Tue Jun 21 12:54:58 2022

Number of Points = 9930

Depth (nm)	Load (N)	Time (s)
-0.173501	76.031076	0.000000
0.179950	70.734971	0.005005
0.091218	68.404814	0.010010
-0.216792	72.959255	0.015014
-0.110249	59.521775	0.020019
-0.799369	62.080537	0.025024
-0.677241	53.794258	0.030029
-1.121394	43.784706	0.035034
-1.496962	35.967035	0.040038
-1.429396	25.015341	0.045043
-1.720726	14.208730	0.050048
-1.773531	6.982906	0.055053
-2.366945	-4.102229	0.060058
-3.114410	2.818767	0.065062
-3.146624	-10.676976	0.070067
-3.757771	-11.826596	0.075072
-4.077925	-3.562077	0.080077
-4.545869	-11.388304	0.085082
-4.525759	-10.840213	0.090086
-4.731597	-9.591667	0.095091
-4.952201	-3.229744	0.100096
-5.037822	-3.237990	0.105101
-4.731755	-10.261964	0.110106
-5.497283	-5.999808	0.115110
-5.947704	-9.369008	0.120115
-6.291973	-9.303244	0.125120
-6.436726	-4.088548	0.130125
-6.207365	-5.793134	0.135130
-6.882136	-4.483115	0.140134
-7.599057	-1.946596	0.145139
-7.866644	-3.328735	0.150144
-7.584595	-9.763639	0.155149
-7.628731	-1.678224	0.160154
-7.765860	1.255025	0.165158
-7.681280	-11.189721	0.170163
-8.866803	-10.361075	0.175168
-9.129317	-4.406414	0.180173
-9.466193	-16.810964	0.185178
-9.659341	-0.905029	0.190182
-9.177951	-8.967594	0.195187
-10.020027	-8.534445	0.200192
-10.764911	-8.351033	0.205197
-11.098461	-6.294767	0.210202
-11.161878	-7.663947	0.215206
-10.260821	-5.077261	0.220211
-11.088930	-1.191513	0.225216
-10.779045	-13.698036	0.230221
-11.387652	-6.827468	0.235226
-12.224611	-7.102013	0.240230
-12.292931	-13.824425	0.245235
-12.869314	-15.504509	0.250240
-12.655028	-10.359533	0.255245
-12.572519	-7.526791	0.260250
-12.965206	-8.221029	0.265254
-13.225140	-10.321346	0.270259
-13.645580	-2.200454	0.275264
-13.942293	-10.250592	0.280269
-14.173043	-4.155757	0.285274
-14.170390	0.788061	0.290278
-14.321868	-5.209395	0.295283
-15.249701	-2.632422	0.300288
-15.356489	-8.912557	0.305293
-15.580798	-4.264452	0.310298
-15.989038	-2.795512	0.315302
-15.783479	-14.155026	0.320307
-16.217045	-6.269551	0.325312
-16.300731	-5.047153	0.330317
-16.591954	-4.791063	0.335322
-17.044966	-3.550720	0.340326
-16.827809	-2.762940	0.345331
-17.434885	2.139177	0.350336
-17.532176	0.965835	0.355341
-17.887244	-4.620210	0.360346
-18.307255	-0.967407	0.365350
-18.423389	1.805288	0.370355
-18.725023	-0.055074	0.375360
-18.849015	-1.674111	0.380365
-18.826779	-1.155183	0.385370
-19.815498	4.232231	0.390374
-19.675363	-1.639272	0.395379
-20.206926	-3.122933	0.400384
-20.401053	-1.694778	0.405389
-20.559844	0.840288	0.410394
-20.958188	-2.440645	0.415398
-20.522494	1.804139	0.420403
-21.002834	-4.106889	0.425408
-21.707530	-7.537973	0.430413
-21.662476	-2.925199	0.435418
-22.230133	1.715436	0.440422
-21.816080	-11.107891	0.445427
-22.171124	-4.573732	0.450432
-22.504948	0.806264	0.455437
-23.133949	5.725235	0.460442
-23.686668	-8.745569	0.465446
-23.634034	-2.197225	0.470451
-23.840349	8.755861	0.475456
-23.788861	-2.132173	0.480461
-23.609069	-3.544392	0.485466
-24.257008	-1.240899	0.490470
-24.608736	-5.476157	0.495475
-25.404906	1.251428	0.500480
-25.868646	1.526813	0.505485
-25.613300	-9.230793	0.510490
-26.026119	-5.261673	0.515494
-25.581643	-11.147853	0.520499
-25.530511	-1.685044	0.525504
-26.016225	-9.018347	0.530509
-26.176832	-4.362636	0.535514
-27.041712	-2.485174	0.540518
-26.985167	-12.408486	0.545523
-27.914977	-3.856330	0.550528
-28.259705	-7.820624	0.555533
-28.284299	-8.886618	0.560538
-28.668912	-1.628084	0.565542
-28.509340	-9.159810	0.570547
-28.894637	1.053113	0.575552
-28.410201	-7.232352	0.580557
-28.075333	-6.190365	0.585562
-28.904568	4.006487	0.590566
-29.327976	-4.087396	0.595571
-30.467068	-0.841601	0.600576
-30.712428	-1.336262	0.605581
-30.401042	-3.066866	0.610586
-31.201409	-5.276991	0.615590
-31.358069	-5.955850	0.620595
-31.460106	1.992929	0.625600
-31.615378	-0.469461	0.630605
-31.671081	-11.278563	0.635610
-32.086649	-5.996327	0.640614
-31.710970	-3.532209	0.645619
-32.209737	0.632496	0.650624
-32.779692	4.973566	0.655629
-33.157782	0.445489	0.660634
-33.241427	-1.577462	0.665638
-33.243960	-1.556645	0.670643
-33.449957	4.777406	0.675648
-33.833661	-5.939296	0.680653
-34.569679	-5.289076	0.685658
-34.780564	-5.925606	0.690662
-35.103434	-6.558588	0.695667
-35.007795	-7.020920	0.700672
-35.080986	-4.110495	0.705677
-35.057430	-4.635876	0.710682
-35.274881	1.481623	0.715686
-35.918128	-5.813554	0.720691
-36.374968	2.264035	0.725696
-36.284590	-8.760278	0.730701
-36.208179	-8.208290	0.735706
-37.358704	0.928415	0.740710
-37.858328	-9.560703	0.745715
-38.127672	1.376372	0.750720
-37.709839	-4.129677	0.755725
-37.848416	1.991928	0.760730
-38.044158	2.063487	0.765734
-37.914596	-5.704608	0.770739
-38.284093	-1.504874	0.775744
-39.064614	-0.177337	0.780749
-39.380648	-6.683495	0.785754
-39.460486	1.506498	0.790758
-39.332757	-6.360750	0.795763
-39.899526	-2.976682	0.800768
-40.808176	-7.205746	0.805773
-41.310250	-8.534645	0.810778
-40.778398	-9.793625	0.815782
-40.485834	-7.957077	0.820787
-41.285008	1.197219	0.825792
-41.293181	-5.574030	0.830797
-41.339644	-10.886365	0.835802
-42.114996	-2.031029	0.840806
-42.539632	-11.409934	0.845811
-42.927242	1.076649	0.850816
-42.822450	3.994699	0.855821
-42.859403	-3.264328	0.860826
-42.936352	9.498191	0.865830
-42.913243	4.855524	0.870835
-43.986508	3.398428	0.875840
-44.198379	4.275410	0.880845
-44.106771	5.121276	0.885850
-44.524277	2.841039	0.890854
-44.200804	-4.781372	0.895859
-45.375170	-0.019738	0.900864
-45.721655	-5.101632	0.905869
-45.929157	-1.576570	0.910874
-45.983307	8.914221	0.915878
-45.755246	4.306088	0.920883
-45.990620	11.401582	0.925888
-45.787161	-1.621703	0.930893
-46.281697	2.903423	0.935898
-47.213519	4.760204	0.940902
-46.868177	-1.497126	0.945907
-47.372510	-4.170476	0.950912
-48.061313	-6.273175	0.955917
-48.532922	-5.802900	0.960922
-48.722083	-5.140233	0.965926
-48.452694	3.032378	0.970931
-48.895586	3.766665	0.975936
-49.246674	-0.081135	0.980941
-48.728758	-0.709895	0.985946
-49.119313	2.520081	0.990950
-49.535674	-11.699791	0.995955
-50.345289	-6.150820	1.000960
-50.939058	10.081749	1.005965
-50.705525	3.243632	1.010970
-51.202756	5.803371	1.015974
-51.041173	-1.609896	1.020979
-51.288577	4.871316	1.025984
-50.854629	1.418809	1.030989
-51.490832	-3.679634	1.035994
-52.115507	5.391106	1.040998
-52.021747	0.094815	1.046003
-52.310878	-3.364829	1.051008
-52.353311	-3.275245	1.056013
-52.956871	-8.939320	1.061018
-53.527556	1.724822	1.066022
-53.458128	-7.921397	1.071027
-53.650017	4.551522	1.076032
-53.962244	4.459248	1.081037
-54.121964	0.781825	1.086042
-54.884692	4.973671	1.091046
-54.977922	-8.708110	1.096051
-55.164475	-9.110093	1.101056
-55.308230	-10.458468	1.106061
-55.161081	-2.077952	1.111066
-55.684864	5.586854	1.116070
-55.794502	-6.877033	1.121075
-56.507598	-9.501402	1.126080
-56.746370	-8.098216	1.131085
-56.985625	-12.033797	1.136090
-57.187054	-6.187723	1.141094
-57.254782	-13.138741	1.146099
-57.204672	-1.186015	1.151104
-57.424963	-3.821155	1.156109
-57.963446	-7.100185	1.161114
-58.644977	1.250823	1.166118
-58.514515	-3.429354	1.171123
-58.737360	-7.624778	1.176128
-58.997072	-3.244511	1.181133
-59.594339	0.443176	1.186138
-60.070825	-0.275068	1.191142
-60.298820	-9.441843	1.196147
-60.587284	-2.389067	1.201152
-59.964649	-3.908370	1.206157
-60.053102	2.012533	1.211162
-60.596074	-3.717225	1.216166
-60.570948	-14.294422	1.221171
-61.370283	-4.112192	1.226176
-61.681348	-2.748142	1.231181
-61.745621	-8.860871	1.236186
-61.926889	-0.007619	1.241190
-61.804887	-7.208312	1.246195
-62.607294	0.607222	1.251200
-63.082065	-7.168729	1.256205
-63.198812	0.731769	1.261210
-63.958101	-2.141878	1.266214
-63.909744	0.643634	1.271219
-63.838120	0.762676	1.276224
-63.798618	-0.287884	1.281229
-63.428614	-1.471915	1.286234
-64.644181	5.537070	1.291238
-65.096465	2.674936	1.296243
-65.451333	0.451816	1.301248
-65.690841	-1.483357	1.306253
-65.291723	-6.850344	1.311258
-65.474878	7.742856	1.316262
-65.449035	-0.087786	1.321267
-66.190037	-4.137015	1.326272
-66.651371	0.330122	1.331277
-66.723026	-5.776846	1.336282
-67.030230	-3.218188	1.341286
-66.763287	-13.747619	1.346291
-67.763597	-3.473695	1.351296
-67.847574	-5.285244	1.356301
-67.986099	-9.429907	1.361306
-68.147858	-0.094447	1.366310
-68.054454	-5.183674	1.371315
-69.176541	-0.153638	1.376320
-69.287047	0.213620	1.381325
-69.220287	-3.801649	1.386330
-69.785582	-3.776630	1.391334
-69.547056	-7.357401	1.396339
-69.896770	-1.082235	1.401344
-70.772588	-5.932408	1.406349
-71.143972	-8.030839	1.411354
-71.248768	-6.729957	1.416358
-70.516628	-5.866050	1.421363
-71.466803	1.317430	1.426368
-71.594247	-5.874117	1.431373
-71.033157	0.816161	1.436378
-71.699141	-6.004207	1.441382
-72.340529	-11.751602	1.446387
-73.019075	3.344745	1.451392
-73.193645	2.706347	1.456397
-72.670975	-3.639945	1.461402
-72.972210	0.432849	1.466406
-73.735822	-4.447747	1.471411
-74.576578	3.415382	1.476416
-74.572273	1.701297	1.481421
-74.402735	2.647722	1.486426
-74.617942	0.329644	1.491430
-74.723945	0.268930	1.496435
-74.628180	-1.055769	1.501440
-74.802900	0.452448	1.506445
-75.138073	0.686024	1.511450
-76.099727	0.064511	1.516454
-76.403359	-13.305164	1.521459
-76.478705	-9.660108	1.526464
-76.532142	-5.347746	1.531469
-76.320163	-8.012837	1.536474
-77.353319	-7.624199	1.541478
-77.785461	-7.728974	1.546483
-77.893338	-2.072835	1.551488
-78.068022	0.982863	1.556493
-78.098913	-7.780842	1.561498
-78.419976	-5.276918	1.566502
-78.388680	-6.037421	1.571507
-78.141895	0.530861	1.576512
-78.725861	0.139839	1.581517
-79.222455	1.859624	1.586522
-79.475415	-9.373631	1.591526
-79.666510	-6.047238	1.596531
-80.472501	-4.173205	1.601536
-80.889914	-1.985435	1.606541
-80.705265	-3.499889	1.611546
-81.325459	-3.612394	1.616550
-81.052162	-4.955445	1.621555
-81.279698	3.753919	1.626560
-81.072373	4.298828	1.631565
-81.307355	-7.655106	1.636570
-82.065572	-2.126877	1.641574
-82.803725	-4.311380	1.646579
-82.788446	-3.166544	1.651584
-83.003267	-4.775469	1.656589
-82.609472	-1.179297	1.661594
-82.869842	2.335578	1.666598
-83.515092	-2.285984	1.671603
-84.375016	-3.320588	1.676608
-84.353985	3.803675	1.681613
-84.051697	-6.652878	1.686618
-84.597724	4.822563	1.691622
-84.849314	-12.627503	1.696627
-85.495057	-1.796815	1.701632
-85.885307	-6.246896	1.706637
-85.690155	0.594166	1.711642
-86.169990	3.465575	1.716646
-86.144005	-0.430461	1.721651
-86.128139	-6.564946	1.726656
-86.228547	-6.467339	1.731661
-86.337846	-9.189727	1.736666
-87.035838	-7.670427	1.741670
-87.282850	-9.370910	1.746675
-87.548762	-12.779732	1.751680
-87.795234	-3.795707	1.756685
-87.505750	-16.583399	1.761690
-88.463249	-0.712698	1.766694
-89.244157	-6.753901	1.771699
-89.642259	0.068394	1.776704
-89.410481	-6.746340	1.781709
-89.103038	-6.180717	1.786714
-89.111083	-9.626327	1.791718
-89.579295	-0.074355	1.796723
-90.376020	-3.861763	1.801728
-91.046649	6.693036	1.806733
-90.684699	-9.210320	1.811738
-91.026502	3.033851	1.816742
-91.142869	-3.349476	1.821747
-90.680241	-2.497966	1.826752
-91.133262	-6.373278	1.831757
-91.691924	-16.925811	1.836762
-92.558692	-4.970228	1.841766
-92.512273	-4.373216	1.846771
-92.292533	-8.286342	1.851776
-92.632286	-5.213174	1.856781
-92.789570	-1.664657	1.861786
-93.628174	-1.070450	1.866790
-93.512160	-2.108424	1.871795
-93.695358	-10.084406	1.876800
-93.927652	3.942292	1.881805
-94.681125	-5.934874	1.886810
-95.408033	3.993635	1.891814
-94.719848	-3.448433	1.896819
-95.338102	-1.629959	1.901824
-95.659768	-3.275059	1.906829
-95.662374	-13.363997	1.911834
-95.646587	-3.088251	1.916838
-95.700045	-5.443376	1.921843
-95.952620	-6.041030	1.926848
-96.871173	-4.708580	1.931853
-96.879485	-14.457159	1.936858
-97.277194	4.891972	1.941862
-97.157115	-2.628082	1.946867
-97.184057	-6.507656	1.951872
-98.102398	-9.320418	1.956877
-99.052668	-16.768966	1.961882
-98.666537	-2.259013	1.966886
-98.423164	-5.897420	1.971891
-98.593326	-6.465506	1.976896
-99.032268	-6.406748	1.981901
-99.028312	-10.467853	1.986906
-99.776588	-1.354346	1.991910
-100.136447	-0.375300	1.996915
-100.477652	-0.108716	2.006912
-99.502572	-0.857685	2.016909
-99.285829	-4.924583	2.026906
-98.943902	-10.609298	2.036902
-98.466234	-4.480518	2.046899
-97.878156	-1.246871	2.056896
-97.583275	-8.246830	2.066893
-96.316940	-4.104787	2.076890
-96.145479	-7.361196	2.086886
-96.048477	-5.902734	2.096883
-95.741933	-5.942295	2.106880
-95.007441	0.946546	2.116877
-94.235679	-3.213459	2.126874
-93.410550	-8.907664	2.136870
-93.267126	-6.460267	2.146867
-93.191545	-1.329484	2.156864
-92.563906	-3.317269	2.166861
-91.826252	-1.837071	2.176858
-91.836894	3.442945	2.186854
-90.764194	-3.450116	2.196851
-90.447997	-6.905558	2.206848
-89.479879	0.742839	2.216845
-88.874299	3.091962	2.226842
-88.674726	-0.847219	2.236838
-88.756524	-4.178262	2.246835
-87.986270	0.067481	2.256832
-87.575957	-5.248208	2.266829
-86.474762	-0.262782	2.276826
-85.960066	4.511743	2.286822
-85.836766	-5.720757	2.296819
-85.634854	-3.283046	2.306816
-84.984861	0.562942	2.316813
-84.452785	-4.357588	2.326810
-83.772060	-3.889084	2.336806
-82.830244	-4.308499	2.346803
-82.726086	0.391953	2.356800
-82.463001	3.545464	2.366797
-82.159165	-1.308617	2.376794
-81.743287	-3.839466	2.386790
-80.212080	1.543222	2.396787
-80.323133	-3.208360	2.406784
-79.433325	-1.885346	2.416781
-79.732785	-1.369503	2.426778
-79.029598	2.518655	2.436774
-78.200131	1.237800	2.446771
-78.134907	5.759761	2.456768
-76.998732	-2.816967	2.466765
-76.594689	-0.192423	2.476762
-76.424367	-2.652176	2.486758
-75.634090	-2.431013	2.496755
-75.114342	-0.782736	2.506752
-74.682281	-3.498637	2.516749
-74.727138	-1.075973	2.526746
-73.907486	-0.568433	2.536742
-73.223696	8.115582	2.546739
-72.585804	7.659170	2.556736
-71.780409	4.832636	2.566733
-71.652479	1.994807	2.576730
-71.477514	5.942193	2.586726
-71.221133	6.805017	2.596723
-70.282706	2.669773	2.606720
-70.038448	2.390780	2.616717
-69.044949	2.149724	2.626714
-68.995503	3.392002	2.636710
-68.219466	-0.668335	2.646707
-67.323858	5.399340	2.656704
-67.305327	-1.216983	2.666701
-67.245940	2.878567	2.676698
-65.918225	-5.023905	2.686694
-65.646150	0.862904	2.696691
-65.488316	1.665188	2.706688
-64.899427	5.763146	2.716685
-64.020625	-3.945999	2.726682
-63.972949	-6.735760	2.736678
-63.281375	-5.625709	2.746675
-62.721032	0.790311	2.756672
-62.604383	-0.300966	2.766669
-61.515068	-3.618690	2.776666
-60.877646	-1.377581	2.786662
-60.803400	-0.918293	2.796659
-60.465090	-4.206090	2.806656
-59.490317	-4.140155	2.816653
-59.205875	-4.499501	2.826650
-58.903468	-4.566234	2.836646
-58.180620	-6.664228	2.846643
-57.759973	-4.495496	2.856640
-57.593506	0.832249	2.866637
-56.688982	-7.805101	2.876634
-56.282795	-5.475510	2.886630
-55.804590	6.101623	2.896627
-54.931601	3.671715	2.906624
-54.834956	1.548401	2.916621
-54.477883	-4.557310	2.926618
-53.238363	-4.404812	2.936614
-53.283805	0.495676	2.946611
-53.074983	-3.639263	2.956608
-51.879791	-9.248138	2.966605
-51.598433	-2.996147	2.976602
-51.497651	-8.826657	2.986598
-50.744502	-4.639721	2.996595
-49.825950	-4.724320	3.006592
-49.865507	-1.383364	3.016589
-49.495553	3.401306	3.026586
-48.609444	-5.741580	3.036582
-48.412148	-4.880034	3.046579
-47.844287	-4.022952	3.056576
-46.690039	-6.724684	3.066573
-46.940595	-3.931664	3.076570
-46.574881	-3.269514	3.086566
-45.532298	-3.130239	3.096563
-44.844816	-11.382507	3.106560
-44.808659	-8.868737	3.116557
-44.197466	-12.220690	3.126554
-43.620579	-13.181114	3.136550
-43.533152	-10.606878	3.146547
-42.589801	-11.093520	3.156544
-42.082549	-10.195379	3.166541
-42.041068	-15.108358	3.176538
-41.021985	-2.674759	3.186534
-40.661437	-3.763945	3.196531
-40.621604	0.220244	3.206528
-39.356284	-3.052133	3.216525
-38.999854	-8.133649	3.226522
-38.980587	-6.263187	3.236518
-38.004459	-10.622406	3.246515
-37.405939	-4.654903	3.256512
-37.510483	3.083025	3.266509
-36.667022	-8.214188	3.276506
-35.961720	-11.097837	3.286502
-35.784008	-6.138279	3.296499
-35.418289	-2.567665	3.306496
-34.674776	-6.068184	3.316493
-34.317462	-7.676088	3.326490
-33.639598	-3.847352	3.336486
-32.872873	-6.992305	3.346483
-32.706700	-2.461177	3.356480
-32.344222	-1.647732	3.366477
-31.333350	-6.120191	3.376474
-31.052140	-2.471761	3.386470
-31.118785	-8.967479	3.396467
-30.351061	1.747855	3.406464
-29.563145	1.712952	3.416461
-29.256071	2.654124	3.426458
-28.224270	-1.506059	3.436454
-27.941293	4.912828	3.446451
-27.969302	-0.292930	3.456448
-27.321357	0.592979	3.466445
-26.347551	-2.707585	3.476442
-26.048930	-0.148562	3.486438
-25.888008	0.829261	3.496435
-25.053449	-0.093611	3.506432
-24.831331	-0.964657	3.516429
-24.310804	-5.701096	3.526426
-23.289534	-8.257901	3.536422
-22.978446	-6.022218	3.546419
-22.744843	-6.373143	3.556416
-22.290499	-4.252270	3.566413
-21.303700	-5.117959	3.576410
-21.176182	-10.475135	3.586406
-20.963636	-14.753147	3.596403
-19.962327	-4.313993	3.606400
-19.683210	-9.943849	3.616397
-19.455058	-13.868001	3.626394
-18.689225	-6.605760	3.636390
-18.288227	-9.715635	3.646387
-17.335917	-2.765436	3.656384
-16.972242	-6.915744	3.666381
-16.989765	-8.494571	3.676378
-15.916649	-8.903706	3.686374
-15.248236	-10.802404	3.696371
-15.285122	-9.921637	3.706368
-15.103980	-5.324820	3.716365
-14.042294	-11.437354	3.726362
-13.632874	-9.052772	3.736358
-13.111556	-10.455671	3.746355
-12.287736	-12.291387	3.756352
-12.008006	-8.912811	3.766349
-12.071116	-7.018038	3.776346
-11.232307	-6.277543	3.786342
-10.406205	-8.997043	3.796339
-10.427108	-5.135969	3.806336
-9.290109	-10.116952	3.816333
-9.267102	-14.547134	3.826330
-8.896184	-10.765962	3.836326
-7.685587	-4.046042	3.846323
-7.343124	-6.106724	3.856320
-7.405437	-10.542340	3.866317
-6.804802	-9.855071	3.876314
-5.981766	-13.336349	3.886310
-5.781232	-13.146536	3.896307
-5.166489	-10.787064	3.906304
-4.480014	-11.186703	3.916301
-4.279642	-11.710346	3.926298
-3.157395	-5.156981	3.936294
-2.965451	-2.188083	3.946291
-3.201617	4.623232	3.956288
-2.330365	11.314985	3.966285
-2.042116	22.291916	3.976282
-1.469474	37.742539	3.986278
-1.226653	56.429731	3.996275
-0.849339	78.067962	4.006272
-0.434369	100.253233	4.016269
0.000000	114.980218	4.021274
-0.047948	126.282100	4.026278
0.466230	137.934908	4.031283
0.197014	153.063468	4.036288
0.137518	156.612995	4.041293
0.998598	178.952315	4.046298
1.013219	182.063922	4.051302
1.144018	188.445483	4.056307
1.354694	185.983635	4.061312
1.338191	191.828959	4.066317
1.553935	195.430204	4.071322
1.308584	194.852454	4.076326
1.342052	189.543979	4.081331
1.222404	178.443998	4.086336
1.124622	189.824626	4.091341
1.228030	184.014587	4.096346
1.041869	189.316520	4.101350
1.071258	195.301853	4.106355
1.670011	189.399128	4.111360
1.114740	194.971955	4.116365
1.457385	188.473259	4.121370
1.303483	200.189187	4.126374
1.450602	190.793616	4.131379
1.346635	193.647211	4.136384
1.201040	199.169564	4.141389
1.368730	193.442216	4.146394
1.076720	199.639036	4.151398
1.241042	197.416732	4.156403
1.422800	190.189869	4.161408
1.098535	198.275599	4.166413
1.354182	193.514643	4.171418
1.384186	198.566674	4.176422
1.642537	197.059534	4.181427
1.387819	190.858870	4.186432
1.174741	198.272021	4.191437
1.237053	192.086347	4.196442
1.290438	196.869681	4.201446
1.405636	202.601044	4.206451
1.653028	200.758472	4.211456
1.434496	199.495669	4.216461
1.737120	200.582085	4.221466
1.336593	201.808028	4.226470
1.550622	213.442516	4.231475
1.422334	225.659205	4.236480
1.263675	223.490184	4.241485
1.660125	225.277001	4.246490
1.452086	222.818575	4.251494
1.842661	227.436560	4.256499
1.820621	222.813536	4.261504
1.713303	231.064642	4.266509
1.525215	229.696153	4.271514
1.875343	227.202130	4.276518
1.922748	230.181036	4.281523
2.123430	224.963852	4.286528
1.646581	232.203628	4.291533
1.924380	221.364985	4.296538
1.772607	227.618120	4.301542
1.816028	220.012966	4.306547
1.799762	217.827865	4.311552
1.540305	217.848405	4.316557
2.066850	213.327734	4.321562
2.039207	225.184786	4.326566
1.457612	214.708686	4.331571
1.879597	216.800498	4.336576
2.116753	228.551346	4.341581
2.005764	216.155575	4.346586
1.803636	212.089856	4.351590
1.643885	212.852050	4.356595
1.848976	224.605836	4.361600
2.001665	224.669227	4.366605
2.060250	228.606519	4.371610
2.159638	233.681804	4.376614
1.862738	227.151060	4.381619
2.121438	223.199062	4.386624
1.951218	232.470748	4.391629
2.144913	227.933755	4.396634
1.801682	212.658632	4.401638
2.035611	218.752185	4.406643
1.809104	222.859231	4.411648
1.475039	221.184379	4.416653
1.568435	225.431249	4.421658
1.510069	230.463982	4.426662
1.714759	227.803021	4.431667
1.837799	223.569984	4.436672
2.146683	245.534536	4.441677
2.037172	249.118218	4.446682
2.230653	262.162957	4.451686
2.363919	263.530211	4.456691
2.131909	251.365603	4.461696
2.007863	267.382917	4.466701
2.408132	262.748953	4.471706
2.357757	269.417086	4.476710
1.984697	262.262331	4.481715
2.298836	251.656623	4.486720
2.165184	260.175352	4.491725
2.347455	266.555525	4.496730
2.604314	262.516599	4.501734
2.180284	254.604029	4.506739
2.276614	237.147749	4.511744
2.264413	247.660374	4.516749
2.355955	254.397354	4.521754
1.991502	252.419290	4.526758
2.301291	256.074635	4.531763
2.564624	265.558120	4.536768
2.436857	270.593874	4.541773
2.711016	258.240261	4.546778
2.309687	245.017358	4.551782
2.143310	243.993572	4.556787
2.373543	249.613550	4.561792
2.101843	267.224140	4.566797
2.287117	268.733349	4.571802
2.431995	265.291163	4.576806
2.701559	272.046032	4.581811
2.709070	267.393237	4.586816
2.357763	283.849781	4.591821
2.683500	268.454945	4.596826
2.258572	269.574425	4.601830
2.391120	275.225981	4.606835
2.458959	271.853383	4.611840
2.477198	268.206019	4.616845
2.711432	266.487375	4.621850
2.343356	268.399614	4.626854
2.185804	280.211915	4.631859
2.406799	263.393869	4.636864
2.367488	266.721628	4.641869
2.790274	273.676088	4.646874
2.462663	273.724885	4.651878
2.210199	266.663034	4.656883
2.283175	268.290298	4.661888
2.312423	292.707745	4.666893
3.017977	286.713100	4.671898
2.758570	297.839762	4.676902
2.159329	294.282013	4.681907
2.748991	291.932824	4.686912
2.876278	305.875394	4.691917
2.934533	294.331659	4.696922
2.901181	300.455691	4.701926
2.864600	300.606074	4.706931
2.891768	295.893972	4.711936
2.991962	299.111610	4.716941
2.851420	296.016634	4.721946
2.863937	309.347128	4.726950
2.920503	303.879879	4.731955
2.931182	288.354461	4.736960
3.020865	291.196530	4.741965
2.772004	284.428698	4.746970
3.027419	285.134579	4.751974
2.730720	291.081199	4.756979
3.014667	288.189045	4.761984
2.581081	301.467110	4.766989
3.151986	287.587463	4.771994
3.060702	298.390674	4.776998
2.861813	295.169196	4.782003
2.920195	297.175596	4.787008
2.733913	298.503612	4.792013
2.889511	284.572957	4.797018
2.954714	297.978783	4.802022
2.835377	296.314146	4.807027
3.052579	285.883521	4.812032
2.817950	294.945485	4.817037
3.003992	289.219602	4.822042
3.036896	295.312532	4.827046
2.762102	296.514898	4.832051
3.196335	293.157203	4.837056
2.683693	291.981774	4.842061
3.074936	287.601297	4.847066
3.068949	288.060182	4.852070
2.844724	292.863468	4.857075
3.092034	304.891529	4.862080
2.783178	327.979516	4.867085
2.835437	323.283576	4.872090
3.177598	322.956241	4.877094
3.169790	330.328951	4.882099
3.271672	325.236236	4.887104
2.972463	325.716050	4.892109
3.124327	326.391917	4.897114
3.195222	324.142836	4.902118
2.883773	330.702871	4.907123
2.841872	320.057604	4.912128
2.929492	328.582945	4.917133
3.402973	337.030778	4.922138
3.344385	357.421201	4.927142
3.174108	370.614676	4.932147
3.330489	356.775983	4.937152
3.314053	357.724617	4.942157
3.281986	365.736591	4.947162
3.254635	364.687407	4.952166
3.342077	361.017116	4.957171
3.319099	354.300058	4.962176
3.288104	362.605689	4.967181
3.196403	356.141553	4.972186
3.375735	358.346583	4.977190
3.570653	360.268812	4.982195
3.522672	358.514996	4.987200
3.324279	370.520810	4.992205
3.423328	360.131803	4.997210
3.399413	361.225930	5.002214
3.548471	367.752347	5.007219
3.854500	356.972083	5.012224
3.691450	365.606246	5.017229
3.592244	365.719836	5.022234
3.985972	367.166318	5.027238
3.658325	369.502663	5.032243
3.844438	364.949323	5.037248
3.616464	369.358972	5.042253
3.990700	354.314386	5.047258
3.461573	366.607429	5.052262
3.559900	367.219740	5.057267
3.870471	363.620837	5.062272
3.477289	366.175634	5.067277
3.875590	354.619945	5.072282
3.868104	362.143975	5.077286
3.338440	361.505750	5.082291
3.908028	360.493880	5.087296
3.581576	367.731902	5.092301
3.323878	358.049832	5.097306
3.530233	360.860950	5.102310
3.547473	358.726523	5.107315
3.920768	363.325112	5.112320
3.436365	366.981952	5.117325
3.755247	362.296906	5.122330
3.740740	366.715015	5.127334
3.346160	372.026067	5.132339
3.814384	378.215273	5.137344
3.809450	388.903802	5.142349
3.944962	393.262542	5.147354
3.962412	398.799407	5.152358
4.080466	403.082500	5.157363
4.064681	387.703843	5.162368
3.796852	388.257596	5.167373
4.016706	398.421285	5.172378
4.200133	390.268930	5.177382
3.734621	378.084477	5.182387
4.133630	370.890030	5.187392
3.928706	379.687033	5.192397
4.092364	374.959014	5.197402
4.199667	371.880011	5.202406
3.710516	368.666525	5.207411
4.148146	377.743511	5.212416
3.818278	392.394922	5.217421
3.947797	395.605949	5.222426
4.288175	395.746599	5.227430
4.306077	401.239187	5.232435
4.174226	393.283490	5.237440
3.904906	392.261940	5.242445
4.374433	389.446586	5.247450
4.444318	391.924311	5.252454
3.944630	383.260306	5.257459
4.249335	372.571026	5.262464
4.100432	377.987427	5.267469
4.383014	369.815901	5.272474
4.135117	371.170505	5.277478
3.995854	370.610701	5.282483
4.372295	386.106577	5.287488
4.323419	393.698848	5.292493
4.276805	386.037480	5.297498
4.138137	387.132061	5.302502
4.198781	393.065328	5.307507
4.442300	386.868908	5.312512
3.965997	391.673316	5.317517
4.242225	391.851625	5.322522
4.137926	403.515881	5.327526
4.121599	395.989208	5.332531
4.357321	398.092157	5.337536
4.523249	397.276187	5.342541
4.388917	395.317029	5.347546
4.648028	401.933773	5.352550
4.246811	399.400547	5.357555
4.684576	389.098106	5.362560
4.435787	399.796043	5.367565
4.325965	390.743247	5.372570
4.138538	391.885962	5.377574
3.901602	395.810862	5.382579
4.431450	396.844075	5.387584
4.016724	399.758049	5.392589
4.197936	398.157299	5.397594
4.391159	403.926335	5.402598
4.437086	418.094421	5.407603
4.822837	424.598836	5.412608
4.503391	429.208753	5.417613
4.520748	426.577398	5.422618
4.601665	423.846715	5.427622
4.719040	427.240324	5.432627
4.417567	419.322767	5.437632
4.613066	430.272958	5.442637
4.835348	423.975056	5.447642
4.828540	433.667564	5.452646
4.269797	425.307547	5.457651
4.743446	428.713793	5.462656
4.513430	437.494460	5.467661
4.738282	433.375146	5.472666
4.710982	432.247013	5.477670
4.753988	425.272719	5.482675
4.947518	424.505262	5.487680
4.697967	437.633183	5.492685
4.755566	436.034743	5.497690
4.751451	431.739232	5.502694
4.650254	439.342360	5.507699
4.826821	428.798584	5.512704
4.641604	432.985282	5.517709
4.447505	433.369153	5.522714
4.406912	427.132541	5.527718
4.450970	442.534326	5.532723
4.828249	427.356553	5.537728
4.532702	437.305661	5.542733
4.666543	434.927935	5.547738
4.968445	443.509619	5.552742
4.901005	436.401066	5.557747
5.075089	444.003803	5.562752
4.870439	428.412469	5.567757
4.584309	439.754218	5.572762
4.765817	454.005461	5.577766
4.721815	462.522479	5.582771
4.963347	465.732338	5.587776
4.869015	483.069100	5.592781
4.912529	468.932070	5.597786
4.951938	470.282915	5.602790
4.786328	460.421148	5.607795
5.079676	461.827428	5.612800
4.736520	468.483349	5.617805
4.897803	467.674460	5.622810
4.892196	464.681034	5.627814
4.717321	474.291086	5.632819
4.808259	466.603545	5.637824
5.161122	482.667615	5.642829
5.106801	491.478223	5.647834
5.138888	493.697196	5.652838
5.313460	502.158702	5.657843
5.447603	499.004779	5.662848
5.454555	495.839161	5.667853
5.011198	472.772619	5.672858
5.120361	474.867921	5.677862
4.982758	482.017693	5.682867
5.303024	486.108465	5.687872
4.834966	492.798696	5.692877
4.923986	500.162359	5.697882
5.578338	490.582363	5.702886
5.111845	497.137949	5.707891
5.283617	497.695872	5.712896
5.180383	501.992942	5.717901
5.132870	495.375004	5.722906
5.535329	497.979818	5.727910
5.156167	496.545066	5.732915
5.356423	501.567820	5.737920
5.199385	499.492820	5.742925
5.485176	503.720931	5.747930
5.240282	501.162789	5.752934
5.204823	505.365557	5.757939
5.308882	495.697301	5.762944
5.405462	497.998542	5.767949
5.215922	505.537001	5.772954
5.435863	502.787822	5.777958
5.265446	495.415086	5.782963
5.405216	498.438147	5.787968
5.344471	517.301729	5.792973
5.744816	528.544074	5.797978
5.844543	517.768852	5.802982
5.356037	512.930331	5.807987
5.534886	504.044965	5.812992
5.723479	511.398459	5.817997
5.438389	504.861892	5.823002
5.359872	513.577455	5.828006
5.700210	518.898287	5.833011
5.815113	526.996714	5.838016
5.518857	519.481013	5.843021
5.632794	522.971119	5.848026
5.644471	535.019040	5.853030
5.563506	532.102610	5.858035
5.752388	532.945620	5.863040
5.385534	538.429546	5.868045
5.153924	535.561545	5.873050
5.566321	535.574630	5.878054
5.417990	542.678252	5.883059
5.856055	540.237700	5.888064
5.566566	537.808892	5.893069
5.653044	535.601208	5.898074
5.826782	540.852938	5.903078
5.418011	537.934745	5.908083
5.694284	536.449669	5.913088
5.560676	543.299244	5.918093
5.639849	544.489981	5.923098
5.732308	550.480597	5.928102
5.882756	568.645613	5.933107
5.908881	565.515287	5.938112
5.684706	573.433080	5.943117
5.967759	563.274351	5.948122
5.945219	567.079131	5.953126
5.978786	571.849089	5.958131
6.061160	570.746397	5.963136
5.959673	575.909918	5.968141
5.859316	559.866638	5.973146
5.919941	556.879790	5.978150
5.896130	562.929725	5.983155
6.296446	559.516612	5.988160
6.170137	557.224375	5.993165
6.035041	547.790661	5.998170
6.050556	535.486763	6.003174
5.661711	542.647776	6.008179
6.042704	553.489586	6.013184
5.987065	558.223003	6.018189
6.064575	559.377509	6.023194
6.152680	570.366107	6.028198
6.051399	573.301223	6.033203
6.182451	566.521073	6.038208
6.368583	572.171166	6.043213
5.561645	568.147684	6.048218
6.155780	560.637260	6.053222
5.716164	567.058969	6.058227
6.037057	562.848727	6.063232
6.134409	574.849141	6.068237
5.886916	567.279163	6.073242
5.916450	569.529552	6.078246
6.278879	571.423280	6.083251
6.534072	553.298783	6.088256
6.494115	575.501347	6.093261
6.270607	563.871062	6.098266
6.265107	546.970825	6.103270
5.898771	544.956329	6.108275
6.179882	541.256490	6.113280
6.005321	544.315825	6.118285
6.076509	539.706870	6.123290
6.390876	539.952474	6.128294
5.923203	537.106197	6.133299
6.171655	536.863642	6.138304
6.077422	540.626216	6.143309
5.978628	535.957989	6.148314
5.824406	536.326378	6.153318
5.946273	543.463602	6.158323
5.828743	541.294633	6.163328
6.003286	558.110180	6.168333
6.055036	571.127342	6.173338
6.490548	567.123481	6.178342
6.166625	556.138952	6.183347
6.060881	542.185628	6.188352
5.643190	543.193220	6.193357
5.617462	562.375879	6.198362
6.236629	565.199191	6.203366
5.779649	566.288280	6.208371
6.361468	562.096400	6.213376
6.066204	576.726862	6.218381
5.965293	572.389520	6.223386
6.150121	574.900535	6.228390
6.139976	571.111768	6.233395
6.289436	568.722555	6.238400
6.167418	575.909454	6.243405
5.910922	568.557252	6.248410
6.300462	567.087753	6.253414
5.952677	578.196492	6.258419
6.260422	567.381066	6.263424
6.032711	584.810084	6.268429
5.755179	567.781211	6.273434
5.862593	573.804486	6.278438
5.802821	567.861282	6.283443
6.044692	567.363076	6.288448
6.223249	573.622430	6.293453
6.071145	575.576892	6.298458
6.139048	575.945008	6.303462
6.057129	586.298313	6.308467
6.370527	573.629903	6.313472
6.143872	580.191196	6.318477
5.970078	578.253547	6.323482
6.563730	576.589809	6.328486
6.079384	574.714834	6.333491
6.116857	555.987004	6.338496
6.265446	553.959860	6.343501
6.078530	549.849104	6.348506
6.273516	546.877897	6.353510
6.081744	551.724632	6.358515
6.152817	545.691884	6.363520
6.199172	547.067043	6.368525
5.923834	547.487063	6.373530
6.316336	540.252373	6.378534
6.066615	549.480381	6.383539
6.000012	539.823979	6.388544
5.831130	547.064803	6.393549
5.639517	548.153954	6.398554
6.053080	554.393330	6.403558
6.183108	568.661492	6.408563
6.153088	559.508553	6.413568
5.976072	554.461947	6.418573
5.954383	559.214607	6.423578
6.180487	552.562979	6.428582
6.025253	565.971202	6.433587
6.129010	557.080085	6.438592
6.012495	553.373269	6.443597
5.946127	553.269084	6.448602
6.097933	566.182251	6.453606
6.153408	575.152726	6.458611
6.338931	561.269952	6.463616
6.119457	554.073445	6.468621
5.834022	547.100992	6.473626
6.165133	550.421543	6.478630
5.735660	561.290411	6.483635
6.188528	562.948929	6.488640
6.347118	571.337341	6.493645
5.994217	560.792941	6.498650
5.951381	549.005070	6.503654
5.750276	557.445341	6.508659
6.210511	569.037155	6.513664
6.110564	569.310715	6.518669
6.166051	575.707078	6.523674
6.197726	568.960551	6.528678
5.966961	578.872578	6.533683
6.131158	566.619616	6.538688
6.121545	575.127646	6.543693
5.898756	575.512324	6.548698
6.438680	562.247346	6.553702
6.172501	556.460874	6.558707
5.885474	550.940122	6.563712
5.529987	552.306638	6.568717
5.790509	564.777124	6.573722
5.916851	570.886856	6.578726
6.100197	568.293705	6.583731
6.158015	570.198406	6.588736
6.058461	575.629595	6.593741
6.321235	581.494139	6.598746
5.898542	574.419486	6.603750
6.024095	578.529502	6.608755
6.404063	575.581927	6.613760
6.214912	576.137063	6.618765
6.223443	590.715456	6.623770
6.126322	579.356295	6.628774
5.958765	578.516801	6.633779
6.034853	574.473194	6.638784
6.156473	580.386372	6.643789
5.978204	577.238778	6.648794
6.089035	578.723444	6.653798
5.909883	581.707373	6.658803
6.338056	569.006936	6.663808
6.221677	575.001556	6.668813
6.087128	583.595994	6.673818
5.854507	566.596589	6.678822
5.832856	575.447222	6.683827
6.034353	579.549399	6.688832
6.401415	572.186885	6.693837
6.085827	580.216516	6.698842
6.202994	572.741457	6.703846
6.147882	578.274812	6.708851
5.956756	577.349036	6.713856
6.055535	579.515339	6.718861
6.156413	576.904859	6.723866
6.406910	566.534248	6.728870
5.920437	560.530473	6.733875
5.943105	552.729279	6.738880
6.113791	555.254868	6.743885
5.979148	563.671507	6.748890
6.258501	564.232536	6.753894
5.945798	566.293317	6.758899
5.955735	561.801457	6.763904
6.370900	563.375442	6.768909
6.317134	557.601157	6.773914
6.258710	553.450967	6.778918
6.080119	554.306679	6.783923
6.310828	546.431175	6.788928
6.234914	553.759421	6.793933
5.749013	552.643283	6.798938
5.903845	541.793994	6.803942
5.628871	552.529919	6.808947
6.010241	547.458735	6.813952
6.227625	560.090484	6.818957
5.903542	556.062432	6.823962
6.033218	565.430687	6.828966
6.043246	571.986529	6.833971
6.034736	575.627366	6.838976
6.069276	576.046789	6.843981
5.879243	585.290195	6.848986
6.057400	576.814187	6.853990
5.668341	580.785438	6.858995
6.170037	578.456694	6.864000
6.338026	578.356919	6.869005
6.152934	576.277279	6.874010
6.100012	582.328490	6.879014
5.980715	570.371513	6.884019
6.185768	575.160240	6.889024
5.935356	572.011569	6.894029
5.941790	576.023103	6.899034
6.247874	565.806487	6.904038
6.279638	581.937844	6.909043
6.238014	570.870444	6.914048
6.277619	570.647475	6.919053
5.962804	559.607364	6.924058
6.012755	549.460998	6.929062
6.036875	558.317659	6.934067
6.052535	567.525808	6.939072
5.999233	568.080945	6.944077
5.850722	573.221073	6.949082
6.109450	573.389850	6.954086
6.323951	577.285230	6.959091
6.180010	574.542224	6.964096
6.224211	578.222089	6.969101
5.862120	565.301647	6.974106
6.131769	555.316435	6.979110
5.868386	574.378618	6.984115
6.112288	563.451810	6.989120
6.244556	578.161455	6.994125
6.011523	574.569639	6.999130
6.441562	555.206291	7.004134
5.864369	561.050864	7.009139
5.730418	552.440263	7.014144
5.965974	566.942952	7.019149
6.066992	571.790150	7.024154
5.962802	567.946111	7.029158
5.770858	577.848551	7.034163
6.165335	580.084095	7.039168
6.193109	572.218305	7.044173
6.047577	579.554737	7.049178
6.071967	575.537057	7.054182
5.881582	580.520328	7.059187
6.115504	572.569092	7.064192
5.901761	580.021410	7.069197
6.184473	570.699655	7.074202
6.040281	566.737324	7.079206
6.061410	574.052471	7.084211
6.015657	567.962886	7.089216
6.226267	571.363190	7.094221
6.082741	580.135535	7.099226
5.929446	570.151478	7.104230
6.002125	573.830574	7.109235
6.088240	568.977593	7.114240
6.252891	577.129972	7.119245
6.053319	579.412184	7.124250
6.148734	574.850120	7.129254
6.113652	580.719783	7.134259
5.967549	585.087321	7.139264
6.072630	580.262179	7.144269
6.129256	576.302113	7.149274
5.944110	574.625057	7.154278
5.839793	576.088318	7.159283
6.122710	580.836723	7.164288
6.056519	579.505443	7.169293
5.912000	578.277517	7.174298
6.205532	569.500605	7.179302
5.769114	585.458081	7.184307
5.993351	568.850323	7.189312
6.116351	580.662178	7.194317
6.134300	585.444396	7.199322
6.248867	574.238645	7.204326
5.847889	579.646537	7.209331
5.813798	577.301728	7.214336
5.856218	582.722040	7.219341
5.790384	581.168891	7.224346
6.256563	582.794817	7.229350
5.585395	581.128779	7.234355
6.222018	578.278223	7.239360
6.122892	581.784088	7.244365
5.877535	585.359360	7.249370
6.281127	580.817502	7.254374
5.882849	584.052227	7.259379
6.117411	581.843300	7.264384
6.032767	575.232069	7.269389
5.964828	584.540112	7.274394
6.607212	589.902913	7.279398
6.293621	587.873756	7.284403
6.253741	584.711533	7.289408
5.953568	581.850930	7.294413
6.018936	582.544289	7.299418
6.167925	578.949795	7.304422
6.064550	581.861974	7.309427
6.010995	577.684922	7.314432
6.364069	581.927371	7.319437
6.077869	578.669378	7.324442
6.245121	580.006168	7.329446
6.031510	578.628652	7.334451
6.088843	583.825079	7.339456
6.110966	582.602710	7.344461
5.877707	589.902563	7.349466
6.218250	581.488663	7.354470
5.896608	585.588272	7.359475
6.154903	576.184911	7.364480
6.090333	579.109608	7.369485
5.909209	584.443008	7.374490
6.531881	579.719827	7.379494
6.117094	586.873908	7.384499
6.015939	581.948133	7.389504
6.289380	582.836938	7.394509
5.821750	589.834202	7.399514
5.926858	587.205654	7.404518
5.811020	587.906326	7.409523
5.514557	577.187592	7.414528
5.764622	582.491425	7.419533
5.349572	580.457364	7.424538
6.136650	593.826987	7.429542
6.274641	614.248345	7.434547
6.324112	616.656075	7.439552
5.902918	612.743549	7.444557
6.165383	611.085513	7.449562
6.260753	615.541543	7.454566
6.182015	607.971623	7.459571
6.174488	600.854257	7.464576
6.225982	588.370304	7.469581
5.900541	585.760166	7.474586
5.988636	579.825032	7.479590
5.751645	591.820438	7.484595
5.986880	602.015262	7.489600
5.783447	611.745769	7.494605
6.051026	607.452383	7.499610
6.235158	602.388780	7.504614
5.741491	609.844249	7.509619
6.006244	612.070296	7.514624
6.265466	607.975240	7.519629
6.277510	620.744843	7.524634
6.561077	606.292645	7.529638
6.491583	622.110265	7.534643
6.249974	598.912245	7.539648
6.248322	591.204652	7.544653
5.736123	582.951102	7.549658
6.093042	581.367612	7.554662
6.103113	584.662199	7.559667
5.968007	576.842718	7.564672
6.196839	587.150682	7.569677
5.896119	581.283683	7.574682
6.120431	575.748500	7.579686
6.215357	582.473814	7.584691
6.372478	583.498707	7.589696
6.043413	581.584993	7.594701
5.850525	586.844563	7.599706
6.105926	576.393802	7.604710
6.120040	582.192564	7.609715
6.063316	583.456129	7.614720
6.224471	576.451744	7.619725
6.021800	591.419732	7.624730
6.011212	582.548127	7.629734
6.130371	589.953217	7.634739
6.346506	587.857654	7.639744
6.295318	589.684304	7.644749
6.047936	585.780892	7.649754
6.174784	585.690297	7.654758
6.266727	588.306486	7.659763
6.416896	589.318322	7.664768
6.444927	582.021220	7.669773
5.933045	586.390325	7.674778
6.021224	574.255521	7.679782
5.921306	584.073657	7.684787
6.022567	581.841219	7.689792
6.265359	575.473553	7.694797
5.656817	584.710877	7.699802
6.121815	579.815281	7.704806
6.078259	588.615478	7.709811
6.187131	586.036432	7.714816
6.348111	580.575674	7.719821
6.196740	587.171667	7.724826
6.061265	584.066124	7.729830
6.187234	584.349043	7.734835
6.293823	582.672815	7.739840
6.175247	585.285186	7.744845
6.134829	587.731477	7.749850
6.422011	578.348196	7.754854
6.127678	568.236136	7.759859
5.920439	564.876662	7.764864
6.078189	555.997720	7.769869
5.515561	566.943108	7.774874
6.253428	572.415796	7.779878
5.978882	579.626968	7.784883
6.158625	584.089935	7.789888
6.275005	587.714830	7.794893
5.977833	591.172977	7.799898
6.294407	581.682210	7.804902
6.306658	580.715849	7.809907
6.108948	565.474298	7.814912
5.823100	551.136374	7.819917
6.138440	556.619428	7.824922
5.767920	560.945778	7.829926
6.069049	579.648670	7.834931
6.328941	579.652672	7.839936
6.073597	568.955354	7.844941
5.956571	582.962706	7.849946
6.202083	576.627940	7.854950
6.052954	584.302226	7.859955
6.049891	577.133021	7.864960
6.221766	582.971176	7.869965
5.793778	572.413745	7.874970
6.025374	575.337549	7.879974
6.099313	584.458108	7.884979
6.301402	582.550569	7.889984
5.974181	577.203217	7.894989
5.756392	582.477960	7.899994
6.161990	589.277932	7.904998
6.167957	589.841410	7.910003
6.098649	582.366244	7.915008
6.078838	590.026419	7.920013
5.888848	592.174235	7.925018
6.042309	586.278991	7.930022
6.067111	582.914440	7.935027
6.047589	580.229569	7.940032
6.015331	583.736202	7.945037
5.975240	594.317816	7.950042
6.010491	585.669902	7.955046
5.990151	585.181569	7.960051
6.095548	583.074743	7.965056
6.484160	583.332128	7.970061
5.796319	585.832347	7.975066
5.830803	581.541256	7.980070
6.079045	583.534804	7.985075
5.838222	583.757886	7.990080
5.885731	585.300400	7.995085
5.847039	586.092295	8.000090
6.246811	586.698705	8.005094
5.883331	583.872462	8.010099
6.185231	577.757274	8.015104
6.121224	583.665078	8.020109
5.915629	585.763973	8.025126
6.151090	582.570539	8.030144
6.094124	581.233283	8.035162
6.003676	574.518072	8.040179
6.133772	578.264459	8.045197
5.936557	577.744273	8.050214
6.057531	576.821616	8.055232
5.805983	581.476028	8.060250
5.736649	581.025211	8.065267
5.778469	575.065408	8.070285
6.045537	602.087580	8.075302
6.283959	604.609815	8.080320
6.122935	614.289471	8.085338
6.095652	617.391500	8.090355
6.483711	607.422044	8.095373
5.924788	597.049406	8.100390
6.236735	589.866006	8.105408
5.894809	588.953471	8.110426
6.269356	600.094920	8.115443
6.503518	609.070985	8.120461
6.349186	599.366536	8.125478
6.641609	590.205199	8.130496
6.035054	589.197912	8.135514
6.199389	588.886538	8.140531
6.425304	581.666604	8.145549
6.324309	584.874527	8.150566
6.371585	583.718421	8.155584
6.796116	580.655084	8.160602
6.617300	589.875104	8.165619
6.777422	587.022469	8.170637
6.418732	581.541360	8.175654
6.083665	560.991999	8.180672
6.284177	569.945466	8.185690
6.108809	566.289983	8.190707
6.453424	568.906628	8.195725
6.271247	565.047759	8.200742
6.289520	561.291121	8.205760
6.431416	555.767479	8.210778
5.964935	552.933578	8.215795
6.227129	553.547668	8.220813
6.213897	570.428316	8.225830
6.401597	566.915651	8.230848
6.580253	574.553931	8.235866
6.222783	562.125258	8.240883
6.204589	550.499606	8.245901
5.979572	563.093172	8.250918
5.988752	572.794221	8.255936
6.376805	573.036706	8.260954
6.310318	586.762623	8.265971
6.577294	580.770454	8.270989
6.232270	585.507271	8.276006
6.256867	578.862962	8.281024
6.435882	582.133171	8.286042
6.195450	586.521588	8.291059
6.325564	584.821288	8.296077
6.529817	580.774417	8.301094
6.330448	580.330369	8.306112
6.383811	584.934291	8.311130
6.296015	582.171133	8.316147
6.374951	584.690249	8.321165
6.065370	588.646445	8.326182
6.298518	575.568027	8.331200
6.394950	578.995798	8.336218
6.412179	585.427236	8.341235
6.367182	579.981971	8.346253
6.685336	587.624715	8.351270
6.559225	591.586158	8.356288
6.601876	581.497746	8.361306
6.468459	581.547862	8.366323
6.692601	583.071147	8.371341
6.726114	581.728553	8.376358
6.342599	580.387108	8.381376
6.373427	566.853650	8.386394
6.310302	574.846907	8.391411
6.326113	574.183184	8.396429
6.540442	585.474176	8.401446
6.550102	587.435905	8.406464
6.444709	575.947697	8.411482
6.447743	582.528128	8.416499
6.836719	575.315050	8.421517
6.614929	582.700179	8.426534
6.807550	563.123403	8.431552
6.675545	563.583690	8.436570
6.308476	553.582237	8.441587
6.535119	546.855078	8.446605
6.300457	543.138558	8.451622
6.296323	553.246890	8.456640
6.736389	557.569066	8.461658
6.352966	564.696916	8.466675
6.573812	559.739096	8.471693
6.460603	571.568536	8.476710
6.972082	571.300851	8.481728
6.576842	565.089038	8.486746
6.314006	557.516811	8.491763
6.326691	558.718638	8.496781
6.695894	574.133104	8.501798
6.824165	573.631456	8.506816
6.673965	560.535236	8.511834
6.331460	556.036034	8.516851
6.635519	559.848879	8.521869
6.396927	560.810445	8.526886
6.717560	582.549663	8.531904
6.767472	578.355921	8.536922
6.542015	581.412811	8.541939
6.791375	581.072201	8.546957
6.720570	570.416796	8.551974
6.526920	565.769329	8.556992
6.413030	561.098223	8.562010
6.312161	572.403805	8.567027
6.566365	580.342745	8.572045
6.749423	584.501793	8.577063
6.753390	585.205492	8.582080
6.423405	577.675868	8.587098
6.178625	585.145509	8.592115
6.524903	583.011211	8.597133
6.475708	589.026513	8.602151
6.475684	590.676283	8.607168
6.704584	587.542394	8.612186
6.506544	583.807990	8.617203
6.727577	581.117896	8.622221
6.747179	581.722949	8.627239
6.680084	586.486769	8.632256
6.854824	586.032934	8.637274
6.378032	590.531747	8.642291
6.706049	577.491353	8.647309
6.458503	585.644871	8.652327
6.503372	598.017801	8.657344
7.082164	607.340117	8.662362
7.091682	606.965802	8.667379
6.806378	588.801513	8.672397
6.712496	592.389140	8.677415
6.498867	582.307539	8.682432
6.693220	585.610836	8.687450
6.585856	603.568259	8.692467
7.163740	601.832979	8.697485
6.830647	600.606403	8.702503
6.624401	597.508549	8.707520
6.424203	596.407004	8.712538
7.109507	605.659322	8.717555
7.005509	607.039519	8.722573
6.352590	601.681137	8.727591
6.562174	609.959743	8.732608
7.117836	616.071732	8.737626
6.440010	618.482326	8.742643
6.997025	613.618025	8.747661
6.835553	616.323009	8.752679
6.587100	614.692284	8.757696
6.942442	611.896288	8.762714
7.039905	615.355194	8.767731
6.888791	619.901259	8.772749
6.790129	618.937023	8.777767
6.710081	613.997518	8.782784
7.074812	611.640097	8.787802
7.008415	616.941375	8.792819
6.681609	621.172068	8.797837
6.511970	620.950247	8.802855
6.702246	616.084868	8.807872
6.854082	612.715523	8.812890
7.065406	614.852115	8.817907
7.095805	612.170160	8.822925
6.900361	608.965403	8.827943
6.507736	623.338628	8.832960
7.098844	610.812479	8.837978
6.728027	618.923439	8.842995
6.828880	615.333024	8.848013
7.343048	621.512512	8.853031
6.494249	610.718015	8.858048
6.658979	619.372928	8.863066
6.940669	642.095780	8.868083
7.045035	643.385181	8.873101
7.077635	645.656484	8.878119
7.116410	653.553975	8.883136
6.927926	644.266546	8.888154
6.983431	646.583266	8.893171
7.131590	651.017188	8.898189
7.126791	650.656266	8.903207
6.944394	645.536074	8.908224
7.333544	637.106087	8.913242
6.987000	629.479383	8.918259
6.965559	621.497293	8.923277
7.043267	632.891253	8.928295
6.976046	649.004205	8.933312
7.091609	642.254457	8.938330
7.005273	659.912615	8.943347
7.135501	652.301825	8.948365
7.606825	639.234500	8.953383
7.030978	637.283600	8.958400
7.128712	623.117202	8.963418
6.994408	619.727527	8.968435
6.660414	626.240762	8.973453
7.294460	629.313197	8.978471
7.288753	643.081853	8.983488
7.625932	642.303694	8.988506
7.057533	623.647891	8.993523
6.975941	619.452687	8.998541
7.038723	623.176770	9.003559
6.973004	634.143723	9.008576
7.235196	636.677775	9.013594
7.144769	657.664352	9.018611
6.888441	651.068697	9.023629
7.271377	652.371020	9.028647
7.145324	654.013519	9.033664
7.219907	649.740087	9.038682
7.054313	648.489706	9.043699
7.393082	655.502928	9.048717
7.384499	644.936572	9.053735
7.247841	643.199147	9.058752
7.269985	643.460102	9.063770
7.430672	647.403003	9.068787
6.950693	641.107364	9.073805
7.180872	641.775181	9.078823
7.052277	646.631679	9.083840
7.205421	633.948522	9.088858
7.149105	639.276876	9.093875
7.288438	654.852906	9.098893
7.451586	650.284903	9.103911
7.272895	656.763380	9.108928
7.438903	645.311866	9.113946
7.441669	654.529806	9.118963
7.188508	660.349791	9.123981
7.381901	641.517033	9.128999
6.983298	652.514322	9.134016
7.355134	643.219929	9.139034
7.536702	649.317112	9.144051
7.426223	650.953488	9.149069
7.529711	648.154312	9.154087
7.265887	653.870161	9.159104
7.607329	638.025305	9.164122
7.420030	655.634827	9.169139
7.403036	647.929135	9.174157
7.387490	631.653667	9.179175
7.434231	646.291537	9.184192
7.346570	641.091096	9.189210
7.409582	640.002455	9.194227
7.396760	647.653779	9.199245
7.696910	635.394675	9.204263
7.383258	626.388597	9.209280
7.261436	623.213769	9.214298
7.390084	623.099237	9.219315
7.518917	627.804446	9.224333
7.796229	616.992747	9.229351
7.546064	620.186012	9.234368
6.965243	615.888844	9.239386
7.130309	629.455598	9.244403
7.221782	638.802137	9.249421
7.490488	641.985857	9.254439
7.341212	661.281110	9.259456
7.404041	648.037342	9.264474
7.529766	654.263845	9.269491
7.731153	650.735509	9.274509
7.500062	650.851009	9.279527
7.249859	657.609027	9.284544
7.286462	644.889258	9.289562
7.593504	647.372186	9.294579
7.433948	655.144263	9.299597
7.853997	645.168305	9.304615
7.598527	656.717055	9.309632
7.670214	654.917964	9.314650
7.636198	651.006195	9.319667
7.320871	651.231700	9.324685
7.428199	642.933018	9.329703
7.413151	646.625116	9.334720
7.383150	646.831718	9.339738
7.203067	646.174251	9.344755
7.299354	644.402189	9.349773
7.287108	643.848024	9.354791
7.461710	643.923113	9.359808
7.291609	652.051243	9.364826
7.289641	661.428623	9.369843
7.493127	680.224960	9.374861
7.807737	674.748457	9.379879
8.098009	691.804163	9.384896
7.688384	678.692932	9.389914
7.780700	666.040686	9.394931
7.271648	653.422290	9.399949
8.013667	667.605304	9.404967
8.023173	665.656283	9.409984
7.439992	649.629901	9.415002
7.559302	654.098521	9.420019
7.547975	654.384703	9.425037
7.596430	663.557290	9.430055
7.764057	675.476122	9.435072
8.018668	678.657460	9.440090
7.910186	654.632866	9.445107
7.735553	656.875499	9.450125
7.812144	649.559402	9.455143
7.498706	654.254791	9.460160
7.638964	653.126980	9.465178
7.500311	652.818930	9.470195
7.685576	679.775262	9.475213
7.814113	685.249389	9.480231
7.887685	676.131525	9.485248
7.939691	677.691394	9.490266
7.651627	663.388463	9.495283
7.805050	676.424935	9.500301
8.212323	671.461404	9.505319
7.674924	661.304633	9.510336
7.448635	656.694037	9.515354
7.528714	655.570681	9.520371
7.802247	675.989564	9.525389
8.120307	678.675779	9.530407
7.876352	678.515866	9.535424
7.725878	691.655427	9.540442
8.296493	675.754867	9.545459
8.040783	676.188992	9.550477
7.861666	660.039787	9.555495
7.532449	656.763477	9.560512
7.597704	673.954844	9.565530
7.818422	677.162658	9.570547
7.619158	689.946145	9.575565
7.956141	672.251709	9.580583
8.028594	688.100248	9.585600
7.819582	688.555379	9.590618
7.896071	672.148887	9.595635
7.968528	683.848066	9.600653
8.192751	677.601932	9.605671
7.796763	688.778723	9.610688
7.807645	679.960984	9.615706
8.119134	678.259181	9.620723
7.672685	683.960010	9.625741
7.935878	681.153672	9.630759
7.888627	687.730074	9.635776
7.743794	689.134362	9.640794
8.140879	674.740010	9.645811
7.989300	692.423181	9.650829
8.003067	680.828751	9.655847
7.845518	675.357605	9.660864
7.688133	678.246164	9.665882
7.602847	681.243251	9.670899
7.971557	680.830713	9.675917
8.057985	677.418646	9.680935
7.694126	677.852963	9.685952
7.736076	679.346786	9.690970
8.111828	695.363993	9.695987
8.296305	706.619074	9.701005
8.050869	691.487059	9.706023
8.315072	699.583451	9.711040
7.825003	686.254839	9.716058
8.085369	696.339148	9.721075
8.199944	702.245096	9.726093
8.000023	696.576640	9.731111
8.153896	689.484721	9.736128
8.109821	694.756346	9.741146
8.286339	697.986444	9.746163
7.719249	698.065856	9.751181
8.082789	699.111175	9.756199
8.132277	701.617865	9.761216
7.976935	705.236757	9.766234
8.268171	697.876826	9.771251
8.218771	701.652967	9.776269
8.099861	694.383789	9.781287
8.270891	700.190629	9.786304
8.126217	703.586114	9.791322
8.260857	703.637507	9.796339
8.521953	701.139369	9.801357
8.026047	704.625298	9.806375
8.151998	705.408403	9.811392
8.166440	707.775630	9.816410
8.439071	699.595599	9.821427
8.181185	703.646408	9.826445
8.184876	702.855757	9.831463
8.373892	701.176988	9.836480
7.767082	703.096728	9.841498
8.164171	703.361734	9.846515
8.091323	710.147883	9.851533
8.004904	696.687857	9.856551
8.247192	695.588422	9.861568
8.137466	705.647806	9.866586
8.296511	697.096451	9.871603
8.110002	701.391724	9.876621
8.297361	696.803558	9.881639
8.713442	696.986683	9.886656
8.373518	697.498135	9.891674
8.366183	693.965772	9.896691
8.368119	703.167344	9.901709
8.331762	701.208197	9.906727
8.538378	700.598892	9.911744
8.458071	704.339209	9.916762
8.622412	705.616715	9.921779
8.055022	703.598662	9.926797
8.368271	709.431951	9.931815
8.286902	704.898125	9.936832
7.959828	705.068493	9.941850
8.122225	701.001358	9.946867
7.982706	711.568800	9.951885
8.310014	725.749679	9.956903
8.485732	727.641804	9.961920
8.254120	747.992077	9.966938
8.577854	728.375469	9.971955
8.442578	739.844932	9.976973
8.459294	740.361104	9.981991
8.600604	731.263878	9.987008
8.457084	737.054713	9.992026
8.590695	735.478023	9.997043
8.580411	727.807005	10.002061
8.388858	734.963195	10.007079
8.304481	737.538119	10.012096
8.656023	735.404504	10.017114
8.879898	739.250749	10.022131
9.031015	742.711822	10.027149
8.704559	726.640486	10.032167
8.666703	710.693414	10.037184
8.248291	713.124840	10.042202
8.633806	704.785964	10.047219
8.435007	706.662549	10.052237
8.318941	721.863246	10.057255
8.493956	725.777812	10.062272
8.776471	732.270493	10.067290
8.855370	733.891659	10.072307
8.828541	729.928682	10.077325
8.611056	718.353227	10.082343
8.637091	706.661476	10.087360
8.307256	711.970191	10.092378
8.454638	721.728365	10.097395
8.742618	730.461744	10.102413
8.796858	731.188619	10.107431
8.763059	735.236578	10.112448
8.779158	726.165208	10.117466
8.629214	712.359409	10.122483
8.644101	719.471959	10.127501
8.888977	714.770332	10.132519
8.630279	708.573447	10.137536
8.194885	704.537196	10.142554
8.569776	728.554114	10.147571
8.802186	731.263969	10.152589
8.796814	730.177197	10.157607
9.077227	731.886640	10.162624
8.475545	745.160802	10.167642
8.770457	726.496160	10.172659
8.681244	734.803054	10.177677
8.776256	736.239279	10.182695
8.766794	732.104931	10.187712
8.852917	736.807010	10.192730
9.114635	736.237002	10.197747
8.902914	738.562949	10.202765
8.622423	743.387940	10.207783
8.858768	734.078137	10.212800
9.084963	738.873157	10.217818
9.048435	719.319366	10.222835
8.751092	710.465254	10.227853
8.512066	710.487191	10.232871
8.992643	720.385846	10.237888
8.617919	733.134648	10.242906
8.751721	740.196416	10.247923
8.780611	743.307277	10.252941
8.859193	745.407997	10.257959
8.853772	731.643600	10.262976
8.719869	743.265585	10.267994
8.823169	740.433355	10.273011
8.913538	740.614514	10.278029
8.945967	739.320312	10.283047
8.608215	730.800814	10.288064
8.622046	739.193396	10.293082
8.683958	734.990933	10.298099
8.775215	736.377782	10.303117
8.819356	733.915171	10.308135
9.145915	724.684524	10.313152
8.955344	745.653553	10.318170
8.721750	743.182998	10.323187
8.924096	736.292861	10.328205
8.624181	750.462673	10.333223
9.009099	754.188953	10.338240
9.199816	767.149250	10.343258
9.145718	761.465284	10.348275
9.467929	766.474322	10.353293
8.890159	754.993538	10.358311
8.985249	735.908849	10.363328
8.890760	749.021866	10.368346
9.199325	755.897623	10.373363
9.506562	758.409669	10.378381
9.106914	758.867631	10.383399
9.100706	737.688807	10.388416
9.395301	736.719675	10.393434
9.032689	740.042996	10.398451
9.598699	742.283067	10.403469
9.119524	745.280828	10.408487
9.086797	742.603005	10.413504
9.104202	735.061248	10.418522
9.046126	735.403989	10.423539
9.273025	737.857293	10.428557
9.460321	737.829499	10.433575
9.393088	730.687171	10.438592
9.247393	738.495575	10.443610
8.875451	742.566068	10.448627
9.094812	744.645051	10.453645
9.214650	737.476861	10.458663
9.315069	741.241588	10.463680
9.122572	741.217633	10.468698
8.920137	741.907489	10.473715
9.259039	742.029384	10.478733
8.958976	736.977856	10.483751
9.314768	740.202291	10.488768
9.177568	748.529736	10.493786
9.056478	736.592656	10.498803
9.262735	736.528259	10.503821
9.063236	748.389838	10.508839
9.142044	768.321433	10.513856
9.164438	764.696340	10.518874
9.517143	777.699109	10.523891
9.515458	761.462940	10.528909
8.995373	774.799989	10.533927
9.363896	772.443097	10.538944
9.249817	767.098177	10.543962
9.423563	764.648744	10.548979
9.527437	763.815911	10.553997
9.597820	770.050051	10.559015
9.335888	758.869307	10.564032
9.348394	762.894252	10.569050
9.137156	767.036953	10.574067
9.269388	749.697971	10.579085
9.125700	762.437671	10.584103
9.035865	757.022602	10.589120
9.253480	758.877479	10.594138
9.281758	765.466602	10.599155
9.338349	768.369348	10.604173
9.170182	763.362503	10.609191
9.569345	760.490724	10.614208
9.000509	766.396878	10.619226
9.126623	769.166860	10.624243
9.102654	782.867801	10.629261
9.314657	796.733605	10.634279
9.785040	807.735127	10.639296
9.742047	804.353518	10.644314
9.726480	805.643503	10.649331
9.704826	805.635350	10.654349
9.848582	805.585634	10.659367
9.700232	794.143942	10.664384
9.524319	784.615383	10.669402
9.641820	771.424264	10.674419
9.725966	767.008672	10.679437
9.522771	775.542719	10.684455
9.556629	766.664043	10.689472
9.323378	763.034829	10.694490
9.482097	782.076878	10.699507
9.692787	801.120187	10.704525
9.514521	803.444934	10.709543
9.564822	801.531264	10.714560
9.432801	799.143481	10.719578
9.337218	798.292497	10.724595
9.628675	794.108303	10.729613
9.200128	803.923317	10.734631
9.574259	795.940196	10.739648
9.344731	797.189236	10.744666
9.415940	799.941938	10.749683
9.559411	808.932350	10.754701
9.352027	805.642133	10.759719
9.532121	811.425073	10.764736
9.953402	818.081810	10.769754
9.684308	819.662190	10.774771
10.091818	824.867348	10.779789
10.162566	815.566020	10.784807
9.907372	802.143693	10.789824
9.936990	796.501360	10.794842
9.332464	806.747464	10.799859
9.786791	795.532334	10.804877
9.754799	800.348868	10.809895
9.878042	790.891627	10.814912
9.740434	801.430468	10.819930
9.386452	796.778380	10.824947
9.945200	803.328099	10.829965
9.997947	808.867180	10.834983
9.490134	805.838905	10.840000
10.069279	812.091565	10.845018
10.056103	819.960344	10.850035
10.254110	802.749380	10.855053
9.846206	812.207456	10.860071
9.819063	795.012131	10.865088
10.064686	797.151730	10.870106
9.363726	794.746748	10.875123
10.249318	801.499810	10.880141
9.493380	799.823973	10.885159
9.647270	815.980795	10.890176
9.769287	814.439086	10.895194
9.986139	824.146452	10.900211
9.919333	827.833384	10.905229
10.045985	830.108037	10.910247
9.951330	832.951594	10.915264
10.267003	835.116604	10.920282
10.316304	832.488564	10.925299
10.250636	829.669338	10.930317
10.088563	819.571958	10.935335
10.013240	813.209633	10.940352
10.035687	816.837297	10.945370
9.984837	818.346500	10.950387
10.336878	825.662704	10.955405
10.235516	818.265371	10.960423
10.137229	811.947005	10.965440
10.050708	800.872216	10.970458
9.866990	814.644518	10.975475
10.331495	811.283588	10.980493
10.016053	802.749726	10.985511
9.708234	797.968346	10.990528
9.599347	819.507382	10.995546
9.601945	822.286016	11.000563
9.855854	823.985686	11.005581
10.324240	830.364169	11.010599
10.083575	824.895317	11.015616
10.588384	827.734876	11.020634
10.226152	840.998600	11.025651
10.716222	828.871666	11.030669
10.530425	827.939167	11.035687
10.570315	832.556810	11.040704
10.512555	828.913481	11.045722
10.284638	818.794330	11.050739
10.067392	806.853040	11.055757
10.177743	810.235056	11.060775
10.258088	818.273772	11.065792
10.722708	812.507040	11.070810
10.060160	814.382483	11.075827
10.168309	803.886054	11.080845
9.988885	817.846614	11.085863
10.004047	822.949033	11.090880
10.078123	824.545812	11.095898
9.682859	839.082657	11.100915
10.193575	829.462808	11.105933
10.115969	839.631128	11.110951
9.787655	838.486414	11.115968
10.511394	832.244111	11.120986
10.346662	837.333019	11.126003
10.236706	834.030992	11.131021
10.006526	846.150469	11.136039
10.218074	855.605202	11.141056
10.769372	862.608521	11.146074
10.401882	863.753252	11.151091
10.452417	862.762326	11.156109
10.427367	865.348705	11.161127
10.480557	860.334305	11.166144
10.727450	843.973426	11.171162
10.021509	852.617143	11.176179
10.250294	868.793899	11.181197
10.072716	862.422897	11.186215
10.101484	868.270286	11.191232
10.409064	867.395448	11.196250
10.431059	867.244640	11.201267
10.548319	860.159888	11.206285
10.563123	863.572304	11.211303
10.212494	864.993364	11.216320
10.538526	863.897371	11.221338
10.283536	868.656370	11.226355
10.560634	857.219767	11.231373
10.787313	864.153619	11.236391
10.844242	875.153186	11.241408
10.726583	864.711430	11.246426
10.353953	868.225404	11.251443
10.269927	868.353951	11.256461
10.546960	866.579491	11.261479
10.416932	863.720524	11.266496
10.905550	862.401555	11.271514
10.614098	866.294980	11.276531
10.568387	863.204739	11.281549
10.738143	863.294411	11.286567
10.579882	865.274926	11.291584
10.614044	863.587139	11.296602
10.887779	876.375127	11.301619
10.593773	861.502945	11.306637
10.793620	871.791869	11.311655
10.879583	878.968703	11.316672
10.669403	857.277061	11.321690
10.161025	872.955449	11.326707
10.366704	885.883054	11.331725
11.099576	885.573588	11.336743
11.027315	895.611144	11.341760
11.069228	885.366955	11.346778
11.119134	890.748276	11.351795
10.849175	874.509958	11.356813
10.958836	865.547810	11.361831
10.925519	867.270639	11.366848
10.849711	851.441119	11.371866
10.705260	861.188653	11.376883
10.835331	861.153407	11.381901
10.867783	855.360591	11.386919
10.936827	865.219618	11.391936
10.970189	862.830422	11.396954
10.754922	863.830661	11.401971
10.688709	856.416860	11.406989
11.050884	863.046791	11.412007
11.046788	878.198786	11.417024
11.107342	868.402682	11.422042
10.797752	855.463703	11.427059
10.910817	868.762125	11.432077
11.010961	868.481060	11.437095
10.643645	874.462146	11.442112
11.071871	880.481964	11.447130
10.747349	881.559742	11.452147
11.197608	886.396441	11.457165
11.425803	878.600822	11.462183
11.051703	879.238799	11.467200
10.870162	862.612248	11.472218
10.850929	873.600805	11.477235
10.835393	887.278002	11.482253
11.024101	889.257361	11.487271
10.911843	891.992431	11.492288
11.215658	888.217564	11.497306
10.855426	889.522111	11.502323
10.871692	887.212904	11.507341
11.179537	892.633398	11.512359
11.042675	892.476614	11.517376
11.141902	888.485636	11.522394
10.841860	885.626473	11.527411
10.688339	890.626145	11.532429
10.965460	882.983045	11.537447
11.296355	891.098020	11.542464
11.204732	890.303852	11.547482
11.401543	890.846898	11.552499
11.210497	891.810452	11.557517
11.256268	886.241786	11.562535
11.153723	887.967814	11.567552
10.965233	885.377567	11.572570
11.029424	895.894079	11.577587
11.139237	899.454149	11.582605
11.203878	898.131372	11.587623
11.308394	916.412912	11.592640
11.503832	904.372109	11.597658
11.567464	899.476040	11.602675
11.540089	889.646454	11.607693
11.719130	883.320715	11.612711
11.349534	892.434717	11.617728
11.444857	897.864816	11.622746
11.518743	894.968927	11.627763
11.351467	892.753889	11.632781
11.496888	885.720364	11.637799
11.305005	893.051870	11.642816
11.537213	882.046679	11.647834
11.278455	885.498101	11.652851
11.498916	886.552166	11.657869
11.570921	883.636120	11.662887
11.218645	891.056781	11.667904
11.395173	897.465906	11.672922
11.347449	897.425851	11.677939
11.444852	886.632341	11.682957
11.588702	887.081405	11.687975
11.294594	887.983289	11.692992
11.239655	879.108623	11.698010
11.274468	884.085767	11.703027
11.370659	883.418366	11.708045
11.229807	881.018647	11.713063
11.043883	910.565074	11.718080
11.612010	916.303089	11.723098
11.822343	926.645035	11.728115
11.705137	920.935635	11.733133
12.082296	924.632141	11.738151
11.566905	910.440243	11.743168
11.391588	892.034757	11.748186
11.868449	908.214962	11.753203
11.462701	903.243475	11.758221
11.627005	895.653694	11.763239
11.374428	900.579619	11.768256
11.926294	911.829128	11.773274
12.016921	919.592191	11.778291
11.657991	892.780480	11.783309
11.731920	886.630800	11.788327
11.485797	888.152661	11.793344
11.603030	898.643857	11.798362
11.844214	900.179508	11.803379
11.522078	902.422194	11.808397
12.011094	917.720908	11.813415
11.967805	903.945699	11.818432
11.714991	897.434786	11.823450
11.718603	890.069246	11.828467
11.422726	886.637373	11.833485
12.035936	891.338434	11.838503
11.801584	913.600706	11.843520
11.616523	903.262995	11.848538
11.707506	913.675875	11.853555
11.949707	922.599219	11.858573
11.861184	916.149277	11.863591
11.595927	928.491546	11.868608
12.074849	921.783078	11.873626
12.116944	924.335514	11.878643
11.834281	921.922266	11.883661
12.104074	912.949321	11.888679
11.923755	916.149583	11.893696
11.861843	910.507405	11.898714
11.943324	914.913864	11.903731
11.947219	917.639941	11.908749
12.288329	909.324056	11.913767
11.629386	893.933953	11.918784
11.596837	914.258173	11.923802
12.014892	916.244832	11.928819
11.954817	922.166005	11.933837
12.191866	914.666133	11.938855
12.064409	920.025261	11.943872
12.207188	920.820551	11.948890
12.287610	915.991772	11.953907
12.038136	920.359340	11.958925
12.361465	911.886563	11.963943
12.055282	900.796505	11.968960
11.762979	892.904794	11.973978
11.863394	896.995922	11.978995
12.125499	914.018350	11.984013
12.076735	908.858620	11.989031
11.896505	920.532502	11.994048
12.000488	914.754195	11.999066
12.006167	910.314550	12.004083
11.984718	924.341168	12.009101
12.188024	926.522437	12.014119
12.266243	918.972883	12.019136
12.406219	924.655034	12.024154
12.388908	915.515467	12.029171
12.015171	922.294056	12.034189
12.420749	915.132008	12.039207
12.340752	921.269463	12.044224
12.335695	920.980621	12.049242
12.507782	921.367926	12.054259
12.374485	917.721337	12.059277
12.375942	918.721517	12.064295
12.469972	914.633759	12.069312
12.163491	922.484627	12.074330
12.310850	912.198158	12.079347
12.162181	914.627071	12.084365
12.379931	920.427438	12.089383
12.255735	920.206355	12.094400
12.020386	915.287746	12.099418
12.295777	918.874336	12.104435
12.162133	923.086116	12.109453
12.030934	917.856179	12.114471
12.422005	909.719808	12.119488
12.092842	924.838279	12.124506
12.320384	920.584324	12.129523
12.291932	920.355259	12.134541
12.532125	920.208081	12.139559
12.458216	921.264834	12.144576
12.253696	912.673568	12.149594
12.397986	936.685690	12.154611
12.304258	941.310532	12.159629
12.686885	948.520947	12.164647
12.961777	949.995906	12.169664
12.463855	936.112890	12.174682
12.343480	923.408257	12.179699
12.251648	935.043891	12.184717
12.378020	939.977152	12.189735
12.304055	941.118557	12.194752
12.451409	941.998126	12.199770
12.743627	944.320573	12.204787
12.215823	948.933442	12.209805
12.657616	949.388286	12.214823
12.507996	938.273456	12.219840
12.176937	950.845133	12.224858
12.891144	934.829198	12.229875
12.563033	944.528067	12.234893
12.780459	940.299795	12.239911
12.706103	948.092160	12.244928
12.481417	951.563938	12.249946
12.578070	948.922132	12.254963
12.699945	952.380614	12.259981
12.883178	954.689221	12.264999
12.569216	946.138106	12.270016
12.623931	951.246616	12.275034
13.278343	951.869393	12.280051
12.363446	957.651829	12.285069
12.957758	953.052496	12.290087
12.841670	960.950987	12.295104
12.397976	967.879363	12.300122
12.593665	971.399246	12.305139
12.674981	989.763845	12.310157
12.804620	983.052955	12.315175
13.070403	981.753554	12.320192
13.000309	990.420002	12.325210
12.960796	980.169157	12.330227
13.217339	979.479530	12.335245
13.069933	976.168321	12.340263
13.088846	967.297910	12.345280
13.072459	986.408181	12.350298
13.168876	960.213836	12.355315
12.562145	962.306814	12.360333
12.839907	965.492252	12.365351
13.102618	975.541317	12.370368
13.313518	970.999565	12.375386
13.246125	964.416188	12.380403
13.072331	961.234937	12.385421
12.700746	955.824330	12.390439
13.065791	966.719399	12.395456
13.158800	969.282309	12.400474
13.131691	967.973538	12.405491
13.042255	972.153602	12.410509
13.106967	982.519699	12.415527
13.214879	979.716188	12.420544
12.866696	979.975483	12.425562
13.348790	974.203831	12.430579
13.095449	982.834480	12.435597
12.898916	978.081464	12.440615
13.109803	981.209872	12.445632
13.051987	984.983144	12.450650
13.137006	986.578915	12.455667
13.056283	976.282143	12.460685
13.151267	989.240370	12.465703
13.298520	982.302951	12.470720
13.335948	977.899366	12.475738
13.445225	984.504695	12.480755
13.366248	980.488481	12.485773
13.250652	978.075904	12.490791
13.258559	974.404738	12.495808
12.924990	986.633567	12.500826
13.296949	974.939054	12.505843
13.531061	979.542688	12.510861
13.493059	971.147823	12.515879
13.400904	981.677291	12.520896
13.194411	985.319285	12.525914
13.256905	982.787063	12.530931
13.260757	986.535951	12.535949
13.110350	974.699207	12.540967
13.179698	974.534259	12.545984
12.719728	986.357264	12.551002
12.950342	989.883966	12.556019
13.416347	1005.302320	12.561037
13.354575	1018.576281	12.566055
13.279966	1018.142268	12.571072
13.322962	1021.880353	12.576090
13.419104	1021.289330	12.581107
13.430276	1024.785450	12.586125
13.408144	1020.719656	12.591143
13.445630	1020.052129	12.596160
12.873318	1014.627891	12.601178
13.371957	1020.453040	12.606195
13.227292	1011.074672	12.611213
13.373979	1030.499713	12.616231
13.810453	1046.987920	12.621248
13.803165	1049.123767	12.626266
14.021993	1045.323960	12.631283
13.950301	1040.470334	12.636301
13.694333	1025.979869	12.641319
13.628616	1008.248984	12.646336
13.842236	1013.296949	12.651354
13.706218	1007.394971	12.656371
13.632272	1010.420163	12.661389
13.600055	1013.982913	12.666407
14.043368	1009.907368	12.671424
13.765915	1010.754534	12.676442
13.788592	1005.107763	12.681459
13.822904	1009.250417	12.686477
13.579082	1012.383657	12.691495
13.789686	1004.784188	12.696512
13.626718	1013.255013	12.701530
13.647367	1008.768374	12.706547
13.681179	1035.985435	12.711565
13.817727	1044.311800	12.716583
13.653272	1046.426824	12.721600
13.641100	1046.397810	12.726618
13.776136	1053.826826	12.731635
13.967774	1045.634436	12.736653
13.962153	1054.170563	12.741671
13.855394	1046.976763	12.746688
13.613696	1044.978743	12.751706
13.765669	1042.367524	12.756723
14.015976	1039.012095	12.761741
14.015015	1049.415883	12.766759
14.185561	1042.574970	12.771776
13.916817	1048.398467	12.776794
14.023384	1045.083768	12.781811
14.217713	1041.102199	12.786829
13.807330	1044.420108	12.791847
13.886155	1038.824261	12.796864
13.732807	1043.557427	12.801882
13.864716	1045.204492	12.806899
14.258583	1033.475206	12.811917
14.059204	1035.264134	12.816935
14.058895	1044.996575	12.821952
13.968077	1044.892399	12.826970
14.189312	1050.836721	12.831987
14.078212	1055.321171	12.837005
14.048776	1057.857129	12.842023
14.294267	1053.829685	12.847040
14.373526	1070.531394	12.852058
14.692634	1063.041484	12.857075
14.434814	1049.123725	12.862093
14.390250	1040.468107	12.867111
14.222763	1036.656685	12.872128
14.104069	1042.125423	12.877146
14.241764	1034.367153	12.882163
14.409064	1039.140524	12.887181
13.800036	1039.606787	12.892199
14.171327	1038.173380	12.897216
14.097164	1052.367498	12.902234
14.158023	1056.456951	12.907251
14.741890	1061.636923	12.912269
14.549181	1071.489821	12.917287
14.790930	1055.598846	12.922304
14.487597	1053.254352	12.927322
14.262084	1037.890754	12.932339
14.818784	1040.235558	12.937357
14.297384	1043.743104	12.942375
14.398808	1035.468811	12.947392
14.434247	1040.135677	12.952410
14.275038	1037.172065	12.957427
14.141005	1042.607518	12.962445
14.066412	1066.698211	12.967463
14.432691	1066.164419	12.972480
14.415919	1065.453907	12.977498
14.465683	1074.558412	12.982515
14.697645	1070.627295	12.987533
14.135653	1072.514460	12.992551
14.146723	1069.788778	12.997568
14.038053	1076.968014	13.002586
14.359325	1077.037716	13.007603
14.442003	1086.644634	13.012621
14.619510	1105.283589	13.017639
14.903642	1099.140748	13.022656
14.495069	1114.060355	13.027674
14.547088	1103.808051	13.032691
14.819179	1101.562351	13.037709
14.835978	1103.547371	13.042727
14.901379	1102.987419	13.047744
14.863224	1099.605338	13.052762
14.873238	1100.393883	13.057779
14.828537	1089.394637	13.062797
14.459077	1093.193164	13.067815
14.785337	1093.039213	13.072832
14.501126	1097.428330	13.077850
14.518025	1102.450634	13.082867
14.864920	1097.174144	13.087885
14.710393	1103.055910	13.092903
14.790352	1095.741802	13.097920
14.576662	1104.547048	13.102938
14.796357	1099.435710	13.107955
14.779275	1099.832299	13.112973
14.738014	1104.343386	13.117991
14.736759	1086.817871	13.123008
15.064574	1100.249429	13.128026
14.904012	1097.740346	13.133043
15.259690	1099.561379	13.138061
14.972925	1105.588268	13.143079
14.889338	1095.802504	13.148096
14.882026	1091.279529	13.153114
14.781439	1101.830946	13.158131
15.242810	1093.035223	13.163149
14.846590	1095.612633	13.168167
14.888296	1091.740573	13.173184
14.728037	1105.031704	13.178202
14.949173	1123.879985	13.183219
15.434823	1128.033363	13.188237
15.150214	1127.923876	13.193255
15.244538	1130.407463	13.198272
15.360934	1125.591560	13.203290
15.268629	1129.652460	13.208307
15.390303	1118.753592	13.213325
15.301172	1117.685386	13.218343
15.358751	1100.284361	13.223360
15.045861	1102.216105	13.228378
15.212576	1098.313107	13.233395
15.360893	1089.127901	13.238413
15.046283	1103.231178	13.243431
15.236565	1114.310797	13.248448
15.359349	1132.016751	13.253466
15.364171	1132.700648	13.258483
15.615468	1122.748787	13.263501
15.180091	1113.238188	13.268519
15.171341	1109.619353	13.273536
15.672141	1124.931675	13.278554
15.633320	1119.689915	13.283571
15.509297	1100.394220	13.288589
15.467053	1108.627396	13.293607
15.364879	1103.410699	13.298624
15.359163	1105.077018	13.303642
15.362567	1105.358800	13.308659
15.626772	1102.949057	13.313677
15.245046	1100.461243	13.318695
15.269801	1101.869767	13.323712
15.414532	1113.421481	13.328730
15.233856	1125.127479	13.333747
15.624079	1131.358406	13.338765
15.116758	1130.428344	13.343783
15.298486	1130.238879	13.348800
15.749790	1127.452098	13.353818
15.545079	1128.390765	13.358835
15.817102	1132.307874	13.363853
15.856638	1128.534980	13.368871
15.740000	1131.843634	13.373888
15.996983	1126.667847	13.378906
15.833338	1137.117923	13.383923
16.026687	1125.698535	13.388941
15.888197	1135.335021	13.393959
15.964653	1125.358568	13.398976
15.630670	1104.731143	13.403994
15.355482	1104.374041	13.409011
15.825617	1117.371037	13.414029
15.673400	1128.359749	13.419047
15.713864	1130.514076	13.424064
15.757502	1131.686413	13.429082
15.606673	1134.194849	13.434099
16.019797	1120.074981	13.439117
15.689884	1127.393629	13.444135
15.762986	1130.470082	13.449152
15.938823	1132.192951	13.454170
15.820747	1128.116640	13.459187
16.124066	1122.235958	13.464205
15.827297	1133.852922	13.469223
15.899857	1126.272710	13.474240
16.178974	1127.094645	13.479258
15.993899	1123.465242	13.484275
15.709002	1137.180571	13.489293
15.999831	1139.385565	13.494311
15.987462	1136.466908	13.499328
15.932558	1132.318325	13.504346
15.935611	1137.276400	13.509363
16.236410	1130.432383	13.514381
15.981685	1137.646856	13.519399
15.966758	1131.590137	13.524416
16.025401	1121.184366	13.529434
15.683821	1133.108347	13.534451
15.896504	1128.422163	13.539469
15.974250	1124.462241	13.544487
16.137533	1122.252666	13.549504
16.053687	1139.957018	13.554522
16.238048	1152.040371	13.559539
16.295463	1156.249315	13.564557
16.329312	1165.238796	13.569575
16.017166	1156.475065	13.574592
16.363692	1160.371182	13.579610
16.033902	1168.458310	13.584627
16.170483	1166.855890	13.589645
16.218383	1162.207218	13.594663
16.205315	1164.810560	13.599680
16.062230	1167.381497	13.604698
16.225037	1168.763230	13.609715
16.545389	1163.537962	13.614733
16.540324	1167.406084	13.619751
16.502667	1163.588092	13.624768
16.359321	1162.409967	13.629786
16.189672	1165.695124	13.634803
16.596354	1161.338607	13.639821
16.138479	1164.234102	13.644839
16.272808	1164.766639	13.649856
16.395484	1157.769434	13.654874
16.869391	1164.418394	13.659891
16.457292	1158.530580	13.664909
16.466405	1159.407463	13.669927
16.349968	1165.599472	13.674944
16.481675	1165.323805	13.679962
16.393928	1165.665169	13.684979
16.743377	1156.845031	13.689997
16.378471	1172.546022	13.695015
16.287963	1166.232128	13.700032
16.699988	1167.169849	13.705050
16.748698	1182.656694	13.710067
16.659121	1185.452231	13.715085
16.673677	1176.488724	13.720103
16.856767	1185.078317	13.725120
16.890802	1184.220808	13.730138
16.350809	1181.459589	13.735155
16.469116	1181.400702	13.740173
16.611509	1185.975493	13.745191
16.835589	1189.527731	13.750208
16.813749	1183.742995	13.755226
17.148309	1178.990553	13.760243
16.943226	1182.082374	13.765261
16.826577	1184.769404	13.770279
16.671631	1186.182104	13.775296
16.885506	1183.197235	13.780314
16.685981	1187.114098	13.785331
17.067072	1184.870415	13.790349
17.308971	1173.539801	13.795367
17.214377	1176.602695	13.800384
16.983309	1176.026086	13.805402
17.084388	1181.667924	13.810419
16.961382	1176.769997	13.815437
17.304998	1179.339080	13.820455
16.958891	1172.293908	13.825472
16.890659	1152.951114	13.830490
16.749960	1169.760218	13.835507
16.952086	1180.113535	13.840525
17.164949	1182.807417	13.845543
16.987143	1175.815474	13.850560
17.112538	1175.857772	13.855578
17.072608	1184.409493	13.860595
17.230465	1183.728325	13.865613
17.065253	1182.203436	13.870631
16.628738	1185.889077	13.875648
17.152793	1188.610167	13.880666
16.686434	1192.880263	13.885683
16.901105	1182.632074	13.890701
17.135458	1179.865462	13.895719
17.074588	1186.988016	13.900736
17.025180	1192.046525	13.905754
16.995084	1216.625345	13.910771
17.397277	1215.565141	13.915789
17.455579	1210.141919	13.920807
17.090782	1221.849345	13.925824
17.571043	1211.223702	13.930842
17.448406	1218.517911	13.935859
17.251920	1220.381575	13.940877
17.626599	1222.114440	13.945895
17.412489	1225.812473	13.950912
17.666869	1213.106175	13.955930
17.204407	1221.352698	13.960947
17.476051	1221.385345	13.965965
17.371034	1222.387034	13.970983
17.092331	1216.511753	13.976000
17.360045	1215.484841	13.981018
17.234420	1215.828936	13.986035
17.271097	1213.521025	13.991053
17.569588	1207.626938	13.996071
17.110072	1216.191860	14.001088
17.403173	1229.304090	14.006106
17.376028	1245.266145	14.011123
17.504771	1246.612976	14.016141
17.792444	1255.198676	14.021159
17.460130	1258.816293	14.026176
17.779331	1247.048818	14.031194
17.697040	1248.369966	14.036211
17.635792	1253.513525	14.041229
17.857776	1251.954433	14.046247
17.520614	1255.266166	14.051264
17.536879	1247.858205	14.056282
17.732583	1244.350755	14.061299
17.775298	1240.864309	14.066317
18.018266	1251.825856	14.071335
17.648773	1249.924954	14.076352
17.773334	1242.943146	14.081370
18.082008	1248.721495	14.086387
17.984691	1248.896339	14.091405
18.184396	1240.922191	14.096423
17.810195	1247.109672	14.101440
17.689115	1241.842517	14.106458
17.609923	1242.293881	14.111475
17.710564	1256.887577	14.116493
17.908907	1243.962585	14.121511
17.729681	1251.554363	14.126528
17.849347	1261.553287	14.131546
18.028239	1261.521767	14.136563
18.157129	1275.399401	14.141581
18.317174	1274.273388	14.146599
17.940459	1280.124692	14.151616
18.216627	1276.811387	14.156634
18.390307	1277.981098	14.161651
18.263752	1275.589580	14.166669
18.614137	1255.154134	14.171687
18.230730	1265.723362	14.176704
18.308811	1245.634981	14.181722
18.267790	1245.319806	14.186739
17.875261	1253.452011	14.191757
18.217327	1244.025581	14.196775
18.133529	1239.021145	14.201792
17.985309	1245.544031	14.206810
18.185275	1265.867609	14.211827
18.348276	1270.464603	14.216845
18.694557	1269.957737	14.221863
18.436252	1276.850826	14.226880
18.555637	1264.640058	14.231898
18.531078	1248.627635	14.236915
18.270414	1241.880086	14.241933
18.224958	1244.776199	14.246951
18.049833	1264.645364	14.251968
18.480076	1269.551640	14.256986
18.427914	1264.754157	14.262003
18.269137	1278.983359	14.267021
18.449794	1275.321311	14.272039
18.501056	1277.694732	14.277056
18.527828	1275.409712	14.282074
18.450585	1270.354968	14.287091
18.428963	1281.136733	14.292109
18.559430	1268.714289	14.297127
18.360483	1282.274177	14.302144
18.461198	1276.990755	14.307162
18.463094	1275.094491	14.312179
18.455012	1285.445286	14.317197
18.578927	1275.936853	14.322215
18.445902	1291.636967	14.327232
18.644937	1299.981862	14.332250
19.018961	1303.669530	14.337267
18.751088	1312.624415	14.342285
19.203512	1304.330439	14.347303
18.802142	1294.929842	14.352320
19.160049	1272.662849	14.357338
18.991567	1277.046238	14.362355
18.432908	1277.687626	14.367373
19.092989	1260.827583	14.372391
18.938474	1282.307495	14.377408
18.863018	1273.270256	14.382426
18.966900	1275.303081	14.387443
18.364256	1273.405352	14.392461
18.680454	1293.290830	14.397479
18.608128	1306.292775	14.402496
18.438148	1306.570201	14.407514
18.853407	1302.616548	14.412531
19.070738	1305.239634	14.417549
19.087101	1299.596164	14.422567
18.839380	1315.958589	14.427584
19.236092	1304.719171	14.432602
19.107765	1299.272885	14.437619
18.899225	1312.062749	14.442637
18.958810	1295.130456	14.447655
18.870415	1305.698497	14.452672
18.997210	1314.143549	14.457690
19.044643	1322.637968	14.462707
18.815629	1335.204474	14.467725
19.419306	1333.985705	14.472743
19.184360	1336.729357	14.477760
19.119431	1341.712928	14.482778
19.508983	1336.221818	14.487795
19.077405	1334.648896	14.492813
19.428764	1335.057707	14.497831
19.707255	1334.286086	14.502848
19.436464	1334.908547	14.507866
19.644852	1330.678518	14.512883
19.189788	1335.039300	14.517901
19.534665	1329.647320	14.522919
19.570242	1330.919824	14.527936
19.518018	1334.505251	14.532954
19.715342	1333.648253	14.537971
19.624312	1324.295853	14.542989
19.545599	1305.208931	14.548007
19.372363	1308.505735	14.553024
19.504100	1301.811290	14.558042
19.452681	1311.191739	14.563059
19.253476	1323.865896	14.568077
19.685597	1324.017637	14.573095
19.305356	1326.918022	14.578112
19.578387	1327.084296	14.583130
19.670534	1324.581360	14.588147
19.570622	1330.600228	14.593165
19.428094	1331.365620	14.598183
19.621653	1336.531972	14.603200
19.670307	1334.888190	14.608218
19.860952	1335.224009	14.613235
19.636042	1336.151072	14.618253
19.648810	1329.577888	14.623271
19.638702	1335.666532	14.628288
19.484448	1334.433114	14.633306
19.768494	1334.170800	14.638323
19.873457	1334.887336	14.643341
19.771292	1324.550970	14.648359
19.346222	1329.377642	14.653376
19.713232	1351.346869	14.658394
20.139970	1353.599073	14.663411
19.926182	1361.904883	14.668429
20.335588	1356.623073	14.673447
20.234006	1358.474975	14.678464
19.875130	1354.827448	14.683482
19.974964	1351.517736	14.688499
19.823100	1364.834076	14.693517
20.238842	1352.821405	14.698535
20.346707	1360.298374	14.703552
19.911295	1360.705974	14.708570
20.283028	1365.957003	14.713587
19.969541	1362.722030	14.718605
20.371121	1356.224607	14.723623
20.292230	1358.449910	14.728640
20.049860	1361.919195	14.733658
20.232141	1358.667875	14.738675
20.124722	1361.395139	14.743693
19.956533	1358.317600	14.748711
20.095728	1359.453265	14.753728
19.854547	1356.977568	14.758746
20.282561	1355.065062	14.763763
20.304940	1361.986118	14.768781
20.186033	1363.946400	14.773799
20.353257	1356.089775	14.778816
20.522593	1363.207359	14.783834
20.574513	1354.702122	14.788851
20.287777	1355.568952	14.793869
20.015512	1362.249433	14.798887
19.864450	1359.366693	14.803904
20.094776	1369.083587	14.808922
20.570359	1380.861024	14.813939
20.511554	1393.143097	14.818957
20.557445	1376.874784	14.823975
21.001502	1383.814999	14.828992
20.413338	1392.804463	14.834010
21.011064	1377.654989	14.839027
20.813098	1383.985386	14.844045
20.875802	1376.038580	14.849063
21.138043	1357.487645	14.854080
20.491653	1350.124405	14.859098
20.700730	1345.171042	14.864115
20.984290	1340.547861	14.869133
20.627838	1341.832527	14.874151
20.586454	1339.832793	14.879168
20.284901	1349.123192	14.884186
20.494467	1360.963561	14.889203
20.506510	1372.386655	14.894221
21.027327	1379.394077	14.899239
21.053546	1373.164705	14.904256
20.728169	1381.885455	14.909274
20.829772	1377.809314	14.914291
21.060558	1379.498703	14.919309
21.062869	1381.116872	14.924327
21.157302	1381.847358	14.929344
20.878126	1386.243989	14.934362
20.864458	1381.147580	14.939379
20.989418	1382.171432	14.944397
20.971146	1387.239810	14.949415
20.913843	1385.130504	14.954432
20.715930	1385.323582	14.959450
20.872390	1386.763079	14.964467
20.922281	1387.388738	14.969485
21.048705	1390.659560	14.974503
21.104910	1383.313424	14.979520
21.223800	1387.159106	14.984538
21.417055	1389.919263	14.989555
20.772574	1385.081638	14.994573
20.936876	1393.451233	14.999591
21.223067	1408.434024	15.004608
21.114462	1412.318959	15.009626
21.457551	1406.135527	15.014643
21.060953	1414.045264	15.019661
21.176179	1426.312324	15.024679
21.736756	1411.339440	15.029696
21.654329	1417.964494	15.034714
21.455612	1413.954215	15.039731
21.207998	1416.121247	15.044749
21.566348	1412.639582	15.049767
21.740755	1418.132751	15.054784
21.685442	1411.731828	15.059802
21.544787	1409.658367	15.064819
21.471279	1420.622834	15.069837
21.478793	1410.851313	15.074855
21.539637	1414.969604	15.079872
21.355399	1413.889961	15.084890
21.718125	1410.792213	15.089907
21.510108	1415.134156	15.094925
21.752624	1412.442134	15.099943
21.758024	1401.728855	15.104960
21.900145	1416.925667	15.109978
21.432418	1406.669859	15.114995
21.442092	1406.697068	15.120013
21.503616	1410.421549	15.125031
21.535346	1411.783672	15.130048
21.482932	1408.324752	15.135066
22.266438	1399.278667	15.140083
21.916129	1406.873652	15.145101
21.639600	1413.952888	15.150119
21.868620	1402.060074	15.155136
21.826359	1417.011043	15.160154
21.937765	1416.574956	15.165171
21.871443	1406.131028	15.170189
22.101660	1420.162089	15.175207
21.869712	1409.111734	15.180224
21.341250	1417.548813	15.185242
22.038361	1432.277365	15.190259
21.962263	1440.790336	15.195277
22.203399	1437.958383	15.200295
22.312515	1439.079350	15.205312
21.981870	1445.574654	15.210330
22.062597	1438.696079	15.215347
22.139534	1441.067636	15.220365
21.803100	1453.146912	15.225383
22.006074	1439.588715	15.230400
22.000931	1437.198327	15.235418
22.341568	1436.325860	15.240435
22.354009	1437.263231	15.245453
22.503031	1431.481999	15.250471
22.262059	1435.061303	15.255488
22.397661	1445.149832	15.260506
22.231257	1427.568997	15.265523
22.281910	1431.824411	15.270541
22.206080	1432.597266	15.275559
22.036523	1439.561557	15.280576
22.024288	1432.294446	15.285594
22.446334	1432.737224	15.290611
22.630423	1438.546116	15.295629
22.421665	1434.124901	15.300647
22.243423	1435.436757	15.305664
21.834493	1450.551230	15.310682
22.543704	1457.472374	15.315699
22.537552	1462.986403	15.320717
22.554566	1473.573322	15.325735
22.804423	1470.602519	15.330752
22.630847	1472.495884	15.335770
22.793162	1466.342363	15.340787
22.497192	1471.629978	15.345805
22.587081	1482.115074	15.350823
23.104947	1462.677992	15.355840
22.606257	1474.142032	15.360858
22.755546	1472.741412	15.365875
22.684908	1477.443690	15.370893
22.563872	1474.974456	15.375911
23.024679	1475.355305	15.380928
22.708348	1476.101847	15.385946
22.339465	1471.029190	15.390963
22.564739	1476.928126	15.395981
22.796549	1471.011912	15.400999
23.067534	1479.707979	15.406016
22.852248	1494.421928	15.411034
23.104120	1497.006257	15.416051
23.422208	1495.550124	15.421069
23.172761	1494.431668	15.426087
23.144936	1470.932607	15.431104
22.949201	1466.226551	15.436122
23.057732	1464.727563	15.441139
22.957246	1473.207188	15.446157
23.019017	1494.092921	15.451175
23.147054	1493.327703	15.456192
23.175676	1500.993057	15.461210
23.513814	1495.622608	15.466227
23.704633	1492.832048	15.471245
23.406339	1482.827658	15.476263
23.278210	1463.685339	15.481280
23.477922	1466.231057	15.486298
23.558421	1464.480413	15.491315
23.525872	1450.370268	15.496333
23.143872	1465.806277	15.501351
23.650540	1456.961117	15.506368
23.608781	1456.167719	15.511386
23.423084	1449.642702	15.516403
23.778972	1459.463269	15.521421
23.277737	1462.028600	15.526439
23.629815	1450.520880	15.531456
23.528447	1458.422696	15.536474
23.420145	1464.396943	15.541491
23.316864	1460.850372	15.546509
23.262371	1471.699523	15.551527
23.847366	1457.043416	15.556544
23.353053	1462.511115	15.561562
23.413437	1469.557814	15.566579
23.848339	1478.903503	15.571597
23.288952	1494.014192	15.576615
23.407231	1490.817144	15.581632
23.629606	1498.878363	15.586650
23.472835	1497.307556	15.591667
23.726587	1495.131766	15.596685
23.259864	1495.461089	15.601703
23.887795	1497.052839	15.606720
23.410816	1504.633415	15.611738
23.496070	1513.214587	15.616755
23.485989	1506.827001	15.621773
23.294502	1529.481084	15.626791
23.966881	1522.392297	15.631808
23.721026	1527.627539	15.636826
23.651733	1526.784365	15.641843
23.942308	1528.119778	15.646861
23.976981	1533.312506	15.651879
23.932881	1523.312060	15.656896
24.209369	1533.875740	15.661914
24.088991	1529.131990	15.666931
24.436505	1529.644593	15.671949
24.127176	1533.806102	15.676967
24.163718	1531.385174	15.681984
24.200595	1522.399662	15.687002
23.855888	1533.617383	15.692019
24.572783	1551.224648	15.697037
24.128247	1562.890415	15.702055
24.640217	1558.131710	15.707072
24.667438	1543.690324	15.712090
23.951019	1534.645685	15.717107
24.384995	1546.032896	15.722125
24.662511	1549.300780	15.727143
24.680399	1538.160144	15.732160
24.485530	1536.921624	15.737178
24.307847	1527.498805	15.742195
24.517209	1518.295364	15.747213
24.299900	1534.797077	15.752231
24.466028	1537.854270	15.757248
24.291563	1546.511933	15.762266
24.554749	1547.260152	15.767283
24.693847	1538.346286	15.772301
24.714248	1554.324014	15.777319
24.667602	1542.442489	15.782336
24.579313	1545.511498	15.787354
24.511944	1550.999868	15.792371
24.656765	1542.023241	15.797389
24.830048	1552.730794	15.802407
24.618997	1547.316230	15.807424
24.789227	1552.129826	15.812442
24.959530	1545.355268	15.817459
24.981819	1542.848117	15.822477
25.031346	1549.449015	15.827495
24.803817	1546.363154	15.832512
25.138597	1542.577491	15.837530
24.993594	1541.347643	15.842547
25.250531	1541.044146	15.847565
24.908167	1549.983549	15.852583
24.916841	1548.019594	15.857600
25.326067	1541.116105	15.862618
25.141035	1546.971594	15.867635
25.234654	1543.199487	15.872653
24.975498	1548.178671	15.877671
25.258473	1543.496472	15.882688
25.367619	1546.168616	15.887706
25.055313	1546.549535	15.892723
25.172902	1547.588399	15.897741
24.978813	1538.153329	15.902759
25.188433	1545.137950	15.907776
25.293719	1550.470565	15.912794
25.082433	1547.643431	15.917811
25.619494	1540.901450	15.922829
25.389782	1540.802947	15.927847
25.396297	1533.820871	15.932864
25.127012	1542.988325	15.937882
25.299210	1548.007892	15.942899
25.155062	1534.642131	15.947917
25.249114	1539.779360	15.952935
25.187423	1532.837319	15.957952
25.758446	1553.071091	15.962970
25.475775	1559.244719	15.967987
25.491050	1560.351313	15.973005
25.895214	1567.177352	15.978023
25.913219	1554.582358	15.983040
25.774029	1544.862210	15.988058
25.896350	1539.051896	15.993075
25.897831	1532.362779	15.998093
25.841311	1531.297019	16.003111
25.498304	1527.180683	16.008128
25.679588	1525.767279	16.013146
25.487476	1535.973125	16.018163
25.848323	1538.605557	16.023181
25.572759	1545.170128	16.028199
25.815249	1561.018174	16.033216
25.934530	1562.363844	16.038234
25.712387	1564.506599	16.043251
25.849774	1556.911899	16.048269
25.934719	1564.049062	16.053287
25.835029	1565.262882	16.058304
26.204826	1560.075358	16.063322
26.100407	1568.771434	16.068339
26.267760	1566.148526	16.073357
26.410711	1566.703271	16.078375
26.156498	1565.466308	16.083392
26.511098	1558.754140	16.088410
25.847270	1565.346003	16.093427
26.226930	1556.692291	16.098445
26.154876	1557.480276	16.103463
25.870881	1556.413599	16.108480
26.132330	1550.870004	16.113498
25.868159	1558.025605	16.118515
25.912136	1552.630225	16.123533
26.133822	1552.813272	16.128551
25.979182	1570.966451	16.133568
26.099662	1585.798509	16.138586
26.145851	1598.731860	16.143603
26.481158	1594.151217	16.148621
26.474194	1601.854009	16.153639
26.072555	1601.760352	16.158656
26.711993	1589.440774	16.163674
26.551953	1592.818523	16.168691
26.741002	1582.831007	16.173709
26.554298	1593.769458	16.178727
26.217675	1595.280388	16.183744
26.772798	1587.322012	16.188762
26.744951	1589.679841	16.193779
26.615869	1582.817835	16.198797
27.116664	1591.177486	16.203815
26.875771	1589.204852	16.208832
26.777797	1597.382554	16.213850
26.526042	1594.971561	16.218867
26.711936	1589.445188	16.223885
27.112813	1592.328088	16.228903
26.965024	1592.446333	16.233920
27.075721	1593.408782	16.238938
27.123574	1597.763523	16.243955
27.234540	1593.534201	16.248973
26.947411	1601.038504	16.253991
26.927573	1600.507216	16.259008
27.183475	1590.299176	16.264026
27.076607	1596.966149	16.269043
26.969443	1592.285940	16.274061
27.225912	1591.740394	16.279079
26.756549	1589.360317	16.284096
27.466012	1587.321259	16.289114
27.219987	1591.530567	16.294131
27.056044	1594.443216	16.299149
27.219720	1592.929966	16.304167
26.768512	1595.882309	16.309184
27.099600	1588.450007	16.314202
27.124283	1608.461721	16.319219
26.885705	1607.765079	16.324237
27.318504	1617.760413	16.329255
27.087786	1614.081759	16.334272
27.260419	1601.866634	16.339290
26.959910	1615.295204	16.344307
27.308735	1609.045388	16.349325
27.569325	1610.547191	16.354343
27.315973	1613.422286	16.359360
27.692726	1615.874145	16.364378
27.735514	1630.453756	16.369395
27.857514	1633.739930	16.374413
27.785092	1611.171664	16.379431
27.502367	1615.827214	16.384448
27.564381	1609.248513	16.389466
27.509831	1635.165901	16.394483
27.641952	1639.377567	16.399501
28.026549	1642.698212	16.404519
27.781091	1649.554692	16.409536
27.889412	1642.319488	16.414554
27.683254	1646.703707	16.419571
27.805584	1644.705565	16.424589
27.776786	1638.938347	16.429607
27.658786	1641.429223	16.434624
27.874637	1638.022680	16.439642
27.543993	1642.906252	16.444659
27.830236	1643.162075	16.449677
27.971466	1632.935201	16.454695
27.822077	1649.186811	16.459712
27.771388	1650.763391	16.464730
27.927127	1667.653473	16.469747
27.924806	1674.696081	16.474765
28.307920	1670.063011	16.479783
28.082381	1677.346521	16.484800
28.283257	1659.325471	16.489818
28.768284	1669.263765	16.494835
28.535853	1667.222002	16.499853
28.753336	1661.980926	16.504871
28.614176	1671.661555	16.509888
28.602865	1658.529991	16.514906
28.471284	1643.653782	16.519923
28.590032	1637.838511	16.524941
28.621359	1624.509363	16.529959
28.594102	1635.537189	16.534976
28.420127	1624.316451	16.539994
28.338354	1625.163528	16.545011
28.111393	1622.804724	16.550029
28.753351	1639.199302	16.555047
28.694192	1652.969436	16.560064
28.823036	1651.626122	16.565082
28.805423	1654.737780	16.570099
28.758774	1646.046736	16.575117
29.016303	1641.667541	16.580135
28.791175	1632.384011	16.585152
28.864067	1624.310193	16.590170
28.600938	1623.822340	16.595187
28.551640	1632.217985	16.600205
28.800372	1647.223746	16.605223
28.753263	1652.940294	16.610240
29.109954	1652.953349	16.615258
28.602746	1657.528760	16.620275
28.743174	1654.894548	16.625293
28.980909	1651.490677	16.630311
28.778871	1657.281700	16.635328
28.937548	1652.823202	16.640346
28.739998	1657.553636	16.645363
28.828209	1658.469813	16.650381
29.220140	1658.334906	16.655399
29.053185	1659.751998	16.660416
29.235490	1668.914433	16.665434
29.290845	1676.888834	16.670451
28.884488	1691.586970	16.675469
29.558884	1696.779335	16.680487
29.509821	1698.759983	16.685504
29.653580	1681.833015	16.690522
29.156721	1668.177117	16.695539
29.399661	1676.337386	16.700557
29.527296	1675.550966	16.705575
29.538085	1684.730393	16.710592
29.382042	1681.728731	16.715610
29.550725	1676.459116	16.720627
29.554672	1687.078661	16.725645
29.459077	1682.402414	16.730663
29.583407	1679.290152	16.735680
29.652398	1680.951248	16.740698
29.753689	1673.529792	16.745715
29.436607	1678.584752	16.750733
29.695155	1679.995561	16.755751
29.560520	1680.586433	16.760768
29.480148	1673.889156	16.765786
29.795142	1676.501252	16.770803
29.480058	1677.254289	16.775821
29.831876	1675.086252	16.780839
29.511541	1675.503936	16.785856
30.169013	1692.314507	16.790874
30.260413	1690.951406	16.795891
29.723381	1689.376616	16.800909
30.017548	1681.458649	16.805927
30.311526	1701.248725	16.810944
30.312062	1693.759691	16.815962
30.209944	1683.662843	16.820979
29.984862	1684.191920	16.825997
30.171549	1679.064993	16.831015
30.030420	1685.987678	16.836032
30.207840	1697.132838	16.841050
30.352131	1701.081480	16.846067
30.097974	1708.996125	16.851085
30.442348	1706.632072	16.856103
30.183681	1711.497053	16.861120
30.054003	1704.257136	16.866138
30.109281	1705.653575	16.871155
30.221314	1709.377244	16.876173
30.385154	1706.025756	16.881191
30.246673	1711.486588	16.886208
30.252422	1708.853408	16.891226
30.261346	1709.062239	16.896243
30.205199	1712.529898	16.901261
31.009120	1726.815847	16.906279
30.718174	1726.382990	16.911296
30.559930	1712.048143	16.916314
30.567925	1708.882698	16.921331
30.578416	1726.484302	16.926349
30.848726	1725.701419	16.931367
30.756086	1738.227557	16.936384
30.797462	1733.905783	16.941402
30.873762	1735.972370	16.946419
30.679927	1736.663993	16.951437
31.064031	1730.538997	16.956455
30.819342	1740.369428	16.961472
30.850403	1737.326536	16.966490
31.055751	1736.129604	16.971507
30.809902	1734.962502	16.976525
31.095023	1727.361760	16.981543
31.117434	1733.918407	16.986560
30.975544	1734.659696	16.991578
31.103101	1726.341339	16.996595
30.848449	1735.324197	17.001613
30.957861	1743.336926	17.006631
30.986307	1730.547539	17.011648
30.939172	1735.982624	17.016666
31.126257	1747.470710	17.021683
30.813101	1759.008961	17.026701
31.350997	1766.014127	17.031719
31.217738	1770.257173	17.036736
31.538039	1761.646249	17.041754
31.832885	1755.573031	17.046771
31.747150	1766.246063	17.051789
31.907853	1761.591527	17.056807
31.800733	1760.664839	17.061824
31.579415	1766.648467	17.066842
31.870028	1744.669899	17.071859
31.409526	1738.729246	17.076877
31.835445	1750.237235	17.081895
31.751585	1752.650034	17.086912
31.741159	1753.161285	17.091930
31.764291	1748.104332	17.096947
31.705985	1760.581889	17.101965
31.958059	1753.951577	17.106983
31.994192	1765.225693	17.112000
31.649014	1758.001750	17.117018
32.170455	1748.175626	17.122035
31.715674	1755.245555	17.127053
31.660471	1760.469777	17.132071
31.891600	1759.111879	17.137088
31.823407	1749.582998	17.142106
31.974848	1751.947385	17.147123
31.721002	1755.241882	17.152141
32.008481	1747.897829	17.157159
31.908020	1743.895997	17.162176
31.993050	1748.997781	17.167194
31.967480	1757.470274	17.172211
32.243144	1784.288359	17.177229
31.940178	1780.701945	17.182247
32.066781	1783.394862	17.187264
32.227854	1794.122321	17.192282
32.586275	1790.249219	17.197299
32.304959	1795.309317	17.202317
32.257738	1792.265204	17.207335
32.468398	1790.673682	17.212352
32.492140	1790.751320	17.217370
32.708703	1778.621697	17.222387
32.261204	1792.512164	17.227405
32.233579	1782.097796	17.232423
32.381781	1784.269021	17.237440
32.327224	1785.963972	17.242458
32.603382	1783.975774	17.247475
32.951509	1802.077860	17.252493
33.204226	1800.853394	17.257511
32.921025	1790.593546	17.262528
32.744734	1789.570829	17.267546
33.056328	1769.922637	17.272563
33.061969	1773.511575	17.277581
33.034157	1772.944593	17.282599
32.891337	1775.730153	17.287616
32.955988	1775.998657	17.292634
33.017869	1772.812071	17.297651
32.950675	1780.899733	17.302669
33.065361	1774.548463	17.307687
32.954810	1772.761310	17.312704
32.704560	1783.678133	17.317722
33.171736	1794.857668	17.322739
32.789353	1809.246429	17.327757
33.219877	1818.567459	17.332775
33.497046	1815.687346	17.337792
33.160793	1828.414921	17.342810
33.020188	1809.351014	17.347827
32.903257	1814.681147	17.352845
33.093055	1814.409236	17.357863
33.547613	1814.098602	17.362880
33.315671	1805.884220	17.367898
33.516560	1805.708112	17.372915
33.719843	1811.788773	17.377933
33.410502	1811.799123	17.382951
33.441099	1817.431997	17.387968
33.540305	1822.738153	17.392986
33.473777	1827.265839	17.398003
33.608935	1840.274030	17.403021
33.686895	1838.233605	17.408039
33.757528	1841.236591	17.413056
33.688762	1840.864186	17.418074
33.846490	1835.618379	17.423091
33.687210	1841.979564	17.428109
33.813990	1839.942077	17.433127
33.905115	1839.318390	17.438144
34.048132	1839.143990	17.443162
34.054053	1831.787070	17.448179
34.033576	1838.600473	17.453197
33.976760	1837.020954	17.458215
33.922197	1836.173355	17.463232
34.129076	1847.010197	17.468250
34.318915	1826.591138	17.473267
34.197274	1835.228796	17.478285
34.118835	1835.801313	17.483303
34.350031	1831.476820	17.488320
34.277842	1836.610572	17.493338
34.572988	1831.684537	17.498355
34.539947	1838.402381	17.503373
34.207043	1834.574450	17.508391
34.396028	1828.523065	17.513408
34.155189	1843.034091	17.518426
34.588057	1826.806742	17.523443
34.327988	1833.785015	17.528461
34.325318	1841.676982	17.533479
34.440196	1844.919497	17.538496
34.340898	1855.096009	17.543514
34.530078	1861.185324	17.548531
34.468164	1865.097286	17.553549
34.439007	1862.741911	17.558567
34.821749	1861.564415	17.563584
34.789595	1859.922934	17.568602
34.932947	1853.185384	17.573619
34.380786	1856.973007	17.578637
34.738085	1855.763897	17.583655
35.233028	1850.068933	17.588672
34.929109	1857.803702	17.593690
34.908330	1859.014714	17.598707
34.998895	1859.559641	17.603725
34.793379	1860.086665	17.608743
34.993433	1858.308307	17.613760
34.923353	1863.434632	17.618778
35.381216	1872.472029	17.623795
35.212969	1867.865238	17.628813
35.182325	1870.313338	17.633831
35.207688	1866.341034	17.638848
35.505704	1873.967083	17.643866
35.349133	1874.946640	17.648883
35.578008	1868.081928	17.653901
35.435904	1851.924564	17.658919
35.471160	1856.557846	17.663936
35.312594	1856.095584	17.668954
35.441311	1870.893873	17.673971
35.755039	1877.991722	17.678989
35.580029	1883.950010	17.684007
35.658162	1873.358616	17.689024
35.466308	1882.201631	17.694042
35.455019	1886.571759	17.699059
35.833433	1885.895379	17.704077
35.547258	1883.642404	17.709095
35.715493	1880.654331	17.714112
35.290691	1887.564628	17.719130
35.473521	1889.883286	17.724147
35.646814	1887.522338	17.729165
35.762364	1886.559952	17.734183
35.886999	1883.310589	17.739200
35.776711	1895.790169	17.744218
35.972075	1908.771520	17.749235
36.262433	1918.119363	17.754253
36.266505	1918.346325	17.759271
36.245237	1911.371436	17.764288
36.222279	1915.566729	17.769306
35.911184	1915.676189	17.774323
36.106497	1908.649297	17.779341
36.220105	1914.136962	17.784359
36.336610	1915.872894	17.789376
36.444858	1920.554740	17.794394
35.923389	1912.268950	17.799411
36.042904	1909.444453	17.804429
36.186932	1913.162086	17.809447
36.374217	1908.094042	17.814464
36.175006	1921.385626	17.819482
36.324636	1924.267672	17.824499
36.740869	1936.760495	17.829517
36.542618	1939.031631	17.834535
36.918368	1947.499192	17.839552
37.037203	1940.603062	17.844570
37.008898	1929.304043	17.849587
36.743247	1918.269535	17.854605
36.381099	1926.860059	17.859623
36.971478	1921.332735	17.864640
36.755430	1928.885662	17.869658
36.878043	1932.528498	17.874675
37.004191	1927.307181	17.879693
36.844327	1937.418578	17.884711
36.874089	1930.607282	17.889728
36.909786	1924.048554	17.894746
36.863589	1934.758068	17.899763
37.137211	1926.419749	17.904781
36.953136	1932.082699	17.909799
37.036960	1928.811344	17.914816
36.923669	1942.012339	17.919834
36.714278	1939.799792	17.924851
36.934446	1949.319122	17.929869
37.164338	1961.961328	17.934887
37.535064	1962.417741	17.939904
37.570801	1964.409972	17.944922
37.246313	1960.575892	17.949939
37.620810	1960.100951	17.954957
37.225123	1965.298548	17.959975
37.530897	1963.410151	17.964992
37.395620	1967.515393	17.970010
38.036447	1961.126533	17.975027
38.023851	1955.997474	17.980045
37.582869	1963.819165	17.985063
37.964693	1958.621645	17.990080
37.832877	1961.308564	17.995098
38.002439	1954.400484	18.000115
38.169742	1953.466534	18.005133
38.289969	1959.768885	18.010151
37.999889	1953.859771	18.015168
37.925548	1956.511581	18.020186
37.557300	1966.048433	18.025203
37.946667	1953.568400	18.030221
37.808075	1961.739239	18.035239
37.809720	1958.627945	18.040256
37.806392	1960.820743	18.045274
37.911918	1956.873726	18.050291
38.120525	1967.651310	18.055309
38.234907	1984.402913	18.060327
38.488282	1986.977627	18.065344
38.346231	1989.228046	18.070362
37.908161	1993.275163	18.075379
38.252185	1985.086576	18.080397
38.371940	1989.553934	18.085415
38.437892	1985.303613	18.090432
38.296806	1988.644449	18.095450
37.858144	1992.629851	18.100467
38.341923	1984.414973	18.105485
38.318293	1993.772334	18.110503
38.962844	2001.514690	18.115520
39.099045	2005.297423	18.120538
38.794909	2008.247929	18.125555
38.953291	2004.568533	18.130573
38.671888	2008.149937	18.135591
39.034779	2002.945300	18.140608
39.315994	2002.241310	18.145626
39.106981	1993.391519	18.150643
38.978995	1977.838000	18.155661
38.735097	1976.248499	18.160679
39.040956	1989.539581	18.165696
39.103482	1995.901897	18.170714
39.140763	2000.974661	18.175731
39.335336	2001.132283	18.180749
39.091994	2013.685566	18.185767
39.424471	2006.416620	18.190784
39.187684	2006.168885	18.195802
39.255617	2012.309834	18.200819
39.270294	1997.424422	18.205837
39.231826	2007.899631	18.210855
39.214675	2007.122208	18.215872
39.072123	2002.159932	18.220890
39.579149	2004.323741	18.225907
39.425817	1999.112851	18.230925
39.607893	1998.754813	18.235943
39.288273	1992.960421	18.240960
39.920592	2007.445130	18.245978
39.369011	2020.214422	18.250995
39.752867	2024.699478	18.256013
39.775627	2027.858857	18.261031
39.741053	2024.462989	18.266048
40.081533	2029.941475	18.271066
39.781983	2037.419696	18.276083
40.182575	2029.622124	18.281101
39.987675	2034.142385	18.286119
39.832907	2030.789253	18.291136
40.237259	2022.714282	18.296154
39.857499	2032.149928	18.301171
40.063197	2024.699599	18.306189
39.897718	2029.922092	18.311207
40.225858	2022.211719	18.316224
40.215925	2032.497963	18.321242
40.067675	2035.211632	18.326259
40.327220	2024.296388	18.331277
40.312845	2031.109258	18.336295
40.278729	2025.106550	18.341312
40.262958	2026.381708	18.346330
40.021246	2031.361307	18.351347
40.331413	2040.361841	18.356365
40.646753	2042.480623	18.361383
40.656896	2051.683603	18.366400
40.974696	2049.439651	18.371418
40.893503	2056.731720	18.376435
41.078935	2048.421325	18.381453
40.667846	2042.824349	18.386471
40.698200	2045.319464	18.391488
40.875554	2055.626681	18.396506
40.659031	2064.530184	18.401523
40.796768	2058.334041	18.406541
40.821424	2056.709118	18.411559
40.743712	2064.785283	18.416576
40.822533	2050.285668	18.421594
40.866201	2059.074034	18.426611
41.127632	2046.896221	18.431629
40.858317	2051.608342	18.436647
40.687832	2053.572525	18.441664
41.042123	2066.826520	18.446682
41.279225	2082.902377	18.451699
41.337075	2085.509091	18.456717
41.290276	2081.503011	18.461735
41.764294	2082.033272	18.466752
41.769226	2066.289146	18.471770
41.446565	2080.081635	18.476787
41.440128	2076.781493	18.481805
41.521242	2075.706685	18.486823
41.411534	2079.329755	18.491840
41.612207	2062.277199	18.496858
41.672338	2074.182624	18.501875
41.746939	2081.700489	18.506893
41.756272	2073.638145	18.511911
41.689005	2072.583969	18.516928
41.949859	2075.313370	18.521946
41.976170	2079.151326	18.526963
41.936845	2073.387265	18.531981
41.553684	2081.273458	18.536999
41.852168	2085.659279	18.542016
41.993378	2095.885890	18.547034
42.311097	2107.797508	18.552051
42.599534	2096.476236	18.557069
42.550408	2096.952567	18.562087
42.167886	2089.520078	18.567104
42.369333	2069.700765	18.572122
42.081281	2076.970796	18.577139
42.329000	2085.891537	18.582157
42.733786	2093.429933	18.587175
42.389905	2094.730292	18.592192
42.719657	2092.237104	18.597210
42.092350	2103.343754	18.602227
42.456776	2101.883045	18.607245
42.567502	2099.627310	18.612263
42.540881	2089.283438	18.617280
42.651104	2095.442221	18.622298
42.525386	2101.319592	18.627315
42.391949	2090.515438	18.632333
42.360599	2100.088714	18.637351
42.545148	2102.366174	18.642368
42.779951	2092.593204	18.647386
42.736911	2108.719413	18.652403
42.738076	2117.497527	18.657421
42.817892	2125.405902	18.662439
42.677076	2130.882228	18.667456
42.948600	2136.259568	18.672474
42.898631	2129.722813	18.677491
42.883401	2127.627306	18.682509
42.995237	2121.457475	18.687527
42.761022	2129.741878	18.692544
42.993855	2138.577709	18.697562
43.211559	2153.119004	18.702579
43.129830	2156.119721	18.707597
43.452299	2154.141920	18.712615
43.388797	2157.267970	18.717632
43.619983	2159.991275	18.722650
43.575374	2160.001096	18.727667
43.578508	2153.358684	18.732685
43.858355	2151.548970	18.737703
43.629205	2155.982021	18.742720
43.288592	2149.458737	18.747738
43.400542	2163.206107	18.752755
43.778390	2173.300275	18.757773
43.624551	2179.694162	18.762791
43.807419	2177.824123	18.767808
44.447519	2168.427711	18.772826
44.059036	2178.947605	18.777843
44.091580	2183.866090	18.782861
44.263037	2178.241110	18.787879
44.135580	2180.693478	18.792896
44.222095	2177.815340	18.797914
44.400989	2179.735467	18.802931
44.352909	2175.756742	18.807949
44.319137	2176.244706	18.812967
44.300372	2177.912119	18.817984
44.183186	2178.194203	18.823002
44.614397	2180.459966	18.828019
44.245313	2174.980006	18.833037
44.496973	2171.237486	18.838055
44.459386	2175.912848	18.843072
44.568210	2172.075865	18.848090
44.676932	2178.599509	18.853107
44.463869	2173.323645	18.858125
44.583430	2176.178433	18.863143
44.776343	2168.975830	18.868160
44.977426	2182.237575	18.873178
44.675265	2189.513931	18.878195
44.560542	2202.964212	18.883213
44.849729	2201.673439	18.888231
44.858556	2198.841233	18.893248
44.882353	2201.387855	18.898266
45.067878	2203.465948	18.903283
44.973504	2199.158648	18.908301
45.048309	2206.370230	18.913319
44.747086	2207.441478	18.918336
44.577141	2214.003800	18.923354
45.128650	2225.003534	18.928371
45.331647	2238.236663	18.933389
45.259899	2227.389127	18.938407
45.263706	2231.206043	18.943424
45.348295	2230.609014	18.948442
45.636783	2231.654273	18.953459
45.481867	2226.604599	18.958477
45.684219	2232.523369	18.963495
45.274076	2235.680060	18.968512
45.501713	2233.901031	18.973530
45.671432	2230.912252	18.978547
45.565914	2248.909261	18.983565
45.946859	2255.913474	18.988583
46.119191	2260.124950	18.993600
46.077130	2261.374952	18.998618
46.211228	2254.960428	19.003635
45.990221	2245.137242	19.008653
46.284426	2234.333440	19.013671
45.975479	2242.959423	19.018688
46.207216	2241.985258	19.023706
46.070137	2251.041467	19.028723
46.194815	2248.058175	19.033741
46.305264	2252.922835	19.038759
46.240517	2254.106511	19.043776
46.192642	2249.495817	19.048794
46.679314	2259.891326	19.053811
46.781927	2258.453482	19.058829
46.895931	2244.220707	19.063847
46.367817	2251.374263	19.068864
46.361392	2252.519146	19.073882
46.526262	2252.732479	19.078899
46.604843	2241.149776	19.083917
46.683771	2249.768232	19.088935
46.549169	2253.797056	19.093952
46.540933	2244.292590	19.098970
46.782792	2243.607312	19.103987
46.737806	2269.377711	19.109005
47.196556	2271.380255	19.114023
47.068595	2281.928343	19.119040
47.231325	2281.239630	19.124058
47.232907	2282.369410	19.129075
46.647540	2286.026405	19.134093
47.285275	2276.404327	19.139111
47.299363	2285.690261	19.144128
47.180967	2267.077252	19.149146
47.490595	2276.274872	19.154163
47.319227	2273.828411	19.159181
47.293207	2269.586548	19.164199
47.027028	2278.459811	19.169216
47.424782	2282.320567	19.174234
47.610174	2271.530426	19.179251
47.458998	2272.609906	19.184269
47.564217	2286.356138	19.189287
47.500379	2292.539096	19.194304
47.790021	2302.683783	19.199322
47.591158	2305.861805	19.204339
47.633370	2306.974228	19.209357
48.103354	2296.424361	19.214375
48.132867	2307.531455	19.219392
48.081132	2294.419040	19.224410
47.888392	2295.334530	19.229427
47.755486	2304.127076	19.234445
47.984452	2295.555393	19.239463
48.218411	2301.102404	19.244480
48.333061	2298.010127	19.249498
48.188105	2298.272007	19.254515
48.104954	2308.525673	19.259533
48.388389	2320.742358	19.264551
48.424183	2322.651157	19.269568
48.296477	2323.563360	19.274586
48.514900	2328.416072	19.279603
48.258422	2329.604334	19.284621
48.484744	2333.011972	19.289639
48.282312	2325.972009	19.294656
48.698663	2327.807952	19.299674
48.696530	2324.363337	19.304691
48.576188	2324.002609	19.309709
48.903624	2325.036702	19.314727
48.506764	2325.274936	19.319744
48.883677	2347.327406	19.324762
48.927456	2346.066626	19.329779
49.101469	2356.345460	19.334797
49.389279	2352.051216	19.339815
49.212828	2355.070411	19.344832
49.151855	2348.301517	19.349850
49.701246	2349.779197	19.354867
49.345078	2352.454510	19.359885
49.467970	2348.992338	19.364903
49.246010	2353.999871	19.369920
49.457430	2361.494430	19.374938
49.695494	2342.329763	19.379955
49.378614	2350.211415	19.384973
49.480379	2347.190163	19.389991
49.677704	2351.485325	19.395008
49.626634	2346.612914	19.400026
49.869653	2358.207551	19.405043
49.611986	2353.221702	19.410061
49.955301	2336.577531	19.415079
49.844554	2347.825601	19.420096
49.845393	2349.763421	19.425114
50.040901	2345.333274	19.430131
49.593456	2350.145061	19.435149
49.683866	2332.759270	19.440167
49.793580	2347.988345	19.445184
49.836465	2366.577482	19.450202
50.278047	2368.775411	19.455219
50.421200	2371.924375	19.460237
50.226717	2371.012903	19.465255
50.099635	2368.744536	19.470272
50.111741	2380.077804	19.475290
50.638784	2366.950205	19.480307
50.328321	2374.672924	19.485325
50.155708	2378.572241	19.490343
49.965898	2383.016952	19.495360
50.564126	2382.570312	19.500378
50.882548	2386.106419	19.505395
50.761983	2395.329277	19.510413
50.883654	2394.037091	19.515431
50.885702	2402.751831	19.520448
50.691665	2403.714788	19.525466
51.007337	2395.794475	19.530483
50.869518	2401.183386	19.535501
50.912774	2397.846600	19.540519
50.951833	2393.214775	19.545536
51.049748	2394.433341	19.550554
51.073812	2404.548444	19.555571
51.130753	2420.335962	19.560589
50.981674	2426.842947	19.565607
51.335744	2419.098951	19.570624
51.312566	2420.434820	19.575642
51.514827	2418.213492	19.580659
51.459258	2420.156723	19.585677
51.531843	2417.024536	19.590695
51.418611	2417.048869	19.595712
51.365335	2425.402685	19.600730
51.909321	2426.151702	19.605747
51.896701	2421.057535	19.610765
51.600819	2420.715241	19.615783
51.925348	2432.220842	19.620800
52.067596	2445.991794	19.625818
52.209307	2444.949842	19.630835
52.303321	2431.353311	19.635853
52.140799	2418.684749	19.640871
51.972619	2415.226268	19.645888
51.965412	2432.223301	19.650906
52.246320	2437.437373	19.655923
52.166819	2445.666401	19.660941
52.265657	2440.384866	19.665959
52.381950	2442.778408	19.670976
52.155624	2444.829449	19.675994
52.381783	2448.173750	19.681011
52.212421	2444.273702	19.686029
52.090101	2447.543809	19.691047
52.263653	2459.164592	19.696064
52.147740	2463.888838	19.701082
52.715458	2472.370574	19.706099
52.677128	2483.908342	19.711117
52.710971	2478.889538	19.716135
52.962638	2476.432056	19.721152
52.714041	2478.103303	19.726170
52.756086	2475.645096	19.731187
52.811360	2479.290943	19.736205
52.997958	2483.902502	19.741223
53.316335	2489.109207	19.746240
52.650126	2496.916090	19.751258
53.463065	2494.515283	19.756275
53.490137	2496.565319	19.761293
53.333039	2495.766160	19.766311
53.407075	2497.771804	19.771328
53.653467	2501.074969	19.776346
53.679877	2486.272192	19.781363
53.720378	2490.616984	19.786381
53.654723	2490.302318	19.791399
53.656931	2488.570430	19.796416
53.440194	2493.309412	19.801434
53.724802	2493.558831	19.806451
53.858898	2493.215420	19.811469
54.043937	2495.088504	19.816487
53.893242	2490.645559	19.821504
53.469361	2500.236831	19.826522
53.844199	2501.852491	19.831539
54.021764	2522.702715	19.836557
53.997286	2515.804469	19.841575
54.402418	2519.034894	19.846592
54.409489	2528.112673	19.851610
54.540336	2510.688096	19.856627
54.176579	2515.919172	19.861645
54.096921	2522.788345	19.866663
54.480671	2519.514057	19.871680
54.362537	2518.989957	19.876698
54.239991	2516.221969	19.881715
54.524794	2524.150151	19.886733
54.578660	2535.669542	19.891751
54.916842	2546.270552	19.896768
55.026929	2551.691699	19.901786
55.140151	2545.985673	19.906803
55.119329	2549.172455	19.911821
55.144346	2544.133436	19.916839
55.382655	2524.610217	19.921856
55.268912	2515.837665	19.926874
55.057209	2508.163684	19.931891
55.470701	2515.952042	19.936909
55.343901	2508.786080	19.941927
55.375372	2504.492112	19.946944
55.282113	2511.560394	19.951962
55.097287	2521.518418	19.956979
55.156216	2539.079847	19.961997
55.296125	2538.221270	19.967015
55.551092	2537.465695	19.972032
55.366506	2541.002446	19.977050
55.887830	2543.261611	19.982067
55.910369	2541.019628	19.987085
55.547664	2538.593389	19.992103
55.423976	2533.408514	19.997120
55.250918	2542.757087	20.002138
55.200207	2555.195832	20.007155
55.778661	2572.300779	20.012173
55.520758	2570.209172	20.017191
55.800639	2567.740704	20.022208
55.382056	2579.182835	20.027226
55.751930	2586.413456	20.032243
55.945053	2595.174228	20.037261
55.968304	2594.085736	20.042279
56.537212	2599.828590	20.047296
56.180230	2601.802854	20.052314
56.296490	2598.510239	20.057331
56.268218	2614.579010	20.062349
56.149166	2627.243315	20.067367
56.704980	2623.487730	20.072384
56.751468	2627.692583	20.077402
56.854553	2626.823168	20.082419
56.956422	2627.478463	20.087437
56.882348	2627.480957	20.092455
57.024828	2624.323375	20.097472
56.826692	2622.876237	20.102490
56.801048	2626.033909	20.107507
56.959861	2634.165305	20.112525
56.592563	2633.909638	20.117543
57.273135	2641.075058	20.122560
57.089280	2662.316437	20.127578
57.218524	2655.615526	20.132595
57.423379	2652.662584	20.137613
57.684975	2655.580562	20.142631
57.763915	2646.650433	20.147648
57.330990	2650.159032	20.152666
57.763827	2652.562402	20.157683
57.650043	2641.298281	20.162701
57.810940	2640.851605	20.167719
58.049470	2644.597471	20.172736
57.898432	2648.002697	20.177754
57.844081	2644.909594	20.182771
58.001889	2638.299242	20.187789
57.438784	2638.146869	20.192807
57.968938	2664.347919	20.197824
58.030849	2671.971327	20.202842
58.069041	2675.990547	20.207859
58.345035	2676.865060	20.212877
57.789508	2686.276655	20.217895
58.447557	2675.595387	20.222912
58.288432	2683.920014	20.227930
58.108609	2675.450853	20.232947
58.512503	2682.487290	20.237965
58.657668	2694.078695	20.242983
58.764746	2691.625040	20.248000
58.756185	2698.557721	20.253018
58.802265	2697.959570	20.258035
59.125716	2690.392176	20.263053
59.005896	2692.737446	20.268071
59.418575	2681.364075	20.273088
59.310822	2688.704541	20.278106
59.589395	2685.038157	20.283123
59.556077	2671.440059	20.288141
59.369293	2665.224965	20.293159
59.467704	2652.626007	20.298176
59.449563	2653.344878	20.303194
59.166574	2654.493062	20.308211
59.119706	2646.757859	20.313229
59.057881	2654.348988	20.318247
59.410655	2664.857893	20.323264
59.311446	2684.765120	20.328282
59.249442	2684.656159	20.333299
59.544805	2695.730141	20.338317
59.422357	2701.737914	20.343335
59.623788	2687.393795	20.348352
59.805114	2690.119152	20.353370
59.448323	2698.171376	20.358387
59.747448	2708.011588	20.363405
59.818959	2728.196922	20.368423
60.120169	2722.441987	20.373440
59.991546	2724.091819	20.378458
60.016171	2728.896032	20.383475
60.242597	2715.267879	20.388493
59.844357	2729.037625	20.393511
60.000067	2733.901635	20.398528
60.155347	2744.199971	20.403546
60.425593	2753.471723	20.408563
60.697754	2752.826292	20.413581
60.437555	2750.055069	20.418599
60.891159	2756.723834	20.423616
60.702289	2750.478341	20.428634
60.701179	2745.163249	20.433651
61.090699	2747.200157	20.438669
60.676299	2741.762147	20.443687
61.084730	2742.570244	20.448704
60.947122	2757.194955	20.453722
61.144519	2770.014079	20.458739
61.442418	2759.392389	20.463757
61.724033	2776.315594	20.468775
61.810594	2758.392524	20.473792
61.835364	2746.393915	20.478810
61.385723	2738.221384	20.483827
61.544346	2731.021052	20.488845
61.562913	2739.262738	20.493863
61.909005	2728.652381	20.498880
61.825180	2735.453829	20.503898
61.401079	2732.910550	20.508915
61.711189	2736.318184	20.513933
61.773620	2752.403183	20.518951
61.892765	2764.198570	20.523968
61.808279	2768.812184	20.528986
61.886496	2761.618065	20.534003
62.023262	2771.589145	20.539021
62.035495	2770.932418	20.544039
62.343848	2767.754428	20.549056
62.066921	2770.234787	20.554074
62.138313	2759.669894	20.559091
62.260071	2766.229425	20.564109
62.120083	2786.372684	20.569127
62.364139	2783.349443	20.574144
62.451362	2794.081554	20.579162
62.367696	2791.711440	20.584179
62.602890	2795.100781	20.589197
62.277958	2796.967392	20.594215
62.659156	2808.429241	20.599232
62.460980	2811.178084	20.604250
62.698971	2816.069838	20.609267
63.058812	2815.246095	20.614285
62.687032	2820.166764	20.619303
63.210375	2812.385491	20.624320
62.933161	2815.616355	20.629338
62.954286	2833.058775	20.634355
63.334092	2844.082264	20.639373
63.192469	2851.392978	20.644391
63.443153	2841.518873	20.649408
63.551152	2844.052445	20.654426
63.353500	2841.542130	20.659443
63.542192	2839.809249	20.664461
64.012080	2844.140920	20.669479
63.897433	2844.063117	20.674496
63.818299	2843.437265	20.679514
63.313187	2835.111649	20.684531
63.608489	2833.534752	20.689549
63.705980	2851.989432	20.694567
63.814380	2862.527517	20.699584
64.108597	2866.102785	20.704602
64.175106	2866.764339	20.709619
64.455979	2859.624421	20.714637
64.571349	2853.862412	20.719655
64.554442	2858.770005	20.724672
64.825413	2848.775598	20.729690
64.842012	2859.682059	20.734707
64.944436	2850.573107	20.739725
64.657608	2855.929756	20.744743
64.703845	2852.864054	20.749760
64.907298	2853.006830	20.754778
64.792546	2857.552248	20.759795
64.955869	2850.568817	20.764813
65.190980	2861.104819	20.769831
64.888776	2851.489591	20.774848
65.077876	2854.881853	20.779866
64.766093	2864.882378	20.784883
65.219205	2856.686694	20.789901
65.218889	2870.580454	20.794919
65.391360	2871.423298	20.799936
65.544661	2886.003505	20.804954
65.376345	2882.411860	20.809971
65.197429	2884.038931	20.814989
65.316026	2883.273241	20.820007
65.422045	2877.967533	20.825024
65.651008	2879.321538	20.830042
65.420876	2884.880244	20.835059
65.910384	2903.501590	20.840077
65.653588	2910.870775	20.845095
65.952211	2915.748978	20.850112
66.318494	2907.725926	20.855130
66.321381	2906.559674	20.860147
66.347071	2907.200822	20.865165
66.309289	2912.482786	20.870183
66.163124	2915.510854	20.875200
66.226189	2904.807073	20.880218
65.955156	2917.801134	20.885235
66.551328	2909.393136	20.890253
66.500774	2929.244582	20.895271
66.549186	2927.348289	20.900288
66.619335	2932.699798	20.905306
66.538700	2933.389263	20.910323
67.060977	2932.024401	20.915341
67.332555	2934.192685	20.920359
67.002870	2929.533561	20.925376
67.209671	2934.492727	20.930394
66.928014	2923.398336	20.935411
67.227535	2923.410630	20.940429
67.275900	2921.268262	20.945447
66.904607	2926.074700	20.950464
67.300456	2932.256212	20.955482
66.987550	2949.693436	20.960499
67.229668	2956.632759	20.965517
67.708236	2951.973667	20.970535
67.691300	2951.821806	20.975552
67.957442	2951.384863	20.980570
67.760714	2956.076178	20.985587
67.949151	2952.185661	20.990605
67.993755	2958.611579	20.995623
67.968198	2960.679053	21.000640
68.337710	2948.727940	21.005658
67.843899	2961.528196	21.010675
68.073306	2951.691406	21.015693
68.220568	2956.930540	21.020711
68.113458	2972.536708	21.025728
68.178792	2981.358232	21.030746
68.126823	2988.044662	21.035763
68.264147	2982.507730	21.040781
67.986041	2981.337602	21.045799
68.318782	2981.727106	21.050816
68.891206	2998.789819	21.055834
68.683272	3008.021599	21.060851
68.892993	3009.517004	21.065869
68.773235	3008.248994	21.070887
69.041154	3005.120570	21.075904
69.100363	3006.002256	21.080922
69.235250	3008.623931	21.085939
69.244870	3006.187153	21.090957
69.401140	3005.113618	21.095975
69.205245	3006.945499	21.100992
69.363731	2998.050034	21.106010
69.176614	3008.268612	21.111027
69.312522	3008.705670	21.116045
69.585660	3024.779292	21.121063
69.400289	3030.439309	21.126080
69.786890	3031.506573	21.131098
69.616896	3036.191123	21.136115
70.045074	3034.222486	21.141133
70.229893	3036.454761	21.146151
69.924151	3028.677972	21.151168
69.915785	3032.762084	21.156186
69.898506	3030.259671	21.161203
69.762715	3038.931442	21.166221
70.130875	3057.099793	21.171239
70.128327	3063.212272	21.176256
70.317879	3054.766397	21.181274
70.258562	3068.118870	21.186291
70.110792	3058.903966	21.191309
70.386222	3070.868607	21.196327
70.425126	3085.931765	21.201344
70.831999	3082.759844	21.206362
70.749378	3086.134543	21.211379
70.917714	3084.322321	21.216397
70.904317	3085.186110	21.221415
70.938323	3093.318724	21.226432
71.025430	3094.348961	21.231450
71.241829	3112.838202	21.236467
71.007161	3116.327069	21.241485
71.422353	3113.627432	21.246503
71.289041	3115.353285	21.251520
71.446536	3109.555463	21.256538
71.457093	3118.773967	21.261555
71.720753	3112.858162	21.266573
71.822467	3116.950450	21.271591
71.462656	3112.955377	21.276608
71.615812	3119.792563	21.281626
71.950150	3133.718949	21.286643
72.044841	3133.782090	21.291661
72.216463	3135.603532	21.296679
72.333741	3141.947801	21.301696
72.242297	3138.916652	21.306714
72.388952	3144.760733	21.311731
72.292586	3139.301421	21.316749
72.261638	3140.924886	21.321767
72.221286	3151.055863	21.326784
72.268344	3142.922146	21.331802
72.514745	3144.341012	21.336819
72.656560	3169.319686	21.341837
72.764949	3161.705385	21.346855
72.575179	3179.126018	21.351872
72.775498	3172.231604	21.356890
72.701530	3171.424156	21.361907
73.191856	3175.126096	21.366925
73.070097	3160.621257	21.371943
73.243269	3162.008150	21.376960
73.317689	3155.153883	21.381978
73.366203	3173.197719	21.386995
73.395111	3161.948181	21.392013
73.800395	3154.177233	21.397031
73.616407	3165.387620	21.402048
73.605199	3165.805731	21.407066
73.802672	3179.488652	21.412083
73.710386	3185.705810	21.417101
73.953536	3183.123633	21.422119
73.991168	3186.402057	21.427136
74.311457	3185.265522	21.432154
73.997275	3182.928792	21.437171
73.905561	3189.235630	21.442189
73.966824	3182.861136	21.447207
74.072382	3188.147414	21.452224
74.079477	3189.856327	21.457242
74.156691	3201.092788	21.462259
74.173200	3220.110580	21.467277
74.430239	3222.956579	21.472295
74.048977	3229.129861	21.477312
74.828687	3218.868680	21.482330
74.595566	3226.066359	21.487347
74.816707	3230.681084	21.492365
74.947449	3239.271034	21.497383
74.715851	3249.582577	21.502400
75.175255	3244.650560	21.507418
75.335800	3242.210805	21.512435
75.269160	3247.522466	21.517453
75.113850	3236.647114	21.522471
75.505906	3243.503465	21.527488
75.823399	3237.995279	21.532506
75.965894	3237.710706	21.537523
75.961678	3233.274400	21.542541
76.355368	3232.873030	21.547559
75.709924	3230.767538	21.552576
75.998738	3220.555351	21.557594
75.949830	3218.134137	21.562611
75.910402	3226.545936	21.567629
76.028597	3227.677344	21.572647
76.053199	3247.828987	21.577664
76.011586	3262.420951	21.582682
75.736900	3261.471124	21.587699
75.588559	3266.188774	21.592717
76.395788	3265.272033	21.597735
76.450239	3286.442121	21.602752
76.510437	3281.045033	21.607770
76.928519	3280.684904	21.612787
76.750185	3284.599960	21.617805
77.007440	3286.487171	21.622823
76.963399	3291.361988	21.627840
77.015327	3275.532868	21.632858
77.251264	3284.842512	21.637875
77.047762	3281.284555	21.642893
77.383139	3281.693319	21.647911
77.325823	3285.154826	21.652928
77.088261	3289.188757	21.657946
77.551218	3293.235846	21.662963
77.417248	3304.083681	21.667981
77.863768	3312.943074	21.672999
77.800596	3327.509531	21.678016
77.782937	3313.142055	21.683034
77.935610	3320.720829	21.688051
77.763317	3324.569926	21.693069
78.118045	3310.970805	21.698087
78.138347	3316.906747	21.703104
78.139076	3308.965674	21.708122
78.040733	3311.917782	21.713139
78.048582	3317.266745	21.718157
78.276114	3306.783516	21.723175
77.893850	3320.841322	21.728192
78.094097	3333.837230	21.733210
78.577263	3340.597821	21.738227
78.339825	3341.890496	21.743245
78.457657	3335.759357	21.748263
78.450557	3344.463537	21.753280
78.499703	3359.161443	21.758298
79.007927	3372.449735	21.763315
78.781038	3376.574450	21.768333
79.063913	3371.859834	21.773351
79.036140	3377.601374	21.778368
79.141415	3374.710461	21.783386
79.025803	3377.036629	21.788403
79.117875	3394.628577	21.793421
79.563886	3394.699304	21.798439
79.310767	3408.425534	21.803456
79.650933	3398.077549	21.808474
79.683733	3400.386628	21.813491
79.390059	3420.702623	21.818509
79.830069	3423.328184	21.823527
79.983736	3431.317525	21.828544
80.222625	3424.201234	21.833562
80.349492	3422.563577	21.838579
79.772720	3429.289447	21.843597
80.393579	3418.155911	21.848615
80.312973	3421.023203	21.853632
80.378320	3444.504173	21.858650
80.875491	3442.333885	21.863667
80.898025	3448.397474	21.868685
81.038239	3443.760795	21.873703
81.100546	3438.837770	21.878720
81.169463	3440.643966	21.883738
81.255665	3440.660477	21.888755
81.382804	3440.524524	21.893773
81.341137	3430.799255	21.898791
81.300706	3438.494715	21.903808
81.378458	3435.208301	21.908826
81.595916	3436.008685	21.913843
81.322708	3431.688917	21.918861
81.899574	3435.073408	21.923879
81.669600	3439.879832	21.928896
81.459921	3428.290429	21.933914
81.591776	3431.853733	21.938931
81.359230	3441.355227	21.943949
81.217688	3450.594385	21.948967
81.732828	3461.866804	21.953984
82.204210	3459.388542	21.959002
82.273750	3454.669850	21.964019
81.785884	3452.980807	21.969037
81.962392	3477.553001	21.974055
82.367154	3476.824558	21.979072
82.569378	3478.540961	21.984090
82.862026	3487.415302	21.989107
82.700035	3484.579253	21.994125
83.275358	3477.551345	21.999143
83.287820	3476.549627	22.004160
82.867952	3484.574503	22.009178
83.147428	3485.020485	22.014195
82.950139	3483.358138	22.019213
83.233169	3481.450100	22.024231
83.449538	3480.395327	22.029248
82.850645	3476.926811	22.034266
83.321361	3470.357618	22.039283
82.979906	3483.166144	22.044301
83.223692	3493.992907	22.049319
83.934275	3511.508169	22.054336
83.701027	3514.414140	22.059354
83.917872	3507.217199	22.064371
83.576842	3507.896648	22.069389
83.752779	3508.141638	22.074407
84.160961	3501.280781	22.079424
84.368817	3505.949763	22.084442
84.517778	3497.153635	22.089459
84.395510	3501.266967	22.094477
84.555196	3507.317714	22.099495
84.521800	3511.370264	22.104512
84.529219	3532.841422	22.109530
84.801475	3521.904920	22.114547
84.897505	3528.402095	22.119565
84.601912	3532.635877	22.124583
84.734969	3533.265966	22.129600
84.507038	3533.375440	22.134618
84.720728	3538.934127	22.139635
84.972984	3553.835623	22.144653
85.108612	3561.095643	22.149671
85.272069	3559.201881	22.154688
85.008229	3559.020020	22.159706
85.117573	3560.334437	22.164723
85.563154	3574.796412	22.169741
85.630494	3586.330491	22.174759
85.873658	3580.403731	22.179776
85.532686	3584.658427	22.184794
85.883995	3583.598630	22.189811
86.255703	3579.063363	22.194829
86.054424	3582.005790	22.199847
86.217970	3583.646316	22.204864
86.269850	3574.112581	22.209882
86.579125	3569.445117	22.214899
86.648572	3581.137131	22.219917
86.865305	3590.222157	22.224935
86.812290	3592.903393	22.229952
86.733337	3593.898552	22.234970
87.106145	3600.936225	22.239987
86.802313	3598.031502	22.245005
86.878540	3605.988867	22.250023
87.064054	3592.845529	22.255040
87.021982	3598.242622	22.260058
87.438287	3598.700603	22.265075
87.360920	3602.554525	22.270093
87.099428	3598.172133	22.275111
87.551534	3593.983832	22.280128
87.492161	3608.529446	22.285146
87.612974	3611.767806	22.290163
87.593233	3627.504667	22.295181
87.752446	3626.622361	22.300199
88.238176	3621.884715	22.305216
87.923038	3630.844415	22.310234
87.746877	3621.084202	22.315251
87.959110	3626.942413	22.320269
88.231908	3641.666554	22.325287
88.373288	3647.551073	22.330304
88.387756	3651.644559	22.335322
88.333510	3659.379034	22.340339
88.223855	3656.974897	22.345357
88.222956	3656.921961	22.350375
88.387262	3664.430857	22.355392
88.567525	3686.037014	22.360410
89.056495	3678.468517	22.365427
88.764336	3687.535483	22.370445
88.761938	3690.549345	22.375463
89.028406	3679.781431	22.380480
88.936262	3702.676186	22.385498
89.222320	3703.051785	22.390515
89.422172	3707.898161	22.395533
89.619617	3713.998650	22.400551
89.797247	3705.308697	22.405568
89.494929	3709.671609	22.410586
89.927665	3702.308108	22.415603
89.860006	3709.153370	22.420621
89.628641	3696.594786	22.425639
90.063645	3721.996335	22.430656
90.156960	3721.449388	22.435674
90.232705	3724.876754	22.440691
90.320554	3729.262483	22.445709
90.172662	3732.164598	22.450727
90.617304	3718.883355	22.455744
90.402014	3726.780372	22.460762
90.511527	3741.402098	22.465779
90.780661	3758.493026	22.470797
90.747164	3765.568910	22.475815
91.032430	3762.205544	22.480832
91.053916	3767.148803	22.485850
91.014079	3759.907228	22.490867
91.157359	3763.873890	22.495885
90.995237	3776.694306	22.500903
91.828821	3780.611646	22.505920
91.544267	3785.165364	22.510938
91.621571	3789.900543	22.515955
91.812035	3779.629858	22.520973
91.892511	3788.489493	22.525991
91.894127	3780.478734	22.531008
91.773613	3783.679517	22.536026
92.106298	3797.462657	22.541043
92.330063	3804.675515	22.546061
92.123639	3809.821508	22.551079
92.263892	3807.849658	22.556096
92.115017	3817.182778	22.561114
92.143432	3810.191727	22.566131
92.404167	3813.858993	22.571149
92.515693	3843.931093	22.576167
92.828464	3836.854754	22.581184
92.625833	3851.881465	22.586202
92.788744	3843.809710	22.591219
92.843077	3852.250815	22.596237
93.333726	3856.189911	22.601255
93.767125	3864.583222	22.606272
93.642362	3869.595617	22.611290
93.816353	3866.584166	22.616307
94.015731	3855.411039	22.621325
94.025863	3863.364122	22.626343
94.133932	3860.400206	22.631360
93.994216	3859.520919	22.636378
93.981621	3866.025195	22.641395
94.353170	3853.622995	22.646413
93.762922	3861.875512	22.651431
94.341868	3862.014012	22.656448
94.157484	3855.770875	22.661466
94.251816	3853.047852	22.666483
94.537688	3850.529765	22.671501
94.245565	3862.399195	22.676519
94.510404	3867.667995	22.681536
94.513597	3885.176377	22.686554
94.503011	3884.490306	22.691571
94.576958	3882.510525	22.696589
94.659857	3902.852995	22.701607
94.797004	3913.404355	22.706624
94.632872	3913.795436	22.711642
95.016303	3915.608676	22.716659
95.331238	3927.906462	22.721677
95.381231	3948.028027	22.726695
95.473076	3940.941757	22.731712
95.487972	3944.387121	22.736730
95.569529	3935.024263	22.741747
95.969999	3936.382650	22.746765
95.703216	3937.603447	22.751783
96.144707	3961.973450	22.756800
96.080543	3973.088970	22.761818
96.126015	3971.354480	22.766835
96.403500	3975.966793	22.771853
96.486249	3966.713973	22.776871
96.522568	3968.481527	22.781888
96.478322	3972.065843	22.786906
96.629745	3962.106274	22.791923
97.080788	3976.951241	22.796941
96.979947	3987.340450	22.801959
97.457676	3993.171772	22.806976
97.436106	3988.394372	22.811994
97.230794	3980.520937	22.817011
97.288011	3980.289454	22.822029
97.295295	3985.380432	22.827047
97.626828	3984.339635	22.832064
97.459619	3979.818670	22.837082
97.470934	3990.443680	22.842099
97.848782	4000.885944	22.847117
98.133026	4014.241009	22.852135
98.328668	4009.054352	22.857152
98.360636	4018.052091	22.862170
98.074316	4020.320384	22.867187
98.073264	4005.825488	22.872205
98.020684	4011.351648	22.877223
98.280196	4015.609413	22.882240
98.410735	4030.915435	22.887258
98.357518	4031.186563	22.892275
98.549335	4038.174862	22.897293
98.370482	4048.742408	22.902311
98.798941	4051.880702	22.907328
98.780938	4062.590943	22.912346
98.662075	4074.447990	22.917363
99.477014	4070.470793	22.922381
99.438956	4092.108933	22.927399
99.575245	4104.287594	22.932416
99.693655	4100.014626	22.937434
99.680545	4098.845028	22.942451
100.438874	4086.230945	22.947469
100.126516	4093.656345	22.952487
100.191024	4092.586513	22.957504
100.193249	4090.989112	22.962522
99.812968	4091.440398	22.967539
100.032793	4083.587086	22.972557
100.005272	4107.123016	22.977575
100.494300	4101.111251	22.982592
100.564566	4118.270938	22.987610
100.434826	4128.264961	22.992627
100.612682	4117.814224	22.997645
100.134604	4127.050042	23.002663
100.713806	4139.115233	23.007680
100.896403	4143.330641	23.012698
101.060491	4147.841288	23.017715
101.200712	4151.191920	23.022733
100.948764	4168.998022	23.027751
101.322134	4172.202164	23.032768
101.767349	4173.887864	23.037786
101.536643	4182.473208	23.042803
102.083456	4169.138050	23.047821
102.179135	4171.080081	23.052839
101.825878	4172.685352	23.057856
102.146246	4164.968921	23.062874
102.266253	4171.198177	23.067891
102.590168	4170.231082	23.072909
102.556390	4178.845246	23.077927
102.595957	4189.090848	23.082944
102.530499	4191.637610	23.087962
102.344956	4204.520923	23.092979
102.934113	4198.164930	23.097997
102.845213	4204.172053	23.103015
103.059806	4198.669546	23.108032
102.892678	4198.642163	23.113050
102.698923	4204.190190	23.118067
102.912733	4211.835665	23.123085
103.280672	4221.840274	23.128103
103.411703	4217.267498	23.133120
103.668185	4223.738002	23.138138
103.369428	4226.495079	23.143155
103.829271	4231.703364	23.148173
103.839270	4255.648334	23.153191
104.040501	4249.179354	23.158208
104.182033	4248.953596	23.163226
104.004965	4256.329896	23.168243
104.164109	4246.644506	23.173261
104.128833	4271.883041	23.178279
104.309505	4282.849562	23.183296
104.613400	4282.555182	23.188314
104.817780	4287.586848	23.193331
105.180737	4284.890153	23.198349
104.934551	4289.490822	23.203367
104.825907	4293.832458	23.208384
104.784433	4305.175205	23.213402
104.970107	4318.293263	23.218419
105.377799	4305.871730	23.223437
105.431636	4311.083473	23.228455
105.502322	4319.955269	23.233472
106.017948	4336.029470	23.238490
105.943030	4351.472202	23.243507
105.968839	4346.997139	23.248525
105.844490	4351.368955	23.253543
106.042125	4347.482086	23.258560
106.077834	4344.274898	23.263578
106.161527	4357.044455	23.268595
106.566216	4356.832615	23.273613
106.141721	4372.737256	23.278631
106.338164	4375.124128	23.283648
106.635759	4365.720520	23.288666
106.539854	4382.179534	23.293683
107.233916	4387.557790	23.298701
107.065608	4404.465114	23.303719
107.325297	4398.268335	23.308736
107.368193	4398.687365	23.313754
107.062883	4402.589855	23.318771
107.583281	4395.971103	23.323789
107.666532	4397.129254	23.328807
107.944857	4406.081700	23.333824
107.880146	4409.089085	23.338842
107.678575	4418.176122	23.343859
108.134408	4410.178829	23.348877
108.291109	4417.119559	23.353895
108.121797	4417.683193	23.358912
108.361481	4404.478230	23.363930
108.287666	4427.339505	23.368947
108.771681	4432.468251	23.373965
108.928829	4443.358451	23.378983
108.614573	4444.703702	23.384000
108.887994	4445.456286	23.389018
108.790285	4438.650040	23.394035
109.261702	4438.944568	23.399053
109.248722	4439.809937	23.404071
109.249714	4436.890419	23.409088
109.413789	4440.954617	23.414106
109.069529	4462.238378	23.419123
109.504300	4460.480331	23.424141
109.464381	4468.349865	23.429159
109.178774	4463.129333	23.434176
109.786268	4485.807797	23.439194
109.531910	4492.092864	23.444211
109.811452	4495.537060	23.449229
110.336325	4500.652764	23.454247
110.716134	4515.503737	23.459264
110.701436	4519.451070	23.464282
110.551197	4530.986036	23.469299
110.803089	4525.924568	23.474317
110.877867	4519.826874	23.479335
111.141126	4526.573599	23.484352
111.129226	4510.330101	23.489370
111.153614	4515.187667	23.494387
111.395826	4513.469372	23.499405
111.502430	4518.166055	23.504423
111.358560	4533.766867	23.509440
111.365751	4543.306116	23.514458
111.516375	4552.600322	23.519475
111.563967	4546.702431	23.524493
111.978804	4549.796618	23.529511
111.764376	4561.451703	23.534528
112.147913	4570.500231	23.539546
111.681122	4575.504506	23.544563
111.929994	4577.574796	23.549581
112.240495	4596.640482	23.554599
112.363525	4608.828031	23.559616
112.568559	4598.687497	23.564634
112.671339	4611.409998	23.569651
112.572175	4621.318941	23.574669
112.905423	4631.601263	23.579687
113.044466	4641.538508	23.584704
113.641049	4635.471720	23.589722
113.100209	4639.739312	23.594739
113.440170	4649.900039	23.599757
113.772584	4660.173855	23.604775
113.832993	4660.855398	23.609792
114.574463	4656.497235	23.614810
113.982984	4665.708825	23.619827
114.259687	4649.541834	23.624845
114.261899	4656.576766	23.629863
113.905975	4659.951374	23.634880
114.330401	4670.057964	23.639898
114.635193	4682.628943	23.644915
114.740756	4690.339828	23.649933
115.025117	4682.189651	23.654951
114.628104	4684.974099	23.659968
114.990319	4674.661007	23.664986
115.166517	4690.511402	23.670003
115.198568	4706.247069	23.675021
115.279393	4717.467482	23.680039
115.378558	4717.807111	23.685056
115.756060	4708.260123	23.690074
115.479347	4720.172143	23.695091
115.725703	4726.221614	23.700109
115.786450	4741.544610	23.705127
115.978903	4746.804428	23.710144
116.548691	4742.432927	23.715162
116.166596	4750.202530	23.720179
116.480396	4742.430989	23.725197
116.461361	4742.102651	23.730215
116.005749	4747.057087	23.735232
116.175772	4755.996163	23.740250
116.222668	4779.864941	23.745267
116.488787	4773.837852	23.750285
116.786097	4793.603740	23.755303
116.903145	4804.332291	23.760320
117.302775	4805.764141	23.765338
117.235711	4806.908619	23.770355
117.226767	4813.780080	23.775373
117.517627	4831.997161	23.780391
117.672585	4844.941968	23.785408
117.917007	4840.369139	23.790426
117.936096	4840.336123	23.795443
117.712898	4842.616920	23.800461
118.372100	4839.634815	23.805479
118.404809	4850.068636	23.810496
118.460453	4847.446356	23.815514
118.545401	4850.188839	23.820531
118.455139	4854.739441	23.825549
118.670326	4848.047388	23.830567
118.754824	4861.680393	23.835584
118.799609	4873.117164	23.840602
118.931606	4884.645824	23.845619
119.149356	4884.917782	23.850637
119.414480	4884.870808	23.855655
119.039329	4911.140071	23.860672
119.501877	4900.351857	23.865690
119.720653	4914.703776	23.870707
119.723480	4917.617381	23.875725
120.195484	4928.394357	23.880743
120.271822	4935.410053	23.885760
120.470035	4934.183353	23.890778
120.263921	4935.457184	23.895795
120.434024	4935.827602	23.900813
120.914765	4927.786547	23.905831
120.823132	4935.689291	23.910848
121.004917	4943.561733	23.915866
121.184974	4942.089954	23.920883
121.139102	4956.581812	23.925901
121.398615	4953.556390	23.930919
121.391644	4955.365877	23.935936
121.709892	4943.740710	23.940954
121.522286	4945.361946	23.945971
121.504762	4944.497805	23.950989
121.794917	4959.008850	23.956007
121.804979	4975.365881	23.961024
122.097982	4972.482187	23.966042
122.270237	4973.900507	23.971059
122.406928	4966.359011	23.976077
122.330435	4973.491385	23.981095
122.702914	4986.890952	23.986112
122.577554	4994.211781	23.991130
122.788853	5008.252358	23.996147
122.722433	5003.312746	24.001165
123.167232	4996.783446	24.006183
123.065771	5014.628592	24.011200
123.200967	5013.658830	24.016218
123.591088	5026.012763	24.021235
123.189840	5035.979856	24.026253
123.328041	5027.745803	24.031271
123.653097	5042.976503	24.036288
123.980051	5045.602557	24.041306
124.131080	5058.609622	24.046323
124.072195	5059.160507	24.051341
124.236431	5055.664120	24.056359
124.379775	5052.560254	24.061376
124.612872	5055.270368	24.066394
124.524412	5068.410814	24.071411
124.422100	5088.820531	24.076429
124.522756	5092.492158	24.081447
124.764506	5088.315065	24.086464
124.905222	5088.394224	24.091482
125.177739	5111.295234	24.096499
125.274253	5111.354146	24.101517
125.556763	5116.721254	24.106535
125.366055	5118.092571	24.111552
125.385153	5114.538292	24.116570
125.853399	5136.138144	24.121587
125.785447	5152.179855	24.126605
125.681827	5141.712038	24.131623
125.880331	5147.549861	24.136640
126.273546	5159.054376	24.141658
126.350622	5171.816240	24.146675
126.098069	5178.359605	24.151693
126.567406	5168.322225	24.156711
126.634376	5183.794261	24.161728
126.638678	5195.798726	24.166746
126.923718	5193.987422	24.171763
126.938380	5204.491411	24.176781
127.111486	5216.911353	24.181799
127.237330	5229.318652	24.186816
127.725777	5223.190789	24.191834
127.775276	5228.446873	24.196851
127.754478	5240.039683	24.201869
128.144800	5254.339096	24.206887
128.214494	5263.292709	24.211904
128.094965	5253.956061	24.216922
128.344366	5259.090061	24.221939
128.154616	5270.329675	24.226957
128.555799	5281.253297	24.231975
128.495243	5287.683799	24.236992
129.093427	5286.134886	24.242010
129.068655	5289.231911	24.247027
129.138791	5301.344482	24.252045
129.360902	5299.336449	24.257063
129.566746	5312.563837	24.262080
129.857722	5305.275441	24.267098
130.127449	5311.520529	24.272115
129.770031	5315.032561	24.277133
129.927737	5306.924299	24.282151
130.043767	5318.572484	24.287168
130.025640	5331.699929	24.292186
130.310183	5335.914533	24.297203
130.111930	5344.242316	24.302221
130.330014	5347.699240	24.307239
130.795460	5356.974090	24.312256
130.908093	5361.646400	24.317274
131.012158	5357.925994	24.322291
130.950645	5371.067743	24.327309
131.758123	5358.375998	24.332327
131.695910	5369.389006	24.337344
131.648235	5384.535256	24.342362
132.264263	5376.384942	24.347379
132.181771	5381.434528	24.352397
132.569793	5381.367995	24.357415
132.620088	5378.879616	24.362432
132.140741	5382.882041	24.367450
132.541181	5375.644798	24.372467
132.661553	5385.024053	24.377485
132.948023	5371.968843	24.382503
132.688161	5373.939173	24.387520
132.972462	5374.698668	24.392538
132.877876	5370.315706	24.397555
132.551081	5388.197006	24.402573
133.067773	5404.221723	24.407591
132.753629	5406.285317	24.412608
132.808040	5404.101838	24.417626
133.081345	5427.423752	24.422643
133.138723	5437.494735	24.427661
133.620177	5446.614195	24.432679
133.426329	5463.735593	24.437696
133.395293	5473.291974	24.442714
134.110395	5480.781039	24.447731
133.998935	5492.869479	24.452749
133.948078	5502.148774	24.457767
134.375153	5509.756424	24.462784
134.163262	5523.746236	24.467802
134.522243	5535.146432	24.472819
134.582645	5536.807000	24.477837
134.891905	5554.471341	24.482855
135.619734	5559.594751	24.487872
135.542430	5558.057625	24.492890
135.902626	5554.539711	24.497907
135.816733	5558.996854	24.502925
135.988232	5558.392009	24.507943
135.684099	5585.638283	24.512960
136.104346	5585.572715	24.517978
136.448052	5581.677902	24.522995
136.351966	5586.583310	24.528013
136.785120	5600.144265	24.533031
136.524374	5608.710151	24.538048
137.069324	5613.683496	24.543066
137.243534	5609.930152	24.548083
137.442833	5614.585038	24.553101
137.193948	5611.398721	24.558119
137.212556	5607.312780	24.563136
137.087617	5627.059839	24.568154
137.550805	5633.562864	24.573171
137.666364	5648.326344	24.578189
137.843405	5657.353770	24.583207
137.842587	5667.227395	24.588224
137.870433	5682.324409	24.593242
138.413801	5683.479724	24.598259
137.936311	5688.790920	24.603277
138.182704	5706.800572	24.608295
138.613011	5716.546142	24.613312
138.140700	5714.168650	24.618330
138.498073	5719.882720	24.623347
138.906327	5728.905774	24.628365
139.055953	5747.249687	24.633383
139.536249	5756.235626	24.638400
139.685798	5762.093597	24.643418
139.548438	5759.022678	24.648435
139.527959	5778.265100	24.653453
139.826584	5783.343079	24.658471
140.596080	5779.128837	24.663488
140.449870	5786.593678	24.668506
140.867602	5776.158053	24.673523
140.476556	5792.301162	24.678541
140.759807	5810.306406	24.683559
141.036988	5806.081516	24.688576
140.812804	5814.435892	24.693594
140.894654	5809.127293	24.698611
141.099640	5825.911324	24.703629
141.202380	5833.141217	24.708647
141.598706	5840.465853	24.713664
141.645690	5851.772225	24.718682
141.582992	5842.457324	24.723699
141.805303	5867.929855	24.728717
141.994470	5878.214009	24.733735
141.984664	5880.487976	24.738752
141.696260	5892.181491	24.743770
142.295359	5890.593780	24.748787
142.176628	5904.918206	24.753805
142.810812	5919.888281	24.758823
142.853252	5924.998481	24.763840
143.049009	5945.719895	24.768858
143.325733	5936.927643	24.773875
143.219560	5933.181264	24.778893
143.247456	5927.625582	24.783911
143.527133	5946.427068	24.788928
143.423368	5958.493323	24.793946
144.055959	5958.814765	24.798963
143.786492	5961.591703	24.803981
144.020156	5978.004117	24.808999
144.269079	5986.132182	24.814016
144.176925	5995.122457	24.819034
144.457545	5998.458117	24.824051
144.593936	6019.155589	24.829069
144.917380	6031.629258	24.834087
144.838052	6034.907163	24.839104
144.896452	6047.902025	24.844122
145.423977	6052.995753	24.849139
145.323490	6064.562192	24.854157
145.285319	6060.517828	24.859175
145.980930	6074.804462	24.864192
146.017076	6086.422333	24.869210
146.014911	6088.763589	24.874227
146.323673	6077.701529	24.879245
146.036236	6090.791490	24.884263
146.552940	6109.415305	24.889280
146.563743	6118.591025	24.894298
146.656456	6115.333084	24.899315
146.834293	6122.054471	24.904333
146.668541	6143.325901	24.909351
147.120137	6149.725518	24.914368
147.316368	6152.985393	24.919386
147.372168	6172.953674	24.924403
147.518558	6180.419090	24.929421
147.504612	6174.129089	24.934439
147.897854	6183.596751	24.939456
147.643970	6196.734802	24.944474
148.324512	6192.228794	24.949491
148.766588	6205.402855	24.954509
148.770401	6226.925146	24.959527
148.803696	6228.185432	24.964544
148.626727	6240.924846	24.969562
148.699639	6231.617194	24.974579
148.884621	6245.701037	24.979597
148.952858	6251.612034	24.984615
149.417545	6267.860479	24.989632
149.297414	6289.244272	24.994650
149.642152	6287.336323	24.999667
149.864560	6288.589722	25.004685
149.811689	6312.719138	25.009703
150.363179	6318.539913	25.014720
150.446094	6325.025845	25.019738
150.390756	6320.028064	25.024755
150.682975	6344.891972	25.029773
150.625636	6348.191506	25.034791
151.116065	6354.320131	25.039808
150.819860	6353.561124	25.044826
151.023564	6365.765030	25.049843
151.538794	6380.744212	25.054861
151.538262	6380.132375	25.059879
151.655910	6384.727757	25.064896
151.720600	6405.427366	25.069914
151.755320	6413.783299	25.074931
151.960688	6420.597136	25.079949
152.109067	6433.191472	25.084967
152.594503	6434.606911	25.089984
152.628263	6451.278965	25.095002
152.723745	6448.458428	25.100019
152.964817	6442.337189	25.105037
152.909648	6460.853673	25.110055
153.485483	6466.178983	25.115072
153.670879	6473.582157	25.120090
153.413777	6471.481611	25.125107
153.707294	6465.988885	25.130125
153.590289	6483.429471	25.135143
153.902608	6487.101826	25.140160
153.858510	6504.797377	25.145178
154.056727	6512.559189	25.150195
154.207090	6516.087444	25.155213
154.179481	6535.443023	25.160231
154.471757	6542.522139	25.165248
154.776257	6553.416183	25.170266
154.988136	6555.635429	25.175283
154.821472	6560.409470	25.180301
154.840179	6575.002389	25.185319
155.193926	6582.117029	25.190336
155.465141	6600.527656	25.195354
155.759501	6610.835043	25.200371
155.906222	6617.331798	25.205389
155.852752	6626.253801	25.210407
156.364613	6631.840232	25.215424
156.353245	6640.310249	25.220442
156.527260	6667.035767	25.225459
156.733362	6664.131502	25.230477
156.697507	6665.667924	25.235495
157.147748	6678.629937	25.240512
157.016585	6687.365560	25.245530
156.835485	6691.034586	25.250547
157.474956	6701.910295	25.255565
157.547900	6717.766431	25.260583
157.401795	6717.072348	25.265600
157.911224	6741.029768	25.270618
158.190458	6746.501161	25.275635
158.129136	6751.045938	25.280653
158.363275	6770.597918	25.285671
158.450284	6772.642528	25.290688
158.444506	6772.322979	25.295706
158.440194	6792.436682	25.300723
158.923023	6795.118358	25.305741
159.377294	6822.724029	25.310759
159.721575	6823.135762	25.315776
159.567705	6831.492420	25.320794
159.658231	6828.208702	25.325811
160.106601	6845.295367	25.330829
159.892616	6866.237841	25.335847
160.175293	6860.115067	25.340864
160.448211	6869.259641	25.345882
160.399431	6883.198439	25.350899
160.694371	6895.831105	25.355917
160.611624	6900.607107	25.360935
161.052110	6913.688291	25.365952
161.225686	6926.249704	25.370970
161.293665	6917.402466	25.375987
161.495805	6937.102517	25.381005
161.227709	6950.524739	25.386023
161.683834	6957.302019	25.391040
162.204459	6960.008974	25.396058
162.250120	6987.372238	25.401075
162.342353	6982.779885	25.406093
162.568528	6994.785214	25.411111
162.357154	6996.291650	25.416128
162.541476	7008.049500	25.421146
162.323217	7021.105140	25.426163
162.831232	7030.796126	25.431181
163.275333	7051.969381	25.436199
163.087495	7048.288243	25.441216
163.621641	7057.637795	25.446234
163.607834	7073.950534	25.451251
164.165845	7080.969357	25.456269
164.152694	7091.180671	25.461287
164.350496	7087.464823	25.466304
164.304682	7090.686198	25.471322
164.658168	7106.204836	25.476339
164.746074	7107.853140	25.481357
164.817067	7120.767241	25.486375
164.929174	7122.762057	25.491392
165.304617	7132.137927	25.496410
165.415399	7150.182702	25.501427
165.553667	7154.662256	25.506445
165.762678	7156.300756	25.511463
166.144558	7171.883286	25.516480
166.062221	7172.045073	25.521498
165.882259	7178.922242	25.526515
166.340676	7182.087726	25.531533
166.165429	7203.040770	25.536551
166.676836	7199.153249	25.541568
166.763042	7204.815082	25.546586
166.836661	7234.493078	25.551603
167.103913	7232.612816	25.556621
167.145391	7245.414540	25.561639
167.596303	7253.734307	25.566656
167.675303	7267.761775	25.571674
167.736287	7278.291764	25.576691
168.000607	7278.623014	25.581709
168.094424	7301.474075	25.586727
168.212881	7298.797670	25.591744
168.752052	7310.292198	25.596762
168.888586	7321.551709	25.601779
169.024251	7319.927164	25.606797
169.227221	7333.598612	25.611815
169.214725	7347.605852	25.616832
169.293037	7345.125130	25.621850
169.339602	7351.975899	25.626867
169.969711	7376.629523	25.631885
169.875824	7388.706254	25.636903
169.844288	7390.554743	25.641920
170.129701	7387.811298	25.646938
170.316185	7410.189525	25.651955
170.599031	7415.324996	25.656973
170.501232	7426.466625	25.661991
170.694508	7439.989320	25.667008
170.822235	7454.384615	25.672026
171.120114	7471.367687	25.677044
171.515281	7477.207687	25.682061
171.772012	7479.154186	25.687079
172.002684	7493.140988	25.692096
172.403385	7509.427298	25.697114
172.452333	7513.304974	25.702132
172.313872	7505.159554	25.707149
172.353961	7520.068030	25.712167
172.611490	7524.156939	25.717184
172.908860	7540.321752	25.722202
172.703818	7542.745646	25.727220
173.064299	7545.140507	25.732237
172.959463	7574.759671	25.737255
173.472470	7572.470041	25.742272
173.409272	7576.178039	25.747290
173.799902	7594.484978	25.752308
174.146201	7589.332870	25.757325
174.410972	7611.493617	25.762343
174.622453	7630.469871	25.767360
174.724530	7628.045824	25.772378
174.879069	7631.659498	25.777396
175.108342	7626.231363	25.782413
175.203833	7631.074176	25.787431
175.235190	7646.608863	25.792448
175.245838	7638.473348	25.797466
174.953374	7656.392469	25.802484
175.385424	7659.496248	25.807501
175.446666	7676.980312	25.812519
175.392599	7697.808391	25.817536
175.864196	7707.371125	25.822554
175.843059	7732.555329	25.827572
176.242057	7745.532215	25.832589
176.569714	7756.505176	25.837607
176.585166	7770.449870	25.842624
177.168003	7773.587787	25.847642
177.170812	7791.688974	25.852660
177.155172	7802.001983	25.857677
177.416108	7808.121909	25.862695
177.307175	7824.320405	25.867712
177.970387	7842.107512	25.872730
178.110327	7852.846157	25.877748
178.032591	7870.760689	25.882765
178.567787	7885.455203	25.887783
178.576125	7887.201835	25.892800
179.286278	7892.114690	25.897818
178.918266	7911.040699	25.902836
179.060879	7908.316081	25.907853
179.495846	7928.399455	25.912871
179.539152	7931.096592	25.917888
179.923225	7941.809059	25.922906
179.657097	7954.437777	25.927924
180.063067	7956.865345	25.932941
180.404970	7975.626639	25.937959
180.756610	7981.868680	25.942976
180.848532	8000.900615	25.947994
180.713766	8001.186097	25.953012
180.925538	8012.553375	25.958029
181.201988	8018.792911	25.963047
181.409586	8032.335794	25.968064
181.739286	8033.688156	25.973082
181.889523	8069.040803	25.978100
182.317085	8054.558682	25.983117
182.723342	8076.028663	25.988135
182.263799	8083.154950	25.993152
182.852364	8084.026485	25.998170
182.696777	8078.199519	26.003188
182.812003	8101.497185	26.008205
183.037213	8104.795205	26.013223
183.223661	8124.058985	26.018240
183.572042	8130.941258	26.023258
183.506256	8139.840939	26.028276
183.795219	8138.934549	26.033293
183.792740	8156.751868	26.038311
183.943688	8174.116857	26.043328
184.032644	8177.699764	26.048346
184.280785	8198.435927	26.053364
184.569661	8201.811653	26.058381
184.710815	8227.155674	26.063399
185.156204	8240.087473	26.068416
185.398444	8244.394152	26.073434
185.857005	8261.305778	26.078452
185.836518	8267.951415	26.083469
185.679141	8264.672208	26.088487
185.899124	8278.608693	26.093504
186.283826	8291.742001	26.098522
186.211153	8301.182511	26.103540
186.505654	8312.636349	26.108557
186.796242	8326.669895	26.113575
186.786209	8329.603585	26.118592
186.876283	8337.559071	26.123610
186.987786	8353.577453	26.128628
187.187125	8367.039275	26.133645
187.611754	8374.575459	26.138663
187.481943	8390.004423	26.143680
187.616982	8393.659310	26.148698
187.561250	8432.004824	26.153716
187.844994	8429.443449	26.158733
188.438383	8443.142594	26.163751
188.434912	8460.867462	26.168768
189.086035	8473.901672	26.173786
189.134333	8482.922087	26.178804
189.372851	8490.007037	26.183821
189.770725	8502.184379	26.188839
189.736937	8515.258750	26.193856
190.139049	8524.366348	26.198874
190.168117	8519.119942	26.203892
190.447198	8541.023595	26.208909
190.442676	8550.288330	26.213927
190.382909	8557.564485	26.218944
190.713918	8569.407914	26.223962
191.193164	8583.725554	26.228980
190.969894	8594.743822	26.233997
191.773598	8614.857609	26.239015
191.626773	8621.431352	26.244032
191.946017	8617.432727	26.249050
192.025804	8633.320358	26.254068
192.305816	8639.934520	26.259085
192.681500	8645.689950	26.264103
192.657191	8662.913542	26.269120
192.673065	8670.158320	26.274138
192.418460	8677.426610	26.279156
193.177807	8693.905265	26.284173
193.412559	8693.140952	26.289191
193.435090	8719.182072	26.294208
193.326403	8732.280048	26.299226
193.531045	8754.156141	26.304244
193.721172	8766.589438	26.309261
194.308379	8782.187609	26.314279
194.055241	8801.751066	26.319296
194.094840	8812.146173	26.324314
194.533797	8829.117580	26.329332
195.202887	8856.137421	26.334349
195.311080	8866.488122	26.339367
195.358048	8873.218949	26.344384
195.604481	8881.249655	26.349402
196.017499	8896.675895	26.354420
196.131570	8905.780980	26.359437
196.382581	8916.932074	26.364455
196.266985	8930.121948	26.369472
196.844445	8941.831898	26.374490
196.989737	8955.019567	26.379508
196.987642	8960.765178	26.384525
197.457881	8976.629475	26.389543
197.682926	8991.219592	26.394560
197.835647	8988.843677	26.399578
198.160986	8994.298763	26.404596
198.156941	9010.340869	26.409613
198.401800	9018.369542	26.414631
198.468871	9025.760408	26.419648
199.255461	9049.359529	26.424666
199.537534	9055.743493	26.429684
199.113043	9059.320215	26.434701
199.629371	9049.885522	26.439719
199.491321	9065.656029	26.444736
199.513177	9084.105296	26.449754
199.753729	9083.184026	26.454772
199.545975	9097.645794	26.459789
199.947208	9108.441287	26.464807
199.986140	9128.467268	26.469824
200.363051	9135.422457	26.474842
200.574246	9149.937021	26.479860
200.416757	9170.424910	26.484877
201.222444	9164.305275	26.489895
201.021731	9192.671830	26.494912
201.183769	9205.227497	26.499930
201.450802	9222.435757	26.504948
201.759964	9239.486595	26.509965
202.151723	9251.399252	26.514983
202.227501	9271.453974	26.520000
202.581507	9267.001186	26.525018
203.001578	9279.588247	26.530036
202.802654	9300.293499	26.535053
203.391749	9305.102372	26.540071
203.515179	9320.142893	26.545088
203.503141	9331.220442	26.550106
203.867967	9344.211380	26.555124
203.944704	9359.780395	26.560141
204.024158	9357.031327	26.565159
204.296447	9381.284075	26.570176
204.703278	9387.126790	26.575194
204.820925	9397.048499	26.580212
204.571476	9421.690979	26.585229
205.235244	9428.591718	26.590247
205.318101	9446.061531	26.595264
205.728517	9467.542937	26.600282
205.843687	9474.833876	26.605300
205.752225	9499.803252	26.610317
206.315617	9494.578363	26.615335
206.529247	9526.961628	26.620352
206.662455	9532.457371	26.625370
206.701665	9544.882381	26.630388
206.932861	9559.907650	26.635405
206.921915	9570.128059	26.640423
207.693854	9591.091283	26.645440
208.011566	9609.888439	26.650458
208.077674	9625.288518	26.655476
208.157720	9625.155593	26.660493
208.678606	9634.393847	26.665511
208.847187	9643.271319	26.670528
209.293399	9647.076658	26.675546
209.612088	9648.757924	26.680564
209.533386	9655.349960	26.685581
209.676394	9662.439425	26.690599
209.848700	9671.102013	26.695616
209.693779	9674.599580	26.700634
210.209529	9689.391154	26.705652
210.361770	9700.047860	26.710669
210.426465	9718.867335	26.715687
210.842960	9735.945050	26.720704
210.949419	9746.226492	26.725722
211.426687	9757.566816	26.730740
211.112663	9770.076474	26.735757
211.366774	9770.021087	26.740775
211.490977	9789.966812	26.745792
211.701961	9801.950773	26.750810
212.367147	9822.545947	26.755828
212.460817	9841.513603	26.760845
212.581672	9842.752591	26.765863
212.596225	9867.163760	26.770880
212.751441	9880.338730	26.775898
213.450609	9885.042901	26.780916
213.317286	9906.084709	26.785933
213.789126	9920.233031	26.790951
213.894727	9938.680445	26.795968
214.082236	9933.412075	26.800986
214.305953	9939.516137	26.806004
214.344591	9962.707076	26.811021
214.761516	9959.677511	26.816039
215.099700	9978.281058	26.821056
215.510051	9997.185445	26.826074
215.656597	10003.072263	26.831092
215.401980	9997.218447	26.836109
215.892559	10008.838786	26.841127
216.103241	10018.737601	26.846144
216.350351	10015.256355	26.851162
216.468678	10032.778445	26.856180
216.572884	10054.619367	26.861197
216.664688	10050.563504	26.866215
217.041048	10079.957948	26.871232
217.081971	10085.961548	26.876250
217.488896	10105.914434	26.881268
217.650242	10125.609414	26.886285
217.764639	10112.221159	26.891303
218.100097	10134.324068	26.896320
218.108568	10156.462230	26.901338
218.146603	10165.085862	26.906356
218.322005	10180.243849	26.911373
218.554740	10200.143754	26.916391
218.837940	10218.915824	26.921408
219.040410	10245.890782	26.926426
219.729914	10254.424736	26.931444
219.728622	10274.116883	26.936461
219.873789	10284.014101	26.941479
220.352653	10294.412294	26.946496
220.731615	10313.973788	26.951514
221.045714	10323.920274	26.956532
221.025293	10335.887004	26.961549
221.281943	10343.659132	26.966567
221.513997	10363.161494	26.971584
221.438676	10376.114260	26.976602
221.980011	10380.128564	26.981620
222.024889	10397.858594	26.986637
222.394828	10411.144991	26.991655
223.010076	10424.156803	26.996672
222.900298	10436.644981	27.001690
223.329769	10442.730931	27.006708
223.076051	10460.873655	27.011725
223.652331	10472.599896	27.016743
223.689635	10493.347933	27.021760
223.824443	10504.580820	27.026778
224.168702	10505.229811	27.031796
224.179608	10528.627055	27.036813
224.433864	10553.280843	27.041831
224.676292	10562.179687	27.046848
224.863237	10585.396605	27.051866
225.217896	10586.890026	27.056884
225.441200	10615.349610	27.061901
225.733057	10617.991085	27.066919
226.164334	10629.171830	27.071936
226.163757	10652.090565	27.076954
226.622149	10648.846018	27.081972
226.647399	10664.713960	27.086989
226.774524	10671.471663	27.092007
227.134065	10692.868589	27.097024
227.407620	10711.114180	27.102042
227.906173	10709.909817	27.107060
227.893042	10719.290677	27.112077
228.117597	10738.677345	27.117095
228.460349	10751.519448	27.122112
228.487319	10766.219602	27.127130
229.179277	10767.105705	27.132148
228.744448	10773.143409	27.137165
228.915014	10783.035942	27.142183
229.120154	10794.014728	27.147200
229.354698	10811.518426	27.152218
229.535730	10825.346971	27.157236
229.337579	10848.347538	27.162253
229.753939	10867.779821	27.167271
230.147189	10866.841843	27.172288
230.438375	10906.106469	27.177306
230.919204	10903.040942	27.182324
230.526792	10930.835630	27.187341
230.839038	10944.256502	27.192359
231.610281	10961.498187	27.197376
231.541078	10984.168757	27.202394
232.133289	10993.670170	27.207412
232.307190	11014.636564	27.212429
232.529451	11020.431647	27.217447
232.916638	11021.506882	27.222464
233.097360	11039.642154	27.227482
233.672359	11051.607757	27.232500
233.697437	11059.598988	27.237517
233.772242	11069.819546	27.242535
234.203632	11088.683916	27.247552
234.023702	11100.828101	27.252570
234.479096	11111.894888	27.257588
234.619650	11129.121401	27.262605
235.083776	11136.376600	27.267623
235.148192	11148.133707	27.272640
235.439250	11158.715612	27.277658
235.656202	11170.485303	27.282676
235.614678	11190.800558	27.287693
236.080732	11216.050600	27.292711
236.185526	11221.219140	27.297728
236.034098	11239.976893	27.302746
236.389080	11253.947192	27.307764
236.967466	11277.877156	27.312781
237.101836	11291.069338	27.317799
237.543137	11314.881807	27.322816
237.474618	11318.156634	27.327834
237.755786	11338.940236	27.332852
238.121792	11361.272985	27.337869
238.427270	11383.535421	27.342887
238.854387	11390.215401	27.347904
238.680915	11416.353206	27.352922
239.289938	11414.307954	27.357940
239.553474	11430.206535	27.362957
239.502101	11451.237574	27.367975
240.086589	11459.713135	27.372992
240.183556	11470.680349	27.378010
240.229169	11489.859598	27.383028
240.501627	11510.120126	27.388045
240.982716	11525.380837	27.393063
241.230496	11542.330035	27.398080
241.457984	11551.715668	27.403098
241.496612	11564.719068	27.408116
241.707011	11569.988423	27.413133
241.497547	11606.119859	27.418151
242.159105	11610.369067	27.423168
242.557833	11638.528802	27.428186
242.723189	11656.498699	27.433204
242.931100	11663.145745	27.438221
243.140172	11678.569816	27.443239
243.486977	11699.046765	27.448256
243.472990	11712.276454	27.453274
243.932809	11731.045472	27.458292
244.067697	11745.057357	27.463309
244.330952	11768.097881	27.468327
244.807013	11774.073412	27.473344
244.719941	11798.910093	27.478362
245.152562	11808.610172	27.483380
245.205116	11814.881166	27.488397
245.390707	11840.506380	27.493415
245.872892	11843.751607	27.498432
245.927964	11868.237093	27.503450
246.207094	11871.698735	27.508468
246.604430	11893.842663	27.513485
246.535470	11910.070949	27.518503
246.847241	11930.005602	27.523520
247.212248	11944.786390	27.528538
247.366282	11960.921084	27.533556
247.684651	11973.575945	27.538573
248.212439	11995.852849	27.543591
248.471905	11999.103461	27.548608
248.623006	12027.506570	27.553626
248.503896	12046.928058	27.558644
249.036441	12047.314302	27.563661
249.314881	12071.785181	27.568679
249.625104	12088.964142	27.573696
249.818022	12106.848032	27.578714
250.073206	12124.255185	27.583732
250.014174	12125.279873	27.588749
250.075483	12155.002868	27.593767
251.307674	12165.350850	27.598784
251.532804	12186.152695	27.603802
251.724474	12200.024778	27.608820
252.019560	12210.773747	27.613837
251.704114	12233.144863	27.618855
252.017986	12239.057592	27.623872
252.676322	12257.830606	27.628890
252.760786	12261.573542	27.633908
253.247835	12272.328595	27.638925
253.260915	12296.109389	27.643943
253.623480	12296.890953	27.648960
253.854792	12316.952864	27.653978
253.867000	12323.856351	27.658996
254.290659	12344.776819	27.664013
254.287871	12366.581054	27.669031
254.745901	12380.123967	27.674048
254.829913	12401.154311	27.679066
254.643616	12415.092296	27.684084
255.118786	12433.158325	27.689101
255.029640	12475.816385	27.694119
255.628339	12483.439160	27.699136
255.818122	12506.563811	27.704154
256.175229	12526.479086	27.709172
256.855549	12547.091005	27.714189
256.573458	12576.859008	27.719207
257.000397	12585.638601	27.724224
257.255703	12614.690512	27.729242
257.525299	12634.382446	27.734260
258.088942	12650.913334	27.739277
258.220293	12665.035335	27.744295
258.705292	12687.860807	27.749312
258.945250	12706.328533	27.754330
259.087654	12710.567846	27.759348
259.254810	12722.165679	27.764365
259.281870	12738.654679	27.769383
259.829866	12754.157622	27.774400
259.998693	12773.122577	27.779418
260.133703	12793.357031	27.784436
260.594398	12801.450361	27.789453
260.808847	12820.417275	27.794471
261.184359	12836.090679	27.799488
261.291205	12861.164785	27.804506
261.715701	12878.771651	27.809524
262.142503	12876.283615	27.814541
262.268870	12899.080499	27.819559
262.573844	12917.865494	27.824576
262.562083	12921.656029	27.829594
262.738612	12954.338328	27.834612
262.977797	12955.466568	27.839629
263.033000	12972.739109	27.844647
263.340731	12998.366417	27.849664
263.783842	13016.514047	27.854682
263.506367	13020.274521	27.859700
264.150133	13048.902016	27.864717
264.149999	13085.522139	27.869735
264.590541	13095.592027	27.874752
265.135366	13124.229729	27.879770
265.111745	13142.635992	27.884788
265.791386	13157.786581	27.889805
265.886026	13190.344225	27.894823
266.126649	13197.602684	27.899840
266.512137	13217.657519	27.904858
266.839489	13225.858236	27.909876
267.512162	13243.594620	27.914893
267.327155	13262.262550	27.919911
267.706581	13272.508139	27.924928
268.047957	13289.319169	27.929946
268.092631	13316.322206	27.934964
268.539648	13325.536994	27.939981
268.664280	13344.265656	27.944999
269.081003	13356.916349	27.950016
269.013553	13387.288563	27.955034
269.153517	13407.054897	27.960052
269.614458	13425.510498	27.965069
269.809432	13446.544311	27.970087
270.203688	13473.444037	27.975104
270.483938	13500.017541	27.980122
270.737369	13511.987770	27.985140
270.956496	13529.156542	27.990157
271.137436	13558.044359	27.995175
271.603228	13579.697003	28.000192
272.135086	13596.565074	28.005210
271.988024	13620.955846	28.010228
272.394487	13628.888361	28.015245
272.916797	13661.505383	28.020263
272.971882	13674.652735	28.025280
273.735356	13699.020558	28.030298
273.720237	13709.174132	28.035316
274.187187	13722.697779	28.040333
274.383977	13741.626136	28.045351
274.741677	13760.228438	28.050368
274.766318	13776.236629	28.055386
274.748374	13792.426822	28.060404
275.322307	13805.272482	28.065421
275.328364	13827.565766	28.070439
275.724095	13846.823796	28.075456
276.204468	13870.672949	28.080474
275.976961	13896.082943	28.085492
276.446062	13905.879108	28.090509
276.471092	13927.685550	28.095527
277.057572	13954.418713	28.100544
277.296078	13974.809287	28.105562
277.914666	14002.233816	28.110580
278.153479	14006.353491	28.115597
278.328858	14033.143801	28.120615
278.685263	14050.846736	28.125632
278.975397	14063.266768	28.130650
279.137897	14085.622765	28.135668
279.612051	14111.246338	28.140685
279.906730	14124.765738	28.145703
280.513393	14132.752043	28.150720
280.393919	14144.710389	28.155738
280.650488	14157.058822	28.160756
281.236953	14157.015403	28.165773
281.137258	14170.937394	28.170791
281.285593	14184.581934	28.175808
281.777167	14201.064866	28.180826
281.636147	14218.204142	28.185844
282.125841	14247.756019	28.190861
282.396611	14262.221968	28.195879
282.544444	14283.015643	28.200896
282.965525	14293.109985	28.205914
282.798585	14319.503522	28.210932
283.310565	14332.058827	28.215949
283.798435	14352.246261	28.220967
283.989878	14370.673467	28.225984
284.611386	14387.325783	28.231002
284.708420	14417.712081	28.236020
284.796272	14425.128765	28.241037
285.333122	14450.783470	28.246055
285.716313	14470.717294	28.251072
286.053471	14481.203901	28.256090
285.796425	14512.712834	28.261108
285.925754	14520.193618	28.266125
286.241442	14555.387261	28.271143
286.335864	14583.824689	28.276160
287.042953	14610.373473	28.281178
287.291518	14640.454558	28.286196
287.493826	14654.880176	28.291213
287.877586	14679.227208	28.296231
288.450158	14706.340590	28.301248
288.987095	14717.672165	28.306266
288.883321	14747.668343	28.311284
289.420942	14762.276543	28.316301
289.774124	14788.573706	28.321319
290.063673	14805.743195	28.326336
290.482508	14817.513631	28.331354
290.513274	14840.054801	28.336372
291.084952	14849.375909	28.341389
290.892223	14868.368468	28.346407
291.057090	14884.122841	28.351424
291.999430	14909.693809	28.356442
291.628722	14935.529444	28.361460
292.033321	14958.016777	28.366477
292.573131	14979.066405	28.371495
292.771244	15000.656488	28.376512
293.416368	15022.454734	28.381530
293.286151	15041.735032	28.386548
293.896729	15057.757815	28.391565
294.103586	15085.901678	28.396583
294.069828	15106.411228	28.401600
294.382639	15127.147142	28.406618
294.662530	15154.810923	28.411636
295.127193	15170.613667	28.416653
295.287046	15196.368194	28.421671
295.483315	15228.900455	28.426688
296.031016	15251.104439	28.431706
296.231060	15278.078683	28.436724
297.050038	15289.732789	28.441741
296.772466	15305.053280	28.446759
297.267058	15334.918384	28.451776
297.594884	15349.839239	28.456794
297.530239	15386.968513	28.461812
298.073884	15401.116049	28.466829
298.758128	15416.368856	28.471847
298.673519	15432.328970	28.476864
299.134661	15454.282761	28.481882
299.099342	15479.231516	28.486900
299.715779	15496.629753	28.491917
300.196285	15511.763485	28.496935
300.291163	15545.113848	28.501952
300.851543	15535.037680	28.506970
300.855611	15564.342892	28.511988
301.284952	15577.960991	28.517005
301.516275	15592.524486	28.522023
301.781227	15628.630399	28.527040
302.124664	15633.645779	28.532058
302.123572	15656.078277	28.537076
302.318484	15676.627919	28.542093
302.678092	15688.282691	28.547111
302.941222	15723.320457	28.552128
303.462078	15738.651048	28.557146
303.347070	15764.258087	28.562164
303.469242	15781.966987	28.567181
303.604865	15811.711112	28.572199
304.264189	15839.526026	28.577216
304.761753	15863.805538	28.582234
305.142466	15891.717095	28.587252
305.334164	15916.504414	28.592269
306.182155	15926.745043	28.597287
306.389427	15956.201733	28.602304
307.239838	15963.103565	28.607322
307.282401	15977.039787	28.612340
307.364103	16002.734427	28.617357
307.577730	16014.101503	28.622375
307.865106	16049.303027	28.627392
308.397177	16066.509349	28.632410
308.627745	16082.231927	28.637428
309.028761	16091.529979	28.642445
309.364318	16113.458151	28.647463
309.571255	16128.418638	28.652480
310.079356	16144.902367	28.657498
310.103007	16171.205846	28.662516
310.393073	16191.800277	28.667533
310.713735	16211.549535	28.672551
310.839024	16229.654036	28.677568
311.232941	16257.861936	28.682586
311.206081	16288.995688	28.687604
311.393944	16312.578409	28.692621
311.552307	16329.118635	28.697639
311.646955	16368.897068	28.702656
312.605237	16391.416086	28.707674
313.004464	16426.276768	28.712692
313.342831	16459.769945	28.717709
313.422447	16477.133552	28.722727
313.688289	16504.576518	28.727744
314.085458	16527.229581	28.732762
314.795825	16556.342407	28.737780
314.887652	16582.513882	28.742797
315.419208	16607.881222	28.747815
315.462377	16635.115362	28.752832
315.917088	16656.985127	28.757850
315.822647	16678.567508	28.762868
316.116869	16698.469895	28.767885
316.903898	16719.717275	28.772903
317.197354	16748.767039	28.777920
317.811805	16766.404971	28.782938
318.315930	16798.375498	28.787956
318.542939	16817.595584	28.792973
318.843835	16826.595366	28.797991
319.209393	16849.091744	28.803008
319.163951	16866.060316	28.808026
319.689857	16882.122541	28.813044
319.826272	16904.143047	28.818061
320.317198	16928.652215	28.823079
320.285924	16952.899489	28.828096
320.687012	16969.159005	28.833114
321.029190	16993.231030	28.838132
321.262391	17024.156028	28.843149
321.988527	17032.938940	28.848167
321.656982	17055.073358	28.853184
321.779879	17062.283660	28.858202
322.433761	17089.195201	28.863220
322.445164	17112.341677	28.868237
323.038456	17141.946234	28.873255
323.013796	17169.586560	28.878272
323.717988	17187.033539	28.883290
323.652790	17218.920986	28.888308
324.178543	17249.930394	28.893325
324.726800	17270.163437	28.898343
324.774010	17303.577252	28.903360
325.464045	17323.482659	28.908378
325.346469	17348.168830	28.913396
325.650545	17382.394667	28.918413
326.044638	17412.308540	28.923431
326.474422	17444.363555	28.928448
326.551475	17467.217491	28.933466
327.203998	17493.343311	28.938484
327.576199	17528.803498	28.943501
328.149207	17550.680086	28.948519
328.242891	17581.397489	28.953536
328.556676	17591.019796	28.958554
328.960234	17617.942101	28.963572
329.231406	17648.370149	28.968589
329.718621	17663.055482	28.973607
330.300922	17692.743238	28.978624
330.716567	17717.012236	28.983642
331.102907	17736.651555	28.988660
330.991200	17757.550891	28.993677
331.475870	17780.411880	28.998695
332.019127	17800.272795	29.003712
332.045266	17822.974856	29.008730
332.540637	17853.263705	29.013748
332.667371	17878.149835	29.018765
333.109006	17906.809801	29.023783
332.959505	17923.482971	29.028800
333.850112	17954.499517	29.033818
334.074616	17986.493394	29.038836
334.374475	18010.682672	29.043853
335.006259	18029.788297	29.048871
334.888816	18062.091142	29.053888
335.203933	18093.351382	29.058906
335.594894	18122.138338	29.063924
335.914240	18143.159134	29.068941
336.501327	18166.749351	29.073959
336.684308	18201.928584	29.078976
337.257678	18217.557039	29.083994
337.594121	18237.914602	29.089012
337.736815	18275.042819	29.094029
338.242018	18292.858105	29.099047
338.583519	18317.055124	29.104064
338.840517	18342.470564	29.109082
339.317225	18368.488137	29.114100
339.400410	18384.618793	29.119117
339.913436	18412.629354	29.124135
340.091745	18443.395820	29.129152
340.585237	18473.695569	29.134170
340.931987	18486.911981	29.139188
341.084457	18518.176291	29.144205
341.530945	18537.123995	29.149223
341.894654	18570.487965	29.154240
341.966397	18597.090002	29.159258
342.146131	18621.547554	29.164276
342.803170	18660.412315	29.169293
342.937013	18688.278006	29.174311
343.363245	18711.728514	29.179328
343.979298	18727.728739	29.184346
344.396777	18756.140352	29.189364
344.384671	18780.571560	29.194381
344.984390	18796.088998	29.199399
345.201966	18826.146559	29.204416
345.665056	18844.874311	29.209434
345.814502	18864.115907	29.214452
346.234053	18894.827511	29.219469
346.431713	18910.819914	29.224487
347.187761	18944.889024	29.229504
347.148389	18975.812314	29.234522
347.816625	18989.117799	29.239540
347.473418	19024.535623	29.244557
347.954477	19040.164366	29.249575
348.649639	19079.605525	29.254592
348.814802	19103.949533	29.259610
349.057153	19134.653070	29.264628
349.388149	19162.025000	29.269645
349.835520	19185.739107	29.274663
350.015187	19226.922856	29.279680
350.688679	19257.361347	29.284698
351.002140	19283.353765	29.289716
350.920562	19314.171154	29.294733
351.246893	19345.901690	29.299751
351.873079	19368.317350	29.304768
352.410496	19401.923817	29.309786
352.776301	19431.511771	29.314804
353.068155	19479.067297	29.319821
353.340512	19505.528791	29.324839
353.880266	19533.524199	29.329856
354.088443	19568.098315	29.334874
354.670652	19589.276073	29.339892
354.685827	19624.605890	29.344909
355.247024	19653.822936	29.349927
356.035529	19677.755602	29.354944
355.974800	19712.760782	29.359962
356.268126	19735.731800	29.364980
356.752117	19772.997616	29.369997
357.146621	19799.850844	29.375015
357.480220	19829.693931	29.380032
357.525018	19860.075187	29.385050
358.186398	19892.938471	29.390068
358.482408	19914.884510	29.395085
358.657981	19944.238411	29.400103
358.944189	19984.871921	29.405120
359.131709	20021.044327	29.410138
359.863302	20042.899520	29.415156
360.129254	20082.757780	29.420173
360.612405	20121.632645	29.425191
361.077832	20153.499348	29.430208
361.082053	20185.139735	29.435226
361.711877	20219.196071	29.440244
361.934800	20251.891405	29.445261
362.179833	20283.354954	29.450279
362.857034	20310.329333	29.455296
363.266639	20359.532778	29.460314
363.504781	20386.266197	29.465332
363.619046	20425.773560	29.470349
363.759234	20450.763769	29.475367
364.313028	20490.767704	29.480384
364.850300	20529.289270	29.485402
364.989247	20551.050864	29.490420
365.367254	20591.908721	29.495437
365.337023	20629.425516	29.500455
365.924960	20662.753386	29.505472
366.220437	20700.225892	29.510490
366.751470	20740.543214	29.515508
367.317379	20788.087041	29.520525
367.466801	20817.941867	29.525543
368.102250	20843.033582	29.530560
368.497881	20873.175705	29.535578
369.205401	20900.738845	29.540596
369.263702	20941.019789	29.545613
369.700873	20960.944595	29.550631
370.221260	20996.802274	29.555648
370.346977	21025.996029	29.560666
371.141863	21049.158598	29.565684
371.127686	21074.651440	29.570701
371.565117	21099.142479	29.575719
372.031896	21132.045126	29.580736
372.018460	21162.485668	29.585754
372.819283	21178.263728	29.590772
372.828149	21229.227842	29.595789
372.965075	21261.091096	29.600807
373.820265	21295.145422	29.605824
373.615140	21334.061318	29.610842
374.151305	21363.764804	29.615860
374.420258	21395.281655	29.620877
374.847287	21442.096636	29.625895
375.429413	21473.099818	29.630912
375.591390	21523.244803	29.635930
376.305519	21552.824564	29.640948
376.560448	21590.258454	29.645965
376.870049	21629.047264	29.650983
376.938107	21658.224849	29.656000
377.055335	21702.685704	29.661018
377.923884	21735.865187	29.666036
378.684325	21779.642696	29.671053
378.762835	21822.380566	29.676071
379.275885	21858.537721	29.681088
379.624343	21896.453490	29.686106
380.047442	21934.388526	29.691124
380.516185	21970.584789	29.696141
380.709820	22010.314505	29.701159
381.487110	22042.323954	29.706176
381.886163	22069.410258	29.711194
382.428167	22110.280911	29.716212
382.484363	22140.021049	29.721229
382.890921	22174.591327	29.726247
383.170289	22212.079310	29.731264
383.459929	22242.629311	29.736282
384.416395	22273.978824	29.741300
384.358013	22316.442577	29.746317
384.643565	22351.753845	29.751335
385.042423	22379.307414	29.756352
385.372272	22420.355840	29.761370
386.033650	22453.878502	29.766388
386.338442	22492.474558	29.771405
386.406816	22526.134927	29.776423
387.188753	22562.488762	29.781440
387.543812	22608.323893	29.786458
388.027302	22630.679219	29.791476
388.595709	22672.638032	29.796493
388.570852	22709.359080	29.801511
389.019432	22739.079478	29.806528
389.333679	22781.731862	29.811546
389.663260	22812.176936	29.816564
390.187969	22847.019171	29.821581
390.865196	22884.679321	29.826599
391.177906	22904.902970	29.831616
391.555537	22951.063277	29.836634
392.056150	22979.605446	29.841652
392.376540	23018.394070	29.846669
392.650480	23052.947086	29.851687
393.220173	23074.449830	29.856704
392.995510	23119.928143	29.861722
393.708249	23150.453905	29.866740
393.884613	23176.755696	29.871757
394.168582	23220.723012	29.876775
394.630552	23247.594209	29.881792
395.088789	23284.756921	29.886810
395.647472	23321.996127	29.891828
395.827864	23355.779941	29.896845
396.155351	23398.045336	29.901863
396.713406	23423.459612	29.906880
396.604404	23450.906586	29.911898
397.107435	23504.569532	29.916916
397.668559	23541.796200	29.921933
398.123586	23578.403428	29.926951
398.746595	23620.292464	29.931968
398.777987	23659.027874	29.936986
399.294756	23701.633274	29.942004
399.996397	23748.059081	29.947021
400.029245	23781.551190	29.952039
400.834675	23811.332672	29.957056
400.699718	23866.756564	29.962074
401.021741	23898.144694	29.967092
401.598649	23946.149717	29.972109
402.309032	23982.381235	29.977127
402.899699	24020.730012	29.982144
403.776882	24056.060441	29.987162
403.645787	24082.622671	29.992180
404.242835	24126.171492	29.997197
404.647690	24154.780364	30.002215
405.133234	24188.002802	30.007232
405.478039	24238.573389	30.012250
405.694605	24254.316978	30.017268
406.135806	24287.461791	30.022285
406.378122	24320.913980	30.027303
407.332877	24368.006078	30.032320
407.517274	24410.762873	30.037338
407.812971	24444.670109	30.042356
408.481081	24474.049684	30.047373
408.872679	24512.375737	30.052391
409.468289	24539.118039	30.057408
409.668212	24583.601107	30.062426
410.215491	24606.399499	30.067444
410.220589	24639.279684	30.072461
410.877449	24678.688206	30.077479
411.279478	24705.693052	30.082496
411.504003	24740.388551	30.087514
411.881285	24785.237048	30.092532
412.331958	24818.119532	30.097549
412.545912	24870.271755	30.102567
412.872324	24904.953880	30.107584
413.407429	24949.249951	30.112602
413.871311	24986.413851	30.117620
414.292857	25021.569355	30.122637
414.137219	25074.600282	30.127655
414.979767	25114.244021	30.132672
415.321679	25159.805877	30.137690
415.512794	25208.698365	30.142708
416.340618	25241.740034	30.147725
416.657049	25289.000234	30.152743
417.250563	25323.597995	30.157760
417.538012	25370.030512	30.162778
418.134375	25405.110556	30.167796
418.886217	25443.514700	30.172813
419.403883	25478.790862	30.177831
419.730830	25509.329492	30.182848
420.372098	25544.777742	30.187866
420.728628	25561.656967	30.192884
421.479563	25600.815472	30.197901
421.645255	25630.712308	30.202919
422.066162	25637.465330	30.207936
422.289052	25670.667870	30.212954
422.959625	25696.087409	30.217972
423.679788	25711.733223	30.222989
423.633333	25738.671975	30.228007
424.132023	25767.725376	30.233024
424.812177	25801.331942	30.238042
424.856192	25817.597588	30.243060
425.160077	25841.387339	30.248077
425.468334	25873.254502	30.253095
425.734827	25901.444434	30.258112
426.010419	25954.201672	30.263130
426.480046	25987.351372	30.268148
427.179408	26019.835410	30.273165
426.858638	26064.966790	30.278183
427.440494	26093.634770	30.283200
427.920467	26134.287164	30.288218
428.259352	26190.870310	30.293236
428.453694	26231.065509	30.298253
429.192792	26282.141481	30.303271
429.639929	26316.620364	30.308288
430.129932	26364.779016	30.313306
430.767771	26405.645656	30.318324
431.127680	26443.009709	30.323341
431.394405	26485.086148	30.328359
431.702922	26519.935360	30.333376
432.047468	26564.759211	30.338394
432.724199	26616.868522	30.343412
433.379152	26652.755251	30.348429
433.636665	26696.489800	30.353447
433.985537	26735.566011	30.358464
434.518712	26782.576777	30.363482
434.902105	26825.284551	30.368500
435.830542	26864.728845	30.373517
435.856203	26912.486390	30.378535
436.542578	26948.248663	30.383552
437.202603	26989.261273	30.388570
437.493518	27026.666394	30.393588
438.094866	27061.818385	30.398605
438.486406	27102.743206	30.403623
438.770160	27139.654499	30.408640
439.100627	27175.949319	30.413658
439.376583	27223.877652	30.418676
440.227753	27256.253723	30.423693
440.398253	27301.912689	30.428711
440.910544	27346.079894	30.433728
441.686042	27387.162664	30.438746
441.214631	27431.158495	30.443764
442.094106	27475.962423	30.448781
442.676936	27516.982748	30.453799
443.079544	27560.174958	30.458816
443.518485	27604.575780	30.463834
443.863575	27646.219353	30.468852
444.340868	27677.904137	30.473869
444.643071	27728.592953	30.478887
445.007683	27772.785683	30.483904
445.548589	27816.930422	30.488922
445.898609	27870.930412	30.493940
446.799975	27919.523743	30.498957
447.165000	27966.773753	30.503975
446.962989	27999.729299	30.508992
447.849085	28037.426126	30.514010
448.317809	28093.779476	30.519028
448.776789	28137.888113	30.524045
449.015461	28181.762016	30.529063
449.698338	28216.678872	30.534080
450.201919	28256.348070	30.539098
450.641552	28316.035174	30.544116
451.222876	28339.407032	30.549133
451.636258	28378.936855	30.554151
451.869620	28415.038964	30.559168
452.486065	28438.269490	30.564186
452.857444	28497.649881	30.569204
453.241699	28515.947043	30.574221
453.499506	28574.472622	30.579239
453.710968	28619.147130	30.584256
454.461427	28661.183490	30.589274
454.700828	28717.232933	30.594292
455.467138	28750.442929	30.599309
455.663410	28799.597073	30.604327
456.170588	28834.165667	30.609344
456.679757	28880.744408	30.614362
456.844046	28939.681038	30.619380
457.767257	28973.811946	30.624397
457.872158	29019.637699	30.629415
458.208439	29084.587891	30.634432
459.192108	29122.229908	30.639450
459.252773	29173.224746	30.644468
459.978083	29212.966693	30.649485
460.209813	29266.107207	30.654503
460.783600	29313.900507	30.659520
461.538683	29368.002151	30.664538
461.738794	29417.586463	30.669556
462.333759	29447.526095	30.674573
462.842302	29501.798303	30.679591
462.867006	29558.690477	30.684608
463.577593	29598.707063	30.689626
464.278998	29649.764467	30.694644
464.691500	29698.352162	30.699661
465.421469	29735.548465	30.704679
465.570444	29785.735415	30.709696
466.282474	29832.854172	30.714714
466.222692	29890.364006	30.719732
467.106218	29931.797726	30.724749
467.646814	29981.166380	30.729767
467.939231	30029.651818	30.734784
468.341685	30065.666249	30.739802
468.679807	30130.739901	30.744820
469.213458	30168.581689	30.749837
469.694508	30220.585876	30.754855
470.189289	30270.171157	30.759872
470.892174	30312.635829	30.764890
471.595761	30372.904659	30.769908
472.100634	30422.394048	30.774925
472.183924	30464.217014	30.779943
472.598278	30504.915711	30.784960
473.216356	30551.689107	30.789978
473.864272	30610.803724	30.794996
474.365111	30649.951894	30.800013
474.863462	30695.909374	30.805031
475.187508	30750.843846	30.810048
475.917245	30787.985626	30.815066
476.433406	30826.626827	30.820084
476.792909	30869.405236	30.825101
477.154452	30920.443695	30.830119
477.606688	30973.783209	30.835136
478.508721	31013.329612	30.840154
479.048062	31056.346907	30.845172
479.505087	31086.772826	30.850189
479.783834	31145.934552	30.855207
480.057185	31184.818654	30.860224
480.868718	31216.675404	30.865242
480.804170	31275.168666	30.870260
481.103265	31308.299910	30.875277
481.519947	31361.974627	30.880295
481.824372	31408.133283	30.885312
482.616812	31456.943779	30.890330
483.177196	31503.748180	30.895348
483.281914	31547.965034	30.900365
484.076242	31591.528325	30.905383
484.481618	31647.957211	30.910400
485.127434	31682.189783	30.915418
485.361003	31736.763653	30.920436
486.255852	31790.458360	30.925453
486.493793	31823.862583	30.930471
486.868212	31868.856000	30.935488
487.268388	31913.192107	30.940506
487.829910	31974.445993	30.945524
488.170591	32016.687569	30.950541
488.945061	32065.597381	30.955559
489.266515	32125.783973	30.960576
489.670296	32167.226614	30.965594
490.212241	32223.943965	30.970612
490.831182	32277.348176	30.975629
491.149447	32320.632321	30.980647
491.507039	32382.666046	30.985664
492.619971	32429.880023	30.990682
492.898321	32483.448500	30.995700
493.373640	32533.857466	31.000717
494.083564	32574.448908	31.005735
494.319336	32629.223954	31.010752
494.964168	32680.835929	31.015770
494.929288	32731.143707	31.020788
495.737808	32787.825058	31.025805
496.256555	32843.592104	31.030823
496.665435	32902.116515	31.035840
497.213121	32952.091850	31.040858
497.683181	33005.854219	31.045876
498.276596	33060.091764	31.050893
498.853816	33120.163664	31.055911
499.049655	33168.307635	31.060928
500.196425	33212.296240	31.065946
500.376147	33275.429101	31.070964
501.156179	33325.755178	31.075981
501.645750	33367.880657	31.080999
501.884295	33427.586783	31.086016
502.846721	33470.965939	31.091034
503.086376	33523.076571	31.096052
503.724630	33580.233568	31.101069
504.249359	33631.934444	31.106087
504.632355	33684.624561	31.111104
505.183829	33736.258200	31.116122
505.766650	33786.924314	31.121140
505.993364	33841.543640	31.126157
506.632595	33886.365799	31.131175
507.376670	33932.382520	31.136192
507.706501	33975.782378	31.141210
508.287334	34015.085684	31.146228
508.981416	34069.388533	31.151245
509.836131	34126.858593	31.156263
510.027062	34169.669689	31.161280
510.402405	34209.035826	31.166298
510.761810	34265.515330	31.171316
511.157114	34315.570191	31.176333
511.756999	34360.721941	31.181351
512.133692	34425.868071	31.186368
512.634589	34478.547328	31.191386
513.017956	34522.233143	31.196404
513.362940	34588.101482	31.201421
514.031607	34623.866519	31.206439
514.372917	34696.584049	31.211456
514.849135	34757.085269	31.216474
515.267417	34812.635239	31.221492
515.820392	34877.561329	31.226509
516.578156	34928.485755	31.231527
516.764601	34980.347490	31.236544
517.597426	35030.754841	31.241562
517.886212	35081.375437	31.246580
518.444147	35126.968420	31.251597
519.134501	35174.518383	31.256615
519.237818	35232.734888	31.261632
519.818795	35284.677391	31.266650
520.290244	35345.714739	31.271668
520.995461	35405.454375	31.276685
521.364033	35446.165638	31.281703
521.908859	35512.600777	31.286720
522.539882	35576.355067	31.291738
523.295230	35632.909060	31.296756
523.486850	35691.014596	31.301773
524.261770	35749.740223	31.306791
524.456738	35814.448045	31.311808
524.648286	35860.352840	31.316826
525.435667	35928.990181	31.321844
525.422960	36004.226994	31.326861
526.869313	36063.426417	31.331879
527.018409	36132.722466	31.336896
527.655489	36198.046538	31.341914
528.137915	36260.720036	31.346932
528.720190	36333.612602	31.351949
529.544786	36396.425633	31.356967
529.475304	36451.988773	31.361984
529.847313	36504.474352	31.367002
530.873255	36577.243988	31.372020
531.576887	36641.217269	31.377037
532.382031	36704.583768	31.382055
532.186848	36768.305383	31.387072
532.728046	36827.663401	31.392090
533.579692	36896.697780	31.397108
533.818800	36966.667029	31.402125
534.481846	37018.118031	31.407143
535.218245	37095.315397	31.412160
536.395770	37157.387759	31.417178
536.363671	37217.874022	31.422196
537.065931	37284.605249	31.427213
537.824777	37338.525324	31.432231
538.058371	37410.463580	31.437248
538.714304	37470.480172	31.442266
539.592761	37529.484828	31.447284
540.033499	37591.734248	31.452301
540.498687	37646.044714	31.457319
540.979746	37705.415553	31.462336
541.487810	37760.811375	31.467354
542.369390	37823.585203	31.472372
542.633183	37887.679845	31.477389
543.360316	37943.794359	31.482407
543.811733	38007.312315	31.487424
544.214085	38060.573853	31.492442
544.901065	38124.763441	31.497460
545.203480	38185.680502	31.502477
545.847882	38237.147510	31.507495
546.227160	38310.185760	31.512512
546.754515	38367.884472	31.517530
547.483678	38430.388899	31.522548
547.718588	38503.716957	31.527565
548.546392	38566.941000	31.532583
548.786101	38628.523316	31.537600
549.234797	38696.188658	31.542618
550.087422	38756.041207	31.547636
550.679771	38822.117590	31.552653
551.614599	38882.815541	31.557671
552.003248	38938.799727	31.562688
552.316534	39002.618623	31.567706
553.159883	39051.283507	31.572724
553.785512	39109.814273	31.577741
554.426108	39161.663311	31.582759
555.045550	39219.021181	31.587776
554.983260	39261.280126	31.592794
555.658552	39312.385193	31.597812
556.226409	39378.818028	31.602829
556.886652	39436.741186	31.607847
557.184183	39500.138268	31.612864
557.501423	39561.982367	31.617882
558.278725	39623.116052	31.622900
558.465342	39676.083376	31.627917
559.558687	39737.856473	31.632935
559.696672	39803.414951	31.637952
559.791582	39878.422646	31.642970
560.592858	39943.234209	31.647988
560.981629	40024.179109	31.653005
561.457775	40095.731069	31.658023
562.378421	40177.055842	31.663040
562.381808	40250.631221	31.668058
563.687771	40313.217101	31.673076
564.069394	40391.569883	31.678093
564.806573	40454.689157	31.683111
565.446251	40525.113985	31.688128
565.777726	40598.046129	31.693146
566.442306	40661.935776	31.698164
566.638143	40749.731511	31.703181
567.705425	40810.776966	31.708199
568.129956	40891.151508	31.713216
568.678263	40960.087258	31.718234
569.573364	41022.762473	31.723252
570.261515	41101.825218	31.728269
570.888112	41168.112724	31.733287
571.092902	41237.715643	31.738304
571.669575	41308.794753	31.743322
572.419088	41380.151767	31.748340
573.158556	41457.938424	31.753357
573.984462	41528.244708	31.758375
574.606593	41593.164321	31.763392
575.177029	41664.116386	31.768410
575.895456	41713.020505	31.773428
576.224099	41780.363450	31.778445
576.516132	41851.033958	31.783463
577.380589	41910.462288	31.788480
578.363446	41982.929044	31.793498
578.911305	42038.043876	31.798516
579.246870	42102.586474	31.803533
579.996343	42168.623600	31.808551
580.491559	42228.969630	31.813568
580.455838	42297.186123	31.818586
581.235569	42354.975538	31.823604
582.029935	42428.826494	31.828621
582.272097	42496.697807	31.833639
582.889284	42569.000033	31.838656
583.099383	42648.183192	31.843674
584.143668	42713.371538	31.848692
584.459970	42793.522801	31.853709
584.897740	42860.150687	31.858727
585.913568	42934.241688	31.863744
586.107004	43017.565204	31.868762
586.797536	43086.096967	31.873780
587.471731	43157.312245	31.878797
587.868484	43231.074301	31.883815
588.596607	43309.047387	31.888832
588.694647	43390.228726	31.893850
589.243422	43456.489907	31.898868
589.843748	43550.224613	31.903885
590.836073	43625.743068	31.908903
591.618561	43687.593409	31.913920
592.022105	43760.361846	31.918938
592.759409	43826.855210	31.923956
593.298544	43899.585966	31.928973
593.812987	43966.381924	31.933991
594.338078	44035.762319	31.939008
594.646062	44110.316103	31.944026
595.543073	44173.844666	31.949044
595.910153	44256.286125	31.954061
596.640606	44328.229088	31.959079
597.127920	44392.473467	31.964096
597.783489	44473.264125	31.969114
598.616781	44542.178605	31.974132
599.173924	44613.573505	31.979149
599.356892	44698.870224	31.984167
600.054583	44772.645387	31.989184
600.591901	44852.809935	31.994202
601.216031	44934.384544	31.999220
602.020395	45020.921896	32.004237
602.870763	45093.435266	32.009255
603.447915	45170.853746	32.014272
603.842362	45257.453688	32.019290
605.064571	45315.321133	32.024308
605.526112	45390.659788	32.029325
605.969174	45469.203710	32.034343
606.626577	45541.513902	32.039360
607.138894	45625.838266	32.044378
607.971373	45694.943405	32.049396
608.761163	45761.861221	32.054413
609.227889	45830.162144	32.059431
610.125414	45901.840327	32.064448
610.731069	45980.589991	32.069466
611.360171	46052.935241	32.074484
611.754681	46123.475418	32.079501
612.093685	46195.885000	32.084519
612.912802	46269.115407	32.089536
613.536660	46348.940412	32.094554
614.467056	46405.410027	32.099572
615.019219	46489.719014	32.104589
615.417243	46559.110765	32.109607
615.901627	46633.007430	32.114624
616.432483	46722.730453	32.119642
617.186416	46786.285173	32.124660
617.830148	46870.264907	32.129677
618.244864	46948.775438	32.134695
619.288395	47014.664102	32.139712
619.868658	47098.023751	32.144730
620.475806	47164.812523	32.149748
621.247543	47240.940915	32.154765
621.558263	47316.719554	32.159783
622.244974	47386.325516	32.164800
622.657273	47470.917791	32.169818
623.245056	47550.264311	32.174836
623.990493	47625.463808	32.179853
624.408290	47713.252205	32.184871
625.300403	47782.225595	32.189888
625.566572	47869.038679	32.194906
626.352364	47942.631593	32.199924
626.910393	48023.241930	32.204941
627.643886	48106.324823	32.209959
628.578297	48189.160083	32.214976
628.810469	48269.891691	32.219994
629.442500	48351.675481	32.225012
630.344048	48432.957092	32.230029
630.805899	48510.828291	32.235047
631.497635	48589.685036	32.240064
631.981794	48661.284090	32.245082
632.565162	48737.935979	32.250100
633.443826	48811.835853	32.255117
634.144595	48888.705790	32.260135
634.696710	48955.759427	32.265152
635.131829	49029.032380	32.270170
635.613697	49108.759768	32.275188
636.281094	49168.524659	32.280205
636.881532	49265.420636	32.285223
637.648902	49319.970847	32.290240
638.242743	49411.351031	32.295258
638.851834	49488.589112	32.300276
639.675297	49564.733980	32.305293
639.999858	49649.846246	32.310311
640.654192	49720.631493	32.315328
641.046073	49813.837814	32.320346
641.776865	49891.837506	32.325364
642.783565	49968.326349	32.330381
642.895349	50061.403331	32.335399
644.038567	50144.203000	32.340416
644.476691	50233.768293	32.345434
645.220734	50314.597507	32.350452
645.976379	50391.615971	32.355469
646.575418	50483.973196	32.360487
647.345120	50562.746158	32.365504
647.783909	50647.638614	32.370522
648.695907	50716.931947	32.375540
649.474349	50802.962831	32.380557
649.880473	50893.029205	32.385575
650.599587	50965.583424	32.390592
651.129809	51054.859319	32.395610
651.689222	51143.435895	32.400628
652.601398	51217.936425	32.405645
652.867321	51313.366060	32.410663
653.579600	51396.138143	32.415680
654.320840	51484.484036	32.420698
654.878883	51580.757407	32.425716
655.956579	51666.628895	32.430733
656.270707	51759.285702	32.435751
657.047770	51842.503823	32.440768
657.444434	51935.255209	32.445786
658.592028	52021.830582	32.450804
659.237683	52104.768321	32.455821
659.663308	52187.256357	32.460839
660.652092	52281.465562	32.465856
661.293025	52369.971053	32.470874
661.676857	52464.578153	32.475892
662.676143	52547.377138	32.480909
663.099303	52625.773546	32.485927
664.504063	52710.382516	32.490944
664.735673	52792.222881	32.495962
665.211737	52872.570044	32.500980
665.906597	52961.979060	32.505997
666.070871	53058.463849	32.511015
667.346631	53144.277483	32.516032
667.862927	53232.339966	32.521050
668.183823	53324.706122	32.526068
668.861272	53405.786629	32.531085
669.581486	53493.936592	32.536103
670.468067	53588.333263	32.541120
671.205121	53679.147494	32.546138
671.477241	53779.490971	32.551156
672.563304	53854.143380	32.556173
673.085771	53949.688744	32.561191
673.729545	54030.929036	32.566208
674.460630	54130.812964	32.571226
674.997017	54229.604956	32.576244
675.596854	54308.288443	32.581261
676.406884	54412.450860	32.586279
676.866779	54495.909628	32.591296
677.843057	54569.224464	32.596314
678.401529	54662.903404	32.601332
679.262919	54755.054162	32.606349
679.989168	54825.492195	32.611367
680.690645	54902.259378	32.616384
681.004032	54989.883076	32.621402
681.661258	55075.283020	32.626420
682.673810	55163.790153	32.631437
683.391266	55248.056175	32.636455
683.800257	55325.284093	32.641472
683.908819	55412.425415	32.646490
684.542204	55513.640450	32.651508
685.843564	55602.354511	32.656525
686.073812	55699.599532	32.661543
687.139512	55797.098584	32.666560
687.935830	55884.677934	32.671578
688.167253	55990.233400	32.676596
689.400444	56082.878560	32.681613
689.787538	56174.583592	32.686631
690.267441	56268.927638	32.691648
690.679537	56362.929486	32.696666
691.463020	56465.344089	32.701684
692.308029	56566.099777	32.706701
692.923707	56672.429396	32.711719
693.722091	56767.809990	32.716736
694.043734	56876.906540	32.721754
694.643642	56986.172503	32.726772
695.911933	57088.623847	32.731789
696.029297	57205.187332	32.736807
696.966022	57307.403963	32.741824
697.852363	57408.972244	32.746842
698.660201	57508.797260	32.751860
699.587227	57622.853174	32.756877
700.125245	57711.633387	32.761895
700.703668	57812.831254	32.766912
701.721227	57926.760169	32.771930
702.157316	58026.080504	32.776948
702.892923	58128.770633	32.781965
704.159942	58231.493448	32.786983
704.316682	58333.073348	32.792000
705.373689	58426.649571	32.797018
706.033010	58533.051346	32.802036
706.894015	58641.234064	32.807053
707.634236	58734.086801	32.812071
708.304343	58839.369822	32.817088
709.018763	58937.068672	32.822106
709.373604	59036.262069	32.827124
710.596207	59123.759779	32.832141
711.378665	59230.125899	32.837159
711.985841	59328.331010	32.842176
712.798640	59434.522548	32.847194
713.326119	59533.102070	32.852212
714.335365	59624.056329	32.857229
715.066835	59723.020148	32.862247
715.573936	59817.268902	32.867264
716.546186	59906.827503	32.872282
716.865993	60014.146440	32.877300
718.075967	60107.420737	32.882317
718.658805	60200.596960	32.887335
719.400999	60302.077248	32.892352
720.345042	60401.590667	32.897370
720.465576	60500.747819	32.902388
721.345284	60589.844401	32.907405
722.081833	60690.291033	32.912423
722.875055	60782.202658	32.917440
723.571973	60880.109688	32.922458
723.844352	60985.829896	32.927476
724.952868	61080.016612	32.932493
725.594014	61169.262636	32.937511
726.319462	61259.184038	32.942528
726.662417	61355.483293	32.947546
727.525225	61441.261802	32.952564
728.223372	61540.701364	32.957581
729.140093	61638.948583	32.962599
729.877430	61722.410407	32.967616
731.150558	61799.564426	32.972634
732.045798	61897.241260	32.977652
732.499849	61979.417329	32.982669
732.797431	62069.874479	32.987687
733.359396	62169.630372	32.992704
734.317138	62271.255443	32.997722
734.413075	62371.841581	33.002740
735.395063	62464.759829	33.007757
736.041542	62576.096155	33.012775
736.771469	62681.243743	33.017792
737.581756	62782.800919	33.022810
738.076810	62893.822679	33.027828
738.983508	62999.821268	33.032845
739.976653	63112.866711	33.037863
740.501491	63215.117981	33.042880
741.451992	63318.177980	33.047898
741.784559	63434.115741	33.052916
742.678018	63539.392358	33.057933
743.084583	63649.054796	33.062951
743.849797	63771.882536	33.067968
744.948419	63879.680732	33.072986
745.666967	64004.217994	33.078004
746.018188	64110.162447	33.083021
746.837614	64226.131566	33.088039
747.663657	64346.013199	33.093056
748.351008	64463.718598	33.098074
749.011229	64585.866840	33.103092
750.049126	64695.417730	33.108109
751.093734	64810.183376	33.113127
751.320406	64930.964041	33.118144
752.562079	65045.957575	33.123162
753.517591	65169.722986	33.128180
754.081906	65277.250155	33.133197
754.988489	65384.051158	33.138215
755.235657	65503.251307	33.143232
756.432322	65609.626173	33.148250
757.094180	65732.552118	33.153268
758.009810	65843.608573	33.158285
758.853763	65957.907970	33.163303
759.533400	66075.851323	33.168320
760.564833	66180.574786	33.173338
761.273555	66290.333896	33.178356
761.898015	66403.660507	33.183373
762.458452	66514.551674	33.188391
763.066436	66626.908614	33.193408
764.323756	66743.002612	33.198426
765.226958	66864.788891	33.203444
765.897466	66973.710717	33.208461
766.220291	67083.044662	33.213479
766.969380	67200.224163	33.218496
768.255514	67303.937460	33.223514
768.562597	67422.879368	33.228532
769.648316	67534.966133	33.233549
770.089156	67658.477293	33.238567
771.060948	67772.322828	33.243584
772.172567	67876.902370	33.248602
772.884564	67997.639343	33.253620
773.525366	68110.624681	33.258637
774.388592	68208.349039	33.263655
775.116434	68331.519489	33.268672
776.076490	68433.566187	33.273690
776.395112	68536.174708	33.278708
777.423380	68639.463005	33.283725
778.036745	68742.320935	33.288743
778.831854	68848.481404	33.293760
779.776058	68945.114564	33.298778
780.570067	69057.599063	33.303796
780.873010	69160.756951	33.308813
781.794506	69263.307193	33.313831
782.434386	69376.950670	33.318848
783.214897	69489.408064	33.323866
783.968619	69601.301412	33.328884
784.653205	69717.051184	33.333901
785.248921	69835.326540	33.338919
785.941933	69956.577284	33.343936
787.264449	70075.720157	33.348954
787.665515	70191.993628	33.353972
788.409924	70309.064572	33.358989
789.307063	70424.245536	33.364007
789.911557	70560.481453	33.369024
790.888920	70670.085980	33.374042
791.764976	70796.572192	33.379060
792.603561	70921.218917	33.384077
793.489126	71033.793504	33.389095
794.111358	71167.848753	33.394112
794.729787	71286.046135	33.399130
795.671039	71416.294006	33.404148
796.332578	71531.330159	33.409165
797.660633	71653.592057	33.414183
798.098067	71785.765657	33.419200
799.184098	71907.955202	33.424218
799.712460	72028.264678	33.429236
800.659736	72157.763499	33.434253
801.334827	72276.968726	33.439271
801.963448	72403.157466	33.444288
803.147385	72533.220149	33.449306
803.791244	72662.120809	33.454324
804.815493	72787.961773	33.459341
805.800670	72910.540437	33.464359
806.457910	73035.684661	33.469376
807.457283	73143.179544	33.474394
808.416178	73264.600927	33.479412
809.047331	73397.251891	33.484429
810.038888	73515.494567	33.489447
810.653403	73642.609825	33.494464
811.754494	73760.380369	33.499482
812.815016	73877.317134	33.504500
813.322808	74000.037798	33.509517
813.935394	74113.438747	33.514535
814.810781	74251.721087	33.519552
815.876687	74367.261895	33.524570
816.553487	74494.397095	33.529588
817.311889	74612.115061	33.534605
818.102004	74732.731355	33.539623
818.682034	74861.529053	33.544640
819.605266	74985.672779	33.549658
820.497524	75106.773871	33.554676
821.026317	75253.145758	33.559693
822.062128	75370.619511	33.564711
822.682069	75509.457983	33.569728
823.748703	75633.752410	33.574746
824.237458	75758.465679	33.579764
825.141866	75888.113839	33.584781
826.390285	76018.477496	33.589799
826.895858	76144.796675	33.594816
827.874796	76259.590155	33.599834
828.784930	76394.053604	33.604852
829.186885	76530.796696	33.609869
830.437465	76644.800891	33.614887
830.859514	76772.573242	33.619904
831.819915	76894.665887	33.624922
832.638671	77004.847082	33.629940
833.311427	77129.740029	33.634957
834.023263	77247.334242	33.639975
834.800157	77378.346815	33.644992
835.633398	77503.455671	33.650010
836.611820	77634.499669	33.655028
836.936772	77758.017809	33.660045
838.007963	77879.888789	33.665063
838.464444	78026.822241	33.670080
839.437241	78161.931187	33.675098
840.368512	78290.115061	33.680116
841.125962	78429.891510	33.685133
842.294978	78574.541042	33.690151
842.773903	78716.009990	33.695168
843.837625	78851.025814	33.700186
844.845596	78988.651533	33.705204
845.416712	79120.549642	33.710221
846.543995	79257.663865	33.715239
847.315386	79397.437694	33.720256
847.986062	79539.847950	33.725274
849.203623	79679.442194	33.730292
849.688462	79832.658034	33.735309
850.498369	79959.283671	33.740327
851.068791	80107.489697	33.745344
851.987855	80257.967019	33.750362
853.243478	80404.834409	33.755380
853.756304	80566.780598	33.760397
854.755650	80713.091384	33.765415
855.598498	80853.140728	33.770432
856.486189	81000.401784	33.775450
857.228622	81154.811236	33.780468
858.196262	81296.000378	33.785485
859.085010	81444.409196	33.790503
859.872497	81603.002297	33.795520
860.642769	81737.210800	33.800538
861.985669	81889.115523	33.805556
862.910893	82037.414608	33.810573
863.893397	82190.431143	33.815591
864.660157	82325.345925	33.820608
865.657116	82476.508275	33.825626
866.537636	82619.826775	33.830644
867.296717	82774.731556	33.835661
868.430484	82918.301063	33.840679
869.122215	83068.062620	33.845696
869.910712	83207.262247	33.850714
870.726541	83354.891967	33.855732
871.556756	83507.335064	33.860749
872.521306	83653.189528	33.865767
873.226014	83794.057894	33.870784
874.020768	83949.932698	33.875802
875.148702	84091.201080	33.880820
876.066351	84261.521441	33.885837
876.905035	84397.493077	33.890855
877.813687	84547.810436	33.895872
878.418662	84696.401025	33.900890
879.537220	84850.804687	33.905908
880.366651	85004.352376	33.910925
881.199287	85153.211941	33.915943
882.104990	85305.154491	33.920960
882.708620	85456.451964	33.925978
883.842137	85613.882740	33.930996
884.546782	85772.720621	33.936013
885.626546	85912.255279	33.941031
886.338995	86070.821803	33.946048
886.938119	86229.136049	33.951066
887.909720	86382.574355	33.956084
888.801161	86531.989800	33.961101
889.435551	86678.556894	33.966119
890.480396	86828.904354	33.971136
891.204803	86972.275477	33.976154
892.179024	87108.645436	33.981172
893.069795	87281.074102	33.986189
894.158188	87424.457385	33.991207
894.945742	87575.073629	33.996224
896.010510	87720.936886	34.001242
897.094492	87876.005296	34.006260
897.791749	88030.752659	34.011277
898.610670	88174.102779	34.016295
899.526037	88326.955506	34.021312
900.201322	88488.727519	34.026330
901.422224	88631.767117	34.031348
902.061917	88792.344695	34.036365
903.099626	88949.794577	34.041383
903.951996	89110.307481	34.046400
904.643711	89270.620206	34.051418
905.960223	89420.477180	34.056436
906.528280	89588.969982	34.061453
907.511226	89750.022500	34.066471
908.649328	89914.664115	34.071488
909.383329	90069.766695	34.076506
910.503318	90235.666591	34.081524
911.375786	90400.178257	34.086541
912.090019	90560.970538	34.091559
912.824308	90733.696858	34.096576
913.763230	90901.890701	34.101594
914.970646	91070.743830	34.106612
915.731805	91243.013662	34.111629
916.607780	91407.791105	34.116647
917.997504	91568.225219	34.121664
918.742542	91738.899979	34.126682
920.002325	91902.446420	34.131700
920.627530	92066.915375	34.136717
921.756457	92234.473111	34.141735
922.909246	92394.743002	34.146752
923.406619	92568.812754	34.151770
924.484595	92721.831055	34.156788
925.805359	92898.855747	34.161805
926.785511	93054.803860	34.166823
927.542540	93217.480184	34.171840
928.120960	93377.465407	34.176858
929.491219	93540.865313	34.181876
930.344522	93709.504141	34.186893
931.292905	93875.159772	34.191911
932.101474	94036.250573	34.196928
932.850166	94201.181852	34.201946
934.144488	94363.719946	34.206964
935.057815	94540.127572	34.211981
935.761987	94709.937289	34.216999
936.765125	94869.716384	34.222016
937.891192	95032.660173	34.227034
938.978871	95195.427811	34.232052
939.905516	95361.964229	34.237069
940.476006	95525.066430	34.242087
941.668915	95683.129242	34.247104
942.620371	95850.095281	34.252122
943.374435	96010.821802	34.257140
944.149399	96188.143932	34.262157
945.101770	96349.099382	34.267175
946.442466	96503.021911	34.272192
946.902380	96682.760881	34.277210
948.123825	96861.476284	34.282228
948.984828	97031.446828	34.287245
949.842462	97196.348310	34.292263
951.160929	97357.401637	34.297280
951.631518	97522.837729	34.302298
952.767556	97679.346239	34.307316
953.385208	97846.349137	34.312333
954.313907	98016.650673	34.317351
955.374558	98170.933616	34.322368
955.918255	98342.345595	34.327386
956.979016	98491.508829	34.332404
957.687982	98673.867134	34.337421
958.883613	98843.971828	34.342439
960.021608	99013.795969	34.347456
960.866860	99187.139069	34.352474
961.630552	99364.694351	34.357492
962.390258	99542.922631	34.362509
963.690316	99715.845911	34.367527
964.884565	99886.597258	34.372544
965.644570	100071.616254	34.377562
966.349596	100237.563106	34.382580
967.149975	100425.078847	34.387597
968.215685	100605.270973	34.392615
969.369922	100793.971852	34.397632
969.990056	100982.825752	34.402650
971.268023	101165.911863	34.407668
972.348716	101354.236459	34.412685
972.934580	101542.201041	34.417703
974.348841	101722.545968	34.422720
974.985800	101915.367543	34.427738
976.221423	102107.357074	34.432756
977.166801	102302.163025	34.437773
978.270226	102488.586248	34.442791
979.497632	102667.651629	34.447808
980.251770	102858.396634	34.452826
981.265183	103043.730629	34.457844
982.338694	103227.738941	34.462861
983.067666	103419.112749	34.467879
984.192738	103604.799527	34.472896
985.354760	103797.294937	34.477914
986.503426	103986.627858	34.482932
987.613643	104176.019162	34.487949
988.408339	104358.219837	34.492967
989.834296	104545.446602	34.497984
990.551611	104738.668350	34.503002
991.166941	104922.042418	34.508020
992.537412	105112.473943	34.513037
993.230950	105299.966490	34.518055
994.306158	105480.178110	34.523072
995.540524	105678.893908	34.528090
996.251397	105877.913068	34.533108
997.518682	106060.617277	34.538125
998.440490	106264.974605	34.543143
999.677108	106442.050342	34.548160
1000.614678	106638.263931	34.553178
1001.570740	106822.506719	34.558196
1002.780464	107015.511628	34.563213
1003.672294	107213.940873	34.568231
1004.795874	107401.972414	34.573248
1005.819526	107591.706397	34.578266
1006.629840	107779.995043	34.583284
1008.064642	107958.580660	34.588301
1008.768894	108164.204423	34.593319
1010.134522	108325.336901	34.598336
1010.974980	108525.810961	34.603354
1012.255124	108710.557770	34.608372
1013.413356	108883.317895	34.613389
1014.203897	109071.960824	34.618407
1015.378812	109246.734538	34.623424
1016.159431	109429.174789	34.628442
1017.161461	109616.266485	34.633460
1018.448841	109796.788677	34.638477
1019.233424	109973.810360	34.643495
1020.400197	110132.592338	34.648512
1021.289210	110311.081021	34.653530
1021.999349	110476.451563	34.658548
1023.155743	110653.479506	34.663565
1023.598530	110837.619143	34.668583
1024.773347	111012.176156	34.673600
1025.818923	111203.958581	34.678618
1026.525174	111389.451812	34.683636
1027.961986	111581.007490	34.688653
1028.345342	111768.279508	34.693671
1029.570009	111949.573651	34.698688
1030.665295	112148.701972	34.703706
1031.301272	112341.016075	34.708724
1032.493452	112537.964880	34.713741
1033.134829	112734.220703	34.718759
1034.587997	112944.887285	34.723776
1035.192420	113144.775343	34.728794
1036.547985	113348.075239	34.733812
1037.500850	113548.199955	34.738829
1038.586951	113757.007683	34.743847
1039.930299	113968.358930	34.748864
1040.745116	114167.294658	34.753882
1041.791472	114375.480099	34.758900
1043.463258	114570.425523	34.763917
1044.084629	114782.396369	34.768935
1045.831737	114979.802718	34.773952
1046.523930	115183.707025	34.778970
1047.585422	115384.346294	34.783988
1048.755084	115584.094881	34.789005
1049.611530	115796.477895	34.794023
1050.821889	115989.938324	34.799040
1052.085974	116196.023277	34.804058
1053.110939	116399.285792	34.809076
1054.161724	116597.452032	34.814093
1055.041696	116805.606799	34.819111
1055.834603	117011.243382	34.824128
1057.105898	117216.257508	34.829146
1058.202362	117425.635367	34.834164
1059.480102	117630.942812	34.839181
1060.320553	117835.817189	34.844199
1061.531091	118050.160362	34.849216
1062.880384	118255.156320	34.854234
1063.702363	118463.662112	34.859252
1064.629230	118659.176763	34.864269
1066.103823	118864.092958	34.869287
1067.179147	119067.822147	34.874304
1067.730994	119283.183009	34.879322
1068.975736	119491.524906	34.884340
1070.156189	119699.017247	34.889357
1070.867915	119914.191597	34.894375
1072.162188	120128.396857	34.899392
1073.458913	120336.013879	34.904410
1074.557319	120546.174216	34.909428
1075.772399	120751.894203	34.914445
1076.911916	120964.293689	34.919463
1077.903844	121158.040176	34.924480
1078.956349	121368.720856	34.929498
1079.886695	121574.683737	34.934516
1081.178198	121777.483568	34.939533
1082.147230	122000.829733	34.944551
1083.266278	122194.257833	34.949568
1084.265544	122404.713887	34.954586
1085.334856	122622.015878	34.959604
1086.718523	122828.140600	34.964621
1087.827182	123039.368764	34.969639
1088.815072	123244.725366	34.974656
1089.917921	123439.266767	34.979674
1090.432466	123638.684534	34.984692
1091.942863	123831.551581	34.989709
1092.504094	124043.929204	34.994727
1093.756628	124234.053290	34.999744
1094.680002	124443.509621	35.004762
1095.657446	124643.985451	35.009780
1097.100519	124847.630123	35.014797
1097.652157	125061.740108	35.019815
1099.050103	125268.234017	35.024832
1099.893858	125479.383622	35.029850
1100.870413	125698.915713	35.034868
1102.281016	125901.926419	35.039885
1103.497987	126129.774196	35.044903
1104.388196	126340.630554	35.049920
1105.689283	126548.822150	35.054938
1106.476555	126768.101673	35.059956
1107.949460	126993.150469	35.064973
1109.067169	127216.358409	35.069991
1109.962887	127431.201205	35.075008
1111.187487	127640.046551	35.080026
1112.275391	127869.855117	35.085044
1113.783725	128079.670519	35.090061
1114.988791	128308.132062	35.095079
1115.676733	128530.900815	35.100096
1116.887431	128749.008901	35.105114
1117.789008	128977.119895	35.110132
1119.066868	129206.082985	35.115149
1120.243327	129426.597136	35.120167
1121.165822	129655.229301	35.125184
1122.505288	129878.850593	35.130202
1123.124929	130114.482538	35.135220
1124.524255	130343.738036	35.140237
1125.849850	130583.287751	35.145255
1126.936783	130817.630758	35.150272
1128.263080	131039.056746	35.155290
1129.001878	131275.324099	35.160308
1130.400028	131506.768523	35.165325
1131.170037	131743.515885	35.170343
1132.564213	131979.971656	35.175360
1133.486831	132224.594936	35.180378
1134.737444	132452.761930	35.185396
1136.266539	132686.614504	35.190413
1137.115036	132926.324012	35.195431
1138.243441	133169.956980	35.200448
1139.198770	133395.415819	35.205466
1140.468056	133638.788150	35.210484
1141.691641	133881.675435	35.215501
1143.033404	134124.101279	35.220519
1144.154286	134357.615016	35.225536
1145.525503	134594.778258	35.230554
1146.481784	134835.485538	35.235572
1147.882626	135068.970737	35.240589
1149.247431	135307.154417	35.245607
1150.256445	135547.224283	35.250624
1151.209133	135795.672818	35.255642
1152.342151	136018.445217	35.260660
1153.806983	136248.251470	35.265677
1154.657904	136485.501633	35.270695
1155.812917	136730.373742	35.275712
1157.269456	136959.235382	35.280730
1158.443885	137197.438740	35.285748
1159.391824	137434.147094	35.290765
1160.474672	137667.855271	35.295783
1161.597021	137906.985155	35.300800
1162.818496	138136.413523	35.305818
1163.559549	138398.698556	35.310836
1164.785693	138627.660357	35.315853
1166.152417	138861.177714	35.320871
1167.189908	139103.322411	35.325888
1168.499144	139330.779041	35.330906
1169.576613	139548.664352	35.335924
1170.816384	139770.784600	35.340941
1171.952859	140005.818706	35.345959
1173.020813	140231.736243	35.350976
1174.133800	140465.217753	35.355994
1175.290146	140703.499415	35.361012
1176.327850	140918.775226	35.366029
1177.521510	141172.396905	35.371047
1178.593526	141414.945283	35.376064
1179.891494	141637.879485	35.381082
1180.881872	141894.405811	35.386100
1182.299808	142128.596270	35.391117
1183.387628	142364.757648	35.396135
1184.565032	142614.841940	35.401152
1185.983139	142856.696411	35.406170
1186.802667	143109.709254	35.411188
1188.490384	143353.348623	35.416205
1189.364492	143591.607895	35.421223
1190.380338	143847.307324	35.426240
1192.314431	144088.552332	35.431258
1192.895694	144344.073553	35.436276
1194.250274	144587.890610	35.441293
1195.722765	144836.369329	35.446311
1196.849938	145089.015703	35.451328
1197.888299	145323.771964	35.456346
1199.096203	145585.881726	35.461364
1200.274258	145841.124746	35.466381
1201.460230	146092.817309	35.471399
1202.751641	146348.083219	35.476416
1204.277099	146595.449303	35.481434
1205.408455	146858.646243	35.486452
1206.755373	147104.536116	35.491469
1207.755961	147365.805254	35.496487
1208.626106	147623.508670	35.501504
1210.013229	147874.051550	35.506522
1211.223492	148134.352992	35.511540
1212.606052	148406.942767	35.516557
1213.896115	148666.093320	35.521575
1214.554333	148926.339402	35.526592
1216.333351	149188.076201	35.531610
1217.408922	149444.325178	35.536628
1218.596058	149718.085687	35.541645
1219.964998	149974.885923	35.546663
1220.946068	150237.129795	35.551680
1222.338524	150504.989700	35.556698
1223.325174	150767.718321	35.561716
1224.870521	151038.765691	35.566733
1226.117143	151297.256726	35.571751
1226.698706	151569.913154	35.576768
1228.488241	151827.988279	35.581786
1229.990071	152107.637495	35.586804
1231.060397	152365.251670	35.591821
1232.145419	152625.668355	35.596839
1233.605032	152893.292983	35.601856
1234.898102	153158.701865	35.606874
1236.102458	153415.996497	35.611892
1237.379631	153684.164142	35.616909
1238.899170	153947.245095	35.621927
1239.864876	154208.402503	35.626944
1241.578686	154464.846105	35.631962
1242.623350	154742.928246	35.636980
1243.639606	154997.968455	35.641997
1244.976512	155249.545038	35.647015
1245.989529	155522.449739	35.652032
1247.634740	155787.691433	35.657050
1248.949269	156041.826492	35.662068
1249.711272	156287.580668	35.667085
1251.353173	156530.996336	35.672103
1252.415588	156778.923842	35.677120
1253.876876	157017.501083	35.682138
1254.875128	157270.871685	35.687156
1256.031289	157519.929991	35.692173
1257.582964	157760.564486	35.697191
1258.514916	158015.396915	35.702208
1259.702660	158265.241125	35.707226
1260.614135	158533.210213	35.712244
1262.040220	158790.312759	35.717261
1263.582782	159051.520705	35.722279
1264.361844	159312.361750	35.727296
1265.799789	159575.810440	35.732314
1266.889887	159842.769040	35.737332
1267.999592	160104.131345	35.742349
1269.392590	160378.947083	35.747367
1270.106454	160662.719557	35.752384
1271.767934	160933.130345	35.757402
1273.071549	161210.732084	35.762420
1274.155868	161499.067052	35.767437
1275.329430	161768.193690	35.772455
1276.558910	162062.420712	35.777472
1278.017685	162343.176080	35.782490
1279.134737	162626.400388	35.787508
1280.443666	162918.146196	35.792525
1281.817451	163208.043594	35.797543
1283.053500	163500.198743	35.802560
1283.762568	163791.275717	35.807578
1285.737553	164092.942724	35.812596
1286.769562	164395.782729	35.817613
1288.156317	164683.315304	35.822631
1289.066098	164983.312141	35.827648
1290.654360	165281.930093	35.832666
1292.363124	165583.575342	35.837684
1293.375958	165872.002293	35.842701
1294.923613	166176.304723	35.847719
1296.292135	166481.945772	35.852736
1297.782884	166774.423390	35.857754
1299.189768	167075.811532	35.862772
1300.455379	167362.861430	35.867789
1301.891975	167653.780375	35.872807
1302.969172	167953.300230	35.877824
1304.730386	168246.643700	35.882842
1305.932230	168540.804806	35.887860
1307.100618	168843.652721	35.892877
1308.437549	169134.673826	35.897895
1309.398852	169429.134227	35.902912
1310.744795	169734.737676	35.907930
1312.491220	170030.468015	35.912948
1313.396091	170328.280843	35.917965
1315.210003	170624.612939	35.922983
1316.232217	170927.295737	35.928000
1317.818767	171219.532364	35.933018
1319.247602	171517.380433	35.938036
1320.430371	171821.514522	35.943053
1322.091414	172106.536484	35.948071
1323.124363	172397.856751	35.953088
1324.710136	172698.579706	35.958106
1326.255581	172994.742736	35.963124
1327.080519	173286.851564	35.968141
1328.547248	173574.274863	35.973159
1329.810597	173881.073823	35.978176
1331.234216	174164.231080	35.983194
1332.677542	174455.077276	35.988212
1333.724807	174759.062130	35.993229
1335.523519	175046.794672	35.998247
1336.959432	175341.987656	36.003264
1337.869258	175620.618829	36.008282
1339.341232	175905.770701	36.013300
1340.563349	176176.510352	36.018317
1342.078947	176444.791659	36.023335
1342.934381	176729.542529	36.028352
1344.554059	177014.473313	36.033370
1345.712150	177292.324066	36.038388
1346.849013	177580.574170	36.043405
1348.012672	177861.752314	36.048423
1349.157216	178155.512558	36.053440
1350.359794	178454.100441	36.058458
1351.844815	178752.313413	36.063476
1352.928484	179066.510006	36.068493
1354.325523	179374.183863	36.073511
1355.635369	179685.237345	36.078528
1356.818248	179994.511410	36.083546
1358.181482	180311.030104	36.088564
1359.099708	180637.676496	36.093581
1360.433717	180953.099690	36.098599
1361.711609	181270.425215	36.103616
1363.140770	181604.633984	36.108634
1364.281309	181931.023196	36.113652
1365.622913	182259.691234	36.118669
1367.359910	182586.848985	36.123687
1368.833365	182928.826657	36.128704
1370.188493	183263.718062	36.133722
1371.661489	183594.339934	36.138740
1373.097011	183930.884943	36.143757
1374.861252	184270.436732	36.148775
1376.215323	184614.818340	36.153792
1377.420554	184933.104032	36.158810
1378.666571	185267.137198	36.163828
1380.061821	185601.833150	36.168845
1381.405961	185931.157529	36.173863
1383.055568	186283.269018	36.178880
1384.346369	186626.454925	36.183898
1386.133943	186959.405867	36.188916
1386.872048	187301.595532	36.193933
1388.323094	187641.714573	36.198951
1389.721657	188008.641147	36.203968
1391.029387	188363.576543	36.208986
1392.581404	188718.143691	36.214004
1394.062893	189069.144900	36.219021
1395.050581	189411.686600	36.224039
1396.416790	189773.640786	36.229056
1397.661343	190120.815647	36.234074
1399.455856	190482.144816	36.239092
1401.035909	190838.154517	36.244109
1402.265169	191183.763945	36.249127
1403.776181	191546.631620	36.254144
1404.998144	191905.588465	36.259162
1406.558219	192262.460370	36.264180
1408.037661	192622.826071	36.269197
1409.605629	192971.169805	36.274215
1411.229637	193326.082258	36.279232
1411.978245	193688.974271	36.284250
1413.186248	194048.897959	36.289268
1415.043146	194411.204736	36.294285
1416.710562	194764.607381	36.299303
1418.246956	195130.589379	36.304320
1419.324731	195486.429393	36.309338
1420.723888	195839.082458	36.314356
1422.094999	196212.664433	36.319373
1423.952577	196563.950713	36.324391
1425.262779	196923.251468	36.329408
1426.378635	197291.435273	36.334426
1427.806128	197643.763238	36.339444
1429.331593	198002.958073	36.344461
1431.168848	198355.069708	36.349479
1432.486979	198684.936548	36.354496
1433.459755	199030.986154	36.359514
1435.137094	199376.730639	36.364532
1436.341104	199722.605859	36.369549
1437.347071	200061.189745	36.374567
1439.242906	200414.648065	36.379584
1440.538432	200774.542899	36.384602
1442.244005	201114.869947	36.389620
1443.336169	201475.347898	36.394637
1444.741175	201831.624166	36.399655
1446.419033	202201.074392	36.404672
1447.356404	202552.479774	36.409690
1448.835592	202913.027921	36.414708
1449.896114	203297.288657	36.419725
1451.474780	203655.005290	36.424743
1453.112898	204025.245788	36.429760
1454.220569	204408.933113	36.434778
1455.867816	204780.229686	36.439796
1457.051534	205167.514286	36.444813
1458.663324	205547.670424	36.449831
1460.406256	205932.225447	36.454848
1461.789222	206318.225876	36.459866
1463.469373	206699.201697	36.464884
1464.835881	207096.153897	36.469901
1466.119629	207477.656086	36.474919
1467.877796	207860.262586	36.479936
1469.201287	208256.351521	36.484954
1470.659758	208636.751026	36.489972
1472.519000	209027.523703	36.494989
1473.626215	209419.438327	36.500007
1475.738011	209805.360446	36.505024
1477.058138	210208.836836	36.510042
1478.795660	210589.237271	36.515060
1480.057057	210985.870105	36.520077
1481.630254	211377.983489	36.525095
1483.218476	211769.639032	36.530112
1484.539198	212166.902392	36.535130
1486.434832	212555.869408	36.540148
1487.905540	212950.952790	36.545165
1489.089981	213338.313750	36.550183
1491.064016	213727.958627	36.555200
1492.314923	214109.495975	36.560218
1493.884015	214503.884148	36.565236
1495.582107	214907.268755	36.570253
1497.104705	215303.623598	36.575271
1498.652652	215679.556253	36.580288
1499.897890	216084.112815	36.585306
1501.496024	216472.662952	36.590324
1502.940664	216858.547830	36.595341
1504.324639	217250.133405	36.600359
1506.280601	217647.340598	36.605376
1507.930576	218045.869840	36.610394
1509.239157	218432.824644	36.615412
1510.932389	218824.416070	36.620429
1512.352759	219213.057051	36.625447
1514.302558	219593.586059	36.630464
1515.386126	219983.911072	36.635482
1516.950211	220378.069541	36.640500
1518.197831	220779.749019	36.645517
1519.957147	221172.633602	36.650535
1521.701563	221557.013380	36.655552
1523.118919	221948.001513	36.660570
1524.680867	222343.462791	36.665588
1525.935078	222730.924719	36.670605
1527.306418	223124.159676	36.675623
1528.853524	223519.475092	36.680640
1530.386815	223914.286141	36.685658
1532.143042	224279.344083	36.690676
1533.358921	224669.536557	36.695693
1534.841779	225061.845169	36.700711
1536.211536	225479.446633	36.705728
1537.165754	225874.842376	36.710746
1538.888130	226260.968434	36.715764
1540.296549	226643.108921	36.720781
1541.491892	227040.576684	36.725799
1543.247845	227432.720583	36.730816
1544.141479	227840.654754	36.735834
1545.634008	228236.984826	36.740852
1547.266364	228660.090515	36.745869
1548.828480	229077.112975	36.750887
1550.255672	229487.885017	36.755904
1552.180426	229916.331181	36.760922
1553.852453	230318.860742	36.765940
1555.449637	230734.510652	36.770957
1556.759757	231171.825395	36.775975
1558.249505	231592.702668	36.780992
1559.585940	232014.292270	36.786010
1561.265261	232446.571080	36.791028
1562.764857	232882.563961	36.796045
1564.469418	233314.002738	36.801063
1566.112388	233744.716203	36.806080
1567.269497	234191.107561	36.811098
1569.046690	234624.493688	36.816116
1570.484199	235074.092448	36.821133
1572.072758	235514.802237	36.826151
1573.927145	235952.751222	36.831168
1575.433273	236407.015944	36.836186
1577.032624	236851.893106	36.841204
1579.187586	237302.648975	36.846221
1580.676334	237746.555830	36.851239
1582.198762	238191.474207	36.856256
1583.601422	238646.167753	36.861274
1585.424403	239087.151926	36.866292
1587.108315	239527.982187	36.871309
1588.718031	239982.060175	36.876327
1590.487289	240428.746082	36.881344
1591.690147	240879.895649	36.886362
1593.456174	241325.923388	36.891380
1595.279160	241771.409106	36.896397
1596.901393	242237.885849	36.901415
1598.592861	242679.000307	36.906432
1599.983660	243139.902987	36.911450
1601.836709	243581.551135	36.916468
1603.525234	244033.337434	36.921485
1605.006021	244486.149483	36.926503
1606.797307	244934.897313	36.931520
1608.280922	245392.638418	36.936538
1610.066720	245832.751538	36.941556
1612.056920	246288.657463	36.946573
1613.235412	246741.167108	36.951591
1615.260470	247181.140878	36.956608
1616.876257	247639.676135	36.961626
1618.521287	248076.335172	36.966644
1620.083324	248521.645427	36.971661
1621.474676	248983.877375	36.976679
1623.535065	249427.785317	36.981696
1625.329539	249870.467476	36.986714
1627.035439	250309.836879	36.991732
1628.868043	250754.494994	36.996749
1630.257136	251191.427991	37.001767
1632.103024	251624.246770	37.006784
1633.797747	252070.478314	37.011802
1635.536197	252506.389255	37.016820
1637.010376	252939.981637	37.021837
1638.640071	253374.793346	37.026855
1640.103367	253787.760599	37.031872
1641.626278	254218.373460	37.036890
1643.331396	254627.439861	37.041908
1645.097505	255043.507650	37.046925
1646.538361	255460.975692	37.051943
1647.984631	255879.459104	37.056960
1649.461273	256316.456613	37.061978
1651.097338	256740.370598	37.066996
1652.764786	257162.069394	37.072013
1653.926338	257601.100662	37.077031
1655.780002	258020.761942	37.082048
1657.222201	258470.390906	37.087066
1658.890217	258911.396255	37.092084
1660.646933	259350.964352	37.097101
1662.057034	259808.803836	37.102119
1663.955330	260253.683141	37.107136
1665.364016	260705.959391	37.112154
1666.742522	261155.827208	37.117172
1668.765323	261618.391718	37.122189
1670.080204	262091.361333	37.127207
1671.611036	262557.944268	37.132224
1673.346525	263027.312945	37.137242
1675.016609	263493.745411	37.142260
1676.773907	263964.405547	37.147277
1678.531005	264451.933147	37.152295
1680.279053	264918.758308	37.157312
1681.952952	265398.119139	37.162330
1683.427401	265875.200845	37.167348
1685.381181	266358.147297	37.172365
1686.688756	266849.506859	37.177383
1688.254796	267325.987846	37.182400
1690.149072	267823.600264	37.187418
1691.478967	268314.192505	37.192436
1693.931201	268796.037978	37.197453
1695.187161	269295.786327	37.202471
1697.273963	269790.036768	37.207488
1699.056990	270291.271701	37.212506
1700.559799	270776.650022	37.217524
1702.474577	271269.936071	37.222541
1703.842124	271766.969753	37.227559
1705.823617	272270.404325	37.232576
1707.747106	272765.286925	37.237594
1709.215845	273270.100011	37.242612
1711.385307	273762.755611	37.247629
1713.466377	274271.174484	37.252647
1714.923796	274766.333667	37.257664
1716.591574	275256.960901	37.262682
1718.178362	275759.869883	37.267700
1719.906161	276244.287013	37.272717
1721.485746	276748.846214	37.277735
1723.276625	277250.879966	37.282752
1725.226463	277753.038723	37.287770
1726.913164	278249.676699	37.292788
1728.966540	278743.839730	37.297805
1730.354101	279249.364604	37.302823
1732.459408	279744.481860	37.307840
1734.278715	280237.866956	37.312858
1736.007733	280742.086832	37.317876
1738.092818	281237.279714	37.322893
1739.547708	281737.020612	37.327911
1741.199247	282222.477335	37.332928
1743.307980	282720.151503	37.337946
1744.684067	283212.483912	37.342964
1746.552578	283705.216153	37.347981
1748.514495	284202.300490	37.352999
1749.988843	284689.379537	37.358016
1751.780454	285185.371256	37.363034
1753.573830	285680.802259	37.368052
1755.342572	286150.783961	37.373069
1756.971770	286626.680220	37.378087
1759.003575	287098.037890	37.383104
1760.408165	287568.735582	37.388122
1762.128556	288043.723046	37.393140
1764.009514	288518.631562	37.398157
1765.622119	288993.582747	37.403175
1767.504759	289475.244142	37.408192
1769.234199	289954.389060	37.413210
1770.354050	290441.913345	37.418228
1772.599205	290914.492488	37.423245
1774.303688	291420.712501	37.428263
1775.970700	291901.663792	37.433280
1777.753256	292393.617604	37.438298
1779.175954	292892.232754	37.443316
1780.866306	293387.296474	37.448333
1782.794091	293889.532329	37.453351
1784.321991	294400.899604	37.458368
1786.041804	294918.277898	37.463386
1787.746080	295435.275391	37.468404
1789.673335	295942.658236	37.473421
1791.656065	296463.186165	37.478439
1793.029342	296987.495049	37.483456
1795.221870	297513.901121	37.488474
1796.581359	298034.981462	37.493492
1798.628493	298566.511319	37.498509
1800.635988	299096.952833	37.503527
1802.228042	299636.070111	37.508544
1804.159430	300164.410500	37.513562
1805.701165	300702.438162	37.518580
1807.788202	301240.804539	37.523597
1809.515604	301775.951005	37.528615
1810.919734	302319.325779	37.533632
1812.991302	302852.377485	37.538650
1815.006766	303412.407053	37.543668
1816.801164	303954.006139	37.548685
1818.474905	304506.517097	37.553703
1820.464665	305051.531231	37.558720
1822.460491	305595.499729	37.563738
1824.007364	306149.621283	37.568756
1826.017243	306706.761120	37.573773
1828.058520	307254.343240	37.578791
1829.757859	307812.390521	37.583808
1831.881950	308367.722759	37.588826
1833.499169	308925.395137	37.593844
1835.738592	309470.491858	37.598861
1837.540980	310028.837093	37.603879
1839.324205	310587.232355	37.608896
1841.238596	311135.621860	37.613914
1843.085981	311692.500335	37.618932
1844.579916	312249.737877	37.623949
1846.788607	312805.964505	37.628967
1848.346475	313365.164020	37.633984
1850.756918	313930.643169	37.639002
1852.205351	314489.598337	37.644020
1854.220575	315048.404839	37.649037
1856.233760	315610.026003	37.654055
1857.999343	316172.242294	37.659072
1860.002164	316715.344961	37.664090
1861.513598	317283.587065	37.669108
1863.598081	317840.277928	37.674125
1865.602226	318392.711671	37.679143
1867.228721	318957.746941	37.684160
1869.218667	319513.474869	37.689178
1870.826365	320068.677304	37.694196
1872.921076	320636.744252	37.699213
1874.717475	321199.066381	37.704231
1876.450184	321757.814060	37.709248
1878.390261	322286.739395	37.714266
1879.828129	322843.444298	37.719284
1881.625804	323383.860538	37.724301
1883.623752	323928.199914	37.729319
1885.268272	324484.018318	37.734336
1887.415596	325024.210284	37.739354
1888.938356	325587.046375	37.744372
1890.939238	326135.859690	37.749389
1892.776708	326693.352611	37.754407
1894.419445	327255.721732	37.759424
1896.573954	327819.930538	37.764442
1898.375945	328391.580106	37.769460
1900.189167	328954.641118	37.774477
1902.229626	329529.642110	37.779495
1903.924740	330112.082112	37.784512
1905.782345	330678.546212	37.789530
1907.746506	331258.543642	37.794548
1909.981082	331839.607437	37.799565
1911.723578	332415.745313	37.804583
1913.190427	333000.147790	37.809600
1915.337751	333587.401813	37.814618
1917.407911	334182.328668	37.819636
1918.836564	334774.130965	37.824653
1921.108908	335371.295945	37.829671
1922.651101	335966.214002	37.834688
1924.884058	336581.775715	37.839706
1926.831681	337186.462138	37.844724
1928.790211	337788.220578	37.849741
1930.738825	338394.238049	37.854759
1932.422879	339004.302564	37.859776
1934.464889	339608.614867	37.864794
1936.541324	340233.702560	37.869812
1938.412907	340861.379864	37.874829
1940.774452	341463.789435	37.879847
1942.729448	342094.254689	37.884864
1944.635745	342700.049227	37.889882
1946.481908	343326.125524	37.894900
1948.756364	343941.666131	37.899917
1950.713535	344554.459360	37.904935
1952.397146	345184.319810	37.909952
1954.439516	345804.899788	37.914970
1956.323360	346435.903217	37.919988
1958.134892	347066.300910	37.925005
1960.194824	347690.304313	37.930023
1962.396378	348326.863437	37.935040
1964.329427	348947.393761	37.940058
1965.998216	349583.211092	37.945076
1968.090721	350216.792378	37.950093
1969.942335	350852.155414	37.955111
1971.866984	351499.145048	37.960128
1973.927129	352137.804789	37.965146
1975.884691	352778.146902	37.970164
1977.906090	353415.576210	37.975181
1979.910853	354056.069181	37.980199
1982.249635	354697.563123	37.985216
1984.129070	355331.434821	37.990234
1986.411688	355971.954471	37.995252
1988.462814	356616.562282	38.000269
1990.381811	357247.201376	38.005287
1992.297612	357891.481845	38.010304
1994.155309	358534.467807	38.015322
1996.333959	359168.231405	38.020340
1998.253978	359819.534076	38.025357
2000.219758	360449.887558	38.030375
2001.946770	361089.378581	38.035392
2004.285171	361732.690754	38.040410
2006.530928	362376.489770	38.045428
2008.493909	363007.564111	38.050445
2010.845186	363619.435923	38.055463
2012.635303	364235.043804	38.060480
2014.886798	364841.712185	38.065498
2016.712392	365441.668083	38.070516
2018.599458	366044.572371	38.075533
2020.716588	366649.559910	38.080551
2022.103805	367272.972902	38.085568
2024.112589	367880.292237	38.090586
2026.187200	368505.042421	38.095604
2028.186337	369126.750694	38.100621
2030.276609	369759.188127	38.105639
2031.868744	370394.360143	38.110656
2034.014677	371033.284974	38.115674
2036.017887	371673.870722	38.120692
2037.802655	372314.430408	38.125709
2039.821510	372954.407370	38.130727
2041.806374	373620.425359	38.135744
2043.695167	374272.700654	38.140762
2045.829956	374936.234336	38.145780
2047.707897	375599.392064	38.150797
2049.902287	376259.669922	38.155815
2051.455849	376927.598171	38.160832
2053.934056	377611.337113	38.165850
2055.788810	378281.877337	38.170868
2057.564323	378959.898095	38.175885
2059.682212	379641.398812	38.180903
2061.655236	380333.179288	38.185920
2063.926054	381019.469958	38.190938
2066.173632	381721.090750	38.195956
2067.843102	382419.039454	38.200973
2070.122076	383111.548151	38.205991
2072.178025	383818.100029	38.211008
2074.327670	384518.789662	38.216026
2076.906271	385224.996382	38.221044
2078.812615	385944.253850	38.226061
2080.932425	386637.752681	38.231079
2083.338620	387345.614220	38.236096
2085.282016	388053.536293	38.241114
2087.678119	388747.982574	38.246132
2089.738608	389459.554728	38.251149
2092.041475	390169.904500	38.256167
2094.153436	390876.112247	38.261184
2096.131494	391568.029451	38.266202
2098.516816	392278.468967	38.271220
2099.981207	392989.829671	38.276237
2102.366679	393694.659627	38.281255
2104.576966	394411.972168	38.286272
2106.947988	395117.987676	38.291290
2109.098516	395832.361238	38.296308
2111.143181	396551.803854	38.301325
2113.755289	397245.006130	38.306343
2115.756809	397947.796372	38.311360
2117.909333	398664.863112	38.316378
2120.139122	399365.148569	38.321396
2122.149550	400079.390790	38.326413
2124.364623	400777.693058	38.331431
2126.622712	401491.403061	38.336448
2129.093736	402198.117081	38.341466
2130.871813	402893.880254	38.346484
2133.126547	403600.974917	38.351501
2135.547086	404297.534756	38.356519
2137.515374	404998.535066	38.361536
2140.004447	405700.749164	38.366554
2141.947777	406401.059331	38.371572
2144.242307	407093.465270	38.376589
2145.928140	407788.766224	38.381607
2147.858507	408502.071726	38.386624
2150.320091	409193.889976	38.391642
2152.631937	409869.173362	38.396660
2154.375697	410539.973870	38.401677
2156.661169	411208.793641	38.406695
2158.696522	411894.153124	38.411712
2160.777708	412560.692827	38.416730
2162.791579	413233.862944	38.421748
2164.700102	413928.308852	38.426765
2166.876176	414609.091270	38.431783
2169.191759	415297.253604	38.436800
2170.897716	415984.561205	38.441818
2172.777189	416681.521502	38.446836
2174.906189	417391.337324	38.451853
2177.312643	418094.579339	38.456871
2179.346376	418811.740633	38.461888
2181.384463	419525.588951	38.466906
2183.331461	420249.029094	38.471924
2185.156584	420977.152914	38.476941
2187.556973	421703.286843	38.481959
2189.716686	422443.061284	38.486976
2191.550872	423182.082456	38.491994
2194.031252	423923.354709	38.497012
2195.636283	424676.597576	38.502029
2198.225777	425421.553398	38.507047
2200.101350	426183.717715	38.512064
2201.972407	426962.870451	38.517082
2204.547801	427719.605230	38.522100
2206.595331	428508.095596	38.527117
2208.671720	429282.734488	38.532135
2211.286261	430058.828609	38.537152
2213.009501	430850.635851	38.542170
2215.509742	431630.493729	38.547188
2217.557723	432432.722963	38.552205
2219.838023	433226.483887	38.557223
2221.967929	434022.773215	38.562240
2223.961772	434830.901001	38.567258
2226.708366	435636.598624	38.572276
2228.819410	436446.370913	38.577293
2230.991743	437248.766171	38.582311
2233.355904	438061.728604	38.587328
2235.160026	438874.703571	38.592346
2237.837681	439695.500090	38.597364
2240.171337	440515.918439	38.602381
2242.602596	441327.385093	38.607399
2244.929854	442138.232024	38.612416
2246.900063	442960.188321	38.617434
2249.643360	443778.495342	38.622452
2251.622872	444598.921410	38.627469
2254.025183	445419.904416	38.632487
2256.398386	446242.783412	38.637504
2258.769438	447068.666466	38.642522
2260.808096	447891.942269	38.647540
2263.144019	448730.918650	38.652557
2265.763573	449541.035515	38.657575
2268.270601	450366.667211	38.662592
2270.033828	451177.570745	38.667610
2272.595328	452006.011918	38.672628
2274.900562	452844.526253	38.677645
2277.126705	453657.735178	38.682663
2279.694408	454489.768020	38.687680
2281.803482	455325.332003	38.692698
2284.019149	456135.765029	38.697716
2286.367851	456968.087584	38.702733
2288.815544	457790.450192	38.707751
2290.799227	458614.827761	38.712768
2292.939616	459444.959659	38.717786
2295.645646	460267.532658	38.722804
2297.539796	461089.953100	38.727821
2299.706365	461914.316631	38.732839
2302.522232	462722.869308	38.737856
2304.558738	463526.665257	38.742874
2307.087702	464315.133807	38.747892
2309.023705	465112.260439	38.752909
2311.272967	465915.064265	38.757927
2313.454055	466723.455785	38.762944
2315.867377	467535.211616	38.767962
2317.784672	468341.406113	38.772980
2320.139905	469153.153930	38.777997
2322.082306	469975.192653	38.783015
2325.020757	470795.111626	38.788032
2326.654061	471613.694905	38.793050
2328.983362	472448.244255	38.798068
2331.246494	473299.489402	38.803085
2333.403926	474141.670919	38.808103
2336.026059	475004.095166	38.813120
2337.966229	475862.500550	38.818138
2340.122895	476715.324939	38.823156
2342.589586	477588.059753	38.828173
2344.820104	478451.246713	38.833191
2347.259744	479320.216825	38.838208
2349.565857	480202.297662	38.843226
2352.024024	481069.060301	38.848244
2354.337822	481956.861822	38.853261
2356.575807	482835.997887	38.858279
2359.000796	483714.656147	38.863296
2361.147664	484621.640814	38.868314
2363.646331	485518.070825	38.873332
2365.735415	486425.528358	38.878349
2368.290520	487325.088470	38.883367
2370.621067	488237.006640	38.888384
2372.806302	489146.529032	38.893402
2375.414104	490057.398008	38.898420
2378.026611	490978.211453	38.903437
2380.371348	491895.285569	38.908455
2383.165729	492818.191492	38.913472
2385.525510	493731.229092	38.918490
2387.894494	494648.354060	38.923508
2390.189767	495567.359155	38.928525
2392.531125	496494.278495	38.933543
2395.530359	497414.833039	38.938560
2397.750711	498338.341277	38.943578
2400.286529	499269.414231	38.948596
2402.557646	500194.627669	38.953613
2404.711940	501109.670622	38.958631
2407.633938	502046.375383	38.963648
2409.732699	502977.564678	38.968666
2412.386324	503911.131215	38.973684
2414.860687	504847.245923	38.978701
2417.239118	505773.741981	38.983719
2419.975777	506711.218960	38.988736
2421.966911	507645.739489	38.993754
2424.524910	508569.373651	38.998772
2427.074682	509514.129649	39.003789
2429.517806	510450.277684	39.008807
2432.106896	511384.985635	39.013824
2434.206997	512334.386904	39.018842
2437.005549	513267.840302	39.023860
2439.388936	514197.678191	39.028877
2442.081708	515140.714321	39.033895
2445.003653	516071.360009	39.038912
2446.983402	517010.822889	39.043930
2449.410133	517935.341567	39.048948
2452.015892	518878.769905	39.053965
2454.042309	519817.802574	39.058983
2456.826857	520747.887072	39.064000
2458.847100	521690.735326	39.069018
2461.398749	522625.630046	39.074036
2463.905374	523533.628526	39.079053
2466.110171	524448.622979	39.084071
2468.308554	525361.900977	39.089088
2470.383565	526273.230134	39.094106
2472.546062	527191.136277	39.099124
2475.324060	528121.573166	39.104141
2477.150177	529052.058450	39.109159
2479.802047	529987.232568	39.114176
2482.226753	530929.734907	39.119194
2484.681103	531879.370457	39.124212
2487.046181	532829.462488	39.129229
2489.021293	533791.938899	39.134247
2491.661530	534761.640298	39.139264
2494.366422	535721.553099	39.144282
2496.484903	536685.272991	39.149300
2498.714686	537671.654345	39.154317
2500.560918	538667.289191	39.159335
2503.616520	539659.988484	39.164352
2506.035797	540669.576918	39.169370
2508.446753	541673.712080	39.174388
2510.894900	542691.854130	39.179405
2512.837044	543714.784228	39.184423
2515.634561	544731.513466	39.189440
2517.722859	545775.241403	39.194458
2520.313633	546814.030822	39.199476
2522.749935	547867.500720	39.204493
2525.156278	548921.900686	39.209511
2527.503509	549974.268758	39.214528
2530.118791	551041.844489	39.219546
2532.295959	552121.070957	39.224564
2535.315370	553199.268525	39.229581
2537.984497	554282.865971	39.234599
2540.651207	555363.411637	39.239616
2543.114216	556459.180335	39.244634
2545.581209	557537.975571	39.249652
2548.231304	558626.299935	39.254669
2550.637066	559739.393386	39.259687
2553.088477	560823.249506	39.264704
2555.878465	561927.956957	39.269722
2558.071301	563041.861315	39.274740
2561.182206	564156.222418	39.279757
2563.590238	565269.850826	39.284775
2566.268025	566379.522918	39.289792
2568.761920	567500.276448	39.294810
2571.456389	568609.151436	39.299828
2574.282429	569733.922716	39.304845
2576.739793	570857.953038	39.309863
2579.108328	571978.937451	39.314880
2581.686117	573097.429451	39.319898
2584.147686	574236.717476	39.324916
2586.734154	575366.046882	39.329933
2589.332905	576505.206841	39.334951
2592.284759	577626.495054	39.339968
2594.610376	578773.620083	39.344986
2597.443693	579912.830628	39.350004
2600.199847	581051.898632	39.355021
2602.811718	582193.994273	39.360039
2605.665838	583309.917929	39.365056
2608.064237	584463.370393	39.370074
2610.438649	585599.119634	39.375092
2613.198731	586749.387366	39.380109
2615.837505	587895.405008	39.385127
2618.543916	589031.729020	39.390144
2621.306615	590177.508400	39.395162
2623.504900	591330.787796	39.400180
2626.175079	592474.307041	39.405197
2628.755964	593633.763551	39.410215
2631.410742	594754.769257	39.415232
2634.537189	595881.000428	39.420250
2636.638814	596978.040900	39.425268
2639.610153	598085.502752	39.430285
2641.731255	599205.368981	39.435303
2644.721234	600304.553649	39.440320
2647.132601	601431.818089	39.445338
2649.613507	602552.352314	39.450356
2652.501589	603663.248820	39.455373
2654.975117	604796.430163	39.460391
2657.108192	605919.995615	39.465408
2660.164600	607051.705184	39.470426
2662.531772	608194.223862	39.475444
2665.648161	609332.850794	39.480461
2668.087616	610490.685330	39.485479
2670.631655	611624.371418	39.490496
2673.505237	612785.398538	39.495514
2675.802524	613936.946975	39.500532
2678.778860	615103.466449	39.505549
2681.183660	616275.807421	39.510567
2684.114245	617450.886748	39.515584
2686.988221	618615.051183	39.520602
2689.390579	619797.514753	39.525620
2692.057976	620964.211998	39.530637
2694.628899	622157.837001	39.535655
2697.623508	623350.560865	39.540672
2700.724687	624538.238612	39.545690
2703.039300	625732.959108	39.550708
2705.675517	626931.639451	39.555725
2708.545079	628132.793908	39.560743
2711.261072	629341.329401	39.565760
2713.863942	630544.602170	39.570778
2716.512181	631752.523727	39.575796
2719.460397	632966.747450	39.580813
2722.224433	634198.881936	39.585831
2725.394204	635406.845514	39.590848
2727.896333	636617.274421	39.595866
2730.756261	637847.463985	39.600884
2733.837887	639060.705430	39.605901
2736.366606	640283.673683	39.610919
2739.067882	641508.513052	39.615936
2741.907482	642733.581986	39.620954
2744.810850	643959.939484	39.625972
2748.074606	645173.672757	39.630989
2750.482064	646403.556512	39.636007
2753.269181	647627.295081	39.641024
2756.409365	648854.066623	39.646042
2758.650576	650088.412222	39.651060
2761.686470	651311.360789	39.656077
2764.124928	652540.785301	39.661095
2767.259404	653773.878714	39.666112
2769.992906	655009.375279	39.671130
2772.438710	656245.461689	39.676148
2775.324651	657489.139250	39.681165
2777.972405	658737.877035	39.686183
2780.454393	659977.320493	39.691200
2783.278542	661227.153804	39.696218
2785.492182	662487.230797	39.701236
2788.562201	663746.155933	39.706253
2791.527322	665012.597568	39.711271
2794.376797	666262.918111	39.716288
2797.336488	667527.584734	39.721306
2800.127424	668805.642207	39.726324
2803.078062	670058.283154	39.731341
2805.706345	671324.836066	39.736359
2808.193194	672583.633950	39.741376
2811.403374	673842.839939	39.746394
2813.808889	675116.177445	39.751412
2816.847555	676366.918655	39.756429
2819.830788	677600.503472	39.761447
2822.453782	678828.914803	39.766464
2825.315285	680050.465478	39.771482
2827.674653	681284.307217	39.776500
2830.847335	682494.005838	39.781517
2833.695117	683736.328427	39.786535
2836.441862	684972.142001	39.791552
2839.271434	686205.092663	39.796570
2841.590604	687461.492074	39.801588
2844.365255	688700.267874	39.806605
2847.086906	689955.657768	39.811623
2849.561637	691223.319151	39.816640
2852.776453	692495.194149	39.821658
2855.408354	693756.367004	39.826676
2858.306780	695048.170780	39.831693
2861.183535	696323.571551	39.836711
2863.868656	697620.787951	39.841728
2866.708977	698897.706679	39.846746
2869.403516	700205.200170	39.851764
2872.367741	701513.742433	39.856781
2875.411918	702811.320449	39.861799
2878.307582	704131.275614	39.866816
2881.054789	705451.103549	39.871834
2883.739281	706778.715493	39.876852
2886.814191	708093.328938	39.881869
2889.583609	709441.020543	39.886887
2892.258544	710767.669581	39.891904
2895.196508	712111.197865	39.896922
2898.203858	713474.400489	39.901940
2901.100910	714831.759646	39.906957
2904.173172	716187.931180	39.911975
2907.051790	717549.902162	39.916992
2910.087844	718911.971925	39.922010
2913.048564	720276.749856	39.927028
2915.884080	721641.522296	39.932045
2918.751298	723012.442882	39.937063
2921.694302	724402.452179	39.942080
2924.775293	725775.448821	39.947098
2927.772130	727159.150864	39.952116
2930.889170	728536.719355	39.957133
2933.982096	729922.852338	39.962151
2936.741000	731307.371551	39.967168
2940.090945	732696.692524	39.972186
2942.908590	734073.962688	39.977204
2946.070944	735456.568041	39.982221
2948.916336	736849.352444	39.987239
2951.817303	738232.755301	39.992256
2954.770679	739622.619626	39.997274
2958.105046	741013.411131	40.002292
2960.981141	742406.746526	40.007309
2963.817921	743798.362817	40.012327
2966.982281	745184.304395	40.017344
2970.308078	746589.249469	40.022362
2973.341395	747980.534258	40.027380
2976.287819	749369.416403	40.032397
2979.250364	750759.328326	40.037415
2981.940109	752146.326029	40.042432
2985.142291	753541.658267	40.047450
2988.256895	754936.111384	40.052468
2991.043802	756328.444474	40.057485
2994.246387	757731.826362	40.062503
2997.252837	759125.286013	40.067520
3000.188488	760518.255317	40.072538
3003.075265	761910.976061	40.077556
3006.049565	763315.476533	40.082573
3009.063262	764715.970224	40.087591
3011.969844	766119.317460	40.092608
3015.235681	767495.646591	40.097626
3018.102002	768852.174868	40.102644
3021.076753	770209.616685	40.107661
3023.778249	771563.906277	40.112679
3026.788471	772902.274065	40.117696
3029.964159	774259.968702	40.122714
3033.034319	775633.536639	40.127732
3035.573381	777002.465876	40.132749
3038.759450	778361.851415	40.137767
3041.609052	779739.393968	40.142784
3044.581140	781120.628930	40.147802
3047.210070	782498.761451	40.152820
3050.213417	783893.638401	40.157837
3053.150049	785287.323240	40.162855
3055.742053	786696.679871	40.167872
3059.122918	788107.294582	40.172890
3062.071023	789536.276586	40.177908
3065.165650	790945.246762	40.182925
3068.091037	792388.406135	40.187943
3070.965570	793827.457278	40.192960
3074.217768	795266.248956	40.197978
3077.526250	796716.780299	40.202996
3080.817676	798165.005561	40.208013
3084.030458	799614.508140	40.213031
3086.936823	801072.908302	40.218048
3090.253551	802522.860675	40.223066
3093.415652	803990.043528	40.228084
3096.445988	805463.536054	40.233101
3099.549881	806926.823114	40.238119
3102.585142	808408.381907	40.243136
3106.062100	809882.214520	40.248154
3109.052018	811369.975814	40.253172
3111.914012	812859.823997	40.258189
3115.351793	814340.749894	40.263207
3118.239838	815846.975701	40.268224
3121.384094	817333.245189	40.273242
3124.814610	818826.896082	40.278260
3127.860024	820331.155671	40.283277
3131.056261	821828.170553	40.288295
3134.193947	823331.098439	40.293312
3137.583259	824839.931755	40.298330
3140.483145	826354.446124	40.303348
3143.790347	827860.793441	40.308365
3146.835236	829364.009844	40.313383
3150.106551	830894.754849	40.318400
3153.472264	832395.803213	40.323418
3156.459590	833917.015673	40.328436
3159.483175	835444.239826	40.333453
3163.068534	836969.742527	40.338471
3165.968062	838494.897098	40.343488
3169.391195	840002.671916	40.348506
3172.255341	841540.042416	40.353524
3175.412964	843074.317314	40.358541
3178.845570	844609.146363	40.363559
3181.776754	846134.450150	40.368576
3184.892030	847685.783932	40.373594
3187.953444	849216.049176	40.378612
3191.255988	850757.845529	40.383629
3194.546002	852302.174532	40.388647
3197.613130	853856.057152	40.393664
3200.968869	855399.990188	40.398682
3203.912407	856950.395914	40.403700
3207.272677	858496.849203	40.408717
3210.358720	860041.793026	40.413735
3213.570901	861604.648968	40.418752
3217.036443	863154.072905	40.423770
3220.316979	864707.685647	40.428788
3223.401893	866266.259408	40.433805
3226.803966	867798.711169	40.438823
3229.974524	869317.931513	40.443840
3233.164490	870819.918866	40.448858
3236.512359	872317.437271	40.453876
3239.756817	873819.143260	40.458893
3243.015189	875312.921567	40.463911
3245.888434	876824.373559	40.468928
3248.805553	878338.137901	40.473946
3252.121468	879847.966935	40.478964
3255.201140	881375.419488	40.483981
3258.617607	882892.659771	40.488999
3261.304726	884436.088381	40.494016
3264.544451	885973.029152	40.499034
3267.445434	887511.644738	40.504052
3270.622186	889085.993759	40.509069
3273.886337	890636.453355	40.514087
3276.908150	892212.093358	40.519104
3280.108382	893794.887230	40.524122
3283.785567	895377.548464	40.529140
3287.102198	896976.018445	40.534157
3290.426463	898574.132292	40.539175
3293.490120	900175.592969	40.544192
3296.596592	901761.473487	40.549210
3300.177900	903382.732931	40.554228
3303.044884	905009.413980	40.559245
3306.829332	906631.524750	40.564263
3309.803141	908263.971111	40.569280
3313.009894	909897.532480	40.574298
3316.373353	911534.429468	40.579316
3319.728563	913191.788752	40.584333
3323.174276	914834.607341	40.589351
3326.133209	916500.348531	40.594368
3329.434679	918167.924299	40.599386
3332.983430	919832.548106	40.604404
3336.345317	921509.835311	40.609421
3339.632861	923177.789436	40.614439
3343.059783	924869.845762	40.619456
3346.607308	926552.913171	40.624474
3350.063655	928252.809690	40.629492
3353.306910	929949.708314	40.634509
3356.759239	931629.942179	40.639527
3360.049461	933302.872392	40.644544
3363.071361	935000.103083	40.649562
3366.987524	936715.772762	40.654580
3370.329479	938416.629614	40.659597
3373.823602	940122.261727	40.664615
3377.485100	941817.463236	40.669632
3380.475564	943526.553439	40.674650
3384.263303	945226.256023	40.679668
3387.372050	946944.702112	40.684685
3390.971317	948646.552785	40.689703
3394.375165	950357.316762	40.694720
3397.021232	952068.300226	40.699738
3400.853763	953824.426840	40.704756
3403.949866	955597.923329	40.709773
3407.617190	957360.024704	40.714791
3410.996473	959138.741849	40.719808
3414.192206	960907.363398	40.724826
3417.457154	962685.297242	40.729844
3420.608314	964466.997540	40.734861
3424.127901	966253.357056	40.739879
3426.978811	968048.738489	40.744896
3430.497279	969841.009069	40.749914
3434.245723	971639.216769	40.754932
3437.329297	973445.842981	40.759949
3440.500304	975251.787219	40.764967
3443.977825	977068.609650	40.769984
3447.151121	978875.942316	40.775002
3450.586477	980668.475830	40.780007
3453.606429	982433.244781	40.785012
3457.131957	984128.105591	40.790016
3460.239197	985764.490232	40.795021
3463.371195	987321.993740	40.800026
3466.392534	988829.658984	40.805031
3469.156292	990265.326109	40.810036
3472.417423	991614.795084	40.815040
3475.084424	992890.095369	40.820045
3477.577720	994098.610303	40.825050
3480.443939	995231.722401	40.830055
3482.410244	996297.670485	40.835060
3485.105675	997280.550628	40.840064
3487.237193	998208.067302	40.845069
3489.346933	999061.764955	40.850074
3491.691199	999871.313049	40.855079
3493.416025	1000605.640127	40.860084
3495.583009	1001267.519049	40.865088
3497.129026	1001894.697072	40.870093
3498.867047	1002444.743228	40.875098
3500.829835	1002938.292298	40.880103
3501.939870	1003396.930548	40.885108
3503.575120	1003788.350931	40.890112
3505.008886	1004154.302599	40.895117
3506.366515	1004457.823784	40.900122
3507.600461	1004727.807453	40.905127
3508.480761	1004951.171848	40.910132
3509.493459	1005137.369531	40.915136
3510.587140	1005297.300444	40.920141
3511.390346	1005424.709360	40.925146
3512.416868	1005511.542740	40.930151
3513.295114	1005566.126337	40.935156
3514.151210	1005602.632565	40.940160
3515.082521	1005612.783154	40.945165
3515.753929	1005592.453546	40.950170
3516.272436	1005520.726000	40.955175
3516.870743	1005462.107694	40.960180
3517.856830	1005353.652903	40.965184
3518.127826	1005252.604823	40.970189
3518.504508	1005114.984627	40.975194
3519.163394	1004963.606855	40.980199
3519.297889	1004799.381050	40.985204
3520.252219	1004608.959390	40.990208
3520.713009	1004416.473616	40.995213
3520.807456	1004192.635996	41.000218
3521.631231	1003957.487293	41.005223
3521.538013	1003713.339357	41.010228
3522.051589	1003449.048642	41.015232
3522.335478	1003174.183285	41.020237
3522.746767	1002904.048994	41.025242
3523.151600	1002607.740343	41.030247
3522.862324	1002314.156625	41.035252
3522.972323	1002007.263307	41.040256
3523.199122	1001695.664917	41.045261
3523.146857	1001382.927967	41.050266
3523.465578	1001060.189511	41.055271
3523.376094	1000730.300359	41.060276
3523.668898	1000389.626343	41.065280
3523.972331	1000053.114073	41.070285
3523.506761	999713.497295	41.075290
3524.046647	999354.426222	41.080295
3524.147556	999003.774271	41.085300
3524.283162	998650.564383	41.090304
3524.153544	998283.749543	41.095309
3524.178050	997914.841414	41.100314
3524.584200	997547.890636	41.105319
3524.239790	997175.393317	41.110324
3524.452483	996787.104979	41.115328
3524.310767	996413.453210	41.120333
3524.270475	996035.183620	41.125338
3524.528721	995651.094283	41.130343
3524.403331	995269.379360	41.135348
3524.397288	994881.386017	41.140352
3524.505373	994492.081145	41.145357
3524.397855	994095.382293	41.150362
3524.446048	993713.144381	41.155367
3524.390703	993328.267482	41.160372
3524.388372	992939.556173	41.165376
3524.706364	992548.621975	41.170381
3524.553735	992141.173861	41.175386
3524.302770	991740.533883	41.180391
3524.338718	991345.470593	41.185396
3524.087001	990946.626311	41.190400
3524.345254	990555.662200	41.195405
3524.489968	990152.700771	41.200410
3524.582828	989742.993218	41.205415
3523.935472	989350.340734	41.210420
3524.146231	988932.951420	41.215424
3524.273598	988537.970330	41.220429
3523.990489	988137.666536	41.225434
3524.339716	987732.744740	41.230439
3524.244648	987330.597912	41.235444
3524.541399	986907.779678	41.240448
3524.015230	986505.743099	41.245453
3523.937141	986111.212569	41.250458
3523.830475	985689.053055	41.255463
3523.825971	985299.721821	41.260468
3523.857753	984897.577290	41.265472
3523.957957	984491.783019	41.270477
3523.646141	984080.075545	41.275482
3523.857470	983679.474258	41.280487
3523.603951	983282.727421	41.285492
3523.685051	982869.599089	41.290496
3523.468714	982476.986735	41.295501
3523.266891	982082.978401	41.300506
3523.298364	981684.902085	41.305511
3522.977782	981289.101352	41.310516
3522.896350	980883.958778	41.315520
3523.557882	980484.035150	41.320525
3523.153707	980094.609452	41.325530
3523.475961	979684.140029	41.330535
3523.097549	979305.690927	41.335540
3522.801474	978898.587286	41.340544
3523.126592	978489.008150	41.345549
3522.724801	978091.729319	41.350554
3522.983191	977694.021040	41.355559
3522.366430	977306.393918	41.360564
3522.376432	976902.614546	41.365568
3522.323653	976508.978456	41.370573
3522.262038	976130.364497	41.375578
3522.560985	975738.864848	41.380583
3522.360425	975352.111550	41.385588
3522.630518	974950.399192	41.390592
3522.001836	974565.813389	41.395597
3521.854987	974179.069685	41.400602
3522.123485	973783.042669	41.405607
3521.998532	973399.077495	41.410612
3522.003042	973015.065245	41.415616
3521.639336	972627.763643	41.420621
3521.617391	972245.268498	41.425626
3521.967443	971862.295392	41.430631
3521.341643	971486.107321	41.435636
3521.422593	971103.616811	41.440640
3521.157908	970724.483092	41.445645
3521.042186	970357.917419	41.450650
3521.283058	969981.194354	41.455655
3520.910263	969608.656257	41.460660
3521.059766	969221.333339	41.465664
3521.166211	968854.145803	41.470669
3520.876975	968478.878972	41.475674
3521.219877	968110.332932	41.480679
3520.901416	967747.645683	41.485684
3520.406756	967367.251507	41.490688
3520.606988	966993.274843	41.495693
3520.367337	966644.206487	41.500698
3520.364403	966273.446287	41.505703
3520.338191	965927.822944	41.510708
3520.209299	965558.016195	41.515712
3519.996465	965192.507046	41.520717
3520.083291	964838.380215	41.525722
3520.384839	964470.390683	41.530727
3520.021729	964106.403816	41.535732
3519.719854	963759.128791	41.540736
3519.753109	963406.097662	41.545741
3519.452644	963057.996630	41.550746
3519.483936	962694.540975	41.555751
3519.414147	962356.447492	41.560756
3519.246747	962009.044656	41.565760
3519.122665	961671.507603	41.570765
3519.011857	961322.682590	41.575770
3519.109739	960970.764959	41.580775
3519.100661	960633.833927	41.585780
3518.907965	960291.426408	41.590784
3519.195777	959948.821385	41.595789
3518.712136	959614.848589	41.600794
3518.678322	959266.376322	41.605799
3518.803239	958938.536075	41.610804
3518.664694	958592.196430	41.615808
3518.954171	958256.547374	41.620813
3518.491028	957921.590914	41.625818
3518.441126	957585.076481	41.630823
3518.085898	957255.259052	41.635828
3518.210741	956926.226032	41.640832
3518.072797	956586.824710	41.645837
3517.752212	956259.101623	41.650842
3518.106495	955930.170115	41.655847
3518.041784	955615.115680	41.660852
3517.718130	955294.006521	41.665856
3517.964672	954965.233929	41.670861
3517.589959	954649.589439	41.675866
3518.091793	954317.697498	41.680871
3517.723294	954004.076472	41.685876
3517.823321	953678.001264	41.690880
3517.641083	953357.349689	41.695885
3517.309120	953049.164429	41.700890
3517.716977	952721.414845	41.705895
3517.427237	952414.292783	41.710900
3517.288381	952108.312189	41.715904
3517.481880	951791.929887	41.720909
3517.245000	951475.311921	41.725914
3517.135726	951169.939571	41.730919
3516.631748	950876.953095	41.735924
3516.892465	950573.110148	41.740928
3516.991415	950268.606132	41.745933
3516.747227	949967.967265	41.750938
3516.932315	949664.656773	41.755943
3516.423415	949369.001379	41.760948
3516.648248	949075.408791	41.765952
3516.756294	948780.000480	41.770957
3516.204830	948496.550182	41.775962
3516.484732	948199.261848	41.780967
3516.312095	947911.793018	41.785972
3516.164855	947613.296904	41.790976
3515.971794	947328.670171	41.795981
3515.866384	947051.766839	41.800986
3515.663713	946762.419865	41.805991
3515.774098	946478.174686	41.810996
3515.754194	946196.233021	41.816000
3515.645670	945925.684124	41.821005
3515.479054	945640.863887	41.826010
3515.866203	945355.266392	41.831015
3515.422066	945078.504228	41.836020
3515.318513	944800.426150	41.841024
3515.324163	944529.114806	41.846029
3515.148642	944254.850018	41.851034
3515.238009	943983.496229	41.856039
3515.064572	943718.493340	41.861044
3514.750246	943442.771554	41.866048
3514.983181	943171.543104	41.871053
3514.871700	942903.518612	41.876058
3515.001768	942648.278378	41.881063
3514.691946	942383.708663	41.886068
3514.832273	942111.290264	41.891072
3514.580001	941852.337055	41.896077
3514.545816	941595.634789	41.901082
3514.600645	941329.226391	41.906087
3514.123046	941082.921425	41.911092
3514.122456	940823.683800	41.916096
3514.352087	940556.152764	41.921101
3513.977158	940311.807079	41.926106
3513.679870	940054.401129	41.931111
3513.919694	939810.314045	41.936116
3513.755283	939564.652474	41.941120
3514.079891	939310.079028	41.946125
3513.689325	939061.650885	41.951130
3513.614786	938814.788736	41.956135
3513.412281	938587.303801	41.961140
3513.598537	938341.047455	41.966144
3513.741817	938082.129218	41.971149
3513.336120	937843.234529	41.976154
3513.494140	937612.962771	41.981159
3513.419363	937371.690481	41.986164
3513.536850	937119.825646	41.991168
3513.220715	936880.200894	41.996173
3512.898248	936662.914537	42.001178
3513.149841	936412.432343	42.006183
3513.216544	936181.633130	42.011188
3512.861653	935944.849737	42.016192
3512.922998	935711.056934	42.021197
3512.859281	935488.978627	42.026202
3512.699595	935246.951021	42.031207
3512.590541	935024.284901	42.036212
3512.873277	934789.359233	42.041216
3512.795208	934554.386570	42.046221
3512.318468	934338.180890	42.051226
3512.556965	934114.075593	42.056231
3512.466550	933895.197112	42.061236
3512.378543	933667.767826	42.066240
3512.467320	933442.411035	42.071245
3511.961077	933215.031129	42.076250
3512.057677	932995.796576	42.081255
3511.817980	932781.215659	42.086260
3511.724871	932573.609136	42.091264
3512.007787	932363.244684	42.096269
3511.620787	932153.558218	42.101274
3512.056788	931945.551870	42.106279
3512.054478	931743.177849	42.111284
3511.836416	931516.733428	42.116288
3512.022012	931303.174574	42.121293
3511.884735	931093.212925	42.126298
3511.758108	930880.840689	42.131303
3511.687346	930677.284976	42.136308
3511.760981	930448.730348	42.141312
3511.659806	930247.467833	42.146317
3511.183643	930040.209217	42.151322
3511.384636	929837.632919	42.156327
3511.204742	929628.196543	42.161332
3511.514941	929427.795626	42.166336
3511.425857	929223.899072	42.171341
3510.998368	929010.541081	42.176346
3510.955308	928819.588768	42.181351
3510.950979	928635.635689	42.186356
3510.933123	928433.618340	42.191360
3510.913469	928224.196354	42.196365
3510.743891	928039.001005	42.201370
3510.811279	927845.401631	42.206375
3510.558310	927659.438232	42.211380
3510.648813	927466.109520	42.216384
3510.485278	927275.025628	42.221389
3510.281797	927101.333570	42.226394
3510.606421	926907.177338	42.231399
3510.579121	926723.065981	42.236404
3510.445308	926538.581435	42.241408
3510.538743	926344.731161	42.246413
3510.447927	926158.496574	42.251418
3510.213271	925975.835235	42.256423
3510.308407	925790.518295	42.261428
3510.215256	925614.356940	42.266432
3510.141028	925421.942598	42.271437
3509.944453	925248.573700	42.276442
3509.895395	925056.911080	42.281447
3509.929547	924882.627204	42.286452
3509.834716	924708.358916	42.291456
3509.977650	924529.046780	42.296461
3509.573814	924350.780117	42.301466
3509.623143	924179.643466	42.306471
3509.464127	924004.593772	42.311476
3509.737759	923838.024211	42.316480
3509.911896	923668.292923	42.321485
3509.812790	923499.851288	42.326490
3509.485360	923320.191686	42.331495
3509.432951	923156.154793	42.336500
3509.528590	922984.780158	42.341504
3509.728189	922804.247201	42.346509
3509.418326	922647.641987	42.351514
3509.672880	922473.051325	42.356519
3509.376981	922313.260422	42.361524
3509.234678	922142.956128	42.366528
3509.066322	921964.090663	42.371533
3508.693977	921808.048424	42.376538
3508.945771	921654.303500	42.381543
3509.101422	921497.876745	42.386548
3508.889768	921335.926842	42.391552
3509.093781	921172.556870	42.396557
3508.887672	921020.504657	42.401562
3508.932952	920863.019529	42.406567
3508.853248	920706.031420	42.411572
3508.820356	920542.489030	42.416576
3508.859486	920392.687698	42.421581
3508.654727	920238.592885	42.426586
3508.836128	920074.519988	42.431591
3508.798406	919922.216721	42.436596
3508.439289	919763.130508	42.441600
3508.525727	919621.382509	42.446605
3508.568944	919476.173823	42.451610
3508.492186	919317.990269	42.456615
3508.377265	919178.092180	42.461620
3508.245900	919026.837707	42.466624
3508.394457	918870.047461	42.471629
3508.244451	918728.411309	42.476634
3508.256766	918580.681544	42.481639
3508.388484	918436.007879	42.486644
3508.271511	918308.695596	42.491648
3508.325556	918142.179076	42.496653
3508.438988	917995.475472	42.501658
3508.381927	917849.277268	42.506663
3508.379823	917709.996539	42.511668
3508.007805	917557.393197	42.516672
3508.015786	917413.290254	42.521677
3507.836869	917281.151028	42.526682
3507.848883	917131.264114	42.531687
3507.780349	916991.013259	42.536692
3507.757658	916849.595981	42.541696
3508.066625	916716.399954	42.546701
3507.615422	916583.133359	42.551706
3507.728722	916442.838436	42.556711
3507.673646	916305.070954	42.561716
3507.478558	916173.581490	42.566720
3507.911449	916044.103683	42.571725
3507.389999	915908.136154	42.576730
3507.638005	915783.978485	42.581735
3507.839528	915648.559411	42.586740
3507.686787	915518.587871	42.591744
3507.582104	915372.331044	42.596749
3507.744209	915240.760260	42.601754
3507.538304	915108.669126	42.606759
3507.215733	914974.282708	42.611764
3507.376828	914851.755357	42.616768
3507.497032	914721.912513	42.621773
3507.357602	914601.836803	42.626778
3507.092162	914455.389305	42.631783
3507.311185	914331.685000	42.636788
3506.952531	914223.869225	42.641792
3506.942738	914102.123789	42.646797
3506.899729	913982.018594	42.651802
3507.307356	913858.465175	42.656807
3507.244460	913736.142409	42.661812
3507.327680	913609.072738	42.666816
3507.118034	913469.910666	42.671821
3507.299072	913346.575708	42.676826
3507.126334	913218.479490	42.681831
3506.950266	913102.615712	42.686836
3506.516137	912998.063722	42.691840
3507.094149	912861.742973	42.696845
3507.075366	912757.214309	42.701850
3506.983316	912628.416617	42.706855
3506.727427	912506.387264	42.711860
3506.865411	912387.180811	42.716864
3506.834354	912266.939749	42.721869
3506.771679	912148.531997	42.726874
3506.624822	912039.385767	42.731879
3506.854495	911917.841484	42.736884
3506.539035	911811.898340	42.741888
3507.028341	911691.366242	42.746893
3506.487102	911571.675842	42.751898
3506.364593	911459.623163	42.756903
3506.406830	911353.804998	42.761908
3506.436321	911246.059498	42.766912
3506.401753	911119.048014	42.771917
3506.166140	911023.484735	42.776922
3506.381106	910910.497917	42.781927
3506.594175	910795.485160	42.786932
3506.401307	910693.644545	42.791937
3506.621420	910571.879377	42.796941
3506.581943	910469.623826	42.801946
3506.651847	910352.601364	42.806951
3506.493910	910245.541887	42.811956
3506.326556	910140.988010	42.816961
3506.144773	910032.482485	42.821965
3506.206453	909920.078987	42.826970
3506.240737	909816.835254	42.831975
3505.897570	909712.687809	42.836980
3506.010237	909603.739759	42.841985
3506.241576	909508.748093	42.846989
3506.184827	909403.583627	42.851994
3506.187747	909285.778375	42.856999
3506.168441	909192.172226	42.862004
3506.001236	909090.008576	42.867009
3506.152121	908982.295286	42.872013
3506.020463	908870.384341	42.877018
3505.837359	908777.280214	42.882023
3506.013681	908683.633229	42.887028
3505.916879	908577.399088	42.892033
3505.660429	908480.734636	42.897037
3505.537370	908385.203560	42.902042
3505.771841	908279.584066	42.907047
3505.893181	908186.901960	42.912052
3505.922788	908079.962486	42.917057
3505.797333	907985.774871	42.922061
3505.433450	907897.989221	42.927066
3505.874746	907794.640698	42.932071
3505.819463	907707.186905	42.937076
3505.615528	907597.287209	42.942081
3505.895902	907501.192259	42.947085
3505.687093	907420.895461	42.952090
3505.669979	907310.573558	42.957095
3505.612820	907224.655486	42.962100
3505.506045	907121.770493	42.967105
3505.667200	907043.914778	42.972109
3505.215065	906951.306509	42.977114
3505.248436	906857.941579	42.982119
3505.504268	906767.335427	42.987124
3505.405493	906679.776162	42.992129
3505.324771	906582.181609	42.997133
3505.458799	906486.286117	43.002138
3505.321252	906395.063536	43.007143
3505.500987	906311.600132	43.012148
3505.237197	906219.527366	43.017153
3505.301245	906140.131669	43.022157
3505.400424	906050.311317	43.027162
3505.450693	905966.960534	43.032167
3505.376079	905881.024563	43.037172
3505.251414	905785.641931	43.042177
3505.498629	905695.019736	43.047181
3505.116337	905603.438629	43.052186
3504.950500	905515.872087	43.057191
3505.129714	905421.108434	43.062196
3505.200131	905349.707543	43.067201
3505.505517	905265.050078	43.072205
3505.040993	905193.831796	43.077210
3505.233472	905092.692993	43.082215
3505.178713	905015.230376	43.087220
3504.750336	904929.434482	43.092225
3505.232902	904838.373665	43.097229
3504.835914	904767.428249	43.102234
3505.106725	904686.144591	43.107239
3505.465583	904595.293159	43.112244
3505.243032	904503.474678	43.117249
3505.069007	904417.532514	43.122253
3504.769340	904353.030540	43.127258
3505.006374	904279.465718	43.132263
3505.150471	904184.976326	43.137268
3504.891040	904109.175226	43.142273
3504.925177	904026.087564	43.147277
3504.895413	903951.597425	43.152282
3504.820456	903859.647538	43.157287
3504.636405	903791.839080	43.162292
3504.767197	903711.625807	43.167297
3504.630095	903622.673790	43.172301
3504.677118	903556.657957	43.177306
3504.600655	903483.327314	43.182311
3504.730118	903407.742139	43.187316
3504.301040	903339.679043	43.192321
3504.633812	903263.189852	43.197325
3504.756664	903188.471382	43.202330
3504.872677	903123.790215	43.207335
3504.919926	903041.747388	43.212340
3504.443367	902968.186371	43.217345
3504.742285	902885.810253	43.222349
3504.394735	902809.233915	43.227354
3504.562289	902729.193535	43.232359
3504.665670	902673.195857	43.237364
3504.428062	902593.413327	43.242369
3504.587834	902511.440711	43.247373
3504.446381	902453.261172	43.252378
3504.371707	902366.112825	43.257383
3504.449429	902299.980590	43.262388
3504.454719	902235.114352	43.267393
3504.591555	902162.406949	43.272397
3504.381814	902090.720993	43.277402
3504.379885	902022.088849	43.282407
3504.887800	901948.159170	43.287412
3504.289735	901876.051789	43.292417
3504.532347	901789.131798	43.297421
3504.281309	901732.314307	43.302426
3504.317229	901650.446048	43.307431
3504.134364	901591.299018	43.312436
3504.435759	901528.692729	43.317441
3504.454873	901454.644009	43.322445
3504.609013	901384.144091	43.327450
3504.614688	901307.585575	43.332455
3504.546692	901235.479166	43.337460
3504.418145	901162.319813	43.342465
3504.526086	901082.748490	43.347469
3504.096691	901030.201311	43.352474
3504.412541	900950.593863	43.357479
3504.287046	900888.823167	43.362484
3504.343892	900828.180360	43.367489
3504.492513	900759.507977	43.372493
3504.488013	900689.218582	43.377498
3504.078182	900608.663769	43.382503
3504.246356	900551.861817	43.387508
3504.206883	900484.568843	43.392513
3504.102914	900424.817190	43.397517
3504.308553	900368.103769	43.402522
3504.045666	900294.279338	43.407527
3504.154573	900228.600374	43.412532
3503.893425	900171.092824	43.417537
3503.929217	900094.319700	43.422541
3504.108460	900044.270229	43.427546
3503.905659	899978.736269	43.432551
3503.786871	899924.775661	43.437556
3503.668579	899866.468931	43.442561
3503.880024	899807.817566	43.447565
3503.706523	899760.624169	43.452570
3503.764811	899692.243356	43.457575
3503.764094	899639.419403	43.462580
3503.939518	899582.413336	43.467585
3503.925845	899519.160597	43.472589
3503.901844	899460.447836	43.477594
3503.918120	899398.540847	43.482599
3504.242481	899342.956451	43.487604
3503.794547	899276.682097	43.492609
3503.932996	899218.519517	43.497613
3503.693641	899152.499073	43.502618
3503.748816	899102.558263	43.507623
3503.608258	899038.451811	43.512628
3503.822085	898982.399168	43.517633
3503.669503	898910.373484	43.522637
3503.651531	898863.436698	43.527642
3503.718802	898804.315732	43.532647
3503.906240	898749.037803	43.537652
3503.500232	898693.084407	43.542657
3503.839037	898621.167248	43.547661
3503.480335	898581.431801	43.552666
3503.730439	898516.482342	43.557671
3503.668032	898468.583691	43.562676
3503.330253	898420.343634	43.567681
3503.170674	898355.653007	43.572685
3503.237151	898318.646857	43.577690
3503.466345	898270.022323	43.582695
3503.761940	898214.238370	43.587700
3503.494020	898168.302941	43.592705
3503.603079	898114.480661	43.597709
3503.613092	898061.736767	43.602714
3503.342825	898004.981398	43.607719
3503.618942	897962.045829	43.612724
3503.288893	897909.936143	43.617729
3503.463595	897848.469056	43.622733
3503.372149	897801.438949	43.627738
3503.429596	897760.469927	43.632743
3503.362996	897715.656887	43.637748
3503.393403	897661.746653	43.642753
3503.218051	897600.044725	43.647757
3503.318091	897554.333498	43.652762
3503.601034	897507.915515	43.657767
3503.412590	897457.227437	43.662772
3503.451269	897399.932050	43.667777
3503.429645	897351.340946	43.672781
3503.348556	897300.054111	43.677786
3503.318611	897258.516187	43.682791
3503.341384	897204.409630	43.687796
3503.098261	897161.746765	43.692801
3503.430770	897115.703856	43.697805
3503.061976	897072.964411	43.702810
3503.305981	897020.848566	43.707815
3503.285074	896974.766124	43.712820
3502.870821	896936.863971	43.717825
3503.044838	896884.275314	43.722829
3503.249637	896848.106321	43.727834
3503.293570	896798.533484	43.732839
3503.461095	896752.514809	43.737844
3503.488464	896698.306040	43.742849
3503.364319	896647.889985	43.747853
3503.212105	896609.942469	43.752858
3503.399580	896554.932969	43.757863
3503.189026	896505.399496	43.762868
3503.004044	896464.171163	43.767873
3503.189965	896418.050117	43.772877
3503.132500	896371.485661	43.777882
3503.481759	896321.954980	43.782887
3503.493840	896279.146791	43.787892
3503.189190	896227.114046	43.792897
3503.454014	896186.582622	43.797901
3503.166401	896134.546220	43.802906
3502.995555	896089.544224	43.807911
3503.249307	896041.283043	43.812916
3503.023481	896009.334850	43.817921
3503.533222	895953.203458	43.822925
3503.523538	895909.719629	43.827930
3503.611473	895853.270206	43.832935
3503.555488	895812.305788	43.837940
3503.297862	895765.479425	43.842945
3503.547761	895692.670000	43.847949
3503.689696	895672.352566	43.852954
3503.411103	895618.087246	43.857959
3503.641368	895558.035766	43.862964
3502.970033	895513.981429	43.867969
3503.265357	895453.048347	43.872973
3502.988597	895421.491805	43.877978
3502.907791	895375.986099	43.882983
3503.106068	895338.262262	43.887988
3502.934886	895296.056719	43.892993
3503.171352	895243.925804	43.897997
3503.136234	895224.602402	43.903002
3503.174594	895168.444280	43.908007
3503.166928	895112.099891	43.913012
3502.939078	895079.953501	43.918017
3503.353128	895021.122507	43.923021
3502.983542	894993.638175	43.928026
3502.899896	894934.791635	43.933031
3502.993120	894903.654515	43.938036
3502.827013	894861.928170	43.943041
3502.651563	894821.942819	43.948045
3502.664282	894793.524651	43.953050
3502.765475	894751.946768	43.958055
3502.891658	894714.327327	43.963060
3502.651489	894686.143597	43.968065
3502.672867	894642.644953	43.973069
3502.825904	894596.031258	43.978074
3502.748569	894573.039623	43.983079
3502.690761	894539.412296	43.988084
3502.869548	894506.712378	43.993089
3502.917870	894463.884539	43.998093
3503.001758	894416.507492	44.003098
3502.604601	894380.808613	44.008103
3502.892259	894339.003672	44.013108
3502.748733	894317.955142	44.018113
3502.941071	894271.912290	44.023117
3502.783833	894237.332934	44.028122
3502.908464	894204.350213	44.033127
3503.027417	894163.635083	44.038132
3502.851019	894130.314871	44.043137
3502.863734	894087.200071	44.048141
3502.692915	894057.841812	44.053146
3502.885147	894000.196817	44.058151
3503.210068	893957.802939	44.063156
3502.915933	893916.960769	44.068161
3503.007067	893876.248170	44.073165
3502.972853	893847.059656	44.078170
3502.721789	893806.306266	44.083175
3503.022393	893760.241444	44.088180
3502.852897	893717.443881	44.093185
3503.027887	893670.238964	44.098189
3503.065362	893648.094735	44.103194
3503.030454	893601.987240	44.108199
3503.113638	893557.310037	44.113204
3502.665907	893511.656525	44.118209
3502.972396	893479.219702	44.123213
3502.880552	893439.984276	44.128218
3502.619591	893396.909344	44.133223
3502.977179	893358.276052	44.138228
3502.966013	893330.434590	44.143233
3502.904055	893285.779174	44.148237
3503.028382	893256.851557	44.153242
3502.853376	893212.600913	44.158247
3502.900428	893171.697187	44.163252
3502.676665	893144.469931	44.168257
3502.491402	893079.820057	44.173261
3502.843996	893065.743004	44.178266
3502.618627	893037.355304	44.183271
3502.779202	892988.793556	44.188276
3502.866215	892964.124716	44.193281
3502.781187	892915.216067	44.198285
3502.846775	892877.594491	44.203290
3502.628264	892853.845688	44.208295
3502.842274	892811.558261	44.213300
3502.769475	892781.693840	44.218305
3503.157948	892735.799656	44.223309
3502.767297	892712.465379	44.228314
3503.196429	892669.658015	44.233319
3502.953899	892625.123871	44.238324
3503.012857	892595.913605	44.243329
3503.261453	892540.758553	44.248333
3502.717682	892501.107669	44.253338
3502.705441	892463.786269	44.258343
3502.805025	892424.318935	44.263348
3502.891931	892382.822830	44.268353
3502.562239	892334.432990	44.273357
3502.718728	892317.872329	44.278362
3502.529350	892283.963289	44.283367
3502.574487	892250.208805	44.288372
3502.397424	892213.976594	44.293377
3502.801948	892180.355882	44.298381
3502.599811	892142.580181	44.303386
3502.523988	892123.833162	44.308391
3502.580296	892073.153435	44.313396
3502.441232	892060.702117	44.318401
3502.994201	892010.616910	44.323405
3502.630231	891987.371970	44.328410
3502.764418	891946.445118	44.333415
3502.697850	891901.586235	44.338420
3502.465107	891875.224728	44.343425
3502.903590	891835.890906	44.348429
3502.934604	891809.485640	44.353434
3502.695003	891775.871974	44.358439
3502.753532	891734.569252	44.363444
3502.630006	891701.516257	44.368449
3502.872201	891670.433659	44.373453
3502.423853	891636.176616	44.378458
3502.713982	891606.633090	44.383463
3502.994895	891578.638263	44.388468
3502.621101	891541.853956	44.393473
3502.825146	891496.367059	44.398477
3502.617040	891461.102288	44.403482
3502.748368	891430.713627	44.408487
3502.833091	891390.564638	44.413492
3502.827485	891354.298732	44.418497
3502.828117	891316.097316	44.423501
3502.514089	891282.202871	44.428506
3502.654372	891252.295355	44.433511
3502.521648	891220.111520	44.438516
3502.735648	891175.877725	44.443521
3502.437875	891141.206046	44.448525
3502.521394	891115.949520	44.453530
3502.448972	891088.784244	44.458535
3502.553148	891053.465512	44.463540
3502.297879	891032.810139	44.468545
3502.179279	891002.750538	44.473549
3502.359265	890965.290977	44.478554
3502.158911	890945.399990	44.483559
3502.488268	890915.556286	44.488564
3502.225857	890906.701394	44.493569
3502.382891	890875.918679	44.498573
3502.222870	890834.452035	44.503578
3502.183960	890814.340552	44.508583
3502.524891	890783.623765	44.513588
3502.191190	890770.718096	44.518593
3502.250417	890727.376839	44.523597
3502.389832	890711.201240	44.528602
3502.032095	890682.436755	44.533607
3502.600820	890660.096706	44.538612
3502.296813	890627.357417	44.543617
3502.444431	890597.445279	44.548621
3502.720781	890562.965683	44.553626
3502.327706	890544.942839	44.558631
3502.498417	890502.258593	44.563636
3502.139369	890483.649590	44.568641
3502.357697	890448.211598	44.573645
3502.287743	890431.682798	44.578650
3502.314142	890399.855049	44.583655
3502.521352	890362.967440	44.588660
3502.279671	890342.307336	44.593665
3502.288277	890315.221774	44.598669
3502.240160	890282.922005	44.603674
3502.194254	890261.648975	44.608679
3502.589649	890236.627387	44.613684
3502.600554	890208.670365	44.618689
3502.442558	890169.036471	44.623693
3502.131249	890144.421110	44.628698
3502.201668	890127.578109	44.633703
3502.524440	890086.800377	44.638708
3502.277654	890061.787098	44.643713
3502.411938	890038.355408	44.648717
3502.328482	890014.185619	44.653722
3502.147833	889988.290511	44.658727
3502.321732	889959.725012	44.663732
3502.268806	889939.612772	44.668737
3502.410514	889906.892670	44.673741
3502.582273	889877.649961	44.678746
3502.325271	889850.799442	44.683751
3502.652260	889806.246267	44.688756
3502.236947	889797.414847	44.693761
3502.489026	889764.095318	44.698765
3502.493768	889738.942451	44.703770
3502.543134	889706.623380	44.708775
3502.470633	889672.389398	44.713780
3502.358412	889643.772729	44.718785
3502.289962	889611.569275	44.723789
3502.480134	889584.160127	44.728794
3502.302052	889563.196512	44.733799
3502.466200	889534.050052	44.738804
3501.856043	889511.029092	44.743809
3502.018079	889477.239021	44.748813
3502.455295	889447.660160	44.753818
3502.173612	889434.355928	44.758823
3501.804966	889412.649203	44.763828
3501.673431	889397.288507	44.768833
3502.278300	889377.356158	44.773837
3502.296517	889349.103513	44.778842
3502.174855	889335.772687	44.783847
3502.466409	889298.187129	44.788852
3502.200781	889286.040867	44.793857
3502.263140	889244.816338	44.798861
3502.365947	889222.353987	44.803866
3502.602707	889185.453956	44.808871
3502.364950	889159.177522	44.813876
3502.121987	889136.868553	44.818881
3502.142794	889111.226546	44.823885
3502.189999	889085.773576	44.828890
3502.027982	889064.321741	44.833895
3502.435963	889050.612741	44.838900
3501.889841	889020.419691	44.843905
3502.137794	889010.994020	44.848909
3502.338263	888984.644588	44.853914
3502.110194	888953.818275	44.858919
3502.177569	888928.845051	44.863924
3502.222867	888907.261720	44.868929
3502.286120	888881.998712	44.873933
3502.112003	888860.257848	44.878938
3502.138738	888839.354600	44.883943
3502.300860	888812.623682	44.888948
3502.197301	888782.646731	44.893953
3502.390870	888756.297392	44.898957
3502.157924	888732.533865	44.903962
3501.929078	888713.994419	44.908967
3502.407837	888679.953974	44.913972
3502.330051	888665.163008	44.918977
3502.438554	888640.278514	44.923981
3502.160685	888611.393724	44.928986
3502.038251	888600.867309	44.933991
3502.193179	888554.978183	44.938996
3502.027791	888552.683281	44.944001
3502.351411	888524.666550	44.949005
3502.117914	888496.838231	44.954010
3502.184529	888466.154274	44.959015
3502.366666	888431.967716	44.964020
3502.146548	888427.649794	44.969025
3502.327324	888385.722275	44.974029
3502.172351	888380.716251	44.979034
3502.118673	888342.794292	44.984039
3502.378258	888311.497142	44.989044
3502.320448	888289.638196	44.994049
3502.470900	888260.003728	44.999053
3502.356091	888238.250742	45.004058
3502.445503	888205.045761	45.009063
3502.630169	888186.630016	45.014068
3502.208825	888163.088706	45.019073
3502.077393	888134.177394	45.024077
3502.310231	888114.979354	45.029082
3502.150215	888095.071840	45.034087
3502.677889	888053.568588	45.039092
3502.354469	888024.107748	45.044097
3502.515692	888002.985773	45.049101
3502.581630	887971.041302	45.054106
3502.512339	887938.151238	45.059111
3502.337847	887907.504031	45.064116
3502.290950	887890.673814	45.069121
3502.249962	887868.810500	45.074125
3502.353365	887819.633806	45.079130
3502.307107	887804.448348	45.084135
3502.283092	887774.840133	45.089140
3502.334027	887766.606163	45.094145
3502.327997	887729.349725	45.099149
3502.423302	887716.947131	45.104154
3502.459974	887684.909124	45.109159
3502.545784	887646.378960	45.114164
3502.165307	887624.957752	45.119169
3502.090404	887596.324752	45.124173
3502.298096	887564.257899	45.129178
3502.166493	887550.634246	45.134183
3502.483750	887519.516854	45.139188
3502.424087	887492.622807	45.144193
3502.479332	887466.096813	45.149197
3502.203467	887441.367252	45.154202
3502.292714	887413.964415	45.159207
3502.439653	887376.583719	45.164212
3501.440753	887363.296072	45.169217
3501.730268	887328.794951	45.174221
3502.375891	887315.720150	45.179226
3502.469199	887304.381579	45.184231
3502.691023	887275.407760	45.189236
3502.234204	887261.837006	45.194241
3502.185045	887229.810614	45.199245
3502.702797	887210.852975	45.204250
3502.143392	887177.265067	45.209255
3502.151217	887151.035786	45.214260
3502.192509	887121.800592	45.219265
3502.129911	887109.809843	45.224269
3502.267682	887077.171107	45.229274
3502.059848	887056.203258	45.234279
3502.221726	887025.592729	45.239284
3502.010161	887002.108892	45.244289
3502.260175	886991.518172	45.249293
3502.412898	886951.907711	45.254298
3502.319534	886946.019210	45.259303
3502.278914	886908.569602	45.264308
3502.013371	886885.190969	45.269313
3502.141718	886857.682265	45.274317
3502.305619	886834.135884	45.279322
3502.175647	886824.575344	45.284327
3502.376200	886786.988425	45.289332
3502.175020	886767.373474	45.294337
3502.209021	886742.977021	45.299341
3502.450702	886710.706255	45.304346
3502.277821	886683.827095	45.309351
3502.459054	886659.502823	45.314356
3502.255168	886648.889469	45.319361
3502.016318	886614.471139	45.324365
3501.985023	886595.892324	45.329370
3501.696149	886567.676644	45.334375
3502.273861	886541.834668	45.339380
3502.198253	886528.973721	45.344385
3501.941599	886493.105703	45.349389
3502.430205	886475.505577	45.354394
3502.181110	886461.511533	45.359399
3502.582276	886419.243046	45.364404
3502.154191	886403.632836	45.369409
3502.151970	886385.435736	45.374413
3502.224727	886361.128083	45.379418
3501.910534	886327.494824	45.384423
3502.487146	886322.269677	45.389428
3502.012413	886285.855523	45.394433
3502.143214	886254.955645	45.399437
3501.947236	886243.469062	45.404442
3502.045721	886213.832663	45.409447
3502.317340	886187.168353	45.414452
3501.926917	886177.552852	45.419457
3502.376936	886154.053365	45.424461
3502.102504	886124.865148	45.429466
3502.088391	886100.183512	45.434471
3502.149472	886090.299877	45.439476
3502.151908	886064.066553	45.444481
3502.030708	886040.563916	45.449485
3501.772524	886020.084606	45.454490
3502.029232	885994.777091	45.459495
3502.385103	885972.454006	45.464500
3502.367596	885959.775824	45.469505
3502.130155	885925.837174	45.474509
3502.498894	885902.640471	45.479514
3502.064549	885878.220731	45.484519
3502.055811	885851.601068	45.489524
3501.964245	885830.900027	45.494529
3502.225562	885804.816486	45.499533
3502.162056	885794.856068	45.504538
3501.989433	885770.199140	45.509543
3502.182306	885752.742355	45.514548
3502.198466	885724.665915	45.519553
3502.329485	885709.445742	45.524557
3502.153676	885682.756022	45.529562
3502.002420	885654.803633	45.534567
3502.037647	885632.144835	45.539572
3502.046267	885615.492459	45.544577
3502.380804	885589.879930	45.549581
3502.083779	885566.501145	45.554586
3501.661049	885535.591819	45.559591
3502.274362	885522.131080	45.564596
3502.105878	885504.926705	45.569601
3501.923648	885486.659627	45.574605
3502.093413	885478.402822	45.579610
3502.251949	885455.142153	45.584615
3502.302328	885420.959500	45.589620
3502.174820	885398.520224	45.594625
3502.110005	885368.325532	45.599629
3502.604171	885342.298361	45.604634
3502.440839	885322.188203	45.609639
3502.527297	885298.357901	45.614644
3502.027506	885274.430460	45.619649
3502.370407	885237.778178	45.624653
3502.390970	885215.120167	45.629658
3502.440126	885202.719790	45.634663
3502.364122	885167.588312	45.639668
3502.379357	885147.448128	45.644673
3502.441414	885124.976561	45.649677
3502.469861	885080.242490	45.654682
3501.847976	885057.689710	45.659687
3502.008373	885037.815682	45.664692
3501.910873	885027.085000	45.669697
3501.763248	884983.831468	45.674701
3502.028823	884969.264918	45.679706
3501.955196	884971.697600	45.684711
3502.198105	884938.545394	45.689716
3501.852717	884929.307667	45.694721
3501.854854	884905.489643	45.699725
3502.213483	884869.510188	45.704730
3501.971604	884867.129587	45.709735
3502.333867	884840.347335	45.714740
3502.140888	884818.110240	45.719745
3502.264321	884790.205244	45.724749
3502.326787	884759.599123	45.729754
3502.287860	884746.050410	45.734759
3502.222929	884706.557280	45.739764
3502.041778	884690.901751	45.744769
3501.825852	884676.316974	45.749773
3502.325235	884642.055755	45.754778
3502.067124	884645.971338	45.759783
3502.631268	884624.673832	45.764788
3502.405000	884592.758852	45.769793
3502.292095	884565.182190	45.774797
3502.275551	884532.748196	45.779802
3501.953195	884507.239122	45.784807
3501.985177	884456.496388	45.789812
3502.016419	884388.905126	45.794817
3501.433191	884255.182193	45.799821
3502.187993	884056.744347	45.804826
3501.597749	883814.072640	45.809831
3501.583529	883503.021509	45.814836
3501.567983	883148.565521	45.819841
3501.442964	882720.495373	45.824845
3501.611667	882231.611465	45.829850
3501.152679	881689.122153	45.834855
3501.268041	881087.970287	45.839860
3500.999350	880417.249763	45.844865
3500.726742	879689.084398	45.849869
3500.792192	878897.290610	45.854874
3500.372920	878048.957653	45.859879
3500.344755	877123.266779	45.864884
3499.737887	876134.789475	45.869889
3499.314703	875079.392576	45.874893
3498.998740	873964.134358	45.879898
3498.055688	872793.759479	45.884903
3498.066608	871539.348450	45.889908
3497.877065	870223.751715	45.894913
3497.293232	868844.340265	45.899917
3496.695762	867374.206349	45.904922
3496.011448	865857.297758	45.909927
3495.585555	864260.198263	45.914932
3495.241242	862615.626215	45.919937
3494.194358	860887.608076	45.924941
3493.939738	859085.941224	45.929946
3493.188606	857223.809243	45.934951
3492.678220	855287.026362	45.939956
3491.951853	853279.298557	45.944961
3491.189465	851213.479409	45.949965
3490.873091	849061.870665	45.954970
3489.785628	846853.622749	45.959975
3489.160144	844563.816565	45.964980
3488.622294	842220.315467	45.969985
3487.612520	839801.063093	45.974989
3486.805205	837302.451221	45.979994
3485.625757	834754.944043	45.984999
3485.184701	832142.778241	45.990004
3483.963345	829450.157919	45.995009
3483.284207	826696.124205	46.000013
3482.364431	823870.370600	46.005018
3481.501731	820982.692368	46.010023
3480.169497	818024.246070	46.015028
3479.033713	815004.039994	46.020033
3477.993356	811922.604216	46.025037
3477.212887	808762.637715	46.030042
3475.834534	805567.373826	46.035047
3475.017395	802282.825825	46.040052
3473.457291	798948.350340	46.045057
3472.390886	795541.639458	46.050061
3471.568714	792064.753778	46.055066
3470.027479	788536.731766	46.060071
3468.823458	784929.605441	46.065076
3467.565896	781278.951852	46.070081
3465.908410	777544.023456	46.075085
3464.864105	773759.209023	46.080090
3463.546527	769911.143835	46.085095
3462.254622	765992.944233	46.090100
3460.916969	762014.543251	46.095105
3459.281892	757981.779483	46.100109
3458.255846	753876.612801	46.105114
3456.647311	749720.635437	46.110119
3454.835193	745500.725515	46.115124
3453.191447	741209.026360	46.120129
3451.662557	736869.800308	46.125133
3450.379570	732459.802581	46.130138
3448.383547	727992.229107	46.135143
3446.943782	723470.421511	46.140148
3445.546912	718887.361367	46.145153
3443.608146	714251.607924	46.150157
3441.856315	709544.664238	46.155162
3440.233277	704778.226428	46.160167
3438.328032	699954.483093	46.165172
3436.606995	695079.014891	46.170177
3434.447667	690140.578415	46.175181
3432.880843	685146.402957	46.180186
3431.035036	680100.213326	46.185191
3428.908693	674998.522840	46.190196
3426.798061	669838.986212	46.195201
3424.758475	664617.398213	46.200205
3423.133010	659328.599895	46.205210
3420.965929	653993.860266	46.210215
3418.879685	648602.150867	46.215220
3416.805575	643171.737009	46.220225
3414.211825	637687.330818	46.225229
3412.470449	632149.417599	46.230234
3409.982801	626566.137324	46.235239
3407.928980	620912.168286	46.240244
3405.853462	615232.597148	46.245249
3403.569604	609485.581939	46.250253
3401.552537	603691.870853	46.255258
3398.884674	597844.066055	46.260263
3396.507493	591950.576186	46.265268
3394.322452	586013.868366	46.270273
3391.260839	580023.401101	46.275277
3388.890673	573992.328763	46.280282
3386.161468	567925.909492	46.285287
3383.951445	561806.131229	46.290292
3381.636345	555646.888398	46.295297
3378.897271	549440.176769	46.300301
3376.076061	543185.081713	46.305306
3373.319845	536903.625856	46.310311
3370.687073	530569.534585	46.315316
3367.777658	524196.101981	46.320321
3364.716085	517791.407900	46.325325
3362.213245	511337.525883	46.330330
3359.433226	504859.831279	46.335335
3356.297679	498332.636031	46.340340
3353.527367	491787.862323	46.345345
3350.342411	485198.106315	46.350349
3347.501032	478560.633358	46.355354
3344.258543	471911.855631	46.360359
3341.497362	465224.431181	46.365364
3338.287800	458513.907674	46.370369
3335.283373	451760.000763	46.375373
3332.095291	444979.344815	46.380378
3328.764506	438176.096321	46.385383
3325.515682	431333.225331	46.390388
3322.088967	424470.263102	46.395393
3318.719493	417597.644682	46.400397
3315.839111	410689.722788	46.405402
3312.108148	403759.245572	46.410407
3308.412381	396811.977080	46.415412
3305.035897	389847.789592	46.420417
3301.861349	382849.235246	46.425421
3298.244384	375822.864660	46.430426
3294.577637	368805.810002	46.435431
3290.560059	361750.826780	46.440436
3287.135468	354691.303438	46.445441
3283.336384	347624.838003	46.450445
3280.109124	340537.743905	46.455450
3276.129872	333446.759092	46.460455
3272.516132	326340.025753	46.465460
3268.743972	319229.550015	46.470465
3264.606260	312102.341514	46.475469
3261.325547	304965.411692	46.480474
3257.069281	297838.374139	46.485479
3252.857302	290685.398700	46.490484
3249.006633	283537.917751	46.495489
3244.912920	276384.915501	46.500493
3241.196667	269236.973165	46.505498
3236.949607	262090.688205	46.510503
3232.706847	254941.273629	46.515508
3228.380978	247799.071272	46.520513
3224.056873	240666.218779	46.525517
3219.987039	233523.942891	46.530522
3215.735905	226388.219386	46.535527
3211.418171	219200.372899	46.540532
3206.964087	212080.592544	46.545537
3202.440994	204992.940799	46.550541
3198.027248	197897.474358	46.555546
3193.055464	190833.834312	46.560551
3188.886379	183781.333331	46.565556
3184.174957	176750.250702	46.570561
3179.587321	169743.326880	46.575565
3174.847399	162745.214114	46.580570
3170.220889	155786.471605	46.585575
3165.241378	148836.938558	46.590580
3160.191866	141930.730034	46.595585
3155.485831	135045.375220	46.600589
3150.696685	128169.817262	46.605594
3145.448503	121344.530766	46.610599
3140.255036	114552.722684	46.615604
3134.714362	107791.656762	46.620609
3129.605810	101094.496377	46.625613
3124.580993	94418.019659	46.630618
3118.569774	87789.983489	46.635623
3113.080801	81217.060976	46.640628
3107.017230	74691.113676	46.645633
3101.093233	68224.914948	46.650637
3094.810573	61827.725370	46.655642
3087.742904	55507.341087	46.660647
3079.342976	49292.827874	46.665652
3063.972087	43369.326856	46.670657
3045.395629	37691.136818	46.675661
3027.275190	32241.633008	46.680666
3009.286000	27085.560061	46.685671
2990.891838	22249.819196	46.690676
2970.644644	17826.387359	46.695681
2947.465032	13863.459158	46.700685
2922.803919	10358.580060	46.705690
2898.690455	7323.378185	46.710695
2875.585469	4746.564458	46.715700
2854.509342	2605.783626	46.720705
2834.463536	936.680225	46.725709
2793.727957	286.569418	46.730714
2752.287849	304.522206	46.735719
2737.497061	299.191849	46.740724
2743.277205	300.606282	46.745729
2758.567942	298.142931	46.750733
2776.141651	287.877318	46.755738
2788.650720	284.941570	46.760743
2794.609499	279.168171	46.765748
2795.700223	287.498888	46.770753
2792.561322	294.014509	46.775757
2789.262907	288.148314	46.780762
2785.349730	285.700892	46.785767
2781.524783	280.981708	46.790772
2778.729734	275.776060	46.795777
2776.005913	279.066108	46.800781
2773.336552	278.280727	46.805786
2770.719290	273.583706	46.810791
2768.136726	278.842428	46.815796
2765.854302	276.616938	46.820801
2762.926705	267.805224	46.825805
2760.123774	270.411318	46.830810
2756.753049	271.752989	46.835815
2753.883405	266.050524	46.840820
2750.349800	264.792839	46.845825
2746.993411	265.281603	46.850829
2744.305714	267.091161	46.855834
2741.108467	266.583535	46.860839
2737.869265	266.286096	46.865844
2734.407940	264.179763	46.870849
2731.006685	263.144564	46.875853
2728.087472	263.531208	46.880858
2724.937388	252.488381	46.885863
2721.935665	263.332399	46.890868
2718.243406	257.899891	46.895873
2714.737042	262.601425	46.900877
2711.533551	256.567682	46.905882
2708.251706	261.618173	46.910887
2705.338646	257.912118	46.915892
2701.902008	256.280883	46.920897
2697.923351	254.046026	46.925901
2694.784451	251.793768	46.930906
2691.170568	253.468066	46.935911
2687.973160	253.903402	46.940916
2685.002740	252.095392	46.945921
2681.453468	253.149642	46.950925
2677.874815	255.838790	46.955930
2674.591987	249.711603	46.960935
2671.142703	248.939338	46.965940
2668.149123	247.506953	46.970945
2664.388144	254.111075	46.975949
2661.377043	248.004181	46.980954
2657.537477	250.301851	46.985959
2653.823055	250.903832	46.990964
2650.816269	247.998307	46.995969
2647.458278	250.077585	47.000973
2643.978821	243.386897	47.005978
2640.086377	241.277975	47.010983
2636.972773	246.655562	47.015988
2633.847358	238.708592	47.020993
2630.287018	242.977431	47.025997
2627.163639	241.354942	47.031002
2623.833364	233.771350	47.036007
2619.927117	236.743120	47.041012
2616.619085	241.538280	47.046017
2613.182215	241.140535	47.051021
2609.177754	237.681755	47.056026
2605.871172	240.481161	47.061031
2602.447350	237.794078	47.066036
2599.060308	230.948461	47.071041
2595.209701	230.640323	47.076045
2591.899032	228.165071	47.081050
2588.911484	226.046966	47.086055
2585.149431	234.784576	47.091060
2581.986696	221.776074	47.096065
2578.618371	231.868384	47.101069
2575.562020	227.078583	47.106074
2571.692652	227.711327	47.111079
2568.223491	229.164484	47.116084
2564.870076	228.949947	47.121089
2561.091215	228.616970	47.126093
2557.801694	221.422576	47.131098
2554.309421	226.832703	47.136103
2550.748048	230.788384	47.141108
2547.145584	220.194142	47.146113
2543.779174	224.835578	47.151117
2540.149653	222.375097	47.156122
2536.432065	222.010319	47.161127
2533.401652	222.387011	47.166132
2529.949919	220.535398	47.171137
2526.607006	224.963785	47.176141
2522.987966	216.114432	47.181146
2519.878234	218.449222	47.186151
2516.057470	228.676231	47.191156
2512.692469	214.436214	47.196161
2508.821609	222.270242	47.201165
2505.398589	218.429442	47.206170
2502.018108	220.072057	47.211175
2498.257097	209.097113	47.216180
2495.562203	223.078027	47.221185
2492.263004	215.907383	47.226189
2488.440788	215.971170	47.231194
2484.390435	223.978507	47.236199
2480.834444	222.256622	47.241204
2477.762630	219.631119	47.246209
2474.217973	220.771582	47.251213
2471.094325	212.109285	47.256218
2467.286173	208.685720	47.261223
2463.773116	205.179903	47.266228
2460.167975	212.252174	47.271233
2456.805296	213.745058	47.276237
2453.865360	209.542361	47.281242
2449.953012	206.080359	47.286247
2446.333828	208.585719	47.291252
2442.865204	208.087166	47.296257
2439.014889	210.606607	47.301261
2435.700120	207.546829	47.306266
2432.530673	204.450240	47.311271
2428.564093	206.561439	47.316276
2425.598171	199.637180	47.321281
2422.434070	214.856326	47.326285
2418.768382	209.172618	47.331290
2415.146018	205.254479	47.336295
2411.211882	210.267763	47.341300
2407.737485	197.629964	47.346305
2404.296407	198.337382	47.351309
2401.400295	204.934868	47.356314
2397.983904	198.860538	47.361319
2394.454595	206.063601	47.366324
2390.811702	204.726342	47.371329
2387.034274	205.954230	47.376333
2383.554141	196.042877	47.381338
2380.198610	197.275128	47.386343
2376.283117	206.564500	47.391348
2372.754338	198.194919	47.396353
2369.417421	208.355954	47.401357
2366.201486	194.882017	47.406362
2363.180961	201.172671	47.411367
2359.373765	199.442815	47.416372
2355.689146	193.701706	47.421377
2352.130396	201.698426	47.426381
2348.681315	197.209245	47.431386
2345.173203	203.890819	47.436391
2341.500374	210.255625	47.441396
2338.069399	201.455903	47.446401
2334.451272	208.447515	47.451405
2331.270565	192.047148	47.456410
2327.795365	206.261127	47.461415
2324.513716	197.432819	47.466420
2321.185661	196.836948	47.471425
2317.039423	208.730872	47.476429
2313.891269	199.387181	47.481434
2310.303709	199.298895	47.486439
2306.626845	198.239047	47.491444
2303.239823	196.817776	47.496449
2299.620588	202.214684	47.501453
2296.274930	194.562659	47.506458
2292.466082	190.673829	47.511463
2289.503290	195.129786	47.516468
2285.953098	190.520590	47.521473
2281.848832	202.556006	47.526477
2278.603784	194.359498	47.531482
2275.453182	200.871779	47.536487
2271.895311	195.514557	47.541492
2268.419647	194.289894	47.546497
2264.913464	195.868957	47.551501
2261.716110	188.924019	47.556506
2258.264952	186.217830	47.561511
2254.206666	196.178528	47.566516
2251.018349	190.949954	47.571521
2246.980205	198.465836	47.576525
2243.732794	194.846864	47.581530
2240.364893	198.298767	47.586535
2237.245182	197.008450	47.591540
2233.628736	192.018709	47.596545
2229.539693	200.440908	47.601549
2226.259930	191.285572	47.606554
2222.733228	190.725132	47.611559
2218.967204	194.805005	47.616564
2215.811431	189.638574	47.621569
2212.206595	194.747610	47.626573
2209.186531	187.023347	47.631578
2205.692724	193.414331	47.636583
2201.825584	194.570342	47.641588
2198.448586	187.062302	47.646593
2194.801943	186.335594	47.651597
2191.600197	182.687414	47.656602
2188.088464	193.845166	47.661607
2184.302473	190.006919	47.666612
2180.774179	193.463636	47.671617
2177.301841	189.402709	47.676621
2173.989350	182.495202	47.681626
2170.475049	185.671957	47.686631
2166.990748	186.398517	47.691636
2163.323702	177.442167	47.696641
2159.517577	176.201898	47.701645
2156.337851	172.174966	47.706650
2153.012442	182.858936	47.711655
2149.322155	181.753867	47.716660
2145.995343	178.538024	47.721665
2142.390306	185.507069	47.726669
2138.789244	180.171299	47.731674
2135.785280	182.486682	47.736679
2132.130488	178.901514	47.741684
2128.939038	172.484577	47.746689
2124.828213	183.864427	47.751693
2121.156037	170.396387	47.756698
2117.514488	187.245982	47.761703
2114.168653	183.635661	47.766708
2111.188098	181.041317	47.771713
2107.594382	182.833469	47.776717
2103.897522	179.670868	47.781722
2100.446003	177.569310	47.786727
2096.425237	174.719509	47.791732
2093.575244	174.751329	47.796737
2089.846210	184.985945	47.801741
2086.418202	183.105678	47.806746
2082.711216	178.785000	47.811751
2079.241997	174.954919	47.816756
2076.310869	168.893265	47.821761
2072.704610	182.870494	47.826765
2069.408482	174.163982	47.831770
2065.272318	179.811188	47.836775
2061.747151	177.864497	47.841780
2058.489715	179.979253	47.846785
2054.946622	180.129108	47.851789
2051.457201	177.505368	47.856794
2047.663582	174.120604	47.861799
2044.107995	176.419983	47.866804
2040.875118	164.102586	47.871809
2037.320650	173.551406	47.876813
2034.005574	179.150853	47.881818
2030.695514	171.705702	47.886823
2026.773602	177.226186	47.891828
2023.222626	168.780453	47.896833
2019.866604	178.494497	47.901837
2016.852310	170.160237	47.906842
2013.205268	168.966435	47.911847
2009.297423	174.863896	47.916852
2005.760578	167.396426	47.921857
2002.082636	178.645273	47.926861
1998.847354	165.791541	47.931866
1995.433951	167.321527	47.936871
1992.016139	168.030916	47.941876
1988.638191	167.341690	47.946881
1984.819613	165.384513	47.951885
1981.386446	164.892476	47.956890
1977.995781	164.171613	47.961895
1974.153405	172.671063	47.966900
1971.054427	166.968734	47.971905
1966.922961	175.487521	47.976909
1963.878209	165.571129	47.981914
1960.660727	171.539906	47.986919
1957.383058	175.477147	47.991924
1953.852599	160.526929	47.996929
1949.814470	176.386344	48.001933
1946.344810	165.868992	48.006938
1942.849882	166.572997	48.011943
1939.172580	171.069407	48.016948
1935.830083	168.050294	48.021953
1932.261084	168.460270	48.026957
1929.130615	170.626958	48.031962
1925.639020	165.481873	48.036967
1921.670295	177.212552	48.041972
1918.781716	169.752732	48.046977
1915.114612	171.923012	48.051981
1911.697333	166.020311	48.056986
1908.356406	160.871864	48.061991
1904.230853	170.125401	48.066996
1900.891580	170.772349	48.072001
1897.276778	166.861077	48.077005
1893.626837	174.968459	48.082010
1890.430274	168.792114	48.087015
1886.765300	174.898395	48.092020
1883.690585	164.147136	48.097025
1880.066864	170.071566	48.102029
1876.238438	173.804022	48.107034
1872.843304	166.651493	48.112039
1869.029390	165.872744	48.117044
1865.918543	162.261882	48.122049
1862.482440	170.670425	48.127053
1858.934749	165.261145	48.132058
1855.380484	165.668350	48.137063
1852.033421	173.022411	48.142068
1848.558775	169.694252	48.147073
1844.934248	164.687422	48.152077
1841.392887	170.506117	48.157082
1837.855446	168.616485	48.162087
1834.207720	163.182507	48.167092
1830.721636	159.371983	48.172097
1826.871901	164.198688	48.177101
1823.722076	163.117870	48.182106
1820.454998	162.027216	48.187111
1816.673936	172.705538	48.192116
1813.477817	161.700680	48.197121
1809.764723	171.077968	48.202125
1806.578973	170.618794	48.207130
1803.128512	167.472372	48.212135
1799.268539	163.569119	48.217140
1795.851372	169.389036	48.222145
1792.657687	160.190435	48.227149
1788.955228	164.811682	48.232154
1785.444231	161.873404	48.237159
1781.623816	167.196542	48.242164
1778.121410	160.413472	48.247169
1774.547751	163.571494	48.252173
1770.861755	160.295679	48.257178
1768.224652	157.563126	48.262183
1764.576533	163.237690	48.267188
1761.095552	160.952795	48.272193
1756.771039	162.317330	48.277197
1753.666212	164.413784	48.282202
1750.723972	158.362086	48.287207
1747.013667	166.065518	48.292212
1743.767791	152.085964	48.297217
1739.866210	148.633456	48.302221
1736.273160	155.583419	48.307226
1732.647692	159.249496	48.312231
1728.940230	169.696473	48.317236
1725.738268	158.779284	48.322241
1722.411418	168.637475	48.327245
1718.963114	157.349538	48.332250
1715.433488	158.723685	48.337255
1711.698987	167.442700	48.342260
1708.379102	160.135000	48.347265
1704.748561	169.259546	48.352269
1701.397909	162.554081	48.357274
1697.912979	159.805549	48.362279
1694.252964	166.951318	48.367284
1691.028901	157.525549	48.372289
1687.342029	166.548507	48.377293
1684.001195	164.409043	48.382298
1680.054509	165.285957	48.387303
1676.182240	166.652215	48.392308
1673.221490	164.684795	48.397313
1670.080049	165.403216	48.402317
1666.401971	162.507831	48.407322
1662.822792	160.730018	48.412327
1659.296701	160.790924	48.417332
1656.104687	154.172363	48.422337
1651.998634	166.561743	48.427341
1648.482085	164.115665	48.432346
1645.113909	161.031745	48.437351
1641.874020	165.853340	48.442356
1638.630525	160.560533	48.447361
1634.798987	167.332312	48.452365
1631.234779	159.374948	48.457370
1627.847728	152.572154	48.462375
1624.137467	164.230532	48.467380
1621.133298	157.219827	48.472385
1617.023242	159.044769	48.477389
1613.458118	149.939854	48.482394
1610.082468	158.093270	48.487399
1606.431728	165.103575	48.492404
1603.185612	156.878379	48.497409
1599.457697	157.987987	48.502413
1596.143798	154.488027	48.507418
1592.973853	145.823810	48.512423
1589.284425	153.074756	48.517428
1585.797980	152.930249	48.522433
1582.137971	158.677554	48.527437
1578.705900	160.968305	48.532442
1575.719317	151.185476	48.537447
1571.488803	157.744386	48.542452
1568.349244	149.845575	48.547457
1564.473159	154.808063	48.552461
1560.994116	155.899073	48.557466
1557.864374	151.760316	48.562471
1554.086902	159.033338	48.567476
1550.615396	155.415991	48.572481
1546.798606	148.089302	48.577485
1543.922772	154.357082	48.582490
1540.477239	154.844239	48.587495
1536.313922	162.954208	48.592500
1533.121230	156.287109	48.597505
1529.931843	154.771386	48.602509
1526.579183	156.393886	48.607514
1522.740554	146.131866	48.612519
1518.776988	154.755858	48.617524
1515.461234	148.805125	48.622529
1512.196805	154.999991	48.627533
1508.946408	150.219335	48.632538
1505.396300	152.085829	48.637543
1501.375810	148.491560	48.642548
1497.756884	149.570409	48.647553
1494.590320	164.219081	48.652557
1491.092407	159.751865	48.657562
1487.908661	156.089182	48.662567
1483.947527	156.581075	48.667572
1480.922750	149.104414	48.672577
1477.378653	154.945120	48.677581
1473.633203	161.359816	48.682586
1470.241223	157.261105	48.687591
1466.377748	158.903735	48.692596
1463.275975	156.903913	48.697601
1459.638696	157.376642	48.702605
1456.069709	151.085166	48.707610
1452.761109	151.466677	48.712615
1448.806762	158.068456	48.717620
1445.562136	149.573973	48.722625
1441.856747	147.927507	48.727629
1438.702117	153.908118	48.732634
1435.514201	150.270832	48.737639
1431.518788	155.181117	48.742644
1428.159999	149.922724	48.747649
1423.985472	157.300142	48.752653
1421.032341	151.896956	48.757658
1417.581996	154.763517	48.762663
1413.773268	158.005844	48.767668
1410.610848	142.864278	48.772673
1407.424106	150.080026	48.777677
1404.043496	154.240661	48.782682
1400.439455	158.189187	48.787687
1396.416930	156.829217	48.792692
1392.818743	140.704525	48.797697
1389.025179	154.863085	48.802701
1385.711716	146.637950	48.807706
1382.787180	142.590320	48.812711
1378.898609	151.309966	48.817716
1375.873169	146.181226	48.822721
1372.044274	147.734152	48.827725
1368.463641	151.651598	48.832730
1365.272152	145.768260	48.837735
1361.538557	146.359995	48.842740
1357.890133	149.514300	48.847745
1354.136486	154.148670	48.852749
1350.721715	153.848831	48.857754
1347.630002	143.890756	48.862759
1344.083447	151.581217	48.867764
1340.729827	151.670690	48.872769
1337.255125	146.510464	48.877773
1333.492648	149.313433	48.882778
1329.962759	143.607816	48.887783
1326.146394	141.343573	48.892788
1323.111062	142.081194	48.897793
1319.684243	149.417589	48.902797
1315.901316	148.262194	48.907802
1312.804691	144.562744	48.912807
1308.774051	153.155162	48.917812
1305.241033	147.211105	48.922817
1301.814747	149.506622	48.927821
1298.552432	155.894864	48.932826
1295.339907	142.152913	48.937831
1291.367162	143.146353	48.942836
1288.084054	129.570011	48.947841
1284.262333	142.083148	48.952845
1281.112919	150.055711	48.957850
1277.364548	143.330102	48.962855
1273.646900	150.616724	48.967860
1270.409009	144.275609	48.972865
1267.207585	135.243887	48.977869
1263.777533	140.884732	48.982874
1259.899563	150.800753	48.987879
1256.425169	151.650468	48.992884
1253.021950	142.941804	48.997889
1249.427641	148.562454	49.002893
1245.755276	147.584008	49.007898
1242.306107	138.554187	49.012903
1238.869411	154.179866	49.017908
1235.542594	144.561290	49.022913
1231.943675	146.029938	49.027917
1228.349782	141.279446	49.032922
1225.025807	135.698735	49.037927
1221.242145	144.961001	49.042932
1218.082057	143.909926	49.047937
1214.402144	141.665648	49.052941
1211.119344	143.122900	49.057946
1207.780772	141.880716	49.062951
1203.721061	141.939808	49.067956
1200.240534	136.921954	49.072961
1196.638358	146.332234	49.077965
1193.061182	150.234241	49.082970
1189.834446	137.569040	49.087975
1186.087951	140.153596	49.092980
1182.716780	136.483253	49.097985
1179.473548	136.951638	49.102989
1175.731832	137.610975	49.107994
1172.610309	134.448952	49.112999
1168.569477	143.149920	49.118004
1165.857768	143.350071	49.123009
1162.172403	146.172593	49.128013
1158.121165	134.804479	49.133018
1154.740863	149.068130	49.138023
1151.077038	147.992246	49.143028
1147.984903	139.000763	49.148033
1144.575141	140.122858	49.153037
1141.038970	148.218060	49.158042
1137.441447	138.473236	49.163047
1133.280037	141.843757	49.168052
1130.125184	135.300766	49.173057
1126.668859	138.010654	49.178061
1123.021565	136.406354	49.183066
1120.004060	132.403682	49.188071
1116.299612	135.822392	49.193076
1113.425691	129.542787	49.198081
1109.737324	135.017861	49.203085
1105.628483	132.088005	49.208090
1102.444369	129.696724	49.213095
1098.564115	144.512337	49.218100
1095.374875	131.667563	49.223105
1091.857364	128.485825	49.228109
1087.966554	140.269324	49.233114
1084.740421	136.577840	49.238119
1081.074963	138.874386	49.243124
1077.868644	132.604575	49.248129
1074.580277	133.120557	49.253133
1070.514797	133.173620	49.258138
1067.501132	130.572038	49.263143
1063.587575	130.758644	49.268148
1060.145888	130.370531	49.273153
1056.853609	126.137858	49.278157
1053.398077	136.958032	49.283162
1049.955303	127.020167	49.288167
1045.946118	136.678016	49.293172
1042.591167	124.111707	49.298177
1038.962475	121.212831	49.303181
1035.580728	133.210756	49.308186
1032.420920	121.777466	49.313191
1028.816555	131.200647	49.318196
1025.237272	136.729382	49.323201
1021.564110	124.591639	49.328205
1018.663361	134.443917	49.333210
1015.003066	132.189065	49.338215
1011.559667	129.795932	49.343220
1007.949604	129.770583	49.348225
1003.983016	133.944328	49.353229
1000.548399	135.124908	49.358234
997.029066	126.061522	49.363239
993.131969	136.210598	49.368244
990.038663	125.772367	49.373249
986.876784	126.906671	49.378253
983.128946	139.365768	49.383258
979.868659	132.701799	49.388263
975.975125	136.417703	49.393268
972.733138	139.106073	49.398273
969.139528	137.527359	49.403277
965.447302	132.017030	49.408282
962.247841	137.651722	49.413287
958.662078	138.003649	49.418292
955.474938	131.743985	49.423297
951.704838	137.486078	49.428301
947.885991	140.727293	49.433306
944.434552	140.284640	49.438311
940.947735	141.008775	49.443316
937.694322	132.820852	49.448321
934.498361	136.645599	49.453325
930.777747	136.847181	49.458330
927.220871	131.188996	49.463335
923.453643	141.043535	49.468340
920.115286	141.883045	49.473345
916.538474	132.859621	49.478349
913.094982	139.458637	49.483354
909.927891	127.522649	49.488359
905.936968	145.633680	49.493364
902.592104	136.595191	49.498369
899.414805	135.112654	49.503373
895.498165	136.445064	49.508378
892.213470	132.756308	49.513383
888.555733	133.085069	49.518388
885.025722	132.344653	49.523393
881.541891	132.090140	49.528397
877.763013	133.446549	49.533402
874.554219	139.567896	49.538407
870.936265	136.465704	49.543412
867.765116	134.881137	49.548417
864.124237	137.016512	49.553421
859.763449	133.978387	49.558426
856.970076	129.608491	49.563431
853.774163	137.501779	49.568436
850.832689	129.479010	49.573441
846.857250	136.108433	49.578445
842.830848	143.975700	49.583450
839.578971	137.174486	49.588455
836.052059	127.927590	49.593460
832.476758	140.722342	49.598465
828.994596	136.144339	49.603469
825.262668	135.027894	49.608474
821.791274	134.903192	49.613479
818.369054	142.741584	49.618484
815.004473	132.065183	49.623489
811.875523	135.341778	49.628493
807.932206	141.194729	49.633498
804.640574	136.045712	49.638503
800.909822	134.734519	49.643508
797.578260	130.404352	49.648513
794.283583	134.659732	49.653517
790.563043	138.757439	49.658522
786.972303	133.002557	49.663527
783.169161	141.455145	49.668532
779.940340	136.389294	49.673537
776.158212	139.076375	49.678541
772.778906	140.543195	49.683546
769.671071	124.524496	49.688551
766.040322	145.528792	49.693556
762.465988	131.888799	49.698561
759.376237	130.158632	49.703565
755.391387	137.168376	49.708570
752.025666	130.375017	49.713575
748.175585	129.083216	49.718580
745.165990	134.837406	49.723585
741.795603	136.374998	49.728589
738.068424	136.171511	49.733594
734.457412	125.852281	49.738599
730.681921	132.167123	49.743604
727.294674	122.281731	49.748609
723.740324	126.261418	49.753613
720.404967	115.465822	49.758618
717.166874	117.699455	49.763623
713.255267	138.262815	49.768628
710.104449	125.755976	49.773633
706.556035	128.331436	49.778637
702.959280	135.905930	49.783642
699.659262	123.029507	49.788647
695.785120	129.616246	49.793652
692.673067	128.003088	49.798657
688.575969	127.855710	49.803661
685.140668	135.545985	49.808666
681.964724	121.289798	49.813671
678.230986	123.652030	49.818676
674.806276	129.399754	49.823681
671.494962	128.670294	49.828685
667.765182	128.904200	49.833690
664.090554	126.865537	49.838695
660.735021	137.780527	49.843700
657.724584	127.037191	49.848705
654.031699	127.636787	49.853709
650.264987	128.734047	49.858714
647.139948	124.127505	49.863719
643.362759	128.493210	49.868724
640.171941	132.316714	49.873729
636.495212	129.689175	49.878733
632.630213	126.470193	49.883738
629.514834	127.434646	49.888743
625.657191	130.785160	49.893748
622.189800	126.744999	49.898753
618.995180	137.236944	49.903757
615.284932	130.907808	49.908762
612.041182	129.109887	49.913767
608.076880	127.713774	49.918772
604.661839	125.226093	49.923777
601.321762	130.971115	49.928781
598.042052	131.617244	49.933786
594.510811	124.132906	49.938791
590.709133	123.876356	49.943796
587.114225	127.618359	49.948801
584.029185	123.773872	49.953805
580.179866	132.235041	49.958810
576.811663	132.082014	49.963815
573.150366	125.419214	49.968820
569.872027	126.878162	49.973825
566.059722	124.621614	49.978829
562.787876	126.865483	49.983834
559.443475	123.705864	49.988839
555.243224	132.459557	49.993844
551.788466	127.758458	49.998849
549.023465	126.816544	50.003853
545.473248	126.830610	50.008858
542.755915	116.976418	50.013863
538.159669	133.385787	50.018868
534.500997	126.867037	50.023873
531.153523	123.740116	50.028877
527.510587	123.416899	50.033882
524.291669	122.222732	50.038887
520.803216	129.920139	50.043892
517.495243	120.396162	50.048897
513.915895	122.252272	50.053901
510.076219	135.602679	50.058906
506.501075	115.613989	50.063911
503.233070	130.567873	50.068916
499.829436	118.089243	50.073921
496.364275	122.331602	50.078925
492.630232	127.183236	50.083930
489.278267	115.099027	50.088935
485.285392	126.950378	50.093940
482.129091	118.924964	50.098945
478.955015	117.887792	50.103949
475.155756	122.450675	50.108954
471.597899	115.983188	50.113959
468.116456	119.792939	50.118964
464.931489	118.983332	50.123969
461.206029	122.432090	50.128973
457.471610	117.304144	50.133978
454.281250	114.709351	50.138983
450.593923	120.649289	50.143988
447.195507	118.340535	50.148993
444.498128	124.332338	50.153997
440.527218	121.927707	50.159002
436.823635	122.343168	50.164007
433.044856	120.506451	50.169012
429.513145	125.880742	50.174017
426.221699	117.833537	50.179021
422.124292	116.621244	50.184026
419.121190	113.063274	50.189031
415.692809	122.814350	50.194036
411.962991	121.979908	50.199041
408.534122	131.884602	50.204045
404.982407	124.438553	50.209050
401.448270	115.938986	50.214055
398.068076	122.403959	50.219060
394.617343	121.488020	50.224065
391.217840	120.734102	50.229069
387.442129	117.843935	50.234074
384.191110	123.114182	50.239079
380.671180	124.004474	50.244084
377.276112	122.072528	50.249089
373.579456	119.655327	50.254093
369.869172	125.355420	50.259098
366.963260	118.924966	50.264103
362.964265	117.741829	50.269108
359.468387	118.555538	50.274113
355.924998	120.046279	50.279117
352.161893	126.451329	50.284122
349.081282	109.116625	50.289127
345.849378	125.270539	50.294132
342.328267	117.448099	50.299137
338.819741	115.804920	50.304141
334.951025	116.918544	50.309146
331.853503	114.467728	50.314151
327.973056	124.947464	50.319156
324.355364	121.205547	50.324161
320.751391	117.765259	50.329165
317.508494	125.123597	50.334170
314.137079	117.420064	50.339175
310.207123	119.150653	50.344180
306.990720	118.043655	50.349185
303.624245	117.736042	50.354189
300.086614	126.652795	50.359194
296.792136	123.111963	50.364199
293.226705	128.581531	50.369204
289.373545	125.127460	50.374209
286.359547	113.418672	50.379213
282.167109	117.339941	50.384218
279.017658	117.224148	50.389223
275.493276	122.038883	50.394228
272.021295	122.472783	50.399233
268.493098	122.721419	50.404237
264.759459	123.388474	50.409242
261.327645	114.665685	50.414247
257.775286	120.010371	50.419252
254.381314	113.696711	50.424257
251.217171	115.170933	50.429261
247.509345	114.744440	50.434266
244.517781	115.129224	50.439271
240.614979	119.740423	50.444276
236.985270	111.716819	50.449281
233.750248	112.099289	50.454285
229.328007	123.729666	50.459290
226.617870	116.136967	50.464295
222.777992	111.309086	50.469300
219.425934	108.781499	50.474305
216.061654	109.833232	50.479309
212.126302	110.186416	50.484314
209.176279	104.565754	50.489319
205.187634	111.349842	50.494324
201.565849	115.018255	50.499329
198.556890	117.379501	50.504333
194.996283	123.753719	50.509338
191.551022	111.131902	50.514343
187.766935	113.350537	50.519348
184.274078	117.874776	50.524353
181.013024	101.623087	50.529357
177.421344	118.680262	50.534362
174.103281	101.664661	50.539367
170.375178	113.060582	50.544372
166.841910	120.010262	50.549377
163.316985	112.988812	50.554381
159.493790	118.469187	50.559386
156.430223	110.004817	50.564391
152.834097	116.186426	50.569396
149.552585	120.329182	50.574401
146.390130	109.869360	50.579405
142.383465	111.470324	50.584410
138.995884	109.024264	50.589415
135.249646	105.077458	50.594420
131.591264	112.548515	50.599425
128.327050	118.926596	50.604429
124.722085	124.525384	50.609434
121.611343	110.130644	50.614439
117.789287	115.620337	50.619444
114.586372	109.152226	50.624449
111.087490	114.520928	50.629453
107.263754	118.757437	50.634458
103.599582	118.962023	50.639463
100.079008	128.438110	50.644468
96.755657	122.362320	50.649473
93.257761	115.119389	50.654477
89.677215	116.820741	50.659482
86.387231	109.899977	50.664487
82.913039	110.231783	50.669492
79.292816	112.586773	50.674497
76.067611	109.658430	50.679501
72.211511	123.834960	50.684506
68.914033	107.040613	50.689511
65.414209	111.741921	50.694516
61.873836	110.210810	50.699521
58.176698	104.618856	50.704525
54.589004	118.108823	50.709530
51.293449	107.551736	50.714535
47.881262	105.335775	50.719540
44.007433	112.178149	50.724545
40.648886	112.022761	50.729549
37.488454	115.476583	50.734554
34.183759	113.839179	50.739559
30.634223	114.071416	50.744564
26.768329	111.724188	50.749569
23.599538	117.367058	50.754573
19.648945	116.060990	50.759578
16.371176	109.312708	50.764583
12.780026	111.794956	50.769588
8.966784	112.428648	50.774593
5.799412	115.465292	50.779597
2.257620	120.525450	50.784602