31.060967
500.532688	28806.540707	31.065984
500.992943	28850.357601	31.071002
501.515078	28906.897253	31.076020
502.127417	28952.752497	31.081037
502.613612	29011.472118	31.086055
503.037518	29068.482845	31.091072
503.659838	29113.933038	31.096090
504.053794	29170.122477	31.101108
504.776660	29220.399047	31.106125
505.473046	29268.913402	31.111143
505.939208	29318.191615	31.116160
506.669517	29358.324338	31.121178
507.022784	29415.259545	31.126196
507.368133	29468.044358	31.131213
508.062300	29505.549033	31.136231
508.285271	29559.572177	31.141248
509.092904	29611.589996	31.146266
509.403553	29649.167903	31.151284
509.807186	29713.421570	31.156301
510.150044	29757.679773	31.161319
510.813933	29807.661755	31.166336
511.472325	29851.107630	31.171354
511.596777	29908.432504	31.176372
512.230581	29963.234454	31.181389
512.948857	30007.093579	31.186407
513.225311	30069.631173	31.191424
513.866849	30120.400195	31.196442
514.378420	30175.106295	31.201460
514.807212	30228.763004	31.206477
515.508508	30276.619928	31.211495
516.430458	30330.409892	31.216512
516.897679	30367.581663	31.221530
517.187887	30408.493199	31.226548
518.044278	30438.350309	31.231565
518.841542	30477.215630	31.236583
518.619331	30523.989232	31.241600
519.277370	30559.703722	31.246618
519.767828	30610.928256	31.251636
519.851953	30659.651887	31.256653
520.572226	30701.657191	31.261671
520.384573	30754.269028	31.266688
520.959179	30804.640929	31.271706
521.587944	30872.253386	31.276724
522.114375	30933.903943	31.281741
522.524572	30981.230395	31.286759
522.883603	31043.880836	31.291776
523.776762	31100.744787	31.296794
524.482539	31153.386673	31.301812
524.976464	31214.415697	31.306829
525.316220	31270.302136	31.311847
525.968475	31332.251945	31.316864
526.547894	31381.119635	31.321882
527.203400	31442.151108	31.326900
527.382774	31500.393410	31.331917
528.039216	31565.766840	31.336935
528.596335	31634.523670	31.341952
528.985672	31681.820741	31.346970
529.896464	31734.727038	31.351988
530.561554	31798.528539	31.357005
531.510843	31839.653028	31.362023
531.312704	31903.660848	31.367040
532.255006	31955.698022	31.372058
532.903735	32010.402894	31.377076
533.030541	32064.512728	31.382093
534.155084	32121.247018	31.387111
534.318914	32179.068143	31.392128
534.485385	32231.288139	31.397146
535.279113	32292.107190	31.402164
535.825812	32347.107662	31.407181
536.288726	32400.648570	31.412199
536.604876	32464.996146	31.417216
537.275134	32521.491337	31.422234
538.332271	32580.614324	31.427252
538.764184	32639.399189	31.432269
539.429554	32687.801871	31.437287
539.683411	32748.355241	31.442304
540.147949	32804.090179	31.447322
540.936355	32856.865457	31.452340
541.245878	32916.876904	31.457357
542.087246	32969.053664	31.462375
542.491216	33028.775328	31.467392
542.951103	33077.017424	31.472410
543.454626	33141.825558	31.477428
544.091535	33198.199039	31.482445
544.807153	33256.061743	31.487463
545.154640	33317.415700	31.492480
545.489187	33373.909188	31.497498
546.227547	33430.746274	31.502516
546.877160	33486.919760	31.507533
548.148525	33538.840862	31.512551
548.180474	33590.686333	31.517568
548.793036	33643.997945	31.522586
549.221371	33686.980093	31.527604
549.600335	33741.917956	31.532621
550.462324	33799.382678	31.537639
550.818754	33858.720522	31.542656
551.391644	33905.147405	31.547674
551.704787	33958.108720	31.552692
552.116599	34015.263622	31.557709
552.899997	34068.680777	31.562727
553.074753	34128.854292	31.567744
553.714872	34182.503774	31.572762
554.192756	34228.798895	31.577780
554.550855	34292.019506	31.582797
555.425386	34336.759746	31.587815
555.752306	34394.608401	31.592832
556.420740	34452.233479	31.597850
557.226951	34510.621747	31.602868
557.691386	34573.472304	31.607885
558.312465	34620.492678	31.612903
559.145948	34671.801554	31.617920
559.392370	34734.237458	31.622938
559.957702	34783.527084	31.627956
560.480978	34844.402745	31.632973
560.770933	34896.540670	31.637991
561.492851	34966.084680	31.643008
561.813695	35025.164020	31.648026
562.498025	35072.178269	31.653044
563.123208	35143.559940	31.658061
563.663955	35201.331631	31.663079
564.094445	35277.416850	31.668096
564.682764	35336.048992	31.673114
564.985487	35404.360638	31.678132
565.668314	35469.668266	31.683149
566.062259	35542.276431	31.688167
566.919722	35603.538052	31.693184
567.647499	35665.528290	31.698202
568.440753	35738.519335	31.703220
568.668179	35802.571667	31.708237
569.642073	35862.423086	31.713255
570.061134	35924.184402	31.718272
570.359775	35990.860941	31.723290
571.630635	36053.109826	31.728308
571.533152	36123.696522	31.733325
572.475318	36171.668314	31.738343
573.265575	36236.121416	31.743360
573.713019	36301.758209	31.748378
574.502791	36364.236105	31.753396
574.538683	36428.518025	31.758413
574.957786	36495.993942	31.763431
575.568236	36560.825130	31.768448
576.020378	36632.790499	31.773466
576.750108	36701.964323	31.778484
577.146167	36771.095775	31.783501
578.174405	36847.540047	31.788519
578.456182	36907.484191	31.793536
579.277088	36974.491411	31.798554
580.037044	37029.723460	31.803572
580.525616	37111.134565	31.808589
580.934731	37173.457293	31.813607
581.489556	37235.746658	31.818624
582.063812	37320.427080	31.823642
582.321619	37385.988702	31.828660
583.123998	37454.866152	31.833677
583.942722	37524.097827	31.838695
585.045308	37584.577549	31.843712
585.210953	37643.104032	31.848730
586.156869	37714.789987	31.853748
586.618679	37773.596153	31.858765
587.201020	37826.540061	31.863783
587.810364	37892.001154	31.868800
588.080382	37954.914572	31.873818
588.848854	38014.264186	31.878836
589.851349	38086.160038	31.883853
590.147742	38141.749930	31.888871
590.924491	38200.571654	31.893888
591.193995	38267.472856	31.898906
592.025587	38309.594393	31.903924
592.382892	38372.718920	31.908941
592.657297	38431.078425	31.913959
593.296580	38481.764224	31.918976
593.706005	38554.227208	31.923994
594.595183	38600.140353	31.929012
595.066080	38675.450314	31.934029
595.762268	38740.713849	31.939047
596.505970	38794.779703	31.944064
596.840070	38861.246253	31.949082
597.613997	38922.476088	31.954100
597.936571	38984.973999	31.959117
598.260957	39050.006585	31.964135
599.230101	39117.173936	31.969152
599.426425	39184.914479	31.974170
600.142410	39239.889033	31.979188
600.437816	39332.361871	31.984205
601.303339	39386.816530	31.989223
602.264038	39459.930553	31.994240
602.707831	39540.829578	31.999258
603.410492	39611.376304	32.004276
604.090763	39677.775914	32.009293
604.489296	39746.151141	32.014311
605.152689	39814.934218	32.019328
605.665891	39888.910016	32.024346
606.625262	39962.477678	32.029364
607.035547	40030.814137	32.034381
607.267782	40101.756254	32.039399
608.174987	40173.265688	32.044416
608.612353	40248.253028	32.049434
609.333147	40317.123191	32.054452
610.037041	40396.407685	32.059469
610.218359	40474.108998	32.064487
611.473713	40548.662329	32.069504
611.618954	40625.353734	32.074522
612.489694	40699.996563	32.079540
612.650877	40775.255878	32.084557
613.710777	40852.879724	32.089575
614.185944	40929.814560	32.094592
614.556799	41014.889810	32.099610
615.369512	41078.923786	32.104628
616.461947	41168.877839	32.109645
616.733183	41232.588366	32.114663
617.644495	41312.840089	32.119680
618.139170	41399.913949	32.124698
618.913169	41459.115938	32.129716
619.265017	41533.649088	32.134733
620.067534	41609.970639	32.139751
620.716195	41674.617873	32.144768
621.283613	41757.728734	32.149786
622.340035	41836.392807	32.154804
622.825216	41911.956730	32.159821
623.387755	41976.871833	32.164839
624.147921	42046.193390	32.169856
624.600097	42123.774725	32.174874
625.315577	42185.931173	32.179892
625.862332	42258.455452	32.184909
626.406797	42328.372566	32.189927
626.944060	42399.124631	32.194944
627.307049	42480.488733	32.199962
628.001907	42554.710340	32.204980
628.684233	42636.884214	32.209997
629.257237	42708.376647	32.215015
630.134066	42779.225526	32.220032
630.877753	42863.486664	32.225050
631.274979	42927.071649	32.230068
631.927281	42995.716831	32.235085
632.420278	43075.006623	32.240103
633.082962	43146.009144	32.245120
633.540871	43218.144563	32.250138
634.104216	43295.980757	32.255156
635.124285	43363.455064	32.260173
635.543889	43432.673941	32.265191
636.408804	43495.706727	32.270208
636.567807	43575.274912	32.275226
637.345684	43638.183653	32.280244
638.143388	43711.379320	32.285261
638.743959	43792.362516	32.290279
639.896890	43862.914079	32.295296
640.341162	43936.222773	32.300314
640.595583	44005.799469	32.305332
641.195019	44072.035576	32.310349
641.798515	44156.767779	32.315367
642.667072	44224.096595	32.320384
642.873802	44314.572328	32.325402
643.495550	44382.381437	32.330420
644.065770	44473.220907	32.335437
644.708080	44554.206800	32.340455
645.711760	44629.815921	32.345472
646.160336	44713.913177	32.350490
646.908149	44791.560867	32.355508
647.602708	44879.012576	32.360525
647.961390	44961.701730	32.365543
648.928256	45037.593294	32.370560
649.445761	45128.804618	32.375578
650.255719	45217.934466	32.380596
651.076251	45296.971053	32.385613
651.522495	45377.424540	32.390631
652.408874	45456.400379	32.395648
653.145605	45532.483577	32.400666
653.937047	45603.609872	32.405684
654.250199	45681.535229	32.410701
654.979542	45755.062777	32.415719
656.249070	45841.811227	32.420736
656.546368	45929.361943	32.425754
657.349026	46000.645766	32.430772
658.254740	46079.182077	32.435789
658.611387	46157.793757	32.440807
659.285332	46234.632254	32.445824
659.799125	46310.878619	32.450842
660.517300	46384.243093	32.455860
661.444812	46464.188956	32.460877
661.546643	46551.853828	32.465895
662.467818	46621.244596	32.470912
663.145361	46717.944473	32.475930
663.811566	46797.259174	32.480948
664.591971	46880.231154	32.485965
665.426354	46959.202915	32.490983
665.932959	47027.646891	32.496000
666.474683	47117.142689	32.501018
666.976518	47190.419746	32.506036
668.183483	47267.120557	32.511053
668.295564	47360.389753	32.516071
669.238784	47431.330420	32.521088
669.659753	47520.876513	32.526106
670.463240	47605.572128	32.531124
671.312075	47670.377401	32.536141
671.720772	47771.005209	32.541159
672.423696	47847.078010	32.546176
672.941749	47931.342258	32.551194
673.743310	48010.339595	32.556212
674.372801	48105.500662	32.561229
674.852556	48187.943812	32.566247
675.714828	48272.440012	32.571264
676.198318	48359.636328	32.576282
676.554053	48444.179182	32.581300
677.518044	48527.099529	32.586317
678.036373	48598.490647	32.591335
678.665380	48680.007972	32.596352
679.400274	48775.552867	32.601370
680.222566	48853.280635	32.606388
680.704065	48931.832555	32.611405
681.397319	49013.176437	32.616423
682.011221	49097.594186	32.621440
682.446931	49190.632412	32.626458
682.765431	49277.838083	32.631476
683.842992	49371.529005	32.636493
684.460903	49470.855144	32.641511
685.461207	49552.772712	32.646528
685.928405	49644.854092	32.651546
686.629617	49734.986362	32.656564
687.614887	49826.897633	32.661581
688.153346	49923.222951	32.666599
688.909484	50007.298997	32.671616
689.676613	50101.139574	32.676634
690.134778	50196.203514	32.681652
691.336934	50278.384512	32.686669
691.966293	50369.858202	32.691687
692.673457	50458.217779	32.696704
693.496612	50547.392428	32.701722
693.588502	50644.243722	32.706740
694.447732	50732.869985	32.711757
694.772521	50837.801250	32.716775
695.995206	50925.749187	32.721792
696.756397	51016.155464	32.726810
697.356194	51112.116467	32.731828
698.150501	51200.218638	32.736845
698.639591	51304.335582	32.741863
699.399739	51404.346181	32.746880
700.222694	51491.958499	32.751898
700.601438	51596.158432	32.756916
701.407052	51679.800805	32.761933
702.065367	51784.454577	32.766951
702.769540	51877.098043	32.771968
703.616195	51975.732684	32.776986
704.495774	52074.754067	32.782004
705.516523	52167.352863	32.787021
706.040379	52268.455708	32.792039
706.688935	52353.990659	32.797056
707.427006	52447.332486	32.802074
708.488185	52538.574368	32.807092
709.048354	52628.857122	32.812109
709.438730	52728.916727	32.817127
710.359355	52823.108323	32.822144
711.438060	52920.483691	32.827162
711.567122	53000.421337	32.832180
712.667138	53088.411969	32.837197
713.040145	53196.873334	32.842215
713.887819	53275.802400	32.847232
714.703352	53383.104902	32.852250
715.181573	53474.959335	32.857268
716.087006	53571.090355	32.862285
716.296678	53664.816018	32.867303
717.632956	53756.371877	32.872320
718.440822	53853.550271	32.877338
719.002106	53947.004298	32.882356
719.676342	54029.737037	32.887373
720.331720	54131.440591	32.892391
721.183346	54224.133943	32.897408
721.838001	54310.933750	32.902426
722.560807	54412.949835	32.907444
723.456495	54501.018501	32.912461
723.836461	54594.019072	32.917479
725.020371	54681.187883	32.922496
725.624021	54767.966544	32.927514
725.984956	54864.674144	32.932532
727.040701	54939.367357	32.937549
727.487308	55034.355620	32.942567
728.482195	55117.381076	32.947584
729.452534	55199.665349	32.952602
729.741895	55286.037011	32.957620
730.638067	55367.032614	32.962637
731.432651	55451.779681	32.967655
731.829379	55539.587979	32.972672
732.526730	55644.862431	32.977690
733.513255	55734.842454	32.982708
734.232415	55822.775594	32.987725
734.747537	55907.330718	32.992743
735.491178	56006.533375	32.997760
736.260247	56100.677226	33.002778
736.902669	56197.306841	33.007796
737.844575	56295.372335	33.012813
738.205856	56392.245286	33.017831
738.635482	56484.835765	33.022848
739.536173	56590.125813	33.027866
740.234066	56694.154556	33.032884
741.175188	56784.633401	33.037901
741.792652	56885.005054	33.042919
742.757615	56985.970603	33.047936
743.487782	57090.918668	33.052954
744.476171	57205.562482	33.057972
745.144613	57294.843855	33.062989
745.488669	57401.513057	33.068007
746.344335	57508.635342	33.073024
747.149905	57606.003098	33.078042
747.781832	57717.966211	33.083060
748.840310	57814.364197	33.088077
749.632521	57928.791819	33.093095
750.515235	58022.508836	33.098112
750.918994	58128.729661	33.103130
751.686147	58234.063077	33.108148
752.604454	58335.359114	33.113165
753.515671	58444.044452	33.118183
754.325207	58544.588541	33.123200
755.315632	58646.006925	33.128218
755.502861	58756.222985	33.133236
756.626377	58852.640468	33.138253
757.585875	58961.548119	33.143271
758.288289	59062.219943	33.148288
758.965386	59153.214478	33.153306
759.762759	59256.860843	33.158324
760.780162	59355.889423	33.163341
761.444583	59463.546689	33.168359
761.979428	59556.955500	33.173376
762.698342	59655.238603	33.178394
763.339060	59758.787049	33.183412
764.272635	59863.640073	33.188429
765.195832	59967.572624	33.193447
765.643891	60072.873601	33.198464
766.846448	60171.350970	33.203482
767.159668	60289.113418	33.208500
768.213224	60380.841216	33.213517
769.141084	60490.716669	33.218535
769.385813	60595.036420	33.223552
770.027521	60692.806407	33.228570
770.800364	60808.726147	33.233588
771.520225	60910.282776	33.238605
772.589106	61024.479878	33.243623
773.069716	61131.904600	33.248640
773.985226	61238.436290	33.253658
774.764756	61353.384664	33.258676
775.621440	61448.329045	33.263693
776.401860	61553.614294	33.268711
776.928168	61652.836411	33.273728
777.791004	61759.619711	33.278746
778.388584	61855.120807	33.283764
779.165110	61952.394147	33.288781
779.673963	62061.582547	33.293799
780.388121	62171.205305	33.298816
781.400214	62274.806218	33.303834
782.042842	62384.555721	33.308852
782.680040	62490.684853	33.313869
783.459392	62610.456795	33.318887
784.434636	62730.361377	33.323904
785.296631	62842.327288	33.328922
785.763304	62958.922959	33.333940
786.661688	63057.407644	33.338957
787.743309	63173.125325	33.343975
788.556091	63290.335654	33.348992
789.566354	63401.116991	33.354010
790.212771	63514.468608	33.359028
791.103316	63619.265801	33.364045
791.665227	63743.587302	33.369063
792.400978	63858.379911	33.374080
793.586424	63957.636851	33.379098
794.080368	64072.514890	33.384116
795.109318	64193.639098	33.389133
796.206958	64303.917745	33.394151
796.884778	64419.867219	33.399168
797.820908	64526.450429	33.404186
798.676395	64642.308543	33.409204
799.237616	64745.136686	33.414221
800.062200	64868.587029	33.419239
800.692062	64977.461045	33.424256
801.612708	65096.010237	33.429274
802.326636	65207.103092	33.434292
803.051056	65332.418680	33.439309
803.968972	65438.307855	33.444327
804.854889	65554.083819	33.449344
805.595153	65665.503489	33.454362
806.224495	65780.488661	33.459380
807.042173	65909.977358	33.464397
807.938752	66027.568563	33.469415
808.693428	66156.740463	33.474432
809.816661	66261.708447	33.479450
810.126410	66375.757188	33.484468
811.173425	66503.156952	33.489485
811.925219	66620.541509	33.494503
812.724415	66748.287208	33.499520
814.024377	66861.371892	33.504538
814.817870	66986.723874	33.509556
815.422650	67095.733162	33.514573
816.327148	67214.537249	33.519591
816.809846	67340.650834	33.524608
817.820811	67454.500924	33.529626
818.654618	67579.034171	33.534644
819.404301	67698.555728	33.539661
820.247847	67814.913845	33.544679
820.496535	67948.789497	33.549696
822.004589	68062.427873	33.554714
822.572815	68188.582945	33.559732
823.382615	68300.030340	33.564749
824.458316	68430.244230	33.569767
824.827522	68557.427066	33.574784
826.219739	68680.034523	33.579802
826.942418	68801.280220	33.584820
827.822762	68919.781727	33.589837
828.855295	69034.066684	33.594855
829.226321	69157.389552	33.599872
830.209776	69258.740921	33.604890
831.124924	69389.101046	33.609908
832.229662	69495.909149	33.614925
832.742276	69601.291874	33.619943
833.471367	69714.954104	33.624960
834.197653	69810.925465	33.629978
835.080023	69938.758816	33.634996
835.329628	70052.065845	33.640013
836.014392	70184.688343	33.645031
836.994879	70300.695941	33.650048
838.113073	70423.870919	33.655066
839.001834	70544.940958	33.660084
839.614374	70671.185573	33.665101
840.577965	70780.786719	33.670119
841.038697	70919.483281	33.675136
842.118462	71044.052993	33.680154
842.938186	71170.506560	33.685172
843.750098	71307.282117	33.690189
844.548079	71429.763318	33.695207
845.454808	71558.595069	33.700224
846.554433	71689.172622	33.705242
847.304727	71825.930036	33.710260
848.190172	71958.037018	33.715277
849.210847	72076.722458	33.720295
850.197568	72207.448288	33.725312
851.102004	72335.481927	33.730330
851.709435	72463.457936	33.735348
852.267443	72604.957005	33.740365
853.737530	72732.052033	33.745383
854.146391	72864.009367	33.750400
855.149092	72995.249538	33.755418
855.868954	73127.391021	33.760436
856.793552	73267.069361	33.765453
857.719811	73400.234484	33.770471
858.448264	73542.773907	33.775488
859.481642	73669.238326	33.780506
860.643762	73804.947180	33.785524
861.288028	73941.109329	33.790541
862.138345	74067.922543	33.795559
862.771434	74212.056851	33.800576
863.790550	74331.652894	33.805594
864.701418	74473.301768	33.810612
865.385500	74622.395009	33.815629
866.595641	74754.477885	33.820647
867.331635	74894.634192	33.825664
868.752242	75024.331153	33.830682
869.327461	75153.637422	33.835700
870.125731	75289.194269	33.840717
870.976108	75423.364548	33.845735
871.814708	75569.617834	33.850752
873.034466	75693.779860	33.855770
873.686800	75825.815940	33.860788
874.315540	75963.156933	33.865805
875.298337	76090.630324	33.870823
876.179502	76237.330053	33.875840
877.007314	76372.572410	33.880858
878.140174	76496.253638	33.885876
879.022216	76635.561930	33.890893
879.830059	76756.053611	33.895911
880.775333	76906.459979	33.900928
881.759786	77042.224468	33.905946
882.471590	77175.081010	33.910964
883.090249	77315.417521	33.915981
884.438157	77443.628949	33.920999
885.146034	77573.800275	33.926016
885.910735	77715.639550	33.931034
887.327847	77845.125885	33.936052
888.188241	77985.907361	33.941069
889.196335	78095.702177	33.946087
889.868901	78220.595028	33.951104
890.462179	78339.979504	33.956122
891.748166	78459.218431	33.961140
892.181983	78594.248436	33.966157
892.465023	78714.767887	33.971175
893.632060	78842.935011	33.976192
894.204721	78974.509501	33.981210
895.246228	79115.318714	33.986228
896.092347	79255.522215	33.991245
897.069938	79381.484408	33.996263
898.118464	79515.374518	34.001280
898.894411	79659.672311	34.006298
899.860799	79797.347909	34.011316
900.443332	79945.576286	34.016333
901.149995	80078.830411	34.021351
902.088047	80237.344933	34.026368
903.166498	80377.396774	34.031386
904.114530	80515.680752	34.036404
904.861021	80658.496809	34.041421
906.051463	80799.753687	34.046439
906.774996	80960.061089	34.051456
907.619118	81099.706969	34.056474
908.660454	81253.099849	34.061492
909.265375	81407.293464	34.066509
910.758451	81554.008923	34.071527
911.511794	81706.212496	34.076544
912.700631	81854.068346	34.081562
913.561198	81989.446559	34.086580
914.382261	82142.451630	34.091597
915.404025	82279.006947	34.096615
916.311247	82434.043214	34.101632
916.893306	82590.709649	34.106650
917.930378	82742.569498	34.111668
919.115128	82895.494137	34.116685
919.809744	83045.217219	34.121703
920.721680	83207.900733	34.126720
921.669295	83352.357973	34.131738
922.786784	83503.848907	34.136756
923.604947	83656.117938	34.141773
924.551263	83805.057738	34.146791
925.243542	83969.984751	34.151808
926.335216	84121.357457	34.156826
927.495753	84275.003870	34.161844
928.400915	84436.482326	34.166861
929.365232	84584.323220	34.171879
930.305764	84741.122106	34.176896
931.043850	84893.595991	34.181914
932.384245	85036.163842	34.186932
933.054226	85195.338999	34.191949
934.083026	85346.679457	34.196967
934.910074	85504.982871	34.201984
935.927147	85665.135214	34.207002
936.915354	85807.955844	34.212020
937.521852	85973.094719	34.217037
938.887471	86123.062029	34.222055
939.869901	86279.155607	34.227072
940.661953	86433.541574	34.232090
941.782752	86582.160195	34.237108
942.444378	86732.981837	34.242125
943.241920	86886.205544	34.247143
944.534425	87050.599432	34.252160
945.544171	87207.365408	34.257178
946.463493	87354.376948	34.262196
946.947840	87514.117407	34.267213
948.210153	87669.876496	34.272231
949.132758	87825.085285	34.277248
949.913013	87977.945567	34.282266
950.806576	88135.730426	34.287284
951.402632	88285.041381	34.292301
952.793143	88430.513526	34.297319
953.574413	88571.284110	34.302336
954.779497	88727.262108	34.307354
955.411684	88866.426370	34.312372
956.414780	89028.894712	34.317389
957.316949	89172.578923	34.322407
958.258957	89315.232191	34.327424
959.225908	89485.917707	34.332442
960.508922	89637.566357	34.337460
960.693914	89793.441539	34.342477
962.054365	89947.231083	34.347495
962.995710	90105.685571	34.352512
963.744853	90269.324505	34.357530
964.692010	90434.703877	34.362548
965.850539	90602.593633	34.367565
966.927425	90760.314858	34.372583
968.050487	90920.238280	34.377600
968.417836	91084.762314	34.382618
969.366916	91243.906537	34.387636
970.366564	91418.961054	34.392653
971.343468	91583.590215	34.397671
972.398431	91759.036776	34.402688
973.174788	91933.391418	34.407706
974.344765	92103.840368	34.412724
975.470337	92287.386839	34.417741
976.263618	92460.577869	34.422759
977.186942	92630.925720	34.427776
978.113729	92812.230433	34.432794
979.292927	92987.690622	34.437812
980.219328	93164.871195	34.442829
981.337185	93343.660751	34.447847
982.380889	93523.369008	34.452864
983.083807	93693.140395	34.457882
984.378004	93873.702279	34.462900
985.318716	94051.298317	34.467917
985.897033	94224.828530	34.472935
987.184955	94403.388792	34.477952
987.980147	94597.198239	34.482970
989.080731	94768.734291	34.487988
990.213512	94962.060343	34.493005
991.388043	95133.517068	34.498023
992.265054	95315.570079	34.503040
993.039171	95508.801449	34.508058
994.347642	95687.354916	34.513076
995.599701	95870.571704	34.518093
996.422274	96047.986371	34.523111
997.669598	96233.112018	34.528128
998.502522	96402.639932	34.533146
999.712382	96573.993128	34.538164
1000.516966	96760.177099	34.543181
1001.310954	96941.173205	34.548199
1002.723273	97112.604230	34.553216
1003.776211	97302.695087	34.558234
1004.750813	97472.441045	34.563252
1005.710652	97661.518118	34.568269
1006.633832	97839.188391	34.573287
1007.607602	98009.824409	34.578304
1008.557564	98191.120257	34.583322
1009.849366	98370.119763	34.588340
1010.807250	98556.677857	34.593357
1011.890917	98726.844721	34.598375
1013.208162	98899.335562	34.603392
1013.965107	99086.044733	34.608410
1014.855809	99257.513267	34.613428
1015.885406	99433.543715	34.618445
1016.665937	99612.528894	34.623463
1017.889889	99783.528012	34.628480
1018.768758	99967.830295	34.633498
1019.932090	100128.293893	34.638516
1020.725168	100295.841158	34.643533
1021.360491	100468.240104	34.648551
1022.659617	100620.434564	34.653568
1023.536407	100813.866837	34.658586
1024.479352	100987.832931	34.663604
1025.269440	101168.530576	34.668621
1026.505372	101341.298276	34.673639
1027.487840	101518.769120	34.678656
1028.124662	101705.707198	34.683674
1029.231686	101887.839090	34.688692
1030.762668	102072.048635	34.693709
1031.268847	102257.891580	34.698727
1032.659800	102446.090648	34.703744
1033.695521	102642.631942	34.708762
1034.544759	102824.819370	34.713780
1035.347471	103014.949750	34.718797
1036.222522	103213.142905	34.723815
1037.626002	103396.388790	34.728832
1038.634361	103601.319185	34.733850
1040.033423	103796.587000	34.738868
1040.546483	104002.298966	34.743885
1041.668534	104193.170309	34.748903
1042.946903	104386.790753	34.753920
1043.691204	104592.266470	34.758938
1044.545539	104782.945728	34.763956
1046.049700	104996.163825	34.768973
1047.178820	105191.068686	34.773991
1048.413291	105387.186082	34.779008
1049.021110	105590.868356	34.784026
1050.187240	105787.886584	34.789044
1051.616552	105994.602464	34.794061
1052.326533	106200.172333	34.799079
1053.997232	106387.384471	34.804096
1054.711816	106591.132749	34.809114
1055.442784	106801.668741	34.814132
1056.700872	107001.175905	34.819149
1057.858344	107207.958804	34.824167
1058.869652	107415.299441	34.829184
1059.839326	107621.077956	34.834202
1061.245646	107818.172784	34.839220
1062.030343	108021.236363	34.844237
1062.912749	108236.217133	34.849255
1064.276014	108436.984219	34.854272
1065.415372	108649.886483	34.859290
1066.478213	108850.224975	34.864308
1067.470084	109052.375376	34.869325
1068.669604	109266.577226	34.874343
1069.888687	109466.476428	34.879360
1070.725196	109670.531837	34.884378
1071.729971	109874.915638	34.889396
1073.214251	110083.224571	34.894413
1073.995683	110296.553592	34.899431
1075.446997	110492.672359	34.904448
1075.912536	110708.349636	34.909466
1077.326581	110910.342664	34.914484
1078.449083	111123.191024	34.919501
1079.266851	111321.143277	34.924519
1080.557759	111521.463652	34.929536
1081.943050	111741.418094	34.934554
1083.129749	111943.620972	34.939572
1084.155035	112142.976314	34.944589
1085.163755	112345.781627	34.949607
1086.757443	112537.596830	34.954624
1087.693743	112747.701419	34.959642
1088.632471	112945.391914	34.964660
1089.466344	113130.027012	34.969677
1090.831650	113329.524678	34.974695
1091.579067	113521.613259	34.979712
1092.502404	113711.533013	34.984730
1093.772449	113905.210128	34.989748
1094.497593	114100.663668	34.994765
1095.642261	114307.413536	34.999783
1096.657702	114492.939784	35.004800
1097.698392	114698.151384	35.009818
1098.347716	114904.126002	35.014836
1099.485709	115108.361612	35.019853
1100.526377	115325.271835	35.024871
1101.638232	115541.373751	35.029888
1102.725634	115746.154454	35.034906
1104.217756	115960.955046	35.039924
1105.432136	116165.629088	35.044941
1105.914369	116384.831646	35.049959
1107.122512	116599.861384	35.054976
1108.562089	116814.423686	35.059994
1109.516692	117030.081411	35.065012
1110.849416	117245.450176	35.070029
1111.825531	117468.900045	35.075047
1113.179890	117677.679723	35.080064
1114.207330	117910.133445	35.085082
1115.407566	118117.028485	35.090100
1116.725215	118334.055105	35.095117
1117.792067	118564.049386	35.100135
1118.963891	118780.013736	35.105152
1119.796507	119005.589961	35.110170
1120.854132	119221.272356	35.115188
1121.865965	119448.811802	35.120205
1122.936958	119681.982120	35.125223
1124.353161	119900.499389	35.130240
1125.271982	120124.954899	35.135258
1126.303883	120356.806511	35.140276
1127.629224	120578.942684	35.145293
1128.943467	120809.407954	35.150311
1130.531404	121033.607720	35.155328
1131.640091	121272.043398	35.160346
1132.565515	121495.557837	35.165364
1133.798183	121709.886290	35.170381
1134.575024	121939.131264	35.175399
1135.968866	122167.705735	35.180416
1137.034709	122392.470980	35.185434
1138.667399	122630.780250	35.190452
1139.994569	122860.511615	35.195469
1140.821724	123080.112891	35.200487
1141.663474	123294.783494	35.205504
1143.288343	123527.524996	35.210522
1144.333108	123755.256827	35.215540
1145.388255	123983.723725	35.220557
1146.376970	124200.252164	35.225575
1147.581585	124430.459357	35.230592
1148.832222	124671.775577	35.235610
1149.872066	124896.272334	35.240628
1151.299704	125120.098294	35.245645
1152.188158	125359.616779	35.250663
1153.342079	125578.497783	35.255680
1154.607362	125813.673679	35.260698
1155.967575	126043.892702	35.265716
1156.975253	126268.164056	35.270733
1157.823325	126501.018730	35.275751
1159.027929	126739.900042	35.280768
1160.195600	126968.776290	35.285786
1161.203544	127192.369896	35.290804
1162.421629	127427.806758	35.295821
1163.368212	127668.461687	35.300839
1164.469609	127896.747352	35.305856
1165.907116	128137.388136	35.310874
1166.293843	128357.974734	35.315892
1167.678622	128582.289242	35.320909
1168.774781	128817.199054	35.325927
1169.992433	129046.969620	35.330944
1171.149115	129288.540302	35.335962
1172.161036	129510.565419	35.340980
1173.605583	129732.229043	35.345997
1174.755230	129979.446934	35.351015
1175.909008	130211.188648	35.356032
1177.086362	130449.849322	35.361050
1178.210425	130680.724730	35.366068
1179.683164	130905.763785	35.371085
1180.921947	131148.615408	35.376103
1182.010966	131383.583506	35.381120
1183.334435	131625.157107	35.386138
1184.319508	131859.093725	35.391156
1185.562992	132089.427160	35.396173
1186.781366	132333.736299	35.401191
1187.703853	132573.266281	35.406208
1189.062413	132817.467175	35.411226
1190.269960	133062.975270	35.416244
1191.636492	133301.879455	35.421261
1192.806678	133547.828424	35.426279
1194.093066	133791.465429	35.431296
1195.336151	134034.655024	35.436314
1196.513503	134273.889200	35.441332
1197.754777	134518.971665	35.446349
1199.115801	134766.089974	35.451367
1200.360195	135009.210526	35.456384
1201.670897	135262.679840	35.461402
1202.952922	135505.582310	35.466420
1204.338958	135746.593002	35.471437
1205.475758	135990.778182	35.476455
1206.817593	136228.782257	35.481472
1207.916056	136477.769782	35.486490
1208.899810	136725.053844	35.491508
1210.478908	136956.266229	35.496525
1211.381111	137218.984669	35.501543
1212.475489	137458.559870	35.506560
1214.038307	137696.512520	35.511578
1215.061272	137944.914849	35.516596
1216.443665	138181.265156	35.521613
1217.368375	138437.003196	35.526631
1218.590827	138693.378635	35.531648
1219.951579	138940.730779	35.536666
1220.974063	139197.155754	35.541684
1222.415007	139444.612422	35.546701
1223.506460	139695.577525	35.551719
1225.028553	139955.425203	35.556736
1226.305733	140201.494282	35.561754
1227.308728	140449.537797	35.566772
1228.937742	140697.048501	35.571789
1229.969827	140944.811811	35.576807
1231.088745	141194.325094	35.581824
1232.573545	141438.365202	35.586842
1233.679952	141696.988637	35.591860
1235.236471	141948.286347	35.596877
1236.310755	142193.135073	35.601895
1237.343454	142439.247774	35.606912
1238.665836	142688.953704	35.611930
1239.860769	142941.611755	35.616948
1241.570790	143191.320587	35.621965
1242.236201	143436.803531	35.626983
1242.978923	143692.445666	35.632000
1244.797479	143948.824870	35.637018
1245.752866	144206.084115	35.642036
1246.978246	144453.421781	35.647053
1248.427488	144722.675826	35.652071
1249.422821	144954.304571	35.657088
1250.867806	145195.270286	35.662106
1251.926358	145444.785584	35.667124
1253.450644	145676.712015	35.672141
1254.462605	145927.937728	35.677159
1255.650972	146164.488312	35.682176
1257.233892	146405.058860	35.687194
1258.035613	146664.123917	35.692212
1259.191000	146901.052538	35.697229
1260.400801	147153.699817	35.702247
1261.433659	147421.774572	35.707264
1263.032423	147673.536795	35.712282
1263.916013	147926.040401	35.717300
1264.897417	148189.144997	35.722317
1266.381103	148453.639657	35.727335
1267.573815	148725.045746	35.732352
1269.162014	148993.560152	35.737370
1270.438839	149265.755324	35.742388
1271.545709	149529.279924	35.747405
1272.607063	149801.539988	35.752423
1273.833108	150081.803373	35.757440
1275.143368	150354.812685	35.762458
1276.262715	150626.802800	35.767476
1277.657685	150908.376195	35.772493
1279.304720	151194.996202	35.777511
1280.310357	151480.113540	35.782528
1281.639769	151760.828921	35.787546
1282.854828	152042.275574	35.792564
1284.442706	152319.007616	35.797581
1285.772839	152604.472929	35.802599
1286.753011	152896.999933	35.807616
1288.434108	153174.826268	35.812634
1289.624427	153457.860245	35.817652
1291.153132	153740.573986	35.822669
1292.192349	154023.713173	35.827687
1293.077093	154311.636731	35.832704
1294.629921	154590.395013	35.837722
1295.985366	154893.733258	35.842740
1297.565761	155178.973176	35.847757
1299.083277	155472.344034	35.852775
1300.105137	155766.369826	35.857792
1301.849956	156049.838300	35.862810
1302.901005	156339.195319	35.867828
1304.411218	156623.594637	35.872845
1305.729631	156911.884098	35.877863
1306.513866	157200.225862	35.882880
1308.452830	157477.202689	35.887898
1309.360169	157781.474283	35.892916
1310.820605	158062.822041	35.897933
1312.206119	158353.863583	35.902951
1312.984515	158652.961753	35.907968
1314.678867	158934.797021	35.912986
1315.855013	159243.107407	35.918004
1317.050584	159540.722257	35.923021
1318.394860	159831.108753	35.928039
1319.798304	160131.979323	35.933056
1321.117630	160425.215915	35.938074
1322.321935	160726.542375	35.943092
1323.863057	161027.904158	35.948109
1325.288069	161326.914845	35.953127
1326.577935	161628.829963	35.958144
1327.887700	161925.643733	35.963162
1329.200193	162212.677294	35.968180
1330.590330	162514.632935	35.973197
1331.716861	162806.281374	35.978215
1332.999922	163108.956743	35.983232
1334.764787	163413.610020	35.988250
1335.793805	163699.698147	35.993268
1337.210189	163986.333173	35.998285
1338.424977	164262.269520	36.003303
1339.788020	164557.202308	36.008320
1341.027911	164832.947827	36.013338
1341.804670	165125.837100	36.018356
1343.385994	165405.145921	36.023373
1345.089261	165701.425934	36.028391
1345.805262	165997.249379	36.033408
1347.276783	166284.397960	36.038426
1348.843808	166586.428923	36.043444
1350.150860	166883.416788	36.048461
1351.334974	167177.432428	36.053479
1352.337976	167488.305228	36.058496
1354.085263	167778.970747	36.063514
1355.228728	168097.057197	36.068532
1356.657448	168406.330640	36.073549
1357.685785	168712.994966	36.078567
1359.332758	169035.560199	36.083584
1361.121466	169340.390061	36.088602
1362.165692	169660.686433	36.093620
1363.302483	169962.709624	36.098637
1364.945397	170269.181319	36.103655
1366.247203	170598.019777	36.108672
1367.603683	170912.194915	36.113690
1368.702476	171230.627774	36.118708
1370.303203	171552.609164	36.123725
1371.623745	171867.405787	36.128743
1373.040050	172205.030796	36.133760
1374.078751	172533.964419	36.138778
1375.448207	172855.041171	36.143796
1376.767657	173198.133375	36.148813
1378.412754	173523.039627	36.153831
1379.648866	173858.815284	36.158848
1380.948623	174196.841691	36.163866
1382.549876	174539.021254	36.168884
1383.683436	174879.440358	36.173901
1385.320606	175206.072495	36.178919
1386.877390	175553.850513	36.183936
1388.483696	175883.131981	36.188954
1389.839294	176219.919453	36.193972
1391.182797	176560.302825	36.198989
1392.732788	176895.082930	36.204007
1394.041383	177242.901137	36.209024
1395.693655	177567.858413	36.214042
1396.504846	177908.288157	36.219060
1397.911231	178254.345761	36.224077
1399.610544	178595.039489	36.229095
1400.801810	178944.437181	36.234112
1402.210099	179281.528341	36.239130
1403.424650	179630.571484	36.244148
1404.984040	179970.332877	36.249165
1406.510202	180315.889602	36.254183
1408.098913	180665.423640	36.259200
1409.215436	181008.438042	36.264218
1410.702318	181363.895483	36.269236
1412.163570	181705.715143	36.274253
1413.861844	182054.719901	36.279271
1415.271153	182412.862627	36.284288
1416.519225	182750.814884	36.289306
1418.367517	183094.343763	36.294324
1419.370229	183453.512566	36.299341
1421.361882	183779.721705	36.304359
1422.563918	184132.033236	36.309376
1423.896234	184471.010419	36.314394
1425.233325	184819.496108	36.319412
1426.614900	185162.150426	36.324429
1428.155256	185502.648136	36.329447
1429.574227	185857.473484	36.334464
1431.228014	186196.979282	36.339482
1432.847554	186530.590266	36.344500
1433.983669	186846.994331	36.349517
1435.351717	187166.738363	36.354535
1436.811080	187494.491579	36.359552
1438.370853	187818.929669	36.364570
1439.521198	188150.330052	36.369588
1440.707710	188482.069093	36.374605
1442.446828	188811.776517	36.379623
1443.519173	189160.535673	36.384640
1444.675715	189488.807175	36.389658
1446.412321	189830.478704	36.394676
1447.821546	190183.796272	36.399693
1449.452989	190530.186122	36.404711
1450.719628	190875.673468	36.409728
1452.060156	191214.854061	36.414746
1453.818439	191571.828936	36.419764
1455.062691	191920.017209	36.424781
1456.337488	192264.724034	36.429799
1457.577616	192633.431872	36.434816
1459.014261	192987.522912	36.439834
1460.456133	193356.798377	36.444852
1461.604490	193720.817961	36.449869
1463.200630	194093.119098	36.454887
1464.521941	194479.178729	36.459904
1466.373033	194846.452918	36.464922
1467.610201	195219.708633	36.469940
1468.660758	195598.380234	36.474957
1470.381701	195973.248868	36.479975
1472.076224	196372.778958	36.484992
1473.791016	196746.535826	36.490010
1475.375020	197125.216995	36.495028
1476.651817	197517.903836	36.500045
1478.168326	197893.578909	36.505063
1479.463068	198279.144825	36.510080
1481.179686	198663.145092	36.515098
1482.494728	199054.272936	36.520116
1484.114373	199438.026962	36.525133
1485.802293	199821.721055	36.530151
1487.157935	200221.101393	36.535168
1488.387703	200601.003086	36.540186
1490.244799	200986.249975	36.545204
1491.395809	201390.571607	36.550221
1493.220949	201781.465363	36.555239
1494.318915	202172.405215	36.560256
1496.069957	202573.269730	36.565274
1497.562431	202961.241081	36.570292
1498.815191	203362.243036	36.575309
1500.666357	203750.959188	36.580327
1502.103251	204152.290505	36.585344
1503.855099	204552.086369	36.590362
1505.232549	204951.006616	36.595380
1506.946102	205342.216978	36.600397
1508.739388	205738.368116	36.605415
1510.474523	206129.223388	36.610432
1511.503164	206522.838421	36.615450
1513.319478	206917.455365	36.620468
1514.520267	207323.540307	36.625485
1516.638388	207709.845209	36.630503
1517.882330	208099.508922	36.635520
1519.364864	208493.096791	36.640538
1520.721941	208880.815501	36.645556
1522.786071	209271.187359	36.650573
1524.222946	209649.461976	36.655591
1525.884507	210048.767159	36.660608
1527.423254	210445.377144	36.665626
1528.988856	210808.283757	36.670644
1530.438426	211203.870764	36.675661
1531.867551	211571.222113	36.680679
1533.159650	211935.067535	36.685696
1534.257075	212307.962445	36.690714
1536.148361	212682.556338	36.695732
1537.403304	213061.447428	36.700749
1538.923822	213426.759651	36.705767
1540.673267	213810.194441	36.710784
1542.178510	214191.182264	36.715802
1543.687643	214569.580498	36.720820
1545.143609	214951.214530	36.725837
1546.995661	215339.210245	36.730855
1548.316099	215720.107864	36.735872
1549.524838	216111.184541	36.740890
1551.186101	216506.607264	36.745908
1552.312749	216903.415217	36.750925
1553.735289	217288.822979	36.755943
1555.312831	217695.337865	36.760960
1557.138318	218107.578839	36.765978
1558.775205	218516.677865	36.770996
1560.203997	218929.978255	36.776013
1562.002796	219323.586114	36.781031
1563.545609	219739.893323	36.786048
1564.754576	220147.139194	36.791066
1566.745722	220553.520837	36.796084
1567.972560	220969.605678	36.801101
1570.027127	221386.215740	36.806119
1571.636430	221805.237662	36.811136
1572.723102	222217.540521	36.816154
1574.441490	222636.395144	36.821172
1576.033730	223051.589240	36.826189
1577.784480	223466.504654	36.831207
1579.290751	223890.148591	36.836224
1580.785188	224313.440411	36.841242
1582.946865	224810.790800	36.846260
1584.077503	225235.060362	36.851277
1585.679099	225654.046599	36.856295
1587.623832	226079.657772	36.861312
1588.851350	226503.128262	36.866330
1590.772952	226937.153579	36.871348
1592.184901	227361.993447	36.876365
1594.109719	227785.302147	36.881383
1595.902436	228205.865373	36.886400
1596.903156	228637.762385	36.891418
1598.662510	229062.067657	36.896436
1600.298035	229501.025480	36.901453
1602.081054	229914.153137	36.906471
1603.615040	230349.091645	36.911488
1605.055818	230793.470595	36.916506
1606.885514	231219.243920	36.921524
1608.484247	231664.615428	36.926541
1609.835478	232098.268406	36.931559
1611.707284	232521.345908	36.936576
1612.863111	232973.271666	36.941594
1614.964241	233403.324395	36.946612
1616.367122	233838.167472	36.951629
1618.006841	234281.024835	36.956647
1619.680297	234720.194569	36.961664
1621.202124	235166.833147	36.966682
1623.086807	235603.201455	36.971700
1624.483490	236045.062018	36.976717
1625.905825	236493.828707	36.981735
1627.441101	236927.387519	36.986752
1628.700491	237380.145942	36.991770
1630.789205	237817.476444	36.996788
1632.360899	238270.464767	37.001805
1633.764865	238716.420039	37.006823
1635.669642	239172.987847	37.011840
1637.418826	239619.853308	37.016858
1638.689949	240043.428604	37.021876
1640.228407	240482.125719	37.026893
1641.577708	240910.770205	37.031911
1643.409437	241342.384079	37.036928
1644.900853	241783.961903	37.041946
1646.915264	242211.050931	37.046964
1648.762098	242650.386984	37.051981
1650.253351	243086.505596	37.056999
1651.789894	243525.818176	37.062016
1653.457052	243968.361428	37.067034
1655.242815	244406.694347	37.072052
1656.664873	244847.501269	37.077069
1658.473571	245295.078318	37.082087
1660.103784	245741.898015	37.087104
1661.309118	246200.219797	37.092122
1663.163439	246649.010548	37.097140
1664.353402	247109.292127	37.102157
1666.098044	247579.847072	37.107175
1667.751505	248044.651201	37.112192
1669.330759	248504.031905	37.117210
1671.341157	248970.784995	37.122228
1672.827055	249446.998961	37.127245
1674.715327	249920.174808	37.132263
1676.720175	250389.623021	37.137280
1678.239552	250868.728843	37.142298
1680.237731	251335.968950	37.147316
1681.927608	251817.054287	37.152333
1683.415363	252286.208494	37.157351
1685.169562	252765.556518	37.162368
1686.664065	253239.384460	37.167386
1688.473546	253707.140101	37.172404
1690.319876	254197.193967	37.177421
1691.986205	254676.049581	37.182439
1693.981340	255153.606342	37.187456
1695.207829	255641.781811	37.192474
1697.329446	256119.546668	37.197492
1699.239288	256602.960770	37.202509
1700.445879	257082.731457	37.207527
1702.094883	257566.900132	37.212544
1703.604217	258064.174637	37.217562
1705.602108	258553.264821	37.222580
1707.476653	259047.125798	37.227597
1709.056165	259539.155633	37.232615
1710.947148	260028.110972	37.237632
1712.411465	260533.115370	37.242650
1714.134010	261014.985406	37.247668
1715.853901	261518.753368	37.252685
1717.476278	262016.465871	37.257703
1719.475293	262511.880470	37.262720
1721.243990	263016.884493	37.267738
1722.827536	263511.808335	37.272756
1724.695883	264010.114273	37.277773
1726.332385	264517.730341	37.282791
1728.490466	265007.147421	37.287808
1729.889818	265520.009538	37.292826
1731.569679	266014.737846	37.297844
1733.284666	266515.429637	37.302861
1735.218751	267027.185900	37.307879
1736.948271	267512.657842	37.312896
1738.293451	268019.302665	37.317914
1740.165266	268523.624448	37.322932
1742.116650	269040.583146	37.327949
1743.692845	269544.012559	37.332967
1745.507924	270046.131692	37.337984
1747.230954	270547.020579	37.343002
1748.869215	271053.231921	37.348020
1750.744375	271565.220589	37.353037
1752.216909	272062.414321	37.358055
1754.334685	272546.189653	37.363072
1755.517236	273038.247498	37.368090
1757.331735	273523.061978	37.373108
1759.281373	274022.967804	37.378125
1760.622496	274514.412539	37.383143
1762.495170	275005.565321	37.388160
1764.241043	275501.716948	37.393178
1766.022140	275987.040332	37.398196
1767.922021	276499.091722	37.403213
1769.441003	276998.351332	37.408231
1771.181081	277504.330285	37.413248
1772.716458	278020.045473	37.418266
1774.375430	278529.032836	37.423284
1776.402274	279042.301919	37.428301
1777.417845	279563.357281	37.433319
1779.299886	280082.947248	37.438336
1781.174886	280615.542675	37.443354
1782.540458	281155.282383	37.448372
1784.922223	281687.409971	37.453389
1786.310801	282226.685416	37.458407
1788.388131	282766.150244	37.463424
1789.693711	283315.952169	37.468442
1791.571591	283860.552082	37.473460
1793.339477	284415.176408	37.478477
1795.309454	284965.625026	37.483495
1797.249669	285522.528468	37.488512
1798.761130	286080.643716	37.493530
1800.254062	286639.902964	37.498548
1802.319981	287207.269879	37.503565
1804.214760	287770.751099	37.508583
1806.394419	288334.513209	37.513600
1807.461365	288903.867062	37.518618
1809.875932	289481.835266	37.523636
1812.113629	290046.266432	37.528653
1814.118216	290620.715885	37.533671
1816.002944	291177.478745	37.538688
1818.094064	291739.158022	37.543706
1819.503020	292309.024520	37.548724
1821.505675	292871.500591	37.553741
1823.134285	293437.058319	37.558759
1825.466842	293994.674048	37.563776
1827.191920	294560.413574	37.568794
1829.309063	295132.994101	37.573812
1831.360197	295688.387457	37.578829
1832.733099	296262.888385	37.583847
1834.872151	296817.524912	37.588864
1836.892073	297393.132093	37.593882
1838.712068	297964.959369	37.598900
1840.716077	298519.177450	37.603917
1842.358759	299091.281735	37.608935
1844.538031	299648.741073	37.613952
1846.013104	300215.837793	37.618970
1847.836707	300784.168965	37.623988
1850.133848	301339.821381	37.629005
1851.689018	301907.199733	37.634023
1853.331271	302463.563252	37.639040
1855.495071	303036.878811	37.644058
1857.563554	303605.990629	37.649076
1859.405206	304165.282359	37.654093
1860.896211	304737.656997	37.659111
1862.784711	305297.518000	37.664128
1864.573063	305870.394884	37.669146
1866.379816	306434.782605	37.674164
1868.569146	306998.163762	37.679181
1869.730373	307572.580349	37.684199
1871.864581	308147.035471	37.689216
1873.684889	308723.214522	37.694234
1875.635110	309290.073362	37.699252
1877.271419	309852.688269	37.704269
1879.007394	310409.314930	37.709287
1880.935811	310956.433629	37.714304
1882.257690	311519.545659	37.719322
1883.856356	312087.153470	37.724340
1885.824614	312655.102334	37.729357
1887.658727	313230.103219	37.734375
1889.433568	313804.144500	37.739392
1891.670249	314384.631220	37.744410
1893.371989	314964.312896	37.749428
1895.249112	315541.650188	37.754445
1896.613118	316133.998645	37.759463
1898.807610	316715.082977	37.764480
1900.541408	317320.132987	37.769498
1902.270461	317918.297185	37.774516
1904.310759	318517.369688	37.779533
1906.080657	319127.603224	37.784551
1907.997874	319730.290975	37.789568
1910.177236	320339.023943	37.794586
1911.924569	320963.285884	37.799604
1914.108253	321576.297795	37.804621
1916.092284	322196.903305	37.809639
1918.056835	322804.201420	37.814656
1920.376843	323419.966153	37.819674
1922.158416	324044.471751	37.824692
1924.312951	324654.234248	37.829709
1925.877962	325284.094969	37.834727
1927.873633	325904.280975	37.839744
1929.653366	326530.970472	37.844762
1931.871287	327162.252592	37.849780
1933.686251	327777.472907	37.854797
1935.720172	328414.103631	37.859815
1937.602187	329037.322320	37.864832
1939.450956	329664.855681	37.869850
1941.472274	330303.981078	37.874868
1943.776706	330930.866776	37.879885
1945.541646	331567.887730	37.884903
1947.548114	332211.588953	37.889920
1949.697114	332845.383951	37.894938
1951.469923	333489.083461	37.899956
1953.530524	334115.973377	37.904973
1955.368223	334768.176537	37.909991
1957.288414	335414.595749	37.915008
1959.572039	336052.290922	37.920026
1961.215269	336701.887818	37.925044
1963.182260	337345.508703	37.930061
1965.148890	337994.604524	37.935079
1967.379522	338645.552305	37.940096
1969.247286	339291.119708	37.945114
1971.097459	339937.443250	37.950132
1973.140838	340581.061406	37.955149
1974.766937	341245.959529	37.960167
1977.258432	341904.715724	37.965184
1979.278134	342550.266489	37.970202
1980.874712	343211.843201	37.975220
1983.138148	343862.158609	37.980237
1984.967178	344518.678935	37.985255
1987.078523	345176.260284	37.990272
1989.365215	345830.478767	37.995290
1990.995673	346482.969129	38.000308
1993.151631	347130.643071	38.005325
1995.489317	347795.763722	38.010343
1997.636858	348455.779690	38.015360
1999.670178	349105.679165	38.020378
2001.402038	349755.771296	38.025396
2003.662236	350402.899135	38.030413
2005.914356	351063.696917	38.035431
2007.570194	351694.892933	38.040448
2009.766068	352323.909859	38.045466
2011.534063	352938.270474	38.050484
2013.713186	353562.907574	38.055501
2015.381548	354191.832134	38.060519
2017.344392	354823.921357	38.065536
2019.554000	355443.679332	38.070554
2021.477740	356079.663818	38.075572
2023.445962	356718.193989	38.080589
2025.454262	357352.546560	38.085607
2027.318525	357983.538603	38.090624
2029.474338	358624.926136	38.095642
2031.465394	359265.772587	38.100660
2033.530442	359915.070709	38.105677
2035.007718	360559.152853	38.110695
2036.806936	361217.556559	38.115712
2039.227985	361873.030602	38.120730
2040.879730	362538.794000	38.125748
2042.731809	363203.447505	38.130765
2044.921792	363882.494103	38.135783
2046.921299	364546.263100	38.140800
2049.042519	365223.851429	38.145818
2050.792195	365912.904435	38.150836
2053.124344	366595.050413	38.155853
2055.283400	367282.717163	38.160871
2057.071882	367976.723254	38.165888
2059.712742	368667.861572	38.170906
2061.402102	369352.701310	38.175924
2063.475478	370049.538469	38.180941
2065.663043	370752.405517	38.185959
2067.374303	371451.583763	38.190976
2069.627807	372151.369110	38.195994
2071.270690	372860.093173	38.201012
2073.562332	373571.232255	38.206029
2075.748538	374290.312653	38.211047
2077.569462	374999.243479	38.216064
2079.883491	375713.454980	38.221082
2081.967927	376445.593923	38.226100
2084.231731	377173.123015	38.231117
2086.452698	377887.938890	38.236135
2088.575495	378612.265420	38.241152
2090.637893	379332.554535	38.246170
2093.086000	380067.167577	38.251188
2094.907897	380787.693412	38.256205
2096.947922	381516.763426	38.261223
2098.793546	382238.978071	38.266240
2101.279617	382964.519444	38.271258
2103.401028	383708.689831	38.276276
2105.479740	384438.144908	38.281293
2107.596418	385181.115990	38.286311
2109.525257	385912.844234	38.291328
2111.887410	386644.661656	38.296346
2114.218143	387387.647488	38.301364
2116.458072	388116.687732	38.306381
2118.588201	388854.500440	38.311399
2120.618684	389587.470328	38.316416
2122.926569	390324.610449	38.321434
2124.989461	391055.993904	38.326452
2127.198495	391789.972008	38.331469
2129.284909	392524.915904	38.336487
2131.259836	393257.275028	38.341504
2133.600980	393986.641117	38.346522
2136.037426	394735.641948	38.351540
2137.858677	395467.085432	38.356557
2139.983564	396201.679512	38.361575
2141.831204	396943.473357	38.366592
2144.418021	397676.839270	38.371610
2146.370765	398425.243474	38.376628
2148.598543	399138.256545	38.381645
2150.993277	399849.349222	38.386663
2153.066119	400565.874988	38.391680
2155.385046	401257.204984	38.396698
2157.220575	401966.563558	38.401716
2159.341022	402660.476767	38.406733
2161.728615	403374.852620	38.411751
2163.127054	404095.226488	38.416768
2165.872426	404803.653871	38.421786
2167.915854	405519.146469	38.426804
2169.780709	406237.031550	38.431821
2172.111694	406957.810459	38.436839
2173.992431	407676.693974	38.441856
2176.347179	408402.548301	38.446874
2178.466111	409128.244779	38.451892
2180.180008	409870.277091	38.456909
2182.660590	410602.308448	38.461927
2184.923549	411347.248954	38.466944
2186.989262	412093.037019	38.471962
2189.414143	412845.988921	38.476980
2191.317905	413592.521193	38.481997
2193.932285	414335.875559	38.487015
2195.943761	415095.948086	38.492032
2198.072885	415843.872948	38.497050
2200.200274	416611.935552	38.502068
2202.333114	417375.593094	38.507085
2205.026449	418132.019247	38.512103
2206.668193	418908.956366	38.517120
2208.858434	419680.360092	38.522138
2211.111391	420456.034522	38.527156
2213.225568	421237.101200	38.532173
2215.690472	422018.819808	38.537191
2217.560033	422805.751867	38.542208
2219.935431	423583.967070	38.547226
2222.072321	424378.045873	38.552244
2224.610471	425167.931332	38.557261
2227.261621	425951.392857	38.562279
2229.204257	426746.844129	38.567296
2231.354640	427539.956573	38.572314
2233.638014	428336.919134	38.577332
2236.169789	429131.637202	38.582349
2238.340803	429921.477731	38.587367
2240.477635	430735.444215	38.592384
2242.424034	431523.091456	38.597402
2245.035245	432333.836408	38.602420
2247.275315	433138.591026	38.607437
2249.833329	433941.493740	38.612455
2251.654450	434750.563748	38.617472
2254.391763	435558.796135	38.622490
2256.453905	436364.530308	38.627508
2258.854988	437169.522143	38.632525
2261.408653	437976.939914	38.637543
2263.497083	438782.229596	38.642560
2266.056005	439579.721196	38.647578
2268.143049	440386.420952	38.652596
2270.399311	441197.668047	38.657613
2272.821725	442001.622667	38.662631
2274.992884	442809.029927	38.667648
2277.119727	443609.584739	38.672666
2279.808693	444426.965590	38.677684
2281.912094	445231.309717	38.682701
2284.817034	446034.176443	38.687719
2286.945515	446846.651547	38.692736
2289.411673	447637.845592	38.697754
2291.631341	448431.377825	38.702772
2293.623445	449233.162605	38.707789
2295.979739	450037.385886	38.712807
2298.450591	450846.313802	38.717824
2300.489838	451626.403922	38.722842
2302.518742	452413.243399	38.727860
2305.098052	453189.190846	38.732877
2307.508283	453958.108167	38.737895
2309.564330	454735.853971	38.742912
2311.711095	455504.049261	38.747930
2313.775783	456291.291566	38.752948
2316.109160	457072.341335	38.757965
2318.671522	457852.059372	38.762983
2320.512857	458640.663337	38.768000
2322.628330	459435.207326	38.773018
2324.828582	460231.475294	38.778036
2327.183520	461048.664758	38.783053
2329.236679	461847.217985	38.788071
2331.214823	462679.415727	38.793088
2333.956565	463487.696429	38.798106
2335.914132	464320.940369	38.803124
2337.857435	465155.465341	38.808141
2340.537668	465984.526549	38.813159
2342.460755	466835.559534	38.818176
2345.072244	467677.042249	38.823194
2347.455361	468530.653569	38.828212
2349.491862	469386.911707	38.833229
2351.777324	470242.534664	38.838247
2354.043447	471116.361887	38.843264
2356.715741	471991.698581	38.848282
2359.251465	472871.008362	38.853300
2361.545211	473760.218478	38.858317
2363.718646	474619.602168	38.863335
2366.079200	475504.222474	38.868352
2368.609552	476384.681297	38.873370
2371.196838	477276.352180	38.878388
2373.367011	478167.796226	38.883405
2375.715837	479055.581768	38.888423
2378.172615	479957.850626	38.893440
2380.691293	480848.601425	38.898458
2382.848162	481755.122860	38.903476
2385.301214	482672.153493	38.908493
2387.925858	483564.217112	38.913511
2390.298669	484472.232106	38.918528
2392.561570	485381.632589	38.923546
2394.803641	486294.826644	38.928564
2397.160790	487213.507395	38.933581
2399.826406	488118.308894	38.938599
2402.247006	489050.714032	38.943616
2404.815802	489965.631957	38.948634
2407.137080	490890.888897	38.953652
2409.514017	491811.343330	38.958669
2412.086816	492728.839868	38.963687
2414.465284	493650.356408	38.968704
2416.928948	494582.203807	38.973722
2419.702799	495493.262042	38.978740
2421.788217	496422.195040	38.983757
2424.752488	497357.591483	38.988775
2427.167652	498283.441463	38.993792
2429.621226	499198.590080	38.998810
2432.230876	500109.274327	39.003828
2434.375642	501040.716093	39.008845
2437.311551	501952.355101	39.013863
2439.604827	502877.112182	39.018880
2442.286896	503799.786304	39.023898
2444.952499	504714.796503	39.028916
2447.508003	505625.285693	39.033933
2450.045976	506536.029311	39.038951
2452.345736	507456.340766	39.043968
2454.791564	508371.029765	39.048986
2457.416694	509278.478330	39.054004
2460.009526	510191.073137	39.059021
2462.306035	511084.055790	39.064039
2464.630476	511970.884593	39.069056
2467.073247	512856.736957	39.074074
2469.688624	513711.515162	39.079092
2471.933571	514597.251861	39.084109
2474.493175	515470.791942	39.089127
2476.907853	516348.338365	39.094144
2479.372298	517225.675903	39.099162
2481.680790	518097.648620	39.104180
2484.048482	518989.765885	39.109197
2486.412863	519873.368157	39.114215
2488.399213	520774.764982	39.119232
2490.654183	521667.047378	39.124250
2493.216027	522572.424089	39.129268
2495.528451	523497.935130	39.134285
2497.935669	524412.343966	39.139303
2500.348198	525340.797740	39.144320
2502.999206	526266.183579	39.149338
2505.467003	527202.217765	39.154356
2507.576755	528150.638909	39.159373
2510.084816	529094.956185	39.164391
2512.747341	530047.092007	39.169408
2515.131499	531005.857470	39.174426
2517.541353	531956.854184	39.179444
2519.823668	532928.850594	39.184461
2522.543342	533900.307388	39.189479
2524.687840	534879.142163	39.194496
2527.263844	535852.555337	39.199514
2529.812232	536843.922771	39.204532
2532.337628	537832.307080	39.209549
2534.902773	538821.119725	39.214567
2537.532405	539830.380415	39.219584
2539.673974	540824.758649	39.224602
2542.583235	541830.007433	39.229620
2544.760956	542844.258828	39.234637
2547.554912	543871.161199	39.239655
2550.011145	544883.257553	39.244672
2551.977655	545914.018866	39.249690
2555.149088	546934.246512	39.254708
2557.135850	547978.679743	39.259725
2559.682270	549021.282342	39.264743
2562.643555	550057.603814	39.269760
2565.136697	551100.107371	39.274778
2568.254009	552150.672075	39.279796
2570.506741	553206.223934	39.284813
2573.224913	554243.372489	39.289831
2575.562871	555297.440098	39.294848
2578.041173	556352.306362	39.299866
2580.892109	557392.204932	39.304884
2583.467722	558466.836435	39.309901
2586.056991	559516.811562	39.314919
2588.777044	560567.837218	39.319936
2591.262066	561637.403548	39.324954
2594.007916	562693.429014	39.329972
2596.027794	563777.513682	39.334989
2599.052571	564833.671658	39.340007
2601.758771	565908.074625	39.345024
2604.105803	566980.690260	39.350042
2607.179066	568050.536338	39.355060
2609.797787	569122.125386	39.360077
2612.040151	570202.220532	39.365095
2614.789948	571272.101693	39.370112
2617.265741	572355.991140	39.375130
2620.242549	573423.545405	39.380148
2622.459731	574521.845580	39.385165
2625.056278	575575.680990	39.390183
2627.351867	576665.852603	39.395200
2630.097624	577752.593803	39.400218
2632.855092	578824.439739	39.405236
2635.473593	579896.566992	39.410253
2638.008694	580941.982445	39.415271
2640.718413	581991.793872	39.420288
2643.054747	583031.397207	39.425306
2645.514483	584092.051884	39.430324
2648.222103	585160.695665	39.435341
2651.182151	586224.791946	39.440359
2653.592376	587278.859433	39.445376
2655.808317	588344.195003	39.450394
2658.662316	589422.712985	39.455412
2660.925963	590500.529534	39.460429
2663.380812	591591.195977	39.465447
2666.123559	592674.499514	39.470464
2668.533518	593792.980555	39.475482
2671.195058	594888.620097	39.480500
2673.823395	596007.906916	39.485517
2676.172545	597121.172465	39.490535
2678.747303	598245.613439	39.495552
2681.288913	599374.808818	39.500570
2684.144138	600515.609710	39.505588
2687.069048	601662.795344	39.510605
2689.101581	602802.554462	39.515623
2692.005639	603972.441904	39.520640
2694.571425	605135.808596	39.525658
2697.420449	606302.212831	39.530676
2699.833848	607476.625914	39.535693
2702.334020	608651.303045	39.540711
2705.222215	609830.796960	39.545728
2707.572813	611034.618708	39.550746
2710.600621	612211.137640	39.555764
2713.450814	613425.974083	39.560781
2716.209482	614629.590389	39.565799
2719.079520	615835.157636	39.570816
2721.566994	617041.706158	39.575834
2724.009186	618259.378339	39.580852
2727.249012	619472.384536	39.585869
2729.672282	620692.638017	39.590887
2732.671923	621907.161924	39.595904
2735.681736	623146.283924	39.600922
2738.700627	624375.168979	39.605940
2741.295449	625591.793170	39.610957
2743.887139	626814.873698	39.615975
2747.063935	628040.165066	39.620992
2749.465866	629281.874293	39.626010
2752.215455	630515.290865	39.631028
2755.216534	631744.227776	39.636045
2757.852563	632976.675957	39.641063
2760.829891	634206.776417	39.646080
2763.594285	635467.314296	39.651098
2766.808761	636699.726925	39.656116
2769.611018	637940.095245	39.661133
2772.328995	639166.806842	39.666151
2775.521878	640401.625593	39.671168
2778.062571	641645.382370	39.676186
2781.510253	642861.006539	39.681204
2784.091246	644096.627179	39.686221
2787.237842	645316.545843	39.691239
2789.971217	646541.471271	39.696256
2792.711702	647770.484310	39.701274
2795.379198	648980.716119	39.706292
2798.449184	650210.721779	39.711309
2801.219772	651439.528865	39.716327
2804.575467	652663.752544	39.721344
2807.358083	653881.691661	39.726362
2810.285402	655077.138798	39.731380
2813.206383	656296.251471	39.736397
2816.012589	657512.990440	39.741415
2818.662390	658698.579383	39.746432
2821.287362	659887.314578	39.751450
2824.234568	661045.680627	39.756468
2827.053851	662215.577924	39.761485
2829.696897	663377.697282	39.766503
2832.547490	664546.112048	39.771520
2835.233505	665715.854804	39.776538
2837.874543	666888.596599	39.781556
2840.835350	668067.210973	39.786573
2843.670013	669247.988236	39.791591
2846.691356	670431.173945	39.796608
2849.040091	671615.466179	39.801626
2851.609149	672809.766825	39.806644
2854.475123	674003.220216	39.811661
2856.787462	675211.576129	39.816679
2859.928205	676416.755965	39.821696
2862.628470	677640.837407	39.826714
2865.305696	678869.730256	39.831732
2868.362813	680097.900121	39.836749
2870.456787	681343.899931	39.841767
2873.576121	682578.484504	39.846784
2876.647336	683841.617352	39.851802
2879.379828	685096.834579	39.856820
2882.147653	686349.588617	39.861837
2884.669124	687623.756102	39.866855
2887.651169	688900.348313	39.871872
2890.393822	690199.331428	39.876890
2893.013699	691487.676023	39.881908
2896.096669	692775.808213	39.886925
2898.599733	694083.693593	39.891943
2902.122428	695403.767581	39.896960
2904.477537	696716.844305	39.901978
2907.050985	698031.375556	39.906996
2910.183991	699366.838174	39.912013
2913.047784	700713.493645	39.917031
2916.148447	702045.429537	39.922048
2919.238018	703382.763330	39.927066
2922.588167	704715.438060	39.932084
2925.886000	706064.512381	39.937101
2928.635485	707396.574791	39.942119
2931.594802	708737.211624	39.947136
2934.459301	710082.457350	39.952154
2937.469579	711434.447851	39.957172
2940.366746	712770.203105	39.962189
2943.120542	714132.152142	39.967207
2946.179674	715476.560286	39.972224
2948.851604	716848.426699	39.977242
2952.050436	718213.154925	39.982260
2955.073317	719575.809772	39.987277
2957.815707	720946.645811	39.992295
2961.194734	722307.360223	39.997312
2964.031998	723676.789654	40.002330
2967.162789	725050.046039	40.007348
2970.252686	726419.768524	40.012365
2973.189041	727789.485007	40.017383
2976.048723	729160.318351	40.022400
2979.403217	730543.386040	40.027418
2982.112021	731915.310789	40.032436
2985.134746	733282.951260	40.037453
2988.109444	734669.869328	40.042471
2991.275676	736043.681999	40.047488
2994.042905	737414.264739	40.052506
2996.923279	738795.795007	40.057524
3000.317258	740167.527880	40.062541
3003.048786	741548.505109	40.067559
3006.202263	742916.742766	40.072576
3008.706050	744316.754494	40.077594
3011.803511	745693.246424	40.082612
3015.222931	747049.331107	40.087629
3017.519507	748411.673711	40.092647
3020.799373	749740.599882	40.097664
3023.702440	751092.171760	40.102682
3026.560159	752444.155110	40.107700
3029.850447	753789.673452	40.112717
3032.255647	755148.446713	40.117735
3035.202006	756494.334953	40.122752
3038.090149	757863.377424	40.127770
3041.070438	759232.995012	40.132788
3044.206800	760601.404567	40.137805
3047.073022	761984.173679	40.142823
3049.817265	763361.888612	40.147840
3053.175351	764761.184099	40.152858
3056.045299	766165.461496	40.157876
3058.988723	767561.400058	40.162893
3061.854871	768974.096216	40.167911
3064.737784	770389.616537	40.172928
3067.877539	771809.589447	40.177946
3070.977386	773239.120116	40.182964
3074.289533	774675.115359	40.187981
3077.023662	776112.544670	40.192999
3080.004246	777557.996404	40.198016
3083.438595	779007.209275	40.203034
3086.405071	780469.410852	40.208052
3089.476903	781921.976791	40.213069
3092.587071	783387.782814	40.218087
3095.643948	784869.434290	40.223104
3098.874748	786345.846819	40.228122
3101.826889	787822.244794	40.233140
3104.865613	789303.811565	40.238157
3107.636523	790792.316383	40.243175
3110.892913	792297.771402	40.248192
3113.909425	793794.175946	40.253210
3116.856529	795308.392826	40.258228
3120.385514	796821.353577	40.263245
3123.263224	798339.184213	40.268263
3126.428829	799861.236233	40.273280
3129.379279	801378.683268	40.278298
3132.208498	802918.955489	40.283316
3135.777839	804457.978274	40.288333
3138.781291	806017.774591	40.293351
3141.997687	807550.683438	40.298368
3145.139004	809102.516351	40.303386
3148.017662	810668.012750	40.308404
3151.425350	812215.912406	40.313421
3154.606374	813767.498957	40.318439
3157.489749	815333.376396	40.323456
3160.626174	816905.631735	40.328474
3163.828081	818490.049233	40.333492
3167.055181	820050.419452	40.338509
3170.248724	821631.843974	40.343527
3173.042565	823215.589522	40.348544
3176.569666	824800.003565	40.353562
3179.677323	826386.395353	40.358580
3182.849726	827981.846585	40.363597
3185.664281	829574.383894	40.368615
3189.011616	831164.007410	40.373632
3192.719121	832775.778353	40.378650
3195.653223	834363.903723	40.383668
3199.129187	835957.534853	40.388685
3202.163862	837550.355847	40.393703
3205.316977	839151.906812	40.398720
3208.662235	840757.254951	40.403738
3211.468897	842359.173590	40.408756
3214.719988	843965.280357	40.413773
3217.665164	845579.485205	40.418791
3221.158013	847192.796373	40.423808
3224.597527	848787.824070	40.428826
3227.663594	850361.136883	40.433844
3230.867430	851925.969268	40.438861
3233.994753	853494.593893	40.443879
3236.505173	855063.407385	40.448896
3240.182816	856623.769463	40.453914
3243.224339	858202.368377	40.458932
3246.250110	859787.060652	40.463949
3249.572033	861367.414284	40.468967
3252.413641	862966.144302	40.473984
3255.889280	864559.599851	40.479002
3258.590960	866175.626544	40.484020
3262.194567	867770.441042	40.489037
3265.249740	869386.224549	40.494055
3268.269361	871012.709898	40.499072
3271.653781	872646.143332	40.504090
3274.746582	874290.592360	40.509108
3277.779950	875934.401344	40.514125
3281.270105	877608.909917	40.519143
3284.165678	879266.123297	40.524160
3287.522287	880930.040545	40.529178
3290.628037	882613.814109	40.534196
3293.797923	884287.142411	40.539213
3296.858202	885995.153009	40.544231
3299.850909	887692.052720	40.549248
3303.225032	889415.120538	40.554266
3306.295048	891132.223221	40.559284
3309.906935	892875.628845	40.564301
3313.359670	894611.586710	40.569319
3316.047752	896351.670820	40.574336
3319.513513	898106.605423	40.579354
3322.801319	899864.973458	40.584372
3326.303408	901623.142262	40.589389
3329.580569	903403.803582	40.594407
3332.770770	905176.021345	40.599424
3335.904191	906957.881984	40.604442
3339.008061	908750.138925	40.609460
3342.540067	910539.629841	40.614477
3346.091515	912343.144862	40.619495
3349.287907	914150.353671	40.624512
3352.573602	915948.115433	40.629530
3355.843743	917766.985789	40.634548
3359.224271	919573.136264	40.639565
3362.535178	921411.317736	40.644583
3365.958405	923223.437873	40.649600
3369.408681	925068.022026	40.654618
3372.596763	926901.567303	40.659636
3376.256695	928730.764554	40.664653
3379.759885	930576.120799	40.669671
3382.414357	932416.953445	40.674688
3386.432626	934257.494624	40.679706
3389.681682	936117.995023	40.684724
3393.156415	937958.573621	40.689741
3396.612806	939822.219537	40.694759
3399.787140	941669.666028	40.699776
3403.496826	943521.908659	40.704794
3406.978467	945379.065398	40.709812
3410.392950	947239.096877	40.714829
3413.840294	949099.022201	40.719847
3416.968596	950956.702473	40.724864
3420.405485	952817.796511	40.729882
3423.729777	954747.990355	40.734900
3426.731380	956655.686239	40.739917
3430.377632	958569.879571	40.744935
3433.664982	960494.930721	40.749952
3437.291362	962427.196023	40.754970
3440.272781	964349.445308	40.759988
3443.950311	966278.845384	40.765005
3447.343701	968193.195340	40.770010
3450.248357	970049.675458	40.775015
3453.764840	971853.627481	40.780020
3456.519066	973620.381018	40.785024
3459.834122	975297.859172	40.790029
3462.980768	976900.621830	40.795034
3465.925539	978437.527488	40.800039
3468.740191	979909.300604	40.805044
3471.528417	981295.082498	40.810048
3474.176359	982613.791469	40.815053
3476.593565	983855.730636	40.820058
3478.928871	985020.535219	40.825063
3481.608573	986109.352634	40.830068
3483.556966	987156.927143	40.835072
3486.101000	988112.554082	40.840077
3488.099629	989009.615110	40.845082
3489.927844	989847.588742	40.850087
3492.155320	990613.054543	40.855092
3493.578727	991318.324135	40.860096
3495.892518	991968.792419	40.865101
3497.288104	992562.340315	40.870106
3498.856988	993101.533712	40.875111
3500.670801	993589.298690	40.880116
3501.799912	994038.561842	40.885120
3502.741185	994437.757394	40.890125
3504.067082	994792.839986	40.895130
3505.237922	995107.997078	40.900135
3506.728151	995376.242985	40.905140
3507.346334	995620.469941	40.910144
3508.557812	995809.376957	40.915149
3509.487343	995989.463223	40.920154
3510.133108	996132.103174	40.925159
3511.429580	996233.445709	40.930164
3511.556882	996315.408324	40.935168
3512.633448	996365.569517	40.940173
3513.656284	996394.513478	40.945178
3514.084130	996388.503800	40.950183
3514.844512	996358.487324	40.955188
3515.583056	996313.187709	40.960192
3516.498312	996245.950857	40.965197
3516.677560	996155.076326	40.970202
3517.139253	996040.589941	40.975207
3517.635071	995905.452399	40.980212
3518.177583	995761.345329	40.985216
3518.347368	995605.707908	40.990221
3518.952268	995425.259530	40.995226
3518.885888	995231.282049	41.000231
3519.942257	995029.029699	41.005236
3519.868585	994818.970120	41.010240
3520.070720	994589.475457	41.015245
3520.839200	994358.612006	41.020250
3520.982192	994115.764048	41.025255
3520.986679	993839.906838	41.030260
3521.315380	993570.314715	41.035264
3521.726434	993293.292401	41.040269
3521.947530	993013.170309	41.045274
3521.998344	992714.843314	41.050279
3522.563913	992398.195693	41.055284
3522.719670	992104.301295	41.060288
3522.533084	991772.444721	41.065293
3522.872456	991458.900225	41.070298
3522.709491	991135.383241	41.075303
3523.041545	990788.472977	41.080308
3523.070261	990448.121833	41.085312
3523.245426	990107.823650	41.090317
3523.329603	989752.410778	41.095322
3523.136137	989408.427221	41.100327
3523.570900	989045.795978	41.105332
3523.521146	988704.378418	41.110336
3523.788835	988324.569131	41.115341
3524.223202	987953.385453	41.120346
3523.875957	987581.233636	41.125351
3524.041011	987194.149544	41.130356
3524.016245	986814.872786	41.135360
3523.851192	986430.131823	41.140365
3524.244107	986052.783741	41.145370
3523.993834	985671.321988	41.150375
3523.950867	985280.727809	41.155380
3523.736338	984906.232946	41.160384
3524.140641	984507.707068	41.165389
3524.346705	984122.553900	41.170394
3524.273204	983735.078775	41.175399
3524.127891	983318.800238	41.180404
3524.258984	982917.475658	41.185408
3524.132507	982516.458072	41.190413
3524.325169	982114.676436	41.195418
3523.910415	981719.311678	41.200423
3524.296303	981318.613546	41.205428
3524.147835	980926.078661	41.210432
3523.915847	980518.884903	41.215437
3523.807848	980110.469928	41.220442
3523.368453	979717.802211	41.225447
3523.782637	979319.009720	41.230452
3523.793968	978928.850266	41.235456
3523.747954	978515.427742	41.240461
3523.768279	978101.182938	41.245466
3523.754783	977699.612849	41.250471
3523.864847	977298.775729	41.255476
3523.764222	976895.209623	41.260480
3523.754170	976502.152398	41.265485
3523.630143	976085.342616	41.270490
3523.309776	975683.290582	41.275495
3523.564846	975279.454126	41.280500
3523.497390	974874.664961	41.285504
3523.471539	974465.344218	41.290509
3523.623105	974070.920413	41.295514
3522.962289	973662.722098	41.300519
3523.294580	973246.803403	41.305524
3522.612553	972859.961157	41.310528
3522.994045	972452.189205	41.315533
3522.714450	972045.572750	41.320538
3522.413423	971658.684378	41.325543
3522.822994	971249.550967	41.330548
3522.746975	970871.471816	41.335552
3522.632343	970473.127614	41.340557
3522.732555	970080.687118	41.345562
3522.025497	969688.646226	41.350567
3522.657819	969288.140210	41.355572
3522.559865	968898.195025	41.360576
3522.034388	968505.260641	41.365581
3522.447243	968117.624334	41.370586
3522.559869	967715.528610	41.375591
3522.569167	967308.528593	41.380596
3522.184163	966927.304471	41.385600
3522.026067	966522.918830	41.390605
3522.291637	966135.858155	41.395610
3522.007536	965745.240039	41.400615
3522.158126	965353.936376	41.405620
3521.779846	964961.224653	41.410624
3521.628544	964568.448702	41.415629
3522.015267	964174.969782	41.420634
3521.540419	963786.404119	41.425639
3521.777621	963410.621613	41.430644
3521.587530	963037.725099	41.435648
3521.861383	962642.690929	41.440653
3521.451516	962245.881245	41.445658
3521.180922	961873.706150	41.450663
3521.368277	961484.875932	41.455668
3521.214657	961093.332499	41.460672
3521.043607	960711.856799	41.465677
3521.332246	960342.135910	41.470682
3520.937342	959964.174913	41.475687
3521.098227	959577.865996	41.480692
3520.434493	959210.777267	41.485696
3520.698233	958834.985713	41.490701
3520.923934	958454.079215	41.495706
3520.478034	958095.214717	41.500711
3520.575751	957714.084382	41.505716
3520.508558	957343.249482	41.510720
3519.998981	956975.306752	41.515725
3520.305123	956602.598036	41.520730
3520.479835	956235.868056	41.525735
3520.457924	955869.637458	41.530740
3520.165135	955505.291465	41.535744
3520.163793	955131.753926	41.540749
3520.377550	954766.983684	41.545754
3520.014765	954387.769124	41.550759
3519.739688	954020.776377	41.555764
3520.060321	953654.545035	41.560768
3519.676176	953305.083847	41.565773
3519.962473	952937.929841	41.570778
3519.590854	952578.317550	41.575783
3519.428078	952227.794844	41.580788
3519.602660	951889.045166	41.585792
3519.547173	951530.226547	41.590797
3519.026360	951184.562880	41.595802
3519.044544	950852.369652	41.600807
3519.317100	950501.459410	41.605812
3519.049835	950154.344950	41.610816
3518.828199	949816.862260	41.615821
3519.110185	949484.345266	41.620826
3518.981541	949145.846199	41.625831
3519.016417	948802.417581	41.630836
3518.692525	948464.958272	41.635840
3518.936163	948121.258223	41.640845
3518.698259	947787.185470	41.645850
3518.491718	947454.617259	41.650855
3518.727658	947096.109558	41.655860
3518.552375	946772.394239	41.660864
3518.322779	946452.209672	41.665869
3518.030828	946112.771552	41.670874
3518.015620	945785.425351	41.675879
3518.306123	945451.113759	41.680884
3517.800986	945132.711862	41.685888
3517.750010	944805.309323	41.690893
3518.005892	944478.027010	41.695898
3517.791993	944159.229761	41.700903
3517.714819	943827.076448	41.705908
3517.973498	943517.452754	41.710912
3517.705483	943199.275766	41.715917
3517.636394	942878.076621	41.720922
3517.347338	942557.468643	41.725927
3517.432839	942233.425678	41.730932
3517.413465	941934.292592	41.735936
3517.182985	941607.292214	41.740941
3517.243874	941297.664355	41.745946
3516.928540	940982.234042	41.750951
3517.113404	940679.544965	41.755956
3516.960221	940367.788491	41.760960
3516.933665	940056.663457	41.765965
3517.145068	939744.809627	41.770970
3516.818332	939445.679892	41.775975
3516.587982	939131.561416	41.780980
3516.540577	938827.844339	41.785984
3516.106895	938535.199551	41.790989
3516.177408	938231.907796	41.795994
3516.318654	937939.422586	41.800999
3516.187972	937639.006345	41.806004
3516.403050	937353.284919	41.811008
3516.281973	937045.832160	41.816013
3516.490411	936751.543169	41.821018
3515.961343	936453.426480	41.826023
3516.054589	936160.466164	41.831028
3515.761952	935880.599502	41.836032
3515.846759	935579.837876	41.841037
3515.851244	935290.968881	41.846042
3515.643483	935003.750053	41.851047
3516.030474	934716.705411	41.856052
3515.844128	934430.699132	41.861056
3515.463932	934132.522164	41.866061
3515.577743	933850.561272	41.871066
3515.328198	933560.967420	41.876071
3515.386884	933279.848841	41.881076
3515.004106	933007.810323	41.886080
3514.970635	932733.972474	41.891085
3515.240480	932453.830987	41.896090
3514.722828	932184.844042	41.901095
3514.910102	931904.975070	41.906100
3514.318862	931633.764171	41.911104
3514.670161	931378.898090	41.916109
3514.702357	931099.684179	41.921114
3514.352141	930825.703722	41.926119
3514.221616	930553.497411	41.931124
3514.263837	930292.100204	41.936128
3514.206233	930031.955037	41.941133
3514.369674	929773.489439	41.946138
3514.300540	929511.207777	41.951143
3514.282111	929235.169651	41.956148
3514.107584	928985.846204	41.961152
3513.947727	928721.811570	41.966157
3514.148576	928458.953250	41.971162
3514.052360	928205.353517	41.976167
3513.994850	927940.494739	41.981172
3514.004509	927678.109775	41.986176
3513.738255	927424.308746	41.991181
3513.918884	927167.251136	41.996186
3513.699774	926926.006099	42.001191
3513.914079	926653.543500	42.006196
3513.626784	926404.502306	42.011200
3513.597338	926156.271982	42.016205
3513.776422	925908.091898	42.021210
3513.542962	925653.624706	42.026215
3513.163024	925398.881193	42.031220
3513.139802	925157.235751	42.036224
3513.204072	924928.446134	42.041229
3513.297053	924669.552679	42.046234
3513.025656	924428.780491	42.051239
3512.876788	924179.805324	42.056244
3513.108229	923945.754652	42.061248
3512.772844	923702.268359	42.066253
3513.053810	923465.400271	42.071258
3512.851080	923229.082233	42.076263
3512.894499	922988.097466	42.081268
3512.834920	922753.177382	42.086272
3512.476107	922521.662327	42.091277
3512.630812	922276.107338	42.096282
3512.439117	922046.275477	42.101287
3512.627896	921816.082588	42.106292
3512.288730	921580.291794	42.111296
3512.254789	921360.119646	42.116301
3512.278116	921118.862251	42.121306
3512.378211	920901.150405	42.126311
3512.268318	920672.208560	42.131316
3511.977801	920448.000959	42.136320
3512.186318	920216.004905	42.141325
3512.072214	919995.405533	42.146330
3511.719035	919774.644119	42.151335
3511.870506	919551.962317	42.156340
3511.647430	919331.450077	42.161344
3511.634843	919109.643180	42.166349
3511.905893	918899.232489	42.171354
3511.841909	918688.965076	42.176359
3511.725510	918457.139748	42.181364
3511.922874	918244.983468	42.186368
3511.526130	918031.088020	42.191373
3511.649931	917815.365814	42.196378
3511.469224	917601.899156	42.201383
3511.617954	917386.637130	42.206388
3511.572662	917163.408486	42.211392
3511.633263	916958.155688	42.216397
3511.881758	916734.861079	42.221402
3511.030380	916526.854066	42.226407
3511.448786	916306.883633	42.231412
3511.456240	916106.999275	42.236416
3511.052895	915893.309759	42.241421
3511.235559	915678.263531	42.246426
3511.090169	915475.010979	42.251431
3510.894373	915264.151511	42.256436
3510.753535	915061.845830	42.261440
3510.721235	914859.129554	42.266445
3510.813537	914663.030635	42.271450
3510.372487	914467.590436	42.276455
3510.328908	914265.624532	42.281460
3510.568024	914067.650070	42.286464
3510.701462	913873.924121	42.291469
3510.801534	913681.738059	42.296474
3510.539318	913477.081938	42.301479
3510.822353	913287.067512	42.306484
3510.569640	913080.757352	42.311488
3510.543842	912889.431306	42.316493
3510.610888	912687.485378	42.321498
3510.130711	912498.725538	42.326503
3510.204160	912297.535003	42.331508
3510.156280	912112.544738	42.336512
3509.821781	911926.246453	42.341517
3510.131551	911724.803313	42.346522
3509.987780	911539.038662	42.351527
3510.089937	911367.875168	42.356532
3509.986889	911181.513535	42.361536
3509.844661	910991.778945	42.366541
3509.895970	910803.547980	42.371546
3509.675194	910624.993513	42.376551
3509.707287	910451.499955	42.381556
3509.949847	910263.990137	42.386560
3509.903697	910080.955476	42.391565
3509.989684	909888.542787	42.396570
3509.596425	909712.204251	42.401575
3509.635025	909530.486936	42.406580
3509.704610	909355.410357	42.411584
3509.131729	909181.976576	42.416589
3509.572387	908996.897675	42.421594
3509.199994	908833.060843	42.426599
3509.211882	908656.525462	42.431604
3509.408363	908486.221230	42.436608
3509.163967	908306.535110	42.441613
3509.170609	908138.276302	42.446618
3509.185768	907981.292954	42.451623
3508.733905	907802.588936	42.456628
3508.777663	907631.029990	42.461632
3508.696138	907469.901465	42.466637
3508.950032	907297.236783	42.471642
3508.399342	907144.759166	42.476647
3508.674838	906982.496815	42.481652
3508.688455	906816.414981	42.486656
3508.701426	906656.211744	42.491661
3508.947223	906497.122965	42.496666
3508.713620	906338.012160	42.501671
3508.653768	906176.070884	42.506676
3508.680379	906015.461104	42.511680
3508.540582	905861.915966	42.516685
3508.727513	905686.800699	42.521690
3508.444768	905541.373479	42.526695
3508.268277	905382.322401	42.531700
3508.306659	905223.810230	42.536704
3508.448586	905074.731290	42.541709
3508.308026	904904.372778	42.546714
3508.392238	904752.882732	42.551719
3508.031855	904606.479069	42.556724
3508.294010	904454.951618	42.561728
3507.969976	904310.656942	42.566733
3508.315253	904148.204018	42.571738
3508.102053	903996.742447	42.576743
3508.334697	903849.738753	42.581748
3508.211711	903697.192713	42.586752
3507.790712	903552.122401	42.591757
3507.950360	903405.601573	42.596762
3507.713671	903256.729483	42.601767
3507.980085	903110.183329	42.606772
3507.720487	902966.615416	42.611776
3507.764276	902828.012683	42.616781
3507.843838	902673.764585	42.621786
3507.660202	902531.427742	42.626791
3507.558531	902387.432872	42.631796
3507.712341	902248.121999	42.636800
3507.715266	902104.778319	42.641805
3507.794763	901955.529955	42.646810
3507.584263	901823.508394	42.651815
3507.602356	901671.559651	42.656820
3507.643858	901545.571808	42.661824
3507.618962	901397.001555	42.666829
3507.530203	901248.148262	42.671834
3507.450726	901110.392274	42.676839
3507.590243	900976.072561	42.681844
3507.793369	900839.808151	42.686848
3507.333250	900693.897867	42.691853
3507.626093	900548.149410	42.696858
3507.185301	900419.029432	42.701863
3507.272577	900278.908209	42.706868
3507.275249	900149.998675	42.711872
3506.962964	900022.876238	42.716877
3507.308103	899888.400115	42.721882
3507.300925	899750.888616	42.726887
3507.183496	899626.525632	42.731892
3507.115750	899494.522413	42.736896
3506.647969	899360.553915	42.741901
3506.725625	899242.524317	42.746906
3506.877652	899120.616800	42.751911
3507.025514	898985.089252	42.756916
3506.963899	898859.154827	42.761920
3506.725542	898737.979450	42.766925
3506.876309	898612.101108	42.771930
3506.902236	898483.246213	42.776935
3506.749809	898355.383692	42.781940
3506.968799	898229.388990	42.786945
3506.557736	898103.591877	42.791949
3506.991186	897974.175247	42.796954
3506.592612	897859.189774	42.801959
3506.641531	897729.154677	42.806964
3506.260887	897614.451081	42.811969
3506.358397	897499.666382	42.816973
3506.440030	897368.748142	42.821978
3506.288579	897268.491236	42.826983
3506.279508	897140.384393	42.831988
3506.401643	897031.093121	42.836993
3506.306341	896911.111007	42.841997
3506.535530	896805.275978	42.847002
3506.354165	896688.588393	42.852007
3506.439095	896558.230604	42.857012
3506.628761	896443.989072	42.862017
3506.429718	896323.045343	42.867021
3506.544330	896206.202438	42.872026
3506.410564	896088.624994	42.877031
3506.107302	895968.753827	42.882036
3506.174255	895865.633738	42.887041
3505.994088	895744.191378	42.892045
3506.361161	895637.248831	42.897050
3506.292009	895532.212322	42.902055
3506.310037	895418.268348	42.907060
3506.381377	895297.064921	42.912065
3505.761830	895192.112800	42.917069
3505.907699	895076.594561	42.922074
3505.750123	894966.343114	42.927079
3505.871896	894859.233043	42.932084
3506.100769	894756.162798	42.937089
3505.681154	894645.948310	42.942093
3505.725086	894535.558657	42.947098
3505.673463	894435.331898	42.952103
3505.737084	894329.091370	42.957108
3505.747639	894219.281053	42.962113
3505.677853	894125.334953	42.967117
3505.787621	894015.504364	42.972122
3505.840847	893918.151237	42.977127
3505.485993	893805.879768	42.982132
3505.930116	893700.144847	42.987137
3505.424231	893597.464704	42.992141
3505.636810	893489.347171	42.997146
3505.564113	893399.159938	43.002151
3505.308089	893301.170483	43.007156
3505.499340	893197.594850	43.012161
3505.436685	893096.766282	43.017165
3505.419523	893006.080273	43.022170
3505.210681	892899.664627	43.027175
3505.417861	892801.686967	43.032180
3505.525827	892705.367688	43.037185
3505.391994	892607.829642	43.042189
3505.697536	892506.543228	43.047194
3505.196177	892418.248277	43.052199
3505.453072	892322.381477	43.057204
3505.400410	892228.304622	43.062209
3505.349136	892130.164637	43.067213
3505.555401	892025.404897	43.072218
3505.488795	891941.672585	43.077223
3505.476579	891835.978351	43.082228
3505.626137	891734.800676	43.087233
3505.295082	891639.406121	43.092237
3505.461106	891529.615161	43.097242
3505.399816	891444.037220	43.102247
3505.093847	891348.536972	43.107252
3505.343536	891258.359551	43.112257
3505.405890	891157.959761	43.117261
3505.510455	891062.870691	43.122266
3505.252395	890970.257750	43.127271
3505.191415	890872.774837	43.132276
3505.385002	890769.251573	43.137281
3505.032574	890682.065942	43.142285
3505.179238	890583.963569	43.147290
3504.994935	890505.065892	43.152295
3505.140401	890417.600759	43.157300
3504.986419	890321.187798	43.162305
3504.734407	890228.561876	43.167309
3505.117069	890136.216827	43.172314
3505.154015	890043.927251	43.177319
3505.005091	889958.148099	43.182324
3504.884862	889861.238173	43.187329
3504.848947	889784.918051	43.192333
3505.277113	889694.202957	43.197338
3504.888332	889614.069099	43.202343
3504.773858	889516.281734	43.207348
3505.266776	889428.744303	43.212353
3504.897562	889336.607026	43.217357
3505.350073	889252.459680	43.222362
3504.433253	889169.600940	43.227367
3504.571746	889069.829328	43.232372
3504.934038	888987.434481	43.237377
3504.647340	888907.177195	43.242381
3504.630864	888820.681973	43.247386
3504.561978	888746.288590	43.252391
3504.342787	888666.016818	43.257396
3504.682954	888601.133131	43.262401
3504.531568	888510.591624	43.267405
3504.672228	888421.258476	43.272410
3504.653757	888347.916017	43.277415
3504.527463	888258.237272	43.282420
3504.635003	888176.937212	43.287425
3504.522662	888102.058840	43.292429
3504.852851	888017.333011	43.297434
3504.335626	887945.906200	43.302439
3504.516230	887856.170637	43.307444
3504.618813	887769.640022	43.312449
3504.781765	887708.936706	43.317453
3504.371940	887613.972113	43.322458
3504.175733	887536.777618	43.327463
3504.275007	887464.081951	43.332468
3504.547116	887381.098345	43.337473
3504.209443	887307.504905	43.342477
3504.421958	887228.884033	43.347482
3504.488055	887165.287515	43.352487
3504.054147	887072.834325	43.357492
3504.179098	887006.322840	43.362497
3504.127729	886933.161383	43.367501
3504.469966	886851.416840	43.372506
3504.522375	886785.689070	43.377511
3504.125470	886699.902237	43.382516
3504.147678	886625.369698	43.387521
3503.900362	886557.656092	43.392525
3504.347631	886478.502376	43.397530
3504.193611	886413.191555	43.402535
3504.090225	886344.677381	43.407540
3504.280279	886263.820774	43.412545
3504.408909	886187.813101	43.417549
3504.117569	886121.456823	43.422554
3504.133663	886052.919509	43.427559
3504.015160	885978.885829	43.432564
3504.313169	885909.913167	43.437569
3503.787755	885839.139252	43.442573
3503.975817	885767.182060	43.447578
3504.123190	885703.943307	43.452583
3503.916323	885621.013365	43.457588
3504.072276	885559.804600	43.462593
3504.025505	885490.786944	43.467597
3504.172353	885418.541782	43.472602
3504.218071	885350.862585	43.477607
3504.068439	885272.371611	43.482612
3504.065633	885204.698702	43.487617
3503.949844	885142.562149	43.492621
3504.186963	885066.521893	43.497626
3503.995548	885010.495888	43.502631
3503.987226	884935.172076	43.507636
3504.091969	884863.991962	43.512641
3503.842167	884801.680193	43.517645
3504.015596	884719.546095	43.522650
3503.975085	884663.588700	43.527655
3503.632255	884599.450423	43.532660
3504.023146	884520.763399	43.537665
3503.899208	884453.004853	43.542669
3503.988793	884384.532534	43.547674
3503.986983	884329.727493	43.552679
3504.025632	884269.492743	43.557684
3503.753185	884190.523209	43.562689
3503.465091	884120.560686	43.567693
3503.910194	884059.385294	43.572698
3503.669656	883997.741207	43.577703
3503.642708	883924.828241	43.582708
3503.732423	883869.229084	43.587713
3503.437883	883807.398198	43.592717
3503.523246	883746.956659	43.597722
3504.005972	883689.547923	43.602727
3503.727761	883625.194555	43.607732
3504.062411	883551.345758	43.612737
3503.790607	883484.471863	43.617741
3503.684154	883420.281617	43.622746
3503.541538	883367.427600	43.627751
3503.532931	883308.546523	43.632756
3503.786889	883246.522459	43.637761
3503.746348	883190.938281	43.642765
3503.602574	883114.354146	43.647770
3503.471537	883055.393828	43.652775
3503.569726	882990.874577	43.657780
3503.613286	882936.920604	43.662785
3503.526550	882870.299717	43.667789
3503.815050	882806.909325	43.672794
3503.678381	882755.501600	43.677799
3503.459412	882692.871566	43.682804
3503.638079	882624.363855	43.687809
3503.423085	882575.970054	43.692813
3503.765108	882520.025868	43.697818
3503.733859	882447.095099	43.702823
3503.526297	882392.015119	43.707828
3503.519539	882337.192125	43.712833
3503.126403	882287.856649	43.717837
3503.458147	882213.507060	43.722842
3503.521494	882165.838916	43.727847
3503.436046	882111.317361	43.732852
3503.594228	882045.421628	43.737857
3503.339229	881993.929812	43.742861
3503.556158	881933.447783	43.747866
3503.627297	881878.220163	43.752871
3503.421752	881824.006320	43.757876
3503.615733	881746.670466	43.762881
3503.478877	881698.159631	43.767885
3503.419635	881635.298173	43.772890
3503.564849	881584.802431	43.777895
3503.164499	881533.330495	43.782900
3503.501133	881465.945679	43.787905
3503.176323	881424.826221	43.792909
3503.103360	881363.804785	43.797914
3503.212273	881312.440757	43.802919
3503.131762	881251.419391	43.807924
3503.499267	881190.517341	43.812929
3503.110224	881148.050166	43.817933
3503.012352	881083.929663	43.822938
3503.031356	881040.716295	43.827943
3502.896448	880989.583369	43.832948
3502.868779	880937.366580	43.837953
3503.148445	880895.853150	43.842957
3503.009814	880845.785336	43.847962
3502.819480	880799.891819	43.852967
3502.491517	880749.176151	43.857972
3502.754620	880702.044489	43.862977
3502.456426	880668.957198	43.867981
3502.808202	880612.605585	43.872986
3502.915905	880577.125504	43.877991
3502.858230	880537.699847	43.882996
3502.865882	880490.124102	43.888001
3502.783659	880444.113088	43.893005
3503.044274	880392.909782	43.898010
3502.710552	880347.327023	43.903015
3502.707267	880304.887060	43.908020
3502.897999	880257.957543	43.913025
3502.583436	880230.393620	43.918029
3502.985795	880169.281410	43.923034
3502.918540	880126.075499	43.928039
3502.942971	880072.679615	43.933044
3503.023867	880028.479570	43.938049
3503.038968	879990.201052	43.943053
3502.955053	879934.011598	43.948058
3503.197276	879882.903771	43.953063
3502.795974	879840.719827	43.958068
3502.935625	879786.236401	43.963073
3502.929016	879748.832031	43.968077
3503.017186	879699.492292	43.973082
3502.934646	879656.576157	43.978087
3502.813230	879614.732102	43.983092
3502.962849	879552.007662	43.988097
3502.758042	879504.846555	43.993101
3502.856356	879467.907656	43.998106
3502.863020	879425.750419	44.003111
3502.667843	879371.512126	44.008116
3502.790623	879324.295596	44.013121
3502.763925	879290.865043	44.018125
3502.823590	879241.913805	44.023130
3502.535780	879195.054623	44.028135
3502.882986	879152.160910	44.033140
3503.181339	879102.587693	44.038145
3502.726194	879066.512783	44.043149
3502.923674	879018.506150	44.048154
3502.651950	878962.629082	44.053159
3502.856599	878930.224467	44.058164
3503.057550	878876.304011	44.063169
3502.708460	878833.425768	44.068173
3502.662312	878794.180325	44.073178
3502.831232	878753.833041	44.078183
3502.657924	878716.449553	44.083188
3503.115058	878668.397281	44.088193
3502.691571	878620.295851	44.093197
3502.855665	878563.083158	44.098202
3502.513446	878530.378735	44.103207
3502.992476	878489.009283	44.108212
3503.142713	878441.684208	44.113217
3502.942242	878402.655429	44.118221
3503.144301	878346.403655	44.123226
3503.156432	878296.289220	44.128231
3502.566822	878244.722604	44.133236
3502.756559	878213.673528	44.138241
3502.682791	878177.724180	44.143245
3502.508809	878118.818090	44.148250
3502.686086	878088.352002	44.153255
3502.540459	878040.393909	44.158260
3503.154276	877990.177737	44.163265
3502.790508	877950.591249	44.168269
3502.573575	877915.924049	44.173274
3502.598295	877885.288172	44.178279
3502.266900	877845.986456	44.183284
3502.910270	877805.554502	44.188289
3503.039970	877762.880372	44.193293
3502.825036	877709.502430	44.198298
3502.567567	877666.988331	44.203303
3502.573277	877620.068220	44.208308
3502.918546	877579.780773	44.213313
3502.439553	877542.924889	44.218317
3502.771566	877506.710702	44.223322
3502.726313	877465.129610	44.228327
3502.526270	877418.920399	44.233332
3502.474863	877373.268008	44.238337
3502.442938	877343.511150	44.243341
3502.590049	877304.514762	44.248346
3502.338193	877259.379243	44.253351
3502.026059	877228.795448	44.258356
3502.702754	877195.043194	44.263361
3502.444888	877162.608101	44.268365
3502.452738	877118.979896	44.273370
3502.575333	877083.476257	44.278375
3502.553517	877049.838255	44.283380
3502.786328	877007.432517	44.288385
3502.454745	876977.238423	44.293389
3502.472478	876940.199972	44.298394
3502.472369	876893.275031	44.303399
3502.430703	876861.287423	44.308404
3502.820881	876810.128517	44.313409
3502.236006	876788.313253	44.318413
3502.504771	876752.201810	44.323418
3502.649967	876713.492695	44.328423
3502.297436	876667.011839	44.333428
3502.618017	876636.029853	44.338433
3502.149780	876600.523690	44.343437
3502.598437	876569.229379	44.348442
3502.875280	876522.837613	44.353447
3502.516745	876474.998804	44.358452
3502.655868	876440.264251	44.363457
3502.473344	876397.243833	44.368461
3502.827526	876360.437195	44.373466
3502.351144	876331.718072	44.378471
3502.367442	876286.724847	44.383476
3502.762256	876250.104753	44.388481
3501.978232	876211.157580	44.393485
3502.343773	876173.475228	44.398490
3502.500742	876137.184515	44.403495
3502.277073	876106.192452	44.408500
3502.600961	876076.079679	44.413505
3502.508129	876038.956820	44.418509
3502.586359	875996.181419	44.423514
3502.667145	875960.968820	44.428519
3502.490270	875926.380275	44.433524
3502.769419	875870.286109	44.438529
3502.665390	875847.515404	44.443533
3502.927833	875810.526517	44.448538
3502.815426	875758.956459	44.453543
3502.405013	875723.726401	44.458548
3502.601116	875670.941081	44.463553
3502.260516	875645.590298	44.468557
3502.582190	875604.129580	44.473562
3502.592892	875566.307874	44.478567
3502.414508	875525.510839	44.483572
3502.468196	875482.347861	44.488577
3502.283988	875456.582595	44.493581
3502.231844	875408.781638	44.498586
3502.528965	875374.790612	44.503591
3502.356159	875345.143863	44.508596
3502.376445	875296.069342	44.513601
3502.087427	875279.145673	44.518605
3502.323523	875233.720299	44.523610
3502.581484	875212.342210	44.528615
3502.307391	875171.170575	44.533620
3502.442192	875134.489436	44.538625
3502.241936	875111.149854	44.543629
3502.345250	875074.473531	44.548634
3502.532193	875037.201302	44.553639
3502.324331	875008.722443	44.558644
3502.495544	874967.185070	44.563649
3502.099329	874938.542936	44.568653
3502.466623	874894.936064	44.573658
3502.236310	874872.376378	44.578663
3502.251481	874840.853394	44.583668
3502.637962	874796.272769	44.588673
3502.246475	874768.307942	44.593677
3502.200756	874732.332968	44.598682
3502.624769	874701.129836	44.603687
3502.484914	874664.685015	44.608692
3502.721037	874625.753273	44.613697
3502.468810	874596.212844	44.618701
3502.333046	874558.796791	44.623706
3502.338439	874510.397148	44.628711
3502.506079	874472.639588	44.633716
3502.505558	874439.080203	44.638721
3502.620929	874408.314355	44.643725
3502.091721	874360.971505	44.648730
3502.507246	874334.132596	44.653735
3502.309469	874304.096763	44.658740
3502.632728	874269.707112	44.663745
3502.305242	874243.766175	44.668749
3502.326380	874195.361366	44.673754
3502.215361	874171.421390	44.678759
3502.307054	874131.443223	44.683764
3502.585316	874095.314005	44.688769
3502.175444	874062.207923	44.693773
3502.446751	874036.943422	44.698778
3502.540988	874006.178970	44.703783
3502.351128	873970.029114	44.708788
3502.393051	873920.842631	44.713793
3502.225512	873887.792651	44.718797
3502.176178	873858.603123	44.723802
3502.147429	873827.955011	44.728807
3502.452628	873801.325878	44.733812
3502.366498	873771.365953	44.738817
3502.346167	873735.477749	44.743821
3502.120153	873703.794443	44.748826
3502.107337	873669.262673	44.753831
3502.197953	873635.489713	44.758836
3502.480863	873600.811818	44.763841
3502.331281	873572.898490	44.768845
3501.948747	873538.232855	44.773850
3501.953677	873493.802317	44.778855
3502.081085	873475.834788	44.783860
3502.205418	873440.309000	44.788865
3502.075926	873423.450743	44.793869
3502.051691	873387.270045	44.798874
3502.332794	873365.784484	44.803879
3502.177366	873337.579980	44.808884
3502.271782	873300.991164	44.813889
3502.066796	873272.406468	44.818893
3501.842606	873245.474014	44.823898
3501.992984	873211.979838	44.828903
3501.714836	873194.272301	44.833908
3502.200464	873156.939049	44.838913
3502.044717	873135.427614	44.843917
3501.871553	873111.881657	44.848922
3502.025763	873074.214428	44.853927
3501.961372	873053.463770	44.858932
3501.996279	873015.233728	44.863937
3502.354871	873000.816286	44.868941
3501.917582	872975.275949	44.873946
3502.210755	872936.808818	44.878951
3501.900825	872903.873832	44.883956
3502.625202	872875.619202	44.888961
3502.416724	872853.630339	44.893965
3502.362134	872805.614749	44.898970
3502.214136	872778.570604	44.903975
3501.582750	872738.702189	44.908980
3501.771241	872728.484017	44.913985
3502.131348	872689.228089	44.918989
3502.249758	872670.192368	44.923994
3502.374676	872640.968144	44.928999
3501.836976	872614.666615	44.934004
3502.332678	872577.425095	44.939009
3502.149519	872545.825568	44.944013
3501.969721	872510.441354	44.949018
3502.155219	872478.295608	44.954023
3501.838807	872449.628281	44.959028
3502.172223	872430.556371	44.964033
3501.652439	872409.781465	44.969037
3501.740058	872391.332083	44.974042
3501.871188	872368.703313	44.979047
3501.757933	872338.352518	44.984052
3502.136833	872310.152129	44.989057
3502.021191	872284.070683	44.994061
3502.163382	872257.752586	44.999066
3502.176820	872226.895205	45.004071
3501.983703	872205.483587	45.009076
3502.152617	872160.239825	45.014081
3502.137267	872145.881927	45.019085
3502.045194	872100.098522	45.024090
3502.148756	872076.114741	45.029095
3501.740746	872065.023389	45.034100
3502.128240	872038.178748	45.039105
3501.964882	871997.160884	45.044109
3501.913921	871981.547025	45.049114
3502.058921	871936.596605	45.054119
3502.014531	871916.906059	45.059124
3501.943932	871889.554014	45.064129
3501.943478	871870.923461	45.069133
3501.708606	871838.940556	45.074138
3501.813412	871816.993277	45.079143
3501.922050	871790.872717	45.084148
3502.235452	871745.602002	45.089153
3501.858775	871740.618224	45.094157
3502.057558	871708.272059	45.099162
3501.874036	871686.371802	45.104167
3501.723796	871665.339328	45.109172
3502.074898	871630.250565	45.114177
3501.805573	871612.245734	45.119181
3502.087738	871581.631854	45.124186
3501.818584	871566.635095	45.129191
3501.889840	871522.664103	45.134196
3502.150932	871504.377477	45.139201
3501.542225	871487.980843	45.144205
3501.873087	871467.547697	45.149210
3501.930736	871456.281445	45.154215
3501.700787	871424.683671	45.159220
3501.934410	871397.376286	45.164225
3501.865975	871361.190546	45.169229
3501.934486	871335.753909	45.174234
3502.172937	871311.259608	45.179239
3501.780535	871295.797248	45.184244
3502.065091	871264.502036	45.189249
3501.728539	871241.848995	45.194253
3502.082725	871216.461829	45.199258
3502.074908	871183.176396	45.204263
3501.654765	871169.562160	45.209268
3501.947037	871137.682732	45.214273
3501.995075	871114.189465	45.219277
3502.056805	871083.997541	45.224282
3501.899226	871058.402874	45.229287
3501.859486	871033.953269	45.234292
3501.922765	870999.781660	45.239297
3501.784671	870995.631388	45.244301
3501.767080	870961.472884	45.249306
3501.691387	870929.750019	45.254311
3501.539218	870926.669574	45.259316
3501.725929	870888.109712	45.264321
3501.604787	870867.748986	45.269325
3501.964599	870855.073095	45.274330
3501.872681	870825.390435	45.279335
3501.702662	870816.683842	45.284340
3502.032386	870790.134267	45.289345
3501.698301	870755.250303	45.294349
3501.916746	870734.930228	45.299354
3501.713867	870703.809439	45.304359
3501.979379	870698.427814	45.309364
3502.121440	870661.523769	45.314369
3501.870735	870634.583857	45.319373
3501.886004	870605.852998	45.324378
3502.184877	870577.366446	45.329383
3502.225171	870566.586656	45.334388
3502.245560	870532.710610	45.339393
3502.272604	870507.374331	45.344397
3502.043508	870473.830226	45.349402
3502.059167	870445.486764	45.354407
3502.318899	870420.111780	45.359412
3502.211292	870388.391296	45.364417
3502.166363	870354.816180	45.369421
3502.143766	870316.481234	45.374426
3502.005292	870296.897898	45.379431
3501.952869	870251.482005	45.384436
3502.159649	870238.053531	45.389441
3501.924317	870213.632790	45.394445
3502.272198	870186.689298	45.399450
3502.036811	870147.320635	45.404455
3502.027938	870140.139515	45.409460
3502.418388	870096.396619	45.414465
3501.991673	870083.266296	45.419469
3501.982103	870041.530189	45.424474
3502.413944	870019.037097	45.429479
3501.968255	869986.302458	45.434484
3502.349637	869957.605231	45.439489
3502.285711	869927.331097	45.444493
3502.324823	869893.836611	45.449498
3502.342765	869867.916718	45.454503
3501.863816	869840.816689	45.459508
3502.104619	869802.629187	45.464513
3502.228741	869772.323286	45.469517
3502.069870	869756.527242	45.474522
3502.434042	869714.047787	45.479527
3502.242065	869694.180079	45.484532
3502.029213	869654.319101	45.489537
3501.973557	869635.690665	45.494541
3502.108029	869601.790547	45.499546
3502.252815	869575.460200	45.504551
3501.942927	869549.981229	45.509556
3502.049360	869518.706229	45.514561
3501.603407	869488.007442	45.519565
3501.977034	869463.871602	45.524570
3501.936423	869433.882351	45.529575
3501.674977	869412.763179	45.534580
3501.964512	869386.990606	45.539585
3502.160121	869376.765536	45.544589
3502.276402	869337.430675	45.549594
3502.189260	869315.214601	45.554599
3501.870851	869285.658682	45.559604
3502.317091	869251.802296	45.564609
3502.440028	869228.192199	45.569613
3502.237754	869196.480986	45.574618
3501.887444	869159.066319	45.579623
3502.168550	869130.381654	45.584628
3502.487605	869100.719797	45.589633
3502.077152	869080.594802	45.594637
3502.046030	869047.010069	45.599642
3502.250147	869031.734791	45.604647
3501.916267	869007.325353	45.609652
3502.102577	868969.044435	45.614657
3502.119287	868928.655388	45.619661
3502.104927	868913.124554	45.624666
3502.345136	868882.697944	45.629671
3501.914216	868848.498378	45.634676
3501.964366	868817.228989	45.639681
3502.013170	868804.988351	45.644685
3502.133698	868771.959600	45.649690
3502.360473	868745.223755	45.654695
3501.695669	868719.411373	45.659700
3501.979367	868701.500810	45.664705
3502.130077	868677.301448	45.669709
3502.015289	868641.106871	45.674714
3501.998833	868607.517257	45.679719
3502.110058	868590.217308	45.684724
3502.202412	868559.036708	45.689729
3502.205051	868530.492142	45.694733
3502.090935	868498.180168	45.699738
3502.235939	868468.252592	45.704743
3501.680044	868439.799614	45.709748
3501.922212	868408.690640	45.714753
3501.905626	868388.692607	45.719757
3501.957749	868362.275106	45.724762
3502.137079	868345.351599	45.729767
3501.644521	868309.799814	45.734772
3501.990683	868297.217871	45.739777
3502.006091	868258.475109	45.744781
3501.915363	868241.692896	45.749786
3501.848521	868206.361642	45.754791
3501.673160	868187.457138	45.759796
3501.916688	868167.027130	45.764801
3502.041899	868137.683738	45.769805
3502.152765	868124.848913	45.774810
3502.033885	868075.252328	45.779815
3501.807296	867992.174302	45.784820
3501.777684	867857.308407	45.789825
3501.827171	867651.929598	45.794829
3501.913561	867393.905467	45.799834
3501.996892	867085.954982	45.804839
3501.413380	866713.514916	45.809844
3501.521501	866264.111600	45.814849
3501.444884	865779.348559	45.819853
3501.275559	865231.516521	45.824858
3501.016313	864619.334916	45.829863
3500.552489	863947.952804	45.834868
3500.840948	863199.507030	45.839873
3500.502345	862407.337687	45.844877
3500.228372	861535.543597	45.849882
3500.007207	860606.938669	45.854887
3499.345687	859624.203724	45.859892
3499.460369	858557.548702	45.864897
3499.065491	857430.875282	45.869901
3498.838208	856239.758651	45.874906
3498.275949	854973.054521	45.879911
3497.759417	853646.226555	45.884916
3497.547030	852234.272853	45.889921
3497.119326	850768.965236	45.894925
3496.417699	849228.362510	45.899930
3495.938079	847607.846945	45.904935
3495.325896	845922.618188	45.909940
3495.132943	844170.292883	45.914945
3494.257877	842348.658293	45.919949
3493.875375	840447.465858	45.924954
3493.506763	838480.823140	45.929959
3492.279850	836444.326527	45.934964
3491.967559	834333.275605	45.939969
3491.203014	832148.997350	45.944973
3490.156126	829893.102514	45.949978
3489.537216	827580.355504	45.954983
3488.660236	825201.036807	45.959988
3488.282250	822750.992767	45.964993
3487.302791	820221.623299	45.969997
3486.061467	817629.180917	45.975002
3485.209424	814982.645387	45.980007
3484.326127	812260.380442	45.985012
3483.714127	809464.504932	45.990017
3482.595221	806612.023325	45.995021
3481.594142	803693.108652	46.000026
3480.875602	800702.162500	46.005031
3479.739978	797642.994639	46.010036
3479.160583	794508.293014	46.015041
3478.011150	791328.118561	46.020045
3476.847862	788057.652801	46.025050
3476.030630	784729.618548	46.030055
3474.883490	781335.892558	46.035060
3473.752805	777855.272127	46.040065
3472.828919	774328.534551	46.045069
3471.619034	770730.681459	46.050074
3470.267035	767070.028526	46.055079
3468.935831	763350.219716	46.060084
3467.971730	759544.186895	46.065089
3466.071463	755703.618294	46.070093
3465.213891	751779.158939	46.075098
3463.909212	747791.353742	46.080103
3462.102336	743745.028666	46.085108
3461.101438	739636.435530	46.090113
3459.525163	735467.904492	46.095117
3458.174256	731232.299646	46.100122
3456.837500	726936.856838	46.105127
3455.006211	722573.014073	46.110132
3454.176242	718137.465768	46.115137
3452.316730	713649.861840	46.120141
3450.607686	709100.617704	46.125146
3449.135642	704474.497488	46.130151
3447.192438	699812.579191	46.135156
3445.764977	695074.839325	46.140161
3444.107394	690278.874822	46.145165
3442.417849	685432.607253	46.150170
3441.059121	680508.633607	46.155175
3438.649334	675533.256221	46.160180
3437.440673	670493.890429	46.165185
3435.406642	665400.683473	46.170189
3433.255089	660247.181135	46.175194
3431.672348	655012.087185	46.180199
3429.749852	649754.127935	46.185204
3427.894716	644423.044934	46.190209
3425.729114	639033.584918	46.195213
3423.949615	633592.592558	46.200218
3422.063331	628096.608859	46.205223
3419.906522	622560.101409	46.210228
3417.745174	616930.879035	46.215233
3415.908691	611280.864274	46.220237
3413.611249	605562.084430	46.225242
3411.368509	599792.676227	46.230247
3408.863790	593978.395031	46.235252
3406.766848	588102.835766	46.240257
3404.505755	582191.448440	46.245261
3402.020974	576212.456218	46.250266
3399.882401	570194.965193	46.255271
3397.234364	564134.790689	46.260276
3394.814971	558018.512557	46.265281
3392.492178	551858.936906	46.270285
3390.043771	545649.599708	46.275290
3387.811265	539393.316575	46.280295
3384.962020	533103.751787	46.285300
3382.375539	526748.775130	46.290305
3379.717154	520363.830509	46.295309
3377.035603	513927.921134	46.300314
3374.166875	507458.014358	46.305319
3371.525628	500948.407688	46.310324
3368.759093	494376.925198	46.315329
3365.816584	487796.916764	46.320333
3362.943036	481173.474166	46.325338
3360.300084	474496.772457	46.330343
3357.345311	467802.535459	46.335348
3354.447028	461051.484088	46.340353
3351.160499	454282.697631	46.345357
3348.189520	447474.416243	46.350362
3345.536611	440633.529968	46.355367
3342.124097	433774.323310	46.360372
3339.102634	426867.789550	46.365377
3335.853773	419943.444850	46.370381
3332.419296	412986.267040	46.375386
3329.438916	406003.193659	46.380391
3325.790108	399009.617304	46.385396
3322.354907	391956.246061	46.390401
3319.113752	384906.089386	46.395405
3315.652040	377835.050831	46.400410
3312.542329	370724.216816	46.405415
3309.050880	363599.512335	46.410420
3305.389331	356449.079009	46.415425
3301.482556	349293.105417	46.420429
3297.512149	342125.618516	46.425434
3294.202079	334940.476425	46.430439
3290.387210	327746.125607	46.435444
3286.775054	320535.944237	46.440449
3283.020611	313309.133768	46.445453
3279.035865	306078.883185	46.450458
3275.306301	298849.380120	46.455463
3271.128245	291615.154666	46.460468
3267.667194	284363.296931	46.465473
3263.747525	277106.290050	46.470477
3259.418683	269853.820097	46.475482
3255.471868	262582.470420	46.480487
3251.259789	255327.739912	46.485492
3247.193230	248069.687348	46.490497
3243.088132	240818.368896	46.495501
3238.470997	233566.926613	46.500506
3234.412415	226281.867040	46.505511
3230.193880	219002.265552	46.510516
3225.484592	211761.064520	46.515521
3221.131579	204548.152114	46.520525
3216.774777	197344.223207	46.525530
3212.342288	190139.731624	46.530535
3207.324066	182972.049522	46.535540
3202.932636	175814.257815	46.540545
3198.455584	168678.785543	46.545549
3193.763180	161562.222936	46.550554
3189.419524	154458.795738	46.555559
3184.308548	147385.845844	46.560564
3179.439672	140335.014315	46.565569
3174.038233	133314.141223	46.570573
3168.917329	126315.878575	46.575578
3164.033176	119361.926164	46.580583
3158.541786	112446.430560	46.585588
3153.230857	105561.482134	46.590593
3147.741583	98744.196523	46.595597
3141.906138	91948.978287	46.600602
3136.621789	85194.872981	46.605607
3130.564779	78530.758360	46.610612
3124.634930	71887.522919	46.615617
3117.977713	65323.260723	46.620621
3111.077215	58849.853546	46.625626
3104.071645	52437.277181	46.630631
3095.923333	46140.935341	46.635636
3085.543793	39993.325878	46.640641
3067.904916	34176.442281	46.645645
3048.669819	28601.198059	46.650650
3029.769124	23293.344633	46.655655
3009.625031	18353.584053	46.660660
2985.591247	13859.978332	46.665665
2958.413235	9887.384556	46.670669
2930.697197	6424.287746	46.675674
2904.076425	3444.367538	46.680679
2876.720207	1060.896251	46.685684
2811.602297	305.431268	46.690689
2750.150072	295.627034	46.695693
2728.273274	307.908074	46.700698
2737.525942	289.151454	46.705703
2762.165486	282.851356	46.710708
2787.480581	282.497553	46.715713
2806.275689	278.522827	46.720717
2816.158810	283.475706	46.725722
2818.730293	280.261122	46.730727
2815.165547	279.786861	46.735732
2810.101024	284.963296	46.740737
2806.230229	274.830660	46.745741
2801.835698	273.452132	46.750746
2798.770612	270.444448	46.755751
2795.975320	269.670773	46.760756
2793.867882	269.025947	46.765761
2791.521235	267.637138	46.770765
2788.891576	268.429089	46.775770
2786.385636	258.396119	46.780775
2782.929093	267.563557	46.785780
2780.080072	269.840596	46.790785
2777.062667	272.361706	46.795789
2773.967602	271.073497	46.800794
2771.440651	256.820081	46.805799
2768.158013	259.136700	46.810804
2764.788508	260.576849	46.815809
2761.710002	258.354067	46.820813
2758.255255	270.017212	46.825818
2755.325820	253.192931	46.830823
2751.921970	257.523902	46.835828
2748.656476	250.109116	46.840833
2745.415915	249.134634	46.845837
2741.849775	250.730384	46.850842
2738.659024	252.180129	46.855847
2735.665452	258.843098	46.860852
2732.184496	249.598594	46.865857
2729.110784	240.258881	46.870861
2725.852207	250.048064	46.875866
2722.724592	244.010496	46.880871
2718.756890	249.219946	46.885876
2715.293190	250.475169	46.890881
2712.349008	244.992263	46.895885
2708.918973	244.893299	46.900890
2705.536645	243.660036	46.905895
2702.062264	247.673112	46.910900
2698.846964	238.333893	46.915905
2695.423775	236.990158	46.920909
2691.824748	241.651356	46.925914
2688.902014	243.636697	46.930919
2685.325642	241.245494	46.935924
2681.638051	235.048946	46.940929
2678.245386	236.909758	46.945933
2674.627039	245.787410	46.950938
2671.228617	233.202157	46.955943
2667.916574	242.940987	46.960948
2664.781086	236.972252	46.965953
2661.653238	235.075794	46.970957
2657.961940	239.976025	46.975962
2654.106397	235.084018	46.980967
2650.139499	232.312871	46.985972
2647.652283	237.297797	46.990977
2644.744764	238.906096	46.995981
2640.514657	246.680935	47.000986
2636.688575	225.416143	47.005991
2633.995000	233.197518	47.010996
2630.336213	237.405258	47.016001
2626.532838	225.828195	47.021005
2622.733687	233.669274	47.026010
2619.888454	226.040787	47.031015
2616.619717	230.048001	47.036020
2613.037442	221.226459	47.041025
2609.960873	230.235758	47.046029
2606.584509	225.788461	47.051034
2602.522731	215.546660	47.056039
2598.684202	223.543439	47.061044
2595.509344	233.480292	47.066049
2592.726978	223.304027	47.071053
2589.150253	222.888742	47.076058
2585.219200	218.117797	47.081063
2581.843932	218.430614	47.086068
2578.755650	222.281770	47.091073
2574.718173	225.243666	47.096077
2571.036164	216.351396	47.101082
2568.178296	224.746015	47.106087
2564.824403	215.257305	47.111092
2560.964959	214.600581	47.116097
2557.700765	216.500260	47.121101
2553.812192	223.159065	47.126106
2550.862199	214.625937	47.131111
2547.048684	226.582427	47.136116
2543.760761	216.659745	47.141121
2540.147784	212.761480	47.146125
2536.591543	214.415333	47.151130
2533.656211	216.166423	47.156135
2529.603711	216.113875	47.161140
2526.234796	218.023753	47.166145
2522.590807	204.572587	47.171149
2519.436513	219.552097	47.176154
2516.324689	209.075843	47.181159
2512.159894	210.785946	47.186164
2508.597181	215.425083	47.191169
2505.494080	208.288389	47.196173
2501.937025	210.056069	47.201178
2498.696552	206.884538	47.206183
2494.881088	212.849303	47.211188
2491.559519	208.611705	47.216193
2488.147883	207.977824	47.221197
2484.243079	208.091568	47.226202
2481.182428	194.926615	47.231207
2477.621552	201.230235	47.236212
2474.407028	201.095468	47.241217
2470.841850	199.771779	47.246221
2467.178581	207.433045	47.251226
2463.771583	206.756185	47.256231
2459.630770	199.154381	47.261236
2456.079841	202.666563	47.266241
2453.236970	192.824631	47.271245
2449.651962	198.095027	47.276250
2446.354682	195.359564	47.281255
2443.140943	205.614894	47.286260
2439.257067	195.678387	47.291265
2435.661446	202.202872	47.296269
2431.963341	192.968436	47.301274
2428.697802	198.576455	47.306279
2425.013124	195.122691	47.311284
2421.405787	201.586562	47.316289
2418.632870	193.209218	47.321293
2415.060402	199.342710	47.326298
2411.759302	192.298172	47.331303
2407.922182	192.916061	47.336308
2404.507754	201.312235	47.341313
2400.952259	193.877716	47.346317
2396.947310	202.534769	47.351322
2393.882923	193.941313	47.356327
2390.368632	193.776752	47.361332
2386.875342	196.550686	47.366337
2383.530349	190.360204	47.371341
2379.880693	193.886563	47.376346
2376.795703	200.657539	47.381351
2372.899104	198.955861	47.386356
2369.190789	198.881953	47.391361
2365.732461	200.932993	47.396365
2362.354729	200.631847	47.401370
2359.376186	188.724707	47.406375
2355.497588	193.083961	47.411380
2351.926676	193.816217	47.416385
2348.355655	194.410946	47.421389
2345.010748	198.036606	47.426394
2341.421472	190.707173	47.431399
2337.608445	193.179498	47.436404
2334.439799	188.188587	47.441409
2331.431969	187.408430	47.446413
2327.629249	190.113107	47.451418
2324.314170	186.338709	47.456423
2320.478177	188.274913	47.461428
2317.010350	190.453260	47.466433
2313.387031	184.604200	47.471437
2310.009418	190.808602	47.476442
2306.621206	189.448321	47.481447
2302.868129	195.075331	47.486452
2299.189127	193.313518	47.491457
2296.030312	183.151870	47.496461
2292.316159	185.724336	47.501466
2288.928633	179.682247	47.506471
2285.152861	189.478083	47.511476
2282.117590	188.741956	47.516481
2278.914219	182.268870	47.521485
2275.281849	188.334786	47.526490
2271.635723	188.402243	47.531495
2268.140722	191.202983	47.536500
2264.678448	187.729798	47.541505
2261.420858	179.944284	47.546509
2257.251425	176.579766	47.551514
2253.997143	179.595538	47.556519
2250.404255	180.624347	47.561524
2246.859110	194.784999	47.566529
2243.700121	181.775796	47.571533
2239.892337	190.477762	47.576538
2237.133302	187.059784	47.581543
2233.306202	181.461114	47.586548
2229.480228	189.727007	47.591553
2226.040879	181.849966	47.596557
2222.311075	192.844204	47.601562
2219.101386	191.066144	47.606567
2215.710019	187.674235	47.611572
2211.742283	193.454957	47.616577
2208.545529	186.953397	47.621581
2205.463227	185.137737	47.626586
2202.277310	175.727377	47.631591
2198.105852	179.009075	47.636596
2194.523252	186.137595	47.641601
2191.074584	189.392119	47.646605
2187.502542	194.965835	47.651610
2183.901927	181.851792	47.656615
2180.477595	177.085750	47.661620
2177.088293	185.419689	47.666625
2173.887628	182.428501	47.671629
2170.170273	187.299020	47.676634
2166.776455	188.362709	47.681639
2163.030690	180.848111	47.686644
2159.439306	179.740135	47.691649
2156.221839	173.793605	47.696653
2152.447393	177.667719	47.701658
2148.984124	182.469262	47.706663
2145.959110	180.986174	47.711668
2142.310902	186.292271	47.716673
2138.775335	183.946059	47.721677
2135.074940	185.285359	47.726682
2131.927595	175.984916	47.731687
2127.923891	184.538345	47.736692
2124.312537	184.633916	47.741697
2121.060336	177.412803	47.746701
2117.617542	183.003504	47.751706
2114.122848	180.121887	47.756711
2110.786624	181.054543	47.761716
2107.121115	187.502372	47.766721
2103.822626	181.256669	47.771725
2099.905152	190.889740	47.776730
2096.763679	177.760741	47.781735
2093.343657	178.634032	47.786740
2089.543175	181.563484	47.791745
2086.805627	170.750681	47.796749
2082.783032	176.088841	47.801754
2079.210469	174.115837	47.806759
2075.672046	175.165578	47.811764
2071.663871	176.563249	47.816769
2068.634101	175.703999	47.821773
2064.852680	173.073030	47.826778
2061.541588	168.831656	47.831783
2058.397501	169.419440	47.836788
2054.917085	173.672310	47.841793
2051.524412	167.536732	47.846797
2047.346426	177.498009	47.851802
2044.222376	176.702099	47.856807
2040.573936	177.947048	47.861812
2036.924885	181.761072	47.866817
2033.799344	165.224401	47.871821
2029.966953	181.615379	47.876826
2026.834545	166.044050	47.881831
2022.889201	173.489323	47.886836
2019.388843	175.913408	47.891841
2016.151505	179.102758	47.896845
2012.530452	174.518717	47.901850
2009.063292	179.951497	47.906855
2005.725476	178.761899	47.911860
2002.277573	170.664250	47.916865
1998.384951	172.008165	47.921869
1994.674747	166.650295	47.926874
1991.327864	165.249079	47.931879
1988.276573	173.777334	47.936884
1984.882534	177.501918	47.941889
1981.575992	171.079048	47.946893
1977.648349	177.505133	47.951898
1974.384765	173.009302	47.956903
1970.883831	170.523900	47.961908
1967.254383	178.266928	47.966913
1963.877153	169.266452	47.971917
1959.966605	177.927954	47.976922
1956.720658	172.672622	47.981927
1953.003902	166.006717	47.986932
1949.613881	170.117642	47.991937
1946.344870	162.881880	47.996941
1942.444867	165.236846	48.001946
1939.044948	158.889230	48.006951
1935.331260	163.061317	48.011956
1931.843393	179.925900	48.016961
1928.634451	166.826935	48.021965
1925.008348	176.068034	48.026970
1922.033662	166.001385	48.031975
1918.449203	167.529696	48.036980
1914.479136	173.004158	48.041985
1911.062783	171.257287	48.046989
1907.905657	179.462067	48.051994
1904.327100	171.535068	48.056999
1900.548341	161.398381	48.062004
1896.861966	162.549453	48.067009
1893.447519	159.239157	48.072013
1889.914774	170.393257	48.077018
1886.769191	174.355511	48.082023
1883.638586	166.930379	48.087028
1879.563881	172.763549	48.092033
1876.267745	170.416077	48.097037
1872.557924	167.330412	48.102042
1869.435567	165.682623	48.107047
1865.749616	164.945308	48.112052
1861.730782	169.157985	48.117057
1858.478593	166.181846	48.122061
1854.699284	177.786772	48.127066
1851.527867	168.805475	48.132071
1848.177254	177.688535	48.137076
1844.575553	172.527373	48.142081
1841.527115	167.383955	48.147085
1837.559134	178.001589	48.152090
1834.054655	170.456105	48.157095
1830.715486	167.204265	48.162100
1827.104661	170.877341	48.167105
1823.673465	163.234119	48.172109
1819.666574	173.388720	48.177114
1816.349762	162.193247	48.182119
1813.061410	164.854784	48.187124
1809.582053	162.632942	48.192129
1806.222811	164.205041	48.197133
1802.594399	169.967508	48.202138
1798.870147	162.902770	48.207143
1795.459277	162.560728	48.212148
1791.661835	169.155282	48.217153
1788.777983	158.188270	48.222157
1785.144581	168.663441	48.227162
1781.466797	165.662151	48.232167
1778.504115	167.122384	48.237172
1774.479571	160.047679	48.242177
1771.023865	165.870242	48.247181
1767.568759	161.599992	48.252186
1763.874396	159.808382	48.257191
1760.731172	161.465992	48.262196
1757.187133	162.299030	48.267201
1753.644597	157.267298	48.272205
1750.416357	156.506558	48.277210
1746.457848	165.073910	48.282215
1743.158235	169.619181	48.287220
1739.081173	164.347391	48.292225
1736.019085	155.132043	48.297229
1732.569190	167.156631	48.302234
1728.780819	158.894438	48.307239
1725.378785	162.511582	48.312244
1721.791809	164.371391	48.317249
1718.215109	155.281134	48.322253
1715.177896	159.735511	48.327258
1711.594335	160.672598	48.332263
1708.417221	155.780831	48.337268
1704.677964	163.555393	48.342273
1701.122904	159.801371	48.347277
1697.062447	162.940034	48.352282
1693.742100	164.974859	48.357287
1690.639425	157.702935	48.362292
1686.959224	158.590489	48.367297
1683.575579	159.747951	48.372301
1680.026522	167.323568	48.377306
1676.672127	161.745363	48.382311
1673.060370	157.826679	48.387316
1669.254338	162.043029	48.392321
1665.834596	158.861064	48.397325
1662.360323	166.069324	48.402330
1658.891186	158.294961	48.407335
1655.909513	157.321864	48.412340
1652.099277	170.283802	48.417345
1648.469167	157.267290	48.422349
1644.945096	154.291827	48.427354
1641.337566	159.439402	48.432359
1637.981434	165.858537	48.437364
1634.420711	169.065450	48.442369
1631.100360	174.246496	48.447373
1627.685436	164.326214	48.452378
1623.740902	167.578199	48.457383
1620.204063	156.913975	48.462388
1616.777175	159.182148	48.467393
1613.775776	160.635263	48.472397
1609.948369	166.738002	48.477402
1606.384174	166.440179	48.482407
1602.809539	156.385678	48.487412
1599.167462	164.121762	48.492417
1595.902216	146.953792	48.497421
1592.330219	154.581996	48.502426
1588.910413	154.050163	48.507431
1585.338391	155.877014	48.512436
1581.856947	161.863208	48.517441
1578.589640	148.129287	48.522445
1575.066548	156.949242	48.527450
1571.499054	148.215763	48.532455
1567.686271	147.455439	48.537460
1564.167257	151.665093	48.542465
1560.788079	152.775529	48.547469
1557.225873	151.731870	48.552474
1553.835044	154.468136	48.557479
1550.317439	150.823294	48.562484
1546.865779	154.131834	48.567489
1544.077678	143.079726	48.572493
1540.263282	158.774569	48.577498
1536.386181	148.814712	48.582503
1532.816266	142.808099	48.587508
1528.907382	149.972225	48.592513
1525.740269	144.012525	48.597517
1522.464772	151.879696	48.602522
1518.978470	156.775650	48.607527
1515.541349	160.516942	48.612532
1511.670796	158.160268	48.617537
1508.349040	144.265697	48.622541
1504.945646	147.619373	48.627546
1501.436407	149.419927	48.632551
1498.179857	146.206981	48.637556
1494.435372	154.340131	48.642561
1490.689775	152.950900	48.647565
1487.169676	161.431196	48.652570
1483.808190	155.435563	48.657575
1480.495316	154.443508	48.662580
1476.500231	156.018496	48.667585
1473.418138	151.590732	48.672589
1469.831543	153.402712	48.677594
1466.182493	151.935977	48.682599
1462.766277	143.004924	48.687604
1459.256183	159.384419	48.692609
1455.729930	157.770509	48.697613
1452.062997	159.016394	48.702618
1449.026782	149.676811	48.707623
1445.476003	150.361416	48.712628
1442.004488	162.206818	48.717633
1438.742178	151.661572	48.722637
1434.675411	152.155977	48.727642
1431.483310	144.710178	48.732647
1427.549771	153.153459	48.737652
1423.708907	145.965061	48.742657
1420.473881	152.580206	48.747661
1417.389291	149.398495	48.752666
1413.670385	143.779313	48.757671
1410.872818	137.019595	48.762676
1406.890889	147.211607	48.767681
1403.687240	149.109138	48.772685
1399.577271	152.990921	48.777690
1395.781706	151.002028	48.782695
1392.426404	150.298060	48.787700
1389.302200	150.684279	48.792705
1386.221669	143.288158	48.797709
1382.227405	138.445457	48.802714
1378.828964	141.636585	48.807719
1375.380320	155.036622	48.812724
1371.327604	148.524832	48.817729
1367.969123	143.987917	48.822733
1364.492130	145.573472	48.827738
1361.219015	141.612495	48.832743
1357.907749	136.925505	48.837748
1354.236547	144.311161	48.842753
1350.791826	134.522748	48.847757
1347.208727	145.279574	48.852762
1343.578281	134.160233	48.857767
1340.329293	139.228036	48.862772
1336.603821	147.020114	48.867777
1333.655215	142.952238	48.872781
1329.725208	144.365235	48.877786
1325.917603	144.092866	48.882791
1322.729840	145.115394	48.887796
1319.206037	152.372520	48.892801
1315.625216	143.643048	48.897805
1312.079602	153.326503	48.902810
1308.626519	146.968052	48.907815
1305.362921	145.827871	48.912820
1301.820555	146.146910	48.917825
1298.264017	144.458998	48.922829
1294.145159	146.782580	48.927834
1290.953261	138.103103	48.932839
1287.956982	142.768829	48.937844
1284.396508	152.933895	48.942849
1280.992929	138.702383	48.947853
1276.940401	142.379014	48.952858
1273.568386	149.434067	48.957863
1270.267426	140.597003	48.962868
1266.295054	153.654864	48.967873
1263.301817	137.112002	48.972877
1259.857540	140.567527	48.977882
1256.210594	149.968801	48.982887
1252.288995	137.429674	48.987892
1248.764913	145.031048	48.992897
1245.547999	146.912724	48.997901
1242.173338	153.157771	49.002906
1238.591706	150.084400	49.007911
1235.378550	148.077708	49.012916
1231.789912	152.043755	49.017921
1228.426328	136.747357	49.022925
1224.631194	140.873840	49.027930
1221.220557	142.360321	49.032935
1217.774293	147.557317	49.037940
1213.743752	155.731252	49.042945
1210.800083	137.110954	49.047949
1207.028094	142.377591	49.052954
1203.495943	151.808273	49.057959
1200.016114	142.086569	49.062964
1196.435959	142.157765	49.067969
1193.123970	147.284430	49.072973
1189.355386	145.784992	49.077978
1185.781214	139.770694	49.082983
1182.737083	143.020801	49.087988
1179.286563	144.206257	49.092993
1175.773268	133.137758	49.097997
1172.072358	141.226635	49.103002
1168.403399	149.607625	49.108007
1164.907061	141.484354	49.113012
1161.486253	145.228131	49.118017
1158.171967	138.810946	49.123021
1154.162092	138.700628	49.128026
1151.001761	143.410729	49.133031
1147.794864	132.620757	49.138036
1143.736423	141.625211	49.143041
1140.208462	135.663698	49.148045
1137.128154	136.357782	49.153050
1133.757452	138.175567	49.158055
1129.995115	136.190289	49.163060
1126.676428	145.853317	49.168065
1123.083172	138.813310	49.173069
1119.613174	140.943331	49.178074
1115.961497	142.062043	49.183079
1112.468318	134.091630	49.188084
1108.848617	131.933206	49.193089
1105.492244	132.552975	49.198093
1102.220414	144.198615	49.203098
1098.336437	138.569510	49.208103
1095.450886	131.035011	49.213108
1091.494616	140.451427	49.218113
1087.819396	139.763680	49.223117
1083.618985	140.661946	49.228122
1080.721023	141.521282	49.233127
1077.968766	135.946219	49.238132
1073.885347	140.505493	49.243137
1070.434477	128.452909	49.248141
1067.008770	142.770897	49.253146
1063.281277	134.506954	49.258151
1060.028662	137.266497	49.263156
1056.359805	137.972899	49.268161
1053.067637	134.292765	49.273165
1049.582169	143.845282	49.278170
1046.059727	135.007928	49.283175
1042.703934	128.506336	49.288180
1038.429565	138.104449	49.293185
1035.360212	134.516544	49.298189
1032.041683	138.413802	49.303194
1028.359418	130.573201	49.308199
1025.034512	136.936852	49.313204
1021.470610	136.924393	49.318209
1018.151127	133.256499	49.323213
1014.250913	134.847572	49.328218
1010.857564	129.584193	49.333223
1007.493440	138.644836	49.338228
1003.856149	141.710950	49.343233
1000.390978	128.402572	49.348237
996.669115	135.350682	49.353242
993.422108	135.480614	49.358247
989.943898	128.256138	49.363252
986.378096	139.906845	49.368257
982.958859	124.054515	49.373261
979.306501	128.213820	49.378266
975.589790	137.106444	49.383271
972.760520	132.097128	49.388276
968.901486	133.550792	49.393281
965.505962	128.885149	49.398285
961.912256	136.797791	49.403290
958.084189	130.095532	49.408295
954.904880	127.465195	49.413300
951.129590	136.792390	49.418305
948.019170	123.328702	49.423309
944.518673	133.634833	49.428314
940.491358	131.511595	49.433319
937.071826	139.386966	49.438324
933.584312	139.507777	49.443329
930.468127	140.228457	49.448333
926.736504	133.345104	49.453338
923.386675	126.782437	49.458343
920.288967	137.373036	49.463348
916.396952	138.484491	49.468353
913.000447	135.308551	49.473357
909.760645	141.872712	49.478362
905.512267	143.372666	49.483367
902.276150	134.922424	49.488372
898.631526	138.643216	49.493377
895.180309	131.181103	49.498381
891.309315	146.899739	49.503386
888.202779	139.191573	49.508391
885.023861	141.894649	49.513396
881.210498	144.030922	49.518401
877.626655	135.180980	49.523405
874.360458	134.857338	49.528410
870.822964	135.172158	49.533415
867.575910	140.726390	49.538420
863.693177	145.758035	49.543425
860.706124	135.456066	49.548429
856.596619	135.502009	49.553434
853.106604	135.560148	49.558439
849.872521	135.445718	49.563444
846.313144	136.420913	49.568449
842.853399	127.699077	49.573453
839.589716	135.945580	49.578458
835.637133	136.789470	49.583463
832.153418	136.925321	49.588468
828.253556	138.263903	49.593473
825.078225	132.835951	49.598477
821.624627	134.220115	49.603482
818.093035	136.832777	49.608487
815.094244	130.561421	49.613492
811.208566	135.065716	49.618497
808.063539	126.574836	49.623501
804.331015	141.528244	49.628506
800.343159	131.676227	49.633511
797.058741	133.523400	49.638516
793.685107	141.087379	49.643521
790.509057	138.660867	49.648525
786.532159	139.650707	49.653530
783.082064	133.666161	49.658535
779.690193	130.421875	49.663540
776.267553	142.915354	49.668545
772.730078	133.672637	49.673549
769.344368	132.312103	49.678554
765.473500	135.172343	49.683559
762.213196	132.931670	49.688564
758.645369	136.882986	49.693569
755.409913	129.286832	49.698573
751.604567	128.353894	49.703578
748.270741	125.554696	49.708583
744.884144	130.107520	49.713588
740.933620	133.790234	49.718593
737.468667	126.483072	49.723597
733.950086	133.291587	49.728602
730.338069	136.706375	49.733607
727.031794	120.860664	49.738612
723.440942	128.208818	49.743617
720.476715	126.422210	49.748621
716.804926	130.959676	49.753626
713.279490	128.245089	49.758631
709.798332	122.093474	49.763636
706.037617	136.872624	49.768641
702.699977	133.307242	49.773645
698.959933	131.758513	49.778650
695.495122	133.840239	49.783655
692.259186	124.572778	49.788660
688.718016	138.746110	49.793665
684.850033	128.546210	49.798669
681.559500	130.427235	49.803674
677.704268	131.950573	49.808679
674.889028	126.190252	49.813684
671.069501	131.269414	49.818689
668.040875	123.649379	49.823693
664.446256	133.245467	49.828698
660.542648	131.639371	49.833703
657.134893	128.953906	49.838708
653.402028	129.397127	49.843713
649.787465	127.800449	49.848717
646.294617	131.496327	49.853722
643.055219	128.537929	49.858727
639.489111	129.235369	49.863732
636.024431	140.927602	49.868737
632.688211	128.579188	49.873741
629.122657	129.081182	49.878746
625.321051	134.988006	49.883751
622.539832	118.576985	49.888756
618.553984	128.813264	49.893761
615.168736	124.063525	49.898765
611.335843	129.885352	49.903770
607.969417	126.177597	49.908775
604.614854	128.326402	49.913780
600.899047	132.049337	49.918785
597.695609	128.483148	49.923789
594.234065	131.228646	49.928794
590.008056	134.315530	49.933799
586.942993	123.270499	49.938804
583.428101	127.639633	49.943809
579.921740	126.406563	49.948813
576.468763	126.168314	49.953818
573.047823	126.393046	49.958823
570.005844	128.284927	49.963828
566.007172	124.178610	49.968833
562.480384	118.676213	49.973837
558.983686	122.360952	49.978842
555.092403	127.467867	49.983847
551.961440	119.255878	49.988852
548.151809	137.310723	49.993857
545.099023	124.976470	49.998861
541.401627	125.333798	50.003866
537.727091	126.280737	50.008871
534.793216	117.918341	50.013876
531.092746	119.259906	50.018881
527.593028	117.418183	50.023885
523.979843	120.741562	50.028890
520.136851	124.234200	50.033895
517.011204	122.227775	50.038900
513.595086	125.097834	50.043905
509.990224	119.939333	50.048909
506.520532	118.446087	50.053914
502.783721	114.379779	50.058919
499.449133	119.952094	50.063924
495.714290	133.329179	50.068929
492.598163	124.617887	50.073933
489.181391	122.637160	50.078938
485.388777	125.645319	50.083943
481.965392	116.432344	50.088948
478.207702	122.050417	50.093953
474.629957	125.796389	50.098957
471.754614	126.035897	50.103962
468.118157	122.960016	50.108967
464.567570	109.428695	50.113972
461.141141	112.182886	50.118977
457.445547	109.480494	50.123981
453.645817	111.828189	50.128986
449.654991	124.417075	50.133991
446.729563	111.931992	50.138996
443.091237	125.462845	50.144001
439.978197	114.154743	50.149005
436.384827	109.289624	50.154010
432.909737	122.057602	50.159015
429.365636	114.696126	50.164020
425.641216	125.621608	50.169025
422.561494	121.978250	50.174029
419.231355	117.704804	50.179034
415.152418	115.223166	50.184039
411.903886	111.662418	50.189044
408.362879	119.809063	50.194049
405.091568	115.236402	50.199053
401.192669	120.140858	50.204058
397.729047	119.004860	50.209063
394.453622	118.728689	50.214068
390.795974	124.441771	50.219073
387.065667	121.842667	50.224077
383.759168	113.380047	50.229082
380.077102	121.839748	50.234087
377.394878	117.250719	50.239092
373.209653	125.971501	50.244097
369.572104	118.248829	50.249101
366.100248	117.101196	50.254106
362.674853	117.886080	50.259111
359.401801	115.664999	50.264116
355.826140	122.545000	50.269121
352.495046	118.150208	50.274125
348.299594	118.942771	50.279130
345.005320	120.948590	50.284135
341.684485	113.976880	50.289140
338.260573	126.220817	50.294145
334.941527	117.055824	50.299149
331.171022	124.201147	50.304154
327.605276	115.824896	50.309159
324.685170	115.552129	50.314164
320.939939	117.084407	50.319169
317.221765	117.127457	50.324173
313.330573	121.211572	50.329178
310.134442	125.375219	50.334183
307.106949	114.886417	50.339188
303.174702	122.131547	50.344193
299.986445	116.891253	50.349197
296.459665	102.962673	50.354202
292.688757	115.198552	50.359207
289.314413	114.321175	50.364212
285.645063	124.981109	50.369217
282.210159	117.152357	50.374221
278.730921	110.016296	50.379226
275.103070	116.241553	50.384231
271.467016	114.365382	50.389236
267.866660	127.500534	50.394241
264.597696	120.381968	50.399245
261.206891	110.073326	50.404250
257.668679	113.717412	50.409255
254.403031	111.953006	50.414260
250.602134	114.371122	50.419265
247.208468	114.740388	50.424269
243.511426	113.831808	50.429274
240.198304	112.074285	50.434279
236.943726	114.204249	50.439284
233.078737	114.147551	50.444289
229.597377	109.819573	50.449293
226.307503	103.487930	50.454298
222.249573	114.837189	50.459303
219.266875	115.477073	50.464308
215.630753	114.060359	50.469313
212.288370	111.376674	50.474317
208.981601	110.350238	50.479322
205.207809	111.146350	50.484327
202.157010	104.227150	50.489332
198.243302	111.984339	50.494337
194.610048	112.498488	50.499341
190.831423	111.498873	50.504346
187.286281	118.887414	50.509351
184.100536	108.954169	50.514356
180.493457	113.296640	50.519361
177.027452	112.600881	50.524365
173.790112	102.749993	50.529370
169.808611	111.035052	50.534375
166.778241	106.752644	50.539380
163.147555	109.508713	50.544385
159.186282	118.230099	50.549389
155.985462	111.300051	50.554394
152.379429	116.237732	50.559399
149.333190	111.038381	50.564404
145.551221	116.624433	50.569409
142.154743	119.774699	50.574413
138.767889	117.240912	50.579418
135.116842	118.805709	50.584423
131.849471	109.605506	50.589428
127.817544	127.168576	50.594433
124.379553	117.632736	50.599437
120.881648	119.504109	50.604442
117.418601	117.120890	50.609447
114.088596	105.314609	50.614452
110.560644	116.094128	50.619457
107.373541	122.385273	50.624461
103.715952	120.650553	50.629466
100.065966	131.498838	50.634471
96.519023	114.090420	50.639476
93.045971	122.662751	50.644481
89.615868	122.704678	50.649485
86.050624	115.291168	50.654490
82.578400	121.972111	50.659495
78.626233	123.087161	50.664500
75.345452	120.343855	50.669505
71.983439	121.514724	50.674509
68.731629	120.792074	50.679514
64.971599	122.862788	50.684519
61.451645	112.673588	50.689524
57.875541	120.532867	50.694529
54.394911	120.360200	50.699533
51.032681	114.495340	50.704538
47.220763	117.454380	50.709543
43.901666	124.134862	50.714548
40.422372	122.371465	50.719553
37.015705	122.239451	50.724557
33.546851	126.609674	50.729562
29.932247	125.923248	50.734567
26.578216	110.927351	50.739572
22.988506	114.303093	50.744577
19.325063	124.989085	50.749581
16.012549	111.013649	50.754586
12.406800	120.490493	50.759591
8.849358	116.019802	50.764596
5.231132	120.661053	50.769601
2.287922	116.124573	50.774605