Tue Jun 21 13:01:03 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
1.089502	127.675117	0.000000
1.137742	114.916405	0.005005
0.570200	110.891085	0.010010
0.464443	98.794686	0.015014
0.540787	92.031492	0.020019
0.494770	96.483540	0.025024
0.356889	87.678285	0.030029
0.202621	83.248873	0.035034
0.270554	79.960753	0.040038
0.061671	55.691343	0.045043
-0.000674	52.604968	0.050048
-0.661622	27.757088	0.055053
-0.900107	31.082837	0.060058
-1.491676	10.740858	0.065062
-1.606370	8.991806	0.070067
-2.347529	7.573227	0.075072
-2.734031	-4.520213	0.080077
-3.304975	-2.730713	0.085082
-3.739244	2.264527	0.090086
-3.538147	1.745849	0.095091
-4.004731	3.293109	0.100096
-3.583363	3.316142	0.105101
-3.477797	2.129721	0.110106
-4.153301	-1.601423	0.115110
-4.556094	-3.385844	0.120115
-5.013833	9.371835	0.125120
-4.999884	-8.319955	0.130125
-5.836176	0.519010	0.135130
-6.568424	-3.507617	0.140134
-5.786315	-3.905242	0.145139
-6.345367	3.209497	0.150144
-6.337893	0.122424	0.155149
-6.597745	0.041985	0.160154
-6.615978	-5.641681	0.165158
-7.019862	-5.764968	0.170163
-7.869851	4.029781	0.175168
-7.696415	-6.039190	0.180173
-7.898935	-2.543185	0.185178
-7.914449	-4.036734	0.190182
-8.013632	-4.352162	0.195187
-9.068042	-1.202502	0.200192
-9.175335	0.222707	0.205197
-9.316451	-5.265773	0.210202
-9.723492	-6.347773	0.215206
-9.123510	-9.169670	0.220211
-9.682914	-2.780863	0.225216
-10.359173	0.102530	0.230221
-10.813069	-3.484354	0.235226
-10.985954	2.092951	0.240230
-11.034772	-5.504519	0.245235
-11.372105	2.847488	0.250240
-11.193220	-1.420000	0.255245
-11.043586	-3.552433	0.260250
-12.070725	-2.067649	0.265254
-12.405486	-12.309783	0.270259
-12.792443	3.486149	0.275264
-12.846205	-6.205785	0.280269
-12.879753	-2.425185	0.285274
-13.145157	1.767165	0.290278
-13.460682	2.327806	0.295283
-14.094336	-2.753908	0.300288
-14.214060	-4.538435	0.305293
-14.362898	-7.268496	0.310298
-14.625552	-4.044720	0.315302
-14.493960	-13.995657	0.320307
-14.727277	0.382251	0.325312
-15.032053	-6.708704	0.330317
-15.732376	-6.318379	0.335322
-15.746971	0.702845	0.340326
-15.919640	1.486892	0.345331
-16.189108	7.049606	0.350336
-16.309602	-8.904303	0.355341
-16.568040	-1.837175	0.360346
-17.333633	-0.648287	0.365350
-17.316903	2.372149	0.370355
-18.048668	8.234799	0.375360
-17.647351	-6.472535	0.380365
-17.414193	-4.144466	0.385370
-18.063894	2.326389	0.390374
-18.624641	-1.031063	0.395379
-18.849001	-2.451548	0.400384
-19.018171	9.333839	0.405389
-19.142145	4.087408	0.410394
-19.164257	4.284715	0.415398
-19.670865	4.225603	0.420403
-20.424022	1.931869	0.425408
-20.454933	-12.660470	0.430413
-20.603606	-1.252629	0.435418
-21.009539	6.573204	0.440422
-20.819219	-2.252800	0.445427
-20.948343	0.945906	0.450432
-21.149665	2.969609	0.455437
-21.968540	-7.750023	0.460442
-22.077697	6.099986	0.465446
-22.377928	1.728712	0.470451
-22.669965	3.475778	0.475456
-22.290532	1.779483	0.480461
-22.907231	9.403025	0.485466
-23.455800	12.224429	0.490470
-23.613759	5.751477	0.495475
-24.106110	6.798622	0.500480
-23.987949	-2.306104	0.505485
-24.012249	-2.309122	0.510490
-24.430199	3.285875	0.515494
-25.006732	-2.323493	0.520499
-25.568282	6.435250	0.525504
-25.399068	4.336279	0.530509
-25.658724	-2.388597	0.535514
-25.775550	10.303550	0.540518
-25.506242	-4.133088	0.545523
-25.731996	-0.552525	0.550528
-26.363429	4.491745	0.555533
-26.989999	-1.026062	0.560538
-27.177604	4.190983	0.565542
-27.201364	-10.687490	0.570547
-27.407820	2.321807	0.575552
-27.441654	2.066203	0.580557
-28.070751	-6.006649	0.585562
-28.755420	10.051709	0.590566
-28.804403	2.394276	0.595571
-28.910880	4.200993	0.600576
-28.903864	4.362101	0.605581
-28.952941	-0.916858	0.610586
-29.324531	4.752750	0.615590
-30.026694	1.948755	0.620595
-30.607664	-0.422824	0.625600
-30.539304	-2.139632	0.630605
-30.548352	13.093685	0.635610
-30.613197	7.102988	0.640614
-30.409890	12.774091	0.645619
-31.315628	6.879034	0.650624
-31.646534	1.398302	0.655629
-32.350155	0.499998	0.660634
-32.264950	1.059006	0.665638
-31.898839	2.898167	0.670643
-32.224927	-1.572621	0.675648
-32.167126	5.360051	0.680653
-32.819163	2.993925	0.685658
-33.385693	7.514383	0.690662
-33.316244	1.591236	0.695667
-33.726928	3.879305	0.700672
-34.302594	0.519393	0.705677
-34.468935	2.287874	0.710682
-35.183616	8.259980	0.715686
-34.795539	-5.617940	0.720691
-34.636623	1.799211	0.725696
-35.354292	-0.481453	0.730701
-35.003567	1.652901	0.735706
-35.569821	2.253091	0.740710
-35.892387	-0.512729	0.745715
-36.529186	8.883036	0.750720
-36.275453	-1.151676	0.755725
-36.389557	1.355061	0.760730
-37.577180	6.908206	0.765734
-37.601416	-8.524103	0.770739
-38.329097	3.743895	0.775744
-38.058756	-1.743063	0.780749
-38.235368	1.215064	0.785754
-38.270847	0.899941	0.790758
-38.109534	-10.336217	0.795763
-38.007297	4.034274	0.800768
-38.815211	-2.718998	0.805773
-39.601087	-1.958117	0.810778
-39.759257	5.011897	0.815782
-39.864557	5.364468	0.820787
-39.734967	1.612683	0.825792
-40.334554	6.091848	0.830797
-41.035446	11.017186	0.835802
-41.457718	14.596947	0.840806
-41.392370	8.172264	0.845811
-41.530713	8.427299	0.850816
-41.540174	8.631195	0.855821
-41.454879	3.296239	0.860826
-42.015703	10.079165	0.865830
-41.918011	0.017605	0.870835
-42.442269	12.746440	0.875840
-42.971642	5.109754	0.880845
-42.989200	-0.309597	0.885850
-43.311406	12.376108	0.890854
-43.064685	4.963140	0.895859
-43.744867	6.963531	0.900864
-44.126397	4.737512	0.905869
-44.584813	-4.005921	0.910874
-44.914161	6.726181	0.915878
-44.715745	-2.904308	0.920883
-44.857864	3.396653	0.925888
-45.080556	-5.930455	0.930893
-45.512658	-2.777874	0.935898
-46.456393	3.332407	0.940902
-46.396881	-0.962870	0.945907
-46.684521	-4.856705	0.950912
-46.588826	-5.824623	0.955917
-46.347803	-4.611410	0.960922
-46.577734	-6.161605	0.965926
-46.910296	-1.417441	0.970931
-47.455765	8.965061	0.975936
-47.498910	1.417169	0.980941
-47.806437	-2.693202	0.985946
-48.834682	6.236758	0.990950
-48.967346	-1.143572	0.995955
-49.327399	9.157313	1.000960
-49.682431	3.863309	1.005965
-49.344958	4.624246	1.010970
-49.500950	9.266949	1.015974
-49.224913	6.305700	1.020979
-49.323197	12.332808	1.025984
-50.232112	14.281096	1.030989
-50.794405	-2.546059	1.035994
-51.062756	10.354304	1.040998
-50.984918	2.891950	1.046003
-51.540658	10.644913	1.051008
-51.257639	6.046024	1.056013
-51.593388	-3.856335	1.061018
-52.460039	5.641035	1.066022
-52.473963	5.258406	1.071027
-52.814498	3.249376	1.076032
-53.015290	-2.499960	1.081037
-52.441835	0.772033	1.086042
-53.110635	7.948956	1.091046
-53.880616	-1.534778	1.096051
-54.101473	-0.203241	1.101056
-54.029196	1.395484	1.106061
-54.141821	6.152166	1.111066
-54.296963	6.636523	1.116070
-54.645433	4.196844	1.121075
-55.575961	14.015005	1.126080
-56.199085	1.843937	1.131085
-55.979132	-0.182531	1.136090
-56.076083	6.706503	1.141094
-56.108782	0.586561	1.146099
-56.408870	-0.395141	1.151104
-56.358716	-2.336460	1.156109
-56.067797	-8.694102	1.161114
-56.904593	7.998811	1.166118
-57.107332	2.011024	1.171123
-57.488790	0.999581	1.176128
-58.108979	1.325138	1.181133
-57.970644	8.903565	1.186138
-58.501465	-2.854573	1.191142
-58.429958	-2.007756	1.196147
-58.995066	5.280459	1.201152
-59.010672	7.448639	1.206157
-58.708047	1.239028	1.211162
-59.552505	9.753362	1.216166
-60.180048	1.744784	1.221171
-60.520246	2.762789	1.226176
-60.640564	6.401669	1.231181
-60.451521	-2.152985	1.236186
-60.914851	-0.186531	1.241190
-60.569147	-8.416071	1.246195
-61.214372	-6.558615	1.251200
-62.042720	-5.823257	1.256205
-61.875886	-8.205599	1.261210
-62.259795	-0.694808	1.266214
-62.361325	-8.269333	1.271219
-62.076845	-3.926513	1.276224
-62.760197	-4.035086	1.281229
-63.288861	-8.814890	1.286234
-64.011580	-2.940516	1.291238
-63.479520	-10.163931	1.296243
-63.988355	-1.854565	1.301248
-64.003677	-3.950208	1.306253
-63.926342	-1.394664	1.311258
-64.556176	2.399042	1.316262
-64.843710	-2.244872	1.321267
-65.243918	10.801449	1.326272
-65.433528	6.981362	1.331277
-65.063611	0.068757	1.336282
-65.990219	7.868931	1.341286
-66.434680	4.270031	1.346291
-66.860541	-0.354528	1.351296
-66.775901	2.631177	1.356301
-67.190563	7.876156	1.361306
-67.397539	8.646745	1.366310
-66.842789	-4.219028	1.371315
-67.103580	6.208285	1.376320
-67.900972	0.657207	1.381325
-68.078871	-8.124979	1.386330
-68.830311	9.031740	1.391334
-68.630610	0.927410	1.396339
-68.863087	2.961207	1.401344
-68.866491	-1.536967	1.406349
-68.829110	-5.536722	1.411354
-69.595508	0.107101	1.416358
-70.237448	-12.546078	1.421363
-70.462819	-7.218986	1.426368
-70.386039	-0.952108	1.431373
-70.191314	-5.673321	1.436378
-70.574481	6.172165	1.441382
-71.366103	-0.429680	1.446387
-71.870549	-6.721908	1.451392
-71.930130	-1.176195	1.456397
-72.025660	2.932967	1.461402
-72.230519	11.367428	1.466406
-71.891518	6.551080	1.471411
-72.026688	1.079971	1.476416
-72.807311	1.462292	1.481421
-73.118170	-3.598670	1.486426
-73.352669	4.383278	1.491430
-73.597774	1.281993	1.496435
-74.072632	-0.953034	1.501440
-74.943300	-4.043662	1.506445
-74.426987	2.956334	1.511450
-75.099298	5.681612	1.516454
-74.987357	-9.383904	1.521459
-74.955848	0.942507	1.526464
-75.378741	-1.435905	1.531469
-75.380773	-7.054761	1.536474
-75.531640	7.427301	1.541478
-76.159485	-10.894238	1.546483
-76.701021	-4.411892	1.551488
-76.934386	-6.765253	1.556493
-76.959270	-2.037312	1.561498
-77.326829	2.793161	1.566502
-76.994406	-6.765388	1.571507
-77.175980	3.132975	1.576512
-77.770982	4.697760	1.581517
-78.046423	-4.499643	1.586522
-78.620057	4.945059	1.591526
-78.365904	-6.776718	1.596531
-78.980954	5.684368	1.601536
-79.768039	-3.897164	1.606541
-79.918696	-0.908802	1.611546
-79.835659	1.940021	1.616550
-79.776106	-1.155082	1.621555
-80.210409	4.826834	1.626560
-80.408843	6.735015	1.631565
-80.160279	-0.036528	1.636570
-80.708201	2.403723	1.641574
-81.114565	5.349581	1.646579
-81.365418	1.711122	1.651584
-81.778385	3.482758	1.656589
-81.796963	6.002880	1.661594
-82.127935	4.608738	1.666598
-81.984295	-2.271326	1.671603
-82.874093	4.518721	1.676608
-83.243602	0.185765	1.681613
-83.201090	-5.202879	1.686618
-83.582009	-0.234034	1.691622
-83.419332	-0.182769	1.696627
-83.863000	1.476143	1.701632
-84.324461	7.096701	1.706637
-84.511834	8.223190	1.711642
-84.870950	2.842647	1.716646
-84.932646	6.168517	1.721651
-84.727779	8.416216	1.726656
-84.943400	6.346838	1.731661
-85.664217	0.855109	1.736666
-86.369341	13.115828	1.741670
-86.451123	0.239832	1.746675
-86.488335	7.357941	1.751680
-86.860614	2.121460	1.756685
-86.470300	1.289059	1.761690
-86.733865	4.146543	1.766694
-87.362038	0.120851	1.771699
-87.958998	9.180475	1.776704
-88.073612	11.232840	1.781709
-87.980319	-8.170916	1.786714
-88.228945	7.192047	1.791718
-88.513858	0.552860	1.796723
-89.052157	-4.516411	1.801728
-89.534759	0.894921	1.806733
-89.915052	-1.450880	1.811738
-90.078969	8.545596	1.816742
-89.729089	-0.668542	1.821747
-90.066918	-0.275289	1.826752
-90.073446	-0.358999	1.831757
-90.027666	0.159176	1.836762
-90.660049	-0.342238	1.841766
-90.682057	-3.164143	1.846771
-91.844440	-4.929710	1.851776
-92.108909	-3.245617	1.856781
-92.287626	-3.401450	1.861786
-92.781193	2.985538	1.866790
-93.032365	1.134773	1.871795
-92.455633	-0.124550	1.876800
-92.673491	1.529526	1.881805
-92.649421	-5.625943	1.886810
-93.050462	-0.801174	1.891814
-93.574403	-11.632772	1.896819
-94.028169	1.532916	1.901824
-94.639458	1.672893	1.906829
-94.453356	-5.037193	1.911834
-94.345109	3.683834	1.916838
-94.602017	-6.081599	1.921843
-95.319735	2.638283	1.926848
-95.893333	-0.341108	1.931853
-96.081722	-6.597466	1.936858
-96.343975	1.321390	1.941862
-96.287814	-2.712455	1.946867
-96.283780	-10.813973	1.951872
-96.720739	-5.534916	1.956877
-96.327493	-8.928593	1.961882
-97.405616	7.029558	1.966886
-97.857553	-1.406507	1.971891
-97.820973	-4.839388	1.976896
-98.197839	-5.960514	1.981901
-97.753594	3.122620	1.986906
-97.915811	0.014715	1.991910
-98.385893	-5.199841	1.996915
-99.121103	-2.689354	2.006912
-98.704294	-7.529557	2.016909
-98.094429	-4.888145	2.026906
-97.915029	-0.533110	2.036902
-97.212892	-2.731823	2.046899
-96.761916	-10.399405	2.056896
-96.401384	-0.002759	2.066893
-95.518447	4.672427	2.076890
-95.341733	0.308846	2.086886
-94.566931	-0.673116	2.096883
-93.885079	-1.538125	2.106880
-93.714491	-0.774527	2.116877
-93.561215	-3.525482	2.126874
-92.496570	0.268609	2.136870
-92.486556	1.579438	2.146867
-91.482998	-3.126369	2.156864
-91.172174	-1.832361	2.166861
-90.876001	-6.802751	2.176858
-89.777289	-0.229529	2.186854
-89.305847	-3.055702	2.196851
-89.129102	4.378754	2.206848
-89.061721	1.286566	2.216845
-88.043321	0.989995	2.226842
-87.948844	-1.577940	2.236838
-87.087246	-1.284831	2.246835
-86.387496	3.399553	2.256832
-86.319409	6.595811	2.266829
-85.614927	-3.559869	2.276826
-84.867484	-7.479546	2.286822
-84.847719	-7.188886	2.296819
-84.336939	1.088473	2.306816
-83.884666	5.898212	2.316813
-83.038274	-2.722611	2.326810
-82.135346	3.754410	2.336806
-82.331839	-1.890748	2.346803
-81.841135	2.911639	2.356800
-81.152657	1.359319	2.366797
-80.375228	4.171361	2.376794
-80.181352	2.295704	2.386790
-79.883511	-3.255470	2.396787
-79.037610	3.931043	2.406784
-78.700393	2.692769	2.416781
-78.028137	-3.047261	2.426778
-77.372290	-5.353103	2.436774
-77.479149	-0.002444	2.446771
-76.540402	1.505886	2.456768
-75.885934	-1.899094	2.466765
-75.532599	-4.518394	2.476762
-75.335228	-4.324524	2.486758
-74.393197	-0.737345	2.496755
-73.952063	3.717795	2.506752
-73.750883	-3.455356	2.516749
-73.055420	0.770748	2.526746
-72.665921	-3.215709	2.536742
-72.245450	-8.387473	2.546739
-71.692408	-2.352004	2.556736
-70.897446	4.988766	2.566733
-70.678235	1.526449	2.576730
-69.834971	-4.494416	2.586726
-69.176140	-1.357659	2.596723
-69.107316	-9.502547	2.606720
-69.109795	0.183044	2.616717
-67.970220	-4.720345	2.626714
-67.450036	-4.857147	2.636710
-67.414353	-0.533632	2.646707
-66.413982	-3.384762	2.656704
-66.259201	-2.939424	2.666701
-65.870887	-8.307005	2.676698
-64.976464	-6.397742	2.686694
-64.566194	-4.082481	2.696691
-64.092984	-2.764386	2.706688
-63.308199	-3.940444	2.716685
-63.037044	0.277884	2.726682
-62.800900	-1.313728	2.736678
-61.789594	-8.217964	2.746675
-61.680124	-4.049326	2.756672
-61.100468	-0.219762	2.766669
-60.476049	-8.867836	2.776666
-60.268770	-11.824133	2.786662
-59.806544	-0.882982	2.796659
-58.970061	0.891641	2.806656
-58.292901	-0.965059	2.816653
-58.364324	-7.096837	2.826650
-57.390513	-10.571888	2.836646
-56.927278	-0.506997	2.846643
-57.022928	-3.202898	2.856640
-55.781998	-4.162660	2.866637
-55.449974	0.298104	2.876634
-55.372296	-1.740681	2.886630
-54.336355	-7.834745	2.896627
-54.026641	4.202385	2.906624
-53.772300	1.290059	2.916621
-52.589580	-2.611204	2.926618
-52.561057	-1.508928	2.936614
-52.428121	-1.855255	2.946611
-51.676950	1.273524	2.956608
-50.937464	1.958127	2.966605
-50.702004	-0.811180	2.976602
-49.400439	-1.120058	2.986598
-49.631014	1.627743	2.996595
-49.068854	8.996206	3.006592
-48.959435	7.815615	3.016589
-47.676489	4.386581	3.026586
-47.431461	4.081757	3.036582
-47.476455	3.326256	3.046579
-46.608808	5.642639	3.056576
-46.212832	5.369920	3.066573
-45.377000	1.514051	3.076570
-44.509675	1.456494	3.086566
-44.472938	0.672243	3.096563
-44.503599	2.512029	3.106560
-43.560913	3.447308	3.116557
-42.793741	3.507698	3.126554
-42.764309	0.994991	3.136550
-41.839222	2.056479	3.146547
-41.163736	-2.598151	3.156544
-41.101568	-2.563668	3.166541
-40.887557	-4.807203	3.176538
-40.061550	-1.093513	3.186534
-39.698726	5.057242	3.196531
-38.571650	1.153341	3.206528
-38.149179	8.114992	3.216525
-38.098478	1.851743	3.226522
-37.797497	-0.668194	3.236518
-36.946739	2.358543	3.246515
-36.571690	4.393537	3.256512
-36.088320	-1.244673	3.266509
-35.483749	4.959903	3.276506
-35.365342	3.290972	3.286502
-34.347956	0.540763	3.296499
-33.544397	2.801372	3.306496
-33.640229	-1.877273	3.316493
-33.471166	1.287643	3.326490
-32.618195	9.632434	3.336486
-32.003094	-2.017209	3.346483
-31.179185	0.141238	3.356480
-30.654964	5.577471	3.366477
-30.435193	-1.534743	3.376474
-30.263794	4.495177	3.386470
-29.317447	1.923890	3.396467
-28.828574	8.134587	3.406464
-28.721382	3.309695	3.416461
-28.050793	5.512106	3.426458
-27.175335	6.063351	3.436454
-27.175930	8.416229	3.446451
-26.819400	16.785935	3.456448
-25.943286	4.835412	3.466445
-25.649530	2.736739	3.476442
-24.528045	5.846090	3.486438
-24.071703	5.694377	3.496435
-24.149144	8.337193	3.506432
-23.922938	8.445479	3.516429
-22.915435	-1.303560	3.526426
-22.452776	-0.781168	3.536422
-22.037103	1.824248	3.546419
-20.959414	6.694230	3.556416
-20.506105	1.874262	3.566413
-20.456807	5.423164	3.576410
-20.312462	3.505919	3.586406
-19.922756	1.946574	3.596403
-19.004714	2.672745	3.606400
-18.206624	1.171636	3.616397
-17.455502	2.365275	3.626394
-17.446869	5.456386	3.636390
-17.514753	1.931951	3.646387
-16.488510	-1.277330	3.656384
-16.103449	3.896241	3.666381
-15.454641	4.297906	3.676378
-14.772219	3.690862	3.686374
-14.484734	7.923684	3.696371
-14.144409	8.889761	3.706368
-12.976931	8.343273	3.716365
-12.497241	3.902056	3.726362
-12.369053	8.875332	3.736358
-12.366198	9.841376	3.746355
-11.719212	16.225656	3.756352
-10.974513	7.356910	3.766349
-10.499223	12.789792	3.776346
-9.820264	9.140102	3.786342
-9.658795	7.848937	3.796339
-9.136761	11.579977	3.806336
-8.328340	7.615039	3.816333
-8.061135	4.833362	3.826330
-6.962852	0.075528	3.836326
-7.095218	1.768949	3.846323
-6.470977	-0.552001	3.856320
-5.930918	2.122327	3.866317
-4.882238	-2.018135	3.876314
-4.838289	0.042447	3.886310
-4.671643	6.274893	3.896307
-4.266601	8.093112	3.906304
-3.257348	4.507281	3.916301
-3.127599	8.728288	3.926298
-2.651073	7.841771	3.936294
-2.246368	20.738106	3.946291
-1.742722	34.765253	3.956288
-1.589079	54.302575	3.966285
-0.967436	64.908561	3.976282
-0.691988	87.735332	3.986278
-0.152017	120.651405	3.996275
0.000000	141.928447	4.001280
0.405295	143.308651	4.006285
0.409722	153.466989	4.011290
0.263908	172.980228	4.016294
1.069976	183.946933	4.021299
0.964223	187.504707	4.026304
0.834340	195.025032	4.031309
0.883226	197.904415	4.036314
1.103590	211.666695	4.041318
1.521494	210.245410	4.046323
1.558285	225.058720	4.051328
1.524212	224.198514	4.056333
1.413469	219.017701	4.061338
1.364822	220.424734	4.066342
1.696452	220.286210	4.071347
1.446930	217.638690	4.076352
1.100127	216.012311	4.081357
1.575735	223.041068	4.086362
1.139688	225.597797	4.091366
1.167838	223.142678	4.096371
1.169944	224.993798	4.101376
1.370823	223.214567	4.106381
1.476265	219.025682	4.111386
0.985255	229.755503	4.116390
1.517956	224.744213	4.121395
1.356783	222.465289	4.126400
1.835595	223.999878	4.131405
1.552617	221.546354	4.136410
1.574552	226.910719	4.141414
1.843851	218.943145	4.146419
1.545056	218.403045	4.151424
2.019672	226.296299	4.156429
1.885865	223.460894	4.161434
1.543952	226.889456	4.166438
1.787722	229.478853	4.171443
1.706864	225.677797	4.176448
1.761402	224.148945	4.181453
2.070132	228.985505	4.186458
1.863675	228.523257	4.191462
2.279213	218.864765	4.196467
2.047417	226.431976	4.201472
2.095498	226.377702	4.206477
2.016095	202.474387	4.211482
1.355066	203.306553	4.216486
1.907223	213.879805	4.221491
1.833749	217.747387	4.226496
1.699989	215.160422	4.231501
1.835488	212.729759	4.236506
1.683336	219.793200	4.241510
1.908848	213.930759	4.246515
1.788773	227.683516	4.251520
1.749426	227.782052	4.256525
2.127968	229.754361	4.261530
1.746546	226.248759	4.266534
1.960557	224.708103	4.271539
2.036871	231.733521	4.276544
1.865146	227.863446	4.281549
1.925393	230.149735	4.286554
1.763694	228.667149	4.291558
2.022486	226.712762	4.296563
1.609291	233.954217	4.301568
1.586090	223.971531	4.306573
1.971057	230.909529	4.311578
1.756576	226.305142	4.316582
1.791645	217.202403	4.321587
2.071014	232.328783	4.326592
1.705941	231.537595	4.331597
1.809355	231.698727	4.336602
1.795697	258.391383	4.341606
1.673507	261.925256	4.346611
1.786879	263.937335	4.351616
2.186074	263.061030	4.356621
2.001024	267.235803	4.361626
1.891448	255.492357	4.366630
2.281239	258.637748	4.371635
2.115965	262.890153	4.376640
2.239878	268.746775	4.381645
2.282128	268.578025	4.386650
2.204280	265.649675	4.391654
2.337805	262.375125	4.396659
2.257001	257.532313	4.401664
2.276249	260.575274	4.406669
2.301119	260.215222	4.411674
2.269534	265.172676	4.416678
2.557497	257.052213	4.421683
2.455206	260.796111	4.426688
2.113601	265.992370	4.431693
2.401509	257.316611	4.436698
2.166664	273.339037	4.441702
2.545454	259.915107	4.446707
2.222679	264.706273	4.451712
2.476491	259.750231	4.456717
2.169942	263.927362	4.461722
2.472710	265.973201	4.466726
2.384121	260.463297	4.471731
2.304236	268.930685	4.476736
2.328617	260.360920	4.481741
2.856404	257.687490	4.486746
2.598229	260.157542	4.491750
2.395592	259.019375	4.496755
2.034369	262.939155	4.501760
2.199508	263.220506	4.506765
2.796799	272.209803	4.511770
2.490419	276.767966	4.516774
2.847143	259.705644	4.521779
2.372676	265.180836	4.526784
1.983835	268.439180	4.531789
2.592023	276.577930	4.536794
2.622714	294.562730	4.541798
2.758248	294.316569	4.546803
2.529287	297.587517	4.551808
3.129236	290.087307	4.556813
2.899370	284.180856	4.561818
2.404728	276.758700	4.566822
2.601458	270.083240	4.571827
2.688550	274.522375	4.576832
2.531162	288.878111	4.581837
3.114379	292.027593	4.586842
2.791395	288.823895	4.591846
2.494104	271.940110	4.596851
2.958362	280.191695	4.601856
2.823937	267.425413	4.606861
2.603501	266.727095	4.611866
2.507943	278.486882	4.616870
3.042278	282.512738	4.621875
2.828247	288.409146	4.626880
2.850879	289.840495	4.631885
2.930601	279.239050	4.636890
2.737852	284.210764	4.641894
3.013652	287.490085	4.646899
2.720812	286.233452	4.651904
3.007663	285.232285	4.656909
2.981616	280.839996	4.661914
2.531931	291.272339	4.666918
3.184014	290.434472	4.671923
2.815582	292.491014	4.676928
2.742787	290.853591	4.681933
2.978608	287.911975	4.686938
2.702750	303.750595	4.691942
2.868697	290.024438	4.696947
3.115620	291.993291	4.701952
3.065711	287.960157	4.706957
3.304816	294.743353	4.711962
2.634716	296.528584	4.716966
2.849522	289.950764	4.721971
2.867864	307.150249	4.726976
2.634260	297.640642	4.731981
2.937516	291.598153	4.736986
2.957288	300.879647	4.741990
2.665145	294.092330	4.746995
2.843508	303.101682	4.752000
3.072469	315.666176	4.757005
3.481028	331.289074	4.762010
3.368126	340.562763	4.767014
3.329238	315.037160	4.772019
2.741839	305.932854	4.777024
2.663304	309.157386	4.782029
3.179471	319.936574	4.787034
2.807054	332.506337	4.792038
3.278047	327.358216	4.797043
3.385385	330.524148	4.802048
3.327179	339.700175	4.807053
3.186633	336.528221	4.812058
3.096828	336.373838	4.817062
3.546676	331.625274	4.822067
3.590421	336.222370	4.827072
3.653440	328.876766	4.832077
3.606396	327.213762	4.837082
3.366890	334.954972	4.842086
3.459713	331.668400	4.847091
3.422315	335.845383	4.852096
3.436009	334.200342	4.857101
3.693190	325.421690	4.862106
3.195188	320.530131	4.867110
3.539412	322.089780	4.872115
3.533556	332.167451	4.877120
3.339403	324.565665	4.882125
3.475243	319.062781	4.887130
3.308577	337.887421	4.892134
3.611023	336.270344	4.897139
3.489003	338.586041	4.902144
3.439675	331.755343	4.907149
3.738710	340.420115	4.912154
3.258236	339.012405	4.917158
3.654255	334.324062	4.922163
3.650160	338.219850	4.927168
3.858302	330.235507	4.932173
3.535915	321.010742	4.937178
3.339338	333.379902	4.942182
3.364019	332.986333	4.947187
3.463579	339.308390	4.952192
3.281385	334.039320	4.957197
3.739612	339.925465	4.962202
3.219565	337.753508	4.967206
3.551013	332.462927	4.972211
3.641746	337.777063	4.977216
3.483454	337.841620	4.982221
3.480665	333.365346	4.987226
3.164299	346.021349	4.992230
3.870310	345.614811	4.997235
3.921854	348.623630	5.002240
3.509048	351.753546	5.007245
3.874575	347.563197	5.012250
3.633033	353.275530	5.017254
3.957465	361.173003	5.022259
3.914812	360.528518	5.027264
3.570359	362.364422	5.032269
3.868324	359.867760	5.037274
3.712018	357.881648	5.042278
3.824095	358.662369	5.047283
3.529985	351.977180	5.052288
3.671341	363.366273	5.057293
4.102587	360.276445	5.062298
3.733739	365.196437	5.067302
4.073816	366.968718	5.072307
3.669567	361.608929	5.077312
3.894803	359.684355	5.082317
3.999557	355.579810	5.087322
3.784687	369.777600	5.092326
3.827885	356.347391	5.097331
4.202752	360.699825	5.102336
3.613122	365.836941	5.107341
3.884653	356.090321	5.112346
3.547362	368.169240	5.117350
3.802679	369.247903	5.122355
3.930223	375.675652	5.127360
4.209183	383.758270	5.132365
4.023905	388.274509	5.137370
3.603268	391.444802	5.142374
3.914933	389.283315	5.147379
3.817442	395.023315	5.152384
3.936188	388.255142	5.157389
3.779095	389.379207	5.162394
3.925596	389.457033	5.167398
4.080013	383.293519	5.172403
4.013430	392.059514	5.177408
3.891690	396.825917	5.182413
4.257022	407.634288	5.187418
4.364926	419.851271	5.192422
4.385282	418.978883	5.197427
4.265726	419.157995	5.202432
4.457353	413.505532	5.207437
4.656466	392.036744	5.212442
4.242461	408.168108	5.217446
3.996885	390.587314	5.222451
4.224240	408.144214	5.227456
4.129487	411.652067	5.232461
4.444306	419.415195	5.237466
4.455448	425.791593	5.242470
4.288136	425.459612	5.247475
4.295648	426.469593	5.252480
4.609641	422.061016	5.257485
4.608169	429.332067	5.262490
4.051999	414.772032	5.267494
4.616492	423.289092	5.272499
4.456286	423.054604	5.277504
4.343862	430.964066	5.282509
4.755467	426.315344	5.287514
4.356125	422.466335	5.292518
4.516125	417.433423	5.297523
4.596471	410.681071	5.302528
4.454449	415.815520	5.307533
4.560430	422.636405	5.312538
4.137556	428.234736	5.317542
4.267868	427.593971	5.322547
4.430087	431.982032	5.327552
4.558361	428.356659	5.332557
4.693214	424.991474	5.337562
4.413440	426.305962	5.342566
4.204414	422.698160	5.347571
4.233092	426.475073	5.352576
4.522830	429.733172	5.357581
4.494103	416.297653	5.362586
4.368971	432.915798	5.367590
4.194549	433.448351	5.372595
4.511570	445.864573	5.377600
4.858706	461.872521	5.382605
4.823958	464.271074	5.387610
4.828538	455.981544	5.392614
4.965202	461.697201	5.397619
4.837932	466.531439	5.402624
4.603539	465.563095	5.407629
4.582477	463.205877	5.412634
4.287588	464.729485	5.417638
4.603167	462.073992	5.422643
4.449527	469.789605	5.427648
4.541627	470.477536	5.432653
4.472322	454.921978	5.437658
4.767924	462.399800	5.442662
4.751155	458.331139	5.447667
4.822187	460.258492	5.452672
4.624056	460.917914	5.457677
5.265391	475.417442	5.462682
4.769203	472.243176	5.467686
4.776608	472.137816	5.472691
5.324746	478.910572	5.477696
5.138022	480.183213	5.482701
5.279790	469.537026	5.487706
4.844627	463.710679	5.492710
4.902066	453.313696	5.497715
4.799941	458.401690	5.502720
5.169575	456.303019	5.507725
5.231494	450.303786	5.512730
5.043531	465.279657	5.517734
4.913306	460.209144	5.522739
5.081563	465.358141	5.527744
4.913376	460.916520	5.532749
4.923146	464.577775	5.537754
5.080506	483.360579	5.542758
5.268212	484.610489	5.547763
5.101466	470.953668	5.552768
5.058598	475.428786	5.557773
5.354438	488.619555	5.562778
5.023759	486.521204	5.567782
5.279635	480.682840	5.572787
5.570435	484.891359	5.577792
4.760688	478.043048	5.582797
5.089324	471.904327	5.587802
5.087315	488.938067	5.592806
5.066953	496.066640	5.597811
5.341212	497.850033	5.602816
4.934801	490.008222	5.607821
5.025870	484.906780	5.612826
5.022474	491.258183	5.617830
5.363727	489.334116	5.622835
5.399613	482.509764	5.627840
5.345551	493.397114	5.632845
5.065700	485.558424	5.637850
5.161896	495.381114	5.642854
5.077526	488.909387	5.647859
5.090284	497.630926	5.652864
5.058831	504.943879	5.657869
5.300497	500.500685	5.662874
5.556825	516.670152	5.667878
5.692506	522.917628	5.672883
5.393262	508.984928	5.677888
5.457597	512.110460	5.682893
5.644355	510.641779	5.687898
5.074039	523.581128	5.692902
5.412937	522.989688	5.697907
5.754478	522.228099	5.702912
5.505899	517.504553	5.707917
5.841865	518.479688	5.712922
5.561073	510.467285	5.717926
5.324232	502.979635	5.722931
5.475315	507.622946	5.727936
5.653180	518.988742	5.732941
5.840518	521.116286	5.737946
5.517049	526.308839	5.742950
5.594165	530.523745	5.747955
5.742103	526.510083	5.752960
5.622938	531.846808	5.757965
5.599515	516.128285	5.762970
5.544149	526.753610	5.767974
5.411497	527.917644	5.772979
5.433972	523.195390	5.777984
5.220251	529.257603	5.782989
5.695720	522.450627	5.787994
5.475546	530.938625	5.792998
5.630078	531.314290	5.798003
5.577296	522.045945	5.803008
5.555838	528.598088	5.808013
5.732752	527.342781	5.813018
5.439249	534.433916	5.818022
5.847850	529.227979	5.823027
5.731399	537.484691	5.828032
5.858344	559.525183	5.833037
6.049937	549.133155	5.838042
5.756389	548.621971	5.843046
6.127977	550.277164	5.848051
5.840368	544.922861	5.853056
5.704446	539.533969	5.858061
5.893970	536.432036	5.863066
5.826842	550.816286	5.868070
5.867668	556.641584	5.873075
6.141717	567.056688	5.878080
5.735923	561.791413	5.883085
6.222439	552.311199	5.888090
5.895244	561.231349	5.893094
6.073729	568.143897	5.898099
6.007634	559.549085	5.903104
6.130756	562.134639	5.908109
6.107913	553.525170	5.913114
5.928881	569.350396	5.918118
5.962781	560.421111	5.923123
6.536867	559.206796	5.928128
6.082392	545.240960	5.933133
6.158448	534.123312	5.938138
5.982502	525.136835	5.943142
6.042364	525.451806	5.948147
6.224041	535.197414	5.953152
6.264117	538.644883	5.958157
6.233196	525.975311	5.963162
5.840208	543.814865	5.968166
6.232803	555.190716	5.973171
6.203978	550.531809	5.978176
6.287847	558.897446	5.983181
6.403120	549.083633	5.988186
6.110091	545.548125	5.993190
6.290283	553.710336	5.998195
6.345318	546.636505	6.003200
6.045462	546.733581	6.008205
5.800087	543.225309	6.013210
5.945660	548.868086	6.018214
6.321865	556.313071	6.023219
6.158761	558.549563	6.028224
5.778975	563.737049	6.033229
6.062715	567.137663	6.038234
6.230256	567.621094	6.043238
6.251127	563.092289	6.048243
6.005470	560.010710	6.053248
6.175994	564.603852	6.058253
6.221635	552.266927	6.063258
6.184852	564.780510	6.068262
6.284950	559.741684	6.073267
5.995014	561.747373	6.078272
5.506926	565.154627	6.083277
6.038988	577.433914	6.088282
5.960013	591.550596	6.093286
6.135921	600.129140	6.098291
6.120668	594.083034	6.103296
5.849939	601.505118	6.108301
5.726563	594.366677	6.113306
5.982627	606.142489	6.118310
6.179373	612.553353	6.123315
6.387024	599.884276	6.128320
6.548263	598.729638	6.133325
6.422391	596.330355	6.138330
6.428408	595.130772	6.143334
6.483517	592.739411	6.148339
6.330037	595.417543	6.153344
6.466044	601.170855	6.158349
6.725225	593.204765	6.163354
6.629076	601.062678	6.168358
6.462633	595.894711	6.173363
6.367061	588.815212	6.178368
6.222476	588.562149	6.183373
6.234706	586.577898	6.188378
6.585050	590.061423	6.193382
6.528479	574.707490	6.198387
6.423969	567.107120	6.203392
5.745417	560.266451	6.208397
6.300204	561.444137	6.213402
6.137808	564.207214	6.218406
6.222780	552.044145	6.223411
6.172219	566.895731	6.228416
6.177023	580.637595	6.233421
6.501764	584.879791	6.238426
6.245031	579.084240	6.243430
6.262513	568.503955	6.248435
6.330253	566.790541	6.253440
5.976917	562.903488	6.258445
6.428745	565.392973	6.263450
6.221767	568.586926	6.268454
6.244270	560.626694	6.273459
6.383279	559.595131	6.278464
6.200447	561.679583	6.283469
6.345204	556.094427	6.288474
6.402162	562.726349	6.293478
6.171633	554.621730	6.298483
6.417070	566.520637	6.303488
6.393453	566.435017	6.308493
6.319851	559.307491	6.313498
5.959925	565.404979	6.318502
5.941031	563.916869	6.323507
6.276116	565.909048	6.328512
6.176541	569.370176	6.333517
6.347244	571.134218	6.338522
6.102654	577.942378	6.343526
6.308030	583.101647	6.348531
6.622916	584.697559	6.353536
5.926309	574.528961	6.358541
6.306523	575.259767	6.363546
6.566620	584.761730	6.368550
6.221620	563.769395	6.373555
6.134952	566.530195	6.378560
5.930570	568.349637	6.383565
6.549030	577.245423	6.388570
6.256117	574.812234	6.393574
6.039286	572.480904	6.398579
6.253166	583.292177	6.403584
6.008825	595.476258	6.408589
6.267320	593.981877	6.413594
6.226889	596.681547	6.418598
6.326494	601.020033	6.423603
6.295917	596.138999	6.428608
6.148912	603.068162	6.433613
6.518072	594.660959	6.438618
6.254275	597.330914	6.443622
6.468257	594.885222	6.448627
6.503414	574.463781	6.453632
5.851908	575.223344	6.458637
5.985460	581.500205	6.463642
6.291847	595.012365	6.468646
6.536148	595.528869	6.473651
6.304749	595.454172	6.478656
6.037509	581.928352	6.483661
6.413201	587.913510	6.488666
6.263766	606.833899	6.493670
6.196068	592.998552	6.498675
6.447612	587.334329	6.503680
6.165953	578.076419	6.508685
6.187822	574.592562	6.513690
6.201521	586.683783	6.518694
6.488179	584.386299	6.523699
6.433143	574.057195	6.528704
5.778291	576.051085	6.533709
6.088550	578.582959	6.538714
6.405590	601.203394	6.543718
6.368537	596.227525	6.548723
6.436231	584.356988	6.553728
6.051680	577.906119	6.558733
6.291246	577.925516	6.563738
6.166442	584.775217	6.568742
6.349575	584.324618	6.573747
6.238075	590.193111	6.578752
6.397140	591.373769	6.583757
6.398113	575.444530	6.588762
6.254393	574.200083	6.593766
6.054921	575.290724	6.598771
6.162456	577.201785	6.603776
6.142344	593.219965	6.608781
6.306056	596.947327	6.613786
6.472347	607.952590	6.618790
6.332573	596.255524	6.623795
6.351670	575.558491	6.628800
6.126670	567.705545	6.633805
6.416234	569.315713	6.638810
6.102220	573.923575	6.643814
6.390956	571.993789	6.648819
6.434428	568.696591	6.653824
6.268033	569.848850	6.658829
6.306590	561.853003	6.663834
6.268754	572.765152	6.668838
6.262471	574.223220	6.673843
6.305752	572.174232	6.678848
6.044794	572.780519	6.683853
6.171468	566.788279	6.688858
6.217209	573.156641	6.693862
6.478746	576.961338	6.698867
6.289006	565.863209	6.703872
6.053459	568.877380	6.708877
6.140138	564.994822	6.713882
6.512127	572.435776	6.718886
6.175550	568.723947	6.723891
6.573467	572.356673	6.728896
6.323061	578.388275	6.733901
6.218841	570.989142	6.738906
6.302108	572.277469	6.743910
6.266610	564.945304	6.748915
6.331603	562.919166	6.753920
6.105993	571.970703	6.758925
6.310104	567.222108	6.763930
5.943202	563.434787	6.768934
5.819608	572.926473	6.773939
5.663579	578.187421	6.778944
5.789451	609.205187	6.783949
6.454037	604.783104	6.788954
6.530982	607.659298	6.793958
6.460137	613.292942	6.798963
6.588363	604.308938	6.803968
6.221426	613.676756	6.808973
6.378766	598.294877	6.813978
6.751135	598.129871	6.818982
6.167800	584.767888	6.823987
6.476499	570.487393	6.828992
6.098131	577.041231	6.833997
5.949038	578.505581	6.839002
6.325845	571.933180	6.844006
6.331574	572.129831	6.849011
6.499996	576.071706	6.854016
6.412818	588.874667	6.859021
6.616208	575.950759	6.864026
6.217450	579.518857	6.869030
6.521747	575.425417	6.874035
6.507500	569.773243	6.879040
6.339798	568.749250	6.884045
6.517037	574.034145	6.889050
6.159118	573.253988	6.894054
6.096488	580.824735	6.899059
6.546126	569.692956	6.904064
6.361335	574.426242	6.909069
6.204138	574.425890	6.914074
6.297167	569.551432	6.919078
6.191038	572.396760	6.924083
6.238632	571.162864	6.929088
6.309885	582.344482	6.934093
6.435193	574.265786	6.939098
6.255516	568.694682	6.944102
6.557023	567.870059	6.949107
6.672656	564.224054	6.954112
6.175425	563.583397	6.959117
6.249628	543.766891	6.964122
5.742204	539.717294	6.969126
5.737706	559.243929	6.974131
6.240825	565.196926	6.979136
5.774786	570.352716	6.984141
5.890704	565.954007	6.989146
6.092212	578.892682	6.994150
6.032600	568.465669	6.999155
6.567427	568.885124	7.004160
6.161251	574.106583	7.009165
5.927493	567.698634	7.014170
5.715669	568.328359	7.019174
6.168118	588.732914	7.024179
6.567067	591.439946	7.029184
5.971617	584.609976	7.034189
6.641673	594.592470	7.039194
6.270570	584.064482	7.044198
5.933184	578.702227	7.049203
6.316583	596.022545	7.054208
6.281600	606.445629	7.059213
6.332645	598.386520	7.064218
6.425542	594.671058	7.069222
6.080064	591.023058	7.074227
6.622121	575.375221	7.079232
6.359548	583.542288	7.084237
6.308733	577.045432	7.089242
6.131611	567.923157	7.094246
6.100256	574.128849	7.099251
6.357980	572.524087	7.104256
6.248789	578.089867	7.109261
6.206980	570.412609	7.114266
6.375316	574.803448	7.119270
6.021152	573.769284	7.124275
6.263812	567.821184	7.129280
6.072712	572.207011	7.134285
6.402555	575.749577	7.139290
6.512807	572.266478	7.144294
6.123298	571.729742	7.149299
6.474251	558.307599	7.154304
5.917515	572.722029	7.159309
6.332580	563.474661	7.164314
6.181544	557.335807	7.169318
5.785407	560.131274	7.174323
6.459907	586.710346	7.179328
6.230957	603.059721	7.184333
6.407065	599.830541	7.189338
6.319931	598.184803	7.194342
5.924394	582.811607	7.199347
6.252370	597.491608	7.204352
6.406115	598.422722	7.209357
6.417184	596.600679	7.214362
6.394297	589.656360	7.219366
6.305422	582.338551	7.224371
6.099865	569.637673	7.229376
6.103282	578.769497	7.234381
5.993895	599.654875	7.239386
6.410105	604.653928	7.244390
6.245636	596.813638	7.249395
6.270277	603.832192	7.254400
6.169370	609.950943	7.259405
6.589111	606.723847	7.264410
6.704710	596.417781	7.269414
6.245034	580.104815	7.274419
6.257351	575.112686	7.279424
5.736532	574.100001	7.284429
6.355962	584.400696	7.289434
6.334221	592.978417	7.294438
6.021950	578.008221	7.299443
6.414072	585.627204	7.304448
6.401361	581.162762	7.309453
6.314064	567.937900	7.314458
6.243774	568.896638	7.319462
6.026500	569.473589	7.324467
6.410014	563.287066	7.329472
6.205827	579.191061	7.334477
6.022174	574.850638	7.339482
6.467336	580.088605	7.344486
6.243384	585.671418	7.349491
6.410269	582.352992	7.354496
5.973692	580.261704	7.359501
6.011998	592.143818	7.364506
6.333154	597.342333	7.369510
6.280794	609.165470	7.374515
6.336543	604.206990	7.379520
6.535490	610.479546	7.384525
6.396891	588.051485	7.389530
6.387481	584.020251	7.394534
6.301580	583.701426	7.399539
6.446577	579.030501	7.404544
6.559587	579.038688	7.409549
6.264943	582.104088	7.414554
6.347233	580.398131	7.419558
6.278981	578.267954	7.424563
6.301192	570.430314	7.429568
6.187044	574.557512	7.434573
5.987682	568.770621	7.439578
6.235001	572.063007	7.444582
6.293373	577.831732	7.449587
6.201156	569.824776	7.454592
5.838535	578.087936	7.459597
5.816964	582.255062	7.464602
6.211102	592.250287	7.469606
6.508060	605.987408	7.474611
6.483732	581.092223	7.479616
6.284944	581.145528	7.484621
6.388217	580.566660	7.489626
6.086539	577.990468	7.494630
6.042205	573.819185	7.499635
6.049794	574.392449	7.504640
6.268419	598.150465	7.509645
6.444331	602.248781	7.514650
6.475335	589.079894	7.519654
6.213463	577.008774	7.524659
6.015124	572.865953	7.529664
6.173095	583.373897	7.534669
6.402776	600.607584	7.539674
6.598168	582.224180	7.544678
6.147893	582.669408	7.549683
6.055248	569.878198	7.554688
6.133521	578.411723	7.559693
6.447773	581.926087	7.564698
6.359123	577.143281	7.569702
6.039622	575.045829	7.574707
6.103641	577.691494	7.579712
6.454188	586.618034	7.584717
6.653681	592.701835	7.589722
6.026374	578.847471	7.594726
5.860180	577.138456	7.599731
6.230594	581.212059	7.604736
6.334510	597.235359	7.609741
6.519342	589.417353	7.614746
6.382849	571.151673	7.619750
6.048683	577.529071	7.624755
6.371743	570.255737	7.629760
5.965582	570.339829	7.634765
6.397923	577.105952	7.639770
6.296600	579.059887	7.644774
6.041063	573.690395	7.649779
6.436020	585.962002	7.654784
6.396859	585.777720	7.659789
5.972080	575.399922	7.664794
6.126210	576.065943	7.669798
6.131501	597.699984	7.674803
6.343038	609.186371	7.679808
6.396226	605.550696	7.684813
6.396934	600.570151	7.689818
6.386245	593.361150	7.694822
6.079391	584.245942	7.699827
6.377050	575.188116	7.704832
6.155270	580.993562	7.709837
6.518330	583.746398	7.714842
6.077617	576.416008	7.719846
6.018004	581.651125	7.724851
6.199663	581.197613	7.729856
6.296099	597.368382	7.734861
6.482363	606.557564	7.739866
6.259880	593.294285	7.744870
5.982991	593.429987	7.749875
6.241547	598.873309	7.754880
6.351179	609.113195	7.759885
6.370322	600.491420	7.764890
6.358756	593.972467	7.769894
5.949852	593.098529	7.774899
6.297220	598.212583	7.779904
5.925918	606.845828	7.784909
6.184692	611.958770	7.789914
6.532440	611.703513	7.794918
6.580599	614.729324	7.799923
6.571416	598.526846	7.804928
6.489761	586.342205	7.809933
6.057364	587.505951	7.814938
6.170206	576.901975	7.819942
6.119904	578.896600	7.824947
6.498426	576.438465	7.829952
6.047516	573.051840	7.834957
6.190275	570.174719	7.839962
6.200715	569.943742	7.844966
6.091387	588.502057	7.849971
6.587461	595.542397	7.854976
6.372322	589.369348	7.859981
6.474056	588.565175	7.864986
6.286000	576.193320	7.869990
6.166490	575.980113	7.874995
6.400446	570.116731	7.880000
6.378548	578.933253	7.885005
5.975087	576.845165	7.890010
6.289220	568.393608	7.895014
6.000353	575.491690	7.900019
6.657991	568.813388	7.905024
6.070152	582.410660	7.910029
5.850716	572.202123	7.915034
6.127652	573.448315	7.920038
6.162363	601.642616	7.925043
6.458114	606.342319	7.930048
6.124612	600.528095	7.935053
6.157261	609.473937	7.940058
6.702934	605.286843	7.945062
6.271681	588.417396	7.950067
6.201497	581.224369	7.955072
6.403632	580.429027	7.960077
6.499169	582.941203	7.965082
6.045715	577.336100	7.970086
6.161603	580.655186	7.975091
6.022913	572.748083	7.980096
6.389718	580.372439	7.985101
6.052414	580.320015	7.990106
6.247494	585.099136	7.995110
6.227081	589.108594	8.000115
6.381959	585.028580	8.005133
6.184962	586.964286	8.010150
6.155804	594.095081	8.015168
6.251580	598.102639	8.020186
6.169172	606.855144	8.025203
6.803693	603.352327	8.030221
6.412976	590.215006	8.035238
6.185815	580.155327	8.040256
6.180639	578.045955	8.045274
6.025311	588.894636	8.050291
6.218514	588.103701	8.055309
6.113591	600.046332	8.060326
6.325091	603.411345	8.065344
6.417283	609.343390	8.070362
6.040477	608.603537	8.075379
6.298344	609.618704	8.080397
6.358886	618.236921	8.085414
6.559897	612.630044	8.090432
6.639463	606.452175	8.095450
6.298512	605.260745	8.100467
6.597247	608.111347	8.105485
6.493071	601.707623	8.110502
5.997649	587.185177	8.115520
6.304030	591.521418	8.120538
6.199945	604.744341	8.125555
6.619239	605.366266	8.130573
6.370123	608.485921	8.135590
6.496751	613.248562	8.140608
6.546355	613.575034	8.145626
6.158314	619.336620	8.150643
6.411112	614.962425	8.155661
6.160833	614.106351	8.160678
6.489083	612.404921	8.165696
6.386443	611.962560	8.170714
6.151180	610.352081	8.175731
6.675432	609.109108	8.180749
6.321705	621.856291	8.185766
6.265693	603.684723	8.190784
6.799155	609.527755	8.195802
6.523327	617.734379	8.200819
6.683003	612.911461	8.205837
6.798048	603.983802	8.210854
6.726189	599.301583	8.215872
6.378230	584.182515	8.220890
6.192219	585.094422	8.225907
6.696783	599.655041	8.230925
6.563981	596.137563	8.235942
6.313659	586.102580	8.240960
6.419090	578.350662	8.245978
6.627250	607.817253	8.250995
6.630570	607.818340	8.256013
6.714174	592.653390	8.261030
6.632581	578.491531	8.266048
6.585170	571.196786	8.271066
6.240293	580.099621	8.276083
6.254457	580.246343	8.281101
6.129349	600.776586	8.286118
6.186436	609.530007	8.291136
6.692673	607.528847	8.296154
6.431458	615.591524	8.301171
6.391083	609.751014	8.306189
6.543309	612.707958	8.311206
6.481851	611.395055	8.316224
6.604283	611.038645	8.321242
6.535571	613.703062	8.326259
6.463767	608.619676	8.331277
6.815507	610.540105	8.336294
6.576401	607.100657	8.341312
6.429934	610.261185	8.346330
6.034380	610.829864	8.351347
6.364104	614.227465	8.356365
6.467608	620.554466	8.361382
6.287709	614.118987	8.366400
6.850468	622.116284	8.371418
6.715658	648.736980	8.376435
6.754426	632.009238	8.381453
6.545397	615.196178	8.386470
6.425428	635.590388	8.391488
6.759547	637.430673	8.396506
6.610733	636.495595	8.401523
6.519159	635.226651	8.406541
6.547962	637.740287	8.411558
6.428640	637.708930	8.416576
6.573786	644.379416	8.421594
6.547064	639.848363	8.426611
6.667590	632.817101	8.431629
6.684006	627.003005	8.436646
6.560767	636.730729	8.441664
6.689868	635.196124	8.446682
6.450591	649.229807	8.451699
6.740922	644.094711	8.456717
6.932091	640.649160	8.461734
6.812080	636.559906	8.466752
6.997590	632.123624	8.471770
6.944229	637.351875	8.476787
6.863098	629.184396	8.481805
6.773336	629.631972	8.486822
6.760095	640.379606	8.491840
6.759263	632.007109	8.496858
6.525342	641.432712	8.501875
6.723438	638.011210	8.506893
6.547529	625.529781	8.511910
6.776851	636.959248	8.516928
7.159927	646.234658	8.521946
6.867813	636.398676	8.526963
6.809917	624.268549	8.531981
7.047627	635.742292	8.536998
6.820087	642.831555	8.542016
6.985533	633.409147	8.547034
7.030164	642.546515	8.552051
6.979574	643.256091	8.557069
7.154255	629.086787	8.562087
6.401148	640.934433	8.567104
7.032243	637.204631	8.572122
6.971274	623.993979	8.577139
6.945515	638.723745	8.582157
7.164792	642.104210	8.587175
6.582702	630.739183	8.592192
6.920286	625.735630	8.597210
6.753436	632.362899	8.602227
6.672043	631.287532	8.607245
6.752391	632.850567	8.612263
6.776339	639.213975	8.617280
6.992075	637.437873	8.622298
6.775816	637.635546	8.627315
6.911203	634.228365	8.632333
6.910512	640.306502	8.637351
6.813690	638.381775	8.642368
6.737160	635.356907	8.647386
6.748324	642.600331	8.652403
6.861976	635.145430	8.657421
6.927894	643.269889	8.662439
6.535096	645.081735	8.667456
6.950637	639.276735	8.672474
7.090423	639.405216	8.677491
6.679261	640.348503	8.682509
6.906161	640.465314	8.687527
6.934900	643.395471	8.692544
7.234067	642.406684	8.697562
6.776695	646.738120	8.702579
6.698902	644.672060	8.707597
7.547522	658.842517	8.712615
7.295952	657.071356	8.717632
7.273825	637.927465	8.722650
6.902179	641.479398	8.727667
7.158226	640.791433	8.732685
7.111888	635.696342	8.737703
6.939383	646.747108	8.742720
7.036826	637.391860	8.747738
6.988215	639.885247	8.752755
6.906004	642.599933	8.757773
6.921543	627.912134	8.762791
6.747162	630.967650	8.767808
7.230273	652.213140	8.772826
7.192934	649.741193	8.777843
7.042577	646.680913	8.782861
7.082483	645.124465	8.787879
6.798815	648.631912	8.792896
7.121303	657.894921	8.797914
7.293898	667.926806	8.802931
6.979626	672.217231	8.807949
7.264137	663.149869	8.812967
7.191698	669.547754	8.817984
7.352562	669.939263	8.823002
7.434580	655.582929	8.828019
6.747666	649.384139	8.833037
7.031282	648.046767	8.838055
7.493875	664.677457	8.843072
7.377829	636.407953	8.848090
7.201947	638.868482	8.853107
6.953352	639.923030	8.858125
7.453365	627.271804	8.863143
7.116620	637.875774	8.868160
7.222018	634.958174	8.873178
6.970077	641.718821	8.878195
7.075161	647.883376	8.883213
7.337457	650.797694	8.888231
7.437843	659.936469	8.893248
6.988007	639.458369	8.898266
7.292773	644.331670	8.903283
7.068811	669.908569	8.908301
7.416932	662.969126	8.913319
7.409730	668.072823	8.918336
7.390791	660.038328	8.923354
7.433214	646.379067	8.928371
7.343469	636.599332	8.933389
7.338729	636.379327	8.938407
7.140673	639.282082	8.943424
7.351918	638.254314	8.948442
7.226023	637.021365	8.953459
7.123352	628.338196	8.958477
7.139186	639.025507	8.963495
7.017010	667.226325	8.968512
7.779415	664.108199	8.973530
7.465698	658.948721	8.978547
7.202471	651.567636	8.983565
7.476539	643.020880	8.988583
7.139917	650.889579	8.993600
7.034933	659.099428	8.998618
7.196459	673.787980	9.003635
7.269472	670.207666	9.008653
7.451407	670.232322	9.013671
7.469365	684.396659	9.018688
7.477464	681.619564	9.023706
7.403572	674.916915	9.028723
7.229285	677.191370	9.033741
7.450698	674.147078	9.038759
7.185204	666.056956	9.043776
7.367715	675.092382	9.048794
7.334124	672.043075	9.053811
7.339112	679.080071	9.058829
7.422863	664.329765	9.063847
7.434736	676.555459	9.068864
7.463944	667.298888	9.073882
7.714731	667.885730	9.078899
7.419836	682.664041	9.083917
7.586825	672.500453	9.088935
7.590048	675.836786	9.093952
7.354942	672.392134	9.098970
7.395181	675.431410	9.103987
7.996108	674.378479	9.109005
7.992340	671.091571	9.114023
7.384502	672.593774	9.119040
7.258786	663.759291	9.124058
7.893037	668.641029	9.129075
7.447402	664.431289	9.134093
7.240595	660.190270	9.139111
7.352905	673.576816	9.144128
7.682899	673.699782	9.149146
8.078333	665.847834	9.154163
7.379715	668.452404	9.159181
7.490099	658.935167	9.164199
7.604795	665.520553	9.169216
7.600104	668.733005	9.174234
7.752498	666.335931	9.179251
7.409085	662.177371	9.184269
7.236906	659.027007	9.189287
7.678687	668.935976	9.194304
7.861000	676.360118	9.199322
7.910311	662.784736	9.204339
7.606036	653.520013	9.209357
7.513040	641.014606	9.214375
7.493348	655.479621	9.219392
7.497441	662.916733	9.224410
7.730246	668.434202	9.229427
7.677346	685.394749	9.234445
7.927217	679.081373	9.239463
7.767374	661.383793	9.244480
7.337530	652.057191	9.249498
7.461395	663.558075	9.254515
7.815134	667.870946	9.259533
8.098871	659.339902	9.264551
7.624796	665.066148	9.269568
7.486242	665.481255	9.274586
7.894173	664.834276	9.279603
7.416468	672.872008	9.284621
7.727738	668.529845	9.289639
8.020150	670.126268	9.294656
7.768297	676.434580	9.299674
7.800241	663.988383	9.304691
7.591617	668.237692	9.309709
7.728113	677.178384	9.314727
7.660616	670.031005	9.319744
7.672043	673.050249	9.324762
7.909314	663.513180	9.329779
7.640579	664.476976	9.334797
7.670796	666.123508	9.339815
7.873960	673.196973	9.344832
7.594558	675.340023	9.349850
7.914973	667.024542	9.354867
7.760402	676.722836	9.359885
8.033143	679.433867	9.364903
8.051035	675.846144	9.369920
7.442640	676.278033	9.374938
7.614997	659.575382	9.379955
7.435559	682.404942	9.384973
8.033252	672.544815	9.389991
7.936883	669.932649	9.395008
7.849586	673.657963	9.400026
8.188710	666.324757	9.405043
7.732362	671.968941	9.410061
7.783269	660.758113	9.415079
7.971006	674.628203	9.420096
7.591062	677.681155	9.425114
8.109731	673.426687	9.430131
7.985938	669.965571	9.435149
8.040107	663.056694	9.440167
8.036393	667.021694	9.445184
7.899147	672.785863	9.450202
7.916521	663.288356	9.455219
7.586115	670.343486	9.460237
7.869789	668.921069	9.465255
8.029339	673.854644	9.470272
7.827982	670.600061	9.475290
8.071651	666.989127	9.480307
8.068396	666.113010	9.485325
7.940105	660.540566	9.490343
8.000896	669.421747	9.495360
7.481739	685.752064	9.500378
7.688740	680.316994	9.505395
7.772336	675.046446	9.510413
7.668853	670.779260	9.515431
7.669460	679.672380	9.520448
7.765441	696.441366	9.525466
8.146710	686.780051	9.530483
8.274237	700.384165	9.535501
8.128332	691.852599	9.540519
8.149780	698.497138	9.545536
8.197953	701.310315	9.550554
8.527359	700.096057	9.555571
8.141230	683.826784	9.560589
7.735341	673.589171	9.565607
8.075728	679.325430	9.570624
8.085814	685.970270	9.575642
8.151784	694.654950	9.580659
7.932889	699.481918	9.585677
7.781348	696.621025	9.590695
8.252719	703.461126	9.595712
8.155397	697.828426	9.600730
8.184089	692.861041	9.605747
7.786682	702.288164	9.610765
8.335560	706.140018	9.615783
8.174774	701.346123	9.620800
7.863151	707.995428	9.625818
8.087662	708.228377	9.630835
8.028386	698.506940	9.635853
8.105564	708.062160	9.640871
7.911167	702.549464	9.645888
7.996273	700.730816	9.650906
8.348727	699.980037	9.655923
8.109846	702.889564	9.660941
8.059115	697.118054	9.665959
8.222048	692.782732	9.670976
8.387713	707.259619	9.675994
8.307870	697.140825	9.681011
8.426740	695.806715	9.686029
7.951886	696.655835	9.691047
8.051345	693.171918	9.696064
8.042753	705.165210	9.701082
8.532321	693.678976	9.706099
8.287752	707.120710	9.711117
8.347330	707.956132	9.716135
8.486791	701.884246	9.721152
8.106739	707.013477	9.726170
8.544453	702.684616	9.731187
8.238058	700.774900	9.736205
8.170938	709.633192	9.741223
8.426890	695.383051	9.746240
8.587737	705.684212	9.751258
8.512763	696.794461	9.756275
8.492232	704.242757	9.761293
7.888319	699.476574	9.766311
8.197429	701.596188	9.771328
8.257931	710.594755	9.776346
8.312619	699.074236	9.781363
8.340943	712.515272	9.786381
8.566982	729.562347	9.791399
8.588944	703.230386	9.796416
8.206913	713.587591	9.801434
8.123697	709.854802	9.806451
8.109111	732.204014	9.811469
8.156410	733.153276	9.816487
8.645095	734.801452	9.821504
8.279925	743.522514	9.826522
8.575099	739.979014	9.831539
8.514609	744.211688	9.836557
8.625425	730.853215	9.841575
8.491922	737.004167	9.846592
8.363689	745.689539	9.851610
8.768757	739.180765	9.856627
8.692078	736.382267	9.861645
8.669630	742.908510	9.866663
8.652739	736.232615	9.871680
8.483558	735.551677	9.876698
8.669494	731.429058	9.881715
8.768921	720.982549	9.886733
8.888867	718.019613	9.891751
8.512279	708.334179	9.896768
7.968057	708.125558	9.901786
8.592668	716.778764	9.906803
8.861098	729.530094	9.911821
8.502851	718.833406	9.916839
8.693635	697.483052	9.921856
8.326797	696.934840	9.926874
8.607907	715.657325	9.931891
8.870843	726.531719	9.936909
8.468252	726.276811	9.941927
8.822939	710.668651	9.946944
8.659021	708.069239	9.951962
8.821399	695.647478	9.956979
8.608229	697.538634	9.961997
8.368484	701.438796	9.967015
8.857823	708.153490	9.972032
8.542130	712.043004	9.977050
8.664118	720.650709	9.982067
8.441750	724.682638	9.987085
8.277031	736.685272	9.992103
8.752525	728.993254	9.997120
8.333816	730.207072	10.002138
8.432524	732.007221	10.007155
8.926597	737.607822	10.012173
8.641025	733.793581	10.017191
8.934669	733.844620	10.022208
8.792560	735.181130	10.027226
8.643903	727.949925	10.032243
8.725937	732.060576	10.037261
9.110135	740.916589	10.042279
8.964264	733.606184	10.047296
8.654178	735.694485	10.052314
8.674540	735.377020	10.057331
8.928670	736.639651	10.062349
8.786992	752.306384	10.067367
8.919964	738.852902	10.072384
9.026732	738.641988	10.077402
8.836560	725.452251	10.082419
8.731127	727.964510	10.087437
8.636718	734.176700	10.092455
8.883911	733.516967	10.097472
8.723597	737.252025	10.102490
8.634606	737.486102	10.107507
8.891384	733.461588	10.112525
8.799968	738.008419	10.117543
8.977926	732.903319	10.122560
8.769392	728.407857	10.127578
8.948006	734.742938	10.132595
8.990126	738.757450	10.137613
8.679387	739.603410	10.142631
8.543256	735.706946	10.147648
8.508361	737.821721	10.152666
8.549726	735.966614	10.157683
8.964869	752.768633	10.162701
9.055690	764.287661	10.167719
9.165636	762.767631	10.172736
9.280471	764.681248	10.177754
8.827965	749.198446	10.182771
8.944670	738.395147	10.187789
8.797216	744.959806	10.192807
9.170757	751.154748	10.197824
9.253469	752.644573	10.202842
8.788300	740.408970	10.207859
9.202320	742.973397	10.212877
8.951592	740.241906	10.217895
9.172165	736.240708	10.222912
8.751193	740.564174	10.227930
8.826532	751.312177	10.232947
9.233227	757.004416	10.237965
9.343864	760.496986	10.242983
9.062022	751.030863	10.248000
9.199520	753.672181	10.253018
9.201326	747.041607	10.258035
9.179172	735.269234	10.263053
8.816796	735.291115	10.268071
8.998940	745.522638	10.273088
9.378811	766.355483	10.278106
8.858878	763.453222	10.283123
9.464226	758.578901	10.288141
9.304739	778.594431	10.293159
9.129199	750.884541	10.298176
8.912361	749.086753	10.303194
9.044593	760.026512	10.308211
9.379259	759.452288	10.313229
9.723100	760.597316	10.318247
9.269289	742.627472	10.323264
9.098396	744.538009	10.328282
8.960448	739.569071	10.333299
8.889569	746.153332	10.338317
9.157525	752.929113	10.343335
9.352412	759.792976	10.348352
9.239322	771.674103	10.353370
8.980956	767.445135	10.358387
9.388564	766.335239	10.363405
9.326867	766.976585	10.368423
9.255422	771.231158	10.373440
9.242804	770.514845	10.378458
8.984104	763.920709	10.383475
9.313900	764.986177	10.388493
9.034685	763.336505	10.393511
9.217884	767.506000	10.398528
8.940026	771.131797	10.403546
8.747781	762.040180	10.408563
9.091809	758.755894	10.413581
9.034185	774.585493	10.418599
9.295699	793.990021	10.423616
9.371323	793.467746	10.428634
8.959064	798.615725	10.433651
9.670353	803.461128	10.438669
9.515892	795.777333	10.443687
9.828131	795.391458	10.448704
9.532866	790.641456	10.453722
9.309974	792.596040	10.458739
9.812606	777.581787	10.463757
9.436001	778.118988	10.468775
9.483386	762.999433	10.473792
9.313621	758.738474	10.478810
9.440552	770.696778	10.483827
9.647101	763.399258	10.488845
9.419519	767.039956	10.493863
9.439550	763.717199	10.498880
9.515657	758.955710	10.503898
9.078565	766.343099	10.508915
9.732502	775.519801	10.513933
9.536355	787.639484	10.518951
9.623968	793.817227	10.523968
9.727406	792.277407	10.528986
9.638848	785.160626	10.534003
9.857907	773.572285	10.539021
9.782967	765.268677	10.544039
9.491524	771.942620	10.549056
9.724236	762.621981	10.554074
9.517366	767.078495	10.559091
9.447418	761.732168	10.564109
9.390276	762.804232	10.569127
9.433009	761.108728	10.574144
9.564438	764.019936	10.579162
9.469403	778.511714	10.584179
9.732797	778.492569	10.589197
9.565792	792.045934	10.594215
9.524034	800.094610	10.599232
9.515808	784.116179	10.604250
9.418403	799.648076	10.609267
9.430027	794.718129	10.614285
9.564463	800.405863	10.619303
9.555261	794.832942	10.624320
9.644109	796.271364	10.629338
9.548290	787.084635	10.634355
9.797021	783.140570	10.639373
9.706313	793.626350	10.644391
9.701187	798.772657	10.649408
9.933038	789.482852	10.654426
9.505705	804.397375	10.659443
9.309157	792.895556	10.664461
8.878117	796.214852	10.669479
9.366849	810.228124	10.674496
9.638175	816.679770	10.679514
9.701152	827.669231	10.684531
9.889986	820.432882	10.689549
9.840064	829.055730	10.694567
10.020040	827.590236	10.699584
10.545386	825.027056	10.704602
10.028538	830.834457	10.709619
9.868415	820.889891	10.714637
9.877050	817.938282	10.719655
9.816394	824.334279	10.724672
10.419016	818.175811	10.729690
9.524057	806.788843	10.734707
9.782505	800.237003	10.739725
10.062390	816.356408	10.744743
10.018325	816.423212	10.749760
10.230813	802.360082	10.754778
9.698113	798.713512	10.759795
9.701132	794.069620	10.764813
10.064126	808.914299	10.769831
9.964004	808.160508	10.774848
10.111132	805.776488	10.779866
9.802269	790.386781	10.784883
9.873773	799.614275	10.789901
10.102549	808.690935	10.794919
9.904279	811.912638	10.799936
10.268968	815.583220	10.804954
9.993895	807.972538	10.809971
9.976496	804.616602	10.814989
9.688992	809.786444	10.820007
9.932885	830.068299	10.825024
10.135007	815.770665	10.830042
9.997984	826.614119	10.835059
10.278490	830.954516	10.840077
10.318874	828.355897	10.845095
10.247371	823.132635	10.850112
10.311762	796.591531	10.855130
9.971883	794.402717	10.860147
10.139406	788.852894	10.865165
10.048927	788.472290	10.870183
9.884567	797.379410	10.875200
10.203310	802.124075	10.880218
10.228463	811.762773	10.885235
10.334184	808.039617	10.890253
10.281966	805.476414	10.895271
10.201436	795.121855	10.900288
10.003958	787.897919	10.905306
10.119395	802.608003	10.910323
10.159250	811.968298	10.915341
10.333176	818.394736	10.920359
10.154059	818.099671	10.925376
10.038573	817.989730	10.930394
10.129854	826.261651	10.935411
9.977880	820.866685	10.940429
10.012310	825.694655	10.945447
9.840212	819.865642	10.950464
10.119493	830.524815	10.955482
9.932848	830.478622	10.960499
10.191304	820.407661	10.965517
10.049642	821.384281	10.970535
10.183654	820.702344	10.975552
10.419127	810.067901	10.980570
9.907991	824.118020	10.985587
10.381104	839.803898	10.990605
10.726082	842.418355	10.995623
10.216924	837.211262	11.000640
10.164484	826.695740	11.005658
10.411527	843.481208	11.010675
10.435893	850.806791	11.015693
10.757538	853.388107	11.020711
10.218916	840.859091	11.025728
10.386729	834.232092	11.030746
10.648514	846.853916	11.035763
10.585033	833.620668	11.040781
10.694889	826.500539	11.045799
10.408883	827.803014	11.050816
10.266204	828.408169	11.055834
10.525677	825.085905	11.060851
10.438401	823.038714	11.065869
10.486075	828.203452	11.070887
10.490579	822.903827	11.075904
10.556307	823.986650	11.080922
10.269975	820.364235	11.085939
10.651506	829.441596	11.090957
10.845791	823.830245	11.095975
10.203508	826.818798	11.100992
10.482477	817.548337	11.106010
10.520977	826.730528	11.111027
10.870215	833.091724	11.116045
10.582852	828.161277	11.121063
10.075649	830.832202	11.126080
10.753156	837.456743	11.131098
10.896375	848.646700	11.136115
10.675926	836.696466	11.141133
10.636778	820.387309	11.146151
10.529320	822.458996	11.151168
10.467856	814.776326	11.156186
10.583986	827.798612	11.161203
10.507320	844.107395	11.166221
10.776350	850.533059	11.171239
10.551852	859.701734	11.176256
10.710760	850.945599	11.181274
10.962604	851.851943	11.186291
10.918339	849.671648	11.191309
11.106225	832.079277	11.196327
10.754259	829.392091	11.201344
10.810582	822.089499	11.206362
10.920465	814.929216	11.211379
10.659469	813.406829	11.216397
10.688922	810.792701	11.221415
10.475847	818.910303	11.226432
10.956077	810.427345	11.231450
10.803843	812.117882	11.236467
10.640260	825.585676	11.241485
11.009519	822.971180	11.246503
10.601933	822.308457	11.251520
10.693457	833.400276	11.256538
10.888868	830.229164	11.261555
10.869880	844.901708	11.266573
11.142022	836.731131	11.271591
10.781401	838.869543	11.276608
10.635585	839.444904	11.281626
10.938353	844.167426	11.286643
10.740012	845.901033	11.291661
10.801577	849.784408	11.296679
10.566205	855.343250	11.301696
10.943272	856.519789	11.306714
10.808857	854.166636	11.311731
10.685765	853.147368	11.316749
10.884613	852.738538	11.321767
10.864389	855.574879	11.326784
11.187625	842.675599	11.331802
10.902175	848.236433	11.336819
10.487670	851.999043	11.341837
10.822077	841.300168	11.346855
10.770194	849.707221	11.351872
10.804578	854.924165	11.356890
11.403870	860.510144	11.361907
11.004911	858.571250	11.366925
11.274661	846.054427	11.371943
10.933953	849.263900	11.376960
10.884821	854.776155	11.381978
11.221098	853.678459	11.386995
10.896633	859.692979	11.392013
11.324510	866.136044	11.397031
11.015265	864.392520	11.402048
11.103613	867.864397	11.407066
11.506052	867.262412	11.412083
10.951426	867.183456	11.417101
10.973117	850.189423	11.422119
11.316813	863.992127	11.427136
11.232258	856.546320	11.432154
11.047115	858.686384	11.437171
10.982002	861.314029	11.442189
11.684609	871.357883	11.447207
11.537595	872.791276	11.452224
11.032462	857.656826	11.457242
11.144166	852.199684	11.462259
10.955707	852.351025	11.467277
11.221922	857.623278	11.472295
11.459882	877.655010	11.477312
11.167886	870.815959	11.482330
11.294031	864.839123	11.487347
11.400197	871.599622	11.492365
11.503398	872.971111	11.497383
11.197436	868.483474	11.502400
11.345355	855.977369	11.507418
11.294738	853.538296	11.512435
11.442933	863.247592	11.517453
11.269489	857.224703	11.522471
11.050605	858.204271	11.527488
11.786055	858.654176	11.532506
11.731511	859.934074	11.537523
11.800650	851.704195	11.542541
11.404452	841.753039	11.547559
11.044133	847.577439	11.552576
11.222437	837.489425	11.557594
11.377470	839.070821	11.562611
11.291195	846.345435	11.567629
11.540603	859.551180	11.572647
11.838479	864.673711	11.577664
11.649676	855.461396	11.582682
11.443350	851.441100	11.587699
11.401077	849.749033	11.592717
11.555516	843.302189	11.597735
11.301943	848.382571	11.602752
11.283104	850.716345	11.607770
11.905129	857.567788	11.612787
11.894727	861.781964	11.617805
11.751018	844.817293	11.622823
11.419408	843.165265	11.627840
11.417255	845.719886	11.632858
11.417584	840.689044	11.637875
11.336155	851.143013	11.642893
11.362441	856.195559	11.647911
11.664099	866.428631	11.652928
11.658341	860.098853	11.657946
11.810694	867.334357	11.662963
11.478623	870.845538	11.667981
12.033961	870.665457	11.672999
11.495269	873.858508	11.678016
11.744991	872.879863	11.683034
11.806767	864.010282	11.688051
11.804240	866.176406	11.693069
11.812739	865.661699	11.698087
11.817959	876.811933	11.703104
11.878514	870.748322	11.708122
11.768046	853.469885	11.713139
11.671637	851.234054	11.718157
11.677197	859.317442	11.723175
11.800813	865.143600	11.728192
11.459798	861.163713	11.733210
11.843496	862.498596	11.738227
11.758710	864.329144	11.743245
11.773578	861.179260	11.748263
11.615583	871.917956	11.753280
11.871736	858.645144	11.758298
11.989170	862.679499	11.763315
12.132323	867.277285	11.768333
12.390441	868.563281	11.773351
12.031364	862.301063	11.778368
11.583381	853.343073	11.783386
11.827817	853.360136	11.788403
11.612345	866.383824	11.793421
11.694874	862.733389	11.798439
11.680101	860.818669	11.803456
11.652551	863.916055	11.808474
11.858592	865.999612	11.813491
11.635165	867.804302	11.818509
12.006666	863.072209	11.823527
12.006814	865.009160	11.828544
11.470123	864.851254	11.833562
11.828850	858.751265	11.838579
11.784678	878.108491	11.843597
11.978607	885.152875	11.848615
12.401772	890.451510	11.853632
12.164299	898.234233	11.858650
12.353555	887.173946	11.863667
12.024658	872.166197	11.868685
11.958749	863.566174	11.873703
12.048146	880.751784	11.878720
11.844476	889.602476	11.883738
12.208844	893.445956	11.888755
12.172361	898.283724	11.893773
12.049136	900.652113	11.898791
12.143356	894.908494	11.903808
12.444998	895.284572	11.908826
12.218122	889.242172	11.913843
12.129364	897.410093	11.918861
12.346240	893.597647	11.923879
12.418034	899.518222	11.928896
12.328401	885.419221	11.933914
12.108063	875.847960	11.938931
12.010983	869.845883	11.943949
12.311552	886.511516	11.948967
12.566102	885.232478	11.953984
12.128009	883.923259	11.959002
12.431182	879.746938	11.964019
12.352057	877.781850	11.969037
12.320864	875.878901	11.974055
12.237620	866.447929	11.979072
12.478641	880.885336	11.984090
12.384342	870.031456	11.989107
12.025490	875.224551	11.994125
12.529021	884.681330	11.999143
12.435245	883.236359	12.004160
12.415321	880.200102	12.009178
12.525791	877.251696	12.014195
12.218033	878.033787	12.019213
12.550571	880.373946	12.024231
12.423982	882.738952	12.029248
12.438427	892.343649	12.034266
12.605452	882.451559	12.039283
12.446735	882.486564	12.044301
12.334613	888.115556	12.049319
12.279454	897.978227	12.054336
12.313485	901.499655	12.059354
12.505926	891.990734	12.064371
12.321679	887.669542	12.069389
12.295610	895.537725	12.074407
12.444470	884.474287	12.079424
12.411473	891.999930	12.084442
12.856293	886.805317	12.089459
12.777310	892.595351	12.094477
12.604214	896.243985	12.099495
12.722996	894.093375	12.104512
12.344078	895.256918	12.109530
12.697368	893.253295	12.114547
12.631577	895.632644	12.119565
12.582659	889.024582	12.124583
12.492398	885.760217	12.129600
12.491363	894.910807	12.134618
12.581711	894.715209	12.139635
12.421464	896.112214	12.144653
12.290916	897.142901	12.149671
12.680071	894.037721	12.154688
12.311546	899.858381	12.159706
12.487733	904.137336	12.164723
12.821356	924.281234	12.169741
12.552684	921.949908	12.174759
12.433203	930.121752	12.179776
12.340421	924.302793	12.184794
13.010684	920.875087	12.189811
12.923228	914.955648	12.194829
13.068128	918.819729	12.199847
13.179871	916.175816	12.204864
12.861250	920.345381	12.209882
13.037066	917.216863	12.214899
13.166652	923.562897	12.219917
13.110037	913.951903	12.224935
13.210666	901.687046	12.229952
13.394255	902.404311	12.234970
13.119292	895.575814	12.239987
12.783268	890.089258	12.245005
12.528103	894.071939	12.250023
12.815229	886.793300	12.255040
12.658360	885.941427	12.260058
12.721803	902.920346	12.265075
13.082009	910.523795	12.270093
12.900589	919.133429	12.275111
13.247169	913.908619	12.280128
12.917019	925.662035	12.285146
12.905488	921.384671	12.290163
12.839183	921.674046	12.295181
12.952499	928.760538	12.300199
13.098707	920.442273	12.305216
13.167441	923.985518	12.310234
13.199877	924.503808	12.315251
13.162986	924.220622	12.320269
13.061556	919.706975	12.325287
13.199320	916.530430	12.330304
13.106996	922.130961	12.335322
13.220064	918.754184	12.340339
13.367196	924.657175	12.345357
13.211776	930.217371	12.350375
13.390958	920.395682	12.355392
12.756444	926.900525	12.360410
13.037115	920.475657	12.365427
13.231063	926.538999	12.370445
13.269379	919.741683	12.375463
13.238394	916.247822	12.380480
13.121299	927.180955	12.385498
13.190066	915.371737	12.390515
13.422702	914.461663	12.395533
12.987230	912.683919	12.400551
13.455880	910.280106	12.405568
13.188397	920.172438	12.410586
13.289398	916.907891	12.415603
13.109667	920.408817	12.420621
13.188832	919.304875	12.425639
13.242309	920.460990	12.430656
13.179164	913.091528	12.435674
13.261895	918.699682	12.440691
13.500910	930.760017	12.445709
13.361325	943.250754	12.450727
13.772527	929.698675	12.455744
13.474065	923.405923	12.460762
13.516724	915.447705	12.465779
13.626100	920.216841	12.470797
13.317588	922.457260	12.475815
13.623636	902.450862	12.480832
13.137180	914.160863	12.485850
13.229848	925.116345	12.490867
13.429366	931.347656	12.495885
13.437834	943.632783	12.500903
14.068658	940.989522	12.505920
13.941261	939.794592	12.510938
13.746090	917.911413	12.515955
13.678907	913.473196	12.520973
13.886707	917.357568	12.525991
13.851381	900.994939	12.531008
13.298588	914.067437	12.536026
13.491922	908.945560	12.541043
13.555909	904.059661	12.546061
13.466970	910.906813	12.551079
13.677387	907.318652	12.556096
13.283567	919.900285	12.561114
13.629840	926.617901	12.566131
13.824856	944.453385	12.571149
14.059294	939.858134	12.576167
13.933236	929.301584	12.581184
13.663093	909.430744	12.586202
13.582212	911.081919	12.591219
14.098300	924.474259	12.596237
13.572997	920.442199	12.601255
13.945638	912.394304	12.606272
13.590852	919.073287	12.611290
13.789247	935.614166	12.616307
13.957830	931.331776	12.621325
13.667839	939.302342	12.626343
14.113068	949.751843	12.631360
14.177007	940.156302	12.636378
14.343303	925.951897	12.641395
14.353245	913.050502	12.646413
14.073986	912.410223	12.651431
14.146031	910.298845	12.656448
14.505777	911.589275	12.661466
14.354984	913.962625	12.666483
14.201147	903.731938	12.671501
13.834351	916.492550	12.676519
14.169299	908.489873	12.681536
14.237199	917.760158	12.686554
14.242171	904.419850	12.691571
13.992522	884.101180	12.696589
13.764966	882.912209	12.701607
14.111304	892.720992	12.706624
14.103908	904.176076	12.711642
14.216712	904.070849	12.716659
14.346021	894.577892	12.721677
13.669196	890.585890	12.726695
13.810045	891.024418	12.731712
13.829963	903.814681	12.736730
14.027187	905.871358	12.741747
14.058144	903.849065	12.746765
14.146747	903.748239	12.751783
14.045012	900.652299	12.756800
14.076804	906.291324	12.761818
13.881580	910.310144	12.766835
14.358111	900.430962	12.771853
14.347678	908.517812	12.776871
14.127146	900.511456	12.781888
13.980191	897.069478	12.786906
13.748863	907.971909	12.791923
14.268264	919.214976	12.796941
14.134960	932.388491	12.801959
14.200700	936.962504	12.806976
14.444037	936.738028	12.811994
14.192173	945.279817	12.817011
14.443759	939.251080	12.822029
14.257788	942.959335	12.827047
14.661304	943.287050	12.832064
14.491276	940.690579	12.837082
14.376966	941.345762	12.842099
14.020964	943.169657	12.847117
13.835225	943.338265	12.852135
14.424513	942.102215	12.857152
14.160318	937.766295	12.862170
13.747126	946.859579	12.867187
14.375228	941.011397	12.872205
14.275439	944.849470	12.877223
14.413146	955.470758	12.882240
14.416592	959.424411	12.887258
14.661741	964.105726	12.892275
14.609498	965.085657	12.897293
14.836646	974.087885	12.902311
14.713859	961.763129	12.907328
14.265883	952.146840	12.912346
14.442628	966.104834	12.917363
14.646518	958.699400	12.922381
14.769378	969.181429	12.927399
14.870870	964.218044	12.932416
14.859937	963.816784	12.937434
14.721002	945.352850	12.942451
14.808597	947.736335	12.947469
14.644945	940.898834	12.952487
14.697159	936.955384	12.957504
14.998048	937.202853	12.962522
14.834589	940.275124	12.967539
14.951511	933.930513	12.972557
14.848408	928.763233	12.977575
14.696212	930.710852	12.982592
14.733578	925.671880	12.987610
14.434067	936.269100	12.992627
14.615398	932.120421	12.997645
14.582140	961.399915	13.002663
14.979769	957.897667	13.007680
14.997202	962.975335	13.012698
14.651913	970.882242	13.017715
15.134354	959.065118	13.022733
15.149544	967.861111	13.027751
14.973296	967.676194	13.032768
15.366056	962.623635	13.037786
14.596698	949.306394	13.042803
15.117191	948.378179	13.047821
14.873190	940.860706	13.052839
15.138817	955.004751	13.057856
15.116984	947.208765	13.062874
14.733343	946.912527	13.067891
14.920467	952.159328	13.072909
15.209901	962.113004	13.077927
15.168572	965.045770	13.082944
15.174127	961.660410	13.087962
15.112176	957.264225	13.092979
15.223571	963.438492	13.097997
15.133828	949.504798	13.103015
15.123635	945.750412	13.108032
14.983806	947.450327	13.113050
15.124080	958.326299	13.118067
15.383126	958.850371	13.123085
15.039434	957.641650	13.128103
14.980557	957.515247	13.133120
15.228203	963.833480	13.138138
14.999910	963.758357	13.143155
15.400442	958.090760	13.148173
15.178130	968.718130	13.153191
15.017909	951.900952	13.158208
15.330347	968.124963	13.163226
15.280837	961.774830	13.168243
15.321228	961.718600	13.173261
15.277286	962.553856	13.178279
15.222624	967.834794	13.183296
15.527212	965.987252	13.188314
15.150702	961.261279	13.193331
15.357703	961.577443	13.198349
15.414834	959.429947	13.203367
15.237874	959.684105	13.208384
15.297113	954.023025	13.213402
15.402388	958.949931	13.218419
15.488840	959.559667	13.223437
15.164376	958.546179	13.228455
15.023894	963.467327	13.233472
15.420440	956.824053	13.238490
14.950080	964.224130	13.243507
15.496897	975.058778	13.248525
15.658266	982.985334	13.253543
15.595378	989.253428	13.258560
15.889090	982.525600	13.263578
15.589004	996.540927	13.268595
15.709356	983.724729	13.273613
15.788534	973.357778	13.278631
15.490085	973.735593	13.283648
15.338970	964.479178	13.288666
15.350329	978.122851	13.293683
15.828752	988.019660	13.298701
15.922536	996.967609	13.303719
15.454771	992.780339	13.308736
15.829404	990.648371	13.313754
15.695568	1004.627515	13.318771
15.986847	991.064927	13.323789
15.965151	987.204959	13.328807
15.927170	986.340873	13.333824
15.687556	962.609949	13.338842
15.606657	977.358222	13.343859
15.778910	985.053065	13.348877
15.846079	995.432527	13.353895
15.624451	999.284883	13.358912
16.089569	991.084633	13.363930
15.950341	999.205061	13.368947
16.144911	996.677729	13.373965
15.917133	990.082705	13.378983
16.001241	982.448286	13.384000
16.191476	974.694332	13.389018
15.537115	977.460906	13.394035
15.686288	978.043328	13.399053
16.202645	984.980827	13.404071
15.831133	983.837338	13.409088
16.110747	984.443435	13.414106
16.119140	986.641230	13.419123
15.985292	991.391609	13.424141
16.098716	985.885318	13.429159
15.811140	991.465845	13.434176
16.079900	980.460828	13.439194
16.094738	982.457957	13.444211
16.148300	989.862233	13.449229
16.406919	985.616493	13.454247
16.198586	986.858483	13.459264
16.209749	986.772448	13.464282
16.194137	998.560445	13.469299
15.926604	986.206490	13.474317
16.019095	990.100527	13.479335
16.113230	991.183382	13.484352
16.046424	992.229897	13.489370
16.000964	990.582830	13.494387
15.931514	982.245914	13.499405
16.050596	992.395921	13.504423
15.925591	994.906346	13.509440
16.125052	985.924924	13.514458
15.728997	993.596164	13.519475
16.076367	1013.324140	13.524493
16.326020	1003.534822	13.529511
16.057346	1012.993962	13.534528
16.385406	1010.015800	13.539546
16.369338	1022.176317	13.544563
15.979796	1011.688144	13.549581
16.400835	1018.628449	13.554599
16.167503	1015.347199	13.559616
16.720196	1005.489197	13.564634
16.411972	1010.791665	13.569651
16.608824	1015.328243	13.574669
16.761176	1004.082259	13.579687
16.369785	1016.160044	13.584704
16.533680	1005.277095	13.589722
16.424436	1008.455751	13.594739
16.827798	1006.154464	13.599757
16.781511	1004.485092	13.604775
16.343375	1003.862062	13.609792
16.852996	995.822544	13.614810
16.896950	1007.264871	13.619827
16.475630	1004.754092	13.624845
16.382944	1006.117480	13.629863
16.339167	1009.251832	13.634880
16.674607	1002.106473	13.639898
16.609418	999.745771	13.644915
16.758468	1008.805437	13.649933
16.886996	996.355184	13.654951
16.801325	1005.580088	13.659968
16.807019	999.433783	13.664986
16.784791	1004.031043	13.670003
17.151887	1014.279755	13.675021
17.115247	998.310926	13.680039
16.834484	1004.406450	13.685056
16.988403	1007.682075	13.690074
16.533040	1002.873875	13.695091
16.697204	1004.971866	13.700109
16.882973	1002.392844	13.705127
16.876930	1002.233283	13.710144
17.186975	1005.511400	13.715162
17.419342	1005.972966	13.720179
17.063941	1001.776535	13.725197
17.077032	996.855729	13.730215
16.597147	1016.449049	13.735232
16.991520	998.119962	13.740250
17.258224	1001.391477	13.745267
16.756767	1001.064354	13.750285
16.751131	1001.245264	13.755303
16.892274	1009.532648	13.760320
17.078914	1001.487556	13.765338
16.694651	1000.533965	13.770355
16.910123	1016.073323	13.775373
17.252598	1020.586971	13.780391
17.003663	1037.437455	13.785408
17.291592	1035.967453	13.790426
17.645282	1042.617752	13.795443
17.155940	1018.833215	13.800461
17.155155	1002.099813	13.805479
16.727748	1011.997818	13.810496
17.209603	1024.351467	13.815514
17.183272	1025.920396	13.820531
17.219008	1039.612053	13.825549
17.447392	1030.169141	13.830567
17.217205	1031.683641	13.835584
17.382104	1026.613283	13.840602
17.762965	1035.454272	13.845619
17.463224	1025.986612	13.850637
17.543971	1008.142895	13.855655
17.442411	1005.416575	13.860672
17.584350	996.239956	13.865690
17.529095	999.231332	13.870707
17.293941	987.868037	13.875725
17.344353	988.886481	13.880743
17.330029	988.840886	13.885760
17.359868	1001.903984	13.890778
17.676312	1001.544967	13.895795
17.344968	1015.093851	13.900813
17.785837	1017.817652	13.905831
17.592700	1014.205743	13.910848
17.293992	1013.057283	13.915866
17.477809	1017.898764	13.920883
17.428819	1031.164697	13.925901
17.597797	1030.433655	13.930919
17.526416	1028.528681	13.935936
17.674192	1017.838936	13.940954
17.581116	1026.169050	13.945971
17.471599	1031.991356	13.950989
17.766945	1023.749125	13.956007
17.650450	1028.347436	13.961024
17.739080	1020.877203	13.966042
18.235400	1025.982282	13.971059
17.847154	1034.565994	13.976077
17.729056	1033.624624	13.981095
17.684658	1030.367201	13.986112
17.948121	1030.900387	13.991130
17.762658	1034.788494	13.996147
17.247493	1030.680712	14.001165
17.934137	1019.998189	14.006183
17.611603	1041.559503	14.011200
17.597069	1036.730656	14.016218
18.070099	1042.373042	14.021235
17.984952	1030.400647	14.026253
18.199668	1022.539077	14.031271
17.842154	1028.237099	14.036288
17.602389	1029.278793	14.041306
18.058705	1024.220415	14.046323
17.982599	1030.429693	14.051341
17.914780	1025.676206	14.056359
17.555699	1040.125734	14.061376
17.621515	1044.266317	14.066394
18.192655	1052.374653	14.071411
18.464090	1055.176515	14.076429
18.287196	1054.050005	14.081447
18.405906	1056.478353	14.086464
18.360337	1043.198260	14.091482
18.314568	1024.802660	14.096499
17.878432	1026.243785	14.101517
18.061893	1023.655299	14.106535
17.972944	1027.964808	14.111552
18.003335	1046.565437	14.116570
18.990521	1043.755282	14.121587
18.287567	1051.267927	14.126605
18.296742	1027.095722	14.131623
18.460926	1024.065957	14.136640
18.099107	1022.895664	14.141658
17.857540	1019.334290	14.146675
18.059052	1034.666932	14.151693
18.225757	1044.396505	14.156711
18.373328	1057.929114	14.161728
18.548587	1047.046223	14.166746
18.708343	1049.451238	14.171763
18.669056	1054.071809	14.176781
18.413320	1042.009152	14.181799
18.442412	1059.391948	14.186816
18.362830	1051.738931	14.191834
18.448023	1050.114316	14.196851
18.338301	1058.796010	14.201869
18.268557	1047.076947	14.206887
18.356801	1045.292778	14.211904
18.290814	1049.878795	14.216922
18.926098	1044.331737	14.221939
18.834445	1050.503835	14.226957
18.334650	1044.782540	14.231975
18.791491	1044.670342	14.236992
18.659231	1049.881483	14.242010
19.017161	1040.548211	14.247027
18.431832	1054.750975	14.252045
18.446473	1046.207981	14.257063
18.678034	1044.705581	14.262080
18.511375	1037.955933	14.267098
18.982878	1034.438680	14.272115
18.855379	1041.681630	14.277133
18.403196	1043.204546	14.282151
18.607566	1044.325448	14.287168
18.565046	1042.367664	14.292186
18.641743	1040.544463	14.297203
18.233931	1057.411041	14.302221
18.676308	1066.143046	14.307239
19.037370	1070.236323	14.312256
19.217814	1069.351025	14.317274
19.197591	1066.765945	14.322291
18.922609	1068.560297	14.327309
19.131601	1071.286285	14.332327
19.221044	1068.960988	14.337344
19.077250	1068.055760	14.342362
19.431440	1067.578684	14.347379
19.040138	1056.239226	14.352397
18.904499	1044.572020	14.357415
19.142986	1056.808126	14.362432
19.089845	1076.360778	14.367450
19.332201	1064.243578	14.372467
19.081365	1062.928137	14.377485
19.184698	1065.062586	14.382503
19.391571	1067.811758	14.387520
19.205877	1057.700413	14.392538
19.071331	1037.043991	14.397555
18.874838	1043.615715	14.402573
19.349912	1051.268322	14.407591
19.521320	1056.424064	14.412608
19.042669	1061.383522	14.417626
19.292992	1070.670541	14.422643
19.273263	1074.349725	14.427661
19.466463	1066.253514	14.432679
19.388794	1067.178216	14.437696
19.165943	1075.747161	14.442714
19.493170	1067.662614	14.447731
19.435959	1067.559161	14.452749
19.433047	1067.758123	14.457767
19.506722	1077.208250	14.462784
19.059393	1065.954832	14.467802
19.357740	1064.645694	14.472819
19.514237	1063.700190	14.477837
19.676235	1073.549848	14.482855
19.624651	1063.644631	14.487872
19.631486	1072.028302	14.492890
19.727898	1062.014725	14.497907
19.479275	1068.184476	14.502925
19.075063	1064.928755	14.507943
19.266581	1058.424109	14.512960
19.471621	1065.544292	14.517978
19.631705	1065.222188	14.522995
19.554264	1069.308550	14.528013
19.595858	1060.734708	14.533031
19.435076	1060.701160	14.538048
19.947982	1065.552335	14.543066
19.843712	1066.929063	14.548083
19.757295	1064.848627	14.553101
20.025182	1064.421273	14.558119
20.090720	1066.117115	14.563136
19.895842	1064.818392	14.568154
19.933554	1060.533229	14.573171
19.760298	1061.544622	14.578189
19.684180	1062.032468	14.583207
19.967418	1063.213144	14.588224
19.698853	1070.586550	14.593242
19.731765	1059.865010	14.598259
20.061186	1073.325790	14.603277
20.009352	1084.522627	14.608295
20.083818	1078.110581	14.613312
19.993357	1091.083443	14.618330
20.148531	1098.520550	14.623347
20.079598	1085.250982	14.628365
19.745467	1081.657286	14.633383
20.104341	1087.156786	14.638400
19.953214	1091.302992	14.643418
19.933588	1090.363816	14.648435
20.210317	1090.566866	14.653453
19.927386	1088.781950	14.658471
20.100066	1081.170610	14.663488
19.872690	1089.260407	14.668506
20.383737	1089.597879	14.673523
19.979342	1092.355363	14.678541
20.078933	1089.638633	14.683559
20.268759	1085.699128	14.688576
19.914733	1098.539267	14.693594
20.427249	1090.274032	14.698611
20.264589	1088.939264	14.703629
20.475680	1094.226632	14.708647
21.010455	1088.583607	14.713664
20.146116	1090.655073	14.718682
20.223215	1087.904273	14.723699
20.198389	1096.118796	14.728717
20.083792	1098.478306	14.733735
20.461678	1109.604006	14.738752
20.756128	1125.043392	14.743770
20.696058	1121.938933	14.748787
20.626600	1122.536305	14.753805
20.492066	1126.090421	14.758823
20.978758	1110.725742	14.763840
20.326184	1109.801612	14.768858
20.632568	1110.665084	14.773875
20.882388	1111.789883	14.778893
20.645909	1102.746332	14.783911
20.975924	1093.949522	14.788928
20.510595	1089.557891	14.793946
20.476764	1091.331211	14.798963
20.992443	1102.187641	14.803981
20.730061	1099.551712	14.808999
20.917299	1091.884020	14.814016
20.810699	1101.891948	14.819034
20.723621	1091.565833	14.824051
20.674377	1093.418475	14.829069
20.672228	1103.300056	14.834087
20.916933	1118.870504	14.839104
21.035257	1131.449784	14.844122
21.075865	1116.719577	14.849139
20.808187	1109.992136	14.854157
20.792148	1110.313348	14.859175
21.491563	1114.734062	14.864192
20.697542	1108.773677	14.869210
20.733001	1102.162968	14.874227
21.396451	1115.167307	14.879245
21.041211	1111.350334	14.884263
21.238166	1103.945192	14.889280
21.160186	1105.021123	14.894298
21.319194	1098.678925	14.899315
21.524912	1081.821482	14.904333
20.993085	1084.769351	14.909351
21.469729	1071.878730	14.914368
20.942963	1077.361497	14.919386
21.040991	1076.695349	14.924403
21.097235	1070.792999	14.929421
20.973426	1074.992942	14.934439
21.028439	1081.477369	14.939456
21.629596	1102.146865	14.944474
21.426483	1097.064196	14.949491
21.264088	1098.514723	14.954509
21.107805	1103.777890	14.959527
21.549597	1103.523307	14.964544
21.246301	1111.865837	14.969562
21.440308	1116.578501	14.974579
21.441085	1108.636568	14.979597
21.301455	1113.214326	14.984615
21.478460	1111.168215	14.989632
21.641834	1108.733430	14.994650
21.406498	1106.563872	14.999667
21.607268	1102.941439	15.004685
21.436506	1112.287185	15.009703
21.705543	1113.310380	15.014720
21.775206	1114.493750	15.019738
21.307747	1117.791191	15.024755
21.777035	1109.351614	15.029773
21.478300	1109.189732	15.034791
21.513042	1111.636716	15.039808
21.405318	1107.725218	15.044826
21.010162	1110.826439	15.049843
21.487470	1112.553706	15.054861
21.556178	1122.197589	15.059879
21.608939	1121.573974	15.064896
21.779674	1136.041763	15.069914
21.787365	1138.027103	15.074931
21.994950	1133.964178	15.079949
22.095711	1135.216019	15.084967
22.117206	1129.676869	15.089984
22.053457	1116.205636	15.095002
22.199924	1110.374942	15.100019
22.007932	1105.019178	15.105037
22.245347	1106.771207	15.110055
22.288491	1099.675384	15.115072
22.157928	1107.731838	15.120090
21.968301	1101.025334	15.125107
22.205983	1100.458498	15.130125
22.107507	1103.576338	15.135143
22.081924	1103.691262	15.140160
22.098646	1106.660504	15.145178
21.786866	1101.394259	15.150195
22.269975	1100.711196	15.155213
21.611089	1106.154435	15.160231
21.921937	1104.721968	15.165248
22.065552	1102.573911	15.170266
21.837457	1119.401742	15.175283
22.235735	1123.229825	15.180301
22.264716	1132.173623	15.185319
22.437424	1120.060038	15.190336
22.332969	1123.629251	15.195354
22.187307	1125.868717	15.200371
22.568250	1118.978753	15.205389
22.013305	1125.386252	15.210407
22.439919	1126.134544	15.215424
22.417425	1131.133842	15.220442
22.178897	1126.466464	15.225459
22.369014	1124.320545	15.230477
22.463578	1126.354096	15.235495
22.507201	1123.952917	15.240512
22.728799	1126.395734	15.245530
22.750081	1128.194577	15.250547
22.824602	1118.831417	15.255565
22.472379	1136.901830	15.260583
22.452497	1123.916224	15.265600
22.548784	1121.425225	15.270618
22.236214	1134.252623	15.275635
22.188589	1123.769565	15.280653
22.181342	1134.679143	15.285671
22.689360	1152.687836	15.290688
22.669219	1153.484516	15.295706
22.655707	1161.134619	15.300723
22.975963	1162.029655	15.305741
23.041609	1167.069092	15.310759
22.638788	1156.910173	15.315776
22.733827	1162.368745	15.320794
22.548532	1162.169575	15.325811
22.915143	1157.230336	15.330829
22.547596	1163.448557	15.335847
23.006684	1158.036538	15.340864
22.860567	1160.964646	15.345882
22.825121	1158.806468	15.350899
23.300215	1146.997506	15.355917
22.967126	1158.074044	15.360935
23.132062	1146.260143	15.365952
23.049815	1150.293386	15.370970
22.969826	1162.064216	15.375987
23.118819	1155.914986	15.381005
22.910503	1153.930311	15.386023
23.233053	1155.176137	15.391040
23.301928	1144.802904	15.396058
23.039320	1147.924309	15.401075
23.292212	1147.587623	15.406093
23.249750	1150.322586	15.411111
23.291105	1145.618699	15.416128
23.072189	1149.811577	15.421146
23.176924	1150.143892	15.426163
23.340553	1144.136333	15.431181
22.899179	1154.770971	15.436199
23.326758	1162.986600	15.441216
23.612259	1172.862326	15.446234
23.358159	1193.699548	15.451251
23.624258	1175.904471	15.456269
23.726699	1180.031546	15.461287
23.465266	1177.546624	15.466304
23.606917	1177.738972	15.471322
23.390778	1172.942285	15.476339
23.731645	1174.809865	15.481357
23.708247	1174.164607	15.486375
23.875393	1157.409136	15.491392
23.570102	1150.916245	15.496410
23.435053	1144.725473	15.501427
23.903620	1140.576418	15.506445
23.646243	1145.972477	15.511463
23.625013	1135.666531	15.516480
23.845009	1139.583585	15.521498
23.653472	1150.113860	15.526515
23.924583	1145.768767	15.531533
23.666410	1152.052335	15.536551
23.776472	1157.067092	15.541568
23.724871	1162.170429	15.546586
23.740089	1183.359093	15.551603
24.043547	1174.318611	15.556621
24.184103	1170.751407	15.561639
23.894838	1165.162523	15.566656
23.925507	1164.215802	15.571674
24.093636	1165.739160	15.576691
24.211281	1162.452121	15.581709
23.658132	1156.566396	15.586727
23.754603	1157.304792	15.591744
24.443440	1159.598201	15.596762
24.058846	1170.280139	15.601779
24.086120	1167.463562	15.606797
24.264884	1172.001213	15.611815
24.279483	1168.942254	15.616832
24.137081	1164.644762	15.621850
23.994454	1177.587752	15.626867
24.005301	1172.560178	15.631885
24.150190	1173.587006	15.636903
24.085452	1168.625884	15.641920
24.484956	1166.778350	15.646938
23.951932	1175.670749	15.651955
24.182963	1167.968998	15.656973
24.254228	1168.640704	15.661991
24.048777	1171.240459	15.667008
23.999174	1169.809013	15.672026
23.857904	1192.173567	15.677043
24.352515	1190.649643	15.682061
24.463809	1198.900341	15.687079
24.418553	1196.302062	15.692096
24.769440	1199.571885	15.697114
24.689133	1198.112843	15.702131
24.448018	1187.476747	15.707149
24.697449	1202.271714	15.712167
24.409191	1203.125391	15.717184
24.854204	1195.771254	15.722202
24.696879	1206.115199	15.727219
24.359430	1195.418279	15.732237
24.699756	1194.284064	15.737255
24.657842	1205.433285	15.742272
24.851902	1187.753270	15.747290
24.928218	1194.481060	15.752307
24.672951	1196.679237	15.757325
24.491349	1198.212872	15.762343
24.698712	1190.665418	15.767360
24.928411	1192.954940	15.772378
24.716170	1194.362549	15.777395
24.719595	1192.610911	15.782413
24.565114	1205.339752	15.787431
25.038547	1214.546214	15.792448
25.020425	1207.183723	15.797466
24.957793	1220.072559	15.802483
24.628131	1211.604596	15.807501
24.864396	1211.915921	15.812519
24.766545	1211.853054	15.817536
25.172855	1211.172073	15.822554
25.323524	1202.167504	15.827571
25.254742	1211.304304	15.832589
25.484780	1207.341575	15.837607
25.341002	1211.823201	15.842624
25.783410	1199.173965	15.847642
25.238367	1207.779404	15.852659
25.227905	1211.127173	15.857677
25.613100	1203.225865	15.862695
25.327036	1216.376492	15.867712
25.638193	1200.456555	15.872730
25.583348	1204.736843	15.877747
25.285261	1203.900855	15.882765
25.681274	1199.694903	15.887783
25.492975	1199.898188	15.892800
25.872148	1193.469890	15.897818
25.798599	1200.902007	15.902835
25.697741	1190.408033	15.907853
25.762533	1174.425376	15.912871
25.533751	1178.895872	15.917888
25.359921	1174.712239	15.922906
25.709489	1179.343654	15.927923
25.744271	1177.267150	15.932941
25.726337	1175.357244	15.937959
25.444789	1178.476280	15.942976
25.173303	1183.885317	15.947994
25.480105	1190.824934	15.953011
25.788279	1200.469371	15.958029
25.776210	1204.657146	15.963047
25.674137	1198.237275	15.968064
26.076350	1196.753453	15.973082
25.742217	1197.607639	15.978099
25.819270	1198.118550	15.983117
25.948940	1200.527390	15.988135
26.087072	1201.910447	15.993152
25.940891	1197.280116	15.998170
26.099732	1198.529826	16.003187
25.986486	1197.241589	16.008205
26.340420	1201.000658	16.013223
26.137331	1199.379669	16.018240
26.169703	1188.839227	16.023258
26.187343	1195.838931	16.028275
25.812087	1198.741997	16.033293
26.026516	1194.836974	16.038311
25.808457	1202.189086	16.043328
25.814729	1197.399263	16.048346
26.061837	1211.252917	16.053363
25.990357	1223.520009	16.058381
26.511943	1224.813984	16.063399
26.080370	1235.888775	16.068416
26.441225	1230.436700	16.073434
26.241005	1236.903220	16.078451
26.611086	1224.805296	16.083469
26.491941	1234.048083	16.088487
26.456421	1234.872117	16.093504
26.894362	1231.865090	16.098522
26.597812	1235.393303	16.103539
26.399440	1229.494865	16.108557
26.344636	1221.277833	16.113575
25.968288	1228.703805	16.118592
26.642502	1220.966437	16.123610
26.812443	1220.703326	16.128627
26.414270	1220.705542	16.133645
26.714197	1227.862056	16.138663
26.441440	1230.092660	16.143680
26.850832	1226.024640	16.148698
26.671298	1227.611872	16.153715
26.267695	1225.639052	16.158733
26.631592	1227.055986	16.163751
26.509506	1247.131281	16.168768
27.054279	1251.555596	16.173786
26.873418	1253.876890	16.178803
26.685711	1257.006386	16.183821
26.928443	1247.840881	16.188839
27.041711	1249.914264	16.193856
26.746864	1256.282290	16.198874
26.685483	1245.595526	16.203891
26.708060	1250.533070	16.208909
27.094237	1247.525950	16.213927
26.664641	1253.371813	16.218944
27.050913	1242.249517	16.223962
27.100386	1243.739383	16.228979
27.130047	1246.873040	16.233997
27.328084	1250.271331	16.239015
27.284924	1258.525589	16.244032
27.314573	1245.097438	16.249050
27.075909	1259.435893	16.254067
27.150775	1260.073150	16.259085
27.299240	1270.033046	16.264103
27.396051	1279.824340	16.269120
27.799544	1283.422076	16.274138
27.572873	1267.473806	16.279155
27.468327	1255.233195	16.284173
27.850995	1245.111471	16.289191
27.788506	1242.160141	16.294208
27.762368	1243.753076	16.299226
27.466844	1242.536355	16.304243
27.353703	1243.319700	16.309261
27.668345	1234.241112	16.314279
27.869607	1239.769128	16.319296
27.915869	1231.776294	16.324314
27.617516	1239.309432	16.329331
27.258845	1246.091950	16.334349
27.562986	1237.620989	16.339367
27.711640	1247.293839	16.344384
27.383866	1237.233461	16.349402
27.611774	1247.660884	16.354419
27.717351	1276.053833	16.359437
27.986781	1271.395998	16.364455
27.984594	1275.914826	16.369472
27.675944	1269.079142	16.374490
27.547933	1272.305840	16.379507
27.627909	1267.114430	16.384525
27.909278	1272.102827	16.389543
27.471157	1274.602941	16.394560
27.924648	1266.531635	16.399578
28.246088	1270.748060	16.404595
27.736683	1286.239613	16.409613
28.094108	1286.626938	16.414631
28.060596	1291.421423	16.419648
28.443626	1296.376066	16.424666
28.380264	1298.573976	16.429683
28.801123	1292.441879	16.434701
28.934017	1271.795975	16.439719
28.359754	1273.325740	16.444736
28.585237	1262.243046	16.449754
28.745010	1261.129276	16.454771
28.523502	1259.992422	16.459789
28.449850	1250.999379	16.464807
28.296009	1259.884155	16.469824
28.602598	1258.864970	16.474842
28.741356	1269.823694	16.479859
28.632473	1261.285288	16.484877
28.686723	1260.638586	16.489895
28.503073	1261.763127	16.494912
28.481536	1264.674169	16.499930
28.828288	1260.192507	16.504947
28.797916	1256.083914	16.509965
28.882089	1264.301737	16.514983
28.561374	1263.308866	16.520000
28.766620	1257.382559	16.525018
28.709210	1256.937020	16.530035
28.108448	1259.404221	16.535053
28.583915	1247.370323	16.540071
28.521338	1266.870055	16.545088
28.800730	1258.278382	16.550106
29.142701	1261.041045	16.555123
28.748494	1256.939549	16.560141
28.864784	1256.986495	16.565159
28.850339	1252.339846	16.570176
28.891002	1261.440442	16.575194
29.177023	1266.080044	16.580211
28.747793	1275.507269	16.585229
29.332851	1276.294687	16.590247
29.369775	1277.988597	16.595264
29.213496	1267.290761	16.600282
29.228675	1261.440806	16.605299
28.831483	1267.280520	16.610317
29.011038	1276.685285	16.615335
29.202464	1282.452735	16.620352
29.494848	1293.393912	16.625370
29.421204	1281.836337	16.630387
29.399236	1287.313934	16.635405
29.249660	1288.460787	16.640423
29.609066	1296.052751	16.645440
29.754657	1294.111029	16.650458
29.376725	1292.448510	16.655475
29.227754	1288.214668	16.660493
29.466773	1282.768182	16.665511
29.038678	1283.460770	16.670528
29.477035	1290.035349	16.675546
29.217077	1287.215525	16.680563
29.346187	1298.126655	16.685581
29.687591	1287.404269	16.690599
29.344882	1287.849259	16.695616
29.431705	1293.009244	16.700634
29.927394	1299.760550	16.705651
29.944237	1313.068578	16.710669
29.991817	1295.428443	16.715687
29.958951	1293.823744	16.720704
29.438778	1288.320294	16.725722
29.815151	1291.888666	16.730739
29.836833	1316.038583	16.735757
29.966174	1321.817903	16.740775
30.052137	1314.252303	16.745792
29.513564	1320.686697	16.750810
29.853749	1318.506061	16.755827
29.869077	1311.791119	16.760845
30.350649	1322.398633	16.765863
29.957190	1323.216194	16.770880
29.867744	1321.253939	16.775898
29.982124	1317.500488	16.780915
29.793375	1320.928589	16.785933
29.959579	1315.810284	16.790951
30.416283	1327.750634	16.795968
30.230544	1324.703951	16.800986
30.377499	1336.955042	16.806003
30.382214	1343.451450	16.811021
30.617238	1342.465762	16.816039
30.444865	1326.819851	16.821056
30.357443	1317.008594	16.826074
30.636459	1309.946452	16.831091
30.208093	1323.479780	16.836109
30.488663	1327.136070	16.841127
30.730655	1333.767591	16.846144
30.684700	1339.558621	16.851162
31.100847	1337.069348	16.856179
30.557276	1319.186919	16.861197
30.256626	1317.757659	16.866215
30.586612	1323.061245	16.871232
30.583709	1324.839707	16.876250
30.868624	1328.609055	16.881267
30.574666	1334.256900	16.886285
30.675946	1336.642904	16.891303
30.806875	1325.990382	16.896320
30.656811	1323.728327	16.901338
31.068507	1326.707405	16.906355
30.959974	1323.693607	16.911373
30.918714	1328.110653	16.916391
30.910822	1329.158459	16.921408
30.753533	1326.046830	16.926426
31.380438	1329.119798	16.931443
30.885725	1334.772540	16.936461
30.974353	1322.851063	16.941479
30.977999	1325.865818	16.946496
31.032126	1334.972102	16.951514
31.344116	1330.559561	16.956531
31.141610	1327.408962	16.961549
30.977958	1325.968040	16.966567
31.322167	1326.303619	16.971584
31.689453	1345.557078	16.976602
31.729038	1334.292914	16.981619
31.320788	1324.995003	16.986637
31.512021	1323.726022	16.991655
31.705518	1324.127500	16.996672
31.213376	1328.432989	17.001690
31.508075	1318.654518	17.006707
31.094196	1320.437646	17.011725
31.411125	1342.019473	17.016743
31.598589	1348.055316	17.021760
31.657325	1363.889084	17.026778
31.950577	1358.854057	17.031795
31.635129	1358.162270	17.036813
31.577497	1359.647047	17.041831
31.890058	1353.415144	17.046848
32.044204	1359.875399	17.051866
32.012411	1356.325667	17.056883
32.022291	1349.895070	17.061901
31.778862	1339.558852	17.066919
32.033652	1337.962029	17.071936
31.568138	1345.919740	17.076954
32.039203	1346.309903	17.081971
31.708593	1350.417001	17.086989
31.977706	1353.262216	17.092007
32.039033	1347.314824	17.097024
31.808773	1356.244593	17.102042
32.253555	1355.009215	17.107059
31.989053	1358.747894	17.112077
32.106054	1350.386992	17.117095
32.143238	1351.369857	17.122112
31.929100	1360.740651	17.127130
32.197417	1352.676341	17.132147
32.038636	1355.330996	17.137165
32.075292	1356.793074	17.142183
32.379414	1371.320491	17.147200
32.085409	1376.078610	17.152218
32.546372	1375.515737	17.157235
32.575310	1385.485264	17.162253
32.454001	1385.247936	17.167271
32.780189	1379.412973	17.172288
32.561162	1389.495607	17.177306
32.784443	1386.538662	17.182323
32.870057	1380.778966	17.187341
32.779307	1385.572328	17.192359
32.741378	1388.130601	17.197376
32.764155	1385.434412	17.202394
32.800222	1368.340580	17.207411
32.798434	1388.198110	17.212429
32.460231	1383.719596	17.217447
32.866393	1381.060318	17.222464
32.798745	1384.967191	17.227482
33.024428	1372.633224	17.232499
33.052846	1373.823837	17.237517
32.991250	1376.532088	17.242535
33.026322	1376.249969	17.247552
32.994117	1376.193553	17.252570
33.023329	1378.413153	17.257587
32.843902	1380.464941	17.262605
32.998052	1377.993454	17.267623
33.145115	1374.462920	17.272640
32.612076	1374.728407	17.277658
32.806035	1375.388074	17.282675
32.912516	1375.953173	17.287693
32.921439	1378.944231	17.292711
32.815074	1393.048307	17.297728
32.980443	1407.374327	17.302746
33.135672	1401.355462	17.307763
33.336343	1407.149774	17.312781
33.297308	1407.239370	17.317799
33.391142	1410.069131	17.322816
33.257792	1406.711792	17.327834
33.704367	1401.171056	17.332851
33.413388	1401.342132	17.337869
33.567777	1395.639152	17.342887
33.544616	1403.879153	17.347904
33.524690	1410.087941	17.352922
33.560571	1415.595374	17.357939
34.101606	1411.688971	17.362957
34.126590	1426.372896	17.367975
34.161946	1403.979997	17.372992
33.906310	1398.107510	17.378010
34.093540	1394.934883	17.383027
34.308195	1388.472725	17.388045
33.816895	1389.578926	17.393063
34.339723	1384.562962	17.398080
34.219158	1389.891964	17.403098
34.092973	1388.113734	17.408115
33.645162	1383.270304	17.413133
33.649693	1381.117680	17.418151
33.965022	1388.232349	17.423168
34.191641	1398.714813	17.428186
34.091999	1412.198117	17.433203
34.298098	1414.552998	17.438221
34.415736	1419.258716	17.443239
34.580828	1423.167218	17.448256
34.590846	1419.077091	17.453274
34.694136	1400.566205	17.458291
34.147537	1396.819034	17.463309
34.138271	1396.123003	17.468327
34.472148	1403.833025	17.473344
34.394473	1407.945105	17.478362
34.366652	1417.187446	17.483379
34.753927	1414.136807	17.488397
34.644961	1417.195029	17.493415
34.603901	1408.554761	17.498432
34.658361	1420.666512	17.503450
34.695424	1417.368353	17.508467
34.761440	1417.072449	17.513485
34.656470	1418.859160	17.518503
34.704443	1419.436704	17.523520
34.384019	1415.754045	17.528538
34.588169	1418.512787	17.533555
34.963814	1422.562013	17.538573
34.702422	1422.539216	17.543591
34.507864	1413.397597	17.548608
34.854595	1435.110839	17.553626
35.001419	1438.321590	17.558643
34.996258	1444.476767	17.563661
35.039880	1451.010479	17.568679
35.496945	1445.525469	17.573696
35.606324	1442.339739	17.578714
35.256132	1438.801372	17.583731
35.458354	1414.191483	17.588749
35.217490	1419.730963	17.593767
35.432891	1414.372199	17.598784
35.111477	1419.202192	17.603802
35.084177	1427.018093	17.608819
35.389459	1443.621345	17.613837
35.385897	1440.020463	17.618855
35.598609	1433.316091	17.623872
35.324131	1442.915033	17.628890
35.372795	1440.533443	17.633907
35.713839	1442.488821	17.638925
35.526056	1435.834622	17.643943
35.611590	1441.676752	17.648960
35.529708	1434.306994	17.653978
35.727036	1435.924756	17.658995
35.911807	1443.815785	17.664013
35.546872	1441.251895	17.669031
35.627896	1437.346460	17.674048
35.887967	1438.915644	17.679066
35.633663	1438.992067	17.684083
35.907477	1440.781808	17.689101
35.578910	1440.186676	17.694119
35.749129	1447.487604	17.699136
36.100094	1460.558546	17.704154
36.184297	1467.780814	17.709171
36.265712	1467.746922	17.714189
35.978174	1470.030795	17.719207
36.429757	1472.536766	17.724224
36.229118	1464.635876	17.729242
36.313533	1467.391224	17.734259
36.639266	1465.764925	17.739277
36.044224	1471.319368	17.744295
36.774106	1465.702565	17.749312
36.262223	1457.810302	17.754330
36.367520	1467.825111	17.759347
36.522045	1460.645327	17.764365
36.280620	1459.060185	17.769383
36.190717	1457.147594	17.774400
36.417275	1456.885735	17.779418
36.494283	1464.487141	17.784435
36.592724	1463.846106	17.789453
36.256386	1464.183353	17.794471
36.461555	1457.749508	17.799488
36.544662	1465.038097	17.804506
36.488557	1457.829019	17.809523
36.801213	1470.916156	17.814541
36.735014	1489.841970	17.819559
36.905580	1488.647658	17.824576
37.274098	1491.387857	17.829594
37.030001	1491.619281	17.834611
37.104318	1485.442522	17.839629
37.183036	1495.555057	17.844647
36.925011	1500.308830	17.849664
37.222006	1493.761734	17.854682
36.950123	1491.772974	17.859699
36.973731	1494.195879	17.864717
36.833936	1492.947445	17.869735
36.892795	1490.423609	17.874752
36.879348	1483.625956	17.879770
36.765383	1486.923206	17.884787
36.819874	1490.699647	17.889805
37.128020	1509.663894	17.894823
37.538201	1521.656980	17.899840
37.673322	1512.949686	17.904858
37.505875	1514.060144	17.909875
37.964222	1518.759477	17.914893
37.491125	1515.863486	17.919911
38.249909	1513.017846	17.924928
37.808129	1496.787636	17.929946
37.651862	1473.625585	17.934963
37.794798	1469.020133	17.939981
37.796092	1487.714299	17.944999
37.944093	1473.841553	17.950016
38.111832	1472.468184	17.955034
37.678741	1477.190309	17.960051
37.837695	1472.229058	17.965069
37.720680	1481.740928	17.970087
37.811381	1474.016199	17.975104
37.824476	1487.903733	17.980122
37.796805	1497.555542	17.985139
38.118507	1499.809405	17.990157
38.240154	1512.156163	17.995175
38.430312	1509.975935	18.000192
38.539331	1504.788297	18.005210
38.430253	1506.099718	18.010227
38.516893	1496.239840	18.015245
38.125141	1495.399265	18.020263
38.341640	1498.903608	18.025280
38.201352	1506.690621	18.030298
38.578211	1507.636935	18.035315
38.400975	1498.071141	18.040333
38.310343	1491.839410	18.045351
38.313754	1504.776208	18.050368
38.564601	1497.370617	18.055386
38.282822	1502.082655	18.060403
38.313935	1493.771725	18.065421
38.021460	1499.065843	18.070439
38.219596	1515.725891	18.075456
38.613073	1523.379648	18.080474
38.335214	1541.601207	18.085491
38.477811	1531.771411	18.090509
38.623527	1539.216596	18.095527
38.637483	1536.495070	18.100544
39.047971	1537.506291	18.105562
38.307504	1535.410863	18.110579
38.825249	1541.307054	18.115597
38.762386	1551.352517	18.120615
38.850139	1562.443909	18.125632
39.311351	1557.067623	18.130650
39.607602	1554.524941	18.135667
39.152385	1549.719298	18.140685
39.119225	1552.064998	18.145703
39.087645	1554.248232	18.150720
39.134376	1551.289782	18.155738
39.099619	1557.966831	18.160755
39.135366	1551.562575	18.165773
39.291641	1554.808007	18.170791
39.294012	1561.029305	18.175808
39.823131	1572.655101	18.180826
39.631074	1574.062944	18.185843
39.617188	1564.103527	18.190861
39.615163	1581.770407	18.195879
39.713735	1578.701793	18.200896
39.920182	1579.583416	18.205914
39.702143	1584.646735	18.210931
39.789859	1573.795687	18.215949
39.963243	1575.031603	18.220967
39.957934	1581.092371	18.225984
40.121221	1572.120932	18.231002
40.020953	1566.140372	18.236019
40.252497	1545.896665	18.241037
40.037801	1539.835850	18.246055
40.043991	1541.547083	18.251072
39.768484	1536.752632	18.256090
39.774453	1550.915416	18.261107
40.141897	1560.711289	18.266125
40.320808	1564.734467	18.271143
39.965497	1562.879196	18.276160
40.452962	1564.920189	18.281178
40.318768	1566.342073	18.286195
40.387890	1558.472450	18.291213
40.316507	1566.757924	18.296231
40.429294	1569.255050	18.301248
40.634581	1562.330987	18.306266
40.299160	1575.933001	18.311283
40.690125	1564.443560	18.316301
40.696960	1567.090906	18.321319
40.581493	1573.616366	18.326336
40.827272	1562.733248	18.331354
40.456580	1564.731297	18.336371
40.739146	1560.286950	18.341389
40.567151	1561.269818	18.346407
40.805066	1569.317466	18.351424
40.419660	1560.766020	18.356442
40.604340	1562.744550	18.361459
40.972132	1567.872670	18.366477
41.006071	1582.700929	18.371495
41.083963	1590.241621	18.376512
41.159065	1580.327694	18.381530
41.034847	1586.082957	18.386547
41.121061	1582.608909	18.391565
41.465520	1585.147205	18.396583
41.042253	1591.871670	18.401600
41.224743	1586.965146	18.406618
41.274256	1595.416049	18.411635
41.327030	1587.446364	18.416653
41.341775	1583.848717	18.421671
41.448380	1591.249222	18.426688
41.623742	1583.752546	18.431706
41.240800	1584.218771	18.436723
41.608731	1576.384702	18.441741
41.744071	1583.611942	18.446759
41.270485	1583.353414	18.451776
41.464108	1581.030870	18.456794
41.377515	1582.706684	18.461811
41.723525	1594.375414	18.466829
41.848383	1606.006756	18.471847
41.552443	1611.759754	18.476864
41.796001	1611.259645	18.481882
41.471952	1621.019660	18.486899
41.629868	1617.317590	18.491917
42.155386	1609.220009	18.496935
42.216139	1606.060802	18.501952
42.530297	1607.003726	18.506970
42.265533	1616.217702	18.511987
42.297725	1610.417948	18.517005
42.612606	1603.887924	18.522023
42.572024	1599.940773	18.527040
42.718909	1605.620445	18.532058
42.369551	1603.346467	18.537075
42.476079	1602.254875	18.542093
42.790979	1601.755946	18.547111
42.336140	1593.814009	18.552128
42.601110	1582.556046	18.557146
42.805931	1588.776510	18.562163
42.562593	1590.077099	18.567181
42.226141	1571.438429	18.572199
42.483769	1592.029247	18.577216
42.742744	1586.984075	18.582234
42.810439	1602.004401	18.587251
42.669493	1598.348278	18.592269
42.915492	1597.022176	18.597287
42.922691	1596.247819	18.602304
43.040647	1599.844092	18.607322
42.936514	1597.484235	18.612339
43.044537	1596.042397	18.617357
42.960178	1586.360775	18.622375
42.882373	1594.491028	18.627392
42.831561	1584.360940	18.632410
43.054636	1600.231912	18.637427
42.813793	1597.431699	18.642445
42.945860	1596.227612	18.647463
42.826271	1601.982114	18.652480
43.098926	1612.242533	18.657498
43.222094	1624.521807	18.662515
43.250365	1627.532937	18.667533
43.301334	1619.110778	18.672551
43.242561	1629.332780	18.677568
43.316318	1620.501728	18.682586
43.272348	1625.832694	18.687603
43.365197	1615.176436	18.692621
43.762951	1639.326005	18.697639
43.724171	1650.504554	18.702656
43.819088	1637.352658	18.707674
43.719557	1648.427485	18.712691
43.910973	1647.858844	18.717709
43.862289	1646.301216	18.722727
43.984395	1653.813358	18.727744
44.023477	1653.836476	18.732762
43.979483	1646.449320	18.737779
44.090170	1652.131853	18.742797
44.278730	1645.049499	18.747815
44.127073	1652.197914	18.752832
44.444074	1649.476584	18.757850
44.426497	1640.963794	18.762867
44.244576	1646.138869	18.767885
44.538599	1645.709537	18.772903
44.307969	1646.883616	18.777920
44.457003	1647.075930	18.782938
44.498232	1640.977423	18.787955
44.572430	1643.593944	18.792973
44.322738	1639.214084	18.797991
43.975551	1644.486995	18.803008
44.279585	1638.771746	18.808026
44.300217	1645.705804	18.813043
44.358447	1651.152534	18.818061
44.470865	1657.083601	18.823079
44.478702	1672.241859	18.828096
44.527095	1670.593351	18.833114
44.628447	1677.027835	18.838131
44.771294	1672.884939	18.843149
44.799031	1667.778029	18.848167
44.504638	1677.874903	18.853184
44.995865	1687.629494	18.858202
45.282472	1691.102982	18.863219
45.444412	1702.672744	18.868237
45.268615	1696.973933	18.873255
45.492115	1700.406690	18.878272
45.252848	1693.939251	18.883290
45.312438	1695.094412	18.888307
45.261422	1692.925352	18.893325
45.663375	1689.994278	18.898343
45.465543	1687.388109	18.903360
45.644847	1693.693944	18.908378
45.819519	1690.756409	18.913395
45.469126	1693.548361	18.918413
45.765469	1691.519030	18.923431
45.513460	1689.689945	18.928448
45.839067	1690.513656	18.933466
45.605685	1691.709453	18.938483
45.676605	1689.090280	18.943501
46.067195	1677.548849	18.948519
45.896161	1693.010368	18.953536
45.864461	1688.040065	18.958554
45.762056	1683.697222	18.963571
46.002753	1686.266102	18.968589
46.341797	1689.371456	18.973607
45.670009	1684.248479	18.978624
46.110233	1693.162696	18.983642
45.979534	1672.062266	18.988659
45.999711	1688.932676	18.993677
46.300271	1678.284502	18.998695
46.432105	1690.191131	19.003712
46.222901	1686.001012	19.008730
46.399783	1678.759158	19.013747
46.493179	1706.178137	19.018765
46.751537	1698.889318	19.023783
46.486951	1696.981212	19.028800
46.561562	1697.700026	19.033818
46.466501	1694.665419	19.038835
46.262316	1697.219382	19.043853
46.922168	1699.565710	19.048871
46.561848	1711.336129	19.053888
46.930459	1703.763696	19.058906
46.916604	1697.901848	19.063923
46.724548	1708.544004	19.068941
47.312297	1699.608903	19.073959
46.702714	1703.541417	19.078976
47.089886	1703.240755	19.083994
47.304399	1699.568665	19.089011
46.875061	1709.727667	19.094029
47.544921	1691.493097	19.099047
47.081811	1698.297433	19.104064
47.070531	1701.607647	19.109082
47.489857	1715.086387	19.114099
47.345859	1723.063887	19.119117
47.445813	1738.953025	19.124135
47.418593	1736.759939	19.129152
47.240251	1726.941428	19.134170
47.333667	1729.139818	19.139187
47.409363	1736.186846	19.144205
47.884848	1735.048327	19.149223
47.825309	1740.690181	19.154240
47.528645	1729.029041	19.159258
47.511107	1729.385946	19.164275
47.849269	1727.135906	19.169293
48.064652	1726.610931	19.174311
47.603731	1723.398314	19.179328
47.684959	1738.963779	19.184346
48.342633	1743.342774	19.189363
48.368128	1759.488752	19.194381
48.381471	1747.174687	19.199399
48.201566	1758.216837	19.204416
48.120001	1755.459121	19.209434
48.581254	1755.480053	19.214451
48.493207	1758.078182	19.219469
48.197817	1755.009410	19.224487
48.346545	1756.308480	19.229504
48.324071	1761.911920	19.234522
49.003064	1760.140090	19.239539
48.311641	1756.689645	19.244557
48.799357	1754.562083	19.249575
48.897601	1751.042304	19.254592
48.589235	1752.963914	19.259610
48.766415	1748.462160	19.264627
48.542466	1751.303264	19.269645
48.505109	1755.222538	19.274663
48.843542	1748.101147	19.279680
48.858490	1751.848372	19.284698
49.035953	1747.238303	19.289715
48.700125	1757.606265	19.294733
48.692160	1745.370533	19.299751
48.902208	1758.669788	19.304768
49.190384	1771.257686	19.309786
49.399155	1775.650389	19.314803
49.095516	1781.569686	19.319821
49.181019	1774.395281	19.324839
48.985679	1777.892289	19.329856
49.173074	1785.657467	19.334874
49.585020	1773.656519	19.339891
48.974693	1774.558828	19.344909
49.379461	1775.347389	19.349927
49.335979	1775.472368	19.354944
49.687909	1787.124910	19.359962
50.003793	1798.228305	19.364979
49.738081	1798.655832	19.369997
50.029653	1793.026844	19.375015
50.041934	1795.394584	19.380032
49.715718	1803.632614	19.385050
50.142305	1790.815046	19.390067
50.195380	1802.482831	19.395085
50.396411	1794.690068	19.400103
50.433428	1784.451999	19.405120
50.010801	1782.200361	19.410138
50.134676	1778.747986	19.415155
50.037361	1791.243035	19.420173
50.472094	1797.972766	19.425191
50.446169	1792.221938	19.430208
50.253860	1801.327174	19.435226
50.112157	1789.560802	19.440243
50.083752	1798.410549	19.445261
49.897496	1789.098826	19.450279
50.468881	1787.116857	19.455296
50.475063	1806.059025	19.460314
50.524294	1816.854613	19.465331
50.702359	1815.799194	19.470349
50.800051	1809.290873	19.475367
50.588080	1817.575349	19.480384
50.614671	1832.062145	19.485402
51.180445	1819.134104	19.490419
50.584185	1817.528542	19.495437
50.590603	1814.749159	19.500455
50.984907	1816.411908	19.505472
51.114452	1836.895518	19.510490
51.365034	1832.788678	19.515507
51.025452	1838.315517	19.520525
51.399351	1836.456006	19.525543
51.588586	1835.378657	19.530560
51.353174	1831.984580	19.535578
51.792514	1830.782353	19.540595
51.752222	1845.205826	19.545613
52.055488	1832.704316	19.550631
51.928246	1830.911642	19.555648
51.575474	1825.490515	19.560666
51.850452	1810.250363	19.565683
51.678181	1824.069677	19.570701
51.764617	1822.498714	19.575719
51.821263	1826.205193	19.580736
52.121999	1824.553076	19.585754
52.294804	1827.005267	19.590771
51.642070	1829.328005	19.595789
52.000235	1824.844294	19.600807
52.426200	1817.761135	19.605824
52.147870	1827.417252	19.610842
52.073658	1830.095779	19.615859
52.128376	1830.665529	19.620877
52.165489	1826.021982	19.625895
52.102674	1819.724488	19.630912
51.904309	1823.653509	19.635930
52.440633	1817.726502	19.640947
52.067345	1824.893978	19.645965
52.296738	1840.776355	19.650983
52.575767	1846.186594	19.656000
52.138540	1855.843447	19.661018
52.580127	1854.427457	19.666035
52.584108	1852.471713	19.671053
52.673922	1854.711662	19.676071
52.777863	1857.231560	19.681088
52.641578	1870.416207	19.686106
52.926603	1864.828041	19.691123
52.729494	1884.072080	19.696141
52.845171	1881.246642	19.701159
53.219480	1876.541341	19.706176
52.536751	1875.198125	19.711194
52.865981	1874.060979	19.716211
53.283006	1878.933017	19.721229
53.170191	1873.773721	19.726247
53.197400	1880.629628	19.731264
53.203736	1906.355473	19.736282
53.377965	1903.461673	19.741299
53.346949	1913.396977	19.746317
53.245974	1906.243546	19.751335
53.591021	1900.594641	19.756352
53.526486	1905.512171	19.761370
53.769715	1906.173547	19.766387
53.666271	1910.095141	19.771405
53.955819	1906.584991	19.776423
54.397387	1905.524912	19.781440
54.175296	1901.712071	19.786458
54.137618	1890.490219	19.791475
54.057118	1894.723369	19.796493
54.130725	1901.433018	19.801511
54.102782	1890.128450	19.806528
54.586462	1907.533386	19.811546
54.487877	1905.685957	19.816563
54.412006	1900.036274	19.821581
54.370233	1888.641476	19.826599
54.753695	1895.583286	19.831616
54.378638	1898.726213	19.836634
54.552514	1901.792030	19.841651
54.539441	1915.789006	19.846669
54.599131	1923.176965	19.851687
54.704295	1918.743781	19.856704
54.640897	1925.126118	19.861722
54.941221	1920.279115	19.866739
55.016267	1922.575064	19.871757
54.864998	1908.075486	19.876775
55.057906	1913.556309	19.881792
54.703508	1923.981787	19.886810
55.067807	1913.721332	19.891827
54.907351	1914.735776	19.896845
55.025868	1904.740043	19.901863
55.158011	1924.800104	19.906880
54.882874	1945.235901	19.911898
55.306601	1950.484026	19.916915
55.066519	1945.230028	19.921933
55.268384	1958.821761	19.926951
55.696761	1950.648749	19.931968
55.396068	1952.405329	19.936986
55.500370	1950.873128	19.942003
55.554542	1947.170441	19.947021
55.755412	1948.240023	19.952039
55.950438	1940.308808	19.957056
55.781575	1959.162034	19.962074
55.925876	1967.179720	19.967091
55.949096	1981.354608	19.972109
55.955168	1966.026149	19.977127
56.200480	1974.060973	19.982144
56.162330	1974.076407	19.987162
56.537969	1965.773140	19.992179
56.390022	1967.602858	19.997197
56.464007	1975.653845	20.002215
56.817178	1958.663554	20.007232
56.745608	1949.045337	20.012250
56.782524	1933.859444	20.017267
56.623398	1926.480193	20.022285
56.582298	1932.877740	20.027303
56.428345	1916.702974	20.032320
56.505723	1922.802153	20.037338
56.616668	1923.961427	20.042355
57.027612	1940.611107	20.047373
56.758306	1954.439910	20.052391
57.091232	1949.310722	20.057408
57.029550	1961.700793	20.062426
57.143129	1960.145401	20.067443
56.943993	1948.333692	20.072461
56.944409	1957.518135	20.077479
57.276571	1952.590258	20.082496
57.224578	1954.765117	20.087514
56.806113	1949.369784	20.092531
56.810721	1951.885278	20.097549
57.122974	1952.566725	20.102567
57.320977	1964.361426	20.107584
57.318499	1987.498257	20.112602
57.650533	1971.604391	20.117619
57.517486	1978.281360	20.122637
57.347881	1991.242487	20.127655
57.748441	1970.055654	20.132672
57.728550	1980.672245	20.137690
57.401505	1990.142823	20.142707
57.990973	1982.485261	20.147725
57.784405	2003.616491	20.152743
57.860091	2003.670952	20.157760
58.120589	2005.920064	20.162778
58.037512	2017.564097	20.167795
58.198311	2009.516465	20.172813
58.043019	2012.269474	20.177831
58.203906	2006.957724	20.182848
58.189149	2012.665491	20.187866
58.341793	2011.553244	20.192883
58.404066	2000.041133	20.197901
58.129683	2011.993223	20.202919
58.698007	2014.053569	20.207936
58.776124	2034.340045	20.212954
58.779761	2033.543027	20.217971
58.955441	2034.200633	20.222989
58.993450	2030.752577	20.228007
59.105545	2031.128578	20.233024
59.163306	2038.252338	20.238042
59.008653	2032.062880	20.243059
59.323454	2027.933544	20.248077
59.241214	2021.725407	20.253095
59.281862	2032.137911	20.258112
59.337949	2021.387853	20.263130
59.365371	2014.528867	20.268147
59.628698	2022.381201	20.273165
59.414784	2024.665166	20.278183
59.710707	2021.395674	20.283200
59.321138	2023.231546	20.288218
59.595846	2021.175440	20.293235
59.755803	2023.971925	20.298253
59.850462	2014.732060	20.303271
59.936581	2016.517909	20.308288
59.785632	2015.559475	20.313306
59.852235	2013.430738	20.318323
59.626833	2006.333297	20.323341
59.264081	2017.284643	20.328359
59.429601	2016.435230	20.333376
59.990649	2032.715658	20.338394
59.869810	2044.491951	20.343411
60.182316	2051.175888	20.348429
60.009864	2049.631626	20.353447
59.930480	2052.171281	20.358464
60.199606	2050.919661	20.363482
60.194214	2061.570129	20.368499
60.512665	2068.496009	20.373517
60.398354	2081.541365	20.378535
60.614601	2080.051642	20.383552
60.589531	2076.190780	20.388570
60.572502	2082.471013	20.393587
60.796695	2072.129319	20.398605
60.618177	2075.947633	20.403623
60.907388	2078.069164	20.408640
60.695014	2071.320333	20.413658
60.987152	2092.284855	20.418675
61.303395	2092.354605	20.423693
61.188684	2117.167349	20.428711
61.570021	2108.537069	20.433728
61.633628	2108.398249	20.438746
61.130559	2102.342833	20.443763
61.389416	2098.475506	20.448781
61.380570	2102.881107	20.453799
61.666771	2107.331953	20.458816
61.777182	2109.623255	20.463834
61.681612	2096.504873	20.468851
61.694886	2100.239861	20.473869
61.463548	2099.262054	20.478887
61.843292	2090.815518	20.483904
61.950210	2097.442568	20.488922
61.575874	2095.643137	20.493939
61.476523	2113.765334	20.498957
61.753387	2118.012998	20.503975
62.283537	2123.720348	20.508992
62.241245	2121.398597	20.514010
62.143720	2117.938711	20.519027
62.173415	2129.639749	20.524045
62.157522	2126.225401	20.529063
62.381576	2120.880712	20.534080
62.523506	2138.558643	20.539098
62.543376	2148.882930	20.544115
63.076256	2138.975923	20.549133
62.810065	2144.882069	20.554151
62.778123	2146.013049	20.559168
63.171576	2145.180615	20.564186
62.754085	2143.390292	20.569203
63.361746	2146.144167	20.574221
62.936890	2141.479770	20.579239
62.820187	2150.812070	20.584256
62.981187	2147.569616	20.589274
62.817032	2145.248354	20.594291
63.328700	2137.187443	20.599309
62.779502	2139.149762	20.604327
63.692283	2149.018319	20.609344
63.422605	2140.753303	20.614362
63.352442	2159.931780	20.619379
63.871798	2164.462152	20.624397
63.883597	2171.069155	20.629415
63.643067	2171.259442	20.634432
63.985109	2162.221845	20.639450
63.782591	2170.829757	20.644467
63.955543	2166.379373	20.649485
63.831477	2180.808365	20.654503
63.802386	2155.615503	20.659520
63.748618	2159.839969	20.664538
63.768911	2172.392624	20.669555
64.156369	2163.108522	20.674573
63.966181	2161.323476	20.679591
63.930087	2167.788796	20.684608
63.820647	2180.466093	20.689626
63.819719	2199.978836	20.694643
64.474203	2191.748183	20.699661
64.308275	2193.706892	20.704679
64.405741	2197.437806	20.709696
64.666862	2213.747218	20.714714
64.429469	2223.851542	20.719731
65.143822	2218.988259	20.724749
65.259127	2231.408691	20.729767
65.164056	2232.517844	20.734784
65.321309	2220.287061	20.739802
65.054420	2223.099138	20.744819
65.277225	2227.945176	20.749837
65.280169	2221.182677	20.754855
65.560268	2216.073961	20.759872
65.480096	2218.846065	20.764890
65.491161	2220.825868	20.769907
65.806338	2207.534260	20.774925
65.997483	2216.343169	20.779943
65.906234	2216.763867	20.784960
65.709106	2211.460143	20.789978
65.569735	2221.651783	20.794995
65.693912	2215.208596	20.800013
65.607446	2215.078875	20.805031
65.461346	2221.433687	20.810048
65.632127	2213.579973	20.815066
65.560139	2220.535135	20.820083
65.975822	2218.877726	20.825101
66.059647	2227.333136	20.830119
66.150583	2234.901511	20.835136
66.205902	2239.988285	20.840154
65.947033	2238.619343	20.845171
66.129487	2237.954130	20.850189
66.235988	2256.060519	20.855207
66.381741	2260.935862	20.860224
66.956965	2268.529583	20.865242
66.864040	2268.937567	20.870259
66.786251	2262.996325	20.875277
66.689238	2265.771619	20.880295
66.765390	2257.471328	20.885312
67.085563	2260.850015	20.890330
67.053205	2261.653105	20.895347
66.785495	2259.965139	20.900365
66.941046	2257.650375	20.905383
67.270981	2276.853304	20.910400
67.511070	2269.228648	20.915418
67.812670	2278.745711	20.920435
67.607197	2267.905321	20.925453
67.585689	2279.695268	20.930471
67.898087	2285.608820	20.935488
67.762810	2279.707799	20.940506
67.737595	2276.066212	20.945523
68.094319	2272.222798	20.950541
67.779833	2268.375555	20.955559
68.047426	2272.655901	20.960576
68.136196	2269.156473	20.965594
67.747120	2264.475483	20.970611
67.732551	2264.475595	20.975629
68.333724	2266.243912	20.980647
68.494963	2262.647050	20.985664
68.556279	2259.924249	20.990682
68.171082	2264.035108	20.995699
68.216063	2260.230715	21.000717
68.685008	2265.582096	21.005735
68.407247	2263.811932	21.010752
68.339975	2256.602756	21.015770
68.336902	2262.146862	21.020787
68.545579	2280.750163	21.025805
68.582707	2294.585224	21.030823
68.558543	2295.092065	21.035840
68.759331	2291.208321	21.040858
68.850772	2298.012043	21.045875
68.774899	2288.847498	21.050893
69.124443	2307.047962	21.055911
69.112262	2315.547270	21.060928
69.143343	2320.049082	21.065946
69.221747	2319.181005	21.070963
69.519397	2313.959898	21.075981
69.643315	2309.825873	21.080999
69.392436	2309.417848	21.086016
69.923772	2307.943259	21.091034
69.594525	2315.294224	21.096051
69.508962	2314.432036	21.101069
69.616454	2320.517724	21.106087
69.636816	2339.346379	21.111104
69.966610	2341.550601	21.116122
70.048173	2341.636376	21.121139
69.744008	2341.919488	21.126157
69.879175	2344.659897	21.131175
69.931164	2346.821531	21.136192
70.852441	2355.357258	21.141210
70.836794	2358.265166	21.146227
70.798470	2351.842136	21.151245
71.004217	2335.345552	21.156263
70.878895	2338.276735	21.161280
70.933347	2327.778323	21.166298
70.873556	2327.410709	21.171315
71.020894	2327.020611	21.176333
71.055480	2321.107985	21.181351
71.068987	2326.405658	21.186368
70.970230	2323.209327	21.191386
70.998791	2342.052770	21.196403
71.111574	2347.139121	21.201421
71.217522	2355.564558	21.206439
71.140229	2365.450724	21.211456
71.282207	2358.830506	21.216474
71.393356	2357.144762	21.221491
71.417612	2360.505535	21.226509
71.602132	2354.486572	21.231527
71.192690	2363.749353	21.236544
71.822667	2381.531408	21.241562
71.655904	2387.294009	21.246579
71.854286	2388.018742	21.251597
72.033627	2387.296163	21.256615
72.171031	2388.244388	21.261632
72.165159	2382.083308	21.266650
72.096718	2389.399393	21.271667
71.670594	2388.217586	21.276685
72.239721	2387.217071	21.281703
71.928210	2400.537877	21.286720
72.311427	2411.101404	21.291738
72.330424	2412.863371	21.296755
72.246595	2410.328758	21.301773
72.343606	2402.956479	21.306791
71.865711	2427.593226	21.311808
72.703070	2431.580842	21.316826
73.227571	2433.781582	21.321843
73.176965	2436.079907	21.326861
73.369407	2430.497815	21.331879
72.787582	2434.327478	21.336896
73.332230	2435.024016	21.341914
73.434953	2429.521743	21.346931
73.405665	2434.919457	21.351949
73.518361	2427.702451	21.356967
73.467686	2436.484591	21.361984
73.710384	2427.151069	21.367002
73.758271	2433.298642	21.372019
73.487314	2435.238155	21.377037
73.567445	2420.594267	21.382055
73.539159	2439.144074	21.387072
74.185964	2434.631692	21.392090
73.850052	2434.529491	21.397107
74.065440	2451.906231	21.402125
74.375780	2457.766644	21.407143
74.060076	2461.169947	21.412160
74.145037	2465.359713	21.417178
74.230388	2459.390596	21.422195
74.152077	2455.510107	21.427213
74.264573	2457.205808	21.432231
74.166917	2464.777567	21.437248
74.100717	2473.800106	21.442266
74.601357	2477.715921	21.447283
74.633643	2491.555109	21.452301
74.559916	2488.701076	21.457319
74.949956	2491.167802	21.462336
75.020219	2490.202240	21.467354
74.949096	2496.477816	21.472371
75.002973	2507.900709	21.477389
75.657245	2510.580396	21.482407
75.480513	2518.685382	21.487424
75.493408	2505.137256	21.492442
75.619201	2504.548741	21.497459
75.894487	2498.786363	21.502477
75.777853	2501.942135	21.507495
75.869671	2504.035776	21.512512
75.950062	2501.756256	21.517530
75.865498	2497.779936	21.522547
75.749197	2493.734065	21.527565
76.092380	2502.779788	21.532583
75.798420	2507.992596	21.537600
76.127168	2503.190318	21.542618
76.216134	2500.356592	21.547635
76.066953	2498.609207	21.552653
76.107511	2495.450407	21.557671
76.216087	2516.484087	21.562688
76.375812	2533.050795	21.567706
76.210974	2529.512193	21.572723
76.106381	2533.240026	21.577741
76.157416	2531.429564	21.582759
76.355619	2556.988883	21.587776
76.576006	2565.840001	21.592794
76.841240	2565.741813	21.597811
76.849753	2558.834142	21.602829
77.059725	2554.443270	21.607847
77.060520	2560.504196	21.612864
77.216649	2581.565919	21.617882
77.267642	2587.472472	21.622899
77.547120	2588.756658	21.627917
77.786470	2587.694585	21.632935
77.598508	2585.704383	21.637952
77.949430	2587.812618	21.642970
78.018731	2595.959984	21.647987
78.204954	2590.559191	21.653005
77.965178	2577.775717	21.658023
77.903329	2582.436307	21.663040
77.922240	2584.010895	21.668058
78.271955	2575.193064	21.673075
77.996887	2579.842103	21.678093
78.642420	2573.775072	21.683111
78.326683	2566.053315	21.688128
78.455571	2568.431789	21.693146
78.451533	2576.712161	21.698163
78.573655	2577.860973	21.703181
78.476370	2574.660409	21.708199
78.828496	2575.585300	21.713216
78.643036	2573.628152	21.718234
79.011337	2568.225961	21.723251
78.598854	2572.181565	21.728269
78.748433	2583.395743	21.733287
78.640707	2587.083948	21.738304
79.004147	2586.813585	21.743322
79.374833	2597.890765	21.748339
79.196714	2595.652853	21.753357
79.080817	2593.224707	21.758375
79.304870	2615.024488	21.763392
79.253275	2620.413360	21.768410
79.540139	2625.819426	21.773427
79.273370	2632.562519	21.778445
79.401691	2626.234232	21.783463
79.813586	2631.962535	21.788480
79.832455	2635.195904	21.793498
80.106782	2647.480489	21.798515
79.975346	2638.934427	21.803533
80.234236	2645.267634	21.808551
80.799462	2644.480757	21.813568
80.616518	2642.536176	21.818586
80.912813	2637.484490	21.823603
80.606086	2636.834504	21.828621
80.817128	2631.467779	21.833639
80.617259	2627.419172	21.838656
80.518929	2631.540900	21.843674
80.938855	2636.586729	21.848691
80.452588	2630.816921	21.853709
81.140600	2650.659891	21.858727
81.201143	2662.829088	21.863744
80.992358	2668.462127	21.868762
81.257383	2666.140990	21.873779
80.951479	2678.275196	21.878797
81.295960	2664.002300	21.883815
81.215000	2662.853483	21.888832
81.128702	2667.879195	21.893850
81.710660	2684.482855	21.898867
81.308292	2683.628215	21.903885
81.638984	2694.075427	21.908903
81.868220	2689.529743	21.913920
81.324001	2693.423718	21.918938
81.976234	2708.480229	21.923955
82.172014	2719.862458	21.928973
82.235750	2721.135523	21.933991
82.224051	2718.060139	21.939008
82.295976	2710.115451	21.944026
82.586971	2710.227973	21.949043
82.790854	2714.117388	21.954061
82.751024	2704.390686	21.959079
82.966864	2707.068193	21.964096
82.728444	2715.339804	21.969114
82.843716	2710.128683	21.974131
83.092639	2721.045783	21.979149
83.122227	2726.856320	21.984167
83.426477	2740.056563	21.989184
83.559378	2730.779231	21.994202
83.231517	2708.881631	21.999219
83.092012	2719.413405	22.004237
83.706962	2734.358390	22.009255
83.387694	2740.901938	22.014272
83.277953	2735.519387	22.019290
83.751885	2729.552763	22.024307
83.757254	2740.483035	22.029325
83.724762	2730.801168	22.034343
83.911627	2732.570813	22.039360
84.023352	2735.765205	22.044378
84.216751	2729.229630	22.049395
83.470309	2740.988369	22.054413
83.910853	2747.975843	22.059431
84.016621	2763.704425	22.064448
84.362900	2769.518453	22.069466
84.596465	2763.363250	22.074483
84.412538	2759.711999	22.079501
84.468815	2754.586621	22.084519
84.540455	2778.808105	22.089536
85.125532	2782.252504	22.094554
85.177959	2783.439645	22.099571
84.488071	2786.208068	22.104589
84.669673	2785.268545	22.109607
85.038658	2783.314459	22.114624
84.952310	2789.529283	22.119642
85.309510	2807.187294	22.124659
85.851951	2807.142035	22.129677
85.945248	2807.003412	22.134695
85.960332	2813.421547	22.139712
85.807823	2811.599868	22.144730
86.325472	2801.438650	22.149747
86.278773	2799.406919	22.154765
85.865827	2780.754259	22.159783
86.099229	2777.559535	22.164800
85.752721	2797.940543	22.169818
86.255425	2797.347491	22.174835
86.428442	2801.605452	22.179853
86.306128	2802.192738	22.184871
86.409972	2805.209696	22.189888
86.480208	2799.826461	22.194906
86.560510	2795.297531	22.199923
86.533945	2809.005789	22.204941
86.657561	2822.571075	22.209959
86.741436	2825.068468	22.214976
86.712719	2833.744825	22.219994
87.108298	2828.659315	22.225011
86.930116	2834.478306	22.230029
86.937413	2835.951291	22.235047
87.281921	2852.750758	22.240064
87.034822	2865.234063	22.245082
87.527746	2850.600959	22.250099
87.921840	2858.453722	22.255117
87.879627	2851.218466	22.260135
88.034744	2848.632406	22.265152
88.052456	2852.025080	22.270170
88.048907	2845.053919	22.275187
88.216479	2853.418238	22.280205
87.740340	2849.175139	22.285223
88.238819	2844.308038	22.290240
87.784271	2853.756542	22.295258
88.389050	2856.868536	22.300275
88.319632	2863.584564	22.305293
88.709465	2873.748462	22.310311
88.822757	2864.846375	22.315328
88.737333	2877.153302	22.320346
88.977306	2865.284727	22.325363
89.113090	2872.217590	22.330381
89.051734	2872.618394	22.335399
89.154342	2865.869824	22.340416
88.852237	2868.398845	22.345434
88.825986	2874.455315	22.350451
89.072673	2898.341285	22.355469
88.933979	2903.013513	22.360487
89.179083	2900.593269	22.365504
89.102892	2902.579337	22.370522
89.385229	2913.437099	22.375539
90.060012	2926.109577	22.380557
89.669364	2934.895526	22.385575
89.919443	2926.374727	22.390592
89.809890	2934.097121	22.395610
90.107480	2930.296019	22.400627
89.987059	2931.520058	22.405645
89.931112	2936.481770	22.410663
90.126098	2945.255414	22.415680
90.406135	2954.974119	22.420698
90.723687	2947.562313	22.425715
90.796669	2956.201032	22.430733
90.722458	2956.621290	22.435751
91.363374	2952.200692	22.440768
91.280188	2952.026322	22.445786
91.136925	2939.856151	22.450803
90.948935	2940.277136	22.455821
91.086436	2952.425549	22.460839
91.236495	2943.472838	22.465856
91.182352	2947.136900	22.470874
91.631339	2953.004077	22.475891
91.664896	2961.892655	22.480909
91.859185	2966.780265	22.485927
92.030987	2954.229543	22.490944
91.726229	2960.452248	22.495962
91.940239	2962.412324	22.500979
91.873383	2957.747462	22.505997
92.030880	2961.607609	22.511015
91.945102	2958.979913	22.516032
91.800485	2964.808751	22.521050
91.988418	2990.330715	22.526067
92.534883	2989.643790	22.531085
92.287497	2993.939124	22.536103
92.974362	2990.237744	22.541120
92.725589	2985.470304	22.546138
92.765159	2979.826707	22.551155
92.891399	2994.049245	22.556173
92.888135	3009.928424	22.561191
92.880337	3013.380480	22.566208
92.865011	3013.249209	22.571226
93.211528	3016.020892	22.576243
93.450388	3011.588099	22.581261
93.165030	3011.856688	22.586279
93.270848	3030.229469	22.591296
93.640704	3049.469662	22.596314
93.812126	3040.209000	22.601331
93.913060	3043.177663	22.606349
93.934750	3040.385296	22.611367
94.082759	3040.284074	22.616384
94.055575	3046.954601	22.621402
94.058133	3061.349267	22.626419
94.514648	3060.447290	22.631437
94.108270	3068.969752	22.636455
94.698041	3062.163275	22.641472
94.777638	3063.651872	22.646490
94.514818	3063.897830	22.651507
94.670412	3066.499147	22.656525
94.653105	3065.221246	22.661543
95.059771	3064.577152	22.666560
95.157801	3087.894664	22.671578
94.960542	3081.460241	22.676595
95.028157	3078.138168	22.681613
95.045060	3086.746083	22.686631
95.710528	3086.933630	22.691648
95.232149	3096.259047	22.696666
95.341439	3096.137461	22.701683
95.869897	3103.134953	22.706701
95.611569	3114.750941	22.711719
96.247610	3113.279815	22.716736
95.906335	3120.438246	22.721754
96.180123	3114.762120	22.726771
96.102061	3116.229184	22.731789
96.337894	3111.604720	22.736807
96.363589	3104.817595	22.741824
96.200689	3115.696455	22.746842
96.237994	3119.228083	22.751859
96.521743	3132.428116	22.756877
96.440531	3139.465931	22.761895
96.847267	3143.665603	22.766912
96.733776	3145.545268	22.771930
96.915098	3145.688554	22.776947
96.927681	3148.084012	22.781965
96.619525	3168.532781	22.786983
97.325654	3163.579623	22.792000
96.971684	3172.266315	22.797018
97.230268	3167.620743	22.802035
97.454755	3182.263844	22.807053
97.623124	3196.771353	22.812071
98.244317	3194.683325	22.817088
97.997790	3198.622237	22.822106
97.840762	3207.457855	22.827123
98.004936	3190.365225	22.832141
98.075050	3197.134285	22.837159
98.678053	3206.662653	22.842176
98.334391	3223.490231	22.847194
98.523818	3218.691904	22.852211
98.923795	3223.571527	22.857229
98.704824	3229.932906	22.862247
99.110672	3217.464889	22.867264
99.124455	3222.507676	22.872282
99.022207	3221.863575	22.877299
99.117761	3219.751932	22.882317
98.997189	3220.398005	22.887335
99.241751	3215.312963	22.892352
99.270225	3227.280802	22.897370
99.322179	3237.165413	22.902387
99.612065	3242.830673	22.907405
99.345407	3248.719196	22.912423
99.728022	3248.809075	22.917440
99.997301	3247.422680	22.922458
99.747463	3245.846616	22.927475
99.922421	3254.998987	22.932493
99.758632	3261.956030	22.937511
100.178422	3271.906547	22.942528
100.086806	3267.752832	22.947546
100.050078	3276.922152	22.952563
100.480071	3292.466077	22.957581
100.407496	3301.564173	22.962599
100.488741	3299.124537	22.967616
100.570904	3300.398930	22.972634
100.842383	3314.818998	22.977651
100.966473	3314.764652	22.982669
101.261572	3324.020021	22.987687
101.321058	3331.264179	22.992704
101.360063	3324.087312	22.997722
101.551165	3329.675641	23.002739
101.612103	3321.322574	23.007757
101.904161	3322.905955	23.012775
102.130505	3331.714788	23.017792
101.928517	3322.066128	23.022810
101.660506	3335.263583	23.027827
102.251750	3344.764452	23.032845
102.050621	3358.056769	23.037863
102.342090	3348.890236	23.042880
102.389164	3356.282934	23.047898
102.536835	3352.239201	23.052915
102.836920	3345.330943	23.057933
102.576204	3344.602039	23.062951
102.512842	3346.119057	23.067968
102.771966	3343.858255	23.072986
103.082675	3357.854892	23.078003
103.344165	3364.449410	23.083021
102.792872	3361.892027	23.088039
103.335957	3365.262401	23.093056
103.268195	3372.011054	23.098074
103.221445	3372.282271	23.103091
103.123676	3368.356739	23.108109
103.192910	3390.496660	23.113127
103.304949	3396.265839	23.118144
103.255762	3401.026556	23.123162
103.456135	3415.695131	23.128179
103.794599	3423.365244	23.133197
103.802700	3422.983212	23.138215
104.189294	3436.038508	23.143232
104.426460	3448.070794	23.148250
104.328420	3452.211195	23.153267
104.826387	3452.977729	23.158285
104.388776	3457.271609	23.163303
104.982549	3450.358386	23.168320
104.731547	3455.798279	23.173338
104.734109	3473.855961	23.178355
105.106657	3477.892861	23.183373
104.945485	3489.011092	23.188391
105.318382	3478.325309	23.193408
105.589179	3485.976732	23.198426
105.914778	3503.256862	23.203443
106.182853	3501.637152	23.208461
105.887024	3495.090123	23.213479
106.044985	3499.064120	23.218496
106.165577	3500.490060	23.223514
106.407027	3502.527956	23.228531
106.813398	3491.846859	23.233549
106.333060	3504.570493	23.238567
106.368913	3491.326015	23.243584
106.624668	3494.817229	23.248602
106.679550	3494.686536	23.253619
106.936954	3488.980702	23.258637
106.840251	3491.570312	23.263655
106.833481	3488.520735	23.268672
107.304154	3488.388926	23.273690
107.215503	3513.387785	23.278707
107.451019	3510.703651	23.283725
107.491486	3513.913545	23.288743
107.269948	3515.852880	23.293760
107.652095	3516.998874	23.298778
107.503075	3521.504076	23.303795
107.603316	3516.602694	23.308813
107.606842	3535.433217	23.313831
107.650043	3542.635676	23.318848
107.802068	3550.184339	23.323866
107.829037	3543.223563	23.328883
107.944025	3552.343907	23.333901
107.998078	3571.971326	23.338919
108.530894	3567.481046	23.343936
108.796115	3575.454343	23.348954
108.450722	3578.605679	23.353971
108.799432	3587.673566	23.358989
108.937090	3600.087058	23.364007
109.185478	3606.929943	23.369024
109.183755	3593.840044	23.374042
109.286016	3602.149429	23.379059
109.381953	3590.214379	23.384077
109.698057	3596.375490	23.389095
109.815727	3591.544831	23.394112
109.980603	3583.772916	23.399130
109.734497	3586.249465	23.404147
109.813805	3586.910497	23.409165
109.649885	3609.362987	23.414183
109.695310	3609.686673	23.419200
110.072712	3621.539162	23.424218
109.961285	3629.210232	23.429235
110.193233	3634.170568	23.434253
110.363618	3643.570414	23.439271
110.525791	3644.837888	23.444288
110.615079	3632.133728	23.449306
110.949065	3652.033839	23.454323
111.058827	3660.782228	23.459341
111.078332	3669.278208	23.464359
111.166705	3661.788642	23.469376
111.803377	3661.524217	23.474394
111.728270	3663.925610	23.479411
111.761832	3659.097436	23.484429
111.385202	3663.475775	23.489447
111.549259	3657.264794	23.494464
111.926332	3671.695666	23.499482
112.059722	3692.173994	23.504499
112.170453	3690.044812	23.509517
112.714253	3695.568973	23.514535
112.750862	3692.345223	23.519552
112.251247	3688.636161	23.524570
112.487247	3687.461172	23.529587
113.051405	3680.802787	23.534605
113.030903	3682.289510	23.539623
112.896238	3693.107395	23.544640
112.955107	3711.024121	23.549658
113.040209	3714.551514	23.554675
113.162521	3709.710206	23.559693
112.944893	3718.155697	23.564711
112.766726	3730.450299	23.569728
113.863902	3743.336624	23.574746
113.754484	3745.727566	23.579763
113.667180	3748.904325	23.584781
113.875705	3747.094817	23.589799
113.858838	3749.613370	23.594816
114.202641	3758.158081	23.599834
114.184856	3763.343689	23.604851
114.240507	3762.370232	23.609869
114.913924	3768.176150	23.614887
114.757504	3761.234222	23.619904
114.785823	3751.591660	23.624922
114.783671	3771.848799	23.629939
115.485962	3781.917066	23.634957
115.682330	3791.035495	23.639975
115.756780	3793.638950	23.644992
115.460449	3775.705262	23.650010
115.443139	3782.402424	23.655027
115.812937	3791.440557	23.660045
115.399606	3786.975744	23.665063
115.384907	3786.048583	23.670080
115.864260	3777.587016	23.675098
115.599145	3793.061462	23.680115
116.114680	3803.946207	23.685133
115.808444	3809.472542	23.690151
116.039070	3813.577129	23.695168
116.471405	3810.005513	23.700186
116.488466	3830.340267	23.705203
116.566503	3833.571176	23.710221
116.752642	3840.324456	23.715239
117.271771	3837.316106	23.720256
117.477624	3836.531192	23.725274
117.200918	3845.160966	23.730291
117.500345	3841.202235	23.735309
117.491342	3835.155683	23.740327
117.043525	3834.446312	23.745344
117.531401	3841.628443	23.750362
117.431280	3849.228448	23.755379
117.565848	3858.997397	23.760397
117.637844	3871.541678	23.765415
117.652013	3867.070640	23.770432
117.846646	3874.034763	23.775450
117.815810	3900.110650	23.780467
118.202828	3903.800728	23.785485
118.166856	3909.587121	23.790503
118.230073	3918.205545	23.795520
118.613714	3926.536243	23.800538
118.420808	3929.572625	23.805555
118.806194	3927.444009	23.810573
118.863558	3947.484797	23.815591
118.898006	3959.977876	23.820608
119.253849	3951.093293	23.825626
119.474537	3958.938312	23.830643
119.438656	3974.156052	23.835661
119.697908	3974.451825	23.840679
119.833357	3980.495733	23.845696
119.980897	3977.632356	23.850714
120.287927	3984.970106	23.855731
120.329065	3975.684000	23.860749
120.453703	3979.607330	23.865767
120.449147	3997.925101	23.870784
120.577102	4002.564532	23.875802
120.473208	4004.393883	23.880819
120.977431	3999.903492	23.885837
121.039125	4000.146135	23.890855
120.692283	4005.932055	23.895872
121.010824	4011.782645	23.900890
121.607898	4028.506127	23.905907
121.534654	4027.919011	23.910925
121.743635	4017.458458	23.915943
121.818260	4020.918352	23.920960
121.855789	4012.314817	23.925978
121.972426	4021.344991	23.930995
121.638933	4026.043502	23.936013
122.247012	4045.078923	23.941031
122.515182	4056.432425	23.946048
122.470750	4051.268958	23.951066
122.657468	4054.125171	23.956083
122.608470	4049.977579	23.961101
122.837286	4045.513872	23.966119
122.526372	4048.380021	23.971136
123.087450	4059.836236	23.976154
122.784429	4072.912919	23.981171
123.026891	4077.601929	23.986189
123.355386	4069.173847	23.991207
123.011957	4102.960509	23.996224
123.547465	4102.440347	24.001242
123.631795	4109.219655	24.006259
123.798234	4106.914633	24.011277
123.908447	4111.005765	24.016295
123.884323	4126.272895	24.021312
124.287839	4130.190255	24.026330
124.489456	4132.327365	24.031347
124.280540	4132.654189	24.036365
124.195191	4133.659092	24.041383
124.099947	4150.612306	24.046400
124.860614	4156.671687	24.051418
124.854311	4160.728571	24.056435
124.892921	4160.697827	24.061453
125.448077	4157.691329	24.066471
125.263398	4157.503821	24.071488
125.553484	4165.327217	24.076506
125.428647	4169.376164	24.081523
125.600058	4179.319558	24.086541
125.777100	4170.521944	24.091559
125.705728	4172.519186	24.096576
126.098577	4172.825922	24.101594
126.117664	4185.786367	24.106611
126.048049	4206.017040	24.111629
126.503431	4209.036710	24.116647
126.471752	4204.965751	24.121664
126.240384	4205.173438	24.126682
126.537332	4223.817996	24.131699
126.527040	4231.047741	24.136717
127.291885	4229.676872	24.141735
126.856353	4235.994968	24.146752
127.149305	4243.788003	24.151770
127.233835	4265.261949	24.156787
127.365157	4261.777478	24.161805
127.646326	4258.393417	24.166823
127.933310	4265.340850	24.171840
127.856638	4271.538908	24.176858
128.024814	4290.693924	24.181875
128.227095	4294.385544	24.186893
128.407829	4284.943837	24.191911
128.604719	4291.698289	24.196928
129.102976	4291.658386	24.201946
128.938132	4296.661395	24.206963
128.650846	4287.476732	24.211981
129.182844	4306.657375	24.216999
128.986568	4318.770756	24.222016
129.352142	4313.837011	24.227034
128.954077	4314.742492	24.232051
129.222417	4313.892477	24.237069
129.382369	4341.523610	24.242087
129.236750	4346.428948	24.247104
129.471279	4346.401994	24.252122
129.892470	4367.743951	24.257139
129.808876	4373.741584	24.262157
130.043142	4373.636708	24.267175
130.022636	4392.194629	24.272192
130.046829	4398.536696	24.277210
130.205316	4407.172692	24.282227
130.696686	4425.231659	24.287245
131.052147	4428.448263	24.292263
130.916601	4443.293123	24.297280
131.254110	4446.593032	24.302298
131.327323	4432.738317	24.307315
131.574716	4433.484176	24.312333
131.818510	4445.425566	24.317351
131.721277	4459.484431	24.322368
132.151631	4463.283239	24.327386
132.502609	4463.886731	24.332403
132.415270	4467.579088	24.337421
132.440869	4453.766889	24.342439
132.283366	4454.980644	24.347456
132.499426	4447.531780	24.352474
132.795038	4454.978748	24.357491
132.324546	4470.698922	24.362509
132.799240	4476.067846	24.367527
132.845312	4491.213452	24.372544
132.946248	4496.129995	24.377562
133.120321	4503.647511	24.382579
133.368240	4510.299103	24.387597
133.749776	4511.663821	24.392615
133.353431	4521.750258	24.397632
133.468011	4511.097882	24.402650
133.427691	4525.221412	24.407667
133.378473	4540.703375	24.412685
134.322870	4537.393738	24.417703
134.361356	4542.339535	24.422720
134.331765	4534.622581	24.427738
134.811188	4546.235220	24.432755
134.632695	4568.242194	24.437773
134.859254	4570.414613	24.442791
134.983569	4570.217682	24.447808
134.856934	4563.420888	24.452826
135.066304	4570.101727	24.457843
134.972025	4593.400552	24.462861
135.391129	4591.127659	24.467879
135.350668	4601.795506	24.472896
135.781508	4603.913633	24.477914
135.960649	4608.223449	24.482931
135.776194	4625.065935	24.487949
136.393534	4618.502707	24.492967
135.949095	4631.582001	24.497984
136.091298	4637.463597	24.503002
135.971995	4639.973655	24.508019
136.293633	4648.035424	24.513037
136.818682	4666.776628	24.518055
136.659436	4674.932989	24.523072
136.782131	4677.510884	24.528090
137.112651	4688.708037	24.533107
137.397612	4706.084038	24.538125
137.842027	4697.693135	24.543143
138.098082	4701.599614	24.548160
138.296724	4702.367735	24.553178
138.649625	4698.162884	24.558195
138.245328	4704.488596	24.563213
138.808161	4695.500809	24.568231
138.841980	4695.237741	24.573248
138.937086	4695.911170	24.578266
139.238217	4695.651887	24.583283
138.731328	4695.184579	24.588301
138.943861	4708.407188	24.593319
138.983064	4721.200932	24.598336
139.035619	4719.028872	24.603354
139.344393	4715.006161	24.608371
139.428749	4722.237788	24.613389
139.648255	4728.245230	24.618407
139.847618	4752.809323	24.623424
139.841911	4748.784327	24.628442
140.141565	4752.679663	24.633459
140.239959	4753.158810	24.638477
140.326696	4768.269599	24.643495
140.511553	4779.877626	24.648512
140.653199	4781.504965	24.653530
140.819902	4783.770018	24.658547
140.740488	4785.020486	24.663565
141.092669	4802.014523	24.668583
140.903268	4819.482572	24.673600
141.192404	4819.534786	24.678618
141.425196	4808.925643	24.683635
140.967725	4830.244374	24.688653
141.567594	4839.654166	24.693671
141.679863	4839.689983	24.698688
141.856602	4853.870804	24.703706
141.639673	4864.550718	24.708723
141.518901	4864.814920	24.713741
142.092188	4883.236523	24.718759
142.482919	4895.584728	24.723776
142.328111	4895.731705	24.728794
142.741837	4901.635390	24.733811
142.898639	4930.391938	24.738829
143.482872	4930.480355	24.743847
143.196130	4931.759646	24.748864
143.492527	4926.879694	24.753882
144.237793	4925.460822	24.758899
143.942891	4921.712054	24.763917
143.827234	4914.224169	24.768935
144.174883	4925.650989	24.773952
143.826261	4930.712189	24.778970
144.469280	4938.249934	24.783987
144.474255	4953.453982	24.789005
144.381696	4941.437673	24.794023
144.430568	4953.940968	24.799040
144.867131	4972.949212	24.804058
145.164818	4975.051633	24.809075
144.760932	4986.154791	24.814093
145.234667	4980.908382	24.819111
145.437465	4984.644972	24.824128
145.087098	5009.416250	24.829146
145.474716	5007.828188	24.834163
145.401509	5013.229727	24.839181
145.577892	5027.318618	24.844199
146.017450	5038.920897	24.849216
146.409576	5043.267241	24.854234
146.644281	5029.930265	24.859251
146.811715	5048.166443	24.864269
146.929703	5050.870403	24.869287
146.706067	5045.700049	24.874304
147.033040	5045.551470	24.879322
147.458814	5039.120595	24.884339
147.407220	5058.835882	24.889357
147.861948	5067.562599	24.894375
148.022729	5078.971638	24.899392
147.925398	5071.150650	24.904410
147.815981	5069.996127	24.909427
148.178597	5071.521544	24.914445
148.192829	5065.680955	24.919463
148.509040	5079.927886	24.924480
148.407317	5103.168841	24.929498
148.343111	5095.251786	24.934515
148.652693	5100.398601	24.939533
148.846864	5115.298192	24.944551
149.001380	5121.205496	24.949568
149.131716	5139.501477	24.954586
149.383478	5125.531534	24.959603
149.343944	5139.735818	24.964621
149.468482	5158.201322	24.969639
149.649589	5151.100511	24.974656
150.023406	5171.554354	24.979674
150.200870	5180.661758	24.984691
150.413926	5185.297690	24.989709
150.145071	5185.938462	24.994727
150.050029	5183.102427	24.999744
150.280157	5200.478603	25.004762
150.484734	5209.824898	25.009779
151.065737	5229.844423	25.014797
151.272811	5229.027345	25.019815
151.420426	5242.521841	25.024832
150.938273	5242.011826	25.029850
151.555568	5247.885879	25.034867
151.892322	5261.327813	25.039885
151.966175	5259.755443	25.044903
152.144500	5265.168194	25.049920
152.258105	5271.966786	25.054938
152.514740	5272.476458	25.059955
152.625557	5282.061205	25.064973
152.728987	5282.739583	25.069991
153.256534	5276.876940	25.075008
153.110055	5287.361968	25.080026
153.399789	5279.201928	25.085043
153.117405	5286.774124	25.090061
153.463017	5297.329695	25.095079
153.725033	5307.875485	25.100096
153.542051	5316.075484	25.105114
153.947358	5314.197782	25.110131
153.726818	5323.147486	25.115149
154.128111	5334.850831	25.120167
153.996247	5337.708042	25.125184
153.961593	5353.769632	25.130202
153.787466	5356.689763	25.135219
154.579469	5370.835348	25.140237
154.627701	5379.049870	25.145255
155.018449	5394.129832	25.150272
155.054719	5407.386935	25.155290
155.364077	5408.584115	25.160307
155.492030	5424.117947	25.165325
155.308424	5432.782003	25.170343
156.086615	5434.363097	25.175360
156.030230	5440.594484	25.180378
156.250120	5445.416021	25.185395
156.377573	5457.720047	25.190413
156.439754	5461.391032	25.195431
156.755459	5463.666959	25.200448
156.771582	5474.744241	25.205466
156.768777	5479.084419	25.210483
156.828458	5487.501090	25.215501
157.180603	5488.488780	25.220519
157.517098	5500.585748	25.225536
157.553725	5507.560218	25.230554
157.837307	5513.678644	25.235571
158.244191	5511.182394	25.240589
158.042156	5512.027129	25.245607
158.575304	5521.954018	25.250624
158.433525	5534.883135	25.255642
158.505510	5535.188682	25.260659
158.806210	5527.978118	25.265677
158.782398	5549.148837	25.270695
159.249076	5556.250607	25.275712
159.207585	5562.567787	25.280730
159.307832	5553.715960	25.285747
159.654528	5565.519877	25.290765
159.538092	5582.167824	25.295783
160.321820	5584.006352	25.300800
160.033428	5586.782408	25.305818
160.157690	5585.738017	25.310835
160.395637	5587.459762	25.315853
160.313610	5610.204376	25.320871
160.824636	5606.435433	25.325888
160.539854	5614.909199	25.330906
161.269513	5623.692312	25.335923
161.343278	5638.852552	25.340941
161.479599	5648.574281	25.345959
161.555319	5635.883749	25.350976
161.517567	5638.450560	25.355994
161.673441	5632.745408	25.361011
161.929369	5650.940854	25.366029
162.352289	5662.451838	25.371047
162.618578	5665.907932	25.376064
162.569357	5667.025091	25.381082
162.814342	5657.289967	25.386099
162.571101	5673.974755	25.391117
162.856086	5678.140539	25.396135
163.329986	5678.942689	25.401152
162.916431	5697.131670	25.406170
163.126645	5685.995620	25.411187
163.706500	5703.994157	25.416205
163.805661	5714.659331	25.421223
163.559885	5713.165823	25.426240
163.689589	5718.556851	25.431258
163.908401	5733.323781	25.436275
164.333425	5743.569577	25.441293
164.054547	5755.852893	25.446311
164.746766	5753.899288	25.451328
164.640435	5770.867105	25.456346
165.006736	5774.682355	25.461363
164.925344	5777.157175	25.466381
165.033763	5786.082609	25.471399
165.049374	5794.587863	25.476416
165.245091	5809.887175	25.481434
165.626071	5818.746239	25.486451
165.982012	5831.241924	25.491469
165.995607	5833.706541	25.496487
166.143507	5842.163928	25.501504
166.331547	5856.335119	25.506522
166.665557	5862.494164	25.511539
166.592869	5861.671388	25.516557
166.895031	5876.198608	25.521575
167.497005	5881.764331	25.526592
167.482930	5887.384000	25.531610
167.764810	5890.203532	25.536627
168.060039	5886.999528	25.541645
167.944956	5892.176741	25.546663
168.361680	5888.209113	25.551680
168.268306	5900.540591	25.556698
168.436728	5901.839117	25.561715
168.602636	5901.363559	25.566733
168.554589	5915.697543	25.571751
169.150756	5919.059701	25.576768
168.744692	5935.451159	25.581786
168.760260	5938.596755	25.586803
169.086785	5949.562336	25.591821
169.189874	5965.291422	25.596839
169.851655	5964.653432	25.601856
169.514157	5975.595853	25.606874
169.775760	5991.913855	25.611891
170.257535	5992.620992	25.616909
170.353330	5994.671126	25.621927
170.523003	5990.727045	25.626944
170.346218	6007.221604	25.631962
170.930749	6023.119933	25.636979
171.029265	6020.569903	25.641997
171.264874	6041.172989	25.647015
171.653546	6039.356243	25.652032
171.405494	6048.791360	25.657050
171.567553	6048.407800	25.662067
172.067190	6058.119255	25.667085
172.255111	6067.215203	25.672103
172.155393	6065.860518	25.677120
172.126491	6077.191415	25.682138
172.468352	6086.630498	25.687156
173.125095	6092.688161	25.692173
172.821960	6093.199169	25.697191
172.688811	6102.130117	25.702208
173.185757	6124.379507	25.707226
173.215223	6126.732061	25.712244
173.639495	6128.261557	25.717261
173.982320	6155.389870	25.722279
174.273568	6144.193613	25.727296
174.316299	6156.603575	25.732314
174.662590	6155.667314	25.737332
175.016204	6148.581607	25.742349
174.699709	6151.619967	25.747367
175.010648	6163.880778	25.752384
175.154261	6174.219126	25.757402
175.468469	6181.528366	25.762420
175.663944	6172.323322	25.767437
175.429738	6177.684963	25.772455
175.672902	6174.726599	25.777472
175.597508	6188.369092	25.782490
175.725397	6206.257934	25.787508
175.984027	6214.011163	25.792525
176.006351	6222.239076	25.797543
176.561478	6234.054673	25.802560
176.205453	6241.136215	25.807578
176.399825	6249.401822	25.812596
176.587249	6261.013667	25.817613
176.851341	6278.363354	25.822631
177.308590	6281.956526	25.827648
177.517964	6292.862190	25.832666
177.708863	6313.412384	25.837684
177.841504	6309.423947	25.842701
178.078149	6324.326315	25.847719
178.277055	6325.404805	25.852736
178.678939	6330.079916	25.857754
178.463734	6343.662986	25.862772
179.178554	6340.903758	25.867789
178.808440	6348.740662	25.872807
179.087220	6344.001820	25.877824
179.347896	6370.362764	25.882842
179.309076	6384.912245	25.887860
179.356291	6381.117515	25.892877
179.814456	6399.927786	25.897895
180.181497	6396.768503	25.902912
180.165740	6408.924485	25.907930
180.439370	6429.383945	25.912948
180.630932	6434.732685	25.917965
180.497581	6438.695403	25.922983
180.880646	6454.979598	25.928000
181.158905	6457.098829	25.933018
181.181982	6466.579887	25.938036
181.485977	6478.052872	25.943053
181.719255	6490.723766	25.948071
182.169762	6488.757322	25.953088
182.442197	6487.575710	25.958106
182.358595	6502.481640	25.963124
182.889879	6512.000678	25.968141
182.861666	6517.500038	25.973159
183.154991	6513.070647	25.978176
183.363781	6510.832308	25.983194
183.606986	6505.753530	25.988212
183.842762	6520.229322	25.993229
183.576184	6535.368787	25.998247
183.883714	6537.662768	26.003264
184.617872	6542.177391	26.008282
184.395943	6536.897565	26.013300
184.470696	6541.482756	26.018317
184.401444	6564.164401	26.023335
184.499822	6567.579967	26.028352
184.588581	6575.516662	26.033370
184.661681	6589.468093	26.038388
184.937044	6585.771020	26.043405
185.169896	6606.435948	26.048423
185.124636	6628.029903	26.053440
185.534433	6632.068947	26.058458
185.665221	6654.673495	26.063476
186.006900	6655.496016	26.068493
186.096927	6666.298821	26.073511
186.317623	6675.385755	26.078528
186.642057	6678.882071	26.083546
187.354642	6678.924060	26.088564
187.618770	6673.108459	26.093581
187.493123	6666.027825	26.098599
187.912154	6681.936890	26.103616
188.003935	6691.361813	26.108634
187.988811	6698.727389	26.113652
188.457909	6707.552676	26.118669
188.167157	6697.715781	26.123687
188.379737	6695.966711	26.128704
188.626908	6697.655548	26.133722
188.800680	6715.772880	26.138740
188.965868	6714.343566	26.143757
189.010451	6728.581821	26.148775
189.091373	6730.684924	26.153792
188.933699	6744.044568	26.158810
189.290004	6761.012471	26.163828
189.497609	6757.867698	26.168845
189.408044	6777.336209	26.173863
189.615159	6791.049812	26.178880
190.183186	6800.462910	26.183898
189.943688	6816.683557	26.188916
190.472926	6829.180490	26.193933
190.603188	6846.523813	26.198951
190.958357	6866.813595	26.203968
191.525316	6866.363775	26.208986
191.545545	6869.312656	26.214004
191.856034	6878.475424	26.219021
192.134383	6896.122742	26.224039
192.206458	6886.898331	26.229056
192.459737	6889.874012	26.234074
192.630242	6912.627523	26.239092
193.094539	6913.747189	26.244109
193.404853	6914.562314	26.249127
193.217351	6919.971608	26.254144
193.545000	6918.298773	26.259162
193.684620	6939.817649	26.264180
194.031190	6942.350191	26.269197
193.998059	6944.606107	26.274215
193.744412	6944.118846	26.279232
193.926881	6953.694322	26.284250
194.268981	6973.053017	26.289268
194.640832	6982.759419	26.294285
194.701445	7010.212389	26.299303
194.765843	7013.420218	26.304320
194.882096	7034.602816	26.309338
195.271534	7043.197301	26.314356
195.624996	7042.630799	26.319373
195.770980	7068.554254	26.324391
195.877297	7065.056769	26.329408
196.273169	7070.608205	26.334426
196.200728	7099.712267	26.339444
196.531259	7093.839836	26.344461
196.553477	7110.850818	26.349479
196.771691	7127.070838	26.354496
197.032585	7129.849172	26.359514
197.394741	7143.883205	26.364532
197.720752	7147.735396	26.369549
197.730648	7163.629182	26.374567
198.117147	7169.824951	26.379584
198.333855	7177.956592	26.384602
198.531184	7180.663539	26.389620
199.045531	7170.444950	26.394637
199.060851	7186.577317	26.399655
199.375898	7200.026075	26.404672
199.626689	7200.881789	26.409690
199.389706	7211.676874	26.414708
199.736418	7204.756470	26.419725
199.987002	7208.959865	26.424743
200.042603	7231.722616	26.429760
200.575487	7232.200806	26.434778
200.296662	7229.633495	26.439796
200.609939	7221.671000	26.444813
200.742050	7236.704959	26.449831
200.601326	7259.475044	26.454848
200.980805	7249.188149	26.459866
201.286109	7264.478604	26.464884
201.159698	7278.806311	26.469901
201.129673	7288.640870	26.474919
201.691623	7316.099596	26.479936
201.699977	7321.564036	26.484954
202.062650	7332.596275	26.489972
202.112564	7342.114373	26.494989
202.802203	7351.010639	26.500007
203.096528	7376.078239	26.505024
203.352171	7379.007935	26.510042
203.004815	7376.540166	26.515060
203.715228	7383.010076	26.520077
203.697887	7397.883821	26.525095
203.934905	7407.809728	26.530112
204.325190	7405.897257	26.535130
204.300989	7417.440221	26.540148
204.346308	7433.283515	26.545165
204.857275	7443.691849	26.550183
204.945183	7455.647938	26.555200
205.494294	7452.310225	26.560218
205.691809	7464.962614	26.565236
205.742722	7462.915695	26.570253
205.927971	7482.820857	26.575271
206.078525	7486.037362	26.580288
206.569984	7488.987119	26.585306
206.386545	7501.623832	26.590324
206.673124	7524.874159	26.595341
206.769186	7520.807192	26.600359
207.139525	7533.007245	26.605376
207.790760	7542.193548	26.610394
207.735798	7548.318399	26.615412
207.604097	7543.684178	26.620429
207.650541	7553.836286	26.625447
208.408183	7558.994811	26.630464
208.468072	7561.542618	26.635482
208.373914	7573.753429	26.640500
208.636096	7593.757060	26.645517
209.201969	7591.851735	26.650535
209.067883	7608.384207	26.655552
209.071928	7617.824992	26.660570
209.638882	7629.602659	26.665588
209.721253	7645.325025	26.670605
210.231560	7657.875375	26.675623
209.973899	7667.264200	26.680640
210.537354	7675.571856	26.685658
210.200907	7683.681897	26.690676
210.707840	7685.547611	26.695693
210.953277	7704.756208	26.700711
211.073445	7709.491760	26.705728
211.531293	7718.864571	26.710746
211.417224	7737.941308	26.715764
211.769707	7744.815638	26.720781
212.600991	7756.203050	26.725799
212.237724	7763.129706	26.730816
212.815330	7764.532374	26.735834
212.781517	7771.167395	26.740852
212.963322	7788.644213	26.745869
213.211467	7787.157749	26.750887
213.610524	7796.404064	26.755904
213.815604	7799.045243	26.760922
213.965090	7825.115078	26.765940
214.479025	7821.497174	26.770957
214.713777	7810.940061	26.775975
214.397182	7820.558503	26.780992
214.707956	7811.798967	26.786010
214.889822	7825.994998	26.791028
214.906872	7846.533422	26.796045
215.079635	7839.731340	26.801063
215.526435	7856.442821	26.806080
215.415162	7876.706346	26.811098
215.519247	7881.876280	26.816116
215.633408	7896.356919	26.821133
216.198357	7899.876711	26.826151
216.133608	7913.486624	26.831168
216.425528	7920.371056	26.836186
216.714164	7942.128142	26.841204
216.824669	7952.573171	26.846221
217.521881	7964.612317	26.851239
217.855898	7978.097982	26.856256
218.299233	7981.400034	26.861274
218.042250	7997.881571	26.866292
218.220421	7998.050644	26.871309
218.519571	8003.404162	26.876327
218.617101	8018.189362	26.881344
218.853493	8017.605189	26.886362
219.155998	8033.995721	26.891380
219.158559	8047.440212	26.896397
219.552981	8048.250929	26.901415
219.589019	8070.503734	26.906432
220.170790	8073.134592	26.911450
220.248592	8094.511657	26.916468
220.413418	8111.394545	26.921485
220.800286	8101.629719	26.926503
220.869753	8129.251726	26.931520
221.160162	8123.116948	26.936538
221.188321	8123.314006	26.941556
221.491263	8147.187990	26.946573
221.828531	8156.399844	26.951591
221.872349	8165.749294	26.956608
222.215568	8174.723855	26.961626
222.419464	8193.379055	26.966644
222.722945	8203.193629	26.971661
223.184355	8212.963948	26.976679
223.258853	8216.367281	26.981696
223.539456	8214.561888	26.986714
223.800798	8225.343696	26.991732
223.947578	8237.014132	26.996749
224.605820	8231.215440	27.001767
224.560931	8251.756761	27.006784
225.159128	8254.263620	27.011802
225.122024	8258.700825	27.016820
224.869247	8267.038355	27.021837
225.498619	8274.023051	27.026855
225.505607	8288.103501	27.031872
225.534892	8291.702603	27.036890
225.927617	8291.116962	27.041908
225.760890	8315.430516	27.046925
226.234290	8317.420808	27.051943
226.005420	8343.001131	27.056960
226.446105	8348.435318	27.061978
226.924953	8365.954976	27.066996
226.687892	8383.355266	27.072013
227.533013	8391.607222	27.077031
227.667295	8409.611709	27.082048
227.781772	8407.028725	27.087066
227.701601	8425.642993	27.092084
228.106631	8437.704084	27.097101
228.508533	8451.792565	27.102119
228.839302	8469.437681	27.107136
228.985501	8472.419572	27.112154
229.393258	8487.536697	27.117172
229.483161	8500.003698	27.122189
229.821808	8493.743420	27.127207
229.807896	8494.002590	27.132224
229.949134	8519.985123	27.137242
230.078369	8521.059547	27.142260
230.045380	8536.018868	27.147277
230.612651	8552.055733	27.152295
230.692965	8570.434063	27.157312
230.787904	8576.387971	27.162330
231.202559	8584.092903	27.167348
231.156315	8612.112231	27.172365
231.996857	8610.099094	27.177383
232.005749	8621.933645	27.182400
231.870641	8631.688744	27.187418
232.319177	8649.193250	27.192436
232.403967	8665.578721	27.197453
232.668054	8683.554940	27.202471
233.270320	8695.583578	27.207488
233.526737	8706.828152	27.212506
234.063023	8724.020443	27.217524
234.324867	8735.504404	27.222541
234.676571	8731.820989	27.227559
234.697133	8748.321162	27.232576
235.118394	8747.627586	27.237594
235.246944	8750.862171	27.242612
235.170338	8755.293448	27.247629
235.724287	8773.027209	27.252647
235.672287	8775.607912	27.257664
236.031645	8787.467285	27.262682
236.277861	8808.109231	27.267700
236.447843	8806.829403	27.272717
236.853267	8818.965556	27.277735
236.818460	8836.517193	27.282752
237.064802	8843.243353	27.287770
237.692010	8858.367043	27.292788
237.693462	8868.066594	27.297805
238.092851	8867.962731	27.302823
237.783602	8891.604368	27.307840
238.524582	8888.857728	27.312858
238.708350	8908.034657	27.317876
238.617351	8923.575860	27.322893
238.762955	8926.674525	27.327911
239.107555	8956.595235	27.332928
239.263149	8952.539321	27.337946
239.206468	8975.460217	27.342964
239.486038	8993.936031	27.347981
240.223523	9014.533158	27.352999
240.494590	9024.188961	27.358016
241.025831	9039.164064	27.363034
241.474235	9042.540342	27.368052
240.984235	9050.810409	27.373069
241.448650	9064.245474	27.378087
241.795375	9074.036096	27.383104
241.993941	9072.872834	27.388122
242.483355	9091.213189	27.393140
242.418016	9115.279567	27.398157
242.610921	9111.042551	27.403175
242.980312	9123.366089	27.408192
242.919066	9128.300678	27.413210
243.414192	9154.113008	27.418228
243.352689	9166.301509	27.423245
243.814295	9175.862841	27.428263
244.379434	9203.821388	27.433280
244.293907	9200.692366	27.438298
244.386825	9211.955695	27.443316
244.693438	9228.739878	27.448333
244.967448	9238.734858	27.453351
245.425818	9264.220218	27.458368
245.620522	9264.444080	27.463386
246.222232	9267.809209	27.468404
246.113163	9278.161468	27.473421
246.436657	9280.385464	27.478439
246.376169	9286.565463	27.483456
246.636495	9300.377985	27.488474
246.918817	9315.343346	27.493492
246.959845	9321.586908	27.498509
247.248930	9344.344744	27.503527
247.266394	9359.475309	27.508544
247.353697	9376.535438	27.513562
248.170030	9390.256001	27.518580
248.180520	9400.788646	27.523597
248.490035	9416.059202	27.528615
248.609356	9429.942444	27.533632
248.702667	9446.041335	27.538650
249.247410	9465.981634	27.543668
249.506445	9487.024107	27.548685
249.561640	9501.655401	27.553703
249.956955	9512.396208	27.558720
250.283292	9531.235165	27.563738
250.817700	9530.447991	27.568756
250.705872	9556.627716	27.573773
250.995257	9558.027847	27.578791
251.468401	9572.647531	27.583808
251.936269	9595.263474	27.588826
252.381517	9589.738264	27.593844
252.337895	9614.578564	27.598861
252.582960	9613.535979	27.603879
253.230357	9621.944998	27.608896
253.022398	9628.719906	27.613914
253.804904	9638.982323	27.618932
253.769141	9646.485812	27.623949
253.799571	9658.733522	27.628967
254.156155	9680.603839	27.633984
254.218417	9683.730628	27.639002
254.821409	9692.384164	27.644020
254.621918	9719.528757	27.649037
255.040712	9730.310729	27.654055
255.023166	9745.811419	27.659072
255.118381	9758.393540	27.664090
255.523587	9770.450098	27.669108
256.045132	9792.369678	27.674125
256.206441	9808.411196	27.679143
256.466406	9818.805131	27.684160
256.711880	9839.023111	27.689178
256.979226	9847.971786	27.694196
257.018970	9874.364069	27.699213
257.723444	9885.076011	27.704231
257.755618	9893.405027	27.709248
257.878635	9904.732400	27.714266
258.479152	9932.960524	27.719284
258.383893	9941.532036	27.724301
258.537546	9969.178730	27.729319
258.664398	9983.635523	27.734336
258.971864	9997.251766	27.739354
259.659245	10007.694035	27.744372
259.513303	10027.126985	27.749389
259.801763	10043.361977	27.754407
260.187376	10053.995248	27.759424
260.404506	10080.130825	27.764442
260.701804	10095.110981	27.769460
260.793908	10117.680353	27.774477
261.047283	10126.894630	27.779495
261.815156	10148.211416	27.784512
261.717811	10166.645404	27.789530
262.177428	10177.543822	27.794548
262.137351	10190.782877	27.799565
262.327258	10209.958770	27.804583
263.170641	10214.576142	27.809600
262.996621	10236.957324	27.814618
263.488400	10228.821992	27.819636
263.570850	10251.972994	27.824653
263.873102	10259.615412	27.829671
264.766227	10264.387646	27.834688
264.616773	10293.923870	27.839706
265.012390	10302.826356	27.844724
265.286754	10304.674956	27.849741
265.391832	10322.277540	27.854759
265.317155	10329.831119	27.859776
265.769635	10354.910302	27.864794
266.331985	10363.425182	27.869812
266.375539	10379.579726	27.874829
266.476193	10384.889698	27.879847
266.789430	10397.925478	27.884864
266.859807	10436.818188	27.889882
267.230647	10437.450953	27.894900
267.219106	10463.966140	27.899917
267.632708	10480.749682	27.904935
268.140253	10501.590841	27.909952
268.137935	10525.146249	27.914970
268.456140	10528.426223	27.919988
268.661110	10551.452591	27.925005
268.763698	10576.185084	27.930023
269.239764	10592.362790	27.935040
269.831352	10621.891189	27.940058
269.961901	10628.525395	27.945076
270.136364	10639.985007	27.950093
270.227189	10661.149040	27.955111
270.614484	10692.737738	27.960128
270.738367	10715.698978	27.965146
271.609331	10727.443592	27.970164
271.789209	10747.625512	27.975181
271.661885	10763.421101	27.980199
272.292910	10774.877718	27.985216
272.396946	10806.678977	27.990234
272.638537	10825.475179	27.995252
273.230331	10838.425814	28.000269
273.645568	10848.763201	28.005287
273.526975	10871.443351	28.010304
273.799705	10889.679819	28.015322
274.428831	10890.136702	28.020340
274.301726	10917.252416	28.025357
274.373792	10942.894989	28.030375
274.957897	10966.388638	28.035392
274.933873	10981.004449	28.040410
275.509791	10990.722855	28.045428
276.043335	11014.836329	28.050445
276.189283	11028.480182	28.055463
276.476147	11041.910056	28.060480
276.457698	11058.937473	28.065498
276.990930	11076.502311	28.070516
277.302291	11096.563631	28.075533
277.590034	11113.294606	28.080551
278.045060	11120.360635	28.085568
277.893861	11147.895145	28.090586
278.385063	11156.348165	28.095604
278.682395	11176.276392	28.100621
278.945973	11195.458596	28.105639
279.149129	11200.339810	28.110656
279.206108	11211.645942	28.115674
279.838535	11229.645195	28.120692
280.235508	11249.640535	28.125709
280.474353	11262.076358	28.130727
280.636940	11275.902030	28.135744
280.985729	11294.665277	28.140762
281.290138	11294.139071	28.145780
281.884026	11313.224195	28.150797
282.170444	11323.833757	28.155815
282.346642	11326.778127	28.160832
282.227088	11340.847527	28.165850
282.182978	11346.781358	28.170868
282.333762	11368.434335	28.175885
282.353758	11388.996493	28.180903
282.866859	11409.631483	28.185920
283.019119	11441.982257	28.190938
283.325630	11448.333974	28.195956
283.652281	11479.414243	28.200973
283.643925	11505.736001	28.205991
284.235744	11525.415789	28.211008
284.462032	11555.449161	28.216026
284.624065	11570.439685	28.221044
285.036915	11600.404440	28.226061
285.432372	11620.959898	28.231079
285.772187	11653.177622	28.236096
285.963676	11665.848510	28.241114
286.788844	11687.390287	28.246132
287.129354	11708.979223	28.251149
287.072735	11731.469100	28.256167
287.662215	11745.451429	28.261184
287.424739	11768.782834	28.266202
288.033046	11778.349807	28.271220
288.292000	11805.521289	28.276237
288.393816	11816.116033	28.281255
289.103117	11840.954890	28.286272
289.029366	11866.728641	28.291290
289.291239	11872.076238	28.296308
289.580877	11901.776722	28.301325
289.564637	11942.916390	28.306343
290.289064	11952.987421	28.311360
290.774121	11983.580720	28.316378
291.102631	11993.826042	28.321396
291.392668	12016.380273	28.326413
291.752258	12035.739833	28.331431
291.955360	12054.458739	28.336448
292.077418	12073.027194	28.341466
292.227277	12083.801685	28.346484
292.666312	12103.821061	28.351501
292.815485	12125.694358	28.356519
293.455071	12146.977512	28.361536
293.466533	12168.979243	28.366554
293.622575	12198.010585	28.371572
294.118041	12216.041489	28.376589
294.730982	12240.819693	28.381607
295.100535	12253.876018	28.386624
294.776872	12282.277776	28.391642
295.384052	12299.023290	28.396660
295.984193	12311.748384	28.401677
295.918393	12343.993646	28.406695
296.195546	12346.964041	28.411712
296.499712	12378.462633	28.416730
296.999272	12403.236214	28.421748
297.467735	12415.571883	28.426765
297.505953	12443.338829	28.431783
298.014203	12446.488462	28.436800
298.222769	12479.454455	28.441818
298.163329	12496.953472	28.446836
298.709358	12513.920499	28.451853
298.675901	12535.321870	28.456871
299.382919	12545.005335	28.461888
299.411515	12583.521656	28.466906
299.714304	12600.190218	28.471924
300.102335	12619.438607	28.476941
300.158650	12629.207765	28.481959
300.625527	12647.953034	28.486976
300.708853	12676.196711	28.491994
301.078238	12693.041877	28.497012
301.780035	12711.609657	28.502029
301.423550	12733.517039	28.507047
301.787582	12750.331633	28.512064
301.933886	12782.953967	28.517082
302.715631	12806.061423	28.522100
303.094125	12824.280988	28.527117
302.807652	12855.712795	28.532135
303.503512	12874.825436	28.537152
304.077835	12892.702208	28.542170
304.254715	12921.474517	28.547188
304.634197	12937.085894	28.552205
304.305926	12964.618115	28.557223
304.871529	12976.230542	28.562240
305.574316	13004.660650	28.567258
305.657247	13017.700418	28.572276
306.620588	13037.147201	28.577293
306.380224	13059.866317	28.582311
306.819841	13078.901841	28.587328
307.027444	13102.646873	28.592346
307.316645	13116.293986	28.597364
308.192259	13131.029157	28.602381
307.866639	13157.409250	28.607399
308.399905	13183.703958	28.612416
308.925036	13196.138007	28.617434
309.183609	13224.259069	28.622452
309.253914	13236.629747	28.627469
309.403919	13255.672439	28.632487
309.927129	13281.242455	28.637504
310.098784	13299.099647	28.642522
310.482942	13323.294868	28.647540
310.643940	13345.323867	28.652557
310.674339	13368.337427	28.657575
311.432370	13392.467717	28.662592
311.878544	13413.567065	28.667610
312.013863	13441.770365	28.672628
312.380860	13457.961115	28.677645
312.786420	13484.710840	28.682663
313.044987	13497.520196	28.687680
313.803313	13532.238066	28.692698
313.998436	13547.281671	28.697716
314.402502	13553.942723	28.702733
314.592479	13576.783597	28.707751
314.593859	13586.757844	28.712768
315.197815	13616.166731	28.717786
315.352213	13633.511797	28.722804
315.702353	13655.293997	28.727821
315.577336	13676.010700	28.732839
316.088450	13690.075451	28.737856
316.356336	13714.005242	28.742874
316.265531	13748.038293	28.747892
316.987706	13773.358661	28.752909
317.375513	13793.647064	28.757927
317.401689	13813.801498	28.762944
317.752595	13843.052525	28.767962
317.927752	13869.030946	28.772980
318.389743	13899.089518	28.777997
318.482622	13928.366069	28.783015
319.112139	13956.597205	28.788032
319.366619	13982.321545	28.793050
319.868786	14004.531367	28.798068
320.331463	14027.969177	28.803085
320.011468	14055.533380	28.808103
320.795944	14076.872310	28.813120
321.156905	14098.246693	28.818138
321.545194	14121.813578	28.823156
321.870155	14132.101815	28.828173
321.990869	14155.298537	28.833191
322.537510	14172.100136	28.838208
322.546351	14196.801641	28.843226
322.820676	14216.899739	28.848244
323.273494	14230.057346	28.853261
323.421269	14263.996817	28.858279
324.155336	14288.754944	28.863296
324.328343	14309.059050	28.868314
324.097706	14335.048637	28.873332
324.582489	14364.456532	28.878349
325.012625	14393.941296	28.883367
325.299632	14420.863477	28.888384
325.952002	14439.261743	28.893402
325.667289	14476.433253	28.898420
326.107830	14499.900621	28.903437
326.218673	14530.073635	28.908455
326.469373	14555.634013	28.913472
327.047491	14588.647117	28.918490
327.437060	14620.197365	28.923508
328.249162	14650.678500	28.928525
328.393403	14672.732548	28.933543
328.974514	14700.262164	28.938560
329.235185	14730.684988	28.943578
329.350221	14754.988341	28.948596
330.206522	14773.933235	28.953613
330.187029	14799.084796	28.958631
330.561013	14824.237466	28.963648
331.020428	14840.367008	28.968666
331.253813	14877.322854	28.973684
331.960318	14890.554062	28.978701
332.399077	14910.836993	28.983719
332.523855	14926.771405	28.988736
333.003968	14946.525842	28.993754
332.959491	14969.924429	28.998772
333.630427	14986.911189	29.003789
333.541636	15013.570286	29.008807
333.834305	15033.532378	29.013824
334.162217	15059.191089	29.018842
334.249362	15095.735044	29.023860
334.699452	15118.344302	29.028877
335.142985	15152.805642	29.033895
335.352641	15177.011999	29.038912
336.006567	15205.413050	29.043930
336.302954	15236.998820	29.048948
336.855813	15253.395433	29.053965
337.026139	15275.387655	29.058983
337.190877	15311.118561	29.064000
337.740672	15328.169859	29.069018
337.768350	15362.984175	29.074036
338.159350	15380.269862	29.079053
338.115721	15415.479098	29.084071
338.217863	15440.961414	29.089088
339.014991	15475.366482	29.094106
339.269677	15509.613944	29.099124
339.723548	15538.015582	29.104141
340.235949	15569.252579	29.109159
340.327473	15606.354907	29.114176
340.881902	15630.775970	29.119194
341.065641	15653.215688	29.124212
341.968266	15680.805645	29.129229
341.851205	15711.800333	29.134247
342.293645	15738.686339	29.139264
342.725213	15767.672103	29.144282
342.465098	15800.596255	29.149300
343.281548	15826.361297	29.154317
343.607616	15857.558752	29.159335
343.919653	15876.634411	29.164352
344.164934	15898.310850	29.169370
344.308766	15925.161467	29.174388
344.898870	15942.507788	29.179405
345.241467	15974.060528	29.184423
345.439201	15999.740675	29.189440
345.999250	16020.465158	29.194458
346.510037	16050.187012	29.199476
346.851550	16075.242939	29.204493
347.289633	16087.348409	29.209511
347.347497	16117.000333	29.214528
347.979529	16139.196283	29.219546
348.044586	16159.865734	29.224564
348.621531	16182.955127	29.229581
348.971281	16210.232387	29.234599
349.155090	16243.761729	29.239616
349.643608	16266.030466	29.244634
349.704451	16296.601169	29.249652
350.423283	16319.867453	29.254669
350.442154	16345.509962	29.259687
350.881775	16373.508726	29.264704
351.272810	16392.707466	29.269722
351.349577	16425.026989	29.274740
351.966082	16451.125592	29.279757
352.175502	16480.196663	29.284775
352.397314	16516.049984	29.289792
352.973434	16535.141020	29.294810
353.555143	16576.595286	29.299828
353.423596	16600.138270	29.304845
353.866727	16626.187030	29.309863
354.239990	16668.968574	29.314880
354.868704	16679.781905	29.319898
354.893399	16715.289974	29.324916
355.184379	16750.810793	29.329933
355.694580	16785.458395	29.334951
355.992143	16821.069700	29.339968
356.555639	16837.905920	29.344986
356.780347	16882.796468	29.350004
357.501572	16918.139250	29.355021
357.703201	16943.213339	29.360039
357.858040	16970.817306	29.365056
358.488486	16997.715230	29.370074
358.960189	17020.107567	29.375092
358.935421	17049.737005	29.380109
359.624857	17073.039168	29.385127
359.770450	17109.384012	29.390144
359.896407	17136.665159	29.395162
360.208449	17176.868245	29.400180
360.972770	17205.719491	29.405197
361.393777	17236.408866	29.410215
361.202423	17268.615198	29.415232
361.659048	17301.245576	29.420250
361.801735	17322.508944	29.425268
362.545418	17359.480465	29.430285
362.968090	17396.757415	29.435303
363.241647	17437.776169	29.440320
363.958981	17465.800178	29.445338
363.996229	17494.433345	29.450356
364.526823	17524.901766	29.455373
364.971423	17553.562198	29.460391
365.366377	17580.452753	29.465408
365.892811	17602.215731	29.470426
366.150710	17633.421510	29.475444
366.462288	17664.123482	29.480461
366.627128	17687.929497	29.485479
366.850724	17724.945348	29.490496
367.723539	17735.622815	29.495514
367.672191	17790.667693	29.500532
368.126417	17810.828674	29.505549
368.417181	17835.373879	29.510567
368.768660	17871.281180	29.515584
369.030102	17889.776387	29.520602
369.204826	17926.725108	29.525620
369.482735	17956.055417	29.530637
370.073110	17992.777853	29.535655
370.330458	18031.377817	29.540672
370.673816	18053.237894	29.545690
371.104469	18091.557089	29.550708
371.192417	18123.406716	29.555725
371.654974	18156.359381	29.560743
372.059831	18194.309469	29.565760
372.806182	18218.206019	29.570778
373.358517	18255.874882	29.575796
373.481066	18284.343951	29.580813
374.245057	18310.756857	29.585831
373.854033	18350.579407	29.590848
374.510648	18378.660724	29.595866
374.984867	18425.109499	29.600884
375.109966	18446.681467	29.605901
375.504994	18485.319601	29.610919
375.795675	18521.832689	29.615936
376.424983	18560.627703	29.620954
376.883017	18604.131675	29.625972
376.817635	18627.242501	29.630989
377.755847	18666.875766	29.636007
377.818059	18701.782801	29.641024
378.409512	18739.157788	29.646042
378.984244	18773.275465	29.651060
379.010480	18806.779300	29.656077
379.359848	18838.572837	29.661095
379.663027	18873.574352	29.666112
380.350918	18907.181710	29.671130
380.477160	18947.476572	29.676148
380.782574	18979.096353	29.681165
381.324381	19014.547385	29.686183
382.000134	19070.070481	29.691200
382.625956	19088.784178	29.696218
382.681564	19120.760873	29.701236
382.891763	19151.592717	29.706253
383.563787	19193.446879	29.711271
383.802063	19230.304409	29.716288
384.580041	19256.528895	29.721306
384.345703	19290.242357	29.726324
385.130287	19327.069595	29.731341
385.830238	19358.255889	29.736359
385.782373	19391.727438	29.741376
386.190322	19418.019723	29.746394
386.358618	19456.751228	29.751412
386.763741	19494.037346	29.756429
387.486252	19527.958687	29.761447
387.741584	19561.990522	29.766464
388.374307	19586.257837	29.771482
388.679396	19624.782633	29.776500
389.133191	19654.793115	29.781517
389.332255	19677.267258	29.786535
389.524247	19721.481899	29.791552
389.907977	19745.981419	29.796570
390.335735	19781.098221	29.801588
390.809051	19826.113199	29.806605
391.579205	19854.975960	29.811623
391.475591	19904.215697	29.816640
392.428416	19921.039487	29.821658
392.462673	19964.443704	29.826676
392.900359	19996.032478	29.831693
393.382015	20021.714406	29.836711
393.232242	20064.520275	29.841728
393.929408	20080.968739	29.846746
394.598426	20119.461244	29.851764
394.355698	20152.925565	29.856781
395.092230	20170.447580	29.861799
395.504088	20210.825912	29.866816
396.033395	20235.417147	29.871834
396.304447	20271.533683	29.876852
396.275889	20301.792271	29.881869
397.110807	20330.506391	29.886887
397.346022	20372.675437	29.891904
397.626937	20413.984067	29.896922
397.871511	20441.493776	29.901940
398.257246	20485.035093	29.906957
399.130870	20515.513692	29.911975
399.690374	20545.178753	29.916992
399.830260	20575.693753	29.922010
400.263075	20607.662878	29.927028
400.380864	20653.606070	29.932045
401.146111	20676.552292	29.937063
401.415753	20719.933690	29.942080
402.161032	20754.288903	29.947098
402.453196	20783.520899	29.952116
402.632850	20823.127144	29.957133
403.193449	20848.434638	29.962151
403.568136	20884.289375	29.967168
404.084954	20914.422542	29.972186
404.482497	20953.997765	29.977204
404.709147	20990.307662	29.982221
405.397078	21014.432314	29.987239
405.840713	21054.159391	29.992256
406.121207	21079.832080	29.997274
406.501206	21110.685141	30.002292
406.813268	21146.848797	30.007309
407.110894	21173.570454	30.012327
407.816687	21217.782828	30.017344
408.162620	21251.683256	30.022362
408.658482	21277.959173	30.027380
408.982003	21326.648320	30.032397
409.534989	21352.019323	30.037415
410.172288	21385.941177	30.042432
410.408721	21412.395837	30.047450
410.725416	21447.624371	30.052468
410.729193	21486.089766	30.057485
411.089922	21515.638067	30.062503
411.368388	21556.543101	30.067520
411.766629	21595.886355	30.072538
412.576765	21640.702229	30.077556
412.602886	21689.894166	30.082573
413.469253	21716.946707	30.087591
413.775371	21746.638473	30.092608
414.478711	21791.097151	30.097626
415.014081	21817.942890	30.102644
415.353423	21858.658828	30.107661
415.602147	21884.079407	30.112679
416.056945	21922.275633	30.117696
416.222229	21958.594611	30.122714
417.006672	21984.208927	30.127732
416.928818	22015.492609	30.132749
417.525947	22057.434097	30.137767
418.306379	22102.877367	30.142784
418.481134	22127.246218	30.147802
418.692558	22169.880956	30.152820
419.384880	22209.016135	30.157837
419.705321	22240.833502	30.162855
419.979662	22278.584200	30.167872
420.432629	22312.383892	30.172890
420.846898	22341.380774	30.177908
420.919730	22388.513994	30.182925
421.511491	22411.286306	30.187943
421.640838	22455.884295	30.192960
422.093666	22499.649914	30.197978
422.599810	22529.109692	30.202996
422.813533	22578.337806	30.208013
423.241884	22616.368097	30.213031
423.768837	22652.975611	30.218048
424.150906	22698.175764	30.223066
424.717144	22735.669451	30.228084
424.814460	22782.621527	30.233101
425.595059	22809.809854	30.238119
426.421664	22857.904510	30.243136
426.595470	22900.186204	30.248154
427.119542	22923.437159	30.253172
427.382090	22971.885667	30.258189
427.784288	23007.055984	30.263207
428.133840	23054.876925	30.268224
428.576927	23094.254078	30.273242
429.421026	23119.221603	30.278260
429.546233	23156.041760	30.283277
430.246700	23193.933698	30.288295
430.658700	23233.280049	30.293312
430.742930	23283.447807	30.298330
431.567666	23300.696724	30.303348
431.746285	23352.793386	30.308365
432.043786	23388.566851	30.313383
432.782943	23429.059542	30.318400
433.080550	23462.597080	30.323418
433.729695	23510.516374	30.328436
434.287578	23548.256081	30.333453
434.659244	23572.821494	30.338471
435.450481	23617.524297	30.343488
435.784167	23652.336706	30.348506
436.083170	23681.850107	30.353524
436.569613	23724.129415	30.358541
436.948476	23752.820752	30.363559
437.007275	23795.502164	30.368576
437.612478	23834.434731	30.373594
438.346053	23871.598878	30.378612
438.587362	23913.424056	30.383629
438.992906	23952.837792	30.388647
439.575413	23987.655439	30.393664
439.764939	24029.316005	30.398682
440.311588	24061.096186	30.403700
440.670365	24099.619124	30.408717
441.302387	24135.334064	30.413735
441.742007	24169.153845	30.418752
442.001205	24212.329845	30.423770
442.344814	24243.636177	30.428788
442.777050	24295.040867	30.433805
443.357416	24334.562173	30.438823
443.618874	24378.633953	30.443840
444.163163	24413.849890	30.448858
444.502290	24456.429787	30.453876
444.872702	24502.909295	30.458893
445.304963	24545.338377	30.463911
446.136235	24588.754984	30.468928
446.284199	24627.875417	30.473946
446.893431	24667.790126	30.478964
447.358082	24711.333948	30.483981
447.816499	24738.594446	30.488999
448.374373	24779.300123	30.494016
448.784669	24839.361712	30.499034
449.011174	24870.079828	30.504052
449.867059	24915.231095	30.509069
450.251522	24948.273018	30.514087
450.693332	24988.402272	30.519104
450.953590	25027.438796	30.524122
451.397214	25061.146128	30.529140
451.931926	25097.648787	30.534157
452.352981	25122.723955	30.539175
452.836757	25156.494221	30.544192
452.818038	25194.854992	30.549210
453.805499	25236.143573	30.554228
454.167690	25270.501933	30.559245
454.715167	25303.659501	30.564263
455.117059	25335.724646	30.569280
455.346869	25370.240741	30.574298
456.070254	25402.511453	30.579316
456.349756	25449.484851	30.584333
456.503881	25479.925849	30.589351
457.089402	25526.577555	30.594368
457.448440	25568.122332	30.599386
458.043462	25604.379521	30.604404
458.467662	25650.925783	30.609421
458.722334	25693.491179	30.614439
459.166768	25735.435433	30.619456
459.524995	25789.083745	30.624474
460.090583	25830.471958	30.629492
460.766051	25875.280249	30.634509
461.161355	25920.387361	30.639527
461.985254	25960.556592	30.644544
462.378535	26008.253944	30.649562
462.896369	26051.205661	30.654580
463.290451	26089.061660	30.659597
463.619800	26123.026558	30.664615
464.041127	26168.994299	30.669632
464.456945	26226.028499	30.674650
464.881997	26258.044214	30.679668
465.564303	26305.789191	30.684685
465.753157	26349.638303	30.689703
466.095632	26392.014248	30.694720
466.541783	26449.290207	30.699738
467.107146	26486.743364	30.704756
467.505594	26537.501080	30.709773
468.380105	26594.381732	30.714791
468.422937	26632.830143	30.719808
469.310914	26688.816178	30.724826
469.841851	26722.338820	30.729844
469.998699	26770.894400	30.734861
470.346678	26821.888421	30.739879
471.413375	26858.694777	30.744896
471.909597	26917.175312	30.749914
472.206208	26957.771649	30.754932
472.955268	27002.567535	30.759949
473.460860	27032.631351	30.764967
474.058670	27069.231843	30.769984
474.407888	27109.731506	30.775002
475.211562	27134.452919	30.780020
475.815962	27176.743280	30.785037
475.959017	27206.245950	30.790055
476.790476	27246.426389	30.795072
476.752459	27285.574158	30.800090
477.298647	27312.332100	30.805108
477.737043	27360.309623	30.810125
477.795992	27407.432092	30.815143
478.360696	27455.215476	30.820160
478.636939	27495.680797	30.825178
479.301319	27538.227098	30.830196
479.523510	27591.698462	30.835213
480.301909	27636.371258	30.840231
480.461101	27668.446195	30.845248
480.969142	27724.728737	30.850266
481.162017	27770.669130	30.855284
481.759162	27817.593240	30.860301
482.372834	27867.293979	30.865319
483.132758	27907.850573	30.870336
483.208805	27966.158107	30.875354
483.756504	27999.292423	30.880372
484.336970	28040.970537	30.885389
484.680981	28082.681568	30.890407
485.208088	28129.760071	30.895424
485.716020	28178.558028	30.900442
485.897351	28222.816917	30.905460
486.754873	28274.421766	30.910477
487.244748	28314.298411	30.915495
487.865481	28351.576080	30.920512
488.101756	28400.353362	30.925530
488.472688	28446.685654	30.930548
489.148754	28494.450311	30.935565
489.451965	28548.119417	30.940583
489.835928	28589.900765	30.945600
490.250126	28643.422452	30.950618
490.892724	28698.266224	30.955636
491.533719	28752.343817	30.960653
492.009110	28802.839879	30.965671
492.350204	28850.433793	30.970688
492.501449	28908.637387	30.975706
493.373568	28953.048825	30.980724
493.824897	29017.149990	30.985741
494.293919	29067.395482	30.990759
495.291288	29116.604077	30.995776
495.496606	29166.423415	31.000794
496.123067	29211.696429	31.005812
496.571391	29275.407832	31.010829
497.243922	29319.629231	31.015847
497.668278	29362.907477	31.020864
498.116702	29428.872028	31.025882
498.545348	29464.215189	31.030900
499.554559	29517.745206	31.035917
499.828220	29556.108234	31.040935
500.577634	29601.844619	31.045952
500.753552	29660.409446	31.050970
501.194181	29712.459817	31.055988
501.933395	29760.870567	31.061005
502.109759	29812.207766	31.066023
502.825518	29860.991807	31.071040
503.501559	29915.442641	31.076058
503.978051	29957.451725	31.081076
504.435577	30007.256958	31.086093
504.596045	30056.783363	31.091111
505.242572	30106.242099	31.096128
506.013270	30160.539208	31.101146
506.156955	30199.045040	31.106164
506.667369	30247.706382	31.111181
506.720884	30305.164097	31.116199
507.739534	30353.905699	31.121216
508.073419	30418.072432	31.126234
508.880937	30460.889287	31.131252
509.135174	30524.072572	31.136269
509.725727	30578.429177	31.141287
510.298044	30620.130562	31.146304
510.953624	30682.929339	31.151322
511.326623	30739.007286	31.156340
511.945550	30776.448179	31.161357
512.265066	30839.378845	31.166375
512.860512	30885.541603	31.171392
513.529071	30934.128192	31.176410
513.953435	30983.698726	31.181428
514.459994	31035.839914	31.186445
515.245695	31088.739649	31.191463
515.596195	31121.524416	31.196480
515.841977	31183.465148	31.201498
516.440425	31223.182149	31.206516
517.169030	31283.140727	31.211533
517.653067	31320.336899	31.216551
518.335704	31363.293358	31.221568
518.643585	31404.223140	31.226586
518.796264	31450.066230	31.231604
519.536721	31488.088029	31.236621
519.899326	31543.157402	31.241639
520.402702	31592.158082	31.246656
520.851215	31647.538562	31.251674
521.396920	31693.168949	31.256692
521.835784	31752.940415	31.261709
521.856046	31802.434965	31.266727
522.461089	31855.537278	31.271744
523.142413	31921.302234	31.276762
523.731919	31982.923838	31.281780
523.906562	32040.427101	31.286797
524.590648	32103.775249	31.291815
525.757823	32151.986076	31.296832
525.792443	32214.905666	31.301850
526.728494	32272.577149	31.306868
527.342138	32329.465975	31.311885
527.853840	32382.519048	31.316903
528.084024	32428.951379	31.321920
528.540526	32492.729851	31.326938
529.346671	32541.143472	31.331956
529.994574	32606.742948	31.336973
530.663636	32658.836784	31.341991
531.284640	32705.397656	31.347008
531.557107	32775.079989	31.352026
532.039818	32813.554346	31.357044
532.600335	32868.781262	31.362061
532.944697	32930.913738	31.367079
533.446349	32980.193069	31.372096
534.264391	33045.958503	31.377114
534.539843	33109.687098	31.382132
535.144690	33157.886417	31.387149
535.668354	33224.035709	31.392167
536.480488	33278.622699	31.397184
537.130312	33333.681655	31.402202
537.185881	33398.447996	31.407220
538.329892	33450.235202	31.412237
538.842178	33512.531258	31.417255
539.016467	33558.609726	31.422272
539.695106	33619.597433	31.427290
540.100082	33678.027195	31.432308
540.676795	33730.827387	31.437325
541.010445	33794.028107	31.442343
541.892085	33849.684594	31.447360
542.573917	33906.494596	31.452378
543.073694	33965.379814	31.457396
543.923140	34012.423843	31.462413
544.284574	34067.280320	31.467431
544.647009	34128.457781	31.472448
545.277079	34179.757797	31.477466
545.732226	34236.713652	31.482484
546.153517	34291.396812	31.487501
546.612152	34355.705451	31.492519
547.404416	34405.941021	31.497536
547.985265	34462.911510	31.502554
548.275576	34528.154337	31.507572
549.335131	34566.338212	31.512589
549.286724	34638.971647	31.517607
549.986026	34690.469957	31.522624
550.745425	34751.347173	31.527642
551.140322	34801.425534	31.532660
551.918205	34865.329719	31.537677
552.077177	34915.128689	31.542695
552.991844	34969.937417	31.547712
553.420016	35021.421576	31.552730
553.562517	35072.350368	31.557748
554.332499	35119.299997	31.562765
554.475937	35184.803049	31.567783
555.095600	35236.259295	31.572800
555.706441	35281.414695	31.577818
556.191129	35348.834356	31.582836
556.757700	35408.297113	31.587853
557.164760	35473.713413	31.592871
558.282231	35528.029514	31.597888
558.397981	35589.432658	31.602906
558.623003	35648.078502	31.607924
559.581739	35702.383521	31.612941
559.977397	35774.212703	31.617959
560.637767	35836.473390	31.622976
561.241686	35902.546695	31.627994
561.952897	35963.751595	31.633012
562.462183	36017.601708	31.638029
562.956114	36088.481678	31.643047
563.429817	36143.313289	31.648064
564.601339	36207.122391	31.653082
564.844502	36272.843288	31.658100
565.465398	36325.852103	31.663117
565.836728	36403.059565	31.668135
566.633501	36458.927553	31.673152
567.236641	36518.539414	31.678170
567.576070	36572.277255	31.683188
568.540869	36634.752289	31.688205
569.201751	36701.570264	31.693223
570.037477	36749.785217	31.698240
570.560955	36806.324428	31.703258
570.789640	36864.408645	31.708276
571.653897	36919.468363	31.713293
572.220356	36978.548090	31.718311
572.624869	37030.774145	31.723328
573.409536	37089.843381	31.728346
573.824291	37150.388029	31.733364
574.258151	37191.584789	31.738381
574.753695	37265.518078	31.743399
575.281448	37326.161400	31.748416
575.993424	37386.944885	31.753434
576.240382	37456.062492	31.758452
576.763195	37520.359163	31.763469
577.396041	37588.924195	31.768487
577.970899	37654.023912	31.773504
578.400443	37721.931836	31.778522
579.051394	37789.787599	31.783540
579.717603	37854.522559	31.788557
580.509737	37925.363525	31.793575
581.735846	37982.475088	31.798592
581.767807	38042.265366	31.803610
582.381010	38114.711737	31.808628
582.769835	38167.716983	31.813645
583.557330	38230.896018	31.818663
584.073620	38295.357484	31.823680
584.752449	38364.836365	31.828698
584.796275	38427.924481	31.833716
585.643141	38486.899582	31.838733
586.319088	38558.197830	31.843751
587.160203	38626.697585	31.848768
587.796388	38684.830665	31.853786
588.019419	38745.125087	31.858804
588.419451	38808.685883	31.863821
589.294269	38880.523824	31.868839
589.841743	38941.115593	31.873856
590.449174	39001.722895	31.878874
590.980816	39062.314528	31.883892
591.650324	39129.168396	31.888909
592.243307	39185.924457	31.893927
592.664960	39245.695228	31.898944
593.501669	39302.846944	31.903962
593.927971	39361.818691	31.908980
594.507049	39409.742235	31.913997
595.222978	39477.628240	31.919015
595.601871	39541.573878	31.924032
596.346334	39588.469854	31.929050
596.598192	39666.534801	31.934068
597.354455	39723.072950	31.939085
598.060169	39778.142283	31.944103
598.750369	39849.844106	31.949120
599.532922	39909.756205	31.954138
599.652446	39968.540742	31.959156
600.308104	40034.680456	31.964173
600.765535	40104.104704	31.969191
601.405509	40166.181535	31.974208
601.941780	40235.334375	31.979226
602.523411	40311.270310	31.984244
603.056112	40376.080471	31.989261
603.665460	40450.020426	31.994279
604.399297	40522.033334	31.999296
605.124576	40586.540883	32.004314
605.098575	40671.137128	32.009332
605.964182	40745.395755	32.014349
606.750370	40813.294006	32.019367
607.334690	40899.422446	32.024384
607.981267	40972.332332	32.029402
608.449025	41045.663552	32.034420
609.187501	41109.242599	32.039437
610.008718	41189.363374	32.044455
610.586405	41267.002348	32.049472
611.338506	41329.790651	32.054490
611.645500	41415.547494	32.059508
612.448151	41481.263976	32.064525
613.179764	41558.310440	32.069543
613.513123	41631.644117	32.074560
614.387468	41704.254011	32.079578
614.536757	41779.235143	32.084596
615.333913	41856.180446	32.089613
616.009289	41926.623634	32.094631
616.532144	42002.904577	32.099648
617.529798	42069.174949	32.104666
618.059533	42158.077601	32.109684
618.456917	42237.774198	32.114701
619.179415	42309.316046	32.119719
619.823220	42389.382956	32.124736
620.397354	42455.345912	32.129754
620.802167	42547.153609	32.134772
621.326379	42610.204952	32.139789
622.289829	42683.867917	32.144807
622.793433	42769.993134	32.149824
623.397878	42846.204047	32.154842
624.266835	42921.304353	32.159860
625.248673	43005.053039	32.164877
625.318443	43075.101916	32.169895
626.105013	43147.851946	32.174912
627.092632	43217.740035	32.179930
627.532594	43293.279061	32.184948
628.166643	43368.663145	32.189965
628.771456	43440.509810	32.194983
629.179015	43519.073546	32.200000
629.802893	43582.837882	32.205018
630.380382	43662.015054	32.210036
631.016784	43744.892775	32.215053
631.831867	43811.445827	32.220071
632.212458	43898.881667	32.225088
633.237677	43967.380223	32.230106
633.921547	44039.954953	32.235124
634.556042	44107.505118	32.240141
635.340442	44167.613794	32.245159
635.645709	44243.589408	32.250176
636.219831	44294.939654	32.255194
636.957582	44370.061169	32.260212
637.395370	44434.058112	32.265229
638.310573	44494.572463	32.270247
638.559948	44562.598459	32.275264
639.486742	44634.039627	32.280282
639.894408	44710.887463	32.285300
640.479335	44785.413879	32.290317
641.343400	44853.351863	32.295335
641.698692	44930.995504	32.300352
642.494451	44997.950663	32.305370
643.074938	45089.460723	32.310388
643.594882	45168.218009	32.315405
644.336724	45228.712881	32.320423
644.640562	45324.005359	32.325440
645.509349	45398.105158	32.330458
645.903473	45485.255620	32.335476
646.618113	45563.461325	32.340493
647.600708	45644.199732	32.345511
647.986246	45732.846363	32.350528
648.809243	45806.266950	32.355546
649.404083	45887.108437	32.360564
649.990321	45960.985619	32.365581
650.708480	46043.970456	32.370599
651.213144	46146.398897	32.375616
652.186583	46222.492985	32.380634
652.906405	46301.373500	32.385652
653.445377	46387.357855	32.390669
654.088900	46467.915875	32.395687
654.838888	46549.110305	32.400704
655.801262	46626.641525	32.405722
656.653165	46702.735543	32.410740
656.790255	46779.955496	32.415757
657.794113	46857.060791	32.420775
658.285745	46948.708220	32.425792
658.903132	47017.209535	32.430810
659.586020	47102.810154	32.435828
660.112465	47179.326246	32.440845
661.114248	47263.128464	32.445863
661.274096	47348.283012	32.450880
662.308653	47426.127669	32.455898
662.871922	47513.278407	32.460916
663.706687	47596.834973	32.465933
664.234715	47669.695744	32.470951
664.901766	47762.044418	32.475968
666.152297	47838.522321	32.480986
666.326859	47917.556585	32.486004
666.855604	48003.107792	32.491021
667.445893	48073.670164	32.496039
668.204563	48161.495797	32.501056
669.235227	48234.746135	32.506074
669.682659	48319.484770	32.511092
670.438381	48407.473087	32.516109
670.965100	48477.551629	32.521127
671.490111	48561.583697	32.526144
672.441930	48642.463095	32.531162
672.966880	48728.836152	32.536180
673.638813	48807.766541	32.541197
674.221172	48891.664236	32.546215
674.645749	48983.528324	32.551232
675.677257	49065.489090	32.556250
676.088605	49159.478582	32.561268
676.691551	49241.488887	32.566285
677.339034	49324.199641	32.571303
677.822004	49405.387215	32.576320
678.642963	49479.097058	32.581338
679.168526	49564.895788	32.586356
679.628056	49649.278230	32.591373
680.407836	49732.259424	32.596391
681.047771	49823.071724	32.601408
681.651930	49908.075691	32.606426
682.349648	50002.413565	32.611444
683.051841	50087.256815	32.616461
683.682208	50168.094734	32.621479
684.137708	50269.166796	32.626496
685.050555	50357.517056	32.631514
685.833836	50449.641479	32.636532
686.286709	50539.660559	32.641549
687.539923	50627.058720	32.646567
687.934789	50720.145714	32.651584
688.749243	50806.195911	32.656602
689.423611	50904.272331	32.661620
689.652667	50998.904218	32.666637
690.586787	51084.683166	32.671655
691.141906	51183.387179	32.676672
692.368860	51277.981694	32.681690
693.059088	51372.381177	32.686708
693.546202	51465.134296	32.691725
694.277347	51549.407434	32.696743
695.203581	51645.095855	32.701760
695.915126	51740.030578	32.706778
696.538052	51822.301211	32.711796
697.000799	51921.100056	32.716813
698.154083	52022.223748	32.721831
699.026068	52099.621421	32.726848
699.403758	52179.084897	32.731866
700.292844	52281.005431	32.736884
700.801956	52371.358519	32.741901
701.960669	52453.574771	32.746919
702.855034	52554.402898	32.751936
703.396056	52643.001952	32.756954
703.832619	52726.122213	32.761972
704.427770	52819.312459	32.766989
705.487926	52900.750852	32.772007
705.847409	53004.304317	32.777024
706.512058	53086.971399	32.782042
707.246205	53181.997839	32.787060
707.544570	53288.999872	32.792077
708.704899	53367.883814	32.797095
709.059098	53471.933423	32.802112
709.814351	53565.094409	32.807130
710.936960	53661.777423	32.812148
711.380672	53758.111993	32.817165
712.392669	53851.440363	32.822183
712.854633	53955.986475	32.827200
713.561860	54050.067520	32.832218
714.263837	54143.783425	32.837236
714.862319	54243.197022	32.842253
715.775198	54329.537092	32.847271
716.206481	54432.561776	32.852288
717.092136	54532.788621	32.857306
717.652240	54631.616595	32.862324
718.240058	54731.040729	32.867341
719.020366	54830.654668	32.872359
719.648241	54929.908896	32.877376
720.470734	55028.050961	32.882394
721.388585	55137.165707	32.887412
721.873433	55241.184072	32.892429
722.703494	55332.041058	32.897447
723.569003	55440.117239	32.902464
724.394736	55541.389044	32.907482
725.239886	55629.736379	32.912500
725.496113	55729.245647	32.917517
726.328843	55806.803409	32.922535
727.142850	55908.413920	32.927552
727.841510	55999.889666	32.932570
728.341166	56088.548945	32.937588
728.746097	56188.332895	32.942605
729.229404	56291.522917	32.947623
730.269768	56389.920024	32.952640
731.062630	56485.818326	32.957658
731.788268	56586.878207	32.962676
731.977652	56696.267346	32.967693
733.198423	56796.241656	32.972711
733.618343	56906.478483	32.977728
734.818367	57005.888553	32.982746
735.752285	57105.362094	32.987764
736.014045	57215.892193	32.992781
737.044409	57307.578151	32.997799
737.805065	57411.821309	33.002816
738.504577	57515.051395	33.007834
739.370698	57620.737955	33.012852
740.495535	57726.862549	33.017869
741.072119	57824.395526	33.022887
741.742057	57926.185474	33.027904
742.223037	58034.889100	33.032922
743.097852	58134.800929	33.037940
743.437329	58254.569326	33.042957
744.557364	58362.732966	33.047975
745.205060	58466.064982	33.052992
745.444323	58574.685111	33.058010
746.166876	58682.928858	33.063028
747.099096	58809.579427	33.068045
748.130324	58913.520184	33.073063
748.921083	59028.440797	33.078080
749.784923	59136.556169	33.083098
750.555910	59244.459964	33.088116
751.425626	59365.461770	33.093133
752.241408	59481.404639	33.098151
753.040737	59582.732827	33.103168
753.381828	59704.418174	33.108186
754.529513	59804.425849	33.113204
755.073035	59925.396473	33.118221
755.803604	60026.529690	33.123239
756.264718	60135.304774	33.128256
756.947319	60245.876651	33.133274
758.063652	60358.039597	33.138292
758.960149	60482.405978	33.143309
759.583095	60591.630750	33.148327
760.341036	60704.328907	33.153344
761.039276	60820.216693	33.158362
761.860638	60934.833338	33.163380
762.538971	61052.552325	33.168397
763.502131	61170.913807	33.173415
764.331574	61281.953689	33.178432
764.762617	61396.138165	33.183450
765.770253	61501.739402	33.188468
766.392318	61626.916614	33.193485
767.336097	61736.088115	33.198503
768.010468	61844.957124	33.203520
768.740454	61963.406002	33.208538
769.684222	62075.019098	33.213556
770.500713	62194.845563	33.218573
771.259785	62303.513371	33.223591
772.103813	62412.698651	33.228608
773.032407	62520.751730	33.233626
773.949987	62638.294869	33.238644
774.683016	62747.373867	33.243661
775.356889	62850.641616	33.248679
776.147395	62954.478443	33.253696
776.724306	63057.978182	33.258714
777.665598	63157.404297	33.263732
778.125482	63267.510989	33.268749
779.089066	63359.279544	33.273767
780.054218	63454.607057	33.278784
780.521459	63575.839403	33.283802
781.655464	63661.651840	33.288820
782.325517	63769.476089	33.293837
782.652917	63878.710329	33.298855
783.580675	63984.925396	33.303872
784.217717	64103.382971	33.308890
784.996051	64206.836176	33.313908
785.499879	64320.544382	33.318925
786.516402	64432.430011	33.323943
787.137654	64550.488174	33.328960
787.838541	64661.921526	33.333978
788.742278	64776.394198	33.338996
789.566637	64897.594155	33.344013
790.349397	65014.882290	33.349031
791.071685	65130.910433	33.354048
791.652168	65257.437728	33.359066
792.527356	65377.083248	33.364084
793.335494	65501.431299	33.369101
794.486075	65627.139534	33.374119
795.301252	65736.833869	33.379136
795.980392	65860.295043	33.384154
796.926927	65981.752924	33.389172
797.322154	66101.829679	33.394189
798.387623	66225.045767	33.399207
799.345175	66351.296036	33.404224
800.275350	66477.071114	33.409242
800.978277	66583.747531	33.414260
801.870489	66713.241375	33.419277
802.791257	66836.156230	33.424295
804.026795	66934.799363	33.429312
804.560188	67055.712211	33.434330
805.080751	67171.721787	33.439348
805.992884	67294.134960	33.444365
806.954708	67406.778921	33.449383
807.801494	67528.590995	33.454400
808.320066	67655.964883	33.459418
809.198975	67775.408481	33.464436
810.293163	67888.715944	33.469453
810.705406	68004.855491	33.474471
811.759334	68127.762163	33.479488
812.625024	68260.538645	33.484506
813.426075	68382.337904	33.489524
814.128791	68499.842065	33.494541
814.882689	68627.903654	33.499559
815.869943	68746.474914	33.504576
816.310789	68879.211719	33.509594
817.449793	69000.301054	33.514612
818.175766	69128.250139	33.519629
818.624067	69255.310129	33.524647
819.770635	69374.256877	33.529664
820.183878	69501.741445	33.534682
821.114162	69629.634452	33.539700
822.155116	69762.378665	33.544717
822.741438	69891.626352	33.549735
823.577728	70009.135706	33.554752
824.437720	70145.206567	33.559770
825.561615	70268.297386	33.564788
826.138195	70398.390726	33.569805
826.860528	70527.436377	33.574823
827.909810	70652.590481	33.579840
828.934419	70789.826985	33.584858
829.751843	70906.338960	33.589876
830.620538	71037.608267	33.594893
831.540741	71152.359311	33.599911
832.503450	71255.101960	33.604928
832.590802	71385.566737	33.609946
833.370958	71484.723618	33.614964
834.349994	71612.247279	33.619981
834.922656	71725.262951	33.624999
835.885022	71845.860060	33.630016
836.721743	71984.298793	33.635034
837.646065	72110.810005	33.640052
838.411318	72242.198596	33.645069
838.855699	72365.046996	33.650087
839.620423	72492.763061	33.655104
840.044766	72639.729163	33.660122
841.070156	72775.751314	33.665140
842.040398	72908.988243	33.670157
842.600107	73052.570396	33.675175
843.620670	73189.525561	33.680192
844.448309	73341.311864	33.685210
845.569346	73480.016658	33.690228
846.422151	73622.529580	33.695245
847.185393	73767.771331	33.700263
848.217718	73900.972432	33.705280
849.148256	74051.020126	33.710298
850.047322	74189.481541	33.715316
850.585256	74327.813825	33.720333
851.580742	74477.373044	33.725351
852.481322	74613.243872	33.730368
853.690721	74758.513267	33.735386
854.470433	74893.760721	33.740404
855.568817	75030.373007	33.745421
856.096506	75174.809210	33.750439
857.302713	75302.367472	33.755456
857.985328	75452.895818	33.760474
859.063603	75582.203500	33.765492
859.697779	75730.028434	33.770509
860.413975	75869.270660	33.775527
861.635186	76003.952242	33.780544
862.476825	76145.420784	33.785562
863.170414	76284.327815	33.790580
864.332203	76434.568544	33.795597
865.026828	76574.002190	33.800615
866.123646	76705.735851	33.805632
867.001798	76846.880249	33.810650
867.999683	76973.907014	33.815668
868.850905	77103.476178	33.820685
869.184703	77261.348432	33.825703
870.438490	77390.846365	33.830720
871.143210	77536.021370	33.835738
872.059884	77687.430672	33.840756
873.117297	77816.293065	33.845773
873.547383	77959.530073	33.850791
874.770199	78101.397106	33.855808
875.566770	78254.379843	33.860826
876.735548	78391.456600	33.865844
877.541789	78525.317506	33.870861
878.304225	78675.398995	33.875879
879.051913	78806.810598	33.880896
879.993798	78951.183817	33.885914
881.146616	79092.784038	33.890932
881.842247	79241.716418	33.895949
882.674757	79375.881677	33.900967
883.656760	79509.504290	33.905984
884.562189	79657.879676	33.911002
885.360101	79791.926610	33.916020
886.352232	79935.551361	33.921037
887.214974	80079.559004	33.926055
888.109488	80214.376889	33.931072
888.850942	80350.663236	33.936090
889.521703	80485.412193	33.941108
890.634259	80623.062180	33.946125
891.566514	80753.455043	33.951143
892.076429	80879.679924	33.956160
892.883499	81015.940430	33.961178
893.953156	81158.048117	33.966196
894.903486	81293.299687	33.971213
895.644166	81428.567750	33.976231
896.497904	81572.839394	33.981248
897.050154	81721.330945	33.986266
897.784010	81865.194059	33.991284
898.698033	82013.823801	33.996301
899.371609	82177.393382	34.001319
900.775848	82322.445454	34.006336
901.427045	82477.467275	34.011354
902.643595	82621.963900	34.016372
903.134216	82766.265144	34.021389
904.307729	82936.084202	34.026407
905.374658	83090.465665	34.031424
905.862897	83240.154412	34.036442
906.752823	83392.036413	34.041460
908.338161	83542.001227	34.046477
908.920041	83702.730693	34.051495
910.056806	83853.448699	34.056512
911.096021	84008.372353	34.061530
912.072687	84148.286778	34.066548
913.079692	84298.181302	34.071565
913.896440	84458.586119	34.076583
915.019646	84600.573345	34.081600
916.105855	84751.906640	34.086618
916.568061	84899.826112	34.091636
917.461585	85043.872446	34.096653
918.255203	85205.058170	34.101671
919.284522	85362.162785	34.106688
920.476464	85520.443788	34.111706
920.836843	85678.970946	34.116724
922.276487	85837.364993	34.121741
923.093816	85989.275963	34.126759
924.164151	86147.600300	34.131776
925.385996	86304.875562	34.136794
925.919154	86455.944337	34.141812
927.016210	86606.914504	34.146829
927.726411	86772.427703	34.151847
928.828720	86924.196344	34.156864
929.635550	87085.981301	34.161882
930.340661	87243.436875	34.166900
931.291198	87395.164036	34.171917
932.239084	87559.814482	34.176935
933.184789	87730.262968	34.181952
934.262267	87886.534845	34.186970
935.239744	88051.183812	34.191988
936.216458	88206.499921	34.197005
936.590680	88365.764259	34.202023
938.257196	88531.473342	34.207040
938.803639	88688.059798	34.212058
939.953508	88843.800746	34.217076
941.389858	89004.020168	34.222093
942.054999	89165.937658	34.227111
942.933461	89326.150240	34.232128
944.073282	89477.606250	34.237146
944.769488	89640.490085	34.242164
945.777092	89793.026830	34.247181
946.565717	89953.043288	34.252199
947.723671	90113.619954	34.257216
948.478951	90271.751759	34.262234
949.528216	90424.690669	34.267252
950.725652	90580.871735	34.272269
951.566138	90747.884612	34.277287
952.623353	90893.781129	34.282304
953.584232	91041.283030	34.287322
954.120897	91188.248395	34.292340
954.929176	91328.416646	34.297357
955.815267	91487.452498	34.302375
956.718039	91627.714452	34.307392
957.616896	91787.142564	34.312410
958.328480	91949.836915	34.317428
959.285424	92102.156122	34.322445
960.490425	92263.669693	34.327463
961.352059	92425.342385	34.332480
962.653313	92581.253349	34.337498
963.558993	92746.914723	34.342516
965.012430	92901.150592	34.347533
965.768832	93061.249875	34.352551
966.563993	93217.305553	34.357568
967.514909	93384.932255	34.362586
968.224478	93541.535835	34.367604
969.507586	93698.096214	34.372621
970.179467	93868.044703	34.377639
971.084492	94039.101499	34.382656
972.092449	94207.414323	34.387674
973.167540	94373.349838	34.392692
974.141525	94540.645123	34.397709
974.802005	94710.025284	34.402727
975.430027	94888.343550	34.407744
977.146345	95059.342895	34.412762
977.990177	95239.242155	34.417780
979.232171	95416.373929	34.422797
979.546975	95590.336958	34.427815
980.228351	95765.297729	34.432832
981.784006	95935.196575	34.437850
982.730250	96130.341210	34.442868
983.593549	96302.123190	34.447885
984.579476	96489.756311	34.452903
985.922061	96666.418227	34.457920
986.910085	96847.451062	34.462938
987.887613	97023.390884	34.467956
988.816079	97197.668787	34.472973
989.863218	97377.201662	34.477991
990.764896	97557.367614	34.483008
992.276845	97734.160982	34.488026
992.871625	97916.064209	34.493044
993.992598	98085.441768	34.498061
994.770547	98275.433349	34.503079
995.871107	98456.357859	34.508096
997.372523	98636.280407	34.513114
998.179166	98814.337525	34.518132
999.540081	98997.172784	34.523149
1000.084286	99170.920070	34.528167
1001.138816	99355.574929	34.533184
1002.250458	99534.536327	34.538202
1002.822316	99713.309662	34.543220
1004.171998	99887.732712	34.548237
1005.050828	100074.751723	34.553255
1006.374486	100248.459775	34.558272
1007.502131	100427.773009	34.563290
1008.229274	100611.946591	34.568308
1009.130854	100784.582084	34.573325
1010.424902	100962.795199	34.578343
1011.107288	101133.652144	34.583360
1012.292814	101319.306226	34.588378
1013.476143	101501.808862	34.593396
1014.800723	101668.301988	34.598413
1015.564881	101851.300625	34.603431
1016.690597	102033.886196	34.608448
1017.720430	102188.945619	34.613466
1018.480990	102372.689355	34.618484
1019.574907	102526.663790	34.623501
1020.527733	102689.045913	34.628519
1021.384180	102861.696414	34.633536
1022.492294	103019.774528	34.638554
1023.376557	103195.126399	34.643572
1024.464046	103362.024189	34.648589
1025.556938	103530.530509	34.653607
1026.208294	103697.350582	34.658624
1027.323412	103863.398496	34.663642
1028.178283	104048.765821	34.668660
1029.362870	104216.083595	34.673677
1030.403038	104402.056005	34.678695
1031.385006	104582.707499	34.683712
1032.521861	104757.584795	34.688730
1033.408261	104940.141600	34.693748
1034.545058	105113.286173	34.698765
1035.432109	105295.275401	34.703783
1036.155746	105489.717428	34.708800
1037.465678	105669.891519	34.713818
1038.688254	105859.567620	34.718836
1039.493037	106039.283131	34.723853
1040.241602	106232.561258	34.728871
1041.602827	106422.978388	34.733888
1042.712002	106626.040930	34.738906
1043.052834	106816.971557	34.743924
1044.518786	107007.882178	34.748941
1045.298358	107219.109894	34.753959
1046.554490	107410.982698	34.758976
1047.496562	107594.903782	34.763994
1048.477427	107817.109825	34.769012
1049.633696	108003.683541	34.774029
1050.936232	108203.027482	34.779047
1051.775541	108406.819444	34.784064
1053.126580	108611.871000	34.789082
1054.031063	108809.017897	34.794100
1055.384955	109012.666011	34.799117
1056.392177	109214.675604	34.804135
1057.134691	109416.540459	34.809152
1058.070760	109617.526114	34.814170
1059.177968	109821.360413	34.819188
1060.340321	110024.997109	34.824205
1061.505406	110240.390219	34.829223
1062.782833	110435.587128	34.834240
1063.968192	110636.336386	34.839258
1064.630175	110849.663979	34.844276
1066.227591	111047.472554	34.849293
1067.264668	111259.955914	34.854311
1068.406766	111456.677266	34.859328
1069.351688	111655.915561	34.864346
1070.646692	111865.979353	34.869364
1071.651431	112067.503661	34.874381
1072.772434	112264.715648	34.879399
1073.735840	112457.090419	34.884416
1075.107347	112648.689615	34.889434
1076.031375	112858.074816	34.894452
1077.026840	113051.727930	34.899469
1078.025227	113261.661292	34.904487
1079.542714	113463.909081	34.909504
1080.738657	113661.105901	34.914522
1081.492051	113861.531872	34.919540
1082.431987	114046.636776	34.924557
1083.542977	114258.586058	34.929575
1084.477651	114455.375563	34.934592
1085.936399	114650.128709	34.939610
1086.739955	114855.545219	34.944628
1088.089770	115047.785221	34.949645
1089.381052	115251.628964	34.954663
1090.376308	115440.686816	34.959680
1091.279340	115632.776600	34.964698
1091.953219	115821.307306	34.969716
1093.263460	116011.482518	34.974733
1094.290362	116199.007112	34.979751
1095.569442	116393.662575	34.984768
1096.878725	116580.040683	34.989786
1097.339251	116771.425745	34.994804
1098.691053	116964.653995	34.999821
1099.807541	117150.814286	35.004839
1100.509084	117351.172116	35.009856
1101.877601	117545.035042	35.014874
1102.610409	117751.877892	35.019892
1103.898862	117948.328941	35.024909
1105.091495	118153.337398	35.029927
1106.076055	118370.001069	35.034944
1107.742535	118567.116078	35.039962
1108.715359	118765.322791	35.044980
1109.535767	118967.636220	35.049997
1110.612583	119173.912831	35.055015
1111.454924	119393.243302	35.060032
1112.586449	119600.743026	35.065050
1113.781676	119822.311939	35.070068
1114.658787	120032.239063	35.075085
1115.880572	120247.939772	35.080103
1116.583850	120469.227420	35.085120
1117.908449	120685.408551	35.090138
1118.930897	120915.580597	35.095156
1119.934979	121137.723262	35.100173
1121.434903	121367.883260	35.105191
1122.234637	121596.741488	35.110208
1123.249630	121810.815049	35.115226
1124.708039	122055.459301	35.120244
1125.916014	122271.912083	35.125261
1127.358670	122499.378356	35.130279
1127.975310	122740.162773	35.135296
1129.673072	122955.741151	35.140314
1130.553784	123187.893200	35.145332
1131.710359	123416.414917	35.150349
1133.052314	123634.439562	35.155367
1133.596599	123873.103240	35.160384
1135.043474	124094.294897	35.165402
1136.080233	124341.017256	35.170420
1137.406608	124563.208135	35.175437
1138.666838	124794.549389	35.180455
1139.753846	125031.066647	35.185472
1141.106742	125249.722147	35.190490
1142.554373	125483.204914	35.195508
1143.768906	125708.971400	35.200525
1144.635076	125932.477750	35.205543
1145.950798	126169.244853	35.210560
1147.203981	126384.249386	35.215578
1148.206219	126615.114754	35.220596
1149.623196	126845.951314	35.225613
1150.890811	127075.736942	35.230631
1151.940076	127302.569112	35.235648
1153.359874	127507.756287	35.240666
1154.501372	127734.525674	35.245684
1155.486070	127956.569472	35.250701
1156.829128	128183.613019	35.255719
1157.634591	128399.136525	35.260736
1158.862219	128616.657818	35.265754
1159.787265	128847.261023	35.270772
1160.949890	129067.622825	35.275789
1161.808220	129291.534957	35.280807
1162.947520	129536.989026	35.285824
1164.524773	129765.526417	35.290842
1165.391097	129995.742126	35.295860
1166.554831	130218.748395	35.300877
1168.016828	130438.639312	35.305895
1168.751076	130655.888646	35.310912
1170.374874	130870.267016	35.315930
1171.365237	131077.640102	35.320948
1172.180965	131301.421378	35.325965
1173.434574	131519.744307	35.330983
1174.777935	131742.008997	35.336000
1175.995481	131952.392595	35.341018
1176.965726	132189.984831	35.346036
1178.104092	132417.054561	35.351053
1179.487689	132624.017699	35.356071
1180.068343	132857.660659	35.361088
1180.990505	133080.891619	35.366106
1182.410808	133327.329868	35.371124
1183.472140	133571.078346	35.376141
1184.433740	133799.695601	35.381159
1185.315214	134053.150302	35.386176
1186.822568	134301.102840	35.391194
1188.183419	134544.263941	35.396212
1189.173760	134792.724032	35.401229
1190.458050	135045.549325	35.406247
1191.383513	135299.209234	35.411264
1192.828930	135547.815326	35.416282
1194.123318	135805.221572	35.421300
1194.804034	136058.281175	35.426317
1196.385283	136312.842039	35.431335
1197.685507	136572.053602	35.436352
1198.504805	136821.178445	35.441370
1199.940679	137093.024871	35.446388
1201.099374	137342.325711	35.451405
1202.773563	137605.185675	35.456423
1203.554086	137868.550431	35.461440
1204.863516	138119.455029	35.466458
1206.385787	138388.635046	35.471476
1207.244982	138656.075637	35.476493
1208.694883	138904.477698	35.481511
1209.419008	139178.436570	35.486528
1211.230448	139435.341397	35.491546
1212.700983	139701.598708	35.496564
1213.944890	139958.690041	35.501581
1215.337255	140210.623418	35.506599
1216.195682	140478.674366	35.511616
1217.474521	140732.506964	35.516634
1218.695849	140987.099066	35.521652
1219.951910	141268.734261	35.526669
1221.067029	141521.280964	35.531687
1222.691598	141786.768102	35.536704
1223.800761	142045.723219	35.541722
1225.141175	142305.694525	35.546740
1225.777309	142576.448664	35.551757
1227.432946	142834.774022	35.556775
1228.816795	143107.120571	35.561792
1229.948866	143353.362603	35.566810
1231.142044	143615.599794	35.571828
1232.602761	143886.367194	35.576845
1233.655766	144145.169508	35.581863
1234.616163	144407.704658	35.586880
1235.396250	144673.467277	35.591898
1236.675043	144951.247660	35.596916
1238.147124	145226.487278	35.601933
1239.740587	145493.706749	35.606951
1240.600124	145767.225583	35.611968
1241.936968	146039.919361	35.616986
1243.664541	146307.186105	35.622004
1244.628799	146574.580989	35.627021
1245.947197	146837.455158	35.632039
1247.565380	147111.924052	35.637056
1248.612316	147358.334456	35.642074
1249.917602	147618.806762	35.647092
1251.106804	147873.516842	35.652109
1252.212749	148118.261179	35.657127
1253.297587	148359.662382	35.662144
1254.501998	148624.863788	35.667162
1255.973597	148873.167305	35.672180
1257.108115	149139.893220	35.677197
1258.705565	149389.828185	35.682215
1259.761119	149646.842837	35.687232
1260.811724	149902.452231	35.692250
1262.067663	150154.414669	35.697268
1263.261951	150430.893436	35.702285
1264.520497	150684.241493	35.707303
1265.371156	150960.616057	35.712320
1266.406652	151228.261047	35.717338
1267.905947	151501.133106	35.722356
1268.988005	151784.844732	35.727373
1270.430059	152061.192978	35.732391
1271.370839	152340.518050	35.737408
1272.409639	152624.915319	35.742426
1273.984609	152913.348468	35.747444
1275.119687	153194.956178	35.752461
1276.546270	153486.487760	35.757479
1277.920170	153776.977425	35.762496
1278.951610	154069.390511	35.767514
1280.303232	154361.702132	35.772532
1281.658066	154656.476273	35.777549
1283.047890	154945.969907	35.782567
1284.258185	155248.840020	35.787584
1285.741175	155537.789839	35.792602
1287.141282	155840.683864	35.797620
1288.258597	156141.901737	35.802637
1289.574754	156432.737716	35.807655
1290.913885	156724.371208	35.812672
1292.322347	157034.529057	35.817690
1293.464448	157320.833441	35.822708
1294.782649	157630.579497	35.827725
1296.447184	157925.719960	35.832743
1297.573487	158227.497507	35.837760
1298.744855	158525.438650	35.842778
1300.446260	158826.567408	35.847796
1301.546608	159127.873845	35.852813
1302.868390	159427.331750	35.857831
1304.523699	159729.768780	35.862848
1305.474650	160029.000566	35.867866
1307.075302	160316.683787	35.872884
1308.488543	160627.362966	35.877901
1309.808366	160922.137937	35.882919
1310.909435	161229.460446	35.887936
1312.068866	161533.210516	35.892954
1313.637442	161813.969574	35.897972
1314.859571	162128.611802	35.902989
1316.257243	162429.740779	35.908007
1317.467409	162724.140518	35.913024
1318.942420	163033.025666	35.918042
1320.857321	163329.178176	35.923060
1321.688700	163638.821145	35.928077
1323.308959	163933.795832	35.933095
1324.731324	164226.445313	35.938112
1325.676561	164515.394640	35.943130
1327.082458	164816.881617	35.948148
1328.377162	165111.017293	35.953165
1329.938063	165415.451810	35.958183
1331.296759	165716.445285	35.963200
1332.532244	166015.634068	35.968218
1333.802335	166305.315540	35.973236
1334.895096	166611.383699	35.978253
1336.349348	166905.720727	35.983271
1337.492694	167196.850098	35.988288
1338.719144	167479.719946	35.993306
1340.294278	167762.445136	35.998324
1341.461969	168054.426217	36.003341
1342.809464	168343.232607	36.008359
1344.055097	168632.628687	36.013376
1345.406324	168925.663642	36.018394
1346.634517	169215.282036	36.023412
1347.954521	169506.320989	36.028429
1349.278438	169809.733316	36.033447
1350.610197	170107.791388	36.038464
1351.806911	170412.751454	36.043482
1353.504554	170696.642064	36.048500
1354.567168	171001.057133	36.053517
1355.844729	171319.270570	36.058535
1356.940729	171625.206974	36.063552
1358.404240	171937.328112	36.068570
1359.973735	172243.355264	36.073588
1361.229596	172558.078224	36.078605
1362.456480	172871.716704	36.083623
1363.925589	173195.215671	36.088640
1365.487382	173519.919793	36.093658
1366.736201	173826.543127	36.098676
1368.042596	174147.296197	36.103693
1369.295582	174471.029838	36.108711
1370.834796	174793.385813	36.113728
1372.000832	175116.325918	36.118746
1373.785262	175444.546910	36.123764
1375.069753	175771.824748	36.128781
1376.408770	176084.183735	36.133799
1377.828547	176415.098515	36.138816
1379.281010	176748.434129	36.143834
1380.747543	177077.556127	36.148852
1382.234318	177412.121562	36.153869
1383.566262	177737.754615	36.158887
1384.609096	178056.190658	36.163904
1386.327336	178399.938481	36.168922
1387.389438	178723.376042	36.173940
1388.723546	179064.818475	36.178957
1390.252044	179392.688792	36.183975
1392.048788	179727.040550	36.188992
1393.068219	180070.546989	36.194010
1394.689347	180405.807902	36.199028
1395.958076	180748.630318	36.204045
1397.494083	181077.906182	36.209063
1398.855427	181425.502717	36.214080
1400.120994	181767.710368	36.219098
1401.856785	182091.387533	36.224116
1403.105173	182433.259605	36.229133
1404.460396	182775.585835	36.234151
1406.088264	183117.919961	36.239168
1407.329710	183451.358937	36.244186
1408.887303	183785.864698	36.249204
1410.393945	184138.747760	36.254221
1411.657673	184479.284750	36.259239
1413.308355	184816.205808	36.264256
1414.619696	185155.672877	36.269274
1415.963759	185494.501946	36.274292
1417.369011	185827.509371	36.279309
1418.826508	186176.046991	36.284327
1420.222924	186519.392492	36.289344
1421.589538	186874.347007	36.294362
1423.360973	187206.654680	36.299380
1424.479117	187558.316059	36.304397
1425.809834	187898.380330	36.309415
1427.351928	188231.442690	36.314432
1428.783683	188580.633931	36.319450
1430.247340	188915.160291	36.324468
1431.516958	189242.396083	36.329485
1432.839864	189566.019722	36.334503
1434.444960	189889.052648	36.339520
1435.572202	190219.998732	36.344538
1436.931925	190548.445510	36.349556
1438.701040	190880.279352	36.354573
1440.207410	191212.285385	36.359591
1441.677699	191541.531762	36.364608
1442.892908	191868.587797	36.369626
1444.183290	192203.542024	36.374644
1445.756892	192542.247045	36.379661
1446.794109	192877.665700	36.384679
1448.259790	193222.244643	36.389696
1449.561847	193576.780084	36.394714
1450.937130	193920.743056	36.399732
1452.443648	194261.817097	36.404749
1454.095056	194613.291868	36.409767
1455.436330	194974.315956	36.414784
1457.278764	195330.295350	36.419802
1458.563499	195680.249628	36.424820
1459.971526	196034.730436	36.429837
1461.488312	196397.269630	36.434855
1462.912083	196742.217243	36.439872
1464.061488	197112.654337	36.444890
1465.592965	197480.668938	36.449908
1467.390925	197839.056114	36.454925
1468.719988	198204.708611	36.459943
1469.640577	198567.167693	36.464960
1471.219332	198947.688111	36.469978
1472.551209	199318.145265	36.474996
1474.079976	199711.806048	36.480013
1475.464026	200091.082633	36.485031
1477.294279	200474.248832	36.490048
1478.468957	200860.394848	36.495066
1480.045841	201252.634340	36.500084
1481.447991	201628.348478	36.505101
1482.971635	202020.194691	36.510119
1484.877951	202406.418626	36.515136
1486.176778	202793.862311	36.520154
1487.712151	203186.880986	36.525172
1488.944617	203563.433072	36.530189
1490.597905	203963.965687	36.535207
1491.893431	204356.496912	36.540224
1493.236030	204747.384474	36.545242
1494.871845	205149.335668	36.550260
1496.553219	205536.019315	36.555277
1497.669811	205938.492144	36.560295
1499.630666	206333.970963	36.565312
1501.128414	206734.581899	36.570330
1502.852737	207137.976292	36.575348
1504.549973	207525.111579	36.580365
1505.710186	207932.387087	36.585383
1507.671081	208316.193931	36.590400
1508.991052	208723.510514	36.595418
1510.398011	209101.292243	36.600436
1512.421878	209510.375707	36.605453
1513.833086	209899.994832	36.610471
1515.489893	210288.660930	36.615488
1516.726152	210682.934667	36.620506
1518.225811	211069.497027	36.625524
1520.011376	211464.521685	36.630541
1521.199581	211868.637211	36.635559
1523.023608	212260.433769	36.640576
1524.470030	212646.630982	36.645594
1525.774013	213046.491523	36.650612
1527.457593	213439.586328	36.655629
1528.466566	213852.146881	36.660647
1530.354246	214227.458809	36.665664
1531.778458	214615.649081	36.670682
1533.466073	214990.514614	36.675700
1535.179168	215370.152170	36.680717
1536.280653	215740.495185	36.685735
1537.927407	216117.352954	36.690752
1539.353038	216496.737719	36.695770
1540.753457	216886.566672	36.700788
1542.505324	217268.567322	36.705805
1543.931512	217649.454944	36.710823
1545.584586	218035.767148	36.715840
1547.120848	218433.300783	36.720858
1548.470321	218819.056578	36.725876
1550.186817	219214.887182	36.730893
1551.549403	219612.022299	36.735911
1553.174929	219999.438581	36.740928
1554.430968	220405.509231	36.745946
1555.782743	220808.771729	36.750964
1557.941332	221211.369057	36.755981
1559.108581	221626.627990	36.760999
1560.521077	222022.900194	36.766016
1562.115390	222450.410239	36.771034
1563.648856	222858.425258	36.776052
1565.275049	223304.703365	36.781069
1566.285935	223775.493806	36.786087
1568.222900	224193.403486	36.791104
1569.659931	224627.170461	36.796122
1571.320822	225052.113680	36.801140
1572.745552	225481.694780	36.806157
1574.398426	225911.138084	36.811175
1576.158716	226329.643085	36.816192
1577.550824	226772.899252	36.821210
1578.968994	227207.795961	36.826228
1580.607775	227644.461101	36.831245
1582.135676	228090.772761	36.836263
1584.005051	228526.767693	36.841280
1585.490915	228970.955568	36.846298
1587.084649	229412.256777	36.851316
1588.507005	229847.974126	36.856333
1590.325861	230303.058935	36.861351
1592.011039	230740.793046	36.866368
1593.652406	231188.518285	36.871386
1595.348381	231628.691734	36.876404
1597.257234	232072.336650	36.881421
1598.674068	232516.165730	36.886439
1600.603111	232958.006355	36.891456
1602.021021	233403.057009	36.896474
1603.513329	233854.980375	36.901492
1605.522646	234298.716496	36.906509
1606.700347	234744.572491	36.911527
1608.406033	235189.885194	36.916544
1610.015616	235647.560122	36.921562
1611.773429	236095.762292	36.926580
1613.511541	236536.399087	36.931597
1614.978637	236985.769137	36.936615
1616.352688	237434.927008	36.941632
1618.011791	237880.380948	36.946650
1619.656555	238330.766257	36.951668
1621.529107	238784.544225	36.956685
1623.162059	239247.075707	36.961703
1624.506184	239682.831193	36.966720
1626.171574	240138.678469	36.971738
1627.617898	240600.811839	36.976756
1629.908677	241055.439966	36.981773
1631.263961	241505.168442	36.986791
1632.735901	241958.866676	36.991808
1634.337513	242415.821249	36.996826
1636.384136	242868.968962	37.001844
1638.177551	243303.640811	37.006861
1639.571314	243742.951858	37.011879
1640.906263	244172.874337	37.016896
1642.954228	244603.467167	37.021914
1644.392870	245032.230679	37.026932
1646.142324	245455.507264	37.031949
1647.443654	245895.471886	37.036967
1649.221494	246325.121050	37.041984
1651.007778	246774.278779	37.047002
1652.456671	247214.271570	37.052020
1654.077674	247637.318114	37.057037
1655.492223	248089.104591	37.062055
1657.128496	248526.603886	37.067072
1658.777258	248981.883704	37.072090
1660.031772	249439.134361	37.077108
1661.957158	249886.850128	37.082125
1663.503719	250350.175592	37.087143
1665.193657	250818.278995	37.092160
1666.652973	251274.125790	37.097178
1668.419366	251742.217361	37.102196
1670.227099	252207.990781	37.107213
1671.876355	252684.282238	37.112231
1673.539998	253160.470034	37.117248
1675.173583	253630.083659	37.122266
1676.741313	254101.080205	37.127284
1678.483064	254571.946635	37.132301
1680.008075	255060.224920	37.137319
1681.791988	255544.446926	37.142336
1683.470876	256025.638061	37.147354
1684.937906	256515.857101	37.152372
1686.916350	257006.550659	37.157389
1688.372403	257498.168908	37.162407
1690.153585	257982.976237	37.167424
1692.010081	258472.724805	37.172442
1693.322566	258974.782228	37.177460
1695.202032	259456.423332	37.182477
1696.855279	259966.629658	37.187495
1698.764033	260465.031966	37.192512
1700.537774	260956.394347	37.197530
1702.079845	261467.812638	37.202548
1703.847493	261969.311613	37.207565
1705.553251	262474.427865	37.212583
1707.505998	262980.951062	37.217600
1709.129587	263484.479964	37.222618
1710.810780	263995.518399	37.227636
1712.608869	264494.318242	37.232653
1714.682068	265000.007352	37.237671
1716.168396	265517.757881	37.242688
1717.768300	266016.106605	37.247706
1719.490369	266528.838263	37.252724
1721.353833	267038.269056	37.257741
1723.223345	267548.282584	37.262759
1724.897816	268053.018524	37.267776
1726.412898	268557.373751	37.272794
1728.566243	269073.968776	37.277812
1730.584954	269592.363558	37.282829
1732.139158	270088.276570	37.287847
1733.393524	270599.124486	37.292864
1735.286689	271100.670306	37.297882
1737.129810	271618.201967	37.302900
1739.099946	272122.197541	37.307917
1740.929428	272641.584132	37.312935
1742.604415	273142.883226	37.317952
1744.226809	273655.926113	37.322970
1746.073973	274164.663275	37.327988
1747.906307	274668.194387	37.333005
1749.683788	275178.414405	37.338023
1751.299694	275691.733741	37.343040
1752.932609	276185.235339	37.348058
1754.724186	276677.083936	37.353076
1756.567028	277164.655420	37.358093
1758.002850	277653.182123	37.363111
1759.651704	278142.282178	37.368128
1761.428575	278621.199122	37.373146
1762.990369	279128.600696	37.378164
1765.045762	279621.541962	37.383181
1766.399613	280129.280119	37.388199
1768.203178	280633.259382	37.393216
1770.250238	281129.982969	37.398234
1771.511812	281651.372921	37.403252
1773.464654	282148.642678	37.408269
1775.011154	282658.450258	37.413287
1776.613640	283182.090836	37.418304
1778.250972	283704.580948	37.423322
1779.735361	284237.509156	37.428340
1781.943106	284762.111535	37.433357
1784.009431	285291.917329	37.438375
1785.311863	285820.297987	37.443392
1787.234300	286359.090363	37.448410
1789.000541	286905.450602	37.453428
1790.744989	287428.494513	37.458445
1792.190564	287980.948970	37.463463
1793.718233	288521.347827	37.468480
1795.907189	289081.498455	37.473498
1797.505766	289639.813819	37.478516
1799.699557	290191.322860	37.483533
1801.415800	290750.350642	37.488551
1803.191030	291302.228827	37.493568
1805.077888	291857.972316	37.498586
1807.347008	292427.416820	37.503604
1809.203055	292974.803782	37.508621
1811.052794	293546.115599	37.513639
1812.649100	294102.963429	37.518656
1814.986510	294649.958255	37.523674
1816.314773	295215.531469	37.528692
1818.220267	295780.244516	37.533709
1820.357253	296342.833722	37.538727
1822.189090	296902.803527	37.543744
1824.132424	297460.008928	37.548762
1825.750612	298030.040499	37.553780
1827.472579	298592.838669	37.558797
1829.510960	299168.382167	37.563815
1831.276245	299733.579675	37.568832
1833.367514	300290.465814	37.573850
1834.791318	300876.158468	37.578868
1836.616349	301439.456827	37.583885
1838.649716	302011.530364	37.588903
1840.573745	302586.589959	37.593920
1842.348547	303162.711916	37.598938
1844.394638	303739.826724	37.603956
1846.160904	304314.088825	37.608973
1848.177246	304883.480572	37.613991
1849.920271	305455.707392	37.619008
1851.943234	306022.855755	37.624026
1854.037854	306609.670554	37.629044
1855.769806	307182.268663	37.634061
1857.700421	307749.954072	37.639079
1859.771241	308319.110788	37.644096
1861.592218	308884.089174	37.649114
1863.151188	309460.483970	37.654132
1865.282558	310032.285175	37.659149
1866.780251	310603.145712	37.664167
1868.575123	311178.600253	37.669184
1870.918820	311757.362763	37.674202
1872.659917	312328.145025	37.679220
1874.192057	312890.450469	37.684237
1875.913022	313468.261619	37.689255
1877.497804	314025.496442	37.694272
1880.069773	314580.532547	37.699290
1881.400106	315138.613515	37.704308
1883.467485	315678.234593	37.709325
1885.129094	316250.167678	37.714343
1886.627642	316810.340826	37.719360
1888.865458	317367.238746	37.724378
1890.614853	317946.507338	37.729396
1892.292144	318513.290026	37.734413
1894.020115	319087.753382	37.739431
1895.932192	319667.335961	37.744448
1897.785116	320241.667244	37.749466
1899.544047	320832.361037	37.754484
1901.605887	321420.485779	37.759501
1903.804942	322011.654823	37.764519
1905.575078	322604.691991	37.769536
1907.442572	323194.660727	37.774554
1909.208355	323788.804722	37.779572
1910.989274	324380.096915	37.784589
1913.058010	324983.091331	37.789607
1915.066538	325589.364998	37.794624
1917.108183	326195.474827	37.799642
1918.663878	326811.281178	37.804660
1920.750077	327411.151122	37.809677
1922.913632	328016.587652	37.814695
1924.632814	328628.996870	37.819712
1926.343150	329254.120389	37.824730
1928.316911	329867.490005	37.829748
1930.366428	330490.183039	37.834765
1932.273996	331117.386169	37.839783
1934.114402	331743.222514	37.844800
1936.086081	332371.543413	37.849818
1937.782180	333011.783362	37.854836
1939.911057	333631.635743	37.859853
1942.256974	334270.052790	37.864871
1943.812554	334908.745082	37.869888
1946.345878	335544.095191	37.874906
1948.465995	336175.292069	37.879924
1950.098146	336806.714244	37.884941
1952.010371	337448.286885	37.889959
1953.877608	338090.341286	37.894976
1956.268371	338712.984492	37.899994
1957.944778	339362.745565	37.905012
1959.663160	340012.719791	37.910029
1962.048146	340647.625309	37.915047
1964.066723	341296.391040	37.920064
1965.930399	341929.386392	37.925082
1967.969995	342576.938799	37.930100
1969.919215	343228.989932	37.935117
1972.153979	343868.650082	37.940135
1974.041804	344512.318290	37.945152
1975.777078	345151.079235	37.950170
1977.858255	345809.012182	37.955188
1979.843288	346454.921960	37.960205
1982.103534	347098.797749	37.965223
1983.963912	347758.820578	37.970240
1985.823734	348401.855946	37.975258
1987.751530	349055.961104	37.980276
1990.111163	349714.883322	37.985293
1992.230800	350351.452847	37.990311
1994.010603	351005.198661	37.995328
1995.883128	351652.169363	38.000346
1997.878283	352309.438291	38.005364
1999.731407	352964.589184	38.010381
2001.923443	353619.978686	38.015399
2003.623586	354273.257149	38.020416
2005.767586	354912.191875	38.025434
2007.847760	355577.592628	38.030452
2009.273923	356216.042508	38.035469
2011.813022	356841.764481	38.040487
2013.537462	357475.223377	38.045504
2015.653793	358106.857134	38.050522
2017.592112	358749.826494	38.055540
2019.220109	359386.113423	38.060557
2021.207172	360022.787741	38.065575
2023.298158	360688.332252	38.070592
2025.136776	361330.642612	38.075610
2027.092123	361987.181267	38.080628
2028.992176	362639.887296	38.085645
2031.169273	363300.426527	38.090663
2032.968095	363968.500777	38.095680
2034.891201	364625.482373	38.100698
2036.798325	365301.557392	38.105716
2038.510644	365984.019820	38.110733
2040.613224	366654.711366	38.115751
2042.978295	367347.416509	38.120768
2044.948023	368035.379923	38.125786
2046.482297	368728.577082	38.130804
2048.697346	369429.664227	38.135821
2051.024425	370135.919238	38.140839
2052.421641	370842.187275	38.145856
2054.656950	371543.331935	38.150874
2056.832448	372267.426444	38.155892
2058.631104	372993.318544	38.160909
2060.928471	373697.479657	38.165927
2062.977000	374417.290557	38.170944
2064.949611	375142.704037	38.175962
2066.844574	375870.524518	38.180980
2069.005784	376599.553783	38.185997
2071.378821	377331.930832	38.191015
2073.543274	378066.659684	38.196032
2075.662011	378812.740770	38.201050
2077.699583	379550.247883	38.206068
2079.263970	380293.420889	38.211085
2081.844926	381029.994328	38.216103
2084.148315	381776.131150	38.221120
2086.264634	382518.884359	38.226138
2088.549526	383263.697395	38.231156
2090.688962	384014.577134	38.236173
2092.348836	384744.551083	38.241191
2094.271149	385499.488794	38.246208
2096.704536	386259.039938	38.251226
2099.385638	387004.132152	38.256244
2101.219606	387756.216905	38.261261
2103.374454	388504.909773	38.266279
2105.740914	389257.833981	38.271296
2107.856047	390006.979028	38.276314
2110.166262	390757.949555	38.281332
2111.708740	391514.706508	38.286349
2114.035021	392255.092831	38.291367
2116.518863	393012.341623	38.296384
2118.517985	393766.888705	38.301402
2120.702677	394512.895381	38.306420
2122.841036	395266.165158	38.311437
2125.518584	396013.827090	38.316455
2127.548909	396768.647899	38.321472
2129.328970	397516.394545	38.326490
2131.658865	398259.951163	38.331508
2133.881342	399021.828725	38.336525
2136.127569	399766.196835	38.341543
2138.066333	400510.824511	38.346560
2140.370696	401256.234032	38.351578
2142.676512	402005.804781	38.356596
2144.551679	402757.529886	38.361613
2147.018628	403490.868600	38.366631
2149.139039	404223.789259	38.371648
2150.994179	404955.442277	38.376666
2152.985367	405673.828181	38.381684
2154.853304	406393.127811	38.386701
2157.201281	407107.414455	38.391719
2159.029181	407828.583121	38.396736
2161.504264	408560.924496	38.401754
2163.197722	409286.915263	38.406772
2165.311615	410027.788233	38.411789
2167.375070	410751.423829	38.416807
2168.958248	411509.796551	38.421824
2171.092495	412258.760623	38.426842
2173.053272	413014.748241	38.431860
2175.176383	413778.995013	38.436877
2177.584317	414542.134008	38.441895
2179.429496	415319.273264	38.446912
2181.638113	416085.666936	38.451930
2184.131117	416864.400271	38.456948
2185.824667	417651.016534	38.461965
2188.442483	418432.745771	38.466983
2190.560576	419227.296179	38.472000
2192.517440	420021.037893	38.477018
2194.675883	420813.708409	38.482036
2196.607862	421612.290863	38.487053
2198.996539	422427.204804	38.492071
2201.150059	423231.952538	38.497088
2203.555076	424041.392264	38.502106
2206.143811	424855.129492	38.507124
2208.005785	425679.086059	38.512141
2210.267399	426485.632887	38.517159
2212.427580	427314.446408	38.522176
2214.808966	428133.271830	38.527194
2216.950643	428948.868717	38.532212
2218.744701	429781.757824	38.537229
2220.941424	430615.563620	38.542247
2223.350934	431454.417449	38.547264
2225.778237	432306.146069	38.552282
2228.146898	433133.810292	38.557300
2230.341081	433977.215057	38.562317
2233.047192	434810.989268	38.567335
2235.004162	435656.295022	38.572352
2237.464216	436498.753605	38.577370
2240.080655	437337.359632	38.582388
2241.805978	438191.516407	38.587405
2244.148754	439027.422791	38.592423
2246.562853	439876.898159	38.597440
2249.069177	440725.415194	38.602458
2251.311134	441564.987624	38.607476
2253.552236	442413.028469	38.612493
2256.137328	443252.834232	38.617511
2258.176097	444107.268513	38.622528
2260.459586	444952.876845	38.627546
2263.157026	445791.706285	38.632564
2264.781426	446638.268190	38.637581
2267.348462	447477.003003	38.642599
2269.591755	448331.388307	38.647616
2272.015405	449181.612609	38.652634
2274.232592	450028.549338	38.657652
2276.149248	450877.271876	38.662669
2278.707668	451728.686404	38.667687
2280.794083	452581.206211	38.672704
2283.049879	453439.579880	38.677722
2285.861358	454286.650835	38.682740
2287.734246	455156.697670	38.687757
2290.049349	456010.707180	38.692775
2292.131513	456866.489159	38.697792
2294.560419	457718.638827	38.702810
2296.976665	458577.023898	38.707828
2299.191093	459423.575906	38.712845
2301.712786	460260.032083	38.717863
2304.091453	461083.384241	38.722880
2306.249958	461907.395879	38.727898
2308.842911	462731.352188	38.732916
2310.827965	463552.493448	38.737933
2313.369642	464373.660257	38.742951
2315.458568	465197.242809	38.747968
2317.935302	466025.325636	38.752986
2320.080188	466853.680668	38.758004
2322.090219	467689.097304	38.763021
2324.198436	468532.445596	38.768039
2327.039748	469369.168136	38.773056
2328.884545	470215.972421	38.778074
2331.270353	471064.064525	38.783092
2333.381221	471918.277372	38.788109
2336.001731	472781.309654	38.793127
2338.775290	473640.286191	38.798144
2340.324807	474510.791425	38.803162
2343.014552	475376.875323	38.808180
2345.481082	476253.108448	38.813197
2347.579878	477125.017058	38.818215
2350.352194	477985.207377	38.823232
2352.539530	478868.281718	38.828250
2354.883001	479739.066323	38.833268
2357.710685	480627.151585	38.838285
2359.752118	481506.536724	38.843303
2362.259606	482381.964626	38.848320
2364.342238	483273.223940	38.853338
2367.023151	484155.807571	38.858356
2369.179633	485049.036297	38.863373
2371.573807	485934.406396	38.868391
2374.337807	486842.286930	38.873408
2375.964619	487752.882802	38.878426
2378.745567	488648.501975	38.883444
2380.891453	489560.533561	38.888461
2383.256209	490457.491407	38.893479
2385.700787	491383.409059	38.898496
2388.137898	492299.841266	38.903514
2390.460108	493208.724663	38.908532
2392.465118	494122.708717	38.913549
2395.358740	495049.464839	38.918567
2397.948371	495977.179261	38.923584
2400.199683	496897.482247	38.928602
2402.238124	497824.177227	38.933620
2404.701411	498760.840311	38.938637
2407.679134	499691.514631	38.943655
2409.987066	500628.098641	38.948672
2412.213298	501553.244319	38.953690
2415.146446	502490.225180	38.958708
2417.282323	503420.677658	38.963725
2419.873343	504355.238354	38.968743
2422.555016	505286.049514	38.973760
2424.487769	506228.931848	38.978778
2427.339982	507154.313356	38.983796
2429.383401	508109.622630	38.988813
2431.968517	509050.115113	38.993831
2434.470779	509989.003308	38.998848
2436.456030	510930.341217	39.003866
2439.290547	511879.548229	39.008884
2441.597308	512827.726976	39.013901
2443.539248	513775.304149	39.018919
2446.030028	514722.078499	39.023936
2448.746470	515680.550495	39.028954
2450.941906	516630.785500	39.033972
2452.944299	517592.230661	39.038989
2455.784331	518557.609427	39.044007
2458.321898	519524.690609	39.049024
2460.374540	520478.994896	39.054042
2462.711761	521423.571119	39.059060
2464.966900	522352.386355	39.064077
2467.431180	523292.543992	39.069095
2470.145525	524236.127551	39.074112
2471.911232	525177.038630	39.079130
2474.423320	526115.400757	39.084148
2476.929085	527072.487908	39.089165
2479.332733	528027.163893	39.094183
2481.802937	528992.139557	39.099200
2484.232647	529968.840006	39.104218
2486.643956	530932.691702	39.109236
2489.243665	531902.288472	39.114253
2491.533740	532882.392365	39.119271
2494.151574	533857.393362	39.124288
2496.307612	534857.267841	39.129306
2499.042949	535841.577948	39.134324
2501.285183	536839.237669	39.139341
2503.533592	537840.399737	39.144359
2506.089737	538848.535479	39.149376
2508.373015	539871.336004	39.154394
2511.338903	540884.542641	39.159412
2513.550912	541906.654697	39.164429
2516.270586	542936.657041	39.169447
2518.694142	543959.691678	39.174464
2521.368268	545003.331088	39.179482
2524.141555	546032.694297	39.184500
2526.464158	547065.273845	39.189517
2528.897569	548106.406579	39.194535
2531.780126	549152.514959	39.199552
2534.023204	550208.150999	39.204570
2537.152579	551245.713282	39.209588
2539.896754	552306.282283	39.214605
2541.960780	553354.365176	39.219623
2544.578549	554405.291043	39.224640
2547.041153	555466.412554	39.229658
2550.003564	556524.352671	39.234676
2552.279742	557591.115516	39.239693
2554.943399	558655.468097	39.244711
2557.412069	559719.064145	39.249728
2559.924295	560806.328552	39.254746
2561.923288	561870.883611	39.259764
2564.651353	562952.510031	39.264781
2567.140720	564045.486840	39.269799
2569.810198	565125.988558	39.274816
2572.219076	566222.009646	39.279834
2574.744913	567315.056581	39.284852
2576.958737	568423.575712	39.289869
2579.110037	569533.415039	39.294887
2582.190331	570638.487079	39.299904
2584.719485	571766.692787	39.304922
2586.963553	572887.367224	39.309940
2589.320706	574008.676406	39.314957
2591.640880	575147.203548	39.319975
2594.333874	576283.006982	39.324992
2596.575898	577435.588412	39.330010
2599.388674	578572.367681	39.335028
2602.046967	579719.050155	39.340045
2604.433934	580877.006152	39.345063
2607.048216	582032.859836	39.350080
2609.046277	583200.590863	39.355098
2611.722699	584352.554544	39.360116
2614.691392	585536.749223	39.365133
2616.985066	586717.681002	39.370151
2619.945790	587880.441887	39.375168
2622.231967	589069.816388	39.380186
2624.732996	590242.298377	39.385204
2627.687840	591418.799786	39.390221
2629.959046	592605.168666	39.395239
2632.999126	593751.911739	39.400256
2635.590533	594915.850873	39.405274
2638.174886	596061.392320	39.410292
2640.691038	597201.924485	39.415309
2643.196975	598359.475162	39.420327
2646.151431	599520.241974	39.425344
2648.586980	600669.862062	39.430362
2650.882396	601823.596528	39.435380
2653.732854	602987.586858	39.440397
2656.194072	604153.024966	39.445415
2658.655810	605328.454673	39.450432
2660.940871	606507.595752	39.455450
2663.694654	607688.588686	39.460468
2666.400417	608896.235646	39.465485
2668.848573	610081.881988	39.470503
2671.657603	611287.904131	39.475520
2674.020985	612504.574018	39.480538
2677.007199	613716.957096	39.485556
2679.649710	614948.768034	39.490573
2682.345633	616170.432192	39.495591
2685.035078	617400.061639	39.500608
2687.840859	618628.134349	39.505626
2690.299702	619879.520209	39.510644
2693.217981	621113.093220	39.515661
2695.589220	622366.706369	39.520679
2698.426445	623608.654321	39.525696
2700.916608	624878.446106	39.530714
2703.495011	626141.428753	39.535732
2706.473512	627397.602613	39.540749
2708.843447	628686.543240	39.545767
2711.998185	629956.919952	39.550784
2714.842639	631241.226641	39.555802
2717.778194	632521.717032	39.560820
2720.377578	633797.763481	39.565837
2723.067656	635084.870290	39.570855
2726.358793	636371.818808	39.575872
2728.950704	637658.024444	39.580890
2731.651857	638941.307800	39.585908
2734.374237	640230.314964	39.590925
2737.273956	641521.575399	39.595943
2740.560447	642805.127339	39.600960
2742.958370	644091.207634	39.605978
2745.355907	645383.308472	39.610996
2748.633268	646677.791631	39.616013
2751.384720	647980.620403	39.621031
2754.295140	649267.502592	39.626048
2756.916886	650567.873200	39.631066
2759.320976	651867.860994	39.636084
2762.468427	653169.648875	39.641101
2765.019803	654476.844108	39.646119
2767.547065	655779.137843	39.651136
2770.535803	657102.251278	39.656154
2773.248969	658406.954770	39.661172
2776.494462	659711.794411	39.666189
2779.071143	661033.048680	39.671207
2782.017163	662337.783840	39.676224
2784.510480	663653.317691	39.681242
2787.286996	664961.508379	39.686260
2790.592855	666277.195775	39.691277
2792.902302	667601.473492	39.696295
2795.724614	668912.299789	39.701312
2798.716224	670226.647449	39.706330
2801.187278	671553.281454	39.711348
2804.476511	672875.764882	39.716365
2807.224615	674202.426928	39.721383
2809.806312	675515.208031	39.726400
2812.535647	676844.380991	39.731418
2815.781159	678150.666585	39.736436
2818.577811	679432.096258	39.741453
2821.127284	680724.318941	39.746471
2823.703629	682005.774576	39.751488
2826.273868	683273.691010	39.756506
2828.917768	684569.329411	39.761524
2831.757751	685857.650374	39.766541
2834.314028	687162.417558	39.771559
2837.245136	688459.587802	39.776576
2839.611482	689766.839302	39.781594
2842.310035	691082.232582	39.786612
2845.433385	692409.469508	39.791629
2847.773289	693743.583710	39.796647
2850.767043	695064.840053	39.801664
2853.134144	696410.999348	39.806682
2855.981095	697762.229887	39.811700
2859.224662	699115.319499	39.816717
2861.910581	700484.651516	39.821735
2864.702229	701840.467875	39.826752
2867.328289	703217.261728	39.831770
2870.014499	704591.647027	39.836788
2873.080393	705973.628514	39.841805
2876.205682	707370.932320	39.846823
2878.763894	708760.029506	39.851840
2881.718183	710155.124726	39.856858
2884.418084	711567.411647	39.861876
2887.457044	712982.180071	39.866893
2890.079325	714402.373587	39.871911
2892.785909	715824.491558	39.876928
2895.495869	717246.467449	39.881946
2898.115121	718705.318044	39.886964
2901.616382	720142.550315	39.891981
2904.144225	721591.068492	39.896999
2906.856366	723047.510643	39.902016
2910.359462	724508.014663	39.907034
2913.312472	725973.688109	39.912052
2916.419478	727431.859623	39.917069
2919.214026	728913.290782	39.922087
2922.093007	730379.273493	39.927104
2924.997736	731846.468867	39.932122
2928.066334	733316.877061	39.937140
2931.283038	734797.508570	39.942157
2934.220147	736288.920857	39.947175
2936.788675	737762.052980	39.952192
2939.968998	739257.904822	39.957210
2942.736483	740740.321638	39.962228
2946.097354	742219.157015	39.967245
2948.969435	743720.037101	39.972263
2952.080301	745215.907285	39.977280
2955.216570	746693.395838	39.982298
2957.921265	748189.503723	39.987316
2961.147461	749677.008601	39.992333
2963.944233	751177.256476	39.997351
2966.866386	752681.428662	40.002368
2969.784380	754184.224232	40.007386
2972.573638	755687.583784	40.012404
2975.794754	757189.591994	40.017421
2978.656796	758703.766746	40.022439
2981.178359	760214.251006	40.027456
2984.307052	761729.302924	40.032474
2987.028236	763248.643133	40.037492
2990.061740	764767.477149	40.042509
2992.987344	766299.641076	40.047527
2996.162999	767830.957612	40.052544
2998.893848	769358.689941	40.057562
3001.877045	770897.859308	40.062580
3004.879745	772423.685330	40.067597
3007.769362	773964.342418	40.072615
3010.568667	775492.953694	40.077632
3013.765402	776992.113214	40.082650
3016.353234	778501.765915	40.087668
3019.359842	779992.533013	40.092685
3022.400197	781505.411687	40.097703
3025.323444	783013.527958	40.102720
3028.435665	784515.754189	40.107738
3030.994027	786027.858378	40.112756
3034.131903	787544.106285	40.117773
3036.921064	789066.362648	40.122791
3039.961729	790599.326114	40.127808
3043.260605	792121.968410	40.132826
3045.862719	793661.932886	40.137844
3049.032297	795218.215039	40.142861
3052.030486	796775.403267	40.147879
3055.100730	798322.686161	40.152896
3058.079905	799880.651211	40.157914
3060.864173	801466.187867	40.162932
3064.189995	803038.160783	40.167949
3067.289302	804631.966693	40.172967
3070.173784	806212.968887	40.177984
3073.220771	807821.931330	40.183002
3076.229337	809431.692686	40.188020
3079.318940	811031.286366	40.193037
3082.198998	812638.010020	40.198055
3085.284740	814263.216787	40.203072
3088.577328	815879.158439	40.208090
3091.343589	817519.838113	40.213108
3094.991688	819143.327101	40.218125
3097.769774	820785.200493	40.223143
3101.060124	822429.801565	40.228160
3104.447491	824069.002480	40.233178
3107.166684	825713.657661	40.238196
3110.561113	827359.348363	40.243213
3113.685695	829023.819097	40.248231
3116.712941	830681.108384	40.253248
3119.937301	832340.035738	40.258266
3122.887859	834019.470755	40.263284
3126.238238	835670.508841	40.268301
3129.197506	837354.571341	40.273319
3132.724249	839034.642265	40.278336
3136.072542	840688.957787	40.283354
3139.102251	842379.559901	40.288372
3142.220396	844045.582767	40.293389
3144.801089	845738.276436	40.298407
3148.405839	847419.947289	40.303424
3152.040920	849098.441087	40.308442
3154.983826	850799.907205	40.313460
3158.038924	852487.975096	40.318477
3161.272390	854174.291652	40.323495
3164.509737	855872.762751	40.328512
3167.971184	857568.205487	40.333530
3171.032740	859269.161658	40.338548
3173.541806	860964.111371	40.343565
3177.123783	862663.453144	40.348583
3180.183333	864365.893741	40.353600
3183.706549	866071.944486	40.358618
3186.385803	867776.295227	40.363636
3189.967364	869488.921617	40.368653
3192.954231	871187.507017	40.373671
3196.463440	872908.554209	40.378688
3199.389182	874615.751662	40.383706
3202.515645	876327.743257	40.388724
3206.125120	878045.056554	40.393741
3209.138891	879758.873407	40.398759
3212.151790	881472.189263	40.403776
3215.748540	883196.885068	40.408794
3218.453807	884923.920780	40.413812
3221.799749	886613.359849	40.418829
3225.227976	888301.615993	40.423847
3228.174912	889979.518337	40.428864
3231.377958	891641.165027	40.433882
3234.702242	893321.692386	40.438900
3238.006110	894986.110439	40.443917
3241.278303	896665.466684	40.448935
3244.442697	898331.239693	40.453952
3247.309653	900009.380919	40.458970
3250.309554	901700.384383	40.463988
3253.476241	903382.283478	40.469005
3257.082552	905077.557969	40.474023
3259.913577	906785.912935	40.479040
3263.211011	908493.761879	40.484058
3266.482540	910208.779720	40.489076
3269.754515	911929.127350	40.494093
3272.937107	913655.485188	40.499111
3275.560443	915395.607209	40.504128
3279.278317	917118.574849	40.509146
3282.654814	918882.329650	40.514164
3285.679297	920624.170041	40.519181
3288.894755	922376.641578	40.524199
3291.816694	924150.072618	40.529216
3295.452237	925923.375687	40.534234
3298.592980	927699.622725	40.539252
3301.592467	929488.809566	40.544269
3305.147192	931280.846170	40.549287
3308.444968	933087.253747	40.554304
3311.281003	934880.294963	40.559322
3314.390751	936690.857491	40.564340
3317.989857	938527.970804	40.569357
3321.644210	940349.610365	40.574375
3324.657627	942176.643440	40.579392
3328.008062	944011.958008	40.584410
3331.326159	945856.367580	40.589428
3334.521446	947691.926781	40.594445
3338.028368	949541.379711	40.599463
3340.941367	951403.045323	40.604480
3344.353562	953279.411243	40.609498
3347.631668	955188.435088	40.614516
3351.000368	957110.503020	40.619533
3354.195339	959031.470357	40.624551
3357.269096	960964.912161	40.629568
3360.707298	962890.611137	40.634586
3364.439174	964836.027325	40.639604
3367.423044	966788.522898	40.644621
3370.693502	968731.719570	40.649639
3374.073824	970697.556109	40.654656
3377.436743	972647.897869	40.659674
3380.567667	974625.105860	40.664692
3384.159245	976588.982975	40.669709
3387.896099	978555.766162	40.674727
3390.735644	980527.278941	40.679744
3394.528137	982508.175979	40.684762
3397.843711	984475.519571	40.689780
3400.979115	986469.356673	40.694797
3404.573392	988447.442639	40.699815
3407.933308	990436.059306	40.704832
3411.211874	992415.149341	40.709850
3414.184567	994410.115451	40.714868
3417.872416	996418.829492	40.719885
3421.093598	998412.345708	40.724903
3424.338220	1000420.683694	40.729920
3428.044369	1002410.672785	40.734938
3431.624734	1004425.875219	40.739956
3435.208387	1006433.668343	40.744973
3438.386570	1008434.804862	40.749991
3441.668383	1010455.073100	40.755008
3445.354188	1012436.158240	40.760013
3448.563022	1014382.618307	40.765018
3451.739090	1016273.979575	40.770023
3455.452345	1018096.624196	40.775028
3458.470060	1019857.317828	40.780032
3461.896742	1021518.423572	40.785037
3464.830594	1023133.572649	40.790042
3467.369253	1024658.708944	40.795047
3470.685945	1026104.172578	40.800052
3473.543325	1027481.267285	40.805056
3476.697696	1028774.526528	40.810061
3478.834199	1029983.160250	40.815066
3481.310203	1031124.901468	40.820071
3483.785312	1032196.170739	40.825076
3486.165998	1033192.574387	40.830080
3488.268542	1034107.122613	40.835085
3490.392361	1034969.879888	40.840090
3492.264199	1035777.144518	40.845095
3494.518316	1036507.954926	40.850100
3496.198867	1037191.980191	40.855104
3498.263551	1037793.802652	40.860109
3500.116434	1038346.888199	40.865114
3501.201540	1038855.498129	40.870119
3503.239754	1039297.814104	40.875124
3504.497495	1039704.088799	40.880128
3505.617166	1040057.414092	40.885133
3506.941683	1040360.255347	40.890138
3508.221230	1040625.992895	40.895143
3509.489354	1040848.251153	40.900148
3510.693338	1041044.141102	40.905152
3511.658250	1041183.847803	40.910157
3512.622102	1041299.017594	40.915162
3513.381734	1041380.702829	40.920167
3514.162321	1041426.066881	40.925172
3514.876055	1041464.197616	40.930176
3515.702163	1041446.482884	40.935181
3516.520213	1041425.292299	40.940186
3517.186783	1041359.020186	40.945191
3517.915365	1041279.214574	40.950196
3518.282491	1041182.177589	40.955200
3519.143368	1041050.670451	40.960205
3519.639951	1040913.424473	40.965210
3520.124087	1040754.828931	40.970215
3520.171451	1040565.291724	40.975220
3520.510356	1040379.274406	40.980224
3521.347199	1040166.504889	40.985229
3521.836476	1039948.470797	40.990234
3522.159769	1039703.402858	40.995239
3522.867653	1039444.443927	41.000244
3522.775367	1039189.276521	41.005248
3523.108061	1038901.849446	41.010253
3523.732519	1038617.934961	41.015258
3523.832850	1038310.222037	41.020263
3524.328369	1037999.044349	41.025268
3524.232828	1037679.827849	41.030272
3524.483263	1037339.851271	41.035277
3524.671732	1037017.263566	41.040282
3524.799492	1036672.239870	41.045287
3525.435900	1036305.165598	41.050292
3525.151798	1035955.524841	41.055296
3525.489360	1035582.264452	41.060301
3525.784361	1035213.337306	41.065306
3525.857279	1034829.143469	41.070311
3526.222086	1034454.159005	41.075316
3526.186339	1034062.000052	41.080320
3526.408222	1033665.902166	41.085325
3526.581705	1033258.466821	41.090330
3526.466942	1032848.727493	41.095335
3526.468785	1032436.230007	41.100340
3526.313022	1032043.174708	41.105344
3526.715740	1031627.745586	41.110349
3526.711006	1031220.964648	41.115354
3526.785205	1030802.141375	41.120359
3527.029651	1030363.031808	41.125364
3527.032547	1029940.768320	41.130368
3527.086444	1029500.073625	41.135373
3526.687154	1029066.388490	41.140378
3526.825952	1028636.646979	41.145383
3526.789715	1028200.124058	41.150388
3526.999032	1027775.339085	41.155392
3526.719951	1027335.399715	41.160397
3527.331276	1026898.765213	41.165402
3526.867908	1026452.007868	41.170407
3527.058947	1026008.496896	41.175412
3527.070400	1025563.139927	41.180416
3526.892391	1025119.134862	41.185421
3526.997035	1024678.051173	41.190426
3526.915833	1024221.074098	41.195431
3527.343588	1023769.014297	41.200436
3526.763976	1023324.157705	41.205440
3527.026468	1022874.378473	41.210445
3526.828422	1022418.242459	41.215450
3526.641794	1021967.689017	41.220455
3527.138027	1021504.385597	41.225460
3526.835015	1021059.206446	41.230464
3526.807798	1020612.298355	41.235469
3526.698462	1020160.035568	41.240474
3526.347615	1019713.787805	41.245479
3526.681330	1019251.876300	41.250484
3526.386875	1018803.219428	41.255488
3526.511315	1018358.628085	41.260493
3526.363404	1017901.728022	41.265498
3526.213533	1017447.798148	41.270503
3526.315435	1016997.476471	41.275508
3526.120890	1016553.376663	41.280512
3526.174391	1016092.706422	41.285517
3526.330797	1015647.409838	41.290522
3526.076118	1015196.032041	41.295527
3526.484471	1014745.576282	41.300532
3526.105453	1014288.420106	41.305536
3525.832091	1013832.665298	41.310541
3525.969717	1013387.386780	41.315546
3526.113279	1012942.266175	41.320551
3526.261940	1012481.575343	41.325556
3525.902054	1012033.358889	41.330560
3525.751047	1011576.915554	41.335565
3525.711371	1011128.962697	41.340570
3525.671544	1010667.183196	41.345575
3525.404756	1010222.400544	41.350580
3525.252643	1009786.597421	41.355584
3524.937111	1009340.490358	41.360589
3525.110851	1008897.376165	41.365594
3525.183439	1008467.943051	41.370599
3525.555914	1008016.274089	41.375604
3525.446627	1007578.349731	41.380608
3525.106243	1007120.215789	41.385613
3525.085410	1006672.488365	41.390618
3524.877310	1006238.169339	41.395623
3525.134444	1005793.242207	41.400628
3524.991146	1005367.302183	41.405632
3524.957536	1004917.687760	41.410637
3524.771060	1004479.049309	41.415642
3524.750145	1004033.737569	41.420647
3524.975401	1003593.309486	41.425652
3524.669179	1003161.881548	41.430656
3524.557567	1002709.186591	41.435661
3524.563662	1002277.542396	41.440666
3524.367008	1001850.081315	41.445671
3524.430058	1001396.863351	41.450676
3524.363392	1000967.271214	41.455680
3523.996681	1000527.479939	41.460685
3524.040089	1000092.257392	41.465690
3524.089320	999673.056453	41.470695
3524.152816	999242.046793	41.475700
3523.739235	998812.153459	41.480704
3523.814508	998375.723046	41.485709
3524.023676	997951.501643	41.490714
3523.560337	997519.863583	41.495719
3523.577064	997085.192914	41.500724
3523.300745	996671.567154	41.505728
3523.590906	996251.781049	41.510733
3523.505302	995826.377980	41.515738
3523.287521	995409.047512	41.520743
3523.339107	994977.130846	41.525748
3523.287305	994569.158025	41.530752
3523.474573	994140.856394	41.535757
3523.256131	993715.706434	41.540762
3522.908364	993304.769061	41.545767
3522.731343	992883.544074	41.550772
3522.542489	992475.345799	41.555776
3522.619191	992064.540977	41.560781
3522.375384	991656.585194	41.565786
3522.472715	991252.442057	41.570791
3522.548113	990835.116541	41.575796
3522.283170	990430.097423	41.580800
3522.378836	990015.729887	41.585805
3522.435204	989609.917046	41.590810
3522.119850	989208.718452	41.595815
3522.096536	988796.816364	41.600820
3521.887378	988397.492942	41.605824
3521.807156	987994.024822	41.610829
3522.315253	987601.938128	41.615834
3521.770871	987199.660329	41.620839
3522.003607	986796.933464	41.625844
3521.748031	986397.672352	41.630848
3521.750259	985995.121804	41.635853
3521.989000	985596.698522	41.640858
3521.448167	985199.839158	41.645863
3521.580460	984803.524190	41.650868
3521.635930	984409.536018	41.655872
3521.540082	984011.447252	41.660877
3521.372291	983616.465241	41.665882
3520.838103	983229.811491	41.670887
3520.995801	982835.209672	41.675892
3521.314984	982456.756345	41.680896
3521.034022	982068.518038	41.685901
3520.930138	981672.805155	41.690906
3520.462409	981301.823799	41.695911
3520.870444	980910.659690	41.700916
3520.519195	980535.118255	41.705920
3520.568256	980154.115734	41.710925
3520.810120	979772.860722	41.715930
3520.555260	979384.630769	41.720935
3520.593700	979014.491552	41.725940
3520.401215	978639.287554	41.730944
3520.238265	978256.923662	41.735949
3520.364675	977880.640537	41.740954
3520.303565	977497.916027	41.745959
3520.522518	977121.958469	41.750964
3520.186794	976742.843389	41.755968
3520.232900	976372.531762	41.760973
3520.333878	975989.679575	41.765978
3520.151369	975615.057091	41.770983
3520.056823	975246.063805	41.775988
3519.815248	974877.266408	41.780992
3519.723676	974510.961782	41.785997
3519.877120	974139.803752	41.791002
3519.419213	973782.407805	41.796007
3519.481005	973401.734977	41.801012
3519.487101	973049.886907	41.806016
3519.427312	972678.571519	41.811021
3519.540084	972307.594745	41.816026
3519.318816	971953.467886	41.821031
3519.334105	971592.923798	41.826036
3518.766499	971245.851158	41.831040
3518.879737	970883.974984	41.836045
3519.282736	970532.787172	41.841050
3518.657601	970174.508961	41.846055
3519.073042	969815.254365	41.851060
3518.763132	969477.129491	41.856064
3518.785517	969117.602482	41.861069
3518.760027	968760.017605	41.866074
3518.985904	968419.981064	41.871079
3518.524500	968065.947151	41.876084
3518.364625	967718.495960	41.881088
3518.567664	967369.593880	41.886093
3518.487962	967022.576681	41.891098
3518.382305	966679.262006	41.896103
3518.327345	966324.172850	41.901108
3517.978754	965992.700648	41.906112
3518.338957	965644.255194	41.911117
3518.376908	965307.883111	41.916122
3517.679260	964967.990105	41.921127
3517.995194	964621.252192	41.926132
3517.831659	964291.119987	41.931136
3518.251364	963945.009613	41.936141
3518.027904	963614.162973	41.941146
3517.490935	963272.674354	41.946151
3517.571357	962947.125547	41.951156
3517.735234	962620.956915	41.956160
3517.619896	962275.323959	41.961165
3517.381041	961951.142695	41.966170
3517.021003	961625.591692	41.971175
3517.092773	961300.734864	41.976180
3517.078523	960972.542859	41.981184
3517.051219	960659.226765	41.986189
3516.982328	960328.851597	41.991194
3516.474528	960022.928708	41.996199
3517.100635	959694.166425	42.001204
3516.821458	959383.370252	42.006208
3517.052169	959050.716478	42.011213
3516.652255	958739.513456	42.016218
3516.318732	958435.241719	42.021223
3516.590467	958114.288873	42.026228
3516.615281	957809.925104	42.031232
3516.460257	957492.732927	42.036237
3516.347785	957178.065227	42.041242
3516.268051	956867.394653	42.046247
3516.309044	956552.569515	42.051252
3516.383377	956258.802800	42.056256
3516.247481	955946.621135	42.061261
3516.261521	955639.300983	42.066266
3515.983834	955328.874382	42.071271
3516.289418	955023.630909	42.076276
3516.031187	954723.269989	42.081280
3515.843034	954420.331753	42.086285
3515.724697	954124.036089	42.091290
3515.478863	953814.699889	42.096295
3515.683795	953528.620180	42.101300
3515.484959	953239.257339	42.106304
3515.476768	952935.230551	42.111309
3515.441383	952638.746948	42.116314
3515.153371	952354.431988	42.121319
3515.519679	952067.968147	42.126324
3515.088907	951790.800490	42.131328
3515.178368	951503.202875	42.136333
3515.419545	951229.528325	42.141338
3514.608964	950958.212330	42.146343
3514.972708	950671.383477	42.151348
3515.062903	950398.358817	42.156352
3514.868082	950119.913534	42.161357
3514.931307	949850.499365	42.166362
3514.638507	949583.904273	42.171367
3515.040987	949300.149413	42.176372
3514.688353	949016.694603	42.181376
3514.489534	948754.442421	42.186381
3514.618377	948487.242290	42.191386
3514.652764	948217.077035	42.196391
3514.565315	947944.907772	42.201396
3514.132959	947683.883493	42.206400
3514.387183	947417.564116	42.211405
3514.579579	947154.399943	42.216410
3514.288206	946881.729315	42.221415
3514.131090	946608.256250	42.226420
3514.163226	946359.150363	42.231424
3513.774876	946095.836227	42.236429
3513.836099	945836.647398	42.241434
3513.507958	945586.031521	42.246439
3513.634747	945326.518981	42.251444
3513.678537	945077.732238	42.256448
3513.497754	944823.128826	42.261453
3513.719228	944569.500054	42.266458
3513.672188	944325.001641	42.271463
3513.545674	944069.873281	42.276468
3513.581414	943823.805054	42.281472
3513.559699	943568.059967	42.286477
3513.479067	943312.695118	42.291482
3513.165950	943075.270142	42.296487
3513.070015	942823.811399	42.301492
3513.176993	942584.187057	42.306496
3513.257775	942337.849181	42.311501
3513.434856	942084.489190	42.316506
3513.021441	941849.036698	42.321511
3513.259535	941596.696870	42.326516
3512.871944	941367.542720	42.331520
3512.782009	941125.296079	42.336525
3512.895078	940878.404480	42.341530
3512.609429	940644.793116	42.346535
3512.851907	940403.128973	42.351540
3512.843986	940183.348913	42.356544
3512.743298	939944.978974	42.361549
3512.542393	939707.477376	42.366554
3512.484578	939481.924368	42.371559
3512.274866	939250.251077	42.376564
3511.928099	939016.768502	42.381568
3512.133318	938795.936116	42.386573
3512.051542	938565.841265	42.391578
3511.776332	938347.466081	42.396583
3511.946663	938117.405834	42.401588
3511.988171	937901.165272	42.406592
3512.035370	937676.955396	42.411597
3511.867349	937466.101595	42.416602
3511.843808	937249.077598	42.421607
3512.391462	937020.825084	42.426612
3511.963520	936805.767524	42.431616
3511.790632	936580.396010	42.436621
3511.667608	936358.555674	42.441626
3511.726389	936147.515528	42.446631
3511.833850	935917.944597	42.451636
3511.795159	935716.687950	42.456640
3511.550876	935498.188874	42.461645
3511.527037	935271.489425	42.466650
3511.322575	935056.707126	42.471655
3511.389815	934844.941651	42.476660
3511.301135	934643.940015	42.481664
3511.530821	934431.459476	42.486669
3511.531920	934217.952465	42.491674
3511.229257	934016.674256	42.496679
3511.431396	933799.854414	42.501684
3511.229597	933593.457133	42.506688
3511.162113	933391.060604	42.511693
3511.503635	933174.480022	42.516698
3510.951993	932969.747618	42.521703
3511.281818	932771.869065	42.526708
3510.794821	932567.878318	42.531712
3510.966781	932357.243548	42.536717
3511.130876	932157.545418	42.541722
3510.765212	931960.231053	42.546727
3511.069943	931750.702271	42.551732
3510.918613	931547.576907	42.556736
3510.980465	931333.847264	42.561741
3510.896206	931138.568181	42.566746
3510.652209	930940.235591	42.571751
3510.696889	930732.917852	42.576756
3510.669258	930555.756358	42.581760
3510.671082	930360.434433	42.586765
3510.564758	930164.931069	42.591770
3510.627115	929972.657979	42.596775
3510.407212	929762.656887	42.601780
3510.404664	929589.972955	42.606784
3510.520726	929388.545688	42.611789
3510.511005	929187.515719	42.616794
3510.179659	929006.510534	42.621799
3510.533663	928815.780484	42.626804
3510.108663	928634.201713	42.631808
3510.094360	928445.344236	42.636813
3510.110740	928253.785101	42.641818
3509.592714	928068.071415	42.646823
3509.904098	927888.651625	42.651828
3509.864897	927715.624702	42.656832
3509.529299	927533.225052	42.661837
3509.837193	927359.745081	42.666842
3509.967131	927178.793971	42.671847
3510.246955	926999.157308	42.676852
3509.862652	926823.563872	42.681856
3509.910626	926635.112519	42.686861
3510.182544	926448.827945	42.691866
3509.530961	926271.050069	42.696871
3509.729234	926086.879307	42.701876
3509.708026	925924.170959	42.706880
3509.756719	925736.264482	42.711885
3509.749501	925546.149935	42.716890
3509.130918	925364.780180	42.721895
3509.211404	925197.323106	42.726900
3509.168456	925033.245550	42.731904
3509.383096	924864.794730	42.736909
3509.526904	924699.426517	42.741914
3508.935659	924515.524082	42.746919
3508.915690	924347.672491	42.751924
3509.112552	924197.662194	42.756928
3509.384267	924024.753122	42.761933
3508.973832	923864.257701	42.766938
3508.963583	923693.115057	42.771943
3509.423223	923524.004921	42.776948
3509.172330	923370.776109	42.781952
3508.877001	923203.511081	42.786957
3508.924471	923027.914454	42.791962
3508.960842	922857.699171	42.796967
3508.928772	922705.569344	42.801972
3508.971706	922540.439840	42.806977
3508.705396	922379.203165	42.811981
3508.996404	922214.311319	42.816986
3508.651025	922067.985693	42.821991
3509.172196	921892.562564	42.826996
3508.832234	921735.743158	42.832001
3508.548407	921572.946297	42.837005
3508.667205	921418.350596	42.842010
3508.370186	921264.107555	42.847015
3508.626804	921103.612339	42.852020
3508.622881	920955.564956	42.857025
3508.650642	920805.584265	42.862029
3508.494991	920643.988905	42.867034
3508.305434	920494.227788	42.872039
3508.360122	920332.203630	42.877044
3508.353615	920197.220453	42.882049
3508.319806	920029.429064	42.887053
3508.632215	919894.193361	42.892058
3508.480062	919745.271317	42.897063
3508.098405	919586.279555	42.902068
3507.913161	919432.928102	42.907073
3507.989633	919281.357537	42.912077
3508.218181	919141.497894	42.917082
3507.927740	919004.414689	42.922087
3508.266897	918855.772197	42.927092
3508.246255	918707.569868	42.932097
3508.238825	918556.666553	42.937101
3507.882357	918393.497278	42.942106
3507.945674	918259.898027	42.947111
3507.726895	918122.395750	42.952116
3507.873614	917984.637273	42.957121
3507.756957	917849.902573	42.962125
3507.619756	917696.301628	42.967130
3507.281666	917569.008211	42.972135
3508.233202	917428.022759	42.977140
3508.128170	917287.111464	42.982145
3507.769737	917146.527067	42.987149
3507.735979	917013.298254	42.992154
3507.521362	916872.105463	42.997159
3507.813122	916730.247943	43.002164
3507.598632	916593.765332	43.007169
3507.615172	916441.836634	43.012173
3507.547231	916309.751596	43.017178
3507.283095	916190.982802	43.022183
3507.305445	916055.410527	43.027188
3507.231150	915917.925042	43.032193
3507.297799	915799.863540	43.037197
3507.678270	915669.326058	43.042202
3507.221620	915537.382655	43.047207
3507.368681	915393.877219	43.052212
3507.307025	915271.877247	43.057217
3507.183289	915143.625163	43.062221
3507.323732	915001.651349	43.067226
3507.056358	914880.928498	43.072231
3507.013191	914743.986176	43.077236
3507.181104	914631.950215	43.082241
3507.079331	914508.976720	43.087245
3507.347029	914381.027516	43.092250
3506.974965	914255.877613	43.097255
3507.069371	914130.070078	43.102260
3507.192550	914006.085029	43.107265
3507.133184	913877.022074	43.112269
3507.151658	913746.016725	43.117274
3506.744293	913631.550589	43.122279
3507.009257	913499.246465	43.127284
3506.819437	913387.147652	43.132289
3506.523930	913263.311113	43.137293
3506.779316	913134.082476	43.142298
3506.992747	913021.042712	43.147303
3506.708286	912895.172920	43.152308
3506.489729	912781.525004	43.157313
3506.508760	912661.765830	43.162317
3506.778551	912550.248618	43.167322
3506.580828	912445.550617	43.172327
3507.005162	912319.454507	43.177332
3506.792430	912209.069734	43.182337
3506.354593	912092.745795	43.187341
3506.951352	911971.045639	43.192346
3506.756677	911847.353267	43.197351
3506.932897	911722.729752	43.202356
3506.557282	911607.541639	43.207361
3506.386578	911491.642792	43.212365
3506.195985	911367.649864	43.217370
3506.193492	911263.186290	43.222375
3506.598256	911135.042501	43.227380
3506.357366	911023.867606	43.232385
3506.408311	910914.569909	43.237389
3506.798790	910802.515523	43.242394
3506.138962	910702.004723	43.247399
3506.310761	910589.307374	43.252404
3506.123659	910490.738855	43.257409
3505.953687	910378.960964	43.262413
3506.261773	910265.945401	43.267418
3506.526129	910165.272554	43.272423
3506.297871	910050.316766	43.277428
3506.273079	909932.915232	43.282433
3506.082605	909825.081620	43.287437
3506.373755	909714.853027	43.292442
3506.083275	909624.576205	43.297447
3506.220763	909508.970497	43.302452
3506.075584	909408.640535	43.307457
3506.372131	909292.522086	43.312461
3506.011447	909190.006357	43.317466
3505.792635	909091.128854	43.322471
3506.160483	908982.319142	43.327476
3506.034233	908878.794921	43.332481
3505.903385	908778.643989	43.337485
3505.980368	908680.867380	43.342490
3505.922558	908581.472167	43.347495
3505.891377	908465.583193	43.352500
3505.693778	908376.716972	43.357505
3505.714768	908272.289366	43.362509
3506.211058	908167.202943	43.367514
3505.535010	908070.696711	43.372519
3505.998986	907966.865348	43.377524
3505.854802	907866.989407	43.382529
3505.800393	907771.918420	43.387533
3505.893684	907665.442422	43.392538
3505.747984	907570.479455	43.397543
3506.242011	907470.780536	43.402548
3506.219919	907370.200481	43.407553
3505.982731	907267.146610	43.412557
3505.943481	907159.236141	43.417562
3505.736253	907060.127589	43.422567
3505.621066	906962.062998	43.427572
3505.661171	906866.575149	43.432577
3505.681404	906774.078828	43.437581
3506.040606	906663.006730	43.442586
3505.833430	906566.107705	43.447591
3505.939050	906461.535627	43.452596
3505.823182	906359.602369	43.457601
3505.304497	906269.404908	43.462605
3505.886232	906167.835490	43.467610
3505.579581	906077.889366	43.472615
3505.683955	905977.166796	43.477620
3505.413016	905888.658657	43.482625
3505.659034	905794.854824	43.487629
3505.793827	905696.726729	43.492634
3505.410004	905603.795178	43.497639
3505.616031	905497.066127	43.502644
3505.705175	905411.578128	43.507649
3505.512152	905317.742121	43.512653
3505.590992	905228.587021	43.517658
3505.560239	905142.439321	43.522663
3505.711679	905051.436374	43.527668
3505.057902	904960.082202	43.532673
3505.238365	904866.273540	43.537677
3505.305790	904767.947227	43.542682
3505.283310	904678.414090	43.547687
3505.450543	904589.620149	43.552692
3505.225246	904504.170042	43.557697
3505.141952	904408.756856	43.562701
3505.489248	904315.393896	43.567706
3505.496784	904237.234637	43.572711
3505.506493	904148.266645	43.577716
3505.118019	904056.178495	43.582721
3504.979481	903969.644461	43.587725
3505.277915	903884.967061	43.592730
3504.990479	903802.507893	43.597735
3504.708503	903714.063539	43.602740
3504.658933	903625.386489	43.607745
3504.817878	903555.684981	43.612749
3505.114493	903474.089783	43.617754
3504.673939	903385.762863	43.622759
3504.985021	903311.979966	43.627764
3505.126979	903238.609998	43.632769
3505.161908	903149.332423	43.637773
3504.910615	903069.944841	43.642778
3504.599165	902985.643844	43.647783
3504.976416	902905.378264	43.652788
3505.119494	902823.123269	43.657793
3504.627991	902737.496965	43.662797
3504.729446	902659.493214	43.667802
3504.769495	902583.042824	43.672807
3505.038973	902504.333588	43.677812
3504.759239	902431.119036	43.682817
3504.860795	902354.269299	43.687821
3504.761833	902272.142615	43.692826
3505.022912	902194.395672	43.697831
3504.825175	902116.530184	43.702836
3504.790146	902041.436179	43.707841
3504.251927	901960.921781	43.712845
3504.814956	901875.591221	43.717850
3504.649484	901801.770423	43.722855
3504.534602	901720.893231	43.727860
3504.298073	901643.317168	43.732865
3504.755794	901575.086389	43.737869
3504.993857	901504.767107	43.742874
3504.634256	901440.820537	43.747879
3504.906308	901353.309554	43.752884
3505.083558	901281.356284	43.757889
3504.979185	901200.566407	43.762893
3504.984883	901118.984867	43.767898
3504.588652	901040.944059	43.772903
3504.855301	900958.351723	43.777908
3504.787364	900878.227047	43.782913
3504.498701	900805.475493	43.787917
3504.888821	900729.231829	43.792922
3504.713615	900655.783777	43.797927
3504.774359	900567.909167	43.802932
3504.812214	900505.238234	43.807937
3504.448585	900434.328797	43.812941
3504.783918	900357.123542	43.817946
3504.832409	900281.606011	43.822951
3504.691275	900194.434749	43.827956
3504.908587	900118.307844	43.832961
3504.574154	900050.865030	43.837965
3504.447308	899955.769447	43.842970
3504.217532	899902.599338	43.847975
3504.242623	899822.347728	43.852980
3504.397081	899760.421837	43.857985
3504.446888	899691.076592	43.862989
3504.424025	899607.353287	43.867994
3503.998926	899552.473757	43.872999
3504.621752	899490.564311	43.878004
3504.478023	899412.555876	43.883009
3504.510093	899348.520970	43.888013
3504.617593	899270.179445	43.893018
3504.139337	899204.681740	43.898023
3504.525777	899132.376801	43.903028
3504.452436	899057.828737	43.908033
3504.555981	898987.113845	43.913037
3504.619669	898922.875733	43.918042
3504.580043	898846.580819	43.923047
3504.513112	898767.874718	43.928052
3504.530912	898697.363495	43.933057
3504.496133	898640.189263	43.938061
3504.382161	898558.590342	43.943066
3504.186169	898496.708316	43.948071
3504.281527	898428.595728	43.953076
3504.418758	898361.731131	43.958081
3504.007420	898288.291111	43.963085
3504.196270	898222.285709	43.968090
3504.102891	898166.661865	43.973095
3504.342433	898090.503935	43.978100
3504.356933	898032.832447	43.983105
3504.034630	897959.759881	43.988109
3504.390437	897892.370722	43.993114
3503.982069	897831.095998	43.998119
3503.903195	897760.685613	44.003124
3504.199066	897706.345557	44.008129
3504.101686	897642.409234	44.013133
3504.613199	897580.883642	44.018138
3504.468116	897521.590923	44.023143
3504.127848	897450.253663	44.028148
3504.234543	897378.358816	44.033153
3504.141283	897323.209703	44.038157
3504.328592	897253.328815	44.043162
3504.137636	897191.335053	44.048167
3504.315657	897115.270749	44.053172
3503.994676	897050.978124	44.058177
3503.920219	896988.576485	44.063181
3504.040033	896928.171122	44.068186
3504.004405	896859.867991	44.073191
3504.258018	896803.883723	44.078196
3503.870676	896743.753188	44.083201
3503.722644	896684.355561	44.088205
3503.859688	896616.794026	44.093210
3503.663315	896563.007218	44.098215
3503.809054	896504.815421	44.103220
3503.734442	896448.205342	44.108225
3503.854414	896397.360243	44.113229
3503.908572	896335.799866	44.118234
3503.880893	896277.344423	44.123239
3503.773070	896213.876834	44.128244
3503.746714	896158.318839	44.133249
3503.798292	896101.974407	44.138253
3503.898388	896040.403256	44.143258
3503.743109	895993.948362	44.148263
3504.095892	895931.464698	44.153268
3503.769323	895868.125914	44.158273
3503.818027	895817.770543	44.163277
3504.036649	895760.235560	44.168282
3503.879901	895706.530737	44.173287
3504.073104	895645.036598	44.178292
3503.915676	895583.212999	44.183297
3503.390588	895526.281376	44.188301
3503.871126	895456.136755	44.193306
3503.328572	895415.539488	44.198311
3503.591284	895353.934104	44.203316
3503.878727	895307.787233	44.208321
3503.559669	895249.079270	44.213325
3503.687826	895189.427196	44.218330
3503.676202	895144.874630	44.223335
3503.718899	895083.689159	44.228340
3503.944704	895030.301512	44.233345
3503.501882	894971.901024	44.238349
3503.484840	894924.448095	44.243354
3503.186957	894876.461123	44.248359
3503.770053	894816.246922	44.253364
3503.564357	894778.875821	44.258369
3503.627225	894725.028882	44.263373
3503.493347	894657.585333	44.268378
3503.275427	894615.865640	44.273383
3503.581472	894566.036725	44.278388
3503.430923	894512.416251	44.283393
3503.227629	894471.079722	44.288397
3503.408917	894412.280682	44.293402
3503.351884	894380.005467	44.298407
3503.846024	894317.674113	44.303412
3503.856571	894275.140985	44.308417
3503.433365	894207.933099	44.313421
3503.575182	894150.781149	44.318426
3503.641644	894109.784212	44.323431
3503.629835	894049.176593	44.328436
3503.792919	893987.572839	44.333441
3503.387048	893945.395857	44.338445
3503.368753	893892.327763	44.343450
3503.445568	893851.327261	44.348455
3503.788951	893801.775525	44.353460
3503.602275	893751.924000	44.358465
3503.310297	893697.932469	44.363469
3503.395072	893642.911621	44.368474
3503.287222	893597.782759	44.373479
3503.320484	893548.279914	44.378484
3503.456427	893501.659999	44.383489
3503.365941	893444.925950	44.388493
3503.477962	893407.106789	44.393498
3503.443262	893352.102820	44.398503
3503.662725	893297.539844	44.403508
3503.446234	893246.141938	44.408513
3503.322960	893207.393416	44.413517
3503.738507	893150.766434	44.418522
3503.552504	893098.588721	44.423527
3503.347165	893047.283868	44.428532
3503.317181	893003.104307	44.433537
3503.304976	892957.471199	44.438541
3503.583498	892899.027280	44.443546
3503.307092	892854.113676	44.448551
3503.503282	892808.348357	44.453556
3503.404765	892752.672311	44.458561
3503.540587	892708.849911	44.463565
3503.852643	892662.000749	44.468570
3503.545259	892601.619826	44.473575
3503.557418	892555.012578	44.478580
3503.656667	892501.912187	44.483585
3503.282366	892451.113276	44.488589
3503.562937	892406.877939	44.493594
3502.902720	892368.792353	44.498599
3503.491301	892310.388030	44.503604
3503.558059	892258.160993	44.508609
3503.464565	892216.113141	44.513613
3503.696275	892155.735385	44.518618
3503.129733	892114.248212	44.523623
3503.177552	892059.024795	44.528628
3503.441155	892019.914376	44.533633
3503.292103	891979.711257	44.538637
3503.452959	891932.590928	44.543642
3503.153005	891899.181269	44.548647
3503.289502	891843.554351	44.553652
3503.376827	891797.412064	44.558657
3503.081977	891751.042252	44.563661
3503.235793	891710.013694	44.568666
3503.062392	891662.269266	44.573671
3503.015739	891619.822484	44.578676
3503.024556	891584.812794	44.583681
3503.153146	891539.532004	44.588685
3503.298209	891486.608060	44.593690
3502.942959	891450.400298	44.598695
3503.127931	891415.747395	44.603700
3503.030830	891345.840858	44.608705
3502.603768	891324.344385	44.613709
3502.544555	891273.483093	44.618714
3502.338364	891255.818515	44.623719
3502.564466	891211.776350	44.628724
3502.900432	891187.832503	44.633729
3502.808165	891144.906141	44.638733
3502.885117	891098.469784	44.643738
3503.076929	891078.611324	44.648743
3503.000279	891023.785296	44.653748
3502.935665	890993.523258	44.658753
3502.897790	890970.123686	44.663757
3503.226460	890925.868991	44.668762
3502.846222	890892.563397	44.673767
3502.773960	890841.216818	44.678772
3502.903977	890798.347958	44.683777
3502.827666	890774.373590	44.688781
3503.078618	890728.292457	44.693786
3503.000071	890705.091949	44.698791
3502.849694	890653.176217	44.703796
3502.926511	890618.052693	44.708801
3502.852724	890576.860074	44.713805
3503.126783	890529.419383	44.718810
3503.132096	890504.946810	44.723815
3502.798126	890460.023882	44.728820
3502.766009	890419.403631	44.733825
3502.744443	890391.549522	44.738829
3502.956659	890347.309553	44.743834
3502.613659	890307.900481	44.748839
3502.776008	890275.179013	44.753844
3503.059509	890241.857012	44.758849
3502.718720	890198.771048	44.763853
3503.056446	890161.376915	44.768858
3502.993824	890131.690395	44.773863
3502.969390	890084.005005	44.778868
3502.891998	890049.580544	44.783873
3503.009976	890013.188994	44.788877
3502.952592	889978.180399	44.793882
3502.770597	889942.805178	44.798887
3503.086533	889901.833714	44.803892
3503.083261	889859.656963	44.808897
3502.939897	889815.084530	44.813901
3502.988867	889781.314810	44.818906
3502.739350	889750.883202	44.823911
3503.131436	889704.964088	44.828916
3503.104894	889672.560529	44.833921
3502.845946	889628.973099	44.838925
3503.067541	889581.629970	44.843930
3503.148392	889553.464697	44.848935
3503.167420	889506.251063	44.853940
3502.994359	889456.359852	44.858945
3502.993187	889427.336777	44.863949
3502.972934	889378.870887	44.868954
3502.902584	889350.439294	44.873959
3502.786815	889314.372068	44.878964
3503.135151	889276.583452	44.883969
3502.961623	889234.913902	44.888973
3503.148606	889194.926131	44.893978
3502.816931	889157.635761	44.898983
3502.484409	889117.055792	44.903988
3502.726855	889093.989389	44.908993
3502.999265	889059.501366	44.913997
3502.926038	889024.973329	44.919002
3502.859657	888988.895925	44.924007
3502.777943	888940.436468	44.929012
3502.977159	888908.378420	44.934017
3503.243722	888870.987630	44.939021
3503.227213	888833.836743	44.944026
3502.958960	888798.468686	44.949031
3503.013011	888755.693862	44.954036
3502.988543	888705.771658	44.959041
3502.798120	888670.099718	44.964045
3502.768312	888628.595612	44.969050
3502.685905	888604.709948	44.974055
3502.748303	888559.416570	44.979060
3502.485845	888533.238050	44.984065
3502.700533	888499.627024	44.989069
3502.817801	888472.805108	44.994074
3502.780919	888436.138814	44.999079
3502.803422	888396.075835	45.004084
3502.789528	888361.824331	45.009089
3502.915841	888315.744406	45.014093
3502.978796	888290.188512	45.019098
3502.710689	888251.333570	45.024103
3502.854575	888204.766041	45.029108
3502.942108	888180.850621	45.034113
3502.937091	888153.079707	45.039117
3502.802611	888109.750552	45.044122
3502.537336	888084.247821	45.049127
3502.455271	888044.489927	45.054132
3502.694002	888013.000998	45.059137
3502.230244	887988.304690	45.064141
3502.712898	887950.872333	45.069146
3502.212926	887928.117122	45.074151
3502.611609	887888.859569	45.079156
3502.673463	887863.011651	45.084161
3502.336558	887831.035942	45.089165
3502.502663	887807.976974	45.094170
3502.085733	887771.465838	45.099175
3502.237588	887749.086390	45.104180
3502.228109	887723.830238	45.109185
3502.049378	887698.214765	45.114189
3502.507834	887675.881295	45.119194
3502.447517	887657.407412	45.124199
3502.437142	887628.280011	45.129204
3502.378228	887599.837889	45.134209
3502.524780	887569.813361	45.139213
3502.745491	887529.034271	45.144218
3502.418598	887510.313505	45.149223
3502.770231	887479.286951	45.154228
3502.563754	887457.158964	45.159233
3502.388072	887414.508816	45.164237
3502.553992	887377.028147	45.169242
3502.027020	887366.759654	45.174247
3502.672232	887326.102753	45.179252
3502.520541	887307.546023	45.184257
3502.488315	887285.388668	45.189261
3502.479025	887241.548461	45.194266
3502.624582	887226.426626	45.199271
3502.365124	887192.111851	45.204276
3502.341412	887164.242475	45.209281
3502.108482	887140.375542	45.214285
3502.505293	887119.308262	45.219290
3502.445152	887095.993378	45.224295
3502.345512	887058.360826	45.229300
3502.221186	887039.508371	45.234305
3502.362212	887011.320763	45.239309
3502.615372	886987.373112	45.244314
3502.347266	886957.994435	45.249319
3502.619914	886925.429345	45.254324
3502.338334	886896.536508	45.259329
3502.515280	886877.633890	45.264333
3502.408246	886847.937753	45.269338
3502.476940	886824.794125	45.274343
3502.180695	886790.676600	45.279348
3502.173614	886763.092915	45.284353
3502.330018	886750.484574	45.289357
3502.444606	886709.426817	45.294362
3502.187540	886690.111139	45.299367
3502.496060	886661.023113	45.304372
3502.478269	886634.311699	45.309377
3501.981857	886616.293496	45.314381
3502.386783	886582.930351	45.319386
3502.114375	886570.198680	45.324391
3502.193957	886543.954769	45.329396
3502.432037	886514.103265	45.334401
3502.302585	886498.444075	45.339405
3502.244434	886467.866787	45.344410
3502.337626	886441.910553	45.349415
3502.466441	886412.947683	45.354420
3502.520057	886386.513745	45.359425
3501.910834	886365.609472	45.364429
3502.330401	886334.565590	45.369434
3502.463530	886313.442028	45.374439
3502.286761	886287.142389	45.379444
3502.167245	886255.122126	45.384449
3501.963121	886240.539316	45.389453
3502.155548	886226.278330	45.394458
3502.076871	886201.317317	45.399463
3501.767227	886173.780670	45.404468
3502.148816	886160.746748	45.409473
3502.106577	886134.811451	45.414477
3502.308205	886109.223060	45.419482
3502.163115	886098.308577	45.424487
3502.104718	886074.311680	45.429492
3502.157847	886056.781995	45.434497
3502.639956	886044.021655	45.439501
3502.640121	886005.784999	45.444506
3502.217666	885991.043925	45.449511
3502.140779	885939.848003	45.454516
3502.347671	885937.974718	45.459521
3502.111023	885909.940771	45.464525
3502.370583	885877.275140	45.469530
3502.241484	885872.843475	45.474535
3502.355660	885831.101926	45.479540
3502.510156	885809.295371	45.484545
3502.386792	885786.372842	45.489549
3502.261726	885748.058310	45.494554
3502.331693	885737.688553	45.499559
3502.244280	885707.015258	45.504564
3502.256212	885678.067969	45.509569
3502.041658	885659.032261	45.514573
3502.450196	885629.341732	45.519578
3502.253550	885613.884833	45.524583
3502.213181	885587.075496	45.529588
3502.227750	885558.708031	45.534593
3502.112245	885552.628118	45.539597
3502.316494	885520.453638	45.544602
3501.944720	885503.089092	45.549607
3502.398881	885487.911876	45.554612
3502.475990	885456.919719	45.559617
3502.268601	885433.235146	45.564621
3502.269001	885399.544594	45.569626
3502.116996	885378.851851	45.574631
3502.247386	885365.470283	45.579636
3502.465758	885332.808373	45.584641
3502.254638	885322.290556	45.589645
3502.311388	885293.721217	45.594650
3502.262451	885265.846852	45.599655
3502.227283	885247.167492	45.604660
3501.888379	885211.692268	45.609665
3502.063610	885191.138572	45.614669
3502.272499	885177.743639	45.619674
3502.249919	885168.743535	45.624679
3502.260439	885133.113445	45.629684
3502.382652	885121.668996	45.634689
3502.077444	885100.806866	45.639693
3502.487885	885071.500442	45.644698
3502.313196	885053.811622	45.649703
3502.087519	885024.512944	45.654708
3502.284604	885004.826354	45.659713
3501.924486	884977.970060	45.664717
3502.259080	884945.964559	45.669722
3501.894927	884937.310830	45.674727
3501.923178	884923.170511	45.679732
3502.012220	884898.273070	45.684737
3502.409729	884877.778465	45.689741
3502.148780	884854.874917	45.694746
3502.231887	884839.950788	45.699751
3502.116768	884817.603997	45.704756
3502.039069	884800.963466	45.709761
3502.108218	884766.676977	45.714765
3502.098394	884751.090171	45.719770
3501.891284	884753.448107	45.724775
3502.119441	884720.006553	45.729780
3502.205786	884689.396068	45.734785
3502.048581	884686.710956	45.739789
3502.360804	884651.028200	45.744794
3502.240358	884633.813284	45.749799
3502.093531	884610.502668	45.754804
3502.178981	884578.633017	45.759809
3502.048869	884574.103696	45.764813
3502.330530	884513.831283	45.769818
3501.914622	884441.472832	45.774823
3502.326240	884306.812335	45.779828
3502.345851	884122.150595	45.784833
3502.065091	883868.874926	45.789837
3502.116297	883542.901612	45.794842
3501.583522	883178.460381	45.799847
3501.765482	882756.636816	45.804852
3501.817760	882273.198730	45.809857
3501.523730	881720.513525	45.814861
3501.503066	881102.237941	45.819866
3501.130150	880437.445724	45.824871
3501.278731	879701.265944	45.829876
3500.580907	878898.549403	45.834881
3500.444061	878027.679965	45.839885
3500.700172	877094.278392	45.844890
3500.146164	876110.925150	45.849895
3499.749314	875033.211764	45.854900
3499.205200	873894.409150	45.859905
3498.947047	872700.329562	45.864909
3498.884078	871419.610536	45.869914
3498.259203	870084.353027	45.874919
3498.306631	868664.803372	45.879924
3497.999857	867166.121648	45.884929
3497.318149	865604.377923	45.889933
3496.973694	863955.699296	45.894938
3496.301904	862238.494865	45.899943
3495.688622	860446.714209	45.904948
3495.609363	858578.561928	45.909953
3494.891515	856647.004512	45.914957
3494.460334	854632.953607	45.919962
3493.616070	852548.030501	45.924967
3493.317551	850384.315760	45.929972
3492.840839	848143.700825	45.934977
3492.407132	845838.933646	45.939981
3491.495757	843455.020687	45.944986
3490.537932	840993.561118	45.949991
3490.117711	838448.958691	45.954996
3489.715298	835849.314834	45.960001
3488.496363	833169.855804	45.965005
3488.055147	830415.793747	45.970010
3487.199199	827596.716813	45.975015
3486.550075	824689.371855	45.980020
3485.836765	821723.528029	45.985025
3484.847475	818678.452831	45.990029
3484.216143	815555.851377	45.995034
3483.189954	812378.033439	46.000039
3482.503241	809117.370764	46.005044
3481.464258	805788.919583	46.010049
3480.362665	802386.561330	46.015053
3479.608606	798906.451276	46.020058
3478.491960	795369.322377	46.025063
3477.772251	791743.587903	46.030068
3476.784624	788054.252669	46.035073
3475.505097	784300.450951	46.040077
3474.841023	780466.893553	46.045082
3473.409203	776577.968474	46.050087
3472.255359	772614.126124	46.055092
3471.220362	768568.934254	46.060097
3469.926544	764462.115368	46.065101
3468.648113	760290.634030	46.070106
3467.546964	756052.454304	46.075111
3466.465860	751745.489976	46.080116
3465.096669	747369.701530	46.085121
3463.820983	742923.551612	46.090125
3462.804861	738409.444063	46.095130
3461.124967	733825.067690	46.100135
3459.763740	729173.637021	46.105140
3458.586290	724446.318081	46.110145
3456.619612	719664.247538	46.115149
3455.515139	714819.153254	46.120154
3454.032228	709911.661973	46.125159
3452.525230	704934.738274	46.130164
3451.359629	699881.081418	46.135169
3449.380318	694762.921750	46.140173
3448.259368	689583.842564	46.145178
3446.307103	684330.116974	46.150183
3444.273976	679014.387505	46.155188
3443.117048	673649.144316	46.160193
3440.898106	668209.030661	46.165197
3439.420418	662696.661203	46.170202
3437.623039	657134.605293	46.175207
3435.799351	651516.034466	46.180212
3433.955018	645816.057518	46.185217
3431.898288	640086.990055	46.190221
3430.673799	634276.566533	46.195226
3428.472851	628418.303854	46.200231
3426.760854	622496.907034	46.205236
3424.764439	616508.748184	46.210241
3422.560796	610469.714905	46.215245
3420.565573	604361.851982	46.220250
3417.761952	598210.886618	46.225255
3416.350922	591993.342485	46.230260
3414.235484	585750.038714	46.235265
3411.754380	579422.610609	46.240269
3409.880954	573046.157815	46.245274
3407.470364	566611.551940	46.250279
3405.103888	560130.013769	46.255284
3403.027399	553588.153238	46.260289
3400.318753	547006.930308	46.265293
3398.139106	540385.214794	46.270298
3395.185622	533691.652745	46.275303
3393.246121	526961.823296	46.280308
3390.573630	520165.185679	46.285313
3387.963504	513349.452996	46.290317
3385.562837	506461.984731	46.295322
3382.996505	499544.456870	46.300327
3380.515120	492577.195695	46.305332
3378.007955	485563.940851	46.310337
3375.189779	478510.039217	46.315341
3372.258666	471411.499447	46.320346
3369.241664	464274.641391	46.325351
3366.556547	457090.525473	46.330356
3363.581105	449869.743894	46.335361
3360.502671	442629.417569	46.340365
3357.809613	435332.146645	46.345370
3354.711422	428014.446343	46.350375
3351.416214	420659.658112	46.355380
3348.740517	413278.430129	46.360385
3345.457592	405860.044520	46.365389
3342.481500	398400.331561	46.370394
3339.081691	390923.752703	46.375399
3335.819773	383410.530549	46.380404
3332.951661	375858.261562	46.385409
3329.300017	368291.786505	46.390413
3326.265944	360693.956317	46.395418
3322.519400	353076.045033	46.400423
3319.269744	345428.893080	46.405428
3315.799302	337769.790203	46.410433
3312.229959	330092.483755	46.415437
3308.562521	322386.004002	46.420442
3304.806281	314682.553675	46.425447
3300.776819	306955.516975	46.430452
3297.507680	299210.406006	46.435457
3293.717945	291463.558577	46.440461
3289.807429	283702.441859	46.445466
3285.919533	275933.409159	46.450471
3282.251940	268164.716804	46.455476
3278.360181	260375.897949	46.460481
3273.918930	252584.617671	46.465485
3270.318337	244794.251474	46.470490
3266.108422	236999.143730	46.475495
3261.975777	229189.875230	46.480500
3258.081003	221320.575433	46.485505
3253.581557	213521.879475	46.490509
3249.464100	205730.342440	46.495514
3245.396073	197957.843230	46.500519
3240.965945	190178.608520	46.505524
3236.514830	182412.182359	46.510529
3231.605288	174668.060155	46.515533
3227.290747	166923.668716	46.520538
3222.488603	159203.683103	46.525543
3217.859472	151500.579416	46.530548
3212.875385	143822.303217	46.535553
3208.042633	136175.528163	46.540557
3203.574139	128538.934399	46.545562
3198.067774	120945.240956	46.550567
3193.010662	113379.571570	46.555572
3187.608301	105855.768135	46.560577
3181.980332	98366.037999	46.565581
3176.791228	90898.501118	46.570586
3170.836808	83513.904439	46.575591
3165.003160	76158.993256	46.580596
3159.291071	68868.482244	46.585601
3152.624234	61640.485145	46.590605
3146.525529	54471.811547	46.595610
3139.227240	47388.360082	46.600615
3131.451832	40398.865640	46.605620
3122.058463	33547.603021	46.610625
3102.441870	27090.206535	46.615629
3077.065411	21008.611120	46.620634
3045.963963	15420.829809	46.625639
3010.709187	10403.241832	46.630644
2975.049980	5993.161516	46.635649
2939.892105	2246.693715	46.640653
2864.331476	347.404032	46.645658
2758.528848	311.021023	46.650663
2710.241996	306.038515	46.655668
2713.376629	308.800784	46.660673
2745.977457	311.286886	46.665677
2786.815824	305.945154	46.670682
2820.111293	303.628644	46.675687
2839.873316	295.362874	46.680692
2846.926897	289.888858	46.685697
2844.275748	288.254209	46.690701
2838.057327	280.517781	46.695706
2831.278815	287.528842	46.700711
2825.320467	294.285009	46.705716
2822.451864	286.260368	46.710721
2819.548793	287.837806	46.715725
2817.119276	274.944117	46.720730
2814.958299	285.336775	46.725735
2812.617336	284.759244	46.730740
2810.320401	277.893424	46.735745
2807.701896	280.474966	46.740749
2805.097761	275.296595	46.745754
2802.320568	267.510679	46.750759
2798.794843	273.433330	46.755764
2795.462180	269.488575	46.760769
2792.083298	276.911278	46.765773
2789.780795	268.305040	46.770778
2786.282647	267.685190	46.775783
2782.964480	258.983679	46.780788
2779.775782	262.571426	46.785793
2776.107698	265.095265	46.790797
2773.063600	259.421164	46.795802
2770.170008	262.536334	46.800807
2767.138591	256.614652	46.805812
2763.955842	249.639665	46.810817
2760.186685	253.885622	46.815821
2756.979171	250.372163	46.820826
2753.598314	259.217256	46.825831
2750.490804	258.329319	46.830836
2747.084235	248.706629	46.835841
2744.031681	256.708581	46.840845
2740.312799	250.758660	46.845850
2736.833441	254.675406	46.850855
2733.420770	247.205555	46.855860
2730.295920	247.614663	46.860865
2726.540982	252.573465	46.865869
2723.625605	257.151797	46.870874
2720.467499	259.199998	46.875879
2716.540502	256.661749	46.880884
2713.351684	247.506379	46.885889
2709.788682	254.152372	46.890893
2706.844361	248.791811	46.895898
2702.850447	250.902158	46.900903
2699.543635	252.496156	46.905908
2696.353129	244.382651	46.910913
2692.712038	253.037063	46.915917
2689.808391	248.896480	46.920922
2686.602726	242.100572	46.925927
2682.965504	257.664089	46.930932
2679.550284	242.945140	46.935937
2675.233033	249.171346	46.940941
2671.988997	248.417683	46.945946
2668.812880	241.339450	46.950951
2665.635700	251.360290	46.955956
2662.379196	249.716310	46.960961
2658.660443	253.281084	46.965965
2655.423842	247.446226	46.970970
2651.267441	243.906290	46.975975
2648.194233	250.570562	46.980980
2645.005902	230.979333	46.985985
2640.916107	241.838320	46.990989
2637.430503	233.395453	46.995994
2634.184348	245.422420	47.000999
2630.884727	234.114642	47.006004
2627.392874	239.471745	47.011009
2623.846726	247.740316	47.016013
2620.426085	236.521191	47.021018
2617.454843	241.127739	47.026023
2614.074454	240.518574	47.031028
2610.896338	238.420832	47.036033
2607.167467	232.411497	47.041037
2603.274954	240.664222	47.046042
2599.805068	232.960007	47.051047
2596.540765	234.950027	47.056052
2592.970357	247.286282	47.061057
2588.890651	242.930563	47.066061
2585.644839	240.937154	47.071066
2582.611841	238.453557	47.076071
2578.903233	237.113952	47.081076
2575.388723	231.963224	47.086081
2572.016393	235.514299	47.091085
2568.849615	227.598662	47.096090
2565.042907	230.063823	47.101095
2561.600203	229.404197	47.106100
2558.260855	230.116801	47.111105
2554.906723	228.356789	47.116109
2551.192068	228.407883	47.121114
2547.930566	225.555499	47.126119
2544.089530	227.099624	47.131124
2541.077275	215.995916	47.136129
2537.307787	219.959879	47.141133
2534.199957	220.364720	47.146138
2530.889472	225.804431	47.151143
2526.889387	227.138404	47.156148
2523.789464	222.464746	47.161153
2519.334920	226.041329	47.166157
2516.029943	228.957329	47.171162
2513.354913	223.153432	47.176167
2509.629971	232.975447	47.181172
2506.040539	220.299092	47.186177
2502.548322	217.044354	47.191181
2499.015855	217.591529	47.196186
2495.297795	221.625575	47.201191
2491.853193	224.385449	47.206196
2488.605619	214.130903	47.211201
2485.024050	222.876251	47.216205
2481.676177	222.509672	47.221210
2477.968552	221.457312	47.226215
2474.414377	226.426166	47.231220
2471.386244	214.816778	47.236225
2467.717581	215.954404	47.241229
2464.085052	216.320384	47.246234
2460.485460	218.001143	47.251239
2457.072901	222.420521	47.256244
2453.636471	216.848902	47.261249
2450.485175	214.885771	47.266253
2447.210292	210.396354	47.271258
2443.456180	215.359351	47.276263
2439.885550	212.145033	47.281268
2436.629429	210.284071	47.286273
2432.683270	212.708012	47.291277
2429.309663	211.757048	47.296282
2425.932392	208.592130	47.301287
2422.317673	215.586255	47.306292
2418.855615	208.908063	47.311297
2414.896825	220.667941	47.316301
2411.705071	212.068815	47.321306
2408.483639	212.320010	47.326311
2404.748662	216.422824	47.331316
2401.540330	203.322532	47.336321
2397.564423	211.604542	47.341325
2394.288565	208.608999	47.346330
2390.319121	209.112347	47.351335
2387.236186	205.419530	47.356340
2384.395225	207.478925	47.361345
2380.409388	217.427950	47.366349
2377.092156	209.965133	47.371354
2373.672858	205.666165	47.376359
2369.919391	213.974430	47.381364
2366.715049	206.578632	47.386369
2362.813471	217.267406	47.391373
2359.600159	215.955141	47.396378
2355.768622	208.098294	47.401383
2352.391569	203.446233	47.406388
2348.859989	209.904121	47.411393
2344.932522	208.648189	47.416397
2341.989032	211.189666	47.421402
2338.361833	211.441190	47.426407
2335.083553	202.426799	47.431412
2331.708617	208.001195	47.436417
2328.016747	211.346262	47.441421
2324.664948	204.882804	47.446426
2320.996058	205.512026	47.451431
2317.286709	199.883349	47.456436
2313.895629	205.553961	47.461441
2310.624245	205.759395	47.466445
2306.903644	198.388882	47.471450
2303.627143	204.670496	47.476455
2300.017909	207.476618	47.481460
2297.369155	201.230821	47.486465
2293.256373	206.249779	47.491469
2289.315140	202.445931	47.496474
2285.690944	197.262040	47.501479
2282.389124	198.524540	47.506484
2279.348260	189.530798	47.511489
2275.544147	194.155632	47.516493
2272.101832	194.034691	47.521498
2268.345063	201.273582	47.526503
2265.036885	197.498644	47.531508
2261.924404	195.082454	47.536513
2257.904534	200.407566	47.541517
2254.610566	192.212231	47.546522
2250.804267	195.571308	47.551527
2247.581133	200.397045	47.556532
2243.923706	197.028484	47.561537
2240.326888	201.777586	47.566541
2237.230743	191.978772	47.571546
2233.622291	196.670991	47.576551
2229.895242	191.762643	47.581556
2226.813447	194.261896	47.586561
2222.938731	199.433812	47.591565
2219.942384	187.558894	47.596570
2216.436180	191.459878	47.601575
2212.507694	198.705649	47.606580
2209.154172	186.744075	47.611585
2205.477982	197.007363	47.616589
2202.346855	190.004943	47.621594
2198.881918	194.045552	47.626599
2194.745794	186.626526	47.631604
2191.444032	189.382745	47.636609
2187.719013	199.095241	47.641613
2184.593273	189.680445	47.646618
2181.207775	191.664491	47.651623
2177.644790	187.016031	47.656628
2174.396137	183.564247	47.661633
2170.932274	197.116300	47.666637
2167.529120	190.560804	47.671642
2163.783571	191.904740	47.676647
2160.053334	197.903974	47.681652
2156.373462	184.842679	47.686657
2152.987669	185.299577	47.691661
2149.562737	186.764243	47.696666
2145.863458	186.722131	47.701671
2142.278766	192.454615	47.706676
2139.341175	188.539445	47.711681
2135.611474	193.900803	47.716685
2131.830094	190.588320	47.721690
2128.674273	193.607020	47.726695
2125.320001	184.789270	47.731700
2121.886033	181.672619	47.736705
2118.225522	193.219437	47.741709
2114.305373	189.670579	47.746714
2111.022151	189.252928	47.751719
2108.044798	189.331403	47.756724
2104.765727	189.098176	47.761729
2100.597914	182.008505	47.766733
2096.775716	184.382239	47.771738
2093.648735	181.671758	47.776743
2090.025528	190.166885	47.781748
2086.749143	172.522118	47.786753
2083.311293	183.038380	47.791757
2079.556438	181.082813	47.796762
2076.092691	181.605919	47.801767
2072.529804	178.364760	47.806772
2069.092285	180.329251	47.811777
2065.445735	182.520275	47.816781
2062.212776	175.881506	47.821786
2058.513310	179.160723	47.826791
2055.075033	178.747206	47.831796
2051.462745	175.475149	47.836801
2048.334363	182.873468	47.841805
2044.766368	173.792704	47.846810
2041.137208	189.276056	47.851815
2037.750590	185.070422	47.856820
2034.480002	183.524124	47.861825
2030.159696	186.054171	47.866829
2027.009295	186.061223	47.871834
2023.619049	185.683408	47.876839
2020.051264	182.703192	47.881844
2016.679965	181.933889	47.886849
2013.111338	193.160512	47.891853
2009.556683	189.602887	47.896858
2005.870063	183.231287	47.901863
2002.557189	189.801281	47.906868
1999.523053	180.757498	47.911873
1995.681373	187.602893	47.916877
1992.431174	181.640936	47.921882
1988.559296	189.680690	47.926887
1985.195297	187.384569	47.931892
1981.482330	176.341969	47.936897
1977.816064	188.072757	47.941901
1974.590462	179.070877	47.946906
1971.230815	176.120460	47.951911
1967.328029	188.258356	47.956916
1964.125853	179.687946	47.961921
1960.360351	176.641959	47.966925
1956.905724	180.234840	47.971930
1953.435990	197.623680	47.976935
1950.296689	181.338550	47.981940
1947.080423	178.186271	47.986945
1943.298826	178.951217	47.991949
1939.791433	172.523040	47.996954
1936.574458	171.631609	48.001959
1932.720185	182.757252	48.006964
1929.006155	189.344410	48.011969
1925.408713	185.988299	48.016973
1921.866065	181.435946	48.021978
1918.639947	177.707505	48.026983
1915.267597	177.578025	48.031988
1911.718709	174.659501	48.036993
1907.893814	180.158499	48.041997
1904.568499	181.665886	48.047002
1901.371466	174.063023	48.052007
1897.748113	180.973266	48.057012
1894.099215	182.207707	48.062017
1890.358402	187.439252	48.067021
1886.444143	182.238081	48.072026
1883.253005	175.830135	48.077031
1880.220084	180.903712	48.082036
1877.171016	178.973815	48.087041
1873.047645	185.419445	48.092045
1869.830330	172.768853	48.097050
1866.193262	175.348005	48.102055
1862.657951	175.506561	48.107060
1859.093963	166.200724	48.112065
1855.339371	180.618150	48.117069
1851.944220	175.089920	48.122074
1848.539035	176.634416	48.127079
1844.821979	178.526834	48.132084
1841.687300	167.115528	48.137089
1838.165950	172.411892	48.142093
1834.608745	173.656097	48.147098
1831.173505	178.034429	48.152103
1827.597524	178.481529	48.157108
1824.264934	173.280240	48.162113
1820.249750	175.477281	48.167117
1816.860657	174.456098	48.172122
1813.691531	173.007849	48.177127
1809.879459	181.979554	48.182132
1806.790821	171.103745	48.187137
1803.175642	171.879396	48.192141
1799.702310	167.051457	48.197146
1796.609261	168.738214	48.202151
1792.493431	178.149063	48.207156
1788.559411	168.900859	48.212161
1785.139346	174.644473	48.217165
1782.110634	170.312421	48.222170
1778.782311	160.546604	48.227175
1775.077516	172.210466	48.232180
1771.964669	161.174899	48.237185
1767.845151	170.361603	48.242189
1764.207287	167.260554	48.247194
1760.756900	165.403546	48.252199
1757.360035	166.920879	48.257204
1754.308202	164.960737	48.262209
1750.301065	165.843411	48.267213
1747.312007	159.787986	48.272218
1743.708198	159.730612	48.277223
1739.593429	170.168471	48.282228
1736.205874	163.944842	48.287233
1732.807150	167.819714	48.292237
1729.469934	157.935031	48.297242
1726.318135	165.554469	48.302247
1722.623987	173.443881	48.307252
1719.342824	159.730447	48.312257
1715.724943	163.414005	48.317261
1711.830766	157.838486	48.322266
1708.397035	156.870146	48.327271
1704.425428	165.971087	48.332276
1701.853966	157.402266	48.337281
1697.976392	162.011438	48.342285
1694.410906	166.065641	48.347290
1690.995807	156.300816	48.352295
1687.353098	158.965886	48.357300
1684.026876	159.150219	48.362305
1680.073675	160.179938	48.367309
1676.887480	162.581726	48.372314
1673.502134	162.136456	48.377319
1669.759515	159.080223	48.382324
1666.862417	160.572870	48.387329
1663.137209	165.138543	48.392333
1659.625519	160.799548	48.397338
1655.938914	161.842468	48.402343
1652.182104	164.926818	48.407348
1649.030121	156.656613	48.412353
1645.280933	164.839929	48.417357
1642.194712	161.064896	48.422362
1638.536019	155.896521	48.427367
1634.798374	151.171788	48.432372
1631.462887	153.016714	48.437377
1627.864127	165.485262	48.442381
1624.264973	157.128722	48.447386
1620.912745	155.803414	48.452391
1617.549611	161.459779	48.457396
1614.082893	157.161147	48.462401
1610.186052	164.559599	48.467405
1606.668069	156.710636	48.472410
1603.549068	154.893912	48.477415
1599.904407	157.924249	48.482420
1596.430950	156.484800	48.487425
1592.854265	156.066469	48.492429
1589.458947	161.365265	48.497434
1585.779613	158.745618	48.502439
1582.323967	158.905428	48.507444
1578.844918	150.366083	48.512449
1575.212295	157.430220	48.517453
1571.862547	156.218205	48.522458
1568.315107	152.690334	48.527463
1564.909942	156.916856	48.532468
1561.450222	152.626977	48.537473
1557.850212	160.258414	48.542477
1554.656611	152.919297	48.547482
1551.075167	156.807119	48.552487
1547.041546	155.900928	48.557492
1543.690575	156.360791	48.562497
1540.016585	158.011295	48.567501
1536.861161	158.833723	48.572506
1533.286662	149.346389	48.577511
1529.870323	160.456763	48.582516
1526.870492	156.302658	48.587521
1522.957298	154.841011	48.592525
1519.301453	151.678606	48.597530
1516.106702	142.921838	48.602535
1512.392724	159.951433	48.607540
1508.991402	151.119476	48.612545
1505.115022	160.022289	48.617549
1501.697018	149.235104	48.622554
1498.224202	149.875570	48.627559
1494.566290	159.345156	48.632564
1491.303683	146.207261	48.637569
1487.682641	158.766403	48.642573
1484.316314	155.873896	48.647578
1481.357737	158.485658	48.652583
1477.072034	150.405315	48.657588
1473.747111	157.152463	48.662593
1470.070884	152.740565	48.667597
1466.604297	151.428547	48.672602
1463.355861	154.525525	48.677607
1459.690514	158.723090	48.682612
1456.404242	146.183913	48.687617
1453.100467	164.403196	48.692621
1449.413417	152.051222	48.697626
1445.831689	156.742729	48.702631
1441.805475	156.383415	48.707636
1438.804152	149.817554	48.712641
1435.009682	159.857561	48.717645
1431.815914	158.437135	48.722650
1428.383961	151.678807	48.727655
1424.917474	155.899773	48.732660
1421.326264	153.179657	48.737665
1417.459674	156.939467	48.742669
1414.178047	156.571179	48.747674
1410.773383	151.502504	48.752679
1407.213248	157.056193	48.757684
1403.891869	145.035350	48.762689
1400.488109	151.616390	48.767693
1396.873155	154.201116	48.772698
1393.196774	147.926241	48.777703
1389.291446	151.214522	48.782708
1386.177469	146.375873	48.787713
1382.761935	154.230716	48.792717
1379.489165	150.257792	48.797722
1376.097945	148.200869	48.802727
1372.060364	152.888048	48.807732
1368.372305	150.661936	48.812737
1364.884051	149.712338	48.817741
1361.836867	146.575166	48.822746
1358.248668	143.052230	48.827751
1354.676117	144.593362	48.832756
1351.511634	139.889582	48.837761
1347.751882	152.402670	48.842765
1344.176928	143.810113	48.847770
1341.001397	153.711965	48.852775
1336.941947	150.699501	48.857780
1333.571965	143.764063	48.862785
1329.883700	154.238294	48.867789
1326.898472	141.049168	48.872794
1323.260117	147.999773	48.877799
1319.386653	155.784519	48.882804
1316.079784	138.651883	48.887809
1312.710485	149.227519	48.892813
1309.024507	143.923235	48.897818
1306.065911	136.633879	48.902823
1302.178202	146.197422	48.907828
1299.094514	139.612326	48.912833
1295.035739	141.038511	48.917837
1291.616363	144.455326	48.922842
1288.127231	147.255351	48.927847
1284.404480	144.185111	48.932852
1281.306508	144.655438	48.937857
1277.457842	140.464025	48.942861
1274.110886	140.414879	48.947866
1270.735236	141.363087	48.952871
1266.584673	146.503763	48.957876
1263.794265	130.422082	48.962881
1259.639707	146.927902	48.967885
1256.611297	149.600285	48.972890
1253.190038	139.196694	48.977895
1249.530833	151.352622	48.982900
1246.407265	149.994725	48.987905
1242.555763	145.765329	48.992909
1238.871836	148.071490	48.997914
1235.479836	146.071833	49.002919
1232.278004	140.797893	49.007924
1228.909591	142.757672	49.012929
1224.958273	153.311771	49.017933
1221.285177	152.789292	49.022938
1218.005142	146.508841	49.027943
1214.477816	137.101417	49.032948
1211.212561	149.567776	49.037953
1207.293144	142.547642	49.042957
1204.242859	140.606961	49.047962
1200.805791	136.208252	49.052967
1196.776803	140.929476	49.057972
1193.881383	142.659530	49.062977
1190.176689	151.724424	49.067981
1186.395267	143.382224	49.072986
1183.389690	147.607675	49.077991
1179.263857	145.052513	49.082996
1176.141630	129.849446	49.088001
1172.677817	148.694433	49.093005
1168.988664	145.576308	49.098010
1165.590840	139.611776	49.103015
1161.778382	143.454799	49.108020
1158.782571	136.646103	49.113025
1154.843583	147.353517	49.118029
1150.837192	141.927305	49.123034
1147.686123	144.640954	49.128039
1144.480829	141.853118	49.133044
1141.555834	139.174247	49.138049
1137.717845	135.592151	49.143053
1133.839199	143.554111	49.148058
1130.786717	143.227670	49.153063
1126.829856	145.843279	49.158068
1123.783996	138.962171	49.163073
1119.983773	141.220953	49.168077
1116.693845	142.623777	49.173082
1112.945732	143.189871	49.178087
1108.975049	138.724750	49.183092
1105.914894	150.428296	49.188097
1102.367663	140.451586	49.193101
1099.040030	144.239362	49.198106
1095.495305	140.001606	49.203111
1091.920655	141.735098	49.208116
1088.704709	149.212779	49.213121
1085.044911	154.101377	49.218125
1081.265805	141.777806	49.223130
1078.105317	143.503412	49.228135
1074.511976	148.520743	49.233140
1070.991706	137.314929	49.238145
1067.385633	150.747847	49.243149
1063.714934	145.888020	49.248154
1060.567096	144.995839	49.253159
1056.632926	143.652524	49.258164
1053.437030	143.583694	49.263169
1049.616427	144.193993	49.268173
1046.215926	138.027534	49.273178
1042.930304	142.931645	49.278183
1039.431979	147.412319	49.283188
1036.251458	140.351076	49.288193
1032.495677	145.139548	49.293197
1028.861948	143.709873	49.298202
1025.286365	143.263192	49.303207
1021.587850	148.115219	49.308212
1018.525443	148.548467	49.313217
1014.995097	147.063227	49.318221
1011.469587	150.170214	49.323226
1007.766808	138.291524	49.328231
1004.073735	149.755828	49.333236
1000.767008	138.318810	49.338241
997.479860	146.973203	49.343245
993.984732	137.199522	49.348250
990.725921	142.401555	49.353255
986.943096	155.075988	49.358260
983.614919	143.600099	49.363265
979.634413	144.423975	49.368269
976.070747	142.934607	49.373274
972.816476	144.730851	49.378279
969.399583	146.835985	49.383284
965.777225	137.532311	49.388289
962.360412	148.720863	49.393293
958.796687	148.972821	49.398298
955.427864	140.034531	49.403303
951.385152	146.735747	49.408308
948.499251	149.577559	49.413313
944.852994	144.036928	49.418317
941.393166	133.447784	49.423322
937.670241	138.095719	49.428327
934.436876	140.294454	49.433332
931.038194	130.230388	49.438337
926.993801	136.307920	49.443341
923.669870	134.171150	49.448346
920.468992	137.978344	49.453351
916.886216	140.103451	49.458356
913.501897	136.260240	49.463361
909.624328	145.434043	49.468365
906.139445	137.392745	49.473370
902.868661	138.049781	49.478375
899.234087	146.113838	49.483380
895.968177	140.062984	49.488385
892.311822	139.983397	49.493389
888.667767	141.218016	49.498394
885.132663	136.337698	49.503399
881.589254	146.397356	49.508404
878.446329	145.462658	49.513409
874.906932	133.586283	49.518413
871.037540	139.525200	49.523418
867.892516	139.005856	49.528423
864.409930	138.693505	49.533428
861.071864	127.162736	49.538433
856.790911	133.254587	49.543437
853.641969	136.969565	49.548442
850.398848	138.460350	49.553447
846.794915	137.705723	49.558452
843.022005	142.753518	49.563457
839.300746	143.686588	49.568461
836.084701	133.776903	49.573466
833.202822	133.383375	49.578471
829.154732	135.617877	49.583476
825.896273	126.191395	49.588481
822.347781	133.554139	49.593485
818.666721	125.299097	49.598490
815.229504	129.651422	49.603495
811.400605	136.430263	49.608500
808.152478	124.370603	49.613505
804.383125	138.126302	49.618509
800.727431	133.589241	49.623514
797.985548	130.815394	49.628519
794.193394	131.450607	49.633524
790.914891	131.706631	49.638529
786.991203	139.399250	49.643533
783.606870	140.167705	49.648538
780.649851	144.009645	49.653543
776.713561	144.337189	49.658548
773.283438	135.813342	49.663553
769.346169	139.159516	49.668557
765.838162	139.878191	49.673562
762.975892	137.684123	49.678567
759.132444	138.700225	49.683572
755.825653	129.686334	49.688577
751.869724	136.219633	49.693581
748.318407	137.129798	49.698586
745.238150	137.458242	49.703591
741.548348	138.326003	49.708596
738.313845	132.303235	49.713601
734.792059	142.966028	49.718605
731.099111	138.502086	49.723610
727.573507	133.505087	49.728615
724.036072	142.852071	49.733620
720.652981	140.212564	49.738625
717.327404	135.893486	49.743629
713.603882	131.781735	49.748634
710.142238	129.731455	49.753639
706.549794	135.993905	49.758644
702.913290	126.656904	49.763649
698.999315	131.600272	49.768653
695.827575	132.754740	49.773658
692.635382	133.699274	49.778663
688.960496	136.751295	49.783668
685.740238	127.466612	49.788673
682.344636	126.778298	49.793677
678.481159	130.987724	49.798682
675.267473	129.042875	49.803687
671.453044	135.212031	49.808692
668.356717	127.452991	49.813697
664.465242	146.961422	49.818701
660.992090	141.367539	49.823706
657.784817	129.231390	49.828711
654.017475	135.052562	49.833716
650.585724	131.525256	49.838721
646.927004	131.313062	49.843725
643.320402	138.380074	49.848730
639.850869	131.630605	49.853735
636.452115	132.742358	49.858740
633.426931	119.174038	49.863745
629.650328	121.700653	49.868749
626.071130	123.232006	49.873754
622.206779	125.361306	49.878759
618.602211	127.876241	49.883764
615.428835	135.968786	49.888769
611.848616	139.329036	49.893773
608.484269	136.762689	49.898778
605.185923	133.074818	49.903783
601.561840	132.979871	49.908788
598.029816	128.850747	49.913793
594.258506	133.661275	49.918797
590.848770	132.555835	49.923802
587.484669	128.951083	49.928807
583.877591	128.662316	49.933812
580.843712	132.383697	49.938817
577.328207	139.778855	49.943821
573.408228	128.269041	49.948826
569.900302	124.409464	49.953831
566.361022	132.089763	49.958836
563.282084	128.073763	49.963841
559.428180	132.037995	49.968845
555.512447	138.915276	49.973850
552.362513	127.497508	49.978855
548.690206	142.825692	49.983860
545.439052	131.070851	49.988865
541.905192	132.256733	49.993869
538.983877	131.801646	49.998874
535.428792	124.952367	50.003879
531.091350	130.444289	50.008884
528.129089	130.916163	50.013889
524.445952	129.609345	50.018893
520.732144	131.937008	50.023898
517.675524	123.380793	50.028903
513.872724	137.996105	50.033908
510.135803	129.848863	50.038913
506.742724	135.820556	50.043917
503.386535	134.558519	50.048922
499.900369	126.637777	50.053927
496.209451	131.939275	50.058932
492.985811	127.747568	50.063937
489.213771	126.541925	50.068941
485.735974	120.316705	50.073946
482.404679	125.059245	50.078951
478.918680	127.622358	50.083956
475.397401	116.769123	50.088961
472.080377	117.334867	50.093965
468.254306	119.049873	50.098970
465.078485	120.264184	50.103975
461.180434	131.456124	50.108980
457.900461	129.650677	50.113985
454.368922	120.731666	50.118989
450.942972	124.811847	50.123994
447.495002	127.912351	50.128999
443.718722	127.744252	50.134004
440.405946	123.115440	50.139009
436.803469	124.338416	50.144013
433.323104	130.171472	50.149018
430.042526	119.831378	50.154023
426.247667	131.093489	50.159028
422.553140	121.976122	50.164033
419.157260	123.257867	50.169037
415.768153	120.467655	50.174042
412.612906	116.157544	50.179047
409.014612	130.501092	50.184052
405.170265	115.413680	50.189057
401.397247	126.603914	50.194061
398.019155	118.702874	50.199066
394.811145	108.341929	50.204071
390.822727	119.032641	50.209076
387.992525	122.290247	50.214081
384.445214	121.661612	50.219085
380.478563	126.640607	50.224090
377.411737	112.651972	50.229095
373.846566	118.115484	50.234100
370.507234	114.282640	50.239105
366.995954	122.542166	50.244109
363.312521	115.997858	50.249114
360.000519	118.462408	50.254119
356.276404	123.505474	50.259124
352.677242	119.166068	50.264129
349.044990	128.088945	50.269133
345.735769	118.429541	50.274138
342.275330	116.549073	50.279143
338.652430	116.918481	50.284148
335.566260	113.197883	50.289153
332.034492	122.998858	50.294157
328.183299	124.095748	50.299162
324.848911	113.153311	50.304167
320.467764	121.951519	50.309172
317.671957	120.951686	50.314177
314.464465	114.481385	50.319181
310.814476	119.002895	50.324186
307.736551	112.991666	50.329191
303.292812	119.318560	50.334196
300.374766	112.503767	50.339201
296.435865	113.108840	50.344205
292.774882	120.622407	50.349210
289.974245	123.622591	50.354215
285.848481	123.765266	50.359220
282.608539	118.544560	50.364225
279.441269	121.749493	50.369229
275.720560	130.677202	50.374234
271.973247	126.098550	50.379239
268.461892	130.314368	50.384244
265.485512	122.040682	50.389249
261.620297	123.119232	50.394253
258.203764	126.577774	50.399258
254.744691	122.580927	50.404263
251.000928	132.843105	50.409268
247.761950	118.199503	50.414273
244.429487	126.557788	50.419277
240.898317	124.206626	50.424282
237.158362	112.675462	50.429287
233.159811	121.051266	50.434292
229.878253	119.113455	50.439297
226.493999	123.585519	50.444301
223.298111	128.841794	50.449306
220.189079	117.306249	50.454311
216.337615	128.538027	50.459316
212.622083	121.136026	50.464321
208.867919	123.592584	50.469325
204.696340	127.637727	50.474330
202.000124	117.788366	50.479335
198.264646	126.842109	50.484340
194.996160	117.790793	50.489345
191.850242	122.293283	50.494349
188.091145	123.956204	50.499354
184.622284	130.538599	50.504359
181.271967	124.618341	50.509364
177.794010	114.961169	50.514369
174.191715	121.369113	50.519373
170.516910	128.345749	50.524378
167.279520	121.610561	50.529383
163.576327	122.883193	50.534388
160.398221	116.411507	50.539393
156.227226	107.449656	50.544397
153.039699	116.741078	50.549402
149.797711	121.953925	50.554407
145.537610	120.129838	50.559412
142.568357	114.701237	50.564417
139.222169	125.527172	50.569421
135.314914	120.583814	50.574426
131.945343	114.120961	50.579431
128.626959	117.035282	50.584436
125.201382	116.475116	50.589441
121.509010	122.565309	50.594445
117.722228	119.591751	50.599450
115.053411	117.167780	50.604455
110.882290	115.037336	50.609460
107.283897	115.593903	50.614465
104.026487	116.390610	50.619469
100.617912	119.919389	50.624474
97.222584	114.992544	50.629479
93.091627	112.144669	50.634484
90.179753	113.894136	50.639489
86.868105	116.149854	50.644493
82.815754	115.765131	50.649498
79.706766	118.283697	50.654503
75.737416	122.688962	50.659508
72.146506	119.427467	50.664513
68.683147	111.335609	50.669517
65.532474	115.541195	50.674522
62.356499	115.011385	50.679527
58.452086	114.992124	50.684532
55.278931	114.225445	50.689537
51.602374	119.908340	50.694541
48.012898	121.322084	50.699546
44.481102	109.939972	50.704551
40.542223	120.889171	50.709556
37.177211	113.403451	50.714561
33.763452	125.536543	50.719565
30.627064	118.988593	50.724570
27.160383	114.337459	50.729575
23.774393	118.901919	50.734580
20.082040	114.073658	50.739585
16.336675	115.536132	50.744589
12.806243	119.708339	50.749594
9.245701	112.084130	50.754599
5.978820	119.532266	50.759604
2.682367	110.521075	50.764609