Tue Jun 21 12:48:45 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
1.056135	84.058723	0.000000
1.278532	85.896216	0.005005
1.672296	78.979989	0.010010
1.162104	93.273981	0.015014
1.040216	74.704301	0.020019
0.679465	59.130856	0.025024
0.716853	68.981945	0.030029
0.657213	42.390816	0.035034
0.306954	36.492328	0.040038
0.087611	21.121058	0.045043
-0.080413	13.648462	0.050048
-0.496980	1.790837	0.055053
-0.412599	-10.661419	0.060058
-1.073080	-16.659476	0.065062
-1.812495	-38.885761	0.070067
-2.031996	-27.486741	0.075072
-2.061672	-30.760874	0.080077
-2.722461	-38.199403	0.085082
-3.690756	-27.471442	0.090086
-3.513207	-27.363265	0.095091
-3.716832	-26.271211	0.100096
-4.194738	-23.479889	0.105101
-3.828394	-25.622973	0.110106
-3.929621	-30.429191	0.115110
-3.722699	-26.246016	0.120115
-4.120455	-23.127961	0.125120
-5.110943	-26.701592	0.130125
-5.157085	-34.748852	0.135130
-5.650411	-18.494687	0.140134
-5.384003	-30.619895	0.145139
-6.311227	-28.086478	0.150144
-7.009060	-14.527363	0.155149
-6.281978	-18.669181	0.160154
-7.343912	-19.756028	0.165158
-7.277365	-23.727882	0.170163
-6.969103	-26.085913	0.175168
-7.317965	-17.779974	0.180173
-6.925437	-26.688424	0.185178
-8.170634	-17.914377	0.190182
-8.479944	-29.581748	0.195187
-8.764859	-24.840963	0.200192
-9.085483	-19.364129	0.205197
-9.050102	-31.403917	0.210202
-9.301917	-22.483967	0.215206
-8.920895	-25.789998	0.220211
-9.041432	-20.508506	0.225216
-9.774729	-19.672890	0.230221
-9.837878	-31.671892	0.235226
-10.512294	-19.694928	0.240230
-10.498946	-23.279488	0.245235
-11.046950	-32.496116	0.250240
-11.863945	-28.830500	0.255245
-11.872550	-21.202901	0.260250
-12.100674	-22.285151	0.265254
-11.878784	-23.859872	0.270259
-12.005668	-31.008921	0.275264
-12.189183	-22.340633	0.280269
-12.059523	-26.066799	0.285274
-12.969420	-15.536756	0.290278
-13.133528	-24.128465	0.295283
-13.549999	-25.856969	0.300288
-13.755420	-21.386866	0.305293
-13.777444	-26.344926	0.310298
-14.229891	-26.611549	0.315302
-14.878308	-26.517357	0.320307
-15.095035	-25.687362	0.325312
-15.280602	-26.689043	0.330317
-15.145113	-35.414816	0.335322
-15.355716	-23.090395	0.340326
-15.217886	-28.013949	0.345331
-16.139047	-17.328122	0.350336
-16.997239	-19.274940	0.355341
-16.804513	-25.245756	0.360346
-17.091318	-15.062798	0.365350
-17.337332	-31.211430	0.370355
-17.314102	-28.996821	0.375360
-17.144441	-23.349777	0.380365
-16.770182	-25.066157	0.385370
-17.716089	-28.006228	0.390374
-18.475195	-17.409002	0.395379
-18.322301	-28.223078	0.400384
-18.708276	-24.687049	0.405389
-18.578904	-24.149588	0.410394
-19.441193	-10.281443	0.415398
-19.830605	-11.761448	0.420403
-19.806845	-18.978862	0.425408
-20.401214	-16.379003	0.430413
-20.214006	-22.303125	0.435418
-20.056193	-11.810966	0.440422
-20.327157	-16.993415	0.445427
-21.199491	-16.655140	0.450432
-21.813618	-23.416652	0.455437
-21.943170	-21.398150	0.460442
-21.681073	-15.845541	0.465446
-21.866668	-19.668687	0.470451
-21.759681	-26.122781	0.475456
-21.766535	-28.498486	0.480461
-22.582086	-27.901241	0.485466
-23.237360	-23.122014	0.490470
-23.245838	-30.387956	0.495475
-23.292474	-23.937073	0.500480
-23.888921	-27.756116	0.505485
-24.487959	-25.091747	0.510490
-25.252498	-15.485020	0.515494
-24.648777	-23.289635	0.520499
-23.994143	-24.188521	0.525504
-24.917917	-15.864731	0.530509
-24.721951	-27.716019	0.535514
-25.258835	-20.476709	0.540518
-25.999688	-25.022099	0.545523
-25.927213	-20.730623	0.550528
-26.512766	-20.911069	0.555533
-26.570566	-24.385574	0.560538
-26.642461	-13.855181	0.565542
-26.637330	-15.217790	0.570547
-27.141206	-19.953977	0.575552
-28.006931	-16.472883	0.580557
-27.614229	-21.243089	0.585562
-28.097648	-19.263074	0.590566
-27.874884	-21.553471	0.595571
-28.126206	-20.049182	0.600576
-29.487258	-8.376849	0.605581
-29.551871	-25.494238	0.610586
-29.690567	-15.044741	0.615590
-29.670219	-19.650475	0.620595
-29.719032	-25.876897	0.625600
-30.024807	-11.843787	0.630605
-29.696850	-32.282769	0.635610
-29.867535	-16.503733	0.640614
-30.565206	-19.341252	0.645619
-31.293751	-22.049733	0.650624
-31.135087	-25.646121	0.655629
-31.145928	-29.969829	0.660634
-32.192497	-20.548859	0.665638
-32.571489	-18.918051	0.670643
-32.635809	-20.499249	0.675648
-32.917761	-17.629472	0.680653
-32.838179	-22.833265	0.685658
-33.037040	-11.970454	0.690662
-32.927825	-19.892684	0.695667
-32.817651	-18.403464	0.700672
-33.234314	-17.529505	0.705677
-33.847355	-24.593113	0.710682
-34.460722	-14.222087	0.715686
-34.756610	-30.495261	0.720691
-34.448304	-18.615522	0.725696
-34.894612	-21.709167	0.730701
-35.484763	-23.821728	0.735706
-35.670475	-21.374395	0.740710
-36.018607	-24.310053	0.745715
-36.128246	-25.606689	0.750720
-36.104655	-20.428197	0.755725
-36.041073	-19.604167	0.760730
-36.952551	-20.863527	0.765734
-37.554782	-16.485972	0.770739
-37.389314	-21.133300	0.775744
-37.794391	-14.791184	0.780749
-37.662538	-21.229269	0.785754
-37.846935	-18.533909	0.790758
-38.300817	-27.392767	0.795763
-38.099197	-32.176516	0.800768
-38.955192	-17.470951	0.805773
-38.869191	-25.694608	0.810778
-39.080257	-19.974648	0.815782
-39.542632	-21.071976	0.820787
-40.280197	-19.960762	0.825792
-40.437909	-18.710550	0.830797
-40.640311	-22.280495	0.835802
-40.973655	-14.056254	0.840806
-40.934008	-24.260170	0.845811
-40.844562	-27.797932	0.850816
-41.125836	-19.545614	0.855821
-40.679791	-25.622118	0.860826
-41.448573	-19.701069	0.865830
-42.199585	-19.929888	0.870835
-42.331997	-21.863099	0.875840
-42.446019	-15.232730	0.880845
-42.401194	-24.655669	0.885850
-43.237690	-16.456047	0.890854
-43.929385	-21.236114	0.895859
-43.809170	-15.480438	0.900864
-44.223036	-15.608013	0.905869
-43.939182	-29.013841	0.910874
-44.516163	-25.471438	0.915878
-44.713132	-21.289854	0.920883
-44.329985	-26.340466	0.925888
-44.478938	-18.864464	0.930893
-44.893287	-23.370780	0.935898
-45.600260	-24.162581	0.940902
-45.534389	-23.616184	0.945907
-45.829903	-24.129607	0.950912
-46.845775	-18.267883	0.955917
-47.055845	-22.029944	0.960922
-47.206310	-16.094270	0.965926
-47.365688	-21.256319	0.970931
-46.958002	-27.069938	0.975936
-47.638620	-11.226382	0.980941
-47.362289	-21.868503	0.985946
-47.671556	-21.988140	0.990950
-48.220827	-23.668600	0.995955
-48.590999	-34.068278	1.000960
-49.103705	-24.047223	1.005965
-48.939791	-23.481542	1.010970
-48.927304	-14.582862	1.015974
-50.024261	-18.751768	1.020979
-49.921684	-19.827607	1.025984
-50.492673	-22.457392	1.030989
-50.418629	-26.949472	1.035994
-50.657813	-18.224604	1.040998
-50.525595	-19.799474	1.046003
-50.354801	-23.269802	1.051008
-51.567209	-17.683369	1.056013
-51.643611	-18.841259	1.061018
-51.867702	-20.200440	1.066022
-51.945553	-15.008700	1.071027
-51.892287	-21.248475	1.076032
-52.047431	-23.233766	1.081037
-52.662083	-25.196635	1.086042
-53.230156	-19.131223	1.091046
-53.559725	-9.241916	1.096051
-53.634018	-17.746870	1.101056
-53.608243	-15.881173	1.106061
-54.345289	-15.463471	1.111066
-55.291874	-12.584660	1.116070
-54.630446	-29.068464	1.121075
-54.999416	-17.625153	1.126080
-55.444837	-16.547912	1.131085
-55.060239	-24.471936	1.136090
-55.159259	-21.390523	1.141094
-55.569672	-15.525661	1.146099
-55.755100	-30.089472	1.151104
-56.383776	-18.449232	1.156109
-56.620325	-26.803977	1.161114
-56.978740	-14.413240	1.166118
-57.069287	-14.902591	1.171123
-57.137156	-20.039143	1.176128
-57.751281	-18.297367	1.181133
-57.734443	-22.062471	1.186138
-58.435511	-21.496413	1.191142
-58.512337	-14.976988	1.196147
-58.326672	-28.530736	1.201152
-58.656830	-16.775751	1.206157
-58.706613	-30.784430	1.211162
-59.541268	-20.460232	1.216166
-60.114425	-24.868022	1.221171
-60.020492	-23.718091	1.226176
-60.382241	-26.712861	1.231181
-60.163966	-15.876709	1.236186
-60.184750	-16.952642	1.241190
-60.698973	-22.790595	1.246195
-61.239346	-16.801796	1.251200
-61.647464	-15.031383	1.256205
-61.476425	-22.403620	1.261210
-61.727419	-30.265795	1.266214
-61.954056	-20.079783	1.271219
-61.735763	-23.970008	1.276224
-62.499061	-24.297824	1.281229
-63.198374	-30.193527	1.286234
-63.359493	-25.985716	1.291238
-63.448519	-28.774050	1.296243
-63.600453	-28.258874	1.301248
-63.684577	-23.458790	1.306253
-64.247771	-15.145968	1.311258
-64.900185	-15.733485	1.316262
-65.314814	-14.627007	1.321267
-64.967917	-19.773640	1.326272
-65.220964	-13.654428	1.331277
-65.235751	-20.301278	1.336282
-65.159675	-15.102272	1.341286
-65.265081	-23.103212	1.346291
-65.911933	-27.639296	1.351296
-66.676497	-18.033550	1.356301
-66.862270	-27.901565	1.361306
-66.803846	-19.598746	1.366310
-66.964118	-19.863233	1.371315
-67.042992	-24.612569	1.376320
-67.796043	-16.149511	1.381325
-67.961731	-19.388489	1.386330
-68.029782	-22.005659	1.391334
-68.188925	-18.866929	1.396339
-68.230946	-20.990143	1.401344
-69.158754	-19.926155	1.406349
-69.673853	-27.271584	1.411354
-69.869366	-18.542702	1.416358
-70.006852	-16.588004	1.421363
-69.934168	-26.380422	1.426368
-69.956006	-26.815242	1.431373
-69.888599	-21.903304	1.436378
-70.027765	-26.667321	1.441382
-70.759272	-27.185498	1.446387
-71.281984	-35.128766	1.451392
-71.630286	-29.708327	1.456397
-71.775970	-28.747621	1.461402
-71.685669	-25.938507	1.466406
-71.566499	-26.297815	1.471411
-71.857609	-23.191300	1.476416
-72.780914	-23.169186	1.481421
-72.706394	-34.467948	1.486426
-72.910619	-26.270229	1.491430
-73.532498	-24.195253	1.496435
-74.318629	-28.821538	1.501440
-74.430142	-22.767012	1.506445
-74.374015	-20.253959	1.511450
-74.666065	-30.411618	1.516454
-74.686074	-18.282154	1.521459
-74.719762	-20.888438	1.526464
-74.611615	-24.994459	1.531469
-74.608323	-26.766425	1.536474
-75.522573	-30.858426	1.541478
-76.173309	-23.061738	1.546483
-75.904797	-36.939996	1.551488
-75.923393	-21.201551	1.556493
-76.579945	-28.870464	1.561498
-77.381136	-28.864428	1.566502
-77.605891	-25.970972	1.571507
-77.356793	-21.939629	1.576512
-77.607107	-24.406635	1.581517
-77.571112	-31.643430	1.586522
-77.610735	-25.255675	1.591526
-78.207714	-25.102702	1.596531
-78.654289	-26.017740	1.601536
-78.891322	-23.686424	1.606541
-79.159624	-30.521177	1.611546
-79.543744	-24.794464	1.616550
-79.777213	-22.110513	1.621555
-80.064758	-25.982875	1.626560
-80.800937	-19.036550	1.631565
-80.815696	-27.319489	1.636570
-80.716851	-24.047662	1.641574
-81.256556	-18.015165	1.646579
-80.769681	-26.696519	1.651584
-81.361972	-21.171537	1.656589
-81.028715	-33.172438	1.661594
-81.490056	-28.634300	1.666598
-82.246853	-34.842525	1.671603
-82.373206	-21.310176	1.676608
-82.593581	-27.280260	1.681613
-82.650101	-34.262565	1.686618
-83.433533	-27.898640	1.691622
-84.001057	-30.176161	1.696627
-83.735774	-26.082381	1.701632
-83.930450	-26.903962	1.706637
-84.007979	-30.804394	1.711642
-84.171388	-22.777022	1.716646
-84.462148	-26.876376	1.721651
-84.601952	-29.058380	1.726656
-85.266979	-18.723200	1.731661
-85.445025	-23.016256	1.736666
-85.532398	-31.166991	1.741670
-85.680347	-25.478207	1.746675
-86.141980	-23.354190	1.751680
-86.930489	-19.494761	1.756685
-87.260300	-18.404696	1.761690
-87.246919	-31.949639	1.766694
-87.254814	-21.562858	1.771699
-87.331428	-24.610570	1.776704
-87.458254	-23.134001	1.781709
-87.432594	-14.394386	1.786714
-87.521535	-18.570184	1.791718
-88.457157	-14.131291	1.796723
-88.493083	-26.758367	1.801728
-88.905775	-14.443889	1.806733
-89.166442	-21.961300	1.811738
-89.261505	-22.928632	1.816742
-90.530287	-27.974232	1.821747
-90.154270	-28.766009	1.826752
-90.543785	-21.216228	1.831757
-90.664203	-26.568638	1.836762
-90.342430	-26.308527	1.841766
-90.550949	-21.157901	1.846771
-90.411297	-19.669421	1.851776
-91.676885	-13.250502	1.856781
-91.817371	-18.542167	1.861786
-91.912558	-22.514071	1.866790
-92.172393	-13.396838	1.871795
-92.084428	-20.479839	1.876800
-92.768762	-20.137363	1.881805
-93.166856	-16.508942	1.886810
-93.422134	-19.084447	1.891814
-93.930292	-6.487753	1.896819
-93.792445	-16.323724	1.901824
-94.018561	-8.779490	1.906829
-93.704104	-24.915557	1.911834
-93.838896	-23.499433	1.916838
-94.799631	-23.441318	1.921843
-95.328283	-22.270765	1.926848
-95.622921	-17.270451	1.931853
-95.589341	-20.853030	1.936858
-95.355649	-31.850581	1.941862
-95.946301	-22.661200	1.946867
-95.706474	-31.774249	1.951872
-96.482283	-20.259616	1.956877
-96.924827	-18.583745	1.961882
-96.801970	-21.681463	1.966886
-96.924600	-23.996354	1.971891
-97.231727	-21.471686	1.976896
-97.895713	-19.984297	1.981901
-98.491805	-27.135156	1.986906
-98.460027	-17.447978	1.991910
-98.783903	-18.288812	1.996915
-98.615572	-18.628129	2.006912
-98.049364	-16.463819	2.016909
-97.690635	-16.882762	2.026906
-97.413449	-16.247121	2.036902
-97.269178	-20.512907	2.046899
-96.226007	-18.835604	2.056896
-95.914336	-21.190996	2.066893
-95.584329	-24.461085	2.076890
-94.724193	-29.135285	2.086886
-94.552824	-27.120162	2.096883
-94.074317	-26.385481	2.106880
-93.270601	-20.723920	2.116877
-93.137785	-18.182365	2.126874
-92.353693	-24.041540	2.136870
-91.586513	-15.143993	2.146867
-91.373392	-22.971204	2.156864
-91.171280	-26.271484	2.166861
-90.366478	-25.113079	2.176858
-90.134828	-23.909741	2.186854
-89.175940	-22.082143	2.196851
-88.607295	-21.963050	2.206848
-88.523438	-22.319477	2.216845
-88.253815	-22.355362	2.226842
-87.156811	-14.518938	2.236838
-87.191900	-24.003489	2.246835
-86.295966	-26.237903	2.256832
-85.534400	-18.708695	2.266829
-85.619990	-22.043721	2.276826
-84.826269	-20.368571	2.286822
-83.996255	-21.220823	2.296819
-84.016356	-26.547095	2.306816
-83.716193	-18.789331	2.316813
-82.680625	-18.259528	2.326810
-82.631609	-17.638458	2.336806
-81.565451	-18.347644	2.346803
-81.042240	-19.717934	2.356800
-80.822388	-19.172183	2.366797
-80.846378	-19.566863	2.376794
-79.795413	-17.071261	2.386790
-79.265039	-22.569907	2.396787
-79.024381	-22.518206	2.406784
-78.236526	-24.382819	2.416781
-78.024356	-24.666446	2.426778
-77.487016	-19.920439	2.436774
-76.890094	-26.440559	2.446771
-76.503435	-26.568339	2.456768
-75.766762	-22.516664	2.466765
-75.237676	-23.806719	2.476762
-75.060343	-28.878201	2.486758
-74.154802	-26.700140	2.496755
-73.496078	-29.599659	2.506752
-73.193909	-30.290199	2.516749
-73.378232	-28.942493	2.526746
-72.527503	-28.789103	2.536742
-72.012907	-22.502904	2.546739
-70.889269	-20.955694	2.556736
-70.460471	-27.011107	2.566733
-70.339971	-23.695348	2.576730
-70.318924	-19.077229	2.586726
-69.406656	-22.255644	2.596723
-69.215289	-26.829558	2.606720
-67.998863	-21.573421	2.616717
-67.433305	-18.267348	2.626714
-67.343051	-20.624007	2.636710
-67.232264	-25.619859	2.646707
-66.236408	-31.623560	2.656704
-65.818415	-27.368152	2.666701
-65.308503	-26.111115	2.676698
-64.599531	-31.197138	2.686694
-64.428767	-27.578506	2.696691
-63.980768	-31.673491	2.706688
-62.763454	-28.344751	2.716685
-62.560179	-23.759381	2.726682
-62.652699	-26.210446	2.736678
-62.230358	-26.609492	2.746675
-60.979739	-23.501438	2.756672
-60.936503	-25.309715	2.766669
-60.503124	-25.471905	2.776666
-59.637634	-22.314098	2.786662
-59.530784	-27.734699	2.796659
-58.564074	-22.460915	2.806656
-57.803704	-25.404533	2.816653
-57.834554	-28.526340	2.826650
-57.706006	-23.634784	2.836646
-56.732147	-29.815830	2.846643
-56.313045	-22.726632	2.856640
-55.878991	-23.254863	2.866637
-54.747273	-21.949843	2.876634
-54.528282	-23.566523	2.886630
-54.445132	-17.388078	2.896627
-54.370490	-17.512791	2.906624
-53.386614	-18.367598	2.916621
-52.812649	-20.048201	2.926618
-51.864768	-20.416913	2.936614
-51.516807	-26.446689	2.946611
-51.405305	-25.473990	2.956608
-51.055003	-27.371845	2.966605
-50.286400	-28.662835	2.976602
-50.039801	-23.473901	2.986598
-49.197688	-20.004973	2.996595
-48.706883	-28.111913	3.006592
-48.441293	-25.778865	3.016589
-47.637656	-21.587713	3.026586
-47.158479	-19.427160	3.036582
-47.000384	-26.339921	3.046579
-45.986978	-24.523712	3.056576
-45.309625	-21.250969	3.066573
-45.039910	-20.361770	3.076570
-45.054092	-23.467371	3.086566
-44.655977	-27.406696	3.096563
-43.656306	-24.593368	3.106560
-43.553760	-27.318188	3.116557
-42.677950	-25.588063	3.126554
-42.500616	-22.292382	3.136550
-41.852314	-28.410424	3.146547
-40.753183	-26.220155	3.156544
-40.486613	-27.914263	3.166541
-40.710321	-30.612716	3.176538
-40.091688	-28.880703	3.186534
-39.410804	-17.485596	3.196531
-38.399889	-21.424449	3.206528
-37.748635	-28.152531	3.216525
-37.578764	-15.782278	3.226522
-37.693537	-24.529486	3.236518
-37.045984	-18.287031	3.246515
-35.878495	-24.598341	3.256512
-36.040306	-24.147056	3.266509
-34.978807	-33.029579	3.276506
-34.382799	-20.982215	3.286502
-34.323944	-26.289161	3.296499
-34.200013	-33.571081	3.306496
-33.239482	-25.113162	3.316493
-32.876546	-25.622105	3.326490
-32.065358	-27.639554	3.336486
-31.442188	-18.976389	3.346483
-31.135664	-20.392986	3.356480
-31.249402	-23.356831	3.366477
-30.044008	-27.527251	3.376474
-29.689939	-22.587484	3.386470
-29.341294	-25.107064	3.396467
-28.678223	-27.930832	3.406464
-28.381709	-27.612153	3.416461
-27.863062	-26.939237	3.426458
-26.765699	-26.411948	3.436454
-26.786952	-28.724454	3.446451
-26.341249	-28.870702	3.456448
-25.674136	-25.322801	3.466445
-25.050306	-28.181563	3.476442
-25.122300	-24.328104	3.486438
-24.079953	-26.166289	3.496435
-23.525969	-29.420314	3.506432
-23.465998	-26.493454	3.516429
-22.653841	-27.351232	3.526426
-22.277121	-27.911854	3.536422
-21.917640	-27.629288	3.546419
-20.621928	-22.317109	3.556416
-20.364869	-29.389507	3.566413
-20.306621	-28.650228	3.576410
-20.303657	-27.341442	3.586406
-19.198917	-31.836421	3.596403
-18.901601	-24.708279	3.606400
-17.531649	-30.412340	3.616397
-17.791792	-30.750922	3.626394
-17.344954	-29.379701	3.636390
-16.778091	-31.954383	3.646387
-15.646140	-32.527444	3.656384
-15.917478	-34.466197	3.666381
-15.441316	-29.840853	3.676378
-14.761753	-29.731226	3.686374
-13.841683	-32.438295	3.696371
-13.845272	-27.920422	3.706368
-13.240018	-28.486877	3.716365
-12.463490	-30.326288	3.726362
-11.946979	-29.862655	3.736358
-12.042736	-26.491520	3.746355
-10.959289	-25.843568	3.756352
-10.443514	-27.138326	3.766349
-10.352278	-27.736633	3.776346
-9.845097	-29.766963	3.786342
-9.158413	-31.774262	3.796339
-8.758644	-30.410855	3.806336
-7.718612	-32.110342	3.816333
-7.395986	-29.379512	3.826330
-6.913744	-30.089593	3.836326
-7.032432	-29.418227	3.846323
-6.553280	-37.926503	3.856320
-5.528560	-29.524850	3.866317
-5.301355	-26.211344	3.876314
-4.391702	-28.097694	3.886310
-4.041204	-23.106750	3.896307
-4.077915	-29.844793	3.906304
-3.455776	-19.461071	3.916301
-2.953892	-11.675444	3.926298
-2.634336	11.401937	3.936294
-2.395429	18.431891	3.946291
-1.776172	35.109847	3.956288
-1.253453	61.098293	3.966285
-0.667442	85.914291	3.976282
-0.167651	106.966536	3.986278
0.000000	118.644556	3.991283
-0.201038	133.068544	3.996288
0.398702	138.460909	4.001293
-0.042189	149.711027	4.006298
0.319031	163.015990	4.011302
0.651324	170.610518	4.016307
0.460420	178.947435	4.021312
0.772749	178.758210	4.026317
0.982541	201.612497	4.031322
1.286084	208.663211	4.036326
1.256987	207.067079	4.041331
1.127864	211.285838	4.046336
1.275162	209.934003	4.051341
0.944744	213.920876	4.056346
0.978731	208.790860	4.061350
1.322754	213.316075	4.066355
1.353218	211.925373	4.071360
1.213035	200.939242	4.076365
1.066177	208.697199	4.081370
1.248519	201.231418	4.086374
1.378118	209.119422	4.091379
1.141962	210.272331	4.096384
1.446529	207.142898	4.101389
1.526422	209.801834	4.106394
1.524972	211.380998	4.111398
1.444208	209.126228	4.116403
1.184440	192.360593	4.121408
1.557200	196.173003	4.126413
1.316237	202.371798	4.131418
1.319374	206.909059	4.136422
1.189503	206.187632	4.141427
1.315424	216.771268	4.146432
1.585006	216.153205	4.151437
1.693264	219.939959	4.156442
1.394549	206.893442	4.161446
1.286775	202.414826	4.166451
1.361289	215.779941	4.171456
1.708475	221.587715	4.176461
1.596730	221.528111	4.181466
1.619921	213.258288	4.186470
1.581470	201.225019	4.191475
0.965991	195.746905	4.196480
1.736394	203.682124	4.201485
1.386358	209.267311	4.206490
1.516035	213.520374	4.211494
1.739615	210.371791	4.216499
1.553645	220.499923	4.221504
1.473007	213.898997	4.226509
1.073381	221.429650	4.231514
1.230168	227.754008	4.236518
1.517388	216.711694	4.241523
0.912758	225.157600	4.246528
1.709619	219.852709	4.251533
1.396564	216.387462	4.256538
1.717034	215.372023	4.261542
1.737075	228.175867	4.266547
1.788498	234.339480	4.271552
1.591799	234.196262	4.276557
1.405023	242.030308	4.281562
1.644760	257.227799	4.286566
1.793867	261.127384	4.291571
1.780753	262.160875	4.296576
2.159698	260.759626	4.301581
1.972744	259.274483	4.306586
2.221595	246.282106	4.311590
1.883532	231.167287	4.316595
1.650651	232.150340	4.321600
1.656226	226.921224	4.326605
1.423273	236.642740	4.331610
1.614277	248.014044	4.336614
1.970735	253.197894	4.341619
1.695615	263.526313	4.346624
2.284167	253.920219	4.351629
1.855686	258.185207	4.356634
1.599899	263.513859	4.361638
1.914263	263.120644	4.366643
2.106217	255.473866	4.371648
2.319718	249.379919	4.376653
2.081541	262.542289	4.381658
2.132402	260.288803	4.386662
2.178061	259.206781	4.391667
2.030462	263.612334	4.396672
2.339322	257.176394	4.401677
2.258996	251.380337	4.406682
1.797053	239.548987	4.411686
1.656185	248.138731	4.416691
1.976707	259.190815	4.421696
1.775927	255.960742	4.426701
1.892220	267.071515	4.431706
1.929710	269.416613	4.436710
2.056693	262.731163	4.441715
1.566537	265.202510	4.446720
2.087761	259.806692	4.451725
1.801083	262.078581	4.456730
1.968734	261.212373	4.461734
2.508376	273.936330	4.466739
1.963520	276.825027	4.471744
2.232202	287.160699	4.476749
2.255250	293.489864	4.481754
2.368844	289.193216	4.486758
2.216609	288.796950	4.491763
2.234549	296.473591	4.496768
2.515504	293.328120	4.501773
2.105012	293.029085	4.506778
2.340854	290.478755	4.511782
2.343126	288.335927	4.516787
2.408051	299.612704	4.521792
2.362930	292.891013	4.526797
2.475737	293.302171	4.531802
2.334102	290.267725	4.536806
2.437584	284.034507	4.541811
1.999589	295.044287	4.546816
2.638599	287.290904	4.551821
2.206730	293.173641	4.556826
2.528077	301.059540	4.561830
2.434272	292.993164	4.566835
2.404688	300.444226	4.571840
2.342144	291.676073	4.576845
2.374611	299.076406	4.581850
2.401636	297.142009	4.586854
2.367904	296.176733	4.591859
2.313044	301.974152	4.596864
2.628820	294.968523	4.601869
2.398254	297.556929	4.606874
2.337400	299.333015	4.611878
2.348730	291.135366	4.616883
2.154288	300.037121	4.621888
2.418272	297.993628	4.626893
2.471226	300.879835	4.631898
2.683259	315.228486	4.636902
2.658212	310.051971	4.641907
2.564105	322.259496	4.646912
2.830170	317.065360	4.651917
2.737611	319.895942	4.656922
3.066467	309.693246	4.661926
2.892551	303.793673	4.666931
2.400566	302.640242	4.671936
2.373095	296.022978	4.676941
2.468990	313.429261	4.681946
2.687035	329.534615	4.686950
3.072975	329.043902	4.691955
3.022145	327.776569	4.696960
2.704017	315.374917	4.701965
2.715005	320.160346	4.706970
2.682866	323.812306	4.711974
2.983504	329.837401	4.716979
3.046939	331.864643	4.721984
2.577298	320.506932	4.726989
2.653890	322.735448	4.731994
2.516634	326.489868	4.736998
2.817114	337.228995	4.742003
2.828950	343.607398	4.747008
3.075197	334.242448	4.752013
3.050374	337.356244	4.757018
2.956317	336.703079	4.762022
3.139961	334.298141	4.767027
2.821054	330.746416	4.772032
3.123908	326.702979	4.777037
3.126858	334.079996	4.782042
2.953918	341.722160	4.787046
2.950110	333.449836	4.792051
2.604203	335.970915	4.797056
2.998995	329.099992	4.802061
2.669606	338.234279	4.807066
2.733007	340.313033	4.812070
2.951859	337.298608	4.817075
3.008384	346.918977	4.822080
3.175896	344.986767	4.827085
2.730876	338.193535	4.832090
3.013585	343.577100	4.837094
3.084054	342.617457	4.842099
3.137531	351.423722	4.847104
3.291868	361.463230	4.852109
3.365438	350.692217	4.857114
2.885541	351.036943	4.862118
3.288398	352.401365	4.867123
3.294087	362.341166	4.872128
3.289417	352.179266	4.877133
3.081650	340.676743	4.882138
3.315074	357.772979	4.887142
3.448780	360.719037	4.892147
3.091067	351.401399	4.897152
3.249271	356.540757	4.902157
3.445753	366.007324	4.907162
3.320808	369.006476	4.912166
3.411644	366.592629	4.917171
3.224413	360.090792	4.922176
3.150291	353.843739	4.927181
2.967391	362.833013	4.932186
3.365842	362.563614	4.937190
3.452450	364.638923	4.942195
3.352105	367.759113	4.947200
3.181238	361.073805	4.952205
3.129159	364.574758	4.957210
3.451017	366.894292	4.962214
3.183511	353.857678	4.967219
2.760366	361.542270	4.972224
3.620147	357.120461	4.977229
3.494008	359.052408	4.982234
3.371995	360.485195	4.987238
3.411029	362.090231	4.992243
3.141751	371.234515	4.997248
3.365466	380.029775	5.002253
3.636304	390.296880	5.007258
3.508901	394.464096	5.012262
3.708342	387.941040	5.017267
3.663751	401.509562	5.022272
3.871318	396.739300	5.027277
3.787953	393.947383	5.032282
3.289742	392.316628	5.037286
3.583133	389.826413	5.042291
3.192787	401.508012	5.047296
3.727242	394.929478	5.052301
3.712074	401.313955	5.057306
3.509167	392.674169	5.062310
3.839256	392.431285	5.067315
3.748185	407.709357	5.072320
4.004163	399.902521	5.077325
3.925541	402.389809	5.082330
3.755282	400.535824	5.087334
3.820994	405.824706	5.092339
3.815063	410.996788	5.097344
4.157198	397.938318	5.102349
3.709852	403.294199	5.107354
3.676006	410.490861	5.112358
3.610863	395.112827	5.117363
3.692162	402.993930	5.122368
3.892983	400.133443	5.127373
3.806770	399.419775	5.132378
3.642026	401.355356	5.137382
3.705471	407.203871	5.142387
3.640467	401.203541	5.147392
3.866777	392.963333	5.152397
3.779691	405.078196	5.157402
3.753274	403.895418	5.162406
3.900005	398.293975	5.167411
3.736897	409.574454	5.172416
3.894171	405.576612	5.177421
4.227837	400.555766	5.182426
3.989126	403.335773	5.187430
4.010247	393.088864	5.192435
3.996291	392.202399	5.197440
3.812210	394.351742	5.202445
3.997394	392.811475	5.207450
3.839035	398.175347	5.212454
4.112891	423.688358	5.217459
3.885679	425.345777	5.222464
4.004961	430.969955	5.227469
4.058548	429.701899	5.232474
4.130465	436.137487	5.237478
4.256090	428.636390	5.242483
4.349709	435.749796	5.247488
4.606822	432.298423	5.252493
4.237578	419.992573	5.257498
4.177811	406.696351	5.262502
4.037832	406.903882	5.267507
4.344511	428.390296	5.272512
4.050511	430.244274	5.277517
4.285532	422.869912	5.282522
4.304717	427.381886	5.287526
4.506370	421.985058	5.292531
4.248711	420.872737	5.297536
3.936660	400.538571	5.302541
4.128672	417.099048	5.307546
4.047713	434.951533	5.312550
4.294758	426.298395	5.317555
4.090920	429.297401	5.322560
4.259578	432.341090	5.327565
4.125820	436.547061	5.332570
4.251373	430.433269	5.337574
3.756651	429.905451	5.342579
4.034345	423.073611	5.347584
3.725906	441.372658	5.352589
4.461696	456.708828	5.357594
4.267603	467.632954	5.362598
4.702142	459.353098	5.367603
4.459896	465.891240	5.372608
4.502143	467.422147	5.377613
4.738271	464.123826	5.382618
4.436222	464.749125	5.387622
4.807665	469.611075	5.392627
4.380103	458.092566	5.397632
4.744027	466.354733	5.402637
4.642703	466.163751	5.407642
4.651148	464.575189	5.412646
4.826498	461.637013	5.417651
4.577302	455.052450	5.422656
4.574719	442.047868	5.427661
4.569368	441.868029	5.432666
4.612260	463.514998	5.437670
5.110174	448.387044	5.442675
4.436239	442.604948	5.447680
4.182211	442.065689	5.452685
4.527551	457.391131	5.457690
4.290460	466.985206	5.462694
4.776529	464.368153	5.467699
4.699938	470.809403	5.472704
4.247351	467.483437	5.477709
4.538762	464.160963	5.482714
4.506668	465.187941	5.487718
4.599713	461.984158	5.492723
4.641581	468.565241	5.497728
4.670842	465.480951	5.502733
4.576774	472.194661	5.507738
4.208770	479.423995	5.512742
4.745531	479.905263	5.517747
4.980962	485.014313	5.522752
4.587116	488.250224	5.527757
4.844528	482.748629	5.532762
4.933215	489.983648	5.537766
5.074719	483.353519	5.542771
4.877885	498.749639	5.547776
5.039009	484.126763	5.552781
5.113800	483.331569	5.557786
4.805023	488.397335	5.562790
5.235945	484.321599	5.567795
5.058421	487.080635	5.572800
4.949487	489.470142	5.577805
4.936055	481.077574	5.582810
4.881995	497.486282	5.587814
5.101251	484.915190	5.592819
4.690936	497.442808	5.597824
5.055483	498.051264	5.602829
5.100593	489.811408	5.607834
4.909613	492.502420	5.612838
5.453764	482.109246	5.617843
4.828093	491.091596	5.622848
4.975294	484.139451	5.627853
4.983332	480.611106	5.632858
5.028273	492.124589	5.637862
5.201725	482.152747	5.642867
5.049831	487.628457	5.647872
5.212876	491.829104	5.652877
5.134946	480.481399	5.657882
5.005917	484.873086	5.662886
5.403779	479.750413	5.667891
5.616465	485.763690	5.672896
5.376916	488.212715	5.677901
5.114975	486.555849	5.682906
5.023372	491.132562	5.687910
5.289192	484.396595	5.692915
5.305866	493.673574	5.697920
4.867909	490.551992	5.702925
4.983305	482.568686	5.707930
4.771121	485.745112	5.712934
5.248452	502.123453	5.717939
5.395933	505.294791	5.722944
5.615922	517.503346	5.727949
5.733300	516.425809	5.732954
5.125302	502.464278	5.737958
5.206204	501.040925	5.742963
5.153595	514.612058	5.747968
5.305442	522.674342	5.752973
5.593943	520.888434	5.757978
5.550843	526.444418	5.762982
5.623989	515.037531	5.767987
5.190588	525.466928	5.772992
5.386137	523.887042	5.777997
5.632775	519.048900	5.783002
5.281709	531.614096	5.788006
5.491094	522.174622	5.793011
5.449488	518.436232	5.798016
5.302582	517.631964	5.803021
5.266937	520.521437	5.808026
5.387163	525.995318	5.813030
5.521896	520.036856	5.818035
5.392883	525.362759	5.823040
5.602209	522.403158	5.828045
5.557120	520.426605	5.833050
5.389711	531.190852	5.838054
5.545829	531.823760	5.843059
5.566276	527.392689	5.848064
5.347696	525.237458	5.853069
5.748909	541.247382	5.858074
5.449445	555.211680	5.863078
5.644769	545.982123	5.868083
5.687384	553.347941	5.873088
5.849393	560.397389	5.878093
6.127790	550.908778	5.883098
5.875149	551.139111	5.888102
5.993610	549.061468	5.893107
5.793991	539.910733	5.898112
5.487535	525.156657	5.903117
5.880953	531.564306	5.908122
5.739146	545.406384	5.913126
6.079055	551.706076	5.918131
6.193954	547.033799	5.923136
6.113193	534.541948	5.928141
5.665659	521.637029	5.933146
5.681738	531.494900	5.938150
6.230614	523.854997	5.943155
5.572408	529.710968	5.948160
5.539246	518.932450	5.953165
6.089567	531.793385	5.958170
6.171251	549.321085	5.963174
5.912031	538.424680	5.968179
5.691972	544.583050	5.973184
5.925753	541.966912	5.978189
6.125745	552.193956	5.983194
5.741040	550.844147	5.988198
6.476029	546.952090	5.993203
5.875057	553.662944	5.998208
5.680993	551.437541	6.003213
6.193209	560.988307	6.008218
6.069163	555.271208	6.013222
6.021058	551.150847	6.018227
5.682650	564.033862	6.023232
6.259979	553.553644	6.028237
6.091171	558.765771	6.033242
5.963095	563.629755	6.038246
6.126375	557.565711	6.043251
5.988860	559.790840	6.048256
5.874425	560.606688	6.053261
5.929857	551.749586	6.058266
6.055356	555.307020	6.063270
6.219907	546.360019	6.068275
6.065860	556.374151	6.073280
6.202833	556.291318	6.078285
6.292235	558.289622	6.083290
5.976581	539.252989	6.088294
5.951636	524.972881	6.093299
5.944959	530.954418	6.098304
5.908745	549.089715	6.103309
6.268775	552.710929	6.108314
6.103090	544.562193	6.113318
6.193337	525.144592	6.118323
6.199433	523.279347	6.123328
5.810511	529.598286	6.128333
6.030571	514.532066	6.133338
5.675217	530.077804	6.138342
6.148462	540.825170	6.143347
6.034207	541.047979	6.148352
6.081331	544.458741	6.153357
6.221781	532.715478	6.158362
6.083393	528.273412	6.163366
6.033235	519.912164	6.168371
5.906832	522.881197	6.173376
5.816827	522.158283	6.178381
5.963404	519.668482	6.183386
5.893881	521.792162	6.188390
6.179350	533.870102	6.193395
6.051800	537.296169	6.198400
6.157173	537.150092	6.203405
6.150617	539.113962	6.208410
5.810601	531.419960	6.213414
5.863810	531.683911	6.218419
5.957537	537.356564	6.223424
6.033854	547.994819	6.228429
6.236464	540.511113	6.233434
6.088933	532.661900	6.238438
5.920059	536.376612	6.243443
6.085742	537.858669	6.248448
5.838699	530.886339	6.253453
6.086599	527.654335	6.258458
6.033630	543.367878	6.263462
6.319101	535.946035	6.268467
6.170165	528.948382	6.273472
5.776479	534.175439	6.278477
6.052037	529.307640	6.283482
5.964876	534.183390	6.288486
5.877854	525.744967	6.293491
5.866599	529.715379	6.298496
6.007303	541.237707	6.303501
6.345462	535.169184	6.308506
5.794436	526.932708	6.313510
6.170731	524.126222	6.318515
6.022913	519.589023	6.323520
5.694826	532.814661	6.328525
5.809931	533.903308	6.333530
6.098380	545.940111	6.338534
6.256191	549.121588	6.343539
6.014659	549.140308	6.348544
6.348439	548.427141	6.353549
6.237618	535.456981	6.358554
6.092793	532.137266	6.363558
5.903061	523.987392	6.368563
6.267483	526.707212	6.373568
5.880387	529.299475	6.378573
6.089779	524.004736	6.383578
6.048688	525.558330	6.388582
6.168202	523.800996	6.393587
5.921950	524.899159	6.398592
6.002951	528.759966	6.403597
6.128279	526.823471	6.408602
5.727050	528.776915	6.413606
6.067050	525.030588	6.418611
6.176467	529.623952	6.423616
5.866502	531.371653	6.428621
6.159130	523.014817	6.433626
5.995387	532.058639	6.438630
6.101921	530.792069	6.443635
5.781621	527.744339	6.448640
6.045624	534.311162	6.453645
6.070158	530.718504	6.458650
5.936738	529.615796	6.463654
5.998829	524.094432	6.468659
6.023829	538.333558	6.473664
5.374470	526.952172	6.478669
6.169071	537.248680	6.483674
5.840046	551.894945	6.488678
6.149737	551.242996	6.493683
6.197283	554.974565	6.498688
6.018257	543.387999	6.503693
6.144198	529.336286	6.508698
5.675756	537.562468	6.513702
6.076977	545.252332	6.518707
6.149907	559.103857	6.523712
5.884490	546.411686	6.528717
6.373087	537.733682	6.533722
5.884278	531.113973	6.538726
5.959065	535.120461	6.543731
5.778048	531.343779	6.548736
5.785276	544.384841	6.553741
6.062087	549.444633	6.558746
6.151695	568.390118	6.563750
6.116338	557.739418	6.568755
5.861791	560.218762	6.573760
6.134584	566.572200	6.578765
5.951504	564.323664	6.583770
5.983364	561.458170	6.588774
6.190783	559.471767	6.593779
6.086630	567.721117	6.598784
6.079175	562.737366	6.603789
5.960369	543.328114	6.608794
6.190074	550.403447	6.613798
6.114226	537.499720	6.618803
5.925143	539.872709	6.623808
5.657539	535.927627	6.628813
6.106078	536.485274	6.633818
6.231284	550.715317	6.638822
6.117827	547.810345	6.643827
5.979517	530.145869	6.648832
5.960436	537.983672	6.653837
6.340962	531.644487	6.658842
6.364301	539.450993	6.663846
5.827070	529.170155	6.668851
5.973481	533.324824	6.673856
5.853009	535.296901	6.678861
5.881167	521.099963	6.683866
5.943049	535.390208	6.688870
6.184478	529.177858	6.693875
5.732677	522.418031	6.698880
5.862502	539.557079	6.703885
5.914508	545.798866	6.708890
5.848108	557.253279	6.713894
5.933485	559.277904	6.718899
6.169258	553.643308	6.723904
6.205982	556.192035	6.728909
6.343089	551.112320	6.733914
6.016427	541.403230	6.738918
5.899294	526.809616	6.743923
5.983856	541.574858	6.748928
5.989332	552.156567	6.753933
6.160284	556.842366	6.758938
5.834155	546.645359	6.763942
5.925505	553.681836	6.768947
6.082039	555.283223	6.773952
6.206840	556.382896	6.778957
6.074006	542.885726	6.783962
6.081791	540.380422	6.788966
6.124015	536.514280	6.793971
5.995443	527.426580	6.798976
5.992104	536.661707	6.803981
6.320282	521.423453	6.808986
5.761297	528.443285	6.813990
5.770392	527.148843	6.818995
6.112834	538.880295	6.824000
5.954002	542.081050	6.829005
6.079789	537.212987	6.834010
6.088907	546.750159	6.839014
6.040639	530.412884	6.844019
6.036346	528.947395	6.849024
6.180458	528.914491	6.854029
6.067337	529.337807	6.859034
5.761387	532.353347	6.864038
6.052451	520.612781	6.869043
6.321846	525.403042	6.874048
5.973656	531.052371	6.879053
5.835931	528.482361	6.884058
6.085871	528.230251	6.889062
5.957240	531.377655	6.894067
6.162100	525.278715	6.899072
5.933146	535.325367	6.904077
6.109634	535.458393	6.909082
5.733390	533.436228	6.914086
5.864165	532.515528	6.919091
6.401319	541.037561	6.924096
5.820405	546.124926	6.929101
6.048344	528.389147	6.934106
6.114365	543.440052	6.939110
6.005115	542.152182	6.944115
5.993034	534.269290	6.949120
5.769517	533.201234	6.954125
6.174678	536.200256	6.959130
5.817611	556.259280	6.964134
6.075394	559.465251	6.969139
6.055073	556.077553	6.974144
6.158517	558.854014	6.979149
6.165322	530.345919	6.984154
5.905345	535.299424	6.989158
5.884920	531.749140	6.994163
6.272050	537.457472	6.999168
6.147993	539.427775	7.004173
6.085731	527.353202	7.009178
5.741525	527.926281	7.014182
5.830172	529.789134	7.019187
6.280286	524.445456	7.024192
5.999716	538.227820	7.029197
5.890849	529.967855	7.034202
5.936923	530.174574	7.039206
6.174235	540.108103	7.044211
5.812007	533.148136	7.049216
6.057682	540.317714	7.054221
6.178218	547.561102	7.059226
5.951815	539.360064	7.064230
5.781168	544.161825	7.069235
6.381303	546.750064	7.074240
5.952765	540.540508	7.079245
5.932707	546.023220	7.084250
5.709644	546.824494	7.089254
5.812381	564.095339	7.094259
6.065233	555.915377	7.099264
5.865272	566.140775	7.104269
5.784674	565.866830	7.109274
6.285733	564.196488	7.114278
6.283995	563.974213	7.119283
6.261975	561.881349	7.124288
5.897491	564.413631	7.129293
6.067997	564.021340	7.134298
5.936059	569.622046	7.139302
6.389563	563.297997	7.144307
6.211119	546.993115	7.149312
5.702428	546.526215	7.154317
5.933112	535.498366	7.159322
6.202970	554.928848	7.164326
5.790185	557.132069	7.169331
5.838337	560.264808	7.174336
5.931436	567.208252	7.179341
6.458198	564.309352	7.184346
6.270187	566.654144	7.189350
5.669666	547.434771	7.194355
6.051979	547.335979	7.199360
6.168101	555.832424	7.204365
6.179883	536.724405	7.209370
5.446647	544.078384	7.214374
5.899523	551.807454	7.219379
6.257051	552.826556	7.224384
6.031736	554.803169	7.229389
6.049817	556.833412	7.234394
6.239186	557.905028	7.239398
6.143235	557.561991	7.244403
6.215256	534.437198	7.249408
5.769835	546.137497	7.254413
6.029623	529.365977	7.259418
5.947239	529.880703	7.264422
5.770469	531.816121	7.269427
5.971896	554.250796	7.274432
6.152974	558.934722	7.279437
6.291320	553.256267	7.284442
5.748746	558.421946	7.289446
6.121762	553.872296	7.294451
5.901679	545.364330	7.299456
5.672919	560.231598	7.304461
6.078451	561.069289	7.309466
6.020360	563.769882	7.314470
6.098008	568.235906	7.319475
6.038941	567.300857	7.324480
5.855659	564.720032	7.329485
6.115169	558.917316	7.334490
5.752437	558.794879	7.339494
5.721122	566.630183	7.344499
5.877660	571.741078	7.349504
5.619295	568.500740	7.354509
5.971031	569.983961	7.359514
5.476919	572.039622	7.364518
5.819326	570.079608	7.369523
5.890620	561.159881	7.374528
5.802476	574.557963	7.379533
6.030198	560.986075	7.384538
6.271482	565.859742	7.389542
6.022620	575.387552	7.394547
6.024802	565.070058	7.399552
5.620402	569.592224	7.404557
6.125438	573.400783	7.409562
6.144428	576.610186	7.414566
5.962627	576.260447	7.419571
6.089905	574.885255	7.424576
5.958141	571.273279	7.429581
5.928716	569.213807	7.434586
5.819239	579.456988	7.439590
6.053545	591.386756	7.444595
6.551231	597.705532	7.449600
6.337879	584.431630	7.454605
6.453758	566.448940	7.459610
6.284204	568.635567	7.464614
6.233816	559.984640	7.469619
6.236895	557.258105	7.474624
6.333401	569.268297	7.479629
6.236061	556.006783	7.484634
6.347101	561.338337	7.489638
5.908370	554.909836	7.494643
6.007571	559.960363	7.499648
6.132783	562.993315	7.504653
6.366802	557.780330	7.509658
6.127803	557.476965	7.514662
5.780921	542.289103	7.519667
6.268108	539.263556	7.524672
6.149646	542.663255	7.529677
5.849491	540.735053	7.534682
5.864229	537.602832	7.539686
5.810269	535.962039	7.544691
5.995650	534.765887	7.549696
6.078897	548.966961	7.554701
5.914166	551.837953	7.559706
6.034918	562.907745	7.564710
5.926307	563.848137	7.569715
5.977043	565.940662	7.574720
6.014013	566.838003	7.579725
6.152206	567.783705	7.584730
6.211093	560.722614	7.589734
5.816731	555.468442	7.594739
5.917683	556.266779	7.599744
5.702920	567.504617	7.604749
5.943642	571.631445	7.609754
6.066140	570.467805	7.614758
5.882874	566.903037	7.619763
6.534431	563.493080	7.624768
5.979816	577.954125	7.629773
5.941576	568.475311	7.634778
6.071163	569.994726	7.639782
6.041216	568.726480	7.644787
6.230986	563.757629	7.649792
5.766220	559.701723	7.654797
5.959690	558.394706	7.659802
5.915339	565.846170	7.664806
5.708164	572.619502	7.669811
6.117886	569.345497	7.674816
5.914878	565.330312	7.679821
5.870442	567.796770	7.684826
5.863328	565.172565	7.689830
5.916550	573.407697	7.694835
6.229872	573.327631	7.699840
6.078671	570.400883	7.704845
6.152301	569.448202	7.709850
6.042981	569.545278	7.714854
5.952609	573.852047	7.719859
6.277145	571.484326	7.724864
5.870142	572.597863	7.729869
6.058565	568.390377	7.734874
6.327266	574.871189	7.739878
5.794854	571.990989	7.744883
6.615695	563.628757	7.749888
5.926052	559.904324	7.754893
5.889292	548.503377	7.759898
5.912877	560.412561	7.764902
5.793901	567.469468	7.769907
6.142707	564.443939	7.774912
5.901821	571.474659	7.779917
6.001928	566.522234	7.784922
5.676696	569.669245	7.789926
5.716863	564.124462	7.794931
5.759733	557.679755	7.799936
5.881045	573.335657	7.804941
5.981592	559.725034	7.809946
6.070489	562.488512	7.814950
5.838677	564.720772	7.819955
5.921729	569.947438	7.824960
5.839363	577.786860	7.829965
5.893850	568.123175	7.834970
6.297147	570.111142	7.839974
5.976095	575.233434	7.844979
6.087860	575.630367	7.849984
6.088584	577.430032	7.854989
6.219115	565.373827	7.859994
6.350793	561.488130	7.864998
5.955033	573.372041	7.870003
6.351896	560.817655	7.875008
6.241406	562.367549	7.880013
6.437643	562.622025	7.885018
6.096220	561.853715	7.890022
6.149345	560.967184	7.895027
6.108680	562.834088	7.900032
6.134908	570.419110	7.905037
5.913334	553.303583	7.910042
5.736478	557.604934	7.915046
5.785140	565.718072	7.920051
5.846407	564.959253	7.925056
5.794613	568.985329	7.930061
5.821272	568.566536	7.935066
6.029612	568.060824	7.940070
5.936709	565.657046	7.945075
6.165642	571.665101	7.950080
5.961323	568.677488	7.955085
5.912103	565.927642	7.960090
6.050792	571.553197	7.965094
5.986684	567.709786	7.970099
6.253360	566.073124	7.975104
5.796994	572.622297	7.980109
5.885213	573.536017	7.985114
5.999474	565.675405	7.990118
5.797571	572.979954	7.995136
6.042614	561.969279	8.000154
6.002182	560.767825	8.005171
6.064966	560.983631	8.010189
6.005037	566.689078	8.015206
5.808324	579.117521	8.020224
6.332939	563.735442	8.025242
6.202499	571.388854	8.030259
5.996497	570.155371	8.035277
6.321411	567.880100	8.040294
5.793419	564.833722	8.045312
6.059261	560.885472	8.050330
6.018710	570.384898	8.055347
6.014218	563.504838	8.060365
5.834360	566.335456	8.065382
5.794063	574.812469	8.070400
6.014048	566.062879	8.075418
6.120276	571.228839	8.080435
5.860993	572.618769	8.085453
6.035637	568.488388	8.090470
6.085008	597.636406	8.095488
6.097878	600.156590	8.100506
6.199447	604.730458	8.105523
6.599940	599.522382	8.110541
6.326039	583.209588	8.115558
6.098010	573.267729	8.120576
6.255104	571.182440	8.125594
5.971604	569.413402	8.130611
5.986643	576.299272	8.135629
6.262988	567.593690	8.140646
5.778767	574.421494	8.145664
6.519923	585.452989	8.150682
6.346268	581.434607	8.155699
6.068356	584.907801	8.160717
6.098239	575.358440	8.165734
6.071554	585.527581	8.170752
6.573001	584.845803	8.175770
6.437814	579.927213	8.180787
6.098020	579.926040	8.185805
6.138304	568.326868	8.190822
6.058726	577.980191	8.195840
6.686427	566.127657	8.200858
6.546336	574.694812	8.205875
6.167698	572.340190	8.210893
6.070784	575.104321	8.215910
6.192160	584.416913	8.220928
6.090588	573.198093	8.225946
6.115698	573.431752	8.230963
5.944939	579.053987	8.235981
6.316011	580.484015	8.240998
5.981989	601.387415	8.246016
6.414208	601.667039	8.251034
6.414887	618.833190	8.256051
6.010661	609.658626	8.261069
5.646014	603.959573	8.266086
5.793443	606.314572	8.271104
6.340934	610.468953	8.276122
6.367669	607.602542	8.281139
6.035988	610.293554	8.286157
6.576601	607.652659	8.291174
6.566528	616.242793	8.296192
6.435094	612.651439	8.301210
6.682283	618.475525	8.306227
6.471859	617.883675	8.311245
6.744671	609.431986	8.316262
6.631777	606.441461	8.321280
6.820773	608.302601	8.326298
6.485636	585.942263	8.331315
6.169877	584.275211	8.336333
6.435830	579.521086	8.341350
6.152462	577.870521	8.346368
6.129321	581.712720	8.351386
6.645875	609.788386	8.356403
6.681499	593.454443	8.361421
6.573116	580.440012	8.366438
6.111499	589.360989	8.371456
6.326430	579.661305	8.376474
6.525256	578.424561	8.381491
6.029356	598.163896	8.386509
6.538546	594.358991	8.391526
6.494683	608.237838	8.396544
6.405749	601.781758	8.401562
6.489757	607.139980	8.406579
6.554882	614.649619	8.411597
6.755250	595.454322	8.416614
6.407490	589.032839	8.421632
6.469409	582.590564	8.426650
6.230799	586.448957	8.431667
6.530817	592.566235	8.436685
6.833409	589.364402	8.441702
6.488724	590.398618	8.446720
6.395644	578.744952	8.451738
6.141357	576.391192	8.456755
6.107138	600.843134	8.461773
6.367060	605.545888	8.466790
6.627727	608.482098	8.471808
6.785594	610.006682	8.476826
6.625221	613.281494	8.481843
6.437114	622.871129	8.486861
6.472606	616.937712	8.491878
6.333279	614.784581	8.496896
6.400750	615.232865	8.501914
6.376633	614.177121	8.506931
6.471057	621.607507	8.511949
6.409865	603.084213	8.516966
6.429683	615.799841	8.521984
6.373059	622.552922	8.527002
6.317523	613.632800	8.532019
6.248846	615.375596	8.537037
6.649256	613.800763	8.542054
6.545712	612.264896	8.547072
6.433312	607.569280	8.552090
6.386197	616.811570	8.557107
6.410122	630.636695	8.562125
6.913135	639.380053	8.567143
6.981116	641.605703	8.572160
6.814040	626.343021	8.577178
6.694818	617.000400	8.582195
6.605735	616.825831	8.587213
6.375203	618.645425	8.592231
6.626486	613.166009	8.597248
6.697153	633.638486	8.602266
6.544381	627.308313	8.607283
7.220124	629.699446	8.612301
6.818286	611.166807	8.617319
6.352390	617.643585	8.622336
6.746679	617.690529	8.627354
6.745244	607.135965	8.632371
6.408631	612.517387	8.637389
6.737625	613.944347	8.642407
6.624730	619.242665	8.647424
6.829708	634.826676	8.652442
6.656834	631.855921	8.657459
6.307738	630.646522	8.662477
6.848544	636.323576	8.667495
6.570012	639.460095	8.672512
6.288070	637.562452	8.677530
6.962491	640.679351	8.682547
6.880271	646.683972	8.687565
7.192546	638.694601	8.692583
6.994039	644.913347	8.697600
6.926460	639.254847	8.702618
6.822160	625.473805	8.707635
6.591670	629.461761	8.712653
6.640357	631.911063	8.717671
6.865008	639.046682	8.722688
6.505863	637.122062	8.727706
7.036055	631.464572	8.732723
6.612950	644.516543	8.737741
7.015678	633.055324	8.742759
6.876648	637.783996	8.747776
6.800943	636.467912	8.752794
7.031056	638.834419	8.757811
6.599881	635.741091	8.762829
6.711967	638.727106	8.767847
6.876140	634.842324	8.772864
6.663981	638.472938	8.777882
6.982179	635.217728	8.782899
6.843563	645.057827	8.787917
7.026546	643.915822	8.792935
7.316646	636.050983	8.797952
6.976184	641.522416	8.802970
7.157127	636.140067	8.807987
6.707505	634.854406	8.813005
6.858810	627.831795	8.818023
6.920744	635.075060	8.823040
6.664715	640.776984	8.828058
7.104596	633.595568	8.833075
6.642482	640.398481	8.838093
6.983816	633.331015	8.843111
6.959737	629.348281	8.848128
7.009195	637.961638	8.853146
7.037188	640.521054	8.858163
6.841093	649.779766	8.863181
7.160721	640.533348	8.868199
7.464268	634.292166	8.873216
6.946078	627.227278	8.878234
6.740940	626.277881	8.883251
6.820149	636.676750	8.888269
7.021654	626.918437	8.893287
6.749751	629.255875	8.898304
6.554192	637.383459	8.903322
7.015412	628.793087	8.908339
6.964360	636.987681	8.913357
7.154187	635.677624	8.918375
7.126961	639.015428	8.923392
7.011212	637.161914	8.928410
7.196682	640.540082	8.933427
7.136051	644.757773	8.938445
6.951684	639.435128	8.943463
7.252216	632.340957	8.948480
7.111376	635.986531	8.953498
7.485445	628.736886	8.958515
7.003327	630.778052	8.963533
6.891806	641.327003	8.968551
7.133842	638.063933	8.973568
7.099738	640.663551	8.978586
6.984334	636.374698	8.983603
7.119324	641.638669	8.988621
7.180150	639.722059	8.993639
7.140792	631.473616	8.998656
7.032470	641.001629	9.003674
7.247836	631.281960	9.008691
6.877599	639.467996	9.013709
7.109867	631.556834	9.018727
7.426072	635.466862	9.023744
7.481647	643.737892	9.028762
7.298471	630.232489	9.033779
7.179050	640.319391	9.038797
7.183925	632.317937	9.043815
7.051526	636.563651	9.048832
6.710147	645.975938	9.053850
7.202322	632.248078	9.058867
7.261083	645.893050	9.063885
7.087504	637.613683	9.068903
7.226342	635.454642	9.073920
7.130802	638.049080	9.078938
7.249448	637.471631	9.083955
7.301976	638.563296	9.088973
7.145951	643.218804	9.093991
7.257045	633.999835	9.099008
7.003280	642.965749	9.104026
7.331797	633.003735	9.109043
7.193107	644.230373	9.114061
7.171723	642.860414	9.119079
7.606602	637.200990	9.124096
6.959642	651.495866	9.129114
7.165800	638.194080	9.134131
7.246865	639.723905	9.139149
7.138466	634.704410	9.144167
6.872793	645.454470	9.149184
7.124144	661.550876	9.154202
7.226546	672.833276	9.159219
7.159586	672.612919	9.164237
7.023951	682.717493	9.169255
7.480116	671.905625	9.174272
7.248598	675.537879	9.179290
7.496280	668.820531	9.184307
7.799532	670.679293	9.189325
7.660131	669.592244	9.194343
7.425615	670.752702	9.199360
7.084333	680.974394	9.204378
7.419711	669.542803	9.209395
7.657785	662.398334	9.214413
7.409904	673.289159	9.219431
7.750605	659.532030	9.224448
7.424899	653.165920	9.229466
7.229100	639.658269	9.234483
7.319177	653.356326	9.239501
7.108568	662.609181	9.244519
7.302784	657.837976	9.249536
7.553456	669.543825	9.254554
7.521324	667.879992	9.259571
7.519976	676.322661	9.264589
7.531734	669.688471	9.269607
7.597606	667.458049	9.274624
7.323059	672.842992	9.279642
7.579332	666.817881	9.284659
7.355992	673.043506	9.289677
7.093462	672.972850	9.294695
7.525622	662.826735	9.299712
7.469848	668.611250	9.304730
7.513860	667.941834	9.309747
7.778113	659.708845	9.314765
7.610641	673.418467	9.319783
7.677431	666.291730	9.324800
7.575406	672.972828	9.329818
7.296113	676.304351	9.334835
7.771455	667.360065	9.339853
7.266652	673.167366	9.344871
7.388467	664.919380	9.349888
7.372632	668.849755	9.354906
7.520247	664.868894	9.359923
7.710703	662.607607	9.364941
7.145940	669.040940	9.369959
7.409700	660.279323	9.374976
7.173431	658.996124	9.379994
7.657058	667.148256	9.385011
7.669277	663.959454	9.390029
7.331622	670.278019	9.395047
7.824708	679.082489	9.400064
7.722133	686.278615	9.405082
7.624602	679.457018	9.410099
7.928702	667.277504	9.415117
7.520570	670.393366	9.420135
7.695475	658.856080	9.425152
7.551718	663.732384	9.430170
7.317554	667.866226	9.435187
7.438623	682.427628	9.440205
7.614439	697.247285	9.445223
7.817366	689.160648	9.450240
8.010872	697.898995	9.455258
7.921672	691.844079	9.460275
8.101738	687.153943	9.465293
7.819693	682.538756	9.470311
7.850236	671.990269	9.475328
7.662605	669.379409	9.480346
7.516937	666.629719	9.485363
7.694318	674.296772	9.490381
7.620993	681.169566	9.495399
7.884613	691.748159	9.500416
7.764907	696.209097	9.505434
7.736763	699.661232	9.510451
8.051372	689.731403	9.515469
7.650265	694.953858	9.520487
7.653918	695.818594	9.525504
7.913420	690.320468	9.530522
7.847419	700.761534	9.535539
8.087490	696.013036	9.540557
7.729904	689.171904	9.545575
7.836639	694.528755	9.550592
7.619888	700.014760	9.555610
7.824023	696.155233	9.560627
8.054104	683.589167	9.565645
7.660446	699.204266	9.570663
7.785399	688.752726	9.575680
8.148772	691.334169	9.580698
8.225056	696.283883	9.585715
8.309596	687.447997	9.590733
7.695971	679.286355	9.595751
7.754243	664.024114	9.600768
7.899274	670.334400	9.605786
7.900462	666.643517	9.610803
7.942091	663.527400	9.615821
7.879544	686.269114	9.620839
8.054717	682.934434	9.625856
8.021465	690.619446	9.630874
7.773733	681.517345	9.635891
8.187630	674.497290	9.640909
7.809114	682.152074	9.645927
7.853684	677.768613	9.650944
8.304095	690.341743	9.655962
8.079349	683.074703	9.660979
8.263143	672.735077	9.665997
7.718494	657.617953	9.671015
7.905579	673.854140	9.676032
7.767556	686.938462	9.681050
7.943638	695.297432	9.686067
8.417322	698.751109	9.691085
8.081637	702.721072	9.696103
8.318605	683.866436	9.701120
7.865220	670.741942	9.706138
7.900608	679.313954	9.711155
7.969731	682.997995	9.716173
7.977102	689.386593	9.721191
7.861069	690.193987	9.726208
8.112159	695.529690	9.731226
7.847377	702.058628	9.736243
8.174947	685.244380	9.741261
7.833574	694.645673	9.746279
8.410829	697.706237	9.751296
8.271488	690.789596	9.756314
7.956994	693.256923	9.761331
8.311944	696.168483	9.766349
8.362401	701.035865	9.771367
7.853432	701.676057	9.776384
8.277087	692.621819	9.781402
8.028182	700.279951	9.786419
8.110132	693.138094	9.791437
7.819805	695.012871	9.796455
7.922012	692.564630	9.801472
8.219766	690.639882	9.806490
8.014236	702.078012	9.811507
8.112486	694.466553	9.816525
8.261240	695.137587	9.821543
8.154321	692.975142	9.826560
8.432414	691.191042	9.831578
8.122739	706.441081	9.836595
8.584749	691.878054	9.841613
8.454785	690.201287	9.846631
8.030136	696.023668	9.851648
8.103329	695.454137	9.856666
8.103931	695.201334	9.861683
8.113366	691.131149	9.866701
8.365454	692.405114	9.871719
8.325523	697.776411	9.876736
8.372464	694.581853	9.881754
8.033485	704.816958	9.886771
8.190755	695.452913	9.891789
8.269092	713.869228	9.896807
8.377991	716.266843	9.901824
8.570228	706.844641	9.906842
8.077072	708.390430	9.911859
8.410857	713.083348	9.916877
8.284208	720.410633	9.921895
8.387867	732.340863	9.926912
8.567187	732.926527	9.931930
8.479162	728.277229	9.936947
8.544453	710.669817	9.941965
8.185443	715.229833	9.946983
8.098367	714.882499	9.952000
8.698947	718.310443	9.957018
8.294379	724.948754	9.962035
8.335075	731.536170	9.967053
8.391005	730.661246	9.972071
8.604134	730.710238	9.977088
8.800652	720.860178	9.982106
8.284562	731.649402	9.987123
8.344825	715.602573	9.992141
8.474478	725.129417	9.997159
8.386246	730.996098	10.002176
8.370851	718.000207	10.007194
8.691375	725.890812	10.012211
8.889502	721.253184	10.017229
8.718469	723.459766	10.022247
8.463662	712.642773	10.027264
8.531524	692.414240	10.032282
8.434842	703.114704	10.037299
8.890146	708.277234	10.042317
8.376831	706.573005	10.047335
8.507966	698.870670	10.052352
8.902112	690.215391	10.057370
8.443000	697.563075	10.062387
8.625526	696.478225	10.067405
8.514000	692.369412	10.072423
8.224807	696.989905	10.077440
8.691641	714.012045	10.082458
8.564751	727.123689	10.087475
8.645785	727.426826	10.092493
8.564416	732.778620	10.097511
8.600510	728.804005	10.102528
8.922067	717.913614	10.107546
8.532827	737.670304	10.112563
8.812799	739.736068	10.117581
8.561097	730.270048	10.122599
8.731452	731.686677	10.127616
8.873581	721.035432	10.132634
8.697805	732.022620	10.137651
8.538631	730.608544	10.142669
8.579647	725.550893	10.147687
8.893950	723.101776	10.152704
8.886497	725.491102	10.157722
8.514344	720.633358	10.162739
8.313499	728.478810	10.167757
8.870467	729.125159	10.172775
8.392928	729.322770	10.177792
8.631677	728.810465	10.182810
8.841822	733.062471	10.187827
8.692959	732.284054	10.192845
8.602670	729.791703	10.197863
8.320053	735.924025	10.202880
8.310921	720.772097	10.207898
8.313606	735.854699	10.212915
8.638477	752.142163	10.217933
8.890379	754.974347	10.222951
8.586566	763.892715	10.227968
8.582675	763.434367	10.232986
8.629815	762.489641	10.238003
8.733044	758.493666	10.243021
9.213316	755.795420	10.248039
8.773604	759.570824	10.253056
9.020133	754.603535	10.258074
9.346743	753.910941	10.263091
8.772728	754.909524	10.268109
9.041184	746.367542	10.273127
8.771539	754.206290	10.278144
9.197492	752.513442	10.283162
9.001787	747.149725	10.288179
8.827026	750.860783	10.293197
9.222904	751.379486	10.298215
8.994767	749.884708	10.303232
8.794804	754.161326	10.308250
8.982656	754.891239	10.313267
8.951595	755.429461	10.318285
8.821508	756.170685	10.323303
8.958441	750.841645	10.328320
9.480639	750.294607	10.333338
9.270049	750.586194	10.338355
8.974597	731.214186	10.343373
8.983543	716.726160	10.348391
9.053909	737.974765	10.353408
9.059785	731.325381	10.358426
8.880332	727.480549	10.363443
9.181539	742.642852	10.368461
9.132162	745.429259	10.373479
9.109322	739.250350	10.378496
9.369278	732.750614	10.383514
9.542028	718.742913	10.388531
9.207835	717.260189	10.393549
9.149366	724.258488	10.398567
8.761974	725.593074	10.403584
8.972681	720.067980	10.408602
8.909468	720.863480	10.413619
8.885508	722.120957	10.418637
9.001110	729.345537	10.423655
9.138924	748.505939	10.428672
9.303783	742.629394	10.433690
8.693690	741.224241	10.438707
8.954337	750.891606	10.443725
9.342125	743.583340	10.448743
9.352080	750.520323	10.453760
9.587417	750.077869	10.458778
9.271319	753.697377	10.463795
9.149150	744.991352	10.468813
9.298692	743.830469	10.473831
8.840693	750.765418	10.478848
9.074484	745.969917	10.483866
9.210718	750.946727	10.488883
9.125535	756.018861	10.493901
9.241224	752.590872	10.498919
9.236144	758.398127	10.503936
9.103995	754.291925	10.508954
9.069860	756.620323	10.513971
8.995918	748.487381	10.518989
9.498159	745.659127	10.524007
9.042358	756.275795	10.529024
8.869309	755.798216	10.534042
9.150302	745.797939	10.539059
9.122917	760.213534	10.544077
9.114940	759.889713	10.549095
9.089169	779.831925	10.554112
9.691185	776.306078	10.559130
9.734993	771.482977	10.564147
9.450679	773.489831	10.569165
9.868267	767.897394	10.574183
9.377106	756.212864	10.579200
9.482303	746.365705	10.584218
9.608362	739.661380	10.589235
9.325736	752.500426	10.594253
9.416104	740.255071	10.599271
9.629713	740.216981	10.604288
9.285467	742.169193	10.609306
9.353528	746.825812	10.614323
9.025669	745.630209	10.619341
9.447096	750.796394	10.624359
9.589896	776.748548	10.629376
9.707683	773.331624	10.634394
9.510657	753.071683	10.639411
9.642251	752.645227	10.644429
9.549819	744.152770	10.649447
9.271970	745.928643	10.654464
9.366660	760.290560	10.659482
9.724081	767.432992	10.664499
9.700339	781.112609	10.669517
9.750460	765.766977	10.674535
9.326093	756.811003	10.679552
9.685605	755.364576	10.684570
9.662038	747.418557	10.689587
9.522466	745.315052	10.694605
9.487003	745.190260	10.699623
9.405954	766.316347	10.704640
9.650476	780.332230	10.709658
9.951436	767.495712	10.714675
9.658858	777.560985	10.719693
9.679247	769.006528	10.724711
9.698273	766.025622	10.729728
9.558543	769.260829	10.734746
9.465857	776.138447	10.739763
9.789998	774.087278	10.744781
10.011330	769.043846	10.749799
9.669269	760.032904	10.754816
9.677290	753.322924	10.759834
9.646420	748.791314	10.764851
9.301003	767.183772	10.769869
9.632254	767.430910	10.774887
9.618986	774.804797	10.779904
9.790526	766.137915	10.784922
9.707175	772.897062	10.789939
9.375309	773.946489	10.794957
9.753589	767.336205	10.799975
9.822281	764.662019	10.804992
9.495575	782.439226	10.810010
9.751452	761.716108	10.815027
9.851068	770.528309	10.820045
9.781963	766.224273	10.825063
9.960350	764.399198	10.830080
9.677600	770.093391	10.835098
9.744276	769.196214	10.840115
9.701965	782.636401	10.845133
9.767629	774.028777	10.850151
9.750871	776.169271	10.855168
9.550194	777.064304	10.860186
9.906061	776.358991	10.865203
9.896463	784.867254	10.870221
9.951856	780.024515	10.875239
10.010492	776.326850	10.880256
10.004231	781.691813	10.885274
10.106075	767.361969	10.890291
9.886524	776.129391	10.895309
9.886644	769.913599	10.900327
9.892976	769.587802	10.905344
9.775737	770.626884	10.910362
10.043574	784.704654	10.915379
9.618441	802.093873	10.920397
9.906205	807.657782	10.925415
10.172774	799.747153	10.930432
10.434527	793.715181	10.935450
10.573430	786.041043	10.940467
10.196986	783.216166	10.945485
9.999154	772.784557	10.950503
10.205554	775.062104	10.955520
9.867645	775.701136	10.960538
10.123018	763.713464	10.965555
9.868933	766.144423	10.970573
9.947012	774.432267	10.975591
10.086159	776.908343	10.980608
10.028018	772.251327	10.985626
10.456037	773.808354	10.990643
10.244932	782.212196	10.995661
10.227124	775.423810	11.000679
10.434142	774.215220	11.005696
10.198644	774.625100	11.010714
10.388505	770.400221	11.015731
10.394617	776.783945	11.020749
10.296629	766.188178	11.025767
9.966323	768.379017	11.030784
10.235199	778.013935	11.035802
10.683611	767.485160	11.040819
10.148985	778.295201	11.045837
10.323376	777.104611	11.050855
10.398450	776.875300	11.055872
10.082469	768.519054	11.060890
10.349792	776.044106	11.065907
10.060770	769.241975	11.070925
10.054024	769.284859	11.075943
10.129461	778.387667	11.080960
10.226618	773.072685	11.085978
10.297176	780.960226	11.090995
10.453313	774.590650	11.096013
9.991762	778.613757	11.101031
10.275881	773.123729	11.106048
9.788132	782.729225	11.111066
9.516581	784.844592	11.116083
9.938467	794.737633	11.121101
10.289769	803.500302	11.126119
10.615252	794.319355	11.131136
10.369464	807.132268	11.136154
10.325233	803.395727	11.141171
10.365333	796.858753	11.146189
10.538521	798.130045	11.151207
10.662639	797.554440	11.156224
10.397137	808.993919	11.161242
10.488182	798.912468	11.166259
10.330131	799.300470	11.171277
10.385705	801.516780	11.176295
10.513585	794.921966	11.181312
10.340967	804.629615	11.186330
10.534362	802.702056	11.191347
10.228584	792.594199	11.196365
10.185901	805.323087	11.201383
10.195236	791.838811	11.206400
10.433445	806.495494	11.211418
10.334539	800.478361	11.216435
10.552669	817.183943	11.221453
10.881663	818.304246	11.226471
10.924753	808.831093	11.231488
10.801138	797.850197	11.236506
10.686181	789.691743	11.241523
10.698081	801.014812	11.246541
10.622639	793.558438	11.251559
10.598486	794.469908	11.256576
10.877544	796.649998	11.261594
10.711174	794.338730	11.266611
10.924876	784.916863	11.271629
11.025199	792.020781	11.276647
11.170536	798.828287	11.281664
10.836785	802.409393	11.286682
11.091556	799.305589	11.291699
10.948130	778.809191	11.296717
10.413996	771.976391	11.301735
10.884111	768.733003	11.306752
10.505964	775.821267	11.311770
10.577279	777.460588	11.316787
10.554074	785.225869	11.321805
10.443325	787.906310	11.326823
10.895679	788.621165	11.331840
11.238551	796.132929	11.336858
10.959726	793.644229	11.341875
11.035988	793.528494	11.346893
10.790270	781.048617	11.351911
10.638700	770.021979	11.356928
10.772561	769.669553	11.361946
10.639684	789.299610	11.366963
10.599616	785.951734	11.371981
10.581404	791.250966	11.376999
10.831420	784.830016	11.382016
10.669408	788.669279	11.387034
10.666728	790.521238	11.392051
10.771517	790.857842	11.397069
10.741126	793.251370	11.402087
10.740416	781.915899	11.407104
10.504908	792.862630	11.412122
10.635119	791.981701	11.417139
10.634020	795.263640	11.422157
10.838673	818.362068	11.427175
11.104959	821.721777	11.432192
11.198684	823.839258	11.437210
11.260354	817.457750	11.442227
11.111281	807.747535	11.447245
10.903570	798.573779	11.452263
11.086411	790.959682	11.457280
10.822892	791.103744	11.462298
10.708335	794.772561	11.467315
11.028564	802.160131	11.472333
10.982478	822.914383	11.477351
11.236604	811.222534	11.482368
11.395130	826.103050	11.487386
11.038615	811.571126	11.492403
11.143209	803.596377	11.497421
10.555622	814.945894	11.502439
11.087644	810.998975	11.507456
11.013875	830.019326	11.512474
11.034382	821.605758	11.517491
11.392961	824.449029	11.522509
11.162458	817.608054	11.527527
11.088010	814.383575	11.532544
11.115662	832.764726	11.537562
11.099954	828.214441	11.542579
11.357331	823.075263	11.547597
11.083287	828.007049	11.552615
11.642796	823.222940	11.557632
11.392774	824.596201	11.562650
11.362944	822.950474	11.567667
11.400195	821.049950	11.572685
11.561948	822.432187	11.577703
11.740190	806.801531	11.582720
11.261451	797.966735	11.587738
11.098667	798.511812	11.592755
11.055381	793.662576	11.597773
11.100696	792.614219	11.602791
11.370753	797.593292	11.607808
11.142215	803.715898	11.612826
11.435596	821.496763	11.617843
11.383879	821.451036	11.622861
11.188774	824.419848	11.627879
10.999941	819.162050	11.632896
11.238812	835.047722	11.637914
11.198389	831.599112	11.642931
11.573190	828.673449	11.647949
11.311034	839.185670	11.652967
11.397032	830.056170	11.657984
11.236018	828.236505	11.663002
11.280477	834.861528	11.668019
11.722171	829.413888	11.673037
11.299959	828.981503	11.678055
11.375975	827.324153	11.683072
11.489323	824.895699	11.688090
11.398868	823.608417	11.693107
11.557953	819.787814	11.698125
10.989362	829.453573	11.703143
11.326440	819.282552	11.708160
11.332981	825.973690	11.713178
11.391552	827.474977	11.718195
11.530797	831.399398	11.723213
11.393770	836.913193	11.728231
11.752746	853.820283	11.733248
12.128869	846.022979	11.738266
11.689899	839.098804	11.743283
11.879530	831.398921	11.748301
11.560975	830.126577	11.753319
11.707706	817.925368	11.758336
11.852518	815.646816	11.763354
12.053133	820.315758	11.768371
11.914942	820.260730	11.773389
11.621850	826.634967	11.778407
11.730056	824.028240	11.783424
11.471952	816.285582	11.788442
11.762017	826.019773	11.793459
11.860306	818.353525	11.798477
11.344137	816.495826	11.803495
11.373103	818.538601	11.808512
11.741385	816.244696	11.813530
11.441715	818.559202	11.818547
11.390827	824.271710	11.823565
11.371868	834.528708	11.828583
11.908145	841.991933	11.833600
11.815098	842.080209	11.838618
11.902968	858.490098	11.843635
12.204140	848.208474	11.848653
12.178158	851.571313	11.853671
11.922625	831.644169	11.858688
11.875253	829.797025	11.863706
11.373805	821.575788	11.868723
11.953502	824.781242	11.873741
11.977286	845.196805	11.878759
11.807912	842.334479	11.883776
11.866921	834.566072	11.888794
11.751268	837.981549	11.893811
11.844166	835.294682	11.898829
11.961538	839.522712	11.903847
11.835340	850.945059	11.908864
11.848257	849.250126	11.913882
11.820299	849.550054	11.918899
12.049228	841.288568	11.923917
11.953255	839.752605	11.928935
11.924179	843.979692	11.933952
12.215793	841.165828	11.938970
11.975221	850.854444	11.943987
11.977024	836.030104	11.949005
11.932243	842.373072	11.954023
12.354296	846.283736	11.959040
12.171053	843.711094	11.964058
11.913425	851.187289	11.969075
12.250756	841.912231	11.974093
12.075933	846.667365	11.979111
11.901958	840.255581	11.984128
12.039478	840.099782	11.989146
12.284451	846.423904	11.994163
12.225826	835.484185	11.999181
12.319332	839.527594	12.004199
12.189705	843.393396	12.009216
12.197314	836.351181	12.014234
12.432137	837.330787	12.019251
12.503376	832.074012	12.024269
11.895298	838.757487	12.029287
12.092529	834.525859	12.034304
12.389003	837.421146	12.039322
12.201530	846.678154	12.044339
12.378782	838.288225	12.049357
12.327388	835.521713	12.054375
12.126312	848.492208	12.059392
12.315537	835.031648	12.064410
12.003845	845.038322	12.069427
12.429971	839.908989	12.074445
12.272483	835.615633	12.079463
12.322263	842.467326	12.084480
12.409001	837.317819	12.089498
12.273701	840.533805	12.094515
12.348172	828.465807	12.099533
12.357699	833.181749	12.104551
12.441111	838.493302	12.109568
12.555962	830.600695	12.114586
12.457995	837.824472	12.119603
12.488324	831.744984	12.124621
12.190380	835.268202	12.129639
12.217470	841.429986	12.134656
12.832698	841.494675	12.139674
12.461738	837.048880	12.144691
12.276653	833.441950	12.149709
12.606127	837.347864	12.154727
12.663121	835.500759	12.159744
12.416500	843.514472	12.164762
12.422863	844.737018	12.169779
12.265682	839.021631	12.174797
12.157588	843.417700	12.179815
12.361526	849.428555	12.184832
12.885714	852.896345	12.189850
12.502816	855.697449	12.194867
12.593367	855.610842	12.199885
12.986803	840.714954	12.204903
12.536174	842.843842	12.209920
12.677216	832.249784	12.214938
12.591925	840.672192	12.219955
13.151301	839.922548	12.224973
12.736590	830.350001	12.229991
12.498393	836.758457	12.235008
12.742900	826.574416	12.240026
12.444155	848.844482	12.245043
12.518960	842.010024	12.250061
12.720665	855.868507	12.255079
12.949706	869.756333	12.260096
13.233884	861.633711	12.265114
12.866625	849.983708	12.270131
12.692483	839.041857	12.275149
13.246823	831.257568	12.280167
12.847234	841.175650	12.285184
12.999453	831.500563	12.290202
12.800910	832.662949	12.295219
12.741836	828.460379	12.300237
12.903685	836.394638	12.305255
12.864580	844.020069	12.310272
13.085215	831.110583	12.315290
12.721476	833.895520	12.320307
12.715251	829.003917	12.325325
12.860925	833.389456	12.330343
12.531435	839.118577	12.335360
12.718374	843.150452	12.340378
12.857671	857.198396	12.345395
13.173387	868.561752	12.350413
12.977581	866.212830	12.355431
12.857088	876.322502	12.360448
13.241654	874.547916	12.365466
12.990558	871.168827	12.370483
13.137212	864.824406	12.375501
13.086230	869.403141	12.380519
13.047202	852.682487	12.385536
13.059446	858.702254	12.390554
12.809064	856.154113	12.395571
13.136088	861.540683	12.400589
13.608137	867.813433	12.405607
13.036833	856.711362	12.410624
13.078854	841.524862	12.415642
12.993947	842.669612	12.420659
13.005530	853.516417	12.425677
13.369897	856.522114	12.430695
13.170375	864.904791	12.435712
13.057346	864.344439	12.440730
13.145157	860.439963	12.445747
13.178928	863.173254	12.450765
13.114789	858.036914	12.455783
13.069821	869.126548	12.460800
13.281250	865.702365	12.465818
13.288781	867.068020	12.470835
13.054619	869.273265	12.475853
13.109303	859.769422	12.480871
13.234491	871.284797	12.485888
13.494890	860.615053	12.490906
13.569222	860.873635	12.495923
13.084495	870.029886	12.500941
13.554291	853.254107	12.505959
13.413386	871.337640	12.510976
13.531145	858.401862	12.515994
12.896893	868.710377	12.521011
13.206122	857.701856	12.526029
13.782239	860.920509	12.531047
13.522453	864.968098	12.536064
13.323164	858.969533	12.541082
13.399603	865.600691	12.546099
13.069339	870.587467	12.551117
13.244238	866.400865	12.556135
13.299140	864.854877	12.561152
13.642765	860.712381	12.566170
13.643108	868.185235	12.571187
13.194531	863.377106	12.576205
13.850137	859.019572	12.581223
13.574248	867.378678	12.586240
13.053413	858.237053	12.591258
13.261351	868.710032	12.596275
12.836215	866.325859	12.601293
13.346030	883.920570	12.606311
13.578543	889.997572	12.611328
13.904064	887.144229	12.616346
13.955295	890.204146	12.621363
14.156482	894.330128	12.626381
14.187591	871.447726	12.631399
13.778785	870.141507	12.636416
14.060630	853.759037	12.641434
14.004896	854.698180	12.646451
13.725611	856.088888	12.651469
13.787611	853.034711	12.656487
13.781119	861.299206	12.661504
13.850063	856.650647	12.666522
13.921604	854.761369	12.671539
13.459760	857.301545	12.676557
13.651222	849.699770	12.681575
13.369227	852.328268	12.686592
13.245132	847.809310	12.691610
13.582700	854.119677	12.696627
13.952121	874.337107	12.701645
14.478929	868.421838	12.706663
13.852929	864.947357	12.711680
14.089859	852.537887	12.716698
13.944102	847.365068	12.721715
13.954269	856.849578	12.726733
13.997223	850.772322	12.731751
13.964137	864.579539	12.736768
13.857266	853.731651	12.741786
13.945876	854.992938	12.746803
13.878465	850.669308	12.751821
13.937551	849.161602	12.756839
14.043087	848.050123	12.761856
14.038599	859.017304	12.766874
14.119652	855.150561	12.771891
13.882517	852.933675	12.776909
13.905972	852.169629	12.781927
13.816851	862.568178	12.786944
13.858788	854.523073	12.791962
14.069120	862.964648	12.796979
13.869301	883.274774	12.801997
14.523004	876.701905	12.807015
14.256735	867.933849	12.812032
13.837557	852.373336	12.817050
14.273622	862.797119	12.822067
14.052127	885.661504	12.827085
14.203979	882.601497	12.832103
14.372475	884.930611	12.837120
14.174159	873.630550	12.842138
14.377518	866.495673	12.847155
14.177145	865.645861	12.852173
14.155251	859.945071	12.857191
13.926439	873.172137	12.862208
14.091219	885.594309	12.867226
14.182687	886.351212	12.872243
13.975396	889.607474	12.877261
14.400523	889.504832	12.882279
14.275889	888.033844	12.887296
14.039016	885.738567	12.892314
14.078764	886.111139	12.897331
14.436769	893.977515	12.902349
14.430426	875.236555	12.907367
14.044189	888.831418	12.912384
13.955163	885.376278	12.917402
14.149592	880.931332	12.922419
14.146973	899.269545	12.927437
14.431378	906.427282	12.932455
14.202104	920.992594	12.937472
14.231255	914.148735	12.942490
14.888921	916.558263	12.947507
14.795108	925.456910	12.952525
14.640168	906.458640	12.957543
14.883353	919.324529	12.962560
14.536906	903.235015	12.967578
14.791373	889.123476	12.972595
14.533644	886.225380	12.977613
14.842879	881.269320	12.982631
14.459664	889.326540	12.987648
14.303770	882.934971	12.992666
14.357042	880.351897	12.997683
14.832952	908.516330	13.002701
14.622824	902.679772	13.007719
15.060446	908.196463	13.012736
14.963700	893.163594	13.017754
14.830233	886.902949	13.022771
14.685269	889.454434	13.027789
14.578367	885.665655	13.032807
14.704656	880.211961	13.037824
14.433647	885.958185	13.042842
14.894146	880.085780	13.047859
14.366431	884.230888	13.052877
15.038338	893.438922	13.057895
15.109322	889.525808	13.062912
14.810116	889.533661	13.067930
14.760135	875.379245	13.072947
14.858570	880.246613	13.077965
14.874445	888.417266	13.082983
15.069505	872.177095	13.088000
14.393193	883.717330	13.093018
14.312712	887.081721	13.098035
14.553429	907.830325	13.103053
14.905379	910.525110	13.108071
15.112145	914.170273	13.113088
15.086370	917.220113	13.118106
15.016014	914.807892	13.123123
14.792389	929.419518	13.128141
15.112835	917.042229	13.133159
15.137929	922.084346	13.138176
14.883295	923.423735	13.143194
15.386593	917.108028	13.148211
14.956314	922.507427	13.153229
15.260216	917.981354	13.158247
15.225008	914.918853	13.163264
15.535120	913.099113	13.168282
15.211913	896.866393	13.173299
14.770783	890.014202	13.178317
14.716475	900.587319	13.183335
14.796549	911.914534	13.188352
14.671175	917.940184	13.193370
15.236633	906.710468	13.198387
14.999810	912.625049	13.203405
14.899874	916.454065	13.208423
15.329360	911.345018	13.213440
15.301417	915.448713	13.218458
15.404329	906.837210	13.223475
15.005804	913.540738	13.228493
15.281489	917.655177	13.233511
15.240975	904.777457	13.238528
15.277906	921.215925	13.243546
15.348306	907.986780	13.248563
15.219616	910.746981	13.253581
15.029504	918.578154	13.258599
15.032267	916.646323	13.263616
15.349810	931.303766	13.268634
15.515911	928.973642	13.273651
15.510731	931.426006	13.278669
15.372984	932.924380	13.283687
15.572454	931.365469	13.288704
15.427216	929.866787	13.293722
15.694484	939.083587	13.298739
15.725424	918.051066	13.303757
15.729222	908.175716	13.308775
15.632329	898.784740	13.313792
15.730058	909.503939	13.318810
15.720744	903.872700	13.323827
15.660230	905.357495	13.328845
15.380328	907.998647	13.333863
15.412631	916.144941	13.338880
15.279011	903.738918	13.343898
15.201024	909.063443	13.348915
15.659338	912.881509	13.353933
15.725913	926.170726	13.358951
15.681931	919.823599	13.363968
15.671916	924.180223	13.368986
15.958721	924.518578	13.374003
15.643513	909.236447	13.379021
15.511930	909.046472	13.384039
15.711108	916.537997	13.389056
15.601357	922.804358	13.394074
15.747891	925.572923	13.399091
15.736784	935.090923	13.404109
15.673522	933.726692	13.409127
15.927252	921.051405	13.414144
15.808905	930.138361	13.419162
15.996622	915.781956	13.424179
16.153062	930.322775	13.429197
15.703510	926.981260	13.434215
15.846362	924.806948	13.439232
15.675097	922.891730	13.444250
16.092788	926.091357	13.449267
15.878098	915.686851	13.454285
15.691353	925.111100	13.459303
15.955574	921.408884	13.464320
15.668700	926.321960	13.469338
15.513869	923.736726	13.474355
15.703857	920.603077	13.479373
15.434565	921.194532	13.484391
15.888108	911.838381	13.489408
15.679890	929.248513	13.494426
16.220856	938.234960	13.499443
16.066581	939.589227	13.504461
16.188586	939.670238	13.509479
16.158328	928.151372	13.514496
15.987525	924.259784	13.519514
16.168205	933.955860	13.524531
16.376923	944.848035	13.529549
15.938837	935.928478	13.534567
16.250629	931.247558	13.539584
16.414636	942.293191	13.544602
16.182736	941.384425	13.549619
16.205272	926.709708	13.554637
16.011117	921.855494	13.559655
16.668765	935.779095	13.564672
16.131897	930.510782	13.569690
16.093528	916.933514	13.574707
16.257571	932.707274	13.579725
16.260590	950.473379	13.584743
16.698045	946.367290	13.589760
16.534134	938.409375	13.594778
16.524281	919.565797	13.599795
16.703516	915.510742	13.604813
16.371873	908.867961	13.609831
16.183833	905.268196	13.614848
15.987762	914.793979	13.619866
16.150194	920.573950	13.624883
16.123163	933.815684	13.629901
16.181777	939.401051	13.634919
16.612833	938.293140	13.639936
16.490246	946.471398	13.644954
16.459577	946.095821	13.649971
16.879274	944.347692	13.654989
16.686981	943.046163	13.660007
16.971360	944.830923	13.665024
16.661644	947.367967	13.670042
16.636347	938.853264	13.675059
17.109196	927.349116	13.680077
16.730845	919.103112	13.685095
16.510169	912.665961	13.690112
16.588314	913.206577	13.695130
16.521966	906.952525	13.700147
16.670203	917.662579	13.705165
16.637666	926.812093	13.710183
17.099190	929.280478	13.715200
16.566698	917.697546	13.720218
16.577148	914.001922	13.725235
17.186234	928.179610	13.730253
16.571676	920.426242	13.735271
16.571845	911.903793	13.740288
16.697316	919.486654	13.745306
16.851678	931.757053	13.750323
16.893598	927.883387	13.755341
16.614782	939.715700	13.760359
17.136757	936.033789	13.765376
16.763581	938.756530	13.770394
16.945775	933.087663	13.775411
16.902764	932.283046	13.780429
16.925178	935.647338	13.785447
17.002043	929.201460	13.790464
17.074955	940.541299	13.795482
17.006039	940.089381	13.800499
17.073212	930.792867	13.805517
16.841642	939.267502	13.810535
16.956291	936.465996	13.815552
17.092735	935.395454	13.820570
16.839102	932.343922	13.825587
17.388810	928.728283	13.830605
17.042017	935.155156	13.835623
17.036550	936.766266	13.840640
17.037796	929.162487	13.845658
16.837687	933.963958	13.850675
17.333519	935.143255	13.855693
16.666900	932.303016	13.860711
17.344181	933.062519	13.865728
17.230752	934.060431	13.870746
17.089969	938.243445	13.875763
17.255117	926.839854	13.880781
17.037936	937.421462	13.885799
17.021406	935.390072	13.890816
17.120355	934.061970	13.895834
16.993532	935.904189	13.900851
17.280159	940.023122	13.905869
17.243137	962.981085	13.910887
17.433558	956.326636	13.915904
17.613169	963.498209	13.920922
17.347392	965.135891	13.925939
17.465476	956.813568	13.930957
17.266584	969.017299	13.935975
17.731629	959.775352	13.940992
17.708880	945.805724	13.946010
17.666094	938.284032	13.951027
17.578854	920.004032	13.956045
17.289219	919.852038	13.961063
17.257140	924.799691	13.966080
17.744330	938.118871	13.971098
17.288424	943.122538	13.976115
17.387732	929.453960	13.981133
17.563951	948.779110	13.986151
17.542579	945.158036	13.991168
17.397208	958.206010	13.996186
17.529224	961.611998	14.001203
17.567962	953.633510	14.006221
17.687795	957.008445	14.011239
17.626025	949.235571	14.016256
17.883650	950.749970	14.021274
17.695603	956.724205	14.026291
17.771002	945.166965	14.031309
18.100168	955.612056	14.036327
17.896978	951.689999	14.041344
18.106604	956.107895	14.046362
18.085989	959.629310	14.051379
18.175622	951.373116	14.056397
17.637099	941.271811	14.061415
17.633362	949.506765	14.066432
17.964100	952.468839	14.071450
17.690020	957.121549	14.076467
18.059514	947.273804	14.081485
18.252377	953.179058	14.086503
17.860896	959.402719	14.091520
18.010376	957.710357	14.096538
17.877169	964.123527	14.101555
18.151742	962.595875	14.106573
17.812004	962.156127	14.111591
17.952466	957.549237	14.116608
18.383620	948.649508	14.121626
18.236351	969.673851	14.126643
18.221098	958.373334	14.131661
18.056616	944.583470	14.136679
17.828236	948.859334	14.141696
18.262551	951.428682	14.146714
17.933919	949.784389	14.151731
18.322668	963.049422	14.156749
18.315331	963.666790	14.161767
17.858269	956.074719	14.166784
18.287378	958.242190	14.171802
18.270766	968.131186	14.176819
18.334842	945.674694	14.181837
18.296880	958.261200	14.186855
17.873913	959.267064	14.191872
18.484683	947.945567	14.196890
18.389132	969.358179	14.201907
18.315262	948.037079	14.206925
18.359711	955.954228	14.211943
18.576893	968.692186	14.216960
18.428169	959.719976	14.221978
18.174479	967.910506	14.226995
18.380815	966.474465	14.232013
18.274313	963.669025	14.237031
18.084823	963.857913	14.242048
18.353304	958.808188	14.247066
18.445050	959.466234	14.252083
18.271666	947.047863	14.257101
18.223275	959.814436	14.262119
18.345159	951.154886	14.267136
18.520837	953.766668	14.272154
18.136738	962.513413	14.277171
18.392383	969.260210	14.282189
18.161993	984.552509	14.287207
18.317467	984.618924	14.292224
18.531315	982.322223	14.297242
18.388218	992.560512	14.302259
18.495034	993.979026	14.307277
18.129226	993.185340	14.312295
18.397031	992.348543	14.317312
18.601454	1002.418275	14.322330
18.889605	1011.245454	14.327347
19.495877	1008.340089	14.332365
19.291670	999.897888	14.337383
19.096241	988.998037	14.342400
19.117342	981.599204	14.347418
18.733083	985.804044	14.352435
18.853747	977.398609	14.357453
19.224582	978.275785	14.362471
19.083830	984.323298	14.367488
19.116173	975.193936	14.372506
18.884586	986.559428	14.377523
19.396324	967.473129	14.382541
19.482036	969.303780	14.387559
18.967372	973.101487	14.392576
19.154162	970.993119	14.397594
19.340601	971.011102	14.402611
19.062173	969.496283	14.407629
18.951280	948.157299	14.412647
18.855230	951.834111	14.417664
19.153568	971.050883	14.422682
19.113857	974.492002	14.427699
19.122779	979.169902	14.432717
19.379130	978.472398	14.437735
18.975179	980.949465	14.442752
19.202499	979.603252	14.447770
18.996406	989.323645	14.452787
19.151886	978.223180	14.457805
19.225700	982.140365	14.462823
19.336333	987.021889	14.467840
19.179473	984.635791	14.472858
18.643404	986.752861	14.477875
18.901539	979.206910	14.482893
18.999071	986.720812	14.487911
19.017131	989.031153	14.492928
19.344927	990.079230	14.497946
19.178091	1006.952697	14.502963
19.227859	1002.986771	14.507981
19.496117	1004.334854	14.512999
19.463014	1006.052906	14.518016
19.377895	999.224388	14.523034
19.307296	1013.117867	14.528051
19.317846	1007.996667	14.533069
19.410917	999.314304	14.538087
19.362813	1007.181846	14.543104
19.802874	1000.095899	14.548122
19.690944	1006.152033	14.553139
19.340019	1000.339933	14.558157
19.474089	1001.274032	14.563175
19.672163	1002.155803	14.568192
19.403778	999.132290	14.573210
19.512667	1006.337246	14.578227
19.495700	996.997541	14.583245
19.651333	994.591978	14.588263
19.309083	1002.737351	14.593280
19.560409	1004.871278	14.598298
19.725767	1023.759361	14.603315
19.784300	1028.194030	14.608333
20.035861	1030.610589	14.613351
19.909486	1028.264710	14.618368
20.202050	1021.800399	14.623386
20.067600	1001.081755	14.628403
19.896270	997.026462	14.633421
20.075825	994.085464	14.638439
19.708141	996.767149	14.643456
19.957304	983.050876	14.648474
19.689059	996.711331	14.653491
19.797337	1001.335385	14.658509
20.166972	1012.004906	14.663527
19.862852	1027.733456	14.668544
20.012751	1025.408757	14.673562
20.335462	1015.991140	14.678579
20.102636	1020.622865	14.683597
20.498100	1006.504407	14.688615
20.185088	1003.503636	14.693632
20.199820	995.552723	14.698650
20.129710	990.850775	14.703667
20.105219	989.721841	14.708685
20.405611	988.933978	14.713703
19.522556	996.138230	14.718720
20.325215	999.840246	14.723738
20.366141	1016.922618	14.728755
20.271134	1025.393584	14.733773
20.455289	1021.861289	14.738791
20.221430	1029.970224	14.743808
20.311721	1025.819636	14.748826
20.463117	1036.211938	14.753843
20.732811	1022.953631	14.758861
20.218795	1002.489168	14.763879
20.162488	1001.105669	14.768896
20.752230	1015.917326	14.773914
20.465588	1015.047933	14.778931
20.418927	1007.655584	14.783949
20.511518	999.702012	14.788967
20.259020	999.386788	14.793984
20.129389	1014.727389	14.799002
20.445733	1017.507221	14.804019
20.345615	1021.925640	14.809037
20.363700	1023.559630	14.814055
20.306524	1022.854594	14.819072
20.295761	1022.925309	14.824090
20.522383	1011.479982	14.829107
20.150530	1022.708890	14.834125
20.133079	1025.260935	14.839143
20.826222	1045.369475	14.844160
21.081027	1049.888181	14.849178
20.829986	1034.611047	14.854195
20.773915	1021.072444	14.859213
20.959455	1027.874182	14.864231
20.554740	1018.751026	14.869248
20.705459	1012.952701	14.874266
21.026732	1041.742962	14.879283
20.646220	1030.380439	14.884301
21.181331	1042.523707	14.889319
21.056756	1030.435758	14.894336
20.847246	1028.431980	14.899354
20.904664	1022.758940	14.904371
20.836603	1030.256978	14.909389
20.991388	1027.543689	14.914407
20.872628	1037.889785	14.919424
21.069550	1040.201224	14.924442
20.984800	1049.072852	14.929459
20.980594	1042.395478	14.934477
21.455291	1052.342144	14.939495
21.417813	1043.152259	14.944512
21.268788	1023.791461	14.949530
21.017066	1020.704163	14.954547
21.179756	1018.449785	14.959565
21.379523	1015.173952	14.964583
21.178342	1023.825877	14.969600
20.844453	1020.891157	14.974618
21.436020	1022.739622	14.979635
21.017946	1037.362289	14.984653
21.320458	1037.508684	14.989671
21.289655	1037.653974	14.994688
21.302575	1053.809562	14.999706
21.637221	1045.760375	15.004723
21.237175	1043.588153	15.009741
21.275959	1042.555427	15.014759
20.902032	1040.662728	15.019776
21.274752	1050.806194	15.024794
21.708534	1047.819939	15.029811
21.432528	1053.470206	15.034829
21.447948	1042.244467	15.039847
21.534296	1049.489002	15.044864
21.534974	1055.180852	15.049882
21.427421	1042.488521	15.054899
21.214038	1051.452707	15.059917
21.505819	1041.078420	15.064935
21.631438	1046.529113	15.069952
21.219793	1047.265794	15.074970
21.309443	1044.087320	15.079987
21.143971	1048.690972	15.085005
21.468712	1060.749015	15.090023
21.669617	1071.054405	15.095040
21.790519	1082.379709	15.100058
21.941996	1077.984731	15.105075
21.521350	1080.241357	15.110093
21.909797	1078.035412	15.115111
21.773628	1091.483929	15.120128
21.749985	1085.563273	15.125146
22.292821	1081.543633	15.130163
22.158552	1076.488909	15.135181
22.249525	1066.524222	15.140199
21.590629	1053.865305	15.145216
21.807494	1052.742462	15.150234
21.999305	1052.596569	15.155251
21.859279	1063.917036	15.160269
21.859594	1066.651966	15.165287
22.010276	1073.026834	15.170304
21.775075	1067.862058	15.175322
22.387472	1061.111313	15.180339
22.560533	1067.694670	15.185357
22.280670	1057.824070	15.190375
22.112121	1043.811570	15.195392
21.805270	1033.385632	15.200410
22.185814	1040.285395	15.205427
22.035723	1059.204103	15.210445
22.336515	1056.539464	15.215463
22.322381	1057.571727	15.220480
22.076455	1074.394585	15.225498
22.664920	1065.328196	15.230515
22.232951	1072.622349	15.235533
22.500610	1076.160621	15.240551
22.535677	1061.311266	15.245568
22.038465	1048.854706	15.250586
22.249223	1053.478735	15.255603
22.361731	1060.624458	15.260621
22.167846	1063.001401	15.265639
22.257965	1061.664514	15.270656
22.236443	1072.933870	15.275674
22.856473	1068.649097	15.280691
22.577398	1068.742588	15.285709
22.313144	1064.554639	15.290727
22.507652	1065.424405	15.295744
22.406315	1078.382908	15.300762
22.448280	1069.661725	15.305779
22.248874	1073.708818	15.310797
22.505082	1076.423818	15.315815
22.320936	1059.262418	15.320832
22.091868	1068.078822	15.325850
22.619047	1090.972290	15.330867
22.688808	1094.017762	15.335885
22.533726	1094.034030	15.340903
23.017054	1091.228533	15.345920
23.043661	1096.848784	15.350938
23.276196	1091.436083	15.355955
23.090542	1078.789330	15.360973
23.177177	1072.529958	15.365991
23.114711	1067.083832	15.371008
22.664592	1076.051408	15.376026
23.314144	1060.197971	15.381043
22.781247	1068.009998	15.386061
22.803366	1060.025546	15.391079
23.016553	1064.158248	15.396096
22.814457	1069.410074	15.401114
22.709807	1061.564720	15.406131
22.880713	1075.239924	15.411149
22.607198	1084.125507	15.416167
23.054181	1086.649474	15.421184
23.060116	1090.114950	15.426202
22.999522	1080.876903	15.431219
23.185334	1093.011517	15.436237
23.232407	1089.940868	15.441255
23.138234	1092.045407	15.446272
23.187204	1092.797153	15.451290
23.438387	1091.969010	15.456307
23.257649	1085.583832	15.461325
23.119259	1091.872326	15.466343
23.345145	1085.693430	15.471360
23.038849	1091.958155	15.476378
23.032432	1086.399989	15.481395
23.179150	1095.914001	15.486413
23.404144	1090.766319	15.491431
23.471836	1103.005538	15.496448
23.370979	1116.194300	15.501466
23.825874	1104.182775	15.506483
23.539651	1101.076372	15.511501
23.258681	1093.517275	15.516519
23.575497	1086.026120	15.521536
23.300176	1100.197664	15.526554
23.645171	1110.588272	15.531571
23.591571	1111.797147	15.536589
23.471290	1117.429130	15.541607
23.556520	1109.791672	15.546624
23.605679	1124.922862	15.551642
23.990892	1127.306282	15.556659
24.061221	1122.158217	15.561677
23.633720	1117.896500	15.566695
24.037763	1116.298578	15.571712
23.861808	1124.982602	15.576730
24.147703	1105.040645	15.581747
24.052311	1094.643429	15.586765
23.728882	1094.663558	15.591783
23.605864	1080.212397	15.596800
23.447321	1088.660454	15.601818
23.801653	1095.107511	15.606835
23.777993	1101.326619	15.611853
24.074622	1110.394571	15.616871
24.256807	1105.389402	15.621888
23.928107	1108.611483	15.626906
24.127950	1113.197575	15.631923
24.490317	1104.603627	15.636941
24.116535	1107.901282	15.641959
24.208224	1115.665419	15.646976
24.049167	1115.645339	15.651994
24.382158	1107.561356	15.657011
24.068436	1112.002180	15.662029
24.311594	1114.408333	15.667047
24.308510	1111.133000	15.672064
24.147063	1107.718935	15.677082
24.174479	1113.709125	15.682099
24.331153	1104.951606	15.687117
24.173985	1110.995587	15.692135
24.232592	1102.248403	15.697152
24.502138	1102.614030	15.702170
24.701750	1109.782753	15.707187
24.524930	1104.791363	15.712205
24.180528	1108.849089	15.717223
24.375688	1099.806468	15.722240
24.082701	1112.685321	15.727258
24.058251	1113.087820	15.732275
23.836354	1107.846814	15.737293
23.971169	1114.035749	15.742311
24.738192	1125.850534	15.747328
24.451903	1135.594534	15.752346
24.580625	1139.216848	15.757363
24.842736	1129.805654	15.762381
24.603519	1138.689919	15.767399
24.830145	1135.538350	15.772416
24.824112	1136.093307	15.777434
24.901726	1140.952001	15.782451
24.997532	1141.521196	15.787469
24.752039	1131.539349	15.792487
25.162934	1130.722551	15.797504
25.390682	1130.654168	15.802522
24.749679	1120.198466	15.807539
24.744645	1103.934888	15.812557
24.737071	1126.274851	15.817575
25.028416	1122.307474	15.822592
24.708394	1128.320951	15.827610
24.788064	1132.934821	15.832627
24.964779	1125.376297	15.837645
25.092133	1130.755476	15.842663
25.321184	1122.015095	15.847680
25.059913	1128.605046	15.852698
25.183017	1129.263025	15.857715
24.922037	1120.107346	15.862733
24.953234	1126.108332	15.867751
25.162917	1127.583839	15.872768
25.302367	1125.794697	15.877786
25.011761	1129.961627	15.882803
25.165633	1119.711696	15.887821
24.566566	1127.339833	15.892839
25.063173	1118.131542	15.897856
24.882868	1130.537434	15.902874
25.266548	1141.304717	15.907891
25.472531	1148.068478	15.912909
25.496668	1157.432752	15.917927
25.754125	1147.741224	15.922944
25.602952	1142.149529	15.927962
25.270265	1123.670568	15.932979
25.316129	1131.043101	15.937997
25.578075	1141.650232	15.943015
25.668084	1143.989626	15.948032
25.987137	1150.013820	15.953050
25.301093	1135.103885	15.958067
25.768343	1135.627715	15.963085
25.713004	1145.207892	15.968103
25.653525	1139.700225	15.973120
25.592852	1146.202637	15.978138
25.472992	1149.921233	15.983155
25.812062	1148.891531	15.988173
25.499996	1147.312187	15.993191
25.725208	1149.811473	15.998208
25.969587	1145.906590	16.003226
25.718438	1149.911878	16.008243
25.911266	1146.317885	16.013261
25.745577	1155.706898	16.018279
25.762525	1142.803717	16.023296
25.687599	1149.859262	16.028314
25.684444	1143.821415	16.033331
26.085235	1144.608605	16.038349
25.646676	1144.338359	16.043367
25.849244	1133.321322	16.048384
25.874389	1149.129326	16.053402
26.356917	1160.303471	16.058419
26.831230	1148.216258	16.063437
26.527372	1149.820502	16.068455
26.237245	1139.550380	16.073472
26.421019	1134.689422	16.078490
26.354467	1139.260186	16.083507
26.521336	1142.797447	16.088525
26.369400	1138.360964	16.093543
26.553127	1135.167287	16.098560
26.404332	1141.914598	16.103578
26.196950	1146.879145	16.108595
26.341864	1129.478932	16.113613
26.105430	1138.925711	16.118631
26.400895	1126.489008	16.123648
26.291800	1138.126445	16.128666
26.155731	1132.606660	16.133683
26.396566	1129.608639	16.138701
26.062718	1129.466326	16.143719
26.413346	1145.040908	16.148736
26.721305	1152.891690	16.153754
26.402941	1168.823523	16.158771
26.765168	1159.172905	16.163789
26.731710	1165.572003	16.168807
26.688020	1163.560434	16.173824
26.731338	1149.282840	16.178842
26.256120	1162.786773	16.183859
26.536687	1163.994648	16.188877
26.912312	1163.058889	16.193895
27.195309	1158.037404	16.198912
26.781431	1161.497216	16.203930
26.812459	1166.479771	16.208947
27.186074	1158.705955	16.213965
26.643423	1160.235177	16.218983
26.716065	1164.339212	16.224000
27.097145	1166.618208	16.229018
26.842412	1166.804516	16.234035
26.923494	1161.627493	16.239053
26.821798	1169.387066	16.244071
26.769854	1166.809163	16.249088
27.058718	1160.229662	16.254106
26.858813	1167.255911	16.259123
26.937870	1157.813596	16.264141
26.797156	1172.403061	16.269159
27.006124	1181.024165	16.274176
27.464565	1180.234924	16.279194
27.218934	1191.179674	16.284211
27.471098	1184.092475	16.289229
27.696373	1182.672569	16.294247
27.627423	1178.759327	16.299264
27.495528	1169.783026	16.304282
27.157869	1152.455609	16.309299
27.206831	1155.133288	16.314317
27.330454	1174.457194	16.319335
27.258993	1186.145520	16.324352
27.494460	1184.269609	16.329370
27.253307	1184.604058	16.334387
27.554087	1181.333117	16.339405
27.503426	1173.621675	16.344423
27.354264	1186.981090	16.349440
27.407275	1182.250429	16.354458
27.276385	1192.475411	16.359475
27.671934	1186.862066	16.364493
27.687406	1187.674481	16.369511
27.773807	1186.874405	16.374528
27.882488	1179.097994	16.379546
27.748061	1183.842210	16.384563
27.933850	1182.627657	16.389581
27.931808	1185.105525	16.394599
27.802657	1187.913488	16.399616
27.684860	1178.938784	16.404634
27.660961	1190.621207	16.409651
27.967252	1200.364759	16.414669
28.288503	1201.151737	16.419687
28.148399	1207.481112	16.424704
28.402622	1181.014942	16.429722
28.166682	1186.521617	16.434739
28.476119	1178.108437	16.439757
28.231728	1177.925719	16.444775
27.738899	1180.164784	16.449792
28.091953	1176.765507	16.454810
27.843441	1190.162241	16.459827
28.089817	1178.772180	16.464845
27.982516	1195.024985	16.469863
28.346411	1208.997477	16.474880
28.322739	1211.089965	16.479898
28.188129	1213.558687	16.484915
28.110720	1210.026749	16.489933
28.159620	1216.626005	16.494951
28.632232	1208.079886	16.499968
28.631611	1202.349069	16.504986
28.581870	1211.417350	16.510003
28.632091	1208.681581	16.515021
28.933743	1206.962813	16.520039
28.476977	1211.950172	16.525056
28.786424	1206.710517	16.530074
28.491727	1211.646631	16.535091
28.724574	1205.771645	16.540109
28.918075	1208.497839	16.545127
28.608444	1212.786442	16.550144
28.633972	1206.014313	16.555162
28.606890	1209.447488	16.560179
28.282843	1211.983798	16.565197
28.473208	1208.300830	16.570215
28.572635	1208.488729	16.575232
28.857629	1203.313753	16.580250
28.843620	1206.388473	16.585267
28.897645	1212.556968	16.590285
28.730665	1209.229621	16.595303
28.463489	1208.177470	16.600320
28.753112	1201.409642	16.605338
28.552600	1227.208383	16.610355
28.979957	1227.928188	16.615373
28.935833	1238.369143	16.620391
28.803438	1231.742834	16.625408
29.090262	1223.795961	16.630426
29.330798	1244.533238	16.635443
29.224898	1238.574965	16.640461
29.704386	1233.325648	16.645479
29.343310	1229.151323	16.650496
29.471437	1231.132459	16.655514
29.242977	1239.013055	16.660531
29.515196	1225.137636	16.665549
29.580321	1223.413939	16.670567
29.505371	1229.228609	16.675584
29.718380	1224.398215	16.680602
29.448485	1228.420800	16.685619
29.319592	1231.472817	16.690637
29.691883	1224.440115	16.695655
29.511613	1232.957989	16.700672
29.884487	1224.722463	16.705690
29.300416	1225.864858	16.710707
29.679458	1234.747981	16.715725
29.999872	1221.503940	16.720743
29.757482	1235.823300	16.725760
29.735704	1224.842166	16.730778
29.831133	1230.451857	16.735795
29.858553	1222.407390	16.740813
29.773564	1221.112871	16.745831
29.768262	1225.980597	16.750848
29.789939	1218.986664	16.755866
29.535002	1225.534269	16.760883
29.672358	1225.965882	16.765901
30.166442	1225.067196	16.770919
29.785008	1223.998137	16.775936
29.571220	1220.806882	16.780954
29.730848	1228.624786	16.785971
29.840741	1217.421071	16.790989
30.033777	1219.896563	16.796007
29.834718	1221.490941	16.801024
30.141021	1225.801570	16.806042
30.052703	1235.289235	16.811059
29.625759	1242.912942	16.816077
30.218551	1238.807434	16.821095
29.923727	1242.656989	16.826112
29.891913	1237.636033	16.831130
30.148664	1243.691446	16.836147
30.197885	1245.023067	16.841165
30.522828	1240.540660	16.846183
30.153041	1246.693915	16.851200
30.302834	1236.253641	16.856218
30.054014	1247.879652	16.861235
30.142882	1262.155207	16.866253
30.255414	1262.575971	16.871271
30.398412	1271.996616	16.876288
30.679326	1272.050923	16.881306
30.565164	1268.725841	16.886323
30.691097	1273.711612	16.891341
31.235596	1263.070926	16.896359
30.877160	1270.197093	16.901376
30.857623	1269.530694	16.906394
30.821739	1254.733452	16.911411
30.475615	1263.930760	16.916429
31.105832	1251.908988	16.921447
31.113262	1255.979358	16.926464
31.367060	1264.278920	16.931482
31.084833	1249.039807	16.936499
30.564796	1230.635046	16.941517
31.166555	1230.803544	16.946535
31.041327	1248.068799	16.951552
31.107288	1246.674481	16.956570
31.258418	1231.021511	16.961587
31.104259	1229.628604	16.966605
31.104327	1218.706454	16.971623
30.747057	1230.124824	16.976640
31.045987	1241.145575	16.981658
31.278791	1250.964319	16.986675
31.182018	1256.044441	16.991693
31.481116	1255.652440	16.996711
31.444765	1261.330813	17.001728
31.244838	1258.817554	17.006746
31.177939	1255.300794	17.011763
30.909769	1256.387733	17.016781
31.000892	1251.622788	17.021799
31.080778	1258.145672	17.026816
31.021218	1251.482098	17.031834
31.244594	1265.382243	17.036851
31.236386	1273.377957	17.041869
31.322782	1272.586933	17.046887
31.234251	1282.078205	17.051904
31.523136	1280.899328	17.056922
31.806593	1276.466299	17.061939
31.682543	1280.787182	17.066957
32.050453	1278.166509	17.071975
31.971042	1273.519950	17.076992
32.054813	1281.171705	17.082010
32.358321	1276.332609	17.087027
31.955065	1274.201827	17.092045
32.120377	1273.091443	17.097063
31.744822	1279.688177	17.102080
32.150947	1276.241114	17.107098
32.300036	1267.188703	17.112115
31.937679	1274.831258	17.117133
32.000117	1270.804899	17.122151
31.981082	1280.856304	17.127168
32.117913	1275.390096	17.132186
32.249756	1272.062466	17.137203
31.676744	1283.220542	17.142221
32.179858	1263.865629	17.147239
31.818772	1271.178451	17.152256
32.081487	1266.607524	17.157274
32.452140	1270.673658	17.162291
31.914455	1268.797809	17.167309
32.558357	1273.354513	17.172327
32.313809	1269.893937	17.177344
32.336163	1273.670901	17.182362
32.199709	1267.131862	17.187379
31.891461	1281.431854	17.192397
32.358516	1288.017804	17.197415
32.591625	1305.985190	17.202432
32.518573	1309.878353	17.207450
32.499516	1306.571766	17.212467
32.729252	1310.201410	17.217485
32.777354	1303.344399	17.222503
32.801651	1293.656743	17.227520
32.954280	1307.299353	17.232538
33.357854	1302.301950	17.237555
33.201260	1298.536652	17.242573
32.990733	1275.413354	17.247591
32.956514	1268.295193	17.252608
32.723403	1265.679162	17.257626
32.867259	1262.324742	17.262643
32.747010	1270.450423	17.267661
33.085307	1287.832666	17.272679
32.863467	1291.414641	17.277696
32.752600	1301.586775	17.282714
33.162168	1296.433659	17.287731
32.877832	1306.386100	17.292749
32.910136	1299.869889	17.297767
33.195402	1300.033710	17.302784
33.304801	1292.131535	17.307802
33.450948	1294.234889	17.312819
33.029284	1294.164593	17.317837
33.271125	1298.266237	17.322855
33.255085	1298.040588	17.327872
33.158862	1292.720836	17.332890
33.398964	1292.761823	17.337907
32.992538	1303.402182	17.342925
33.186906	1293.343064	17.347943
33.065950	1307.961274	17.352960
33.068997	1314.845718	17.357978
33.346528	1316.206073	17.362995
33.472964	1330.956172	17.368013
33.554289	1314.575319	17.373031
33.509628	1318.177174	17.378048
33.425049	1323.910405	17.383066
33.978996	1319.375096	17.388083
33.638277	1322.605116	17.393101
33.660991	1315.315303	17.398119
34.054113	1318.185232	17.403136
33.890193	1314.677043	17.408154
33.908105	1313.068632	17.413171
34.037859	1318.328190	17.418189
33.978818	1321.717076	17.423207
34.350337	1309.492039	17.428224
33.977255	1318.710378	17.433242
34.235148	1325.276648	17.438259
33.967717	1318.858879	17.443277
33.946263	1314.720812	17.448295
34.027852	1317.388787	17.453312
34.130804	1332.967170	17.458330
34.343301	1330.195848	17.463347
34.487878	1350.303105	17.468365
34.917796	1333.454674	17.473383
34.481278	1316.985159	17.478400
34.133123	1319.364457	17.483418
34.366820	1301.371801	17.488435
34.308990	1309.301737	17.493453
34.638988	1316.623767	17.498471
34.374720	1314.021548	17.503488
34.275720	1328.851886	17.508506
34.878126	1329.973019	17.513523
34.599742	1336.003696	17.518541
34.396442	1339.869615	17.523559
34.538104	1336.015158	17.528576
34.326924	1337.792260	17.533594
34.363011	1340.212265	17.538611
34.269050	1346.450199	17.543629
34.339867	1341.845672	17.548647
34.915935	1343.016049	17.553664
34.439126	1356.346006	17.558682
34.897429	1356.433538	17.563699
34.894028	1365.436363	17.568717
35.044557	1368.554341	17.573735
35.262924	1364.545051	17.578752
35.168650	1362.327662	17.583770
35.190533	1363.312250	17.588787
35.143468	1365.773193	17.593805
35.301110	1369.273059	17.598823
35.536632	1348.836776	17.603840
34.937699	1346.003358	17.608858
35.307440	1335.198650	17.613875
35.062271	1333.949542	17.618893
35.350962	1349.016092	17.623911
35.459444	1351.433560	17.628928
35.194667	1363.311114	17.633946
35.453953	1354.060093	17.638963
35.639286	1355.462490	17.643981
35.710695	1357.295163	17.648999
35.393944	1355.772083	17.654016
35.239816	1364.529003	17.659034
35.602137	1362.098609	17.664051
35.298360	1360.367872	17.669069
35.377210	1363.680393	17.674087
35.657162	1360.103814	17.679104
35.446049	1364.965112	17.684122
35.685653	1355.563415	17.689139
35.630449	1361.745725	17.694157
35.690120	1367.015330	17.699175
35.759010	1359.272188	17.704192
35.577187	1365.352240	17.709210
36.143153	1379.284735	17.714227
36.252442	1386.856333	17.719245
35.819449	1384.172594	17.724263
36.160474	1387.544462	17.729280
36.043764	1390.304732	17.734298
36.490796	1382.925730	17.739315
36.493149	1382.890733	17.744333
36.300798	1361.554823	17.749351
35.977488	1358.808045	17.754368
35.667921	1362.660858	17.759386
35.855146	1367.255808	17.764403
36.094264	1382.823112	17.769421
36.388885	1387.313672	17.774439
36.434747	1379.069222	17.779456
36.239715	1384.755018	17.784474
36.256212	1380.507107	17.789491
36.226218	1385.480152	17.794509
36.118284	1374.306882	17.799527
36.688468	1384.401731	17.804544
36.786955	1398.457712	17.809562
36.843020	1406.320413	17.814579
36.755993	1398.543228	17.819597
36.800296	1402.864220	17.824615
37.001730	1387.207093	17.829632
36.887723	1383.319763	17.834650
36.649855	1377.700213	17.839667
36.834872	1389.148588	17.844685
36.628187	1391.444630	17.849703
37.086190	1398.692748	17.854720
36.942262	1409.210973	17.859738
36.884273	1404.945863	17.864755
37.031794	1397.001102	17.869773
37.068321	1401.943846	17.874791
37.124495	1401.670018	17.879808
37.375698	1402.438686	17.884826
37.157584	1395.902090	17.889843
37.376466	1397.813103	17.894861
37.258220	1400.348435	17.899879
37.569951	1402.514149	17.904896
37.488908	1407.351168	17.909914
37.301841	1395.226430	17.914931
37.581474	1393.094759	17.919949
37.000472	1405.489268	17.924967
37.094912	1399.848936	17.929984
37.205783	1401.837675	17.935002
37.197572	1398.358015	17.940019
37.535963	1402.219292	17.945037
37.371876	1399.278821	17.950055
37.546129	1396.108707	17.955072
37.520758	1401.729015	17.960090
37.657741	1412.940089	17.965107
37.894018	1414.959640	17.970125
37.840204	1426.689713	17.975143
38.078331	1416.977990	17.980160
38.361372	1412.235153	17.985178
37.926065	1394.874026	17.990195
37.957533	1388.032724	17.995213
37.796550	1393.142026	18.000231
38.284866	1390.816354	18.005248
38.019845	1387.433156	18.010266
37.870671	1386.767352	18.015283
38.031117	1398.779245	18.020301
37.857892	1416.378614	18.025319
38.306835	1419.503489	18.030336
38.400787	1423.850911	18.035354
38.570146	1425.545721	18.040371
38.469524	1414.451131	18.045389
38.203312	1420.205811	18.050407
38.407417	1419.955125	18.055424
38.189074	1421.735785	18.060442
38.318877	1420.230488	18.065459
38.589055	1428.600260	18.070477
38.459376	1408.280669	18.075495
38.591848	1417.399212	18.080512
38.633308	1421.564777	18.085530
38.900781	1413.308417	18.090547
38.958312	1419.269723	18.095565
38.781415	1417.561277	18.100583
38.804243	1409.781250	18.105600
38.885882	1411.739792	18.110618
38.743241	1420.944443	18.115635
38.677653	1425.002538	18.120653
38.703555	1417.029481	18.125671
39.017932	1418.697521	18.130688
38.756176	1422.800697	18.135706
38.967224	1420.003221	18.140723
39.110920	1418.173580	18.145741
38.714610	1422.075810	18.150759
39.230310	1435.338734	18.155776
38.997434	1445.746517	18.160794
39.062107	1447.265358	18.165811
39.459626	1444.766526	18.170829
39.179791	1450.753392	18.175847
39.423170	1443.290762	18.180864
39.245265	1446.297787	18.185882
39.190098	1435.204710	18.190899
39.334928	1434.528017	18.195917
39.156827	1438.787422	18.200935
39.572767	1433.250140	18.205952
39.650404	1430.432628	18.210970
39.554107	1433.509207	18.215987
39.282317	1426.986210	18.221005
39.574782	1455.160760	18.226023
39.870200	1460.365770	18.231040
39.901039	1467.233082	18.236058
40.048386	1463.061907	18.241075
40.147726	1441.389795	18.246093
39.837199	1441.265268	18.251111
40.069864	1426.442292	18.256128
39.769151	1429.941690	18.261146
40.063157	1453.869180	18.266163
40.176670	1449.944159	18.271181
40.084510	1443.882351	18.276199
40.030089	1434.847398	18.281216
40.197138	1440.045311	18.286234
39.936419	1454.373419	18.291251
40.369859	1451.339902	18.296269
40.460688	1455.956352	18.301287
40.352803	1450.762492	18.306304
40.656979	1456.412109	18.311322
40.272629	1464.189105	18.316339
40.319551	1454.340123	18.321357
40.331826	1462.867185	18.326375
40.583822	1454.787379	18.331392
40.468122	1462.071863	18.336410
40.388335	1464.366194	18.341427
40.486461	1453.463468	18.346445
40.338518	1461.770604	18.351463
40.755512	1455.915425	18.356480
40.679814	1448.826883	18.361498
40.565245	1449.295493	18.366515
40.613566	1442.427755	18.371533
40.686452	1450.954222	18.376551
40.840870	1463.174247	18.381568
41.010404	1468.435144	18.386586
40.864337	1475.174273	18.391603
40.970043	1466.498611	18.396621
40.999015	1466.627314	18.401639
40.894134	1467.084085	18.406656
41.056309	1473.930046	18.411674
40.847596	1475.783132	18.416691
40.639802	1465.401915	18.421709
40.916744	1476.922535	18.426727
41.135762	1482.777600	18.431744
41.516617	1492.142853	18.436762
41.529612	1506.595370	18.441779
41.582476	1497.309546	18.446797
41.425289	1497.302147	18.451815
41.614807	1499.388112	18.456832
41.642703	1497.002050	18.461850
41.474398	1502.041341	18.466867
41.503692	1495.623971	18.471885
41.585620	1489.812844	18.476903
41.868921	1493.295081	18.481920
41.900494	1484.062791	18.486938
41.887142	1495.707477	18.491955
42.062966	1497.177997	18.496973
41.873585	1496.204675	18.501991
41.824407	1493.573503	18.507008
42.169476	1488.606201	18.512026
41.758545	1490.416001	18.517043
41.702083	1490.531292	18.522061
41.750218	1493.193026	18.527079
41.807769	1488.922934	18.532096
42.525442	1508.991408	18.537114
42.119703	1507.397614	18.542131
42.407537	1505.607876	18.547149
42.816414	1502.811487	18.552167
42.465669	1502.712516	18.557184
42.436954	1481.193047	18.562202
42.340302	1483.848832	18.567219
42.625327	1486.315042	18.572237
42.632905	1487.928379	18.577255
42.116970	1483.023332	18.582272
42.578570	1490.582708	18.587290
42.382433	1501.120270	18.592307
42.447931	1504.260624	18.597325
42.752000	1504.018975	18.602343
42.860681	1516.347009	18.607360
43.110677	1508.432467	18.612378
42.829493	1505.931047	18.617395
43.203346	1512.200640	18.622413
43.061972	1513.101641	18.627431
42.769806	1512.891396	18.632448
42.909665	1508.589953	18.637466
42.905288	1504.402551	18.642483
42.993697	1513.964272	18.647501
42.860766	1512.278456	18.652519
43.086231	1515.703345	18.657536
43.313473	1503.045356	18.662554
43.313972	1512.196438	18.667571
43.261923	1501.479961	18.672589
43.080244	1517.850931	18.677607
42.989155	1504.743291	18.682624
43.170145	1506.999567	18.687642
43.324366	1526.855458	18.692659
43.634731	1528.556852	18.697677
43.728725	1539.540492	18.702695
43.515997	1537.905681	18.707712
43.765985	1532.557260	18.712730
43.672781	1541.148287	18.717747
43.612788	1531.624438	18.722765
43.437442	1529.153915	18.727783
43.293851	1535.965101	18.732800
43.809634	1535.094303	18.737818
43.607331	1538.709320	18.742835
43.422084	1538.803417	18.747853
43.584852	1538.056033	18.752871
43.870276	1555.546545	18.757888
44.479429	1553.511471	18.762906
44.103018	1567.741517	18.767923
44.459949	1562.346244	18.772941
44.371438	1559.360550	18.777959
43.911201	1568.905278	18.782976
44.354438	1553.915424	18.787994
43.981271	1557.170155	18.793011
44.134837	1550.279037	18.798029
44.218241	1551.800299	18.803047
44.225467	1555.860939	18.808064
44.287728	1543.180628	18.813082
44.641619	1559.929496	18.818099
44.812321	1568.528414	18.823117
44.723759	1562.431712	18.828135
45.254529	1554.485222	18.833152
45.247115	1543.419987	18.838170
45.184982	1543.833855	18.843187
45.355682	1542.233192	18.848205
44.983311	1544.279526	18.853223
45.093227	1548.679065	18.858240
45.362098	1540.871223	18.863258
45.101810	1542.416716	18.868275
45.338556	1542.148419	18.873293
45.237067	1530.447199	18.878311
45.005914	1543.332310	18.883328
45.135777	1537.598661	18.888346
45.071296	1538.701497	18.893363
45.091178	1538.892730	18.898381
45.007540	1541.598338	18.903399
44.725663	1542.692683	18.908416
45.293513	1535.323920	18.913434
45.031082	1536.609138	18.918451
45.015139	1556.323166	18.923469
45.322490	1564.191189	18.928487
45.510608	1574.144704	18.933504
45.420942	1569.402116	18.938522
45.547593	1571.723698	18.943539
45.562183	1558.887489	18.948557
45.707486	1557.820556	18.953575
45.637873	1573.713976	18.958592
45.917621	1564.413773	18.963610
45.686381	1562.124546	18.968627
45.793925	1563.103230	18.973645
45.614900	1557.911664	18.978663
46.085847	1583.212808	18.983680
45.983777	1585.464390	18.988698
46.074106	1592.756158	18.993715
46.454392	1591.203070	18.998733
46.559950	1582.755321	19.003751
46.558359	1583.912707	19.008768
46.435267	1552.964683	19.013786
46.076698	1561.201236	19.018803
45.959125	1554.417610	19.023821
46.064203	1568.061633	19.028839
46.262940	1588.394483	19.033856
46.371970	1595.731188	19.038874
46.317491	1592.520562	19.043891
46.198176	1593.159254	19.048909
46.598808	1582.780756	19.053927
46.267079	1594.673509	19.058944
46.556489	1602.303578	19.063962
46.813305	1609.256370	19.068979
46.553519	1610.037219	19.073997
47.042627	1609.419654	19.079015
46.921595	1620.949193	19.084032
47.083375	1612.138968	19.089050
47.281933	1619.670703	19.094067
47.237448	1616.304086	19.099085
47.467472	1608.049099	19.104103
47.568877	1615.780384	19.109120
47.112264	1607.385549	19.114138
47.590801	1606.205167	19.119155
47.241589	1613.971695	19.124173
47.458099	1609.928398	19.129191
47.494058	1613.823272	19.134208
47.547944	1603.628160	19.139226
47.252534	1611.190108	19.144243
47.413874	1608.787838	19.149261
47.515747	1607.519038	19.154279
47.656096	1615.554898	19.159296
47.668822	1616.704798	19.164314
47.862703	1607.407370	19.169331
47.359122	1615.328593	19.174349
47.580696	1613.498239	19.179367
47.427568	1615.622452	19.184384
47.471639	1627.314028	19.189402
47.882326	1639.972076	19.194419
47.993032	1642.220324	19.199437
48.114072	1641.885751	19.204455
47.615057	1650.220410	19.209472
48.226352	1644.323540	19.214490
48.169359	1642.689309	19.219507
48.061708	1637.769757	19.224525
48.050874	1635.713709	19.229543
47.752945	1644.220187	19.234560
47.969420	1667.655332	19.239578
48.277287	1667.733133	19.244595
48.373218	1679.933880	19.249613
48.361367	1668.894488	19.254631
48.182144	1672.607682	19.259648
48.436499	1674.683330	19.264666
48.469800	1673.038082	19.269683
48.179485	1674.154305	19.274701
48.650468	1679.959063	19.279719
49.145618	1686.778725	19.284736
49.170294	1694.056609	19.289754
49.344814	1689.224571	19.294771
48.604432	1676.777842	19.299789
49.338688	1668.577522	19.304807
49.046858	1672.303851	19.309824
49.285349	1680.242391	19.314842
49.293737	1656.712981	19.319859
49.124676	1653.001235	19.324877
49.343224	1660.543066	19.329895
49.528651	1670.116771	19.334912
49.500291	1667.828187	19.339930
49.740930	1653.059974	19.344947
49.245178	1654.212575	19.349965
49.312488	1651.741223	19.354983
49.283029	1664.509966	19.360000
49.283171	1671.970643	19.365018
49.816127	1677.314743	19.370035
49.475680	1684.231030	19.375053
49.492951	1675.623439	19.380071
49.652693	1681.703356	19.385088
49.801812	1679.324753	19.390106
49.815767	1672.872054	19.395123
49.498373	1688.227482	19.400141
49.898927	1680.529657	19.405159
50.246668	1671.857505	19.410176
49.923892	1677.827159	19.415194
50.125961	1683.871722	19.420211
50.190323	1703.725397	19.425229
50.436359	1707.248893	19.430247
50.821045	1697.448948	19.435264
50.280172	1685.645166	19.440282
50.202683	1669.463464	19.445299
50.200328	1679.432050	19.450317
50.330143	1697.055575	19.455335
50.387268	1693.116602	19.460352
50.341176	1701.112117	19.465370
50.545030	1692.653544	19.470387
50.396074	1704.077531	19.475405
50.731732	1699.363297	19.480423
50.720315	1688.304528	19.485440
50.518972	1694.279278	19.490458
51.011555	1689.050871	19.495475
50.928823	1702.496975	19.500493
50.987025	1689.591231	19.505511
50.604007	1698.823249	19.510528
50.866400	1712.641352	19.515546
51.174292	1713.326634	19.520563
50.884570	1719.915245	19.525581
51.150329	1723.213430	19.530599
51.241478	1722.251910	19.535616
51.006764	1723.302237	19.540634
51.114997	1714.950430	19.545651
51.048614	1725.628866	19.550669
51.657172	1732.188036	19.555687
51.959213	1745.569284	19.560704
52.060174	1727.508744	19.565722
51.878394	1715.321067	19.570739
51.486822	1715.187515	19.575757
51.623630	1711.692433	19.580775
51.690327	1715.573975	19.585792
51.637754	1726.691072	19.590810
52.031522	1727.052291	19.595827
52.098262	1748.405248	19.600845
52.034816	1744.428351	19.605863
52.575113	1737.068387	19.610880
52.416294	1718.471339	19.615898
52.459481	1713.647259	19.620915
51.864299	1722.896705	19.625933
51.964125	1711.977768	19.630951
52.101265	1706.067654	19.635968
52.049999	1728.279499	19.640986
52.194925	1731.620135	19.646003
52.350776	1734.989277	19.651021
52.205241	1743.460339	19.656039
52.249789	1744.227417	19.661056
51.747219	1741.347650	19.666074
52.267474	1738.843411	19.671091
52.083470	1758.084731	19.676109
52.484013	1760.618079	19.681127
52.729207	1760.001921	19.686144
52.338524	1764.897014	19.691162
53.132801	1756.662300	19.696179
53.054842	1763.831619	19.701197
53.121248	1769.109301	19.706215
53.090733	1759.243026	19.711232
53.485876	1766.134402	19.716250
53.371365	1755.341082	19.721267
53.354668	1759.615188	19.726285
53.323128	1751.619973	19.731303
53.332272	1756.921699	19.736320
52.855531	1758.271948	19.741338
53.279606	1761.506919	19.746355
53.200467	1783.856925	19.751373
53.356863	1792.141797	19.756391
53.496747	1791.643469	19.761408
53.380724	1789.517416	19.766426
53.689093	1784.385623	19.771443
53.524435	1795.998500	19.776461
53.594726	1785.825356	19.781479
53.992945	1785.507485	19.786496
53.724334	1785.292940	19.791514
54.019499	1785.500013	19.796531
54.182103	1797.772491	19.801549
53.959342	1803.665395	19.806567
54.400949	1811.911320	19.811584
54.491236	1813.216111	19.816602
54.672307	1792.726843	19.821619
54.348693	1787.196537	19.826637
54.372349	1781.034317	19.831655
54.636084	1771.143328	19.836672
54.148951	1783.131642	19.841690
54.295524	1778.876258	19.846707
54.553209	1796.329509	19.851725
54.387781	1798.585313	19.856743
54.671058	1808.832282	19.861760
54.573639	1810.726822	19.866778
54.883649	1811.083014	19.871795
54.913637	1815.416728	19.876813
54.582199	1801.013970	19.881831
54.963013	1812.082203	19.886848
54.292572	1821.183536	19.891866
54.838083	1814.545517	19.896883
55.375475	1826.268946	19.901901
54.991536	1823.488027	19.906919
55.523418	1824.746471	19.911936
55.358858	1828.554521	19.916954
55.499994	1825.523664	19.921971
55.518173	1811.076393	19.926989
55.330733	1807.139696	19.932007
54.976567	1804.210541	19.937024
54.964239	1824.826292	19.942042
55.368816	1829.547599	19.947059
55.300807	1832.483350	19.952077
55.540444	1835.189026	19.957095
55.875559	1823.341667	19.962112
55.777254	1834.549486	19.967130
55.694649	1822.926809	19.972147
55.853713	1831.955366	19.977165
55.614306	1828.944999	19.982183
55.993758	1837.935887	19.987200
55.789178	1855.183065	19.992218
56.129166	1860.507605	19.997235
56.256261	1856.748741	20.002253
56.137996	1858.974303	20.007271
56.328774	1856.943899	20.012288
56.373181	1855.695224	20.017306
56.557820	1855.314289	20.022323
56.293724	1850.485929	20.027341
56.168755	1858.403639	20.032359
56.130497	1848.150000	20.037376
56.448347	1856.404236	20.042394
56.796205	1867.984668	20.047411
56.883797	1878.157390	20.052429
56.820664	1879.761610	20.057447
57.072081	1877.061309	20.062464
57.018460	1875.094992	20.067482
56.818469	1873.907650	20.072499
57.345254	1878.433931	20.077517
57.342306	1874.950536	20.082535
57.343647	1860.185922	20.087552
57.234900	1855.324751	20.092570
57.344185	1827.526337	20.097587
57.109775	1846.917847	20.102605
57.300325	1856.716809	20.107623
57.499579	1866.719850	20.112640
57.143709	1872.106858	20.117658
57.293722	1871.890714	20.122675
57.654459	1869.382159	20.127693
57.349271	1878.656909	20.132711
57.491972	1873.257631	20.137728
57.342528	1874.250541	20.142746
57.923318	1874.763477	20.147763
57.813381	1885.736247	20.152781
57.920200	1888.143839	20.157799
58.037018	1887.520586	20.162816
57.830506	1893.660050	20.167834
57.929386	1884.180152	20.172851
57.666263	1891.267589	20.177869
57.611693	1889.145126	20.182887
57.894808	1886.253351	20.187904
58.054291	1902.942653	20.192922
57.966813	1917.196043	20.197939
58.254287	1913.759829	20.202957
58.118995	1921.373369	20.207975
58.672271	1911.278834	20.212992
58.680780	1913.716095	20.218010
58.728850	1920.311851	20.223027
58.754288	1912.406334	20.228045
58.549386	1912.598570	20.233063
59.010287	1924.475293	20.238080
58.912208	1932.148426	20.243098
59.396530	1939.155431	20.248115
59.419328	1908.143959	20.253133
59.253646	1906.949752	20.258151
59.265318	1901.405621	20.263168
59.212257	1900.185680	20.268186
59.304319	1904.225278	20.273203
59.501543	1899.769344	20.278221
58.829346	1900.662588	20.283239
59.272050	1905.989429	20.288256
59.213556	1925.118833	20.293274
59.534337	1926.390980	20.298291
59.479127	1929.063208	20.303309
59.684096	1934.239261	20.308327
59.577928	1929.612683	20.313344
59.897401	1932.867374	20.318362
59.423334	1928.543450	20.323379
59.913736	1916.136046	20.328397
59.576171	1926.945744	20.333415
59.700789	1928.536599	20.338432
59.788975	1933.667026	20.343450
59.730145	1949.477941	20.348467
60.174190	1954.690400	20.353485
59.854525	1959.745845	20.358503
59.930028	1954.433259	20.363520
59.736030	1957.235954	20.368538
60.376334	1975.696945	20.373555
60.809466	1985.648346	20.378573
60.948422	1980.187052	20.383591
60.827433	1973.140415	20.388608
61.009218	1962.740815	20.393626
60.688277	1948.040505	20.398643
61.112781	1942.363829	20.403661
60.808860	1949.710416	20.408679
60.896938	1937.784187	20.413696
60.913392	1954.014934	20.418714
60.829121	1971.061213	20.423731
61.022410	1964.916109	20.428749
60.942904	1973.786215	20.433767
61.189658	1980.072714	20.438784
61.393926	1977.065628	20.443802
60.998922	1979.228365	20.448819
61.514141	1972.597659	20.453837
61.224840	1980.114677	20.458855
61.211883	1975.532496	20.463872
60.967215	1974.742316	20.468890
61.546229	1990.720894	20.473907
61.667791	1989.291713	20.478925
61.567329	2000.892145	20.483943
61.498333	2000.535487	20.488960
61.681871	2002.468571	20.493978
61.690703	1999.952120	20.498995
62.068555	2009.474883	20.504013
62.280735	2015.529320	20.509031
62.228942	2001.224170	20.514048
62.450753	1999.065378	20.519066
62.146618	1995.251895	20.524083
62.277850	1993.841191	20.529101
62.390365	2013.455394	20.534119
62.467079	2015.559321	20.539136
62.414006	2016.587859	20.544154
62.722086	2018.934587	20.549171
62.604799	2013.931469	20.554189
62.788148	2017.427620	20.559207
63.063635	2014.945757	20.564224
62.960262	2023.301719	20.569242
63.024712	2021.664662	20.574259
62.930497	2011.680424	20.579277
62.940165	2019.696398	20.584295
62.758761	2013.935765	20.589312
63.016234	2016.422766	20.594330
63.034951	2015.831893	20.599347
63.231085	2010.162691	20.604365
62.925998	2016.400810	20.609383
63.227857	2016.057158	20.614400
63.203518	2032.228203	20.619418
63.174401	2040.330534	20.624435
63.410028	2047.216558	20.629453
63.347794	2052.558551	20.634471
63.787269	2054.824078	20.639488
63.545779	2043.789370	20.644506
63.731301	2052.925884	20.649523
63.887252	2049.462991	20.654541
63.816443	2045.154549	20.659559
63.965410	2039.517162	20.664576
63.789397	2044.401206	20.669594
63.906970	2052.525319	20.674611
64.119616	2064.893664	20.679629
63.802127	2069.191280	20.684647
63.890999	2075.835860	20.689664
64.186404	2074.110949	20.694682
64.140077	2069.701200	20.699699
64.328690	2064.587177	20.704717
64.668690	2069.920844	20.709735
64.633159	2076.260422	20.714752
64.483142	2072.690307	20.719770
64.741734	2088.156276	20.724787
65.391354	2087.110926	20.729805
65.263452	2082.880827	20.734823
64.851069	2082.021558	20.739840
64.770971	2062.764585	20.744858
65.044214	2077.080839	20.749875
65.112825	2086.043023	20.754893
65.491727	2082.504623	20.759911
65.305899	2080.571589	20.764928
65.482821	2079.142289	20.769946
65.497194	2090.554476	20.774963
65.440820	2077.767779	20.779981
65.375510	2077.243574	20.784999
65.551045	2080.466222	20.790016
65.871750	2070.071502	20.795034
65.541160	2081.137639	20.800051
65.709825	2066.705766	20.805069
65.711501	2073.438013	20.810087
65.477113	2077.152563	20.815104
66.043468	2091.288010	20.820122
66.179476	2107.521563	20.825139
66.083459	2097.713558	20.830157
66.171196	2110.545155	20.835175
66.200133	2105.311490	20.840192
66.224991	2108.172859	20.845210
66.541315	2103.142405	20.850227
66.493025	2103.618957	20.855245
66.648008	2102.903153	20.860263
66.470462	2104.364524	20.865280
66.796582	2097.248918	20.870298
66.865272	2097.800986	20.875315
67.045194	2095.334934	20.880333
66.839219	2096.180125	20.885351
66.833275	2101.062800	20.890368
66.802792	2096.245288	20.895386
66.837426	2100.559809	20.900403
66.793310	2091.523554	20.905421
67.129349	2107.648394	20.910439
66.984101	2122.362733	20.915456
67.572226	2122.657530	20.920474
67.106334	2136.209578	20.925491
67.395918	2127.049543	20.930509
67.394376	2126.219099	20.935527
67.469169	2129.960817	20.940544
67.604091	2121.371689	20.945562
67.438293	2127.037952	20.950579
67.440563	2120.112970	20.955597
67.498674	2130.315149	20.960615
68.055663	2138.559863	20.965632
67.775068	2147.539744	20.970650
68.046332	2151.787145	20.975667
67.901781	2146.945983	20.980685
68.249953	2154.897317	20.985703
68.101308	2153.071901	20.990720
68.450584	2146.594193	20.995738
68.163279	2154.577517	21.000755
68.448398	2156.968621	21.005773
68.374873	2149.436469	21.010791
68.176579	2148.526392	21.015808
68.501662	2145.218945	21.020826
68.317751	2163.976482	21.025843
68.591128	2175.548217	21.030861
68.698162	2171.900082	21.035879
68.575348	2173.032307	21.040896
69.087114	2178.045828	21.045914
69.086545	2184.991102	21.050931
68.763240	2179.269652	21.055949
69.010492	2176.208559	21.060967
69.075163	2180.298828	21.065984
69.678103	2186.221306	21.071002
69.460764	2198.219992	21.076019
69.814761	2195.437295	21.081037
69.855354	2188.809886	21.086055
69.514887	2187.404036	21.091072
69.659290	2167.958968	21.096090
70.068200	2188.175520	21.101107
69.750034	2180.087380	21.106125
69.787390	2184.423521	21.111143
69.765562	2187.540283	21.116160
69.949150	2193.877094	21.121178
70.047251	2186.862984	21.126195
70.208625	2190.500614	21.131213
70.351451	2190.030135	21.136231
69.942774	2202.352248	21.141248
70.187357	2186.435983	21.146266
70.332992	2201.800685	21.151283
70.207053	2200.012450	21.156301
70.334040	2208.869760	21.161319
70.390441	2226.767077	21.166336
70.745195	2229.219107	21.171354
70.391861	2224.660926	21.176371
70.583938	2223.877161	21.181389
70.791289	2228.972601	21.186407
70.326986	2230.218855	21.191424
70.653060	2236.578550	21.196442
70.855703	2244.342994	21.201459
71.227073	2231.826304	21.206477
71.335781	2229.790150	21.211495
71.449607	2231.800951	21.216512
71.784305	2232.431818	21.221530
71.682317	2231.666427	21.226547
71.838694	2231.396468	21.231565
71.669333	2229.059884	21.236583
71.260998	2233.206438	21.241600
71.751372	2223.443787	21.246618
71.653057	2237.523667	21.251635
71.737066	2241.656422	21.256653
71.985413	2257.353793	21.261671
71.922425	2260.325015	21.266688
72.001266	2251.558479	21.271706
71.908215	2265.316632	21.276723
72.038810	2261.375194	21.281741
72.235213	2256.270842	21.286759
72.323518	2262.825042	21.291776
72.196010	2259.903546	21.296794
72.627436	2273.761489	21.301811
72.530770	2282.153095	21.306829
72.751542	2288.604266	21.311847
72.640128	2287.130165	21.316864
72.782306	2280.309117	21.321882
72.934751	2276.748719	21.326899
72.809572	2276.356867	21.331917
73.253092	2269.979651	21.336935
73.198222	2279.467138	21.341952
73.326362	2271.910985	21.346970
73.327414	2264.599116	21.351987
72.951486	2276.724911	21.357005
73.357842	2266.379662	21.362023
73.183954	2276.322306	21.367040
73.395494	2272.206038	21.372058
73.290046	2277.318244	21.377075
73.129137	2301.083774	21.382093
73.842060	2301.446499	21.387111
74.029304	2304.481814	21.392128
73.965132	2302.549475	21.397146
73.869274	2309.714923	21.402163
74.042651	2303.144616	21.407181
74.098090	2302.090545	21.412199
74.176298	2307.041244	21.417216
74.251807	2289.291760	21.422234
74.385162	2295.522359	21.427251
74.211200	2296.965043	21.432269
74.326552	2307.509845	21.437287
74.418390	2315.728912	21.442304
74.589056	2317.413369	21.447322
74.686377	2319.239897	21.452339
74.453967	2319.619377	21.457357
74.550204	2317.664807	21.462375
74.895572	2321.912978	21.467392
74.816952	2335.492024	21.472410
75.125584	2344.052788	21.477427
74.738032	2345.400914	21.482445
75.192173	2338.885685	21.487463
75.003146	2348.161164	21.492480
75.378181	2343.182333	21.497498
75.256510	2340.022443	21.502515
74.965921	2353.603136	21.507533
75.678284	2362.799458	21.512551
75.458567	2367.865651	21.517568
75.800720	2366.462906	21.522586
76.011869	2363.262079	21.527603
76.040853	2366.571260	21.532621
76.332954	2363.347186	21.537639
76.119719	2372.305018	21.542656
76.198507	2367.767376	21.547674
76.301087	2358.755892	21.552691
76.222807	2364.163643	21.557709
76.553466	2361.520222	21.562727
76.067636	2369.365650	21.567744
76.231729	2371.922505	21.572762
76.951619	2384.553986	21.577779
76.755946	2395.444848	21.582797
77.249908	2393.825618	21.587815
77.247825	2385.203120	21.592832
77.146542	2361.038014	21.597850
77.164851	2358.038416	21.602867
77.084313	2359.530995	21.607885
77.323662	2338.003751	21.612903
77.067662	2353.868196	21.617920
77.269907	2372.134465	21.622938
77.744228	2382.255691	21.627955
77.686050	2385.430875	21.632973
77.734807	2382.063615	21.637991
77.739854	2383.689276	21.643008
77.904068	2372.032013	21.648026
77.776929	2360.889164	21.653043
77.498969	2353.414779	21.658061
77.794173	2363.990473	21.663079
77.920233	2381.437438	21.668096
77.555399	2377.696510	21.673114
77.988908	2377.735405	21.678131
77.853473	2378.842960	21.683149
78.238203	2377.362690	21.688167
77.995186	2382.484323	21.693184
78.268445	2403.506727	21.698202
78.297800	2398.121705	21.703219
78.329884	2411.246639	21.708237
78.160408	2400.463152	21.713255
78.440685	2405.911161	21.718272
78.307443	2413.901392	21.723290
78.686082	2416.866849	21.728307
78.405280	2431.715347	21.733325
78.753815	2421.130344	21.738343
78.786371	2428.278914	21.743360
78.941470	2440.479912	21.748378
79.301447	2450.513022	21.753395
79.700946	2459.352128	21.758413
79.806599	2459.242935	21.763431
79.981618	2464.227264	21.768448
79.778003	2462.748332	21.773466
79.878971	2463.357670	21.778483
80.116956	2456.183263	21.783501
80.011293	2442.957944	21.788519
80.103591	2437.408935	21.793536
79.939913	2429.478953	21.798554
80.451416	2439.250341	21.803571
80.060785	2447.955290	21.808589
80.268552	2455.946958	21.813607
80.410325	2447.516367	21.818624
80.428270	2459.261323	21.823642
80.345530	2449.576101	21.828659
80.438994	2458.686362	21.833677
80.651106	2449.410219	21.838695
80.415359	2452.601432	21.843712
80.379102	2450.308133	21.848730
80.731349	2462.491074	21.853747
80.433385	2477.983045	21.858765
80.557044	2477.542111	21.863783
80.865052	2474.308294	21.868800
80.844233	2488.173589	21.873818
81.569007	2490.883312	21.878835
81.524887	2500.822724	21.883853
81.583756	2506.695246	21.888871
81.615516	2500.538486	21.893888
81.401817	2504.446572	21.898906
81.775705	2493.731724	21.903923
81.654340	2497.756812	21.908941
82.079214	2496.223031	21.913959
81.995759	2497.029058	21.918976
81.817724	2509.414804	21.923994
81.940535	2494.473561	21.929011
81.760677	2496.066067	21.934029
82.090533	2511.559244	21.939047
81.919308	2521.759099	21.944064
82.352002	2529.908062	21.949082
82.548606	2527.228538	21.954099
82.502720	2529.159123	21.959117
82.375117	2525.572592	21.964135
82.528773	2526.568903	21.969152
82.824907	2542.766162	21.974170
83.004318	2534.244642	21.979187
83.204861	2546.011008	21.984205
83.343957	2538.449761	21.989223
83.383376	2542.695498	21.994240
83.298810	2546.619224	21.999258
83.582538	2546.690795	22.004275
83.673364	2538.910362	22.009293
83.624258	2533.599705	22.014311
83.594790	2517.670994	22.019328
83.149233	2531.444045	22.024346
83.580801	2535.403577	22.029363
83.596930	2542.882893	22.034381
83.509382	2535.855661	22.039399
83.778217	2543.820726	22.044416
83.605770	2551.883271	22.049434
83.768621	2557.767338	22.054451
83.906303	2574.198752	22.059469
84.165297	2570.603716	22.064487
83.995130	2576.008644	22.069504
83.988498	2567.421053	22.074522
83.980513	2581.296117	22.079539
84.588092	2593.827068	22.084557
84.627725	2598.068059	22.089575
84.755448	2589.082990	22.094592
84.599013	2587.714352	22.099610
84.858730	2584.301882	22.104627
84.783902	2600.580309	22.109645
84.927452	2614.659461	22.114663
85.451544	2613.353746	22.119680
85.159589	2623.236626	22.124698
85.249721	2624.002894	22.129715
85.461713	2619.384459	22.134733
85.556097	2621.204423	22.139751
85.410875	2615.603333	22.144768
85.535480	2632.074377	22.149786
85.990754	2635.688255	22.154803
85.836516	2645.182181	22.159821
85.923162	2644.852103	22.164839
86.293248	2646.768950	22.169856
86.134163	2642.076900	22.174874
86.185962	2642.556583	22.179891
86.381643	2645.588993	22.184909
86.380102	2641.727609	22.189927
86.621040	2635.035341	22.194944
86.942092	2644.108422	22.199962
86.732425	2626.110870	22.204979
86.611113	2642.808482	22.209997
86.512560	2656.758062	22.215015
87.050433	2655.470536	22.220032
86.955630	2662.941109	22.225050
87.108957	2672.417988	22.230067
87.279728	2665.190829	22.235085
87.095789	2675.988206	22.240103
87.151892	2666.120794	22.245120
87.256948	2671.387659	22.250138
87.376568	2687.122528	22.255155
87.256546	2690.382822	22.260173
87.258542	2703.966559	22.265191
87.928027	2691.613151	22.270208
87.525052	2694.595469	22.275226
87.623920	2708.441931	22.280243
88.074856	2720.549282	22.285261
88.237151	2730.792089	22.290279
88.265285	2720.881239	22.295296
88.658382	2714.254301	22.300314
88.309728	2717.219361	22.305331
88.450191	2715.409399	22.310349
88.677026	2718.607151	22.315367
88.722960	2709.954081	22.320384
88.604521	2719.106667	22.325402
88.765718	2707.410674	22.330419
89.073937	2707.229749	22.335437
88.812776	2719.882592	22.340455
89.187346	2724.744195	22.345472
89.191643	2730.217147	22.350490
89.156816	2742.979395	22.355507
89.573122	2733.246017	22.360525
89.339187	2741.965344	22.365543
89.730084	2740.111158	22.370560
89.562804	2737.145760	22.375578
89.506564	2733.072921	22.380595
89.995383	2731.646650	22.385613
89.908253	2734.824336	22.390631
90.020011	2733.767605	22.395648
89.707925	2726.295933	22.400666
90.264665	2737.903461	22.405683
90.299290	2761.535735	22.410701
90.238471	2775.244117	22.415719
90.288478	2755.317058	22.420736
90.144995	2756.482669	22.425754
89.972735	2759.308680	22.430771
90.273017	2762.065115	22.435789
90.526853	2781.609640	22.440807
90.339407	2785.594164	22.445824
90.380404	2799.254210	22.450842
90.594758	2797.604852	22.455859
90.580677	2812.900926	22.460877
90.939703	2814.687333	22.465895
91.143634	2805.546597	22.470912
91.743695	2820.417741	22.475930
91.694271	2820.848829	22.480947
91.576097	2824.174992	22.485965
91.788394	2844.303685	22.490983
92.277424	2825.822866	22.496000
92.190000	2831.198432	22.501018
92.155982	2829.496486	22.506035
92.348507	2824.244156	22.511053
92.488305	2829.826214	22.516071
92.963537	2821.728036	22.521088
92.802844	2812.604750	22.526106
92.618792	2797.569526	22.531123
92.921961	2786.230706	22.536141
92.870538	2788.093336	22.541159
92.799263	2780.325054	22.546176
92.595779	2794.093297	22.551194
92.668676	2805.030928	22.556211
92.464115	2806.716932	22.561229
92.459992	2823.511485	22.566247
93.007028	2826.392049	22.571264
92.965580	2839.775207	22.576282
93.174697	2855.633235	22.581299
93.295497	2855.872347	22.586317
93.440513	2854.026967	22.591335
93.356856	2855.129526	22.596352
93.292108	2862.031787	22.601370
93.657590	2869.035272	22.606387
93.889045	2872.261033	22.611405
93.649857	2886.539247	22.616423
93.790321	2874.366208	22.621440
94.059925	2891.240719	22.626458
93.964915	2906.354993	22.631475
94.227492	2910.592230	22.636493
94.275055	2906.011173	22.641511
94.269118	2907.055194	22.646528
94.441509	2915.087605	22.651546
94.894385	2927.474348	22.656563
95.412858	2927.711404	22.661581
95.255358	2932.566278	22.666599
95.365395	2929.815973	22.671616
95.278050	2902.855353	22.676634
95.042148	2901.146665	22.681651
95.663013	2908.280733	22.686669
95.328499	2921.698310	22.691687
95.613504	2931.508299	22.696704
95.650266	2927.662551	22.701722
95.471270	2936.857577	22.706739
95.616199	2926.057499	22.711757
95.337987	2929.284580	22.716775
95.759193	2925.705917	22.721792
95.932878	2938.639332	22.726810
95.903756	2953.758885	22.731827
96.177472	2957.390696	22.736845
96.241676	2961.089088	22.741863
96.121794	2951.369543	22.746880
96.093913	2957.910592	22.751898
96.005175	2970.696915	22.756915
96.637611	2965.729607	22.761933
96.856133	2981.220426	22.766951
96.885157	2970.760008	22.771968
96.933451	2978.628336	22.776986
96.801834	2975.682973	22.782003
97.142242	2985.762589	22.787021
97.363974	3003.728316	22.792039
97.457655	3005.188566	22.797056
97.595821	3006.550498	22.802074
97.532311	3002.323266	22.807091
97.799559	2995.185504	22.812109
98.093189	3001.184713	22.817127
97.661966	2999.880827	22.822144
97.887336	3000.532588	22.827162
97.956520	3011.518622	22.832179
98.501931	3016.728444	22.837197
98.554804	3031.058048	22.842215
98.357221	3027.421958	22.847232
98.651930	3026.206164	22.852250
98.567769	3029.823616	22.857267
98.818925	3023.464167	22.862285
98.751714	3029.470371	22.867303
98.615971	3029.583443	22.872320
98.979707	3018.358455	22.877338
98.938360	3039.242059	22.882355
99.007162	3047.299170	22.887373
98.610405	3058.523421	22.892391
98.735672	3057.898724	22.897408
99.283637	3061.316238	22.902426
99.245814	3086.270571	22.907443
99.720740	3084.248088	22.912461
99.776100	3084.442523	22.917479
99.669335	3090.408837	22.922496
99.878259	3090.146702	22.927514
99.886415	3111.943162	22.932531
100.432867	3110.959329	22.937549
100.431500	3106.036281	22.942567
100.350428	3115.178974	22.947584
100.882695	3109.056440	22.952602
100.756445	3105.310874	22.957619
101.089412	3109.451464	22.962637
101.067111	3111.204970	22.967655
100.967800	3100.136125	22.972672
101.239420	3096.110098	22.977690
101.246686	3102.029582	22.982707
101.416347	3095.391050	22.987725
101.106122	3095.274324	22.992743
101.388871	3094.960592	22.997760
101.620014	3085.758095	23.002778
101.386435	3100.132040	23.007795
101.419833	3091.976552	23.012813
101.574671	3107.157930	23.017831
101.838154	3119.769118	23.022848
102.187069	3120.004327	23.027866
101.653469	3121.169195	23.032883
102.143685	3124.857335	23.037901
101.876979	3126.105979	23.042919
101.858179	3122.875348	23.047936
102.201127	3141.084182	23.052954
102.274965	3155.069450	23.057971
102.408788	3150.418522	23.062989
102.303988	3152.926710	23.068007
102.243882	3161.562366	23.073024
103.065750	3161.481451	23.078042
103.307414	3169.196587	23.083059
103.184366	3168.570476	23.088077
103.237652	3158.033073	23.093095
103.084456	3168.159096	23.098112
103.508907	3170.218994	23.103130
103.802553	3190.084640	23.108147
103.733393	3187.876216	23.113165
103.830205	3192.731589	23.118183
103.795456	3203.140022	23.123200
104.062128	3194.815135	23.128218
103.691541	3199.384867	23.133235
103.856897	3195.284667	23.138253
104.409619	3202.683331	23.143271
104.509161	3216.801420	23.148288
104.492034	3215.021431	23.153306
104.588570	3225.080943	23.158323
104.975541	3222.532006	23.163341
104.999966	3215.053206	23.168359
105.088237	3214.827976	23.173376
105.324184	3211.750838	23.178394
104.525085	3225.369229	23.183411
104.503105	3226.796677	23.188429
104.947997	3244.783614	23.193447
105.076920	3247.559058	23.198464
105.302935	3253.948734	23.203482
105.606776	3271.929919	23.208499
105.297057	3275.658797	23.213517
105.827726	3276.606517	23.218535
105.761344	3280.234470	23.223552
106.445540	3281.110704	23.228570
106.301416	3303.005485	23.233587
106.241930	3291.879511	23.238605
106.734037	3296.550557	23.243623
106.535837	3302.767156	23.248640
107.037047	3287.108104	23.253658
106.782555	3300.461961	23.258675
106.765910	3298.112136	23.263693
107.398520	3291.027146	23.268711
107.294112	3289.747085	23.273728
107.675004	3283.658209	23.278746
107.235862	3292.082647	23.283763
107.435728	3286.737205	23.288781
107.753385	3279.485445	23.293799
107.437961	3297.594784	23.298816
107.538505	3297.597074	23.303834
107.424600	3299.542165	23.308851
107.716039	3309.843508	23.313869
107.993864	3316.688856	23.318887
107.833542	3323.409878	23.323904
107.887607	3320.625854	23.328922
108.198563	3337.881841	23.333939
108.504249	3347.653233	23.338957
108.470936	3345.834565	23.343975
108.547861	3349.405733	23.348992
108.644414	3342.216933	23.354010
108.485817	3356.530661	23.359027
108.823920	3359.292754	23.364045
109.143394	3376.566274	23.369063
109.057824	3367.635760	23.374080
108.781624	3363.156605	23.379098
109.064762	3369.291567	23.384115
109.201936	3368.822386	23.389133
109.683788	3386.332448	23.394151
109.498940	3394.803037	23.399168
109.695830	3388.069704	23.404186
109.857077	3386.694858	23.409203
109.904649	3384.180433	23.414221
110.321565	3386.519199	23.419239
110.146471	3395.363020	23.424256
110.408157	3404.974784	23.429274
110.509681	3407.802437	23.434291
110.403938	3419.548119	23.439309
110.593826	3406.358492	23.444327
110.808465	3412.291009	23.449344
110.792208	3416.529665	23.454362
110.922137	3435.971890	23.459379
110.822292	3441.332396	23.464397
111.222416	3440.568073	23.469415
111.185311	3437.315994	23.474432
111.549318	3432.420155	23.479450
111.818966	3431.727046	23.484467
111.817356	3443.918947	23.489485
111.934679	3451.837903	23.494503
111.730825	3457.678683	23.499520
112.208109	3460.111415	23.504538
112.157857	3465.615705	23.509555
112.091303	3465.831904	23.514573
112.495366	3460.059635	23.519591
112.374783	3458.879888	23.524608
112.425463	3473.827264	23.529626
112.829305	3487.372712	23.534643
112.887019	3489.429980	23.539661
112.881494	3483.787335	23.544679
112.454202	3487.475878	23.549696
112.957220	3494.943550	23.554714
113.198331	3508.780952	23.559731
113.292013	3517.431898	23.564749
113.685477	3506.986776	23.569767
113.526316	3509.228397	23.574784
114.066653	3502.904746	23.579802
113.676197	3510.908591	23.584819
114.127027	3528.389693	23.589837
114.266621	3538.135941	23.594855
114.306649	3544.500617	23.599872
114.445633	3536.669584	23.604890
114.321091	3532.872444	23.609907
114.266151	3533.037503	23.614925
114.548307	3531.263839	23.619943
114.232126	3537.263814	23.624960
114.971781	3549.386225	23.629978
114.861499	3552.852197	23.634995
114.753908	3561.651860	23.640013
115.082530	3561.892014	23.645031
114.883129	3560.342582	23.650048
115.081094	3577.351761	23.655066
115.468175	3591.739159	23.660083
115.389068	3591.833406	23.665101
115.843280	3590.638807	23.670119
115.831490	3615.223878	23.675136
116.097888	3612.129415	23.680154
116.107394	3606.042448	23.685171
116.123705	3611.179424	23.690189
116.560486	3603.541210	23.695207
116.543442	3610.407158	23.700224
116.613607	3602.852874	23.705242
116.528159	3599.952511	23.710259
116.819738	3611.023815	23.715277
117.064486	3623.666863	23.720295
117.157096	3634.423442	23.725312
117.064332	3635.111367	23.730330
117.578796	3630.041718	23.735347
117.579207	3632.313638	23.740365
117.733817	3622.503339	23.745383
117.824658	3625.413126	23.750400
117.458352	3630.308298	23.755418
117.781078	3633.109606	23.760435
117.606485	3641.500667	23.765453
118.307094	3653.152002	23.770471
118.009556	3655.298429	23.775488
118.297124	3648.525166	23.780506
118.306521	3649.302096	23.785523
118.341314	3658.657056	23.790541
118.353366	3658.602335	23.795559
118.662464	3670.569324	23.800576
118.695226	3673.430854	23.805594
119.288017	3669.163688	23.810611
118.969097	3685.360806	23.815629
119.234608	3675.960122	23.820647
119.443312	3684.363346	23.825664
119.248120	3702.427651	23.830682
119.810901	3701.204831	23.835699
119.725024	3710.756203	23.840717
119.996240	3696.701177	23.845735
119.748606	3702.187436	23.850752
119.939124	3715.494349	23.855770
120.351095	3727.438838	23.860787
120.258210	3729.264343	23.865805
120.628773	3728.818724	23.870823
120.887133	3734.564573	23.875840
120.558747	3730.167583	23.880858
121.017913	3721.488851	23.885875
120.716131	3724.954278	23.890893
121.051153	3736.887889	23.895911
121.085520	3743.857998	23.900928
121.413460	3742.597275	23.905946
121.605848	3738.080985	23.910963
121.425066	3751.376165	23.915981
121.549850	3745.449217	23.920999
121.889482	3764.438964	23.926016
121.872494	3766.274352	23.931034
122.181673	3764.250879	23.936051
121.972648	3776.632518	23.941069
122.277267	3768.918455	23.946087
122.435306	3771.783674	23.951104
122.244581	3794.242446	23.956122
122.762772	3800.139816	23.961139
122.545843	3803.759740	23.966157
122.873862	3793.451267	23.971175
122.813676	3797.890633	23.976192
122.666892	3824.115540	23.981210
123.166395	3824.992069	23.986227
123.166253	3833.365769	23.991245
123.201546	3826.331792	23.996263
123.616704	3848.611184	24.001280
123.586806	3855.652227	24.006298
124.146680	3854.228669	24.011315
124.066406	3854.649142	24.016333
124.120782	3855.231207	24.021351
124.056207	3851.326015	24.026368
124.322417	3858.425137	24.031386
124.520792	3873.075173	24.036403
124.836958	3876.424149	24.041421
124.752131	3867.791695	24.046439
124.698487	3866.625246	24.051456
125.031049	3870.177047	24.056474
125.017768	3860.971252	24.061491
125.070522	3867.520201	24.066509
124.989303	3881.973193	24.071527
125.328432	3898.864455	24.076544
125.345497	3892.171706	24.081562
125.533926	3895.096099	24.086579
125.549445	3896.489836	24.091597
125.781763	3915.862942	24.096615
126.345886	3921.253074	24.101632
126.050326	3929.472556	24.106650
126.264942	3921.913104	24.111667
126.476968	3922.104055	24.116685
126.770683	3918.161971	24.121703
126.512388	3929.736413	24.126720
126.759181	3943.610274	24.131738
127.124292	3944.270443	24.136755
126.718903	3962.251325	24.141773
127.077414	3935.424982	24.146791
127.135342	3953.436249	24.151808
127.446989	3967.149765	24.156826
127.656468	3975.031284	24.161843
127.607924	3970.603251	24.166861
127.530398	3969.409641	24.171879
127.976608	3990.439811	24.176896
128.069686	3998.582383	24.181914
128.593975	3995.268350	24.186931
128.656489	4002.185088	24.191949
128.815061	3987.183343	24.196967
128.869136	3987.106701	24.201984
128.731711	3994.198291	24.207002
128.731471	3996.817668	24.212019
128.942572	4010.380914	24.217037
128.817167	4012.660331	24.222055
129.077906	4018.329108	24.227072
129.049248	4020.776788	24.232090
129.356793	4034.171308	24.237107
129.321365	4046.557888	24.242125
129.631320	4042.901319	24.247143
130.165177	4047.907469	24.252160
129.986658	4062.229076	24.257178
130.052540	4072.975813	24.262195
130.295776	4075.337536	24.267213
130.107406	4076.509099	24.272231
130.390180	4080.858293	24.277248
130.523361	4101.778208	24.282266
130.808380	4106.396373	24.287283
130.910038	4112.230127	24.292301
131.035001	4110.030385	24.297319
131.117906	4097.377659	24.302336
131.255301	4126.272204	24.307354
131.583468	4127.408654	24.312371
131.613729	4125.767983	24.317389
131.843510	4118.691044	24.322407
132.245901	4120.947671	24.327424
131.866021	4117.329692	24.332442
132.409363	4120.099290	24.337459
132.440346	4132.998650	24.342477
132.535485	4141.373277	24.347495
133.047362	4138.221138	24.352512
132.517578	4142.547373	24.357530
132.913788	4144.122238	24.362547
132.958938	4135.715795	24.367565
132.851904	4135.678426	24.372583
132.971496	4136.195759	24.377600
132.625653	4161.561126	24.382618
133.005558	4160.562680	24.387635
133.189251	4170.517411	24.392653
133.040171	4186.647942	24.397671
133.513122	4189.198459	24.402688
133.684769	4202.729027	24.407706
134.010559	4201.093760	24.412723
134.260709	4218.353701	24.417741
134.423196	4223.909665	24.422759
134.663787	4219.760518	24.427776
134.825290	4216.438775	24.432794
135.219987	4223.025764	24.437811
135.089256	4221.562157	24.442829
135.233914	4212.179194	24.447847
135.340028	4218.442243	24.452864
135.321878	4223.472902	24.457882
135.724227	4232.984317	24.462899
135.992044	4232.891975	24.467917
135.752288	4244.431289	24.472935
135.951204	4233.239026	24.477952
136.001600	4239.538085	24.482970
136.279366	4234.581069	24.487987
136.131788	4238.542425	24.493005
136.323683	4250.271740	24.498023
136.617421	4264.505894	24.503040
136.275861	4269.812984	24.508058
136.296298	4265.350607	24.513075
136.519492	4272.729134	24.518093
136.753472	4291.204639	24.523111
136.948886	4292.019714	24.528128
136.889550	4317.337898	24.533146
137.369156	4318.594985	24.538163
137.301238	4327.564523	24.543181
137.179365	4333.575549	24.548199
137.858596	4349.826637	24.553216
137.795328	4351.909168	24.558234
137.656232	4359.288651	24.563251
138.309260	4360.687138	24.568269
138.673485	4381.870016	24.573287
138.676457	4377.071069	24.578304
138.682160	4382.490025	24.583322
138.763391	4382.430148	24.588339
138.814299	4388.433066	24.593357
138.718383	4409.989854	24.598375
139.087004	4412.390723	24.603392
139.188212	4416.200678	24.608410
139.415604	4427.115442	24.613427
140.179318	4424.652395	24.618445
140.130526	4438.940266	24.623463
140.050941	4431.604901	24.628480
140.154143	4437.180206	24.633498
140.122866	4437.850897	24.638515
140.697251	4444.675996	24.643533
140.602613	4460.148857	24.648551
140.932279	4456.331421	24.653568
140.704867	4456.815647	24.658586
141.066163	4462.343506	24.663603
141.303082	4454.839960	24.668621
141.205580	4465.876269	24.673639
141.398741	4472.825925	24.678656
141.545935	4484.653384	24.683674
141.573769	4484.459015	24.688691
142.065921	4474.226093	24.693709
141.889602	4481.366081	24.698727
142.317608	4491.430990	24.703744
141.982406	4507.187076	24.708762
142.417212	4509.343889	24.713779
142.488156	4508.121719	24.718797
142.297644	4498.478270	24.723815
142.548611	4511.009963	24.728832
142.844727	4526.125227	24.733850
142.543952	4539.650820	24.738867
142.909706	4536.357412	24.743885
142.977665	4542.211081	24.748903
143.456383	4551.540724	24.753920
143.497005	4552.392467	24.758938
143.749724	4552.380591	24.763955
143.643185	4553.497687	24.768973
144.036050	4572.145681	24.773991
144.210085	4573.779427	24.779008
144.300077	4578.794658	24.784026
144.267823	4584.931914	24.789043
144.380265	4576.671605	24.794061
145.030466	4601.377407	24.799079
145.087341	4604.085086	24.804096
144.985153	4597.811856	24.809114
145.482358	4610.088647	24.814131
145.406482	4598.406083	24.819149
145.333893	4602.641784	24.824167
145.888582	4613.652126	24.829184
146.020781	4634.167324	24.834202
145.875276	4635.772073	24.839219
146.308784	4627.945291	24.844237
146.520997	4637.783765	24.849255
146.435415	4633.148249	24.854272
146.287873	4635.766918	24.859290
146.392520	4638.361161	24.864307
146.881472	4653.098886	24.869325
146.697697	4655.255749	24.874343
146.995606	4662.879621	24.879360
147.288629	4676.791370	24.884378
147.215650	4675.714299	24.889395
147.498245	4674.316891	24.894413
147.350525	4683.743238	24.899431
147.538875	4699.109627	24.904448
148.101001	4703.170968	24.909466
148.406986	4705.261718	24.914483
148.623160	4698.254503	24.919501
148.537024	4715.037490	24.924519
148.657335	4728.202133	24.929536
148.868628	4739.758491	24.934554
148.825109	4734.247302	24.939571
149.446376	4738.366591	24.944589
149.447691	4747.404450	24.949607
149.551816	4730.692555	24.954624
149.668296	4748.863578	24.959642
149.748778	4756.647928	24.964659
150.099286	4753.983110	24.969677
149.888531	4756.810730	24.974695
150.100350	4761.030890	24.979712
149.889392	4760.655534	24.984730
149.782666	4781.353815	24.989747
150.442846	4785.229619	24.994765
150.366372	4798.060683	24.999783
150.526131	4820.058479	25.004800
150.504482	4823.368294	25.009818
150.658116	4829.439431	25.014835
151.068481	4839.785496	25.019853
151.329647	4849.009573	25.024871
151.542663	4854.929127	25.029888
151.728813	4853.375194	25.034906
152.093574	4866.612892	25.039923
152.258708	4866.907705	25.044941
152.210612	4876.148346	25.049959
152.284819	4864.244633	25.054976
152.656475	4872.462825	25.059994
152.616912	4871.803131	25.065011
152.926334	4883.059824	25.070029
152.893190	4898.041730	25.075047
152.952091	4897.045981	25.080064
153.320332	4887.945354	25.085082
153.230724	4899.934404	25.090099
153.709501	4904.912151	25.095117
153.884527	4918.141926	25.100135
153.771013	4924.392002	25.105152
153.951736	4925.799433	25.110170
154.076146	4915.848417	25.115187
154.513759	4912.044505	25.120205
154.610903	4918.517237	25.125223
154.606786	4932.275214	25.130240
154.750447	4935.754577	25.135258
154.821567	4943.526392	25.140275
155.022277	4941.933812	25.145293
155.031940	4953.001550	25.150311
154.860882	4959.490349	25.155328
155.825598	4961.299599	25.160346
155.746541	4974.052477	25.165363
155.825459	4962.671645	25.170381
155.607602	4986.140367	25.175399
156.224054	4985.946989	25.180416
156.571811	4979.175402	25.185434
156.263989	4992.493054	25.190451
156.807997	5003.150245	25.195469
156.771477	5006.175096	25.200487
156.872544	5010.854701	25.205504
157.235213	5013.878047	25.210522
157.143829	5006.697943	25.215539
157.456945	5028.802954	25.220557
157.545663	5040.546793	25.225575
157.413429	5042.929084	25.230592
157.961085	5041.044358	25.235610
158.065499	5064.425978	25.240627
158.039174	5062.853646	25.245645
158.372545	5074.213622	25.250663
158.503559	5078.351950	25.255680
158.588990	5088.377088	25.260698
158.500948	5102.935897	25.265715
158.780414	5108.701207	25.270733
159.013705	5121.886854	25.275751
159.063454	5134.282241	25.280768
159.237710	5126.191767	25.285786
159.093351	5134.978312	25.290803
159.488334	5159.568156	25.295821
159.690700	5166.164548	25.300839
159.991711	5186.992754	25.305856
160.626607	5182.652064	25.310874
160.622498	5186.985271	25.315891
160.701159	5187.005364	25.320909
160.635861	5176.994231	25.325927
160.833158	5201.962619	25.330944
161.213167	5205.211530	25.335962
160.961730	5220.196803	25.340979
161.282129	5215.004025	25.345997
161.605860	5231.090427	25.351015
161.776643	5240.231250	25.356032
162.550645	5237.971156	25.361050
162.111224	5238.306207	25.366067
162.457672	5235.768784	25.371085
162.633557	5236.703707	25.376103
162.646572	5241.576739	25.381120
162.840420	5252.309399	25.386138
162.590386	5271.707330	25.391155
162.876623	5271.852151	25.396173
162.999732	5268.986257	25.401191
163.189163	5273.967133	25.406208
163.469546	5280.908221	25.411226
163.189157	5294.604353	25.416243
163.917114	5293.033137	25.421261
163.602640	5304.284735	25.426279
163.777362	5311.768651	25.431296
164.159785	5309.615117	25.436314
164.185537	5326.303047	25.441331
164.620457	5328.692298	25.446349
164.542143	5338.717926	25.451367
164.859767	5342.845906	25.456384
164.903523	5342.147983	25.461402
164.879803	5370.131893	25.466419
164.993745	5373.020854	25.471437
165.381946	5377.593962	25.476455
165.466833	5392.117321	25.481472
165.844032	5388.151604	25.486490
165.987166	5398.187864	25.491507
166.090734	5424.455897	25.496525
166.256186	5427.482045	25.501543
166.235697	5432.381161	25.506560
166.501997	5435.299254	25.511578
166.523596	5463.385302	25.516595
166.804936	5455.642376	25.521613
166.974607	5470.625903	25.526631
167.104613	5486.991943	25.531648
167.660187	5490.550517	25.536666
167.864321	5509.161562	25.541683
167.861872	5513.692270	25.546701
168.007967	5506.161522	25.551719
168.233082	5523.618430	25.556736
168.549543	5528.084532	25.561754
168.855759	5537.382680	25.566771
168.800937	5544.679454	25.571789
168.983307	5540.585284	25.576807
169.075054	5543.919795	25.581824
169.529329	5553.701443	25.586842
169.642238	5564.861993	25.591859
169.498347	5562.077267	25.596877
169.828367	5557.488451	25.601895
169.955480	5579.837682	25.606912
170.191871	5589.468762	25.611930
170.187285	5602.821785	25.616947
170.481069	5596.817334	25.621965
170.679621	5606.180603	25.626983
170.862355	5622.758583	25.632000
171.013852	5628.905206	25.637018
171.001364	5633.967668	25.642035
170.974390	5642.949290	25.647053
171.546548	5649.002650	25.652071
171.418211	5661.579154	25.657088
171.489417	5666.522232	25.662106
172.118476	5682.896431	25.667123
171.854346	5680.712056	25.672141
172.364785	5700.026357	25.677159
172.279713	5708.000832	25.682176
172.892376	5706.460481	25.687194
173.139620	5715.291207	25.692212
173.178818	5719.427576	25.697229
173.409908	5729.439247	25.702247
173.226352	5738.879243	25.707264
173.673925	5734.419774	25.712282
173.690438	5741.174768	25.717300
174.010075	5753.129005	25.722317
174.271822	5758.177612	25.727335
174.254902	5766.924507	25.732352
174.520999	5758.360904	25.737370
174.615217	5763.542000	25.742388
174.627116	5782.553794	25.747405
174.837156	5788.401734	25.752423
174.780785	5789.745318	25.757440
175.225610	5787.382126	25.762458
175.439586	5811.839920	25.767476
175.735700	5814.125421	25.772493
176.036964	5816.108415	25.777511
175.862490	5815.133129	25.782528
176.109499	5814.434616	25.787546
176.362489	5831.479267	25.792564
176.538970	5835.681940	25.797581
176.654734	5839.333097	25.802599
176.329311	5835.225253	25.807616
176.882707	5848.511313	25.812634
177.265516	5862.732959	25.817652
176.873323	5860.381518	25.822669
177.283837	5879.217172	25.827687
177.497497	5894.583690	25.832704
177.696412	5893.358344	25.837722
177.972133	5909.315554	25.842740
178.079628	5916.881773	25.847757
178.637133	5920.281816	25.852775
178.635656	5931.956975	25.857792
178.797498	5938.236688	25.862810
179.134597	5947.365354	25.867828
179.131927	5937.710402	25.872845
179.561196	5955.423834	25.877863
179.327921	5970.615528	25.882880
179.683207	5966.391020	25.887898
180.099190	5963.386727	25.892916
180.052130	5984.928126	25.897933
180.164734	5986.031095	25.902951
180.500985	5992.459172	25.907968
180.626909	6000.028681	25.912986
180.858124	6006.834096	25.918004
180.644686	6026.115049	25.923021
181.423166	6031.882363	25.928039
181.415034	6031.301692	25.933056
181.313892	6047.501798	25.938074
181.562818	6050.452026	25.943092
181.728907	6064.344274	25.948109
182.074437	6070.280943	25.953127
182.238753	6086.860098	25.958144
182.436600	6078.804615	25.963162
182.596892	6087.917738	25.968180
182.386481	6103.406647	25.973197
182.534398	6111.163962	25.978215
182.570480	6130.237544	25.983232
182.802231	6140.225738	25.988250
183.255730	6153.634137	25.993268
183.882815	6173.228220	25.998285
184.018675	6174.203695	26.003303
183.870189	6182.351158	26.008320
184.547580	6195.618561	26.013338
184.898484	6209.858404	26.018356
184.717260	6212.236378	26.023373
184.987535	6199.443044	26.028391
185.131738	6222.245607	26.033408
185.256732	6230.910191	26.038426
185.756288	6230.396692	26.043444
185.497478	6232.084155	26.048461
185.800536	6237.759336	26.053479
185.817890	6253.454852	26.058496
186.074388	6253.400612	26.063514
186.351777	6261.585519	26.068532
186.162273	6273.952884	26.073549
186.542273	6275.229782	26.078567
186.612762	6281.746870	26.083584
186.810365	6285.716177	26.088602
187.048582	6298.202572	26.093620
186.829005	6323.263012	26.098637
187.538514	6314.854908	26.103655
187.395919	6337.048224	26.108672
187.628638	6339.356901	26.113690
187.696242	6346.734595	26.118708
188.051043	6368.803080	26.123725
188.405374	6369.563605	26.128743
188.434207	6376.962697	26.133760
188.559436	6387.989466	26.138778
188.892340	6390.099620	26.143796
188.818975	6408.408739	26.148813
189.099617	6411.991776	26.153831
189.302833	6425.494613	26.158848
189.876556	6448.580834	26.163866
190.347249	6451.128171	26.168884
190.321611	6452.814862	26.173901
190.839093	6443.194001	26.178919
190.999703	6450.880857	26.183936
191.194398	6469.159848	26.188954
191.062006	6476.369074	26.193972
191.373935	6486.012614	26.198989
191.782378	6485.540972	26.204007
191.718276	6485.186941	26.209024
191.549617	6492.451800	26.214042
191.791847	6503.017410	26.219060
191.737533	6509.215775	26.224077
192.018974	6519.894628	26.229095
192.517393	6530.069703	26.234112
192.204006	6543.421868	26.239130
192.684272	6562.910780	26.244148
193.036306	6562.379949	26.249165
193.186384	6569.591290	26.254183
193.506183	6584.231234	26.259200
193.583016	6589.438321	26.264218
194.074027	6593.131502	26.269236
194.114444	6618.887397	26.274253
194.040601	6615.257549	26.279271
194.579303	6627.121049	26.284288
194.512831	6634.984214	26.289306
195.156059	6645.026695	26.294324
195.026831	6645.682188	26.299341
195.427615	6646.935986	26.304359
195.733905	6664.495715	26.309376
195.686129	6681.212212	26.314394
195.921078	6673.297578	26.319412
195.801568	6686.197946	26.324429
195.847717	6706.459917	26.329447
196.262433	6710.545407	26.334464
195.987271	6725.973177	26.339482
196.562963	6731.910590	26.344500
196.364476	6747.818763	26.349517
196.816906	6760.670193	26.354535
197.166991	6767.412937	26.359552
197.373819	6785.192482	26.364570
197.887735	6787.710665	26.369588
197.718550	6799.274809	26.374605
198.197844	6816.271244	26.379623
198.655448	6817.619622	26.384640
198.894876	6820.319516	26.389658
199.119361	6825.072961	26.394676
199.125657	6836.780581	26.399693
199.174711	6836.047846	26.404711
199.825259	6842.845642	26.409728
199.594055	6845.921977	26.414746
199.804374	6860.811087	26.419764
200.107144	6869.673439	26.424781
200.191123	6869.963613	26.429799
200.578375	6862.215864	26.434816
200.418576	6878.224884	26.439834
200.468329	6883.295559	26.444852
200.725134	6905.629918	26.449869
200.723420	6908.090914	26.454887
200.883519	6916.087633	26.459904
201.331287	6939.531759	26.464922
201.608992	6939.618152	26.469940
201.504803	6955.630647	26.474957
201.977910	6963.188041	26.479975
201.952030	6973.856637	26.484992
202.002619	6987.395460	26.490010
202.489006	6998.770880	26.495028
202.476055	7021.128792	26.500045
202.729006	7025.370323	26.505063
203.347723	7043.713686	26.510080
203.650319	7052.690383	26.515098
203.925741	7050.655946	26.520116
203.910357	7061.859271	26.525133
204.295958	7078.169679	26.530151
204.647653	7077.708992	26.535168
204.245515	7082.509536	26.540186
204.438399	7098.129569	26.545204
204.609190	7105.891462	26.550221
204.805549	7122.791707	26.555239
205.158570	7128.463666	26.560256
205.149742	7152.554761	26.565274
205.698578	7169.228141	26.570292
205.920615	7181.854970	26.575309
206.332900	7192.852895	26.580327
206.454076	7193.283426	26.585344
206.478381	7204.676414	26.590362
206.938956	7216.880181	26.595380
207.238856	7223.886638	26.600397
207.228974	7228.349751	26.605415
207.406184	7235.167788	26.610432
207.366957	7246.587864	26.615450
207.796679	7250.800980	26.620468
208.153245	7276.168475	26.625485
207.998489	7285.005977	26.630503
208.573943	7278.918034	26.635520
208.815505	7311.442637	26.640538
208.870728	7308.867246	26.645556
208.969234	7322.422052	26.650573
209.229486	7335.407376	26.655591
209.662050	7344.258749	26.660608
209.544719	7350.332391	26.665626
209.811801	7360.788909	26.670644
210.043012	7371.493982	26.675661
210.346364	7386.207495	26.680679
210.558269	7402.545416	26.685696
211.255464	7409.594101	26.690714
210.976289	7403.298642	26.695732
211.199190	7424.681510	26.700749
211.203134	7439.155555	26.705767
211.828207	7442.172172	26.710784
211.535931	7466.417003	26.715802
212.046252	7454.499017	26.720820
212.253989	7469.016546	26.725837
212.576587	7495.592038	26.730855
212.929933	7490.422217	26.735872
212.904778	7510.204705	26.740890
213.036191	7517.476282	26.745908
213.418519	7519.627247	26.750925
213.110023	7541.152592	26.755943
213.814532	7553.574603	26.760960
214.047961	7556.300036	26.765978
214.089497	7552.759576	26.770996
214.116082	7577.937204	26.776013
214.225406	7580.054601	26.781031
214.945430	7579.989008	26.786048
214.768138	7609.717115	26.791066
215.028769	7607.457412	26.796084
215.317458	7610.087060	26.801101
215.394262	7635.304515	26.806119
215.803725	7632.579844	26.811136
215.850500	7641.690598	26.816154
216.215937	7652.686359	26.821172
216.721485	7654.565667	26.826189
216.547104	7661.045875	26.831207
217.232766	7672.202107	26.836224
217.106739	7687.454089	26.841242
217.204413	7687.116573	26.846260
217.513772	7706.313803	26.851277
217.640534	7714.414120	26.856295
218.038523	7720.623154	26.861312
217.982792	7736.138456	26.866330
218.234891	7747.293257	26.871348
218.746080	7760.584769	26.876365
218.675144	7779.506326	26.881383
219.311123	7783.915454	26.886400
219.307442	7802.124054	26.891418
219.313058	7811.832502	26.896436
219.991593	7805.234979	26.901453
219.772042	7832.747573	26.906471
220.320264	7830.954608	26.911488
220.452794	7856.492452	26.916506
220.537061	7861.150477	26.921524
220.999646	7870.527307	26.926541
221.046964	7884.723601	26.931559
221.627643	7895.685475	26.936576
221.517078	7899.316284	26.941594
221.907661	7916.601136	26.946612
222.072354	7926.448742	26.951629
222.183491	7933.807364	26.956647
222.384158	7937.670239	26.961664
222.612450	7954.261235	26.966682
222.519301	7968.532059	26.971700
222.810217	7985.044189	26.976717
223.301798	7999.976032	26.981735
223.556786	8011.713454	26.986752
223.567492	8016.264755	26.991770
223.893157	8040.143487	26.996788
224.576365	8044.369209	27.001805
224.511417	8055.013488	27.006823
224.733599	8062.033970	27.011840
224.979252	8080.736478	27.016858
225.219058	8076.535263	27.021876
225.593157	8094.709229	27.026893
225.714822	8110.221524	27.031911
225.965234	8115.491754	27.036928
226.429052	8120.309950	27.041946
226.425436	8121.341722	27.046964
226.506860	8125.204689	27.051981
226.374851	8140.411618	27.056999
226.798394	8161.883573	27.062016
226.958121	8160.746471	27.067034
227.014283	8175.112497	27.072052
227.612845	8187.742389	27.077069
227.662895	8210.411358	27.082087
228.035790	8214.935844	27.087104
228.328256	8235.500861	27.092122
228.265514	8243.758068	27.097140
228.445986	8247.264367	27.102157
228.438922	8270.918091	27.107175
229.130749	8277.277213	27.112192
229.042170	8297.387057	27.117210
229.336426	8319.392656	27.122228
230.009700	8316.996802	27.127245
230.080958	8345.681555	27.132263
230.165376	8345.808623	27.137280
230.485871	8351.045273	27.142298
230.646785	8363.918693	27.147316
231.188000	8367.368454	27.152333
230.934935	8378.921630	27.157351
231.276110	8395.443984	27.162368
231.419754	8409.744536	27.167386
231.839046	8429.536515	27.172404
232.063661	8428.256312	27.177421
232.307185	8447.010017	27.182439
232.431930	8458.343160	27.187456
232.675248	8474.056238	27.192474
232.895442	8483.307343	27.197492
233.274750	8487.869445	27.202509
233.249849	8512.531643	27.207527
233.830958	8524.185524	27.212544
234.082498	8533.670156	27.217562
234.284230	8552.861015	27.222580
234.505134	8559.922104	27.227597
234.505781	8568.859841	27.232615
235.185177	8585.153099	27.237632
235.595001	8596.640813	27.242650
235.445160	8601.983763	27.247668
235.478859	8617.668663	27.252685
235.415438	8620.725437	27.257703
235.736447	8638.287275	27.262720
236.031262	8657.707842	27.267738
236.073280	8676.909532	27.272756
236.705940	8689.163936	27.277773
236.938684	8705.426483	27.282791
237.084591	8727.159429	27.287808
237.044479	8745.019853	27.292826
237.618774	8767.977016	27.297844
237.790448	8769.825078	27.302861
237.944639	8787.467475	27.307879
238.093581	8800.933262	27.312896
239.134416	8816.480786	27.317914
239.180006	8825.801956	27.322932
239.837049	8819.167407	27.327949
239.987958	8847.055262	27.332967
239.910553	8854.057939	27.337984
240.292918	8853.693756	27.343002
240.504076	8858.453958	27.348020
240.921512	8864.972179	27.353037
240.900620	8884.197924	27.358055
241.362221	8876.476289	27.363072
241.814772	8888.855194	27.368090
241.430072	8898.224002	27.373108
241.976471	8901.216120	27.378125
242.172970	8911.430895	27.383143
242.323390	8926.973096	27.388160
242.611695	8925.308122	27.393178
242.371151	8937.816764	27.398196
243.044870	8951.588118	27.403213
243.131286	8961.785698	27.408231
243.333526	8982.618699	27.413248
243.615046	8985.650741	27.418266
243.662483	8994.410024	27.423284
244.333896	9011.044570	27.428301
244.261591	9025.481467	27.433319
244.369619	9051.781539	27.438336
244.829293	9049.070382	27.443354
245.036733	9066.178039	27.448372
245.055835	9073.652469	27.453389
245.358784	9101.208367	27.458407
245.379339	9092.274776	27.463424
246.113226	9117.222729	27.468442
246.511945	9125.942054	27.473460
246.401833	9124.551773	27.478477
246.356855	9146.749376	27.483495
246.528215	9151.002623	27.488512
247.076520	9162.945216	27.493530
247.219536	9178.858357	27.498548
247.575906	9193.162210	27.503565
247.762720	9206.886764	27.508583
247.860936	9227.783782	27.513600
248.408290	9240.216592	27.518618
248.241753	9267.169059	27.523636
248.572962	9266.601423	27.528653
249.082603	9288.289888	27.533671
249.416717	9295.136406	27.538688
249.503702	9312.938610	27.543706
249.478291	9335.977743	27.548724
250.023317	9347.794972	27.553741
250.222233	9368.250099	27.558759
250.548783	9389.593234	27.563776
250.947894	9390.392987	27.568794
251.091683	9419.666377	27.573812
251.444178	9417.666158	27.578829
251.647999	9428.455927	27.583847
251.888224	9447.305100	27.588864
252.317589	9456.704912	27.593882
252.205154	9481.654878	27.598900
252.777669	9489.192301	27.603917
252.975238	9509.777030	27.608935
253.255347	9516.248926	27.613952
253.637924	9530.774840	27.618970
253.944896	9549.705257	27.623988
254.131390	9544.130690	27.629005
254.541002	9562.237426	27.634023
254.355226	9576.187046	27.639040
254.588352	9589.994071	27.644058
254.751870	9612.207436	27.649076
254.970075	9620.686697	27.654093
255.559267	9635.694515	27.659111
255.462222	9647.382698	27.664128
256.012097	9667.208166	27.669146
256.200009	9681.519071	27.674164
256.323920	9697.337413	27.679181
256.854929	9711.270914	27.684199
257.032895	9725.166754	27.689216
257.486897	9739.562865	27.694234
257.602506	9749.763204	27.699252
257.950743	9752.478681	27.704269
258.359823	9778.428379	27.709287
258.282615	9788.952937	27.714304
258.723221	9793.000286	27.719322
258.660490	9828.841915	27.724340
258.909691	9829.796495	27.729357
259.575523	9845.244029	27.734375
259.626400	9861.411017	27.739392
260.077661	9870.872051	27.744410
260.054304	9882.018795	27.749428
260.527489	9905.036871	27.754445
260.959654	9906.877400	27.759463
260.898627	9922.576104	27.764480
261.395939	9931.073929	27.769498
261.276193	9950.172354	27.774516
261.819453	9962.329882	27.779533
261.820425	9979.877629	27.784551
262.126446	9993.888010	27.789568
262.420679	9988.561740	27.794586
262.859984	10012.957174	27.799604
263.085480	10033.872775	27.804621
263.289358	10044.918992	27.809639
263.411497	10051.616573	27.814656
263.761538	10058.162198	27.819674
263.951643	10063.417847	27.824692
264.248709	10086.850583	27.829709
264.022282	10097.400831	27.834727
264.429074	10114.868945	27.839744
265.238638	10129.375145	27.844762
265.140966	10161.321194	27.849780
265.218718	10169.181127	27.854797
265.535650	10180.557731	27.859815
265.569891	10200.542482	27.864832
265.986547	10215.681823	27.869850
266.446780	10240.791064	27.874868
266.699934	10258.763768	27.879885
266.872886	10283.466838	27.884903
267.268599	10302.564655	27.889920
267.628489	10313.199192	27.894938
267.654702	10329.702412	27.899956
268.051019	10343.897475	27.904973
268.618653	10366.895065	27.909991
268.437341	10387.308070	27.915008
269.140900	10386.523561	27.920026
269.421282	10403.320403	27.925044
269.642862	10419.168982	27.930061
270.437501	10434.136453	27.935079
270.132974	10437.521043	27.940096
270.754907	10451.857695	27.945114
270.942719	10466.027504	27.950132
271.027399	10486.383999	27.955149
271.480751	10495.118665	27.960167
271.544972	10516.937673	27.965184
271.976388	10528.896700	27.970202
272.007786	10540.576874	27.975220
272.074868	10554.869953	27.980237
272.563286	10570.667421	27.985255
272.592751	10596.453589	27.990272
273.059084	10610.114954	27.995290
272.875765	10635.159586	28.000308
273.040149	10649.066352	28.005325
274.024379	10659.071488	28.010343
274.110682	10689.105950	28.015360
274.360856	10707.620116	28.020378
274.968795	10720.673547	28.025396
275.078228	10741.048326	28.030413
275.751924	10751.226253	28.035431
275.675043	10775.134727	28.040448
275.746694	10779.153585	28.045466
275.880615	10804.576138	28.050484
276.215844	10820.033642	28.055501
276.893419	10837.274936	28.060519
277.330977	10850.485885	28.065536
277.677407	10868.136564	28.070554
277.977307	10872.785771	28.075572
278.051129	10891.398671	28.080589
278.359931	10897.250268	28.085607
278.799875	10912.121690	28.090624
278.897893	10924.889397	28.095642
279.430707	10939.551657	28.100660
279.273976	10946.495101	28.105677
279.703610	10963.100007	28.110695
279.779141	10985.670977	28.115712
280.267699	10999.217117	28.120730
280.375866	11004.273126	28.125748
280.188807	11015.175146	28.130765
280.641025	11026.464564	28.135783
281.067558	11046.656454	28.140800
281.167265	11063.892797	28.145818
281.265467	11077.979492	28.150836
281.380660	11110.071028	28.155853
281.826441	11122.177816	28.160871
282.118560	11146.771089	28.165888
282.609087	11153.512938	28.170906
282.896680	11178.740462	28.175924
282.956663	11201.081094	28.180941
283.679963	11211.512680	28.185959
283.668154	11239.167675	28.190976
284.142101	11249.481408	28.195994
284.464385	11273.723214	28.201012
284.656870	11282.273004	28.206029
285.313258	11293.987362	28.211047
285.356695	11321.920144	28.216064
285.294526	11334.229353	28.221082
286.067473	11351.044137	28.226100
286.094489	11370.806195	28.231117
286.772113	11372.386449	28.236135
286.847976	11395.578791	28.241152
286.976500	11410.831559	28.246170
287.291990	11423.180749	28.251188
287.815312	11452.747195	28.256205
288.106963	11470.562027	28.261223
288.405314	11482.058449	28.266240
288.468328	11500.130193	28.271258
288.782823	11518.622036	28.276276
289.240043	11544.244364	28.281293
289.578254	11540.376582	28.286311
289.566672	11570.242939	28.291328
289.713512	11578.345037	28.296346
290.441990	11596.305162	28.301364
290.379487	11621.411685	28.306381
290.890206	11629.850680	28.311399
291.145483	11657.599274	28.316416
291.316795	11672.693930	28.321434
291.831293	11690.421692	28.326452
291.630232	11712.620294	28.331469
292.253815	11728.093972	28.336487
292.344867	11760.052121	28.341504
292.876229	11767.082147	28.346522
293.344938	11793.197773	28.351540
293.327299	11812.280705	28.356557
293.710640	11832.181322	28.361575
293.904553	11847.047057	28.366592
294.434452	11862.369334	28.371610
295.049478	11876.134804	28.376628
295.350355	11891.168822	28.381645
295.881820	11906.999874	28.386663
296.108664	11919.557943	28.391680
296.454177	11919.179321	28.396698
297.132256	11931.152143	28.401716
297.034665	11942.036823	28.406733
297.228632	11944.053333	28.411751
297.266243	11959.901571	28.416768
297.529778	11972.600161	28.421786
298.305286	11984.024264	28.426804
298.209407	12012.751878	28.431821
298.402915	12013.870246	28.436839
298.839365	12026.452010	28.441856
298.671110	12043.164871	28.446874
299.028524	12052.864922	28.451892
299.139702	12080.523057	28.456909
299.426686	12097.297720	28.461927
299.664731	12119.080660	28.466944
299.895905	12144.727172	28.471962
300.307546	12164.725945	28.476980
300.191597	12189.689334	28.481997
300.671792	12201.628925	28.487015
301.281825	12234.332581	28.492032
301.538212	12255.794346	28.497050
301.942011	12268.838703	28.502068
302.234284	12290.860308	28.507085
302.472089	12303.911682	28.512103
302.981145	12331.373589	28.517120
303.110966	12345.960431	28.522138
303.733119	12359.197220	28.527156
303.877262	12376.834178	28.532173
303.970562	12392.144127	28.537191
304.566759	12406.069179	28.542208
304.713062	12427.141241	28.547226
305.191659	12440.405009	28.552244
305.360336	12463.028805	28.557261
305.749733	12482.259470	28.562279
306.089631	12504.150563	28.567296
306.176126	12532.488030	28.572314
306.392512	12539.996021	28.577332
306.795821	12567.693304	28.582349
307.273906	12587.648507	28.587367
307.499622	12599.386251	28.592384
307.407871	12618.978803	28.597402
307.897738	12641.366879	28.602420
308.220742	12665.388447	28.607437
308.575022	12682.904281	28.612455
308.659147	12709.564114	28.617472
308.870518	12734.735760	28.622490
309.604961	12757.521617	28.627508
309.884927	12791.344766	28.632525
310.157673	12815.508827	28.637543
310.575286	12829.533143	28.642560
311.025639	12860.064513	28.647578
311.623500	12872.944859	28.652596
311.553304	12892.611391	28.657613
312.190096	12911.183855	28.662631
312.314258	12922.379189	28.667648
312.319189	12953.895345	28.672666
312.759224	12967.969651	28.677684
313.295275	12986.998561	28.682701
313.551363	13000.320105	28.687719
313.572366	13028.245348	28.692736
314.060512	13054.706494	28.697754
314.624939	13076.740852	28.702772
314.447951	13096.759405	28.707789
314.734959	13113.060756	28.712807
315.373674	13135.445364	28.717824
315.650945	13151.809827	28.722842
315.831460	13173.123039	28.727860
315.994785	13204.832518	28.732877
316.571088	13223.735271	28.737895
316.429020	13248.652597	28.742912
317.084391	13275.835003	28.747930
317.487867	13295.975205	28.752948
317.800120	13324.019799	28.757965
317.793061	13349.748617	28.762983
318.497796	13368.100755	28.768000
318.460183	13398.762757	28.773018
318.870272	13413.838420	28.778036
319.473377	13447.402993	28.783053
319.555994	13459.749729	28.788071
320.373448	13489.547001	28.793088
320.461720	13509.455962	28.798106
320.896650	13521.077792	28.803124
321.318604	13543.098540	28.808141
321.511392	13560.520698	28.813159
321.848150	13581.472897	28.818176
321.913076	13594.114221	28.823194
322.473092	13614.889248	28.828212
322.548532	13639.389777	28.833229
322.932127	13637.290140	28.838247
323.060215	13653.889407	28.843264
323.159096	13686.951661	28.848282
323.777967	13696.653550	28.853300
324.359950	13725.038732	28.858317
324.562683	13746.561775	28.863335
324.802715	13751.497527	28.868352
324.909400	13771.621249	28.873370
325.503093	13785.462799	28.878388
325.546996	13821.976425	28.883405
325.892481	13839.780218	28.888423
326.277538	13865.183328	28.893440
326.321272	13892.050354	28.898458
326.765217	13915.270466	28.903476
326.795673	13951.556508	28.908493
327.403527	13980.845642	28.913511
327.585804	14007.975188	28.918528
327.986655	14039.799848	28.923546
328.520548	14060.419011	28.928564
329.221936	14084.711009	28.933581
329.189089	14116.933842	28.938599
329.766684	14134.108524	28.943616
329.548978	14167.887661	28.948634
330.280081	14179.585449	28.953652
330.836485	14204.598234	28.958669
331.089608	14238.904791	28.963687
331.363847	14252.717658	28.968704
331.875412	14282.428316	28.973722
332.135436	14278.011764	28.978740
332.287954	14321.012903	28.983757
332.465051	14341.626858	28.988775
333.182723	14368.104155	28.993792
333.249904	14398.578892	28.998810
333.708914	14420.884687	29.003828
334.126241	14443.580396	29.008845
334.585531	14473.129837	29.013863
334.792609	14494.798143	29.018880
334.910823	14517.110042	29.023898
334.935688	14545.899348	29.028916
335.557001	14569.057934	29.033933
335.972842	14593.213550	29.038951
336.695613	14617.580031	29.043968
336.970965	14654.476441	29.048986
337.118053	14657.957359	29.054004
337.803154	14687.977315	29.059021
337.875534	14707.704384	29.064039
338.367442	14730.016188	29.069056
338.488269	14756.996382	29.074074
338.733856	14775.747628	29.079092
339.157351	14789.436951	29.084109
339.214430	14820.528822	29.089127
339.958229	14853.784570	29.094144
340.226952	14867.034622	29.099162
340.933612	14899.068819	29.104180
341.122412	14920.811638	29.109197
341.215113	14949.842602	29.114215
341.942359	14958.518594	29.119232
341.606642	14988.837300	29.124250
342.035534	15017.360394	29.129268
342.168981	15039.281176	29.134285
342.764050	15069.341950	29.139303
343.197899	15087.644719	29.144320
343.720778	15117.361323	29.149338
344.090029	15137.709630	29.154356
344.573922	15142.006511	29.159373
344.604689	15165.690817	29.164391
345.361748	15181.927467	29.169408
345.428189	15204.110166	29.174426
345.547249	15220.999371	29.179444
345.939169	15239.430613	29.184461
346.085136	15265.545328	29.189479
346.859093	15282.386098	29.194496
347.303173	15302.772661	29.199514
347.158375	15323.646025	29.204532
347.464869	15342.616381	29.209549
348.146406	15369.477982	29.214567
348.503652	15384.551602	29.219584
348.564012	15417.707253	29.224602
349.131086	15445.338176	29.229620
349.467593	15461.327900	29.234637
349.583759	15483.724985	29.239655
350.116881	15502.744706	29.244672
350.262830	15543.909161	29.249690
350.603833	15561.715569	29.254708
350.769260	15582.791680	29.259725
351.191074	15626.390013	29.264743
351.590731	15640.946165	29.269760
351.963177	15680.281351	29.274778
352.408331	15721.425099	29.279796
352.786923	15740.109723	29.284813
352.568631	15782.241369	29.289831
353.241098	15807.383979	29.294848
353.422509	15837.790458	29.299866
354.152845	15863.751083	29.304884
354.396375	15892.684663	29.309901
354.672571	15934.741161	29.314919
355.167012	15952.814196	29.319936
355.372298	15987.942493	29.324954
355.766575	16019.132133	29.329972
356.564486	16043.675869	29.334989
356.801946	16072.547720	29.340007
357.404952	16097.855164	29.345024
357.700058	16124.526608	29.350042
358.245062	16150.824149	29.355060
358.509662	16169.247557	29.360077
358.675127	16204.337194	29.365095
359.026825	16220.183279	29.370112
359.246725	16249.948922	29.375130
359.873111	16278.502988	29.380148
360.552865	16303.194344	29.385165
360.609992	16326.721480	29.390183
360.702448	16346.398323	29.395200
361.013039	16372.460747	29.400218
361.153362	16409.227387	29.405236
361.573243	16433.113921	29.410253
361.926759	16474.968268	29.415271
362.592450	16496.062053	29.420288
362.685892	16530.060914	29.425306
363.090471	16554.456139	29.430324
363.756813	16584.153223	29.435341
364.046981	16615.449492	29.440359
364.418693	16639.807723	29.445376
364.590943	16673.412375	29.450394
364.733478	16695.171496	29.455412
365.464754	16715.792856	29.460429
365.656169	16752.149847	29.465447
366.018764	16787.931612	29.470464
366.408267	16818.568695	29.475482
366.739252	16846.814816	29.480500
367.203183	16870.754591	29.485517
367.504398	16906.409633	29.490535
368.148658	16925.024833	29.495552
368.433974	16948.029582	29.500570
368.695172	16972.751806	29.505588
369.125399	16988.661295	29.510605
369.389668	17026.305711	29.515623
369.644375	17046.010127	29.520640
369.974533	17075.998607	29.525658
370.390761	17106.414268	29.530676
370.920389	17125.562548	29.535693
371.127029	17161.227485	29.540711
371.419380	17184.923407	29.545728
371.737909	17204.582769	29.550746
372.032595	17256.212641	29.555764
372.890841	17276.526794	29.560781
372.841051	17313.010057	29.565799
373.387484	17335.622180	29.570816
373.587100	17365.002250	29.575834
374.140514	17389.022546	29.580852
374.887780	17414.555621	29.585869
375.437539	17458.979382	29.590887
375.311724	17478.373692	29.595904
375.168589	17499.247942	29.600922
375.789192	17535.541922	29.605940
376.540097	17565.956632	29.610957
377.416215	17591.339392	29.615975
377.680662	17619.949373	29.620992
378.201559	17652.840958	29.626010
378.130888	17675.588782	29.631028
378.780710	17693.188740	29.636045
378.664230	17722.878707	29.641063
379.376153	17752.308666	29.646080
379.756229	17780.185682	29.651098
379.904376	17810.716363	29.656116
380.214158	17843.654302	29.661133
380.514478	17877.188173	29.666151
381.060369	17908.651066	29.671168
381.683829	17936.335153	29.676186
381.793026	17971.567103	29.681204
382.290919	17994.760395	29.686221
382.621300	18036.434917	29.691239
382.809198	18056.109025	29.696256
383.590921	18087.968317	29.701274
383.998223	18106.720227	29.706292
384.973007	18127.894206	29.711309
385.162578	18149.511876	29.716327
385.933881	18167.620335	29.721344
386.146754	18186.204307	29.726362
386.349195	18215.482944	29.731380
386.501968	18228.151111	29.736397
386.679648	18260.438602	29.741415
386.778514	18291.517460	29.746432
387.407340	18319.893354	29.751450
387.506916	18357.725686	29.756468
388.040429	18376.983544	29.761485
388.047552	18419.576416	29.766503
388.905476	18453.446381	29.771520
389.212724	18494.085418	29.776538
389.135350	18526.024672	29.781556
389.727311	18553.234181	29.786573
389.918584	18594.967803	29.791591
390.602518	18631.572141	29.796608
390.848431	18656.663562	29.801626
390.906804	18698.294897	29.806644
391.612998	18731.216277	29.811661
392.025265	18776.188123	29.816679
392.273389	18810.076182	29.821696
392.892221	18846.917205	29.826714
393.116136	18878.343781	29.831732
393.771379	18904.917523	29.836749
394.119993	18940.731457	29.841767
394.277208	18969.689412	29.846784
394.613145	19001.067725	29.851802
394.867195	19030.457486	29.856820
395.606700	19070.931797	29.861837
395.709324	19099.681454	29.866855
395.899248	19145.228680	29.871872
396.969945	19170.900112	29.876890
396.882341	19205.233934	29.881908
397.280394	19235.334882	29.886925
397.736486	19274.642667	29.891943
398.145618	19307.932807	29.896960
398.864688	19345.839842	29.901978
399.017286	19392.346146	29.906996
399.659906	19412.197266	29.912013
400.019952	19446.370786	29.917031
400.078100	19485.153719	29.922048
400.643616	19514.305173	29.927066
401.105817	19560.030760	29.932084
401.596502	19587.687539	29.937101
402.074925	19622.738890	29.942119
402.126116	19666.792264	29.947136
402.490233	19703.432961	29.952154
402.929128	19744.215632	29.957172
403.172353	19787.789795	29.962189
403.632598	19828.023641	29.967207
404.179880	19874.756053	29.972224
404.524808	19907.722198	29.977242
405.079989	19946.805473	29.982260
405.478218	19980.666328	29.987277
405.728950	20022.620694	29.992295
406.372384	20057.418615	29.997312
407.140940	20105.089388	30.002330
407.230889	20134.363194	30.007348
407.595161	20180.056225	30.012365
408.193424	20210.923558	30.017383
408.486628	20249.410787	30.022400
409.073305	20284.735704	30.027418
409.346960	20332.872147	30.032436
409.683022	20355.802248	30.037453
410.369589	20394.300388	30.042471
410.540044	20431.506049	30.047488
411.025070	20465.864347	30.052506
411.437185	20504.914262	30.057524
411.775476	20544.127844	30.062541
412.360106	20578.736342	30.067559
412.692879	20618.324676	30.072576
413.261084	20647.624284	30.077594
413.577923	20691.384111	30.082612
414.040049	20727.534668	30.087629
414.472544	20771.352818	30.092647
414.541909	20808.490900	30.097664
415.369229	20841.490986	30.102682
415.731530	20874.219649	30.107700
416.221739	20918.485867	30.112717
416.604739	20939.190603	30.117735
416.655127	20982.873876	30.122752
417.008217	21015.661099	30.127770
417.493861	21067.170211	30.132788
417.758486	21100.088913	30.137805
418.409033	21138.886407	30.142823
418.710856	21181.763883	30.147840
419.707366	21214.282609	30.152858
420.001703	21256.042047	30.157876
420.142321	21294.367708	30.162893
420.665544	21332.259608	30.167911
420.979434	21360.375855	30.172928
421.400556	21391.891170	30.177946
421.938543	21438.260506	30.182964
421.945681	21458.788419	30.187981
422.720931	21494.994443	30.192999
422.834214	21537.667512	30.198016
423.416836	21553.010583	30.203034
423.778885	21597.815387	30.208052
424.271819	21628.083089	30.213069
424.859491	21667.262740	30.218087
425.311136	21705.123173	30.223104
425.590538	21741.082241	30.228122
426.127522	21779.565729	30.233140
426.802422	21811.399331	30.238157
427.364855	21833.860370	30.243175
427.415796	21871.439022	30.248192
427.635447	21908.125765	30.253210
427.911670	21941.878301	30.258228
428.909195	21975.183565	30.263245
429.292054	22010.690893	30.268263
429.469812	22056.202271	30.273280
429.968702	22091.376786	30.278298
430.382805	22128.610509	30.283316
430.479670	22175.393877	30.288333
431.104108	22207.324876	30.293351
431.618684	22248.785413	30.298368
432.090950	22285.954667	30.303386
432.370749	22324.527683	30.308404
432.830443	22370.362221	30.313421
433.340502	22402.213176	30.318439
433.757901	22453.163838	30.323456
434.131424	22479.023520	30.328474
434.334367	22539.283260	30.333492
434.546487	22577.967391	30.338509
435.466047	22620.951269	30.343527
435.712082	22670.259489	30.348544
435.853817	22694.932649	30.353562
436.429435	22750.044550	30.358580
436.562558	22792.080440	30.363597
437.191452	22834.397068	30.368615
437.573730	22896.386593	30.373632
438.443900	22933.844636	30.378650
439.031930	22989.822538	30.383668
439.190827	23032.125978	30.388685
439.517898	23073.411409	30.393703
439.848782	23122.503479	30.398720
440.500442	23171.419608	30.403738
441.136033	23211.602530	30.408756
441.490592	23260.470314	30.413773
442.123710	23306.644517	30.418791
442.452016	23347.026840	30.423808
443.034834	23388.709093	30.428826
443.696090	23430.618159	30.433844
443.794240	23479.147388	30.438861
444.718404	23506.286276	30.443879
445.001540	23551.826791	30.448896
445.161490	23596.541001	30.453914
445.498730	23634.424667	30.458932
446.045239	23687.986408	30.463949
446.538665	23721.130947	30.468967
446.772208	23776.449432	30.473984
447.152200	23817.488210	30.479002
447.760454	23862.693477	30.484020
448.055846	23911.568185	30.489037
448.902048	23937.000199	30.494055
449.391260	23980.859829	30.499072
449.871355	24013.761136	30.504090
450.412404	24055.641167	30.509108
450.826130	24097.684299	30.514125
451.356686	24127.338362	30.519143
451.496701	24168.225303	30.524160
452.019476	24207.752717	30.529178
452.141204	24235.112294	30.534196
452.480722	24282.514159	30.539213
453.184647	24315.773255	30.544231
453.527585	24359.434128	30.549248
453.671651	24406.493354	30.554266
454.476715	24453.862808	30.559284
454.656775	24494.337032	30.564301
455.224231	24533.473013	30.569319
455.445958	24581.942337	30.574336
456.177713	24628.516971	30.579354
457.110461	24658.263102	30.584372
456.884030	24716.218682	30.589389
457.834197	24752.983054	30.594407
457.823823	24791.420418	30.599424
458.787199	24835.352013	30.604442
459.052470	24883.067463	30.609460
459.143823	24932.483504	30.614477
460.324206	24973.058265	30.619495
460.551991	25013.957930	30.624512
461.020537	25060.735002	30.629530
461.677400	25109.253665	30.634548
461.799082	25147.244162	30.639565
462.471901	25189.814844	30.644583
462.913572	25240.236748	30.649600
463.275805	25281.389213	30.654618
463.589489	25316.982683	30.659636
463.861485	25373.063265	30.664653
464.906755	25421.162111	30.669671
464.976946	25471.160418	30.674688
465.788663	25517.169093	30.679706
466.194328	25558.542137	30.684724
466.712284	25609.602269	30.689741
467.144316	25647.154542	30.694759
467.083525	25693.409007	30.699776
468.121502	25746.676631	30.704794
468.626230	25798.288353	30.709812
468.949009	25841.536810	30.714829
469.528111	25873.655659	30.719847
469.825205	25931.367821	30.724864
470.413366	25974.222570	30.729882
471.189331	26013.381043	30.734900
471.202184	26066.980166	30.739917
472.128029	26102.682143	30.744935
472.529849	26151.984063	30.749952
472.663965	26205.998848	30.754970
473.441427	26241.467013	30.759988
473.612236	26298.072042	30.765005
474.198031	26333.184126	30.770023
474.527495	26383.426063	30.775040
474.730390	26432.020422	30.780058
475.349825	26472.117456	30.785076
475.801280	26520.399654	30.790093
476.337002	26567.131846	30.795111
476.898037	26623.947801	30.800128
477.428438	26683.863505	30.805146
478.187734	26723.073665	30.810164
478.641336	26776.747155	30.815181
479.049701	26817.599132	30.820199
479.457039	26868.958886	30.825216
479.826182	26912.331684	30.830234
480.497340	26944.427830	30.835252
481.069226	26991.221427	30.840269
481.617115	27042.085264	30.845287
481.782148	27083.479699	30.850304
482.115990	27130.470789	30.855322
482.998088	27164.292653	30.860340
483.282465	27213.818922	30.865357
483.885077	27245.885961	30.870375
484.078933	27286.295051	30.875392
484.347957	27335.906226	30.880410
485.306083	27376.368866	30.885428
485.153476	27428.728293	30.890445
485.729224	27474.011519	30.895463
486.343932	27522.455615	30.900480
486.757842	27573.639712	30.905498
487.458064	27619.615657	30.910516
487.663229	27665.118434	30.915533
488.294241	27705.336285	30.920551
488.820380	27752.265690	30.925568
488.905190	27807.792067	30.930586
489.938325	27851.028944	30.935604
490.153248	27913.565823	30.940621
490.475209	27959.403363	30.945639
491.396777	28011.668814	30.950656
491.386034	28080.884215	30.955674
491.968832	28122.076341	30.960692
492.586259	28178.427469	30.965709
493.339434	28227.342750	30.970727
493.636941	28275.551200	30.975744
493.900877	28334.336828	30.980762
494.612950	28378.871110	30.985780
494.949571	28432.726810	30.990797
496.138424	28486.290225	30.995815
496.475139	28553.759058	31.000832
496.639827	28601.296337	31.005850
497.319593	28646.038554	31.010868
497.422316	28708.167795	31.015885
498.436324	28761.284615	31.020903
498.813221	28812.162994	31.025920
499.257232	28875.028213	31.030938
500.232049	28909.361839	31.035956
500.507775	28967.731210	31.040973
500.842493	29013.458988	31.045991
501.544306	29057.917831	31.051008
501.854882	29115.606789	31.056026
502.680046	29159.117948	31.061044
503.207479	29209.597144	31.066061
503.426160	29256.878034	31.071079
504.454690	29299.081312	31.076096
504.396773	29353.601410	31.081114
505.210692	29404.576408	31.086132
505.580991	29451.889525	31.091149
506.164008	29507.218973	31.096167
506.618875	29552.868335	31.101184
507.015738	29602.307052	31.106202
507.823565	29654.378555	31.111220
507.932263	29712.585593	31.116237
508.267640	29755.901644	31.121255
508.772190	29807.345464	31.126272
509.741244	29861.372240	31.131290
510.287872	29916.860442	31.136308
510.467650	29973.696772	31.141325
511.234872	30035.036120	31.146343
511.949224	30074.478968	31.151360
512.378149	30123.005194	31.156378
512.902122	30160.230186	31.161396
513.500610	30207.031166	31.166413
513.943063	30261.130536	31.171431
514.780835	30300.663898	31.176448
515.257961	30345.402975	31.181466
515.553127	30383.953578	31.186484
516.046771	30427.655260	31.191501
516.553239	30481.508082	31.196519
516.918908	30516.210691	31.201536
517.260295	30570.595921	31.206554
517.977846	30603.634516	31.211572
518.421682	30650.380233	31.216589
518.516354	30698.354412	31.221607
519.082537	30747.285594	31.226624
519.342713	30805.764610	31.231642
520.099289	30849.562660	31.236660
520.412485	30900.943532	31.241677
520.768036	30963.143033	31.246695
521.149884	31014.440305	31.251712
521.556987	31077.202770	31.256730
522.379674	31134.535955	31.261748
522.503779	31209.073711	31.266765
522.881288	31272.068942	31.271783
523.924990	31329.852100	31.276800
524.149323	31389.885061	31.281818
524.870653	31444.427828	31.286836
525.284696	31508.844047	31.291853
525.648918	31583.987331	31.296871
526.496935	31633.836705	31.301888
526.808652	31704.748441	31.306906
527.796393	31770.926021	31.311924
528.442001	31823.974234	31.316941
528.786397	31895.909972	31.321959
529.554148	31958.344526	31.326976
529.940281	32010.540106	31.331994
530.624146	32066.561400	31.337012
530.648668	32120.735619	31.342029
531.636888	32180.947781	31.347047
532.432932	32234.915803	31.352064
532.640710	32305.181342	31.357082
533.511245	32360.147159	31.362100
533.765960	32429.979440	31.367117
534.211064	32484.949773	31.372135
535.011077	32541.559200	31.377152
535.727156	32605.572857	31.382170
536.465102	32656.131220	31.387188
536.529491	32700.755221	31.392205
537.063700	32763.691957	31.397223
537.779531	32816.103569	31.402240
538.186682	32877.424011	31.407258
538.825812	32937.475615	31.412276
539.434052	32992.041857	31.417293
539.855027	33055.610540	31.422311
540.646486	33105.394523	31.427328
541.178075	33169.604826	31.432346
541.629675	33226.280395	31.437364
542.446253	33281.996404	31.442381
542.870306	33340.595506	31.447399
543.377597	33390.297924	31.452416
543.776835	33448.279827	31.457434
544.045538	33504.942364	31.462452
544.735135	33563.088024	31.467469
545.323623	33626.347014	31.472487
545.859834	33680.220410	31.477504
546.288828	33749.259035	31.482522
546.763943	33801.833294	31.487540
547.610407	33871.320850	31.492557
547.999589	33924.884805	31.497575
548.665234	33977.607932	31.502592
548.958451	34035.524077	31.507610
549.997760	34097.028128	31.512628
550.534850	34151.672804	31.517645
550.963028	34208.055565	31.522663
551.548533	34261.477592	31.527680
551.709739	34330.064151	31.532698
552.363433	34390.364385	31.537716
553.282065	34430.998122	31.542733
553.512089	34497.033503	31.547751
554.124962	34544.828166	31.552768
554.775275	34594.112631	31.557786
555.206401	34642.209029	31.562804
556.003287	34696.203301	31.567821
556.260663	34751.350531	31.572839
556.885478	34797.379760	31.577856
557.163746	34861.338242	31.582874
557.839930	34921.024297	31.587892
557.981857	34981.089292	31.592909
558.377115	35041.961514	31.597927
559.202386	35110.709431	31.602944
559.664609	35176.961365	31.607962
560.206531	35235.373585	31.612980
561.126303	35302.976770	31.617997
561.216750	35361.558779	31.623015
561.960135	35427.569444	31.628032
562.674537	35491.596867	31.633050
562.886475	35565.068386	31.638068
563.664757	35620.921095	31.643085
564.350878	35701.100162	31.648103
564.930832	35760.451447	31.653120
565.379148	35834.045909	31.658138
566.392896	35889.020979	31.663156
566.924533	35956.334200	31.668173
567.600557	36015.367446	31.673191
568.250819	36076.172564	31.678208
568.568451	36136.022967	31.683226
569.279645	36198.399627	31.688244
569.807219	36256.530323	31.693261
570.599528	36321.892316	31.698279
571.247964	36383.402591	31.703296
571.758929	36447.836338	31.708314
572.295402	36501.453031	31.713332
572.959977	36556.276443	31.718349
573.171859	36626.498257	31.723367
574.297158	36683.837066	31.728384
574.532881	36744.492085	31.733402
575.051726	36807.398198	31.738420
575.286201	36874.584098	31.743437
576.076935	36940.614555	31.748455
576.650301	36995.779483	31.753472
577.144788	37075.930070	31.758490
577.558937	37145.366076	31.763508
578.553527	37199.095256	31.768525
578.663110	37283.890233	31.773543
579.264250	37345.774576	31.778560
580.338695	37408.410935	31.783578
580.249478	37482.987963	31.788596
581.043790	37538.357865	31.793613
581.591694	37624.451766	31.798631
582.339585	37685.864781	31.803648
582.966593	37753.364593	31.808666
583.246586	37817.027065	31.813684
584.082716	37881.200620	31.818701
584.588418	37962.792585	31.823719
585.428723	38023.370778	31.828736
586.194390	38099.308192	31.833754
586.403620	38168.621027	31.838772
587.108339	38229.257058	31.843789
587.805183	38300.389915	31.848807
588.272161	38366.450707	31.853824
588.783615	38424.471061	31.858842
589.358804	38501.581164	31.863860
590.354693	38565.134113	31.868877
590.619358	38632.046881	31.873895
591.083004	38697.250839	31.878912
591.799309	38755.721305	31.883930
592.388533	38825.021106	31.888948
593.001902	38886.375195	31.893965
593.525572	38941.427974	31.898983
594.308234	39001.595968	31.904000
594.604526	39068.110520	31.909018
594.965311	39136.091947	31.914036
595.875256	39190.263999	31.919053
596.528510	39264.154095	31.924071
596.888458	39329.731008	31.929088
597.553026	39388.085788	31.934106
597.661136	39471.940998	31.939124
598.277896	39531.390045	31.944141
598.644386	39613.296505	31.949159
599.569066	39691.726965	31.954176
600.169186	39767.121010	31.959194
600.611281	39841.506093	31.964212
601.465317	39902.530185	31.969229
602.169417	39987.084643	31.974247
602.834631	40064.972464	31.979264
603.413400	40137.539918	31.984282
603.707796	40212.557043	31.989300
604.565222	40284.308709	31.994317
605.077393	40361.004567	31.999335
605.765085	40434.290712	32.004352
606.144235	40513.364225	32.009370
606.711240	40598.335622	32.014388
607.624738	40666.906833	32.019405
608.381915	40742.758734	32.024423
608.819467	40825.504876	32.029440
609.793326	40897.987857	32.034458
609.809353	40979.156507	32.039476
611.087489	41043.703665	32.044493
611.742641	41121.057770	32.049511
612.334992	41193.257762	32.054528
613.562925	41254.385478	32.059546
613.686350	41330.900277	32.064564
614.411852	41389.194489	32.069581
614.900403	41466.852264	32.074599
615.504666	41543.581991	32.079616
616.338343	41610.297783	32.084634
617.048210	41681.261612	32.089652
617.451562	41736.030101	32.094669
618.059178	41821.132991	32.099687
618.231311	41889.771408	32.104704
618.959064	41956.528070	32.109722
619.526159	42048.158146	32.114740
620.275404	42112.278767	32.119757
620.738410	42189.792250	32.124775
621.426085	42275.212318	32.129792
622.027850	42340.406306	32.134810
622.581487	42427.165791	32.139828
623.384836	42490.132703	32.144845
624.377491	42572.355947	32.149863
624.737962	42644.925141	32.154880
625.330854	42717.983425	32.159898
625.744207	42795.873886	32.164916
626.519698	42864.273996	32.169933
627.250788	42938.993106	32.174951
627.932438	43017.746244	32.179968
628.956041	43086.245043	32.184986
629.012110	43157.477377	32.190004
629.691567	43228.524757	32.195021
630.671738	43297.883997	32.200039
630.696300	43368.213031	32.205056
631.468008	43436.783206	32.210074
632.159803	43528.355722	32.215092
632.854198	43591.031797	32.220109
633.493920	43662.788342	32.225127
633.498079	43745.792829	32.230144
634.551475	43805.846408	32.235162
635.465480	43885.739324	32.240180
635.799284	43950.272841	32.245197
636.524653	44016.607860	32.250215
636.970616	44080.659123	32.255232
638.121963	44160.671820	32.260250
638.583680	44237.663553	32.265268
639.444841	44305.009629	32.270285
639.764662	44374.422114	32.275303
640.535838	44438.907055	32.280320
641.237772	44503.820469	32.285338
641.551041	44585.726066	32.290356
642.447759	44647.229164	32.295373
642.998050	44725.572312	32.300391
643.486550	44789.050588	32.305408
644.650682	44860.807054	32.310426
645.218319	44939.445037	32.315444
645.848376	45016.001616	32.320461
646.278899	45076.926459	32.325479
647.133997	45157.844977	32.330496
647.561417	45226.516542	32.335514
647.983851	45306.746281	32.340532
648.530793	45384.593809	32.345549
649.426226	45468.427851	32.350567
650.053211	45546.145968	32.355584
650.815585	45620.204300	32.360602
651.092277	45708.755216	32.365620
651.702527	45776.154380	32.370637
652.625874	45863.809602	32.375655
652.783371	45944.613225	32.380672
653.985833	46026.251655	32.385690
654.634871	46122.113207	32.390708
655.206742	46197.755803	32.395725
655.664139	46287.776340	32.400743
656.411471	46366.744211	32.405760
657.381735	46447.210254	32.410778
657.756418	46537.580393	32.415796
658.270511	46612.924730	32.420813
659.024113	46699.216109	32.425831
659.559017	46789.286201	32.430848
660.712856	46869.938406	32.435866
660.923506	46963.843019	32.440884
661.555853	47044.392759	32.445901
662.579827	47136.189942	32.450919
663.185259	47220.881839	32.455936
664.045505	47293.664158	32.460954
665.047497	47385.504077	32.465972
665.233322	47462.140870	32.470989
666.065970	47538.345685	32.476007
666.688702	47633.976040	32.481024
667.508901	47705.209631	32.486042
667.993307	47797.579290	32.491060
668.438006	47877.933054	32.496077
669.323947	47959.041587	32.501095
669.845361	48051.523200	32.506112
670.127004	48130.231188	32.511130
671.071325	48222.927901	32.516148
671.918674	48313.878842	32.521165
672.429228	48394.820777	32.526183
672.692211	48481.804598	32.531200
673.682931	48571.763477	32.536218
674.221805	48665.022085	32.541236
674.821895	48756.120251	32.546253
675.552881	48845.595955	32.551271
676.129782	48939.986583	32.556288
677.108105	49030.038094	32.561306
677.861684	49113.627407	32.566324
678.360355	49196.280174	32.571341
678.939502	49275.600571	32.576359
679.648739	49362.527187	32.581376
680.631991	49433.620213	32.586394
680.650674	49515.772616	32.591412
681.540732	49605.156055	32.596429
682.208696	49684.371850	32.601447
682.962473	49772.821616	32.606464
683.569146	49852.878906	32.611482
684.250912	49958.412754	32.616500
684.800842	50044.743427	32.621517
685.832217	50127.324695	32.626535
686.411716	50223.442548	32.631552
686.955750	50305.593522	32.636570
687.566803	50403.368422	32.641588
688.173167	50502.490127	32.646605
688.889043	50591.107835	32.651623
689.765975	50685.087817	32.656640
690.604097	50781.374122	32.661658
691.231099	50871.334418	32.666676
691.738184	50971.239324	32.671693
693.124271	51048.351985	32.676711
693.404151	51157.815533	32.681728
694.081615	51242.405828	32.686746
694.822746	51329.298105	32.691764
695.599859	51421.384013	32.696781
696.228247	51516.318837	32.701799
696.523282	51608.434839	32.706816
697.355041	51711.859189	32.711834
698.120361	51808.705931	32.716852
698.868877	51914.533141	32.721869
699.726843	52003.241183	32.726887
700.460255	52096.588390	32.731904
701.135777	52190.893262	32.736922
701.907676	52290.129366	32.741940
702.643347	52383.111145	32.746957
703.380023	52466.092267	32.751975
703.992786	52577.069187	32.756992
705.155841	52660.909311	32.762010
705.805677	52752.864616	32.767028
706.422023	52848.022715	32.772045
707.001187	52935.808166	32.777063
707.626124	53033.164357	32.782080
708.358360	53129.473461	32.787098
708.945061	53229.383074	32.792116
709.786399	53319.199160	32.797133
710.475527	53417.766012	32.802151
711.195136	53521.862925	32.807168
712.071642	53600.194590	32.812186
712.802791	53692.260890	32.817204
713.175603	53797.699205	32.822221
714.251545	53887.005219	32.827239
715.086289	53985.576101	32.832256
715.692628	54077.544804	32.837274
716.175984	54176.073674	32.842292
716.598657	54263.290705	32.847309
717.920116	54363.097167	32.852327
718.326005	54470.309053	32.857344
719.090275	54566.190241	32.862362
719.836993	54661.935794	32.867380
720.138472	54761.015777	32.872397
721.164065	54864.885930	32.877415
721.607691	54955.760949	32.882432
722.205214	55051.362466	32.887450
722.842433	55165.269093	32.892468
723.718386	55265.513967	32.897485
724.624820	55370.335318	32.902503
725.140195	55470.508183	32.907520
725.931542	55569.763921	32.912538
726.877361	55658.157980	32.917556
727.320211	55751.355745	32.922573
728.145183	55836.826048	32.927591
728.505696	55932.464695	32.932608
729.498772	56033.016330	32.937626
730.293662	56126.618895	32.942644
731.312879	56226.484745	32.947661
732.072408	56318.602800	32.952679
732.135907	56415.341840	32.957696
733.199763	56522.361182	32.962714
733.866941	56618.969755	32.967732
734.497094	56730.371536	32.972749
735.223909	56828.532068	32.977767
735.694287	56935.778179	32.982784
736.522277	57042.523369	32.987802
737.450663	57139.337697	32.992820
738.003361	57250.439226	32.997837
738.612619	57355.901549	33.002855
739.600766	57476.670295	33.007872
740.192306	57581.289947	33.012890
741.072660	57683.347261	33.017908
741.631211	57803.854111	33.022925
742.455886	57897.738095	33.027943
743.381883	58017.123778	33.032960
743.860985	58136.811595	33.037978
744.826815	58242.131116	33.042996
745.888733	58357.028416	33.048013
746.820751	58453.551463	33.053031
747.185685	58567.225494	33.058048
748.022879	58676.455148	33.063066
749.147546	58780.695825	33.068084
749.772431	58894.897477	33.073101
750.361077	59005.086386	33.078119
751.133134	59104.950576	33.083136
751.964845	59202.504968	33.088154
752.950412	59311.144725	33.093172
753.695339	59427.636285	33.098189
754.289979	59525.724403	33.103207
755.086395	59641.235402	33.108224
755.720401	59744.538373	33.113242
756.604615	59849.051852	33.118260
757.169443	59971.030524	33.123277
758.209617	60073.048206	33.128295
758.847006	60187.419396	33.133312
759.311823	60296.807867	33.138330
760.371565	60410.832363	33.143348
761.073902	60523.854815	33.148365
762.070519	60623.689336	33.153383
762.995060	60730.893120	33.158400
763.448523	60830.281268	33.163418
764.646723	60940.183920	33.168436
765.312998	61034.051767	33.173453
765.771995	61148.767559	33.178471
766.394149	61259.209643	33.183488
767.012731	61362.738268	33.188506
768.277644	61471.690988	33.193524
768.710924	61587.753452	33.198541
769.810915	61693.903014	33.203559
770.670669	61801.654064	33.208576
771.044473	61920.243866	33.213594
771.941591	62013.831516	33.218612
772.658799	62138.357817	33.223629
773.753494	62235.598798	33.228647
774.339691	62348.366103	33.233664
775.054730	62456.018107	33.238682
776.215407	62556.290023	33.243700
776.396616	62662.748268	33.248717
777.267692	62760.287877	33.253735
778.423981	62856.023541	33.258752
778.876988	62964.024949	33.263770
779.888022	63055.967681	33.268788
780.141421	63163.883051	33.273805
781.004653	63262.930749	33.278823
781.679157	63370.227609	33.283840
782.425705	63482.563719	33.288858
783.478618	63586.682777	33.293876
784.039410	63700.365604	33.298893
784.617859	63808.919587	33.303911
785.287944	63923.419967	33.308928
785.987111	64036.462262	33.313946
786.817248	64151.430491	33.318964
787.666334	64275.334691	33.323981
788.474512	64391.717557	33.328999
789.246978	64505.357139	33.334016
789.903705	64620.268144	33.339034
791.230365	64745.505852	33.344052
791.705683	64866.535876	33.349069
792.921463	64967.758602	33.354087
793.871067	65082.604752	33.359104
794.353064	65209.704449	33.364122
795.466297	65311.609585	33.369140
796.090978	65433.794033	33.374157
796.691272	65536.872452	33.379175
797.517574	65655.661657	33.384192
798.346345	65778.244245	33.389210
799.214900	65888.607065	33.394228
799.803009	66011.610138	33.399245
800.597981	66138.973487	33.404263
801.381268	66258.898537	33.409280
802.019353	66393.490146	33.414298
802.935045	66509.190565	33.419316
803.617300	66631.328215	33.424333
804.673429	66760.593028	33.429351
805.418674	66883.410838	33.434368
806.333443	67015.438106	33.439386
807.135827	67135.630531	33.444404
807.969697	67263.544292	33.449421
808.725419	67380.445584	33.454439
809.540965	67514.673597	33.459456
810.672415	67637.362372	33.464474
811.659560	67752.526715	33.469492
811.856837	67887.263989	33.474509
813.177661	67993.124645	33.479527
813.917392	68123.082384	33.484544
814.592666	68250.269636	33.489562
815.557883	68368.741355	33.494580
816.259645	68503.544523	33.499597
817.041310	68619.967841	33.504615
817.826768	68743.308257	33.509632
818.492016	68879.947124	33.514650
819.405966	68988.990857	33.519668
820.064007	69113.492600	33.524685
820.810885	69253.180623	33.529703
821.588930	69381.375623	33.534720
822.218616	69516.816771	33.539738
823.280844	69646.812672	33.544756
823.910070	69781.680180	33.549773
824.680270	69906.888824	33.554791
825.852716	70035.882459	33.559808
826.475535	70173.586257	33.564826
827.525247	70301.286569	33.569844
828.530338	70428.198293	33.574861
829.219303	70563.263181	33.579879
830.044933	70682.548591	33.584896
830.822062	70815.090121	33.589914
831.655434	70930.347644	33.594932
832.588904	71049.990336	33.599949
833.130134	71167.814173	33.604967
834.182582	71285.351751	33.609984
834.977260	71412.645552	33.615002
835.641430	71532.297520	33.620020
836.447979	71658.117412	33.625037
837.383947	71788.760545	33.630055
838.331363	71911.358849	33.635072
838.876975	72038.918860	33.640090
839.588534	72168.665491	33.645108
840.645100	72295.573367	33.650125
841.459559	72423.230298	33.655143
842.349922	72551.805035	33.660160
842.909214	72690.224697	33.665178
843.893382	72821.599655	33.670196
844.860993	72957.563035	33.675213
845.579033	73088.749634	33.680231
846.520354	73221.304036	33.685248
847.079661	73349.312156	33.690266
848.235290	73485.146546	33.695284
849.037820	73631.101951	33.700301
849.814922	73776.177144	33.705319
850.968499	73897.848186	33.710336
851.944284	74045.852062	33.715354
852.607537	74175.504795	33.720372
853.746805	74314.401699	33.725389
854.527086	74443.322005	33.730407
855.772331	74583.822140	33.735424
856.282913	74711.365622	33.740442
857.227706	74839.565353	33.745460
857.976896	74969.796744	33.750477
858.494582	75113.987650	33.755495
859.683259	75236.577379	33.760512
860.701904	75389.111660	33.765530
861.481810	75526.349014	33.770548
862.555208	75659.395960	33.775565
863.122766	75795.670793	33.780583
863.837548	75938.664399	33.785600
864.771617	76074.051777	33.790618
865.471217	76212.818318	33.795636
866.400020	76357.322511	33.800653
867.070095	76507.828591	33.805671
868.047959	76636.501329	33.810688
869.075130	76795.115929	33.815706
869.754289	76934.921352	33.820724
870.722603	77074.565978	33.825741
871.715046	77227.977469	33.830759
872.750172	77360.155415	33.835776
873.294354	77514.927039	33.840794
874.559276	77651.812678	33.845812
875.439651	77798.630331	33.850829
876.290867	77934.030076	33.855847
877.242164	78070.356581	33.860864
877.902234	78213.184077	33.865882
878.613361	78354.776887	33.870900
879.815927	78502.077211	33.875917
880.431816	78641.511583	33.880935
881.513603	78782.090620	33.885952
882.244478	78944.109407	33.890970
882.858633	79077.695502	33.895988
883.959604	79221.765917	33.901005
884.854602	79375.682655	33.906023
886.196282	79503.951138	33.911040
887.065371	79657.880412	33.916058
888.030695	79795.176585	33.921076
888.748631	79933.741744	33.926093
889.616500	80066.785653	33.931111
890.647579	80185.253451	33.936128
891.486920	80322.592637	33.941146
892.420363	80450.864418	33.946164
893.164355	80570.336949	33.951181
893.828317	80708.662722	33.956199
894.957750	80837.941772	33.961216
895.666984	80975.319072	33.966234
896.285932	81115.033884	33.971252
897.348077	81255.258281	33.976269
897.923104	81393.735775	33.981287
898.737537	81533.458779	33.986304
899.639607	81686.415745	33.991322
900.481455	81825.807026	33.996340
901.804703	81956.730560	34.001357
902.012986	82123.280700	34.006375
903.247036	82267.721686	34.011392
904.029653	82417.552633	34.016410
904.824326	82566.110896	34.021428
905.899035	82722.013444	34.026445
906.560034	82876.941545	34.031463
907.639386	83034.642251	34.036480
908.829709	83196.602650	34.041498
909.488228	83351.382506	34.046516
910.741681	83499.219244	34.051533
911.727072	83655.876806	34.056551
912.581846	83816.663280	34.061568
913.224541	83967.476493	34.066586
914.311336	84125.196065	34.071604
915.461418	84275.598364	34.076621
916.007542	84437.946054	34.081639
916.917578	84593.344316	34.086656
917.786451	84749.807082	34.091674
918.898368	84906.623002	34.096692
920.004120	85068.464939	34.101709
920.844326	85234.888680	34.106727
921.819560	85385.080295	34.111744
923.123899	85541.893975	34.116762
923.759834	85694.206455	34.121780
924.656736	85846.255303	34.126797
925.610273	86004.193129	34.131815
926.970232	86163.026617	34.136832
927.803618	86319.569036	34.141850
928.584133	86481.765607	34.146868
929.994591	86626.565228	34.151885
930.492958	86785.539077	34.156903
931.379332	86941.899694	34.161920
932.405544	87094.390842	34.166938
933.062858	87249.323295	34.171956
934.428878	87402.443661	34.176973
935.081752	87561.713585	34.181991
935.986056	87729.023983	34.187008
937.000921	87878.718718	34.192026
937.707371	88028.009771	34.197044
938.655060	88186.842795	34.202061
939.566100	88356.327083	34.207079
940.624442	88517.377896	34.212096
941.493441	88675.151382	34.217114
942.407231	88843.221131	34.222132
943.704956	88995.261926	34.227149
944.616939	89156.872852	34.232167
945.225315	89315.661927	34.237184
946.348957	89474.828835	34.242202
947.115552	89640.156620	34.247220
948.639265	89799.677218	34.252237
949.256899	89960.418260	34.257255
950.512265	90115.966618	34.262272
951.249330	90271.399172	34.267290
952.035973	90424.349965	34.272308
953.147184	90562.267667	34.277325
954.248663	90708.130522	34.282343
955.056746	90850.023908	34.287360
955.836985	91004.612304	34.292378
956.487282	91155.754881	34.297396
958.035830	91290.617139	34.302413
958.848986	91465.500276	34.307431
959.498828	91606.291360	34.312448
960.645523	91761.159433	34.317466
961.328133	91918.611600	34.322484
962.457862	92065.376711	34.327501
963.175971	92225.736448	34.332519
964.062625	92386.309885	34.337536
965.046563	92546.121428	34.342554
965.926449	92713.438914	34.347572
967.153454	92871.927527	34.352589
968.044961	93048.353467	34.357607
969.108661	93213.384351	34.362624
969.978095	93374.770984	34.367642
970.633956	93546.365700	34.372660
971.831204	93707.909195	34.377677
973.020058	93880.582771	34.382695
973.740024	94040.776863	34.387712
975.089241	94205.570982	34.392730
976.039748	94379.990188	34.397748
977.432244	94539.373702	34.402765
978.323410	94700.138777	34.407783
979.304558	94871.701597	34.412800
980.324105	95041.778034	34.417818
981.267914	95206.114147	34.422836
982.134985	95362.291891	34.427853
983.056457	95533.951454	34.432871
983.833334	95699.559143	34.437888
985.209370	95877.336826	34.442906
985.963659	96053.534737	34.447924
986.906066	96214.358119	34.452941
988.015805	96384.011026	34.457959
988.576303	96561.111821	34.462976
989.828805	96731.287893	34.467994
990.806619	96904.574496	34.473012
991.855351	97072.330354	34.478029
993.158176	97254.023212	34.483047
993.927571	97432.576975	34.488064
995.174105	97595.106185	34.493082
996.134101	97782.132983	34.498100
997.351979	97940.718806	34.503117
998.489492	98112.031126	34.508135
999.152058	98290.513670	34.513152
1000.356871	98455.942186	34.518170
1001.050147	98633.535750	34.523188
1001.994518	98799.231156	34.528205
1003.051109	98979.020886	34.533223
1003.928538	99154.827630	34.538240
1005.324681	99326.162377	34.543258
1006.016627	99504.446008	34.548276
1006.953065	99685.900365	34.553293
1008.340297	99851.694012	34.558311
1008.957405	100037.939424	34.563328
1010.220118	100209.669385	34.568346
1010.974960	100388.683219	34.573364
1012.228973	100562.474675	34.578381
1013.285101	100737.224418	34.583399
1014.325321	100905.855441	34.588416
1015.172618	101075.298247	34.593434
1016.295559	101258.075183	34.598452
1017.190580	101428.525473	34.603469
1018.500976	101606.145282	34.608487
1019.231633	101769.343603	34.613504
1020.524073	101926.802162	34.618522
1021.182555	102087.095495	34.623540
1022.378633	102252.961566	34.628557
1023.389521	102418.897309	34.633575
1023.997807	102586.774921	34.638592
1025.402444	102751.140694	34.643610
1025.975524	102926.422014	34.648628
1027.180921	103094.748724	34.653645
1027.949576	103267.169587	34.658663
1028.935912	103445.343135	34.663680
1029.890977	103611.795944	34.668698
1031.178514	103806.259070	34.673716
1032.054341	103982.111636	34.678733
1033.355683	104159.136150	34.683751
1034.039085	104346.649025	34.688768
1034.869965	104517.484750	34.693786
1035.786610	104719.754107	34.698804
1036.818696	104905.047624	34.703821
1038.067250	105089.610076	34.708839
1039.219225	105279.838411	34.713856
1040.164244	105472.204752	34.718874
1041.160509	105672.277161	34.723892
1042.477573	105854.477882	34.728909
1043.455211	106044.297243	34.733927
1044.457094	106247.602746	34.738944
1045.801568	106432.994617	34.743962
1046.507138	106631.374450	34.748980
1047.273040	106807.808598	34.753997
1048.836893	107005.757990	34.759015
1049.721070	107202.415300	34.764032
1051.101683	107395.128817	34.769050
1052.061898	107592.105731	34.774068
1053.305878	107780.107454	34.779085
1054.281099	107975.868738	34.784103
1055.232767	108172.673988	34.789120
1056.708542	108362.300757	34.794138
1057.627362	108557.480260	34.799156
1058.318277	108757.702209	34.804173
1059.409752	108948.878638	34.809191
1060.780460	109145.748355	34.814208
1062.105449	109338.991633	34.819226
1062.884016	109526.208427	34.824244
1063.887002	109719.228969	34.829261
1065.503813	109909.805949	34.834279
1066.426170	110110.062927	34.839296
1067.564007	110295.984205	34.844314
1068.423353	110482.712843	34.849332
1069.591308	110685.758287	34.854349
1071.115189	110865.931848	34.859367
1071.859804	111059.181910	34.864384
1072.738191	111244.937164	34.869402
1073.785056	111445.145299	34.874420
1075.059013	111633.498045	34.879437
1076.091501	111829.442212	34.884455
1077.011215	112035.655015	34.889472
1078.563481	112212.247574	34.894490
1079.472981	112417.033384	34.899508
1080.637938	112605.904837	34.904525
1081.703393	112797.771142	34.909543
1082.420288	112989.062963	34.914560
1083.712689	113184.403632	34.919578
1084.705947	113376.501226	34.924596
1085.912631	113566.398467	34.929613
1087.470524	113758.836080	34.934631
1087.971541	113955.693901	34.939648
1089.384389	114137.262661	34.944666
1090.333578	114330.881717	34.949684
1091.384116	114509.193430	34.954701
1092.360475	114692.155550	34.959719
1093.087010	114873.500453	34.964736
1094.151388	115061.682930	34.969754
1095.384282	115240.792641	34.974772
1096.051087	115428.333783	34.979789
1097.049227	115620.787969	34.984807
1097.430957	115823.367295	34.989824
1098.746250	116022.740241	34.994842
1099.955245	116228.733292	34.999860
1100.541361	116437.706950	35.004877
1101.645797	116649.371241	35.009895
1102.776301	116863.997665	35.014912
1104.181040	117081.177812	35.019930
1105.084488	117302.611107	35.024948
1106.037554	117523.898527	35.029965
1107.377697	117735.569877	35.034983
1108.250743	117958.483055	35.040000
1109.176615	118178.880364	35.045018
1110.745148	118403.075799	35.050036
1111.810535	118622.832541	35.055053
1113.012803	118835.814529	35.060071
1113.816289	119070.050537	35.065088
1115.468983	119293.111181	35.070106
1116.647730	119514.414511	35.075124
1117.784543	119740.047488	35.080141
1118.989220	119958.764877	35.085159
1119.939594	120193.986684	35.090176
1121.325910	120399.853413	35.095194
1122.782879	120629.013794	35.100212
1123.980156	120846.167683	35.105229
1125.216473	121057.791622	35.110247
1126.004969	121278.095622	35.115264
1127.363614	121492.832519	35.120282
1128.906966	121724.420227	35.125300
1129.780108	121944.347683	35.130317
1130.949114	122146.562108	35.135335
1131.878174	122368.460396	35.140352
1133.112336	122582.009156	35.145370
1134.775379	122805.208713	35.150388
1135.531517	123021.095427	35.155405
1136.838489	123229.187353	35.160423
1137.833528	123456.152063	35.165440
1139.249002	123675.001408	35.170458
1140.755766	123883.242261	35.175476
1141.263768	124107.960488	35.180493
1142.666994	124314.599224	35.185511
1143.964212	124533.233544	35.190528
1144.928001	124747.830928	35.195546
1146.170280	124964.018720	35.200564
1147.050438	125185.362853	35.205581
1148.521189	125401.579355	35.210599
1149.561970	125622.773369	35.215616
1150.767493	125837.325793	35.220634
1151.993121	126056.667297	35.225652
1153.166212	126287.400694	35.230669
1154.204958	126497.764725	35.235687
1155.047331	126722.256822	35.240704
1156.223079	126939.534237	35.245722
1157.447764	127158.047221	35.250740
1158.557382	127384.046276	35.255757
1159.966680	127604.775350	35.260775
1161.050546	127835.306919	35.265792
1162.246895	128054.515361	35.270810
1163.479566	128274.251703	35.275828
1164.247207	128493.825636	35.280845
1165.596206	128706.865894	35.285863
1166.686332	128929.342948	35.290880
1167.291423	129141.495097	35.295898
1168.642127	129348.784717	35.300916
1169.837967	129580.261318	35.305933
1171.329223	129791.206592	35.310951
1172.703437	130002.666988	35.315968
1173.410891	130209.396778	35.320986
1174.647754	130428.868626	35.326004
1175.188130	130647.455707	35.331021
1176.482602	130863.713959	35.336039
1177.752763	131087.203233	35.341056
1178.501773	131320.921397	35.346074
1179.794903	131544.879109	35.351092
1180.918320	131785.320733	35.356109
1182.080465	132010.609050	35.361127
1183.141965	132267.100600	35.366144
1184.137052	132495.462372	35.371162
1185.573339	132735.567814	35.376180
1186.487037	132985.155175	35.381197
1187.889941	133227.146000	35.386215
1189.001866	133479.239843	35.391232
1190.046205	133724.082655	35.396250
1191.294632	133974.585772	35.401268
1192.259973	134231.007340	35.406285
1193.739379	134464.513398	35.411303
1195.022699	134724.258535	35.416320
1196.049782	134983.756492	35.421338
1197.488968	135239.562467	35.426356
1198.455069	135495.702191	35.431373
1199.945288	135751.541734	35.436391
1201.242856	136008.010979	35.441408
1202.662970	136260.278083	35.446426
1203.920149	136517.442573	35.451444
1204.922166	136767.246934	35.456461
1206.413848	137030.043939	35.461479
1207.744545	137266.599200	35.466496
1208.880378	137522.777183	35.471514
1210.379608	137765.368601	35.476532
1211.408520	138030.139100	35.481549
1212.862157	138280.425272	35.486567
1214.062470	138521.752909	35.491584
1215.097689	138776.207307	35.496602
1216.581752	139029.511668	35.501620
1217.506928	139283.709108	35.506637
1218.903978	139540.252250	35.511655
1220.429258	139794.924885	35.516672
1221.078043	140046.688462	35.521690
1222.506043	140294.051958	35.526708
1223.660511	140562.168877	35.531725
1225.235502	140804.553866	35.536743
1226.547892	141059.156935	35.541760
1227.728697	141319.540472	35.546778
1228.861944	141569.929013	35.551796
1229.991116	141827.306964	35.556813
1231.156964	142073.458465	35.561831
1232.491496	142332.099613	35.566848
1233.488900	142588.008635	35.571866
1235.170858	142838.011233	35.576884
1235.906665	143097.048645	35.581901
1237.375792	143354.762052	35.586919
1238.899108	143623.310730	35.591936
1239.835472	143881.509154	35.596954
1241.523218	144125.344171	35.601972
1242.281110	144385.909119	35.606989
1243.648374	144635.913033	35.612007
1244.864912	144896.989250	35.617024
1245.868993	145158.901433	35.622042
1247.301064	145411.398339	35.627060
1248.392009	145667.897454	35.632077
1249.732368	145915.467141	35.637095
1250.960009	146156.830291	35.642112
1251.764192	146407.979526	35.647130
1252.922329	146641.836915	35.652148
1254.095596	146910.772444	35.657165
1255.478488	147160.322030	35.662183
1256.874131	147417.480680	35.667200
1257.926240	147679.365092	35.672218
1259.353635	147940.415701	35.677236
1260.422807	148204.266840	35.682253
1261.583419	148452.073690	35.687271
1262.708924	148718.709410	35.692288
1263.917119	148988.986081	35.697306
1265.561200	149246.395451	35.702324
1266.596201	149530.288255	35.707341
1267.836972	149786.360184	35.712359
1269.229537	150058.085391	35.717376
1270.441656	150327.965242	35.722394
1272.034665	150607.043053	35.727412
1272.688355	150866.479050	35.732429
1273.794777	151156.384374	35.737447
1275.199054	151434.713100	35.742464
1276.457259	151722.162367	35.747482
1277.721708	151998.400117	35.752500
1278.735918	152299.237626	35.757517
1280.203831	152586.696790	35.762535
1281.646820	152868.644560	35.767552
1282.622190	153162.747213	35.772570
1284.010684	153449.540986	35.777588
1285.167597	153745.508051	35.782605
1286.464461	154053.086080	35.787623
1287.924429	154341.942232	35.792640
1289.083221	154652.224291	35.797658
1290.270148	154947.447106	35.802676
1291.738945	155244.274608	35.807693
1293.112143	155563.623613	35.812711
1294.343016	155851.120672	35.817728
1295.528367	156168.805782	35.822746
1297.538198	156466.377577	35.827764
1298.640838	156767.869138	35.832781
1299.434706	157068.513324	35.837799
1301.500046	157367.947443	35.842816
1302.608137	157666.451023	35.847834
1304.201244	157975.418649	35.852852
1305.153108	158278.557560	35.857869
1306.505932	158580.693690	35.862887
1308.211506	158878.244786	35.867904
1309.098454	159182.327243	35.872922
1310.819648	159473.130974	35.877940
1312.147921	159777.601611	35.882957
1313.561675	160074.740216	35.887975
1314.892013	160365.475290	35.892992
1315.835651	160671.513105	35.898010
1317.437868	160970.644174	35.903028
1318.728782	161277.098454	35.908045
1320.161873	161585.497970	35.913063
1321.199839	161875.987399	35.918080
1322.409445	162185.887270	35.923098
1323.684327	162482.355457	35.928116
1325.126453	162799.199407	35.933133
1326.377474	163098.111817	35.938151
1328.098591	163396.301561	35.943168
1329.270570	163717.624942	35.948186
1330.706612	164013.683817	35.953204
1331.974809	164320.316065	35.958221
1333.586157	164613.888643	35.963239
1335.257403	164907.415247	35.968256
1335.759715	165209.561922	35.973274
1337.429673	165496.482204	35.978292
1338.782385	165790.955569	35.983309
1339.976414	166071.055848	35.988327
1341.284064	166337.410244	35.993344
1342.240118	166646.584648	35.998362
1343.884075	166935.206176	36.003380
1345.407658	167227.275417	36.008397
1346.014530	167521.705918	36.013415
1347.448295	167815.570277	36.018432
1349.469268	168121.394005	36.023450
1350.085808	168411.654081	36.028468
1351.363221	168711.107913	36.033485
1352.876550	169020.726842	36.038503
1354.390246	169322.620049	36.043520
1355.850985	169629.752020	36.048538
1357.354810	169931.219438	36.053556
1358.516610	170242.516294	36.058573
1359.822646	170553.854860	36.063591
1361.312783	170859.771973	36.068608
1362.149505	171174.326620	36.073626
1363.504344	171497.490322	36.078644
1364.735374	171805.486839	36.083661
1366.253825	172133.767320	36.088679
1367.515772	172445.430337	36.093696
1368.844079	172780.383672	36.098714
1370.218860	173107.514460	36.103732
1372.071267	173441.002587	36.108749
1373.493396	173761.023406	36.113767
1375.026164	174080.215876	36.118784
1376.151791	174415.810604	36.123802
1377.438420	174733.461732	36.128820
1379.281061	175069.310517	36.133837
1380.171469	175395.140872	36.138855
1381.640005	175714.265848	36.143872
1382.871052	176054.397789	36.148890
1384.933551	176386.081959	36.153908
1386.124578	176715.716780	36.158925
1387.351899	177041.502313	36.163943
1388.909516	177367.248076	36.168960
1390.282328	177706.390634	36.173978
1391.426882	178033.401971	36.178996
1392.997580	178371.754799	36.184013
1394.311731	178712.259103	36.189031
1396.158478	179041.420015	36.194048
1397.695866	179381.244599	36.199066
1398.726004	179709.275546	36.204084
1400.282172	180043.681910	36.209101
1401.939163	180385.130605	36.214119
1403.238413	180711.041894	36.219136
1404.498539	181047.052068	36.224154
1406.059794	181380.603070	36.229172
1407.378321	181704.702318	36.234189
1408.463512	182059.253466	36.239207
1409.971347	182385.902172	36.244224
1411.408847	182734.967137	36.249242
1412.495997	183071.488314	36.254260
1414.086624	183407.547602	36.259277
1415.795919	183752.728290	36.264295
1417.006911	184094.985259	36.269312
1418.483205	184443.394766	36.274330
1419.950257	184789.307447	36.279348
1421.605818	185114.869212	36.284365
1422.931546	185460.289012	36.289383
1424.478821	185796.966650	36.294400
1426.126867	186141.474244	36.299418
1427.453036	186477.367419	36.304436
1428.814292	186816.722159	36.309453
1430.250839	187154.670172	36.314471
1431.728449	187464.356996	36.319488
1433.051450	187798.519435	36.324506
1434.458434	188107.954825	36.329524
1435.760898	188423.362632	36.334541
1436.808553	188765.916117	36.339559
1438.197160	189090.389568	36.344576
1439.765588	189414.657379	36.349594
1440.590459	189755.920559	36.354612
1442.339951	190083.513413	36.359629
1443.872203	190430.782264	36.364647
1445.397259	190772.011730	36.369664
1446.843609	191117.445350	36.374682
1447.804309	191455.141284	36.379700
1449.401200	191798.611627	36.384717
1450.087319	192154.269067	36.389735
1451.614497	192506.222329	36.394752
1453.108469	192876.387639	36.399770
1454.561725	193243.692807	36.404788
1456.365387	193601.458996	36.409805
1457.479663	193985.429716	36.414823
1459.289609	194337.955945	36.419840
1460.379587	194711.169510	36.424858
1461.581539	195089.216393	36.429876
1463.690576	195455.994385	36.434893
1464.905656	195824.851895	36.439911
1466.630454	196201.904812	36.444928
1467.759892	196579.566104	36.449946
1469.489083	196954.400873	36.454964
1471.212332	197327.334373	36.459981
1472.198152	197712.262475	36.464999
1474.051801	198079.452774	36.470016
1475.501413	198480.572177	36.475034
1477.002219	198851.684565	36.480052
1478.752359	199227.328396	36.485069
1480.247087	199616.791917	36.490087
1481.541228	200000.336197	36.495104
1482.721427	200383.850628	36.500122
1484.615522	200764.214742	36.505140
1485.979476	201157.390428	36.510157
1487.579569	201546.313999	36.515175
1489.111859	201929.410417	36.520192
1490.774623	202317.946911	36.525210
1492.103237	202715.618915	36.530228
1493.751259	203092.442825	36.535245
1495.481476	203476.758976	36.540263
1496.452921	203860.491459	36.545280
1498.066299	204246.710051	36.550298
1500.044507	204642.050378	36.555316
1501.898933	205028.055385	36.560333
1503.106499	205408.557035	36.565351
1504.501997	205797.790675	36.570368
1506.233810	206186.170769	36.575386
1507.205589	206578.474916	36.580404
1508.920913	206959.954161	36.585421
1510.440309	207350.889223	36.590439
1511.628378	207746.210841	36.595456
1513.421172	208141.205930	36.600474
1514.830741	208532.012513	36.605492
1516.407924	208921.053672	36.610509
1518.118611	209319.991663	36.615527
1519.138008	209710.081040	36.620544
1520.943197	210105.553342	36.625562
1522.558118	210507.941289	36.630580
1523.968277	210912.625239	36.635597
1525.615024	211309.627704	36.640615
1527.079905	211693.862213	36.645632
1528.591240	212096.300102	36.650650
1529.866315	212486.791620	36.655668
1531.560998	212868.961564	36.660685
1532.947498	213257.482500	36.665703
1534.109042	213624.962738	36.670720
1536.074374	214008.210268	36.675738
1536.892046	214394.112551	36.680756
1538.675483	214774.802808	36.685773
1539.889229	215180.681431	36.690791
1541.512831	215581.287587	36.695808
1543.378018	215980.788816	36.700826
1544.345089	216379.424183	36.705844
1545.884201	216772.201361	36.710861
1547.336347	217193.110057	36.715879
1549.395774	217604.929290	36.720896
1550.693907	218007.326280	36.725914
1551.773210	218415.526445	36.730932
1553.155078	218833.278856	36.735949
1554.656335	219269.604948	36.740967
1556.135321	219685.947841	36.745984
1557.691790	220107.435523	36.751002
1559.216756	220547.953794	36.756020
1561.021619	220981.849310	36.761037
1562.087671	221423.843911	36.766055
1563.235329	221870.424047	36.771072
1565.488345	222315.401000	36.776090
1566.971606	222764.443779	36.781108
1568.170013	223206.067956	36.786125
1570.237728	223646.127828	36.791143
1571.779616	224178.629264	36.796160
1573.526039	224624.409988	36.801178
1574.801168	225088.989897	36.806196
1576.618939	225530.469598	36.811213
1578.388834	225991.465992	36.816231
1579.992496	226449.799133	36.821248
1581.666587	226898.394017	36.826266
1583.303898	227347.174339	36.831284
1585.433905	227793.487169	36.836301
1586.915226	228240.162672	36.841319
1588.663507	228698.098791	36.846336
1590.595041	229140.079981	36.851354
1592.065681	229585.542415	36.856372
1593.505639	230024.534126	36.861389
1595.059600	230474.278313	36.866407
1596.868666	230925.963019	36.871424
1598.860875	231378.457084	36.876442
1600.494171	231823.239072	36.881460
1601.952371	232261.015161	36.886477
1603.709946	232707.684260	36.891495
1605.158814	233158.266619	36.896512
1606.802611	233592.408751	36.901530
1608.277518	234052.895827	36.906548
1609.858421	234490.581512	36.911565
1611.646541	234940.426848	36.916583
1613.116083	235397.514648	36.921600
1615.159388	235832.002937	36.926618
1616.540149	236287.075552	36.931636
1618.240207	236733.104301	36.936653
1620.167348	237177.140654	36.941671
1621.490400	237629.990701	36.946688
1623.196530	238066.572038	36.951706
1624.380649	238522.520727	36.956724
1626.220209	238968.506139	36.961741
1627.761522	239417.183600	36.966759
1629.277139	239879.583449	36.971776
1630.746720	240328.655686	36.976794
1632.663564	240784.792991	36.981812
1634.203260	241245.032483	36.986829
1635.302198	241707.454083	36.991847
1636.858131	242156.236153	36.996864
1638.894458	242595.921781	37.001882
1640.160539	243044.981936	37.006900
1641.639227	243487.479267	37.011917
1643.253800	243925.865047	37.016935
1644.755444	244388.250303	37.021952
1646.947777	244826.796062	37.026970
1648.403380	245281.061463	37.031988
1649.573211	245715.636771	37.037005
1651.224596	246186.306753	37.042023
1652.575093	246646.637337	37.047040
1654.320245	247096.767590	37.052058
1655.716233	247569.818727	37.057076
1657.510779	248030.179356	37.062093
1659.143096	248506.622021	37.067111
1660.297449	248988.910685	37.072128
1662.360205	249466.756720	37.077146
1663.911999	249960.132739	37.082164
1665.621715	250446.878377	37.087181
1667.072664	250936.741009	37.092199
1668.796423	251433.875131	37.097216
1670.638085	251923.851917	37.102234
1672.002004	252425.593477	37.107252
1673.571863	252924.811881	37.112269
1675.547827	253423.074435	37.117287
1676.847781	253930.340101	37.122304
1679.071537	254430.670793	37.127322
1680.717991	254947.837850	37.132340
1682.161894	255454.851889	37.137357
1684.168210	255958.191358	37.142375
1685.702580	256474.793255	37.147392
1687.894374	256978.610449	37.152410
1689.487760	257490.198384	37.157428
1691.102069	257989.182892	37.162445
1693.023525	258508.312329	37.167463
1694.672584	259026.496034	37.172480
1696.441676	259537.242118	37.177498
1698.630092	260042.406361	37.182516
1700.479793	260545.543389	37.187533
1702.264885	261044.067569	37.192551
1703.757500	261554.833482	37.197568
1705.657250	262064.388807	37.202586
1707.311011	262561.105091	37.207604
1708.762478	263083.892870	37.212621
1711.019142	263588.053799	37.217639
1712.286104	264097.331516	37.222656
1714.133753	264601.102087	37.227674
1715.747295	265116.520200	37.232692
1717.338145	265633.364212	37.237709
1719.477130	266138.558802	37.242727
1720.871613	266659.752829	37.247744
1722.995318	267170.664640	37.252762
1724.620708	267683.969886	37.257780
1726.626586	268208.389025	37.262797
1728.749358	268707.639253	37.267815
1730.016770	269221.204990	37.272832
1731.651702	269725.183242	37.277850
1733.498907	270251.912122	37.282868
1735.385106	270757.727229	37.287885
1737.437975	271254.419841	37.292903
1738.608779	271772.036835	37.297920
1740.495810	272281.939253	37.302938
1742.284946	272788.580021	37.307956
1744.023580	273313.060883	37.312973
1745.718844	273819.639095	37.317991
1747.124184	274334.799486	37.323008
1748.832504	274847.520976	37.328026
1750.516249	275372.616460	37.333044
1752.022224	275879.145635	37.338061
1753.966942	276386.337924	37.343079
1755.494955	276887.094938	37.348096
1757.098296	277379.100027	37.353114
1759.202060	277887.862971	37.358132
1760.377003	278392.866178	37.363149
1762.418678	278903.338841	37.368167
1764.029954	279405.549451	37.373184
1766.242049	279919.115793	37.378202
1767.871862	280427.518751	37.383220
1769.516748	280941.379212	37.388237
1771.584063	281449.275269	37.393255
1772.776177	281978.143742	37.398272
1774.354411	282487.463872	37.403290
1775.959112	283018.318539	37.408308
1777.511974	283551.313795	37.413325
1779.286477	284071.087443	37.418343
1780.806561	284630.679695	37.423360
1782.701015	285168.921995	37.428378
1784.514219	285731.891012	37.433396
1786.032026	286273.976353	37.438413
1787.892465	286837.720815	37.443431
1789.624333	287394.829324	37.448448
1791.484043	287960.423735	37.453466
1793.328040	288524.799214	37.458484
1795.071659	289089.341338	37.463501
1797.119784	289651.443161	37.468519
1798.834137	290228.329812	37.473536
1800.877561	290801.451126	37.478554
1802.666512	291360.413297	37.483572
1804.153252	291941.342936	37.488589
1806.181460	292512.680896	37.493607
1807.817407	293097.339517	37.498624
1809.679888	293668.546914	37.503642
1811.603715	294253.685616	37.508660
1813.500203	294830.317105	37.513677
1815.563148	295411.312192	37.518695
1817.056167	296003.700889	37.523712
1819.157915	296587.655029	37.528730
1821.268647	297175.338115	37.533748
1823.087175	297760.958115	37.538765
1824.740923	298339.338098	37.543783
1826.853688	298927.061765	37.548800
1828.513740	299508.862833	37.553818
1830.444032	300092.977887	37.558836
1832.058957	300684.176740	37.563853
1834.097994	301286.324522	37.568871
1836.031996	301875.710928	37.573888
1837.911088	302463.324906	37.578906
1839.973128	303046.562046	37.583924
1841.797982	303639.612492	37.588941
1843.859331	304211.210477	37.593959
1845.785028	304809.773067	37.598976
1847.623526	305386.428833	37.603994
1849.671381	305974.499952	37.609012
1851.242188	306558.303095	37.614029
1853.446289	307130.721840	37.619047
1855.297526	307730.571624	37.624064
1857.281005	308317.595852	37.629082
1859.346101	308899.650294	37.634100
1860.884304	309477.241820	37.639117
1863.131255	310051.944084	37.644135
1864.311642	310638.576139	37.649152
1866.416538	311222.867193	37.654170
1868.488270	311793.192347	37.659188
1870.321289	312378.281378	37.664205
1872.316167	312959.834781	37.669223
1873.865793	313544.758412	37.674240
1875.908970	314118.854395	37.679258
1878.136143	314672.905419	37.684276
1880.042749	315226.903587	37.689293
1881.575068	315775.779104	37.694311
1883.463911	316328.019571	37.699328
1885.161060	316883.740789	37.704346
1887.256240	317432.332744	37.709364
1889.022583	317999.942726	37.714381
1891.173339	318549.100648	37.719399
1892.673278	319113.571361	37.724416
1894.349588	319678.592233	37.729434
1896.321886	320250.237407	37.734452
1898.455983	320828.604997	37.739469
1900.107174	321391.837999	37.744487
1902.161784	321964.394101	37.749504
1903.801594	322544.097577	37.754522
1905.822671	323122.463311	37.759540
1907.200809	323714.031217	37.764557
1909.341124	324289.015045	37.769575
1911.228271	324885.210308	37.774592
1913.311191	325482.687715	37.779610
1915.067637	326077.293426	37.784628
1917.026543	326679.425744	37.789645
1918.772129	327268.867532	37.794663
1920.576163	327874.364660	37.799680
1922.254095	328485.563318	37.804698
1924.640800	329097.450952	37.809716
1926.460950	329714.350852	37.814733
1928.306366	330323.903016	37.819751
1930.591436	330949.750675	37.824768
1932.376122	331566.103210	37.829786
1934.497180	332169.192449	37.834804
1935.575717	332799.432772	37.839821
1937.703649	333429.619524	37.844839
1939.630626	334054.881980	37.849856
1942.108441	334692.078874	37.854874
1944.079489	335314.197030	37.859892
1945.669862	335958.988515	37.864909
1947.692646	336585.779348	37.869927
1949.884774	337225.937493	37.874944
1951.871510	337865.613973	37.879962
1954.044886	338493.346848	37.884980
1955.927853	339137.822047	37.889997
1958.065305	339762.321524	37.895015
1959.799773	340404.444452	37.900032
1962.174046	341042.087737	37.905050
1964.085696	341664.950813	37.910068
1965.980190	342311.794337	37.915085
1968.111688	342948.996058	37.920103
1969.945092	343570.527860	37.925120
1971.805416	344228.772743	37.930138
1974.258816	344857.723438	37.935156
1976.247157	345503.087140	37.940173
1978.113554	346138.513350	37.945191
1980.147177	346777.735523	37.950208
1981.953951	347423.863952	37.955226
1984.431894	348058.680595	37.960244
1986.465671	348709.803670	37.965261
1988.171027	349341.963717	37.970279
1990.076964	349973.954862	37.975296
1991.612476	350623.939719	37.980314
1993.851685	351261.516587	37.985332
1995.731444	351924.748149	37.990349
1997.958598	352563.145480	37.995367
2000.063358	353203.609031	38.000384
2001.759968	353861.613866	38.005402
2004.077026	354504.941076	38.010420
2005.679767	355160.226272	38.015437
2007.868630	355787.493232	38.020455
2009.824500	356413.444475	38.025472
2011.344544	357041.767221	38.030490
2013.628121	357673.531928	38.035508
2015.111011	358304.226617	38.040525
2017.145392	358929.796870	38.045543
2019.185574	359571.163020	38.050560
2020.822288	360210.632003	38.055578
2023.119635	360860.206133	38.060596
2024.876244	361502.450802	38.065613
2026.661264	362164.240573	38.070631
2028.480105	362815.104741	38.075648
2030.293106	363478.491354	38.080666
2032.530870	364152.248385	38.085684
2034.304380	364828.175852	38.090701
2036.281380	365501.115150	38.095719
2038.460771	366188.240190	38.100736
2040.316181	366876.953616	38.105754
2042.146806	367559.672063	38.110772
2044.171881	368260.381075	38.115789
2046.099500	368952.595543	38.120807
2048.416936	369644.910222	38.125824
2050.124752	370361.307224	38.130842
2052.114344	371065.519659	38.135860
2054.243351	371790.163668	38.140877
2056.363742	372507.008081	38.145895
2058.280185	373225.647151	38.150912
2060.434824	373950.851807	38.155930
2062.758828	374678.499010	38.160948
2064.577430	375406.747123	38.165965
2066.522449	376141.223139	38.170983
2069.051869	376868.892121	38.176000
2071.341456	377606.373962	38.181018
2073.494081	378332.628613	38.186036
2075.681759	379062.589601	38.191053
2077.970007	379808.417410	38.196071
2080.262890	380530.975497	38.201088
2082.121290	381265.126854	38.206106
2084.429726	382004.284203	38.211124
2086.751093	382740.304135	38.216141
2088.872107	383466.807217	38.221159
2091.018099	384195.166181	38.226176
2092.884590	384933.620292	38.231194
2095.111749	385658.053752	38.236212
2097.026596	386399.001474	38.241229
2099.198340	387137.252940	38.246247
2101.421474	387874.413941	38.251264
2103.510616	388623.824160	38.256282
2105.603501	389359.298614	38.261300
2108.110794	390094.839359	38.266317
2109.941414	390844.188039	38.271335
2112.197958	391580.038924	38.276352
2114.101716	392339.326190	38.281370
2115.802544	393073.382383	38.286388
2118.071130	393825.475037	38.291405
2120.446479	394584.425285	38.296423
2122.784588	395312.314662	38.301440
2124.661032	396076.327607	38.306458
2127.144083	396831.477059	38.311476
2129.562236	397575.745607	38.316493
2131.181711	398320.557867	38.321511
2133.711378	399063.021408	38.326528
2135.863661	399811.204613	38.331546
2138.065814	400551.251150	38.336564
2140.332582	401290.304967	38.341581
2142.416420	402033.880176	38.346599
2144.799702	402771.482544	38.351616
2146.471604	403521.269205	38.356634
2149.250924	404247.340058	38.361652
2150.959877	404969.438816	38.366669
2153.242050	405687.117056	38.371687
2155.696844	406391.801816	38.376704
2157.157286	407110.313328	38.381722
2159.266694	407813.473130	38.386740
2161.242935	408534.420718	38.391757
2163.042345	409256.416935	38.396775
2165.303691	409982.066685	38.401792
2167.422650	410705.541811	38.406810
2169.283447	411451.330817	38.411828
2171.497890	412188.428363	38.416845
2173.337850	412928.555994	38.421863
2175.687923	413682.610531	38.426880
2177.979925	414432.043284	38.431898
2179.917750	415183.615062	38.436916
2182.281634	415956.115454	38.441933
2184.285418	416722.346105	38.446951
2186.567830	417478.707236	38.451968
2188.372855	418249.812628	38.456986
2190.191159	419030.819096	38.462004
2192.673777	419809.564715	38.467021
2194.719743	420596.663767	38.472039
2197.214200	421391.462840	38.477056
2199.184475	422183.867034	38.482074
2201.400664	422982.231262	38.487092
2203.726754	423771.234372	38.492109
2205.532329	424583.438212	38.497127
2208.057807	425382.230307	38.502144
2210.537221	426203.129757	38.507162
2212.655406	427011.049087	38.512180
2215.092606	427818.382360	38.517197
2217.057556	428637.157312	38.522215
2219.764199	429441.353678	38.527232
2222.200311	430262.019895	38.532250
2224.128595	431066.694464	38.537268
2226.542242	431887.257122	38.542285
2228.648105	432697.212058	38.547303
2231.056238	433521.413221	38.552320
2233.140508	434343.107792	38.557338
2235.686189	435165.709161	38.562356
2237.893352	435988.438116	38.567373
2240.299746	436812.875841	38.572391
2242.451415	437630.898624	38.577408
2244.198918	438457.460162	38.582426
2246.874324	439290.619026	38.587444
2249.496548	440111.560783	38.592461
2251.414271	440944.783033	38.597479
2253.694891	441766.580285	38.602496
2256.177286	442598.635168	38.607514
2258.173703	443441.161065	38.612532
2260.676293	444257.870416	38.617549
2262.927310	445103.275092	38.622567
2265.243548	445928.097405	38.627584
2267.645977	446762.738237	38.632602
2269.856167	447602.689698	38.637620
2272.234819	448430.238400	38.642637
2274.051298	449275.449557	38.647655
2276.108115	450109.055605	38.652672
2278.564196	450956.268925	38.657690
2281.121690	451805.858904	38.662708
2283.647173	452638.376964	38.667725
2285.816984	453483.107772	38.672743
2288.302729	454335.792305	38.677760
2290.208901	455172.103441	38.682778
2292.068038	456012.939047	38.687796
2294.610861	456864.801377	38.692813
2296.427114	457712.905491	38.697831
2298.880716	458554.700995	38.702848
2301.359774	459395.193343	38.707866
2303.557107	460211.886569	38.712884
2305.708416	461033.356445	38.717901
2307.622107	461852.557008	38.722919
2310.179015	462692.695677	38.727936
2312.405733	463512.332016	38.732954
2314.444373	464351.828528	38.737972
2316.558417	465185.009673	38.742989
2318.693041	466038.417720	38.748007
2320.726397	466890.288971	38.753024
2323.002550	467757.596559	38.758042
2325.801135	468610.529079	38.763060
2328.279361	469466.760993	38.768077
2330.352343	470342.625908	38.773095
2332.540604	471207.821376	38.778112
2334.964975	472083.901761	38.783130
2337.289204	472952.935777	38.788148
2339.834223	473853.012030	38.793165
2341.763178	474745.518920	38.798183
2344.505619	475627.443260	38.803200
2346.669964	476529.827272	38.808218
2349.210676	477414.881998	38.813236
2351.687648	478305.510813	38.818253
2353.775257	479217.422355	38.823271
2356.190259	480103.883163	38.828288
2358.690487	481015.788153	38.833306
2360.744589	481917.419803	38.838324
2363.554215	482829.384225	38.843341
2365.775785	483743.065558	38.848359
2368.233823	484659.488514	38.853376
2370.687013	485573.946694	38.858394
2372.864364	486503.699423	38.863412
2375.827523	487423.076647	38.868429
2377.863937	488334.482400	38.873447
2380.206651	489272.289302	38.878464
2382.441257	490182.707946	38.883482
2385.006660	491126.283444	38.888500
2387.564338	492047.502647	38.893517
2389.800474	492984.773096	38.898535
2392.018383	493922.701822	38.903552
2394.696398	494856.971097	38.908570
2396.924798	495810.537197	38.913588
2399.673080	496745.145119	38.918605
2401.584791	497691.089608	38.923623
2403.923784	498630.705429	38.928640
2406.630337	499592.201440	38.933658
2408.949509	500543.869935	38.938676
2411.464027	501484.304842	38.943693
2413.945940	502444.764899	38.948711
2416.399144	503402.349493	38.953728
2419.020693	504355.967369	38.958746
2420.800419	505314.307727	38.963764
2423.531738	506271.375771	38.968781
2425.920219	507243.317903	38.973799
2428.356547	508204.505152	38.978816
2431.228200	509158.807600	38.983834
2433.525467	510122.373242	38.988852
2436.219558	511084.958280	38.993869
2438.516533	512038.427179	38.998887
2440.703588	513015.092205	39.003904
2443.570030	513973.995369	39.008922
2445.692609	514945.864088	39.013940
2448.030641	515913.000748	39.018957
2450.460244	516874.368237	39.023975
2453.110044	517850.554287	39.028992
2455.434474	518826.379703	39.034010
2457.486722	519795.538018	39.039028
2460.375816	520751.953166	39.044045
2462.715036	521694.898969	39.049063
2465.069617	522636.171981	39.054080
2467.720457	523580.661981	39.059098
2470.109405	524524.733249	39.064116
2472.789200	525459.027957	39.069133
2475.291177	526397.624629	39.074151
2477.561213	527332.977909	39.079168
2479.695134	528270.460044	39.084186
2481.896557	529225.544225	39.089204
2484.191845	530180.148470	39.094221
2486.598253	531148.617300	39.099239
2489.011703	532122.356977	39.104256
2491.729693	533086.518512	39.109274
2494.020335	534083.100581	39.114292
2496.544906	535047.717640	39.119309
2498.623911	536041.884774	39.124327
2500.893134	537031.775235	39.129344
2503.659403	538044.963713	39.134362
2505.958636	539064.346143	39.139380
2508.422547	540059.227629	39.144397
2510.605588	541080.547443	39.149415
2513.044099	542101.751345	39.154432
2515.909595	543116.925656	39.159450
2518.019098	544158.053919	39.164468
2520.676426	545206.357006	39.169485
2523.168615	546255.865646	39.174503
2525.387584	547302.373149	39.179520
2528.147739	548356.606287	39.184538
2530.679792	549415.924615	39.189556
2533.265447	550462.785012	39.194573
2535.581699	551528.209394	39.199591
2538.221137	552603.399393	39.204608
2541.156393	553667.649088	39.209626
2543.362399	554753.596263	39.214644
2546.191750	555816.186085	39.219661
2548.459052	556919.235271	39.224679
2551.433756	557982.081329	39.229696
2553.810252	559074.382596	39.234714
2556.346166	560167.722997	39.239732
2559.300480	561262.561521	39.244749
2562.116481	562347.235716	39.249767
2564.263599	563449.308183	39.254784
2566.850643	564536.801783	39.259802
2569.466120	565632.334770	39.264820
2572.183756	566733.884114	39.269837
2574.716400	567831.805208	39.274855
2577.266184	568937.863069	39.279872
2579.910557	570037.434550	39.284890
2582.660946	571136.542434	39.289908
2585.371033	572243.341442	39.294925
2587.583151	573342.547807	39.299943
2590.359047	574459.179149	39.304960
2593.184987	575563.760924	39.309978
2595.622143	576683.411373	39.314996
2597.962559	577796.104305	39.320013
2601.061575	578905.763370	39.325031
2603.203026	580023.054999	39.330048
2605.838191	581141.668693	39.335066
2608.316364	582267.478265	39.340084
2610.945891	583373.903609	39.345101
2613.257629	584519.340736	39.350119
2615.316105	585663.207689	39.355136
2618.305271	586786.509995	39.360154
2620.670307	587927.756038	39.365172
2623.051292	589070.194341	39.370189
2625.929414	590228.328815	39.375207
2628.124417	591379.147257	39.380224
2630.756366	592508.837460	39.385242
2632.614324	593646.964879	39.390260
2635.736164	594776.558142	39.395277
2638.297053	595901.526933	39.400295
2640.908196	597030.186198	39.405312
2643.431507	598170.119809	39.410330
2645.306624	599317.109755	39.415348
2648.290959	600452.436712	39.420365
2651.081870	601602.454219	39.425383
2653.385513	602760.597586	39.430400
2655.892527	603923.045724	39.435418
2658.197739	605093.067106	39.440436
2660.807381	606264.719860	39.445453
2663.782940	607442.947109	39.450471
2665.921574	608636.050797	39.455488
2668.153357	609833.665820	39.460506
2671.270293	611048.766627	39.465524
2673.662538	612262.654463	39.470541
2676.481453	613473.138724	39.475559
2678.851270	614703.019128	39.480576
2681.543122	615927.059185	39.485594
2684.009060	617168.250291	39.490612
2686.621477	618415.876108	39.495629
2689.649372	619663.341130	39.500647
2692.437965	620924.247961	39.505664
2695.528275	622163.468886	39.510682
2697.938444	623426.545907	39.515700
2701.024972	624689.713144	39.520717
2704.096798	625936.197913	39.525735
2706.680938	627201.899686	39.530752
2709.384533	628457.292282	39.535770
2712.320931	629723.784758	39.540788
2715.005852	630994.211860	39.545805
2717.970295	632251.508196	39.550823
2720.691540	633530.510465	39.555840
2723.546688	634809.284437	39.560858
2726.518812	636073.108745	39.565876
2729.028367	637351.876876	39.570893
2731.871300	638614.115292	39.575911
2734.674575	639899.405685	39.580928
2737.313803	641169.796128	39.585946
2740.440611	642455.560931	39.590964
2742.886984	643723.969793	39.595981
2745.854734	645007.493544	39.600999
2748.576838	646295.931109	39.606016
2751.455891	647587.867542	39.611034
2754.389398	648876.887367	39.616052
2756.728663	650160.107565	39.621069
2759.869693	651446.519098	39.626087
2762.328080	652750.416581	39.631104
2765.458044	654033.704343	39.636122
2768.074557	655330.509739	39.641140
2770.862776	656635.732936	39.646157
2773.686414	657917.568599	39.651175
2776.185236	659219.556656	39.656192
2779.021405	660529.331076	39.661210
2781.704948	661827.752790	39.666228
2784.703819	663128.088501	39.671245
2787.420182	664433.122893	39.676263
2789.942685	665745.127869	39.681280
2793.179228	667049.769893	39.686298
2795.895385	668363.373420	39.691316
2798.542349	669679.691731	39.696333
2801.438525	670991.061100	39.701351
2804.230520	672300.723770	39.706368
2806.933024	673605.395790	39.711386
2809.991370	674928.569600	39.716404
2812.572332	676242.836435	39.721421
2815.713503	677531.130317	39.726439
2817.832760	678829.501367	39.731456
2820.992509	680096.514227	39.736474
2823.870335	681380.389562	39.741492
2826.331756	682652.629946	39.746509
2828.902714	683924.526322	39.751527
2831.783685	685213.673931	39.756544
2834.608242	686504.336072	39.761562
2837.344649	687794.928078	39.766580
2840.035371	689094.625219	39.771597
2842.654750	690386.304792	39.776615
2845.194545	691702.573166	39.781632
2847.721083	693023.760213	39.786650
2850.512318	694337.266394	39.791668
2853.221735	695673.556755	39.796685
2856.095911	697021.322014	39.801703
2858.778771	698374.515883	39.806720
2861.854488	699726.197075	39.811738
2864.392213	701088.961084	39.816756
2867.042285	702459.671473	39.821773
2869.631483	703832.455298	39.826791
2872.305806	705228.789873	39.831808
2875.531514	706622.925250	39.836826
2878.579492	708015.526685	39.841844
2880.858400	709425.064366	39.846861
2883.552168	710834.400153	39.851879
2886.794303	712250.392547	39.856896
2889.594193	713681.318221	39.861914
2892.702604	715114.276812	39.866932
2895.177610	716549.124779	39.871949
2898.283896	717989.757959	39.876967
2900.970765	719443.963007	39.881984
2903.700727	720893.703590	39.887002
2906.909985	722340.887024	39.892020
2909.444094	723813.339546	39.897037
2912.946149	725277.164450	39.902055
2915.945677	726756.872819	39.907072
2918.767136	728215.343557	39.912090
2922.211447	729678.736913	39.917108
2925.027399	731156.343812	39.922125
2928.163946	732624.788637	39.927143
2931.055427	734106.091122	39.932160
2933.419892	735576.594077	39.937178
2936.927875	737059.323479	39.942196
2939.771516	738542.972804	39.947213
2942.718583	740028.055389	39.952231
2945.744579	741522.466080	39.957248
2948.913608	743003.796824	39.962266
2951.994289	744484.469038	39.967284
2954.819819	745983.638409	39.972301
2958.319166	747465.157265	39.977319
2961.637582	748957.660670	39.982336
2964.559264	750436.589730	39.987354
2967.624409	751911.714854	39.992372
2970.191874	753407.425089	39.997389
2973.739861	754868.901007	40.002407
2976.391380	756362.888667	40.007424
2979.511173	757848.138491	40.012442
2982.428762	759338.200908	40.017460
2985.425419	760822.790834	40.022477
2988.199534	762308.060497	40.027495
2991.223484	763787.437954	40.032512
2994.215635	765296.920308	40.037530
2997.757807	766771.393850	40.042548
3000.681203	768257.278806	40.047565
3003.535926	769736.193848	40.052583
3006.472463	771228.558505	40.057600
3009.401203	772711.730541	40.062618
3012.612007	774169.163089	40.067636
3015.447523	775629.707051	40.072653
3018.545006	777065.072124	40.077671
3021.815029	778502.874793	40.082688
3024.753444	779935.588498	40.087706
3027.424755	781369.779964	40.092724
3030.306621	782818.516542	40.097741
3033.413739	784257.114151	40.102759
3036.488450	785699.596661	40.107776
3038.989167	787158.503541	40.112794
3042.423621	788624.653662	40.117812
3044.917981	790099.575531	40.122829
3048.045415	791555.612883	40.127847
3050.793398	793034.583892	40.132864
3053.697916	794520.123867	40.137882
3056.741420	796012.671133	40.142900
3059.256418	797530.787079	40.147917
3062.691058	799033.002071	40.152935
3065.588650	800545.110019	40.157952
3067.874871	802065.892461	40.162970
3071.287869	803602.588855	40.167988
3074.394843	805149.897297	40.173005
3077.340107	806696.882617	40.178023
3080.696750	808259.237950	40.183040
3083.593876	809822.189650	40.188058
3086.652579	811384.949658	40.193076
3089.364730	812972.512601	40.198093
3092.390757	814546.659097	40.203111
3095.475509	816122.672407	40.208128
3098.587698	817726.181591	40.213146
3101.505982	819323.480713	40.218164
3104.626971	820942.853828	40.223181
3107.541530	822555.474879	40.228199
3111.078222	824174.182282	40.233216
3113.836673	825799.200831	40.238234
3117.144364	827429.233346	40.243252
3120.437481	829059.056041	40.248269
3123.593925	830698.041204	40.253287
3126.575197	832330.357992	40.258304
3129.508040	833980.237426	40.263322
3132.813749	835628.610277	40.268340
3136.119315	837286.779497	40.273357
3139.053306	838938.887354	40.278375
3142.201060	840596.076626	40.283392
3145.450081	842273.337744	40.288410
3148.861389	843927.667149	40.293428
3151.589756	845602.671318	40.298445
3154.868488	847262.658569	40.303463
3158.294013	848940.446349	40.308480
3161.634625	850623.430325	40.313498
3164.532248	852295.253603	40.318516
3168.071667	853980.498797	40.323533
3170.927115	855663.455822	40.328551
3174.316508	857331.990566	40.333568
3177.094616	859022.092935	40.338586
3180.986952	860703.205090	40.343604
3183.875678	862392.549404	40.348621
3186.888428	864071.420976	40.353639
3190.259713	865762.265962	40.358656
3193.540412	867465.243377	40.363674
3196.289470	869157.174113	40.368692
3199.450104	870854.270406	40.373709
3202.789928	872553.660992	40.378727
3206.245434	874249.741075	40.383744
3209.087496	875965.264720	40.388762
3212.394997	877655.169687	40.393780
3215.159149	879365.655431	40.398797
3218.575967	881084.812001	40.403815
3221.970026	882782.309284	40.408832
3224.872165	884457.565607	40.413850
3228.102330	886123.787776	40.418868
3231.362638	887789.718218	40.423885
3234.266903	889445.865798	40.428903
3237.240114	891117.442422	40.433920
3240.387233	892798.725500	40.438938
3243.669812	894493.953161	40.443956
3246.689161	896186.502379	40.448973
3249.865289	897882.182205	40.453991
3252.964157	899573.320413	40.459008
3256.133343	901280.117377	40.464026
3259.047582	902998.663567	40.469044
3262.099637	904725.320752	40.474061
3265.106992	906464.823683	40.479079
3268.789184	908200.593363	40.484096
3271.637582	909952.686160	40.489114
3275.051043	911703.649227	40.494132
3278.257795	913463.889861	40.499149
3281.790678	915241.281802	40.504167
3284.806921	917015.684067	40.509184
3287.954471	918798.989714	40.514202
3291.276092	920587.630169	40.519220
3294.132921	922385.828071	40.524237
3297.547515	924189.855003	40.529255
3300.962747	926002.191097	40.534272
3303.767166	927828.101211	40.539290
3307.535096	929641.348404	40.544308
3310.700747	931471.505366	40.549325
3314.063122	933312.772418	40.554343
3317.285391	935144.711452	40.559360
3320.613135	937000.006774	40.564378
3323.873396	938852.839246	40.569396
3327.380805	940712.716783	40.574413
3330.436212	942579.553283	40.579431
3334.007045	944445.919157	40.584448
3337.373626	946318.710799	40.589466
3340.755888	948191.677533	40.594484
3343.855949	950061.144044	40.599501
3346.651497	951945.906768	40.604519
3350.390030	953878.195142	40.609536
3353.671580	955827.506637	40.614554
3357.003399	957778.009253	40.619572
3360.192407	959733.642477	40.624589
3363.456137	961708.141431	40.629607
3366.800335	963666.419443	40.634624
3370.017131	965649.145704	40.639642
3373.240770	967619.376067	40.644660
3376.485481	969598.879432	40.649677
3379.715874	971600.233956	40.654695
3383.346454	973587.367628	40.659712
3386.459031	975598.460069	40.664730
3389.635108	977603.086104	40.669748
3393.089788	979609.300749	40.674765
3396.388441	981626.617879	40.679783
3400.002936	983631.489250	40.684800
3403.164565	985670.369053	40.689818
3406.556979	987695.349784	40.694836
3409.941722	989708.331992	40.699853
3413.095788	991746.104779	40.704871
3416.973750	993778.557458	40.709888
3420.009264	995818.676395	40.714906
3423.863007	997858.217356	40.719924
3426.918906	999896.766715	40.724941
3430.046689	1001941.264047	40.729959
3434.141555	1003983.310548	40.734976
3437.279723	1006030.980827	40.739994
3440.533269	1008073.139758	40.745012
3444.228420	1010095.247462	40.750016
3447.501472	1012077.649210	40.755021
3450.808337	1013985.773725	40.760026
3453.960434	1015847.186522	40.765031
3456.856796	1017625.963226	40.770036
3460.482135	1019353.631751	40.775040
3462.802801	1020985.302189	40.780045
3466.245424	1022542.367175	40.785050
3469.105001	1024044.353184	40.790055
3472.084583	1025452.539811	40.795060
3475.000483	1026783.781350	40.800064
3477.340170	1028037.732866	40.805069
3479.993033	1029204.232650	40.810074
3482.669550	1030314.062267	40.815079
3484.909544	1031344.398686	40.820084
3487.228406	1032294.523769	40.825088
3489.162363	1033184.964874	40.830093
3491.069055	1034008.244564	40.835098
3493.343585	1034788.406327	40.840103
3494.972121	1035484.735564	40.845108
3496.806893	1036128.157304	40.850112
3498.917524	1036705.048137	40.855117
3500.644313	1037230.712980	40.860122
3501.900830	1037701.411208	40.865127
3503.399002	1038133.855562	40.870132
3505.094599	1038499.940827	40.875136
3506.183316	1038821.554814	40.880141
3507.327414	1039098.499542	40.885146
3508.826596	1039351.989330	40.890151
3509.814126	1039557.918848	40.895156
3511.146906	1039710.838341	40.900160
3511.606859	1039837.425185	40.905165
3512.997596	1039931.973779	40.910170
3513.884677	1039991.340657	40.915175
3514.712418	1040019.994475	40.920180
3515.699216	1040013.938683	40.925184
3516.013441	1039995.530827	40.930189
3516.851310	1039946.410658	40.935194
3517.379104	1039854.831220	40.940199
3518.146276	1039774.224987	40.945204
3518.701468	1039642.445464	40.950208
3519.507409	1039514.872782	40.955213
3520.030112	1039339.805633	40.960218
3520.465571	1039166.486607	40.965223
3520.846973	1038961.959892	40.970228
3521.707927	1038750.389080	40.975232
3521.893131	1038520.463897	40.980237
3521.977547	1038262.133273	40.985242
3522.457411	1038019.575417	40.990247
3522.830372	1037745.130017	40.995252
3523.614439	1037458.811392	41.000256
3523.681787	1037168.149714	41.005261
3523.964209	1036860.230908	41.010266
3524.300382	1036539.525582	41.015271
3524.772338	1036204.664531	41.020276
3524.845901	1035870.912470	41.025280
3524.782061	1035539.386861	41.030285
3525.151382	1035172.379801	41.035290
3525.388314	1034815.040501	41.040295
3525.498604	1034454.411061	41.045300
3525.816344	1034081.538112	41.050304
3525.903024	1033696.201279	41.055309
3526.122160	1033309.268319	41.060314
3526.223850	1032911.977246	41.065319
3526.233561	1032506.933673	41.070324
3526.595335	1032101.996152	41.075328
3526.663076	1031695.336047	41.080333
3526.892644	1031282.136510	41.085338
3526.450346	1030866.597777	41.090343
3526.363039	1030452.614795	41.095348
3526.514379	1030032.077208	41.100352
3526.810939	1029618.065831	41.105357
3527.114084	1029177.402905	41.110362
3526.994678	1028749.940521	41.115367
3527.115017	1028315.241649	41.120372
3527.419949	1027873.507344	41.125376
3527.235383	1027436.563380	41.130381
3527.617571	1026982.061160	41.135386
3527.496653	1026540.872626	41.140391
3527.205622	1026090.669965	41.145396
3527.675763	1025637.593535	41.150400
3527.307737	1025188.977543	41.155405
3527.664896	1024709.302476	41.160410
3527.309068	1024270.976607	41.165415
3527.401793	1023805.218887	41.170420
3527.872934	1023351.278797	41.175424
3527.645506	1022891.021026	41.180429
3527.349494	1022426.472377	41.185434
3527.661492	1021968.472780	41.190439
3527.489409	1021503.148620	41.195444
3527.597699	1021032.117058	41.200448
3527.323286	1020576.038993	41.205453
3527.558786	1020098.606338	41.210458
3527.482420	1019638.638030	41.215463
3527.332891	1019167.589147	41.220468
3527.523318	1018685.873754	41.225472
3527.112353	1018225.844636	41.230477
3527.136045	1017742.426856	41.235482
3527.127914	1017270.613332	41.240487
3527.297581	1016806.297902	41.245492
3527.282391	1016332.757460	41.250496
3526.974152	1015864.853074	41.255501
3527.311405	1015394.086290	41.260506
3527.155671	1014926.563782	41.265511
3527.160571	1014456.258379	41.270516
3527.095162	1013974.471830	41.275520
3526.968675	1013509.058972	41.280525
3527.185117	1013028.795125	41.285530
3527.164010	1012560.956521	41.290535
3526.932276	1012087.967657	41.295540
3527.082310	1011609.923854	41.300544
3526.877621	1011139.763897	41.305549
3526.698868	1010665.287117	41.310554
3526.729803	1010196.077814	41.315559
3526.458330	1009729.696157	41.320564
3526.496712	1009259.339066	41.325568
3526.625914	1008788.344820	41.330573
3526.461015	1008326.881326	41.335578
3526.494110	1007857.671148	41.340583
3526.465013	1007393.776833	41.345588
3526.379200	1006916.442274	41.350592
3525.951122	1006448.065383	41.355597
3526.065010	1005983.934312	41.360602
3526.121930	1005514.914020	41.365607
3526.007524	1005051.813163	41.370612
3526.020559	1004589.139424	41.375616
3526.050072	1004124.383165	41.380621
3526.313995	1003646.714291	41.385626
3526.108009	1003190.963360	41.390631
3525.918911	1002729.240231	41.395636
3525.973605	1002249.542535	41.400640
3526.012718	1001784.300322	41.405645
3525.799561	1001323.730836	41.410650
3525.498519	1000853.798594	41.415655
3525.300827	1000402.491200	41.420660
3525.732309	999941.605625	41.425664
3525.441765	999475.060025	41.430669
3525.399776	999014.371538	41.435674
3525.179318	998551.144412	41.440679
3525.286531	998097.461665	41.445684
3525.284451	997632.858047	41.450688
3524.860700	997171.693091	41.455693
3524.977803	996717.411383	41.460698
3524.924158	996269.158163	41.465703
3524.721170	995812.811935	41.470708
3524.913941	995352.078899	41.475712
3524.350300	994911.982522	41.480717
3524.486203	994460.925501	41.485722
3524.470400	994018.429343	41.490727
3523.942003	993558.935678	41.495732
3524.265502	993119.138480	41.500736
3523.789746	992686.453762	41.505741
3523.961570	992242.424164	41.510746
3524.075265	991812.596255	41.515751
3524.008883	991371.558556	41.520756
3524.359853	990926.422024	41.525760
3523.575702	990489.332422	41.530765
3523.665395	990039.978403	41.535770
3523.750005	989609.111262	41.540775
3523.901826	989172.838479	41.545780
3523.841121	988729.742452	41.550784
3523.515981	988291.140659	41.555789
3523.248493	987858.346246	41.560794
3523.597214	987427.075211	41.565799
3523.639102	986994.261614	41.570804
3523.614239	986556.354321	41.575808
3523.621261	986129.625360	41.580813
3523.451067	985679.189208	41.585818
3523.334857	985247.634529	41.590823
3523.098059	984815.091370	41.595828
3523.426779	984383.397911	41.600832
3523.066976	983948.955392	41.605837
3522.870405	983518.551472	41.610842
3522.790567	983084.192073	41.615847
3522.488224	982663.695562	41.620852
3522.858060	982244.228595	41.625856
3522.858124	981826.744003	41.630861
3522.364198	981408.236389	41.635866
3522.680446	980983.999714	41.640871
3522.432340	980570.564517	41.645876
3522.518098	980145.815328	41.650880
3522.510856	979732.865635	41.655885
3522.196116	979300.112121	41.660890
3522.286709	978876.537271	41.665895
3522.180766	978474.549043	41.670900
3522.311926	978045.729266	41.675904
3522.244399	977632.930708	41.680909
3522.292693	977214.612390	41.685914
3521.973764	976797.691773	41.690919
3521.699963	976386.595802	41.695924
3522.055571	975980.838631	41.700928
3521.490996	975575.595159	41.705933
3521.532267	975164.652609	41.710938
3521.939757	974749.906244	41.715943
3521.309425	974347.225456	41.720948
3521.368814	973925.830196	41.725952
3521.013310	973529.693616	41.730957
3521.488451	973126.842609	41.735962
3521.249151	972724.276514	41.740967
3520.994269	972331.266881	41.745972
3521.212760	971921.137840	41.750976
3520.994523	971537.650593	41.755981
3520.971806	971139.338032	41.760986
3521.301150	970737.418831	41.765991
3520.824963	970341.766282	41.770996
3520.513978	969924.930462	41.776000
3520.661737	969545.162359	41.781005
3520.682248	969152.280657	41.786010
3520.434921	968763.525385	41.791015
3520.365129	968379.019697	41.796020
3520.415119	967984.291965	41.801024
3519.930136	967605.576098	41.806029
3520.273079	967216.716666	41.811034
3520.225717	966822.414416	41.816039
3519.942681	966447.895254	41.821044
3520.103138	966057.715016	41.826048
3520.092964	965687.799798	41.831053
3520.207215	965312.064346	41.836058
3520.198411	964920.464222	41.841063
3519.875302	964535.742926	41.846068
3519.930680	964152.793947	41.851072
3519.822363	963781.890992	41.856077
3519.720554	963408.318950	41.861082
3519.718051	963017.959232	41.866087
3519.477511	962638.875652	41.871092
3519.609092	962264.995038	41.876096
3519.430917	961895.353245	41.881101
3519.362206	961532.429021	41.886106
3519.487721	961144.860006	41.891111
3519.368449	960776.508225	41.896116
3519.588668	960401.022352	41.901120
3519.116660	960029.153581	41.906125
3519.124439	959662.767372	41.911130
3519.261434	959289.182617	41.916135
3518.964978	958929.463875	41.921140
3518.939537	958552.623955	41.926144
3518.780492	958195.189041	41.931149
3518.972325	957829.048025	41.936154
3518.878654	957462.440650	41.941159
3518.593022	957109.860849	41.946164
3518.519596	956733.498178	41.951168
3518.402200	956388.788069	41.956173
3518.315452	956027.382994	41.961178
3518.358371	955680.643079	41.966183
3518.063646	955334.330230	41.971188
3518.251243	954965.458465	41.976192
3518.351824	954626.785821	41.981197
3518.193938	954267.930453	41.986202
3518.176245	953917.269328	41.991207
3518.096368	953578.466864	41.996212
3518.190821	953218.033261	42.001216
3518.171121	952867.799296	42.006221
3517.990215	952516.046837	42.011226
3518.247151	952180.363324	42.016231
3517.561199	951840.509494	42.021236
3517.836274	951505.447939	42.026240
3517.406932	951170.289119	42.031245
3517.401236	950846.229823	42.036250
3517.290592	950504.374719	42.041255
3517.201129	950178.469314	42.046260
3517.207363	949845.160677	42.051264
3517.126911	949518.350656	42.056269
3517.012391	949200.998021	42.061274
3517.259845	948875.432490	42.066279
3517.012908	948561.315463	42.071284
3517.245904	948233.797648	42.076288
3516.833620	947918.232936	42.081293
3516.980679	947593.463910	42.086298
3516.636864	947266.649390	42.091303
3516.465307	946956.633348	42.096308
3516.489542	946639.195068	42.101312
3516.451651	946331.895541	42.106317
3516.406440	946020.653430	42.111322
3516.508945	945703.910517	42.116327
3516.390173	945392.355323	42.121332
3516.381159	945078.560740	42.126336
3516.041311	944760.779407	42.131341
3516.191298	944453.145386	42.136346
3516.268625	944145.792349	42.141351
3515.664854	943855.007900	42.146356
3515.755680	943536.026666	42.151360
3515.349130	943241.535260	42.156365
3515.693125	942936.365490	42.161370
3515.529662	942653.967173	42.166375
3515.647368	942361.255449	42.171380
3515.712602	942055.888157	42.176384
3515.827069	941762.855761	42.181389
3515.254783	941458.037431	42.186394
3515.514412	941165.330718	42.191399
3515.047408	940879.435879	42.196404
3515.324853	940582.284877	42.201408
3515.043625	940294.985504	42.206413
3515.038230	940013.951174	42.211418
3515.159981	939713.804802	42.216423
3514.580043	939430.724768	42.221428
3515.121661	939146.390024	42.226432
3514.776294	938873.595012	42.231437
3514.755110	938581.844018	42.236442
3515.011838	938297.126453	42.241447
3514.535844	938017.020942	42.246452
3514.707978	937730.080958	42.251456
3514.442453	937458.541455	42.256461
3514.731118	937180.662700	42.261466
3514.969202	936893.474195	42.266471
3514.913662	936616.197683	42.271476
3514.785262	936322.515990	42.276480
3514.395997	936052.842452	42.281485
3514.107028	935768.461038	42.286490
3514.230359	935495.988364	42.291495
3514.085285	935227.575321	42.296500
3514.445012	934952.157276	42.301504
3514.241837	934680.271801	42.306509
3514.222445	934409.013695	42.311514
3514.262503	934143.105645	42.316519
3513.957756	933869.563701	42.321524
3513.963804	933593.749020	42.326528
3513.532815	933336.323321	42.331533
3513.683785	933071.974565	42.336538
3513.798678	932809.346256	42.341543
3513.633656	932548.286848	42.346548
3513.276349	932290.990017	42.351552
3513.649409	932031.640345	42.356557
3513.422023	931769.976781	42.361562
3513.675073	931503.900722	42.366567
3513.302974	931255.292772	42.371572
3513.135681	930991.468532	42.376576
3513.185127	930740.750604	42.381581
3513.154838	930499.732720	42.386586
3513.199359	930241.117750	42.391591
3512.968792	929989.834277	42.396596
3513.039358	929740.121998	42.401600
3512.867632	929490.533947	42.406605
3512.990653	929234.546313	42.411610
3512.669517	929000.231806	42.416615
3512.385689	928753.509259	42.421620
3512.691297	928503.219887	42.426624
3512.767852	928265.349230	42.431629
3512.316918	928029.668438	42.436634
3512.405387	927783.223899	42.441639
3512.512211	927539.359128	42.446644
3512.392821	927297.730438	42.451648
3512.357768	927068.184165	42.456653
3512.730831	926832.026443	42.461658
3512.550203	926587.108515	42.466663
3512.110615	926358.751583	42.471668
3512.177337	926114.540070	42.476672
3512.214299	925883.393354	42.481677
3512.068011	925657.360919	42.486682
3512.178224	925420.126919	42.491687
3511.890728	925197.270249	42.496692
3512.319279	924947.947545	42.501696
3511.929301	924727.106885	42.506701
3511.925155	924494.849605	42.511706
3511.884385	924265.472493	42.516711
3511.669524	924048.901343	42.521716
3511.400065	923806.562939	42.526720
3511.487728	923594.346417	42.531725
3511.349446	923381.677968	42.536730
3511.586428	923151.053667	42.541735
3511.441052	922937.695721	42.546740
3511.621302	922712.639449	42.551744
3511.661288	922495.867605	42.556749
3511.532454	922272.478777	42.561754
3511.559210	922045.688789	42.566759
3511.422456	921827.765047	42.571764
3511.557511	921613.346635	42.576768
3511.441565	921395.594384	42.581773
3510.990827	921173.367360	42.586778
3511.125140	920955.171342	42.591783
3511.104807	920754.308406	42.596788
3510.907181	920524.701633	42.601792
3510.845831	920315.074366	42.606797
3510.671537	920106.323507	42.611802
3510.601376	919903.512914	42.616807
3510.474650	919708.305487	42.621812
3510.804748	919495.406707	42.626816
3510.970692	919286.471972	42.631821
3510.706476	919082.604112	42.636826
3511.086374	918874.965523	42.641831
3510.294341	918667.608305	42.646836
3510.540830	918464.402990	42.651840
3510.802100	918254.161648	42.656845
3510.519475	918064.791793	42.661850
3510.833448	917854.430056	42.666855
3510.495971	917651.771833	42.671860
3510.436597	917444.054675	42.676864
3510.388472	917247.398145	42.681869
3510.368709	917050.248498	42.686874
3510.306943	916852.039649	42.691879
3510.192088	916660.090194	42.696884
3510.012496	916454.473134	42.701888
3510.203144	916266.599459	42.706893
3510.162305	916079.816585	42.711898
3510.371575	915881.046354	42.716903
3510.095882	915683.793163	42.721908
3510.248119	915483.862366	42.726912
3510.582258	915298.820608	42.731917
3510.020256	915100.437930	42.736922
3509.929209	914898.888672	42.741927
3509.864933	914710.040391	42.746932
3509.859379	914530.903464	42.751936
3510.146518	914345.837208	42.756941
3509.870957	914145.446377	42.761946
3510.107368	913950.646893	42.766951
3509.793528	913757.279701	42.771956
3509.792232	913578.881537	42.776960
3509.678146	913392.307912	42.781965
3509.527810	913209.683668	42.786970
3509.624677	913015.548300	42.791975
3509.544336	912839.932952	42.796980
3509.571805	912657.164686	42.801985
3509.626745	912482.768117	42.806989
3509.247024	912292.828689	42.811994
3509.503255	912114.725916	42.816999
3508.982831	911943.875803	42.822004
3509.235062	911749.284665	42.827009
3509.253963	911582.767090	42.832013
3509.008869	911392.099816	42.837018
3508.872312	911227.813562	42.842023
3509.014839	911046.514736	42.847028
3509.107956	910876.686885	42.852033
3509.141688	910705.996172	42.857037
3508.647990	910536.158127	42.862042
3509.130404	910361.720308	42.867047
3508.965846	910195.094635	42.872052
3508.765338	910026.734811	42.877057
3508.958255	909860.907676	42.882061
3508.912391	909685.667987	42.887066
3509.075231	909514.437164	42.892071
3508.774087	909352.821381	42.897076
3508.581057	909172.480302	42.902081
3508.954224	909014.889008	42.907085
3508.400186	908844.333990	42.912090
3508.833599	908680.745719	42.917095
3508.886123	908518.179545	42.922100
3508.728456	908345.036977	42.927105
3508.962719	908177.995530	42.932109
3508.567720	908014.813346	42.937114
3508.650715	907854.440477	42.942119
3508.259779	907687.390816	42.947124
3508.420116	907524.199126	42.952129
3508.787882	907361.064902	42.957133
3508.338159	907201.725303	42.962138
3508.398314	907043.936659	42.967143
3507.995977	906887.955753	42.972148
3508.515624	906723.427534	42.977153
3508.445589	906566.514817	42.982157
3508.162634	906411.658285	42.987162
3508.291347	906245.733526	42.992167
3508.223618	906093.822849	42.997172
3508.000378	905939.329162	43.002177
3508.072189	905782.178018	43.007181
3507.938770	905632.098394	43.012186
3507.989787	905472.144363	43.017191
3508.228042	905338.588484	43.022196
3507.660008	905182.394084	43.027201
3507.660644	905036.038853	43.032205
3507.318509	904890.797537	43.037210
3507.617668	904743.710088	43.042215
3507.178903	904607.643196	43.047220
3507.104916	904454.434528	43.052225
3507.523075	904321.789542	43.057229
3507.194733	904190.615289	43.062234
3507.249807	904046.733944	43.067239
3507.272760	903912.310938	43.072244
3507.225735	903772.492240	43.077249
3507.287976	903640.951228	43.082253
3506.941498	903502.622645	43.087258
3507.093868	903368.165231	43.092263
3507.086830	903241.934117	43.097268
3507.254998	903108.046905	43.102273
3507.386005	902961.519318	43.107277
3507.272578	902835.393076	43.112282
3507.090745	902682.539670	43.117287
3507.076281	902561.023834	43.122292
3507.195098	902421.530135	43.127297
3506.917288	902297.445844	43.132301
3506.973782	902152.067663	43.137306
3507.107732	902019.704520	43.142311
3506.781156	901905.465640	43.147316
3506.837692	901765.579754	43.152321
3507.273045	901631.709786	43.157325
3506.546660	901516.466945	43.162330
3507.112037	901377.066778	43.167335
3506.912418	901254.105012	43.172340
3507.039201	901117.570418	43.177345
3506.844218	900989.871369	43.182349
3506.820937	900864.072127	43.187354
3506.771081	900733.446843	43.192359
3506.650964	900607.657816	43.197364
3506.501943	900487.760678	43.202369
3506.850600	900369.903276	43.207373
3506.820129	900238.008032	43.212378
3506.825393	900107.841941	43.217383
3506.588892	899987.176045	43.222388
3506.538177	899859.813824	43.227393
3506.820317	899736.546364	43.232397
3506.359473	899617.937468	43.237402
3506.916163	899497.902980	43.242407
3506.753835	899374.314531	43.247412
3506.849920	899238.222278	43.252417
3506.771726	899113.938215	43.257421
3506.792847	898993.401750	43.262426
3506.398648	898862.693216	43.267431
3506.346192	898745.157678	43.272436
3506.436481	898626.340527	43.277441
3506.715131	898508.359156	43.282445
3506.436254	898392.109245	43.287450
3506.400747	898253.793310	43.292455
3506.423798	898144.056980	43.297460
3506.489912	898022.333213	43.302465
3506.808990	897904.525774	43.307469
3506.239116	897797.875026	43.312474
3506.526907	897662.775847	43.317479
3506.323854	897551.229771	43.322484
3506.380582	897434.904876	43.327489
3506.688368	897319.502333	43.332493
3506.392447	897198.689983	43.337498
3506.320147	897073.973620	43.342503
3506.248197	896965.389454	43.347508
3506.037165	896846.004840	43.352513
3506.229074	896734.957318	43.357517
3506.537868	896620.313333	43.362522
3506.287657	896506.049001	43.367527
3506.210018	896383.540682	43.372532
3506.197541	896275.030116	43.377537
3506.199098	896158.977997	43.382541
3505.639130	896050.070174	43.387546
3505.953909	895938.117118	43.392551
3506.144156	895830.241085	43.397556
3506.102919	895719.888557	43.402561
3505.907473	895613.811438	43.407565
3505.860334	895501.619486	43.412570
3505.834575	895392.321100	43.417575
3505.796636	895283.505843	43.422580
3505.990633	895172.234113	43.427585
3506.027239	895061.566031	43.432589
3505.776018	894965.827439	43.437594
3505.571557	894860.994206	43.442599
3505.801902	894747.581824	43.447604
3505.844766	894650.629621	43.452609
3505.949707	894540.326764	43.457613
3505.566623	894439.188184	43.462618
3505.704656	894331.678960	43.467623
3505.836962	894232.191696	43.472628
3505.741837	894122.783679	43.477633
3505.910787	894016.133391	43.482637
3505.318120	893926.716904	43.487642
3505.520165	893818.607442	43.492647
3505.758308	893719.190455	43.497652
3505.841073	893611.773426	43.502657
3505.595200	893509.242290	43.507661
3505.398004	893404.187683	43.512666
3505.508405	893299.660537	43.517671
3505.385052	893212.765854	43.522676
3505.252980	893110.982251	43.527681
3505.722877	893014.608635	43.532685
3505.441771	892914.489706	43.537690
3505.777397	892801.988127	43.542695
3505.521333	892709.016330	43.547700
3505.044466	892608.827602	43.552705
3505.415047	892502.502567	43.557709
3505.254294	892414.441584	43.562714
3505.370117	892321.305513	43.567719
3505.163886	892226.673830	43.572724
3505.358294	892132.748163	43.577729
3505.596491	892037.169835	43.582733
3505.316586	891934.906130	43.587738
3504.992160	891834.098487	43.592743
3504.926657	891751.040186	43.597748
3505.023592	891652.867673	43.602753
3505.264846	891570.626576	43.607757
3505.038321	891477.339752	43.612762
3505.343142	891381.449371	43.617767
3505.327109	891294.991403	43.622772
3505.233381	891197.519487	43.627777
3505.284555	891103.987401	43.632781
3505.026419	891010.891618	43.637786
3505.211305	890909.500192	43.642791
3505.051129	890821.221155	43.647796
3504.989786	890731.860529	43.652801
3505.016499	890639.775733	43.657805
3504.960789	890550.701528	43.662810
3504.866602	890458.827197	43.667815
3505.035559	890387.124265	43.672820
3504.889077	890293.127876	43.677825
3505.107493	890202.358694	43.682829
3504.846873	890117.277501	43.687834
3505.122594	890023.981008	43.692839
3504.935816	889943.334847	43.697844
3504.656739	889858.446329	43.702849
3505.067639	889764.542930	43.707853
3504.830074	889676.549246	43.712858
3504.890811	889584.538659	43.717863
3505.197104	889504.385551	43.722868
3505.041065	889416.374452	43.727873
3505.239537	889325.110978	43.732877
3505.035988	889237.201709	43.737882
3504.813061	889142.715350	43.742887
3504.862133	889053.020160	43.747892
3504.914559	888976.868304	43.752897
3505.229482	888888.868292	43.757901
3504.710950	888797.908092	43.762906
3504.772262	888704.044983	43.767911
3504.742792	888624.225206	43.772916
3504.595227	888552.454786	43.777921
3504.983342	888458.437075	43.782925
3504.852680	888383.275139	43.787930
3504.563954	888295.365513	43.792935
3504.350410	888209.861278	43.797940
3504.669192	888131.041705	43.802945
3504.716227	888059.136311	43.807949
3504.399845	887974.903508	43.812954
3504.380045	887887.620735	43.817959
3504.422584	887809.132586	43.822964
3504.335156	887732.503465	43.827969
3504.275772	887646.384837	43.832973
3503.968793	887581.886656	43.837978
3504.276182	887506.931448	43.842983
3504.285745	887435.605115	43.847988
3504.064889	887366.735337	43.852993
3504.349763	887296.813615	43.857997
3504.558491	887222.354870	43.863002
3504.223731	887139.177482	43.868007
3504.102525	887079.095079	43.873012
3503.770276	887001.915889	43.878017
3504.313431	886921.300705	43.883021
3503.939962	886861.160809	43.888026
3504.241661	886786.003613	43.893031
3504.332575	886711.654488	43.898036
3504.075142	886639.394412	43.903041
3503.960098	886572.917510	43.908045
3504.120300	886507.943191	43.913050
3504.121659	886426.829620	43.918055
3503.956375	886371.780446	43.923060
3504.313552	886305.029074	43.928065
3504.406003	886215.282615	43.933069
3504.145133	886154.439223	43.938074
3504.414360	886082.085413	43.943079
3504.728462	886006.432049	43.948084
3504.301107	885928.286173	43.953089
3504.334421	885840.576511	43.958093
3503.866611	885780.924938	43.963098
3504.228114	885699.451422	43.968103
3504.305642	885635.255385	43.973108
3503.814127	885569.700252	43.978113
3504.183115	885488.319345	43.983117
3504.051243	885419.895763	43.988122
3504.142527	885362.955302	43.993127
3503.974057	885289.211517	43.998132
3504.255255	885221.588862	44.003137
3504.192605	885152.182566	44.008141
3503.844000	885087.372955	44.013146
3504.141383	885015.485278	44.018151
3504.082977	884932.133800	44.023156
3503.851903	884874.176634	44.028161
3504.146070	884793.766519	44.033165
3503.995751	884731.728100	44.038170
3504.026831	884664.721103	44.043175
3503.972667	884606.635293	44.048180
3503.845850	884538.394125	44.053185
3504.314617	884470.828649	44.058189
3503.865168	884402.639040	44.063194
3503.784919	884342.908804	44.068199
3503.885902	884268.333009	44.073204
3503.652619	884214.049179	44.078209
3504.109761	884132.731580	44.083213
3503.580884	884085.564053	44.088218
3503.728915	884012.236060	44.093223
3504.277090	883946.878619	44.098228
3503.889428	883883.417697	44.103233
3503.781244	883811.775619	44.108237
3503.680337	883746.426027	44.113242
3503.935048	883695.736853	44.118247
3503.989612	883622.225661	44.123252
3503.562518	883565.256136	44.128257
3503.729866	883498.600611	44.133261
3503.622673	883439.833967	44.138266
3503.696758	883379.874717	44.143271
3503.529437	883315.499679	44.148276
3503.187076	883263.452410	44.153281
3503.784136	883202.436696	44.158285
3503.323962	883145.274807	44.163290
3503.476860	883086.461744	44.168295
3503.593607	883032.109205	44.173300
3503.509320	882967.716640	44.178305
3503.656733	882907.740447	44.183309
3503.224090	882862.774761	44.188314
3503.521343	882794.346397	44.193319
3503.578835	882732.736678	44.198324
3503.558755	882687.701668	44.203329
3503.700036	882626.561307	44.208333
3503.818557	882575.400533	44.213338
3503.749598	882498.892883	44.218343
3503.824896	882436.114773	44.223348
3503.725658	882378.692166	44.228353
3504.018321	882315.586361	44.233357
3503.855495	882256.816944	44.238362
3503.630389	882184.592919	44.243367
3503.627290	882129.186188	44.248372
3503.646490	882076.584407	44.253377
3504.023937	882005.905639	44.258381
3503.504785	881945.641897	44.263386
3503.499677	881884.130396	44.268391
3503.626846	881829.668063	44.273396
3503.489472	881773.505107	44.278401
3503.366000	881708.039488	44.283405
3503.284535	881661.262945	44.288410
3503.416678	881597.303956	44.293415
3503.465979	881543.529910	44.298420
3503.532962	881494.983809	44.303425
3503.390928	881432.811974	44.308429
3503.355785	881382.828598	44.313434
3503.521588	881320.798611	44.318439
3503.818958	881265.915463	44.323444
3503.453284	881206.393841	44.328449
3503.536423	881149.704146	44.333453
3503.422861	881098.956201	44.338458
3503.472504	881038.783145	44.343463
3503.408962	880986.088290	44.348468
3503.233699	880932.442504	44.353473
3503.494794	880874.364415	44.358477
3503.464047	880823.600434	44.363482
3503.628858	880772.222462	44.368487
3503.440642	880716.639053	44.373492
3503.249939	880668.419212	44.378497
3503.637326	880607.507842	44.383501
3503.517652	880552.299145	44.388506
3503.230606	880488.978451	44.393511
3503.164111	880450.231905	44.398516
3503.202972	880395.286290	44.403521
3503.413837	880336.532876	44.408525
3503.067123	880293.374239	44.413530
3503.162361	880235.995420	44.418535
3503.201969	880176.977928	44.423540
3502.902479	880132.841339	44.428545
3503.378757	880076.754775	44.433549
3503.541509	880040.584058	44.438554
3503.308622	879977.539610	44.443559
3503.259294	879927.158524	44.448564
3503.065079	879881.646056	44.453569
3503.074399	879826.699974	44.458573
3502.894757	879788.839833	44.463578
3503.035223	879731.545529	44.468583
3503.371538	879678.094677	44.473588
3503.204306	879632.866552	44.478593
3503.650214	879584.242172	44.483597
3503.332470	879535.743205	44.488602
3503.262356	879482.551352	44.493607
3503.013740	879429.291514	44.498612
3503.072499	879381.116881	44.503617
3503.002703	879318.619943	44.508621
3502.891964	879280.260599	44.513626
3503.051725	879230.323644	44.518631
3503.246010	879188.521444	44.523636
3502.862679	879127.334020	44.528641
3502.966759	879080.409359	44.533645
3503.018221	879051.131967	44.538650
3502.914098	879000.461195	44.543655
3502.934982	878954.130741	44.548660
3502.789754	878906.276574	44.553665
3503.148428	878854.559097	44.558669
3503.212838	878814.810967	44.563674
3502.886646	878780.748385	44.568679
3502.917065	878728.793118	44.573684
3503.180688	878690.077470	44.578689
3503.297600	878640.045634	44.583693
3502.763058	878596.905440	44.588698
3502.823044	878539.031208	44.593703
3503.207960	878495.254154	44.598708
3503.001502	878458.165251	44.603713
3503.056524	878405.524582	44.608717
3503.082649	878361.708719	44.613722
3503.338421	878313.977517	44.618727
3503.024793	878254.998890	44.623732
3502.924070	878211.590528	44.628737
3503.112767	878162.899840	44.633741
3502.901050	878122.998660	44.638746
3502.978488	878077.233570	44.643751
3502.999478	878024.207361	44.648756
3502.840049	877991.663672	44.653761
3503.110080	877935.396784	44.658765
3503.233156	877893.015492	44.663770
3502.879594	877843.248261	44.668775
3503.201318	877798.507066	44.673780
3502.992399	877757.633565	44.678785
3503.226694	877703.890757	44.683789
3502.943937	877657.600111	44.688794
3503.085241	877624.520141	44.693799
3503.294573	877566.127028	44.698804
3502.589561	877526.109185	44.703809
3503.038318	877470.874781	44.708813
3502.869829	877425.920692	44.713818
3502.731597	877380.864329	44.718823
3503.071352	877342.127276	44.723828
3503.210804	877300.417639	44.728833
3503.208109	877246.031077	44.733837
3503.104318	877209.886854	44.738842
3502.984832	877165.504388	44.743847
3502.652578	877115.145795	44.748852
3502.740967	877082.847097	44.753857
3503.056494	877039.652360	44.758861
3503.166313	876991.546687	44.763866
3502.729174	876945.566728	44.768871
3503.068173	876897.519482	44.773876
3502.739597	876860.537574	44.778881
3503.293704	876819.822709	44.783885
3503.058271	876779.916326	44.788890
3502.998181	876735.714747	44.793895
3502.968251	876684.042238	44.798900
3502.777255	876642.479347	44.803905
3502.865285	876587.199145	44.808909
3503.046127	876548.773940	44.813914
3502.883537	876504.684475	44.818919
3503.112499	876455.100410	44.823924
3502.674955	876418.230638	44.828929
3502.731093	876378.273498	44.833933
3502.824682	876340.055233	44.838938
3502.735556	876300.315423	44.843943
3502.938238	876245.788835	44.848948
3502.759625	876210.620446	44.853953
3502.737370	876170.189993	44.858957
3502.940411	876123.613322	44.863962
3502.976781	876084.530141	44.868967
3502.976441	876038.665071	44.873972
3502.618094	876008.567366	44.878977
3503.158095	875955.243098	44.883981
3503.038769	875917.154144	44.888986
3502.886348	875874.318888	44.893991
3502.952663	875836.586708	44.898996
3503.019465	875797.787526	44.904001
3502.761339	875743.914053	44.909005
3502.653133	875704.658234	44.914010
3502.526819	875666.374869	44.919015
3502.725317	875620.473792	44.924020
3502.628223	875594.112904	44.929025
3502.553677	875547.965328	44.934029
3502.298067	875523.278814	44.939034
3501.935374	875475.917467	44.944039
3502.922091	875447.534817	44.949044
3502.450702	875417.840627	44.954049
3502.475666	875375.457414	44.959053
3502.256390	875344.072694	44.964058
3502.747315	875300.739371	44.969063
3502.766895	875265.532699	44.974068
3502.648738	875227.633066	44.979073
3502.434550	875183.639216	44.984077
3502.568978	875149.867647	44.989082
3502.410498	875121.769099	44.994087
3502.842024	875071.073252	44.999092
3502.501921	875043.392186	45.004097
3502.320623	875008.701997	45.009101
3502.581802	874967.149795	45.014106
3502.844471	874941.308631	45.019111
3502.618886	874904.782416	45.024116
3502.233996	874880.599442	45.029121
3502.633292	874837.568788	45.034125
3502.723407	874810.494656	45.039130
3502.485516	874765.822693	45.044135
3502.648728	874709.348689	45.049140
3502.605592	874695.001489	45.054145
3502.578066	874646.220428	45.059149
3502.370739	874617.642584	45.064154
3502.607012	874579.195451	45.069159
3502.685273	874553.092004	45.074164
3502.561947	874524.984829	45.079169
3502.630494	874469.494052	45.084173
3502.692423	874442.325890	45.089178
3502.553810	874402.096504	45.094183
3502.440681	874357.885875	45.099188
3502.352868	874322.691290	45.104193
3502.614990	874289.184762	45.109197
3502.739049	874271.123156	45.114202
3502.694466	874222.050425	45.119207
3502.570241	874185.503070	45.124212
3502.527950	874149.620976	45.129217
3502.506924	874104.714299	45.134221
3502.600090	874078.897304	45.139226
3502.683512	874041.053860	45.144231
3502.456398	874004.231340	45.149236
3502.289058	873969.629761	45.154241
3502.092742	873939.397814	45.159245
3502.677248	873915.342182	45.164250
3502.317825	873896.680080	45.169255
3502.598236	873847.550705	45.174260
3502.363440	873816.160435	45.179265
3502.386945	873776.967132	45.184269
3502.401314	873748.348566	45.189274
3502.255921	873715.778982	45.194279
3502.525866	873674.992323	45.199284
3502.012889	873651.795481	45.204289
3502.274386	873614.987047	45.209293
3502.406041	873585.087284	45.214298
3502.419215	873561.221359	45.219303
3502.408451	873524.942260	45.224308
3502.310176	873498.087192	45.229313
3502.378272	873454.713046	45.234317
3502.669698	873429.733647	45.239322
3502.332539	873393.022469	45.244327
3502.554509	873350.107259	45.249332
3502.364067	873330.251398	45.254337
3502.528171	873292.680924	45.259341
3502.752070	873263.831478	45.264346
3502.403462	873224.210771	45.269351
3502.246611	873190.379020	45.274356
3502.188823	873158.374024	45.279361
3502.638998	873131.038878	45.284365
3502.577185	873087.489425	45.289370
3502.193797	873067.567458	45.294375
3502.331349	873032.328086	45.299380
3502.390046	872995.355195	45.304385
3502.593328	872963.112100	45.309389
3502.861771	872935.708983	45.314394
3502.083166	872901.686971	45.319399
3502.340844	872851.388886	45.324404
3502.126406	872845.020990	45.329409
3502.424201	872801.895292	45.334413
3502.447277	872775.113980	45.339418
3502.195616	872749.348018	45.344423
3502.401121	872710.796838	45.349428
3502.273515	872686.562507	45.354433
3502.340902	872655.698441	45.359437
3502.296904	872621.747836	45.364442
3502.373380	872585.933743	45.369447
3502.628188	872554.359109	45.374452
3501.918745	872532.839656	45.379457
3502.236089	872497.664518	45.384461
3502.344974	872464.367001	45.389466
3501.933533	872447.746434	45.394471
3502.537252	872400.783426	45.399476
3502.568569	872380.790826	45.404481
3502.424324	872348.116523	45.409485
3502.254261	872327.768814	45.414490
3502.355663	872294.374550	45.419495
3502.137355	872260.547629	45.424500
3502.213461	872227.254186	45.429505
3502.132592	872206.697308	45.434509
3502.301016	872166.499210	45.439514
3502.159565	872161.282916	45.444519
3502.373699	872116.516522	45.449524
3501.950674	872092.619534	45.454529
3502.067473	872065.625523	45.459533
3502.213852	872021.257703	45.464538
3502.131790	872002.835035	45.469543
3502.492853	871971.336838	45.474548
3502.192601	871960.712656	45.479553
3502.149831	871909.873915	45.484557
3501.851230	871891.195474	45.489562
3501.736943	871881.413824	45.494567
3501.831667	871839.187926	45.499572
3502.254043	871814.762394	45.504577
3502.506855	871794.052079	45.509581
3502.181120	871771.399241	45.514586
3502.268027	871747.222776	45.519591
3502.725613	871702.122049	45.524596
3502.358605	871676.661552	45.529601
3502.008154	871656.826458	45.534605
3501.923959	871619.092250	45.539610
3501.942567	871591.238915	45.544615
3502.228323	871572.560236	45.549620
3502.220685	871544.613968	45.554625
3502.386235	871515.959749	45.559629
3502.349497	871480.157659	45.564634
3501.972438	871447.710851	45.569639
3502.220824	871422.924215	45.574644
3501.865809	871400.857043	45.579649
3502.123899	871385.869961	45.584653
3502.276791	871350.909238	45.589658
3502.169290	871333.459125	45.594663
3502.068959	871297.957549	45.599668
3502.271979	871277.544780	45.604673
3502.169385	871248.739366	45.609677
3502.096679	871209.933177	45.614682
3502.279296	871192.337807	45.619687
3502.359076	871156.417529	45.624692
3501.965505	871141.149011	45.629697
3502.170846	871103.169740	45.634701
3502.258593	871075.108508	45.639706
3502.032913	871044.284376	45.644711
3502.265350	871014.258049	45.649716
3501.685503	870999.602151	45.654721
3502.401984	870964.740411	45.659725
3502.269276	870947.584471	45.664730
3502.188925	870920.035455	45.669735
3502.280481	870897.310537	45.674740
3501.951598	870877.469289	45.679745
3502.315253	870839.753413	45.684749
3502.394662	870825.958989	45.689754
3501.946656	870793.520304	45.694759
3502.125813	870781.165131	45.699764
3502.042376	870746.530964	45.704769
3502.221379	870717.094267	45.709773
3501.945480	870690.158730	45.714778
3501.794904	870664.464135	45.719783
3502.421891	870643.008801	45.724788
3502.431902	870609.231936	45.729793
3502.259164	870591.305120	45.734797
3502.236495	870556.077500	45.739802
3502.190600	870534.150298	45.744807
3502.274226	870502.204779	45.749812
3502.220681	870484.355061	45.754817
3501.912059	870429.568134	45.759821
3502.460223	870347.851087	45.764826
3502.040615	870201.163969	45.769831
3502.135428	869991.199098	45.774836
3502.060253	869748.348362	45.779841
3501.922127	869429.683235	45.784845
3502.317115	869048.490593	45.789850
3501.940066	868605.361913	45.794855
3501.887643	868093.791513	45.799860
3501.302874	867543.617426	45.804865
3501.349876	866928.124880	45.809869
3501.331817	866244.592074	45.814874
3501.082249	865503.125746	45.819879
3501.126560	864683.604935	45.824884
3500.722736	863809.634407	45.829889
3500.165520	862869.480552	45.834893
3500.032389	861848.049406	45.839898
3499.940845	860774.722084	45.844903
3500.058848	859617.162802	45.849908
3499.521364	858401.141219	45.854913
3499.456391	857099.395491	45.859917
3499.328034	855730.348743	45.864922
3498.834930	854276.586820	45.869927
3498.434472	852743.231891	45.874932
3497.763155	851159.008976	45.879937
3497.696342	849486.045554	45.884941
3497.085438	847733.228799	45.889946
3496.419692	845905.090196	45.894951
3495.743188	844003.118358	45.899956
3495.342746	842036.025961	45.904961
3494.934966	839980.440930	45.909965
3494.696643	837856.936442	45.914970
3493.885842	835662.349230	45.919975
3493.282886	833377.294948	45.924980
3492.809509	831025.624804	45.929985
3492.197187	828597.055080	45.934989
3491.567357	826084.641947	45.939994
3490.949436	823509.802646	45.944999
3490.297696	820844.156086	45.950004
3489.542192	818113.985693	45.955009
3488.817841	815309.552541	45.960013
3488.456652	812421.018737	45.965018
3487.409016	809472.857504	45.970023
3486.893078	806429.554232	45.975028
3485.524601	803329.765291	45.980033
3484.727819	800152.288111	45.985037
3484.206894	796900.167394	45.990042
3483.172372	793577.123155	45.995047
3482.548026	790168.616332	46.000052
3481.537622	786708.586154	46.005057
3480.733595	783175.331674	46.010061
3480.080815	779557.007728	46.015066
3478.901998	775872.321442	46.020071
3478.196279	772101.517867	46.025076
3476.884332	768272.898364	46.030081
3476.152572	764373.868707	46.035085
3474.881740	760391.399362	46.040090
3473.564790	756350.914923	46.045095
3472.649097	752233.206939	46.050100
3471.659941	748049.270851	46.055105
3470.642723	743792.043982	46.060109
3469.683659	739452.364266	46.065114
3468.367430	735063.945511	46.070119
3467.045458	730572.696680	46.075124
3465.902517	726032.998439	46.080129
3464.205499	721415.173281	46.085133
3463.207396	716733.348977	46.090138
3461.820185	711979.439312	46.095143
3460.771324	707157.357276	46.100148
3459.159981	702277.803644	46.105153
3457.588745	697322.967163	46.110157
3456.439753	692290.355682	46.115162
3454.843760	687197.090886	46.120167
3453.702384	682023.338298	46.125172
3451.867165	676799.338751	46.130177
3450.071941	671494.713631	46.135181
3448.756962	666121.669228	46.140186
3446.976193	660690.773051	46.145191
3445.800340	655190.859850	46.150196
3444.158186	649623.787144	46.155201
3442.320258	644001.396912	46.160205
3440.581646	638294.033144	46.165210
3438.399523	632552.001561	46.170215
3436.872482	626728.190769	46.175220
3435.023948	620851.946979	46.180225
3433.254492	614917.811001	46.185229
3431.617993	608914.953562	46.190234
3429.333438	602864.081326	46.195239
3427.899867	596735.354461	46.200244
3425.592454	590553.265227	46.205249
3423.720186	584310.893364	46.210253
3421.817166	578010.652837	46.215258
3419.527065	571656.406260	46.220263
3417.511012	565239.272424	46.225268
3415.379708	558762.818877	46.230273
3413.315734	552231.637420	46.235277
3411.393121	545637.290973	46.240282
3408.625078	539008.932829	46.245287
3406.417682	532309.469921	46.250292
3403.981902	525571.477986	46.255297
3401.921209	518760.335793	46.260301
3399.480937	511915.367309	46.265306
3396.752948	505012.583138	46.270311
3394.421754	498062.452583	46.275316
3392.347244	491067.505983	46.280321
3389.517966	484022.578342	46.285325
3387.097620	476927.204341	46.290330
3384.313704	469791.219938	46.295335
3381.722869	462598.870953	46.300340
3379.007801	455366.261853	46.305345
3375.745070	448094.935665	46.310349
3373.202685	440781.544955	46.315354
3370.264770	433436.987179	46.320359
3367.544208	426041.332976	46.325364
3364.471424	418632.101806	46.330369
3361.598893	411169.320441	46.335373
3358.535395	403669.064272	46.340378
3355.224395	396143.689933	46.345383
3351.957828	388585.738503	46.350388
3348.807176	380995.764532	46.355393
3345.638591	373368.282287	46.360397
3342.519081	365718.777856	46.365402
3338.901264	358038.891675	46.370407
3335.957440	350344.705763	46.375412
3332.690202	342619.313177	46.380417
3328.741333	334865.594145	46.385421
3325.266150	327103.822782	46.390426
3321.794834	319326.983959	46.395431
3318.108685	311520.100726	46.400436
3314.599827	303705.341676	46.405441
3311.258299	295875.285883	46.410445
3307.455611	288022.282028	46.415450
3303.248112	280155.679321	46.420455
3299.688015	272286.219626	46.425460
3295.682327	264399.506868	46.430465
3291.624609	256523.228137	46.435469
3287.741296	248625.019428	46.440474
3283.808932	240736.465396	46.445479
3279.805005	232826.390945	46.450484
3275.675140	224882.272727	46.455489
3271.416312	216938.360080	46.460493
3267.242694	209042.517399	46.465498
3263.224755	201153.560664	46.470503
3258.883818	193264.966867	46.475508
3254.442646	185393.019650	46.480513
3249.885899	177530.543892	46.485517
3245.739526	169662.772633	46.490522
3240.596638	161817.585661	46.495527
3235.947907	153989.757445	46.500532
3231.066162	146181.283639	46.505537
3226.281517	138410.355314	46.510541
3221.606244	130645.823760	46.515546
3216.245610	122929.822101	46.520551
3211.160756	115227.999393	46.525556
3206.177968	107574.405354	46.530561
3200.673323	99947.297025	46.535565
3195.039246	92365.208142	46.540570
3189.352774	84829.381026	46.545575
3183.629809	77341.919241	46.550580
3177.585060	69906.801905	46.555585
3170.702045	62546.598884	46.560589
3164.254655	55244.335806	46.565594
3156.322008	48053.740137	46.570599
3144.501476	41059.824829	46.575604
3123.204172	34447.808587	46.580609
3102.186979	28074.264794	46.585613
3081.918592	21999.944338	46.590618
3061.178395	16316.277367	46.595623
3035.937823	11115.586383	46.600628
3004.614412	6568.172590	46.605633
2969.873155	2647.949556	46.610637
2898.842124	370.212334	46.615642
2782.779903	316.949705	46.620647
2723.493560	298.281036	46.625652
2720.072695	291.970502	46.630657
2750.848473	284.469837	46.635661
2793.080684	281.244901	46.640666
2828.546397	291.637185	46.645671
2851.220670	284.469675	46.650676
2860.103577	278.316913	46.655681
2858.915828	279.083226	46.660685
2852.958018	263.681980	46.665690
2845.815372	283.330938	46.670695
2839.675633	281.860167	46.675700
2835.530459	272.633920	46.680705
2832.533835	265.761148	46.685709
2831.037783	254.390835	46.690714
2828.939576	263.892962	46.695719
2826.567313	264.347144	46.700724
2824.263005	264.959040	46.705729
2821.056765	266.894725	46.710733
2818.926947	254.497022	46.715738
2815.689888	256.355699	46.720743
2812.578365	260.918180	46.725748
2809.275444	255.278836	46.730753
2805.919410	265.278198	46.735757
2802.961362	260.386720	46.740762
2800.024987	269.146605	46.745767
2796.760110	254.882245	46.750772
2793.393994	246.892336	46.755777
2790.021230	251.824729	46.760781
2786.869718	246.846781	46.765786
2783.793678	259.051238	46.770791
2780.762181	245.710636	46.775796
2777.794606	243.833383	46.780801
2774.051306	246.672336	46.785805
2770.983614	249.622027	46.790810
2767.410935	259.627945	46.795815
2764.367396	252.594040	46.800820
2760.425526	249.193828	46.805825
2756.816093	251.252911	46.810829
2754.102120	251.717724	46.815834
2750.980613	256.207685	46.820839
2747.665496	241.775242	46.825844
2744.166863	238.412028	46.830849
2740.580788	250.489104	46.835853
2737.244219	242.873261	46.840858
2733.962319	236.233932	46.845863
2730.447740	243.458011	46.850868
2727.057205	240.164592	46.855873
2723.550174	246.853029	46.860877
2720.131427	236.522307	46.865882
2717.174321	236.755321	46.870887
2713.524524	234.693088	46.875892
2710.676276	233.670808	46.880897
2706.852196	239.386573	46.885901
2703.571614	233.974123	46.890906
2699.792073	235.848579	46.895911
2695.884402	236.180440	46.900916
2693.038735	225.643091	46.905921
2689.627588	242.745257	46.910925
2686.078938	230.968959	46.915930
2682.445429	229.946423	46.920935
2678.797310	232.672643	46.925940
2675.666567	228.851327	46.930945
2672.669484	226.551172	46.935949
2669.445644	223.884676	46.940954
2665.210354	215.845703	46.945959
2661.491194	227.209473	46.950964
2658.625691	216.854219	46.955969
2654.945621	227.407573	46.960973
2651.601201	218.955977	46.965978
2647.704419	218.637614	46.970983
2644.827998	221.327682	46.975988
2641.604277	220.977980	46.980993
2638.061978	223.072636	46.985997
2635.146108	220.727134	46.991002
2630.930380	227.096842	46.996007
2627.409770	228.492100	47.001012
2624.328824	217.550005	47.006017
2620.389467	225.182489	47.011021
2616.648794	214.848944	47.016026
2613.425222	222.455268	47.021031
2610.258089	216.783806	47.026036
2606.997917	224.719816	47.031041
2602.919960	231.794213	47.036045
2600.002780	217.334526	47.041050
2596.438071	222.859158	47.046055
2592.544912	220.949270	47.051060
2589.758450	213.273158	47.056065
2585.890601	216.834148	47.061069
2582.393885	212.066063	47.066074
2578.388616	217.530798	47.071079
2575.190711	218.679044	47.076084
2572.067089	213.215532	47.081089
2568.743257	217.362450	47.086093
2565.352283	216.257349	47.091098
2561.343875	221.430550	47.096103
2558.070483	213.544728	47.101108
2554.601923	205.794530	47.106113
2551.156124	215.443736	47.111117
2548.065073	200.617327	47.116122
2544.248445	199.822459	47.121127
2540.472013	215.633958	47.126132
2537.492268	210.795978	47.131137
2533.567268	210.906646	47.136141
2530.225206	206.013619	47.141146
2526.800014	213.390010	47.146151
2523.115085	212.878906	47.151156
2519.710563	208.093286	47.156161
2516.007871	215.581792	47.161165
2512.896183	209.153720	47.166170
2509.254737	205.560870	47.171175
2505.848350	214.268594	47.176180
2502.236855	209.253893	47.181185
2498.568077	207.359542	47.186189
2495.407977	198.962511	47.191194
2491.877706	202.516790	47.196199
2488.499693	216.104041	47.201204
2484.975829	208.768757	47.206209
2481.658763	209.835296	47.211213
2478.349724	203.283924	47.216218
2474.525304	205.647463	47.221223
2470.846040	203.686189	47.226228
2467.489160	202.102700	47.231233
2463.854883	212.707412	47.236237
2460.796985	194.531852	47.241242
2457.371278	203.294096	47.246247
2453.373902	208.413850	47.251252
2449.937817	196.246616	47.256257
2446.242335	204.841058	47.261261
2442.865259	195.559876	47.266266
2439.590071	202.332952	47.271271
2436.073195	199.887859	47.276276
2432.937126	200.807727	47.281281
2429.059232	203.214463	47.286285
2425.811110	189.103401	47.291290
2422.235622	203.286286	47.296295
2418.399060	202.847258	47.301300
2415.025162	200.440544	47.306305
2411.471854	201.005804	47.311309
2408.126323	195.651071	47.316314
2404.858771	197.030363	47.321319
2401.653598	190.308970	47.326324
2398.065768	193.515822	47.331329
2393.896804	208.110071	47.336333
2390.436717	197.516696	47.341338
2386.688063	192.966777	47.346343
2383.522444	191.562930	47.351348
2380.753450	189.946002	47.356353
2376.931969	196.277260	47.361357
2373.605601	183.870966	47.366362
2369.713656	189.983759	47.371367
2366.071507	193.585401	47.376372
2363.032927	191.785254	47.381377
2359.053936	197.986233	47.386381
2355.606850	196.273260	47.391386
2352.303501	191.579210	47.396391
2348.523981	205.317861	47.401396
2345.151639	190.226455	47.406401
2341.576768	190.891233	47.411405
2338.062687	191.436651	47.416410
2334.742636	195.840418	47.421415
2331.625891	193.351845	47.426420
2327.709576	187.352952	47.431425
2324.027025	199.084634	47.436429
2320.902358	190.735759	47.441434
2317.525749	194.438645	47.446439
2314.117839	196.929699	47.451444
2310.286555	186.087458	47.456449
2306.618217	193.393803	47.461453
2302.993892	198.388340	47.466458
2299.966519	194.347156	47.471463
2296.455118	192.821464	47.476468
2293.396841	188.821698	47.481473
2289.143306	183.637682	47.486477
2285.691664	189.315330	47.491482
2282.547902	186.507217	47.496487
2278.902817	197.682555	47.501492
2275.519224	195.306749	47.506497
2271.538204	192.092999	47.511501
2268.308731	199.742122	47.516506
2264.971320	181.416727	47.521511
2261.088576	190.023452	47.526516
2257.798381	184.105763	47.531521
2254.122157	192.858767	47.536525
2251.270577	189.230242	47.541530
2247.687955	189.136605	47.546535
2243.884564	188.664611	47.551540
2239.974027	181.949087	47.556545
2236.795098	187.550561	47.561549
2233.555506	186.032137	47.566554
2230.162570	178.585072	47.571559
2226.223841	183.507440	47.576564
2223.044567	176.636072	47.581569
2219.479080	176.195860	47.586573
2215.792351	179.189856	47.591578
2212.439426	178.554906	47.596583
2208.635791	177.756973	47.601588
2205.722779	179.475497	47.606593
2201.868852	184.343033	47.611597
2198.175206	179.857797	47.616602
2194.721815	173.738386	47.621607
2190.968591	177.432097	47.626612
2188.116651	178.397363	47.631617
2184.384259	184.217536	47.636621
2180.941463	186.857905	47.641626
2177.477065	178.606678	47.646631
2173.991915	183.212648	47.651636
2170.627713	172.896887	47.656641
2166.746993	184.677757	47.661645
2163.567024	174.974910	47.666650
2160.112634	177.002294	47.671655
2156.564324	181.593839	47.676660
2153.138410	172.494821	47.681665
2149.228208	177.576525	47.686669
2145.886009	178.917397	47.691674
2142.402380	166.665346	47.696679
2138.662848	171.587051	47.701684
2135.281130	164.114140	47.706689
2131.623250	174.839364	47.711693
2128.420309	164.667517	47.716698
2125.221248	171.098836	47.721703
2121.424391	179.060969	47.726708
2118.316417	173.520608	47.731713
2113.921165	178.345969	47.736717
2110.908221	178.311895	47.741722
2107.686395	174.776570	47.746727
2103.519232	175.590831	47.751732
2100.717693	168.840706	47.756737
2096.900451	182.613945	47.761741
2093.454180	171.826144	47.766746
2090.190551	170.240155	47.771751
2086.215406	176.280849	47.776756
2082.779390	166.507078	47.781761
2079.463224	179.039786	47.786765
2076.149062	175.328509	47.791770
2072.129140	172.709826	47.796775
2068.651102	173.163050	47.801780
2065.330972	166.297696	47.806785
2062.036942	169.932443	47.811789
2058.772512	168.819040	47.816794
2055.224088	178.570523	47.821799
2051.191578	175.463546	47.826804
2048.169130	168.737702	47.831809
2044.332289	174.799792	47.836813
2040.862718	176.508890	47.841818
2037.640867	169.316121	47.846823
2033.490183	167.870151	47.851828
2030.287011	177.143508	47.856833
2026.734361	182.484173	47.861837
2023.115529	170.654754	47.866842
2019.761504	177.548443	47.871847
2016.443154	170.323869	47.876852
2012.852207	171.422531	47.881857
2009.025338	179.844766	47.886861
2005.916020	176.729817	47.891866
2002.622374	175.098523	47.896871
1998.795635	181.805072	47.901876
1995.655840	165.473981	47.906881
1991.993637	166.463259	47.911885
1988.569851	170.018840	47.916890
1985.303782	165.714774	47.921895
1981.152243	170.854813	47.926900
1977.605758	165.191808	47.931905
1973.987181	169.905393	47.936909
1970.924611	167.064353	47.941914
1967.636976	162.357935	47.946919
1963.996326	169.909761	47.951924
1960.063655	168.205841	47.956929
1956.668784	167.724227	47.961933
1953.533427	171.951302	47.966938
1949.947158	162.457618	47.971943
1946.523793	165.300563	47.976948
1943.392179	171.710984	47.981953
1939.755545	162.205894	47.986957
1935.904788	167.934488	47.991962
1932.257592	161.693175	47.996967
1928.543374	166.033039	48.001972
1924.956306	159.941845	48.006977
1921.686426	165.418410	48.011981
1918.629298	164.167262	48.016986
1915.250409	163.826307	48.021991
1911.290703	169.221255	48.026996
1907.572788	166.394567	48.032001
1904.235554	158.470083	48.037005
1900.985619	162.228092	48.042010
1897.888085	163.802824	48.047015
1893.789954	165.761681	48.052020
1890.651411	148.318283	48.057025
1886.802793	167.428938	48.062029
1883.083062	167.185351	48.067034
1879.994044	174.207828	48.072039
1876.107592	170.477955	48.077044
1872.592666	161.747506	48.082049
1869.459205	154.767210	48.087053
1865.847002	161.089120	48.092058
1862.544792	164.551688	48.097063
1858.353176	168.919350	48.102068
1855.367347	159.497464	48.107073
1851.759768	164.167679	48.112077
1848.441600	154.677163	48.117082
1845.335836	155.486625	48.122087
1840.883631	166.285026	48.127092
1837.889511	163.084267	48.132097
1834.469837	162.993229	48.137101
1831.126211	165.479119	48.142106
1827.760358	158.839170	48.147111
1823.759246	171.107846	48.152116
1820.373021	159.474236	48.157121
1816.653574	165.673983	48.162125
1813.234460	163.727680	48.167130
1809.733638	160.621694	48.172135
1806.206728	152.959510	48.177140
1802.454042	156.376944	48.182145
1799.129303	164.943707	48.187149
1796.055053	163.642384	48.192154
1792.593807	154.692380	48.197159
1788.820533	167.836135	48.202164
1785.380866	161.455874	48.207169
1782.136076	156.834280	48.212173
1778.168844	156.390514	48.217178
1774.985656	158.756596	48.222183
1770.576840	172.010685	48.227188
1767.669282	158.867926	48.232193
1764.257422	158.038191	48.237197
1760.723742	156.194921	48.242202
1757.660339	150.167927	48.247207
1753.714182	166.440265	48.252212
1750.224725	149.183228	48.257217
1746.798581	154.098632	48.262221
1743.350535	157.817638	48.267226
1740.079585	155.602015	48.272231
1736.162468	158.646855	48.277236
1732.878238	146.790259	48.282241
1729.196129	158.545899	48.287245
1725.910311	151.869524	48.292250
1722.557533	155.040779	48.297255
1718.411246	156.457952	48.302260
1715.076891	160.178521	48.307265
1711.634306	153.140284	48.312269
1708.107862	160.086921	48.317274
1704.951693	157.708894	48.322279
1701.217730	160.985569	48.327284
1697.774886	162.882901	48.332289
1694.327261	162.504323	48.337293
1690.716546	159.408495	48.342298
1687.315114	159.061955	48.347303
1683.446718	167.216976	48.352308
1680.083088	158.220940	48.357313
1676.783706	165.066148	48.362317
1673.269229	161.854776	48.367322
1669.889860	152.449309	48.372327
1666.218376	163.374218	48.377332
1662.827897	157.891914	48.382337
1659.024328	161.911262	48.387341
1655.504018	159.710653	48.392346
1652.265104	152.070872	48.397351
1648.688506	154.820345	48.402356
1645.504539	154.037110	48.407361
1641.522972	148.745041	48.412365
1638.284077	163.532049	48.417370
1634.866995	151.038764	48.422375
1630.964128	161.131069	48.427380
1627.934307	147.825102	48.432385
1624.420653	160.440807	48.437389
1620.941023	154.991817	48.442394
1617.582284	152.914322	48.447399
1613.182396	158.576412	48.452404
1610.052303	162.984970	48.457409
1606.918130	154.182956	48.462413
1602.939498	152.758277	48.467418
1599.391092	147.117610	48.472423
1596.032319	158.635598	48.477428
1592.911524	155.570788	48.482433
1588.973108	153.058651	48.487437
1585.442472	158.236724	48.492442
1582.312200	149.973019	48.497447
1578.683557	161.582775	48.502452
1575.044310	154.945971	48.507457
1571.531538	155.071004	48.512461
1568.112904	159.632645	48.517466
1564.707064	150.871807	48.522471
1561.061776	155.343621	48.527476
1557.764363	154.044997	48.532481
1554.161831	155.028499	48.537485
1550.375407	149.367211	48.542490
1546.971334	140.651687	48.547495
1543.299351	149.152052	48.552500
1540.488464	144.565700	48.557505
1537.053907	140.728301	48.562509
1533.261799	151.636913	48.567514
1529.736763	142.674194	48.572519
1525.874173	153.327461	48.577524
1522.332533	141.329662	48.582529
1518.942521	144.951810	48.587533
1516.109742	146.223732	48.592538
1512.358041	148.311950	48.597543
1508.392428	141.341767	48.602548
1505.107892	143.904745	48.607553
1501.860106	155.627240	48.612557
1497.831967	161.706349	48.617562
1494.029629	154.179336	48.622567
1490.701607	153.279115	48.627572
1487.841599	142.325104	48.632577
1484.142330	150.749112	48.637581
1480.553378	148.262004	48.642586
1477.231333	151.251334	48.647591
1473.681703	151.878247	48.652596
1469.997676	151.222966	48.657601
1466.615193	146.611537	48.662605
1463.119435	143.480322	48.667610
1459.772258	146.401197	48.672615
1455.884295	146.352701	48.677620
1452.287269	151.227675	48.682625
1449.055310	155.269146	48.687629
1445.424574	147.860837	48.692634
1442.091998	147.564273	48.697639
1438.426249	157.287579	48.702644
1435.004154	144.149610	48.707649
1431.676524	140.234236	48.712653
1427.807826	142.364747	48.717658
1424.406980	148.568754	48.722663
1421.203382	158.242135	48.727668
1417.968114	147.757893	48.732673
1413.940025	152.443454	48.737677
1410.201536	150.611613	48.742682
1406.794893	148.704208	48.747687
1403.477354	152.357283	48.752692
1399.873212	146.478728	48.757697
1396.864266	142.408487	48.762701
1393.067982	152.812308	48.767706
1389.720229	145.767346	48.772711
1385.979200	143.955088	48.777716
1382.480872	142.735582	48.782721
1379.127154	152.757036	48.787725
1375.175936	146.331618	48.792730
1371.807137	144.861799	48.797735
1368.209989	145.937105	48.802740
1365.182808	133.416329	48.807745
1361.786361	146.339408	48.812749
1358.135977	146.486164	48.817754
1354.864034	138.938516	48.822759
1350.598552	142.297390	48.827764
1346.993509	142.530199	48.832769
1343.949014	141.567633	48.837773
1340.248604	151.714299	48.842778
1336.941580	141.291719	48.847783
1333.087631	139.130134	48.852788
1330.271097	143.030591	48.857793
1326.695776	137.411179	48.862797
1322.851870	150.638145	48.867802
1319.389824	137.444529	48.872807
1315.706859	145.916084	48.877812
1312.417735	141.823146	48.882817
1309.034059	143.986459	48.887821
1305.275040	145.329126	48.892826
1302.138424	140.439198	48.897831
1298.569960	142.345543	48.902836
1294.630809	143.987557	48.907841
1291.335315	147.153388	48.912845
1288.079673	142.428977	48.917850
1284.628912	142.777232	48.922855
1280.627123	151.814201	48.927860
1277.192366	143.020694	48.932865
1273.961736	137.170098	48.937869
1270.319367	142.363504	48.942874
1267.210057	146.363309	48.947879
1263.100731	143.635015	48.952884
1259.704445	142.654092	48.957889
1256.758122	135.300552	48.962893
1253.108404	139.040607	48.967898
1249.870393	137.708709	48.972903
1245.701778	144.942577	48.977908
1241.967557	146.372168	48.982913
1238.681499	137.432161	48.987917
1235.214026	136.137023	48.992922
1232.271914	129.935655	48.997927
1228.330937	130.838602	49.002932
1224.838450	138.056616	49.007937
1221.397671	143.793354	49.012941
1217.887538	153.331043	49.017946
1214.315463	135.331984	49.022951
1210.928303	143.246762	49.027956
1206.994804	137.957609	49.032961
1203.789264	138.170662	49.037965
1200.299829	140.040533	49.042970
1197.027924	134.070131	49.047975
1193.115423	131.700883	49.052980
1189.664051	134.540303	49.057985
1186.291407	140.475570	49.062989
1182.653853	140.111214	49.067994
1179.452684	128.812854	49.072999
1175.483650	142.457450	49.078004
1172.364592	139.509874	49.083009
1168.799006	136.791232	49.088013
1165.219077	150.120893	49.093018
1161.799353	137.438039	49.098023
1158.079417	140.469889	49.103028
1154.829872	134.609883	49.108033
1151.120096	132.040603	49.113037
1148.048363	141.680889	49.118042
1144.651806	135.253184	49.123047
1140.799362	140.865240	49.128052
1137.243718	144.386376	49.133057
1133.661453	139.453628	49.138061
1130.068992	149.998976	49.143066
1126.767206	133.030610	49.148071
1123.125523	128.134537	49.153076
1119.793306	134.552560	49.158081
1116.708598	131.777740	49.163085
1112.700117	138.791060	49.168090
1109.160803	139.567510	49.173095
1105.422862	143.402386	49.178100
1101.949686	146.870840	49.183105
1098.873639	143.101792	49.188109
1095.482471	140.144206	49.193114
1092.116373	138.939374	49.198119
1088.137001	137.900872	49.203124
1084.611286	146.874272	49.208129
1081.237183	133.426569	49.213133
1077.673108	137.294483	49.218138
1074.130581	132.740815	49.223143
1070.457556	130.579145	49.228148
1067.075454	130.223952	49.233153
1063.846769	140.296358	49.238157
1060.100951	141.590272	49.243162
1056.842483	133.554397	49.248167
1053.259691	134.608235	49.253172
1049.524727	138.204474	49.258177
1046.638427	132.230815	49.263181
1042.786323	136.359506	49.268186
1039.561568	126.437054	49.273191
1035.340147	131.336839	49.278196
1032.124155	137.276893	49.283201
1028.395510	132.052111	49.288205
1025.056561	131.664751	49.293210
1021.829846	134.684809	49.298215
1018.115556	139.703812	49.303220
1014.730149	136.383815	49.308225
1011.178617	132.671951	49.313229
1007.547930	139.942373	49.318234
1004.427282	135.751562	49.323239
1000.635748	138.939827	49.328244
996.844931	138.192280	49.333249
993.536873	133.526890	49.338253
990.139427	141.927979	49.343258
986.848846	134.035015	49.348263
983.223009	137.284102	49.353268
979.692723	129.096300	49.358273
976.000871	127.329143	49.363277
972.307836	137.516480	49.368282
969.327386	123.922286	49.373287
965.649247	137.219367	49.378292
962.218136	136.856768	49.383297
958.743036	135.915946	49.388301
954.792823	130.263142	49.393306
951.498502	131.042613	49.398311
948.041714	136.579917	49.403316
944.404698	136.522131	49.408321
941.473483	130.504666	49.413325
937.535749	132.878674	49.418330
933.750150	129.808252	49.423335
930.177829	133.551344	49.428340
927.211287	126.473719	49.433345
923.587105	124.970701	49.438349
920.048051	144.486194	49.443354
916.585749	128.786021	49.448359
912.974419	136.254199	49.453364
909.498794	133.561544	49.458369
906.346265	138.774062	49.463373
902.375204	132.913209	49.468378
898.891078	133.297862	49.473383
895.376621	138.781594	49.478388
892.163462	131.672357	49.483393
888.891309	124.246685	49.488397
885.234126	125.672310	49.493402
881.583965	121.954373	49.498407
877.583601	135.800122	49.503412
874.513495	128.296641	49.508417
870.928141	125.335437	49.513421
867.377356	125.034738	49.518426
864.121532	129.542113	49.523431
860.608549	123.564296	49.528436
857.035071	131.946828	49.533441
853.664510	132.812588	49.538445
850.027590	132.828074	49.543450
846.686510	127.608617	49.548455
842.940206	132.671925	49.553460
839.322569	124.200718	49.558465
835.767309	122.492391	49.563469
832.320942	128.681631	49.568474
828.941330	123.264517	49.573479
825.484456	133.372836	49.578484
822.020580	128.340854	49.583489
818.758522	127.669396	49.588493
814.883101	132.584570	49.593498
811.440639	128.337613	49.598503
807.571230	128.884537	49.603508
804.126122	128.060832	49.608513
800.782560	125.838975	49.613517
797.109115	137.581171	49.618522
794.390107	125.682017	49.623527
790.826848	132.656093	49.628532
787.240583	126.759724	49.633537
783.807372	132.433946	49.638541
779.613822	134.143149	49.643546
776.023433	133.397173	49.648551
772.748399	134.740139	49.653556
769.260250	132.751794	49.658561
766.251229	125.934499	49.663565
762.497138	136.405594	49.668570
759.085611	125.207506	49.673575
755.072363	134.540415	49.678580
751.866291	138.239636	49.683585
748.529692	134.199195	49.688589
745.165572	129.744561	49.693594
741.427493	129.316681	49.698599
738.012532	126.351674	49.703604
734.352798	126.048187	49.708609
730.940695	122.172795	49.713613
726.815375	128.973688	49.718618
724.119029	118.897983	49.723623
720.507147	130.938283	49.728628
716.635291	128.764813	49.733633
713.337701	117.184825	49.738637
709.854900	129.586414	49.743642
706.523022	119.929030	49.748647
702.741727	119.481890	49.753652
699.200828	124.761551	49.758657
695.934225	116.950514	49.763661
691.749489	130.313233	49.768666
688.797688	124.656540	49.773671
685.700737	120.483561	49.778676
682.155075	127.084797	49.783681
678.579783	112.110420	49.788685
674.989467	127.711077	49.793690
671.085223	120.632092	49.798695
667.846319	121.542910	49.803700
664.618128	130.374623	49.808705
661.067598	118.530654	49.813709
656.926812	123.672789	49.818714
653.449686	129.174398	49.823719
650.414020	116.508011	49.828724
646.611639	130.763604	49.833729
643.246584	121.075650	49.838733
639.545793	130.330315	49.843738
636.675354	122.230396	49.848743
632.926830	120.295701	49.853748
629.138568	121.593836	49.858753
625.755907	119.848247	49.863757
621.945011	122.638838	49.868762
618.738685	109.250447	49.873767
615.293175	118.521891	49.878772
611.745218	125.633869	49.883777
608.427175	124.318649	49.888781
605.031889	123.389374	49.893786
601.027106	117.554919	49.898791
597.504669	124.445418	49.903796
594.061585	130.836162	49.908801
590.984165	124.636337	49.913805
587.184044	127.165875	49.918810
583.687632	122.949348	49.923815
580.392385	118.049119	49.928820
576.645329	121.498945	49.933825
573.555013	120.075623	49.938829
569.534344	127.865751	49.943834
566.220312	126.663959	49.948839
562.591540	122.103686	49.953844
558.946090	124.811701	49.958849
555.996285	115.215356	49.963853
552.129920	122.603052	49.968858
548.684720	114.322232	49.973863
545.214081	120.804000	49.978868
541.823934	122.294055	49.983873
538.305682	115.202245	49.988877
534.533252	123.527349	49.993882
531.353969	114.572843	49.998887
527.783993	120.131938	50.003892
524.511156	120.393912	50.008897
520.827341	114.480575	50.013901
517.104797	113.029696	50.018906
513.424136	116.841946	50.023911
510.107586	125.727055	50.028916
506.624804	119.719091	50.033921
503.342909	128.862311	50.038925
499.524888	127.441453	50.043930
495.829901	112.016415	50.048935
492.933070	120.101935	50.053940
489.094214	120.468848	50.058945
485.886861	114.605953	50.063949
481.958078	115.731710	50.068954
478.771506	118.484426	50.073959
475.272732	112.345148	50.078964
471.631863	110.090266	50.083969
468.355043	117.033353	50.088973
464.268335	120.575788	50.093978
460.711126	122.983143	50.098983
457.569929	111.894523	50.103988
454.145297	124.812157	50.108993
450.997399	111.402008	50.113997
447.433014	121.089886	50.119002
443.512552	120.062155	50.124007
439.853265	114.205218	50.129012
435.936089	135.053419	50.134017
432.838693	119.962694	50.139021
429.669236	118.339056	50.144026
426.242092	119.398816	50.149031
422.912700	118.228687	50.154036
419.107774	117.920486	50.159041
415.959716	115.012016	50.164045
412.000769	119.715987	50.169050
408.431848	121.155416	50.174055
404.987515	126.792284	50.179060
401.291052	116.993039	50.184065
398.346457	118.476559	50.189069
394.351601	116.856154	50.194074
391.250708	114.123617	50.199079
387.522452	110.339315	50.204084
384.170063	109.110271	50.209089
380.737414	108.187753	50.214093
377.242011	117.249761	50.219098
373.733095	111.499423	50.224103
370.036253	117.544163	50.229108
366.479363	115.684154	50.234113
363.033909	106.672614	50.239117
359.072829	119.810715	50.244122
355.595167	116.427787	50.249127
352.715768	113.027737	50.254132
349.091351	110.902058	50.259137
346.008650	106.019731	50.264141
341.910699	112.089637	50.269146
338.554845	108.810688	50.274151
334.941854	115.921397	50.279156
331.297735	118.275751	50.284161
327.904549	107.670985	50.289165
324.571090	117.144112	50.294170
321.089470	118.574293	50.299175
317.784955	107.606167	50.304180
314.080468	121.450722	50.309185
310.748969	110.589681	50.314189
306.914576	122.501333	50.319194
302.880043	120.178357	50.324199
299.952798	120.014476	50.329204
296.156770	120.584041	50.334209
293.028408	118.935155	50.339213
289.396381	127.364494	50.344218
285.821319	121.309638	50.349223
282.481492	112.052957	50.354228
278.685716	122.430665	50.359233
275.506828	117.148919	50.364237
272.299634	121.712394	50.369242
268.745651	114.510508	50.374247
265.280904	111.775148	50.379252
261.341111	102.628856	50.384257
258.168668	106.955110	50.389261
253.977067	114.056875	50.394266
250.650581	105.852183	50.399271
247.412147	109.163818	50.404276
243.845517	111.344192	50.409281
240.614270	96.120712	50.414285
236.679364	114.354702	50.419290
233.361114	111.464481	50.424295
229.965150	103.687688	50.429300
226.310542	118.268987	50.434305
222.902938	108.659891	50.439309
218.907626	112.469608	50.444314
215.879953	113.999761	50.449319
212.412769	107.458251	50.454324
208.697376	115.188078	50.459329
205.367721	117.760630	50.464333
201.578874	112.863492	50.469338
198.099433	114.615658	50.474343
194.909524	114.541115	50.479348
191.357092	120.383503	50.484353
188.310916	109.093494	50.489357
184.505348	117.627019	50.494362
180.886556	110.764310	50.499367
177.113465	110.810796	50.504372
173.853768	113.254770	50.509377
170.735721	114.718416	50.514381
166.994053	112.443191	50.519386
162.898158	109.716304	50.524391
159.715718	115.956660	50.529396
156.258472	117.680123	50.534401
152.996791	103.899935	50.539405
149.334429	121.520351	50.544410
145.798748	118.930824	50.549415
141.944353	118.114042	50.554420
138.597004	120.198603	50.559425
135.658878	110.392668	50.564429
131.811754	119.855658	50.569434
128.193903	117.099189	50.574439
124.886423	126.990652	50.579444
121.458274	122.476095	50.584449
117.897239	113.603691	50.589453
114.172949	116.817276	50.594458
110.784667	108.513415	50.599463
107.437446	116.447979	50.604468
103.513111	120.420099	50.609473
100.601805	116.305434	50.614477
96.790667	119.130850	50.619482
93.135563	109.990080	50.624487
89.493821	103.749115	50.629492
86.128940	123.246114	50.634497
82.775301	114.299146	50.639501
79.355353	117.990241	50.644506
75.502532	103.956745	50.649511
72.417415	105.412838	50.654516
68.925052	106.594976	50.659521
65.729819	106.897926	50.664525
61.389173	116.299620	50.669530
58.147865	111.817529	50.674535
55.043259	105.553567	50.679540
51.054008	114.923725	50.684545
47.685302	106.838485	50.689549
44.375015	110.722004	50.694554
40.522177	113.903458	50.699559
37.318181	109.433362	50.704564
33.685904	115.597526	50.709569
30.068439	105.830758	50.714573
26.246218	116.494635	50.719578
22.908538	112.331243	50.724583
19.917519	105.949832	50.729588
16.471228	104.485621	50.734593
12.696347	101.418213	50.739597
8.974276	110.832173	50.744602
5.589919	110.468710	50.749607
2.336624	108.505855	50.754612