Tue Jun 21 12:51:55 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.387482	104.444263	0.000000
-0.402852	104.580339	0.005005
-0.346513	96.294673	0.010010
-0.391891	110.433989	0.015014
-0.318104	102.242322	0.020019
-0.271460	98.098144	0.025024
-0.567784	93.226157	0.030029
-0.352319	74.622174	0.035034
-0.833756	65.423313	0.040038
-1.208562	54.803559	0.045043
-1.660922	45.982131	0.050048
-1.873366	42.517075	0.055053
-1.793684	28.590344	0.060058
-2.437734	23.815031	0.065062
-2.937546	16.894500	0.070067
-2.901040	18.841343	0.075072
-3.241126	9.641013	0.080077
-3.489753	-5.163131	0.085082
-3.680791	0.175264	0.090086
-4.092294	-6.293778	0.095091
-4.535287	-2.445165	0.100096
-5.162856	0.426823	0.105101
-5.179376	-1.029647	0.110106
-5.240241	3.013605	0.115110
-5.611930	6.545928	0.120115
-5.386699	1.902945	0.125120
-6.442999	0.406519	0.130125
-6.458183	-4.990721	0.135130
-7.041490	3.384077	0.140134
-7.020096	2.974497	0.145139
-7.208539	-2.645259	0.150144
-7.269574	4.853920	0.155149
-7.261137	-1.812336	0.160154
-8.276122	-1.005817	0.165158
-8.573308	-4.549970	0.170163
-8.524966	0.556387	0.175168
-8.856477	11.622363	0.180173
-8.293658	3.362794	0.185178
-8.799865	1.045342	0.190182
-8.810230	3.688637	0.195187
-9.555917	-3.028566	0.200192
-10.406488	6.305327	0.205197
-9.848749	-0.019730	0.210202
-10.184898	-2.376589	0.215206
-10.618269	8.331122	0.220211
-11.515468	0.743901	0.225216
-11.736307	12.573584	0.230221
-11.642800	1.025024	0.235226
-11.707427	8.215775	0.240230
-11.854011	1.826787	0.245235
-11.672757	2.117317	0.250240
-12.030928	10.756956	0.255245
-12.465060	4.087023	0.260250
-12.918292	5.582160	0.265254
-13.294723	1.621730	0.270259
-13.535886	2.700897	0.275264
-13.801199	10.963842	0.280269
-13.455979	8.283202	0.285274
-13.850299	6.499362	0.290278
-14.431985	14.053977	0.295283
-14.658972	0.048209	0.300288
-14.951059	5.413798	0.305293
-15.111261	2.724700	0.310298
-15.037933	7.364569	0.315302
-15.653156	9.168323	0.320307
-16.307353	1.628875	0.325312
-16.556460	8.037753	0.330317
-16.220855	1.379479	0.335322
-16.418253	-2.482131	0.340326
-16.687753	2.224965	0.345331
-17.139913	2.432916	0.350336
-17.767474	12.714578	0.355341
-17.739421	2.853993	0.360346
-17.750779	-5.463623	0.365350
-18.272104	-8.802531	0.370355
-17.736819	-1.279558	0.375360
-18.901558	4.077208	0.380365
-19.209596	-0.256455	0.385370
-19.347901	1.915877	0.390374
-19.539093	2.081206	0.395379
-19.358047	2.353813	0.400384
-19.621478	8.099260	0.405389
-19.640427	-11.088190	0.410394
-20.289189	-6.702106	0.415398
-20.905350	2.623753	0.420403
-20.626296	-5.297559	0.425408
-21.132502	4.585320	0.430413
-21.289431	-4.014058	0.435418
-22.543844	-1.777477	0.440422
-22.483841	7.706368	0.445427
-22.020127	-3.231177	0.450432
-22.477325	2.713299	0.455437
-22.446676	-1.493717	0.460442
-22.683174	-5.547172	0.465446
-22.896302	-6.017964	0.470451
-23.554907	0.836023	0.475456
-24.128078	5.448169	0.480461
-24.364419	-8.107699	0.485466
-24.295417	1.801681	0.490470
-24.402029	4.539453	0.495475
-24.319705	-4.456716	0.500480
-24.673288	0.788025	0.505485
-25.040986	0.254818	0.510490
-25.493754	5.571437	0.515494
-25.987157	1.190325	0.520499
-26.310376	-6.008863	0.525504
-26.534532	1.927778	0.530509
-26.231411	-3.480730	0.535514
-26.035630	8.970428	0.540518
-26.822563	-4.167089	0.545523
-27.061627	-0.807294	0.550528
-27.702238	-2.976588	0.555533
-27.403406	-0.932687	0.560538
-28.013764	-3.875405	0.565542
-28.259643	3.740813	0.570547
-28.028999	-2.757209	0.575552
-28.794126	-1.941147	0.580557
-28.740649	-4.943671	0.585562
-29.171097	3.322343	0.590566
-29.153610	-2.995341	0.595571
-29.746198	-1.852454	0.600576
-30.572383	-0.554063	0.605581
-30.687954	3.619410	0.610586
-30.776236	5.114499	0.615590
-30.496974	4.205982	0.620595
-30.435457	-3.309505	0.625600
-30.797501	5.505215	0.630605
-30.790810	7.874352	0.635610
-31.832614	2.233111	0.640614
-32.287957	5.407511	0.645619
-32.017476	-1.057247	0.650624
-32.584649	7.932930	0.655629
-32.616261	1.863530	0.660634
-32.867396	11.061460	0.665638
-33.700580	7.648492	0.670643
-33.975822	3.200668	0.675648
-34.030650	11.535712	0.680653
-34.146652	-2.491191	0.685658
-34.335318	-5.807434	0.690662
-34.546825	11.420527	0.695667
-34.127958	-0.964532	0.700672
-34.507202	-3.147111	0.705677
-34.817241	-6.322093	0.710682
-35.629801	-0.062830	0.715686
-35.850279	3.916672	0.720691
-35.859189	7.233422	0.725696
-35.975424	6.983780	0.730701
-36.810889	2.896312	0.735706
-37.237498	4.738296	0.740710
-37.077279	3.302286	0.745715
-37.266702	0.178567	0.750720
-37.501242	2.139507	0.755725
-37.571189	-5.285536	0.760730
-37.405906	0.306429	0.765734
-38.015465	0.680752	0.770739
-38.369466	3.406605	0.775744
-38.816753	8.463614	0.780749
-39.194625	2.619682	0.785754
-38.861489	4.427811	0.790758
-39.300421	7.693030	0.795763
-39.259094	0.723158	0.800768
-40.404292	-1.252660	0.805773
-40.385358	-8.166922	0.810778
-40.456563	1.015611	0.815782
-40.690009	-2.508903	0.820787
-40.475399	-5.191198	0.825792
-41.436379	4.848885	0.830797
-41.681413	4.502368	0.835802
-41.806892	-7.298026	0.840806
-42.334498	-3.564455	0.845811
-42.229462	-3.844227	0.850816
-42.220001	5.512219	0.855821
-42.227172	-3.713231	0.860826
-43.055114	2.578972	0.865830
-43.149470	2.101733	0.870835
-43.034856	-1.825555	0.875840
-43.442060	8.666281	0.880845
-44.239459	2.242991	0.885850
-44.811217	-0.292704	0.890854
-45.107129	6.153524	0.895859
-44.293184	-11.134578	0.900864
-44.783259	3.172798	0.905869
-45.022066	0.109551	0.910874
-44.685729	0.245736	0.915878
-45.899860	6.900853	0.920883
-46.129799	0.310580	0.925888
-46.531815	10.622577	0.930893
-46.616047	1.840072	0.935898
-46.667283	1.222098	0.940902
-46.771914	7.690128	0.945907
-47.023424	1.828824	0.950912
-48.004215	3.914331	0.955917
-48.183504	4.628645	0.960922
-48.306303	10.502948	0.965926
-48.648613	2.578169	0.970931
-48.402087	0.414902	0.975936
-48.813173	4.026566	0.980941
-48.547069	1.598196	0.985946
-48.421902	-0.429732	0.990950
-49.153992	8.948877	0.995955
-49.096004	-4.414588	1.000960
-49.980417	6.644080	1.005965
-50.451014	-8.856189	1.010970
-51.154343	-4.696286	1.015974
-51.901780	5.902803	1.020979
-50.928723	-0.710665	1.025984
-50.542541	9.204997	1.030989
-51.284878	1.848676	1.035994
-51.448034	11.354873	1.040998
-51.680722	2.230900	1.046003
-52.189185	1.930771	1.051008
-53.326995	5.189577	1.056013
-53.709757	-4.059710	1.061018
-52.803967	0.481567	1.066022
-53.316714	2.842398	1.071027
-53.472203	-11.406466	1.076032
-54.021827	3.056403	1.081037
-53.694651	-5.322403	1.086042
-53.661933	-2.447077	1.091046
-54.232351	4.858017	1.096051
-54.751789	-3.726119	1.101056
-55.203527	-2.085002	1.106061
-55.332967	1.717412	1.111066
-55.192060	-4.036010	1.116070
-55.786277	-7.635555	1.121075
-56.237016	-7.824869	1.126080
-56.450378	-5.000354	1.131085
-56.335033	-7.493347	1.136090
-56.792879	-3.301477	1.141094
-56.927690	0.652195	1.146099
-56.621796	-7.761959	1.151104
-57.821221	0.068011	1.156109
-58.109662	-9.884400	1.161114
-57.728527	-3.211081	1.166118
-58.224408	5.252053	1.171123
-57.794376	-8.800145	1.176128
-58.647770	-6.648316	1.181133
-59.397998	-2.632789	1.186138
-59.681351	-6.231323	1.191142
-59.809295	6.494055	1.196147
-59.228459	-3.117665	1.201152
-59.435066	6.093409	1.206157
-60.367306	3.425013	1.211162
-60.427020	-3.832017	1.216166
-61.058295	11.998285	1.221171
-61.005683	-1.211950	1.226176
-61.319808	0.919247	1.231181
-61.392754	-3.542536	1.236186
-61.604590	1.452984	1.241190
-62.579487	12.950316	1.246195
-62.665463	-0.846728	1.251200
-63.106297	-3.872768	1.256205
-62.996425	2.560724	1.261210
-63.058092	-6.849084	1.266214
-63.283870	-0.855710	1.271219
-62.788574	-13.161459	1.276224
-63.357809	3.260425	1.281229
-64.028406	0.402872	1.286234
-64.458823	3.006011	1.291238
-64.659508	3.254413	1.296243
-64.398335	0.591243	1.301248
-64.746318	0.032871	1.306253
-65.371958	-1.916698	1.311258
-65.861670	0.428281	1.316262
-66.156304	10.745583	1.321267
-66.083843	-3.145185	1.326272
-66.266809	3.487564	1.331277
-66.067528	5.769751	1.336282
-66.598172	-1.434155	1.341286
-67.026688	0.854909	1.346291
-67.215207	-7.741203	1.351296
-67.368360	-8.255274	1.356301
-67.777575	-6.451689	1.361306
-67.794466	-2.222731	1.366310
-68.595522	-4.847728	1.371315
-68.900169	8.186337	1.376320
-69.493133	6.274770	1.381325
-69.498937	2.970671	1.386330
-69.060443	-1.579757	1.391334
-69.305559	7.206325	1.396339
-69.389340	-10.868864	1.401344
-69.634737	-0.059089	1.406349
-70.356292	-5.865831	1.411354
-70.292837	-0.683246	1.416358
-70.766703	-2.195399	1.421363
-70.924557	-9.959895	1.426368
-71.054621	0.237597	1.431373
-71.969115	1.131682	1.436378
-72.279477	4.302401	1.441382
-72.662880	3.439095	1.446387
-72.435513	1.177768	1.451392
-72.730298	-1.998355	1.456397
-72.803062	-10.883192	1.461402
-72.503061	-5.298742	1.466406
-72.769603	-0.466632	1.471411
-73.324760	-10.755921	1.476416
-74.123565	1.460333	1.481421
-74.118685	-2.694659	1.486426
-74.119708	-5.254615	1.491430
-74.523125	-3.904475	1.496435
-74.383604	-3.745762	1.501440
-75.219857	-3.474985	1.506445
-75.784042	-7.102786	1.511450
-75.790166	-0.337117	1.516454
-76.201813	3.266550	1.521459
-75.806730	-5.185661	1.526464
-75.902646	-3.270765	1.531469
-76.000167	3.951871	1.536474
-76.938443	1.941598	1.541478
-77.469862	-0.841913	1.546483
-77.109917	-1.108253	1.551488
-77.617490	-4.557174	1.556493
-77.511407	-3.261810	1.561498
-77.269767	-1.919434	1.566502
-78.304454	-0.015422	1.571507
-78.475071	1.983871	1.576512
-78.978105	2.526447	1.581517
-78.816102	3.120503	1.586522
-79.670162	-8.573039	1.591526
-80.385739	4.103427	1.596531
-79.675708	-2.319472	1.601536
-80.285083	-5.187950	1.606541
-80.638016	12.347785	1.611546
-80.585087	7.275127	1.616550
-80.690151	-1.545559	1.621555
-80.500246	-4.890355	1.626560
-80.906208	9.605757	1.631565
-81.580872	-2.000085	1.636570
-81.995981	-3.672730	1.641574
-82.304249	5.298448	1.646579
-82.239768	-3.859339	1.651584
-82.322721	-0.492441	1.656589
-82.547250	-0.827156	1.661594
-83.258852	-7.573467	1.666598
-83.621504	7.763806	1.671603
-83.839431	-2.250999	1.676608
-84.032644	-1.149973	1.681613
-83.823065	-6.195881	1.686618
-83.799645	-7.451369	1.691622
-84.564335	3.947409	1.696627
-84.917509	-1.143042	1.701632
-85.249443	1.521932	1.706637
-85.239988	-7.009481	1.711642
-85.212954	-3.199435	1.716646
-85.822656	0.849064	1.721651
-86.483790	-10.779533	1.726656
-86.701465	-1.043305	1.731661
-87.237441	-3.904203	1.736666
-86.983177	-2.860905	1.741670
-87.390097	2.886597	1.746675
-87.227749	-11.110807	1.751680
-87.223056	-5.719384	1.756685
-87.281005	-3.174771	1.761690
-87.851022	-10.682750	1.766694
-88.365096	1.517923	1.771699
-88.561108	-5.911890	1.776704
-88.766439	5.571656	1.781709
-89.032503	2.370057	1.786714
-89.169806	-4.876488	1.791718
-90.031986	-3.868717	1.796723
-90.182479	-5.825536	1.801728
-90.458336	-5.365771	1.806733
-90.541943	-2.919720	1.811738
-90.633576	-5.245038	1.816742
-90.859796	-1.723386	1.821747
-90.365657	-4.408759	1.826752
-90.929992	4.088405	1.831757
-91.785683	3.584319	1.836762
-92.041697	-3.973888	1.841766
-91.878419	1.057780	1.846771
-91.963481	-11.221909	1.851776
-92.557882	1.946173	1.856781
-93.073515	0.238475	1.861786
-93.390059	-3.139861	1.866790
-93.573226	5.758701	1.871795
-93.590975	-2.767025	1.876800
-93.569848	-0.550846	1.881805
-94.018788	-0.756438	1.886810
-93.865924	1.202900	1.891814
-94.651784	15.036732	1.896819
-95.011855	-4.169203	1.901824
-94.905343	1.890697	1.906829
-95.096446	3.967385	1.911834
-95.470189	-0.591201	1.916838
-95.986297	3.863303	1.921843
-96.279438	-1.740880	1.926848
-96.378707	4.953784	1.931853
-96.594273	-1.904868	1.936858
-96.606877	0.623553	1.941862
-97.144039	11.746672	1.946867
-97.807654	0.431451	1.951872
-98.130520	-2.617870	1.956877
-97.933727	3.057277	1.961882
-98.195483	-7.926667	1.966886
-98.475658	-2.183187	1.971891
-98.258626	-1.936080	1.976896
-98.126722	-4.642172	1.981901
-98.762107	-1.860836	1.986906
-99.656146	-5.216544	1.991910
-100.308135	4.841834	1.996915
-99.933829	-3.246212	2.006912
-99.653507	-1.515797	2.016909
-98.848758	0.490535	2.026906
-98.409783	-2.417965	2.036902
-98.518366	0.013480	2.046899
-97.557017	6.255804	2.056896
-96.870926	4.458501	2.066893
-96.785786	-1.627855	2.076890
-95.843145	5.145517	2.086886
-95.658318	-0.362419	2.096883
-95.358686	-3.567732	2.106880
-94.580855	-3.607487	2.116877
-94.280980	-4.301328	2.126874
-93.588627	4.586367	2.136870
-93.074558	-7.800904	2.146867
-92.707207	-5.486809	2.156864
-91.895822	-6.446943	2.166861
-91.363466	2.086303	2.176858
-91.459705	-3.636292	2.186854
-90.296014	-1.623212	2.196851
-89.844728	-6.838785	2.206848
-89.810204	-6.923980	2.216845
-89.120842	1.406030	2.226842
-88.612403	-1.792964	2.236838
-88.111151	3.662306	2.246835
-87.206795	-3.457353	2.256832
-86.915820	-1.200356	2.266829
-86.742647	0.725633	2.276826
-86.000066	7.451525	2.286822
-85.634467	-0.991058	2.296819
-85.303395	-5.103952	2.306816
-84.369594	-1.472310	2.316813
-83.656379	-0.459689	2.326810
-83.686069	3.661683	2.336806
-83.194229	-2.832665	2.346803
-82.337145	-4.506537	2.356800
-82.140686	-2.025631	2.366797
-81.697716	-1.004809	2.376794
-81.076623	0.766979	2.386790
-80.600537	-1.040197	2.396787
-79.844237	0.296245	2.406784
-79.257781	-1.104596	2.416781
-79.225557	-2.180699	2.426778
-78.474913	2.615618	2.436774
-77.710452	-0.082413	2.446771
-77.227546	-4.849368	2.456768
-77.135409	-1.050083	2.466765
-76.937913	-2.051207	2.476762
-76.013363	-3.208301	2.486758
-75.745871	1.706164	2.496755
-74.714813	-6.299703	2.506752
-74.372558	-4.608785	2.516749
-74.066359	-2.672619	2.526746
-73.676017	-3.459290	2.536742
-72.692871	-1.875692	2.546739
-72.439039	-8.567724	2.556736
-72.509434	-5.797423	2.566733
-71.417066	1.144003	2.576730
-71.216734	-1.583898	2.586726
-70.490072	-2.307713	2.596723
-69.740479	-2.258220	2.606720
-69.874747	-0.607926	2.616717
-68.884863	-3.441685	2.626714
-68.459366	3.949040	2.636710
-68.128585	-6.708640	2.646707
-66.965088	-4.160656	2.656704
-66.828171	-2.616326	2.666701
-66.599702	-3.498099	2.676698
-66.506191	2.066784	2.686694
-65.591885	-9.076575	2.696691
-65.088695	2.183251	2.706688
-63.799118	4.732487	2.716685
-63.878002	1.483556	2.726682
-63.673628	7.681918	2.736678
-63.311279	-4.083324	2.746675
-62.374430	-2.966658	2.756672
-61.909060	1.303313	2.766669
-61.677892	5.939273	2.776666
-60.884594	-2.903711	2.786662
-60.454991	-1.062865	2.796659
-60.088952	-0.492442	2.806656
-58.882701	-3.769451	2.816653
-58.663740	-1.427222	2.826650
-58.855473	0.253335	2.836646
-58.356390	-3.348762	2.846643
-57.305980	0.435674	2.856640
-57.013811	4.481024	2.866637
-56.393142	3.512567	2.876634
-56.035641	3.595578	2.886630
-55.444155	3.656635	2.896627
-55.010112	2.310871	2.906624
-54.128934	1.140415	2.916621
-54.158639	3.357260	2.926618
-53.602801	4.649253	2.936614
-52.769884	5.903068	2.946611
-52.081804	0.406831	2.956608
-52.356115	-1.106349	2.966605
-51.512212	-3.050503	2.976602
-50.902795	-0.056091	2.986598
-50.542895	-1.992213	2.996595
-49.353973	-2.586690	3.006592
-49.623923	3.363413	3.016589
-49.152590	1.213227	3.026586
-48.626969	-1.281054	3.036582
-47.646126	-11.985524	3.046579
-47.633579	-4.036798	3.056576
-46.820522	-2.404281	3.066573
-46.200265	2.748149	3.076570
-46.181412	-0.456507	3.086566
-45.827518	0.003898	3.096563
-45.025403	-4.488515	3.106560
-44.526543	-3.532071	3.116557
-43.331711	-2.138824	3.126554
-43.286459	2.333302	3.136550
-43.186303	-0.229425	3.146547
-42.801637	3.211606	3.156544
-42.053936	1.833068	3.166541
-41.081545	5.270823	3.176538
-40.844151	3.396877	3.186534
-40.196949	1.994279	3.196531
-39.924734	0.480101	3.206528
-39.667916	1.495794	3.216525
-38.888694	0.694717	3.226522
-38.375499	2.356937	3.236518
-38.390553	1.570619	3.246515
-37.276432	5.005454	3.256512
-36.917252	-8.914331	3.266509
-36.261626	-2.259980	3.276506
-35.597986	10.496676	3.286502
-35.269517	-1.044231	3.296499
-35.061907	-2.576558	3.306496
-34.511719	0.329663	3.316493
-33.893791	3.000406	3.326490
-33.761860	6.060061	3.336486
-32.848332	-1.079683	3.346483
-32.372574	-2.504866	3.356480
-31.853464	-0.815568	3.366477
-30.976016	-5.752179	3.376474
-30.989854	2.178199	3.386470
-30.503768	3.351537	3.396467
-30.148830	-4.760298	3.406464
-29.174049	1.880524	3.416461
-29.034510	1.098441	3.426458
-28.118902	-0.196066	3.436454
-27.480165	-2.458932	3.446451
-27.263212	-0.213777	3.456448
-27.360968	-4.335285	3.466445
-26.426615	-4.576205	3.476442
-26.028100	3.219304	3.486438
-25.563905	-3.377950	3.496435
-24.774641	-7.134793	3.506432
-24.094710	-9.393810	3.516429
-23.899764	-3.237158	3.526426
-23.460407	-5.633769	3.536422
-22.571859	-3.962969	3.546419
-22.420627	-8.691987	3.556416
-22.192622	-4.941874	3.566413
-21.327094	-10.623580	3.576410
-20.923182	-4.586692	3.586406
-20.343855	-2.557636	3.596403
-19.958576	-6.366726	3.606400
-19.672778	-2.172524	3.616397
-18.518521	2.399890	3.626394
-18.092800	-2.514870	3.636390
-18.374557	-7.870063	3.646387
-16.949140	-8.349379	3.656384
-16.431501	-4.039847	3.666381
-16.225022	-2.862687	3.676378
-16.216983	-3.119348	3.686374
-15.632295	-3.749304	3.696371
-14.809243	-5.187537	3.706368
-14.437402	-5.898032	3.716365
-13.590727	-5.997186	3.726362
-13.152489	-2.657099	3.736358
-13.000891	-4.409152	3.746355
-12.660524	-7.669616	3.756352
-11.830547	-2.616915	3.766349
-11.362669	-1.934524	3.776346
-10.645945	-4.174144	3.786342
-9.972176	-3.412038	3.796339
-10.002788	-3.352879	3.806336
-9.677587	-7.628992	3.816333
-8.695483	-1.984025	3.826330
-8.214708	1.572490	3.836326
-8.046862	-9.748772	3.846323
-7.175084	-6.869127	3.856320
-6.444192	-4.624903	3.866317
-6.467837	-0.401391	3.876314
-6.003314	-7.414615	3.886310
-5.245395	-6.748045	3.896307
-4.827431	-9.141705	3.906304
-4.705449	0.705292	3.916301
-3.806030	9.096966	3.926298
-3.720302	16.908122	3.936294
-2.999448	25.741935	3.946291
-2.841607	27.666124	3.956288
-2.320281	45.657529	3.966285
-1.643435	66.132160	3.976282
-1.396243	80.540713	3.986278
-0.917907	97.425301	3.996275
-0.868035	121.800071	4.006272
0.000000	146.794710	4.011277
0.199512	149.165291	4.016282
0.014895	161.390864	4.021286
0.159846	170.035291	4.026291
0.234786	187.267327	4.031296
0.165585	186.678960	4.036301
0.323746	195.125654	4.041306
0.347339	215.039729	4.046310
0.936479	215.210429	4.051315
0.592238	226.039889	4.056320
0.981048	218.728410	4.061325
0.735084	219.378587	4.066330
0.510177	221.687638	4.071334
0.860660	225.139498	4.076339
1.003749	228.935321	4.081344
1.219865	240.034707	4.086349
1.210910	225.835746	4.091354
0.840139	219.965093	4.096358
1.154033	229.630617	4.101363
0.809784	232.800675	4.106368
0.700330	251.007372	4.111373
1.139215	243.261146	4.116378
0.981365	252.007856	4.121382
1.342131	252.026929	4.126387
1.102613	251.540566	4.131392
1.454789	255.626392	4.136397
1.607569	251.451180	4.141402
1.139553	239.491622	4.146406
0.942876	238.343206	4.151411
0.852284	242.674226	4.156416
1.111395	252.556237	4.161421
1.059322	256.062528	4.166426
0.910389	252.896331	4.171430
1.293448	255.258834	4.176435
1.194597	258.039766	4.181440
1.261858	262.612439	4.186445
1.373599	260.844818	4.191450
1.181350	262.895876	4.196454
1.111949	252.700008	4.201459
0.970356	258.869774	4.206464
1.017520	258.732981	4.211469
1.119577	250.541291	4.216474
1.081288	265.765912	4.221478
1.333665	270.189927	4.226483
1.799852	282.770782	4.231488
1.439187	279.486112	4.236493
1.587357	271.429055	4.241498
1.347258	264.790025	4.246502
1.728056	257.473737	4.251507
1.581029	265.483188	4.256512
1.636984	264.492839	4.261517
1.803816	260.443961	4.266522
1.571456	260.937965	4.271526
1.865584	265.072873	4.276531
1.159320	265.041500	4.281536
1.385755	257.628621	4.286541
1.542928	267.255197	4.291546
1.521115	264.548266	4.296550
1.438940	260.920888	4.301555
1.458365	270.209544	4.306560
1.282670	264.439379	4.311565
1.231828	262.562517	4.316570
1.462230	282.701735	4.321574
2.006981	279.812578	4.326579
1.855236	282.183326	4.331584
1.962087	279.515276	4.336589
1.874107	267.102434	4.341594
1.333750	266.937816	4.346598
1.543593	265.484095	4.351603
1.606732	267.673624	4.356608
1.510775	267.987567	4.361613
1.672080	285.737431	4.366618
1.836527	288.180145	4.371622
1.849102	289.947658	4.376627
1.940603	291.356763	4.381632
1.970243	290.282757	4.386637
1.775653	275.102349	4.391642
1.399256	272.958524	4.396646
1.690883	271.613806	4.401651
1.550723	280.407134	4.406656
1.960326	281.868744	4.411661
1.718652	283.050234	4.416666
1.920150	284.972552	4.421670
2.193168	283.694260	4.426675
2.035735	291.488969	4.431680
1.982081	288.118729	4.436685
2.225572	289.067143	4.441690
1.696674	289.437186	4.446694
2.198109	286.013116	4.451699
1.737499	274.335681	4.456704
1.933982	276.505499	4.461709
2.009424	287.863241	4.466714
1.928423	294.603752	4.471718
2.161981	292.061931	4.476723
1.965618	277.969140	4.481728
2.074786	292.886784	4.486733
2.398067	285.136394	4.491738
1.713008	274.388285	4.496742
1.842133	276.968273	4.501747
1.547521	285.798823	4.506752
1.852942	287.526329	4.511757
2.499618	286.515321	4.516762
2.075650	295.074053	4.521766
2.227500	290.073326	4.526771
2.255046	294.727967	4.531776
1.996767	299.011980	4.536781
1.974506	290.589446	4.541786
1.520986	301.414558	4.546790
1.711172	290.429154	4.551795
1.716342	296.702705	4.556800
1.672835	319.833373	4.561805
2.041900	321.985474	4.566810
2.181630	323.201098	4.571814
2.455393	310.886192	4.576819
2.213238	322.383378	4.581824
2.313561	328.647106	4.586829
2.052915	321.812142	4.591834
2.079394	328.085137	4.596838
2.307434	314.725595	4.601843
2.376495	323.284795	4.606848
2.316054	319.330961	4.611853
2.130430	323.168806	4.616858
2.015993	330.066621	4.621862
2.115865	326.784617	4.626867
1.871745	322.720101	4.631872
2.129990	340.949490	4.636877
2.673950	341.819342	4.641882
2.624841	350.741887	4.646886
2.570165	341.887787	4.651891
2.461044	335.615793	4.656896
2.581708	343.023874	4.661901
2.573607	337.441423	4.666906
2.148635	330.260896	4.671910
2.495454	337.671190	4.676915
2.784865	347.678093	4.681920
2.583333	341.736152	4.686925
2.635557	337.129217	4.691930
2.241434	336.909203	4.696934
2.174934	339.897720	4.701939
2.419480	349.476528	4.706944
2.724893	354.416112	4.711949
2.965718	353.651289	4.716954
2.463546	356.037845	4.721958
2.418189	350.964178	4.726963
2.498422	355.703849	4.731968
2.398081	355.306129	4.736973
2.612832	362.401647	4.741978
2.561433	360.091117	4.746982
2.481303	361.355780	4.751987
3.062984	360.052813	4.756992
2.708060	356.057155	4.761997
2.826997	353.936478	4.767002
2.467467	359.475963	4.772006
2.786400	352.242890	4.777011
2.817790	362.901512	4.782016
2.560940	351.592847	4.787021
2.593982	351.755977	4.792026
2.656272	358.429571	4.797030
2.621426	350.855273	4.802035
2.738757	358.520058	4.807040
2.577057	350.721475	4.812045
2.968230	358.695532	4.817050
2.869184	372.638939	4.822054
3.185819	370.486511	4.827059
3.140928	357.994236	4.832064
2.570918	361.835750	4.837069
2.755002	346.993558	4.842074
2.737794	374.707070	4.847078
3.228946	374.081557	4.852083
3.037221	385.563533	4.857088
3.131189	377.162950	4.862093
3.054015	366.597298	4.867098
2.418990	369.217401	4.872102
2.770266	371.793574	4.877107
3.120024	390.736837	4.882112
3.327394	393.354011	4.887117
3.145643	390.682225	4.892122
2.821133	398.780139	4.897126
2.868576	396.303259	4.902131
2.940954	396.960918	4.907136
2.861690	395.316080	4.912141
2.864326	385.291327	4.917146
2.873466	392.262639	4.922150
2.886777	396.110581	4.927155
3.391917	389.955896	4.932160
3.287411	399.064457	4.937165
3.294458	388.750462	4.942170
3.009127	388.948156	4.947174
3.012562	388.901682	4.952179
2.813169	398.257629	4.957184
2.950106	384.846807	4.962189
3.016153	389.981343	4.967194
2.891340	411.640246	4.972198
3.142440	417.683481	4.977203
3.269871	432.739925	4.982208
3.635162	425.911580	4.987213
3.550388	421.106285	4.992218
3.378660	428.500662	4.997222
3.452624	417.805360	5.002227
3.381687	405.460233	5.007232
3.273051	401.968829	5.012237
3.487322	391.892055	5.017242
2.964139	402.777317	5.022246
3.367142	400.180583	5.027251
3.319547	413.522309	5.032256
3.231019	419.198885	5.037261
3.259289	418.283166	5.042266
3.008421	428.276574	5.047270
3.328721	423.767899	5.052275
3.356239	419.834402	5.057280
3.524407	432.303897	5.062285
3.429107	428.424284	5.067290
3.207009	435.102574	5.072294
3.484496	428.016243	5.077299
3.493381	426.423111	5.082304
3.475185	425.267820	5.087309
3.340608	426.237800	5.092314
3.282916	423.552569	5.097318
3.332598	426.633756	5.102323
3.379508	444.463328	5.107328
3.463458	460.512707	5.112333
3.561227	457.220762	5.117338
3.859809	466.440418	5.122342
3.765384	466.029086	5.127347
3.762155	463.293192	5.132352
3.505090	462.857088	5.137357
3.862175	455.355978	5.142362
3.509199	463.749517	5.147366
3.571915	456.671108	5.152371
4.080403	463.986020	5.157376
3.707944	465.137476	5.162381
3.918471	462.653710	5.167386
3.530061	453.770742	5.172390
3.852870	456.010839	5.177395
4.029300	447.652410	5.182400
3.943332	438.902501	5.187405
3.550156	435.642717	5.192410
3.490397	437.686659	5.197414
3.799430	448.332519	5.202419
3.910155	453.541771	5.207424
3.924165	451.215660	5.212429
3.938458	450.699300	5.217434
4.089587	461.177726	5.222438
3.811292	452.311849	5.227443
3.912552	446.608436	5.232448
3.713597	453.701458	5.237453
3.572024	451.846504	5.242458
3.429855	455.049451	5.247462
3.765759	454.388862	5.252467
4.017474	455.665875	5.257472
3.924723	454.956284	5.262477
4.309599	446.265358	5.267482
4.170795	463.547698	5.272486
4.250729	461.708359	5.277491
4.149694	463.320060	5.282496
4.100484	456.093038	5.287501
3.958598	454.073753	5.292506
3.943067	457.189621	5.297510
4.158359	456.116634	5.302515
4.157822	457.932910	5.307520
4.308142	455.252106	5.312525
4.436444	459.081614	5.317530
4.232596	456.006957	5.322534
4.220862	455.288687	5.327539
3.895763	445.095959	5.332544
3.857697	456.145432	5.337549
4.052061	461.849578	5.342554
3.964581	466.258489	5.347558
3.995637	456.965453	5.352563
4.104792	459.757563	5.357568
3.947617	466.518457	5.362573
3.950902	461.263633	5.367578
3.862119	472.441498	5.372582
3.516763	466.411630	5.377587
4.251903	481.929121	5.382592
4.387691	489.439950	5.387597
4.624663	483.328647	5.392602
4.300318	499.802663	5.397606
4.225541	502.545315	5.402611
4.277106	494.781598	5.407616
4.352382	497.122681	5.412621
4.680607	489.240534	5.417626
4.128236	490.962692	5.422630
4.213406	490.140360	5.427635
4.343330	499.822901	5.432640
4.145827	498.960941	5.437645
4.392923	493.491878	5.442650
4.269716	487.143416	5.447654
4.398946	492.764030	5.452659
4.512133	493.283705	5.457664
4.204524	499.104336	5.462669
4.550518	491.468091	5.467674
4.596141	486.956138	5.472678
4.785255	488.148403	5.477683
4.734519	491.862916	5.482688
4.565996	487.368267	5.487693
4.684421	481.550108	5.492698
4.638985	494.495880	5.497702
4.741584	486.125778	5.502707
4.746373	488.502606	5.507712
4.332978	497.015691	5.512717
4.723996	491.486486	5.517722
4.890675	492.149057	5.522726
4.502636	491.971842	5.527731
4.589069	491.793616	5.532736
4.437504	497.404486	5.537741
4.861233	488.343208	5.542746
4.596020	489.701283	5.547750
4.502802	499.926555	5.552755
4.771209	496.052610	5.557760
4.546255	495.868125	5.562765
4.721850	495.487464	5.567770
4.525217	496.822935	5.572774
4.632382	496.877688	5.577779
4.375195	489.591945	5.582784
4.077324	498.237853	5.587789
4.469944	488.362767	5.592794
4.579189	519.468587	5.597798
4.991638	522.383751	5.602803
5.296539	517.877796	5.607808
4.724105	514.193204	5.612813
4.817371	512.932226	5.617818
4.942067	513.914928	5.622822
4.982982	514.296790	5.627827
4.686009	509.116336	5.632832
4.561332	520.656575	5.637837
5.342557	520.696606	5.642842
4.994575	526.312581	5.647846
4.767532	535.365141	5.652851
5.136981	528.314647	5.657856
4.885254	526.818731	5.662861
5.007347	522.794757	5.667866
4.930456	527.142729	5.672870
4.824712	525.340641	5.677875
5.034274	523.680722	5.682880
4.806714	529.681305	5.687885
4.894105	521.976962	5.692890
4.622235	528.945928	5.697894
4.837764	530.071857	5.702899
4.777412	525.342803	5.707904
4.730307	536.343114	5.712909
5.175840	528.129528	5.717914
4.949608	524.765119	5.722918
4.681806	528.447305	5.727923
4.897902	545.655971	5.732928
5.229214	553.875468	5.737933
5.404414	549.301388	5.742938
5.139533	555.588581	5.747942
5.434248	545.738156	5.752947
5.446842	537.887529	5.757952
5.409009	551.780310	5.762957
5.310818	531.500989	5.767962
4.793685	536.087233	5.772966
5.082871	541.966141	5.777971
5.361969	543.312236	5.782976
5.471089	561.821938	5.787981
5.555721	558.617989	5.792986
5.440519	557.081505	5.797990
5.226351	549.501875	5.802995
5.595206	540.796183	5.808000
5.367634	538.182675	5.813005
5.265813	524.682009	5.818010
5.378479	533.344221	5.823014
5.547527	539.368924	5.828019
5.440572	529.172383	5.833024
4.960835	531.758510	5.838029
5.018844	534.050951	5.843034
5.540436	556.038154	5.848038
5.510475	558.005149	5.853043
5.485617	557.352393	5.858048
5.329183	557.873498	5.863053
5.442752	563.569945	5.868058
5.548964	555.798530	5.873062
5.486255	554.959438	5.878067
5.710770	554.299530	5.883072
5.478719	558.471916	5.888077
5.740760	549.862053	5.893082
5.221719	554.460460	5.898086
5.200915	549.904430	5.903091
5.581885	552.249565	5.908096
5.272905	557.587750	5.913101
5.455207	547.365204	5.918106
5.694501	554.361233	5.923110
5.659174	561.579951	5.928115
5.542597	557.970238	5.933120
5.565878	556.941866	5.938125
5.910829	550.252605	5.943130
5.849639	552.225953	5.948134
5.550342	556.636613	5.953139
5.771856	554.130687	5.958144
5.707904	559.649518	5.963149
5.655074	552.792078	5.968154
5.413922	560.845092	5.973158
4.939394	555.857816	5.978163
5.841488	569.031367	5.983168
5.799590	588.443879	5.988173
6.013470	576.729122	5.993178
5.863362	597.071671	5.998182
5.894541	589.830289	6.003187
6.217279	586.750306	6.008192
5.777382	579.155349	6.013197
5.954841	573.394476	6.018202
5.597273	561.887628	6.023206
5.488417	567.357458	6.028211
5.912306	576.597083	6.033216
6.020666	585.391860	6.038221
6.250056	588.853395	6.043226
5.573348	569.903792	6.048230
5.907407	574.921783	6.053235
5.850681	572.049880	6.058240
5.953288	577.094358	6.063245
5.870044	570.288518	6.068250
5.767025	564.037326	6.073254
5.867694	571.058685	6.078259
6.115474	567.434222	6.083264
5.603842	561.443691	6.088269
6.125298	557.749048	6.093274
5.800533	556.634645	6.098278
5.675469	555.655307	6.103283
6.082798	557.063053	6.108288
5.510219	559.028135	6.113293
5.892848	546.075366	6.118298
5.624756	568.096060	6.123302
5.823798	578.221877	6.128307
6.100188	576.959185	6.133312
5.675546	572.781817	6.138317
6.071123	570.897895	6.143322
5.610979	573.522028	6.148326
5.771820	592.940245	6.153331
6.081346	593.895900	6.158336
5.906355	581.936100	6.163341
5.659375	568.451737	6.168346
5.800634	585.256253	6.173350
5.953371	584.668615	6.178355
5.794513	591.739471	6.183360
5.691257	590.642062	6.188365
5.969836	596.930848	6.193370
6.075728	596.358662	6.198374
5.922727	586.243119	6.203379
5.484071	572.613279	6.208384
5.564448	587.684375	6.213389
6.044216	595.049493	6.218394
5.768094	594.712054	6.223398
5.699812	601.038346	6.228403
5.930915	590.077332	6.233408
6.082636	595.185910	6.238413
5.892330	589.809567	6.243418
6.015579	591.707584	6.248422
5.700722	585.810560	6.253427
6.129954	591.750167	6.258432
5.610620	574.414204	6.263437
5.931717	582.770191	6.268442
5.806672	582.721310	6.273446
5.788865	592.482640	6.278451
6.185663	584.273543	6.283456
5.813337	571.791900	6.288461
5.796169	553.415706	6.293466
5.876701	553.547688	6.298470
5.525382	567.096132	6.303475
6.037038	574.733224	6.308480
5.805933	591.217157	6.313485
5.989896	591.905090	6.318490
5.735114	581.610444	6.323494
5.946181	584.385504	6.328499
6.077836	572.907952	6.333504
5.711156	572.009274	6.338509
5.692010	558.227888	6.343514
5.418432	566.185828	6.348518
5.757656	584.793620	6.353523
5.897790	592.754704	6.358528
5.802424	593.126967	6.363533
5.842684	588.748683	6.368538
5.848136	589.800668	6.373542
6.064631	593.941416	6.378547
6.204625	589.008074	6.383552
5.913846	593.937130	6.388557
5.835903	573.666439	6.393562
6.132044	569.009375	6.398566
5.939988	557.652928	6.403571
5.960312	557.589645	6.408576
5.234068	562.231639	6.413581
5.813297	571.052634	6.418586
5.925779	583.509172	6.423590
6.009440	590.089735	6.428595
5.719315	575.807161	6.433600
5.570520	586.171740	6.438605
5.979185	590.347959	6.443610
5.995075	594.126257	6.448614
5.994021	592.249794	6.453619
6.087971	581.001869	6.458624
5.842149	575.033230	6.463629
5.784541	569.661364	6.468634
5.896680	564.417292	6.473638
5.533680	554.748984	6.478643
5.990054	568.789847	6.483648
5.611999	572.661394	6.488653
6.005788	580.197825	6.493658
6.004027	584.507719	6.498662
5.584430	557.343479	6.503667
6.055782	570.746624	6.508672
5.782688	569.978877	6.513677
6.149289	557.975790	6.518682
5.822220	556.196928	6.523686
5.600068	554.961337	6.528691
5.897629	549.431602	6.533696
5.725052	558.747290	6.538701
5.974560	560.815421	6.543706
6.041739	564.558973	6.548710
5.815743	571.063912	6.553715
5.942408	560.113306	6.558720
5.595335	565.630277	6.563725
5.804946	552.709113	6.568730
5.700655	564.048273	6.573734
5.797592	580.560364	6.578739
6.021089	593.589760	6.583744
5.735276	597.387626	6.588749
5.969547	599.847245	6.593754
5.941463	586.822537	6.598758
5.526703	568.951047	6.603763
5.833714	571.158256	6.608768
5.707318	590.736714	6.613773
5.756746	583.336020	6.618778
5.989239	592.324755	6.623782
6.074015	585.707373	6.628787
6.217783	591.997167	6.633792
5.616375	583.622617	6.638797
5.743573	576.659774	6.643802
5.742123	579.537711	6.648806
5.673688	596.964446	6.653811
5.982615	587.958826	6.658816
5.757684	605.316761	6.663821
5.782359	585.234100	6.668826
5.830349	590.240659	6.673830
5.768321	600.836372	6.678835
5.837664	589.152643	6.683840
5.552835	600.730906	6.688845
5.915462	595.389104	6.693850
5.903393	588.785191	6.698854
5.635289	602.832380	6.703859
5.816790	596.701209	6.708864
5.602016	599.629472	6.713869
5.771737	596.643302	6.718874
6.088861	597.274453	6.723878
6.077055	598.583669	6.728883
6.093737	599.242074	6.733888
5.908402	595.603480	6.738893
6.014807	594.254673	6.743898
5.734854	592.051418	6.748902
5.774082	598.186247	6.753907
6.343030	592.219442	6.758912
6.044558	599.214749	6.763917
6.042390	581.764922	6.768922
5.591453	565.964992	6.773926
5.555952	575.685234	6.778931
5.723308	580.756880	6.783936
5.938065	588.809209	6.788941
5.912695	599.162041	6.793946
5.932583	599.439244	6.798950
6.037296	597.456464	6.803955
6.206265	583.144041	6.808960
5.458441	569.016988	6.813965
5.626770	568.140033	6.818970
6.095135	589.267404	6.823974
5.715179	588.026366	6.828979
5.727733	591.744237	6.833984
5.617759	598.588150	6.838989
5.851090	588.726352	6.843994
5.909867	594.010758	6.848998
6.035128	598.613789	6.854003
5.684973	599.528305	6.859008
5.750967	603.147736	6.864013
5.887855	602.920699	6.869018
6.227156	597.758983	6.874022
5.646018	602.464580	6.879027
5.852780	593.541589	6.884032
5.659610	596.980544	6.889037
5.610550	597.196739	6.894042
5.839483	594.317591	6.899046
5.809011	604.730080	6.904051
6.016775	589.494578	6.909056
5.785107	596.601765	6.914061
6.165649	589.688729	6.919066
6.034162	594.284938	6.924070
5.720580	595.086833	6.929075
6.264413	590.092737	6.934080
6.025717	582.276199	6.939085
5.712676	567.874682	6.944090
5.791417	568.482946	6.949094
5.378623	570.968402	6.954099
5.962009	589.472620	6.959104
5.779743	598.766255	6.964109
5.839077	592.338189	6.969114
5.698310	598.848563	6.974118
5.664933	593.204689	6.979123
5.513755	591.195607	6.984128
5.818979	595.791926	6.989133
5.807669	593.791258	6.994138
5.651069	593.285430	6.999142
5.749092	604.635323	7.004147
5.770580	596.413772	7.009152
5.597984	602.243461	7.014157
5.504425	598.921203	7.019162
5.718808	605.620632	7.024166
5.899468	595.970023	7.029171
6.091434	598.916975	7.034176
5.789546	596.704327	7.039181
6.069555	593.154445	7.044186
6.340003	597.379602	7.049190
6.151845	598.659015	7.054195
6.269343	592.007794	7.059200
6.087913	598.116209	7.064205
6.002528	595.514273	7.069210
6.041513	596.264103	7.074214
5.883693	588.655192	7.079219
6.019288	580.477903	7.084224
5.460226	575.069679	7.089229
5.991759	583.596845	7.094234
6.001537	584.167391	7.099238
5.700115	581.249372	7.104243
5.615470	579.124289	7.109248
5.724924	600.323539	7.114253
5.881025	597.836529	7.119258
5.984423	600.084167	7.124262
5.905230	600.245360	7.129267
5.945341	602.805410	7.134272
5.801649	601.921115	7.139277
6.057810	594.229245	7.144282
6.123583	577.726460	7.149286
5.664143	570.973046	7.154291
5.936255	572.036130	7.159296
5.667811	566.779100	7.164301
5.628323	568.475344	7.169306
5.992917	572.300288	7.174310
5.904951	579.361964	7.179315
6.074612	571.033402	7.184320
5.746800	566.224694	7.189325
6.072709	564.732781	7.194330
6.043336	561.971795	7.199334
5.637333	562.477787	7.204339
5.929986	560.867846	7.209344
6.194701	566.106893	7.214349
5.885505	561.221101	7.219354
6.290941	563.898652	7.224358
5.742584	563.686808	7.229363
5.912014	565.297148	7.234368
5.926806	564.664073	7.239373
6.155022	558.077811	7.244378
6.109711	559.327844	7.249382
5.568071	562.043814	7.254387
5.935535	555.446138	7.259392
5.883153	566.449712	7.264397
5.927090	560.336598	7.269402
6.116744	565.507362	7.274406
5.421250	565.752846	7.279411
5.871550	560.228601	7.284416
5.737790	559.319378	7.289421
6.162979	567.868486	7.294426
5.857839	555.559652	7.299430
5.792697	566.077710	7.304435
6.075406	566.429205	7.309440
5.723506	559.760212	7.314445
5.722946	565.766043	7.319450
5.799863	565.941446	7.324454
5.735859	568.023406	7.329459
6.092295	561.832496	7.334464
6.026546	564.001179	7.339469
6.057360	561.148331	7.344474
5.805248	566.947364	7.349478
5.715010	570.098912	7.354483
5.873295	567.179961	7.359488
5.780650	570.462745	7.364493
5.804194	569.034911	7.369498
5.526037	567.627434	7.374502
5.679461	566.000093	7.379507
5.655354	563.891037	7.384512
5.837278	575.019611	7.389517
5.841305	560.330368	7.394522
5.886955	568.882726	7.399526
5.522586	566.082487	7.404531
5.646770	567.840826	7.409536
5.677852	573.852867	7.414541
5.883322	559.854310	7.419546
6.007908	565.800345	7.424550
5.733469	568.667439	7.429555
6.195580	567.624420	7.434560
5.672473	568.472257	7.439565
6.077663	566.087275	7.444570
6.109434	570.095798	7.449574
5.812931	568.674388	7.454579
6.052589	558.177704	7.459584
5.813621	566.117284	7.464589
6.187914	566.435063	7.469594
5.971612	564.964062	7.474598
5.700171	561.691395	7.479603
5.730493	565.338038	7.484608
5.948724	559.496218	7.489613
5.855599	568.301458	7.494618
5.747986	561.657530	7.499622
5.455108	564.973863	7.504627
5.785240	559.959710	7.509632
5.679543	566.716071	7.514637
5.930787	564.235216	7.519642
6.121423	562.805171	7.524646
5.511509	566.679391	7.529651
5.805130	557.527923	7.534656
5.795566	567.267743	7.539661
6.009972	564.024150	7.544666
5.961899	569.457471	7.549670
5.849544	567.762445	7.554675
6.077517	560.585384	7.559680
5.902007	568.911112	7.564685
5.970093	560.090631	7.569690
5.753088	558.088309	7.574694
5.612132	563.926756	7.579699
6.010800	549.048838	7.584704
6.126207	571.139041	7.589709
5.892331	562.093861	7.594714
6.014594	561.010026	7.599718
6.007600	566.854116	7.604723
5.877684	566.833078	7.609728
6.027538	571.573917	7.614733
6.087410	564.330558	7.619738
6.171705	562.597444	7.624742
5.958951	557.989524	7.629747
5.753868	551.029616	7.634752
5.778409	550.329410	7.639757
5.495252	564.808866	7.644762
5.856230	570.275295	7.649766
5.696981	575.381287	7.654771
6.143203	566.126595	7.659776
6.008460	566.706469	7.664781
5.998774	566.082578	7.669786
5.964211	550.407703	7.674790
5.116665	546.091387	7.679795
5.951034	550.958640	7.684800
5.622341	560.592441	7.689805
5.690776	573.298994	7.694810
5.958423	563.867258	7.699814
5.987263	564.963717	7.704819
5.975572	564.500398	7.709824
5.765379	568.160029	7.714829
5.806656	556.166017	7.719834
5.963895	559.306185	7.724838
5.711446	561.141493	7.729843
5.880404	557.393327	7.734848
5.726854	565.371650	7.739853
5.812764	569.502835	7.744858
5.519308	569.539662	7.749862
5.638940	562.211814	7.754867
5.714148	567.214450	7.759872
5.697493	563.404071	7.764877
5.670163	568.096496	7.769882
5.890563	568.876078	7.774886
5.421932	566.140070	7.779891
5.646008	561.989280	7.784896
5.867413	568.919209	7.789901
5.914223	563.246477	7.794906
5.811051	556.908088	7.799910
5.422826	565.959334	7.804915
5.858504	573.319507	7.809920
6.348197	587.064976	7.814925
5.907619	577.304120	7.819930
5.858946	572.778944	7.824934
5.782031	569.490444	7.829939
6.203272	567.079320	7.834944
6.065979	572.162139	7.839949
6.249869	567.207326	7.844954
5.809790	569.157574	7.849958
5.896172	571.293962	7.854963
5.809963	567.063911	7.859968
5.726403	572.883187	7.864973
5.803586	564.983567	7.869978
6.172493	565.150681	7.874982
5.966403	569.625834	7.879987
5.994652	568.102498	7.884992
6.247458	573.165123	7.889997
5.831881	565.800192	7.895002
5.973880	568.057418	7.900006
5.674275	569.418826	7.905011
6.160097	566.972341	7.910016
5.982672	571.487347	7.915021
5.815046	575.220841	7.920026
6.173047	563.782187	7.925030
5.610772	565.799042	7.930035
6.006460	557.353334	7.935040
5.914287	552.569353	7.940045
5.387475	545.926961	7.945050
6.032307	546.129294	7.950054
6.012719	562.426615	7.955059
6.137268	556.280420	7.960064
5.417156	552.911744	7.965069
5.678050	558.184574	7.970074
5.894979	560.707839	7.975078
5.903529	568.253787	7.980083
5.969521	563.884668	7.985088
5.765489	564.283608	7.990093
5.731269	557.997739	7.995098
6.177547	564.960288	8.000102
5.649359	572.228259	8.005107
6.139352	561.224002	8.010112
5.888967	549.835715	8.015130
6.049101	535.861415	8.020147
5.940391	530.679459	8.025165
6.024617	542.123848	8.030182
5.407860	535.760355	8.035200
5.568026	549.795735	8.040218
5.949425	560.857686	8.045235
6.065177	553.868594	8.050253
6.068160	556.090465	8.055270
5.938664	548.285745	8.060288
5.657787	546.342702	8.065306
5.539265	555.072043	8.070323
5.875221	554.957043	8.075341
5.924276	565.489817	8.080358
6.327745	561.605623	8.085376
5.758535	575.663777	8.090394
5.648950	571.488578	8.095411
6.057008	574.998403	8.100429
5.747999	578.056532	8.105446
6.149810	570.625603	8.110464
5.959302	571.410716	8.115482
5.701232	565.199811	8.120499
5.605144	572.139544	8.125517
5.573180	573.109414	8.130534
5.886861	569.123952	8.135552
5.763819	569.714836	8.140570
5.895244	572.457333	8.145587
6.144656	572.748566	8.150605
5.890103	572.049109	8.155622
6.239414	570.831971	8.160640
6.300926	573.330354	8.165658
6.077624	571.192747	8.170675
6.302547	568.097318	8.175693
5.970907	567.820047	8.180710
6.199446	565.940080	8.185728
6.240843	571.814794	8.190746
5.954663	574.398505	8.195763
6.035324	571.157092	8.200781
5.740300	575.344128	8.205798
6.076975	567.764549	8.210816
5.723617	568.830548	8.215834
5.454061	573.646985	8.220851
5.828662	567.588582	8.225869
6.074815	574.091947	8.230886
6.213112	570.885870	8.235904
6.040256	567.880716	8.240922
6.131742	565.456552	8.245939
6.307050	566.114559	8.250957
6.166610	571.065511	8.255974
6.310095	570.521389	8.260992
6.012745	571.854867	8.266010
6.067139	570.789706	8.271027
6.290067	570.396985	8.276045
6.058806	576.174734	8.281062
6.125317	568.866843	8.286080
6.339041	570.622746	8.291098
5.964397	575.562286	8.296115
6.512616	563.750323	8.301133
5.935510	567.452015	8.306150
6.095811	580.006594	8.311168
6.394581	569.281532	8.316186
6.066835	569.163448	8.321203
6.385407	567.332544	8.326221
5.909392	564.532107	8.331238
6.075348	569.156357	8.336256
6.072515	577.640192	8.341274
6.077070	575.886874	8.346291
6.057760	565.655596	8.351309
5.762084	572.104398	8.356326
5.883957	572.102401	8.361344
6.017571	587.468698	8.366362
5.905540	602.942020	8.371379
6.019299	603.755094	8.376397
5.903691	603.603850	8.381414
5.929586	609.372492	8.386432
6.301871	602.678673	8.391450
6.089674	606.672683	8.396467
6.173001	602.262001	8.401485
6.189369	615.450246	8.406502
6.300235	604.706277	8.411520
6.398662	616.314500	8.416538
6.271022	613.351257	8.421555
6.616460	597.596920	8.426573
6.592713	617.681321	8.431590
6.275602	610.057628	8.436608
6.239488	603.924316	8.441626
6.206425	610.065689	8.446643
6.080288	614.390310	8.451661
6.370846	603.990972	8.456678
6.351297	607.511773	8.461696
6.485543	606.936898	8.466714
6.139593	608.892166	8.471731
6.278151	604.653035	8.476749
6.597132	609.536585	8.481766
6.344895	604.689767	8.486784
6.319963	604.570357	8.491802
5.973912	607.955470	8.496819
6.509686	601.290089	8.501837
6.497115	612.412392	8.506854
6.371537	616.206640	8.511872
6.309427	600.998298	8.516890
6.121613	602.801798	8.521907
6.576640	608.480484	8.526925
6.372141	607.187735	8.531942
6.358132	610.286386	8.536960
6.494597	600.291282	8.541978
6.459046	602.868336	8.546995
6.315293	607.739145	8.552013
6.478937	616.185592	8.557030
6.416327	608.111515	8.562048
6.569578	610.624239	8.567066
6.372161	611.991957	8.572083
6.406318	600.139899	8.577101
6.188221	609.885301	8.582119
6.200363	611.302565	8.587136
6.317496	604.452583	8.592154
6.211117	605.941831	8.597171
6.408176	625.933581	8.602189
6.613580	629.136446	8.607207
6.452791	635.267485	8.612224
6.771994	628.018308	8.617242
6.332830	623.265031	8.622259
6.504087	612.206745	8.627277
6.544698	621.184953	8.632295
6.346503	620.223421	8.637312
6.683548	627.390848	8.642330
6.599223	626.072687	8.647347
6.249336	604.658848	8.652365
6.504749	619.134593	8.657383
6.545724	630.749191	8.662400
6.617391	632.527443	8.667418
6.760051	636.739061	8.672435
6.599800	625.157350	8.677453
6.400251	624.015739	8.682471
6.444993	630.879229	8.687488
6.597644	632.070486	8.692506
6.592428	635.236185	8.697523
6.529965	631.403145	8.702541
6.768340	635.346174	8.707559
6.274292	648.069392	8.712576
6.614793	638.840035	8.717594
6.533402	640.410182	8.722611
6.784285	639.110919	8.727629
6.696186	638.728362	8.732647
6.573886	636.919276	8.737664
6.819255	631.859351	8.742682
6.671274	641.221926	8.747699
6.560615	637.716923	8.752717
6.504760	629.609829	8.757735
6.503312	631.530888	8.762752
6.770325	628.430249	8.767770
6.517371	637.742886	8.772787
6.607552	648.454130	8.777805
6.876490	639.886187	8.782823
6.568678	629.012723	8.787840
6.851306	637.325313	8.792858
6.597834	645.189706	8.797875
6.659464	636.668690	8.802893
6.324452	636.079397	8.807911
6.199664	644.736997	8.812928
6.638702	640.526835	8.817946
6.229999	637.127874	8.822963
6.374137	640.694801	8.827981
6.646222	643.938593	8.832999
6.661251	651.822304	8.838016
6.817129	657.051361	8.843034
6.881400	658.238358	8.848051
6.722442	649.797560	8.853069
7.021927	637.353147	8.858087
6.719137	634.173248	8.863104
6.772007	635.416852	8.868122
6.820087	641.049950	8.873139
6.515616	641.375227	8.878157
6.676554	648.183266	8.883175
6.482777	674.324853	8.888192
6.708336	667.714354	8.893210
6.631087	666.197786	8.898227
6.772882	670.126897	8.903245
6.999374	660.827827	8.908263
6.764494	675.275368	8.913280
7.158207	668.640568	8.918298
7.287838	670.913527	8.923315
7.500489	656.442656	8.928333
6.977624	641.086174	8.933351
6.821060	642.728215	8.938368
7.246620	636.623555	8.943386
7.084323	639.618428	8.948403
6.999955	640.277314	8.953421
7.001666	636.137602	8.958439
6.794293	637.923086	8.963456
6.963053	631.604273	8.968474
6.806499	632.274719	8.973491
6.831925	633.971264	8.978509
7.036538	635.503894	8.983527
6.912317	629.908751	8.988544
6.832779	639.511156	8.993562
7.056807	645.106066	8.998579
7.070248	644.236647	9.003597
6.828460	645.237329	9.008615
6.811240	644.592657	9.013632
6.994285	640.543775	9.018650
6.784341	643.992968	9.023667
7.091450	630.517048	9.028685
6.982057	632.108759	9.033703
6.579275	640.462411	9.038720
6.681969	632.852650	9.043738
6.946189	640.999010	9.048755
6.766291	644.836510	9.053773
6.895804	647.924789	9.058791
6.830209	655.850590	9.063808
6.932989	666.923912	9.068826
7.360364	669.865240	9.073843
6.813326	673.919043	9.078861
7.062524	675.173839	9.083879
6.794630	678.425561	9.088896
7.182083	666.290161	9.093914
7.171663	671.283391	9.098931
6.985958	675.948188	9.103949
7.245638	668.017551	9.108967
7.024455	673.189766	9.113984
6.965241	669.853786	9.119002
7.192424	672.580642	9.124019
6.931479	677.420093	9.129037
7.128976	673.792799	9.134055
7.073489	666.403298	9.139072
7.404811	669.488477	9.144090
7.285754	671.056204	9.149107
7.006440	668.015709	9.154125
7.863615	655.515154	9.159143
7.330555	649.865268	9.164160
7.221837	632.259250	9.169178
7.283154	632.502305	9.174195
6.921008	638.270649	9.179213
7.118086	631.451510	9.184231
6.887847	633.767125	9.189248
7.143501	626.195815	9.194266
7.169047	639.189265	9.199283
7.199528	650.761524	9.204301
7.181246	637.377665	9.209319
7.060227	647.656588	9.214336
7.291731	649.256416	9.219354
7.555296	655.208540	9.224371
7.062801	641.025697	9.229389
7.035419	636.328632	9.234407
6.717797	648.607703	9.239424
7.009580	652.295845	9.244442
7.222637	660.802634	9.249459
7.038129	664.928680	9.254477
7.127836	656.909666	9.259495
7.059863	663.018260	9.264512
7.771531	659.272761	9.269530
7.523525	657.577789	9.274547
7.164256	666.957256	9.279565
7.670796	657.402380	9.284583
7.257180	659.530660	9.289600
7.350719	661.649368	9.294618
7.173611	662.215351	9.299635
7.275052	663.838292	9.304653
7.463532	660.482557	9.309671
7.305190	667.687153	9.314688
7.038504	668.470712	9.319706
7.339175	671.446407	9.324723
7.283271	677.123113	9.329741
7.455564	666.090994	9.334759
7.552901	669.469233	9.339776
7.388691	665.477452	9.344794
7.260546	665.190103	9.349811
7.054320	670.975551	9.354829
7.470457	661.931675	9.359847
7.265115	659.362762	9.364864
7.092028	670.416416	9.369882
7.389281	667.093846	9.374899
7.149730	670.762501	9.379917
7.402749	662.083803	9.384935
7.229152	673.272574	9.389952
7.323038	672.313065	9.394970
7.231780	660.137262	9.399987
7.032591	674.709593	9.405005
7.203325	677.198567	9.410023
7.280575	691.560976	9.415040
7.740461	688.607905	9.420058
7.695025	686.714041	9.425075
7.408611	692.836772	9.430093
7.620107	697.333055	9.435111
7.632359	696.033539	9.440128
7.829887	694.593115	9.445146
7.423084	687.673958	9.450163
7.359718	684.887448	9.455181
7.614612	685.485828	9.460199
7.761955	685.792194	9.465216
7.640445	687.567009	9.470234
7.769360	663.823939	9.475251
7.484408	679.210033	9.480269
7.299256	666.138409	9.485287
7.519867	668.619911	9.490304
7.338499	674.365026	9.495322
7.813074	683.272198	9.500339
7.510496	682.001982	9.505357
7.747635	681.123864	9.510375
7.822506	686.019121	9.515392
7.257480	674.918153	9.520410
7.819790	673.008691	9.525427
7.622291	667.165447	9.530445
7.473400	662.601480	9.535463
7.447914	676.393127	9.540480
7.589087	687.962045	9.545498
7.935156	692.619102	9.550515
7.688366	695.457514	9.555533
7.692156	677.326546	9.560551
7.688833	669.973285	9.565568
7.434951	676.863410	9.570586
7.622926	686.707752	9.575603
7.319317	686.362061	9.580621
7.596319	687.577610	9.585639
8.027165	686.538289	9.590656
7.769083	692.457915	9.595674
7.770182	690.839400	9.600691
7.817444	691.334769	9.605709
7.818968	691.622369	9.610727
7.885315	685.838179	9.615744
7.335931	692.487496	9.620762
7.482107	689.460788	9.625779
7.546376	691.608361	9.630797
7.644707	691.566958	9.635815
7.365390	687.255275	9.640832
7.348397	694.875428	9.645850
7.528518	687.604768	9.650867
7.615934	689.753231	9.655885
7.472254	694.510282	9.660903
7.839139	704.293909	9.665920
7.751965	714.625141	9.670938
7.937240	723.140896	9.675955
8.044459	726.850169	9.680973
7.876247	712.662379	9.685991
8.014782	696.344010	9.691008
8.006337	691.011546	9.696026
8.007897	681.360363	9.701043
8.064058	690.372648	9.706061
7.874432	684.715484	9.711079
7.939353	687.469211	9.716096
7.810244	693.744231	9.721114
7.980352	676.456932	9.726131
7.796680	686.330925	9.731149
7.750086	687.147722	9.736167
8.068591	688.930380	9.741184
7.669219	691.157481	9.746202
7.744031	682.113029	9.751219
7.561258	690.305087	9.756237
7.716485	700.984732	9.761255
8.157150	710.577022	9.766272
7.742543	724.726042	9.771290
8.122946	721.681014	9.776307
8.367741	727.697688	9.781325
8.026604	703.543443	9.786343
8.030042	689.771713	9.791360
7.983966	687.572068	9.796378
8.337564	691.344073	9.801395
8.065203	691.797097	9.806413
8.052519	693.525154	9.811431
8.125416	691.527449	9.816448
7.821151	690.261449	9.821466
8.240072	679.232968	9.826483
8.215704	687.504693	9.831501
7.740629	677.533642	9.836519
7.960868	672.608960	9.841536
7.896613	688.069142	9.846554
8.257657	686.618177	9.851571
8.132288	690.732074	9.856589
7.934120	685.901867	9.861607
8.186470	679.195200	9.866624
7.925500	686.939209	9.871642
8.064760	687.058341	9.876659
8.040574	692.822315	9.881677
7.961983	687.597525	9.886695
8.088752	705.367292	9.891712
8.097380	714.022128	9.896730
8.583450	713.806685	9.901747
8.147387	704.666115	9.906765
8.076605	694.942656	9.911783
8.117415	688.954044	9.916800
7.763512	703.591782	9.921818
8.355285	716.985997	9.926835
8.388166	722.692504	9.931853
8.463766	707.671872	9.936871
8.339625	695.896737	9.941888
8.173018	699.361599	9.946906
8.183148	686.609963	9.951923
8.052662	695.290187	9.956941
8.024681	690.861692	9.961959
8.430394	708.773451	9.966976
8.197781	708.305380	9.971994
8.393950	707.330114	9.977011
8.170085	705.724046	9.982029
8.011653	710.194585	9.987047
8.359890	709.655922	9.992064
8.180600	720.540963	9.997082
8.487142	716.536963	10.002099
8.083349	722.272866	10.007117
8.396773	731.754356	10.012135
8.591297	719.561891	10.017152
8.051263	721.605607	10.022170
8.372517	727.515138	10.027187
8.466753	723.156943	10.032205
8.381860	725.248909	10.037223
8.638333	722.817281	10.042240
8.166629	710.924894	10.047258
8.455914	700.546961	10.052275
8.300879	710.711880	10.057293
8.446136	706.527120	10.062311
8.633047	687.696171	10.067328
8.166034	699.942149	10.072346
7.920440	697.143295	10.077363
8.298240	711.434302	10.082381
8.297775	728.764955	10.087399
8.304256	724.092963	10.092416
8.313001	727.469743	10.097434
8.467685	725.262439	10.102451
8.427203	723.834260	10.107469
7.983296	717.652687	10.112487
8.367218	722.348365	10.117504
8.182187	729.178296	10.122522
8.656795	719.226725	10.127539
8.557859	719.639222	10.132557
8.286410	732.738225	10.137575
8.385153	719.637656	10.142592
8.132031	723.461318	10.147610
8.597171	725.622826	10.152627
8.460016	716.986660	10.157645
8.286389	720.248370	10.162663
8.260298	722.840805	10.167680
8.547061	746.254669	10.172698
8.636934	752.971378	10.177715
8.645222	744.285523	10.182733
8.323344	755.994155	10.187751
8.832501	749.813407	10.192768
8.744849	757.360257	10.197786
8.654912	737.760568	10.202803
8.640269	728.427375	10.207821
8.388145	736.159708	10.212839
8.632566	733.177743	10.217856
8.657592	752.378111	10.222874
8.646524	755.483390	10.227891
9.122262	739.677218	10.232909
8.356119	742.828396	10.237927
8.708123	724.464920	10.242944
8.635023	725.587665	10.247962
8.244851	729.495829	10.252979
8.601934	745.206360	10.257997
8.852606	756.347378	10.263015
8.575309	756.625246	10.268032
8.730035	749.891410	10.273050
8.464119	753.013299	10.278067
8.702133	753.042462	10.283085
8.759057	753.246485	10.288103
9.035622	742.056502	10.293120
8.623551	750.765668	10.298138
8.636221	749.151529	10.303155
8.692290	744.913028	10.308173
8.867366	745.606906	10.313191
8.966680	751.729959	10.318208
8.567044	758.179320	10.323226
8.981183	753.123692	10.328243
9.370740	751.199522	10.333261
9.276216	737.273114	10.338279
8.329232	731.929914	10.343296
8.530869	730.960039	10.348314
8.667918	742.082855	10.353331
8.773459	742.915800	10.358349
8.715985	758.303672	10.363367
8.645151	748.340044	10.368384
9.038999	744.694787	10.373402
8.847882	751.817059	10.378419
8.952302	746.696189	10.383437
8.480969	755.284863	10.388455
8.875470	751.286760	10.393472
8.960998	748.007893	10.398490
8.691518	751.745298	10.403507
9.221906	753.571221	10.408525
9.007594	752.474956	10.413543
9.232271	743.699337	10.418560
9.016829	757.705571	10.423578
9.230854	747.532972	10.428595
9.223196	747.384323	10.433613
8.604977	757.568492	10.438631
8.983021	756.825691	10.443648
8.928231	750.929259	10.448666
8.927382	749.711825	10.453683
8.919685	746.115737	10.458701
9.089303	748.703327	10.463719
8.886828	746.889788	10.468736
8.955739	753.163930	10.473754
8.633392	753.785066	10.478771
9.118391	743.714836	10.483789
9.077771	752.058968	10.488807
9.457353	752.176100	10.493824
9.576462	743.929350	10.498842
9.044366	741.913714	10.503859
9.133841	740.943121	10.508877
9.227770	738.963973	10.513895
9.393907	743.000483	10.518912
9.253495	741.848283	10.523930
8.876617	731.031850	10.528947
9.269262	726.660460	10.533965
9.059449	733.414187	10.538983
9.124383	738.379606	10.544000
9.286179	733.052008	10.549018
9.001462	740.107101	10.554035
9.448416	729.332983	10.559053
9.324460	726.204156	10.564071
9.230062	718.146309	10.569088
9.296006	711.061070	10.574106
9.365190	715.645879	10.579123
9.218782	710.187050	10.584141
8.902371	719.986987	10.589159
8.840716	713.971240	10.594176
9.416313	726.054438	10.599194
9.189786	739.001528	10.604211
9.452005	738.706622	10.609229
8.994073	733.683993	10.614247
9.064652	740.938507	10.619264
9.135373	748.933904	10.624282
9.034590	745.766986	10.629299
9.314543	740.284001	10.634317
9.180291	740.957844	10.639335
9.103979	749.179152	10.644352
8.922118	746.739793	10.649370
8.933837	752.625396	10.654387
9.213365	743.959979	10.659405
8.825966	754.824389	10.664423
8.879908	762.415902	10.669440
9.329609	775.856920	10.674458
9.563426	780.973119	10.679475
9.499820	776.637897	10.684493
9.305091	784.448933	10.689511
9.579170	781.489606	10.694528
9.523142	778.425895	10.699546
9.562307	772.696958	10.704563
9.540609	762.893678	10.709581
9.338807	762.929925	10.714599
9.428382	768.503445	10.719616
9.945822	764.125553	10.724634
9.322431	759.502733	10.729651
9.577891	748.087908	10.734669
9.419189	748.820127	10.739687
9.401898	754.021990	10.744704
9.437741	745.355587	10.749722
9.470665	748.445313	10.754739
9.379969	737.966111	10.759757
9.453222	756.792377	10.764775
9.607593	762.075654	10.769792
9.694743	757.934359	10.774810
9.688523	758.475985	10.779827
9.414535	745.130044	10.784845
9.464543	744.973028	10.789863
9.259298	747.993142	10.794880
9.698124	753.043104	10.799898
9.668864	773.190624	10.804915
9.813329	766.381712	10.809933
9.610450	758.482744	10.814951
9.581004	745.433693	10.819968
9.740713	753.151773	10.824986
9.781403	746.069125	10.830003
9.809352	743.624551	10.835021
9.538536	740.137384	10.840039
9.592693	744.853423	10.845056
9.522988	732.859809	10.850074
9.501065	745.398637	10.855091
9.525087	752.729366	10.860109
9.800578	774.095251	10.865127
9.700115	769.167347	10.870144
9.921906	779.751777	10.875162
9.588666	770.091807	10.880179
9.610643	769.998484	10.885197
9.627255	772.296865	10.890215
9.658180	772.037895	10.895232
9.760718	770.088025	10.900250
9.805650	781.447370	10.905267
9.901454	775.671260	10.910285
9.741876	778.688150	10.915303
9.806694	779.686886	10.920320
9.924090	768.297269	10.925338
9.796761	773.785455	10.930355
9.946198	770.922355	10.935373
9.963243	776.389391	10.940391
9.620683	773.836487	10.945408
10.115970	777.834645	10.950426
9.980813	768.399736	10.955443
9.590436	746.787692	10.960461
9.878118	766.581951	10.965479
9.938554	776.132525	10.970496
9.767978	768.710066	10.975514
9.808560	782.197970	10.980531
9.964023	771.479176	10.985549
10.023888	776.156093	10.990567
9.571508	778.979353	10.995584
9.709775	775.822843	11.000602
9.490711	789.896632	11.005619
9.863453	780.610279	11.010637
9.602022	778.845079	11.015655
9.846053	787.936148	11.020672
10.031723	776.406880	11.025690
9.710790	780.940566	11.030707
9.555821	780.800168	11.035725
9.903043	778.613728	11.040743
9.963658	792.994732	11.045760
10.328608	796.790473	11.050778
10.005926	791.857234	11.055795
10.160392	785.200980	11.060813
10.310999	774.188910	11.065831
9.848748	781.127757	11.070848
9.947580	767.574401	11.075866
10.175917	771.429369	11.080883
9.821338	774.012430	11.085901
10.185223	781.016438	11.090919
10.215193	790.814178	11.095936
10.445769	786.493229	11.100954
10.526165	779.194160	11.105971
10.212875	774.058595	11.110989
10.341478	770.878490	11.116007
10.314205	776.217439	11.121024
10.394130	764.848201	11.126042
9.991120	778.637889	11.131059
9.933324	775.063081	11.136077
10.197517	771.460546	11.141095
10.025835	770.497764	11.146112
10.359914	767.820221	11.151130
10.274504	769.099330	11.156147
9.477519	770.828533	11.161165
10.274773	774.205852	11.166183
10.039497	778.087198	11.171200
10.461160	781.405065	11.176218
10.333169	777.693069	11.181235
10.187649	767.698490	11.186253
10.330281	777.378359	11.191271
10.457888	784.316380	11.196288
10.444176	776.761256	11.201306
10.385230	779.712272	11.206323
10.330963	777.167927	11.211341
10.507392	773.265768	11.216359
10.157349	780.135249	11.221376
10.201746	773.492896	11.226394
10.087055	776.732261	11.231411
10.058382	779.410169	11.236429
10.789363	788.189516	11.241447
10.582660	806.169333	11.246464
10.448669	780.300834	11.251482
9.998424	782.439526	11.256499
10.124557	786.189773	11.261517
10.284592	791.183161	11.266535
10.320416	798.488337	11.271552
10.710570	796.938058	11.276570
10.671447	792.172815	11.281587
10.583803	800.025574	11.286605
10.636010	791.116290	11.291623
10.428380	796.474088	11.296640
10.623399	792.780251	11.301658
10.486757	799.944310	11.306675
10.695931	800.949851	11.311693
10.688686	790.611118	11.316711
10.137817	785.466860	11.321728
10.426848	788.869285	11.326746
10.595685	789.453969	11.331763
10.447448	788.996332	11.336781
10.435189	798.052684	11.341799
10.294233	792.939755	11.346816
10.483678	802.793375	11.351834
10.583164	798.454367	11.356851
10.296478	804.981497	11.361869
10.640003	791.181708	11.366887
10.733173	801.832330	11.371904
10.666357	800.447085	11.376922
10.518096	800.345338	11.381939
10.308319	798.433007	11.386957
10.838922	803.447711	11.391975
10.594302	800.760874	11.396992
10.819522	802.963303	11.402010
10.629091	804.897961	11.407027
10.536543	801.369057	11.412045
10.969777	805.331830	11.417063
10.743532	807.644052	11.422080
10.800826	792.303552	11.427098
10.620009	806.454482	11.432115
10.476657	811.668577	11.437133
10.608061	804.244127	11.442151
10.472397	813.433514	11.447168
10.590525	827.718418	11.452186
10.665464	821.672138	11.457203
10.905815	833.789280	11.462221
11.028279	831.940428	11.467239
10.764877	837.304719	11.472256
11.083792	842.301341	11.477274
10.713028	820.301713	11.482291
10.862527	824.679565	11.487309
11.085403	832.984440	11.492327
10.533292	838.010729	11.497344
11.046203	815.947456	11.502362
11.148873	827.509075	11.507379
10.941089	826.083393	11.512397
11.496418	808.305410	11.517415
11.036056	804.724424	11.522432
10.868568	794.853144	11.527450
11.067566	790.553169	11.532467
11.180908	789.452250	11.537485
10.978616	787.357194	11.542503
10.975332	793.017750	11.547520
10.759692	786.595999	11.552538
11.052295	784.270579	11.557555
10.872499	791.772470	11.562573
11.024249	789.232589	11.567591
10.723622	789.779661	11.572608
10.777916	797.159333	11.577626
11.153703	809.726840	11.582643
10.950406	823.184300	11.587661
11.026675	820.223864	11.592679
10.920256	824.319700	11.597696
11.306348	819.998973	11.602714
11.456234	822.835106	11.607731
11.106764	813.208898	11.612749
11.158139	800.778668	11.617767
10.971270	809.432466	11.622784
11.030373	815.264186	11.627802
11.379591	821.536820	11.632819
11.218272	821.131740	11.637837
11.430134	812.007435	11.642855
11.248595	802.063283	11.647872
11.216495	808.020333	11.652890
11.366752	788.612290	11.657907
11.027898	791.917909	11.662925
11.427177	783.559395	11.667943
11.094849	790.368865	11.672960
10.940109	778.401107	11.677978
11.207714	795.775236	11.682995
11.221276	811.622241	11.688013
11.645278	810.443896	11.693031
11.266661	803.212161	11.698048
11.047981	805.222753	11.703066
11.555222	812.477826	11.708083
11.466888	824.244289	11.713101
11.647621	807.444430	11.718119
11.367009	793.607838	11.723136
11.075681	793.775437	11.728154
11.534631	788.109654	11.733171
11.199626	791.641789	11.738189
11.640331	793.533352	11.743207
11.348522	795.384801	11.748224
11.271628	786.311475	11.753242
11.456872	785.634060	11.758259
11.283611	807.786072	11.763277
11.497436	805.253232	11.768295
11.692608	810.257343	11.773312
11.204151	800.460466	11.778330
11.497474	791.305756	11.783347
11.594643	810.882419	11.788365
11.427344	809.653962	11.793383
11.812000	808.147110	11.798400
11.350243	800.938985	11.803418
11.465947	798.173981	11.808435
11.395092	803.863051	11.813453
11.484777	805.446617	11.818471
11.764917	820.730619	11.823488
11.611043	820.521933	11.828506
11.555207	818.123502	11.833523
11.488135	821.587657	11.838541
11.563212	809.912512	11.843559
11.736752	811.663680	11.848576
11.345918	817.840363	11.853594
11.637331	812.853854	11.858611
11.651451	818.608382	11.863629
11.657224	815.647810	11.868647
11.468716	816.262140	11.873664
11.175926	815.455229	11.878682
11.282819	817.748902	11.883699
11.313725	822.303470	11.888717
11.169598	811.153573	11.893735
11.367674	817.816174	11.898752
11.655399	833.722916	11.903770
12.356396	833.418736	11.908787
11.842434	832.928748	11.913805
11.967374	813.618562	11.918823
11.989857	809.890303	11.923840
11.695796	814.834487	11.928858
11.911995	807.749913	11.933875
11.667748	808.321507	11.938893
12.172216	815.318393	11.943911
12.396107	809.652156	11.948928
11.794272	818.269559	11.953946
12.093281	805.921543	11.958963
12.006771	806.634725	11.963981
11.823693	806.353714	11.968999
12.045402	805.906862	11.974016
11.923921	801.894978	11.979034
11.975114	800.898439	11.984051
11.692959	810.123105	11.989069
11.690371	804.845535	11.994087
11.813705	809.649740	11.999104
12.056520	818.354041	12.004122
12.089560	802.775432	12.009139
11.582243	806.567193	12.014157
11.875800	804.710091	12.019175
11.878545	814.626129	12.024192
11.566916	806.015260	12.029210
11.697688	805.607480	12.034227
11.800256	829.760202	12.039245
12.174721	826.477566	12.044263
12.153266	835.755924	12.049280
12.117692	841.236814	12.054298
12.408801	837.989238	12.059315
12.140999	834.393681	12.064333
12.355098	820.288542	12.069351
12.154013	814.130498	12.074368
11.814422	810.579510	12.079386
12.154250	807.805738	12.084403
12.208801	818.303326	12.089421
12.301824	819.611946	12.094439
12.562266	807.668719	12.099456
11.935582	814.400175	12.104474
12.103066	805.239917	12.109491
12.111292	807.807788	12.114509
12.104852	806.770794	12.119527
11.963661	815.723315	12.124544
11.886873	835.822097	12.129562
11.881031	832.285127	12.134579
12.052641	847.163525	12.139597
11.989365	837.862727	12.144615
12.011955	835.248562	12.149632
12.035105	846.452121	12.154650
12.097659	838.128076	12.159667
12.180501	843.383070	12.164685
12.136775	840.491710	12.169703
12.329434	838.145431	12.174720
12.412267	857.762714	12.179738
12.907848	844.429802	12.184755
12.528907	844.698125	12.189773
12.345116	841.990974	12.194791
12.187745	834.007270	12.199808
12.197853	834.999715	12.204826
12.456531	833.062957	12.209843
12.256047	829.820803	12.214861
12.201545	837.197250	12.219879
12.056502	850.392344	12.224896
11.998178	865.790700	12.229914
12.633191	864.071136	12.234931
12.692807	860.518203	12.239949
12.825025	859.196054	12.244967
13.008638	866.411832	12.249984
12.583114	863.288427	12.255002
12.622190	855.782394	12.260019
12.640922	833.823365	12.265037
12.549468	829.591946	12.270055
12.533655	827.451440	12.275072
12.938031	833.376380	12.280090
12.690840	821.506964	12.285107
12.602338	825.238828	12.290125
12.575114	831.459239	12.295143
12.930644	827.535283	12.300160
12.686930	833.037249	12.305178
12.898351	828.730483	12.310195
12.800480	832.625703	12.315213
12.452046	832.906691	12.320231
12.459012	826.542940	12.325248
12.765935	835.047275	12.330266
13.135684	822.014731	12.335283
12.786072	825.672120	12.340301
12.560670	833.402044	12.345319
12.875361	824.076856	12.350336
12.504220	832.934400	12.355354
12.937115	823.069980	12.360371
12.879429	828.256117	12.365389
12.865581	832.704324	12.370407
13.320222	827.196713	12.375424
12.908745	830.848206	12.380442
12.732906	832.034032	12.385459
12.975706	832.154918	12.390477
12.780002	836.017128	12.395495
13.030760	822.167715	12.400512
12.520065	835.217842	12.405530
13.003859	828.582625	12.410547
13.111003	821.251549	12.415565
12.685171	823.376755	12.420583
13.050628	823.543076	12.425600
12.448828	828.598455	12.430618
12.439258	823.694457	12.435635
12.830432	815.504976	12.440653
12.873762	834.076856	12.445671
13.112134	831.341139	12.450688
12.970548	840.571285	12.455706
12.816731	856.855873	12.460723
13.372406	859.606712	12.465741
13.179695	852.875246	12.470759
13.214876	833.415340	12.475776
13.174184	836.766473	12.480794
12.906175	834.120116	12.485811
13.167393	825.466741	12.490829
13.210284	831.310993	12.495847
13.198241	827.603800	12.500864
12.738235	838.143694	12.505882
13.223257	832.519638	12.510899
13.170886	832.202811	12.515917
12.947604	830.661197	12.520935
13.174731	822.006775	12.525952
13.366862	844.694370	12.530970
13.271683	844.829884	12.535987
12.830171	834.363434	12.541005
13.211932	841.075153	12.546023
13.339972	852.779827	12.551040
13.189738	862.359827	12.556058
13.297173	853.312629	12.561075
13.499430	851.411587	12.566093
13.640698	857.741504	12.571111
13.117422	830.226440	12.576128
13.293959	830.308301	12.581146
13.514933	839.266611	12.586163
13.690190	827.896895	12.591181
13.333234	824.825133	12.596199
13.412703	819.250126	12.601216
12.945625	822.968302	12.606234
13.259210	822.334985	12.611251
13.581280	813.630203	12.616269
13.301603	822.285204	12.621287
13.309578	827.147491	12.626304
13.418277	842.012287	12.631322
13.582887	853.149910	12.636339
13.726628	836.921865	12.641357
13.308341	840.047349	12.646375
13.482936	831.275643	12.651392
13.337876	835.246390	12.656410
13.452680	855.528028	12.661427
13.905138	846.636291	12.666445
13.071301	841.361319	12.671463
13.268522	845.496248	12.676480
13.332665	857.402834	12.681498
12.885904	856.482840	12.686515
13.571356	857.420544	12.691533
13.441293	860.032187	12.696551
13.532819	860.102929	12.701568
13.288777	860.043025	12.706586
13.307617	857.370425	12.711603
13.510201	871.236286	12.716621
13.610610	892.284492	12.721639
13.797459	891.409572	12.726656
13.566210	888.226041	12.731674
13.831746	894.075574	12.736691
13.756526	876.725530	12.741709
13.805129	888.902025	12.746727
13.730522	879.868420	12.751744
13.729757	890.640165	12.756762
13.761377	893.793913	12.761779
13.815562	884.120504	12.766797
13.924142	892.469533	12.771815
13.962329	875.151497	12.776832
14.004162	878.134661	12.781850
13.971176	874.911610	12.786867
13.549402	853.666802	12.791885
13.769564	877.248972	12.796903
14.092400	883.964562	12.801920
14.183495	873.211871	12.806938
14.026685	867.244890	12.811955
14.161721	851.132833	12.816973
13.653824	857.388361	12.821991
13.668026	850.582872	12.827008
13.853584	859.954913	12.832026
13.905064	879.890000	12.837043
14.258049	871.854050	12.842061
14.315367	865.086689	12.847079
13.948114	857.208589	12.852096
13.925998	855.370683	12.857114
13.849798	857.041169	12.862131
14.013702	845.337116	12.867149
13.809324	856.601979	12.872167
13.845481	865.634607	12.877184
14.074589	876.619447	12.882202
13.965378	883.666409	12.887219
14.199644	864.835277	12.892237
14.202736	878.052321	12.897255
14.033114	874.918034	12.902272
14.334169	880.201077	12.907290
14.051185	879.516154	12.912307
14.384028	871.389450	12.917325
13.965224	876.890111	12.922343
14.012282	871.001177	12.927360
14.221822	879.112232	12.932378
14.089665	884.257571	12.937395
14.478191	870.520336	12.942413
14.253766	878.360351	12.947431
14.129928	870.582483	12.952448
14.362843	868.146861	12.957466
13.962511	877.226969	12.962483
14.300426	865.560620	12.967501
14.511564	875.714617	12.972519
14.258313	872.386314	12.977536
14.478008	876.270691	12.982554
14.437028	880.695453	12.987571
14.257041	863.611579	12.992589
14.333507	878.210894	12.997607
14.381903	880.816611	13.002624
14.486101	876.037452	13.007642
14.116097	885.717239	13.012659
14.113438	876.400870	13.017677
14.323664	875.500821	13.022695
14.449986	876.099634	13.027712
14.759086	873.019930	13.032730
14.155550	871.767644	13.037747
14.714817	870.038969	13.042765
14.599241	873.018671	13.047783
14.182043	877.680129	13.052800
14.550607	877.608940	13.057818
14.230405	895.052562	13.062835
14.538493	897.650319	13.067853
14.689600	911.713314	13.072871
14.734834	907.631673	13.077888
14.990307	907.367015	13.082906
14.584904	898.620053	13.087923
14.689827	899.437362	13.092941
14.835079	899.096077	13.097959
14.746870	889.306879	13.102976
14.535892	867.525990	13.107994
14.643306	891.352430	13.113011
14.746774	895.012761	13.118029
15.005065	893.986253	13.123047
14.754297	886.895899	13.128064
14.962918	877.905157	13.133082
14.397590	876.474111	13.138099
14.751847	884.050599	13.143117
14.793692	892.755938	13.148135
14.727595	913.554592	13.153152
14.780670	907.477255	13.158170
14.720309	909.062844	13.163187
14.925317	912.244181	13.168205
14.976511	902.958247	13.173223
14.656481	912.168379	13.178240
15.023225	912.941547	13.183258
15.034968	905.717563	13.188275
15.097778	905.616297	13.193293
15.222994	907.254224	13.198311
14.835964	901.278502	13.203328
15.071741	891.956105	13.208346
14.727263	913.657115	13.213363
14.985062	911.463023	13.218381
15.250677	911.776187	13.223399
15.001106	910.204668	13.228416
15.269841	903.876670	13.233434
14.975569	899.248521	13.238451
15.042314	898.604895	13.243469
15.304962	901.180257	13.248487
14.811081	903.412407	13.253504
14.839422	900.693346	13.258522
15.077774	903.732553	13.263539
15.067303	901.468323	13.268557
14.758352	902.181730	13.273575
14.901339	913.243846	13.278592
15.370371	905.709506	13.283610
15.094181	910.033073	13.288627
14.966138	907.031652	13.293645
14.940852	908.084292	13.298663
14.965634	902.468313	13.303680
15.243587	900.667325	13.308698
15.114316	909.730126	13.313715
15.069577	898.805824	13.318733
15.372905	920.734206	13.323751
15.312350	929.628168	13.328768
15.715623	920.653986	13.333786
15.382870	909.601390	13.338803
15.040999	899.928595	13.343821
15.237440	907.800112	13.348839
15.086184	925.940958	13.353856
15.482774	921.988528	13.358874
15.522857	929.538718	13.363891
15.623726	931.717664	13.368909
15.655881	922.899810	13.373927
15.675029	919.762208	13.378944
16.014995	924.442787	13.383962
15.664105	906.753334	13.388979
15.447389	892.706474	13.393997
15.231163	889.714146	13.399015
15.312220	899.909383	13.404032
15.637760	898.069021	13.409050
15.694969	914.745086	13.414067
15.654437	910.200503	13.419085
15.900610	899.157953	13.424103
15.608425	893.598006	13.429120
15.793720	885.197315	13.434138
15.521595	895.476621	13.439155
15.542194	883.443528	13.444173
15.778403	890.369126	13.449191
15.526674	891.427372	13.454208
15.301221	890.619148	13.459226
15.411773	913.519556	13.464243
15.448895	928.106536	13.469261
15.827347	923.578000	13.474279
15.777287	928.687714	13.479296
15.954672	920.473345	13.484314
15.935259	931.758813	13.489331
15.830282	929.839348	13.494349
16.064426	919.167657	13.499367
15.904097	924.907413	13.504384
16.212720	914.902496	13.509402
16.030242	902.865222	13.514419
15.781274	893.043983	13.519437
16.007807	895.817048	13.524455
15.842504	891.238408	13.529472
15.406811	886.611239	13.534490
15.604530	901.793620	13.539507
16.038437	913.045349	13.544525
16.331617	915.916431	13.549543
16.020732	917.963958	13.554560
16.069747	914.849362	13.559578
15.991928	914.188337	13.564595
15.804911	918.276678	13.569613
15.991095	915.225193	13.574631
16.149105	923.294805	13.579648
16.045599	905.753358	13.584666
16.075722	917.553819	13.589683
16.078111	915.574059	13.594701
16.452627	911.272940	13.599719
16.190646	921.167922	13.604736
16.089089	914.384723	13.609754
16.152829	918.933095	13.614771
15.986368	912.600782	13.619789
16.226948	916.411241	13.624807
16.143624	918.988384	13.629824
16.098677	916.988511	13.634842
16.367308	923.893401	13.639859
16.065773	923.570588	13.644877
16.269071	921.054039	13.649895
16.098587	924.325113	13.654912
16.340662	911.840383	13.659930
16.095541	913.409324	13.664947
16.247064	917.914815	13.669965
16.104876	914.343713	13.674983
16.240718	921.564671	13.680000
16.593075	910.662005	13.685018
16.151394	917.338068	13.690035
16.160720	920.152615	13.695053
16.431063	929.566956	13.700071
16.651116	945.028739	13.705088
16.636572	940.965649	13.710106
16.333148	924.691877	13.715123
16.281504	936.983429	13.720141
16.723368	942.239241	13.725159
16.569322	943.242735	13.730176
16.857248	939.726779	13.735194
16.710564	923.835303	13.740211
16.497927	913.808437	13.745229
16.783769	916.002025	13.750247
16.224155	920.252452	13.755264
16.513431	925.212673	13.760282
16.756823	937.517968	13.765299
16.856803	942.637486	13.770317
16.883848	923.707925	13.775335
16.815066	925.935039	13.780352
16.492054	912.236456	13.785370
16.701339	915.955251	13.790387
16.732901	913.139596	13.795405
16.728137	922.316428	13.800423
16.696848	936.610033	13.805440
17.083316	944.493016	13.810458
17.026198	927.451714	13.815475
16.807393	921.989444	13.820493
16.898996	915.569125	13.825511
16.490152	919.043045	13.830528
16.648124	912.821963	13.835546
16.844559	921.343066	13.840563
17.127246	944.898058	13.845581
16.818091	938.581095	13.850599
16.723784	938.349946	13.855616
16.928929	950.254121	13.860634
17.063100	945.659734	13.865651
16.822636	957.388893	13.870669
17.002207	951.922062	13.875687
17.205798	951.515213	13.880704
17.109390	944.900432	13.885722
17.252448	944.696905	13.890739
17.127684	953.944411	13.895757
17.349966	924.897516	13.900775
17.013752	927.055139	13.905792
16.741504	908.503486	13.910810
17.080013	923.686197	13.915827
17.020918	938.338723	13.920845
17.218192	936.342044	13.925863
16.957749	949.324845	13.930880
17.001307	943.000655	13.935898
17.092931	950.897030	13.940915
17.297602	948.215296	13.945933
17.297750	942.616767	13.950951
17.056410	944.194140	13.955968
16.789196	952.769593	13.960986
17.344097	944.595059	13.966003
17.009771	947.399981	13.971021
17.291526	941.119417	13.976039
17.509431	940.068100	13.981056
17.502336	944.488451	13.986074
17.745889	944.434811	13.991091
17.160835	945.773441	13.996109
17.444407	943.754992	14.001127
17.140389	945.278179	14.006144
17.165439	946.907894	14.011162
17.248362	939.609905	14.016179
17.108213	959.094169	14.021197
17.683921	956.065574	14.026215
17.677226	970.400411	14.031232
17.520201	957.421517	14.036250
17.299219	938.674339	14.041267
17.408466	952.075040	14.046285
17.621076	964.786619	14.051303
17.604152	969.112151	14.056320
17.304446	966.013558	14.061338
17.604676	966.496574	14.066355
17.516458	968.836357	14.071373
17.533844	957.845822	14.076391
17.626629	962.709069	14.081408
17.778044	963.554901	14.086426
17.902415	961.374236	14.091443
17.761694	964.505357	14.096461
17.827907	961.800092	14.101479
17.733625	958.341514	14.106496
17.815843	964.547794	14.111514
17.867376	960.807601	14.116531
17.903509	963.182696	14.121549
18.161136	952.009477	14.126567
18.113219	970.771033	14.131584
17.899444	963.104463	14.136602
18.148268	963.675121	14.141619
17.705637	959.666770	14.146637
18.178152	954.519132	14.151655
18.153029	949.585387	14.156672
17.890497	940.222644	14.161690
17.895341	930.378644	14.166707
17.656221	935.605882	14.171725
17.746182	944.747752	14.176743
18.181392	960.091250	14.181760
17.789700	956.386263	14.186778
18.225083	958.077163	14.191795
18.112703	967.690328	14.196813
17.960421	962.829994	14.201831
18.069672	955.816603	14.206848
18.061098	957.694790	14.211866
18.221747	956.348241	14.216883
18.002791	960.358026	14.221901
18.026427	953.289524	14.226919
18.360236	946.261394	14.231936
17.907383	968.581581	14.236954
18.048514	951.530260	14.241971
17.944128	958.915812	14.246989
18.462670	951.950000	14.252007
18.347322	951.392427	14.257024
17.617240	959.470537	14.262042
18.096073	951.446384	14.267059
17.929749	958.932740	14.272077
18.365986	960.286111	14.277095
18.481696	971.229563	14.282112
18.328811	959.947155	14.287130
18.484408	962.429234	14.292147
18.179619	974.047016	14.297165
18.427385	977.814963	14.302183
18.676778	987.408392	14.307200
18.440118	991.458123	14.312218
18.652126	979.894030	14.317235
18.284389	978.792445	14.322253
18.469126	995.473857	14.327271
18.740753	988.598912	14.332288
18.767721	990.192882	14.337306
18.679939	976.884802	14.342323
18.335398	967.741125	14.347341
18.272620	967.886235	14.352359
18.750170	978.389084	14.357376
18.814429	985.660113	14.362394
18.811000	985.480841	14.367411
18.531634	980.896653	14.372429
18.726570	981.807719	14.377447
18.561457	985.226729	14.382464
18.527035	986.728900	14.387482
18.734802	987.329585	14.392499
18.690417	978.738145	14.397517
18.806367	980.069752	14.402535
18.854685	978.331582	14.407552
18.716099	982.372551	14.412570
18.722088	975.576635	14.417587
18.859642	977.019228	14.422605
18.552652	977.620900	14.427623
18.888293	978.978726	14.432640
18.568855	986.643198	14.437658
18.793691	985.935598	14.442675
18.613323	990.785818	14.447693
18.708899	980.897630	14.452711
18.697419	989.728384	14.457728
19.304853	1003.048212	14.462746
19.185809	1012.553851	14.467763
19.066242	1008.503015	14.472781
19.095874	1012.438582	14.477799
19.647687	997.793916	14.482816
19.303898	989.420543	14.487834
19.412473	975.143374	14.492851
19.503944	978.810436	14.497869
19.228411	973.838229	14.502887
19.554280	969.916000	14.507904
19.340340	970.149917	14.512922
19.450745	970.637989	14.517939
19.503477	976.561372	14.522957
19.401912	971.700118	14.527975
19.539551	978.753097	14.532992
19.496468	966.274992	14.538010
19.501167	943.895705	14.543027
19.154276	940.860440	14.548045
18.990126	947.284271	14.553063
19.362218	953.998823	14.558080
19.448208	964.056677	14.563098
19.462344	972.657599	14.568115
19.399102	969.359620	14.573133
19.123744	985.166852	14.578151
19.655103	973.135333	14.583168
19.325907	985.378792	14.588186
19.465475	971.334280	14.593203
19.545618	965.379992	14.598221
19.666082	976.773429	14.603239
19.829090	972.493143	14.608256
19.666585	968.451396	14.613274
19.711859	959.847482	14.618291
19.694680	948.933933	14.623309
19.377793	944.122121	14.628327
19.801989	945.231039	14.633344
19.340585	956.905841	14.638362
19.324847	966.448674	14.643379
19.726129	973.578069	14.648397
19.064107	971.634305	14.653415
19.689667	968.333291	14.658432
19.395739	974.013300	14.663450
19.459748	968.589219	14.668467
19.662788	974.759749	14.673485
19.661558	972.205802	14.678503
19.918254	974.245176	14.683520
19.711939	976.636010	14.688538
19.952293	971.868920	14.693555
19.754329	974.041844	14.698573
19.522094	987.007408	14.703591
19.905697	995.734165	14.708608
19.636174	1005.889101	14.713626
19.714110	1005.510143	14.718643
19.800357	1010.396928	14.723661
19.635384	1012.007329	14.728679
20.076672	1006.670758	14.733696
19.896087	1014.718535	14.738714
20.224017	1001.936063	14.743731
20.150391	999.702748	14.748749
20.149378	1011.806063	14.753767
20.608349	1001.680530	14.758784
20.173473	1004.407628	14.763802
19.801568	997.180594	14.768819
20.241915	1009.850956	14.773837
19.985764	1005.802660	14.778855
20.593529	1002.684893	14.783872
20.262948	1009.689436	14.788890
20.145150	1009.973180	14.793907
20.520771	1001.459418	14.798925
19.842571	1001.702496	14.803943
20.087299	1006.251238	14.808960
19.903422	1006.212078	14.813978
20.059749	1005.996117	14.818995
20.338039	1020.596792	14.824013
20.518898	1038.056029	14.829031
20.722609	1039.386495	14.834048
20.340093	1019.537268	14.839066
20.086419	1014.285061	14.844083
20.676048	1026.529160	14.849101
20.677696	1022.164953	14.854119
20.733491	1005.591859	14.859136
20.727637	1010.682075	14.864154
20.468016	994.989141	14.869171
20.774169	995.434959	14.874189
20.233983	1009.449131	14.879207
20.596002	990.296705	14.884224
20.322962	1008.010586	14.889242
20.369236	1013.196499	14.894259
20.808761	1024.246600	14.899277
20.686836	1030.781579	14.904295
20.630673	1037.482438	14.909312
20.776312	1031.141309	14.914330
20.746634	1027.048420	14.919347
20.596611	1032.472740	14.924365
20.947172	1031.957304	14.929383
20.997656	1027.257069	14.934400
21.249293	1036.645440	14.939418
20.783417	1021.929116	14.944435
20.892426	1006.038522	14.949453
20.321221	1004.234828	14.954471
20.772772	1018.745397	14.959488
20.914898	1025.061856	14.964506
21.067095	1032.697859	14.969523
21.371011	1029.520168	14.974541
21.228943	1038.833186	14.979559
21.200063	1021.415072	14.984576
20.993642	1000.048972	14.989594
20.591258	1007.113433	14.994611
21.286613	1014.774052	14.999629
20.903112	1024.476632	15.004647
21.050611	1018.185986	15.009664
20.945717	1032.398563	15.014682
20.920797	1016.950985	15.019699
21.157057	1016.156850	15.024717
20.913311	1033.169479	15.029735
20.823439	1018.242872	15.034752
20.949952	1023.023391	15.039770
21.120136	1030.193440	15.044787
21.315600	1025.525103	15.049805
21.358582	1027.727426	15.054823
21.500644	1025.211946	15.059840
21.060969	1032.336528	15.064858
21.143324	1030.047854	15.069875
21.578134	1034.532454	15.074893
21.304991	1028.803563	15.079911
21.220590	1027.270821	15.084928
21.314301	1039.980496	15.089946
21.451410	1045.608055	15.094963
22.030321	1047.950372	15.099981
21.496232	1053.041065	15.104999
21.462105	1032.730211	15.110016
21.672810	1017.087717	15.115034
21.748305	1027.106407	15.120051
21.782555	1027.233876	15.125069
21.632648	1026.740289	15.130087
21.565059	1023.649310	15.135104
21.365539	1024.988672	15.140122
21.457780	1033.548742	15.145139
21.526047	1032.516291	15.150157
21.431676	1045.133497	15.155175
21.491954	1039.623398	15.160192
21.628498	1041.642915	15.165210
21.553595	1037.836241	15.170227
21.835481	1038.701418	15.175245
21.714356	1042.429680	15.180263
21.972075	1040.054096	15.185280
21.948649	1033.184681	15.190298
21.869619	1042.007753	15.195315
21.995389	1045.045946	15.200333
21.827931	1041.170742	15.205351
22.010938	1039.116179	15.210368
21.916090	1044.165239	15.215386
22.098507	1049.382162	15.220403
22.098299	1036.988630	15.225421
21.991477	1052.207413	15.230439
22.009663	1044.468930	15.235456
22.446998	1035.245350	15.240474
22.185483	1046.972945	15.245491
22.300036	1042.134542	15.250509
22.028522	1043.821248	15.255527
22.154221	1041.865147	15.260544
21.940371	1041.318763	15.265562
21.867957	1037.885679	15.270579
22.143168	1041.213682	15.275597
21.978122	1047.394798	15.280615
21.997786	1045.069654	15.285632
22.492535	1039.415569	15.290650
22.519321	1048.939208	15.295667
22.575601	1037.371330	15.300685
22.008813	1046.722791	15.305703
21.958067	1046.811187	15.310720
21.805006	1037.066491	15.315738
22.039712	1053.934174	15.320755
22.397510	1061.270803	15.325773
22.199295	1065.414971	15.330791
22.428419	1072.247340	15.335808
22.775782	1068.930561	15.340826
22.331277	1077.628744	15.345843
22.341464	1070.211246	15.350861
22.599215	1077.992387	15.355879
22.376601	1077.970664	15.360896
22.678948	1073.663735	15.365914
22.380776	1073.012025	15.370931
22.829120	1067.838039	15.375949
22.346633	1074.135900	15.380967
22.237588	1063.387871	15.385984
22.840655	1063.572329	15.391002
22.699474	1075.686305	15.396019
22.673609	1061.670286	15.401037
22.419511	1076.506801	15.406055
22.905664	1085.792199	15.411072
23.190237	1068.240637	15.416090
23.092573	1067.669502	15.421107
22.936925	1062.161685	15.426125
22.903401	1062.938937	15.431143
22.968516	1066.364724	15.436160
23.231648	1051.645371	15.441178
23.076708	1065.791466	15.446195
23.153856	1053.535106	15.451213
23.276263	1055.930967	15.456231
23.489141	1054.217900	15.461248
23.922575	1060.477870	15.466266
23.308820	1052.977481	15.471283
22.971288	1037.663926	15.476301
23.217926	1032.309973	15.481319
23.007613	1034.055438	15.486336
23.207747	1032.838560	15.491354
23.039633	1043.348369	15.496371
23.550899	1048.704533	15.501389
23.063685	1043.668146	15.506407
22.947145	1056.711457	15.511424
23.026715	1049.076583	15.516442
23.138177	1068.054770	15.521459
23.297023	1055.098685	15.526477
23.271102	1054.878650	15.531495
23.148298	1058.598928	15.536512
23.563485	1060.935287	15.541530
23.292995	1057.240519	15.546547
23.424265	1056.411013	15.551565
23.344158	1060.169101	15.556583
23.163449	1050.541175	15.561600
23.699047	1058.571171	15.566618
23.344138	1058.744576	15.571635
23.284143	1056.262547	15.576653
23.316345	1053.116851	15.581671
23.122183	1051.436539	15.586688
23.593571	1059.179540	15.591706
23.787025	1064.257638	15.596723
23.682206	1065.599825	15.601741
23.456817	1061.169268	15.606759
23.191132	1072.834189	15.611776
23.736509	1078.484706	15.616794
23.880038	1090.330297	15.621811
23.981975	1080.055572	15.626829
23.920406	1079.959546	15.631847
23.401101	1090.062593	15.636864
23.669143	1084.486188	15.641882
23.858534	1084.241130	15.646899
23.815941	1093.976671	15.651917
23.941273	1078.228965	15.656935
23.981107	1081.057386	15.661952
24.054397	1081.982301	15.666970
23.797062	1083.545407	15.671987
24.066805	1080.175340	15.677005
24.222777	1084.010087	15.682023
23.810699	1085.981086	15.687040
23.896852	1076.663275	15.692058
23.769716	1077.698146	15.697075
23.557444	1080.179349	15.702093
23.571920	1080.294740	15.707111
24.037084	1103.209936	15.712128
24.513489	1105.268458	15.717146
24.435266	1117.331886	15.722163
24.169749	1106.738078	15.727181
24.600765	1097.850537	15.732199
24.098562	1094.155547	15.737216
24.304825	1095.132458	15.742234
24.231829	1110.437033	15.747251
24.303847	1114.245926	15.752269
23.907822	1115.489098	15.757287
24.023355	1120.965931	15.762304
24.404719	1112.692489	15.767322
24.351299	1108.539339	15.772339
24.175848	1111.352627	15.777357
24.377143	1105.188073	15.782375
24.204830	1112.812104	15.787392
24.554892	1108.918905	15.792410
24.575166	1101.524918	15.797427
24.744929	1102.640152	15.802445
24.694717	1103.829999	15.807463
24.667314	1103.624382	15.812480
25.130509	1105.293766	15.817498
24.981045	1106.356744	15.822515
24.928563	1110.986620	15.827533
24.644116	1101.012466	15.832551
24.620612	1114.030184	15.837568
24.991796	1104.920270	15.842586
25.330012	1118.340287	15.847603
25.048772	1104.462181	15.852621
24.986417	1105.875685	15.857639
25.005685	1108.615000	15.862656
25.097385	1106.836956	15.867674
24.950775	1116.012587	15.872691
24.859074	1109.913082	15.877709
25.317403	1109.389641	15.882727
24.852204	1101.281972	15.887744
25.034938	1097.095627	15.892762
25.021019	1104.837910	15.897779
25.052547	1104.945753	15.902797
25.330738	1105.678085	15.907815
24.648222	1107.010424	15.912832
25.109764	1105.762854	15.917850
25.050255	1110.835217	15.922867
24.866775	1101.576998	15.927885
25.268213	1095.735989	15.932903
25.044470	1105.390512	15.937920
25.252878	1101.205820	15.942938
25.367471	1107.790642	15.947955
25.421096	1108.218437	15.952973
25.345542	1099.655318	15.957991
25.248026	1105.872518	15.963008
25.088446	1097.391421	15.968026
25.154673	1106.148747	15.973043
25.116831	1101.669013	15.978061
25.230126	1101.929847	15.983079
25.336032	1102.224973	15.988096
25.208209	1105.893339	15.993114
25.593656	1114.077356	15.998131
25.536499	1133.442982	16.003149
25.801317	1134.031865	16.008167
25.760012	1133.524228	16.013184
25.805721	1128.089342	16.018202
25.581123	1118.311560	16.023219
25.356993	1129.188959	16.028237
26.235691	1124.392500	16.033255
25.697469	1127.114683	16.038272
25.360724	1129.096442	16.043290
25.501908	1121.219841	16.048307
25.615579	1123.461653	16.053325
25.903060	1128.295076	16.058343
25.694551	1132.723635	16.063360
25.871770	1124.777681	16.068378
25.808793	1133.191073	16.073395
25.404536	1128.726336	16.078413
25.922337	1128.655238	16.083431
25.570959	1126.978510	16.088448
25.671232	1126.880488	16.093466
25.797372	1133.826783	16.098483
25.766409	1154.000671	16.103501
26.048061	1158.739008	16.108519
26.250082	1153.391220	16.113536
26.279405	1159.072494	16.118554
26.427448	1161.850336	16.123571
26.530716	1155.301612	16.128589
26.503082	1148.748188	16.133607
26.538182	1144.401635	16.138624
26.157302	1132.576162	16.143642
26.183067	1134.080586	16.148659
26.155536	1141.721601	16.153677
26.595040	1134.968002	16.158695
26.524475	1143.398404	16.163712
26.479383	1131.728347	16.168730
26.199913	1130.790476	16.173747
26.267765	1147.609120	16.178765
26.068068	1150.165021	16.183783
26.358332	1141.537368	16.188800
26.195045	1150.468545	16.193818
26.388293	1144.703328	16.198835
26.176678	1157.024693	16.203853
26.704062	1149.773086	16.208871
26.339502	1153.397593	16.213888
26.714811	1146.014874	16.218906
26.974696	1139.093383	16.223923
26.567720	1147.355088	16.228941
26.748891	1145.538603	16.233959
26.479019	1147.595115	16.238976
26.373905	1148.105494	16.243994
26.588427	1155.067479	16.249011
26.723473	1160.319842	16.254029
26.870747	1176.699394	16.259047
27.059994	1172.213534	16.264064
26.931166	1177.403299	16.269082
26.934331	1172.016781	16.274099
27.233745	1169.615769	16.279117
27.133201	1159.054843	16.284135
26.942371	1143.710198	16.289152
26.859051	1144.362633	16.294170
27.403428	1155.052958	16.299187
26.980807	1154.491140	16.304205
27.222492	1154.737802	16.309223
27.081570	1152.740010	16.314240
26.733965	1155.228673	16.319258
27.152962	1164.880741	16.324275
27.041499	1170.545174	16.329293
27.179961	1166.156305	16.334311
27.160188	1168.419432	16.339328
27.227101	1170.718597	16.344346
27.737149	1164.546202	16.349363
27.328449	1176.691167	16.354381
27.372110	1168.938561	16.359399
27.400889	1160.776231	16.364416
27.732992	1166.884130	16.369434
27.733729	1157.204441	16.374451
27.534145	1166.281790	16.379469
27.488750	1160.492304	16.384487
27.492125	1168.817172	16.389504
27.196191	1164.123076	16.394522
27.824929	1162.749001	16.399539
27.510989	1166.840313	16.404557
27.976885	1157.732401	16.409575
27.770100	1166.560557	16.414592
27.488463	1164.121117	16.419610
27.787443	1157.277394	16.424627
27.830958	1159.311936	16.429645
27.956215	1154.524874	16.434663
27.748530	1153.236542	16.439680
27.768483	1159.402818	16.444698
27.919877	1160.295515	16.449715
27.704074	1161.102560	16.454733
27.772250	1148.414159	16.459751
27.887645	1155.698454	16.464768
27.741915	1153.014471	16.469786
27.953060	1151.703243	16.474803
27.720761	1163.793794	16.479821
27.941541	1157.131913	16.484839
27.970018	1156.759566	16.489856
28.060766	1164.718793	16.494874
28.210903	1164.963292	16.499891
28.099062	1180.447198	16.504909
28.393213	1179.646619	16.509927
28.252265	1194.588130	16.514944
27.725071	1185.056074	16.519962
28.452985	1189.988237	16.524979
28.305406	1198.075525	16.529997
28.167097	1180.639919	16.535015
28.373584	1187.662696	16.540032
28.168471	1182.476404	16.545050
28.322971	1186.316539	16.550067
28.094745	1192.234953	16.555085
28.061571	1188.654004	16.560103
28.279751	1175.089584	16.565120
28.225885	1186.917150	16.570138
28.550708	1173.763802	16.575155
28.383142	1187.262904	16.580173
28.351399	1182.151052	16.585191
28.758529	1205.644893	16.590208
28.419705	1210.765900	16.595226
28.881572	1210.955239	16.600243
28.761761	1204.075331	16.605261
28.910877	1207.143942	16.610279
29.294218	1198.441792	16.615296
28.743407	1187.060939	16.620314
28.756423	1172.806103	16.625331
28.703373	1169.366240	16.630349
28.954379	1180.366570	16.635367
29.225031	1180.094670	16.640384
28.922331	1172.256111	16.645402
29.106380	1173.735510	16.650419
28.746763	1169.862959	16.655437
29.066140	1173.572249	16.660455
29.106647	1181.123280	16.665472
28.959896	1186.043583	16.670490
29.209711	1185.135781	16.675507
28.863426	1198.053084	16.680525
29.550991	1192.378435	16.685543
29.592121	1190.694186	16.690560
29.410546	1181.730083	16.695578
28.976527	1168.456334	16.700595
29.054364	1173.017407	16.705613
29.170477	1184.318020	16.710631
29.595271	1195.080928	16.715648
29.469485	1197.572237	16.720666
29.773869	1187.009596	16.725683
29.650879	1174.104408	16.730701
29.501588	1170.115536	16.735719
29.562448	1166.599334	16.740736
29.429510	1166.214740	16.745754
29.374623	1151.526692	16.750771
29.437383	1162.669593	16.755789
29.348865	1177.253991	16.760807
29.580919	1179.661243	16.765824
29.607364	1200.865027	16.770842
29.704735	1186.033235	16.775859
29.435717	1197.951550	16.780877
29.907904	1194.625101	16.785895
29.897648	1189.802594	16.790912
29.610166	1196.850083	16.795930
29.386313	1192.633400	16.800947
29.555877	1202.029557	16.805965
29.268753	1191.634933	16.810983
29.939115	1192.257453	16.816000
29.658850	1199.212018	16.821018
30.083311	1210.800167	16.826035
30.055471	1230.388219	16.831053
30.238693	1228.339107	16.836071
30.159662	1212.923915	16.841088
29.944452	1201.987074	16.846106
30.143792	1217.290360	16.851123
30.107523	1217.123610	16.856141
29.812565	1222.424362	16.861159
29.993856	1217.242185	16.866176
30.033986	1222.812246	16.871194
30.034188	1223.509121	16.876211
30.091052	1213.930730	16.881229
30.180061	1216.234117	16.886247
30.186465	1218.694487	16.891264
30.198672	1220.016129	16.896282
30.526569	1216.879311	16.901299
30.370031	1214.941969	16.906317
30.649708	1216.626006	16.911335
30.802307	1213.462703	16.916352
30.277774	1213.917732	16.921370
30.661549	1214.129451	16.926387
30.506581	1211.407224	16.931405
30.434751	1212.505385	16.936423
30.515416	1210.231531	16.941440
30.334022	1222.039296	16.946458
30.467471	1236.730299	16.951475
30.672381	1237.855078	16.956493
30.646354	1245.766756	16.961511
30.730406	1232.941408	16.966528
30.523554	1243.779806	16.971546
31.112113	1231.232724	16.976563
31.159830	1238.382599	16.981581
30.781080	1243.721641	16.986599
31.197586	1239.623711	16.991616
30.803686	1247.190406	16.996634
30.936279	1239.901375	17.001651
31.369564	1236.210894	17.006669
31.162306	1239.371984	17.011687
31.220533	1235.381411	17.016704
30.907617	1243.015795	17.021722
31.121979	1243.213047	17.026739
31.609182	1233.724800	17.031757
31.489026	1235.655355	17.036775
31.526522	1226.723454	17.041792
30.920614	1241.410905	17.046810
31.300670	1245.666451	17.051827
31.402714	1247.672811	17.056845
31.620255	1243.054688	17.061863
31.776461	1227.732810	17.066880
31.530454	1238.900515	17.071898
31.553489	1237.209808	17.076915
31.493716	1235.982015	17.081933
31.592100	1244.171115	17.086951
31.737070	1228.652282	17.091968
31.261210	1234.121571	17.096986
31.476630	1232.716718	17.102003
31.673680	1237.781286	17.107021
31.557871	1231.531790	17.112039
31.749611	1231.566256	17.117056
31.240095	1240.196161	17.122074
31.250668	1236.659531	17.127091
31.875415	1233.700716	17.132109
31.519744	1241.060295	17.137127
31.847119	1240.312479	17.142144
31.648744	1259.032369	17.147162
31.742437	1268.270661	17.152179
31.912206	1260.460908	17.157197
31.983200	1262.955471	17.162215
32.188475	1258.429531	17.167232
32.003135	1266.325866	17.172250
32.209265	1264.969005	17.177267
32.377016	1264.361001	17.182285
32.241537	1265.590962	17.187303
32.075381	1259.410814	17.192320
32.325537	1267.879514	17.197338
32.067209	1264.869675	17.202355
32.373147	1259.931799	17.207373
32.402988	1256.538033	17.212391
32.322642	1249.172054	17.217408
32.213628	1253.671572	17.222426
32.092345	1263.369069	17.227443
32.162085	1250.544108	17.232461
31.859020	1259.831161	17.237479
32.430706	1252.448159	17.242496
32.724761	1254.993185	17.247514
32.492047	1262.281235	17.252531
32.335301	1257.786106	17.257549
32.589686	1274.198026	17.262567
32.876013	1270.913359	17.267584
32.857537	1282.371366	17.272602
32.728439	1273.932367	17.277619
32.918939	1257.353234	17.282637
32.625836	1261.748987	17.287655
32.726031	1258.586085	17.292672
33.002793	1268.201142	17.297690
32.776034	1276.351186	17.302707
32.999986	1276.691730	17.307725
33.056383	1288.866855	17.312743
33.201637	1274.832938	17.317760
33.244910	1260.018694	17.322778
33.002965	1254.186522	17.327795
32.947912	1252.184735	17.332813
32.634587	1262.983691	17.337831
32.963518	1270.724798	17.342848
33.298699	1272.822476	17.347866
33.206481	1284.399779	17.352883
32.805672	1281.700924	17.357901
32.843349	1291.308340	17.362919
32.972020	1281.671955	17.367936
33.099922	1278.941066	17.372954
32.821356	1282.676558	17.377971
33.215947	1300.949110	17.382989
32.993415	1314.174752	17.388007
33.123811	1318.188198	17.393024
33.421959	1317.402305	17.398042
33.475704	1307.129898	17.403059
33.667909	1309.972107	17.408077
33.453584	1315.226861	17.413095
33.704926	1310.102739	17.418112
33.502317	1308.128920	17.423130
33.545100	1301.708651	17.428147
33.797671	1310.349018	17.433165
33.828091	1302.571373	17.438183
33.907275	1305.094507	17.443200
33.814802	1311.317647	17.448218
33.839643	1304.977905	17.453235
33.546278	1306.578493	17.458253
33.611429	1328.451621	17.463271
33.948065	1338.551680	17.468288
34.238997	1331.802126	17.473306
34.288145	1345.395006	17.478323
34.462421	1328.527150	17.483341
34.334756	1325.568102	17.488359
34.412341	1310.107196	17.493376
34.302753	1293.152130	17.498394
34.269955	1297.290229	17.503411
34.365459	1294.540687	17.508429
34.108620	1296.284436	17.513447
33.939998	1294.475067	17.518464
34.219304	1300.237045	17.523482
34.153858	1325.461648	17.528499
34.611863	1327.061446	17.533517
34.751640	1327.706081	17.538535
34.383295	1329.067123	17.543552
34.626244	1329.646644	17.548570
34.401170	1327.905279	17.553587
35.006300	1322.798161	17.558605
34.631136	1323.966634	17.563623
34.559807	1306.763097	17.568640
34.636907	1305.748851	17.573658
34.706978	1317.297337	17.578675
34.798814	1312.451195	17.583693
34.760210	1320.923251	17.588711
34.934703	1319.352729	17.593728
34.702609	1309.752047	17.598746
34.650892	1321.190784	17.603763
35.222720	1313.287267	17.608781
34.756584	1319.633304	17.613799
34.551920	1318.857440	17.618816
34.950845	1319.726876	17.623834
34.714702	1313.391762	17.628851
34.762986	1325.424956	17.633869
34.825128	1318.692030	17.638887
34.811547	1312.528723	17.643904
34.952048	1313.670865	17.648922
34.850909	1339.082893	17.653939
34.938037	1349.341988	17.658957
35.068786	1347.722015	17.663975
35.145537	1348.510942	17.668992
35.556148	1346.346213	17.674010
35.387212	1347.241962	17.679027
35.549717	1338.962121	17.684045
35.309281	1356.670213	17.689063
35.545991	1350.121358	17.694080
35.780169	1338.800567	17.699098
35.674466	1346.253056	17.704115
35.665012	1346.592091	17.709133
35.779883	1340.329158	17.714151
35.692527	1340.711408	17.719168
35.809071	1338.610331	17.724186
35.621811	1347.817240	17.729203
35.825845	1337.523470	17.734221
35.776567	1348.454352	17.739239
35.743763	1348.456709	17.744256
35.998342	1339.071483	17.749274
35.797184	1340.634367	17.754291
35.855631	1344.604223	17.759309
35.853033	1342.528385	17.764327
35.717871	1339.765062	17.769344
35.931029	1340.841240	17.774362
35.651246	1344.499784	17.779379
35.889924	1354.742056	17.784397
35.708785	1358.182304	17.789415
35.915454	1362.710290	17.794432
36.053321	1355.727807	17.799450
35.767501	1365.023878	17.804467
35.634989	1366.537997	17.809485
36.123091	1370.696162	17.814503
35.957164	1389.672644	17.819520
36.379178	1391.599664	17.824538
36.389979	1395.371520	17.829555
36.442624	1392.505437	17.834573
36.432871	1391.384308	17.839591
36.735402	1388.431574	17.844608
36.811753	1384.726540	17.849626
36.583737	1398.600790	17.854643
37.008295	1386.789391	17.859661
36.520802	1385.944215	17.864679
36.808768	1391.985104	17.869696
37.080612	1374.938839	17.874714
36.779454	1388.021266	17.879731
36.646897	1376.208029	17.884749
36.699494	1393.188126	17.889767
37.123389	1382.380763	17.894784
37.094865	1380.999755	17.899802
36.723496	1384.385288	17.904819
37.036883	1384.117334	17.909837
37.077122	1377.089589	17.914855
36.950103	1378.889803	17.919872
37.163926	1378.001730	17.924890
36.850593	1376.046236	17.929907
36.763069	1373.813199	17.934925
37.132248	1391.697946	17.939943
37.265804	1399.537610	17.944960
37.536782	1393.053928	17.949978
37.016221	1409.462026	17.954995
37.558558	1401.290123	17.960013
37.491423	1399.414725	17.965031
37.218105	1397.418351	17.970048
37.831821	1400.683690	17.975066
37.637490	1399.872253	17.980083
37.773115	1395.331035	17.985101
37.819783	1393.231679	17.990119
37.751974	1387.911954	17.995136
37.426590	1377.426690	18.000154
37.485517	1389.599114	18.005171
37.752872	1390.516717	18.010189
37.894604	1385.970554	18.015207
37.542931	1403.199094	18.020224
37.858369	1389.942001	18.025242
37.802010	1404.265779	18.030259
37.812982	1401.400689	18.035277
37.896285	1399.918487	18.040295
37.678907	1407.240285	18.045312
38.036512	1398.336777	18.050330
37.837552	1396.566670	18.055347
38.239374	1398.798999	18.060365
38.382595	1395.506113	18.065383
37.755584	1404.502014	18.070400
38.038387	1397.003000	18.075418
38.081661	1419.816874	18.080435
38.226314	1428.385415	18.085453
38.492147	1431.930408	18.090471
38.330787	1439.839396	18.095488
38.703873	1429.804973	18.100506
38.440148	1432.406166	18.105523
38.397840	1426.397174	18.110541
38.511920	1413.682057	18.115559
38.290004	1423.414033	18.120576
38.625797	1417.903062	18.125594
38.387526	1432.005021	18.130611
38.404179	1426.591771	18.135629
38.592927	1419.691384	18.140647
38.390327	1426.305241	18.145664
38.564542	1415.914391	18.150682
38.713491	1443.804047	18.155699
38.475317	1450.742305	18.160717
38.898081	1448.672006	18.165735
38.535321	1448.573486	18.170752
38.742767	1452.887593	18.175770
38.927001	1446.768249	18.180787
39.254041	1458.030199	18.185805
39.481176	1443.675095	18.190823
39.629413	1442.031350	18.195840
39.445365	1438.073361	18.200858
39.244597	1439.358633	18.205875
39.004202	1431.165928	18.210893
39.655545	1425.583020	18.215911
39.589629	1443.863883	18.220928
39.491522	1427.685107	18.225946
39.189105	1433.739912	18.230963
39.542044	1430.317412	18.235981
39.721786	1423.351980	18.240999
39.705572	1432.976280	18.246016
39.997590	1435.119317	18.251034
39.808048	1435.338963	18.256051
39.786471	1431.403678	18.261069
39.980246	1433.792507	18.266087
39.604529	1429.722162	18.271104
39.625367	1425.621197	18.276122
39.608010	1434.746088	18.281139
39.981817	1427.769780	18.286157
40.036142	1426.825831	18.291175
39.658058	1439.097819	18.296192
39.603745	1431.826654	18.301210
40.166193	1438.797299	18.306227
39.578276	1434.790436	18.311245
39.929268	1433.681224	18.316263
39.367252	1433.803491	18.321280
39.792414	1436.076054	18.326298
39.757114	1448.148773	18.331315
39.784295	1459.312740	18.336333
39.749410	1465.017750	18.341351
40.066200	1463.429952	18.346368
40.112408	1461.708612	18.351386
39.781335	1463.981201	18.356403
40.133840	1478.120420	18.361421
40.825252	1477.208774	18.366439
40.647995	1475.716558	18.371456
40.805348	1480.670851	18.376474
40.551873	1484.957350	18.381491
40.672573	1483.580363	18.386509
40.281683	1485.915222	18.391527
40.604404	1482.358739	18.396544
41.079484	1469.914115	18.401562
40.780646	1480.107284	18.406579
40.958667	1478.303488	18.411597
41.066915	1475.701803	18.416615
40.961881	1475.439744	18.421632
41.137957	1471.480383	18.426650
41.288717	1472.712965	18.431667
41.349136	1472.101466	18.436685
41.466335	1471.566391	18.441703
41.088231	1473.021580	18.446720
41.152340	1451.513211	18.451738
41.104213	1466.758115	18.456755
41.167013	1472.425693	18.461773
41.352652	1468.328137	18.466791
41.179564	1474.549730	18.471808
41.135897	1477.614096	18.476826
41.527087	1477.471052	18.481843
41.364378	1478.490973	18.486861
41.357239	1471.495440	18.491879
41.246345	1475.645730	18.496896
40.980363	1477.834316	18.501914
40.993188	1471.203978	18.506931
41.232588	1488.975289	18.511949
41.698310	1511.438643	18.516967
41.593166	1503.051064	18.521984
41.734648	1506.542256	18.527002
42.039386	1508.869809	18.532019
41.616803	1511.703223	18.537037
42.060681	1509.862883	18.542055
41.983123	1513.572627	18.547072
42.115630	1503.236655	18.552090
42.153036	1506.561223	18.557107
41.827104	1513.477426	18.562125
42.031549	1502.890174	18.567143
42.097909	1501.570609	18.572160
42.188656	1496.785219	18.577178
42.586673	1495.870184	18.582195
42.274013	1505.636134	18.587213
42.253247	1503.979816	18.592231
42.253560	1502.594809	18.597248
42.397896	1496.341501	18.602266
42.577809	1499.963728	18.607283
42.207262	1505.273941	18.612301
41.973969	1497.156401	18.617319
42.371910	1510.067269	18.622336
42.453311	1518.805387	18.627354
42.552471	1522.002410	18.632371
42.408995	1531.510837	18.637389
42.673816	1522.248608	18.642407
42.940582	1520.881685	18.647424
42.909652	1524.420720	18.652442
42.961410	1525.135055	18.657459
42.917758	1520.203802	18.662477
43.154057	1513.656522	18.667495
43.027517	1523.972765	18.672512
42.804646	1521.428261	18.677530
43.111883	1519.653851	18.682547
43.177988	1522.867372	18.687565
43.433575	1514.202736	18.692583
43.125804	1516.559662	18.697600
43.127966	1523.853038	18.702618
43.411079	1517.492098	18.707635
43.436423	1533.034743	18.712653
43.420966	1510.896950	18.717671
43.267572	1513.425951	18.722688
43.118403	1514.975125	18.727706
43.250202	1510.815214	18.732723
43.417019	1509.727044	18.737741
43.350360	1517.968814	18.742759
43.332718	1511.260040	18.747776
43.327726	1519.826638	18.752794
43.656511	1535.474159	18.757811
43.717891	1548.397479	18.762829
43.840821	1544.921308	18.767847
43.791883	1545.767671	18.772864
44.045886	1541.098543	18.777882
44.201848	1533.815740	18.782899
43.839226	1539.869137	18.787917
44.098319	1543.114880	18.792935
44.032366	1539.444395	18.797952
43.950864	1537.967420	18.802970
44.079341	1538.204882	18.807987
44.175178	1542.930012	18.813005
44.137848	1533.204423	18.818023
43.730174	1540.866059	18.823040
43.899474	1540.798731	18.828058
44.133686	1534.545881	18.833075
44.121326	1559.059321	18.838093
44.531664	1558.298148	18.843111
44.573038	1552.740997	18.848128
44.742622	1562.768865	18.853146
45.002686	1559.125890	18.858163
44.457961	1559.492930	18.863181
44.749122	1563.583759	18.868199
44.586886	1564.199671	18.873216
44.602599	1560.211329	18.878234
44.987625	1557.938604	18.883251
45.133072	1562.762219	18.888269
45.032352	1561.380549	18.893287
44.826892	1560.516221	18.898304
44.874570	1565.818229	18.903322
44.970755	1557.261065	18.908339
44.931034	1551.795295	18.913357
44.874885	1551.128291	18.918375
45.252666	1554.731548	18.923392
44.791347	1558.203272	18.928410
44.897408	1558.281060	18.933427
45.023055	1560.574890	18.938445
45.122139	1556.555422	18.943463
45.368725	1564.084329	18.948480
45.506118	1583.343894	18.953498
45.166921	1580.368642	18.958515
44.901980	1590.538554	18.963533
45.467276	1587.799362	18.968551
45.622526	1591.163884	18.973568
45.707433	1594.593204	18.978586
45.783174	1586.396889	18.983603
45.602996	1587.408685	18.988621
45.820185	1586.858626	18.993639
45.985150	1579.012108	18.998656
45.634044	1587.384084	19.003674
45.883043	1587.113402	19.008691
45.724466	1596.216102	19.013709
45.825328	1588.226650	19.018727
46.161878	1587.333993	19.023744
45.884935	1588.576772	19.028762
45.992722	1585.722389	19.033779
46.214412	1582.819620	19.038797
45.924670	1590.699548	19.043815
45.910699	1602.346022	19.048832
45.793810	1614.937498	19.053850
46.397953	1611.068641	19.058867
46.412755	1614.837525	19.063885
46.615110	1610.615117	19.068903
46.479861	1607.971838	19.073920
46.411751	1611.395789	19.078938
46.498004	1608.001267	19.083955
46.420959	1606.785359	19.088973
46.832151	1615.261051	19.093991
46.995608	1608.107682	19.099008
46.806371	1611.042240	19.104026
47.276824	1608.184103	19.109043
47.187135	1607.626981	19.114061
46.760089	1603.808789	19.119079
46.921712	1599.751790	19.124096
46.954590	1606.430276	19.129114
47.021430	1595.457085	19.134131
46.833858	1609.582700	19.139149
46.834141	1616.216982	19.144167
47.467421	1618.593303	19.149184
47.144190	1619.169339	19.154202
47.132230	1625.535966	19.159219
47.537369	1627.241008	19.164237
47.371961	1633.617299	19.169255
47.622938	1638.324644	19.174272
47.483415	1634.821437	19.179290
47.589048	1630.447715	19.184307
47.637578	1631.909048	19.189325
47.799246	1634.481964	19.194343
47.734975	1625.072590	19.199360
47.443481	1635.601652	19.204378
47.924259	1619.973283	19.209395
48.089184	1625.585031	19.214413
47.431129	1628.623990	19.219431
47.774234	1627.370009	19.224448
47.930450	1620.344998	19.229466
47.962006	1629.665448	19.234483
47.469715	1632.214756	19.239501
47.531190	1623.947948	19.244519
48.123140	1624.848829	19.249536
47.881018	1639.343346	19.254554
48.100018	1652.638688	19.259571
48.372992	1649.215208	19.264589
48.159058	1651.617248	19.269607
48.562483	1647.311930	19.274624
48.037018	1652.922253	19.279642
48.522751	1645.096606	19.284659
48.323893	1645.384726	19.289677
48.533671	1648.735114	19.294695
48.846756	1644.175464	19.299712
48.514668	1649.555735	19.304730
48.481430	1649.573124	19.309747
48.687686	1646.778017	19.314765
48.685901	1646.659096	19.319783
48.893464	1634.868085	19.324800
48.897897	1648.609581	19.329818
48.746250	1644.657197	19.334835
48.887349	1633.428768	19.339853
49.020120	1634.500562	19.344871
49.213046	1634.045463	19.349888
48.663791	1642.531774	19.354906
48.925794	1657.644413	19.359923
49.472471	1669.742596	19.364941
49.267091	1672.576295	19.369959
49.552377	1671.548420	19.374976
49.513771	1668.219047	19.379994
49.592401	1667.128146	19.385011
49.534761	1671.270064	19.390029
49.257035	1669.865724	19.395047
49.775480	1669.566570	19.400064
49.713423	1678.487981	19.405082
49.784882	1667.213972	19.410099
49.813459	1674.351470	19.415117
49.719318	1670.650581	19.420135
49.617878	1673.545023	19.425152
49.723288	1667.918173	19.430170
49.867561	1667.508925	19.435187
50.009129	1665.458386	19.440205
49.822831	1667.763332	19.445223
49.816571	1663.899469	19.450240
49.732461	1672.747756	19.455258
49.728584	1664.316157	19.460275
50.260692	1673.297453	19.465293
50.142719	1689.441546	19.470311
50.375744	1680.535277	19.475328
50.200391	1693.682563	19.480346
50.363495	1684.196134	19.485363
50.260616	1683.849068	19.490381
50.010361	1685.467752	19.495399
50.536459	1683.146061	19.500416
50.458037	1688.158752	19.505434
50.290665	1681.878240	19.510451
50.545548	1684.501873	19.515469
50.224986	1708.450830	19.520487
50.351742	1706.201557	19.525504
50.672539	1714.198961	19.530522
50.881146	1709.760135	19.535539
50.669706	1707.421582	19.540557
50.385156	1716.671983	19.545575
50.884200	1721.217807	19.550592
50.955069	1744.325229	19.555610
51.069744	1732.315272	19.560627
51.251780	1732.736390	19.565645
51.289952	1735.222291	19.570663
51.623752	1729.581618	19.575680
51.621255	1742.979461	19.580698
51.481086	1731.199891	19.585715
51.711048	1734.271756	19.590733
51.573213	1733.626538	19.595751
51.542634	1729.296208	19.600768
51.410811	1730.065753	19.605786
51.889921	1723.358889	19.610803
51.888213	1730.777020	19.615821
51.409379	1729.822512	19.620839
52.017940	1726.304868	19.625856
51.723139	1722.380891	19.630874
51.711071	1720.300665	19.635891
52.205368	1716.737375	19.640909
51.786973	1719.883126	19.645927
51.874061	1716.184896	19.650944
52.048564	1719.090744	19.655962
51.957983	1726.897606	19.660979
52.152349	1729.049768	19.665997
52.529776	1753.624568	19.671015
52.964536	1741.724991	19.676032
52.598367	1729.522603	19.681050
52.530940	1725.210974	19.686067
52.484604	1725.617936	19.691085
52.282367	1728.468448	19.696103
52.723942	1716.446107	19.701120
52.471883	1716.965086	19.706138
52.448602	1720.074549	19.711155
52.744409	1736.602151	19.716173
52.366822	1747.123103	19.721191
52.550509	1744.405732	19.726208
52.619538	1755.632275	19.731226
52.521946	1752.376037	19.736243
52.474998	1751.159464	19.741261
52.584367	1763.774229	19.746279
53.182333	1771.532067	19.751296
53.086951	1769.390432	19.756314
53.166459	1771.437994	19.761331
53.241028	1769.805232	19.766349
53.156640	1781.303655	19.771367
53.394179	1777.044668	19.776384
53.314771	1771.112158	19.781402
53.609029	1779.145487	19.786419
53.590256	1771.276932	19.791437
53.419542	1772.608043	19.796455
53.142478	1776.249307	19.801472
53.363456	1780.817567	19.806490
53.659440	1795.803060	19.811507
53.967496	1792.818235	19.816525
53.815560	1803.647535	19.821543
54.240939	1789.380943	19.826560
53.979570	1803.047293	19.831578
54.256747	1801.242003	19.836595
54.363579	1794.102255	19.841613
54.315996	1799.907129	19.846631
54.388744	1783.493784	19.851648
54.498748	1796.423434	19.856666
54.518029	1794.046666	19.861683
54.788620	1766.501633	19.866701
54.254409	1764.923214	19.871719
54.365638	1763.558402	19.876736
54.380637	1764.798131	19.881754
54.494195	1782.868179	19.886771
54.508207	1777.949738	19.891789
54.880031	1785.827312	19.896807
54.655313	1791.161507	19.901824
54.492836	1792.129046	19.906842
54.461456	1787.416545	19.911859
55.017922	1777.374764	19.916877
54.689861	1793.219102	19.921895
54.571779	1788.793400	19.926912
54.595744	1787.611147	19.931930
54.713783	1801.761532	19.936947
54.925251	1818.190586	19.941965
54.887469	1820.945773	19.946983
55.039443	1813.341449	19.952000
55.126856	1823.823649	19.957018
54.774947	1822.539059	19.962035
55.098393	1822.709991	19.967053
55.146668	1846.886283	19.972071
55.522623	1849.464701	19.977088
55.666592	1842.506580	19.982106
55.567967	1849.422696	19.987123
55.604100	1849.578208	19.992141
55.802559	1850.956862	19.997159
56.013996	1843.514728	20.002176
56.056299	1834.003327	20.007194
56.189816	1839.694764	20.012211
56.360482	1836.938981	20.017229
56.205230	1833.972592	20.022247
56.150804	1834.517907	20.027264
56.278297	1831.794470	20.032282
56.145284	1832.448861	20.037299
56.275058	1834.562125	20.042317
56.280451	1834.410124	20.047335
56.264954	1830.189082	20.052352
55.960599	1825.420584	20.057370
56.023650	1835.182800	20.062387
55.975721	1829.072612	20.067405
55.616264	1841.454432	20.072423
55.864225	1847.244247	20.077440
56.346884	1856.866132	20.082458
56.398291	1866.728722	20.087475
56.775389	1871.725105	20.092493
56.811874	1891.918707	20.097511
56.921631	1889.279301	20.102528
57.050297	1883.185916	20.107546
56.988870	1888.276961	20.112563
57.169442	1885.026214	20.117581
57.292397	1880.728295	20.122599
57.243580	1884.414077	20.127616
57.723797	1884.507477	20.132634
57.125300	1886.231874	20.137651
57.484405	1877.988094	20.142669
57.397492	1880.712449	20.147687
57.427738	1874.798752	20.152704
57.520974	1877.257447	20.157722
57.168860	1876.915029	20.162739
57.356325	1884.268052	20.167757
57.403802	1874.891598	20.172775
57.580126	1873.930179	20.177792
57.927660	1877.159381	20.182810
57.749171	1892.815665	20.187827
57.662170	1899.179475	20.192845
57.818492	1903.330124	20.197863
58.126133	1901.463872	20.202880
58.051757	1895.078505	20.207898
57.931275	1901.301793	20.212915
58.252219	1898.574662	20.217933
58.326165	1903.311401	20.222951
58.399500	1894.303102	20.227968
58.412763	1887.808737	20.232986
58.125468	1895.776604	20.238003
58.436519	1890.498703	20.243021
58.796494	1896.409756	20.248039
58.409770	1900.023142	20.253056
58.612642	1915.930091	20.258074
58.761010	1930.696450	20.263091
59.236789	1930.025216	20.268109
59.195493	1934.595216	20.273127
59.099599	1919.031715	20.278144
59.083205	1896.714389	20.283162
58.851546	1891.187758	20.288179
59.078500	1913.344375	20.293197
59.031087	1914.424369	20.298215
58.925286	1924.076800	20.303232
59.368435	1918.785678	20.308250
59.219145	1927.035442	20.313267
59.273324	1914.678659	20.318285
59.351976	1931.423925	20.323303
59.506591	1920.938736	20.328320
59.741011	1911.054527	20.333338
59.285821	1921.284108	20.338355
59.589936	1924.764609	20.343373
59.698931	1917.701219	20.348391
59.487892	1919.681551	20.353408
59.464337	1912.679088	20.358426
59.454376	1925.265709	20.363443
59.870551	1940.433808	20.368461
59.796045	1939.986367	20.373479
59.960350	1937.943052	20.378496
60.212949	1931.931099	20.383514
60.163462	1940.936014	20.388531
60.295309	1937.522454	20.393549
60.038746	1939.107167	20.398567
60.020060	1940.037521	20.403584
60.257169	1945.055926	20.408602
59.973363	1964.795557	20.413619
60.357731	1967.719854	20.418637
60.571917	1973.981462	20.423655
60.133288	1971.395439	20.428672
60.401568	1971.765277	20.433690
60.222213	1980.594469	20.438707
60.892255	1990.020841	20.443725
61.211643	1991.733037	20.448743
61.210599	1993.680183	20.453760
61.122299	1994.993729	20.458778
61.352110	2000.068479	20.463795
61.337399	1988.436843	20.468813
61.916689	1984.990527	20.473831
61.461173	1983.267554	20.478848
61.644803	1964.226935	20.483866
61.426928	1957.425134	20.488883
61.241119	1956.577214	20.493901
61.592285	1960.853888	20.498919
61.631701	1985.698808	20.503936
61.689908	1982.072622	20.508954
61.486373	1984.001325	20.513971
61.733775	1982.198583	20.518989
61.963251	1988.421050	20.524007
61.741147	1981.486471	20.529024
62.242822	1987.200078	20.534042
62.130215	1994.563860	20.539059
62.153968	1989.398851	20.544077
62.301720	1979.110828	20.549095
62.546718	1982.068834	20.554112
62.356159	1980.920511	20.559130
62.078382	1987.375001	20.564147
62.173985	1974.292004	20.569165
62.319816	1983.339409	20.574183
62.096199	1984.119440	20.579200
62.196328	1987.461286	20.584218
62.367651	2009.713868	20.589235
62.476190	2008.446727	20.594253
62.872429	2009.020581	20.599271
62.573624	2011.931622	20.604288
63.089439	2004.038216	20.609306
62.860189	2012.873719	20.614323
62.800266	2014.886130	20.619341
62.940871	2014.629848	20.624359
62.757980	2012.707397	20.629376
63.119414	2028.063391	20.634394
63.164657	2032.757284	20.639411
62.929048	2034.004276	20.644429
63.090725	2036.108349	20.649447
63.269052	2029.091699	20.654464
63.399422	2024.090919	20.659482
63.328436	2032.020284	20.664499
63.346013	2029.037053	20.669517
63.510006	2048.363660	20.674535
63.780004	2058.735864	20.679552
63.964962	2048.051072	20.684570
63.711259	2056.618201	20.689587
63.795644	2062.127692	20.694605
63.873893	2056.043769	20.699623
63.838239	2059.078574	20.704640
63.951031	2058.704452	20.709658
63.963965	2054.303833	20.714675
64.115460	2064.182261	20.719693
64.330411	2051.750324	20.724711
64.450069	2070.795315	20.729728
64.565495	2073.607465	20.734746
64.581533	2080.929515	20.739763
64.764823	2078.036163	20.744781
64.990089	2077.407189	20.749799
64.588775	2077.111102	20.754816
64.850548	2073.315752	20.759834
65.006326	2076.068464	20.764851
64.969247	2077.275896	20.769869
64.979033	2076.208964	20.774887
65.011636	2078.526545	20.779904
65.398708	2080.878746	20.784922
65.158577	2076.215288	20.789939
64.996855	2075.225574	20.794957
65.250525	2066.326297	20.799975
65.080026	2074.807609	20.804992
65.466667	2069.202556	20.810010
65.233279	2072.979181	20.815027
65.000874	2067.613244	20.820045
65.460222	2080.859710	20.825063
65.432517	2095.932160	20.830080
65.776391	2082.245349	20.835098
66.083942	2092.657816	20.840115
65.968752	2097.711373	20.845133
66.005760	2094.790268	20.850151
65.968278	2093.419734	20.855168
65.920177	2094.901048	20.860186
66.000947	2098.872914	20.865203
66.017478	2094.283887	20.870221
66.260220	2089.185738	20.875239
66.108625	2086.725403	20.880256
66.232103	2092.808372	20.885274
66.594416	2107.482389	20.890291
66.605436	2107.895219	20.895309
66.946989	2107.935202	20.900327
66.676466	2113.753089	20.905344
67.005878	2112.095027	20.910362
67.164378	2107.376187	20.915379
66.887013	2113.513721	20.920397
67.402061	2105.846777	20.925415
67.493810	2098.925536	20.930432
67.576143	2083.146134	20.935450
67.484063	2071.843790	20.940467
67.300023	2074.524022	20.945485
67.312826	2070.003732	20.950503
66.896091	2074.725702	20.955520
67.041159	2070.264617	20.960538
67.318090	2077.475749	20.965555
67.111856	2094.808141	20.970573
67.423535	2092.428978	20.975591
67.154670	2105.143261	20.980608
67.587127	2097.425427	20.985626
67.665126	2095.708990	20.990643
67.925668	2103.035057	20.995661
67.901367	2099.394158	21.000679
67.717305	2110.720739	21.005696
67.938458	2138.177236	21.010714
68.110488	2135.285738	21.015731
67.959774	2144.247293	21.020749
68.156262	2133.164064	21.025767
68.411017	2138.893414	21.030784
67.935129	2139.304971	21.035802
68.102878	2134.447973	21.040819
68.197482	2140.744410	21.045837
68.287918	2144.106005	21.050855
68.130567	2163.122563	21.055872
68.229397	2167.959204	21.060890
68.499624	2163.484456	21.065907
68.370345	2172.500748	21.070925
68.897686	2191.824856	21.075943
68.885430	2202.625795	21.080960
68.806459	2192.829518	21.085978
69.038367	2200.962370	21.090995
68.961869	2199.697897	21.096013
69.363730	2198.794789	21.101031
69.005673	2196.732808	21.106048
69.315872	2199.314693	21.111066
69.362421	2196.450653	21.116083
69.403967	2219.666792	21.121101
69.618482	2220.185308	21.126119
69.970835	2216.948571	21.131136
70.146006	2220.306389	21.136154
70.306133	2216.635714	21.141171
70.190777	2220.343222	21.146189
70.371299	2204.269477	21.151207
70.266724	2195.469995	21.156224
70.146462	2175.670742	21.161242
70.228324	2180.702723	21.166259
69.870050	2176.893472	21.171277
70.339114	2193.780686	21.176295
70.423791	2208.581086	21.181312
70.158920	2202.955506	21.186330
70.627928	2201.906629	21.191347
70.460684	2199.548477	21.196365
70.555610	2196.268538	21.201383
70.178205	2211.078910	21.206400
70.128456	2217.447312	21.211418
70.688509	2224.535649	21.216435
70.496526	2239.883874	21.221453
71.050128	2232.825864	21.226471
71.264623	2237.683141	21.231488
71.065988	2225.791611	21.236506
71.137794	2237.129464	21.241523
71.310976	2242.546361	21.246541
71.592416	2249.157197	21.251559
71.768575	2252.295952	21.256576
71.542679	2247.259992	21.261594
71.859873	2246.108290	21.266611
71.738690	2252.103479	21.271629
71.958568	2244.819605	21.276647
71.879813	2241.072724	21.281664
72.078076	2237.194146	21.286682
71.939752	2232.320469	21.291699
72.017763	2244.783331	21.296717
72.072962	2254.330959	21.301735
71.959298	2252.602143	21.306752
72.214112	2241.346575	21.311770
72.409686	2239.949252	21.316787
72.296458	2251.593354	21.321805
72.128647	2239.404571	21.326823
72.104748	2236.110044	21.331840
72.101110	2252.034995	21.336858
72.627371	2255.789827	21.341875
72.423304	2280.354259	21.346893
72.529518	2276.081052	21.351911
72.081192	2278.889333	21.356928
72.501943	2275.849537	21.361946
73.088967	2278.924207	21.366963
73.111419	2287.852842	21.371981
73.181267	2291.952556	21.376999
73.669918	2294.964380	21.382016
73.350248	2298.360051	21.387034
73.533369	2285.370968	21.392051
73.445129	2288.339325	21.397069
73.532125	2288.464766	21.402087
73.377378	2297.946391	21.407104
73.543886	2303.272284	21.412122
73.835189	2295.103688	21.417139
73.806767	2289.731854	21.422157
73.766797	2287.661290	21.427175
73.891602	2300.513710	21.432192
73.540372	2291.602250	21.437210
73.779779	2300.026052	21.442227
73.784557	2319.785677	21.447245
73.924298	2324.361644	21.452263
74.166659	2325.757878	21.457280
74.120620	2331.607578	21.462298
74.415205	2329.472561	21.467315
74.454386	2334.584890	21.472333
74.689311	2336.086692	21.477351
74.955815	2350.025979	21.482368
74.635385	2348.987323	21.487386
75.039942	2344.975739	21.492403
74.964461	2342.964200	21.497421
75.558800	2347.568061	21.502439
75.596771	2340.160317	21.507456
75.160185	2326.285571	21.512474
75.513637	2317.573971	21.517491
75.734042	2304.874775	21.522509
75.612940	2308.670268	21.527527
75.963020	2302.357374	21.532544
75.294979	2310.473535	21.537562
75.232111	2311.998655	21.542579
75.171096	2317.572864	21.547597
75.763792	2334.713003	21.552615
76.146657	2340.128290	21.557632
75.402011	2341.669440	21.562650
75.626462	2335.598604	21.567667
75.918142	2329.415453	21.572685
75.911215	2332.781399	21.577703
76.229284	2352.005311	21.582720
75.757368	2359.761056	21.587738
76.276771	2360.208230	21.592755
76.548675	2369.477912	21.597773
75.892809	2365.364719	21.602791
76.363867	2363.307176	21.607808
75.930215	2374.489044	21.612826
76.588224	2377.361421	21.617843
76.498955	2386.510983	21.622861
76.706898	2385.358856	21.627879
76.708003	2381.178618	21.632896
76.549869	2391.960925	21.637914
77.124711	2400.915100	21.642931
77.383512	2402.608634	21.647949
77.360669	2410.949927	21.652967
77.684042	2407.788033	21.657984
77.638416	2414.127879	21.663002
77.549564	2406.536367	21.668019
77.674077	2414.412690	21.673037
77.598876	2415.324475	21.678055
77.793873	2408.272217	21.683072
77.598415	2415.636922	21.688090
77.859729	2412.567590	21.693107
77.424048	2413.739464	21.698125
77.552798	2406.424144	21.703143
77.796080	2420.787441	21.708160
77.990466	2424.709081	21.713178
78.204049	2425.221460	21.718195
78.180956	2436.173575	21.723213
78.095784	2431.619005	21.728231
78.173744	2431.882171	21.733248
78.125623	2436.418800	21.738266
78.680573	2450.322625	21.743283
78.400095	2458.276655	21.748301
78.737496	2461.933274	21.753319
78.845564	2452.783462	21.758336
78.586500	2461.783218	21.763354
78.640893	2454.215212	21.768371
79.009876	2458.983592	21.773389
78.764679	2483.018115	21.778407
79.438042	2491.033144	21.783424
79.289498	2486.643390	21.788442
79.448476	2478.824578	21.793459
79.457671	2488.383511	21.798477
79.102109	2486.497071	21.803495
79.437951	2480.875479	21.808512
79.229813	2498.677952	21.813530
80.036308	2509.604187	21.818547
79.855156	2515.225525	21.823565
79.611196	2512.183529	21.828583
79.682395	2509.296846	21.833600
80.085740	2512.243699	21.838618
80.178620	2502.342785	21.843635
80.294465	2516.498516	21.848653
80.595899	2527.926129	21.853671
80.786721	2524.811356	21.858688
80.579774	2529.960958	21.863706
80.964379	2527.175145	21.868723
80.982726	2530.842872	21.873741
81.239033	2524.043024	21.878759
81.236763	2489.091849	21.883776
80.800310	2482.807923	21.888794
81.129048	2499.597833	21.893811
81.058051	2509.766153	21.898829
81.033893	2515.793019	21.903847
81.360353	2508.762652	21.908864
81.124822	2512.405476	21.913882
81.070193	2507.661958	21.918899
81.304003	2506.081499	21.923917
81.390877	2515.329933	21.928935
81.393880	2527.413291	21.933952
81.443084	2548.123780	21.938970
81.654958	2548.201380	21.943987
81.972156	2552.015706	21.949005
81.752789	2549.346425	21.954023
81.578111	2549.463222	21.959040
81.326446	2564.790543	21.964058
81.849059	2575.711069	21.969075
82.223170	2576.548471	21.974093
81.919245	2577.913909	21.979111
82.083767	2587.856266	21.984128
82.368136	2609.834676	21.989146
82.751501	2595.216804	21.994163
82.905566	2598.515597	21.999181
82.955078	2597.707029	22.004199
83.277195	2593.433818	22.009216
82.946607	2605.370882	22.014234
83.213948	2595.254397	22.019251
83.688985	2581.458814	22.024269
83.100366	2590.086016	22.029287
83.504375	2594.113946	22.034304
83.797399	2594.049756	22.039322
83.809955	2595.167508	22.044339
83.532413	2586.060989	22.049357
83.473857	2598.272318	22.054375
83.704345	2583.069494	22.059392
83.601620	2588.039644	22.064410
83.578239	2585.871012	22.069427
83.832501	2588.238195	22.074445
83.413913	2590.601815	22.079463
83.979620	2606.733668	22.084480
83.908410	2615.470112	22.089498
83.910218	2627.767932	22.094515
84.063352	2618.443621	22.099533
84.130743	2636.321111	22.104551
84.541411	2645.733743	22.109568
84.523515	2648.810214	22.114586
84.466826	2659.628669	22.119603
84.486353	2649.865012	22.124621
84.658133	2655.513404	22.129639
84.714937	2658.010148	22.134656
84.795641	2675.335048	22.139674
85.067259	2677.404076	22.144691
85.023616	2680.735227	22.149709
84.865815	2686.695304	22.154727
85.158257	2669.652877	22.159744
85.533878	2698.038790	22.164762
85.540808	2703.056180	22.169779
85.994257	2702.040954	22.174797
85.566301	2706.310212	22.179815
85.869390	2705.195857	22.184832
86.002897	2694.032101	22.189850
86.172919	2692.138934	22.194867
86.032077	2689.626325	22.199885
86.075555	2692.698156	22.204903
86.311392	2687.579302	22.209920
86.592193	2689.136146	22.214938
86.696739	2695.536681	22.219955
86.853475	2688.893022	22.224973
86.547265	2685.414416	22.229991
86.801470	2692.978443	22.235008
86.663341	2683.962177	22.240026
86.489256	2692.900355	22.245043
87.078281	2705.299058	22.250061
86.875755	2715.860182	22.255079
87.082877	2715.493657	22.260096
87.149311	2719.031804	22.265114
87.317227	2712.515426	22.270131
87.439395	2711.356217	22.275149
87.263099	2719.338015	22.280167
87.289219	2715.694923	22.285184
87.471467	2730.527305	22.290202
87.551770	2734.903378	22.295219
87.750719	2733.681450	22.300237
87.492899	2747.317327	22.305255
87.811976	2741.283428	22.310272
87.724068	2750.116812	22.315290
87.953244	2758.282696	22.320307
88.235789	2757.999753	22.325325
88.550909	2767.851538	22.330343
88.312231	2763.167944	22.335360
88.249867	2768.227539	22.340378
88.605659	2761.913123	22.345395
88.969142	2759.576863	22.350413
88.405015	2764.244301	22.355431
88.809547	2754.737723	22.360448
89.050435	2750.903541	22.365466
89.064557	2760.175190	22.370483
89.242907	2764.648432	22.375501
89.163861	2780.787997	22.380519
89.480423	2782.716911	22.385536
89.634490	2782.513905	22.390554
89.705304	2789.465381	22.395571
90.067033	2775.595468	22.400589
89.587361	2764.581613	22.405607
89.593545	2769.612534	22.410624
89.308148	2771.275730	22.415642
89.600017	2780.792766	22.420659
90.261413	2775.265211	22.425677
90.066602	2779.076958	22.430695
89.823958	2775.933503	22.435712
90.062867	2780.840850	22.440730
89.812516	2795.913436	22.445747
90.160757	2798.013105	22.450765
90.222191	2800.358307	22.455783
90.123160	2803.872290	22.460800
90.781833	2820.976453	22.465818
90.563414	2825.784717	22.470835
90.710968	2832.899111	22.475853
90.418631	2835.505662	22.480871
91.095090	2829.330662	22.485888
91.215845	2829.041038	22.490906
91.270652	2835.525462	22.495923
91.580375	2849.257240	22.500941
91.532743	2861.821325	22.505959
91.706713	2860.014106	22.510976
91.776819	2866.765324	22.515994
91.624641	2865.471196	22.521011
91.858853	2858.839049	22.526029
91.669683	2864.308677	22.531047
92.039436	2855.033406	22.536064
92.138681	2852.723952	22.541082
91.732341	2854.841468	22.546099
92.112237	2865.290119	22.551117
92.304743	2878.943291	22.556135
92.319606	2883.743660	22.561152
92.721982	2881.346609	22.566170
92.455079	2882.255118	22.571187
92.894041	2877.221086	22.576205
92.811039	2881.008439	22.581223
93.077982	2880.132753	22.586240
93.043653	2874.931000	22.591258
93.033138	2884.688731	22.596275
93.081334	2891.301056	22.601293
93.111272	2904.524041	22.606311
92.909669	2913.197981	22.611328
93.331910	2900.004611	22.616346
93.380860	2906.432156	22.621363
93.664842	2909.566580	22.626381
93.751528	2929.478391	22.631399
93.702756	2927.338721	22.636416
93.975874	2934.175657	22.641434
93.762040	2944.313180	22.646451
93.895230	2930.927463	22.651469
93.826580	2941.520122	22.656487
94.189430	2952.442561	22.661504
94.644149	2955.758588	22.666522
94.498050	2971.091271	22.671539
94.558727	2961.505267	22.676557
94.809623	2965.486593	22.681575
94.674985	2962.336636	22.686592
94.710072	2961.057956	22.691610
95.186564	2961.853625	22.696627
95.234621	2962.775745	22.701645
94.959514	2962.550479	22.706663
94.953824	2958.776758	22.711680
95.112395	2972.652185	22.716698
94.899783	2990.665031	22.721715
95.230012	2987.055785	22.726733
95.187599	2996.016433	22.731751
95.707112	2992.879829	22.736768
95.932469	2999.033301	22.741786
95.577119	3008.894270	22.746803
96.080542	3013.550004	22.751821
96.031855	3009.526674	22.756839
96.144357	3006.593687	22.761856
96.486545	3006.878870	22.766874
96.342703	3010.494422	22.771891
96.468484	3015.993855	22.776909
96.594286	3009.019718	22.781927
96.322877	3008.930465	22.786944
96.700200	3012.127416	22.791962
96.604267	3035.505734	22.796979
96.668818	3034.406833	22.801997
97.157549	3038.996498	22.807015
96.970494	3035.192545	22.812032
97.166187	3029.190776	22.817050
97.238395	3035.472384	22.822067
97.483647	3046.256865	22.827085
97.539402	3053.860225	22.832103
97.749729	3050.411774	22.837120
97.793704	3050.502609	22.842138
98.030219	3057.778771	22.847155
98.039311	3052.661117	22.852173
98.090716	3061.272774	22.857191
98.078591	3046.672319	22.862208
98.124658	3049.336274	22.867226
98.187928	3050.817350	22.872243
98.361442	3065.025062	22.877261
98.305381	3073.129272	22.882279
98.344674	3080.313677	22.887296
98.931236	3071.624488	22.892314
98.824126	3078.918573	22.897331
98.846607	3076.324917	22.902349
99.106860	3075.391662	22.907367
98.722485	3077.539824	22.912384
99.152577	3090.754202	22.917402
99.432432	3105.420373	22.922419
99.264008	3101.935004	22.927437
99.483092	3098.459894	22.932455
99.481570	3100.492699	22.937472
99.752216	3095.616399	22.942490
99.961138	3110.411260	22.947507
100.139878	3116.543360	22.952525
100.072299	3122.319750	22.957543
100.162894	3130.571773	22.962560
100.430942	3122.616067	22.967578
100.311609	3133.274733	22.972595
100.250142	3125.644081	22.977613
100.432855	3124.162582	22.982631
100.333870	3129.192920	22.987648
100.929848	3114.861442	22.992666
100.462907	3125.820985	22.997683
100.728795	3131.348054	23.002701
100.769123	3138.719341	23.007719
101.021962	3144.397408	23.012736
101.143731	3141.147083	23.017754
100.883775	3142.356454	23.022771
101.259733	3153.220166	23.027789
101.767560	3161.755918	23.032807
101.735865	3171.860282	23.037824
101.426332	3162.049988	23.042842
101.515923	3159.542855	23.047859
101.798907	3174.418437	23.052877
102.149703	3154.820684	23.057895
102.102599	3159.084099	23.062912
102.532572	3159.890632	23.067930
102.229032	3159.181044	23.072947
102.060137	3163.104352	23.077965
102.126581	3171.422213	23.082983
102.208534	3192.769933	23.088000
102.476747	3189.831606	23.093018
102.507923	3198.310060	23.098035
102.443192	3193.868429	23.103053
103.035755	3212.158106	23.108071
102.849452	3225.547100	23.113088
103.085376	3222.405430	23.118106
103.240951	3220.254330	23.123123
103.439364	3220.192811	23.128141
103.818431	3217.102648	23.133159
103.586850	3214.553395	23.138176
103.807447	3227.297798	23.143194
103.770418	3238.305544	23.148211
103.883014	3240.183632	23.153229
104.056807	3238.983157	23.158247
103.934199	3252.367928	23.163264
104.206232	3243.328317	23.168282
104.130246	3238.869637	23.173299
104.250745	3259.400745	23.178317
104.566535	3271.793561	23.183335
104.510292	3272.515228	23.188352
104.330235	3266.229874	23.193370
104.435748	3275.648132	23.198387
104.589300	3280.553234	23.203405
105.137314	3294.253039	23.208423
104.988071	3302.690941	23.213440
105.348292	3296.259031	23.218458
105.809055	3304.181326	23.223475
105.409779	3300.331333	23.228493
105.681313	3294.283832	23.233511
105.498266	3307.840486	23.238528
106.057042	3314.329869	23.243546
105.784545	3320.332406	23.248563
105.898051	3326.576582	23.253581
105.912240	3322.670728	23.258599
105.892843	3322.755125	23.263616
106.315127	3328.366620	23.268634
106.213347	3345.762246	23.273651
106.222704	3348.699682	23.278669
106.645119	3349.009784	23.283687
106.811510	3353.605662	23.288704
106.950067	3341.355448	23.293722
106.841485	3355.656985	23.298739
107.132912	3376.100097	23.303757
107.317043	3364.824714	23.308775
107.328502	3373.509700	23.313792
107.481747	3373.299343	23.318810
107.145565	3364.450134	23.323827
107.215402	3374.010988	23.328845
107.701177	3386.635624	23.333863
107.795585	3398.687591	23.338880
108.183973	3396.485323	23.343898
108.216584	3389.551646	23.348915
107.866821	3391.546464	23.353933
108.318278	3383.591760	23.358951
108.430554	3399.995598	23.363968
108.667001	3390.012079	23.368986
108.530586	3408.199818	23.374003
108.493264	3416.779506	23.379021
108.722806	3415.981646	23.384039
108.637728	3423.701821	23.389056
109.030553	3414.140085	23.394074
109.066880	3417.688495	23.399091
108.981581	3413.459286	23.404109
109.493020	3420.067195	23.409127
109.794868	3427.919003	23.414144
109.786162	3441.155534	23.419162
109.722619	3432.357222	23.424179
109.410703	3436.662980	23.429197
110.134021	3437.928108	23.434215
109.947134	3441.981251	23.439232
110.025720	3435.896735	23.444250
110.130276	3431.298254	23.449267
110.039323	3432.764738	23.454285
110.289536	3446.271042	23.459303
110.296875	3458.327628	23.464320
110.178871	3466.963619	23.469338
110.413252	3467.450148	23.474355
110.318273	3482.354345	23.479373
110.889653	3482.534263	23.484391
110.859380	3499.734340	23.489408
110.946963	3500.755473	23.494426
111.194079	3500.452005	23.499443
111.290506	3526.517255	23.504461
111.653632	3520.009961	23.509479
111.527920	3527.402621	23.514496
111.780112	3527.225492	23.519514
111.949150	3523.991675	23.524531
111.727557	3526.230676	23.529549
112.030643	3524.874505	23.534567
112.201223	3537.966067	23.539584
112.384650	3536.698612	23.544602
112.657089	3532.487318	23.549619
112.328256	3539.764382	23.554637
112.793454	3539.242894	23.559655
112.763701	3533.642477	23.564672
112.813187	3534.960113	23.569690
113.018288	3555.887497	23.574707
113.003466	3572.967365	23.579725
113.543444	3557.251670	23.584743
113.435512	3569.924744	23.589760
113.412191	3563.511339	23.594778
113.624008	3561.024856	23.599795
113.646791	3566.590361	23.604813
113.873835	3561.611675	23.609831
113.726110	3574.118485	23.614848
113.713421	3587.329025	23.619866
114.069041	3587.576560	23.624883
113.910570	3594.670700	23.629901
114.041936	3589.654295	23.634919
114.108985	3607.591230	23.639936
114.394848	3619.574658	23.644954
114.762970	3613.166511	23.649971
114.492033	3621.410137	23.654989
114.719699	3625.379730	23.660007
114.695966	3640.967253	23.665024
115.070825	3649.077199	23.670042
115.204463	3651.307412	23.675059
114.965575	3639.066300	23.680077
115.545503	3658.223273	23.685095
115.586819	3660.595167	23.690112
115.662158	3670.758127	23.695130
116.236318	3672.337380	23.700147
115.958161	3666.631565	23.705165
116.257916	3660.921424	23.710183
116.258561	3668.125885	23.715200
116.045192	3658.693502	23.720218
116.523158	3669.948616	23.725235
116.658240	3683.233603	23.730253
116.862508	3686.289640	23.735271
116.834859	3677.339952	23.740288
117.394375	3684.043178	23.745306
117.563943	3674.270578	23.750323
117.068362	3674.158975	23.755341
117.711826	3665.017070	23.760359
117.760199	3677.276114	23.765376
117.512184	3670.403736	23.770394
117.551341	3672.697238	23.775411
117.333125	3672.200300	23.780429
117.623898	3665.906526	23.785447
117.830188	3675.310704	23.790464
117.825519	3682.590865	23.795482
117.828297	3696.614005	23.800499
118.247211	3710.248927	23.805517
118.322644	3711.977693	23.810535
117.948135	3710.756134	23.815552
117.857316	3730.996819	23.820570
118.384510	3730.684778	23.825587
118.273384	3745.320995	23.830605
118.664722	3752.244640	23.835623
118.678598	3763.489636	23.840640
118.974887	3767.187238	23.845658
119.377330	3761.754588	23.850675
119.379421	3787.665790	23.855693
119.813662	3782.390883	23.860711
119.698954	3787.937492	23.865728
119.765173	3793.736078	23.870746
119.977782	3782.564357	23.875763
119.829874	3786.406775	23.880781
120.077763	3798.033978	23.885799
120.177956	3808.033441	23.890816
120.215829	3816.260299	23.895834
120.590291	3814.940719	23.900851
120.688483	3815.369088	23.905869
120.825064	3810.435226	23.910887
120.748680	3822.681963	23.915904
121.131623	3835.633088	23.920922
120.834738	3834.201789	23.925939
120.674767	3840.528856	23.930957
120.922080	3854.625447	23.935975
121.548474	3859.884400	23.940992
121.522772	3865.211546	23.946010
121.729966	3867.033099	23.951027
121.776869	3879.607550	23.956045
121.941842	3898.657903	23.961063
122.150734	3899.025028	23.966080
122.232370	3902.045891	23.971098
122.725035	3901.107581	23.976115
122.647875	3903.041973	23.981133
122.335544	3900.282320	23.986151
122.777543	3900.973897	23.991168
122.839407	3905.077720	23.996186
122.901940	3921.408439	24.001203
122.974876	3929.156646	24.006221
123.049092	3929.062531	24.011239
123.487067	3931.705460	24.016256
123.302750	3925.142156	24.021274
123.650544	3926.590386	24.026291
123.556812	3945.815931	24.031309
123.865612	3942.376185	24.036327
123.967222	3948.794259	24.041344
123.628376	3943.292908	24.046362
123.988787	3951.628272	24.051379
124.134242	3968.349308	24.056397
124.506931	3962.390727	24.061415
124.649683	3972.999484	24.066432
124.578788	3976.607117	24.071450
124.604630	3971.798248	24.076467
124.641310	3966.838745	24.081485
125.074496	3983.126276	24.086503
125.148986	3994.741776	24.091520
125.186564	4005.812130	24.096538
125.040893	4000.674900	24.101555
125.128327	3997.944335	24.106573
125.504549	4009.768987	24.111591
125.659899	4022.667383	24.116608
125.657852	4022.304748	24.121626
125.716467	4026.387879	24.126643
126.037412	4043.476853	24.131661
126.526054	4044.185128	24.136679
126.328545	4054.892800	24.141696
126.604950	4055.074708	24.146714
126.688378	4045.333465	24.151731
126.772750	4051.071651	24.156749
127.169912	4050.000303	24.161767
127.054271	4053.601974	24.166784
127.019629	4063.220317	24.171802
127.691685	4072.554709	24.176819
127.538044	4078.214182	24.181837
127.511237	4076.920064	24.186855
127.834581	4070.756193	24.191872
127.886603	4072.546364	24.196890
127.955042	4068.605354	24.201907
128.242624	4094.134311	24.206925
128.219685	4098.305776	24.211943
128.475364	4099.744860	24.216960
128.233989	4108.312244	24.221978
128.333479	4100.399309	24.226995
128.785861	4099.740143	24.232013
128.604710	4132.083274	24.237031
128.601197	4128.997605	24.242048
128.929805	4134.164592	24.247066
129.107221	4130.865474	24.252083
129.360108	4145.789098	24.257101
129.340507	4156.071258	24.262119
129.727277	4159.903999	24.267136
129.468776	4167.137024	24.272154
129.681094	4169.825229	24.277171
129.685088	4187.910297	24.282189
129.995305	4180.742878	24.287207
130.088669	4183.071189	24.292224
130.210077	4196.032837	24.297242
130.441453	4207.975336	24.302259
130.550701	4209.209501	24.307277
130.761903	4219.812606	24.312295
131.168077	4207.173259	24.317312
131.062883	4213.288616	24.322330
131.294228	4231.343182	24.327347
131.490925	4245.897401	24.332365
131.515873	4243.560668	24.337383
132.168975	4242.234301	24.342400
131.885409	4249.309281	24.347418
132.226006	4239.035495	24.352435
131.940498	4241.713202	24.357453
132.037562	4241.149083	24.362471
132.210615	4233.296356	24.367488
132.357588	4250.919957	24.372506
132.313355	4257.201646	24.377523
132.045028	4258.736161	24.382541
132.470426	4262.922436	24.387559
132.881099	4279.369148	24.392576
132.600704	4292.328095	24.397594
132.881859	4291.231835	24.402611
133.228592	4289.851444	24.407629
132.849618	4296.460268	24.412647
133.091739	4308.720017	24.417664
133.161648	4322.018699	24.422682
133.537604	4322.469219	24.427699
133.456453	4349.268509	24.432717
134.104465	4358.059715	24.437735
133.939608	4346.084187	24.442752
133.785934	4358.006282	24.447770
134.129804	4369.740483	24.452787
134.391251	4369.153870	24.457805
134.574760	4375.297096	24.462823
134.698478	4374.075689	24.467840
134.844165	4393.492894	24.472858
135.055329	4400.331676	24.477875
135.418825	4406.105687	24.482893
135.225579	4398.851412	24.487911
135.430498	4396.168269	24.492928
135.265521	4419.951095	24.497946
135.747396	4420.422673	24.502963
136.183648	4419.983528	24.507981
136.042905	4431.774380	24.512999
136.407074	4432.224493	24.518016
136.348657	4441.009056	24.523034
136.629277	4451.103884	24.528051
136.870447	4446.626217	24.533069
136.915071	4451.651315	24.538087
137.289027	4446.528716	24.543104
137.129560	4446.483525	24.548122
137.209235	4439.563644	24.553139
137.412530	4454.502861	24.558157
137.287586	4466.286399	24.563175
137.602950	4473.837230	24.568192
137.428724	4487.059913	24.573210
138.011722	4469.458679	24.578227
138.019426	4482.241714	24.583245
137.953732	4499.818898	24.588263
137.893664	4506.956222	24.593280
138.046969	4507.176631	24.598298
138.413809	4521.933690	24.603315
138.525342	4525.457693	24.608333
138.897261	4530.446744	24.613351
139.356805	4533.338223	24.618368
139.303343	4534.774187	24.623386
139.004722	4536.402737	24.628403
139.493853	4556.528782	24.633421
139.721247	4563.197989	24.638439
139.697463	4559.393407	24.643456
139.581125	4566.432180	24.648474
139.874939	4572.179198	24.653491
140.192730	4578.773592	24.658509
140.298598	4592.000395	24.663527
140.665271	4586.435565	24.668544
140.700987	4584.856987	24.673562
140.526315	4583.114776	24.678579
140.775498	4589.638628	24.683597
140.739098	4616.596350	24.688615
140.927860	4625.481066	24.693632
141.078797	4615.892104	24.698650
141.048886	4618.019586	24.703667
141.592265	4637.969794	24.708685
141.580922	4648.819522	24.713703
141.795628	4646.476516	24.718720
141.948041	4647.576774	24.723738
141.874573	4649.966639	24.728755
142.135814	4658.325889	24.733773
142.222966	4677.095527	24.738791
143.018615	4664.075526	24.743808
142.939814	4673.747231	24.748826
142.635562	4676.558060	24.753843
142.971832	4682.764324	24.758861
142.898736	4676.613084	24.763879
143.189613	4667.354536	24.768896
143.387513	4688.724476	24.773914
143.437660	4688.893449	24.778931
143.634726	4689.349183	24.783949
143.305991	4701.173723	24.788967
143.391823	4692.747689	24.793984
143.423767	4713.158328	24.799002
143.833582	4720.736171	24.804019
144.226717	4722.795205	24.809037
144.301528	4747.023176	24.814055
144.457051	4746.603723	24.819072
144.484857	4749.832127	24.824090
144.549999	4763.181588	24.829107
144.778621	4770.393309	24.834125
144.645499	4787.379493	24.839143
144.876333	4779.594109	24.844160
145.512502	4799.536249	24.849178
145.457191	4807.439220	24.854195
145.616298	4803.188468	24.859213
145.554243	4823.543931	24.864231
145.556927	4826.224428	24.869248
145.988071	4834.839167	24.874266
145.994004	4855.732348	24.879283
146.302884	4861.006803	24.884301
145.933338	4869.880129	24.889319
146.647723	4885.240760	24.894336
146.919068	4894.417532	24.899354
147.282315	4886.248682	24.904371
147.626138	4887.884316	24.909389
147.309925	4884.234390	24.914407
147.804517	4898.678468	24.919424
148.015474	4914.313851	24.924442
147.911528	4914.533540	24.929459
148.196817	4908.329965	24.934477
148.015679	4917.012250	24.939495
148.396461	4907.965497	24.944512
148.607422	4914.183148	24.949530
148.382195	4933.183585	24.954547
148.925505	4937.956164	24.959565
148.954587	4945.794828	24.964583
149.376798	4935.089667	24.969600
149.371864	4943.567955	24.974618
149.069692	4939.858987	24.979635
149.615611	4956.161159	24.984653
149.664594	4962.883700	24.989671
149.487111	4963.632210	24.994688
149.614204	4966.566996	24.999706
149.873169	4986.372567	25.004723
150.261427	4981.801092	25.009741
150.065189	4991.818488	25.014759
150.337038	5001.196858	25.019776
150.695187	5011.772234	25.024794
150.567258	5025.351561	25.029811
151.071028	5025.584840	25.034829
150.995212	5026.102301	25.039847
151.126172	5042.964707	25.044864
151.434871	5050.603555	25.049882
151.629392	5045.994042	25.054899
151.808200	5043.652195	25.059917
152.045657	5047.864286	25.064935
151.741169	5068.559480	25.069952
152.064828	5059.756007	25.074970
151.889147	5078.831900	25.079987
152.626515	5068.023282	25.085005
152.446470	5078.072706	25.090023
152.797814	5087.159165	25.095040
152.971855	5105.125776	25.100058
152.943278	5105.707876	25.105075
152.973610	5104.632612	25.110093
153.088304	5110.401607	25.115111
153.427251	5125.348146	25.120128
153.840709	5122.817013	25.125146
153.577475	5128.868317	25.130163
153.911178	5128.946247	25.135181
153.803202	5144.999309	25.140199
154.136140	5146.394987	25.145216
153.996450	5159.760580	25.150234
154.289859	5164.884909	25.155251
154.623129	5180.778324	25.160269
154.925959	5188.702528	25.165287
155.086702	5192.835211	25.170304
155.096344	5186.090414	25.175322
155.037638	5216.048815	25.180339
155.765019	5221.349406	25.185357
155.583036	5212.153072	25.190375
155.667702	5216.192032	25.195392
155.867183	5239.657430	25.200410
155.886960	5235.107507	25.205427
156.020532	5231.584658	25.210445
156.238291	5257.833529	25.215463
156.089525	5265.641151	25.220480
156.769703	5273.857341	25.225498
156.825169	5285.281623	25.230515
157.054318	5295.390243	25.235533
157.230268	5292.601484	25.240551
157.231792	5291.135607	25.245568
157.472863	5303.766475	25.250586
157.367984	5320.231110	25.255603
157.791245	5307.966888	25.260621
158.029216	5323.220165	25.265639
158.005347	5336.773869	25.270656
158.622003	5335.776366	25.275674
158.697095	5339.644461	25.280691
159.329687	5333.495063	25.285709
159.361436	5340.963315	25.290727
159.363262	5339.998291	25.295744
159.093401	5327.674744	25.300762
159.338047	5354.039825	25.305779
159.622670	5361.002333	25.310797
159.820763	5366.632389	25.315815
159.906332	5363.244260	25.320832
160.195020	5369.632732	25.325850
159.942780	5374.649777	25.330867
160.252540	5392.034271	25.335885
160.404840	5396.203060	25.340903
160.939544	5392.534220	25.345920
161.058747	5387.651182	25.350938
160.693002	5404.598568	25.355955
160.708159	5411.358405	25.360973
161.173794	5423.463097	25.365991
161.163680	5420.483017	25.371008
161.200622	5443.381782	25.376026
161.234513	5461.967424	25.381043
161.558449	5456.122683	25.386061
161.900616	5482.493100	25.391079
162.019761	5485.198534	25.396096
162.195602	5483.060314	25.401114
162.365161	5506.716936	25.406131
163.017213	5515.144261	25.411149
162.953671	5509.341595	25.416167
162.798341	5520.385094	25.421184
162.902137	5508.689482	25.426202
163.463628	5540.560500	25.431219
163.280390	5541.867608	25.436237
163.819591	5541.132586	25.441255
163.641857	5536.014337	25.446272
164.114374	5531.322431	25.451290
164.004034	5544.406256	25.456307
164.210528	5553.910766	25.461325
164.673270	5561.318798	25.466343
164.599577	5565.151722	25.471360
164.821911	5562.945150	25.476378
164.665349	5573.297376	25.481395
165.024568	5574.640700	25.486413
165.419991	5585.914408	25.491431
165.021439	5592.238746	25.496448
165.399858	5600.394014	25.501466
165.265586	5617.504934	25.506483
165.665153	5613.564641	25.511501
166.251812	5632.050309	25.516519
166.088387	5647.853940	25.521536
166.526332	5647.522391	25.526554
166.469878	5652.680384	25.531571
166.762781	5654.934926	25.536589
166.932822	5670.529003	25.541607
167.113152	5669.417054	25.546624
167.508690	5661.375567	25.551642
167.289840	5666.527369	25.556659
167.721819	5672.687467	25.561677
167.913028	5689.082992	25.566695
167.793853	5684.273192	25.571712
168.063741	5697.626567	25.576730
168.045977	5692.194306	25.581747
168.258752	5707.667931	25.586765
168.315114	5710.081356	25.591783
168.892951	5731.417380	25.596800
168.970425	5736.789511	25.601818
169.056406	5746.825247	25.606835
168.964286	5743.628700	25.611853
169.515949	5772.071776	25.616871
169.723948	5773.243249	25.621888
170.041128	5767.127787	25.626906
169.868230	5782.437713	25.631923
170.083238	5789.745884	25.636941
170.269024	5803.349554	25.641959
170.331984	5810.130002	25.646976
170.624352	5803.630341	25.651994
170.448235	5821.584065	25.657011
171.009074	5840.759477	25.662029
170.909264	5836.765544	25.667047
170.744226	5862.026540	25.672064
171.003752	5860.768360	25.677082
171.326311	5881.293860	25.682100
172.035906	5894.023277	25.687117
172.017972	5889.326611	25.692135
172.156358	5901.827674	25.697152
172.540198	5908.814957	25.702170
172.278506	5918.071908	25.707188
173.033218	5909.206058	25.712205
173.268475	5918.393343	25.717223
173.082638	5922.982917	25.722240
172.891826	5936.069360	25.727258
173.318991	5951.620361	25.732276
173.538009	5947.752408	25.737293
173.567755	5974.856660	25.742311
173.424436	5985.400718	25.747328
173.860608	5976.453669	25.752346
173.888395	6004.134046	25.757364
174.261519	6004.066050	25.762381
174.424505	6002.276444	25.767399
174.472563	6028.923299	25.772416
174.954201	6036.468626	25.777434
174.821542	6039.954633	25.782452
175.382275	6033.940522	25.787469
175.419767	6043.884446	25.792487
175.512373	6062.718627	25.797504
175.501819	6072.531113	25.802522
175.878038	6076.875673	25.807540
175.891512	6087.304839	25.812557
176.366238	6093.360361	25.817575
176.217569	6106.899942	25.822592
176.544287	6098.000087	25.827610
176.962901	6107.212262	25.832628
177.017436	6116.706037	25.837645
177.339513	6113.404616	25.842663
176.985047	6126.456085	25.847680
177.414047	6136.529798	25.852698
177.569244	6142.395646	25.857716
177.648591	6155.469839	25.862733
178.180201	6169.178826	25.867751
178.128637	6174.423606	25.872768
178.354310	6179.472055	25.877786
178.257627	6197.383124	25.882804
178.724493	6211.688077	25.887821
178.924973	6213.736677	25.892839
178.734967	6228.145662	25.897856
179.000798	6230.277961	25.902874
179.173653	6245.618522	25.907892
179.286416	6260.884770	25.912909
179.711650	6264.385587	25.917927
179.786490	6294.184509	25.922944
180.060469	6295.623136	25.927962
180.438655	6295.566904	25.932980
180.759645	6315.786051	25.937997
180.731742	6328.744243	25.943015
181.068071	6327.318149	25.948032
181.177842	6323.183066	25.953050
181.428088	6343.509263	25.958068
181.556482	6348.979505	25.963085
181.787571	6344.552597	25.968103
181.925119	6358.494752	25.973120
182.429326	6364.114660	25.978138
182.363819	6374.843004	25.983156
182.457745	6378.118293	25.988173
182.884698	6372.164011	25.993191
183.067329	6382.433832	25.998208
183.312006	6401.945819	26.003226
183.264487	6406.325175	26.008244
183.538120	6409.256452	26.013261
183.900877	6396.681627	26.018279
183.918197	6407.827909	26.023296
184.185189	6420.662532	26.028314
184.253461	6429.615473	26.033332
184.273760	6434.971315	26.038349
184.744975	6429.467305	26.043367
184.557877	6446.801315	26.048384
184.758491	6449.774618	26.053402
184.834149	6461.581566	26.058420
185.005436	6473.720832	26.063437
185.265061	6476.653653	26.068455
185.100123	6494.244757	26.073472
185.672940	6500.774115	26.078490
186.071835	6515.641163	26.083508
185.895210	6521.732216	26.088525
186.210305	6529.035188	26.093543
186.045296	6551.360135	26.098560
186.129280	6559.808028	26.103578
186.458219	6568.958129	26.108596
186.679402	6581.145928	26.113613
186.826472	6573.325488	26.118631
187.096576	6598.369905	26.123648
187.281750	6599.685422	26.128666
187.383721	6603.384759	26.133684
187.550238	6625.469042	26.138701
187.797139	6632.206001	26.143719
187.785471	6637.642030	26.148736
188.285310	6652.301096	26.153754
188.480562	6660.053240	26.158772
188.427064	6669.819644	26.163789
188.813445	6684.824399	26.168807
189.127762	6697.783738	26.173824
189.342936	6712.857032	26.178842
189.389332	6718.572548	26.183860
189.389968	6730.741048	26.188877
189.866084	6739.376960	26.193895
190.323316	6742.474821	26.198912
190.605352	6754.875587	26.203930
190.757001	6764.540350	26.208948
190.461848	6784.714015	26.213965
191.221794	6785.915494	26.218983
191.056153	6784.774101	26.224000
191.363950	6804.266682	26.229018
191.618403	6817.924447	26.234036
191.454306	6819.388384	26.239053
192.039804	6826.527793	26.244071
192.432246	6836.990812	26.249088
192.233707	6834.941171	26.254106
192.588213	6838.885466	26.259124
192.406726	6856.164645	26.264141
193.311980	6861.927861	26.269159
193.140829	6861.630175	26.274176
193.222698	6879.672351	26.279194
193.582398	6885.007604	26.284212
193.862208	6891.691179	26.289229
194.062670	6889.964586	26.294247
194.198096	6910.011994	26.299264
194.206879	6914.943776	26.304282
194.849645	6918.318149	26.309300
194.603875	6919.997258	26.314317
194.890305	6926.389103	26.319335
195.137658	6941.076844	26.324352
195.169708	6948.739571	26.329370
195.538700	6949.419759	26.334388
195.411207	6966.119846	26.339405
195.903559	6972.846250	26.344423
195.912896	6990.026244	26.349440
195.853679	7014.997446	26.354458
196.298098	7008.166509	26.359476
196.497538	7026.986514	26.364493
196.834804	7034.722421	26.369511
196.836936	7034.090429	26.374528
196.749971	7053.383221	26.379546
197.277947	7063.436417	26.384564
197.195033	7079.622768	26.389581
197.726692	7086.013465	26.394599
197.905996	7088.580826	26.399616
197.615478	7116.556078	26.404634
198.070987	7113.837301	26.409652
198.381726	7135.756638	26.414669
198.652972	7144.255761	26.419687
198.975942	7140.462472	26.424704
199.204784	7176.504330	26.429722
199.903727	7171.560220	26.434740
199.337234	7188.184340	26.439757
200.053611	7177.415592	26.444775
200.124545	7183.622664	26.449792
200.248272	7195.227643	26.454810
200.526367	7204.048615	26.459828
200.193669	7217.881115	26.464845
200.702941	7215.751273	26.469863
200.526291	7236.221752	26.474880
200.733856	7247.366274	26.479898
200.923187	7251.344319	26.484916
201.025652	7267.236299	26.489933
201.567954	7278.746054	26.494951
201.753358	7295.539623	26.499968
201.607362	7313.135585	26.504986
202.191840	7323.630151	26.510004
201.989020	7342.732947	26.515021
202.467374	7340.531801	26.520039
202.793047	7356.115167	26.525056
202.950199	7371.187665	26.530074
203.471116	7378.877586	26.535092
203.126846	7400.178680	26.540109
203.476284	7391.409042	26.545127
203.887661	7417.435671	26.550144
204.302729	7423.985229	26.555162
204.261190	7422.646801	26.560180
204.513847	7446.558804	26.565197
204.736539	7445.963540	26.570215
205.437630	7452.804469	26.575232
205.064356	7469.204698	26.580250
205.401527	7487.486508	26.585268
205.421881	7495.797346	26.590285
205.831343	7496.321986	26.595303
206.072611	7499.825968	26.600320
206.034556	7514.435455	26.605338
206.368710	7521.649086	26.610356
206.786598	7528.885093	26.615373
206.824592	7535.366360	26.620391
207.113402	7549.356990	26.625408
207.198313	7567.910660	26.630426
207.417447	7567.605066	26.635444
207.432495	7584.752461	26.640461
207.839297	7587.720205	26.645479
208.229960	7596.786641	26.650496
208.306581	7620.398788	26.655514
208.901434	7612.176817	26.660532
208.996703	7630.201085	26.665549
208.885100	7644.358909	26.670567
209.248668	7654.260890	26.675584
208.945635	7664.937262	26.680602
209.475171	7668.696040	26.685620
209.357881	7688.757119	26.690637
210.149128	7704.273996	26.695655
210.419854	7713.591939	26.700672
210.159159	7722.845043	26.705690
210.556625	7729.273971	26.710708
210.618686	7748.294806	26.715725
210.532166	7752.697530	26.720743
210.455724	7775.031585	26.725760
211.022936	7796.251639	26.730778
211.736282	7808.666117	26.735796
211.566535	7821.375668	26.740813
212.129866	7832.840599	26.745831
212.434252	7838.567374	26.750848
212.624229	7847.014948	26.755866
212.938040	7855.542854	26.760884
213.392711	7869.800916	26.765901
213.063970	7868.820353	26.770919
213.515124	7874.520482	26.775936
213.539535	7892.486669	26.780954
213.860582	7898.035047	26.785972
213.639347	7906.231699	26.790989
213.564336	7918.574324	26.796007
214.179268	7926.246587	26.801024
214.259180	7944.398999	26.806042
214.387274	7946.850518	26.811060
214.893396	7960.572372	26.816077
215.103236	7973.246779	26.821095
215.178018	7983.210950	26.826112
215.226577	7999.706525	26.831130
215.691563	8008.560025	26.836148
216.091383	8023.255037	26.841165
215.900136	8042.196057	26.846183
216.362767	8049.832150	26.851200
216.100974	8072.547840	26.856218
216.772790	8076.250081	26.861236
216.943448	8101.047865	26.866253
216.988473	8112.204934	26.871271
217.137625	8119.785822	26.876288
217.610161	8137.000657	26.881306
217.932758	8133.029172	26.886324
217.999820	8167.302458	26.891341
217.785744	8181.085431	26.896359
218.583953	8195.054536	26.901376
218.377516	8218.810528	26.906394
218.726611	8232.475112	26.911412
218.836972	8255.256281	26.916429
218.684132	8271.548367	26.921447
219.776724	8285.794156	26.926464
220.201916	8306.594906	26.931482
220.730857	8295.667386	26.936500
221.202798	8310.766650	26.941517
220.785128	8335.002064	26.946535
221.548095	8332.635514	26.951552
221.356861	8339.895527	26.956570
221.444124	8330.315657	26.961588
221.549284	8354.596106	26.966605
221.789185	8359.087542	26.971623
221.914151	8368.522951	26.976640
221.986345	8383.849944	26.981658
222.694471	8394.190052	26.986676
222.840040	8401.939456	26.991693
223.010447	8423.137018	26.996711
223.076228	8418.969289	27.001728
223.366463	8442.817487	27.006746
223.524844	8450.311929	27.011764
223.866364	8462.860157	27.016781
224.250244	8481.464655	27.021799
224.494193	8466.420964	27.026816
224.539252	8483.435954	27.031834
225.160714	8490.693845	27.036852
225.197086	8497.406581	27.041869
225.021058	8500.935750	27.046887
225.702326	8519.264980	27.051904
225.863443	8532.513499	27.056922
225.732092	8527.093559	27.061940
225.905929	8540.544005	27.066957
226.056176	8554.938152	27.071975
226.240837	8566.196100	27.076992
226.407236	8583.894570	27.082010
226.601143	8601.097737	27.087028
226.928961	8616.379487	27.092045
227.252104	8637.626887	27.097063
227.736076	8650.809456	27.102080
227.613830	8657.450047	27.107098
227.823637	8676.424685	27.112116
228.149567	8683.555917	27.117133
228.172644	8704.028298	27.122151
228.392135	8715.514549	27.127168
228.812033	8733.836089	27.132186
228.825369	8745.282437	27.137204
229.291623	8753.071883	27.142221
229.409838	8768.754784	27.147239
229.804238	8767.128233	27.152256
230.138848	8790.646624	27.157274
229.867746	8801.413782	27.162292
230.390863	8814.362344	27.167309
230.472486	8835.363242	27.172327
231.211750	8839.605147	27.177344
231.043243	8862.219072	27.182362
231.508954	8877.865038	27.187380
231.949878	8876.952368	27.192397
231.893602	8893.621408	27.197415
232.349373	8902.621095	27.202432
232.118450	8920.510963	27.207450
232.622746	8935.806345	27.212468
232.999883	8948.534186	27.217485
233.112273	8952.453708	27.222503
233.141217	8960.845026	27.227520
233.339989	8977.395521	27.232538
233.573769	8994.858778	27.237556
233.882422	9004.718700	27.242573
234.267177	9021.233727	27.247591
234.258708	9032.514520	27.252608
234.402737	9050.117162	27.257626
234.812264	9066.457188	27.262644
235.182804	9083.442570	27.267661
235.401084	9089.435352	27.272679
236.032457	9106.323226	27.277696
235.694281	9124.998368	27.282714
235.908171	9132.055391	27.287732
236.268186	9145.993885	27.292749
236.735242	9158.027944	27.297767
237.181064	9171.745860	27.302784
237.303646	9182.256674	27.307802
237.474205	9180.899532	27.312820
237.774952	9200.033837	27.317837
237.870123	9206.261317	27.322855
238.009151	9218.674287	27.327872
238.337682	9238.338154	27.332890
238.260349	9251.310839	27.337908
238.669067	9265.218530	27.342925
238.692305	9284.173566	27.347943
239.113272	9296.765232	27.352960
239.438692	9307.576574	27.357978
239.685269	9332.005257	27.362996
240.049332	9338.386801	27.368013
240.179347	9355.998401	27.373031
240.515408	9355.320494	27.378048
240.986515	9374.485104	27.383066
241.030801	9389.806650	27.388084
241.642292	9400.453320	27.393101
241.283358	9419.113332	27.398119
241.713565	9422.184693	27.403136
241.742785	9437.664761	27.408154
242.134496	9443.509223	27.413172
242.632700	9455.629735	27.418189
242.580656	9475.940645	27.423207
242.782246	9472.433968	27.428224
243.040359	9505.893063	27.433242
243.382220	9511.919905	27.438260
243.540458	9527.164423	27.443277
243.854865	9537.913144	27.448295
244.366785	9554.323378	27.453312
244.193221	9568.935112	27.458330
244.671970	9589.149637	27.463348
245.075760	9590.593083	27.468365
245.540207	9606.458982	27.473383
245.750855	9602.483612	27.478400
245.680015	9600.504642	27.483418
245.897536	9609.742694	27.488436
246.401168	9618.125894	27.493453
246.510381	9631.503661	27.498471
246.541383	9631.033801	27.503488
246.527010	9646.151019	27.508506
246.918469	9664.208906	27.513524
247.307127	9668.791109	27.518541
247.269289	9694.077285	27.523559
247.750799	9697.670400	27.528576
247.948838	9719.668665	27.533594
247.670225	9729.800351	27.538612
248.299367	9753.973338	27.543629
248.205063	9766.309548	27.548647
248.239757	9788.344399	27.553664
248.967394	9806.811607	27.558682
249.286587	9831.078558	27.563700
249.793164	9836.452736	27.568717
249.626735	9864.513866	27.573735
249.965813	9881.005042	27.578752
250.556734	9881.359507	27.583770
250.636745	9902.266742	27.588788
251.023341	9913.339376	27.593805
250.903972	9931.082698	27.598823
251.602805	9943.557189	27.603840
251.506836	9954.902745	27.608858
252.080845	9974.344108	27.613876
252.384483	9984.829417	27.618893
252.233847	10006.679383	27.623911
252.811752	10013.995608	27.628928
253.224367	10020.299273	27.633946
253.235621	10035.384253	27.638964
253.591413	10047.158512	27.643981
253.977286	10058.857685	27.648999
254.132460	10065.349729	27.654016
254.526211	10082.358328	27.659034
254.445265	10096.961511	27.664052
254.757128	10109.360742	27.669069
255.010444	10128.725385	27.674087
255.195939	10141.804181	27.679104
255.662750	10155.250030	27.684122
255.724777	10166.048828	27.689140
256.210925	10176.860151	27.694157
256.038637	10192.875360	27.699175
257.139387	10198.646854	27.704192
257.472761	10213.746434	27.709210
257.624469	10224.217658	27.714228
258.258028	10231.538165	27.719245
258.329762	10233.378556	27.724263
258.399953	10236.600270	27.729280
258.815256	10235.977756	27.734298
258.649758	10261.339526	27.739316
258.814038	10262.023032	27.744333
259.262897	10272.348198	27.749351
259.643211	10285.464980	27.754368
260.183398	10296.802379	27.759386
259.910800	10299.226834	27.764404
260.111561	10311.377536	27.769421
260.257547	10322.857412	27.774439
260.583416	10341.514644	27.779456
260.817942	10351.842250	27.784474
260.650488	10368.509161	27.789492
261.091393	10394.085899	27.794509
261.399869	10414.830716	27.799527
261.461964	10422.496437	27.804544
261.700563	10432.562645	27.809562
261.618414	10459.362919	27.814580
261.792075	10469.946482	27.819597
262.165968	10486.096897	27.824615
262.194128	10522.189750	27.829632
263.107529	10522.574367	27.834650
263.170573	10557.544361	27.839668
263.285482	10568.216498	27.844685
264.050601	10584.119472	27.849703
264.110044	10603.309574	27.854720
264.247766	10613.426471	27.859738
264.541578	10646.179267	27.864756
265.023356	10658.063905	27.869773
264.958469	10675.791936	27.874791
265.297809	10692.094817	27.879808
265.801250	10711.076043	27.884826
265.563826	10737.790606	27.889844
266.286907	10750.982603	27.894861
266.788632	10776.560123	27.899879
266.693073	10783.119960	27.904896
267.227064	10800.526822	27.909914
267.872691	10820.593947	27.914932
268.090264	10835.708554	27.919949
268.259047	10852.096554	27.924967
268.629814	10858.635959	27.929984
268.858788	10872.762310	27.935002
269.192778	10884.890605	27.940020
269.437691	10895.465805	27.945037
269.633683	10908.633303	27.950055
269.556968	10920.010227	27.955072
270.267910	10930.224679	27.960090
269.872545	10955.133170	27.965108
270.560868	10961.779202	27.970125
270.406852	10975.954857	27.975143
270.670665	11004.041294	27.980160
271.016520	11021.988501	27.985178
271.206402	11043.776413	27.990196
271.561810	11056.351953	27.995213
272.116812	11076.757425	28.000231
272.370817	11104.539967	28.005248
272.837118	11113.723523	28.010266
272.818368	11129.083944	28.015284
273.442937	11142.130269	28.020301
273.686382	11153.982239	28.025319
273.590114	11186.520216	28.030336
274.385809	11180.120234	28.035354
274.019267	11219.623726	28.040372
274.307421	11225.849198	28.045389
274.918302	11245.273392	28.050407
275.184301	11260.000622	28.055424
275.973489	11280.876561	28.060442
276.033557	11294.018023	28.065460
276.230408	11301.585432	28.070477
276.468110	11315.917152	28.075495
276.541958	11337.880668	28.080512
277.033066	11353.884914	28.085530
276.819154	11367.946339	28.090548
277.177320	11382.908973	28.095565
277.685241	11407.134455	28.100583
277.745314	11427.614415	28.105600
277.990033	11438.823467	28.110618
277.887885	11456.634158	28.115636
278.440120	11474.717892	28.120653
279.014720	11500.594928	28.125671
278.988170	11516.915085	28.130688
279.361430	11537.597046	28.135706
279.757535	11563.907130	28.140724
279.965913	11578.765524	28.145741
280.285347	11587.592320	28.150759
280.355595	11602.399537	28.155776
280.818421	11608.418180	28.160794
281.065160	11634.776740	28.165812
281.728921	11648.689982	28.170829
281.974993	11661.849805	28.175847
282.039385	11671.158510	28.180864
282.521854	11691.494825	28.185882
282.317055	11701.160114	28.190900
282.646796	11729.028892	28.195917
282.984109	11734.088205	28.200935
283.438347	11760.477232	28.205952
283.698339	11762.608891	28.210970
283.699533	11798.850877	28.215988
283.973970	11809.596705	28.221005
284.198696	11826.841557	28.226023
284.521509	11859.144479	28.231040
284.844885	11873.509787	28.236058
285.305741	11907.764461	28.241076
285.380278	11928.371877	28.246093
285.723618	11941.553647	28.251111
286.123546	11948.840340	28.256128
286.641542	11975.888893	28.261146
286.590717	11998.488513	28.266164
287.178018	12011.552744	28.271181
287.354089	12037.050642	28.276199
287.584428	12061.925021	28.281216
287.953195	12062.778044	28.286234
288.011644	12102.493836	28.291252
288.688454	12108.494584	28.296269
289.228254	12131.742003	28.301287
289.576358	12159.595875	28.306304
289.983758	12163.559540	28.311322
289.692399	12184.914915	28.316340
289.965841	12199.101251	28.321357
290.481157	12208.989607	28.326375
290.488822	12227.443249	28.331392
291.009449	12249.408113	28.336410
291.121369	12267.034552	28.341428
291.519246	12278.088039	28.346445
292.362543	12310.201702	28.351463
292.321232	12335.791206	28.356480
292.811271	12334.005082	28.361498
292.664443	12353.548148	28.366516
293.186614	12365.198861	28.371533
293.687640	12382.062911	28.376551
293.537539	12403.209238	28.381568
294.085313	12419.670046	28.386586
294.594883	12429.181278	28.391604
294.708047	12439.178888	28.396621
295.413938	12452.100930	28.401639
295.392015	12470.351728	28.406656
295.582183	12473.227824	28.411674
295.735166	12494.278403	28.416692
296.265869	12504.195911	28.421709
296.770793	12517.083506	28.426727
296.832870	12544.123373	28.431744
296.954284	12539.386724	28.436762
297.139664	12564.051841	28.441780
297.445822	12583.463473	28.446797
297.720350	12601.454181	28.451815
297.732216	12635.263088	28.456832
298.300830	12653.545571	28.461850
298.649517	12672.880930	28.466868
298.581352	12696.357438	28.471885
299.129101	12714.317231	28.476903
299.049113	12736.063835	28.481920
299.692528	12750.252453	28.486938
300.066827	12773.906405	28.491956
300.230715	12803.673508	28.496973
300.427685	12804.075932	28.501991
300.606424	12839.290145	28.507008
300.851488	12847.953438	28.512026
301.317350	12867.506022	28.517044
301.203982	12889.201622	28.522061
301.703562	12913.723860	28.527079
302.058872	12943.637614	28.532096
302.558422	12960.064403	28.537114
302.612127	12979.029755	28.542132
302.896196	13005.735794	28.547149
303.552271	13017.374271	28.552167
303.864156	13051.604009	28.557184
304.406522	13057.944131	28.562202
304.792981	13085.229057	28.567220
304.943937	13095.630559	28.572237
305.222072	13112.806475	28.577255
305.388605	13135.540322	28.582272
305.632038	13162.655209	28.587290
305.871630	13177.862913	28.592308
306.316685	13194.467586	28.597325
306.916741	13218.338546	28.602343
306.815491	13240.993938	28.607360
307.124523	13250.329245	28.612378
307.207965	13276.946011	28.617396
307.693991	13304.145481	28.622413
308.188111	13321.798056	28.627431
308.361207	13359.507497	28.632448
308.778371	13369.510520	28.637466
309.028941	13408.338794	28.642484
309.342190	13434.129794	28.647501
309.896627	13444.568751	28.652519
310.096153	13473.377714	28.657536
310.267184	13491.061885	28.662554
310.745100	13509.161770	28.667572
310.972402	13527.032088	28.672589
311.703463	13557.185789	28.677607
311.692074	13570.813713	28.682624
312.201587	13598.860820	28.687642
312.500221	13617.898270	28.692660
312.642035	13631.940589	28.697677
312.955558	13648.862206	28.702695
312.914983	13679.561488	28.707712
313.265287	13704.161633	28.712730
313.936324	13724.656832	28.717748
314.306714	13751.248940	28.722765
314.710665	13760.532582	28.727783
314.802717	13784.332430	28.732800
315.290716	13808.416652	28.737818
315.506891	13824.788777	28.742836
315.708497	13842.633750	28.747853
316.271767	13871.023878	28.752871
315.977522	13897.483523	28.757888
316.682893	13912.452490	28.762906
316.841676	13938.961726	28.767924
317.172366	13967.579639	28.772941
317.671276	13984.407880	28.777959
317.844776	14016.730340	28.782976
318.212188	14038.264358	28.787994
318.345192	14052.407786	28.793012
318.897208	14078.059418	28.798029
319.505736	14094.434643	28.803047
319.192385	14115.335973	28.808064
319.637142	14138.676069	28.813082
319.990541	14169.311060	28.818100
320.697904	14206.842616	28.823117
320.895017	14216.490147	28.828135
321.010104	14236.381394	28.833152
321.464223	14245.704292	28.838170
322.063715	14269.556397	28.843188
321.703468	14300.011877	28.848205
322.273234	14312.683703	28.853223
322.249164	14332.107944	28.858240
322.696379	14358.445611	28.863258
323.064899	14376.083868	28.868276
323.198799	14415.546931	28.873293
323.341584	14429.250919	28.878311
323.861514	14457.384460	28.883328
324.332872	14478.135882	28.888346
324.692566	14504.359032	28.893364
325.071704	14531.152697	28.898381
325.904137	14555.713727	28.903399
325.940447	14575.974619	28.908416
326.274200	14594.868699	28.913434
326.472954	14620.248673	28.918452
326.618114	14642.338804	28.923469
327.322693	14662.730338	28.928487
327.556158	14677.688278	28.933504
328.171000	14702.276086	28.938522
328.604334	14719.163221	28.943540
329.049796	14737.961748	28.948557
329.473750	14765.230665	28.953575
329.582974	14773.088437	28.958592
329.940916	14790.484596	28.963610
330.660454	14795.101768	28.968628
330.501507	14828.008845	28.973645
330.795954	14833.474983	28.978663
331.026315	14856.977677	28.983680
331.036803	14880.584569	28.988698
331.556215	14902.513813	28.993716
331.674685	14940.611048	28.998733
332.431525	14964.910961	29.003751
332.649453	14987.927304	29.008768
332.718903	14999.987403	29.013786
332.963156	15034.391673	29.018804
333.140824	15066.337240	29.023821
333.608889	15083.014105	29.028839
334.104057	15112.297140	29.033856
334.555885	15146.391465	29.038874
335.073613	15166.574981	29.043892
334.827670	15192.640983	29.048909
335.562905	15208.807220	29.053927
335.936858	15244.933677	29.058944
335.939426	15264.887348	29.063962
336.975950	15292.427726	29.068980
337.224551	15311.628314	29.073997
337.611426	15337.766337	29.079015
337.974501	15354.919517	29.084032
338.309013	15376.536395	29.089050
338.529091	15403.974090	29.094068
338.816255	15420.498405	29.099085
339.132508	15433.841951	29.104103
339.229385	15463.612369	29.109120
339.394872	15492.619652	29.114138
339.905210	15505.655304	29.119156
339.912688	15538.298252	29.124173
340.497179	15566.613728	29.129191
341.079952	15602.807284	29.134208
341.091083	15623.365225	29.139226
341.683829	15648.604345	29.144244
341.907568	15672.898970	29.149261
342.046546	15696.711160	29.154279
342.589430	15721.626068	29.159296
342.900020	15747.875093	29.164314
343.317068	15768.411742	29.169332
343.550775	15801.728632	29.174349
344.045458	15819.013406	29.179367
344.401136	15838.132261	29.184384
344.647754	15865.787001	29.189402
345.345584	15885.979423	29.194420
345.244821	15913.297684	29.199437
345.655285	15928.325193	29.204455
346.029960	15948.377302	29.209472
346.136558	15972.373361	29.214490
346.955300	15993.081816	29.219508
346.919054	16019.451725	29.224525
347.232117	16046.917658	29.229543
347.794973	16076.263714	29.234560
347.758399	16099.615333	29.239578
349.212149	16114.607475	29.244596
349.619875	16121.497546	29.249613
350.214487	16134.371585	29.254631
350.664221	16151.419833	29.259648
350.643175	16158.432899	29.264666
351.369680	16167.486414	29.269684
351.313408	16188.573219	29.274701
351.657362	16194.487151	29.279719
351.952978	16210.701919	29.284736
352.153847	16227.337477	29.289754
352.788455	16237.136039	29.294772
352.586780	16250.405191	29.299789
352.754197	16278.428386	29.304807
353.287059	16304.365667	29.309824
353.344233	16334.721133	29.314842
354.119199	16354.396965	29.319860
353.973361	16387.700618	29.324877
354.275147	16414.700883	29.329895
354.578563	16446.741803	29.334912
355.115779	16480.629301	29.339930
355.367150	16512.450404	29.344948
355.508738	16543.668686	29.349965
355.633980	16574.732106	29.354983
355.985439	16600.282162	29.360000
356.268856	16646.174363	29.365018
356.986345	16680.588862	29.370036
357.059709	16721.243369	29.375053
357.575468	16744.840234	29.380071
358.039565	16773.228152	29.385088
358.505503	16796.111394	29.390106
359.247193	16835.889493	29.395124
359.616878	16868.024297	29.400141
359.920343	16889.623076	29.405159
360.156910	16906.663248	29.410176
360.637677	16943.672664	29.415194
361.197106	16958.633899	29.420212
361.400943	16984.688179	29.425229
361.961174	17015.053060	29.430247
362.265989	17035.250462	29.435264
362.645559	17059.609610	29.440282
363.239239	17076.683857	29.445300
363.458336	17104.225422	29.450317
363.676210	17131.223404	29.455335
364.108263	17150.674779	29.460352
364.712967	17183.326165	29.465370
365.030957	17202.102893	29.470388
364.977009	17226.373248	29.475405
365.568415	17246.107324	29.480423
366.179164	17281.590580	29.485440
366.155260	17295.326115	29.490458
366.578391	17318.081599	29.495476
366.899770	17348.503962	29.500493
367.367701	17377.834938	29.505511
367.768389	17398.172974	29.510528
367.703699	17420.503325	29.515546
368.093729	17440.376577	29.520564
368.550048	17466.055640	29.525581
368.682368	17498.074889	29.530599
369.296897	17523.535541	29.535616
369.198591	17555.739672	29.540634
369.552015	17570.210627	29.545652
369.840494	17612.146403	29.550669
370.369315	17647.010300	29.555687
370.661092	17670.850484	29.560704
370.718451	17709.246380	29.565722
371.356963	17738.801983	29.570740
371.540455	17777.330071	29.575757
371.883657	17814.646370	29.580775
372.664708	17848.723313	29.585792
373.039642	17892.125720	29.590810
373.582634	17906.652297	29.595828
373.928242	17935.216302	29.600845
373.990962	17980.669490	29.605863
375.076161	18001.453027	29.610880
375.522216	18035.525892	29.615898
375.708297	18054.161468	29.620916
376.174866	18083.199126	29.625933
376.499058	18114.981297	29.630951
376.824354	18137.423048	29.635968
377.042228	18166.208795	29.640986
377.439421	18200.346835	29.646004
377.940153	18232.431063	29.651021
378.080277	18259.509953	29.656039
378.516319	18285.439562	29.661056
378.940993	18317.571222	29.666074
379.565348	18337.149808	29.671092
380.120342	18372.669846	29.676109
380.073889	18411.142868	29.681127
380.580574	18426.870857	29.686144
380.961402	18464.727836	29.691162
381.490238	18487.640839	29.696180
382.121703	18519.631467	29.701197
382.022067	18541.218707	29.706215
382.746865	18562.177678	29.711232
382.816953	18606.381216	29.716250
383.323523	18634.440536	29.721268
383.453089	18659.948509	29.726285
383.606724	18695.324412	29.731303
384.661353	18725.772977	29.736320
384.619555	18759.269093	29.741338
385.215129	18787.178363	29.746356
385.875702	18828.294178	29.751373
385.876458	18855.475924	29.756391
386.386436	18879.822463	29.761408
386.591654	18913.583847	29.766426
386.966782	18943.002306	29.771444
387.278572	18986.739618	29.776461
387.609356	19010.168525	29.781479
388.552866	19040.926134	29.786496
388.632934	19073.368522	29.791514
389.153839	19096.832300	29.796532
389.524434	19133.768655	29.801549
390.033956	19166.974127	29.806567
390.559927	19181.170416	29.811584
390.793802	19213.225021	29.816602
391.317903	19247.516041	29.821620
391.589075	19272.916381	29.826637
391.817300	19303.945775	29.831655
392.211307	19328.268018	29.836672
392.586817	19374.865089	29.841690
393.148053	19393.328140	29.846708
393.343343	19415.939744	29.851725
393.587189	19444.397051	29.856743
394.006746	19469.801510	29.861760
394.377483	19499.190144	29.866778
394.955981	19538.166146	29.871796
395.220724	19563.088718	29.876813
395.541325	19587.111327	29.881831
396.004807	19621.712693	29.886848
396.128590	19641.777679	29.891866
396.323613	19677.263895	29.896884
397.216805	19704.280406	29.901901
397.537696	19734.100221	29.906919
398.103845	19766.556524	29.911936
398.479107	19788.624884	29.916954
398.702458	19834.884226	29.921972
399.088664	19854.593874	29.926989
399.673606	19893.099814	29.932007
400.324264	19913.697528	29.937024
400.182698	19946.867253	29.942042
400.634005	19984.755423	29.947060
401.501010	20010.897024	29.952077
401.361027	20054.290935	29.957095
402.047256	20075.972394	29.962112
402.522839	20112.721681	29.967130
402.797781	20150.975231	29.972148
403.353965	20172.990506	29.977165
403.839480	20204.924954	29.982183
404.007503	20244.262202	29.987200
404.394747	20274.723141	29.992218
404.988141	20305.247770	29.997236
405.476353	20330.386759	30.002253
405.455389	20380.891324	30.007271
406.158595	20399.888543	30.012288
406.400979	20435.387442	30.017306
406.740821	20466.884541	30.022324
407.210380	20500.318423	30.027341
407.729286	20540.006644	30.032359
408.038522	20562.110598	30.037376
408.512759	20601.725948	30.042394
408.945576	20640.818490	30.047412
409.714085	20670.841807	30.052429
409.779169	20704.912206	30.057447
410.061138	20737.333853	30.062464
410.827490	20765.837791	30.067482
410.922556	20795.394142	30.072500
411.512809	20837.106739	30.077517
411.799252	20874.259509	30.082535
412.434125	20894.075857	30.087552
412.774768	20935.248210	30.092570
412.974210	20972.382484	30.097588
413.239982	21005.221996	30.102605
413.677951	21038.605413	30.107623
414.160791	21079.754587	30.112640
414.681600	21124.265411	30.117658
414.976724	21153.868116	30.122676
415.470232	21188.289571	30.127693
415.865213	21231.840790	30.132711
416.445574	21266.675320	30.137728
417.204187	21293.368212	30.142746
417.255399	21324.172045	30.147764
417.908308	21355.689949	30.152781
418.191346	21396.581266	30.157799
418.895119	21429.986117	30.162816
418.854576	21454.063275	30.167834
419.018927	21488.602884	30.172852
419.690686	21518.418251	30.177869
419.737413	21567.205975	30.182887
420.627922	21598.166264	30.187904
421.071387	21629.167478	30.192922
421.117374	21665.172913	30.197940
421.966380	21693.023006	30.202957
422.408320	21736.249249	30.207975
422.801433	21752.453269	30.212992
422.867481	21782.517557	30.218010
423.330536	21821.882187	30.223028
424.055825	21839.343188	30.228045
424.224090	21882.824806	30.233063
424.981917	21905.649401	30.238080
425.089235	21942.067850	30.243098
425.363030	21979.084809	30.248116
426.003554	22005.763683	30.253133
426.074996	22044.438358	30.258151
426.459789	22083.969498	30.263168
427.063939	22120.537899	30.268186
427.202567	22158.903703	30.273204
427.923052	22198.852597	30.278221
428.077184	22245.694494	30.283239
428.741516	22283.465851	30.288256
429.280150	22308.873811	30.293274
429.534574	22359.430161	30.298292
430.242452	22391.166385	30.303309
430.506765	22424.183918	30.308327
430.917910	22460.884333	30.313344
431.377722	22498.806701	30.318362
431.942440	22534.414348	30.323380
432.241883	22576.223513	30.328397
432.912875	22614.158496	30.333415
433.610963	22638.214442	30.338432
434.133166	22677.514505	30.343450
434.403246	22719.705749	30.348468
434.825088	22744.370495	30.353485
435.177792	22784.285444	30.358503
435.707925	22822.606880	30.363520
436.237343	22866.330854	30.368538
436.366026	22899.480559	30.373556
437.325177	22935.102617	30.378573
437.526136	22961.198184	30.383591
437.786273	23001.042232	30.388608
438.331757	23028.265122	30.393626
438.314453	23068.593612	30.398644
439.285750	23105.809823	30.403661
439.792446	23144.020750	30.408679
440.199089	23180.226744	30.413696
440.414977	23213.756853	30.418714
440.723414	23256.189074	30.423732
441.260575	23284.370930	30.428749
441.605681	23337.099187	30.433767
441.877683	23370.164591	30.438784
442.366413	23412.272483	30.443802
442.677672	23455.870074	30.448820
443.746842	23488.209291	30.453837
443.993025	23530.351305	30.458855
444.492252	23569.991540	30.463872
445.118798	23605.657431	30.468890
445.321089	23643.336387	30.473908
445.835432	23686.932500	30.478925
445.831595	23717.087463	30.483943
446.520828	23749.849594	30.488960
447.351357	23788.155033	30.493978
447.387160	23834.174057	30.498996
448.312831	23858.283958	30.504013
448.822111	23895.819630	30.509031
448.998242	23931.584393	30.514048
449.631506	23970.045887	30.519066
449.848211	24009.071570	30.524084
450.517661	24036.349676	30.529101
450.775918	24076.358974	30.534119
451.202141	24103.721592	30.539136
451.477756	24131.500269	30.544154
451.689236	24171.413449	30.549172
452.236951	24202.042554	30.554189
452.354785	24251.013859	30.559207
453.003127	24285.673022	30.564224
453.610879	24313.579963	30.569242
453.920187	24359.369053	30.574260
454.358422	24401.793680	30.579277
454.640124	24437.460025	30.584295
455.095827	24482.354709	30.589312
455.841553	24519.578224	30.594330
456.314553	24563.527204	30.599348
456.825720	24590.570603	30.604365
457.150122	24644.031747	30.609383
457.512428	24684.182949	30.614400
458.403501	24717.001851	30.619418
458.353332	24760.930672	30.624436
459.335091	24790.151678	30.629453
459.626663	24828.302620	30.634471
459.897465	24872.986060	30.639488
460.844576	24907.880913	30.644506
460.818787	24955.632124	30.649524
461.026636	24996.273270	30.654541
461.434461	25039.565582	30.659559
462.041712	25088.262731	30.664576
462.961251	25129.464562	30.669594
463.276368	25180.068104	30.674612
463.669855	25222.713495	30.679629
464.282658	25249.103975	30.684647
464.376318	25308.661368	30.689664
465.396029	25345.339825	30.694682
465.779881	25388.523433	30.699700
466.450511	25427.862039	30.704717
466.906353	25464.924246	30.709735
467.036584	25501.207703	30.714752
467.719323	25541.869335	30.719770
468.258721	25583.904792	30.724788
468.760553	25613.960483	30.729805
469.421830	25656.619414	30.734823
469.757224	25694.105788	30.739840
469.902007	25737.279364	30.744858
470.496709	25785.696683	30.749876
470.714913	25818.982318	30.754893
471.631424	25871.721599	30.759911
471.937947	25904.680511	30.764928
472.440571	25940.269258	30.769946
473.041654	25986.705191	30.774964
473.413472	26023.851901	30.779981
473.757902	26064.447732	30.784999
473.967990	26110.197972	30.790016
474.614144	26146.066208	30.795034
475.145115	26187.476821	30.800052
475.522765	26237.057423	30.805069
476.061425	26280.731808	30.810087
476.613766	26329.898938	30.815104
477.219630	26365.439936	30.820122
477.190952	26421.406506	30.825140
477.771200	26462.828552	30.830157
478.630564	26493.662529	30.835175
478.863294	26543.006175	30.840192
479.518259	26593.374672	30.845210
479.905700	26623.820120	30.850228
480.198320	26671.794670	30.855245
480.958481	26709.708207	30.860263
481.241775	26764.621153	30.865280
481.855529	26800.063952	30.870298
482.119813	26848.611481	30.875316
482.629474	26892.131333	30.880333
483.390278	26930.367004	30.885351
483.185728	26976.699170	30.890368
483.906389	27000.298547	30.895386
484.292457	27054.264832	30.900404
484.799128	27100.088482	30.905421
485.231963	27142.514445	30.910439
485.528227	27188.341600	30.915456
485.976443	27231.607493	30.920474
486.556236	27281.122936	30.925492
487.157923	27328.007163	30.930509
487.864763	27368.098139	30.935527
488.099870	27418.021165	30.940544
488.759765	27457.779424	30.945562
489.396546	27511.939085	30.950580
489.963169	27560.164127	30.955597
490.712382	27596.349552	30.960615
490.916614	27650.208977	30.965632
491.740412	27687.073108	30.970650
492.086215	27732.048065	30.975668
492.234166	27775.093701	30.980685
492.887029	27811.623599	30.985703
493.119839	27865.677704	30.990720
493.964104	27901.286511	30.995738
494.064558	27951.545659	31.000756
494.716926	27998.590508	31.005773
495.431046	28051.685395	31.010791
495.662463	28100.822322	31.015808
496.538513	28146.492972	31.020826
496.820944	28206.596934	31.025844
497.442893	28248.902820	31.030861
498.128913	28283.674206	31.035879
498.484632	28339.709534	31.040896
499.270842	28386.414657	31.045914
499.337378	28426.992598	31.050932
499.916126	28471.930921	31.055949
500.717764	28520.375273	31.060967
501.020433	28564.059755	31.065984
501.789651	28598.474134	31.071002
502.017267	28660.901180	31.076020
502.733694	28702.716163	31.081037
503.098971	28737.730817	31.086055
503.451545	28798.708554	31.091072
503.915429	28839.899989	31.096090
504.724299	28896.445764	31.101108
504.905239	28936.857681	31.106125
505.545671	28981.269716	31.111143
505.937870	29030.347952	31.116160
506.483579	29070.696666	31.121178
506.986372	29128.262378	31.126196
507.368718	29176.285772	31.131213
507.773566	29217.399529	31.136231
508.408282	29288.077731	31.141248
509.293115	29329.822182	31.146266
509.557775	29379.632354	31.151284
510.231999	29434.435397	31.156301
510.674669	29460.948793	31.161319
511.259340	29527.039509	31.166336
511.823366	29565.408186	31.171354
512.026088	29612.967172	31.176372
512.838137	29667.319064	31.181389
513.218252	29709.469742	31.186407
513.563364	29759.403345	31.191424
513.874009	29805.752412	31.196442
514.544463	29858.620241	31.201460
514.987425	29909.175389	31.206477
515.863661	29960.804263	31.211495
516.059559	30011.356415	31.216512
516.685272	30052.552321	31.221530
517.061454	30103.715381	31.226548
517.684327	30133.228820	31.231565
517.980091	30173.993729	31.236583
518.315579	30232.130264	31.241600
519.108975	30278.492197	31.246618
519.881924	30311.224522	31.251636
520.273034	30360.249868	31.256653
520.766159	30408.226753	31.261671
520.712499	30454.713534	31.266688
521.221385	30505.357297	31.271706
521.692426	30568.249359	31.276724
522.511812	30627.711164	31.281741
522.947422	30664.333459	31.286759
523.221091	30731.556070	31.291776
523.493103	30791.534945	31.296794
524.305788	30848.370349	31.301812
524.929960	30905.704097	31.306829
525.575432	30958.115554	31.311847
525.815269	31021.593338	31.316864
526.635768	31084.360004	31.321882
527.122370	31135.693948	31.326900
527.778821	31188.915168	31.331917
528.674526	31245.375264	31.336935
529.063819	31308.223541	31.341952
529.657709	31351.018004	31.346970
530.004670	31410.200917	31.351988
530.316179	31470.327015	31.357005
531.148235	31520.096689	31.362023
531.832347	31574.292635	31.367040
532.533366	31632.783493	31.372058
533.053873	31674.035310	31.377076
533.206683	31735.854580	31.382093
534.231160	31785.965494	31.387111
534.580068	31836.459693	31.392128
535.168931	31896.017556	31.397146
535.686100	31946.818696	31.402164
536.264500	32006.242980	31.407181
536.767092	32051.149420	31.412199
536.919178	32115.510223	31.417216
537.322885	32160.550052	31.422234
538.371138	32222.658304	31.427252
538.559649	32282.851685	31.432269
538.899823	32329.641099	31.437287
539.686165	32391.805902	31.442304
540.064575	32461.592601	31.447322
540.952012	32505.896931	31.452340
541.263364	32580.049743	31.457357
542.210396	32632.908521	31.462375
542.205152	32691.437687	31.467392
542.764434	32747.081008	31.472410
543.819055	32813.030537	31.477428
543.910394	32878.761031	31.482445
544.722503	32923.675265	31.487463
545.345270	32985.503167	31.492480
545.765930	33042.956395	31.497498
546.418338	33093.306126	31.502516
546.871219	33153.285152	31.507533
547.400673	33209.203077	31.512551
547.709081	33273.444379	31.517568
548.401077	33326.202259	31.522586
549.146129	33382.227058	31.527604
549.380496	33453.256392	31.532621
550.105953	33496.911532	31.537639
550.656810	33551.927632	31.542656
551.130623	33601.803445	31.547674
551.390285	33671.617685	31.552692
551.868758	33735.068834	31.557709
552.830600	33786.697872	31.562727
553.298292	33853.054467	31.567744
553.942109	33899.835633	31.572762
554.787558	33955.413287	31.577780
554.927948	34007.298795	31.582797
555.470564	34059.632289	31.587815
556.174425	34105.662458	31.592832
556.729501	34162.636309	31.597850
557.227491	34217.814683	31.602868
557.742114	34275.306821	31.607885
558.317571	34325.401362	31.612903
558.977214	34395.259543	31.617920
559.688487	34449.276718	31.622938
559.922577	34491.481863	31.627956
560.076131	34560.218896	31.632973
560.893549	34617.210748	31.637991
561.455361	34682.238855	31.643008
561.974394	34738.668226	31.648026
562.911823	34793.469546	31.653044
563.222505	34857.195434	31.658061
563.905032	34910.808491	31.663079
564.389288	34984.273616	31.668096
565.050449	35031.237911	31.673114
565.660402	35095.969207	31.678132
566.341689	35157.716038	31.683149
566.928209	35209.973039	31.688167
567.573035	35273.866036	31.693184
568.059775	35333.026210	31.698202
568.575650	35394.753883	31.703220
568.903883	35453.341042	31.708237
569.945578	35511.308543	31.713255
570.318925	35575.127597	31.718272
570.557767	35638.631437	31.723290
571.411185	35700.187537	31.728308
571.754925	35766.000468	31.733325
572.500517	35830.175434	31.738343
572.896547	35900.266130	31.743360
573.728399	35956.606535	31.748378
574.179255	36015.778043	31.753396
574.761400	36087.827011	31.758413
575.691425	36141.964573	31.763431
576.097617	36204.031931	31.768448
576.223790	36275.891975	31.773466
576.864695	36337.466473	31.778484
577.491971	36404.178504	31.783501
578.259567	36472.328872	31.788519
578.966788	36544.138033	31.793536
579.368822	36607.078567	31.798554
580.312896	36667.006994	31.803572
580.430012	36731.001928	31.808589
581.301215	36798.647169	31.813607
581.977046	36861.887318	31.818624
582.450302	36924.432110	31.823642
583.164699	36978.838261	31.828660
583.594778	37056.095662	31.833677
584.359872	37107.766794	31.838695
584.768467	37174.546250	31.843712
585.428891	37238.917059	31.848730
586.093621	37291.328113	31.853748
586.503845	37361.567305	31.858765
587.175657	37428.051637	31.863783
587.803966	37481.103689	31.868800
588.585482	37549.038014	31.873818
589.229367	37604.575058	31.878836
589.817820	37681.872044	31.883853
590.506686	37728.138051	31.888871
590.930664	37784.116045	31.893888
591.581381	37845.476249	31.898906
592.263783	37889.707854	31.903924
592.402207	37956.951527	31.908941
592.877867	38007.104361	31.913959
593.238183	38060.840042	31.918976
593.282825	38129.072050	31.923994
594.067488	38192.759667	31.929012
595.022729	38261.021432	31.934029
595.488649	38332.344138	31.939047
595.842849	38400.314460	31.944064
596.311300	38466.845699	31.949082
597.352859	38535.214157	31.954100
597.577167	38615.050061	31.959117
598.105571	38682.907386	31.964135
598.826944	38756.771544	31.969152
599.628486	38840.045126	31.974170
600.088687	38895.736443	31.979188
600.556953	38977.768432	31.984205
601.231399	39050.754536	31.989223
602.132328	39127.936500	31.994240
602.303438	39193.992419	31.999258
603.586821	39270.410935	32.004276
603.711423	39337.336831	32.009293
604.785513	39410.409769	32.014311
605.738932	39478.812122	32.019328
606.133684	39554.337133	32.024346
606.500296	39609.780940	32.029364
607.341269	39689.052303	32.034381
607.967832	39760.874853	32.039399
608.492774	39825.712826	32.044416
608.892617	39898.975021	32.049434
609.984758	39961.393100	32.054452
610.515398	40030.568259	32.059469
611.009496	40097.511554	32.064487
611.434912	40159.238784	32.069504
611.954418	40233.290655	32.074522
612.922991	40296.879399	32.079540
613.537572	40373.290041	32.084557
614.043661	40438.401622	32.089575
614.502590	40513.367501	32.094592
615.199817	40598.651985	32.099610
615.724772	40659.029060	32.104628
616.187683	40736.609093	32.109645
617.286250	40807.448447	32.114663
617.883277	40875.602423	32.119680
618.192433	40948.059831	32.124698
618.917176	41027.684507	32.129716
619.785797	41096.050076	32.134733
620.499415	41170.619750	32.139751
621.200608	41240.497333	32.144768
621.770097	41307.994490	32.149786
622.604290	41365.023644	32.154804
622.916091	41427.089609	32.159821
623.261865	41504.887979	32.164839
624.152398	41577.374792	32.169856
624.500909	41654.551398	32.174874
625.087555	41726.315588	32.179892
625.809159	41803.064867	32.184909
626.512992	41880.341483	32.189927
627.534760	41952.438671	32.194944
627.653915	42022.854334	32.199962
628.138538	42086.797659	32.204980
628.629042	42171.116461	32.209997
629.320812	42242.527439	32.215015
630.390601	42317.424817	32.220032
630.674118	42397.728235	32.225050
631.057293	42473.775392	32.230068
631.621269	42560.243326	32.235085
632.583357	42627.443538	32.240103
633.498505	42689.120279	32.245120
633.829562	42751.970476	32.250138
634.127219	42826.542999	32.255156
634.817028	42904.962805	32.260173
635.417641	42967.949100	32.265191
636.456076	43040.647634	32.270208
636.682434	43114.437464	32.275226
637.260800	43194.818669	32.280244
638.036205	43270.153774	32.285261
638.453243	43337.329896	32.290279
639.381399	43419.359166	32.295296
640.013002	43504.551028	32.300314
640.493318	43576.201011	32.305332
641.108275	43655.255197	32.310349
641.689572	43741.463670	32.315367
642.368444	43814.262589	32.320384
642.886191	43902.506227	32.325402
643.793563	43981.178724	32.330420
644.658185	44053.256360	32.335437
644.805860	44144.340928	32.340455
645.833119	44216.303876	32.345472
646.659283	44303.137495	32.350490
647.083820	44375.794376	32.355508
647.518224	44461.989413	32.360525
648.104230	44549.583820	32.365543
649.118787	44623.861758	32.370560
649.956727	44718.327178	32.375578
650.484068	44779.752898	32.380596
651.252598	44862.885314	32.385613
651.861612	44945.728725	32.390631
652.544556	45023.470170	32.395648
653.139488	45110.374188	32.400666
654.019426	45185.412346	32.405684
654.599558	45265.780023	32.410701
655.124355	45338.127210	32.415719
656.002122	45414.871788	32.420736
656.295424	45498.354028	32.425754
656.859259	45576.060616	32.430772
657.485186	45661.162141	32.435789
657.898481	45756.021940	32.440807
658.735068	45834.044450	32.445824
659.445152	45932.812716	32.450842
660.190225	46009.941650	32.455860
661.064266	46101.818632	32.460877
661.454946	46184.864643	32.465895
662.249637	46265.895797	32.470912
662.568069	46369.262625	32.475930
663.247028	46453.436843	32.480948
664.655208	46535.037126	32.485965
664.956788	46618.810299	32.490983
666.095415	46699.420092	32.496000
666.429669	46783.949643	32.501018
667.443626	46866.680789	32.506036
668.070323	46939.159340	32.511053
668.683214	47019.595354	32.516071
669.837084	47103.400198	32.521088
670.092658	47180.867506	32.526106
670.363666	47264.882271	32.531124
671.213064	47342.166733	32.536141
672.011180	47416.005110	32.541159
672.731186	47497.113871	32.546176
673.409404	47584.880754	32.551194
674.110757	47660.008780	32.556212
674.528880	47740.104245	32.561229
674.912365	47835.067772	32.566247
676.009796	47914.179957	32.571264
676.822248	47990.345712	32.576282
677.363283	48077.903853	32.581300
678.054515	48150.306851	32.586317
678.284440	48222.960135	32.591335
678.959262	48293.180942	32.596352
679.529863	48379.175432	32.601370
680.089066	48456.989298	32.606388
681.166971	48536.609443	32.611405
681.493322	48620.842083	32.616423
681.946823	48702.432720	32.621440
682.420576	48793.517223	32.626458
683.263892	48881.398544	32.631476
684.193112	48964.468626	32.636493
684.982888	49062.412449	32.641511
685.907141	49137.815755	32.646528
686.361527	49236.333909	32.651546
687.265169	49315.765032	32.656564
687.909043	49397.399769	32.661581
688.264612	49493.895290	32.666599
689.185819	49565.460201	32.671616
689.831139	49658.683909	32.676634
690.356319	49746.966078	32.681652
691.091433	49836.534145	32.686669
691.802250	49931.864484	32.691687
692.802602	50024.898578	32.696704
693.393462	50113.414759	32.701722
693.999954	50203.703828	32.706740
695.149131	50286.102054	32.711757
695.508361	50383.482636	32.716775
696.225310	50471.954332	32.721792
696.910362	50559.774733	32.726810
697.343542	50651.414832	32.731828
698.084425	50745.581859	32.736845
698.883893	50843.359396	32.741863
699.953154	50924.908109	32.746880
700.480735	51017.772496	32.751898
700.711845	51101.336817	32.756916
702.196106	51195.288300	32.761933
702.663192	51288.732546	32.766951
703.826453	51368.138635	32.771968
704.118345	51466.401267	32.776986
704.840156	51558.617005	32.782004
705.818531	51638.010560	32.787021
706.289598	51728.480746	32.792039
707.034987	51818.609052	32.797056
707.963299	51910.476423	32.802074
708.503708	51998.358842	32.807092
709.508109	52080.940263	32.812109
709.896590	52184.168788	32.817127
710.711121	52262.101034	32.822144
711.160233	52358.004624	32.827162
712.075515	52452.201604	32.832180
712.788492	52537.846709	32.837197
713.236958	52628.975533	32.842215
714.191671	52718.043571	32.847232
715.183203	52812.495022	32.852250
715.435494	52904.832694	32.857268
716.280335	52988.120355	32.862285
716.661846	53088.650753	32.867303
717.598873	53182.133727	32.872320
718.593713	53272.246426	32.877338
719.292539	53377.457971	32.882356
720.027113	53461.814671	32.887373
720.298031	53556.205684	32.892391
720.766456	53645.788005	32.897408
721.515383	53749.236825	32.902426
722.493017	53835.197632	32.907444
723.573359	53926.783955	32.912461
723.898704	54034.790247	32.917479
724.715204	54125.062721	32.922496
725.492918	54198.535441	32.927514
726.155838	54303.119730	32.932532
726.876720	54382.333231	32.937549
727.517344	54478.278675	32.942567
728.356285	54552.033229	32.947584
729.001034	54647.340657	32.952602
729.439728	54745.506969	32.957620
730.046575	54827.957204	32.962637
730.768578	54931.119708	32.967655
731.534388	55027.318804	32.972672
732.442271	55121.864680	32.977690
732.857537	55215.993324	32.982708
733.744850	55314.176707	32.987725
734.399968	55421.832730	32.992743
735.177616	55518.537745	32.997760
735.863582	55621.577110	33.002778
736.554062	55729.791319	33.007796
737.383657	55825.307629	33.012813
738.065138	55935.318978	33.017831
738.632072	56027.214792	33.022848
739.179651	56138.032947	33.027866
740.015954	56256.235005	33.032884
741.169068	56362.651065	33.037901
741.493752	56477.969158	33.042919
742.474787	56582.190572	33.047936
743.385236	56679.195211	33.052954
744.124504	56798.572918	33.057972
744.710013	56903.676596	33.062989
745.419405	57013.885170	33.068007
746.259107	57115.301761	33.073024
747.092545	57225.415152	33.078042
747.873234	57330.103312	33.083060
748.731046	57430.684364	33.088077
749.169471	57549.528618	33.093095
750.437996	57660.703592	33.098112
750.970918	57761.769761	33.103130
751.753658	57877.955418	33.108148
752.721928	57982.401094	33.113165
753.174344	58085.991035	33.118183
754.012878	58183.318189	33.123200
754.873140	58300.738412	33.128218
755.426375	58414.772244	33.133236
756.539250	58515.392373	33.138253
756.924488	58636.710182	33.143271
758.131150	58736.816649	33.148288
758.717140	58843.680953	33.153306
759.114311	58955.733982	33.158324
760.002648	59070.379665	33.163341
761.003065	59170.560317	33.168359
761.801307	59294.088898	33.173376
762.276139	59394.509272	33.178394
762.936315	59509.271020	33.183412
764.051726	59613.820884	33.188429
764.516927	59723.079800	33.193447
765.331017	59840.402846	33.198464
766.198376	59952.295134	33.203482
767.002476	60070.834619	33.208500
767.821665	60172.124619	33.213517
768.724680	60295.199556	33.218535
769.567288	60406.504341	33.223552
770.118848	60512.112768	33.228570
770.841524	60618.717325	33.233588
771.584146	60731.784825	33.238605
772.863951	60842.488772	33.243623
773.043764	60948.552809	33.248640
774.037640	61059.096654	33.253658
774.812388	61168.678709	33.258676
775.679662	61280.944897	33.263693
776.211216	61382.623473	33.268711
776.911574	61489.615499	33.273728
777.918489	61588.290057	33.278746
778.744207	61688.587855	33.283764
779.740313	61787.480061	33.288781
780.270479	61891.765499	33.293799
780.774662	61994.418702	33.298816
781.451181	62092.233832	33.303834
782.204091	62208.215327	33.308852
783.160852	62309.252978	33.313869
783.798549	62410.166916	33.318887
784.487760	62517.924649	33.323904
785.643351	62630.390729	33.328922
786.353639	62748.992856	33.333940
786.873338	62859.725972	33.338957
787.623148	62967.469712	33.343975
788.332533	63083.773068	33.348992
789.459938	63191.095223	33.354010
789.957470	63310.443727	33.359028
790.941812	63426.311626	33.364045
791.886177	63544.614120	33.369063
792.780022	63651.370464	33.374080
793.605890	63762.778397	33.379098
794.144006	63878.804811	33.384116
795.248533	63988.499050	33.389133
795.796367	64107.110552	33.394151
796.503364	64232.055726	33.399168
797.740204	64345.541769	33.404186
798.231187	64470.372390	33.409204
799.076999	64573.392795	33.414221
799.585652	64697.728781	33.419239
800.369997	64817.803423	33.424256
801.751773	64935.365091	33.429274
802.288022	65068.043241	33.434292
803.029570	65178.492854	33.439309
803.866442	65293.820292	33.444327
804.410423	65409.828983	33.449344
805.615175	65533.264598	33.454362
806.151654	65658.568937	33.459380
806.967413	65779.958856	33.464397
807.945040	65898.161759	33.469415
808.693952	66024.571094	33.474432
809.703854	66150.761010	33.479450
810.387726	66273.041709	33.484468
811.317822	66395.048480	33.489485
812.163869	66508.079862	33.494503
812.732121	66644.555952	33.499520
813.548524	66752.851964	33.504538
814.314298	66878.429124	33.509556
815.458171	67003.868630	33.514573
816.056688	67129.595073	33.519591
816.781120	67256.471065	33.524608
817.996451	67363.066757	33.529626
818.379562	67497.808737	33.534644
819.584120	67615.459001	33.539661
820.578707	67738.208928	33.544679
821.210432	67868.284118	33.549696
822.061632	67980.804097	33.554714
822.765969	68108.213292	33.559732
823.539635	68227.354478	33.564749
824.709943	68340.885787	33.569767
825.131900	68465.024448	33.574784
825.998015	68581.654880	33.579802
826.760321	68714.988821	33.584820
827.840661	68832.053079	33.589837
828.627203	68961.205202	33.594855
829.310999	69077.969674	33.599872
830.300853	69192.287795	33.604890
831.175464	69319.404202	33.609908
831.499378	69426.935418	33.614925
832.489979	69541.906553	33.619943
833.150393	69662.402327	33.624960
834.162675	69769.214407	33.629978
834.646683	69892.472211	33.634996
835.536545	70002.928834	33.640013
836.510020	70128.667909	33.645031
837.432476	70250.483133	33.650048
838.303867	70377.094180	33.655066
838.920913	70502.932337	33.660084
839.858473	70621.914349	33.665101
840.387940	70747.306821	33.670119
841.048647	70876.706308	33.675136
841.646185	70989.979673	33.680154
842.830610	71146.427933	33.685172
844.240260	71277.141387	33.690189
844.880791	71397.239156	33.695207
845.561879	71526.715057	33.700224
846.681115	71658.920629	33.705242
847.491394	71785.752420	33.710260
848.133233	71920.074755	33.715277
849.311672	72044.969045	33.720295
850.014158	72180.193579	33.725312
850.774913	72316.712022	33.730330
851.771593	72448.626497	33.735348
852.467858	72573.103991	33.740365
853.253536	72711.138521	33.745383
854.198979	72845.555502	33.750400
855.342459	72977.341401	33.755418
856.205757	73115.093727	33.760436
857.108994	73239.294166	33.765453
858.139565	73371.202307	33.770471
858.540907	73512.631959	33.775488
859.408632	73652.360079	33.780506
860.245727	73786.743864	33.785524
860.999959	73928.098869	33.790541
862.270594	74073.549749	33.795559
862.694254	74213.234729	33.800576
863.883099	74338.722294	33.805594
865.009279	74480.487354	33.810612
865.419625	74614.396567	33.815629
866.730066	74762.893828	33.820647
867.431344	74898.154370	33.825664
868.538662	75030.236898	33.830682
869.348415	75167.985693	33.835700
869.481638	75302.880967	33.840717
870.749958	75443.294223	33.845735
871.613688	75586.140736	33.850752
872.427504	75729.300017	33.855770
873.229185	75873.543776	33.860788
874.083767	76011.201870	33.865805
875.073483	76143.810175	33.870823
876.036627	76298.579937	33.875840
877.151160	76430.403997	33.880858
877.999954	76564.847071	33.885876
879.249493	76701.931810	33.890893
880.166873	76832.804155	33.895911
880.779932	76975.378498	33.900928
881.809753	77108.833503	33.905946
882.845231	77241.902535	33.910964
883.339285	77377.604651	33.915981
884.209903	77508.045930	33.920999
884.589261	77656.140973	33.926016
885.615685	77788.373492	33.931034
886.414816	77940.278445	33.936052
887.602669	78083.422648	33.941069
888.758181	78210.828975	33.946087
889.364868	78348.529858	33.951104
889.835182	78476.000402	33.956122
891.366010	78606.977785	33.961140
892.046836	78739.911958	33.966157
892.911972	78862.790249	33.971175
893.416309	78998.354986	33.976192
894.251164	79134.346637	33.981210
895.020972	79275.056249	33.986228
896.211394	79414.571184	33.991245
897.211376	79551.645063	33.996263
898.085926	79692.523407	34.001280
898.747878	79834.709301	34.006298
899.554828	79984.817543	34.011316
900.491515	80124.859599	34.016333
901.707582	80261.010074	34.021351
902.309671	80414.096656	34.026368
903.065828	80560.326555	34.031386
903.826690	80715.223491	34.036404
904.587009	80868.704497	34.041421
905.659877	81023.507652	34.046439
906.429837	81173.136415	34.051456
906.980949	81331.039267	34.056474
908.349917	81485.347420	34.061492
909.041596	81644.121214	34.066509
910.414986	81796.488521	34.071527
911.065970	81966.121206	34.076544
912.148706	82110.934180	34.081562
913.190976	82269.863113	34.086580
914.145545	82433.280600	34.091597
915.404577	82580.806832	34.096615
916.310440	82735.725112	34.101632
917.099059	82889.392139	34.106650
917.890776	83043.901147	34.111668
918.761853	83201.213525	34.116685
919.766789	83353.057366	34.121703
920.429200	83513.139604	34.126720
921.432281	83666.770017	34.131738
922.635900	83835.907509	34.136756
923.273244	83990.144675	34.141773
924.364628	84145.478303	34.146791
925.048018	84316.451619	34.151808
925.903387	84465.967455	34.156826
927.502655	84638.246945	34.161844
928.013025	84804.544978	34.166861
929.193169	84959.154382	34.171879
930.159100	85120.507275	34.176896
930.970637	85270.668267	34.181914
932.136700	85439.994483	34.186932
932.712866	85600.497660	34.191949
934.305747	85749.298654	34.196967
935.061868	85906.743270	34.201984
935.598073	86066.889250	34.207002
936.638309	86224.105512	34.212020
937.610369	86392.521541	34.217037
938.481541	86538.567768	34.222055
939.367833	86718.871232	34.227072
940.401961	86866.544112	34.232090
941.714313	87033.908656	34.237108
942.547324	87202.859707	34.242125
943.431371	87351.971577	34.247143
944.186122	87511.648280	34.252160
945.067285	87672.520148	34.257178
945.749417	87831.926254	34.262196
946.697530	88004.572276	34.267213
947.995501	88174.491194	34.272231
948.823479	88336.053476	34.277248
949.736199	88492.046594	34.282266
950.845210	88658.412071	34.287284
951.545752	88819.391185	34.292301
952.834400	88973.838125	34.297319
953.292857	89126.664029	34.302336
954.005229	89282.885304	34.307354
954.944406	89431.874533	34.312372
955.978569	89591.848073	34.317389
956.890343	89750.305061	34.322407
957.636446	89922.713581	34.327424
958.601546	90090.106420	34.332442
959.951531	90258.183576	34.337460
960.446228	90425.890701	34.342477
961.105493	90587.027746	34.347495
962.865799	90764.673106	34.352512
963.305326	90934.127008	34.357530
963.983231	91110.017235	34.362548
964.805024	91293.441819	34.367565
965.990871	91462.389940	34.372583
967.217888	91648.509687	34.377600
967.967803	91827.494491	34.382618
969.403197	91997.550658	34.387636
970.464636	92184.587985	34.392653
970.969518	92358.332273	34.397671
972.183184	92542.296446	34.402688
972.999583	92726.910002	34.407706
974.596008	92900.015610	34.412724
974.977892	93087.431734	34.417741
976.394122	93256.639041	34.422759
977.383688	93436.868264	34.427776
977.921697	93623.566415	34.432794
979.368642	93783.885467	34.437812
980.227569	93978.698545	34.442829
981.378310	94149.709246	34.447847
982.403867	94327.660330	34.452864
983.343798	94510.988255	34.457882
984.462152	94688.768353	34.462900
985.429100	94871.436175	34.467917
986.540291	95053.518124	34.472935
987.522673	95234.635222	34.477952
988.225609	95425.548207	34.482970
989.605947	95595.682711	34.487988
990.237434	95783.723715	34.493005
991.993973	95953.564247	34.498023
992.597898	96132.060111	34.503040
993.473543	96313.215373	34.508058
994.839694	96486.555128	34.513076
995.833086	96664.389013	34.518093
997.091335	96833.083494	34.523111
998.001362	97008.217839	34.528128
999.230269	97182.503031	34.533146
1000.418263	97344.932671	34.538164
1000.979034	97528.643039	34.543181
1001.796770	97692.161706	34.548199
1003.188025	97860.942393	34.553216
1004.391491	98051.305184	34.558234
1005.479832	98212.731316	34.563252
1006.393282	98384.285101	34.568269
1007.363333	98553.576894	34.573287
1008.613386	98724.653161	34.578304
1009.279929	98898.770970	34.583322
1010.464367	99064.225807	34.588340
1011.334517	99239.679787	34.593357
1012.347023	99411.743291	34.598375
1013.425740	99572.362958	34.603392
1014.064247	99736.063737	34.608410
1015.182031	99909.290794	34.613428
1015.799331	100103.931845	34.618445
1016.980987	100274.725939	34.623463
1018.053970	100443.443460	34.628480
1018.881306	100616.546051	34.633498
1019.935672	100773.631705	34.638516
1020.853686	100953.008696	34.643533
1022.027291	101111.197371	34.648551
1022.887444	101280.170852	34.653568
1023.751893	101446.491785	34.658586
1025.146489	101618.063717	34.663604
1025.600112	101791.432280	34.668621
1026.655634	101965.126712	34.673639
1027.833163	102139.498633	34.678656
1028.659495	102328.005437	34.683674
1029.902671	102500.874624	34.688692
1030.745359	102697.986417	34.693709
1031.836636	102877.481081	34.698727
1033.117248	103047.732617	34.703744
1033.433139	103237.799433	34.708762
1034.682207	103422.096777	34.713780
1035.496551	103623.133482	34.718797
1036.562965	103807.628379	34.723815
1037.368109	104001.767433	34.728832
1038.392811	104194.858457	34.733850
1039.308508	104399.025162	34.738868
1040.247917	104598.718875	34.743885
1041.389244	104802.040857	34.748903
1042.952932	105005.725183	34.753920
1043.990642	105211.334476	34.758938
1045.310815	105408.362365	34.763956
1046.084099	105601.517924	34.768973
1046.984974	105806.077915	34.773991
1048.325031	105999.813928	34.779008
1049.096482	106206.361540	34.784026
1050.399153	106405.590860	34.789044
1051.409005	106611.937547	34.794061
1052.445440	106814.760341	34.799079
1053.965012	107009.575942	34.804096
1054.650985	107219.413326	34.809114
1056.003747	107408.445719	34.814132
1057.089515	107627.466440	34.819149
1057.902741	107821.176103	34.824167
1059.096851	108021.030709	34.829184
1059.967841	108226.716131	34.834202
1061.260545	108427.317437	34.839220
1062.516711	108626.013609	34.844237
1063.676066	108829.565946	34.849255
1064.884822	109039.394403	34.854272
1065.774072	109236.965037	34.859290
1066.932305	109434.796644	34.864308
1068.187838	109635.729718	34.869325
1068.834011	109833.053525	34.874343
1070.338941	110025.359866	34.879360
1071.367621	110235.569334	34.884378
1072.599237	110416.155596	34.889396
1073.411421	110624.579728	34.894413
1074.541287	110835.397783	34.899431
1075.733400	111023.164485	34.904448
1076.761739	111223.842757	34.909466
1077.778608	111430.275640	34.914484
1078.879978	111620.937047	34.919501
1079.447867	111835.694089	34.924519
1080.725820	112022.883341	34.929536
1081.791763	112238.612630	34.934554
1082.968649	112449.941981	34.939572
1083.983768	112649.707992	34.944589
1085.028286	112863.596076	34.949607
1086.243867	113060.709493	34.954624
1087.084795	113265.664883	34.959642
1088.187406	113467.474636	34.964660
1089.406703	113680.263228	34.969677
1090.175682	113878.153041	34.974695
1091.443646	114069.867890	34.979712
1092.244308	114271.847378	34.984730
1093.107518	114464.924101	34.989748
1094.786766	114667.762056	34.994765
1095.596179	114862.611448	34.999783
1096.667673	115059.268618	35.004800
1097.691616	115268.845432	35.009818
1098.836780	115468.255258	35.014836
1099.635249	115680.925813	35.019853
1100.613081	115886.815212	35.024871
1101.774167	116094.715685	35.029888
1102.735662	116324.177273	35.034906
1103.989823	116527.985726	35.039924
1104.964793	116743.954641	35.044941
1106.383246	116971.229932	35.049959
1107.423903	117175.813181	35.054976
1108.567662	117394.483260	35.059994
1109.559218	117610.088505	35.065012
1110.755482	117836.305019	35.070029
1111.855192	118064.135806	35.075047
1113.270107	118267.663936	35.080064
1113.920762	118497.130908	35.085082
1115.198838	118717.258652	35.090100
1116.473941	118946.562588	35.095117
1117.483323	119170.957739	35.100135
1118.568579	119397.736991	35.105152
1119.383421	119631.443395	35.110170
1120.611451	119854.439121	35.115188
1122.182939	120086.034612	35.120205
1122.742317	120321.043263	35.125223
1124.316979	120540.400751	35.130240
1125.598624	120776.611529	35.135258
1127.078800	121002.172070	35.140276
1127.976040	121228.692420	35.145293
1129.290532	121454.511907	35.150311
1130.656020	121676.041384	35.155328
1131.231845	121902.239845	35.160346
1132.493195	122124.829037	35.165364
1134.021131	122357.754833	35.170381
1134.796281	122587.372545	35.175399
1135.872085	122812.785582	35.180416
1137.250124	123055.525140	35.185434
1138.088030	123289.053842	35.190452
1139.518021	123508.976771	35.195469
1140.531067	123741.719641	35.200487
1141.787787	123969.202560	35.205504
1142.855791	124207.478244	35.210522
1144.312233	124432.587028	35.215540
1144.909825	124659.613789	35.220557
1146.245533	124901.526068	35.225575
1147.438441	125136.189030	35.230592
1148.492799	125365.186058	35.235610
1149.831237	125592.097308	35.240628
1151.035419	125838.943666	35.245645
1151.986783	126077.696880	35.250663
1153.316778	126310.787259	35.255680
1154.424488	126553.257287	35.260698
1155.659537	126784.541820	35.265716
1156.567128	127010.596860	35.270733
1157.971263	127253.517708	35.275751
1159.394556	127476.905244	35.280768
1160.549261	127713.267302	35.285786
1161.408158	127944.914217	35.290804
1162.646661	128175.232585	35.295821
1163.747957	128410.353923	35.300839
1164.693671	128632.675257	35.305856
1165.875942	128871.411840	35.310874
1166.836961	129096.738030	35.315892
1168.295647	129319.537166	35.320909
1169.480122	129542.776159	35.325927
1170.877806	129762.026627	35.330944
1171.833857	129983.050199	35.335962
1172.969957	130209.863846	35.340980
1174.208824	130428.625477	35.345997
1175.105649	130658.334013	35.351015
1176.343983	130879.215763	35.356032
1177.443854	131117.463222	35.361050
1178.408486	131350.043079	35.366068
1179.824398	131590.701065	35.371085
1180.791130	131817.313309	35.376103
1182.126379	132058.748744	35.381120
1183.141295	132293.228649	35.386138
1184.327714	132533.944321	35.391156
1185.790790	132763.688454	35.396173
1186.602504	133012.392779	35.401191
1187.915379	133254.893071	35.406208
1188.894827	133503.915726	35.411226
1190.359368	133753.912328	35.416244
1191.134488	133997.483214	35.421261
1191.832940	134251.641716	35.426279
1193.226573	134502.010744	35.431296
1194.549947	134764.830228	35.436314
1195.870238	135018.929924	35.441332
1197.255909	135277.889130	35.446349
1198.448646	135528.324541	35.451367
1200.072900	135779.299074	35.456384
1201.278000	136035.530220	35.461402
1202.653829	136285.471996	35.466420
1204.022354	136541.844854	35.471437
1205.044882	136790.492225	35.476455
1206.549398	137043.930389	35.481472
1207.932479	137301.029356	35.486490
1208.637933	137553.310222	35.491508
1210.147153	137789.319798	35.496525
1211.373105	138048.618562	35.501543
1212.774630	138296.555132	35.506560
1213.937653	138543.226982	35.511578
1215.002453	138794.912523	35.516596
1216.303523	139051.442458	35.521613
1217.664307	139305.289076	35.526631
1219.038552	139549.118458	35.531648
1219.978371	139810.823707	35.536666
1220.597288	140068.640575	35.541684
1222.485592	140320.974717	35.546701
1223.428523	140582.178136	35.551719
1224.479195	140842.934601	35.556736
1225.915006	141097.022993	35.561754
1226.977510	141356.424593	35.566772
1228.518891	141617.803199	35.571789
1229.299130	141893.232746	35.576807
1230.858835	142144.556659	35.581824
1232.252194	142405.318929	35.586842
1232.968058	142663.392677	35.591860
1234.608993	142919.882480	35.596877
1235.612041	143191.886942	35.601895
1236.691745	143452.087459	35.606912
1238.140777	143719.583906	35.611930
1239.226308	143984.238453	35.616948
1241.012654	144243.719287	35.621965
1241.921886	144513.771119	35.626983
1243.142829	144775.784116	35.632000
1244.368978	145029.846807	35.637018
1245.717456	145286.845914	35.642036
1247.008719	145566.379178	35.647053
1248.026700	145817.666490	35.652071
1249.016787	146065.929172	35.657088
1250.460926	146325.608454	35.662106
1251.552466	146582.912903	35.667124
1253.271441	146815.943127	35.672141
1254.108024	147077.719317	35.677159
1255.545075	147330.304847	35.682176
1256.640586	147578.040446	35.687194
1257.945018	147849.421575	35.692212
1259.131812	148091.095954	35.697229
1260.149200	148356.833750	35.702247
1261.552673	148620.302827	35.707264
1262.578499	148876.175702	35.712282
1263.725857	149143.762058	35.717300
1265.078701	149417.404276	35.722317
1266.318958	149691.029061	35.727335
1267.168971	149963.591535	35.732352
1268.820010	150243.443388	35.737370
1270.040551	150528.036008	35.742388
1271.148321	150797.619356	35.747405
1272.471090	151075.083712	35.752423
1273.789802	151355.582196	35.757440
1275.208149	151646.048493	35.762458
1276.253597	151929.868820	35.767476
1277.564462	152213.634703	35.772493
1278.800966	152501.714911	35.777511
1280.147264	152784.933750	35.782528
1281.379661	153079.031301	35.787546
1282.704681	153369.221660	35.792564
1284.046688	153666.793791	35.797581
1285.489687	153953.810578	35.802599
1286.689040	154248.556698	35.807616
1288.167762	154524.472646	35.812634
1289.559959	154826.662614	35.817652
1291.239187	155115.094970	35.822669
1292.209983	155409.494362	35.827687
1293.801561	155699.213991	35.832704
1295.133171	155979.198349	35.837722
1296.224271	156271.859072	35.842740
1297.657439	156556.727272	35.847757
1298.965611	156850.827885	35.852775
1300.447655	157140.664911	35.857792
1301.826297	157426.740768	35.862810
1302.971785	157725.581089	35.867828
1304.442882	158007.763921	35.872845
1305.886948	158289.103224	35.877863
1307.051024	158584.420098	35.882880
1308.082175	158867.861426	35.887898
1309.390650	159175.312093	35.892916
1310.926410	159461.833026	35.897933
1312.358717	159766.514713	35.902951
1313.826188	160053.939109	35.907968
1314.836136	160339.652302	35.912986
1316.241836	160627.775970	35.918004
1317.986524	160911.202233	35.923021
1318.992227	161199.979563	35.928039
1320.117605	161500.944005	35.933056
1322.117213	161789.104402	35.938074
1323.504432	162091.679123	35.943092
1324.547796	162359.498976	35.948109
1326.209657	162651.045143	35.953127
1327.235237	162940.135607	35.958144
1328.511404	163229.110494	35.963162
1329.921063	163510.160895	35.968180
1331.377473	163794.009392	35.973197
1332.617968	164073.442040	35.978215
1333.518513	164359.822186	35.983232
1334.888874	164657.494980	35.988250
1336.206595	164948.834501	35.993268
1337.729259	165217.988665	35.998285
1339.015529	165484.328715	36.003303
1340.395571	165765.246392	36.008320
1341.451720	166036.956903	36.013338
1342.597467	166320.644843	36.018356
1344.177808	166599.720298	36.023373
1345.351705	166881.097873	36.028391
1346.378353	167176.268768	36.033408
1348.064959	167451.005174	36.038426
1348.942695	167738.591148	36.043444
1350.567411	168023.758826	36.048461
1351.578963	168320.805028	36.053479
1353.315058	168617.302017	36.058496
1354.424366	168906.760535	36.063514
1355.668694	169211.565252	36.068532
1357.163210	169505.519355	36.073549
1358.424653	169800.947768	36.078567
1359.549234	170115.434934	36.083584
1361.117294	170413.887470	36.088602
1362.438672	170728.358980	36.093620
1363.729580	171031.264610	36.098637
1364.944072	171344.831604	36.103655
1365.999208	171659.886376	36.108672
1367.415991	171973.639880	36.113690
1369.003902	172299.181664	36.118708
1370.359909	172611.058632	36.123725
1372.046277	172928.707882	36.128743
1373.713647	173258.291313	36.133760
1375.141210	173576.127241	36.138778
1376.179235	173889.016899	36.143796
1377.652846	174210.034728	36.148813
1379.322217	174532.748273	36.153831
1380.280398	174859.947115	36.158848
1381.972707	175168.574349	36.163866
1383.408655	175488.147401	36.168884
1384.606048	175814.665866	36.173901
1386.219509	176140.178597	36.178919
1387.285414	176468.398339	36.183936
1388.746945	176789.891960	36.188954
1390.219711	177122.160748	36.193972
1391.699160	177450.800890	36.198989
1393.235007	177777.783965	36.204007
1394.416721	178099.814502	36.209024
1396.009146	178427.465084	36.214042
1397.166439	178769.328298	36.219060
1398.493016	179095.669088	36.224077
1400.036236	179420.922726	36.229095
1401.627946	179759.243163	36.234112
1403.123391	180087.389980	36.239130
1404.054799	180422.980837	36.244148
1405.859044	180753.035415	36.249165
1407.705557	181077.170465	36.254183
1408.606679	181410.297648	36.259200
1410.441644	181736.748680	36.264218
1411.740011	182072.378264	36.269236
1413.230146	182396.072578	36.274253
1414.808596	182721.747013	36.279271
1415.976858	183054.637243	36.284288
1417.550202	183383.451642	36.289306
1419.090064	183712.425882	36.294324
1420.444511	184040.404613	36.299341
1421.877438	184365.364079	36.304359
1423.112363	184704.371447	36.309376
1424.699648	185028.890446	36.314394
1426.285385	185363.743966	36.319412
1427.585200	185682.614983	36.324429
1429.341758	186009.345763	36.329447
1430.266796	186340.163537	36.334464
1431.879144	186652.565480	36.339482
1433.351193	186964.306868	36.344500
1434.758652	187268.469771	36.349517
1435.873794	187575.399072	36.354535
1437.089788	187901.950797	36.359552
1438.841757	188205.858634	36.364570
1440.337195	188533.662535	36.369588
1441.480617	188848.718099	36.374605
1443.046123	189157.053873	36.379623
1443.954511	189497.768595	36.384640
1445.548774	189807.169336	36.389658
1446.830935	190147.077069	36.394676
1448.331908	190481.263471	36.399693
1449.788668	190813.097862	36.404711
1451.088072	191143.830266	36.409728
1452.400627	191491.370034	36.414746
1453.971478	191826.377491	36.419764
1454.909040	192173.234119	36.424781
1456.634397	192517.880573	36.429799
1457.920494	192876.273989	36.434816
1459.266307	193222.827848	36.439834
1460.558753	193588.371610	36.444852
1462.191368	193941.737409	36.449869
1464.344588	194297.456651	36.454887
1465.327335	194668.021673	36.459904
1466.904587	195023.395806	36.464922
1468.533618	195388.297634	36.469940
1469.980763	195739.088767	36.474957
1471.537599	196106.494893	36.479975
1472.762117	196460.399029	36.484992
1474.184134	196831.233934	36.490010
1475.943494	197197.558953	36.495028
1477.421409	197551.198537	36.500045
1478.797507	197923.672194	36.505063
1480.194822	198293.300502	36.510080
1481.998548	198659.486519	36.515098
1483.650051	199034.231468	36.520116
1485.297595	199388.779445	36.525133
1486.689356	199757.794480	36.530151
1488.303203	200134.113271	36.535168
1490.065982	200491.225201	36.540186
1491.256434	200858.793836	36.545204
1492.912765	201232.203997	36.550221
1494.703880	201585.850617	36.555239
1496.370487	201962.195815	36.560256
1497.631186	202320.415617	36.565274
1499.455684	202683.889387	36.570292
1500.636281	203036.691718	36.575309
1502.438948	203405.124451	36.580327
1503.946398	203761.875779	36.585344
1505.486580	204119.702658	36.590362
1507.017911	204492.654965	36.595380
1508.533050	204853.219351	36.600397
1510.086629	205205.246558	36.605415
1511.542127	205569.315923	36.610432
1512.979883	205930.240999	36.615450
1514.321990	206291.932705	36.620468
1515.858401	206661.161673	36.625485
1517.324184	207017.224013	36.630503
1519.049583	207395.364251	36.635520
1520.840992	207749.395250	36.640538
1522.060961	208113.616892	36.645556
1523.524058	208475.298547	36.650573
1525.159339	208844.622837	36.655591
1526.465418	209212.809581	36.660608
1528.173991	209574.353938	36.665626
1529.420407	209935.481001	36.670644
1531.256146	210290.721948	36.675661
1532.693614	210647.833317	36.680679
1533.888860	210991.323006	36.685696
1535.361112	211343.149109	36.690714
1536.901227	211699.562195	36.695732
1538.605718	212049.702022	36.700749
1540.227203	212393.609377	36.705767
1541.275491	212751.707985	36.710784
1542.772976	213106.102064	36.715802
1544.530715	213463.527579	36.720820
1546.085220	213832.010419	36.725837
1547.702694	214187.760353	36.730855
1548.803598	214569.680022	36.735872
1550.460832	214934.162930	36.740890
1551.931656	215298.322491	36.745908
1553.093216	215679.855708	36.750925
1554.869475	216053.441011	36.755943
1555.996136	216431.757487	36.760960
1557.395499	216821.713416	36.765978
1559.276321	217209.864294	36.770996
1560.491673	217601.783967	36.776013
1562.263724	217997.397539	36.781031
1563.714402	218401.955164	36.786048
1565.363754	218800.868530	36.791066
1567.119277	219191.663788	36.796084
1568.492703	219600.048670	36.801101
1570.279522	219993.991191	36.806119
1572.030596	220403.053359	36.811136
1573.360319	220805.836981	36.816154
1574.910517	221212.395526	36.821172
1576.546958	221612.947155	36.826189
1578.161369	222018.736103	36.831207
1579.673850	222429.242225	36.836224
1581.276544	222842.478064	36.841242
1583.195114	223246.290822	36.846260
1584.745721	223656.185467	36.851277
1586.368263	224060.710347	36.856295
1587.805356	224506.414758	36.861312
1589.345202	224965.235546	36.866330
1590.978571	225381.675600	36.871348
1592.557112	225794.925724	36.876365
1594.430119	226204.216965	36.881383
1595.875070	226634.408361	36.886400
1597.532910	227042.086839	36.891418
1599.224587	227458.066908	36.896436
1600.584769	227891.476920	36.901453
1602.330064	228305.469568	36.906471
1603.770338	228724.847990	36.911488
1605.658324	229147.862225	36.916506
1607.528214	229572.150774	36.921524
1608.781716	229979.066699	36.926541
1610.939706	230397.442547	36.931559
1612.324197	230832.305573	36.936576
1614.051498	231247.605292	36.941594
1615.691121	231662.209419	36.946612
1617.247600	232090.570425	36.951629
1618.718915	232510.513490	36.956647
1620.333480	232930.713431	36.961664
1622.156406	233357.586011	36.966682
1623.382428	233780.468697	36.971700
1625.341350	234210.826434	36.976717
1626.829475	234627.724035	36.981735
1628.476997	235053.664691	36.986752
1630.347682	235481.550855	36.991770
1632.046556	235904.259085	36.996788
1633.332661	236327.823948	37.001805
1635.314734	236748.099591	37.006823
1636.971298	237174.602608	37.011840
1638.524557	237578.820739	37.016858
1640.502882	237989.269188	37.021876
1642.228670	238381.064299	37.026893
1643.644338	238770.498199	37.031911
1645.098249	239164.321087	37.036928
1646.740307	239576.250792	37.041946
1648.369790	239968.496633	37.046964
1649.424984	240373.615386	37.051981
1651.434555	240780.025151	37.056999
1652.801413	241193.629064	37.062016
1654.439588	241615.622489	37.067034
1655.937141	242026.234178	37.072052
1657.749660	242453.179133	37.077069
1659.784367	242867.005798	37.082087
1660.984622	243288.947370	37.087104
1662.510833	243712.309118	37.092122
1664.386772	244127.815131	37.097140
1665.792887	244567.481119	37.102157
1667.484831	245000.318024	37.107175
1669.024885	245423.527589	37.112192
1670.714047	245873.970310	37.117210
1672.285578	246303.755181	37.122228
1673.983613	246748.609015	37.127245
1675.764831	247196.142390	37.132263
1677.245451	247642.811471	37.137280
1678.808746	248094.979872	37.142298
1680.768696	248543.120410	37.147316
1682.080723	248998.938566	37.152333
1683.921731	249447.252142	37.157351
1685.502486	249909.148993	37.162368
1687.300102	250365.929855	37.167386
1689.265746	250835.410346	37.172404
1690.534534	251297.995092	37.177421
1692.558731	251760.709473	37.182439
1694.374570	252229.047328	37.187456
1695.378471	252702.549470	37.192474
1697.092695	253170.091864	37.197492
1698.686709	253658.408844	37.202509
1700.834927	254137.336981	37.207527
1702.262611	254605.689610	37.212544
1704.164019	255099.113440	37.217562
1705.967948	255571.722890	37.222580
1707.806021	256056.012376	37.227597
1709.570612	256524.919748	37.232615
1710.978314	257012.024134	37.237632
1712.816922	257499.133646	37.242650
1714.803756	257974.634830	37.247668
1716.319151	258467.894616	37.252685
1717.971340	258953.790259	37.257703
1719.994229	259434.315360	37.262720
1721.570275	259933.636450	37.267738
1723.357109	260409.704029	37.272756
1725.030635	260896.942265	37.277773
1726.728218	261374.167499	37.282791
1728.576525	261872.249172	37.287808
1730.540849	262360.073968	37.292826
1732.516359	262832.502326	37.297844
1733.946376	263322.015314	37.302861
1735.676890	263810.208230	37.307879
1737.418389	264295.833303	37.312896
1739.352288	264788.234320	37.317914
1741.143547	265270.751293	37.322932
1742.761362	265762.975130	37.327949
1744.524695	266248.391871	37.332967
1746.410658	266727.081498	37.337984
1748.074993	267227.603109	37.343002
1749.765985	267704.063102	37.348020
1751.435654	268198.079594	37.353037
1752.994854	268680.275965	37.358055
1754.861060	269149.033696	37.363072
1756.556669	269619.800463	37.368090
1758.298953	270087.307351	37.373108
1759.854719	270558.654857	37.378125
1761.707377	271024.110027	37.383143
1763.456578	271500.377807	37.388160
1764.658528	271975.998573	37.393178
1767.117207	272449.302613	37.398196
1768.779110	272939.503243	37.403213
1770.123854	273423.607976	37.408231
1772.049366	273900.985867	37.413248
1773.406909	274399.337584	37.418266
1775.602238	274889.446582	37.423284
1777.047403	275381.482088	37.428301
1778.601347	275875.353005	37.433319
1780.372370	276378.738309	37.438336
1782.337672	276878.762725	37.443354
1784.190209	277387.670014	37.448372
1785.820044	277891.608668	37.453389
1787.236466	278408.129996	37.458407
1789.543922	278918.558798	37.463424
1791.037742	279436.131615	37.468442
1792.993291	279949.841928	37.473460
1794.515560	280480.692435	37.478477
1796.666593	280999.524173	37.483495
1798.610359	281512.774895	37.488512
1800.332711	282045.797741	37.493530
1802.297038	282563.665092	37.498548
1804.098304	283096.290630	37.503565
1805.741253	283628.661195	37.508583
1807.327118	284148.084802	37.513600
1809.279178	284693.482457	37.518618
1811.391364	285224.474746	37.523636
1812.861465	285761.286460	37.528653
1814.581391	286307.021521	37.533671
1816.644498	286834.510897	37.538688
1818.001593	287389.192116	37.543706
1819.746854	287929.938320	37.548724
1821.905730	288472.468354	37.553741
1823.622647	289024.518177	37.558759
1825.738775	289574.188372	37.563776
1827.414250	290133.682724	37.568794
1829.237755	290672.525331	37.573812
1831.077822	291241.334908	37.578829
1832.935037	291792.790953	37.583847
1835.136260	292349.724862	37.588864
1836.740226	292919.149860	37.593882
1838.456946	293451.241619	37.598900
1840.629378	294032.022552	37.603917
1842.196008	294583.869234	37.608935
1844.216977	295145.620066	37.613952
1845.782852	295698.959954	37.618970
1848.058875	296261.247189	37.623988
1850.183007	296823.531190	37.629005
1851.753033	297381.255786	37.634023
1853.921197	297949.926991	37.639040
1855.254354	298513.323122	37.644058
1857.128755	299066.518283	37.649076
1859.106802	299635.795667	37.654093
1860.748379	300200.629923	37.659111
1862.934762	300758.411972	37.664128
1864.526692	301340.645290	37.669146
1866.164554	301898.231931	37.674164
1868.197414	302467.889963	37.679181
1869.886348	303039.531484	37.684199
1871.985936	303617.120722	37.689216
1873.799710	304190.486809	37.694234
1875.660834	304763.358867	37.699252
1877.574616	305315.317191	37.704269
1878.633741	305863.222760	37.709287
1881.003186	306413.041758	37.714304
1882.373839	306976.532828	37.719322
1884.483704	307531.314271	37.724340
1886.004293	308093.020768	37.729357
1887.813493	308663.741975	37.734375
1889.903143	309235.250921	37.739392
1891.555998	309810.865769	37.744410
1893.540794	310384.466235	37.749428
1895.660464	310967.004607	37.754445
1897.449026	311543.270048	37.759463
1899.215567	312120.677564	37.764480
1901.047943	312715.363282	37.769498
1902.727195	313291.938284	37.774516
1904.609487	313888.866520	37.779533
1906.249598	314491.949772	37.784551
1908.633092	315075.911046	37.789568
1910.223660	315688.438877	37.794586
1912.510644	316293.304761	37.799604
1914.244525	316894.016214	37.804621
1916.137406	317509.601659	37.809639
1918.127793	318121.280514	37.814656
1920.142093	318729.039585	37.819674
1921.824062	319346.370020	37.824692
1923.893420	319955.378550	37.829709
1925.451776	320580.106952	37.834727
1927.833084	321206.826392	37.839744
1929.931089	321839.248744	37.844762
1931.822081	322466.036972	37.849780
1934.265340	323085.466216	37.854797
1935.910870	323714.974037	37.859815
1937.907675	324331.671823	37.864832
1939.717342	324960.682948	37.869850
1941.798808	325585.098067	37.874868
1944.012047	326218.625093	37.879885
1945.816346	326845.332619	37.884903
1947.699392	327469.634049	37.889920
1949.660431	328115.749935	37.894938
1951.642402	328748.348839	37.899956
1953.738648	329373.051799	37.904973
1955.963643	330003.032705	37.909991
1957.968710	330636.368692	37.915008
1960.032205	331281.518228	37.920026
1962.245100	331912.444582	37.925044
1964.211828	332548.583227	37.930061
1965.962623	333181.957728	37.935079
1968.168305	333809.360304	37.940096
1969.993283	334438.950850	37.945114
1971.746022	335079.588474	37.950132
1973.600326	335706.544609	37.955149
1975.659723	336353.284742	37.960167
1977.363278	336989.845826	37.965184
1979.636660	337634.199421	37.970202
1981.676572	338281.959527	37.975220
1984.122444	338911.292331	37.980237
1985.651222	339565.415557	37.985255
1987.554019	340199.949331	37.990272
1989.619155	340855.845486	37.995290
1991.285746	341498.346346	38.000308
1993.621615	342144.510169	38.005325
1995.352399	342792.085160	38.010343
1997.417610	343444.266363	38.015360
1999.241249	344093.762878	38.020378
2001.327107	344751.481202	38.025396
2003.378819	345403.358653	38.030413
2005.181789	346052.907827	38.035431
2007.235825	346700.147754	38.040448
2009.041595	347336.176807	38.045466
2010.965535	347977.227854	38.050484
2012.745879	348612.152098	38.055501
2014.500852	349255.852324	38.060519
2016.569356	349883.579959	38.065536
2018.616397	350531.527788	38.070554
2020.208749	351181.368332	38.075572
2022.091733	351828.715179	38.080589
2023.916726	352492.530958	38.085607
2026.007585	353143.528820	38.090624
2028.231358	353813.729231	38.095642
2029.968618	354486.536935	38.100660
2031.820846	355154.874505	38.105677
2033.886294	355847.880451	38.110695
2036.201629	356524.543917	38.115712
2038.129871	357204.025946	38.120730
2039.863743	357893.322722	38.125748
2042.342455	358579.896989	38.130765
2044.010343	359283.846342	38.135783
2045.953520	359969.140823	38.140800
2048.113160	360677.779838	38.145818
2049.811591	361381.915732	38.150836
2052.074075	362089.117243	38.155853
2054.177665	362808.078362	38.160871
2056.491269	363517.630406	38.165888
2058.704910	364236.927516	38.170906
2060.285816	364958.522685	38.175924
2062.732073	365683.157720	38.180941
2064.564108	366403.745500	38.185959
2066.858311	367131.675666	38.190976
2068.975289	367845.745676	38.195994
2071.390823	368578.421849	38.201012
2073.873486	369309.499798	38.206029
2075.665109	370031.089449	38.211047
2077.846655	370750.266977	38.216064
2079.739418	371490.783393	38.221082
2081.692171	372221.281629	38.226100
2083.988987	372946.610288	38.231117
2086.004702	373684.372632	38.236135
2087.722277	374413.368342	38.241152
2090.481088	375161.071010	38.246170
2092.503806	375902.513695	38.251188
2094.802863	376630.961349	38.256205
2096.546432	377372.367885	38.261223
2099.521085	378114.341280	38.266240
2102.048339	378854.597274	38.271258
2103.823388	379587.632854	38.276276
2106.065452	380303.966401	38.281293
2108.229685	381040.963114	38.286311
2109.948499	381771.145508	38.291328
2112.136576	382499.256568	38.296346
2114.403044	383229.721905	38.301364
2117.040226	383953.365429	38.306381
2118.967628	384699.421334	38.311399
2120.864536	385422.748525	38.316416
2123.401259	386152.925768	38.321434
2125.120577	386890.750782	38.326452
2127.351677	387616.026565	38.331469
2128.948964	388352.646080	38.336487
2131.267146	389084.616932	38.341504
2133.728170	389829.069761	38.346522
2135.598289	390572.410833	38.351540
2137.832066	391299.324172	38.356557
2140.028688	392044.704995	38.361575
2142.117927	392793.380446	38.366592
2144.125393	393525.524894	38.371610
2146.485215	394274.397787	38.376628
2148.669805	394996.794967	38.381645
2150.748426	395724.615905	38.386663
2152.755643	396434.081591	38.391680
2154.794178	397146.718323	38.396698
2156.582836	397855.222744	38.401716
2158.877290	398570.342186	38.406733
2160.813058	399294.220751	38.411751
2163.135381	400017.079747	38.416768
2164.703652	400743.618013	38.421786
2166.807687	401485.937396	38.426804
2169.011288	402215.779475	38.431821
2170.994148	402956.940091	38.436839
2172.956948	403710.930731	38.441856
2175.040657	404459.534983	38.446874
2177.210364	405222.850680	38.451892
2178.972792	405988.163410	38.456909
2181.049873	406755.125724	38.461927
2183.446589	407531.564826	38.466944
2185.258001	408310.231768	38.471962
2187.240120	409099.057287	38.476980
2189.626141	409890.022292	38.481997
2191.683847	410678.130402	38.487015
2194.274402	411476.664792	38.492032
2196.238145	412288.627397	38.497050
2198.069634	413101.093447	38.502068
2200.510549	413905.126139	38.507085
2202.309424	414728.640842	38.512103
2204.724073	415544.632459	38.517120
2207.197041	416374.163310	38.522138
2209.395235	417188.922974	38.527156
2211.345010	418023.475851	38.532173
2213.756593	418854.886342	38.537191
2215.738568	419692.164596	38.542208
2218.584564	420522.030419	38.547226
2221.036584	421366.417255	38.552244
2223.294839	422192.956903	38.557261
2225.763791	423035.511833	38.562279
2227.970241	423876.334341	38.567296
2230.314996	424699.636232	38.572314
2232.267056	425543.127090	38.577332
2234.942916	426372.343084	38.582349
2237.238620	427202.504686	38.587367
2239.742736	428048.297816	38.592384
2242.180635	428875.745377	38.597402
2244.333219	429708.982413	38.602420
2246.828330	430538.640656	38.607437
2249.040019	431370.645012	38.612455
2251.281701	432198.008588	38.617472
2253.928370	433032.362372	38.622490
2256.294857	433874.324692	38.627508
2258.321325	434698.850853	38.632525
2260.955439	435526.334475	38.637543
2262.956047	436353.133585	38.642560
2265.530344	437176.720933	38.647578
2267.659975	438008.246285	38.652596
2270.086362	438837.465444	38.657613
2272.248022	439666.748281	38.662631
2274.403268	440492.307588	38.667648
2276.938950	441325.515056	38.672666
2279.056366	442167.361625	38.677684
2281.311733	442980.314325	38.682701
2283.646275	443816.243567	38.687719
2286.014904	444655.575374	38.692736
2288.391380	445474.030868	38.697754
2290.358403	446308.255540	38.702772
2292.660202	447141.735071	38.707789
2295.042928	447978.810843	38.712807
2297.311326	448807.476220	38.717824
2299.795833	449633.848156	38.722842
2301.838543	450447.565879	38.727860
2304.191326	451248.759520	38.732877
2306.144169	452055.450486	38.737895
2308.344577	452862.575175	38.742912
2310.846043	453666.736422	38.747930
2312.811169	454485.872340	38.752948
2314.768419	455296.937151	38.757965
2317.148043	456119.378125	38.762983
2318.992027	456951.733878	38.768000
2321.282624	457772.100508	38.773018
2323.428093	458615.966987	38.778036
2325.591135	459458.177550	38.783053
2328.030544	460317.090790	38.788071
2330.268525	461170.035444	38.793088
2332.383283	462032.770355	38.798106
2334.495234	462898.602106	38.803124
2337.175951	463766.424924	38.808141
2339.100821	464646.969651	38.813159
2341.238412	465530.674237	38.818176
2343.546123	466411.884933	38.823194
2345.871271	467315.035456	38.828212
2348.722894	468213.711123	38.833229
2350.810183	469112.976261	38.838247
2352.864426	470030.495715	38.843264
2355.290449	470927.901679	38.848282
2357.284391	471848.728671	38.853300
2359.799487	472793.977763	38.858317
2362.020844	473718.060889	38.863335
2363.999883	474664.718821	38.868352
2366.773899	475594.073724	38.873370
2368.763850	476540.988066	38.878388
2370.935375	477484.844029	38.883405
2373.309629	478448.618161	38.888423
2375.860700	479414.787067	38.893440
2378.650384	480371.775508	38.898458
2380.918899	481336.273094	38.903476
2383.214531	482287.586258	38.908493
2385.993030	483269.215945	38.913511
2388.066250	484230.611743	38.918528
2390.615607	485192.079146	38.923546
2393.003926	486171.543671	38.928564
2395.340120	487139.755891	38.933581
2398.057348	488122.389629	38.938599
2400.268132	489096.269233	38.943616
2403.170815	490083.405946	38.948634
2405.260363	491072.639541	38.953652
2407.733856	492046.663815	38.958669
2410.479811	493023.414042	38.963687
2412.892530	494011.668675	38.968704
2415.342292	494986.438290	38.973722
2417.592164	495971.023727	38.978740
2420.187638	496960.186943	38.983757
2422.540247	497941.563095	38.988775
2425.090056	498938.891177	38.993792
2427.455447	499920.149369	38.998810
2429.959508	500910.708699	39.003828
2432.517340	501905.991497	39.008845
2435.022742	502887.555381	39.013863
2437.408791	503884.108766	39.018880
2440.230932	504864.443094	39.023898
2442.402880	505858.541297	39.028916
2444.460235	506841.454379	39.033933
2447.494684	507827.373316	39.038951
2449.791506	508823.184621	39.043968
2452.470364	509797.949946	39.048986
2454.955325	510794.111737	39.054004
2457.371123	511774.042210	39.059021
2459.897536	512752.885781	39.064039
2462.177474	513711.498945	39.069056
2464.921029	514662.316847	39.074074
2467.188801	515607.612195	39.079092
2469.686695	516555.331848	39.084109
2472.313398	517503.073238	39.089127
2474.332311	518474.436879	39.094144
2476.520129	519412.258219	39.099162
2478.774271	520382.102395	39.104180
2481.109149	521356.959691	39.109197
2483.584616	522332.134445	39.114215
2485.914787	523309.083834	39.119232
2488.166592	524303.308751	39.124250
2490.318527	525292.649817	39.129268
2492.900505	526293.286164	39.134285
2495.303640	527293.079381	39.139303
2497.649355	528311.445159	39.144320
2499.952127	529324.662955	39.149338
2502.318663	530363.124251	39.154356
2504.633532	531381.636014	39.159373
2507.305517	532427.754250	39.164391
2509.582220	533482.218238	39.169408
2511.912130	534522.051522	39.174426
2514.560848	535573.383107	39.179444
2516.883045	536642.707663	39.184461
2519.409174	537696.923868	39.189479
2521.705727	538777.717312	39.194496
2524.376407	539860.731791	39.199514
2527.030168	540943.716792	39.204532
2529.473293	542027.810631	39.209549
2532.243576	543112.924000	39.214567
2534.376385	544221.094314	39.219584
2537.039755	545302.333771	39.224602
2539.734199	546402.996015	39.229620
2542.069918	547524.850042	39.234637
2544.768178	548630.111513	39.239655
2547.413332	549738.007844	39.244672
2550.397088	550846.663622	39.249690
2552.750085	551972.474747	39.254708
2555.569694	553093.994016	39.259725
2558.373874	554194.112813	39.264743
2561.183661	555316.454380	39.269760
2563.494538	556427.678909	39.274778
2566.182845	557540.005054	39.279796
2568.381240	558656.388837	39.284813
2571.117268	559789.419997	39.289831
2573.581702	560907.278309	39.294848
2576.106432	562036.584706	39.299866
2578.674115	563176.886678	39.304884
2581.453861	564301.887305	39.309901
2584.110385	565438.360916	39.314919
2586.444269	566569.716650	39.319936
2589.309396	567713.086224	39.324954
2591.828625	568839.090945	39.329972
2594.462259	569985.810546	39.334989
2597.137234	571117.462275	39.340007
2599.753499	572263.778909	39.345024
2602.393205	573416.963741	39.350042
2605.226004	574547.178918	39.355060
2607.723241	575698.923749	39.360077
2610.598286	576832.739445	39.365095
2613.104369	577973.686876	39.370112
2615.686715	579124.449204	39.375130
2618.602022	580266.271972	39.380148
2620.778747	581405.853938	39.385165
2623.350162	582560.309753	39.390183
2626.016990	583707.570639	39.395200
2628.616537	584850.372563	39.400218
2631.389160	585987.774306	39.405236
2633.977444	587111.514353	39.410253
2636.804987	588219.220497	39.415271
2638.764704	589326.666944	39.420288
2641.336201	590446.589441	39.425306
2643.944321	591552.119037	39.430324
2646.454935	592681.462798	39.435341
2649.152946	593813.072876	39.440359
2651.719685	594945.898638	39.445376
2654.195041	596062.450573	39.450394
2656.839630	597211.074426	39.455412
2659.067658	598350.088260	39.460429
2661.908232	599507.368170	39.465447
2664.297158	600657.446683	39.470464
2666.637819	601826.093823	39.475482
2669.217959	602985.571594	39.480500
2671.589275	604182.509488	39.485517
2674.123482	605366.031387	39.490535
2676.602866	606573.361598	39.495552
2679.541570	607769.228248	39.500570
2682.065950	608973.742937	39.505588
2684.567929	610196.393626	39.510605
2687.380535	611405.903315	39.515623
2689.910535	612643.839911	39.520640
2692.517124	613869.922952	39.525658
2695.148604	615101.517331	39.530676
2698.391099	616348.924615	39.535693
2701.081281	617585.832226	39.540711
2703.880251	618833.630555	39.545728
2706.804598	620089.413413	39.550746
2709.346203	621337.017778	39.555764
2711.855564	622596.427821	39.560781
2715.005506	623843.493091	39.565799
2717.579455	625115.839939	39.570816
2720.480481	626373.094851	39.575834
2723.326891	627639.251945	39.580852
2726.166244	628911.502729	39.585869
2728.980714	630168.523506	39.590887
2731.440419	631444.627501	39.595904
2734.041934	632724.597537	39.600922
2737.297698	634006.699706	39.605940
2740.077407	635295.062237	39.610957
2742.863392	636565.097709	39.615975
2745.394380	637840.558918	39.620992
2748.170714	639130.441840	39.626010
2751.382578	640409.564660	39.631028
2753.780191	641701.981207	39.636045
2756.418078	642976.937267	39.641063
2759.413685	644269.179486	39.646080
2762.044265	645571.140694	39.651098
2764.923801	646864.417368	39.656116
2767.820445	648164.005955	39.661133
2770.741635	649459.933105	39.666151
2773.542671	650755.662348	39.671168
2776.119132	652052.505997	39.676186
2779.121744	653352.099591	39.681204
2781.645410	654658.227443	39.686221
2784.596265	655956.789404	39.691239
2787.327012	657251.629999	39.696256
2789.830630	658554.503901	39.701274
2793.125438	659869.820268	39.706292
2795.661506	661176.620148	39.711309
2798.474147	662477.921523	39.716327
2801.040752	663788.295932	39.721344
2803.845066	665093.326747	39.726362
2807.338219	666409.411288	39.731380
2809.926374	667712.428626	39.736397
2812.820755	669038.249078	39.741415
2815.237890	670325.017789	39.746432
2817.916740	671605.799273	39.751450
2821.092097	672875.584125	39.756468
2823.544424	674150.039619	39.761485
2826.605287	675415.322799	39.766503
2829.415294	676688.975091	39.771520
2832.012716	677969.793411	39.776538
2834.852065	679234.245139	39.781556
2837.241679	680526.917691	39.786573
2839.930082	681811.212288	39.791591
2842.535097	683104.430325	39.796608
2845.541425	684414.135544	39.801626
2848.189065	685716.660386	39.806644
2850.702550	687034.411450	39.811661
2853.523259	688356.536489	39.816679
2856.188760	689677.252312	39.821696
2858.850956	691014.597910	39.826714
2861.714696	692367.935923	39.831732
2864.416424	693711.817955	39.836749
2867.558341	695072.636838	39.841767
2870.186917	696443.796124	39.846784
2872.891264	697813.242289	39.851802
2876.073763	699187.602419	39.856820
2878.362830	700570.173068	39.861837
2881.372531	701962.715649	39.866855
2883.969882	703368.533420	39.871872
2886.718729	704773.355151	39.876890
2889.922372	706181.044202	39.881908
2892.772937	707607.978237	39.886925
2895.843147	709019.830987	39.891943
2898.397812	710452.035411	39.896960
2901.005812	711893.644405	39.901978
2904.167476	713332.739411	39.906996
2907.257178	714770.413724	39.912013
2909.726222	716222.493084	39.917031
2912.606896	717678.953646	39.922048
2915.531671	719147.470390	39.927066
2918.390756	720611.535621	39.932084
2921.187294	722095.775188	39.937101
2923.889504	723572.496794	39.942119
2926.857709	725056.868508	39.947136
2929.710703	726547.663065	39.952154
2932.626908	728037.484153	39.957172
2935.796514	729535.884078	39.962189
2938.636905	731042.064009	39.967207
2941.364240	732546.994967	39.972224
2944.057169	734065.179959	39.977242
2947.242297	735582.947976	39.982260
2949.886584	737111.869783	39.987277
2952.711963	738626.898654	39.992295
2956.053500	740161.141067	39.997312
2958.890525	741703.111596	40.002330
2961.952288	743234.288656	40.007348
2965.031274	744780.598689	40.012365
2967.845856	746313.879033	40.017383
2971.110494	747862.310512	40.022400
2973.720486	749411.921830	40.027418
2976.685517	750954.464496	40.032436
2979.694284	752501.371858	40.037453
2982.602160	754067.882124	40.042471
2985.905017	755622.583962	40.047488
2988.795142	757184.717600	40.052506
2991.793692	758730.221456	40.057524
2994.360351	760298.167530	40.062541
2997.333296	761863.852141	40.067559
3000.462391	763428.841515	40.072576
3003.349774	765010.019541	40.077594
3006.482916	766576.121703	40.082612
3009.315154	768141.158060	40.087629
3012.442468	769679.620446	40.092647
3015.412320	771206.045267	40.097664
3017.975039	772746.222797	40.102682
3021.103833	774276.799571	40.107700
3023.967866	775806.756572	40.112717
3026.868611	777342.475000	40.117735
3029.964770	778880.782351	40.122752
3032.498648	780439.026226	40.127770
3035.446367	781992.008542	40.132788
3038.715943	783558.534421	40.137805
3041.849445	785125.280305	40.142823
3044.622181	786695.567034	40.147840
3047.079777	788284.433248	40.152858
3050.254454	789877.579938	40.157876
3053.015892	791474.748124	40.162893
3055.804002	793076.155189	40.167911
3059.026944	794697.990084	40.172928
3061.994973	796334.915662	40.177946
3064.968835	797965.728635	40.182964
3067.749799	799609.650211	40.187981
3070.350427	801261.285117	40.192999
3073.727356	802916.750775	40.198016
3076.786244	804590.259648	40.203034
3079.827015	806266.638879	40.208052
3082.954658	807952.320073	40.213069
3085.898502	809651.933204	40.218087
3089.319382	811342.002705	40.223104
3092.345796	813040.995191	40.228122
3095.280992	814735.569388	40.233140
3098.345336	816445.317077	40.238157
3101.096569	818160.340715	40.243175
3104.763199	819875.210803	40.248192
3107.808656	821594.471879	40.253210
3110.969702	823328.336916	40.258228
3114.033559	825055.764069	40.263245
3117.452084	826785.846325	40.268263
3120.821018	828519.669755	40.273280
3123.704501	830262.563123	40.278298
3126.859487	831991.354462	40.283316
3129.936302	833744.724725	40.288333
3133.258605	835497.090403	40.293351
3136.547395	837245.089715	40.298368
3139.483154	838996.610220	40.303386
3142.654695	840750.139571	40.308404
3145.780482	842507.422502	40.313421
3148.965277	844270.429840	40.318439
3152.064579	846033.638347	40.323456
3155.210376	847809.170545	40.328474
3158.496890	849577.569782	40.333492
3161.768396	851345.761017	40.338509
3164.703184	853122.921751	40.343527
3168.015124	854895.530374	40.348544
3171.057714	856688.244405	40.353562
3174.234985	858464.116351	40.358580
3177.449830	860245.673147	40.363597
3180.762446	862039.974976	40.368615
3183.913427	863821.949411	40.373632
3186.964189	865627.056789	40.378650
3190.218238	867409.990456	40.383668
3193.680334	869204.561593	40.388685
3196.831122	870996.516425	40.393703
3200.019962	872786.281532	40.398720
3202.853596	874593.367190	40.403738
3206.403335	876402.201310	40.408756
3209.305551	878202.949500	40.413773
3212.404544	880003.790326	40.418791
3215.696474	881812.838680	40.423808
3218.477911	883607.887092	40.428826
3221.737546	885373.719163	40.433844
3224.297453	887156.408558	40.438861
3227.210853	888917.547460	40.443879
3230.878857	890700.405776	40.448896
3233.726876	892492.200218	40.453914
3236.769313	894275.012529	40.458932
3239.752855	896068.746317	40.463949
3242.817961	897868.259072	40.468967
3246.004121	899681.435185	40.473984
3248.728944	901504.599733	40.479002
3251.773918	903339.248433	40.484020
3254.899210	905186.465648	40.489037
3257.885722	907047.138363	40.494055
3261.209186	908896.169159	40.499072
3264.071480	910779.938912	40.504090
3267.513229	912652.878917	40.509108
3270.504174	914532.459518	40.514125
3273.265488	916445.908590	40.519143
3276.929683	918350.185341	40.524160
3279.722297	920274.762712	40.529178
3282.473186	922205.377750	40.534196
3286.057262	924150.124150	40.539213
3289.232749	926109.763345	40.544231
3292.863687	928065.255852	40.549248
3295.825219	930037.096361	40.554266
3299.253309	932001.329168	40.559284
3302.594018	933979.587963	40.564301
3305.644546	935957.056311	40.569319
3309.184964	937955.124274	40.574336
3312.641106	939965.445870	40.579354
3315.721012	941950.969104	40.584372
3319.323903	943950.646043	40.589389
3322.549931	945972.054238	40.594407
3325.806064	947976.340091	40.599424
3329.427161	950010.509808	40.604442
3332.496657	952022.021836	40.609460
3336.212836	954089.997777	40.614477
3339.416874	956177.451972	40.619495
3343.075415	958246.478074	40.624512
3346.197707	960347.688165	40.629530
3349.668962	962425.897145	40.634548
3352.950577	964518.622061	40.639565
3356.096604	966617.246134	40.644583
3359.975206	968708.834564	40.649600
3363.554973	970815.220948	40.654618
3366.774825	972910.653196	40.659636
3370.445047	975012.945738	40.664653
3373.598029	977099.251811	40.669671
3377.354982	979204.081828	40.674688
3380.882924	981307.784222	40.679706
3384.128767	983398.881900	40.684724
3387.377226	985511.591858	40.689741
3390.245671	987630.000197	40.694759
3394.209642	989728.381828	40.699776
3397.360287	991834.675783	40.704794
3400.712401	993943.167080	40.709812
3404.380064	996061.894609	40.714829
3407.987677	998185.762053	40.719847
3411.094572	1000287.952194	40.724864
3414.621169	1002395.112638	40.729882
3418.243406	1004505.835406	40.734900
3421.938091	1006607.032071	40.739917
3424.903221	1008725.202735	40.744935
3428.357495	1010829.225267	40.749952
3431.544350	1012948.773136	40.754970
3434.881251	1015075.821691	40.759988
3438.984332	1017194.100920	40.765005
3442.150302	1019299.422892	40.770010
3445.692182	1021343.290309	40.775015
3448.903187	1023330.457690	40.780020
3452.567163	1025239.350769	40.785024
3455.747111	1027090.538728	40.790029
3458.639217	1028853.745953	40.795034
3461.571099	1030547.001562	40.800039
3465.153345	1032175.395704	40.805044
3467.787197	1033703.364595	40.810048
3470.262232	1035156.968434	40.815053
3473.028463	1036537.834421	40.820058
3475.805739	1037852.054769	40.825063
3478.303557	1039072.668641	40.830068
3480.612718	1040225.516890	40.835072
3482.767114	1041309.573507	40.840077
3484.560440	1042334.376612	40.845082
3487.181539	1043267.803611	40.850087
3488.887719	1044158.650437	40.855092
3490.867979	1044988.305563	40.860096
3492.548553	1045750.328148	40.865101
3494.574162	1046452.842309	40.870106
3496.392073	1047097.409017	40.875111
3497.337976	1047676.439722	40.880116
3498.798390	1048236.996144	40.885120
3500.533591	1048717.968293	40.890125
3501.759567	1049176.412813	40.895130
3503.267628	1049576.906349	40.900135
3504.586035	1049944.709622	40.905140
3505.525114	1050259.223849	40.910144
3506.709694	1050532.312289	40.915149
3507.480643	1050779.228188	40.920154
3508.468854	1050984.347533	40.925159
3509.396237	1051164.593769	40.930164
3510.022058	1051301.208196	40.935168
3511.183007	1051417.580920	40.940173
3511.659918	1051517.288426	40.945178
3512.752126	1051581.221335	40.950183
3513.165529	1051614.992975	40.955188
3513.750798	1051623.766260	40.960192
3514.397263	1051614.693812	40.965197
3514.769319	1051575.104763	40.970202
3515.617331	1051520.589808	40.975207
3516.153010	1051446.264944	40.980212
3516.379997	1051359.359782	40.985216
3517.150060	1051244.114134	40.990221
3517.488782	1051133.083090	40.995226
3517.774257	1050981.755154	41.000231
3518.385832	1050830.369356	41.005236
3518.575370	1050655.038976	41.010240
3519.203505	1050469.409321	41.015245
3519.575452	1050266.843538	41.020250
3519.815744	1050057.445055	41.025255
3520.229063	1049840.584264	41.030260
3520.450907	1049611.401697	41.035264
3520.903949	1049348.414654	41.040269
3520.960343	1049104.095868	41.045274
3520.942239	1048845.792263	41.050279
3520.880903	1048574.847196	41.055284
3521.091223	1048305.580504	41.060288
3521.489710	1048021.606028	41.065293
3521.506920	1047733.338334	41.070298
3521.895881	1047442.871779	41.075303
3522.200530	1047124.519099	41.080308
3522.079296	1046811.911338	41.085312
3522.150664	1046496.841731	41.090317
3522.489177	1046191.264049	41.095322
3522.458733	1045863.050633	41.100327
3522.522940	1045536.925498	41.105332
3522.654995	1045203.144838	41.110336
3522.790740	1044855.926234	41.115341
3522.718529	1044523.972305	41.120346
3522.954300	1044181.811201	41.125351
3523.132478	1043828.825454	41.130356
3523.052840	1043488.507852	41.135360
3523.206971	1043123.895075	41.140365
3523.163645	1042769.429993	41.145370
3523.114964	1042396.594912	41.150375
3523.350571	1042044.548355	41.155380
3523.192539	1041672.938122	41.160384
3523.326718	1041312.072789	41.165389
3523.251882	1040945.519316	41.170394
3523.207164	1040565.702263	41.175399
3523.608828	1040194.190590	41.180404
3523.181958	1039820.568410	41.185408
3523.359701	1039446.338375	41.190413
3523.301425	1039072.025374	41.195418
3523.420264	1038695.821919	41.200423
3523.432819	1038302.794993	41.205428
3522.814293	1037918.445868	41.210432
3523.218577	1037538.057794	41.215437
3522.713574	1037170.359381	41.220442
3522.940325	1036787.919349	41.225447
3523.025279	1036409.440003	41.230452
3522.576603	1036038.467195	41.235456
3522.769760	1035653.634363	41.240461
3522.754360	1035283.023226	41.245466
3522.936810	1034905.585812	41.250471
3523.031613	1034523.301907	41.255476
3522.559058	1034141.762201	41.260480
3522.905227	1033754.935306	41.265485
3522.474005	1033386.297475	41.270490
3522.714292	1032994.792352	41.275495
3522.624740	1032613.278262	41.280500
3522.563512	1032235.603234	41.285504
3522.148941	1031850.897838	41.290509
3522.086218	1031478.106115	41.295514
3522.344666	1031099.624117	41.300519
3522.455715	1030726.076114	41.305524
3522.374984	1030336.759665	41.310528
3522.632623	1029963.426769	41.315533
3522.097198	1029578.100478	41.320538
3522.080210	1029194.210944	41.325543
3522.130679	1028817.641126	41.330548
3521.868431	1028437.224921	41.335552
3522.168181	1028044.878283	41.340557
3521.793908	1027677.596145	41.345562
3522.009919	1027302.930208	41.350567
3521.879598	1026925.003680	41.355572
3521.529145	1026548.443673	41.360576
3521.902380	1026166.702777	41.365581
3521.692177	1025788.518817	41.370586
3521.420410	1025432.017076	41.375591
3521.387526	1025038.545417	41.380596
3521.265015	1024663.176997	41.385600
3521.255280	1024293.480966	41.390605
3520.861415	1023923.533102	41.395610
3521.115388	1023552.485072	41.400615
3521.098364	1023190.565994	41.405620
3520.848640	1022818.001780	41.410624
3521.016235	1022455.229454	41.415629
3520.866566	1022096.168927	41.420634
3520.805912	1021729.413353	41.425639
3521.047845	1021365.491956	41.430644
3520.577391	1020986.056721	41.435648
3520.643364	1020618.044204	41.440653
3520.340422	1020263.350989	41.445658
3520.778078	1019904.634911	41.450663
3520.610715	1019530.868777	41.455668
3520.274176	1019170.196933	41.460672
3520.364133	1018804.097767	41.465677
3520.215682	1018450.719059	41.470682
3520.082074	1018085.967630	41.475687
3520.204291	1017733.760047	41.480692
3519.759365	1017377.452617	41.485696
3519.953357	1017027.322946	41.490701
3520.034942	1016678.160110	41.495706
3519.981578	1016319.004513	41.500711
3519.753043	1015962.086443	41.505716
3519.584206	1015616.391832	41.510720
3519.848689	1015260.803480	41.515725
3519.573951	1014915.374280	41.520730
3519.581345	1014553.087273	41.525735
3519.555717	1014206.505864	41.530740
3519.677857	1013859.975800	41.535744
3519.149100	1013500.912402	41.540749
3518.935110	1013170.023547	41.545754
3518.848606	1012830.356801	41.550759
3518.990752	1012488.495926	41.555764
3518.450222	1012150.222121	41.560768
3518.521409	1011803.088184	41.565773
3518.393859	1011496.847099	41.570778
3518.619265	1011154.697232	41.575783
3518.652408	1010827.611389	41.580788
3518.651995	1010488.274601	41.585792
3518.514710	1010147.094458	41.590797
3518.150946	1009825.746367	41.595802
3517.909195	1009482.989033	41.600807
3518.210157	1009166.933684	41.605812
3517.994467	1008842.882171	41.610816
3518.110079	1008517.688710	41.615821
3517.972136	1008182.413350	41.620826
3518.038936	1007859.910521	41.625831
3518.073934	1007532.632963	41.630836
3517.524713	1007213.109814	41.635840
3517.586045	1006882.874810	41.640845
3517.364841	1006577.644962	41.645850
3517.214818	1006254.794446	41.650855
3517.613653	1005946.706823	41.655860
3517.420147	1005623.049700	41.660864
3517.251008	1005301.703085	41.665869
3517.208668	1004986.344777	41.670874
3517.398577	1004677.055640	41.675879
3517.296255	1004362.352907	41.680884
3517.127043	1004042.101315	41.685888
3517.045790	1003736.014008	41.690893
3517.087773	1003436.405183	41.695898
3517.160058	1003124.230268	41.700903
3516.996141	1002808.381314	41.705908
3516.950048	1002499.692570	41.710912
3516.909238	1002192.153278	41.715917
3516.601172	1001892.033872	41.720922
3516.642126	1001581.237919	41.725927
3516.444618	1001283.597169	41.730932
3516.138834	1000980.024098	41.735936
3516.591750	1000674.655775	41.740941
3516.315514	1000380.580249	41.745946
3516.106031	1000082.780951	41.750951
3515.801982	999780.505415	41.755956
3516.031210	999493.695851	41.760960
3515.972943	999202.150568	41.765965
3516.084952	998909.880957	41.770970
3515.787038	998617.274473	41.775975
3516.023393	998332.740755	41.780980
3515.861120	998032.392439	41.785984
3515.869092	997742.805151	41.790989
3515.754531	997465.294293	41.795994
3515.511994	997168.223155	41.800999
3515.697409	996879.146584	41.806004
3515.229208	996598.730800	41.811008
3515.423440	996317.218335	41.816013
3515.121928	996028.762788	41.821018
3515.110110	995741.705481	41.826023
3515.048599	995480.253140	41.831028
3514.851345	995198.262677	41.836032
3514.954245	994917.182647	41.841037
3515.286228	994652.510799	41.846042
3514.946179	994369.820884	41.851047
3515.032976	994095.813013	41.856052
3514.778513	993825.647100	41.861056
3514.746177	993536.338494	41.866061
3514.617245	993270.801373	41.871066
3514.493622	993003.107627	41.876071
3514.525006	992728.068584	41.881076
3514.498916	992467.543211	41.886080
3514.350693	992188.415420	41.891085
3514.141942	991936.275392	41.896090
3514.206629	991665.369378	41.901095
3514.224067	991409.173363	41.906100
3514.052016	991156.018126	41.911104
3513.813761	990878.302585	41.916109
3513.650393	990633.894056	41.921114
3513.875989	990376.447592	41.926119
3514.039337	990117.537623	41.931124
3513.627975	989864.461716	41.936128
3513.991734	989602.960871	41.941133
3513.658833	989353.261144	41.946138
3513.614451	989094.631256	41.951143
3513.782444	988849.603935	41.956148
3513.393487	988593.640384	41.961152
3513.693450	988329.751506	41.966157
3513.278423	988085.177307	41.971162
3513.521800	987842.629393	41.976167
3513.645820	987599.505704	41.981172
3513.268308	987341.241010	41.986176
3513.264842	987090.900038	41.991181
3512.879843	986851.826783	41.996186
3512.956708	986616.081060	42.001191
3513.509001	986369.323059	42.006196
3513.133548	986126.901498	42.011200
3513.029204	985876.426181	42.016205
3512.717531	985641.972222	42.021210
3512.694905	985401.705298	42.026215
3512.836066	985166.279165	42.031220
3512.553822	984931.693550	42.036224
3512.803051	984690.083513	42.041229
3512.760585	984451.438398	42.046234
3512.393049	984223.179723	42.051239
3512.487368	983984.199780	42.056244
3512.442036	983760.358087	42.061248
3512.429191	983519.327077	42.066253
3512.364466	983299.373926	42.071258
3512.251250	983067.904185	42.076263
3512.252961	982831.623805	42.081268
3512.170779	982619.162335	42.086272
3512.212114	982389.201206	42.091277
3511.983496	982166.205555	42.096282
3511.796022	981933.823517	42.101287
3511.881801	981703.534579	42.106292
3511.838967	981493.562742	42.111296
3511.936300	981277.800230	42.116301
3511.792233	981050.256279	42.121306
3512.025209	980836.212041	42.126311
3511.865583	980603.478324	42.131316
3512.143336	980395.463628	42.136320
3511.886715	980161.946766	42.141325
3511.561088	979946.691826	42.146330
3511.334983	979726.432160	42.151335
3511.674027	979501.383449	42.156340
3511.335001	979311.008743	42.161344
3511.702539	979086.915593	42.166349
3511.503048	978878.631274	42.171354
3511.480315	978663.375714	42.176359
3511.866013	978438.570459	42.181364
3511.262080	978230.524478	42.186368
3511.602787	978007.858581	42.191373
3511.506761	977800.690080	42.196378
3511.309079	977577.900757	42.201383
3510.998311	977375.441234	42.206388
3510.858112	977176.365759	42.211392
3511.154580	976965.487611	42.216397
3511.144250	976755.629250	42.221402
3510.917728	976559.868395	42.226407
3510.864213	976349.416006	42.231412
3510.801980	976154.786723	42.236416
3510.938437	975939.890912	42.241421
3510.515727	975743.939007	42.246426
3510.397404	975545.389451	42.251431
3510.371241	975350.042780	42.256436
3510.269611	975154.310955	42.261440
3510.446380	974961.360818	42.266445
3510.466564	974770.971109	42.271450
3510.313535	974576.303074	42.276455
3510.011611	974386.931043	42.281460
3510.022107	974200.433647	42.286464
3510.122520	974017.923065	42.291469
3510.214996	973824.557499	42.296474
3510.028613	973640.224833	42.301479
3510.155269	973455.541386	42.306484
3509.987480	973264.937033	42.311488
3509.854482	973067.379289	42.316493
3509.922392	972889.335280	42.321498
3509.482882	972701.201124	42.326503
3509.840613	972520.066982	42.331508
3509.496653	972346.669350	42.336512
3509.483688	972154.535872	42.341517
3509.469969	971995.251369	42.346522
3509.520752	971830.084647	42.351527
3509.318652	971638.845109	42.356532
3509.383501	971469.362938	42.361536
3509.674540	971284.680217	42.366541
3509.284332	971113.697767	42.371546
3509.500762	970935.177374	42.376551
3509.602560	970752.855932	42.381556
3509.349706	970592.104760	42.386560
3509.424863	970407.331538	42.391565
3509.231436	970235.312361	42.396570
3509.145765	970067.378553	42.401575
3509.017564	969893.284227	42.406580
3508.875912	969724.860515	42.411584
3509.572407	969557.663329	42.416589
3508.983793	969388.227290	42.421594
3508.822415	969222.237763	42.426599
3509.434392	969043.201999	42.431604
3509.222041	968879.265454	42.436608
3509.167620	968698.959025	42.441613
3509.136703	968537.624497	42.446618
3509.360632	968362.447280	42.451623
3509.268998	968192.111269	42.456628
3508.927013	968021.615743	42.461632
3508.999866	967847.524064	42.466637
3508.735465	967688.259060	42.471642
3508.395210	967528.219255	42.476647
3508.870284	967366.377011	42.481652
3508.824605	967197.667578	42.486656
3508.829473	967042.254897	42.491661
3508.722615	966873.741762	42.496666
3508.343999	966716.915390	42.501671
3508.563497	966558.909564	42.506676
3508.526679	966407.499490	42.511680
3508.596094	966236.002245	42.516685
3508.573906	966082.036263	42.521690
3508.372179	965929.466147	42.526695
3508.189875	965760.541233	42.531700
3508.029195	965613.437778	42.536704
3508.274993	965457.746753	42.541709
3508.348592	965307.366340	42.546714
3508.314842	965159.153475	42.551719
3507.848503	965009.735322	42.556724
3507.655282	964863.890771	42.561728
3507.973588	964713.062877	42.566733
3508.002955	964566.292940	42.571738
3507.630244	964421.445832	42.576743
3508.130304	964275.667971	42.581748
3507.903707	964138.231186	42.586752
3507.711425	963987.370459	42.591757
3507.929779	963847.111657	42.596762
3507.813709	963703.673017	42.601767
3507.916287	963547.953879	42.606772
3507.344703	963404.386960	42.611776
3507.583953	963268.419515	42.616781
3507.559983	963138.074479	42.621786
3507.153605	962998.485512	42.626791
3507.862073	962854.302236	42.631796
3507.385848	962723.140852	42.636800
3507.510027	962580.124322	42.641805
3507.627272	962452.189079	42.646810
3507.235291	962306.802140	42.651815
3507.445713	962169.736057	42.656820
3507.148279	962029.811783	42.661824
3507.441312	961891.452075	42.666829
3507.305238	961755.118893	42.671834
3507.253637	961630.033970	42.676839
3507.366335	961488.069760	42.681844
3507.299808	961362.393708	42.686848
3507.398054	961217.486273	42.691853
3507.239929	961094.954415	42.696858
3507.345822	960958.072650	42.701863
3507.303003	960815.431680	42.706868
3507.078698	960698.388816	42.711872
3507.302259	960555.795508	42.716877
3507.414746	960431.147402	42.721882
3507.104895	960294.024406	42.726887
3507.256817	960156.038192	42.731892
3507.124508	960027.404291	42.736896
3506.738896	959888.716330	42.741901
3506.962738	959769.229003	42.746906
3506.867544	959644.500100	42.751911
3506.925998	959513.471447	42.756916
3506.844359	959395.006649	42.761920
3507.207311	959262.158157	42.766925
3506.939402	959132.742618	42.771930
3506.798027	959008.693578	42.776935
3506.680686	958877.973453	42.781940
3506.629822	958768.115286	42.786945
3506.678042	958635.598233	42.791949
3506.963429	958514.702616	42.796954
3506.669969	958393.605779	42.801959
3506.695803	958268.533114	42.806964
3506.415701	958148.115038	42.811969
3506.340207	958025.896357	42.816973
3506.671989	957924.584943	42.821978
3506.514562	957807.864422	42.826983
3506.585857	957666.204965	42.831988
3506.113653	957558.059617	42.836993
3506.337116	957447.640950	42.841997
3506.181271	957325.910827	42.847002
3506.356864	957207.946904	42.852007
3506.609089	957094.477653	42.857012
3506.214062	956989.348070	42.862017
3506.616637	956864.771133	42.867021
3506.567676	956751.050626	42.872026
3506.749296	956636.701621	42.877031
3506.449069	956511.154340	42.882036
3506.141466	956388.939210	42.887041
3506.039527	956282.277718	42.892045
3505.832656	956178.377015	42.897050
3505.843010	956065.319588	42.902055
3505.926090	955960.386647	42.907060
3506.203830	955862.185738	42.912065
3506.202064	955743.632758	42.917069
3506.091203	955627.939114	42.922074
3506.170125	955516.232506	42.927079
3506.321278	955400.000811	42.932084
3505.866580	955298.674809	42.937089
3505.919100	955188.731430	42.942093
3505.882523	955081.742776	42.947098
3505.938519	954971.108184	42.952103
3505.788404	954859.328527	42.957108
3505.647802	954763.531657	42.962113
3505.697201	954651.126642	42.967117
3505.826358	954544.689206	42.972122
3505.719650	954453.099057	42.977127
3505.981701	954349.578592	42.982132
3505.498496	954256.478010	42.987137
3505.727371	954145.701043	42.992141
3505.497183	954048.043406	42.997146
3505.627747	953949.932325	43.002151
3505.771328	953828.177179	43.007156
3505.604913	953735.212187	43.012161
3505.511788	953630.560225	43.017165
3505.622959	953542.549292	43.022170
3505.238681	953443.042959	43.027175
3505.575515	953340.276889	43.032180
3505.240922	953243.603859	43.037185
3505.460356	953143.208085	43.042189
3505.529339	953042.639143	43.047194
3505.165172	952948.614906	43.052199
3505.298335	952853.428008	43.057204
3505.213109	952770.146903	43.062209
3505.460032	952669.934605	43.067213
3505.382037	952579.291140	43.072218
3505.366004	952485.952673	43.077223
3505.695487	952391.710007	43.082228
3505.343726	952305.036608	43.087233
3505.436766	952202.988120	43.092237
3505.344784	952108.044619	43.097242
3505.111543	952022.207536	43.102247
3505.191538	951922.928870	43.107252
3504.867870	951829.644097	43.112257
3504.813369	951750.467379	43.117261
3504.969477	951671.828557	43.122266
3505.132520	951587.257777	43.127271
3505.004919	951494.317117	43.132276
3504.888891	951412.276062	43.137281
3505.145148	951324.720667	43.142285
3505.094531	951239.988040	43.147290
3504.795218	951148.695335	43.152295
3505.089383	951057.303224	43.157300
3504.823984	950975.088445	43.162305
3504.993848	950894.235411	43.167309
3504.802137	950814.110236	43.172314
3505.001221	950727.223582	43.177319
3504.961787	950641.235654	43.182324
3504.974239	950569.777746	43.187329
3505.032001	950464.639221	43.192333
3504.983824	950382.092122	43.197338
3504.800406	950309.993217	43.202343
3505.189586	950213.213233	43.207348
3504.994515	950139.487545	43.212353
3504.921665	950046.607158	43.217357
3504.891751	949959.266833	43.222362
3504.822911	949885.803695	43.227367
3504.917870	949798.822740	43.232372
3504.823192	949720.386520	43.237377
3504.579562	949634.606636	43.242381
3504.774401	949553.823956	43.247386
3504.797689	949466.275092	43.252391
3504.639980	949386.600316	43.257396
3504.466096	949308.553548	43.262401
3504.402858	949226.277311	43.267405
3504.675320	949152.077627	43.272410
3504.355499	949084.672444	43.277415
3504.722300	949006.436310	43.282420
3504.346602	948933.488485	43.287425
3504.358779	948849.375686	43.292429
3504.380823	948780.379134	43.297434
3504.550560	948708.869313	43.302439
3504.476345	948633.092452	43.307444
3504.417463	948558.268899	43.312449
3504.532824	948477.960823	43.317453
3504.185256	948405.862119	43.322458
3504.657501	948330.947749	43.327463
3504.794781	948263.839256	43.332468
3504.468557	948186.853202	43.337473
3504.403928	948097.859898	43.342477
3504.535406	948029.409437	43.347482
3504.160593	947955.777603	43.352487
3504.448650	947886.055247	43.357492
3504.573046	947821.144372	43.362497
3504.291303	947734.286133	43.367501
3504.128789	947653.723801	43.372506
3504.114764	947588.067084	43.377511
3504.359041	947504.276842	43.382516
3504.111479	947449.951207	43.387521
3504.339189	947380.806233	43.392525
3504.232132	947309.035355	43.397530
3504.259337	947238.102836	43.402535
3504.266536	947159.897800	43.407540
3503.880213	947091.615865	43.412545
3503.765221	947026.638665	43.417549
3504.085956	946964.269167	43.422554
3503.977433	946897.661942	43.427559
3504.193019	946839.041580	43.432564
3503.705342	946764.836887	43.437569
3504.042797	946709.162563	43.442573
3504.079637	946627.881192	43.447578
3503.827499	946572.972647	43.452583
3504.153622	946497.864173	43.457588
3503.855499	946433.866991	43.462593
3504.066683	946365.572709	43.467597
3504.252927	946299.770808	43.472602
3503.630882	946229.792979	43.477607
3503.866302	946164.651422	43.482612
3503.785839	946110.762800	43.487617
3503.978541	946053.477639	43.492621
3504.069942	945986.921429	43.497626
3503.837531	945913.236853	43.502631
3503.767539	945844.790499	43.507636
3503.808210	945793.655238	43.512641
3504.170689	945730.785193	43.517645
3503.917251	945655.951422	43.522650
3503.781030	945600.917658	43.527655
3503.791272	945529.868637	43.532660
3503.709107	945478.558982	43.537665
3504.061256	945414.346243	43.542669
3504.079630	945356.794799	43.547674
3503.578894	945290.614414	43.552679
3503.982448	945220.741171	43.557684
3503.934394	945173.636196	43.562689
3503.916473	945104.405365	43.567693
3503.967594	945043.972241	43.572698
3503.629088	944977.761112	43.577703
3504.240206	944905.838409	43.582708
3503.820891	944849.311044	43.587713
3504.058164	944775.149763	43.592717
3504.038627	944718.172036	43.597722
3503.599013	944657.432164	43.602727
3503.875436	944593.892076	43.607732
3503.749160	944528.693681	43.612737
3503.449470	944480.474589	43.617741
3503.756972	944406.775306	43.622746
3503.356930	944357.326550	43.627751
3503.486877	944288.251961	43.632756
3503.603494	944242.643760	43.637761
3503.554368	944169.382949	43.642765
3503.550487	944114.503080	43.647770
3503.444989	944060.309824	43.652775
3503.394237	944001.605311	43.657780
3503.131279	943944.467592	43.662785
3503.608402	943884.046498	43.667789
3503.637805	943832.989453	43.672794
3503.250611	943789.567490	43.677799
3503.670192	943731.357130	43.682804
3503.305608	943670.018568	43.687809
3503.413941	943618.659045	43.692813
3503.371606	943571.059575	43.697818
3503.032624	943517.665401	43.702823
3503.364422	943460.424350	43.707828
3503.432773	943415.391550	43.712833
3503.473671	943362.603730	43.717837
3503.337807	943311.281388	43.722842
3503.138341	943248.473726	43.727847
3503.441699	943200.334926	43.732852
3503.504480	943143.805262	43.737857
3503.427182	943093.620666	43.742861
3503.433463	943028.573109	43.747866
3503.313794	942989.315471	43.752871
3503.250557	942922.074652	43.757876
3503.331419	942886.519405	43.762881
3503.378470	942825.390414	43.767885
3502.988880	942780.044325	43.772890
3503.390451	942722.975242	43.777895
3503.479523	942675.633305	43.782900
3503.114859	942619.647365	43.787905
3503.280618	942573.441530	43.792909
3503.052858	942514.940930	43.797914
3502.978208	942472.510302	43.802919
3502.979630	942429.204510	43.807924
3503.114430	942378.594809	43.812929
3503.210178	942324.733467	43.817933
3503.408145	942272.866783	43.822938
3503.273704	942230.827276	43.827943
3503.245767	942165.008016	43.832948
3503.228925	942124.864560	43.837953
3503.083203	942064.620694	43.842957
3503.256745	942019.366804	43.847962
3503.259338	941976.248673	43.852967
3503.153504	941935.639326	43.857972
3502.957768	941884.504351	43.862977
3503.353648	941834.421250	43.867981
3503.436681	941791.000867	43.872986
3502.830295	941738.494788	43.877991
3503.174918	941679.794648	43.882996
3503.089068	941643.875058	43.888001
3503.092367	941597.399829	43.893005
3503.078199	941554.185129	43.898010
3502.959164	941497.954957	43.903015
3503.335875	941455.345826	43.908020
3502.987081	941410.939307	43.913025
3502.753429	941351.564103	43.918029
3502.940914	941309.368266	43.923034
3502.786415	941272.882440	43.928039
3503.131825	941226.060037	43.933044
3502.885411	941187.001298	43.938049
3502.748600	941143.324224	43.943053
3502.741442	941101.254598	43.948058
3502.887007	941061.459502	43.953063
3503.075219	941007.377598	43.958068
3502.678662	940973.900450	43.963073
3502.648045	940914.103453	43.968077
3502.820501	940887.815637	43.973082
3502.933099	940847.640985	43.978087
3502.990634	940799.712111	43.983092
3502.998374	940756.966371	43.988097
3502.691183	940712.930389	43.993101
3503.118123	940657.942955	43.998106
3502.897011	940629.897677	44.003111
3502.850044	940578.533651	44.008116
3502.921165	940527.341351	44.013121
3502.802573	940479.917770	44.018125
3502.674014	940442.367541	44.023130
3502.805912	940407.266145	44.028135
3502.910299	940358.942108	44.033140
3503.013730	940321.544484	44.038145
3503.021411	940266.142746	44.043149
3502.953896	940225.322021	44.048154
3502.850499	940186.903155	44.053159
3502.878109	940141.177713	44.058164
3502.684556	940110.920510	44.063169
3502.526851	940073.084862	44.068173
3502.725619	940021.962419	44.073178
3502.656607	939980.469045	44.078183
3502.797736	939940.857825	44.083188
3502.859927	939909.407056	44.088193
3502.667002	939867.741486	44.093197
3502.797365	939817.970304	44.098202
3502.573745	939776.404918	44.103207
3502.912757	939731.103867	44.108212
3502.774578	939697.671790	44.113217
3502.963866	939651.436117	44.118221
3503.323692	939607.280889	44.123226
3503.194430	939571.450000	44.128231
3502.994405	939525.181483	44.133236
3502.961426	939479.747808	44.138241
3503.029831	939423.847794	44.143245
3502.939129	939385.804387	44.148250
3502.798619	939346.426783	44.153255
3503.016326	939296.348636	44.158260
3502.785521	939265.996793	44.163265
3502.832836	939216.233552	44.168269
3503.051194	939174.974029	44.173274
3502.652107	939140.430929	44.178279
3502.934719	939095.613007	44.183284
3503.104615	939046.403176	44.188289
3502.599548	939004.782130	44.193293
3502.783435	938959.212323	44.198298
3502.725162	938924.324023	44.203303
3503.003440	938875.286473	44.208308
3502.707994	938835.355286	44.213313
3502.900565	938799.178443	44.218317
3502.759986	938755.002574	44.223322
3502.831181	938725.268970	44.228327
3502.775623	938674.175224	44.233332
3502.872852	938634.081927	44.238337
3502.692269	938584.829608	44.243341
3503.017193	938541.917569	44.248346
3502.623129	938511.204706	44.253351
3503.034109	938465.689064	44.258356
3502.813159	938430.536619	44.263361
3502.606174	938398.737560	44.268365
3502.711086	938345.696494	44.273370
3502.695451	938309.934104	44.278375
3502.406368	938271.148173	44.283380
3502.551818	938238.714763	44.288385
3502.431101	938193.859669	44.293389
3502.890497	938158.976862	44.298394
3502.583313	938124.411889	44.303399
3503.009066	938087.232821	44.308404
3502.743557	938046.715333	44.313409
3502.541023	938003.598105	44.318413
3502.649990	937962.059359	44.323418
3502.822680	937917.441232	44.328423
3503.154760	937872.508787	44.333428
3502.913567	937840.903754	44.338433
3503.037802	937791.593741	44.343437
3503.065141	937742.682809	44.348442
3502.471537	937717.560086	44.353447
3502.888005	937657.843889	44.358452
3502.713837	937633.514735	44.363457
3503.038439	937584.553353	44.368461
3502.899584	937542.668513	44.373466
3502.592765	937512.127195	44.378471
3503.121462	937461.788445	44.383476
3502.692434	937416.402072	44.388481
3502.664683	937370.565586	44.393485
3502.840122	937338.121657	44.398490
3502.617917	937308.140625	44.403495
3502.905900	937259.757662	44.408500
3502.741684	937219.696599	44.413505
3502.740259	937187.568590	44.418509
3502.801132	937133.275717	44.423514
3502.877900	937109.478226	44.428519
3503.177699	937053.322927	44.433524
3502.797631	937017.419926	44.438529
3502.809485	936971.381605	44.443533
3502.920345	936918.804649	44.448538
3502.476572	936886.939493	44.453543
3502.768803	936844.210756	44.458548
3502.567593	936808.564591	44.463553
3502.426364	936779.430403	44.468557
3502.833883	936722.486511	44.473562
3502.886704	936697.060550	44.478567
3502.897154	936643.346399	44.483572
3502.654677	936623.819585	44.488577
3502.604953	936578.267536	44.493581
3503.032444	936537.144602	44.498586
3502.683326	936499.122758	44.503591
3502.610417	936461.246972	44.508596
3502.929357	936424.457394	44.513601
3502.696135	936379.797128	44.518605
3502.724129	936339.697669	44.523610
3502.737787	936310.535358	44.528615
3502.656479	936263.163262	44.533620
3502.637086	936227.866884	44.538625
3502.468240	936185.016895	44.543629
3502.917141	936163.743756	44.548634
3502.629301	936125.037630	44.553639
3502.352331	936072.803864	44.558644
3502.445883	936044.490247	44.563649
3502.366539	936013.423074	44.568653
3502.537966	935985.096307	44.573658
3502.387891	935952.697439	44.578663
3502.295395	935907.242538	44.583668
3502.464826	935885.534670	44.588673
3502.263709	935848.443017	44.593677
3502.754658	935805.289370	44.598682
3502.526025	935773.286059	44.603687
3502.353375	935729.665526	44.608692
3502.682673	935713.782484	44.613697
3502.210871	935677.981344	44.618701
3502.645178	935636.658378	44.623706
3502.345728	935625.675355	44.628711
3502.412437	935552.082333	44.633716
3502.316211	935534.829820	44.638721
3502.380573	935501.721288	44.643725
3502.646917	935473.376128	44.648730
3502.257254	935447.441390	44.653735
3502.465143	935403.083890	44.658740
3502.425386	935376.419587	44.663745
3502.410719	935332.002213	44.668749
3502.419749	935303.314769	44.673754
3502.308388	935277.621163	44.678759
3502.759107	935228.425152	44.683764
3502.436992	935204.396914	44.688769
3502.320557	935158.939482	44.693773
3502.346551	935127.753772	44.698778
3502.338730	935088.322264	44.703783
3502.381881	935057.613033	44.708788
3502.378878	935035.066562	44.713793
3502.312356	934993.725114	44.718797
3502.379006	934962.051995	44.723802
3502.638062	934939.845729	44.728807
3502.881472	934906.703955	44.733812
3502.297765	934857.770845	44.738817
3502.702037	934824.698002	44.743821
3502.493970	934785.393162	44.748826
3502.202381	934767.402716	44.753831
3502.562618	934720.327764	44.758836
3502.509212	934695.389371	44.763841
3502.345210	934663.176745	44.768845
3502.538622	934627.354799	44.773850
3502.729056	934604.870570	44.778855
3502.673371	934562.468466	44.783860
3502.274328	934520.026632	44.788865
3502.344008	934484.416007	44.793869
3502.834539	934447.776251	44.798874
3502.327525	934416.962007	44.803879
3502.738627	934386.284198	44.808884
3502.478331	934345.065533	44.813889
3502.186864	934320.356498	44.818893
3502.435357	934280.492878	44.823898
3502.061251	934249.943635	44.828903
3502.430272	934215.049549	44.833908
3502.747364	934187.264871	44.838913
3502.859124	934152.604676	44.843917
3502.591166	934100.445777	44.848922
3502.588542	934074.056643	44.853927
3502.689367	934040.932916	44.858932
3502.387555	933989.738129	44.863937
3502.608329	933966.382503	44.868941
3502.210389	933931.420965	44.873946
3502.539734	933909.582644	44.878951
3502.233303	933868.655745	44.883956
3502.418170	933836.956386	44.888961
3502.253265	933810.688635	44.893965
3502.388167	933771.031814	44.898970
3502.349182	933749.733352	44.903975
3502.390052	933717.577156	44.908980
3502.302338	933681.219282	44.913985
3502.491216	933649.326196	44.918989
3502.572978	933612.076192	44.923994
3502.338939	933581.404020	44.928999
3502.410161	933547.706243	44.934004
3502.358322	933512.876852	44.939009
3502.592437	933481.071270	44.944013
3502.732290	933442.082975	44.949018
3502.324716	933413.549844	44.954023
3502.378330	933371.887949	44.959028
3502.314338	933339.458798	44.964033
3502.424900	933308.248385	44.969037
3502.602505	933270.884207	44.974042
3502.273114	933245.792464	44.979047
3502.403606	933209.875280	44.984052
3502.755290	933181.311785	44.989057
3502.379435	933147.205212	44.994061
3502.645656	933115.776059	44.999066
3502.620548	933087.178151	45.004071
3502.741810	933045.310573	45.009076
3502.600024	933015.387759	45.014081
3502.335743	932978.574221	45.019085
3502.305076	932947.288960	45.024090
3502.582374	932915.088924	45.029095
3502.572089	932874.489452	45.034100
3502.264779	932836.530198	45.039105
3502.475495	932815.666754	45.044109
3502.453751	932773.148680	45.049114
3502.320645	932742.167039	45.054119
3502.509384	932707.868622	45.059124
3502.479209	932673.222096	45.064129
3502.352059	932646.942326	45.069133
3502.514030	932605.160543	45.074138
3502.256747	932571.798627	45.079143
3502.448812	932539.322376	45.084148
3502.492281	932498.327195	45.089153
3502.256263	932463.137255	45.094157
3502.522102	932429.016312	45.099162
3502.374427	932408.018320	45.104167
3502.470668	932364.517592	45.109172
3502.474071	932330.631237	45.114177
3502.230626	932304.080938	45.119181
3502.110593	932274.534320	45.124186
3502.372334	932255.772159	45.129191
3501.919531	932213.416592	45.134196
3501.844555	932195.669655	45.139201
3502.043285	932164.533960	45.144205
3502.246693	932143.957065	45.149210
3501.797575	932105.823922	45.154215
3502.057973	932089.749348	45.159220
3502.056931	932064.885887	45.164225
3502.032363	932039.066189	45.169229
3502.406454	932005.308680	45.174234
3502.165175	931986.916438	45.179239
3501.633861	931952.731751	45.184244
3502.150299	931920.294264	45.189249
3502.278202	931908.561045	45.194253
3502.555870	931859.458161	45.199258
3502.062413	931848.307187	45.204263
3502.127493	931805.287011	45.209268
3501.837050	931794.390489	45.214273
3501.932706	931761.253320	45.219277
3501.914761	931733.894968	45.224282
3501.824771	931711.444626	45.229287
3502.002218	931690.006196	45.234292
3502.115335	931674.530663	45.239297
3501.805142	931639.635476	45.244301
3501.990888	931619.347474	45.249306
3502.070855	931594.948495	45.254311
3501.805150	931575.982800	45.259316
3501.998186	931547.916673	45.264321
3501.829621	931518.373826	45.269325
3502.180830	931494.121715	45.274330
3501.915392	931475.731673	45.279335
3501.666550	931454.746559	45.284340
3501.687323	931430.164552	45.289345
3501.946416	931397.766269	45.294349
3502.167542	931380.735905	45.299354
3501.751709	931356.225484	45.304359
3501.776706	931329.818089	45.309364
3501.710049	931319.075742	45.314369
3501.712420	931291.327705	45.319373
3501.759808	931257.139190	45.324378
3501.746621	931261.462054	45.329383
3501.752353	931230.256651	45.334388
3502.221287	931217.505577	45.339393
3502.112238	931192.559798	45.344397
3502.106171	931164.524443	45.349402
3501.955622	931147.554563	45.354407
3501.947799	931111.069823	45.359412
3501.672345	931084.326637	45.364417
3501.973154	931060.945002	45.369421
3502.184801	931041.610697	45.374426
3501.798054	931019.110291	45.379431
3501.998798	930996.032910	45.384436
3501.993870	930979.998687	45.389441
3501.871230	930951.789374	45.394445
3502.283297	930927.812709	45.399450
3501.993238	930900.974982	45.404455
3501.812095	930881.992866	45.409460
3501.923633	930855.184767	45.414465
3501.956801	930825.220733	45.419469
3502.347018	930801.343119	45.424474
3502.073130	930781.703769	45.429479
3502.015177	930749.929896	45.434484
3501.988787	930726.216601	45.439489
3501.930079	930703.756834	45.444493
3502.229836	930680.661771	45.449498
3501.995897	930665.528542	45.454503
3501.880543	930619.743757	45.459508
3502.034157	930590.622782	45.464513
3501.662849	930578.392709	45.469517
3501.901963	930551.754112	45.474522
3502.040195	930538.095630	45.479527
3502.051654	930508.997627	45.484532
3501.943917	930488.273515	45.489537
3501.850604	930460.728950	45.494541
3502.287476	930431.848524	45.499546
3502.184734	930424.471311	45.504551
3502.028370	930378.403111	45.509556
3502.164386	930371.370608	45.514561
3501.969166	930342.017650	45.519565
3502.357750	930323.227763	45.524570
3501.765919	930289.234347	45.529575
3501.778267	930260.422929	45.534580
3501.989355	930238.012773	45.539585
3502.038882	930210.059246	45.544589
3501.832839	930201.354282	45.549594
3501.922078	930163.886708	45.554599
3502.190001	930144.251766	45.559604
3501.965160	930125.466206	45.564609
3501.740882	930094.388047	45.569613
3502.167250	930068.676528	45.574618
3501.767000	930056.834156	45.579623
3501.915897	930031.264203	45.584628
3501.751337	930003.825040	45.589633
3501.735308	929988.269831	45.594637
3501.915691	929969.897144	45.599642
3501.676777	929927.007846	45.604647
3501.583816	929912.329429	45.609652
3501.648585	929908.669384	45.614657
3501.699791	929886.668240	45.619661
3501.901389	929865.890735	45.624666
3501.708922	929854.589912	45.629671
3501.547084	929814.856301	45.634676
3501.676890	929798.604231	45.639681
3501.670269	929791.018220	45.644685
3501.771491	929760.556763	45.649690
3501.517002	929750.418425	45.654695
3501.732585	929733.287656	45.659700
3501.596782	929712.277012	45.664705
3501.486194	929692.606720	45.669709
3501.619916	929667.805855	45.674714
3501.644296	929663.576041	45.679719
3501.524682	929636.991960	45.684724
3501.672089	929623.809833	45.689729
3501.469488	929619.041118	45.694733
3501.910195	929594.477468	45.699738
3501.797564	929575.287297	45.704743
3501.670378	929554.946920	45.709748
3501.615937	929530.272458	45.714753
3501.549975	929510.306004	45.719757
3501.557688	929492.440342	45.724762
3501.683290	929493.668318	45.729767
3501.628956	929456.411500	45.734772
3501.726559	929443.525272	45.739777
3501.504214	929438.279413	45.744781
3501.570458	929414.737092	45.749786
3501.460889	929403.325603	45.754791
3501.542247	929382.373925	45.759796
3501.337089	929389.323225	45.764801
3501.535250	929371.137637	45.769805
3501.835259	929339.488445	45.774810
3501.871455	929316.046686	45.779815
3501.706813	929216.182133	45.784820
3501.466156	929094.236115	45.789825
3501.769563	928908.416720	45.794829
3502.010107	928642.679036	45.799834
3501.463309	928337.190347	45.804839
3500.917612	927974.809004	45.809844
3500.869373	927553.808277	45.814849
3501.012289	927074.224794	45.819853
3500.898086	926523.431596	45.824858
3500.485810	925938.319710	45.829863
3500.522408	925264.926958	45.834868
3500.241304	924547.087918	45.839873
3500.282499	923756.604058	45.844877
3499.732883	922905.422135	45.849882
3499.243968	921985.807949	45.854887
3498.818852	921010.712974	45.859892
3498.819990	919972.446722	45.864897
3498.300648	918871.514206	45.869901
3498.014950	917681.282888	45.874906
3497.547201	916434.883278	45.879911
3497.363683	915121.222289	45.884916
3496.852141	913728.793959	45.889921
3496.165190	912290.081040	45.894925
3495.984192	910772.649336	45.899930
3495.248673	909188.949848	45.904935
3494.668549	907531.577419	45.909940
3494.240057	905793.812203	45.914945
3493.206497	904005.619305	45.919949
3492.593758	902141.879074	45.924954
3491.886240	900216.894577	45.929959
3491.341168	898218.005761	45.934964
3490.877216	896145.247104	45.939969
3489.699076	894020.808641	45.944973
3489.178163	891803.407413	45.949978
3488.573414	889534.660937	45.954983
3487.793750	887191.493543	45.959988
3486.830390	884797.348460	45.964993
3485.973674	882301.460185	45.969997
3485.383860	879767.150675	45.975002
3484.313063	877167.062889	45.980007
3483.455393	874478.693248	45.985012
3482.534192	871740.594986	45.990017
3481.001690	868925.128458	45.995021
3480.416358	866052.332724	46.000026
3479.370208	863121.491776	46.005031
3478.070771	860110.912109	46.010036
3477.432795	857037.746338	46.015041
3476.063526	853904.767939	46.020045
3475.355217	850700.469105	46.025050
3474.123008	847444.918331	46.030055
3472.845601	844116.816401	46.035060
3471.917956	840713.899075	46.040065
3470.104929	837272.758501	46.045069
3469.010080	833740.848214	46.050074
3467.804190	830163.644832	46.055079
3466.389409	826527.079049	46.060084
3465.524238	822811.089974	46.065089
3464.068094	819049.263694	46.070093
3462.922261	815206.388694	46.075098
3461.307933	811323.227191	46.080103
3459.828863	807348.265050	46.085108
3458.629830	803334.842343	46.090113
3457.012245	799238.178419	46.095117
3455.805785	795086.341738	46.100122
3453.948040	790886.163381	46.105127
3452.577469	786619.106714	46.110132
3450.853283	782290.675346	46.115137
3449.156191	777901.755483	46.120141
3447.595871	773450.424504	46.125146
3445.686811	768948.356018	46.130151
3444.408145	764383.737977	46.135156
3442.840718	759760.782299	46.140161
3440.864343	755069.954301	46.145165
3439.564692	750324.369753	46.150170
3437.774126	745523.462031	46.155175
3435.833180	740650.538438	46.160180
3434.128454	735734.637578	46.165185
3431.947973	730746.418924	46.170189
3430.102716	725708.546193	46.175194
3428.114473	720626.351336	46.180199
3426.320912	715473.343353	46.185204
3424.205639	710267.390219	46.190209
3422.044454	705006.206274	46.195213
3420.012207	699698.751599	46.200218
3417.982724	694335.110423	46.205223
3415.802286	688910.574113	46.210228
3414.074574	683438.773237	46.215233
3411.824413	677913.753285	46.220237
3409.643422	672316.176738	46.225242
3407.221211	666678.340964	46.230247
3404.610029	660991.283493	46.235252
3402.523239	655264.192496	46.240257
3400.099095	649482.302692	46.245261
3398.061597	643661.155136	46.250266
3395.258923	637787.020389	46.255271
3392.912998	631859.764007	46.260276
3390.351152	625889.933809	46.265281
3388.166757	619881.680184	46.270285
3385.677655	613818.566055	46.275290
3383.121278	607718.384307	46.280295
3380.618050	601571.932172	46.285300
3378.317327	595373.449574	46.290305
3375.329778	589138.040277	46.295309
3372.591164	582852.386474	46.300314
3369.770439	576536.552592	46.305319
3366.700467	570187.720232	46.310324
3364.289427	563794.682313	46.315329
3361.517740	557361.289607	46.320333
3358.853260	550885.864975	46.325338
3355.856781	544380.242081	46.330343
3352.732490	537829.939948	46.335348
3349.948280	531251.044750	46.340353
3346.707680	524637.766458	46.345357
3343.703844	517982.191639	46.350362
3340.857301	511313.060327	46.355367
3337.908318	504595.086014	46.360372
3335.056059	497866.946050	46.365377
3331.688912	491078.109355	46.370381
3328.492732	484271.648320	46.375386
3325.292457	477440.867736	46.380391
3322.084053	470589.926107	46.385396
3319.095944	463692.547046	46.390401
3315.744533	456788.602734	46.395405
3312.573592	449834.015998	46.400410
3309.156987	442880.173903	46.405415
3305.751885	435890.486120	46.410420
3302.225632	428876.244355	46.415425
3298.678661	421843.056375	46.420429
3295.452262	414799.849735	46.425434
3291.456531	407737.460754	46.430439
3287.916634	400643.769219	46.435444
3284.206015	393546.769270	46.440449
3280.585411	386442.310941	46.445453
3276.706459	379300.511719	46.450458
3273.095337	372165.163248	46.455463
3269.381589	365019.507958	46.460468
3265.657580	357853.287441	46.465473
3261.318455	350702.503179	46.470477
3257.808258	343531.416676	46.475482
3253.844387	336358.593483	46.480487
3249.950856	329177.495976	46.485492
3245.875995	321987.998923	46.490497
3241.889738	314817.284718	46.495501
3237.724713	307623.738318	46.500506
3233.493436	300434.289272	46.505511
3229.637402	293252.216276	46.510516
3225.390314	286070.021713	46.515521
3220.953995	278892.499788	46.520525
3217.289559	271716.425070	46.525530
3212.846671	264549.605825	46.530535
3208.568908	257390.143219	46.535540
3204.475125	250232.877515	46.540545
3199.706505	243097.879100	46.545549
3195.348203	235948.715474	46.550554
3191.130580	228808.568161	46.555559
3186.710794	221628.002889	46.560564
3182.321471	214515.370092	46.565569
3177.876468	207446.723358	46.570573
3173.478608	200374.337103	46.575578
3168.932062	193332.097629	46.580583
3164.176225	186292.093715	46.585588
3159.716721	179283.962074	46.590593
3154.764284	172292.116315	46.595597
3150.214697	165323.673193	46.600602
3144.734261	158395.713844	46.605607
3139.955953	151485.917506	46.610612
3135.348144	144599.249706	46.615617
3130.329271	137754.992384	46.620621
3125.097732	130935.171627	46.625626
3119.799272	124163.968620	46.630631
3114.442517	117420.835644	46.635636
3109.138817	110727.198765	46.640641
3103.477477	104078.848455	46.645645
3098.087838	97476.907948	46.650650
3092.494281	90921.885681	46.655655
3086.335386	84436.051735	46.660660
3080.749410	77988.670021	46.665665
3074.351593	71624.554427	46.670669
3068.147203	65320.874309	46.675674
3061.121152	59081.570823	46.680679
3053.835272	52926.748201	46.685684
3045.922000	46884.921267	46.690689
3035.327491	41021.162934	46.695693
3017.701670	35463.189243	46.700698
2996.729693	30223.233450	46.705703
2971.962229	25368.763870	46.710708
2945.591975	20949.574723	46.715713
2918.079306	17006.135191	46.720717
2892.847108	13518.876463	46.725722
2869.740023	10502.631807	46.730727
2849.028231	7942.772446	46.735732
2830.906634	5799.403283	46.740737
2815.601768	4050.527406	46.745741
2803.170770	2657.561257	46.750746
2792.178425	1581.765510	46.755751
2782.683054	777.004479	46.760756
2770.523138	306.669610	46.765761
2750.726898	311.875863	46.770765
2742.723413	293.061986	46.775770
2743.892586	297.993354	46.780775
2749.275956	302.444098	46.785780
2756.267957	294.439157	46.790785
2760.423718	297.043648	46.795789
2762.716665	287.554468	46.800794
2762.369356	296.606343	46.805799
2760.169743	286.952612	46.810804
2757.165902	286.699984	46.815809
2753.883074	289.085292	46.820813
2751.240150	282.519718	46.825818
2748.215320	282.474611	46.830823
2745.241486	287.182580	46.835828
2742.420552	285.849128	46.840833
2739.581262	287.075086	46.845837
2737.295347	280.391412	46.850842
2734.749159	284.349570	46.855847
2731.585772	285.480606	46.860852
2728.533656	276.299494	46.865857
2725.038484	286.224010	46.870861
2721.965895	279.502406	46.875866
2719.082587	275.520661	46.880871
2715.666737	278.931625	46.885876
2713.139160	264.212192	46.890881
2709.612023	274.160929	46.895885
2705.994229	277.982934	46.900890
2703.183608	271.797124	46.905895
2699.783600	270.941305	46.910900
2696.445841	268.980755	46.915905
2692.703989	274.587087	46.920909
2689.631476	272.918651	46.925914
2686.655882	272.912030	46.930919
2683.376018	264.364117	46.935924
2680.533773	264.096711	46.940929
2676.352786	260.721050	46.945933
2673.203553	260.687045	46.950938
2669.626045	265.667929	46.955943
2666.533426	258.854164	46.960948
2663.001526	253.475344	46.965953
2659.622787	254.890611	46.970957
2656.735761	250.182910	46.975962
2653.400783	251.231797	46.980967
2649.305175	257.176359	46.985972
2646.401454	255.943458	46.990977
2642.508421	256.037344	46.995981
2639.290855	252.937677	47.000986
2636.118869	252.057694	47.005991
2632.677602	253.332133	47.010996
2629.376885	252.570491	47.016001
2625.886201	249.195420	47.021005
2622.377235	252.942289	47.026010
2618.986190	249.363305	47.031015
2615.605294	247.201935	47.036020
2612.487312	247.471454	47.041025
2608.323360	252.816353	47.046029
2604.757535	247.775896	47.051034
2602.299652	250.901354	47.056039
2598.857415	247.112179	47.061044
2595.671265	241.390999	47.066049
2591.350898	243.831195	47.071053
2587.433490	239.675243	47.076058
2584.514821	239.983325	47.081063
2581.344816	241.294336	47.086068
2578.184048	241.255585	47.091073
2574.372402	243.770107	47.096077
2570.843973	240.344079	47.101082
2567.045579	238.323083	47.106087
2563.077123	237.942043	47.111092
2560.689829	233.090760	47.116097
2556.969265	248.086738	47.121101
2553.872134	243.023831	47.126106
2550.420830	236.226333	47.131111
2547.030833	245.974119	47.136116
2543.254353	238.217928	47.141121
2539.477033	236.387659	47.146125
2536.186085	233.081523	47.151130
2533.235663	234.633786	47.156135
2529.035520	226.203556	47.161140
2525.971720	232.194593	47.166145
2522.308297	234.659430	47.171149
2519.126935	228.089739	47.176154
2515.422873	233.738093	47.181159
2511.971721	235.552197	47.186164
2508.419022	229.816196	47.191169
2504.593430	232.487785	47.196173
2501.616628	232.049691	47.201178
2498.475601	228.907102	47.206183
2494.611127	231.967564	47.211188
2491.512680	227.688369	47.216193
2487.833442	228.547506	47.221197
2484.244770	224.121101	47.226202
2480.656776	226.468531	47.231207
2476.837868	225.209969	47.236212
2473.708258	228.401358	47.241217
2470.021142	229.811207	47.246221
2467.132546	228.367921	47.251226
2463.208648	221.002404	47.256231
2459.817659	217.517863	47.261236
2456.275643	216.685261	47.266241
2453.096286	224.800252	47.271245
2449.560342	223.140186	47.276250
2446.026998	218.209748	47.281255
2442.341376	222.305581	47.286260
2438.951046	220.819224	47.291265
2435.526390	223.968164	47.296269
2432.009033	213.355221	47.301274
2428.920533	225.692540	47.306279
2424.743283	228.369740	47.311284
2421.264600	220.051814	47.316289
2418.069791	222.420427	47.321293
2414.723123	219.347361	47.326298
2411.226191	219.683109	47.331303
2407.655218	220.693358	47.336308
2404.451777	219.401541	47.341313
2400.544366	217.781910	47.346317
2396.934613	216.063024	47.351322
2393.680389	220.965060	47.356327
2389.908779	222.217227	47.361332
2387.032618	221.361593	47.366337
2382.853036	223.712415	47.371341
2379.516412	224.588882	47.376346
2376.625940	222.902836	47.381351
2372.668228	222.737252	47.386356
2369.069483	218.266818	47.391361
2365.444476	221.221144	47.396365
2362.229211	217.474409	47.401370
2358.904041	218.795384	47.406375
2355.273639	222.446828	47.411380
2352.090650	210.381384	47.416385
2348.675670	212.026819	47.421389
2345.138162	216.350668	47.426394
2341.030520	214.419582	47.431399
2337.938821	221.145092	47.436404
2334.433444	209.718393	47.441409
2330.536016	211.446640	47.446413
2327.399267	208.404502	47.451418
2323.902514	210.439980	47.456423
2320.219851	212.291246	47.461428
2316.859266	205.173088	47.466433
2313.246174	221.387981	47.471437
2310.028520	204.642434	47.476442
2306.690355	206.084782	47.481447
2302.810450	213.623032	47.486452
2299.427480	208.030277	47.491457
2295.370874	208.719386	47.496461
2291.995762	208.098133	47.501466
2288.987182	202.451671	47.506471
2285.518042	211.244697	47.511476
2282.706439	209.286186	47.516481
2278.953316	210.501639	47.521485
2275.337137	212.181919	47.526490
2271.371426	209.480724	47.531495
2267.539723	210.403281	47.536500
2264.660712	205.372262	47.541505
2261.093568	215.317576	47.546509
2257.317625	211.299979	47.551514
2254.246952	204.600124	47.556519
2250.320483	206.724555	47.561524
2246.756179	205.172927	47.566529
2243.080077	205.445821	47.571533
2239.894552	204.561428	47.576538
2236.917374	207.307257	47.581543
2233.033230	209.615147	47.586548
2229.588966	203.158543	47.591553
2225.835940	206.325325	47.596557
2222.642129	197.726490	47.601562
2219.041111	197.823806	47.606567
2215.462297	197.071262	47.611572
2212.230683	201.682539	47.616577
2208.916033	202.496881	47.621581
2205.011014	201.230651	47.626586
2201.417894	194.730371	47.631591
2197.802951	203.196254	47.636596
2194.419587	198.607320	47.641601
2191.011148	210.099868	47.646605
2187.898638	202.429540	47.651610
2184.479867	198.732914	47.656615
2180.589327	204.697042	47.661620
2177.128487	192.503373	47.666625
2173.508960	196.209780	47.671629
2170.087212	204.744230	47.676634
2166.209990	193.693445	47.681639
2162.840283	202.484530	47.686644
2159.866066	192.610780	47.691649
2156.213450	203.565058	47.696653
2152.696834	200.214565	47.701658
2149.507422	199.710557	47.706663
2145.524713	200.441462	47.711668
2142.162280	197.239968	47.716673
2138.213527	206.082477	47.721677
2134.994007	199.001751	47.726682
2131.192439	197.721065	47.731687
2128.221859	201.785482	47.736692
2125.174216	192.565040	47.741697
2121.439949	193.006095	47.746701
2117.655573	193.066272	47.751706
2114.096001	193.153664	47.756711
2110.318279	191.320847	47.761716
2107.174981	189.162252	47.766721
2103.165506	196.967721	47.771725
2099.935059	197.578194	47.776730
2096.534458	196.370055	47.781735
2092.931165	190.258726	47.786740
2089.954173	185.961338	47.791745
2086.338437	189.519371	47.796749
2082.929079	190.756945	47.801754
2079.385220	181.302149	47.806759
2075.817758	195.100685	47.811764
2072.129090	188.346526	47.816769
2068.349416	194.482661	47.821773
2065.021016	190.093339	47.826778
2061.776869	193.832560	47.831783
2058.126050	193.250685	47.836788
2054.844318	183.869446	47.841793
2050.974234	192.847617	47.846797
2047.525548	194.150320	47.851802
2044.071009	190.796567	47.856807
2040.463569	189.926136	47.861812
2036.933792	183.239901	47.866817
2033.886909	187.747170	47.871821
2030.531301	185.670063	47.876826
2026.902168	187.674917	47.881831
2022.855557	183.686432	47.886836
2019.246594	185.506605	47.891841
2016.146160	190.283809	47.896845
2012.579102	188.777216	47.901850
2009.148802	187.225938	47.906855
2005.528676	189.634262	47.911860
2002.343244	183.044125	47.916865
1998.628924	199.108745	47.921869
1994.799372	188.249366	47.926874
1991.434572	179.917340	47.931879
1988.100953	188.721114	47.936884
1984.723608	182.814104	47.941889
1981.173336	192.286336	47.946893
1978.069149	184.382526	47.951898
1974.762342	195.165346	47.956903
1970.577269	191.070514	47.961908
1967.096669	189.301225	47.966913
1963.601568	192.775683	47.971917
1959.942771	191.314275	47.976922
1956.810381	184.122800	47.981927
1952.831292	187.404277	47.986932
1949.848322	181.153517	47.991937
1945.914588	188.332271	47.996941
1942.559529	187.173754	48.001946
1939.289282	189.652611	48.006951
1935.523789	185.754135	48.011956
1931.938124	190.076346	48.016961
1928.825312	189.687908	48.021965
1925.245197	192.178880	48.026970
1921.701487	179.985707	48.031975
1917.703236	193.634466	48.036980
1914.621173	182.826745	48.041985
1910.954532	185.673021	48.046989
1907.392967	180.068630	48.051994
1904.074367	177.837696	48.056999
1900.430882	189.998142	48.062004
1897.468688	183.841471	48.067009
1893.796474	190.459844	48.072013
1890.085949	180.120038	48.077018
1886.885783	178.317713	48.082023
1883.092754	190.200941	48.087028
1879.659762	181.024602	48.092033
1876.151943	181.259915	48.097037
1872.408776	174.934871	48.102042
1869.348528	177.356392	48.107047
1865.588209	180.240670	48.112052
1862.026627	175.235642	48.117057
1858.521281	187.230618	48.122061
1855.096638	180.120844	48.127066
1851.944902	170.915442	48.132071
1848.150264	184.064098	48.137076
1844.621511	178.661941	48.142081
1840.843168	179.460179	48.147085
1837.470641	181.089478	48.152090
1834.206091	173.128005	48.157095
1830.546345	184.815195	48.162100
1827.210930	175.009059	48.167105
1823.651924	179.630645	48.172109
1819.971430	176.901080	48.177114
1816.816723	181.275519	48.182119
1813.011643	184.128750	48.187124
1809.508500	174.474264	48.192129
1805.974907	182.536028	48.197133
1802.669516	179.369371	48.202138
1799.222784	184.091425	48.207143
1795.147665	187.031904	48.212148
1792.044825	186.596521	48.217153
1788.392770	181.044867	48.222157
1785.143162	178.244348	48.227162
1781.804729	170.905887	48.232167
1777.929297	188.288436	48.237172
1774.904055	173.792836	48.242177
1771.297919	174.648326	48.247181
1767.460039	182.868130	48.252186
1764.034395	184.247346	48.257191
1760.137620	180.589752	48.262196
1757.014388	176.602495	48.267201
1753.585262	173.093410	48.272205
1750.161795	171.507254	48.277210
1746.849211	173.045015	48.282215
1743.207712	180.531246	48.287220
1739.702888	169.016782	48.292225
1735.814025	174.823873	48.297229
1732.428795	177.269566	48.302234
1729.172911	165.256161	48.307239
1725.074974	175.689685	48.312244
1722.256428	164.967255	48.317249
1718.690869	164.424446	48.322253
1715.033259	171.751537	48.327258
1711.397181	165.344610	48.332263
1707.734528	163.930219	48.337268
1704.528876	164.429113	48.342273
1701.158524	170.017756	48.347277
1696.931666	171.237130	48.352282
1694.193560	170.363058	48.357287
1690.690548	172.655369	48.362292
1687.294978	158.227154	48.367297
1683.499273	166.543843	48.372301
1679.844514	167.429735	48.377306
1676.608301	164.286280	48.382311
1672.473354	176.933196	48.387316
1669.587716	167.251997	48.392321
1666.215724	176.502365	48.397325
1662.792592	175.466794	48.402330
1659.155798	170.066654	48.407335
1655.497045	174.213464	48.412340
1651.945952	159.776045	48.417345
1648.403553	168.023873	48.422349
1645.029192	167.219828	48.427354
1641.441232	170.174468	48.432359
1637.908878	172.747150	48.437364
1635.104050	172.479904	48.442369
1631.285314	170.153014	48.447373
1627.447067	169.259862	48.452378
1623.960092	177.059869	48.457383
1620.377035	173.737545	48.462388
1616.591382	166.510604	48.467393
1613.296014	171.873790	48.472397
1609.771652	173.323498	48.477402
1606.958101	163.463882	48.482407
1602.970994	175.255229	48.487412
1599.586073	169.228216	48.492417
1595.935370	161.878946	48.497421
1592.253204	164.573702	48.502426
1588.498284	169.646379	48.507431
1585.011339	170.486263	48.512436
1582.093450	150.694287	48.517441
1578.828236	169.045095	48.522445
1574.876464	168.061420	48.527450
1571.593455	157.818223	48.532455
1567.914362	168.092864	48.537460
1564.359426	160.157884	48.542465
1560.969115	159.557624	48.547469
1557.426953	167.826983	48.552474
1554.070289	162.637186	48.557479
1550.164700	166.542072	48.562484
1547.262324	158.842844	48.567489
1543.197750	162.012081	48.572493
1539.873064	160.040342	48.577498
1536.544514	152.830300	48.582503
1532.754976	159.418968	48.587508
1529.403019	159.315804	48.592513
1525.842350	157.302755	48.597517
1522.336849	163.615780	48.602522
1518.985439	161.163612	48.607527
1515.571207	170.243248	48.612532
1512.145664	159.965832	48.617537
1508.607492	165.001171	48.622541
1504.516204	164.178551	48.627546
1501.263753	156.674752	48.632551
1497.780521	153.983897	48.637556
1494.325661	158.051345	48.642561
1490.929106	167.364486	48.647565
1487.335261	162.081719	48.652570
1484.191030	155.074906	48.657575
1480.038068	161.982186	48.662580
1476.793069	154.533614	48.667585
1473.355989	159.625286	48.672589
1469.485748	160.551489	48.677594
1466.509589	152.181526	48.682599
1462.766486	167.219317	48.687604
1459.649473	166.636325	48.692609
1455.845737	171.344396	48.697613
1452.378206	165.205251	48.702618
1449.033732	156.703367	48.707623
1445.335274	163.863145	48.712628
1441.610237	152.392255	48.717633
1438.257033	166.282632	48.722637
1434.365730	165.696785	48.727642
1431.143482	155.915697	48.732647
1427.585000	165.399300	48.737652
1424.754393	166.096296	48.742657
1421.244147	162.742960	48.747661
1417.386388	164.854529	48.752666
1413.988290	155.450820	48.757671
1409.745410	157.731818	48.762676
1406.745714	156.509238	48.767681
1402.985528	161.321449	48.772685
1399.815923	152.171656	48.777690
1396.576057	159.550300	48.782695
1392.930163	155.024524	48.787700
1389.421644	159.055132	48.792705
1385.736777	157.458779	48.797709
1381.830467	157.565352	48.802714
1379.055468	152.778035	48.807719
1375.520952	158.551500	48.812724
1371.990164	148.472960	48.817729
1368.232550	152.700254	48.822733
1364.539359	152.212165	48.827738
1361.676654	152.506409	48.832743
1357.750008	163.357287	48.837748
1353.986328	151.213826	48.842753
1350.373012	147.637623	48.847757
1347.061906	165.330903	48.852762
1343.723207	164.048165	48.857767
1340.397347	159.831453	48.862772
1336.797721	150.339364	48.867777
1333.500988	154.442752	48.872781
1329.829896	158.992436	48.877786
1326.314852	148.402003	48.882791
1322.685812	158.702475	48.887796
1319.667355	150.744747	48.892801
1316.090460	151.158845	48.897805
1311.897218	144.200844	48.902810
1308.969317	147.531681	48.907815
1304.940410	154.529698	48.912820
1301.683898	154.530313	48.917825
1298.034175	146.606303	48.922829
1294.642866	152.512245	48.927834
1291.320377	154.387433	48.932839
1287.346435	156.146725	48.937844
1284.193412	150.522491	48.942849
1280.954194	156.365414	48.947853
1277.423063	152.361275	48.952858
1273.683979	151.144972	48.957863
1270.084242	162.040348	48.962868
1266.806268	153.824024	48.967873
1263.094329	156.003178	48.972877
1259.575573	164.367340	48.977882
1256.505743	156.418149	48.982887
1253.004540	161.562211	48.987892
1248.771705	157.753617	48.992897
1245.458819	155.620698	48.997901
1242.499463	155.215051	49.002906
1238.749824	146.952006	49.007911
1234.790100	157.422842	49.012916
1231.479763	153.993397	49.017921
1228.343606	153.276184	49.022925
1224.522801	154.308480	49.027930
1220.710522	148.179951	49.032935
1217.544473	152.966309	49.037940
1214.546320	153.382100	49.042945
1210.751367	152.865965	49.047949
1207.279500	150.642730	49.052954
1203.867562	155.966447	49.057959
1199.964915	150.561713	49.062964
1196.663061	147.967606	49.067969
1193.118080	150.089218	49.072973
1189.622332	141.444235	49.077978
1186.273923	143.704841	49.082983
1182.247982	156.338631	49.087988
1179.073773	146.039890	49.092993
1175.493265	149.743723	49.097997
1171.883954	160.030183	49.103002
1168.839983	154.200337	49.108007
1165.441647	151.850720	49.113012
1161.752145	154.510315	49.118017
1158.041220	152.420772	49.123021
1154.367219	152.580500	49.128026
1151.416080	150.938615	49.133031
1147.376090	164.649856	49.138036
1144.032847	151.032630	49.143041
1140.288805	156.486287	49.148045
1137.015112	153.755745	49.153050
1133.624216	151.509315	49.158055
1129.853466	160.037378	49.163060
1126.469918	147.425957	49.168065
1123.285177	147.513502	49.173069
1119.512735	154.030979	49.178074
1116.209471	148.590964	49.183079
1112.623040	153.851042	49.188084
1109.276588	141.744612	49.193089
1105.562166	144.517300	49.198093
1102.084728	148.449042	49.203098
1098.568615	144.255493	49.208103
1094.836143	149.948021	49.213108
1091.542573	150.056148	49.218113
1087.878902	149.024868	49.223117
1084.370205	154.124112	49.228122
1081.375152	142.940174	49.233127
1077.477328	147.799860	49.238132
1074.152127	142.046386	49.243137
1070.330526	146.553068	49.248141
1066.495260	148.572008	49.253146
1063.332611	147.123222	49.258151
1060.162877	158.826579	49.263156
1056.717956	151.413568	49.268161
1052.858325	154.455008	49.273165
1049.223735	154.222707	49.278170
1046.483539	152.514636	49.283175
1042.215604	145.965704	49.288180
1038.903318	152.435572	49.293185
1035.962321	150.305058	49.298189
1032.024290	150.551367	49.303194
1028.477082	144.770109	49.308199
1024.759862	146.300888	49.313204
1021.258002	147.348892	49.318209
1018.065083	151.187472	49.323213
1014.135404	147.821140	49.328218
1010.921818	138.801089	49.333223
1007.469679	149.963497	49.338228
1004.139090	146.164807	49.343233
1000.753599	146.319182	49.348237
996.974028	153.107495	49.353242
993.447886	145.082806	49.358247
989.930350	148.798665	49.363252
986.498824	149.679761	49.368257
982.769557	145.402363	49.373261
979.071342	152.215914	49.378266
975.774018	139.005664	49.383271
972.710348	145.291983	49.388276
969.275931	142.057904	49.393281
965.449588	140.134628	49.398285
961.817560	143.957649	49.403290
958.470980	140.860609	49.408295
954.709490	137.046587	49.413300
951.448883	144.181673	49.418305
947.778136	136.721646	49.423309
944.130398	149.953554	49.428314
940.909727	140.259245	49.433319
937.201032	144.672965	49.438324
934.128714	132.214304	49.443329
930.643033	139.742027	49.448333
926.898270	145.625566	49.453338
923.644425	138.871952	49.458343
919.614899	143.114372	49.463348
916.164181	147.587468	49.468353
912.745561	142.087167	49.473357
909.206178	142.293308	49.478362
905.934437	143.227369	49.483367
902.381124	146.914872	49.488372
899.171945	141.286407	49.493377
895.578198	144.595204	49.498381
891.588999	149.107843	49.503386
888.070615	138.221566	49.508391
884.546829	150.885799	49.513396
881.673028	143.598121	49.518401
878.255777	137.036543	49.523405
874.203931	147.754755	49.528410
870.723510	143.321253	49.533415
867.264673	150.700529	49.538420
863.680116	138.660535	49.543425
860.247271	140.837067	49.548429
856.623089	141.670993	49.553434
853.638345	134.691971	49.558439
849.829054	143.010329	49.563444
846.533348	140.810146	49.568449
842.690086	138.360322	49.573453
839.512655	143.771207	49.578458
835.906382	143.008692	49.583463
831.947983	137.908938	49.588468
828.524865	146.036356	49.593473
825.315693	138.584161	49.598477
821.762855	135.984493	49.603482
818.326115	133.097643	49.608487
814.640667	137.824141	49.613492
811.291088	136.038622	49.618497
808.098214	134.555948	49.623501
803.874025	145.518608	49.628506
800.499987	137.751323	49.633511
797.421569	148.912832	49.638516
793.819839	137.918473	49.643521
790.590326	142.499718	49.648525
786.965356	142.849171	49.653530
783.360903	139.677705	49.658535
779.609936	151.672330	49.663540
775.980087	138.886872	49.668545
772.966518	142.663191	49.673549
769.254604	141.894919	49.678554
765.852956	141.653919	49.683559
762.429200	146.115957	49.688564
758.626306	146.288450	49.693569
755.279264	133.128065	49.698573
751.861675	139.633892	49.703578
747.922464	137.708561	49.708583
744.395421	139.970816	49.713588
741.493716	140.879897	49.718593
738.081272	135.021149	49.723597
733.948935	139.046298	49.728602
730.905462	135.138368	49.733607
727.344893	140.246843	49.738612
723.519890	133.665823	49.743617
720.327841	134.476919	49.748621
716.257270	131.572259	49.753626
712.922241	131.289693	49.758631
709.408236	137.332168	49.763636
705.935279	136.489886	49.768641
702.719747	131.164161	49.773645
699.145959	140.963561	49.778650
696.101636	128.989665	49.783655
691.958287	135.958368	49.788660
688.702585	137.972127	49.793665
685.434418	131.204896	49.798669
681.394338	144.463403	49.803674
678.088792	128.274609	49.808679
674.734239	141.830761	49.813684
671.117330	138.891940	49.818689
667.715473	127.738148	49.823693
663.687332	139.891381	49.828698
660.481662	129.145396	49.833703
657.147023	136.139786	49.838708
653.865744	133.131641	49.843713
650.158352	129.339924	49.848717
646.645340	128.567465	49.853722
643.270929	129.812339	49.858727
639.722983	144.163413	49.863732
636.079716	131.732955	49.868737
632.508826	133.589526	49.873741
628.921875	136.792618	49.878746
625.602093	128.765695	49.883751
622.338209	130.937145	49.888756
618.678428	133.653625	49.893761
614.944751	134.893036	49.898765
611.009655	132.051115	49.903770
608.367592	133.451121	49.908775
604.723962	132.509679	49.913780
600.628362	132.317909	49.918785
597.898711	128.744738	49.923789
594.143030	129.520515	49.928794
590.759656	127.763256	49.933799
586.680969	131.629882	49.938804
583.777000	129.194196	49.943809
580.264240	120.286566	49.948813
576.427859	131.181493	49.953818
572.990111	124.459189	49.958823
569.530226	136.948074	49.963828
565.923631	130.831314	49.968833
562.379826	121.888973	49.973837
558.782333	123.210092	49.978842
555.969763	127.459062	49.983847
551.835192	127.930719	49.988852
548.464973	132.498902	49.993857
545.333124	134.969429	49.998861
541.272844	138.213021	50.003866
538.276648	126.605049	50.008871
534.439105	141.624532	50.013876
530.981986	128.158739	50.018881
527.291476	128.403611	50.023885
523.812706	141.547258	50.028890
520.837205	125.009576	50.033895
517.317153	130.525711	50.038900
513.681977	129.444221	50.043905
510.030546	131.466954	50.048909
505.961933	128.228675	50.053914
502.632136	124.193455	50.058919
499.032120	127.847354	50.063924
495.814858	130.453410	50.068929
492.685081	120.165070	50.073933
489.205023	135.185612	50.078938
486.134658	117.760063	50.083943
482.465684	119.516555	50.088948
478.346406	126.072577	50.093953
474.905506	121.622810	50.098957
471.115831	132.260262	50.103962
468.226257	127.769585	50.108967
464.346398	113.417732	50.113972
460.799032	122.793382	50.118977
457.412224	123.928164	50.123981
453.713446	130.101254	50.128986
450.226661	123.008287	50.133991
446.855923	126.386890	50.138996
443.611951	132.956358	50.144001
440.197701	124.906155	50.149005
436.400374	127.617325	50.154010
432.956016	119.097720	50.159015
429.298343	122.421599	50.164020
425.447161	126.665715	50.169025
422.306281	125.518682	50.174029
418.910729	126.785973	50.179034
415.291140	118.674859	50.184039
412.092912	126.680878	50.189044
408.728762	117.838796	50.194049
404.795652	116.672320	50.199053
400.982458	135.152290	50.204058
397.943077	121.699191	50.209063
394.299644	117.063969	50.214068
390.653389	124.672320	50.219073
387.653615	121.003492	50.224077
384.255416	136.602957	50.229082
380.779424	123.452027	50.234087
376.555326	127.519719	50.239092
373.442483	126.564234	50.244097
369.800284	125.810027	50.249101
366.102638	130.224342	50.254106
362.708267	121.927013	50.259111
359.076765	125.167882	50.264116
355.769896	127.836229	50.269121
352.623267	123.228931	50.274125
348.770969	127.591501	50.279130
345.462671	118.632090	50.284135
341.801275	130.565820	50.289140
338.519565	114.513126	50.294145
335.065722	123.009453	50.299149
331.070776	130.010938	50.304154
327.772600	120.002210	50.309159
324.489181	138.488483	50.314164
320.847299	122.010163	50.319169
317.590367	127.143875	50.324173
313.463061	131.162453	50.329178
310.195890	113.435158	50.334183
306.702405	122.336881	50.339188
303.372090	123.629575	50.344193
300.121269	129.930713	50.349197
295.987425	136.005838	50.354202
292.838486	117.026230	50.359207
289.219750	129.091465	50.364212
285.416095	128.657888	50.369217
282.283606	129.550217	50.374221
278.829161	127.861410	50.379226
275.523342	117.508855	50.384231
272.047682	132.162749	50.389236
268.272254	129.554612	50.394241
264.703371	125.451612	50.399245
261.106673	129.191387	50.404250
257.455473	121.830592	50.409255
254.180504	130.983704	50.414260
250.971222	124.412515	50.419265
247.376867	121.037772	50.424269
243.436550	125.335475	50.429274
240.500770	110.860341	50.434279
236.612110	120.989636	50.439284
232.864913	120.000141	50.444289
229.629595	125.316424	50.449293
225.919598	128.685244	50.454298
222.847052	122.174522	50.459303
219.037197	137.525709	50.464308
215.549505	131.174683	50.469313
212.554193	122.337031	50.474317
208.457433	127.102694	50.479322
204.858715	123.371533	50.484327
201.490768	130.273478	50.489332
198.182063	123.197825	50.494337
194.658734	116.607831	50.499341
191.054022	129.597107	50.504346
187.567348	124.489548	50.509351
184.502122	120.092685	50.514356
180.609969	125.918528	50.519361
177.251438	124.397251	50.524365
173.650404	125.489179	50.529370
170.319906	118.655739	50.534375
166.566413	126.204857	50.539380
163.387166	119.809528	50.544385
160.002243	123.597204	50.549389
155.903639	122.825401	50.554394
152.596961	123.934129	50.559399
148.946596	128.577597	50.564404
145.464291	123.751146	50.569409
142.082427	119.921585	50.574413
138.419576	119.351163	50.579418
135.266907	118.586956	50.584423
131.807914	124.765594	50.589428
127.846845	122.152801	50.594433
124.885280	122.892625	50.599437
121.140798	127.736402	50.604442
117.736372	126.678025	50.609447
113.731339	130.560115	50.614452
110.552781	129.893355	50.619457
107.475963	128.844681	50.624461
103.605389	125.262418	50.629466
100.066736	121.182778	50.634471
96.283269	123.236792	50.639476
92.836655	116.173805	50.644481
89.690127	114.738466	50.649485
86.188992	116.931631	50.654490
82.925721	122.916677	50.659495
79.086394	113.608129	50.664500
75.263283	125.750176	50.669505
72.074586	117.869173	50.674509
68.471639	122.347380	50.679514
65.176483	120.078852	50.684519
61.618819	130.507508	50.689524
57.609662	130.487438	50.694529
54.547587	122.140886	50.699533
51.029062	119.486466	50.704538
47.930128	114.571367	50.709543
44.038666	121.192273	50.714548
40.301399	123.870354	50.719553
36.802602	120.543911	50.724557
33.341932	127.016339	50.729562
29.986281	120.253488	50.734567
26.508956	122.440786	50.739572
23.165072	112.119824	50.744577
19.975754	112.577947	50.749581
16.197590	129.433639	50.754586
12.304659	121.478670	50.759591
8.713827	127.738827	50.764596
5.165957	127.193684	50.769601
2.515526	118.435650	50.774605