Tue Jun 21 12:58:01 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.734692	84.531136	0.000000
0.408572	90.110562	0.005005
0.524600	80.684657	0.010010
0.511007	72.999597	0.015014
0.344225	64.412831	0.020019
0.326954	49.197324	0.025024
-0.176498	49.862091	0.030029
-0.191713	19.065957	0.035034
-0.943031	14.613462	0.040038
-1.012192	8.980829	0.045043
-1.322520	-12.559965	0.050048
-1.854176	-17.418233	0.055053
-1.717642	-19.241850	0.060058
-2.562292	-20.346906	0.065062
-2.955932	-17.291083	0.070067
-2.947777	-17.654093	0.075072
-3.366129	-21.581750	0.080077
-4.233305	-30.735455	0.085082
-4.882873	-20.887471	0.090086
-4.382481	-16.921788	0.095091
-4.077077	-19.555992	0.100096
-5.044815	-15.370090	0.105101
-4.727248	-20.773711	0.110106
-4.862406	-24.212107	0.115110
-5.081478	-17.807044	0.120115
-5.442738	-16.501009	0.125120
-6.442322	-10.714787	0.130125
-6.600646	-18.362416	0.135130
-6.522509	-15.770107	0.140134
-6.731218	-17.073808	0.145139
-6.509403	-16.116320	0.150144
-7.299798	-9.578758	0.155149
-7.502118	-24.076829	0.160154
-8.184655	-16.034112	0.165158
-8.395505	-15.048589	0.170163
-8.028743	-24.046888	0.175168
-8.399682	-23.087544	0.180173
-8.243478	-26.276806	0.185178
-8.906838	-15.645490	0.190182
-9.446396	-17.122917	0.195187
-9.412767	-22.523722	0.200192
-9.990964	-18.190981	0.205197
-9.612235	-28.705594	0.210202
-9.534727	-19.729847	0.215206
-10.394124	-20.485746	0.220211
-10.806240	-36.071495	0.225216
-11.281286	-20.866006	0.230221
-11.517525	-26.790638	0.235226
-11.166073	-24.107035	0.240230
-11.186208	-16.125069	0.245235
-11.809904	-22.106311	0.250240
-12.225371	-19.825353	0.255245
-12.534620	-31.141667	0.260250
-13.228802	-28.117577	0.265254
-13.089714	-25.834125	0.270259
-12.907889	-23.745414	0.275264
-13.581133	-13.770961	0.280269
-13.620886	-17.931018	0.285274
-13.974802	-17.815724	0.290278
-14.322312	-21.972375	0.295283
-14.307553	-29.785411	0.300288
-14.945038	-19.330654	0.305293
-15.395995	-22.072265	0.310298
-15.813276	-25.018365	0.315302
-15.958385	-28.066760	0.320307
-15.762353	-24.496654	0.325312
-15.806390	-23.443442	0.330317
-15.631936	-31.923465	0.335322
-16.013603	-20.435605	0.340326
-16.725404	-27.448515	0.345331
-16.768730	-22.996949	0.350336
-17.645192	-23.089348	0.355341
-17.461294	-24.786818	0.360346
-17.450983	-25.541101	0.365350
-18.347001	-15.490884	0.370355
-18.444424	-16.642912	0.375360
-18.813009	-22.411442	0.380365
-18.832151	-24.560730	0.385370
-18.727274	-14.872404	0.390374
-19.005502	-21.718340	0.395379
-19.214317	-21.240301	0.400384
-19.759604	-22.936803	0.405389
-20.327353	-21.276697	0.410394
-20.416664	-24.810695	0.415398
-20.447672	-22.722852	0.420403
-20.674685	-25.986986	0.425408
-20.665753	-16.343158	0.430413
-21.135949	-26.023174	0.435418
-21.520797	-26.316762	0.440422
-22.140746	-25.134636	0.445427
-22.093835	-27.973292	0.450432
-22.020780	-21.845906	0.455437
-22.340966	-25.831848	0.460442
-22.037598	-20.317629	0.465446
-23.338957	-20.863783	0.470451
-23.511432	-25.581427	0.475456
-23.775030	-18.788137	0.480461
-23.795087	-30.417160	0.485466
-23.769708	-19.485893	0.490470
-24.043276	-33.059882	0.495475
-24.470282	-23.796354	0.500480
-25.011072	-19.818297	0.505485
-25.087745	-26.517046	0.510490
-25.084234	-23.678739	0.515494
-25.129206	-21.205363	0.520499
-25.444990	-24.181687	0.525504
-26.391477	-22.608047	0.530509
-26.453848	-25.090576	0.535514
-26.932236	-25.529697	0.540518
-27.052042	-30.150291	0.545523
-27.082505	-20.578086	0.550528
-27.429967	-19.014842	0.555533
-27.238827	-25.948367	0.560538
-27.503050	-14.685770	0.565542
-28.399458	-19.943417	0.570547
-28.713777	-23.213221	0.575552
-28.685733	-13.126583	0.580557
-28.512575	-34.042134	0.585562
-28.581313	-24.319343	0.590566
-28.992159	-20.349188	0.595571
-29.670492	-25.258343	0.600576
-30.390485	-21.047949	0.605581
-30.286282	-21.855076	0.610586
-30.311487	-28.557414	0.615590
-30.826017	-24.712368	0.620595
-30.405791	-28.184321	0.625600
-30.438219	-22.345334	0.630605
-30.887476	-23.444229	0.635610
-31.643061	-23.140268	0.640614
-32.092879	-17.953217	0.645619
-31.908416	-24.365270	0.650624
-32.015544	-20.067516	0.655629
-32.192368	-21.697754	0.660634
-32.870338	-20.745975	0.665638
-33.238059	-15.951398	0.670643
-33.462487	-20.869218	0.675648
-33.868959	-17.116655	0.680653
-33.567136	-23.993721	0.685658
-33.820270	-26.000856	0.690662
-34.387324	-20.210483	0.695667
-34.813702	-26.879540	0.700672
-35.167193	-21.268980	0.705677
-35.116402	-25.518225	0.710682
-35.400700	-26.640094	0.715686
-35.268937	-26.388357	0.720691
-35.396394	-32.189510	0.725696
-36.175933	-19.847813	0.730701
-36.666549	-31.437191	0.735706
-36.788258	-29.329791	0.740710
-36.996205	-28.214706	0.745715
-36.858592	-29.798938	0.750720
-37.109641	-27.928034	0.755725
-37.134927	-33.227909	0.760730
-37.725177	-28.064768	0.765734
-37.836167	-20.785659	0.770739
-38.293672	-22.139917	0.775744
-38.462728	-19.873320	0.780749
-38.208037	-16.383376	0.785754
-38.896000	-25.499262	0.790758
-39.721396	-21.942938	0.795763
-39.873430	-22.456230	0.800768
-39.965495	-26.594596	0.805773
-39.755863	-20.984345	0.810778
-39.594936	-19.869566	0.815782
-40.746729	-25.376970	0.820787
-40.804072	-22.368154	0.825792
-41.245219	-18.457113	0.830797
-41.254638	-20.635045	0.835802
-41.372440	-19.647959	0.840806
-41.793843	-26.477876	0.845811
-42.526064	-29.226777	0.850816
-42.736430	-20.281309	0.855821
-43.227345	-19.246446	0.860826
-42.773488	-28.345794	0.865830
-43.019902	-19.744031	0.870835
-42.889153	-20.842082	0.875840
-43.400709	-17.928741	0.880845
-43.395579	-23.936359	0.885850
-44.222710	-22.191462	0.890854
-44.601654	-16.332387	0.895859
-44.663479	-21.549255	0.900864
-44.959762	-11.518232	0.905869
-44.553612	-18.959979	0.910874
-45.015312	-22.558799	0.915878
-46.040772	-17.157231	0.920883
-45.967303	-17.744373	0.925888
-46.339734	-27.179896	0.930893
-46.594732	-22.180606	0.935898
-46.361487	-21.685590	0.940902
-46.470056	-25.415308	0.945907
-46.476364	-26.555191	0.950912
-47.593353	-21.777431	0.955917
-47.617532	-15.650519	0.960922
-47.678883	-11.995955	0.965926
-47.887849	-12.193952	0.970931
-47.823324	-31.823251	0.975936
-48.619103	-24.187036	0.980941
-48.799598	-20.549052	0.985946
-49.522787	-18.084722	0.990950
-49.534187	-15.342217	0.995955
-49.304298	-24.466243	1.000960
-49.377244	-23.693588	1.005965
-50.073387	-26.415903	1.010970
-50.554497	-22.310976	1.015974
-51.072771	-18.450506	1.020979
-50.790689	-14.633776	1.025984
-51.201405	-24.199514	1.030989
-50.875951	-23.470339	1.035994
-51.370929	-29.982202	1.040998
-52.096359	-25.382752	1.046003
-52.099492	-26.859810	1.051008
-52.517751	-19.239342	1.056013
-52.654906	-27.581922	1.061018
-52.560193	-24.574805	1.066022
-52.932803	-24.450689	1.071027
-53.552076	-29.868673	1.076032
-54.321602	-17.556258	1.081037
-54.169502	-24.814443	1.086042
-54.173695	-23.087030	1.091046
-54.437517	-17.800342	1.096051
-54.298444	-28.007683	1.101056
-54.356082	-22.308774	1.106061
-54.504434	-31.894670	1.111066
-55.184199	-17.862956	1.116070
-55.908634	-23.693319	1.121075
-55.656956	-27.501244	1.126080
-56.260619	-18.213785	1.131085
-55.902648	-19.798202	1.136090
-56.853950	-22.493060	1.141094
-57.348976	-10.375084	1.146099
-57.597271	-22.854705	1.151104
-57.734274	-17.680581	1.156109
-57.357690	-18.395275	1.161114
-57.364321	-27.031790	1.166118
-57.603565	-19.677964	1.171123
-58.503536	-26.963793	1.176128
-59.133691	-27.685617	1.181133
-59.183667	-31.675255	1.186138
-59.376155	-23.268312	1.191142
-59.264059	-23.599398	1.196147
-59.080847	-31.036385	1.201152
-59.222211	-22.767161	1.206157
-59.905187	-27.486298	1.211162
-60.432129	-24.507261	1.216166
-60.671423	-27.294968	1.221171
-60.679055	-23.232141	1.226176
-61.168676	-24.397361	1.231181
-61.289560	-20.955926	1.236186
-62.060909	-20.845105	1.241190
-62.284916	-24.424677	1.246195
-62.202220	-23.349040	1.251200
-62.391761	-22.916222	1.256205
-62.034976	-19.847918	1.261210
-62.513582	-36.098311	1.266214
-63.379285	-22.418636	1.271219
-63.410138	-22.151020	1.276224
-63.844142	-24.820840	1.281229
-63.645389	-25.139439	1.286234
-63.536337	-18.946780	1.291238
-64.195266	-16.300294	1.296243
-64.538693	-28.404022	1.301248
-65.185040	-28.201816	1.306253
-65.443718	-26.210063	1.311258
-65.323020	-25.842830	1.316262
-65.268064	-17.564478	1.321267
-65.544155	-25.612716	1.326272
-66.403962	-10.937671	1.331277
-66.618211	-23.542907	1.336282
-66.938538	-20.477910	1.341286
-66.862845	-27.324433	1.346291
-67.046569	-25.473753	1.351296
-67.200450	-11.330014	1.356301
-67.474506	-29.485204	1.361306
-68.458231	-18.420770	1.366310
-68.641477	-24.639910	1.371315
-68.716078	-29.015204	1.376320
-68.744725	-29.853610	1.381325
-68.707732	-24.710869	1.386330
-68.703439	-28.492034	1.391334
-69.002958	-23.719211	1.396339
-69.130998	-20.610479	1.401344
-70.453349	-21.707451	1.406349
-70.209488	-25.845996	1.411354
-70.322613	-27.122701	1.416358
-70.455105	-17.585895	1.421363
-70.556878	-32.227875	1.426368
-71.043364	-16.374620	1.431373
-71.637243	-24.065745	1.436378
-71.675888	-26.048804	1.441382
-71.970878	-15.670298	1.446387
-71.637497	-26.692836	1.451392
-71.969053	-24.808202	1.456397
-72.643088	-24.784929	1.461402
-73.078003	-24.760211	1.466406
-73.546540	-15.324632	1.471411
-73.093020	-30.105738	1.476416
-73.578800	-20.423403	1.481421
-73.902985	-34.175082	1.486426
-74.431267	-23.029393	1.491430
-75.028554	-20.427846	1.496435
-75.138838	-23.448459	1.501440
-75.337381	-13.827107	1.506445
-74.672136	-19.383225	1.511450
-74.641111	-19.577552	1.516454
-75.233478	-11.969094	1.521459
-76.136266	-15.482826	1.526464
-76.584732	-9.288804	1.531469
-76.539187	-19.983466	1.536474
-76.792396	-15.390384	1.541478
-77.040325	-18.795696	1.546483
-76.701368	-24.224368	1.551488
-77.222930	-16.859110	1.556493
-77.647129	-22.189814	1.561498
-78.187486	-23.721561	1.566502
-78.389356	-17.361972	1.571507
-78.305674	-19.707465	1.576512
-78.746790	-24.322994	1.581517
-78.279088	-19.719655	1.586522
-78.872236	-22.088430	1.591526
-79.506801	-16.972209	1.596531
-79.585396	-24.554097	1.601536
-80.123017	-13.927617	1.606541
-80.082379	-12.715761	1.611546
-80.162574	-20.428021	1.616550
-81.021906	-12.111719	1.621555
-81.113098	-23.288511	1.626560
-81.664658	-8.786662	1.631565
-81.818699	-16.425520	1.636570
-81.915922	-13.669592	1.641574
-82.233699	-13.465754	1.646579
-81.949413	-28.081886	1.651584
-81.884372	-8.577145	1.656589
-82.134750	-23.595503	1.661594
-82.547104	-15.866095	1.666598
-83.213329	-21.540727	1.671603
-83.457012	-24.977327	1.676608
-83.627009	-9.395715	1.681613
-83.673005	-15.250420	1.686618
-83.965362	-24.483710	1.691622
-85.084221	-18.095394	1.696627
-84.675439	-30.627780	1.701632
-85.107143	-18.490499	1.706637
-85.724056	-25.387683	1.711642
-84.900853	-16.041710	1.716646
-85.173269	-16.191705	1.721651
-85.497044	-30.210050	1.726656
-86.174395	-28.912836	1.731661
-86.279977	-25.309954	1.736666
-86.411042	-17.917804	1.741670
-87.074170	-22.830846	1.746675
-87.558744	-24.179431	1.751680
-88.079172	-13.369318	1.756685
-88.062877	-27.348870	1.761690
-88.119741	-24.403478	1.766694
-88.170293	-21.117351	1.771699
-88.172355	-26.450474	1.776704
-88.066955	-19.222398	1.781709
-88.506973	-13.960597	1.786714
-88.933243	-9.081925	1.791718
-90.050365	-14.860076	1.796723
-89.256020	-13.573144	1.801728
-89.220636	-10.153247	1.806733
-90.157027	-17.586367	1.811738
-90.930861	-13.191025	1.816742
-91.649087	-19.889886	1.821747
-91.688737	-18.745049	1.826752
-91.016777	-11.890419	1.831757
-90.839778	-19.228899	1.836762
-91.106486	-23.539028	1.841766
-91.607592	-10.364510	1.846771
-92.364876	-14.102431	1.851776
-92.602056	-21.620957	1.856781
-92.654261	-21.579106	1.861786
-92.952011	-10.797187	1.866790
-93.403637	-16.041652	1.871795
-93.341740	-14.141467	1.876800
-93.303373	-11.408981	1.881805
-94.143336	-16.687010	1.886810
-94.329494	-12.382087	1.891814
-94.896025	-15.383972	1.896819
-94.857932	-23.098454	1.901824
-95.244449	-21.567217	1.906829
-94.944161	-16.057627	1.911834
-94.558573	-17.442972	1.916838
-95.503898	-19.279425	1.921843
-95.833889	-17.460760	1.926848
-96.217849	-18.203422	1.931853
-96.398122	-16.742058	1.936858
-96.769209	-15.264486	1.941862
-97.555469	-14.675221	1.946867
-97.477364	-25.834857	1.951872
-97.757545	-17.702679	1.956877
-97.912381	-27.308021	1.961882
-98.055900	-30.420609	1.966886
-98.146456	-16.671178	1.971891
-98.154916	-28.281196	1.976896
-98.075177	-21.154248	1.981901
-99.213906	-15.504017	1.986906
-99.080928	-22.278725	1.991910
-99.443896	-22.872522	1.996915
-99.607172	-25.772084	2.006912
-99.749343	-24.964807	2.016909
-98.732516	-20.093282	2.026906
-98.268849	-23.094431	2.036902
-98.032153	-19.002600	2.046899
-97.437551	-21.759286	2.056896
-97.141038	-23.536569	2.066893
-96.462714	-21.361351	2.076890
-95.613406	-22.365944	2.086886
-95.414102	-17.586446	2.096883
-95.294649	-22.961882	2.106880
-94.141196	-21.310315	2.116877
-93.711486	-28.179310	2.126874
-93.645332	-24.764023	2.136870
-93.057010	-28.220110	2.146867
-92.312663	-22.099963	2.156864
-92.064010	-23.956256	2.166861
-90.740704	-19.574323	2.176858
-90.816112	-24.295290	2.186854
-90.590317	-26.061453	2.196851
-90.168584	-23.387713	2.206848
-89.517447	-28.598883	2.216845
-89.148476	-29.145153	2.226842
-88.245676	-26.377010	2.236838
-87.737897	-18.443560	2.246835
-87.727084	-20.739018	2.256832
-87.010796	-27.088007	2.266829
-86.682779	-24.751240	2.276826
-85.322620	-25.602934	2.286822
-85.132554	-22.802901	2.296819
-85.314961	-22.466130	2.306816
-84.451149	-22.330879	2.316813
-83.734179	-23.934170	2.326810
-83.471663	-20.865760	2.336806
-83.000061	-16.635793	2.346803
-82.141215	-23.991579	2.356800
-81.768643	-19.413267	2.366797
-81.687318	-24.583222	2.376794
-80.778522	-19.963505	2.386790
-80.367769	-28.447588	2.396787
-80.053419	-26.815518	2.406784
-79.255930	-24.995534	2.416781
-78.542093	-25.337707	2.426778
-78.710475	-21.949374	2.436774
-77.732948	-25.158125	2.446771
-77.363488	-14.569724	2.456768
-76.974362	-28.339993	2.466765
-75.834289	-27.659315	2.476762
-75.609031	-19.622962	2.486758
-75.405781	-26.546331	2.496755
-75.306049	-32.729785	2.506752
-74.559341	-25.910771	2.516749
-74.088276	-22.427391	2.526746
-73.140287	-20.506664	2.536742
-72.608883	-18.229657	2.546739
-72.667620	-25.829445	2.556736
-71.799391	-26.530316	2.566733
-71.186582	-29.544701	2.576730
-70.936006	-24.669763	2.586726
-70.521132	-20.488293	2.596723
-69.480204	-20.195651	2.606720
-69.111175	-17.245846	2.616717
-69.185888	-23.674664	2.626714
-68.106122	-20.474854	2.636710
-67.812571	-21.204835	2.646707
-67.684266	-23.008596	2.656704
-66.313404	-14.572559	2.666701
-66.068851	-17.837553	2.676698
-65.840800	-16.572727	2.686694
-65.774189	-20.231482	2.696691
-65.330908	-26.440614	2.706688
-64.237154	-22.642657	2.716685
-63.230520	-17.999225	2.726682
-63.139418	-24.213263	2.736678
-62.786723	-21.766967	2.746675
-62.877382	-22.594748	2.756672
-62.089461	-21.189489	2.766669
-61.241088	-16.357234	2.776666
-60.445424	-22.834362	2.786662
-60.226590	-15.911325	2.796659
-59.610794	-21.787841	2.806656
-59.807982	-25.970967	2.816653
-58.711112	-27.159206	2.826650
-58.489958	-24.067744	2.836646
-57.804328	-19.929924	2.846643
-57.048788	-17.096682	2.856640
-56.771064	-28.051083	2.866637
-56.540616	-26.558838	2.876634
-55.478964	-28.103616	2.886630
-55.121151	-16.111413	2.896627
-55.175374	-21.922416	2.906624
-54.575819	-19.159764	2.916621
-54.014447	-22.849278	2.926618
-53.052764	-17.831087	2.936614
-52.248203	-18.854540	2.946611
-52.127342	-22.159313	2.956608
-52.227398	-17.077128	2.966605
-51.384778	-16.570851	2.976602
-50.496524	-20.571161	2.986598
-50.343010	-12.560658	2.996595
-50.055351	-19.034276	3.006592
-49.168148	-16.313527	3.016589
-49.050477	-18.941041	3.026586
-47.808793	-18.677096	3.036582
-47.640603	-13.381877	3.046579
-47.502290	-17.849569	3.056576
-46.973922	-20.127398	3.066573
-46.125557	-23.167156	3.076570
-45.923188	-23.581903	3.086566
-45.336760	-19.438322	3.096563
-44.483620	-17.222494	3.106560
-44.335816	-21.027868	3.116557
-44.212378	-23.750189	3.126554
-43.084609	-22.009194	3.136550
-42.771725	-18.691470	3.146547
-42.382579	-17.975341	3.156544
-40.837532	-19.419179	3.166541
-41.626979	-21.834827	3.176538
-41.251042	-18.060648	3.186534
-40.426484	-21.140921	3.196531
-39.919408	-19.922102	3.206528
-38.822535	-18.041038	3.216525
-38.404974	-15.890399	3.226522
-38.170622	-19.315526	3.236518
-38.256927	-17.162260	3.246515
-37.280668	-20.016917	3.256512
-36.672721	-22.834292	3.266509
-36.237170	-22.655576	3.276506
-35.864958	-20.257953	3.286502
-34.967240	-24.717634	3.296499
-34.627150	-19.721377	3.306496
-34.574844	-18.647162	3.316493
-33.484723	-24.082177	3.326490
-33.320338	-24.517899	3.336486
-33.163858	-30.576791	3.346483
-32.136712	-21.853242	3.356480
-31.831821	-21.433568	3.366477
-30.948496	-20.370908	3.376474
-30.417254	-23.406755	3.386470
-30.175157	-19.033461	3.396467
-29.938021	-23.461204	3.406464
-29.257851	-23.034322	3.416461
-28.576176	-27.765075	3.426458
-28.263669	-17.754263	3.436454
-27.993027	-20.788054	3.446451
-27.139696	-22.568429	3.456448
-26.935796	-19.509473	3.466445
-25.892122	-25.853198	3.476442
-25.408433	-22.412011	3.486438
-25.191702	-20.552748	3.496435
-25.177702	-24.791201	3.506432
-24.122421	-21.505523	3.516429
-23.615582	-19.214167	3.526426
-23.439963	-16.497686	3.536422
-22.191664	-20.852806	3.546419
-21.982183	-17.601733	3.556416
-21.710215	-22.309691	3.566413
-21.568657	-18.221263	3.576410
-20.594740	-18.340939	3.586406
-20.257246	-15.127462	3.596403
-20.079284	-14.037304	3.606400
-19.006354	-17.923953	3.616397
-18.719033	-16.125972	3.626394
-18.235255	-16.629008	3.636390
-17.283658	-17.141543	3.646387
-17.270084	-22.975235	3.656384
-17.098591	-14.317451	3.666381
-15.901015	-18.870056	3.676378
-15.481435	-12.972926	3.686374
-15.407648	-16.277018	3.696371
-15.021206	-15.369176	3.706368
-14.472853	-15.455527	3.716365
-13.641519	-12.604200	3.726362
-12.544311	-13.533054	3.736358
-12.408968	-16.018862	3.746355
-12.541070	-16.177870	3.756352
-12.322390	-18.206432	3.766349
-11.469308	-13.088839	3.776346
-9.907834	-15.314665	3.786342
-10.335516	-16.612218	3.796339
-9.649647	-17.020880	3.806336
-9.347598	-14.793414	3.816333
-8.973288	-17.084851	3.826330
-8.144936	-15.755035	3.836326
-7.622292	-13.016587	3.846323
-6.482910	-11.221982	3.856320
-7.069587	-18.686936	3.866317
-6.507290	-10.099395	3.876314
-5.594219	-17.104349	3.886310
-5.094196	-6.961766	3.896307
-5.029432	-13.549235	3.906304
-4.231000	-10.700954	3.916301
-3.783847	-3.652505	3.926298
-3.187325	6.221000	3.936294
-2.850123	16.008824	3.946291
-2.634896	24.352143	3.956288
-2.126940	32.730177	3.966285
-1.828162	49.215460	3.976282
-1.205882	71.918408	3.986278
-0.815644	96.725788	3.996275
-0.414833	110.954786	4.006272
0.000000	128.178419	4.011277
-0.093903	139.896792	4.016282
0.070978	163.205648	4.021286
0.272850	173.936146	4.026291
0.423158	177.455066	4.031296
0.684446	190.214414	4.036301
0.974843	202.340633	4.041306
1.138231	212.251087	4.046310
1.269689	206.934052	4.051315
0.944221	211.844049	4.056320
1.311483	210.428377	4.061325
1.322747	212.388087	4.066330
1.276130	213.508639	4.071334
1.508368	214.670435	4.076339
1.078006	205.589495	4.081344
1.326992	198.634845	4.086349
1.084794	202.352165	4.091354
1.142425	204.696895	4.096358
1.379115	209.661017	4.101363
0.988999	211.518074	4.106368
1.611741	211.041845	4.111373
0.936160	215.522003	4.116378
1.116633	210.093052	4.121382
1.198188	215.182716	4.126387
1.090768	217.975500	4.131392
1.528125	213.595872	4.136397
1.368269	213.052094	4.141402
1.459000	216.064854	4.146406
1.425885	220.060926	4.151411
0.927679	221.082009	4.156416
1.061967	219.149412	4.161421
1.002753	216.662374	4.166426
0.856895	213.767581	4.171430
1.340134	216.580960	4.176435
1.076734	215.345101	4.181440
1.188205	214.101237	4.186445
1.316759	232.682314	4.191450
1.599125	235.882585	4.196454
2.024016	234.732653	4.201459
1.497564	227.087250	4.206464
1.840874	220.413766	4.211469
1.377644	220.538478	4.216474
1.336257	222.364628	4.221478
1.551589	219.416735	4.226483
1.193282	227.095870	4.231488
1.642725	230.615195	4.236493
1.474476	238.951174	4.241498
1.767168	239.611199	4.246502
1.744419	238.128680	4.251507
1.930931	239.853750	4.256512
1.423835	223.018931	4.261517
1.375116	225.726219	4.266522
1.602648	230.822500	4.271526
1.712524	239.667730	4.276531
1.440233	245.828729	4.281536
1.565591	243.043141	4.286541
1.592374	256.648679	4.291546
1.547983	247.364679	4.296550
1.989379	244.857296	4.301555
1.562277	250.333125	4.306560
2.138686	244.629225	4.311565
2.017627	251.464742	4.316570
2.049347	241.607311	4.321574
1.744892	230.657450	4.326579
1.464113	232.099561	4.331584
1.883214	235.246011	4.336589
1.593162	241.468953	4.341594
1.909864	248.260397	4.346598
1.917144	253.699819	4.351603
1.722383	255.220437	4.356608
1.776512	243.691995	4.361613
1.764611	261.572928	4.366618
1.978937	252.158664	4.371622
1.938611	243.108232	4.376627
1.825180	257.882923	4.381632
2.168554	251.432208	4.386637
1.950120	251.422846	4.391642
1.638205	247.941038	4.396646
1.960026	243.142446	4.401651
1.677104	253.903943	4.406656
1.934464	240.974898	4.411661
1.645892	246.873373	4.416666
1.554170	245.377016	4.421670
2.076925	249.049376	4.426675
1.772082	258.823875	4.431680
2.131925	257.466261	4.436685
1.986333	258.002314	4.441690
1.938274	262.266290	4.446694
2.367396	269.089646	4.451699
2.013167	287.846835	4.456704
2.399907	281.854445	4.461709
2.083348	269.105661	4.466714
2.031948	263.729098	4.471718
2.085388	266.989583	4.476723
2.211419	282.042555	4.481728
2.424840	271.444209	4.486733
2.312505	276.247497	4.491738
2.137154	257.307375	4.496742
2.209099	249.790008	4.501747
1.923900	258.568059	4.506752
2.618280	268.137044	4.511757
2.062074	276.166883	4.516762
2.123165	271.990641	4.521766
2.251519	278.409338	4.526771
2.245555	281.859634	4.531776
2.200593	275.677852	4.536781
2.313146	291.655615	4.541786
2.286429	276.688516	4.546790
2.424144	278.833118	4.551795
2.348344	290.289504	4.556800
2.583506	281.269011	4.561805
2.401876	290.701864	4.566810
2.482953	283.731565	4.571814
2.478435	281.474632	4.576819
2.097869	291.233077	4.581824
2.353703	288.608017	4.586829
2.330546	282.949117	4.591834
2.656253	284.730275	4.596838
2.625726	287.361546	4.601843
2.104049	280.789236	4.606848
2.321127	283.507972	4.611853
2.331376	293.077973	4.616858
2.371356	285.090102	4.621862
2.258630	285.371674	4.626867
2.593184	291.646315	4.631872
2.456659	280.043250	4.636877
2.211793	286.201302	4.641882
2.220825	284.510653	4.646886
2.430684	302.960540	4.651891
2.430165	304.874458	4.656896
2.775533	312.663855	4.661901
2.535270	317.600428	4.666906
2.540520	312.691234	4.671910
2.851901	313.484528	4.676915
2.567367	322.210605	4.681920
2.765047	316.284634	4.686925
2.473515	320.592494	4.691930
2.795451	313.704253	4.696934
2.836219	316.347207	4.701939
2.563418	322.320653	4.706944
2.724723	320.047702	4.711949
2.731148	313.036470	4.716954
2.627266	317.817849	4.721958
2.964576	313.206707	4.726963
2.695351	314.719730	4.731968
2.918627	311.882788	4.736973
2.589512	311.765853	4.741978
2.623974	313.415270	4.746982
2.675945	316.664760	4.751987
2.785985	313.755991	4.756992
2.948090	311.550201	4.761997
2.886041	317.513019	4.767002
2.748955	314.110781	4.772006
2.910008	311.580742	4.777011
2.241802	316.384525	4.782016
2.675890	323.035596	4.787021
2.981764	339.525062	4.792026
3.090220	345.089451	4.797030
3.277103	346.894196	4.802035
2.856237	345.473842	4.807040
3.115555	340.768451	4.812045
2.994129	353.592294	4.817050
2.598985	353.791969	4.822054
3.214309	347.623763	4.827059
3.015239	351.196037	4.832064
3.100356	347.055461	4.837069
3.014671	353.989952	4.842074
2.915295	349.705873	4.847078
3.135939	350.857760	4.852083
2.935914	353.640643	4.857088
2.925265	348.527064	4.862093
2.826932	350.654522	4.867098
3.052369	347.740057	4.872102
3.355156	351.647388	4.877107
2.719623	357.766360	4.882112
3.104651	353.410553	4.887117
3.410219	358.218866	4.892122
3.244878	347.763306	4.897126
3.096164	350.151699	4.902131
2.888446	344.453875	4.907136
2.891795	348.496039	4.912141
3.231776	360.934452	4.917146
3.198779	366.348220	4.922150
3.494554	366.817112	4.927155
3.251721	382.358695	4.932160
3.250742	373.781401	4.937165
3.470797	377.425376	4.942170
3.415805	369.817868	4.947174
3.547844	364.263877	4.952179
2.958400	365.434859	4.957184
3.300643	366.134835	4.962189
3.153920	379.889983	4.967194
3.199510	378.103679	4.972198
3.379722	373.075114	4.977203
3.651324	380.443997	4.982208
3.636910	378.798267	4.987213
3.542302	379.435207	4.992218
3.231185	379.853433	4.997222
3.509101	385.006939	5.002227
3.222067	383.455883	5.007232
3.462340	382.676920	5.012237
3.361993	380.822624	5.017242
3.310611	376.056387	5.022246
3.559262	374.089639	5.027251
3.338483	378.269961	5.032256
3.326068	378.710951	5.037261
3.073940	382.765235	5.042266
3.592648	382.028574	5.047270
3.452584	379.940497	5.052275
3.445596	395.490401	5.057280
3.924117	398.432076	5.062285
3.622241	391.240975	5.067290
3.482582	401.644165	5.072294
3.628058	403.217783	5.077299
3.755295	410.373385	5.082304
3.730693	407.543530	5.087309
3.846564	417.216494	5.092314
3.826035	410.131733	5.097318
3.906126	393.789341	5.102323
3.417455	393.459060	5.107328
4.161039	400.403863	5.112333
3.624817	403.716039	5.117338
3.502405	392.783082	5.122342
3.935724	394.851124	5.127347
3.996208	402.782858	5.132352
4.103765	400.760929	5.137357
3.701498	393.849700	5.142362
3.624014	387.080651	5.147366
3.725939	396.148306	5.152371
3.648946	406.215119	5.157376
4.139404	415.682787	5.162381
4.063205	411.120749	5.167386
3.802905	408.377482	5.172390
3.955537	407.420427	5.177395
3.701808	424.127761	5.182400
4.148844	414.364056	5.187405
4.234572	430.073485	5.192410
3.908976	407.999054	5.197414
4.149736	386.984513	5.202419
3.761765	403.802067	5.207424
4.102741	408.022778	5.212429
4.025827	406.781085	5.217434
3.750022	414.745817	5.222438
3.991954	410.175699	5.227443
3.916678	404.534462	5.232448
4.114707	418.857727	5.237453
3.948543	422.114549	5.242458
3.878881	418.195738	5.247462
4.575151	424.914739	5.252467
3.838216	432.839013	5.257472
4.432346	432.580643	5.262477
4.198244	421.786537	5.267482
4.524035	425.042609	5.272486
4.348876	418.913310	5.277491
4.009301	415.780597	5.282496
4.278840	417.967131	5.287501
4.098795	425.632830	5.292506
3.891331	424.022220	5.297510
3.954385	430.937049	5.302515
3.898410	424.179814	5.307520
4.464482	417.528560	5.312525
4.518217	429.932928	5.317530
4.303897	429.759093	5.322534
4.602005	427.334216	5.327539
4.231660	427.992742	5.332544
4.413808	427.063952	5.337549
4.299401	427.972554	5.342554
4.041332	424.405616	5.347558
4.065225	423.212548	5.352563
4.033364	428.503799	5.357568
3.738241	419.070190	5.362573
4.025325	424.077739	5.367578
4.010224	422.194917	5.372582
4.337368	432.030837	5.377587
4.130553	446.057469	5.382592
4.553985	450.323739	5.387597
4.658034	444.028412	5.392602
4.165372	454.215000	5.397606
4.322848	448.157498	5.402611
4.046003	455.138687	5.407616
4.680626	456.496333	5.412621
4.570215	451.350298	5.417626
4.874123	454.521790	5.422630
4.776290	449.815516	5.427635
4.479238	462.162552	5.432640
4.490194	446.368710	5.437645
4.558559	450.990575	5.442650
4.579818	453.148565	5.447654
4.535736	450.745023	5.452659
4.382682	454.593673	5.457664
4.481543	450.406392	5.462669
4.674960	457.655449	5.467674
4.399138	454.775422	5.472678
4.760352	448.151763	5.477683
4.616472	458.556281	5.482688
4.623105	450.592791	5.487693
4.625012	460.655257	5.492698
4.623788	455.326758	5.497702
4.912166	448.466906	5.502707
4.815323	460.480240	5.507712
4.514958	448.439444	5.512717
4.674001	454.071669	5.517722
4.588350	458.397375	5.522726
4.738143	447.679596	5.527731
4.638865	452.514719	5.532736
4.805231	466.548446	5.537741
4.875503	475.951538	5.542746
4.604654	481.838879	5.547750
5.118050	485.002921	5.552755
4.772042	485.862258	5.557760
5.068427	485.729363	5.562765
4.969917	477.254005	5.567770
4.728260	477.587123	5.572774
5.310220	481.707762	5.577779
5.073394	475.357567	5.582784
4.816888	467.502961	5.587789
4.608145	458.240129	5.592794
4.496863	480.623888	5.597798
4.933469	476.756605	5.602803
4.701832	483.642109	5.607808
4.914665	484.806745	5.612813
5.007028	492.063080	5.617818
4.888544	491.158216	5.622822
5.261508	483.672786	5.627827
5.243891	494.232646	5.632832
5.194612	487.556959	5.637837
4.938155	489.536961	5.642842
4.869137	492.314160	5.647846
5.184968	488.288873	5.652851
4.886127	494.395362	5.657856
5.062763	491.910075	5.662861
5.120881	490.001898	5.667866
5.159548	487.839612	5.672870
5.323330	490.127340	5.677875
5.149824	491.081450	5.682880
5.410515	483.343072	5.687885
5.227270	492.979771	5.692890
5.209530	497.330949	5.697894
5.503010	484.022354	5.702899
5.069456	486.154031	5.707904
5.042768	484.247663	5.712909
5.036452	489.509051	5.717914
4.893524	488.883129	5.722918
4.969457	486.192905	5.727923
5.132723	497.253066	5.732928
5.272914	507.157091	5.737933
5.282758	515.422879	5.742938
5.417836	519.330791	5.747942
5.245199	520.565969	5.752947
5.305579	513.951247	5.757952
5.537671	518.859988	5.762957
5.540890	511.912742	5.767962
5.448582	531.757810	5.772966
5.750122	509.432764	5.777971
5.591843	499.460401	5.782976
5.425985	488.826634	5.787981
5.122000	492.178518	5.792986
5.242949	499.272448	5.797990
5.553864	513.245774	5.802995
5.564283	515.207636	5.808000
5.620014	517.555689	5.813005
5.551395	512.695369	5.818010
5.419288	517.086803	5.823014
5.476876	511.826889	5.828019
5.495933	518.600249	5.833024
5.808384	515.223580	5.838029
5.663485	518.540839	5.843034
5.183994	516.758584	5.848038
5.530121	516.375711	5.853043
5.260599	520.250767	5.858048
5.498232	516.762359	5.863053
5.668726	519.110156	5.868058
5.619339	518.672004	5.873062
5.808338	515.035751	5.878067
5.406818	523.928725	5.883072
5.501540	515.464764	5.888077
5.444546	508.333504	5.893082
5.469220	518.422036	5.898086
5.985433	510.291449	5.903091
5.773872	520.637160	5.908096
5.803848	522.054284	5.913101
5.654600	522.690805	5.918106
5.513674	514.554968	5.923110
5.823579	517.273373	5.928115
5.619037	524.018244	5.933120
5.892079	528.890409	5.938125
5.749108	535.678963	5.943130
5.767283	548.903343	5.948134
6.016655	552.242153	5.953139
5.773575	549.293932	5.958144
5.797010	556.146308	5.963149
5.838292	547.783928	5.968154
5.869155	553.929582	5.973158
6.076367	554.342891	5.978163
6.267525	554.469953	5.983168
6.378857	541.296851	5.988173
6.355598	527.160332	5.993178
5.687041	520.649932	5.998182
5.812682	514.243253	6.003187
5.914846	524.549451	6.008192
5.978902	513.645128	6.013197
6.158217	516.373317	6.018202
5.862377	523.043910	6.023206
5.960566	520.834465	6.028211
5.887145	525.805836	6.033216
5.767581	521.741534	6.038221
5.797864	535.798253	6.043226
5.785518	551.795980	6.048230
6.376731	542.541140	6.053235
6.051614	546.903762	6.058240
6.139663	542.797577	6.063245
6.480026	539.644209	6.068250
6.188255	527.363541	6.073254
6.079160	524.377154	6.078259
5.902264	519.917601	6.083264
6.072944	517.827976	6.088269
6.009444	517.997995	6.093274
5.655426	525.876078	6.098278
6.047315	513.692776	6.103283
5.668093	522.680925	6.108288
5.736912	532.687956	6.113293
6.362695	547.447673	6.118298
5.605702	551.870956	6.123302
6.378901	547.201973	6.128307
6.210729	552.537348	6.133312
6.033898	538.390727	6.138317
5.950744	523.590212	6.143322
5.899521	518.581571	6.148326
6.060802	527.537055	6.153331
6.074479	537.667283	6.158336
6.260916	534.078220	6.163341
6.102703	529.440728	6.168346
5.784552	522.928347	6.173350
5.906516	516.980106	6.178355
5.708231	528.946353	6.183360
5.859097	538.979073	6.188365
6.165298	546.351187	6.193370
6.000517	551.983392	6.198374
6.273490	542.578975	6.203379
5.754458	542.530586	6.208384
5.917995	545.190152	6.213389
6.020516	550.481295	6.218394
6.031063	551.929463	6.223398
6.224554	537.652847	6.228403
6.216056	544.622399	6.233408
6.128893	528.224086	6.238413
6.092643	519.069214	6.243418
5.672363	515.790195	6.248422
5.964456	520.885355	6.253427
6.112843	541.066315	6.258432
6.179433	528.240651	6.263437
6.023908	520.487700	6.268442
5.446327	526.684956	6.273446
5.795066	535.770039	6.278451
6.104756	549.362931	6.283456
6.081602	547.215017	6.288461
6.005481	554.360747	6.293466
6.006822	548.980087	6.298470
6.230216	550.446687	6.303475
5.965888	550.924659	6.308480
6.147748	552.033648	6.313485
6.118546	546.583649	6.318490
5.810631	529.357143	6.323494
6.127528	542.898711	6.328499
6.001026	546.469472	6.333504
6.021169	540.410206	6.338509
5.926908	542.756261	6.343514
5.655726	546.267702	6.348518
6.068362	543.563945	6.353523
6.009361	550.979563	6.358528
6.051183	550.750288	6.363533
6.062807	557.277628	6.368538
5.941355	565.982560	6.373542
5.995304	550.254509	6.378547
5.976762	551.986731	6.383552
5.797619	554.767573	6.388557
6.252974	557.658650	6.393562
5.971545	558.156820	6.398566
6.141541	552.948729	6.403571
5.997858	558.257949	6.408576
6.076414	553.513161	6.413581
6.311385	556.616560	6.418586
5.811838	539.511169	6.423590
5.976594	533.612078	6.428595
6.122012	551.579976	6.433600
5.955651	539.788657	6.438605
6.116187	546.677332	6.443610
6.008424	541.672322	6.448614
6.051967	528.926450	6.453619
5.884594	537.845782	6.458624
5.969580	543.815322	6.463629
6.206900	545.278036	6.468634
5.716288	545.639948	6.473638
5.912619	553.269435	6.478643
5.689544	554.213404	6.483648
5.909086	548.410417	6.488653
6.013919	560.425758	6.493658
6.047001	560.973282	6.498662
6.193048	554.014009	6.503667
5.725947	558.707404	6.508672
5.861390	551.833363	6.513677
6.206834	544.816408	6.518682
6.182813	559.963172	6.523686
6.219261	554.130904	6.528691
5.877344	559.017290	6.533696
6.103023	553.824647	6.538701
6.141468	562.867193	6.543706
6.067160	558.315850	6.548710
6.288396	549.306981	6.553715
6.198453	552.463589	6.558720
5.923359	535.052259	6.563725
5.696616	529.086765	6.568730
5.727184	545.908381	6.573734
6.404674	550.088011	6.578739
6.244018	550.109537	6.583744
5.900328	536.584148	6.588749
6.087298	528.671665	6.593754
5.665422	537.720957	6.598758
6.021463	547.889026	6.603763
6.214605	554.917351	6.608768
6.131045	541.050900	6.613773
6.187581	523.001133	6.618778
6.193126	522.758724	6.623782
6.379567	507.657435	6.628787
6.031390	517.871841	6.633792
5.835111	509.539544	6.638797
6.018750	509.550236	6.643802
5.732769	526.215461	6.648806
6.244946	520.044139	6.653811
5.893693	524.372008	6.658816
6.004684	519.706913	6.663821
5.977731	524.593034	6.668826
5.795511	520.529636	6.673830
6.083507	515.529749	6.678835
5.712736	522.262677	6.683840
5.797405	523.277642	6.688845
5.953208	533.499974	6.693850
5.588766	545.984928	6.698854
6.375321	544.413953	6.703859
6.421572	550.577976	6.708864
6.330918	535.952351	6.713869
6.182887	523.237810	6.718874
6.093461	524.652011	6.723878
6.116306	510.661798	6.728883
5.899737	524.121184	6.733888
5.968260	520.833057	6.738893
5.909959	525.590572	6.743898
5.914362	527.716435	6.748902
6.356261	526.064198	6.753907
6.133058	520.168375	6.758912
5.734777	514.563218	6.763917
5.834585	521.087386	6.768922
5.639624	530.256182	6.773926
5.733844	523.831416	6.778931
6.112723	538.710748	6.783936
6.255979	537.580789	6.788941
6.179494	526.418717	6.793946
5.619834	521.123858	6.798950
5.923952	523.979782	6.803955
6.164727	539.066891	6.808960
6.056793	534.642093	6.813965
6.065475	523.572878	6.818970
5.884348	523.605884	6.823974
6.095039	531.854012	6.828979
5.975554	541.094383	6.833984
5.962868	533.633123	6.838989
6.165599	535.722397	6.843994
5.578547	534.213703	6.848998
5.829294	548.254252	6.854003
6.170229	550.625732	6.859008
5.757601	551.096884	6.864013
6.147680	547.728469	6.869018
6.151095	553.270463	6.874022
6.509904	540.067040	6.879027
6.427632	532.559285	6.884032
6.083159	527.573545	6.889037
6.266028	520.760536	6.894042
5.982013	521.341029	6.899046
6.291659	520.297187	6.904051
6.153159	523.187922	6.909056
5.963178	521.933763	6.914061
6.203993	517.142186	6.919066
5.825453	519.662990	6.924070
5.962915	521.556060	6.929075
5.883709	525.065900	6.934080
6.117089	519.713134	6.939085
6.099916	517.133243	6.944090
5.862210	530.014770	6.949094
5.944641	513.963335	6.954099
5.781829	521.726871	6.959104
5.651248	514.857429	6.964109
6.106349	519.091242	6.969114
5.757072	522.662576	6.974118
5.865334	514.780697	6.979123
5.681822	523.222960	6.984128
6.044418	532.089067	6.989133
6.200456	544.194586	6.994138
6.101029	537.427131	6.999142
6.150243	525.357397	7.004147
5.839084	517.521682	7.009152
6.204140	516.268957	7.014157
6.289627	519.560302	7.019162
5.776514	516.936630	7.024166
6.152113	517.288508	7.029171
6.181513	514.144011	7.034176
6.112589	512.942033	7.039181
6.036441	512.776892	7.044186
5.879513	514.502424	7.049190
6.131512	510.025728	7.054195
6.053641	517.903863	7.059200
6.519551	518.866749	7.064205
6.390084	520.217327	7.069210
5.709104	520.382833	7.074214
6.105203	511.090067	7.079219
5.969355	512.840130	7.084224
6.273206	519.937923	7.089229
6.482120	521.289106	7.094234
6.535225	525.060220	7.099238
6.530007	506.922422	7.104243
6.047467	492.816401	7.109248
6.006590	493.548447	7.114253
6.034222	485.731045	7.119258
5.734239	498.040706	7.124262
5.784390	493.499952	7.129267
5.811157	487.633397	7.134272
5.548062	493.915914	7.139277
6.178616	504.002385	7.144282
5.782596	515.748177	7.149286
5.988704	510.163122	7.154291
5.733491	521.761870	7.159296
5.902940	516.104145	7.164301
6.395899	515.398777	7.169306
6.039128	517.539254	7.174310
5.934014	518.110844	7.179315
5.956766	518.965165	7.184320
6.048558	521.972876	7.189325
6.382357	513.421768	7.194330
6.090627	528.568626	7.199334
6.268724	511.086423	7.204339
6.206634	505.603009	7.209344
6.009013	495.147761	7.214349
6.028966	487.777223	7.219354
5.716355	493.010395	7.224358
5.949647	494.502385	7.229363
6.211659	514.808948	7.234368
5.907170	504.538537	7.239373
6.067534	504.335219	7.244378
6.091937	514.194879	7.249382
6.024437	491.977144	7.254387
5.918538	494.697500	7.259392
5.879001	499.791522	7.264397
5.926558	507.492194	7.269402
6.084362	521.396750	7.274406
6.342067	517.544873	7.279411
6.036194	497.224362	7.284416
5.934536	496.715141	7.289421
6.002846	494.707790	7.294426
5.909115	500.405963	7.299430
6.052745	494.232925	7.304435
6.024345	487.568188	7.309440
6.466207	484.052482	7.314445
6.409589	486.260275	7.319450
5.905517	493.590903	7.324454
6.138277	489.496489	7.329459
6.164881	493.785659	7.334464
5.844083	494.161089	7.339469
6.121065	496.580644	7.344474
5.742962	498.759975	7.349478
5.724841	490.264588	7.354483
5.722205	492.827930	7.359488
5.782098	492.385496	7.364493
5.864190	496.985367	7.369498
5.976955	510.408363	7.374502
5.860853	515.801606	7.379507
6.037593	524.028317	7.384512
5.674881	534.531285	7.389517
6.473882	517.618007	7.394522
6.017753	525.505104	7.399526
5.989644	522.233964	7.404531
5.860052	523.454516	7.409536
6.266215	523.206747	7.414541
6.040438	513.538997	7.419546
5.737433	507.094171	7.424550
6.189994	519.969927	7.429555
5.930693	520.503110	7.434560
5.614637	520.408283	7.439565
6.305541	521.843051	7.444570
6.031476	520.772330	7.449574
6.391176	515.488833	7.454579
5.996649	499.399566	7.459584
5.990603	493.385701	7.464589
5.963940	491.120762	7.469594
5.805599	492.430138	7.474598
6.276238	497.413829	7.479603
5.975702	494.897637	7.484608
5.688869	493.995192	7.489613
5.923074	505.291472	7.494618
5.790207	518.507091	7.499622
5.963465	508.036402	7.504627
6.008863	514.213970	7.509632
6.013075	520.465259	7.514637
5.737131	512.654105	7.519642
5.878171	514.560198	7.524646
6.122562	514.258504	7.529651
5.962845	520.848735	7.534656
5.727364	525.565929	7.539661
5.736017	519.016209	7.544666
5.985809	525.553433	7.549670
6.085216	518.942113	7.554675
6.063172	515.431781	7.559680
5.778676	524.412928	7.564685
5.992908	514.189623	7.569690
6.081547	519.418326	7.574694
6.063952	514.280780	7.579699
6.000471	512.823332	7.584704
5.827952	516.435649	7.589709
6.284403	518.624400	7.594714
5.972762	528.778890	7.599718
6.001060	526.024715	7.604723
6.093574	531.774943	7.609728
5.930395	526.350294	7.614733
6.201071	522.982120	7.619738
6.133571	520.261175	7.624742
6.099042	517.767435	7.629747
6.255346	520.200465	7.634752
5.899003	527.125977	7.639757
6.281440	516.159460	7.644762
6.035513	519.122449	7.649766
5.952347	514.248159	7.654771
6.144507	520.846824	7.659776
6.259659	527.775961	7.664781
6.196507	517.509783	7.669786
5.952520	518.811636	7.674790
6.040933	518.949001	7.679795
5.846294	516.761602	7.684800
5.733703	519.392688	7.689805
5.922278	505.851219	7.694810
6.011041	525.274971	7.699814
6.051103	524.514156	7.704819
5.702683	517.518176	7.709824
5.765982	522.145241	7.714829
6.089121	532.621074	7.719834
6.071983	523.914154	7.724838
6.295647	510.908569	7.729843
6.172313	521.185798	7.734848
5.799832	526.992894	7.739853
5.934947	517.418518	7.744858
6.128934	521.568877	7.749862
6.251971	521.665184	7.754867
6.160175	526.030409	7.759872
6.341035	522.901877	7.764877
6.626706	514.074568	7.769882
5.785496	503.219708	7.774886
6.148027	495.243835	7.779891
6.071033	493.164638	7.784896
6.134113	490.770381	7.789901
6.195002	487.221654	7.794906
5.989986	496.281782	7.799910
6.190405	492.284288	7.804915
6.036411	498.514601	7.809920
5.721729	489.624504	7.814925
6.018825	488.416977	7.819930
5.878767	487.275720	7.824934
6.119624	481.461532	7.829939
6.088100	492.314177	7.834944
5.983550	484.040115	7.839949
6.003356	497.350419	7.844954
5.988337	493.744205	7.849958
5.895669	485.366544	7.854963
6.164904	492.492356	7.859968
5.848342	489.326808	7.864973
6.207580	489.537337	7.869978
6.159578	488.278614	7.874982
5.945055	484.893898	7.879987
5.774479	498.028717	7.884992
5.977833	491.502814	7.889997
6.492557	495.218005	7.895002
6.153153	493.098390	7.900006
6.175001	490.209323	7.905011
6.127291	486.590961	7.910016
5.972083	495.938061	7.915021
6.230331	487.107020	7.920026
5.893778	493.135489	7.925030
6.077107	485.305527	7.930035
6.128089	497.407883	7.935040
5.922147	496.364167	7.940045
5.690141	490.062504	7.945050
5.570968	494.035007	7.950054
5.929131	485.006462	7.955059
5.874744	484.792330	7.960064
6.118055	490.601639	7.965069
6.140894	496.119874	7.970074
5.845794	494.318928	7.975078
5.723681	484.527665	7.980083
5.752845	489.411784	7.985088
5.872191	479.118767	7.990093
5.811209	482.503426	7.995098
5.683804	511.736208	8.000102
6.022331	515.516693	8.005107
6.101227	524.000361	8.010112
6.070732	509.632716	8.015130
6.276243	513.418551	8.020147
6.140512	529.541935	8.025165
6.031009	505.607650	8.030182
6.100751	504.681455	8.035200
6.272961	510.781304	8.040218
6.419924	498.383088	8.045235
5.963338	491.490736	8.050253
5.933564	486.718305	8.055270
6.129516	490.002406	8.060288
5.744508	488.160049	8.065306
6.039961	489.894517	8.070323
5.848116	489.334450	8.075341
6.265591	486.958649	8.080358
6.179509	495.127692	8.085376
5.995518	497.334042	8.090394
6.150831	493.008092	8.095411
6.056573	489.972789	8.100429
6.294124	479.008698	8.105446
6.073374	490.362606	8.110464
6.091255	494.683800	8.115482
6.197619	484.498855	8.120499
5.721726	493.151903	8.125517
5.968134	501.286954	8.130534
6.212192	513.302048	8.135552
6.217167	521.555035	8.140570
6.245734	520.526807	8.145587
5.838289	510.595811	8.150605
6.155296	522.712999	8.155622
6.303166	524.244758	8.160640
6.189122	517.711000	8.165658
6.350074	520.462949	8.170675
6.287444	514.460011	8.175693
5.908579	486.413563	8.180710
6.175250	497.004529	8.185728
5.963117	517.620353	8.190746
6.200376	509.966689	8.195763
5.968240	523.586915	8.200781
6.115591	517.935006	8.205798
6.324096	514.952116	8.210816
6.202144	519.762582	8.215834
6.539107	517.904797	8.220851
6.068380	515.859717	8.225869
6.375120	518.027721	8.230886
6.356406	518.177123	8.235904
6.286848	522.351595	8.240922
6.320627	521.395727	8.245939
6.003590	522.735591	8.250957
6.160613	521.875842	8.255974
6.316234	527.285579	8.260992
6.296033	525.224552	8.266010
6.243309	518.879051	8.271027
6.089394	524.613251	8.276045
6.242502	523.628569	8.281062
6.444376	523.042083	8.286080
6.032612	518.378167	8.291098
6.376724	516.528648	8.296115
6.200639	526.522130	8.301133
6.442440	523.785086	8.306150
6.526023	536.000774	8.311168
6.039634	522.934042	8.316186
6.196251	517.589239	8.321203
6.242480	530.290012	8.326221
6.559075	523.903234	8.331238
6.277814	514.077121	8.336256
6.205446	528.247823	8.341274
6.305800	516.967274	8.346291
6.337666	524.329651	8.351309
6.350943	515.861163	8.356326
6.630640	514.686634	8.361344
6.126751	525.265461	8.366362
5.991724	520.874793	8.371379
6.019513	525.168767	8.376397
6.202813	519.566609	8.381414
6.178875	525.718823	8.386432
6.293208	528.008447	8.391450
6.676025	514.381875	8.396467
6.340006	516.742921	8.401485
6.297101	535.690900	8.406502
6.405016	519.330508	8.411520
6.009182	526.238547	8.416538
6.598770	537.592943	8.421555
6.507581	547.761148	8.426573
6.480179	536.842661	8.431590
6.360740	535.294882	8.436608
6.452543	552.593129	8.441626
6.461318	552.538189	8.446643
6.570950	558.444495	8.451661
6.404555	548.655044	8.456678
6.392700	540.324947	8.461696
6.611544	555.472777	8.466714
6.638557	546.596514	8.471731
6.461648	531.057236	8.476749
6.342302	522.355605	8.481766
6.579277	540.001819	8.486784
6.748506	549.024616	8.491802
6.501232	528.511699	8.496819
6.416618	522.659238	8.501837
6.484298	527.089117	8.506854
6.863878	533.670742	8.511872
6.437449	530.821332	8.516890
6.177770	516.351411	8.521907
6.310976	538.187745	8.526925
6.361170	549.344479	8.531942
6.645703	547.540646	8.536960
6.604100	556.225745	8.541978
6.535527	556.358208	8.546995
6.729525	557.502831	8.552013
6.580773	557.327135	8.557030
6.577454	559.018176	8.562048
6.510789	562.636115	8.567066
6.247626	555.356809	8.572083
6.412199	559.318911	8.577101
6.651899	564.865909	8.582119
6.933853	554.535314	8.587136
6.400552	559.621374	8.592154
6.670167	560.014351	8.597171
6.629965	556.055381	8.602189
6.226373	559.414171	8.607207
6.537863	554.705476	8.612224
6.293745	554.597144	8.617242
6.299835	556.060658	8.622259
6.589041	566.623729	8.627277
6.411842	571.929351	8.632295
6.717649	564.033813	8.637312
6.762019	566.479506	8.642330
6.884019	566.398928	8.647347
6.950086	553.187938	8.652365
6.612791	557.800428	8.657383
6.822883	552.733353	8.662400
6.638550	551.312059	8.667418
6.483775	556.118523	8.672435
6.873296	560.709670	8.677453
6.511420	565.582318	8.682471
6.936910	558.078552	8.687488
6.649971	564.506403	8.692506
6.708408	558.391872	8.697523
6.601712	554.753341	8.702541
6.687801	559.027041	8.707559
6.875645	554.512432	8.712576
6.414047	559.675785	8.717594
7.119713	574.335962	8.722611
6.734278	569.949542	8.727629
6.523413	563.455023	8.732647
6.795740	570.579586	8.737664
6.615467	587.236945	8.742682
6.966965	575.792137	8.747699
7.156124	580.124558	8.752717
6.654407	572.424736	8.757735
6.783878	566.446067	8.762752
6.898455	574.424258	8.767770
6.507944	567.845122	8.772787
6.518545	567.257042	8.777805
6.979599	575.690819	8.782823
7.267986	579.207255	8.787840
6.773097	586.986589	8.792858
6.623812	589.213188	8.797875
6.916742	586.801109	8.802893
6.900606	588.463569	8.807911
7.043408	577.270823	8.812928
7.046644	584.014191	8.817946
6.700968	571.674659	8.822963
6.983652	580.323789	8.827981
7.067957	581.243680	8.832999
6.917749	574.346815	8.838016
6.758297	568.066208	8.843034
6.759307	579.139184	8.848051
6.973737	575.471488	8.853069
6.791408	591.098551	8.858087
6.893782	581.539753	8.863104
6.968320	587.694779	8.868122
6.927327	580.152703	8.873139
7.070184	580.354283	8.878157
6.915313	591.043264	8.883175
6.893421	580.385234	8.888192
6.789816	574.932329	8.893210
6.853930	584.128054	8.898227
7.108316	572.524733	8.903245
6.919590	577.121879	8.908263
7.059600	588.650160	8.913280
6.784901	579.081957	8.918298
6.879351	582.486423	8.923315
7.095894	588.368344	8.928333
7.083877	587.936164	8.933351
7.117093	585.602128	8.938368
6.880924	589.070987	8.943386
7.076563	585.497930	8.948403
7.279381	577.743249	8.953421
6.766880	591.803242	8.958439
7.027713	587.648953	8.963456
6.933163	585.693137	8.968474
6.851690	579.545076	8.973491
6.762395	573.133959	8.978509
6.750899	591.678998	8.983527
6.942755	582.040819	8.988544
7.516762	582.892219	8.993562
7.077115	577.431773	8.998579
7.229381	575.810655	9.003597
6.782748	592.732190	9.008615
6.941560	579.279654	9.013632
7.117294	580.041304	9.018650
7.014763	583.482718	9.023667
6.852295	579.857747	9.028685
7.022585	600.025735	9.033703
7.347764	612.836871	9.038720
7.424640	609.709825	9.043738
6.902077	593.742319	9.048755
7.380715	581.593033	9.053773
7.170766	588.694714	9.058791
7.367364	584.945525	9.063808
7.279845	584.449868	9.068826
7.080884	588.931397	9.073843
7.249591	578.023712	9.078861
6.840733	586.171058	9.083879
7.295961	582.709337	9.088896
7.517789	581.542024	9.093914
6.867066	585.996396	9.098931
7.161911	585.784251	9.103949
7.251516	603.862002	9.108967
7.600167	599.921107	9.113984
7.501298	582.827221	9.119002
7.376444	589.482950	9.124019
7.459359	579.758292	9.129037
7.093143	580.365211	9.134055
7.425577	586.009058	9.139072
7.228907	588.932041	9.144090
7.186504	586.395580	9.149107
7.414832	585.581104	9.154125
7.059514	579.879149	9.159143
7.253009	579.555055	9.164160
7.161486	582.257687	9.169178
7.018002	583.346784	9.174195
7.213430	577.861093	9.179213
6.990245	595.453459	9.184231
7.241994	605.063963	9.189248
7.660219	612.077384	9.194266
7.348416	614.728904	9.199283
7.626815	619.030615	9.204301
7.292326	613.970630	9.209319
6.979585	597.956565	9.214336
7.437892	604.179537	9.219354
7.194467	612.902418	9.224371
7.375730	613.258258	9.229389
7.336177	615.968627	9.234407
7.537180	615.428342	9.239424
7.583018	607.998441	9.244442
7.546450	602.677724	9.249459
7.663696	601.193102	9.254477
7.680121	594.331428	9.259495
7.251773	580.677318	9.264512
7.558051	587.054582	9.269530
7.231150	584.524683	9.274547
7.594877	589.304350	9.279565
7.411104	592.134260	9.284583
7.135418	583.424233	9.289600
7.659066	602.871354	9.294618
7.767688	609.670310	9.299635
7.645321	585.458325	9.304653
7.363685	580.979718	9.309671
7.635048	585.421552	9.314688
7.369500	581.434738	9.319706
7.330516	579.776788	9.324723
7.395383	580.816425	9.329741
7.422239	609.480264	9.334759
7.681007	609.413848	9.339776
7.966286	606.480231	9.344794
7.473147	597.258601	9.349811
7.161689	585.359033	9.354829
7.269884	587.704009	9.359847
7.377424	601.563707	9.364864
7.790663	597.321191	9.369882
7.551238	614.650340	9.374899
7.947249	596.659583	9.379917
7.817105	605.272763	9.384935
7.785451	586.768225	9.389952
7.526085	574.690562	9.394970
6.999272	572.812034	9.399987
7.543064	592.663261	9.405005
7.524750	609.103876	9.410023
7.543875	599.744667	9.415040
8.032482	593.855131	9.420058
7.590794	605.831103	9.425075
7.903089	610.109090	9.430093
7.639416	603.599285	9.435111
7.426539	606.848163	9.440128
7.590017	598.760638	9.445146
7.528556	600.869553	9.450163
7.839634	599.019392	9.455181
7.622280	601.717864	9.460199
7.283461	605.767862	9.465216
7.686623	601.490008	9.470234
7.425686	606.776635	9.475251
7.615489	605.352829	9.480269
7.452189	617.334283	9.485287
7.424101	607.775420	9.490304
7.661243	599.982763	9.495322
7.496118	610.266592	9.500339
7.850293	601.782944	9.505357
7.863189	602.817804	9.510375
7.625354	611.679513	9.515392
7.927394	605.350030	9.520410
7.868817	610.102788	9.525427
7.852708	606.304570	9.530445
7.899159	610.062046	9.535463
7.860385	607.445852	9.540480
8.136386	605.499537	9.545498
7.592526	610.638145	9.550515
7.684333	604.018692	9.555533
7.517938	600.604393	9.560551
7.518113	610.073105	9.565568
7.699037	602.335029	9.570586
7.665566	603.162226	9.575603
7.756433	619.010006	9.580621
7.790519	630.023805	9.585639
8.109376	639.025224	9.590656
8.124349	634.043971	9.595674
7.904913	624.911246	9.600691
7.871668	614.237161	9.605709
8.011432	611.792964	9.610727
7.884935	615.517273	9.615744
7.648256	602.540809	9.620762
7.420611	610.630407	9.625779
8.044077	621.354098	9.630797
8.166491	636.908502	9.635815
7.805905	632.490195	9.640832
8.172667	639.686549	9.645850
8.042282	623.795794	9.650867
7.826702	617.748069	9.655885
8.380121	623.973409	9.660903
7.886233	611.422182	9.665920
8.141936	599.738510	9.670938
7.715412	606.274525	9.675955
7.844368	597.569135	9.680973
7.719552	611.499992	9.685991
8.033580	624.309441	9.691008
8.208843	621.323572	9.696026
7.836921	636.949991	9.701043
8.351950	639.171312	9.706061
8.262971	634.192313	9.711079
7.855105	625.848223	9.716096
8.322101	617.633662	9.721114
8.094264	619.316221	9.726131
7.946801	603.157466	9.731149
7.977399	601.921036	9.736167
8.074996	603.746149	9.741184
8.339010	604.021362	9.746202
8.049148	602.439202	9.751219
7.951869	610.037558	9.756237
8.205866	611.780479	9.761255
7.757817	602.466739	9.766272
8.325629	612.390636	9.771290
8.424625	608.589891	9.776307
8.394697	607.875261	9.781325
8.131963	600.260254	9.786343
7.747545	597.199753	9.791360
7.893505	593.018818	9.796378
8.150461	613.232509	9.801395
8.316392	622.791884	9.806413
8.157783	616.188303	9.811431
8.170562	607.516317	9.816448
8.332598	603.847252	9.821466
7.965309	606.715425	9.826483
8.259986	609.630668	9.831501
8.242991	608.449359	9.836519
7.885766	617.748531	9.841536
8.301545	620.819303	9.846554
8.288705	635.979987	9.851571
8.335089	635.375546	9.856589
8.589700	628.218133	9.861607
7.939836	616.697784	9.866624
8.371394	616.585435	9.871642
7.998289	619.975801	9.876659
8.336562	623.151921	9.881677
8.611678	633.706152	9.886695
8.180883	620.886217	9.891712
8.440076	615.394088	9.896730
8.304460	607.110825	9.901747
8.121096	605.176012	9.906765
8.206287	600.609888	9.911783
8.141073	618.288122	9.916800
8.486775	621.686620	9.921818
8.272255	631.248372	9.926835
8.417514	628.130470	9.931853
8.406862	630.730551	9.936871
8.480794	640.355168	9.941888
8.449701	629.927945	9.946906
8.332414	629.581300	9.951923
8.298946	623.388857	9.956941
8.416718	623.659154	9.961959
7.810443	636.324960	9.966976
8.141934	632.240845	9.971994
8.420777	635.235875	9.977011
8.107064	638.864426	9.982029
8.660463	630.137945	9.987047
8.134601	635.422390	9.992064
8.259519	630.603237	9.997082
8.335202	640.443299	10.002099
8.457402	627.946725	10.007117
8.406412	627.261564	10.012135
8.239078	638.340609	10.017152
8.560659	626.956225	10.022170
8.236601	639.883551	10.027187
8.505666	633.143401	10.032205
8.487603	629.755317	10.037223
8.103589	637.557849	10.042240
8.503713	643.625522	10.047258
8.751428	671.785609	10.052275
8.701160	663.311029	10.057293
8.544427	646.211695	10.062311
8.434400	648.574706	10.067328
8.334569	645.372983	10.072346
8.617124	663.467275	10.077363
8.738435	662.200859	10.082381
8.782250	638.706897	10.087399
8.535400	644.966342	10.092416
8.649388	634.390296	10.097434
8.389656	639.124407	10.102451
8.641140	639.575307	10.107469
8.818950	638.150728	10.112487
8.390927	645.041710	10.117504
8.651448	642.001170	10.122522
8.474825	641.648210	10.127539
8.647754	660.371638	10.132557
8.592442	657.945564	10.137575
8.541939	665.449592	10.142592
8.881291	661.572029	10.147610
8.935989	666.224950	10.152627
8.826171	651.691703	10.157645
8.846880	645.353281	10.162663
8.661634	639.253676	10.167680
8.369860	639.612261	10.172698
8.639663	648.652121	10.177715
8.495421	658.539240	10.182733
8.779986	668.487243	10.187751
8.932521	669.330096	10.192768
8.889625	666.264208	10.197786
8.997491	653.487326	10.202803
8.823738	653.886601	10.207821
8.590553	640.078869	10.212839
8.078344	648.908478	10.217856
8.884011	664.779273	10.222874
9.215220	665.589391	10.227891
9.069694	665.943050	10.232909
9.053215	646.445043	10.237927
8.678967	634.029488	10.242944
8.720042	632.541336	10.247962
8.665204	639.280763	10.252979
8.521608	667.955612	10.257997
9.109623	660.982331	10.263015
8.939607	681.544355	10.268032
9.183106	672.095195	10.273050
9.227018	649.091724	10.278067
8.706835	638.116780	10.283085
8.716693	640.885109	10.288103
8.138038	640.394797	10.293120
8.423197	651.036348	10.298138
8.692012	663.168318	10.303155
8.802139	670.557173	10.308173
9.362174	664.214077	10.313191
9.065008	667.956818	10.318208
8.460643	664.652032	10.323226
8.506142	666.345237	10.328243
8.583271	667.619056	10.333261
8.858183	664.455270	10.338279
8.474357	664.638558	10.343296
8.699560	683.546653	10.348314
8.957528	694.258874	10.353331
9.015055	699.408946	10.358349
9.481675	682.839779	10.363367
9.224567	694.437244	10.368384
9.398330	685.754304	10.373402
9.427978	669.060278	10.378419
9.267385	672.793395	10.383437
9.403818	666.789718	10.388455
8.942552	666.657108	10.393472
9.209653	665.445680	10.398490
9.363825	658.390312	10.403507
8.845608	662.290120	10.408525
9.221047	662.400435	10.413543
9.183280	666.867893	10.418560
9.271528	669.467350	10.423578
9.716451	663.138592	10.428595
8.853737	658.792401	10.433613
9.236029	661.591577	10.438631
9.385513	666.420917	10.443648
9.166641	669.503488	10.448666
9.143614	668.853063	10.453683
9.032954	668.986394	10.458701
9.255728	671.809231	10.463719
9.189782	672.742196	10.468736
9.064248	669.267182	10.473754
9.261130	664.771121	10.478771
9.008576	670.106773	10.483789
9.091526	661.604622	10.488807
8.797054	661.584937	10.493824
9.325354	658.368565	10.498842
9.231868	657.349909	10.503859
8.778735	663.068750	10.508877
9.138507	664.280807	10.513895
9.165327	664.304370	10.518912
9.197533	667.646134	10.523930
9.282038	665.396896	10.528947
9.276828	667.083144	10.533965
9.472220	660.382739	10.538983
9.040194	666.321301	10.544000
9.153365	665.592815	10.549018
9.467199	660.846301	10.554035
9.127642	669.835904	10.559053
9.376029	664.139654	10.564071
9.378314	665.947882	10.569088
9.288968	662.800321	10.574106
9.180032	660.639410	10.579123
9.295181	668.710856	10.584141
9.682600	665.338294	10.589159
9.184686	672.589266	10.594176
9.276820	664.519032	10.599194
9.438623	661.841665	10.604211
9.064824	683.815305	10.609229
9.478061	688.510432	10.614247
9.414421	699.977839	10.619264
9.686674	699.249779	10.624282
9.637583	696.006574	10.629299
9.374698	680.646727	10.634317
9.173481	670.050808	10.639335
9.626922	690.668259	10.644352
9.555459	692.308004	10.649370
9.349642	686.449568	10.654387
9.665930	697.434008	10.659405
9.554598	686.469671	10.664423
9.648023	692.385404	10.669440
9.346143	683.502502	10.674458
9.373532	674.695390	10.679475
9.313739	690.535910	10.684493
9.287044	690.978941	10.689511
9.715544	693.911015	10.694528
9.394861	699.489834	10.699546
9.387913	695.838887	10.704563
9.142784	701.401653	10.709581
9.229238	697.793110	10.714599
9.415424	704.082441	10.719616
9.218281	700.705886	10.724634
9.590142	693.804602	10.729651
9.458039	697.731816	10.734669
9.879750	714.137867	10.739687
9.681865	703.594520	10.744704
9.496673	699.963639	10.749722
9.704144	695.683913	10.754739
9.412505	700.617016	10.759757
9.698525	707.406323	10.764775
9.569087	725.469308	10.769792
9.652142	732.112324	10.774810
9.762165	724.994555	10.779827
9.944675	733.029291	10.784845
9.892666	714.120515	10.789863
9.701486	699.793598	10.794880
9.532071	700.951954	10.799898
9.663869	705.478741	10.804915
9.878834	719.496337	10.809933
10.120470	716.058933	10.814951
9.807995	705.375119	10.819968
9.363670	698.384193	10.824986
9.932703	699.450978	10.830003
9.993376	706.528767	10.835021
10.285531	695.735786	10.840039
10.419308	688.974316	10.845056
10.090538	690.862561	10.850074
9.970508	696.902219	10.855091
9.867619	703.433107	10.860109
9.391573	696.042340	10.865127
9.929182	692.434285	10.870144
9.654661	695.661107	10.875162
9.769968	689.465261	10.880179
9.742280	693.326367	10.885197
9.789606	691.932444	10.890215
9.805966	696.328352	10.895232
9.570691	697.480685	10.900250
9.841388	685.720061	10.905267
9.840032	698.784934	10.910285
10.032930	697.456664	10.915303
10.211342	708.832031	10.920320
9.981865	702.793265	10.925338
9.926479	690.595323	10.930355
9.745208	690.905691	10.935373
9.908967	708.859481	10.940391
10.191734	714.839534	10.945408
9.793306	716.420043	10.950426
10.135731	709.803925	10.955443
9.939912	725.779204	10.960461
10.179892	726.127293	10.965479
10.254699	717.848889	10.970496
9.742615	709.582636	10.975514
10.157422	712.220541	10.980531
10.161292	728.524941	10.985549
10.382311	722.850916	10.990567
10.081948	701.465311	10.995584
9.687493	701.808225	11.000602
10.190595	709.037544	11.005619
10.031798	718.018501	11.010637
10.209414	724.541924	11.015655
10.574027	714.278635	11.020672
10.112988	697.857550	11.025690
10.067063	692.684406	11.030707
9.998637	696.099529	11.035725
10.201134	698.720623	11.040743
10.256786	695.551013	11.045760
10.075053	698.793572	11.050778
10.230630	696.942379	11.055795
10.409562	711.037583	11.060813
9.999949	702.463045	11.065831
10.021794	699.184866	11.070848
10.202474	724.340576	11.075866
10.305127	720.419914	11.080883
10.139318	723.445680	11.085901
10.127905	727.517867	11.090919
10.230586	718.133728	11.095936
10.315808	720.537250	11.100954
10.529049	717.082895	11.105971
10.557576	726.317862	11.110989
10.448776	727.456735	11.116007
10.267829	705.277378	11.121024
9.920553	703.959818	11.126042
10.114869	711.643002	11.131059
10.215367	731.072564	11.136077
10.371190	726.299048	11.141095
10.468411	713.710483	11.146112
10.125356	718.112372	11.151130
10.588463	714.842614	11.156147
10.751731	718.874458	11.161165
10.186157	726.292555	11.166183
10.313071	720.682537	11.171200
10.228989	721.993684	11.176218
10.461216	723.886277	11.181235
10.575792	720.710843	11.186253
10.312710	719.995841	11.191271
10.456727	717.167874	11.196288
10.094140	723.106770	11.201306
10.220379	718.201943	11.206323
10.444757	733.581696	11.211341
10.262501	724.225051	11.216359
10.221716	725.293609	11.221376
10.335176	733.692909	11.226394
10.350410	728.316723	11.231411
10.370407	729.114208	11.236429
10.206502	747.429763	11.241447
10.845406	740.518096	11.246464
10.793855	748.332950	11.251482
10.537632	739.775509	11.256499
10.747638	735.802816	11.261517
10.481037	728.622614	11.266535
10.580620	725.845702	11.271552
10.439548	730.608614	11.276570
10.943961	741.911521	11.281587
10.810298	735.447451	11.286605
10.434313	731.715879	11.291623
10.626575	719.236762	11.296640
10.620165	748.567746	11.301658
10.600909	744.435781	11.306675
10.838429	740.542385	11.311693
10.532384	739.560889	11.316711
10.766048	739.914748	11.321728
10.734352	737.734344	11.326746
10.939734	734.072243	11.331763
10.754624	733.502194	11.336781
10.512961	730.621954	11.341799
10.947149	719.519233	11.346816
10.555057	738.278051	11.351834
10.400575	741.997576	11.356851
10.764962	738.773292	11.361869
10.275145	751.286450	11.366887
10.800740	744.525032	11.371904
10.537813	753.139416	11.376922
10.765262	741.866593	11.381939
10.881728	745.393230	11.386957
10.607615	753.419734	11.391975
11.125218	750.477935	11.396992
10.640067	755.921024	11.402010
10.930731	757.271691	11.407027
11.214855	744.619870	11.412045
10.815420	752.184869	11.417063
10.743596	753.095192	11.422080
10.972003	752.488557	11.427098
10.792810	750.286908	11.432115
11.165983	755.112305	11.437133
10.827690	753.891279	11.442151
11.005361	746.303662	11.447168
11.293233	756.029926	11.452186
11.051791	752.814230	11.457203
11.143126	740.855717	11.462221
10.762252	750.905300	11.467239
10.727579	745.263765	11.472256
10.995726	751.080515	11.477274
11.160628	752.956308	11.482291
11.602908	746.812590	11.487309
11.243126	753.281319	11.492327
11.593516	742.252691	11.497344
10.958505	737.543986	11.502362
11.025181	726.280868	11.507379
11.226525	728.419114	11.512397
10.733736	743.520802	11.517415
10.977990	735.481638	11.522432
11.112888	738.500525	11.527450
10.954613	751.792202	11.532467
11.167962	751.362461	11.537485
10.609816	750.073909	11.542503
11.081088	745.913471	11.547520
11.231685	747.145605	11.552538
11.317325	747.641293	11.557555
11.056651	743.913063	11.562573
11.049639	743.866642	11.567591
10.834814	744.321537	11.572608
10.889372	741.852848	11.577626
10.775499	751.635791	11.582643
11.047619	741.866907	11.587661
10.682005	755.896818	11.592679
11.112698	768.583531	11.597696
11.351155	786.545514	11.602714
11.281929	773.954148	11.607731
11.477991	774.530365	11.612749
11.563075	780.651440	11.617767
11.479127	779.524509	11.622784
11.487622	783.402874	11.627802
10.873867	764.661065	11.632819
11.181558	768.909152	11.637837
11.324857	777.373217	11.642855
11.630351	782.080308	11.647872
11.372584	778.730703	11.652890
11.124321	780.747746	11.657907
11.515081	772.955943	11.662925
11.272959	781.928689	11.667943
11.383480	777.566182	11.672960
11.485355	779.288644	11.677978
11.410140	779.596412	11.682995
11.424479	772.070079	11.688013
11.416707	779.869827	11.693031
11.300646	772.243439	11.698048
11.291358	775.645244	11.703066
11.028700	782.255374	11.708083
11.733938	769.217284	11.713101
10.977024	771.300442	11.718119
11.236484	773.062555	11.723136
11.374390	773.118903	11.728154
11.170128	778.610365	11.733171
11.595296	777.352283	11.738189
11.226079	779.303926	11.743207
11.701226	793.185991	11.748224
11.659482	794.751538	11.753242
11.505245	801.923615	11.758259
11.660800	802.658107	11.763277
11.697831	808.893050	11.768295
11.464037	790.581182	11.773312
11.865885	789.585215	11.778330
11.710401	782.705076	11.783347
11.785166	775.446279	11.788365
11.307859	773.465241	11.793383
11.634330	781.142718	11.798400
11.999648	791.495516	11.803418
11.583993	783.142788	11.808435
11.592218	769.575265	11.813453
11.607598	783.107098	11.818471
11.986446	784.758109	11.823488
11.807528	774.804848	11.828506
11.748696	779.305352	11.833523
11.954243	770.930471	11.838541
11.946207	776.261494	11.843559
11.723426	762.306268	11.848576
11.645509	763.201460	11.853594
11.201478	772.337155	11.858611
11.700221	784.583502	11.863629
11.597858	797.329767	11.868647
11.795224	803.902707	11.873664
12.168018	805.480317	11.878682
12.107724	798.485200	11.883699
12.437236	793.586058	11.888717
11.838720	787.777650	11.893735
12.009375	769.778736	11.898752
12.067341	769.482198	11.903770
11.735423	766.251955	11.908787
12.053469	765.013581	11.913805
11.994608	767.326407	11.918823
11.660196	764.048549	11.923840
12.052107	762.166087	11.928858
11.397318	767.973080	11.933875
12.005727	776.026681	11.938893
11.796562	787.351722	11.943911
12.312135	788.129351	11.948928
12.268141	776.205030	11.953946
11.624778	769.480482	11.958963
11.998911	782.420260	11.963981
11.917510	793.375743	11.968999
11.878351	800.270509	11.974016
12.253052	799.278250	11.979034
12.073472	788.414901	11.984051
12.288601	795.173468	11.989069
11.881967	804.078985	11.994087
11.825413	793.967268	11.999104
12.444535	791.530671	12.004122
11.899942	800.309038	12.009139
12.228068	791.133180	12.014157
12.165353	798.327500	12.019175
12.081251	789.782079	12.024192
12.452183	801.195710	12.029210
12.439221	797.730371	12.034227
12.349171	787.357684	12.039245
12.434984	796.200156	12.044263
12.178789	780.900515	12.049280
12.225662	761.382819	12.054298
12.029655	769.669218	12.059315
12.345855	775.375663	12.064333
12.406817	774.046006	12.069351
12.077538	787.540037	12.074368
12.461984	781.666498	12.079386
12.341195	786.621334	12.084403
12.050444	779.680527	12.089421
12.209935	795.176592	12.094439
12.117334	799.829143	12.099456
12.462510	788.413570	12.104474
12.102339	796.424427	12.109491
12.328978	794.990567	12.114509
12.355042	793.611572	12.119527
12.110954	800.459568	12.124544
12.426019	796.088381	12.129562
12.445903	799.290095	12.134579
12.397533	793.357125	12.139597
12.343607	791.379596	12.144615
12.313754	800.115246	12.149632
12.242213	795.813981	12.154650
12.259981	791.699493	12.159667
12.201389	787.864566	12.164685
12.632138	790.586455	12.169703
12.197770	786.353934	12.174720
12.271273	780.050806	12.179738
12.250141	788.007487	12.184755
12.623161	802.953661	12.189773
12.665803	810.252188	12.194791
12.435055	799.439822	12.199808
12.765583	798.421414	12.204826
12.598719	797.942431	12.209843
12.748182	791.330673	12.214861
12.462009	786.060673	12.219879
12.259950	787.893697	12.224896
12.317261	798.473477	12.229914
12.760557	818.532571	12.234931
13.038702	814.307250	12.239949
13.221631	821.712467	12.244967
12.595118	806.669780	12.249984
12.659897	788.078172	12.255002
12.619087	793.329593	12.260019
12.670015	787.434511	12.265037
12.565313	789.059298	12.270055
12.770276	797.512769	12.275072
12.955809	786.944457	12.280090
12.500351	792.025968	12.285107
12.443696	800.559767	12.290125
12.740850	813.443424	12.295143
13.026681	817.020768	12.300160
13.265030	809.006559	12.305178
12.558453	803.999069	12.310195
12.703120	808.798151	12.315213
12.669479	812.432726	12.320231
12.384057	823.241707	12.325248
12.960218	818.626109	12.330266
12.804908	819.451052	12.335283
12.788631	821.008448	12.340301
13.063368	808.235695	12.345319
12.387909	824.949126	12.350336
12.801529	823.655159	12.355354
12.890308	816.526694	12.360371
12.918016	816.801673	12.365389
12.856175	813.423947	12.370407
12.705936	816.132602	12.375424
13.078356	816.047366	12.380442
12.799680	821.098039	12.385459
12.955813	827.655770	12.390477
12.891108	813.313710	12.395495
12.664011	816.736238	12.400512
13.513171	830.827651	12.405530
13.163235	828.111377	12.410547
13.181524	818.424631	12.415565
13.074655	815.679133	12.420583
12.759019	817.108548	12.425600
12.894673	820.578878	12.430618
13.019487	835.052429	12.435635
13.387107	847.980743	12.440653
13.479967	841.046069	12.445671
13.453939	825.492928	12.450688
13.500746	815.321958	12.455706
13.226275	817.509086	12.460723
13.244393	817.646683	12.465741
13.160686	813.284439	12.470759
13.238187	818.142281	12.475776
13.344302	809.615742	12.480794
13.393083	816.222346	12.485811
13.507731	808.157757	12.490829
13.293117	812.433291	12.495847
13.134819	814.916126	12.500864
12.976342	814.163326	12.505882
13.295688	817.337110	12.510899
13.074674	815.047499	12.515917
13.570573	812.482098	12.520935
13.478133	812.742328	12.525952
13.516870	810.653395	12.530970
13.099834	819.053582	12.535987
13.480232	815.173515	12.541005
13.514541	821.387655	12.546023
12.948578	818.221351	12.551040
13.174484	816.305744	12.556058
12.784304	812.712323	12.561075
13.103424	821.646879	12.566093
12.973711	833.109184	12.571111
13.065150	845.224215	12.576128
13.454021	842.533625	12.581146
13.640570	848.282037	12.586163
13.640655	852.148033	12.591181
13.738763	841.406373	12.596199
13.638398	851.444216	12.601216
13.525933	855.263104	12.606234
13.937583	848.350046	12.611251
13.402831	843.167642	12.616269
13.336610	851.210164	12.621287
13.338199	848.972266	12.626304
13.676419	843.955530	12.631322
13.891417	846.134443	12.636339
13.564922	852.535498	12.641357
13.767018	846.205539	12.646375
13.564771	855.335497	12.651392
13.676183	848.029655	12.656410
13.606575	845.262629	12.661427
13.347843	851.658762	12.666445
13.458261	843.627532	12.671463
13.473070	847.823356	12.676480
13.833945	847.377845	12.681498
13.593161	851.130189	12.686515
13.400873	848.360249	12.691533
13.614479	843.720823	12.696551
13.854873	850.145326	12.701568
13.730442	850.094333	12.706586
13.585442	859.210877	12.711603
13.786200	878.820076	12.716621
14.309286	875.239187	12.721639
14.175565	859.611722	12.726656
13.950586	842.923845	12.731674
13.909857	855.383982	12.736691
13.897754	844.559393	12.741709
14.126329	840.515099	12.746727
13.948005	841.135990	12.751744
14.249041	835.388442	12.756762
14.042752	842.990003	12.761779
14.052768	839.144490	12.766797
14.216856	836.199798	12.771815
13.868304	842.223418	12.776832
13.888058	837.013761	12.781850
14.380489	837.791681	12.786867
13.845359	840.513288	12.791885
14.127796	832.017380	12.796903
13.751274	841.204925	12.801920
13.975878	826.277966	12.806938
14.233128	832.032774	12.811955
14.162832	841.785331	12.816973
14.047032	831.527896	12.821991
13.988580	837.681421	12.827008
13.988728	843.685096	12.832026
13.998480	841.513561	12.837043
14.138069	844.761995	12.842061
14.130793	839.376507	12.847079
14.069882	846.068212	12.852096
14.035333	839.600678	12.857114
14.185645	836.485441	12.862131
14.026075	838.981088	12.867149
14.251078	839.074980	12.872167
14.165465	844.296044	12.877184
14.000513	834.859698	12.882202
14.115528	833.254958	12.887219
14.078635	838.627393	12.892237
14.287406	843.546179	12.897255
14.478254	867.969372	12.902272
14.264970	869.271219	12.907290
14.502742	862.771574	12.912307
14.397698	853.113890	12.917325
14.430480	847.295802	12.922343
14.121188	850.585890	12.927360
14.515044	862.983913	12.932378
14.572237	855.569335	12.937395
14.247972	847.431349	12.942413
14.573987	844.329928	12.947431
14.521090	845.574507	12.952448
14.254160	830.593509	12.957466
14.546271	844.427586	12.962483
14.139405	851.443890	12.967501
14.462177	862.182897	12.972519
14.519791	864.970522	12.977536
14.721512	871.325457	12.982554
14.547466	869.928019	12.987571
14.487558	875.737722	12.992589
14.638859	866.980452	12.997607
14.487334	872.910045	13.002624
14.472446	863.116172	13.007642
14.633580	864.329642	13.012659
14.494724	872.424358	13.017677
14.619157	864.521499	13.022695
14.436948	876.129923	13.027712
14.716853	875.937572	13.032730
14.853438	869.709785	13.037747
14.730394	871.064009	13.042765
14.887704	868.507424	13.047783
14.714283	864.568269	13.052800
14.483921	873.251339	13.057818
14.526718	866.925309	13.062835
14.310010	864.805049	13.067853
14.518167	867.466570	13.072871
14.688479	865.614098	13.077888
14.761521	867.346070	13.082906
14.691886	870.038631	13.087923
14.512042	875.193422	13.092941
14.549760	862.534279	13.097959
14.662817	883.026468	13.102976
14.771041	893.943931	13.107994
14.861472	893.560129	13.113011
14.866950	899.777106	13.118029
14.992312	893.973196	13.123047
15.050422	895.691896	13.128064
15.007442	885.417643	13.133082
14.762068	884.006819	13.138099
14.675794	894.692720	13.143117
14.979007	897.126312	13.148135
15.069884	897.980176	13.153152
14.997270	901.359031	13.158170
15.289476	895.601507	13.163187
14.879388	901.758169	13.168205
14.980984	899.123406	13.173223
14.980599	904.022123	13.178240
15.039960	903.524967	13.183258
15.375839	906.843270	13.188275
15.247743	904.692977	13.193293
15.318395	896.335248	13.198311
15.123307	878.674710	13.203328
14.942503	873.486046	13.208346
15.177903	866.756094	13.213363
14.983358	896.416528	13.218381
15.356584	897.350799	13.223399
15.157754	899.387229	13.228416
15.270814	905.210427	13.233434
15.033480	889.384350	13.238451
15.058390	897.404720	13.243469
15.123430	889.260906	13.248487
15.001887	898.225170	13.253504
14.915186	894.573209	13.258522
15.523573	891.200623	13.263539
15.199207	895.965591	13.268557
14.987025	891.770261	13.273575
15.223803	903.676240	13.278592
14.963856	899.156943	13.283610
15.541114	887.471383	13.288627
15.498018	893.314921	13.293645
15.088241	899.318388	13.298663
15.320000	890.133234	13.303680
15.092121	897.923033	13.308698
15.424350	904.539823	13.313715
15.167296	924.651247	13.318733
15.662269	920.946268	13.323751
15.898663	921.638248	13.328768
15.654866	912.096019	13.333786
15.641161	892.219701	13.338803
15.621008	885.619848	13.343821
15.421381	885.675397	13.348839
15.644222	885.857832	13.353856
15.585580	884.328690	13.358874
15.274091	886.164098	13.363891
15.721571	897.983611	13.368909
15.454899	890.898616	13.373927
16.084360	906.932299	13.378944
15.609786	895.051627	13.383962
15.919891	880.987977	13.388979
15.624763	883.540328	13.393997
15.736061	876.727776	13.399015
15.743191	875.659375	13.404032
15.566552	883.610360	13.409050
15.941404	879.530417	13.414067
15.960826	880.882311	13.419085
15.892187	878.876106	13.424103
15.447349	876.464894	13.429120
15.447405	881.012760	13.434138
15.492103	888.385783	13.439155
15.617069	906.458819	13.444173
15.990525	911.192097	13.449191
15.924200	909.824847	13.454208
15.894246	915.205215	13.459226
16.542482	905.664487	13.464243
15.886749	893.744131	13.469261
15.779153	882.851474	13.474279
15.795542	881.783508	13.479296
15.969617	878.377334	13.484314
16.071136	877.772809	13.489331
16.132055	883.207406	13.494349
15.900057	875.873380	13.499367
16.096471	878.794711	13.504384
15.983679	879.600412	13.509402
16.227167	871.457767	13.514419
15.770141	875.075853	13.519437
15.786011	876.389753	13.524455
16.204424	891.440697	13.529472
15.955350	900.414268	13.534490
15.869955	901.478021	13.539507
15.902956	919.559609	13.544525
16.169753	912.766566	13.549543
16.020891	909.876437	13.554560
15.878921	914.078949	13.559578
16.230326	908.541134	13.564595
15.761592	905.348869	13.569613
16.116633	910.881618	13.574631
16.371167	897.800734	13.579648
16.039504	914.895895	13.584666
16.217223	903.417420	13.589683
16.365250	911.419379	13.594701
16.118530	915.871116	13.599719
16.271789	906.699344	13.604736
15.804096	915.321740	13.609754
15.726997	914.973552	13.614771
16.563534	922.070992	13.619789
16.568424	930.773010	13.624807
16.897703	928.471786	13.629824
16.422538	929.282378	13.634842
16.460522	917.174697	13.639859
16.360401	907.391366	13.644877
16.397356	902.901247	13.649895
16.398250	902.673604	13.654912
16.382374	908.723261	13.659930
16.488379	904.831130	13.664947
16.557081	911.226217	13.669965
16.882684	918.957448	13.674983
16.800308	916.084653	13.680000
16.298311	913.229376	13.685018
16.362883	904.838005	13.690035
16.387574	911.597844	13.695053
16.453713	922.194357	13.700071
16.327404	928.176486	13.705088
16.466444	930.026664	13.710106
16.826989	926.904549	13.715123
16.892567	933.249377	13.720141
17.063688	937.189824	13.725159
17.262176	936.333424	13.730176
16.523775	916.068041	13.735194
16.749764	909.889605	13.740211
16.875442	910.943210	13.745229
16.590491	911.145165	13.750247
16.743058	904.297816	13.755264
16.700746	912.460421	13.760282
16.600320	914.617167	13.765299
16.448194	921.453531	13.770317
16.468226	931.127410	13.775335
16.757563	926.851388	13.780352
16.496480	939.671687	13.785370
16.683736	931.600130	13.790387
16.555717	928.692767	13.795405
16.557978	929.582172	13.800423
17.057553	927.838156	13.805440
17.025522	933.495634	13.810458
17.004940	931.372021	13.815475
17.011898	928.969844	13.820493
16.788532	932.469334	13.825511
17.143254	929.242675	13.830528
16.959571	934.152857	13.835546
17.112998	923.453947	13.840563
17.044513	926.634102	13.845581
16.706005	928.271242	13.850599
16.897766	941.113798	13.855616
17.133353	960.247668	13.860634
17.445120	960.568917	13.865651
17.443442	947.019807	13.870669
17.072215	939.245045	13.875687
17.242246	929.213432	13.880704
17.082188	934.675978	13.885722
17.191135	934.935932	13.890739
17.236424	939.818830	13.895757
17.624314	937.035872	13.900775
17.367128	926.732103	13.905792
17.330131	933.856875	13.910810
17.378440	924.280048	13.915827
17.385039	926.567887	13.920845
17.375465	928.170244	13.925863
17.788249	924.973340	13.930880
17.092412	934.910635	13.935898
17.497603	925.999485	13.940915
17.436658	918.394211	13.945933
17.353179	923.886197	13.950951
17.461791	922.102200	13.955968
17.148344	926.579162	13.960986
17.112904	925.924088	13.966003
17.330890	925.495544	13.971021
17.030597	935.869289	13.976039
17.433662	944.527430	13.981056
17.663150	956.324819	13.986074
17.632355	955.644960	13.991091
17.386872	948.334785	13.996109
17.066035	961.777965	14.001127
17.427241	947.451473	14.006144
17.600172	958.534243	14.011162
17.825360	970.789817	14.016179
18.091364	957.869575	14.021197
17.721014	949.400596	14.026215
18.245660	945.386774	14.031232
17.791926	947.835482	14.036250
17.786768	925.210577	14.041267
17.779649	924.687816	14.046285
17.795974	917.340209	14.051303
17.602840	919.989452	14.056320
17.824977	923.476585	14.061338
17.851808	922.847420	14.066355
17.777790	917.194621	14.071373
17.868596	921.026715	14.076391
17.928329	924.113594	14.081408
17.661425	925.025916	14.086426
17.863929	941.360244	14.091443
18.192511	945.220292	14.096461
17.890914	930.784283	14.101479
17.929225	919.778074	14.106496
17.798091	927.647927	14.111514
17.513985	920.189837	14.116531
17.975737	938.452802	14.121549
17.867192	947.807052	14.126567
18.056082	944.914136	14.131584
18.302597	943.986006	14.136602
17.973190	954.150026	14.141619
18.575058	943.453616	14.146637
18.201509	936.960681	14.151655
18.324050	923.319767	14.156672
18.189191	925.674334	14.161690
18.066790	916.804095	14.166707
18.466716	911.729485	14.171725
17.850545	912.870892	14.176743
18.080075	912.488859	14.181760
17.990447	919.326290	14.186778
17.907183	917.478794	14.191795
18.410943	936.501304	14.196813
18.078081	945.841911	14.201831
18.398776	946.028615	14.206848
18.328172	945.085675	14.211866
18.021987	939.194946	14.216883
18.388201	945.343153	14.221901
18.037027	949.269699	14.226919
18.135326	950.358154	14.231936
18.175576	948.209899	14.236954
18.040880	955.418967	14.241971
18.220151	947.649892	14.246989
18.059475	945.439637	14.252007
18.255567	939.603920	14.257024
18.504083	939.152998	14.262042
18.084730	950.089752	14.267059
18.450456	950.918579	14.272077
18.015639	958.821018	14.277095
18.541071	961.268610	14.282112
18.530010	978.516651	14.287130
18.059758	977.932787	14.292147
18.525958	970.009108	14.297165
18.495965	975.448162	14.302183
18.657776	968.946878	14.307200
18.860101	970.249596	14.312218
18.763693	977.155101	14.317235
18.843513	973.401929	14.322253
18.879346	977.947836	14.327271
18.740827	971.816741	14.332288
18.945400	969.394827	14.337306
18.834273	971.820272	14.342323
18.934172	963.470261	14.347341
18.625155	974.942284	14.352359
18.774765	975.128185	14.357376
18.879048	966.514072	14.362394
18.749206	966.048637	14.367411
19.027668	962.949949	14.372429
18.807288	973.719132	14.377447
18.884632	966.703511	14.382464
19.000047	972.148800	14.387482
18.658068	975.213628	14.392499
18.965512	976.987503	14.397517
18.917010	980.498992	14.402535
18.973725	971.259313	14.407552
19.161798	968.011819	14.412570
18.657811	968.480349	14.417587
19.072490	966.562599	14.422605
18.859568	980.378461	14.427623
18.661628	968.626722	14.432640
19.119991	973.854994	14.437658
18.910917	978.333979	14.442675
18.699383	961.671699	14.447693
18.822580	975.095299	14.452711
18.825218	971.267903	14.457728
19.039182	987.458656	14.462746
19.037572	1001.545046	14.467763
19.606718	998.345858	14.472781
19.166610	1004.057941	14.477799
19.427509	999.832276	14.482816
19.219546	997.207418	14.487834
19.286311	1003.668610	14.492851
19.701336	993.575522	14.497869
19.241232	980.162526	14.502887
19.380436	973.797656	14.507904
19.510195	971.541667	14.512922
18.869340	975.323280	14.517939
19.461231	973.052577	14.522957
19.738226	985.890112	14.527975
19.449212	978.211161	14.532992
19.672333	977.020772	14.538010
19.170406	968.946389	14.543027
19.516434	962.957496	14.548045
19.381134	971.078838	14.553063
19.472744	975.926520	14.558080
19.480733	993.006863	14.563098
19.422087	999.771485	14.568115
19.893882	990.709117	14.573133
19.813609	997.401732	14.578151
19.464417	978.869388	14.583168
19.600169	968.170618	14.588186
19.677560	985.952424	14.593203
19.787949	983.392173	14.598221
19.212788	979.782886	14.603239
19.475754	982.309374	14.608256
19.780552	991.601898	14.613274
19.732662	1003.112589	14.618291
19.904232	991.711048	14.623309
19.610303	998.173697	14.628327
19.836008	995.938824	14.633344
20.100983	986.177269	14.638362
19.903519	1000.484664	14.643379
20.128031	991.129396	14.648397
20.171619	993.489463	14.653415
20.165292	976.144789	14.658432
20.048509	968.326305	14.663450
19.831864	960.997963	14.668467
19.911755	957.775470	14.673485
19.889814	954.521416	14.678503
19.695332	961.122695	14.683520
20.076048	968.579875	14.688538
19.846620	987.316389	14.693555
20.011463	987.063565	14.698573
19.761902	991.346115	14.703591
19.822961	989.236140	14.708608
20.419723	987.562636	14.713626
19.892114	992.250662	14.718643
20.215346	989.236285	14.723661
20.162324	990.349799	14.728679
20.119237	991.714808	14.733696
20.283426	988.307491	14.738714
20.422265	994.613049	14.743731
20.311965	987.812734	14.748749
20.138519	991.874028	14.753767
20.013536	989.783441	14.758784
20.294540	986.982741	14.763802
20.152656	991.051013	14.768819
20.253684	985.455815	14.773837
20.195076	988.335933	14.778855
20.067859	987.717313	14.783872
20.233850	978.711100	14.788890
20.085924	985.557032	14.793907
20.489409	991.357762	14.798925
20.727065	993.972691	14.803943
20.365743	990.629950	14.808960
20.348355	976.970034	14.813978
19.933958	995.057291	14.818995
20.334272	1005.023351	14.824013
20.843064	1003.041984	14.829031
20.481885	1010.959814	14.834048
20.652971	1008.900906	14.839066
20.994786	1011.211594	14.844083
21.062614	1004.904197	14.849101
20.882219	992.392476	14.854119
20.558313	990.387188	14.859136
21.006365	986.056130	14.864154
20.553333	985.836329	14.869171
20.352439	979.832877	14.874189
20.608534	979.062207	14.879207
20.617970	1000.327193	14.884224
20.922416	995.807715	14.889242
20.668140	1010.421365	14.894259
20.918408	1010.509501	14.899277
20.700352	1013.608538	14.904295
20.513168	1011.701470	14.909312
20.750034	1006.905001	14.914330
20.750094	1010.492311	14.919347
20.579428	1006.195590	14.924365
20.721452	1005.443414	14.929383
20.649906	1008.477641	14.934400
20.914681	998.382659	14.939418
20.844303	999.645893	14.944435
20.780201	997.777892	14.949453
21.118120	1011.732483	14.954471
21.210105	1017.926916	14.959488
21.118479	1015.034375	14.964506
21.095755	1007.546347	14.969523
21.001344	1001.860675	14.974541
21.497936	1005.930704	14.979559
20.973632	1010.708343	14.984576
20.957872	1007.016263	14.989594
21.086170	1020.367013	14.994611
21.461956	1029.239160	14.999629
21.130232	1026.962731	15.004647
21.337140	1040.455988	15.009664
21.382519	1035.640825	15.014682
21.176374	1036.952920	15.019699
21.666671	1032.388091	15.024717
21.580966	1025.307319	15.029735
21.355948	1024.606076	15.034752
21.330908	1009.785236	15.039770
21.136873	1013.793254	15.044787
21.411229	1021.068472	15.049805
21.703690	1031.521289	15.054823
21.582461	1031.713457	15.059840
21.523201	1017.725411	15.064858
21.733901	1021.648304	15.069875
21.441124	1015.520294	15.074893
21.742583	996.078251	15.079911
21.325014	996.009264	15.084928
21.436577	999.961558	15.089946
21.095762	1017.516598	15.094963
21.698061	1023.721805	15.099981
21.728483	1026.899382	15.104999
21.329009	1025.878220	15.110016
21.455063	1014.252318	15.115034
21.699244	1019.099946	15.120051
21.545153	1025.719366	15.125069
21.863366	1027.125730	15.130087
21.758142	1027.618387	15.135104
21.689553	1025.215712	15.140122
21.808662	1021.241070	15.145139
21.918070	1022.720196	15.150157
21.797689	1014.293252	15.155175
21.908959	1019.644760	15.160192
21.919526	1018.471453	15.165210
21.866590	1019.772350	15.170227
21.601225	1025.678333	15.175245
21.958202	1031.803697	15.180263
21.712868	1028.084274	15.185280
21.852909	1030.020123	15.190298
22.306275	1047.615734	15.195315
22.314421	1044.370065	15.200333
22.381764	1026.682044	15.205351
22.059802	1030.337247	15.210368
22.028713	1018.623586	15.215386
21.960983	1022.889028	15.220403
21.748720	1029.005897	15.225421
22.254222	1043.493770	15.230439
22.239022	1055.533714	15.235456
22.459084	1051.969498	15.240474
22.420247	1042.748748	15.245491
22.117437	1028.225451	15.250509
22.379635	1022.038612	15.255527
22.240099	1032.431471	15.260544
22.314644	1026.788677	15.265562
22.412170	1029.689404	15.270579
22.308605	1027.348818	15.275597
22.480641	1035.013020	15.280615
22.542043	1045.139158	15.285632
22.467239	1032.700862	15.290650
22.223966	1031.597539	15.295667
22.738450	1037.261407	15.300685
22.518523	1032.669303	15.305703
22.369973	1028.978341	15.310720
22.555631	1030.990098	15.315738
22.868851	1037.414037	15.320755
22.611236	1030.299526	15.325773
22.715128	1018.454070	15.330791
22.558610	1015.676207	15.335808
22.594658	1016.708442	15.340826
22.115235	1021.394797	15.345843
22.491134	1039.665012	15.350861
22.756939	1046.187355	15.355879
22.732765	1055.563131	15.360896
23.120813	1045.543766	15.365914
23.029636	1048.028908	15.370931
22.738512	1050.233785	15.375949
22.960644	1050.867899	15.380967
22.796251	1049.500340	15.385984
22.863776	1046.840487	15.391002
22.840111	1048.431017	15.396019
23.040878	1057.203819	15.401037
23.134637	1046.680840	15.406055
22.955160	1047.442082	15.411072
22.677379	1044.098094	15.416090
22.877810	1044.451166	15.421107
22.248803	1043.973504	15.426125
22.329240	1042.156366	15.431143
22.624866	1055.149923	15.436160
22.914148	1065.959577	15.441178
23.067323	1068.084194	15.446195
22.940662	1075.548671	15.451213
23.077175	1075.497774	15.456231
23.161678	1077.405031	15.461248
23.230047	1071.873476	15.466266
23.236236	1071.912660	15.471283
23.061045	1074.787690	15.476301
23.421280	1062.908809	15.481319
23.663419	1068.942183	15.486336
23.358149	1065.476762	15.491354
23.517146	1060.374677	15.496371
23.585203	1065.520372	15.501389
23.764247	1062.248369	15.506407
23.601270	1068.299220	15.511424
23.292601	1057.230292	15.516442
23.527434	1043.723035	15.521459
23.444539	1056.297398	15.526477
23.508974	1047.161510	15.531495
23.470866	1044.487653	15.536512
23.928442	1052.523071	15.541530
23.513725	1035.370358	15.546547
23.231940	1042.874285	15.551565
23.668419	1042.696556	15.556583
23.665324	1052.657401	15.561600
23.590903	1063.234373	15.566618
23.112344	1060.867690	15.571635
23.322156	1071.560196	15.576653
23.337995	1057.296695	15.581671
23.485532	1066.370826	15.586688
23.798914	1062.030158	15.591706
23.816987	1055.860896	15.596723
23.606409	1066.755288	15.601741
23.673887	1054.602459	15.606759
24.080108	1069.663077	15.611776
23.855915	1066.111398	15.616794
24.096646	1059.611969	15.621811
23.539421	1061.965630	15.626829
23.791217	1066.121484	15.631847
23.645284	1061.333268	15.636864
23.669833	1077.874760	15.641882
24.377013	1081.422949	15.646899
24.080412	1089.052575	15.651917
24.555106	1080.400685	15.656935
24.289384	1081.419903	15.661952
23.899768	1072.149742	15.666970
24.271359	1070.807994	15.671987
23.804340	1065.302497	15.677005
24.065534	1069.248535	15.682023
24.279731	1081.589479	15.687040
24.485714	1084.375411	15.692058
24.644219	1076.193582	15.697075
24.281143	1074.856952	15.702093
23.872149	1065.294345	15.707111
24.313013	1072.824684	15.712128
24.283123	1076.511060	15.717146
24.642511	1077.079142	15.722163
24.142701	1088.732048	15.727181
24.466387	1079.622502	15.732199
24.234644	1083.684024	15.737216
24.138821	1089.061186	15.742234
24.330288	1073.027309	15.747251
24.172887	1089.122186	15.752269
24.243569	1086.144096	15.757287
24.700709	1086.551903	15.762304
24.748323	1088.235356	15.767322
24.618787	1085.067593	15.772339
24.541334	1090.353528	15.777357
24.693841	1076.912234	15.782375
24.897244	1081.056027	15.787392
24.518024	1072.930170	15.792410
24.888915	1074.246322	15.797427
24.719309	1083.960359	15.802445
24.522356	1073.572111	15.807463
24.158900	1078.231799	15.812480
24.488350	1092.911858	15.817498
25.031550	1105.138897	15.822515
25.019109	1105.663434	15.827533
25.471266	1105.973251	15.832551
25.170814	1093.288814	15.837568
25.012153	1075.898388	15.842586
24.877821	1069.475231	15.847603
24.986449	1071.181649	15.852621
25.253060	1062.459110	15.857639
25.107301	1073.349073	15.862656
25.057656	1074.762811	15.867674
25.068705	1062.974426	15.872691
24.698546	1069.498150	15.877709
25.017308	1064.343626	15.882727
25.394359	1071.951065	15.887744
25.139159	1069.142291	15.892762
25.386213	1060.080090	15.897779
24.814866	1064.693099	15.902797
25.078374	1067.048650	15.907815
25.202730	1079.999725	15.912832
25.219674	1092.440267	15.917850
25.421155	1095.352532	15.922867
25.550611	1102.170696	15.927885
25.282301	1095.950022	15.932903
25.557429	1095.368315	15.937920
25.644384	1091.332053	15.942938
25.450147	1081.927569	15.947955
25.545727	1077.895393	15.952973
25.258139	1070.272851	15.957991
25.437802	1081.372705	15.963008
25.370476	1095.227944	15.968026
25.536954	1094.099680	15.973043
25.606686	1095.112563	15.978061
25.713172	1091.456912	15.983079
25.875138	1090.469548	15.988096
25.626014	1097.585821	15.993114
25.651933	1089.094455	15.998131
25.319976	1092.259217	16.003149
25.685031	1085.201019	16.008167
25.286987	1094.752895	16.013184
25.513312	1097.011068	16.018202
25.761176	1089.591577	16.023219
25.495352	1096.820454	16.028237
25.262766	1086.851470	16.033255
25.657545	1108.732303	16.038272
25.815081	1121.152344	16.043290
26.009745	1111.118897	16.048307
26.078260	1119.077438	16.053325
26.270522	1116.510301	16.058343
26.527408	1119.017740	16.063360
26.131245	1109.137242	16.068378
26.073513	1103.353730	16.073395
25.882881	1095.501348	16.078413
26.155772	1100.224960	16.083431
26.527715	1121.952512	16.088448
26.134936	1103.435896	16.093466
26.501287	1085.807348	16.098483
26.220260	1090.560868	16.103501
26.109393	1089.078541	16.108519
26.183819	1082.023981	16.113536
25.974592	1086.084138	16.118554
26.206222	1100.074125	16.123571
26.238333	1121.102852	16.128589
26.386889	1115.882010	16.133607
26.525172	1111.559298	16.138624
26.324327	1120.775003	16.143642
26.373416	1113.209286	16.148659
26.614579	1111.161202	16.153677
26.527953	1105.473415	16.158695
26.446022	1115.947339	16.163712
26.405470	1122.396430	16.168730
26.387223	1122.471550	16.173747
26.610751	1124.506182	16.178765
26.926384	1117.400643	16.183783
26.800268	1112.555587	16.188800
26.517487	1111.038733	16.193818
26.829705	1107.513969	16.198835
26.939623	1118.428160	16.203853
26.821470	1114.271528	16.208871
26.625017	1109.817636	16.213888
26.757127	1116.122783	16.218906
26.852353	1109.121852	16.223923
27.115405	1109.304326	16.228941
26.777250	1114.521236	16.233959
26.845491	1109.186533	16.238976
27.016840	1113.115571	16.243994
27.174670	1112.019051	16.249011
26.841476	1112.270726	16.254029
26.875846	1105.962529	16.259047
27.205703	1102.815541	16.264064
26.691673	1108.898553	16.269082
27.379840	1110.342876	16.274099
27.318748	1109.331030	16.279117
27.117466	1105.814523	16.284135
27.237239	1106.579759	16.289152
27.165319	1114.003695	16.294170
27.164099	1097.527303	16.299187
27.128693	1100.643750	16.304205
26.822526	1104.585715	16.309223
27.421843	1103.860173	16.314240
27.257162	1110.254225	16.319258
27.524029	1100.831644	16.324275
27.231761	1107.947586	16.329293
27.073687	1106.244734	16.334311
27.237917	1094.495919	16.339328
27.179493	1110.167356	16.344346
27.403820	1112.904587	16.349363
27.303878	1126.753051	16.354381
27.635653	1127.396966	16.359399
27.726351	1131.083859	16.364416
27.882746	1128.335262	16.369434
27.955869	1126.126817	16.374451
27.643476	1100.598680	16.379469
27.239014	1099.142919	16.384487
27.499030	1107.752795	16.389504
27.045431	1123.988877	16.394522
27.483662	1123.405358	16.399539
27.822084	1125.139084	16.404557
27.739943	1131.467117	16.409575
27.608212	1125.880883	16.414592
27.449807	1126.592972	16.419610
27.559284	1127.334717	16.424627
27.827665	1132.836622	16.429645
27.987959	1151.922570	16.434663
28.132028	1148.082736	16.439680
28.316264	1152.256887	16.444698
28.115650	1141.350709	16.449715
27.675460	1124.832411	16.454733
28.051345	1147.607740	16.459751
27.973662	1140.166542	16.464768
28.445899	1143.223742	16.469786
28.798735	1143.209465	16.474803
28.457794	1130.323440	16.479821
28.308116	1126.738937	16.484839
28.477192	1111.475239	16.489856
28.255024	1114.412777	16.494874
28.173246	1115.725938	16.499891
28.146786	1108.795942	16.504909
27.844333	1118.905608	16.509927
28.316285	1127.496543	16.514944
28.428953	1140.622433	16.519962
28.679699	1147.019757	16.524979
28.645634	1154.479963	16.529997
28.528326	1155.419100	16.535015
28.906303	1144.416722	16.540032
28.617726	1121.384534	16.545050
28.223104	1112.667523	16.550067
28.354119	1123.186111	16.555085
28.381525	1128.385800	16.560103
28.757712	1134.124572	16.565120
28.593873	1141.473586	16.570138
28.602898	1146.781441	16.575155
28.564691	1141.386402	16.580173
28.320986	1154.635879	16.585191
28.471651	1140.483044	16.590208
28.713212	1146.127580	16.595226
28.745627	1142.780630	16.600243
28.952210	1134.462467	16.605261
28.606430	1150.270893	16.610279
28.572264	1141.303241	16.615296
28.207444	1148.655618	16.620314
28.474205	1155.338474	16.625331
29.122097	1165.840400	16.630349
28.830036	1172.957519	16.635367
28.966600	1162.314384	16.640384
28.814403	1176.257369	16.645402
28.769415	1167.106459	16.650419
28.883926	1173.933428	16.655437
28.862450	1181.771080	16.660455
29.175393	1191.821413	16.665472
29.461062	1198.874376	16.670490
29.826653	1198.032417	16.675507
29.608529	1184.636259	16.680525
29.716492	1181.933467	16.685543
29.394093	1166.778259	16.690560
29.499395	1161.730307	16.695578
29.419323	1165.560836	16.700595
29.614652	1175.568824	16.705613
29.415664	1171.124782	16.710631
29.680441	1160.089957	16.715648
29.657510	1169.493942	16.720666
29.608025	1169.708483	16.725683
29.744455	1158.310669	16.730701
29.458168	1166.244522	16.735719
29.959478	1154.912668	16.740736
29.644257	1163.318620	16.745754
29.509733	1157.498985	16.750771
29.667061	1158.761928	16.755789
29.673465	1166.446535	16.760807
29.835233	1154.285495	16.765824
29.742432	1162.414860	16.770842
29.783360	1165.621040	16.775859
29.641691	1164.567810	16.780877
29.462491	1168.087203	16.785895
29.729148	1188.322482	16.790912
29.575863	1195.303642	16.795930
29.859547	1189.422621	16.800947
30.032200	1188.829534	16.805965
30.179869	1192.929832	16.810983
30.071920	1183.832643	16.816000
29.963532	1186.241526	16.821018
29.992367	1174.289091	16.826035
30.219816	1175.491213	16.831053
30.499478	1182.721143	16.836071
30.589505	1185.512515	16.841088
30.564020	1174.871402	16.846106
30.546683	1170.698061	16.851123
30.685592	1171.488871	16.856141
30.375671	1180.791175	16.861159
30.636917	1175.746135	16.866176
30.433855	1171.733071	16.871194
30.439510	1173.538045	16.876211
30.724193	1169.653268	16.881229
30.499975	1165.808271	16.886247
30.359280	1153.711487	16.891264
30.408234	1154.961667	16.896282
30.320456	1166.958598	16.901299
30.738350	1171.053909	16.906317
30.515455	1175.406895	16.911335
30.776900	1173.249148	16.916352
30.671270	1176.581169	16.921370
30.332472	1177.660916	16.926387
30.830503	1170.027133	16.931405
30.816730	1180.861460	16.936423
30.678740	1168.492570	16.941440
30.848271	1181.879545	16.946458
30.642015	1185.255395	16.951475
31.013021	1169.516877	16.956493
30.969884	1175.734928	16.961511
31.027842	1174.184088	16.966528
31.270403	1179.913508	16.971546
31.216447	1178.928821	16.976563
30.972669	1164.860174	16.981581
30.623826	1169.680064	16.986599
30.656748	1173.537159	16.991616
31.025034	1170.847562	16.996634
30.675981	1172.157347	17.001651
30.982781	1185.144047	17.006669
30.983399	1199.044426	17.011687
31.456097	1205.244003	17.016704
31.425259	1210.046682	17.021722
31.448095	1210.692938	17.026739
31.604014	1199.743825	17.031757
31.546791	1205.622103	17.036775
31.419442	1206.146774	17.041792
31.262837	1200.937063	17.046810
31.583424	1203.558375	17.051827
31.778966	1206.233069	17.056845
31.359576	1203.465629	17.061863
31.435853	1205.088051	17.066880
31.127597	1201.342391	17.071898
30.955975	1210.277727	17.076915
31.564950	1197.491829	17.081933
31.244093	1206.460928	17.086951
31.148653	1207.745257	17.091968
31.661635	1214.130683	17.096986
31.630674	1228.367411	17.102003
31.876737	1232.300644	17.107021
31.883505	1229.231538	17.112039
31.881114	1226.327331	17.117056
31.948136	1224.435623	17.122074
32.124776	1227.371712	17.127091
32.135980	1218.536262	17.132109
32.175877	1226.495268	17.137127
32.302130	1234.028964	17.142144
32.503418	1228.318260	17.147162
32.277387	1212.865561	17.152179
32.399128	1200.769772	17.157197
31.862331	1193.814401	17.162215
31.675529	1197.048453	17.167232
32.126438	1201.507587	17.172250
31.941010	1207.442921	17.177267
32.708698	1214.707015	17.182285
32.623157	1223.311971	17.187303
32.451387	1217.800442	17.192320
32.241371	1215.392416	17.197338
32.247352	1227.864803	17.202355
32.410268	1222.895871	17.207373
32.376871	1225.517534	17.212391
32.273597	1217.944712	17.217408
32.428363	1225.005977	17.222426
32.152073	1224.480533	17.227443
32.729638	1220.390165	17.232461
32.710128	1221.740661	17.237479
32.183926	1222.007761	17.242496
32.307997	1216.902747	17.247514
32.534694	1226.583141	17.252531
32.553044	1239.127503	17.257549
32.745728	1251.874105	17.262567
32.655495	1254.516208	17.267584
32.822509	1248.121424	17.272602
32.642205	1256.496818	17.277619
33.201102	1253.907532	17.282637
33.148426	1250.026629	17.287655
32.949115	1254.036369	17.292672
33.317163	1240.236023	17.297690
32.894852	1251.133714	17.302707
33.155334	1248.528882	17.307725
32.751669	1246.163546	17.312743
32.655264	1238.386431	17.317760
33.106549	1247.061956	17.322778
32.891385	1247.669671	17.327795
33.634185	1240.034694	17.332813
33.618108	1239.371677	17.337831
33.464620	1247.612708	17.342848
33.535135	1237.558792	17.347866
33.290841	1245.312901	17.352883
33.424647	1238.533865	17.357901
33.624573	1241.266499	17.362919
33.287148	1241.850365	17.367936
33.435238	1235.750445	17.372954
33.547529	1244.670679	17.377971
33.373968	1239.319671	17.382989
33.346865	1242.927280	17.388007
33.341672	1233.427623	17.393024
33.468238	1232.836260	17.398042
33.207124	1245.028879	17.403059
33.527311	1247.942384	17.408077
33.577279	1262.006298	17.413095
33.672992	1270.852522	17.418112
33.992538	1263.897053	17.423130
33.851964	1270.746224	17.428147
34.012904	1272.601086	17.433165
34.062129	1269.933988	17.438183
33.634219	1266.991967	17.443200
33.535795	1264.824899	17.448218
33.907819	1266.047183	17.453235
34.073756	1257.141603	17.458253
33.843917	1257.979303	17.463271
33.746426	1267.789385	17.468288
34.298472	1275.586449	17.473306
34.269871	1288.798454	17.478323
34.351241	1285.895721	17.483341
34.528677	1287.947849	17.488359
34.353598	1276.286575	17.493376
34.604862	1254.168324	17.498394
34.243970	1257.780814	17.503411
34.509028	1247.925776	17.508429
34.498134	1246.106807	17.513447
34.503638	1258.026554	17.518464
34.355575	1243.696322	17.523482
34.061863	1262.868213	17.528499
34.469752	1275.757937	17.533517
34.764544	1275.060766	17.538535
34.689284	1283.394767	17.543552
34.664517	1283.143021	17.548570
34.818807	1280.087272	17.553587
34.682727	1279.489005	17.558605
34.727087	1282.599367	17.563623
34.610338	1285.873805	17.568640
35.130967	1274.949681	17.573658
34.822330	1281.019221	17.578675
34.668885	1285.047358	17.583693
34.732193	1279.536251	17.588711
34.996981	1280.295988	17.593728
35.236848	1271.940745	17.598746
35.080905	1271.780403	17.603763
35.326604	1279.780554	17.608781
35.191344	1278.256972	17.613799
35.310993	1282.089498	17.618816
35.325320	1271.393303	17.623834
34.893726	1285.827522	17.628851
35.272616	1270.911595	17.633869
35.735250	1283.129283	17.638887
35.333218	1278.280650	17.643904
35.465654	1271.986068	17.648922
35.491632	1279.031676	17.653939
35.224233	1275.870953	17.658957
35.382319	1274.716900	17.663975
35.076442	1273.733371	17.668992
35.412369	1269.385370	17.674010
35.521017	1283.826981	17.679027
35.325009	1284.103973	17.684045
35.137210	1272.581420	17.689063
34.897273	1273.729841	17.694080
35.079107	1280.279967	17.699098
35.425772	1285.172126	17.704115
35.380291	1299.405813	17.709133
35.490535	1301.543871	17.714151
35.378971	1300.469898	17.719168
35.569769	1302.686348	17.724186
35.728953	1315.812165	17.729203
35.989521	1326.795259	17.734221
36.228825	1319.294400	17.739239
36.056803	1335.205343	17.744256
36.584107	1329.161097	17.749274
36.673661	1316.731184	17.754291
36.067448	1304.598373	17.759309
35.917246	1289.679487	17.764327
35.755591	1300.405708	17.769344
36.457426	1303.837910	17.774362
36.066304	1307.327859	17.779379
36.359132	1318.540246	17.784397
36.176799	1322.648765	17.789415
36.255958	1334.578422	17.794432
36.641160	1321.902309	17.799450
36.939095	1323.144740	17.804467
36.908354	1321.740459	17.809485
36.500380	1297.830156	17.814503
36.246241	1296.896718	17.819520
36.585301	1298.328003	17.824538
36.525055	1313.886564	17.829555
36.584817	1311.836207	17.834573
37.040677	1314.234750	17.839591
36.739192	1330.826955	17.844608
36.758500	1318.323240	17.849626
36.586360	1320.700574	17.854643
36.632513	1321.094159	17.859661
37.082574	1312.189533	17.864679
36.828149	1323.486240	17.869696
37.158544	1321.467841	17.874714
37.095860	1321.268435	17.879731
36.610310	1321.782343	17.884749
36.858115	1324.362972	17.889767
36.655807	1318.237970	17.894784
36.737789	1328.121521	17.899802
36.812238	1320.720792	17.904819
37.156601	1324.004319	17.909837
37.032492	1322.802502	17.914855
37.176414	1329.401446	17.919872
37.293365	1340.829976	17.924890
37.451581	1341.714053	17.929907
37.046597	1356.638805	17.934925
37.425645	1345.316822	17.939943
37.364210	1351.196641	17.944960
37.534559	1348.366956	17.949978
37.524301	1350.685207	17.954995
37.453541	1344.227395	17.960013
37.653342	1341.735743	17.965031
37.665654	1347.166742	17.970048
37.912606	1338.922886	17.975066
37.729507	1340.683545	17.980083
37.745577	1346.797768	17.985101
37.753171	1337.693955	17.990119
37.815636	1331.868407	17.995136
38.048741	1340.142324	18.000154
37.753013	1335.891415	18.005171
37.622061	1334.534434	18.010189
37.714717	1332.710121	18.015207
37.461715	1336.429564	18.020224
37.815736	1339.431184	18.025242
37.575440	1341.118244	18.030259
38.013648	1337.102102	18.035277
38.255941	1343.252880	18.040295
38.039589	1360.955413	18.045312
38.320649	1362.579769	18.050330
38.330390	1364.252201	18.055347
38.395690	1371.989361	18.060365
38.533886	1355.695512	18.065383
38.370356	1354.590770	18.070400
38.509758	1348.904837	18.075418
38.371828	1346.003366	18.080435
38.440201	1365.028421	18.085453
38.468805	1354.064848	18.090471
38.449676	1364.086028	18.095488
38.794526	1366.955316	18.100506
38.894069	1355.335123	18.105523
38.543343	1362.026221	18.110541
38.718725	1356.674873	18.115559
38.469317	1366.744421	18.120576
38.321164	1364.024952	18.125594
38.399452	1364.837227	18.130611
38.793816	1367.624695	18.135629
38.910338	1365.355094	18.140647
38.997028	1364.599859	18.145664
38.404946	1353.046944	18.150682
38.981484	1356.921158	18.155699
39.059110	1382.016659	18.160717
39.356722	1367.812120	18.165735
38.995418	1364.061030	18.170752
38.990438	1372.094863	18.175770
39.117781	1361.084621	18.180787
39.341947	1376.846148	18.185805
39.219110	1375.947262	18.190823
39.447287	1378.296509	18.195840
39.356187	1379.695879	18.200858
39.508860	1378.138391	18.205875
39.270764	1374.575162	18.210893
39.360864	1366.421831	18.215911
39.481574	1383.637088	18.220928
39.435420	1378.480681	18.225946
39.688012	1375.407850	18.230963
39.363245	1381.030499	18.235981
39.677803	1373.038814	18.240999
39.696225	1374.952326	18.246016
39.901474	1371.225926	18.251034
39.491549	1369.710807	18.256051
39.414916	1376.613610	18.261069
39.620497	1375.571369	18.266087
39.720677	1380.207133	18.271104
39.742360	1369.208868	18.276122
40.015083	1381.235642	18.281139
40.174516	1391.759944	18.286157
39.856673	1382.425348	18.291175
39.769037	1390.055953	18.296192
40.103512	1396.212355	18.301210
40.192129	1393.175727	18.306227
40.007503	1402.666468	18.311245
40.381398	1395.017699	18.316263
40.035611	1397.408443	18.321280
40.149852	1395.727396	18.326298
40.746194	1399.262126	18.331315
40.465236	1400.687030	18.336333
40.347862	1393.423539	18.341351
40.774251	1398.396627	18.346368
40.229575	1389.944064	18.351386
40.563463	1389.658914	18.356403
40.526121	1395.066656	18.361421
40.226467	1385.595584	18.366439
40.766565	1382.190504	18.371456
40.558814	1393.554335	18.376474
40.509946	1392.508950	18.381491
40.251918	1391.400562	18.386509
40.658957	1412.617209	18.391527
40.752411	1416.602136	18.396544
40.925188	1417.432232	18.401562
41.164479	1420.166649	18.406579
40.887590	1422.441265	18.411597
40.963738	1410.873722	18.416615
41.341149	1408.103835	18.421632
41.221268	1413.885089	18.426650
41.165354	1407.251171	18.431667
41.086791	1410.381519	18.436685
41.217636	1416.389365	18.441703
41.376177	1411.684874	18.446720
41.387437	1413.288557	18.451738
41.742707	1404.844450	18.456755
41.352954	1415.491198	18.461773
41.637753	1411.456739	18.466791
41.780619	1412.645327	18.471808
41.432716	1407.715250	18.476826
41.702481	1408.921801	18.481843
41.477420	1404.736730	18.486861
41.535344	1406.750396	18.491879
41.842619	1405.016520	18.496896
41.536011	1408.629898	18.501914
41.762340	1406.131088	18.506931
41.453899	1409.971932	18.511949
41.762129	1396.585677	18.516967
41.852818	1401.891515	18.521984
41.681740	1405.202532	18.527002
41.669404	1410.989205	18.532019
41.787384	1424.052253	18.537037
41.993267	1432.761431	18.542055
42.315434	1433.658131	18.547072
41.877570	1435.243269	18.552090
42.224325	1436.831165	18.557107
42.039073	1440.570517	18.562125
41.974824	1442.740243	18.567143
42.189420	1432.507228	18.572160
42.251064	1440.046605	18.577178
42.426723	1437.469566	18.582195
42.521202	1430.974514	18.587213
42.571362	1430.720201	18.592231
42.352265	1435.674199	18.597248
42.348097	1443.115814	18.602266
42.512649	1440.784706	18.607283
42.245678	1433.768799	18.612301
42.643548	1442.736742	18.617319
43.011648	1450.573015	18.622336
42.766692	1455.162800	18.627354
42.783623	1434.143714	18.632371
42.711170	1436.943138	18.637389
42.430999	1452.160304	18.642407
42.766628	1446.371372	18.647424
42.651829	1454.655713	18.652442
43.219766	1457.554221	18.657459
43.212921	1460.441209	18.662477
43.362614	1449.693343	18.667495
43.399666	1451.441970	18.672512
43.133184	1459.627414	18.677530
43.393843	1450.081636	18.682547
43.224188	1455.697919	18.687565
43.203140	1455.551066	18.692583
43.540161	1448.931201	18.697600
43.361347	1452.800198	18.702618
43.503443	1456.751884	18.707635
43.534289	1451.002393	18.712653
43.565945	1454.550323	18.717671
43.587538	1449.108661	18.722688
43.476176	1456.649133	18.727706
43.957623	1442.630620	18.732723
43.829693	1443.703815	18.737741
43.595676	1443.835529	18.742759
43.892273	1442.659711	18.747776
43.316154	1445.798436	18.752794
43.625721	1441.871678	18.757811
43.695943	1440.560904	18.762829
43.790652	1442.009041	18.767847
43.841984	1440.299037	18.772864
43.578648	1459.023624	18.777882
44.195749	1460.461249	18.782899
43.969437	1472.198286	18.787917
44.130597	1478.516489	18.792935
44.431896	1475.320220	18.797952
44.364202	1476.967690	18.802970
44.382939	1467.243850	18.807987
44.532605	1466.423459	18.813005
44.258414	1467.472448	18.818023
44.414708	1465.539158	18.823040
44.163789	1467.680347	18.828058
44.544420	1467.378008	18.833075
44.727792	1465.873301	18.838093
44.556496	1465.683609	18.843111
44.877075	1459.107407	18.848128
44.780472	1458.953379	18.853146
44.622700	1461.552369	18.858163
44.547227	1460.953507	18.863181
44.501149	1467.478459	18.868199
44.487720	1467.266958	18.873216
44.492418	1473.711065	18.878234
44.910571	1482.251266	18.883251
44.864292	1492.268757	18.888269
44.850979	1494.113523	18.893287
45.436627	1485.176506	18.898304
44.794433	1491.476159	18.903322
45.457760	1485.385711	18.908339
45.501078	1484.975838	18.913357
45.118490	1487.941977	18.918375
45.343566	1478.420577	18.923392
45.298521	1486.886690	18.928410
45.509208	1474.931077	18.933427
45.597448	1481.080254	18.938445
45.209786	1483.761801	18.943463
45.320701	1477.877389	18.948480
45.177278	1485.520034	18.953498
45.307024	1486.821036	18.958515
45.303573	1489.667311	18.963533
45.515341	1509.877062	18.968551
45.977847	1507.024958	18.973568
45.750762	1518.653104	18.978586
45.969754	1508.464980	18.983603
46.072992	1515.169164	18.988621
46.201774	1507.727460	18.993639
46.340653	1494.551839	18.998656
45.842745	1486.326516	19.003674
45.926005	1478.016779	19.008691
46.085643	1490.152520	19.013709
45.854736	1505.021031	19.018727
46.231851	1516.429055	19.023744
46.216219	1512.220694	19.028762
46.379068	1510.562295	19.033779
46.107015	1506.135372	19.038797
46.154032	1511.921310	19.043815
46.289144	1500.945508	19.048832
46.077640	1506.187246	19.053850
46.424829	1503.303844	19.058867
46.541341	1495.956302	19.063885
46.471587	1502.637157	19.068903
46.378197	1496.337357	19.073920
46.252002	1508.809809	19.078938
46.680705	1516.040809	19.083955
46.661890	1522.714025	19.088973
46.717270	1526.670640	19.093991
46.728766	1520.265274	19.099008
46.571316	1531.301981	19.104026
46.496224	1531.401476	19.109043
47.026130	1533.582283	19.114061
47.175519	1529.039902	19.119079
47.306232	1522.498655	19.124096
47.082437	1526.908186	19.129114
47.217661	1527.563011	19.134131
47.508268	1541.533005	19.139149
47.290479	1543.218721	19.144167
47.582711	1527.938158	19.149184
47.307103	1523.472055	19.154202
47.461324	1525.002471	19.159219
47.652391	1530.021654	19.164237
47.255334	1547.568888	19.169255
47.674315	1543.701941	19.174272
47.447285	1547.909652	19.179290
47.356591	1537.524362	19.184307
47.740702	1536.743494	19.189325
47.838884	1538.992637	19.194343
48.220626	1526.814174	19.199360
48.301888	1527.912184	19.204378
47.834763	1532.032481	19.209395
48.021788	1533.927150	19.214413
47.527917	1539.349117	19.219431
48.198195	1526.569337	19.224448
48.220142	1532.073214	19.229466
48.437438	1528.604625	19.234483
48.261715	1532.564467	19.239501
48.143820	1534.054115	19.244519
48.435838	1534.726680	19.249536
48.464360	1538.559398	19.254554
48.400778	1539.075883	19.259571
48.584912	1534.829321	19.264589
48.300437	1540.924882	19.269607
48.340496	1532.380931	19.274624
48.351269	1537.274852	19.279642
48.552435	1539.750249	19.284659
48.396525	1534.419838	19.289677
48.537565	1534.874095	19.294695
48.455206	1535.140934	19.299712
48.551767	1547.818659	19.304730
48.511309	1563.685610	19.309747
49.153703	1557.761592	19.314765
48.474542	1562.648106	19.319783
48.740517	1565.468681	19.324800
49.124244	1569.738262	19.329818
49.286277	1565.813461	19.334835
49.149121	1570.016533	19.339853
48.890119	1560.796101	19.344871
48.988745	1555.038498	19.349888
48.765967	1562.366762	19.354906
48.954385	1577.779296	19.359923
49.298744	1577.599890	19.364941
49.140529	1590.429284	19.369959
49.206176	1589.038153	19.374976
49.309623	1590.963991	19.379994
49.903391	1586.648407	19.385011
49.707779	1580.560380	19.390029
49.621912	1589.646695	19.395047
50.053809	1577.381935	19.400064
49.803354	1585.505342	19.405082
49.822588	1584.276227	19.410099
50.089134	1571.884126	19.415117
50.138300	1581.113825	19.420135
50.329824	1578.747128	19.425152
50.065332	1575.290979	19.430170
49.953489	1578.132777	19.435187
50.162101	1569.647117	19.440205
50.237438	1575.578784	19.445223
50.459490	1577.664115	19.450240
50.235335	1582.293406	19.455258
50.220710	1595.053753	19.460275
50.299026	1583.077849	19.465293
50.208216	1586.259866	19.470311
50.003113	1579.243884	19.475328
50.232014	1590.405244	19.480346
50.380311	1596.769720	19.485363
50.854324	1594.999160	19.490381
50.784140	1604.241942	19.495399
50.977470	1602.330849	19.500416
50.858162	1605.956959	19.505434
50.653942	1609.082168	19.510451
51.101550	1598.848651	19.515469
50.621126	1605.567233	19.520487
50.488593	1595.109697	19.525504
50.528198	1600.329179	19.530522
50.815748	1600.441463	19.535539
51.193243	1613.205008	19.540557
50.911090	1629.808898	19.545575
51.060292	1628.105503	19.550592
51.646088	1624.716034	19.555610
51.330996	1634.141511	19.560627
51.392884	1626.965945	19.565645
51.355452	1637.289546	19.570663
51.456843	1638.824784	19.575680
51.534363	1632.839938	19.580698
51.621221	1631.838205	19.585715
51.797998	1628.538902	19.590733
51.617984	1631.342784	19.595751
51.945685	1629.621250	19.600768
51.818687	1620.343493	19.605786
51.518869	1622.890045	19.610803
51.927738	1622.880273	19.615821
52.032989	1624.945974	19.620839
52.057748	1619.812784	19.625856
52.008098	1613.887190	19.630874
52.151924	1619.055563	19.635891
52.152833	1606.047968	19.640909
52.027412	1622.763301	19.645927
51.882619	1617.486926	19.650944
52.307189	1616.331639	19.655962
52.262819	1620.265030	19.660979
52.264132	1616.212890	19.665997
52.266562	1616.846007	19.671015
52.492794	1639.710230	19.676032
52.368437	1645.883257	19.681050
52.237715	1647.349054	19.686067
52.594608	1646.684894	19.691085
52.584772	1649.639736	19.696103
52.295748	1648.266774	19.701120
52.695255	1647.775480	19.706138
52.347314	1646.376446	19.711155
52.623562	1647.673284	19.716173
52.824808	1671.083425	19.721191
52.869936	1674.949648	19.726208
53.245255	1678.261198	19.731226
52.882617	1678.079956	19.736243
53.399780	1673.130966	19.741261
53.466802	1676.991990	19.746279
53.443765	1671.245434	19.751296
53.466815	1668.381420	19.756314
53.238739	1682.772859	19.761331
53.344390	1666.693522	19.766349
53.442977	1674.712332	19.771367
53.313759	1665.925468	19.776384
53.606590	1668.569175	19.781402
53.562475	1669.564333	19.786419
53.728274	1661.214847	19.791437
53.511434	1664.641371	19.796455
53.514861	1659.936898	19.801472
53.886848	1667.022636	19.806490
53.543140	1674.194990	19.811507
53.898968	1676.105035	19.816525
54.110918	1682.660976	19.821543
54.178419	1686.116409	19.826560
54.176840	1686.446253	19.831578
54.053739	1684.336362	19.836595
54.114023	1677.679151	19.841613
54.250274	1676.148762	19.846631
54.498072	1666.021907	19.851648
54.632755	1666.550057	19.856666
54.411532	1676.614744	19.861683
54.430786	1665.789506	19.866701
54.659727	1673.391848	19.871719
54.533425	1667.201366	19.876736
54.562388	1665.584411	19.881754
54.323438	1675.081951	19.886771
54.896934	1670.253163	19.891789
54.710536	1665.821853	19.896807
54.675161	1671.434879	19.901824
54.658187	1682.652765	19.906842
54.808800	1693.805902	19.911859
54.904157	1703.530785	19.916877
54.927976	1696.312277	19.921895
55.034404	1704.252245	19.926912
54.930105	1698.209682	19.931930
54.790327	1702.232908	19.936947
55.115928	1703.065276	19.941965
55.173551	1708.093227	19.946983
55.478457	1720.190922	19.952000
56.087865	1709.751801	19.957018
56.148285	1721.385644	19.962035
56.133391	1702.343133	19.967053
55.870409	1687.974036	19.972071
55.502229	1688.210249	19.977088
55.651381	1687.863951	19.982106
55.325963	1703.676653	19.987123
55.739843	1692.580149	19.992141
55.828803	1686.802444	19.997159
55.846290	1694.601227	20.002176
56.291533	1702.959900	20.007194
55.952422	1703.160198	20.012211
55.929264	1708.757434	20.017229
56.167450	1717.663789	20.022247
56.329087	1713.390588	20.027264
56.399958	1713.974581	20.032282
56.308109	1721.914710	20.037299
56.191214	1719.011260	20.042317
56.561474	1722.982324	20.047335
56.036093	1721.572899	20.052352
56.508046	1713.381356	20.057370
56.506546	1713.272208	20.062387
56.511186	1716.297501	20.067405
56.349332	1722.831494	20.072423
56.235045	1715.975611	20.077440
56.848322	1732.208118	20.082458
56.752136	1742.573407	20.087475
56.827450	1740.890502	20.092493
56.820111	1745.163466	20.097511
56.719533	1746.238451	20.102528
56.880674	1733.469181	20.107546
57.087595	1742.230332	20.112563
57.479787	1741.356778	20.117581
57.082943	1743.876894	20.122599
57.293209	1754.903269	20.127616
57.895822	1761.785508	20.132634
57.514423	1760.356964	20.137651
57.483335	1750.223081	20.142669
57.906217	1759.300849	20.147687
57.612748	1754.445111	20.152704
57.856308	1757.125338	20.157722
57.915422	1770.100393	20.162739
57.967488	1758.992883	20.167757
58.063751	1750.445806	20.172775
57.782598	1749.251847	20.177792
57.547101	1744.262497	20.182810
57.776664	1756.988450	20.187827
58.356897	1759.829864	20.192845
58.394229	1752.550037	20.197863
58.086905	1760.072709	20.202880
58.200647	1754.063708	20.207898
58.165593	1759.827107	20.212915
57.948834	1751.320440	20.217933
58.451128	1746.597515	20.222951
58.141037	1764.373903	20.227968
58.550283	1758.395106	20.232986
58.508163	1783.474864	20.238003
58.590475	1785.540842	20.243021
58.579113	1783.789999	20.248039
58.652747	1788.799577	20.253056
58.858109	1782.063969	20.258074
58.752374	1790.632030	20.263091
58.880550	1785.716311	20.268109
59.123465	1780.128043	20.273127
58.880716	1776.236353	20.278144
58.947783	1777.800517	20.283162
58.952792	1777.396981	20.288179
59.358844	1789.655938	20.293197
59.701339	1796.477719	20.298215
59.518026	1788.321010	20.303232
59.599284	1776.675970	20.308250
59.561730	1764.221074	20.313267
59.735848	1775.805030	20.318285
59.833983	1766.336363	20.323303
59.146456	1772.034570	20.328320
59.544645	1766.546583	20.333338
59.383794	1786.227835	20.338355
59.560208	1790.188099	20.343373
59.704403	1796.721055	20.348391
59.926220	1790.569735	20.353408
60.233216	1790.585099	20.358426
60.094512	1792.654602	20.363443
59.976710	1797.499421	20.368461
60.345443	1795.185241	20.373479
59.938415	1797.497207	20.378496
60.405684	1792.272580	20.383514
60.366440	1791.945269	20.388531
60.178409	1793.167809	20.393549
60.460021	1789.546779	20.398567
60.472207	1796.127971	20.403584
60.374317	1809.072755	20.408602
60.765068	1816.455066	20.413619
60.750482	1817.674875	20.418637
61.055777	1810.064034	20.423655
61.078949	1815.628441	20.428672
61.251129	1811.015668	20.433690
61.017079	1813.393878	20.438707
61.237538	1818.871681	20.443725
61.242817	1813.914096	20.448743
60.920913	1813.860754	20.453760
61.135775	1810.914560	20.458778
61.278833	1813.431514	20.463795
61.161253	1809.008060	20.468813
61.194027	1805.445550	20.473831
61.108629	1810.306662	20.478848
61.402030	1807.003365	20.483866
61.295544	1803.630452	20.488883
61.028047	1816.819863	20.493901
61.436316	1829.873773	20.498919
61.543019	1831.662486	20.503936
61.767320	1829.406469	20.508954
61.486945	1836.910936	20.513971
61.526602	1842.054899	20.518989
61.766236	1835.384067	20.524007
61.960241	1859.896498	20.529024
62.314385	1851.627144	20.534042
62.212141	1860.005292	20.539059
62.208108	1862.778109	20.544077
62.472033	1857.574925	20.549095
62.573181	1863.315417	20.554112
62.289263	1851.629602	20.559130
62.453560	1867.575562	20.564147
62.492190	1859.604906	20.569165
62.906404	1850.898828	20.574183
62.702824	1864.832828	20.579200
62.984140	1861.028362	20.584218
63.076383	1850.920057	20.589235
62.596547	1859.567028	20.594253
63.222164	1847.569593	20.599271
62.983131	1850.476988	20.604288
62.748491	1849.918638	20.609306
63.052600	1847.936810	20.614323
62.819185	1849.030254	20.619341
63.030213	1844.563010	20.624359
63.155286	1862.850931	20.629376
63.142708	1875.698966	20.634394
63.365433	1870.412440	20.639411
63.282163	1886.397836	20.644429
63.408420	1886.308873	20.649447
63.332294	1891.790534	20.654464
63.485965	1885.245333	20.659482
63.649757	1881.227640	20.664499
63.382944	1876.152092	20.669517
63.794959	1888.003834	20.674535
63.844838	1891.056711	20.679552
63.922371	1909.935248	20.684570
64.409584	1909.273123	20.689587
63.910786	1907.415568	20.694605
64.405078	1900.811600	20.699623
64.392905	1905.391714	20.704640
64.474998	1895.993736	20.709658
64.951486	1896.114111	20.714675
64.714656	1887.707151	20.719693
64.495339	1872.699537	20.724711
64.724017	1865.410809	20.729728
64.538106	1859.587212	20.734746
64.691954	1868.086351	20.739763
64.616604	1887.380733	20.744781
64.966601	1883.012124	20.749799
64.656522	1888.791186	20.754816
64.630948	1893.583362	20.759834
65.370699	1891.256558	20.764851
65.413445	1900.333964	20.769869
65.565678	1890.390113	20.774887
65.179728	1893.597438	20.779904
65.275170	1886.139813	20.784922
65.351714	1886.266172	20.789939
65.301181	1891.080590	20.794957
65.484213	1893.473613	20.799975
65.450571	1890.557526	20.804992
65.325548	1896.927617	20.810010
65.403858	1880.027373	20.815027
65.267122	1892.344788	20.820045
65.811689	1903.656475	20.825063
65.481471	1911.882631	20.830080
65.554823	1929.602805	20.835098
65.982848	1913.376526	20.840115
65.583406	1916.295139	20.845133
65.676551	1916.144334	20.850151
65.495315	1924.125351	20.855168
66.032837	1939.097758	20.860186
66.198491	1942.627156	20.865203
66.420897	1953.297324	20.870221
66.669703	1945.497735	20.875239
66.425239	1943.868148	20.880256
66.602369	1946.436177	20.885274
66.692300	1945.416199	20.890291
66.359623	1945.723309	20.895309
66.862402	1941.100642	20.900327
66.726708	1938.282154	20.905344
66.572029	1945.094192	20.910362
66.779212	1956.984234	20.915379
66.590895	1969.792152	20.920397
67.167663	1966.447809	20.925415
66.967768	1976.545380	20.930432
66.915133	1967.799996	20.935450
67.258018	1964.966438	20.940467
67.061580	1965.518714	20.945485
67.279341	1980.040944	20.950503
67.653127	1991.304198	20.955520
67.493080	1995.243845	20.960538
67.743484	1991.882667	20.965555
68.017644	1999.409964	20.970573
67.948952	1986.609249	20.975591
67.812769	1990.590614	20.980608
67.786949	1989.375619	20.985626
68.458187	1981.480477	20.990643
67.866170	1991.995354	20.995661
68.028388	1980.640307	21.000679
68.039292	1982.150404	21.005696
68.011697	1985.059825	21.010714
68.093667	1981.910794	21.015731
68.165783	1985.717901	21.020749
68.205692	1982.030938	21.025767
68.366736	1986.488298	21.030784
68.307108	1975.261722	21.035802
68.463315	1984.815286	21.040819
68.800875	2001.694926	21.045837
68.884018	1995.333802	21.050855
69.293288	1999.722901	21.055872
68.809566	1991.427237	21.060890
69.333810	1990.174711	21.065907
68.958248	2001.231329	21.070925
69.249994	1989.134338	21.075943
69.145488	1999.816539	21.080960
69.267999	1992.492180	21.085978
69.248725	1992.044232	21.090995
69.601130	1989.303978	21.096013
69.575938	1989.368834	21.101031
69.732195	1998.371202	21.106048
69.425176	1996.791338	21.111066
69.880994	1992.211472	21.116083
69.422320	2003.529891	21.121101
69.393219	1999.313785	21.126119
69.584750	1992.026031	21.131136
69.422328	2005.301750	21.136154
69.453817	2006.719069	21.141171
69.777303	2017.176870	21.146189
70.341729	2019.313845	21.151207
70.399415	2015.484951	21.156224
69.896287	2012.666656	21.161242
69.875333	2020.662917	21.166259
70.500876	2031.463246	21.171277
70.170961	2038.099215	21.176295
70.406139	2044.098299	21.181312
70.067682	2049.643923	21.186330
70.451436	2035.447743	21.191347
70.514529	2046.230969	21.196365
70.935021	2046.381092	21.201383
70.708829	2044.487438	21.206400
71.389710	2058.359816	21.211418
71.392523	2050.758783	21.216435
71.468607	2053.977437	21.221453
71.271862	2033.618920	21.226471
71.621059	2028.410616	21.231488
71.265625	2031.289285	21.236506
71.522638	2023.344200	21.241523
71.786973	2027.109254	21.246541
71.350578	2022.684587	21.251559
71.508694	2028.872807	21.256576
71.305731	2051.743741	21.261594
71.735630	2050.402892	21.266611
71.869894	2060.835752	21.271629
71.955249	2063.722154	21.276647
72.040982	2052.481691	21.281664
71.946069	2069.040479	21.286682
71.978556	2061.769578	21.291699
71.785153	2063.935970	21.296717
71.666551	2062.803657	21.301735
72.267245	2076.179076	21.306752
71.966401	2086.445012	21.311770
72.527061	2072.133284	21.316787
72.399413	2077.369596	21.321805
72.337928	2080.596860	21.326823
72.632278	2082.264372	21.331840
72.528815	2084.028068	21.336858
72.726260	2076.715280	21.341875
72.918852	2099.561736	21.346893
73.013037	2110.441044	21.351911
73.067590	2117.418520	21.356928
72.673961	2120.115333	21.361946
73.277594	2110.067075	21.366963
73.374127	2107.021910	21.371981
72.944617	2113.051545	21.376999
73.226835	2102.641928	21.382016
73.188676	2109.915076	21.387034
73.110728	2108.104352	21.392051
73.408245	2113.746280	21.397069
73.767230	2128.160224	21.402087
74.035700	2124.710197	21.407104
73.628308	2133.264611	21.412122
73.859970	2134.392490	21.417139
73.809161	2141.216156	21.422157
73.678353	2139.279531	21.427175
74.377052	2125.695320	21.432192
73.918757	2136.739746	21.437210
74.234007	2123.330446	21.442227
74.239206	2116.898317	21.447245
74.411098	2132.518085	21.452263
74.681363	2140.542177	21.457280
74.578973	2153.596658	21.462298
74.641639	2155.779329	21.467315
75.034435	2166.810422	21.472333
74.699974	2161.662118	21.477351
74.947637	2151.944041	21.482368
74.684075	2157.067051	21.487386
74.853249	2150.651461	21.492403
74.613992	2154.351891	21.497421
74.874745	2156.374988	21.502439
75.356504	2152.542777	21.507456
75.195239	2158.955197	21.512474
75.013815	2171.192039	21.517491
75.075265	2173.622954	21.522509
75.393156	2176.787424	21.527527
75.700176	2169.791895	21.532544
75.239616	2179.956772	21.537562
75.528688	2174.479231	21.542579
75.591621	2188.218205	21.547597
75.576583	2196.182474	21.552615
76.017332	2202.338929	21.557632
75.871955	2202.858742	21.562650
75.770379	2194.902073	21.567667
76.134454	2203.207527	21.572685
76.429190	2208.924363	21.577703
76.417326	2209.367343	21.582720
76.513654	2229.442811	21.587738
76.755592	2227.605488	21.592755
76.663292	2233.341925	21.597773
76.963453	2228.928321	21.602791
77.423185	2224.828469	21.607808
77.006894	2212.088270	21.612826
77.117005	2192.142931	21.617843
76.967321	2196.953780	21.622861
76.981124	2186.894466	21.627879
77.161249	2192.755868	21.632896
77.253822	2216.765952	21.637914
77.694639	2224.261829	21.642931
77.308405	2224.349455	21.647949
77.330726	2219.405455	21.652967
77.219790	2219.569945	21.657984
77.337091	2227.801700	21.663002
77.345672	2214.811223	21.668019
77.416812	2215.318416	21.673037
77.311877	2224.730712	21.678055
77.796256	2230.174808	21.683072
77.826872	2252.372296	21.688090
77.858240	2253.176639	21.693107
78.138545	2238.183589	21.698125
78.242709	2245.270237	21.703143
78.212819	2246.233154	21.708160
78.285112	2241.645848	21.713178
78.281992	2240.322741	21.718195
78.711801	2231.489455	21.723213
78.669654	2243.687939	21.728231
78.928304	2233.119532	21.733248
78.533942	2237.224024	21.738266
78.616782	2232.764115	21.743283
78.764893	2232.112847	21.748301
78.889194	2252.547508	21.753319
79.126805	2255.516223	21.758336
79.090864	2261.979197	21.763354
79.467493	2264.828828	21.768371
79.503878	2255.641754	21.773389
79.521033	2260.597841	21.778407
79.632675	2255.718177	21.783424
79.517515	2263.875837	21.788442
79.397386	2255.479276	21.793459
79.455915	2255.320814	21.798477
79.295681	2255.061558	21.803495
79.753029	2241.506184	21.808512
79.700904	2261.007822	21.813530
80.136773	2276.808054	21.818547
80.390247	2275.200716	21.823565
80.039139	2282.820655	21.828583
80.360662	2280.016958	21.833600
79.890173	2282.083581	21.838618
80.247041	2283.938806	21.843635
80.411237	2273.910050	21.848653
80.446354	2277.008362	21.853671
80.379613	2270.811319	21.858688
80.674136	2283.878935	21.863706
80.793403	2299.344192	21.868723
80.898385	2295.944820	21.873741
80.693022	2313.824577	21.878759
80.745181	2307.688939	21.883776
80.795043	2306.627932	21.888794
81.073450	2304.246349	21.893811
81.327675	2300.706906	21.898829
81.241869	2313.824920	21.903847
81.434606	2321.316642	21.908864
81.726891	2327.891842	21.913882
81.825809	2330.331146	21.918899
81.746156	2317.221722	21.923917
81.837375	2323.034504	21.928935
82.184317	2316.330740	21.933952
81.827247	2315.593813	21.938970
81.901177	2320.807855	21.943987
82.460691	2313.543674	21.949005
82.308110	2327.681464	21.954023
82.513446	2318.636859	21.959040
82.126349	2318.100582	21.964058
81.868696	2316.964107	21.969075
82.290623	2316.100563	21.974093
82.250862	2324.682406	21.979111
82.763388	2317.962642	21.984128
82.663965	2337.198572	21.989146
82.606585	2340.419698	21.994163
82.896906	2332.590207	21.999181
82.751344	2332.263951	22.004199
83.247524	2328.623414	22.009216
82.878385	2329.742117	22.014234
82.628913	2339.174476	22.019251
83.065405	2346.864839	22.024269
82.907407	2355.015072	22.029287
83.215891	2359.218590	22.034304
83.621448	2367.372770	22.039322
83.419503	2367.310979	22.044339
83.869233	2361.646135	22.049357
83.539682	2367.530963	22.054375
83.501580	2365.465568	22.059392
83.746752	2384.898058	22.064410
83.680036	2390.302348	22.069427
83.877972	2380.032885	22.074445
83.920732	2390.851215	22.079463
84.391856	2392.644621	22.084480
84.164597	2399.356269	22.089498
84.146006	2416.371712	22.094515
84.292229	2422.416383	22.099533
84.440974	2424.320652	22.104551
84.844997	2415.028122	22.109568
85.105064	2424.496253	22.114586
84.906797	2413.753363	22.119603
85.142069	2416.611860	22.124621
84.857883	2425.686613	22.129639
85.316974	2415.094740	22.134656
85.281219	2411.705258	22.139674
85.117493	2419.598585	22.144691
85.128085	2418.553128	22.149709
85.445159	2434.147981	22.154727
85.481513	2449.250322	22.159744
85.614344	2433.961012	22.164762
85.437161	2448.369928	22.169779
85.718762	2434.620639	22.174797
85.973202	2441.770689	22.179815
85.880157	2429.331928	22.184832
86.086287	2440.781153	22.189850
85.742306	2463.260267	22.194867
85.774924	2461.535926	22.199885
86.228674	2467.333229	22.204903
86.180380	2469.704010	22.209920
86.564498	2451.502837	22.214938
86.770647	2465.795542	22.219955
86.357446	2466.519558	22.224973
86.731800	2480.816319	22.229991
87.043841	2481.234813	22.235008
87.287583	2489.285527	22.240026
87.093632	2488.110143	22.245043
87.526831	2484.699303	22.250061
87.304299	2484.083801	22.255079
87.064320	2481.037978	22.260096
87.409012	2484.616602	22.265114
87.231764	2479.982743	22.270131
87.531471	2476.921584	22.275149
87.737112	2485.128219	22.280167
87.594312	2485.076715	22.285184
87.527263	2479.181625	22.290202
87.716631	2500.242096	22.295219
88.128074	2504.757760	22.300237
88.111421	2507.033145	22.305255
87.839955	2508.471141	22.310272
88.305054	2510.637234	22.315290
88.256274	2510.873330	22.320307
88.375108	2507.226329	22.325325
87.651698	2504.118014	22.330343
88.034477	2528.461655	22.335360
88.696399	2528.263920	22.340378
88.639668	2531.295596	22.345395
88.679640	2534.856964	22.350413
88.851724	2534.260775	22.355431
89.013500	2530.781865	22.360448
89.158529	2525.404040	22.365466
89.367229	2545.245550	22.370483
89.710003	2542.647750	22.375501
89.092865	2532.898989	22.380519
89.209055	2556.067053	22.385536
89.440953	2552.882060	22.390554
89.511999	2566.138893	22.395571
89.665475	2556.257803	22.400589
89.445936	2561.309871	22.405607
89.619851	2557.461600	22.410624
90.094754	2553.076065	22.415642
89.542312	2565.874282	22.420659
90.272943	2577.052503	22.425677
90.231886	2576.271903	22.430695
90.477806	2576.565513	22.435712
90.880727	2576.938647	22.440730
90.658196	2578.228774	22.445747
90.913310	2577.511348	22.450765
90.676959	2574.062912	22.455783
90.793800	2570.248499	22.460800
90.825360	2572.838372	22.465818
90.845245	2577.966954	22.470835
90.861876	2564.740979	22.475853
90.872248	2579.180384	22.480871
91.115782	2591.063713	22.485888
91.151999	2592.340136	22.490906
91.142058	2598.958798	22.495923
91.477337	2601.024343	22.500941
91.913383	2597.624426	22.505959
91.747439	2596.429435	22.510976
91.928645	2593.659546	22.515994
91.508544	2603.064799	22.521011
91.742093	2608.866329	22.526029
91.992193	2619.735140	22.531047
92.129040	2627.077985	22.536064
92.626790	2622.854801	22.541082
92.443742	2622.852482	22.546099
92.514647	2621.014690	22.551117
92.661993	2611.651937	22.556135
92.528195	2618.370647	22.561152
92.934651	2614.831128	22.566170
92.743910	2619.146903	22.571187
92.840207	2623.814000	22.576205
93.069384	2631.299445	22.581223
93.111016	2641.915367	22.586240
93.399581	2653.520403	22.591258
92.977663	2648.128523	22.596275
93.152465	2646.929083	22.601293
93.083166	2649.064770	22.606311
92.992272	2648.671577	22.611328
93.620762	2657.052011	22.616346
93.705401	2674.439647	22.621363
93.782820	2675.332851	22.626381
93.690629	2671.641217	22.631399
93.518376	2680.162115	22.636416
93.968582	2680.197085	22.641434
93.885050	2695.602999	22.646451
94.155092	2705.768125	22.651469
94.299493	2706.293129	22.656487
93.977863	2707.004748	22.661504
94.180489	2697.302453	22.666522
94.517366	2724.228987	22.671539
94.526791	2718.093570	22.676557
94.569348	2724.916601	22.681575
94.650559	2727.881773	22.686592
94.951128	2724.970041	22.691610
94.955648	2732.486038	22.696627
94.895660	2734.708391	22.701645
95.291224	2745.446899	22.706663
94.801548	2751.320977	22.711680
95.282858	2744.745189	22.716698
95.178043	2750.291354	22.721715
95.260691	2759.371711	22.726733
95.828607	2772.299979	22.731751
95.798100	2782.806671	22.736768
96.258814	2776.817395	22.741786
96.139484	2770.541058	22.746803
96.134858	2772.616444	22.751821
96.566171	2769.866143	22.756839
96.329529	2773.226101	22.761856
96.797922	2761.347711	22.766874
96.850885	2776.489749	22.771891
96.921209	2767.878687	22.776909
96.896933	2768.943470	22.781927
96.542430	2769.213651	22.786944
96.852940	2759.698194	22.791962
96.762402	2778.381581	22.796979
97.172588	2787.867602	22.801997
97.392475	2799.388836	22.807015
97.089608	2801.648261	22.812032
97.656850	2799.018374	22.817050
97.508285	2802.585820	22.822067
97.550634	2799.837704	22.827085
97.530658	2792.631845	22.832103
97.665496	2800.633030	22.837120
97.727748	2799.308107	22.842138
97.608347	2818.020337	22.847155
98.018456	2817.896186	22.852173
98.174116	2818.593359	22.857191
98.072657	2826.707702	22.862208
98.138816	2825.046671	22.867226
97.916159	2841.346304	22.872243
98.138826	2845.148383	22.877261
98.701321	2851.471572	22.882279
98.383382	2842.909003	22.887296
98.904224	2847.588167	22.892314
98.729737	2865.069710	22.897331
99.073000	2868.138777	22.902349
99.336591	2866.400562	22.907367
99.248077	2874.677760	22.912384
99.488214	2867.005538	22.917402
99.516390	2864.677507	22.922419
99.471884	2867.682813	22.927437
99.596422	2867.208666	22.932455
99.822680	2887.104796	22.937472
100.040067	2888.542996	22.942490
99.915301	2893.370014	22.947507
100.300369	2894.351676	22.952525
100.168276	2887.311198	22.957543
100.363134	2888.592485	22.962560
100.470996	2895.042937	22.967578
100.235247	2899.912350	22.972595
100.189272	2888.875389	22.977613
100.436932	2888.148161	22.982631
100.688845	2905.860752	22.987648
101.142167	2905.829061	22.992666
100.972492	2915.057593	22.997683
100.827189	2910.806931	23.002701
101.073249	2912.983756	23.007719
100.935705	2924.729630	23.012736
101.201245	2924.348682	23.017754
101.825000	2936.600857	23.022771
101.806772	2948.278957	23.027789
101.542191	2936.539904	23.032807
101.611868	2944.383826	23.037824
101.840355	2939.853534	23.042842
101.941052	2937.542622	23.047859
102.019389	2939.603507	23.052877
102.325622	2928.768464	23.057895
101.777996	2945.215324	23.062912
102.187212	2931.466126	23.067930
102.326122	2952.284359	23.072947
102.275993	2963.330690	23.077965
102.662815	2962.938323	23.082983
102.545437	2962.629435	23.088000
102.621057	2962.746113	23.093018
102.642328	2971.838331	23.098035
102.984917	2992.370905	23.103053
103.310897	2987.187786	23.108071
103.085493	2994.242325	23.113088
103.252629	2991.434929	23.118106
103.310650	3001.947192	23.123123
103.019007	2995.000017	23.128141
103.421799	3005.823344	23.133159
103.472364	3027.313057	23.138176
103.800187	3019.180926	23.143194
103.919645	3018.113074	23.148211
103.900483	3018.764390	23.153229
104.178921	3030.429659	23.158247
104.424137	3050.800856	23.163264
104.625904	3052.149129	23.168282
104.720253	3049.570329	23.173299
104.806317	3041.678626	23.178317
105.101648	3044.817088	23.183335
104.956698	3044.652146	23.188352
105.071968	3044.508693	23.193370
104.937336	3045.297250	23.198387
104.608548	3047.572420	23.203405
104.992506	3049.294109	23.208423
104.926271	3069.269610	23.213440
105.102955	3065.237275	23.218458
105.236320	3074.045221	23.223475
105.139404	3084.201659	23.228493
105.428683	3096.192772	23.233511
105.685829	3106.626070	23.238528
105.772363	3106.318461	23.243546
105.977599	3108.792259	23.248563
105.938535	3119.659685	23.253581
106.111129	3121.666796	23.258599
106.396316	3118.964253	23.263616
106.405168	3128.691358	23.268634
106.616786	3117.508427	23.273651
106.743497	3126.829759	23.278669
106.813609	3135.293846	23.283687
106.791820	3151.091600	23.288704
106.955376	3152.596618	23.293722
107.468336	3142.782030	23.298739
107.078687	3150.491454	23.303757
107.335429	3144.791348	23.308775
107.409622	3148.669270	23.313792
107.587116	3167.020132	23.318810
107.587924	3166.762939	23.323827
107.716804	3176.307980	23.328845
107.906568	3166.976064	23.333863
107.950002	3183.642670	23.338880
107.977772	3176.350374	23.343898
108.165195	3165.462784	23.348915
108.515062	3180.568263	23.353933
108.448673	3183.548509	23.358951
108.909034	3194.575844	23.363968
108.891349	3199.051334	23.368986
108.965649	3202.925708	23.374003
108.709119	3198.110645	23.379021
108.967530	3193.875751	23.384039
108.910371	3196.587908	23.389056
109.009239	3192.269969	23.394074
109.174783	3186.300666	23.399091
109.136386	3195.359975	23.404109
109.038247	3205.611980	23.409127
108.955817	3218.540804	23.414144
109.105708	3217.465931	23.419162
109.502948	3227.791462	23.424179
109.564243	3252.010309	23.429197
109.585865	3250.363301	23.434215
109.923073	3250.200820	23.439232
109.738517	3266.171324	23.444250
110.335543	3270.799812	23.449267
110.130821	3287.337517	23.454285
110.327870	3273.672365	23.459303
110.446722	3284.217665	23.464320
110.725775	3299.753140	23.469338
111.370869	3297.594589	23.474355
111.028927	3300.639379	23.479373
111.212167	3296.892545	23.484391
111.252475	3301.228921	23.489408
111.225938	3296.304481	23.494426
111.909981	3295.589641	23.499443
111.585252	3300.625499	23.504461
111.514278	3299.704918	23.509479
111.910507	3316.356567	23.514496
111.920474	3324.871663	23.519514
111.960295	3326.119200	23.524531
111.925429	3329.666366	23.529549
112.304327	3319.142288	23.534567
112.120933	3325.215108	23.539584
112.175750	3343.617594	23.544602
112.127131	3350.457176	23.549619
112.441396	3350.131152	23.554637
112.628148	3349.997912	23.559655
112.897881	3368.175454	23.564672
112.931252	3376.164597	23.569690
113.130195	3377.499192	23.574707
113.069207	3380.269895	23.579725
113.233322	3382.851739	23.584743
113.358374	3382.411748	23.589760
113.452740	3407.409703	23.594778
113.676836	3400.304510	23.599795
113.735319	3410.441731	23.604813
113.853246	3413.300155	23.609831
114.269334	3400.987767	23.614848
114.222160	3402.607235	23.619866
114.851780	3417.692615	23.624883
114.416333	3415.010109	23.629901
114.594878	3417.584057	23.634919
114.913445	3427.017127	23.639936
114.902647	3430.786342	23.644954
115.127119	3428.696627	23.649971
115.063402	3433.687345	23.654989
115.075337	3424.386688	23.660007
115.374383	3426.869418	23.665024
114.986795	3427.440394	23.670042
114.919374	3429.907805	23.675059
114.948732	3450.995658	23.680077
115.073610	3454.011226	23.685095
115.423362	3461.497584	23.690112
115.714946	3473.053908	23.695130
116.040947	3483.827677	23.700147
115.685548	3490.977985	23.705165
115.514289	3484.240609	23.710183
116.013247	3498.072741	23.715200
116.295272	3510.714273	23.720218
116.974855	3511.365293	23.725235
116.717765	3517.268870	23.730253
116.780519	3515.195681	23.735271
117.318865	3506.361433	23.740288
116.983961	3513.399289	23.745306
117.374695	3505.854991	23.750323
117.418021	3500.995701	23.755341
117.691178	3503.150800	23.760359
117.576917	3501.771174	23.765376
117.493022	3521.222551	23.770394
117.740404	3516.010142	23.775411
118.031394	3524.964314	23.780429
118.000414	3529.960667	23.785447
118.141388	3526.616495	23.790464
117.805364	3535.986727	23.795482
117.795580	3529.606109	23.800499
118.139360	3553.008479	23.805517
118.075087	3563.465768	23.810535
118.769468	3548.085154	23.815552
118.257523	3553.938408	23.820570
118.637599	3574.831338	23.825587
118.909552	3582.321578	23.830605
118.862209	3581.482511	23.835623
119.321676	3578.436824	23.840640
119.587952	3604.101602	23.845658
120.075896	3605.447827	23.850675
119.851304	3608.685872	23.855693
119.946972	3606.035494	23.860711
120.318767	3598.483262	23.865728
120.404734	3602.873587	23.870746
120.745059	3595.787650	23.875763
120.561792	3592.241995	23.880781
120.687110	3589.971012	23.885799
120.873208	3593.076484	23.890816
120.354545	3593.306915	23.895834
120.810013	3594.251376	23.900851
120.865725	3597.744231	23.905869
120.753845	3595.148298	23.910887
120.918429	3593.522078	23.915904
120.833552	3606.003145	23.920922
121.170352	3616.383041	23.925939
120.828764	3621.572599	23.930957
121.104251	3628.021197	23.935975
121.694610	3643.292454	23.940992
121.699076	3650.094240	23.946010
121.692800	3654.348650	23.951027
121.741824	3665.583023	23.956045
121.676389	3676.682397	23.961063
122.052614	3684.437352	23.966080
121.964469	3687.352782	23.971098
122.374151	3692.274262	23.976115
122.444819	3707.404426	23.981133
122.923002	3710.950213	23.986151
122.872676	3715.904941	23.991168
122.923450	3712.843416	23.996186
122.947142	3701.523051	24.001203
123.158518	3715.623099	24.006221
123.377322	3727.722443	24.011239
123.675391	3727.081728	24.016256
123.506702	3731.912337	24.021274
123.743483	3730.811232	24.026291
123.881560	3728.673962	24.031309
123.586243	3733.141231	24.036327
123.964195	3750.410628	24.041344
124.219890	3771.221643	24.046362
124.122500	3764.215580	24.051379
123.943625	3766.770404	24.056397
124.200771	3787.936368	24.061415
124.755632	3790.168901	24.066432
124.671845	3793.338784	24.071450
124.843347	3799.102600	24.076467
124.915161	3795.270145	24.081485
124.669483	3800.616348	24.086503
125.216095	3810.722627	24.091520
125.128629	3819.943986	24.096538
125.551789	3821.524217	24.101555
125.703578	3831.794316	24.106573
125.610479	3844.127305	24.111591
125.693636	3848.791826	24.116608
125.574892	3848.933210	24.121626
125.943183	3851.176559	24.126643
126.344825	3866.219399	24.131661
126.135536	3885.023780	24.136679
126.458614	3879.519150	24.141696
126.396467	3880.529640	24.146714
126.882271	3878.287529	24.151731
127.047347	3895.706914	24.156749
126.841161	3910.764589	24.161767
127.369222	3896.664904	24.166784
127.701023	3902.514835	24.171802
127.836451	3895.303215	24.176819
127.703878	3900.760666	24.181837
127.701099	3898.441939	24.186855
127.951147	3888.415656	24.191872
127.837537	3916.189811	24.196890
128.043927	3913.767150	24.201907
128.659098	3920.037172	24.206925
128.518016	3924.028892	24.211943
128.653235	3922.399232	24.216960
128.642948	3914.703777	24.221978
128.695047	3914.901535	24.226995
128.747518	3917.248371	24.232013
128.702969	3929.719080	24.237031
128.968960	3926.169059	24.242048
128.738278	3943.561091	24.247066
128.949751	3947.635415	24.252083
129.350430	3958.088047	24.257101
129.224535	3975.919529	24.262119
129.570775	3978.881618	24.267136
129.446676	3998.617845	24.272154
129.772709	3999.653852	24.277171
130.007284	4000.314390	24.282189
130.158989	4019.333223	24.287207
130.259318	4021.115371	24.292224
130.271110	4029.580147	24.297242
130.674001	4036.844566	24.302259
130.551319	4040.236326	24.307277
130.889832	4058.579296	24.312295
131.184839	4060.364656	24.317312
131.430438	4069.211284	24.322330
131.612977	4062.572194	24.327347
131.769617	4054.015045	24.332365
131.574947	4061.027958	24.337383
131.830780	4062.825317	24.342400
132.031193	4081.747959	24.347418
131.907987	4088.164708	24.352435
132.194798	4077.325004	24.357453
132.205936	4081.518370	24.362471
132.397621	4076.815077	24.367488
132.241411	4096.544930	24.372506
132.377105	4099.623804	24.377523
132.552221	4105.827364	24.382541
132.648465	4111.249368	24.387559
132.762179	4128.806670	24.392576
132.958379	4133.216696	24.397594
132.997646	4145.840657	24.402611
133.506499	4148.587637	24.407629
133.057222	4148.600645	24.412647
133.378195	4161.301621	24.417664
133.520375	4173.858164	24.422682
133.731820	4178.782299	24.427699
133.616369	4166.108030	24.432717
133.939313	4193.214237	24.437735
134.176011	4194.496584	24.442752
134.416905	4201.384683	24.447770
134.837725	4195.699168	24.452787
134.952060	4200.991415	24.457805
135.170057	4216.250855	24.462823
135.361684	4218.182505	24.467840
135.679858	4230.665067	24.472858
135.440874	4228.876030	24.477875
135.631779	4218.819953	24.482893
135.322659	4217.526076	24.487911
135.650118	4215.462129	24.492928
135.826379	4220.095990	24.497946
135.427426	4230.156692	24.502963
135.846875	4238.356419	24.507981
136.052434	4242.153799	24.512999
135.873799	4240.338232	24.518016
136.105494	4265.635740	24.523034
136.104612	4269.534246	24.528051
136.722350	4281.531745	24.533069
136.700367	4296.343508	24.538087
136.866858	4294.724383	24.543104
137.113025	4292.033617	24.548122
137.011486	4316.349190	24.553139
137.376027	4313.463201	24.558157
137.491056	4321.217221	24.563175
138.190022	4320.229749	24.568192
137.839214	4328.648399	24.573210
137.998241	4334.987808	24.578227
138.141344	4341.525954	24.583245
138.022626	4351.983724	24.588263
137.808233	4361.110645	24.593280
138.547443	4372.376954	24.598298
138.538317	4383.820717	24.603315
138.907120	4378.472154	24.608333
138.705995	4384.562492	24.613351
138.895362	4386.574080	24.618368
139.209840	4396.850692	24.623386
138.981033	4408.987654	24.628403
139.748769	4407.991943	24.633421
139.608534	4414.993638	24.638439
139.522158	4427.659890	24.643456
139.994784	4431.083908	24.648474
139.835377	4430.601598	24.653491
140.209838	4436.625803	24.658509
140.059300	4454.451669	24.663527
140.606150	4461.083681	24.668544
140.784918	4459.056133	24.673562
140.664610	4465.859241	24.678579
141.198521	4461.147217	24.683597
141.166203	4495.127402	24.688615
141.069565	4488.879299	24.693632
141.391938	4488.316438	24.698650
141.104562	4497.775265	24.703667
141.427363	4504.860214	24.708685
141.530266	4523.332516	24.713703
141.707643	4524.051375	24.718720
141.985553	4525.926252	24.723738
141.972356	4544.654853	24.728755
142.367844	4553.128054	24.733773
142.208205	4558.577613	24.738791
142.441039	4553.286154	24.743808
142.510872	4560.922554	24.748826
142.630167	4574.342425	24.753843
143.085000	4583.201956	24.758861
143.161423	4583.884766	24.763879
143.271701	4585.441667	24.768896
143.364421	4588.873487	24.773914
143.560781	4602.472786	24.778931
143.670422	4602.921707	24.783949
143.808350	4610.925671	24.788967
143.847309	4608.065968	24.793984
143.940204	4615.540278	24.799002
144.001038	4625.484158	24.804019
144.126029	4626.606259	24.809037
144.397987	4641.175157	24.814055
144.797146	4655.103202	24.819072
144.828485	4664.108497	24.824090
145.001061	4665.405437	24.829107
145.395533	4660.273046	24.834125
144.817462	4668.076617	24.839143
145.510055	4681.897039	24.844160
145.540627	4685.202922	24.849178
145.937673	4692.445777	24.854195
145.754323	4690.897920	24.859213
145.844991	4700.313181	24.864231
146.036598	4712.183884	24.869248
146.765166	4709.317102	24.874266
146.480680	4722.041590	24.879283
146.835892	4712.741619	24.884301
147.392641	4727.542244	24.889319
147.537596	4733.521079	24.894336
147.203477	4727.472072	24.899354
147.171016	4743.958767	24.904371
147.097425	4734.056409	24.909389
147.201872	4743.175656	24.914407
147.258440	4754.798615	24.919424
147.463373	4766.267072	24.924442
147.414147	4786.137588	24.929459
147.626233	4790.755449	24.934477
148.075824	4805.983421	24.939495
147.890656	4811.174247	24.944512
148.319232	4821.707896	24.949530
148.307039	4825.195728	24.954547
149.035943	4829.971397	24.959565
149.401967	4845.619626	24.964583
149.322517	4850.017210	24.969600
149.552257	4850.865240	24.974618
149.417379	4859.950145	24.979635
149.885483	4858.304657	24.984653
149.603427	4850.426131	24.989671
149.844233	4863.864722	24.994688
150.141946	4877.078899	24.999706
150.228106	4875.298175	25.004723
150.718747	4877.321380	25.009741
150.636582	4876.896361	25.014759
150.546906	4893.436788	25.019776
151.000409	4896.527785	25.024794
150.289711	4910.283031	25.029811
150.696488	4906.629154	25.034829
151.172388	4924.925979	25.039847
150.876057	4942.981301	25.044864
151.219500	4946.420521	25.049882
151.538325	4962.112908	25.054899
152.072364	4967.791147	25.059917
152.355705	4973.747164	25.064935
152.367838	4970.212162	25.069952
152.452699	4968.007929	25.074970
152.435748	4972.800800	25.079987
152.344881	4991.941302	25.085005
152.778870	5007.056280	25.090023
152.696793	5004.263010	25.095040
152.536562	4993.680980	25.100058
152.799765	5023.131302	25.105075
152.915412	5028.370057	25.110093
153.422856	5028.081332	25.115111
153.105257	5050.752335	25.120128
153.509958	5056.316556	25.125146
153.936645	5052.025350	25.130163
153.807588	5057.710228	25.135181
154.318339	5078.739865	25.140199
154.273205	5088.259749	25.145216
154.415038	5087.011639	25.150234
154.554936	5094.119260	25.155251
154.737070	5107.435460	25.160269
154.873816	5106.396899	25.165287
154.972941	5109.866365	25.170304
155.474458	5110.907265	25.175322
155.548875	5129.158171	25.180339
155.699362	5128.997847	25.185357
156.090330	5134.159554	25.190375
155.826209	5139.298188	25.195392
156.331143	5142.186976	25.200410
156.277274	5160.155938	25.205427
156.110631	5161.836713	25.210445
156.277854	5155.147721	25.215463
156.333624	5173.569521	25.220480
157.011535	5177.320433	25.225498
157.280255	5184.221687	25.230515
157.264970	5183.138982	25.235533
157.310392	5194.423875	25.240551
157.320335	5211.279715	25.245568
157.702659	5211.673272	25.250586
157.773469	5228.528505	25.255603
157.849883	5237.052539	25.260621
157.880651	5247.087636	25.265639
158.400591	5253.256617	25.270656
158.763720	5252.101809	25.275674
158.593204	5269.700352	25.280691
158.931259	5267.286406	25.285709
159.029803	5264.619129	25.290727
159.062088	5266.930129	25.295744
159.233372	5270.367994	25.300762
159.590860	5286.538672	25.305779
159.821489	5295.156920	25.310797
160.169149	5292.394841	25.315815
160.084770	5307.285616	25.320832
160.543410	5293.216661	25.325850
160.269310	5293.201448	25.330867
160.173341	5318.791174	25.335885
160.786952	5318.032794	25.340903
160.566589	5326.268133	25.345920
161.143168	5323.541396	25.350938
161.067149	5339.965042	25.355955
161.116428	5345.726823	25.360973
161.277229	5354.041628	25.365991
160.968577	5366.166552	25.371008
161.369307	5372.831021	25.376026
161.627222	5376.968126	25.381043
161.490071	5398.418127	25.386061
161.737707	5414.459842	25.391079
161.923861	5418.507239	25.396096
162.364161	5430.798056	25.401114
162.726355	5443.520027	25.406131
162.648117	5442.561927	25.411149
163.040279	5449.449950	25.416167
163.186021	5470.690971	25.421184
163.705269	5466.285883	25.426202
163.716420	5472.377725	25.431219
163.865113	5473.351835	25.436237
163.753006	5468.660619	25.441255
163.787561	5481.096620	25.446272
163.947750	5469.121521	25.451290
163.860789	5492.388990	25.456307
164.034870	5500.690647	25.461325
164.153348	5503.885275	25.466343
164.338930	5534.014135	25.471360
164.472182	5529.027100	25.476378
164.463910	5537.740164	25.481395
164.452590	5560.805399	25.486413
165.144571	5567.062588	25.491431
165.061663	5585.304626	25.496448
165.881873	5592.265191	25.501466
165.945932	5591.593054	25.506483
166.220286	5603.224689	25.511501
166.225436	5606.281366	25.516519
166.341295	5622.701105	25.521536
166.319229	5618.647075	25.526554
166.653228	5633.093995	25.531571
166.942840	5651.766691	25.536589
167.649630	5645.495385	25.541607
167.186032	5648.556424	25.546624
167.535742	5651.167778	25.551642
167.839579	5664.884884	25.556659
167.714817	5676.651957	25.561677
168.210744	5671.541828	25.566695
167.997749	5684.874311	25.571712
168.605185	5672.772248	25.576730
168.648428	5679.863843	25.581747
168.353418	5697.627604	25.586765
168.837661	5705.436174	25.591783
168.450348	5706.200531	25.596800
168.754917	5716.257544	25.601818
168.833461	5720.924567	25.606835
169.120433	5736.103967	25.611853
169.520933	5746.817738	25.616871
169.522341	5762.565048	25.621888
169.709587	5759.226924	25.626906
169.927812	5776.607302	25.631923
169.904190	5785.601071	25.636941
170.399937	5793.857507	25.641959
170.470005	5808.178157	25.646976
170.501353	5810.635100	25.651994
171.098832	5817.142745	25.657011
170.881398	5837.195227	25.662029
171.144224	5843.648019	25.667047
171.459592	5848.041952	25.672064
171.620762	5862.834315	25.677082
171.610457	5871.277747	25.682100
171.626983	5875.288759	25.687117
171.957447	5894.470868	25.692135
172.064375	5903.046919	25.697152
172.058715	5900.462947	25.702170
172.742746	5916.739312	25.707188
172.367206	5924.224845	25.712205
172.983437	5926.744079	25.717223
172.711501	5961.396396	25.722240
172.982276	5955.012062	25.727258
173.450561	5970.744511	25.732276
173.419840	5992.089482	25.737293
173.836109	5991.371622	25.742311
174.293559	6010.758898	25.747328
174.494185	6020.187462	25.752346
174.697187	6014.048249	25.757364
174.580186	6019.314034	25.762381
174.883383	6008.330889	25.767399
174.892650	6019.671189	25.772416
175.041465	6016.806435	25.777434
175.549001	6033.393321	25.782452
175.258774	6038.786243	25.787469
175.257351	6044.463734	25.792487
175.464073	6054.231563	25.797504
175.884252	6063.874272	25.802522
176.008124	6076.621244	25.807540
175.936568	6086.434374	25.812557
176.042951	6086.426268	25.817575
176.327127	6109.051931	25.822592
176.774047	6111.053399	25.827610
177.088618	6119.065119	25.832628
177.064803	6125.478052	25.837645
177.376275	6129.568685	25.842663
177.625903	6140.555016	25.847680
177.686673	6154.446685	25.852698
177.781023	6156.395470	25.857716
177.786413	6159.886986	25.862733
178.309511	6168.388772	25.867751
178.262140	6184.959776	25.872768
178.282670	6188.331435	25.877786
179.031084	6188.161120	25.882804
178.423952	6213.649457	25.887821
178.729587	6211.907864	25.892839
179.179976	6225.896559	25.897856
179.226375	6235.872198	25.902874
179.822115	6236.923575	25.907892
179.632806	6245.943459	25.912909
180.162949	6262.609546	25.917927
179.587277	6280.796910	25.922944
180.088638	6290.645282	25.927962
180.700472	6287.423429	25.932980
180.761248	6299.392601	25.937997
181.176865	6311.340846	25.943015
181.126062	6325.929292	25.948032
181.209097	6339.919042	25.953050
181.412771	6332.135791	25.958068
181.568848	6350.511639	25.963085
182.005525	6357.042192	25.968103
181.918659	6358.131756	25.973120
181.947998	6368.902670	25.978138
182.511312	6379.045658	25.983156
182.731122	6394.531388	25.988173
182.689102	6388.950074	25.993191
183.220697	6410.132419	25.998208
183.140862	6415.729294	26.003226
183.241965	6422.450903	26.008244
183.232091	6429.442933	26.013261
183.865213	6439.305029	26.018279
183.837864	6448.516393	26.023296
183.915399	6451.054006	26.028314
184.184770	6469.323808	26.033332
184.405461	6483.796566	26.038349
184.377588	6480.557704	26.043367
184.362887	6498.053837	26.048384
184.605970	6517.857659	26.053402
184.874429	6524.744580	26.058420
185.162104	6539.062160	26.063437
185.350652	6542.075266	26.068455
185.600873	6559.682778	26.073472
185.937719	6573.067547	26.078490
185.898564	6575.273205	26.083508
186.216054	6583.038143	26.088525
186.486173	6598.425164	26.093543
186.525224	6607.249129	26.098560
186.830377	6616.313391	26.103578
187.169736	6605.786989	26.108596
187.030398	6627.490275	26.113613
187.335762	6630.810937	26.118631
187.265030	6636.334705	26.123648
187.343465	6638.787133	26.128666
188.126571	6644.364894	26.133684
187.830005	6658.370508	26.138701
188.104163	6658.068400	26.143719
188.215058	6679.322326	26.148736
188.417664	6691.042257	26.153754
188.474518	6694.437153	26.158772
188.554629	6713.341126	26.163789
189.156354	6719.898069	26.168807
189.139654	6731.008454	26.173824
188.821507	6751.059857	26.178842
189.840374	6754.671224	26.183860
189.737617	6778.875784	26.188877
189.925592	6783.723497	26.193895
190.229505	6791.644379	26.198912
190.074628	6811.512872	26.203930
190.670686	6813.897754	26.208948
190.842059	6831.931357	26.213965
191.365018	6835.121521	26.218983
191.688245	6837.880816	26.224000
191.270962	6842.479020	26.229018
191.764602	6857.856071	26.234036
191.763545	6868.724513	26.239053
191.953150	6873.020616	26.244071
192.418687	6881.029787	26.249088
192.383748	6904.932663	26.254106
192.763349	6894.254479	26.259124
193.130694	6906.295447	26.264141
193.094429	6917.843206	26.269159
193.260452	6929.945088	26.274176
192.971944	6932.686731	26.279194
193.569781	6939.731978	26.284212
193.453428	6959.636813	26.289229
193.691917	6970.142723	26.294247
194.318193	6977.992218	26.299264
194.212641	6995.733152	26.304282
194.599847	7009.766085	26.309300
195.141472	7019.322323	26.314317
194.742272	7022.204395	26.319335
194.975954	7029.463562	26.324352
195.075970	7042.631940	26.329370
195.460454	7048.820908	26.334388
195.738733	7071.020428	26.339405
195.954695	7076.084146	26.344423
196.432055	7076.252506	26.349440
196.425024	7092.501133	26.354458
196.908237	7098.962854	26.359476
196.990120	7106.731608	26.364493
197.226715	7113.253065	26.369511
197.364233	7109.021001	26.374528
197.249222	7121.940689	26.379546
197.967452	7130.130282	26.384564
197.685867	7136.573692	26.389581
198.064155	7151.362036	26.394599
198.250833	7158.827540	26.399616
198.210857	7161.794315	26.404634
198.331661	7172.515187	26.409652
198.262088	7185.692065	26.414669
198.265733	7198.373985	26.419687
199.075303	7212.289130	26.424704
198.750267	7229.026128	26.429722
199.254511	7238.424850	26.434740
199.470563	7256.128588	26.439757
199.882235	7250.983861	26.444775
200.153083	7264.185582	26.449792
199.876480	7279.991448	26.454810
200.139316	7281.072807	26.459828
200.357174	7295.563317	26.464845
200.649919	7311.337190	26.469863
200.977767	7320.209054	26.474880
201.105106	7344.012470	26.479898
201.086847	7338.172466	26.484916
201.193819	7352.937384	26.489933
201.152389	7374.223757	26.494951
201.853458	7383.702622	26.499968
202.046353	7399.949974	26.504986
202.246675	7400.793567	26.510004
202.365903	7427.472741	26.515021
202.382266	7435.566792	26.520039
202.842651	7454.619008	26.525056
202.858180	7466.531959	26.530074
203.251711	7473.564794	26.535092
203.604843	7488.504129	26.540109
203.732438	7499.315470	26.545127
204.187683	7515.150079	26.550144
204.273546	7534.288809	26.555162
204.367086	7533.179264	26.560180
204.753138	7538.623002	26.565197
204.876782	7556.218703	26.570215
205.366252	7554.036933	26.575232
205.358445	7571.462212	26.580250
205.427577	7577.809144	26.585268
206.001626	7587.608486	26.590285
206.032023	7586.729159	26.595303
206.011988	7603.050564	26.600320
206.136240	7620.526505	26.605338
206.379994	7633.617226	26.610356
206.893445	7644.105636	26.615373
206.923426	7645.611543	26.620391
207.319538	7660.240659	26.625408
207.391903	7680.045046	26.630426
207.762888	7679.757615	26.635444
208.115846	7692.102466	26.640461
207.778465	7702.939717	26.645479
208.399600	7704.293418	26.650496
208.131863	7726.119494	26.655514
208.532382	7729.286789	26.660532
208.724089	7748.463394	26.665549
208.958568	7762.845238	26.670567
209.450653	7768.210849	26.675584
209.004282	7777.074072	26.680602
209.594220	7786.760629	26.685620
209.600662	7813.399253	26.690637
209.756824	7837.275043	26.695655
210.337245	7829.623263	26.700672
210.304962	7855.882389	26.705690
210.596759	7864.183131	26.710708
210.424885	7875.303459	26.715725
210.749071	7892.466962	26.720743
211.723140	7908.776145	26.725760
211.742054	7918.752664	26.730778
211.871699	7928.862888	26.735796
211.958532	7939.356736	26.740813
211.983233	7955.249666	26.745831
212.574635	7950.124592	26.750848
212.387170	7978.161496	26.755866
212.736624	7984.180181	26.760884
212.975171	7990.492143	26.765901
213.329754	8010.128125	26.770919
213.324157	8015.265845	26.775936
213.550687	8019.516762	26.780954
213.620561	8043.099144	26.785972
214.363332	8044.698993	26.790989
214.221524	8053.513526	26.796007
214.667930	8059.160926	26.801024
214.572432	8083.200054	26.806042
214.987234	8083.744292	26.811060
215.310228	8089.639787	26.816077
214.833876	8104.800512	26.821095
215.236106	8112.583684	26.826112
215.283146	8128.628271	26.831130
215.780811	8140.251589	26.836148
215.974785	8162.550875	26.841165
215.651475	8173.111983	26.846183
216.424015	8189.315389	26.851200
216.780001	8200.773150	26.856218
216.755341	8222.503734	26.861236
217.098138	8232.397687	26.866253
217.243045	8254.982507	26.871271
217.520456	8258.125388	26.876288
217.723019	8283.693309	26.881306
217.983424	8295.364681	26.886324
218.231073	8290.131768	26.891341
217.828233	8331.485396	26.896359
218.631291	8332.909083	26.901376
218.789974	8358.246490	26.906394
219.063362	8365.572957	26.911412
219.630439	8383.934321	26.916429
219.859872	8390.344056	26.921447
219.899422	8389.166978	26.926464
220.213558	8415.362588	26.931482
220.601338	8426.223653	26.936500
220.821205	8431.807070	26.941517
220.950748	8444.475441	26.946535
221.280652	8450.614127	26.951552
221.544492	8454.376097	26.956570
221.221469	8474.861362	26.961588
221.873337	8473.462393	26.966605
221.984873	8486.919948	26.971623
222.254195	8509.193854	26.976640
222.235729	8520.901314	26.981658
222.468873	8532.546651	26.986676
222.889367	8545.567115	26.991693
222.879407	8547.739066	26.996711
223.021587	8565.525022	27.001728
223.198441	8590.793618	27.006746
223.387663	8592.372512	27.011764
223.995248	8597.905985	27.016781
224.237335	8625.215930	27.021799
224.704389	8634.417612	27.026816
224.813237	8632.956483	27.031834
225.087771	8651.331922	27.036852
225.296561	8655.030580	27.041869
225.383309	8668.060702	27.046887
225.655906	8687.295155	27.051904
225.751420	8695.663485	27.056922
225.604859	8698.895544	27.061940
225.980491	8713.019340	27.066957
226.315442	8732.913908	27.071975
226.753520	8742.612011	27.076992
226.988154	8751.052659	27.082010
226.648024	8772.063419	27.087028
227.280653	8773.029315	27.092045
227.254688	8793.704504	27.097063
227.846821	8809.103382	27.102080
228.004877	8817.527595	27.107098
227.950692	8833.552620	27.112116
228.600660	8845.446655	27.117133
228.681264	8859.487862	27.122151
229.002342	8873.755540	27.127168
229.166307	8880.730108	27.132186
229.459352	8889.745683	27.137204
229.659204	8891.351994	27.142221
229.550417	8913.007636	27.147239
229.706323	8913.360009	27.152256
230.040641	8934.225462	27.157274
230.089737	8935.989079	27.162292
230.511579	8952.263135	27.167309
230.705499	8969.245328	27.172327
230.906761	8986.595789	27.177344
231.489922	9000.125382	27.182362
231.360528	9014.691481	27.187380
231.956472	9024.977298	27.192397
231.753254	9036.147734	27.197415
232.187939	9054.998150	27.202432
232.450986	9059.348864	27.207450
232.703401	9084.760136	27.212468
232.963588	9094.882576	27.217485
233.094625	9102.908858	27.222503
233.119257	9119.391424	27.227520
233.602950	9122.417615	27.232538
233.544010	9147.719033	27.237556
234.068279	9157.749744	27.242573
234.425403	9177.277241	27.247591
234.699410	9186.578160	27.252608
235.096007	9196.904965	27.257626
235.099042	9214.344419	27.262644
235.596580	9214.120312	27.267661
235.847901	9240.237865	27.272679
235.901608	9246.031838	27.277696
235.840653	9257.145791	27.282714
236.072026	9285.712001	27.287732
236.458610	9293.334484	27.292749
236.722338	9318.854544	27.297767
236.962757	9323.659690	27.302784
237.086491	9344.033506	27.307802
237.210140	9358.469797	27.312820
237.544174	9372.927209	27.317837
238.069926	9391.903962	27.322855
238.362316	9398.902402	27.327872
238.744906	9401.090630	27.332890
238.808554	9421.676166	27.337908
239.139172	9431.415323	27.342925
239.072667	9443.753765	27.347943
239.358401	9464.670493	27.352960
239.791102	9467.401891	27.357978
239.733348	9493.618286	27.362996
240.224359	9498.835774	27.368013
240.120163	9507.939513	27.373031
240.460282	9519.890071	27.378048
240.776402	9541.703108	27.383066
241.305833	9560.868525	27.388084
241.278391	9568.614033	27.393101
241.521265	9583.278947	27.398119
241.601442	9598.775939	27.403136
242.014266	9611.518874	27.408154
242.213732	9628.581205	27.413172
242.584372	9637.715133	27.418189
242.911111	9654.939982	27.423207
242.618293	9668.232273	27.428224
242.903158	9682.015077	27.433242
243.341260	9706.429960	27.438260
244.002341	9712.116472	27.443277
244.146117	9723.843647	27.448295
244.373062	9750.677455	27.453312
244.746547	9756.146885	27.458330
244.801319	9759.533326	27.463348
244.977488	9779.970707	27.468365
245.294023	9790.792501	27.473383
245.413874	9798.702024	27.478400
245.644448	9815.410404	27.483418
245.898337	9826.008612	27.488436
246.215823	9825.015464	27.493453
246.462706	9837.449653	27.498471
246.446991	9847.221183	27.503488
246.944227	9854.051986	27.508506
246.715645	9878.881586	27.513524
247.296736	9896.271786	27.518541
247.745339	9910.221485	27.523559
248.009121	9920.681826	27.528576
248.094409	9932.110797	27.533594
247.846580	9951.458126	27.538612
248.471447	9956.326664	27.543629
248.700839	9977.705594	27.548647
248.844585	9996.349238	27.553664
249.328441	10006.861442	27.558682
249.202546	10030.952634	27.563700
249.668848	10042.201229	27.568717
250.081055	10064.850709	27.573735
250.301696	10077.940170	27.578752
250.502950	10094.863255	27.583770
250.702260	10104.832544	27.588788
250.675879	10127.252974	27.593805
250.953628	10144.974122	27.598823
251.455073	10165.722914	27.603840
251.816838	10183.867443	27.608858
251.885855	10208.936634	27.613876
252.162948	10222.228794	27.618893
252.706628	10237.900996	27.623911
253.049749	10257.316316	27.628928
253.264966	10267.614750	27.633946
253.266274	10285.280183	27.638964
253.350442	10290.747267	27.643981
253.704232	10302.302228	27.648999
253.751453	10329.107663	27.654016
254.570924	10346.158727	27.659034
254.679860	10354.811686	27.664052
254.938477	10369.123337	27.669069
255.069318	10390.086605	27.674087
255.328321	10410.359022	27.679104
255.383215	10426.018563	27.684122
255.893955	10442.125003	27.689140
256.132310	10449.462166	27.694157
256.336679	10471.733793	27.699175
256.784963	10489.078866	27.704192
256.653705	10505.963670	27.709210
257.050834	10525.302618	27.714228
257.297675	10546.127135	27.719245
257.722238	10561.260787	27.724263
257.888706	10574.546340	27.729280
258.526574	10588.351063	27.734298
258.356552	10609.365993	27.739316
259.095250	10614.727207	27.744333
259.329391	10624.465728	27.749351
259.178124	10641.008906	27.754368
259.798988	10656.956308	27.759386
260.197997	10678.249003	27.764404
260.265567	10680.453316	27.769421
260.501868	10692.189516	27.774439
260.525595	10708.456411	27.779456
260.727275	10720.122728	27.784474
260.559529	10743.433267	27.789492
260.798400	10760.056953	27.794509
261.625297	10777.724141	27.799527
261.942184	10799.399308	27.804544
262.336432	10808.753750	27.809562
262.877705	10825.410962	27.814580
262.957075	10847.097145	27.819597
262.769061	10844.755282	27.824615
263.133905	10853.481176	27.829632
263.559430	10864.945095	27.834650
263.411134	10877.781919	27.839668
263.561145	10897.171674	27.844685
263.835361	10910.860388	27.849703
264.254558	10941.654892	27.854720
264.489198	10956.235757	27.859738
265.022712	10968.055324	27.864756
265.113502	10985.053567	27.869773
265.430094	10996.488339	27.874791
265.617517	11024.336919	27.879808
265.871990	11027.870205	27.884826
266.246468	11052.027425	27.889844
266.070286	11071.187749	27.894861
266.575339	11093.087435	27.899879
267.111675	11110.380785	27.904896
267.589637	11119.367008	27.909914
267.434728	11143.175509	27.914932
267.672688	11158.001824	27.919949
268.044685	11189.595642	27.924967
268.409489	11197.603186	27.929984
268.743403	11219.525068	27.935002
268.899305	11234.946492	27.940020
269.265041	11248.889799	27.945037
269.573824	11258.436711	27.950055
269.616531	11286.183635	27.955072
270.124153	11294.947591	27.960090
270.458489	11312.083927	27.965108
270.524419	11328.115973	27.970125
271.059968	11351.569398	27.975143
271.149466	11367.657461	27.980160
271.671704	11382.544080	27.985178
271.568175	11397.951874	27.990196
271.401954	11420.213665	27.995213
271.753340	11430.201148	28.000231
272.201192	11461.040749	28.005248
272.649481	11469.184309	28.010266
273.063650	11494.219635	28.015284
273.436957	11518.899332	28.020301
273.403935	11534.933779	28.025319
273.730000	11556.309043	28.030336
274.192120	11578.470197	28.035354
274.466827	11598.947936	28.040372
274.530518	11614.381833	28.045389
275.229302	11627.638445	28.050407
275.404792	11638.140519	28.055424
275.648376	11648.615570	28.060442
275.953798	11672.534596	28.065460
276.100870	11681.227652	28.070477
276.387973	11697.139935	28.075495
276.708750	11718.552532	28.080512
277.052544	11737.826126	28.085530
277.269266	11755.313320	28.090548
277.547865	11772.616951	28.095565
277.809617	11783.511400	28.100583
277.821815	11808.309616	28.105600
278.358168	11818.129628	28.110618
278.817677	11834.527226	28.115636
278.960148	11861.373010	28.120653
279.356589	11872.416990	28.125671
279.043603	11895.255263	28.130688
279.749129	11902.317995	28.135706
280.324777	11928.134087	28.140724
280.367893	11948.240887	28.145741
280.942195	11943.686282	28.150759
281.271850	11967.948415	28.155776
281.491274	11969.695991	28.160794
281.335029	11973.155645	28.165812
281.552112	12000.326538	28.170829
281.705886	11998.712696	28.175847
281.919780	12026.243450	28.180864
282.283608	12040.726694	28.185882
282.324499	12067.080637	28.190900
282.406981	12098.599659	28.195917
282.944402	12103.948998	28.200935
283.557896	12139.663354	28.205952
283.591222	12148.419612	28.210970
284.293857	12159.413106	28.215988
284.092285	12194.819681	28.221005
284.634856	12196.367239	28.226023
284.566967	12231.056813	28.231040
285.068297	12239.045429	28.236058
285.328174	12261.263057	28.241076
285.486380	12286.152872	28.246093
285.807491	12301.339951	28.251111
286.174142	12325.769842	28.256128
286.611294	12338.711049	28.261146
286.987343	12363.117378	28.266164
286.922369	12389.237226	28.271181
287.535154	12411.199661	28.276199
287.705194	12433.810604	28.281216
287.937752	12442.337059	28.286234
288.590287	12466.354237	28.291252
288.892962	12491.759406	28.296269
289.296890	12502.834095	28.301287
289.647582	12527.665630	28.306304
289.658845	12533.603336	28.311322
290.364990	12555.446505	28.316340
290.146462	12566.394187	28.321357
290.749372	12589.285122	28.326375
290.815893	12609.705620	28.331392
291.052569	12622.856737	28.336410
291.568317	12648.152816	28.341428
291.463157	12672.722783	28.346445
291.980980	12685.296337	28.351463
292.052791	12698.020945	28.356480
292.639650	12721.448954	28.361498
292.683035	12729.018779	28.366516
292.946908	12762.926504	28.371533
293.347543	12781.241656	28.376551
293.620044	12796.968328	28.381568
294.103632	12823.896344	28.386586
294.316165	12837.387302	28.391604
294.580298	12854.617263	28.396621
295.106680	12875.953230	28.401639
295.449857	12886.480363	28.406656
295.489928	12923.186478	28.411674
295.944582	12937.751622	28.416692
296.230040	12951.578884	28.421709
296.648514	12961.242601	28.426727
296.700688	12989.031839	28.431744
296.863164	13012.899280	28.436762
297.307792	13023.658706	28.441780
297.475040	13058.662555	28.446797
297.683958	13063.266013	28.451815
298.034682	13099.095314	28.456832
298.420539	13116.346379	28.461850
298.481112	13130.292964	28.466868
298.532671	13161.571738	28.471885
298.890012	13175.880564	28.476903
299.459790	13209.256344	28.481920
299.859162	13227.275930	28.486938
300.068924	13238.589711	28.491956
300.467451	13260.604520	28.496973
300.898825	13276.450346	28.501991
300.960346	13288.803616	28.507008
301.061190	13319.187270	28.512026
301.531903	13329.086834	28.517044
301.882432	13360.433126	28.522061
302.394903	13371.424253	28.527079
302.830477	13380.595264	28.532096
302.809137	13395.531159	28.537114
303.138853	13415.619124	28.542132
303.387953	13437.920516	28.547149
304.008007	13451.519465	28.552167
303.964855	13466.287253	28.557184
304.012967	13494.167853	28.562202
304.445282	13510.997164	28.567220
304.706400	13536.013693	28.572237
305.201125	13561.609381	28.577255
305.835978	13583.298681	28.582272
305.642105	13602.055149	28.587290
306.019233	13623.936879	28.592308
306.263356	13654.745023	28.597325
306.750787	13670.958619	28.602343
306.739258	13698.017311	28.607360
306.861600	13730.968626	28.612378
307.569681	13734.501502	28.617396
307.997084	13756.231673	28.622413
308.682158	13783.611761	28.627431
308.591661	13811.183306	28.632448
308.932435	13826.511972	28.637466
309.552452	13846.905445	28.642484
309.904992	13862.457569	28.647501
309.743440	13881.104989	28.652519
310.334361	13910.294382	28.657536
310.392632	13928.055996	28.662554
311.024893	13944.439743	28.667572
311.125651	13976.083874	28.672589
311.320366	13988.499156	28.677607
311.699683	14021.775737	28.682624
311.828363	14051.678607	28.687642
312.402639	14071.922329	28.692660
312.809327	14104.138604	28.697677
313.243761	14116.994999	28.702695
313.662581	14135.622297	28.707712
313.784562	14152.360216	28.712730
314.436336	14170.980519	28.717748
314.446095	14187.666126	28.722765
314.916710	14211.028838	28.727783
315.499483	14231.671669	28.732800
315.292280	14259.748707	28.737818
315.589053	14261.434875	28.742836
315.973075	14292.230520	28.747853
316.098506	14307.098823	28.752871
316.554247	14326.174133	28.757888
316.513750	14345.539640	28.762906
316.806216	14383.301043	28.767924
317.093880	14410.131718	28.772941
317.578819	14437.356901	28.777959
318.009506	14452.395461	28.782976
318.503640	14483.899810	28.787994
318.970372	14502.144491	28.793012
319.179197	14525.457994	28.798029
319.207729	14545.003016	28.803047
319.821270	14566.645142	28.808064
319.983473	14590.005854	28.813082
320.424780	14608.607905	28.818100
320.621948	14628.823322	28.823117
320.908991	14654.689935	28.828135
321.535309	14671.035995	28.833152
321.762579	14691.642106	28.838170
321.995335	14698.505355	28.843188
322.174771	14716.042876	28.848205
322.448836	14742.572160	28.853223
322.554691	14765.865221	28.858240
322.899389	14788.390623	28.863258
322.982339	14811.252534	28.868276
323.490015	14839.672463	28.873293
323.659186	14865.259456	28.878311
324.331072	14883.812623	28.883328
324.435439	14911.120497	28.888346
324.839145	14927.137999	28.893364
325.036034	14965.034768	28.898381
325.473923	14981.489556	28.903399
325.999825	15007.061858	28.908416
326.109058	15038.019442	28.913434
326.509266	15065.732531	28.918452
326.722995	15096.803748	28.923469
327.253987	15129.523165	28.928487
327.989950	15151.796747	28.933504
327.887841	15176.346317	28.938522
328.382661	15189.288130	28.943540
328.985930	15208.658432	28.948557
329.139340	15240.565804	28.953575
329.697852	15257.795284	28.958592
329.644126	15287.298728	28.963610
329.830841	15303.563717	28.968628
330.379143	15337.703950	28.973645
330.312986	15359.209012	28.978663
330.843705	15374.312248	28.983680
331.059388	15406.743954	28.988698
331.756247	15431.111228	28.993716
332.087190	15451.668033	28.998733
332.488231	15477.343695	29.003751
332.897096	15494.360190	29.008768
333.026873	15514.163859	29.013786
333.620846	15539.339562	29.018804
334.114548	15565.662019	29.023821
334.179010	15581.086923	29.028839
334.632965	15605.023381	29.033856
334.798634	15625.872558	29.038874
335.353324	15640.138271	29.043892
335.259554	15669.136765	29.048909
335.570259	15692.414570	29.053927
336.055626	15723.230801	29.058944
336.153040	15751.023532	29.063962
336.532456	15770.346433	29.068980
336.924853	15805.462312	29.073997
337.264615	15833.437316	29.079015
337.999427	15851.773107	29.084032
337.928891	15888.214136	29.089050
338.820613	15902.816772	29.094068
338.884399	15920.707299	29.099085
339.010491	15950.733841	29.104103
339.524083	15973.302267	29.109120
339.860442	15993.025034	29.114138
340.411185	16019.047175	29.119156
340.822790	16040.248650	29.124173
341.078002	16056.897103	29.129191
341.891628	16078.517566	29.134208
341.787925	16090.775768	29.139226
342.207443	16118.203713	29.144244
342.609722	16130.381352	29.149261
343.054321	16159.424005	29.154279
343.516002	16170.734371	29.159296
343.304285	16191.225868	29.164314
343.676094	16209.002678	29.169332
343.916175	16225.899698	29.174349
344.098030	16253.707672	29.179367
344.659679	16266.423331	29.184384
344.831551	16299.773536	29.189402
345.008788	16314.773789	29.194420
345.569747	16342.115647	29.199437
345.736006	16366.081912	29.204455
346.113856	16386.375192	29.209472
346.108616	16417.805120	29.214490
346.439822	16441.042758	29.219508
347.029938	16463.510920	29.224525
346.926332	16493.188703	29.229543
347.532286	16525.526489	29.234560
347.926433	16554.679069	29.239578
348.440078	16581.042407	29.244596
348.978841	16606.411728	29.249613
349.317276	16644.104501	29.254631
349.598273	16665.793400	29.259648
349.919425	16692.614372	29.264666
350.377955	16715.118841	29.269684
350.683231	16740.438740	29.274701
350.665182	16781.212574	29.279719
351.231670	16791.421531	29.284736
352.139799	16830.795350	29.289754
352.525281	16852.487693	29.294772
352.593089	16878.029955	29.299789
352.922051	16905.967578	29.304807
353.279537	16920.079461	29.309824
353.309677	16949.821046	29.314842
354.386450	16987.526388	29.319860
354.609283	17001.509300	29.324877
354.536140	17031.988502	29.329895
354.872030	17054.387626	29.334912
355.268624	17077.782427	29.339930
355.586476	17105.947640	29.344948
356.042378	17129.581758	29.349965
356.202614	17165.886517	29.354983
357.046295	17192.246650	29.360000
357.070957	17226.934595	29.365018
357.402037	17249.919600	29.370036
357.645053	17271.508387	29.375053
357.487762	17297.213080	29.380071
357.998393	17340.011510	29.385088
358.813492	17383.653450	29.390106
359.059816	17417.485404	29.395124
359.550783	17432.896618	29.400141
359.707200	17486.656130	29.405159
360.277937	17510.604398	29.410176
360.549246	17542.208221	29.415194
361.156476	17565.504218	29.420212
361.760387	17586.322743	29.425229
361.698519	17620.644348	29.430247
362.414892	17655.902852	29.435264
362.619723	17667.784843	29.440282
362.613437	17696.488653	29.445300
363.200852	17728.410963	29.450317
363.688512	17754.602340	29.455335
364.050611	17779.813532	29.460352
364.197437	17820.155918	29.465370
364.466450	17846.464022	29.470388
365.401336	17873.847415	29.475405
365.549998	17906.616694	29.480423
365.816241	17924.343457	29.485440
366.289516	17960.681692	29.490458
366.599650	17986.355802	29.495476
366.779433	18007.599743	29.500493
367.553884	18038.449688	29.505511
367.973504	18059.436456	29.510528
368.252049	18095.914410	29.515546
368.399471	18102.449544	29.520564
368.792130	18128.184307	29.525581
369.019339	18154.258624	29.530599
369.454835	18178.515571	29.535616
369.555809	18203.505783	29.540634
369.743902	18227.021838	29.545652
370.177129	18254.400605	29.550669
370.026054	18291.120344	29.555687
370.739678	18327.884651	29.560704
371.593877	18360.471845	29.565722
371.728340	18390.480920	29.570740
372.369546	18418.118754	29.575757
372.633438	18453.964608	29.580775
372.963829	18477.883109	29.585792
373.505071	18508.887605	29.590810
373.670264	18541.705843	29.595828
373.970363	18559.760312	29.600845
374.180018	18597.745252	29.605863
374.757908	18630.585221	29.610880
374.983833	18663.092540	29.615898
375.162174	18700.116518	29.620916
375.913890	18731.925280	29.625933
376.010890	18773.328151	29.630951
376.221395	18810.509427	29.635968
376.599134	18852.649545	29.640986
376.876556	18882.705209	29.646004
377.780460	18916.079817	29.651021
378.074492	18960.274045	29.656039
378.784844	18992.626161	29.661056
379.096553	19023.620730	29.666074
379.312305	19058.930377	29.671092
379.773752	19081.776522	29.676109
380.534914	19120.074960	29.681127
381.014768	19141.398380	29.686144
381.295877	19166.358642	29.691162
381.497209	19195.880410	29.696180
382.246903	19226.164377	29.701197
382.424763	19260.416566	29.706215
382.681834	19276.267063	29.711232
383.250553	19304.834329	29.716250
383.408971	19342.501520	29.721268
383.966959	19373.113869	29.726285
384.145766	19401.778938	29.731303
384.671975	19427.498332	29.736320
385.007223	19457.997928	29.741338
384.781555	19492.041478	29.746356
385.723818	19526.161397	29.751373
386.174447	19559.035289	29.756391
386.537357	19585.973830	29.761408
386.935849	19620.354202	29.766426
386.891501	19656.241032	29.771444
387.419719	19688.038155	29.776461
387.901774	19726.669534	29.781479
388.414115	19752.968750	29.786496
388.996183	19781.154665	29.791514
389.278402	19822.031274	29.796532
389.757907	19843.125467	29.801549
389.922291	19874.161757	29.806567
390.339650	19903.456675	29.811584
390.651173	19939.242646	29.816602
391.005102	19968.139837	29.821620
391.325707	20006.784391	29.826637
391.877823	20036.427741	29.831655
392.490776	20068.968332	29.836672
393.045030	20095.858683	29.841690
393.328603	20140.286360	29.846708
393.929574	20163.506621	29.851725
393.557562	20192.696190	29.856743
394.011208	20218.476107	29.861760
394.478811	20245.160311	29.866778
394.925637	20276.644083	29.871796
395.481598	20296.486967	29.876813
395.407612	20334.615803	29.881831
396.057372	20355.349795	29.886848
396.430407	20389.351258	29.891866
396.728289	20429.365909	29.896884
397.083338	20457.544810	29.901901
397.338699	20494.079124	29.906919
397.615435	20522.993198	29.911936
398.281078	20555.787737	29.916954
398.741209	20595.570967	29.921972
399.734836	20620.700849	29.926989
399.927642	20651.513138	29.932007
400.120747	20682.033751	29.937024
400.656263	20713.866297	29.942042
400.897755	20747.133453	29.947060
401.514283	20777.666152	29.952077
401.665817	20815.408732	29.957095
402.151953	20839.454614	29.962112
402.834831	20872.368322	29.967130
403.040932	20910.527787	29.972148
403.563428	20930.463677	29.977165
403.994638	20964.713674	29.982183
404.311336	21000.691824	29.987200
404.584106	21028.443825	29.992218
404.718473	21065.196486	29.997236
405.376948	21097.870286	30.002253
405.637180	21131.038919	30.007271
405.777119	21166.222059	30.012288
406.316196	21208.667767	30.017306
406.508899	21251.954530	30.022324
407.156733	21284.463321	30.027341
407.276101	21325.408370	30.032359
408.073049	21374.084017	30.037376
408.702431	21413.467484	30.042394
408.888918	21447.799955	30.047412
409.718576	21477.609620	30.052429
409.779357	21512.565340	30.057447
410.126900	21557.117032	30.062464
410.749093	21593.342315	30.067482
410.856638	21625.200106	30.072500
411.459235	21654.207252	30.077517
411.910871	21698.450391	30.082535
412.246508	21742.671847	30.087552
412.743350	21768.762341	30.092570
413.007628	21803.811125	30.097588
413.885593	21839.723405	30.102605
413.949403	21875.846182	30.107623
414.241788	21907.623457	30.112640
414.917834	21945.056276	30.117658
415.371914	21983.694308	30.122676
415.991051	22018.987554	30.127693
416.147262	22052.064832	30.132711
416.640609	22089.383141	30.137728
417.227706	22118.895071	30.142746
417.224368	22161.995852	30.147764
417.717830	22187.639741	30.152781
418.345599	22226.008330	30.157799
418.391766	22269.211567	30.162816
418.793699	22293.068470	30.167834
419.369794	22331.751752	30.172852
419.603326	22375.368914	30.177869
420.363437	22405.481862	30.182887
420.175686	22445.933284	30.187904
421.040437	22482.268551	30.192922
421.414438	22509.463798	30.197940
421.799008	22548.455216	30.202957
422.207781	22583.855409	30.207975
422.759462	22616.879380	30.212992
423.531955	22643.915862	30.218010
423.563227	22679.645215	30.223028
424.171681	22701.448575	30.228045
424.727719	22735.072834	30.233063
424.959338	22758.747279	30.238080
425.494226	22782.709017	30.243098
425.695069	22820.733314	30.248116
426.545233	22849.808767	30.253133
426.977422	22882.671691	30.258151
427.275723	22908.719532	30.263168
427.618610	22936.094067	30.268186
427.806704	22979.374962	30.273204
428.069906	23011.138633	30.278221
428.579342	23050.187805	30.283239
428.962113	23094.007607	30.288256
429.402941	23125.458257	30.293274
429.865319	23167.730762	30.298292
430.039493	23202.381044	30.303309
430.889968	23242.208396	30.308327
431.034252	23281.234950	30.313344
432.027131	23319.305901	30.318362
432.064131	23352.913201	30.323380
432.481657	23390.436146	30.328397
432.943861	23426.912592	30.333415
433.205019	23476.491902	30.338432
433.678086	23509.617347	30.343450
434.160985	23552.302141	30.348468
434.314150	23591.941360	30.353485
434.890437	23630.580259	30.358503
435.029297	23681.665876	30.363520
436.097631	23713.012191	30.368538
436.495817	23759.876229	30.373556
436.808128	23802.922616	30.378573
437.692281	23834.930415	30.383591
437.680711	23877.882354	30.388608
438.293647	23917.428897	30.393626
438.685428	23954.507908	30.398644
439.308124	23983.108855	30.403661
439.848081	24014.486394	30.408679
439.883538	24058.907049	30.413696
440.380372	24092.654176	30.418714
441.325198	24134.574845	30.423732
441.651702	24167.959216	30.428749
442.060416	24208.962669	30.433767
442.655821	24246.008617	30.438784
443.214653	24284.448453	30.443802
443.182501	24316.709719	30.448820
443.981139	24346.638379	30.453837
444.162920	24380.655836	30.458855
444.797424	24430.078354	30.463872
445.218010	24462.697074	30.468890
445.618292	24505.144022	30.473908
445.629248	24538.899891	30.478925
445.935839	24574.817889	30.483943
446.596072	24614.197361	30.488960
447.176341	24654.703539	30.493978
447.830907	24695.963956	30.498996
448.185594	24741.491095	30.504013
448.757209	24764.588482	30.509031
449.127292	24811.885852	30.514048
449.844175	24833.703967	30.519066
450.188898	24877.551985	30.524084
450.406658	24921.323347	30.529101
450.904285	24946.246836	30.534119
450.821569	24981.753838	30.539136
451.624165	25020.766887	30.544154
451.983471	25057.071437	30.549172
452.297844	25091.128290	30.554189
452.743963	25130.326745	30.559207
452.868297	25167.326474	30.564224
453.415783	25205.429605	30.569242
454.038268	25243.867369	30.574260
454.262839	25285.001647	30.579277
454.901279	25324.525141	30.584295
455.319609	25381.064157	30.589312
455.751844	25414.297827	30.594330
456.294157	25452.582153	30.599348
456.844182	25501.242648	30.604365
457.136400	25541.388538	30.609383
457.498314	25587.348850	30.614400
458.032446	25631.962314	30.619418
458.701460	25676.976242	30.624436
458.686538	25722.772168	30.629453
459.648527	25760.432582	30.634471
459.939252	25807.644886	30.639488
460.333575	25857.259508	30.644506
460.835894	25901.336399	30.649524
461.337107	25947.091670	30.654541
461.895000	25987.853884	30.659559
462.390718	26029.951294	30.664576
463.096255	26081.678919	30.669594
463.623359	26117.948477	30.674612
463.709284	26164.243040	30.679629
464.351466	26206.628924	30.684647
464.600435	26252.701174	30.689664
465.526376	26290.043816	30.694682
465.649140	26320.008906	30.699700
465.717518	26372.432705	30.704717
466.495621	26414.941709	30.709735
467.010626	26461.087204	30.714752
467.525694	26517.052454	30.719770
468.546664	26560.862249	30.724788
468.716178	26604.721575	30.729805
469.454701	26638.484180	30.734823
469.197043	26690.786247	30.739840
469.940832	26729.522697	30.744858
470.331751	26774.743231	30.749876
470.932785	26832.837146	30.754893
471.481683	26868.256125	30.759911
472.069691	26918.756538	30.764928
472.185995	26959.477403	30.769946
472.974855	27002.840939	30.774964
473.396026	27046.678667	30.779981
473.902094	27089.616041	30.784999
474.201960	27143.962815	30.790016
474.850745	27176.567842	30.795034
475.378852	27216.653354	30.800052
475.511759	27264.195429	30.805069
476.362069	27299.846168	30.810087
476.608223	27348.136286	30.815104
477.354265	27397.419524	30.820122
477.960649	27430.502076	30.825140
477.982891	27478.662418	30.830157
478.845038	27515.901548	30.835175
479.381495	27564.298804	30.840192
479.850695	27600.297140	30.845210
480.463131	27636.694564	30.850228
480.697431	27681.214666	30.855245
481.299628	27714.585522	30.860263
481.519220	27759.010464	30.865280
481.713602	27812.856272	30.870298
482.206066	27858.700065	30.875316
482.599931	27892.471675	30.880333
483.183269	27931.246828	30.885351
483.581064	27976.491439	30.890368
484.120508	28019.589634	30.895386
484.607285	28062.870158	30.900404
484.539539	28116.283922	30.905421
485.721775	28150.771036	30.910439
486.229364	28196.420780	30.915456
486.473661	28229.804529	30.920474
486.703401	28278.528986	30.925492
487.038189	28337.078949	30.930509
487.865001	28379.168290	30.935527
488.299864	28438.613754	30.940544
488.513432	28485.467545	30.945562
489.474672	28532.210361	30.950580
489.552082	28594.311874	30.955597
490.210545	28632.814313	30.960615
490.255011	28681.680971	30.965632
490.837870	28743.289253	30.970650
491.906980	28798.163790	30.975668
491.915907	28853.554652	30.980685
492.847977	28899.438859	30.985703
493.099918	28944.120161	30.990720
493.848650	28999.679314	30.995738
494.481776	29039.505570	31.000756
494.711129	29103.864711	31.005773
495.313015	29150.100771	31.010791
495.516101	29207.735291	31.015808
496.195265	29259.356864	31.020826
496.898036	29318.385556	31.025844
497.412930	29366.772455	31.030861
497.832209	29404.464346	31.035879
498.469452	29460.302115	31.040896
499.139403	29522.545492	31.045914
499.578398	29557.552749	31.050932
499.837089	29611.371372	31.055949
500.549138	29658.123734	31.060967
501.395192	29707.781864	31.065984
501.288456	29751.354079	31.071002
501.858402	29801.092866	31.076020
502.170780	29859.752591	31.081037
502.800367	29909.948758	31.086055
503.187185	29958.153407	31.091072
503.755238	30014.288340	31.096090
504.464363	30071.416033	31.101108
505.144503	30121.938876	31.106125
505.927064	30174.776506	31.111143
506.114403	30217.919454	31.116160
506.595600	30268.481948	31.121178
507.536764	30307.755306	31.126196
507.463963	30362.744825	31.131213
508.123113	30407.034343	31.136231
508.605545	30456.376148	31.141248
509.214842	30517.046067	31.146266
509.684803	30565.781305	31.151284
510.387742	30620.009085	31.156301
510.841544	30657.095323	31.161319
511.152470	30703.913687	31.166336
511.477944	30755.872686	31.171354
512.335567	30804.560214	31.176372
512.583583	30852.679849	31.181389
513.230621	30905.920723	31.186407
513.798213	30958.972971	31.191424
514.175179	31012.233612	31.196442
514.807816	31059.801112	31.201460
515.149826	31114.702250	31.206477
515.704707	31159.840739	31.211495
516.624858	31210.084040	31.216512
516.848409	31261.064333	31.221530
517.246123	31297.773103	31.226548
517.944222	31344.355563	31.231565
518.304349	31387.807240	31.236583
518.842117	31429.468981	31.241600
518.984202	31490.673917	31.246618
519.709282	31527.250114	31.251636
520.201716	31576.842667	31.256653
520.792959	31622.402290	31.261671
521.189970	31670.105082	31.266688
521.553413	31731.091214	31.271706
522.275927	31770.934114	31.276724
522.859087	31830.032044	31.281741
523.491109	31877.784860	31.286759
523.803167	31921.009147	31.291776
524.246772	31970.885402	31.296794
524.834536	32027.976408	31.301812
525.586432	32093.045694	31.306829
525.865460	32138.188150	31.311847
526.596985	32194.631135	31.316864
526.775224	32250.963900	31.321882
527.298656	32310.073313	31.326900
527.763295	32366.475808	31.331917
528.095925	32417.242584	31.336935
528.724724	32482.545082	31.341952
529.278938	32550.996712	31.346970
530.084055	32598.148529	31.351988
530.503099	32657.920092	31.357005
530.622945	32723.736838	31.362023
531.383048	32779.451185	31.367040
531.864124	32838.954339	31.372058
532.696529	32905.070383	31.377076
533.064455	32973.059040	31.382093
533.858572	33026.991956	31.387111
534.883906	33085.146808	31.392128
534.969481	33146.442531	31.397146
535.857793	33185.128321	31.402164
536.353797	33251.140377	31.407181
536.803696	33294.894273	31.412199
537.438287	33345.238215	31.417216
537.848927	33407.860058	31.422234
538.711930	33459.968398	31.427252
538.844378	33516.457902	31.432269
539.328724	33562.885906	31.437287
540.462071	33623.602822	31.442304
540.557370	33681.847238	31.447322
541.164864	33733.288625	31.452340
541.875878	33798.847424	31.457357
542.279115	33843.598122	31.462375
543.371275	33896.222070	31.467392
543.473498	33944.778135	31.472410
543.864965	33996.492704	31.477428
544.458305	34057.884259	31.482445
544.950282	34110.368308	31.487463
545.403385	34160.501584	31.492480
545.907591	34230.287044	31.497498
546.514361	34286.536396	31.502516
547.013232	34339.780522	31.507533
547.482051	34397.138643	31.512551
548.274498	34454.033143	31.517568
548.457990	34526.599448	31.522586
549.177898	34569.778454	31.527604
549.623696	34629.719448	31.532621
550.219270	34684.561238	31.537639
551.016810	34745.274411	31.542656
551.053482	34811.592291	31.547674
551.789018	34872.054213	31.552692
552.529924	34924.224895	31.557709
552.985142	34981.265231	31.562727
553.888352	35032.077577	31.567744
554.073958	35084.179650	31.572762
554.754038	35123.446915	31.577780
555.492097	35171.156292	31.582797
555.424371	35230.436297	31.587815
556.163242	35282.198082	31.592832
556.488801	35344.095959	31.597850
557.411460	35391.541836	31.602868
557.628768	35450.478741	31.607885
558.251775	35512.744575	31.612903
559.181535	35572.479242	31.617920
559.408075	35635.827335	31.622938
560.341252	35684.155931	31.627956
560.841541	35743.959070	31.632973
560.924285	35794.858827	31.637991
561.847078	35856.536562	31.643008
562.125837	35914.186608	31.648026
562.740091	35975.827431	31.653044
563.518841	36044.154266	31.658061
563.944349	36111.709748	31.663079
564.496185	36166.686380	31.668096
565.136799	36228.869713	31.673114
565.314850	36296.921313	31.678132
566.286455	36359.858306	31.683149
566.888411	36424.643067	31.688167
567.382779	36487.530063	31.693184
568.123956	36547.081384	31.698202
568.612465	36608.454800	31.703220
569.177935	36676.390070	31.708237
569.482605	36739.590230	31.713255
570.229520	36795.581204	31.718272
570.839584	36862.660770	31.723290
571.450633	36927.291169	31.728308
572.205251	36997.538287	31.733325
573.154289	37052.502391	31.738343
573.731710	37110.513991	31.743360
574.148752	37165.026732	31.748378
574.381508	37219.314468	31.753396
575.473779	37277.705396	31.758413
575.653500	37352.205869	31.763431
576.443007	37404.173675	31.768448
577.230147	37471.731208	31.773466
577.519026	37525.770690	31.778484
578.321298	37583.045887	31.783501
578.837646	37653.798952	31.788519
579.437233	37697.772355	31.793536
579.585322	37759.262800	31.798554
579.888665	37823.227639	31.803572
580.982289	37888.905298	31.808589
581.463747	37961.985300	31.813607
582.077363	38013.993421	31.818624
582.632605	38086.622971	31.823642
583.026091	38149.671295	31.828660
583.821482	38215.655150	31.833677
584.175303	38282.978052	31.838695
585.083068	38338.517888	31.843712
585.256792	38417.326009	31.848730
586.045916	38468.188983	31.853748
586.943702	38532.787115	31.858765
587.444737	38604.550179	31.863783
587.756643	38659.564581	31.868800
588.326055	38726.114813	31.873818
588.483497	38800.643824	31.878836
589.394753	38858.612071	31.883853
590.064593	38937.943261	31.888871
590.953488	39005.489642	31.893888
591.135324	39057.941497	31.898906
591.510760	39128.215373	31.903924
592.688643	39179.454780	31.908941
593.291463	39250.767921	31.913959
593.802645	39294.870282	31.918976
594.317550	39357.012501	31.923994
594.746303	39420.425544	31.929012
595.254018	39472.509000	31.934029
595.665732	39544.786125	31.939047
596.356948	39599.289184	31.944064
596.971397	39665.642818	31.949082
597.483516	39728.342338	31.954100
598.163927	39805.150142	31.959117
598.602228	39873.951740	31.964135
599.227740	39936.835244	31.969152
599.685357	40012.531710	31.974170
600.430310	40090.753738	31.979188
600.723257	40151.978857	31.984205
601.578102	40225.773218	31.989223
602.064119	40294.928373	31.994240
602.748890	40365.960794	31.999258
603.519736	40438.090462	32.004276
604.225616	40520.026928	32.009293
604.634795	40587.383848	32.014311
605.242309	40659.336207	32.019328
605.675898	40730.029603	32.024346
606.354421	40810.232428	32.029364
607.221249	40878.717482	32.034381
607.402621	40962.144364	32.039399
608.426796	41029.183318	32.044416
609.037218	41106.352231	32.049434
609.446713	41172.770455	32.054452
610.178211	41252.732819	32.059469
610.671343	41330.989138	32.064487
611.517432	41411.094235	32.069504
612.024162	41497.554111	32.074522
612.668196	41560.459025	32.079540
613.484017	41629.801388	32.084557
613.969259	41708.988784	32.089575
614.625864	41782.777964	32.094592
615.205652	41855.361506	32.099610
615.779119	41933.843860	32.104628
616.845071	41996.869878	32.109645
617.350273	42076.873236	32.114663
618.330668	42139.304566	32.119680
618.642313	42219.296358	32.124698
619.437332	42273.322879	32.129716
620.327494	42341.765283	32.134733
620.593883	42416.410833	32.139751
621.399342	42485.196126	32.144768
622.100290	42557.610820	32.149786
622.284778	42627.067670	32.154804
622.754839	42688.660208	32.159821
622.916905	42761.849969	32.164839
624.089740	42836.454584	32.169856
624.385603	42912.057050	32.174874
625.293046	42984.922305	32.179892
626.167492	43055.305351	32.184909
626.546490	43141.282515	32.189927
627.342904	43200.937834	32.194944
627.974910	43284.723662	32.199962
628.496365	43364.161534	32.204980
629.425301	43432.500494	32.209997
630.088988	43508.142397	32.215015
630.550763	43570.004433	32.220032
631.014070	43654.350266	32.225050
631.431954	43719.352199	32.230068
632.742703	43780.474569	32.235085
632.987348	43862.180018	32.240103
633.696435	43912.101892	32.245120
634.136480	43980.662664	32.250138
634.720863	44050.557519	32.255156
635.399092	44118.122676	32.260173
635.838838	44193.384449	32.265191
636.438288	44256.463711	32.270208
637.305241	44320.054652	32.275226
637.938906	44395.629323	32.280244
638.830630	44455.146573	32.285261
638.934019	44523.818702	32.290279
639.650541	44598.521628	32.295296
640.401440	44672.192953	32.300314
640.845818	44751.501045	32.305332
641.599902	44824.035707	32.310349
642.289041	44918.965708	32.315367
642.739415	44981.516325	32.320384
643.362135	45061.067772	32.325402
643.588638	45137.003282	32.330420
644.502146	45217.653511	32.335437
645.122622	45304.456354	32.340455
645.724855	45375.537309	32.345472
646.769055	45462.867586	32.350490
646.967216	45551.828676	32.355508
648.016223	45626.929071	32.360525
648.241268	45707.325833	32.365543
649.009695	45786.830971	32.370560
649.708862	45871.899267	32.375578
650.203673	45960.936356	32.380596
651.063394	46046.165184	32.385613
651.643426	46132.994311	32.390631
652.328342	46216.629706	32.395648
653.108009	46295.298295	32.400666
653.561700	46389.043070	32.405684
654.063376	46471.699389	32.410701
654.541188	46559.627371	32.415719
655.548758	46644.935484	32.420736
656.724088	46730.538335	32.425754
657.079678	46819.457220	32.430772
657.782298	46900.310561	32.435789
658.816540	46990.851688	32.440807
659.339775	47067.756389	32.445824
660.398800	47143.489575	32.450842
660.948315	47228.279225	32.455860
661.712347	47306.698791	32.460877
661.961126	47377.419389	32.465895
662.876913	47454.781786	32.470912
663.751336	47539.288533	32.475930
664.576846	47622.051020	32.480948
665.171594	47689.064818	32.485965
665.521396	47765.018861	32.490983
665.882203	47837.424840	32.496000
666.718484	47921.330075	32.501018
667.415855	48005.722903	32.506036
668.365553	48091.934506	32.511053
668.479990	48181.360719	32.516071
669.355201	48261.521750	32.521088
669.966451	48341.335170	32.526106
670.205468	48431.190400	32.531124
671.241464	48504.955770	32.536141
671.795406	48603.905888	32.541159
672.366423	48679.230057	32.546176
673.474493	48764.818426	32.551194
674.369301	48853.262789	32.556212
674.557951	48932.052658	32.561229
675.301386	49012.652365	32.566247
676.130430	49097.037690	32.571264
676.740403	49181.709134	32.576282
677.223447	49263.423639	32.581300
677.940215	49339.790645	32.586317
678.598837	49420.229224	32.591335
678.945312	49503.195940	32.596352
679.891895	49577.589790	32.601370
680.481282	49665.624131	32.606388
680.703308	49754.041804	32.611405
681.099976	49825.312314	32.616423
682.069653	49915.956916	32.621440
683.125034	50000.807794	32.626458
683.590278	50094.319279	32.631476
684.051647	50181.859163	32.636493
684.821437	50274.781040	32.641511
685.473825	50356.547964	32.646528
686.465937	50442.055584	32.651546
687.176504	50535.727607	32.656564
687.940450	50621.040030	32.661581
688.459161	50696.633420	32.666599
689.042851	50797.352353	32.671616
689.979256	50884.380945	32.676634
690.128362	50989.184186	32.681652
691.109546	51083.452130	32.686669
691.693099	51178.152712	32.691687
692.283375	51275.796517	32.696704
693.093695	51363.719907	32.701722
693.384485	51464.680273	32.706740
694.326607	51560.056217	32.711757
694.969708	51659.158847	32.716775
696.159925	51773.725121	32.721792
696.862701	51862.464558	32.726810
697.567859	51963.447408	32.731828
698.045035	52067.286135	32.736845
698.549907	52154.297033	32.741863
699.109807	52264.870333	32.746880
699.909504	52360.621225	32.751898
700.491477	52472.177603	32.756916
701.208897	52577.982017	32.761933
702.110311	52678.759202	32.766951
702.673527	52782.088387	32.771968
703.879328	52878.899209	32.776986
704.737991	52991.966969	32.782004
705.615787	53082.294052	32.787021
706.211346	53172.339706	32.792039
707.035472	53274.680638	32.797056
707.856898	53364.948850	32.802074
708.310523	53462.259740	32.807092
709.084346	53557.584819	32.812109
709.976506	53652.284248	32.817127
710.459742	53750.046567	32.822144
711.543734	53836.192004	32.827162
712.076140	53935.027512	32.832180
712.740174	54024.465515	32.837197
713.761587	54122.039565	32.842215
714.447833	54215.297297	32.847232
715.254857	54297.029867	32.852250
715.948169	54393.200007	32.857268
716.840390	54477.781436	32.862285
717.494129	54567.160420	32.867303
717.963183	54658.270012	32.872320
718.895878	54741.424233	32.877338
719.422990	54833.112641	32.882356
720.106982	54924.541739	32.887373
720.844402	55011.874334	32.892391
721.702782	55102.302353	32.897408
722.465752	55188.399383	32.902426
723.436885	55283.321046	32.907444
724.070103	55367.652151	32.912461
724.935737	55451.439676	32.917479
725.427449	55533.874020	32.922496
726.573185	55597.876247	32.927514
727.371153	55677.575076	32.932532
727.909196	55758.511467	32.937549
728.737917	55830.212588	32.942567
729.254515	55905.061815	32.947584
729.481165	55985.001714	32.952602
729.966441	56065.682692	32.957620
730.942794	56157.890564	32.962637
731.434594	56240.542665	32.967655
731.842512	56338.210159	32.972672
732.705281	56429.288028	32.977690
733.301877	56518.249241	32.982708
734.032709	56624.787159	32.987725
734.300898	56722.340627	32.992743
734.988005	56828.368700	32.997760
736.273915	56926.197155	33.002778
736.670583	57026.839869	33.007796
737.332863	57126.788276	33.012813
737.795829	57228.501619	33.017831
738.550467	57344.960627	33.022848
739.625370	57452.223308	33.027866
740.592560	57564.174367	33.032884
740.779944	57655.919321	33.037901
742.258705	57770.826529	33.042919
742.650710	57879.683194	33.047936
743.426950	57995.314557	33.052954
743.956303	58095.112830	33.057972
744.856315	58209.770708	33.062989
746.006503	58305.675612	33.068007
746.501661	58421.109452	33.073024
747.298074	58515.974265	33.078042
748.281296	58624.206313	33.083060
748.781708	58737.296497	33.088077
749.829664	58838.737950	33.093095
750.431988	58956.116242	33.098112
751.295166	59047.856865	33.103130
751.951106	59159.432214	33.108148
752.679176	59266.294266	33.113165
753.381629	59368.737189	33.118183
753.968949	59490.456513	33.123200
754.937755	59597.697610	33.128218
755.769182	59698.831595	33.133236
756.404028	59807.487841	33.138253
757.492841	59922.370690	33.143271
757.859842	60026.901167	33.148288
758.859139	60140.188429	33.153306
759.851136	60246.291492	33.158324
760.421469	60351.030170	33.163341
761.174038	60454.304549	33.168359
761.842988	60561.290641	33.173376
762.598034	60671.233596	33.178394
763.429490	60777.833688	33.183412
764.178864	60896.222765	33.188429
765.340398	61000.620498	33.193447
766.050949	61115.389356	33.198464
766.629961	61221.268746	33.203482
767.390237	61308.270961	33.208500
767.872067	61429.437838	33.213517
768.941817	61540.180369	33.218535
769.996837	61640.098741	33.223552
770.725891	61745.444056	33.228570
771.513734	61846.924582	33.233588
772.224822	61951.635541	33.238605
773.063048	62045.176238	33.243623
773.535540	62161.943441	33.248640
774.657517	62263.762648	33.253658
775.432516	62365.355315	33.258676
776.267078	62465.756632	33.263693
776.776930	62561.970832	33.268711
777.821105	62651.175701	33.273728
778.846325	62744.606481	33.278746
779.454705	62829.611249	33.283764
780.329216	62924.932461	33.288781
780.969601	63010.944042	33.293799
781.580801	63105.462624	33.298816
782.355020	63189.872552	33.303834
783.169034	63297.278754	33.308852
784.040134	63394.758200	33.313869
784.873600	63489.203848	33.318887
785.133600	63590.672814	33.323904
785.614538	63694.065315	33.328922
786.330451	63795.093242	33.333940
787.292830	63908.704524	33.338957
788.286408	64022.943402	33.343975
789.086203	64131.601588	33.348992
789.659043	64240.885771	33.354010
790.595830	64348.296081	33.359028
791.277280	64456.406611	33.364045
792.005922	64560.773894	33.369063
792.635005	64687.372027	33.374080
793.546041	64798.107726	33.379098
794.703852	64907.684274	33.384116
795.312497	65027.624889	33.389133
796.098009	65136.998712	33.394151
796.570848	65254.801083	33.399168
797.902789	65371.766633	33.404186
798.798374	65478.089601	33.409204
799.128775	65585.062910	33.414221
800.434241	65697.805377	33.419239
801.313514	65810.283884	33.424256
801.785046	65919.201660	33.429274
802.515286	66036.763559	33.434292
803.491962	66165.393074	33.439309
804.279481	66271.150000	33.444327
805.121164	66386.634451	33.449344
805.974534	66497.395009	33.454362
807.101604	66608.199393	33.459380
807.787979	66719.696819	33.464397
808.943463	66827.197497	33.469415
809.878436	66948.271056	33.474432
810.205640	67051.958489	33.479450
811.256357	67153.864008	33.484468
811.723881	67268.745022	33.489485
813.052858	67379.507427	33.494503
813.599792	67494.547239	33.499520
814.027289	67596.716033	33.504538
815.307568	67711.768507	33.509556
815.883138	67835.176354	33.514573
816.927908	67937.181474	33.519591
817.591792	68059.437969	33.524608
818.203110	68178.839732	33.529626
819.215280	68283.804560	33.534644
819.898449	68404.732106	33.539661
820.610411	68525.295185	33.544679
821.212763	68632.188387	33.549696
822.254499	68760.152742	33.554714
823.295178	68871.147669	33.559732
823.886109	68998.726455	33.564749
825.009850	69104.201678	33.569767
825.971640	69215.717278	33.574784
826.370497	69338.587698	33.579802
827.542800	69452.700058	33.584820
828.110738	69573.008353	33.589837
829.255341	69685.052595	33.594855
830.003619	69800.166427	33.599872
830.477992	69914.377715	33.604890
831.601846	70008.861526	33.609908
832.338395	70117.010919	33.614925
833.079192	70216.566942	33.619943
833.824365	70336.413915	33.624960
834.816019	70445.224649	33.629978
835.778719	70548.406677	33.634996
836.718909	70658.466368	33.640013
837.285099	70764.655356	33.645031
838.096845	70869.545903	33.650048
838.569805	70983.054891	33.655066
839.444063	71094.822394	33.660084
840.079741	71226.485665	33.665101
840.791839	71330.648767	33.670119
842.235150	71453.782229	33.675136
842.422275	71579.963441	33.680154
843.696092	71684.338881	33.685172
844.676133	71818.212663	33.690189
845.448800	71937.671930	33.695207
846.303090	72061.007449	33.700224
846.971379	72189.452415	33.705242
847.996143	72305.109375	33.710260
848.500708	72438.882240	33.715277
849.602040	72550.385731	33.720295
850.521897	72681.770549	33.725312
851.232834	72810.041388	33.730330
852.115168	72924.586894	33.735348
852.955160	73065.960157	33.740365
854.112634	73184.104161	33.745383
854.847044	73315.453910	33.750400
855.677531	73436.480230	33.755418
856.595482	73556.069820	33.760436
857.211071	73691.526891	33.765453
858.008252	73814.483371	33.770471
859.296560	73955.908416	33.775488
860.148656	74087.338205	33.780506
861.084421	74200.648331	33.785524
861.840526	74337.800060	33.790541
862.814759	74461.268464	33.795559
863.564091	74582.415734	33.800576
864.280454	74717.786588	33.805594
865.487116	74843.742177	33.810612
866.335060	74969.498506	33.815629
866.752474	75101.771528	33.820647
868.255627	75229.476481	33.825664
868.971811	75354.257504	33.830682
869.641807	75488.609842	33.835700
870.536835	75619.023407	33.840717
871.442925	75747.266509	33.845735
872.548630	75877.558212	33.850752
873.066423	76008.732195	33.855770
874.531971	76126.841090	33.860788
874.710869	76263.967437	33.865805
875.828462	76395.354436	33.870823
876.654692	76524.772719	33.875840
877.239349	76662.998229	33.880858
878.815490	76791.332638	33.885876
879.562242	76921.803693	33.890893
880.361679	77045.853085	33.895911
881.228853	77167.444114	33.900928
881.964777	77298.633914	33.905946
882.874212	77429.928621	33.910964
883.993215	77570.810238	33.915981
884.916819	77682.900457	33.920999
886.130144	77808.466979	33.926016
886.738456	77944.887465	33.931034
887.534109	78061.909268	33.936052
888.334271	78190.538199	33.941069
889.275042	78311.756407	33.946087
890.474897	78430.218762	33.951104
891.106619	78555.240449	33.956122
892.295730	78657.145397	33.961140
893.008078	78766.922848	33.966157
893.908810	78890.991022	33.971175
894.625907	78993.905432	33.976192
895.353084	79118.414733	33.981210
896.234164	79239.584560	33.986228
896.941583	79350.928143	33.991245
898.085581	79474.453235	33.996263
899.031386	79607.051466	34.001280
899.388818	79732.669072	34.006298
900.748459	79854.946009	34.011316
901.202178	79991.119795	34.016333
902.014285	80122.357764	34.021351
902.954178	80252.170975	34.026368
903.649850	80399.554944	34.031386
904.542797	80522.614862	34.036404
905.213625	80663.735452	34.041421
906.560490	80808.414326	34.046439
907.491388	80945.248763	34.051456
908.451262	81098.458010	34.056474
909.284185	81231.558875	34.061492
910.296802	81377.005187	34.066509
911.352593	81527.335607	34.071527
912.525872	81658.756789	34.076544
913.096090	81795.763524	34.081562
913.856403	81938.414539	34.086580
914.947698	82077.228419	34.091597
915.648251	82215.222033	34.096615
917.015460	82367.771400	34.101632
917.292872	82515.560855	34.106650
918.629441	82651.958818	34.111668
919.145296	82800.919080	34.116685
920.152738	82954.790865	34.121703
921.331124	83098.297335	34.126720
922.087977	83253.471597	34.131738
923.168201	83394.161694	34.136756
923.656967	83546.440235	34.141773
924.672203	83691.514828	34.146791
925.914256	83840.247822	34.151808
926.278472	84009.481203	34.156826
927.376754	84162.055279	34.161844
928.743825	84313.212911	34.166861
929.591921	84459.332300	34.171879
930.691430	84611.364985	34.176896
931.121102	84770.260667	34.181914
932.360792	84916.482682	34.186932
933.554173	85069.559504	34.191949
934.174785	85222.365056	34.196967
935.534738	85364.843142	34.201984
936.412856	85531.585513	34.207002
937.393917	85677.994274	34.212020
938.399609	85824.526429	34.217037
939.143686	85973.064329	34.222055
940.095313	86122.011785	34.227072
941.112950	86277.650318	34.232090
942.346161	86426.439244	34.237108
943.039589	86570.382694	34.242125
943.992079	86731.369333	34.247143
945.189609	86866.998726	34.252160
945.491926	87019.159893	34.257178
946.218113	87175.460036	34.262196
947.673464	87331.646966	34.267213
948.253982	87479.961971	34.272231
949.299134	87636.484524	34.277248
950.225403	87799.343234	34.282266
951.319692	87951.183261	34.287284
952.312084	88090.916279	34.292301
952.927227	88243.558823	34.297319
954.232223	88363.579924	34.302336
954.743137	88517.507116	34.307354
955.751810	88660.746677	34.312372
956.977587	88807.596351	34.317389
957.798603	88957.798315	34.322407
958.553326	89106.474369	34.327424
959.325123	89265.362737	34.332442
960.596345	89419.885147	34.337460
961.269033	89580.317176	34.342477
962.432517	89726.132250	34.347495
963.382629	89878.729858	34.352512
964.311215	90037.654380	34.357530
964.815322	90198.346250	34.362548
966.056702	90362.796833	34.367565
966.815770	90528.929491	34.372583
967.788311	90689.597812	34.377600
968.980393	90858.787610	34.382618
969.955800	91021.951268	34.387636
970.759116	91181.366063	34.392653
971.725127	91357.261186	34.397671
972.892568	91519.174935	34.402688
973.700020	91689.826550	34.407706
974.869857	91860.723244	34.412724
975.983019	92025.136718	34.417741
977.107181	92184.764553	34.422759
978.374548	92353.376375	34.427776
979.041136	92521.658309	34.432794
979.856316	92683.460839	34.437812
981.009300	92846.689676	34.442829
981.893446	93021.243207	34.447847
983.010708	93181.049599	34.452864
983.718310	93356.501859	34.457882
984.852216	93527.916210	34.462900
986.094206	93707.896917	34.467917
987.081660	93871.425798	34.472935
988.085838	94031.275416	34.477952
989.002315	94194.115577	34.482970
989.928914	94370.254127	34.487988
991.017898	94540.442314	34.493005
992.180274	94719.405477	34.498023
993.206040	94879.636819	34.503040
994.358148	95060.712030	34.508058
995.205381	95217.063128	34.513076
996.546489	95383.240149	34.518093
997.079228	95555.907409	34.523111
998.191031	95721.675171	34.528128
999.362295	95893.352969	34.533146
1000.022038	96059.571213	34.538164
1001.340133	96228.365759	34.543181
1002.067185	96400.152148	34.548199
1003.191200	96573.216126	34.553216
1003.846970	96742.997260	34.558234
1004.772722	96924.655209	34.563252
1006.323462	97093.796961	34.568269
1006.967594	97272.091837	34.573287
1008.200287	97447.758413	34.578304
1009.194883	97620.983964	34.583322
1009.785150	97793.980019	34.588340
1010.874500	97961.595901	34.593357
1011.934087	98149.697935	34.598375
1013.026223	98327.552687	34.603392
1013.971986	98501.919250	34.608410
1015.256305	98680.536067	34.613428
1016.258581	98854.471541	34.618445
1016.918676	99034.314645	34.623463
1018.278675	99210.985393	34.628480
1019.400551	99382.910427	34.633498
1020.420076	99540.538827	34.638516
1021.792347	99683.345566	34.643533
1022.449374	99854.723857	34.648551
1023.471722	100020.218133	34.653568
1024.451742	100180.560468	34.658586
1025.260699	100336.709087	34.663604
1026.309248	100501.353744	34.668621
1026.907077	100686.746079	34.673639
1027.935017	100852.960262	34.678656
1028.947629	101029.333795	34.683674
1029.859693	101199.096026	34.688692
1031.046559	101380.324780	34.693709
1031.516097	101555.360767	34.698727
1032.531806	101739.754506	34.703744
1033.812400	101929.956284	34.708762
1034.733361	102123.422802	34.713780
1036.017036	102306.338960	34.718797
1036.784166	102501.017781	34.723815
1038.176929	102690.807688	34.728832
1039.064248	102872.324362	34.733850
1039.760044	103063.777224	34.738868
1041.218227	103256.599804	34.743885
1041.936974	103453.079379	34.748903
1043.335312	103642.039454	34.753920
1044.368261	103841.028182	34.758938
1045.404025	104026.859555	34.763956
1046.622627	104224.288094	34.768973
1047.359640	104423.456813	34.773991
1048.728081	104608.540741	34.779008
1049.498776	104812.443454	34.784026
1050.616859	105008.931968	34.789044
1052.005767	105207.973503	34.794061
1053.000209	105394.327959	34.799079
1054.262544	105589.847057	34.804096
1055.369781	105791.193959	34.809114
1056.455916	105985.377249	34.814132
1057.659427	106167.548315	34.819149
1058.501128	106362.534703	34.824167
1059.539887	106547.674028	34.829184
1060.707782	106745.902367	34.834202
1061.505808	106939.304302	34.839220
1063.200449	107134.066644	34.844237
1064.273271	107337.280143	34.849255
1064.947356	107535.431314	34.854272
1066.379196	107720.653092	34.859290
1066.833130	107922.415393	34.864308
1068.260712	108113.796423	34.869325
1069.247823	108314.802189	34.874343
1069.825694	108517.169107	34.879360
1071.187663	108710.933876	34.884378
1072.606981	108913.937313	34.889396
1073.611691	109114.718111	34.894413
1074.388860	109314.562656	34.899431
1075.271552	109513.707200	34.904448
1076.926096	109714.663669	34.909466
1077.223481	109929.437979	34.914484
1078.758965	110131.506590	34.919501
1079.753674	110340.848552	34.924519
1080.530135	110554.497165	34.929536
1081.649772	110760.312764	34.934554
1082.851309	110969.701340	34.939572
1083.921556	111163.645777	34.944589
1084.793465	111378.817828	34.949607
1085.855107	111584.699855	34.954624
1087.068444	111796.803727	34.959642
1088.084560	112009.587912	34.964660
1089.558977	112209.515623	34.969677
1090.461666	112418.305842	34.974695
1091.171994	112620.719167	34.979712
1092.325297	112812.001043	34.984730
1093.498596	113014.644738	34.989748
1094.801984	113213.493103	34.994765
1095.763250	113414.223764	34.999783
1096.652852	113621.960980	35.004800
1097.826946	113816.312190	35.009818
1098.749075	114028.468540	35.014836
1100.125877	114225.044177	35.019853
1100.809598	114435.431314	35.024871
1102.199192	114651.252533	35.029888
1103.368538	114869.316313	35.034906
1103.861687	115086.657372	35.039924
1105.116258	115290.444321	35.044941
1106.174184	115508.366741	35.049959
1107.172777	115730.177635	35.054976
1108.527325	115951.044512	35.059994
1109.391559	116175.034988	35.065012
1110.350250	116397.795269	35.070029
1111.393647	116613.156496	35.075047
1112.725769	116847.679940	35.080064
1114.109922	117081.550506	35.085082
1115.132005	117306.778129	35.090100
1116.611354	117523.163794	35.095117
1117.583398	117760.997926	35.100135
1118.745953	117979.834176	35.105152
1120.133662	118200.459487	35.110170
1121.034025	118434.826493	35.115188
1122.003746	118662.265452	35.120205
1123.153029	118889.549794	35.125223
1124.033228	119127.853831	35.130240
1125.531739	119357.478990	35.135258
1126.779674	119595.523314	35.140276
1128.378280	119819.838833	35.145293
1129.289306	120038.934915	35.150311
1130.167530	120283.343837	35.155328
1131.386554	120496.233870	35.160346
1132.371218	120734.850520	35.165364
1133.834758	120967.028492	35.170381
1135.209009	121195.826877	35.175399
1136.439342	121413.879293	35.180416
1137.714460	121624.689924	35.185434
1138.636367	121861.425171	35.190452
1139.906910	122077.752350	35.195469
1141.493529	122314.748827	35.200487
1142.256970	122534.939644	35.205504
1143.721198	122744.877870	35.210522
1144.821524	122977.258332	35.215540
1145.784814	123196.153674	35.220557
1147.403216	123419.606066	35.225575
1148.112204	123643.210459	35.230592
1149.482423	123855.770035	35.235610
1150.247760	124095.070840	35.240628
1151.609227	124311.209005	35.245645
1152.812744	124538.882552	35.250663
1153.981800	124758.502967	35.255680
1155.275619	124981.830471	35.260698
1156.198947	125211.938077	35.265716
1157.485388	125432.266371	35.270733
1158.717578	125654.620418	35.275751
1159.934390	125882.631348	35.280768
1160.819650	126091.877363	35.285786
1161.563504	126327.384284	35.290804
1162.889331	126560.198523	35.295821
1164.315146	126785.786122	35.300839
1165.184889	127020.111466	35.305856
1166.404547	127235.305125	35.310874
1167.741262	127463.168521	35.315892
1168.966303	127669.517218	35.320909
1170.043260	127879.326715	35.325927
1170.789310	128095.529915	35.330944
1172.170308	128299.550131	35.335962
1173.628676	128527.654727	35.340980
1174.601312	128735.421149	35.345997
1175.169375	128966.211203	35.351015
1176.140161	129192.373157	35.356032
1177.539644	129409.085850	35.361050
1178.880659	129649.057116	35.366068
1180.133858	129869.244976	35.371085
1181.345615	130107.200276	35.376103
1182.082797	130341.673836	35.381120
1183.573207	130563.449855	35.386138
1184.227417	130812.302711	35.391156
1185.279972	131039.592552	35.396173
1186.801544	131281.485815	35.401191
1187.668869	131538.802337	35.406208
1188.942181	131781.703843	35.411226
1189.876527	132036.731488	35.416244
1191.084462	132290.080618	35.421261
1192.664645	132538.565644	35.426279
1193.572598	132796.848972	35.431296
1195.076847	133044.006674	35.436314
1196.002445	133299.185193	35.441332
1196.977186	133560.125788	35.446349
1198.499294	133810.950134	35.451367
1199.321992	134085.256748	35.456384
1201.008348	134343.715285	35.461402
1202.355337	134605.566211	35.466420
1203.339579	134863.904033	35.471437
1204.554281	135115.930204	35.476455
1205.703108	135385.642398	35.481472
1207.343395	135640.784424	35.486490
1209.053018	135897.134072	35.491508
1210.048884	136159.854112	35.496525
1211.118768	136406.715933	35.501543
1211.794368	136671.635611	35.506560
1213.269362	136926.472518	35.511578
1214.739313	137183.594375	35.516596
1216.168045	137453.885657	35.521613
1217.878422	137700.258115	35.526631
1218.908217	137963.785494	35.531648
1220.354939	138210.015077	35.536666
1221.308989	138461.539052	35.541684
1222.403340	138717.555540	35.546701
1224.006320	138961.976981	35.551719
1224.886390	139225.970030	35.556736
1226.134659	139477.693805	35.561754
1227.294061	139744.345447	35.566772
1228.468943	140000.244141	35.571789
1230.184391	140258.667450	35.576807
1231.312162	140516.035962	35.581824
1232.614119	140768.254854	35.586842
1233.698071	141029.806188	35.591860
1234.808596	141290.619650	35.596877
1236.078126	141552.106211	35.601895
1237.211435	141811.436216	35.606912
1238.543943	142059.855314	35.611930
1240.005597	142321.189086	35.616948
1240.674296	142585.635851	35.621965
1242.182873	142848.994723	35.626983
1243.350587	143108.556907	35.632000
1244.751616	143362.071636	35.637018
1245.910600	143630.236833	35.642036
1247.077128	143892.848445	35.647053
1248.390564	144139.865084	35.652071
1249.412541	144394.147322	35.657088
1250.899844	144631.006206	35.662106
1252.040780	144881.937032	35.667124
1253.263750	145128.265302	35.672141
1254.521266	145369.415408	35.677159
1255.202391	145635.873860	35.682176
1256.830127	145889.927088	35.687194
1258.124740	146152.749703	35.692212
1258.927188	146398.953255	35.697229
1260.510641	146653.577177	35.702247
1261.751085	146914.588030	35.707264
1263.235176	147173.455210	35.712282
1264.819348	147430.836519	35.717300
1265.928926	147699.090924	35.722317
1267.038776	147952.648072	35.727335
1267.808570	148217.804447	35.732352
1269.421582	148487.795022	35.737370
1270.673948	148752.951576	35.742388
1271.590790	149024.037711	35.747405
1273.431401	149284.623740	35.752423
1274.400912	149565.826223	35.757440
1275.830040	149830.250982	35.762458
1276.724737	150111.406516	35.767476
1278.032317	150385.951247	35.772493
1279.308988	150654.326201	35.777511
1280.339335	150953.476250	35.782528
1282.067648	151235.199989	35.787546
1283.287033	151522.463988	35.792564
1284.693042	151810.244721	35.797581
1286.221321	152088.646603	35.802599
1287.361930	152369.194783	35.807616
1288.317376	152650.333724	35.812634
1289.893022	152928.366034	35.817652
1291.040930	153218.711493	35.822669
1292.871313	153490.832878	35.827687
1294.057709	153783.637005	35.832704
1295.562108	154056.957853	35.837722
1297.114474	154339.532570	35.842740
1298.120780	154619.117162	35.847757
1299.849834	154899.802052	35.852775
1300.678549	155183.441146	35.857792
1302.272553	155445.797005	35.862810
1303.588754	155734.357431	35.867828
1305.001795	156017.779090	35.872845
1306.432558	156295.060112	35.877863
1307.628162	156574.855600	35.882880
1308.594513	156852.547076	35.887898
1310.239039	157130.166451	35.892916
1311.286030	157414.343548	35.897933
1312.905654	157696.436335	35.902951
1314.186018	157980.832572	35.907968
1315.298721	158265.207773	35.912986
1316.913709	158555.680086	35.918004
1318.076803	158834.329505	35.923021
1319.710590	159116.252211	35.928039
1320.946064	159408.252234	35.933056
1322.183695	159672.293025	35.938074
1323.651852	159954.933933	35.943092
1324.702586	160241.071152	35.948109
1326.340144	160514.502771	35.953127
1327.699991	160796.824784	35.958144
1328.606184	161080.746110	35.963162
1330.061069	161364.312258	35.968180
1331.072484	161654.893436	35.973197
1332.486855	161933.306492	35.978215
1333.808690	162231.325760	35.983232
1335.227616	162509.145562	35.988250
1336.720032	162796.102653	35.993268
1337.581229	163076.048321	35.998285
1338.985135	163342.812569	36.003303
1340.112144	163616.107626	36.008320
1341.474837	163894.643567	36.013338
1342.793577	164164.814624	36.018356
1343.902363	164456.325032	36.023373
1345.066672	164735.812716	36.028391
1346.092671	165024.803032	36.033408
1347.479995	165318.227153	36.038426
1349.241442	165603.179124	36.043444
1350.321326	165901.872827	36.048461
1351.761467	166185.536718	36.053479
1352.971508	166489.668907	36.058496
1354.237182	166792.144477	36.063514
1355.745428	167087.654018	36.068532
1357.132762	167395.112912	36.073549
1358.537683	167694.310592	36.078567
1359.767417	168007.154418	36.083584
1361.215328	168310.219213	36.088602
1362.833584	168607.344781	36.093620
1363.833862	168915.258700	36.098637
1365.240796	169219.668715	36.103655
1366.705342	169538.727422	36.108672
1368.173697	169850.110622	36.113690
1369.475531	170150.420133	36.118708
1370.836852	170476.443573	36.123725
1372.225916	170786.856416	36.128743
1373.658623	171106.121579	36.133760
1374.868041	171420.134160	36.138778
1376.531532	171734.847897	36.143796
1377.755751	172070.765231	36.148813
1379.456728	172384.360398	36.153831
1380.689863	172699.012104	36.158848
1382.082247	173011.659895	36.163866
1383.392385	173329.894399	36.168884
1384.555164	173663.498128	36.173901
1386.336478	173977.483911	36.178919
1388.098063	174306.323026	36.183936
1388.771325	174623.414963	36.188954
1390.636093	174952.520607	36.193972
1391.723929	175282.442172	36.198989
1392.954098	175603.928331	36.204007
1394.316449	175940.002143	36.209024
1395.968871	176270.433519	36.214042
1397.289308	176605.503490	36.219060
1398.490076	176935.315912	36.224077
1399.838971	177259.103009	36.229095
1401.698081	177591.577686	36.234112
1403.094708	177943.866349	36.239130
1404.785243	178271.537883	36.244148
1406.245187	178596.076707	36.249165
1407.356085	178925.422010	36.254183
1409.056282	179251.676766	36.259200
1410.151745	179584.303353	36.264218
1412.104855	179898.336130	36.269236
1413.391709	180238.982053	36.274253
1414.584413	180566.115873	36.279271
1416.260031	180890.468485	36.284288
1417.945885	181218.438732	36.289306
1419.622073	181544.077209	36.294324
1420.996495	181867.292515	36.299341
1422.133845	182188.987771	36.304359
1424.131443	182510.479351	36.309376
1424.984246	182830.334276	36.314394
1426.387448	183157.626991	36.319412
1428.165159	183477.548693	36.324429
1429.566373	183795.237067	36.329447
1430.719556	184107.891061	36.334464
1432.321394	184418.721052	36.339482
1433.846140	184706.387789	36.344500
1435.176058	185024.475856	36.349517
1436.530339	185319.701049	36.354535
1437.930003	185631.624807	36.359552
1438.934927	185931.759841	36.364570
1440.594340	186251.552154	36.369588
1441.599512	186574.259674	36.374605
1443.106333	186878.302602	36.379623
1444.737655	187205.670372	36.384640
1445.989222	187534.029417	36.389658
1447.593882	187848.647984	36.394676
1448.420694	188176.458879	36.399693
1449.890871	188513.736617	36.404711
1451.563315	188836.943208	36.409728
1452.539265	189179.206380	36.414746
1454.212461	189512.660772	36.419764
1455.483681	189855.729596	36.424781
1456.873822	190197.574785	36.429799
1458.460407	190536.393579	36.434816
1459.698760	190891.482753	36.439834
1461.286411	191234.164443	36.444852
1462.919026	191579.963534	36.449869
1464.034319	191939.966639	36.454887
1465.818798	192293.463091	36.459904
1466.508692	192642.153339	36.464922
1468.333824	192999.976083	36.469940
1469.680504	193367.858250	36.474957
1471.158973	193732.775535	36.479975
1472.834521	194108.973795	36.484992
1474.002588	194485.181971	36.490010
1475.659574	194852.881871	36.495028
1477.170544	195225.521138	36.500045
1478.574899	195591.172263	36.505063
1480.459257	195964.668174	36.510080
1482.018545	196343.971062	36.515098
1483.645246	196707.750844	36.520116
1485.288041	197072.634507	36.525133
1486.790211	197432.947513	36.530151
1488.171780	197804.035835	36.535168
1489.533175	198178.443193	36.540186
1491.664523	198540.042044	36.545204
1493.164453	198906.952559	36.550221
1494.311192	199284.702469	36.555239
1496.007182	199638.723257	36.560256
1497.356653	200023.515528	36.565274
1499.270104	200381.008356	36.570292
1500.615733	200753.108882	36.575309
1502.141472	201124.064315	36.580327
1503.753000	201486.056411	36.585344
1505.187220	201859.290785	36.590362
1506.780338	202223.727404	36.595380
1508.199629	202589.261107	36.600397
1509.176902	202964.024104	36.605415
1510.956838	203332.142876	36.610432
1512.486377	203715.338079	36.615450
1513.972467	204080.258689	36.620468
1515.729033	204459.420632	36.625485
1516.843965	204829.027946	36.630503
1518.463184	205197.791905	36.635520
1520.121798	205583.730572	36.640538
1521.480194	205965.873474	36.645556
1523.122001	206342.435358	36.650573
1524.755958	206712.092924	36.655591
1526.479664	207095.450740	36.660608
1527.856859	207470.690405	36.665626
1529.516380	207832.235203	36.670644
1530.989132	208210.548073	36.675661
1532.337569	208568.642995	36.680679
1534.112382	208913.171253	36.685696
1535.370633	209270.204826	36.690714
1536.820040	209624.783050	36.695732
1538.566616	209985.929336	36.700749
1540.046746	210338.486527	36.705767
1541.520502	210698.512719	36.710784
1542.887823	211065.211847	36.715802
1544.151839	211422.609124	36.720820
1545.720452	211793.722462	36.725837
1547.195435	212165.462366	36.730855
1549.166834	212537.198015	36.735872
1550.331010	212919.176528	36.740890
1551.983939	213289.571107	36.745908
1553.392842	213658.712275	36.750925
1554.736323	214049.885080	36.755943
1556.427222	214425.459032	36.760960
1557.588785	214819.382665	36.765978
1559.139123	215206.792772	36.770996
1560.952029	215610.009181	36.776013
1562.623850	215997.504046	36.781031
1564.210123	216391.033885	36.786048
1565.448302	216795.289945	36.791066
1566.689047	217197.972576	36.796084
1568.571494	217594.760067	36.801101
1570.222570	218009.645483	36.806119
1572.037585	218410.130084	36.811136
1573.344387	218817.126019	36.816154
1574.865398	219227.415381	36.821172
1576.147839	219646.355904	36.826189
1577.335853	220064.500940	36.831207
1579.076768	220475.368419	36.836224
1580.919445	220907.022361	36.841242
1582.387335	221338.892333	36.846260
1584.042029	221755.798471	36.851277
1585.549369	222187.792243	36.856295
1587.106206	222614.140856	36.861312
1588.551137	223041.804925	36.866330
1590.356854	223493.997684	36.871348
1592.231477	223913.542350	36.876365
1593.778464	224351.049404	36.881383
1595.643648	224804.024753	36.886400
1596.866913	225282.152112	36.891418
1598.322277	225712.465660	36.896436
1600.278485	226150.038571	36.901453
1602.263182	226589.284703	36.906471
1604.236140	227010.500131	36.911488
1605.353174	227441.891446	36.916506
1607.186665	227877.814091	36.921524
1608.749162	228299.584070	36.926541
1610.143992	228739.290450	36.931559
1612.063821	229171.672333	36.936576
1613.588873	229604.628792	36.941594
1615.524649	230035.410464	36.946612
1617.268123	230458.935154	36.951629
1618.623194	230896.114739	36.956647
1620.260253	231316.458970	36.961664
1621.910276	231748.105717	36.966682
1624.171304	232174.699527	36.971700
1625.615453	232594.748939	36.976717
1626.809564	233026.296755	36.981735
1628.770725	233456.931581	36.986752
1630.537932	233874.111434	36.991770
1631.838575	234298.431024	36.996788
1633.683106	234732.898658	37.001805
1635.259924	235164.465030	37.006823
1636.886667	235577.633414	37.011840
1638.529192	236008.149531	37.016858
1640.101129	236419.652394	37.021876
1641.758945	236812.903466	37.026893
1643.155415	237230.533547	37.031911
1645.052486	237633.577331	37.036928
1646.630723	238042.237654	37.041946
1648.099104	238454.168425	37.046964
1649.858277	238862.851331	37.051981
1651.065676	239283.768418	37.056999
1652.760261	239691.828554	37.062016
1653.777266	240127.283406	37.067034
1655.306924	240547.692472	37.072052
1657.016947	240981.053123	37.077069
1658.375137	241431.162074	37.082087
1660.087408	241866.022724	37.087104
1661.779583	242307.161880	37.092122
1663.239480	242755.300472	37.097140
1664.853581	243218.147863	37.102157
1666.541017	243673.490171	37.107175
1668.406382	244124.739418	37.112192
1669.980540	244576.240708	37.117210
1671.444923	245040.258977	37.122228
1673.625703	245506.471273	37.127245
1675.007232	245963.696676	37.132263
1676.897861	246433.641665	37.137280
1678.337737	246893.907058	37.142298
1679.831543	247378.754172	37.147316
1681.681890	247839.486439	37.152333
1683.537199	248322.217426	37.157351
1685.513861	248792.913327	37.162368
1687.440852	249258.740578	37.167386
1688.850001	249732.071555	37.172404
1690.806379	250199.749349	37.177421
1692.491560	250679.386445	37.182439
1694.346691	251146.827811	37.187456
1696.121255	251616.594569	37.192474
1697.742432	252092.687025	37.197492
1699.597901	252560.027843	37.202509
1700.807736	253034.461509	37.207527
1702.976553	253508.000384	37.212544
1704.943026	253993.969741	37.217562
1706.474438	254469.900727	37.222580
1708.068691	254947.803014	37.227597
1709.732365	255434.483569	37.232615
1711.425867	255907.238379	37.237632
1713.124132	256377.934880	37.242650
1715.216824	256865.510349	37.247668
1717.039922	257333.849341	37.252685
1718.722262	257819.257264	37.257703
1720.274861	258295.084210	37.262720
1722.386504	258787.483400	37.267738
1724.004511	259262.537444	37.272756
1725.832013	259736.108859	37.277773
1727.726271	260216.121620	37.282791
1729.355583	260696.000225	37.287808
1731.290869	261167.521298	37.292826
1732.527913	261651.147902	37.297844
1734.689617	262119.811501	37.302861
1736.560375	262605.085884	37.307879
1737.923319	263077.539062	37.312896
1740.049566	263553.625598	37.317914
1741.547513	264034.108773	37.322932
1743.530240	264509.227705	37.327949
1745.151227	264992.509668	37.332967
1746.979902	265461.759821	37.337984
1748.659775	265935.632146	37.343002
1749.975092	266414.111434	37.348020
1751.848800	266895.241588	37.353037
1753.569282	267370.833307	37.358055
1755.615860	267827.292997	37.363072
1757.191016	268286.268765	37.368090
1758.805971	268750.241845	37.373108
1760.589583	269211.722446	37.378125
1762.025845	269673.437680	37.383143
1763.784796	270139.976393	37.388160
1765.704813	270598.435182	37.393178
1767.045382	271073.754913	37.398196
1769.148441	271541.301781	37.403213
1770.189500	272021.826337	37.408231
1772.106770	272493.289068	37.413248
1773.771131	272983.717792	37.418266
1775.526100	273469.177191	37.423284
1777.090479	273964.548806	37.428301
1778.767026	274458.249807	37.433319
1780.428936	274957.718636	37.438336
1782.480327	275461.516755	37.443354
1783.938445	275967.291582	37.448372
1785.963537	276465.300182	37.453389
1787.327572	276992.756470	37.458407
1788.949998	277503.860624	37.463424
1791.481717	278019.893817	37.468442
1792.875521	278542.997631	37.473460
1794.793904	279060.577443	37.478477
1796.538323	279592.892357	37.483495
1798.684862	280112.870303	37.488512
1800.495221	280623.960913	37.493530
1802.152471	281158.698996	37.498548
1804.169265	281687.330526	37.503565
1805.729524	282213.571919	37.508583
1807.350876	282742.290964	37.513600
1808.844122	283282.129924	37.518618
1811.151387	283835.803410	37.523636
1813.091837	284369.138389	37.528653
1814.980995	284907.966688	37.533671
1816.608293	285443.331015	37.538688
1818.561695	285985.497859	37.543706
1820.628131	286523.148109	37.548724
1822.585942	287074.403733	37.553741
1824.300284	287612.692296	37.558759
1826.093709	288154.572619	37.563776
1827.968223	288691.890738	37.568794
1829.990745	289240.028244	37.573812
1831.805295	289777.631325	37.578829
1833.583801	290334.694677	37.583847
1835.247922	290872.953063	37.588864
1837.354405	291426.223671	37.593882
1839.000951	291969.255439	37.598900
1840.883943	292521.338847	37.603917
1843.053381	293073.042221	37.608935
1844.964005	293621.077438	37.613952
1846.748424	294170.908873	37.618970
1848.357594	294719.115662	37.623988
1850.649918	295260.374612	37.629005
1852.561205	295805.478303	37.634023
1854.413437	296356.125987	37.639040
1856.245119	296904.005796	37.644058
1858.106124	297446.722029	37.649076
1860.154749	297990.318817	37.654093
1861.721958	298544.786544	37.659111
1863.368380	299098.400039	37.664128
1865.847764	299641.662920	37.669146
1867.506475	300195.242919	37.674164
1869.476052	300743.841289	37.679181
1871.110522	301293.177624	37.684199
1872.875768	301844.140042	37.689216
1874.510774	302391.844492	37.694234
1876.498521	302948.554266	37.699252
1878.624671	303474.228045	37.704269
1880.491822	303996.665355	37.709287
1881.889854	304528.700870	37.714304
1884.037515	305054.895179	37.719322
1885.546718	305590.766218	37.724340
1887.543953	306126.578755	37.729357
1889.281276	306653.212079	37.734375
1891.681671	307189.408500	37.739392
1893.804499	307719.831694	37.744410
1895.386964	308252.702523	37.749428
1897.325581	308783.352471	37.754445
1899.195210	309327.114316	37.759463
1900.854779	309876.824233	37.764480
1902.769260	310419.606230	37.769498
1904.280406	310979.770313	37.774516
1906.408191	311534.038580	37.779533
1908.231652	312100.847153	37.784551
1909.765263	312662.925263	37.789568
1911.714514	313230.212508	37.794586
1913.056240	313812.400353	37.799604
1915.123920	314376.891359	37.804621
1917.000860	314972.033959	37.809639
1918.810899	315555.857344	37.814656
1920.938957	316140.842320	37.819674
1922.488092	316744.530970	37.824692
1923.885125	317340.063136	37.829709
1926.230378	317943.356034	37.834727
1927.753484	318552.060949	37.839744
1930.197220	319159.872038	37.844762
1931.889340	319781.437065	37.849780
1934.075344	320402.737007	37.854797
1935.712759	321009.978798	37.859815
1937.341943	321649.208882	37.864832
1939.688599	322267.519215	37.869850
1941.450595	322900.748131	37.874868
1943.543776	323519.494419	37.879885
1945.553943	324159.271178	37.884903
1947.530395	324792.496392	37.889920
1949.950377	325408.453236	37.894938
1951.688038	326046.097300	37.899956
1953.581629	326686.171613	37.904973
1955.710113	327319.980095	37.909991
1957.646351	327957.977235	37.915008
1959.837455	328587.293432	37.920026
1961.825239	329220.546120	37.925044
1963.620152	329864.080255	37.930061
1965.857791	330494.611965	37.935079
1967.452481	331146.770933	37.940096
1969.628268	331776.308450	37.945114
1971.707266	332423.447570	37.950132
1973.694674	333055.210286	37.955149
1975.857723	333695.491712	37.960167
1977.788494	334339.332515	37.965184
1980.053385	334973.159474	37.970202
1982.107331	335610.618382	37.975220
1984.140368	336245.229999	37.980237
1986.301368	336868.542218	37.985255
1988.147455	337517.866724	37.990272
1990.336635	338150.957069	37.995290
1992.246614	338780.836628	38.000308
1994.024206	339422.787151	38.005325
1996.413463	340060.034258	38.010343
1998.212720	340696.203071	38.015360
2000.142878	341317.519033	38.020378
2002.113310	341960.902570	38.025396
2004.096429	342596.813434	38.030413
2006.452719	343241.106226	38.035431
2008.155936	343868.696218	38.040448
2010.322966	344478.714340	38.045466
2012.056146	345083.745623	38.050484
2013.999421	345698.175698	38.055501
2016.198118	346314.357467	38.060519
2017.958626	346924.918507	38.065536
2019.867454	347531.462527	38.070554
2021.893551	348158.687884	38.075572
2023.847919	348775.181546	38.080589
2025.931587	349406.643636	38.085607
2027.411562	350028.375498	38.090624
2029.622887	350658.377707	38.095642
2031.469771	351302.616609	38.100660
2033.181263	351929.891753	38.105677
2035.481079	352580.711017	38.110695
2037.564805	353230.211285	38.115712
2039.659672	353875.233906	38.120730
2041.814518	354527.189551	38.125748
2043.852067	355183.924913	38.130765
2045.742617	355833.036781	38.135783
2047.436793	356493.868184	38.140800
2049.555538	357153.654823	38.145818
2051.724941	357826.108894	38.150836
2053.398370	358493.635497	38.155853
2056.108113	359167.094698	38.160871
2057.947631	359844.720412	38.165888
2060.007415	360514.661687	38.170906
2061.948130	361196.966838	38.175924
2063.807521	361894.267413	38.180941
2066.135749	362565.753433	38.185959
2068.103858	363264.102646	38.190976
2070.227855	363950.845439	38.195994
2072.406013	364637.693929	38.201012
2074.335558	365337.458038	38.206029
2076.592580	366030.559731	38.211047
2078.813578	366728.322205	38.216064
2081.100810	367430.677503	38.221082
2082.997816	368126.006930	38.226100
2084.686194	368821.433886	38.231117
2087.205918	369535.708891	38.236135
2088.941227	370242.160394	38.241152
2091.324237	370951.890063	38.246170
2093.411631	371663.911978	38.251188
2095.595031	372373.621290	38.256205
2097.738950	373077.794013	38.261223
2099.352422	373799.083611	38.266240
2101.917481	374515.763141	38.271258
2104.120989	375226.882950	38.276276
2106.127832	375947.404089	38.281293
2108.463503	376661.744238	38.286311
2110.243678	377383.135105	38.291328
2112.545129	378094.357271	38.296346
2114.817272	378819.034678	38.301364
2116.675236	379542.801340	38.306381
2119.005101	380259.526654	38.311399
2121.251095	380978.202911	38.316416
2123.488796	381708.452742	38.321434
2125.613995	382418.927666	38.326452
2127.705094	383155.356380	38.331469
2129.867861	383863.942838	38.336487
2132.298406	384594.552860	38.341504
2134.399981	385300.658641	38.346522
2136.275598	386022.682362	38.351540
2138.375386	386744.196404	38.356557
2140.761303	387467.142553	38.361575
2142.863223	388201.856528	38.366592
2144.857591	388911.930445	38.371610
2147.361033	389634.224192	38.376628
2149.229567	390345.629695	38.381645
2151.642818	391036.269710	38.386663
2153.445729	391731.760373	38.391680
2155.633206	392407.932931	38.396698
2157.917318	393109.091947	38.401716
2159.667823	393807.458628	38.406733
2161.953815	394498.446454	38.411751
2163.979128	395210.244398	38.416768
2166.024958	395899.085071	38.421786
2168.177914	396608.091194	38.426804
2170.039965	397320.828391	38.431821
2172.069030	398029.161722	38.436839
2174.302826	398753.029455	38.441856
2176.090304	399478.549292	38.446874
2178.161748	400207.171611	38.451892
2180.126955	400945.396894	38.456909
2182.597323	401689.829244	38.461927
2184.634831	402433.350636	38.466944
2186.788896	403174.932846	38.471962
2189.341203	403930.188022	38.476980
2191.173372	404679.232770	38.481997
2193.969289	405422.752336	38.487015
2195.846178	406175.980404	38.492032
2198.156035	406938.692931	38.497050
2200.773893	407689.755698	38.502068
2202.714419	408450.966885	38.507085
2205.158077	409207.995084	38.512103
2207.316023	409970.976845	38.517120
2209.420246	410731.285986	38.522138
2211.809624	411501.734577	38.527156
2213.835221	412273.158045	38.532173
2215.922869	413048.322756	38.537191
2218.155875	413823.693889	38.542208
2220.033915	414602.899731	38.547226
2222.741950	415381.742626	38.552244
2224.583218	416177.572220	38.557261
2227.077906	416962.582148	38.562279
2229.393405	417766.185690	38.567296
2231.341300	418551.110431	38.572314
2233.875745	419344.219949	38.577332
2235.834232	420141.172569	38.582349
2238.242015	420932.986819	38.587367
2240.526192	421728.265261	38.592384
2243.088779	422534.461002	38.597402
2245.471063	423332.380988	38.602420
2247.178821	424136.057642	38.607437
2249.257805	424938.785876	38.612455
2251.872016	425747.222073	38.617472
2254.128179	426567.132965	38.622490
2256.599879	427368.450181	38.627508
2258.669033	428181.704527	38.632525
2260.753019	428993.156851	38.637543
2262.882111	429812.876365	38.642560
2265.116468	430628.702828	38.647578
2267.828079	431447.459489	38.652596
2270.098272	432266.361629	38.657613
2272.748948	433091.904263	38.662631
2274.836565	433915.435241	38.667648
2277.160414	434711.769175	38.672666
2279.289864	435529.921168	38.677684
2281.636764	436355.650086	38.682701
2284.035740	437170.054932	38.687719
2286.942433	437983.132188	38.692736
2289.046607	438790.594312	38.697754
2291.168814	439601.516002	38.702772
2293.009920	440429.507050	38.707789
2295.448498	441245.123836	38.712807
2297.796031	442056.121316	38.717824
2299.956526	442874.354915	38.722842
2302.302072	443679.272113	38.727860
2304.611018	444466.610569	38.732877
2306.664737	445255.480343	38.737895
2308.747770	446038.802525	38.742912
2310.887116	446837.616787	38.747930
2313.492965	447632.328248	38.752948
2315.386302	448436.940656	38.757965
2317.378290	449240.039577	38.762983
2319.758898	450061.150899	38.768000
2321.882040	450874.939253	38.773018
2324.181546	451700.096752	38.778036
2325.902228	452541.652022	38.783053
2328.424930	453371.258154	38.788071
2330.867054	454222.740347	38.793088
2332.789562	455058.951731	38.798106
2335.220974	455915.472925	38.803124
2337.545194	456773.442270	38.808141
2339.571036	457629.655163	38.813159
2342.118844	458502.278071	38.818176
2344.340011	459370.670562	38.823194
2346.656332	460238.201020	38.828212
2348.447333	461140.104557	38.833229
2350.642065	462015.160547	38.838247
2353.130294	462928.494109	38.843264
2355.470486	463839.383779	38.848282
2357.937553	464732.268097	38.853300
2360.224956	465635.350270	38.858317
2362.736805	466552.099593	38.863335
2365.157032	467470.387297	38.868352
2366.885148	468391.726950	38.873370
2369.735819	469316.626960	38.878388
2371.661801	470251.032913	38.883405
2374.253079	471184.676988	38.888423
2376.581155	472131.454301	38.893440
2378.914256	473082.174374	38.898458
2381.343415	474026.414866	38.903476
2384.134086	474983.984912	38.908493
2386.397618	475937.097171	38.913511
2389.257586	476884.506026	38.918528
2391.413703	477842.740320	38.923546
2394.337001	478794.535586	38.928564
2396.487250	479748.529960	38.933581
2399.181564	480689.810432	38.938599
2401.551146	481648.062330	38.943616
2404.136306	482605.520909	38.948634
2406.717877	483552.477519	38.953652
2408.962878	484494.340281	38.958669
2411.217392	485444.835199	38.963687
2414.041541	486398.819983	38.968704
2416.393680	487353.840747	38.973722
2419.019393	488302.606326	38.978740
2421.359211	489262.522554	38.983757
2424.043254	490204.966922	38.988775
2426.723631	491153.215166	38.993792
2428.976557	492114.552693	38.998810
2431.603873	493055.791328	39.003828
2434.232277	494012.620916	39.008845
2436.431218	494956.096474	39.013863
2438.985448	495898.401543	39.018880
2441.156554	496862.008210	39.023898
2444.224247	497799.279221	39.028916
2446.534766	498751.555018	39.033933
2448.839194	499699.691714	39.038951
2451.520515	500639.389584	39.043968
2453.782305	501579.910484	39.048986
2456.291985	502521.295254	39.054004
2458.721157	503473.684116	39.059021
2461.068080	504411.860667	39.064039
2463.782182	505321.230208	39.069056
2465.982697	506242.584038	39.074074
2468.392546	507146.506279	39.079092
2471.113240	508070.090424	39.084109
2473.155374	508970.139325	39.089127
2475.428444	509891.272668	39.094144
2477.470979	510808.963094	39.099162
2480.634082	511733.825428	39.104180
2482.717638	512665.112294	39.109197
2485.020749	513583.909540	39.114215
2488.066034	514523.697548	39.119232
2490.173682	515466.607531	39.124250
2492.547201	516408.156921	39.129268
2494.881719	517359.481425	39.134285
2497.130470	518308.040869	39.139303
2499.300200	519270.813132	39.144320
2501.796926	520238.257137	39.149338
2504.494115	521195.481472	39.154356
2506.730874	522188.234197	39.159373
2508.947925	523170.750790	39.164391
2511.575655	524154.747571	39.169408
2513.887927	525155.402143	39.174426
2516.744090	526148.447192	39.179444
2519.444522	527158.421881	39.184461
2521.880683	528160.113959	39.189479
2524.156779	529162.922886	39.194496
2526.246513	530181.251295	39.199514
2529.109905	531188.558179	39.204532
2531.559778	532218.365408	39.209549
2534.461965	533257.941429	39.214567
2536.926320	534277.634608	39.219584
2539.146431	535313.552236	39.224602
2542.123260	536347.861681	39.229620
2544.480881	537385.671038	39.234637
2546.776315	538432.573173	39.239655
2549.542074	539473.031835	39.244672
2552.133918	540521.794427	39.249690
2554.613219	541567.831754	39.254708
2557.470585	542624.141675	39.259725
2559.989422	543687.067413	39.264743
2562.305099	544735.511535	39.269760
2564.947059	545808.716813	39.274778
2567.695991	546869.300205	39.279796
2570.286052	547924.599135	39.284813
2572.970267	548987.997220	39.289831
2575.809782	550050.131034	39.294848
2578.095164	551126.802130	39.299866
2580.827671	552183.559481	39.304884
2583.463321	553264.025021	39.309901
2586.231910	554336.290617	39.314919
2588.998850	555397.214015	39.319936
2591.446776	556472.829766	39.324954
2594.249788	557534.532740	39.329972
2596.947008	558610.789287	39.334989
2598.947763	559683.456246	39.340007
2601.958494	560758.833465	39.345024
2604.498182	561835.506593	39.350042
2607.406560	562902.336839	39.355060
2610.103052	563992.619130	39.360077
2612.222392	565052.071322	39.365095
2615.234039	566129.467417	39.370112
2617.431272	567214.791048	39.375130
2620.439452	568292.609661	39.380148
2622.654354	569373.028893	39.385165
2625.504469	570457.318067	39.390183
2628.344709	571532.682624	39.395200
2630.884115	572617.441201	39.400218
2633.146708	573674.852053	39.405236
2635.942351	574721.297506	39.410253
2638.304981	575785.640081	39.415271
2641.175632	576838.720373	39.420288
2643.441095	577883.333228	39.425306
2645.714395	578922.138364	39.430324
2648.623789	579983.724388	39.435341
2651.201838	581050.790784	39.440359
2654.114230	582103.165811	39.445376
2656.391384	583179.073806	39.450394
2658.926589	584245.818962	39.455412
2661.464927	585325.405537	39.460429
2664.088138	586397.412228	39.465447
2666.523052	587478.728903	39.470464
2668.862236	588567.532994	39.475482
2671.696729	589669.187627	39.480500
2674.480144	590779.268680	39.485517
2677.140300	591896.733025	39.490535
2679.734709	593001.226032	39.495552
2682.276000	594131.326235	39.500570
2685.029362	595255.371867	39.505588
2687.865706	596377.492997	39.510605
2690.275256	597516.305672	39.515623
2692.599215	598644.955002	39.520640
2695.229464	599791.972419	39.525658
2697.833516	600943.587253	39.530676
2701.047403	602100.243533	39.535693
2703.195335	603271.026415	39.540711
2706.211238	604437.291769	39.545728
2709.124813	605610.662154	39.550746
2711.616063	606771.169467	39.555764
2714.502486	607948.256345	39.560781
2716.826687	609145.877710	39.565799
2719.935568	610316.276111	39.570816
2722.600186	611503.283797	39.575834
2724.979417	612704.217816	39.580852
2728.299356	613892.313652	39.585869
2731.316024	615087.883490	39.590887
2733.945634	616282.587756	39.595904
2736.669028	617477.846898	39.600922
2739.299973	618683.039495	39.605940
2742.316442	619881.437416	39.610957
2744.898770	621086.522534	39.615975
2747.660219	622292.793660	39.620992
2750.541613	623506.555864	39.626010
2753.103189	624703.945732	39.631028
2755.932969	625927.336227	39.636045
2758.743133	627151.189512	39.641063
2761.516874	628369.014545	39.646080
2763.918421	629600.145663	39.651098
2766.727439	630809.644015	39.656116
2769.640813	632047.196869	39.661133
2772.134065	633280.779218	39.666151
2775.412240	634502.455914	39.671168
2778.323428	635738.125356	39.676186
2780.843286	636975.159784	39.681204
2783.735758	638207.593869	39.686221
2786.420010	639448.497019	39.691239
2788.873093	640677.465106	39.696256
2792.000073	641943.137538	39.701274
2794.706903	643169.918846	39.706292
2797.995840	644410.769070	39.711309
2800.665665	645645.635791	39.716327
2803.165831	646900.272960	39.721344
2805.730880	648138.142600	39.726362
2808.791112	649389.435633	39.731380
2811.868389	650626.215640	39.736397
2814.623457	651879.589429	39.741415
2817.528272	653114.045548	39.746432
2819.626939	654347.783208	39.751450
2822.695764	655534.181787	39.756468
2825.726058	656741.263570	39.761485
2828.373047	657949.704186	39.766503
2831.242520	659152.530871	39.771520
2833.880176	660370.433164	39.776538
2836.609099	661580.301763	39.781556
2839.468012	662803.487318	39.786573
2842.042749	664026.116617	39.791591
2845.543626	665256.648848	39.796608
2848.116552	666465.829624	39.801626
2850.782947	667695.787476	39.806644
2853.699699	668929.077004	39.811661
2856.145419	670185.511955	39.816679
2858.937759	671428.145812	39.821696
2862.026503	672691.700358	39.826714
2864.507865	673946.185851	39.831732
2868.005283	675206.301140	39.836749
2870.594727	676469.775851	39.841767
2873.038808	677735.090764	39.846784
2876.419105	679014.588590	39.851802
2879.127230	680297.398512	39.856820
2882.189022	681567.998863	39.861837
2884.745856	682864.484514	39.866855
2887.727362	684158.729708	39.871872
2890.674186	685452.548461	39.876890
2893.302340	686756.860481	39.881908
2896.536754	688065.203466	39.886925
2899.462659	689389.588665	39.891943
2902.251096	690697.821100	39.896960
2904.821105	692006.692420	39.901978
2907.954439	693336.166301	39.906996
2911.148023	694667.515029	39.912013
2913.824739	695997.360297	39.917031
2916.789996	697330.330071	39.922048
2919.918820	698666.789890	39.927066
2922.660797	700011.736210	39.932084
2925.448808	701344.522159	39.937101
2928.437980	702697.242437	39.942119
2931.216991	704046.962220	39.947136
2934.413895	705396.154984	39.952154
2936.949482	706762.831636	39.957172
2940.497593	708122.883451	39.962189
2943.322692	709493.188653	39.967207
2946.149261	710836.684867	39.972224
2948.944497	712214.281851	39.977242
2951.574284	713586.534657	39.982260
2954.938872	714955.523720	39.987277
2957.923668	716339.246968	39.992295
2961.037854	717717.080905	39.997312
2964.191156	719098.144136	40.002330
2966.846690	720484.550503	40.007348
2969.744749	721862.576065	40.012365
2972.843149	723250.672496	40.017383
2976.192240	724630.239040	40.022400
2978.783218	726013.356662	40.027418
2981.500470	727410.254290	40.032436
2984.902474	728786.049298	40.037453
2988.139928	730186.140911	40.042471
2991.109561	731571.712061	40.047488
2994.103660	732954.770384	40.052506
2996.707820	734342.099444	40.057524
2999.791054	735728.912673	40.062541
3003.174048	737135.919285	40.067559
3005.852105	738523.548661	40.072576
3009.319777	739917.713417	40.077594
3012.024787	741314.768012	40.082612
3015.043141	742688.540277	40.087629
3018.341672	744049.501373	40.092647
3021.201892	745398.416530	40.097664
3024.303298	746740.306007	40.102682
3027.018932	748084.591365	40.107700
3029.919009	749428.367716	40.112717
3032.775919	750780.294409	40.117735
3035.906286	752123.614409	40.122752
3039.186001	753484.702414	40.127770
3041.974556	754847.255363	40.132788
3044.956732	756205.989068	40.137805
3047.878871	757584.132458	40.142823
3050.459119	758959.031187	40.147840
3053.876825	760340.973324	40.152858
3056.780804	761725.355234	40.157876
3059.704114	763114.202105	40.162893
3062.789636	764523.618655	40.167911
3065.723345	765913.519463	40.172928
3068.673271	767325.774036	40.177946
3071.574785	768747.451973	40.182964
3074.884685	770173.360630	40.187981
3077.911088	771591.032103	40.192999
3080.956984	773025.130388	40.198016
3083.950966	774463.230425	40.203034
3086.833664	775907.499348	40.208052
3090.145139	777357.352545	40.213069
3093.081942	778812.868998	40.218087
3096.105647	780270.140275	40.223104
3099.234285	781732.743183	40.228122
3102.148205	783208.329905	40.233140
3105.280421	784686.569341	40.238157
3108.753309	786181.070666	40.243175
3111.405835	787664.167217	40.248192
3114.713546	789141.258715	40.253210
3117.630887	790641.531369	40.258228
3120.892757	792139.566854	40.263245
3124.248140	793642.068714	40.268263
3127.363720	795148.696095	40.273280
3130.889441	796649.986074	40.278298
3133.949622	798164.393631	40.283316
3136.933641	799665.856638	40.288333
3140.405064	801176.993748	40.293351
3143.283413	802696.361113	40.298368
3146.661458	804201.273481	40.303386
3150.023864	805742.385864	40.308404
3153.191101	807259.618902	40.313421
3156.525909	808779.076937	40.318439
3159.490709	810298.842359	40.323456
3163.154669	811814.291752	40.328474
3165.974331	813332.372826	40.333492
3169.531588	814851.698811	40.338509
3172.777008	816368.388303	40.343527
3175.880916	817894.030901	40.348544
3179.033303	819407.506411	40.353562
3182.272043	820945.456045	40.358580
3185.379832	822464.631920	40.363597
3188.594197	823992.608297	40.368615
3191.477038	825517.115071	40.373632
3195.235386	827042.000237	40.378650
3198.172707	828578.896354	40.383668
3201.802529	830110.443474	40.388685
3204.771392	831637.549037	40.393703
3207.579603	833160.570837	40.398720
3210.932430	834691.517104	40.403738
3213.871403	836227.180312	40.408756
3217.200298	837755.939023	40.413773
3220.226916	839298.003784	40.418791
3223.407208	840845.554953	40.423808
3226.719953	842372.186153	40.428826
3229.574911	843872.077387	40.433844
3232.498322	845389.097997	40.438861
3235.860139	846889.936294	40.443879
3239.248884	848397.309073	40.448896
3242.551107	849896.949823	40.453914
3245.824540	851399.341784	40.458932
3248.809731	852904.427421	40.463949
3251.942014	854418.829477	40.468967
3254.692271	855937.386708	40.473984
3257.911047	857468.104263	40.479002
3260.838211	859014.394783	40.484020
3264.190195	860545.678550	40.489037
3267.679546	862103.990351	40.494055
3270.564919	863658.318806	40.499072
3273.658850	865226.845032	40.504090
3276.988057	866807.517880	40.509108
3280.013577	868375.138743	40.514125
3283.592090	869962.493831	40.519143
3286.796586	871548.617792	40.524160
3289.930573	873150.878289	40.529178
3293.124860	874771.947970	40.534196
3296.323877	876373.616892	40.539213
3299.568590	877980.741449	40.544231
3302.691153	879613.545526	40.549248
3306.170074	881244.096646	40.554266
3309.677169	882901.141417	40.559284
3312.726836	884550.063669	40.564301
3315.901558	886193.283071	40.569319
3319.203730	887852.906513	40.574336
3322.509282	889509.832289	40.579354
3325.856246	891190.776525	40.584372
3329.271810	892868.226515	40.589389
3332.395373	894546.677895	40.594407
3335.427434	896229.082870	40.599424
3338.704437	897919.234870	40.604442
3342.004753	899623.711726	40.609460
3344.962316	901330.810796	40.614477
3348.654535	903042.660712	40.619495
3351.856211	904780.436592	40.624512
3355.329168	906485.781779	40.629530
3358.706462	908219.953521	40.634548
3361.973442	909948.793142	40.639565
3365.646045	911677.505078	40.644583
3369.304742	913417.686887	40.649600
3372.829360	915143.602458	40.654618
3375.868013	916883.168734	40.659636
3379.285472	918633.636344	40.664653
3382.917245	920367.382194	40.669671
3386.224835	922111.658039	40.674688
3390.001163	923849.538199	40.679706
3392.990914	925601.366409	40.684724
3396.389960	927353.800030	40.689741
3399.790120	929098.185022	40.694759
3403.520165	930868.090434	40.699776
3406.905559	932606.823527	40.704794
3410.355473	934364.594838	40.709812
3413.778747	936113.363826	40.714829
3417.232988	937873.692304	40.719847
3420.615740	939626.173216	40.724864
3424.469548	941367.281877	40.729882
3427.776490	943130.351811	40.734900
3430.972553	944884.625009	40.739917
3434.804891	946623.587508	40.744935
3438.097153	948371.882837	40.749952
3441.469588	950121.381734	40.754970
3444.864073	951887.161834	40.759988
3448.475498	953659.746052	40.765005
3452.188392	955423.006432	40.770010
3455.366824	957146.115993	40.775015
3458.751655	958815.752880	40.780020
3461.947684	960414.783563	40.785024
3465.109053	961945.885760	40.790029
3468.662046	963385.344039	40.795034
3471.388456	964775.135698	40.800039
3474.016929	966067.017663	40.805044
3476.973468	967308.645053	40.810048
3479.416142	968476.021706	40.815053
3482.063196	969554.400769	40.820058
3484.847998	970577.097825	40.825063
3487.230335	971508.342194	40.830068
3489.554537	972384.592403	40.835072
3491.597045	973182.447408	40.840077
3494.216992	973905.512923	40.845082
3495.598038	974586.956785	40.850087
3497.319402	975186.171962	40.855092
3498.992982	975748.003668	40.860096
3500.435138	976255.882422	40.865101
3502.294583	976692.715457	40.870106
3503.863909	977106.018232	40.875111
3505.281525	977452.105846	40.880116
3506.504762	977755.418768	40.885120
3507.501388	978019.680970	40.890125
3508.639212	978233.116113	40.895130
3510.019812	978431.070943	40.900135
3511.262045	978578.839226	40.905140
3512.176245	978696.087528	40.910144
3513.070299	978771.632954	40.915149
3514.078713	978817.077328	40.920154
3514.810183	978835.318156	40.925159
3515.368054	978810.321371	40.930164
3515.963313	978775.746938	40.935168
3516.728143	978711.746276	40.940173
3517.658351	978630.234806	40.945178
3518.121317	978531.022983	40.950183
3518.833293	978400.024576	40.955188
3519.226230	978243.484592	40.960192
3519.396380	978087.172383	40.965197
3520.180755	977898.128948	40.970202
3520.575136	977694.295309	40.975207
3521.422319	977475.140279	40.980212
3521.401053	977246.350596	40.985216
3521.838011	977012.982194	40.990221
3522.141290	976752.367560	40.995226
3522.394989	976479.926752	41.000231
3522.512222	976205.052671	41.005236
3523.051334	975909.086939	41.010240
3522.898587	975626.509950	41.015245
3523.437462	975303.444148	41.020250
3523.444806	974991.100459	41.025255
3523.555308	974675.106450	41.030260
3523.899284	974344.004144	41.035264
3524.170215	974001.653627	41.040269
3524.226576	973654.919031	41.045274
3524.272819	973312.075528	41.050279
3524.495201	972958.623704	41.055284
3524.481679	972602.060210	41.060288
3524.552582	972236.562742	41.065293
3524.840418	971867.290386	41.070298
3524.733092	971489.747053	41.075303
3525.103985	971109.361722	41.080308
3524.972524	970729.816349	41.085312
3524.577562	970354.984186	41.090317
3524.683134	969968.991681	41.095322
3525.033946	969591.247848	41.100327
3525.093308	969186.036736	41.105332
3525.363058	968799.057993	41.110336
3525.246316	968395.581150	41.115341
3525.308662	967986.175357	41.120346
3525.296120	967594.465041	41.125351
3525.369480	967179.813455	41.130356
3525.228762	966779.652264	41.135360
3525.201606	966371.516297	41.140365
3525.256293	965952.472511	41.145370
3524.753289	965547.195067	41.150375
3524.710553	965141.421608	41.155380
3524.849655	964738.624656	41.160384
3524.805980	964326.429886	41.165389
3524.932650	963924.165412	41.170394
3524.967527	963511.605539	41.175399
3525.097469	963107.324853	41.180404
3525.028433	962691.393507	41.185408
3524.568116	962259.041161	41.190413
3524.607436	961852.826238	41.195418
3524.467292	961447.885733	41.200423
3524.571737	961032.883543	41.205428
3524.721422	960614.708736	41.210432
3524.382108	960199.719618	41.215437
3524.549574	959793.828260	41.220442
3524.322168	959381.211516	41.225447
3524.032042	958963.283291	41.230452
3524.539151	958546.467580	41.235456
3524.173344	958152.996040	41.240461
3524.390978	957734.503014	41.245466
3523.948271	957325.499568	41.250471
3523.843942	956912.391738	41.255476
3523.950441	956514.220744	41.260480
3523.713791	956099.605822	41.265485
3524.185652	955679.647172	41.270490
3523.821901	955277.840108	41.275495
3523.894972	954864.948767	41.280500
3523.711064	954459.328278	41.285504
3523.575441	954045.922359	41.290509
3523.600697	953629.321293	41.295514
3523.423294	953242.939120	41.300519
3523.305788	952829.541286	41.305524
3523.316404	952435.125932	41.310528
3522.866781	952048.392318	41.315533
3523.010322	951647.377300	41.320538
3522.884072	951270.764542	41.325543
3522.768654	950882.643996	41.330548
3522.933099	950486.890762	41.335552
3522.920846	950098.693617	41.340557
3523.096955	949706.513334	41.345562
3522.769874	949318.787201	41.350567
3522.709457	948918.261215	41.355572
3522.936900	948540.144967	41.360576
3522.537187	948151.672564	41.365581
3522.461693	947751.440689	41.370586
3522.251974	947371.874687	41.375591
3522.514258	946995.553228	41.380596
3522.338494	946609.320328	41.385600
3521.874837	946226.552445	41.390605
3522.204629	945841.423226	41.395610
3521.950207	945470.437125	41.400615
3521.840170	945089.537297	41.405620
3521.965801	944714.029224	41.410624
3521.352813	944330.378986	41.415629
3521.343245	943956.753603	41.420634
3521.399844	943586.155523	41.425639
3521.297784	943222.262643	41.430644
3521.242851	942848.085703	41.435648
3521.269564	942487.473028	41.440653
3521.586102	942109.349250	41.445658
3521.178115	941746.840400	41.450663
3521.234014	941372.730408	41.455668
3521.013046	941006.305916	41.460672
3520.740605	940643.026861	41.465677
3520.879756	940269.590518	41.470682
3520.540612	939905.408326	41.475687
3520.563591	939543.921019	41.480692
3520.415373	939190.489827	41.485696
3520.244365	938835.312693	41.490701
3520.457248	938480.239916	41.495706
3520.317053	938129.036706	41.500711
3520.257487	937765.809787	41.505716
3520.157242	937410.620065	41.510720
3519.567287	937076.107053	41.515725
3519.917176	936713.794669	41.520730
3519.773959	936367.173533	41.525735
3519.712245	936023.873499	41.530740
3519.739750	935684.949229	41.535744
3519.416929	935328.407993	41.540749
3519.765016	934993.991433	41.545754
3519.363342	934654.303845	41.550759
3519.234174	934304.377893	41.555764
3519.081750	933966.811914	41.560768
3518.891400	933643.242205	41.565773
3519.256805	933298.926215	41.570778
3518.826528	932970.555951	41.575783
3518.702087	932627.524639	41.580788
3518.709631	932294.336761	41.585792
3518.476393	931965.487581	41.590797
3518.618864	931641.932423	41.595802
3518.539615	931309.848920	41.600807
3518.487218	930976.299896	41.605812
3518.533864	930659.037710	41.610816
3518.262821	930336.815323	41.615821
3518.092640	929997.078191	41.620826
3517.690503	929693.085169	41.625831
3517.689523	929370.855709	41.630836
3517.976573	929055.379053	41.635840
3517.613882	928738.357736	41.640845
3518.255897	928428.548988	41.645850
3518.096693	928109.439350	41.650855
3517.932364	927793.193729	41.655860
3517.965838	927473.341742	41.660864
3517.477041	927158.168825	41.665869
3517.566272	926837.500854	41.670874
3517.624340	926526.140363	41.675879
3517.288731	926211.559047	41.680884
3517.470202	925902.448423	41.685888
3517.437234	925588.165038	41.690893
3517.444504	925284.814394	41.695898
3517.045588	924974.976891	41.700903
3516.936331	924671.706874	41.705908
3516.608907	924366.629044	41.710912
3516.715708	924062.808337	41.715917
3516.737413	923758.503726	41.720922
3516.574233	923465.366181	41.725927
3516.767849	923163.018773	41.730932
3516.885439	922870.956494	41.735936
3516.489586	922575.116180	41.740941
3516.466564	922282.371960	41.745946
3516.185828	921980.421011	41.750951
3516.211249	921688.790744	41.755956
3516.459766	921399.993680	41.760960
3516.132900	921098.000950	41.765965
3516.036084	920802.687519	41.770970
3515.908493	920531.125951	41.775975
3515.825051	920247.901954	41.780980
3515.761075	919959.368041	41.785984
3515.601624	919673.336234	41.790989
3515.794840	919396.757618	41.795994
3515.690993	919118.962830	41.800999
3515.436712	918828.571665	41.806004
3514.875460	918553.614125	41.811008
3515.457995	918279.320432	41.816013
3515.384686	918006.564708	41.821018
3515.361718	917739.562336	41.826023
3515.215002	917461.689824	41.831028
3515.293321	917195.799200	41.836032
3514.900268	916920.249986	41.841037
3515.015502	916632.087341	41.846042
3515.157837	916366.915910	41.851047
3514.817362	916098.633739	41.856052
3514.861805	915835.378283	41.861056
3514.688494	915570.027542	41.866061
3514.750535	915301.350981	41.871066
3514.419791	915053.623696	41.876071
3514.167115	914787.284979	41.881076
3514.633171	914523.126376	41.886080
3514.338951	914270.060399	41.891085
3514.342535	914004.989820	41.896090
3514.124033	913734.259762	41.901095
3514.126104	913491.415880	41.906100
3514.248408	913231.104831	41.911104
3513.897718	912976.350708	41.916109
3513.884996	912722.588860	41.921114
3513.846777	912484.909639	41.926119
3513.728405	912228.155563	41.931124
3513.790402	911983.404399	41.936128
3513.719246	911734.520749	41.941133
3513.927268	911487.796254	41.946138
3513.762426	911237.074597	41.951143
3513.689822	910987.771942	41.956148
3513.727689	910732.849843	41.961152
3513.315366	910504.495442	41.966157
3513.316691	910257.557150	41.971162
3513.210234	910004.649296	41.976167
3513.336784	909770.585030	41.981172
3513.540533	909531.967344	41.986176
3513.239837	909298.531865	41.991181
3513.000739	909046.276812	41.996186
3513.442715	908810.095338	42.001191
3513.086173	908564.875775	42.006196
3512.758099	908332.078932	42.011200
3512.899144	908093.698805	42.016205
3513.181502	907857.213722	42.021210
3512.897313	907635.373259	42.026215
3512.869519	907398.244673	42.031220
3512.985615	907167.929554	42.036224
3512.605361	906933.153743	42.041229
3512.890206	906694.207569	42.046234
3512.506725	906472.819240	42.051239
3512.310325	906241.166839	42.056244
3512.483476	906026.035169	42.061248
3512.215374	905794.858295	42.066253
3512.198670	905569.032646	42.071258
3512.393314	905345.188943	42.076263
3512.298985	905118.682518	42.081268
3512.278893	904895.049066	42.086272
3511.962454	904685.156201	42.091277
3512.345731	904461.438910	42.096282
3512.255141	904245.606543	42.101287
3512.029261	904030.849568	42.106292
3512.194271	903801.255579	42.111296
3511.696404	903588.166878	42.116301
3511.857047	903373.031431	42.121306
3511.576945	903164.619528	42.126311
3511.803610	902941.928828	42.131316
3511.443680	902726.371712	42.136320
3511.329425	902532.676145	42.141325
3511.731308	902325.858038	42.146330
3511.555190	902120.671979	42.151335
3511.490820	901902.042077	42.156340
3511.520830	901700.861036	42.161344
3511.289568	901497.205817	42.166349
3511.321234	901284.038727	42.171354
3510.995582	901085.500874	42.176359
3510.923475	900879.576473	42.181364
3510.978770	900682.892623	42.186368
3510.916542	900478.013966	42.191373
3511.156255	900284.568721	42.196378
3510.811020	900083.681276	42.201383
3510.758192	899887.759946	42.206388
3510.861864	899694.896252	42.211392
3510.671668	899500.915494	42.216397
3510.747253	899297.999226	42.221402
3510.906415	899107.327548	42.226407
3510.636562	898918.362019	42.231412
3510.607502	898725.969964	42.236416
3510.381979	898536.501409	42.241421
3510.759840	898336.012079	42.246426
3510.556429	898161.402614	42.251431
3510.253118	897971.831334	42.256436
3510.683283	897769.864316	42.261440
3510.524341	897584.410179	42.266445
3510.460519	897396.325842	42.271450
3510.187624	897207.400188	42.276455
3510.116776	897032.250954	42.281460
3510.299190	896831.837130	42.286464
3510.129499	896656.789189	42.291469
3510.320558	896468.438800	42.296474
3510.182734	896300.331595	42.301479
3509.787469	896114.481740	42.306484
3510.128923	895919.807337	42.311488
3509.924283	895748.699127	42.316493
3509.606704	895563.108323	42.321498
3509.720412	895390.004048	42.326503
3509.707629	895213.146132	42.331508
3509.566299	895029.441782	42.336512
3509.611510	894871.893557	42.341517
3509.834817	894698.073592	42.346522
3509.721056	894527.493566	42.351527
3509.359888	894348.153038	42.356532
3509.678555	894166.761573	42.361536
3509.051889	894009.010160	42.366541
3509.401539	893832.629624	42.371546
3509.145734	893665.527290	42.376551
3509.194242	893495.469655	42.381556
3509.451428	893327.499494	42.386560
3509.032617	893172.107623	42.391565
3509.247585	892997.850448	42.396570
3509.256853	892830.389923	42.401575
3509.113178	892672.135191	42.406580
3509.017902	892506.229417	42.411584
3508.652464	892352.643594	42.416589
3509.112694	892191.375207	42.421594
3509.298328	892031.501319	42.426599
3509.042054	891860.865022	42.431604
3509.172109	891698.283291	42.436608
3509.049080	891538.156354	42.441613
3508.800442	891373.596908	42.446618
3508.937619	891215.255588	42.451623
3508.799952	891059.663242	42.456628
3509.121775	890897.994368	42.461632
3509.042380	890741.029700	42.466637
3508.632005	890580.052823	42.471642
3508.971206	890424.074490	42.476647
3508.691873	890268.774202	42.481652
3508.806956	890107.310569	42.486656
3508.652206	889949.175858	42.491661
3508.692889	889798.163208	42.496666
3508.969692	889642.947845	42.501671
3508.430424	889481.864658	42.506676
3508.751643	889319.474235	42.511680
3508.364475	889167.451296	42.516685
3508.194508	889023.225390	42.521690
3508.584519	888870.969824	42.526695
3508.277197	888722.792120	42.531700
3508.193823	888579.701905	42.536704
3508.527612	888429.959663	42.541709
3508.268051	888279.343651	42.546714
3508.277904	888126.356929	42.551719
3508.138627	887972.229492	42.556724
3508.127191	887826.012110	42.561728
3507.681701	887677.733513	42.566733
3507.946415	887529.721199	42.571738
3507.716471	887392.722555	42.576743
3507.687920	887251.525908	42.581748
3507.559974	887111.600364	42.586752
3507.348461	886985.235144	42.591757
3507.936509	886839.087567	42.596762
3507.779111	886712.417102	42.601767
3507.526783	886574.047667	42.606772
3507.382657	886437.399392	42.611776
3507.061717	886313.457369	42.616781
3507.394585	886172.949197	42.621786
3507.421796	886040.716067	42.626791
3507.301173	885917.797376	42.631796
3507.427834	885790.091881	42.636800
3507.270756	885653.136803	42.641805
3507.314631	885529.311497	42.646810
3507.107552	885401.458799	42.651815
3506.953940	885281.145945	42.656820
3507.198506	885138.497332	42.661824
3506.691440	885028.306329	42.666829
3506.788141	884896.326085	42.671834
3506.997884	884780.299881	42.676839
3507.131630	884659.829974	42.681844
3507.044171	884530.776480	42.686848
3507.022000	884409.649285	42.691853
3506.756570	884281.006872	42.696858
3507.314635	884161.328191	42.701863
3506.899606	884039.773843	42.706868
3507.048403	883922.965881	42.711872
3506.750235	883807.003917	42.716877
3507.019655	883689.106162	42.721882
3507.287178	883557.745246	42.726887
3507.131637	883427.613200	42.731892
3507.055841	883311.604720	42.736896
3506.650125	883187.706700	42.741901
3506.871986	883060.506574	42.746906
3506.788260	882952.918258	42.751911
3506.850435	882825.545604	42.756916
3506.797055	882704.000606	42.761920
3506.902325	882592.693947	42.766925
3506.865273	882454.578227	42.771930
3506.628594	882341.192163	42.776935
3506.897446	882233.629343	42.781940
3506.424282	882104.101238	42.786945
3506.610325	881994.900926	42.791949
3506.890270	881882.292642	42.796954
3506.757149	881766.553457	42.801959
3506.332852	881646.306861	42.806964
3506.406497	881527.041388	42.811969
3506.418078	881425.027997	42.816973
3506.418873	881294.919453	42.821978
3506.378445	881194.266922	42.826983
3506.196091	881089.082518	42.831988
3506.771078	880971.854556	42.836993
3506.100090	880872.172332	42.841997
3506.182513	880743.200704	42.847002
3505.972413	880641.500828	42.852007
3506.028796	880533.360368	42.857012
3506.476518	880427.285114	42.862017
3505.866906	880320.219383	42.867021
3505.686947	880222.189307	42.872026
3506.104022	880129.873191	42.877031
3505.920315	880012.363419	42.882036
3506.023985	879907.401350	42.887041
3505.721671	879811.128806	42.892045
3505.960451	879704.687277	42.897050
3505.973696	879594.598465	42.902055
3505.585641	879490.679028	42.907060
3505.722961	879397.137639	42.912065
3505.605635	879306.156450	42.917069
3505.608333	879206.819425	42.922074
3505.456831	879111.092023	42.927079
3506.031899	879010.397465	42.932084
3505.865303	878903.232843	42.937089
3505.302795	878807.471283	42.942093
3505.328142	878722.175882	42.947098
3505.684739	878627.713804	42.952103
3505.588412	878537.589559	42.957108
3505.647503	878442.010404	42.962113
3505.444220	878342.401910	42.967117
3505.515771	878240.032393	42.972122
3505.742387	878154.307870	42.977127
3505.373798	878064.027354	42.982132
3506.059235	877966.010868	42.987137
3505.636902	877869.920119	42.992141
3505.595785	877763.780345	42.997146
3505.493881	877667.730439	43.002151
3505.568979	877565.542481	43.007156
3505.440428	877479.478877	43.012161
3505.643019	877398.788348	43.017165
3505.502196	877291.783990	43.022170
3505.392254	877195.824656	43.027175
3505.466029	877112.630789	43.032180
3505.571233	877000.442300	43.037185
3505.325848	876924.763583	43.042189
3505.255997	876824.913512	43.047194
3505.282626	876747.151668	43.052199
3505.240067	876651.366277	43.057204
3505.401967	876561.750971	43.062209
3504.806539	876484.185103	43.067213
3505.116560	876385.137637	43.072218
3505.062862	876305.250057	43.077223
3505.091089	876224.087371	43.082228
3505.409013	876125.809964	43.087233
3505.177302	876051.960133	43.092237
3505.085219	875963.250286	43.097242
3505.366649	875879.423010	43.102247
3505.295671	875798.270816	43.107252
3505.351581	875709.144888	43.112257
3504.999378	875613.975510	43.117261
3505.185396	875523.758639	43.122266
3504.914768	875441.567711	43.127271
3505.050297	875351.065594	43.132276
3505.033922	875262.332751	43.137281
3504.825095	875196.614729	43.142285
3505.112512	875101.428699	43.147290
3505.120651	875014.433778	43.152295
3504.753221	874948.545162	43.157300
3504.970810	874847.741445	43.162305
3504.843374	874768.815107	43.167309
3504.863430	874692.191150	43.172314
3504.692959	874618.022344	43.177319
3504.490587	874543.178926	43.182324
3505.105388	874461.992404	43.187329
3504.617793	874371.674968	43.192333
3505.104187	874293.902094	43.197338
3504.900433	874227.687500	43.202343
3504.807068	874144.188389	43.207348
3504.589068	874057.410661	43.212353
3504.562795	873991.843185	43.217357
3504.747295	873901.310846	43.222362
3504.816292	873824.376600	43.227367
3504.276075	873745.504635	43.232372
3504.735525	873672.287258	43.237377
3504.497511	873609.951627	43.242381
3504.278644	873524.815358	43.247386
3504.595618	873457.051245	43.252391
3504.438120	873373.357829	43.257396
3504.423344	873297.885716	43.262401
3504.350974	873242.697795	43.267405
3504.511379	873159.919120	43.272410
3504.485564	873097.252101	43.277415
3504.299109	873023.454039	43.282420
3504.139592	872946.740100	43.287425
3504.124806	872875.531387	43.292429
3504.172799	872813.431325	43.297434
3504.591536	872743.410860	43.302439
3504.248038	872663.812957	43.307444
3504.746783	872592.807319	43.312449
3504.253053	872529.435216	43.317453
3504.158292	872456.876325	43.322458
3504.071198	872379.560981	43.327463
3504.037025	872317.469277	43.332468
3504.206171	872243.991061	43.337473
3504.297979	872183.138575	43.342477
3504.151655	872113.883010	43.347482
3503.940728	872049.391854	43.352487
3503.868175	871988.273358	43.357492
3504.391084	871918.226028	43.362497
3504.036533	871858.317068	43.367501
3504.564055	871787.491161	43.372506
3504.373646	871720.664192	43.377511
3503.726976	871647.895252	43.382516
3504.184391	871571.547128	43.387521
3503.799542	871508.534364	43.392525
3504.074652	871444.732909	43.397530
3503.902513	871394.008196	43.402535
3503.730271	871327.756080	43.407540
3504.120981	871267.524304	43.412545
3503.776948	871212.265257	43.417549
3504.195941	871143.487544	43.422554
3504.378340	871079.988604	43.427559
3504.112902	871012.486718	43.432564
3504.171016	870952.694757	43.437569
3503.777485	870883.562665	43.442573
3503.785294	870808.831674	43.447578
3503.986379	870759.495856	43.452583
3504.091204	870705.711011	43.457588
3504.040187	870635.160855	43.462593
3503.927485	870577.043210	43.467597
3503.924161	870507.745418	43.472602
3504.002333	870444.353946	43.477607
3503.967172	870384.086368	43.482612
3504.096915	870324.567493	43.487617
3503.688311	870268.145613	43.492621
3503.894161	870198.518589	43.497626
3503.709143	870135.943703	43.502631
3503.991195	870080.571021	43.507636
3503.875337	870020.701328	43.512641
3503.883176	869956.054418	43.517645
3503.806753	869887.732140	43.522650
3504.126686	869826.915103	43.527655
3503.767093	869768.441993	43.532660
3503.791685	869702.915964	43.537665
3503.648256	869647.900588	43.542669
3503.792147	869594.390520	43.547674
3503.726742	869538.778853	43.552679
3503.831002	869483.235790	43.557684
3503.902706	869405.467435	43.562689
3503.648236	869367.747106	43.567693
3503.668668	869298.722612	43.572698
3503.676847	869242.707763	43.577703
3503.607690	869183.307380	43.582708
3504.044361	869124.988027	43.587713
3503.753783	869072.709832	43.592717
3503.512602	869011.588639	43.597722
3503.404573	868950.639049	43.602727
3503.515350	868901.885285	43.607732
3503.768381	868843.108029	43.612737
3503.502772	868796.454185	43.617741
3503.823794	868733.004571	43.622746
3503.821635	868688.733631	43.627751
3503.276406	868629.891627	43.632756
3503.445197	868577.533425	43.637761
3503.449208	868523.260127	43.642765
3503.418060	868464.428890	43.647770
3503.493932	868420.531475	43.652775
3503.844221	868370.568839	43.657780
3503.813006	868301.055903	43.662785
3503.432456	868251.795244	43.667789
3503.435180	868191.305153	43.672794
3503.604344	868132.826040	43.677799
3503.267767	868100.257318	43.682804
3503.680659	868032.221638	43.687809
3503.718505	867983.860817	43.692813
3503.506483	867928.549653	43.697818
3503.400822	867862.053963	43.702823
3503.036207	867815.117489	43.707828
3503.547983	867764.540603	43.712833
3503.217171	867725.851492	43.717837
3503.276263	867667.191775	43.722842
3503.706939	867618.277775	43.727847
3503.363133	867570.850442	43.732852
3503.590992	867517.210900	43.737857
3503.502454	867484.889287	43.742861
3503.581141	867414.182700	43.747866
3503.706806	867365.414002	43.752871
3503.411019	867316.131692	43.757876
3503.630713	867260.160590	43.762881
3503.186048	867202.841762	43.767885
3503.112598	867147.986129	43.772890
3503.299705	867095.320654	43.777895
3503.308851	867057.445237	43.782900
3503.782691	867006.188438	43.787905
3503.439506	866946.713942	43.792909
3503.332583	866894.872073	43.797914
3503.450359	866842.701388	43.802919
3503.208922	866789.812494	43.807924
3503.534672	866735.858506	43.812929
3503.546034	866689.725354	43.817933
3503.328479	866645.086359	43.822938
3503.688928	866583.647071	43.827943
3502.996660	866535.880492	43.832948
3503.339956	866483.766663	43.837953
3503.157095	866445.044924	43.842957
3503.227224	866398.414243	43.847962
3503.216915	866338.393268	43.852967
3503.395709	866290.481229	43.857972
3503.446003	866241.230212	43.862977
3503.102329	866196.220160	43.867981
3503.081875	866145.037474	43.872986
3503.408969	866098.847777	43.877991
3503.176531	866056.829339	43.882996
3503.553380	866010.727900	43.888001
3503.124276	865960.873664	43.893005
3503.410197	865910.415555	43.898010
3503.594921	865858.419579	43.903015
3503.153088	865821.970543	43.908020
3503.276960	865760.561844	43.913025
3503.409500	865720.326472	43.918029
3503.278652	865669.449338	43.923034
3503.234624	865613.797794	43.928039
3503.120756	865563.985473	43.933044
3503.535832	865519.428177	43.938049
3503.274749	865472.456351	43.943053
3503.143950	865418.565795	43.948058
3503.243291	865369.493856	43.953063
3503.291934	865331.892502	43.958068
3503.524853	865274.832231	43.963073
3503.277037	865235.530568	43.968077
3503.210815	865189.981572	43.973082
3503.227769	865136.355582	43.978087
3503.437286	865089.594672	43.983092
3503.421139	865040.053359	43.988097
3503.222752	865000.353437	43.993101
3503.136774	864939.650983	43.998106
3503.409526	864900.649961	44.003111
3503.158752	864856.683220	44.008116
3503.178506	864805.676842	44.013121
3502.850917	864762.110665	44.018125
3503.124929	864713.684670	44.023130
3502.861992	864669.524267	44.028135
3503.091706	864624.505158	44.033140
3503.419040	864577.623725	44.038145
3503.034371	864538.534374	44.043149
3503.122648	864488.582719	44.048154
3503.027102	864432.248690	44.053159
3503.207015	864404.529772	44.058164
3503.280374	864340.588906	44.063169
3503.285637	864307.943321	44.068173
3502.787874	864249.730710	44.073178
3503.047747	864209.658615	44.078183
3502.644377	864169.501207	44.083188
3502.629510	864131.417048	44.088193
3502.687925	864104.494054	44.093197
3502.795024	864060.656878	44.098202
3503.210832	864018.906088	44.103207
3503.054614	863979.678318	44.108212
3503.128466	863940.801043	44.113217
3502.993746	863900.694751	44.118221
3502.958655	863863.195219	44.123226
3503.356537	863812.992650	44.128231
3502.824442	863773.145311	44.133236
3503.125593	863717.905262	44.138241
3503.009477	863683.915972	44.143245
3503.028566	863639.798748	44.148250
3503.173425	863595.271806	44.153255
3503.240116	863552.214957	44.158260
3503.237320	863501.395635	44.163265
3502.988376	863470.342137	44.168269
3502.843142	863412.840752	44.173274
3503.254135	863380.997867	44.178279
3502.700915	863338.527493	44.183284
3503.222916	863281.595143	44.188289
3502.937235	863248.700258	44.193293
3503.018241	863212.052135	44.198298
3502.833004	863165.827275	44.203303
3502.856589	863138.419847	44.208308
3502.732539	863081.494882	44.213313
3502.658439	863047.883808	44.218317
3502.381814	863006.823197	44.223322
3502.815460	862984.109243	44.228327
3502.538680	862938.383621	44.233332
3502.961613	862897.595733	44.238337
3502.702696	862856.822728	44.243341
3502.808712	862807.437368	44.248346
3502.821762	862777.697692	44.253351
3502.891698	862750.961150	44.258356
3502.664893	862706.294549	44.263361
3502.902055	862672.532929	44.268365
3502.794673	862626.291126	44.273370
3502.651616	862594.243847	44.278375
3502.458687	862552.486074	44.283380
3502.725737	862522.120185	44.288385
3502.437332	862491.068166	44.293389
3502.726405	862453.798065	44.298394
3502.644802	862416.200055	44.303399
3502.744419	862371.282831	44.308404
3502.913454	862329.658267	44.313409
3502.824715	862296.337007	44.318413
3503.013597	862255.680562	44.323418
3502.826941	862228.595234	44.328423
3502.596518	862188.104609	44.333428
3503.087666	862147.203256	44.338433
3502.780171	862107.502327	44.343437
3502.602847	862067.585306	44.348442
3502.642359	862026.174389	44.353447
3502.626792	861999.934597	44.358452
3502.628724	861952.406123	44.363457
3502.809891	861924.092494	44.368461
3502.514022	861904.021784	44.373466
3503.094035	861849.690749	44.378471
3503.060973	861814.996921	44.383476
3502.796877	861780.438155	44.388481
3502.648512	861739.445029	44.393485
3502.577952	861686.094504	44.398490
3502.770555	861658.749750	44.403495
3502.490662	861629.830314	44.408500
3502.610216	861586.070406	44.413505
3502.875978	861560.268370	44.418509
3502.610443	861503.060307	44.423514
3502.806626	861471.923234	44.428519
3502.812834	861436.540356	44.433524
3502.774412	861403.108703	44.438529
3502.670563	861370.465280	44.443533
3502.411280	861332.209404	44.448538
3502.171377	861296.283027	44.453543
3502.318577	861263.889287	44.458548
3502.540260	861246.064078	44.463553
3502.456306	861211.375189	44.468557
3502.333211	861180.775264	44.473562
3502.471399	861152.562334	44.478567
3502.180101	861115.768488	44.483572
3502.360201	861089.395321	44.488577
3501.975840	861059.323873	44.493581
3501.876114	861038.731939	44.498586
3502.688797	861011.184907	44.503591
3502.332517	860981.691709	44.508596
3502.779011	860961.398364	44.513601
3502.600111	860924.195996	44.518605
3502.712898	860876.640853	44.523610
3502.623805	860840.589726	44.528615
3502.267570	860807.109946	44.533620
3502.556325	860785.675444	44.538625
3502.475983	860756.621762	44.543629
3502.258285	860718.744031	44.548634
3502.264132	860687.828739	44.553639
3502.240034	860662.751167	44.558644
3502.323475	860635.808669	44.563649
3502.508452	860613.807365	44.568653
3502.747011	860574.006451	44.573658
3502.789881	860534.043082	44.578663
3502.803491	860494.959237	44.583668
3502.571490	860476.137122	44.588673
3502.427984	860439.217615	44.593677
3502.431733	860410.828964	44.598682
3502.872723	860373.715543	44.603687
3502.308483	860343.378529	44.608692
3502.569800	860308.627612	44.613697
3502.234083	860276.405408	44.618701
3502.029882	860245.522478	44.623706
3502.310042	860221.754077	44.628711
3502.486261	860187.210935	44.633716
3502.724879	860158.101848	44.638721
3502.600399	860129.927462	44.643725
3502.195395	860086.048753	44.648730
3502.321422	860065.805234	44.653735
3502.048752	860047.182943	44.658740
3502.550131	860011.029624	44.663745
3502.542011	859977.099020	44.668749
3502.776592	859935.155609	44.673754
3502.892273	859907.718447	44.678759
3502.144327	859866.908719	44.683764
3502.448825	859829.133879	44.688769
3502.339356	859808.928307	44.693773
3502.305597	859783.459793	44.698778
3502.402588	859745.135243	44.703783
3502.488000	859719.452368	44.708788
3502.644423	859692.688142	44.713793
3502.572960	859665.864113	44.718797
3502.513035	859626.786821	44.723802
3502.474427	859601.804509	44.728807
3502.277355	859564.694066	44.733812
3502.719857	859527.575258	44.738817
3502.409688	859497.483867	44.743821
3501.979038	859468.287290	44.748826
3502.399289	859444.298317	44.753831
3502.224677	859429.352913	44.758836
3502.700526	859381.240121	44.763841
3502.173174	859368.200168	44.768845
3501.859421	859340.928447	44.773850
3502.250984	859307.803404	44.778855
3501.875784	859291.626626	44.783860
3501.976496	859259.424378	44.788865
3502.226597	859240.032823	44.793869
3502.180963	859219.814783	44.798874
3502.130732	859190.554200	44.803879
3502.296932	859169.231462	44.808884
3502.232593	859143.376358	44.813889
3502.134694	859108.580559	44.818893
3501.977590	859088.672171	44.823898
3502.316962	859059.152289	44.828903
3501.910647	859031.310986	44.833908
3502.189304	859008.510535	44.838913
3502.188184	858980.310516	44.843917
3502.134500	858962.815741	44.848922
3502.068342	858931.222713	44.853927
3501.991963	858904.007174	44.858932
3502.168962	858885.598978	44.863937
3502.147226	858857.596278	44.868941
3502.199224	858833.860075	44.873946
3502.411106	858801.150874	44.878951
3502.276055	858791.934863	44.883956
3502.302356	858745.058080	44.888961
3502.274173	858733.684957	44.893965
3502.067830	858700.168903	44.898970
3502.364360	858688.839445	44.903975
3502.117196	858659.997756	44.908980
3502.401431	858623.191284	44.913985
3501.972623	858599.047144	44.918989
3502.089041	858571.798362	44.923994
3502.311492	858551.825691	44.928999
3502.024989	858526.393577	44.934004
3502.236976	858509.534482	44.939009
3502.139533	858483.195790	44.944013
3502.240574	858451.475487	44.949018
3502.228935	858423.858141	44.954023
3502.019975	858405.414839	44.959028
3502.091470	858381.868174	44.964033
3501.915755	858357.486876	44.969037
3501.970953	858335.109744	44.974042
3502.035404	858317.010142	44.979047
3502.158455	858283.632041	44.984052
3502.390244	858263.559639	44.989057
3502.116284	858232.191744	44.994061
3502.100552	858205.546631	44.999066
3502.275655	858183.149190	45.004071
3502.022136	858159.363451	45.009076
3501.973551	858130.875571	45.014081
3502.239188	858108.851966	45.019085
3502.294462	858080.152226	45.024090
3502.426551	858063.791353	45.029095
3502.368670	858035.012787	45.034100
3502.362207	857994.651906	45.039105
3502.100853	857986.330811	45.044109
3502.031369	857948.995017	45.049114
3502.623397	857921.859504	45.054119
3502.430348	857898.257306	45.059124
3502.204497	857874.368640	45.064129
3502.169072	857842.278626	45.069133
3501.908504	857814.796805	45.074138
3501.802710	857790.985296	45.079143
3501.906067	857764.902213	45.084148
3501.917096	857758.481167	45.089153
3502.074096	857742.601644	45.094157
3501.881170	857713.260242	45.099162
3502.205759	857689.474693	45.104167
3501.704670	857678.469311	45.109172
3502.106225	857646.209012	45.114177
3502.138834	857629.960636	45.119181
3502.111512	857596.700833	45.124186
3502.162438	857582.102808	45.129191
3501.781788	857566.019614	45.134196
3502.034485	857526.682866	45.139201
3501.889068	857509.977175	45.144205
3501.577394	857499.815656	45.149210
3501.951254	857453.649854	45.154215
3501.936596	857459.682857	45.159220
3501.791091	857438.210917	45.164225
3502.041169	857401.208204	45.169229
3502.220537	857394.564507	45.174234
3502.038794	857362.982428	45.179239
3501.854723	857352.896909	45.184244
3501.909422	857329.640774	45.189249
3501.985490	857305.700147	45.194253
3502.106197	857277.180406	45.199258
3501.961079	857259.695826	45.204263
3501.586527	857237.969112	45.209268
3502.085871	857220.572783	45.214273
3502.186357	857206.354781	45.219277
3501.837834	857167.406597	45.224282
3502.650935	857154.238324	45.229287
3502.220141	857128.532355	45.234292
3502.214219	857104.993541	45.239297
3502.017553	857064.657873	45.244301
3501.934619	857053.582469	45.249306
3502.167993	857035.353980	45.254311
3501.916043	857014.092638	45.259316
3501.929278	856987.340184	45.264321
3502.320385	856961.109004	45.269325
3502.136912	856941.295246	45.274330
3501.962220	856913.406132	45.279335
3501.474230	856890.724121	45.284340
3502.067872	856880.412416	45.289345
3501.814022	856871.504910	45.294349
3502.020627	856834.700499	45.299354
3502.329130	856811.108755	45.304359
3501.839784	856797.667923	45.309364
3502.045097	856765.435334	45.314369
3501.876549	856754.373495	45.319373
3501.699517	856741.464751	45.324378
3501.672990	856720.067971	45.329383
3501.569895	856704.909566	45.334388
3501.760271	856700.208879	45.339393
3501.910923	856674.016091	45.344397
3501.530490	856648.786206	45.349402
3502.025678	856632.458978	45.354407
3501.769283	856610.418730	45.359412
3501.698949	856578.619696	45.364417
3502.045750	856584.885848	45.369421
3501.921601	856559.807934	45.374426
3501.822613	856529.278016	45.379431
3501.666567	856529.984748	45.384436
3501.697776	856505.075577	45.389441
3501.833011	856492.114861	45.394445
3501.567267	856459.082736	45.399450
3501.686522	856450.404993	45.404455
3501.642682	856455.568247	45.409460
3501.850532	856421.776917	45.414465
3502.132229	856393.712966	45.419469
3502.367785	856380.346352	45.424474
3502.257386	856349.136434	45.429479
3502.110093	856340.502451	45.434484
3502.032829	856298.293671	45.439489
3502.136540	856294.871660	45.444493
3502.077125	856272.992316	45.449498
3502.260739	856235.409823	45.454503
3501.964313	856220.768505	45.459508
3501.961723	856185.648542	45.464513
3502.246530	856171.495066	45.469517
3501.994993	856159.083806	45.474522
3501.863711	856117.369119	45.479527
3501.723838	856108.928164	45.484532
3501.943448	856093.909659	45.489537
3502.123600	856062.553127	45.494541
3501.859098	856058.024184	45.499546
3502.104523	856016.635905	45.504551
3501.823056	856004.813001	45.509556
3501.745291	855996.361657	45.514561
3501.987845	855963.243121	45.519565
3501.834421	855948.869464	45.524570
3502.193266	855931.006196	45.529575
3501.844101	855909.367878	45.534580
3501.951491	855877.827810	45.539585
3501.964361	855877.436576	45.544589
3501.648017	855850.830765	45.549594
3502.027994	855828.390987	45.554599
3501.817197	855833.971438	45.559604
3501.632564	855796.641520	45.564609
3501.612107	855781.078048	45.569613
3501.779319	855771.613102	45.574618
3501.613387	855752.668256	45.579623
3501.550845	855730.301028	45.584628
3501.818248	855716.052081	45.589633
3502.021553	855704.829789	45.594637
3502.071361	855686.043783	45.599642
3502.275619	855662.270225	45.604647
3501.684832	855644.076107	45.609652
3501.915853	855625.162764	45.614657
3501.867804	855594.230627	45.619661
3501.629829	855594.269887	45.624666
3501.736417	855561.658074	45.629671
3502.087107	855538.832882	45.634676
3501.666747	855524.113021	45.639681
3501.800156	855508.037022	45.644685
3502.003079	855484.652189	45.649690
3502.095957	855484.247748	45.654695
3501.951795	855449.633398	45.659700
3501.730225	855430.696726	45.664705
3501.669563	855426.717523	45.669709
3501.692845	855398.788915	45.674714
3502.158346	855375.165807	45.679719
3501.801793	855368.316326	45.684724
3502.209297	855343.048555	45.689729
3502.083801	855310.862852	45.694733
3501.704682	855297.692464	45.699738
3502.144569	855261.910524	45.704743
3501.879186	855248.915895	45.709748
3501.856468	855233.837919	45.714753
3501.368385	855217.182442	45.719757
3501.545127	855198.179430	45.724762
3502.100221	855190.401132	45.729767
3501.906138	855182.746254	45.734772
3501.525562	855140.092986	45.739777
3501.600687	855134.242458	45.744781
3501.766620	855127.695838	45.749786
3501.737422	855101.525992	45.754791
3501.639322	855088.600767	45.759796
3501.661520	855081.591259	45.764801
3501.937871	855066.852819	45.769805
3501.543643	855046.191928	45.774810
3501.786918	855001.196903	45.779815
3501.367034	854936.752221	45.784820
3501.464394	854805.079049	45.789825
3501.589243	854626.202659	45.794829
3501.457835	854383.427486	45.799834
3501.667302	854064.579900	45.804839
3501.501382	853724.463415	45.809844
3501.413692	853295.548781	45.814849
3501.134528	852815.337988	45.819853
3500.844848	852259.257481	45.824858
3500.881876	851665.882590	45.829863
3500.463755	851004.173700	45.834868
3500.179621	850286.476590	45.839873
3499.988820	849493.689897	45.844877
3499.776097	848654.733512	45.849882
3499.831119	847742.361350	45.854887
3499.232728	846771.308500	45.859892
3499.011740	845716.528188	45.864897
3499.053758	844606.945557	45.869901
3498.027363	843430.760673	45.874906
3497.856308	842190.252422	45.879911
3497.204664	840899.744957	45.884916
3496.923001	839505.710523	45.889921
3496.758263	838054.420239	45.894925
3495.913262	836536.842573	45.899930
3495.685521	834952.034366	45.904935
3495.122249	833298.053759	45.909940
3494.648769	831559.005593	45.914945
3494.372067	829751.804261	45.919949
3493.642369	827893.359066	45.924954
3493.063136	825926.197518	45.929959
3492.315660	823912.466246	45.934964
3491.392878	821834.128781	45.939969
3490.809861	819683.654922	45.944973
3489.897287	817456.977255	45.949978
3489.588683	815166.156983	45.954983
3489.204997	812808.158949	45.959988
3488.320947	810362.312990	45.964993
3487.381765	807860.898816	45.969997
3486.082478	805285.525433	45.975002
3485.614381	802648.915664	45.980007
3484.570066	799948.636699	45.985012
3483.964411	797167.126236	45.990017
3482.994703	794330.402562	45.995021
3482.132690	791414.502683	46.000026
3481.215734	788432.976496	46.005031
3480.307896	785393.605927	46.010036
3479.410116	782267.206804	46.015041
3478.217627	779088.369291	46.020045
3476.967691	775835.973644	46.025050
3476.213015	772517.130965	46.030055
3474.780363	769144.620380	46.035060
3473.714289	765689.664294	46.040065
3472.520399	762188.100191	46.045069
3471.398317	758610.483100	46.050074
3470.270792	754959.892164	46.055079
3469.079399	751263.463364	46.060084
3467.702040	747493.295656	46.065089
3466.685783	743653.509741	46.070093
3465.166989	739753.364070	46.075098
3464.025353	735792.246918	46.080103
3462.638109	731770.734271	46.085108
3461.238855	727684.605560	46.090113
3459.889002	723529.957928	46.095117
3458.302335	719304.574761	46.100122
3457.089246	715026.876393	46.105127
3455.610047	710680.729325	46.110132
3454.039589	706271.885061	46.115137
3452.458573	701805.079665	46.120141
3450.934646	697273.477684	46.125146
3449.691420	692668.314391	46.130151
3447.744549	688014.601256	46.135156
3446.013338	683308.854694	46.140161
3444.970607	678515.922667	46.145165
3442.406589	673688.953649	46.150170
3441.341725	668773.517114	46.155175
3439.450192	663817.197597	46.160180
3437.727054	658803.078137	46.165185
3435.952987	653708.014706	46.170189
3433.807039	648568.555425	46.175194
3432.036591	643355.496232	46.180199
3429.777915	638103.675859	46.185204
3427.962271	632798.957773	46.190209
3426.009953	627437.192713	46.195213
3423.760559	622029.086335	46.200218
3421.797750	616559.027213	46.205223
3419.614020	611026.149219	46.210228
3417.662538	605453.262943	46.215233
3415.794051	599817.188081	46.220237
3413.507960	594141.269685	46.225242
3411.673990	588397.265968	46.230247
3409.169478	582605.828445	46.235252
3406.818442	576759.311847	46.240257
3404.368367	570867.396439	46.245261
3402.311647	564919.067845	46.250266
3399.800786	558920.841606	46.255271
3397.795619	552879.957053	46.260276
3394.878019	546787.474175	46.265281
3392.556763	540652.315456	46.270285
3389.940255	534482.706995	46.275290
3387.498531	528241.385360	46.280295
3385.108821	521977.027092	46.285300
3382.320912	515643.464389	46.290305
3379.855589	509283.975896	46.295309
3377.218674	502880.527428	46.300314
3374.563833	496422.740924	46.305319
3371.604256	489935.262831	46.310324
3368.659123	483403.144851	46.315329
3365.690506	476836.897912	46.320333
3362.946963	470242.089275	46.325338
3360.127407	463593.931676	46.330343
3357.100431	456927.544806	46.335348
3354.102473	450218.912287	46.340353
3351.282965	443474.081413	46.345357
3348.303976	436703.958989	46.350362
3345.354180	429884.157408	46.355367
3341.809992	423041.189394	46.360372
3338.672355	416167.206862	46.365377
3335.579617	409272.256089	46.370381
3332.301924	402353.544743	46.375386
3328.984802	395396.935240	46.380391
3325.349707	388432.063093	46.385396
3322.062187	381437.441787	46.390401
3318.940258	374401.954102	46.395405
3315.087016	367356.860601	46.400410
3311.762385	360267.416368	46.405415
3308.137554	353191.444009	46.410420
3304.663878	346085.250285	46.415425
3301.178834	338971.050437	46.420429
3297.432351	331842.786169	46.425434
3294.035729	324687.203764	46.430439
3289.928797	317527.215065	46.435444
3286.514981	310363.390207	46.440449
3282.522709	303175.785602	46.445453
3278.542882	295986.033013	46.450458
3274.988245	288778.697451	46.455463
3271.294777	281581.107756	46.460468
3267.054046	274364.136259	46.465473
3263.102448	267142.710158	46.470477
3258.822686	259914.450696	46.475482
3254.993783	252692.310325	46.480487
3250.981482	245465.789151	46.485492
3246.853160	238243.550910	46.490497
3242.762044	231023.344660	46.495501
3238.242935	223743.052540	46.500506
3234.377805	216499.130097	46.505511
3229.573838	209287.737299	46.510516
3225.160998	202093.387500	46.515521
3221.106104	194905.392174	46.520525
3216.619186	187737.956966	46.525530
3212.052116	180574.132259	46.530535
3207.438946	173424.510559	46.535540
3202.584967	166286.460141	46.540545
3197.935560	159173.575584	46.545549
3193.313334	152100.077771	46.550554
3188.831515	145015.628259	46.555559
3183.724622	137998.483984	46.560564
3178.842568	130964.696667	46.565569
3174.081641	123980.248529	46.570573
3168.823532	117030.062197	46.575578
3163.596806	110104.166120	46.580583
3158.488081	103209.416526	46.585588
3153.019676	96362.940201	46.590593
3147.575828	89557.127305	46.595597
3141.972145	82796.639847	46.600602
3136.327297	76083.044539	46.605607
3130.276756	69426.135475	46.610612
3124.108417	62832.282574	46.615617
3117.435047	56308.354856	46.620621
3109.958113	49856.229258	46.625626
3102.205315	43515.854617	46.630631
3087.529911	37432.790149	46.635636
3068.175295	31646.151175	46.640641
3049.175595	26096.851073	46.645645
3030.393784	20850.361364	46.650650
3011.282100	15925.866981	46.655655
2987.793798	11507.358943	46.660660
2959.703652	7612.236263	46.665665
2931.061725	4232.084545	46.670669
2902.453294	1400.113972	46.675674
2832.690411	284.349451	46.680679
2755.750401	278.186918	46.685684
2723.505972	286.203818	46.690689
2729.714601	281.570419	46.695693
2755.821254	266.901978	46.700698
2786.576986	259.431763	46.705703
2810.194609	268.864094	46.710708
2823.153827	270.433347	46.715713
2826.904645	254.911634	46.720717
2824.056985	265.276277	46.725722
2818.600330	256.378521	46.730727
2813.764188	254.051349	46.735732
2809.073383	246.775713	46.740737
2805.871703	247.573573	46.745741
2802.660366	246.041622	46.750746
2800.564339	250.238046	46.755751
2798.383819	245.985173	46.760756
2795.942909	250.006820	46.765761
2793.595037	235.648811	46.770765
2790.364811	247.467052	46.775770
2787.470833	234.694218	46.780775
2784.316759	240.512523	46.785780
2781.483344	240.148072	46.790785
2778.353679	239.967878	46.795789
2775.220873	239.756630	46.800794
2772.161515	242.101875	46.805799
2768.980327	229.499193	46.810804
2765.312935	238.633093	46.815809
2762.241539	235.925995	46.820813
2759.241452	238.519591	46.825818
2756.095252	225.970747	46.830823
2752.885877	230.680444	46.835828
2749.689631	224.828980	46.840833
2746.659858	221.260141	46.845837
2743.148383	232.517776	46.850842
2739.219849	229.335625	46.855847
2735.825769	225.672185	46.860852
2732.689783	224.031152	46.865857
2729.876211	222.178654	46.870861
2726.247430	236.571296	46.875866
2723.145968	222.610020	46.880871
2719.739247	221.334152	46.885876
2715.987790	227.200937	46.890881
2712.730679	226.733170	46.895885
2709.206397	233.515640	46.900890
2705.792313	225.602797	46.905895
2702.659705	225.754671	46.910900
2699.278741	215.694817	46.915905
2695.960748	217.707041	46.920909
2692.349067	222.898364	46.925914
2688.813187	215.703439	46.930919
2685.990287	215.336123	46.935924
2682.578792	214.350372	46.940929
2679.028114	213.466922	46.945933
2675.053428	218.786041	46.950938
2671.830852	218.792144	46.955943
2668.236569	214.535034	46.960948
2664.985423	210.154998	46.965953
2662.101244	209.502979	46.970957
2658.274742	212.873573	46.975962
2654.766100	209.968737	46.980967
2650.799873	205.749734	46.985972
2646.968386	210.611089	46.990977
2644.812935	210.522024	46.995981
2641.031122	211.984064	47.000986
2637.531324	201.268573	47.005991
2634.290803	210.936752	47.010996
2630.766495	215.246970	47.016001
2627.679345	207.092771	47.021005
2624.218276	208.124181	47.026010
2620.087352	208.251009	47.031015
2616.658471	203.855345	47.036020
2613.045150	203.588909	47.041025
2610.045583	207.887927	47.046029
2606.546366	207.129440	47.051034
2603.165136	206.868915	47.056039
2599.328426	208.447004	47.061044
2595.712897	211.377486	47.066049
2592.880249	214.492941	47.071053
2589.571918	210.912946	47.076058
2585.687335	212.726678	47.081063
2582.430080	203.364437	47.086068
2578.435669	200.359851	47.091073
2575.241854	193.148437	47.096077
2571.796939	198.788692	47.101082
2568.512500	207.470341	47.106087
2565.166391	196.116212	47.111092
2561.147046	207.853618	47.116097
2558.247564	196.621942	47.121101
2554.065092	200.997412	47.126106
2550.689750	195.174472	47.131111
2547.914271	201.598614	47.136116
2543.865951	201.219308	47.141121
2540.751297	192.222333	47.146125
2536.913200	214.263436	47.151130
2533.787413	195.970354	47.156135
2529.881370	190.938738	47.161140
2526.455732	191.877142	47.166145
2523.370361	187.325792	47.171149
2519.746217	195.206672	47.176154
2516.225699	199.339912	47.181159
2512.817079	196.421833	47.186164
2509.273770	195.574785	47.191169
2505.849253	192.703540	47.196173
2502.314898	201.906405	47.201178
2498.865296	183.188456	47.206183
2495.173198	191.916109	47.211188
2491.108863	196.845998	47.216193
2488.622698	187.638767	47.221197
2484.631534	193.726817	47.226202
2481.245052	187.538321	47.231207
2477.883633	187.055958	47.236212
2474.095378	190.836759	47.241217
2471.453744	187.521365	47.246221
2467.574282	191.559166	47.251226
2463.990755	183.828622	47.256231
2460.550933	179.951525	47.261236
2456.792621	186.037272	47.266241
2453.235001	185.620464	47.271245
2449.731481	186.284642	47.276250
2446.363333	185.262302	47.281255
2442.854086	189.208425	47.286260
2439.641194	188.773404	47.291265
2436.452149	190.033161	47.296269
2432.727805	189.765843	47.301274
2429.148507	178.250813	47.306279
2425.628705	185.471195	47.311284
2422.012107	191.229671	47.316289
2418.596986	182.997353	47.321293
2415.182544	185.250643	47.326298
2411.740123	183.015296	47.331303
2408.523240	180.114587	47.336308
2404.721896	184.693473	47.341313
2400.873837	191.171195	47.346317
2397.442988	191.151863	47.351322
2394.104776	185.300812	47.356327
2390.679978	181.079097	47.361332
2387.037486	191.779540	47.366337
2384.033764	178.071211	47.371341
2379.959143	186.983246	47.376346
2376.547500	182.895535	47.381351
2373.470793	175.569036	47.386356
2369.178303	185.778446	47.391361
2366.275269	172.494374	47.396365
2362.672402	185.488689	47.401370
2359.225956	181.250442	47.406375
2355.856852	177.405558	47.411380
2352.488197	177.102280	47.416385
2349.058581	162.462990	47.421389
2345.372415	178.942282	47.426394
2341.486973	172.487564	47.431399
2338.351815	171.608588	47.436404
2334.614525	179.563712	47.441409
2331.361890	176.404521	47.446413
2327.654347	176.250546	47.451418
2324.448165	169.676803	47.456423
2320.754521	178.705565	47.461428
2316.755226	171.970100	47.466433
2314.222860	164.695477	47.471437
2310.292258	173.083325	47.476442
2306.866911	172.817065	47.481447
2303.145736	172.844150	47.486452
2299.659321	183.873299	47.491457
2296.510301	169.441702	47.496461
2292.728093	171.440633	47.501466
2289.068178	165.273751	47.506471
2285.848145	177.366600	47.511476
2282.304315	177.700494	47.516481
2279.145165	172.584470	47.521485
2275.354442	173.286122	47.526490
2272.063618	170.789041	47.531495
2268.359918	170.391946	47.536500
2264.435424	176.887114	47.541505
2261.747011	165.472423	47.546509
2258.153200	158.307164	47.551514
2254.623535	169.775252	47.556519
2251.049884	177.263937	47.561524
2246.972582	173.642621	47.566529
2243.779183	159.986648	47.571533
2240.307150	172.661440	47.576538
2236.828158	167.171801	47.581543
2233.217970	168.796438	47.586548
2229.657829	173.020473	47.591553
2226.524868	168.085466	47.596557
2222.903719	168.008281	47.601562
2219.547619	166.537726	47.606567
2216.196976	162.472629	47.611572
2212.714724	166.606654	47.616577
2209.156574	160.396199	47.621581
2204.971711	171.340612	47.626586
2201.402735	163.796547	47.631591
2198.468734	166.348562	47.636596
2195.071116	168.301434	47.641601
2191.204033	158.128296	47.646605
2187.458896	170.115485	47.651610
2184.234930	157.400003	47.656615
2180.909228	164.231692	47.661620
2177.279681	162.445185	47.666625
2173.992427	159.054424	47.671629
2170.471893	164.225308	47.676634
2166.982122	157.707982	47.681639
2163.912901	161.564463	47.686644
2160.011541	164.997110	47.691649
2156.900004	155.132810	47.696653
2152.533299	167.206468	47.701658
2149.103469	167.430661	47.706663
2146.045957	155.690214	47.711668
2142.488410	155.586998	47.716673
2138.772040	152.760272	47.721677
2135.413128	159.662396	47.726682
2131.960347	147.586041	47.731687
2128.844680	158.518931	47.736692
2124.781028	160.255623	47.741697
2121.225154	148.892910	47.746701
2117.795663	149.556940	47.751706
2114.348598	144.114822	47.756711
2110.770386	150.728941	47.761716
2107.616099	160.553841	47.766721
2104.400249	154.133616	47.771725
2100.323903	158.364434	47.776730
2096.657101	155.369119	47.781735
2093.164517	147.407989	47.786740
2090.048644	158.220555	47.791745
2086.892570	148.524695	47.796749
2082.911210	156.724924	47.801754
2079.336888	155.651638	47.806759
2076.053475	148.657480	47.811764
2072.249673	163.333907	47.816769
2068.793201	149.615752	47.821773
2064.822129	150.292685	47.826778
2061.859855	159.569660	47.831783
2058.782618	158.107636	47.836788
2055.043843	150.495633	47.841793
2051.546582	158.809730	47.846797
2047.996261	160.439219	47.851802
2044.564244	162.813273	47.856807
2041.015595	160.132191	47.861812
2037.334560	155.014515	47.866817
2033.992075	155.761524	47.871821
2030.134892	158.499442	47.876826
2026.668001	165.720017	47.881831
2023.355871	152.892337	47.886836
2019.955102	168.096827	47.891841
2016.920650	155.070355	47.896845
2012.832703	159.864394	47.901850
2009.478729	159.413886	47.906855
2005.853139	156.661076	47.911860
2002.075144	158.977051	47.916865
1998.882336	153.914546	47.921869
1995.154452	156.684025	47.926874
1991.676417	157.719463	47.931879
1988.560530	159.046359	47.936884
1984.924786	154.703106	47.941889
1981.683116	149.479762	47.946893
1978.441513	156.259400	47.951898
1974.646806	151.859132	47.956903
1970.531262	157.661629	47.961908
1967.102062	158.789465	47.966913
1963.741126	148.085184	47.971917
1960.395216	146.399218	47.976922
1956.862284	147.333237	47.981927
1953.614346	149.948489	47.986932
1949.865925	147.527415	47.991937
1946.263866	149.468239	47.996941
1942.827612	146.474636	48.001946
1939.585586	150.322689	48.006951
1935.974124	149.222098	48.011956
1932.195151	154.354323	48.016961
1929.091505	150.306072	48.021965
1925.193742	148.935059	48.026970
1922.081255	146.343851	48.031975
1918.751929	148.319375	48.036980
1914.858238	154.458047	48.041985
1911.470572	149.287680	48.046989
1907.879369	150.978881	48.051994
1904.052569	155.400119	48.056999
1900.950169	141.963651	48.062004
1897.514578	154.084992	48.067009
1894.105339	146.406465	48.072013
1890.236791	148.309057	48.077018
1886.704010	141.881157	48.082023
1883.480574	142.940729	48.087028
1879.678963	149.637092	48.092033
1876.610998	137.707370	48.097037
1872.922842	151.412056	48.102042
1869.350420	150.979968	48.107047
1866.230686	140.348416	48.112052
1861.956551	148.983555	48.117057
1858.955271	138.797375	48.122061
1854.934661	144.412396	48.127066
1851.608993	138.766117	48.132071
1848.582730	134.874067	48.137076
1844.698140	147.139458	48.142081
1841.377300	138.709510	48.147085
1837.767139	147.394836	48.152090
1834.181293	141.460805	48.157095
1831.031679	135.406373	48.162100
1827.408245	150.511963	48.167105
1824.309245	141.889484	48.172109
1820.685919	142.959306	48.177114
1817.078747	144.473041	48.182119
1813.410271	141.418635	48.187124
1809.391514	143.135937	48.192129
1806.164955	132.209103	48.197133
1802.763269	137.546094	48.202138
1799.572563	145.035742	48.207143
1795.854155	142.474264	48.212148
1792.302104	146.203517	48.217153
1788.898904	140.838473	48.222157
1785.421503	133.164196	48.227162
1781.732718	136.482093	48.232167
1778.405832	137.426804	48.237172
1774.355446	145.503876	48.242177
1771.256956	129.971332	48.247181
1767.932535	138.142395	48.252186
1764.206906	132.967000	48.257191
1760.946640	136.790155	48.262196
1757.031751	138.437059	48.267201
1753.768382	134.754745	48.272205
1750.469266	139.433672	48.277210
1746.733947	129.888637	48.282215
1743.367983	133.716831	48.287220
1739.740597	134.902434	48.292225
1736.410768	127.227500	48.297229
1732.594652	146.324383	48.302234
1729.259421	139.890223	48.307239
1725.758103	142.432632	48.312244
1722.118150	138.697900	48.317249
1719.065400	139.325034	48.322253
1715.245586	147.366035	48.327258
1711.709192	133.065841	48.332263
1708.245609	125.357774	48.337268
1704.621692	140.091524	48.342273
1701.390690	136.075133	48.347277
1698.012705	136.952564	48.352282
1694.391659	132.898003	48.357287
1690.881325	130.670667	48.362292
1686.976982	134.340780	48.367297
1683.357068	128.701805	48.372301
1680.442604	138.378573	48.377306
1676.907103	136.853393	48.382311
1673.242529	124.403752	48.387316
1669.784541	138.223662	48.392321
1666.351240	127.885228	48.397325
1662.817272	135.342075	48.402330
1659.185686	138.859596	48.407335
1656.075842	135.106599	48.412340
1652.195051	141.444027	48.417345
1648.547616	132.615304	48.422349
1645.139524	124.129486	48.427354
1641.391717	130.784172	48.432359
1637.952315	132.255717	48.437364
1634.621131	133.481459	48.442369
1631.248035	127.088763	48.447373
1627.664582	137.725241	48.452378
1624.444604	126.593224	48.457383
1620.905725	125.521341	48.462388
1617.271266	127.356856	48.467393
1613.977548	128.597734	48.472397
1610.282092	124.176254	48.477402
1606.735796	131.755946	48.482407
1603.425899	128.365006	48.487412
1599.300842	122.954812	48.492417
1596.408377	120.037587	48.497421
1592.731611	129.930735	48.502426
1588.798941	126.284936	48.507431
1585.383599	124.998684	48.512436
1582.065997	125.364584	48.517441
1578.650220	116.988237	48.522445
1575.006419	129.842537	48.527450
1571.640196	133.335810	48.532455
1567.987212	119.804122	48.537460
1564.472742	128.299363	48.542465
1561.676531	120.701569	48.547469
1557.691119	135.064941	48.552474
1553.889276	123.389952	48.557479
1550.725349	129.237606	48.562484
1546.775075	135.989164	48.567489
1543.889086	119.790615	48.572493
1540.553048	123.403243	48.577498
1536.753448	124.876364	48.582503
1533.199896	120.350593	48.587508
1529.442893	129.698377	48.592513
1525.852945	125.522782	48.597517
1522.397340	133.434071	48.602522
1519.184692	122.733102	48.607527
1515.488515	122.529140	48.612532
1511.749271	135.667243	48.617537
1508.583366	126.925034	48.622541
1505.283187	126.312074	48.627546
1501.723579	122.386053	48.632551
1498.246113	121.041459	48.637556
1494.723035	133.177878	48.642561
1491.215942	120.956554	48.647565
1487.606469	122.491637	48.652570
1484.088571	127.092039	48.657575
1480.609852	116.313121	48.662580
1476.828651	124.771392	48.667585
1473.461680	119.666629	48.672589
1469.911837	126.189659	48.677594
1466.797381	123.921940	48.682599
1463.602007	121.823099	48.687604
1459.719418	131.103478	48.692609
1456.477828	125.292649	48.697613
1452.557190	126.225401	48.702618
1448.664917	126.327016	48.707623
1445.596577	122.337216	48.712628
1441.589455	128.617730	48.717633
1438.729791	124.609826	48.722637
1434.961442	126.642450	48.727642
1431.451874	129.316085	48.732647
1428.098381	121.506385	48.737652
1424.676504	124.076334	48.742657
1421.242076	123.568899	48.747661
1417.408720	124.195787	48.752666
1413.739554	123.915808	48.757671
1410.882976	127.421063	48.762676
1407.107490	137.560754	48.767681
1403.725600	122.919970	48.772685
1400.026584	133.130301	48.777690
1396.446683	132.325463	48.782695
1393.208135	130.796023	48.787700
1389.098798	139.913045	48.792705
1386.003083	126.986810	48.797709
1382.247346	134.651593	48.802714
1379.153612	133.722211	48.807719
1375.369390	126.291984	48.812724
1371.737681	127.815438	48.817729
1368.737964	120.490586	48.822733
1365.208877	127.872429	48.827738
1361.475597	124.716033	48.832743
1358.394907	126.709257	48.837748
1354.337610	131.136251	48.842753
1350.794013	125.338321	48.847757
1347.436993	122.089948	48.852762
1343.900299	125.686936	48.857767
1340.257725	131.187388	48.862772
1336.518391	135.412457	48.867777
1333.150693	120.322421	48.872781
1329.894135	125.987986	48.877786
1326.918527	127.232922	48.882791
1323.392567	128.703018	48.887796
1319.462547	133.179651	48.892801
1316.038746	125.969136	48.897805
1312.423488	121.770669	48.902810
1308.899784	122.589583	48.907815
1305.729285	122.022821	48.912820
1301.953755	126.065242	48.917825
1298.574643	124.827091	48.922829
1295.210858	125.740746	48.927834
1291.403588	120.652863	48.932839
1287.952668	116.060204	48.937844
1284.198009	134.286797	48.942849
1280.834804	125.954098	48.947853
1277.445302	118.281507	48.952858
1273.765966	124.131844	48.957863
1270.426215	116.460114	48.962868
1266.412991	121.667863	48.967873
1263.458897	114.686613	48.972877
1259.822554	117.964462	48.977882
1256.193952	123.307753	48.982887
1253.074055	123.939976	48.987892
1249.392566	126.808323	48.992897
1246.169104	127.361370	48.997901
1242.390724	120.238543	49.002906
1238.884288	120.154006	49.007911
1235.406151	107.392955	49.012916
1231.533486	115.761734	49.017921
1228.024649	122.211848	49.022925
1224.695585	120.561726	49.027930
1221.282241	126.565666	49.032935
1218.345869	107.221474	49.037940
1214.523362	123.028708	49.042945
1210.724226	113.930047	49.047949
1207.045028	121.483828	49.052954
1203.909393	124.087327	49.057959
1200.654060	114.712488	49.062964
1197.308522	121.819993	49.067969
1193.632268	116.964117	49.072973
1189.613003	124.276943	49.077978
1186.169851	114.268730	49.082983
1182.631667	120.273797	49.087988
1179.169056	133.114783	49.092993
1175.696454	125.637758	49.097997
1172.298615	121.470361	49.103002
1168.993142	112.034573	49.108007
1165.310572	114.576766	49.113012
1161.689946	109.450054	49.118017
1158.120384	114.420751	49.123021
1154.673053	118.101771	49.128026
1150.961387	110.880976	49.133031
1148.093285	113.402785	49.138036
1144.404733	113.113796	49.143041
1141.051454	118.022107	49.148045
1137.355888	113.057584	49.153050
1133.559226	116.373678	49.158055
1130.711308	110.613659	49.163060
1126.544587	119.344706	49.168065
1123.079195	107.162611	49.173069
1119.396305	112.670281	49.178074
1116.462129	117.237385	49.183079
1112.853174	111.934140	49.188084
1109.129862	115.800341	49.193089
1105.927877	111.449851	49.198093
1102.020245	114.486141	49.203098
1098.605349	107.413664	49.208103
1095.638857	117.719562	49.213108
1091.920571	109.046920	49.218113
1088.447011	103.751308	49.223117
1084.607579	112.824130	49.228122
1081.162644	113.338924	49.233127
1078.009328	103.549690	49.238132
1074.162018	117.422276	49.243137
1070.833030	109.476410	49.248141
1067.015885	116.792616	49.253146
1063.425432	114.080944	49.258151
1060.334486	114.138996	49.263156
1056.404574	112.252878	49.268161
1053.295246	104.654332	49.273165
1049.971476	103.544764	49.278170
1046.226131	113.444687	49.283175
1042.852568	111.050602	49.288180
1039.269925	114.127138	49.293185
1035.961665	113.709248	49.298189
1032.100682	121.861548	49.303194
1028.268091	112.363457	49.308199
1024.980365	111.205520	49.313204
1021.783863	117.887507	49.318209
1018.300330	116.921992	49.323213
1014.938447	121.666643	49.328218
1011.058710	114.641895	49.333223
1007.639420	112.700985	49.338228
1004.005056	120.879375	49.343233
1000.561700	113.013059	49.348237
997.309422	111.082231	49.353242
993.448305	108.497469	49.358247
990.379354	112.998726	49.363252
986.694560	111.652900	49.368257
983.174003	116.479065	49.373261
979.831063	108.557880	49.378266
976.021130	116.265861	49.383271
972.900803	111.722392	49.388276
969.129631	118.942665	49.393281
965.500384	122.812368	49.398285
961.977324	110.616272	49.403290
958.346757	115.262126	49.408295
955.023192	97.416647	49.413300
951.455914	119.112412	49.418305
948.492813	105.421847	49.423309
945.022672	99.446951	49.428314
941.146973	100.840591	49.433319
937.642593	104.059763	49.438324
933.813075	111.244716	49.443329
930.483232	105.702870	49.448333
926.892158	109.812169	49.453338
923.465160	104.181217	49.458343
920.380013	100.117817	49.463348
916.835779	113.096181	49.468353
912.671245	111.733061	49.473357
909.568721	100.064811	49.478362
905.935744	109.831993	49.483367
902.804617	101.519258	49.488372
898.871882	112.984376	49.493377
895.644597	98.108736	49.498381
892.333921	99.797527	49.503386
888.621866	103.658090	49.508391
885.126289	100.420171	49.513396
881.228742	104.302340	49.518401
877.666717	107.357040	49.523405
874.158522	105.656496	49.528410
870.810499	108.648180	49.533415
868.227595	100.697888	49.538420
864.403671	115.982052	49.543425
860.615342	113.113439	49.548429
857.140855	109.117041	49.553434
853.399193	120.575856	49.558439
849.912636	109.548967	49.563444
846.234753	114.538600	49.568449
843.219130	96.472190	49.573453
839.687639	107.743899	49.578458
836.076606	108.763513	49.583463
832.418520	98.969167	49.588468
828.800634	107.064439	49.593473
825.171130	100.761388	49.598477
821.709930	105.151999	49.603482
818.080176	105.550548	49.608487
815.299494	103.639931	49.613492
811.605774	113.329216	49.618497
808.159068	111.898772	49.623501
804.746363	109.628762	49.628506
800.652566	109.145221	49.633511
797.143347	107.389654	49.638516
793.734110	107.255051	49.643521
790.548084	105.521413	49.648525
787.642929	106.318140	49.653530
783.873607	109.105079	49.658535
780.181601	101.786256	49.663540
776.182057	108.655300	49.668545
772.825381	99.329951	49.673549
769.298058	107.388184	49.678554
765.736716	104.494739	49.683559
762.529109	102.199915	49.688564
758.512428	109.802744	49.693569
755.620939	104.018031	49.698573
751.889023	107.671036	49.703578
748.506350	103.448984	49.708583
745.256549	98.313589	49.713588
741.440828	106.175442	49.718593
738.054477	99.647540	49.723597
734.708417	101.023206	49.728602
730.636430	92.117559	49.733607
727.046669	95.920721	49.738612
723.698837	109.287244	49.743617
719.739293	97.943263	49.748621
716.849398	98.257392	49.753626
713.202120	104.584344	49.758631
710.027960	89.658451	49.763636
706.053637	93.154057	49.768641
703.049105	95.484992	49.773645
699.863946	102.639898	49.778650
695.844316	107.096934	49.783655
692.408003	104.922090	49.788660
688.986042	108.380011	49.793665
685.687605	99.349789	49.798669
681.859034	104.901231	49.803674
677.958298	100.230358	49.808679
674.623873	100.960829	49.813684
671.087311	94.084278	49.818689
667.601095	107.454388	49.823693
664.522385	95.797599	49.828698
660.720022	105.176202	49.833703
658.065390	96.059822	49.838708
653.833711	96.004756	49.843713
650.299230	98.806825	49.848717
646.315411	100.779830	49.853722
643.188444	98.486950	49.858727
640.086236	97.903644	49.863732
636.259300	97.840242	49.868737
633.114843	93.607490	49.873741
629.407372	97.223593	49.878746
625.725519	102.563730	49.883751
622.593028	103.906909	49.888756
618.631400	100.802163	49.893761
615.550470	90.775190	49.898765
611.769746	100.095783	49.903770
607.957614	97.628376	49.908775
604.604787	95.390852	49.913780
601.188037	95.325723	49.918785
597.776793	94.716616	49.923789
594.624064	94.449546	49.928794
590.690362	94.900149	49.933799
587.260928	89.771910	49.938804
583.709314	90.430441	49.943809
580.630104	97.335627	49.948813
576.927431	93.449842	49.953818
572.957981	94.954033	49.958823
570.138916	101.627926	49.963828
566.231224	97.660038	49.968833
562.578067	92.486349	49.973837
559.088392	94.817927	49.978842
555.731532	96.431922	49.983847
552.404897	92.588922	49.988852
548.529552	104.984915	49.993857
545.245020	90.625235	49.998861
541.701449	87.290759	50.003866
537.801705	97.740128	50.008871
534.963648	93.173378	50.013876
531.503005	92.914481	50.018881
528.122766	86.675439	50.023885
524.152849	91.538603	50.028890
520.212279	98.398888	50.033895
517.028678	93.662194	50.038900
513.635227	99.052773	50.043905
510.246338	93.624055	50.048909
506.844381	91.106233	50.053914
502.969337	94.806604	50.058919
499.345118	93.326454	50.063924
496.016695	93.991734	50.068929
492.859387	96.088986	50.073933
489.496984	95.060636	50.078938
485.656122	94.514027	50.083943
482.343292	96.632681	50.088948
478.139939	104.529680	50.093953
475.105348	93.938270	50.098957
471.659942	96.602205	50.103962
468.447553	96.453831	50.108967
464.938612	93.988675	50.113972
460.857776	95.560929	50.118977
457.372312	89.323375	50.123981
454.134628	83.198153	50.128986
450.790629	83.624309	50.133991
447.423051	90.552829	50.138996
443.298095	97.272404	50.144001
439.920314	88.797018	50.149005
436.515155	93.225604	50.154010
433.303454	98.311274	50.159015
429.906024	97.153591	50.164020
426.334406	98.718173	50.169025
422.699184	99.679570	50.174029
419.136901	90.049143	50.179034
415.284496	99.748398	50.184039
412.172621	94.831983	50.189044
408.623689	101.186109	50.194049
404.922841	92.896235	50.199053
401.352100	88.468597	50.204058
397.709495	94.045139	50.209063
394.443288	92.146678	50.214068
390.966358	97.917218	50.219073
387.622106	90.647969	50.224077
384.279540	83.646823	50.229082
380.560053	95.581228	50.234087
377.422555	90.236720	50.239092
373.357245	89.514237	50.244097
369.992164	92.221393	50.249101
366.412503	94.078424	50.254106
362.922677	95.900462	50.259111
359.806721	87.710180	50.264116
355.949002	95.934487	50.269121
352.720114	85.771788	50.274125
349.102458	88.251992	50.279130
345.227386	91.745497	50.284135
342.467947	89.908637	50.289140
338.237747	98.318734	50.294145
334.851366	90.142642	50.299149
331.847152	89.229970	50.304154
328.179525	93.633208	50.309159
324.703473	85.685289	50.314164
320.642483	94.394773	50.319169
317.381218	92.506406	50.324173
314.019965	90.750429	50.329178
310.493477	86.009480	50.334183
307.046244	87.612770	50.339188
303.147790	92.106923	50.344193
300.174596	88.579380	50.349197
296.339211	82.277146	50.354202
292.624481	88.917110	50.359207
289.442013	73.618440	50.364212
286.008733	98.423104	50.369217
282.637117	88.486159	50.374221
278.970237	88.065057	50.379226
275.654440	81.482266	50.384231
272.106763	81.709221	50.389236
268.658073	89.567915	50.394241
265.034020	90.813731	50.399245
261.421387	89.595901	50.404250
257.827391	85.386152	50.409255
254.590097	83.717054	50.414260
250.985526	93.345021	50.419265
247.227698	90.271029	50.424269
243.896160	82.382143	50.429274
240.040086	82.289579	50.434279
237.006111	82.412978	50.439284
233.477222	88.351286	50.444289
230.010117	89.921815	50.449293
226.711127	90.834425	50.454298
222.888467	92.225634	50.459303
219.638243	84.905841	50.464308
215.588253	89.508823	50.469313
212.283568	86.030695	50.474317
209.037132	86.877787	50.479322
205.189553	84.382083	50.484327
201.888125	83.953435	50.489332
198.387339	88.886629	50.494337
194.776947	85.124245	50.499341
191.314565	84.725211	50.504346
187.970326	88.293381	50.509351
184.406384	81.999600	50.514356
180.640742	88.339843	50.519361
177.604806	94.789777	50.524365
174.129788	84.469460	50.529370
170.383395	100.221386	50.534375
166.887059	87.388973	50.539380
163.411482	89.763519	50.544385
159.727971	91.374075	50.549389
156.081946	86.854924	50.554394
152.526739	89.448285	50.559399
149.635356	90.209606	50.564404
145.917665	98.314406	50.569409
142.277108	92.675076	50.574413
138.684895	88.276286	50.579418
135.198492	94.328801	50.584423
132.016164	91.262840	50.589428
128.345983	94.814373	50.594433
124.556684	97.289829	50.599437
121.329571	96.652394	50.604442
117.920675	92.472900	50.609447
114.215755	79.234628	50.614452
110.779548	93.465484	50.619457
106.978283	85.397752	50.624461
103.713076	89.574703	50.629466
100.048565	94.252300	50.634471
97.126869	81.686534	50.639476
93.304408	93.406725	50.644481
89.875286	91.783132	50.649485
86.315374	95.920287	50.654490
82.623556	93.454555	50.659495
79.290062	87.645056	50.664500
75.577045	87.151848	50.669505
72.098886	93.378476	50.674509
68.938792	100.300147	50.679514
65.234803	104.215692	50.684519
61.851944	94.423279	50.689524
58.142826	101.547555	50.694529
54.821319	100.204738	50.699533
51.649443	93.811029	50.704538
47.660400	92.513826	50.709543
44.516628	80.186749	50.714548
40.699123	91.299552	50.719553
36.959509	89.063777	50.724557
33.879678	84.055331	50.729562
29.985002	91.937134	50.734567
26.791332	89.220247	50.739572
23.229675	89.210948	50.744577
19.723787	91.444402	50.749581
16.370546	90.414912	50.754586
12.504371	88.645106	50.759591
9.120775	89.715356	50.764596
5.557921	88.884964	50.769601
1.843148	85.984037	50.774605