Tue Jun 21 12:45:44 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.257586	126.257148	0.000000
0.132886	118.338679	0.005005
-0.288754	107.490416	0.010010
-0.120912	95.741394	0.015014
-0.320625	98.575506	0.020019
0.034296	91.948316	0.025024
-0.346581	87.408426	0.030029
-0.394138	75.096177	0.035034
-0.867473	58.208996	0.040038
-1.046937	52.093991	0.045043
-1.162124	43.823519	0.050048
-1.314613	30.394998	0.055053
-1.615191	16.683170	0.060058
-1.854192	3.948417	0.065062
-2.270180	-3.950762	0.070067
-2.397347	-18.355894	0.075072
-2.940399	-20.040319	0.080077
-3.527196	-24.788401	0.085082
-3.895608	-34.460983	0.090086
-4.292684	-35.534561	0.095091
-5.303123	-35.925226	0.100096
-5.273102	-35.394763	0.105101
-5.532253	-24.942057	0.110106
-5.402904	-35.579342	0.115110
-5.661799	-36.058544	0.120115
-5.655834	-27.201174	0.125120
-5.732823	-32.626070	0.130125
-5.862776	-17.878682	0.135130
-6.406352	-32.812765	0.140134
-6.839637	-23.755376	0.145139
-7.273849	-21.278502	0.150144
-7.372720	-32.852823	0.155149
-7.485241	-30.137562	0.160154
-7.607217	-42.494422	0.165158
-8.427407	-24.655379	0.170163
-8.738891	-32.686893	0.175168
-8.905678	-32.749780	0.180173
-8.945781	-26.633830	0.185178
-8.967912	-33.046977	0.190182
-8.984191	-24.040488	0.195187
-9.275212	-36.552682	0.200192
-9.767591	-32.535464	0.205197
-10.458993	-35.335709	0.210202
-10.232828	-35.128595	0.215206
-10.508712	-25.833241	0.220211
-10.544894	-30.770180	0.225216
-11.379490	-30.386816	0.230221
-12.101842	-30.063480	0.235226
-11.441280	-33.591396	0.240230
-12.222779	-27.372211	0.245235
-11.978949	-28.689264	0.250240
-11.825635	-29.627446	0.255245
-12.540774	-31.281793	0.260250
-12.507275	-33.467013	0.265254
-13.204378	-27.932341	0.270259
-13.979375	-33.151664	0.275264
-13.922412	-36.696053	0.280269
-14.064872	-24.081745	0.285274
-13.701420	-34.729577	0.290278
-14.208775	-30.049996	0.295283
-14.197673	-36.328143	0.300288
-15.017685	-34.687814	0.305293
-15.783141	-20.477315	0.310298
-15.541536	-32.809931	0.315302
-15.483419	-31.712840	0.320307
-15.637313	-31.488769	0.325312
-15.362503	-33.417555	0.330317
-16.302911	-30.213748	0.335322
-16.580779	-32.917107	0.340326
-16.932328	-27.832942	0.345331
-17.293166	-28.165812	0.350336
-17.122026	-31.196309	0.355341
-17.536691	-26.024141	0.360346
-18.274789	-33.436814	0.365350
-18.390655	-30.433879	0.370355
-18.620239	-25.126599	0.375360
-18.614652	-27.521896	0.380365
-18.872809	-18.864097	0.385370
-18.623727	-38.696611	0.390374
-19.075296	-27.450733	0.395379
-20.062243	-28.792287	0.400384
-19.850384	-31.532739	0.405389
-20.394323	-26.355541	0.410394
-20.146347	-25.664232	0.415398
-20.142726	-31.789195	0.420403
-20.786628	-36.837626	0.425408
-21.321524	-32.576370	0.430413
-21.785563	-29.266349	0.435418
-21.432620	-32.005892	0.440422
-21.716382	-27.363139	0.445427
-21.936729	-24.221344	0.450432
-22.334070	-36.333103	0.455437
-23.178349	-30.456944	0.460442
-22.747543	-34.865006	0.465446
-23.224880	-30.253542	0.470451
-23.518074	-39.114115	0.475456
-23.556094	-30.397268	0.480461
-23.762472	-26.689665	0.485466
-23.660933	-30.038578	0.490470
-24.388827	-27.947992	0.495475
-24.382908	-28.927873	0.500480
-24.436789	-26.215218	0.505485
-25.008564	-26.449022	0.510490
-25.541156	-37.481662	0.515494
-25.892834	-26.741711	0.520499
-26.268186	-31.575714	0.525504
-26.614111	-36.261853	0.530509
-26.543112	-27.848402	0.535514
-26.161821	-37.128313	0.540518
-26.631004	-27.282951	0.545523
-27.002686	-25.531763	0.550528
-27.619006	-33.029721	0.555533
-28.041262	-29.736880	0.560538
-27.683667	-31.875920	0.565542
-27.671314	-30.142745	0.570547
-27.970664	-23.913614	0.575552
-28.578260	-30.246185	0.580557
-29.440233	-26.908943	0.585562
-29.573448	-30.838409	0.590566
-29.419643	-25.196401	0.595571
-29.657303	-29.677878	0.600576
-29.419258	-36.964879	0.605581
-30.278471	-24.702913	0.610586
-30.779369	-31.010529	0.615590
-31.281851	-25.650164	0.620595
-31.248073	-32.736397	0.625600
-31.422131	-20.790945	0.630605
-31.558146	-26.865159	0.635610
-31.168378	-31.752458	0.640614
-31.399127	-27.529529	0.645619
-31.741784	-25.966273	0.650624
-32.246272	-28.745174	0.655629
-32.746083	-16.561071	0.660634
-32.962209	-28.101568	0.665638
-33.114717	-27.397417	0.670643
-32.992595	-30.308699	0.675648
-33.592961	-22.006658	0.680653
-34.394555	-20.653139	0.685658
-34.152710	-20.287402	0.690662
-34.212514	-21.375391	0.695667
-34.531578	-27.114609	0.700672
-34.335366	-26.624099	0.705677
-35.360569	-22.905018	0.710682
-35.869296	-36.497074	0.715686
-35.940086	-22.535800	0.720691
-36.237114	-26.512929	0.725696
-36.020544	-30.670027	0.730701
-36.060464	-30.572376	0.735706
-36.271416	-33.970179	0.740710
-37.098171	-27.701464	0.745715
-37.308220	-25.116867	0.750720
-37.190498	-33.506770	0.755725
-37.661868	-36.277735	0.760730
-37.437013	-36.696150	0.765734
-38.208932	-38.421995	0.770739
-38.729614	-31.651435	0.775744
-38.869516	-37.898061	0.780749
-39.049539	-32.239845	0.785754
-39.106502	-28.683476	0.790758
-38.975440	-30.769018	0.795763
-39.909699	-30.292184	0.800768
-40.224807	-32.423817	0.805773
-40.474631	-33.467708	0.810778
-40.604111	-34.096606	0.815782
-40.682992	-32.474813	0.820787
-40.747634	-28.145995	0.825792
-40.624490	-33.573641	0.830797
-41.576151	-37.387103	0.835802
-42.239825	-35.994856	0.840806
-42.358139	-27.662339	0.845811
-42.563263	-31.570424	0.850816
-42.160331	-26.727235	0.855821
-42.633874	-31.935300	0.860826
-42.532794	-33.647455	0.865830
-42.562770	-28.166822	0.870835
-43.282198	-29.514192	0.875840
-43.495644	-34.551025	0.880845
-44.437658	-28.675056	0.885850
-44.327951	-31.957833	0.890854
-44.133464	-30.786239	0.895859
-44.504739	-31.831329	0.900864
-45.393543	-28.932456	0.905869
-45.845536	-33.232607	0.910874
-45.778028	-32.322368	0.915878
-45.564997	-36.887161	0.920883
-45.871407	-33.652577	0.925888
-45.720673	-38.076417	0.930893
-46.123064	-29.029673	0.935898
-46.411329	-33.158223	0.940902
-46.764905	-27.465739	0.945907
-47.229078	-37.905667	0.950912
-47.157253	-34.911123	0.955917
-47.769666	-31.922059	0.960922
-48.088312	-39.534031	0.965926
-48.603458	-34.715420	0.970931
-48.959660	-41.970312	0.975936
-48.895022	-43.742538	0.980941
-49.226812	-34.311047	0.985946
-48.584555	-36.522685	0.990950
-48.770679	-31.508145	0.995955
-49.565656	-21.859242	1.000960
-49.748777	-30.019751	1.005965
-50.341639	-25.650422	1.010970
-50.379929	-31.530458	1.015974
-50.290386	-26.312535	1.020979
-51.159906	-29.583712	1.025984
-51.528241	-31.545506	1.030989
-51.987711	-28.644127	1.035994
-51.930626	-39.100718	1.040998
-52.175783	-34.729772	1.046003
-51.968552	-37.865702	1.051008
-51.585479	-42.262898	1.056013
-52.634507	-30.401265	1.061018
-53.247860	-39.694844	1.066022
-53.253906	-38.521220	1.071027
-53.418755	-24.842742	1.076032
-53.353728	-30.082177	1.081037
-53.880890	-23.007436	1.086042
-54.332396	-20.980968	1.091046
-54.912122	-32.017639	1.096051
-54.936910	-27.046787	1.101056
-55.105685	-34.890977	1.106061
-55.110385	-35.118246	1.111066
-54.885470	-35.982249	1.116070
-55.465910	-36.348997	1.121075
-56.346015	-33.126359	1.126080
-56.374694	-44.940602	1.131085
-56.593758	-36.327373	1.136090
-56.363278	-44.668060	1.141094
-56.805572	-34.546153	1.146099
-57.118267	-34.855024	1.151104
-57.574393	-32.524688	1.156109
-58.059054	-31.364549	1.161114
-58.199318	-33.523359	1.166118
-58.509203	-29.780460	1.171123
-58.457709	-26.338154	1.176128
-58.058168	-33.027539	1.181133
-58.983768	-30.814420	1.186138
-59.576936	-39.030153	1.191142
-59.434487	-38.587179	1.196147
-60.005406	-23.965491	1.201152
-59.772896	-33.471772	1.206157
-59.767239	-27.667691	1.211162
-60.066032	-33.696985	1.216166
-61.109666	-29.290497	1.221171
-61.574179	-35.639849	1.226176
-61.161292	-33.170454	1.231181
-61.693380	-35.526433	1.236186
-61.426953	-33.172692	1.241190
-61.721659	-32.931416	1.246195
-61.711002	-32.786888	1.251200
-62.516175	-38.905576	1.256205
-62.940657	-29.552268	1.261210
-63.151294	-32.415940	1.266214
-63.220308	-23.047497	1.271219
-63.583622	-28.423787	1.276224
-63.508951	-35.502580	1.281229
-64.110210	-24.407537	1.286234
-64.598696	-36.908330	1.291238
-64.790069	-32.220494	1.296243
-65.227307	-31.324345	1.301248
-65.301755	-33.208120	1.306253
-64.993519	-28.402532	1.311258
-65.171368	-33.343237	1.316262
-65.178528	-35.911849	1.321267
-65.923445	-34.592182	1.326272
-66.309537	-37.711745	1.331277
-66.872645	-28.821509	1.336282
-66.837515	-33.493001	1.341286
-66.679292	-39.069717	1.346291
-67.223363	-30.270251	1.351296
-67.616030	-35.242867	1.356301
-68.268730	-31.476149	1.361306
-68.369117	-30.153109	1.366310
-68.221493	-29.894906	1.371315
-68.525648	-25.542209	1.376320
-68.101410	-33.269513	1.381325
-68.594150	-33.237371	1.386330
-69.072860	-33.059356	1.391334
-70.000133	-32.692798	1.396339
-70.422032	-29.779287	1.401344
-69.807254	-37.115852	1.406349
-70.051499	-30.574394	1.411354
-70.053874	-29.531617	1.416358
-70.786885	-31.523590	1.421363
-71.257124	-24.684617	1.426368
-71.759097	-28.538211	1.431373
-71.816019	-24.069775	1.436378
-71.363609	-34.245716	1.441382
-71.636398	-37.478565	1.446387
-71.854448	-27.816478	1.451392
-72.388290	-39.921205	1.456397
-73.006443	-23.624231	1.461402
-73.151567	-34.374317	1.466406
-72.980675	-26.890868	1.471411
-73.173198	-27.474199	1.476416
-73.735382	-33.046063	1.481421
-74.260337	-32.094341	1.486426
-74.309038	-31.456714	1.491430
-74.632858	-30.511662	1.496435
-74.860541	-32.762357	1.501440
-74.370109	-32.519290	1.506445
-75.188535	-26.131181	1.511450
-75.882957	-30.018811	1.516454
-75.780813	-29.858847	1.521459
-75.866129	-21.017543	1.526464
-76.001256	-31.257206	1.531469
-76.029958	-24.186082	1.536474
-76.662513	-24.698511	1.541478
-77.279898	-25.833079	1.546483
-77.704908	-15.624039	1.551488
-77.395012	-19.438436	1.556493
-77.567950	-22.216790	1.561498
-77.930519	-18.452533	1.566502
-78.800398	-16.491554	1.571507
-79.216816	-13.226511	1.576512
-78.443176	-30.366262	1.581517
-78.866446	-11.290146	1.586522
-78.942438	-17.851846	1.591526
-78.986060	-20.435142	1.596531
-80.011066	-21.075963	1.601536
-80.279244	-18.816612	1.606541
-80.653937	-14.880245	1.611546
-81.082028	-24.266866	1.616550
-81.076720	-26.879181	1.621555
-81.328669	-21.097359	1.626560
-80.998374	-23.567349	1.631565
-81.330469	-15.495421	1.636570
-81.145276	-18.195151	1.641574
-81.598375	-19.715087	1.646579
-82.484911	-22.512603	1.651584
-82.267043	-34.474242	1.656589
-82.612908	-18.950911	1.661594
-83.177932	-28.477453	1.666598
-83.456956	-27.982832	1.671603
-83.968898	-16.678010	1.676608
-83.927090	-23.806618	1.681613
-84.208674	-17.514320	1.686618
-84.258281	-28.276477	1.691622
-84.129752	-29.131228	1.696627
-84.527268	-26.696538	1.701632
-84.862587	-25.868573	1.706637
-85.523767	-28.955798	1.711642
-85.890499	-26.843321	1.716646
-85.585657	-30.368575	1.721651
-85.731533	-24.948273	1.726656
-85.867807	-28.965832	1.731661
-86.763693	-23.631082	1.736666
-87.240088	-32.631212	1.741670
-87.382856	-32.876265	1.746675
-87.867192	-28.882868	1.751680
-87.457507	-22.619611	1.756685
-87.747898	-25.653199	1.761690
-87.726839	-24.343168	1.766694
-87.673923	-30.735587	1.771699
-88.396112	-29.844340	1.776704
-88.741779	-33.447550	1.781709
-88.969734	-25.674272	1.786714
-89.097815	-23.256577	1.791718
-89.175608	-30.276180	1.796723
-89.927080	-30.361617	1.801728
-90.145141	-29.592538	1.806733
-90.369481	-27.932447	1.811738
-90.304745	-36.904188	1.816742
-90.546584	-25.339226	1.821747
-91.159299	-27.402424	1.826752
-91.785246	-36.564657	1.831757
-91.892581	-22.139131	1.836762
-92.100090	-29.367341	1.841766
-91.729206	-30.125676	1.846771
-92.439467	-21.409384	1.851776
-92.290967	-41.036575	1.856781
-92.699725	-26.329859	1.861786
-93.305917	-26.448434	1.866790
-93.734741	-35.952336	1.871795
-94.039674	-30.989752	1.876800
-93.622622	-30.799260	1.881805
-93.825718	-28.423014	1.886810
-93.953108	-28.962666	1.891814
-94.399695	-29.436431	1.896819
-95.362407	-29.778936	1.901824
-95.006855	-24.246122	1.906829
-95.231005	-27.655154	1.911834
-95.674688	-25.178481	1.916838
-95.157543	-34.519569	1.921843
-96.089218	-25.669128	1.926848
-96.523375	-36.981887	1.931853
-97.209649	-34.875885	1.936858
-96.987538	-28.701742	1.941862
-96.880756	-30.157915	1.946867
-97.084637	-31.057070	1.951872
-97.231855	-30.935530	1.956877
-98.144277	-29.838531	1.961882
-98.566115	-26.912991	1.966886
-98.551157	-34.884889	1.971891
-98.754694	-27.677661	1.976896
-98.711281	-37.563270	1.981901
-98.995851	-33.737934	1.986906
-99.019991	-24.948403	1.991910
-98.709532	-32.867616	1.996915
-99.845973	-27.126605	2.006912
-99.749619	-33.050235	2.016909
-99.072045	-35.377051	2.026906
-99.021091	-30.076224	2.036902
-98.181647	-31.411295	2.046899
-97.336704	-31.797877	2.056896
-96.714105	-27.886304	2.066893
-96.305636	-34.043009	2.076890
-96.185043	-25.522596	2.086886
-96.073035	-26.060064	2.096883
-94.833956	-32.289327	2.106880
-94.654508	-32.671005	2.116877
-93.963610	-25.091500	2.126874
-93.089314	-29.944625	2.136870
-92.952338	-30.892663	2.146867
-92.759933	-31.393457	2.156864
-92.270342	-31.886565	2.166861
-91.463380	-29.048185	2.176858
-91.049654	-30.040278	2.186854
-90.205162	-32.887318	2.196851
-89.981638	-31.921451	2.206848
-89.628619	-26.637652	2.216845
-89.224874	-27.531670	2.226842
-88.486553	-31.326333	2.236838
-88.089447	-28.873533	2.246835
-87.145062	-21.861781	2.256832
-87.045374	-23.232799	2.266829
-86.822747	-23.141890	2.276826
-85.666505	-28.807947	2.286822
-85.362901	-25.075902	2.296819
-85.207691	-28.056363	2.306816
-84.663857	-31.384522	2.316813
-84.036782	-26.508482	2.326810
-83.748039	-26.161979	2.336806
-82.528452	-34.064525	2.346803
-82.327535	-29.214132	2.356800
-82.240664	-30.990449	2.366797
-81.640037	-31.443657	2.376794
-81.108675	-28.011331	2.386790
-80.512546	-26.120427	2.396787
-79.393805	-30.233373	2.406784
-79.611855	-26.728504	2.416781
-79.145360	-26.710583	2.426778
-78.661109	-26.407918	2.436774
-77.562680	-32.669602	2.446771
-77.474647	-33.004724	2.456768
-77.469806	-34.586862	2.466765
-76.613964	-34.698822	2.476762
-76.151251	-27.019086	2.486758
-75.108964	-35.510316	2.496755
-74.733530	-26.719327	2.506752
-74.741232	-30.724753	2.516749
-74.224776	-31.223099	2.526746
-73.413316	-32.192146	2.536742
-72.864877	-36.044471	2.546739
-72.652489	-29.047232	2.556736
-71.594866	-29.075243	2.566733
-71.476736	-26.071012	2.576730
-71.238644	-26.990943	2.586726
-70.113846	-31.232530	2.596723
-70.103894	-34.160678	2.606720
-69.843738	-35.563408	2.616717
-68.872353	-30.924783	2.626714
-68.488516	-29.405944	2.636710
-68.103290	-37.348529	2.646707
-66.954969	-26.341578	2.656704
-66.739800	-30.584069	2.666701
-66.687174	-37.395915	2.676698
-66.253442	-33.104914	2.686694
-65.377208	-31.720574	2.696691
-64.978379	-29.876620	2.706688
-64.192850	-23.154098	2.716685
-63.740477	-32.063925	2.726682
-63.528651	-28.674507	2.736678
-63.104901	-30.356251	2.746675
-62.380879	-26.069260	2.756672
-62.001797	-25.960396	2.766669
-61.638154	-27.088430	2.776666
-60.527174	-25.650691	2.786662
-60.391440	-24.677198	2.796659
-60.228764	-29.978750	2.806656
-59.241765	-26.202204	2.816653
-58.797369	-26.842929	2.826650
-58.671002	-26.069422	2.836646
-58.023568	-25.662582	2.846643
-57.427681	-28.399884	2.856640
-57.087880	-26.655419	2.866637
-56.152090	-24.591167	2.876634
-55.556455	-23.417611	2.886630
-55.713124	-24.994540	2.896627
-55.083235	-24.857463	2.906624
-54.305248	-29.989826	2.916621
-53.954307	-30.719794	2.926618
-53.581009	-29.496377	2.936614
-52.707539	-30.863156	2.946611
-52.383596	-31.947863	2.956608
-52.112619	-37.229016	2.966605
-51.336347	-34.304733	2.976602
-51.120624	-33.917683	2.986598
-50.325946	-37.761387	2.996595
-49.961227	-29.286338	3.006592
-49.598416	-27.514662	3.016589
-48.537297	-30.382356	3.026586
-48.058649	-28.496097	3.036582
-48.151009	-37.311363	3.046579
-47.752874	-32.753848	3.056576
-47.029810	-25.954985	3.066573
-46.549133	-35.133669	3.076570
-45.792897	-34.123240	3.086566
-44.885179	-30.057536	3.096563
-44.803094	-33.511551	3.106560
-44.675862	-32.752808	3.116557
-43.770288	-31.508866	3.126554
-43.221905	-28.413667	3.136550
-43.248826	-31.135161	3.146547
-42.210197	-27.060904	3.156544
-41.694921	-29.139737	3.166541
-41.323252	-35.003846	3.176538
-41.310878	-30.403588	3.186534
-40.223565	-38.650938	3.196531
-39.992724	-43.874662	3.206528
-39.387003	-30.384491	3.216525
-38.643089	-30.808470	3.226522
-38.540063	-34.635240	3.236518
-37.840790	-33.319592	3.246515
-36.859909	-33.831615	3.256512
-36.757599	-26.334625	3.266509
-36.783334	-29.254890	3.276506
-36.148423	-33.741161	3.286502
-35.294335	-37.918149	3.296499
-34.999155	-30.242672	3.306496
-33.832507	-27.786896	3.316493
-33.672530	-27.682645	3.326490
-33.864240	-27.063928	3.336486
-33.051407	-27.260042	3.346483
-32.036708	-33.221154	3.356480
-31.826089	-32.102981	3.366477
-31.718481	-31.668585	3.376474
-30.837768	-30.402345	3.386470
-30.494175	-31.442884	3.396467
-29.353222	-29.999431	3.406464
-29.236048	-29.340977	3.416461
-29.074941	-28.380773	3.426458
-28.482573	-30.751165	3.436454
-27.722370	-31.468882	3.446451
-27.037331	-37.312766	3.456448
-27.321665	-35.856557	3.466445
-26.630868	-36.343065	3.476442
-26.043830	-34.785161	3.486438
-25.134315	-37.761113	3.496435
-24.548427	-34.132122	3.506432
-24.452197	-26.369952	3.516429
-24.177660	-27.700177	3.526426
-22.953735	-28.409921	3.536422
-22.611778	-31.427234	3.546419
-22.651864	-28.605253	3.556416
-21.875687	-32.050521	3.566413
-21.184793	-32.971536	3.576410
-21.095199	-31.787678	3.586406
-20.272913	-32.777476	3.596403
-19.785476	-26.168787	3.606400
-19.600664	-29.437882	3.616397
-18.556882	-32.950385	3.626394
-17.968322	-33.014910	3.636390
-18.059822	-28.442499	3.646387
-17.544290	-28.238860	3.656384
-16.875813	-28.121602	3.666381
-16.576973	-27.862716	3.676378
-15.226610	-34.809052	3.686374
-14.823947	-25.796522	3.696371
-14.908609	-28.386941	3.706368
-14.631872	-24.068350	3.716365
-14.147437	-30.165911	3.726362
-13.222097	-27.586392	3.736358
-12.968434	-27.979369	3.746355
-11.853738	-32.007853	3.756352
-11.511255	-32.909107	3.766349
-11.427310	-27.638632	3.776346
-11.186126	-23.517075	3.786342
-10.207728	-28.992237	3.796339
-10.053699	-27.200209	3.806336
-8.880057	-22.924039	3.816333
-8.564339	-29.976848	3.826330
-8.714458	-32.904967	3.836326
-7.927619	-32.889900	3.846323
-6.732746	-34.841793	3.856320
-6.632616	-27.531553	3.866317
-6.497931	-31.303502	3.876314
-6.316279	-30.723496	3.886310
-5.052382	-30.047269	3.896307
-4.987256	-33.375381	3.906304
-4.124982	-26.998486	3.916301
-3.881275	-23.804617	3.926298
-3.738315	-17.392379	3.936294
-3.050907	-5.559421	3.946291
-2.854233	-0.855510	3.956288
-2.461631	24.726136	3.966285
-1.907808	34.180174	3.976282
-1.278999	54.495996	3.986278
-0.970729	80.185948	3.996275
-0.330307	100.830077	4.006272
0.000000	127.087451	4.011277
-0.178718	116.646907	4.016282
0.167820	142.214759	4.021286
0.017359	151.596011	4.026291
0.515825	155.014468	4.031296
0.571023	173.325254	4.036301
0.617910	173.868521	4.041306
0.531926	188.779718	4.046310
0.475443	177.848442	4.051315
0.769103	180.952916	4.056320
0.892527	198.475325	4.061325
1.143596	199.640333	4.066330
0.909262	194.528734	4.071334
0.954067	196.629526	4.076339
0.853811	186.507269	4.081344
0.600369	199.162239	4.086349
0.850086	208.447461	4.091354
0.998134	220.618795	4.096358
1.055423	225.215211	4.101363
1.243305	230.400956	4.106368
1.132768	228.503982	4.111373
1.436510	232.952633	4.116378
1.319625	230.448715	4.121382
1.291219	235.777432	4.126387
1.227907	230.078644	4.131392
1.299343	223.466966	4.136397
1.074369	206.410818	4.141402
0.919756	209.938420	4.146406
0.955369	225.646094	4.151411
1.442848	219.829265	4.156416
1.161750	232.203295	4.161421
1.413241	239.121979	4.166426
1.502747	239.325877	4.171430
1.294118	234.254606	4.176435
1.657479	229.544467	4.181440
1.229996	224.029518	4.186445
0.986792	217.017847	4.191450
1.337205	226.173134	4.196454
1.370359	233.143560	4.201459
1.416708	227.471607	4.206464
1.446222	237.080829	4.211469
1.422470	236.316009	4.216474
1.428859	236.223259	4.221478
1.344831	235.387315	4.226483
1.610650	231.463137	4.231488
1.624310	236.970977	4.236493
1.648580	222.886869	4.241498
1.398456	209.421671	4.246502
0.945625	205.242946	4.251507
1.868252	227.202958	4.256512
1.490675	243.544243	4.261517
1.416311	227.106253	4.266522
1.702779	230.565161	4.271526
1.351280	239.670136	4.276531
1.872453	228.185742	4.281536
1.387032	231.839169	4.286541
1.470188	235.911520	4.291546
1.558783	241.012280	4.296550
1.346298	239.545409	4.301555
1.576543	231.359126	4.306560
1.563706	234.189352	4.311565
1.327387	233.363826	4.316570
1.754106	228.529529	4.321574
1.441020	235.680430	4.326579
1.385822	233.027175	4.331584
1.447460	241.899949	4.336589
1.478746	236.680019	4.341594
1.555708	227.448570	4.346598
1.450408	234.874485	4.351603
1.604749	231.759101	4.356608
1.655834	249.271642	4.361613
1.845012	258.566327	4.366618
2.296905	260.653195	4.371622
1.550875	251.705029	4.376627
1.756590	248.406491	4.381632
1.784406	261.867433	4.386637
1.913439	260.666061	4.391642
1.744863	254.029190	4.396646
1.552807	259.959857	4.401651
1.975836	259.758844	4.406656
1.970890	263.097884	4.411661
2.005447	271.777428	4.416666
1.994452	262.230970	4.421670
1.887669	274.139857	4.426675
1.879557	276.843999	4.431680
1.960967	273.336143	4.436685
1.874948	272.320752	4.441690
2.138627	271.639364	4.446694
2.035933	272.240163	4.451699
2.158387	264.389227	4.456704
1.829595	260.821031	4.461709
2.083127	269.761897	4.466714
2.276157	263.634262	4.471718
1.873137	251.730219	4.476723
2.108900	255.956487	4.481728
1.892093	268.707667	4.486733
1.972840	268.122286	4.491738
2.080258	275.702440	4.496742
1.909189	271.245563	4.501747
2.149655	258.757796	4.506752
2.225820	269.268839	4.511757
2.159591	266.392638	4.516762
1.922783	268.860943	4.521766
1.768159	274.321675	4.526771
1.961530	269.275389	4.531776
2.002776	279.004452	4.536781
1.952187	263.295397	4.541786
1.925710	270.175467	4.546790
1.876811	276.514208	4.551795
2.010334	276.818168	4.556800
2.429050	288.267671	4.561805
2.526829	291.597403	4.566810
2.271127	279.870425	4.571814
2.368181	280.143917	4.576819
2.240453	269.779680	4.581824
2.270805	277.480343	4.586829
2.059406	276.924197	4.591834
2.411834	284.627770	4.596838
2.218763	293.691347	4.601843
2.550037	293.499608	4.606848
2.207867	302.209978	4.611853
2.220140	299.274003	4.616858
2.327398	307.416216	4.621862
2.126251	319.129612	4.626867
2.449811	314.326974	4.631872
2.502907	309.297786	4.636877
2.457381	303.175895	4.641882
2.263784	296.419024	4.646886
2.228814	310.095437	4.651891
2.438010	305.678788	4.656896
2.590173	303.307713	4.661901
2.462839	308.325059	4.666906
2.509865	309.936299	4.671910
2.385271	310.802395	4.676915
2.588806	308.892081	4.681920
2.294264	319.580776	4.686925
2.512357	306.796920	4.691930
2.510929	306.404130	4.696934
2.566953	310.999991	4.701939
2.716462	310.733368	4.706944
2.629204	312.553131	4.711949
2.370878	306.718081	4.716954
2.579243	306.438160	4.721958
2.544405	318.955201	4.726963
2.850979	306.653392	4.731968
2.478435	308.014818	4.736973
2.809662	336.656889	4.741978
3.197278	327.799398	4.746982
2.793980	322.065705	4.751987
2.548231	316.989504	4.756992
2.375230	314.179717	4.761997
2.741048	322.688795	4.767002
2.798758	327.608016	4.772006
2.542255	341.060853	4.777011
2.699345	337.297329	4.782016
2.742336	344.064299	4.787021
2.593364	336.166314	4.792026
3.147923	341.213825	4.797030
2.434286	340.383662	4.802035
3.072836	340.570644	4.807040
2.642996	339.580412	4.812045
2.606739	335.072973	4.817050
2.860380	333.303348	4.822054
2.427653	339.565367	4.827059
2.805775	336.461845	4.832064
2.774715	342.615714	4.837069
2.747737	340.027625	4.842074
2.870874	339.131913	4.847078
2.989653	361.777380	4.852083
3.134433	361.645137	4.857088
3.024109	355.589604	4.862093
2.814481	346.276087	4.867098
3.297442	347.314497	4.872102
3.055470	364.316835	4.877107
2.783698	344.659078	4.882112
2.697727	365.621024	4.887117
3.009055	372.961636	4.892122
3.158685	371.552994	4.897126
2.922803	378.049430	4.902131
3.087812	368.678994	4.907136
3.015319	377.210165	4.912141
3.186152	377.550179	4.917146
3.086869	375.858134	4.922150
3.123282	387.799439	4.927155
3.343419	385.981484	4.932160
3.137538	391.125136	4.937165
3.169665	383.992412	4.942170
3.344813	380.990772	4.947174
3.135238	380.545619	4.952179
3.132972	390.689658	4.957184
2.972635	380.835934	4.962189
3.243869	379.577063	4.967194
3.465208	378.815854	4.972198
3.176311	374.877132	4.977203
2.979749	377.085999	4.982208
2.952090	382.560673	4.987213
3.218113	381.207351	4.992218
3.190027	381.576556	4.997222
3.056288	387.668115	5.002227
3.381507	395.054785	5.007232
3.311645	406.629485	5.012237
3.342461	406.597219	5.017242
3.706656	411.495710	5.022246
3.485799	416.958580	5.027251
3.578443	416.564220	5.032256
3.338108	405.840043	5.037261
3.323620	408.295433	5.042266
3.863058	407.494967	5.047270
3.487970	403.438689	5.052275
3.331388	388.214357	5.057280
2.921695	391.532830	5.062285
3.119489	414.300269	5.067290
3.332797	414.841246	5.072294
2.894760	426.588227	5.077299
3.300558	417.347403	5.082304
3.185468	414.357112	5.087309
3.180140	437.769380	5.092314
3.334834	448.183672	5.097318
3.151099	451.729965	5.102323
3.700394	451.013509	5.107328
3.601303	452.544765	5.112333
3.602982	457.350955	5.117338
3.705593	446.329206	5.122342
3.502990	455.773150	5.127347
3.615643	448.072933	5.132352
3.767139	455.342763	5.137357
3.923762	461.555586	5.142362
3.631995	456.851642	5.147366
3.563523	459.927732	5.152371
3.728588	447.277062	5.157376
3.521110	452.921846	5.162381
3.498934	448.810866	5.167386
3.592170	448.158287	5.172390
3.246644	452.682547	5.177395
3.602569	460.524951	5.182400
3.673533	479.237442	5.187405
3.774103	481.216752	5.192410
4.095745	482.519679	5.197414
4.130203	482.401559	5.202419
4.247957	481.994160	5.207424
3.935952	470.560332	5.212429
3.617767	458.585642	5.217434
3.972524	466.280040	5.222438
4.108784	476.502432	5.227443
3.962054	473.833705	5.232448
3.947947	467.722530	5.237453
3.721977	467.509792	5.242458
3.941702	480.699969	5.247462
4.006697	489.920832	5.252467
4.246775	487.612133	5.257472
3.997792	482.639423	5.262477
4.157675	482.315034	5.267482
3.966789	472.725614	5.272486
4.063301	482.770475	5.277491
4.140113	476.644241	5.282496
4.054447	469.658465	5.287501
3.900643	468.122258	5.292506
4.094594	475.941762	5.297510
4.109343	494.180097	5.302515
4.395873	487.644580	5.307520
3.885705	479.247665	5.312525
3.894712	482.218376	5.317530
4.387158	483.589716	5.322534
4.189516	480.082634	5.327539
4.106306	479.603133	5.332544
3.985885	480.536037	5.337549
4.006737	483.776525	5.342554
3.729104	484.500036	5.347558
3.929575	487.234600	5.352563
4.087840	484.248760	5.357568
4.149538	485.363844	5.362573
4.063450	485.729237	5.367578
4.511551	482.064902	5.372582
4.360243	489.208468	5.377587
4.138285	479.719505	5.382592
4.181384	482.488810	5.387597
3.746782	490.626519	5.392602
4.687977	507.488148	5.397606
4.465538	500.964680	5.402611
4.834892	491.020410	5.407616
4.474967	484.119708	5.412621
4.562551	488.517990	5.417626
4.519026	481.278555	5.422630
4.176159	492.957532	5.427635
4.273179	479.541967	5.432640
4.212472	494.501961	5.437645
4.414262	492.681900	5.442650
4.189920	484.248110	5.447654
4.264145	510.803962	5.452659
4.779297	509.094420	5.457664
4.278207	516.660605	5.462669
4.467348	525.377644	5.467674
4.483379	524.416578	5.472678
4.347403	525.587882	5.477683
4.797412	528.942221	5.482688
4.539997	525.237819	5.487693
4.385001	522.309569	5.492698
4.689176	523.235117	5.497702
4.598570	516.065033	5.502707
4.946422	516.328574	5.507712
4.736872	523.511993	5.512717
4.394973	526.052404	5.517722
4.843423	521.861300	5.522726
4.407470	525.013253	5.527731
4.636201	514.650803	5.532736
4.454337	525.588180	5.537741
4.286317	524.176081	5.542746
4.452766	524.770407	5.547750
4.327906	529.232889	5.552755
4.302984	524.487893	5.557760
4.749515	534.389970	5.562765
4.226799	542.446192	5.567770
4.731469	547.350475	5.572774
4.506547	556.732658	5.577779
4.769610	549.959850	5.582784
4.264144	552.014265	5.587789
4.210391	548.767905	5.592794
4.419777	542.469516	5.597798
4.506017	571.913732	5.602803
4.881995	572.385745	5.607808
4.947010	588.927222	5.612813
4.619526	575.378607	5.617818
4.776412	578.638030	5.622822
5.017703	583.123765	5.627827
4.955687	580.890929	5.632832
5.210358	580.763378	5.637837
4.799399	589.507007	5.642842
5.264147	574.047189	5.647846
4.771789	579.886409	5.652851
4.922457	581.700747	5.657856
4.994442	583.847413	5.662861
4.863520	583.752337	5.667866
5.027977	581.931344	5.672870
4.700241	576.115777	5.677875
5.105105	586.192132	5.682880
5.273169	588.815452	5.687885
5.200195	585.928862	5.692890
5.185018	575.047497	5.697894
4.860165	572.851476	5.702899
4.920839	571.363021	5.707904
5.197016	587.546878	5.712909
4.882157	581.073609	5.717914
5.191729	575.422275	5.722918
5.324062	584.563368	5.727923
5.550535	576.347532	5.732928
5.062092	580.409247	5.737933
4.948460	580.321372	5.742938
5.133518	583.720584	5.747942
4.935418	582.823192	5.752947
5.015857	585.902276	5.757952
5.321804	585.423256	5.762957
5.384901	593.367697	5.767962
5.225952	575.655101	5.772966
5.104181	579.269901	5.777971
5.439313	581.550993	5.782976
5.465539	583.039802	5.787981
4.847987	581.384417	5.792986
5.544244	598.654155	5.797990
5.464180	610.345351	5.802995
5.447570	595.882266	5.808000
5.484059	590.769499	5.813005
5.354005	590.956872	5.818010
5.165541	588.881336	5.823014
5.236267	605.398993	5.828019
5.355721	608.808680	5.833024
5.259513	608.206608	5.838029
5.402809	620.553099	5.843034
5.660785	610.944916	5.848038
5.400896	614.182189	5.853043
5.350713	611.918380	5.858048
5.466215	608.531495	5.863053
5.524206	606.634195	5.868058
5.386351	612.568650	5.873062
5.302129	619.054677	5.878067
5.522046	614.378438	5.883072
5.529982	617.374415	5.888077
5.505488	614.538403	5.893082
5.920947	618.152857	5.898086
5.556343	619.936093	5.903091
5.623703	613.431291	5.908096
5.484790	611.381095	5.913101
5.547104	617.314375	5.918106
5.533610	623.058133	5.923110
5.497526	632.988487	5.928115
5.420927	622.810521	5.933120
5.332728	623.818218	5.938125
5.501584	640.899848	5.943130
5.929729	644.788486	5.948134
5.958270	656.513042	5.953139
5.932301	645.684131	5.958144
5.409233	633.813486	5.963149
5.382323	641.029273	5.968154
5.631453	644.504719	5.973158
5.853838	649.833294	5.978163
6.015034	648.481718	5.983168
6.072594	650.752344	5.988173
5.866839	654.740822	5.993178
5.888744	652.869226	5.998182
5.530401	660.506961	6.003187
6.020548	658.978165	6.008192
5.996212	658.459703	6.013197
5.933670	667.251456	6.018202
6.331420	648.163079	6.023206
5.895748	647.046900	6.028211
5.875518	625.925284	6.033216
5.729251	620.954860	6.038221
5.715648	631.018445	6.043226
5.865401	640.294037	6.048230
5.840659	651.255806	6.053235
5.730261	654.576476	6.058240
6.024177	643.565535	6.063245
5.779599	657.160335	6.068250
6.104877	649.126034	6.073254
5.873637	656.573006	6.078259
6.154237	650.718048	6.083264
5.899864	636.329424	6.088269
5.793145	634.395851	6.093274
6.106891	641.277371	6.098278
5.585075	629.747528	6.103283
5.660799	640.929068	6.108288
6.125461	642.221351	6.113293
5.864336	655.959792	6.118298
6.141049	653.116915	6.123302
6.177797	643.139216	6.128307
5.996520	622.182413	6.133312
6.045074	618.285236	6.138317
5.726009	620.420094	6.143322
5.727101	616.209110	6.148326
5.462385	627.399259	6.153331
5.638837	638.405060	6.158336
6.180125	646.638190	6.163341
5.971570	656.465294	6.168346
5.939635	632.625447	6.173350
5.656575	635.175865	6.178355
5.691116	640.366618	6.183360
5.683592	649.847445	6.188365
5.964968	650.486092	6.193370
6.123564	653.074680	6.198374
5.894712	651.469577	6.203379
6.175430	656.302244	6.208384
6.031125	647.719734	6.213389
6.017613	633.996132	6.218394
6.022453	617.073756	6.223398
5.747923	616.927865	6.228403
5.706746	626.584753	6.233408
5.942281	624.772904	6.238413
5.801902	623.664268	6.243418
5.830364	621.445847	6.248422
5.901084	628.705454	6.253427
5.660905	633.718305	6.258432
5.905106	642.745000	6.263437
5.849747	655.673419	6.268442
5.878250	653.712716	6.273446
6.056403	658.307007	6.278451
5.908007	651.129064	6.283456
5.831587	644.516233	6.288461
5.845414	655.842621	6.293466
5.960863	646.145137	6.298470
5.940424	643.237405	6.303475
5.810934	640.651244	6.308480
6.178735	636.260336	6.313485
5.730647	639.895835	6.318490
5.824448	624.967263	6.323494
5.745574	637.410943	6.328499
5.980981	638.348873	6.333504
6.067684	644.402845	6.338509
5.608384	645.212293	6.343514
6.131437	644.000901	6.348518
5.662851	634.273049	6.353523
5.802577	641.480976	6.358528
5.929856	650.611894	6.363533
6.107931	659.160141	6.368538
5.792703	652.924701	6.373542
5.779685	659.225687	6.378547
5.828421	660.485017	6.383552
6.162224	655.833322	6.388557
5.851824	646.437641	6.393562
5.800095	631.494482	6.398566
5.726801	648.267318	6.403571
5.817366	654.221194	6.408576
5.979432	661.458190	6.413581
5.940972	661.885757	6.418586
5.999539	661.033873	6.423590
5.702404	665.095504	6.428595
6.138392	652.307054	6.433600
6.003249	648.698412	6.438605
5.920380	653.773629	6.443610
5.903035	636.270379	6.448614
5.531487	648.254970	6.453619
5.768658	646.841083	6.458624
6.127511	656.965361	6.463629
5.892543	661.751993	6.468634
5.788205	654.294026	6.473638
6.042338	661.694964	6.478643
5.941138	649.482116	6.483648
5.866797	643.871438	6.488653
5.726749	641.943383	6.493658
6.042394	654.255836	6.498662
6.032375	647.065242	6.503667
5.777259	637.317037	6.508672
5.857979	635.496879	6.513677
5.834764	650.857142	6.518682
6.138056	650.887110	6.523686
5.573161	642.628821	6.528691
6.022460	640.032462	6.533696
5.848697	640.609127	6.538701
5.863139	660.593196	6.543706
6.129083	652.335066	6.548710
6.009529	639.807150	6.553715
5.832276	627.455750	6.558720
6.136115	625.379203	6.563725
5.731835	625.597382	6.568730
5.761948	631.425094	6.573734
5.561170	625.316351	6.578739
5.771835	639.132947	6.583744
6.072983	655.196110	6.588749
5.773015	664.189787	6.593754
6.187588	657.003475	6.598758
5.928110	647.793150	6.603763
5.891321	630.666891	6.608768
5.814985	622.328500	6.613773
5.669237	636.386062	6.618778
6.119306	642.530237	6.623782
6.031007	630.584837	6.628787
5.814033	631.437830	6.633792
5.967082	627.409679	6.638797
5.839920	635.038326	6.643802
5.899567	622.642175	6.648806
5.896160	622.050390	6.653811
6.131405	623.554321	6.658816
6.157842	628.240427	6.663821
5.670249	625.897884	6.668826
6.081146	623.961088	6.673830
5.747674	624.595378	6.678835
5.631994	630.486700	6.683840
5.843898	629.643369	6.688845
5.705613	631.435308	6.693850
5.818091	629.754346	6.698854
5.829408	647.122561	6.703859
6.057224	649.336183	6.708864
6.053089	631.950733	6.713869
5.554287	627.097492	6.718874
6.128391	634.823538	6.723878
5.984898	639.712632	6.728883
5.833462	627.873203	6.733888
5.911929	632.343091	6.738893
5.525467	621.224598	6.743898
6.025985	630.507617	6.748902
5.839669	647.867118	6.753907
5.838504	646.116563	6.758912
5.995554	644.015775	6.763917
5.787568	646.590075	6.768922
5.867087	638.281518	6.773926
6.096399	644.939027	6.778931
5.806584	647.177582	6.783936
6.041387	635.288792	6.788941
5.811077	641.328161	6.793946
5.876437	631.460584	6.798950
6.038275	624.981574	6.803955
5.781702	635.338388	6.808960
5.785483	619.702062	6.813965
5.427977	634.062283	6.818970
6.174718	647.071397	6.823974
5.970925	652.880621	6.828979
6.186742	651.222802	6.833984
6.063892	634.421801	6.838989
5.718504	631.058344	6.843994
5.849489	621.790876	6.848998
5.808861	629.977087	6.854003
5.519050	631.890421	6.859008
5.928219	639.283041	6.864013
6.024606	659.106717	6.869018
6.035018	654.835372	6.874022
5.900919	639.097928	6.879027
5.716134	634.004422	6.884032
5.791978	641.810217	6.889037
5.866087	657.357237	6.894042
6.112210	658.358912	6.899046
5.601578	651.934017	6.904051
5.709244	648.596178	6.909056
6.025727	659.319894	6.914061
6.035796	671.547980	6.919066
6.076111	652.648242	6.924070
5.932385	634.560871	6.929075
5.768714	630.392954	6.934080
5.899387	625.752803	6.939085
5.652627	641.375043	6.944090
6.098199	643.147264	6.949094
6.127224	649.344587	6.954099
6.091090	632.824846	6.959104
5.644817	619.968995	6.964109
5.494642	622.517931	6.969114
5.966649	648.473945	6.974118
5.839628	654.611069	6.979123
5.903941	653.041488	6.984128
5.935651	655.170362	6.989133
5.588307	650.297559	6.994138
5.835962	648.657361	6.999142
5.958197	661.914355	7.004147
5.562692	660.344347	7.009152
6.172001	659.791212	7.014157
5.967233	668.355498	7.019162
5.975138	656.058666	7.024166
5.574329	661.245736	7.029171
5.883597	659.570864	7.034176
6.172578	659.872770	7.039181
6.026090	659.071419	7.044186
6.031282	653.440857	7.049190
5.826775	656.178771	7.054195
5.787342	663.512285	7.059200
6.017149	663.348001	7.064205
5.639159	662.403824	7.069210
5.800871	663.785348	7.074214
6.090798	663.931988	7.079219
5.837476	662.970719	7.084224
5.882272	658.694468	7.089229
5.807251	658.909039	7.094234
6.107894	657.520162	7.099238
6.145619	654.690416	7.104243
5.929440	638.998534	7.109248
5.826859	634.310569	7.114253
5.587945	636.128250	7.119258
5.651158	646.772729	7.124262
5.861061	659.827335	7.129267
5.644683	659.138990	7.134272
6.228832	651.326654	7.139277
5.804399	653.316354	7.144282
5.778932	656.108293	7.149286
5.945055	659.755362	7.154291
5.963967	663.059358	7.159296
6.113932	663.064196	7.164301
5.794970	665.682530	7.169306
5.823426	653.566220	7.174310
5.524005	658.854905	7.179315
5.945732	655.848692	7.184320
5.979147	644.528829	7.189325
5.927318	658.500210	7.194330
6.195388	651.816122	7.199334
6.047404	661.910268	7.204339
5.712609	661.353228	7.209344
6.026927	658.419661	7.214349
6.154946	656.842293	7.219354
5.741370	642.062451	7.224358
5.627302	644.554102	7.229363
5.883880	649.846624	7.234368
6.041696	656.812780	7.239373
6.113291	663.066208	7.244378
5.666045	641.776892	7.249382
5.501171	643.587839	7.254387
5.500202	659.756291	7.259392
5.787210	657.612273	7.264397
5.734278	667.823297	7.269402
5.907132	654.240109	7.274406
5.920326	660.135362	7.279411
5.815317	658.486859	7.284416
5.740982	652.229685	7.289421
5.797908	665.048741	7.294426
5.804101	664.294334	7.299430
6.105203	661.249680	7.304435
5.774910	663.459419	7.309440
6.058880	662.724136	7.314445
5.768603	665.344430	7.319450
6.194143	656.242085	7.324454
5.869269	652.158480	7.329459
5.836229	660.352923	7.334464
5.914824	655.999638	7.339469
5.819401	661.560030	7.344474
6.037873	654.599982	7.349478
5.738909	668.785167	7.354483
5.734206	665.363709	7.359488
5.621473	660.717675	7.364493
5.589974	668.175387	7.369498
5.648602	662.755418	7.374502
5.827894	659.872233	7.379507
5.849293	661.963347	7.384512
6.079816	666.466874	7.389517
5.675816	668.818275	7.394522
5.772190	667.249304	7.399526
6.048824	655.257663	7.404531
5.559558	657.688700	7.409536
5.942421	666.907156	7.414541
5.594887	663.920576	7.419546
5.798776	678.736485	7.424550
5.837991	688.669009	7.429555
5.671581	689.930419	7.434560
6.066969	687.522957	7.439565
5.532247	688.836674	7.444570
5.982742	693.057500	7.449574
6.077328	682.692089	7.454579
6.183780	689.183671	7.459584
6.174398	683.264235	7.464589
5.705367	679.641410	7.469594
5.818068	662.602452	7.474598
5.932841	663.196856	7.479603
5.902239	671.532197	7.484608
6.238961	650.952149	7.489613
5.883468	666.096302	7.494618
5.728336	664.331773	7.499622
5.789611	653.622603	7.504627
5.638536	655.618346	7.509632
5.973100	665.791251	7.514637
5.893516	678.671998	7.519642
6.380311	674.233352	7.524646
6.225113	669.371746	7.529651
5.999757	657.358243	7.534656
5.956766	648.991425	7.539661
5.972246	653.339136	7.544666
5.958671	655.050830	7.549670
6.014630	655.274892	7.554675
5.880832	658.895845	7.559680
6.092548	652.585777	7.564685
5.914997	662.098714	7.569690
6.001348	653.982807	7.574694
6.080077	654.540553	7.579699
5.853617	664.014227	7.584704
6.167414	656.116806	7.589709
5.686769	655.391706	7.594714
5.950538	659.058522	7.599718
6.035909	656.582811	7.604723
5.967399	660.035870	7.609728
6.017779	655.608321	7.614733
5.783190	654.707494	7.619738
5.947289	657.904958	7.624742
6.015799	657.648190	7.629747
5.834813	672.045521	7.634752
6.250218	653.051702	7.639757
6.092453	661.027620	7.644762
5.919868	641.604673	7.649766
5.774261	636.592298	7.654771
5.513087	629.952838	7.659776
6.098041	640.734307	7.664781
5.935620	648.094889	7.669786
6.045670	642.742981	7.674790
6.346489	638.531694	7.679795
5.517962	634.706735	7.684800
5.764237	630.044282	7.689805
5.514114	637.021540	7.694810
5.831524	653.370522	7.699814
6.068194	649.838845	7.704819
5.891345	658.287201	7.709824
6.010996	653.727408	7.714829
5.838917	652.073041	7.719834
5.776568	655.458377	7.724838
5.936907	659.240201	7.729843
5.891474	666.397102	7.734848
6.318585	646.605668	7.739853
6.135476	640.251263	7.744858
5.873685	632.627958	7.749862
6.055503	621.761894	7.754867
5.855526	631.376801	7.759872
5.893992	627.424064	7.764877
5.578945	633.698484	7.769882
5.655665	625.795343	7.774886
5.841118	623.162952	7.779891
5.767977	638.745783	7.784896
6.318568	637.036871	7.789901
6.264393	630.274725	7.794906
5.832399	623.588170	7.799910
5.837801	625.948734	7.804915
5.637309	623.560623	7.809920
6.030202	623.336575	7.814925
5.899661	623.621515	7.819930
5.807286	615.295257	7.824934
6.048117	627.829654	7.829939
5.688419	630.807969	7.834944
5.691756	622.236941	7.839949
5.984017	627.154518	7.844954
5.740887	622.896749	7.849958
5.633460	620.438366	7.854963
5.933968	642.583294	7.859968
5.913745	652.130954	7.864973
6.358404	644.741534	7.869978
5.853813	639.709667	7.874982
5.732410	628.066158	7.879987
5.650925	630.405589	7.884992
5.839107	638.021093	7.889997
5.941698	646.206488	7.895002
5.760664	652.687641	7.900006
5.876199	649.890795	7.905011
6.054281	652.355777	7.910016
6.267214	645.160629	7.915021
5.865978	638.848660	7.920026
5.787800	625.950005	7.925030
5.624468	627.980139	7.930035
5.506533	641.443837	7.935040
6.063752	649.505800	7.940045
5.922079	667.616907	7.945050
6.122536	658.870736	7.950054
6.083551	644.114114	7.955059
5.851513	636.790576	7.960064
5.909037	622.817622	7.965069
5.647080	633.982059	7.970074
5.767246	629.921068	7.975078
5.777631	639.432471	7.980083
5.876513	655.475846	7.985088
6.223183	651.142900	7.990093
5.913144	647.271153	7.995098
5.575645	625.564662	8.000102
6.027404	633.942065	8.005107
6.121309	644.423193	8.010112
6.310318	626.426765	8.015130
5.724040	636.835091	8.020147
5.530062	629.507107	8.025165
5.972583	632.265220	8.030182
5.692013	638.191309	8.035200
6.018294	633.777381	8.040218
5.976302	638.751422	8.045235
5.973212	625.903191	8.050253
6.167248	629.324459	8.055270
5.782685	631.517606	8.060288
6.036070	625.345782	8.065306
5.969667	632.878823	8.070323
5.681908	625.152222	8.075341
5.747082	636.699446	8.080358
5.832442	653.684345	8.085376
5.936556	656.917372	8.090394
6.131128	663.033672	8.095411
6.045340	666.146975	8.100429
6.054182	662.952859	8.105446
5.890940	668.983146	8.110464
6.047161	666.583866	8.115482
6.229931	668.267348	8.120499
5.836330	657.378132	8.125517
5.881705	641.864543	8.130534
6.114162	661.983955	8.135552
6.206750	655.904097	8.140570
6.259765	646.985297	8.145587
5.899810	647.913818	8.150605
5.593501	637.691616	8.155622
5.888374	661.421729	8.160640
6.044862	664.355551	8.165658
6.011817	669.160414	8.170675
5.887603	667.698070	8.175693
6.249465	662.610172	8.180710
5.775523	665.704291	8.185728
5.839882	668.606129	8.190746
5.727864	667.153576	8.195763
6.167427	668.018990	8.200781
6.090245	663.512032	8.205798
5.660627	668.941192	8.210816
5.856910	663.219334	8.215834
6.376537	670.604566	8.220851
5.648655	671.468825	8.225869
5.883336	659.846078	8.230886
5.925524	663.188962	8.235904
6.117876	666.292819	8.240922
5.976111	672.295930	8.245939
6.044943	695.197042	8.250957
6.191032	690.935371	8.255974
6.478206	694.136124	8.260992
6.015248	679.949908	8.266010
6.139417	672.560559	8.271027
5.796838	671.388297	8.276045
6.494978	681.804029	8.281062
6.040045	687.016140	8.286080
6.057585	684.032377	8.291098
6.311847	697.253747	8.296115
6.205303	690.694281	8.301133
6.108774	685.854712	8.306150
6.247561	698.076760	8.311168
6.232946	690.258836	8.316186
6.421284	700.083055	8.321203
5.806949	689.884662	8.326221
6.180401	687.636404	8.331238
6.017421	705.382519	8.336256
6.237209	696.244748	8.341274
6.140570	705.279594	8.346291
6.234903	699.743493	8.351309
6.398340	701.074295	8.356326
6.280510	703.645699	8.361344
5.964408	705.709416	8.366362
6.184635	696.862893	8.371379
6.074428	710.198167	8.376397
6.607112	701.943959	8.381414
6.233786	707.192561	8.386432
6.146734	703.932430	8.391450
6.329388	697.504589	8.396467
6.117926	709.971642	8.401485
6.563477	689.971517	8.406502
6.441351	695.863518	8.411520
5.921712	704.760547	8.416538
6.436479	698.788312	8.421555
6.101852	705.011550	8.426573
6.287161	703.487319	8.431590
6.044201	699.605405	8.436608
6.100756	692.653991	8.441626
6.640761	697.853705	8.446643
6.160726	696.789630	8.451661
6.117238	683.628768	8.456678
6.164450	705.816195	8.461696
6.071047	690.184207	8.466714
6.140952	695.520817	8.471731
6.193872	700.453177	8.476749
6.785887	706.862323	8.481766
6.398281	707.606853	8.486784
6.235735	696.962010	8.491802
6.103041	704.522597	8.496819
6.449732	719.233318	8.501837
6.433551	729.089454	8.506854
6.532825	734.874339	8.511872
6.200037	735.443267	8.516890
6.380261	735.884727	8.521907
6.356484	738.122863	8.526925
6.637399	725.623956	8.531942
6.598160	732.163231	8.536960
6.426148	722.472641	8.541978
6.447485	718.835523	8.546995
6.715968	729.954684	8.552013
6.532058	712.470049	8.557030
6.602728	709.316075	8.562048
6.302240	699.835739	8.567066
6.103928	700.667027	8.572083
6.472642	707.830431	8.577101
6.565852	716.427964	8.582119
6.304145	733.937719	8.587136
6.549404	731.791781	8.592154
6.615758	731.670633	8.597171
6.434273	730.276031	8.602189
6.651391	731.240092	8.607207
6.478449	732.521093	8.612224
6.553184	735.002744	8.617242
6.733341	733.314412	8.622259
6.592796	726.312161	8.627277
6.632226	710.881372	8.632295
6.509776	702.600617	8.637312
6.235406	708.375715	8.642330
6.648771	718.335114	8.647347
6.281483	733.561300	8.652365
6.685149	733.352014	8.657383
6.579795	738.377915	8.662400
6.059294	739.653087	8.667418
6.582021	732.778389	8.672435
6.314847	737.851557	8.677453
6.301654	739.991883	8.682471
6.464868	746.761012	8.687488
6.285985	742.699194	8.692506
6.167939	740.178400	8.697523
6.268247	737.065966	8.702541
6.351464	747.416256	8.707559
6.415794	769.168678	8.712576
6.406681	775.009319	8.717594
6.746195	774.775225	8.722611
6.517865	773.271847	8.727629
6.805325	779.227150	8.732647
6.635253	773.609223	8.737664
6.735165	773.328589	8.742682
6.787897	771.214920	8.747699
7.003780	777.557252	8.752717
6.976818	777.926728	8.757735
6.850340	777.025349	8.762752
6.728259	763.084562	8.767770
6.761427	739.928031	8.772787
6.660478	739.555468	8.777805
6.592380	736.584695	8.782823
6.871861	750.487330	8.787840
6.843251	745.384147	8.792858
6.934187	736.389730	8.797875
6.886137	739.064145	8.802893
6.950152	739.301239	8.807911
6.884849	730.820859	8.812928
6.452749	732.675453	8.817946
6.790761	735.992199	8.822963
6.817083	745.524002	8.827981
6.904272	734.235843	8.832999
6.824485	740.369655	8.838016
6.937709	747.651758	8.843034
7.069705	739.242633	8.848051
6.603013	740.593143	8.853069
6.904934	742.809234	8.858087
7.032978	735.287726	8.863104
7.118422	734.612660	8.868122
6.751578	732.907038	8.873139
6.793639	748.556372	8.878157
6.809177	739.042184	8.883175
6.950213	730.642196	8.888192
6.688418	743.821902	8.893210
6.824907	734.661290	8.898227
7.096841	734.496651	8.903245
6.897461	732.162938	8.908263
6.786146	736.018237	8.913280
6.793682	732.253488	8.918298
6.959485	733.825620	8.923315
6.815385	728.065227	8.928333
6.789518	732.832701	8.933351
6.823023	734.667279	8.938368
6.899313	744.994306	8.943386
7.181667	736.054801	8.948403
6.868430	736.962993	8.953421
6.937956	737.774339	8.958439
6.932070	736.176259	8.963456
6.698742	731.086509	8.968474
7.022120	727.887536	8.973491
6.762992	734.793915	8.978509
6.773427	736.837026	8.983527
6.981176	738.291195	8.988544
7.013358	737.667466	8.993562
7.008224	730.467209	8.998579
6.686289	738.815800	9.003597
6.709802	737.939584	9.008615
6.644565	733.504639	9.013632
6.997585	751.377554	9.018650
7.478773	753.891897	9.023667
7.033997	755.187206	9.028685
6.951983	740.467406	9.033703
6.821673	739.314709	9.038720
6.856748	750.884324	9.043738
7.058627	759.955986	9.048755
6.832708	770.419683	9.053773
7.061610	775.206003	9.058791
7.256011	773.612940	9.063808
6.719724	766.608490	9.068826
7.137596	758.584670	9.073843
6.924148	772.146531	9.078861
7.035327	766.906814	9.083879
7.223532	768.007942	9.088896
6.881600	762.665708	9.093914
7.155563	776.640535	9.098931
7.139875	771.403321	9.103949
7.314625	765.796797	9.108967
7.310420	768.025792	9.113984
6.996614	770.752881	9.119002
7.038578	766.464339	9.124019
7.010580	759.159593	9.129037
7.075215	774.075725	9.134055
7.107345	766.518512	9.139072
6.921989	773.538276	9.144090
7.463453	774.617913	9.149107
7.175603	776.269108	9.154125
6.865649	778.260166	9.159143
7.171976	771.569309	9.164160
7.106175	772.770370	9.169178
7.187288	766.544738	9.174195
7.376103	765.447063	9.179213
7.579503	769.983682	9.184231
7.302602	765.246394	9.189248
7.306896	770.537204	9.194266
7.331698	762.289117	9.199283
7.271482	768.096487	9.204301
7.091764	767.529105	9.209319
7.388106	755.884660	9.214336
7.161915	767.715649	9.219354
7.421044	775.158635	9.224371
7.307713	764.217028	9.229389
7.258554	768.891526	9.234407
7.506987	760.663491	9.239424
7.226041	768.431720	9.244442
7.539760	772.855588	9.249459
7.205819	763.372485	9.254477
7.009416	767.685953	9.259495
7.429366	769.901794	9.264512
7.079786	772.639138	9.269530
7.068783	768.273938	9.274547
7.336060	775.165997	9.279565
7.216236	784.263780	9.284583
7.345400	769.307025	9.289600
7.271570	780.441177	9.294618
7.099549	769.806513	9.299635
7.031125	774.343265	9.304653
7.054863	776.313316	9.309671
7.380259	770.696017	9.314688
7.587542	776.681131	9.319706
7.338467	769.948393	9.324723
6.973191	772.879271	9.329741
7.112428	768.162438	9.334759
7.407078	763.226181	9.339776
7.070156	779.618187	9.344794
7.373154	787.216897	9.349811
7.887634	796.030134	9.354829
7.197558	792.202158	9.359847
7.604605	786.553223	9.364864
7.335217	788.603309	9.369882
7.375218	794.303154	9.374899
7.322858	792.032878	9.379917
7.761747	806.039080	9.384935
7.550560	787.166428	9.389952
7.104138	786.492035	9.394970
7.341981	796.222295	9.399987
7.532549	798.524548	9.405005
7.445666	805.846507	9.410023
7.705832	798.011372	9.415040
7.392631	810.657943	9.420058
7.360228	799.508826	9.425075
7.662896	808.881920	9.430093
7.365527	811.248832	9.435111
7.611958	810.198303	9.440128
7.438742	813.167066	9.445146
7.415302	808.838558	9.450163
7.684611	813.927239	9.455181
7.686809	809.644090	9.460199
7.595030	810.995511	9.465216
7.588144	807.085894	9.470234
7.638174	808.110305	9.475251
7.853289	809.561293	9.480269
7.229016	811.544170	9.485287
7.581016	806.738947	9.490304
7.551469	805.926234	9.495322
7.300475	807.838245	9.500339
7.546195	806.270931	9.505357
7.600167	814.073088	9.510375
7.514469	807.486893	9.515392
7.664993	805.433006	9.520410
7.567923	818.625654	9.525427
7.915010	805.008300	9.530445
7.686325	807.866175	9.535463
8.020410	799.921953	9.540480
7.719891	808.972905	9.545498
7.892477	806.326418	9.550515
8.012993	803.836184	9.555533
7.581209	814.770986	9.560551
7.437495	805.556737	9.565568
7.694675	808.939637	9.570586
7.921834	812.862522	9.575603
8.180441	801.971892	9.580621
7.932060	806.299095	9.585639
7.941282	790.417347	9.590656
7.429491	789.965578	9.595674
7.376447	790.326382	9.600691
7.817826	804.066436	9.605709
7.712998	809.249352	9.610727
7.747087	801.593771	9.615744
7.477563	814.368538	9.620762
7.296655	804.765979	9.625779
7.401995	806.780392	9.630797
7.052976	807.073678	9.635815
7.311524	799.458091	9.640832
7.444988	817.196581	9.645850
7.685794	830.087632	9.650867
7.981011	835.449969	9.655885
7.923415	840.476656	9.660903
8.048078	838.715616	9.665920
7.790868	842.714386	9.670938
7.843141	843.208138	9.675955
8.084774	832.214003	9.680973
7.878607	837.930219	9.685991
7.933987	841.686290	9.691008
8.122028	835.707085	9.696026
7.909552	842.374302	9.701043
7.911454	825.469370	9.706061
7.772378	825.164533	9.711079
7.798012	829.044419	9.716096
7.780810	833.114067	9.721114
8.020547	832.324869	9.726131
8.382063	831.593061	9.731149
7.880206	835.852802	9.736167
7.984280	824.166526	9.741184
7.983360	817.274570	9.746202
7.817313	820.538196	9.751219
8.149466	829.230470	9.756237
7.932220	828.143341	9.761255
7.605756	823.587855	9.766272
7.857961	830.365905	9.771290
8.053597	830.409560	9.776307
8.127599	832.728757	9.781325
7.611967	831.083194	9.786343
8.156590	836.942789	9.791360
8.142963	831.771352	9.796378
8.079279	831.995343	9.801395
8.221377	830.914060	9.806413
8.139490	836.723470	9.811431
8.333896	835.124495	9.816448
8.131804	826.377358	9.821466
7.788558	819.835380	9.826483
8.221940	820.510499	9.831501
7.957483	831.663262	9.836519
7.920611	841.630371	9.841536
8.012439	838.615774	9.846554
8.083078	840.928837	9.851571
8.140438	830.209694	9.856589
8.082545	833.453838	9.861607
8.133879	839.195915	9.866624
8.099090	837.398290	9.871642
8.252087	844.986830	9.876659
8.392961	835.879760	9.881677
8.098563	836.293129	9.886695
8.413691	844.321727	9.891712
8.514564	832.066711	9.896730
7.947226	829.068753	9.901747
8.395731	813.843731	9.906765
8.455182	811.113621	9.911783
8.342474	810.703636	9.916800
8.171553	800.312851	9.921818
7.946628	809.266644	9.926835
8.427434	808.856798	9.931853
8.522129	808.192795	9.936871
8.140242	801.222600	9.941888
8.510747	806.954331	9.946906
8.206435	811.869902	9.951923
8.574211	800.697035	9.956941
8.455758	808.034459	9.961959
7.890182	810.337521	9.966976
8.165794	789.618596	9.971994
7.846600	799.869424	9.977011
8.111756	798.500457	9.982029
8.207152	813.989458	9.987047
7.964309	824.907546	9.992064
8.568978	830.322571	9.997082
8.331847	831.948838	10.002099
8.422355	831.253639	10.007117
8.610523	826.356253	10.012135
8.175870	828.567563	10.017152
8.277731	815.770690	10.022170
8.387636	832.227731	10.027187
8.304919	831.643102	10.032205
8.258108	831.484002	10.037223
8.513379	832.979915	10.042240
8.587637	823.435480	10.047258
8.482787	838.852552	10.052275
8.139573	832.899118	10.057293
8.304896	836.474392	10.062311
8.315952	838.534342	10.067328
8.268569	828.402990	10.072346
8.205063	841.108233	10.077363
8.670946	830.157670	10.082381
8.449094	830.946802	10.087399
8.272122	830.999798	10.092416
8.463295	833.344079	10.097434
8.355918	832.508428	10.102451
8.359954	832.770022	10.107469
8.337658	834.677234	10.112487
8.238071	839.252235	10.117504
8.571733	830.356539	10.122522
8.056404	842.595289	10.127539
8.308777	825.211108	10.132557
8.517453	839.289318	10.137575
8.341203	836.973018	10.142592
8.596229	832.783422	10.147610
8.405152	837.311764	10.152627
8.406736	836.827344	10.157645
8.635934	852.644603	10.162663
8.537314	870.736138	10.167680
8.703509	863.109042	10.172698
8.764801	868.108965	10.177715
8.585163	851.480118	10.182733
8.498030	848.660893	10.187751
8.387104	860.214217	10.192768
8.931327	875.291177	10.197786
8.589760	864.926639	10.202803
8.492871	860.631538	10.207821
8.719703	859.633462	10.212839
8.667613	865.241107	10.217856
8.938081	865.390081	10.222874
8.458102	859.768718	10.227891
8.953449	863.467688	10.232909
8.796841	848.603057	10.237927
8.150905	837.501181	10.242944
8.906155	852.889221	10.247962
8.518682	868.407057	10.252979
8.787616	867.372482	10.257997
8.658153	877.047873	10.263015
8.772938	877.503323	10.268032
9.038093	874.863542	10.273050
8.366089	870.103857	10.278067
8.283006	875.173749	10.283085
8.885559	877.102295	10.288103
8.483022	879.424036	10.293120
8.632380	876.906181	10.298138
8.749326	884.607792	10.303155
8.460024	881.124039	10.308173
8.598385	871.361095	10.313191
8.597912	874.311501	10.318208
9.007310	876.263763	10.323226
8.744822	872.955879	10.328243
8.936174	872.161700	10.333261
9.182134	877.566065	10.338279
8.467888	878.472561	10.343296
8.724534	873.740585	10.348314
8.577572	876.777056	10.353331
8.323739	877.889582	10.358349
8.836420	893.258384	10.363367
8.785581	910.679485	10.368384
9.106989	902.819196	10.373402
9.240250	909.709886	10.378419
9.174456	899.423276	10.383437
9.109109	877.939077	10.388455
8.740295	874.430305	10.393472
8.859682	864.087070	10.398490
8.709838	877.229060	10.403507
8.888094	896.912891	10.408525
9.243965	894.535632	10.413543
9.127737	901.371179	10.418560
9.015327	880.108540	10.423578
9.147681	874.664896	10.428595
9.077206	875.614388	10.433613
9.031862	875.145610	10.438631
8.623746	869.980432	10.443648
9.306418	869.102926	10.448666
9.100050	869.383614	10.453683
9.037436	875.954772	10.458701
8.981892	867.351841	10.463719
9.229567	873.663752	10.468736
9.194746	868.407234	10.473754
9.189965	873.741313	10.478771
8.939706	869.436569	10.483789
9.175857	870.577400	10.488807
8.834897	879.057557	10.493824
9.245129	865.401743	10.498842
9.033088	868.221047	10.503859
9.073021	872.749727	10.508877
9.056885	865.003617	10.513895
8.945788	868.847496	10.518912
9.200962	877.823792	10.523930
9.092264	888.232332	10.528947
9.154430	902.108492	10.533965
9.562433	887.688101	10.538983
9.182559	880.215198	10.544000
9.244779	875.520535	10.549018
9.138868	873.737438	10.554035
9.278870	882.528093	10.559053
9.422280	867.665337	10.564071
9.319404	868.615863	10.569088
9.626580	874.990360	10.574106
9.044041	873.022422	10.579123
9.098898	869.602149	10.584141
9.250822	869.892795	10.589159
8.958931	877.023943	10.594176
8.700680	869.528150	10.599194
8.997526	891.551676	10.604211
9.128800	902.727932	10.609229
9.187371	893.999401	10.614247
9.323853	907.485718	10.619264
9.351099	901.589805	10.624282
9.306457	907.389531	10.629299
9.061160	908.636466	10.634317
9.273669	896.825097	10.639335
9.412079	901.652819	10.644352
9.366219	902.602173	10.649370
9.488786	898.282138	10.654387
9.109419	913.629392	10.659405
9.114307	906.545106	10.664423
9.321141	911.302054	10.669440
9.485087	913.141036	10.674458
9.200266	908.284941	10.679475
9.384919	908.715438	10.684493
9.787550	902.433755	10.689511
9.440859	907.801236	10.694528
9.613590	897.924321	10.699546
9.543667	895.486473	10.704563
9.167649	908.310053	10.709581
9.391563	898.026648	10.714599
9.364308	902.027510	10.719616
9.489650	905.934997	10.724634
9.682347	903.102888	10.729651
9.592759	901.450938	10.734669
9.439695	902.575124	10.739687
9.248953	905.638535	10.744704
9.087981	907.905713	10.749722
9.257149	907.888793	10.754739
9.607309	920.222071	10.759757
9.493276	931.700769	10.764775
9.597115	940.454927	10.769792
9.659371	923.592254	10.774810
9.728370	928.073226	10.779827
9.516612	915.162463	10.784845
9.619035	902.470539	10.789863
9.590519	906.151547	10.794880
9.428019	905.950976	10.799898
9.750432	923.030375	10.804915
9.723561	927.086295	10.809933
9.764412	916.517458	10.814951
9.562091	905.883781	10.819968
9.567020	897.461756	10.824986
9.689542	916.161184	10.830003
9.581140	932.495826	10.835021
9.589028	929.473065	10.840039
9.928413	934.225392	10.845056
9.776198	925.773470	10.850074
9.642717	909.020781	10.855091
9.647207	923.896232	10.860109
9.952782	929.828123	10.865127
9.523268	920.421771	10.870144
9.475709	925.859797	10.875162
9.749635	929.376560	10.880179
9.628023	934.487496	10.885197
9.890638	934.741704	10.890215
9.742316	929.953941	10.895232
9.813614	936.052182	10.900250
9.818349	931.748500	10.905267
9.703702	931.088844	10.910285
9.625240	933.300238	10.915303
9.756058	932.097593	10.920320
9.827007	926.929836	10.925338
9.961767	924.854922	10.930355
9.599676	933.153183	10.935373
10.033378	930.481152	10.940391
9.740848	927.422709	10.945408
10.047629	931.527313	10.950426
9.770159	920.951737	10.955443
9.858297	929.587235	10.960461
10.257279	923.416380	10.965479
10.319298	930.504302	10.970496
9.819008	928.236528	10.975514
10.241627	931.200345	10.980531
10.108928	930.476751	10.985549
10.080225	926.469934	10.990567
9.773278	923.896929	10.995584
9.755520	932.635393	11.000602
10.179830	929.849175	11.005619
9.717205	936.182279	11.010637
10.092244	936.324962	11.015655
10.435020	926.696237	11.020672
9.974588	931.618407	11.025690
9.825729	928.919620	11.030707
9.911978	940.735616	11.035725
10.075602	923.618373	11.040743
10.264985	924.215402	11.045760
9.871279	931.958291	11.050778
10.233212	926.775811	11.055795
9.698190	931.866232	11.060813
9.773574	935.598542	11.065831
9.899184	923.797999	11.070848
10.031731	931.770660	11.075866
10.236009	928.926394	11.080883
9.911206	923.123019	11.085901
10.200839	928.664259	11.090919
10.592091	932.932821	11.095936
9.710016	930.864482	11.100954
9.896078	928.841307	11.105971
9.976493	940.888574	11.110989
10.093987	932.778584	11.116007
10.044086	923.594003	11.121024
10.089033	932.639393	11.126042
10.189531	925.736108	11.131059
10.023246	930.951287	11.136077
9.875747	930.974206	11.141095
10.157131	941.999261	11.146112
9.984971	956.435905	11.151130
10.381780	957.703283	11.156147
10.470583	956.404842	11.161165
10.497663	955.224886	11.166183
10.590639	958.442892	11.171200
10.083489	945.208986	11.176218
10.744709	941.778443	11.181235
10.231975	939.874524	11.186253
10.468263	925.826219	11.191271
10.237571	928.850188	11.196288
10.304348	934.466914	11.201306
10.385086	917.016961	11.206323
10.425399	928.939763	11.211341
10.634185	923.408645	11.216359
10.338096	924.147085	11.221376
10.341257	927.648056	11.226394
10.484305	927.362639	11.231411
10.382493	929.248779	11.236429
10.343950	929.314284	11.241447
10.301058	925.448394	11.246464
10.244131	923.402467	11.251482
10.768192	927.275430	11.256499
10.287521	923.333614	11.261517
10.183356	926.872829	11.266535
10.514585	923.264659	11.271552
10.500264	946.559029	11.276570
10.317397	940.875445	11.281587
10.645778	951.145906	11.286605
10.616262	946.778210	11.291623
10.492720	945.247620	11.296640
10.528706	956.713699	11.301658
10.725220	949.376017	11.306675
10.615382	950.352503	11.311693
10.273707	952.580715	11.316711
10.668926	945.419177	11.321728
10.447318	949.342003	11.326746
10.618960	952.593043	11.331763
10.631855	962.066181	11.336781
10.265608	949.243568	11.341799
10.585819	949.259902	11.346816
10.074936	956.346644	11.351834
10.363908	953.006478	11.356851
10.282774	957.035960	11.361869
10.376315	952.383723	11.366887
10.411881	950.140988	11.371904
10.203601	963.835618	11.376922
10.873593	976.442738	11.381939
10.903471	985.049333	11.386957
10.991326	979.130362	11.391975
11.150051	962.742992	11.396992
10.631893	947.696807	11.402010
10.869232	944.171107	11.407027
10.850565	943.767986	11.412045
10.791571	947.722542	11.417063
11.021320	946.133845	11.422080
10.882118	940.597355	11.427098
10.987298	939.349744	11.432115
10.907366	941.238956	11.437133
11.067492	950.142454	11.442151
11.004862	933.466979	11.447168
11.029813	948.581575	11.452186
11.032802	941.186970	11.457203
10.853224	946.777175	11.462221
11.071052	937.748243	11.467239
11.138804	935.193500	11.472256
10.996966	942.258494	11.477274
10.910170	932.869002	11.482291
11.174636	941.160360	11.487309
11.007265	926.342318	11.492327
10.766661	913.142251	11.497344
10.575203	923.025960	11.502362
11.191982	924.770274	11.507379
10.924714	929.975010	11.512397
10.728186	923.313028	11.517415
11.221468	927.281635	11.522432
10.726546	939.828486	11.527450
10.780680	935.274114	11.532467
11.500030	938.130137	11.537485
11.201430	936.612789	11.542503
11.071295	923.075931	11.547520
10.795031	912.583623	11.552538
10.930690	927.637348	11.557555
11.025305	933.792355	11.562573
11.194825	941.532530	11.567591
11.266693	934.016685	11.572608
11.138261	940.852302	11.577626
10.976362	925.713288	11.582643
11.079992	929.046842	11.587661
10.617952	940.865051	11.592679
11.245622	934.076820	11.597696
10.671939	942.592006	11.602714
10.843502	937.992204	11.607731
10.832406	937.911832	11.612749
11.123093	951.740354	11.617767
11.291173	940.943747	11.622784
10.931978	948.037256	11.627802
11.117409	939.001878	11.632819
11.107803	944.952896	11.637837
10.740155	937.438965	11.642855
10.643386	943.798494	11.647872
10.978621	969.824269	11.652890
11.125136	967.792678	11.657907
11.466224	979.533041	11.662925
11.394632	979.303637	11.667943
11.727086	976.073584	11.672960
11.425956	974.564919	11.677978
11.397977	966.592776	11.682995
11.286411	961.898912	11.688013
11.270073	974.224815	11.693031
11.506497	966.666745	11.698048
11.260392	964.351363	11.703066
11.398901	970.625488	11.708083
11.681566	966.643476	11.713101
11.327507	961.490968	11.718119
11.553604	942.166204	11.723136
11.285714	937.473432	11.728154
11.216510	936.495239	11.733171
11.615312	940.486187	11.738189
11.211586	949.699974	11.743207
11.627035	950.781595	11.748224
11.481503	954.197750	11.753242
11.237970	943.522843	11.758259
11.500600	949.494528	11.763277
11.388278	966.986501	11.768295
11.615938	968.883440	11.773312
11.343063	966.324863	11.778330
11.324550	971.742742	11.783347
11.387860	960.936307	11.788365
11.621501	969.071374	11.793383
11.094997	972.407317	11.798400
11.624714	969.946931	11.803418
11.114970	977.534261	11.808435
11.968704	971.555791	11.813453
11.358333	968.710987	11.818471
11.808875	973.683494	11.823488
11.890783	976.777358	11.828506
11.863887	982.145843	11.833523
11.689294	962.968897	11.838541
11.644602	973.305874	11.843559
11.719622	959.419670	11.848576
11.647803	966.548274	11.853594
11.653559	972.812101	11.858611
11.444417	969.959516	11.863629
11.524533	974.811874	11.868647
12.017354	968.006196	11.873664
11.909733	964.348251	11.878682
11.894229	968.077904	11.883699
11.646876	969.245659	11.888717
11.434142	967.054668	11.893735
11.645922	967.189741	11.898752
11.675717	976.560093	11.903770
11.477731	967.642911	11.908787
11.886000	963.666084	11.913805
11.716757	971.766690	11.918823
11.579506	972.199707	11.923840
11.536823	971.841899	11.928858
11.506593	968.554980	11.933875
12.045857	959.600363	11.938893
11.704079	973.455686	11.943911
11.653559	966.802577	11.948928
11.797393	972.657728	11.953946
11.579890	976.416501	11.958963
11.600856	979.399595	11.963981
11.754639	1002.379216	11.968999
11.843466	996.901399	11.974016
11.988941	998.040721	11.979034
12.058596	999.934696	11.984051
11.931928	994.851606	11.989069
11.909226	1004.705059	11.994087
12.101268	1001.594705	11.999104
12.068811	1008.056993	12.004122
11.919204	1008.083017	12.009139
11.880736	1001.657810	12.014157
11.777005	1006.770140	12.019175
12.068165	1003.627625	12.024192
11.922856	1004.472592	12.029210
11.753946	997.086347	12.034227
12.278221	1001.918706	12.039245
11.974252	1006.622478	12.044263
11.895141	1010.135122	12.049280
12.056432	999.424636	12.054298
11.903927	1001.608932	12.059315
12.079858	996.450538	12.064333
11.744989	1001.112182	12.069351
12.481726	994.207838	12.074368
12.050049	996.037983	12.079386
11.809701	1001.256395	12.084403
12.115524	1003.311649	12.089421
12.069166	1027.012217	12.094439
12.605770	1027.190349	12.099456
12.194006	1023.714638	12.104474
12.246885	1022.655991	12.109491
12.529243	1012.128983	12.114509
12.464233	1006.708920	12.119527
12.313587	1002.569919	12.124544
12.548036	993.545290	12.129562
12.456586	987.699706	12.134579
12.434021	989.056610	12.139597
12.603631	994.751601	12.144615
12.335545	986.845977	12.149632
12.492453	999.035342	12.154650
12.448810	995.030588	12.159667
12.604008	987.495800	12.164685
12.237422	989.526575	12.169703
12.413418	988.094407	12.174720
12.233584	984.825959	12.179738
12.371096	987.511420	12.184755
12.466186	980.513734	12.189773
12.297347	987.365117	12.194791
12.305382	995.275756	12.199808
12.348607	992.268390	12.204826
12.352415	996.383419	12.209843
12.584695	994.150621	12.214861
12.275131	995.854645	12.219879
12.564460	991.341622	12.224896
12.292300	983.871697	12.229914
12.259991	996.804963	12.234931
12.573400	983.542623	12.239949
12.740217	987.093277	12.244967
12.357416	983.407275	12.249984
12.672561	979.945845	12.255002
12.597729	983.987676	12.260019
12.522881	982.635627	12.265037
12.730666	994.883490	12.270055
12.731902	993.332234	12.275072
12.916505	990.973872	12.280090
12.420954	994.584998	12.285107
12.407939	992.947917	12.290125
12.766370	992.760686	12.295143
12.861650	999.182920	12.300160
12.665073	988.767519	12.305178
12.434482	997.690076	12.310195
12.675359	990.401325	12.315213
12.637706	987.841194	12.320231
12.434355	993.428265	12.325248
12.712015	997.669988	12.330266
12.687834	1026.023004	12.335283
12.912564	1018.015681	12.340301
12.875469	1022.898092	12.345319
12.741743	1013.206097	12.350336
12.960914	1009.478280	12.355354
12.648598	1007.062837	12.360371
12.964701	1009.802978	12.365389
12.876041	1007.699304	12.370407
12.697981	1002.698341	12.375424
13.125206	1005.071668	12.380442
12.775888	1001.974583	12.385459
12.573445	1001.403868	12.390477
12.926715	1023.380051	12.395495
12.776920	1031.660532	12.400512
12.886825	1026.763445	12.405530
12.736420	1029.590681	12.410547
12.973679	1018.858547	12.415565
13.296677	1026.454457	12.420583
13.159569	1029.218864	12.425600
13.186867	1029.302599	12.430618
13.064446	1023.202692	12.435635
13.173293	1010.663153	12.440653
13.152135	993.311874	12.445671
12.866944	988.369992	12.450688
12.989378	992.861424	12.455706
13.066327	994.224683	12.460723
13.066152	996.723112	12.465741
12.792103	993.070672	12.470759
13.074733	1008.911132	12.475776
13.177759	1007.423725	12.480794
13.205271	1014.516218	12.485811
13.133744	1013.230149	12.490829
13.324970	1018.371590	12.495847
12.822139	1003.364544	12.500864
12.973748	1009.556597	12.505882
12.873592	1017.857983	12.510899
12.938387	1015.640319	12.515917
13.185093	1020.879263	12.520935
13.163375	1018.083032	12.525952
13.272630	1007.796102	12.530970
13.124554	1015.702681	12.535987
13.269958	1017.588052	12.541005
13.041484	1028.083052	12.546023
13.295995	1024.684800	12.551040
13.008573	1021.529826	12.556058
13.075015	1022.873569	12.561075
13.483852	1018.997024	12.566093
13.085823	1011.922324	12.571111
12.913986	1012.156352	12.576128
13.152339	1020.806789	12.581146
13.213451	1040.745231	12.586163
13.619313	1045.522805	12.591181
13.918892	1047.160610	12.596199
13.468643	1031.220846	12.601216
13.515242	1026.287394	12.606234
13.133133	1026.650333	12.611251
13.071975	1022.087862	12.616269
13.291834	1022.737721	12.621287
13.298530	1047.979873	12.626304
13.744008	1047.881373	12.631322
13.733053	1047.905698	12.636339
13.396204	1046.637184	12.641357
13.484426	1042.077136	12.646375
13.404402	1037.727620	12.651392
13.339886	1043.990513	12.656410
13.141326	1047.734750	12.661427
13.420972	1043.869356	12.666445
13.701903	1040.608847	12.671463
13.561591	1048.227159	12.676480
13.739317	1047.683251	12.681498
13.486612	1044.524097	12.686515
13.311810	1046.380608	12.691533
13.384546	1046.157617	12.696551
13.393383	1042.653985	12.701568
13.729301	1046.294756	12.706586
13.604342	1053.284173	12.711603
13.666446	1043.348322	12.716621
13.816708	1042.975097	12.721639
13.374920	1055.975824	12.726656
13.668205	1041.967187	12.731674
13.834205	1049.944606	12.736691
13.359083	1050.970169	12.741709
13.602537	1066.875835	12.746727
14.072618	1079.550788	12.751744
14.060095	1070.474493	12.756762
14.029750	1060.667716	12.761779
13.616353	1053.922302	12.766797
13.884865	1038.874104	12.771815
13.743841	1049.484555	12.776832
13.868395	1047.577058	12.781850
14.055023	1054.266463	12.786867
13.715711	1058.002514	12.791885
14.060083	1048.835639	12.796903
14.124762	1047.112853	12.801920
14.045412	1034.728865	12.806938
13.881037	1037.362753	12.811955
13.817107	1045.288090	12.816973
13.870318	1037.988662	12.821991
13.945515	1046.469286	12.827008
14.041478	1047.715626	12.832026
13.692421	1049.640361	12.837043
13.730086	1057.606359	12.842061
14.085484	1063.932006	12.847079
13.995797	1070.396709	12.852096
14.185610	1065.566297	12.857114
14.329115	1078.937825	12.862131
14.473967	1064.765957	12.867149
14.276195	1044.043589	12.872167
14.103036	1047.553706	12.877184
14.195763	1032.343685	12.882202
14.282768	1029.947938	12.887219
14.293799	1030.769773	12.892237
14.331964	1022.995302	12.897255
14.045820	1031.608191	12.902272
14.277245	1027.805903	12.907290
14.439298	1026.782324	12.912307
13.774939	1034.634252	12.917325
14.267558	1022.726406	12.922343
14.195420	1030.973161	12.927360
13.910994	1024.551273	12.932378
14.277787	1026.680683	12.937395
14.172617	1033.334149	12.942413
13.892572	1037.169432	12.947431
13.873951	1062.835470	12.952448
14.027207	1058.882738	12.957466
14.300804	1059.720543	12.962483
14.235886	1071.056176	12.967501
14.503121	1064.638981	12.972519
14.607954	1065.515756	12.977536
14.542736	1061.365743	12.982554
14.114231	1064.757522	12.987571
14.536564	1064.984498	12.992589
14.833805	1066.341993	12.997607
14.215479	1065.652353	13.002624
14.530902	1065.600192	13.007642
14.714857	1064.865494	13.012659
14.606621	1067.875512	13.017677
14.747253	1065.516546	13.022695
14.416304	1066.143840	13.027712
14.466231	1060.312612	13.032730
14.314334	1065.719148	13.037747
14.414507	1062.498014	13.042765
14.462584	1069.033996	13.047783
14.329509	1071.106033	13.052800
14.381509	1062.134803	13.057818
14.785599	1069.281495	13.062835
14.413648	1061.899708	13.067853
14.856341	1065.706655	13.072871
14.765605	1058.778286	13.077888
14.523352	1064.965505	13.082906
14.773227	1060.304671	13.087923
14.695971	1061.642291	13.092941
14.823200	1064.608593	13.097959
14.607885	1075.247505	13.102976
14.476609	1070.449789	13.107994
14.698295	1066.101484	13.113011
14.518180	1070.268247	13.118029
14.467433	1064.595416	13.123047
14.745505	1075.551039	13.128064
14.963766	1083.087552	13.133082
15.291403	1071.545560	13.138099
14.628970	1064.998460	13.143117
14.895240	1056.538584	13.148135
14.867194	1061.099835	13.153152
14.945246	1062.386936	13.158170
15.258515	1050.299719	13.163187
15.047486	1051.255174	13.168205
14.922727	1061.447600	13.173223
14.794385	1053.477858	13.178240
14.826630	1059.775128	13.183258
14.945757	1056.845728	13.188275
14.725008	1060.734189	13.193293
14.881834	1057.429662	13.198311
14.698411	1054.495640	13.203328
14.900969	1078.492459	13.208346
15.350705	1080.876244	13.213363
15.060466	1075.926508	13.218381
14.746475	1068.072931	13.223399
14.641059	1071.909620	13.228416
14.913021	1083.515845	13.233434
15.038589	1087.405624	13.238451
15.144464	1086.065764	13.243469
15.572815	1087.059830	13.248487
15.180114	1092.944030	13.253504
15.063239	1080.671334	13.258522
15.100036	1084.852575	13.263539
15.179121	1087.124514	13.268557
15.441073	1078.512984	13.273575
15.086298	1089.416329	13.278592
15.079286	1087.610532	13.283610
15.111310	1078.303635	13.288627
14.731637	1087.721387	13.293645
15.120548	1080.251000	13.298663
15.030754	1087.514914	13.303680
15.056044	1091.916560	13.308698
15.406741	1084.965080	13.313715
15.042942	1095.515604	13.318733
15.117004	1095.515221	13.323751
15.725489	1110.808142	13.328768
15.702397	1119.975928	13.333786
15.675215	1095.812354	13.338803
14.839506	1095.816955	13.343821
15.116295	1102.021387	13.348839
15.392693	1104.995672	13.353856
15.465060	1123.185562	13.358874
15.816805	1124.529706	13.363891
15.535789	1122.818882	13.368909
15.738601	1104.672146	13.373927
15.510378	1095.973669	13.378944
15.355838	1101.557815	13.383962
15.626068	1088.693468	13.388979
15.225936	1089.896767	13.393997
15.609398	1103.754156	13.399015
15.843993	1118.422799	13.404032
15.430698	1106.734582	13.409050
15.757843	1113.473970	13.414067
15.575008	1110.921718	13.419085
15.860721	1111.259505	13.424103
15.888718	1090.518979	13.429120
15.156988	1088.227696	13.434138
15.847450	1103.958990	13.439155
16.120190	1117.257972	13.444173
16.012521	1106.017163	13.449191
16.097311	1096.458612	13.454208
15.574080	1089.076273	13.459226
15.785667	1083.774942	13.464243
15.921367	1096.859205	13.469261
15.932325	1082.172502	13.474279
15.696793	1093.154919	13.479296
15.808583	1092.737672	13.484314
16.008148	1082.378259	13.489331
15.716346	1083.302604	13.494349
15.852655	1079.206614	13.499367
16.091942	1077.841514	13.504384
15.635010	1086.363034	13.509402
15.655249	1074.827454	13.514419
15.680884	1084.764290	13.519437
15.902276	1091.703065	13.524455
15.914705	1085.306402	13.529472
15.917435	1074.797704	13.534490
16.025020	1086.168954	13.539507
15.695917	1084.633415	13.544525
16.020523	1093.307798	13.549543
16.021118	1112.172923	13.554560
15.985823	1118.472740	13.559578
16.099594	1111.864015	13.564595
16.039525	1128.602264	13.569613
16.227466	1113.542534	13.574631
16.209372	1116.413229	13.579648
15.824924	1117.122609	13.584666
16.055554	1114.846369	13.589683
15.835383	1119.132373	13.594701
16.035897	1113.394296	13.599719
16.191552	1110.909612	13.604736
15.990300	1121.915900	13.609754
16.224750	1110.982599	13.614771
16.300220	1121.920624	13.619789
16.284399	1123.579563	13.624807
16.396336	1115.288908	13.629824
16.203950	1123.699715	13.634842
16.089019	1113.261654	13.639859
16.044688	1124.006139	13.644877
15.668782	1113.687669	13.649895
16.121582	1110.475062	13.654912
16.087850	1113.448736	13.659930
16.454616	1128.059676	13.664947
16.642159	1135.917040	13.669965
16.949877	1135.433097	13.674983
16.484828	1115.764309	13.680000
16.297085	1118.415860	13.685018
16.477346	1107.977740	13.690035
16.630004	1114.497604	13.695053
16.328923	1100.788116	13.700071
16.375855	1113.842606	13.705088
16.568810	1114.775656	13.710106
16.740181	1109.837657	13.715123
16.322282	1109.266002	13.720141
16.144724	1116.251559	13.725159
16.732746	1117.285326	13.730176
16.820277	1116.963037	13.735194
16.762704	1105.052930	13.740211
16.507551	1106.553473	13.745229
16.553026	1110.019133	13.750247
16.548286	1107.958635	13.755264
16.328534	1120.216371	13.760282
16.415797	1127.632083	13.765299
16.980067	1132.457467	13.770317
17.192262	1137.075412	13.775335
17.221576	1119.441626	13.780352
16.648389	1111.235290	13.785370
17.039966	1101.963326	13.790387
16.859541	1104.045963	13.795405
16.966031	1100.183245	13.800423
16.940907	1095.853361	13.805440
16.626390	1108.874789	13.810458
16.770598	1096.000596	13.815475
16.762796	1101.448636	13.820493
16.706158	1105.017815	13.825511
16.757317	1106.567633	13.830528
16.779522	1096.835592	13.835546
16.944906	1094.912667	13.840563
17.128305	1097.573228	13.845581
16.917011	1105.621812	13.850599
16.799460	1104.253596	13.855616
16.404215	1104.423836	13.860634
16.686347	1122.303801	13.865651
16.727757	1128.104320	13.870669
16.767402	1130.840263	13.875687
17.267302	1125.764397	13.880704
17.332391	1131.073215	13.885722
17.279113	1128.595567	13.890739
17.017911	1125.869681	13.895757
17.085875	1129.691847	13.900775
17.500485	1124.734037	13.905792
16.933832	1125.115726	13.910810
16.782555	1126.072314	13.915827
17.310683	1121.901590	13.920845
16.994285	1136.497320	13.925863
17.096463	1132.153432	13.930880
17.118373	1129.562943	13.935898
17.180665	1134.328935	13.940915
17.115861	1126.041950	13.945933
16.918504	1122.538193	13.950951
17.199004	1123.126835	13.955968
17.062127	1128.086824	13.960986
17.340849	1133.919306	13.966003
17.303515	1137.888434	13.971021
17.225152	1155.247441	13.976039
17.604278	1153.684380	13.981056
17.459109	1157.818609	13.986074
17.400319	1151.258914	13.991091
17.580809	1135.375617	13.996109
17.155446	1147.384359	14.001127
17.459036	1153.794604	14.006144
17.230690	1160.262621	14.011162
17.480263	1164.674785	14.016179
17.816819	1161.303862	14.021197
17.939048	1164.199359	14.026215
17.706019	1140.781986	14.031232
17.559897	1143.809315	14.036250
17.402341	1125.587192	14.041267
17.512116	1126.628895	14.046285
17.306435	1149.125754	14.051303
17.556015	1146.513310	14.056320
17.285270	1156.652021	14.061338
17.509928	1155.457048	14.066355
17.684641	1153.108568	14.071373
17.574166	1157.596097	14.076391
18.019922	1157.730223	14.081408
18.034306	1153.791407	14.086426
17.982537	1151.896954	14.091443
17.692736	1160.621147	14.096461
17.773187	1149.987720	14.101479
18.205443	1158.782499	14.106496
18.126516	1154.998895	14.111514
18.044407	1127.981847	14.116531
18.306015	1113.523680	14.121549
17.746742	1112.601430	14.126567
17.922223	1117.379382	14.131584
18.127637	1109.957869	14.136602
17.675410	1104.010176	14.141619
17.738213	1109.595735	14.146637
17.556910	1112.050949	14.151655
17.939075	1127.243966	14.156672
17.898286	1143.461338	14.161690
17.754215	1147.206024	14.166707
17.800501	1139.880137	14.171725
17.957905	1147.180309	14.176743
18.097421	1140.460225	14.181760
18.028176	1138.901728	14.186778
18.041567	1143.800226	14.191795
18.132045	1135.507208	14.196813
18.102981	1145.116143	14.201831
18.583526	1139.724195	14.206848
18.505207	1138.526639	14.211866
18.121838	1143.969169	14.216883
18.476581	1138.866548	14.221901
18.024331	1124.982864	14.226919
18.266315	1123.679909	14.231936
18.650763	1130.953108	14.236954
18.065232	1110.838149	14.241971
18.154804	1109.976169	14.246989
18.010593	1121.263553	14.252007
18.234888	1129.547099	14.257024
18.215036	1132.531077	14.262042
18.049286	1127.679210	14.267059
18.150500	1134.361534	14.272077
18.602643	1137.254364	14.277095
18.613094	1137.681825	14.282112
18.081725	1132.415316	14.287130
18.135505	1139.558634	14.292147
18.793647	1136.692716	14.297165
18.607118	1151.527184	14.302183
18.420715	1140.030892	14.307200
18.373753	1129.895729	14.312218
18.365613	1144.145156	14.317235
18.546350	1147.972273	14.322253
18.342596	1143.318816	14.327271
18.376994	1138.384986	14.332288
18.507686	1140.571618	14.337306
18.541547	1143.465210	14.342323
18.671793	1131.662954	14.347341
18.085045	1151.328909	14.352359
18.480433	1156.689732	14.357376
18.859188	1164.301674	14.362394
18.669534	1177.176502	14.367411
19.012317	1166.605921	14.372429
18.791949	1181.067685	14.377447
18.897087	1162.039835	14.382464
18.794332	1157.059027	14.387482
18.426016	1152.126526	14.392499
18.856594	1151.990338	14.397517
18.820380	1172.114747	14.402535
18.900063	1168.382825	14.407552
18.961245	1169.729814	14.412570
18.816744	1173.168680	14.417587
19.237008	1169.532719	14.422605
19.112477	1170.766763	14.427623
18.722644	1151.253187	14.432640
19.015775	1155.343578	14.437658
18.863266	1163.582059	14.442675
19.252177	1162.820898	14.447693
18.858632	1159.450797	14.452711
18.956861	1161.093217	14.457728
19.162137	1161.851399	14.462746
18.816011	1168.247587	14.467763
19.051849	1157.767160	14.472781
19.149692	1166.370081	14.477799
18.833854	1164.491795	14.482816
18.905318	1155.359812	14.487834
19.068006	1164.220885	14.492851
19.218752	1154.512797	14.497869
19.161137	1166.256334	14.502887
18.982139	1166.174630	14.507904
19.175139	1167.999384	14.512922
18.742162	1172.093482	14.517939
19.350786	1155.952660	14.522957
19.171349	1165.460527	14.527975
19.032914	1170.866444	14.532992
19.400456	1161.357880	14.538010
19.190649	1163.643417	14.543027
18.953851	1155.498280	14.548045
18.873322	1175.180437	14.553063
19.262821	1195.525713	14.558080
19.409557	1186.793442	14.563098
19.305322	1194.256643	14.568115
19.459672	1184.827460	14.573133
19.657263	1182.884625	14.578151
19.864876	1179.468122	14.583168
19.935908	1181.511888	14.588186
19.809175	1185.125762	14.593203
19.856042	1175.645094	14.598221
19.955203	1166.630562	14.603239
19.641753	1164.319215	14.608256
19.523457	1152.599830	14.613274
19.582110	1159.053786	14.618291
19.779753	1145.876224	14.623309
19.916758	1149.656648	14.628327
19.566833	1149.053657	14.633344
20.059156	1145.907725	14.638362
19.751914	1160.012211	14.643379
20.213986	1143.405526	14.648397
19.647244	1148.053249	14.653415
19.583861	1147.814609	14.658432
20.005481	1146.908272	14.663450
19.738220	1147.619114	14.668467
19.921403	1141.366195	14.673485
19.634473	1147.969101	14.678503
19.678615	1146.442220	14.683520
20.031519	1146.363381	14.688538
19.122017	1155.172077	14.693555
19.559363	1148.610147	14.698573
19.653207	1157.214907	14.703591
19.969071	1180.101026	14.708608
20.075499	1174.103711	14.713626
19.897506	1185.566810	14.718643
20.086115	1174.600898	14.723661
19.986505	1181.112565	14.728679
19.949207	1185.025795	14.733696
19.999620	1190.894136	14.738714
19.868821	1187.278952	14.743731
19.972584	1180.218323	14.748749
20.141087	1184.095507	14.753767
20.131410	1184.413312	14.758784
20.417593	1179.587773	14.763802
20.288838	1177.975742	14.768819
20.290380	1180.105028	14.773837
20.564467	1172.885100	14.778855
20.123825	1181.573654	14.783872
20.165150	1179.213794	14.788890
20.102866	1170.934635	14.793907
20.386917	1179.540194	14.798925
20.219287	1180.082969	14.803943
20.131630	1186.655649	14.808960
20.358500	1175.421203	14.813978
20.204240	1180.254563	14.818995
20.381578	1180.309124	14.824013
20.506667	1170.584410	14.829031
19.978006	1179.378480	14.834048
20.326016	1177.470972	14.839066
20.052076	1181.286383	14.844083
20.299007	1185.881269	14.849101
20.425806	1207.676324	14.854119
20.371118	1213.391215	14.859136
20.822558	1210.663840	14.864154
20.428365	1203.488418	14.869171
20.612606	1209.661370	14.874189
20.833216	1208.550133	14.879207
20.332035	1210.454408	14.884224
20.494709	1211.048785	14.889242
20.524531	1205.397599	14.894259
20.376973	1199.438788	14.899277
20.835697	1208.629203	14.904295
20.619682	1212.028346	14.909312
20.916581	1199.893332	14.914330
20.691307	1198.831520	14.919347
20.678917	1196.566377	14.924365
20.382737	1196.140306	14.929383
20.554522	1201.738953	14.934400
20.856424	1194.138042	14.939418
20.665157	1202.121551	14.944435
20.522741	1206.862015	14.949453
21.001199	1222.177760	14.954471
20.864465	1227.872385	14.959488
21.435047	1230.806643	14.964506
21.188006	1222.237192	14.969523
21.202582	1205.254946	14.974541
21.298666	1206.961504	14.979559
21.118059	1199.111756	14.984576
21.127156	1194.256899	14.989594
21.237138	1193.076976	14.994611
21.162463	1200.382140	14.999629
21.277521	1194.060561	15.004647
20.695793	1194.630569	15.009664
21.135186	1189.435177	15.014682
21.452743	1191.589299	15.019699
21.428006	1193.685537	15.024717
21.446073	1193.092867	15.029735
20.841893	1199.307000	15.034752
21.126431	1191.873921	15.039770
21.048735	1197.061528	15.044787
20.977281	1201.718982	15.049805
21.282379	1203.621632	15.054823
21.177901	1218.783514	15.059840
21.508932	1220.607858	15.064858
21.308016	1231.733457	15.069875
21.594157	1225.697702	15.074893
21.548855	1231.218530	15.079911
21.575631	1232.413745	15.084928
21.509947	1226.096099	15.089946
21.597736	1225.385979	15.094963
21.454159	1232.204547	15.099981
21.542767	1221.964200	15.104999
21.723294	1227.390941	15.110016
21.754744	1221.185162	15.115034
21.623051	1221.154284	15.120051
21.122665	1219.619928	15.125069
21.454211	1222.894546	15.130087
21.651722	1232.873488	15.135104
21.813957	1227.121236	15.140122
21.554023	1234.897239	15.145139
21.450945	1229.766465	15.150157
21.493813	1219.013234	15.155175
21.415016	1227.781656	15.160192
21.515833	1221.679743	15.165210
21.586197	1224.417702	15.170227
21.712045	1225.021722	15.175245
21.643976	1222.954766	15.180263
21.819456	1236.984900	15.185280
22.137108	1243.141679	15.190298
21.804012	1232.653445	15.195315
21.681613	1237.669338	15.200333
22.223274	1238.201748	15.205351
22.161897	1243.211081	15.210368
21.779620	1225.946503	15.215386
21.955946	1233.273897	15.220403
22.173594	1243.029437	15.225421
22.315345	1234.841259	15.230439
21.956022	1238.904674	15.235456
21.895468	1222.902544	15.240474
22.157105	1227.216274	15.245491
22.515281	1248.486076	15.250509
22.431288	1223.682905	15.255527
22.222113	1224.686487	15.260544
22.078783	1224.114635	15.265562
22.147145	1219.685380	15.270579
22.174671	1225.164226	15.275597
22.360054	1217.176308	15.280615
22.269077	1224.953069	15.285632
22.363054	1211.041848	15.290650
22.294703	1215.779499	15.295667
22.030853	1228.849329	15.300685
22.345611	1243.217421	15.305703
22.365594	1253.748990	15.310720
22.552159	1259.272771	15.315738
22.441352	1242.261248	15.320755
22.755504	1247.026907	15.325773
22.973195	1241.734747	15.330791
22.653439	1226.336152	15.335808
22.499407	1209.460952	15.340826
22.585020	1212.049538	15.345843
22.527309	1213.415824	15.350861
22.780291	1196.415369	15.355879
22.750822	1208.869614	15.360896
22.653992	1202.878780	15.365914
22.766499	1198.191440	15.370931
22.430469	1208.726813	15.375949
22.625123	1199.125597	15.380967
22.677278	1216.064251	15.385984
22.889440	1208.628582	15.391002
22.812031	1205.091164	15.396019
22.694366	1212.177867	15.401037
22.827034	1209.143837	15.406055
22.615394	1210.374986	15.411072
22.491883	1227.593915	15.416090
22.824740	1239.407099	15.421107
22.977472	1240.403902	15.426125
22.823997	1234.799593	15.431143
23.131651	1241.761158	15.436160
22.899997	1235.378473	15.441178
23.178297	1234.532478	15.446195
23.094170	1239.899113	15.451213
23.095242	1239.233666	15.456231
22.859690	1235.567313	15.461248
22.784831	1243.470151	15.466266
22.937046	1240.467524	15.471283
22.940731	1242.856694	15.476301
22.723196	1231.340686	15.481319
23.066061	1241.380995	15.486336
22.696594	1238.815532	15.491354
23.034222	1240.849018	15.496371
23.146225	1258.287244	15.501389
23.854480	1256.991321	15.506407
23.391283	1250.745787	15.511424
22.957383	1236.455822	15.516442
23.538725	1245.414543	15.521459
23.246129	1235.088888	15.526477
23.525760	1224.257865	15.531495
23.552747	1228.958868	15.536512
23.390705	1230.595575	15.541530
23.575758	1218.647173	15.546547
23.532907	1235.755120	15.551565
23.375812	1237.548092	15.556583
23.374222	1228.163602	15.561600
23.302748	1230.299080	15.566618
23.586643	1235.640992	15.571635
23.862258	1246.836116	15.576653
23.331799	1240.167875	15.581671
23.385047	1240.466995	15.586688
23.497240	1253.791499	15.591706
23.857756	1258.130596	15.596723
23.720550	1266.768952	15.601741
23.854484	1266.919675	15.606759
23.733720	1257.020660	15.611776
23.581399	1260.825400	15.616794
23.697677	1255.527982	15.621811
23.717019	1265.755340	15.626829
23.768348	1264.818190	15.631847
23.586838	1262.795997	15.636864
23.613256	1262.303120	15.641882
23.767138	1253.907022	15.646899
23.529848	1257.656147	15.651917
23.592174	1252.489315	15.656935
23.631837	1258.069704	15.661952
23.856494	1260.078593	15.666970
24.021858	1274.773415	15.671987
23.669048	1290.005621	15.677005
23.945338	1281.369164	15.682023
24.181835	1282.653275	15.687040
23.656846	1291.286173	15.692058
24.223858	1279.878402	15.697075
24.142421	1282.124983	15.702093
24.050889	1279.263102	15.707111
24.570429	1279.849963	15.712128
24.459720	1279.583331	15.717146
24.371834	1273.746891	15.722163
24.422189	1291.820548	15.727181
24.527045	1278.644065	15.732199
24.453980	1280.319586	15.737216
24.132011	1283.252835	15.742234
24.404022	1274.722994	15.747251
24.418173	1274.964022	15.752269
24.275397	1280.245896	15.757287
24.398227	1270.758890	15.762304
24.572305	1279.585073	15.767322
24.871887	1271.684908	15.772339
24.568420	1288.345526	15.777357
24.478693	1285.299490	15.782375
24.645670	1273.960326	15.787392
24.656316	1269.629588	15.792410
24.858788	1277.197550	15.797427
24.508694	1280.661429	15.802445
24.586648	1273.495979	15.807463
24.555341	1275.662213	15.812480
24.572408	1274.034293	15.817498
24.744213	1272.596888	15.822515
24.833933	1276.933193	15.827533
24.497807	1275.811780	15.832551
24.951710	1273.193828	15.837568
24.566235	1285.312998	15.842586
24.996876	1273.309321	15.847603
24.615241	1278.015404	15.852621
24.610274	1280.443414	15.857639
24.580184	1273.115150	15.862656
24.804198	1283.749958	15.867674
25.056268	1273.556524	15.872691
24.610892	1274.735438	15.877709
24.864228	1274.736078	15.882727
24.689120	1283.096866	15.887744
24.987930	1301.869930	15.892762
25.004523	1304.467598	15.897779
25.194801	1310.428571	15.902797
25.145342	1315.550125	15.907815
25.467324	1320.895209	15.912832
25.233930	1308.853038	15.917850
25.196276	1306.608990	15.922867
25.249248	1319.761471	15.927885
25.168104	1312.955019	15.932903
25.181130	1313.307257	15.937920
24.618668	1322.921950	15.942938
24.699666	1313.056418	15.947955
24.648365	1312.680344	15.952973
24.921445	1320.066954	15.957991
25.298130	1327.010828	15.963008
25.534068	1343.491637	15.968026
25.194686	1346.025424	15.973043
25.136021	1341.185286	15.978061
25.361397	1340.512613	15.983079
25.633088	1336.615788	15.988096
25.743166	1334.975610	15.993114
25.125008	1335.564646	15.998131
25.801454	1334.656261	16.003149
25.930466	1328.557116	16.008167
25.848203	1323.446486	16.013184
25.999767	1327.492256	16.018202
26.201888	1328.900565	16.023219
26.158139	1322.819794	16.028237
25.617940	1315.913373	16.033255
25.836820	1295.116950	16.038272
25.683489	1293.752673	16.043290
25.666433	1286.761214	16.048307
26.029116	1295.475468	16.053325
25.813383	1310.552321	16.058343
26.119837	1317.427507	16.063360
25.952192	1313.204625	16.068378
25.987933	1290.614944	16.073395
25.904121	1303.473138	16.078413
25.826059	1311.443863	16.083431
26.266220	1311.800568	16.088448
26.232543	1318.514757	16.093466
25.875827	1301.719868	16.098483
26.319003	1305.158693	16.103501
26.163043	1307.778242	16.108519
26.161448	1295.533134	16.113536
25.920104	1297.129044	16.118554
26.421452	1307.434486	16.123571
26.441050	1316.957519	16.128589
26.201279	1302.780226	16.133607
26.316579	1289.721293	16.138624
26.085267	1303.535389	16.143642
26.377289	1313.468418	16.148659
26.437982	1319.067394	16.153677
26.208737	1329.112340	16.158695
26.218271	1324.870745	16.163712
26.479542	1324.329923	16.168730
26.606362	1319.003179	16.173747
26.546713	1325.217350	16.178765
26.523398	1330.258597	16.183783
26.732661	1320.846222	16.188800
26.275346	1316.835869	16.193818
26.576511	1318.017938	16.198835
26.694890	1322.928635	16.203853
26.838372	1322.006143	16.208871
26.700047	1316.715037	16.213888
26.434655	1322.865639	16.218906
26.440192	1322.449052	16.223923
26.669487	1323.174526	16.228941
26.707562	1320.322671	16.233959
26.707348	1315.867343	16.238976
26.449716	1325.881554	16.243994
26.835562	1314.487221	16.249011
26.743178	1319.928871	16.254029
26.620509	1322.478343	16.259047
26.635602	1321.929861	16.264064
26.387725	1331.511365	16.269082
26.873085	1338.943147	16.274099
27.104622	1347.750012	16.279117
26.907261	1352.203166	16.284135
26.616775	1347.598653	16.289152
26.772289	1353.312254	16.294170
26.691996	1352.865783	16.299187
27.077163	1350.790295	16.304205
26.784305	1351.372708	16.309223
27.052345	1342.489950	16.314240
27.047834	1350.921343	16.319258
27.076392	1351.012746	16.324275
27.357372	1344.841582	16.329293
27.185310	1361.972638	16.334311
27.604889	1368.015347	16.339328
27.460408	1363.442163	16.344346
27.294767	1343.426660	16.349363
27.398369	1334.703416	16.354381
27.476352	1340.885748	16.359399
27.944529	1344.071628	16.364416
27.522460	1346.907685	16.369434
27.594119	1342.904614	16.374451
27.844974	1340.934042	16.379469
27.509460	1347.163587	16.384487
27.409796	1339.724373	16.389504
27.710301	1342.864789	16.394522
27.652825	1350.250639	16.399539
27.862162	1342.640574	16.404557
27.635125	1345.830551	16.409575
27.768828	1342.190034	16.414592
27.813077	1340.185565	16.419610
27.871370	1347.828223	16.424627
27.839555	1338.330169	16.429645
27.611053	1344.057355	16.434663
27.674104	1339.708078	16.439680
28.078936	1348.648057	16.444698
27.616873	1348.318345	16.449715
28.030210	1354.254210	16.454733
27.671190	1355.291667	16.459751
27.798291	1357.510027	16.464768
27.936060	1364.607652	16.469786
27.773109	1377.179409	16.474803
28.322138	1369.765441	16.479821
28.024433	1373.224207	16.484839
28.324281	1368.118399	16.489856
28.336351	1369.599520	16.494874
28.283154	1372.093796	16.499891
28.483447	1365.435598	16.504909
28.572001	1370.586679	16.509927
28.207722	1353.128429	16.514944
28.067019	1352.395510	16.519962
28.488629	1356.637906	16.524979
28.514207	1358.056160	16.529997
28.313330	1358.590272	16.535015
28.557720	1359.401830	16.540032
28.461641	1354.180093	16.545050
28.201789	1355.122784	16.550067
28.364406	1350.394817	16.555085
28.502822	1363.844600	16.560103
28.163912	1365.972019	16.565120
28.169934	1365.777000	16.570138
27.907989	1373.397502	16.575155
27.942469	1362.603041	16.580173
28.162993	1375.027047	16.585191
28.504516	1381.697245	16.590208
28.402612	1399.328529	16.595226
28.462517	1403.572959	16.600243
28.814225	1393.536173	16.605261
28.847960	1403.636831	16.610279
28.897377	1401.773623	16.615296
28.875150	1391.775923	16.620314
28.697724	1399.179690	16.625331
29.000059	1402.420602	16.630349
29.013161	1401.062613	16.635367
28.828353	1401.478319	16.640384
28.817035	1393.762249	16.645402
28.647056	1400.084875	16.650419
28.894259	1392.490956	16.655437
28.581126	1399.875462	16.660455
29.097529	1405.555701	16.665472
29.283852	1422.615669	16.670490
29.193792	1428.678619	16.675507
29.483662	1414.463128	16.680525
28.996684	1408.200208	16.685543
28.981412	1398.504498	16.690560
29.308641	1409.618753	16.695578
28.890038	1439.397663	16.700595
29.232476	1423.960478	16.705613
29.155212	1423.387916	16.710631
29.252536	1426.091132	16.715648
29.383243	1429.543145	16.720666
29.692436	1432.915603	16.725683
29.838237	1417.324767	16.730701
29.794059	1422.732487	16.735719
29.802058	1418.904896	16.740736
29.933616	1420.110333	16.745754
29.825110	1412.675304	16.750771
29.484882	1396.073250	16.755789
29.612517	1394.616376	16.760807
29.768701	1407.927036	16.765824
29.793739	1395.498308	16.770842
29.558429	1400.059333	16.775859
29.686069	1394.767860	16.780877
29.457995	1415.146792	16.785895
29.273381	1419.094317	16.790912
29.807213	1417.178847	16.795930
29.325416	1424.744047	16.800947
29.501473	1415.914274	16.805965
29.348531	1422.564005	16.810983
30.015822	1432.363319	16.816000
30.040525	1459.656289	16.821018
30.013530	1460.070274	16.826035
30.376663	1442.930839	16.831053
30.120588	1447.710669	16.836071
30.083486	1443.990540	16.841088
30.433068	1441.325268	16.846106
30.273595	1432.682539	16.851123
30.129357	1415.304710	16.856141
30.018010	1426.520734	16.861159
30.125233	1435.585633	16.866176
30.359292	1441.534289	16.871194
30.263767	1453.963448	16.876211
30.449598	1455.829975	16.881229
30.273384	1452.787597	16.886247
30.369023	1449.116745	16.891264
30.469820	1440.182885	16.896282
30.270158	1451.305677	16.901299
30.180157	1448.670674	16.906317
30.299248	1438.160965	16.911335
30.405299	1442.306820	16.916352
30.464111	1441.193225	16.921370
30.269098	1442.085027	16.926387
30.325527	1440.437187	16.931405
30.260579	1435.868135	16.936423
30.441338	1448.608624	16.941440
30.835333	1458.357540	16.946458
30.497732	1466.145732	16.951475
30.392571	1465.119129	16.956493
30.761488	1470.460825	16.961511
30.537936	1465.812909	16.966528
31.114266	1463.914806	16.971546
30.987185	1471.868533	16.976563
31.127478	1464.944246	16.981581
31.250331	1471.371166	16.986599
30.875524	1473.362418	16.991616
31.047409	1461.928605	16.996634
30.977787	1476.555837	17.001651
31.049339	1475.268872	17.006669
31.031240	1472.726288	17.011687
30.920004	1473.251467	17.016704
31.182364	1470.752600	17.021722
31.239894	1472.219904	17.026739
31.479558	1469.359445	17.031757
31.365519	1467.116998	17.036775
30.982065	1466.906943	17.041792
31.297702	1459.882758	17.046810
31.231243	1470.355953	17.051827
31.179054	1458.887592	17.056845
31.311296	1462.885810	17.061863
31.223299	1460.720154	17.066880
31.517791	1463.736395	17.071898
31.545632	1470.973137	17.076915
31.646329	1471.117161	17.081933
31.230959	1479.092645	17.086951
31.696740	1488.156076	17.091968
31.962183	1483.220493	17.096986
31.780901	1477.650620	17.102003
31.886687	1471.998176	17.107021
31.839174	1457.271587	17.112039
31.909801	1452.285990	17.117056
32.027118	1462.000015	17.122074
31.676128	1450.220511	17.127091
32.102206	1455.996827	17.132109
32.017776	1447.468828	17.137127
31.896771	1457.693175	17.142144
32.159059	1450.523498	17.147162
31.789994	1452.101595	17.152179
31.971676	1448.781847	17.157197
32.217347	1449.572332	17.162215
32.149072	1443.668014	17.167232
32.073377	1439.759002	17.172250
31.975476	1446.540180	17.177267
32.057416	1454.701805	17.182285
32.168722	1451.844886	17.187303
31.972151	1463.063237	17.192320
32.203856	1470.669761	17.197338
32.097290	1481.333462	17.202355
32.182512	1483.246572	17.207373
32.668404	1484.159485	17.212391
32.322001	1489.339321	17.217408
32.388538	1475.884766	17.222426
32.420260	1478.197677	17.227443
32.547820	1477.813635	17.232461
32.868457	1479.477135	17.237479
32.587265	1480.540688	17.242496
32.668131	1474.070328	17.247514
32.800807	1473.586228	17.252531
33.040880	1467.559190	17.257549
32.969483	1440.877221	17.262567
32.560209	1442.480479	17.267584
32.577216	1440.945858	17.272602
32.672318	1438.091625	17.277619
32.671176	1449.707129	17.282637
32.909182	1458.606687	17.287655
32.784226	1463.021112	17.292672
33.002425	1466.542896	17.297690
33.024610	1466.088903	17.302707
32.681846	1466.072502	17.307725
32.877536	1462.570905	17.312743
32.553866	1472.519768	17.317760
33.164741	1469.621463	17.322778
32.924971	1465.630558	17.327795
32.723414	1463.998269	17.332813
33.164031	1459.226599	17.337831
32.865665	1464.631542	17.342848
32.882872	1466.300402	17.347866
33.109240	1470.515711	17.352883
33.266370	1475.065713	17.357901
33.167030	1493.909663	17.362919
33.262815	1500.542258	17.367936
33.144520	1503.791031	17.372954
33.109520	1501.349273	17.377971
33.033107	1505.222210	17.382989
33.505104	1496.267797	17.388007
33.027843	1502.681897	17.393024
33.021558	1495.948008	17.398042
33.190763	1513.446342	17.403059
33.339141	1517.546625	17.408077
33.638977	1537.341061	17.413095
33.901700	1533.980317	17.418112
33.718856	1532.687046	17.423130
34.090379	1533.772837	17.428147
34.154019	1532.040328	17.433165
34.192243	1514.619576	17.438183
33.725168	1508.786387	17.443200
33.513780	1500.367176	17.448218
33.948013	1509.098444	17.453235
34.022575	1525.251840	17.458253
34.195090	1523.070597	17.463271
33.764247	1530.887253	17.468288
33.991605	1522.765063	17.473306
33.830374	1526.984332	17.478323
33.653791	1528.320329	17.483341
33.889625	1525.847107	17.488359
33.863147	1524.839754	17.493376
34.346886	1519.138882	17.498394
34.177440	1516.994579	17.503411
34.058741	1512.882828	17.508429
34.421219	1525.124002	17.513447
34.062280	1525.380356	17.518464
34.129325	1523.270908	17.523482
34.291389	1535.650787	17.528499
34.081196	1544.231697	17.533517
34.785200	1542.749844	17.538535
34.596236	1541.164280	17.543552
34.524413	1551.473064	17.548570
34.548559	1536.889257	17.553587
34.622461	1540.969990	17.558605
34.994681	1532.713572	17.563623
34.880525	1536.065210	17.568640
34.635416	1534.740123	17.573658
34.837322	1532.663461	17.578675
34.805305	1526.019645	17.583693
35.234097	1527.695163	17.588711
35.059134	1513.822298	17.593728
34.822682	1502.249377	17.598746
35.131214	1498.031060	17.603763
34.978645	1505.701626	17.608781
35.004765	1485.577020	17.613799
35.139582	1484.720914	17.618816
34.955583	1492.828958	17.623834
35.294747	1483.646155	17.628851
35.037508	1490.177360	17.633869
35.330597	1491.184010	17.638887
35.001141	1491.720126	17.643904
34.884364	1495.217070	17.648922
35.144698	1496.435442	17.653939
35.182689	1524.002702	17.658957
35.743050	1523.367073	17.663975
35.539952	1528.847601	17.668992
35.227510	1516.038439	17.674010
35.501172	1511.410540	17.679027
35.303751	1528.693616	17.684045
35.583575	1523.976111	17.689063
35.630759	1522.629791	17.694080
35.302425	1522.101947	17.699098
35.543994	1522.102961	17.704115
35.328675	1536.854376	17.709133
35.216447	1526.763224	17.714151
35.346478	1534.115357	17.719168
35.297124	1532.059040	17.724186
35.182797	1537.582745	17.729203
35.507857	1541.799843	17.734221
35.820116	1551.704085	17.739239
35.933501	1555.901905	17.744256
35.854981	1553.402384	17.749274
35.858266	1555.122379	17.754291
35.572724	1561.812630	17.759309
35.841820	1561.872866	17.764327
36.002362	1554.880225	17.769344
36.042633	1550.297654	17.774362
36.208622	1557.050931	17.779379
36.178098	1561.217858	17.784397
35.864506	1555.249788	17.789415
36.077695	1556.167311	17.794432
36.370045	1561.484709	17.799450
36.568663	1570.132586	17.804467
36.321330	1570.577941	17.809485
36.416494	1562.533131	17.814503
36.332877	1565.523026	17.819520
36.166575	1577.739989	17.824538
36.407354	1573.837201	17.829555
36.230870	1582.671212	17.834573
36.483651	1574.612895	17.839591
36.596419	1573.371459	17.844608
36.692511	1583.048130	17.849626
36.883163	1579.854822	17.854643
36.746147	1576.392149	17.859661
36.704117	1571.209814	17.864679
36.786891	1577.155227	17.869696
36.429878	1589.469132	17.874714
36.786636	1580.096352	17.879731
36.494699	1584.677437	17.884749
36.870257	1573.919264	17.889767
36.702526	1583.200645	17.894784
36.633347	1582.488154	17.899802
37.114938	1595.994700	17.904819
36.693313	1614.064996	17.909837
36.660365	1627.960706	17.914855
37.449806	1618.200902	17.919872
36.974388	1621.169464	17.924890
37.028718	1608.038863	17.929907
37.211476	1615.212224	17.934925
37.233366	1606.597634	17.939943
37.416409	1606.005977	17.944960
37.439798	1617.438805	17.949978
37.345252	1619.451384	17.954995
37.304578	1614.764480	17.960013
37.332329	1609.065852	17.965031
37.732470	1603.468950	17.970048
37.446459	1603.532128	17.975066
37.604240	1606.783634	17.980083
37.391725	1607.716138	17.985101
37.529178	1607.971007	17.990119
37.700656	1598.121415	17.995136
37.321858	1608.688154	18.000154
37.719501	1599.861742	18.005171
37.691675	1618.112111	18.010189
37.630571	1624.613257	18.015207
37.754425	1625.386522	18.020224
37.784222	1636.674995	18.025242
37.809488	1635.061034	18.030259
38.057393	1628.973581	18.035277
38.065448	1640.683768	18.040295
38.317331	1628.888553	18.045312
38.183004	1631.873078	18.050330
38.256988	1625.629386	18.055347
37.843994	1636.038813	18.060365
38.016926	1635.144104	18.065383
38.169969	1628.677083	18.070400
37.904469	1633.370734	18.075418
38.104480	1621.417578	18.080435
38.069559	1625.550211	18.085453
38.063918	1627.403187	18.090471
38.266541	1637.637845	18.095488
38.296206	1652.633056	18.100506
38.686104	1654.269752	18.105523
38.584197	1654.042995	18.110541
38.916714	1656.536441	18.115559
39.086753	1654.926459	18.120576
38.652631	1649.200358	18.125594
38.714165	1639.503591	18.130611
38.970388	1635.481300	18.135629
38.739474	1635.915277	18.140647
38.923410	1626.001005	18.145664
38.914217	1627.498270	18.150682
39.011848	1631.975886	18.155699
38.834679	1631.323401	18.160717
38.569779	1634.149626	18.165735
39.099590	1644.428142	18.170752
39.038864	1649.718208	18.175770
39.195799	1642.775338	18.180787
39.050314	1644.171156	18.185805
38.844071	1647.077434	18.190823
38.997814	1640.507142	18.195840
38.655801	1639.652817	18.200858
38.701907	1635.794847	18.205875
38.863938	1642.174013	18.210893
39.161040	1663.893086	18.215911
39.330287	1669.859649	18.220928
39.516278	1677.876603	18.225946
39.577413	1667.828308	18.230963
39.512206	1670.021863	18.235981
39.278608	1671.651173	18.240999
39.863474	1675.993398	18.246016
39.515917	1674.928965	18.251034
39.780638	1665.366648	18.256051
39.882811	1668.384067	18.261069
39.728688	1667.882489	18.266087
39.727979	1667.683463	18.271104
39.857648	1669.850656	18.276122
40.048294	1667.627020	18.281139
39.634030	1668.475217	18.286157
39.706683	1669.990037	18.291175
39.884590	1661.879900	18.296192
39.824748	1662.002478	18.301210
40.072634	1668.383974	18.306227
40.222192	1656.995446	18.311245
39.836018	1657.369698	18.316263
40.037652	1666.234847	18.321280
40.190995	1665.054402	18.326298
40.014356	1661.364018	18.331315
39.998631	1661.598189	18.336333
40.071501	1671.711046	18.341351
40.478988	1678.906675	18.346368
40.158004	1693.053289	18.351386
40.451453	1689.065766	18.356403
40.711029	1697.822913	18.361421
40.798924	1696.329679	18.366439
41.113203	1690.116251	18.371456
40.577245	1678.304994	18.376474
40.564832	1667.782654	18.381491
40.452395	1673.306095	18.386509
40.665645	1681.471687	18.391527
40.870659	1690.320936	18.396544
40.798298	1696.658227	18.401562
40.873555	1690.082406	18.406579
41.100388	1690.741377	18.411597
40.999866	1687.776183	18.416615
41.270489	1684.897173	18.421632
40.825164	1677.963066	18.426650
41.092188	1684.363841	18.431667
41.052240	1682.720909	18.436685
40.826088	1694.744723	18.441703
40.932723	1683.669979	18.446720
40.865777	1681.483877	18.451738
40.785158	1687.579616	18.456755
40.932488	1687.221824	18.461773
40.953375	1688.416475	18.466791
41.116218	1686.234842	18.471808
41.254984	1702.996694	18.476826
41.580769	1703.901094	18.481843
41.651712	1708.007164	18.486861
41.272878	1710.645179	18.491879
41.626394	1704.604778	18.496896
41.327955	1703.720399	18.501914
41.828659	1702.637947	18.506931
41.520790	1704.243337	18.511949
41.479028	1703.116062	18.516967
41.970348	1691.382728	18.521984
41.716520	1704.209169	18.527002
41.824869	1709.986617	18.532019
41.874614	1711.776496	18.537037
41.890762	1701.978542	18.542055
41.862048	1707.226713	18.547072
41.838653	1702.503063	18.552090
41.811761	1706.265487	18.557107
41.990328	1714.375029	18.562125
41.883177	1724.642139	18.567143
42.305858	1728.590366	18.572160
42.344427	1732.329359	18.577178
42.331463	1730.930382	18.582195
42.315678	1739.863858	18.587213
41.982927	1743.458824	18.592231
42.187002	1728.862367	18.597248
42.296529	1729.349424	18.602266
42.203126	1731.538208	18.607283
42.045082	1732.510519	18.612301
42.103645	1736.563922	18.617319
42.416035	1739.272921	18.622336
42.358987	1750.784914	18.627354
42.471165	1759.051537	18.632371
42.991337	1760.041077	18.637389
42.404260	1765.095105	18.642407
42.560240	1752.588897	18.647424
42.769739	1754.964539	18.652442
42.717241	1753.842975	18.657459
43.083481	1747.659110	18.662477
42.823617	1758.467676	18.667495
43.026064	1763.558296	18.672512
43.110825	1759.800589	18.677530
42.865144	1764.425643	18.682547
43.179752	1758.674737	18.687565
42.794557	1762.017759	18.692583
43.167129	1764.096318	18.697600
43.199167	1778.367628	18.702618
43.120054	1786.006876	18.707635
43.205265	1791.451174	18.712653
43.345011	1789.514694	18.717671
43.577487	1784.817155	18.722688
43.924899	1788.988887	18.727706
43.897968	1780.057084	18.732723
43.942125	1775.966722	18.737741
43.453361	1759.272728	18.742759
43.765153	1760.660162	18.747776
43.871304	1780.610604	18.752794
43.943275	1771.682902	18.757811
44.185036	1748.773004	18.762829
43.506859	1749.010961	18.767847
43.574116	1748.818396	18.772864
43.858127	1755.632534	18.777882
44.147600	1779.678649	18.782899
44.137677	1767.295176	18.787917
44.032223	1780.727827	18.792935
44.152161	1778.514310	18.797952
44.180916	1766.831922	18.802970
44.240181	1769.821819	18.807987
44.175587	1770.766848	18.813005
44.000873	1771.166718	18.818023
44.307727	1773.980973	18.823040
44.063933	1765.540210	18.828058
44.076743	1773.554393	18.833075
44.448151	1765.920829	18.838093
44.191507	1769.935488	18.843111
44.430438	1773.951948	18.848128
44.613479	1771.143330	18.853146
44.258241	1773.729023	18.858163
44.150294	1780.418308	18.863181
44.284115	1802.126028	18.868199
44.582153	1794.065617	18.873216
44.765680	1791.158095	18.878234
44.789437	1791.193602	18.883251
45.039716	1796.830257	18.888269
44.834722	1794.963458	18.893287
44.835267	1798.283955	18.898304
45.067577	1794.797481	18.903322
44.950951	1794.867256	18.908339
45.574205	1789.221534	18.913357
44.841877	1794.018516	18.918375
44.905333	1797.035678	18.923392
44.873525	1798.681195	18.928410
45.221520	1815.047100	18.933427
44.964842	1821.342520	18.938445
45.351648	1819.396623	18.943463
45.570791	1819.600174	18.948480
45.153243	1825.085212	18.953498
44.835850	1830.589889	18.958515
45.614928	1816.821381	18.963533
45.560914	1828.199069	18.968551
45.293781	1810.798232	18.973568
45.649551	1810.601202	18.978586
45.797841	1819.955200	18.983603
45.840567	1815.801284	18.988621
45.860692	1814.325953	18.993639
45.271296	1824.154076	18.998656
45.441272	1825.518541	19.003674
45.623996	1839.451565	19.008691
45.830812	1846.216713	19.013709
45.994079	1852.964272	19.018727
46.032931	1852.768142	19.023744
46.112818	1846.513934	19.028762
46.102093	1843.636205	19.033779
46.250133	1841.570390	19.038797
46.306573	1844.058793	19.043815
46.366874	1852.814773	19.048832
46.131165	1839.772160	19.053850
46.186128	1846.411269	19.058867
46.380663	1842.132601	19.063885
46.425700	1847.550106	19.068903
46.546063	1860.956065	19.073920
46.703711	1866.334850	19.078938
46.408496	1873.942601	19.083955
46.541363	1869.998158	19.088973
46.638403	1877.609858	19.093991
46.765029	1869.411647	19.099008
46.751089	1863.113519	19.104026
46.751330	1871.359365	19.109043
47.088464	1868.477183	19.114061
47.121489	1869.457235	19.119079
46.930048	1870.964228	19.124096
46.976097	1861.139176	19.129114
47.026103	1865.405450	19.134131
46.998745	1859.989482	19.139149
47.067179	1867.581111	19.144167
46.788962	1860.275151	19.149184
47.056311	1864.283779	19.154202
47.113098	1883.465742	19.159219
47.195034	1883.672328	19.164237
47.291193	1888.794762	19.169255
47.344249	1888.759669	19.174272
47.837155	1887.402113	19.179290
47.332423	1896.797750	19.184307
47.577162	1893.614714	19.189325
47.661719	1888.575882	19.194343
47.957924	1892.230521	19.199360
47.904128	1882.869634	19.204378
47.776767	1887.721593	19.209395
47.781345	1881.425904	19.214413
47.685558	1888.817959	19.219431
47.759447	1891.015286	19.224448
47.819590	1878.327991	19.229466
48.016754	1885.054596	19.234483
48.180787	1880.123869	19.239501
47.729453	1880.990026	19.244519
48.079799	1893.803197	19.249536
48.516593	1907.001679	19.254554
48.620238	1907.158607	19.259571
48.549252	1885.899932	19.264589
48.504023	1880.777473	19.269607
48.765044	1865.362782	19.274624
48.994292	1877.364875	19.279642
48.490083	1871.295564	19.284659
48.565274	1867.057517	19.289677
48.274662	1871.832170	19.294695
48.394177	1870.901804	19.299712
48.365506	1865.879366	19.304730
48.184139	1878.267172	19.309747
48.838337	1892.712739	19.314765
48.355646	1900.595251	19.319783
48.603928	1906.713389	19.324800
48.715679	1901.603907	19.329818
48.967489	1897.914965	19.334835
49.121195	1896.196243	19.339853
49.032812	1901.296482	19.344871
48.514700	1902.263856	19.349888
49.144009	1907.550384	19.354906
48.752867	1918.608756	19.359923
48.956482	1923.215761	19.364941
49.147537	1927.082705	19.369959
49.167463	1937.388364	19.374976
49.317528	1935.447795	19.379994
49.018054	1943.444876	19.385011
49.224409	1939.754395	19.390029
49.573093	1931.177248	19.395047
49.401126	1936.335434	19.400064
49.799367	1942.268516	19.405082
49.652235	1959.219326	19.410099
49.875782	1963.599021	19.415117
50.178511	1961.200090	19.420135
50.267775	1954.132456	19.425152
50.115826	1934.698974	19.430170
50.172997	1929.704822	19.435187
50.147604	1919.397457	19.440205
50.297554	1924.647614	19.445223
49.635464	1929.487338	19.450240
50.171816	1926.721768	19.455258
50.140592	1928.436888	19.460275
50.053053	1932.576740	19.465293
50.019908	1951.870531	19.470311
50.008430	1965.118485	19.475328
50.339301	1959.299457	19.480346
50.320373	1962.790934	19.485363
50.124551	1961.684425	19.490381
50.495861	1951.668053	19.495399
50.607794	1960.314754	19.500416
50.562872	1956.639104	19.505434
50.476599	1959.496833	19.510451
50.379771	1969.102144	19.515469
50.837707	1976.422633	19.520487
50.454973	1983.980753	19.525504
50.681699	1982.908216	19.530522
51.136650	1980.722665	19.535539
50.886100	1987.286828	19.540557
50.882953	1986.318103	19.545575
50.902565	1994.229696	19.550592
50.818193	1975.077502	19.555610
50.802372	1999.688695	19.560627
50.993039	2011.480345	19.565645
51.462191	2018.072205	19.570663
51.302368	2023.639444	19.575680
51.315815	2010.281408	19.580698
51.737517	2013.518435	19.585715
51.724360	2011.772211	19.590733
51.918169	2011.153953	19.595751
52.076244	2008.877788	19.600768
51.887453	2000.942370	19.605786
52.154288	1991.073984	19.610803
51.865969	1980.249864	19.615821
51.884158	1975.331839	19.620839
51.630215	1973.960536	19.625856
51.838257	1971.227666	19.630874
51.842921	1977.236562	19.635891
51.642292	1976.396208	19.640909
51.860400	1994.760632	19.645927
51.979185	2006.099208	19.650944
52.226519	2004.096854	19.655962
52.123585	2007.327834	19.660979
51.948288	2006.047445	19.665997
52.396605	1990.961864	19.671015
52.411393	2006.502020	19.676032
52.591808	2000.669700	19.681050
52.529502	2002.606910	19.686067
52.277533	2012.910394	19.691085
52.451820	2003.928215	19.696103
52.088749	2009.749187	19.701120
52.330650	2008.644607	19.706138
52.678738	2024.893787	19.711155
52.525587	2029.278000	19.716173
52.740928	2039.083247	19.721191
52.678272	2046.332485	19.726208
52.828305	2035.836542	19.731226
52.907869	2031.988288	19.736243
53.080771	2037.859504	19.741261
53.081726	2030.038720	19.746279
52.866741	2033.728429	19.751296
52.697236	2035.469213	19.756314
52.960668	2048.934718	19.761331
52.979797	2066.189227	19.766349
53.327728	2066.415159	19.771367
53.039394	2065.813739	19.776384
53.015511	2065.333103	19.781402
53.439661	2059.445836	19.786419
53.103420	2054.903411	19.791437
53.550977	2066.481696	19.796455
53.677658	2073.511795	19.801472
53.962478	2081.677560	19.806490
53.930344	2078.392690	19.811507
53.944639	2081.607030	19.816525
54.182285	2078.664115	19.821543
54.134864	2075.902659	19.826560
53.890319	2080.056736	19.831578
54.723116	2075.834530	19.836595
54.239880	2077.819005	19.841613
54.360742	2066.563281	19.846631
53.980549	2057.506341	19.851648
54.253636	2066.231145	19.856666
54.367305	2072.570463	19.861683
54.112284	2078.248763	19.866701
54.372795	2077.968682	19.871719
54.086251	2082.622643	19.876736
54.253601	2074.268757	19.881754
54.326595	2082.927091	19.886771
53.973648	2077.866937	19.891789
54.481038	2082.652832	19.896807
54.573618	2102.450812	19.901824
54.380825	2100.574868	19.906842
54.602173	2099.048474	19.911859
54.571643	2108.001926	19.916877
55.037053	2093.174055	19.921895
54.629315	2095.237766	19.926912
54.516259	2113.484718	19.931930
55.163974	2120.891180	19.936947
54.692720	2124.489874	19.941965
54.707368	2127.488409	19.946983
55.056091	2134.492400	19.952000
55.223121	2137.146797	19.957018
55.441543	2132.084934	19.962035
55.428660	2154.158395	19.967053
56.181453	2147.763906	19.972071
56.056353	2138.022138	19.977088
55.714713	2116.779615	19.982106
56.187124	2120.047639	19.987123
55.418940	2123.300603	19.992141
55.586880	2114.372956	19.997159
55.568984	2114.705922	20.002176
55.593230	2121.018727	20.007194
55.865230	2123.103753	20.012211
56.022763	2143.018200	20.017229
56.345841	2139.458744	20.022247
55.671639	2132.960768	20.027264
55.949591	2144.203402	20.032282
56.303619	2154.014498	20.037299
56.316753	2149.422070	20.042317
56.381500	2147.938531	20.047335
56.389996	2152.925564	20.052352
56.328185	2149.326683	20.057370
56.576304	2147.739550	20.062387
56.309601	2160.271242	20.067405
56.238715	2143.956869	20.072423
56.411771	2152.469929	20.077440
56.338013	2154.855920	20.082458
56.757459	2162.166336	20.087475
56.585014	2174.095796	20.092493
56.655337	2170.541963	20.097511
56.609308	2178.425541	20.102528
56.697184	2185.582987	20.107546
56.726743	2176.193948	20.112563
56.586906	2188.140461	20.117581
56.731620	2204.521539	20.122599
57.214600	2212.505344	20.127616
57.188853	2216.444087	20.132634
57.334853	2210.468563	20.137651
57.389713	2221.096985	20.142669
57.335712	2211.404031	20.147687
57.370154	2213.110277	20.152704
57.349956	2209.596228	20.157722
58.061445	2204.893268	20.162739
57.618758	2211.432250	20.167757
57.816970	2206.066610	20.172775
57.918357	2203.276161	20.177792
57.783835	2210.039324	20.182810
57.969633	2213.598143	20.187827
57.973840	2224.444805	20.192845
58.188799	2232.925774	20.197863
58.001110	2230.961564	20.202880
58.249455	2237.006985	20.207898
58.676923	2232.170723	20.212915
58.392822	2235.344736	20.217933
58.687985	2229.444903	20.222951
58.283646	2217.737034	20.227968
58.545923	2209.369327	20.232986
58.720503	2219.084188	20.238003
58.620373	2215.509748	20.243021
58.436822	2213.333428	20.248039
58.510405	2225.249357	20.253056
58.448755	2231.928412	20.258074
58.967460	2219.271609	20.263091
58.768087	2224.168274	20.268109
58.579002	2228.144696	20.273127
58.820258	2221.654949	20.278144
58.755977	2222.434986	20.283162
59.021814	2219.835816	20.288179
59.202886	2223.541883	20.293197
59.195501	2223.253794	20.298215
58.930602	2219.334967	20.303232
59.124538	2237.667852	20.308250
59.727506	2239.560292	20.313267
59.378727	2250.488650	20.318285
59.021047	2247.799796	20.323303
59.416838	2249.190298	20.328320
59.278284	2255.044661	20.333338
59.379081	2244.222858	20.338355
59.404346	2256.644075	20.343373
59.537557	2246.134240	20.348391
59.566890	2245.697939	20.353408
59.358530	2271.224551	20.358426
60.025022	2271.256395	20.363443
60.004557	2280.902011	20.368461
60.237455	2270.496132	20.373479
60.393666	2273.926787	20.378496
60.184351	2269.330210	20.383514
60.363335	2262.490505	20.388531
60.319611	2267.836236	20.393549
60.189893	2269.232254	20.398567
60.378604	2271.569685	20.403584
60.099592	2267.984692	20.408602
60.493677	2267.498232	20.413619
60.499460	2267.348912	20.418637
60.360622	2270.763852	20.423655
60.506695	2275.842321	20.428672
60.462886	2299.173526	20.433690
60.829695	2293.781122	20.438707
60.954351	2307.395427	20.443725
60.824903	2295.943177	20.448743
60.832442	2295.683719	20.453760
60.589756	2307.530419	20.458778
61.140032	2288.183773	20.463795
61.108552	2293.154240	20.468813
60.850264	2298.665042	20.473831
61.457464	2303.083676	20.478848
61.241774	2323.450721	20.483866
61.451216	2316.699654	20.488883
61.518630	2320.425745	20.493901
61.225640	2317.290714	20.498919
61.745223	2314.796766	20.503936
61.552195	2325.381261	20.508954
61.623902	2326.109650	20.513971
61.942329	2324.511253	20.518989
61.792195	2312.513965	20.524007
61.822632	2323.477619	20.529024
61.844335	2327.586495	20.534042
62.192587	2338.516435	20.539059
62.068413	2352.235762	20.544077
61.954547	2357.352574	20.549095
62.380156	2354.389904	20.554112
62.510475	2356.555905	20.559130
62.271542	2348.043543	20.564147
62.094786	2351.510056	20.569165
62.208257	2361.027241	20.574183
62.520357	2345.420145	20.579200
62.227183	2352.764391	20.584218
62.372208	2347.316954	20.589235
62.622580	2366.244219	20.594253
62.675476	2371.241687	20.599271
62.756572	2356.789028	20.604288
62.590788	2362.125472	20.609306
62.798213	2364.492891	20.614323
62.954741	2362.024796	20.619341
62.974788	2373.744968	20.624359
63.014234	2362.130839	20.629376
62.723819	2379.324345	20.634394
63.470840	2391.611595	20.639411
63.503978	2395.294951	20.644429
63.274052	2394.816923	20.649447
63.429382	2396.716964	20.654464
63.618441	2405.547610	20.659482
63.881512	2400.134548	20.664499
64.083456	2393.270118	20.669517
63.833355	2398.805978	20.674535
63.936378	2395.456140	20.679552
63.786211	2393.391596	20.684570
63.645814	2396.293408	20.689587
64.075954	2395.719868	20.694605
63.593320	2393.883217	20.699623
64.023207	2388.272452	20.704640
64.031296	2384.309168	20.709658
64.034727	2380.388391	20.714675
64.257533	2383.369046	20.719693
64.099017	2390.127991	20.724711
64.267716	2401.746401	20.729728
64.222824	2419.066235	20.734746
64.263772	2412.191050	20.739763
64.310548	2411.475070	20.744781
63.966077	2427.341288	20.749799
64.640452	2418.007154	20.754816
64.523817	2432.100521	20.759834
64.562121	2454.424213	20.764851
64.807676	2450.361748	20.769869
65.082429	2454.038578	20.774887
65.324362	2459.929629	20.779904
64.963774	2453.337459	20.784922
65.022854	2451.515835	20.789939
65.262474	2452.302653	20.794957
65.262750	2457.945117	20.799975
65.518517	2445.745864	20.804992
65.437374	2456.126873	20.810010
65.318714	2449.370624	20.815027
65.650845	2455.399896	20.820045
65.674578	2463.767764	20.825063
65.629825	2467.801455	20.830080
65.777154	2467.477507	20.835098
66.095303	2460.571364	20.840115
65.951176	2461.469363	20.845133
65.811205	2471.057715	20.850151
66.146324	2463.952292	20.855168
65.787259	2470.673215	20.860186
65.769237	2463.542402	20.865203
66.206879	2457.669684	20.870221
66.294881	2464.007113	20.875239
65.997404	2458.409665	20.880256
66.178340	2476.682778	20.885274
66.072118	2487.113631	20.890291
66.408299	2486.690299	20.895309
66.852303	2487.761799	20.900327
66.707417	2482.156402	20.905344
66.755415	2488.198872	20.910362
66.638867	2487.170542	20.915379
66.646875	2489.389099	20.920397
66.971330	2503.544149	20.925415
66.974647	2510.956705	20.930432
67.096878	2515.179701	20.935450
67.454222	2512.986224	20.940467
67.670698	2502.924662	20.945485
67.117668	2515.575311	20.950503
67.542184	2513.012029	20.955520
67.549112	2511.447080	20.960538
67.717868	2510.867206	20.965555
67.944557	2509.247758	20.970573
67.717856	2505.788308	20.975591
67.740109	2502.048647	20.980608
67.695928	2509.041483	20.985626
67.441589	2506.003169	20.990643
67.531255	2507.587699	20.995661
67.542437	2509.142703	21.000679
67.668496	2498.318116	21.005696
67.550634	2515.860781	21.010714
67.474661	2520.638676	21.015731
67.646497	2530.061255	21.020749
67.716669	2539.179789	21.025767
67.957768	2538.369025	21.030784
68.217727	2557.452032	21.035802
68.205220	2566.201176	21.040819
68.661568	2567.391119	21.045837
68.469709	2559.928786	21.050855
68.481178	2563.600415	21.055872
68.995276	2566.580908	21.060890
68.752093	2574.698525	21.065907
68.869124	2560.014910	21.070925
68.488900	2571.043191	21.075943
69.014496	2581.476192	21.080960
69.536465	2593.261069	21.085978
69.260047	2604.856082	21.090995
69.649876	2594.907105	21.096013
69.096491	2585.762383	21.101031
69.475547	2592.455635	21.106048
69.845633	2592.011332	21.111066
69.612064	2594.808127	21.116083
69.631318	2594.019132	21.121101
69.364547	2591.315164	21.126119
69.724691	2595.411382	21.131136
69.779543	2586.287610	21.136154
69.706917	2586.630829	21.141171
70.064917	2583.134001	21.146189
69.765076	2590.356618	21.151207
69.465944	2586.619754	21.156224
69.917485	2598.606073	21.161242
69.888881	2617.712916	21.166259
70.068033	2614.778407	21.171277
69.900734	2623.993399	21.176295
70.198872	2617.763380	21.181312
70.313154	2603.736916	21.186330
70.199374	2633.270374	21.191347
70.843795	2633.961828	21.196365
70.592689	2637.497017	21.201383
70.888896	2639.615905	21.206400
70.955535	2644.202495	21.211418
70.802111	2642.599119	21.216435
71.317400	2636.770174	21.221453
71.234923	2654.909146	21.226471
71.047718	2631.141358	21.231488
71.383135	2638.587182	21.236506
71.062795	2635.089660	21.241523
70.706075	2633.777836	21.246541
70.884893	2645.382154	21.251559
70.881156	2664.759759	21.256576
71.552797	2664.393485	21.261594
71.737776	2668.578967	21.266611
71.750650	2664.063207	21.271629
71.687540	2664.337524	21.276647
71.830947	2665.180051	21.281664
72.132241	2657.999034	21.286682
72.016708	2662.761473	21.291699
72.220881	2658.912513	21.296717
71.946608	2668.844899	21.301735
72.113492	2675.892632	21.306752
72.425799	2677.855699	21.311770
72.092391	2696.069340	21.316787
72.147108	2684.279990	21.321805
72.495028	2688.410937	21.326823
72.588405	2691.073687	21.331840
72.536909	2685.550398	21.336858
72.438373	2695.810421	21.341875
72.613877	2685.971288	21.346893
72.669610	2689.225352	21.351911
72.480884	2694.547597	21.356928
72.607834	2700.873555	21.361946
72.685003	2720.122077	21.366963
72.798254	2712.763494	21.371981
72.926459	2722.928507	21.376999
72.763105	2718.509239	21.382016
73.022092	2729.191617	21.387034
73.143623	2751.063340	21.392051
73.433081	2754.803954	21.397069
73.579813	2745.828274	21.402087
73.782639	2750.400222	21.407104
73.449821	2753.046143	21.412122
73.525123	2750.886734	21.417139
73.576623	2739.190008	21.422157
74.125839	2740.646499	21.427175
73.924016	2747.953360	21.432192
74.050699	2751.495712	21.437210
74.144806	2770.274527	21.442227
74.385947	2766.543839	21.447245
74.284363	2765.794529	21.452263
74.307560	2772.426301	21.457280
74.562261	2758.035477	21.462298
74.145100	2769.521621	21.467315
74.282535	2762.514550	21.472333
74.224033	2770.474513	21.477351
74.458993	2767.179527	21.482368
74.676852	2782.780936	21.487386
74.930781	2799.855636	21.492403
74.938004	2800.714026	21.497421
75.439984	2799.761621	21.502439
75.089171	2799.691027	21.507456
75.407407	2790.447930	21.512474
74.892380	2797.460189	21.517491
75.215068	2793.589605	21.522509
75.452187	2788.300403	21.527527
75.171697	2796.164448	21.532544
75.453943	2793.616410	21.537562
75.113564	2816.643529	21.542579
75.709864	2822.028764	21.547597
75.938528	2817.434313	21.552615
75.613880	2826.190794	21.557632
75.965583	2815.351463	21.562650
75.718011	2823.725860	21.567667
76.174495	2810.709957	21.572685
76.031674	2818.863842	21.577703
75.876346	2826.835142	21.582720
76.114873	2835.997239	21.587738
76.340413	2844.108257	21.592755
76.499906	2838.442882	21.597773
76.701967	2840.353353	21.602791
76.587897	2849.910481	21.607808
76.747831	2842.620885	21.612826
76.582684	2843.462538	21.617843
76.484109	2851.227980	21.622861
76.764172	2846.888812	21.627879
76.670856	2857.528816	21.632896
77.071860	2862.563299	21.637914
76.841523	2862.998784	21.642931
76.977727	2860.730843	21.647949
77.056964	2859.308623	21.652967
76.863266	2867.055175	21.657984
77.030182	2876.293331	21.663002
77.012529	2892.837857	21.668019
77.299347	2883.368391	21.673037
77.244975	2891.447034	21.678055
77.521491	2890.252011	21.683072
77.651906	2889.100472	21.688090
77.670404	2926.451033	21.693107
77.704951	2915.887394	21.698125
77.877088	2915.621541	21.703143
77.830325	2921.419611	21.708160
77.980496	2910.746272	21.713178
78.130805	2917.086169	21.718195
78.388869	2934.919846	21.723213
78.712264	2942.744218	21.728231
78.431305	2940.786696	21.733248
78.555000	2949.501298	21.738266
78.724536	2950.308409	21.743283
78.853078	2943.386201	21.748301
78.936351	2942.867714	21.753319
78.827081	2939.728122	21.758336
79.332089	2935.800936	21.763354
78.836176	2946.681298	21.768371
79.119148	2939.214972	21.773389
79.689014	2936.838993	21.778407
79.210158	2943.240551	21.783424
79.264675	2928.249591	21.788442
79.405070	2933.347722	21.793459
78.943995	2939.916822	21.798477
79.414664	2949.750453	21.803495
79.440514	2964.799533	21.808512
79.367253	2965.779929	21.813530
79.568256	2971.212162	21.818547
79.866742	2977.874037	21.823565
79.877034	2986.838559	21.828583
79.802546	3001.158551	21.833600
80.080974	2992.607027	21.838618
80.216651	2994.330065	21.843635
80.248127	2999.899443	21.848653
80.246014	2991.622344	21.853671
80.285281	2990.490221	21.858688
80.726545	3008.207421	21.863706
80.205306	3016.633139	21.868723
80.464748	3015.802778	21.873741
81.045949	3016.349982	21.878759
80.849836	3021.368807	21.883776
81.204807	3021.221906	21.888794
81.136482	3023.652803	21.893811
80.858620	3019.548104	21.898829
80.853578	3018.260308	21.903847
80.919546	3037.902451	21.908864
81.059798	3046.088725	21.913882
81.305264	3048.577129	21.918899
81.352784	3046.420705	21.923917
81.709056	3037.926747	21.928935
81.411390	3059.042248	21.933952
81.836370	3059.022351	21.938970
82.050945	3069.407957	21.943987
81.790248	3082.346516	21.949005
82.285204	3074.846996	21.954023
81.983303	3067.936943	21.959040
82.103817	3060.744726	21.964058
82.534382	3067.253656	21.969075
82.208902	3069.277883	21.974093
82.376504	3062.497594	21.979111
82.203861	3081.386311	21.984128
82.391888	3069.489550	21.989146
82.550987	3085.158476	21.994163
82.556402	3103.107414	21.999181
82.899285	3105.973830	22.004199
82.597837	3103.476714	22.009216
82.895194	3105.160395	22.014234
83.017510	3100.342109	22.019251
82.983700	3107.561076	22.024269
83.013169	3099.269635	22.029287
82.997762	3123.573054	22.034304
83.046054	3127.583635	22.039322
83.398055	3127.160032	22.044339
83.502815	3129.806011	22.049357
83.706923	3114.596385	22.054375
83.653438	3128.662991	22.059392
83.834749	3128.220402	22.064410
83.521685	3126.418974	22.069427
83.462879	3149.824806	22.074445
83.912795	3151.894297	22.079463
83.967531	3156.347170	22.084480
83.963752	3161.755890	22.089498
84.481659	3147.556586	22.094515
84.051869	3159.963702	22.099533
84.401948	3167.239619	22.104551
84.582903	3180.094502	22.109568
84.605427	3189.023252	22.114586
84.800194	3187.966559	22.119603
84.737894	3187.007160	22.124621
85.012197	3179.296462	22.129639
85.318403	3184.481801	22.134656
85.024285	3177.570016	22.139674
85.209644	3178.968674	22.144691
85.004293	3184.584024	22.149709
85.354582	3171.771252	22.154727
85.116070	3192.548759	22.159744
85.464727	3199.749722	22.164762
85.529487	3203.367004	22.169779
85.352067	3209.395891	22.174797
85.799903	3206.014775	22.179815
85.825365	3213.681505	22.184832
86.005679	3216.029527	22.189850
86.390321	3201.560083	22.194867
85.833151	3211.778653	22.199885
86.069090	3228.710724	22.204903
86.033287	3243.094618	22.209920
86.117910	3242.130576	22.214938
86.267641	3241.383337	22.219955
86.062753	3239.915991	22.224973
86.578673	3245.321378	22.229991
86.697528	3263.929349	22.235008
86.854539	3274.159251	22.240026
87.339863	3270.113970	22.245043
87.073109	3274.038940	22.250061
87.344957	3271.649258	22.255079
87.176688	3269.870301	22.260096
86.958609	3263.512091	22.265114
87.213357	3264.067683	22.270131
87.473117	3261.495732	22.275149
87.857849	3251.997234	22.280167
87.573033	3264.790314	22.285184
87.024213	3258.843205	22.290202
87.399963	3258.487722	22.295219
87.818040	3269.906418	22.300237
88.085652	3279.676625	22.305255
87.768198	3287.702564	22.310272
87.930372	3279.586715	22.315290
87.945583	3271.211707	22.320307
87.632528	3287.563409	22.325325
88.119465	3303.403101	22.330343
88.073741	3315.277405	22.335360
88.022421	3310.117290	22.340378
88.510144	3317.751239	22.345395
88.437509	3326.387522	22.350413
88.426690	3331.300561	22.355431
88.706178	3342.851718	22.360448
88.831830	3340.001532	22.365466
89.017044	3340.033147	22.370483
88.766450	3343.388860	22.375501
89.031906	3345.584206	22.380519
89.331150	3358.777959	22.385536
89.131542	3369.397322	22.390554
89.544505	3364.012663	22.395571
89.387413	3365.070750	22.400589
89.399923	3368.762477	22.405607
89.681441	3364.483170	22.410624
89.810141	3354.463945	22.415642
89.867488	3351.136428	22.420659
89.890202	3377.000641	22.425677
90.083420	3377.026207	22.430695
90.236649	3377.362759	22.435712
90.364977	3387.043090	22.440730
90.562480	3386.635612	22.445747
90.647351	3385.298643	22.450765
90.705240	3380.512201	22.455783
90.605777	3372.707764	22.460800
90.438999	3384.930548	22.465818
90.625923	3365.469885	22.470835
90.777199	3396.194502	22.475853
90.914453	3411.807524	22.480871
91.246786	3409.953540	22.485888
91.174065	3417.442903	22.490906
91.376019	3413.164550	22.495923
91.243008	3418.874317	22.500941
91.118734	3402.734808	22.505959
91.370890	3405.952169	22.510976
91.417932	3433.866231	22.515994
91.692039	3427.585141	22.521011
91.614341	3448.038293	22.526029
91.448575	3442.938033	22.531047
92.000053	3431.490331	22.536064
91.873099	3453.536084	22.541082
92.083592	3464.545933	22.546099
92.025397	3469.481035	22.551117
92.408406	3469.785056	22.556135
92.519512	3465.376831	22.561152
92.348096	3472.982968	22.566170
92.511466	3477.732550	22.571187
92.813383	3491.191359	22.576205
92.680820	3501.960754	22.581223
93.071297	3489.357632	22.586240
93.244232	3502.099527	22.591258
93.506205	3483.590583	22.596275
93.420789	3487.669462	22.601293
93.244005	3498.304821	22.606311
93.528393	3492.876045	22.611328
93.157071	3496.712859	22.616346
93.215153	3498.650795	22.621363
93.583741	3517.141331	22.626381
93.444651	3523.767216	22.631399
93.655867	3517.418935	22.636416
93.571021	3529.882628	22.641434
93.777813	3529.759078	22.646451
93.856618	3547.343967	22.651469
93.972198	3538.389924	22.656487
94.272588	3548.266697	22.661504
94.131278	3551.238566	22.666522
94.550520	3541.303024	22.671539
94.252405	3564.820761	22.676557
94.497286	3569.977795	22.681575
94.620369	3575.650729	22.686592
95.216905	3577.755854	22.691610
95.105204	3569.193799	22.696627
95.073182	3581.834244	22.701645
95.085844	3578.597947	22.706663
95.563581	3574.602670	22.711680
95.336474	3580.948627	22.716698
95.661692	3566.766675	22.721715
95.598130	3564.362790	22.726733
95.863875	3568.210298	22.731751
95.666480	3572.913329	22.736768
95.868750	3578.369584	22.741786
95.741282	3585.881480	22.746803
95.676607	3589.948289	22.751821
96.037029	3600.089207	22.756839
96.212205	3601.308860	22.761856
95.701369	3603.148460	22.766874
95.743052	3610.641023	22.771891
95.910790	3622.649923	22.776909
96.002365	3628.222568	22.781927
96.603674	3634.106539	22.786944
96.265238	3659.866820	22.791962
96.611687	3660.244231	22.796979
96.427987	3666.043200	22.801997
96.499653	3672.918542	22.807015
96.980087	3686.370800	22.812032
96.632793	3704.181948	22.817050
97.462030	3695.947562	22.822067
97.286194	3697.167064	22.827085
97.495503	3702.167017	22.832103
97.929574	3716.500324	22.837120
97.830440	3719.035261	22.842138
98.196789	3712.388344	22.847155
98.180088	3710.902788	22.852173
98.341849	3715.866124	22.857191
98.644001	3703.629865	22.862208
98.521495	3705.533938	22.867226
98.505772	3704.799504	22.872243
98.667040	3708.915561	22.877261
98.398345	3709.057376	22.882279
99.098307	3699.118174	22.887296
98.843122	3706.856813	22.892314
98.661944	3698.625920	22.897331
98.605354	3697.776188	22.902349
98.826324	3708.393871	22.907367
99.328915	3723.848671	22.912384
99.113063	3733.068021	22.917402
99.208799	3727.874365	22.922419
99.175003	3731.241515	22.927437
99.078149	3728.405261	22.932455
99.607400	3735.999466	22.937472
99.346384	3755.760831	22.942490
99.536278	3760.041870	22.947507
99.310849	3763.678190	22.952525
99.645798	3778.617418	22.957543
99.949071	3789.404232	22.962560
99.763455	3797.782669	22.967578
100.049973	3798.552739	22.972595
100.254715	3795.965793	22.977613
99.985897	3823.400093	22.982631
100.272165	3815.937533	22.987648
100.507164	3825.875710	22.992666
100.839117	3821.277649	22.997683
100.933369	3833.482763	23.002701
100.988287	3844.047311	23.007719
101.611066	3840.713486	23.012736
101.231693	3843.165690	23.017754
101.465253	3845.876305	23.022771
101.715976	3844.750061	23.027789
101.179652	3848.503633	23.032807
101.567019	3846.222710	23.037824
101.548175	3852.929233	23.042842
101.389040	3843.348355	23.047859
101.576771	3848.040073	23.052877
101.840687	3872.375582	23.057895
102.271244	3864.779644	23.062912
101.997527	3876.828362	23.067930
102.121246	3871.976532	23.072947
102.295811	3869.826130	23.077965
101.951625	3881.955033	23.082983
102.586969	3894.034380	23.088000
102.747665	3899.181049	23.093018
102.761880	3906.193190	23.098035
102.690467	3902.762054	23.103053
102.717620	3905.639158	23.108071
102.959928	3925.080751	23.113088
102.985444	3933.786562	23.118106
103.269590	3925.559620	23.123123
103.247776	3927.835296	23.128141
103.143928	3927.619454	23.133159
103.353065	3937.835254	23.138176
103.338671	3959.167701	23.143194
103.640313	3963.824842	23.148211
103.559022	3956.542776	23.153229
103.925599	3960.572536	23.158247
104.237384	3974.102579	23.163264
103.921273	3993.286267	23.168282
103.963260	3990.272623	23.173299
104.200650	3992.768424	23.178317
104.227026	3995.547233	23.183335
104.706292	4009.847338	23.188352
105.042368	4010.339093	23.193370
104.933242	4019.234200	23.198387
105.205529	4007.451933	23.203405
104.778723	4012.066680	23.208423
105.350366	3998.837001	23.213440
105.320242	4005.250135	23.218458
105.443306	4024.361147	23.223475
105.576775	4026.908811	23.228493
105.693453	4034.484450	23.233511
105.767247	4033.356379	23.238528
106.072564	4033.408277	23.243546
105.707962	4032.762304	23.248563
106.148585	4033.533647	23.253581
106.273031	4033.646204	23.258599
106.437737	4041.654121	23.263616
106.137856	4061.438449	23.268634
106.197387	4072.670603	23.273651
106.542306	4061.203094	23.278669
106.572073	4068.254471	23.283687
106.638191	4063.606639	23.288704
106.581378	4070.745592	23.293722
106.756221	4093.857414	23.298739
107.102616	4086.692695	23.303757
107.153755	4091.504755	23.308775
107.223804	4095.253672	23.313792
107.316325	4098.127076	23.318810
107.272905	4121.336503	23.323827
107.594816	4123.679726	23.328845
107.704077	4118.733348	23.333863
108.038636	4126.954171	23.338880
107.847318	4116.688185	23.343898
108.077982	4119.494619	23.348915
108.014547	4130.127388	23.353933
108.244877	4145.242975	23.358951
108.258183	4140.553462	23.363968
108.435740	4144.085346	23.368986
108.165929	4149.243523	23.374003
108.527948	4147.277043	23.379021
108.386409	4164.931002	23.384039
108.675828	4174.086248	23.389056
108.963773	4178.299979	23.394074
108.845118	4167.659664	23.399091
109.069708	4171.857107	23.404109
109.165235	4193.303190	23.409127
109.613570	4201.700523	23.414144
109.435356	4196.934810	23.419162
109.302674	4208.345367	23.424179
109.322074	4203.513857	23.429197
109.430527	4216.697397	23.434215
109.727548	4226.298734	23.439232
109.920776	4233.838957	23.444250
109.982016	4238.180019	23.449267
110.560267	4225.171929	23.454285
110.560825	4243.307260	23.459303
110.687681	4251.734220	23.464320
110.681878	4259.412938	23.469338
110.658675	4266.980349	23.474355
111.029958	4255.132679	23.479373
110.945381	4259.522303	23.484391
111.138027	4249.605326	23.489408
111.303943	4250.045722	23.494426
111.006512	4265.307083	23.499443
111.526242	4270.002237	23.504461
111.287471	4285.058596	23.509479
111.702740	4287.106811	23.514496
111.617893	4285.685248	23.519514
111.955245	4286.336672	23.524531
111.933161	4291.570436	23.529549
111.931272	4308.309942	23.534567
112.212168	4309.974826	23.539584
112.498356	4304.737634	23.544602
112.218961	4306.066075	23.549619
112.564151	4309.676560	23.554637
112.786066	4320.007838	23.559655
112.653603	4336.663462	23.564672
112.834831	4337.192680	23.569690
113.011576	4333.348644	23.574707
112.989277	4335.400009	23.579725
113.060581	4338.208454	23.584743
112.942391	4358.438746	23.589760
113.836379	4358.277413	23.594778
113.752972	4369.981557	23.599795
113.653792	4372.412650	23.604813
113.437878	4371.492393	23.609831
113.396321	4370.504678	23.614848
113.806975	4377.481319	23.619866
114.053242	4399.721771	23.624883
114.218757	4397.266441	23.629901
114.140108	4397.933981	23.634919
114.013980	4415.994405	23.639936
114.622196	4414.862092	23.644954
114.305371	4431.908249	23.649971
114.558827	4422.682799	23.654989
114.639237	4440.086107	23.660007
114.701355	4459.206951	23.665024
115.138788	4454.799156	23.670042
115.059192	4464.716585	23.675059
115.421347	4467.032722	23.680077
115.471744	4478.873877	23.685095
115.740227	4480.216366	23.690112
115.786990	4484.166118	23.695130
115.578916	4486.034836	23.700147
115.657398	4488.178217	23.705165
116.083477	4496.513240	23.710183
116.020220	4508.945783	23.715200
116.173053	4514.702731	23.720218
116.246589	4520.194019	23.725235
116.608281	4520.662650	23.730253
116.565741	4518.612685	23.735271
116.700500	4517.625696	23.740288
116.888851	4525.869361	23.745306
117.009971	4539.326718	23.750323
116.845618	4541.137800	23.755341
116.992075	4549.061580	23.760359
117.070359	4543.051492	23.765376
117.437323	4542.553715	23.770394
117.228720	4561.331243	23.775411
117.666062	4572.702815	23.780429
117.556621	4572.972234	23.785447
117.695639	4578.132954	23.790464
117.700097	4572.496564	23.795482
117.874182	4589.278901	23.800499
118.018340	4590.798707	23.805517
117.926370	4597.293201	23.810535
118.130641	4607.095204	23.815552
118.256635	4616.359672	23.820570
118.619835	4628.587030	23.825587
118.439281	4624.320884	23.830605
118.746567	4643.116266	23.835623
118.702190	4649.908473	23.840640
119.100271	4652.829046	23.845658
119.017468	4662.338388	23.850675
119.191924	4676.647043	23.855693
119.232919	4690.613955	23.860711
119.409854	4685.694786	23.865728
119.988150	4694.838737	23.870746
120.021530	4705.510206	23.875763
119.992751	4702.384497	23.880781
120.376961	4703.678705	23.885799
120.071491	4700.313710	23.890816
120.613265	4700.520991	23.895834
120.486072	4713.488794	23.900851
120.766019	4721.718185	23.905869
121.011121	4729.790324	23.910887
121.130311	4738.840200	23.915904
121.347140	4725.155960	23.920922
121.446639	4738.202810	23.925939
121.361669	4738.554811	23.930957
121.607217	4731.757750	23.935975
121.379734	4730.487347	23.940992
121.788199	4731.240426	23.946010
121.464712	4744.484110	23.951027
122.003078	4758.793231	23.956045
122.002562	4760.374022	23.961063
121.957836	4770.564666	23.966080
122.090662	4760.391078	23.971098
122.300144	4776.342390	23.976115
122.477461	4784.247004	23.981133
122.669554	4793.052510	23.986151
122.559097	4801.874247	23.991168
122.536118	4783.581463	23.996186
122.520085	4802.293529	24.001203
122.808400	4824.325216	24.006221
123.152220	4816.168264	24.011239
122.902342	4834.949801	24.016256
123.765391	4846.658262	24.021274
123.649996	4854.826379	24.026291
123.419012	4863.959506	24.031309
123.702997	4861.292325	24.036327
123.738914	4856.637445	24.041344
123.679631	4878.677142	24.046362
123.697420	4886.336508	24.051379
124.032670	4883.033933	24.056397
124.766320	4883.461471	24.061415
124.455811	4898.406643	24.066432
124.924680	4899.520675	24.071450
125.034609	4909.688955	24.076467
124.858624	4912.843234	24.081485
125.099082	4909.779229	24.086503
125.159875	4901.726585	24.091520
125.461676	4898.865856	24.096538
125.857100	4902.166525	24.101555
125.333744	4910.080099	24.106573
125.821310	4919.395143	24.111591
125.528201	4929.186762	24.116608
125.759851	4927.187430	24.121626
125.985517	4930.267339	24.126643
126.225351	4933.413420	24.131661
126.183665	4925.120983	24.136679
126.133070	4955.528064	24.141696
126.497705	4959.385929	24.146714
126.508150	4970.837133	24.151731
126.777180	4967.709319	24.156749
126.808515	4967.605754	24.161767
126.847614	4981.737054	24.166784
127.097565	4987.739571	24.171802
127.186599	4993.841190	24.176819
127.184689	4992.590123	24.181837
127.372590	5014.771802	24.186855
127.232097	5023.800255	24.191872
127.269307	5026.280537	24.196890
127.417830	5036.191271	24.201907
127.698918	5045.579954	24.206925
128.070072	5043.235394	24.211943
127.849652	5062.032800	24.216960
128.336464	5073.459552	24.221978
128.647597	5078.159561	24.226995
128.334194	5075.785782	24.232013
128.720786	5088.014352	24.237031
129.223752	5096.819752	24.242048
129.239068	5097.861615	24.247066
129.163598	5101.198547	24.252083
129.096885	5103.069922	24.257101
129.490863	5120.059781	24.262119
130.017502	5128.730542	24.267136
129.706300	5129.716992	24.272154
129.822453	5129.660815	24.277171
129.890961	5132.571463	24.282189
130.346945	5124.202039	24.287207
130.497378	5142.389198	24.292224
130.123686	5153.200824	24.297242
130.578721	5155.202408	24.302259
130.618240	5167.742104	24.307277
130.849886	5163.686369	24.312295
130.971449	5167.875935	24.317312
130.601197	5178.897294	24.322330
131.040748	5195.908042	24.327347
131.306148	5188.243522	24.332365
131.574823	5192.842696	24.337383
131.220625	5206.174546	24.342400
131.400858	5202.499841	24.347418
131.834772	5208.754728	24.352435
131.906212	5216.633772	24.357453
131.878579	5232.027028	24.362471
131.907620	5254.540141	24.367488
131.923987	5244.099629	24.372506
132.538526	5252.308557	24.377523
132.234880	5271.985548	24.382541
132.707491	5269.538311	24.387559
132.784946	5280.266667	24.392576
133.004909	5276.211263	24.397594
133.233143	5277.968457	24.402611
133.185791	5304.256592	24.407629
133.646490	5291.628597	24.412647
133.417560	5308.157089	24.417664
133.602288	5305.648822	24.422682
133.880549	5300.834763	24.427699
133.506825	5303.069663	24.432717
133.841152	5311.403774	24.437735
133.665107	5328.990715	24.442752
134.130777	5324.464595	24.447770
134.392445	5338.412085	24.452787
134.165490	5363.271438	24.457805
134.647562	5355.109435	24.462823
134.581116	5366.783156	24.467840
134.776150	5385.030156	24.472858
135.105434	5391.118143	24.477875
134.883953	5404.970839	24.482893
135.551034	5402.335441	24.487911
135.583753	5408.112605	24.492928
135.875495	5413.980777	24.497946
136.032826	5416.460923	24.502963
135.995576	5413.087595	24.507981
136.366048	5420.576992	24.512999
136.244264	5414.965140	24.518016
136.489297	5425.570552	24.523034
136.722156	5417.455291	24.528051
136.280486	5436.175570	24.533069
136.552213	5435.685662	24.538087
136.659588	5451.488381	24.543104
136.805101	5454.489515	24.548122
136.894095	5469.590397	24.553139
136.732201	5485.830742	24.558157
137.329985	5483.085515	24.563175
137.680162	5495.170001	24.568192
137.924795	5508.458093	24.573210
137.854735	5501.677514	24.578227
137.696329	5506.410497	24.583245
138.084069	5517.412134	24.588263
138.358361	5530.585858	24.593280
138.535006	5531.879062	24.598298
138.662224	5522.565184	24.603315
138.482231	5533.048074	24.608333
138.824762	5544.757391	24.613351
138.797806	5555.454390	24.618368
138.862367	5572.006238	24.623386
139.195316	5553.412627	24.628403
139.017054	5576.744971	24.633421
139.468057	5586.169642	24.638439
139.553282	5586.406059	24.643456
139.684444	5594.406934	24.648474
140.182566	5604.540534	24.653491
140.219609	5615.253756	24.658509
140.340316	5616.125409	24.663527
140.346505	5618.712521	24.668544
140.576018	5611.049800	24.673562
140.871664	5610.059736	24.678579
140.785353	5640.980478	24.683597
141.354199	5642.543491	24.688615
140.962444	5651.814740	24.693632
141.151773	5647.612305	24.698650
141.563438	5643.751113	24.703667
141.057012	5662.785608	24.708685
141.606309	5663.820226	24.713703
142.031193	5669.920060	24.718720
141.502054	5679.818165	24.723738
141.862712	5674.760371	24.728755
142.155847	5697.198887	24.733773
142.362803	5710.316963	24.738791
142.304936	5709.465757	24.743808
142.227134	5712.020321	24.748826
142.602276	5721.229227	24.753843
142.634789	5730.192421	24.758861
143.023866	5735.197919	24.763879
143.112440	5731.800541	24.768896
142.854191	5748.226443	24.773914
143.594869	5765.410061	24.778931
143.286706	5768.773056	24.783949
143.243747	5776.438186	24.788967
143.580455	5785.182501	24.793984
143.546790	5801.416904	24.799002
144.056322	5797.950606	24.804019
144.049082	5814.665817	24.809037
144.127192	5830.951055	24.814055
144.183632	5828.067775	24.819072
144.500924	5843.102864	24.824090
144.982592	5857.771290	24.829107
144.995679	5866.179358	24.834125
145.021315	5859.401685	24.839143
145.326325	5859.071654	24.844160
145.193623	5880.679112	24.849178
145.690361	5885.439212	24.854195
145.560192	5888.215131	24.859213
145.795259	5894.799360	24.864231
145.653696	5908.617210	24.869248
145.663926	5924.703488	24.874266
146.181386	5922.793762	24.879283
146.498304	5948.131862	24.884301
146.538875	5946.960324	24.889319
146.608103	5950.225434	24.894336
146.772050	5962.955455	24.899354
147.071546	5963.009119	24.904371
146.994095	5970.612319	24.909389
147.274398	5974.700208	24.914407
147.490261	5986.457604	24.919424
147.868050	5998.214980	24.924442
148.105970	6000.800808	24.929459
147.887468	6003.254268	24.934477
147.731306	6013.665794	24.939495
148.360760	6027.441162	24.944512
148.447410	6032.545658	24.949530
148.359477	6030.984249	24.954547
148.502830	6041.102042	24.959565
148.855405	6054.853176	24.964583
148.949265	6067.538176	24.969600
149.011158	6065.807036	24.974618
149.287718	6077.966380	24.979635
149.448334	6086.494276	24.984653
149.430450	6092.058744	24.989671
149.827667	6097.197695	24.994688
149.908507	6103.130185	24.999706
150.402091	6113.966642	25.004723
149.997607	6127.017741	25.009741
150.463081	6130.515798	25.014759
150.911740	6125.831594	25.019776
150.446793	6122.815620	25.024794
150.937752	6137.631631	25.029811
150.975105	6147.718209	25.034829
151.067963	6151.235428	25.039847
151.276134	6150.566991	25.044864
151.188590	6163.568011	25.049882
150.824989	6174.974108	25.054899
151.321850	6183.720484	25.059917
151.242686	6201.413648	25.064935
151.697459	6210.760096	25.069952
151.526468	6229.437282	25.074970
152.102650	6237.647568	25.079987
152.113613	6242.574054	25.085005
152.301296	6260.825646	25.090023
152.852843	6275.417519	25.095040
152.596304	6283.009560	25.100058
152.745653	6277.188685	25.105075
152.977004	6281.602964	25.110093
153.019314	6299.494302	25.115111
153.695473	6304.910072	25.120128
153.622961	6307.418172	25.125146
153.532252	6304.474891	25.130163
153.831381	6312.122239	25.135181
154.088190	6318.484082	25.140199
154.737087	6322.459055	25.145216
154.641730	6325.760942	25.150234
154.652136	6320.205647	25.155251
154.462770	6341.992456	25.160269
154.276205	6353.474127	25.165287
154.803875	6344.590471	25.170304
155.477102	6379.345585	25.175322
155.499137	6371.963380	25.180339
155.646808	6383.047114	25.185357
155.788571	6386.809122	25.190375
156.207108	6389.978685	25.195392
155.896839	6397.932540	25.200410
156.028936	6413.150059	25.205427
156.415091	6426.140608	25.210445
156.288598	6427.321819	25.215463
156.531204	6419.316280	25.220480
156.331061	6435.893164	25.225498
156.829460	6441.217115	25.230515
156.505232	6445.752563	25.235533
156.688140	6469.970024	25.240551
157.192745	6466.850965	25.245568
156.950314	6490.706458	25.250586
157.443344	6498.586445	25.255603
157.650359	6507.338456	25.260621
157.804476	6530.513204	25.265639
157.977608	6529.982878	25.270656
158.391111	6533.131251	25.275674
158.481137	6550.358072	25.280691
158.810991	6554.059837	25.285709
158.842964	6557.944033	25.290727
159.146287	6552.070785	25.295744
159.055289	6572.534913	25.300762
159.189328	6571.093444	25.305779
159.595534	6582.909564	25.310797
159.514541	6580.076469	25.315815
159.627620	6594.761709	25.320832
160.053540	6619.622062	25.325850
160.002660	6612.802387	25.330867
160.085638	6611.354402	25.335885
160.121037	6635.732802	25.340903
160.585177	6642.571639	25.345920
160.498229	6658.492015	25.350938
160.873921	6660.869257	25.355955
161.023480	6678.351801	25.360973
160.966693	6684.628658	25.365991
161.131951	6679.761217	25.371008
161.250732	6690.752279	25.376026
161.613306	6704.551946	25.381043
161.805043	6707.904840	25.386061
162.041251	6731.620803	25.391079
162.337479	6746.079734	25.396096
162.193852	6747.688354	25.401114
162.706641	6736.502252	25.406131
162.898211	6751.596040	25.411149
162.764014	6777.523707	25.416167
162.845599	6777.073905	25.421184
162.976180	6779.123119	25.426202
163.115280	6774.485252	25.431219
163.535816	6779.440980	25.436237
162.982125	6797.081828	25.441255
163.565816	6800.835360	25.446272
163.868151	6808.119306	25.451290
163.781725	6822.449468	25.456307
164.026032	6828.315783	25.461325
164.328635	6839.341892	25.466343
164.501136	6858.125209	25.471360
164.535057	6859.058561	25.476378
164.554500	6861.508990	25.481395
164.669137	6883.410834	25.486413
164.903011	6904.128006	25.491431
165.207452	6896.418395	25.496448
165.258122	6909.148239	25.501466
165.255796	6926.395484	25.506483
165.831135	6925.425204	25.511501
166.244215	6943.125131	25.516519
166.536846	6946.453496	25.521536
166.399748	6955.873168	25.526554
166.273845	6947.851969	25.531571
166.923768	6964.544664	25.536589
166.747704	6972.697921	25.541607
166.997073	6967.391125	25.546624
166.911572	6983.508504	25.551642
167.386772	7002.015029	25.556659
167.476503	6997.043420	25.561677
167.239094	7020.765759	25.566695
167.633353	7039.387337	25.571712
167.903941	7046.124490	25.576730
167.898458	7060.654924	25.581747
168.001967	7061.451527	25.586765
168.023806	7080.692484	25.591783
168.233587	7098.516825	25.596800
168.866319	7107.126222	25.601818
168.995534	7131.992390	25.606835
169.351065	7134.313179	25.611853
169.273089	7139.346826	25.616871
169.634212	7159.999156	25.621888
169.638428	7156.005776	25.626906
169.833087	7171.058492	25.631923
170.229956	7171.854582	25.636941
170.323846	7195.363222	25.641959
169.926087	7190.654213	25.646976
170.668916	7206.839482	25.651994
170.938470	7219.938207	25.657011
171.037224	7214.059989	25.662029
171.107903	7227.746174	25.667047
171.630317	7228.820803	25.672064
171.579382	7249.199612	25.677082
171.631430	7256.016356	25.682100
172.104958	7241.339868	25.687117
171.733289	7256.924376	25.692135
172.440904	7269.519756	25.697152
172.519097	7282.669906	25.702170
172.759662	7281.940924	25.707188
172.832443	7278.244147	25.712205
172.867108	7296.719974	25.717223
173.125552	7303.204036	25.722240
173.423079	7314.130492	25.727258
173.179120	7320.324371	25.732276
173.787801	7326.792995	25.737293
173.702345	7347.783378	25.742311
173.584423	7346.008613	25.747328
173.770722	7357.782163	25.752346
173.608159	7375.303756	25.757364
174.031098	7387.826631	25.762381
174.378368	7398.852824	25.767399
174.451119	7407.806367	25.772416
174.690325	7406.586084	25.777434
174.600399	7422.861390	25.782452
174.855987	7425.698954	25.787469
174.915948	7442.066832	25.792487
175.059469	7466.485319	25.797504
175.227259	7473.278269	25.802522
175.402185	7495.742842	25.807540
175.678612	7504.662720	25.812557
176.003533	7524.027330	25.817575
176.418078	7525.983944	25.822592
176.732968	7537.097515	25.827610
176.565786	7534.490409	25.832628
176.695724	7554.442664	25.837645
177.180336	7567.986570	25.842663
177.118255	7561.374720	25.847680
177.666491	7581.909187	25.852698
177.360148	7594.862526	25.857716
177.967416	7600.624929	25.862733
177.898191	7615.368074	25.867751
178.489341	7625.769575	25.872768
178.279973	7628.364343	25.877786
178.243646	7652.293792	25.882804
178.679984	7654.426412	25.887821
179.110126	7655.098865	25.892839
178.886912	7669.257869	25.897856
178.997699	7684.085494	25.902874
178.982190	7689.078252	25.907892
179.650738	7699.325989	25.912909
179.719523	7713.974696	25.917927
180.019091	7719.751848	25.922944
180.282598	7741.237160	25.927962
180.711254	7753.582144	25.932980
180.686887	7744.233771	25.937997
180.907546	7750.387920	25.943015
181.177757	7767.780795	25.948032
181.466859	7767.082355	25.953050
181.362371	7779.409280	25.958068
181.650768	7779.300952	25.963085
181.795774	7799.406198	25.968103
181.717658	7805.439685	25.973120
182.337771	7809.314255	25.978138
182.162341	7809.463888	25.983156
182.304358	7819.895759	25.988173
182.787661	7829.385748	25.993191
182.828971	7834.448704	25.998208
183.247675	7854.860818	26.003226
182.973802	7873.966574	26.008244
183.137237	7864.554745	26.013261
183.799127	7872.950203	26.018279
183.852246	7893.147188	26.023296
184.066109	7896.680998	26.028314
183.604939	7900.564451	26.033332
184.249081	7918.461955	26.038349
184.454998	7930.365018	26.043367
184.405434	7928.240151	26.048384
184.656748	7937.895433	26.053402
184.517922	7952.942656	26.058420
184.756632	7969.250762	26.063437
185.049051	7974.386411	26.068455
185.101801	7986.049411	26.073472
185.895819	8000.888682	26.078490
185.837521	8015.665047	26.083508
186.032612	8011.266473	26.088525
186.501740	8035.868245	26.093543
186.493903	8047.105708	26.098560
186.780823	8049.249728	26.103578
186.759857	8046.713646	26.108596
186.850741	8064.580809	26.113613
186.967357	8068.671136	26.118631
187.352913	8076.936000	26.123648
187.347796	8080.702247	26.128666
187.602832	8097.650566	26.133684
187.960941	8108.890509	26.138701
188.112893	8101.886160	26.143719
188.134898	8131.093895	26.148736
188.300570	8143.509501	26.153754
188.130455	8141.180061	26.158772
188.566437	8163.836314	26.163789
188.768811	8166.277929	26.168807
188.487235	8191.617074	26.173824
189.266859	8197.017954	26.178842
189.525077	8212.818144	26.183860
189.880226	8227.752338	26.188877
189.862072	8232.922157	26.193895
189.615414	8239.977829	26.198912
190.504564	8257.189213	26.203930
190.586233	8264.129886	26.208948
190.572343	8281.987067	26.213965
190.811954	8291.198642	26.218983
190.913073	8293.563299	26.224000
191.288689	8303.499928	26.229018
191.201978	8326.060976	26.234036
191.585225	8329.223387	26.239053
192.159454	8345.551957	26.244071
191.881847	8359.284956	26.249088
192.090200	8355.705705	26.254106
192.561879	8376.628838	26.259124
192.636002	8378.890057	26.264141
193.091230	8387.881662	26.269159
192.912963	8403.321043	26.274176
193.479491	8405.316417	26.279194
193.566685	8420.963157	26.284212
193.793900	8429.656167	26.289229
193.934202	8434.884107	26.294247
193.212194	8449.863703	26.299264
193.833903	8462.236359	26.304282
193.974984	8479.209463	26.309300
194.083942	8496.027203	26.314317
194.422917	8511.867887	26.319335
194.110904	8528.738809	26.324352
194.962758	8540.744148	26.329370
195.296624	8558.744155	26.334388
195.344625	8570.906226	26.339405
195.923806	8583.740549	26.344423
195.929784	8596.546098	26.349440
196.305270	8601.112835	26.354458
196.562612	8619.375297	26.359476
196.579725	8625.840771	26.364493
196.838596	8623.915256	26.369511
197.108443	8645.731594	26.374528
197.024656	8651.571763	26.379546
197.299573	8660.918715	26.384564
197.341361	8679.145244	26.389581
197.939739	8686.042312	26.394599
197.823064	8694.957825	26.399616
198.132493	8708.823177	26.404634
198.768426	8715.789666	26.409652
198.578149	8719.577262	26.414669
198.953220	8724.463145	26.419687
198.903598	8739.811442	26.424704
199.361611	8744.130594	26.429722
199.458641	8745.199345	26.434740
199.438397	8766.298957	26.439757
199.887410	8779.311752	26.444775
199.845179	8782.981900	26.449792
200.006752	8775.137488	26.454810
200.261950	8799.849905	26.459828
200.289027	8806.378399	26.464845
200.850551	8806.099599	26.469863
200.833300	8833.355950	26.474880
201.223951	8847.037032	26.479898
200.949179	8838.102086	26.484916
201.030182	8862.656737	26.489933
201.725369	8859.806604	26.494951
201.414441	8882.991650	26.499968
201.948776	8894.235273	26.504986
202.050864	8902.003148	26.510004
202.545150	8924.460978	26.515021
202.750239	8934.623962	26.520039
202.511596	8945.463841	26.525056
202.741838	8962.037478	26.530074
203.045177	8966.314549	26.535092
203.289439	8984.304662	26.540109
203.618320	8984.191204	26.545127
203.776743	9013.838811	26.550144
204.035285	9022.482056	26.555162
204.299707	9034.824500	26.560180
204.228645	9060.154587	26.565197
204.378558	9059.133305	26.570215
204.526485	9088.726856	26.575232
204.907790	9097.114274	26.580250
205.108586	9109.956518	26.585268
205.272684	9126.538912	26.590285
205.756468	9141.466848	26.595303
205.985908	9156.389637	26.600320
205.913306	9153.096206	26.605338
206.525851	9186.447142	26.610356
206.588208	9181.332073	26.615373
206.860992	9192.500251	26.620391
207.179541	9216.510364	26.625408
207.126070	9225.878924	26.630426
207.589182	9234.635733	26.635444
207.846536	9254.023872	26.640461
208.238956	9254.517517	26.645479
208.345026	9251.790840	26.650496
208.666186	9266.902585	26.655514
208.604817	9278.980098	26.660532
208.680855	9291.116803	26.665549
208.865823	9297.149051	26.670567
208.958912	9308.983588	26.675584
209.342020	9313.378320	26.680602
209.578406	9330.071853	26.685620
209.579784	9355.752796	26.690637
209.995760	9349.445507	26.695655
209.939408	9369.401719	26.700672
210.034697	9377.585327	26.705690
210.545540	9393.983763	26.710708
210.547827	9408.872702	26.715725
210.664313	9414.940752	26.720743
210.751420	9430.096123	26.725760
211.083815	9441.915564	26.730778
211.474374	9461.518241	26.735796
211.569809	9477.939838	26.740813
211.953475	9487.560757	26.745831
212.114472	9502.790622	26.750848
212.201304	9523.789210	26.755866
212.887450	9530.240406	26.760884
212.744352	9547.738303	26.765901
213.252682	9559.341211	26.770919
213.462653	9562.285976	26.775936
213.306420	9578.779275	26.780954
213.970885	9593.193227	26.785972
213.975165	9601.710287	26.790989
214.155120	9601.942117	26.796007
214.418410	9614.907559	26.801024
214.201570	9627.158390	26.806042
214.673055	9632.993651	26.811060
214.870936	9648.196278	26.816077
215.301883	9651.941126	26.821095
215.090005	9666.725528	26.826112
215.560246	9680.354758	26.831130
215.491735	9696.867532	26.836148
215.633101	9717.748628	26.841165
216.091887	9722.243602	26.846183
216.345858	9740.237684	26.851200
216.713851	9748.887625	26.856218
216.848193	9753.920820	26.861236
216.962707	9785.484404	26.866253
217.249953	9785.459769	26.871271
217.487955	9808.181853	26.876288
217.573229	9817.502579	26.881306
218.112601	9826.618938	26.886324
218.291773	9840.970856	26.891341
218.417184	9841.823061	26.896359
218.950697	9855.991861	26.901376
218.972390	9870.841775	26.906394
219.149154	9873.363525	26.911412
219.242925	9907.794487	26.916429
219.599655	9896.973158	26.921447
219.719524	9911.969148	26.926464
219.406266	9940.870918	26.931482
219.633651	9950.159530	26.936500
220.055803	9969.643364	26.941517
220.417430	9996.728673	26.946535
220.601840	9999.955852	26.951552
220.586928	10030.690497	26.956570
221.225616	10036.328058	26.961588
221.493647	10060.320224	26.966605
221.558746	10070.049377	26.971623
221.754406	10086.715775	26.976640
222.050440	10099.400450	26.981658
222.832831	10120.958264	26.986676
222.729193	10137.704986	26.991693
222.709893	10138.541772	26.996711
223.354627	10161.203327	27.001728
223.374511	10166.827562	27.006746
223.738525	10169.880083	27.011764
223.828366	10191.916615	27.016781
224.093724	10190.599624	27.021799
224.286235	10212.041709	27.026816
224.467309	10225.118158	27.031834
224.835927	10223.272769	27.036852
224.712615	10240.143392	27.041869
225.258444	10259.142284	27.046887
225.614782	10263.618132	27.051904
225.794505	10288.319337	27.056922
226.188998	10290.682996	27.061940
225.947750	10305.899850	27.066957
226.254033	10319.667065	27.071975
226.263854	10330.641640	27.076992
226.237948	10351.860869	27.082010
226.824599	10359.130894	27.087028
226.622117	10380.725252	27.092045
226.990218	10387.330292	27.097063
227.465648	10398.256987	27.102080
227.267302	10420.604676	27.107098
227.797399	10438.876845	27.112116
227.920954	10459.309630	27.117133
228.278468	10476.215929	27.122151
228.443616	10488.691740	27.127168
228.556429	10506.728955	27.132186
228.965527	10517.618654	27.137204
229.311902	10539.275996	27.142221
229.529731	10545.987125	27.147239
229.839721	10552.391498	27.152256
229.976574	10568.639541	27.157274
230.185167	10574.184621	27.162292
230.533150	10598.996322	27.167309
230.908973	10610.993006	27.172327
231.183990	10618.679512	27.177344
230.982213	10639.037960	27.182362
231.409090	10634.649941	27.187380
231.541605	10649.970695	27.192397
231.975594	10670.879433	27.197415
232.122115	10683.971429	27.202432
232.227634	10696.625873	27.207450
232.701409	10697.953047	27.212468
232.530028	10722.370321	27.217485
232.919774	10736.898538	27.222503
233.591069	10735.498551	27.227520
233.554137	10759.058497	27.232538
233.979919	10766.075649	27.237556
234.278020	10778.535979	27.242573
234.234184	10793.563040	27.247591
234.907564	10799.226647	27.252608
234.792394	10824.498264	27.257626
234.971022	10833.319591	27.262644
235.162751	10848.304557	27.267661
235.145708	10868.224601	27.272679
235.538306	10873.972532	27.277696
235.775620	10890.119180	27.282714
236.232103	10902.019216	27.287732
235.987025	10921.422417	27.292749
235.850781	10941.593916	27.297767
236.396541	10956.766192	27.302784
236.477154	10990.561895	27.307802
236.868368	11000.328230	27.312820
237.085791	11019.480080	27.317837
237.595648	11044.366518	27.322855
237.947602	11055.365313	27.327872
238.038270	11081.269797	27.332890
238.583485	11086.264546	27.337908
238.811254	11113.687466	27.342925
239.112516	11127.118204	27.347943
239.229836	11143.445695	27.352960
239.337765	11157.882277	27.357978
239.542101	11174.365576	27.362996
239.584246	11187.762046	27.368013
239.706095	11204.569454	27.373031
240.324908	11225.111104	27.378048
240.461632	11251.783510	27.383066
240.870315	11254.089026	27.388084
241.218979	11273.435332	27.393101
241.243924	11297.570427	27.398119
241.671040	11299.562473	27.403136
241.525956	11315.405693	27.408154
242.017417	11338.978288	27.413172
242.552453	11344.092986	27.418189
242.536692	11379.467044	27.423207
242.968886	11388.456278	27.428224
243.334164	11397.001194	27.433242
243.394825	11412.351900	27.438260
243.661779	11414.890480	27.443277
243.904495	11438.510699	27.448295
244.144594	11437.048094	27.453312
244.227408	11455.865043	27.458330
244.566570	11471.902441	27.463348
244.863441	11489.128696	27.468365
244.864780	11508.011192	27.473383
245.011470	11514.003337	27.478400
245.286577	11532.125136	27.483418
245.501166	11550.164001	27.488436
245.711246	11563.222551	27.493453
245.997695	11588.422573	27.498471
246.408074	11601.268357	27.503488
246.268110	11613.976762	27.508506
246.466829	11634.035369	27.513524
246.868216	11645.024808	27.518541
247.124200	11671.534766	27.523559
247.311112	11682.190996	27.528576
247.575463	11714.539571	27.533594
247.687492	11726.763548	27.538612
247.825627	11749.553748	27.543629
247.974673	11776.560626	27.548647
248.336618	11793.046830	27.553664
248.708524	11814.551954	27.558682
249.228318	11836.729139	27.563700
249.199722	11852.285710	27.568717
249.551205	11880.636518	27.573735
250.205669	11897.657462	27.578752
250.541820	11911.891476	27.583770
250.600605	11918.435678	27.588788
251.127953	11932.370170	27.593805
251.473945	11945.263131	27.598823
251.503588	11964.518096	27.603840
251.681504	11980.990832	27.608858
252.160575	11990.500547	27.613876
252.385458	12007.003355	27.618893
252.075424	12018.640294	27.623911
252.785562	12041.827880	27.628928
253.061849	12061.054739	27.633946
253.504794	12067.844276	27.638964
253.430230	12082.493112	27.643981
253.535922	12102.728434	27.648999
254.062835	12115.739711	27.654016
254.314508	12138.743313	27.659034
254.710122	12152.283777	27.664052
254.726977	12164.578994	27.669069
254.783802	12185.908270	27.674087
255.210991	12200.455245	27.679104
255.208346	12221.543851	27.684122
255.293732	12247.805639	27.689140
255.898078	12255.239854	27.694157
256.276443	12284.545042	27.699175
256.510719	12306.139788	27.704192
256.744455	12318.336185	27.709210
257.110131	12335.263566	27.714228
257.332665	12344.800198	27.719245
257.249573	12373.966039	27.724263
257.829965	12391.685269	27.729280
257.955195	12417.920250	27.734298
258.046234	12427.319534	27.739316
258.671708	12439.630827	27.744333
258.494527	12461.623247	27.749351
258.833416	12477.321297	27.754368
258.793616	12497.240803	27.759386
259.087193	12509.284033	27.764404
259.926515	12522.113126	27.769421
259.659483	12556.848980	27.774439
259.973455	12580.295175	27.779456
260.642623	12591.064433	27.784474
260.661855	12623.382902	27.789492
261.130962	12635.898305	27.794509
261.392858	12654.605051	27.799527
261.520015	12674.252873	27.804544
261.648192	12689.322554	27.809562
262.102553	12704.708592	27.814580
262.428540	12723.685320	27.819597
262.734445	12737.970768	27.824615
262.605919	12752.644898	27.829632
263.345735	12771.482264	27.834650
263.189392	12789.511416	27.839668
263.582979	12805.837398	27.844685
263.803566	12828.074924	27.849703
264.107296	12853.322903	27.854720
264.558155	12864.766727	27.859738
264.158353	12880.685151	27.864756
264.448381	12901.472467	27.869773
264.841623	12935.086513	27.874791
265.480844	12953.428566	27.879808
265.210093	12985.485296	27.884826
265.553350	13007.518377	27.889844
266.248967	13018.954890	27.894861
266.245232	13046.644755	27.899879
266.562985	13066.137001	27.904896
266.881191	13091.488540	27.909914
267.227809	13114.181529	27.914932
267.848389	13125.342141	27.919949
268.076183	13157.422272	27.924967
268.266148	13163.329066	27.929984
268.417115	13183.626002	27.935002
268.624662	13207.273527	27.940020
268.851002	13220.965828	27.945037
269.326800	13243.971717	27.950055
269.746156	13260.388448	27.955072
269.875012	13276.355279	27.960090
270.065079	13302.065612	27.965108
270.455416	13321.424799	27.970125
270.743825	13329.996072	27.975143
270.823132	13358.140780	27.980160
271.235356	13378.024360	27.985178
271.092870	13392.928315	27.990196
271.861951	13417.611588	27.995213
272.198612	13447.584530	28.000231
272.093805	13461.270385	28.005248
272.625088	13479.087188	28.010266
272.676529	13500.444290	28.015284
273.313663	13521.515353	28.020301
273.367570	13546.799455	28.025319
273.826491	13557.084086	28.030336
274.000637	13563.502688	28.035354
273.811973	13590.897856	28.040372
273.950876	13612.240627	28.045389
274.508323	13636.399787	28.050407
274.772902	13660.973093	28.055424
275.159740	13685.811453	28.060442
275.136779	13704.478301	28.065460
275.789259	13729.931525	28.070477
276.110090	13757.880918	28.075495
276.644833	13767.120848	28.080512
276.852775	13789.867676	28.085530
277.106059	13818.628966	28.090548
276.806427	13835.190505	28.095565
277.140507	13853.445396	28.100583
277.596329	13874.348350	28.105600
278.271860	13893.307982	28.110618
278.173822	13923.553905	28.115636
278.593821	13935.837309	28.120653
278.922634	13962.876366	28.125671
278.898529	13983.275772	28.130688
279.779066	14002.463217	28.135706
279.783375	14023.554574	28.140724
280.165761	14042.066453	28.145741
280.518403	14059.506845	28.150759
280.739419	14072.192081	28.155776
281.170776	14080.368143	28.160794
281.069767	14094.358072	28.165812
281.794367	14100.937937	28.170829
281.813598	14116.023816	28.175847
281.847805	14134.442133	28.180864
282.389387	14153.146857	28.185882
282.694115	14175.181589	28.190900
282.786309	14182.852771	28.195917
282.806062	14207.046618	28.200935
283.053097	14227.250146	28.205952
283.714390	14239.719214	28.210970
283.594256	14287.154735	28.215988
283.785484	14293.890736	28.221005
284.090281	14315.184899	28.226023
284.490641	14347.989005	28.231040
284.997688	14364.590917	28.236058
285.100529	14394.768209	28.241076
285.225153	14414.771581	28.246093
285.687879	14437.861696	28.251111
285.846682	14468.025131	28.256128
286.198537	14476.140477	28.261146
286.329523	14503.749038	28.266164
286.893169	14533.431073	28.271181
287.476169	14552.149887	28.276199
287.377361	14576.850913	28.281216
288.142521	14598.811578	28.286234
288.073452	14626.669384	28.291252
288.639926	14641.378316	28.296269
288.863209	14659.584675	28.301287
288.937901	14680.528106	28.306304
289.341893	14698.428779	28.311322
289.394077	14724.257159	28.316340
289.992471	14747.927325	28.321357
290.061646	14777.070665	28.326375
290.519853	14788.828274	28.331392
290.976118	14802.890478	28.336410
291.183948	14830.148006	28.341428
291.523693	14852.956450	28.346445
291.621315	14869.495828	28.351463
291.642216	14893.230271	28.356480
292.322025	14916.335564	28.361498
292.457001	14946.368276	28.366516
293.165354	14960.716721	28.371533
293.223093	14987.871689	28.376551
293.372541	15005.078781	28.381568
293.672170	15034.871624	28.386586
293.812309	15053.412135	28.391604
294.228503	15076.153071	28.396621
294.678704	15105.806061	28.401639
294.827853	15128.737853	28.406656
295.356269	15142.709599	28.411674
295.416049	15174.436912	28.416692
295.562365	15187.292990	28.421709
296.181893	15208.673342	28.426727
296.371842	15238.924453	28.431744
296.718171	15253.850056	28.436762
296.718970	15277.230594	28.441780
296.930596	15303.697051	28.446797
297.452297	15326.575333	28.451815
297.699873	15347.112719	28.456832
298.162527	15373.559803	28.461850
298.232726	15410.898553	28.466868
298.587021	15433.240426	28.471885
299.031658	15462.562410	28.476903
298.846688	15483.203085	28.481920
299.534903	15506.550550	28.486938
299.592713	15525.937440	28.491956
300.226330	15549.147418	28.496973
300.375703	15576.697994	28.501991
300.433441	15604.019475	28.507008
300.845793	15616.161976	28.512026
301.294550	15644.518978	28.517044
301.446655	15665.855928	28.522061
301.835229	15685.768295	28.527079
302.018444	15721.922661	28.532096
302.647958	15727.253247	28.537114
302.875673	15760.490679	28.542132
303.040413	15782.166147	28.547149
303.664134	15788.296845	28.552167
303.649188	15826.112454	28.557184
304.224592	15838.710449	28.562202
304.255074	15863.899539	28.567220
304.599057	15883.045608	28.572237
305.152868	15910.480936	28.577255
304.932741	15935.361697	28.582272
305.500061	15957.341170	28.587290
305.991074	15990.833389	28.592308
306.333810	16013.469564	28.597325
306.720470	16031.190142	28.602343
306.775722	16057.172996	28.607360
306.993728	16078.625670	28.612378
307.304860	16108.434312	28.617396
307.941033	16139.472260	28.622413
308.272839	16151.850738	28.627431
308.398728	16184.338252	28.632448
308.766728	16197.606077	28.637466
309.103135	16211.318912	28.642484
309.249538	16249.291625	28.647501
309.939729	16272.428635	28.652519
310.112268	16303.056572	28.657536
310.425179	16311.336900	28.662554
310.710670	16340.086236	28.667572
310.929301	16350.699279	28.672589
311.374061	16369.986859	28.677607
311.683651	16406.137567	28.682624
311.987148	16432.997304	28.687642
312.065357	16452.143889	28.692660
312.639928	16477.226517	28.697677
313.373826	16486.058300	28.702695
313.339460	16520.404620	28.707712
313.710672	16531.536337	28.712730
313.811793	16561.159879	28.717748
314.121605	16584.046609	28.722765
314.745046	16597.850968	28.727783
314.878214	16635.765284	28.732800
315.041567	16648.224035	28.737818
315.678220	16665.010165	28.742836
315.667330	16701.471498	28.747853
315.842581	16715.067984	28.752871
316.095960	16753.363049	28.757888
316.420453	16766.788281	28.762906
316.880583	16798.260138	28.767924
316.840714	16824.816372	28.772941
317.320654	16855.977682	28.777959
317.558503	16883.156394	28.782976
318.142520	16903.059949	28.787994
318.046361	16936.337588	28.793012
318.555014	16968.552061	28.798029
319.075998	16993.582866	28.803047
319.001360	17022.197532	28.808064
319.259736	17046.863619	28.813082
319.870409	17088.027542	28.818100
320.168060	17119.616753	28.823117
320.829979	17145.738925	28.828135
320.977978	17172.209447	28.833152
321.270844	17190.132801	28.838170
321.938207	17207.694686	28.843188
321.988024	17231.701981	28.848205
322.223160	17247.990834	28.853223
322.207035	17275.778131	28.858240
322.881165	17300.497159	28.863258
323.009217	17321.424071	28.868276
323.031413	17350.232927	28.873293
323.992870	17378.924202	28.878311
323.850698	17408.457111	28.883328
324.277833	17431.190026	28.888346
324.678879	17451.931622	28.893364
324.683744	17494.385398	28.898381
325.529626	17509.288685	28.903399
325.353720	17540.427421	28.908416
325.870664	17569.217822	28.913434
326.001317	17596.428055	28.918452
326.498362	17633.174655	28.923469
327.126096	17652.044081	28.928487
327.317771	17681.496995	28.933504
327.555054	17712.591308	28.938522
328.022862	17746.053088	28.943540
328.271516	17775.252398	28.948557
328.476183	17799.553312	28.953575
328.714373	17834.068469	28.958592
329.250367	17860.201575	28.963610
329.769461	17890.544928	28.968628
330.196260	17920.517394	28.973645
330.489286	17942.855460	28.978663
330.616387	17982.640315	28.983680
331.277606	17999.827297	28.988698
331.777412	18019.958950	28.993716
331.580126	18056.813526	28.998733
332.078991	18071.345973	29.003751
332.151525	18100.545052	29.008768
332.375487	18133.308630	29.013786
333.113696	18157.781868	29.018804
333.283470	18197.273262	29.023821
333.377928	18224.077487	29.028839
334.112954	18256.734650	29.033856
334.422123	18280.497170	29.038874
334.678443	18306.081374	29.043892
334.600801	18340.358214	29.048909
335.470366	18372.157821	29.053927
335.740891	18404.010922	29.058944
336.090556	18434.454250	29.063962
336.325174	18460.822627	29.068980
336.550299	18488.321358	29.073997
337.141656	18517.490470	29.079015
337.326047	18544.903026	29.084032
337.960097	18583.494001	29.089050
338.211855	18606.098328	29.094068
338.448108	18639.098911	29.099085
339.218882	18654.997805	29.104103
339.536161	18677.028583	29.109120
339.535896	18713.366442	29.114138
340.125484	18726.068346	29.119156
340.396951	18760.817962	29.124173
340.702420	18770.401351	29.129191
341.189186	18798.197809	29.134208
341.539983	18830.457783	29.139226
341.811126	18848.772760	29.144244
342.072855	18877.199355	29.149261
342.236038	18899.222824	29.154279
342.620640	18925.466216	29.159296
342.861675	18955.703035	29.164314
343.470626	18981.248828	29.169332
343.540046	19011.503117	29.174349
343.534547	19026.383154	29.179367
344.049337	19046.390602	29.184384
344.268985	19081.404855	29.189402
344.516488	19108.235615	29.194420
344.896988	19145.812016	29.199437
345.162109	19177.093632	29.204455
345.677843	19206.856626	29.209472
345.607546	19242.616028	29.214490
346.300513	19267.374279	29.219508
346.474877	19312.391704	29.224525
346.888329	19334.066900	29.229543
347.299270	19367.694270	29.234560
347.469776	19403.866626	29.239578
348.216040	19427.421275	29.244596
348.141587	19467.879946	29.249613
348.709809	19507.571769	29.254631
349.527387	19535.524382	29.259648
349.722239	19562.123371	29.264666
350.241111	19583.641128	29.269684
350.585912	19611.121898	29.274701
351.049206	19647.377176	29.279719
351.587219	19675.357375	29.284736
351.757077	19697.664571	29.289754
352.116027	19717.288708	29.294772
352.647120	19737.232799	29.299789
352.974617	19759.474573	29.304807
353.429295	19787.711545	29.309824
353.564767	19807.338091	29.314842
354.159471	19832.490246	29.319860
354.585336	19864.139110	29.324877
354.764075	19882.098438	29.329895
354.961988	19905.987314	29.334912
355.371432	19929.935809	29.339930
355.576968	19958.406648	29.344948
355.677170	19995.058587	29.349965
355.930808	20027.314874	29.354983
356.367226	20054.002366	29.360000
356.822063	20088.241945	29.365018
356.991556	20115.583860	29.370036
357.245475	20148.217142	29.375053
357.507887	20189.545689	29.380071
357.991067	20225.888792	29.385088
358.360797	20262.583417	29.390106
358.672659	20290.483826	29.395124
359.151878	20333.473292	29.400141
359.370133	20367.438846	29.405159
359.888074	20399.680483	29.410176
360.233073	20438.872246	29.415194
360.892332	20469.595975	29.420212
361.024099	20501.075560	29.425229
361.441112	20526.838372	29.430247
361.951245	20560.377613	29.435264
362.319494	20591.343656	29.440282
362.832868	20620.775301	29.445300
363.041382	20661.043377	29.450317
363.495762	20689.934653	29.455335
364.055046	20712.905585	29.460352
364.374016	20739.957318	29.465370
364.679060	20772.457215	29.470388
364.944424	20799.748110	29.475405
365.056800	20826.911432	29.480423
365.730951	20867.206995	29.485440
365.869558	20892.642771	29.490458
366.513962	20918.434769	29.495476
366.420332	20953.599373	29.500493
366.778257	20987.126815	29.505511
367.345603	21023.296888	29.510528
367.583955	21049.033307	29.515546
368.043441	21073.404011	29.520564
368.324512	21103.101991	29.525581
368.909515	21132.973613	29.530599
369.230111	21158.855835	29.535616
369.750941	21187.087364	29.540634
369.884219	21211.177994	29.545652
370.016173	21240.311205	29.550669
370.195783	21279.182264	29.555687
370.678365	21301.316844	29.560704
370.680606	21345.523071	29.565722
371.285794	21378.849542	29.570740
371.785887	21421.898245	29.575757
371.987621	21459.039536	29.580775
372.455899	21475.539890	29.585792
372.495010	21522.507647	29.590810
373.285472	21556.108116	29.595828
373.833061	21595.412520	29.600845
374.032998	21631.447611	29.605863
374.597106	21658.665223	29.610880
375.010518	21697.605767	29.615898
375.486549	21729.368090	29.620916
376.020981	21763.060224	29.625933
376.038651	21805.138045	29.630951
376.790361	21832.624474	29.635968
376.622226	21868.687875	29.640986
377.385608	21899.898394	29.646004
377.839672	21935.721782	29.651021
378.240712	21974.091063	29.656039
378.933349	21992.374397	29.661056
379.241253	22020.585795	29.666074
379.642021	22054.899811	29.671092
380.004197	22080.595232	29.676109
380.130315	22107.401980	29.681127
380.649230	22135.075649	29.686144
381.063647	22170.440940	29.691162
381.357254	22191.086351	29.696180
381.638530	22226.581017	29.701197
381.970382	22267.078485	29.706215
382.631641	22282.767169	29.711232
383.058951	22325.443898	29.716250
383.438779	22355.556625	29.721268
383.765666	22388.245231	29.726285
383.954837	22425.277188	29.731303
384.224345	22449.216155	29.736320
384.518374	22490.956648	29.741338
384.993884	22523.233016	29.746356
385.297929	22554.752560	29.751373
385.858486	22602.428577	29.756391
386.269933	22637.363279	29.761408
386.352338	22667.946801	29.766426
387.086876	22690.692740	29.771444
387.464315	22727.954377	29.776461
387.718316	22766.291441	29.781479
388.052266	22801.073736	29.786496
388.135866	22838.636544	29.791514
388.330488	22874.605771	29.796532
388.980064	22916.184392	29.801549
389.175208	22961.269598	29.806567
389.759697	22993.475210	29.811584
390.416496	23034.502594	29.816602
390.592799	23071.713121	29.821620
391.184473	23107.098333	29.826637
391.577883	23146.378235	29.831655
392.433070	23180.303942	29.836672
392.457804	23209.448816	29.841690
392.971206	23244.259086	29.846708
393.480224	23266.063866	29.851725
393.739410	23299.277920	29.856743
394.091720	23328.947509	29.861760
394.417475	23360.990063	29.866778
394.461951	23388.181337	29.871796
395.201157	23412.217386	29.876813
395.249689	23456.429325	29.881831
395.609743	23493.542554	29.886848
395.991687	23530.560779	29.891866
396.286844	23568.870760	29.896884
396.683538	23594.567490	29.901901
397.198018	23640.226105	29.906919
397.508328	23674.432206	29.911936
398.331935	23720.948196	29.916954
397.901856	23756.374546	29.921972
398.885249	23788.138754	29.926989
399.472170	23832.051250	29.932007
399.519980	23859.466650	29.937024
399.987137	23890.887554	29.942042
400.401921	23938.077347	29.947060
401.036341	23960.516703	29.952077
401.253805	24007.436566	29.957095
401.485327	24041.205427	29.962112
402.333602	24087.923341	29.967130
402.631566	24120.719407	29.972148
403.099517	24154.307435	29.977165
403.169240	24198.530400	29.982183
403.870384	24240.835440	29.987200
404.444091	24279.553512	29.992218
404.652316	24316.834009	29.997236
405.323042	24356.346775	30.002253
405.564359	24396.214559	30.007271
406.236295	24415.046425	30.012288
406.569603	24450.543419	30.017306
406.542581	24494.202817	30.022324
407.041002	24523.342501	30.027341
407.380404	24561.431332	30.032359
408.260626	24587.593606	30.037376
408.598609	24629.593841	30.042394
409.020540	24680.370656	30.047412
409.712998	24698.007203	30.052429
410.095431	24741.369220	30.057447
410.505388	24772.107314	30.062464
411.246972	24807.032826	30.067482
411.433335	24830.477933	30.072500
411.888697	24857.136735	30.077517
412.141972	24895.678981	30.082535
412.565168	24926.658027	30.087552
413.016478	24960.098994	30.092570
413.483690	24993.575243	30.097588
413.841169	25022.512006	30.102605
413.689142	25058.724557	30.107623
414.084661	25088.345891	30.112640
414.731224	25119.950689	30.117658
414.883335	25167.177875	30.122676
415.093266	25198.861386	30.127693
415.378125	25246.918445	30.132711
416.256813	25292.246780	30.137728
416.426784	25325.198808	30.142746
416.634886	25379.309197	30.147764
417.699567	25419.424752	30.152781
418.066130	25462.255002	30.157799
418.155163	25499.444240	30.162816
418.942022	25530.219097	30.167834
419.288579	25571.248716	30.172852
419.740737	25606.151206	30.177869
419.965928	25652.112243	30.182887
420.376409	25679.060477	30.187904
420.960215	25718.388895	30.192922
421.255473	25756.938740	30.197940
421.777987	25772.812902	30.202957
421.781032	25814.218528	30.207975
422.171642	25850.510116	30.212992
422.973702	25887.683128	30.218010
423.154446	25925.097832	30.223028
423.858389	25956.104821	30.228045
424.461801	25990.194485	30.233063
424.766094	26025.611213	30.238080
425.252981	26063.205818	30.243098
425.308327	26108.300352	30.248116
426.049883	26143.212816	30.253133
426.292864	26169.265318	30.258151
426.438205	26212.389543	30.263168
426.705600	26243.636475	30.268186
427.039931	26298.583686	30.273204
427.333639	26331.192259	30.278221
427.721505	26381.408790	30.283239
428.476297	26427.284247	30.288256
429.200802	26479.426305	30.293274
429.469470	26520.896914	30.298292
430.171774	26562.740632	30.303309
430.413870	26608.840212	30.308327
430.766178	26645.512031	30.313344
431.171479	26683.067861	30.318362
431.644720	26741.207854	30.323380
431.890945	26786.808822	30.328397
432.376259	26822.026885	30.333415
433.150530	26868.944415	30.338432
433.563093	26907.171431	30.343450
433.804261	26951.969281	30.348468
434.576987	26988.455537	30.353485
435.278567	27038.461180	30.358503
435.582720	27075.242822	30.363520
435.905851	27102.766081	30.368538
436.179442	27154.852307	30.373556
436.491482	27188.475216	30.378573
436.685333	27233.862056	30.383591
437.417226	27286.213522	30.388608
437.962782	27331.655978	30.393626
438.233729	27380.405809	30.398644
438.597914	27422.279169	30.403661
439.193057	27463.070247	30.408679
439.962575	27505.895659	30.413696
440.598328	27538.538229	30.418714
440.802206	27583.123058	30.423732
441.325395	27625.238736	30.428749
441.468667	27665.767527	30.433767
442.014245	27696.816468	30.438784
442.377440	27737.807462	30.443802
442.734960	27792.512665	30.448820
443.237051	27826.972882	30.453837
443.930328	27880.988717	30.458855
444.470776	27928.932062	30.463872
444.790672	27961.864298	30.468890
445.136156	28008.284878	30.473908
446.020064	28044.038848	30.478925
446.400520	28080.305244	30.483943
446.778480	28112.045149	30.488960
447.235217	28147.163373	30.493978
447.561941	28191.972344	30.498996
448.052225	28225.167114	30.504013
448.634352	28272.470412	30.509031
448.662704	28315.013513	30.514048
449.007194	28350.008758	30.519066
449.378722	28394.700420	30.524084
449.754568	28438.763687	30.529101
450.326398	28491.769914	30.534119
450.596953	28525.963820	30.539136
451.219964	28562.796794	30.544154
451.386856	28609.904723	30.549172
451.576719	28658.327678	30.554189
452.140463	28692.590119	30.559207
452.764620	28734.887370	30.564224
453.490251	28776.224644	30.569242
453.880788	28820.100309	30.574260
454.264108	28859.727731	30.579277
454.783060	28903.058653	30.584295
454.774060	28953.613296	30.589312
455.821036	28998.248360	30.594330
455.980675	29048.043444	30.599348
456.438541	29097.634731	30.604365
456.988201	29132.165374	30.609383
457.388560	29187.224361	30.614400
458.222788	29227.711844	30.619418
457.986573	29276.197553	30.624436
458.779540	29319.752329	30.629453
459.375736	29359.544416	30.634471
459.514079	29417.319696	30.639488
460.482837	29447.219590	30.644506
460.598044	29512.242731	30.649524
461.010360	29555.271111	30.654541
461.401395	29609.449581	30.659559
461.742396	29661.121990	30.664576
462.785165	29712.520671	30.669594
462.921626	29753.175320	30.674612
463.205310	29802.513476	30.679629
463.877207	29850.380399	30.684647
464.302765	29907.084387	30.689664
464.768827	29951.007177	30.694682
464.818524	30008.527740	30.699700
465.718085	30050.138971	30.704717
466.702219	30105.388189	30.709735
466.835019	30153.193706	30.714752
467.436384	30190.794061	30.719770
467.948296	30245.658071	30.724788
468.731796	30294.842333	30.729805
468.883893	30336.268737	30.734823
468.978637	30381.960953	30.739840
469.367294	30430.343282	30.744858
470.198656	30482.782529	30.749876
470.798113	30523.453839	30.754893
471.330886	30571.020771	30.759911
471.668317	30624.302563	30.764928
472.308540	30666.191651	30.769946
472.572021	30707.168239	30.774964
473.226691	30760.738704	30.779981
474.106963	30803.197341	30.784999
474.102795	30853.949114	30.790016
474.655253	30899.200928	30.795034
475.048376	30946.911881	30.800052
475.626753	30985.025726	30.805069
476.158827	31037.194320	30.810087
476.358388	31093.191741	30.815104
476.810964	31136.185775	30.820122
477.239955	31183.907209	30.825140
477.860137	31227.104062	30.830157
478.247996	31278.808172	30.835175
478.525699	31325.586361	30.840192
478.952490	31380.483765	30.845210
479.416663	31427.976012	30.850228
479.866766	31481.923289	30.855245
480.482802	31530.299405	30.860263
481.006029	31588.065442	30.865280
481.449447	31638.401470	30.870298
481.848637	31681.743284	30.875316
482.201308	31739.304543	30.880333
483.136963	31782.005646	30.885351
483.456567	31828.610997	30.890368
483.905403	31867.391875	30.895386
484.381639	31908.459101	30.900404
484.782407	31959.011353	30.905421
485.156045	32006.075225	30.910439
485.703336	32057.297696	30.915456
485.941091	32104.519997	30.920474
486.403088	32158.379014	30.925492
486.854934	32208.917215	30.930509
487.522490	32261.918967	30.935527
488.098801	32316.501075	30.940544
488.755140	32365.245146	30.945562
489.029096	32418.369294	30.950580
489.386567	32464.048655	30.955597
489.851246	32509.543151	30.960615
489.936189	32573.945160	30.965632
490.852497	32634.360123	30.970650
491.457566	32695.423186	30.975668
491.811449	32746.547118	30.980685
492.410649	32795.248181	30.985703
493.049567	32861.941985	30.990720
493.622127	32911.209460	30.995738
493.952018	32966.080472	31.000756
494.410322	33023.334945	31.005773
495.055855	33060.037917	31.010791
495.795946	33119.088925	31.015808
495.988745	33167.631054	31.020826
496.893498	33216.831783	31.025844
497.337643	33271.893101	31.030861
498.088983	33324.467616	31.035879
498.496889	33376.890845	31.040896
498.632718	33422.713477	31.045914
499.437885	33470.315699	31.050932
499.727791	33525.043577	31.055949
500.240882	33570.611666	31.060967
500.286854	33632.205937	31.065984
501.093110	33684.406369	31.071002
501.802184	33738.541696	31.076020
502.418590	33788.568018	31.081037
502.777172	33831.331676	31.086055
503.413026	33898.099288	31.091072
503.879749	33945.837676	31.096090
504.630691	33993.308260	31.101108
504.744622	34055.053683	31.106125
505.507090	34101.692686	31.111143
505.805978	34151.782033	31.116160
506.579222	34203.844281	31.121178
507.562315	34254.344557	31.126196
507.572777	34300.363749	31.131213
508.029869	34348.805392	31.136231
508.671060	34402.723590	31.141248
509.096541	34437.354573	31.146266
509.603688	34493.254986	31.151284
509.854211	34545.013399	31.156301
510.547129	34604.821902	31.161319
510.969609	34657.117081	31.166336
511.074780	34716.316299	31.171354
511.998660	34767.206525	31.176372
512.242995	34822.750656	31.181389
513.049836	34877.037356	31.186407
513.345915	34928.527397	31.191424
513.701256	34991.110278	31.196442
514.298949	35039.505273	31.201460
514.811916	35101.642719	31.206477
515.398103	35147.013369	31.211495
515.846825	35203.534757	31.216512
516.153176	35257.536177	31.221530
516.883399	35299.077290	31.226548
517.035970	35364.967762	31.231565
518.087555	35406.601123	31.236583
518.295331	35457.119464	31.241600
518.547540	35515.779398	31.246618
519.520087	35565.584481	31.251636
519.859798	35616.857818	31.256653
520.494719	35666.921034	31.261671
520.617624	35728.522384	31.266688
520.949480	35784.506313	31.271706
521.948327	35835.096803	31.276724
522.659587	35907.647627	31.281741
522.820348	35950.426970	31.286759
523.802867	36020.178104	31.291776
524.030574	36075.047129	31.296794
525.048661	36119.218879	31.301812
525.275517	36183.534616	31.306829
525.583398	36225.813693	31.311847
526.270013	36280.730498	31.316864
526.548839	36334.739696	31.321882
527.237983	36398.462095	31.326900
527.506677	36451.835774	31.331917
528.445104	36516.647250	31.336935
528.939710	36575.977501	31.341952
529.423329	36639.166641	31.346970
530.015744	36683.659548	31.351988
530.631331	36751.886648	31.357005
531.013844	36816.055782	31.362023
531.496979	36864.477786	31.367040
532.106997	36920.526517	31.372058
532.549134	36967.434267	31.377076
532.976724	37037.824025	31.382093
533.739942	37094.409760	31.387111
534.534905	37162.703414	31.392128
534.605697	37230.691050	31.397146
535.173983	37283.310592	31.402164
535.712615	37345.846047	31.407181
536.883981	37399.180469	31.412199
537.150871	37463.150078	31.417216
537.446452	37520.265875	31.422234
538.497800	37573.017803	31.427252
538.805903	37633.392407	31.432269
539.354013	37691.978862	31.437287
539.939386	37743.040811	31.442304
540.135946	37803.885801	31.447322
540.505906	37854.172509	31.452340
541.037435	37923.980344	31.457357
541.776571	37990.730231	31.462375
541.977928	38064.459869	31.467392
542.866904	38129.013833	31.472410
543.559957	38186.444726	31.477428
543.904294	38250.142296	31.482445
544.547021	38303.238568	31.487463
545.089143	38372.528703	31.492480
545.376111	38434.724445	31.497498
546.238034	38496.323378	31.502516
546.644758	38561.290101	31.507533
547.251383	38616.972148	31.512551
547.742783	38678.857119	31.517568
547.883904	38757.514274	31.522586
548.852320	38813.695771	31.527604
549.253937	38882.092521	31.532621
550.136247	38941.618860	31.537639
550.882021	38992.780875	31.542656
551.152606	39065.104715	31.547674
552.075811	39119.773142	31.552692
552.254984	39178.684256	31.557709
552.664771	39230.720098	31.562727
553.421477	39300.038217	31.567744
553.584362	39354.365962	31.572762
554.272643	39403.429981	31.577780
554.723827	39467.751757	31.582797
555.316046	39517.485411	31.587815
556.057346	39571.945378	31.592832
556.507172	39634.175065	31.597850
557.051270	39693.661951	31.602868
557.367267	39750.771866	31.607885
557.594201	39810.251629	31.612903
558.269753	39880.867009	31.617920
558.991720	39956.165947	31.622938
559.887181	40028.633260	31.627956
559.893062	40092.169098	31.632973
560.885110	40156.154405	31.637991
561.263306	40219.629079	31.643008
561.828178	40287.486333	31.648026
562.510061	40346.778908	31.653044
562.762937	40417.662007	31.658061
563.277458	40489.212382	31.663079
564.179835	40559.874916	31.668096
564.586193	40629.470684	31.673114
565.362015	40695.343578	31.678132
565.883626	40773.434980	31.683149
566.439901	40834.833470	31.688167
567.031783	40904.178591	31.693184
567.459817	40969.570173	31.698202
568.237543	41035.459751	31.703220
568.660017	41109.600680	31.708237
569.361297	41175.695982	31.713255
570.099996	41244.434046	31.718272
570.419096	41311.919006	31.723290
570.846450	41382.035037	31.728308
571.675790	41462.509336	31.733325
571.993934	41536.726063	31.738343
573.102989	41603.955102	31.743360
573.191198	41673.424326	31.748378
574.156481	41739.547415	31.753396
574.682599	41818.056055	31.758413
575.055287	41882.411861	31.763431
576.128360	41949.493410	31.768448
576.482198	42026.901190	31.773466
577.098691	42076.129426	31.778484
577.876630	42144.968524	31.783501
578.265782	42210.623487	31.788519
579.123133	42274.467931	31.793536
579.212870	42350.746289	31.798554
579.997094	42404.800234	31.803572
580.704668	42479.032064	31.808589
581.082560	42543.364039	31.813607
581.944533	42609.346302	31.818624
582.657707	42677.184616	31.823642
583.011274	42739.194408	31.828660
583.744437	42811.623700	31.833677
584.036777	42889.149428	31.838695
584.655135	42938.957421	31.843712
585.088498	43014.906957	31.848730
585.833701	43074.387220	31.853748
586.292533	43147.740936	31.858765
586.769245	43224.397705	31.863783
587.449478	43296.275630	31.868800
587.574554	43369.565458	31.873818
588.232862	43440.759263	31.878836
589.137093	43521.151141	31.883853
589.681577	43596.866796	31.888871
590.624281	43660.247201	31.893888
591.031151	43735.736752	31.898906
591.599945	43796.063112	31.903924
592.655680	43859.674928	31.908941
592.956491	43924.715890	31.913959
593.591240	43970.217162	31.918976
593.988327	44037.828543	31.923994
594.762826	44089.135666	31.929012
595.396446	44162.271832	31.934029
595.495400	44231.644595	31.939047
595.822310	44282.584251	31.944064
596.660335	44355.864173	31.949082
597.189385	44437.569277	31.954100
597.665943	44503.315712	31.959117
598.037007	44583.658270	31.964135
598.955639	44652.716989	31.969152
599.143047	44738.117443	31.974170
600.057166	44802.665273	31.979188
600.751547	44882.311463	31.984205
601.183526	44957.072359	31.989223
602.185746	45027.002757	31.994240
602.962972	45097.115892	31.999258
603.583646	45173.283154	32.004276
604.229364	45238.704192	32.009293
604.925576	45313.684871	32.014311
605.583153	45377.942405	32.019328
605.710704	45449.910541	32.024346
606.673717	45524.099540	32.029364
606.952353	45592.550790	32.034381
607.502512	45670.484263	32.039399
608.280244	45744.190068	32.044416
609.185442	45819.618158	32.049434
609.354530	45902.083869	32.054452
610.033755	45966.046148	32.059469
610.627554	46051.303198	32.064487
611.474840	46126.511573	32.069504
612.373680	46193.523472	32.074522
612.581090	46260.166854	32.079540
613.435228	46335.087561	32.084557
613.680151	46420.403991	32.089575
614.701848	46494.220773	32.094592
615.171739	46564.235460	32.099610
615.745589	46645.674281	32.104628
616.718086	46717.586384	32.109645
616.819286	46791.903987	32.114663
617.609199	46866.104777	32.119680
617.961946	46949.002550	32.124698
618.726141	47019.304965	32.129716
619.464338	47092.526753	32.134733
619.780714	47183.184394	32.139751
620.664031	47254.273257	32.144768
620.788024	47341.094925	32.149786
621.622978	47418.915823	32.154804
622.342015	47503.271260	32.159821
622.809609	47593.921625	32.164839
624.223362	47675.835400	32.169856
624.724321	47750.978021	32.174874
625.347666	47822.115171	32.179892
625.963677	47896.209788	32.184909
626.614276	47975.658303	32.189927
627.199333	48047.383721	32.194944
627.900436	48116.715283	32.199962
628.078113	48205.085800	32.204980
629.105876	48267.937013	32.209997
629.549184	48352.218647	32.215015
630.062649	48412.600452	32.220032
630.511325	48495.312204	32.225050
631.196065	48582.100421	32.230068
632.033514	48662.307270	32.235085
632.177253	48731.070037	32.240103
633.131156	48810.354980	32.245120
633.753909	48886.603089	32.250138
634.224921	48961.569075	32.255156
635.207341	49021.985753	32.260173
635.466936	49101.292016	32.265191
636.190052	49177.167785	32.270208
636.471376	49254.114976	32.275226
637.071101	49328.634724	32.280244
637.949861	49411.418234	32.285261
638.264189	49501.566052	32.290279
638.735863	49579.231584	32.295296
639.442765	49664.817678	32.300314
640.140656	49746.621864	32.305332
641.036824	49831.378307	32.310349
641.447530	49922.712350	32.315367
642.211208	50009.336023	32.320384
642.802183	50096.667728	32.325402
643.413163	50190.815687	32.330420
644.359296	50274.618264	32.335437
644.661164	50360.625044	32.340455
645.422367	50447.023676	32.345472
646.331319	50531.338882	32.350490
646.835269	50624.464338	32.355508
647.429357	50701.668773	32.360525
648.045100	50792.148612	32.365543
648.621509	50883.184976	32.370560
649.533723	50977.147944	32.375578
649.896134	51068.568028	32.380596
650.661859	51154.236263	32.385613
651.001386	51248.011007	32.390631
651.694039	51335.593643	32.395648
652.383719	51433.765081	32.400666
653.396010	51528.465927	32.405684
654.436580	51611.532160	32.410701
654.927833	51706.977087	32.415719
655.883055	51783.999730	32.420736
656.594801	51869.730587	32.425754
657.148285	51962.588924	32.430772
658.105658	52038.771985	32.435789
658.330541	52128.975239	32.440807
658.842804	52207.810178	32.445824
659.809907	52296.312009	32.450842
660.248784	52386.651626	32.455860
660.731836	52478.551145	32.460877
661.540201	52558.425160	32.465895
662.484385	52644.872779	32.470912
663.053156	52723.725722	32.475930
663.492028	52822.248893	32.480948
664.571670	52906.868363	32.485965
665.308487	52994.362688	32.490983
665.680048	53086.384590	32.496000
666.609223	53158.804892	32.501018
666.856399	53247.739706	32.506036
667.692741	53329.602396	32.511053
668.300793	53422.262774	32.516071
669.092069	53521.369275	32.521088
669.840230	53599.071448	32.526106
670.371055	53692.251319	32.531124
671.248062	53775.423306	32.536141
671.534564	53862.237819	32.541159
672.128178	53955.673913	32.546176
673.014040	54034.245889	32.551194
673.241362	54136.797438	32.556212
674.021903	54222.122838	32.561229
674.979886	54315.146534	32.566247
675.241948	54414.837908	32.571264
675.899675	54508.619842	32.576282
676.443214	54599.053407	32.581300
677.369045	54691.363899	32.586317
678.154298	54767.661853	32.591335
678.651465	54859.393244	32.596352
679.563037	54937.958247	32.601370
680.300837	55035.438394	32.606388
681.138120	55119.829460	32.611405
681.259209	55195.632355	32.616423
682.291960	55292.433115	32.621440
683.032300	55362.238938	32.626458
683.301254	55458.073737	32.631476
684.076825	55549.888640	32.636493
684.669650	55634.834153	32.641511
685.138275	55732.874074	32.646528
685.975590	55831.182062	32.651546
686.673746	55927.478899	32.656564
687.476446	56014.546032	32.661581
688.485804	56112.763764	32.666599
688.999596	56201.446589	32.671616
689.629781	56293.516457	32.676634
690.268025	56388.264658	32.681652
690.993099	56486.221631	32.686669
691.802990	56574.914005	32.691687
692.341351	56674.564692	32.696704
693.190009	56767.750676	32.701722
693.800228	56867.851733	32.706740
694.408293	56959.536548	32.711757
695.417631	57058.176003	32.716775
696.017220	57166.874393	32.721792
696.651330	57249.842043	32.726810
697.444958	57365.460571	32.731828
698.172920	57449.171834	32.736845
698.933060	57548.158254	32.741863
699.314707	57645.842792	32.746880
700.410689	57738.581624	32.751898
701.153146	57849.490824	32.756916
701.633813	57947.615448	32.761933
702.264968	58041.178267	32.766951
702.400741	58140.384641	32.771968
703.353684	58237.156009	32.776986
704.259145	58335.610385	32.782004
705.416963	58443.717775	32.787021
706.013098	58547.949926	32.792039
706.492429	58650.362912	32.797056
707.438910	58751.043378	32.802074
708.147652	58855.625034	32.807092
708.763838	58938.457263	32.812109
709.757215	59048.459428	32.817127
710.258835	59148.495009	32.822144
711.199259	59242.220795	32.827162
711.593534	59344.834646	32.832180
712.622234	59442.484049	32.837197
713.228673	59538.352029	32.842215
713.782174	59630.873310	32.847232
714.746096	59722.164239	32.852250
715.562794	59843.316848	32.857268
716.251872	59923.966956	32.862285
716.884765	60022.196553	32.867303
717.439546	60114.239498	32.872320
718.558894	60210.032126	32.877338
719.197184	60314.986896	32.882356
719.824517	60405.331666	32.887373
720.625061	60506.500053	32.892391
721.526396	60596.155679	32.897408
722.432521	60689.287076	32.902426
723.458148	60786.260858	32.907444
723.848466	60872.671415	32.912461
724.261730	60962.738049	32.917479
724.913993	61046.558892	32.922496
725.771371	61130.655852	32.927514
726.868715	61212.652990	32.932532
727.076116	61289.185071	32.937549
727.738127	61381.468819	32.942567
728.228710	61477.352453	32.947584
728.678161	61563.357952	32.952602
729.561368	61665.504419	32.957620
730.049989	61753.002219	32.962637
731.044668	61841.554402	32.967655
731.372355	61951.170401	32.972672
732.292789	62052.648966	32.977690
732.729001	62148.968222	32.982708
733.263031	62260.056078	32.987725
734.485405	62358.901007	32.992743
734.890806	62465.251669	32.997760
735.309367	62570.715778	33.002778
736.235545	62684.180918	33.007796
736.956484	62799.791834	33.012813
737.873774	62909.928543	33.017831
738.438915	63030.263019	33.022848
739.270315	63135.585875	33.027866
739.981510	63241.807785	33.032884
740.627262	63357.693427	33.037901
741.821429	63475.669804	33.042919
742.441721	63588.678501	33.047936
743.321323	63701.373109	33.052954
743.813180	63810.617843	33.057972
745.114353	63916.201995	33.062989
745.891158	64013.839014	33.068007
746.580501	64128.722990	33.073024
747.515231	64231.897713	33.078042
748.426511	64334.748114	33.083060
748.998292	64443.325530	33.088077
749.921166	64539.189813	33.093095
750.535207	64641.547252	33.098112
751.441605	64745.095857	33.103130
752.089173	64856.387481	33.108148
752.778848	64970.492176	33.113165
753.572921	65067.164077	33.118183
754.309581	65180.061034	33.123200
755.084046	65276.351525	33.128218
755.955420	65375.528111	33.133236
756.560341	65482.455483	33.138253
757.414025	65592.756030	33.143271
758.069728	65703.930711	33.148288
758.933604	65811.771530	33.153306
759.785493	65924.811495	33.158324
760.296592	66030.448551	33.163341
761.112360	66133.380515	33.168359
762.054004	66236.785280	33.173376
762.859501	66347.767904	33.178394
763.538312	66459.195649	33.183412
764.214418	66561.596473	33.188429
765.323656	66675.950846	33.193447
765.908753	66786.713037	33.198464
766.624676	66885.486250	33.203482
767.125665	66984.061556	33.208500
768.154190	67103.204883	33.213517
768.311699	67196.343950	33.218535
769.477494	67321.130575	33.223552
770.236943	67443.816579	33.228570
770.945596	67544.029255	33.233588
771.488193	67657.249812	33.238605
772.435021	67762.507360	33.243623
773.246786	67877.050222	33.248640
773.878496	67996.182029	33.253658
774.970675	68104.945209	33.258676
775.339864	68218.943514	33.263693
776.413767	68316.178391	33.268711
777.059538	68432.123719	33.273728
777.780722	68530.214574	33.278746
778.553399	68627.639803	33.283764
779.070954	68738.170473	33.288781
780.342776	68841.280468	33.293799
781.013291	68955.953680	33.298816
781.376103	69066.347255	33.303834
782.529093	69173.215317	33.308852
783.089000	69284.456301	33.313869
783.741192	69390.238546	33.318887
784.821104	69499.598925	33.323904
785.359406	69612.520780	33.328922
786.198304	69724.976190	33.333940
786.832645	69835.885258	33.338957
788.014589	69941.867150	33.343975
788.771656	70061.261664	33.348992
789.390427	70175.279728	33.354010
790.241986	70292.611194	33.359028
790.865227	70412.036120	33.364045
791.905709	70514.914240	33.369063
792.690408	70632.511554	33.374080
793.432866	70761.106471	33.379098
794.373383	70876.776022	33.384116
794.766153	70995.805998	33.389133
795.959814	71118.883964	33.394151
796.745907	71233.600838	33.399168
797.443972	71352.133318	33.404186
798.539333	71467.704549	33.409204
799.090560	71595.716367	33.414221
800.211779	71709.444450	33.419239
800.849562	71824.682239	33.424256
801.536986	71940.146408	33.429274
802.297001	72054.220614	33.434292
802.837846	72181.649509	33.439309
803.943561	72295.686779	33.444327
804.817296	72413.019790	33.449344
805.419328	72545.297402	33.454362
806.382795	72666.031828	33.459380
807.585619	72792.823613	33.464397
808.567608	72895.286397	33.469415
809.122489	73019.903721	33.474432
809.820840	73136.011167	33.479450
810.982799	73255.565061	33.484468
811.579615	73369.837592	33.489485
812.691526	73478.428664	33.494503
813.320755	73595.979247	33.499520
814.080125	73715.127933	33.504538
815.132907	73830.845272	33.509556
815.725846	73943.009146	33.514573
816.756411	74061.330655	33.519591
817.618840	74175.405359	33.524608
818.110954	74294.266212	33.529626
819.539641	74402.227637	33.534644
819.898459	74529.883764	33.539661
820.419054	74645.168497	33.544679
821.439433	74768.080750	33.549696
822.453255	74878.832676	33.554714
823.319753	74996.244007	33.559732
823.869337	75118.723795	33.564749
825.043736	75234.010997	33.569767
825.825880	75348.060795	33.574784
826.189560	75471.578914	33.579802
827.248241	75577.526479	33.584820
827.692429	75699.691713	33.589837
828.703085	75819.790590	33.594855
829.731786	75941.873137	33.599872
830.591230	76063.149467	33.604890
831.179537	76165.768539	33.609908
831.946054	76278.073720	33.614925
833.263427	76389.567316	33.619943
834.017694	76498.662554	33.624960
834.538387	76610.674851	33.629978
835.554882	76716.388170	33.634996
835.936125	76832.561243	33.640013
836.742177	76947.159281	33.645031
838.202537	77062.984303	33.650048
838.441286	77184.565496	33.655066
839.192106	77300.205494	33.660084
839.823664	77417.927853	33.665101
840.935327	77550.758476	33.670119
841.551535	77675.569073	33.675136
841.957840	77800.895811	33.680154
843.265010	77933.746979	33.685172
843.591253	78066.160255	33.690189
844.612330	78185.852703	33.695207
845.191568	78328.574178	33.700224
846.012197	78468.264646	33.705242
847.135371	78606.957105	33.710260
847.440452	78745.975493	33.715277
848.384005	78884.319832	33.720295
849.260821	79023.498403	33.725312
849.855916	79178.912046	33.730330
850.850371	79322.665512	33.735348
851.847254	79474.605135	33.740365
852.680469	79615.470919	33.745383
853.682986	79767.386276	33.750400
854.224001	79924.420778	33.755418
855.415262	80067.551793	33.760436
856.263278	80223.354629	33.765453
857.170377	80360.461480	33.770471
858.281970	80513.464541	33.775488
859.036207	80667.343811	33.780506
859.908978	80791.920465	33.785524
860.422107	80949.827035	33.790541
861.757615	81086.133566	33.795559
862.826149	81242.583830	33.800576
863.602252	81389.967220	33.805594
864.609747	81540.381605	33.810612
865.249403	81680.615277	33.815629
865.927950	81832.427196	33.820647
867.135719	81970.076044	33.825664
867.533151	82125.789261	33.830682
868.651391	82265.637363	33.835700
869.486137	82423.880519	33.840717
870.444128	82576.138299	33.845735
871.513552	82724.607917	33.850752
872.136107	82874.455717	33.855770
872.842670	83020.564096	33.860788
874.080552	83175.645606	33.865805
874.702324	83322.851818	33.870823
875.503239	83464.948801	33.875840
875.743285	83632.909250	33.880858
877.144499	83784.121022	33.885876
878.398562	83937.015813	33.890893
879.186725	84088.368923	33.895911
880.059336	84238.209517	33.900928
881.263586	84390.179117	33.905946
882.056001	84541.844513	33.910964
882.985880	84693.076892	33.915981
883.854296	84843.858523	33.920999
884.412602	84993.388979	33.926016
885.234334	85147.293357	33.931034
886.062719	85294.971442	33.936052
887.496079	85450.826765	33.941069
888.457800	85594.409790	33.946087
889.463048	85730.222575	33.951104
890.244720	85873.235969	33.956122
890.888532	86007.351061	33.961140
891.845944	86146.920136	33.966157
892.739654	86279.331277	33.971175
893.286469	86418.602863	33.976192
893.966821	86565.484502	33.981210
895.050721	86707.826545	33.986228
895.969974	86851.728022	33.991245
896.700971	87000.901016	33.996263
897.763370	87146.204397	34.001280
898.306712	87299.903155	34.006298
899.141389	87451.624685	34.011316
900.126249	87610.909704	34.016333
900.784026	87770.730823	34.021351
901.816372	87931.965536	34.026368
902.917866	88096.138849	34.031386
903.868493	88249.314452	34.036404
904.985436	88398.596959	34.041421
905.473380	88561.432105	34.046439
906.492893	88720.845407	34.051456
907.415657	88889.508922	34.056474
908.505792	89045.634601	34.061492
908.962774	89205.878272	34.066509
909.736290	89371.348669	34.071527
911.034677	89530.271931	34.076544
911.984822	89703.651454	34.081562
913.191148	89858.643058	34.086580
914.021487	90027.488096	34.091597
914.575008	90186.861654	34.096615
915.892359	90352.375458	34.101632
916.469032	90523.803776	34.106650
917.438328	90682.327080	34.111668
918.784994	90854.434182	34.116685
919.150293	91021.413782	34.121703
920.788096	91187.354998	34.126720
921.469884	91350.537756	34.131738
922.423371	91517.037434	34.136756
923.625391	91672.832551	34.141773
924.243508	91844.750721	34.146791
925.171689	92014.036507	34.151808
926.001899	92177.174960	34.156826
927.201421	92342.088936	34.161844
928.222389	92509.229843	34.166861
929.014942	92667.738390	34.171879
930.065424	92835.781757	34.176896
931.063073	93006.385801	34.181914
931.992238	93165.672501	34.186932
932.906883	93328.374278	34.191949
933.505922	93504.978519	34.196967
934.688256	93661.004799	34.201984
935.638613	93837.350785	34.207002
936.510016	94000.684478	34.212020
937.676975	94155.437832	34.217037
938.152036	94332.207770	34.222055
939.403977	94500.406454	34.227072
940.392730	94674.891104	34.232090
941.314218	94831.474327	34.237108
942.259259	95011.051532	34.242125
943.106753	95171.959877	34.247143
944.406322	95328.736925	34.252160
944.685319	95505.161526	34.257178
945.593265	95672.526180	34.262196
946.673104	95841.401777	34.267213
947.570810	96018.449349	34.272231
948.689790	96175.736371	34.277248
949.657478	96349.210762	34.282266
950.321710	96516.526430	34.287284
951.543685	96681.712590	34.292301
952.121934	96847.860902	34.297319
953.087344	97012.477615	34.302336
954.256344	97171.794725	34.307354
955.012232	97349.046090	34.312372
956.289246	97506.650865	34.317389
956.816747	97680.783348	34.322407
957.460958	97840.571317	34.327424
958.545197	98012.214685	34.332442
959.260040	98184.116559	34.337460
960.327349	98367.242889	34.342477
961.216635	98551.090050	34.347495
961.605583	98726.360556	34.352512
962.746011	98922.178674	34.357530
963.745280	99098.933577	34.362548
964.920409	99285.328184	34.367565
965.550391	99483.488898	34.372583
966.508203	99669.295469	34.377600
967.592300	99864.427394	34.382618
968.461237	100060.096558	34.387636
969.479899	100258.756169	34.392653
970.383540	100449.642427	34.397671
971.814648	100649.832374	34.402688
972.247906	100847.485349	34.407706
973.515061	101034.206724	34.412724
974.703040	101233.162454	34.417741
975.769538	101431.563632	34.422759
976.670166	101616.975881	34.427776
977.545628	101819.603185	34.432794
978.674290	102019.252275	34.437812
980.031666	102208.860843	34.442829
980.471649	102416.731575	34.447847
981.431795	102604.369861	34.452864
982.365620	102804.639746	34.457882
983.466913	103002.603963	34.462900
984.355378	103207.323171	34.467917
985.291798	103416.037935	34.472935
986.274501	103616.932852	34.477952
987.322755	103826.354262	34.482970
988.433175	104033.880060	34.487988
989.527544	104235.913725	34.493005
990.639295	104439.605142	34.498023
991.198904	104639.146735	34.503040
992.490819	104845.534428	34.508058
993.395667	105059.194109	34.513076
994.619511	105259.947720	34.518093
995.628518	105464.385948	34.523111
997.023950	105672.586768	34.528128
998.159323	105870.725264	34.533146
999.048791	106061.800578	34.538164
999.894069	106260.585224	34.543181
1001.155670	106474.855927	34.548199
1002.009077	106671.045832	34.553216
1003.309404	106865.960026	34.558234
1004.102409	107065.164615	34.563252
1005.218239	107260.606163	34.568269
1006.049255	107452.271063	34.573287
1006.983883	107656.789063	34.578304
1008.455765	107856.773913	34.583322
1009.430613	108054.423153	34.588340
1010.367411	108251.117480	34.593357
1011.170360	108440.691423	34.598375
1012.518000	108635.572631	34.603392
1013.538931	108830.559932	34.608410
1014.466767	109031.732785	34.613428
1015.522204	109219.205734	34.618445
1016.446154	109421.154798	34.623463
1017.471617	109611.244816	34.628480
1018.768852	109784.431173	34.633498
1019.602015	109982.510581	34.638516
1020.815854	110152.330896	34.643533
1021.421074	110329.397342	34.648551
1022.644036	110503.221244	34.653568
1023.679588	110691.644998	34.658586
1024.506165	110881.143352	34.663604
1025.884180	111070.526499	34.668621
1026.559583	111248.030641	34.673639
1027.406617	111431.980876	34.678656
1028.753299	111625.414101	34.683674
1029.480949	111817.367518	34.688692
1030.896434	112013.566408	34.693709
1031.308745	112205.422636	34.698727
1032.379060	112403.024198	34.703744
1033.448431	112592.924877	34.708762
1034.225449	112809.403210	34.713780
1035.545653	113004.155300	34.718797
1036.607028	113206.768178	34.723815
1037.515682	113414.462655	34.728832
1038.712875	113609.011265	34.733850
1039.572872	113812.573994	34.738868
1040.456253	114014.639376	34.743885
1041.592273	114225.317524	34.748903
1042.501124	114439.822941	34.753920
1043.617923	114637.622650	34.758938
1044.465849	114861.846127	34.763956
1045.447777	115067.196841	34.768973
1046.598617	115291.094907	34.773991
1048.122261	115506.621709	34.779008
1048.934837	115714.349029	34.784026
1049.974025	115943.516043	34.789044
1051.027008	116157.807924	34.794061
1052.177666	116376.114387	34.799079
1053.122498	116579.201526	34.804096
1054.398473	116800.645415	34.809114
1054.944212	117022.186411	34.814132
1056.660701	117246.449781	34.819149
1057.406014	117468.176621	34.824167
1058.314133	117679.298157	34.829184
1059.923076	117900.049261	34.834202
1060.749467	118125.454973	34.839220
1061.751432	118327.493326	34.844237
1062.876624	118549.064291	34.849255
1063.655640	118784.353790	34.854272
1065.186359	119000.184431	34.859290
1066.180334	119220.071578	34.864308
1067.301874	119439.128315	34.869325
1068.534173	119664.935036	34.874343
1069.554932	119881.338037	34.879360
1070.475233	120104.044471	34.884378
1071.639609	120325.394362	34.889396
1072.756991	120534.132366	34.894413
1073.819365	120759.886909	34.899431
1074.666492	120978.151480	34.904448
1076.273601	121204.364267	34.909466
1076.985060	121429.421610	34.914484
1077.956916	121634.579826	34.919501
1079.165541	121867.035058	34.924519
1080.184629	122092.908307	34.929536
1081.939591	122302.972720	34.934554
1082.720014	122526.113379	34.939572
1083.737677	122736.214033	34.944589
1084.745527	122968.736397	34.949607
1085.839287	123185.506321	34.954624
1086.847295	123400.885259	34.959642
1087.694658	123621.082815	34.964660
1088.679994	123841.791455	34.969677
1090.320731	124047.856843	34.974695
1090.918194	124268.125787	34.979712
1092.126914	124471.806814	34.984730
1093.226758	124688.510497	34.989748
1094.393094	124895.382495	34.994765
1095.167912	125115.653620	34.999783
1096.059795	125322.713312	35.004800
1097.446037	125543.672236	35.009818
1098.128796	125765.294055	35.014836
1099.572209	125981.417817	35.019853
1100.338136	126207.984744	35.024871
1101.263700	126432.182169	35.029888
1102.667743	126652.322304	35.034906
1103.774720	126890.359072	35.039924
1104.882460	127112.009065	35.044941
1106.052331	127343.840968	35.049959
1107.067444	127578.045059	35.054976
1108.256512	127802.322941	35.059994
1108.628583	128043.113803	35.065012
1109.833465	128283.730815	35.070029
1111.337979	128518.025852	35.075047
1112.030794	128757.742498	35.080064
1113.594872	129001.322409	35.085082
1114.953379	129254.774495	35.090100
1115.686865	129482.726963	35.095117
1117.174150	129729.899776	35.100135
1118.195882	129968.164258	35.105152
1119.661065	130207.700883	35.110170
1120.582007	130441.827859	35.115188
1121.316972	130687.890274	35.120205
1122.842131	130936.587394	35.125223
1123.824000	131185.642479	35.130240
1124.988871	131424.249161	35.135258
1126.302945	131675.218002	35.140276
1127.700934	131919.430929	35.145293
1128.628441	132153.163721	35.150311
1129.460382	132402.024866	35.155328
1131.161645	132639.943421	35.160346
1132.010706	132895.549701	35.165364
1132.905470	133137.611210	35.170381
1134.555719	133380.018690	35.175399
1135.566237	133623.192964	35.180416
1136.613006	133862.813371	35.185434
1137.846459	134111.469133	35.190452
1139.186068	134359.323224	35.195469
1140.187360	134607.298510	35.200487
1141.335066	134845.235966	35.205504
1142.555759	135093.064549	35.210522
1144.167916	135333.565770	35.215540
1144.943007	135591.664908	35.220557
1146.752615	135815.541327	35.225575
1147.122842	136064.379913	35.230592
1148.988405	136319.008085	35.235610
1150.305178	136552.023334	35.240628
1151.005198	136791.494142	35.245645
1152.530693	137023.311749	35.250663
1153.397860	137267.905882	35.255680
1154.313141	137503.415781	35.260698
1155.841723	137748.588735	35.265716
1156.578301	137987.212549	35.270733
1157.818284	138221.266419	35.275751
1158.682397	138472.627786	35.280768
1159.984486	138724.337033	35.285786
1161.036783	138971.195189	35.290804
1162.105352	139219.256998	35.295821
1163.426394	139464.451328	35.300839
1164.421687	139713.923603	35.305856
1165.714881	139965.706889	35.310874
1167.074723	140198.397806	35.315892
1167.851676	140439.035546	35.320909
1169.056260	140666.835476	35.325927
1170.089815	140913.381045	35.330944
1171.031628	141137.601003	35.335962
1172.493752	141374.974627	35.340980
1173.342369	141618.575918	35.345997
1174.395262	141860.433281	35.351015
1175.271855	142109.105568	35.356032
1176.619964	142360.757716	35.361050
1177.947976	142619.440130	35.366068
1178.856885	142880.032454	35.371085
1179.983764	143126.172455	35.376103
1181.237461	143393.305667	35.381120
1182.412612	143649.421308	35.386138
1183.777161	143901.956755	35.391156
1184.712036	144164.367672	35.396173
1186.235521	144425.224865	35.401191
1187.143684	144693.135139	35.406208
1188.238877	144946.445365	35.411226
1189.474543	145213.798137	35.416244
1190.606637	145485.164778	35.421261
1191.954181	145747.531773	35.426279
1193.240066	146029.643996	35.431296
1194.641190	146299.577277	35.436314
1195.948452	146576.553996	35.441332
1197.069735	146836.924463	35.446349
1198.308800	147103.022419	35.451367
1199.512274	147386.452398	35.456384
1200.787869	147646.207054	35.461402
1201.794224	147916.268289	35.466420
1202.933906	148191.788400	35.471437
1204.375629	148462.339713	35.476455
1205.157493	148754.803987	35.481472
1206.835263	149021.972086	35.486490
1208.322856	149295.502405	35.491508
1209.146831	149571.972778	35.496525
1210.479395	149843.338551	35.501543
1212.010982	150112.415753	35.506560
1213.028197	150390.559799	35.511578
1214.686018	150654.369066	35.516596
1215.441951	150933.067648	35.521613
1217.043013	151210.334844	35.526631
1218.410892	151482.264670	35.531648
1219.426814	151756.981662	35.536666
1220.793803	152027.647141	35.541684
1222.025194	152300.556668	35.546701
1223.395820	152563.982723	35.551719
1224.386788	152840.753774	35.556736
1225.481174	153110.596741	35.561754
1226.914482	153384.533387	35.566772
1227.700468	153656.993404	35.571789
1229.366772	153926.037187	35.576807
1230.494742	154213.310965	35.581824
1231.594942	154486.143445	35.586842
1233.121780	154765.173648	35.591860
1234.117918	155045.143453	35.596877
1235.541192	155323.497067	35.601895
1236.439324	155603.106484	35.606912
1237.654353	155883.033369	35.611930
1239.144279	156155.774940	35.616948
1239.958037	156436.621973	35.621965
1241.589071	156720.456534	35.626983
1242.952956	156997.601206	35.632000
1244.112881	157282.646644	35.637018
1245.430995	157561.401173	35.642036
1246.690534	157839.862850	35.647053
1247.295915	158106.839597	35.652071
1248.884008	158379.732287	35.657088
1250.099018	158647.969234	35.662106
1251.061596	158911.923671	35.667124
1252.203184	159187.914895	35.672141
1253.578790	159446.577756	35.677159
1255.061305	159722.452793	35.682176
1256.172122	159994.280672	35.687194
1257.424425	160272.531763	35.692212
1258.545022	160553.102789	35.697229
1259.831847	160814.097870	35.702247
1260.954974	161101.307370	35.707264
1262.353566	161388.321070	35.712282
1263.652350	161662.894540	35.717300
1264.690445	161954.336043	35.722317
1266.001143	162243.742607	35.727335
1267.273703	162529.186326	35.732352
1268.183701	162806.330893	35.737370
1269.230658	163101.267858	35.742388
1270.480606	163401.502090	35.747405
1272.004530	163703.824673	35.752423
1273.309603	164006.198245	35.757440
1274.419644	164312.361776	35.762458
1275.983268	164607.693139	35.767476
1276.823905	164923.434156	35.772493
1278.064938	165226.359731	35.777511
1279.598272	165538.247719	35.782528
1280.594783	165849.351163	35.787546
1281.957359	166165.052941	35.792564
1282.780149	166481.950093	35.797581
1284.382443	166804.062562	35.802599
1285.829583	167114.034591	35.807616
1286.809956	167429.580150	35.812634
1288.424029	167755.605686	35.817652
1289.521866	168081.820426	35.822669
1291.213337	168403.168342	35.827687
1292.405613	168725.946095	35.832704
1293.617594	169043.063505	35.837722
1295.256028	169369.654985	35.842740
1296.480718	169689.566434	35.847757
1297.943390	170010.582833	35.852775
1299.457445	170331.453395	35.857792
1300.588011	170646.780746	35.862810
1301.883383	170959.532369	35.867828
1303.326902	171290.776046	35.872845
1304.570958	171601.624296	35.877863
1306.251039	171932.313133	35.882880
1307.708305	172247.216596	35.887898
1309.078787	172556.895468	35.892916
1310.102722	172886.887265	35.897933
1311.544280	173192.713392	35.902951
1312.904783	173509.176748	35.907968
1313.974059	173828.964472	35.912986
1315.544950	174145.054604	35.918004
1317.053221	174460.040378	35.923021
1318.180586	174778.035404	35.928039
1319.430751	175091.646569	35.933056
1320.797124	175418.578686	35.938074
1322.611344	175718.508685	35.943092
1323.651467	176040.968183	35.948109
1324.933396	176354.937515	35.953127
1326.543670	176660.478357	35.958144
1327.571208	176983.453712	35.963162
1328.942335	177294.749055	35.968180
1330.584046	177609.897891	35.973197
1332.043420	177921.880565	35.978215
1333.527578	178233.899144	35.983232
1334.513733	178546.979207	35.988250
1335.846225	178850.345509	35.993268
1337.020874	179148.891409	35.998285
1338.059668	179444.250441	36.003303
1339.631037	179745.285315	36.008320
1340.871102	180043.685976	36.013338
1342.105697	180340.667736	36.018356
1343.163057	180643.353899	36.023373
1344.338018	180947.431223	36.028391
1345.859942	181263.142635	36.033408
1346.931225	181588.855903	36.038426
1348.449182	181892.742374	36.043444
1349.554242	182209.822959	36.048461
1351.049432	182534.304241	36.053479
1352.392172	182853.088253	36.058496
1353.443812	183176.580526	36.063514
1355.165278	183481.749729	36.068532
1356.693004	183819.268964	36.073549
1357.788516	184148.268522	36.078567
1359.181535	184465.111648	36.083584
1360.306846	184800.989862	36.088602
1361.953958	185120.574573	36.093620
1362.963154	185458.786138	36.098637
1364.361115	185784.978301	36.103655
1365.806884	186128.046814	36.108672
1367.034842	186457.774384	36.113690
1368.511793	186799.331290	36.118708
1370.126793	187152.609135	36.123725
1371.064350	187490.438511	36.128743
1372.393905	187836.735381	36.133760
1373.695810	188190.185598	36.138778
1375.285364	188541.000852	36.143796
1376.983514	188896.332069	36.148813
1378.275963	189232.830845	36.153831
1379.480370	189586.039045	36.158848
1380.839199	189945.659864	36.163866
1382.146614	190294.907324	36.168884
1383.802504	190650.738455	36.173901
1384.981491	190996.964554	36.178919
1386.876260	191361.583130	36.183936
1388.044215	191709.897050	36.188954
1389.558318	192060.821660	36.193972
1391.197726	192416.361192	36.198989
1392.523189	192775.674269	36.204007
1393.928666	193111.401590	36.209024
1395.421242	193472.976180	36.214042
1396.589643	193820.489429	36.219060
1398.121663	194179.420976	36.224077
1399.518485	194535.342725	36.229095
1400.999707	194869.962409	36.234112
1402.253813	195239.025960	36.239130
1403.504677	195590.229601	36.244148
1405.346918	195949.005539	36.249165
1406.525748	196319.560368	36.254183
1408.284443	196666.788332	36.259200
1409.670733	197018.129615	36.264218
1411.310709	197372.490535	36.269236
1412.229220	197729.232431	36.274253
1413.933484	198075.270636	36.279271
1415.292107	198440.119778	36.284288
1416.551256	198793.751266	36.289306
1418.002807	199140.446076	36.294324
1419.522461	199499.307070	36.299341
1420.966125	199855.427388	36.304359
1422.433905	200203.572230	36.309376
1423.539077	200575.457562	36.314394
1425.131138	200935.939128	36.319412
1426.605248	201286.221291	36.324429
1427.773863	201650.598121	36.329447
1429.537490	201996.112779	36.334464
1430.915284	202346.911211	36.339482
1432.581149	202679.037526	36.344500
1434.025710	203006.592961	36.349517
1435.383349	203355.875948	36.354535
1437.002628	203681.881885	36.359552
1438.035931	204013.534681	36.364570
1439.475091	204358.225277	36.369588
1440.961646	204703.315929	36.374605
1442.126902	205041.858698	36.379623
1443.812025	205384.050060	36.384640
1445.153161	205742.526962	36.389658
1446.456098	206086.130514	36.394676
1448.055581	206440.034989	36.399693
1449.161574	206801.603011	36.404711
1450.796521	207148.864031	36.409728
1451.942759	207512.333281	36.414746
1453.308950	207873.825097	36.419764
1454.920079	208236.903369	36.424781
1455.981123	208607.400780	36.429799
1457.460830	208971.545262	36.434816
1458.985989	209360.736785	36.439834
1460.325302	209734.151893	36.444852
1461.786697	210099.739223	36.449869
1463.194706	210492.637794	36.454887
1464.790738	210861.761628	36.459904
1466.272416	211247.515163	36.464922
1467.922104	211631.058566	36.469940
1469.385060	212012.983738	36.474957
1470.598535	212403.789842	36.479975
1472.342678	212782.751271	36.484992
1473.800543	213180.021989	36.490010
1475.081017	213569.349108	36.495028
1477.096790	213953.324594	36.500045
1478.340745	214346.597621	36.505063
1480.025036	214734.034370	36.510080
1481.525486	215111.471117	36.515098
1483.279676	215499.991579	36.520116
1484.743991	215895.876053	36.525133
1486.252693	216284.897437	36.530151
1488.016627	216673.827420	36.535168
1489.506006	217058.359678	36.540186
1490.917234	217433.356684	36.545204
1492.169176	217825.347389	36.550221
1493.626599	218218.753375	36.555239
1495.215937	218599.287531	36.560256
1496.845241	219001.582966	36.565274
1498.064746	219397.039275	36.570292
1499.984133	219791.619486	36.575309
1501.415525	220183.614938	36.580327
1502.898049	220573.673076	36.585344
1504.231778	220968.252822	36.590362
1505.695641	221356.869131	36.595380
1507.348978	221751.119510	36.600397
1508.469796	222155.034769	36.605415
1510.173262	222545.622190	36.610432
1512.228457	222950.605083	36.615450
1513.632149	223335.377487	36.620468
1514.975710	223730.270118	36.625485
1516.598480	224144.497862	36.630503
1518.031816	224595.181548	36.635520
1519.412325	224987.278286	36.640538
1520.903905	225385.784108	36.645556
1522.562556	225785.660615	36.650573
1523.744271	226188.182610	36.655591
1525.152992	226583.302345	36.660608
1526.742036	226983.956156	36.665626
1528.014203	227397.643109	36.670644
1529.952270	227785.719380	36.675661
1531.618835	228178.743928	36.680679
1533.046430	228554.968569	36.685696
1534.516851	228937.511919	36.690714
1535.696780	229321.044149	36.695732
1537.874152	229703.853821	36.700749
1539.063931	230092.923886	36.705767
1540.512109	230472.198385	36.710784
1542.144285	230852.230903	36.715802
1543.404236	231254.323154	36.720820
1544.950555	231642.957415	36.725837
1546.536187	232039.562129	36.730855
1548.454848	232433.979143	36.735872
1549.909649	232821.234434	36.740890
1551.321698	233233.924446	36.745908
1553.203189	233617.148564	36.750925
1554.291322	234017.091789	36.755943
1556.158695	234420.260232	36.760960
1557.634486	234821.868630	36.765978
1559.110721	235226.653095	36.770996
1560.680224	235623.726380	36.776013
1562.300014	236031.181549	36.781031
1563.976744	236439.263272	36.786048
1565.900322	236843.215419	36.791066
1567.314068	237265.161001	36.796084
1568.962620	237664.003746	36.801101
1570.429399	238073.851001	36.806119
1571.435414	238487.102890	36.811136
1573.346777	238896.243317	36.816154
1574.876334	239320.333292	36.821172
1576.693702	239734.063270	36.826189
1577.989010	240160.073367	36.831207
1579.531722	240581.115362	36.836224
1581.263717	241006.826300	36.841242
1582.566833	241437.435327	36.846260
1584.198065	241847.795984	36.851277
1585.713009	242290.336084	36.856295
1587.425016	242722.835813	36.861312
1589.436348	243152.822767	36.866330
1590.552846	243585.498512	36.871348
1592.638500	244010.597260	36.876365
1594.530619	244440.148692	36.881383
1595.944404	244870.999116	36.886400
1597.231801	245301.362986	36.891418
1598.800088	245738.768433	36.896436
1600.706010	246168.243826	36.901453
1601.881882	246613.336130	36.906471
1603.309981	247046.447984	36.911488
1605.211628	247480.625267	36.916506
1606.682186	247927.397935	36.921524
1608.321642	248369.977131	36.926541
1610.047712	248800.907928	36.931559
1611.887871	249243.912168	36.936576
1613.246503	249691.238713	36.941594
1614.778488	250137.571738	36.946612
1616.628415	250578.009936	36.951629
1617.979044	251018.632608	36.956647
1619.644891	251462.201136	36.961664
1621.580515	251915.505661	36.966682
1623.012211	252361.577649	36.971700
1624.518856	252801.718611	36.976717
1626.268982	253251.472848	36.981735
1627.754665	253706.021436	36.986752
1629.345354	254161.873892	36.991770
1630.739472	254617.073157	36.996788
1632.767020	255056.036907	37.001805
1634.697139	255506.143553	37.006823
1635.958735	255953.541021	37.011840
1637.676279	256398.145146	37.016858
1639.131043	256838.702853	37.021876
1640.812089	257258.417960	37.026893
1642.764524	257686.369769	37.031911
1643.855295	258122.720030	37.036928
1645.839143	258558.008264	37.041946
1647.203139	258994.364218	37.046964
1648.929234	259434.470832	37.051981
1650.246253	259872.079246	37.056999
1651.621029	260325.961571	37.062016
1653.469680	260762.338870	37.067034
1654.797537	261219.480369	37.072052
1656.375746	261671.093269	37.077069
1657.891285	262119.591764	37.082087
1659.465601	262589.469916	37.087104
1661.210689	263058.252704	37.092122
1662.421772	263528.419025	37.097140
1664.328122	264001.899663	37.102157
1665.695542	264494.089568	37.107175
1667.258606	264970.064980	37.112192
1668.978231	265453.736735	37.117210
1670.479351	265946.995768	37.122228
1672.423444	266431.925178	37.127245
1674.116069	266938.488296	37.132263
1675.362161	267421.144160	37.137280
1677.150071	267928.401767	37.142298
1678.727507	268428.606113	37.147316
1680.595494	268922.055477	37.152333
1682.295653	269427.979385	37.157351
1683.941809	269943.539232	37.162368
1685.962954	270447.554303	37.167386
1687.304051	270960.927594	37.172404
1689.013758	271462.604722	37.177421
1690.871980	271982.851333	37.182439
1692.815149	272499.374229	37.187456
1694.631612	273008.321749	37.192474
1695.963674	273538.254713	37.197492
1697.895003	274044.412478	37.202509
1699.629952	274552.989545	37.207527
1701.465774	275076.485582	37.212544
1703.523188	275589.401913	37.217562
1705.053032	276111.193501	37.222580
1706.791762	276623.601375	37.227597
1708.575068	277147.330119	37.232615
1710.637533	277661.841322	37.237632
1712.111048	278173.298706	37.242650
1713.833519	278691.927893	37.247668
1715.706083	279214.087241	37.252685
1717.236349	279726.572816	37.257703
1718.628281	280246.116190	37.262720
1720.831982	280766.260701	37.267738
1723.040516	281301.186732	37.272756
1723.974188	281808.964192	37.277773
1726.091561	282328.483401	37.282791
1727.989028	282860.585687	37.287808
1729.813687	283369.862466	37.292826
1731.262301	283892.383061	37.297844
1733.271763	284415.647569	37.302861
1735.238620	284924.641938	37.307879
1736.811970	285439.364066	37.312896
1739.008432	285960.001564	37.317914
1740.557503	286481.531598	37.322932
1742.316539	286991.569337	37.327949
1744.230940	287508.844205	37.332967
1745.981792	288030.792499	37.337984
1747.778143	288521.082277	37.343002
1749.415045	289035.806430	37.348020
1751.260780	289542.848619	37.353037
1752.946694	290049.889853	37.358055
1754.268828	290549.851755	37.363072
1756.165158	291028.279242	37.368090
1758.217515	291523.341492	37.373108
1759.645879	292013.729657	37.378125
1761.460264	292508.725646	37.383143
1762.888116	293006.653595	37.388160
1764.571031	293499.432026	37.393178
1766.208906	293999.048257	37.398196
1767.842801	294507.324136	37.403213
1769.818257	295016.658894	37.408231
1771.136413	295526.607876	37.413248
1772.894211	296039.732958	37.418266
1774.918434	296554.868926	37.423284
1776.863075	297070.117163	37.428301
1779.241692	297576.122338	37.433319
1780.669253	298103.947015	37.438336
1782.590674	298603.774680	37.443354
1784.356141	299115.385016	37.448372
1786.293593	299638.571262	37.453389
1788.096756	300141.052225	37.458407
1789.599413	300675.708457	37.463424
1791.769855	301194.809681	37.468442
1793.459666	301720.540029	37.473460
1794.998879	302239.638216	37.478477
1796.610593	302762.429542	37.483495
1798.667153	303303.481137	37.488512
1800.388295	303835.010277	37.493530
1801.836181	304376.613141	37.498548
1803.919015	304920.012598	37.503565
1805.937126	305455.800452	37.508583
1807.300340	305997.077182	37.513600
1809.383104	306541.558572	37.518618
1811.256095	307090.210666	37.523636
1813.128124	307638.224446	37.528653
1815.035575	308177.949785	37.533671
1816.706014	308724.084992	37.538688
1818.493115	309277.612698	37.543706
1820.700872	309830.762386	37.548724
1822.031502	310374.885507	37.553741
1824.011086	310926.668502	37.558759
1826.093255	311473.275546	37.563776
1827.820705	312037.256290	37.568794
1829.788168	312583.595031	37.573812
1831.540019	313142.078388	37.578829
1833.663855	313693.004957	37.583847
1835.136560	314252.668802	37.588864
1837.301156	314807.465536	37.593882
1839.427033	315363.661051	37.598900
1840.519725	315923.247805	37.603917
1842.975880	316474.936347	37.608935
1844.484243	317039.955887	37.613952
1846.649091	317601.332889	37.618970
1848.428473	318164.444877	37.623988
1850.367500	318721.685700	37.629005
1852.354305	319276.679573	37.634023
1854.196475	319827.376171	37.639040
1856.115166	320387.501189	37.644058
1858.066764	320945.457768	37.649076
1859.767879	321512.464753	37.654093
1861.667707	322061.101831	37.659111
1863.465133	322617.952285	37.664128
1865.678259	323179.578775	37.669146
1867.217865	323740.651351	37.674164
1869.291541	324304.423590	37.679181
1871.604891	324846.900002	37.684199
1873.460486	325402.624331	37.689216
1875.052633	325956.965312	37.694234
1877.295964	326492.710527	37.699252
1879.031476	327030.565920	37.704269
1880.828705	327549.898048	37.709287
1882.636409	328075.570957	37.714304
1884.474033	328600.218695	37.719322
1886.333527	329115.033008	37.724340
1888.057692	329650.911401	37.729357
1890.088758	330177.645440	37.734375
1891.669405	330712.953670	37.739392
1893.235682	331240.871624	37.744410
1895.591952	331783.454573	37.749428
1896.790806	332337.342595	37.754445
1898.912974	332878.506471	37.759463
1900.470674	333441.209286	37.764480
1902.302165	333989.442052	37.769498
1904.173613	334546.369839	37.774516
1905.935435	335118.744081	37.779533
1907.697073	335678.369031	37.784551
1909.757369	336256.723303	37.789568
1911.644713	336833.119790	37.794586
1913.604492	337413.610144	37.799604
1915.588777	337992.744601	37.804621
1917.339424	338566.682125	37.809639
1919.081326	339160.641905	37.814656
1920.970662	339746.930144	37.819674
1922.923219	340340.917385	37.824692
1925.120344	340933.486527	37.829709
1926.940213	341516.795711	37.834727
1928.881538	342130.637360	37.839744
1930.666734	342721.755446	37.844762
1932.923375	343328.118579	37.849780
1934.685568	343926.789234	37.854797
1936.450888	344539.512567	37.859815
1938.494781	345146.192310	37.864832
1940.149688	345749.629108	37.869850
1942.356981	346361.392851	37.874868
1944.526128	346983.737872	37.879885
1946.586647	347595.306503	37.884903
1948.501371	348217.676820	37.889920
1950.569393	348828.339444	37.894938
1952.669077	349439.242359	37.899956
1954.539943	350060.757057	37.904973
1956.689951	350673.157435	37.909991
1958.703039	351291.535438	37.915008
1960.908035	351910.761222	37.920026
1963.081267	352518.386706	37.925044
1965.120003	353139.119637	37.930061
1967.018593	353754.081239	37.935079
1969.030835	354361.961060	37.940096
1971.087868	354972.057746	37.945114
1973.345665	355585.664841	37.950132
1974.712278	356193.447304	37.955149
1976.895773	356803.217401	37.960167
1978.573553	357417.426171	37.965184
1980.840990	358048.172810	37.970202
1982.937862	358668.027879	37.975220
1984.741542	359289.494963	37.980237
1986.748598	359900.770377	37.985255
1988.872474	360528.229259	37.990272
1990.787627	361143.687098	37.995290
1992.874314	361755.250810	38.000308
1995.002279	362383.161742	38.005325
1996.455172	362999.631017	38.010343
1998.752366	363612.754661	38.015360
2000.705255	364240.740701	38.020378
2002.557813	364862.416403	38.025396
2004.585287	365497.041423	38.030413
2006.765616	366123.259418	38.035431
2008.511076	366741.573646	38.040448
2010.152114	367346.323888	38.045466
2012.564530	367944.823780	38.050484
2014.424770	368554.718304	38.055501
2016.093789	369157.785732	38.060519
2018.256166	369764.845569	38.065536
2020.404128	370370.959237	38.070554
2022.283781	370987.125888	38.075572
2024.204386	371592.698692	38.080589
2026.209376	372207.023025	38.085607
2028.154225	372825.024343	38.090624
2029.888925	373449.035125	38.095642
2031.921376	374069.105407	38.100660
2033.947939	374716.226302	38.105677
2036.058314	375344.326119	38.110695
2037.744257	375981.031147	38.115712
2039.653611	376628.541652	38.120730
2041.695436	377260.472774	38.125748
2043.436572	377927.082269	38.130765
2045.269354	378585.320661	38.135783
2047.465211	379247.568972	38.140800
2049.201441	379920.606372	38.145818
2051.404975	380590.053854	38.150836
2053.077755	381266.396405	38.155853
2055.395177	381943.328706	38.160871
2057.586502	382627.722418	38.165888
2059.288671	383323.845844	38.170906
2061.663809	384003.109450	38.175924
2063.663315	384710.512849	38.180941
2065.490510	385393.894304	38.185959
2068.205430	386093.695314	38.190976
2069.840147	386811.912827	38.195994
2072.111713	387501.133516	38.201012
2074.282079	388203.589078	38.206029
2076.130503	388918.503769	38.211047
2078.414357	389612.771465	38.216064
2080.187468	390334.586563	38.221082
2082.477065	391038.834272	38.226100
2084.598454	391759.569855	38.231117
2086.988500	392473.146770	38.236135
2089.125871	393182.135486	38.241152
2091.149439	393906.232741	38.246170
2093.420117	394627.813216	38.251188
2095.317582	395349.285800	38.256205
2097.650242	396059.593498	38.261223
2099.839997	396775.888866	38.266240
2101.880576	397510.894709	38.271258
2104.022882	398235.398804	38.276276
2106.188646	398949.288046	38.281293
2108.214203	399672.812532	38.286311
2110.618154	400393.443558	38.291328
2112.457107	401125.476724	38.296346
2114.785507	401849.656439	38.301364
2117.131327	402570.926161	38.306381
2119.500621	403286.573844	38.311399
2121.425477	404004.303639	38.316416
2123.600095	404725.419567	38.321434
2126.055280	405450.752276	38.326452
2128.080901	406164.811903	38.331469
2129.867248	406884.390154	38.336487
2132.336348	407597.300579	38.341504
2134.475031	408338.012388	38.346522
2136.767150	409047.012642	38.351540
2138.701808	409771.379209	38.356557
2140.693798	410503.670841	38.361575
2142.883804	411216.835667	38.366592
2145.004408	411944.582941	38.371610
2147.301722	412662.073298	38.376628
2149.222047	413383.608269	38.381645
2151.042794	414091.842626	38.386663
2153.349671	414786.528718	38.391680
2155.183768	415482.869847	38.396698
2157.293556	416179.982476	38.401716
2159.417686	416881.835010	38.406733
2161.421510	417593.792679	38.411751
2163.773023	418303.368619	38.416768
2165.403846	419026.237043	38.421786
2167.643750	419737.639826	38.426804
2169.727588	420461.379922	38.431821
2171.645604	421191.709928	38.436839
2173.649813	421924.308459	38.441856
2175.704411	422672.144679	38.446874
2177.868416	423403.407113	38.451892
2180.224170	424153.148877	38.456909
2182.178589	424909.769552	38.461927
2184.219269	425663.719603	38.466944
2186.512492	426422.819545	38.471962
2188.362519	427181.259966	38.476980
2190.612215	427957.380880	38.481997
2192.927151	428736.199668	38.487015
2195.174181	429496.931222	38.492032
2197.199085	430275.190569	38.497050
2199.382606	431067.622642	38.502068
2201.756987	431847.037880	38.507085
2204.203333	432636.994386	38.512103
2206.207455	433436.462279	38.517120
2208.617302	434229.002682	38.522138
2211.092359	435017.354847	38.527156
2213.423531	435823.619927	38.532173
2214.859500	436623.273304	38.537191
2217.898290	437409.678561	38.542208
2219.645101	438220.256754	38.547226
2221.967510	439013.859770	38.552244
2224.109923	439829.476248	38.557261
2226.398177	440641.092069	38.562279
2228.591951	441451.985482	38.567296
2230.703853	442272.223016	38.572314
2233.007998	443091.386398	38.577332
2235.381852	443897.050064	38.582349
2237.618867	444726.484194	38.587367
2239.948397	445543.831292	38.592384
2242.395181	446376.354789	38.597402
2244.773189	447188.117676	38.602420
2247.248705	448006.106028	38.607437
2249.079565	448838.079203	38.612455
2251.586673	449657.314045	38.617472
2254.090316	450485.672186	38.622490
2256.324615	451308.175508	38.627508
2258.750420	452127.378301	38.632525
2260.674308	452947.845507	38.637543
2263.145719	453783.360703	38.642560
2265.204634	454610.819543	38.647578
2267.548675	455435.821566	38.652596
2270.250410	456273.169884	38.657613
2272.284583	457092.543838	38.662631
2274.918205	457917.802382	38.667648
2276.743803	458757.670461	38.672666
2279.380949	459589.129255	38.677684
2281.722576	460408.570902	38.682701
2283.982796	461240.175099	38.687719
2286.542248	462058.603180	38.692736
2288.611148	462889.159028	38.697754
2290.849904	463711.109980	38.702772
2293.326666	464543.702244	38.707789
2295.606980	465371.945128	38.712807
2297.890809	466194.441526	38.717824
2299.766110	467014.848049	38.722842
2302.458387	467810.879439	38.727860
2304.741955	468604.368313	38.732877
2306.620904	469403.803125	38.737895
2308.977687	470193.373930	38.742912
2311.057325	471009.129793	38.747930
2313.342720	471808.093561	38.752948
2315.540317	472611.332344	38.757965
2317.698813	473424.141886	38.762983
2320.422906	474252.836605	38.768000
2322.185847	475072.257563	38.773018
2324.457637	475889.639049	38.778036
2327.130981	476717.323260	38.783053
2328.973333	477551.067406	38.788071
2331.522061	478377.738022	38.793088
2333.780648	479212.954230	38.798106
2336.119113	480052.967117	38.803124
2338.564886	480898.276320	38.808141
2340.627210	481745.881682	38.813159
2342.903565	482591.392193	38.818176
2345.311596	483450.574785	38.823194
2347.150546	484310.365447	38.828212
2349.434664	485179.886021	38.833229
2351.571109	486058.879346	38.838247
2354.345329	486941.408902	38.843264
2356.773010	487814.108132	38.848282
2358.881509	488702.312816	38.853300
2361.266604	489593.808483	38.858317
2363.407354	490483.986607	38.863335
2365.837872	491377.654502	38.868352
2368.135881	492280.936997	38.873370
2370.578282	493196.864943	38.878388
2373.072529	494105.822347	38.883405
2375.426800	495021.465327	38.888423
2377.534002	495935.031136	38.893440
2379.751036	496854.230655	38.898458
2382.163659	497785.859269	38.903476
2384.488585	498720.023484	38.908493
2386.468840	499662.919199	38.913511
2389.109911	500599.902300	38.918528
2391.336436	501542.751734	38.923546
2393.649768	502494.107057	38.928564
2396.549584	503438.804914	38.933581
2398.475126	504401.965361	38.938599
2400.951405	505344.353834	38.943616
2403.274756	506309.453887	38.948634
2405.736646	507282.692126	38.953652
2408.324325	508236.793220	38.958669
2410.182880	509219.542873	38.963687
2413.073779	510188.047604	38.968704
2415.433344	511159.000778	38.973722
2417.434718	512140.941993	38.978740
2420.340402	513114.003959	38.983757
2422.486580	514104.065115	38.988775
2424.936622	515083.229060	38.993792
2427.632992	516066.675174	38.998810
2429.619133	517062.471312	39.003828
2432.317171	518045.489597	39.008845
2434.808901	519043.694938	39.013863
2437.459189	520033.194491	39.018880
2439.690552	521020.432357	39.023898
2441.718719	522025.874892	39.028916
2444.796022	523009.116745	39.033933
2447.161436	524003.240973	39.038951
2449.466169	524998.568792	39.043968
2452.002474	525994.850050	39.048986
2454.438548	526997.225008	39.054004
2456.801650	527996.926292	39.059021
2459.248633	528997.654156	39.064039
2461.626401	529960.062747	39.069056
2464.439818	530927.824012	39.074074
2466.584567	531902.830387	39.079092
2469.341407	532861.613587	39.084109
2471.354135	533824.382471	39.089127
2473.873094	534790.980075	39.094144
2476.308202	535762.307949	39.099162
2478.765276	536744.788747	39.104180
2480.956242	537727.397232	39.109197
2483.356020	538713.778146	39.114215
2485.790702	539708.386618	39.119232
2488.351277	540704.514589	39.124250
2490.560935	541701.334644	39.129268
2493.080004	542708.043238	39.134285
2495.298152	543718.853801	39.139303
2497.745358	544738.254526	39.144320
2500.204485	545768.491852	39.149338
2502.324290	546792.171497	39.154356
2505.010257	547829.761335	39.159373
2507.722122	548876.620795	39.164391
2509.766038	549918.332326	39.169408
2512.759862	550952.870403	39.174426
2514.999577	552017.564808	39.179444
2517.777579	553059.619062	39.184461
2520.224781	554112.604339	39.189479
2522.781015	555183.631824	39.194496
2525.612746	556245.282121	39.199514
2527.834935	557311.320334	39.204532
2530.318956	558382.204284	39.209549
2532.785456	559456.069433	39.214567
2535.452358	560541.067195	39.219584
2538.193581	561615.264076	39.224602
2540.437559	562706.482251	39.229620
2543.431653	563794.221181	39.234637
2545.747657	564885.797853	39.239655
2548.319794	565967.097137	39.244672
2551.113203	567070.060966	39.249690
2553.316272	568174.082135	39.254708
2556.341979	569269.639575	39.259725
2558.688850	570372.995814	39.264743
2561.125705	571482.315094	39.269760
2563.920858	572586.007778	39.274778
2565.947840	573707.245277	39.279796
2568.512476	574807.871089	39.284813
2571.224569	575934.969179	39.289831
2573.642205	577055.341550	39.294848
2576.248863	578184.411341	39.299866
2579.272181	579319.128519	39.304884
2581.805511	580430.850368	39.309901
2584.238593	581561.045024	39.314919
2586.563376	582702.787897	39.319936
2589.631991	583847.360271	39.324954
2592.021143	584978.098941	39.329972
2594.472388	586108.972755	39.334989
2597.108494	587243.871114	39.340007
2599.523939	588394.638648	39.345024
2602.267828	589545.291863	39.350042
2604.940872	590691.736681	39.355060
2607.641010	591836.112482	39.360077
2610.033663	592983.184536	39.365095
2612.692668	594130.752785	39.370112
2615.614485	595281.121631	39.375130
2617.949875	596432.075645	39.380148
2620.640459	597582.306968	39.385165
2623.260789	598742.001858	39.390183
2626.280313	599897.709417	39.395200
2628.708055	601042.283521	39.400218
2631.424410	602178.635884	39.405236
2634.348459	603300.223885	39.410253
2637.286455	604409.536153	39.415271
2639.663453	605527.291810	39.420288
2642.446930	606626.503635	39.425306
2644.657814	607723.001103	39.430324
2647.300240	608835.282679	39.435341
2650.155758	609945.067773	39.440359
2652.533207	611055.572384	39.445376
2655.310395	612161.849071	39.450394
2657.653840	613303.449285	39.455412
2660.112331	614414.106159	39.460429
2662.680506	615553.337257	39.465447
2665.502608	616698.909024	39.470464
2668.443350	617831.792885	39.475482
2670.564485	618970.043840	39.480500
2673.063013	620115.611791	39.485517
2675.837193	621281.155779	39.490535
2678.237476	622438.440321	39.495552
2680.698162	623603.985902	39.500570
2683.365840	624793.853628	39.505588
2685.955253	625978.856338	39.510605
2688.399156	627161.653773	39.515623
2691.014513	628372.212260	39.520640
2694.057130	629570.576364	39.525658
2696.601702	630777.675671	39.530676
2698.822006	631989.433713	39.535693
2701.363166	633211.433369	39.540711
2704.158531	634450.969611	39.545728
2706.738251	635673.423961	39.550746
2709.232223	636929.086405	39.555764
2711.973904	638168.687510	39.560781
2714.933261	639427.862150	39.565799
2717.176995	640690.792243	39.570816
2720.149263	641955.741224	39.575834
2722.792758	643228.717585	39.580852
2725.305655	644501.007742	39.585869
2728.177642	645784.747139	39.590887
2730.665968	647065.744329	39.595904
2733.659810	648344.102380	39.600922
2736.673312	649647.764752	39.605940
2738.907227	650945.554689	39.610957
2741.812445	652245.955081	39.615975
2744.645177	653549.086894	39.620992
2747.513990	654838.689798	39.626010
2750.467319	656163.027908	39.631028
2752.933789	657457.135779	39.636045
2755.947299	658758.302634	39.641063
2758.664372	660077.269676	39.646080
2761.569840	661391.346810	39.651098
2764.137453	662706.147492	39.656116
2767.243508	664025.856365	39.661133
2770.241102	665333.856567	39.666151
2772.678077	666657.095893	39.671168
2775.592174	667972.262223	39.676186
2778.525671	669297.241941	39.681204
2781.090412	670617.471674	39.686221
2783.876203	671934.794954	39.691239
2786.522669	673268.961966	39.696256
2789.565789	674589.699061	39.701274
2792.446997	675921.112627	39.706292
2794.784289	677252.226672	39.711309
2798.035502	678583.794145	39.716327
2800.331835	679925.065955	39.721344
2803.754288	681250.854098	39.726362
2806.177108	682584.662577	39.731380
2808.848989	683928.665283	39.736397
2812.024586	685252.722152	39.741415
2814.481906	686579.484930	39.746432
2817.515470	687889.526199	39.751450
2820.316216	689189.438690	39.756468
2823.155945	690482.804276	39.761485
2826.003691	691771.267778	39.766503
2828.593065	693065.244161	39.771520
2831.353374	694356.077440	39.776538
2834.144774	695657.679568	39.781556
2836.687286	696972.471779	39.786573
2839.282436	698279.819682	39.791591
2841.843483	699610.528431	39.796608
2844.539627	700934.965043	39.801626
2847.439521	702269.872731	39.806644
2849.946574	703627.980982	39.811661
2852.866144	704960.390421	39.816679
2855.757556	706317.071831	39.821696
2858.320785	707680.924346	39.826714
2860.766272	709066.469235	39.831732
2863.568711	710442.372221	39.836749
2866.628979	711821.525629	39.841767
2869.526880	713224.588370	39.846784
2872.053373	714613.424064	39.851802
2875.052723	716024.022821	39.856820
2877.797644	717437.939526	39.861837
2880.616180	718856.007970	39.866855
2883.594612	720277.864722	39.871872
2886.197238	721718.084091	39.876890
2888.949101	723151.452930	39.881908
2891.676040	724607.266717	39.886925
2894.925873	726048.107338	39.891943
2897.419619	727510.512729	39.896960
2900.202265	728970.731402	39.901978
2903.261233	730439.237845	39.906996
2905.843241	731919.212833	39.912013
2909.016591	733400.399622	39.917031
2911.825389	734894.506681	39.922048
2915.087434	736380.067088	39.927066
2918.145090	737874.071242	39.932084
2920.734644	739364.912056	39.937101
2924.027612	740860.191791	39.942119
2926.941659	742361.860924	39.947136
2929.688966	743873.183858	39.952154
2932.672969	745384.226493	39.957172
2935.682625	746894.036770	39.962189
2938.971640	748393.848903	39.967207
2941.994092	749911.647922	39.972224
2944.978254	751418.563684	39.977242
2948.241943	752929.867972	39.982260
2951.017086	754449.524987	39.987277
2954.367425	755956.328960	39.992295
2957.209719	757457.799860	39.997312
2960.371215	758975.853083	40.002330
2963.669363	760475.569903	40.007348
2966.620348	761991.232783	40.012365
2969.984036	763491.815439	40.017383
2972.802017	765014.810361	40.022400
2975.777631	766513.180099	40.027418
2978.870112	768018.160935	40.032436
2981.636778	769515.125249	40.037453
2984.887398	771029.298971	40.042471
2987.815085	772522.630408	40.047488
2990.769631	774022.334470	40.052506
2994.187078	775534.325520	40.057524
2996.863686	777042.738037	40.062541
3000.036059	778547.123887	40.067559
3002.983687	780041.713804	40.072576
3005.788049	781543.575018	40.077594
3008.959075	783045.995039	40.082612
3012.178018	784547.112058	40.087629
3015.078204	786007.315023	40.092647
3017.900763	787467.771389	40.097664
3020.650667	788922.401004	40.102682
3023.584791	790368.566697	40.107700
3026.561354	791836.184346	40.112717
3029.958740	793296.323849	40.117735
3032.420963	794762.338103	40.122752
3035.307618	796239.776381	40.127770
3038.614873	797713.846235	40.132788
3040.996146	799204.006302	40.137805
3044.091225	800691.673217	40.142823
3046.855883	802192.871068	40.147840
3049.607603	803697.852682	40.152858
3052.960010	805217.418622	40.157876
3055.707948	806743.151628	40.162893
3058.574130	808268.132843	40.167911
3061.605955	809803.935930	40.172928
3064.257266	811354.990756	40.177946
3067.295048	812904.111414	40.182964
3069.870854	814482.985944	40.187981
3073.146808	816043.064278	40.192999
3076.063768	817625.096564	40.198016
3079.146818	819210.483598	40.203034
3082.280130	820796.898778	40.208052
3085.164781	822411.997589	40.213069
3088.382019	824016.844165	40.218087
3091.570796	825623.985092	40.223104
3094.608204	827243.088428	40.228122
3098.070830	828860.550635	40.233140
3100.802001	830484.795365	40.238157
3103.722282	832119.171180	40.243175
3107.005256	833765.052348	40.248192
3109.990355	835414.310347	40.253210
3113.274537	837069.373380	40.258228
3116.228342	838729.560589	40.263245
3119.692980	840375.222073	40.268263
3122.684703	842037.409689	40.273280
3125.738286	843703.234454	40.278298
3128.820824	845379.307440	40.283316
3131.775949	847055.051696	40.288333
3135.190464	848733.478112	40.293351
3138.027992	850426.020685	40.298368
3141.336072	852119.967275	40.303386
3144.318743	853808.165357	40.308404
3147.041186	855508.270368	40.313421
3150.322796	857204.029816	40.318439
3153.502632	858925.332288	40.323456
3156.632151	860642.667489	40.328474
3160.199574	862352.757404	40.333492
3163.050804	864062.968140	40.338509
3166.160060	865791.255111	40.343527
3169.528221	867527.527462	40.348544
3172.330834	869248.672886	40.353562
3175.566720	870977.770697	40.358580
3178.364194	872722.891206	40.363597
3181.947080	874455.179960	40.368615
3185.205361	876207.713133	40.373632
3188.136444	877944.696421	40.378650
3191.400942	879682.561741	40.383668
3194.654225	881440.496138	40.388685
3197.778771	883188.648843	40.393703
3201.112949	884945.995846	40.398720
3204.048573	886689.456462	40.403738
3207.540866	888434.326272	40.408756
3210.586385	890200.932734	40.413773
3214.193787	891965.648953	40.418791
3217.537541	893718.678713	40.423808
3220.470158	895467.381201	40.428826
3224.241538	897167.994594	40.433844
3227.240826	898873.233871	40.438861
3230.256155	900575.451080	40.443879
3233.823489	902268.396826	40.448896
3237.187008	903978.382362	40.453914
3239.989777	905664.266320	40.458932
3243.313252	907384.760263	40.463949
3246.292712	909075.928714	40.468967
3249.680175	910786.989037	40.473984
3252.779604	912500.736989	40.479002
3255.899107	914233.353626	40.484020
3258.915916	915954.394020	40.489037
3261.795491	917682.979167	40.494055
3265.219477	919425.034356	40.499072
3268.671869	921175.640118	40.504090
3271.527365	922922.227837	40.509108
3274.999949	924690.393060	40.514125
3277.701697	926461.840868	40.519143
3281.320451	928228.909375	40.524160
3284.505755	930002.743400	40.529178
3287.771006	931793.304171	40.534196
3291.102542	933588.417401	40.539213
3294.426713	935396.796421	40.544231
3297.908012	937195.822110	40.549248
3301.323102	939010.019336	40.554266
3304.735857	940801.217095	40.559284
3307.713119	942608.019710	40.564301
3311.034347	944430.089087	40.569319
3314.899090	946253.622534	40.574336
3317.496549	948088.269436	40.579354
3321.420601	949911.831027	40.584372
3324.437304	951740.996613	40.589389
3327.650390	953609.475972	40.594407
3331.048213	955489.995836	40.599424
3334.404362	957383.012771	40.604442
3338.065172	959268.906669	40.609460
3341.501059	961175.620657	40.614477
3344.867279	963075.365112	40.619495
3348.143204	964963.559876	40.624512
3351.541322	966880.107700	40.629530
3355.041629	968782.043885	40.634548
3358.422476	970687.954403	40.639565
3361.832312	972590.495805	40.644583
3365.680501	974492.235499	40.649600
3369.042865	976404.825875	40.654618
3372.641048	978302.318498	40.659636
3376.240315	980196.064010	40.664653
3379.730743	982112.857953	40.669671
3383.514240	984003.751093	40.674688
3386.507593	985889.865743	40.679706
3390.342404	987792.627198	40.684724
3393.568875	989686.490306	40.689741
3396.863638	991588.458935	40.694759
3400.712908	993474.735323	40.699776
3404.047622	995378.730500	40.704794
3407.128654	997259.308839	40.709812
3410.687999	999160.830409	40.714829
3414.053622	1001053.981795	40.719847
3417.729384	1002945.963002	40.724864
3421.181417	1004847.335326	40.729882
3424.595057	1006730.139461	40.734900
3427.943074	1008637.909048	40.739917
3431.392284	1010533.294039	40.744935
3434.861859	1012438.399337	40.749952
3438.481747	1014328.409861	40.754970
3441.625457	1016220.475886	40.759988
3445.112529	1018120.747943	40.765005
3447.966073	1020017.988202	40.770010
3451.603438	1021852.019198	40.775015
3454.966473	1023631.330166	40.780020
3458.199765	1025353.139751	40.785024
3461.851760	1026996.880702	40.790029
3464.480750	1028576.121790	40.795034
3467.935825	1030070.481800	40.800039
3470.673385	1031507.665550	40.805044
3473.807173	1032851.161079	40.810048
3476.426163	1034124.397170	40.815053
3478.654311	1035331.365800	40.820058
3481.705074	1036455.185631	40.825063
3483.719652	1037523.759576	40.830068
3486.368168	1038496.353406	40.835072
3488.495988	1039421.904900	40.840077
3490.634762	1040271.754505	40.845082
3492.864030	1041060.702521	40.850087
3494.864373	1041791.918041	40.855092
3496.567811	1042438.299323	40.860096
3498.572088	1043045.642854	40.865101
3499.901321	1043594.233217	40.870106
3501.676938	1044086.895874	40.875111
3503.122586	1044532.364984	40.880116
3504.544168	1044911.682555	40.885120
3506.000904	1045259.985646	40.890125
3507.461179	1045565.028022	40.895130
3508.608526	1045812.392501	40.900135
3509.706053	1046042.093569	40.905140
3510.951733	1046206.525030	40.910144
3511.918012	1046347.451535	40.915149
3512.874276	1046455.180649	40.920154
3513.962739	1046515.602250	40.925159
3515.028748	1046552.192184	40.930164
3515.771670	1046554.964779	40.935168
3516.714267	1046523.254986	40.940173
3517.523760	1046481.724132	40.945178
3518.322536	1046380.268578	40.950183
3518.833673	1046285.420667	40.955188
3519.568806	1046156.178962	40.960192
3520.261159	1046005.130867	40.965197
3520.551515	1045832.912827	40.970202
3521.330894	1045642.850547	40.975207
3521.419695	1045435.715614	40.980212
3522.338951	1045219.073680	40.985216
3522.868858	1044965.035993	40.990221
3522.878837	1044715.512646	40.995226
3523.834018	1044428.753434	41.000231
3524.100921	1044144.313171	41.005236
3524.416702	1043840.734538	41.010240
3524.582014	1043525.191915	41.015245
3524.952038	1043200.231745	41.020250
3525.614207	1042859.561498	41.025255
3525.210505	1042518.949344	41.030260
3525.915703	1042156.887451	41.035264
3526.039800	1041786.108889	41.040269
3525.955877	1041427.799449	41.045274
3526.425454	1041036.340963	41.050279
3526.513012	1040651.293387	41.055284
3526.512885	1040256.572889	41.060288
3527.017336	1039860.002159	41.065293
3526.877850	1039458.388304	41.070298
3527.082740	1039045.286613	41.075303
3527.310930	1038631.860456	41.080308
3527.597394	1038197.809137	41.085312
3527.899753	1037776.285779	41.090317
3527.853595	1037342.125774	41.095322
3527.838326	1036897.776946	41.100327
3528.096347	1036456.151092	41.105332
3527.776488	1036004.530595	41.110336
3527.784823	1035549.918700	41.115341
3527.961979	1035119.996057	41.120346
3528.180411	1034659.571744	41.125351
3527.890060	1034207.703801	41.130356
3527.947451	1033752.646855	41.135360
3527.913865	1033289.636035	41.140365
3528.009309	1032837.399858	41.145370
3528.403558	1032370.469465	41.150375
3528.274789	1031907.843184	41.155380
3528.412576	1031433.620157	41.160384
3528.627541	1030958.182854	41.165389
3528.545241	1030478.108707	41.170394
3528.726617	1029992.433050	41.175399
3528.517120	1029523.331142	41.180404
3528.467889	1029034.996699	41.185408
3528.604653	1028550.558090	41.190413
3528.488193	1028068.636427	41.195418
3528.370440	1027573.311270	41.200423
3528.488748	1027090.685557	41.205428
3528.532484	1026612.194703	41.210432
3528.291621	1026122.959177	41.215437
3528.200572	1025633.268686	41.220442
3528.104926	1025142.373614	41.225447
3528.391441	1024673.266767	41.230452
3528.306201	1024176.084995	41.235456
3528.032567	1023687.804337	41.240461
3528.279019	1023206.178562	41.245466
3528.283907	1022706.138018	41.250471
3527.785282	1022221.739829	41.255476
3527.889391	1021729.252313	41.260480
3528.251937	1021240.071691	41.265485
3527.834053	1020747.099108	41.270490
3528.128161	1020247.857753	41.275495
3527.959337	1019767.167980	41.280500
3527.739451	1019280.821096	41.285504
3527.814714	1018782.357983	41.290509
3527.664618	1018295.526205	41.295514
3527.845130	1017803.650899	41.300519
3527.785184	1017318.174379	41.305524
3527.574815	1016817.740626	41.310528
3527.832870	1016328.342571	41.315533
3527.625909	1015840.724999	41.320538
3527.565788	1015344.404454	41.325543
3527.589293	1014858.992586	41.330548
3527.460505	1014368.322867	41.335552
3527.525320	1013870.007407	41.340557
3527.362705	1013387.119761	41.345562
3527.459731	1012886.090807	41.350567
3527.209859	1012400.414505	41.355572
3526.947261	1011910.814434	41.360576
3526.922645	1011419.870152	41.365581
3526.813795	1010940.842018	41.370586
3526.870574	1010456.015565	41.375591
3526.715329	1009980.604016	41.380596
3526.639574	1009505.042083	41.385600
3527.105096	1009015.750136	41.390605
3526.376421	1008531.858860	41.395610
3526.450162	1008042.255433	41.400615
3526.807517	1007576.953138	41.405620
3526.254315	1007103.404896	41.410624
3526.695694	1006608.854536	41.415629
3526.296160	1006137.823979	41.420634
3526.331416	1005639.853643	41.425639
3526.115516	1005171.045037	41.430644
3526.082915	1004685.347814	41.435648
3526.137576	1004219.429476	41.440653
3525.967900	1003745.633313	41.445658
3525.874823	1003267.894895	41.450663
3525.561522	1002795.987646	41.455668
3525.390064	1002320.321596	41.460672
3525.480630	1001854.591277	41.465677
3525.421257	1001389.528234	41.470682
3525.339903	1000916.258413	41.475687
3525.364475	1000457.039356	41.480692
3525.195628	999976.116220	41.485696
3524.948488	999511.513450	41.490701
3525.080861	999056.639264	41.495706
3525.196193	998588.689465	41.500711
3525.290129	998129.951366	41.505716
3524.836297	997669.319469	41.510720
3525.026744	997210.783026	41.515725
3524.857273	996754.021217	41.520730
3524.624201	996287.398996	41.525735
3524.443944	995824.429886	41.530740
3524.445635	995367.528095	41.535744
3524.349083	994906.515251	41.540749
3523.729740	994463.959350	41.545754
3524.349395	994011.424187	41.550759
3524.217715	993561.801709	41.555764
3523.965560	993110.702116	41.560768
3524.493703	992653.007773	41.565773
3524.467355	992213.101432	41.570778
3524.444778	991751.137880	41.575783
3524.303329	991298.999048	41.580788
3523.834602	990852.140988	41.585792
3524.178261	990401.702552	41.590797
3523.793477	989958.074238	41.595802
3523.655967	989506.181947	41.600807
3523.553000	989059.805026	41.605812
3523.377882	988622.082317	41.610816
3523.571044	988175.782204	41.615821
3523.337428	987746.289737	41.620826
3523.681390	987304.869643	41.625831
3523.398343	986854.838544	41.630836
3523.062827	986428.091679	41.635840
3523.409487	985986.178718	41.640845
3522.763568	985533.274119	41.645850
3522.893726	985093.863910	41.650855
3523.049655	984664.757600	41.655860
3522.726344	984234.234314	41.660864
3522.656445	983806.076270	41.665869
3522.585323	983372.909247	41.670874
3522.536959	982952.978580	41.675879
3522.729558	982536.295782	41.680884
3522.329223	982094.692021	41.685888
3522.155287	981677.421187	41.690893
3522.240942	981259.686564	41.695898
3522.326438	980832.060563	41.700903
3522.345603	980399.043285	41.705908
3522.023555	979985.578690	41.710912
3521.941474	979575.560136	41.715917
3521.815436	979152.725844	41.720922
3521.870277	978726.119062	41.725927
3522.105454	978318.790385	41.730932
3521.984739	977903.579062	41.735936
3521.727284	977475.269733	41.740941
3521.745553	977064.859040	41.745946
3521.512637	976640.879475	41.750951
3521.555168	976237.830887	41.755956
3521.308547	975830.697396	41.760960
3521.506985	975410.073340	41.765965
3521.267751	974998.286322	41.770970
3521.569981	974591.658353	41.775975
3521.150884	974186.684259	41.780980
3520.995566	973775.870652	41.785984
3520.997782	973371.160461	41.790989
3520.544314	972975.784535	41.795994
3520.703059	972573.143017	41.800999
3520.931144	972175.252994	41.806004
3520.733899	971775.351894	41.811008
3520.532737	971382.366863	41.816013
3520.483647	970995.589035	41.821018
3520.490886	970586.867108	41.826023
3520.576726	970187.493229	41.831028
3520.218320	969799.414083	41.836032
3520.070507	969402.078229	41.841037
3519.782135	969024.891769	41.846042
3519.682187	968644.909945	41.851047
3519.835136	968255.957251	41.856052
3519.709243	967870.840419	41.861056
3519.876342	967487.900258	41.866061
3519.465515	967118.143845	41.871066
3519.309728	966728.649210	41.876071
3519.415578	966352.886035	41.881076
3519.349611	965985.153200	41.886080
3519.462775	965599.942572	41.891085
3519.246636	965233.263170	41.896090
3519.127634	964846.865536	41.901095
3519.314063	964484.967318	41.906100
3519.237890	964120.935409	41.911104
3519.163309	963731.615907	41.916109
3518.845066	963363.756918	41.921114
3518.890037	962988.077587	41.926119
3519.020719	962630.576949	41.931124
3518.808680	962263.903387	41.936128
3518.559640	961895.449367	41.941133
3518.545489	961530.263745	41.946138
3518.532304	961168.189761	41.951143
3518.039582	960809.797031	41.956148
3518.038662	960455.612072	41.961152
3518.147572	960087.963202	41.966157
3518.069184	959754.422863	41.971162
3517.971127	959392.839205	41.976167
3518.131815	959043.146681	41.981172
3517.830849	958694.881132	41.986176
3517.859417	958333.602202	41.991181
3517.972929	957987.087910	41.996186
3517.991433	957632.236116	42.001191
3518.049038	957286.767265	42.006196
3517.424233	956944.527406	42.011200
3517.646153	956591.931047	42.016205
3517.367593	956261.359030	42.021210
3517.357824	955906.209625	42.026215
3517.491988	955573.176833	42.031220
3517.232798	955231.559627	42.036224
3517.298460	954889.574466	42.041229
3517.310916	954557.287726	42.046234
3517.004528	954216.599046	42.051239
3517.157958	953874.637420	42.056244
3516.802908	953544.609072	42.061248
3517.594106	953202.012095	42.066253
3517.175879	952871.955740	42.071258
3516.803818	952543.195599	42.076263
3516.985354	952213.551499	42.081268
3516.938240	951898.651153	42.086272
3516.583673	951561.689460	42.091277
3516.409720	951252.699684	42.096282
3516.406577	950930.654564	42.101287
3516.599172	950613.339705	42.106292
3516.319758	950301.726978	42.111296
3516.391911	949979.322457	42.116301
3516.174871	949674.836353	42.121306
3515.772174	949357.541581	42.126311
3515.895369	949050.283205	42.131316
3515.938538	948743.689419	42.136320
3515.846359	948436.621099	42.141325
3515.615136	948132.715492	42.146330
3515.857586	947833.977816	42.151335
3515.777839	947535.850121	42.156340
3515.647840	947240.010669	42.161344
3515.750455	946929.948515	42.166349
3515.567910	946643.464464	42.171354
3515.551352	946322.472001	42.176359
3515.499066	946021.954303	42.181364
3515.256832	945730.163415	42.186368
3515.220249	945428.076520	42.191373
3515.088697	945137.861670	42.196378
3515.091920	944848.661693	42.201383
3515.115530	944547.854036	42.206388
3514.765750	944274.577801	42.211392
3514.956717	943974.762725	42.216397
3514.841394	943693.946292	42.221402
3514.657036	943408.911195	42.226407
3514.687811	943121.430053	42.231412
3514.564411	942851.873188	42.236416
3514.374252	942556.349785	42.241421
3514.228499	942290.599668	42.246426
3514.524339	941994.293487	42.251431
3514.574789	941728.961367	42.256436
3514.417741	941447.646785	42.261440
3514.205720	941156.167800	42.266445
3514.080173	940888.234259	42.271450
3514.018950	940619.892948	42.276455
3513.903252	940342.920515	42.281460
3513.859838	940068.509453	42.286464
3513.962832	939795.785249	42.291469
3514.070392	939532.152950	42.296474
3513.485927	939262.869300	42.301479
3513.403957	938996.556867	42.306484
3513.420201	938738.939467	42.311488
3513.610623	938466.418996	42.316493
3513.362511	938219.174747	42.321498
3513.527254	937944.713577	42.326503
3513.557675	937683.589730	42.331508
3513.361897	937433.518722	42.336512
3513.582729	937163.610585	42.341517
3513.187731	936913.451654	42.346522
3513.411953	936651.477130	42.351527
3513.468948	936400.739688	42.356532
3512.938668	936145.770419	42.361536
3513.213462	935872.525504	42.366541
3513.128945	935638.178839	42.371546
3512.893605	935372.570712	42.376551
3513.074472	935120.408584	42.381556
3512.944327	934862.720636	42.386560
3512.824969	934610.583530	42.391565
3512.482914	934371.713080	42.396570
3512.342094	934121.379255	42.401575
3512.762326	933881.017509	42.406580
3512.295637	933641.462716	42.411584
3512.664970	933389.666515	42.416589
3512.238561	933155.745521	42.421594
3512.422830	932913.458992	42.426599
3512.318455	932674.568470	42.431604
3512.250170	932435.565209	42.436608
3512.305536	932200.370619	42.441613
3511.908372	931968.216138	42.446618
3511.812836	931717.568845	42.451623
3512.099523	931492.961242	42.456628
3512.029504	931261.489932	42.461632
3512.260330	931018.916926	42.466637
3511.940692	930798.700578	42.471642
3512.194997	930566.953462	42.476647
3511.953644	930327.787536	42.481652
3511.535571	930104.773713	42.486656
3511.873463	929864.339065	42.491661
3511.431286	929642.558299	42.496666
3511.578139	929416.445181	42.501671
3511.599305	929194.185182	42.506676
3511.560872	928971.061224	42.511680
3511.726598	928746.741570	42.516685
3511.756842	928526.085170	42.521690
3511.219969	928303.687793	42.526695
3511.377782	928076.651351	42.531700
3511.104159	927853.711464	42.536704
3511.158178	927631.669064	42.541709
3511.204061	927419.995700	42.546714
3510.919394	927202.026688	42.551719
3511.144100	926974.932343	42.556724
3510.465928	926764.697552	42.561728
3510.497840	926559.815093	42.566733
3511.037562	926358.300786	42.571738
3510.686572	926144.431924	42.576743
3511.030313	925936.302726	42.581748
3510.560264	925739.448611	42.586752
3511.102913	925517.814562	42.591757
3510.657071	925309.118254	42.596762
3510.413874	925102.495163	42.601767
3510.712893	924896.447672	42.606772
3510.316420	924701.177454	42.611776
3510.808169	924480.854776	42.616781
3510.104997	924279.755482	42.621786
3509.921167	924070.102530	42.626791
3510.133946	923882.970440	42.631796
3510.057289	923689.341352	42.636800
3510.497128	923490.812543	42.641805
3510.241757	923298.064186	42.646810
3509.732641	923101.600482	42.651815
3510.190902	922902.277645	42.656820
3509.995276	922711.806370	42.661824
3510.014126	922500.904848	42.666829
3509.874642	922326.663548	42.671834
3510.025535	922139.192505	42.676839
3509.850617	921932.051559	42.681844
3509.691297	921747.022515	42.686848
3509.875818	921548.464200	42.691853
3509.466587	921362.405074	42.696858
3509.513532	921177.226322	42.701863
3509.625920	920992.222837	42.706868
3509.465628	920813.895808	42.711872
3509.477497	920623.701420	42.716877
3509.918694	920434.872726	42.721882
3509.218147	920251.709570	42.726887
3509.459363	920070.501764	42.731892
3509.023219	919890.265446	42.736896
3509.110849	919701.276979	42.741901
3509.115805	919541.162673	42.746906
3509.295663	919367.639341	42.751911
3509.641823	919180.995807	42.756916
3509.234589	918998.126835	42.761920
3509.560304	918812.725032	42.766925
3509.226223	918639.263072	42.771930
3509.109135	918458.541618	42.776935
3509.272062	918276.035590	42.781940
3508.987722	918105.628253	42.786945
3508.910292	917925.267518	42.791949
3508.575751	917751.199752	42.796954
3508.695451	917586.484882	42.801959
3508.741127	917410.418404	42.806964
3508.718090	917239.459559	42.811969
3508.913184	917064.416180	42.816973
3508.943915	916909.033398	42.821978
3508.944969	916737.188386	42.826983
3508.968591	916569.377835	42.831988
3508.954856	916400.990598	42.836993
3508.670081	916215.889705	42.841997
3508.642426	916055.196667	42.847002
3508.472947	915887.204365	42.852007
3508.939652	915721.798231	42.857012
3508.434216	915551.154783	42.862017
3508.599046	915387.328960	42.867021
3508.623866	915227.180687	42.872026
3508.266282	915054.378759	42.877031
3508.440382	914900.359695	42.882036
3508.007906	914744.317446	42.887041
3507.910355	914581.377472	42.892045
3508.264305	914430.301191	42.897050
3508.302569	914276.575890	42.902055
3508.409661	914113.973554	42.907060
3508.173371	913950.170774	42.912065
3508.060655	913776.228583	42.917069
3508.214920	913616.975112	42.922074
3507.868609	913462.712362	42.927079
3508.276057	913299.843727	42.932084
3507.640255	913156.505754	42.937089
3507.861611	913001.462151	42.942093
3507.765548	912850.320131	42.947098
3507.728929	912695.695762	42.952103
3508.181126	912546.381938	42.957108
3507.843411	912393.147515	42.962113
3508.013200	912236.838281	42.967117
3508.115077	912097.494267	42.972122
3507.934726	911940.752528	42.977127
3507.872663	911779.265175	42.982132
3507.722455	911640.240188	42.987137
3507.716934	911475.747363	42.992141
3507.639338	911335.835432	42.997146
3507.430340	911188.521052	43.002151
3507.782499	911041.784893	43.007156
3507.334788	910900.670029	43.012161
3507.783966	910746.778222	43.017165
3507.440561	910602.168903	43.022170
3507.190187	910458.407914	43.027175
3507.483277	910312.625919	43.032180
3507.267176	910180.321962	43.037185
3507.593480	910036.165797	43.042189
3507.361469	909894.314900	43.047194
3507.561695	909759.522433	43.052199
3507.770264	909608.819601	43.057204
3507.476833	909485.862373	43.062209
3507.429884	909327.289115	43.067213
3507.385258	909181.532911	43.072218
3507.565915	909037.181873	43.077223
3507.609579	908890.632191	43.082228
3507.122717	908751.011379	43.087233
3507.089204	908604.756078	43.092237
3507.203681	908485.855285	43.097242
3507.148629	908351.649073	43.102247
3507.165375	908209.617544	43.107252
3507.277021	908065.927512	43.112257
3507.219777	907927.854385	43.117261
3507.086052	907794.901206	43.122266
3507.066819	907663.276028	43.127271
3507.190037	907527.863309	43.132276
3506.801742	907396.389034	43.137281
3507.209905	907257.258166	43.142285
3507.418802	907120.760568	43.147290
3506.881156	906974.448867	43.152295
3507.153472	906844.781571	43.157300
3506.624207	906713.217888	43.162305
3507.086413	906588.914464	43.167309
3506.893632	906455.263766	43.172314
3506.526796	906318.069675	43.177319
3506.939084	906190.003791	43.182324
3506.807715	906064.918330	43.187329
3506.594695	905931.547757	43.192333
3506.793323	905800.807175	43.197338
3506.477561	905683.267741	43.202343
3506.451054	905551.883138	43.207348
3506.457972	905442.388835	43.212353
3506.932819	905302.522791	43.217357
3506.536143	905174.277409	43.222362
3506.334771	905055.934083	43.227367
3506.483347	904936.662273	43.232372
3506.494401	904815.673902	43.237377
3506.394430	904684.184464	43.242381
3506.400587	904564.735198	43.247386
3506.154779	904448.701966	43.252391
3506.475268	904316.941627	43.257396
3506.230215	904208.911967	43.262401
3506.013094	904088.620868	43.267405
3505.930313	903966.375118	43.272410
3506.087917	903863.483233	43.277415
3506.185060	903742.746917	43.282420
3506.149287	903638.145742	43.287425
3506.264793	903516.050477	43.292429
3505.862190	903395.485499	43.297434
3505.369514	903285.934685	43.302439
3505.778855	903177.680763	43.307444
3505.999877	903073.123221	43.312449
3506.359055	902953.967407	43.317453
3506.232410	902844.926735	43.322458
3505.966733	902729.922754	43.327463
3506.000315	902602.898664	43.332468
3506.029612	902493.149810	43.337473
3506.007206	902378.098525	43.342477
3506.037491	902265.545863	43.347482
3505.881167	902165.859836	43.352487
3505.849967	902048.776164	43.357492
3505.708547	901942.519710	43.362497
3505.478635	901835.407024	43.367501
3505.552476	901723.512037	43.372506
3505.432994	901621.589959	43.377511
3505.640429	901506.579462	43.382516
3505.412619	901414.904568	43.387521
3505.741496	901312.903017	43.392525
3505.835194	901206.207715	43.397530
3505.564081	901101.404858	43.402535
3505.717263	900999.330016	43.407540
3505.161782	900900.652745	43.412545
3505.567416	900789.843081	43.417549
3505.633721	900686.425157	43.422554
3505.063526	900584.558514	43.427559
3505.390437	900481.286990	43.432564
3505.132046	900388.248590	43.437569
3505.532136	900287.471959	43.442573
3505.255953	900205.055009	43.447578
3505.388899	900099.008158	43.452583
3505.428614	899990.463988	43.457588
3505.016063	899896.090940	43.462593
3505.481745	899787.086406	43.467597
3505.585223	899690.403826	43.472602
3505.257396	899590.507212	43.477607
3505.225786	899493.650367	43.482612
3505.358513	899395.123010	43.487617
3504.836390	899304.717671	43.492621
3505.140439	899206.351942	43.497626
3504.969923	899117.720660	43.502631
3504.841123	899027.632394	43.507636
3504.830304	898936.847171	43.512641
3504.907824	898839.961117	43.517645
3504.922662	898755.060390	43.522650
3504.399469	898668.894805	43.527655
3504.801144	898569.632609	43.532660
3505.132354	898484.675693	43.537665
3504.913730	898395.751224	43.542669
3504.854057	898303.514983	43.547674
3504.750837	898221.716682	43.552679
3504.589337	898140.989357	43.557684
3504.706385	898054.129325	43.562689
3504.574264	897956.006874	43.567693
3504.670140	897869.533893	43.572698
3504.637579	897792.740991	43.577703
3504.937952	897698.310303	43.582708
3504.841848	897611.285379	43.587713
3504.820158	897520.962220	43.592717
3504.599416	897446.031146	43.597722
3504.780058	897353.643207	43.602727
3504.741434	897267.086567	43.607732
3504.627854	897194.453177	43.612737
3504.698405	897097.345178	43.617741
3504.649418	897011.462636	43.622746
3504.550941	896937.180990	43.627751
3504.688385	896843.922301	43.632756
3504.477107	896763.473372	43.637761
3504.343808	896669.096972	43.642765
3504.564157	896592.342739	43.647770
3504.546543	896514.467182	43.652775
3504.642640	896420.145468	43.657780
3504.528679	896356.584210	43.662785
3504.543473	896273.385525	43.667789
3504.704943	896195.669343	43.672794
3504.654025	896116.634255	43.677799
3504.565085	896021.370086	43.682804
3504.388105	895940.903831	43.687809
3504.174686	895865.660741	43.692813
3504.306831	895781.082610	43.697818
3504.267705	895701.170063	43.702823
3504.510885	895634.256179	43.707828
3504.380177	895545.755644	43.712833
3504.401285	895465.733220	43.717837
3504.498977	895388.596352	43.722842
3504.115571	895311.827632	43.727847
3504.488495	895243.051520	43.732852
3504.223853	895159.495965	43.737857
3504.314076	895078.973472	43.742861
3504.523787	895004.615746	43.747866
3504.411734	894929.343550	43.752871
3504.496174	894838.960188	43.757876
3504.211630	894769.223488	43.762881
3504.300092	894689.082381	43.767885
3504.177810	894612.647815	43.772890
3504.079991	894534.758324	43.777895
3504.222195	894456.828222	43.782900
3503.941260	894389.792730	43.787905
3504.040421	894318.924028	43.792909
3504.322540	894242.997840	43.797914
3503.980858	894178.483098	43.802919
3503.977649	894098.058783	43.807924
3504.087650	894026.121335	43.812929
3504.207242	893951.088033	43.817933
3504.203778	893877.910728	43.822938
3504.153585	893807.253607	43.827943
3504.301224	893726.315842	43.832948
3504.052357	893670.480485	43.837953
3503.961153	893583.876367	43.842957
3504.239891	893507.844273	43.847962
3504.131961	893455.077192	43.852967
3503.966703	893368.288649	43.857972
3503.830325	893307.984034	43.862977
3503.614897	893234.156637	43.867981
3503.721912	893174.583952	43.872986
3503.842598	893100.506088	43.877991
3503.987132	893023.619515	43.882996
3503.766076	892971.059961	43.888001
3503.880395	892903.361752	43.893005
3503.745049	892839.861398	43.898010
3503.511488	892768.351438	43.903015
3503.563582	892701.821344	43.908020
3503.317318	892644.331798	43.913025
3503.679278	892574.848478	43.918029
3504.271227	892516.929479	43.923034
3503.711255	892459.393063	43.928039
3504.130918	892393.959144	43.933044
3503.892554	892325.151861	43.938049
3503.678565	892252.085088	43.943053
3504.057513	892188.879552	43.948058
3503.628100	892119.424383	43.953063
3504.047563	892050.698814	43.958068
3503.808244	891992.814767	43.963073
3503.753210	891921.651600	43.968077
3503.961564	891847.059536	43.973082
3503.496483	891786.889717	43.978087
3503.734156	891720.801157	43.983092
3503.584716	891659.707647	43.988097
3503.783122	891589.078828	43.993101
3503.602212	891524.700998	43.998106
3503.387539	891468.354922	44.003111
3503.620640	891406.905560	44.008116
3503.836495	891341.203058	44.013121
3503.746248	891277.000929	44.018125
3503.508244	891215.820560	44.023130
3503.514924	891157.984250	44.028135
3503.903410	891087.511362	44.033140
3503.727253	891030.961204	44.038145
3503.647360	890966.753892	44.043149
3503.974548	890897.352667	44.048154
3503.530864	890836.782452	44.053159
3503.842960	890772.605105	44.058164
3503.768891	890708.393940	44.063169
3503.727143	890638.663479	44.068173
3503.682577	890584.311879	44.073178
3503.424265	890520.902765	44.078183
3503.747259	890459.815349	44.083188
3503.711459	890396.755111	44.088193
3503.535759	890332.653211	44.093197
3503.484367	890264.467452	44.098202
3503.496619	890204.395815	44.103207
3503.492741	890149.162809	44.108212
3503.446571	890091.034251	44.113217
3503.504630	890028.534901	44.118221
3503.611858	889968.638618	44.123226
3503.464581	889909.170586	44.128231
3503.316865	889851.346539	44.133236
3503.402162	889791.355283	44.138241
3503.469591	889727.400043	44.143245
3503.410543	889673.429160	44.148250
3503.293175	889623.530496	44.153255
3503.528311	889566.511174	44.158260
3503.536714	889514.559264	44.163265
3503.336179	889445.614414	44.168269
3503.666705	889389.448315	44.173274
3503.405565	889336.861994	44.178279
3503.368361	889277.562780	44.183284
3503.510451	889223.651282	44.188289
3503.375478	889159.916571	44.193293
3503.586941	889095.640328	44.198298
3503.255308	889040.740917	44.203303
3503.290580	888978.137151	44.208308
3503.223956	888922.902698	44.213313
3503.391847	888869.757656	44.218317
3503.449597	888815.565971	44.223322
3503.266479	888770.218191	44.228327
3503.630031	888699.623378	44.233332
3503.464808	888641.209505	44.238337
3503.486676	888589.440537	44.243341
3503.439278	888530.232059	44.248346
3502.979071	888486.862882	44.253351
3503.304033	888422.463667	44.258356
3503.276558	888370.313816	44.263361
3503.487126	888316.866357	44.268365
3503.381330	888259.890266	44.273370
3503.180930	888208.057727	44.278375
3503.398025	888156.155938	44.283380
3503.119072	888094.949058	44.288385
3502.674457	888038.413664	44.293389
3502.954219	887994.144720	44.298394
3502.627510	887949.104434	44.303399
3502.949506	887898.344270	44.308404
3502.991715	887856.919736	44.313409
3503.141346	887806.283931	44.318413
3503.103347	887751.130297	44.323418
3503.119558	887705.644521	44.328423
3503.012945	887653.501223	44.333428
3503.116510	887609.935780	44.338433
3502.933621	887552.481524	44.343437
3503.014390	887498.370438	44.348442
3502.876519	887455.037157	44.353447
3502.869248	887399.391211	44.358452
3502.996375	887352.142367	44.363457
3502.996110	887301.236491	44.368461
3503.368260	887254.527160	44.373466
3502.788243	887213.006957	44.378471
3503.176509	887151.680137	44.383476
3503.113197	887104.170293	44.388481
3502.832034	887056.115247	44.393485
3503.153036	887001.959931	44.398490
3503.209434	886962.559125	44.403495
3503.315899	886899.243559	44.408500
3502.923321	886862.529278	44.413505
3503.036545	886810.535721	44.418509
3503.276746	886758.907932	44.423514
3502.997797	886707.171634	44.428519
3503.408199	886654.450183	44.433524
3503.208873	886611.120693	44.438529
3502.931834	886552.897669	44.443533
3503.223351	886502.904612	44.448538
3502.902649	886450.398547	44.453543
3503.003025	886409.050841	44.458548
3503.018436	886359.876396	44.463553
3503.207346	886304.284378	44.468557
3503.218285	886251.431478	44.473562
3502.638219	886210.968841	44.478567
3502.624408	886161.313531	44.483572
3502.830427	886114.428771	44.488577
3502.788446	886064.002870	44.493581
3503.087888	886020.296375	44.498586
3502.798970	885977.460902	44.503591
3503.033535	885927.181852	44.508596
3502.775550	885885.502235	44.513601
3502.773928	885836.326148	44.518605
3502.906670	885791.677349	44.523610
3502.835083	885751.805357	44.528615
3502.613120	885700.631497	44.533620
3503.214092	885658.421502	44.538625
3503.290942	885614.167774	44.543629
3503.270410	885557.054162	44.548634
3502.961574	885514.993018	44.553639
3502.811822	885467.774402	44.558644
3502.715327	885411.736787	44.563649
3502.652959	885370.311666	44.568653
3502.847809	885317.807193	44.573658
3502.725060	885289.461190	44.578663
3502.621705	885240.877690	44.583668
3502.882533	885205.691074	44.588673
3502.883798	885155.734215	44.593677
3503.032916	885106.527099	44.598682
3502.721152	885069.884931	44.603687
3502.986671	885022.691087	44.608692
3502.912373	884975.165572	44.613697
3502.717202	884935.017864	44.618701
3502.524333	884883.541533	44.623706
3502.645201	884847.407601	44.628711
3502.866354	884796.540033	44.633716
3502.849681	884762.655134	44.638721
3502.555593	884730.268086	44.643725
3502.955805	884672.398679	44.648730
3502.819697	884637.177191	44.653735
3502.488816	884593.563797	44.658740
3502.583298	884552.978422	44.663745
3502.565315	884522.384413	44.668749
3502.920218	884466.844256	44.673754
3502.772826	884433.366281	44.678759
3502.669618	884391.747243	44.683764
3502.708289	884348.167947	44.688769
3502.373937	884299.033640	44.693773
3502.696123	884264.315364	44.698778
3502.845316	884223.815506	44.703783
3502.979991	884171.988404	44.708788
3502.907751	884124.939748	44.713793
3502.869015	884082.339541	44.718797
3502.938869	884035.944589	44.723802
3502.657956	883997.644375	44.728807
3502.642829	883957.169732	44.733812
3502.666989	883918.915571	44.738817
3502.503158	883868.200141	44.743821
3502.022291	883823.153108	44.748826
3501.947563	883799.149618	44.753831
3501.983596	883775.902491	44.758836
3502.162828	883737.912107	44.763841
3502.363818	883721.513179	44.768845
3502.575072	883677.803584	44.773850
3502.030268	883646.323353	44.778855
3501.929363	883609.056167	44.783860
3502.575103	883574.474153	44.788865
3502.154654	883542.101289	44.793869
3502.667513	883499.115403	44.798874
3502.560163	883467.368442	44.803879
3502.349227	883423.339117	44.808884
3502.305417	883398.554123	44.813889
3502.381751	883355.735943	44.818893
3502.363935	883315.741507	44.823898
3502.286248	883285.441362	44.828903
3502.469282	883253.451698	44.833908
3502.444572	883219.655973	44.838913
3501.998728	883185.251495	44.843917
3502.446972	883149.343619	44.848922
3502.319489	883115.757921	44.853927
3502.090849	883071.438299	44.858932
3502.483349	883027.209707	44.863937
3502.189622	883014.861198	44.868941
3502.407445	882964.462413	44.873946
3502.193612	882946.386308	44.878951
3502.217111	882914.033654	44.883956
3502.275433	882881.190815	44.888961
3501.811867	882849.789733	44.893965
3502.157606	882823.485297	44.898970
3502.431652	882787.216474	44.903975
3502.178140	882752.487181	44.908980
3502.248488	882724.290553	44.913985
3502.529531	882708.456725	44.918989
3502.711949	882663.678850	44.923994
3502.278484	882634.693078	44.928999
3502.163979	882608.560359	44.934004
3502.383631	882565.519042	44.939009
3502.281401	882540.062005	44.944013
3502.058904	882500.483129	44.949018
3502.147853	882476.447216	44.954023
3502.281895	882433.419029	44.959028
3502.496022	882406.262648	44.964033
3502.104847	882363.514200	44.969037
3502.192342	882341.027765	44.974042
3502.443850	882306.890648	44.979047
3502.457992	882271.726937	44.984052
3502.416324	882233.569413	44.989057
3502.273085	882203.274437	44.994061
3502.685313	882166.397802	44.999066
3502.451969	882132.145813	45.004071
3502.343046	882094.289057	45.009076
3502.461674	882054.360349	45.014081
3502.490580	882029.170078	45.019085
3502.648809	881968.117033	45.024090
3502.477417	881938.987749	45.029095
3502.287706	881905.599065	45.034100
3502.812916	881866.764527	45.039105
3502.431506	881834.375723	45.044109
3502.389031	881786.334550	45.049114
3502.457885	881765.302047	45.054119
3502.659996	881734.463377	45.059124
3502.240744	881691.133385	45.064129
3502.331046	881663.412710	45.069133
3502.772164	881625.559165	45.074138
3502.167826	881584.971363	45.079143
3502.075525	881549.045833	45.084148
3502.386670	881518.963069	45.089153
3502.408158	881493.577956	45.094157
3502.370577	881450.861434	45.099162
3502.103668	881434.145661	45.104167
3502.442420	881396.210619	45.109172
3502.485207	881358.808487	45.114177
3502.372383	881332.088496	45.119181
3502.546699	881290.110923	45.124186
3502.332372	881263.310460	45.129191
3502.176812	881222.936840	45.134196
3502.256463	881192.406131	45.139201
3502.010018	881158.731874	45.144205
3502.262287	881127.687977	45.149210
3502.296265	881091.545062	45.154215
3502.230891	881065.784869	45.159220
3502.516067	881031.925411	45.164225
3501.905719	881005.673432	45.169229
3501.995843	880959.928851	45.174234
3502.400924	880938.450435	45.179239
3502.321235	880904.650354	45.184244
3502.065228	880875.335928	45.189249
3501.927099	880844.161073	45.194253
3502.371881	880811.533581	45.199258
3502.354816	880791.965052	45.204263
3502.252226	880763.787450	45.209268
3502.048511	880719.930291	45.214273
3502.266834	880705.360943	45.219277
3502.355055	880664.458852	45.224282
3502.258398	880639.380167	45.229287
3502.281627	880593.062394	45.234292
3502.349598	880571.735068	45.239297
3502.315933	880544.320188	45.244301
3502.372475	880511.561207	45.249306
3502.036066	880472.084233	45.254311
3502.079233	880447.175474	45.259316
3502.131971	880404.824004	45.264321
3502.024941	880390.888847	45.269325
3502.016222	880348.547096	45.274330
3502.091963	880328.186559	45.279335
3502.140232	880305.020483	45.284340
3502.399128	880268.835430	45.289345
3502.038991	880242.441894	45.294349
3502.405516	880206.529417	45.299354
3502.460589	880184.815215	45.304359
3502.374053	880146.360756	45.309364
3502.363402	880104.986552	45.314369
3502.038149	880083.237734	45.319373
3502.095260	880037.200682	45.324378
3502.213765	880025.553116	45.329383
3502.037959	879993.314022	45.334388
3502.287228	879973.020563	45.339393
3502.200301	879936.793535	45.344397
3502.302145	879903.345372	45.349402
3502.331664	879878.533347	45.354407
3501.943361	879839.932786	45.359412
3502.331127	879809.731720	45.364417
3502.317009	879791.903643	45.369421
3502.404681	879754.774580	45.374426
3502.167844	879718.958526	45.379431
3501.945506	879689.923327	45.384436
3502.086706	879662.184789	45.389441
3502.028023	879633.800698	45.394445
3502.293607	879594.993884	45.399450
3502.238606	879577.365707	45.404455
3502.290144	879544.020691	45.409460
3502.232177	879498.870552	45.414465
3501.961537	879469.842220	45.419469
3501.996059	879442.023306	45.424474
3502.139996	879416.996656	45.429479
3502.005570	879387.073272	45.434484
3502.294909	879355.723149	45.439489
3502.000561	879342.688567	45.444493
3502.199759	879296.331551	45.449498
3502.345397	879282.449040	45.454503
3501.900365	879238.329798	45.459508
3502.124834	879220.654504	45.464513
3502.160179	879193.221933	45.469517
3502.185884	879156.874613	45.474522
3501.989515	879125.409453	45.479527
3502.281634	879105.202854	45.484532
3501.883171	879082.977796	45.489537
3501.585955	879052.401109	45.494541
3502.027211	879029.359081	45.499546
3502.149554	879003.074297	45.504551
3502.387089	878976.382744	45.509556
3502.277481	878934.338154	45.514561
3501.896171	878916.180236	45.519565
3502.105289	878881.254782	45.524570
3502.211684	878844.504555	45.529575
3502.080811	878828.146593	45.534580
3502.075439	878794.128247	45.539585
3501.755741	878782.259648	45.544589
3501.783876	878744.843240	45.549594
3502.105524	878731.511963	45.554599
3502.120979	878699.912699	45.559604
3502.187816	878664.621707	45.564609
3502.117832	878658.914818	45.569613
3502.225903	878615.378226	45.574618
3502.071601	878594.661877	45.579623
3502.225554	878561.972882	45.584628
3502.294171	878528.231581	45.589633
3501.821979	878505.337999	45.594637
3502.158055	878477.658686	45.599642
3502.155967	878453.039695	45.604647
3501.763756	878427.224819	45.609652
3501.974256	878383.669635	45.614657
3501.593141	878356.398696	45.619661
3501.602062	878353.974081	45.624666
3501.882423	878335.899207	45.629671
3501.934039	878309.622975	45.634676
3502.200431	878283.311240	45.639681
3501.824327	878251.386357	45.644685
3502.100949	878217.415142	45.649690
3501.853436	878197.778989	45.654695
3501.840814	878180.624290	45.659700
3502.012134	878154.618438	45.664705
3501.718677	878130.433828	45.669709
3501.562884	878100.216606	45.674714
3501.692509	878096.221072	45.679719
3501.862798	878070.796617	45.684724
3502.005923	878037.524892	45.689729
3501.756945	878021.087205	45.694733
3502.034502	877987.986920	45.699738
3501.959606	877974.040721	45.704743
3501.939370	877944.575844	45.709748
3501.722488	877914.464667	45.714753
3501.638943	877909.050089	45.719757
3502.084940	877873.594947	45.724762
3501.804662	877849.697818	45.729767
3501.763342	877844.663972	45.734772
3501.699717	877796.981316	45.739777
3501.594251	877789.825359	45.744781
3502.141585	877767.439488	45.749786
3501.881585	877744.507973	45.754791
3502.060436	877719.177529	45.759796
3501.820038	877693.334411	45.764801
3502.016780	877667.031400	45.769805
3502.055845	877646.376788	45.774810
3501.745454	877603.095528	45.779815
3501.730119	877511.972878	45.784820
3501.678633	877371.413126	45.789825
3501.607953	877179.567928	45.794829
3501.831938	876932.308580	45.799834
3501.484362	876619.008598	45.804839
3501.545317	876250.258904	45.809844
3501.616881	875811.860057	45.814849
3501.237349	875326.468658	45.819853
3501.297477	874768.515711	45.824858
3501.369718	874151.048914	45.829863
3501.079512	873478.379841	45.834868
3500.800085	872726.658226	45.839873
3500.601453	871925.049985	45.844877
3500.622028	871051.676531	45.849882
3500.324598	870122.416423	45.854887
3499.924763	869111.482236	45.859892
3499.842353	868028.279297	45.864897
3499.196707	866884.762150	45.869901
3498.851625	865667.738399	45.874906
3498.693333	864378.737405	45.879911
3498.484161	863030.288966	45.884916
3498.313184	861586.083741	45.889921
3497.675917	860083.666516	45.894925
3497.244148	858498.572207	45.899930
3496.804178	856836.415155	45.904935
3496.401071	855102.089380	45.909940
3495.963503	853291.946153	45.914945
3495.451198	851410.503532	45.919949
3495.079602	849454.059906	45.924954
3494.558525	847411.196350	45.929959
3493.940449	845301.703724	45.934964
3493.313333	843103.373155	45.939969
3492.707695	840847.708865	45.944973
3492.082725	838500.513742	45.949978
3491.650868	836083.518160	45.954983
3490.663008	833597.698896	45.959988
3490.408676	831036.566475	45.964993
3489.320509	828402.982702	45.969997
3488.412036	825686.629801	45.975002
3488.040533	822906.960910	45.980007
3486.872147	820044.310521	45.985012
3486.158806	817114.767734	45.990017
3485.168510	814114.358480	45.995021
3484.281246	811033.675726	46.000026
3483.908252	807889.410389	46.005031
3482.467653	804678.264094	46.010036
3481.853334	801391.600169	46.015041
3481.012468	798039.704258	46.020045
3479.912125	794593.136283	46.025050
3479.053348	791091.529230	46.030055
3477.857168	787523.212461	46.035060
3476.933140	783878.656103	46.040065
3475.771771	780171.570890	46.045069
3474.960708	776381.498214	46.050074
3473.870640	772522.811884	46.055079
3472.460563	768603.461517	46.060084
3471.224617	764619.245495	46.065089
3470.373407	760558.304375	46.070093
3468.988572	756433.224292	46.075098
3467.881768	752238.653131	46.080103
3466.485949	747965.254676	46.085108
3465.532124	743638.709986	46.090113
3464.119151	739237.784057	46.095117
3462.701326	734760.770087	46.100122
3461.733726	730227.253504	46.105127
3460.126189	725615.842267	46.110132
3459.028853	720938.987282	46.115137
3457.340380	716198.824511	46.120141
3455.568961	711390.280966	46.125146
3454.045409	706520.718832	46.130151
3452.339011	701587.903905	46.135156
3451.474569	696587.319481	46.140161
3449.774303	691532.944796	46.145165
3448.391795	686392.578788	46.150170
3447.015803	681188.330094	46.155175
3445.019095	675927.959089	46.160180
3443.237084	670590.232853	46.165185
3441.531142	665193.596856	46.170189
3439.915531	659727.860821	46.175194
3438.131290	654219.220520	46.180199
3436.294009	648634.848746	46.185204
3434.406364	642987.018883	46.190209
3432.406924	637295.399055	46.195213
3430.771654	631530.956486	46.200218
3429.125915	625712.770106	46.205223
3426.915805	619847.062767	46.210228
3425.088503	613904.425533	46.215233
3422.974730	607912.545657	46.220237
3421.006369	601861.143502	46.225242
3418.850784	595744.264578	46.230247
3416.477129	589583.882289	46.235252
3414.927675	583355.338522	46.240257
3412.441372	577085.995764	46.245261
3410.077363	570754.347127	46.250266
3408.289224	564371.218821	46.255271
3405.846943	557940.887933	46.260276
3403.762849	551443.434151	46.265281
3401.341708	544897.907346	46.270285
3399.219768	538312.633583	46.275290
3396.371344	531659.489720	46.280295
3393.960160	524968.159307	46.285300
3391.644244	518216.651995	46.290305
3388.938350	511427.941573	46.295309
3386.231531	504588.195547	46.300314
3383.837953	497709.570140	46.305319
3380.621903	490795.982745	46.310324
3378.436655	483823.228520	46.315329
3375.661004	476833.064984	46.320333
3373.140515	469788.947626	46.325338
3370.359647	462693.068335	46.330343
3367.450575	455562.016964	46.335348
3364.921808	448379.081068	46.340353
3361.837214	441175.146260	46.345357
3358.578729	433923.836666	46.350362
3355.950558	426643.750275	46.355367
3352.400161	419328.816267	46.360372
3349.410388	411977.562518	46.365377
3346.457086	404601.828985	46.370381
3343.376629	397191.077198	46.375386
3340.205175	389762.250801	46.380391
3336.851195	382290.287601	46.385396
3333.728990	374781.167888	46.390401
3330.165053	367264.202003	46.395405
3326.747629	359716.424422	46.400410
3323.278167	352150.117016	46.405415
3319.691734	344560.552852	46.410420
3316.439932	336966.280491	46.415425
3312.761516	329341.264114	46.420429
3309.230438	321697.036683	46.425434
3305.544885	314035.608921	46.430439
3301.881668	306370.728862	46.435444
3298.063078	298687.282738	46.440449
3294.214476	290997.146626	46.445453
3290.554013	283287.686799	46.450458
3286.907632	275576.205896	46.455463
3282.989803	267855.655440	46.460468
3279.174343	260117.400926	46.465473
3274.948206	252394.824647	46.470477
3270.895856	244659.851745	46.475482
3266.828617	236914.868208	46.480487
3262.289953	229177.278652	46.485492
3258.374621	221366.904921	46.490497
3254.028016	213640.693798	46.495501
3249.782848	205921.164174	46.500506
3245.526453	198205.479742	46.505511
3241.188018	190509.137791	46.510516
3236.834373	182804.300244	46.515521
3231.970254	175127.400765	46.520525
3227.652566	167461.113873	46.525530
3222.795896	159816.878907	46.530535
3217.714059	152200.185387	46.535540
3213.130017	144590.080306	46.540545
3208.230915	137025.254189	46.545549
3203.245124	129476.365616	46.550554
3198.280009	121962.969785	46.555559
3193.079445	114476.182887	46.560564
3188.263843	107018.564635	46.565569
3182.797286	99618.186765	46.570573
3177.022332	92248.851563	46.575578
3171.225563	84915.234927	46.580583
3165.493694	77643.871753	46.585588
3159.479679	70423.889843	46.590593
3153.373189	63284.264718	46.595597
3146.532674	56188.869790	46.600602
3139.325545	49189.334574	46.605607
3129.493467	42343.492981	46.610612
3110.906030	35842.529609	46.615617
3089.767342	29617.374814	46.620621
3068.690600	23672.751150	46.625626
3048.074328	18081.539712	46.630631
3024.434911	12944.273061	46.635636
2996.429821	8367.301313	46.640641
2964.017476	4444.320572	46.645645
2926.652504	1226.089268	46.650650
2831.760948	296.700020	46.655655
2745.992681	300.582015	46.660660
2715.818283	300.972011	46.665665
2729.036099	281.006880	46.670669
2763.792658	271.989029	46.675674
2800.673050	256.538102	46.680679
2828.023541	273.212766	46.685684
2842.852017	275.173027	46.690689
2845.928434	267.798788	46.695693
2842.559372	257.390716	46.700698
2836.716306	250.350179	46.705703
2830.760302	255.466446	46.710708
2825.512092	250.600381	46.715713
2821.814616	258.716620	46.720717
2819.193460	253.997712	46.725722
2816.765592	252.836186	46.730727
2815.023211	249.067941	46.735732
2813.066485	247.762772	46.740737
2810.596363	247.604802	46.745741
2807.400027	260.284606	46.750746
2804.530476	248.075299	46.755751
2801.438083	249.965802	46.760756
2798.390401	250.075609	46.765761
2795.630528	235.473794	46.770765
2792.473747	249.130231	46.775770
2789.410914	237.684185	46.780775
2785.641774	243.465467	46.785780
2782.371134	232.396698	46.790785
2779.686086	232.807820	46.795789
2776.344442	241.039031	46.800794
2773.461277	238.967122	46.805799
2769.914777	239.068472	46.810804
2766.819987	236.998331	46.815809
2763.121710	228.894759	46.820813
2759.451395	233.538056	46.825818
2756.403087	233.824810	46.830823
2753.473796	238.007597	46.835828
2749.946671	230.891319	46.840833
2746.934968	228.674474	46.845837
2743.218820	230.221938	46.850842
2739.724023	227.788401	46.855847
2736.469710	223.997335	46.860852
2733.748948	221.903786	46.865857
2730.114333	216.299148	46.870861
2726.654358	225.871702	46.875866
2723.294214	215.355716	46.880871
2719.596763	221.877474	46.885876
2716.267725	227.035593	46.890881
2712.830400	214.834418	46.895885
2709.675733	217.131116	46.900890
2706.619298	218.930487	46.905895
2703.043355	218.805853	46.910900
2699.645158	219.213132	46.915905
2695.604832	220.245776	46.920909
2692.138395	217.847459	46.925914
2688.783057	218.163605	46.930919
2685.546242	226.725279	46.935924
2682.326344	223.929096	46.940929
2679.028635	212.201029	46.945933
2674.911174	213.348642	46.950938
2671.515100	209.433011	46.955943
2668.560227	218.182606	46.960948
2665.664965	211.200524	46.965953
2662.614758	213.307536	46.970957
2658.104289	213.600008	46.975962
2654.767518	203.557399	46.980967
2650.735351	208.833161	46.985972
2647.987956	210.351862	46.990977
2644.890637	207.164476	46.995981
2640.924695	205.490384	47.000986
2637.496843	199.483859	47.005991
2633.840820	213.775680	47.010996
2630.510575	199.760313	47.016001
2627.368359	213.955901	47.021005
2623.797740	203.476708	47.026010
2620.404656	201.845445	47.031015
2616.395155	203.955287	47.036020
2613.410323	206.779729	47.041025
2610.011662	206.258849	47.046029
2606.571536	206.806118	47.051034
2603.339292	204.475783	47.056039
2599.433903	207.936035	47.061044
2596.031052	204.091832	47.066049
2592.497101	209.223845	47.071053
2589.005755	208.019686	47.076058
2585.880400	198.108799	47.081063
2581.995227	200.417988	47.086068
2578.813140	202.480506	47.091073
2575.489960	200.703545	47.096077
2571.239333	198.964798	47.101082
2568.354726	192.190212	47.106087
2564.470926	203.578478	47.111092
2561.144409	200.917988	47.116097
2557.978231	196.585999	47.121101
2554.301218	205.200650	47.126106
2551.170128	194.880662	47.131111
2547.192628	197.720571	47.136116
2544.086085	192.766596	47.141121
2540.636353	194.605715	47.146125
2536.924400	197.517446	47.151130
2533.670343	204.834840	47.156135
2529.700022	192.247786	47.161140
2526.023599	202.745389	47.166145
2522.962636	196.671688	47.171149
2519.586014	203.699098	47.176154
2516.374613	191.562642	47.181159
2512.627441	200.672779	47.186164
2509.027575	194.763023	47.191169
2505.853026	192.200237	47.196173
2501.989033	199.741063	47.201178
2498.553018	190.627866	47.206183
2494.912082	196.799036	47.211188
2491.828571	186.685163	47.216193
2488.000011	189.092825	47.221197
2485.248060	188.121916	47.226202
2481.833586	192.358871	47.231207
2477.712527	193.282663	47.236212
2474.076951	195.990806	47.241217
2470.827332	193.196915	47.246221
2467.117623	194.944012	47.251226
2464.000139	185.638946	47.256231
2460.338635	192.067314	47.261236
2456.581312	186.487104	47.266241
2453.343895	184.696863	47.271245
2449.698053	188.036630	47.276250
2446.498037	182.564741	47.281255
2443.054465	187.405453	47.286260
2439.458611	183.177823	47.291265
2436.036597	176.849224	47.296269
2432.332707	183.529701	47.301274
2428.712579	185.049700	47.306279
2425.252231	189.561266	47.311284
2421.412203	183.773517	47.316289
2418.128036	178.257720	47.321293
2415.087088	188.158910	47.326298
2412.062943	184.173594	47.331303
2408.098322	179.380896	47.336308
2404.768526	184.725410	47.341313
2401.102145	183.684077	47.346317
2397.261037	181.414133	47.351322
2393.889667	181.456057	47.356327
2390.225415	185.606818	47.361332
2387.144775	180.542904	47.366337
2383.801064	181.459226	47.371341
2379.870607	182.886822	47.376346
2376.622121	184.885829	47.381351
2372.870629	175.834685	47.386356
2369.492516	175.827417	47.391361
2366.265227	181.279751	47.396365
2362.517730	191.667423	47.401370
2358.678733	177.434549	47.406375
2355.395400	174.337665	47.411380
2352.022393	181.397921	47.416385
2348.789645	175.177073	47.421389
2345.135225	180.817547	47.426394
2341.459980	179.506576	47.431399
2338.224621	186.664498	47.436404
2334.508852	184.225906	47.441409
2331.509308	171.642391	47.446413
2328.111320	177.134373	47.451418
2324.214745	174.397067	47.456423
2320.677339	179.916017	47.461428
2316.651714	172.459897	47.466433
2313.303924	172.392998	47.471437
2309.860576	174.270290	47.476442
2306.866963	175.637018	47.481447
2303.383814	174.062094	47.486452
2299.820797	184.342186	47.491457
2296.450005	179.765122	47.496461
2292.501597	175.632123	47.501466
2289.247535	173.802709	47.506471
2285.281302	173.439696	47.511476
2282.015894	172.888758	47.516481
2278.662878	174.474881	47.521485
2275.056394	186.183018	47.526490
2271.836042	178.566163	47.531495
2268.382248	182.050575	47.536500
2265.298845	174.010318	47.541505
2261.624713	170.633464	47.546509
2257.737432	181.639258	47.551514
2253.820140	175.209438	47.556519
2250.265868	177.710525	47.561524
2246.887706	175.377690	47.566529
2243.804687	167.210498	47.571533
2240.302775	170.439028	47.576538
2236.518747	171.538459	47.581543
2233.056646	180.508163	47.586548
2229.770728	169.494886	47.591553
2226.544644	168.105702	47.596557
2223.246848	169.640908	47.601562
2219.413704	165.231809	47.606567
2215.813952	175.628524	47.611572
2212.141862	174.716747	47.616577
2208.761190	169.950159	47.621581
2205.334759	179.645729	47.626586
2202.118077	158.704294	47.631591
2198.223495	167.357449	47.636596
2194.341509	170.555620	47.641601
2191.225023	160.302977	47.646605
2187.612528	169.192550	47.651610
2184.407904	162.717745	47.656615
2180.901429	166.175983	47.661620
2177.352982	170.726525	47.666625
2174.077279	163.276762	47.671629
2169.922321	174.801413	47.676634
2166.470037	164.212708	47.681639
2163.457382	162.204002	47.686644
2159.591166	165.450114	47.691649
2156.386654	158.081953	47.696653
2152.699966	165.413760	47.701658
2149.520704	156.276819	47.706663
2145.681181	151.700705	47.711668
2142.300501	161.793690	47.716673
2138.713609	162.233102	47.721677
2135.158153	163.822753	47.726682
2131.843309	154.826224	47.731687
2128.186110	153.426203	47.736692
2124.856598	157.139031	47.741697
2121.324606	150.018567	47.746701
2117.629681	156.087199	47.751706
2114.593717	157.645152	47.756711
2110.808169	151.532545	47.761716
2106.863301	159.065280	47.766721
2103.407410	147.633212	47.771725
2100.031640	154.884501	47.776730
2096.715225	151.764456	47.781735
2093.259897	151.690405	47.786740
2089.638088	170.170926	47.791745
2086.624749	159.523619	47.796749
2082.866276	158.076616	47.801754
2079.160408	157.349508	47.806759
2075.736282	150.424987	47.811764
2072.426087	147.754461	47.816769
2069.010647	154.532390	47.821773
2065.212300	157.501350	47.826778
2061.600909	152.455854	47.831783
2058.150478	156.782292	47.836788
2054.757489	154.230632	47.841793
2051.623387	145.808775	47.846797
2047.551904	158.450279	47.851802
2043.966662	146.875633	47.856807
2040.382796	163.064120	47.861812
2037.298817	149.256480	47.866817
2033.890854	154.373963	47.871821
2030.048333	157.195925	47.876826
2026.728022	153.511787	47.881831
2023.626973	148.458411	47.886836
2019.864643	155.133617	47.891841
2016.165078	146.098696	47.896845
2012.852503	156.908296	47.901850
2009.427087	155.232293	47.906855
2005.688982	152.021519	47.911860
2002.241981	149.193268	47.916865
1998.886457	145.947142	47.921869
1995.058236	149.695252	47.926874
1991.754320	151.532565	47.931879
1988.066876	157.968683	47.936884
1985.051762	152.398319	47.941889
1981.495265	143.807298	47.946893
1977.485012	151.847431	47.951898
1974.306130	146.568361	47.956903
1970.900328	151.015362	47.961908
1967.404935	156.490305	47.966913
1963.611741	152.303938	47.971917
1960.145363	151.567957	47.976922
1957.062952	146.668238	47.981927
1953.267275	156.178850	47.986932
1949.455899	149.851008	47.991937
1946.342141	143.361379	47.996941
1942.843602	143.644259	48.001946
1939.212337	138.347186	48.006951
1935.404819	140.527017	48.011956
1932.154335	144.984699	48.016961
1929.117751	139.225124	48.021965
1924.807476	147.976724	48.026970
1921.596002	145.967666	48.031975
1918.397513	140.904807	48.036980
1914.743175	151.994692	48.041985
1911.313339	144.913375	48.046989
1907.582287	148.644514	48.051994
1904.201357	146.111301	48.056999
1900.374776	153.236284	48.062004
1897.132077	152.263498	48.067009
1893.802045	142.422099	48.072013
1890.227075	150.923215	48.077018
1886.627092	150.796836	48.082023
1883.496820	152.679937	48.087028
1879.761899	150.691654	48.092033
1876.227491	146.474260	48.097037
1872.493443	152.985645	48.102042
1869.416277	141.565224	48.107047
1865.855931	144.632961	48.112052
1861.890695	146.897512	48.117057
1858.694274	141.101831	48.122061
1855.407406	150.236990	48.127066
1852.074127	150.242017	48.132071
1848.499510	145.615493	48.137076
1844.359669	150.701845	48.142081
1841.126649	137.771300	48.147085
1837.445624	146.278127	48.152090
1834.232764	144.723436	48.157095
1830.981756	150.943511	48.162100
1827.009541	143.942976	48.167105
1823.623393	137.546979	48.172109
1819.893759	144.008532	48.177114
1816.643429	139.646972	48.182119
1813.290350	148.918996	48.187124
1809.366086	137.972061	48.192129
1806.139066	138.499290	48.197133
1803.169372	145.487920	48.202138
1799.231525	139.367788	48.207143
1795.699013	147.693424	48.212148
1792.179602	151.102954	48.217153
1788.611705	144.655505	48.222157
1784.968651	153.455660	48.227162
1781.690575	143.891120	48.232167
1778.251625	139.718422	48.237172
1774.547412	140.507437	48.242177
1771.535953	138.094445	48.247181
1767.634709	132.885332	48.252186
1764.162918	135.720650	48.257191
1760.512199	140.498535	48.262196
1756.986471	141.158224	48.267201
1753.919641	138.432135	48.272205
1750.359399	146.552018	48.277210
1747.004613	137.813023	48.282215
1743.220667	136.352743	48.287220
1739.568334	143.870766	48.292225
1736.085142	139.109051	48.297229
1732.055132	148.712202	48.302234
1728.842170	148.941942	48.307239
1725.585454	140.641035	48.312244
1722.100094	137.994375	48.317249
1718.804214	137.361635	48.322253
1715.116855	134.828868	48.327258
1711.908545	139.031074	48.332263
1708.262178	135.971354	48.337268
1704.213324	139.237135	48.342273
1701.121457	139.165284	48.347277
1697.653137	144.240071	48.352282
1694.369030	136.922715	48.357287
1690.811081	138.787006	48.362292
1686.969746	138.039964	48.367297
1683.771585	137.395051	48.372301
1679.808351	137.159727	48.377306
1676.243164	134.270343	48.382311
1672.838690	144.931130	48.387316
1669.321054	151.680418	48.392321
1666.021636	138.152788	48.397325
1662.714543	131.424367	48.402330
1659.325384	134.847792	48.407335
1655.363459	137.246943	48.412340
1651.858454	139.584022	48.417345
1648.814618	134.777017	48.422349
1645.109797	143.729157	48.427354
1641.791661	143.180663	48.432359
1638.621324	140.144567	48.437364
1634.439223	145.075663	48.442369
1631.054170	141.945989	48.447373
1627.166195	140.637380	48.452378
1624.127937	136.190009	48.457383
1620.921484	136.574645	48.462388
1616.952989	140.599209	48.467393
1613.489763	134.816617	48.472397
1609.669352	131.849476	48.477402
1606.538565	135.810816	48.482407
1602.898684	135.029767	48.487412
1598.875112	132.559754	48.492417
1595.988318	128.909095	48.497421
1592.820223	144.407111	48.502426
1589.091426	123.370530	48.507431
1586.063365	127.131184	48.512436
1581.955025	136.084130	48.517441
1578.744627	123.098571	48.522445
1574.833325	136.177084	48.527450
1571.211735	129.585165	48.532455
1567.899283	122.467767	48.537460
1564.385565	130.765182	48.542465
1561.072212	126.492770	48.547469
1557.384050	134.512157	48.552474
1553.792015	120.804671	48.557479
1550.337397	121.500717	48.562484
1546.788961	134.112571	48.567489
1543.831920	130.069997	48.572493
1539.837248	128.956503	48.577498
1536.679755	126.364345	48.582503
1533.130409	137.052310	48.587508
1529.764758	132.614707	48.592513
1526.185983	128.218642	48.597517
1522.325601	124.568879	48.602522
1518.679917	126.034173	48.607527
1515.442875	132.152672	48.612532
1511.633764	133.243593	48.617537
1508.625824	130.315340	48.622541
1505.024935	130.242685	48.627546
1501.255675	127.651205	48.632551
1497.984599	135.769051	48.637556
1494.587206	135.856561	48.642561
1491.338376	132.568321	48.647565
1487.373818	132.542361	48.652570
1484.093698	127.711375	48.657575
1480.363569	125.308416	48.662580
1476.381489	136.041292	48.667585
1473.398078	125.880898	48.672589
1469.934943	132.942179	48.677594
1466.358376	134.123764	48.682599
1463.061401	125.560754	48.687604
1459.440669	138.600209	48.692609
1456.079393	131.304676	48.697613
1452.768717	126.827659	48.702618
1448.918828	133.219760	48.707623
1445.614779	125.304808	48.712628
1441.688565	129.399092	48.717633
1437.906958	127.702662	48.722637
1434.448179	134.711347	48.727642
1431.301069	132.548929	48.732647
1428.041011	125.043104	48.737652
1424.470482	134.684603	48.742657
1420.966013	121.584580	48.747661
1417.238506	132.085781	48.752666
1413.793405	129.280758	48.757671
1410.614557	124.730479	48.762676
1407.017676	121.102981	48.767681
1403.509931	117.749658	48.772685
1399.514327	134.024106	48.777690
1396.232713	134.160042	48.782695
1392.785178	123.410010	48.787700
1389.190871	124.313774	48.792705
1385.738225	118.130015	48.797709
1382.494052	122.554639	48.802714
1378.820608	127.073898	48.807719
1375.875429	127.748230	48.812724
1372.015491	129.185114	48.817729
1368.605308	116.816878	48.822733
1364.944486	128.649383	48.827738
1361.272292	126.502566	48.832743
1357.858150	121.166346	48.837748
1353.880211	128.711812	48.842753
1350.411117	127.141602	48.847757
1347.681821	125.724992	48.852762
1343.709196	126.445243	48.857767
1340.278603	127.459924	48.862772
1336.920515	130.140588	48.867777
1333.500187	122.963456	48.872781
1329.617708	121.531253	48.877786
1326.376518	133.031966	48.882791
1323.170276	122.501609	48.887796
1319.239300	130.086109	48.892801
1315.826664	120.378834	48.897805
1312.203661	126.362342	48.902810
1308.688257	127.921312	48.907815
1305.254432	125.750728	48.912820
1301.891292	125.888960	48.917825
1298.333953	123.358134	48.922829
1294.923243	122.284094	48.927834
1291.296097	127.940721	48.932839
1287.992449	121.959546	48.937844
1283.882847	129.888158	48.942849
1280.782550	129.080135	48.947853
1277.017609	124.399704	48.952858
1273.483587	128.815877	48.957863
1270.272727	120.118414	48.962868
1266.818933	131.214242	48.967873
1263.428638	123.937283	48.972877
1259.647216	116.858979	48.977882
1256.006892	124.974073	48.982887
1252.653153	109.533536	48.987892
1249.282292	123.108034	48.992897
1245.878238	114.892462	48.997901
1242.489663	127.739747	49.002906
1238.509035	114.827936	49.007911
1235.373717	115.166938	49.012916
1231.532399	126.441699	49.017921
1228.125394	117.418332	49.022925
1224.791810	123.564419	49.027930
1221.089583	119.138893	49.032935
1217.727656	115.651696	49.037940
1214.046135	124.565151	49.042945
1210.844760	114.138282	49.047949
1206.975103	125.383605	49.052954
1203.531938	125.038835	49.057959
1200.372040	113.272496	49.062964
1196.422982	120.960522	49.067969
1193.229757	114.995309	49.072973
1189.793192	113.981076	49.077978
1186.344095	124.332014	49.082983
1182.945006	113.793009	49.087988
1179.082087	121.293546	49.092993
1175.309322	103.645874	49.097997
1172.073027	111.471430	49.103002
1169.150723	111.830121	49.108007
1165.265898	117.264809	49.113012
1161.867426	120.957313	49.118017
1158.262337	119.959718	49.123021
1154.276405	116.971202	49.128026
1150.994841	122.548693	49.133031
1147.483575	117.007289	49.138036
1144.079381	120.715552	49.143041
1140.565650	113.084561	49.148045
1137.150946	113.456997	49.153050
1133.642672	120.281069	49.158055
1130.493192	116.082143	49.163060
1126.337963	119.662199	49.168065
1123.141596	110.470303	49.173069
1119.739815	121.440006	49.178074
1116.199128	118.794684	49.183079
1113.090402	105.338450	49.188084
1108.811147	120.723621	49.193089
1105.676999	107.468735	49.198093
1102.295113	111.312263	49.203098
1098.036461	119.107204	49.208103
1095.130422	113.468340	49.213108
1091.371331	119.289998	49.218113
1087.820619	117.576408	49.223117
1084.673234	112.881460	49.228122
1081.126540	115.654664	49.233127
1077.614696	119.673426	49.238132
1073.860107	114.732164	49.243137
1070.651020	113.627326	49.248141
1067.270619	115.505351	49.253146
1063.650057	115.938324	49.258151
1060.124667	116.569082	49.263156
1056.423564	113.619598	49.268161
1052.863832	114.336160	49.273165
1049.433620	119.699519	49.278170
1045.497537	123.566253	49.283175
1042.608681	113.290116	49.288180
1039.031367	123.061261	49.293185
1035.744311	114.461050	49.298189
1032.276921	114.369852	49.303194
1028.684325	113.455546	49.308199
1025.089011	108.330122	49.313204
1021.618916	120.851202	49.318209
1017.791919	111.454643	49.323213
1014.590399	110.867986	49.328218
1011.083496	121.127361	49.333223
1007.655367	109.048754	49.338228
1004.100180	122.523440	49.343233
1000.439930	122.287344	49.348237
996.855124	115.289250	49.353242
993.521912	114.172433	49.358247
990.252532	113.979849	49.363252
986.462961	110.694190	49.368257
982.503010	107.770210	49.373261
979.477849	110.337659	49.378266
975.964941	118.134295	49.383271
972.700974	115.374656	49.388276
969.325051	114.264329	49.393281
965.552968	116.573460	49.398285
961.904230	110.307831	49.403290
958.244552	113.822066	49.408295
954.938271	100.155915	49.413300
951.509165	112.660783	49.418305
947.796611	117.733065	49.423309
944.338759	105.077684	49.428314
940.503612	111.532857	49.433319
937.725752	108.385205	49.438324
933.746779	116.580608	49.443329
930.310935	112.605809	49.448333
927.096230	108.453937	49.453338
923.207894	118.314683	49.458343
920.163836	111.857719	49.463348
916.500420	115.118238	49.468353
912.905286	107.238451	49.473357
909.782507	106.761591	49.478362
906.024864	114.016804	49.483367
902.420378	102.400225	49.488372
898.813802	115.664823	49.493377
895.385632	111.054345	49.498381
891.909086	120.093973	49.503386
888.496346	109.493153	49.508391
885.095750	101.149446	49.513396
881.222090	108.325393	49.518401
877.661129	96.011753	49.523405
874.290440	114.298843	49.528410
870.793887	104.177422	49.533415
867.372602	109.715258	49.538420
863.690622	111.772173	49.543425
860.361274	109.896651	49.548429
856.964382	108.810796	49.553434
853.276224	113.654349	49.558439
850.053271	102.614480	49.563444
846.163215	105.290533	49.568449
842.922939	108.172487	49.573453
839.321743	111.435799	49.578458
835.203994	113.136200	49.583463
832.087696	103.644374	49.588468
828.940959	106.480278	49.593473
825.657419	105.715119	49.598477
822.170575	100.815050	49.603482
818.161361	106.765313	49.608487
815.050279	105.563543	49.613492
811.100460	105.407470	49.618497
808.097888	111.597158	49.623501
804.552477	103.015804	49.628506
800.901708	97.341485	49.633511
797.281250	103.967078	49.638516
793.584239	119.627575	49.643521
789.984344	113.784804	49.648525
786.837807	109.273662	49.653530
783.309283	111.713548	49.658535
779.866259	106.702465	49.663540
776.187362	108.472606	49.668545
772.722564	110.502945	49.673549
769.132364	104.423761	49.678554
765.627011	102.468300	49.683559
762.844488	103.513952	49.688564
758.751273	109.597747	49.693569
755.231885	101.941392	49.698573
751.931107	109.645864	49.703578
748.412602	104.711428	49.708583
744.762059	96.776829	49.713588
741.150179	108.208557	49.718593
737.637365	100.274465	49.723597
734.110672	106.897817	49.728602
730.625381	107.060827	49.733607
727.386827	103.506052	49.738612
723.470198	103.551770	49.743617
720.270410	100.829465	49.748621
716.667288	102.162254	49.753626
713.025705	109.094515	49.758631
709.914558	101.034206	49.763636
706.262225	106.819357	49.768641
702.829211	112.042921	49.773645
699.618494	104.793962	49.778650
695.815614	93.065560	49.783655
692.388788	102.861965	49.788660
688.648401	100.320289	49.793665
685.043800	98.946484	49.798669
681.739070	99.084990	49.803674
678.141045	99.352534	49.808679
674.893719	105.912937	49.813684
671.260514	100.186886	49.818689
667.601790	108.217037	49.823693
663.963682	107.584857	49.828698
660.549963	113.062981	49.833703
657.344590	97.453611	49.838708
653.077971	105.526918	49.843713
650.292405	102.347975	49.848717
647.164282	107.111663	49.853722
643.342297	106.017962	49.858727
639.418389	103.109650	49.863732
635.895835	104.059168	49.868737
632.247030	104.438555	49.873741
629.362234	102.648912	49.878746
625.527260	116.376349	49.883751
622.469090	97.447137	49.888756
618.708242	94.185080	49.893761
615.220899	103.836839	49.898765
611.717069	109.708989	49.903770
607.673140	109.980510	49.908775
604.514110	98.592041	49.913780
600.937935	109.219538	49.918785
598.002763	101.968091	49.923789
594.252467	104.203278	49.928794
590.374613	106.948178	49.933799
587.158348	100.829190	49.938804
583.386769	99.109936	49.943809
579.884529	103.866698	49.948813
576.870925	101.040090	49.953818
573.227488	100.774533	49.958823
569.673568	103.183463	49.963828
565.996308	101.330611	49.968833
562.650321	102.797988	49.973837
559.229944	98.450144	49.978842
555.532855	101.487017	49.983847
552.423741	98.944608	49.988852
548.481295	109.923030	49.993857
545.152998	104.975647	49.998861
541.721414	92.484629	50.003866
537.924121	106.699620	50.008871
534.281229	90.497940	50.013876
530.799341	113.039833	50.018881
527.526744	101.306332	50.023885
524.267432	98.546666	50.028890
520.639639	102.214825	50.033895
517.156746	96.562314	50.038900
513.402309	99.063670	50.043905
509.884362	106.198615	50.048909
506.538143	101.485114	50.053914
502.862634	114.071104	50.058919
499.640483	95.774372	50.063924
495.883565	99.405111	50.068929
492.327355	97.910190	50.073933
489.642213	93.905465	50.078938
485.924244	101.504704	50.083943
481.960864	96.015801	50.088948
478.423490	96.379047	50.093953
474.919065	99.002653	50.098957
471.366662	102.327246	50.103962
467.743977	109.868703	50.108967
464.503677	96.031248	50.113972
461.122798	99.183606	50.118977
457.659905	94.683634	50.123981
454.468553	94.924713	50.128986
450.360322	97.410077	50.133991
446.918544	95.849291	50.138996
443.235980	98.773148	50.144001
439.543109	93.723979	50.149005
436.414350	100.395950	50.154010
432.819290	104.674845	50.159015
429.782504	96.801568	50.164020
426.238680	88.373039	50.169025
422.602745	104.288095	50.174029
418.686797	97.851690	50.179034
415.023568	105.227817	50.184039
411.852201	103.931334	50.189044
408.344663	99.222906	50.194049
405.025552	95.978312	50.199053
401.545969	96.852628	50.204058
397.697452	104.765797	50.209063
394.585224	100.031028	50.214068
391.283582	104.671063	50.219073
387.140175	102.036512	50.224077
384.042983	104.595159	50.229082
380.319631	103.773282	50.234087
376.917466	91.712082	50.239092
373.525933	97.431433	50.244097
369.824527	94.928187	50.249101
366.458185	97.437460	50.254106
362.614153	96.860535	50.259111
359.212215	94.113358	50.264116
355.786672	94.727952	50.269121
352.380063	98.783316	50.274125
349.186038	92.897053	50.279130
345.147109	101.771427	50.284135
341.896832	92.623249	50.289140
338.383497	103.982707	50.294145
334.651432	99.288614	50.299149
331.719561	81.406171	50.304154
327.786852	91.654582	50.309159
324.448759	85.586565	50.314164
320.757561	100.274525	50.319169
317.306322	100.325274	50.324173
313.821873	84.685264	50.329178
310.040765	89.958438	50.334183
306.647831	86.830733	50.339188
303.242861	96.118999	50.344193
299.847052	90.349651	50.349197
296.282383	93.874732	50.354202
293.068184	104.613816	50.359207
289.849915	87.517041	50.364212
286.147317	91.792537	50.369217
282.215362	98.475409	50.374221
278.874041	84.400686	50.379226
275.277741	91.379849	50.384231
271.526677	83.624741	50.389236
268.418927	83.732337	50.394241
264.678630	90.456706	50.399245
261.454495	96.501659	50.404250
257.447351	91.865410	50.409255
254.397885	91.741957	50.414260
250.666057	89.938473	50.419265
247.098957	97.896937	50.424269
243.773039	93.846697	50.429274
240.334312	100.327977	50.434279
236.970499	90.530507	50.439284
232.943020	95.173196	50.444289
229.328270	99.726649	50.449293
226.141399	98.157590	50.454298
222.626920	96.595801	50.459303
219.252101	91.524968	50.464308
216.043542	88.063512	50.469313
212.069082	100.791543	50.474317
208.981582	92.009427	50.479322
205.342698	100.461502	50.484327
202.105045	96.844437	50.489332
198.133356	98.985184	50.494337
194.401763	94.367315	50.499341
191.414742	95.232086	50.504346
187.885034	99.111801	50.509351
184.235560	93.258448	50.514356
180.619444	90.404794	50.519361
176.800828	99.057933	50.524365
174.040270	85.154550	50.529370
169.750987	101.173201	50.534375
166.810472	88.207751	50.539380
163.539303	91.379070	50.544385
159.862403	103.398980	50.549389
156.126131	86.668307	50.554394
152.572650	100.486427	50.559399
149.442203	96.837842	50.564404
145.682532	100.876038	50.569409
141.957714	97.967399	50.574413
138.929232	89.321994	50.579418
135.008641	90.466873	50.584423
131.301192	92.297134	50.589428
128.257584	89.108386	50.594433
124.757097	94.507330	50.599437
121.512212	89.296470	50.604442
117.535456	99.238980	50.609447
113.905307	95.648885	50.614452
110.648457	97.049751	50.619457
107.292739	89.419771	50.624461
103.907053	84.287295	50.629466
99.860954	95.837344	50.634471
96.614901	88.799771	50.639476
93.113672	84.957075	50.644481
89.169659	102.086455	50.649485
86.119749	90.245049	50.654490
82.850202	87.390932	50.659495
79.252245	86.023451	50.664500
75.744958	89.661752	50.669505
71.884829	102.109892	50.674509
68.612183	96.373035	50.679514
65.110067	91.871607	50.684519
61.777331	89.785735	50.689524
58.187062	83.839226	50.694529
54.293048	83.338347	50.699533
51.215532	77.834421	50.704538
47.182130	102.730338	50.709543
43.899605	88.711019	50.714548
40.725801	84.265759	50.719553
36.923793	87.845937	50.724557
33.915247	88.273140	50.729562
30.007777	87.588227	50.734567
26.651812	85.307121	50.739572
23.085695	92.475657	50.744577
19.806158	93.814241	50.749581
16.034552	87.197259	50.754586
12.309437	91.761858	50.759591
9.000858	92.996725	50.764596
5.551132	94.071841	50.769601
1.952323	89.767437	50.774605