Tue Jun 21 13:04:05 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.501601	114.954226	0.000000
0.465498	117.306754	0.005005
0.753661	113.847952	0.010010
0.837739	96.473762	0.015014
0.570489	94.592074	0.020019
-0.063331	62.900214	0.025024
-0.433124	70.324024	0.030029
-0.535468	49.670674	0.035034
-0.673128	26.592247	0.040038
-0.924242	37.341391	0.045043
-0.844077	11.511803	0.050048
-1.389395	6.820364	0.055053
-1.768443	-15.515719	0.060058
-2.384919	-14.662545	0.065062
-2.976099	-8.028148	0.070067
-2.993674	-8.816896	0.075072
-3.935871	-2.485491	0.080077
-4.293195	1.400012	0.085082
-3.316524	-4.934453	0.090086
-4.232362	1.092444	0.095091
-4.171835	-4.891206	0.100096
-4.542966	3.295487	0.105101
-4.667669	3.418792	0.110106
-5.639278	-5.758674	0.115110
-5.931103	0.205938	0.120115
-6.238318	0.087146	0.125120
-5.974658	3.052662	0.130125
-6.072561	1.244571	0.135130
-6.081983	-4.865827	0.140134
-6.427967	5.174989	0.145139
-6.139039	2.136799	0.150144
-6.735779	0.917076	0.155149
-7.398123	-1.576817	0.160154
-7.549272	-5.484595	0.165158
-7.879000	-0.254299	0.170163
-8.314279	-5.443869	0.175168
-8.630661	0.661561	0.180173
-9.201222	-1.540085	0.185178
-9.170457	-3.659957	0.190182
-9.763424	-0.994024	0.195187
-9.377426	-5.060014	0.200192
-9.255304	0.137295	0.205197
-9.197848	1.041476	0.210202
-9.481407	3.758786	0.215206
-10.347395	5.577195	0.220211
-10.773901	2.124873	0.225216
-10.775001	-0.614085	0.230221
-11.119774	3.452663	0.235226
-11.719519	-6.292736	0.240230
-12.208005	2.674109	0.245235
-12.500876	-5.099441	0.250240
-12.538614	-0.905148	0.255245
-12.150742	-1.428529	0.260250
-12.607109	-5.011275	0.265254
-12.625891	-2.052072	0.270259
-12.275932	1.495494	0.275264
-13.266654	-3.902637	0.280269
-13.360376	-2.132388	0.285274
-13.669943	1.970561	0.290278
-14.458042	8.849313	0.295283
-14.798313	-0.925440	0.300288
-15.034397	10.092726	0.305293
-15.170097	-1.233395	0.310298
-15.303581	2.618594	0.315302
-15.574775	3.875170	0.320307
-15.365760	-2.745591	0.325312
-15.496744	-1.402516	0.330317
-15.465678	0.812972	0.335322
-16.289584	-5.795991	0.340326
-16.828257	1.572873	0.345331
-16.708639	-0.630385	0.350336
-17.004747	-2.209307	0.355341
-17.947592	0.427343	0.360346
-17.905673	-7.410327	0.365350
-18.309777	4.121097	0.370355
-18.268684	-2.466135	0.375360
-18.738937	4.469896	0.380365
-18.910396	-0.928135	0.385370
-18.461574	-5.297370	0.390374
-18.433160	7.326107	0.395379
-19.078687	3.391463	0.400384
-19.589714	5.955620	0.405389
-19.895786	4.141745	0.410394
-19.936554	-0.812616	0.415398
-20.822422	-2.667231	0.420403
-21.159183	0.794548	0.425408
-21.297757	2.459547	0.430413
-21.142099	-1.304269	0.435418
-21.513612	-3.989189	0.440422
-21.620950	-2.353832	0.445427
-21.305561	-7.493856	0.450432
-21.698611	9.671378	0.455437
-22.872615	3.386984	0.460442
-23.108110	-0.532480	0.465446
-23.308673	-3.690497	0.470451
-23.033897	-9.616482	0.475456
-23.233370	1.552100	0.480461
-23.664427	1.529987	0.485466
-23.467765	-6.202081	0.490470
-24.509263	-0.720126	0.495475
-24.623243	4.909763	0.500480
-24.452878	-7.081137	0.505485
-24.425702	0.386029	0.510490
-24.957808	3.914691	0.515494
-26.233394	-0.856106	0.520499
-26.214683	-5.170101	0.525504
-26.314840	-0.670460	0.530509
-25.938951	3.814091	0.535514
-25.708052	-4.345941	0.540518
-26.412396	-3.807758	0.545523
-26.621294	-3.279396	0.550528
-27.682479	2.022301	0.555533
-28.107837	2.011085	0.560538
-27.934542	-1.322308	0.565542
-28.364669	3.976121	0.570547
-27.886841	-8.268748	0.575552
-28.120185	-5.850820	0.580557
-28.379118	-3.007348	0.585562
-28.325451	-1.485282	0.590566
-29.323905	7.529705	0.595571
-29.458701	1.562414	0.600576
-29.587338	5.757158	0.605581
-29.913214	5.535885	0.610586
-30.397178	-2.176419	0.615590
-31.146203	5.374491	0.620595
-30.997317	4.827142	0.625600
-31.321141	2.779013	0.630605
-31.415914	1.681791	0.635610
-31.269518	-4.998259	0.640614
-31.483327	7.772875	0.645619
-31.788025	5.188581	0.650624
-31.606095	2.507128	0.655629
-32.622855	3.177559	0.660634
-32.785641	1.278192	0.665638
-33.214410	2.299594	0.670643
-33.275281	3.204820	0.675648
-33.431650	8.518892	0.680653
-33.306662	6.470440	0.685658
-33.678564	-0.376961	0.690662
-34.539490	13.450709	0.695667
-34.342914	0.717437	0.700672
-34.681073	6.339063	0.705677
-34.742236	12.799466	0.710682
-35.351845	1.831051	0.715686
-36.310197	4.471062	0.720691
-36.144356	-7.711684	0.725696
-36.252875	-2.035934	0.730701
-36.518394	9.525035	0.735706
-36.183954	-0.234758	0.740710
-36.403525	8.174887	0.745715
-36.190728	7.927557	0.750720
-36.857291	6.890094	0.755725
-37.386285	8.318419	0.760730
-37.499124	-2.466054	0.765734
-37.787672	8.201059	0.770739
-38.190598	6.195037	0.775744
-38.657110	9.783089	0.780749
-38.961374	0.488409	0.785754
-38.711582	2.980054	0.790758
-38.998835	14.245271	0.795763
-39.242007	3.139609	0.800768
-39.890840	9.766790	0.805773
-40.472656	1.451261	0.810778
-40.811933	8.785925	0.815782
-41.236937	13.719429	0.820787
-40.755025	7.055643	0.825792
-40.837933	5.247043	0.830797
-41.085225	9.971938	0.835802
-40.929372	7.164364	0.840806
-41.448963	6.187811	0.845811
-42.082832	-0.259428	0.850816
-42.156064	3.401629	0.855821
-42.382268	14.843413	0.860826
-42.369689	7.995092	0.865830
-43.155235	1.622106	0.870835
-43.490705	1.277708	0.875840
-43.598833	5.089978	0.880845
-43.790424	4.989338	0.885850
-43.789212	2.262824	0.890854
-43.853744	3.607525	0.895859
-44.223425	-5.609816	0.900864
-45.101318	0.136314	0.905869
-45.516456	3.558977	0.910874
-45.211936	-0.836685	0.915878
-45.561357	5.264747	0.920883
-45.397847	1.392281	0.925888
-45.408518	2.931316	0.930893
-46.505720	11.537210	0.935898
-46.687829	-4.520373	0.940902
-47.187704	-1.473016	0.945907
-47.067451	-0.197199	0.950912
-47.110811	6.774700	0.955917
-47.288282	7.654638	0.960922
-47.099794	2.360986	0.965926
-48.066492	8.482550	0.970931
-48.501035	-3.416267	0.975936
-48.736209	6.929627	0.980941
-48.482874	14.895500	0.985946
-48.710900	5.785330	0.990950
-49.201124	5.083141	0.995955
-49.860205	5.247582	1.000960
-50.064393	4.115988	1.005965
-50.376408	-0.751814	1.010970
-50.466071	4.805375	1.015974
-50.760968	9.788964	1.020979
-50.230297	-3.692466	1.025984
-50.438674	0.564025	1.030989
-51.287301	4.831430	1.035994
-51.450350	-1.115787	1.040998
-51.765586	5.610858	1.046003
-51.968726	5.450365	1.051008
-52.038488	6.735943	1.056013
-52.541458	3.633729	1.061018
-53.007169	2.553141	1.066022
-53.346923	10.327543	1.071027
-53.647101	3.510100	1.076032
-53.369520	6.359842	1.081037
-53.628098	10.319769	1.086042
-53.391209	-3.775852	1.091046
-54.508686	9.747784	1.096051
-54.389744	4.056378	1.101056
-54.821940	-5.302949	1.106061
-55.116332	7.553948	1.111066
-54.984707	-3.296265	1.116070
-55.346128	7.277933	1.121075
-55.955680	1.769133	1.126080
-56.350320	0.373869	1.131085
-56.780961	14.866731	1.136090
-56.661320	-4.027167	1.141094
-56.879938	5.214471	1.146099
-56.585641	0.940677	1.151104
-56.715623	-6.854117	1.156109
-57.234895	-0.252144	1.161114
-57.432273	0.771591	1.166118
-57.986291	1.552468	1.171123
-58.146340	3.210960	1.176128
-58.855148	-0.145468	1.181133
-59.557877	8.059832	1.186138
-59.171086	-4.726838	1.191142
-59.690817	2.902134	1.196147
-59.605136	-3.521392	1.201152
-59.827016	-2.750329	1.206157
-60.035685	3.884075	1.211162
-59.842353	-3.658396	1.216166
-60.245432	1.038226	1.221171
-60.593886	3.164617	1.226176
-61.306987	-3.896028	1.231181
-61.483202	7.883594	1.236186
-61.299377	-6.342357	1.241190
-61.623954	4.979353	1.246195
-61.930902	2.052865	1.251200
-62.827132	-2.938607	1.256205
-63.063177	0.449465	1.261210
-62.659112	-9.446369	1.266214
-63.173359	-5.639267	1.271219
-63.360155	0.129760	1.276224
-63.407170	-2.050835	1.281229
-63.301036	-5.280162	1.286234
-63.397677	-4.796041	1.291238
-64.289846	-0.591676	1.296243
-64.389746	-0.600545	1.301248
-64.628908	-3.668103	1.306253
-64.962731	-2.609536	1.311258
-65.704986	-2.530775	1.316262
-66.115028	3.790658	1.321267
-66.027557	2.639379	1.326272
-66.009859	5.285687	1.331277
-66.400229	0.971161	1.336282
-66.216221	-2.039788	1.341286
-66.239534	3.319340	1.346291
-66.888553	3.995183	1.351296
-67.343730	4.265176	1.356301
-67.637481	6.278908	1.361306
-67.549503	-2.990936	1.366310
-67.999317	12.799012	1.371315
-68.634284	5.930454	1.376320
-69.224288	1.227485	1.381325
-68.841712	-1.370968	1.386330
-68.621118	10.788520	1.391334
-69.530696	1.475491	1.396339
-69.505722	-5.625093	1.401344
-69.526993	3.668912	1.406349
-69.878167	9.307692	1.411354
-70.262669	1.865450	1.416358
-71.061827	9.923724	1.421363
-71.075936	9.324631	1.426368
-71.220029	5.995451	1.431373
-71.313444	14.378286	1.436378
-71.289251	0.473780	1.441382
-71.426173	2.252367	1.446387
-71.883777	6.537899	1.451392
-72.428352	3.946172	1.456397
-73.109489	6.996517	1.461402
-72.708936	5.579874	1.466406
-72.970772	11.965764	1.471411
-73.035375	0.974985	1.476416
-73.626314	0.587649	1.481421
-74.544439	0.751185	1.486426
-74.450505	1.939403	1.491430
-74.668724	2.304144	1.496435
-74.563120	-3.644936	1.501440
-74.428438	-5.092535	1.506445
-74.372724	-0.625219	1.511450
-74.860367	-1.609623	1.516454
-75.649615	0.410588	1.521459
-76.205993	-3.448428	1.526464
-76.108100	-7.301343	1.531469
-76.105585	1.417048	1.536474
-76.124090	-9.772968	1.541478
-76.724245	-3.207525	1.546483
-77.439988	1.186665	1.551488
-77.518070	-4.074087	1.556493
-77.864877	-0.555389	1.561498
-77.598010	-2.297790	1.566502
-77.768261	0.468838	1.571507
-77.954260	-0.375884	1.576512
-78.660113	-10.000881	1.581517
-79.226950	1.363511	1.586522
-79.288314	-0.474703	1.591526
-79.538456	1.946207	1.596531
-79.756965	-2.032501	1.601536
-79.284688	-2.567301	1.606541
-80.156576	5.535576	1.611546
-80.629963	-3.607358	1.616550
-81.099964	-6.056920	1.621555
-81.109085	1.122424	1.626560
-81.059396	0.338916	1.631565
-81.287890	4.465343	1.636570
-80.984892	-1.874588	1.641574
-81.577166	1.080923	1.646579
-82.091600	6.218677	1.651584
-82.261234	-1.207050	1.656589
-82.896655	5.473954	1.661594
-82.585324	-14.773015	1.666598
-82.941573	-0.126334	1.671603
-83.672400	0.007765	1.676608
-83.856545	-8.747750	1.681613
-84.563634	-0.808723	1.686618
-84.150210	-4.836042	1.691622
-84.321573	-3.569158	1.696627
-84.315981	-8.458571	1.701632
-84.139639	-4.355186	1.706637
-84.938107	0.839669	1.711642
-85.316613	-7.646859	1.716646
-85.962490	-2.996064	1.721651
-85.891593	-15.469731	1.726656
-85.720088	-5.637761	1.731661
-86.138712	-3.809956	1.736666
-86.607327	-9.934678	1.741670
-87.249871	4.688381	1.746675
-87.680374	-4.551637	1.751680
-87.478904	-8.178393	1.756685
-87.717938	-2.764796	1.761690
-87.471702	-1.064266	1.766694
-87.822508	-6.149216	1.771699
-87.950666	-5.808665	1.776704
-88.642864	-8.906173	1.781709
-88.925023	3.073324	1.786714
-89.025087	-1.456812	1.791718
-88.988855	1.854793	1.796723
-89.643818	3.042913	1.801728
-89.954067	-1.512995	1.806733
-90.361828	7.509157	1.811738
-90.364515	-2.087254	1.816742
-90.555965	-0.083952	1.821747
-90.468428	3.437012	1.826752
-90.723268	-2.014295	1.831757
-91.456067	-3.311717	1.836762
-91.691567	-3.883813	1.841766
-91.777934	-2.331060	1.846771
-92.074495	-4.301014	1.851776
-92.266259	6.487805	1.856781
-93.193754	-4.554435	1.861786
-93.280811	1.559982	1.866790
-93.452779	2.161165	1.871795
-93.349152	-6.241028	1.876800
-93.516665	6.776795	1.881805
-93.825972	-1.751979	1.886810
-93.678256	2.903945	1.891814
-93.980347	3.887402	1.896819
-94.757015	0.719227	1.901824
-94.945446	-3.440679	1.906829
-95.093541	6.032392	1.911834
-95.138995	-2.652163	1.916838
-95.520693	0.440352	1.921843
-95.901510	-2.272223	1.926848
-96.285053	1.063120	1.931853
-96.676829	0.263727	1.936858
-96.857222	-6.808369	1.941862
-96.754371	-6.691174	1.946867
-96.974435	-7.320487	1.951872
-96.975425	-5.432594	1.956877
-97.694805	7.157639	1.961882
-98.077097	-9.923691	1.966886
-98.572808	-3.371400	1.971891
-98.757007	7.145228	1.976896
-98.556019	-3.118747	1.981901
-98.973000	4.572341	1.986906
-98.427734	-0.901757	1.991910
-98.998304	-1.671145	1.996915
-99.989800	1.511073	2.006912
-99.166473	3.468225	2.016909
-99.039022	7.517073	2.026906
-98.497850	-0.873834	2.036902
-97.263545	4.970327	2.046899
-97.139503	-5.323203	2.056896
-97.261000	-2.772913	2.066893
-96.901878	2.728153	2.076890
-96.099085	-1.922710	2.086886
-94.713599	-0.901164	2.096883
-94.569788	-4.044378	2.106880
-94.727489	1.224167	2.116877
-93.937505	-1.274842	2.126874
-92.860242	5.552829	2.136870
-93.099936	-0.885633	2.146867
-92.668870	1.812621	2.156864
-91.587097	4.057731	2.166861
-91.405505	-0.350955	2.176858
-90.911180	-2.014212	2.186854
-90.128553	-5.812509	2.196851
-89.938002	-10.679297	2.206848
-89.615291	-5.002477	2.216845
-89.037101	-2.904353	2.226842
-88.482900	-6.038474	2.236838
-87.133450	-7.257704	2.246835
-87.081983	-1.299452	2.256832
-87.107534	2.045248	2.266829
-86.567268	-9.393856	2.276826
-85.448186	-4.441481	2.286822
-85.528395	-8.164655	2.296819
-85.075035	-4.350573	2.306816
-84.249811	-3.558699	2.316813
-83.968714	-2.626130	2.326810
-83.017825	-2.544443	2.336806
-82.584178	-2.758436	2.346803
-82.334183	0.201376	2.356800
-82.222708	3.206654	2.366797
-81.370292	0.564333	2.376794
-81.043894	-0.280177	2.386790
-79.965170	4.458973	2.396787
-79.493453	-0.324172	2.406784
-79.436984	-8.018336	2.416781
-79.178536	1.973336	2.426778
-78.049137	-7.993516	2.436774
-77.753056	0.320942	2.446771
-77.324470	7.476353	2.456768
-76.655232	0.597701	2.466765
-76.454262	-3.078186	2.476762
-75.932277	-1.801996	2.486758
-75.097578	-1.542206	2.496755
-74.809776	-3.068910	2.506752
-74.273662	-1.119711	2.516749
-73.590147	-4.338868	2.526746
-73.073811	-3.127736	2.536742
-72.905358	-2.633131	2.546739
-72.579548	-9.279448	2.556736
-71.751398	-3.551181	2.566733
-71.421855	-0.174793	2.576730
-70.616045	-7.295378	2.586726
-70.114555	-4.687227	2.596723
-69.909273	2.068697	2.606720
-69.122736	-6.228876	2.616717
-68.640663	-3.944908	2.626714
-68.395910	-4.528322	2.636710
-67.813541	-3.852911	2.646707
-66.805990	-1.193615	2.656704
-66.410750	0.865260	2.666701
-66.758927	-4.093499	2.676698
-65.909218	-1.876340	2.686694
-65.242845	-5.943462	2.696691
-65.032509	-5.556957	2.706688
-64.106330	-6.264283	2.716685
-63.816098	-5.364641	2.726682
-63.382564	-6.931680	2.736678
-62.507538	-9.138310	2.746675
-62.292972	-7.797180	2.756672
-62.113567	-9.484153	2.766669
-61.169410	-0.297191	2.776666
-60.957958	-3.831960	2.786662
-59.941510	-5.313950	2.796659
-59.357094	-4.818285	2.806656
-59.257161	-12.455431	2.816653
-59.293568	-2.584853	2.826650
-58.429451	-3.907061	2.836646
-57.871679	-4.302046	2.846643
-56.561082	-7.708429	2.856640
-56.621170	-4.508571	2.866637
-56.124245	-2.279816	2.876634
-55.995873	1.062908	2.886630
-55.152604	-9.274844	2.896627
-54.405671	0.946541	2.906624
-54.050176	-2.954498	2.916621
-54.357101	-2.950216	2.926618
-53.170215	-1.872650	2.936614
-52.997127	-5.491756	2.946611
-51.770284	-4.794442	2.956608
-51.358343	-5.591667	2.966605
-51.209897	-1.944627	2.976602
-51.060073	-3.265516	2.986598
-50.518809	-1.647332	2.996595
-49.949658	1.871356	3.006592
-48.828717	-3.624899	3.016589
-48.206086	-4.343007	3.026586
-48.408764	-4.897374	3.036582
-48.133655	-4.718983	3.046579
-46.994206	-4.006206	3.056576
-46.553730	-0.670316	3.066573
-46.782978	-2.241406	3.076570
-45.795221	5.323082	3.086566
-45.133540	-3.673818	3.096563
-44.656338	-8.944915	3.106560
-43.729818	-4.881191	3.116557
-43.614642	0.234087	3.126554
-43.610886	-4.362098	3.136550
-42.640154	-11.286915	3.146547
-42.244286	2.383577	3.156544
-41.826844	4.165122	3.166541
-40.980215	-6.358325	3.176538
-40.549630	-6.249347	3.186534
-40.402389	-6.201329	3.196531
-39.932511	-2.914368	3.206528
-39.164860	-4.142749	3.216525
-38.711813	-5.105244	3.226522
-37.832284	-2.742655	3.236518
-37.776719	-4.889452	3.246515
-37.446859	-5.731371	3.256512
-36.561582	-5.349938	3.266509
-36.157381	1.157484	3.276506
-36.041454	-6.376409	3.286502
-34.709793	-9.126535	3.296499
-34.398305	-6.442260	3.306496
-34.379382	-7.461690	3.316493
-34.092140	-6.754197	3.326490
-32.985894	-1.025143	3.336486
-32.817985	-0.607505	3.346483
-31.845468	-9.182656	3.356480
-31.368624	-6.816018	3.366477
-31.021539	-8.780704	3.376474
-30.899403	-3.640301	3.386470
-30.519282	0.975669	3.396467
-29.325132	-6.777872	3.406464
-29.329750	-10.845312	3.416461
-28.704465	-8.757745	3.426458
-28.066449	-5.797969	3.436454
-27.558642	-15.770348	3.446451
-27.555885	-7.012735	3.456448
-26.555836	-4.462438	3.466445
-26.252507	-4.751070	3.476442
-25.335411	-7.694739	3.486438
-24.582352	-8.793456	3.496435
-24.411848	-12.613473	3.506432
-24.211104	-9.135533	3.516429
-24.259828	-7.492753	3.526426
-23.041572	-8.186790	3.536422
-22.709408	-9.597938	3.546419
-22.263699	-12.495160	3.556416
-21.401031	-12.294525	3.566413
-21.163232	-10.876822	3.576410
-20.965599	-9.719801	3.586406
-20.264740	-4.654484	3.596403
-19.681930	-12.717961	3.606400
-18.584586	-3.917343	3.616397
-18.346511	-8.992946	3.626394
-18.512062	-3.776449	3.636390
-18.072239	-6.377702	3.646387
-16.792808	-8.497174	3.656384
-16.360614	-13.612428	3.666381
-16.384521	-8.293132	3.676378
-15.935406	-2.246408	3.686374
-15.252919	-10.273044	3.696371
-14.205348	-9.215668	3.706368
-13.841073	-5.814203	3.716365
-13.741566	-2.526961	3.726362
-13.556531	-11.068524	3.736358
-12.551844	-7.740110	3.746355
-12.168359	-5.598668	3.756352
-11.803357	-8.090910	3.766349
-10.683886	-2.658838	3.776346
-10.280175	-4.915251	3.786342
-10.471074	-9.626601	3.796339
-9.748182	-6.038525	3.806336
-8.874075	-13.473111	3.816333
-8.786888	-8.475702	3.826330
-8.292191	-3.298394	3.836326
-7.583403	-7.608450	3.846323
-7.236113	-8.851586	3.856320
-6.193616	-3.551003	3.866317
-5.602624	-6.017440	3.876314
-5.453944	-2.983940	3.886310
-5.501382	-6.178274	3.896307
-4.936346	-4.193941	3.906304
-3.976714	-2.607290	3.916301
-3.886871	-0.670922	3.926298
-3.023931	7.578927	3.936294
-2.670587	7.738043	3.946291
-2.558830	14.876188	3.956288
-2.133662	23.340799	3.966285
-1.460217	40.617751	3.976282
-1.215102	59.154726	3.986278
-0.786141	75.959268	3.996275
-0.255760	101.672044	4.006272
0.000000	133.045308	4.011277
0.366488	133.003805	4.016282
0.126476	148.024870	4.021286
0.453520	170.032047	4.026291
0.665575	167.144098	4.031296
0.653260	170.210206	4.036301
0.789640	177.466975	4.041306
0.805371	192.693193	4.046310
0.931337	195.912629	4.051315
1.154951	205.557528	4.056320
0.956485	200.775243	4.061325
1.158913	202.567122	4.066330
0.936007	199.019076	4.071334
1.504695	197.533930	4.076339
1.224138	203.986738	4.081344
1.269450	200.602664	4.086349
1.280090	212.676517	4.091354
1.010441	214.748443	4.096358
0.970500	200.223484	4.101363
1.126441	206.607566	4.106368
0.796687	206.100792	4.111373
1.179444	211.775389	4.116378
1.520501	226.617627	4.121382
1.769348	226.477005	4.126387
1.584172	223.612396	4.131392
1.704232	212.449192	4.136397
1.446494	215.329998	4.141402
1.350627	217.461357	4.146406
1.422009	206.859350	4.151411
1.282397	212.306879	4.156416
1.128257	219.309456	4.161421
1.315187	215.178495	4.166426
1.686160	221.131712	4.171430
1.491329	216.914583	4.176435
1.288828	226.556449	4.181440
1.699249	225.156708	4.186445
1.352873	233.211548	4.191450
1.440913	231.248712	4.196454
1.891928	229.392323	4.201459
1.930044	233.714820	4.206464
1.641854	220.089560	4.211469
1.757599	213.866193	4.216474
1.282932	219.096488	4.221478
1.540272	204.808633	4.226483
1.457741	217.097424	4.231488
1.667142	207.685783	4.236493
1.573097	207.056110	4.241498
1.712517	223.132523	4.246502
1.989231	228.073032	4.251507
1.684361	222.780881	4.256512
1.769749	211.732150	4.261517
1.778829	212.746180	4.266522
1.514174	218.116933	4.271526
1.583091	219.879614	4.276531
1.579256	219.686113	4.281536
1.600242	232.384021	4.286541
1.757115	237.677482	4.291546
1.658478	241.128495	4.296550
1.888127	237.155427	4.301555
1.784835	237.753137	4.306560
1.572182	232.092480	4.311565
1.856972	240.138123	4.316570
1.639316	242.057979	4.321574
1.594592	234.140404	4.326579
1.572719	242.419166	4.331584
1.481727	239.401612	4.336589
1.853879	226.628422	4.341594
1.468617	241.822224	4.346598
1.464482	244.639927	4.351603
1.781203	266.631586	4.356608
1.761209	270.465046	4.361613
1.978453	268.986978	4.366618
2.004845	281.165628	4.371622
1.864791	267.145592	4.376627
1.958879	281.270414	4.381632
1.755870	279.215460	4.386637
1.834820	276.003995	4.391642
1.971639	281.958120	4.396646
2.141891	277.847664	4.401651
1.971843	274.754590	4.406656
1.858662	281.065456	4.411661
2.072051	272.963432	4.416666
2.141908	273.940959	4.421670
2.431312	269.563315	4.426675
2.413215	272.120482	4.431680
2.075910	271.864192	4.436685
2.627990	273.494381	4.441690
2.039530	278.858784	4.446694
2.157044	264.202512	4.451699
2.235561	267.080139	4.456704
2.209284	267.969390	4.461709
2.426088	267.797369	4.466714
2.322105	280.627703	4.471718
2.446637	279.308253	4.476723
2.486082	271.071244	4.481728
2.383699	271.887848	4.486733
2.404878	276.943308	4.491738
2.220475	275.782366	4.496742
2.400702	267.425352	4.501747
1.980673	272.649774	4.506752
2.040068	270.621030	4.511757
2.080521	272.681870	4.516762
1.932326	272.274877	4.521766
2.425705	273.991748	4.526771
2.426193	267.887099	4.531776
1.865232	271.219115	4.536781
2.128970	277.283253	4.541786
1.831665	278.427548	4.546790
2.274519	278.388398	4.551795
2.357686	298.194791	4.556800
2.630699	302.671603	4.561805
2.500071	298.340416	4.566810
2.348448	303.126913	4.571814
2.495889	306.411687	4.576819
2.596781	308.310574	4.581824
2.656369	303.433430	4.586829
2.631057	297.744292	4.591834
2.495667	298.710420	4.596838
2.502209	296.537882	4.601843
2.519683	300.813692	4.606848
2.290993	308.903746	4.611853
2.549424	307.348604	4.616858
2.512604	308.868319	4.621862
2.613631	304.488903	4.626867
2.585620	311.200481	4.631872
2.527618	310.615551	4.636877
2.820421	307.802612	4.641882
2.292766	313.726868	4.646886
2.879752	312.651313	4.651891
2.859079	309.204339	4.656896
2.542475	312.099252	4.661901
2.878553	307.641051	4.666906
2.828733	313.197083	4.671910
2.525150	309.467402	4.676915
2.453680	308.514300	4.681920
2.449052	310.799089	4.686925
2.853541	309.442357	4.691930
2.807413	305.249914	4.696934
2.502361	310.139176	4.701939
2.673068	303.422802	4.706944
2.517430	305.022972	4.711949
2.646855	307.477374	4.716954
2.310738	316.607032	4.721958
2.372041	329.905156	4.726963
3.098980	337.320156	4.731968
2.925556	340.938485	4.736973
3.044019	341.145652	4.741978
2.793453	346.901096	4.746982
3.051660	348.562195	4.751987
2.956273	350.924377	4.756992
3.006842	352.042055	4.761997
3.167732	349.652732	4.767002
2.947226	358.764652	4.772006
3.251406	341.909838	4.777011
3.103295	344.250163	4.782016
2.951799	351.081664	4.787021
3.079740	340.124268	4.792026
3.048314	345.936567	4.797030
3.046684	339.525776	4.802035
2.849007	333.864772	4.807040
2.561200	341.391367	4.812045
2.791639	344.532952	4.817050
2.390374	347.533652	4.822054
3.058342	348.411748	4.827059
2.730385	349.651109	4.832064
2.772349	358.691151	4.837069
3.133047	360.080714	4.842074
3.236696	373.784102	4.847078
3.208552	369.189844	4.852083
3.288865	369.347877	4.857088
3.055547	375.498308	4.862093
3.447175	371.576333	4.867098
3.079851	365.659046	4.872102
3.306387	369.282983	4.877107
3.303587	378.067002	4.882112
3.285728	374.190929	4.887117
3.255505	366.036250	4.892122
3.234562	372.586446	4.897126
3.334419	377.651604	4.902131
3.440458	371.113843	4.907136
3.338230	370.095776	4.912141
3.382940	371.460308	4.917146
3.466684	370.256141	4.922150
3.312387	363.431740	4.927155
3.213099	359.557511	4.932160
3.592449	373.600449	4.937165
3.649515	370.307339	4.942170
3.169508	365.720218	4.947174
2.784942	355.883897	4.952179
3.495059	377.922266	4.957184
3.780246	375.464798	4.962189
3.998748	374.321593	4.967194
3.577206	373.201293	4.972198
3.761170	355.669175	4.977203
3.742018	350.555817	4.982208
3.351818	364.275851	4.987213
3.474270	354.603825	4.992218
3.442957	358.648162	4.997222
3.055994	344.770768	5.002227
3.516282	358.275766	5.007232
3.466947	372.364824	5.012237
3.838312	377.731351	5.017242
3.655191	379.099866	5.022246
3.679270	372.729600	5.027251
3.575010	366.161345	5.032256
3.644445	372.254736	5.037261
3.705399	368.504539	5.042266
3.355040	369.163886	5.047270
3.382309	374.900566	5.052275
3.774061	375.905113	5.057280
3.598790	377.525907	5.062285
3.861300	376.185180	5.067290
3.386759	386.968602	5.072294
3.608213	384.229626	5.077299
3.562000	391.989948	5.082304
3.523685	389.063889	5.087309
3.941848	372.425987	5.092314
3.646332	382.679905	5.097318
3.641624	380.612229	5.102323
3.482477	377.300060	5.107328
3.439549	383.919614	5.112333
3.798842	381.687469	5.117338
3.651424	389.690303	5.122342
4.083977	401.751075	5.127347
3.972226	401.737654	5.132352
3.720473	389.152498	5.137357
4.123209	391.095741	5.142362
3.722429	395.274480	5.147366
3.906967	396.369977	5.152371
3.842799	405.446959	5.157376
4.266709	406.951764	5.162381
3.949403	392.368162	5.167386
3.785438	397.314603	5.172390
4.120750	406.166184	5.177395
4.153417	413.632445	5.182400
4.130132	402.635911	5.187405
3.993352	383.652366	5.192410
3.931761	381.153059	5.197414
3.911652	389.955343	5.202419
3.992755	402.980885	5.207424
3.944470	409.405577	5.212429
3.963781	412.816772	5.217434
3.620648	418.188551	5.222438
3.774266	420.745331	5.227443
3.708910	408.608827	5.232448
3.844065	418.046107	5.237453
4.060372	412.876570	5.242458
3.824777	417.042565	5.247462
3.964567	414.981347	5.252467
4.280644	435.078903	5.257472
4.086085	442.271206	5.262477
4.234960	444.664590	5.267482
4.129127	443.355645	5.272486
4.353552	446.663419	5.277491
4.163421	449.063801	5.282496
4.073346	455.841566	5.287501
4.288115	435.424884	5.292506
3.705180	441.996338	5.297510
4.205256	447.318882	5.302515
4.280558	445.801154	5.307520
3.792519	447.947162	5.312525
4.302208	435.826912	5.317530
4.283176	444.915191	5.322534
4.367130	442.115696	5.327539
4.358340	444.315154	5.332544
4.155693	442.026666	5.337549
4.401356	444.478617	5.342554
4.589159	446.381088	5.347558
4.500007	439.294851	5.352563
4.242720	447.240129	5.357568
4.039976	447.976468	5.362573
4.638823	469.212660	5.367578
4.789752	465.296576	5.372582
4.363837	454.180388	5.377587
4.541335	452.198962	5.382592
4.196254	455.726549	5.387597
4.902743	465.692053	5.392602
4.487113	465.200082	5.397606
4.623674	450.452466	5.402611
4.563177	442.139561	5.407616
4.336892	451.375435	5.412621
4.558681	463.791239	5.417626
4.530715	475.868730	5.422630
4.712347	477.851952	5.427635
4.834957	469.539496	5.432640
4.713182	479.281029	5.437645
4.671980	465.704640	5.442650
4.778293	470.899201	5.447654
4.529331	456.321192	5.452659
4.603697	465.810008	5.457664
4.357123	479.256726	5.462669
4.839236	479.195881	5.467674
4.808806	475.828236	5.472678
4.927398	474.883120	5.477683
5.129876	479.483161	5.482688
4.625479	464.859427	5.487693
4.604192	462.022101	5.492698
4.984614	485.311881	5.497702
4.933248	472.434567	5.502707
4.624537	464.322201	5.507712
4.511478	472.363987	5.512717
4.776435	478.505952	5.517722
4.580359	489.913499	5.522726
4.987534	490.886886	5.527731
4.763311	479.097507	5.532736
4.699333	490.441937	5.537741
4.773188	483.127599	5.542746
4.901065	478.661201	5.547750
4.938015	478.679200	5.552755
4.870195	478.585488	5.557760
4.777300	482.923236	5.562765
5.093698	478.885422	5.567770
4.865253	489.474437	5.572774
4.691304	496.762219	5.577779
4.785253	493.520203	5.582784
5.095067	482.837874	5.587789
5.238141	485.391083	5.592794
4.988462	487.240887	5.597798
5.156631	480.218191	5.602803
5.053316	487.238127	5.607808
4.824012	489.540017	5.612813
5.016224	485.402585	5.617818
4.997267	485.107981	5.622822
5.252300	478.479592	5.627827
4.768538	480.214233	5.632832
5.086758	503.780947	5.637837
5.577556	503.349638	5.642842
5.342485	501.282992	5.647846
5.015216	498.595587	5.652851
5.596525	493.032277	5.657856
5.064971	491.746264	5.662861
5.166422	484.489124	5.667866
4.865191	487.419018	5.672870
4.694591	502.415907	5.677875
5.356453	507.126965	5.682880
4.967362	514.046229	5.687885
5.336081	518.633357	5.692890
4.878513	528.304622	5.697894
5.256167	521.269716	5.702899
5.262768	519.965827	5.707904
5.162340	525.169775	5.712909
5.269226	517.030202	5.717914
5.443017	521.945816	5.722918
5.076768	517.908546	5.727923
5.415349	515.419916	5.732928
4.944221	523.582787	5.737933
5.053537	520.071615	5.742938
4.945835	522.552491	5.747942
5.403150	545.043426	5.752947
5.156007	542.730520	5.757952
5.254591	547.169981	5.762957
5.451571	543.160410	5.767962
5.187468	547.686964	5.772966
5.393862	550.827639	5.777971
5.839209	555.657645	5.782976
5.465905	555.915066	5.787981
5.835218	553.529878	5.792986
5.250981	554.077191	5.797990
5.119651	555.280654	5.802995
5.578194	558.013117	5.808000
5.150085	557.568794	5.813005
5.517303	554.521876	5.818010
5.612786	562.700862	5.823014
5.607441	564.154214	5.828019
5.837584	565.834193	5.833024
5.670660	563.115293	5.838029
5.877653	562.473646	5.843034
5.338972	564.632593	5.848038
5.678380	559.613323	5.853043
5.606836	553.335977	5.858048
5.310925	558.110924	5.863053
5.785792	570.311248	5.868058
5.642448	587.479780	5.873062
6.040321	591.045797	5.878067
6.183381	575.083539	5.883072
5.617343	565.953223	5.888077
5.882824	554.043032	5.893082
6.270076	556.761645	5.898086
5.832311	560.076478	5.903091
5.773981	553.274781	5.908096
5.631584	558.780516	5.913101
5.676055	553.476976	5.918106
5.680632	553.641632	5.923110
5.884349	545.497653	5.928115
5.984196	551.221394	5.933120
5.399368	554.898818	5.938125
5.703991	569.023180	5.943130
5.606646	581.062511	5.948134
5.785445	583.185735	5.953139
6.209039	576.226870	5.958144
6.095269	589.179062	5.963149
6.106229	570.723970	5.968154
5.981568	581.958729	5.973158
5.720580	590.073419	5.978163
6.062055	589.274718	5.983168
5.812609	587.253067	5.988173
6.310899	579.308349	5.993178
6.223057	584.619757	5.998182
5.735087	590.169307	6.003187
5.932610	581.182704	6.008192
5.821113	579.504277	6.013197
6.135026	579.235264	6.018202
5.757898	586.244934	6.023206
5.559479	582.982441	6.028211
6.224989	580.252586	6.033216
5.663182	590.601649	6.038221
5.807256	577.577230	6.043226
6.267383	590.377952	6.048230
5.866006	591.619030	6.053235
5.923872	596.703448	6.058240
6.160327	611.193560	6.063245
6.573425	612.788586	6.068250
6.287440	600.923695	6.073254
6.324241	583.268276	6.078259
6.364160	589.015965	6.083264
6.071585	581.702661	6.088269
6.615993	587.308005	6.093274
6.022572	593.774101	6.098278
6.313553	588.616020	6.103283
6.233254	589.530416	6.108288
5.965807	593.687523	6.113293
6.083458	574.351789	6.118298
5.846059	589.236288	6.123302
6.117036	590.734269	6.128307
6.133232	582.564291	6.133312
5.867515	593.688816	6.138317
5.804057	583.470408	6.143322
5.970238	582.657123	6.148326
5.819471	577.830709	6.153331
5.642283	574.043525	6.158336
5.476875	581.812628	6.163341
6.129897	594.807960	6.168346
6.632071	608.788149	6.173350
6.133352	595.783126	6.178355
6.077508	586.172844	6.183360
6.119099	592.263038	6.188365
6.439092	579.266518	6.193370
6.256829	584.444964	6.198374
6.223024	581.715462	6.203379
6.035554	576.885654	6.208384
5.996904	585.971344	6.213389
6.498800	581.194728	6.218394
6.084169	579.183853	6.223398
5.819044	585.575061	6.228403
6.028972	587.199780	6.233408
5.803291	588.165878	6.238413
6.435430	587.415349	6.243418
6.377651	589.367581	6.248422
5.959381	584.559412	6.253427
6.295642	574.082611	6.258432
5.941900	580.497569	6.263437
5.848894	577.331684	6.268442
5.952674	574.858639	6.273446
6.206208	574.658827	6.278451
6.262108	575.370103	6.283456
5.950462	577.455739	6.288461
6.113213	583.118161	6.293466
6.075694	576.108761	6.298470
6.026278	581.370785	6.303475
5.878845	579.802701	6.308480
5.549405	591.910074	6.313485
6.145951	580.522659	6.318490
6.258828	584.082980	6.323494
6.131658	590.169939	6.328499
6.174341	582.780793	6.333504
5.986566	583.845599	6.338509
5.938447	577.872413	6.343514
6.027935	584.588136	6.348518
6.143437	573.943249	6.353523
6.125296	576.247088	6.358528
5.962926	581.330475	6.363533
6.082663	582.806335	6.368538
6.242536	587.076603	6.373542
5.987919	581.382114	6.378547
6.152848	581.507982	6.383552
6.073793	577.341442	6.388557
6.121312	582.761074	6.393562
5.942209	581.235137	6.398566
5.857272	578.948253	6.403571
6.354046	579.692695	6.408576
6.177753	589.570018	6.413581
6.004451	588.523842	6.418586
6.230778	581.922068	6.423590
6.062893	577.781682	6.428595
6.342503	584.738845	6.433600
5.897975	579.761957	6.438605
5.988921	583.309333	6.443610
5.990722	587.360876	6.448614
5.941495	583.706821	6.453619
6.120695	578.191121	6.458624
6.202548	579.854216	6.463629
6.374008	580.311719	6.468634
6.390585	581.473720	6.473638
6.105355	577.414336	6.478643
6.298997	579.742901	6.483648
5.952816	593.560833	6.488653
6.229277	577.481167	6.493658
5.989211	581.064015	6.498662
5.913331	580.396586	6.503667
6.076074	590.866231	6.508672
5.942705	585.569631	6.513677
6.121384	581.801665	6.518682
6.165404	580.057426	6.523686
6.354383	587.533409	6.528691
6.191761	587.564721	6.533696
5.950914	589.454911	6.538701
6.109446	584.250483	6.543706
6.219699	588.589748	6.548710
6.224558	585.450282	6.553715
6.133150	580.183047	6.558720
6.099157	587.007824	6.563725
6.314879	584.007891	6.568730
6.288237	591.202256	6.573734
6.315096	576.784484	6.578739
6.173654	586.916327	6.583744
6.392994	577.475781	6.588749
6.359229	562.220879	6.593754
6.083705	561.354832	6.598758
5.546703	562.568044	6.603763
6.006802	559.109091	6.608768
6.290353	579.911990	6.613773
6.339888	563.420374	6.618778
6.169541	558.854343	6.623782
5.899640	561.615862	6.628787
6.103352	549.325367	6.633792
5.743327	557.909927	6.638797
6.022172	552.919830	6.643802
6.031248	566.405398	6.648806
6.489696	571.523133	6.653811
6.352909	557.981633	6.658816
5.830171	560.913290	6.663821
6.011637	552.603674	6.668826
6.163709	552.072160	6.673830
5.725555	555.978288	6.678835
5.981292	556.594705	6.683840
6.106574	575.239643	6.688845
6.494516	578.191205	6.693850
5.976277	561.201191	6.698854
5.830483	561.306482	6.703859
6.098226	562.591277	6.708864
6.069178	568.635930	6.713869
6.463795	563.391232	6.718874
5.997138	559.660273	6.723878
6.194042	560.243412	6.728883
5.968671	557.222195	6.733888
5.985539	561.777809	6.738893
6.062348	559.257529	6.743898
5.834086	560.616957	6.748902
6.056801	574.829679	6.753907
6.473548	580.804268	6.758912
6.367968	580.387052	6.763917
6.014851	558.687991	6.768922
6.120454	561.443178	6.773926
5.974743	560.143590	6.778931
6.155215	556.535573	6.783936
5.819343	559.528840	6.788941
5.880924	559.624065	6.793946
5.839865	570.443187	6.798950
6.125690	580.129131	6.803955
6.525935	573.390418	6.808960
6.032360	575.605047	6.813965
6.283837	559.022964	6.818970
6.398341	555.324439	6.823974
6.206252	560.368536	6.828979
6.090167	553.815579	6.833984
6.119115	564.040556	6.838989
6.574939	561.947314	6.843994
6.065649	557.926417	6.848998
6.051413	564.542482	6.854003
6.232860	551.466705	6.859008
5.992889	563.856238	6.864013
6.165245	561.996816	6.869018
6.153579	558.646175	6.874022
5.788451	568.570541	6.879027
6.376624	559.961897	6.884032
6.043806	572.391282	6.889037
6.280155	563.708478	6.894042
6.332953	568.163026	6.899046
6.049134	564.842451	6.904051
6.151147	568.241762	6.909056
6.064702	572.715816	6.914061
6.323787	569.218709	6.919066
6.022589	573.053814	6.924070
5.899503	586.696857	6.929075
6.131944	577.223555	6.934080
5.966493	590.171873	6.939085
6.386601	576.029397	6.944090
6.316406	576.656371	6.949094
6.105348	581.675988	6.954099
6.085551	565.393190	6.959104
5.721139	576.469121	6.964109
5.998277	572.148284	6.969114
6.027691	572.398815	6.974118
6.164077	572.620975	6.979123
6.266482	563.600403	6.984128
5.726051	572.246024	6.989133
5.955671	564.808566	6.994138
6.156668	571.653825	6.999142
6.016732	569.596281	7.004147
6.156326	564.958007	7.009152
5.824712	571.408173	7.014157
6.202664	575.751061	7.019162
6.579312	567.687959	7.024166
5.714033	567.028501	7.029171
5.938185	565.319163	7.034176
5.945647	584.446583	7.039181
6.216603	572.553232	7.044186
6.159902	568.716103	7.049190
6.094923	571.988154	7.054195
6.322248	562.915124	7.059200
6.021085	568.933400	7.064205
6.131365	570.355766	7.069210
6.096502	565.393141	7.074214
5.888325	568.923541	7.079219
6.197062	564.989590	7.084224
5.881429	574.714738	7.089229
6.125546	573.759487	7.094234
5.825941	569.427984	7.099238
6.007181	572.648213	7.104243
6.268494	567.053797	7.109248
6.154337	573.880792	7.114253
6.203483	572.039798	7.119258
6.025640	572.440881	7.124262
6.115840	573.921631	7.129267
6.139151	565.518411	7.134272
6.171188	570.105261	7.139277
6.563921	564.519278	7.144282
6.247765	571.199548	7.149286
6.010867	565.827940	7.154291
6.161406	549.401115	7.159296
5.985976	560.847131	7.164301
6.356546	562.632917	7.169306
6.351135	551.721331	7.174310
5.797315	542.296547	7.179315
6.107446	530.817273	7.184320
5.843502	534.780983	7.189325
5.909585	547.552591	7.194330
5.915567	567.003083	7.199334
6.212224	564.112695	7.204339
6.314702	565.210347	7.209344
5.833715	565.931983	7.214349
6.173839	558.231331	7.219354
6.110180	564.616798	7.224358
6.183550	560.275438	7.229363
6.103508	562.716218	7.234368
5.969289	565.739835	7.239373
6.144763	555.960629	7.244378
6.082755	567.836029	7.249382
6.000422	571.832430	7.254387
6.097038	566.468350	7.259392
5.927859	571.641073	7.264397
6.099941	564.764512	7.269402
6.072997	563.464990	7.274406
6.188915	566.252808	7.279411
5.941057	558.629982	7.284416
5.823328	562.558437	7.289421
5.967699	563.786500	7.294426
5.942573	560.372373	7.299430
5.904669	570.246700	7.304435
5.741440	562.569009	7.309440
5.867726	574.258519	7.314445
5.867175	569.407431	7.319450
6.111032	568.208508	7.324454
5.800544	569.498078	7.329459
5.976892	566.704377	7.334464
5.833788	575.839918	7.339469
5.998236	573.815841	7.344474
6.012928	577.833277	7.349478
5.827385	571.042376	7.354483
6.428263	586.015004	7.359488
5.916758	590.146414	7.364493
6.330995	582.662196	7.369498
6.102900	574.499323	7.374502
5.787856	572.784348	7.379507
6.208185	580.042636	7.384512
5.890482	578.519522	7.389517
6.355672	579.814248	7.394522
6.165411	580.810397	7.399526
6.177044	579.234524	7.404531
6.259863	563.452361	7.409536
5.964704	575.716061	7.414541
5.984815	567.047947	7.419546
6.250467	569.903327	7.424550
5.768757	568.525578	7.429555
5.946218	563.725333	7.434560
5.849544	568.993796	7.439565
6.174865	595.547801	7.444570
6.226806	603.217380	7.449574
6.263277	585.742777	7.454579
6.119646	568.825902	7.459584
6.197229	574.721275	7.464589
6.272873	575.882573	7.469594
6.116235	572.920817	7.474598
5.999303	576.600692	7.479603
6.085712	570.401774	7.484608
6.063659	575.436664	7.489613
5.999852	569.901215	7.494618
6.182886	572.000450	7.499622
5.575700	576.631974	7.504627
6.176776	566.052126	7.509632
5.989082	587.131790	7.514637
6.103940	577.461870	7.519642
6.039686	572.283482	7.524646
6.246696	584.081985	7.529651
6.231753	572.911275	7.534656
5.938705	570.790281	7.539661
6.092490	563.188170	7.544666
5.945033	576.360636	7.549670
5.830348	571.842021	7.554675
5.736007	571.978063	7.559680
6.477180	605.471970	7.564685
6.418816	595.524844	7.569690
6.162902	585.723315	7.574694
5.822305	574.141200	7.579699
6.160030	574.869353	7.584704
6.039694	568.045554	7.589709
6.292140	576.206449	7.594714
6.261714	571.872011	7.599718
6.015547	570.317121	7.604723
6.378283	574.061429	7.609728
6.011239	571.866647	7.614733
6.284171	572.320372	7.619738
6.200057	568.147370	7.624742
5.442410	570.937558	7.629747
5.760799	568.040414	7.634752
5.829736	589.272755	7.639757
6.178360	595.861111	7.644762
5.912129	601.691469	7.649766
5.917274	613.781542	7.654771
6.507313	605.542776	7.659776
6.009337	612.187654	7.664781
6.432843	599.929398	7.669786
5.818792	579.482623	7.674790
5.820787	588.675054	7.679795
6.685542	592.182312	7.684800
6.047326	594.285519	7.689805
5.881055	579.709488	7.694810
5.905693	584.957277	7.699814
5.900371	595.326285	7.704819
6.109044	596.614352	7.709824
5.823420	609.454708	7.714829
5.524017	605.138160	7.719834
5.812289	599.607943	7.724838
5.885644	602.959712	7.729843
6.347309	598.727704	7.734848
6.180733	606.028327	7.739853
6.189376	599.073238	7.744858
6.369166	603.851917	7.749862
6.028173	600.859902	7.754867
6.091175	607.750918	7.759872
6.319966	610.201150	7.764877
6.230509	608.050780	7.769882
6.467419	604.272575	7.774886
6.070136	609.536560	7.779891
6.223194	591.850632	7.784896
6.208061	601.743310	7.789901
5.905288	595.179018	7.794906
5.679476	588.991338	7.799910
6.041959	602.708903	7.804915
6.119118	606.049780	7.809920
6.251903	607.893101	7.814925
6.052142	598.032339	7.819930
6.672469	605.272914	7.824934
6.110775	592.435208	7.829939
6.508338	576.334109	7.834944
6.133371	573.996580	7.839949
5.865758	567.537581	7.844954
5.722960	574.611060	7.849958
6.033352	581.592331	7.854963
6.555050	575.259368	7.859968
6.121804	585.791190	7.864973
6.007350	580.602562	7.869978
6.357367	574.212776	7.874982
5.951577	578.624465	7.879987
5.956480	571.903264	7.884992
6.079685	578.671419	7.889997
5.777067	579.863976	7.895002
6.197756	574.430444	7.900006
5.956649	578.312631	7.905011
6.104350	575.774295	7.910016
5.900781	587.345960	7.915021
6.086073	581.868718	7.920026
6.309975	586.931362	7.925030
6.177042	577.777472	7.930035
6.222392	569.223976	7.935040
5.911311	577.166190	7.940045
6.060624	576.660392	7.945050
6.009302	576.819109	7.950054
5.895488	578.651755	7.955059
6.093056	577.267299	7.960064
5.826984	581.580075	7.965069
6.091871	589.427513	7.970074
6.481723	580.856039	7.975078
6.212683	577.198720	7.980083
6.403519	573.869404	7.985088
6.186744	581.796202	7.990093
6.480268	575.982532	7.995098
6.415001	571.060264	8.000102
6.049804	578.530916	8.005107
6.147815	567.858144	8.010112
6.218212	577.277125	8.015130
5.769816	570.012936	8.020147
5.843552	574.728402	8.025165
5.913519	585.153166	8.030182
6.181709	577.073511	8.035200
6.305880	579.655573	8.040218
6.218574	584.800831	8.045235
6.420654	579.968324	8.050253
6.450295	582.312710	8.055270
6.389872	579.243831	8.060288
6.530711	582.078037	8.065306
6.472991	566.944959	8.070323
6.478522	549.707668	8.075341
5.993085	558.075318	8.080358
6.380238	539.993600	8.085376
5.957487	548.707927	8.090394
5.950252	546.668364	8.095411
6.236585	537.879082	8.100429
6.002524	542.849035	8.105446
6.234984	546.501667	8.110464
6.125949	540.255633	8.115482
5.910600	551.624013	8.120499
5.918776	550.465498	8.125517
5.823106	571.471089	8.130534
6.375519	569.523288	8.135552
6.391578	579.055855	8.140570
6.045859	571.481179	8.145587
6.172502	578.926873	8.150605
6.025831	580.925480	8.155622
5.989269	571.992612	8.160640
6.270608	579.695939	8.165658
6.123938	576.592132	8.170675
6.031279	571.037815	8.175693
6.269547	577.369627	8.180710
6.094010	574.325715	8.185728
6.058217	586.863915	8.190746
6.185716	584.722120	8.195763
6.359475	575.934332	8.200781
6.039747	580.627164	8.205798
6.558628	577.518851	8.210816
6.127591	581.252620	8.215834
6.313197	575.875241	8.220851
6.258522	572.387329	8.225869
6.004587	583.239126	8.230886
6.102269	575.903013	8.235904
6.328321	579.063833	8.240922
6.310742	586.321813	8.245939
6.563599	568.635503	8.250957
6.233744	580.701560	8.255974
6.473870	577.522091	8.260992
6.319905	573.993734	8.266010
6.040175	578.657502	8.271027
6.550869	567.869766	8.276045
6.302238	571.641041	8.281062
6.458088	568.627880	8.286080
6.527815	573.360347	8.291098
6.492094	580.687465	8.296115
6.469442	573.952145	8.301133
6.227705	574.292787	8.306150
6.634935	572.339500	8.311168
6.384413	576.743921	8.316186
6.263084	576.371167	8.321203
6.348562	567.121854	8.326221
6.085751	566.556007	8.331238
5.948587	573.916454	8.336256
6.302029	583.319933	8.341274
6.183419	591.262316	8.346291
6.657495	593.872262	8.351309
6.156446	607.402025	8.356326
6.537059	605.926930	8.361344
6.639060	600.017162	8.366362
6.248055	610.045668	8.371379
6.500174	597.303024	8.376397
6.508234	616.723887	8.381414
6.579811	608.451984	8.386432
6.563656	610.045149	8.391450
6.304276	608.742167	8.396467
6.312166	604.190217	8.401485
6.506162	605.548793	8.406502
6.340611	609.053974	8.411520
6.552445	607.614897	8.416538
6.360116	605.464843	8.421555
6.702723	609.288215	8.426573
6.489875	604.751951	8.431590
6.487509	609.363304	8.436608
6.510221	612.641262	8.441626
6.318472	612.801000	8.446643
6.431984	606.029341	8.451661
6.194269	610.796981	8.456678
6.245344	601.068927	8.461696
6.467493	606.955417	8.466714
5.968729	607.458888	8.471731
6.557964	605.194573	8.476749
6.449655	615.063286	8.481766
6.666747	625.743224	8.486784
6.755046	619.552271	8.491802
6.123447	617.599946	8.496819
6.414116	618.500221	8.501837
6.759983	634.919494	8.506854
7.010321	637.628696	8.511872
7.101262	629.667729	8.516890
6.631736	619.343432	8.521907
6.279366	617.062998	8.526925
6.512876	616.257495	8.531942
6.456449	619.568242	8.536960
6.643664	625.781370	8.541978
6.447783	635.708098	8.546995
6.906279	637.378171	8.552013
6.628476	648.047954	8.557030
6.773269	641.383493	8.562048
6.571996	639.075674	8.567066
6.741954	637.323273	8.572083
6.909477	622.680368	8.577101
6.335104	619.143077	8.582119
6.424992	629.035866	8.587136
6.998044	640.773730	8.592154
6.393263	645.370090	8.597171
7.244948	634.411284	8.602189
6.686061	627.812173	8.607207
6.712005	622.686595	8.612224
6.790056	614.806899	8.617242
6.357312	622.400947	8.622259
6.971072	632.395955	8.627277
6.917360	637.012866	8.632295
6.643648	623.311866	8.637312
6.673935	624.038736	8.642330
6.713917	637.495078	8.647347
6.705795	636.481963	8.652365
6.942814	643.112021	8.657383
6.681475	648.603421	8.662400
7.257806	636.563114	8.667418
6.701922	626.689699	8.672435
6.632689	620.392162	8.677453
6.449505	620.644964	8.682471
6.651094	638.874238	8.687488
6.915443	636.614506	8.692506
6.859171	648.298327	8.697523
7.151695	641.609010	8.702541
6.758488	639.031417	8.707559
6.755945	627.014143	8.712576
6.639500	627.211015	8.717594
6.366659	640.566019	8.722611
6.771801	632.849460	8.727629
6.915656	642.272721	8.732647
6.706428	641.176772	8.737664
7.138002	640.917567	8.742682
6.703318	645.072795	8.747699
7.002577	641.249112	8.752717
6.871419	634.408316	8.757735
6.667804	642.343543	8.762752
6.755038	640.635546	8.767770
6.815685	646.693668	8.772787
7.097851	649.638532	8.777805
6.658160	652.135246	8.782823
6.813729	645.084378	8.787840
7.095334	639.953465	8.792858
6.789273	648.804421	8.797875
6.686176	637.065978	8.802893
7.096061	653.090442	8.807911
7.161872	650.047887	8.812928
7.120333	641.004196	8.817946
6.955148	646.503687	8.822963
6.588980	651.419570	8.827981
6.772396	645.216400	8.832999
6.952079	659.972774	8.838016
7.031243	634.147549	8.843034
6.791740	655.011924	8.848051
7.060557	642.158020	8.853069
7.035749	651.441115	8.858087
6.859535	649.742099	8.863104
7.020735	643.724486	8.868122
6.940400	650.422057	8.873139
7.065733	644.230473	8.878157
7.186895	646.909102	8.883175
7.083744	651.194068	8.888192
7.024231	647.066429	8.893210
6.913061	647.561228	8.898227
7.107753	648.184896	8.903245
6.913484	653.754950	8.908263
6.747219	643.357981	8.913280
7.059239	639.327868	8.918298
7.080173	648.806524	8.923315
7.007176	643.110745	8.928333
7.102236	655.051777	8.933351
6.914441	654.638456	8.938368
7.314585	657.685038	8.943386
7.284567	661.473281	8.948403
6.933390	649.093272	8.953421
7.021786	656.145165	8.958439
7.247238	667.550869	8.963456
7.715401	660.315563	8.968474
7.185915	648.699287	8.973491
7.251177	645.532816	8.978509
7.137988	632.825635	8.983527
7.164973	636.325317	8.988544
7.101129	639.716426	8.993562
7.018690	641.311515	8.998579
7.048194	644.501353	9.003597
7.089288	648.302619	9.008615
6.641169	656.554306	9.013632
7.045240	653.332518	9.018650
7.098117	668.929925	9.023667
6.960688	663.620376	9.028685
7.270732	672.467350	9.033703
7.320970	678.355565	9.038720
7.446403	672.650932	9.043738
7.126903	673.487690	9.048755
7.103495	672.042091	9.053773
7.398563	668.830082	9.058791
7.183504	671.787604	9.063808
7.179181	661.510648	9.068826
7.223293	677.316195	9.073843
7.478720	664.984144	9.078861
7.273623	672.932229	9.083879
7.410480	671.599453	9.088896
7.623710	669.640683	9.093914
7.320862	671.708467	9.098931
7.468646	664.338820	9.103949
7.115627	654.430220	9.108967
7.379172	665.506012	9.113984
7.419074	662.504750	9.119002
7.257478	656.510271	9.124019
7.385872	657.796058	9.129037
7.638122	666.218375	9.134055
7.231630	662.089530	9.139072
7.098041	640.758697	9.144090
7.006138	653.506229	9.149107
7.163904	678.834885	9.154125
7.207573	673.952403	9.159143
7.025970	677.229563	9.164160
7.749388	666.778952	9.169178
7.291979	669.975017	9.174195
7.448948	673.875599	9.179213
7.753459	668.790487	9.184231
7.326610	666.173580	9.189248
7.669731	649.455243	9.194266
7.347260	668.183114	9.199283
7.575688	678.904123	9.204301
7.510845	665.636975	9.209319
7.116861	680.814325	9.214336
7.385686	672.729792	9.219354
7.487931	679.522725	9.224371
7.334523	672.598200	9.229389
7.383247	663.883623	9.234407
7.492395	667.869282	9.239424
7.422720	671.166487	9.244442
7.200135	672.774945	9.249459
7.196629	673.055865	9.254477
7.158182	664.108100	9.259495
7.233291	665.787727	9.264512
7.253273	663.638136	9.269530
7.519246	668.803659	9.274547
7.085583	668.222795	9.279565
7.804228	685.726387	9.284583
7.181596	686.122032	9.289600
7.302659	688.950282	9.294618
7.479966	694.237181	9.299635
7.570517	703.763394	9.304653
7.524609	699.426021	9.309671
7.417273	705.588355	9.314688
7.802134	707.882010	9.319706
7.675106	704.983180	9.324723
7.672132	701.590216	9.329741
7.981314	689.428760	9.334759
7.879480	694.904787	9.339776
7.785920	677.962289	9.344794
7.890991	672.184654	9.349811
7.479751	674.610917	9.354829
7.787313	659.483399	9.359847
7.210759	663.072397	9.364864
7.144147	669.381507	9.369882
7.547914	688.299757	9.374899
7.826678	693.213972	9.379917
7.792245	687.431087	9.384935
7.589375	683.715343	9.389952
7.400070	691.328953	9.394970
7.576763	696.269518	9.399987
7.597513	698.375448	9.405005
7.780458	684.599171	9.410023
7.388244	696.773669	9.415040
7.544617	695.520726	9.420058
7.634555	694.180364	9.425075
7.600428	695.903278	9.430093
7.686704	690.866106	9.435111
7.665727	698.808518	9.440128
8.084310	691.135372	9.445146
8.115060	694.988359	9.450163
7.638633	703.406167	9.455181
8.015737	691.947593	9.460199
7.554183	697.279655	9.465216
7.643809	698.005364	9.470234
7.928368	697.328009	9.475251
7.836700	704.617996	9.480269
7.639233	695.585134	9.485287
7.495869	702.773844	9.490304
7.763528	699.008133	9.495322
8.054891	691.846574	9.500339
8.006710	698.604585	9.505357
8.280444	692.968689	9.510375
7.814546	702.329972	9.515392
7.968671	694.917925	9.520410
7.565116	695.582787	9.525427
7.646052	701.506082	9.530445
8.190604	686.928236	9.535463
7.993980	697.022833	9.540480
7.889548	695.596160	9.545498
7.788157	687.966993	9.550515
7.927623	698.621256	9.555533
8.230996	685.698606	9.560551
7.814970	699.837167	9.565568
8.109382	690.926389	9.570586
7.979016	680.015214	9.575603
7.534072	673.888524	9.580621
7.877069	678.718874	9.585639
7.876668	694.699910	9.590656
7.994454	699.306944	9.595674
8.305040	697.771788	9.600691
7.707739	695.809442	9.605709
7.922456	698.613130	9.610727
7.910244	699.013990	9.615744
7.827750	690.810073	9.620762
8.009210	691.398535	9.625779
7.627792	689.766168	9.630797
7.998830	686.861635	9.635815
7.970813	699.412023	9.640832
7.882966	704.419623	9.645850
7.961342	700.831702	9.650867
7.778964	696.992490	9.655885
7.808123	694.009141	9.660903
7.742842	688.098301	9.665920
7.867654	697.682220	9.670938
7.791240	698.757451	9.675955
8.184479	699.197859	9.680973
8.061298	693.341484	9.685991
7.967943	695.534808	9.691008
8.194156	703.238271	9.696026
8.295845	696.526597	9.701043
7.788669	700.523775	9.706061
8.242143	700.242440	9.711079
7.891154	700.008887	9.716096
8.046255	702.914569	9.721114
8.321993	693.923422	9.726131
8.192492	701.786961	9.731149
8.351895	693.711482	9.736167
8.174125	700.742118	9.741184
7.921867	701.398462	9.746202
8.286900	692.927931	9.751219
8.037450	706.225184	9.756237
8.262905	695.947163	9.761255
8.310428	691.921466	9.766272
7.906229	702.168935	9.771290
8.000108	693.900774	9.776307
7.729685	717.617033	9.781325
8.097264	720.589890	9.786343
8.243557	732.060321	9.791360
8.140673	729.881856	9.796378
8.492609	725.314040	9.801395
8.190715	737.092533	9.806413
8.445622	729.057517	9.811431
8.605761	730.070353	9.816448
8.523854	720.338458	9.821466
8.381669	707.247064	9.826483
8.079883	711.849173	9.831501
8.318502	701.392601	9.836519
8.299578	703.992867	9.841536
8.341256	701.489700	9.846554
8.421232	705.040461	9.851571
8.312994	707.467340	9.856589
8.219923	705.405357	9.861607
8.009780	706.014179	9.866624
8.191649	718.735327	9.871642
8.807393	719.677050	9.876659
8.366852	715.165268	9.881677
8.160937	707.453406	9.886695
8.396222	706.194875	9.891712
8.239328	703.275402	9.896730
8.717034	714.742513	9.901747
8.284053	701.326857	9.906765
8.332820	700.517297	9.911783
8.356179	698.669487	9.916800
7.877990	704.336963	9.921818
8.432368	723.333854	9.926835
8.662756	725.986143	9.931853
8.416431	732.954528	9.936871
8.584178	724.351697	9.941888
8.581556	737.002628	9.946906
8.641941	724.009953	9.951923
8.226946	717.137778	9.956941
8.325150	715.070498	9.961959
8.511018	731.936029	9.966976
8.323053	732.415989	9.971994
8.617903	738.464891	9.977011
8.334018	734.752707	9.982029
8.367956	729.629313	9.987047
8.615892	724.825189	9.992064
8.538402	731.355011	9.997082
8.659228	724.980687	10.002099
8.430023	729.601884	10.007117
8.397852	721.029403	10.012135
8.702414	732.448037	10.017152
8.584833	735.321323	10.022170
8.843674	713.674636	10.027187
8.415767	722.220631	10.032205
8.515614	723.084011	10.037223
8.708979	727.633266	10.042240
8.587533	729.987142	10.047258
8.685886	722.592584	10.052275
8.791592	736.257407	10.057293
8.648723	720.058025	10.062311
8.578064	706.355217	10.067328
8.371340	726.331240	10.072346
8.754122	720.619800	10.077363
8.515464	723.623363	10.082381
8.747231	726.737208	10.087399
8.765578	725.152020	10.092416
8.700282	722.134704	10.097434
8.915954	719.666891	10.102451
8.691210	701.905587	10.107469
8.732296	690.416440	10.112487
8.542056	694.024541	10.117504
8.236548	699.163452	10.122522
8.482543	713.240038	10.127539
8.577777	726.512121	10.132557
8.551034	730.756899	10.137575
8.732392	722.573051	10.142592
8.414683	727.389206	10.147610
8.649036	725.308828	10.152627
8.913076	729.581042	10.157645
8.705337	731.327590	10.162663
8.757122	728.494416	10.167680
8.488355	733.120984	10.172698
8.840300	725.033683	10.177715
8.857891	726.187832	10.182733
8.550786	729.601920	10.187751
8.699200	728.931361	10.192768
8.387458	733.313484	10.197786
8.777380	728.898816	10.202803
8.819017	729.327372	10.207821
8.715877	728.492574	10.212839
8.962951	733.282135	10.217856
8.791727	744.105192	10.222874
8.996786	731.892839	10.227891
9.022591	732.399209	10.232909
8.645746	727.659960	10.237927
9.182226	727.231817	10.242944
8.648047	733.878992	10.247962
8.896243	727.723720	10.252979
8.527102	732.353917	10.257997
8.850091	747.098848	10.263015
9.354760	740.988499	10.268032
8.856071	757.307607	10.273050
9.168532	759.629006	10.278067
9.103568	739.847217	10.283085
8.718629	731.112290	10.288103
9.030305	735.898242	10.293120
8.984133	747.900919	10.298138
9.005190	738.703507	10.303155
9.180660	733.384244	10.308173
8.745139	742.307081	10.313191
9.429529	733.293910	10.318208
8.928967	731.409236	10.323226
8.899734	715.515039	10.328243
9.125690	718.188925	10.333261
8.845514	723.522062	10.338279
9.349698	725.478658	10.343296
9.037834	730.363134	10.348314
8.920593	729.533032	10.353331
8.685893	725.900496	10.358349
9.054297	750.583009	10.363367
9.678342	746.284678	10.368384
9.180262	735.217829	10.373402
9.028421	719.858861	10.378419
9.251651	728.258460	10.383437
9.188140	723.490948	10.388455
9.091943	714.050383	10.393472
9.217401	715.004004	10.398490
9.070294	715.428382	10.403507
9.270686	715.707822	10.408525
9.237209	726.648207	10.413543
9.381939	707.331314	10.418560
8.963364	720.864447	10.423578
9.122425	717.453702	10.428595
9.347727	710.917605	10.433613
9.041379	715.413784	10.438631
9.293737	713.155239	10.443648
9.144101	717.410915	10.448666
9.197803	704.979172	10.453683
9.447601	712.338990	10.458701
9.214191	709.619970	10.463719
9.527978	702.920021	10.468736
9.003236	720.772448	10.473754
8.991667	720.836213	10.478771
9.631351	714.523214	10.483789
9.326572	720.148989	10.488807
9.349049	719.319374	10.493824
9.043498	721.332890	10.498842
9.329841	715.405151	10.503859
9.233216	709.163292	10.508877
9.612900	720.900562	10.513895
9.905145	704.755911	10.518912
9.481460	703.713184	10.523930
9.350098	707.381614	10.528947
9.333276	702.969348	10.533965
9.183082	716.679677	10.538983
9.394086	707.256747	10.544000
9.090161	710.951784	10.549018
8.836101	712.103279	10.554035
9.066945	708.966460	10.559053
9.399336	729.870874	10.564071
9.729176	726.267291	10.569088
9.106272	718.773281	10.574106
9.338589	731.257753	10.579123
9.516370	739.017676	10.584141
9.472072	742.441789	10.589159
9.577328	741.485873	10.594176
9.631244	751.366981	10.599194
9.639598	729.214142	10.604211
9.312804	719.098807	10.609229
9.329457	731.876456	10.614247
9.727927	733.961181	10.619264
9.547942	726.173760	10.624282
9.464228	725.556598	10.629299
9.483957	726.659216	10.634317
9.526048	733.732984	10.639335
9.854898	730.673234	10.644352
9.592991	725.539777	10.649370
9.475116	710.046856	10.654387
9.426845	713.433040	10.659405
9.243908	729.887225	10.664423
9.442788	735.646130	10.669440
9.332480	746.309897	10.674458
9.625454	746.277174	10.679475
9.733848	740.248191	10.684493
9.657103	743.098575	10.689511
9.626063	744.926883	10.694528
9.735703	754.545631	10.699546
9.801086	747.051408	10.704563
9.908088	751.102401	10.709581
10.060177	746.141317	10.714599
9.676109	731.619959	10.719616
9.545606	716.449183	10.724634
9.385409	716.301746	10.729651
9.659661	724.231504	10.734669
9.479191	743.003664	10.739687
9.835672	739.844066	10.744704
9.997631	743.838716	10.749722
9.555575	746.400793	10.754739
9.630253	745.545998	10.759757
10.003323	748.815967	10.764775
9.838953	743.512032	10.769792
9.926248	744.903445	10.774810
9.558331	734.603975	10.779827
9.422362	736.644134	10.784845
9.259884	741.227908	10.789863
9.470748	741.901262	10.794880
9.286985	750.998151	10.799898
9.497857	747.834318	10.804915
9.654058	750.350085	10.809933
9.652702	745.460863	10.814951
9.672834	756.474277	10.819968
10.008831	760.758992	10.824986
9.922818	762.029113	10.830003
10.097031	747.139327	10.835021
9.855633	747.595854	10.840039
10.024582	743.869705	10.845056
9.761740	743.660135	10.850074
9.628978	746.897728	10.855091
10.059323	750.424340	10.860109
9.963010	754.866067	10.865127
9.690979	747.536765	10.870144
10.082621	763.157301	10.875162
9.947726	757.191430	10.880179
10.163756	758.648531	10.885197
9.879110	757.997715	10.890215
9.925011	749.416227	10.895232
10.071291	756.762895	10.900250
9.936694	758.634728	10.905267
10.292995	755.749945	10.910285
9.887431	753.392476	10.915303
10.010379	751.136458	10.920320
10.187645	743.417423	10.925338
9.868264	744.385654	10.930355
10.113078	741.124868	10.935373
10.024920	740.543873	10.940391
10.310171	742.649315	10.945408
10.117472	742.010438	10.950426
9.861985	742.452370	10.955443
9.966501	735.924453	10.960461
9.972899	751.487516	10.965479
10.256248	762.212480	10.970496
10.436785	760.696883	10.975514
10.146214	749.893284	10.980531
10.148661	742.431138	10.985549
9.947795	739.818528	10.990567
10.097681	747.760230	10.995584
10.636337	755.199790	11.000602
9.843741	753.899266	11.005619
9.995288	747.845025	11.010637
10.445743	758.842693	11.015655
10.242114	755.635296	11.020672
10.247660	745.708599	11.025690
10.298865	741.842901	11.030707
10.509184	731.228799	11.035725
10.185787	737.005293	11.040743
10.237076	731.099542	11.045760
10.162364	728.318022	11.050778
10.200480	735.995565	11.055795
10.225217	732.379907	11.060813
10.095654	743.841697	11.065831
10.342700	748.678116	11.070848
10.586939	762.230264	11.075866
10.166182	751.647816	11.080883
10.436558	746.959648	11.085901
10.299635	749.805826	11.090919
10.243083	746.929175	11.095936
10.233522	748.414182	11.100954
10.319947	761.644449	11.105971
10.541830	756.782428	11.110989
10.720947	762.200934	11.116007
10.496027	755.543711	11.121024
10.662840	745.807620	11.126042
10.358518	748.187451	11.131059
10.525748	731.764277	11.136077
10.384138	742.030492	11.141095
10.512122	737.564712	11.146112
10.545642	733.712967	11.151130
10.142847	742.463465	11.156147
10.617521	727.607405	11.161165
10.250498	741.776471	11.166183
10.114879	731.488141	11.171200
10.569322	738.995178	11.176218
10.569145	748.578566	11.181235
10.528039	737.601391	11.186253
10.389524	738.077100	11.191271
10.370772	749.342602	11.196288
10.823298	752.422654	11.201306
10.328640	754.338361	11.206323
10.588572	750.171577	11.211341
10.572882	756.798257	11.216359
10.658760	759.698090	11.221376
10.808269	765.023473	11.226394
10.285369	752.341126	11.231411
10.542277	764.234185	11.236429
10.668464	765.998273	11.241447
10.672616	765.197278	11.246464
10.867184	761.234218	11.251482
10.655593	755.421985	11.256499
10.344611	751.315093	11.261517
10.599846	752.351552	11.266535
10.874299	756.472451	11.271552
10.925471	757.438769	11.276570
10.496375	753.432139	11.281587
10.406825	752.410847	11.286605
10.626177	755.209842	11.291623
11.019033	761.341339	11.296640
10.878988	754.570461	11.301658
10.741588	759.732732	11.306675
10.612721	760.574934	11.311693
10.906390	760.767674	11.316711
10.874326	754.900124	11.321728
11.158536	749.658121	11.326746
10.532467	748.865820	11.331763
10.739986	737.712838	11.336781
10.966534	754.478749	11.341799
10.674612	751.778465	11.346816
10.582478	753.396037	11.351834
10.554795	761.615954	11.356851
10.439966	756.490808	11.361869
10.498863	754.680411	11.366887
10.903189	753.954484	11.371904
10.834747	754.106797	11.376922
10.903856	762.011491	11.381939
10.336299	756.733371	11.386957
11.130480	754.500450	11.391975
10.577726	757.719799	11.396992
10.644590	756.909602	11.402010
10.582262	765.653340	11.407027
11.007760	782.266659	11.412045
11.006214	785.635674	11.417063
11.087965	792.876515	11.422080
11.114388	778.098568	11.427098
10.866936	775.610590	11.432115
11.058239	774.998671	11.437133
11.152156	769.864151	11.442151
10.936832	765.564260	11.447168
11.036154	760.209963	11.452186
10.445291	767.607835	11.457203
10.833277	778.568620	11.462221
11.347777	787.540458	11.467239
10.855039	788.777148	11.472256
11.447196	790.081818	11.477274
11.390338	793.086391	11.482291
11.513473	783.854727	11.487309
11.397156	769.187034	11.492327
10.924932	765.485164	11.497344
10.801950	758.365809	11.502362
11.117133	757.206636	11.507379
11.432367	757.882786	11.512397
11.200374	749.826027	11.517415
10.923829	756.347877	11.522432
11.457985	749.885811	11.527450
11.192789	760.253206	11.532467
11.176492	754.090542	11.537485
11.383845	752.435868	11.542503
10.991465	763.255797	11.547520
11.051095	755.233419	11.552538
11.196692	758.835528	11.557555
11.025495	759.411132	11.562573
11.176889	764.748801	11.567591
11.094144	776.370570	11.572608
11.316389	771.600606	11.577626
11.090492	781.407207	11.582643
11.513232	787.853039	11.587661
11.447891	777.249908	11.592679
11.172713	792.539183	11.597696
11.393036	784.623638	11.602714
11.505811	787.262344	11.607731
11.499566	778.939461	11.612749
11.911600	774.510096	11.617767
11.620176	771.690047	11.622784
11.354830	751.678839	11.627802
11.161386	757.904269	11.632819
11.143925	745.534274	11.637837
11.439070	753.694826	11.642855
11.305203	753.821360	11.647872
11.348053	762.297299	11.652890
11.588472	768.887481	11.657907
11.553600	773.332425	11.662925
11.586222	766.378628	11.667943
11.480126	769.383082	11.672960
11.536687	748.793800	11.677978
11.301404	743.809070	11.682995
10.634018	757.155494	11.688013
11.752960	772.023754	11.693031
11.247001	776.074289	11.698048
11.930139	778.537844	11.703066
11.311723	772.521724	11.708083
11.407665	779.304329	11.713101
11.718113	771.610862	11.718119
11.387479	770.175183	11.723136
11.505368	774.312171	11.728154
11.684479	784.522550	11.733171
11.526160	779.613642	11.738189
11.597914	774.902059	11.743207
11.342007	778.209259	11.748224
11.964359	774.575338	11.753242
11.851782	780.704319	11.758259
11.735255	777.832869	11.763277
11.621702	783.525817	11.768295
11.293753	782.487309	11.773312
11.800441	776.835642	11.778330
11.676909	782.346394	11.783347
11.657713	779.300567	11.788365
11.683022	781.832896	11.793383
11.474592	792.592072	11.798400
11.597266	782.144015	11.803418
11.485734	790.834106	11.808435
11.719424	787.215724	11.813453
11.916586	780.917709	11.818471
11.824763	790.032859	11.823488
11.650534	780.854768	11.828506
11.534976	784.804835	11.833523
11.597762	783.796503	11.838541
12.109455	798.620074	11.843559
11.923186	807.045793	11.848576
11.621003	793.109999	11.853594
11.707761	799.140629	11.858611
11.558390	808.412950	11.863629
12.271774	803.628575	11.868647
12.071794	814.974526	11.873664
11.767689	804.587281	11.878682
12.017899	803.038885	11.883699
12.087982	812.018189	11.888717
12.083278	802.636432	11.893735
11.783724	789.818651	11.898752
12.093702	793.678967	11.903770
12.303241	796.365821	11.908787
11.765145	787.890069	11.913805
11.917575	774.124670	11.918823
11.827929	794.289651	11.923840
12.386708	798.028853	11.928858
12.571067	788.812244	11.933875
12.222720	781.055428	11.938893
12.279899	769.094686	11.943911
11.701497	776.098788	11.948928
12.019519	772.871146	11.953946
11.920796	777.138879	11.958963
11.848535	770.962249	11.963981
12.092237	764.608111	11.968999
11.948613	771.865790	11.974016
12.172990	789.054124	11.979034
12.262744	795.010638	11.984051
12.151733	796.853375	11.989069
12.247972	790.114219	11.994087
12.113419	786.178092	11.999104
12.269277	781.885234	12.004122
12.307217	775.800584	12.009139
11.919586	779.742162	12.014157
12.010256	783.672252	12.019175
12.266452	790.591309	12.024192
12.331722	798.254544	12.029210
12.510958	802.856552	12.034227
12.530164	798.695367	12.039245
12.413925	778.489758	12.044263
12.043169	773.121174	12.049280
12.110558	768.965796	12.054298
12.587473	777.503720	12.059315
12.127644	782.434365	12.064333
12.426540	782.362868	12.069351
12.382736	795.558827	12.074368
13.023106	788.224085	12.079386
12.539514	770.174479	12.084403
12.315021	768.924364	12.089421
12.204591	760.958487	12.094439
12.512527	761.537032	12.099456
12.153401	766.604926	12.104474
12.298963	752.088363	12.109491
12.261247	761.479561	12.114509
12.326473	766.977554	12.119527
12.711381	784.520775	12.124544
12.645412	779.650116	12.129562
12.448307	765.596165	12.134579
12.136535	766.507628	12.139597
12.623749	767.410011	12.144615
12.585829	782.212376	12.149632
12.515656	779.566702	12.154650
12.682466	771.433659	12.159667
12.362429	765.735436	12.164685
12.601589	770.728278	12.169703
12.549206	780.344345	12.174720
12.672221	778.628440	12.179738
12.580452	766.300259	12.184755
12.442153	778.241841	12.189773
12.434433	781.719745	12.194791
12.422683	788.433970	12.199808
12.861101	791.536443	12.204826
12.975732	791.683637	12.209843
12.519583	797.413242	12.214861
12.778613	795.255150	12.219879
12.999389	793.032925	12.224896
12.297013	784.143456	12.229914
12.498208	771.416385	12.234931
12.390786	787.268395	12.239949
12.717816	780.596926	12.244967
12.835108	795.841294	12.249984
12.739238	791.320839	12.255002
12.982004	789.576837	12.260019
12.842556	796.882653	12.265037
12.869985	795.883718	12.270055
12.651524	790.595416	12.275072
12.783038	797.682358	12.280090
13.045967	796.312949	12.285107
12.469429	794.430217	12.290125
12.746132	790.044516	12.295143
12.858596	792.199441	12.300160
12.539989	797.088598	12.305178
12.975389	792.010117	12.310195
12.534089	790.863613	12.315213
12.681203	791.211323	12.320231
13.004150	793.597917	12.325248
12.477715	792.956823	12.330266
12.964451	793.948258	12.335283
12.661928	793.278354	12.340301
13.107379	803.897770	12.345319
13.107234	802.273906	12.350336
12.805905	801.706948	12.355354
13.265219	794.830114	12.360371
12.675130	796.262048	12.365389
13.005840	812.710004	12.370407
13.311578	816.302538	12.375424
12.898618	821.633682	12.380442
13.337880	812.618144	12.385459
13.157924	809.246194	12.390477
13.235231	789.426611	12.395495
13.037475	795.487030	12.400512
12.953595	795.117518	12.405530
13.224403	789.781662	12.410547
13.166346	798.110166	12.415565
13.112566	792.625705	12.420583
13.141033	801.533553	12.425600
12.877755	808.353606	12.430618
13.249508	810.120735	12.435635
13.294672	827.206904	12.440653
13.271138	818.617191	12.445671
13.078860	824.349959	12.450688
12.953828	819.378049	12.455706
12.994405	821.733062	12.460723
13.230528	824.632830	12.465741
13.303269	817.151528	12.470759
13.302603	823.969439	12.475776
13.291883	816.370862	12.480794
13.721650	824.294210	12.485811
13.559427	825.615143	12.490829
13.684077	823.654881	12.495847
13.656557	806.439115	12.500864
13.286560	795.772644	12.505882
13.515433	792.442050	12.510899
13.018480	788.896623	12.515917
13.261564	787.626559	12.520935
13.469088	796.556326	12.525952
13.147784	809.993119	12.530970
13.591698	809.233471	12.535987
13.474185	830.171576	12.541005
13.385901	819.895427	12.546023
13.722176	821.219637	12.551040
13.072164	816.199625	12.556058
13.373182	816.741525	12.561075
13.598797	821.216574	12.566093
13.579125	829.411973	12.571111
13.432852	816.769565	12.576128
13.720990	815.466055	12.581146
13.828911	817.172941	12.586163
13.469366	813.944108	12.591181
13.401810	816.897310	12.596199
13.946543	820.884106	12.601216
13.491057	822.417764	12.606234
13.341125	810.536557	12.611251
13.359643	826.546879	12.616269
13.385427	822.303106	12.621287
13.859012	816.123863	12.626304
13.394983	818.486057	12.631322
13.542498	811.850599	12.636339
13.240752	811.594717	12.641357
13.323044	817.381226	12.646375
13.653862	813.262527	12.651392
13.401506	822.662927	12.656410
13.799476	816.592656	12.661427
13.772976	821.424397	12.666445
14.053265	830.100414	12.671463
13.923810	821.308172	12.676480
13.846471	824.099224	12.681498
14.002400	821.614518	12.686515
13.738203	821.535873	12.691533
13.761756	820.671430	12.696551
13.743931	815.547524	12.701568
13.607928	820.183234	12.706586
13.939878	820.090517	12.711603
14.029369	836.330028	12.716621
13.986351	823.466197	12.721639
14.134023	818.187727	12.726656
14.003884	827.329716	12.731674
13.911931	805.076454	12.736691
13.971117	809.206243	12.741709
13.965022	824.887978	12.746727
13.972192	806.441728	12.751744
13.979608	811.536339	12.756762
13.922738	805.950816	12.761779
13.945179	810.915386	12.766797
14.198520	812.599373	12.771815
14.178061	811.784342	12.776832
14.139479	813.561941	12.781850
14.184014	807.049830	12.786867
14.086459	820.385019	12.791885
14.209179	812.102964	12.796903
14.420907	807.332368	12.801920
13.537491	811.935546	12.806938
13.966496	812.725530	12.811955
14.000465	815.528069	12.816973
13.940146	820.588232	12.821991
14.226912	822.321013	12.827008
13.928173	840.782185	12.832026
14.239519	835.561642	12.837043
14.197058	839.708270	12.842061
14.095113	839.926364	12.847079
14.615249	835.911737	12.852096
14.677114	829.606186	12.857114
14.217674	823.099572	12.862131
14.201292	808.773937	12.867149
13.956485	802.271159	12.872167
14.280186	812.763899	12.877184
14.194601	833.151475	12.882202
14.446784	825.110561	12.887219
14.598932	834.732162	12.892237
14.347901	833.195899	12.897255
14.360581	823.617953	12.902272
14.456801	833.808235	12.907290
14.332072	825.188033	12.912307
14.486584	825.168002	12.917325
14.450743	832.674777	12.922343
14.654694	826.616159	12.927360
14.462348	814.913223	12.932378
14.421930	807.674273	12.937395
14.183210	807.890213	12.942413
14.127590	827.830324	12.947431
14.446517	829.934139	12.952448
14.213753	839.297842	12.957466
14.790479	829.567048	12.962483
14.633433	835.477836	12.967501
14.385545	833.962311	12.972519
14.554361	827.893369	12.977536
14.313872	833.339257	12.982554
14.557782	835.602338	12.987571
14.439820	837.134436	12.992589
14.401646	838.611591	12.997607
14.483673	842.885631	13.002624
14.583774	834.442751	13.007642
14.726518	834.717567	13.012659
14.507741	833.092503	13.017677
14.163717	838.227207	13.022695
14.759899	848.754375	13.027712
14.576296	856.006903	13.032730
14.880072	860.662319	13.037747
15.121097	855.182954	13.042765
14.538280	845.905560	13.047783
15.137928	844.487870	13.052800
14.716611	828.678559	13.057818
14.647786	829.728921	13.062835
15.115306	827.004440	13.067853
15.042064	828.370872	13.072871
15.117494	827.974585	13.077888
14.856129	839.862581	13.082906
14.564394	834.637969	13.087923
14.761379	835.945877	13.092941
14.647274	824.618541	13.097959
15.232347	845.921801	13.102976
14.612280	841.753079	13.107994
14.307561	851.100359	13.113011
14.920590	852.362997	13.118029
14.934735	863.203078	13.123047
15.068463	857.371813	13.128064
15.047418	864.140757	13.133082
15.205856	862.000494	13.138099
15.336209	864.153649	13.143117
14.865333	863.812785	13.148135
15.161904	861.850820	13.153152
14.828717	865.230281	13.158170
15.127953	862.737586	13.163187
15.322850	857.644975	13.168205
15.282557	862.651051	13.173223
15.412652	864.557016	13.178240
15.013893	849.640361	13.183258
15.134015	855.497387	13.188275
15.395515	856.618244	13.193293
15.011566	835.520715	13.198311
14.938051	843.038852	13.203328
15.295865	854.455059	13.208346
15.442588	856.355514	13.213363
15.523761	849.171998	13.218381
14.848418	838.204896	13.223399
15.037117	845.370968	13.228416
15.386257	857.815728	13.233434
15.100854	853.836062	13.238451
15.320707	860.668260	13.243469
15.044630	865.194507	13.248487
15.341597	856.894205	13.253504
15.370133	857.727670	13.258522
15.581109	859.837161	13.263539
15.233225	861.889592	13.268557
15.250452	860.088838	13.273575
15.816463	858.309020	13.278592
15.450071	862.260092	13.283610
15.254469	859.633993	13.288627
15.687244	861.411889	13.293645
15.431447	863.268766	13.298663
15.630009	861.230909	13.303680
15.521975	860.154406	13.308698
15.543066	851.223444	13.313715
15.689112	851.280402	13.318733
15.379083	868.033324	13.323751
15.547467	856.243854	13.328768
15.295487	860.606275	13.333786
15.328490	859.453665	13.338803
15.893292	855.041499	13.343821
15.617227	862.417603	13.348839
15.591169	859.564619	13.353856
15.519891	857.317127	13.358874
15.516384	862.382069	13.363891
15.314878	860.730915	13.368909
15.067387	866.263009	13.373927
15.209911	854.119967	13.378944
14.971797	870.631467	13.383962
15.367317	880.395466	13.388979
15.856674	882.847428	13.393997
16.189916	891.642659	13.399015
16.392536	886.329084	13.404032
16.271812	888.854117	13.409050
16.057383	880.318813	13.414067
15.949401	863.858790	13.419085
15.752236	867.425167	13.424103
15.841416	858.630950	13.429120
15.579510	854.758018	13.434138
15.520582	862.492242	13.439155
16.111772	872.620273	13.444173
16.168268	887.840155	13.449191
15.754941	870.761427	13.454208
15.718606	873.277995	13.459226
15.962177	884.985569	13.464243
16.180975	881.939682	13.469261
16.245828	881.310511	13.474279
15.785228	867.946524	13.479296
16.079822	856.547159	13.484314
15.741027	866.508723	13.489331
16.244612	871.636543	13.494349
16.088995	878.887991	13.499367
16.207525	873.767470	13.504384
16.301050	866.043344	13.509402
16.187447	859.692824	13.514419
16.358260	851.237832	13.519437
16.197182	845.083359	13.524455
16.190867	843.242413	13.529472
16.025867	845.581079	13.534490
15.947196	846.562210	13.539507
16.198163	841.964231	13.544525
16.091249	853.536126	13.549543
15.655942	847.761689	13.554560
16.057133	865.513320	13.559578
16.303571	878.935686	13.564595
16.447452	873.664911	13.569613
16.335797	878.072602	13.574631
16.378166	880.584406	13.579648
16.436565	878.892575	13.584666
16.311817	879.545921	13.589683
16.313353	869.317067	13.594701
16.081944	885.870385	13.599719
16.277305	882.946090	13.604736
16.709688	872.888399	13.609754
16.124804	883.952089	13.614771
16.446130	876.687457	13.619789
16.388688	883.764784	13.624807
16.596503	876.955936	13.629824
16.582479	870.855051	13.634842
16.527319	875.748637	13.639859
16.597669	875.079582	13.644877
16.214375	882.637616	13.649895
15.957562	882.206190	13.654912
16.618567	872.322445	13.659930
16.817785	886.829356	13.664947
16.648236	884.580023	13.669965
16.193075	879.233644	13.674983
16.499411	877.783816	13.680000
16.675697	872.515156	13.685018
16.461200	887.675191	13.690035
16.571252	878.503903	13.695053
16.617029	878.719583	13.700071
16.793152	879.756552	13.705088
16.703239	871.945875	13.710106
16.364992	875.017135	13.715123
16.477190	878.534650	13.720141
16.333212	884.410617	13.725159
16.844050	904.377889	13.730176
17.046269	902.859476	13.735194
16.605469	915.287848	13.740211
16.961162	904.417283	13.745229
16.960669	907.784969	13.750247
17.252324	907.538301	13.755264
16.809803	878.573611	13.760282
16.658922	883.430690	13.765299
16.590173	892.015727	13.770317
17.231755	895.302681	13.775335
16.993724	898.613245	13.780352
16.892433	894.651112	13.785370
16.820689	902.035525	13.790387
16.973357	902.263820	13.795405
16.853868	901.004180	13.800423
16.982789	905.011035	13.805440
17.107455	900.478832	13.810458
16.963425	902.925053	13.815475
17.266442	899.810889	13.820493
17.280425	902.289210	13.825511
16.912080	906.642960	13.830528
17.108639	901.905161	13.835546
17.128607	902.966414	13.840563
17.345278	898.681170	13.845581
17.108808	907.916006	13.850599
17.042963	901.580001	13.855616
17.294234	899.391685	13.860634
17.282316	902.534894	13.865651
17.330893	895.639418	13.870669
17.082348	893.200024	13.875687
17.107216	901.821531	13.880704
17.486942	895.668428	13.885722
16.997893	902.447170	13.890739
17.444812	901.613008	13.895757
17.344423	897.559390	13.900775
17.276869	906.247382	13.905792
17.405183	903.520791	13.910810
17.320439	906.052072	13.915827
17.227014	894.634257	13.920845
17.332716	899.067770	13.925863
17.014325	898.834721	13.930880
17.278713	887.613555	13.935898
17.399894	907.810700	13.940915
17.242499	900.537142	13.945933
17.157172	897.573893	13.950951
17.452598	899.266275	13.955968
17.469189	896.517241	13.960986
17.265990	907.310668	13.966003
16.968130	899.562755	13.971021
17.082795	911.778286	13.976039
17.365426	927.755608	13.981056
17.715152	918.275724	13.986074
17.671290	930.919470	13.991091
17.383455	917.866187	13.996109
17.713032	925.205024	14.001127
17.681266	925.579995	14.006144
17.620318	921.707233	14.011162
17.556457	925.117697	14.016179
17.644402	915.007964	14.021197
17.973681	914.191313	14.026215
17.831680	930.461775	14.031232
17.846588	919.422049	14.036250
17.748020	926.317237	14.041267
17.670387	931.146061	14.046285
18.113187	923.165656	14.051303
17.639014	915.691800	14.056320
17.783288	915.247499	14.061338
17.932587	928.234439	14.066355
17.935603	916.082560	14.071373
18.078035	920.023012	14.076391
17.908251	920.997976	14.081408
17.973062	916.288680	14.086426
18.152568	919.535622	14.091443
17.887425	919.924041	14.096461
17.842040	914.151546	14.101479
17.625600	912.166260	14.106496
18.244897	917.659564	14.111514
17.869900	918.380726	14.116531
17.576358	914.929140	14.121549
18.140364	908.865592	14.126567
17.942940	912.820980	14.131584
17.954676	912.326188	14.136602
17.981482	908.766443	14.141619
18.289413	909.686712	14.146637
18.194915	906.908829	14.151655
17.950666	913.899785	14.156672
17.920722	914.702781	14.161690
17.968354	911.471068	14.166707
18.347447	926.685206	14.171725
18.400230	911.823637	14.176743
17.944690	920.435337	14.181760
18.417937	934.554020	14.186778
18.390293	918.481406	14.191795
18.493526	917.410859	14.196813
18.452890	916.877104	14.201831
18.068565	919.932776	14.206848
18.182213	913.922933	14.211866
18.312707	927.344068	14.216883
18.025913	951.609434	14.221901
18.516598	942.814825	14.226919
18.135397	948.150988	14.231936
18.352031	951.259511	14.236954
18.286930	946.025678	14.241971
18.221085	953.398904	14.246989
18.465316	933.823531	14.252007
18.277064	950.026085	14.257024
18.458979	936.549742	14.262042
18.328196	950.808614	14.267059
18.326194	942.113697	14.272077
18.629901	934.132696	14.277095
18.375664	945.734172	14.282112
18.615883	927.453510	14.287130
18.605756	936.810719	14.292147
18.670642	938.045632	14.297165
18.899803	935.245646	14.302183
18.576927	936.062898	14.307200
18.723386	929.121673	14.312218
18.921634	943.508331	14.317235
18.625098	939.808821	14.322253
18.834337	928.613293	14.327271
18.798825	940.403734	14.332288
18.803908	937.554241	14.337306
19.181840	935.400063	14.342323
18.836113	930.986291	14.347341
18.998583	927.524151	14.352359
18.908950	926.621360	14.357376
18.780218	930.437825	14.362394
19.082857	924.393141	14.367411
18.716261	931.830329	14.372429
18.957393	933.212428	14.377447
18.999294	938.664346	14.382464
19.063190	930.240401	14.387482
19.106654	941.615028	14.392499
19.168607	939.322234	14.397517
19.086828	937.678805	14.402535
19.317027	933.625552	14.407552
19.371012	922.362827	14.412570
19.270324	929.920150	14.417587
19.135564	933.942329	14.422605
19.194861	923.558606	14.427623
18.829758	930.647137	14.432640
19.030319	926.862168	14.437658
18.960529	933.516384	14.442675
19.249017	927.551204	14.447693
19.204779	927.374328	14.452711
19.211124	933.453364	14.457728
19.231930	923.043339	14.462746
19.401140	930.731554	14.467763
18.987046	934.570076	14.472781
19.198632	933.531190	14.477799
19.148059	932.111324	14.482816
19.162581	938.555133	14.487834
19.402892	931.615689	14.492851
19.457247	934.460148	14.497869
19.661884	931.196134	14.502887
19.032065	934.125537	14.507904
19.311107	926.531284	14.512922
19.265009	927.896380	14.517939
19.241127	941.195065	14.522957
19.598195	943.553199	14.527975
19.820641	966.552428	14.532992
19.837936	942.011683	14.538010
19.586346	932.702222	14.543027
19.421122	930.272252	14.548045
19.567715	933.012072	14.553063
19.454031	932.839609	14.558080
19.317096	933.142234	14.563098
19.531503	929.104196	14.568115
19.592860	962.469399	14.573133
19.900147	961.182785	14.578151
19.541877	966.523425	14.583168
19.474501	960.592749	14.588186
19.638665	945.637510	14.593203
19.419973	962.047077	14.598221
19.544490	954.237070	14.603239
19.509413	965.366463	14.608256
19.413820	947.348461	14.613274
19.653778	951.785348	14.618291
19.591078	955.348376	14.623309
19.909700	944.539431	14.628327
19.853302	946.844382	14.633344
19.727017	947.588926	14.638362
19.811840	950.501174	14.643379
19.936921	952.357983	14.648397
20.111658	949.123718	14.653415
20.044263	952.784763	14.658432
19.790837	953.590516	14.663450
20.105023	953.965287	14.668467
19.853959	967.770490	14.673485
20.307933	970.607838	14.678503
20.389343	962.749455	14.683520
20.108129	953.684640	14.688538
20.178283	945.663176	14.693555
20.286055	948.559026	14.698573
20.313325	942.700870	14.703591
20.016297	945.482655	14.708608
19.917432	947.724562	14.713626
20.375093	946.251639	14.718643
20.061876	952.517450	14.723661
20.154550	945.127269	14.728679
20.100590	953.303610	14.733696
20.280561	959.674365	14.738714
20.190115	958.407943	14.743731
20.463845	975.763502	14.748749
20.416833	968.948386	14.753767
20.261175	964.139367	14.758784
20.284341	984.906756	14.763802
20.324716	978.643284	14.768819
20.253365	975.545428	14.773837
20.353235	978.297716	14.778855
20.410579	984.902558	14.783872
20.405299	978.943090	14.788890
20.648386	970.670546	14.793907
20.801123	974.305775	14.798925
20.557525	963.406456	14.803943
20.533862	975.416212	14.808960
20.326909	982.965173	14.813978
20.790654	971.637711	14.818995
20.524722	972.258536	14.824013
20.573117	964.045004	14.829031
20.819563	970.770096	14.834048
20.854571	977.103054	14.839066
20.858566	970.481845	14.844083
20.436308	977.757806	14.849101
20.875804	971.286915	14.854119
20.867537	980.055679	14.859136
20.906690	980.425994	14.864154
20.902120	957.769083	14.869171
20.770924	948.099534	14.874189
20.746991	940.750317	14.879207
20.748930	941.070890	14.884224
20.963434	957.294554	14.889242
21.010407	970.685070	14.894259
20.654619	962.059746	14.899277
20.842215	962.937348	14.904295
20.854811	965.922187	14.909312
20.854965	971.497954	14.914330
20.994624	974.224756	14.919347
20.836565	969.865327	14.924365
21.210612	958.937357	14.929383
21.393050	960.297289	14.934400
21.096436	966.274148	14.939418
21.144879	961.815570	14.944435
21.001815	971.083794	14.949453
21.312899	962.770863	14.954471
21.007207	966.561129	14.959488
21.035401	972.696009	14.964506
21.224766	971.530097	14.969523
21.310814	973.224875	14.974541
21.110115	973.528612	14.979559
21.439230	977.115345	14.984576
21.101399	976.034367	14.989594
21.310105	966.928183	14.994611
21.294913	969.610156	14.999629
21.115941	965.689999	15.004647
20.841234	966.213856	15.009664
20.621233	971.850486	15.014682
21.311010	968.138431	15.019699
21.160222	971.253863	15.024717
21.529630	969.907752	15.029735
21.594546	966.953862	15.034752
21.312588	973.042858	15.039770
21.398993	967.181988	15.044787
21.248196	962.339883	15.049805
21.295237	976.266985	15.054823
21.505184	981.860377	15.059840
21.506458	990.202781	15.064858
21.456503	979.555626	15.069875
21.159416	997.727746	15.074893
21.652355	984.255370	15.079911
21.802396	989.108321	15.084928
21.383122	992.178061	15.089946
21.582639	986.791347	15.094963
21.485971	988.892351	15.099981
21.653650	984.557718	15.104999
22.197751	989.542655	15.110016
21.833806	985.300381	15.115034
21.828037	984.865570	15.120051
21.662692	996.006713	15.125069
21.668861	988.961925	15.130087
21.749769	988.880463	15.135104
21.523878	994.831056	15.140122
21.482528	988.682682	15.145139
21.528768	997.445186	15.150157
21.792824	1019.259698	15.155175
21.787644	1018.887778	15.160192
21.762728	1016.534951	15.165210
22.075560	1020.881054	15.170227
22.318130	1015.627354	15.175245
22.477006	1013.790136	15.180263
22.501270	1016.951392	15.185280
22.063258	1013.337492	15.190298
22.162627	996.763076	15.195315
22.066692	992.332332	15.200333
22.163387	992.244319	15.205351
22.118590	984.303284	15.210368
21.756813	991.125554	15.215386
22.067140	1002.455644	15.220403
22.628017	1010.720357	15.225421
22.512758	1014.205097	15.230439
22.559552	997.578758	15.235456
22.323760	989.833512	15.240474
22.584876	978.799824	15.245491
22.371576	984.164494	15.250509
22.082071	985.106138	15.255527
22.199430	982.404180	15.260544
22.115750	985.232137	15.265562
22.122116	1000.208472	15.270579
22.348287	1011.191888	15.275597
22.195819	1010.475080	15.280615
22.476825	1012.347020	15.285632
22.473488	1015.879761	15.290650
22.510948	1008.612862	15.295667
22.692487	1008.467101	15.300685
22.642964	1005.773875	15.305703
23.113319	1004.207904	15.310720
22.810670	1005.295027	15.315738
22.924714	1006.342286	15.320755
23.003945	999.873954	15.325773
22.535663	989.192128	15.330791
22.838876	975.912191	15.335808
22.597694	985.260054	15.340826
22.621615	972.999161	15.345843
23.138002	996.066293	15.350861
23.077743	985.407061	15.355879
22.996416	976.698095	15.360896
22.589321	965.136505	15.365914
22.819700	964.006714	15.370931
23.089258	976.211215	15.375949
22.707873	964.594190	15.380967
22.995730	968.841268	15.385984
22.815022	972.013228	15.391002
23.180101	968.940347	15.396019
22.911019	965.719728	15.401037
22.920856	968.101899	15.406055
23.184090	974.266363	15.411072
23.126009	975.930678	15.416090
23.072420	968.556831	15.421107
23.071285	973.853691	15.426125
22.915940	972.075594	15.431143
23.245434	974.773719	15.436160
22.984308	995.846848	15.441178
23.342105	993.603875	15.446195
22.864745	1002.097190	15.451213
23.073985	1008.126125	15.456231
23.176289	1000.177653	15.461248
23.005320	1002.622051	15.466266
23.144971	1003.449329	15.471283
23.042379	1009.742489	15.476301
23.202528	1005.658299	15.481319
23.332953	1008.668909	15.486336
23.213959	1004.422288	15.491354
23.359082	1004.293581	15.496371
23.409540	1006.347391	15.501389
23.098457	1009.052776	15.506407
23.616218	1012.822840	15.511424
23.408824	1016.888562	15.516442
23.457984	1020.910230	15.521459
23.552159	1025.597647	15.526477
23.183655	1034.636320	15.531495
23.476874	1031.079675	15.536512
23.521509	1038.450001	15.541530
23.646175	1031.373367	15.546547
23.770066	1025.153526	15.551565
23.446107	1035.250923	15.556583
23.875935	1030.048097	15.561600
23.698023	1026.750561	15.566618
23.582407	1034.282061	15.571635
23.813742	1034.894561	15.576653
23.357372	1035.496135	15.581671
23.598376	1030.702908	15.586688
23.596199	1035.348017	15.591706
24.075302	1038.706000	15.596723
23.833374	1028.776006	15.601741
23.533813	1024.225434	15.606759
24.010181	1027.900390	15.611776
24.080208	1034.740546	15.616794
23.848593	1029.590948	15.621811
24.363965	1033.158270	15.626829
24.077869	1027.653534	15.631847
23.997676	1028.067628	15.636864
24.132383	1030.967695	15.641882
24.028349	1034.024612	15.646899
24.044448	1026.281338	15.651917
23.887562	1032.255951	15.656935
23.856538	1025.128332	15.661952
24.078073	1033.893719	15.666970
24.051074	1047.131596	15.671987
24.333672	1060.944181	15.677005
24.384834	1061.614468	15.682023
24.457643	1048.297034	15.687040
24.220718	1049.279186	15.692058
24.286372	1055.412227	15.697075
24.540801	1046.542905	15.702093
24.167345	1055.110379	15.707111
24.656049	1056.995964	15.712128
24.683484	1056.628878	15.717146
24.257520	1035.388824	15.722163
24.447301	1029.454910	15.727181
24.412412	1047.313997	15.732199
24.414486	1044.559861	15.737216
24.026579	1049.514899	15.742234
24.571425	1042.222628	15.747251
24.584959	1043.468808	15.752269
24.168896	1053.779100	15.757287
24.411373	1040.699709	15.762304
24.323630	1050.319043	15.767322
24.491132	1049.444137	15.772339
24.735548	1056.383374	15.777357
24.586201	1054.441682	15.782375
24.574673	1042.645249	15.787392
24.707105	1057.283455	15.792410
24.616011	1058.907578	15.797427
25.141636	1059.058372	15.802445
24.968876	1064.212820	15.807463
25.311405	1057.370957	15.812480
25.022048	1050.429797	15.817498
25.243172	1050.573533	15.822515
25.185596	1038.079636	15.827533
25.006978	1043.500392	15.832551
25.151212	1041.533317	15.837568
25.281339	1045.953774	15.842586
25.336268	1043.466860	15.847603
25.212967	1038.409162	15.852621
25.173759	1038.578683	15.857639
25.492512	1041.935660	15.862656
25.206142	1043.220477	15.867674
25.221514	1040.405874	15.872691
25.153167	1036.261484	15.877709
25.221640	1047.050967	15.882727
25.236549	1034.735614	15.887744
25.083159	1040.831300	15.892762
24.939929	1042.056590	15.897779
25.317127	1039.440726	15.902797
25.321814	1044.524842	15.907815
25.305030	1039.097945	15.912832
25.373452	1047.414301	15.917850
25.291338	1050.098315	15.922867
25.363973	1042.784631	15.927885
25.267983	1045.449683	15.932903
25.355825	1034.865102	15.937920
25.247244	1041.302569	15.942938
25.166108	1042.823470	15.947955
25.431497	1041.902042	15.952973
24.933267	1045.020691	15.957991
25.442966	1051.447119	15.963008
25.607491	1053.490710	15.968026
25.622453	1057.673949	15.973043
25.531694	1059.428721	15.978061
25.538187	1060.820551	15.983079
25.663833	1062.146197	15.988096
25.784697	1060.832966	15.993114
25.490980	1058.264021	15.998131
25.812799	1061.439793	16.003149
25.725330	1064.584915	16.008167
25.684189	1052.698499	16.013184
25.675597	1053.988500	16.018202
25.219810	1057.524911	16.023219
25.828299	1057.117123	16.028237
25.852815	1074.883731	16.033255
26.187247	1081.268723	16.038272
26.386296	1080.745666	16.043290
26.174987	1067.780761	16.048307
26.250139	1057.610851	16.053325
25.923163	1052.822298	16.058343
25.962775	1053.455915	16.063360
25.756330	1060.544217	16.068378
25.503331	1074.080553	16.073395
25.925510	1083.026123	16.078413
25.941431	1091.177186	16.083431
25.901724	1086.363890	16.088448
25.942121	1094.736879	16.093466
25.821844	1103.588824	16.098483
26.379452	1092.592965	16.103501
26.042429	1104.303540	16.108519
26.267499	1112.180620	16.113536
26.555633	1116.017078	16.118554
26.748370	1115.173815	16.123571
26.461258	1099.086893	16.128589
26.764050	1086.772647	16.133607
26.745767	1082.021944	16.138624
26.677018	1069.556642	16.143642
26.323429	1085.959151	16.148659
26.760487	1083.523519	16.153677
26.357494	1086.139809	16.158695
26.479249	1085.391370	16.163712
26.608670	1083.229505	16.168730
26.622955	1088.758488	16.173747
26.714925	1078.296025	16.178765
26.527252	1081.811667	16.183783
26.653860	1090.608946	16.188800
27.018482	1090.791912	16.193818
26.611354	1104.135693	16.198835
26.618362	1093.268011	16.203853
26.696570	1105.252339	16.208871
26.883404	1107.611917	16.213888
27.235138	1105.960070	16.218906
26.900116	1102.199572	16.223923
26.793991	1089.929019	16.228941
26.865154	1104.615996	16.233959
27.093413	1107.024618	16.238976
26.990601	1110.778175	16.243994
26.976590	1117.409456	16.249011
27.114050	1116.142289	16.254029
27.016588	1115.616361	16.259047
27.069626	1125.241957	16.264064
27.320248	1107.797916	16.269082
26.990713	1115.174331	16.274099
27.542320	1110.087137	16.279117
27.490764	1114.936897	16.284135
27.323827	1092.770831	16.289152
27.234813	1084.226850	16.294170
27.142166	1086.608688	16.299187
27.197647	1092.851692	16.304205
27.256324	1102.542873	16.309223
27.277842	1107.634066	16.314240
27.311224	1103.997205	16.319258
27.278597	1108.543445	16.324275
27.414732	1102.268790	16.329293
27.487853	1105.380637	16.334311
27.061053	1107.715449	16.339328
27.493786	1094.298615	16.344346
27.158562	1109.019030	16.349363
27.507968	1105.793604	16.354381
27.400423	1108.746003	16.359399
27.501134	1106.085363	16.364416
27.599594	1108.428473	16.369434
27.297866	1114.803860	16.374451
27.692352	1130.960110	16.379469
27.773773	1127.872358	16.384487
27.726442	1137.480724	16.389504
28.147310	1128.651116	16.394522
27.615250	1131.680111	16.399539
27.884290	1122.681558	16.404557
28.137093	1124.253862	16.409575
28.018124	1129.210061	16.414592
28.240588	1127.968188	16.419610
28.068933	1122.834219	16.424627
27.930920	1101.801504	16.429645
28.052771	1125.460913	16.434663
28.100749	1124.579417	16.439680
28.167807	1110.093627	16.444698
27.847510	1116.224460	16.449715
27.932755	1123.923131	16.454733
27.988710	1125.622515	16.459751
27.789747	1127.428675	16.464768
27.803841	1120.493140	16.469786
27.885755	1117.296651	16.474803
28.125128	1120.406562	16.479821
28.254477	1125.690529	16.484839
27.556985	1127.478846	16.489856
28.219606	1135.938585	16.494874
28.379739	1144.320907	16.499891
28.738621	1147.467726	16.504909
28.749010	1151.247823	16.509927
28.407227	1142.740153	16.514944
28.765865	1141.792650	16.519962
28.425126	1130.108928	16.524979
28.428109	1131.717087	16.529997
28.545368	1135.231855	16.535015
28.455500	1142.966617	16.540032
29.064020	1141.254138	16.545050
28.667859	1140.844596	16.550067
28.585315	1125.047778	16.555085
28.679216	1124.414182	16.560103
28.703024	1143.254968	16.565120
29.146540	1136.784132	16.570138
28.761474	1127.533266	16.575155
28.987630	1119.422497	16.580173
28.846529	1107.851794	16.585191
28.588362	1120.920144	16.590208
28.429788	1107.764196	16.595226
28.740900	1129.083687	16.600243
28.989971	1146.836423	16.605261
29.177170	1141.951287	16.610279
28.980074	1140.290317	16.615296
29.224140	1148.089076	16.620314
29.013442	1144.078461	16.625331
29.062537	1140.547254	16.630349
29.331578	1137.927630	16.635367
29.230764	1144.390230	16.640384
29.569376	1140.307557	16.645402
29.044256	1131.858202	16.650419
29.163929	1135.860744	16.655437
29.191040	1137.899147	16.660455
29.060602	1146.520917	16.665472
29.323215	1139.291869	16.670490
29.244733	1139.340339	16.675507
29.442042	1134.761789	16.680525
29.319335	1139.641053	16.685543
28.964757	1144.460291	16.690560
29.398541	1148.271065	16.695578
29.117680	1141.200115	16.700595
28.987512	1136.020691	16.705613
29.308059	1139.856906	16.710631
29.191704	1161.578315	16.715648
29.722401	1168.415083	16.720666
29.495012	1165.140669	16.725683
29.643859	1166.391619	16.730701
29.950557	1170.808070	16.735719
29.837494	1172.233880	16.740736
29.743832	1165.627970	16.745754
30.030054	1174.283910	16.750771
29.922830	1161.762702	16.755789
30.042627	1160.795298	16.760807
29.625890	1167.324392	16.765824
29.668597	1165.820162	16.770842
29.671741	1172.286819	16.775859
29.704035	1166.791123	16.780877
29.864067	1164.807244	16.785895
29.947564	1162.721474	16.790912
29.726744	1161.927790	16.795930
30.213317	1154.951800	16.800947
29.648160	1162.520791	16.805965
30.163139	1153.954712	16.810983
29.930515	1170.727425	16.816000
30.249002	1163.341088	16.821018
30.001258	1178.470692	16.826035
30.245085	1182.808190	16.831053
30.610251	1179.945484	16.836071
30.304578	1176.984809	16.841088
30.369547	1155.782193	16.846106
30.428553	1154.452820	16.851123
30.053566	1158.306967	16.856141
30.616555	1156.076844	16.861159
30.685820	1182.251271	16.866176
30.588077	1163.972355	16.871194
30.598152	1160.894049	16.876211
30.326028	1147.277355	16.881229
30.506220	1145.997599	16.886247
30.602070	1155.168501	16.891264
30.689000	1155.533272	16.896282
30.499671	1159.319670	16.901299
30.543110	1178.388344	16.906317
30.854083	1172.822485	16.911335
30.892336	1185.720158	16.916352
30.722424	1179.216236	16.921370
30.775562	1185.504546	16.926387
30.732260	1184.541707	16.931405
30.909425	1177.006721	16.936423
30.542032	1182.426107	16.941440
30.951585	1181.504422	16.946458
30.984656	1179.614396	16.951475
30.667477	1184.839647	16.956493
31.268822	1175.516756	16.961511
31.251153	1182.588421	16.966528
31.119369	1186.232231	16.971546
31.389908	1188.999997	16.976563
31.190819	1182.381222	16.981581
31.509750	1174.644422	16.986599
30.871506	1180.386994	16.991616
31.064162	1182.223587	16.996634
30.858977	1173.045268	17.001651
30.871732	1186.951466	17.006669
30.741568	1179.212650	17.011687
30.498682	1180.922942	17.016704
30.943028	1197.115492	17.021722
31.240583	1207.414805	17.026739
31.326335	1216.900006	17.031757
31.714013	1199.702845	17.036775
31.435906	1211.410437	17.041792
31.820311	1209.376015	17.046810
31.767936	1205.259642	17.051827
31.544254	1203.379845	17.056845
32.000220	1196.549845	17.061863
31.852174	1200.598702	17.066880
32.100767	1204.096070	17.071898
31.966067	1186.010250	17.076915
31.471468	1183.278488	17.081933
31.931566	1169.868869	17.086951
31.598215	1173.447235	17.091968
31.727514	1173.709718	17.096986
32.223263	1186.637148	17.102003
32.095697	1190.267268	17.107021
31.674561	1174.117421	17.112039
31.934624	1186.381534	17.117056
32.470436	1194.410348	17.122074
32.102641	1175.880472	17.127091
31.755246	1170.126787	17.132109
31.964632	1164.154143	17.137127
31.590596	1179.633391	17.142144
31.786975	1187.310149	17.147162
32.341468	1196.367731	17.152179
31.792772	1208.321302	17.157197
31.858591	1194.119883	17.162215
32.040114	1191.145068	17.167232
31.984699	1197.055305	17.172250
32.354759	1206.235162	17.177267
32.058300	1204.613472	17.182285
32.446472	1219.512626	17.187303
32.497653	1223.345828	17.192320
32.300703	1227.515779	17.197338
32.896294	1216.078122	17.202355
33.007659	1222.788291	17.207373
32.711605	1209.072359	17.212391
32.434913	1198.227563	17.217408
32.608988	1197.928317	17.222426
32.599929	1192.273321	17.227443
32.347934	1197.576757	17.232461
32.576118	1200.749165	17.237479
32.719266	1215.423541	17.242496
32.628112	1221.596392	17.247514
32.882638	1224.714838	17.252531
32.907761	1225.302438	17.257549
33.156233	1216.868246	17.262567
33.169077	1221.710525	17.267584
32.916791	1209.597934	17.272602
33.188086	1197.833290	17.277619
32.832038	1197.533636	17.282637
33.114995	1190.418122	17.287655
32.701234	1202.311550	17.292672
32.976224	1205.354559	17.297690
32.898950	1214.729355	17.302707
32.609556	1219.940962	17.307725
32.955972	1220.943459	17.312743
32.909246	1217.514713	17.317760
32.909486	1224.555874	17.322778
33.284827	1219.997031	17.327795
33.013154	1226.098596	17.332813
33.225652	1216.687315	17.337831
33.113944	1232.001134	17.342848
33.221714	1245.434577	17.347866
33.498000	1242.687362	17.352883
33.143082	1255.980896	17.357901
33.423387	1248.101246	17.362919
33.368838	1246.322175	17.367936
33.266637	1244.680125	17.372954
33.436783	1244.595303	17.377971
32.948972	1241.458086	17.382989
33.092367	1254.801781	17.388007
33.731703	1269.240115	17.393024
33.692547	1273.473711	17.398042
33.600568	1264.314781	17.403059
33.586836	1268.291023	17.408077
33.929898	1268.001195	17.413095
34.441977	1262.573655	17.418112
34.391640	1260.471451	17.423130
34.501365	1259.782081	17.428147
34.198592	1250.185239	17.433165
34.087185	1239.851616	17.438183
34.393843	1238.919014	17.443200
34.235250	1233.435216	17.448218
34.272457	1235.802267	17.453235
34.047743	1235.481260	17.458253
34.264631	1226.118064	17.463271
34.056249	1231.342637	17.468288
34.029383	1233.536838	17.473306
34.216271	1217.652400	17.478323
34.289586	1221.750040	17.483341
34.338266	1227.459593	17.488359
34.289992	1231.159268	17.493376
34.121299	1235.876890	17.498394
34.540314	1242.634943	17.503411
34.732116	1263.947606	17.508429
34.455704	1256.817599	17.513447
34.608175	1255.135347	17.518464
34.324353	1250.943902	17.523482
34.815657	1252.123981	17.528499
34.457709	1256.291858	17.533517
34.649280	1256.589700	17.538535
34.660790	1261.860943	17.543552
34.651797	1265.033268	17.548570
34.603711	1263.027933	17.553587
34.572228	1269.027540	17.558605
34.877191	1258.228907	17.563623
34.615228	1261.411623	17.568640
34.442702	1266.516495	17.573658
34.629888	1264.848966	17.578675
34.677305	1261.951459	17.583693
34.683982	1270.397842	17.588711
34.866075	1288.565760	17.593728
34.830230	1292.565354	17.598746
35.129857	1288.258000	17.603763
35.123676	1291.953082	17.608781
35.368453	1292.311798	17.613799
35.267561	1283.900773	17.618816
35.302723	1290.961378	17.623834
35.441923	1288.343545	17.628851
35.427235	1290.260152	17.633869
35.489907	1289.756914	17.638887
35.338140	1290.191920	17.643904
35.448618	1287.088302	17.648922
35.517770	1280.594751	17.653939
35.752884	1288.260815	17.658957
35.563360	1289.462293	17.663975
35.744156	1283.767953	17.668992
35.463052	1287.571154	17.674010
35.718949	1290.213413	17.679027
35.601820	1293.011925	17.684045
35.269218	1287.154567	17.689063
35.821688	1287.177695	17.694080
35.601508	1286.041780	17.699098
35.643241	1281.870041	17.704115
35.402110	1279.315973	17.709133
35.038487	1288.255954	17.714151
35.964577	1287.223144	17.719168
35.691585	1305.519191	17.724186
36.202183	1301.706417	17.729203
36.146543	1310.508015	17.734221
36.008305	1316.908774	17.739239
36.326861	1302.418956	17.744256
35.758255	1301.472226	17.749274
36.352196	1297.973599	17.754291
36.483401	1311.615419	17.759309
36.208346	1304.337924	17.764327
36.338535	1288.907675	17.769344
36.188314	1299.434733	17.774362
36.391969	1298.327848	17.779379
36.340890	1314.248232	17.784397
36.269208	1307.178001	17.789415
36.736292	1304.247218	17.794432
36.665720	1314.309139	17.799450
36.734899	1301.078307	17.804467
36.470113	1284.936706	17.809485
36.163729	1284.950867	17.814503
36.895985	1295.415264	17.819520
36.735973	1307.383683	17.824538
36.574713	1293.820942	17.829555
36.431420	1303.735845	17.834573
36.724508	1296.267038	17.839591
37.051696	1295.803464	17.844608
36.787432	1304.062449	17.849626
36.878727	1301.645849	17.854643
36.937370	1300.233454	17.859661
36.961416	1304.366045	17.864679
37.166944	1294.682255	17.869696
36.812259	1306.973846	17.874714
36.730911	1295.734833	17.879731
36.853540	1308.341084	17.884749
36.731013	1305.605958	17.889767
36.922157	1295.713136	17.894784
36.815629	1295.520979	17.899802
36.867280	1312.675507	17.904819
37.233638	1323.652862	17.909837
36.872267	1332.362185	17.914855
37.374007	1327.946159	17.919872
37.359688	1335.680712	17.924890
37.298320	1325.418273	17.929907
37.563840	1322.093704	17.934925
37.081218	1327.976699	17.939943
37.435221	1322.281224	17.944960
37.516721	1335.343905	17.949978
37.579779	1325.966358	17.954995
37.671601	1328.810592	17.960013
37.670820	1329.425712	17.965031
37.782508	1316.520106	17.970048
37.878995	1330.151943	17.975066
37.709219	1323.750297	17.980083
37.578040	1320.093391	17.985101
37.405347	1319.388184	17.990119
37.773505	1318.393820	17.995136
37.749024	1320.480159	18.000154
37.685883	1326.296452	18.005171
37.967968	1344.110483	18.010189
37.830891	1352.259065	18.015207
37.990196	1341.822283	18.020224
38.153923	1342.541658	18.025242
38.096308	1352.421147	18.030259
38.035598	1351.364725	18.035277
38.144698	1357.047786	18.040295
38.235578	1350.159276	18.045312
38.132681	1352.117268	18.050330
37.955444	1346.497543	18.055347
38.114783	1349.721539	18.060365
38.330389	1351.236642	18.065383
38.223862	1346.896525	18.070400
38.031006	1365.897471	18.075418
38.176035	1377.409930	18.080435
38.490956	1377.681050	18.085453
38.669519	1373.779540	18.090471
39.061661	1364.511650	18.095488
39.052714	1370.484730	18.100506
38.738744	1365.084880	18.105523
38.814126	1366.372813	18.110541
38.906640	1371.038564	18.115559
39.109931	1371.125022	18.120576
39.278132	1373.678275	18.125594
39.321003	1350.565302	18.130611
38.923599	1343.391510	18.135629
38.936037	1342.472581	18.140647
39.623950	1333.726591	18.145664
38.921339	1335.864588	18.150682
38.798301	1337.090494	18.155699
39.141421	1328.757497	18.160717
38.870650	1333.158592	18.165735
39.047300	1329.286936	18.170752
38.899826	1342.663516	18.175770
39.273555	1358.423844	18.180787
39.382396	1361.950293	18.185805
39.286499	1375.304582	18.190823
39.243913	1371.020405	18.195840
39.577088	1363.726815	18.200858
39.345440	1367.841919	18.205875
39.599452	1366.015286	18.210893
39.659537	1367.202210	18.215911
39.573473	1373.629786	18.220928
39.772740	1375.350744	18.225946
39.524761	1366.261677	18.230963
39.448744	1365.438494	18.235981
39.508314	1374.422229	18.240999
39.758422	1357.145707	18.246016
39.802364	1363.659625	18.251034
39.878950	1369.181935	18.256051
39.730136	1366.411782	18.261069
39.426869	1370.622996	18.266087
39.637561	1370.977122	18.271104
39.862962	1370.727641	18.276122
39.742762	1382.320240	18.281139
40.062058	1379.154863	18.286157
39.918667	1386.025394	18.291175
40.001792	1386.424265	18.296192
39.805467	1384.848965	18.301210
39.751902	1379.663075	18.306227
40.147586	1393.731246	18.311245
39.825064	1390.444190	18.316263
40.059835	1402.146135	18.321280
40.087493	1408.142303	18.326298
40.552152	1408.265010	18.331315
40.969174	1407.542861	18.336333
40.574185	1419.345553	18.341351
40.444782	1402.469610	18.346368
40.532516	1406.408615	18.351386
40.678205	1399.066919	18.356403
40.960420	1399.472982	18.361421
40.440231	1401.674088	18.366439
40.712070	1395.797706	18.371456
40.907488	1395.380358	18.376474
41.085190	1401.079241	18.381491
41.127692	1401.484052	18.386509
40.916008	1405.640741	18.391527
41.004278	1403.346278	18.396544
41.039393	1399.638196	18.401562
40.939298	1403.725621	18.406579
41.241576	1393.824965	18.411597
40.938723	1393.576339	18.416615
41.449065	1394.958787	18.421632
41.419208	1392.753175	18.426650
41.030315	1398.825399	18.431667
41.031025	1389.848288	18.436685
40.858631	1396.336624	18.441703
40.897547	1389.420875	18.446720
41.123480	1397.934564	18.451738
40.998252	1398.330140	18.456755
41.446540	1410.504998	18.461773
41.506343	1422.006405	18.466791
41.552731	1423.221192	18.471808
41.519249	1423.637404	18.476826
41.070654	1431.518321	18.481843
41.467801	1425.198350	18.486861
41.483546	1425.009567	18.491879
41.802751	1430.597238	18.496896
41.955557	1428.098780	18.501914
42.111059	1425.661687	18.506931
41.980065	1419.166967	18.511949
41.562513	1426.249051	18.516967
41.646364	1420.765987	18.521984
41.981628	1415.734597	18.527002
42.053461	1413.472381	18.532019
42.268186	1420.794648	18.537037
42.024925	1423.685721	18.542055
42.006566	1438.178391	18.547072
42.232106	1452.711399	18.552090
42.120356	1454.368116	18.557107
42.708025	1448.608709	18.562125
42.308196	1451.793425	18.567143
42.098645	1449.845903	18.572160
42.561519	1445.029198	18.577178
42.205708	1452.949093	18.582195
42.665239	1446.500675	18.587213
42.558664	1442.867618	18.592231
42.600132	1444.203298	18.597248
42.356945	1450.808102	18.602266
42.505317	1443.229724	18.607283
42.635058	1439.008726	18.612301
42.207462	1442.172447	18.617319
42.481476	1444.167253	18.622336
42.763117	1434.923523	18.627354
42.520204	1439.838140	18.632371
42.538644	1446.407496	18.637389
42.912482	1461.378549	18.642407
43.119997	1463.362715	18.647424
42.988962	1469.046603	18.652442
43.020903	1473.655880	18.657459
43.262218	1455.998424	18.662477
43.230856	1463.089020	18.667495
43.216129	1458.366746	18.672512
43.604419	1451.443906	18.677530
43.236118	1457.877306	18.682547
43.567308	1453.920188	18.687565
43.551704	1453.078729	18.692583
43.575314	1448.627273	18.697600
43.647708	1449.343667	18.702618
43.722708	1447.067142	18.707635
43.734085	1448.076314	18.712653
43.715129	1445.296848	18.717671
43.258188	1433.926226	18.722688
43.687276	1438.531544	18.727706
43.718371	1454.626653	18.732723
44.026658	1451.890245	18.737741
43.829821	1456.505508	18.742759
43.815196	1458.006775	18.747776
44.200601	1457.051280	18.752794
43.721862	1458.296327	18.757811
44.008225	1453.702151	18.762829
43.841016	1457.114097	18.767847
43.846642	1450.253438	18.772864
44.005477	1445.319754	18.777882
43.922032	1451.602443	18.782899
44.070467	1448.077158	18.787917
44.111970	1450.953762	18.792935
44.112054	1445.475504	18.797952
44.055028	1442.660611	18.802970
44.175510	1456.934249	18.807987
44.321797	1468.461922	18.813005
44.193531	1483.661016	18.818023
44.289781	1489.368695	18.823040
44.714095	1482.395783	18.828058
44.378688	1486.818647	18.833075
44.358161	1481.955989	18.838093
44.572260	1484.810319	18.843111
44.413968	1485.553101	18.848128
44.777498	1484.898074	18.853146
44.344648	1482.940277	18.858163
44.678419	1495.166054	18.863181
44.703272	1509.878013	18.868199
45.149302	1511.777417	18.873216
45.486786	1499.247260	18.878234
45.277694	1512.224350	18.883251
45.198279	1501.875805	18.888269
44.994708	1481.934915	18.893287
45.254151	1498.997763	18.898304
45.084320	1486.289415	18.903322
45.161989	1501.973715	18.908339
45.225721	1497.957724	18.913357
45.231545	1500.683159	18.918375
45.355655	1499.257151	18.923392
45.361176	1491.599647	18.928410
45.118931	1500.596816	18.933427
45.659282	1493.521222	18.938445
45.553298	1492.178588	18.943463
45.450801	1502.772685	18.948480
45.648691	1486.499539	18.953498
45.605997	1490.349532	18.958515
45.358687	1497.455822	18.963533
45.990516	1491.130824	18.968551
45.785759	1499.133604	18.973568
45.629819	1495.035483	18.978586
45.226589	1495.709768	18.983603
45.866530	1520.144226	18.988621
46.286058	1523.936984	18.993639
45.999165	1528.830957	18.998656
46.016128	1528.391580	19.003674
45.938723	1533.493386	19.008691
46.111706	1528.173478	19.013709
46.502569	1521.825769	19.018727
46.368604	1523.015702	19.023744
46.296710	1524.870157	19.028762
46.500194	1532.330952	19.033779
46.524189	1531.759308	19.038797
46.150930	1531.345566	19.043815
46.221305	1530.021365	19.048832
46.332752	1520.675452	19.053850
46.101828	1529.738873	19.058867
46.489506	1515.142137	19.063885
46.395195	1521.622714	19.068903
46.757884	1537.236629	19.073920
46.782391	1539.397956	19.078938
46.954867	1551.429226	19.083955
47.051220	1552.836931	19.088973
47.138923	1552.682294	19.093991
46.871232	1550.484151	19.099008
47.114700	1543.603361	19.104026
46.986000	1545.106989	19.109043
47.134270	1543.430521	19.114061
47.034962	1545.683217	19.119079
46.981418	1541.098446	19.124096
47.092466	1550.535963	19.129114
47.170486	1551.977411	19.134131
47.140836	1541.484774	19.139149
47.495789	1542.035490	19.144167
47.076078	1549.816015	19.149184
47.404814	1541.298673	19.154202
47.238507	1540.787279	19.159219
47.305374	1543.820723	19.164237
47.846094	1569.679162	19.169255
47.460928	1572.633522	19.174272
47.760952	1567.120518	19.179290
47.516526	1586.115312	19.184307
47.663902	1570.485875	19.189325
47.854296	1570.677620	19.194343
47.706097	1572.067157	19.199360
48.038806	1564.546386	19.204378
48.099773	1571.098911	19.209395
48.144167	1560.030617	19.214413
48.127200	1565.718488	19.219431
48.107414	1576.314293	19.224448
48.315665	1564.438159	19.229466
48.212659	1572.611923	19.234483
48.471813	1564.928529	19.239501
48.374156	1562.127428	19.244519
48.001061	1572.937637	19.249536
48.443656	1563.154585	19.254554
48.433612	1571.108626	19.259571
48.750349	1569.294812	19.264589
48.366036	1549.587304	19.269607
48.465810	1556.974732	19.274624
48.438018	1558.973069	19.279642
48.420866	1566.534586	19.284659
48.769379	1572.701312	19.289677
48.689686	1582.224367	19.294695
48.764302	1584.041972	19.299712
49.468657	1575.954542	19.304730
49.477628	1575.825147	19.309747
49.171665	1554.437341	19.314765
49.213982	1547.472533	19.319783
48.854400	1550.243519	19.324800
49.147998	1552.238640	19.329818
48.866931	1552.444670	19.334835
48.750080	1548.430220	19.339853
49.418250	1561.684927	19.344871
49.649167	1578.609675	19.349888
49.364580	1569.478912	19.354906
49.353103	1580.240273	19.359923
49.407050	1570.324324	19.364941
49.758597	1576.041338	19.369959
49.444944	1576.509849	19.374976
49.435754	1568.818523	19.379994
49.283899	1578.296831	19.385011
49.453475	1570.171575	19.390029
49.302542	1568.047796	19.395047
49.138169	1567.791986	19.400064
49.521934	1587.835125	19.405082
49.607909	1601.781147	19.410099
49.848309	1597.003595	19.415117
50.229970	1604.292797	19.420135
50.109941	1602.859565	19.425152
50.027345	1600.834703	19.430170
50.193508	1602.027310	19.435187
49.805329	1601.566037	19.440205
50.057390	1596.659389	19.445223
49.939296	1592.613637	19.450240
50.098170	1594.964535	19.455258
50.458195	1607.611250	19.460275
50.306544	1620.286793	19.465293
50.745761	1619.456630	19.470311
50.721295	1625.663088	19.475328
50.746997	1619.638401	19.480346
50.600785	1617.055960	19.485363
50.611406	1624.632591	19.490381
50.621812	1622.648627	19.495399
50.692567	1625.214514	19.500416
51.155820	1618.901630	19.505434
51.166597	1617.312486	19.510451
50.780552	1619.354402	19.515469
50.918157	1619.171424	19.520487
50.845121	1622.433560	19.525504
51.074819	1616.015648	19.530522
51.307900	1613.401901	19.535539
50.818189	1634.748391	19.540557
51.025800	1610.454209	19.545575
51.025389	1626.134634	19.550592
51.356515	1620.384178	19.555610
51.134269	1620.115902	19.560627
51.108197	1644.382488	19.565645
51.569991	1640.599762	19.570663
51.671621	1645.178260	19.575680
51.901470	1641.403624	19.580698
51.804314	1641.666604	19.585715
51.596324	1650.729448	19.590733
52.134464	1655.963627	19.595751
52.021416	1643.313464	19.600768
51.997989	1638.060686	19.605786
52.060373	1629.711414	19.610803
51.874874	1639.139031	19.615821
52.215136	1620.505161	19.620839
51.773131	1626.650833	19.625856
51.968966	1628.809395	19.630874
52.200256	1629.549095	19.635891
52.228648	1630.927508	19.640909
52.551496	1630.708740	19.645927
52.149673	1631.458780	19.650944
52.055088	1626.869756	19.655962
52.099778	1626.515549	19.660979
52.065079	1630.687087	19.665997
52.185174	1624.508580	19.671015
51.817247	1635.768370	19.676032
51.964331	1638.764141	19.681050
52.387383	1654.461093	19.686067
52.245253	1660.043345	19.691085
52.725767	1658.516971	19.696103
52.664887	1657.392051	19.701120
52.786320	1654.608595	19.706138
52.689692	1662.043160	19.711155
52.561356	1679.890496	19.716173
53.090281	1686.973857	19.721191
53.206479	1690.208611	19.726208
53.221945	1679.921010	19.731226
53.262264	1684.276992	19.736243
53.117099	1689.353455	19.741261
53.652663	1675.218306	19.746279
53.824594	1689.043481	19.751296
53.565939	1673.139042	19.756314
53.982638	1669.766534	19.761331
53.647455	1666.169308	19.766349
53.749442	1645.971312	19.771367
53.551134	1656.624685	19.776384
53.473103	1651.827400	19.781402
53.573350	1656.589989	19.786419
53.578425	1680.860924	19.791437
53.683059	1685.034604	19.796455
53.933699	1680.057692	19.801472
53.908625	1687.822549	19.806490
54.028327	1675.226736	19.811507
53.695489	1678.599618	19.816525
54.225845	1677.140974	19.821543
53.954198	1676.455284	19.826560
54.085370	1680.283229	19.831578
54.006432	1676.222704	19.836595
53.906686	1686.467256	19.841613
54.194131	1685.360645	19.846631
54.466232	1693.152677	19.851648
54.199321	1704.744218	19.856666
54.166852	1696.607074	19.861683
54.196583	1705.843975	19.866701
54.429807	1696.003380	19.871719
54.343420	1699.081915	19.876736
54.306385	1702.009759	19.881754
54.782756	1710.595148	19.886771
54.876362	1718.724624	19.891789
55.058380	1721.094938	19.896807
54.997535	1720.553083	19.901824
55.151350	1718.138665	19.906842
55.251999	1723.249635	19.911859
55.033240	1722.472902	19.916877
55.074999	1720.819168	19.921895
55.140881	1720.885862	19.926912
55.565722	1725.911658	19.931930
55.280079	1715.495935	19.936947
55.163012	1721.049255	19.941965
55.654823	1713.262698	19.946983
55.650019	1719.653734	19.952000
55.413084	1721.541051	19.957018
55.428254	1709.468821	19.962035
55.175124	1722.181722	19.967053
55.348826	1716.424226	19.972071
55.722563	1717.879719	19.977088
55.705408	1717.153069	19.982106
55.983459	1721.675213	19.987123
55.673605	1727.529750	19.992141
55.800825	1742.770260	19.997159
56.200657	1733.390642	20.002176
55.913673	1735.526406	20.007194
55.948391	1726.684416	20.012211
55.910772	1736.235639	20.017229
56.194168	1738.398617	20.022247
56.288731	1729.133721	20.027264
56.206033	1736.826253	20.032282
56.524608	1730.336491	20.037299
56.401297	1730.998294	20.042317
56.266967	1730.498134	20.047335
56.533066	1728.573788	20.052352
56.332293	1739.768968	20.057370
56.982848	1753.927160	20.062387
56.717446	1765.457866	20.067405
56.988390	1759.064956	20.072423
57.125196	1760.100230	20.077440
57.038621	1764.100472	20.082458
57.046740	1760.479451	20.087475
57.135901	1761.631277	20.092493
57.285297	1749.331277	20.097511
57.534628	1743.157309	20.102528
57.403077	1734.936549	20.107546
57.311655	1721.405176	20.112563
57.158318	1724.188894	20.117581
57.383531	1728.086713	20.122599
57.407862	1739.447772	20.127616
57.331037	1759.289443	20.132634
57.380102	1745.292264	20.137651
57.013505	1758.666114	20.142669
57.493353	1758.807966	20.147687
57.482682	1752.721533	20.152704
57.289965	1762.233097	20.157722
57.351892	1768.612317	20.162739
57.706028	1781.594406	20.167757
57.816393	1780.597030	20.172775
57.815482	1776.626316	20.177792
57.773037	1787.430351	20.182810
58.129951	1772.604608	20.187827
57.925039	1782.414270	20.192845
57.667809	1780.923423	20.197863
58.062854	1786.457721	20.202880
58.032807	1807.498020	20.207898
58.400502	1806.954104	20.212915
58.556025	1807.058319	20.217933
58.577562	1807.026449	20.222951
58.508980	1805.766965	20.227968
58.354481	1804.570133	20.232986
58.903917	1797.505498	20.238003
58.587402	1799.094580	20.243021
58.270813	1802.071486	20.248039
58.784374	1805.033382	20.253056
58.709332	1825.043347	20.258074
59.190556	1824.064092	20.263091
59.307974	1830.560135	20.268109
59.241271	1830.280273	20.273127
59.361291	1828.050964	20.278144
59.389212	1828.868836	20.283162
59.746876	1825.032835	20.288179
59.185745	1808.811405	20.293197
59.276772	1812.560596	20.298215
59.549093	1810.782850	20.303232
59.258907	1818.719623	20.308250
59.510410	1813.723235	20.313267
59.424175	1815.930497	20.318285
59.357621	1810.003689	20.323303
59.636725	1808.793725	20.328320
59.436065	1810.882136	20.333338
60.038480	1806.470175	20.338355
59.848068	1820.776334	20.343373
59.894049	1821.339243	20.348391
60.012743	1812.827005	20.353408
59.549054	1817.351911	20.358426
59.949884	1820.187985	20.363443
60.155400	1835.438458	20.368461
60.029326	1841.240559	20.373479
60.242658	1846.880952	20.378496
60.108934	1849.603176	20.383514
60.788133	1838.881550	20.388531
60.627478	1843.499991	20.393549
60.722953	1841.465692	20.398567
60.733900	1846.955341	20.403584
60.460624	1849.678230	20.408602
60.542148	1844.226505	20.413619
60.836092	1845.727113	20.418637
60.585998	1835.012112	20.423655
60.738164	1830.638868	20.428672
60.211154	1844.996057	20.433690
60.886549	1857.578162	20.438707
60.736660	1866.295679	20.443725
60.679598	1867.353611	20.448743
61.085970	1864.665067	20.453760
60.921770	1880.395703	20.458778
60.730237	1892.571370	20.463795
61.553078	1900.212868	20.468813
61.337841	1905.250215	20.473831
61.758180	1894.797794	20.478848
61.793746	1899.979049	20.483866
61.651191	1889.290300	20.488883
61.773596	1888.233836	20.493901
62.253669	1889.329608	20.498919
62.327594	1887.739036	20.503936
61.810889	1896.360610	20.508954
62.118299	1887.348571	20.513971
62.206967	1888.933173	20.518989
62.139474	1890.486150	20.524007
62.186428	1889.257530	20.529024
62.192825	1891.754195	20.534042
62.326870	1884.860664	20.539059
62.393212	1877.855509	20.544077
62.030970	1890.036997	20.549095
62.087395	1877.965679	20.554112
62.263862	1879.828661	20.559130
62.219156	1881.619207	20.564147
62.371297	1893.232449	20.569165
62.309578	1916.971889	20.574183
62.671496	1912.120971	20.579200
62.521307	1916.186115	20.584218
62.828949	1914.799368	20.589235
63.007944	1906.454262	20.594253
62.884064	1920.410514	20.599271
63.141291	1905.155079	20.604288
62.995245	1912.192033	20.609306
63.175347	1912.056741	20.614323
63.309397	1926.205729	20.619341
63.459856	1934.627880	20.624359
63.687188	1935.966294	20.629376
63.622260	1918.324767	20.634394
63.369693	1904.652984	20.639411
63.615945	1916.870752	20.644429
63.401088	1925.474253	20.649447
63.901937	1917.424283	20.654464
63.759601	1926.173654	20.659482
63.589206	1927.047989	20.664499
63.919192	1927.846561	20.669517
64.001728	1935.214582	20.674535
64.251579	1930.181816	20.679552
63.900139	1935.557479	20.684570
63.918096	1922.133807	20.689587
64.308223	1931.314320	20.694605
64.009142	1932.941867	20.699623
63.571848	1933.178098	20.704640
63.901504	1934.157830	20.709658
64.180205	1946.644664	20.714675
64.246710	1955.021277	20.719693
64.328281	1960.662267	20.724711
64.472495	1949.207475	20.729728
64.831284	1956.758512	20.734746
64.835925	1959.364536	20.739763
64.678033	1953.730361	20.744781
64.411037	1957.453038	20.749799
64.991824	1949.161858	20.754816
64.914105	1954.407165	20.759834
64.873611	1967.036238	20.764851
65.470082	1980.590195	20.769869
64.921352	1979.356653	20.774887
65.233322	1973.969091	20.779904
65.178752	1983.367363	20.784922
65.113380	1987.127925	20.789939
65.425597	1991.891348	20.794957
65.142542	1989.645682	20.799975
65.466151	1982.890016	20.804992
65.406789	1982.008134	20.810010
65.525024	1994.289287	20.815027
65.916830	1994.234299	20.820045
65.814044	2001.421614	20.825063
66.006522	2004.227259	20.830080
66.134454	2001.177698	20.835098
66.103947	2004.097037	20.840115
66.181841	1991.072841	20.845133
65.864876	2003.846541	20.850151
66.015402	1995.905324	20.855168
66.208624	2002.049903	20.860186
66.238231	2000.315474	20.865203
66.689089	2002.003507	20.870221
66.607719	1998.427958	20.875239
66.506064	1997.840880	20.880256
66.889757	2000.514468	20.885274
66.789938	2001.290899	20.890291
66.847718	1996.736381	20.895309
66.562835	2001.723478	20.900327
66.983633	2013.237996	20.905344
66.698724	2023.047275	20.910362
66.768495	2021.693210	20.915379
66.873668	2025.062541	20.920397
67.070983	2025.963403	20.925415
67.211365	2023.825973	20.930432
67.216474	2021.258174	20.935450
66.965234	2025.658196	20.940467
67.449700	2024.267753	20.945485
67.600385	2039.370021	20.950503
67.642396	2041.168275	20.955520
67.733709	2042.575678	20.960538
67.637463	2038.576586	20.965555
67.926454	2027.827706	20.970573
67.550906	2041.015478	20.975591
68.008779	2040.691671	20.980608
67.953148	2038.620946	20.985626
67.933146	2034.552144	20.990643
68.135072	2035.803433	20.995661
67.920638	2030.999874	21.000679
67.915702	2027.705371	21.005696
67.508009	2031.872238	21.010714
67.789359	2048.645839	21.015731
68.291058	2046.663154	21.020749
68.231907	2060.769055	21.025767
68.574095	2063.823946	21.030784
68.699812	2055.524198	21.035802
68.585508	2056.240430	21.040819
68.612517	2052.064230	21.045837
68.913650	2050.349012	21.050855
68.506346	2053.285077	21.055872
68.693879	2074.111754	21.060890
69.047253	2078.080571	21.065907
69.621016	2083.165295	21.070925
69.485558	2080.690448	21.075943
69.494084	2081.556427	21.080960
69.663846	2082.109088	21.085978
69.317352	2062.591518	21.090995
69.435723	2053.622496	21.096013
69.798598	2068.871160	21.101031
69.381810	2076.923516	21.106048
69.726133	2077.704368	21.111066
70.034190	2070.604379	21.116083
70.018145	2072.819741	21.121101
69.712076	2079.120645	21.126119
69.918391	2078.987705	21.131136
70.069139	2072.469683	21.136154
69.645726	2074.931240	21.141171
69.922343	2074.005929	21.146189
69.924757	2071.375179	21.151207
69.818413	2072.308998	21.156224
70.063822	2092.994224	21.161242
70.112661	2103.903053	21.166259
70.266259	2095.459687	21.171277
69.922254	2103.105899	21.176295
70.350028	2103.744978	21.181312
70.172913	2112.080513	21.186330
70.197986	2125.828423	21.191347
70.860996	2124.706057	21.196365
70.886268	2124.757035	21.201383
70.674905	2120.399017	21.206400
70.806827	2124.704523	21.211418
70.811600	2150.553852	21.216435
71.406139	2141.711457	21.221453
71.580588	2155.576791	21.226471
71.372464	2143.438829	21.231488
71.697109	2149.323117	21.236506
71.390086	2149.090913	21.241523
71.833205	2140.040118	21.246541
71.661023	2147.757118	21.251559
71.596276	2148.652163	21.256576
72.177835	2142.098609	21.261594
71.845025	2143.302220	21.266611
71.990708	2146.853066	21.271629
72.143253	2142.080052	21.276647
72.012564	2137.798833	21.281664
72.023341	2139.081386	21.286682
71.903613	2149.766574	21.291699
72.229896	2132.438389	21.296717
72.225742	2138.643263	21.301735
72.192219	2140.548133	21.306752
72.215193	2145.358314	21.311770
72.444781	2165.143469	21.316787
72.747797	2158.034826	21.321805
72.764015	2165.424961	21.326823
72.642773	2161.340210	21.331840
72.921065	2154.377399	21.336858
72.980996	2167.457346	21.341875
73.207674	2162.310622	21.346893
72.988436	2174.663542	21.351911
72.977744	2167.491871	21.356928
73.225548	2159.519110	21.361946
73.178106	2161.464083	21.366963
73.347769	2159.301313	21.371981
73.388105	2157.420203	21.376999
73.236676	2157.289800	21.382016
73.213530	2155.752677	21.387034
72.914570	2160.681916	21.392051
73.526708	2168.720262	21.397069
73.608123	2180.984824	21.402087
73.548153	2178.945903	21.407104
73.607027	2195.063166	21.412122
73.462423	2189.377097	21.417139
73.914819	2192.433453	21.422157
73.587521	2216.376778	21.427175
73.835879	2223.831658	21.432192
74.201040	2212.030236	21.437210
74.175756	2213.412470	21.442227
74.269779	2217.258905	21.447245
74.533354	2211.068220	21.452263
74.581427	2226.806581	21.457280
74.647980	2238.148022	21.462298
74.612519	2238.524029	21.467315
75.214599	2238.369264	21.472333
75.076938	2240.659513	21.477351
75.109390	2241.475081	21.482368
75.639234	2234.516256	21.487386
75.142031	2232.822960	21.492403
75.393712	2222.489589	21.497421
75.576536	2213.468069	21.502439
75.297968	2208.225056	21.507456
75.503797	2209.156804	21.512474
75.201891	2226.358283	21.517491
75.555183	2232.067380	21.522509
75.765655	2231.705002	21.527527
75.463524	2236.169811	21.532544
75.564716	2221.500948	21.537562
75.314311	2232.911007	21.542579
75.571472	2238.673820	21.547597
75.958038	2243.882510	21.552615
75.817038	2262.395237	21.557632
76.215368	2261.581658	21.562650
76.220812	2269.988630	21.567667
76.347232	2261.905594	21.572685
76.406752	2259.824042	21.577703
76.302523	2264.084431	21.582720
76.556280	2256.986655	21.587738
76.310962	2263.876417	21.592755
76.201825	2259.148270	21.597773
76.128445	2261.320788	21.602791
76.339083	2279.526878	21.607808
76.675211	2270.579159	21.612826
76.705726	2285.811017	21.617843
76.677647	2276.277112	21.622861
76.959881	2303.378449	21.627879
77.354548	2301.422511	21.632896
77.881937	2295.482221	21.637914
77.755816	2301.016379	21.642931
77.656642	2306.548440	21.647949
77.780634	2284.922679	21.652967
77.494055	2281.447186	21.657984
77.779089	2285.012000	21.663002
77.927051	2295.005694	21.668019
77.840618	2296.221675	21.673037
77.980723	2299.462442	21.678055
77.640818	2303.105142	21.683072
77.929247	2294.669266	21.688090
78.345247	2298.825418	21.693107
78.245906	2296.794575	21.698125
78.385353	2295.609667	21.703143
78.091128	2309.936613	21.708160
78.081852	2299.821603	21.713178
78.146244	2302.796548	21.718195
78.104454	2301.756613	21.723213
78.482450	2310.551156	21.728231
78.436803	2317.907117	21.733248
78.603492	2323.288466	21.738266
78.700520	2327.369087	21.743283
78.877048	2320.076579	21.748301
79.341299	2324.807847	21.753319
78.847540	2325.056579	21.758336
79.212780	2316.661126	21.763354
79.093553	2328.173555	21.768371
79.110014	2338.068966	21.773389
79.439229	2343.908475	21.778407
79.393034	2355.124174	21.783424
79.732842	2351.295728	21.788442
79.753072	2354.681558	21.793459
79.660171	2346.082009	21.798477
79.495026	2353.488876	21.803495
79.379321	2350.417379	21.808512
79.740087	2356.137490	21.813530
79.640519	2374.702154	21.818547
80.073320	2375.576252	21.823565
80.422466	2383.595654	21.828583
80.123742	2384.479449	21.833600
80.462521	2376.789561	21.838618
80.462707	2377.535278	21.843635
80.708532	2375.288606	21.848653
80.787651	2377.002011	21.853671
80.431883	2386.013367	21.858688
80.825723	2369.054462	21.863706
81.298775	2382.626846	21.868723
81.172064	2389.847831	21.873741
81.365742	2370.130195	21.878759
80.797533	2370.901514	21.883776
80.972309	2374.720050	21.888794
80.925473	2390.892422	21.893811
81.077772	2391.288923	21.898829
81.259590	2387.787036	21.903847
81.437783	2391.530597	21.908864
81.244485	2387.369522	21.913882
81.367986	2394.880200	21.918899
81.560761	2416.559267	21.923917
82.105092	2407.616370	21.928935
81.771259	2414.645270	21.933952
81.952600	2418.405246	21.938970
82.104318	2413.304711	21.943987
81.814253	2409.516757	21.949005
82.181303	2409.392638	21.954023
82.148574	2422.212143	21.959040
82.281672	2432.724161	21.964058
82.291408	2440.529696	21.969075
82.528166	2453.460127	21.974093
82.789341	2442.792738	21.979111
82.462720	2449.418863	21.984128
82.843093	2445.217123	21.989146
83.134096	2441.345946	21.994163
83.115606	2437.694527	21.999181
83.137656	2428.436890	22.004199
83.020624	2435.822837	22.009216
83.198610	2431.271913	22.014234
83.140243	2432.381677	22.019251
83.090255	2447.589619	22.024269
83.556158	2447.282982	22.029287
83.442004	2458.760414	22.034304
83.878026	2451.421731	22.039322
83.640748	2459.509131	22.044339
83.433283	2466.443505	22.049357
83.731102	2448.259400	22.054375
83.836994	2455.660419	22.059392
83.882899	2448.055209	22.064410
83.924797	2447.319929	22.069427
83.994646	2457.499111	22.074445
84.354876	2468.352702	22.079463
84.294630	2481.080349	22.084480
84.142728	2475.273724	22.089498
84.374284	2484.927303	22.094515
84.171637	2485.517622	22.099533
84.596510	2479.283590	22.104551
84.345649	2495.989092	22.109568
84.783002	2505.773581	22.114586
84.887562	2510.410121	22.119603
84.617124	2518.182944	22.124621
85.055996	2513.706131	22.129639
84.985319	2509.703078	22.134656
85.202265	2511.831105	22.139674
85.411882	2527.297734	22.144691
85.379607	2541.183465	22.149709
85.864250	2532.587408	22.154727
85.495786	2542.636843	22.159744
85.840255	2534.635287	22.164762
85.980350	2529.288199	22.169779
85.521920	2531.319770	22.174797
86.176391	2527.119874	22.179815
86.112046	2524.367023	22.184832
86.173735	2518.683687	22.189850
86.160164	2523.687054	22.194867
86.255724	2516.761819	22.199885
86.385855	2521.408303	22.204903
86.367433	2550.028833	22.209920
86.506325	2552.406417	22.214938
86.635509	2551.789365	22.219955
86.702361	2552.637839	22.224973
86.832132	2552.567968	22.229991
86.772827	2558.446293	22.235008
87.187166	2545.378134	22.240026
87.109403	2546.209211	22.245043
87.009365	2552.403352	22.250061
87.119754	2556.662541	22.255079
87.026673	2575.120457	22.260096
87.331202	2571.500962	22.265114
87.439631	2580.323361	22.270131
87.266331	2583.171169	22.275149
87.613324	2575.973948	22.280167
87.400906	2587.534678	22.285184
87.666296	2595.212129	22.290202
87.883567	2598.129140	22.295219
88.125463	2603.446951	22.300237
88.425228	2595.085420	22.305255
88.285299	2600.955849	22.310272
88.042575	2604.369128	22.315290
88.306684	2599.474347	22.320307
88.679851	2590.421489	22.325325
88.465670	2593.807203	22.330343
88.453233	2602.832708	22.335360
88.744441	2620.196672	22.340378
88.981635	2619.403457	22.345395
88.703982	2629.167422	22.350413
88.947274	2628.704714	22.355431
88.629792	2622.900643	22.360448
88.856954	2620.242827	22.365466
89.314927	2620.172949	22.370483
89.306512	2628.208369	22.375501
89.333402	2625.494729	22.380519
89.465103	2641.640557	22.385536
89.491608	2649.716272	22.390554
89.825741	2647.817564	22.395571
89.321274	2653.558986	22.400589
89.822392	2651.278275	22.405607
89.907309	2650.114182	22.410624
89.950748	2646.886346	22.415642
89.634014	2650.791448	22.420659
90.009086	2668.999905	22.425677
90.356931	2663.710900	22.430695
90.559359	2668.389162	22.435712
90.715488	2667.779850	22.440730
90.658277	2666.815678	22.445747
90.674244	2669.964864	22.450765
90.901431	2663.127621	22.455783
91.214651	2664.210526	22.460800
90.881534	2672.839923	22.465818
90.936007	2658.157124	22.470835
90.587536	2666.127598	22.475853
90.823936	2683.606619	22.480871
91.313108	2693.850003	22.485888
91.289413	2698.401922	22.490906
91.265663	2691.713701	22.495923
91.259987	2695.280678	22.500941
91.316440	2702.317926	22.505959
91.472798	2721.299323	22.510976
91.651150	2726.094982	22.515994
92.031730	2721.611226	22.521011
91.945626	2730.133217	22.526029
92.200444	2721.783391	22.531047
92.246966	2721.699348	22.536064
92.007092	2729.078998	22.541082
92.614742	2737.325488	22.546099
92.755924	2743.736872	22.551117
92.985472	2743.213441	22.556135
93.152115	2745.338410	22.561152
92.637705	2751.137030	22.566170
92.812899	2739.348159	22.571187
92.597084	2744.722508	22.576205
92.796340	2738.102864	22.581223
92.960887	2741.329047	22.586240
92.818782	2755.117003	22.591258
92.774918	2753.386386	22.596275
92.686888	2771.684238	22.601293
92.789115	2770.451517	22.606311
93.032462	2794.155959	22.611328
93.366869	2802.858385	22.616346
93.719947	2795.711636	22.621363
93.855632	2811.568770	22.626381
93.976679	2816.433398	22.631399
94.553645	2814.403119	22.636416
94.524493	2818.450820	22.641434
94.814153	2804.205752	22.646451
94.909589	2798.751785	22.651469
94.900784	2779.945570	22.656487
94.755237	2767.206557	22.661504
94.774437	2769.126397	22.666522
95.256785	2763.888718	22.671539
95.099067	2774.535344	22.676557
95.037314	2762.108471	22.681575
95.113172	2770.687533	22.686592
94.969042	2769.677897	22.691610
95.206591	2768.678696	22.696627
95.258397	2786.428178	22.701645
95.212271	2797.852467	22.706663
95.599880	2805.856271	22.711680
95.435067	2802.849905	22.716698
95.585033	2800.102864	22.721715
95.744139	2799.774178	22.726733
95.493710	2799.852694	22.731751
95.643063	2800.108739	22.736768
95.750110	2811.033625	22.741786
95.904125	2828.148468	22.746803
95.581015	2838.668179	22.751821
95.907044	2841.729841	22.756839
95.851871	2835.123145	22.761856
95.837567	2863.085248	22.766874
96.076827	2859.974565	22.771891
96.234856	2870.848530	22.776909
96.674814	2878.170421	22.781927
96.795064	2882.170959	22.786944
96.692980	2892.892320	22.791962
96.765623	2882.579888	22.796979
96.806588	2892.989746	22.801997
97.113343	2912.817807	22.807015
97.483906	2914.917700	22.812032
97.423520	2919.239517	22.817050
97.721060	2919.855707	22.822067
97.220432	2919.585458	22.827085
97.597918	2910.079301	22.832103
97.995627	2921.449489	22.837120
97.814478	2939.681059	22.842138
98.100409	2934.921944	22.847155
98.054059	2950.353807	22.852173
98.215587	2943.011521	22.857191
98.240775	2941.600187	22.862208
98.268876	2949.015107	22.867226
98.573719	2942.716113	22.872243
98.717278	2944.577587	22.877261
98.857796	2957.585402	22.882279
99.230723	2963.286008	22.887296
99.335435	2966.108723	22.892314
99.692535	2950.495547	22.897331
99.367486	2940.176081	22.902349
99.137700	2945.651639	22.907367
99.273391	2939.019598	22.912384
99.183166	2946.444658	22.917402
99.585158	2950.054837	22.922419
99.584685	2951.479883	22.927437
99.365476	2952.412752	22.932455
99.578483	2956.709396	22.937472
99.371593	2977.894739	22.942490
99.419887	2969.707333	22.947507
99.829091	2981.052431	22.952525
100.024385	2994.803242	22.957543
100.337524	3006.562331	22.962560
100.327403	3015.267584	22.967578
100.451676	3000.896557	22.972595
100.585702	3011.302504	22.977613
100.411638	3012.096789	22.982631
100.802279	3009.464996	22.987648
100.908555	3032.089640	22.992666
101.161330	3030.044500	22.997683
101.281037	3038.222319	23.002701
101.264849	3036.343768	23.007719
101.447589	3040.249347	23.012736
101.334861	3039.978263	23.017754
101.632103	3041.536720	23.022771
101.251573	3038.875501	23.027789
101.545298	3043.847844	23.032807
102.022126	3049.076513	23.037824
101.804955	3064.302498	23.042842
102.117795	3063.282545	23.047859
102.149547	3065.166482	23.052877
102.342429	3060.086090	23.057895
102.301653	3057.660375	23.062912
102.213362	3069.648588	23.067930
102.187909	3056.765822	23.072947
102.022526	3065.777544	23.077965
102.083752	3088.396735	23.082983
102.888346	3083.802120	23.088000
102.522209	3092.343898	23.093018
102.938443	3094.325614	23.098035
102.839198	3102.494832	23.103053
102.543842	3115.600143	23.108071
103.263462	3105.458821	23.113088
103.657337	3115.641878	23.118106
103.773052	3111.049488	23.123123
103.629913	3102.623997	23.128141
103.828737	3115.020657	23.133159
103.939327	3121.863681	23.138176
103.707689	3141.300417	23.143194
104.020439	3136.754145	23.148211
104.087969	3148.069706	23.153229
103.817915	3149.313003	23.158247
104.386849	3139.726187	23.163264
104.166801	3142.877927	23.168282
104.356180	3156.508195	23.173299
104.754197	3160.418324	23.178317
104.886494	3164.357879	23.183335
104.872298	3149.411551	23.188352
104.976016	3159.489118	23.193370
104.991865	3156.280314	23.198387
105.156317	3167.166415	23.203405
105.369511	3184.748277	23.208423
105.341709	3180.686766	23.213440
105.528541	3179.994785	23.218458
105.850716	3186.852024	23.223475
105.881129	3179.281310	23.228493
105.983400	3184.214917	23.233511
105.935199	3176.290649	23.238528
105.804561	3181.459293	23.243546
106.073865	3189.152534	23.248563
106.210497	3204.548841	23.253581
106.171142	3208.263258	23.258599
106.549572	3197.675953	23.263616
106.489668	3205.567817	23.268634
106.511335	3199.446721	23.273651
106.935365	3215.788864	23.278669
106.863755	3232.007551	23.283687
106.713614	3223.341790	23.288704
106.777301	3230.272950	23.293722
106.853523	3223.954210	23.298739
107.228393	3237.266013	23.303757
107.253945	3248.384244	23.308775
107.610728	3256.882807	23.313792
107.654878	3255.135200	23.318810
107.944453	3252.216919	23.323827
107.981521	3246.845301	23.328845
107.792578	3251.032179	23.333863
107.766202	3245.926605	23.338880
108.074274	3266.661686	23.343898
108.199957	3281.743313	23.348915
108.470097	3270.630129	23.353933
108.344083	3282.347949	23.358951
108.729219	3270.220345	23.363968
108.801222	3277.313552	23.368986
108.840980	3276.958550	23.374003
109.089421	3277.032432	23.379021
108.988573	3279.968380	23.384039
109.345857	3286.117019	23.389056
109.384432	3310.203431	23.394074
109.679099	3299.894521	23.399091
109.870000	3305.484825	23.404109
109.300732	3317.603260	23.409127
109.846066	3302.170797	23.414144
109.815274	3303.915890	23.419162
109.705272	3301.261415	23.424179
110.067763	3295.376404	23.429197
109.752145	3305.189204	23.434215
110.071608	3301.652120	23.439232
109.785628	3319.834158	23.444250
110.172901	3334.301204	23.449267
110.520890	3327.420834	23.454285
110.295182	3334.831498	23.459303
110.325523	3337.419322	23.464320
110.437698	3352.394187	23.469338
110.583303	3362.016868	23.474355
110.727573	3358.509171	23.479373
110.860026	3385.826582	23.484391
111.534463	3385.498796	23.489408
111.617226	3387.775160	23.494426
111.185984	3382.959825	23.499443
111.435095	3388.404680	23.504461
111.739988	3387.647470	23.509479
111.998745	3400.808539	23.514496
111.934890	3409.103174	23.519514
111.911615	3415.247935	23.524531
112.089616	3405.616221	23.529549
112.024553	3419.886946	23.534567
112.224810	3426.299461	23.539584
112.429071	3437.970591	23.544602
112.313472	3441.241728	23.549619
112.745848	3439.699147	23.554637
113.065305	3439.210815	23.559655
112.885711	3427.629003	23.564672
113.170596	3444.431088	23.569690
113.181093	3455.553929	23.574707
113.707553	3448.319905	23.579725
113.684777	3461.046478	23.584743
114.068951	3460.284801	23.589760
113.709696	3454.693656	23.594778
113.673098	3454.546590	23.599795
114.086166	3461.049098	23.604813
114.230522	3456.139231	23.609831
113.955619	3449.552116	23.614848
114.317112	3457.633819	23.619866
114.243324	3473.640100	23.624883
114.533505	3475.243083	23.629901
114.400877	3480.387743	23.634919
114.620970	3485.142864	23.639936
114.731997	3472.193453	23.644954
114.915029	3483.334211	23.649971
114.878158	3499.711223	23.654989
114.943295	3517.052979	23.660007
115.352176	3512.516673	23.665024
115.267434	3507.154108	23.670042
115.667049	3506.291043	23.675059
115.366624	3504.712674	23.680077
115.432480	3533.087559	23.685095
115.683247	3523.909924	23.690112
115.944542	3530.682108	23.695130
116.009043	3539.736760	23.700147
116.288536	3531.698207	23.705165
116.445903	3538.980181	23.710183
116.584822	3544.704389	23.715200
116.998892	3547.146818	23.720218
116.843791	3536.730306	23.725235
117.183891	3530.658734	23.730253
116.874522	3525.558971	23.735271
116.908237	3541.381755	23.740288
117.032320	3546.615053	23.745306
117.360494	3546.172132	23.750323
117.571907	3543.187989	23.755341
117.452999	3547.001888	23.760359
117.110301	3543.909460	23.765376
117.275251	3548.157918	23.770394
117.323408	3574.000454	23.775411
117.949234	3573.511008	23.780429
117.980988	3574.439769	23.785447
117.985258	3580.161871	23.790464
118.356831	3580.642196	23.795482
118.048951	3592.426189	23.800499
118.446786	3591.238176	23.805517
118.435644	3602.766330	23.810535
118.346748	3600.505997	23.815552
118.555088	3601.383080	23.820570
118.301853	3626.397537	23.825587
118.850897	3622.774728	23.830605
118.616230	3634.011129	23.835623
119.020185	3648.278042	23.840640
119.198499	3657.483626	23.845658
119.501084	3656.736630	23.850675
119.861791	3655.659891	23.855693
119.550852	3656.283535	23.860711
120.021803	3673.207445	23.865728
120.297446	3676.435511	23.870746
120.066381	3682.531303	23.875763
120.058209	3694.982383	23.880781
120.307122	3683.838166	23.885799
120.378541	3683.209767	23.890816
120.980134	3696.484820	23.895834
120.804211	3701.658770	23.900851
121.044362	3708.099841	23.905869
121.112711	3713.399517	23.910887
121.174659	3708.459508	23.915904
121.002653	3708.814843	23.920922
121.266496	3717.483398	23.925939
121.285347	3729.029122	23.930957
121.789254	3730.163225	23.935975
121.869875	3732.982193	23.940992
121.980064	3733.910184	23.946010
122.005098	3740.395546	23.951027
122.402352	3732.924089	23.956045
121.782926	3741.217167	23.961063
122.110117	3747.541074	23.966080
122.524382	3755.611046	23.971098
122.701629	3758.463634	23.976115
122.933930	3755.905186	23.981133
122.598485	3759.673086	23.986151
122.499460	3761.907150	23.991168
122.972550	3778.793413	23.996186
123.111237	3786.952733	24.001203
123.732355	3776.561507	24.006221
123.721391	3781.756998	24.011239
123.649154	3786.793320	24.016256
123.764091	3782.124081	24.021274
123.719093	3788.639958	24.026291
124.011365	3799.542353	24.031309
124.103970	3809.409157	24.036327
124.155915	3817.392276	24.041344
124.442354	3804.753755	24.046362
124.428904	3807.654462	24.051379
124.561854	3805.523536	24.056397
124.172568	3802.330092	24.061415
124.520541	3824.392173	24.066432
124.297305	3829.144803	24.071450
124.731005	3836.011034	24.076467
125.034844	3833.378123	24.081485
124.930117	3850.153798	24.086503
125.156652	3856.176653	24.091520
125.602753	3850.158286	24.096538
125.451500	3860.060771	24.101555
125.603928	3855.217563	24.106573
125.689449	3869.278700	24.111591
125.564516	3873.438213	24.116608
126.189700	3881.306377	24.121626
125.992974	3885.769948	24.126643
126.332767	3891.995751	24.131661
126.620797	3911.087129	24.136679
126.349082	3919.579070	24.141696
126.499411	3908.825085	24.146714
126.608628	3916.654657	24.151731
127.171716	3940.129531	24.156749
127.084503	3934.673908	24.161767
126.831820	3945.114970	24.166784
127.501850	3943.426682	24.171802
127.444526	3943.571669	24.176819
127.269884	3952.537392	24.181837
127.495514	3959.935839	24.186855
127.418029	3962.393172	24.191872
128.288229	3972.637323	24.196890
128.071447	3981.800620	24.201907
128.451878	3989.152976	24.206925
129.004061	3990.076715	24.211943
128.889954	3987.400751	24.216960
128.777989	3988.339943	24.221978
128.801080	3986.284670	24.226995
128.947915	3988.166991	24.232013
129.317959	3986.373223	24.237031
129.466565	3983.180465	24.242048
129.628145	3994.786233	24.247066
129.151197	4016.718188	24.252083
129.473009	4012.231200	24.257101
129.796384	4010.003356	24.262119
129.771314	4008.175772	24.267136
130.092856	4013.192649	24.272154
129.553054	4030.015346	24.277171
129.941759	4032.334081	24.282189
130.159169	4043.898353	24.287207
130.188236	4051.771975	24.292224
130.629765	4064.187485	24.297242
130.543516	4073.540281	24.302259
130.738004	4072.775726	24.307277
130.844002	4081.498179	24.312295
131.091476	4092.339286	24.317312
131.506306	4092.248599	24.322330
131.518520	4101.889096	24.327347
131.409867	4092.702515	24.332365
131.435821	4091.255512	24.337383
131.403596	4116.221558	24.342400
131.895339	4120.677923	24.347418
132.032592	4125.437899	24.352435
131.876517	4115.197568	24.357453
132.050414	4140.370510	24.362471
132.281346	4154.740954	24.367488
132.669498	4150.090163	24.372506
132.600302	4157.850952	24.377523
132.796700	4150.685824	24.382541
133.074832	4168.042652	24.387559
133.001979	4170.496888	24.392576
133.624343	4170.237174	24.397594
133.389909	4177.899324	24.402611
133.320186	4185.979952	24.407629
133.877961	4173.988847	24.412647
133.600467	4180.051565	24.417664
133.780927	4185.232036	24.422682
134.060576	4196.783755	24.427699
133.995120	4199.514768	24.432717
134.331783	4208.433788	24.437735
134.006981	4209.601175	24.442752
134.317717	4205.000199	24.447770
134.274510	4227.940345	24.452787
134.189454	4236.759093	24.457805
134.657641	4242.141595	24.462823
134.871286	4262.609726	24.467840
135.464548	4261.308984	24.472858
135.460011	4271.283910	24.477875
135.537973	4259.635214	24.482893
135.673035	4262.613404	24.487911
135.626468	4264.003280	24.492928
135.922299	4269.865584	24.497946
136.092304	4280.682634	24.502963
136.406059	4283.636756	24.507981
136.563557	4281.018943	24.512999
136.565257	4279.947655	24.518016
136.141535	4281.347208	24.523034
136.396196	4308.591657	24.528051
136.658568	4312.506425	24.533069
136.961683	4306.218989	24.538087
136.711630	4322.064733	24.543104
137.122056	4336.326085	24.548122
137.445323	4339.866935	24.553139
137.662284	4340.799731	24.558157
137.573997	4342.067364	24.563175
137.808146	4349.502388	24.568192
137.992699	4357.104709	24.573210
137.527937	4365.960404	24.578227
138.030523	4369.968511	24.583245
138.308348	4371.372419	24.588263
138.578106	4387.552717	24.593280
138.891661	4383.797830	24.598298
139.092748	4386.450884	24.603315
139.088977	4382.981645	24.608333
139.067145	4384.383187	24.613351
139.089023	4389.114305	24.618368
139.596055	4401.868120	24.623386
139.799440	4410.132823	24.628403
139.800749	4409.336443	24.633421
139.793945	4400.092656	24.638439
139.717443	4410.941943	24.643456
140.089534	4406.402418	24.648474
140.029051	4425.685217	24.653491
139.839957	4434.832380	24.658509
140.442238	4421.966635	24.663527
140.481110	4447.213614	24.668544
140.841078	4451.313082	24.673562
140.702191	4458.891034	24.678579
140.795225	4456.954065	24.683597
140.946933	4460.880891	24.688615
141.175614	4483.468467	24.693632
141.486097	4481.982986	24.698650
141.587881	4488.168103	24.703667
141.412607	4490.411743	24.708685
141.597001	4495.388479	24.713703
141.832368	4515.823417	24.718720
142.169617	4516.381126	24.723738
141.959246	4519.154300	24.728755
142.062130	4532.447660	24.733773
142.491737	4548.137794	24.738791
142.183476	4557.720582	24.743808
142.135445	4550.956438	24.748826
142.464593	4564.587239	24.753843
142.632547	4581.872199	24.758861
142.994987	4580.478913	24.763879
143.119072	4597.864084	24.768896
143.866761	4601.613522	24.773914
144.326970	4591.366145	24.778931
144.366921	4589.136316	24.783949
144.460141	4591.388285	24.788967
144.566998	4588.932378	24.793984
144.809453	4583.478654	24.799002
144.922895	4578.065192	24.804019
144.996981	4578.676709	24.809037
145.131995	4576.634332	24.814055
145.132874	4585.423297	24.819072
144.720993	4572.996247	24.824090
144.596943	4579.147909	24.829107
144.829317	4596.785281	24.834125
145.523380	4591.658439	24.839143
145.696315	4614.323162	24.844160
145.570985	4609.170522	24.849178
145.754065	4621.569410	24.854195
145.834576	4636.378664	24.859213
146.232091	4637.690328	24.864231
146.091916	4645.617468	24.869248
146.221919	4644.627296	24.874266
146.309927	4659.723576	24.879283
146.291201	4662.639884	24.884301
146.805796	4672.263714	24.889319
146.831750	4683.583724	24.894336
147.115683	4695.858079	24.899354
147.343703	4697.283652	24.904371
147.135215	4692.408582	24.909389
147.640326	4708.749500	24.914407
147.515856	4727.019437	24.919424
147.499237	4729.614873	24.924442
148.166035	4735.662444	24.929459
148.182719	4752.093719	24.934477
148.514989	4749.685525	24.939495
148.991673	4740.021268	24.944512
148.848732	4744.956193	24.949530
149.168698	4740.610280	24.954547
149.061328	4745.096708	24.959565
149.247455	4735.812907	24.964583
149.282941	4765.237381	24.969600
149.551882	4766.410467	24.974618
149.949576	4770.654987	24.979635
149.704357	4775.320182	24.984653
150.160558	4760.959143	24.989671
150.030647	4772.155384	24.994688
149.829607	4778.005632	24.999706
150.289319	4784.649825	25.004723
150.253052	4784.787394	25.009741
150.736475	4782.947993	25.014759
150.502730	4802.772640	25.019776
150.481359	4811.611094	25.024794
150.972166	4811.348742	25.029811
150.625499	4822.301319	25.034829
151.148777	4834.744862	25.039847
151.378941	4844.259950	25.044864
151.637028	4846.725657	25.049882
151.645538	4848.100953	25.054899
151.855336	4866.614987	25.059917
151.926304	4870.519842	25.064935
152.365930	4882.239324	25.069952
152.549605	4875.240576	25.074970
152.662195	4873.837439	25.079987
152.682770	4889.799612	25.085005
153.157100	4891.378955	25.090023
153.441936	4887.303440	25.095040
153.614402	4894.258281	25.100058
153.853558	4887.919774	25.105075
153.712848	4879.735886	25.110093
153.755309	4878.012793	25.115111
153.876303	4884.618597	25.120128
153.637869	4886.971982	25.125146
153.695527	4881.369185	25.130163
153.512507	4902.669335	25.135181
153.770261	4914.740278	25.140199
154.107483	4920.480203	25.145216
154.206985	4933.325549	25.150234
154.567709	4939.675894	25.155251
154.429767	4958.887112	25.160269
154.862235	4972.047524	25.165287
154.969257	4970.946940	25.170304
155.247506	4990.897342	25.175322
155.559274	4999.310590	25.180339
155.795647	5005.807561	25.185357
155.688880	5006.341926	25.190375
155.780283	5014.706607	25.195392
155.508416	5034.845010	25.200410
156.210414	5038.982520	25.205427
156.303632	5063.903311	25.210445
156.860790	5052.802395	25.215463
157.080897	5061.133192	25.220480
156.792011	5063.498106	25.225498
157.317317	5068.750154	25.230515
157.284365	5089.868197	25.235533
157.869653	5089.121593	25.240551
157.996172	5084.011373	25.245568
157.996379	5092.862163	25.250586
158.221587	5078.947043	25.255603
158.018555	5091.630745	25.260621
158.459483	5102.837465	25.265639
158.612778	5106.937458	25.270656
158.155781	5116.706660	25.275674
158.567371	5118.596482	25.280691
158.928354	5140.044739	25.285709
159.169819	5143.620581	25.290727
159.269219	5148.169764	25.295744
159.392917	5147.972910	25.300762
159.699908	5146.723434	25.305779
158.987213	5163.697244	25.310797
159.629870	5164.907727	25.315815
160.193208	5166.478665	25.320832
160.424008	5199.460619	25.325850
160.695053	5187.898197	25.330867
160.638601	5194.841452	25.335885
160.926272	5192.235018	25.340903
161.358658	5184.962622	25.345920
161.189318	5191.108630	25.350938
161.270128	5185.851578	25.355955
161.255735	5194.963957	25.360973
161.588800	5203.675434	25.365991
161.479659	5209.716186	25.371008
161.577520	5217.236404	25.376026
161.829381	5221.661133	25.381043
161.558010	5241.192490	25.386061
162.089158	5250.539859	25.391079
162.224935	5257.574181	25.396096
162.325646	5272.105822	25.401114
162.497341	5277.691350	25.406131
162.547426	5286.756879	25.411149
162.320407	5294.293902	25.416167
162.899636	5304.987992	25.421184
162.863235	5316.492836	25.426202
163.293684	5323.172820	25.431219
163.377538	5332.291853	25.436237
163.602933	5340.762114	25.441255
163.728677	5356.615989	25.446272
163.763314	5356.380321	25.451290
164.482502	5363.725290	25.456307
164.392397	5384.638177	25.461325
164.589097	5388.400270	25.466343
164.917655	5387.037730	25.471360
165.002103	5392.866145	25.476378
165.270740	5377.145501	25.481395
165.362657	5408.514272	25.486413
165.293961	5413.901792	25.491431
165.485512	5417.968756	25.496448
165.603383	5428.362051	25.501466
165.971413	5434.530242	25.506483
165.881231	5439.444047	25.511501
165.819535	5445.395125	25.516519
166.563533	5465.582487	25.521536
166.534864	5466.967143	25.526554
166.878436	5469.189607	25.531571
167.177971	5473.512791	25.536589
167.266973	5489.994295	25.541607
167.421905	5488.275357	25.546624
167.659376	5504.944161	25.551642
167.685971	5491.842855	25.556659
168.225052	5495.263970	25.561677
168.184118	5498.955954	25.566695
168.455847	5512.065458	25.571712
168.139979	5527.198715	25.576730
168.388749	5523.397581	25.581747
168.633282	5522.505747	25.586765
168.735507	5541.451086	25.591783
169.081418	5554.657034	25.596800
168.822436	5558.113407	25.601818
168.937050	5562.277418	25.606835
169.615254	5573.192374	25.611853
169.822041	5585.454994	25.616871
170.085129	5584.217479	25.621888
169.364127	5597.914343	25.626906
170.081338	5611.162833	25.631923
170.144776	5625.371753	25.636941
170.436905	5634.544693	25.641959
170.887150	5631.844328	25.646976
170.713245	5639.306562	25.651994
171.368754	5636.591118	25.657011
171.360108	5648.006547	25.662029
171.375612	5656.018685	25.667047
171.546094	5659.786759	25.672064
171.474299	5656.303298	25.677082
171.670860	5672.735683	25.682100
171.944762	5676.338570	25.687117
171.842079	5690.455333	25.692135
172.225565	5705.298921	25.697152
172.111493	5715.130647	25.702170
172.296527	5726.369150	25.707188
172.452440	5742.479904	25.712205
172.625947	5742.941903	25.717223
173.173063	5761.179041	25.722240
173.424121	5769.559435	25.727258
173.479330	5767.677401	25.732276
173.948439	5782.681737	25.737293
174.050932	5795.322512	25.742311
174.427656	5793.134425	25.747328
174.578745	5786.557316	25.752346
174.968592	5790.337151	25.757364
174.780852	5786.364846	25.762381
174.779702	5790.889905	25.767399
175.261963	5801.768937	25.772416
175.246902	5818.754757	25.777434
175.458215	5810.926391	25.782452
175.799804	5815.703461	25.787469
175.890241	5807.517842	25.792487
175.983958	5801.066004	25.797504
175.707849	5823.754037	25.802522
175.794137	5841.164166	25.807540
176.399522	5849.957725	25.812557
176.137369	5859.637630	25.817575
176.375619	5874.187225	25.822592
176.161180	5888.803111	25.827610
176.889158	5901.101775	25.832628
176.902886	5918.667347	25.837645
177.171191	5925.817862	25.842663
177.375140	5926.758424	25.847680
177.354840	5946.575948	25.852698
177.630017	5949.697452	25.857716
177.992946	5960.283664	25.862733
178.210688	5978.624415	25.867751
178.782246	5982.356886	25.872768
178.715259	5991.530414	25.877786
178.861458	5999.549444	25.882804
179.318987	6001.165555	25.887821
179.079534	6001.657334	25.892839
179.457687	6017.585080	25.897856
179.539899	6032.556827	25.902874
179.410635	6034.921448	25.907892
179.526998	6050.647615	25.912909
179.660171	6061.490103	25.917927
180.174066	6084.141452	25.922944
179.647928	6093.583231	25.927962
180.617813	6104.799978	25.932980
180.877949	6114.922072	25.937997
180.967556	6116.935421	25.943015
181.251174	6119.564083	25.948032
181.407353	6134.168461	25.953050
181.490710	6144.852276	25.958068
181.694170	6140.956104	25.963085
181.740098	6151.385415	25.968103
182.025148	6164.931180	25.973120
182.143593	6176.388961	25.978138
181.988377	6180.252823	25.983156
182.568800	6198.978012	25.988173
182.663875	6212.972712	25.993191
183.203955	6221.177117	25.998208
182.967132	6236.505898	26.003226
183.066029	6241.039727	26.008244
183.310955	6252.032400	26.013261
183.484290	6276.229819	26.018279
184.030564	6262.926061	26.023296
184.349054	6271.770504	26.028314
184.213363	6296.153798	26.033332
184.559463	6303.378245	26.038349
184.731434	6297.889134	26.043367
185.243961	6299.500111	26.048384
185.576774	6313.772961	26.053402
185.681282	6320.341928	26.058420
186.022766	6310.946422	26.063437
185.936079	6322.038148	26.068455
186.036665	6316.675843	26.073472
185.943275	6326.275321	26.078490
186.066002	6340.984671	26.083508
186.485396	6343.761023	26.088525
186.416066	6352.650810	26.093543
186.625044	6346.467158	26.098560
186.569976	6362.152703	26.103578
186.757205	6376.474127	26.108596
186.921543	6374.893738	26.113613
187.237160	6393.525159	26.118631
187.458600	6393.834317	26.123648
187.886006	6406.498194	26.128666
187.881602	6406.060249	26.133684
188.366705	6426.097159	26.138701
188.536290	6430.133366	26.143719
188.451406	6427.640392	26.148736
188.385936	6435.307952	26.153754
188.678225	6448.276995	26.158772
189.064454	6443.864517	26.163789
188.872085	6467.306770	26.168807
189.133993	6479.712188	26.173824
189.374714	6490.227622	26.178842
189.433901	6512.327107	26.183860
189.912177	6517.659898	26.188877
189.763261	6533.988903	26.193895
190.044570	6547.799477	26.198912
190.199865	6561.841228	26.203930
190.093751	6580.182728	26.208948
190.934113	6582.516088	26.213965
190.736896	6606.758027	26.218983
191.495043	6604.083722	26.224000
191.654678	6615.381410	26.229018
191.830044	6620.877016	26.234036
192.048893	6632.940752	26.239053
192.050250	6641.487397	26.244071
192.010020	6635.006985	26.249088
192.676035	6656.397358	26.254106
192.942145	6659.092022	26.259124
193.107126	6658.621303	26.264141
193.108691	6692.386292	26.269159
193.363906	6686.854123	26.274176
193.635960	6687.248641	26.279194
193.635644	6696.415477	26.284212
193.822139	6710.107201	26.289229
194.004798	6720.195250	26.294247
194.549927	6730.859728	26.299264
194.669908	6746.708075	26.304282
194.910727	6756.129611	26.309300
195.157405	6750.770543	26.314317
195.171971	6750.314483	26.319335
195.195650	6761.426053	26.324352
195.579253	6782.399417	26.329370
195.779634	6780.002518	26.334388
195.612056	6787.735198	26.339405
196.303325	6813.014223	26.344423
196.423413	6803.806311	26.349440
196.560153	6813.415246	26.354458
196.768102	6828.118816	26.359476
197.248173	6826.616868	26.364493
197.243497	6840.633361	26.369511
196.952262	6833.844699	26.374528
197.674854	6850.930843	26.379546
197.592907	6865.046793	26.384564
197.695580	6866.268048	26.389581
197.481221	6874.978918	26.394599
197.963395	6889.123591	26.399616
198.110191	6900.094364	26.404634
197.993708	6917.543180	26.409652
198.291708	6927.790281	26.414669
198.487908	6957.586850	26.419687
198.970275	6969.051125	26.424704
199.497028	6976.303476	26.429722
199.175004	6990.942910	26.434740
199.907849	7005.276978	26.439757
199.785999	7018.726998	26.444775
200.334280	7016.026719	26.449792
200.581416	7024.828260	26.454810
200.285566	7014.807675	26.459828
200.585280	7019.432937	26.464845
201.071521	7033.174565	26.469863
201.483724	7038.446795	26.474880
201.657612	7042.685666	26.479898
201.453183	7063.155751	26.484916
201.873565	7069.760957	26.489933
201.773384	7069.048985	26.494951
201.815496	7084.470249	26.499968
202.184859	7089.540066	26.504986
202.266531	7104.711409	26.510004
202.536147	7110.416858	26.515021
202.513431	7123.040824	26.520039
202.761008	7139.317416	26.525056
203.168708	7152.534166	26.530074
203.315749	7167.771153	26.535092
203.428318	7179.058919	26.540109
203.364004	7193.744097	26.545127
203.537681	7215.544405	26.550144
204.227766	7222.239722	26.555162
204.452490	7244.898071	26.560180
204.773271	7247.617657	26.565197
205.403734	7255.123932	26.570215
205.066627	7266.107323	26.575232
205.598834	7276.615987	26.580250
205.413915	7280.125846	26.585268
205.829093	7296.227557	26.590285
205.870872	7305.134141	26.595303
206.154781	7312.174789	26.600320
206.560864	7327.376924	26.605338
206.062010	7340.201186	26.610356
206.693135	7346.552645	26.615373
206.530709	7363.220291	26.620391
207.177722	7383.645937	26.625408
207.360584	7393.769828	26.630426
207.960901	7402.279169	26.635444
208.377125	7407.069577	26.640461
208.539835	7423.310098	26.645479
208.686436	7419.110315	26.650496
209.368927	7407.819244	26.655514
209.261574	7427.702650	26.660532
209.429469	7410.392935	26.665549
209.489755	7420.624568	26.670567
209.499120	7433.477414	26.675584
209.735026	7436.173274	26.680602
209.637388	7450.913043	26.685620
210.109599	7462.970916	26.690637
210.298518	7480.521030	26.695655
210.281510	7484.175643	26.700672
210.614401	7485.641619	26.705690
210.407488	7496.291687	26.710708
211.063374	7510.000134	26.715725
211.164015	7514.791617	26.720743
211.367634	7532.414975	26.725760
211.718430	7548.410233	26.730778
211.778713	7556.734148	26.735796
211.994162	7559.786306	26.740813
212.166916	7582.838924	26.745831
212.411938	7592.635209	26.750848
212.455657	7595.094305	26.755866
212.654055	7615.682737	26.760884
213.166324	7614.462113	26.765901
213.653884	7639.190918	26.770919
213.634804	7640.239401	26.775936
214.161190	7642.533532	26.780954
213.852617	7651.912639	26.785972
214.088100	7668.186262	26.790989
214.180339	7674.219030	26.796007
214.641866	7677.426613	26.801024
214.714345	7702.386496	26.806042
214.906420	7715.163637	26.811060
215.192363	7715.953677	26.816077
215.490144	7730.729073	26.821095
215.275578	7748.179281	26.826112
215.509469	7745.320610	26.831130
215.735595	7769.550952	26.836148
216.134273	7768.236479	26.841165
216.428645	7788.818700	26.846183
216.496253	7807.434548	26.851200
217.116377	7817.108223	26.856218
216.947183	7827.576609	26.861236
217.431519	7826.882847	26.866253
217.186590	7839.736367	26.871271
217.623455	7862.927633	26.876288
218.074873	7864.069179	26.881306
218.271067	7884.017123	26.886324
218.378537	7888.524799	26.891341
219.117147	7907.502317	26.896359
218.729044	7909.520141	26.901376
219.123387	7914.147332	26.906394
219.288514	7943.820131	26.911412
219.552801	7952.375944	26.916429
219.690892	7957.254312	26.921447
220.062920	7962.496480	26.926464
220.494372	7964.531462	26.931482
220.209471	7976.333014	26.936500
220.844447	8002.469268	26.941517
220.988079	8002.464439	26.946535
221.051356	8015.356093	26.951552
221.643337	8024.920336	26.956570
222.044333	8034.001029	26.961588
221.589915	8040.081104	26.966605
222.004338	8059.145553	26.971623
222.007785	8063.889485	26.976640
222.181974	8085.423074	26.981658
222.371960	8099.143776	26.986676
223.056310	8111.137093	26.991693
223.235428	8119.457385	26.996711
222.949065	8127.881519	27.001728
223.596541	8141.958200	27.006746
224.047666	8145.804086	27.011764
223.852823	8163.041158	27.016781
224.522907	8181.656177	27.021799
224.442576	8186.600706	27.026816
224.765396	8203.847445	27.031834
225.227863	8211.901104	27.036852
225.082302	8217.037619	27.041869
225.488743	8242.622876	27.046887
225.651327	8242.639330	27.051904
225.761704	8252.166850	27.056922
226.169848	8268.629919	27.061940
226.499514	8270.561268	27.066957
226.830647	8281.763220	27.071975
226.572891	8301.422899	27.076992
227.073988	8306.978604	27.082010
227.139519	8321.885948	27.087028
227.372383	8330.026515	27.092045
227.915512	8335.908486	27.097063
228.055251	8359.529349	27.102080
228.397130	8355.571918	27.107098
228.526833	8365.189259	27.112116
228.329393	8383.641691	27.117133
228.798985	8387.619284	27.122151
228.914165	8399.448659	27.127168
229.266930	8417.787208	27.132186
229.133338	8434.153431	27.137204
229.289706	8432.102304	27.142221
230.089292	8443.683715	27.147239
229.883513	8455.932563	27.152256
230.143028	8454.346458	27.157274
230.398713	8470.853880	27.162292
230.265850	8478.770688	27.167309
230.744192	8504.935273	27.172327
230.854273	8516.991663	27.177344
231.373253	8533.301954	27.182362
231.297174	8543.612023	27.187380
231.331353	8567.716227	27.192397
231.810408	8569.499995	27.197415
232.147082	8596.904466	27.202432
232.352041	8615.411079	27.207450
232.626693	8626.970811	27.212468
232.675305	8643.412644	27.217485
233.332337	8657.595337	27.222503
233.400570	8675.116328	27.227520
233.805833	8687.513134	27.232538
233.827175	8693.715576	27.237556
234.226447	8709.925338	27.242573
234.744914	8723.678067	27.247591
234.736877	8735.446162	27.252608
234.976388	8736.405433	27.257626
235.140498	8756.950598	27.262644
235.484553	8772.225829	27.267661
235.737750	8795.388986	27.272679
235.894411	8799.606759	27.277696
236.295225	8815.721843	27.282714
236.286267	8826.012317	27.287732
236.405426	8837.408877	27.292749
236.809144	8850.083358	27.297767
236.776576	8878.108744	27.302784
237.000801	8882.119202	27.307802
237.299903	8905.330850	27.312820
237.597593	8917.913437	27.317837
238.239728	8934.583457	27.322855
238.178261	8949.726681	27.327872
238.804132	8950.017793	27.332890
239.334881	8967.691783	27.337908
239.038813	8969.388058	27.342925
239.649883	8977.264682	27.347943
239.498683	8998.108922	27.352960
240.069222	9005.302182	27.357978
240.224601	9011.150120	27.362996
240.463484	9036.378379	27.368013
240.450641	9030.844876	27.373031
240.635176	9052.698679	27.378048
240.844602	9057.749915	27.383066
241.052974	9069.985820	27.388084
241.397182	9091.591092	27.393101
241.742487	9097.171291	27.398119
241.626679	9122.174011	27.403136
242.173134	9124.685622	27.408154
242.195834	9150.862091	27.413172
242.651940	9161.604396	27.418189
242.930078	9180.517860	27.423207
242.881468	9193.738581	27.428224
243.248124	9204.964450	27.433242
243.400633	9226.819065	27.438260
243.508431	9244.422361	27.443277
243.824643	9257.054143	27.448295
243.820881	9282.936638	27.453312
244.003036	9295.950658	27.458330
244.432626	9312.714553	27.463348
244.790223	9329.371427	27.468365
245.178079	9342.006385	27.473383
245.696830	9357.457296	27.478400
245.796917	9355.297989	27.483418
245.802724	9379.454589	27.488436
245.969044	9384.377564	27.493453
246.636802	9404.259589	27.498471
246.771441	9425.577009	27.503488
246.940675	9428.321275	27.508506
247.155395	9436.538675	27.513524
247.101854	9449.405916	27.518541
247.842053	9457.392966	27.523559
247.991189	9472.391530	27.528576
248.115496	9483.504880	27.533594
248.255213	9497.130327	27.538612
248.333536	9516.137135	27.543629
249.038472	9533.340965	27.548647
249.059112	9541.888332	27.553664
249.511807	9557.188873	27.558682
249.768814	9569.825975	27.563700
249.790937	9584.905542	27.568717
250.471175	9590.053117	27.573735
250.668798	9605.503854	27.578752
250.819573	9622.492269	27.583770
251.201972	9632.082723	27.588788
251.128589	9642.445833	27.593805
251.709669	9655.441380	27.598823
251.188655	9676.894449	27.603840
251.606733	9697.240431	27.608858
252.243555	9710.071597	27.613876
252.501160	9730.908202	27.618893
252.813264	9733.505974	27.623911
252.985354	9756.039520	27.628928
252.989789	9772.377955	27.633946
253.375912	9786.230714	27.638964
253.332887	9804.395299	27.643981
254.001870	9810.014344	27.648999
254.062224	9832.623216	27.654016
254.395395	9851.040706	27.659034
254.754435	9859.637794	27.664052
254.730479	9880.518837	27.669069
255.363988	9894.077064	27.674087
255.299323	9915.494301	27.679104
255.889047	9931.858126	27.684122
256.090258	9934.858741	27.689140
256.582422	9949.776547	27.694157
256.815674	9963.778452	27.699175
256.964244	9977.094016	27.704192
257.148643	9994.872168	27.709210
257.468189	9999.459569	27.714228
257.532964	10008.987016	27.719245
257.743125	10031.795111	27.724263
258.049245	10049.222290	27.729280
258.317659	10053.536131	27.734298
258.204895	10078.862052	27.739316
258.503139	10101.199515	27.744333
259.267130	10107.062134	27.749351
259.587137	10120.055580	27.754368
259.990761	10137.270547	27.759386
259.995373	10147.754214	27.764404
260.580064	10160.115374	27.769421
260.726329	10177.727506	27.774439
260.819665	10190.280318	27.779456
261.335315	10186.079392	27.784474
261.499411	10214.192727	27.789492
261.611785	10217.218342	27.794509
261.971352	10229.670393	27.799527
262.185417	10245.137144	27.804544
262.342088	10256.243309	27.809562
262.910735	10256.206736	27.814580
262.842958	10282.175491	27.819597
263.262878	10269.603124	27.824615
263.175896	10287.472214	27.829632
263.639455	10306.328740	27.834650
263.762587	10309.342349	27.839668
263.592994	10332.320875	27.844685
264.012047	10338.307644	27.849703
264.095654	10359.697776	27.854720
264.426566	10376.619355	27.859738
265.026256	10394.696339	27.864756
265.087826	10419.782009	27.869773
265.353932	10427.929173	27.874791
265.657721	10442.364949	27.879808
266.008786	10454.461690	27.884826
266.402283	10465.970777	27.889844
266.410437	10483.540714	27.894861
266.955406	10498.644889	27.899879
267.347309	10506.026758	27.904896
267.834672	10522.363225	27.909914
268.063377	10533.539593	27.914932
268.187425	10554.329255	27.919949
268.509748	10569.111093	27.924967
268.946898	10582.501507	27.929984
269.039052	10590.627913	27.935002
269.382302	10592.542334	27.940020
269.180069	10608.608564	27.945037
269.673594	10622.161431	27.950055
270.137743	10638.557008	27.955072
269.982882	10659.481211	27.960090
269.931632	10664.716342	27.965108
270.611598	10698.182096	27.970125
270.893528	10718.610210	27.975143
271.148226	10734.317304	27.980160
271.298021	10760.326448	27.985178
271.828026	10769.708794	27.990196
271.961153	10794.149766	27.995213
272.270006	10803.007783	28.000231
272.772452	10822.058593	28.005248
273.047288	10839.669076	28.010266
273.356964	10850.796020	28.015284
273.599435	10865.395958	28.020301
273.866231	10890.241970	28.025319
273.865924	10899.557752	28.030336
274.263666	10915.520248	28.035354
275.061428	10923.014764	28.040372
274.736829	10945.010563	28.045389
274.865690	10954.525598	28.050407
274.913394	10984.979807	28.055424
275.269748	11013.840338	28.060442
276.144947	11019.450106	28.065460
276.315078	11037.007227	28.070477
276.332953	11045.278519	28.075495
276.923448	11065.539393	28.080512
277.300059	11087.665135	28.085530
277.757665	11101.552107	28.090548
277.834617	11117.870447	28.095565
277.602102	11124.397903	28.100583
278.131908	11151.996160	28.105600
278.363220	11165.791433	28.110618
278.760521	11172.699992	28.115636
278.901884	11199.201296	28.120653
279.093298	11208.945642	28.125671
279.747488	11239.211700	28.130688
279.785073	11254.025539	28.135706
280.216230	11262.493263	28.140724
280.325130	11280.861271	28.145741
280.708511	11290.665285	28.150759
281.054657	11298.928067	28.155776
280.912247	11309.914280	28.160794
281.225982	11320.501966	28.165812
281.349226	11354.660025	28.170829
282.037671	11360.504102	28.175847
281.983388	11383.103393	28.180864
282.116426	11412.962823	28.185882
282.339414	11418.302503	28.190900
282.818407	11441.002699	28.195917
282.861563	11462.545958	28.200935
283.386516	11473.092480	28.205952
283.635673	11496.108134	28.210970
284.094319	11520.742145	28.215988
284.725403	11536.390871	28.221005
284.486468	11555.505384	28.226023
285.037199	11572.829904	28.231040
285.060207	11586.259764	28.236058
286.111412	11600.709171	28.241076
286.111900	11619.360241	28.246093
286.199888	11637.325559	28.251111
286.565119	11655.330101	28.256128
286.875953	11680.069187	28.261146
287.019140	11684.498745	28.266164
287.228008	11711.084262	28.271181
287.224165	11725.279796	28.276199
287.974003	11749.593343	28.281216
288.112668	11774.608473	28.286234
288.403678	11789.469100	28.291252
289.062470	11807.072238	28.296269
289.257796	11830.867851	28.301287
289.655862	11833.942608	28.306304
290.009857	11846.786848	28.311322
290.616186	11867.723713	28.316340
290.658273	11883.065282	28.321357
290.802055	11891.068762	28.326375
291.397157	11908.101074	28.331392
291.232623	11922.736244	28.336410
291.742529	11926.581995	28.341428
291.856340	11946.305155	28.346445
292.010907	11965.274649	28.351463
292.439878	11978.380779	28.356480
292.576209	11998.634482	28.361498
292.950434	12016.606420	28.366516
293.528432	12039.445502	28.371533
293.743696	12050.765396	28.376551
294.125642	12067.262705	28.381568
294.302410	12091.718898	28.386586
294.773008	12096.373300	28.391604
295.298900	12118.010871	28.396621
295.264999	12143.576737	28.401639
295.612557	12139.366897	28.406656
295.146340	12171.804142	28.411674
295.664412	12182.297114	28.416692
295.833819	12213.119569	28.421709
296.172413	12236.865274	28.426727
296.325977	12246.183150	28.431744
296.535389	12277.552231	28.436762
297.254144	12299.046235	28.441780
297.967242	12312.348290	28.446797
297.923296	12335.408922	28.451815
298.516144	12350.147615	28.456832
298.461815	12373.928616	28.461850
298.960985	12394.395381	28.466868
299.108373	12412.595985	28.471885
299.180993	12428.627976	28.476903
299.520599	12448.295461	28.481920
299.597783	12467.153856	28.486938
300.385769	12477.030300	28.491956
300.868431	12480.838147	28.496973
301.352599	12506.638738	28.501991
301.632894	12515.574915	28.507008
301.593250	12524.291425	28.512026
301.853218	12543.745281	28.517044
302.354691	12561.376858	28.522061
302.203080	12579.411243	28.527079
302.554436	12589.429366	28.532096
302.578682	12620.790360	28.537114
303.043672	12636.852166	28.542132
303.661258	12659.011086	28.547149
303.677721	12679.009695	28.552167
304.162747	12691.706847	28.557184
304.294165	12718.302105	28.562202
304.732467	12737.439861	28.567220
305.013181	12750.221306	28.572237
305.151882	12777.759423	28.577255
305.779301	12787.427825	28.582272
305.988035	12817.129172	28.587290
306.261927	12837.695245	28.592308
306.836673	12855.633349	28.597325
307.149999	12882.086876	28.602343
307.010661	12894.296560	28.607360
307.463714	12933.573943	28.612378
307.649609	12953.009030	28.617396
308.328193	12964.059036	28.622413
308.335020	12989.715620	28.627431
308.994272	13002.433033	28.632448
309.068841	13023.183620	28.637466
308.967661	13042.092690	28.642484
309.408336	13071.707257	28.647501
309.649047	13101.195805	28.652519
310.253333	13120.547658	28.657536
310.506693	13146.362252	28.662554
310.756828	13167.323507	28.667572
311.394812	13187.205684	28.672589
311.578763	13217.099399	28.677607
312.117808	13229.272696	28.682624
312.100256	13250.825221	28.687642
312.329284	13275.982146	28.692660
312.758683	13287.562164	28.697677
312.993179	13316.254696	28.702695
313.724839	13342.899764	28.707712
313.513292	13363.895136	28.712730
314.144082	13387.828979	28.717748
314.588871	13407.399842	28.722765
314.528456	13430.814613	28.727783
315.139661	13448.493607	28.732800
315.703135	13469.665000	28.737818
315.913752	13490.306985	28.742836
316.339919	13499.292055	28.747853
316.320134	13521.992618	28.752871
316.687049	13528.765381	28.757888
316.855947	13554.964957	28.762906
317.093543	13575.935117	28.767924
317.659977	13600.776660	28.772941
317.568685	13629.290418	28.777959
317.896957	13651.019478	28.782976
318.310776	13683.353460	28.787994
318.482502	13717.248414	28.793012
318.819549	13741.335412	28.798029
319.122876	13763.811046	28.803047
319.392389	13783.061498	28.808064
319.728652	13824.788981	28.813082
320.298018	13841.209792	28.818100
320.683444	13865.147123	28.823117
320.836470	13900.869000	28.828135
321.345094	13910.151126	28.833152
321.922404	13929.237332	28.838170
321.947852	13943.612767	28.843188
322.423507	13963.084627	28.848205
322.521963	13980.395172	28.853223
323.140903	13994.547914	28.858240
323.388975	14022.656310	28.863258
323.803841	14040.648978	28.868276
323.943162	14058.332664	28.873293
324.198830	14076.531388	28.878311
324.664745	14094.960108	28.883328
324.779026	14112.411593	28.888346
324.876527	14137.720850	28.893364
325.411624	14154.185474	28.898381
325.863127	14182.796328	28.903399
325.983794	14200.316195	28.908416
326.275283	14225.576143	28.913434
326.768582	14251.236143	28.918452
326.763260	14278.375093	28.923469
327.168349	14306.402826	28.928487
327.559572	14328.450186	28.933504
327.649966	14355.425272	28.938522
327.990857	14385.057161	28.943540
328.607195	14424.424581	28.948557
328.281638	14447.720777	28.953575
329.219893	14475.290177	28.958592
329.577582	14499.281887	28.963610
329.814455	14531.437214	28.968628
330.388664	14555.747787	28.973645
330.654418	14577.209458	28.978663
331.345740	14601.525933	28.983680
331.767024	14628.353713	28.988698
331.864996	14647.684008	28.993716
332.251462	14672.325285	28.998733
332.624268	14697.698590	29.003751
333.091037	14716.627491	29.008768
333.446885	14724.573623	29.013786
333.561839	14753.953573	29.018804
334.071083	14770.021193	29.023821
334.256367	14797.937993	29.028839
334.579619	14809.596555	29.033856
334.708481	14840.105999	29.038874
334.995008	14862.368420	29.043892
335.518722	14879.838066	29.048909
335.787849	14922.077505	29.053927
336.146864	14942.324796	29.058944
336.457843	14966.673242	29.063962
336.801278	14998.709400	29.068980
337.348111	15017.737303	29.073997
337.400426	15042.521127	29.079015
337.653510	15069.141048	29.084032
338.065592	15103.227624	29.089050
338.154105	15127.633618	29.094068
338.494031	15152.852303	29.099085
338.986860	15185.191935	29.104103
339.122401	15213.095607	29.109120
339.801187	15235.537914	29.114138
339.950086	15258.856025	29.119156
340.763454	15292.703202	29.124173
340.827343	15326.628785	29.129191
341.198532	15339.788169	29.134208
341.620804	15354.616139	29.139226
341.781663	15397.990637	29.144244
342.295787	15410.218553	29.149261
342.399382	15440.367622	29.154279
342.884001	15468.552827	29.159296
343.838357	15487.189137	29.164314
343.676481	15501.715150	29.169332
344.157587	15532.194372	29.174349
344.371762	15545.266424	29.179367
344.440621	15564.476522	29.184384
344.952937	15593.672414	29.189402
345.180011	15610.843600	29.194420
345.396124	15634.877739	29.199437
345.578062	15662.933688	29.204455
346.177859	15678.270047	29.209472
346.650182	15703.218627	29.214490
346.555562	15730.685259	29.219508
347.379516	15751.100906	29.224525
347.917984	15786.052224	29.229543
347.904682	15804.199657	29.234560
348.578543	15822.977345	29.239578
348.767608	15851.421757	29.244596
348.935111	15874.520145	29.249613
349.000956	15889.514771	29.254631
349.851893	15915.707685	29.259648
350.341303	15946.730093	29.264666
350.210070	15973.282680	29.269684
350.441244	15997.510305	29.274701
350.898797	16039.106698	29.279719
351.232211	16062.732720	29.284736
351.853001	16090.221829	29.289754
352.193520	16125.769342	29.294772
352.816234	16154.979483	29.299789
353.034088	16179.587876	29.304807
353.285991	16204.203280	29.309824
353.455899	16228.457146	29.314842
353.838254	16261.003172	29.319860
353.980739	16278.726552	29.324877
354.226565	16313.828302	29.329895
354.566633	16339.204829	29.334912
355.301360	16365.803874	29.339930
355.468947	16408.273568	29.344948
355.957709	16437.749123	29.349965
355.939722	16464.911106	29.354983
356.350550	16499.853536	29.360000
357.178765	16528.264263	29.365018
357.425371	16573.055753	29.370036
358.227496	16590.686057	29.375053
358.502540	16616.513552	29.380071
358.932458	16645.384469	29.385088
359.450059	16663.769690	29.390106
359.181891	16696.670138	29.395124
359.828937	16710.781176	29.400141
360.285929	16746.879786	29.405159
360.532597	16778.645381	29.410176
361.293076	16798.216910	29.415194
361.246371	16819.209887	29.420212
361.542430	16849.148398	29.425229
362.121405	16874.077945	29.430247
362.134199	16901.727355	29.435264
362.787415	16921.045658	29.440282
362.823655	16960.138415	29.445300
363.259363	16981.371747	29.450317
363.620225	17002.429912	29.455335
363.753933	17038.417150	29.460352
364.845031	17056.931731	29.465370
365.108466	17090.941402	29.470388
365.417459	17117.747685	29.475405
366.002225	17146.704192	29.480423
365.918465	17173.039614	29.485440
366.498259	17192.278960	29.490458
366.933667	17211.745571	29.495476
367.174592	17235.136362	29.500493
367.417860	17272.390687	29.505511
367.530228	17295.985696	29.510528
368.022480	17321.507211	29.515546
368.334907	17360.853130	29.520564
368.376816	17379.057779	29.525581
368.859824	17407.727348	29.530599
369.046724	17445.082818	29.535616
369.414531	17468.098259	29.540634
369.504998	17500.595719	29.545652
370.133688	17532.039431	29.550669
370.682791	17568.247542	29.555687
370.790551	17608.094524	29.560704
371.656923	17629.768156	29.565722
371.676556	17668.945723	29.570740
371.926988	17696.954373	29.575757
372.538995	17730.682242	29.580775
372.816135	17765.833904	29.585792
373.362525	17786.198702	29.590810
373.632758	17827.504275	29.595828
374.089640	17849.931697	29.600845
374.323187	17892.985419	29.605863
374.763891	17932.098646	29.610880
375.539930	17946.088504	29.615898
375.440083	17976.982086	29.620916
375.853100	18006.608539	29.625933
376.539804	18042.211640	29.630951
376.608568	18073.570911	29.635968
377.401670	18100.383786	29.640986
377.551306	18127.755630	29.646004
378.042294	18162.588982	29.651021
378.456991	18194.791367	29.656039
379.076970	18230.539910	29.661056
379.354685	18257.808796	29.666074
379.865137	18281.853236	29.671092
380.018896	18313.684434	29.676109
380.498229	18342.064583	29.681127
380.927845	18365.892363	29.686144
381.730907	18395.860103	29.691162
381.755224	18423.472298	29.696180
382.428836	18447.795806	29.701197
382.633252	18472.058273	29.706215
382.843489	18506.673965	29.711232
383.280408	18521.363628	29.716250
383.703412	18546.433432	29.721268
384.363526	18576.201298	29.726285
384.336904	18595.038166	29.731303
384.550061	18633.541196	29.736320
385.049046	18659.167699	29.741338
385.368263	18699.461539	29.746356
385.810658	18725.357628	29.751373
386.338880	18747.432358	29.756391
386.134224	18793.324491	29.761408
386.643641	18816.732976	29.766426
386.980073	18860.986062	29.771444
387.509509	18900.720626	29.776461
388.096029	18936.728460	29.781479
388.312136	18969.972589	29.786496
388.922835	18997.789799	29.791514
389.076365	19033.819053	29.796532
389.652668	19066.142990	29.801549
390.046526	19083.632272	29.806567
390.101445	19129.589569	29.811584
390.765912	19149.608582	29.816602
391.400597	19182.320364	29.821620
391.754160	19209.581405	29.826637
391.988207	19247.924740	29.831655
392.415292	19280.587516	29.836672
392.833957	19315.944464	29.841690
393.288400	19346.465064	29.846708
393.651163	19367.781309	29.851725
394.016756	19391.042560	29.856743
394.235088	19428.436680	29.861760
394.823367	19453.508871	29.866778
394.956680	19488.383689	29.871796
395.487206	19514.682624	29.876813
395.754551	19532.462904	29.881831
395.889422	19567.853161	29.886848
396.509540	19603.814306	29.891866
396.823706	19636.937901	29.896884
397.248421	19670.495740	29.901901
397.586068	19691.212728	29.906919
397.962459	19731.682473	29.911936
398.214110	19764.140316	29.916954
398.428182	19801.447684	29.921972
398.776596	19836.694385	29.926989
399.485416	19860.348811	29.932007
399.618328	19913.413616	29.937024
400.393741	19941.954017	29.942042
400.692086	19989.475198	29.947060
401.168407	20029.383620	29.952077
401.831397	20055.864865	29.957095
402.098741	20100.506311	29.962112
402.659440	20133.216431	29.967130
403.332356	20160.965369	29.972148
403.405467	20197.265841	29.977165
404.003384	20225.522354	29.982183
404.297359	20257.464899	29.987200
404.838890	20282.637513	29.992218
404.757984	20317.407607	29.997236
405.068799	20357.552314	30.002253
405.677135	20380.897743	30.007271
405.775691	20428.502104	30.012288
406.414920	20464.966455	30.017306
406.953196	20505.627272	30.022324
407.357660	20540.669093	30.027341
407.748836	20572.995043	30.032359
408.189600	20620.631605	30.037376
408.732123	20651.512094	30.042394
409.058643	20692.801230	30.047412
409.552891	20730.195153	30.052429
410.064299	20754.375432	30.057447
410.634680	20802.021013	30.062464
410.926176	20819.841229	30.067482
411.164197	20849.334550	30.072500
411.355031	20891.516952	30.077517
412.116217	20923.323527	30.082535
412.123441	20970.772674	30.087552
412.676064	20996.917338	30.092570
412.960710	21040.623436	30.097588
413.722313	21087.629575	30.102605
414.078196	21121.359371	30.107623
414.363230	21163.202063	30.112640
414.787856	21191.533026	30.117658
415.229962	21237.327939	30.122676
415.916824	21267.037824	30.127693
416.679388	21293.752088	30.132711
416.593709	21335.427931	30.137728
417.254690	21362.652629	30.142746
417.616495	21399.885479	30.147764
417.870686	21434.777433	30.152781
418.289543	21460.998564	30.157799
418.371709	21495.897038	30.162816
418.862927	21533.293244	30.167834
419.690489	21574.689252	30.172852
420.095967	21614.796057	30.177869
420.637798	21650.941672	30.182887
420.825243	21682.778406	30.187904
420.900157	21717.640696	30.192922
421.563955	21748.293416	30.197940
421.724270	21791.194231	30.202957
422.336408	21816.546667	30.207975
422.600401	21851.461510	30.212992
423.176038	21883.702681	30.218010
423.403017	21914.612474	30.223028
423.613160	21959.206808	30.228045
424.207409	21990.260941	30.233063
424.668257	22030.870446	30.238080
425.300458	22067.872382	30.243098
425.756655	22095.557884	30.248116
426.222838	22134.643575	30.253133
426.595426	22166.439542	30.258151
426.959028	22199.545799	30.263168
427.405845	22236.815303	30.268186
427.860822	22269.395691	30.273204
428.061203	22310.572470	30.278221
428.997401	22337.344801	30.283239
429.182403	22382.329150	30.288256
429.448806	22419.682524	30.293274
430.046033	22454.407856	30.298292
430.255929	22488.683311	30.303309
431.005595	22527.052843	30.308327
431.485081	22571.098049	30.313344
431.669408	22600.008838	30.318362
432.052585	22635.277705	30.323380
432.449397	22683.928646	30.328397
432.693304	22713.025297	30.333415
433.536352	22756.157743	30.338432
433.728688	22793.234055	30.343450
434.292815	22837.861997	30.348468
434.505982	22880.455637	30.353485
435.365409	22916.046797	30.358503
435.550763	22960.188991	30.363520
436.020415	22990.227996	30.368538
436.828175	23029.159878	30.373556
437.230122	23075.803725	30.378573
437.575243	23113.615508	30.383591
438.083633	23144.742733	30.388608
438.469373	23176.790717	30.393626
438.935307	23213.754861	30.398644
439.360776	23260.409514	30.403661
439.751260	23281.918500	30.408679
440.092517	23332.466462	30.413696
440.175003	23373.772552	30.418714
440.707313	23413.422661	30.423732
441.262552	23461.964454	30.428749
441.670578	23501.334143	30.433767
441.993515	23537.291346	30.438784
442.422135	23591.651237	30.443802
442.839803	23631.918480	30.448820
443.100919	23676.360647	30.453837
444.377311	23726.602063	30.458855
444.509791	23765.366682	30.463872
445.301892	23798.840380	30.468890
445.717363	23820.073099	30.473908
446.311876	23873.228452	30.478925
446.591286	23900.990307	30.483943
447.014324	23934.736658	30.488960
447.227866	23982.224719	30.493978
448.057862	24010.567426	30.498996
448.319018	24059.757257	30.504013
448.646946	24092.810022	30.509031
448.773931	24125.202232	30.514048
449.063711	24169.224614	30.519066
449.558877	24207.498124	30.524084
450.011807	24268.052121	30.529101
450.536688	24304.942641	30.534119
451.157456	24342.640566	30.539136
451.526502	24387.565051	30.544154
452.025772	24411.001905	30.549172
452.267993	24455.007659	30.554189
452.823633	24495.653090	30.559207
453.232726	24533.771255	30.564224
453.698982	24573.192126	30.569242
454.151954	24615.958576	30.574260
454.417080	24650.360126	30.579277
454.933266	24695.970733	30.584295
455.429204	24736.459449	30.589312
455.800102	24772.840267	30.594330
456.465593	24810.739991	30.599348
456.926604	24862.438090	30.604365
457.335215	24900.664390	30.609383
458.008556	24945.221418	30.614400
458.211168	24988.995385	30.619418
458.921767	25029.055005	30.624436
459.284704	25066.002350	30.629453
459.615245	25098.167157	30.634471
460.325295	25154.893622	30.639488
460.174074	25192.752708	30.644506
460.939714	25231.911069	30.649524
461.308109	25280.096246	30.654541
461.697022	25329.643922	30.659559
462.240781	25375.554574	30.664576
462.385719	25431.274654	30.669594
463.079589	25480.885852	30.674612
463.404573	25533.952172	30.679629
464.273879	25577.989510	30.684647
464.805985	25612.796706	30.689664
465.185437	25666.463188	30.694682
465.846438	25704.832457	30.699700
465.899361	25757.389338	30.704717
466.334590	25793.685969	30.709735
467.202811	25844.187255	30.714752
467.704690	25896.354839	30.719770
468.305418	25933.188994	30.724788
468.585958	25990.311026	30.729805
469.051773	26025.833436	30.734823
469.460152	26070.374139	30.739840
470.061244	26129.847175	30.744858
470.664787	26167.384779	30.749876
471.259070	26204.889300	30.754893
471.493627	26243.131613	30.759911
472.184680	26278.049490	30.764928
472.374370	26329.923067	30.769946
473.353271	26370.556516	30.774964
473.102243	26426.462043	30.779981
473.826869	26461.516682	30.784999
474.271358	26514.988931	30.790016
474.519988	26564.686390	30.795034
475.274696	26599.890898	30.800052
475.586328	26651.007127	30.805069
476.349820	26701.685976	30.810087
477.141308	26743.682486	30.815104
476.975686	26792.950748	30.820122
477.487701	26817.180542	30.825140
477.828973	26878.547655	30.830157
478.549631	26921.086266	30.835175
478.958381	26962.865894	30.840192
479.235318	27026.436538	30.845210
479.984502	27072.443891	30.850228
480.297563	27122.529755	30.855245
480.640294	27164.749807	30.860263
481.111374	27216.809756	30.865280
481.770861	27271.163574	30.870298
482.253926	27324.092512	30.875316
482.753869	27360.085198	30.880333
482.974219	27397.338728	30.885351
483.780164	27443.700449	30.890368
484.303204	27484.191132	30.895386
485.028938	27518.285588	30.900404
485.196743	27560.339965	30.905421
485.559895	27598.333705	30.910439
486.035829	27639.065985	30.915456
486.242538	27699.073397	30.920474
486.667767	27744.852226	30.925492
487.500620	27798.273633	30.930509
487.703947	27846.622615	30.935527
488.220421	27900.920050	30.940544
488.567246	27947.355934	30.945562
489.375144	27997.835636	30.950580
489.833974	28046.275390	30.955597
490.070423	28094.963440	30.960615
490.839627	28142.850510	30.965632
491.109359	28196.110790	30.970650
491.639394	28251.621634	30.975668
492.145664	28307.969432	30.980685
492.291712	28366.695746	30.985703
493.034144	28416.152744	30.990720
493.426147	28482.725599	30.995738
493.945440	28525.746283	31.000756
494.713724	28595.200693	31.005773
495.206143	28651.447786	31.010791
496.017322	28690.612758	31.015808
496.311248	28743.362784	31.020826
496.891200	28791.857127	31.025844
497.424005	28845.120024	31.030861
497.607449	28896.437578	31.035879
498.478230	28947.158858	31.040896
498.996167	29015.602651	31.045914
499.318091	29054.559152	31.050932
499.806078	29114.026418	31.055949
500.437585	29164.847866	31.060967
500.751925	29214.021462	31.065984
501.268621	29273.165876	31.071002
501.941574	29315.879140	31.076020
502.465194	29372.053981	31.081037
502.786961	29424.530130	31.086055
503.576613	29480.061862	31.091072
503.851388	29542.824909	31.096090
504.577102	29586.839406	31.101108
504.867840	29645.404095	31.106125
505.113868	29707.118729	31.111143
505.579683	29758.477267	31.116160
506.377569	29818.984116	31.121178
507.314496	29873.647189	31.126196
507.441817	29926.876356	31.131213
507.747734	29977.962268	31.136231
508.524319	30023.752032	31.141248
508.550077	30085.845186	31.146266
509.184521	30145.222305	31.151284
509.943479	30200.622576	31.156301
510.071221	30258.493770	31.161319
511.167195	30313.810238	31.166336
511.379029	30380.981719	31.171354
512.013358	30426.319652	31.176372
512.527577	30481.120818	31.181389
512.856504	30544.367522	31.186407
513.510086	30585.329681	31.191424
513.934153	30647.535596	31.196442
514.322169	30713.679014	31.201460
515.063788	30767.884983	31.206477
515.484975	30820.071193	31.211495
515.961250	30871.939235	31.216512
516.652628	30930.006492	31.221530
516.971692	30988.223891	31.226548
517.487476	31039.240294	31.231565
517.896547	31086.289460	31.236583
518.461369	31138.642159	31.241600
518.771315	31192.772567	31.246618
519.342589	31246.228850	31.251636
519.902523	31298.002265	31.256653
520.061042	31352.271806	31.261671
520.920529	31416.777989	31.266688
521.488505	31475.883461	31.271706
521.840939	31530.888198	31.276724
522.233313	31590.780381	31.281741
522.639869	31658.129594	31.286759
523.442338	31716.143191	31.291776
523.687278	31784.993168	31.296794
524.190844	31852.317601	31.301812
524.708091	31907.709590	31.306829
525.108297	31971.738448	31.311847
525.950921	32045.687446	31.316864
526.232081	32108.436474	31.321882
526.841204	32176.867997	31.326900
527.397164	32236.943552	31.331917
527.766326	32308.999850	31.336935
528.693466	32365.574999	31.341952
529.217605	32444.929997	31.346970
529.666994	32501.300638	31.351988
530.685837	32560.631739	31.357005
531.456088	32620.509050	31.362023
532.073865	32678.739376	31.367040
532.511387	32732.152853	31.372058
533.051857	32789.023685	31.377076
533.422734	32845.231698	31.382093
533.733435	32911.699045	31.387111
534.560069	32965.490615	31.392128
534.606692	33035.324914	31.397146
535.286160	33087.897913	31.402164
535.872249	33150.985145	31.407181
536.380016	33216.004162	31.412199
537.050129	33275.247038	31.417216
537.622430	33337.166480	31.422234
538.497352	33400.023777	31.427252
539.001330	33452.087275	31.432269
539.587658	33509.716484	31.437287
540.313891	33566.309764	31.442304
540.704819	33621.270422	31.447322
541.431690	33676.904624	31.452340
542.102094	33736.859013	31.457357
542.014511	33782.949812	31.462375
543.008114	33834.586285	31.467392
543.019446	33895.849426	31.472410
543.894198	33946.057413	31.477428
544.557808	34006.405141	31.482445
545.007670	34067.725695	31.487463
545.188345	34117.417856	31.492480
545.569165	34187.554805	31.497498
546.184351	34250.915660	31.502516
547.115060	34304.646713	31.507533
547.584196	34371.001756	31.512551
548.292402	34426.657160	31.517568
548.814860	34492.511523	31.522586
548.889417	34542.424393	31.527604
549.791222	34607.509507	31.532621
549.854337	34667.883080	31.537639
550.475698	34734.069110	31.542656
551.706018	34794.492987	31.547674
552.303144	34855.507842	31.552692
552.846619	34907.771016	31.557709
553.175794	34958.627552	31.562727
553.863960	34997.344007	31.567744
554.549001	35059.193947	31.572762
554.717923	35105.280414	31.577780
555.726220	35146.929733	31.582797
556.193050	35205.783429	31.587815
556.447594	35251.373243	31.592832
556.888440	35306.097266	31.597850
557.163494	35356.758745	31.602868
558.159963	35408.036347	31.607885
558.312640	35470.427091	31.612903
559.341108	35524.893597	31.617920
559.659178	35588.917443	31.622938
559.980498	35662.254409	31.627956
560.895905	35702.348685	31.632973
561.139163	35774.487107	31.637991
561.813975	35821.495326	31.643008
562.379323	35892.810851	31.648026
562.940147	35954.829601	31.653044
563.699558	36012.662294	31.658061
564.098949	36084.002877	31.663079
564.604276	36131.112536	31.668096
564.947882	36200.449212	31.673114
565.492097	36260.297191	31.678132
566.133595	36334.615967	31.683149
566.582180	36401.969768	31.688167
567.381628	36457.546924	31.693184
567.969162	36530.789713	31.698202
568.151208	36596.843808	31.703220
569.436875	36657.432065	31.708237
569.695310	36726.431353	31.713255
569.946520	36791.344789	31.718272
570.821292	36860.624515	31.723290
571.494650	36930.212424	31.728308
572.067465	36987.391047	31.733325
572.497904	37060.191686	31.738343
573.085829	37132.710901	31.743360
573.717011	37185.761544	31.748378
574.039967	37258.587074	31.753396
574.848376	37330.398306	31.758413
575.109770	37395.091272	31.763431
576.223035	37466.805260	31.768448
576.505955	37535.197552	31.773466
577.120920	37610.760081	31.778484
577.732561	37669.288508	31.783501
578.210035	37741.711641	31.788519
578.603142	37817.835697	31.793536
579.519650	37872.902269	31.798554
579.671604	37945.544203	31.803572
580.374525	38020.468909	31.808589
581.070081	38094.719660	31.813607
581.887559	38156.845515	31.818624
582.695530	38236.901917	31.823642
583.183229	38300.414855	31.828660
584.311155	38352.244067	31.833677
584.575452	38417.524133	31.838695
585.094821	38480.890417	31.843712
586.008203	38549.229549	31.848730
585.941808	38608.305616	31.853748
586.564929	38674.287957	31.858765
586.804001	38750.599215	31.863783
587.523710	38812.775044	31.868800
588.214325	38889.122652	31.873818
588.768006	38961.790544	31.878836
589.756165	39022.445384	31.883853
590.324749	39095.256544	31.888871
590.412491	39159.627794	31.893888
591.091704	39225.277708	31.898906
591.608165	39295.004774	31.903924
592.718060	39357.768171	31.908941
592.502102	39425.887058	31.913959
593.384702	39482.700271	31.918976
594.182004	39548.139246	31.923994
594.461564	39621.997832	31.929012
594.981360	39676.611464	31.934029
595.270422	39751.592792	31.939047
595.984647	39819.098355	31.944064
596.658188	39887.778898	31.949082
596.939852	39974.454991	31.954100
597.912987	40055.391697	31.959117
598.391776	40129.121496	31.964135
599.042968	40202.883046	31.969152
599.924973	40286.891641	31.974170
600.151003	40349.084905	31.979188
601.030095	40418.478434	31.984205
601.687236	40501.003607	31.989223
602.265530	40565.731105	31.994240
603.103803	40642.115236	31.999258
603.573483	40712.553086	32.004276
604.286995	40780.078076	32.009293
604.826003	40851.549923	32.014311
605.366064	40926.870177	32.019328
605.848642	40992.334787	32.024346
606.343230	41069.522587	32.029364
606.975201	41150.062783	32.034381
607.603488	41231.547879	32.039399
608.056591	41310.006340	32.044416
608.908442	41389.384151	32.049434
609.519690	41468.221216	32.054452
610.254629	41551.959980	32.059469
610.889582	41635.526241	32.064487
611.460048	41712.328476	32.069504
611.978600	41767.156868	32.074522
612.605891	41855.783029	32.079540
613.430822	41924.149332	32.084557
613.813011	42005.763788	32.089575
614.253013	42101.860282	32.094592
615.106184	42160.252552	32.099610
615.577783	42244.641023	32.104628
616.386742	42325.551688	32.109645
616.976054	42408.071322	32.114663
617.241145	42485.842860	32.119680
618.184707	42553.383609	32.124698
618.470792	42648.469666	32.129716
619.508396	42720.734463	32.134733
619.955121	42805.871544	32.139751
620.582371	42889.810957	32.144768
621.531361	42957.958471	32.149786
621.762818	43047.823988	32.154804
622.753984	43126.160048	32.159821
623.505092	43201.820857	32.164839
624.312428	43278.694558	32.169856
624.711053	43350.489717	32.174874
625.188716	43431.497880	32.179892
625.673889	43503.209845	32.184909
626.547412	43591.184677	32.189927
626.968425	43666.030536	32.194944
627.603528	43740.677090	32.199962
627.981146	43816.474795	32.204980
628.909212	43897.672526	32.209997
629.410278	43990.124951	32.215015
630.122862	44063.721171	32.220032
630.953873	44139.659882	32.225050
631.236294	44239.058270	32.230068
631.879712	44306.415044	32.235085
632.643306	44379.066282	32.240103
632.827122	44459.698077	32.245120
633.759292	44532.003107	32.250138
634.517994	44611.280583	32.255156
635.077385	44671.718572	32.260173
635.869297	44759.093499	32.265191
636.132019	44843.550348	32.270208
636.787121	44912.918752	32.275226
637.099087	45004.854867	32.280244
637.933577	45079.101154	32.285261
638.650690	45161.097079	32.290279
639.231553	45249.993294	32.295296
639.799385	45323.271048	32.300314
640.660746	45407.233515	32.305332
641.452216	45489.082784	32.310349
642.027476	45559.919321	32.315367
642.911503	45650.684003	32.320384
643.544027	45724.059972	32.325402
644.050692	45807.628184	32.330420
644.714847	45870.850457	32.335437
645.752790	45948.470582	32.340455
646.388794	46034.674094	32.345472
647.071825	46102.599136	32.350490
647.331533	46176.613258	32.355508
648.024450	46245.888725	32.360525
648.675293	46330.588001	32.365543
649.168266	46411.243292	32.370560
650.175363	46487.474956	32.375578
650.545521	46573.544899	32.380596
651.125399	46655.361583	32.385613
652.004309	46739.557585	32.390631
652.385955	46833.193165	32.395648
653.300530	46919.373559	32.400666
653.904972	47001.118193	32.405684
654.381533	47084.741220	32.410701
655.289238	47170.465983	32.415719
655.553613	47255.997550	32.420736
656.532078	47342.867210	32.425754
656.578587	47431.704150	32.430772
657.505848	47527.829832	32.435789
658.678053	47604.922916	32.440807
659.409516	47700.535517	32.445824
660.509026	47779.444592	32.450842
660.880898	47866.641213	32.455860
661.442930	47935.868693	32.460877
661.979329	48019.290114	32.465895
662.662396	48106.951123	32.470912
663.538416	48192.265687	32.475930
663.978714	48272.144870	32.480948
664.567198	48362.128157	32.485965
665.443297	48442.858146	32.490983
665.941349	48521.345524	32.496000
666.660113	48595.921575	32.501018
667.628627	48680.850346	32.506036
667.715015	48760.171095	32.511053
668.955229	48841.891068	32.516071
669.460821	48937.780925	32.521088
670.549030	49012.954402	32.526106
670.771364	49097.569454	32.531124
671.219248	49185.675405	32.536141
672.329666	49262.270585	32.541159
672.740155	49348.621121	32.546176
673.468974	49428.978513	32.551194
673.986042	49518.227342	32.556212
674.674332	49607.182954	32.561229
675.368334	49683.166486	32.566247
675.806491	49774.507781	32.571264
676.915892	49861.496697	32.576282
677.609895	49934.133285	32.581300
678.024729	50012.643672	32.586317
678.957821	50088.608201	32.591335
679.576750	50166.166336	32.596352
680.078659	50235.841601	32.601370
680.752502	50315.835923	32.606388
680.999217	50399.230309	32.611405
681.885453	50472.266679	32.616423
682.706805	50566.469964	32.621440
683.331520	50639.126981	32.626458
684.027205	50716.301915	32.631476
684.614912	50800.380724	32.636493
685.403496	50887.591578	32.641511
685.720879	50978.374195	32.646528
686.520742	51061.149277	32.651546
686.968357	51147.015273	32.656564
687.621948	51242.216136	32.661581
688.806301	51323.336771	32.666599
689.383151	51427.736639	32.671616
690.157979	51502.052475	32.676634
690.907631	51588.748576	32.681652
691.547510	51684.421361	32.686669
692.185231	51767.681131	32.691687
692.881408	51862.100933	32.696704
693.673008	51956.972905	32.701722
694.264755	52042.193572	32.706740
695.172279	52132.555435	32.711757
695.811608	52220.125470	32.716775
696.500739	52308.439460	32.721792
696.832547	52397.413138	32.726810
697.701353	52499.079115	32.731828
698.411356	52598.042625	32.736845
699.077131	52687.985853	32.741863
699.607595	52783.650536	32.746880
700.429853	52869.904389	32.751898
701.308746	52965.442826	32.756916
701.480406	53064.965271	32.761933
702.792570	53163.743579	32.766951
703.337699	53266.345275	32.771968
704.064364	53366.358690	32.776986
705.239133	53449.385150	32.782004
705.176708	53551.880344	32.787021
706.109645	53648.341920	32.792039
706.386639	53744.362799	32.797056
707.272327	53852.711247	32.802074
708.252722	53955.888990	32.807092
709.081379	54046.127406	32.812109
709.800937	54135.979916	32.817127
710.541910	54225.248012	32.822144
711.344014	54324.198666	32.827162
712.250201	54416.100301	32.832180
712.892254	54519.027362	32.837197
713.894075	54600.842575	32.842215
714.781263	54706.345875	32.847232
715.565628	54786.580313	32.852250
716.031600	54870.064891	32.857268
716.518205	54960.553624	32.862285
717.369029	55052.334688	32.867303
717.943467	55148.395332	32.872320
718.478590	55245.429688	32.877338
718.968943	55329.771499	32.882356
719.906391	55440.179963	32.887373
720.773818	55524.605557	32.892391
721.487067	55620.740306	32.897408
722.452042	55710.597285	32.902426
722.772946	55806.582997	32.907444
723.632209	55914.289960	32.912461
724.390290	56000.795596	32.917479
725.017980	56096.586627	32.922496
725.584841	56191.844755	32.927514
726.293678	56268.281069	32.932532
726.567877	56371.322821	32.937549
727.402002	56453.268201	32.942567
728.434478	56556.987992	32.947584
728.844349	56639.718364	32.952602
729.796851	56737.657770	32.957620
730.293821	56838.611387	32.962637
731.090768	56921.038771	32.967655
731.705748	57030.845888	32.972672
732.148981	57121.484322	32.977690
732.927252	57217.653932	32.982708
733.581236	57337.225789	32.987725
734.665092	57435.052094	32.992743
735.134805	57552.191193	32.997760
735.812493	57644.189778	33.002778
736.907949	57743.197388	33.007796
737.513191	57851.626668	33.012813
738.311878	57956.454046	33.017831
739.355838	58067.383936	33.022848
739.806611	58167.770494	33.027866
740.521715	58260.593569	33.032884
741.649780	58371.732411	33.037901
742.293003	58471.962260	33.042919
742.963872	58573.060145	33.047936
743.333732	58672.603130	33.052954
744.595134	58769.414376	33.057972
745.314624	58888.453764	33.062989
746.170610	58986.590741	33.068007
746.903676	59083.629923	33.073024
747.636350	59191.836781	33.078042
748.819406	59284.909478	33.083060
749.259920	59396.401527	33.088077
750.251823	59489.601583	33.093095
750.975635	59599.891346	33.098112
751.649144	59694.326842	33.103130
752.787856	59786.897264	33.108148
753.477439	59896.865663	33.113165
754.391554	59974.735730	33.118183
755.044283	60077.139748	33.123200
755.592106	60174.037829	33.128218
756.596609	60268.547652	33.133236
756.834169	60371.312551	33.138253
757.660466	60468.412460	33.143271
758.467764	60577.012537	33.148288
759.516909	60679.657389	33.153306
760.353827	60775.581432	33.158324
760.931061	60882.874963	33.163341
762.131030	60969.373095	33.168359
762.606123	61076.899434	33.173376
763.155963	61182.795938	33.178394
764.268853	61275.864084	33.183412
764.641675	61380.615284	33.188429
765.588483	61476.954241	33.193447
766.164642	61576.780710	33.198464
767.232099	61683.150399	33.203482
767.744330	61772.869107	33.208500
768.643875	61889.279529	33.213517
768.937726	61980.457418	33.218535
769.786490	62090.221683	33.223552
770.315525	62199.976213	33.228570
771.286330	62296.845999	33.233588
771.919444	62417.873423	33.238605
772.802076	62523.753411	33.243623
773.895910	62625.623166	33.248640
774.561989	62742.045431	33.253658
775.433338	62830.931884	33.258676
776.223488	62937.632060	33.263693
776.836417	63041.068847	33.268711
777.519721	63138.299878	33.273728
778.312809	63233.357718	33.278746
779.328492	63321.565021	33.283764
780.079581	63420.372767	33.288781
780.861912	63505.964576	33.293799
781.551541	63603.569699	33.298816
782.143165	63712.253642	33.303834
782.724359	63805.832067	33.308852
783.436946	63906.785090	33.313869
784.288805	64014.068496	33.318887
785.152166	64123.310174	33.323904
785.556528	64228.570015	33.328922
786.694286	64330.175413	33.333940
787.351378	64446.368540	33.338957
787.995544	64553.000045	33.343975
788.835458	64662.084076	33.348992
789.193193	64788.354557	33.354010
789.838002	64891.782661	33.359028
790.743610	65007.539556	33.364045
791.744069	65123.104398	33.369063
792.852830	65250.935022	33.374080
793.616143	65365.282413	33.379098
794.463630	65477.195271	33.384116
795.224005	65598.890318	33.389133
795.751396	65709.997600	33.394151
797.109065	65826.904381	33.399168
797.669984	65954.336813	33.404186
798.399464	66065.684399	33.409204
799.316570	66182.678679	33.414221
800.152968	66298.789234	33.419239
801.233632	66418.027377	33.424256
801.802522	66526.521116	33.429274
802.772967	66632.729936	33.434292
803.456834	66761.006735	33.439309
804.799158	66870.512312	33.444327
805.305371	66984.127102	33.449344
806.086582	67109.418480	33.454362
806.843084	67219.452678	33.459380
807.098629	67326.187864	33.464397
808.255848	67454.776255	33.469415
809.255675	67571.315686	33.474432
810.154309	67692.532127	33.479450
811.002488	67804.982026	33.484468
811.393320	67928.294349	33.489485
812.392032	68044.792315	33.494503
813.403955	68164.513248	33.499520
814.076347	68285.903279	33.504538
815.110103	68400.753528	33.509556
815.803929	68523.962296	33.514573
816.586632	68634.423135	33.519591
817.593439	68747.199544	33.524608
818.475584	68872.649052	33.529626
819.501437	68984.943040	33.534644
820.348843	69107.775711	33.539661
820.902454	69216.785270	33.544679
822.061427	69323.652962	33.549696
822.422247	69452.435762	33.554714
823.253675	69547.117513	33.559732
824.082197	69679.852068	33.564749
824.996685	69789.519366	33.569767
826.157220	69902.238522	33.574784
826.546877	70016.824626	33.579802
827.443360	70134.729376	33.584820
828.228859	70247.455468	33.589837
829.154396	70359.324327	33.594855
830.098895	70475.155315	33.599872
830.885546	70599.454626	33.604890
831.336167	70704.359684	33.609908
832.325422	70801.423740	33.614925
832.964779	70911.319333	33.619943
833.957798	71016.313260	33.624960
834.796308	71127.277293	33.629978
834.850465	71244.435838	33.634996
836.055480	71361.733502	33.640013
837.182059	71472.196374	33.645031
838.380502	71581.294681	33.650048
839.040544	71702.345682	33.655066
839.949643	71818.234015	33.660084
840.499397	71921.825927	33.665101
841.203861	72043.200320	33.670119
842.192677	72150.318905	33.675136
842.641584	72280.147474	33.680154
843.387912	72393.384521	33.685172
844.452851	72526.186055	33.690189
845.158144	72649.056131	33.695207
846.154608	72777.633521	33.700224
846.845600	72906.002910	33.705242
847.593770	73029.139973	33.710260
848.708314	73160.210724	33.715277
849.322088	73283.662360	33.720295
850.393290	73417.612957	33.725312
851.319861	73547.831751	33.730330
852.354144	73671.886398	33.735348
853.186985	73801.692162	33.740365
853.754911	73929.423882	33.745383
854.918951	74051.587242	33.750400
855.718359	74189.129127	33.755418
857.012777	74319.677466	33.760436
857.665337	74445.304829	33.765453
858.268291	74569.024808	33.770471
859.392917	74690.869379	33.775488
860.045731	74823.500064	33.780506
860.805663	74943.660784	33.785524
861.912046	75085.002841	33.790541
862.281478	75210.358844	33.795559
863.319130	75334.232596	33.800576
864.196875	75485.032460	33.805594
865.061212	75612.408702	33.810612
866.292982	75736.404403	33.815629
867.006695	75888.182864	33.820647
868.123161	76009.991806	33.825664
868.475702	76143.179745	33.830682
869.741742	76266.571886	33.835700
870.461882	76402.230561	33.840717
871.114013	76544.947374	33.845735
872.014043	76678.560308	33.850752
872.671239	76811.050390	33.855770
874.113359	76953.120519	33.860788
875.247484	77083.509310	33.865805
875.267616	77216.695403	33.870823
876.731534	77348.372146	33.875840
877.328595	77493.482438	33.880858
878.204584	77619.989058	33.885876
879.154655	77753.650768	33.890893
879.802721	77890.728331	33.895911
880.963502	78023.585110	33.900928
881.964665	78159.511626	33.905946
882.524761	78306.815592	33.910964
883.777105	78429.184593	33.915981
884.757443	78577.300088	33.920999
885.511419	78699.468330	33.926016
886.374905	78845.473184	33.931034
887.315942	78969.984084	33.936052
888.224338	79104.052928	33.941069
889.102580	79237.982063	33.946087
889.821168	79350.816531	33.951104
890.645461	79484.762380	33.956122
891.651009	79606.451129	33.961140
892.684559	79729.957766	33.966157
893.527843	79851.181247	33.971175
894.141589	79979.616998	33.976192
895.143481	80108.963493	33.981210
895.933456	80240.939454	33.986228
896.823391	80367.800825	33.991245
897.643820	80512.469791	33.996263
898.513998	80634.180125	34.001280
899.469892	80763.544286	34.006298
900.043101	80901.025766	34.011316
901.111466	81041.273013	34.016333
901.677799	81183.413473	34.021351
902.890713	81316.236723	34.026368
903.909855	81455.520402	34.031386
904.905283	81594.600081	34.036404
905.782761	81726.633450	34.041421
906.786665	81864.030528	34.046439
907.837067	82005.039523	34.051456
908.665943	82143.416203	34.056474
909.824480	82284.339443	34.061492
910.935125	82410.321583	34.066509
911.663887	82553.506570	34.071527
912.172637	82689.990864	34.076544
913.143309	82830.518306	34.081562
914.151095	82973.090353	34.086580
915.159390	83106.084356	34.091597
915.544423	83253.632794	34.096615
916.698038	83395.202670	34.101632
917.539751	83555.723637	34.106650
918.401981	83704.322239	34.111668
919.637854	83845.204281	34.116685
920.030861	83993.274937	34.121703
921.411959	84146.814283	34.126720
922.273053	84297.650357	34.131738
923.079836	84444.459631	34.136756
924.116671	84593.617164	34.141773
924.873957	84743.701375	34.146791
926.205551	84900.018915	34.151808
926.916895	85040.216688	34.156826
928.052073	85195.347507	34.161844
929.043658	85329.597202	34.166861
929.761917	85477.294485	34.171879
930.824901	85630.668439	34.176896
932.017967	85778.852262	34.181914
932.942389	85929.618819	34.186932
933.886769	86065.304255	34.191949
934.567226	86226.870072	34.196967
935.946997	86362.023305	34.201984
937.038461	86516.961298	34.207002
937.792701	86656.535205	34.212020
939.063610	86787.779322	34.217037
939.678098	86928.776406	34.222055
940.511895	87078.730041	34.227072
940.985016	87226.554797	34.232090
942.284818	87377.471055	34.237108
943.277086	87524.939726	34.242125
944.108739	87678.656378	34.247143
944.994114	87820.082263	34.252160
945.771529	87966.209681	34.257178
946.399085	88132.663642	34.262196
947.735605	88279.402965	34.267213
948.543788	88429.198523	34.272231
949.311313	88579.919355	34.277248
950.087647	88732.772342	34.282266
951.191760	88889.147655	34.287284
952.519416	89035.513402	34.292301
953.065103	89186.407647	34.297319
954.010551	89329.250148	34.302336
955.024910	89463.810685	34.307354
955.983717	89621.303330	34.312372
956.955491	89762.846703	34.317389
958.067056	89912.177379	34.322407
958.395222	90063.910533	34.327424
959.281604	90210.438707	34.332442
960.190183	90375.292287	34.337460
961.344912	90525.239857	34.342477
962.058430	90700.893270	34.347495
962.910141	90858.057310	34.352512
963.906488	91014.230126	34.357530
964.631542	91185.011852	34.362548
965.964690	91352.662616	34.367565
966.843558	91525.395974	34.372583
967.790073	91689.125670	34.377600
968.775934	91858.191793	34.382618
969.474086	92033.775139	34.387636
970.794809	92197.066628	34.392653
971.803036	92368.835203	34.397671
972.773002	92543.503834	34.402688
973.833812	92715.399074	34.407706
974.376467	92894.349928	34.412724
975.524256	93064.524290	34.417741
976.280187	93233.194905	34.422759
977.327929	93407.128950	34.427776
978.491966	93592.970023	34.432794
979.136274	93779.012376	34.437812
980.328130	93946.058709	34.442829
981.535203	94138.251832	34.447847
982.084256	94316.857531	34.452864
983.587416	94503.219089	34.457882
984.266083	94681.660409	34.462900
985.562600	94860.741459	34.467917
986.390401	95034.058716	34.472935
987.221183	95217.542749	34.477952
988.508286	95409.884451	34.482970
989.288148	95603.343331	34.487988
990.705229	95775.745413	34.493005
991.223897	95958.672498	34.498023
992.390277	96152.280632	34.503040
993.564504	96336.659344	34.508058
994.471034	96521.229281	34.513076
995.596319	96693.666968	34.518093
996.226884	96890.711884	34.523111
997.191019	97070.300593	34.528128
998.491249	97255.557845	34.533146
999.372922	97446.323668	34.538164
1000.556778	97630.153214	34.543181
1001.233983	97827.216754	34.548199
1002.296665	98020.571580	34.553216
1003.429506	98200.178444	34.558234
1004.310106	98402.720644	34.563252
1005.750080	98582.437711	34.568269
1006.524699	98771.319319	34.573287
1007.895700	98961.104019	34.578304
1008.716603	99145.397121	34.583322
1009.252354	99331.581052	34.588340
1010.519482	99522.969895	34.593357
1011.779697	99718.191682	34.598375
1012.663626	99899.250916	34.603392
1013.874751	100080.985428	34.608410
1014.525484	100269.822657	34.613428
1015.580031	100467.793982	34.618445
1016.548376	100658.607598	34.623463
1017.489018	100835.346050	34.628480
1018.628165	101013.680092	34.633498
1019.621039	101201.043013	34.638516
1020.717324	101375.131849	34.643533
1021.622225	101545.353220	34.648551
1022.536571	101731.909871	34.653568
1023.819408	101905.768827	34.658586
1024.582282	102093.834756	34.663604
1025.642875	102268.885280	34.668621
1026.581826	102454.613604	34.673639
1027.349108	102638.991286	34.678656
1028.611339	102825.207019	34.683674
1029.646990	103027.025578	34.688692
1030.572135	103212.698277	34.693709
1031.254787	103408.398085	34.698727
1032.098005	103604.326095	34.703744
1033.495260	103801.139124	34.708762
1034.347050	104001.906477	34.713780
1035.731345	104195.849783	34.718797
1036.385549	104402.769848	34.723815
1037.305256	104607.659277	34.728832
1038.414106	104810.479988	34.733850
1039.450488	105013.947487	34.738868
1040.557363	105224.117370	34.743885
1041.537033	105434.689910	34.748903
1042.601550	105634.066689	34.753920
1043.765940	105848.411547	34.758938
1044.554909	106064.808681	34.763956
1045.546179	106277.019829	34.768973
1046.918203	106490.119638	34.773991
1047.746694	106706.021487	34.779008
1049.067665	106919.981777	34.784026
1049.720587	107143.946340	34.789044
1050.923920	107354.725068	34.794061
1052.462258	107564.905421	34.799079
1053.367930	107786.249662	34.804096
1054.484830	107990.220558	34.809114
1055.342897	108204.938943	34.814132
1056.489920	108414.151979	34.819149
1057.700598	108638.518095	34.824167
1058.344683	108862.701081	34.829184
1059.759024	109076.688414	34.834202
1060.768990	109296.115084	34.839220
1062.003682	109506.614092	34.844237
1063.173594	109720.697579	34.849255
1063.913442	109952.410680	34.854272
1065.074859	110159.012656	34.859290
1066.030940	110388.983616	34.864308
1067.194544	110603.771777	34.869325
1068.496178	110812.889021	34.874343
1069.597756	111044.589562	34.879360
1070.617588	111254.390145	34.884378
1071.862068	111485.247358	34.889396
1072.735014	111691.148478	34.894413
1073.601171	111916.168523	34.899431
1074.874865	112129.518880	34.904448
1076.077082	112354.106874	34.909466
1077.140673	112577.668122	34.914484
1078.581456	112796.722137	34.919501
1079.773420	113004.239848	34.924519
1081.060575	113223.753357	34.929536
1082.147724	113421.865941	34.934554
1082.784894	113638.741029	34.939572
1083.823401	113853.448380	34.944589
1085.289178	114056.798525	34.949607
1086.062689	114285.273679	34.954624
1087.250246	114491.941637	34.959642
1088.457471	114713.836524	34.964660
1089.250591	114920.091393	34.969677
1090.420723	115124.397664	34.974695
1091.334923	115329.191162	34.979712
1092.401493	115522.659483	34.984730
1093.322414	115743.368138	34.989748
1094.244572	115947.366578	34.994765
1095.642546	116152.187392	34.999783
1096.205845	116373.086754	35.004800
1097.473386	116571.913811	35.009818
1098.471098	116793.074028	35.014836
1099.580192	117010.378389	35.019853
1100.671963	117230.031313	35.024871
1101.311150	117458.351447	35.029888
1102.797691	117670.631505	35.034906
1103.646233	117903.697433	35.039924
1104.882012	118138.551183	35.044941
1105.612152	118351.468138	35.049959
1106.990010	118586.935592	35.054976
1107.973886	118817.769057	35.059994
1109.261401	119054.218254	35.065012
1110.797791	119300.068469	35.070029
1111.452062	119525.031788	35.075047
1112.350160	119767.836248	35.080064
1113.906985	120002.195796	35.085082
1115.002719	120235.112823	35.090100
1116.015736	120479.260069	35.095117
1117.114591	120712.129674	35.100135
1117.963069	120944.307526	35.105152
1119.525679	121187.647471	35.110170
1120.717752	121435.169202	35.115188
1121.754104	121664.888556	35.120205
1122.985342	121912.724613	35.125223
1123.921175	122147.026447	35.130240
1125.315080	122389.187565	35.135258
1126.488519	122633.718909	35.140276
1127.721737	122867.622400	35.145293
1128.836844	123107.389543	35.150311
1129.855616	123355.171317	35.155328
1131.107026	123581.942363	35.160346
1132.434356	123832.465186	35.165364
1133.238100	124070.529880	35.170381
1134.508066	124313.854963	35.175399
1135.363266	124561.217440	35.180416
1136.884347	124800.271901	35.185434
1138.166196	125042.979857	35.190452
1139.310303	125290.541318	35.195469
1140.524789	125527.637014	35.200487
1141.556329	125768.807866	35.205504
1142.937264	126007.045793	35.210522
1144.248677	126244.371833	35.215540
1145.117913	126492.394042	35.220557
1146.262481	126734.288922	35.225575
1147.516674	126973.277745	35.230592
1148.605699	127210.343804	35.235610
1149.904945	127455.590263	35.240628
1151.167084	127691.338548	35.245645
1152.515778	127928.240423	35.250663
1153.296322	128174.833147	35.255680
1154.847578	128406.102739	35.260698
1155.840279	128643.753370	35.265716
1157.095773	128878.092091	35.270733
1158.561760	129122.145288	35.275751
1159.514253	129361.037538	35.280768
1160.324436	129598.345305	35.285786
1161.402571	129825.976906	35.290804
1162.429974	130069.159258	35.295821
1163.862590	130309.513115	35.300839
1165.118100	130550.278358	35.305856
1166.304235	130778.089096	35.310874
1167.277953	131007.381683	35.315892
1168.437839	131239.269165	35.320909
1169.673192	131464.718862	35.325927
1170.563582	131689.770816	35.330944
1172.044084	131910.277283	35.335962
1172.782551	132143.572034	35.340980
1173.740849	132381.687381	35.345997
1174.910101	132607.333510	35.351015
1175.890486	132847.489638	35.356032
1177.183094	133098.358844	35.361050
1178.620815	133339.152942	35.366068
1179.623613	133587.538389	35.371085
1180.776072	133830.272208	35.376103
1181.700695	134081.121090	35.381120
1182.854559	134328.016614	35.386138
1183.901627	134579.863293	35.391156
1184.773347	134831.981771	35.396173
1186.106086	135088.006845	35.401191
1187.117035	135358.248464	35.406208
1188.600164	135611.324119	35.411226
1189.534021	135887.364038	35.416244
1190.813968	136154.879916	35.421261
1191.816656	136411.920675	35.426279
1192.912617	136681.322252	35.431296
1194.092029	136951.954718	35.436314
1195.435230	137225.744665	35.441332
1196.648440	137496.185763	35.446349
1198.270579	137767.220749	35.451367
1199.183793	138041.963275	35.456384
1200.305699	138320.642117	35.461402
1201.790399	138589.614369	35.466420
1202.884637	138864.878865	35.471437
1204.161696	139151.653685	35.476455
1205.357073	139423.457167	35.481472
1206.632292	139693.461784	35.486490
1208.281215	139972.586913	35.491508
1209.311290	140246.947537	35.496525
1210.828964	140509.221819	35.501543
1212.088564	140789.800058	35.506560
1213.021286	141058.819568	35.511578
1214.715296	141332.457753	35.516596
1215.644781	141605.767977	35.521613
1217.099986	141867.720512	35.526631
1218.285410	142141.766146	35.531648
1219.750453	142411.177310	35.536666
1221.176662	142686.049694	35.541684
1222.079100	142951.183140	35.546701
1223.550381	143216.503539	35.551719
1224.691125	143485.012790	35.556736
1225.618051	143752.671742	35.561754
1226.927334	144021.537639	35.566772
1228.372092	144298.854315	35.571789
1229.756674	144560.077673	35.576807
1230.700189	144837.988652	35.581824
1231.928085	145112.430744	35.586842
1233.006738	145379.556886	35.591860
1234.075189	145659.102201	35.596877
1235.276701	145932.045775	35.601895
1236.585474	146209.374341	35.606912
1237.255200	146494.534066	35.611930
1238.728158	146773.057289	35.616948
1239.759915	147068.193305	35.621965
1241.223153	147354.978770	35.626983
1242.281425	147641.934880	35.632000
1243.318235	147923.113511	35.637018
1245.061476	148215.794889	35.642036
1246.158838	148505.173670	35.647053
1247.580134	148784.367531	35.652071
1248.753195	149055.221062	35.657088
1249.895259	149321.490411	35.662106
1250.979715	149593.859113	35.667124
1252.060506	149873.079376	35.672141
1253.817301	150136.792378	35.677159
1254.912389	150428.520215	35.682176
1256.061312	150704.234764	35.687194
1257.526035	150964.450448	35.692212
1258.404657	151256.651711	35.697229
1259.351806	151534.752154	35.702247
1260.749359	151817.917177	35.707264
1261.888039	152101.596399	35.712282
1263.081299	152389.023204	35.717300
1264.355029	152688.603027	35.722317
1265.736123	152974.772803	35.727335
1266.697681	153277.389616	35.732352
1267.859020	153569.790118	35.737370
1269.438811	153873.374905	35.742388
1270.572783	154171.771598	35.747405
1271.885738	154479.502374	35.752423
1273.270596	154786.513333	35.757440
1274.589190	155083.491127	35.762458
1276.180417	155388.341602	35.767476
1277.328312	155700.992991	35.772493
1278.398974	155995.481589	35.777511
1279.866978	156305.788803	35.782528
1281.169848	156616.886859	35.787546
1282.869262	156909.844842	35.792564
1284.172563	157207.158195	35.797581
1285.423344	157513.451269	35.802599
1286.567700	157813.992191	35.807616
1287.954018	158120.622677	35.812634
1289.630718	158407.467988	35.817652
1290.979170	158724.600661	35.822669
1292.493901	159025.850510	35.827687
1293.544062	159326.760712	35.832704
1294.784185	159627.159639	35.837722
1296.349261	159936.552543	35.842740
1297.293039	160242.751931	35.847757
1298.513948	160531.260566	35.852775
1299.860615	160834.238742	35.857792
1301.324726	161143.720774	35.862810
1302.770565	161453.030499	35.867828
1303.869088	161757.921370	35.872845
1305.617468	162056.604517	35.877863
1307.078056	162349.983322	35.882880
1308.362763	162670.074722	35.887898
1310.114033	162971.453568	35.892916
1311.069107	163263.019113	35.897933
1311.932986	163561.440343	35.902951
1313.267290	163872.181791	35.907968
1314.359585	164175.873001	35.912986
1316.458994	164467.587482	35.918004
1317.513978	164771.200227	35.923021
1318.880609	165083.505664	35.928039
1320.588438	165388.105993	35.933056
1321.633194	165687.298648	35.938074
1323.218549	165975.542794	35.943092
1324.492562	166285.753165	35.948109
1325.699076	166578.644384	35.953127
1327.090215	166891.948333	35.958144
1328.244983	167182.999561	35.963162
1329.913179	167480.159947	35.968180
1330.929160	167788.507452	35.973197
1332.081695	168090.946847	35.978215
1333.324104	168389.985454	35.983232
1334.637833	168704.774109	35.988250
1335.786921	169003.083534	35.993268
1337.049746	169291.973375	35.998285
1338.599185	169577.924508	36.003303
1340.059569	169867.597456	36.008320
1340.850915	170168.727213	36.013338
1342.457580	170448.037698	36.018356
1343.879950	170758.964893	36.023373
1344.703325	171049.816466	36.028391
1346.269237	171343.846495	36.033408
1347.369870	171662.840176	36.038426
1348.501728	171960.498988	36.043444
1349.962898	172268.308078	36.048461
1351.240472	172580.819493	36.053479
1352.736383	172885.784266	36.058496
1354.062933	173197.910943	36.063514
1355.908687	173507.568062	36.068532
1356.903349	173818.345002	36.073549
1358.195726	174137.019046	36.078567
1359.634054	174453.069490	36.083584
1360.988607	174777.080242	36.088602
1362.378971	175089.893931	36.093620
1363.607631	175419.145683	36.098637
1365.136539	175736.166681	36.103655
1366.425401	176061.250147	36.108672
1367.869863	176393.658215	36.113690
1369.120539	176717.521259	36.118708
1370.578390	177044.677298	36.123725
1371.692311	177375.877416	36.128743
1373.145416	177702.429347	36.133760
1374.232372	178041.443567	36.138778
1375.681371	178371.122627	36.143796
1377.075582	178715.954123	36.148813
1378.069699	179061.564807	36.153831
1379.781568	179400.002507	36.158848
1381.446412	179741.635894	36.163866
1382.839915	180091.007778	36.168884
1384.084176	180431.877540	36.173901
1385.410270	180775.705992	36.178919
1387.043173	181108.964060	36.183936
1388.447309	181457.505624	36.188954
1390.114410	181801.868278	36.193972
1391.298794	182149.194150	36.198989
1392.600415	182494.840171	36.204007
1394.042493	182841.010998	36.209024
1395.283333	183192.167505	36.214042
1396.847259	183531.874677	36.219060
1398.176752	183883.287562	36.224077
1399.465269	184241.855675	36.229095
1400.895896	184581.489861	36.234112
1402.091889	184940.318988	36.239130
1403.852991	185296.023356	36.244148
1405.446189	185647.886261	36.249165
1406.770442	185999.046908	36.254183
1408.329544	186346.020153	36.259200
1409.607280	186723.887535	36.264218
1411.151565	187069.522139	36.269236
1412.548500	187428.955943	36.274253
1413.825403	187786.761632	36.279271
1415.470147	188129.123703	36.284288
1416.301238	188488.467211	36.289306
1417.916355	188849.028954	36.294324
1419.201350	189210.815336	36.299341
1420.377711	189572.748837	36.304359
1421.954300	189937.246144	36.309376
1423.379497	190307.622828	36.314394
1425.031329	190661.512303	36.319412
1426.655770	191023.342490	36.324429
1427.591818	191388.855790	36.329447
1429.142102	191739.099611	36.334464
1430.363631	192096.419983	36.339482
1431.843223	192439.075317	36.344500
1433.085320	192793.654251	36.349517
1434.438223	193152.647457	36.354535
1435.745549	193486.755226	36.359552
1437.270490	193849.405576	36.364570
1438.893512	194201.225484	36.369588
1440.504250	194556.807180	36.374605
1441.382723	194926.806830	36.379623
1443.164570	195271.827085	36.384640
1444.399758	195632.453412	36.389658
1446.130253	195991.286001	36.394676
1447.566158	196363.804356	36.399693
1448.899452	196734.234296	36.404711
1450.481118	197086.356048	36.409728
1451.643632	197464.473849	36.414746
1452.749220	197833.398655	36.419764
1454.245641	198207.745573	36.424781
1455.850728	198590.786108	36.429799
1457.670075	198968.461022	36.434816
1459.156773	199351.792010	36.439834
1460.495354	199727.138258	36.444852
1462.255169	200101.007641	36.449869
1463.151715	200488.416380	36.454887
1464.661920	200858.141236	36.459904
1466.155011	201255.028763	36.464922
1467.702974	201650.157303	36.469940
1469.413286	202036.919473	36.474957
1470.310954	202426.370038	36.479975
1472.229834	202823.322833	36.484992
1473.655221	203213.693455	36.490010
1475.250268	203606.183897	36.495028
1477.079774	204003.767272	36.500045
1478.212321	204394.395640	36.505063
1479.586853	204788.198432	36.510080
1481.062100	205189.896996	36.515098
1482.348435	205581.801182	36.520116
1484.009278	205985.441325	36.525133
1485.548780	206386.906963	36.530151
1487.022198	206782.468554	36.535168
1488.660299	207189.242250	36.540186
1490.215243	207597.517391	36.545204
1491.727232	208003.173292	36.550221
1493.182399	208392.866862	36.555239
1494.676301	208801.945443	36.560256
1496.126939	209209.712635	36.565274
1497.741675	209618.470558	36.570292
1499.288639	210022.086300	36.575309
1500.626405	210429.979694	36.580327
1502.503633	210838.979540	36.585344
1503.877106	211250.985155	36.590362
1504.813262	211647.954097	36.595380
1506.877682	212056.903396	36.600397
1508.626284	212467.176617	36.605415
1510.005549	212872.154034	36.610432
1511.781172	213286.642444	36.615450
1513.107363	213681.676688	36.620468
1514.859881	214085.835980	36.625485
1516.466222	214499.773755	36.630503
1518.292958	214905.473612	36.635520
1519.319074	215305.034330	36.640538
1521.085775	215702.188596	36.645556
1523.046905	216104.010971	36.650573
1524.443690	216501.661436	36.655591
1525.937164	216890.382890	36.660608
1527.422464	217302.778183	36.665626
1528.808398	217687.533065	36.670644
1530.611516	218073.668202	36.675661
1531.714414	218463.298482	36.680679
1533.464484	218838.320843	36.685696
1535.024534	219223.281379	36.690714
1536.507016	219598.884082	36.695732
1537.864211	219976.210542	36.700749
1539.186515	220363.373436	36.705767
1540.976892	220743.272523	36.710784
1542.550766	221129.507657	36.715802
1543.770632	221513.770724	36.720820
1545.749583	221902.379966	36.725837
1546.788409	222294.854171	36.730855
1548.149453	222671.097155	36.735872
1550.083039	223082.424945	36.740890
1551.236742	223480.675322	36.745908
1552.902852	223868.834979	36.750925
1553.965125	224280.234757	36.755943
1555.941027	224685.516077	36.760960
1557.337413	225100.698835	36.765978
1558.749227	225582.885438	36.770996
1560.183601	225997.836351	36.776013
1561.838478	226412.218808	36.781031
1563.296239	226826.152580	36.786048
1564.984129	227248.076145	36.791066
1566.320101	227684.156405	36.796084
1568.086041	228092.607612	36.801101
1569.333854	228524.107713	36.806119
1570.875748	228953.833360	36.811136
1572.514675	229381.055053	36.816154
1574.257205	229822.764755	36.821172
1576.025613	230249.002460	36.826189
1577.766981	230698.055892	36.831207
1579.066830	231118.124936	36.836224
1580.615744	231557.992230	36.841242
1582.291392	232005.256992	36.846260
1584.103707	232434.110020	36.851277
1585.447540	232878.206169	36.856295
1587.534280	233311.232858	36.861312
1589.369031	233751.795748	36.866330
1590.944068	234191.285059	36.871348
1592.462378	234622.554802	36.876365
1593.692299	235059.029799	36.881383
1595.266626	235503.094895	36.886400
1597.029928	235950.127288	36.891418
1598.701921	236388.513868	36.896436
1600.200450	236819.665223	36.901453
1601.733365	237274.511855	36.906471
1603.397361	237717.881631	36.911488
1605.351505	238170.323801	36.916506
1606.966182	238613.729134	36.921524
1608.451454	239052.863846	36.926541
1610.265075	239498.194173	36.931559
1611.681153	239938.866286	36.936576
1613.421681	240386.852348	36.941594
1614.757879	240833.102532	36.946612
1616.658289	241278.422097	36.951629
1618.335776	241728.885216	36.956647
1620.158591	242176.327674	36.961664
1621.926966	242610.697634	36.966682
1623.054914	243055.182734	36.971700
1624.790820	243491.134491	36.976717
1626.540431	243954.036888	36.981735
1628.241517	244398.683541	36.986752
1629.673904	244844.086543	36.991770
1631.192677	245296.334686	36.996788
1633.011188	245731.818942	37.001805
1634.717560	246185.104299	37.006823
1636.489191	246626.541766	37.011840
1638.378058	247066.080623	37.016858
1639.850805	247497.432814	37.021876
1641.589904	247911.670726	37.026893
1642.819948	248332.521743	37.031911
1644.509907	248757.031474	37.036928
1646.049855	249185.681709	37.041946
1647.662041	249608.071283	37.046964
1649.732438	250032.544820	37.051981
1650.847827	250470.462311	37.056999
1652.270044	250898.346072	37.062016
1653.881723	251336.919007	37.067034
1655.069217	251777.442186	37.072052
1656.642144	252222.499996	37.077069
1658.516941	252696.061445	37.082087
1660.012645	253146.568912	37.087104
1661.971738	253595.018653	37.092122
1663.303944	254060.058896	37.097140
1665.019021	254516.805479	37.102157
1666.523907	254982.935392	37.107175
1668.157247	255449.272907	37.112192
1670.470225	255911.713236	37.117210
1671.280437	256390.202783	37.122228
1672.931284	256854.810410	37.127245
1674.917015	257338.618515	37.132263
1676.215382	257816.468840	37.137280
1677.978543	258294.293241	37.142298
1679.397361	258794.351622	37.147316
1681.085756	259269.546433	37.152333
1682.917595	259762.322000	37.157351
1684.824613	260259.556060	37.162368
1686.637089	260746.237865	37.167386
1687.901744	261246.880226	37.172404
1689.880199	261739.021440	37.177421
1691.797402	262240.648001	37.182439
1693.516746	262736.870723	37.187456
1695.258501	263238.449577	37.192474
1696.710768	263736.824348	37.197492
1698.727074	264223.013714	37.202509
1700.299820	264736.000173	37.207527
1701.924349	265242.550681	37.212544
1703.548970	265742.699163	37.217562
1705.264434	266256.829322	37.222580
1707.378229	266759.360185	37.227597
1709.349008	267259.018216	37.232615
1710.683338	267766.579574	37.237632
1712.387607	268269.811544	37.242650
1714.048806	268790.705099	37.247668
1715.947245	269287.298977	37.252685
1717.636906	269808.338892	37.257703
1719.399795	270319.763680	37.262720
1721.579384	270824.209318	37.267738
1722.782376	271339.433868	37.272756
1724.752530	271846.630620	37.277773
1726.883771	272354.028555	37.282791
1728.256794	272865.970920	37.287808
1729.959944	273377.070362	37.292826
1731.307671	273889.345275	37.297844
1733.368642	274399.138967	37.302861
1735.151120	274916.598392	37.307879
1737.036840	275430.788186	37.312896
1738.571467	275938.709687	37.317914
1740.204468	276452.786607	37.322932
1742.155105	276961.043597	37.327949
1744.013236	277485.622913	37.332967
1745.637773	278007.292890	37.337984
1747.192916	278525.137322	37.343002
1748.784840	279037.563744	37.348020
1750.838641	279555.348581	37.353037
1752.526278	280063.692218	37.358055
1753.822614	280575.883994	37.363072
1755.870643	281058.941428	37.368090
1757.865991	281563.140465	37.373108
1759.299160	282056.914662	37.378125
1761.548194	282547.758544	37.383143
1763.100644	283059.824659	37.388160
1764.814805	283542.727129	37.393178
1766.475646	284053.044973	37.398196
1768.259472	284554.501260	37.403213
1769.767645	285052.750132	37.408231
1771.031583	285568.894665	37.413248
1773.154970	286074.887518	37.418266
1774.977966	286607.878579	37.423284
1776.626563	287124.233588	37.428301
1778.900194	287643.099776	37.433319
1780.090887	288175.910018	37.438336
1782.042355	288691.396430	37.443354
1783.307605	289225.993705	37.448372
1785.056125	289763.303053	37.453389
1787.055473	290300.492573	37.458407
1788.551331	290846.754630	37.463424
1790.666048	291378.154746	37.468442
1792.409764	291930.187746	37.473460
1793.810327	292473.156426	37.478477
1795.963287	293026.412245	37.483495
1797.611192	293582.974628	37.488512
1799.540120	294129.099602	37.493530
1801.051795	294694.060938	37.498548
1802.948303	295248.720050	37.503565
1804.849468	295821.231125	37.508583
1806.363172	296382.754696	37.513600
1808.568343	296941.087909	37.518618
1810.234458	297521.273813	37.523636
1812.323344	298090.846331	37.528653
1813.910290	298653.742653	37.533671
1815.607458	299232.694707	37.538688
1817.906570	299803.416648	37.543706
1819.503005	300381.184966	37.548724
1821.550997	300953.490978	37.553741
1823.418944	301524.350265	37.558759
1824.950462	302107.071485	37.563776
1827.336544	302675.374701	37.568794
1829.236548	303259.018361	37.573812
1831.001479	303831.505947	37.578829
1832.933088	304403.987773	37.583847
1834.600603	304993.144315	37.588864
1836.916784	305560.069491	37.593882
1838.823648	306139.096399	37.598900
1840.477893	306711.431152	37.603917
1842.577065	307277.720526	37.608935
1844.416816	307862.333862	37.613952
1846.494916	308423.920713	37.618970
1848.196284	308991.889384	37.623988
1850.056170	309567.725810	37.629005
1851.865119	310136.201945	37.634023
1853.597436	310701.613877	37.639040
1855.838625	311281.996737	37.644058
1857.772833	311856.382055	37.649076
1859.293836	312428.545817	37.654093
1861.362713	312987.409856	37.659111
1862.807552	313571.182633	37.664128
1865.204481	314145.524895	37.669146
1867.223186	314731.961647	37.674164
1868.835352	315285.398719	37.679181
1870.765414	315857.087475	37.684199
1872.561000	316439.560442	37.689216
1874.301376	317008.833518	37.694234
1876.214361	317572.207789	37.699252
1877.905174	318128.428145	37.704269
1880.018972	318671.649573	37.709287
1881.606448	319228.792139	37.714304
1883.285144	319782.512548	37.719322
1884.986313	320335.082035	37.724340
1886.887730	320893.682340	37.729357
1888.994419	321449.908013	37.734375
1891.002801	322014.117863	37.739392
1892.529069	322580.535184	37.744410
1894.410604	323144.222824	37.749428
1896.267236	323720.883900	37.754445
1898.342405	324282.548942	37.759463
1899.938925	324862.593881	37.764480
1901.622905	325444.929350	37.769498
1903.344793	326020.677210	37.774516
1905.354234	326616.810192	37.779533
1907.514805	327205.168751	37.784551
1909.036701	327804.290081	37.789568
1910.832210	328392.214745	37.794586
1912.979221	328995.206639	37.799604
1914.912521	329596.221925	37.804621
1916.798720	330200.970644	37.809639
1918.887933	330805.171680	37.814656
1920.527233	331407.028796	37.819674
1922.152915	332025.560653	37.824692
1924.553598	332643.424545	37.829709
1926.420517	333257.917148	37.834727
1928.211958	333874.522315	37.839744
1930.441506	334488.661900	37.844762
1932.027919	335119.172505	37.849780
1933.838928	335748.724717	37.854797
1936.175451	336361.708125	37.859815
1938.273485	337002.874815	37.864832
1940.307189	337624.219416	37.869850
1941.811421	338248.867674	37.874868
1943.665780	338881.649295	37.879885
1945.983423	339512.087456	37.884903
1947.831531	340150.438486	37.889920
1949.938460	340795.642617	37.894938
1952.233214	341426.517298	37.899956
1953.949960	342060.398219	37.904973
1956.153877	342693.302132	37.909991
1958.013152	343332.549169	37.915008
1959.904627	343970.614888	37.920026
1962.121465	344603.136218	37.925044
1963.957102	345256.828167	37.930061
1965.949969	345892.211764	37.935079
1967.879681	346537.317398	37.940096
1969.729707	347188.340494	37.945114
1971.842306	347830.098619	37.950132
1973.789736	348478.955510	37.955149
1975.487022	349128.935665	37.960167
1977.800936	349782.382849	37.965184
1979.706369	350429.366014	37.970202
1981.505176	351071.510403	37.975220
1983.178446	351736.454106	37.980237
1985.420638	352384.266519	37.985255
1987.523627	353046.708581	37.990272
1989.864031	353694.561301	37.995290
1992.109384	354351.072722	38.000308
1993.816212	355006.952443	38.005325
1995.827341	355659.802989	38.010343
1997.721228	356319.488239	38.015360
1999.715500	356965.368831	38.020378
2001.680674	357615.354550	38.025396
2003.593259	358276.705520	38.030413
2005.857826	358934.816179	38.035431
2007.576346	359580.777222	38.040448
2009.345812	360222.304927	38.045466
2011.626028	360847.576859	38.050484
2013.142017	361483.722188	38.055501
2015.249405	362124.453104	38.060519
2017.016023	362767.234038	38.065536
2019.163139	363405.578099	38.070554
2020.798299	364060.841017	38.075572
2022.803090	364712.404132	38.080589
2025.001453	365354.614229	38.085607
2026.792923	366020.167973	38.090624
2028.652468	366678.596047	38.095642
2030.651223	367345.385950	38.100660
2032.340718	368022.691217	38.105677
2034.574242	368689.291526	38.110695
2036.606089	369360.250553	38.115712
2038.340329	370048.595897	38.120730
2040.535580	370744.765788	38.125748
2042.456618	371436.757225	38.130765
2044.471706	372124.179852	38.135783
2046.339649	372822.519560	38.140800
2048.487106	373527.697962	38.145818
2050.461848	374219.322324	38.150836
2052.572819	374942.992527	38.155853
2054.495410	375653.744920	38.160871
2056.469435	376366.300226	38.165888
2058.613250	377087.916914	38.170906
2060.565320	377806.304134	38.175924
2062.794778	378543.598636	38.180941
2064.863632	379269.391100	38.185959
2066.829694	379995.311701	38.190976
2068.670713	380730.441775	38.195994
2071.045712	381462.297937	38.201012
2072.934867	382213.006747	38.206029
2074.988033	382946.759455	38.211047
2077.507851	383691.118317	38.216064
2079.413702	384447.528593	38.221082
2081.711196	385182.052565	38.226100
2083.615351	385935.157613	38.231117
2085.957345	386690.555739	38.236135
2088.326726	387439.568109	38.241152
2090.097770	388187.622085	38.246170
2092.377994	388934.636211	38.251188
2094.655556	389691.722120	38.256205
2096.712791	390436.328762	38.261223
2098.744978	391190.351240	38.266240
2100.878543	391953.311619	38.271258
2103.257852	392705.312989	38.276276
2105.152737	393455.854868	38.281293
2107.271078	394207.481746	38.286311
2109.701443	394968.644187	38.291328
2111.672594	395732.524194	38.296346
2114.103149	396486.500505	38.301364
2116.527526	397241.345568	38.306381
2118.680750	397990.488473	38.311399
2121.084270	398736.276327	38.316416
2123.006492	399490.968636	38.321434
2125.440916	400237.954392	38.326452
2127.239839	400977.955680	38.331469
2129.699432	401722.389841	38.336487
2131.424570	402475.414232	38.341504
2133.766287	403220.537940	38.346522
2135.885044	403972.190425	38.351540
2138.131477	404726.259286	38.356557
2139.900296	405464.500762	38.361575
2142.211098	406217.200965	38.366592
2144.045350	406973.607439	38.371610
2146.465627	407718.242608	38.376628
2147.898624	408463.172375	38.381645
2150.575809	409200.783144	38.386663
2152.789966	409930.799891	38.391680
2154.998509	410650.234540	38.396698
2157.193465	411371.247875	38.401716
2159.007314	412101.955256	38.406733
2161.355589	412824.018280	38.411751
2163.490358	413548.325644	38.416768
2165.319271	414275.905427	38.421786
2168.037989	415007.117102	38.426804
2169.759180	415741.511985	38.431821
2171.846327	416484.056426	38.436839
2174.135250	417220.290845	38.441856
2175.683660	417968.554004	38.446874
2178.266432	418715.788770	38.451892
2180.065937	419477.514075	38.456909
2182.284393	420235.981979	38.461927
2184.138897	421002.868336	38.466944
2186.467766	421778.388382	38.471962
2188.530385	422548.585740	38.476980
2190.760113	423328.504588	38.481997
2192.684686	424110.879619	38.487015
2195.303572	424894.583464	38.492032
2197.230854	425687.186354	38.497050
2199.970941	426473.502843	38.502068
2201.937199	427256.377384	38.507085
2203.872888	428056.444903	38.512103
2206.031263	428852.196321	38.517120
2208.202422	429649.083388	38.522138
2210.444797	430452.563462	38.527156
2212.797765	431268.602500	38.532173
2214.904114	432084.097053	38.537191
2217.513704	432893.810932	38.542208
2219.411430	433715.407515	38.547226
2221.876625	434520.482405	38.552244
2224.146188	435354.106583	38.557261
2226.055874	436171.564594	38.562279
2228.537757	436992.694495	38.567296
2229.970888	437816.902956	38.572314
2232.623485	438645.181486	38.577332
2235.214944	439487.203538	38.582349
2236.993628	440323.002949	38.587367
2239.490969	441156.527245	38.592384
2241.728660	442004.179620	38.597402
2243.943431	442843.050278	38.602420
2246.499142	443689.472192	38.607437
2248.732146	444533.992131	38.612455
2251.174036	445377.433042	38.617472
2253.521924	446217.619043	38.622490
2255.879467	447051.245218	38.627508
2258.021235	447901.111857	38.632525
2260.420942	448737.599259	38.637543
2263.032389	449586.259001	38.642560
2264.913321	450429.391217	38.647578
2267.651099	451262.384991	38.652596
2269.801394	452116.379951	38.657613
2272.097281	452961.668320	38.662631
2274.563983	453794.403589	38.667648
2276.729356	454640.858764	38.672666
2279.125552	455476.420199	38.677684
2281.544063	456315.432781	38.682701
2283.730291	457158.696361	38.687719
2286.329156	457991.087898	38.692736
2288.224846	458842.014449	38.697754
2290.517805	459678.431530	38.702772
2293.149082	460517.639442	38.707789
2295.070293	461356.828223	38.712807
2297.769226	462192.567682	38.717824
2300.023742	463029.356185	38.722842
2302.003330	463831.127688	38.727860
2304.120475	464640.121848	38.732877
2306.465194	465449.752611	38.737895
2309.227902	466260.796935	38.742912
2310.907923	467075.776248	38.747930
2313.477363	467877.738994	38.752948
2315.643856	468697.825093	38.757965
2317.743615	469512.733217	38.762983
2320.109198	470332.463881	38.768000
2322.164334	471159.536605	38.773018
2324.246629	471990.155909	38.778036
2326.588036	472826.404757	38.783053
2329.048918	473680.177030	38.788071
2331.196692	474526.536281	38.793088
2333.067881	475390.279440	38.798106
2335.235176	476242.518127	38.803124
2337.850638	477108.634575	38.808141
2340.009484	477976.957479	38.813159
2342.830342	478841.493823	38.818176
2345.221733	479727.270833	38.823194
2347.348999	480590.576282	38.828212
2349.336764	481469.871145	38.833229
2351.698435	482357.191111	38.838247
2354.397026	483235.474718	38.843264
2356.734644	484132.203432	38.848282
2359.232001	485014.774979	38.853300
2361.392889	485904.527005	38.858317
2363.576068	486814.928120	38.863335
2365.913428	487704.711873	38.868352
2368.257508	488627.259124	38.873370
2370.472529	489533.778870	38.878388
2372.795691	490447.703345	38.883405
2374.983281	491373.260275	38.888423
2377.935462	492290.566978	38.893440
2380.233432	493216.662847	38.898458
2382.615271	494146.983982	38.903476
2384.954200	495068.280080	38.908493
2387.079560	496004.798852	38.913511
2389.867307	496936.868138	38.918528
2392.344193	497871.863268	38.923546
2394.698049	498812.577550	38.928564
2396.990817	499756.426972	38.933581
2399.121120	500700.350635	38.938599
2402.108542	501631.469761	38.943616
2404.397276	502592.811790	38.948634
2406.750103	503536.738542	38.953652
2409.297212	504486.428681	38.958669
2411.160679	505430.528684	38.963687
2413.769281	506391.746110	38.968704
2416.255130	507344.002409	38.973722
2418.779980	508301.338645	38.978740
2421.273914	509269.663670	38.983757
2423.884693	510231.307009	38.988775
2426.242940	511185.725681	38.993792
2428.079448	512156.201893	38.998810
2430.996803	513118.930383	39.003828
2433.687755	514087.130886	39.008845
2435.621810	515053.733503	39.013863
2438.263604	516010.937769	39.018880
2440.622115	516986.270167	39.023898
2443.153657	517959.648422	39.028916
2445.696435	518929.033641	39.033933
2447.693794	519905.904044	39.038951
2450.113847	520865.010641	39.043968
2452.747942	521844.876371	39.048986
2455.297975	522829.478056	39.054004
2457.930716	523798.287644	39.059021
2460.169002	524788.152216	39.064039
2462.640396	525724.732516	39.069056
2464.942005	526678.857044	39.074074
2467.317746	527613.824146	39.079092
2469.761209	528567.200154	39.084109
2472.155114	529517.049033	39.089127
2474.770257	530456.076946	39.094144
2477.133902	531424.234041	39.099162
2479.233713	532378.829840	39.104180
2481.788088	533341.341823	39.109197
2483.622007	534312.415010	39.114215
2486.592162	535286.658031	39.119232
2489.119420	536272.030132	39.124250
2491.187800	537243.320607	39.129268
2493.564002	538230.193629	39.134285
2496.121508	539232.465329	39.139303
2498.652579	540236.331081	39.144320
2500.693748	541242.470422	39.149338
2503.052675	542259.854267	39.154356
2505.738564	543265.491431	39.159373
2508.053211	544300.239141	39.164391
2510.392808	545323.489773	39.169408
2512.756243	546361.546681	39.174426
2515.359299	547404.263418	39.179444
2517.885092	548446.059431	39.184461
2520.268881	549502.581492	39.189479
2523.053361	550563.983370	39.194496
2525.228196	551625.956304	39.199514
2527.972126	552691.472122	39.204532
2530.574465	553757.480419	39.209549
2532.875128	554835.867909	39.214567
2535.535356	555908.280260	39.219584
2538.437522	556987.903282	39.224602
2540.707684	558069.653553	39.229620
2543.705780	559142.453809	39.234637
2545.774695	560227.327135	39.239655
2548.879736	561313.397144	39.244672
2551.448731	562402.429366	39.249690
2553.815819	563497.280638	39.254708
2556.748863	564579.542289	39.259725
2559.475649	565687.508739	39.264743
2562.023724	566766.789161	39.269760
2564.494517	567860.853531	39.274778
2567.085978	568951.842903	39.279796
2569.949645	570042.493654	39.284813
2572.881933	571138.962851	39.289831
2575.125017	572232.791082	39.294848
2577.875131	573329.703329	39.299866
2580.075100	574430.675706	39.304884
2582.978767	575525.514697	39.309901
2585.904569	576628.884091	39.314919
2588.474528	577728.853359	39.319936
2590.804548	578815.220634	39.324954
2593.124161	579921.156965	39.329972
2596.014992	581019.226292	39.334989
2598.361707	582133.034641	39.340007
2601.025320	583233.150089	39.345024
2603.717022	584343.139972	39.350042
2606.045940	585462.113089	39.355060
2608.729926	586576.512744	39.360077
2611.320404	587696.389192	39.365095
2614.056629	588804.909875	39.370112
2616.545755	589935.420915	39.375130
2619.165119	591064.951607	39.380148
2621.961836	592181.117188	39.385165
2624.564410	593304.825609	39.390183
2627.090255	594415.213668	39.395200
2629.561551	595540.584540	39.400218
2632.410475	596659.223492	39.405236
2635.223659	597751.717148	39.410253
2637.223470	598833.625531	39.415271
2639.940368	599917.868764	39.420288
2642.908565	600999.615672	39.425306
2645.606465	602083.008002	39.430324
2648.139352	603160.067782	39.435341
2650.812941	604268.639094	39.440359
2652.881405	605360.585371	39.445376
2655.808176	606450.133329	39.450394
2658.415832	607557.544453	39.455412
2660.933478	608659.407888	39.460429
2663.698167	609774.831755	39.465447
2666.221445	610876.277000	39.470464
2668.796640	612001.766212	39.475482
2671.283273	613128.907091	39.480500
2673.971066	614258.251101	39.485517
2676.788485	615390.058992	39.490535
2679.398803	616522.185036	39.495552
2681.960400	617663.202093	39.500570
2684.393022	618814.719950	39.505588
2687.511826	619974.900888	39.510605
2689.940357	621129.224286	39.515623
2692.094263	622289.167452	39.520640
2695.232790	623460.466936	39.525658
2697.747857	624636.188824	39.530676
2700.523440	625811.639144	39.535693
2702.997623	626999.048972	39.540711
2705.644281	628198.785243	39.545728
2708.725303	629387.526876	39.550746
2710.991940	630594.845952	39.555764
2713.588813	631794.233161	39.560781
2716.265619	633011.094129	39.565799
2719.024418	634217.666628	39.570816
2721.885745	635438.308298	39.575834
2724.385076	636661.461740	39.580852
2727.430240	637884.830056	39.585869
2730.124579	639116.643664	39.590887
2732.989055	640353.520362	39.595904
2736.168676	641576.727319	39.600922
2738.712798	642810.666460	39.605940
2741.560522	644043.558331	39.610957
2744.427610	645274.950971	39.615975
2747.213860	646512.140465	39.620992
2750.622418	647741.198678	39.626010
2753.475896	648972.939755	39.631028
2755.962661	650201.898405	39.636045
2758.863614	651430.039446	39.641063
2761.615548	652670.261621	39.646080
2764.823812	653894.359861	39.651098
2767.398375	655123.691536	39.656116
2770.221437	656359.304159	39.661133
2773.362015	657593.662967	39.666151
2775.763370	658818.028279	39.671168
2779.066824	660048.862752	39.676186
2781.487274	661280.981312	39.681204
2784.036685	662509.238183	39.686221
2786.667755	663741.058237	39.691239
2789.800903	664980.351535	39.696256
2792.882768	666214.716111	39.701274
2795.662341	667452.404046	39.706292
2798.570889	668677.970556	39.711309
2801.178095	669912.531036	39.716327
2803.942402	671154.663021	39.721344
2806.694088	672378.532624	39.726362
2809.319152	673624.936526	39.731380
2812.359241	674853.904957	39.736397
2815.071234	676088.879778	39.741415
2817.509098	677322.393979	39.746432
2821.111213	678517.883543	39.751450
2823.638107	679725.917278	39.756468
2826.244510	680917.434240	39.761485
2829.086908	682104.137955	39.766503
2831.687079	683302.847105	39.771520
2834.524329	684508.908495	39.776538
2836.851962	685715.142393	39.781556
2839.727046	686923.310253	39.786573
2842.507562	688136.743373	39.791591
2845.146026	689365.374093	39.796608
2848.174540	690593.127388	39.801626
2850.911338	691822.943922	39.806644
2853.302640	693065.349612	39.811661
2856.370671	694310.645302	39.816679
2858.928679	695578.220526	39.821696
2861.502008	696830.138242	39.826714
2864.446642	698091.784024	39.831732
2867.310227	699357.674698	39.836749
2870.318195	700640.461262	39.841767
2872.933667	701923.718907	39.846784
2875.744108	703202.096795	39.851802
2878.417485	704495.867879	39.856820
2880.814901	705801.331784	39.861837
2883.880809	707124.469240	39.866855
2886.422557	708446.845507	39.871872
2889.885199	709767.875365	39.876890
2893.136784	711100.668090	39.881908
2895.502003	712425.031845	39.886925
2898.404391	713750.189163	39.891943
2901.521881	715112.121186	39.896960
2904.683725	716439.287828	39.901978
2907.124858	717791.248625	39.906996
2910.416919	719156.799947	39.912013
2913.431187	720499.423175	39.917031
2916.181852	721856.213296	39.922048
2919.465241	723217.093676	39.927066
2922.252739	724570.910936	39.932084
2925.590328	725925.601037	39.937101
2928.736796	727291.810670	39.942119
2931.425292	728653.865469	39.947136
2934.428444	730008.625976	39.952154
2937.293208	731378.939345	39.957172
2940.079724	732752.441166	39.962189
2943.476458	734132.126124	39.967207
2946.029732	735504.851542	39.972224
2949.186318	736865.495274	39.977242
2951.937801	738247.687932	39.982260
2954.821583	739623.796712	39.987277
2958.097689	741012.922038	39.992295
2961.036711	742403.190808	39.997312
2964.002782	743797.747037	40.002330
2966.703805	745185.788393	40.007348
2969.595665	746584.496449	40.012365
2972.702266	747973.750941	40.017383
2975.581263	749373.981529	40.022400
2978.697020	750765.199467	40.027418
2981.783844	752171.787953	40.032436
2984.465003	753575.625508	40.037453
2987.841401	754974.069100	40.042471
2990.147912	756387.696519	40.047488
2993.508522	757782.527217	40.052506
2996.479313	759198.821834	40.057524
2998.973342	760620.097357	40.062541
3002.192418	762023.078024	40.067559
3005.102956	763447.491501	40.072576
3007.963557	764870.659488	40.077594
3011.206781	766302.098656	40.082612
3014.074894	767708.105540	40.087629
3017.129926	769098.480517	40.092647
3020.031699	770468.176722	40.097664
3023.145420	771843.480198	40.102682
3026.101816	773227.493522	40.107700
3028.781971	774612.519491	40.112717
3031.925793	775978.645106	40.117735
3034.815586	777382.655789	40.122752
3038.081229	778764.833564	40.127770
3041.085214	780160.042064	40.132788
3043.501921	781565.922240	40.137805
3046.818343	782971.968680	40.142823
3049.772674	784395.947736	40.147840
3052.746775	785804.389372	40.152858
3056.001337	787233.687651	40.157876
3058.509415	788668.067069	40.162893
3061.785949	790092.277045	40.167911
3064.602415	791541.069849	40.172928
3067.870846	792984.640554	40.177946
3070.820211	794446.873351	40.182964
3073.564184	795900.510131	40.187981
3077.055078	797360.477571	40.192999
3079.777247	798824.621942	40.198016
3082.917156	800300.672018	40.203034
3085.714038	801779.937523	40.208052
3089.053815	803282.129574	40.213069
3092.388573	804763.453488	40.218087
3095.434769	806275.357750	40.223104
3098.591998	807771.656927	40.228122
3101.624880	809275.369726	40.233140
3104.516049	810793.284905	40.238157
3108.001431	812297.131697	40.243175
3110.990876	813829.638582	40.248192
3114.213248	815342.030216	40.253210
3117.260057	816864.946983	40.258228
3120.275008	818395.281937	40.263245
3123.689406	819932.908855	40.268263
3126.655876	821473.863113	40.273280
3129.534975	823002.913154	40.278298
3132.921632	824547.860016	40.283316
3135.928787	826086.412057	40.288333
3139.329208	827634.529153	40.293351
3142.402458	829191.591008	40.298368
3145.505285	830742.672788	40.303386
3148.928317	832298.590626	40.308404
3151.619947	833858.831313	40.313421
3155.065003	835416.135733	40.318439
3158.335676	836982.776056	40.323456
3161.776148	838550.902298	40.328474
3164.770888	840104.220118	40.333492
3168.030833	841676.470480	40.338509
3171.180606	843240.763888	40.343527
3174.462495	844807.370037	40.348544
3177.654649	846381.570821	40.353562
3181.171583	847942.399550	40.358580
3184.214493	849520.791328	40.363597
3187.751351	851090.446764	40.368615
3190.781424	852658.623921	40.373632
3194.093374	854224.124842	40.378650
3197.585603	855779.203198	40.383668
3200.288674	857358.079850	40.388685
3203.819953	858922.931042	40.393703
3206.962813	860492.682090	40.398720
3210.317028	862050.166411	40.403738
3213.403157	863617.956917	40.408756
3216.341012	865197.381059	40.413773
3219.739951	866766.919395	40.418791
3223.149955	868340.017075	40.423808
3226.165108	869892.531657	40.428826
3229.368982	871425.446404	40.433844
3232.611961	872943.831822	40.438861
3235.825262	874463.382001	40.443879
3238.922801	875984.012220	40.448896
3242.086824	877506.560599	40.453914
3245.456592	879033.224831	40.458932
3248.337084	880556.963084	40.463949
3251.522096	882092.042099	40.468967
3254.225014	883637.035661	40.473984
3257.149516	885187.859263	40.479002
3260.550079	886749.581678	40.484020
3263.719534	888324.046442	40.489037
3266.571286	889895.624496	40.494055
3269.639237	891484.486270	40.499072
3273.003973	893078.258653	40.504090
3275.892937	894677.159688	40.509108
3278.972544	896298.229869	40.514125
3282.169282	897912.554265	40.519143
3285.045840	899551.130155	40.524160
3287.907489	901187.017124	40.529178
3291.159947	902846.238368	40.534196
3294.408449	904512.571580	40.539213
3297.974435	906179.894241	40.544231
3300.903363	907868.367190	40.549248
3304.277022	909553.560241	40.554266
3307.531134	911245.179964	40.559284
3310.586316	912956.685004	40.564301
3314.068591	914663.359098	40.569319
3317.112865	916387.435368	40.574336
3320.378410	918113.426093	40.579354
3323.750142	919832.708721	40.584372
3326.586439	921576.287085	40.589389
3329.761437	923319.725979	40.594407
3333.219280	925082.879898	40.599424
3336.536234	926847.969184	40.604442
3339.808944	928614.782209	40.609460
3343.325891	930397.635312	40.614477
3346.554574	932172.180873	40.619495
3349.842614	933965.073833	40.624512
3353.137230	935747.499891	40.629530
3356.819129	937538.057495	40.634548
3359.838874	939339.873150	40.639565
3363.482288	941151.287272	40.644583
3366.857875	942952.367536	40.649600
3370.097462	944764.211146	40.654618
3373.434852	946571.678655	40.659636
3376.743549	948391.497748	40.664653
3380.531098	950209.160645	40.669671
3383.578553	952025.058711	40.674688
3386.941765	953879.050462	40.679706
3390.412305	955762.802970	40.684724
3393.506328	957633.682646	40.689741
3396.781150	959515.850686	40.694759
3400.242445	961395.516613	40.699776
3403.480439	963295.021230	40.704794
3406.906870	965180.587117	40.709812
3410.249445	967092.685958	40.714829
3413.805005	968986.254855	40.719847
3417.186584	970890.738676	40.724864
3420.500794	972802.304950	40.729882
3424.355529	974698.325927	40.734900
3427.440544	976616.942416	40.739917
3431.061527	978516.511212	40.744935
3434.487581	980420.252512	40.749952
3437.640181	982336.644495	40.754970
3441.100742	984240.565297	40.759988
3444.206093	986156.167201	40.765005
3447.874529	988050.468724	40.770010
3451.214945	989892.151694	40.775015
3454.284255	991700.345559	40.780020
3457.594223	993422.782140	40.785024
3460.868388	995083.931571	40.790029
3464.056984	996664.091089	40.795034
3467.124154	998173.456777	40.800039
3469.687529	999623.046617	40.805044
3472.539111	1000972.012628	40.810048
3475.337836	1002254.428276	40.815053
3478.357994	1003467.473357	40.820058
3481.060916	1004601.753076	40.825063
3483.572445	1005651.558860	40.830068
3486.043175	1006622.063995	40.835072
3488.059357	1007540.391895	40.840077
3490.133730	1008380.736347	40.845082
3492.193108	1009174.230951	40.850087
3494.303252	1009878.437397	40.855092
3496.192628	1010536.070703	40.860096
3497.722330	1011132.700398	40.865101
3499.370987	1011678.559910	40.870106
3500.976789	1012175.632529	40.875111
3502.431506	1012615.308334	40.880116
3504.272690	1012997.026835	40.885120
3505.337122	1013349.822394	40.890125
3506.492230	1013646.960872	40.895130
3507.752055	1013897.572821	40.900135
3508.981783	1014120.904651	40.905140
3510.108610	1014288.339742	40.910144
3511.202213	1014442.381765	40.915149
3511.994565	1014546.195969	40.920154
3513.281876	1014633.622093	40.925159
3513.911977	1014684.178967	40.930164
3514.663905	1014684.831546	40.935168
3515.424427	1014685.870911	40.940173
3516.015721	1014649.767680	40.945178
3516.804938	1014584.127793	40.950183
3517.369478	1014507.168890	40.955188
3518.038815	1014394.669447	40.960192
3518.732394	1014264.402210	40.965197
3519.019193	1014112.360412	40.970202
3519.956301	1013956.033662	40.975207
3520.354341	1013778.630983	40.980212
3520.544232	1013571.068374	40.985216
3520.949875	1013358.608892	40.990221
3521.278102	1013133.339943	40.995226
3521.873563	1012883.359263	41.000231
3522.155722	1012637.011269	41.005236
3522.541018	1012362.867642	41.010240
3522.848148	1012088.820630	41.015245
3523.385733	1011794.137048	41.020250
3523.533319	1011488.529347	41.025255
3523.461865	1011184.300686	41.030260
3523.832652	1010861.530610	41.035264
3524.031669	1010532.263140	41.040269
3524.677613	1010194.355526	41.045274
3524.654704	1009848.281437	41.050279
3524.713958	1009498.675502	41.055284
3525.049770	1009131.807421	41.060288
3524.813653	1008775.987912	41.065293
3525.276391	1008404.776869	41.070298
3525.241435	1008038.384464	41.075303
3525.041998	1007653.144018	41.080308
3525.342990	1007277.901356	41.085312
3525.709608	1006893.779087	41.090317
3525.880594	1006498.777415	41.095322
3526.231606	1006104.301613	41.100327
3525.797528	1005692.430567	41.105332
3525.822765	1005281.911967	41.110336
3525.942696	1004876.986647	41.115341
3525.984047	1004458.725148	41.120346
3526.294334	1004050.111759	41.125351
3526.134280	1003640.184910	41.130356
3525.997854	1003215.053685	41.135360
3526.052573	1002807.267703	41.140365
3525.988962	1002376.420548	41.145370
3526.327151	1001953.645036	41.150375
3525.836069	1001527.472528	41.155380
3526.061628	1001097.842139	41.160384
3526.154966	1000677.638219	41.165389
3526.179429	1000241.165424	41.170394
3526.208262	999815.070068	41.175399
3526.191300	999391.674957	41.180404
3526.344656	998952.454014	41.185408
3526.325452	998516.439276	41.190413
3526.413185	998067.135529	41.195418
3526.090529	997628.668975	41.200423
3526.423938	997203.981702	41.205428
3526.429390	996761.013087	41.210432
3526.194127	996317.952121	41.215437
3525.751172	995872.164227	41.220442
3526.342420	995426.852563	41.225447
3526.278339	994993.787613	41.230452
3526.162563	994537.712320	41.235456
3526.198784	994101.738184	41.240461
3526.059922	993649.588875	41.245466
3525.825583	993206.771621	41.250471
3526.008066	992767.553401	41.255476
3525.881756	992312.080313	41.260480
3525.747868	991885.415152	41.265485
3525.694534	991434.439449	41.270490
3526.048404	990989.208361	41.275495
3525.867609	990551.242948	41.280500
3526.121691	990101.280348	41.285504
3526.027721	989651.729385	41.290509
3525.701053	989203.351065	41.295514
3525.709591	988751.469761	41.300519
3525.664014	988309.994441	41.305524
3525.941346	987860.435665	41.310528
3525.542523	987414.170907	41.315533
3525.590843	986963.798848	41.320538
3525.653372	986516.412395	41.325543
3525.426071	986076.354231	41.330548
3525.451300	985623.051147	41.335552
3525.333003	985181.930386	41.340557
3525.317717	984741.636575	41.345562
3525.273078	984285.018836	41.350567
3524.762003	983847.372062	41.355572
3525.023430	983404.587398	41.360576
3524.675429	982965.674982	41.365581
3524.930723	982534.144846	41.370586
3524.937625	982093.252339	41.375591
3524.617422	981655.698662	41.380596
3524.693047	981214.629301	41.385600
3524.756491	980784.169892	41.390605
3524.601079	980342.094819	41.395610
3524.835156	979899.237801	41.400615
3524.549917	979470.494436	41.405620
3524.443125	979030.262881	41.410624
3524.313454	978594.298675	41.415629
3524.110495	978159.876119	41.420634
3524.352142	977722.221345	41.425639
3523.773971	977291.799709	41.430644
3523.943465	976860.831679	41.435648
3524.079464	976435.503730	41.440653
3524.181160	976010.833805	41.445658
3524.086549	975572.092680	41.450663
3524.088022	975155.779906	41.455668
3524.099675	974708.354834	41.460672
3523.756970	974279.426894	41.465677
3523.542140	973848.295198	41.470682
3523.784996	973431.035180	41.475687
3523.993456	973000.845292	41.480692
3523.557925	972566.133823	41.485696
3523.292466	972138.499356	41.490701
3523.188177	971723.910036	41.495706
3523.347562	971298.783190	41.500711
3523.044467	970878.493329	41.505716
3522.865463	970451.598954	41.510720
3522.813936	970044.997710	41.515725
3522.388070	969632.266411	41.520730
3522.749140	969225.147783	41.525735
3522.625761	968817.590894	41.530740
3522.427314	968405.125188	41.535744
3522.563588	967999.326461	41.540749
3522.211463	967588.295146	41.545754
3522.899716	967174.420636	41.550759
3522.285517	966763.667058	41.555764
3522.456598	966351.873809	41.560768
3522.473431	965952.508056	41.565773
3522.275022	965544.241707	41.570778
3522.288925	965133.953366	41.575783
3521.782003	964732.924831	41.580788
3521.947295	964325.980636	41.585792
3522.055052	963926.459125	41.590797
3521.597725	963526.121604	41.595802
3521.964431	963121.898943	41.600807
3521.745120	962735.178004	41.605812
3521.828261	962322.620902	41.610816
3521.363982	961927.266565	41.615821
3521.439662	961528.955222	41.620826
3521.862108	961137.025122	41.625831
3521.367899	960744.533540	41.630836
3521.552409	960338.871792	41.635840
3521.575395	959948.494347	41.640845
3521.315089	959561.468963	41.645850
3521.361577	959150.846548	41.650855
3521.106940	958771.901382	41.655860
3521.313807	958368.645485	41.660864
3520.981883	957981.623823	41.665869
3520.822634	957590.528557	41.670874
3520.862920	957201.726748	41.675879
3520.840961	956817.026752	41.680884
3520.682953	956432.225472	41.685888
3520.567700	956052.588400	41.690893
3520.597290	955670.843206	41.695898
3520.719881	955278.269973	41.700903
3520.557584	954896.701343	41.705908
3520.789048	954513.375253	41.710912
3520.400671	954129.537316	41.715917
3520.174589	953752.121338	41.720922
3520.228553	953366.786533	41.725927
3520.328955	952994.760930	41.730932
3520.097944	952608.147106	41.735936
3520.037964	952253.609131	41.740941
3519.782326	951894.178852	41.745946
3520.001842	951519.151233	41.750951
3519.996787	951160.488675	41.755956
3519.778772	950798.966368	41.760960
3519.759555	950437.577019	41.765965
3519.477618	950080.414737	41.770970
3519.405249	949722.427574	41.775975
3519.291232	949375.903869	41.780980
3519.384476	949008.845529	41.785984
3519.349351	948658.815549	41.790989
3519.327852	948315.267030	41.795994
3519.319231	947951.882074	41.800999
3519.001973	947600.199291	41.806004
3519.118646	947249.282410	41.811008
3518.974517	946907.861454	41.816013
3518.997918	946563.613975	41.821018
3519.000748	946213.602497	41.826023
3518.673339	945869.462120	41.831028
3519.099356	945522.110560	41.836032
3519.264598	945180.619839	41.841037
3518.856035	944832.305971	41.846042
3518.723979	944473.579715	41.851047
3518.413400	944134.013575	41.856052
3518.683722	943791.168543	41.861056
3518.343262	943450.796177	41.866061
3518.482153	943127.661657	41.871066
3518.439421	942772.826166	41.876071
3518.098806	942444.458854	41.881076
3518.062329	942104.331165	41.886080
3517.966029	941772.814986	41.891085
3517.610369	941443.716058	41.896090
3518.108314	941109.280630	41.901095
3517.952241	940786.623908	41.906100
3517.701044	940455.145028	41.911104
3517.653402	940129.650172	41.916109
3517.539843	939799.448798	41.921114
3517.770945	939473.867056	41.926119
3517.720192	939152.433830	41.931124
3517.791693	938824.536987	41.936128
3517.684001	938509.305467	41.941133
3517.448277	938181.514752	41.946138
3517.891537	937846.591381	41.951143
3516.943213	937522.616611	41.956148
3517.334055	937205.018641	41.961152
3517.198982	936880.294705	41.966157
3516.951868	936569.764866	41.971162
3517.185051	936248.873756	41.976167
3516.684585	935941.801706	41.981172
3516.611099	935619.195907	41.986176
3516.731752	935308.338976	41.991181
3516.685902	935004.974868	41.996186
3516.950180	934689.260395	42.001191
3516.849433	934384.430284	42.006196
3516.729154	934066.054999	42.011200
3516.494543	933757.180199	42.016205
3516.142528	933458.863784	42.021210
3516.448597	933139.306583	42.026215
3516.384404	932846.091012	42.031220
3516.141126	932538.586080	42.036224
3516.170112	932235.242230	42.041229
3516.202514	931951.560719	42.046234
3516.046978	931642.165173	42.051239
3516.004283	931344.158430	42.056244
3516.183618	931038.512939	42.061248
3516.099263	930743.167760	42.066253
3515.932709	930450.796557	42.071258
3515.789711	930148.225771	42.076263
3515.646551	929853.416955	42.081268
3515.590742	929558.289252	42.086272
3515.415431	929275.267130	42.091277
3514.993644	928988.236245	42.096282
3515.217335	928703.292913	42.101287
3515.018977	928426.761532	42.106292
3515.174090	928136.899878	42.111296
3515.276075	927857.599512	42.116301
3515.185005	927571.782857	42.121306
3515.327598	927278.994229	42.126311
3514.882605	927009.155956	42.131316
3515.091153	926728.529773	42.136320
3515.059623	926446.294699	42.141325
3514.735116	926173.319141	42.146330
3514.864196	925882.378340	42.151335
3514.639241	925612.817776	42.156340
3514.881133	925341.148201	42.161344
3514.959056	925055.169165	42.166349
3514.916443	924788.420860	42.171354
3514.812820	924505.614734	42.176359
3514.541778	924224.840240	42.181364
3514.467586	923955.940669	42.186368
3514.600956	923676.801519	42.191373
3514.369629	923415.592823	42.196378
3514.552465	923140.263875	42.201383
3514.523923	922878.995719	42.206388
3514.479181	922596.848781	42.211392
3514.258288	922322.121532	42.216397
3513.936459	922066.344225	42.221402
3514.047264	921798.845270	42.226407
3513.958889	921537.714317	42.231412
3514.125619	921268.159891	42.236416
3513.909340	921018.471893	42.241421
3514.142000	920758.500950	42.246426
3513.757828	920488.036346	42.251431
3513.391115	920234.584840	42.256436
3513.667968	919975.627323	42.261440
3513.809316	919714.466669	42.266445
3513.413641	919469.932678	42.271450
3513.489214	919210.394396	42.276455
3513.096026	918970.264025	42.281460
3513.262784	918708.184603	42.286464
3513.564053	918469.746212	42.291469
3513.333447	918222.818967	42.296474
3513.375155	917963.611642	42.301479
3513.102423	917720.711102	42.306484
3512.944375	917466.133269	42.311488
3513.279475	917221.858925	42.316493
3513.110714	916986.128339	42.321498
3512.976917	916738.925233	42.326503
3512.739736	916498.371124	42.331508
3512.525289	916255.395596	42.336512
3512.776412	916013.199119	42.341517
3512.401000	915782.746284	42.346522
3512.722657	915541.191280	42.351527
3512.445718	915313.494963	42.356532
3512.519554	915067.048582	42.361536
3512.678906	914837.430793	42.366541
3512.355941	914610.194295	42.371546
3512.606765	914369.754942	42.376551
3512.356364	914134.203588	42.381556
3512.052724	913903.178084	42.386560
3512.294706	913675.809726	42.391565
3511.937116	913445.159110	42.396570
3512.313687	913214.185166	42.401575
3511.897185	912993.062472	42.406580
3511.967557	912758.073513	42.411584
3512.130647	912540.112774	42.416589
3511.883954	912312.672102	42.421594
3511.881454	912084.507297	42.426599
3511.965076	911870.290956	42.431604
3511.839175	911646.753566	42.436608
3511.990314	911422.390516	42.441613
3511.874981	911199.507792	42.446618
3512.054991	910978.784016	42.451623
3511.743141	910757.265023	42.456628
3511.771108	910529.994562	42.461632
3511.963658	910310.205782	42.466637
3512.074179	910086.276973	42.471642
3511.703348	909861.647228	42.476647
3511.523397	909652.689806	42.481652
3511.603553	909433.270229	42.486656
3511.851799	909216.995640	42.491661
3511.538233	908989.910872	42.496666
3511.675841	908771.998148	42.501671
3511.413601	908556.360315	42.506676
3511.448910	908335.940431	42.511680
3511.497329	908122.452203	42.516685
3511.157622	907917.987535	42.521690
3511.197704	907698.505792	42.526695
3511.019181	907500.460117	42.531700
3511.121419	907275.358126	42.536704
3510.953321	907078.838716	42.541709
3510.760664	906870.839273	42.546714
3511.147445	906667.848433	42.551719
3510.971279	906465.907461	42.556724
3510.938239	906252.650089	42.561728
3510.885460	906050.673708	42.566733
3510.961969	905856.385829	42.571738
3510.967709	905647.439754	42.576743
3510.644667	905436.031748	42.581748
3510.335008	905233.103309	42.586752
3510.724157	905036.323444	42.591757
3510.383061	904841.490096	42.596762
3510.839681	904644.106389	42.601767
3510.641756	904451.937428	42.606772
3510.505411	904249.137602	42.611776
3510.312267	904047.111730	42.616781
3510.214634	903857.221662	42.621786
3510.288592	903663.533294	42.626791
3510.104986	903477.118546	42.631796
3510.014101	903283.540676	42.636800
3510.210922	903087.013350	42.641805
3509.995149	902906.858171	42.646810
3510.044208	902718.546029	42.651815
3510.046368	902533.323972	42.656820
3509.835744	902340.794964	42.661824
3509.853002	902158.839884	42.666829
3509.961162	901975.415957	42.671834
3510.029541	901786.586664	42.676839
3509.735310	901589.701589	42.681844
3509.377962	901410.680088	42.686848
3509.479599	901220.474697	42.691853
3509.628721	901045.895698	42.696858
3509.881035	900858.742747	42.701863
3509.799715	900694.135464	42.706868
3509.546742	900498.460528	42.711872
3509.669316	900309.862338	42.716877
3509.465302	900130.195421	42.721882
3509.540592	899963.899400	42.726887
3509.461292	899788.063643	42.731892
3509.371889	899602.373738	42.736896
3509.574200	899437.393255	42.741901
3509.489475	899259.320673	42.746906
3509.188217	899069.495269	42.751911
3509.235240	898913.024151	42.756916
3509.270429	898737.233338	42.761920
3509.340389	898567.902830	42.766925
3508.915625	898400.194228	42.771930
3509.120776	898223.393492	42.776935
3509.285086	898062.725883	42.781940
3508.968371	897875.084618	42.786945
3509.211973	897709.950253	42.791949
3509.171279	897548.818796	42.796954
3509.321805	897371.130952	42.801959
3509.088405	897203.645147	42.806964
3508.797576	897038.869088	42.811969
3509.067688	896865.589999	42.816973
3508.731112	896709.024460	42.821978
3508.916743	896533.043725	42.826983
3508.634684	896374.913982	42.831988
3508.761000	896211.687800	42.836993
3509.145050	896044.839055	42.841997
3508.773859	895886.807021	42.847002
3508.814856	895718.555673	42.852007
3508.618819	895550.338392	42.857012
3508.728310	895398.881812	42.862017
3508.677741	895240.295740	42.867021
3508.241158	895073.843611	42.872026
3508.676850	894907.822811	42.877031
3508.627044	894758.211795	42.882036
3508.383981	894587.074113	42.887041
3508.366065	894433.583007	42.892045
3508.017812	894284.588666	42.897050
3508.532353	894125.878425	42.902055
3508.060244	893972.739720	42.907060
3508.306395	893823.345381	42.912065
3508.211452	893674.486688	42.917069
3507.969386	893527.001802	42.922074
3508.239205	893368.214115	42.927079
3508.313603	893226.470006	42.932084
3507.893452	893066.820799	42.937089
3508.245670	892917.481949	42.942093
3507.844786	892776.675144	42.947098
3507.992213	892624.268345	42.952103
3507.985344	892483.776167	42.957108
3508.066406	892335.530405	42.962113
3507.809137	892185.595972	42.967117
3507.981207	892040.615306	42.972122
3507.963930	891888.119319	42.977127
3507.511870	891748.069221	42.982132
3507.763969	891608.286514	42.987137
3507.921449	891456.330478	42.992141
3507.786234	891321.440102	42.997146
3507.863321	891160.591886	43.002151
3508.079462	891026.603837	43.007156
3508.069926	890871.855002	43.012161
3507.626218	890735.163961	43.017165
3507.749375	890587.833238	43.022170
3507.907109	890443.007953	43.027175
3507.323595	890310.005453	43.032180
3507.670133	890166.979963	43.037185
3507.712898	890029.708301	43.042189
3507.291181	889895.315247	43.047194
3507.552773	889752.583647	43.052199
3507.402420	889624.621074	43.057204
3507.154080	889481.096070	43.062209
3507.405016	889342.419278	43.067213
3507.306438	889227.500043	43.072218
3507.559858	889078.851434	43.077223
3507.243932	888952.449187	43.082228
3507.077748	888815.473211	43.087233
3507.462701	888675.016670	43.092237
3506.968760	888548.441361	43.097242
3507.117715	888399.598906	43.102247
3507.065446	888275.944461	43.107252
3506.813919	888157.835855	43.112257
3506.934250	888027.857857	43.117261
3506.844181	887909.524026	43.122266
3507.210961	887778.628879	43.127271
3507.094991	887660.003879	43.132276
3506.844324	887525.236958	43.137281
3506.832862	887400.202137	43.142285
3507.043774	887281.321942	43.147290
3506.670905	887145.792046	43.152295
3506.675139	887024.424255	43.157300
3506.625758	886900.643071	43.162305
3506.587579	886780.148220	43.167309
3506.808836	886661.931101	43.172314
3507.191754	886537.296587	43.177319
3506.737797	886419.088953	43.182324
3506.590341	886290.664697	43.187329
3506.355690	886164.962339	43.192333
3506.422364	886057.793464	43.197338
3506.500086	885930.292123	43.202343
3506.464972	885811.035023	43.207348
3506.503493	885702.412129	43.212353
3506.306755	885588.211037	43.217357
3506.423289	885474.440135	43.222362
3506.555345	885349.240516	43.227367
3506.631128	885244.281792	43.232372
3506.278543	885118.866598	43.237377
3506.393246	884996.760367	43.242381
3506.040817	884889.735756	43.247386
3506.372019	884778.433171	43.252391
3505.976881	884675.671837	43.257396
3506.306464	884561.266979	43.262401
3506.137812	884443.068828	43.267405
3506.157274	884338.490310	43.272410
3506.293434	884227.983950	43.277415
3505.999863	884114.447612	43.282420
3506.385185	884000.216193	43.287425
3505.963690	883890.666812	43.292429
3505.613104	883793.595925	43.297434
3505.763458	883679.881118	43.302439
3506.034836	883572.632613	43.307444
3506.060115	883471.330185	43.312449
3506.200703	883360.322385	43.317453
3505.853702	883260.433465	43.322458
3505.795787	883146.645704	43.327463
3505.837225	883039.812665	43.332468
3506.154700	882935.256668	43.337473
3506.039428	882822.440555	43.342477
3505.912587	882721.924990	43.347482
3506.027419	882625.435931	43.352487
3505.814489	882522.703369	43.357492
3505.887159	882415.272573	43.362497
3506.061393	882313.731747	43.367501
3505.558733	882208.232330	43.372506
3505.511681	882091.709947	43.377511
3505.440244	881992.528819	43.382516
3505.444077	881895.949109	43.387521
3505.579590	881800.799188	43.392525
3505.299843	881721.215901	43.397530
3505.492976	881619.466136	43.402535
3505.373240	881526.485050	43.407540
3505.398758	881427.762737	43.412545
3505.647051	881324.448694	43.417549
3505.569789	881232.134085	43.422554
3505.317713	881129.577205	43.427559
3505.361372	881038.983522	43.432564
3505.357781	880937.641836	43.437569
3505.515644	880844.894830	43.442573
3505.486819	880765.450956	43.447578
3505.605192	880658.367869	43.452583
3505.279649	880559.301165	43.457588
3505.415199	880464.420165	43.462593
3505.795911	880370.563091	43.467597
3505.664981	880278.532961	43.472602
3505.600490	880168.176525	43.477607
3505.588788	880076.511173	43.482612
3505.641257	879977.469242	43.487617
3505.615230	879882.024016	43.492621
3505.085278	879776.388268	43.497626
3505.295493	879688.944138	43.502631
3505.564305	879592.767276	43.507636
3505.290908	879499.973116	43.512641
3505.508630	879406.708927	43.517645
3505.232754	879308.194344	43.522650
3505.621358	879206.951926	43.527655
3505.727739	879117.384255	43.532660
3505.129239	879023.473117	43.537665
3505.197048	878935.168954	43.542669
3505.311946	878847.727994	43.547674
3505.343828	878759.620953	43.552679
3505.721891	878661.278540	43.557684
3505.782931	878572.776198	43.562689
3505.626473	878464.535220	43.567693
3505.338437	878373.664206	43.572698
3505.382487	878279.538374	43.577703
3505.446345	878177.944010	43.582708
3505.307619	878095.767975	43.587713
3505.141867	878010.105593	43.592717
3505.034773	877912.024451	43.597722
3505.074281	877809.749185	43.602727
3505.233911	877732.947457	43.607732
3504.701239	877649.085175	43.612737
3505.177617	877551.095771	43.617741
3504.914635	877466.701745	43.622746
3505.042913	877375.649775	43.627751
3504.935044	877285.604772	43.632756
3505.067689	877207.540331	43.637761
3505.085050	877119.217216	43.642765
3504.813212	877038.114787	43.647770
3504.747228	876953.874857	43.652775
3504.961140	876869.975423	43.657780
3504.926154	876789.412270	43.662785
3505.138420	876707.352938	43.667789
3504.776672	876622.963095	43.672794
3504.998994	876535.470086	43.677799
3504.953764	876445.595848	43.682804
3504.757720	876364.665586	43.687809
3505.035493	876277.450503	43.692813
3504.437862	876206.086623	43.697818
3504.618968	876120.921408	43.702823
3504.603590	876033.847990	43.707828
3504.591571	875958.021098	43.712833
3504.923610	875876.803207	43.717837
3504.492491	875807.346466	43.722842
3504.718742	875719.452837	43.727847
3505.062625	875641.526826	43.732852
3504.905309	875555.827381	43.737857
3504.703334	875464.606385	43.742861
3504.446173	875388.715597	43.747866
3504.541928	875312.959650	43.752871
3504.505627	875242.558407	43.757876
3504.475028	875173.319164	43.762881
3504.527368	875087.869338	43.767885
3504.206607	875017.512282	43.772890
3504.488976	874938.035397	43.777895
3504.443245	874866.564396	43.782900
3504.182050	874795.806943	43.787905
3504.796764	874719.860918	43.792909
3504.130696	874642.088140	43.797914
3504.706894	874560.133024	43.802919
3504.355529	874489.095786	43.807924
3504.220838	874423.356653	43.812929
3504.728335	874348.781452	43.817933
3504.710225	874281.857604	43.822938
3504.374152	874191.900027	43.827943
3504.240309	874120.628536	43.832948
3504.416403	874053.185117	43.837953
3504.629585	873966.140614	43.842957
3504.468374	873910.197269	43.847962
3504.407819	873826.881900	43.852967
3504.451747	873745.682253	43.857972
3504.265943	873672.764857	43.862977
3504.649739	873601.013816	43.867981
3504.251992	873523.473158	43.872986
3504.511769	873449.800553	43.877991
3504.475856	873380.444225	43.882996
3504.094731	873311.046949	43.888001
3504.263539	873236.998645	43.893005
3504.285962	873173.354057	43.898010
3504.346465	873096.120374	43.903015
3504.274708	873026.183721	43.908020
3503.809484	872963.975462	43.913025
3504.225449	872881.053398	43.918029
3503.861710	872817.662659	43.923034
3504.020027	872748.072908	43.928039
3504.433895	872686.299034	43.933044
3504.199497	872623.952162	43.938049
3504.345522	872544.562713	43.943053
3503.951290	872490.778918	43.948058
3503.945580	872415.196726	43.953063
3504.132993	872355.106175	43.958068
3503.817600	872290.343459	43.963073
3504.269782	872220.505066	43.968077
3504.003146	872161.263602	43.973082
3503.954060	872084.422956	43.978087
3503.985351	872013.875228	43.983092
3503.744238	871959.091064	43.988097
3504.022700	871885.201934	43.993101
3503.762598	871822.268680	43.998106
3504.164962	871764.853773	44.003111
3504.099315	871697.423455	44.008116
3503.831388	871628.376030	44.013121
3503.994602	871564.108794	44.018125
3503.953408	871505.697025	44.023130
3503.972984	871436.891138	44.028135
3503.782665	871372.777127	44.033140
3503.657563	871315.056618	44.038145
3503.711505	871264.099225	44.043149
3503.923141	871190.503632	44.048154
3503.630249	871131.838528	44.053159
3503.767778	871063.688233	44.058164
3503.493886	871001.719066	44.063169
3504.021752	870944.954942	44.068173
3503.649778	870886.203399	44.073178
3503.657612	870825.059444	44.078183
3503.803162	870766.318509	44.083188
3503.472302	870702.123387	44.088193
3503.472986	870652.140086	44.093197
3503.108458	870603.672376	44.098202
3503.575943	870554.096628	44.103207
3503.774050	870501.653121	44.108212
3503.315345	870446.890901	44.113217
3503.582740	870377.352557	44.118221
3503.566301	870327.175238	44.123226
3503.471927	870264.392352	44.128231
3503.747373	870218.922048	44.133236
3503.283581	870160.760860	44.138241
3503.383874	870099.691309	44.143245
3503.749200	870056.243309	44.148250
3503.600971	869995.990163	44.153255
3503.788673	869948.202676	44.158260
3503.378746	869892.068395	44.163265
3503.462165	869825.854245	44.168269
3503.475751	869772.658195	44.173274
3503.433711	869711.608131	44.178279
3503.333319	869657.944486	44.183284
3503.208846	869612.341318	44.188289
3503.585878	869558.015688	44.193293
3503.494242	869507.746807	44.198298
3503.595502	869462.202378	44.203303
3503.349981	869403.318331	44.208308
3503.227722	869349.461371	44.213313
3503.388525	869297.013449	44.218317
3503.286947	869246.452779	44.223322
3503.448498	869196.139567	44.228327
3503.451525	869140.318506	44.233332
3503.173386	869103.085627	44.238337
3503.524349	869032.061677	44.243341
3503.463462	868980.618324	44.248346
3503.624935	868921.274152	44.253351
3503.805757	868869.207521	44.258356
3503.779628	868819.989998	44.263361
3503.553496	868757.213002	44.268365
3503.069854	868705.934026	44.273370
3503.386092	868650.930584	44.278375
3503.570530	868600.899869	44.283380
3503.442628	868551.017284	44.288385
3503.182248	868480.670060	44.293389
3503.003816	868440.698100	44.298394
3503.380208	868389.954363	44.303399
3503.146171	868348.631663	44.308404
3503.071139	868307.185388	44.313409
3503.281059	868252.195808	44.318413
3503.139988	868206.584668	44.323418
3503.131536	868159.009419	44.328423
3503.347959	868116.057371	44.333428
3503.374838	868062.649753	44.338433
3503.542577	868004.266449	44.343437
3503.433373	867960.687251	44.348442
3503.415617	867904.663911	44.353447
3503.422499	867846.596876	44.358452
3502.989486	867796.369879	44.363457
3503.510246	867752.976689	44.368461
3503.404071	867696.965979	44.373466
3503.692182	867650.600182	44.378471
3503.284039	867594.055639	44.383476
3503.169260	867555.329653	44.388481
3503.151355	867495.612515	44.393485
3503.020443	867456.500125	44.398490
3503.206104	867404.614208	44.403495
3502.837810	867360.879125	44.408500
3502.827760	867315.725171	44.413505
3503.279600	867255.539818	44.418509
3503.151348	867220.892526	44.423514
3503.323274	867183.282237	44.428519
3503.192081	867126.299213	44.433524
3503.269146	867082.780068	44.438529
3503.305818	867028.584740	44.443533
3503.089718	866992.105437	44.448538
3503.141359	866945.287591	44.453543
3503.117526	866895.859682	44.458548
3503.013148	866850.523544	44.463553
3503.177421	866799.024395	44.468557
3502.922677	866752.158406	44.473562
3503.070830	866720.182004	44.478567
3503.223045	866675.190745	44.483572
3502.981253	866623.077154	44.488577
3503.161987	866572.447440	44.493581
3503.000654	866526.826882	44.498586
3503.059048	866494.281336	44.503591
3503.037834	866438.924764	44.508596
3502.609769	866399.174587	44.513601
3502.921974	866356.485567	44.518605
3502.736955	866320.288441	44.523610
3502.875352	866275.976355	44.528615
3502.756948	866232.289013	44.533620
3502.396077	866194.954584	44.538625
3503.082966	866141.615419	44.543629
3502.828087	866110.964851	44.548634
3502.818719	866067.064089	44.553639
3502.880291	866021.208716	44.558644
3502.868347	865990.031857	44.563649
3503.095352	865940.846174	44.568653
3502.737419	865897.098732	44.573658
3502.619431	865854.088503	44.578663
3502.817258	865812.191538	44.583668
3502.881320	865782.166685	44.588673
3503.310227	865737.122839	44.593677
3503.101220	865706.559789	44.598682
3502.958934	865657.238365	44.603687
3503.229421	865616.008020	44.608692
3502.890135	865577.986251	44.613697
3503.283005	865525.467185	44.618701
3503.024533	865481.311784	44.623706
3503.108758	865436.419622	44.628711
3503.031758	865391.747969	44.633716
3502.777974	865345.065148	44.638721
3502.805843	865299.306981	44.643725
3502.417260	865279.456940	44.648730
3502.611645	865227.745123	44.653735
3503.205898	865193.549986	44.658740
3502.748084	865165.550915	44.663745
3502.974900	865113.055622	44.668749
3502.527376	865070.774112	44.673754
3502.510470	865038.621698	44.678759
3503.104305	864988.396359	44.683764
3502.711317	864956.596909	44.688769
3502.900079	864912.752251	44.693773
3502.613685	864879.866207	44.698778
3502.611621	864837.315372	44.703783
3502.988604	864792.855939	44.708788
3502.666142	864772.799033	44.713793
3502.894132	864721.465949	44.718797
3502.634946	864687.214257	44.723802
3502.560828	864658.761008	44.728807
3502.940203	864610.025144	44.733812
3502.445837	864574.354263	44.738817
3502.632973	864536.239195	44.743821
3502.408247	864504.992566	44.748826
3502.349983	864477.021623	44.753831
3502.654973	864434.805986	44.758836
3502.728867	864396.417226	44.763841
3503.139861	864359.235725	44.768845
3502.768991	864321.697023	44.773850
3502.806907	864278.358406	44.778855
3502.641842	864248.849471	44.783860
3502.650167	864204.932250	44.788865
3502.656218	864170.342449	44.793869
3502.901292	864130.369240	44.798874
3502.791436	864093.660562	44.803879
3502.887056	864052.739852	44.808884
3502.834337	864017.673051	44.813889
3502.851935	863980.942691	44.818893
3502.849076	863941.883553	44.823898
3502.608296	863901.308732	44.828903
3503.079473	863855.272268	44.833908
3502.648478	863820.946804	44.838913
3502.803157	863785.941656	44.843917
3502.574918	863761.979220	44.848922
3502.638705	863709.498607	44.853927
3502.961800	863676.116923	44.858932
3502.565703	863638.578133	44.863937
3502.600812	863597.858654	44.868941
3502.735078	863571.892357	44.873946
3502.720045	863530.694841	44.878951
3502.639885	863485.912449	44.883956
3502.717573	863465.299417	44.888961
3502.692832	863415.940327	44.893965
3502.623155	863382.718910	44.898970
3502.847221	863337.982476	44.903975
3502.915873	863305.903929	44.908980
3502.728172	863280.961169	44.913985
3502.723314	863231.208601	44.918989
3502.712891	863196.421601	44.923994
3502.368049	863168.783351	44.928999
3502.898981	863125.646786	44.934004
3502.791127	863095.053853	44.939009
3502.479474	863048.168467	44.944013
3502.840485	863011.570007	44.949018
3502.674475	862981.860691	44.954023
3503.093936	862942.628351	44.959028
3502.691467	862902.656552	44.964033
3502.757667	862867.757862	44.969037
3502.361654	862836.628014	44.974042
3502.729253	862813.243923	44.979047
3502.782941	862758.424379	44.984052
3502.848804	862721.095334	44.989057
3502.880908	862685.909666	44.994061
3502.734906	862647.448869	44.999066
3502.753302	862609.835408	45.004071
3502.910669	862568.797321	45.009076
3502.523156	862534.263020	45.014081
3502.649335	862492.452066	45.019085
3502.777174	862469.689277	45.024090
3502.260246	862419.528479	45.029095
3502.708883	862387.382471	45.034100
3502.398758	862362.358911	45.039105
3502.463120	862322.403560	45.044109
3502.562208	862298.770161	45.049114
3502.622815	862262.216681	45.054119
3502.644803	862210.993465	45.059124
3502.154124	862188.039950	45.064129
3502.397668	862154.954586	45.069133
3502.444262	862138.327051	45.074138
3502.414050	862104.120203	45.079143
3502.628249	862068.123409	45.084148
3502.247309	862032.127259	45.089153
3502.679313	862010.478969	45.094157
3502.700434	861973.638675	45.099162
3502.401007	861933.060333	45.104167
3502.552287	861902.224299	45.109172
3502.791928	861868.846434	45.114177
3502.458238	861836.729212	45.119181
3502.571573	861796.081951	45.124186
3502.538284	861762.942867	45.129191
3502.397796	861734.098021	45.134196
3502.566149	861713.658503	45.139201
3502.862548	861668.120258	45.144205
3502.425073	861633.491858	45.149210
3502.456373	861604.423692	45.154215
3502.531309	861569.030096	45.159220
3502.478817	861545.710349	45.164225
3502.611151	861500.781094	45.169229
3502.650978	861473.168937	45.174234
3502.347136	861433.073998	45.179239
3502.834101	861405.582275	45.184244
3502.541521	861374.233467	45.189249
3502.755616	861330.553147	45.194253
3502.508297	861306.098114	45.199258
3502.166482	861270.285412	45.204263
3502.464094	861237.283359	45.209268
3502.559208	861204.314489	45.214273
3502.180213	861168.312896	45.219277
3502.514885	861141.233905	45.224282
3502.403473	861120.935698	45.229287
3502.587312	861069.190153	45.234292
3502.303249	861060.876963	45.239297
3502.677876	861001.030991	45.244301
3502.689290	860986.739161	45.249306
3502.373421	860955.392030	45.254311
3502.689657	860920.635389	45.259316
3502.314823	860899.893784	45.264321
3502.530078	860859.029049	45.269325
3502.444510	860828.323810	45.274330
3502.077590	860799.511836	45.279335
3502.235632	860762.350006	45.284340
3502.258506	860745.722574	45.289345
3502.579433	860713.005487	45.294349
3502.451554	860686.292329	45.299354
3502.214288	860658.041618	45.304359
3502.712003	860628.308651	45.309364
3502.533920	860597.617491	45.314369
3502.776802	860560.634889	45.319373
3502.696370	860518.552757	45.324378
3502.318457	860482.546925	45.329383
3502.476782	860461.618765	45.334388
3502.187334	860434.347806	45.339393
3502.590538	860398.504444	45.344397
3502.460827	860367.706936	45.349402
3502.567597	860340.273056	45.354407
3502.648519	860302.343359	45.359412
3502.572791	860272.411472	45.364417
3502.244114	860232.701600	45.369421
3502.417545	860205.547801	45.374426
3502.460636	860174.623623	45.379431
3502.659583	860140.173533	45.384436
3502.397362	860110.854924	45.389441
3502.877502	860077.038724	45.394445
3502.577613	860045.003692	45.399450
3502.391222	860004.685536	45.404455
3502.358718	859975.911791	45.409460
3502.500132	859950.220536	45.414465
3502.299014	859926.335709	45.419469
3502.563756	859895.762512	45.424474
3502.497410	859861.743472	45.429479
3502.819369	859823.868318	45.434484
3502.431655	859797.485761	45.439489
3502.309943	859757.835926	45.444493
3502.635869	859731.918893	45.449498
3502.259889	859705.728467	45.454503
3502.286289	859666.442562	45.459508
3502.227238	859645.547419	45.464513
3502.198288	859611.715288	45.469517
3502.524499	859586.672689	45.474522
3502.289427	859560.652890	45.479527
3502.482750	859526.880903	45.484532
3502.540118	859503.729707	45.489537
3502.843935	859464.591267	45.494541
3502.718266	859434.857968	45.499546
3502.325072	859403.710058	45.504551
3502.730395	859360.081360	45.509556
3502.562461	859334.924670	45.514561
3502.443211	859287.297911	45.519565
3502.398468	859268.246642	45.524570
3502.286930	859235.398416	45.529575
3502.543656	859201.614186	45.534580
3502.272708	859172.778701	45.539585
3502.525272	859139.092052	45.544589
3502.390264	859113.053858	45.549594
3502.209500	859083.814131	45.554599
3502.502143	859047.883827	45.559604
3502.522208	859033.877723	45.564609
3502.359954	859005.995962	45.569613
3502.552801	858979.805943	45.574618
3502.310567	858940.462385	45.579623
3502.144365	858916.276119	45.584628
3502.434091	858883.457135	45.589633
3502.209615	858854.126266	45.594637
3502.333025	858824.348958	45.599642
3502.124627	858805.614945	45.604647
3502.445555	858763.746323	45.609652
3502.053825	858743.778122	45.614657
3502.229038	858722.743980	45.619661
3502.362230	858691.213967	45.624666
3502.320369	858670.409904	45.629671
3502.370993	858635.586780	45.634676
3502.325685	858611.184891	45.639681
3502.062578	858576.024122	45.644685
3501.987224	858558.920671	45.649690
3502.146574	858535.457258	45.654695
3502.383621	858507.312936	45.659700
3502.383339	858495.059458	45.664705
3502.151099	858452.988096	45.669709
3502.446409	858436.212239	45.674714
3502.193516	858399.298242	45.679719
3502.491971	858377.756350	45.684724
3502.055473	858332.508479	45.689729
3502.439088	858302.491258	45.694733
3502.551811	858286.620357	45.699738
3502.294752	858261.571183	45.704743
3502.357903	858226.062886	45.709748
3502.331456	858195.626426	45.714753
3501.948829	858167.096358	45.719757
3501.536658	858138.571024	45.724762
3501.498621	858131.574876	45.729767
3502.323117	858110.820687	45.734772
3502.008942	858091.615628	45.739777
3502.517184	858070.427123	45.744781
3502.327615	858043.420788	45.749786
3501.935141	858024.909224	45.754791
3502.204904	858009.595282	45.759796
3501.921669	857968.015278	45.764801
3502.044191	857949.710416	45.769805
3502.083730	857931.030132	45.774810
3501.803410	857881.765550	45.779815
3502.252125	857791.336117	45.784820
3501.649753	857665.480075	45.789825
3502.167648	857459.775671	45.794829
3501.935050	857212.750722	45.799834
3501.767366	856900.044224	45.804839
3501.935334	856527.341178	45.809844
3501.873744	856094.723810	45.814849
3501.784705	855591.638167	45.819853
3501.585572	855041.044724	45.824858
3501.520646	854412.236318	45.829863
3501.339631	853726.058169	45.834868
3501.059036	852996.699841	45.839873
3500.694984	852185.690284	45.844877
3500.811939	851316.271997	45.849882
3500.570852	850380.379136	45.854887
3500.092884	849359.749223	45.859892
3499.864383	848297.316697	45.864897
3500.036640	847151.043986	45.869901
3499.714373	845934.383453	45.874906
3499.090499	844633.714894	45.879911
3498.829189	843264.280805	45.884916
3498.353913	841840.417712	45.889921
3498.230414	840323.616929	45.894925
3498.142583	838747.230270	45.899930
3497.454663	837090.241475	45.904935
3496.920878	835349.683141	45.909940
3496.767295	833536.484878	45.914945
3496.286278	831653.292126	45.919949
3495.912586	829684.929097	45.924954
3495.219468	827651.767211	45.929959
3494.871824	825524.751514	45.934964
3494.085205	823346.511081	45.939969
3493.394060	821080.813272	45.944973
3493.033612	818747.887929	45.949978
3492.336180	816328.787043	45.954983
3491.817402	813835.675888	45.959988
3491.068785	811275.353244	45.964993
3490.622853	808635.360639	45.969997
3490.049372	805935.193089	45.975002
3489.303009	803137.717119	45.980007
3488.349206	800260.685548	45.985012
3487.970999	797340.886882	45.990017
3487.025812	794336.921394	45.995021
3486.282686	791245.369496	46.000026
3485.423455	788090.064015	46.005031
3484.628829	784853.592337	46.010036
3483.818234	781560.710951	46.015041
3482.779941	778181.465639	46.020045
3482.161614	774739.473117	46.025050
3480.766373	771219.632959	46.030055
3479.964059	767631.676097	46.035060
3479.183550	763988.877370	46.040065
3478.335229	760253.938985	46.045069
3476.879806	756439.663068	46.050074
3475.562975	752584.345082	46.055079
3474.956174	748645.058446	46.060084
3473.789414	744631.790800	46.065089
3472.973923	740545.188530	46.070093
3471.555829	736390.166049	46.075098
3470.474041	732179.258125	46.080103
3469.453749	727886.388292	46.085108
3468.385732	723527.825708	46.090113
3467.180092	719079.801385	46.095117
3465.498655	714579.666496	46.100122
3464.430718	710011.100573	46.105127
3463.545702	705370.864630	46.110132
3462.177783	700666.139167	46.115137
3460.856180	695879.309795	46.120141
3459.443896	691024.029798	46.125146
3457.979450	686103.649894	46.130151
3456.498689	681107.284871	46.135156
3455.062828	676052.528212	46.140161
3453.856989	670932.111781	46.145165
3452.554586	665731.952650	46.150170
3450.747090	660471.096497	46.155175
3449.521924	655114.446419	46.160180
3447.758517	649728.435958	46.165185
3446.100289	644255.408808	46.170189
3444.433627	638734.008521	46.175194
3442.756903	633142.883227	46.180199
3440.995553	627487.641476	46.185204
3439.000459	621772.966153	46.190209
3437.167521	615986.467587	46.195213
3435.503923	610152.161047	46.200218
3433.929138	604254.984990	46.205223
3432.277934	598271.176170	46.210228
3430.050285	592253.539861	46.215233
3428.335689	586156.468245	46.220237
3426.487334	580013.349453	46.225242
3423.941016	573810.183235	46.230247
3422.238906	567525.650088	46.235252
3419.813084	561215.252339	46.240257
3418.253796	554836.888013	46.245261
3415.868387	548391.816653	46.250266
3413.542225	541885.366431	46.255271
3411.423643	535340.710305	46.260276
3409.150369	528738.142519	46.265281
3406.927022	522077.223262	46.270285
3404.801369	515356.682004	46.275290
3402.102813	508598.719225	46.280295
3399.960111	501783.360032	46.285300
3397.425921	494923.873252	46.290305
3395.200928	487998.412298	46.295309
3392.067946	481029.409768	46.300314
3389.984008	474032.836696	46.305319
3387.384727	466955.860803	46.310324
3384.617922	459863.756358	46.315329
3381.865877	452717.427464	46.320333
3379.284409	445519.471303	46.325338
3376.257322	438287.281527	46.330343
3373.583803	431012.820830	46.335348
3370.710123	423700.705199	46.340353
3367.944446	416348.307426	46.345357
3364.764915	408959.003643	46.350362
3361.709953	401547.382713	46.355367
3358.822038	394072.533994	46.360372
3355.476908	386580.620918	46.365377
3352.749807	379055.059117	46.370381
3349.535179	371486.044019	46.375386
3346.513265	363884.987840	46.380391
3343.066817	356263.121789	46.385396
3339.461176	348627.827245	46.390401
3336.108336	340948.500864	46.395405
3333.083753	333247.311652	46.400410
3329.543713	325538.883009	46.405415
3326.169237	317786.426569	46.410420
3322.467159	310025.689724	46.415425
3319.069451	302249.932792	46.420429
3315.319883	294443.077975	46.425434
3311.453982	286637.817475	46.430439
3308.095538	278806.737176	46.435444
3304.632608	270967.573637	46.440449
3300.551169	263113.321097	46.445453
3296.815626	255243.938230	46.450458
3292.667923	247375.586477	46.455463
3288.959712	239501.215509	46.460468
3284.950500	231621.372859	46.465473
3280.881549	223653.251994	46.470477
3276.773598	215741.795035	46.475482
3272.606866	207839.311938	46.480487
3268.579032	199947.008715	46.485492
3264.191875	192062.055713	46.490497
3259.779912	184181.206800	46.495501
3255.189201	176313.067187	46.500506
3250.628182	168455.859261	46.505511
3246.137373	160607.757079	46.510516
3241.428479	152782.046234	46.515521
3236.502282	144975.475438	46.520525
3231.471777	137188.093707	46.525530
3226.139111	129428.565172	46.530535
3221.710625	121696.278993	46.535540
3216.412053	114010.534986	46.540545
3211.027980	106341.922105	46.545549
3205.409161	98715.647669	46.550554
3199.753054	91135.033841	46.555559
3194.210159	83598.182606	46.560564
3188.007721	76122.694250	46.565569
3181.678295	68701.489916	46.570573
3175.057274	61358.072196	46.575578
3167.668723	54093.742223	46.580583
3159.497447	46911.234792	46.585588
3147.333206	39953.333564	46.590593
3126.058372	33390.760079	46.595597
3098.972445	27224.290789	46.600602
3066.619717	21577.344906	46.605607
3033.151330	16480.335697	46.610612
2999.587681	11967.695909	46.615617
2968.800745	8033.676096	46.620621
2940.831327	4719.246845	46.625626
2915.164421	1997.880008	46.630631
2872.876286	366.826325	46.635636
2800.805556	324.928329	46.640641
2765.482673	320.887623	46.645645
2766.475653	302.429337	46.650650
2788.131081	298.153448	46.655655
2815.662833	280.218992	46.660660
2837.865356	296.500641	46.665665
2850.903580	291.863510	46.670669
2855.865475	291.679602	46.675674
2854.022546	289.121819	46.680679
2850.078200	284.570634	46.685684
2844.881761	281.366666	46.690689
2839.954656	285.076183	46.695693
2836.935218	287.715941	46.700698
2833.684476	274.657350	46.705703
2831.892419	269.043820	46.710708
2829.547661	276.551226	46.715713
2827.138230	268.135065	46.720717
2825.040093	263.083551	46.725722
2821.458612	275.995371	46.730727
2818.727396	270.261697	46.735732
2815.794944	270.006306	46.740737
2812.839229	266.758304	46.745741
2809.818381	259.519339	46.750746
2806.455654	267.502161	46.755751
2803.214381	257.759770	46.760756
2799.887104	255.541244	46.765761
2797.027117	258.242727	46.770765
2793.990203	247.808298	46.775770
2790.780998	255.204947	46.780775
2787.189099	259.710130	46.785780
2784.146734	251.766277	46.790785
2780.687357	254.315249	46.795789
2777.674423	255.165646	46.800794
2774.076696	247.938219	46.805799
2771.252150	245.397983	46.810804
2767.813972	251.719017	46.815809
2763.991690	252.824918	46.820813
2761.162407	245.191276	46.825818
2757.559971	244.270909	46.830823
2754.053403	242.294339	46.835828
2750.799734	249.271295	46.840833
2747.756968	251.410935	46.845837
2744.624562	249.897960	46.850842
2740.875862	243.737043	46.855847
2737.211035	244.143653	46.860852
2734.065194	237.937344	46.865857
2730.645586	246.175078	46.870861
2727.480081	237.151211	46.875866
2723.397699	240.288872	46.880871
2720.457790	241.049500	46.885876
2717.262331	237.757450	46.890881
2713.799634	241.650121	46.895885
2710.567554	247.125711	46.900890
2706.729931	244.655189	46.905895
2703.435020	234.061327	46.910900
2699.675514	239.820503	46.915905
2696.072910	239.612218	46.920909
2693.265038	235.127828	46.925914
2689.745283	247.942685	46.930919
2686.170780	230.907157	46.935924
2682.937462	228.099341	46.940929
2679.218587	232.923527	46.945933
2675.926672	232.623733	46.950938
2672.132931	232.032588	46.955943
2669.210038	226.697312	46.960948
2665.598775	229.693336	46.965953
2662.002162	239.223303	46.970957
2658.887775	226.405250	46.975962
2654.818505	227.628952	46.980967
2652.054695	225.989301	46.985972
2648.667296	221.217337	46.990977
2645.152374	229.168514	46.995981
2641.795694	217.853555	47.000986
2637.531328	227.701721	47.005991
2634.500885	220.145968	47.010996
2631.097352	219.616762	47.016001
2627.793505	228.193422	47.021005
2624.186452	223.972784	47.026010
2620.616495	226.078721	47.031015
2617.547714	223.994879	47.036020
2613.615344	225.387049	47.041025
2609.948201	230.490469	47.046029
2607.026616	224.377097	47.051034
2603.181911	228.336036	47.056039
2599.550116	221.531562	47.061044
2596.333055	224.936593	47.066049
2593.027120	218.864164	47.071053
2589.772097	219.803169	47.076058
2586.033201	218.642984	47.081063
2582.531644	226.900635	47.086068
2579.256824	220.901227	47.091073
2575.167901	216.382441	47.096077
2571.971368	212.166719	47.101082
2568.401417	221.828105	47.106087
2565.166811	226.758343	47.111092
2561.599586	227.618250	47.116097
2557.970510	222.438665	47.121101
2555.064210	211.884205	47.126106
2551.485490	225.180894	47.131111
2547.982629	220.817610	47.136116
2544.420198	218.307330	47.141121
2540.338323	213.973308	47.146125
2537.092397	214.490902	47.151130
2533.772139	216.125089	47.156135
2530.411749	214.712636	47.161140
2526.411092	209.090792	47.166145
2523.028955	215.704646	47.171149
2520.301342	203.047852	47.176154
2516.600075	216.068373	47.181159
2513.132063	215.710525	47.186164
2509.568302	204.783495	47.191169
2505.844212	213.402343	47.196173
2502.465238	212.618943	47.201178
2499.240903	211.710563	47.206183
2496.074391	203.488848	47.211188
2492.197758	203.644251	47.216193
2488.139136	216.016105	47.221197
2485.310826	207.697330	47.226202
2481.330760	214.288730	47.231207
2477.936826	202.889482	47.236212
2474.620357	208.778347	47.241217
2470.968268	203.077906	47.246221
2467.984836	205.533524	47.251226
2463.782855	210.124609	47.256231
2460.466273	205.703811	47.261236
2456.859957	207.779944	47.266241
2453.331606	207.265937	47.271245
2450.048295	203.099159	47.276250
2446.542825	202.131246	47.281255
2443.159300	195.511294	47.286260
2439.495775	212.434558	47.291265
2436.086266	204.714575	47.296269
2432.995696	199.590862	47.301274
2429.001168	201.331873	47.306279
2425.869491	206.507267	47.311284
2422.579947	199.549361	47.316289
2418.683545	201.164659	47.321293
2415.367327	196.179836	47.326298
2411.579613	204.226298	47.331303
2408.595208	208.767610	47.336308
2404.730618	206.676341	47.341313
2400.713668	197.702504	47.346317
2397.797569	192.624810	47.351322
2394.248232	205.740695	47.356327
2390.704432	194.695624	47.361332
2387.699554	196.745147	47.366337
2384.187384	200.395568	47.371341
2380.862476	200.104969	47.376346
2376.794467	198.089730	47.381351
2373.066144	185.340712	47.386356
2369.414955	190.244310	47.391361
2365.499215	191.409351	47.396365
2362.818297	192.587237	47.401370
2359.390912	193.895650	47.406375
2356.259404	187.529782	47.411380
2352.663929	184.941631	47.416385
2349.025191	196.758597	47.421389
2345.833085	195.518203	47.426394
2341.981817	192.356582	47.431399
2338.222706	187.553073	47.436404
2334.896299	187.687627	47.441409
2331.217136	194.083227	47.446413
2328.082141	183.269504	47.451418
2324.154061	193.182353	47.456423
2320.821032	185.512994	47.461428
2317.453604	182.214095	47.466433
2313.956668	183.143483	47.471437
2310.578014	185.787969	47.476442
2306.955556	190.036039	47.481447
2303.292269	186.722448	47.486452
2299.917026	187.402446	47.491457
2296.064572	183.824080	47.496461
2293.066038	183.570042	47.501466
2289.529547	182.393646	47.506471
2286.032562	174.310922	47.511476
2282.487579	175.035334	47.516481
2278.852333	188.716232	47.521485
2275.400468	184.115042	47.526490
2271.499138	183.003035	47.531495
2268.277004	184.341956	47.536500
2265.215196	183.519780	47.541505
2261.723093	183.862306	47.546509
2258.308940	179.407646	47.551514
2254.285826	191.803973	47.556519
2250.476901	183.330336	47.561524
2247.406449	173.713551	47.566529
2243.613284	175.396399	47.571533
2240.370725	183.730476	47.576538
2237.267233	186.152173	47.581543
2233.480301	180.320466	47.586548
2229.889979	179.721736	47.591553
2226.321007	176.895064	47.596557
2223.131282	170.356962	47.601562
2219.681671	180.199562	47.606567
2216.142130	181.497580	47.611572
2212.782481	174.521224	47.616577
2208.991541	184.009918	47.621581
2205.283967	177.487665	47.626586
2201.453799	176.866788	47.631591
2198.657959	169.739338	47.636596
2195.060995	177.668204	47.641601
2191.398533	191.550004	47.646605
2188.116451	178.949683	47.651610
2184.539147	180.734877	47.656615
2180.541110	177.514545	47.661620
2177.321675	178.148772	47.666625
2174.031277	186.167742	47.671629
2170.854648	185.567647	47.676634
2167.281860	182.266059	47.681639
2163.820730	186.129023	47.686644
2160.026847	175.859558	47.691649
2156.505306	177.761269	47.696653
2153.281395	176.221564	47.701658
2149.313987	182.848207	47.706663
2145.682099	178.045560	47.711668
2142.503938	171.278863	47.716673
2138.845306	173.881480	47.721677
2135.456160	170.888233	47.726682
2131.903786	175.004273	47.731687
2128.569989	178.020563	47.736692
2124.715250	170.559858	47.741697
2121.519988	185.070630	47.746701
2118.105015	172.361874	47.751706
2114.440178	174.619400	47.756711
2110.646565	188.794640	47.761716
2107.526537	170.820703	47.766721
2104.343065	177.617491	47.771725
2101.033466	174.108902	47.776730
2096.980808	172.276081	47.781735
2093.355527	182.215850	47.786740
2089.877366	178.794304	47.791745
2086.359546	185.758800	47.796749
2083.046093	176.285865	47.801754
2079.357663	182.109101	47.806759
2076.052442	173.731826	47.811764
2072.668288	165.919750	47.816769
2068.948725	179.453068	47.821773
2065.557176	172.814414	47.826778
2061.807509	179.468510	47.831783
2058.324903	175.917676	47.836788
2055.083838	167.540286	47.841793
2051.392933	165.344060	47.846797
2048.239648	165.040742	47.851802
2044.273103	172.455689	47.856807
2040.982898	171.375167	47.861812
2037.697994	170.471576	47.866817
2034.081465	173.912523	47.871821
2030.473325	159.010549	47.876826
2026.917810	167.850897	47.881831
2023.485887	164.350332	47.886836
2019.803276	168.644250	47.891841
2016.592805	174.134027	47.896845
2012.985028	170.674548	47.901850
2009.372746	176.611948	47.906855
2006.022794	174.626056	47.911860
2002.424535	165.056958	47.916865
1998.748965	169.580023	47.921869
1995.615971	171.464055	47.926874
1991.775533	177.389220	47.931879
1988.596509	165.137330	47.936884
1985.456750	160.542644	47.941889
1981.505357	172.002371	47.946893
1977.961264	168.998519	47.951898
1974.460523	170.709057	47.956903
1970.685990	168.904809	47.961908
1967.815410	158.807466	47.966913
1963.895114	170.417967	47.971917
1960.408409	161.586885	47.976922
1956.925351	164.578405	47.981927
1953.529782	163.587771	47.986932
1949.778556	166.258705	47.991937
1946.506666	164.571958	47.996941
1942.863891	162.124551	48.001946
1939.257684	164.526446	48.006951
1936.041020	153.885193	48.011956
1933.042498	158.657611	48.016961
1928.964114	160.111532	48.021965
1925.439056	159.784052	48.026970
1921.826035	166.541774	48.031975
1918.462377	175.164811	48.036980
1914.986455	161.818042	48.041985
1911.244742	168.850016	48.046989
1908.022660	161.001831	48.051994
1904.347685	158.600820	48.056999
1900.981177	163.442720	48.062004
1897.441615	157.491119	48.067009
1893.630808	156.438869	48.072013
1890.305129	152.108414	48.077018
1886.887602	154.082530	48.082023
1883.308139	159.653263	48.087028
1880.452101	153.005048	48.092033
1876.798013	156.321275	48.097037
1872.901081	159.704061	48.102042
1869.152449	166.408834	48.107047
1865.720321	160.181589	48.112052
1862.455420	153.919229	48.117057
1859.135254	167.122264	48.122061
1855.848608	160.897637	48.127066
1851.855889	164.206670	48.132071
1848.302198	166.722899	48.137076
1844.701774	161.204487	48.142081
1841.122221	162.036954	48.147085
1837.905157	153.877977	48.152090
1834.554056	159.346887	48.157095
1831.035761	154.818984	48.162100
1827.647068	161.068269	48.167105
1824.186936	164.036558	48.172109
1820.487324	158.878711	48.177114
1816.748234	157.865195	48.182119
1813.066816	161.654665	48.187124
1809.718197	149.180917	48.192129
1806.264458	157.131760	48.197133
1803.033941	149.697690	48.202138
1799.360769	159.336513	48.207143
1795.924254	158.653897	48.212148
1792.293649	153.668990	48.217153
1788.858669	159.383067	48.222157
1785.646710	151.699270	48.227162
1781.727578	158.944757	48.232167
1778.342906	163.257318	48.237172
1775.204898	159.736017	48.242177
1771.725846	160.237177	48.247181
1767.786926	158.942351	48.252186
1764.137706	157.125860	48.257191
1760.572191	164.884640	48.262196
1757.264020	157.449418	48.267201
1753.691489	159.627629	48.272205
1750.092857	162.037686	48.277210
1746.701560	157.853551	48.282215
1743.635935	160.044920	48.287220
1740.268669	142.328851	48.292225
1736.073729	152.881352	48.297229
1732.901398	150.063544	48.302234
1729.647645	146.874181	48.307239
1725.917968	153.986978	48.312244
1722.383906	148.087106	48.317249
1718.542402	152.350458	48.322253
1715.289766	153.146770	48.327258
1711.727064	152.908157	48.332263
1708.453160	155.951532	48.337268
1704.823423	154.031424	48.342273
1701.007030	166.269843	48.347277
1697.672130	156.293215	48.352282
1694.272617	150.058551	48.357287
1690.896176	156.801417	48.362292
1687.502965	149.880557	48.367297
1683.769670	156.457419	48.372301
1680.307775	157.928494	48.377306
1676.882476	161.646938	48.382311
1673.027101	168.269043	48.387316
1669.811066	147.681234	48.392321
1666.646470	154.166911	48.397325
1663.207150	156.570642	48.402330
1659.038767	155.835584	48.407335
1655.584369	155.408618	48.412340
1652.353769	158.567424	48.417345
1648.712730	167.073254	48.422349
1645.332047	153.854458	48.427354
1641.673656	158.336065	48.432359
1638.210398	151.973643	48.437364
1634.825728	153.760560	48.442369
1631.177811	156.524388	48.447373
1627.897876	154.884585	48.452378
1624.190907	158.559815	48.457383
1620.859694	155.510809	48.462388
1617.397016	160.018312	48.467393
1613.727580	155.936281	48.472397
1610.311817	147.866358	48.477402
1606.793616	149.109588	48.482407
1603.153211	154.061271	48.487412
1600.102191	149.385698	48.492417
1595.955879	151.304214	48.497421
1592.307123	148.757434	48.502426
1589.146785	152.721849	48.507431
1585.792812	150.663324	48.512436
1582.135662	145.984710	48.517441
1578.427415	150.348106	48.522445
1575.349543	143.368721	48.527450
1571.959271	148.764941	48.532455
1568.380760	145.644751	48.537460
1565.029793	145.335743	48.542465
1560.971530	155.050001	48.547469
1558.090248	146.679072	48.552474
1554.399866	155.793418	48.557479
1550.502743	147.188178	48.562484
1546.981616	147.786245	48.567489
1543.444011	152.435041	48.572493
1540.359140	144.305565	48.577498
1536.825935	149.698195	48.582503
1533.233335	154.183810	48.587508
1529.670774	148.447465	48.592513
1525.994233	142.945059	48.597517
1522.506728	142.911237	48.602522
1519.073495	155.169732	48.607527
1515.859136	146.156283	48.612532
1511.992608	142.219984	48.617537
1508.726837	159.675741	48.622541
1505.528271	144.300461	48.627546
1501.783232	143.675560	48.632551
1498.258596	151.043736	48.637556
1494.578760	145.375741	48.642561
1490.739515	142.170827	48.647565
1487.257564	148.369239	48.652570
1484.156404	142.800792	48.657575
1480.632098	137.496655	48.662580
1477.447491	136.536432	48.667585
1473.267132	142.554657	48.672589
1469.998438	148.773290	48.677594
1466.727560	146.505559	48.682599
1462.955194	148.899546	48.687604
1459.858642	142.258809	48.692609
1456.436808	141.941660	48.697613
1452.966323	138.412390	48.702618
1449.100753	148.678414	48.707623
1445.451352	150.297472	48.712628
1442.263368	140.005908	48.717633
1438.313635	144.845434	48.722637
1434.665556	145.759785	48.727642
1431.579458	148.786317	48.732647
1428.167372	140.553333	48.737652
1425.052387	140.109519	48.742657
1421.006841	150.846360	48.747661
1417.698152	132.177639	48.752666
1414.254292	140.949009	48.757671
1410.306420	144.863919	48.762676
1407.037911	134.322052	48.767681
1403.248364	139.343914	48.772685
1400.136983	137.151897	48.777690
1396.665426	134.674069	48.782695
1393.255988	147.714305	48.787700
1389.463363	138.267669	48.792705
1385.844341	148.518248	48.797709
1382.268413	133.533233	48.802714
1378.946589	134.637416	48.807719
1375.439897	146.066882	48.812724
1372.446511	133.734314	48.817729
1368.571618	146.762890	48.822733
1364.809807	134.741254	48.827738
1361.351075	139.309255	48.832743
1358.028294	142.206623	48.837748
1354.837860	140.992883	48.842753
1351.267244	145.869473	48.847757
1347.713581	144.894759	48.852762
1344.182325	146.310449	48.857767
1340.484865	152.543400	48.862772
1336.998305	142.734624	48.867777
1333.531981	145.847351	48.872781
1330.120796	139.669771	48.877786
1326.481223	140.915907	48.882791
1322.432826	143.138558	48.887796
1319.270654	144.502337	48.892801
1315.365203	151.298946	48.897805
1312.578887	142.488221	48.902810
1309.121639	138.438470	48.907815
1305.380081	138.113305	48.912820
1302.723108	135.140960	48.917825
1298.478185	138.895883	48.922829
1295.115366	142.152556	48.927834
1291.502598	136.621459	48.932839
1288.066547	136.489915	48.937844
1284.421299	133.619373	48.942849
1280.764569	141.900706	48.947853
1277.465085	135.742793	48.952858
1274.246188	136.277491	48.957863
1270.295761	135.032162	48.962868
1267.164899	137.431954	48.967873
1263.674457	141.542115	48.972877
1259.865822	130.319251	48.977882
1256.032276	145.858309	48.982887
1252.701374	142.603511	48.987892
1249.561099	138.242504	48.992897
1246.146055	142.587873	48.997901
1242.625771	134.912454	49.002906
1238.985397	133.863951	49.007911
1235.333806	131.012654	49.012916
1231.992603	137.754132	49.017921
1228.418933	136.954701	49.022925
1224.706999	138.472180	49.027930
1221.217623	137.955024	49.032935
1217.911711	130.327071	49.037940
1215.058189	128.524332	49.042945
1210.478892	132.492874	49.047949
1207.135012	136.751714	49.052954
1203.909741	128.100469	49.057959
1200.423525	138.456101	49.062964
1197.028033	133.101107	49.067969
1193.620152	127.547671	49.072973
1190.086127	127.939950	49.077978
1186.330083	141.422217	49.082983
1182.207780	131.943847	49.087988
1179.508238	127.137261	49.092993
1175.770471	129.915890	49.097997
1172.631006	136.350743	49.103002
1168.970718	124.196877	49.108007
1165.445900	131.811186	49.113012
1161.937018	123.749149	49.118017
1158.386016	136.014692	49.123021
1154.570564	132.010476	49.128026
1151.396685	132.757848	49.133031
1147.619367	138.039358	49.138036
1144.579408	131.431734	49.143041
1141.173674	138.621044	49.148045
1137.232727	125.616908	49.153050
1133.853895	131.586569	49.158055
1130.268621	128.505352	49.163060
1126.504813	130.644217	49.168065
1123.459118	135.846618	49.173069
1119.976468	124.517504	49.178074
1116.406469	133.617373	49.183079
1112.767676	137.771115	49.188084
1109.205419	127.397259	49.193089
1105.743765	137.431574	49.198093
1102.541817	133.938107	49.203098
1099.060389	131.431559	49.208103
1095.166149	133.261476	49.213108
1091.978651	130.838353	49.218113
1088.133359	132.794372	49.223117
1084.422283	133.411766	49.228122
1081.517809	129.472285	49.233127
1077.701983	131.747665	49.238132
1074.198834	118.024537	49.243137
1070.583889	131.651874	49.248141
1067.274062	125.912026	49.253146
1063.881656	133.556017	49.258151
1059.879141	127.761591	49.263156
1056.839455	131.294948	49.268161
1053.242219	125.699132	49.273165
1049.903267	130.090664	49.278170
1046.258793	127.468444	49.283175
1042.724417	130.009502	49.288180
1039.394089	119.704321	49.293185
1035.837564	127.072948	49.298189
1032.429995	133.520645	49.303194
1029.017354	120.986150	49.308199
1025.074669	131.348700	49.313204
1021.778869	122.441087	49.318209
1017.996263	131.222354	49.323213
1014.407040	127.618942	49.328218
1011.173909	132.559163	49.333223
1007.953086	130.915174	49.338228
1004.437572	127.489223	49.343233
1000.741593	133.198443	49.348237
997.117302	126.922982	49.353242
993.694345	124.543210	49.358247
990.012870	141.723808	49.363252
986.857645	130.953790	49.368257
983.139227	126.616758	49.373261
979.566678	126.141961	49.378266
975.922017	128.808460	49.383271
972.553728	134.053052	49.388276
969.569043	122.325791	49.393281
965.797406	129.351945	49.398285
962.400847	132.485964	49.403290
958.739066	132.942373	49.408295
954.791898	134.706962	49.413300
951.681677	125.074287	49.418305
948.002452	125.384008	49.423309
944.557089	127.541597	49.428314
941.216869	130.046084	49.433319
937.615187	130.489019	49.438324
933.891204	129.646996	49.443329
930.555883	130.014510	49.448333
927.295492	123.308135	49.453338
923.651654	131.339732	49.458343
920.001236	127.925702	49.463348
916.802906	124.198526	49.468353
913.259384	123.383509	49.473357
909.676557	129.054154	49.478362
906.056120	121.617797	49.483367
902.462069	124.597050	49.488372
899.123631	121.110328	49.493377
895.505166	132.540822	49.498381
892.303262	120.603468	49.503386
888.983555	125.170123	49.508391
885.016174	126.832541	49.513396
881.752148	118.879045	49.518401
877.698641	131.542038	49.523405
874.410168	122.767524	49.528410
871.083383	127.164271	49.533415
867.557009	122.318617	49.538420
864.332348	118.973540	49.543425
860.751181	122.028445	49.548429
856.787370	124.706185	49.553434
853.422106	127.041616	49.558439
849.742741	129.543653	49.563444
846.973162	118.885408	49.568449
843.187984	120.845304	49.573453
839.612988	127.406469	49.578458
836.526618	125.346682	49.583463
832.460198	138.192611	49.588468
829.166317	121.714216	49.593473
825.232090	133.152980	49.598477
822.272722	118.564611	49.603482
818.533690	125.270337	49.608487
814.793972	130.246330	49.613492
811.210388	121.792020	49.618497
807.775255	127.751878	49.623501
804.545297	119.966071	49.628506
801.292932	122.618535	49.633511
797.266477	131.692696	49.638516
794.165112	125.546015	49.643521
790.621383	128.623397	49.648525
786.958815	126.129105	49.653530
783.766907	122.595148	49.658535
779.847473	126.803062	49.663540
776.720331	121.331604	49.668545
772.796385	134.218341	49.673549
769.503199	130.587085	49.678554
766.027531	125.361148	49.683559
762.143707	133.037100	49.688564
758.992940	125.155347	49.693569
755.654426	132.652891	49.698573
751.817820	129.643756	49.703578
748.514373	124.181946	49.708583
744.801246	131.411716	49.713588
741.359934	121.256772	49.718593
738.038747	125.960926	49.723597
734.478969	116.394903	49.728602
731.545942	121.838404	49.733607
727.377406	132.440224	49.738612
724.321190	119.299040	49.743617
720.479836	129.499625	49.748621
716.575693	129.049702	49.753626
713.195859	122.388912	49.758631
709.936109	122.590561	49.763636
706.342534	114.875448	49.768641
702.699212	120.067845	49.773645
699.400052	121.871880	49.778650
696.077753	121.924045	49.783655
692.505230	125.423434	49.788660
689.232700	121.505845	49.793665
685.128165	122.821319	49.798669
682.003863	124.917901	49.803674
678.850663	124.677279	49.808679
674.845044	133.713955	49.813684
671.453750	119.169341	49.818689
667.640967	120.243965	49.823693
664.256695	115.967577	49.828698
660.677164	121.766720	49.833703
657.173364	117.846767	49.838708
653.823564	112.179189	49.843713
650.190028	122.008787	49.848717
646.907575	115.078763	49.853722
643.340358	116.714458	49.858727
639.571566	124.890072	49.863732
636.642296	120.633544	49.868737
632.996663	112.442257	49.873741
629.414076	114.539706	49.878746
626.293476	116.066793	49.883751
622.559248	125.838479	49.888756
618.888333	120.152618	49.893761
615.317128	117.473849	49.898765
611.908538	119.185939	49.903770
608.451380	116.646767	49.908775
604.754182	120.284463	49.913780
601.331126	109.108378	49.918785
597.598656	113.496462	49.923789
594.314301	116.564824	49.928794
590.856642	111.786579	49.933799
587.159934	121.340734	49.938804
584.378718	113.618999	49.943809
580.527218	117.233305	49.948813
576.748850	124.816176	49.953818
573.108616	112.911567	49.958823
569.593253	122.287334	49.963828
566.138139	114.078200	49.968833
562.794825	121.761371	49.973837
559.257172	114.881736	49.978842
556.098545	113.404608	49.983847
552.019453	119.075736	49.988852
548.559802	112.017443	49.993857
544.931148	124.505608	49.998861
541.603180	128.470619	50.003866
538.576548	118.414386	50.008871
534.652029	126.956649	50.013876
531.671713	117.922655	50.018881
528.247540	116.396344	50.023885
524.389503	112.722786	50.028890
520.498392	114.892884	50.033895
517.070109	125.376529	50.038900
513.792123	112.123039	50.043905
510.280226	123.513665	50.048909
506.678810	124.631399	50.053914
502.943522	116.974847	50.058919
499.488057	121.247910	50.063924
496.473378	122.083462	50.068929
492.632378	122.517815	50.073933
489.029643	115.452662	50.078938
485.922832	114.167702	50.083943
482.393402	117.399244	50.088948
478.771241	117.816340	50.093953
475.170253	122.001219	50.098957
471.787846	112.246444	50.103962
468.435167	114.435034	50.108967
464.496516	118.911219	50.113972
461.290583	112.407365	50.118977
457.968090	119.481735	50.123981
454.155466	116.671964	50.128986
450.615095	111.505553	50.133991
446.824218	121.494142	50.138996
443.643516	113.788693	50.144001
439.877294	120.458955	50.149005
436.473717	118.033208	50.154010
433.271712	115.498329	50.159015
429.820596	118.171122	50.164020
426.426093	110.946457	50.169025
422.803748	110.053322	50.174029
419.275664	113.516559	50.179034
415.948064	118.497482	50.184039
411.948709	120.483516	50.189044
408.691193	113.521345	50.194049
404.959853	116.227508	50.199053
401.673911	117.935248	50.204058
398.148710	113.040668	50.209063
394.231490	116.621410	50.214068
391.326629	115.139111	50.219073
387.415408	121.398091	50.224077
383.857947	113.769253	50.229082
380.501794	118.680728	50.234087
376.970135	119.261321	50.239092
374.135472	111.797228	50.244097
369.952094	114.929294	50.249101
366.441676	123.370793	50.254106
363.185999	121.491519	50.259111
359.781579	123.116285	50.264116
356.372139	106.025408	50.269121
352.559327	113.307295	50.274125
349.154489	113.481130	50.279130
345.640051	114.883366	50.284135
341.691216	121.255763	50.289140
338.741920	122.632747	50.294145
334.802590	112.921331	50.299149
331.459934	119.165187	50.304154
328.298481	106.337967	50.309159
324.867484	119.175017	50.314164
321.157633	108.563477	50.319169
317.585583	116.150683	50.324173
313.882850	120.446658	50.329178
310.710693	119.686701	50.334183
307.092489	117.324803	50.339188
303.754926	114.106198	50.344193
299.699104	116.105233	50.349197
296.541348	120.494933	50.354202
293.031903	116.441247	50.359207
289.135181	119.800435	50.364212
285.804771	112.995079	50.369217
282.467879	118.989570	50.374221
279.039107	111.431683	50.379226
275.468052	110.993132	50.384231
272.261259	120.088531	50.389236
268.823960	119.036826	50.394241
264.722838	113.295022	50.399245
261.259844	119.392889	50.404250
258.355214	119.365201	50.409255
254.407552	122.835861	50.414260
250.891626	113.423856	50.419265
247.554987	117.822481	50.424269
243.953759	111.602293	50.429274
240.642996	111.888318	50.434279
237.064554	112.810661	50.439284
233.389751	109.104479	50.444289
229.822021	117.711259	50.449293
226.471690	117.873998	50.454298
223.417027	116.118637	50.459303
219.570163	121.214865	50.464308
216.405913	109.037042	50.469313
212.543667	124.399026	50.474317
208.428457	122.045487	50.479322
205.241352	111.048165	50.484327
201.800595	114.073636	50.489332
198.512443	108.853459	50.494337
194.860721	105.989072	50.499341
191.336422	115.119521	50.504346
187.713917	111.574824	50.509351
184.131747	116.622526	50.514356
181.105195	109.735383	50.519361
177.390098	122.031901	50.524365
174.036818	114.780895	50.529370
170.383012	115.706890	50.534375
166.733508	116.631584	50.539380
163.129125	113.932449	50.544385
160.172616	107.855628	50.549389
156.185140	120.536473	50.554394
152.865370	111.609300	50.559399
149.012940	113.147967	50.564404
145.988563	107.747806	50.569409
142.359474	122.035428	50.574413
138.769543	119.970918	50.579418
135.344668	108.635720	50.584423
131.728933	122.223165	50.589428
128.602651	114.481536	50.594433
124.883826	119.119351	50.599437
120.983518	110.680032	50.604442
118.307500	106.744065	50.609447
114.435229	108.024972	50.614452
111.024261	105.304716	50.619457
107.310029	117.317964	50.624461
103.673613	111.169838	50.629466
100.582652	110.335816	50.634471
96.662474	120.692999	50.639476
93.381808	108.961789	50.644481
89.869384	112.703105	50.649485
86.343361	107.420187	50.654490
82.910997	111.430441	50.659495
79.061046	109.850278	50.664500
75.910575	118.802687	50.669505
72.428886	114.412088	50.674509
68.671393	107.073986	50.679514
65.558349	99.577090	50.684519
61.874269	110.568115	50.689524
58.625717	107.309320	50.694529
54.912309	113.727241	50.699533
51.175234	104.335074	50.704538
47.506487	114.625403	50.709543
43.913579	104.119492	50.714548
40.454898	109.340245	50.719553
37.047188	113.523265	50.724557
33.840291	104.131733	50.729562
30.781324	102.777620	50.734567
26.610839	116.023251	50.739572
23.122669	99.969123	50.744577
19.659482	111.380038	50.749581
16.639525	103.409358	50.754586
13.123384	107.671917	50.759591
9.274592	110.407729	50.764596
5.777479	111.961688	50.769601
2.380634	121.192336	50.774605