Tue Jun 21 13:07:15 2022

Number of Points = 9931

Depth (nm)	Load (N)	Time (s)
-0.367865	83.087832	0.000000
-0.384852	81.293783	0.005005
-0.949293	73.507756	0.010010
-0.384319	78.477864	0.015014
-0.849224	69.458989	0.020019
-0.826676	61.138083	0.025024
-1.437250	51.340190	0.030029
-1.200906	42.214289	0.035034
-1.404683	35.465341	0.040038
-1.870961	26.291812	0.045043
-2.052167	14.111476	0.050048
-2.137827	5.462987	0.055053
-2.850159	1.232570	0.060058
-3.152021	-20.220576	0.065062
-3.445460	-10.647442	0.070067
-4.142501	-7.674965	0.075072
-4.504955	-13.062262	0.080077
-5.033886	-11.029894	0.085082
-5.014638	-9.237285	0.090086
-5.291091	-6.539284	0.095091
-5.528395	-12.659481	0.100096
-5.483884	-7.915202	0.105101
-5.750847	-9.367505	0.110106
-5.453222	-6.202364	0.115110
-6.111844	-5.817366	0.120115
-6.575583	-10.508080	0.125120
-6.839412	-10.312972	0.130125
-6.976264	-16.819801	0.135130
-6.997706	-7.388201	0.140134
-7.677540	-13.206804	0.145139
-8.434359	-13.596456	0.150144
-8.608875	-14.809310	0.155149
-8.816370	-5.365056	0.160154
-8.719795	-6.958069	0.165158
-8.808786	-3.523090	0.170163
-8.640453	-6.454854	0.175168
-8.801315	-6.942205	0.180173
-9.265657	-7.193020	0.185178
-9.494941	-5.961122	0.190182
-10.105338	1.279141	0.195187
-10.304395	-4.295253	0.200192
-9.886932	-11.411872	0.205197
-10.983702	-5.183115	0.210202
-11.375194	-14.812212	0.215206
-11.809903	-6.576887	0.220211
-11.680084	-15.717476	0.225216
-11.758937	-9.742724	0.230221
-12.045252	-10.303428	0.235226
-11.495492	-5.986766	0.240230
-12.614501	-9.831537	0.245235
-13.417832	-16.735936	0.250240
-13.431507	-8.206055	0.255245
-13.371139	-8.314653	0.260250
-12.958346	-3.573539	0.265254
-13.242938	0.290076	0.270259
-13.607980	-10.415909	0.275264
-14.365621	-18.149766	0.280269
-15.043061	2.171365	0.285274
-14.687891	-16.681787	0.290278
-15.335393	-9.442094	0.295283
-14.959307	-6.616731	0.300288
-15.424652	-11.072942	0.305293
-15.664200	-9.298060	0.310298
-16.001991	-11.429102	0.315302
-16.534540	-3.540469	0.320307
-16.285164	-6.556891	0.325312
-17.398704	-6.176677	0.330317
-17.783386	-5.965899	0.335322
-17.128661	-3.482675	0.340326
-17.817288	-2.626211	0.345331
-18.037121	-8.346741	0.350336
-18.065515	-9.792175	0.355341
-18.439788	-10.329631	0.360346
-18.034902	-7.689794	0.365350
-18.673239	-15.593380	0.370355
-19.240572	-3.884736	0.375360
-19.398371	-11.554928	0.380365
-19.497967	-8.341969	0.385370
-19.339608	-20.146148	0.390374
-19.557344	-9.546592	0.395379
-20.759578	-13.122624	0.400384
-21.005632	-14.900830	0.405389
-21.199165	-7.413473	0.410394
-20.993285	-13.245936	0.415398
-21.271436	-6.977504	0.420403
-21.103739	-15.995704	0.425408
-21.635293	-7.352044	0.430413
-22.111866	-6.913126	0.435418
-22.244893	-19.515217	0.440422
-22.659681	-6.269945	0.445427
-22.507371	-7.954871	0.450432
-23.130888	-12.722131	0.455437
-23.623459	-11.684222	0.460442
-23.688544	-17.295793	0.465446
-23.699220	-7.557152	0.470451
-23.984361	-11.142377	0.475456
-24.066988	-14.461585	0.480461
-24.720048	-3.220237	0.485466
-25.021508	-12.755116	0.490470
-25.323625	-3.080494	0.495475
-25.508718	-9.332274	0.500480
-25.794065	-11.323013	0.505485
-25.577832	-2.810679	0.510490
-25.421866	-12.275476	0.515494
-26.357687	-6.569267	0.520499
-26.342549	-8.139718	0.525504
-26.670177	-16.371020	0.530509
-26.961555	-6.344360	0.535514
-27.184924	-14.038027	0.540518
-28.279275	-0.759743	0.545523
-28.172927	-6.631769	0.550528
-28.491808	-10.535033	0.555533
-28.725417	-7.823999	0.560538
-28.373888	-20.562766	0.565542
-28.412678	-0.821786	0.570547
-28.615146	-11.420305	0.575552
-29.137540	-12.787882	0.580557
-29.937241	-8.455944	0.585562
-30.094261	-12.816197	0.590566
-30.292116	-8.671539	0.595571
-30.035060	-19.519603	0.600576
-30.526024	-17.690853	0.605581
-30.408811	1.835251	0.610586
-31.046803	-14.190821	0.615590
-32.245908	-6.407494	0.620595
-31.924742	-12.459144	0.625600
-31.783019	-8.980478	0.630605
-31.934208	-8.112962	0.635610
-32.000215	-8.806446	0.640614
-32.390397	-13.313580	0.645619
-32.813339	-12.602145	0.650624
-33.272633	-12.730460	0.655629
-33.856699	-11.704237	0.660634
-33.572997	-13.722114	0.665638
-33.805207	-10.883835	0.670643
-33.576686	-8.223675	0.675648
-34.230563	1.755670	0.680653
-34.937917	-7.575244	0.685658
-34.795462	-2.972294	0.690662
-34.932997	-7.450622	0.695667
-35.286727	-10.298105	0.700672
-35.649946	-7.076419	0.705677
-36.747028	-8.751189	0.710682
-36.430450	-12.017710	0.715686
-36.291070	-7.231324	0.720691
-36.696610	-12.740341	0.725696
-36.526841	-15.653793	0.730701
-36.903391	-9.803002	0.735706
-36.852926	-17.608711	0.740710
-37.931917	-7.698094	0.745715
-38.151715	-8.317172	0.750720
-38.415466	-9.125120	0.755725
-38.508715	-6.884090	0.760730
-38.442285	-1.173944	0.765734
-38.409174	-11.443841	0.770739
-39.206358	-4.150152	0.775744
-39.927996	-11.936735	0.780749
-39.939387	-6.864310	0.785754
-39.614142	-14.325988	0.790758
-40.017926	-5.866877	0.795763
-40.043272	-5.213191	0.800768
-39.913538	-11.699439	0.805773
-40.533936	-6.077626	0.810778
-40.943976	-7.947075	0.815782
-41.244242	-8.702998	0.820787
-41.787876	-1.792680	0.825792
-42.511239	-14.298987	0.830797
-42.723383	-12.446552	0.835802
-42.247751	-7.484970	0.840806
-42.646974	-6.885995	0.845811
-42.745471	-14.583960	0.850816
-42.950146	-3.279323	0.855821
-43.071972	-6.304328	0.860826
-43.438074	-8.594663	0.865830
-44.110600	-9.605264	0.870835
-44.712155	-2.474012	0.875840
-44.629504	-12.078022	0.880845
-44.975273	-4.910195	0.885850
-44.670835	-11.852995	0.890854
-44.867158	-11.601576	0.895859
-45.242507	-5.626861	0.900864
-46.011274	-6.510820	0.905869
-46.576043	-4.940783	0.910874
-46.522522	-12.906445	0.915878
-46.416917	-13.835152	0.920883
-46.383027	-9.630402	0.925888
-46.104115	-14.327664	0.930893
-46.760108	-11.615355	0.935898
-47.214812	-17.043213	0.940902
-47.902730	-7.809681	0.945907
-48.159267	-5.785515	0.950912
-47.857685	-7.453129	0.955917
-48.246891	1.315556	0.960922
-48.622060	-9.267386	0.965926
-49.357462	1.306013	0.970931
-49.571890	-9.983360	0.975936
-49.609388	-12.325546	0.980941
-49.951710	-8.447043	0.985946
-49.562085	-2.928553	0.990950
-49.390265	-8.968694	0.995955
-50.264171	-9.643039	1.000960
-50.685523	-14.467056	1.005965
-51.234902	-9.670411	1.010970
-51.179925	-9.300768	1.015974
-51.509373	-4.155545	1.020979
-51.692301	-5.655702	1.025984
-51.194248	-9.140927	1.030989
-52.495560	-13.709505	1.035994
-52.432464	-17.014560	1.040998
-52.805520	-11.613280	1.046003
-53.381001	-14.864682	1.051008
-52.833770	-14.270100	1.056013
-52.648711	-7.463684	1.061018
-53.324327	-23.228159	1.066022
-53.820376	-20.941740	1.071027
-53.776722	-6.930764	1.076032
-54.654423	-11.725780	1.081037
-55.651660	-9.211913	1.086042
-54.856062	-10.476687	1.091046
-55.210787	-13.031949	1.096051
-55.751217	-14.422977	1.101056
-55.499152	-11.696073	1.106061
-56.211070	-11.099778	1.111066
-55.676753	-13.956187	1.116070
-56.159888	-8.221339	1.121075
-57.085763	0.564785	1.126080
-57.183646	3.132380	1.131085
-57.800141	-7.287264	1.136090
-57.540632	-8.175747	1.141094
-57.925196	-9.602651	1.146099
-57.803579	-7.644857	1.151104
-57.329485	-13.837272	1.156109
-58.145314	-9.468127	1.161114
-59.003940	-16.292909	1.166118
-59.334441	-5.695399	1.171123
-59.133141	-11.046598	1.176128
-59.013707	-6.421684	1.181133
-59.530022	-2.158969	1.186138
-59.581514	-11.089762	1.191142
-60.514907	-7.818052	1.196147
-60.884954	-12.061131	1.201152
-60.535628	-15.171459	1.206157
-60.942397	-3.393106	1.211162
-60.728761	-9.865227	1.216166
-61.215071	-8.563926	1.221171
-62.065667	-8.042146	1.226176
-62.431543	-14.765405	1.231181
-62.503817	-0.513819	1.236186
-62.510829	-11.659148	1.241190
-62.551085	-5.025578	1.246195
-62.583897	-8.710997	1.251200
-62.771191	-9.009067	1.256205
-63.794882	-6.277697	1.261210
-63.870547	-6.056324	1.266214
-64.051144	-4.038418	1.271219
-64.275627	-8.690403	1.276224
-64.317525	-7.555641	1.281229
-64.728020	5.091206	1.286234
-64.197605	-11.065402	1.291238
-65.226274	-9.403937	1.296243
-65.647696	-9.272515	1.301248
-65.468746	-7.289683	1.306253
-65.791218	-6.601789	1.311258
-65.830860	-8.244272	1.316262
-66.529670	-5.717663	1.321267
-67.049941	-7.886363	1.326272
-66.920368	-8.727280	1.331277
-67.080110	-6.993239	1.336282
-66.984139	-10.915866	1.341286
-67.817018	-0.772297	1.346291
-68.369967	-5.499338	1.351296
-68.471560	-5.925856	1.356301
-68.784970	0.528978	1.361306
-68.783377	-12.153026	1.366310
-68.740132	-5.198412	1.371315
-68.789139	-0.317682	1.376320
-69.167778	-5.251979	1.381325
-70.027563	-5.123145	1.386330
-69.969452	-8.552879	1.391334
-70.422390	-12.726779	1.396339
-70.170052	-5.015486	1.401344
-70.364624	-8.011472	1.406349
-70.794138	1.204730	1.411354
-71.482517	-4.692367	1.416358
-71.651624	1.972410	1.421363
-71.731580	-6.955051	1.426368
-71.605593	-3.327557	1.431373
-71.968501	-3.334091	1.436378
-72.714279	-15.863118	1.441382
-73.201105	-5.420871	1.446387
-73.445152	-8.524695	1.451392
-72.914985	-3.259967	1.456397
-73.424227	0.254080	1.461402
-73.130232	-5.319671	1.466406
-73.771308	-0.131521	1.471411
-74.641172	-6.738165	1.476416
-75.054344	-6.612845	1.481421
-74.893540	-2.069571	1.486426
-75.078567	-6.739732	1.491430
-75.260562	-1.308522	1.496435
-75.483955	-7.908167	1.501440
-75.445262	-6.837466	1.506445
-75.822824	-6.033692	1.511450
-75.883680	-10.991604	1.516454
-76.315959	-4.273380	1.521459
-76.742482	-4.038499	1.526464
-76.836459	-9.288110	1.531469
-77.429034	2.302767	1.536474
-77.507061	-7.945171	1.541478
-78.145108	-11.792810	1.546483
-78.258529	-2.916078	1.551488
-78.055812	-9.489595	1.556493
-78.515354	-6.500200	1.561498
-78.440776	-11.882311	1.566502
-78.626136	-9.653062	1.571507
-79.424412	-2.972892	1.576512
-79.865305	-9.067061	1.581517
-80.229065	-11.269177	1.586522
-80.040252	-0.932899	1.591526
-80.038575	-3.839038	1.596531
-80.012056	-8.282963	1.601536
-79.867997	-7.447568	1.606541
-81.033448	-2.212636	1.611546
-81.302512	-0.620131	1.616550
-81.319204	-1.889706	1.621555
-81.619372	-4.920497	1.626560
-82.070387	-3.016660	1.631565
-83.032932	-4.262990	1.636570
-83.164133	-15.721240	1.641574
-82.461188	-9.373948	1.646579
-83.013061	-7.351783	1.651584
-83.311145	0.840201	1.656589
-83.340016	3.329866	1.661594
-83.380692	-7.282614	1.666598
-83.685852	-4.021996	1.671603
-84.373252	-3.337602	1.676608
-84.945357	-12.818177	1.681613
-85.198872	-6.344257	1.686618
-84.968091	-14.561862	1.691622
-85.109615	-5.264697	1.696627
-84.998137	-10.335410	1.701632
-85.164996	-12.488636	1.706637
-85.980891	-8.136841	1.711642
-85.959326	-19.132974	1.716646
-86.194441	-4.116994	1.721651
-87.183622	-9.374836	1.726656
-87.257867	-10.650270	1.731661
-88.226800	-2.493018	1.736666
-87.444331	-9.653512	1.741670
-87.749292	-0.295139	1.746675
-88.392561	-9.588304	1.751680
-88.181381	-13.989006	1.756685
-88.452825	7.200643	1.761690
-88.086790	-8.535064	1.766694
-88.927652	1.402631	1.771699
-89.651856	-5.686538	1.776704
-89.478934	-11.858480	1.781709
-89.890582	-9.515191	1.786714
-89.920396	-6.233474	1.791718
-89.682130	-4.079709	1.796723
-90.269830	-8.751459	1.801728
-90.782608	-9.704050	1.806733
-91.516589	3.144367	1.811738
-91.323227	-13.236236	1.816742
-91.704744	0.001949	1.821747
-91.662286	-11.025079	1.826752
-91.424341	-9.985404	1.831757
-92.234284	-0.871170	1.836762
-91.959854	-3.043607	1.841766
-92.405048	-4.167625	1.846771
-93.070488	-8.910169	1.851776
-93.667765	-4.165969	1.856781
-94.430827	-7.608497	1.861786
-94.137763	-8.951669	1.866790
-93.501365	-10.135423	1.871795
-94.400063	-12.828512	1.876800
-94.390870	-8.913503	1.881805
-94.525914	-2.077757	1.886810
-94.420745	-3.987533	1.891814
-95.751528	-2.047910	1.896819
-96.298650	4.980601	1.901824
-95.994297	1.541658	1.906829
-96.220995	5.422132	1.911834
-96.072992	-1.017613	1.916838
-95.866024	-2.564383	1.921843
-96.166818	-9.079574	1.926848
-96.913071	-5.710977	1.931853
-97.514713	-6.470264	1.936858
-97.375756	-13.899117	1.941862
-97.625282	-10.245154	1.946867
-98.024599	-2.597227	1.951872
-98.656022	-6.140686	1.956877
-99.202708	-3.592300	1.961882
-99.157243	-14.068475	1.966886
-99.227510	-6.989886	1.971891
-99.266917	-3.546544	1.976896
-99.011091	-12.366611	1.981901
-99.262306	-0.720184	1.986906
-99.583437	-10.271922	1.991910
-100.384227	-1.230639	1.996915
-100.592362	-9.530924	2.006912
-100.551819	-5.486806	2.016909
-99.768363	-1.573824	2.026906
-99.709625	-8.145637	2.036902
-98.266471	-9.397533	2.046899
-98.085843	-4.589630	2.056896
-97.974183	-6.909273	2.066893
-97.222857	-4.830294	2.076890
-96.376898	-5.719708	2.086886
-96.311104	1.645993	2.096883
-96.072156	-3.546683	2.106880
-95.440227	-2.540184	2.116877
-94.841169	-4.181421	2.126874
-93.659698	-5.488969	2.136870
-93.350303	-1.629067	2.146867
-93.470229	-7.766241	2.156864
-93.285989	-3.305699	2.166861
-92.473499	-7.829492	2.176858
-91.958544	-8.685228	2.186854
-91.098861	-8.258820	2.196851
-90.739936	-6.510816	2.206848
-90.543585	-0.246740	2.216845
-89.664972	-6.740547	2.226842
-89.439772	0.274517	2.236838
-88.384442	-5.284930	2.246835
-87.693850	-5.798688	2.256832
-87.609787	-8.835738	2.266829
-87.707780	-0.231120	2.276826
-86.768371	-7.979389	2.286822
-86.315521	-9.708442	2.296819
-85.526152	-6.337821	2.306816
-84.632040	-8.128887	2.316813
-84.989987	-5.166352	2.326810
-84.809964	-8.376967	2.336806
-83.595896	-8.749205	2.346803
-83.040618	-2.209663	2.356800
-82.819069	-7.240597	2.366797
-81.641392	1.805188	2.376794
-81.415275	1.371119	2.386790
-81.490512	0.121136	2.396787
-81.319840	-8.747972	2.406784
-80.417722	2.313576	2.416781
-79.497410	0.212111	2.426778
-78.690391	0.878222	2.436774
-78.388284	-2.409913	2.446771
-78.231190	-0.937308	2.456768
-78.145193	-0.180836	2.466765
-77.263927	0.917349	2.476762
-76.903305	-2.739884	2.486758
-75.745183	2.729483	2.496755
-75.446338	1.192498	2.506752
-75.180431	-3.539328	2.516749
-74.979702	-0.361277	2.526746
-74.418187	0.612233	2.536742
-74.079163	1.856925	2.546739
-72.658659	-1.211767	2.556736
-72.292145	0.292940	2.566733
-72.390747	9.166184	2.576730
-72.034442	-1.050580	2.586726
-71.044932	0.513174	2.596723
-70.688127	3.938640	2.606720
-70.356375	3.417725	2.616717
-69.094161	1.590202	2.626714
-69.021153	6.999404	2.636710
-69.084737	5.678137	2.646707
-68.471766	-3.785057	2.656704
-67.997788	2.213725	2.666701
-67.097774	3.775901	2.676698
-66.402132	6.619480	2.686694
-66.103620	1.451911	2.696691
-65.946320	2.630079	2.706688
-65.014661	8.086966	2.716685
-64.913056	5.679282	2.726682
-64.047072	11.161667	2.736678
-63.134684	3.926062	2.746675
-63.039125	2.043378	2.756672
-62.964003	5.213583	2.766669
-62.087015	-2.121866	2.776666
-61.546676	2.527284	2.786662
-61.492945	-3.477423	2.796659
-60.450759	3.143315	2.806656
-59.997575	0.053829	2.816653
-59.915447	8.606891	2.826650
-59.247184	1.792266	2.836646
-58.524440	5.848486	2.846643
-58.212927	3.717832	2.856640
-57.363537	3.044017	2.866637
-56.628685	3.484190	2.876634
-56.384263	3.837236	2.886630
-56.551883	3.060949	2.896627
-56.262443	-5.289803	2.906624
-55.217147	1.145677	2.916621
-54.185669	0.694223	2.926618
-53.937727	0.518935	2.936614
-54.037583	-0.879904	2.946611
-53.176453	-2.674394	2.956608
-52.354235	0.428600	2.966605
-51.937967	3.396492	2.976602
-51.802198	-0.534110	2.986598
-51.223375	-1.675261	2.996595
-50.330726	-4.494907	3.006592
-50.519246	-1.447807	3.016589
-49.591195	0.007183	3.026586
-49.020720	2.247912	3.036582
-48.449242	2.650925	3.046579
-48.253654	-0.730415	3.056576
-47.251136	1.490140	3.066573
-47.168877	6.976253	3.076570
-47.215503	3.942467	3.086566
-46.132479	2.889918	3.096563
-45.769122	-1.293148	3.106560
-44.524690	2.982349	3.116557
-44.067293	7.012174	3.126554
-44.037249	-0.529981	3.136550
-44.120566	5.957848	3.146547
-43.374288	11.568339	3.156544
-42.641949	1.830686	3.166541
-42.379231	-4.391001	3.176538
-41.334437	0.696439	3.186534
-41.242626	3.230618	3.196531
-40.664734	3.234435	3.206528
-39.615372	-1.462541	3.216525
-39.776611	10.143219	3.226522
-39.421419	4.274515	3.236518
-38.249652	0.657624	3.246515
-37.852513	-1.892654	3.256512
-37.793814	-1.978315	3.266509
-36.791811	0.156377	3.276506
-36.335461	4.843942	3.286502
-36.150504	0.634107	3.296499
-36.001198	-0.431766	3.306496
-35.135363	1.341171	3.316493
-34.726043	5.301900	3.326490
-34.121328	-2.025010	3.336486
-33.231896	-6.232952	3.346483
-32.959376	-3.288082	3.356480
-32.496067	1.109855	3.366477
-32.066200	2.425655	3.376474
-31.946094	0.813156	3.386470
-31.176960	-0.608663	3.396467
-30.138792	-2.655540	3.406464
-29.879388	6.413110	3.416461
-29.990396	0.131990	3.426458
-29.343844	4.632559	3.436454
-28.273081	-2.307990	3.446451
-27.978502	-1.096241	3.456448
-27.245719	-1.487162	3.466445
-26.778144	-3.529847	3.476442
-26.835136	-0.784901	3.486438
-26.733874	5.361165	3.496435
-25.507933	2.029116	3.506432
-24.896499	-7.750352	3.516429
-24.180295	-4.441499	3.526426
-23.871073	-4.926275	3.536422
-23.538900	-5.626467	3.546419
-23.331565	-9.163472	3.556416
-22.149301	-1.638650	3.566413
-21.805288	-8.433559	3.576410
-21.748076	-2.097039	3.586406
-21.377367	-9.662408	3.596403
-20.235117	-5.806847	3.606400
-20.526014	-8.644090	3.616397
-19.463184	-4.441852	3.626394
-18.713523	1.007246	3.636390
-18.490111	-6.081657	3.646387
-18.534835	-7.208461	3.656384
-17.722412	-4.369789	3.666381
-16.901412	-3.960275	3.676378
-16.344317	-2.399985	3.686374
-15.844961	-0.390309	3.696371
-15.678775	2.434257	3.706368
-15.102069	-2.353579	3.716365
-14.629874	6.255027	3.726362
-14.434795	-3.657036	3.736358
-13.261666	-2.356431	3.746355
-12.482849	-5.841065	3.756352
-12.589231	-2.188925	3.766349
-12.416774	-8.861572	3.776346
-11.142543	-8.085504	3.786342
-11.042786	-1.243688	3.796339
-10.881976	-7.868171	3.806336
-9.629724	-4.491394	3.816333
-9.500418	-2.420835	3.826330
-9.249901	-4.478355	3.836326
-8.291422	2.255844	3.846323
-7.678275	2.453192	3.856320
-7.692156	-2.207803	3.866317
-7.031769	-0.940446	3.876314
-6.202593	0.600477	3.886310
-5.633582	0.160608	3.896307
-5.819434	-1.230315	3.906304
-5.579845	1.437068	3.916301
-4.684780	-2.440450	3.926298
-3.576313	6.050349	3.936294
-3.204340	14.870180	3.946291
-2.884356	16.378452	3.956288
-3.125211	17.997968	3.966285
-2.609627	29.720476	3.976282
-1.827910	44.956271	3.986278
-1.597294	65.388387	3.996275
-0.859570	74.963721	4.006272
-0.762677	92.552809	4.016269
-0.321213	117.062064	4.026266
0.000000	137.520102	4.031270
0.238216	154.645523	4.036275
0.520579	166.566824	4.041280
0.162656	170.918202	4.046285
0.513043	179.172413	4.051290
0.474451	193.493201	4.056294
0.972220	192.586767	4.061299
1.118420	189.963119	4.066304
0.669815	208.656694	4.071309
1.416752	218.875848	4.076314
0.907289	226.543309	4.081318
0.819700	227.847075	4.086323
1.259622	214.228158	4.091328
1.052861	238.524151	4.096333
1.085451	223.298475	4.101338
1.005476	234.160734	4.106342
1.076599	235.662789	4.111347
1.349312	239.195402	4.116352
1.401119	248.549316	4.121357
1.746030	247.845596	4.126362
1.410750	235.784135	4.131366
1.403468	226.636899	4.136371
1.254577	234.524282	4.141376
1.351184	247.593131	4.146381
1.870512	255.255618	4.151386
1.370768	242.121827	4.156390
1.169878	245.696753	4.161395
1.490865	248.639627	4.166400
1.319513	264.031899	4.171405
1.488774	263.223470	4.176410
1.712697	261.417333	4.181414
1.728775	261.622334	4.186419
1.724417	265.302462	4.191424
1.447015	266.226412	4.196429
1.770748	267.566857	4.201434
1.337574	268.631649	4.206438
1.536575	268.468519	4.211443
1.692212	269.446862	4.216448
1.547896	263.689846	4.221453
1.717697	262.703724	4.226458
1.569100	268.228168	4.231462
1.515718	263.727140	4.236467
1.980672	258.210236	4.241472
1.305572	270.414682	4.246477
1.614717	261.896234	4.251482
1.856977	271.939298	4.256486
1.758807	264.981543	4.261491
1.834807	269.002387	4.266496
1.759399	274.542341	4.271501
1.713504	266.687519	4.276506
1.904789	265.111355	4.281510
1.915018	256.279900	4.286515
1.797498	256.588129	4.291520
1.708654	265.225330	4.296525
1.800484	259.005532	4.301530
1.997064	263.150464	4.306534
1.775518	269.255514	4.311539
2.084934	267.678930	4.316544
2.136889	275.530117	4.321549
1.562558	268.333889	4.326554
1.711936	270.484856	4.331558
1.605398	269.174881	4.336563
1.716049	258.409473	4.341568
1.713679	278.894268	4.346573
1.711647	272.020641	4.351578
1.872466	278.250835	4.356582
1.905547	283.057087	4.361587
1.988071	295.410594	4.366592
1.871369	301.191239	4.371597
2.005223	302.253704	4.376602
2.175459	304.124357	4.381606
2.020171	304.444958	4.386611
2.281216	299.770492	4.391616
1.972760	305.553883	4.396621
2.147290	310.187138	4.401626
2.118020	308.466534	4.406630
2.107469	309.385766	4.411635
1.878115	307.183835	4.416640
1.934590	308.826655	4.421645
1.975072	301.141431	4.426650
1.983978	309.335631	4.431654
2.073153	307.457277	4.436659
2.184642	293.824594	4.441664
1.977310	306.198874	4.446669
1.914393	307.515334	4.451674
2.117662	306.639110	4.456678
2.020063	309.364382	4.461683
2.454336	301.433781	4.466688
2.214933	307.106280	4.471693
2.145180	302.798579	4.476698
2.226796	313.013906	4.481702
2.078598	311.221824	4.486707
2.432238	309.120100	4.491712
2.265222	324.653797	4.496717
2.511972	319.264569	4.501722
2.255310	326.476006	4.506726
2.356203	318.670458	4.511731
2.510303	324.853042	4.516736
2.106578	326.041625	4.521741
2.299679	321.715653	4.526746
2.554335	329.597831	4.531750
2.624183	335.268861	4.536755
2.655232	338.679698	4.541760
2.430836	328.645602	4.546765
2.378251	311.750457	4.551770
2.242698	330.752087	4.556774
2.243640	342.382676	4.561779
2.723098	335.348777	4.566784
2.662531	349.723078	4.571789
2.750524	340.687478	4.576794
2.664216	336.532486	4.581798
2.472354	337.932265	4.586803
2.345259	323.342903	4.591808
2.434974	343.020028	4.596813
2.389499	337.724372	4.601818
2.423349	334.014411	4.606822
2.556239	339.094831	4.611827
2.923823	332.487947	4.616832
2.487709	343.756570	4.621837
2.440316	339.768198	4.626842
2.431364	330.914421	4.631846
2.406086	337.846008	4.636851
2.710136	339.607482	4.641856
2.414667	342.653440	4.646861
2.340456	339.666261	4.651866
2.518112	340.842839	4.656870
2.617210	354.294003	4.661875
3.052842	359.328837	4.666880
2.978401	357.968547	4.671885
2.681680	346.289568	4.676890
2.834265	343.264045	4.681894
2.489954	339.768060	4.686899
2.713884	358.407480	4.691904
2.982026	364.075483	4.696909
3.114220	352.631745	4.701914
2.935366	349.664260	4.706918
2.449949	344.221617	4.711923
2.808264	361.567145	4.716928
2.741883	367.172732	4.721933
2.828842	361.940981	4.726938
2.918842	371.597675	4.731942
3.100992	367.883081	4.736947
2.936376	365.716401	4.741952
2.735648	373.197831	4.746957
2.994790	369.170928	4.751962
2.803313	369.666444	4.756966
2.820814	373.149389	4.761971
3.106653	367.346168	4.766976
2.487123	379.726008	4.771981
2.734700	365.414381	4.776986
2.536043	364.005196	4.781990
2.677714	371.441176	4.786995
2.491130	376.030646	4.792000
2.713384	389.859478	4.797005
2.960088	402.440648	4.802010
3.099922	390.287961	4.807014
2.955150	401.841687	4.812019
3.365330	387.268874	4.817024
2.975257	401.649832	4.822029
2.939582	394.289558	4.827034
3.010653	401.624169	4.832038
3.266818	402.428201	4.837043
3.316280	403.830255	4.842048
3.304396	398.777663	4.847053
3.177983	394.020705	4.852058
2.952045	398.468299	4.857062
2.976919	394.935244	4.862067
3.451986	396.473042	4.867072
3.184482	400.294261	4.872077
3.291324	405.528401	4.877082
2.927685	407.983382	4.882086
3.243555	421.242614	4.887091
3.741912	427.128468	4.892096
3.565313	425.536046	4.897101
3.436275	414.848306	4.902106
3.330452	411.174874	4.907110
3.425886	412.279624	4.912115
3.420959	403.079402	4.917120
3.384233	413.933244	4.922125
3.403155	397.364404	4.927130
3.047340	409.059249	4.932134
3.315005	429.514329	4.937139
3.730592	428.486314	4.942144
3.495143	432.001291	4.947149
3.384113	414.803522	4.952154
3.413683	427.806069	4.957158
3.301216	434.200773	4.962163
4.028920	435.224312	4.967168
3.510749	421.873583	4.972173
3.782802	409.791538	4.977178
3.132577	416.897884	4.982182
3.629578	423.237840	4.987187
3.811911	431.074620	4.992192
3.349931	422.718900	4.997197
3.768064	421.029380	5.002202
3.508418	423.490232	5.007206
3.213477	428.290657	5.012211
3.723432	425.871762	5.017216
3.707886	440.112197	5.022221
3.675891	436.766549	5.027226
3.917173	446.377914	5.032230
3.825785	434.257363	5.037235
3.990177	424.848723	5.042240
3.645195	419.170857	5.047245
3.879461	405.532349	5.052250
3.719978	402.616901	5.057254
3.869213	404.348961	5.062259
4.005147	407.694689	5.067264
3.521825	399.074925	5.072269
3.450036	403.924234	5.077274
3.652862	405.000544	5.082278
3.816172	422.481245	5.087283
3.895227	422.832901	5.092288
3.964046	439.014202	5.097293
4.074142	434.844619	5.102298
4.032187	413.668114	5.107302
3.813089	409.347817	5.112307
4.055313	403.469120	5.117312
3.330455	407.630901	5.122317
4.033542	416.228815	5.127322
4.167252	429.337653	5.132326
3.894951	424.762714	5.137331
3.720296	420.225283	5.142336
3.727954	430.631328	5.147341
4.226155	437.073904	5.152346
4.071626	437.201186	5.157350
3.772476	446.139917	5.162355
4.283674	434.169811	5.167360
4.252820	433.249269	5.172365
3.892838	428.882042	5.177370
3.867212	432.186644	5.182374
3.901928	444.423862	5.187379
4.584145	436.383463	5.192384
4.120515	443.949507	5.197389
4.084266	437.458981	5.202394
4.013010	438.943585	5.207398
3.998480	440.138574	5.212403
4.236465	432.691922	5.217408
3.795667	436.669523	5.222413
4.133092	441.881873	5.227418
3.845597	440.831945	5.232422
4.056493	436.394063	5.237427
4.251514	435.554916	5.242432
3.922669	452.408305	5.247437
3.797179	440.818712	5.252442
3.862651	441.935727	5.257446
3.841407	443.714373	5.262451
4.315513	455.661968	5.267456
4.430094	463.234498	5.272461
4.453435	444.125318	5.277466
4.244000	442.422691	5.282470
3.676060	441.832626	5.287475
4.251785	454.508150	5.292480
4.362062	462.210255	5.297485
4.578109	472.981235	5.302490
4.246204	478.490324	5.307494
4.045440	467.167152	5.312499
4.360186	468.068247	5.317504
3.943851	474.612940	5.322509
4.162072	478.893471	5.327514
4.569169	469.956316	5.332518
3.783241	474.594145	5.337523
4.135873	469.231338	5.342528
4.275093	480.384070	5.347533
4.432535	491.414600	5.352538
4.394329	503.232950	5.357542
4.207987	508.410491	5.362547
4.364404	497.663585	5.367552
4.511938	512.199733	5.372557
4.612640	505.324185	5.377562
4.311931	510.231364	5.382566
4.265206	502.993838	5.387571
4.382074	497.193289	5.392576
4.934487	510.994990	5.397581
4.545372	509.534446	5.402586
4.473263	504.320500	5.407590
4.623486	509.669054	5.412595
4.729237	498.659195	5.417600
4.585324	506.672979	5.422605
4.780173	501.299188	5.427610
4.859199	502.973816	5.432614
4.546808	500.970514	5.437619
4.912878	500.179016	5.442624
4.692910	495.577235	5.447629
4.707440	501.005680	5.452634
4.248763	505.220304	5.457638
4.609687	510.309395	5.462643
4.862281	503.102426	5.467648
4.571561	507.257664	5.472653
4.613637	505.147121	5.477658
4.486622	500.981064	5.482662
4.740895	512.965697	5.487667
5.065597	513.806734	5.492672
4.898144	512.099516	5.497677
4.977913	502.739573	5.502682
4.985077	500.150736	5.507686
4.541477	508.369057	5.512691
4.893338	508.652651	5.517696
4.981721	516.607056	5.522701
4.793450	520.551151	5.527706
5.016927	524.860820	5.532710
4.906774	536.697425	5.537715
4.943804	536.160513	5.542720
5.132447	533.798163	5.547725
5.104667	528.539374	5.552730
4.884199	518.942008	5.557734
5.056499	518.648317	5.562739
5.161040	518.422088	5.567744
4.876324	511.240544	5.572749
5.196798	506.343641	5.577754
5.149648	509.977433	5.582758
4.851479	504.002879	5.587763
5.035960	508.905494	5.592768
5.155907	535.516720	5.597773
4.914254	525.735581	5.602778
4.939135	525.706661	5.607782
5.091927	540.588888	5.612787
5.536894	527.014449	5.617792
4.989120	537.732769	5.622797
5.284002	536.132912	5.627802
5.143707	535.466307	5.632806
4.965161	539.060689	5.637811
4.989075	533.146063	5.642816
5.027864	534.099173	5.647821
5.212323	527.209154	5.652826
5.417454	532.787602	5.657830
5.030240	544.746264	5.662835
4.955905	537.791741	5.667840
5.001399	532.421556	5.672845
4.989469	532.871755	5.677850
5.023779	531.982450	5.682854
4.806068	538.023032	5.687859
5.201527	553.113934	5.692864
5.527934	568.953353	5.697869
5.155940	573.511814	5.702874
5.425243	572.634114	5.707878
5.136957	583.966445	5.712883
5.694152	570.069874	5.717888
5.400741	565.513781	5.722893
5.590602	572.814792	5.727898
5.427558	576.250913	5.732902
5.326325	581.923327	5.737907
5.460148	575.364916	5.742912
5.098897	581.866392	5.747917
5.697554	577.064107	5.752922
5.600288	575.446101	5.757926
5.166010	580.405809	5.762931
4.983910	571.804745	5.767936
5.119266	577.627230	5.772941
5.187121	568.740075	5.777946
5.437108	571.877901	5.782950
5.370661	576.303477	5.787955
5.369912	566.205751	5.792960
5.511545	576.900717	5.797965
5.763987	595.815137	5.802970
6.028265	590.726028	5.807974
5.784572	583.713685	5.812979
5.807667	577.122694	5.817984
5.411596	573.733502	5.822989
5.603351	574.328766	5.827994
5.936155	576.321131	5.832998
5.633598	581.147334	5.838003
5.832362	580.711713	5.843008
5.386705	572.227306	5.848013
5.356735	570.287740	5.853018
5.571708	583.646110	5.858022
5.790136	593.050591	5.863027
5.940056	604.933775	5.868032
5.698914	605.563228	5.873037
5.663435	601.740753	5.878042
6.020751	604.310232	5.883046
5.744095	605.689936	5.888051
6.069307	606.400254	5.893056
5.761027	608.391425	5.898061
5.416983	612.473625	5.903066
5.335995	605.049515	5.908070
5.369974	608.817113	5.913075
5.498047	600.742881	5.918080
5.924690	610.458833	5.923085
5.955090	604.944497	5.928090
6.222887	600.276125	5.933094
5.851033	606.220301	5.938099
6.057714	596.985911	5.943104
5.762103	608.547599	5.948109
5.946170	606.088903	5.953114
6.251565	600.707825	5.958118
5.744473	610.512480	5.963123
6.036777	599.396669	5.968128
6.155790	604.731084	5.973133
5.882165	610.149264	5.978138
5.658351	615.527426	5.983142
5.793580	612.593134	5.988147
6.065114	630.707966	5.993152
6.141317	644.013983	5.998157
6.534375	634.939143	6.003162
6.610742	618.270961	6.008166
6.092257	615.931558	6.013171
6.300221	609.547343	6.018176
6.110227	609.068939	6.023181
5.716166	607.429230	6.028186
6.303903	604.792589	6.033190
5.955588	610.227873	6.038195
6.244765	617.275058	6.043200
6.633835	616.162027	6.048205
6.220001	612.515079	6.053210
5.993417	615.697096	6.058214
5.927631	618.482276	6.063219
6.207471	616.662301	6.068224
6.324833	615.868566	6.073229
6.221607	604.103280	6.078234
6.501952	601.838021	6.083238
6.200152	607.433539	6.088243
6.192374	605.429908	6.093248
6.223056	610.037146	6.098253
6.067014	613.092827	6.103258
6.133641	597.756556	6.108262
5.917440	599.270504	6.113267
6.212237	602.595692	6.118272
5.864350	610.900441	6.123277
5.919529	613.869048	6.128282
6.291035	630.417804	6.133286
6.228914	648.104815	6.138291
6.469316	633.165400	6.143296
6.004428	632.720674	6.148301
6.252176	626.148113	6.153306
6.237968	621.739560	6.158310
5.940133	614.937258	6.163315
6.197991	620.853143	6.168320
6.498373	631.697495	6.173325
6.308511	622.071118	6.178330
6.700242	607.975364	6.183334
6.210331	619.234346	6.188339
6.619272	613.903213	6.193344
6.385086	611.983249	6.198349
6.065888	609.420808	6.203354
6.244848	607.028870	6.208358
6.013565	606.783654	6.213363
6.202094	607.472401	6.218368
6.144018	610.401348	6.223373
6.023257	606.985505	6.228378
6.078297	602.174361	6.233382
5.829121	609.541773	6.238387
5.797449	609.540767	6.243392
5.801070	610.722305	6.248397
6.134017	632.954360	6.253402
6.251722	636.435375	6.258406
6.089907	646.000141	6.263411
6.307955	633.287282	6.268416
6.051904	638.925558	6.273421
6.294843	639.319546	6.278426
6.440418	634.453538	6.283430
6.103432	631.034222	6.288435
6.111046	614.658443	6.293440
6.139009	619.230218	6.298445
6.227467	621.637407	6.303450
6.345249	617.011236	6.308454
6.230475	613.794702	6.313459
6.063697	602.112365	6.318464
5.780056	610.241103	6.323469
6.165099	637.921216	6.328474
6.446504	640.762578	6.333478
6.273519	642.320683	6.338483
6.499141	624.843150	6.343488
5.930541	615.333168	6.348493
6.255831	617.204629	6.353498
6.382756	614.067266	6.358502
6.237877	614.912655	6.363507
6.303126	604.541511	6.368512
6.193035	611.167769	6.373517
6.411771	606.363066	6.378522
6.371660	610.837771	6.383526
5.914483	616.609591	6.388531
6.373381	608.458669	6.393536
6.174410	608.797560	6.398541
5.911858	612.460138	6.403546
6.098850	609.086479	6.408550
6.175322	612.714232	6.413555
6.259569	608.077632	6.418560
6.351451	613.927656	6.423565
6.252888	610.119769	6.428570
6.259643	610.706792	6.433574
5.860712	613.886760	6.438579
6.337423	603.678570	6.443584
6.200958	617.023923	6.448589
6.191351	607.244369	6.453594
6.310505	616.839357	6.458598
5.925480	613.973057	6.463603
6.152893	611.680251	6.468608
6.012276	609.903258	6.473613
6.081110	614.875773	6.478618
6.158259	611.405845	6.483622
5.934398	617.813346	6.488627
6.128760	614.459187	6.493632
6.145270	617.525567	6.498637
5.921602	621.404901	6.503642
5.884199	630.406368	6.508646
6.650944	642.292823	6.513651
6.356740	635.100359	6.518656
5.994773	635.971829	6.523661
6.136868	638.934929	6.528666
6.208054	630.435555	6.533670
5.906430	643.117386	6.538675
6.462822	642.586827	6.543680
6.283021	643.605345	6.548685
6.082486	639.281712	6.553690
6.309070	636.968517	6.558694
6.062018	630.250944	6.563699
6.054946	625.579139	6.568704
6.306310	643.571818	6.573709
5.904800	642.349728	6.578714
6.360270	634.597792	6.583718
6.223726	653.818240	6.588723
6.167553	649.068518	6.593728
6.453881	641.893196	6.598733
6.315821	628.890408	6.603738
6.294567	623.331732	6.608742
6.289652	615.391603	6.613747
6.324483	615.950690	6.618752
6.210500	614.090547	6.623757
6.054139	613.474356	6.628762
6.295438	609.640583	6.633766
5.632688	625.801132	6.638771
6.021414	612.420643	6.643776
5.986057	634.624685	6.648781
6.520906	636.051373	6.653786
6.452178	622.197225	6.658790
6.099884	623.434937	6.663795
6.206473	613.712509	6.668800
6.213645	609.512955	6.673805
6.042409	616.092506	6.678810
6.327092	613.647737	6.683814
6.136196	611.978924	6.688819
6.262369	619.250837	6.693824
6.065270	611.958434	6.698829
5.937324	615.592803	6.703834
6.250192	611.993855	6.708838
5.922998	622.826675	6.713843
6.111618	634.564151	6.718848
5.994316	636.774918	6.723853
6.090615	646.160778	6.728858
6.641769	648.773157	6.733862
6.115320	642.838322	6.738867
6.428903	650.302016	6.743872
6.348754	628.181934	6.748877
6.163863	622.848880	6.753882
6.554433	617.225961	6.758886
5.758432	618.573849	6.763891
6.183818	611.018131	6.768896
6.058859	620.035471	6.773901
5.986156	621.473562	6.778906
6.424313	628.128436	6.783910
6.424990	630.254938	6.788915
6.263785	622.594071	6.793920
6.064844	626.722303	6.798925
6.377888	614.547469	6.803930
6.434559	611.740051	6.808934
6.253022	614.428558	6.813939
6.187598	613.468143	6.818944
5.888437	620.819762	6.823949
5.798838	618.133852	6.828954
5.888079	612.962617	6.833958
6.105916	632.211582	6.838963
6.629046	636.372203	6.843968
6.359619	625.519300	6.848973
5.860683	624.885240	6.853978
6.144656	613.926106	6.858982
5.918363	627.215101	6.863987
6.267392	634.350462	6.868992
6.339116	637.181155	6.873997
5.953986	638.948049	6.879002
6.298666	632.216955	6.884006
5.968114	640.784667	6.889011
6.431900	645.045895	6.894016
5.895940	640.097764	6.899021
6.184197	641.825776	6.904026
6.369427	645.915264	6.909030
5.923264	652.259538	6.914035
6.043321	640.669986	6.919040
6.165243	660.775148	6.924045
6.337084	655.105155	6.929050
6.381703	649.782634	6.934054
6.100916	655.185044	6.939059
6.463540	643.320092	6.944064
6.252371	642.004125	6.949069
5.832066	627.067556	6.954074
6.021432	637.356426	6.959078
6.041943	644.269517	6.964083
6.338589	645.432927	6.969088
6.193388	649.641465	6.974093
6.181212	651.744049	6.979098
6.213636	643.802459	6.984102
5.978878	656.813841	6.989107
6.154912	654.060653	6.994112
5.937766	661.481988	6.999117
6.392391	656.928301	7.004122
6.428806	646.776217	7.009126
6.092160	653.390475	7.014131
6.579372	649.645626	7.019136
6.264363	652.562462	7.024141
5.876744	642.758847	7.029146
5.914427	642.510731	7.034150
6.000644	642.560064	7.039155
6.289332	650.987354	7.044160
6.289065	651.346625	7.049165
5.925269	655.947760	7.054170
6.154964	649.558548	7.059174
6.079651	653.353333	7.064179
6.036310	653.134421	7.069184
5.848253	651.319298	7.074189
6.192595	650.213276	7.079194
6.335198	648.892405	7.084198
6.099406	650.683907	7.089203
6.309843	651.740030	7.094208
6.088490	647.316435	7.099213
6.060097	644.263987	7.104218
6.412905	637.363804	7.109222
6.316221	652.444138	7.114227
6.456329	649.788072	7.119232
6.353987	648.828637	7.124237
6.105348	655.383724	7.129242
6.180458	645.094199	7.134246
6.137072	652.613056	7.139251
6.266030	653.746610	7.144256
6.402787	645.620002	7.149261
6.097626	646.720849	7.154266
6.188767	644.743458	7.159270
5.907023	652.234294	7.164275
6.194879	649.136977	7.169280
6.341911	649.413838	7.174285
6.044376	655.261856	7.179290
5.978594	644.934880	7.184294
5.842918	661.881031	7.189299
6.498177	648.990382	7.194304
6.159561	649.959024	7.199309
5.867089	654.527825	7.204314
6.068465	648.217504	7.209318
6.134759	650.644944	7.214323
6.170321	641.146994	7.219328
6.146916	650.034854	7.224333
6.123204	647.881903	7.229338
6.266748	648.649538	7.234342
6.182803	657.532428	7.239347
6.220474	646.754958	7.244352
6.312825	650.936396	7.249357
6.151843	661.795988	7.254362
6.252962	657.805637	7.259366
6.258351	655.667995	7.264371
6.304497	646.752815	7.269376
6.300886	655.375725	7.274381
5.953480	651.444648	7.279386
6.274397	646.836141	7.284390
5.973638	657.567713	7.289395
6.411408	655.860510	7.294400
6.379532	647.857733	7.299405
6.129429	647.040776	7.304410
6.243941	648.966877	7.309414
5.965857	658.904145	7.314419
6.012276	649.255992	7.319424
6.121497	651.526738	7.324429
5.876394	641.217222	7.329434
5.827175	641.593282	7.334438
6.132244	648.532666	7.339443
6.409901	645.864875	7.344448
6.407587	646.129761	7.349453
6.345351	656.640281	7.354458
6.412468	651.429676	7.359462
6.258833	652.115881	7.364467
6.296117	645.121514	7.369472
6.464881	648.270832	7.374477
6.018489	651.126540	7.379482
6.133756	646.473939	7.384486
5.883270	647.517187	7.389491
6.649389	649.803879	7.394496
6.176046	648.106644	7.399501
6.014267	654.101106	7.404506
5.909097	649.436460	7.409510
6.137129	657.394258	7.414515
6.121861	644.684108	7.419520
6.502016	650.365046	7.424525
5.928869	648.384378	7.429530
6.224692	638.648756	7.434534
6.128908	651.085749	7.439539
6.242340	644.420568	7.444544
6.333473	651.724940	7.449549
6.072810	646.772269	7.454554
6.211156	643.588804	7.459558
5.954990	650.361422	7.464563
6.375005	654.139703	7.469568
6.422713	657.241183	7.474573
6.204251	651.314549	7.479578
6.263554	640.683085	7.484582
6.052657	647.585555	7.489587
6.256016	650.735855	7.494592
6.378397	643.616097	7.499597
6.392351	646.718822	7.504602
6.098313	647.586543	7.509606
6.203955	650.168498	7.514611
6.433410	652.133979	7.519616
6.257746	651.678856	7.524621
6.240451	655.143945	7.529626
6.434122	638.135441	7.534630
5.986127	627.118711	7.539635
5.982161	633.720499	7.544640
5.929782	636.008530	7.549645
6.113967	651.589385	7.554650
6.310140	653.162537	7.559654
6.343839	660.549045	7.564659
6.293558	644.635522	7.569664
6.241366	649.516591	7.574669
6.181104	652.880652	7.579674
5.860380	639.845347	7.584678
5.757960	648.274644	7.589683
6.313964	649.929509	7.594688
6.070577	641.813752	7.599693
6.221902	653.486375	7.604698
6.335379	656.340548	7.609702
6.315790	653.693954	7.614707
6.399921	652.110038	7.619712
6.117009	657.854991	7.624717
6.188841	651.892918	7.629722
6.633505	651.886053	7.634726
6.147216	644.872214	7.639731
6.007123	628.237891	7.644736
6.311966	628.487436	7.649741
6.410806	631.786074	7.654746
6.308913	626.311398	7.659750
5.847826	629.377138	7.664755
5.913706	622.845351	7.669760
6.094480	625.375392	7.674765
6.349880	647.161094	7.679770
6.407655	636.288341	7.684774
6.149518	636.777931	7.689779
5.860028	619.887736	7.694784
5.959858	630.635051	7.699789
6.155046	650.959747	7.704794
6.718463	640.106670	7.709798
6.041626	642.448769	7.714803
6.087439	629.563539	7.719808
6.009554	639.493693	7.724813
6.174487	644.291840	7.729818
6.481308	643.461995	7.734822
6.256107	649.662720	7.739827
5.978321	636.454936	7.744832
5.893948	636.076658	7.749837
6.019092	654.495983	7.754842
6.337019	649.304234	7.759846
6.221020	661.047967	7.764851
6.270654	648.126568	7.769856
6.346653	652.151657	7.774861
5.873747	654.587471	7.779866
6.307152	653.739823	7.784870
6.266422	663.626739	7.789875
5.933258	650.262741	7.794880
6.124328	653.814101	7.799885
6.083283	666.416492	7.804890
6.294980	652.459048	7.809894
5.837487	658.070695	7.814899
5.997488	657.556437	7.819904
5.908085	664.800721	7.824909
5.910479	654.416271	7.829914
6.278002	649.191840	7.834918
6.019065	659.841892	7.839923
5.986714	660.869149	7.844928
5.979055	656.767750	7.849933
5.947191	650.345675	7.854938
6.070595	654.460007	7.859942
6.510835	661.794984	7.864947
6.100309	656.014215	7.869952
6.171588	658.241515	7.874957
6.101935	655.696750	7.879962
6.303421	649.220249	7.884966
6.139226	655.359171	7.889971
6.328417	652.169654	7.894976
6.452364	650.348256	7.899981
5.996290	659.563125	7.904986
6.198248	654.608048	7.909990
6.002712	666.682675	7.914995
6.242103	658.706806	7.920000
6.458741	657.399723	7.925005
6.359863	660.141449	7.930010
6.299554	650.791588	7.935014
6.001807	666.549352	7.940019
6.504125	661.010530	7.945024
6.350862	659.535782	7.950029
6.153001	660.749503	7.955034
6.217066	659.203641	7.960038
6.352376	666.695678	7.965043
6.289501	656.438071	7.970048
6.238883	655.738062	7.975053
6.215045	667.519426	7.980058
6.097119	654.055450	7.985062
5.788839	661.160737	7.990067
6.299342	660.160209	7.995072
5.969882	665.795257	8.000077
5.772013	660.310412	8.005082
6.292559	658.155351	8.010086
6.335806	659.386771	8.015091
6.477948	660.361454	8.020096
6.601841	660.220230	8.025101
6.540326	661.967483	8.030106
6.402645	651.834994	8.035123
6.116390	665.320211	8.040141
6.111828	658.162811	8.045158
6.505945	661.611966	8.050176
6.365855	643.646976	8.055194
6.133561	630.208799	8.060211
6.187893	629.143242	8.065229
6.263276	631.249981	8.070246
6.214349	631.056192	8.075264
6.242465	638.148396	8.080282
6.243020	623.556777	8.085299
6.122961	639.322179	8.090317
6.296210	634.380087	8.095334
6.377967	634.162690	8.100352
6.223523	636.033094	8.105370
6.376175	622.766599	8.110387
5.963951	623.394336	8.115405
6.391445	642.903868	8.120422
6.337206	637.051472	8.125440
5.934139	636.557292	8.130458
6.391655	639.271186	8.135475
6.272320	654.259760	8.140493
6.685397	650.979813	8.145510
6.198344	641.923305	8.150528
5.958626	633.358096	8.155546
6.492457	645.417818	8.160563
6.314605	658.206776	8.165581
6.608272	648.709194	8.170598
6.573752	631.788876	8.175616
6.083935	634.253755	8.180634
5.911506	626.073446	8.185651
6.082071	644.963755	8.190669
6.252186	647.639813	8.195686
6.511387	662.308644	8.200704
6.426752	652.774889	8.205722
6.797312	649.516155	8.210739
6.467878	643.302265	8.215757
6.133519	634.029544	8.220774
6.222927	632.740082	8.225792
6.293634	650.221039	8.230810
6.412573	650.733266	8.235827
6.242841	662.377253	8.240845
6.376476	663.896434	8.245862
6.385254	653.105554	8.250880
6.356619	663.931346	8.255898
6.676846	654.361650	8.260915
6.515301	660.295186	8.265933
6.530306	661.429705	8.270950
7.062421	648.993211	8.275968
6.427545	637.871943	8.280986
6.345301	633.642982	8.286003
5.928551	639.536097	8.291021
6.147844	651.865217	8.296038
6.564557	648.813788	8.301056
6.143351	656.993726	8.306074
6.097671	660.489722	8.311091
6.144796	666.835137	8.316109
6.112284	665.044239	8.321126
6.471782	660.691732	8.326144
6.086249	669.657847	8.331162
6.416052	664.707144	8.336179
6.333888	664.182658	8.341197
6.295844	658.339777	8.346214
6.415889	669.290550	8.351232
6.412755	682.286408	8.356250
6.580601	683.619228	8.361267
6.592511	687.210018	8.366285
6.459542	692.886094	8.371302
6.709161	682.541506	8.376320
6.569941	681.748925	8.381338
6.849825	681.659341	8.386355
6.875036	667.648602	8.391373
6.713070	655.090435	8.396390
6.670633	653.353541	8.401408
6.761702	659.429881	8.406426
6.852852	649.444212	8.411443
6.451901	655.945309	8.416461
6.559825	657.526617	8.421478
6.716741	656.609415	8.426496
6.586351	660.928443	8.431514
6.780915	659.398746	8.436531
6.681140	657.500883	8.441549
6.415395	653.301121	8.446566
6.524316	654.326786	8.451584
6.176642	650.563400	8.456602
6.727920	652.448041	8.461619
6.782636	655.900642	8.466637
6.472721	661.239100	8.471654
6.617705	652.577110	8.476672
6.708824	662.403604	8.481690
6.762182	663.450674	8.486707
6.521711	648.054901	8.491725
6.500545	653.620722	8.496742
6.615032	648.128155	8.501760
6.432490	663.240189	8.506778
6.734005	645.996119	8.511795
6.588698	652.195056	8.516813
6.453012	653.699387	8.521830
6.643529	668.502817	8.526848
6.747366	682.013607	8.531866
6.852482	674.459715	8.536883
6.761136	663.616514	8.541901
6.616312	662.387487	8.546918
6.642889	668.624107	8.551936
6.434713	679.855601	8.556954
6.743183	682.361914	8.561971
6.733545	691.820881	8.566989
6.621551	688.353479	8.572007
7.148713	679.913606	8.577024
6.848186	690.154554	8.582042
6.967734	682.094755	8.587059
6.724131	669.530804	8.592077
6.571210	667.818109	8.597095
6.681417	661.157419	8.602112
6.746705	682.384749	8.607130
7.179931	683.648824	8.612147
6.967260	676.183377	8.617165
6.346701	664.413301	8.622183
6.590977	669.815891	8.627200
6.639756	681.306394	8.632218
6.738970	686.839303	8.637235
6.798009	685.017496	8.642253
6.692658	682.004086	8.647271
6.744028	685.426147	8.652288
6.652799	686.202296	8.657306
6.724832	687.009282	8.662323
6.648136	682.662467	8.667341
6.576933	698.366692	8.672359
6.639213	683.983286	8.677376
6.646602	687.729934	8.682394
6.678788	690.886685	8.687411
6.743605	700.395137	8.692429
6.753646	714.471454	8.697447
7.010631	716.876461	8.702464
6.874505	717.453366	8.707482
7.155391	725.090334	8.712499
7.239573	704.302865	8.717517
6.598594	692.864082	8.722535
6.844016	691.747589	8.727552
6.878472	696.884949	8.732570
7.002234	691.684908	8.737587
6.869884	694.829931	8.742605
6.787188	717.746675	8.747623
7.344326	712.030009	8.752640
6.969393	716.090351	8.757658
6.661690	696.716130	8.762675
6.820242	709.261248	8.767693
7.032016	717.999357	8.772711
7.246590	723.773004	8.777728
7.108090	718.699841	8.782746
6.899575	704.618722	8.787763
6.990087	698.151424	8.792781
6.929750	698.986235	8.797799
7.063584	698.291344	8.802816
7.285432	710.896450	8.807834
6.981472	697.008691	8.812851
7.052413	700.106667	8.817869
6.821815	692.069018	8.822887
6.775248	691.168581	8.827904
7.088367	710.861300	8.832922
7.167582	720.553196	8.837939
7.459700	715.638243	8.842957
7.229053	708.629274	8.847975
7.130709	694.998791	8.852992
6.852936	694.356310	8.858010
6.738025	698.814116	8.863027
7.271769	700.169415	8.868045
6.893522	712.756968	8.873063
6.955909	710.964524	8.878080
7.070375	721.123783	8.883098
7.040807	719.973300	8.888115
7.041936	727.465660	8.893133
7.135777	727.749381	8.898151
7.367273	729.561795	8.903168
7.323539	722.776185	8.908186
6.936138	726.598844	8.913203
7.246853	730.486209	8.918221
7.060030	735.824388	8.923239
7.512001	720.802043	8.928256
7.202449	729.095018	8.933274
6.979481	713.320713	8.938291
7.016119	718.340403	8.943309
7.325518	725.817148	8.948327
7.725177	718.005418	8.953344
7.183333	711.620779	8.958362
7.069799	701.557953	8.963379
7.139492	697.302634	8.968397
6.954969	702.025102	8.973415
7.295447	705.770139	8.978432
7.170526	715.193096	8.983450
7.092557	726.165675	8.988467
7.075708	722.959266	8.993485
6.830476	731.354577	8.998503
7.130903	717.036032	9.003520
7.226525	719.084316	9.008538
6.913003	718.089507	9.013555
7.105176	720.183218	9.018573
7.010175	730.181117	9.023591
7.231984	724.673114	9.028608
6.948362	731.935872	9.033626
6.935291	722.686270	9.038643
7.329737	728.509264	9.043661
7.205564	736.161739	9.048679
7.567922	736.405721	9.053696
7.300208	737.417778	9.058714
7.255509	727.949407	9.063731
7.357337	727.290128	9.068749
7.167950	726.309800	9.073767
7.602164	734.366240	9.078784
7.365502	736.471124	9.083802
7.131211	730.520563	9.088819
7.221751	730.704837	9.093837
7.341660	740.587633	9.098855
7.442132	740.389576	9.103872
7.703867	755.047051	9.108890
7.140837	743.461473	9.113907
7.370571	735.510559	9.118925
7.549361	749.274729	9.123943
7.451151	738.947150	9.128960
7.394035	729.164317	9.133978
7.352045	740.776581	9.138995
7.342774	739.797134	9.144013
7.571998	745.372312	9.149031
7.397785	737.979203	9.154048
7.489062	741.828896	9.159066
7.324230	739.032792	9.164083
7.538503	735.379078	9.169101
7.692626	743.796845	9.174119
7.633674	737.751109	9.179136
7.621293	723.310742	9.184154
7.343053	731.025732	9.189171
7.674632	709.043026	9.194189
7.586660	723.692241	9.199207
7.495278	722.468139	9.204224
7.369167	722.534753	9.209242
7.646477	716.782143	9.214259
7.679596	717.889652	9.219277
7.488961	729.640687	9.224295
7.375070	721.712036	9.229312
7.479674	721.628643	9.234330
7.336319	728.057195	9.239347
7.712463	725.267179	9.244365
7.331438	726.440903	9.249383
7.387780	721.692542	9.254400
7.827319	729.332374	9.259418
7.581567	738.834011	9.264435
7.332075	724.989173	9.269453
7.416771	725.419676	9.274471
7.639331	739.497832	9.279488
7.782141	744.332243	9.284506
7.623313	752.206200	9.289523
7.699478	746.114859	9.294541
7.448417	737.197553	9.299559
7.788945	736.086567	9.304576
7.527471	741.672135	9.309594
7.558396	748.654088	9.314611
7.412798	739.988594	9.319629
7.583213	747.950542	9.324647
7.457787	746.340758	9.329664
7.567403	737.070045	9.334682
7.288497	751.851685	9.339699
7.800806	738.183430	9.344717
7.983637	743.913131	9.349735
7.591233	745.429273	9.354752
7.695642	742.773221	9.359770
7.717707	750.106623	9.364787
7.965592	741.116144	9.369805
7.902974	746.364472	9.374823
7.584209	747.572374	9.379840
7.944429	740.855685	9.384858
7.657683	743.923534	9.389875
7.771013	742.096273	9.394893
7.735354	739.652775	9.399911
7.849254	743.658556	9.404928
7.921895	747.050732	9.409946
7.743189	751.566752	9.414963
7.879598	743.465942	9.419981
7.729952	741.251543	9.424999
7.809182	743.269870	9.430016
7.865663	742.455510	9.435034
7.563185	746.722747	9.440051
7.708688	738.870026	9.445069
7.670003	747.707102	9.450087
7.650063	746.315271	9.455104
7.864701	747.209271	9.460122
7.588157	748.209405	9.465139
7.712323	746.861031	9.470157
7.929885	747.789190	9.475175
7.783962	748.861785	9.480192
7.591944	748.042906	9.485210
7.675171	749.742086	9.490227
7.782658	743.697132	9.495245
7.769301	753.691369	9.500263
7.682343	748.314008	9.505280
7.816761	752.155379	9.510298
7.955253	752.056531	9.515315
7.685198	752.789465	9.520333
7.995244	757.374153	9.525351
7.861668	760.143035	9.530368
7.860847	750.505189	9.535386
7.750282	752.203390	9.540403
8.476830	766.859890	9.545421
8.138499	763.280351	9.550439
8.155795	751.059725	9.555456
8.229018	745.283028	9.560474
7.922020	752.573680	9.565491
8.168657	754.719792	9.570509
8.024302	750.865236	9.575527
7.819344	750.842156	9.580544
8.065241	743.589310	9.585562
8.073193	749.670000	9.590579
7.638812	750.388808	9.595597
7.662999	746.857113	9.600615
7.670363	747.452775	9.605632
8.207670	750.747144	9.610650
7.945728	766.923549	9.615667
7.971357	765.350165	9.620685
8.180172	776.662279	9.625703
7.903221	778.597471	9.630720
8.019101	774.182523	9.635738
8.083995	780.067980	9.640755
8.406866	770.961136	9.645773
8.357386	763.635544	9.650791
8.005759	762.029753	9.655808
8.396985	752.649016	9.660826
7.846693	749.815957	9.665843
7.853291	743.284981	9.670861
8.065094	758.039699	9.675879
8.118990	775.805850	9.680896
8.399407	778.738454	9.685914
8.068294	768.368323	9.690931
7.932996	757.167001	9.695949
8.078250	769.139991	9.700967
8.082872	778.991905	9.705984
8.142968	776.206185	9.711002
8.050339	783.566467	9.716019
8.076595	777.854618	9.721037
7.995991	774.647339	9.726055
8.124099	784.542191	9.731072
8.268105	775.770457	9.736090
7.927273	782.356922	9.741107
7.891036	783.977861	9.746125
8.129300	794.348154	9.751143
7.875994	784.368651	9.756160
8.206352	781.132688	9.761178
7.779941	788.902948	9.766195
8.143827	777.269365	9.771213
8.145318	782.938956	9.776231
8.526173	800.432502	9.781248
8.680156	782.920205	9.786266
8.311157	780.535834	9.791283
8.299283	780.949260	9.796301
8.188997	770.746882	9.801319
8.196951	777.783043	9.806336
8.109911	776.673172	9.811354
8.115319	787.566243	9.816371
8.484143	796.507513	9.821389
8.628587	799.188241	9.826407
8.346209	789.259610	9.831424
8.412222	774.958568	9.836442
8.421136	779.900984	9.841459
8.029679	770.098688	9.846477
8.438705	778.384507	9.851495
8.068883	796.375953	9.856512
8.841528	800.808468	9.861530
8.314307	790.754245	9.866547
8.170684	783.240306	9.871565
8.456090	789.134920	9.876583
8.431583	795.935925	9.881600
8.833235	787.976989	9.886618
8.737787	783.986774	9.891635
8.807893	769.859853	9.896653
8.640011	769.771582	9.901671
8.477307	772.675597	9.906688
8.754906	764.894686	9.911706
8.632369	768.471539	9.916723
8.622916	773.505966	9.921741
8.815037	772.173502	9.926759
8.337305	770.983844	9.931776
8.328844	774.197340	9.936794
8.278957	770.994817	9.941811
8.251322	770.103051	9.946829
8.123116	765.692304	9.951847
8.284266	770.795719	9.956864
8.653331	771.720051	9.961882
8.451798	772.563286	9.966899
8.419029	767.973753	9.971917
8.215190	775.180408	9.976935
8.425052	774.704014	9.981952
8.866259	778.546951	9.986970
8.620229	778.263757	9.991987
8.751756	762.575969	9.997005
8.812133	767.654733	10.002023
8.538630	785.724307	10.007040
8.729087	776.392549	10.012058
8.659080	774.025595	10.017075
8.752908	773.692031	10.022093
8.773984	771.685565	10.027111
8.769847	771.216262	10.032128
8.739147	769.229788	10.037146
8.781078	771.968429	10.042163
8.616319	770.336418	10.047181
8.659928	773.083836	10.052199
8.744663	778.557368	10.057216
8.361366	774.562854	10.062234
8.703427	779.420185	10.067251
8.745161	778.633067	10.072269
8.841358	767.059171	10.077287
8.583185	769.872307	10.082304
8.416927	763.815983	10.087322
8.747248	771.477071	10.092339
8.418563	766.034225	10.097357
8.663383	768.066866	10.102375
8.510586	769.670098	10.107392
8.778187	767.790520	10.112410
8.658577	775.221797	10.117427
8.791645	782.384873	10.122445
8.927148	784.903309	10.127463
8.489446	785.867536	10.132480
8.829721	794.070659	10.137498
8.926585	795.513662	10.142515
8.734847	800.962907	10.147533
9.387255	789.911427	10.152551
8.562987	790.280645	10.157568
8.967884	774.216887	10.162586
8.961842	770.577206	10.167603
8.788582	769.071793	10.172621
8.915140	770.476020	10.177639
8.699945	780.542277	10.182656
9.103081	774.480243	10.187674
8.778085	773.330252	10.192691
8.604248	777.162833	10.197709
9.111072	773.722857	10.202727
8.791500	774.238806	10.207744
8.715971	769.716586	10.212762
8.860194	785.165160	10.217779
8.586308	795.525776	10.222797
8.869456	794.959691	10.227815
8.592644	800.825758	10.232832
9.011139	801.780488	10.237850
8.982074	795.722299	10.242867
9.025170	802.434953	10.247885
9.223327	797.698123	10.252903
9.033821	803.590676	10.257920
8.892228	799.695102	10.262938
9.179966	799.507372	10.267955
9.056476	801.977362	10.272973
9.339351	795.448252	10.277991
8.806495	802.218482	10.283008
8.867156	800.808576	10.288026
8.871699	793.564571	10.293043
8.679458	783.198993	10.298061
8.846996	795.202957	10.303079
8.945922	797.665644	10.308096
9.273475	789.756375	10.313114
9.114143	791.057953	10.318131
8.847620	790.263613	10.323149
9.002687	789.600239	10.328167
9.045657	796.504633	10.333184
9.048532	794.975957	10.338202
9.070543	800.478779	10.343219
8.885127	813.246676	10.348237
8.958105	793.175867	10.353255
8.867890	801.978202	10.358272
9.105350	798.263943	10.363290
9.248670	802.009763	10.368307
9.073573	802.330539	10.373325
8.967798	802.827621	10.378343
9.024434	821.544108	10.383360
9.520039	831.599780	10.388378
9.571239	827.947457	10.393395
9.381787	816.222803	10.398413
9.320946	806.023630	10.403431
9.248737	799.977702	10.408448
9.090336	801.144881	10.413466
9.396096	793.098676	10.418483
9.125066	797.217814	10.423501
9.009768	790.783770	10.428519
9.141816	794.072030	10.433536
8.798275	794.560454	10.438554
9.179750	810.478009	10.443571
9.211536	829.226571	10.448589
9.537633	819.379439	10.453607
9.291083	830.405201	10.458624
9.336363	831.576843	10.463642
9.604281	826.032036	10.468659
9.126340	836.632363	10.473677
9.640653	826.312349	10.478695
9.334234	826.026950	10.483712
9.285274	814.723499	10.488730
9.207221	812.432277	10.493747
9.578518	831.020298	10.498765
9.516403	818.924967	10.503783
9.172322	809.071891	10.508800
9.386921	816.404543	10.513818
9.462150	825.123593	10.518835
9.344856	827.450836	10.523853
9.688587	817.347648	10.528871
9.473750	808.696730	10.533888
9.337791	802.958586	10.538906
9.436669	796.887479	10.543923
9.298109	808.163046	10.548941
9.591530	819.769433	10.553959
9.306354	822.686258	10.558976
9.393203	826.869759	10.563994
9.849445	822.919671	10.569011
9.550424	819.076536	10.574029
9.626965	803.171052	10.579047
9.235736	800.352193	10.584064
9.420637	808.686163	10.589082
9.754370	821.382276	10.594099
9.310912	816.719401	10.599117
9.102074	818.426402	10.604135
9.570570	828.428689	10.609152
9.684454	831.821141	10.614170
9.836983	834.048591	10.619187
9.647318	829.342507	10.624205
9.695652	827.481119	10.629223
9.937419	825.534162	10.634240
9.846997	814.562756	10.639258
9.882378	795.664644	10.644275
9.237573	791.284317	10.649293
9.373232	792.928759	10.654311
9.445722	797.189036	10.659328
9.859314	806.211870	10.664346
9.688928	796.525305	10.669363
9.500681	799.234746	10.674381
9.518079	794.830195	10.679399
9.615799	820.163150	10.684416
9.686279	825.876054	10.689434
9.822219	823.906859	10.694451
10.006429	826.910912	10.699469
9.820240	809.605298	10.704487
9.496308	804.609660	10.709504
9.360941	810.089729	10.714522
9.744542	806.529213	10.719539
9.627344	833.896886	10.724557
9.789576	817.279202	10.729575
9.684746	826.544576	10.734592
9.541933	829.598057	10.739610
9.891638	820.327694	10.744627
9.743340	823.719859	10.749645
10.014603	822.990396	10.754663
9.576640	828.810326	10.759680
9.331620	827.634490	10.764698
9.908396	829.477533	10.769715
9.634638	835.496642	10.774733
9.802717	819.902738	10.779751
9.495977	832.536812	10.784768
9.403531	836.748430	10.789786
9.974249	831.192850	10.794803
10.158402	835.877932	10.799821
10.007545	827.207354	10.804839
9.809412	832.780498	10.809856
9.620393	833.790159	10.814874
9.791650	821.987662	10.819891
9.561844	836.017589	10.824909
9.484532	833.876234	10.829927
9.827982	850.024524	10.834944
9.917709	853.035960	10.839962
10.279386	862.609916	10.844979
10.213253	864.255105	10.849997
10.397202	855.860552	10.855015
10.299294	836.146314	10.860032
9.739467	834.041158	10.865050
10.127613	834.436377	10.870067
9.817724	834.942457	10.875085
9.933884	829.786933	10.880103
10.297396	834.028950	10.885120
9.902791	834.092388	10.890138
10.022986	818.996547	10.895155
9.527606	834.658162	10.900173
10.112045	841.788648	10.905191
10.268766	845.316915	10.910208
10.240594	853.208656	10.915226
10.295166	837.751635	10.920243
10.085387	838.014378	10.925261
9.990857	834.224775	10.930279
10.033273	830.810903	10.935296
9.764801	840.617924	10.940314
10.096357	845.775032	10.945331
10.112725	853.132259	10.950349
10.216401	854.458791	10.955367
10.211292	856.100173	10.960384
10.319370	859.044008	10.965402
10.256077	851.923407	10.970419
10.461353	858.399398	10.975437
10.193576	842.921736	10.980455
10.212658	832.140049	10.985472
9.962054	828.582580	10.990490
10.161258	835.968576	10.995507
10.205533	843.128667	11.000525
10.484610	845.863485	11.005543
10.374175	837.159438	11.010560
10.298166	834.320264	11.015578
10.143560	821.446586	11.020595
9.679438	829.918351	11.025613
10.218490	848.112491	11.030631
10.401484	855.829510	11.035648
10.020307	857.544187	11.040666
10.122110	858.200197	11.045683
10.155720	857.606536	11.050701
10.164337	856.305238	11.055719
10.412982	855.413779	11.060736
10.453050	857.469707	11.065754
10.598594	848.920107	11.070771
10.354711	853.033190	11.075789
10.367244	856.637301	11.080807
10.373169	854.951822	11.085824
10.254674	853.677084	11.090842
10.343877	851.426662	11.095859
10.265012	860.566503	11.100877
10.212467	854.694849	11.105895
10.433794	857.254594	11.110912
10.281888	862.925994	11.115930
10.585817	854.787545	11.120947
10.416287	854.323974	11.125965
10.399468	855.215757	11.130983
10.603618	862.442292	11.136000
10.393221	858.538806	11.141018
10.732490	849.461876	11.146035
10.448550	856.240516	11.151053
10.225361	862.475267	11.156071
10.489627	862.783919	11.161088
10.691610	857.033888	11.166106
10.560530	856.017914	11.171123
10.646553	855.715166	11.176141
10.245015	860.541724	11.181159
10.574950	856.679468	11.186176
10.281796	866.579171	11.191194
10.578644	854.823172	11.196211
10.707661	858.881595	11.201229
10.135396	863.823821	11.206247
10.366148	869.957819	11.211264
10.706259	887.022799	11.216282
11.038563	884.354182	11.221299
10.495576	883.511920	11.226317
10.194087	889.782087	11.231335
10.363808	879.988367	11.236352
10.406885	887.688022	11.241370
11.259834	889.064102	11.246387
11.115685	895.096416	11.251405
11.021101	882.461556	11.256423
11.045061	863.651075	11.261440
10.664893	862.879093	11.266458
10.987012	860.656240	11.271475
10.772610	855.169636	11.276493
10.652229	854.202675	11.281511
10.717083	856.006479	11.286528
10.645526	859.174144	11.291546
10.954344	859.569902	11.296563
10.985269	850.293254	11.301581
10.645678	855.629212	11.306599
10.781721	853.824555	11.311616
10.530876	850.949371	11.316634
10.882393	853.602119	11.321651
10.859597	849.840791	11.326669
10.577153	855.628680	11.331687
11.022436	870.201939	11.336704
10.834215	877.013554	11.341722
11.073771	878.417584	11.346739
11.220701	865.538031	11.351757
10.794932	855.109110	11.356775
10.857671	850.233672	11.361792
10.675792	856.363947	11.366810
10.747897	859.296417	11.371827
11.183980	878.244615	11.376845
11.089030	875.408570	11.381863
11.132421	856.808255	11.386880
10.572162	859.498603	11.391898
10.515566	865.823086	11.396915
10.860333	871.688612	11.401933
10.888320	880.252137	11.406951
11.171697	877.431789	11.411968
10.815735	892.268445	11.416986
10.531517	886.715836	11.422003
10.727182	887.988558	11.427021
10.730460	887.761713	11.432039
11.047433	889.193080	11.437056
10.686879	893.771534	11.442074
10.658071	891.149327	11.447091
10.947776	901.694630	11.452109
11.132041	907.168261	11.457127
11.114251	903.793474	11.462144
11.324839	914.975086	11.467162
11.407077	911.162887	11.472179
11.337707	894.119712	11.477197
11.183834	883.959514	11.482215
11.317369	878.621972	11.487232
11.264843	881.329032	11.492250
11.282130	871.034993	11.497267
11.539166	878.157115	11.502285
11.127764	887.404395	11.507303
11.439664	880.262204	11.512320
11.466204	881.135786	11.517338
11.354128	878.106916	11.522355
11.363083	873.104163	11.527373
11.340872	878.658428	11.532391
11.415990	875.113546	11.537408
11.307685	882.947708	11.542426
11.368141	873.561831	11.547443
11.281886	872.536859	11.552461
10.923540	877.595628	11.557479
11.453989	879.180613	11.562496
11.175449	882.240044	11.567514
11.320160	877.503772	11.572531
11.379050	877.823204	11.577549
11.035728	880.521331	11.582567
11.383174	882.330705	11.587584
11.058751	875.843069	11.592602
11.413047	875.560856	11.597619
11.307555	874.351676	11.602637
11.155884	887.954952	11.607655
11.298926	877.140110	11.612672
11.553583	874.793786	11.617690
11.246134	879.889009	11.622707
11.490672	879.484819	11.627725
11.179595	886.889196	11.632743
11.263029	881.264294	11.637760
11.684961	892.960474	11.642778
11.561877	897.682670	11.647795
11.557821	883.700597	11.652813
11.298091	884.403088	11.657831
11.772704	880.682216	11.662848
11.653903	875.088441	11.667866
11.425132	880.211972	11.672883
11.540444	874.429438	11.677901
11.668492	876.130659	11.682919
11.702009	873.128467	11.687936
11.564830	879.439529	11.692954
11.904295	873.893488	11.697971
11.794070	879.535946	11.702989
11.454130	874.239800	11.708007
11.622198	874.925387	11.713024
11.810695	877.176020	11.718042
11.337794	874.711599	11.723059
11.575275	876.391944	11.728077
11.598804	874.174833	11.733095
11.723237	869.239175	11.738112
11.870137	874.896533	11.743130
12.082399	871.110055	11.748147
12.044315	870.107814	11.753165
11.622184	873.292983	11.758183
11.679199	863.699423	11.763200
11.866841	872.347132	11.768218
11.725053	876.077191	11.773235
11.813298	878.466073	11.778253
11.740536	873.894941	11.783271
11.865667	866.306540	11.788288
11.582225	875.835366	11.793306
11.500727	880.673894	11.798323
12.064738	878.276345	11.803341
11.710310	883.773817	11.808359
11.829800	874.530519	11.813376
11.605852	872.984278	11.818394
11.514954	874.211541	11.823411
11.533145	876.256921	11.828429
11.709098	880.298524	11.833447
11.933967	884.191089	11.838464
11.900559	897.146079	11.843482
11.828662	905.290745	11.848499
12.052657	897.435970	11.853517
11.762830	911.537712	11.858535
12.099511	903.516644	11.863552
12.065492	903.687295	11.868570
11.755768	892.780492	11.873587
11.782269	902.002513	11.878605
11.809648	903.836936	11.883623
11.966176	892.356889	11.888640
12.087339	905.126850	11.893658
11.989216	898.809596	11.898675
12.076950	903.887419	11.903693
11.874383	909.479039	11.908711
12.123700	901.834626	11.913728
11.818950	905.070834	11.918746
11.987503	911.078146	11.923763
11.991878	899.944533	11.928781
11.851771	915.154505	11.933799
12.010723	903.188637	11.938816
12.063033	903.276099	11.943834
12.045347	901.655939	11.948851
12.025163	905.095408	11.953869
11.567780	911.318567	11.958887
11.602058	909.077231	11.963904
12.021432	911.260901	11.968922
12.208946	932.217952	11.973939
12.183135	932.068754	11.978957
12.371931	937.374330	11.983975
12.576948	928.305807	11.988992
12.358580	920.536080	11.994010
12.336916	903.263746	11.999027
12.413660	889.602918	12.004045
12.259795	900.151593	12.009063
12.217781	897.134739	12.014080
12.000487	902.721710	12.019098
12.064720	911.843398	12.024115
12.474891	911.713737	12.029133
12.145842	912.231652	12.034151
12.225252	921.631529	12.039168
12.589069	922.549654	12.044186
12.413590	927.589576	12.049203
12.703007	908.287467	12.054221
12.553856	903.723857	12.059239
12.186355	897.781115	12.064256
12.473943	892.408217	12.069274
11.940124	905.405527	12.074291
12.447541	909.372566	12.079309
12.482486	913.771369	12.084327
12.557911	922.832158	12.089344
12.612008	903.633979	12.094362
12.385752	905.583232	12.099379
12.233459	898.447821	12.104397
12.257274	906.957724	12.109415
12.665705	934.649936	12.114432
12.721372	926.782470	12.119450
12.550081	926.750271	12.124467
12.656181	907.508044	12.129485
12.819840	914.874768	12.134503
12.548292	901.278689	12.139520
12.395225	896.909815	12.144538
12.541356	904.051493	12.149555
12.387905	896.439525	12.154573
12.395997	902.628515	12.159591
12.315749	925.658542	12.164608
12.596468	927.823049	12.169626
12.532424	931.402852	12.174643
12.484149	934.364324	12.179661
12.739167	931.792352	12.184679
12.428841	935.505059	12.189696
12.824516	931.515369	12.194714
12.429018	939.935674	12.199731
12.348162	933.598226	12.204749
12.368397	937.329815	12.209767
12.635135	936.130251	12.214784
12.866457	935.986112	12.219802
12.616344	938.692830	12.224819
12.787781	925.346591	12.229837
12.655556	929.889610	12.234855
12.428481	930.528823	12.239872
12.562323	921.858292	12.244890
12.619647	935.072294	12.249907
12.828104	938.326674	12.254925
12.771395	937.807806	12.259943
13.078778	953.773603	12.264960
12.694569	936.481346	12.269978
12.914138	939.796875	12.274995
12.748691	946.851984	12.280013
13.025822	946.166424	12.285031
12.996453	947.900411	12.290048
13.340702	940.848501	12.295066
13.031595	932.191471	12.300083
13.411355	924.897871	12.305101
13.067798	921.571118	12.310119
12.662987	926.884436	12.315136
13.185032	923.994246	12.320154
12.659280	922.853077	12.325171
12.837177	921.080062	12.330189
12.959872	928.343343	12.335207
13.272954	930.256440	12.340224
13.112525	921.418504	12.345242
12.610165	935.845211	12.350259
12.728455	924.594690	12.355277
12.730376	932.801553	12.360295
12.846534	941.041471	12.365312
13.379575	947.635266	12.370330
13.269430	960.807338	12.375347
13.484706	953.412227	12.380365
12.988806	933.500786	12.385383
13.129180	935.338549	12.390400
13.263397	916.216847	12.395418
12.888291	921.795705	12.400435
13.201398	937.378664	12.405453
13.176811	937.925690	12.410471
13.288462	953.951456	12.415488
13.559546	944.575539	12.420506
13.233355	931.832932	12.425523
13.180610	928.494635	12.430541
13.128815	915.745974	12.435559
13.030432	919.068086	12.440576
13.450603	928.657594	12.445594
13.161801	935.463844	12.450611
13.517859	944.316373	12.455629
13.369829	932.950897	12.460647
13.006379	927.881843	12.465664
13.263430	931.159276	12.470682
13.261924	946.152242	12.475699
13.300350	950.058374	12.480717
13.459832	944.625965	12.485735
13.109177	956.515476	12.490752
13.424980	951.117414	12.495770
13.053660	958.292440	12.500787
13.267703	954.360378	12.505805
13.483192	945.048782	12.510823
13.237804	956.536626	12.515840
13.265784	954.908899	12.520858
13.681590	954.534614	12.525875
13.801775	948.385120	12.530893
13.751951	944.127084	12.535911
13.479539	955.432402	12.540928
13.768057	946.421692	12.545946
13.727359	939.496514	12.550963
13.893704	937.055360	12.555981
13.627603	918.711722	12.560999
13.050406	922.504441	12.566016
13.124433	927.945548	12.571034
13.256111	945.828536	12.576051
13.518002	957.394581	12.581069
13.669795	947.352617	12.586087
13.551052	951.552086	12.591104
13.663350	947.468770	12.596122
13.283662	952.972811	12.601139
13.568797	946.538141	12.606157
13.713544	945.257993	12.611175
13.654872	949.305395	12.616192
13.599248	943.634207	12.621210
13.548331	945.496954	12.626227
13.782196	950.109275	12.631245
13.835752	944.802275	12.636263
13.825249	953.659604	12.641280
13.970751	945.815046	12.646298
13.646284	952.777596	12.651315
13.750881	951.434807	12.656333
13.743957	949.769162	12.661351
13.770522	948.054665	12.666368
13.659837	947.059716	12.671386
13.852742	949.330102	12.676403
13.684192	950.882420	12.681421
13.760825	948.231721	12.686439
13.850764	955.070536	12.691456
14.050000	945.517154	12.696474
13.958739	956.219667	12.701491
13.886563	956.817091	12.706509
14.343101	945.741245	12.711527
13.954552	961.480962	12.716544
14.258193	956.658904	12.721562
13.911406	957.904136	12.726579
14.098168	946.528093	12.731597
13.829523	947.341507	12.736615
13.574709	949.836415	12.741632
13.953083	942.731218	12.746650
13.563894	944.138582	12.751667
13.861590	964.263688	12.756685
14.072634	970.296664	12.761703
13.883912	982.009386	12.766720
14.259526	983.550732	12.771738
14.394673	982.789079	12.776755
14.326325	974.396477	12.781773
14.258833	951.953546	12.786791
13.872816	947.917312	12.791808
14.049400	944.948501	12.796826
13.931214	959.781674	12.801843
14.019284	973.277614	12.806861
14.238078	975.538992	12.811879
14.044858	973.023126	12.816896
13.930699	977.610409	12.821914
14.270010	979.318783	12.826931
14.211897	978.374180	12.831949
14.227765	980.434131	12.836967
14.234330	979.691013	12.841984
14.424077	975.907058	12.847002
14.392154	974.814816	12.852019
13.960948	978.031823	12.857037
14.550450	975.282809	12.862055
14.209245	971.258834	12.867072
14.454285	977.750730	12.872090
14.357783	972.800838	12.877107
14.038344	971.825494	12.882125
14.387761	974.800646	12.887143
14.105001	982.653116	12.892160
14.331636	979.410667	12.897178
14.196828	975.430857	12.902195
14.290442	977.976339	12.907213
14.490797	973.742614	12.912231
14.381490	977.354725	12.917248
14.334154	975.066267	12.922266
14.563797	977.788035	12.927283
14.168972	980.399829	12.932301
14.269617	983.133116	12.937319
14.269731	987.382990	12.942336
14.457485	998.096021	12.947354
14.735679	1002.500238	12.952371
15.037079	1008.407248	12.957389
15.173470	986.951332	12.962407
14.607427	984.356652	12.967424
14.523954	976.562985	12.972442
14.743987	971.846889	12.977459
14.635485	974.238837	12.982477
14.721418	968.018239	12.987495
14.934461	973.256036	12.992512
14.509806	968.458116	12.997530
14.593513	971.349318	13.002547
14.369991	973.297339	13.007565
14.447204	959.883212	13.012583
14.375683	971.922174	13.017600
14.763558	986.769998	13.022618
14.880205	990.765153	13.027635
14.773314	997.728702	13.032653
14.803138	1001.598871	13.037671
14.934232	1006.977803	13.042688
15.047879	996.388997	13.047706
15.044434	981.160721	13.052723
14.865156	978.881118	13.057741
15.186237	964.853401	13.062759
14.205520	973.944620	13.067776
14.533808	962.067197	13.072794
14.720269	987.494783	13.077811
14.490894	998.947331	13.082829
14.850826	993.963584	13.087847
14.582257	1003.588053	13.092864
14.718085	997.967818	13.097882
14.797388	996.054827	13.102899
14.944862	1001.802290	13.107917
14.839328	994.915381	13.112935
14.686177	1000.552787	13.117952
15.175751	994.264947	13.122970
15.189448	998.337384	13.127987
14.994148	1004.073498	13.133005
15.108076	989.869832	13.138023
14.752359	1002.729074	13.143040
15.150134	994.609264	13.148058
15.493198	994.780073	13.153075
15.126919	998.454030	13.158093
15.391483	994.177385	13.163111
15.116435	1009.791275	13.168128
15.258416	1001.863810	13.173146
15.196694	990.445419	13.178163
15.319421	997.025291	13.183181
15.002170	986.672796	13.188199
14.741514	1005.031824	13.193216
15.069969	999.598187	13.198234
15.144584	1004.149102	13.203251
15.183644	1012.197501	13.208269
15.488366	1007.653584	13.213287
15.108433	1006.191030	13.218304
14.661950	1012.784850	13.223322
14.884387	1019.729702	13.228339
15.253218	1023.581929	13.233357
15.549276	1023.238495	13.238375
15.516762	1019.216146	13.243392
15.476524	1027.214694	13.248410
15.588745	1024.207314	13.253427
15.545191	1021.607211	13.258445
15.936379	1019.005984	13.263463
15.725952	1019.603076	13.268480
15.575353	1006.706927	13.273498
15.805775	987.846755	13.278515
15.453658	987.917329	13.283533
15.487080	987.929576	13.288551
15.632458	995.578488	13.293568
15.107786	979.717259	13.298586
15.577491	982.810678	13.303603
15.582180	997.025534	13.308621
15.701691	989.348637	13.313639
15.543487	985.743943	13.318656
15.491494	988.279287	13.323674
15.648623	986.096334	13.328691
15.649908	988.252005	13.333709
15.665513	982.420196	13.338727
15.702560	987.779656	13.343744
15.486997	987.869744	13.348762
15.604959	985.408249	13.353779
15.470025	986.081024	13.358797
15.657457	978.474379	13.363815
15.586685	994.796130	13.368832
15.889063	1005.282715	13.373850
16.022676	1000.788786	13.378867
15.504984	992.842217	13.383885
15.582573	991.294063	13.388903
15.787550	1008.435488	13.393920
15.831770	1025.563395	13.398938
16.175461	1024.786893	13.403955
15.628212	1024.638213	13.408973
15.705842	1015.057682	13.413991
15.701694	1024.169107	13.419008
15.897130	1016.551669	13.424026
16.153044	1023.470114	13.429043
16.012649	1017.750734	13.434061
16.012922	1015.700833	13.439079
15.830863	1016.357792	13.444096
15.719683	1018.660431	13.449114
16.270261	1014.001001	13.454131
15.962772	1020.099386	13.459149
15.750371	1018.905535	13.464167
15.769747	1018.199663	13.469184
15.746872	1028.905075	13.474202
15.946338	1023.470348	13.479219
15.855940	1025.211694	13.484237
15.998718	1010.020199	13.489255
15.895322	1028.904769	13.494272
15.664402	1032.495299	13.499290
16.060687	1017.069307	13.504307
16.089967	1013.155621	13.509325
16.138275	1016.437717	13.514343
15.674644	1015.533488	13.519360
15.709900	1025.837949	13.524378
16.428082	1031.540920	13.529395
16.113041	1044.620224	13.534413
15.960263	1043.633026	13.539431
16.331691	1046.424239	13.544448
16.292618	1033.208431	13.549466
16.774598	1035.563635	13.554483
16.494644	1038.201298	13.559501
16.762092	1023.502120	13.564519
16.274590	1018.589399	13.569536
16.230205	1013.422604	13.574554
16.264832	1013.522837	13.579571
15.949749	1012.637317	13.584589
16.018070	1006.002312	13.589607
16.390811	1025.613123	13.594624
16.347347	1042.326451	13.599642
16.624720	1032.354580	13.604659
16.346900	1041.005838	13.609677
16.641568	1041.176787	13.614695
16.498441	1036.089325	13.619712
16.288669	1037.286680	13.624730
16.458059	1035.655213	13.629747
16.574897	1038.405907	13.634765
16.773335	1043.139079	13.639783
16.691709	1043.067230	13.644800
16.444676	1039.504397	13.649818
16.477535	1029.210824	13.654835
16.716561	1042.907804	13.659853
16.645135	1041.090630	13.664871
16.636861	1037.962654	13.669888
16.408521	1037.961160	13.674906
16.591830	1028.312730	13.679923
16.426118	1039.271320	13.684941
16.636748	1032.227322	13.689959
16.894454	1043.445711	13.694976
16.828472	1040.713497	13.699994
16.617472	1041.858695	13.705011
16.803009	1040.312740	13.710029
17.052809	1030.990294	13.715047
16.981010	1034.203308	13.720064
16.896164	1037.096055	13.725082
17.099598	1027.563973	13.730099
16.636419	1017.680091	13.735117
16.421835	1017.241691	13.740135
16.737274	1025.476608	13.745152
16.543766	1030.724659	13.750170
16.720214	1025.414605	13.755187
16.373988	1041.106057	13.760205
16.371938	1039.707301	13.765223
16.674961	1043.797194	13.770240
16.706484	1033.615253	13.775258
17.024686	1049.779744	13.780275
16.875427	1061.635199	13.785293
17.106217	1063.898541	13.790311
17.145668	1062.428740	13.795328
17.007149	1061.835622	13.800346
17.466034	1045.622887	13.805363
17.168874	1041.170749	13.810381
17.192146	1038.389111	13.815399
17.355354	1023.170205	13.820416
16.758485	1035.706821	13.825434
17.026260	1029.119880	13.830451
17.157499	1037.471521	13.835469
16.993031	1041.442373	13.840487
16.727458	1033.769379	13.845504
17.207226	1051.910587	13.850522
17.020307	1062.161313	13.855539
17.269849	1063.114511	13.860557
17.580340	1063.544642	13.865575
17.625273	1054.086819	13.870592
17.132283	1045.052314	13.875610
17.424042	1037.516551	13.880627
17.489003	1030.552577	13.885645
17.237739	1037.225101	13.890663
17.268316	1031.027816	13.895680
17.250829	1035.799888	13.900698
17.114471	1029.702290	13.905715
17.128395	1037.257246	13.910733
17.444486	1050.883206	13.915751
17.527088	1061.507792	13.920768
17.484505	1058.393761	13.925786
17.840334	1055.490520	13.930803
17.656030	1033.082167	13.935821
17.254371	1041.256312	13.940839
17.344045	1031.920617	13.945856
17.276633	1030.716930	13.950874
17.603749	1044.854820	13.955891
17.687411	1054.511938	13.960909
17.769798	1055.261326	13.965927
17.606620	1029.537789	13.970944
17.167531	1040.223942	13.975962
17.236402	1043.277450	13.980979
17.667354	1059.503987	13.985997
17.944862	1062.084385	13.991015
17.790298	1052.961161	13.996032
17.621448	1057.513431	14.001050
17.733380	1053.669903	14.006067
17.704328	1058.430119	14.011085
17.833582	1057.354095	14.016103
17.692841	1053.113052	14.021120
17.532254	1066.827012	14.026138
17.643178	1057.814543	14.031155
17.614223	1050.949966	14.036173
17.698247	1058.144519	14.041191
17.961199	1058.867157	14.046208
17.807147	1067.142830	14.051226
17.513778	1056.308791	14.056243
17.484417	1058.985669	14.061261
17.570832	1058.413177	14.066279
17.690898	1053.086467	14.071296
17.767741	1059.364525	14.076314
17.927834	1060.664018	14.081331
17.436287	1066.338583	14.086349
17.772102	1072.080476	14.091367
18.138590	1085.548521	14.096384
18.303610	1095.324472	14.101402
18.317505	1085.070616	14.106419
18.296577	1079.114903	14.111437
17.922848	1067.924096	14.116455
18.169405	1046.301042	14.121472
17.921374	1048.711776	14.126490
17.957232	1064.800992	14.131507
18.483135	1078.726475	14.136525
17.799867	1080.285298	14.141543
18.533977	1076.216305	14.146560
18.497377	1077.746394	14.151578
18.311186	1056.601267	14.156595
18.047767	1058.414966	14.161613
17.962007	1055.677756	14.166631
18.317715	1062.525366	14.171648
18.072356	1058.972486	14.176666
18.126438	1073.914247	14.181683
18.478762	1082.700548	14.186701
18.149388	1082.737043	14.191719
18.367696	1080.641975	14.196736
18.135311	1083.257202	14.201754
18.363548	1084.291879	14.206771
18.155274	1083.533939	14.211789
18.194364	1088.031314	14.216807
18.179125	1083.339575	14.221824
18.447745	1084.403784	14.226842
18.807694	1083.869460	14.231859
18.409711	1079.456446	14.236877
18.247252	1086.439471	14.241895
18.434255	1082.037462	14.246912
18.412674	1086.000020	14.251930
18.739718	1085.265246	14.256947
18.791845	1088.182170	14.261965
18.446420	1087.668979	14.266983
18.604738	1075.078696	14.272000
18.145460	1081.915993	14.277018
18.339300	1075.762914	14.282035
18.976041	1080.532966	14.287053
18.499386	1083.089825	14.292071
19.015437	1079.423855	14.297088
19.084677	1078.412096	14.302106
18.976993	1081.155488	14.307123
18.912654	1082.307899	14.312141
18.432972	1083.392476	14.317159
18.900124	1074.108027	14.322176
18.592247	1084.933108	14.327194
18.526671	1082.540964	14.332211
18.763647	1075.755173	14.337229
18.595921	1077.327839	14.342247
18.809581	1077.174813	14.347264
18.789225	1080.873003	14.352282
18.629426	1079.999953	14.357299
19.018342	1072.881534	14.362317
18.800433	1082.257908	14.367335
18.896389	1076.157650	14.372352
18.431871	1086.468924	14.377370
18.909287	1105.313317	14.382387
19.105041	1113.161026	14.387405
19.003011	1119.451405	14.392423
19.292803	1108.205817	14.397440
19.550241	1104.853127	14.402458
19.346933	1091.149127	14.407475
19.341345	1075.980559	14.412493
18.883085	1078.719798	14.417511
18.992179	1074.396044	14.422528
18.842549	1083.620960	14.427546
18.761164	1084.775801	14.432563
19.116162	1096.846200	14.437581
19.181066	1114.201875	14.442599
19.276292	1110.802818	14.447616
19.664495	1112.737750	14.452634
19.162092	1109.984877	14.457651
19.375964	1105.046539	14.462669
19.467545	1116.734996	14.467687
19.087396	1099.645026	14.472704
19.020066	1104.373407	14.477722
19.217206	1112.352771	14.482739
19.517954	1105.869782	14.487757
19.402510	1109.528608	14.492775
19.376883	1105.910200	14.497792
19.327587	1116.154709	14.502810
19.278243	1110.849337	14.507827
19.238295	1105.335332	14.512845
19.069681	1112.078057	14.517863
19.313083	1102.890481	14.522880
19.309068	1102.874283	14.527898
19.529904	1103.645628	14.532915
19.627461	1101.178439	14.537933
19.234856	1102.323399	14.542951
19.562572	1107.587528	14.547968
19.560443	1111.408293	14.552986
19.379303	1102.376445	14.558003
19.368198	1101.944112	14.563021
19.490639	1112.148370	14.568039
19.545225	1122.181986	14.573056
19.553434	1120.542556	14.578074
19.822084	1127.939632	14.583091
20.083470	1124.345741	14.588109
20.018686	1123.621517	14.593127
19.593026	1113.630971	14.598144
19.656469	1110.563937	14.603162
19.508834	1113.896215	14.608179
19.800515	1110.311483	14.613197
19.896353	1115.549839	14.618215
20.270857	1122.301059	14.623232
20.237252	1116.423019	14.628250
19.395092	1109.706062	14.633267
20.014120	1109.437096	14.638285
20.119257	1113.340490	14.643303
19.950819	1115.671128	14.648320
20.238005	1111.245828	14.653338
20.000588	1115.423654	14.658355
20.158119	1094.464467	14.663373
19.785463	1093.438086	14.668391
20.049793	1108.656867	14.673408
20.502133	1103.010561	14.678426
19.788145	1098.494754	14.683443
19.838047	1095.536655	14.688461
19.927154	1100.772971	14.693479
20.165019	1108.583390	14.698496
20.214841	1110.850722	14.703514
20.202749	1114.782189	14.708531
20.345072	1106.660526	14.713549
20.497778	1121.068303	14.718567
20.501878	1106.524459	14.723584
20.366452	1103.792315	14.728602
20.192991	1096.834721	14.733619
20.317457	1097.914927	14.738637
20.209117	1097.505387	14.743655
20.209740	1099.389144	14.748672
20.396284	1097.918211	14.753690
20.342115	1107.574170	14.758707
20.780363	1105.105684	14.763725
20.367108	1101.505795	14.768743
20.259647	1099.444196	14.773760
20.201131	1101.339714	14.778778
20.038123	1106.920918	14.783795
20.371965	1100.355290	14.788813
20.396067	1115.445751	14.793831
20.373857	1111.433088	14.798848
20.491416	1101.297878	14.803866
20.082700	1112.501475	14.808883
20.340387	1108.454671	14.813901
20.323094	1110.062665	14.818919
20.344653	1122.630409	14.823936
20.872925	1122.138683	14.828954
20.357208	1133.495047	14.833971
20.865259	1138.132101	14.838989
20.783918	1141.133338	14.844007
21.053694	1128.016697	14.849024
20.763809	1110.938146	14.854042
20.496567	1113.436320	14.859059
20.768545	1107.503746	14.864077
20.745418	1124.009864	14.869095
20.906900	1126.716568	14.874112
21.047705	1128.868053	14.879130
21.075310	1125.898680	14.884147
21.128115	1101.325443	14.889165
21.247534	1106.228012	14.894183
21.216112	1098.637076	14.899200
21.217909	1087.901378	14.904218
21.072673	1099.394003	14.909235
20.873292	1090.576593	14.914253
21.071759	1097.505765	14.919271
20.932616	1098.172943	14.924288
20.886819	1095.462179	14.929306
21.023917	1095.260021	14.934323
20.921967	1095.051384	14.939341
20.772193	1096.202983	14.944359
20.794580	1096.037142	14.949376
20.669271	1097.744121	14.954394
20.863142	1119.925530	14.959411
21.242298	1124.094962	14.964429
20.932659	1133.438526	14.969447
21.080545	1141.121739	14.974464
21.323826	1128.933473	14.979482
21.129889	1130.678589	14.984499
21.296082	1128.797650	14.989517
21.131706	1146.334629	14.994535
21.337462	1137.756397	14.999552
21.432900	1126.066614	15.004570
21.159852	1130.663717	15.009587
21.347964	1122.036842	15.014605
21.391643	1131.059311	15.019623
21.462456	1128.942599	15.024640
21.473443	1124.368941	15.029658
21.193246	1126.088972	15.034675
21.538534	1125.776359	15.039693
21.574505	1126.392495	15.044711
21.378755	1128.015868	15.049728
21.790030	1124.333774	15.054746
21.356058	1123.741152	15.059763
21.498738	1121.776708	15.064781
21.511090	1125.338394	15.069799
21.441046	1121.424592	15.074816
21.760816	1122.474035	15.079834
21.529807	1135.114318	15.084851
21.195960	1126.932912	15.089869
21.466018	1138.260740	15.094887
21.974014	1158.291437	15.099904
22.041949	1149.056119	15.104922
21.786018	1150.992206	15.109939
21.650964	1144.187674	15.114957
21.572180	1147.138885	15.119975
21.900548	1154.291448	15.124992
22.244492	1150.918125	15.130010
21.637872	1160.986845	15.135027
21.694007	1155.600214	15.140045
21.956112	1152.514450	15.145063
22.223403	1156.557536	15.150080
22.302775	1151.037930	15.155098
21.887477	1150.844958	15.160115
22.052710	1137.347207	15.165133
22.196388	1137.060104	15.170151
21.775110	1132.537942	15.175168
21.649595	1133.599703	15.180186
21.534466	1149.532518	15.185203
21.880922	1146.814666	15.190221
22.340128	1147.032386	15.195239
22.175711	1150.282019	15.200256
22.223394	1145.905423	15.205274
22.284715	1154.343506	15.210291
22.363883	1149.451474	15.215309
22.371876	1146.225904	15.220327
22.081890	1150.978175	15.225344
22.171273	1143.042813	15.230362
22.037099	1149.251915	15.235379
22.235074	1139.073838	15.240397
22.381619	1136.037133	15.245415
22.019169	1143.770600	15.250432
22.152908	1147.702337	15.255450
22.242043	1153.215823	15.260467
22.051085	1150.765299	15.265485
22.513667	1145.231059	15.270503
22.099554	1154.721852	15.275520
22.424794	1159.919876	15.280538
22.158916	1165.448057	15.285555
22.548302	1175.803820	15.290573
22.715876	1174.063981	15.295591
22.453417	1178.875874	15.300608
22.708177	1176.079502	15.305626
22.626944	1180.189753	15.310643
22.860245	1174.835983	15.315661
22.745624	1169.592973	15.320679
22.769213	1172.070951	15.325696
22.949874	1159.110768	15.330714
22.783649	1168.606586	15.335731
22.930894	1155.582256	15.340749
22.759276	1148.697166	15.345767
22.667395	1142.477594	15.350784
22.686759	1134.458952	15.355802
22.569932	1157.427272	15.360819
22.835926	1168.856974	15.365837
23.177969	1169.003546	15.370855
22.966103	1168.259975	15.375872
23.243863	1166.964477	15.380890
22.780676	1152.921575	15.385907
22.828315	1157.858487	15.390925
22.891664	1166.412772	15.395943
22.898367	1175.027228	15.400960
23.206811	1171.879064	15.405978
23.115474	1173.124139	15.410995
23.056524	1177.269281	15.416013
23.353008	1173.430203	15.421031
23.194252	1171.927860	15.426048
23.314643	1163.562562	15.431066
22.917111	1156.535353	15.436083
23.017617	1151.835057	15.441101
23.142119	1161.472095	15.446119
23.265671	1175.737904	15.451136
23.718291	1171.274959	15.456154
23.156241	1158.123594	15.461171
23.335305	1161.932085	15.466189
23.349807	1162.874603	15.471207
23.319632	1165.827216	15.476224
23.472712	1165.643277	15.481242
22.923701	1166.535801	15.486259
22.955299	1173.140286	15.491277
23.429992	1165.839123	15.496295
23.339700	1177.297512	15.501312
23.365732	1169.697027	15.506330
23.218770	1178.063708	15.511347
23.120497	1175.470671	15.516365
23.466851	1177.057827	15.521383
23.248869	1176.014489	15.526400
23.586514	1165.608549	15.531418
23.400959	1169.317185	15.536435
23.712186	1177.257614	15.541453
23.497239	1166.514840	15.546471
23.322343	1177.349854	15.551488
23.687611	1186.308870	15.556506
23.821807	1195.926607	15.561523
24.073526	1196.466079	15.566541
23.771693	1191.742236	15.571559
23.706537	1194.132159	15.576576
23.579179	1186.503916	15.581594
23.784942	1190.672944	15.586611
23.399366	1198.689394	15.591629
23.979903	1186.933808	15.596647
23.752852	1201.543907	15.601664
23.691521	1204.195002	15.606682
23.619701	1198.188616	15.611699
23.531108	1198.464761	15.616717
24.050404	1197.875703	15.621735
23.878119	1199.652674	15.626752
23.884259	1201.148533	15.631770
23.704157	1199.783969	15.636787
23.957855	1214.542029	15.641805
24.258637	1209.295181	15.646823
24.088145	1224.614816	15.651840
24.354200	1213.956138	15.656858
24.374775	1212.710308	15.661875
24.049757	1204.535667	15.666893
24.337751	1193.158035	15.671911
24.208823	1195.879769	15.676928
24.242713	1190.084223	15.681946
24.297980	1192.392002	15.686963
24.199102	1205.062036	15.691981
24.696087	1202.571212	15.696999
24.595960	1200.872154	15.702016
24.841849	1192.391575	15.707034
24.422601	1177.768161	15.712051
24.117579	1187.123591	15.717069
24.351330	1178.220631	15.722087
24.250645	1183.106523	15.727104
24.140606	1180.165443	15.732122
24.279173	1198.784570	15.737139
24.427877	1219.899616	15.742157
24.520731	1214.359645	15.747175
24.381808	1222.660060	15.752192
24.501020	1220.545557	15.757210
24.750639	1211.834040	15.762227
24.389992	1220.336124	15.767245
24.737722	1215.059848	15.772263
24.550683	1222.609588	15.777280
24.523187	1215.444705	15.782298
24.808923	1212.909332	15.787315
24.833232	1218.442237	15.792333
24.963653	1203.489994	15.797351
24.790556	1212.234634	15.802368
24.724477	1214.108190	15.807386
25.008200	1219.087524	15.812403
25.055326	1213.324816	15.817421
25.226193	1210.106121	15.822439
25.100589	1213.530832	15.827456
25.079599	1214.681587	15.832474
25.299643	1210.926416	15.837491
25.121049	1214.289431	15.842509
25.273690	1211.903652	15.847527
25.149873	1215.807977	15.852544
25.235525	1211.615622	15.857562
25.072800	1207.832101	15.862579
24.960881	1207.101111	15.867597
25.014385	1204.108932	15.872615
25.225287	1209.740855	15.877632
24.998157	1216.178362	15.882650
25.102899	1208.568762	15.887667
25.029310	1212.255719	15.892685
25.537694	1202.700594	15.897703
25.377405	1214.037533	15.902720
25.091104	1208.097759	15.907738
25.371435	1203.231455	15.912755
25.167898	1215.052315	15.917773
25.113009	1207.304191	15.922791
25.171077	1209.832369	15.927808
25.119323	1205.304903	15.932826
25.490408	1213.428741	15.937843
25.084405	1220.185231	15.942861
25.333402	1221.662926	15.947879
25.232119	1241.483601	15.952896
25.306688	1238.459581	15.957914
25.378139	1237.291150	15.962931
25.241500	1241.810188	15.967949
25.620290	1231.882813	15.972967
25.621185	1237.180237	15.977984
25.618978	1236.018098	15.983002
25.971863	1235.369588	15.988019
25.462232	1239.076785	15.993037
25.645328	1236.779659	15.998055
25.503847	1237.795253	16.003072
25.457820	1241.490251	16.008090
25.836225	1254.464751	16.013107
25.797978	1264.546508	16.018125
25.699491	1268.013984	16.023143
25.836759	1266.920478	16.028160
26.056264	1270.359709	16.033178
26.055913	1269.893701	16.038195
25.674939	1263.595969	16.043213
26.137199	1263.984442	16.048231
26.029902	1275.699256	16.053248
25.934561	1265.153139	16.058266
25.930264	1266.201530	16.063283
25.857746	1272.409527	16.068301
25.561316	1269.698895	16.073319
25.804239	1266.033620	16.078336
26.042224	1275.270057	16.083354
26.457527	1276.979269	16.088371
26.133511	1287.368196	16.093389
26.366627	1283.895088	16.098407
26.539196	1289.897553	16.103424
26.812794	1273.555029	16.108442
26.522947	1256.084193	16.113459
26.408319	1266.151827	16.118477
26.453970	1261.668451	16.123495
26.640957	1253.797578	16.128512
26.437050	1248.320906	16.133530
26.527985	1250.472004	16.138547
26.307586	1252.448676	16.143565
26.750152	1255.895850	16.148583
26.785197	1243.886458	16.153600
26.518702	1251.615507	16.158618
26.954139	1254.705996	16.163635
26.762243	1255.900801	16.168653
26.609760	1250.946310	16.173671
26.612724	1255.341057	16.178688
26.300536	1254.503072	16.183706
26.395139	1257.154733	16.188723
26.603855	1256.536000	16.193741
26.578222	1253.882103	16.198759
26.716474	1257.995007	16.203776
26.706627	1280.206442	16.208794
27.069624	1276.036648	16.213811
26.932463	1279.751864	16.218829
26.915124	1280.153610	16.223847
26.923065	1279.240569	16.228864
26.949553	1277.964229	16.233882
26.777495	1281.942698	16.238899
26.936408	1285.042367	16.243917
26.907616	1280.797291	16.248935
26.833712	1278.582870	16.253952
26.731924	1283.224886	16.258970
27.027048	1279.225776	16.263987
27.066906	1281.286913	16.269005
27.217857	1277.001446	16.274023
27.292434	1280.023742	16.279040
27.046879	1272.286290	16.284058
27.125627	1283.338035	16.289075
27.271969	1281.889884	16.294093
27.228914	1270.877634	16.299111
27.275930	1276.443020	16.304128
27.085613	1282.896506	16.309146
27.511485	1271.147569	16.314163
27.413224	1278.416501	16.319181
27.465691	1271.258429	16.324199
27.764058	1276.056621	16.329216
27.740004	1283.444367	16.334234
27.691769	1270.714508	16.339251
27.391660	1283.776187	16.344269
27.245353	1275.202633	16.349287
27.450208	1281.072586	16.354304
27.446356	1279.533952	16.359322
27.795880	1267.722464	16.364339
27.869759	1275.948303	16.369357
27.775840	1278.550870	16.374375
27.632662	1270.975204	16.379392
27.326554	1278.458863	16.384410
27.744745	1271.971320	16.389427
27.535062	1276.839857	16.394445
27.875447	1294.498931	16.399463
28.043288	1292.362193	16.404480
27.886593	1286.454471	16.409498
27.953031	1282.997545	16.414515
27.772567	1285.044772	16.419533
28.193503	1290.341953	16.424551
27.899387	1285.076264	16.429568
28.111076	1305.462902	16.434586
28.391400	1287.542115	16.439603
28.073547	1276.150569	16.444621
27.929387	1275.482394	16.449639
28.178750	1274.180173	16.454656
28.290804	1278.770638	16.459674
28.225997	1268.511976	16.464691
28.103452	1278.456916	16.469709
27.960656	1269.982782	16.474727
28.103774	1275.972008	16.479744
28.266132	1292.984983	16.484762
28.283897	1297.911926	16.489779
28.685816	1304.923250	16.494797
28.455828	1298.464678	16.499815
28.673037	1305.069981	16.504832
28.648274	1295.038524	16.509850
28.274877	1271.830050	16.514867
28.215889	1285.277385	16.519885
28.288632	1295.225039	16.524903
28.394485	1303.154265	16.529920
28.284015	1301.180536	16.534938
28.461552	1293.281680	16.539955
28.169251	1301.845325	16.544973
28.183000	1300.739199	16.549991
28.302377	1304.119429	16.555008
28.094636	1314.652503	16.560026
28.511733	1314.607913	16.565043
28.821418	1325.537987	16.570061
28.867102	1331.526833	16.575079
29.069245	1325.884869	16.580096
28.534567	1329.902922	16.585114
28.698906	1326.378596	16.590131
28.726242	1330.513428	16.595149
28.712323	1329.878408	16.600167
28.997154	1333.826513	16.605184
28.960524	1336.355432	16.610202
28.886137	1333.277319	16.615219
28.661750	1328.217782	16.620237
28.795426	1333.845609	16.625255
29.156212	1326.975430	16.630272
29.095887	1328.100818	16.635290
29.161498	1320.796061	16.640307
29.110773	1322.998578	16.645325
29.044130	1326.360796	16.650343
29.608964	1326.949212	16.655360
29.301976	1330.341386	16.660378
29.309040	1323.103802	16.665395
29.145901	1328.232753	16.670413
29.452963	1327.832768	16.675431
29.346330	1324.189140	16.680448
29.008147	1322.236579	16.685466
29.267346	1331.222691	16.690483
29.170023	1338.026543	16.695501
29.066904	1357.117369	16.700519
29.597856	1352.605183	16.705536
29.416680	1356.684392	16.710554
29.490082	1361.809225	16.715571
29.396283	1358.170158	16.720589
29.567528	1351.198284	16.725607
30.051853	1351.970895	16.730624
29.724354	1356.147559	16.735642
29.882795	1353.589542	16.740659
29.838328	1347.265976	16.745677
29.968706	1348.327505	16.750695
30.043528	1343.966832	16.755712
29.951618	1349.901698	16.760730
30.108208	1344.089321	16.765747
29.955510	1350.615738	16.770765
30.032856	1346.257796	16.775783
30.176506	1331.673705	16.780800
29.949668	1324.905551	16.785818
29.874462	1309.038060	16.790835
30.427238	1314.188224	16.795853
30.001234	1307.868009	16.800871
30.259894	1302.688339	16.805888
29.942535	1308.399895	16.810906
29.873756	1307.664907	16.815923
29.906073	1316.051976	16.820941
29.854832	1329.875619	16.825959
30.203260	1328.340853	16.830976
29.975805	1341.000005	16.835994
29.959424	1335.168242	16.841011
30.220663	1334.369552	16.846029
30.264029	1340.365085	16.851047
30.615683	1338.725848	16.856064
29.993219	1347.247338	16.861082
30.233768	1338.259699	16.866099
30.180379	1332.382490	16.871117
30.067731	1351.563074	16.876135
30.768022	1361.189540	16.881152
30.507352	1375.388053	16.886170
30.691199	1380.570589	16.891187
30.925692	1375.977565	16.896205
30.754208	1357.398843	16.901223
30.981014	1358.713300	16.906240
30.621458	1344.498734	16.911258
30.481241	1334.983998	16.916275
30.664934	1336.573302	16.921293
30.881238	1349.336539	16.926311
30.860188	1351.535328	16.931328
30.749650	1359.865367	16.936346
30.821368	1357.339032	16.941363
31.209214	1352.520232	16.946381
30.449000	1359.306300	16.951399
30.887742	1354.214903	16.956416
30.842112	1367.828993	16.961434
31.139045	1370.663310	16.966451
30.818533	1367.758226	16.971469
30.671841	1380.169789	16.976487
30.895293	1370.623947	16.981504
30.702188	1369.817023	16.986522
30.936635	1367.206656	16.991539
30.787587	1367.882965	16.996557
31.041200	1384.700225	17.001575
31.213031	1398.842499	17.006592
31.201644	1402.342432	17.011610
31.482080	1390.955671	17.016627
31.477155	1391.679376	17.021645
31.117711	1406.310015	17.026663
31.568701	1403.070880	17.031680
31.175712	1404.117106	17.036698
31.201291	1398.479943	17.041715
31.408072	1394.425353	17.046733
31.314311	1407.626981	17.051751
31.920036	1402.389418	17.056768
31.466340	1392.423803	17.061786
31.655518	1393.676777	17.066803
31.651852	1396.957324	17.071821
31.663977	1402.458454	17.076839
31.907287	1384.507859	17.081856
31.508660	1386.123512	17.086874
31.513858	1390.322655	17.091891
31.743278	1390.867007	17.096909
32.076862	1390.146492	17.101927
32.001826	1384.222849	17.106944
32.037623	1388.613772	17.111962
32.018656	1389.250433	17.116979
32.175886	1384.384772	17.121997
31.958823	1382.251126	17.127015
32.019977	1382.657594	17.132032
31.797324	1385.167718	17.137050
31.637347	1391.241034	17.142067
31.918498	1385.148571	17.147085
31.961328	1395.781547	17.152103
32.115008	1401.717106	17.157120
32.243833	1416.612177	17.162138
32.308137	1421.494446	17.167155
32.531159	1411.646291	17.172173
32.236124	1420.513599	17.177191
32.515579	1413.803697	17.182208
32.494316	1408.352237	17.187226
32.282907	1423.161133	17.192243
32.603503	1410.235444	17.197261
32.288101	1416.801822	17.202279
32.728254	1410.855460	17.207296
32.937308	1410.055172	17.212314
32.691222	1391.310811	17.217331
32.765074	1385.232989	17.222349
32.376418	1374.927093	17.227367
32.691544	1366.144015	17.232384
32.620836	1381.404369	17.237402
32.412844	1376.685403	17.242419
32.926183	1388.353442	17.247437
32.383482	1403.871102	17.252455
32.508197	1394.703400	17.257472
32.909734	1409.004497	17.262490
32.690198	1404.239403	17.267507
32.971945	1405.535317	17.272525
32.843297	1405.590936	17.277543
33.128083	1400.371869	17.282560
32.975304	1398.406708	17.287578
32.815839	1406.573617	17.292595
32.979159	1407.148993	17.297613
32.918626	1406.672868	17.302631
33.224423	1402.141651	17.307648
33.079473	1410.635682	17.312666
32.872307	1402.432759	17.317683
33.014859	1403.227713	17.322701
32.994283	1410.765335	17.327719
33.215037	1401.485666	17.332736
32.910656	1411.757646	17.337754
33.102493	1428.754472	17.342771
33.396044	1431.936601	17.347789
33.523411	1440.115875	17.352807
33.709017	1425.101526	17.357824
33.861612	1436.827365	17.362842
33.453859	1437.596513	17.367859
34.105211	1423.821961	17.372877
33.459277	1412.402749	17.377895
33.461268	1399.141247	17.382912
33.596180	1411.192431	17.387930
33.497283	1415.913535	17.392947
33.789961	1423.289453	17.397965
33.566162	1431.678049	17.402983
33.696231	1431.617207	17.408000
33.647353	1432.932831	17.413018
33.684492	1432.101165	17.418035
33.818789	1433.287247	17.423053
33.805794	1436.990995	17.428071
33.780111	1427.397002	17.433088
34.071607	1430.824743	17.438106
33.807117	1441.237774	17.443123
33.615339	1429.807128	17.448141
33.792319	1431.050708	17.453159
33.902388	1427.814476	17.458176
33.857473	1441.298986	17.463194
34.055803	1450.053517	17.468211
34.422530	1443.126005	17.473229
34.365948	1452.286915	17.478247
34.299296	1445.138251	17.483264
34.177930	1443.087568	17.488282
34.328383	1444.348534	17.493299
34.362356	1433.647032	17.498317
34.541066	1441.837491	17.503335
34.109714	1438.182250	17.508352
34.272600	1437.504565	17.513370
34.515591	1444.596598	17.518387
34.712151	1430.843408	17.523405
33.786275	1440.214784	17.528423
34.335315	1438.610963	17.533440
34.377393	1442.094179	17.538458
34.351632	1457.486928	17.543475
34.974307	1459.746070	17.548493
34.892987	1473.546082	17.553511
34.885865	1465.163941	17.558528
34.883934	1460.076187	17.563546
34.786083	1454.600778	17.568563
35.040513	1452.331573	17.573581
35.143785	1462.264436	17.578599
34.781642	1448.767125	17.583616
34.765608	1447.510410	17.588634
34.757418	1472.631658	17.593651
35.212684	1464.204844	17.598669
35.332700	1456.739048	17.603687
35.094087	1457.595150	17.608704
35.184681	1457.719977	17.613722
35.216551	1468.698909	17.618739
35.446771	1462.617605	17.623757
35.111270	1448.291875	17.628775
35.042335	1442.051849	17.633792
35.158830	1453.949425	17.638810
35.283986	1471.539617	17.643827
35.262909	1465.167641	17.648845
35.353856	1467.309320	17.653863
35.088320	1458.577848	17.658880
35.493286	1467.056050	17.663898
35.314056	1466.264540	17.668915
35.467685	1458.250270	17.673933
35.244176	1458.860960	17.678951
35.340358	1458.810454	17.683968
35.492115	1458.096815	17.688986
35.006668	1468.164171	17.694003
35.494760	1483.021865	17.699021
35.625622	1482.080585	17.704039
35.798449	1486.433098	17.709056
35.800318	1491.848951	17.714074
35.662918	1494.958751	17.719091
35.558766	1484.042686	17.724109
36.162208	1493.128584	17.729127
36.043596	1486.584563	17.734144
35.965530	1479.509032	17.739162
36.012452	1489.047310	17.744179
36.049210	1488.155075	17.749197
36.294717	1494.945931	17.754215
36.148022	1484.077067	17.759232
36.294604	1480.365098	17.764250
36.032468	1487.844331	17.769267
36.235273	1478.980970	17.774285
35.997471	1486.259718	17.779303
35.837925	1488.167681	17.784320
36.607177	1496.975735	17.789338
36.526118	1514.205242	17.794355
36.537527	1503.254281	17.799373
36.763134	1501.294563	17.804391
36.388366	1490.658733	17.809408
36.538529	1481.201729	17.814426
36.544805	1483.130660	17.819443
36.816555	1490.336850	17.824461
36.923944	1483.510134	17.829479
36.439568	1481.426642	17.834496
36.664871	1475.781577	17.839514
36.595170	1487.600955	17.844531
36.985161	1491.987590	17.849549
37.135839	1501.839796	17.854567
36.827152	1484.508433	17.859584
37.022790	1481.403690	17.864602
36.906695	1479.653702	17.869619
37.050405	1473.915456	17.874637
37.015806	1481.654252	17.879655
36.885289	1490.915221	17.884672
37.240232	1497.706461	17.889690
36.965058	1505.168177	17.894707
37.059796	1502.204939	17.899725
36.937538	1497.355992	17.904743
36.730515	1500.727319	17.909760
37.465004	1495.889268	17.914778
37.046452	1504.716839	17.919795
37.144675	1499.023517	17.924813
36.935812	1491.788930	17.929831
37.284002	1504.348569	17.934848
37.280521	1498.739016	17.939866
37.183214	1507.104739	17.944883
37.383471	1511.670039	17.949901
37.400543	1519.879823	17.954919
37.591499	1514.942001	17.959936
37.933774	1522.753060	17.964954
38.000200	1523.785821	17.969971
37.708411	1506.038253	17.974989
37.673044	1496.127318	17.980007
37.702566	1495.678010	17.985024
37.850353	1493.329607	17.990042
37.475325	1499.027946	17.995059
37.548860	1513.203924	18.000077
37.769237	1521.722170	18.005095
37.716966	1527.219834	18.010112
37.901924	1525.629440	18.015130
37.467227	1533.408132	18.020147
37.644674	1525.022169	18.025165
37.804113	1524.470247	18.030183
37.799159	1537.673816	18.035200
38.234988	1541.808783	18.040218
37.922737	1555.702223	18.045235
38.307158	1550.995741	18.050253
38.571892	1554.488177	18.055271
38.607303	1552.768606	18.060288
38.766460	1536.064442	18.065306
38.565744	1523.180884	18.070323
38.460041	1522.264993	18.075341
38.467175	1515.239511	18.080359
38.203958	1506.814319	18.085376
38.381944	1525.992664	18.090394
38.531199	1532.901442	18.095411
38.778951	1538.208488	18.100429
38.963016	1543.394586	18.105447
38.950625	1541.080178	18.110464
38.816340	1522.566751	18.115482
38.349345	1522.519339	18.120499
38.422441	1530.344658	18.125517
38.736097	1534.966778	18.130535
38.944219	1544.198479	18.135552
38.824745	1538.956540	18.140570
39.127625	1546.833977	18.145587
39.012165	1541.887041	18.150605
38.920117	1539.094487	18.155623
38.880596	1552.058911	18.160640
38.906087	1539.859928	18.165658
38.925726	1540.355164	18.170675
39.171404	1550.081829	18.175693
38.986831	1541.117614	18.180711
39.094352	1537.599893	18.185728
39.086589	1541.028786	18.190746
39.221630	1559.907986	18.195763
39.203665	1569.867686	18.200781
39.382923	1573.726641	18.205799
38.780410	1574.930011	18.210816
39.447712	1573.052266	18.215834
39.427451	1567.675780	18.220851
39.161069	1570.420732	18.225869
39.212716	1572.163422	18.230887
39.270694	1576.429466	18.235904
39.804319	1584.814777	18.240922
40.011495	1598.352957	18.245939
40.031776	1590.221329	18.250957
40.320356	1575.126793	18.255975
39.916092	1570.904438	18.260992
40.278859	1558.516523	18.266010
40.095390	1559.356413	18.271027
39.842318	1548.629920	18.276045
39.892800	1547.672418	18.281063
39.940661	1561.846786	18.286080
40.213978	1557.440982	18.291098
40.066546	1557.888292	18.296115
40.111251	1554.203803	18.301133
40.100088	1556.088386	18.306151
39.949393	1551.595311	18.311168
39.962387	1546.213720	18.316186
40.100883	1561.135282	18.321203
40.252630	1578.619224	18.326221
40.727275	1588.683591	18.331239
40.604846	1586.641333	18.336256
40.455932	1570.520030	18.341274
40.245643	1568.628936	18.346291
40.204320	1580.815339	18.351309
40.660104	1580.554503	18.356327
40.515557	1582.368262	18.361344
40.832117	1584.191498	18.366362
40.399646	1578.062004	18.371379
40.547834	1584.358384	18.376397
40.644537	1580.971185	18.381415
40.330359	1579.919730	18.386432
40.479731	1575.811608	18.391450
40.761582	1579.840585	18.396467
40.358425	1592.434546	18.401485
40.936539	1593.047154	18.406503
40.790495	1603.827688	18.411520
40.803717	1599.377143	18.416538
40.739079	1612.130816	18.421555
40.983604	1600.968746	18.426573
41.098811	1604.303276	18.431591
41.234941	1612.287883	18.436608
41.234211	1607.292795	18.441626
41.138823	1602.543304	18.446643
41.152385	1603.637185	18.451661
41.083020	1606.334561	18.456679
41.289306	1623.773697	18.461696
41.483024	1629.005469	18.466714
41.980428	1621.173564	18.471731
41.849378	1619.118556	18.476749
42.254048	1610.531144	18.481767
41.934004	1596.361772	18.486784
41.714156	1595.558870	18.491802
41.728355	1586.120378	18.496819
41.528431	1585.422052	18.501837
41.905660	1585.247845	18.506855
42.005559	1585.310109	18.511872
41.911095	1583.306134	18.516890
42.182129	1579.175110	18.521907
42.043812	1590.681914	18.526925
42.331686	1585.907549	18.531943
42.139325	1591.287881	18.536960
42.137215	1582.006817	18.541978
42.184852	1581.216713	18.546995
42.344993	1596.189055	18.552013
42.596977	1598.600150	18.557031
42.297669	1589.044669	18.562048
41.898707	1580.289945	18.567066
42.431861	1587.170221	18.572083
42.152958	1596.762515	18.577101
42.032293	1583.754234	18.582119
41.836154	1586.888739	18.587136
41.852743	1600.295487	18.592154
42.363829	1605.216828	18.597171
42.013806	1615.742563	18.602189
42.582380	1614.875649	18.607207
42.469185	1615.421229	18.612224
42.768074	1620.745821	18.617242
42.682580	1610.251380	18.622259
42.423982	1618.733634	18.627277
42.774068	1616.319826	18.632295
42.519889	1619.701348	18.637312
42.951682	1623.590943	18.642330
42.908730	1625.809539	18.647347
42.951633	1643.033229	18.652365
43.581203	1638.719595	18.657383
43.289463	1626.304173	18.662400
43.025305	1620.886951	18.667418
43.065177	1611.135138	18.672435
42.839683	1615.058366	18.677453
42.865200	1618.445545	18.682471
43.307098	1633.493711	18.687488
43.447041	1641.444238	18.692506
43.434008	1638.508268	18.697523
43.303594	1638.357092	18.702541
43.412965	1634.911090	18.707559
43.551172	1640.709539	18.712576
43.525846	1644.281914	18.717594
43.544548	1640.775727	18.722611
43.208428	1636.290888	18.727629
43.211819	1637.807323	18.732647
43.438336	1634.163971	18.737664
43.610876	1642.470913	18.742682
43.343813	1636.989205	18.747699
43.377945	1647.414345	18.752717
43.557173	1663.124932	18.757735
43.809591	1667.751327	18.762752
44.050503	1661.751641	18.767770
44.237211	1669.318847	18.772787
43.829732	1668.359607	18.777805
44.125625	1671.529193	18.782823
44.135228	1666.822928	18.787840
44.070107	1664.044397	18.792858
44.020536	1667.043230	18.797875
44.377347	1664.967673	18.802893
44.618249	1656.752236	18.807911
44.627526	1663.381099	18.812928
44.394109	1676.434819	18.817946
44.623507	1667.472065	18.822963
44.458706	1673.503376	18.827981
44.761841	1673.035924	18.832999
44.427109	1664.532723	18.838016
44.518818	1674.453858	18.843034
45.023054	1666.169616	18.848051
44.543814	1667.429745	18.853069
44.774770	1665.034868	18.858087
44.626160	1664.071348	18.863104
44.624146	1674.415089	18.868122
45.247095	1653.038713	18.873139
44.960030	1665.423746	18.878157
44.930253	1665.535435	18.883175
45.014053	1664.483039	18.888192
44.838983	1667.256982	18.893210
44.948434	1671.025946	18.898227
44.725643	1670.212110	18.903245
45.198929	1676.933047	18.908263
45.063883	1689.220093	18.913280
45.072820	1692.856098	18.918298
45.253080	1695.845622	18.923315
45.060909	1695.831050	18.928333
45.265565	1693.107451	18.933351
45.170759	1692.894079	18.938368
45.248626	1694.772599	18.943386
45.531357	1685.681318	18.948403
45.332362	1691.223020	18.953421
45.265354	1690.665280	18.958439
45.385047	1704.426701	18.963456
45.333474	1720.025167	18.968474
45.522728	1715.446228	18.973491
45.592493	1725.134413	18.978509
45.781709	1708.814853	18.983527
45.913147	1714.667994	18.988544
45.516100	1725.000800	18.993562
45.763324	1722.513456	18.998579
45.870661	1723.428432	19.003597
45.942301	1703.489344	19.008615
46.119157	1713.870424	19.013632
45.873375	1725.885676	19.018650
46.579189	1727.882274	19.023667
46.619221	1737.020662	19.028685
46.417939	1721.471657	19.033703
46.494649	1709.477841	19.038720
46.302733	1715.452634	19.043738
46.623385	1701.205426	19.048755
46.458199	1700.164333	19.053773
46.187913	1695.414638	19.058791
46.424255	1710.374080	19.063808
46.787259	1723.159005	19.068826
46.745094	1712.064797	19.073843
46.514085	1731.350882	19.078861
46.541413	1725.937721	19.083879
46.772884	1729.782953	19.088896
46.920475	1727.743998	19.093914
46.918916	1728.151017	19.098931
46.782124	1731.918642	19.103949
46.896666	1727.020178	19.108967
46.776880	1726.067629	19.113984
46.810319	1719.047935	19.119002
47.118862	1726.338696	19.124019
46.900441	1725.596181	19.129037
47.027542	1716.016868	19.134055
47.117923	1729.547731	19.139072
47.125257	1745.498676	19.144090
47.377858	1748.899858	19.149107
47.505044	1759.284076	19.154125
47.654280	1753.158194	19.159143
47.760254	1748.805241	19.164160
47.119585	1756.433894	19.169178
47.368902	1753.648559	19.174195
47.652628	1756.768603	19.179213
47.751260	1759.392912	19.184231
47.968844	1751.436406	19.189248
47.481194	1754.264090	19.194266
47.646257	1751.902158	19.199283
47.526750	1758.818923	19.204301
47.477331	1760.628763	19.209319
47.825407	1759.682209	19.214336
47.394378	1762.502094	19.219354
47.887809	1767.093338	19.224371
47.608381	1776.511418	19.229389
47.951022	1779.335488	19.234407
47.957059	1772.697871	19.239424
47.897977	1785.320843	19.244442
48.241371	1780.627386	19.249459
48.151481	1782.211249	19.254477
47.857080	1784.338823	19.259495
48.190641	1799.964545	19.264512
48.409031	1812.153009	19.269530
48.476108	1805.508027	19.274547
48.427901	1812.816559	19.279565
48.600775	1817.434910	19.284583
48.701911	1802.236149	19.289600
48.839455	1809.362740	19.294618
48.887000	1803.611555	19.299635
48.728818	1809.493396	19.304653
48.456706	1805.910913	19.309671
48.936400	1801.662997	19.314688
48.949487	1807.622385	19.319706
49.024589	1797.747691	19.324723
48.694683	1810.937187	19.329741
48.796686	1805.903371	19.334759
49.004438	1808.382060	19.339776
49.031218	1816.553385	19.344794
49.413456	1822.207952	19.349811
49.045643	1827.139456	19.354829
49.140621	1824.459586	19.359847
49.398051	1827.564707	19.364864
49.329439	1826.246193	19.369882
49.673266	1827.916911	19.374899
49.321564	1828.527580	19.379917
49.439109	1829.921981	19.384935
49.655257	1822.231035	19.389952
49.509097	1829.347523	19.394970
49.845205	1820.073702	19.399987
49.631482	1822.091858	19.405005
49.582841	1820.489719	19.410023
49.633970	1815.367866	19.415040
49.604416	1818.649245	19.420058
49.830869	1834.249822	19.425075
49.975894	1842.161028	19.430093
50.186984	1846.598648	19.435111
50.400386	1853.274897	19.440128
50.047882	1850.952584	19.445146
50.141979	1842.911752	19.450163
50.303620	1841.592909	19.455181
50.193937	1851.797507	19.460199
50.474454	1847.031369	19.465216
50.673485	1846.461463	19.470234
50.884204	1843.491161	19.475251
50.549828	1844.950943	19.480269
50.439519	1845.900388	19.485287
50.576236	1840.889948	19.490304
51.003687	1845.332295	19.495322
51.088676	1839.931201	19.500339
50.741007	1827.092195	19.505357
50.725027	1824.155496	19.510375
51.109495	1819.420973	19.515392
50.741323	1828.399048	19.520410
50.928401	1836.374549	19.525427
51.004712	1838.700201	19.530445
50.897281	1842.623623	19.535463
51.110010	1834.375354	19.540480
50.763346	1839.783683	19.545498
51.178278	1840.235918	19.550515
51.139776	1828.372900	19.555533
50.795118	1838.714035	19.560551
51.396726	1836.951078	19.565568
50.982461	1840.506007	19.570586
51.153812	1847.755760	19.575603
51.517896	1858.600826	19.580621
51.300870	1866.259388	19.585639
51.904015	1863.444582	19.590656
51.335049	1868.919257	19.595674
51.418578	1865.412127	19.600691
51.317720	1857.779952	19.605709
51.176535	1866.924405	19.610727
51.655928	1873.668828	19.615744
51.676465	1890.344519	19.620762
51.795382	1892.852498	19.625779
51.985579	1892.276967	19.630797
51.712836	1894.743495	19.635815
51.901116	1901.855823	19.640832
52.027559	1908.905950	19.645850
52.194557	1897.878947	19.650867
51.974205	1893.034701	19.655885
52.020833	1903.025653	19.660903
52.254402	1894.454999	19.665920
51.790426	1912.418833	19.670938
52.070365	1923.518827	19.675955
52.355660	1935.434100	19.680973
52.151435	1932.623434	19.685991
52.574465	1925.912376	19.691008
52.335689	1929.850480	19.696026
52.748389	1928.586912	19.701043
52.665752	1924.916728	19.706061
52.683075	1925.734414	19.711079
53.079359	1931.167793	19.716096
52.968899	1947.011674	19.721114
53.172039	1947.237165	19.726131
53.293765	1930.821458	19.731149
52.945836	1923.790013	19.736167
53.149458	1921.053160	19.741184
52.871289	1929.506538	19.746202
53.343308	1941.052703	19.751219
53.409555	1944.278087	19.756237
53.138291	1954.068552	19.761255
53.516110	1942.514475	19.766272
53.253196	1951.452750	19.771290
53.583204	1942.501133	19.776307
53.778818	1939.462447	19.781325
53.309713	1940.953207	19.786343
53.603041	1933.365965	19.791360
53.562541	1935.372383	19.796378
53.505791	1939.039401	19.801395
54.041109	1931.535716	19.806413
53.679995	1936.825602	19.811431
53.909232	1926.849713	19.816448
53.807760	1931.946997	19.821466
53.766384	1945.485297	19.826483
53.933458	1959.219021	19.831501
53.942258	1965.296505	19.836519
53.973678	1968.033949	19.841536
54.293942	1968.427847	19.846554
53.720897	1972.735883	19.851571
54.269732	1961.336944	19.856589
54.178594	1961.616672	19.861607
54.800868	1957.260854	19.866624
54.237051	1968.312786	19.871642
54.535441	1971.235954	19.876659
54.816676	1978.466393	19.881677
54.609708	1975.342779	19.886695
54.810481	1981.708176	19.891712
54.962782	1983.067308	19.896730
54.903146	1988.873843	19.901747
55.347286	1972.831096	19.906765
55.705830	1957.004510	19.911783
55.315230	1951.795512	19.916800
55.314857	1947.854216	19.921818
55.075449	1941.262284	19.926835
55.611713	1943.813376	19.931853
55.159809	1942.834306	19.936871
55.606393	1930.741281	19.941888
55.537903	1932.103895	19.946906
55.397318	1929.809868	19.951923
55.657025	1940.641172	19.956941
55.369937	1935.495750	19.961959
55.588113	1938.136912	19.966976
55.722364	1942.288851	19.971994
55.457432	1939.928401	19.977011
55.782944	1933.651606	19.982029
55.598172	1944.411622	19.987047
55.535912	1930.595725	19.992064
55.425553	1931.934562	19.997082
55.091939	1938.286058	20.002099
55.670980	1955.430380	20.007117
55.485023	1971.494666	20.012135
55.635888	1964.507388	20.017152
55.726363	1968.016962	20.022170
55.768355	1978.656383	20.027187
55.725433	1992.621761	20.032205
55.746734	2005.270580	20.037223
55.912411	2004.860526	20.042240
56.005430	2002.922307	20.047258
56.032285	2013.853242	20.052275
56.338534	2035.168910	20.057293
56.218599	2033.476582	20.062311
56.392984	2028.485043	20.067328
56.502616	2032.947390	20.072346
56.430899	2035.690899	20.077363
56.643312	2028.569777	20.082381
56.677730	2033.463093	20.087399
57.113799	2040.178935	20.092416
57.479442	2051.870753	20.097434
57.308289	2040.399626	20.102451
57.106574	2029.950917	20.107469
57.247635	2023.150281	20.112487
57.249639	2022.304323	20.117504
57.480952	2031.194277	20.122522
57.395891	2032.788390	20.127539
57.391599	2016.607243	20.132557
57.304108	2024.116478	20.137575
57.243924	2025.011965	20.142592
57.482206	2038.331989	20.147610
57.486121	2052.449513	20.152627
57.902897	2049.493482	20.157645
57.899697	2050.472844	20.162663
58.018090	2060.478000	20.167680
58.236012	2047.882179	20.172698
57.926457	2042.647919	20.177715
58.319175	2023.206848	20.182733
57.899718	2016.744305	20.187751
57.998538	2017.499288	20.192768
57.933751	2021.541681	20.197786
57.792777	2039.287609	20.202803
58.330818	2049.682736	20.207821
57.671984	2057.665731	20.212839
57.744344	2043.340816	20.217856
58.018366	2046.520796	20.222874
57.990474	2065.139787	20.227891
58.155948	2061.532035	20.232909
58.468965	2085.037266	20.237927
58.346673	2088.189564	20.242944
58.672861	2084.404011	20.247962
58.192214	2079.125231	20.252979
58.638171	2082.027924	20.257997
58.625736	2093.811115	20.263015
58.655083	2101.284506	20.268032
58.898289	2101.089179	20.273050
58.995454	2105.308722	20.278067
59.178504	2094.845082	20.283085
59.136571	2105.398088	20.288103
59.510478	2102.025904	20.293120
59.599336	2097.464658	20.298138
59.723738	2107.935005	20.303155
59.596589	2098.034552	20.308173
59.696292	2090.118652	20.313191
59.409382	2097.449124	20.318208
59.747200	2097.092852	20.323226
59.477742	2097.752512	20.328243
59.618184	2099.227795	20.333261
59.482190	2098.582640	20.338279
59.423882	2093.764651	20.343296
59.606358	2096.289700	20.348314
59.323977	2100.265776	20.353331
59.474563	2089.879171	20.358349
59.643091	2105.884507	20.363367
59.698037	2124.960341	20.368384
60.148350	2121.587706	20.373402
59.642456	2137.653165	20.378419
59.871566	2129.795743	20.383437
60.154364	2126.062249	20.388455
60.078520	2133.779851	20.393472
60.543043	2126.099601	20.398490
60.384953	2152.554686	20.403507
60.512636	2147.849591	20.408525
60.654969	2152.838860	20.413543
60.507725	2146.276464	20.418560
60.947105	2149.904694	20.423578
60.832980	2145.462872	20.428595
60.946375	2144.228372	20.433613
60.892790	2135.122829	20.438631
61.039836	2144.771314	20.443648
61.486580	2127.039338	20.448666
61.058431	2134.691648	20.453683
61.133452	2122.395421	20.458701
61.232709	2128.231212	20.463719
61.137805	2137.400839	20.468736
61.237822	2131.560921	20.473754
61.247235	2134.478029	20.478771
61.568830	2134.472092	20.483789
61.406371	2136.609363	20.488807
61.301064	2134.753967	20.493824
61.500246	2129.829551	20.498842
61.016679	2142.357344	20.503859
61.429244	2155.362776	20.508877
61.504655	2160.334780	20.513895
61.693033	2167.315320	20.518912
61.595371	2152.599543	20.523930
61.379441	2167.507535	20.528947
61.967916	2165.289616	20.533965
61.938329	2182.649535	20.538983
61.882018	2184.370010	20.544000
62.118167	2190.727273	20.549018
62.106640	2194.756955	20.554035
62.286722	2186.880850	20.559053
62.468502	2190.465517	20.564071
62.391597	2188.628247	20.569088
62.429670	2183.840337	20.574106
62.519807	2195.203063	20.579123
62.949713	2201.393993	20.584141
62.845917	2204.263320	20.589159
62.570493	2208.852468	20.594176
62.944715	2210.753245	20.599194
62.882005	2221.531826	20.604211
63.188171	2209.188991	20.609229
63.006922	2218.107991	20.614247
62.790941	2216.506746	20.619264
63.233113	2207.302146	20.624282
63.047569	2220.178309	20.629299
63.115759	2210.898615	20.634317
63.224334	2212.504388	20.639335
63.021559	2212.260851	20.644352
63.249048	2210.692876	20.649370
63.480261	2229.954622	20.654387
63.400188	2231.001844	20.659405
63.557878	2225.165729	20.664423
63.324626	2237.293082	20.669440
63.698533	2233.296435	20.674458
63.566576	2229.081567	20.679475
63.817124	2234.991959	20.684493
63.987028	2228.190395	20.689511
63.803924	2220.145658	20.694528
64.030885	2228.628163	20.699546
64.217520	2233.470354	20.704563
64.460487	2234.287311	20.709581
64.492912	2233.271731	20.714599
64.241170	2231.316548	20.719616
64.470831	2235.070864	20.724634
64.276270	2224.930694	20.729651
64.692870	2243.954274	20.734669
64.885776	2249.821064	20.739687
64.375899	2252.127689	20.744704
64.870391	2246.575971	20.749722
64.758889	2260.480895	20.754739
65.024943	2255.338666	20.759757
65.005968	2251.517700	20.764775
64.640364	2262.298427	20.769792
65.171145	2254.706362	20.774810
65.131989	2254.034929	20.779827
65.053828	2248.995760	20.784845
65.385315	2240.389806	20.789863
65.419446	2238.066804	20.794880
65.520634	2249.273404	20.799898
65.727824	2254.548043	20.804915
65.442620	2250.666822	20.809933
65.309096	2245.315155	20.814951
65.224112	2249.657026	20.819968
65.206726	2247.254754	20.824986
65.329334	2260.768145	20.830003
65.714669	2277.415348	20.835021
65.580348	2277.736879	20.840039
65.304811	2284.084804	20.845056
65.789404	2274.399892	20.850074
65.697750	2295.226659	20.855091
65.973795	2303.970775	20.860109
66.158285	2315.255759	20.865127
65.943689	2316.971746	20.870144
66.107525	2313.307513	20.875162
65.770792	2317.973776	20.880179
65.960302	2322.609998	20.885197
66.301020	2339.567424	20.890215
66.482068	2344.266867	20.895232
66.951156	2324.274564	20.900250
66.726208	2340.078743	20.905267
66.762256	2336.126987	20.910285
66.880175	2331.552986	20.915303
66.965506	2326.602082	20.920320
67.033106	2334.164531	20.925338
66.802148	2340.257448	20.930355
66.754483	2331.747688	20.935373
66.935567	2359.037163	20.940391
67.082711	2367.269955	20.945408
67.571229	2359.621054	20.950426
67.489818	2363.649752	20.955443
67.703299	2360.991116	20.960461
68.047702	2351.958926	20.965479
67.830100	2357.906325	20.970496
68.157343	2357.971505	20.975514
67.823969	2364.879459	20.980531
67.966522	2356.467723	20.985549
68.019234	2358.523726	20.990567
67.708047	2355.096410	20.995584
68.072028	2347.016932	21.000602
67.951325	2351.897842	21.005619
68.132885	2357.420078	21.010637
68.316127	2348.912629	21.015655
68.081070	2358.980830	21.020672
68.367692	2351.706322	21.025690
68.236405	2357.952043	21.030707
68.221236	2350.595609	21.035725
68.349750	2350.699204	21.040743
68.197556	2355.134914	21.045760
68.374009	2351.491025	21.050778
68.345696	2372.979093	21.055795
68.296278	2376.373727	21.060813
68.488090	2383.903428	21.065831
68.316852	2384.344465	21.070848
68.585248	2389.057019	21.075866
68.841611	2405.305614	21.080883
68.916909	2414.282254	21.085901
68.963207	2413.298225	21.090919
68.898558	2416.806025	21.095936
69.050255	2409.851877	21.100954
69.212878	2415.045363	21.105971
69.198636	2439.452603	21.110989
69.809503	2447.678347	21.116007
69.439295	2439.588093	21.121024
69.314603	2434.882963	21.126042
69.558591	2441.816622	21.131059
69.284926	2444.361344	21.136077
69.493578	2442.644883	21.141095
69.620589	2462.249384	21.146112
70.094410	2467.629956	21.151130
70.450116	2466.037578	21.156147
70.433833	2467.703422	21.161165
70.567955	2463.138906	21.166183
70.381018	2464.718432	21.171200
70.348787	2459.612532	21.176218
70.292222	2453.422809	21.181235
70.299662	2461.562634	21.186253
70.416177	2458.162121	21.191271
70.562953	2462.171962	21.196288
70.740873	2457.268288	21.201306
71.034627	2458.010703	21.206323
70.523225	2462.918539	21.211341
71.258947	2461.536878	21.216359
70.919902	2472.243663	21.221376
71.123880	2471.550863	21.226394
71.032205	2481.561936	21.231411
70.918844	2488.390206	21.236429
71.154474	2465.893320	21.241447
71.071450	2483.527003	21.246464
71.334551	2478.887581	21.251482
71.463894	2479.811558	21.256499
71.068094	2478.598346	21.261517
71.674297	2491.349153	21.266535
71.866086	2511.678859	21.271552
71.773546	2505.138752	21.276570
72.269207	2509.012094	21.281587
71.792345	2515.321001	21.286605
72.223849	2507.166478	21.291623
72.555905	2513.985582	21.296640
72.461427	2516.919963	21.301658
72.250026	2502.779018	21.306675
71.976664	2518.892592	21.311693
72.422592	2509.455684	21.316711
72.211887	2504.147810	21.321728
72.210805	2506.861202	21.326746
72.327542	2500.095884	21.331763
72.153896	2504.657636	21.336781
72.477676	2503.443789	21.341799
72.662571	2511.416456	21.346816
72.651979	2516.259893	21.351834
72.582853	2519.213307	21.356851
72.802097	2517.559654	21.361869
73.164860	2519.635213	21.366887
72.926268	2518.785361	21.371904
72.780654	2519.941491	21.376922
72.828818	2523.627891	21.381939
72.970274	2543.357276	21.386957
72.863255	2545.199185	21.391975
72.842223	2560.598542	21.396992
73.536573	2548.882154	21.402010
73.482707	2555.184824	21.407027
73.338948	2564.854159	21.412045
73.682391	2576.269717	21.417063
73.680613	2573.818351	21.422080
73.965167	2567.298857	21.427098
74.069582	2566.608365	21.432115
73.903696	2571.687387	21.437133
74.095202	2565.659313	21.442151
74.194324	2560.708414	21.447168
74.321906	2558.562423	21.452186
74.476832	2573.035360	21.457203
74.132933	2571.471793	21.462221
74.632117	2581.818199	21.467239
74.586890	2592.573667	21.472256
74.525628	2594.933630	21.477274
74.702187	2599.590978	21.482291
74.603075	2604.282159	21.487309
74.770416	2602.814268	21.492327
74.781300	2599.039458	21.497344
74.944367	2603.888029	21.502362
74.955128	2603.487468	21.507379
74.781756	2606.833379	21.512397
75.402316	2615.394638	21.517415
75.317087	2625.522460	21.522432
75.235281	2614.995625	21.527450
75.437940	2616.628384	21.532467
75.410911	2615.916737	21.537485
75.857019	2613.716031	21.542503
75.742967	2616.005992	21.547520
75.842190	2617.600362	21.552538
75.757044	2616.759352	21.557555
75.965822	2615.180655	21.562573
75.817081	2613.577684	21.567591
75.996344	2639.497393	21.572608
76.321706	2643.711585	21.577626
76.490317	2645.904353	21.582643
75.822222	2663.347689	21.587661
76.289015	2648.943524	21.592679
76.325761	2646.807836	21.597696
76.517465	2646.702927	21.602714
76.534025	2642.619666	21.607731
76.319612	2642.761931	21.612749
76.552660	2646.194506	21.617767
76.891831	2663.615172	21.622784
76.921270	2678.292068	21.627802
76.653792	2669.850015	21.632819
76.791285	2681.078082	21.637837
76.824178	2674.574226	21.642855
76.953658	2677.051842	21.647872
77.090278	2686.731526	21.652890
77.035174	2698.417114	21.657907
77.256438	2705.034158	21.662925
77.259725	2703.839107	21.667943
77.664080	2705.265241	21.672960
77.682311	2718.265565	21.677978
77.327844	2705.115122	21.682995
77.481252	2711.685526	21.688013
78.007542	2731.529790	21.693031
77.737918	2729.845240	21.698048
78.116589	2736.062193	21.703066
78.315870	2736.758055	21.708083
78.110525	2735.277050	21.713101
78.062418	2729.824058	21.718119
78.540915	2728.314875	21.723136
78.140362	2733.639117	21.728154
78.167146	2715.022004	21.733171
77.990492	2727.958928	21.738189
78.417788	2743.268486	21.743207
78.527484	2750.526902	21.748224
78.500117	2758.460425	21.753242
79.060625	2751.023841	21.758259
78.855521	2762.732344	21.763277
79.010446	2749.782582	21.768295
79.067762	2749.492822	21.773312
78.959940	2748.079927	21.778330
79.351036	2755.886679	21.783347
79.481197	2771.209632	21.788365
79.198324	2776.040353	21.793383
79.758714	2775.644462	21.798400
79.626346	2782.557116	21.803418
79.542130	2773.605888	21.808435
79.687247	2774.400885	21.813453
79.778406	2772.111278	21.818471
79.986342	2772.933672	21.823488
79.350160	2782.509068	21.828506
79.942185	2783.458828	21.833523
79.922062	2796.523446	21.838541
79.843512	2802.428303	21.843559
79.908697	2804.409460	21.848576
80.020355	2806.942808	21.853594
80.406742	2807.535642	21.858611
80.301755	2827.182952	21.863629
80.710038	2827.772555	21.868647
80.594455	2835.725842	21.873664
81.018062	2834.467488	21.878682
81.377377	2828.716672	21.883699
81.245306	2825.450553	21.888717
81.419747	2830.139426	21.893735
81.407831	2825.984054	21.898752
81.293230	2821.764575	21.903770
81.675217	2825.520589	21.908787
81.726780	2815.608200	21.913805
81.643945	2818.435583	21.918823
81.717387	2820.505540	21.923840
81.464351	2823.979262	21.928858
81.518822	2815.880706	21.933875
81.878894	2822.700032	21.938893
81.624441	2821.781129	21.943911
81.913891	2814.721311	21.948928
81.281771	2823.074705	21.953946
81.798792	2825.405890	21.958963
81.685545	2839.228541	21.963981
81.652483	2847.975320	21.968999
82.255438	2843.062182	21.974016
81.968426	2859.100801	21.979034
82.256612	2869.426424	21.984051
82.306695	2879.139455	21.989069
82.091136	2891.691585	21.994087
82.921312	2878.046404	21.999104
82.445911	2871.412434	22.004122
82.723816	2885.834196	22.009139
83.144283	2910.232801	22.014157
82.612076	2921.888879	22.019175
83.322955	2914.372988	22.024192
83.020508	2912.170972	22.029210
83.453950	2905.111291	22.034227
83.347205	2911.950462	22.039245
83.547304	2907.111486	22.044263
83.606677	2899.719220	22.049280
83.307431	2911.964330	22.054298
83.400677	2902.687952	22.059315
83.454937	2918.512240	22.064333
83.472002	2925.625825	22.069351
83.833059	2913.895841	22.074368
83.735920	2927.550534	22.079386
84.117132	2929.138803	22.084403
84.449039	2923.461393	22.089421
84.135665	2928.085776	22.094439
84.410082	2924.831474	22.099456
84.053919	2932.728572	22.104474
84.168553	2941.122182	22.109491
84.433606	2953.013241	22.114509
84.529870	2957.982836	22.119527
85.042669	2950.300100	22.124544
84.644487	2960.141736	22.129562
84.969802	2955.044591	22.134579
84.995274	2950.695971	22.139597
84.846384	2973.865603	22.144615
85.277640	2972.995771	22.149632
84.995424	2980.962152	22.154650
85.565637	2972.409982	22.159667
85.121654	2982.749809	22.164685
85.375693	2977.042356	22.169703
85.478040	2974.072068	22.174720
85.363078	2988.097907	22.179738
86.011085	3002.976656	22.184755
85.769117	3000.195666	22.189773
85.857634	3008.293216	22.194791
86.383552	2999.399516	22.199808
86.259771	3005.573379	22.204826
86.440642	2991.916303	22.209843
86.358557	2998.071054	22.214861
86.205993	3000.011903	22.219879
86.229849	2995.242241	22.224896
86.110486	2997.754022	22.229914
86.335329	3013.159577	22.234931
86.884948	3017.636770	22.239949
86.464147	3025.381609	22.244967
86.629787	3026.030294	22.249984
86.611652	3034.965670	22.255002
86.710977	3048.695430	22.260019
87.226011	3055.179332	22.265037
87.445061	3057.197650	22.270055
87.688906	3045.890161	22.275072
87.508807	3048.562414	22.280090
87.985469	3044.293410	22.285107
87.770379	3042.089906	22.290125
87.972484	3048.411816	22.295143
88.284536	3038.382135	22.300160
88.109905	3045.686583	22.305178
87.725608	3041.496736	22.310195
88.326355	3040.758695	22.315213
88.231330	3039.245614	22.320231
88.294455	3039.248614	22.325248
87.993434	3038.383081	22.330266
88.584021	3039.961895	22.335283
88.590235	3034.332464	22.340301
88.470550	3038.127493	22.345319
88.813167	3058.977480	22.350336
88.817847	3062.050677	22.355354
89.031068	3069.553937	22.360371
89.053820	3069.647882	22.365389
88.500054	3074.229029	22.370407
88.947402	3070.203084	22.375424
88.879582	3072.922505	22.380442
89.056607	3063.182118	22.385459
89.094161	3068.916264	22.390477
89.158207	3081.877807	22.395495
89.429139	3087.426062	22.400512
89.173407	3094.647888	22.405530
89.579735	3094.083781	22.410547
89.430372	3093.085644	22.415565
89.494459	3099.924962	22.420583
89.865450	3110.162226	22.425600
89.587104	3123.258452	22.430618
89.735193	3125.306641	22.435635
90.160869	3127.326981	22.440653
90.000631	3124.623391	22.445671
90.169918	3137.614804	22.450688
90.061718	3146.332849	22.455706
90.628126	3151.545957	22.460723
90.518549	3159.320049	22.465741
90.994841	3151.318425	22.470759
90.892557	3142.142002	22.475776
90.736512	3146.161602	22.480794
91.012872	3140.776804	22.485811
91.582577	3161.254651	22.490829
91.285649	3169.008975	22.495847
91.543112	3167.218601	22.500864
91.516474	3172.290511	22.505882
91.516884	3168.756297	22.510899
91.968922	3160.983510	22.515917
91.674546	3166.944319	22.520935
92.037759	3160.106802	22.525952
92.167560	3161.479216	22.530970
92.172356	3155.604677	22.535987
92.372818	3160.916569	22.541005
92.101692	3160.516204	22.546023
92.011195	3151.500832	22.551040
92.260095	3153.436654	22.556058
92.002584	3159.041322	22.561075
92.400929	3155.911352	22.566093
92.397084	3175.250198	22.571111
93.053253	3184.982375	22.576128
92.877302	3189.175772	22.581146
92.690937	3199.260467	22.586163
92.613168	3196.638495	22.591181
92.831044	3198.053816	22.596199
93.085163	3191.604465	22.601216
93.123042	3195.891213	22.606234
92.969009	3218.389549	22.611251
93.256313	3219.235445	22.616269
93.155335	3223.549128	22.621287
93.181575	3220.430748	22.626304
93.686199	3239.527204	22.631322
93.774771	3242.445194	22.636339
93.922076	3242.176357	22.641357
93.524635	3253.416624	22.646375
93.760112	3235.022634	22.651392
93.955233	3245.400534	22.656410
94.223684	3262.852087	22.661427
94.607373	3258.970506	22.666445
94.498103	3268.030170	22.671463
94.801937	3270.628637	22.676480
94.522214	3270.169055	22.681498
94.588233	3265.791191	22.686515
94.744730	3264.356929	22.691533
94.907550	3269.928661	22.696551
95.036035	3267.714307	22.701568
94.984572	3263.987458	22.706586
95.265393	3266.049913	22.711603
95.485183	3270.311682	22.716621
95.176464	3288.744351	22.721639
95.728471	3288.370709	22.726656
95.801097	3301.894067	22.731674
95.773909	3303.810257	22.736691
95.912642	3293.407492	22.741709
95.535059	3302.621847	22.746727
95.672530	3289.185894	22.751744
95.908789	3276.151358	22.756762
95.798545	3291.311061	22.761779
95.743036	3288.292432	22.766797
96.136426	3308.632324	22.771815
96.338726	3303.511336	22.776832
96.416353	3310.413866	22.781850
96.440242	3310.699377	22.786867
96.659864	3308.519934	22.791885
96.527260	3309.710585	22.796903
96.645370	3321.624680	22.801920
96.739256	3330.368430	22.806938
96.626651	3338.419127	22.811955
97.305788	3331.556399	22.816973
96.924928	3334.247764	22.821991
97.349700	3340.538047	22.827008
97.186293	3358.096251	22.832026
97.465522	3359.543953	22.837043
97.578075	3356.752632	22.842061
97.394632	3355.225415	22.847079
97.953602	3351.170287	22.852096
97.990691	3362.078423	22.857114
97.930170	3387.865040	22.862131
98.384283	3374.263978	22.867149
98.427540	3382.366066	22.872167
98.449772	3376.071975	22.877184
98.715862	3369.201624	22.882202
98.394894	3382.259449	22.887219
98.524545	3376.848068	22.892237
98.514764	3380.621439	22.897255
98.561542	3378.922229	22.902272
98.773476	3389.192705	22.907290
98.716259	3394.183520	22.912307
98.861509	3394.643056	22.917325
99.047566	3404.886721	22.922343
98.657809	3406.219179	22.927360
98.786139	3422.427429	22.932378
99.077183	3430.541279	22.937395
99.582401	3436.644246	22.942413
99.574657	3451.524110	22.947431
99.397924	3459.603992	22.952448
99.879293	3456.707885	22.957466
100.100182	3459.314210	22.962483
100.341797	3458.429684	22.967501
100.206668	3452.436058	22.972519
100.417410	3455.904007	22.977536
100.694072	3465.237723	22.982554
100.928208	3483.341344	22.987571
100.943207	3475.247407	22.992589
100.792121	3471.579133	22.997607
100.953587	3484.794992	23.002624
101.075379	3489.060840	23.007642
101.213360	3486.023131	23.012659
101.847660	3487.153760	23.017677
101.526009	3488.799003	23.022695
101.468300	3483.686748	23.027712
101.598337	3485.031195	23.032730
101.710654	3481.642969	23.037747
101.745869	3473.541749	23.042765
101.582864	3477.406268	23.047783
101.608232	3475.929910	23.052800
101.787022	3476.614238	23.057818
101.590731	3482.424658	23.062835
101.955766	3482.428861	23.067853
102.003224	3492.141921	23.072871
101.992733	3504.168404	23.077888
102.307074	3506.338348	23.082906
102.253238	3514.019125	23.087923
102.481814	3510.725832	23.092941
101.829345	3521.563183	23.097959
101.907404	3539.458430	23.102976
102.621395	3536.281638	23.107994
102.546377	3553.248190	23.113011
102.825999	3557.943888	23.118029
103.145972	3571.520240	23.123047
103.170614	3565.083529	23.128064
103.712959	3562.005239	23.133082
102.911637	3561.199275	23.138099
103.419140	3577.256314	23.143117
103.639032	3591.906867	23.148135
103.895804	3595.178619	23.153152
103.868663	3592.557255	23.158170
104.008966	3594.617819	23.163187
104.148389	3597.055350	23.168205
104.306347	3598.843666	23.173223
104.507502	3618.119982	23.178240
104.800673	3628.608298	23.183258
104.488572	3621.836322	23.188275
104.865163	3617.738873	23.193293
104.829721	3614.773558	23.198311
104.811291	3622.878897	23.203328
104.927483	3614.738602	23.208346
104.672694	3616.827571	23.213363
105.165522	3627.216286	23.218381
105.145519	3643.764719	23.223399
105.123170	3645.842770	23.228416
105.521785	3647.934600	23.233434
105.205327	3650.472423	23.238451
105.611233	3661.613444	23.243469
105.408000	3674.266534	23.248487
105.659422	3679.589067	23.253504
105.747340	3674.095506	23.258522
105.949944	3685.279260	23.263539
106.030990	3701.203856	23.268557
106.090025	3702.310438	23.273575
106.390453	3712.494025	23.278592
106.679136	3699.003942	23.283610
106.569601	3698.884329	23.288627
106.799154	3707.356976	23.293645
106.938669	3717.474676	23.298663
106.928374	3724.099387	23.303680
106.891312	3719.441966	23.308698
107.083695	3726.813148	23.313715
107.366367	3714.936470	23.318733
107.339279	3721.324951	23.323751
107.230593	3741.609539	23.328768
107.909920	3738.672338	23.333786
107.581295	3748.313946	23.338803
107.893251	3741.513410	23.343821
108.332881	3744.313915	23.348839
108.374462	3740.923563	23.353856
108.265965	3733.327564	23.358874
108.305260	3738.505686	23.363891
108.597174	3737.031243	23.368909
108.471680	3732.379797	23.373927
108.299717	3743.268078	23.378944
108.994757	3756.723824	23.383962
108.748852	3763.047750	23.388979
108.935231	3767.078934	23.393997
109.098826	3758.737777	23.399015
109.079515	3767.857649	23.404032
109.054502	3762.168945	23.409050
109.067511	3763.948991	23.414067
109.338966	3766.519828	23.419085
109.271722	3783.346740	23.424103
109.102197	3797.397693	23.429120
109.718590	3796.517645	23.434138
109.494496	3798.663768	23.439155
109.986691	3806.043232	23.444173
110.333118	3817.682076	23.449191
109.947338	3823.635821	23.454208
110.136094	3816.729648	23.459226
110.300275	3827.280798	23.464243
110.569384	3825.434085	23.469261
110.244341	3826.290835	23.474279
110.305112	3834.020914	23.479296
110.595863	3834.633959	23.484314
110.934490	3851.710721	23.489331
110.457055	3855.693147	23.494349
110.883825	3861.400157	23.499367
111.027801	3875.928093	23.504384
111.430916	3875.369220	23.509402
111.377785	3877.193305	23.514419
111.670696	3873.898342	23.519437
111.901317	3887.463774	23.524455
111.780199	3897.870447	23.529472
112.234691	3894.596372	23.534490
112.181761	3901.059688	23.539507
112.148452	3903.793227	23.544525
112.545773	3891.919484	23.549543
112.526481	3899.095445	23.554560
112.646347	3906.293258	23.559578
112.714426	3903.110720	23.564595
112.644900	3902.978181	23.569613
112.898351	3920.076601	23.574631
112.742546	3921.468017	23.579648
113.155049	3924.078136	23.584666
112.873873	3930.877722	23.589683
113.112879	3931.581635	23.594701
113.400681	3934.914868	23.599719
113.147031	3958.228120	23.604736
113.505895	3958.368801	23.609754
113.574174	3969.877405	23.614771
113.689115	3958.857572	23.619789
113.659039	3972.802511	23.624807
113.545635	3991.617115	23.629824
114.508362	3983.615652	23.634842
114.222189	3994.154456	23.639859
114.130778	3994.160992	23.644877
114.374544	4014.452944	23.649895
114.677700	4012.869512	23.654912
114.924693	4014.715588	23.659930
114.766443	4016.140494	23.664947
115.016618	4020.980206	23.669965
115.488348	4023.185200	23.674983
115.327214	4039.348298	23.680000
115.737208	4033.486672	23.685018
116.042263	4030.145958	23.690035
115.917101	4029.609179	23.695053
116.525542	4017.366479	23.700071
116.216587	4015.205544	23.705088
116.397508	3996.732673	23.710106
116.350539	3994.959928	23.715123
115.838456	3998.457893	23.720141
116.457528	3999.617861	23.725159
116.474867	4015.414328	23.730176
116.645413	4017.288024	23.735194
116.658982	4014.871298	23.740211
116.536014	4017.070010	23.745229
116.832546	4012.289545	23.750247
116.774309	4013.551412	23.755264
116.954107	4020.548775	23.760282
116.721862	4025.937723	23.765299
116.925697	4041.657663	23.770317
117.179036	4043.782263	23.775335
117.149630	4060.858366	23.780352
117.212326	4067.589266	23.785370
117.661334	4076.954273	23.790387
117.575630	4077.722977	23.795405
117.877529	4086.985555	23.800423
117.444720	4091.750933	23.805440
117.801508	4109.089185	23.810458
118.107728	4101.756288	23.815475
118.042506	4123.491886	23.820493
118.372549	4125.205310	23.825511
118.346893	4138.673210	23.830528
118.731981	4128.129089	23.835546
118.885983	4134.816550	23.840563
119.096822	4147.583779	23.845581
119.558393	4152.436573	23.850599
119.376649	4154.200868	23.855616
119.308652	4152.544991	23.860634
119.394770	4159.201175	23.865651
119.324587	4153.518232	23.870669
119.752566	4167.637155	23.875687
120.045169	4182.696765	23.880704
120.217119	4185.479060	23.885722
119.961564	4178.165895	23.890739
120.106105	4184.673812	23.895757
120.330541	4179.872944	23.900775
120.216030	4193.658802	23.905792
120.557634	4201.630410	23.910810
120.829371	4209.385992	23.915827
120.467828	4215.906832	23.920845
120.903376	4210.585883	23.925863
121.159451	4218.624424	23.930880
121.255166	4235.465793	23.935898
121.691529	4237.846781	23.940915
121.332570	4240.131059	23.945933
121.618530	4233.675618	23.950951
121.641362	4238.438844	23.955968
121.586514	4236.159417	23.960986
121.620283	4248.278765	23.966003
122.126435	4268.863096	23.971021
122.246210	4261.853169	23.976039
122.199668	4271.074314	23.981056
122.019307	4270.100920	23.986074
122.533075	4282.336922	23.991091
122.337264	4294.562043	23.996109
122.760905	4287.669542	24.001127
122.770038	4296.919287	24.006144
123.017890	4302.266645	24.011162
123.150054	4308.070242	24.016179
123.298261	4330.242525	24.021197
123.494716	4318.871878	24.026215
123.544361	4310.607179	24.031232
123.658114	4315.434130	24.036250
124.019994	4315.187636	24.041267
123.977698	4325.632731	24.046285
124.462230	4340.062976	24.051303
124.084552	4342.306265	24.056320
124.289924	4343.426861	24.061338
124.224729	4342.785637	24.066355
124.416072	4338.684022	24.071373
124.443382	4336.664254	24.076391
124.534912	4349.002503	24.081408
124.888127	4360.610703	24.086426
124.998759	4366.339132	24.091443
124.956039	4365.462650	24.096461
124.949528	4361.726915	24.101479
125.166864	4368.171666	24.106496
125.174752	4387.124958	24.111514
125.199326	4398.980543	24.116531
125.155234	4402.255420	24.121549
125.586506	4402.794429	24.126567
125.578868	4418.950617	24.131584
125.967585	4428.136020	24.136602
126.274635	4427.385125	24.141619
126.007789	4432.060911	24.146637
126.642793	4434.820929	24.151655
126.364054	4451.930860	24.156672
126.900390	4442.596360	24.161690
127.058316	4450.846582	24.166707
126.937091	4455.338395	24.171725
127.310806	4445.146404	24.176743
127.478607	4458.852678	24.181760
127.372495	4473.785630	24.186778
127.675406	4470.375876	24.191795
127.685824	4472.892787	24.196813
127.632997	4477.598521	24.201831
127.783509	4476.983796	24.206848
127.755458	4467.756896	24.211866
128.283603	4485.675968	24.216883
128.241777	4503.383070	24.221901
128.833331	4500.682355	24.226919
128.342049	4506.425432	24.231936
128.271538	4499.798149	24.236954
128.659706	4501.212175	24.241971
128.871520	4524.166474	24.246989
129.184452	4532.058731	24.252007
129.048594	4525.060295	24.257024
129.244398	4529.999735	24.262042
129.491233	4520.153172	24.267059
129.121567	4531.296817	24.272077
129.786328	4547.213446	24.277095
129.678409	4540.154461	24.282112
129.606496	4540.118392	24.287130
130.119731	4550.646500	24.292147
130.096418	4571.250370	24.297165
130.433262	4579.285964	24.302183
130.528673	4581.124128	24.307200
130.789621	4575.420075	24.312218
130.678477	4569.260207	24.317235
130.563402	4588.198659	24.322253
130.721571	4594.649361	24.327271
130.693270	4604.626094	24.332288
130.893536	4605.838124	24.337306
131.470642	4628.394238	24.342323
131.274835	4633.100063	24.347341
131.609730	4627.662543	24.352359
131.751044	4640.829949	24.357376
131.593519	4640.494607	24.362394
131.940874	4652.709623	24.367411
131.808024	4664.599347	24.372429
132.346107	4661.896432	24.377447
132.245261	4660.551511	24.382464
132.461881	4687.079177	24.387482
132.717501	4687.218848	24.392499
132.985063	4708.668618	24.397517
132.831502	4694.827589	24.402535
132.897609	4693.050220	24.407552
132.991428	4707.830585	24.412570
133.388640	4709.276999	24.417587
133.479950	4723.871144	24.422605
133.594576	4719.728578	24.427623
133.723317	4709.514758	24.432640
133.148941	4715.269304	24.437658
133.560999	4731.391769	24.442675
133.733739	4749.589713	24.447693
133.943655	4742.409500	24.452711
134.203005	4760.512000	24.457728
134.350415	4774.974045	24.462746
134.805618	4775.662682	24.467763
134.549078	4771.082238	24.472781
134.925468	4774.411225	24.477799
134.966265	4779.715846	24.482816
135.361106	4797.364373	24.487834
135.561353	4803.241938	24.492851
135.732280	4807.120014	24.497869
135.872233	4798.585725	24.502887
135.822723	4804.960638	24.507904
135.841312	4801.639627	24.512922
136.228650	4792.213031	24.517939
136.502389	4792.826965	24.522957
136.293389	4800.445064	24.527975
136.521229	4805.513962	24.532992
136.560356	4822.602384	24.538010
136.959620	4821.750361	24.543027
136.623738	4824.754670	24.548045
136.703954	4820.265733	24.553063
136.767187	4832.257006	24.558080
137.281528	4846.248837	24.563098
137.188898	4846.009066	24.568115
137.102046	4857.595196	24.573133
137.319862	4868.281899	24.578151
137.628883	4881.326446	24.583168
137.701268	4875.463701	24.588186
137.644190	4883.095278	24.593203
138.125298	4905.806297	24.598221
138.072003	4900.686549	24.603239
138.425487	4915.602111	24.608256
138.410971	4916.334654	24.613274
138.935665	4925.975106	24.618291
138.691436	4937.829920	24.623309
138.998307	4933.875203	24.628327
139.397851	4926.225624	24.633344
139.152623	4935.923453	24.638362
139.416865	4951.572086	24.643379
139.711553	4960.815112	24.648397
139.834729	4962.868457	24.653415
140.068630	4961.473603	24.658432
140.008342	4959.610020	24.663450
140.111989	4964.452233	24.668467
140.320250	4977.019734	24.673485
140.350802	4977.429791	24.678503
140.910831	4976.933117	24.683520
140.483024	4984.559176	24.688538
140.687633	4987.026693	24.693555
140.803541	5005.677745	24.698573
140.783770	5007.353100	24.703591
141.268599	5002.265515	24.708608
141.237353	5016.702230	24.713626
141.637211	5025.974350	24.718643
141.641570	5040.066535	24.723661
141.620891	5035.620231	24.728679
141.869907	5035.418406	24.733696
141.905031	5051.075930	24.738714
142.161735	5057.094671	24.743731
141.943474	5063.576383	24.748749
142.066995	5074.203231	24.753767
142.209499	5084.784413	24.758784
142.318709	5094.759168	24.763802
142.784311	5088.976946	24.768819
142.480793	5112.483665	24.773837
142.574247	5131.495356	24.778855
143.138264	5129.594553	24.783872
143.364097	5150.323324	24.788890
143.535834	5155.539449	24.793907
143.742792	5158.283045	24.798925
143.788799	5155.537866	24.803943
143.835258	5155.297904	24.808960
144.119267	5175.627225	24.813978
144.331890	5184.466551	24.818995
144.248058	5187.162997	24.824013
144.429914	5191.407159	24.829031
144.412960	5198.546309	24.834048
144.639219	5210.655795	24.839066
144.737751	5216.232960	24.844083
144.811648	5227.227263	24.849101
145.182013	5241.952896	24.854119
145.361645	5242.231167	24.859136
145.028243	5260.435526	24.864154
145.474055	5270.769723	24.869171
145.873761	5280.128653	24.874189
145.642762	5288.994226	24.879207
146.105769	5300.718049	24.884224
146.443149	5309.747078	24.889242
146.505513	5311.894020	24.894259
146.741498	5313.099405	24.899277
146.800584	5321.649193	24.904295
146.840341	5325.183672	24.909312
147.171558	5338.129626	24.914330
147.164028	5338.647596	24.919347
147.511279	5336.073826	24.924365
147.411147	5358.040581	24.929383
147.343296	5364.760571	24.934400
147.597594	5370.448255	24.939418
147.854823	5376.481996	24.944435
147.990840	5390.677137	24.949453
148.080106	5392.268323	24.954471
148.590309	5389.289524	24.959488
148.825113	5415.104211	24.964506
148.516130	5421.987010	24.969523
148.724249	5426.011875	24.974541
148.833736	5431.266751	24.979559
149.424498	5435.940256	24.984576
149.300007	5457.003086	24.989594
148.947813	5453.254225	24.994611
149.350889	5460.711452	24.999629
149.480717	5472.159773	25.004647
149.929931	5477.837280	25.009664
149.572245	5484.960509	25.014682
149.664253	5498.352597	25.019699
150.493207	5511.951907	25.024717
150.449835	5514.764575	25.029735
150.656311	5520.165670	25.034752
150.908394	5536.875430	25.039770
150.805185	5541.485858	25.044787
150.966755	5544.089755	25.049805
150.949891	5545.667811	25.054823
151.108697	5562.830158	25.059840
150.876292	5578.122943	25.064858
151.446292	5578.686289	25.069875
151.758302	5590.433752	25.074893
151.733360	5608.558302	25.079911
151.872928	5597.754565	25.084928
152.308200	5612.919520	25.089946
152.746791	5610.612547	25.094963
152.630953	5610.582958	25.099981
152.367462	5627.660919	25.104999
152.948987	5624.650579	25.110016
153.242935	5643.348520	25.115034
153.166903	5656.396024	25.120051
153.653518	5650.572317	25.125069
153.376918	5654.963388	25.130087
154.124884	5648.027635	25.135104
154.209741	5643.061196	25.140122
154.158238	5644.472511	25.145139
154.254562	5654.519850	25.150157
154.208103	5668.231145	25.155175
154.544328	5678.237207	25.160192
154.497421	5682.097218	25.165210
154.415177	5679.349553	25.170227
154.796238	5682.529106	25.175245
154.646961	5705.721331	25.180263
155.164207	5706.142196	25.185280
155.305620	5709.618977	25.190298
155.221061	5721.385722	25.195315
155.533204	5729.433873	25.200333
155.436956	5746.785140	25.205351
155.566173	5757.732850	25.210368
155.717399	5767.561668	25.215386
155.609944	5776.047909	25.220403
156.103746	5793.168438	25.225421
156.754479	5803.860505	25.230439
156.520700	5799.365778	25.235456
156.952507	5809.586871	25.240474
156.906536	5825.909157	25.245491
157.229257	5826.229123	25.250509
157.482290	5831.304422	25.255527
157.950301	5839.327613	25.260544
158.038040	5855.206419	25.265562
158.341621	5860.118986	25.270579
158.701929	5849.604606	25.275597
158.438562	5853.557202	25.280615
158.512374	5849.374629	25.285632
158.682318	5854.460540	25.290650
158.490674	5848.024443	25.295667
159.019966	5859.250178	25.300685
159.115729	5878.130854	25.305703
159.340319	5872.696208	25.310720
159.462828	5866.367981	25.315738
159.548786	5873.937764	25.320755
159.351646	5878.062916	25.325773
159.604684	5893.824608	25.330791
159.731323	5895.918458	25.335808
159.688681	5899.695904	25.340826
159.810576	5925.092991	25.345843
160.091816	5932.588729	25.350861
160.105897	5952.216289	25.355879
160.507539	5951.196843	25.360896
160.624183	5958.225217	25.365914
160.819453	5983.017172	25.370931
161.061826	5991.807920	25.375949
161.023879	6006.181275	25.380967
161.763303	6004.261575	25.385984
161.894627	6013.620480	25.391002
161.936500	6028.155493	25.396019
162.190480	6012.180690	25.401037
162.051152	6018.055857	25.406055
162.516371	6027.776146	25.411072
162.449962	6036.769262	25.416090
162.622243	6047.094909	25.421107
162.974535	6038.687051	25.426125
163.164633	6057.758683	25.431143
162.861210	6062.719820	25.436160
163.162463	6064.153110	25.441178
163.328403	6067.653477	25.446195
163.674179	6061.143287	25.451213
163.553736	6084.993686	25.456231
163.777669	6108.644549	25.461248
163.525500	6106.788179	25.466266
163.676771	6115.442854	25.471283
164.245861	6132.929350	25.476301
164.091979	6142.344999	25.481319
164.175139	6154.476538	25.486336
164.248324	6166.404954	25.491354
164.509337	6180.148491	25.496371
164.815721	6191.842201	25.501389
164.909311	6202.531473	25.506407
165.124770	6214.613589	25.511424
165.514964	6229.521957	25.516442
165.890166	6228.694328	25.521459
165.893790	6236.722928	25.526477
166.197464	6244.708947	25.531495
166.372507	6247.026395	25.536512
167.017643	6252.220437	25.541530
166.800261	6269.130776	25.546547
166.928590	6275.374448	25.551565
167.258997	6280.673373	25.556583
167.461461	6284.526115	25.561600
167.839440	6273.593447	25.566618
167.519774	6280.494136	25.571635
167.930320	6292.498333	25.576653
167.753817	6312.408358	25.581671
167.963828	6309.774453	25.586688
168.207413	6312.117584	25.591706
168.026262	6332.687657	25.596723
167.984636	6327.742732	25.601741
168.550190	6349.492751	25.606759
168.712470	6357.429773	25.611776
169.089715	6365.643904	25.616794
168.915658	6378.495567	25.621811
169.264141	6386.889327	25.626829
169.233869	6393.142761	25.631847
169.694803	6415.767145	25.636864
169.948450	6414.357085	25.641882
169.729624	6429.300303	25.646899
169.891731	6438.938703	25.651917
170.260451	6449.702316	25.656935
170.423885	6455.734672	25.661952
170.996353	6468.776305	25.666970
170.898012	6484.022563	25.671988
170.965628	6480.139368	25.677005
171.164138	6493.342960	25.682023
171.736225	6500.423776	25.687040
171.747319	6510.218757	25.692058
171.660650	6516.714719	25.697076
171.857028	6514.798222	25.702093
171.864943	6535.473521	25.707111
171.912629	6541.365966	25.712128
172.368702	6548.231291	25.717146
172.426524	6562.381356	25.722164
172.898779	6566.590418	25.727181
173.201707	6568.546479	25.732199
173.214246	6591.628932	25.737216
173.477419	6599.408382	25.742234
173.489876	6599.799423	25.747252
173.614586	6597.333185	25.752269
173.925961	6612.180924	25.757287
173.862212	6627.509022	25.762304
174.471428	6623.985094	25.767322
174.089580	6634.608437	25.772340
174.556745	6641.271903	25.777357
174.666739	6653.284385	25.782375
174.973214	6657.369686	25.787392
175.063854	6651.316588	25.792410
174.927749	6672.238026	25.797428
175.286379	6678.520134	25.802445
175.616924	6688.422234	25.807463
175.779046	6696.290138	25.812480
176.132743	6691.859370	25.817498
175.859553	6713.527412	25.822516
176.225445	6711.042495	25.827533
176.436573	6710.880796	25.832551
176.405372	6728.273566	25.837568
176.474706	6740.142402	25.842586
176.845016	6746.126444	25.847604
177.109630	6749.017520	25.852621
177.061304	6764.592885	25.857639
177.290522	6771.011452	25.862656
177.779890	6771.813471	25.867674
177.596383	6796.895464	25.872692
177.920425	6801.658435	25.877709
178.459696	6800.573621	25.882727
178.182226	6822.655255	25.887744
178.709842	6818.806099	25.892762
178.970689	6825.814137	25.897780
178.813186	6824.739124	25.902797
179.061750	6850.358537	25.907815
178.784848	6854.505021	25.912832
179.348562	6855.483776	25.917850
179.453345	6880.823003	25.922868
179.507930	6890.785092	25.927885
179.673096	6895.642920	25.932903
179.792684	6921.847769	25.937920
180.052212	6925.591976	25.942938
180.189985	6950.733661	25.947956
180.624223	6948.430374	25.952973
180.777279	6968.288238	25.957991
180.704598	6983.423604	25.963008
181.208155	6983.804245	25.968026
181.069010	7002.782649	25.973044
181.591822	7013.247028	25.978061
181.902119	7009.486578	25.983079
182.111842	7035.878337	25.988096
182.144399	7048.741235	25.993114
181.980860	7053.455033	25.998132
182.623775	7058.755262	26.003149
182.715938	7075.135519	26.008167
182.583885	7085.439759	26.013184
182.916736	7074.636892	26.018202
183.370959	7105.096804	26.023220
183.291051	7107.563711	26.028237
183.442019	7118.939621	26.033255
183.537608	7129.968676	26.038272
184.214098	7131.641629	26.043290
184.171760	7150.906652	26.048308
184.372955	7157.672656	26.053325
184.882168	7164.341986	26.058343
184.782362	7165.997735	26.063360
185.333304	7171.677136	26.068378
185.341768	7190.725850	26.073396
185.571379	7188.428836	26.078413
185.461025	7183.087791	26.083431
185.889220	7188.525221	26.088448
186.236790	7200.272723	26.093466
186.055020	7216.485800	26.098484
186.397566	7222.920448	26.103501
186.766215	7218.528020	26.108519
186.557145	7218.498106	26.113536
187.177586	7237.929203	26.118554
186.861574	7247.696082	26.123572
186.695607	7250.816069	26.128589
187.085752	7248.962718	26.133607
187.274271	7276.056274	26.138624
187.832547	7272.072756	26.143642
187.592771	7289.840948	26.148660
187.840692	7289.647160	26.153677
188.101374	7304.109310	26.158695
188.011806	7305.252170	26.163712
188.357255	7326.761132	26.168730
188.560717	7341.270597	26.173748
188.764718	7346.345050	26.178765
189.161088	7360.280669	26.183783
188.869386	7382.836471	26.188800
188.921077	7371.497845	26.193818
189.584552	7403.454959	26.198836
189.770788	7399.863830	26.203853
190.103321	7409.830644	26.208871
190.341533	7428.820342	26.213888
190.803660	7429.623757	26.218906
190.630211	7442.798344	26.223924
191.206748	7455.367505	26.228941
191.147023	7458.525083	26.233959
191.226893	7465.291610	26.238976
191.537390	7467.478902	26.243994
191.348307	7484.233820	26.249012
191.249854	7494.845477	26.254029
191.694655	7507.541252	26.259047
191.899600	7516.617102	26.264064
192.290022	7530.960307	26.269082
192.523665	7542.834050	26.274100
192.437887	7539.507687	26.279117
193.066289	7561.911426	26.284135
193.093038	7581.342765	26.289152
193.377136	7586.352048	26.294170
193.648286	7604.595276	26.299188
193.853590	7607.705859	26.304205
193.997585	7617.214852	26.309223
193.915524	7630.756501	26.314240
194.347898	7640.747105	26.319258
194.212695	7640.332377	26.324276
194.599392	7664.636041	26.329293
195.150523	7668.482604	26.334311
195.219295	7678.981628	26.339328
195.593799	7703.569368	26.344346
195.824774	7699.067267	26.349364
195.638622	7710.415911	26.354381
195.613723	7719.054152	26.359399
195.930779	7728.391988	26.364416
196.196065	7736.377241	26.369434
196.514574	7758.355994	26.374452
196.701649	7772.335287	26.379469
196.881293	7761.028767	26.384487
196.910577	7786.994772	26.389504
197.325368	7790.764685	26.394522
197.527561	7800.669825	26.399540
197.559907	7818.165907	26.404557
198.454832	7824.896126	26.409575
198.533931	7821.027246	26.414592
198.337035	7818.966955	26.419610
198.282025	7830.297914	26.424628
198.669974	7838.835579	26.429645
198.841250	7850.583603	26.434663
198.802520	7865.175388	26.439680
198.959682	7878.520890	26.444698
198.858869	7892.064289	26.449716
199.120021	7908.075560	26.454733
199.271575	7921.778074	26.459751
199.547172	7929.150449	26.464768
199.854505	7942.219075	26.469786
200.151774	7971.974054	26.474804
200.057954	7976.197648	26.479821
200.539000	7988.592413	26.484839
200.678329	8007.573964	26.489856
201.413921	8010.292781	26.494874
201.459317	8029.243432	26.499892
201.660774	8041.389126	26.504909
201.950972	8026.963640	26.509927
201.906331	8047.000519	26.514944
201.991342	8057.156807	26.519962
202.538886	8056.262753	26.524980
202.449228	8073.170402	26.529997
203.052342	8081.601685	26.535015
202.867409	8093.007115	26.540032
203.067047	8104.240972	26.545050
203.337420	8123.527086	26.550068
203.346487	8125.546958	26.555085
204.017309	8131.301391	26.560103
204.038225	8145.210839	26.565120
204.164188	8154.764888	26.570138
204.461413	8171.991433	26.575156
204.490182	8186.132784	26.580173
204.729465	8180.710680	26.585191
205.048116	8203.298940	26.590208
205.133403	8217.827979	26.595226
205.218899	8224.539545	26.600244
205.217959	8253.053322	26.605261
205.829118	8261.759864	26.610279
205.758864	8268.096274	26.615296
205.957188	8288.986526	26.620314
206.452869	8294.395838	26.625332
206.334641	8316.124687	26.630349
206.686842	8330.496210	26.635367
206.700060	8333.408715	26.640384
207.158051	8351.240605	26.645402
207.583814	8369.385856	26.650420
207.359883	8385.288850	26.655437
207.852939	8387.340494	26.660455
208.317691	8400.359018	26.665472
208.563986	8415.603636	26.670490
208.891730	8430.650455	26.675508
209.032009	8427.615760	26.680525
209.344280	8419.025800	26.685543
209.158564	8449.961312	26.690560
209.435399	8455.163494	26.695578
209.768741	8467.156915	26.700596
209.945268	8491.396589	26.705613
210.097118	8503.550847	26.710631
209.987383	8510.332663	26.715648
210.619071	8520.839888	26.720666
210.947522	8529.873028	26.725684
210.703941	8534.207424	26.730701
211.032496	8542.126679	26.735719
211.203771	8561.397429	26.740736
211.638768	8574.347761	26.745754
211.894291	8583.916069	26.750772
212.122035	8584.822945	26.755789
212.161333	8593.547136	26.760807
212.192831	8622.387844	26.765824
212.671190	8616.565228	26.770842
213.092817	8630.146444	26.775860
212.867976	8650.928399	26.780877
213.256909	8640.790300	26.785895
213.689610	8663.450923	26.790912
213.774788	8679.748908	26.795930
213.904071	8672.473144	26.800948
214.014019	8683.801032	26.805965
214.636525	8695.155154	26.810983
214.911778	8712.024340	26.816000
214.999313	8709.590717	26.821018
214.925907	8709.684860	26.826036
214.908570	8720.428848	26.831053
215.264691	8726.813810	26.836071
215.403543	8736.483450	26.841088
215.273076	8748.976887	26.846106
215.674965	8751.775499	26.851124
215.609035	8770.707645	26.856141
216.037916	8791.664372	26.861159
216.413745	8803.306763	26.866176
216.506908	8821.394149	26.871194
216.729580	8836.219264	26.876212
216.379869	8854.825086	26.881229
217.009337	8871.924126	26.886247
217.494008	8891.033108	26.891264
217.483232	8904.124460	26.896282
217.855202	8913.000150	26.901300
217.971907	8929.416062	26.906317
218.482322	8942.402262	26.911335
218.836934	8956.193367	26.916352
218.896732	8979.348652	26.921370
219.040912	8986.217830	26.926388
219.222704	9002.495423	26.931405
219.635999	9010.850701	26.936423
219.878193	9016.534616	26.941440
219.820575	9037.713999	26.946458
220.211063	9049.663737	26.951476
220.455197	9072.519224	26.956493
220.638840	9070.354023	26.961511
221.136377	9092.329400	26.966528
221.262858	9105.747968	26.971546
221.444925	9108.365607	26.976564
221.204803	9127.386091	26.981581
221.504563	9127.731999	26.986599
221.947812	9150.565665	26.991616
222.455825	9175.030374	26.996634
222.584383	9173.172847	27.001652
222.762172	9196.002467	27.006669
223.172375	9201.872913	27.011687
223.421813	9211.591495	27.016704
223.280360	9237.209982	27.021722
223.661606	9238.115908	27.026740
223.711635	9249.101977	27.031757
224.170965	9252.048727	27.036775
224.510813	9262.690624	27.041792
224.223852	9288.987140	27.046810
225.018820	9289.049404	27.051828
225.250806	9304.305905	27.056845
225.878878	9309.047668	27.061863
225.682716	9324.659452	27.066880
225.742942	9324.185542	27.071898
226.100517	9343.407488	27.076916
226.172000	9350.459019	27.081933
226.395033	9349.274358	27.086951
227.204350	9362.248449	27.091968
226.705124	9365.223910	27.096986
227.179263	9375.113373	27.102004
227.212050	9398.657387	27.107021
227.657316	9406.966617	27.112039
227.754251	9420.946519	27.117056
227.362150	9441.494849	27.122074
228.207271	9447.473796	27.127092
228.329718	9467.012115	27.132109
228.343612	9477.842037	27.137127
228.798061	9489.479792	27.142144
228.855072	9499.465954	27.147162
229.119735	9516.138429	27.152180
229.114157	9530.292955	27.157197
229.433384	9543.942319	27.162215
229.890448	9559.285489	27.167232
229.998944	9574.424824	27.172250
230.110703	9573.607562	27.177268
230.414319	9597.025892	27.182285
230.827890	9603.409575	27.187303
230.767468	9615.744772	27.192320
230.785099	9632.085630	27.197338
231.381949	9647.133165	27.202356
231.434022	9666.038954	27.207373
231.749406	9683.602090	27.212391
232.317280	9695.949939	27.217408
232.089101	9720.316761	27.222426
232.771845	9719.677555	27.227444
232.749025	9731.703311	27.232461
233.055977	9744.968066	27.237479
233.541333	9756.886087	27.242496
233.244743	9767.899951	27.247514
233.990088	9774.257144	27.252532
233.992369	9799.172066	27.257549
234.622056	9800.718357	27.262567
234.730545	9812.202483	27.267584
234.908414	9835.730212	27.272602
235.123675	9842.508423	27.277620
235.311183	9846.003693	27.282637
235.240855	9871.908421	27.287655
235.662738	9879.924763	27.292672
235.892129	9898.496589	27.297690
236.273798	9903.755160	27.302708
236.715329	9928.614117	27.307725
236.647738	9935.366709	27.312743
237.427488	9942.934663	27.317760
237.386030	9977.132852	27.322778
237.795217	9967.519984	27.327796
238.006574	9975.749270	27.332813
237.990563	9992.143332	27.337831
238.175733	9992.323881	27.342848
238.561099	10014.334849	27.347866
238.948048	10012.399790	27.352884
239.048561	10023.682918	27.357901
238.999427	10043.971984	27.362919
239.324037	10046.940398	27.367936
239.402822	10066.243237	27.372954
239.793695	10086.619449	27.377972
239.969027	10092.768602	27.382989
240.356414	10119.547290	27.388007
240.555994	10120.084703	27.393024
240.611707	10148.007114	27.398042
241.082218	10149.249691	27.403060
241.308091	10171.727672	27.408077
241.289027	10186.043360	27.413095
241.929731	10201.429228	27.418112
241.764063	10215.188579	27.423130
242.191920	10225.032658	27.428148
242.527134	10235.409683	27.433165
242.480564	10246.065778	27.438183
242.869962	10269.806507	27.443200
242.899086	10277.835278	27.448218
243.554583	10307.373006	27.453236
243.678613	10311.922766	27.458253
243.753935	10330.887726	27.463271
244.232406	10324.073388	27.468288
244.087933	10362.544543	27.473306
244.692704	10363.110221	27.478324
244.891601	10385.124990	27.483341
245.051621	10407.458208	27.488359
245.349966	10396.764400	27.493376
245.097475	10427.770703	27.498394
245.457526	10435.485575	27.503412
245.729138	10462.741733	27.508429
246.026668	10478.345392	27.513447
246.448331	10486.576369	27.518464
246.349628	10500.714073	27.523482
246.400608	10521.443328	27.528500
246.912151	10534.770988	27.533517
246.956640	10561.345606	27.538535
247.890206	10569.958295	27.543552
247.892998	10587.076244	27.548570
248.172400	10600.302147	27.553588
248.579152	10617.244537	27.558605
248.659514	10627.780604	27.563623
249.088181	10637.222211	27.568640
248.988917	10663.222026	27.573658
249.612491	10680.982624	27.578676
249.740739	10692.237206	27.583693
249.988181	10705.681207	27.588711
250.600770	10702.417427	27.593728
250.501910	10725.727544	27.598746
251.116908	10729.352361	27.603764
251.280645	10740.158328	27.608781
251.321101	10754.167646	27.613799
251.725368	10763.873360	27.618816
251.596590	10784.142661	27.623834
252.055810	10799.346424	27.628852
252.608909	10806.569411	27.633869
252.429523	10836.947504	27.638887
252.648956	10838.717021	27.643904
253.304600	10850.851907	27.648922
253.639855	10866.629331	27.653940
253.446276	10884.665656	27.658957
253.487134	10902.857010	27.663975
254.140009	10913.284314	27.668992
254.415934	10932.752523	27.674010
254.782956	10937.119635	27.679028
254.671808	10956.057893	27.684045
254.516741	10972.573664	27.689063
255.036033	10991.120824	27.694080
255.427478	11007.177445	27.699098
255.571740	11024.188925	27.704116
256.009662	11035.439759	27.709133
256.309200	11058.088779	27.714151
256.752732	11073.454548	27.719168
256.897673	11093.270811	27.724186
257.369694	11097.404710	27.729204
257.868923	11108.208965	27.734221
258.035629	11121.709223	27.739239
258.697155	11137.257998	27.744256
258.386162	11144.324777	27.749274
258.750455	11146.454834	27.754292
258.983025	11170.957150	27.759309
259.089044	11179.344730	27.764327
259.566147	11183.131145	27.769344
259.645669	11209.157394	27.774362
259.862811	11206.589277	27.779380
260.484049	11218.851470	27.784397
260.408585	11241.830701	27.789415
260.982710	11238.311608	27.794432
261.124407	11252.351873	27.799450
261.089323	11270.822514	27.804468
261.274976	11282.282309	27.809485
261.466845	11301.248026	27.814503
262.368053	11306.806339	27.819520
262.125757	11332.867148	27.824538
262.141734	11335.916831	27.829556
262.652848	11345.179754	27.834573
262.631713	11356.883408	27.839591
262.911954	11367.917907	27.844608
262.672065	11386.499794	27.849626
262.999449	11395.074605	27.854644
263.416114	11427.228737	27.859661
263.709168	11449.824229	27.864679
264.229836	11463.456851	27.869696
264.698819	11482.282364	27.874714
264.571282	11493.953305	27.879732
264.924836	11517.164462	27.884749
265.019123	11537.906762	27.889767
265.438161	11549.230416	27.894784
265.837010	11574.542565	27.899802
266.003955	11586.416954	27.904820
266.813428	11602.324608	27.909837
267.141795	11619.481154	27.914855
267.534162	11617.101428	27.919872
267.638400	11640.968592	27.924890
267.883196	11653.354885	27.929908
268.069723	11651.527664	27.934925
268.176180	11674.748433	27.939943
268.590777	11679.243393	27.944960
268.614197	11703.905624	27.949978
268.742943	11716.984044	27.954996
269.185764	11723.261308	27.960013
269.336445	11747.010634	27.965031
269.441651	11760.152865	27.970048
269.653868	11776.403803	27.975066
270.191484	11798.393584	27.980084
270.667466	11810.313109	27.985101
270.886194	11834.741507	27.990119
271.165241	11845.850594	27.995136
271.294516	11871.701060	28.000154
271.526195	11876.828316	28.005172
271.804579	11892.296266	28.010189
271.637956	11926.139519	28.015207
272.369838	11937.033466	28.020224
272.500478	11958.581837	28.025242
272.844854	11984.231416	28.030260
273.202090	12007.319752	28.035277
273.336551	12030.265351	28.040295
273.679265	12029.376647	28.045312
274.036874	12063.238994	28.050330
274.268727	12074.174828	28.055348
274.506509	12089.857698	28.060365
274.841106	12116.279690	28.065383
275.288630	12125.515769	28.070400
275.455328	12146.880352	28.075418
275.534804	12168.358678	28.080436
276.189107	12186.813955	28.085453
276.149837	12196.776749	28.090471
276.653867	12218.914489	28.095488
276.976083	12226.899653	28.100506
277.182155	12251.836623	28.105524
277.644755	12247.818899	28.110541
277.821970	12268.899823	28.115559
277.871394	12281.148742	28.120576
278.279051	12303.222180	28.125594
278.219516	12315.147198	28.130612
279.024393	12328.371061	28.135629
279.129322	12355.833709	28.140647
279.611622	12369.876872	28.145664
279.893456	12368.482920	28.150682
279.971433	12397.026417	28.155700
280.309782	12412.990793	28.160717
280.661123	12432.582274	28.165735
280.827698	12438.335077	28.170752
281.595181	12446.125306	28.175770
281.371829	12458.132700	28.180788
281.398960	12466.478850	28.185805
281.688036	12483.655422	28.190823
282.240877	12504.352998	28.195840
282.393667	12514.389781	28.200858
282.201223	12537.364992	28.205876
282.875549	12546.440853	28.210893
283.061448	12570.020085	28.215911
283.157072	12589.553226	28.220928
283.627928	12602.110844	28.225946
283.763772	12625.370657	28.230964
284.489462	12635.509674	28.235981
284.705550	12664.126909	28.240999
284.939465	12681.222995	28.246016
285.017424	12702.294120	28.251034
285.379806	12717.307702	28.256052
285.782126	12729.612012	28.261069
286.024201	12758.776678	28.266087
286.425079	12766.082481	28.271104
286.838048	12777.904414	28.276122
286.661154	12797.430906	28.281140
287.485224	12814.848642	28.286157
287.359526	12826.422526	28.291175
287.820427	12853.762481	28.296192
287.980228	12865.159911	28.301210
288.217141	12887.940050	28.306228
288.569315	12896.076603	28.311245
288.727748	12923.919030	28.316263
289.026657	12937.873271	28.321280
289.488242	12961.949557	28.326298
289.645361	12981.085311	28.331316
289.937090	12997.619010	28.336333
290.112570	13022.946753	28.341351
290.799140	13043.859273	28.346368
291.266061	13053.949981	28.351386
291.216677	13078.911592	28.356404
292.159139	13079.376580	28.361421
292.115773	13108.792415	28.366439
292.568015	13125.001823	28.371456
292.922402	13117.824703	28.376474
293.207044	13150.853538	28.381492
293.534161	13159.605837	28.386509
293.684573	13172.144445	28.391527
293.663691	13192.562787	28.396544
294.228588	13194.896311	28.401562
294.482551	13221.717979	28.406580
294.803025	13234.312012	28.411597
294.936226	13247.061552	28.416615
294.768034	13265.844889	28.421632
295.359865	13275.120779	28.426650
295.737175	13304.119050	28.431668
296.164932	13320.236572	28.436685
296.191167	13345.433499	28.441703
296.560702	13364.657469	28.446720
297.095316	13378.238971	28.451738
297.139109	13406.055493	28.456756
297.360790	13408.501016	28.461773
297.668214	13429.380655	28.466791
298.129348	13447.311450	28.471808
298.407041	13466.771378	28.476826
298.284103	13493.632238	28.481844
298.660657	13509.094936	28.486861
298.978011	13537.767863	28.491879
299.586914	13565.432809	28.496896
299.701432	13572.321459	28.501914
299.729596	13607.213931	28.506932
300.285414	13613.433833	28.511949
300.625185	13627.307830	28.516967
300.944021	13649.908420	28.521984
301.380802	13664.032735	28.527002
301.516495	13689.620258	28.532020
301.756658	13711.340364	28.537037
301.967614	13723.658191	28.542055
302.493042	13744.157006	28.547072
302.993194	13759.520684	28.552090
303.201652	13785.367385	28.557108
303.350998	13784.843137	28.562125
303.703034	13801.063501	28.567143
303.796606	13810.789380	28.572160
304.036800	13832.626267	28.577178
304.475469	13859.711550	28.582196
304.801139	13881.390938	28.587213
305.220102	13904.641962	28.592231
305.489675	13932.749821	28.597248
305.735536	13935.944761	28.602266
306.140556	13970.903290	28.607284
306.248298	13981.998065	28.612301
306.578777	14005.657885	28.617319
306.938116	14037.013440	28.622336
307.310437	14038.639808	28.627354
307.155823	14067.974915	28.632372
307.797503	14090.098725	28.637389
308.437669	14108.772872	28.642407
308.642958	14135.758550	28.647424
309.242827	14155.927202	28.652442
309.370865	14171.247265	28.657460
309.687912	14176.781925	28.662477
310.395121	14202.001423	28.667495
310.715965	14222.706490	28.672512
310.996603	14228.155784	28.677530
311.040292	14244.640392	28.682548
311.225308	14260.827391	28.687565
311.556350	14285.726299	28.692583
311.740077	14299.714956	28.697600
312.132882	14308.808463	28.702618
312.387998	14339.675935	28.707636
312.614246	14355.195835	28.712653
313.019437	14370.597873	28.717671
313.072747	14401.251421	28.722688
313.692738	14416.668384	28.727706
313.954887	14442.474138	28.732724
314.060343	14462.630438	28.737741
314.695942	14483.628899	28.742759
314.584728	14506.924402	28.747776
314.943244	14536.840519	28.752794
315.180846	14569.178651	28.757812
315.700679	14583.847950	28.762829
315.908478	14599.858144	28.767847
316.242575	14631.961352	28.772864
316.334020	14644.283893	28.777882
316.754791	14671.868375	28.782900
317.361045	14699.655466	28.787917
317.803102	14721.822630	28.792935
318.166534	14752.126046	28.797952
318.493524	14759.071444	28.802970
318.668654	14791.847477	28.807988
318.899066	14802.189616	28.813005
319.254670	14828.387145	28.818023
319.553216	14841.220888	28.823040
319.961331	14863.080216	28.828058
319.840933	14893.418266	28.833076
320.338943	14919.136873	28.838093
320.837609	14937.792834	28.843111
320.827241	14961.923392	28.848128
321.330770	14975.929044	28.853146
321.872456	15006.707786	28.858164
322.031769	15023.847042	28.863181
322.586736	15038.659091	28.868199
322.549480	15059.288939	28.873216
322.705023	15088.689588	28.878234
323.108089	15108.149632	28.883252
323.612547	15130.341696	28.888269
324.020668	15158.116650	28.893287
323.888593	15180.909043	28.898304
324.309566	15195.440792	28.903322
324.819891	15226.157361	28.908340
324.957948	15237.976147	28.913357
325.776847	15262.404908	28.918375
325.551145	15301.043792	28.923392
326.362698	15317.121830	28.928410
326.729561	15335.549451	28.933428
327.241197	15373.395025	28.938445
327.612498	15374.719079	28.943463
327.786014	15392.389110	28.948480
328.026497	15413.843473	28.953498
328.555085	15423.934906	28.958516
329.047995	15451.191950	28.963533
328.967264	15468.855283	28.968551
329.407956	15490.743155	28.973568
329.523155	15502.542272	28.978586
330.057513	15528.334626	28.983604
330.265883	15558.203375	28.988621
330.751230	15569.616585	28.993639
331.017051	15595.171354	28.998656
331.569913	15619.288464	29.003674
331.795915	15645.764088	29.008692
331.944116	15664.422140	29.013709
332.110292	15679.324336	29.018727
332.556223	15704.308833	29.023744
332.774180	15729.718843	29.028762
333.169857	15758.655373	29.033780
333.187961	15788.519777	29.038797
333.572284	15811.022665	29.043815
334.112569	15840.792856	29.048832
334.338853	15865.727261	29.053850
334.752548	15896.599782	29.058868
334.868818	15916.844340	29.063885
335.687286	15937.689880	29.068903
335.806721	15968.474108	29.073920
336.525397	15988.630085	29.078938
336.533911	16015.777514	29.083956
336.872776	16041.043471	29.088973
337.390291	16062.364559	29.093991
337.543865	16088.223967	29.099008
338.096050	16103.817672	29.104026
338.479049	16127.545940	29.109044
338.695552	16158.525672	29.114061
339.037911	16174.830376	29.119079
339.560326	16200.398783	29.124096
339.441360	16224.076290	29.129114
340.056004	16249.664186	29.134132
340.352864	16275.014689	29.139149
340.450881	16293.694369	29.144167
340.904293	16334.212489	29.149184
341.041642	16344.090246	29.154202
341.698363	16377.011976	29.159220
341.715936	16408.803770	29.164237
342.570168	16424.070366	29.169255
342.434897	16458.234600	29.174272
342.672823	16480.882428	29.179290
343.464906	16499.597212	29.184308
343.546778	16518.621866	29.189325
344.038228	16550.076994	29.194343
344.484877	16569.391265	29.199360
344.841651	16589.910521	29.204378
345.454531	16608.300427	29.209396
345.325441	16624.630010	29.214413
345.925489	16642.337974	29.219431
346.162175	16663.997931	29.224448
346.335171	16687.118638	29.229466
346.515907	16706.978340	29.234484
346.873651	16737.855389	29.239501
347.521768	16761.807083	29.244519
347.597346	16794.365551	29.249536
347.853700	16817.537272	29.254554
348.207951	16841.890809	29.259572
348.473109	16877.121414	29.264589
349.135329	16895.369488	29.269607
349.344800	16921.692262	29.274624
349.508034	16948.427841	29.279642
350.067683	16981.207634	29.284660
350.114428	17008.094999	29.289677
351.072017	17022.569502	29.294695
351.148779	17058.129595	29.299712
351.891227	17076.394542	29.304730
352.361587	17107.417579	29.309748
352.035626	17137.539977	29.314765
352.508025	17152.695475	29.319783
353.080518	17183.760076	29.324800
353.383752	17219.778001	29.329818
353.945067	17237.912319	29.334836
354.092925	17255.366327	29.339853
354.582862	17279.581402	29.344871
354.790033	17314.032786	29.349888
355.259570	17340.086189	29.354906
355.803576	17360.335808	29.359924
355.765080	17380.122256	29.364941
356.217417	17409.399095	29.369959
356.914020	17430.868863	29.374976
357.432375	17464.912802	29.379994
357.501498	17475.790902	29.385012
357.589961	17509.281843	29.390029
358.220078	17523.032263	29.395047
358.646199	17550.187177	29.400064
359.084523	17575.787394	29.405082
359.630997	17595.352750	29.410100
359.629102	17628.691791	29.415117
360.263641	17641.825217	29.420135
360.923212	17669.909584	29.425152
360.939511	17681.272627	29.430170
361.325815	17704.230186	29.435188
361.535701	17724.519785	29.440205
361.737992	17744.014593	29.445223
362.343784	17771.643000	29.450240
362.704973	17796.236402	29.455258
362.987379	17826.618775	29.460276
363.148987	17853.285142	29.465293
364.018223	17871.228895	29.470311
364.009663	17893.739738	29.475328
364.498683	17920.506513	29.480346
364.741881	17946.880504	29.485364
365.001492	17973.947016	29.490381
365.619390	18001.301084	29.495399
365.840938	18030.766973	29.500416
365.867526	18056.256364	29.505434
366.776704	18079.361214	29.510452
366.930217	18112.866249	29.515469
367.158192	18129.083038	29.520487
367.596688	18152.380967	29.525504
367.614651	18176.721181	29.530522
368.443270	18191.061993	29.535540
368.660285	18222.130620	29.540557
368.873476	18241.100832	29.545575
369.198665	18261.792911	29.550592
369.562674	18292.840495	29.555610
370.166966	18311.922622	29.560628
370.299761	18328.100181	29.565645
370.561140	18363.523735	29.570663
370.912660	18389.377615	29.575680
371.133337	18420.652520	29.580698
371.445537	18449.850340	29.585716
371.786728	18483.208401	29.590733
372.202282	18510.771781	29.595751
372.718106	18541.857762	29.600768
372.827589	18570.833957	29.605786
373.667202	18606.900113	29.610804
373.965556	18638.071135	29.615821
374.198733	18671.024955	29.620839
374.566908	18694.340010	29.625856
374.646283	18725.322000	29.630874
375.428137	18760.091149	29.635892
375.389677	18793.397579	29.640909
376.182999	18825.013578	29.645927
376.624662	18867.675962	29.650944
376.607958	18894.219008	29.655962
377.440734	18922.302050	29.660980
377.693256	18960.140371	29.665997
378.377556	18990.967561	29.671015
378.971798	19017.337172	29.676032
379.043731	19045.860066	29.681050
379.570884	19067.802997	29.686068
379.603970	19103.742007	29.691085
380.403716	19123.579397	29.696103
380.732650	19152.212861	29.701120
381.042860	19182.856380	29.706138
381.776885	19209.617786	29.711156
381.931600	19233.178599	29.716173
382.131526	19253.102800	29.721191
382.566694	19274.317106	29.726208
383.043078	19305.138297	29.731226
383.597378	19324.313415	29.736244
384.012006	19355.884314	29.741261
384.476180	19387.158565	29.746279
384.912825	19407.102106	29.751296
385.095075	19430.647604	29.756314
385.373700	19458.673490	29.761332
385.934942	19489.069498	29.766349
386.497941	19510.256642	29.771367
386.813358	19529.673329	29.776384
387.084649	19554.596360	29.781402
387.594640	19574.780211	29.786420
387.754407	19601.241568	29.791437
387.950971	19634.260100	29.796455
388.498305	19652.989005	29.801472
388.412944	19688.974098	29.806490
388.955459	19711.971632	29.811508
389.147474	19751.565440	29.816525
389.639103	19786.001651	29.821543
390.093948	19818.493792	29.826560
390.241773	19846.436343	29.831578
391.124110	19869.194972	29.836596
391.563511	19908.317801	29.841613
391.499855	19937.936729	29.846631
392.365047	19964.313446	29.851648
392.774881	19994.235649	29.856666
393.288195	20023.314643	29.861684
393.299574	20056.678396	29.866701
393.556645	20088.305128	29.871719
393.941858	20103.290133	29.876736
394.204084	20145.640192	29.881754
394.653621	20174.692164	29.886772
394.928561	20201.457035	29.891789
395.360495	20233.854446	29.896807
395.953189	20251.800820	29.901824
395.954876	20298.094937	29.906842
396.398487	20320.313480	29.911860
396.824837	20356.544829	29.916877
397.594970	20382.073944	29.921895
397.907858	20410.308594	29.926912
397.882361	20441.866084	29.931930
398.611763	20465.681955	29.936948
398.893631	20507.845209	29.941965
399.121333	20544.838248	29.946983
399.971462	20576.683080	29.952000
399.909357	20625.520753	29.957018
400.425618	20646.972488	29.962036
400.967777	20688.787247	29.967053
401.137229	20722.485636	29.972071
401.745841	20753.416893	29.977088
402.104969	20793.094285	29.982106
403.059294	20832.149814	29.987124
403.124187	20855.700964	29.992141
403.186765	20897.458437	29.997159
403.860988	20922.945910	30.002176
404.168310	20964.106476	30.007194
404.771343	20992.803356	30.012212
405.411414	21017.475170	30.017229
405.540970	21056.183669	30.022247
406.064758	21083.356540	30.027264
406.230074	21127.804769	30.032282
406.958546	21162.674462	30.037300
407.510350	21195.342423	30.042317
407.787715	21219.905851	30.047335
408.453451	21252.369017	30.052352
408.436644	21282.744105	30.057370
408.525814	21317.292627	30.062388
408.959848	21361.107306	30.067405
409.506564	21398.459370	30.072423
410.094474	21432.362698	30.077440
410.183300	21474.784210	30.082458
410.743369	21519.076689	30.087476
411.227498	21543.724625	30.092493
411.282997	21587.427517	30.097511
411.871158	21614.089187	30.102528
412.396598	21659.084685	30.107546
412.551019	21683.298596	30.112564
413.163917	21723.462814	30.117581
413.633509	21766.952579	30.122599
414.370828	21803.969681	30.127616
414.495896	21849.651612	30.132634
415.361999	21877.712022	30.137652
415.608390	21919.025329	30.142669
416.073652	21943.998634	30.147687
416.513413	21976.770219	30.152704
417.181513	22015.615691	30.157722
417.489606	22034.714817	30.162740
418.266348	22065.880828	30.167757
418.348118	22096.950616	30.172775
419.119334	22115.720906	30.177792
419.159410	22143.166325	30.182810
419.987839	22158.992779	30.187828
420.577836	22191.071354	30.192845
420.527780	22216.852517	30.197863
421.061222	22232.347848	30.202880
421.391914	22268.356303	30.207898
421.759382	22285.558449	30.212916
422.204015	22313.850167	30.217933
422.336392	22336.641647	30.222951
422.628893	22360.204526	30.227968
422.909181	22398.118508	30.232986
423.445543	22428.219617	30.238004
423.798291	22461.818603	30.243021
424.184284	22497.785280	30.248039
424.840159	22517.166416	30.253056
425.051779	22550.140855	30.258074
425.748503	22585.300992	30.263092
425.987254	22618.239537	30.268109
426.098317	22650.478659	30.273127
426.617739	22694.117088	30.278144
426.526547	22724.532295	30.283162
427.220718	22766.448455	30.288180
427.206015	22800.028499	30.293197
427.710295	22841.525287	30.298215
428.217101	22890.543402	30.303232
428.518591	22940.615870	30.308250
429.089614	22988.067268	30.313268
429.719732	23024.291113	30.318285
429.999164	23075.187602	30.323303
431.016430	23106.549104	30.328320
431.261668	23152.045923	30.333338
431.939302	23192.519863	30.338356
432.328886	23225.153934	30.343373
432.700008	23269.780288	30.348391
433.117310	23306.766903	30.353408
433.573962	23343.264554	30.358426
433.574719	23378.672390	30.363444
434.161714	23419.530867	30.368461
434.645437	23469.514809	30.373479
435.389631	23508.089337	30.378496
435.562418	23548.622438	30.383514
436.059417	23585.210122	30.388532
436.560810	23623.293667	30.393549
436.776690	23668.377256	30.398567
437.669754	23706.432440	30.403584
438.060997	23747.283096	30.408602
438.197100	23791.780974	30.413620
438.891449	23828.550987	30.418637
439.194856	23868.719457	30.423655
439.862976	23904.002173	30.428672
440.328383	23945.645280	30.433690
440.748593	23981.294036	30.438708
441.525220	24003.375577	30.443725
441.736506	24053.832095	30.448743
441.976771	24086.911999	30.453760
442.544069	24122.022614	30.458778
443.198050	24167.722585	30.463796
443.714068	24205.257794	30.468813
443.801096	24241.488942	30.473831
444.231024	24273.774559	30.478848
444.731757	24314.655763	30.483866
445.083098	24355.896109	30.488884
445.863817	24387.313313	30.493901
445.964715	24435.136703	30.498919
446.235114	24459.810050	30.503936
446.969941	24515.536816	30.508954
447.181631	24549.410850	30.513972
447.956598	24583.964478	30.518989
448.424721	24626.804176	30.524007
449.002353	24663.232585	30.529024
449.294909	24701.493447	30.534042
449.776758	24731.052532	30.539060
450.319462	24762.711674	30.544077
450.388670	24805.491668	30.549095
450.779143	24843.402310	30.554112
451.385800	24874.546421	30.559130
451.895090	24907.132355	30.564148
452.537559	24942.683252	30.569165
452.563198	24976.036947	30.574183
453.436813	25009.010671	30.579200
453.488926	25044.129578	30.584218
453.771831	25092.710058	30.589236
454.313908	25111.273985	30.594253
454.643923	25162.322865	30.599271
454.890586	25204.601364	30.604288
455.295792	25246.099886	30.609306
455.353083	25292.235938	30.614324
455.917905	25338.202965	30.619341
456.081450	25391.976897	30.624359
456.948796	25434.638996	30.629376
457.367937	25481.245581	30.634394
457.711790	25534.034395	30.639412
458.621746	25579.762010	30.644429
459.040633	25632.034033	30.649447
459.696535	25675.567592	30.654464
460.094806	25722.477936	30.659482
460.483737	25774.269593	30.664500
461.133674	25811.025979	30.669517
461.671843	25865.439644	30.674535
462.458070	25900.142314	30.679552
463.091308	25939.034032	30.684570
463.008179	25981.665516	30.689588
463.843891	26016.527410	30.694605
463.780505	26070.325238	30.699623
464.658135	26099.865347	30.704640
465.507069	26143.961160	30.709658
465.393839	26198.149308	30.714676
466.377944	26222.230778	30.719693
466.370542	26279.117555	30.724711
466.691010	26313.661555	30.729728
467.175874	26355.039165	30.734746
467.548280	26401.845234	30.739764
468.096610	26444.893838	30.744781
468.581432	26489.378843	30.749799
469.032859	26542.424218	30.754816
469.532701	26589.092994	30.759834
470.382885	26639.006596	30.764852
470.779208	26679.478545	30.769869
470.976266	26726.942240	30.774887
471.854840	26758.950091	30.779904
472.276024	26809.556600	30.784922
472.712201	26850.716333	30.789940
473.356329	26878.444752	30.794957
473.466560	26921.914030	30.799975
473.932509	26970.721864	30.804992
474.887779	27007.237852	30.810010
474.965687	27051.886273	30.815028
475.704467	27092.876637	30.820045
476.088706	27143.367210	30.825063
476.512039	27185.939930	30.830080
476.749452	27224.543584	30.835098
476.919891	27269.830239	30.840116
477.624291	27307.934096	30.845133
477.815826	27361.062839	30.850151
479.025728	27407.143140	30.855168
479.358728	27453.911255	30.860186
479.629051	27488.860218	30.865204
480.153079	27537.940796	30.870221
480.343323	27586.316489	30.875239
480.620197	27629.886147	30.880256
481.683213	27681.139787	30.885274
482.022523	27731.784617	30.890292
482.633092	27773.330937	30.895309
483.209633	27816.239478	30.900327
483.257709	27858.295490	30.905344
484.151973	27890.611996	30.910362
484.484782	27930.015330	30.915380
484.921281	27961.306742	30.920397
485.203795	28004.816467	30.925415
485.649880	28056.438294	30.930432
486.423234	28099.794479	30.935450
486.639274	28150.344201	30.940468
487.394342	28176.810239	30.945485
487.572816	28224.170685	30.950503
487.707068	28272.986590	30.955520
488.625424	28321.275390	30.960538
488.817769	28380.713402	30.965556
489.352788	28428.535935	30.970573
489.978909	28471.500983	30.975591
490.221676	28524.728906	30.980608
490.987491	28572.668227	30.985626
491.211951	28633.332144	30.990644
491.962499	28678.671592	30.995661
492.362278	28735.095212	31.000679
492.932093	28779.136657	31.005696
493.534080	28823.677660	31.010714
494.067861	28879.477004	31.015732
494.685934	28925.552004	31.020749
495.076308	28977.371909	31.025767
495.173265	29029.309927	31.030784
495.965947	29082.142531	31.035802
496.431820	29142.200392	31.040820
496.801649	29188.064771	31.045837
497.543649	29237.442175	31.050855
498.091760	29282.901871	31.055872
498.827109	29330.375082	31.060890
499.290859	29381.672948	31.065908
499.613649	29424.154198	31.070925
500.179568	29480.694703	31.075943
500.776694	29535.201600	31.080960
501.603113	29576.132836	31.085978
501.765745	29620.022929	31.090996
502.088630	29669.723300	31.096013
502.751326	29720.822027	31.101031
503.087253	29773.148627	31.106048
503.810398	29822.521337	31.111066
504.053125	29873.765721	31.116084
505.107678	29922.093204	31.121101
505.248267	29966.451597	31.126119
505.975966	30023.487661	31.131136
506.621595	30058.420681	31.136154
506.487313	30110.261338	31.141172
507.394045	30164.655861	31.146189
508.061031	30213.127152	31.151207
508.370113	30252.902477	31.156224
508.525950	30307.740353	31.161242
508.990301	30358.971566	31.166260
509.427794	30400.533843	31.171277
510.329946	30464.931712	31.176295
510.694380	30524.777611	31.181312
511.114683	30565.690013	31.186330
511.909368	30620.568291	31.191348
512.700563	30664.429553	31.196365
512.854116	30704.827956	31.201383
513.483288	30752.906289	31.206400
513.968312	30805.135564	31.211418
514.474642	30864.741432	31.216436
515.088372	30906.805814	31.221453
515.905810	30948.025705	31.226471
516.018946	31013.849767	31.231488
516.603698	31045.305164	31.236506
517.139805	31089.865979	31.241524
517.404502	31130.243810	31.246541
518.158993	31183.868404	31.251559
518.426101	31221.554629	31.256576
519.329761	31254.484769	31.261594
519.512459	31313.255922	31.266612
520.041169	31344.894667	31.271629
520.489249	31388.852370	31.276647
521.004556	31444.322148	31.281664
521.562807	31493.092620	31.286682
521.723253	31544.806682	31.291700
522.648512	31594.289755	31.296717
523.439111	31642.334336	31.301735
523.641979	31692.139153	31.306752
524.287723	31725.409451	31.311770
524.296227	31796.750329	31.316788
525.104314	31841.656145	31.321805
525.732961	31894.123616	31.326823
525.816355	31950.016689	31.331840
526.240225	31991.824777	31.336858
526.792632	32055.554275	31.341876
527.352106	32119.453224	31.346893
527.880458	32180.299956	31.351911
528.216802	32240.875747	31.356928
529.083865	32292.080642	31.361946
529.373070	32360.600558	31.366964
530.435667	32420.981065	31.371981
530.920112	32464.575699	31.376999
531.324227	32526.261439	31.382016
531.704689	32581.889620	31.387034
532.455821	32644.228336	31.392052
533.229184	32698.154167	31.397069
533.730124	32749.231632	31.402087
534.179012	32814.413585	31.407104
534.761079	32873.385732	31.412122
535.183284	32918.553769	31.417140
535.880958	32974.439934	31.422157
536.480992	33030.986166	31.427175
536.822772	33088.313712	31.432192
537.528192	33138.231920	31.437210
537.854912	33197.752285	31.442228
538.582679	33243.722599	31.447245
539.282548	33299.025634	31.452263
539.598293	33362.865243	31.457280
540.135831	33409.217734	31.462298
540.538668	33472.879234	31.467316
541.040839	33524.047075	31.472333
541.667305	33595.109881	31.477351
542.517422	33655.791661	31.482368
543.026186	33707.214545	31.487386
543.523700	33763.691705	31.492404
544.236396	33817.025071	31.497421
545.007082	33857.663041	31.502439
545.005695	33919.212418	31.507456
545.942063	33965.664461	31.512474
546.614183	34019.241825	31.517492
546.800791	34075.821904	31.522509
548.047123	34124.753987	31.527527
548.519574	34169.651794	31.532544
549.088602	34217.916723	31.537562
549.388092	34267.715909	31.542580
549.767348	34327.480651	31.547597
550.377220	34375.761339	31.552615
550.838926	34417.919155	31.557632
551.764062	34460.969228	31.562650
552.040582	34519.031687	31.567668
552.489389	34571.943905	31.572685
552.701572	34623.693053	31.577703
553.081767	34680.927829	31.582720
553.805639	34715.475229	31.587738
554.299122	34782.430576	31.592756
554.725448	34823.515891	31.597773
555.168113	34876.950744	31.602791
555.871318	34937.547568	31.607808
556.297957	34987.760073	31.612826
557.107521	35044.751393	31.617844
557.324583	35102.393214	31.622861
557.991788	35145.897881	31.627879
558.646828	35216.956082	31.632896
559.045583	35272.643257	31.637914
559.552083	35318.463002	31.642932
560.221939	35391.712839	31.647949
560.758746	35440.721733	31.652967
561.311933	35507.938162	31.657984
561.971255	35560.853176	31.663002
562.577567	35612.521022	31.668020
563.315579	35666.174459	31.673037
564.290057	35725.103700	31.678055
564.521773	35782.470697	31.683072
565.290546	35826.477797	31.688090
565.747958	35884.325369	31.693108
566.498751	35940.388743	31.698125
567.293904	35992.105335	31.703143
567.565337	36053.121367	31.708160
567.864489	36100.931032	31.713178
568.456364	36164.270967	31.718196
568.763021	36215.586137	31.723213
569.754347	36275.429666	31.728231
569.907521	36345.767381	31.733248
570.417815	36395.490233	31.738266
570.982705	36462.304292	31.743284
571.188587	36529.080155	31.748301
572.176453	36594.669560	31.753319
572.822620	36660.549296	31.758336
573.009968	36720.861877	31.763354
573.889857	36794.436151	31.768372
574.209851	36864.590468	31.773389
574.849155	36918.488050	31.778407
575.329248	36997.520165	31.783424
576.119353	37065.110344	31.788442
576.916208	37133.037380	31.793460
577.288477	37202.695130	31.798477
577.853387	37265.999192	31.803495
578.267433	37333.946128	31.808512
579.337472	37402.586492	31.813530
579.913893	37460.296310	31.818548
580.285299	37525.195679	31.823565
581.026040	37581.881290	31.828583
581.586932	37648.413150	31.833600
582.224697	37712.047600	31.838618
582.765294	37782.462504	31.843636
582.953914	37846.948210	31.848653
583.736132	37913.750593	31.853671
584.403617	37978.918235	31.858688
584.769123	38051.013958	31.863706
585.771239	38109.220407	31.868724
586.314775	38180.002510	31.873741
586.970927	38229.084428	31.878759
587.409262	38297.381309	31.883776
588.273109	38363.073378	31.888794
589.035977	38427.560822	31.893812
589.287443	38491.539679	31.898829
589.966814	38548.490974	31.903847
590.765794	38612.666914	31.908864
591.259639	38677.979417	31.913882
591.527545	38724.734238	31.918900
591.940712	38786.392555	31.923917
592.846352	38848.629327	31.928935
593.101421	38901.400008	31.933952
593.776652	38961.131073	31.938970
594.073001	39017.907299	31.943988
594.548365	39088.041309	31.949005
595.147701	39159.272525	31.954023
595.735279	39216.326316	31.959040
596.433528	39288.551796	31.964058
596.756535	39355.337571	31.969076
597.335308	39426.061845	31.974093
598.258857	39496.407369	31.979111
598.804291	39575.739722	31.984128
599.150645	39643.633843	31.989146
600.085955	39706.894556	31.994164
600.629206	39774.987028	31.999181
601.319403	39844.728519	32.004199
601.847087	39911.937026	32.009216
602.523842	39981.416092	32.014234
603.293280	40049.655252	32.019252
603.623090	40126.793809	32.024269
604.643888	40184.874346	32.029287
605.043699	40259.466960	32.034304
605.656137	40325.147680	32.039322
606.441793	40384.675698	32.044340
606.696245	40464.975512	32.049357
607.600680	40525.968059	32.054375
608.210646	40597.970210	32.059392
608.957418	40662.837532	32.064410
609.547480	40731.727648	32.069428
610.331877	40810.312326	32.074445
610.813472	40873.964652	32.079463
611.400515	40938.960392	32.084480
611.742446	41015.522939	32.089498
612.614786	41082.631339	32.094516
612.948240	41152.042176	32.099533
613.649547	41228.394613	32.104551
614.078602	41303.352815	32.109568
614.886870	41373.803508	32.114586
615.730632	41441.681937	32.119604
616.150978	41514.644038	32.124621
616.968425	41578.565242	32.129639
617.624961	41649.180996	32.134656
618.039721	41719.256117	32.139674
618.716042	41786.462642	32.144692
618.897186	41871.472109	32.149709
619.776481	41940.104188	32.154727
620.359335	42021.739234	32.159744
620.926010	42100.371722	32.164762
621.561478	42168.375671	32.169780
622.364689	42249.747948	32.174797
623.120516	42311.241386	32.179815
623.825098	42397.742090	32.184832
624.397978	42466.193175	32.189850
625.081658	42541.973009	32.194868
625.344125	42619.941334	32.199885
625.874603	42696.324913	32.204903
626.705458	42767.209699	32.209920
627.534439	42835.338777	32.214938
628.316190	42903.832689	32.219956
628.485250	42985.571991	32.224973
629.330097	43057.838459	32.229991
630.371284	43119.682021	32.235008
630.523962	43204.165533	32.240026
631.030670	43266.189566	32.245044
631.805232	43341.281943	32.250061
632.451679	43400.400646	32.255079
633.244842	43483.964865	32.260096
634.085268	43547.128106	32.265114
634.704907	43602.235696	32.270132
634.761864	43664.704870	32.275149
635.801530	43721.227301	32.280167
636.425499	43795.547592	32.285184
636.704415	43866.868865	32.290202
637.520916	43930.305741	32.295220
637.950634	44005.486251	32.300237
638.803757	44069.132245	32.305255
639.579224	44144.994963	32.310272
640.113412	44220.954739	32.315290
640.645694	44278.042730	32.320308
640.768401	44353.869036	32.325325
641.242280	44431.601535	32.330343
641.825856	44510.989705	32.335360
642.492559	44586.689063	32.340378
643.421978	44670.630723	32.345396
643.786584	44752.800067	32.350413
644.670632	44844.849212	32.355431
645.197350	44928.634455	32.360448
645.288367	45013.278399	32.365466
646.488588	45089.883013	32.370484
647.168245	45187.591404	32.375501
647.934701	45259.408836	32.380519
648.615254	45343.448347	32.385536
649.079302	45438.354949	32.390554
650.109348	45509.918163	32.395572
650.720787	45604.273878	32.400589
651.663464	45671.083992	32.405607
652.324514	45752.052913	32.410624
652.613032	45839.440388	32.415642
653.444859	45908.590637	32.420660
654.274291	46002.981749	32.425677
654.974021	46078.331114	32.430695
655.901413	46154.738879	32.435712
656.534990	46226.149347	32.440730
657.101084	46304.591130	32.445748
657.620235	46380.704190	32.450765
658.597227	46456.880761	32.455783
659.300325	46526.837716	32.460800
659.934284	46609.854775	32.465818
660.736423	46679.716962	32.470836
661.237096	46759.999876	32.475853
661.721054	46824.963620	32.480871
662.581712	46897.876962	32.485888
662.914256	46980.686552	32.490906
663.952054	47052.645903	32.495924
664.514071	47129.465414	32.500941
665.092466	47205.638295	32.505959
665.637817	47283.869650	32.510976
665.881848	47372.446313	32.515994
666.896320	47446.969009	32.521012
667.987790	47531.594477	32.526029
668.720847	47612.881541	32.531047
669.306098	47676.931388	32.536064
669.566491	47758.973092	32.541082
670.765745	47840.686140	32.546100
671.323702	47919.053812	32.551117
671.486587	47983.029283	32.556135
672.430434	48058.822987	32.561152
672.959380	48157.629563	32.566170
673.667098	48226.928787	32.571188
674.205196	48310.594425	32.576205
674.737334	48392.410717	32.581223
675.484828	48464.518166	32.586240
675.960225	48568.609914	32.591258
677.171088	48641.933088	32.596276
677.830225	48713.645522	32.601293
678.657866	48782.781639	32.606311
679.255466	48847.866111	32.611328
679.543111	48923.219093	32.616346
680.780386	48984.894656	32.621364
681.195414	49066.360518	32.626381
681.636794	49144.073450	32.631399
682.444166	49214.019843	32.636416
682.497128	49293.790535	32.641434
683.771389	49370.529644	32.646452
684.335956	49454.483298	32.651469
684.490566	49528.619422	32.656487
685.430643	49615.846904	32.661504
685.944249	49699.393148	32.666522
686.680713	49777.890483	32.671540
687.459073	49867.186191	32.676557
687.614057	49959.810204	32.681575
688.546110	50048.020086	32.686592
689.123738	50146.626688	32.691610
690.136140	50231.719338	32.696628
690.341513	50319.232620	32.701645
691.418944	50413.696070	32.706663
692.384582	50503.396455	32.711680
693.090812	50598.939263	32.716698
693.630230	50677.510751	32.721716
694.483978	50777.331997	32.726733
695.136258	50869.953906	32.731751
695.952313	50956.465688	32.736768
696.299922	51043.143788	32.741786
697.578608	51125.675740	32.746804
698.179111	51213.847864	32.751821
698.909456	51304.589014	32.756839
699.726511	51388.815685	32.761856
699.977982	51482.865051	32.766874
700.873104	51568.715790	32.771892
701.889465	51664.256761	32.776909
702.196459	51739.977606	32.781927
702.652094	51835.890144	32.786944
703.615903	51936.153997	32.791962
704.350705	52026.266021	32.796980
705.233548	52111.230408	32.801997
705.624615	52213.100331	32.807015
706.400140	52301.235791	32.812032
706.881298	52398.517801	32.817050
707.824025	52495.066900	32.822068
708.421089	52583.391096	32.827085
709.247423	52673.648910	32.832103
710.360695	52768.598024	32.837120
711.097782	52862.662154	32.842138
711.940316	52942.803685	32.847156
712.775345	53031.602287	32.852173
713.335369	53122.607508	32.857191
714.245221	53203.389716	32.862208
714.876429	53282.443000	32.867226
715.282764	53369.064848	32.872244
715.971220	53456.960876	32.877261
716.805930	53561.165270	32.882279
717.673479	53639.795497	32.887296
718.137248	53734.344964	32.892314
718.654546	53811.188926	32.897332
719.459417	53901.070532	32.902349
719.827410	54003.060976	32.907367
721.027654	54094.110111	32.912384
721.685249	54184.617604	32.917402
722.416460	54264.934583	32.922420
723.047750	54366.011428	32.927437
724.067160	54469.002232	32.932455
724.916441	54542.552819	32.937472
725.070942	54638.225582	32.942490
725.993347	54710.981218	32.947508
726.860810	54806.631638	32.952525
727.186949	54891.213623	32.957543
728.082264	54972.852172	32.962560
729.051382	55060.355087	32.967578
729.840098	55133.810478	32.972596
730.648109	55219.344081	32.977613
730.985442	55298.826857	32.982631
731.418676	55376.303718	32.987648
731.962175	55480.446360	32.992666
733.047458	55568.418842	32.997684
733.866111	55650.824792	33.002701
734.524209	55748.662757	33.007719
734.923519	55844.572550	33.012736
735.963981	55944.768326	33.017754
736.669329	56032.673016	33.022772
737.400675	56130.507062	33.027789
737.859689	56228.835278	33.032807
738.666808	56325.874206	33.037824
739.766544	56430.928208	33.042842
740.560898	56520.583321	33.047860
741.387340	56619.749986	33.052877
741.844837	56712.229415	33.057895
742.799152	56796.513386	33.062912
743.686769	56899.721857	33.067930
744.221518	56991.892803	33.072948
744.996753	57087.973881	33.077965
745.571561	57200.158324	33.082983
746.438172	57286.702191	33.088000
746.877772	57376.539889	33.093018
747.813465	57481.721341	33.098036
748.861460	57580.565435	33.103053
749.353960	57673.688087	33.108071
750.220104	57775.703947	33.113088
751.088825	57883.268355	33.118106
751.825257	57970.942607	33.123124
752.674111	58067.951484	33.128141
753.546799	58169.848193	33.133159
754.304459	58246.833836	33.138176
755.017337	58354.685646	33.143194
755.706979	58452.272514	33.148212
756.609522	58549.635050	33.153229
757.211274	58647.648178	33.158247
758.369608	58742.106525	33.163264
758.800245	58833.089757	33.168282
759.615467	58930.190506	33.173300
760.362705	59016.767887	33.178317
761.428239	59118.953486	33.183335
762.240249	59212.776141	33.188352
762.829659	59308.866967	33.193370
763.380400	59409.742493	33.198388
764.473702	59493.427037	33.203405
765.034624	59594.099559	33.208423
765.667189	59695.443290	33.213440
766.797640	59784.842490	33.218458
767.377494	59877.663822	33.223476
768.024217	59976.788280	33.228493
768.614430	60081.945636	33.233511
769.744873	60171.548785	33.238528
770.553612	60276.481399	33.243546
771.194190	60375.008398	33.248564
772.031200	60465.944382	33.253581
772.500004	60562.901684	33.258599
773.416750	60663.558571	33.263616
774.232595	60769.124578	33.268634
774.881118	60872.133780	33.273652
775.785513	60956.614044	33.278669
776.325845	61067.409882	33.283687
777.188723	61147.543035	33.288704
777.803711	61244.207615	33.293722
778.406042	61344.357344	33.298740
779.158692	61427.840735	33.303757
779.749712	61538.731871	33.308775
780.504305	61626.968819	33.313792
781.494206	61730.570582	33.318810
781.810273	61826.604727	33.323828
782.773455	61927.620438	33.328845
783.534221	62039.200443	33.333863
784.387041	62129.028768	33.338880
785.286952	62243.930547	33.343898
785.966508	62347.403455	33.348916
786.731595	62448.296473	33.353933
787.341080	62556.402560	33.358951
788.052011	62672.892929	33.363968
789.078125	62781.443282	33.368986
789.804162	62898.444424	33.374004
790.431427	63004.615701	33.379021
791.181008	63121.190704	33.384039
791.797685	63232.042480	33.389056
792.688545	63340.226238	33.394074
793.735172	63466.596042	33.399092
794.833612	63574.538095	33.404109
795.328251	63688.364499	33.409127
796.229198	63792.187308	33.414144
797.169399	63909.582276	33.419162
797.879483	64027.749243	33.424180
799.079066	64132.573705	33.429197
799.451829	64247.681287	33.434215
800.143363	64362.256353	33.439232
801.006571	64474.610109	33.444250
802.135643	64588.437659	33.449268
802.866574	64707.249836	33.454285
803.583988	64821.722009	33.459303
804.485707	64940.469340	33.464320
805.447416	65045.698083	33.469338
806.078541	65170.952196	33.474356
807.112664	65267.073192	33.479373
807.860733	65379.981898	33.484391
809.062296	65498.423622	33.489408
809.774745	65605.725705	33.494426
810.242808	65716.969333	33.499444
811.177770	65819.848356	33.504461
812.078771	65946.320530	33.509479
812.988825	66053.478431	33.514496
813.966986	66157.730153	33.519514
814.472334	66266.005523	33.524532
815.464464	66386.592139	33.529549
816.070963	66504.531057	33.534567
816.888164	66608.558756	33.539584
817.768270	66720.605684	33.544602
818.276162	66836.741997	33.549620
819.465388	66944.686478	33.554637
820.294065	67066.916192	33.559655
821.026207	67173.299982	33.564672
822.092755	67290.452796	33.569690
822.940950	67406.200880	33.574708
823.957530	67506.166379	33.579725
824.288046	67627.078162	33.584743
825.192218	67733.006395	33.589760
826.142730	67844.345858	33.594778
826.677606	67960.174084	33.599796
827.613613	68068.994445	33.604813
828.518199	68177.529724	33.609831
829.206661	68293.764307	33.614848
830.092261	68401.924517	33.619866
830.465604	68524.775387	33.624884
831.475204	68632.189154	33.629901
832.471021	68754.729753	33.634919
833.187270	68855.807192	33.639936
833.958908	68955.314216	33.644954
834.570284	69066.943803	33.649972
835.665582	69177.210396	33.654989
836.222537	69295.046596	33.660007
836.920818	69400.144636	33.665024
837.832192	69516.905450	33.670042
838.776228	69636.095860	33.675060
839.513557	69738.685197	33.680077
840.566005	69868.747252	33.685095
841.144282	69991.958384	33.690112
842.594717	70103.024645	33.695130
843.001580	70225.449784	33.700148
844.073970	70333.987261	33.705165
844.890130	70454.082301	33.710183
845.748690	70574.512458	33.715200
846.540984	70688.966065	33.720218
847.131449	70812.331652	33.725236
847.990479	70923.417768	33.730253
848.886916	71056.984369	33.735271
849.621641	71184.824189	33.740288
850.809736	71291.488267	33.745306
851.451857	71427.464212	33.750324
852.542256	71547.741324	33.755341
853.522035	71677.649286	33.760359
854.239914	71799.804286	33.765376
855.226848	71916.325346	33.770394
856.311173	72037.194290	33.775412
857.335351	72159.635822	33.780429
858.063365	72276.397678	33.785447
858.972874	72396.500742	33.790464
860.131426	72506.053040	33.795482
860.801911	72631.325578	33.800500
861.784507	72734.773961	33.805517
862.686475	72852.395494	33.810535
863.355648	72969.417442	33.815552
864.411117	73085.863887	33.820570
864.782451	73219.916436	33.825588
866.382737	73333.580055	33.830605
867.148352	73444.555423	33.835623
867.672320	73573.139830	33.840640
868.250069	73690.427409	33.845658
868.656995	73828.898422	33.850676
870.308971	73950.677027	33.855693
870.963257	74081.013664	33.860711
871.803374	74199.810038	33.865728
872.792467	74325.254636	33.870746
873.342679	74454.168745	33.875764
874.164716	74575.702293	33.880781
875.066944	74705.223727	33.885799
875.675958	74842.010698	33.890816
876.682986	74958.747079	33.895834
877.634437	75096.883056	33.900852
878.426554	75230.132005	33.905869
879.286887	75373.331846	33.910887
880.202644	75511.248634	33.915904
881.016999	75639.189939	33.920922
882.093703	75769.163130	33.925940
883.128964	75903.286703	33.930957
883.563233	76030.047135	33.935975
884.446230	76174.690489	33.940992
885.591138	76296.717743	33.946010
886.254439	76444.593287	33.951028
887.076148	76570.419887	33.956045
887.910150	76699.742923	33.961063
888.806850	76846.583185	33.966080
889.864784	76970.462805	33.971098
890.341019	77100.182567	33.976116
891.187140	77225.275115	33.981133
892.396660	77353.818778	33.986151
892.732109	77485.467962	33.991168
894.256795	77615.232393	33.996186
895.066345	77754.420441	34.001204
895.681041	77883.691734	34.006221
896.668638	78010.681880	34.011239
897.086021	78154.118377	34.016256
898.184134	78297.829072	34.021274
898.920012	78429.910979	34.026292
899.928584	78576.763089	34.031309
900.667219	78715.260366	34.036327
901.512828	78859.010085	34.041344
902.930342	78999.825904	34.046362
903.598812	79150.893997	34.051380
904.379447	79297.427938	34.056397
905.514417	79434.744433	34.061415
906.369471	79583.140369	34.066432
907.415200	79724.180343	34.071450
908.309653	79872.603294	34.076468
909.334616	80023.409513	34.081485
910.530500	80154.641031	34.086503
911.328900	80309.819954	34.091520
912.023050	80442.236846	34.096538
913.041168	80595.116638	34.101556
913.821515	80740.002513	34.106573
914.942130	80885.952784	34.111591
915.719738	81031.878473	34.116608
916.376975	81184.429675	34.121626
917.477297	81330.942869	34.126644
918.394142	81480.878296	34.131661
919.611053	81626.526371	34.136679
920.250771	81773.270408	34.141696
921.632006	81921.872964	34.146714
922.556423	82063.421995	34.151732
923.295430	82219.806805	34.156749
924.451602	82361.363638	34.161767
925.219553	82511.419009	34.166784
926.391733	82655.676503	34.171802
927.070547	82816.649551	34.176820
927.829622	82963.824337	34.181837
929.088750	83105.577512	34.186855
929.894331	83258.611476	34.191872
931.127329	83404.394711	34.196890
932.203679	83551.324645	34.201908
932.682610	83703.713281	34.206925
933.854188	83856.026344	34.211943
934.658674	84002.422011	34.216960
935.461714	84147.249713	34.221978
936.480484	84305.241126	34.226996
937.346474	84452.736719	34.232013
938.745761	84598.835320	34.237031
939.244934	84759.307445	34.242048
940.221846	84894.670729	34.247066
941.031903	85050.797194	34.252084
941.793927	85198.827225	34.257101
942.812346	85358.781019	34.262119
943.666279	85517.548228	34.267136
944.898450	85664.839080	34.272154
945.931509	85822.363850	34.277172
946.824422	85979.653421	34.282189
947.732743	86126.273052	34.287207
948.430319	86296.252383	34.292224
949.495748	86443.809829	34.297242
950.261699	86593.252783	34.302260
950.965810	86743.010648	34.307277
952.269965	86890.588372	34.312295
952.854322	87043.120571	34.317312
953.898140	87192.445442	34.322330
954.905109	87341.979848	34.327348
955.711383	87484.884968	34.332365
956.952520	87631.167842	34.337383
957.870914	87799.817912	34.342400
958.797496	87946.211699	34.347418
959.792753	88093.499966	34.352436
960.717380	88233.573985	34.357453
961.908258	88387.685205	34.362471
962.691611	88546.940118	34.367488
963.804974	88693.136758	34.372506
964.509985	88856.703648	34.377524
965.526568	89004.930634	34.382541
966.908776	89154.857399	34.387559
967.582647	89326.185037	34.392576
968.499656	89478.437380	34.397594
969.562379	89627.749112	34.402612
970.588319	89785.662152	34.407629
971.375817	89932.135430	34.412647
972.215089	90105.998079	34.417664
973.516944	90262.634531	34.422682
974.396567	90422.202444	34.427700
975.143568	90585.407117	34.432717
976.502557	90745.954827	34.437735
977.280279	90912.821067	34.442752
978.608129	91067.901539	34.447770
979.593480	91232.729370	34.452788
980.308094	91384.432311	34.457805
981.299852	91549.913136	34.462823
982.438878	91715.649222	34.467840
983.787956	91879.687130	34.472858
985.021060	92034.966680	34.477876
986.134142	92193.229167	34.482893
986.717938	92343.782490	34.487911
987.716642	92504.496369	34.492928
988.560743	92662.369655	34.497946
989.460706	92818.842250	34.502964
990.258702	92986.770070	34.507981
991.615320	93152.562240	34.512999
992.203268	93324.362798	34.518016
993.489259	93498.163227	34.523034
994.490717	93649.725234	34.528052
994.932004	93829.744146	34.533069
996.290024	93992.193352	34.538087
996.876160	94169.336086	34.543104
998.257677	94343.120366	34.548122
999.065038	94499.182227	34.553140
1000.516016	94688.035199	34.558157
1001.663660	94846.473678	34.563175
1002.741430	95017.774619	34.568192
1003.555436	95182.891598	34.573210
1004.754846	95342.400798	34.578228
1005.433745	95512.486104	34.583245
1006.742171	95671.314729	34.588263
1007.424747	95844.585773	34.593280
1008.414422	96014.787713	34.598298
1009.686140	96177.309846	34.603316
1010.776849	96352.112169	34.608333
1011.837758	96501.909315	34.613351
1012.736279	96684.202924	34.618368
1013.728118	96853.827827	34.623386
1014.832687	97011.445261	34.628404
1015.207545	97184.358660	34.633421
1016.105046	97360.130558	34.638439
1017.250447	97537.711242	34.643456
1018.408932	97699.249074	34.648474
1019.667649	97857.941539	34.653492
1020.235626	98029.872876	34.658509
1021.458559	98178.007234	34.663527
1022.775121	98341.403291	34.668544
1023.774165	98502.782706	34.673562
1024.887195	98654.673250	34.678580
1025.381357	98822.747660	34.683597
1026.704291	98988.172746	34.688615
1027.714988	99155.435890	34.693632
1028.397474	99315.847189	34.698650
1029.669754	99476.415228	34.703668
1030.233573	99659.121207	34.708685
1031.262236	99829.196846	34.713703
1032.073999	100004.697375	34.718720
1033.322236	100168.135470	34.723738
1034.683490	100347.631186	34.728756
1035.064034	100537.927033	34.733773
1036.128870	100717.493343	34.738791
1036.974249	100891.430526	34.743808
1038.260197	101088.108499	34.748826
1039.351109	101260.924895	34.753844
1040.393245	101465.066651	34.758861
1042.016256	101641.564933	34.763879
1042.361016	101840.715317	34.768896
1043.511955	102020.244811	34.773914
1045.055612	102199.761275	34.778932
1045.553246	102400.150710	34.783949
1047.205284	102563.556239	34.788967
1048.104861	102766.408463	34.793984
1049.059232	102944.241903	34.799002
1050.344163	103133.799456	34.804020
1050.998082	103334.455184	34.809037
1052.141525	103514.376162	34.814055
1053.524035	103710.861767	34.819072
1054.561818	103901.542221	34.824090
1056.021773	104093.585352	34.829108
1056.621035	104272.816312	34.834125
1057.851661	104456.516057	34.839143
1058.798508	104645.367905	34.844160
1060.096899	104845.143419	34.849178
1061.369608	105024.888734	34.854196
1062.395550	105215.466686	34.859213
1063.629060	105399.603137	34.864231
1064.823853	105587.546836	34.869248
1065.220328	105780.803968	34.874266
1066.628006	105954.023311	34.879284
1067.702693	106156.480112	34.884301
1068.677409	106338.183428	34.889319
1069.744556	106532.513037	34.894336
1070.886149	106719.472947	34.899354
1072.001665	106901.270813	34.904372
1072.791610	107099.196812	34.909389
1074.065108	107289.546039	34.914407
1075.026217	107477.250382	34.919424
1075.727700	107664.910298	34.924442
1077.219177	107858.368740	34.929460
1077.989835	108056.038989	34.934477
1078.994559	108249.264055	34.939495
1080.281792	108446.965764	34.944512
1081.129938	108647.439513	34.949530
1082.670367	108837.413553	34.954548
1083.638702	109033.512927	34.959565
1084.894663	109227.792796	34.964583
1085.917492	109430.004156	34.969600
1086.610738	109624.772573	34.974618
1088.111961	109821.524225	34.979636
1089.239709	110019.251090	34.984653
1089.871238	110211.677781	34.989671
1091.057421	110403.127404	34.994688
1092.108040	110578.626976	34.999706
1093.148193	110774.967685	35.004724
1093.873018	110959.175563	35.009741
1094.842787	111150.653514	35.014759
1095.859211	111340.212229	35.019776
1097.145856	111549.464327	35.024794
1098.707537	111733.247665	35.029812
1099.540139	111931.366461	35.034829
1100.258086	112124.121614	35.039847
1101.474075	112321.331043	35.044864
1102.170333	112532.119702	35.049882
1103.433015	112730.021080	35.054900
1104.645065	112942.868566	35.059917
1105.989374	113140.696026	35.064935
1107.161931	113343.202743	35.069952
1108.348954	113548.039619	35.074970
1109.843726	113743.426710	35.079988
1110.538124	113948.753367	35.085005
1111.584528	114149.551106	35.090023
1113.059959	114352.065722	35.095040
1113.806619	114563.051395	35.100058
1115.176212	114755.919681	35.105076
1115.891889	114977.517920	35.110093
1117.082336	115192.603219	35.115111
1118.319049	115391.528569	35.120128
1119.357674	115612.305532	35.125146
1120.507145	115824.196927	35.130164
1121.407704	116039.121178	35.135181
1123.021610	116250.736250	35.140199
1124.480108	116475.631643	35.145216
1125.186987	116688.806306	35.150234
1126.254065	116895.118996	35.155252
1127.403698	117114.634866	35.160269
1128.759376	117335.119331	35.165287
1129.724720	117545.140660	35.170304
1130.750342	117764.720009	35.175322
1131.821737	117983.976690	35.180340
1132.858891	118213.314136	35.185357
1134.076404	118435.679825	35.190375
1135.370554	118657.109554	35.195392
1136.073618	118892.767177	35.200410
1137.480770	119109.784740	35.205428
1138.340757	119341.808712	35.210445
1139.712483	119560.609498	35.215463
1140.610064	119785.534697	35.220480
1141.905133	120026.691825	35.225498
1143.486108	120255.397898	35.230516
1144.380105	120483.142201	35.235533
1145.396336	120706.762308	35.240551
1146.705312	120935.581997	35.245568
1147.750883	121160.924115	35.250586
1149.408413	121393.326675	35.255604
1150.046281	121620.006925	35.260621
1151.534003	121839.084276	35.265639
1152.692381	122069.179537	35.270656
1153.778095	122304.319675	35.275674
1155.124932	122513.135002	35.280692
1156.190582	122749.004315	35.285709
1157.291927	122974.870555	35.290727
1158.452179	123194.975154	35.295744
1159.414326	123433.591693	35.300762
1160.747296	123660.286582	35.305780
1161.859718	123891.658113	35.310797
1162.892973	124120.902680	35.315815
1163.907774	124340.874946	35.320832
1165.225562	124585.740598	35.325850
1166.757453	124800.903430	35.330868
1167.428383	125019.682759	35.335885
1168.930769	125239.530245	35.340903
1170.467746	125447.928904	35.345920
1171.468841	125670.688688	35.350938
1172.632241	125873.917577	35.355956
1173.571962	126092.558770	35.360973
1174.675351	126308.791673	35.365991
1175.997560	126514.356001	35.371008
1177.075905	126736.451681	35.376026
1178.082310	126949.713913	35.381044
1179.364658	127170.765023	35.386061
1180.331405	127395.570949	35.391079
1181.546622	127618.740386	35.396096
1182.595040	127847.870933	35.401114
1183.829416	128075.438734	35.406132
1185.102270	128307.983214	35.411149
1185.996936	128548.615439	35.416167
1187.489686	128771.874019	35.421184
1188.288248	129009.699054	35.426202
1189.714466	129247.574246	35.431220
1191.083938	129476.955206	35.436237
1192.009079	129724.461658	35.441255
1193.422890	129958.389416	35.446272
1194.317824	130201.430001	35.451290
1195.598421	130435.953734	35.456308
1196.741920	130679.590703	35.461325
1197.692922	130929.320634	35.466343
1199.542496	131162.576783	35.471360
1200.687577	131416.068691	35.476378
1202.134698	131658.750250	35.481396
1203.047230	131887.095943	35.486413
1204.079907	132146.025155	35.491431
1205.529030	132377.695695	35.496448
1206.837664	132631.880080	35.501466
1207.683733	132882.529959	35.506484
1209.036711	133130.740035	35.511501
1210.057925	133381.009862	35.516519
1211.471725	133623.014466	35.521536
1212.614574	133877.629025	35.526554
1213.757208	134133.145715	35.531572
1214.984430	134383.287770	35.536589
1216.053582	134648.595113	35.541607
1217.271591	134895.623872	35.546624
1218.504748	135155.127093	35.551642
1219.917492	135411.547263	35.556660
1221.063599	135678.434944	35.561677
1222.393959	135929.953628	35.566695
1224.004722	136181.668761	35.571712
1224.982569	136439.677502	35.576730
1226.347805	136692.210470	35.581748
1227.735076	136946.149037	35.586765
1228.639090	137204.125180	35.591783
1230.411885	137451.436271	35.596800
1231.355468	137707.786856	35.601818
1232.533892	137964.480947	35.606836
1233.924579	138220.241689	35.611853
1235.153905	138474.610968	35.616871
1236.421437	138725.235444	35.621888
1237.645091	138984.376907	35.626906
1238.888264	139235.884057	35.631924
1240.391937	139493.613727	35.636941
1241.678313	139737.040529	35.641959
1242.921217	139994.550805	35.646976
1244.093013	140250.515143	35.651994
1245.405333	140505.519843	35.657012
1246.620284	140742.308593	35.662029
1247.875831	141006.912511	35.667047
1248.988196	141243.036921	35.672064
1249.814081	141488.936104	35.677082
1251.214591	141732.801945	35.682100
1252.321982	141957.709864	35.687117
1253.299816	142211.793324	35.692135
1254.500774	142458.322105	35.697152
1255.623240	142708.378168	35.702170
1256.689283	142952.536055	35.707188
1257.868715	143211.564335	35.712205
1259.175905	143464.499179	35.717223
1260.664118	143724.773656	35.722240
1261.805712	143987.047564	35.727258
1262.834017	144250.787807	35.732276
1264.194478	144513.841032	35.737293
1265.241151	144780.219893	35.742311
1266.643653	145053.428041	35.747328
1267.808354	145326.068854	35.752346
1268.847358	145592.784746	35.757364
1270.257122	145871.831547	35.762381
1271.388532	146161.224297	35.767399
1273.011454	146428.927825	35.772416
1274.055619	146709.411177	35.777434
1275.390391	146989.785249	35.782452
1276.523668	147265.007684	35.787469
1277.798446	147548.680702	35.792487
1279.237973	147831.529682	35.797504
1280.619343	148116.483095	35.802522
1282.079330	148402.034493	35.807540
1283.817672	148686.552827	35.812557
1284.466128	148973.954957	35.817575
1285.947650	149241.397985	35.822592
1287.222519	149526.189603	35.827610
1288.585525	149821.254952	35.832628
1289.988847	150102.491101	35.837645
1291.375480	150394.576471	35.842663
1292.830507	150674.476595	35.847680
1293.780279	150968.147957	35.852698
1295.377085	151254.599078	35.857716
1296.510341	151547.458213	35.862733
1297.730704	151831.832336	35.867751
1299.311932	152116.567510	35.872768
1300.731378	152411.377373	35.877786
1302.207420	152695.817137	35.882804
1303.591871	152966.727296	35.887821
1304.523432	153272.685121	35.892839
1306.091371	153546.296171	35.897856
1307.317412	153834.527573	35.902874
1308.277553	154124.821925	35.907892
1310.581905	154409.873103	35.912909
1311.688040	154695.086340	35.917927
1313.237506	154984.592011	35.922944
1314.489898	155263.607628	35.927962
1315.585479	155542.042249	35.932980
1317.019318	155823.974795	35.937997
1318.201477	156104.479443	35.943015
1319.540089	156391.087273	35.948032
1320.963462	156666.519907	35.953050
1322.309332	156958.001845	35.958068
1323.813353	157230.684946	35.963085
1324.565348	157507.008144	35.968103
1326.242530	157797.553413	35.973120
1327.769898	158086.070408	35.978138
1328.685986	158379.092539	35.983156
1330.172042	158661.099823	35.988173
1331.026489	158949.188653	35.993191
1332.702614	159225.700664	35.998208
1333.538964	159524.681389	36.003226
1334.449118	159824.908051	36.008244
1336.506961	160106.120336	36.013261
1337.578324	160384.554259	36.018279
1338.800801	160670.298020	36.023296
1339.938547	160950.196427	36.028314
1341.033302	161233.491225	36.033332
1342.570173	161517.298477	36.038349
1343.898545	161813.270971	36.043367
1345.572520	162089.815100	36.048384
1346.562063	162385.606552	36.053402
1347.986511	162668.387092	36.058420
1349.506786	162959.210204	36.063437
1350.146895	163256.854400	36.068455
1352.100338	163540.555622	36.073472
1353.186568	163845.755442	36.078490
1354.195510	164153.710764	36.083508
1355.870906	164449.022516	36.088525
1356.876474	164762.844537	36.093543
1358.388150	165067.246771	36.098560
1359.870590	165365.578340	36.103578
1361.148316	165681.557051	36.108596
1362.645493	165994.012481	36.113613
1363.792723	166306.781730	36.118631
1365.059378	166618.493000	36.123648
1366.857937	166935.397019	36.128666
1368.082232	167258.044666	36.133684
1369.791403	167563.154755	36.138701
1371.024493	167880.273135	36.143719
1372.380981	168186.828838	36.148736
1373.848956	168504.128509	36.153754
1375.129338	168825.445795	36.158772
1376.546713	169135.741161	36.163789
1377.944580	169462.233422	36.168807
1380.012453	169781.232061	36.173824
1381.291135	170097.736614	36.178842
1382.196006	170410.536312	36.183860
1383.607970	170731.350329	36.188877
1385.054507	171051.209120	36.193895
1386.535342	171369.605110	36.198912
1387.656063	171689.369841	36.203930
1389.263462	172021.187975	36.208948
1390.882361	172338.983990	36.213965
1391.941441	172665.262863	36.218983
1393.221363	172988.702936	36.224000
1394.577019	173314.658071	36.229018
1396.240796	173650.970675	36.234036
1397.769293	173974.668221	36.239053
1399.171089	174307.716483	36.244071
1400.465427	174632.891179	36.249088
1401.730845	174956.562626	36.254106
1402.886541	175281.574205	36.259124
1404.869075	175613.088678	36.264141
1406.030002	175954.132531	36.269159
1407.722845	176278.770049	36.274176
1409.423833	176601.669654	36.279194
1410.475675	176935.846965	36.284212
1412.061438	177256.548878	36.289229
1413.159724	177591.700130	36.294247
1414.683861	177933.623985	36.299264
1416.528910	178255.012833	36.304282
1417.550615	178582.758708	36.309300
1419.264226	178904.642975	36.314317
1420.748977	179240.134695	36.319335
1422.129325	179567.484931	36.324352
1423.703189	179897.813279	36.329370
1424.907477	180226.554828	36.334388
1426.409912	180543.546984	36.339405
1427.827868	180886.929564	36.344423
1428.978827	181204.948416	36.349440
1430.740461	181529.582573	36.354458
1432.025222	181855.312921	36.359476
1433.715233	182150.947655	36.364493
1435.093563	182461.130537	36.369511
1436.173169	182768.026389	36.374528
1437.526838	183080.514308	36.379546
1438.659713	183403.423287	36.384564
1440.248549	183713.121645	36.389581
1441.568674	184042.438802	36.394599
1442.974691	184366.196865	36.399616
1444.420336	184686.865847	36.404634
1445.309784	185019.928352	36.409652
1447.233002	185357.937447	36.414669
1448.436243	185692.246850	36.419687
1449.654889	186051.079502	36.424704
1451.320897	186372.546853	36.429722
1452.291396	186720.914512	36.434740
1454.108718	187064.028817	36.439757
1455.601617	187418.064674	36.444775
1456.694666	187767.053161	36.449792
1458.019413	188121.057665	36.454810
1459.553146	188476.299203	36.459828
1460.840306	188824.487653	36.464845
1462.061321	189185.294417	36.469863
1463.429715	189554.114504	36.474880
1465.453618	189928.502946	36.479898
1466.676936	190282.588033	36.484916
1468.287415	190652.187378	36.489933
1469.552621	191036.140128	36.494951
1471.199912	191409.571798	36.499968
1473.034264	191776.640189	36.504986
1473.942961	192155.644508	36.510004
1475.426996	192517.773474	36.515021
1477.338252	192895.245643	36.520039
1478.895499	193274.911364	36.525056
1480.583030	193653.859635	36.530074
1481.646519	194028.812759	36.535092
1483.485085	194403.462307	36.540109
1485.070663	194773.890233	36.545127
1486.500806	195156.647834	36.550144
1488.367916	195520.762028	36.555162
1489.571449	195901.809516	36.560180
1491.213359	196274.026821	36.565197
1492.577223	196657.362830	36.570215
1494.141541	197033.418663	36.575232
1495.841873	197409.606506	36.580250
1497.142958	197790.902715	36.585268
1498.837796	198160.430334	36.590285
1500.337131	198544.376905	36.595303
1501.725218	198924.014647	36.600320
1503.441697	199301.683112	36.605338
1505.074856	199671.203718	36.610356
1506.741644	200053.632908	36.615373
1507.973845	200433.876040	36.620391
1509.230948	200811.361984	36.625408
1510.805709	201188.822853	36.630426
1512.190801	201578.112209	36.635444
1513.784653	201955.700946	36.640461
1515.391721	202343.180239	36.645479
1516.728393	202733.461484	36.650496
1518.571068	203104.361959	36.655514
1519.724602	203502.981312	36.660532
1521.318026	203888.795030	36.665549
1522.788775	204271.583713	36.670567
1524.204385	204660.985968	36.675584
1525.781240	205047.303558	36.680602
1526.848194	205440.068682	36.685620
1528.592838	205831.923914	36.690637
1530.488769	206216.670989	36.695655
1531.677955	206602.349368	36.700672
1533.521355	206967.084926	36.705690
1535.034979	207337.654047	36.710708
1536.795388	207706.342963	36.715725
1538.325795	208072.519337	36.720743
1539.410243	208440.586828	36.725760
1541.030104	208812.364168	36.730778
1542.508909	209194.921590	36.735796
1543.966204	209560.227858	36.740813
1545.476114	209951.024578	36.745831
1546.708497	210339.938867	36.750848
1548.274706	210719.733348	36.755866
1549.914674	211102.666476	36.760884
1551.745157	211490.115794	36.765901
1553.390639	211886.765557	36.770919
1554.819514	212288.329063	36.775936
1556.219295	212666.483387	36.780954
1557.826846	213069.366943	36.785972
1559.391743	213467.357736	36.790989
1560.896190	213871.887321	36.796007
1562.364673	214266.976877	36.801024
1564.180922	214670.671158	36.806042
1565.773335	215070.721545	36.811060
1567.037245	215480.021817	36.816077
1568.756428	215885.235813	36.821095
1570.116515	216295.006255	36.826112
1571.870524	216702.783119	36.831130
1573.299880	217127.682758	36.836148
1574.979156	217538.878775	36.841165
1576.771206	217947.416450	36.846183
1578.199781	218367.445063	36.851200
1580.045729	218782.758554	36.856218
1581.322830	219202.968019	36.861236
1582.558864	219624.836878	36.866253
1584.530498	220036.553425	36.871271
1585.713142	220467.247823	36.876288
1587.460365	220889.900826	36.881306
1589.215686	221316.313190	36.886324
1590.805259	221751.161697	36.891341
1592.542960	222176.970724	36.896359
1593.940506	222604.412317	36.901376
1595.767540	223034.019713	36.906394
1597.410348	223467.088079	36.911412
1598.791616	223902.309429	36.916429
1600.746395	224337.463042	36.921447
1602.415129	224829.103774	36.926464
1603.820093	225264.986570	36.931482
1605.526748	225695.690287	36.936500
1606.972066	226125.422669	36.941517
1608.961306	226558.368678	36.946535
1610.185404	226999.977028	36.951552
1612.128441	227427.955161	36.956570
1613.760206	227863.403023	36.961588
1615.457747	228298.638240	36.966605
1617.060974	228725.482864	36.971623
1618.612462	229165.825095	36.976640
1620.370679	229592.138787	36.981658
1622.114344	230036.109711	36.986676
1623.370272	230464.693464	36.991693
1625.466208	230893.469929	36.996711
1626.783672	231329.844133	37.001728
1628.961004	231755.993336	37.006746
1630.530360	232184.276257	37.011764
1631.919080	232610.634310	37.016781
1633.604028	233044.285554	37.021799
1635.375381	233475.205756	37.026816
1637.255680	233900.596994	37.031834
1638.575026	234323.719653	37.036852
1640.474762	234732.827455	37.041869
1642.110221	235134.308606	37.046887
1643.456845	235552.070055	37.051904
1644.873470	235951.150662	37.056922
1646.615080	236369.458412	37.061940
1648.082808	236787.913964	37.066957
1649.750929	237192.290104	37.071975
1651.108629	237616.303274	37.076992
1652.634629	238033.862859	37.082010
1654.330677	238459.396878	37.087028
1655.638172	238884.538734	37.092045
1657.220510	239317.205903	37.097063
1658.574540	239757.049688	37.102080
1660.427717	240200.927078	37.107098
1662.169581	240640.581556	37.112116
1663.511632	241083.097185	37.117133
1665.165652	241527.746726	37.122151
1666.743488	241987.625745	37.127168
1668.516803	242448.235408	37.132186
1670.171976	242895.783113	37.137204
1671.800717	243363.759634	37.142221
1673.931061	243809.045772	37.147239
1675.568766	244287.107241	37.152256
1677.284729	244733.682621	37.157274
1678.892674	245196.889917	37.162292
1680.323036	245663.328001	37.167309
1682.261399	246130.444945	37.172327
1683.818906	246599.022621	37.177344
1685.545833	247073.110787	37.182362
1687.160695	247549.097913	37.187380
1688.898218	248020.950110	37.192397
1690.734762	248497.765512	37.197415
1692.309400	248975.767872	37.202432
1693.652291	249449.642949	37.207450
1695.606079	249928.676056	37.212468
1697.186593	250417.297468	37.217485
1698.903597	250908.157689	37.222503
1700.650203	251397.413075	37.227520
1702.829200	251875.572486	37.232538
1704.097367	252364.577460	37.237556
1705.929051	252857.020764	37.242573
1707.918587	253345.170593	37.247591
1709.572196	253827.330244	37.252608
1711.516757	254319.628810	37.257626
1713.231214	254800.635780	37.262644
1714.646511	255297.035954	37.267661
1716.667875	255781.574501	37.272679
1718.300569	256270.165721	37.277696
1720.359498	256757.289494	37.282714
1722.121524	257242.734987	37.287732
1723.665874	257735.558066	37.292749
1725.590771	258214.600554	37.297767
1727.191893	258715.238544	37.302784
1729.103745	259201.777174	37.307802
1731.011132	259683.058022	37.312820
1732.519485	260173.626113	37.317837
1734.600458	260659.399921	37.322855
1736.291177	261146.406618	37.327872
1737.641963	261640.074162	37.332890
1739.838489	262121.001816	37.337908
1741.274586	262610.183907	37.342925
1742.960069	263091.881422	37.347943
1744.548605	263591.249936	37.352960
1746.585534	264081.195703	37.357978
1748.245234	264565.944990	37.362996
1749.707819	265064.952267	37.368013
1751.525299	265546.677194	37.373031
1753.210553	266047.272688	37.378048
1754.698484	266526.434687	37.383066
1756.558445	266994.560662	37.388084
1758.137522	267475.459508	37.393101
1759.899969	267950.154629	37.398119
1761.491420	268429.932672	37.403136
1762.811664	268916.867784	37.408154
1764.788972	269398.155935	37.413172
1766.546645	269889.869535	37.418189
1768.376213	270380.884714	37.423207
1769.809293	270882.100411	37.428224
1771.616591	271379.087487	37.433242
1773.515137	271879.945341	37.438260
1774.730528	272391.787566	37.443277
1776.733233	272886.860127	37.448295
1778.274368	273399.612078	37.453312
1780.276379	273923.337078	37.458330
1781.850253	274440.120660	37.463348
1783.580769	274968.130629	37.468365
1785.317397	275488.466940	37.473383
1787.224530	276021.119518	37.478400
1788.831426	276545.361503	37.483418
1790.468593	277079.859784	37.488436
1792.619049	277616.354979	37.493453
1794.530872	278155.301444	37.498471
1796.184098	278700.334911	37.503488
1798.000923	279242.494874	37.508506
1799.893048	279776.385295	37.513524
1801.689035	280317.072404	37.518541
1803.479552	280864.109300	37.523559
1805.031321	281411.717428	37.528576
1806.939840	281965.818576	37.533594
1808.812470	282509.737883	37.538612
1810.679205	283083.223705	37.543629
1812.573133	283624.798966	37.548647
1813.950823	284190.893702	37.553664
1815.725388	284749.706952	37.558682
1818.028974	285311.377360	37.563700
1819.868323	285884.603617	37.568717
1821.379305	286443.657407	37.573735
1823.477927	287018.055700	37.578752
1825.302329	287590.591930	37.583770
1827.455453	288145.545142	37.588788
1828.999053	288721.780784	37.593805
1830.750404	289278.878587	37.598823
1833.117339	289853.144578	37.603840
1834.412686	290418.796555	37.608858
1836.779338	291000.321945	37.613876
1838.513765	291581.288658	37.618893
1840.574285	292150.387886	37.623911
1842.208226	292719.021504	37.628928
1843.993924	293293.443857	37.633946
1845.823639	293867.805337	37.638964
1847.683822	294452.115462	37.643981
1849.430239	295017.925377	37.648999
1851.550594	295601.881800	37.654016
1853.141490	296186.811526	37.659034
1855.015457	296760.719087	37.664052
1856.531358	297344.130990	37.669069
1858.688913	297922.252410	37.674087
1860.636826	298507.161189	37.679104
1862.399927	299092.833690	37.684122
1864.221620	299673.057929	37.689140
1866.092386	300252.584932	37.694157
1867.910947	300844.892198	37.699175
1869.887234	301435.645932	37.704192
1871.714989	302016.363145	37.709210
1873.934383	302600.186758	37.714228
1875.552633	303186.925045	37.719245
1877.513091	303751.761679	37.724263
1879.193524	304314.710867	37.729280
1881.034316	304876.360193	37.734298
1882.969316	305435.704702	37.739316
1884.887115	306006.679972	37.744333
1886.817151	306569.802027	37.749351
1888.551426	307139.098505	37.754368
1890.311522	307708.259886	37.759386
1892.245439	308275.864929	37.764404
1894.056804	308852.222320	37.769421
1895.808816	309432.496293	37.774439
1897.798558	310011.050740	37.779456
1899.187811	310596.175825	37.784474
1901.408416	311182.860715	37.789492
1903.027802	311781.321919	37.794509
1904.979509	312378.276105	37.799527
1906.678890	312975.495808	37.804544
1908.605113	313582.272195	37.809562
1910.499721	314181.100616	37.814580
1912.441653	314797.514020	37.819597
1914.419156	315401.575193	37.824615
1916.373954	316016.249329	37.829632
1917.974726	316644.663338	37.834650
1919.801030	317250.968323	37.839668
1921.963645	317887.530986	37.844685
1923.761981	318506.373416	37.849703
1925.814149	319142.764900	37.854720
1927.351815	319776.518420	37.859738
1929.517085	320410.543162	37.864756
1931.450831	321048.916541	37.869773
1933.626203	321687.624649	37.874791
1935.683926	322325.558764	37.879808
1937.178092	322982.698555	37.884826
1939.739456	323622.339239	37.889844
1941.252902	324263.492094	37.894861
1943.081374	324914.056648	37.899879
1945.504794	325568.375269	37.904896
1947.455229	326206.236666	37.909914
1949.635502	326861.444705	37.914932
1951.453212	327513.049477	37.919949
1953.252322	328159.115509	37.924967
1955.540245	328814.538038	37.929984
1957.138089	329474.509955	37.935002
1959.203299	330125.841589	37.940020
1961.238906	330779.760156	37.945037
1963.115288	331450.478116	37.950055
1965.029960	332104.858207	37.955072
1966.859998	332774.679358	37.960090
1968.983369	333425.632980	37.965108
1971.037009	334097.812682	37.970125
1972.755774	334766.637686	37.975143
1974.846610	335435.849834	37.980160
1976.607393	336111.454191	37.985178
1978.569030	336786.331335	37.990196
1980.808727	337449.705672	37.995213
1982.857771	338116.352082	38.000231
1985.057068	338789.970808	38.005248
1986.804562	339464.467460	38.010266
1988.908603	340137.627091	38.015284
1990.778265	340817.872630	38.020301
1992.849481	341490.714803	38.025319
1994.968209	342161.585545	38.030336
1996.663726	342847.263428	38.035354
1998.876083	343519.775120	38.040372
2000.849299	344198.458956	38.045389
2002.912930	344883.285568	38.050407
2004.918681	345549.330774	38.055424
2006.610029	346218.616232	38.060442
2008.580549	346870.258286	38.065460
2010.835855	347523.366847	38.070477
2012.884370	348181.144479	38.075495
2014.784936	348826.171906	38.080512
2016.759245	349488.003303	38.085530
2018.821047	350129.990868	38.090548
2020.843412	350806.437465	38.095565
2022.820870	351461.945537	38.100583
2024.792007	352122.317071	38.105600
2026.547758	352789.362590	38.110618
2028.341651	353452.331479	38.115636
2030.457728	354130.055896	38.120653
2032.655949	354807.679860	38.125671
2034.752532	355475.413862	38.130688
2036.737532	356167.209944	38.135706
2039.030575	356837.909270	38.140724
2040.963931	357517.080919	38.145741
2043.006446	358213.907934	38.150759
2045.166965	358893.602867	38.155776
2047.448223	359576.006622	38.160794
2049.564103	360262.663117	38.165812
2051.453646	360949.370581	38.170829
2053.348575	361641.443804	38.175847
2055.656885	362327.804566	38.180864
2057.655998	363037.873998	38.185882
2059.776951	363728.807599	38.190900
2061.773176	364426.801900	38.195917
2063.760818	365135.185833	38.200935
2065.982281	365837.480570	38.205952
2068.000672	366547.253753	38.210970
2069.971180	367248.726618	38.215988
2072.317055	367955.730294	38.221005
2074.236507	368667.407479	38.226023
2076.409692	369377.887655	38.231040
2078.424003	370100.073414	38.236058
2080.610862	370812.552676	38.241076
2082.867739	371529.622564	38.246093
2084.596219	372247.399494	38.251111
2086.996821	372956.351714	38.256128
2089.003366	373670.782352	38.261146
2091.384085	374405.299245	38.266164
2093.835924	375123.456534	38.271181
2095.534352	375849.534467	38.276199
2098.152211	376556.425440	38.281216
2100.096898	377284.740368	38.286234
2102.228842	377999.670117	38.291252
2104.481121	378718.470197	38.296269
2106.505311	379441.882448	38.301287
2108.746072	380153.376183	38.306304
2111.076266	380878.507331	38.311322
2112.997471	381603.943749	38.316340
2115.312366	382320.069808	38.321357
2117.014985	383038.157617	38.326375
2119.482579	383762.416659	38.331392
2121.264110	384482.259800	38.336410
2123.375670	385202.285961	38.341428
2125.688229	385927.891137	38.346445
2127.454017	386665.587053	38.351463
2129.828488	387390.464174	38.356480
2131.657770	388117.746945	38.361498
2133.732246	388854.326730	38.366516
2136.307190	389581.198913	38.371533
2138.366161	390320.788544	38.376551
2140.840145	391048.910386	38.381568
2142.644994	391786.402806	38.386586
2144.784211	392516.040542	38.391604
2147.093352	393247.330930	38.396621
2148.874526	393969.540753	38.401639
2151.341034	394675.449555	38.406656
2153.085909	395388.126536	38.411674
2155.402387	396099.399507	38.416692
2157.745157	396794.811117	38.421709
2159.230289	397507.429188	38.426727
2161.659353	398206.467850	38.431744
2163.763340	398917.910278	38.436762
2165.684496	399639.577979	38.441780
2167.753403	400361.456621	38.446797
2169.723187	401087.666597	38.451815
2171.848228	401810.639678	38.456832
2174.006981	402545.928761	38.461850
2176.557007	403279.689827	38.466868
2178.784760	404023.265166	38.471885
2180.349690	404768.247622	38.476903
2182.243902	405500.107663	38.481920
2184.655753	406262.645432	38.486938
2186.681960	407008.327452	38.491956
2188.697974	407763.364422	38.496973
2190.763301	408545.706946	38.501991
2193.084471	409315.470351	38.507008
2195.065159	410091.626246	38.512026
2197.411616	410869.092501	38.517044
2199.703335	411657.158535	38.522061
2201.910586	412441.795594	38.527079
2204.100245	413225.348408	38.532096
2206.188743	414009.907650	38.537114
2208.541370	414812.280812	38.542132
2210.766218	415592.717498	38.547149
2212.770397	416400.873426	38.552167
2215.418860	417186.991521	38.557184
2217.719679	418003.227959	38.562202
2219.680564	418803.287373	38.567220
2222.306716	419599.261387	38.572237
2224.109268	420417.401432	38.577255
2226.521120	421231.818642	38.582272
2228.893094	422040.696052	38.587290
2231.264931	422854.535009	38.592308
2233.645808	423663.636415	38.597325
2235.334417	424488.826140	38.602343
2238.054526	425296.501119	38.607360
2240.116597	426119.548674	38.612378
2242.080862	426941.875558	38.617396
2244.606814	427754.006621	38.622413
2247.192216	428585.743462	38.627431
2249.441265	429406.622460	38.632448
2251.562521	430230.582153	38.637466
2253.290902	431067.283873	38.642484
2256.365051	431895.027146	38.647501
2258.359126	432717.452647	38.652519
2260.890205	433555.451378	38.657536
2263.273095	434378.766157	38.662554
2265.505832	435208.149769	38.667572
2267.720188	436029.712415	38.672589
2269.696838	436878.259085	38.677607
2272.060383	437704.949341	38.682624
2274.652399	438523.474884	38.687642
2276.594510	439373.755369	38.692660
2278.836898	440193.896995	38.697677
2281.501555	441038.479366	38.702695
2283.614575	441874.468491	38.707712
2285.603655	442716.062506	38.712730
2288.025977	443550.773289	38.717748
2290.776760	444383.526136	38.722765
2292.658808	445223.978930	38.727783
2295.199758	446063.835122	38.732800
2297.613499	446904.387816	38.737818
2299.649987	447725.444602	38.742836
2302.166216	448531.570260	38.747853
2304.653007	449343.234032	38.752871
2306.643032	450148.424164	38.757888
2309.237557	450936.237427	38.762906
2311.043118	451743.824669	38.767924
2313.639718	452554.587975	38.772941
2315.832740	453366.195461	38.777959
2317.859551	454183.613970	38.782976
2319.868376	454996.553301	38.787994
2321.779959	455826.921177	38.793012
2324.170363	456649.996583	38.798029
2326.670358	457490.918927	38.803047
2328.839558	458314.064677	38.808064
2330.732247	459172.712724	38.813082
2332.785920	460025.837818	38.818100
2335.289637	460884.514116	38.823117
2337.731127	461745.994509	38.828135
2340.027897	462620.654226	38.833152
2342.573389	463480.070809	38.838170
2344.586352	464356.924436	38.843188
2347.267633	465229.130513	38.848205
2349.162675	466111.029615	38.853223
2351.708247	466990.911571	38.858240
2353.908306	467884.454588	38.863258
2356.421526	468769.415308	38.868276
2358.731863	469659.724760	38.873293
2361.082550	470564.840839	38.878311
2363.429240	471471.228157	38.883328
2366.271551	472371.781409	38.888346
2368.622870	473292.984473	38.893364
2370.941894	474183.585146	38.898381
2373.846875	475094.606011	38.903399
2375.881603	475997.694543	38.908416
2378.218101	476910.892176	38.913434
2380.621362	477836.912845	38.918452
2383.195029	478747.202461	38.923469
2385.442757	479654.015979	38.928487
2387.857659	480569.897154	38.933504
2390.302694	481495.371994	38.938522
2392.638820	482418.292720	38.943540
2395.198467	483333.050616	38.948557
2397.362759	484257.066511	38.953575
2400.112845	485189.924453	38.958592
2402.524798	486123.495987	38.963610
2404.521180	487048.050771	38.968628
2407.283109	487983.434987	38.973645
2409.782890	488922.194453	38.978663
2412.114521	489861.234072	38.983680
2414.588107	490783.998712	38.988698
2417.043532	491733.061172	38.993716
2419.465068	492663.304220	38.998733
2421.766655	493607.847870	39.003751
2424.270328	494551.195958	39.008768
2426.644387	495485.128365	39.013786
2429.044084	496437.420670	39.018804
2432.033523	497372.862885	39.023821
2434.124754	498324.746405	39.028839
2436.479389	499257.161587	39.033856
2438.928655	500211.854953	39.038874
2441.085097	501155.445218	39.043892
2443.718607	502104.198844	39.048909
2446.209552	503055.695272	39.053927
2448.651694	504010.473072	39.058944
2451.308856	504956.334883	39.063962
2453.752837	505902.328259	39.068980
2456.403741	506844.400335	39.073997
2459.029382	507800.387688	39.079015
2461.261412	508734.906149	39.084032
2463.596823	509650.297077	39.089050
2466.388494	510570.601313	39.094068
2468.685652	511484.683473	39.099085
2470.730067	512394.671935	39.104103
2473.124756	513309.892762	39.109120
2475.582888	514240.774205	39.114138
2477.616451	515174.996550	39.119156
2480.083225	516101.180005	39.124173
2482.765960	517018.706559	39.129191
2485.142539	517976.135271	39.134208
2487.789586	518915.674817	39.139226
2489.588676	519857.513645	39.144244
2492.216349	520796.437600	39.149261
2494.619753	521761.434495	39.154279
2496.631687	522720.994786	39.159296
2499.642815	523697.404066	39.164314
2501.757401	524669.163919	39.169332
2504.062870	525657.498973	39.174349
2506.628559	526659.876388	39.179367
2508.861308	527643.560098	39.184384
2511.362630	528633.982167	39.189402
2513.601300	529648.346704	39.194420
2516.072911	530659.481806	39.199437
2518.654237	531675.966044	39.204455
2521.226851	532692.129500	39.209472
2524.083322	533705.205698	39.214490
2526.076963	534747.192589	39.219508
2528.890128	535778.602128	39.224525
2531.108673	536811.495351	39.229543
2533.757411	537853.149796	39.234560
2536.433293	538895.227095	39.239578
2538.858185	539944.011361	39.244596
2541.692912	540997.781951	39.249613
2544.065441	542058.844353	39.254631
2546.623092	543117.130402	39.259648
2549.152063	544171.166779	39.264666
2551.922074	545239.769357	39.269684
2554.499068	546303.343189	39.274701
2557.119199	547372.108264	39.279719
2559.722791	548444.313066	39.284736
2562.658217	549510.346363	39.289754
2565.167683	550580.841341	39.294772
2568.092855	551650.781692	39.299789
2571.001804	552725.315235	39.304807
2573.375902	553783.114832	39.309824
2575.988012	554852.502247	39.314842
2578.830561	555928.450315	39.319860
2581.283459	557000.758323	39.324877
2584.004411	558065.248475	39.329895
2586.436231	559134.172580	39.334912
2589.489247	560197.180958	39.339930
2591.939034	561263.518614	39.344948
2594.599984	562339.077566	39.349965
2597.400918	563403.224555	39.354983
2599.723591	564465.857066	39.360000
2602.710498	565531.004898	39.365018
2605.370155	566604.504637	39.370036
2607.764884	567665.959040	39.375053
2610.718836	568732.555265	39.380071
2612.986853	569795.912878	39.385088
2615.653052	570865.842520	39.390106
2618.419612	571940.182889	39.395124
2620.896056	573003.338500	39.400141
2623.468427	574070.002009	39.405159
2626.075025	575147.608828	39.410176
2628.991787	576212.227246	39.415194
2631.570827	577285.740978	39.420212
2634.066437	578338.908919	39.425229
2636.458730	579377.708448	39.430247
2639.308166	580419.906515	39.435264
2641.615006	581454.783572	39.440282
2644.092646	582491.250348	39.445300
2646.736568	583531.463096	39.450317
2649.543097	584567.549093	39.455335
2651.577796	585603.674108	39.460352
2654.133572	586658.875254	39.465370
2656.458814	587718.182811	39.470388
2659.231396	588788.701286	39.475405
2661.761667	589856.207184	39.480423
2664.272662	590934.846470	39.485440
2666.933651	592011.308861	39.490458
2669.648512	593101.393491	39.495476
2672.137654	594190.212496	39.500493
2675.228832	595278.681359	39.505511
2677.653336	596384.390600	39.510528
2680.443960	597477.263230	39.515546
2682.856592	598585.721249	39.520564
2685.345136	599697.916978	39.525581
2687.997744	600821.345190	39.530599
2690.671574	601948.215336	39.535616
2693.349489	603074.824252	39.540634
2696.008304	604205.980914	39.545652
2698.483563	605356.726301	39.550669
2701.332932	606494.281468	39.555687
2704.078996	607652.256778	39.560704
2706.988353	608791.222674	39.565722
2709.412477	609961.423224	39.570740
2712.503693	611107.679236	39.575757
2715.165453	612276.698309	39.580775
2718.115506	613442.946391	39.585792
2720.729110	614608.577372	39.590810
2723.260471	615785.550400	39.595828
2725.879661	616960.083335	39.600845
2729.122562	618136.787621	39.605863
2731.624206	619315.437280	39.610880
2734.362374	620493.570741	39.615898
2737.410080	621678.972302	39.620916
2739.776413	622864.556436	39.625933
2742.934248	624054.576814	39.630951
2745.629778	625247.589482	39.635968
2748.808961	626426.251982	39.640986
2751.803706	627624.645358	39.646004
2754.211107	628809.115932	39.651021
2757.089114	629992.377889	39.656039
2759.956744	631199.577344	39.661056
2762.948341	632369.421436	39.666074
2765.682739	633565.387076	39.671092
2768.378983	634762.969427	39.676109
2771.762762	635955.509391	39.681127
2774.316918	637149.097329	39.686144
2776.798991	638340.863021	39.691162
2779.881939	639525.257188	39.696180
2782.375572	640714.451333	39.701197
2785.382033	641907.712879	39.706215
2788.103906	643105.919537	39.711232
2791.200250	644293.650081	39.716250
2794.098297	645493.640817	39.721268
2796.609828	646680.190716	39.726285
2799.791306	647887.877473	39.731303
2802.008650	649081.620858	39.736320
2804.626121	650276.501687	39.741338
2807.633840	651476.158632	39.746356
2810.401106	652674.514639	39.751373
2813.224270	653879.143761	39.756391
2815.667245	655092.307056	39.761408
2818.786781	656275.820926	39.766426
2821.486855	657447.208449	39.771444
2823.905847	658624.926161	39.776461
2826.760329	659795.409044	39.781479
2829.411165	660959.561198	39.786496
2832.552874	662122.994753	39.791514
2835.150713	663304.346641	39.796532
2837.558761	664493.398610	39.801549
2840.692301	665674.719261	39.806567
2842.983040	666866.083833	39.811584
2845.661772	668057.335123	39.816602
2848.495072	669273.681588	39.821620
2851.130934	670484.632296	39.826637
2853.819327	671696.911028	39.831655
2856.287872	672927.666944	39.836672
2859.285599	674159.516582	39.841690
2861.849962	675411.160023	39.846708
2864.570132	676655.203724	39.851725
2867.585092	677904.598446	39.856743
2870.066592	679180.944637	39.861760
2873.330549	680448.389936	39.866778
2876.074695	681719.819862	39.871796
2878.737114	683003.653621	39.876813
2881.834743	684280.282358	39.881831
2884.347055	685583.146631	39.886848
2887.198938	686880.703690	39.891866
2890.415828	688193.701394	39.896884
2893.647960	689509.384182	39.901901
2896.360664	690813.595213	39.906919
2898.956115	692131.578981	39.911936
2901.827147	693444.014095	39.916954
2904.936136	694767.824065	39.921972
2908.178769	696093.844617	39.926989
2910.936954	697438.937628	39.932007
2913.631275	698772.431568	39.937024
2916.557665	700114.062889	39.942042
2920.193424	701450.265926	39.947060
2922.711735	702790.958312	39.952077
2926.039711	704127.891157	39.957095
2929.070518	705476.606866	39.962112
2931.823310	706825.108041	39.967130
2935.140861	708165.875213	39.972148
2937.755418	709518.285156	39.977165
2941.025829	710856.508965	39.982183
2944.066524	712209.016033	39.987200
2947.087624	713559.825778	39.992218
2950.266704	714915.491180	39.997236
2953.075478	716268.129587	40.002253
2956.401722	717613.340571	40.007271
2959.126813	718969.069754	40.012288
2962.080809	720326.469808	40.017306
2965.331363	721665.896255	40.022324
2968.373322	723019.874419	40.027341
2971.644433	724375.026499	40.032359
2974.242841	725727.348036	40.037376
2977.483127	727079.093876	40.042394
2980.453906	728422.162335	40.047412
2983.353859	729768.528769	40.052429
2986.851404	731116.351828	40.057447
2989.436930	732481.731425	40.062464
2992.320868	733819.723215	40.067482
2995.772332	735157.991467	40.072500
2998.468783	736520.347444	40.077517
3001.450107	737868.063053	40.082535
3004.492835	739222.448780	40.087552
3007.556694	740574.182769	40.092570
3010.501518	741922.795437	40.097588
3013.260157	743294.141356	40.102605
3016.170946	744630.361449	40.107623
3019.086142	745961.965431	40.112640
3021.577800	747280.744254	40.117658
3024.850702	748591.679994	40.122676
3027.771767	749915.855759	40.127693
3030.541806	751236.923342	40.132711
3033.508383	752566.944114	40.137728
3036.197344	753909.339890	40.142746
3039.140726	755234.421243	40.147764
3041.832843	756597.913690	40.152781
3044.935748	757952.578909	40.157799
3048.082481	759316.691139	40.162816
3050.709900	760686.056305	40.167834
3053.842464	762054.155361	40.172852
3056.762315	763441.077192	40.177869
3059.940047	764832.323308	40.182887
3062.870244	766219.565545	40.187904
3065.298096	767622.020272	40.192922
3068.339573	769032.661961	40.197940
3071.410380	770457.822415	40.202957
3074.941350	771871.822932	40.207975
3077.637214	773297.725024	40.212992
3080.563156	774745.413701	40.218010
3083.616565	776180.518998	40.223028
3086.680291	777640.427680	40.228045
3089.969828	779084.740744	40.233063
3093.667558	780547.641661	40.238080
3096.455573	782005.293561	40.243098
3099.658329	783465.427285	40.248116
3102.393143	784939.858441	40.253133
3105.885796	786404.838476	40.258151
3108.788451	787883.047573	40.263168
3112.264289	789375.412086	40.268186
3115.174025	790836.633962	40.273204
3118.431630	792329.881170	40.278221
3121.644334	793809.348546	40.283239
3124.850305	795299.475041	40.288256
3128.149663	796792.304306	40.293274
3131.502170	798281.819007	40.298292
3134.368066	799781.910658	40.303309
3137.538952	801281.822834	40.308327
3141.176966	802783.093211	40.313344
3144.037988	804288.663708	40.318362
3147.320120	805796.377004	40.323380
3150.617204	807303.364142	40.328397
3153.341985	808811.138674	40.333415
3156.863500	810320.841585	40.338432
3160.026939	811830.364465	40.343450
3163.229528	813338.273186	40.348468
3166.419067	814857.956625	40.353485
3169.848804	816369.053777	40.358503
3173.336794	817886.047387	40.363520
3176.132930	819392.268608	40.368538
3179.389149	820899.291989	40.373556
3182.160693	822414.051600	40.378573
3185.727817	823934.671907	40.383591
3189.317285	825449.573698	40.388608
3192.128508	826968.348033	40.393626
3195.772776	828476.641757	40.398644
3198.676673	829997.424397	40.403661
3202.204130	831514.143421	40.408679
3205.571563	833025.225086	40.413696
3208.433549	834539.930969	40.418714
3211.867582	836053.844993	40.423732
3214.983727	837575.142689	40.428749
3218.560842	839091.866670	40.433767
3221.464249	840605.811069	40.438784
3224.556816	842124.177554	40.443802
3227.728310	843629.817814	40.448820
3230.811587	845119.559260	40.453837
3233.592878	846584.700157	40.458855
3236.894967	848070.206578	40.463872
3239.707287	849555.926360	40.468890
3243.263960	851030.874474	40.473908
3246.088686	852524.721168	40.478925
3249.153126	854001.762562	40.483943
3252.202662	855508.344646	40.488960
3255.172034	857027.475714	40.493978
3258.203616	858533.513144	40.498996
3261.102509	860061.700665	40.504013
3264.327270	861599.146935	40.509031
3267.629455	863142.782800	40.514048
3270.457535	864688.138579	40.519066
3273.441222	866252.061789	40.524084
3276.997326	867829.334642	40.529101
3279.948530	869408.229274	40.534119
3283.168847	871003.990619	40.539136
3286.369244	872594.586249	40.544154
3289.381161	874193.204690	40.549172
3292.905540	875820.905053	40.554189
3295.602711	877439.590408	40.559207
3298.980628	879066.805647	40.564224
3302.389933	880721.494480	40.569242
3305.152370	882363.744776	40.574260
3308.238270	884021.319746	40.579277
3312.027358	885689.024266	40.584295
3315.167575	887360.313262	40.589312
3318.216839	889042.231393	40.594330
3321.774232	890719.907963	40.599348
3325.303873	892421.885347	40.604365
3328.406363	894121.594202	40.609383
3331.712067	895815.075269	40.614400
3334.990388	897529.351471	40.619418
3338.597334	899235.636448	40.624436
3341.927615	900951.273471	40.629453
3345.153669	902665.729901	40.634471
3348.756130	904387.106437	40.639488
3351.875409	906110.244546	40.644506
3355.600987	907841.790252	40.649524
3359.008614	909577.462816	40.654541
3362.482239	911305.466039	40.659559
3366.273057	913035.084804	40.664576
3369.648932	914777.003097	40.669594
3373.119435	916500.777015	40.674612
3376.648627	918236.764355	40.679629
3379.645054	919969.693443	40.684647
3383.369217	921703.099246	40.689664
3386.588093	923441.306417	40.694682
3389.983980	925183.141239	40.699700
3393.721447	926919.369617	40.704717
3397.035846	928658.265238	40.709735
3400.468487	930407.109706	40.714752
3403.942769	932144.167753	40.719770
3407.473648	933879.688639	40.724788
3411.078608	935624.003424	40.729805
3414.454465	937367.968006	40.734823
3417.791343	939098.161625	40.739840
3421.425106	940844.939646	40.744858
3424.714777	942575.610944	40.749876
3428.150974	944316.093081	40.754893
3431.524680	946055.617148	40.759911
3435.269788	947794.015031	40.764928
3438.337137	949528.786379	40.769946
3441.796949	951271.586268	40.774964
3444.981629	953031.230913	40.779981
3448.299826	954822.053419	40.784999
3452.346282	956580.765591	40.790004
3455.161046	958310.457188	40.795008
3458.339644	959977.151687	40.800013
3461.383222	961580.299625	40.805018
3464.482959	963124.622994	40.810023
3467.553489	964595.692177	40.815028
3470.367082	965988.902023	40.820032
3473.562404	967308.705379	40.825037
3476.137092	968557.274523	40.830042
3478.590764	969740.931906	40.835047
3481.569870	970843.571333	40.840052
3483.545773	971883.972649	40.845056
3485.935211	972845.902220	40.850061
3488.349667	973738.945568	40.855066
3490.294138	974574.847400	40.860071
3492.542964	975336.598503	40.865076
3494.329553	976048.392480	40.870080
3496.252181	976687.775386	40.875085
3498.225050	977277.548191	40.880090
3499.477190	977805.349667	40.885095
3501.661534	978276.101539	40.890100
3503.022897	978716.575280	40.895104
3504.344501	979094.420459	40.900109
3505.703823	979431.804790	40.905114
3506.839687	979713.935446	40.910119
3508.238225	979961.539463	40.915124
3508.969411	980171.454654	40.920128
3510.329080	980333.512343	40.925133
3511.247007	980473.278998	40.930138
3512.022096	980581.724451	40.935143
3512.955029	980652.357016	40.940148
3513.738918	980703.681631	40.945152
3514.585890	980723.166696	40.950157
3515.023975	980710.109215	40.955162
3515.560307	980687.760211	40.960167
3516.308577	980622.123611	40.965172
3516.986097	980553.861711	40.970176
3517.635269	980446.841108	40.975181
3518.103495	980324.713959	40.980186
3518.780416	980193.957213	40.985191
3519.205928	980033.261622	40.990196
3519.218566	979874.484856	40.995200
3520.278233	979686.138007	41.000205
3520.434492	979483.969064	41.005210
3520.848258	979266.222753	41.010215
3521.260465	979027.959151	41.015220
3521.442827	978794.411510	41.020224
3521.695889	978532.517940	41.025229
3522.261087	978269.681863	41.030234
3522.018552	977997.101003	41.035239
3522.211354	977708.512654	41.040244
3522.368385	977425.093235	41.045248
3522.312233	977129.971412	41.050253
3522.635759	976829.300559	41.055258
3522.998862	976518.348242	41.060263
3523.515341	976201.197930	41.065268
3523.443620	975882.270314	41.070272
3523.598075	975540.322825	41.075277
3523.734976	975205.687441	41.080282
3523.681554	974871.454777	41.085287
3523.983084	974508.994928	41.090292
3524.227883	974165.484300	41.095296
3524.056189	973802.568950	41.100301
3524.359642	973441.116459	41.105306
3524.043379	973076.614770	41.110311
3524.411302	972712.270480	41.115316
3524.272145	972340.262139	41.120320
3524.496022	971965.040751	41.125325
3524.615325	971593.332475	41.130330
3524.241149	971216.889352	41.135335
3524.405329	970826.542559	41.140340
3524.303385	970453.720993	41.145344
3524.299876	970064.132401	41.150349
3524.574381	969675.938889	41.155354
3524.099304	969287.646936	41.160359
3524.160204	968895.913966	41.165364
3524.145831	968523.441681	41.170368
3524.189789	968133.518473	41.175373
3524.184727	967744.653269	41.180378
3523.986570	967358.435823	41.185383
3524.095045	966949.534088	41.190388
3523.858119	966569.435733	41.195392
3524.073243	966170.542187	41.200397
3523.896917	965794.395756	41.205402
3524.213574	965404.438098	41.210407
3524.379477	965007.234041	41.215412
3524.067689	964605.577408	41.220416
3523.721604	964212.417060	41.225421
3524.213145	963817.329227	41.230426
3523.803150	963423.929654	41.235431
3523.998672	963017.475827	41.240436
3523.591887	962625.098392	41.245440
3523.841559	962222.889017	41.250445
3523.790273	961833.141616	41.255450
3523.566023	961444.963731	41.260455
3523.456690	961045.768117	41.265460
3523.445281	960648.880139	41.270464
3523.432920	960253.434721	41.275469
3523.617937	959855.381898	41.280474
3523.218079	959466.903630	41.285479
3523.377654	959074.386869	41.290484
3522.942021	958686.841941	41.295488
3522.957621	958276.162658	41.300493
3522.493787	957893.763955	41.305498
3522.632618	957514.377567	41.310503
3523.084912	957126.777559	41.315508
3523.212685	956731.459567	41.320512
3522.566515	956340.654241	41.325517
3522.547019	955948.836691	41.330522
3522.284662	955568.407879	41.335527
3522.690657	955180.684810	41.340532
3522.430146	954807.266550	41.345536
3522.354003	954417.610163	41.350541
3522.228085	954030.486008	41.355546
3521.979772	953655.912315	41.360551
3522.304970	953270.330536	41.365556
3521.733302	952900.666254	41.370560
3521.696299	952517.078639	41.375565
3522.043392	952159.767462	41.380570
3521.673549	951783.039782	41.385575
3521.374231	951412.871927	41.390580
3521.191617	951058.057437	41.395584
3521.365349	950699.333342	41.400589
3521.336307	950352.383888	41.405594
3520.849968	949985.491448	41.410599
3520.975978	949624.882055	41.415604
3521.108085	949281.181989	41.420608
3520.884453	948920.867632	41.425613
3520.552068	948563.225312	41.430618
3520.910630	948216.641341	41.435623
3520.812129	947862.835412	41.440628
3520.533478	947511.044786	41.445632
3520.607584	947144.430791	41.450637
3520.612134	946807.382200	41.455642
3520.308713	946456.193534	41.460647
3520.172721	946102.655523	41.465652
3519.994776	945762.026095	41.470656
3520.032610	945415.401850	41.475661
3520.315055	945073.023229	41.480666
3520.008817	944734.932612	41.485671
3519.934918	944395.823844	41.490676
3519.928025	944057.160674	41.495680
3519.674233	943714.780356	41.500685
3519.550216	943375.133958	41.505690
3519.484869	943031.240486	41.510695
3519.581563	942693.812197	41.515700
3519.086125	942371.789184	41.520704
3519.240707	942031.625569	41.525709
3519.466365	941709.921759	41.530714
3518.975139	941378.254113	41.535719
3519.151221	941050.288748	41.540724
3518.978905	940719.772391	41.545728
3518.776402	940389.240008	41.550733
3518.980784	940054.018654	41.555738
3518.883040	939738.955927	41.560743
3518.746283	939399.339147	41.565748
3518.581051	939087.507589	41.570752
3518.743894	938760.646567	41.575757
3518.561713	938435.931355	41.580762
3518.500833	938127.764724	41.585767
3518.598713	937796.059643	41.590772
3518.476807	937477.412222	41.595776
3517.888168	937156.424636	41.600781
3517.585824	936839.590342	41.605786
3517.743031	936535.322337	41.610791
3518.020399	936217.299840	41.615796
3518.026601	935912.732840	41.620800
3517.730870	935597.645093	41.625805
3517.909724	935295.220344	41.630810
3517.357424	934986.182437	41.635815
3517.670967	934678.710853	41.640820
3517.492075	934381.377936	41.645824
3517.480907	934059.338190	41.650829
3517.331037	933751.696908	41.655834
3516.969058	933461.827795	41.660839
3517.621544	933161.409877	41.665844
3517.277899	932859.123300	41.670848
3517.183709	932556.010399	41.675853
3517.036353	932255.672746	41.680858
3516.823149	931965.888995	41.685863
3516.534731	931671.109434	41.690868
3516.520717	931381.164840	41.695872
3516.553054	931089.948520	41.700877
3516.514649	930801.992604	41.705882
3516.294236	930523.461698	41.710887
3516.275653	930224.428032	41.715892
3516.275774	929951.304613	41.720896
3516.227627	929660.791403	41.725901
3516.429177	929381.170629	41.730906
3516.028364	929098.848858	41.735911
3516.101810	928812.015300	41.740916
3515.542958	928543.330304	41.745920
3515.550848	928254.844460	41.750925
3515.928916	927990.780641	41.755930
3515.433590	927726.175093	41.760935
3515.606339	927442.806339	41.765940
3515.422682	927169.378293	41.770944
3515.377052	926894.664301	41.775949
3515.379637	926627.616036	41.780954
3514.922148	926362.552266	41.785959
3515.271878	926094.363054	41.790964
3515.245255	925831.700777	41.795968
3514.900178	925576.382915	41.800973
3515.330850	925311.697471	41.805978
3514.982694	925048.953658	41.810983
3514.915364	924776.729911	41.815988
3514.881424	924520.253041	41.820992
3514.497096	924260.360606	41.825997
3514.617253	923997.199709	41.831002
3514.216292	923752.380100	41.836007
3514.463709	923482.346450	41.841012
3514.469653	923230.801441	41.846016
3514.488901	922981.646550	41.851021
3514.354099	922713.945215	41.856026
3514.156005	922470.572526	41.861031
3514.251755	922212.040755	41.866036
3514.268045	921982.075374	41.871040
3514.095913	921731.066753	41.876045
3513.972413	921480.230822	41.881050
3513.974315	921238.404800	41.886055
3513.930733	920981.183729	41.891060
3513.749896	920745.330038	41.896064
3513.595734	920492.914073	41.901069
3513.952563	920250.889193	41.906074
3513.519964	920005.327352	41.911079
3513.684447	919768.796904	41.916084
3513.695767	919541.133974	41.921088
3513.570008	919297.317735	41.926093
3513.692740	919061.629359	41.931098
3513.643767	918824.996666	41.936103
3513.327171	918582.430806	41.941108
3512.757463	918354.428822	41.946112
3512.966513	918121.284009	41.951117
3512.984060	917880.267973	41.956122
3512.869181	917669.969182	41.961127
3513.420060	917437.508799	41.966132
3513.184326	917212.291714	41.971136
3512.982782	916974.159587	41.976141
3512.853154	916744.380999	41.981146
3512.754432	916522.674937	41.986151
3512.692425	916288.148376	41.991156
3512.869142	916075.236641	41.996160
3512.351234	915852.416962	42.001165
3512.486763	915628.710184	42.006170
3512.307493	915414.675812	42.011175
3512.635869	915190.919337	42.016180
3512.469311	914976.576806	42.021184
3512.137854	914750.984936	42.026189
3511.818886	914537.517078	42.031194
3511.991551	914332.050449	42.036199
3512.449426	914116.319231	42.041204
3511.850869	913901.331505	42.046208
3512.017126	913688.906504	42.051213
3512.076606	913477.165181	42.056218
3511.651506	913283.991762	42.061223
3511.782000	913062.685618	42.066228
3511.621786	912869.453962	42.071232
3511.454410	912658.970878	42.076237
3511.571087	912448.143883	42.081242
3511.717596	912253.876545	42.086247
3511.413317	912038.092837	42.091252
3511.779563	911845.509285	42.096256
3511.504330	911641.268371	42.101261
3511.793950	911441.263324	42.106266
3511.615285	911236.124165	42.111271
3511.646418	911031.713792	42.116276
3511.315726	910825.235140	42.121280
3511.104295	910618.439959	42.126285
3511.062822	910425.681178	42.131290
3510.915587	910239.583846	42.136295
3510.876947	910036.979457	42.141300
3510.843340	909857.790701	42.146304
3511.003868	909656.007071	42.151309
3511.581229	909463.787542	42.156314
3511.019923	909271.459711	42.161319
3510.821504	909080.897151	42.166324
3510.795704	908891.842167	42.171328
3510.681371	908691.514790	42.176333
3510.769822	908495.678411	42.181338
3510.095058	908318.088074	42.186343
3510.417271	908136.663662	42.191348
3510.342262	907954.527332	42.196352
3510.052613	907769.527455	42.201357
3510.608842	907586.117860	42.206362
3510.089428	907411.365882	42.211367
3510.306539	907220.574419	42.216372
3510.305100	907044.278938	42.221376
3510.165040	906867.904252	42.226381
3510.553463	906680.923888	42.231386
3509.786229	906522.870540	42.236391
3510.434707	906334.967626	42.241396
3510.290011	906161.368496	42.246400
3510.269109	905984.174466	42.251405
3510.253841	905792.889975	42.256410
3510.219307	905631.121350	42.261415
3509.836715	905444.805275	42.266420
3509.651209	905277.166496	42.271424
3509.517058	905107.198763	42.276429
3510.114773	904925.624148	42.281434
3509.607750	904772.302196	42.286439
3509.815130	904593.965026	42.291444
3509.670636	904425.618483	42.296448
3509.669301	904261.585402	42.301453
3509.558054	904089.267079	42.306458
3509.559813	903923.486654	42.311463
3509.724743	903755.551420	42.316468
3509.572523	903593.357082	42.321472
3509.425399	903425.077318	42.326477
3509.625385	903265.131579	42.331482
3509.455778	903103.794484	42.336487
3509.360473	902933.464649	42.341492
3509.361088	902767.457113	42.346496
3509.411644	902601.919031	42.351501
3509.418973	902446.325051	42.356506
3509.038121	902299.864105	42.361511
3509.081689	902127.266786	42.366516
3509.135274	901976.092439	42.371520
3508.793576	901810.499073	42.376525
3509.025459	901651.563889	42.381530
3509.018596	901504.730947	42.386535
3508.928000	901344.585191	42.391540
3508.743737	901184.546843	42.396544
3508.730662	901038.957825	42.401549
3508.916274	900888.697915	42.406554
3508.390748	900739.902881	42.411559
3508.742565	900582.559086	42.416564
3508.754623	900440.716078	42.421568
3508.616107	900287.500223	42.426573
3508.242960	900128.718212	42.431578
3508.317924	899996.123653	42.436583
3508.364070	899850.011275	42.441588
3508.294918	899695.609071	42.446592
3508.475551	899558.447999	42.451597
3508.611097	899409.219140	42.456602
3508.383117	899271.635532	42.461607
3508.587146	899124.512561	42.466612
3508.194089	898974.007150	42.471616
3508.097281	898823.931841	42.476621
3508.354644	898679.975802	42.481626
3508.317474	898555.865547	42.486631
3508.220413	898407.807601	42.491636
3508.054818	898267.194858	42.496640
3508.043039	898136.309569	42.501645
3508.200497	897982.306125	42.506650
3507.900070	897853.200626	42.511655
3507.690140	897710.166281	42.516660
3507.817525	897574.608058	42.521664
3507.936146	897442.525948	42.526669
3508.327413	897314.936555	42.531674
3507.477492	897182.235048	42.536679
3507.732385	897041.039472	42.541684
3507.703990	896914.089880	42.546688
3507.619390	896784.731203	42.551693
3507.928140	896645.256053	42.556698
3507.431776	896521.563300	42.561703
3507.666256	896393.979002	42.566708
3507.422123	896257.677456	42.571712
3507.269466	896128.508274	42.576717
3507.490722	896006.908579	42.581722
3507.495947	895884.568789	42.586727
3507.481245	895737.200503	42.591732
3507.696757	895630.185981	42.596736
3507.713895	895498.945066	42.601741
3507.775089	895366.630776	42.606746
3507.117319	895246.029407	42.611751
3507.176773	895111.776544	42.616756
3507.209973	894985.933445	42.621760
3507.319955	894864.327631	42.626765
3507.331521	894740.222408	42.631770
3506.958561	894625.940165	42.636775
3507.255912	894493.276676	42.641780
3507.014641	894373.554763	42.646784
3507.133113	894266.530570	42.651789
3507.318313	894138.130448	42.656794
3506.870686	894020.658404	42.661799
3507.140145	893905.095845	42.666804
3506.927441	893785.550200	42.671808
3506.775136	893657.484865	42.676813
3506.898790	893538.361986	42.681818
3506.930178	893430.949750	42.686823
3506.936420	893314.258459	42.691828
3506.977501	893198.042448	42.696832
3506.896520	893075.946519	42.701837
3506.780949	892968.356419	42.706842
3506.796499	892854.554741	42.711847
3506.810384	892735.433188	42.716852
3506.909287	892625.384073	42.721856
3506.789521	892508.793770	42.726861
3506.827069	892387.147049	42.731866
3506.503948	892280.351740	42.736871
3506.665968	892168.446195	42.741876
3506.611508	892058.121329	42.746880
3506.392467	891950.142300	42.751885
3506.542299	891835.137776	42.756890
3506.496801	891727.899593	42.761895
3506.285071	891607.534534	42.766900
3506.089297	891510.374639	42.771904
3506.247973	891399.615125	42.776909
3506.282665	891306.475677	42.781914
3506.415250	891213.028443	42.786919
3506.461365	891104.216054	42.791924
3506.090306	891003.401213	42.796929
3506.002206	890889.480798	42.801933
3506.210334	890789.727416	42.806938
3505.861428	890686.388584	42.811943
3506.026398	890583.737027	42.816948
3506.018947	890492.042166	42.821953
3505.830162	890398.344421	42.826957
3506.109096	890305.341927	42.831962
3505.325785	890206.709045	42.836967
3505.539519	890105.975539	42.841972
3505.807984	890014.130852	42.846977
3505.518855	889925.762330	42.851981
3506.020404	889836.585019	42.856986
3505.781816	889731.759749	42.861991
3505.781806	889629.118308	42.866996
3505.655375	889549.423892	42.872001
3505.792942	889461.171409	42.877005
3506.007648	889372.034153	42.882010
3505.845073	889269.993557	42.887015
3505.664085	889166.115951	42.892020
3505.680974	889076.426212	42.897025
3505.529199	888985.795341	42.902029
3505.618792	888888.544031	42.907034
3505.689375	888809.967954	42.912039
3505.803677	888714.160953	42.917044
3505.356864	888620.960515	42.922049
3505.250377	888529.347413	42.927053
3505.502147	888435.351560	42.932058
3505.428253	888346.633020	42.937063
3505.641076	888255.446770	42.942068
3505.307650	888164.929668	42.947073
3505.299898	888072.712443	42.952077
3505.590606	887981.799336	42.957082
3505.292308	887900.465330	42.962087
3505.302212	887806.982933	42.967092
3505.534581	887726.042897	42.972097
3505.063295	887649.669282	42.977101
3505.594523	887566.161632	42.982106
3505.245504	887474.765277	42.987111
3505.358346	887393.259604	42.992116
3505.518691	887302.841175	42.997121
3505.405119	887220.983251	43.002125
3505.483494	887128.639967	43.007130
3505.211788	887040.998548	43.012135
3505.282746	886958.912938	43.017140
3505.019063	886878.720255	43.022145
3504.714668	886801.727193	43.027149
3505.362006	886726.899265	43.032154
3505.112551	886643.119739	43.037159
3505.077369	886551.947444	43.042164
3504.916063	886476.087983	43.047169
3504.785910	886401.383939	43.052173
3505.221158	886321.165165	43.057178
3505.201397	886245.182560	43.062183
3505.236176	886147.990893	43.067188
3505.001163	886075.332705	43.072193
3505.057967	885996.720600	43.077197
3505.045534	885919.764492	43.082202
3505.058671	885841.641493	43.087207
3505.146614	885759.632872	43.092212
3505.063452	885675.811937	43.097217
3504.884756	885598.201296	43.102221
3505.018591	885518.214682	43.107226
3504.709992	885450.207655	43.112231
3504.822908	885367.608503	43.117236
3504.654233	885285.925893	43.122241
3504.792504	885215.228507	43.127245
3505.002697	885136.192194	43.132250
3504.748083	885060.232735	43.137255
3505.006891	884989.222283	43.142260
3504.781833	884919.452521	43.147265
3504.496924	884836.136780	43.152269
3504.438277	884758.301470	43.157274
3504.618055	884691.366951	43.162279
3504.349299	884623.440482	43.167284
3504.688011	884554.541700	43.172289
3504.609636	884485.033025	43.177293
3504.678076	884413.950074	43.182298
3504.421153	884334.302000	43.187303
3504.583505	884269.592580	43.192308
3504.590433	884205.779534	43.197313
3504.384545	884129.509364	43.202317
3504.538128	884065.670618	43.207322
3504.717168	884002.795332	43.212327
3504.562214	883917.314612	43.217332
3504.743037	883853.372211	43.222337
3504.418717	883783.701988	43.227341
3504.399124	883706.814543	43.232346
3504.558259	883651.879646	43.237351
3504.933022	883567.565450	43.242356
3504.737034	883506.683440	43.247361
3504.170475	883433.853089	43.252365
3504.494276	883354.870675	43.257370
3504.204187	883293.130316	43.262375
3504.092774	883238.720329	43.267380
3504.187238	883173.622509	43.272385
3504.596528	883115.735862	43.277389
3504.572098	883045.523136	43.282394
3504.114399	882978.964487	43.287399
3504.398282	882897.076867	43.292404
3504.352932	882834.710201	43.297409
3504.270604	882781.647118	43.302413
3504.352781	882708.700806	43.307418
3504.035200	882657.903063	43.312423
3504.152144	882574.101253	43.317428
3504.448769	882521.263945	43.322433
3504.283733	882462.496834	43.327437
3503.817076	882399.710616	43.332442
3504.010777	882334.877663	43.337447
3504.183919	882269.175599	43.342452
3503.848643	882211.208915	43.347457
3503.689331	882147.691289	43.352461
3504.056631	882097.550755	43.357466
3504.108022	882044.458931	43.362471
3504.057102	881983.343357	43.367476
3504.032902	881919.316640	43.372481
3504.204659	881866.493977	43.377485
3504.102901	881801.703779	43.382490
3503.626807	881744.724377	43.387495
3503.938933	881688.002053	43.392500
3504.032311	881628.796472	43.397505
3503.968418	881576.881887	43.402509
3504.385894	881505.609056	43.407514
3504.072477	881451.118785	43.412519
3504.123179	881392.208470	43.417524
3503.886754	881323.656879	43.422529
3503.874057	881268.340317	43.427533
3504.237785	881215.770788	43.432538
3503.745208	881160.241618	43.437543
3503.987114	881097.518407	43.442548
3504.230925	881041.382369	43.447553
3504.030425	880985.706536	43.452557
3503.845215	880913.072494	43.457562
3503.927953	880866.068659	43.462567
3504.057327	880795.125299	43.467572
3504.196412	880744.429432	43.472577
3504.109201	880691.251258	43.477581
3504.199778	880625.834990	43.482586
3503.988815	880574.904651	43.487591
3503.541438	880504.149675	43.492596
3504.176000	880459.764683	43.497601
3504.028167	880389.637233	43.502605
3503.949554	880335.194765	43.507610
3503.804442	880285.123120	43.512615
3504.056078	880216.478137	43.517620
3504.135604	880163.558392	43.522625
3503.699651	880108.494393	43.527629
3504.145489	880041.947173	43.532634
3503.872808	879994.025881	43.537639
3503.972501	879932.767153	43.542644
3504.013598	879882.855196	43.547649
3504.075396	879812.686299	43.552653
3503.773402	879764.089619	43.557658
3503.687512	879704.991013	43.562663
3503.545310	879645.610364	43.567668
3503.866173	879596.231322	43.572673
3503.415542	879544.459324	43.577677
3503.842880	879483.723382	43.582682
3503.333524	879434.673579	43.587687
3503.234943	879388.269226	43.592692
3503.742342	879348.354734	43.597697
3503.558495	879300.122391	43.602701
3503.693797	879232.938763	43.607706
3503.456414	879191.982938	43.612711
3503.556918	879131.781778	43.617716
3503.614964	879078.080446	43.622721
3503.201574	879028.042257	43.627725
3503.586630	878985.625591	43.632730
3503.701533	878941.508580	43.637735
3503.723902	878895.468081	43.642740
3504.029763	878832.225493	43.647745
3503.335209	878787.368392	43.652749
3503.700181	878729.639508	43.657754
3503.580161	878688.273138	43.662759
3503.574608	878631.282797	43.667764
3503.485603	878581.478129	43.672769
3503.348824	878542.633552	43.677773
3503.534404	878487.161139	43.682778
3503.197929	878449.318113	43.687783
3502.806786	878394.327548	43.692788
3503.334079	878349.750439	43.697793
3503.174164	878308.387966	43.702797
3503.335229	878265.227571	43.707802
3503.352211	878228.003400	43.712807
3503.077990	878183.072424	43.717812
3503.314900	878136.409040	43.722817
3503.054992	878102.137668	43.727821
3503.260804	878049.662724	43.732826
3503.216458	878022.043818	43.737831
3503.158221	877976.591007	43.742836
3503.251351	877927.235464	43.747841
3502.615789	877888.080990	43.752845
3502.979718	877849.246273	43.757850
3503.132009	877812.191053	43.762855
3503.202498	877760.220513	43.767860
3503.026805	877716.626882	43.772865
3503.097341	877674.058704	43.777869
3503.091254	877631.599783	43.782874
3503.087267	877599.028251	43.787879
3502.890210	877553.498100	43.792884
3503.082544	877515.561936	43.797889
3503.158319	877475.511974	43.802893
3503.133226	877429.176982	43.807898
3502.872348	877394.416922	43.812903
3503.336306	877355.950256	43.817908
3503.409469	877309.404244	43.822913
3502.878899	877276.820738	43.827917
3503.347271	877225.458556	43.832922
3503.216021	877192.614900	43.837927
3503.316900	877146.547776	43.842932
3503.267759	877099.729409	43.847937
3502.964882	877066.525527	43.852941
3503.594293	877021.436802	43.857946
3503.393693	876983.561952	43.862951
3503.284819	876931.516700	43.867956
3503.074890	876885.886554	43.872961
3502.953943	876855.075336	43.877965
3503.317404	876801.593767	43.882970
3503.169076	876762.933249	43.887975
3503.360800	876723.634718	43.892980
3503.475562	876679.403819	43.897985
3503.277481	876631.830622	43.902989
3503.221094	876581.615824	43.907994
3503.097042	876541.786357	43.912999
3503.096786	876496.700408	43.918004
3503.324141	876451.770536	43.923009
3503.284631	876433.160690	43.928013
3503.297927	876383.223605	43.933018
3503.093354	876344.181761	43.938023
3503.333955	876296.824474	43.943028
3503.384148	876252.407088	43.948033
3502.931153	876210.108519	43.953037
3503.263978	876163.510684	43.958042
3503.247414	876132.678494	43.963047
3503.173183	876084.013851	43.968052
3503.600811	876046.029476	43.973057
3503.251512	876001.482085	43.978061
3503.157435	875951.849945	43.983066
3503.330951	875905.179352	43.988071
3503.577007	875860.338871	43.993076
3503.281871	875817.041774	43.998081
3503.077561	875781.196197	44.003085
3503.522216	875723.618696	44.008090
3503.226553	875687.981548	44.013095
3503.124262	875635.438915	44.018100
3503.465265	875598.338701	44.023105
3503.162878	875548.058667	44.028109
3503.232690	875505.281010	44.033114
3503.237330	875465.520054	44.038119
3503.151315	875430.137740	44.043124
3503.109787	875397.269305	44.048129
3502.944630	875350.456175	44.053133
3503.310330	875307.628340	44.058138
3502.936343	875266.182798	44.063143
3503.028809	875230.575925	44.068148
3503.044306	875189.065674	44.073153
3502.941660	875156.012005	44.078157
3503.041861	875110.317035	44.083162
3502.676160	875081.476528	44.088167
3502.726625	875028.806353	44.093172
3502.735996	875008.341273	44.098177
3502.446464	874979.099781	44.103181
3502.901179	874940.909885	44.108186
3502.689116	874906.030127	44.113191
3502.650758	874875.873872	44.118196
3502.674826	874829.219412	44.123201
3502.536567	874801.115961	44.128205
3503.065767	874768.343978	44.133210
3502.843343	874741.320977	44.138215
3502.788757	874697.200135	44.143220
3502.820310	874663.054720	44.148225
3502.887404	874631.909952	44.153229
3502.752667	874592.263081	44.158234
3502.603306	874564.645290	44.163239
3502.649902	874535.152242	44.168244
3502.568397	874511.887655	44.173249
3502.519065	874469.607103	44.178253
3502.604970	874445.247751	44.183258
3502.648422	874419.537382	44.188263
3502.733653	874378.882906	44.193268
3503.100673	874342.546500	44.198273
3502.570613	874318.676089	44.203277
3502.890670	874274.102391	44.208282
3502.739261	874255.795113	44.213287
3502.867395	874206.984687	44.218292
3502.613302	874175.017459	44.223297
3502.459879	874146.040417	44.228301
3502.701828	874108.074212	44.233306
3502.492603	874086.865972	44.238311
3502.834429	874052.762923	44.243316
3502.733495	874014.173610	44.248321
3502.613109	873991.010383	44.253325
3502.992682	873957.870578	44.258330
3502.635152	873921.553965	44.263335
3502.727858	873882.640887	44.268340
3502.772038	873846.354633	44.273345
3502.657711	873819.891634	44.278349
3503.082991	873784.803263	44.283354
3502.828947	873753.415776	44.288359
3502.826811	873715.099253	44.293364
3502.801941	873666.794617	44.298369
3502.822137	873652.143428	44.303373
3502.783047	873611.989209	44.308378
3502.594763	873581.269024	44.313383
3502.579442	873547.900969	44.318388
3502.429118	873514.554969	44.323393
3502.578435	873491.151338	44.328397
3503.052978	873447.419063	44.333402
3502.408421	873425.504100	44.338407
3502.671890	873386.947680	44.343412
3502.642648	873364.543074	44.348417
3502.234334	873325.126820	44.353421
3502.532755	873310.719986	44.358426
3502.702184	873270.238065	44.363431
3502.379270	873243.224783	44.368436
3502.536360	873208.371221	44.373441
3502.356540	873197.826429	44.378445
3502.604999	873155.875504	44.383450
3502.312717	873139.625287	44.388455
3502.319210	873101.303381	44.393460
3502.342973	873084.515868	44.398465
3501.926073	873063.338179	44.403469
3502.559348	873020.546772	44.408474
3502.410849	873014.168205	44.413479
3502.478747	872983.111666	44.418484
3502.598526	872960.680986	44.423489
3502.452333	872928.592241	44.428493
3502.654328	872888.102352	44.433498
3502.446555	872870.576231	44.438503
3502.535022	872838.739397	44.443508
3502.714322	872806.499347	44.448513
3502.498733	872781.212640	44.453517
3502.383384	872740.288925	44.458522
3502.390213	872719.428282	44.463527
3502.682684	872699.005614	44.468532
3502.709934	872674.648663	44.473537
3502.340411	872640.169598	44.478541
3502.425909	872612.504020	44.483546
3502.446945	872587.759643	44.488551
3502.247566	872561.110996	44.493556
3502.269634	872529.574519	44.498561
3502.347151	872514.328933	44.503565
3502.572550	872474.317497	44.508570
3502.354541	872460.866921	44.513575
3502.150037	872432.181000	44.518580
3502.482604	872396.420535	44.523585
3502.326311	872378.981507	44.528589
3502.905284	872345.605817	44.533594
3502.405395	872320.461014	44.538599
3502.294933	872287.489668	44.543604
3502.702001	872266.270410	44.548609
3502.543346	872231.172056	44.553613
3502.473461	872203.045027	44.558618
3502.377155	872184.237126	44.563623
3502.479017	872158.895469	44.568628
3502.861129	872124.192544	44.573633
3502.350033	872090.218767	44.578637
3502.618468	872061.453139	44.583642
3502.767927	872046.000438	44.588647
3502.694421	872014.865109	44.593652
3502.850017	871972.144876	44.598657
3502.397964	871953.588924	44.603661
3502.553300	871913.876368	44.608666
3502.780253	871893.073597	44.613671
3502.798211	871846.202633	44.618676
3502.645787	871817.019985	44.623681
3502.271050	871789.135297	44.628685
3502.796308	871772.455533	44.633690
3502.333045	871741.480025	44.638695
3502.411809	871715.849176	44.643700
3502.567838	871682.927613	44.648705
3502.061883	871662.729978	44.653709
3502.115013	871628.563564	44.658714
3502.271961	871610.585479	44.663719
3502.181501	871588.475386	44.668724
3502.442664	871552.430503	44.673729
3502.433294	871543.698459	44.678733
3502.626314	871505.044419	44.683738
3502.094284	871487.761722	44.688743
3502.163686	871458.346686	44.693748
3502.419183	871439.381429	44.698753
3502.158879	871418.463194	44.703757
3502.328784	871390.001691	44.708762
3502.127714	871374.410914	44.713767
3502.087763	871339.481831	44.718772
3502.369483	871330.119253	44.723777
3502.316573	871311.883710	44.728781
3502.502663	871281.769268	44.733786
3502.356921	871261.413877	44.738791
3502.092431	871226.909309	44.743796
3502.806435	871210.779160	44.748801
3502.286299	871178.742582	44.753805
3502.267927	871145.749741	44.758810
3502.484811	871138.241440	44.763815
3502.496574	871096.509103	44.768820
3502.554951	871069.423116	44.773825
3502.108596	871051.057499	44.778829
3502.638589	871020.011640	44.783834
3502.212487	870998.731050	44.788839
3502.009319	870972.270008	44.793844
3502.383192	870946.781335	44.798849
3502.079276	870927.906619	44.803853
3502.348638	870905.249456	44.808858
3502.488420	870883.875224	44.813863
3502.198332	870859.077874	44.818868
3502.576029	870824.853383	44.823873
3502.500957	870810.793209	44.828877
3502.394598	870777.812829	44.833882
3502.170584	870765.621096	44.838887
3502.285829	870735.030302	44.843892
3502.284442	870720.084290	44.848897
3502.142334	870691.282644	44.853901
3502.038666	870664.027405	44.858906
3502.195946	870653.713722	44.863911
3502.164700	870620.623043	44.868916
3502.424507	870604.274929	44.873921
3502.172373	870585.681765	44.878925
3502.170582	870545.209536	44.883930
3501.877166	870538.852183	44.888935
3502.378654	870511.787720	44.893940
3502.280824	870490.062997	44.898945
3502.383541	870476.166858	44.903949
3502.390133	870438.021914	44.908954
3502.483227	870423.350769	44.913959
3502.316221	870396.007683	44.918964
3502.376653	870372.994688	44.923969
3502.125955	870332.950268	44.928973
3502.265796	870310.506312	44.933978
3502.281058	870288.956346	44.938983
3502.214948	870256.742944	44.943988
3502.414573	870234.871224	44.948993
3502.248501	870208.400682	44.953997
3502.203586	870192.101646	44.959002
3502.135684	870166.197119	44.964007
3502.111699	870148.244443	44.969012
3502.249612	870127.741385	44.974017
3502.087816	870108.840659	44.979021
3502.022995	870089.050317	44.984026
3502.489523	870071.501920	44.989031
3501.961072	870043.246120	44.994036
3502.199934	870019.425847	44.999041
3501.892680	870010.837702	45.004045
3502.228003	869983.312901	45.009050
3502.419702	869976.389691	45.014055
3502.076526	869938.590382	45.019060
3502.225600	869916.531694	45.024065
3502.326867	869905.158212	45.029069
3502.221799	869881.005782	45.034074
3502.292161	869862.551366	45.039079
3501.956764	869833.874496	45.044084
3502.026935	869805.907221	45.049089
3501.624096	869802.964518	45.054093
3502.140465	869775.894280	45.059098
3502.170990	869759.969914	45.064103
3502.228672	869748.312107	45.069108
3502.773818	869722.401725	45.074113
3502.093643	869702.517343	45.079117
3502.436879	869667.903633	45.084122
3502.501081	869637.218560	45.089127
3502.292483	869617.353273	45.094132
3502.407632	869584.621026	45.099137
3502.165622	869573.885906	45.104141
3502.266728	869537.272805	45.109146
3502.279690	869529.990235	45.114151
3502.562443	869510.237787	45.119156
3502.580996	869476.841349	45.124161
3502.241039	869453.114186	45.129165
3502.451426	869421.141952	45.134170
3502.421267	869395.227866	45.139175
3501.886986	869368.620114	45.144180
3502.234395	869362.641304	45.149185
3502.247370	869330.506957	45.154189
3502.296638	869308.074165	45.159194
3502.143792	869292.275843	45.164199
3502.097593	869267.140462	45.169204
3502.038155	869248.996772	45.174209
3502.177700	869240.722216	45.179213
3502.456128	869202.039212	45.184218
3502.482503	869184.560740	45.189223
3502.389757	869154.481526	45.194228
3502.245028	869133.244993	45.199233
3501.974765	869111.737827	45.204237
3502.419464	869090.015711	45.209242
3502.510075	869071.264279	45.214247
3502.096645	869047.450528	45.219252
3502.652756	869022.894459	45.224257
3502.284829	868999.073019	45.229261
3502.346911	868984.015128	45.234266
3502.367430	868950.906680	45.239271
3502.464660	868925.066654	45.244276
3502.206000	868896.760975	45.249281
3501.812989	868872.069409	45.254285
3502.281769	868862.866333	45.259290
3502.207028	868832.297112	45.264295
3501.863501	868809.732998	45.269300
3502.319371	868798.201910	45.274305
3502.133090	868770.660392	45.279309
3502.392663	868747.802511	45.284314
3502.194742	868734.631465	45.289319
3502.080379	868706.592373	45.294324
3502.327810	868697.231339	45.299329
3501.898687	868677.593434	45.304333
3502.331261	868648.104739	45.309338
3502.056763	868628.441197	45.314343
3502.141460	868595.126034	45.319348
3502.383199	868572.173334	45.324353
3502.168119	868560.169797	45.329357
3502.248020	868528.893927	45.334362
3501.983573	868516.218808	45.339367
3501.924657	868484.868489	45.344372
3502.104434	868468.236467	45.349377
3501.848803	868465.074657	45.354381
3501.933963	868440.205436	45.359386
3502.285572	868426.554812	45.364391
3501.697540	868401.019608	45.369396
3501.964894	868398.062874	45.374401
3502.152565	868364.244005	45.379405
3502.060562	868335.325661	45.384410
3501.880089	868332.636862	45.389415
3502.093399	868319.105871	45.394420
3502.390052	868290.705838	45.399425
3502.264581	868279.172442	45.404429
3502.050067	868243.768562	45.409434
3502.002947	868229.503522	45.414439
3502.002165	868217.561087	45.419444
3502.237790	868196.355661	45.424449
3502.121672	868180.451258	45.429453
3501.953487	868159.797708	45.434458
3502.086624	868137.055430	45.439463
3501.943330	868130.962055	45.444468
3502.195019	868109.268196	45.449473
3501.538582	868093.938063	45.454477
3502.503790	868069.310703	45.459482
3502.532848	868052.993654	45.464487
3502.203364	868027.122966	45.469492
3502.361449	868010.687447	45.474497
3502.361509	867985.053578	45.479501
3502.430561	867960.087924	45.484506
3502.077907	867925.870112	45.489511
3501.983615	867923.943723	45.494516
3502.174705	867902.259101	45.499521
3502.222951	867884.967438	45.504525
3502.371935	867854.550572	45.509530
3502.183484	867827.684782	45.514535
3502.049688	867809.160579	45.519540
3502.331961	867795.034441	45.524545
3502.432371	867770.257034	45.529549
3502.488387	867750.341952	45.534554
3502.210923	867721.451204	45.539559
3501.998226	867697.016389	45.544564
3502.355779	867678.605038	45.549569
3502.357454	867648.891125	45.554573
3502.158048	867632.416366	45.559578
3501.999247	867605.059173	45.564583
3502.061400	867587.278839	45.569588
3502.336731	867569.948856	45.574593
3501.956025	867556.999543	45.579597
3501.905599	867527.487823	45.584602
3501.894701	867522.051756	45.589607
3502.314251	867503.144126	45.594612
3502.281346	867471.590014	45.599617
3501.886868	867463.498101	45.604621
3502.189049	867435.869975	45.609626
3502.287135	867415.267100	45.614631
3502.020616	867405.406090	45.619636
3502.161333	867359.742142	45.624641
3501.892729	867361.534413	45.629645
3502.130322	867354.989061	45.634650
3502.152649	867327.309435	45.639655
3502.054443	867309.748917	45.644660
3502.187989	867283.118967	45.649665
3502.063562	867269.349930	45.654669
3502.216686	867242.133913	45.659674
3502.242133	867227.368984	45.664679
3502.024403	867208.274091	45.669684
3501.903763	867182.559571	45.674689
3502.226877	867171.241472	45.679693
3502.086216	867140.577379	45.684698
3502.071214	867134.170517	45.689703
3502.003614	867110.097855	45.694708
3501.858751	867083.512889	45.699713
3502.024211	867077.464686	45.704717
3502.179493	867061.027036	45.709722
3501.903069	867028.928040	45.714727
3501.821553	867021.366649	45.719732
3502.099098	867002.966417	45.724737
3502.001413	866985.599095	45.729741
3502.056264	866965.487375	45.734746
3501.866699	866953.379299	45.739751
3501.984119	866934.519663	45.744756
3502.303559	866907.857426	45.749761
3501.807528	866909.881528	45.754765
3501.967613	866888.781057	45.759770
3501.642360	866866.303726	45.764775
3502.038634	866863.713474	45.769780
3502.181064	866847.471592	45.774785
3502.089171	866818.060337	45.779789
3502.105228	866794.652451	45.784794
3502.091776	866780.669775	45.789799
3501.909566	866750.884601	45.794804
3502.127229	866715.400504	45.799809
3501.570903	866639.544750	45.804813
3501.908452	866512.260469	45.809818
3502.483838	866326.173858	45.814823
3501.949963	866078.101890	45.819828
3501.850499	865770.696591	45.824833
3501.655142	865408.310434	45.829837
3501.910177	864981.323136	45.834842
3501.569320	864487.853163	45.839847
3501.384097	863951.662673	45.844852
3501.350006	863342.325977	45.849857
3500.919271	862687.414376	45.854861
3500.873170	861953.835304	45.859866
3500.408220	861162.592560	45.864871
3500.342247	860318.973453	45.869876
3500.053550	859402.153158	45.874881
3499.402067	858419.513156	45.879885
3499.033218	857382.393345	45.884890
3498.779924	856274.741875	45.889895
3498.276963	855111.858016	45.894900
3498.300103	853865.359341	45.899905
3497.576724	852567.334577	45.904909
3497.188226	851189.240418	45.909914
3496.763048	849745.207021	45.914919
3495.859909	848236.431179	45.919924
3495.898100	846662.048629	45.924929
3494.921535	845016.290998	45.929933
3494.675652	843283.022867	45.934938
3493.763844	841505.555159	45.939943
3493.292160	839656.455367	45.944948
3492.958878	837732.590530	45.949953
3492.111011	835747.911685	45.954957
3491.475054	833666.608189	45.959962
3490.791508	831539.517399	45.964967
3490.167699	829337.953306	45.969972
3489.767235	827065.872839	45.974977
3488.230842	824730.127548	45.979981
3487.440989	822323.937052	45.984986
3486.747069	819860.300332	45.989991
3485.770124	817325.126129	45.994996
3484.984708	814719.630813	46.000001
3484.176953	812052.001855	46.005005
3483.287833	809318.261642	46.010010
3482.442586	806510.914525	46.015015
3481.429281	803648.301393	46.020020
3480.622521	800697.183755	46.025025
3479.342080	797702.183430	46.030029
3478.646376	794645.302977	46.035034
3477.474872	791513.480165	46.040039
3475.888325	788325.732929	46.045044
3475.187561	785045.495262	46.050049
3473.963410	781734.373551	46.055053
3472.592636	778339.172127	46.060058
3471.452949	774892.417385	46.065063
3470.049982	771366.248950	46.070068
3468.830380	767787.353793	46.075073
3467.961695	764156.234493	46.080077
3466.497513	760451.427494	46.085082
3464.814390	756689.560026	46.090087
3463.660888	752856.465596	46.095092
3462.405429	748954.284007	46.100097
3460.764029	745016.590687	46.105101
3459.337826	741008.631547	46.110106
3458.249302	736925.697515	46.115111
3456.588405	732789.380878	46.120116
3454.753489	728585.487681	46.125121
3453.282295	724337.685800	46.130125
3451.559327	720025.206115	46.135130
3450.342003	715645.069159	46.140135
3448.638091	711203.463608	46.145140
3446.820542	706705.025617	46.150145
3445.175003	702164.205393	46.155149
3443.559289	697548.324450	46.160154
3441.775493	692877.820312	46.165159
3439.944718	688146.147225	46.170164
3438.286115	683352.905121	46.175169
3436.490550	678518.307735	46.180173
3434.689266	673595.295356	46.185178
3432.565990	668632.242787	46.190183
3430.535425	663619.673131	46.195188
3429.115126	658545.927135	46.200193
3426.727968	653420.348094	46.205197
3424.737182	648213.031916	46.210202
3423.237590	642970.529899	46.215207
3420.754620	637677.212382	46.220212
3418.911857	632327.219249	46.225217
3416.811882	626932.173659	46.230221
3414.484280	621466.542082	46.235226
3412.439728	615961.260744	46.240231
3410.116247	610412.246390	46.245236
3407.774120	604799.415900	46.250241
3405.779314	599145.457099	46.255245
3403.125042	593432.542897	46.260250
3400.985708	587680.647591	46.265255
3398.553333	581879.090496	46.270260
3396.282455	576013.543352	46.275265
3393.789561	570124.194348	46.280269
3391.466477	564173.591363	46.285274
3389.252969	558182.520633	46.290279
3386.396101	552147.833403	46.295284
3383.946553	546045.307504	46.300289
3381.157233	539919.726338	46.305293
3379.073332	533751.773478	46.310298
3376.016996	527542.541191	46.315303
3373.066482	521274.135952	46.320308
3370.887379	514973.520350	46.325313
3367.553769	508647.103726	46.330317
3364.980730	502262.800783	46.335322
3362.368136	495847.148146	46.340327
3359.596739	489393.012565	46.345332
3356.891329	482904.483740	46.350337
3353.488352	476375.744937	46.355341
3351.012905	469815.725700	46.360346
3347.984748	463213.865710	46.365351
3344.571687	456594.753477	46.370356
3341.794115	449912.691914	46.375361
3338.485727	443228.452140	46.380365
3335.462060	436504.122703	46.385370
3332.578448	429740.123606	46.390375
3329.090366	422950.709115	46.395380
3326.164251	416142.447484	46.400385
3322.966879	409304.289280	46.405389
3319.332318	402437.715955	46.410394
3316.145916	395539.871696	46.415399
3312.631375	388642.840417	46.420404
3309.618631	381691.862009	46.425409
3305.914339	374741.135881	46.430413
3302.324639	367741.785189	46.435418
3298.771891	360743.656972	46.440423
3294.907082	353727.839756	46.445428
3291.619086	346695.662705	46.450433
3288.083050	339647.034500	46.455437
3284.079119	332576.623885	46.460442
3280.635355	325518.575461	46.465447
3276.812118	318438.386287	46.470452
3273.245662	311334.681914	46.475457
3269.445512	304232.653081	46.480461
3265.518318	297122.210449	46.485466
3261.513773	289986.879655	46.490471
3257.696691	282861.539410	46.495476
3253.579945	275725.731450	46.500481
3249.641721	268585.933498	46.505485
3245.649854	261459.438117	46.510490
3241.933225	254307.415492	46.515495
3237.684439	247172.619591	46.520500
3233.588275	240025.509071	46.525505
3229.289146	232893.328863	46.530509
3225.275507	225739.594121	46.535514
3220.951947	218540.178328	46.540519
3216.658554	211408.326938	46.545524
3212.478872	204294.428788	46.550529
3208.165375	197184.021521	46.555533
3203.744131	190076.373447	46.560538
3199.509513	182997.431976	46.565543
3194.802643	175921.375221	46.570548
3190.405501	168858.706537	46.575553
3186.119525	161812.108828	46.580557
3180.941413	154790.779187	46.585562
3176.550944	147776.890030	46.590567
3171.387937	140799.179830	46.595572
3166.928897	133838.110884	46.600577
3161.621266	126904.280018	46.605581
3156.429249	120000.998231	46.610586
3151.943379	113133.665329	46.615591
3146.397899	106307.198843	46.620596
3141.395767	99496.704898	46.625601
3135.887726	92742.217060	46.630605
3130.535356	86024.715541	46.635610
3124.951211	79356.004434	46.640615
3118.853912	72731.369700	46.645620
3113.393270	66155.010473	46.650625
3107.068654	59653.034958	46.655629
3100.181210	53217.944599	46.660634
3093.453044	46861.142256	46.665639
3084.648270	40611.939239	46.670644
3069.988751	34633.460848	46.675649
3051.047482	28941.230428	46.680653
3032.591690	23470.104228	46.685658
3014.374997	18292.280252	46.690663
2991.590028	13552.544415	46.695668
2964.823116	9310.577791	46.700673
2935.768895	5616.792248	46.705677
2906.118714	2439.456149	46.710682
2856.302686	411.706291	46.715687
2764.087322	309.075566	46.720692
2713.723846	306.557395	46.725697
2708.009575	293.433748	46.730701
2730.301357	283.139470	46.735706
2762.320006	277.754674	46.740711
2789.907893	283.486862	46.745716
2807.720104	284.597594	46.750721
2815.162523	284.215970	46.755725
2814.466316	283.138159	46.760730
2809.817245	276.438986	46.765735
2803.925934	276.114498	46.770740
2799.100142	262.129400	46.775745
2794.933521	271.921509	46.780749
2791.670662	278.579903	46.785754
2789.597182	264.925741	46.790759
2787.237012	265.826328	46.795764
2785.760919	256.445145	46.800769
2783.028056	258.464981	46.805773
2780.032543	260.889685	46.810778
2777.249567	260.090269	46.815783
2773.577068	266.486299	46.820788
2770.828188	260.742962	46.825793
2767.496103	251.038494	46.830797
2764.272177	258.645215	46.835802
2761.539885	262.049127	46.840807
2758.530675	259.771459	46.845812
2755.672595	255.594894	46.850817
2752.191268	251.896906	46.855821
2748.543188	260.802273	46.860826
2745.236963	248.689927	46.865831
2742.233859	259.454802	46.870836
2739.046394	254.809243	46.875841
2735.573842	250.280192	46.880845
2732.638009	246.637851	46.885850
2729.517460	237.546196	46.890855
2725.747366	245.883228	46.895860
2722.869295	231.691718	46.900865
2719.362268	241.069148	46.905869
2715.946138	246.664718	46.910874
2712.427923	229.543722	46.915879
2708.739860	245.020482	46.920884
2705.692618	240.304057	46.925889
2702.491819	244.618875	46.930893
2698.540307	244.591323	46.935898
2695.473625	239.567101	46.940903
2691.910375	238.047915	46.945908
2688.852591	244.360320	46.950913
2685.682333	236.405301	46.955917
2682.383511	237.598568	46.960922
2678.538668	232.781306	46.965927
2675.263863	238.970865	46.970932
2672.131246	242.935811	46.975937
2668.482571	225.778762	46.980941
2664.502894	238.187239	46.985946
2661.458692	235.290230	46.990951
2658.297245	234.219434	46.995956
2655.056173	235.557904	47.000961
2651.382419	233.460616	47.005965
2647.498906	232.637252	47.010970
2644.095168	221.566092	47.015975
2640.402896	232.115557	47.020980
2637.301323	233.534820	47.025985
2634.665455	225.674396	47.030989
2631.013001	228.953936	47.035994
2626.993363	228.256458	47.040999
2622.875749	231.494755	47.046004
2620.379179	227.813154	47.051009
2617.101380	232.591850	47.056013
2613.605168	224.145621	47.061018
2610.354772	225.360938	47.066023
2606.667813	225.606731	47.071028
2603.375795	223.101926	47.076033
2599.593843	215.967433	47.081037
2596.119481	219.975791	47.086042
2593.167789	215.729929	47.091047
2588.647242	223.497823	47.096052
2585.033439	225.972966	47.101057
2581.990703	220.266413	47.106061
2578.741577	221.105407	47.111066
2575.850496	215.651690	47.116071
2571.911172	219.535903	47.121076
2568.590816	221.081696	47.126081
2565.183458	217.476632	47.131085
2561.344555	218.028944	47.136090
2558.149887	223.776714	47.141095
2554.430060	231.349343	47.146100
2551.030511	217.107079	47.151105
2547.299066	218.747174	47.156109
2543.840198	219.934183	47.161114
2540.814231	212.919283	47.166119
2537.163064	215.278272	47.171124
2533.912541	213.643654	47.176129
2529.882094	214.444677	47.181133
2526.765962	212.534892	47.186138
2523.270813	216.508443	47.191143
2519.850794	223.596670	47.196148
2516.288210	219.002925	47.201153
2513.081232	213.920684	47.206157
2509.212627	214.319670	47.211162
2505.886835	215.069535	47.216167
2502.343521	219.192346	47.221172
2498.900017	216.171112	47.226177
2495.389872	211.152340	47.231181
2491.704474	214.443726	47.236186
2488.618533	212.626863	47.241191
2484.897758	215.840420	47.246196
2481.542854	202.122695	47.251201
2478.171995	207.079634	47.256205
2474.614684	207.190063	47.261210
2471.086356	203.913875	47.266215
2467.166590	212.245573	47.271220
2463.819399	201.657605	47.276225
2460.437510	206.712086	47.281229
2456.852706	201.190807	47.286234
2453.701567	206.432569	47.291239
2450.151511	215.932889	47.296244
2446.846876	204.748648	47.301249
2443.291308	204.002548	47.306253
2439.321956	208.310179	47.311258
2436.357670	196.637597	47.316263
2432.296335	208.022459	47.321268
2429.514601	204.459869	47.326273
2425.780643	206.569941	47.331277
2422.369709	203.127986	47.336282
2419.087733	197.063991	47.341287
2414.908012	192.391040	47.346292
2411.682285	199.050598	47.351297
2408.300708	206.584451	47.356301
2404.509222	203.928777	47.361306
2401.148442	206.223550	47.366311
2397.373850	209.205296	47.371316
2394.413393	201.073788	47.376321
2390.986640	198.489349	47.381325
2387.228173	205.609047	47.386330
2384.100858	198.942720	47.391335
2380.139265	203.663529	47.396340
2376.534807	200.437672	47.401345
2373.491819	199.956305	47.406349
2370.112607	206.238256	47.411354
2366.755241	205.099939	47.416359
2362.942543	200.953732	47.421364
2359.515063	200.096365	47.426369
2356.372366	207.881698	47.431373
2352.459376	196.761848	47.436378
2348.955053	199.115082	47.441383
2344.912405	195.480074	47.446388
2341.921881	192.788139	47.451393
2338.466515	191.613331	47.456397
2334.538607	201.800081	47.461402
2331.412317	198.956509	47.466407
2327.811300	206.099394	47.471412
2324.337453	193.977996	47.476417
2320.911123	197.301328	47.481421
2317.547001	201.091957	47.486426
2314.120143	190.265658	47.491431
2310.620709	190.748307	47.496436
2306.864311	195.786561	47.501441
2303.711705	193.286975	47.506445
2299.929966	204.311802	47.511450
2296.960871	190.391225	47.516455
2292.338835	200.132937	47.521460
2289.317831	192.931505	47.526465
2286.433512	200.706976	47.531469
2282.326602	195.717823	47.536474
2279.495625	182.802806	47.541479
2275.458905	194.060763	47.546484
2272.386766	190.620019	47.551489
2268.308922	190.857383	47.556493
2264.901320	192.360942	47.561498
2261.796459	185.755925	47.566503
2257.960062	198.416082	47.571508
2254.292300	185.498724	47.576513
2250.893462	191.586248	47.581517
2247.574530	194.108849	47.586522
2244.189759	186.351805	47.591527
2240.238167	188.558724	47.596532
2236.876318	182.035031	47.601537
2233.638070	189.230957	47.606541
2229.837424	193.741974	47.611546
2226.525390	184.437233	47.616551
2223.029828	187.921445	47.621556
2219.734789	182.215170	47.626561
2215.959265	179.266926	47.631565
2212.666931	190.282434	47.636570
2209.251022	177.469376	47.641575
2205.481377	186.362560	47.646580
2201.830353	186.859658	47.651585
2198.417707	181.173804	47.656589
2194.748277	185.985832	47.661594
2191.627497	179.705950	47.666599
2188.109928	184.802339	47.671604
2184.218102	185.651204	47.676609
2181.350175	183.617390	47.681613
2177.622588	183.184651	47.686618
2174.382069	180.450430	47.691623
2170.614518	178.338023	47.696628
2167.075190	177.814415	47.701633
2163.882060	179.343015	47.706637
2160.082135	182.402723	47.711642
2156.564033	174.082261	47.716647
2152.867824	195.036827	47.721652
2149.209179	184.538240	47.726657
2146.099384	182.098790	47.731661
2142.740686	183.481083	47.736666
2139.368676	180.904171	47.741671
2135.527609	184.989558	47.746676
2131.989309	179.753915	47.751681
2128.486905	183.590387	47.756685
2124.761223	186.360797	47.761690
2121.844107	178.206942	47.766695
2117.935035	182.013678	47.771700
2114.593978	184.118894	47.776705
2110.986646	179.612195	47.781709
2107.606544	181.798655	47.786714
2104.284045	176.320786	47.791719
2100.555988	174.974895	47.796724
2097.034667	173.238869	47.801729
2093.657897	174.721862	47.806733
2089.896464	176.325211	47.811738
2086.576429	169.373216	47.816743
2082.583526	171.399606	47.821748
2079.938746	164.814070	47.826753
2076.355340	167.477741	47.831757
2072.629497	175.549355	47.836762
2068.779503	168.449856	47.841767
2065.570416	167.001520	47.846772
2061.786034	179.016385	47.851777
2058.472904	170.648935	47.856781
2055.042934	182.748351	47.861786
2051.945225	166.969163	47.866791
2048.294350	175.235818	47.871796
2045.000262	177.544872	47.876801
2041.212085	169.836656	47.881805
2037.308050	178.198605	47.886810
2034.021382	170.206486	47.891815
2030.292326	175.864998	47.896820
2026.748686	171.655503	47.901825
2023.371027	172.098513	47.906829
2019.941159	177.830961	47.911834
2016.774644	172.075001	47.916839
2013.374768	179.260446	47.921844
2009.500830	165.859159	47.926849
2006.365974	165.215197	47.931853
2002.297243	168.826181	47.936858
1998.622176	161.892435	47.941863
1995.449235	170.484936	47.946868
1992.154026	171.996168	47.951873
1989.077878	167.266864	47.956877
1984.968835	172.616374	47.961882
1982.040327	174.291822	47.966887
1978.264230	174.492422	47.971892
1974.523570	172.103207	47.976897
1971.063054	159.589991	47.981901
1967.040240	173.458236	47.986906
1964.360844	161.874746	47.991911
1960.650104	165.071626	47.996916
1956.882769	168.898884	48.001921
1953.516836	170.795781	48.006925
1949.870675	164.392880	48.011930
1946.722702	159.363280	48.016935
1943.204091	172.148348	48.021940
1939.494317	168.810185	48.026945
1936.488749	162.537711	48.031949
1932.455836	171.822070	48.036954
1929.508074	173.456327	48.041959
1925.543479	173.948392	48.046964
1921.951036	173.239556	48.051969
1918.359709	163.839510	48.056973
1914.525756	168.802439	48.061978
1911.716195	165.239245	48.066983
1907.981973	165.050935	48.071988
1904.699272	163.118955	48.076993
1900.742874	168.091857	48.081997
1897.341737	167.050499	48.087002
1893.989200	160.896342	48.092007
1890.880372	167.316656	48.097012
1886.999842	160.664602	48.102017
1883.571049	157.614765	48.107021
1880.160125	166.311364	48.112026
1876.937324	152.201372	48.117031
1872.917851	169.044411	48.122036
1869.368253	165.851139	48.127041
1866.221082	159.541324	48.132045
1862.430244	163.190784	48.137050
1859.126496	157.303884	48.142055
1855.747244	161.594206	48.147060
1852.000924	157.233030	48.152065
1848.468372	158.547347	48.157069
1844.785475	160.231252	48.162074
1841.608816	161.744512	48.167079
1837.599503	174.403296	48.172084
1834.159401	165.561479	48.177089
1831.097702	161.671947	48.182093
1827.486801	168.237987	48.187098
1824.583257	155.645725	48.192103
1820.798151	166.940374	48.197108
1817.154494	166.494645	48.202113
1813.416081	159.645522	48.207117
1809.825532	162.723398	48.212122
1806.543138	160.410967	48.217127
1802.537744	165.579314	48.222132
1799.397504	154.863004	48.227137
1796.341863	151.854802	48.232141
1792.283431	158.126357	48.237146
1788.818326	156.838316	48.242151
1785.074996	159.964537	48.247156
1781.992320	159.694350	48.252161
1779.047031	161.463070	48.257165
1774.976823	162.308578	48.262170
1771.464912	152.954352	48.267175
1767.677596	158.010723	48.272180
1764.074043	156.150200	48.277185
1761.164388	151.908611	48.282189
1757.321572	169.189644	48.287194
1754.195383	159.372293	48.292199
1750.508331	157.728044	48.297204
1747.022874	165.816804	48.302209
1743.764275	151.191270	48.307213
1740.034229	164.271279	48.312218
1736.498896	160.758040	48.317223
1732.890904	165.060974	48.322228
1729.017599	159.050601	48.327233
1726.138079	157.219879	48.332237
1722.276531	167.342006	48.337242
1719.274465	155.385942	48.342247
1715.656468	160.777878	48.347252
1711.951176	158.216481	48.352257
1708.375859	165.883992	48.357261
1705.047512	164.596508	48.362266
1701.601869	159.757951	48.367271
1697.561667	162.452172	48.372276
1694.482550	154.585091	48.377281
1690.776204	150.801965	48.382285
1686.857584	154.422939	48.387290
1683.688462	158.605644	48.392295
1680.470967	152.428950	48.397300
1677.061624	156.395990	48.402305
1674.045463	159.236587	48.407309
1669.948252	155.783081	48.412314
1666.585556	146.942240	48.417319
1662.716260	160.584235	48.422324
1659.275205	161.238473	48.427329
1656.111134	144.155137	48.432333
1652.183283	158.453293	48.437338
1648.807788	152.727006	48.442343
1645.467057	158.845564	48.447348
1641.993544	149.125358	48.452353
1638.302820	148.975660	48.457357
1634.762930	155.596007	48.462362
1631.622663	151.360836	48.467367
1628.085778	155.620323	48.472372
1624.180094	151.921891	48.477377
1621.087659	150.832099	48.482381
1617.456276	161.852047	48.487386
1614.023830	153.154987	48.492391
1610.267546	154.940788	48.497396
1607.020422	154.056537	48.502401
1603.376692	157.840942	48.507405
1599.444298	157.639838	48.512410
1596.393522	146.518379	48.517415
1592.832759	151.909625	48.522420
1589.525303	154.498253	48.527425
1585.621205	155.336802	48.532429
1581.893644	150.812911	48.537434
1578.965781	145.147302	48.542439
1575.353999	158.095586	48.547444
1571.727205	149.111778	48.552449
1568.514864	141.714769	48.557453
1564.890720	154.762585	48.562458
1561.700001	152.395322	48.567463
1557.893489	151.146108	48.572468
1554.258070	146.812643	48.577473
1550.922025	149.546921	48.582477
1547.089282	146.385500	48.587482
1543.974837	141.335067	48.592487
1540.323918	152.768950	48.597492
1536.578945	148.993717	48.602497
1533.157582	149.963889	48.607501
1529.483468	155.319842	48.612506
1526.147340	147.886287	48.617511
1522.801939	145.369179	48.622516
1519.282394	143.889843	48.627521
1515.672767	150.573102	48.632525
1512.132953	150.597286	48.637530
1508.767924	154.153758	48.642535
1505.431642	149.023382	48.647540
1501.822314	154.221434	48.652545
1498.324074	150.050448	48.657549
1494.645794	157.187107	48.662554
1491.621333	152.506056	48.667559
1488.166171	145.374990	48.672564
1484.308553	147.668218	48.677569
1480.752625	148.620606	48.682573
1477.009083	149.419884	48.687578
1473.798829	138.627597	48.692583
1470.680790	151.085068	48.697588
1466.326520	140.871983	48.702593
1462.954349	146.549473	48.707597
1459.723185	149.124594	48.712602
1456.485466	143.671897	48.717607
1452.632933	150.724504	48.722612
1449.234582	147.832773	48.727617
1445.885991	154.396967	48.732621
1442.085276	155.747614	48.737626
1438.617535	143.208836	48.742631
1434.993432	149.127293	48.747636
1431.801513	154.261542	48.752641
1428.104040	145.441099	48.757645
1424.368455	146.549320	48.762650
1421.339414	145.355846	48.767655
1417.816470	144.406805	48.772660
1414.214489	151.390010	48.777665
1410.780396	143.175692	48.782669
1407.391997	146.375164	48.787674
1403.806641	141.451207	48.792679
1400.326009	142.515534	48.797684
1396.469501	143.510954	48.802689
1393.135730	147.306249	48.807693
1389.526307	142.631572	48.812698
1386.451290	141.877298	48.817703
1382.651223	136.893138	48.822708
1379.302132	138.596230	48.827713
1375.558561	138.598744	48.832717
1371.931406	141.918215	48.837722
1368.629568	140.616533	48.842727
1365.168185	139.555927	48.847732
1361.548505	137.745358	48.852737
1358.212702	132.551874	48.857741
1354.544324	141.606694	48.862746
1351.254815	134.267210	48.867751
1347.593766	140.243338	48.872756
1344.096888	136.165991	48.877761
1340.934249	133.594147	48.882765
1336.962319	145.295331	48.887770
1333.760568	141.225253	48.892775
1330.085572	137.310363	48.897780
1326.327519	138.021583	48.902785
1323.115739	135.266062	48.907789
1319.641960	141.754528	48.912794
1316.499392	132.933839	48.917799
1312.268324	139.019211	48.922804
1308.755428	134.735164	48.927809
1305.582309	129.504571	48.932813
1302.236124	137.832457	48.937818
1298.649051	131.201311	48.942823
1295.436073	132.138592	48.947828
1291.420050	128.049816	48.952833
1288.066055	128.085292	48.957837
1284.372045	131.537044	48.962842
1281.259540	126.075630	48.967847
1277.933118	135.652766	48.972852
1274.505767	140.971467	48.977857
1270.921510	130.753463	48.982861
1266.849600	135.794103	48.987866
1263.221069	129.149319	48.992871
1259.713532	136.631869	48.997876
1256.061767	133.618588	49.002881
1253.346302	135.584273	49.007885
1249.670704	143.930142	49.012890
1246.300597	126.748827	49.017895
1242.635742	146.719467	49.022900
1239.067774	143.690372	49.027905
1235.776607	137.246969	49.032909
1232.105597	140.636943	49.037914
1228.731517	135.931589	49.042919
1224.901077	140.186412	49.047924
1221.109075	140.718622	49.052929
1217.903856	131.118820	49.057933
1214.400168	134.675524	49.062938
1211.020227	123.990843	49.067943
1207.440385	125.587357	49.072948
1204.114645	134.032893	49.077953
1200.838140	141.426971	49.082957
1197.130910	141.889142	49.087962
1193.633077	137.594016	49.092967
1190.088001	137.083547	49.097972
1186.193329	142.248090	49.102977
1182.960183	145.985650	49.107981
1179.469111	138.384012	49.112986
1176.141604	134.204798	49.117991
1172.447540	130.617422	49.122996
1168.671685	141.673777	49.128001
1165.468008	130.202214	49.133005
1161.839987	135.957524	49.138010
1158.434996	141.169402	49.143015
1154.734611	141.522335	49.148020
1151.057742	137.891283	49.153025
1148.533689	132.637761	49.158029
1144.635012	147.736574	49.163034
1141.281423	135.643531	49.168039
1137.671422	141.221042	49.173044
1133.757164	131.389444	49.178049
1130.243036	142.086025	49.183053
1126.622595	129.641853	49.188058
1123.323600	132.412530	49.193063
1120.063613	133.107876	49.198068
1116.177960	143.328347	49.203073
1113.174878	132.281088	49.208077
1109.583364	138.293256	49.213082
1106.212000	131.377373	49.218087
1102.171633	134.995266	49.223092
1098.868197	139.311255	49.228097
1095.503341	133.135503	49.233101
1091.848342	136.173454	49.238106
1088.266142	127.276647	49.243111
1085.041797	131.225346	49.248116
1081.324612	137.394279	49.253121
1078.236389	130.336684	49.258125
1074.587119	136.486893	49.263130
1071.185077	129.866790	49.268135
1067.108790	131.875249	49.273140
1063.630402	132.698312	49.278145
1060.469565	134.191914	49.283149
1056.407815	146.781969	49.288154
1053.590469	132.788978	49.293159
1049.954040	132.227617	49.298164
1046.599015	135.952858	49.303169
1042.914429	132.049075	49.308173
1038.988871	140.974564	49.313178
1035.748471	131.538202	49.318183
1032.171851	135.355745	49.323188
1028.590907	135.948529	49.328193
1025.554707	124.602527	49.333197
1021.648809	141.937457	49.338202
1018.687898	131.791446	49.343207
1014.901548	136.678123	49.348212
1011.131943	145.009714	49.353217
1008.010024	136.450678	49.358221
1004.278134	140.980651	49.363226
1000.896885	130.216047	49.368231
997.382312	134.148664	49.373236
994.201559	139.239115	49.378241
990.626500	134.165802	49.383245
986.439785	139.550284	49.388250
982.940662	132.321143	49.393255
979.426060	129.524783	49.398260
976.416997	133.062620	49.403265
973.138813	128.373188	49.408269
969.402572	136.832887	49.413274
966.127784	130.409490	49.418279
962.301628	126.123661	49.423284
958.366657	130.402099	49.428289
955.344184	129.812300	49.433293
951.815458	128.519440	49.438298
948.231292	125.529972	49.443303
944.783405	133.725326	49.448308
941.125703	130.539043	49.453313
938.134092	123.724882	49.458317
934.299307	127.969406	49.463322
930.781550	125.474942	49.468327
926.952697	131.897880	49.473332
923.347039	136.049070	49.478337
920.246471	128.337888	49.483341
916.910721	139.675068	49.488346
913.507096	128.801365	49.493351
910.005927	125.576988	49.498356
905.707165	130.447260	49.503361
902.231840	131.833139	49.508365
899.248001	132.073894	49.513370
895.865940	134.987133	49.518375
892.513305	129.395421	49.523380
888.882345	130.542027	49.528385
885.642085	130.127219	49.533389
882.050024	130.615001	49.538394
877.846306	132.891770	49.543399
874.387178	132.893831	49.548404
870.955182	137.023246	49.553409
868.070554	124.583920	49.558413
864.376289	129.902650	49.563418
860.513870	128.818384	49.568423
856.945719	130.553150	49.573428
853.356779	128.565442	49.578433
850.387704	117.486136	49.583437
846.705361	127.625419	49.588442
843.559488	122.516179	49.593447
840.071535	128.031687	49.598452
835.889649	119.783288	49.603457
833.103275	121.369428	49.608461
828.978112	120.721546	49.613466
825.630870	123.982703	49.618471
821.891949	130.552862	49.623476
818.702337	131.213894	49.628481
815.002172	121.350756	49.633485
811.536657	126.482109	49.638490
808.187954	121.060711	49.643495
804.539186	127.101711	49.648500
801.030075	124.586584	49.653505
797.449189	119.830933	49.658509
794.008486	135.733957	49.663514
790.883593	122.420766	49.668519
787.407717	128.237819	49.673524
783.754442	129.399448	49.678529
780.327290	124.052223	49.683533
776.441203	122.940768	49.688538
773.036924	116.382069	49.693543
769.592092	128.828846	49.698548
766.224411	128.336732	49.703553
762.600173	123.089019	49.708557
758.899243	121.478871	49.713562
755.252676	133.278614	49.718567
752.109307	125.897684	49.723572
748.546752	133.243465	49.728577
745.190040	119.793033	49.733581
741.852382	125.397613	49.738586
738.160288	113.310026	49.743591
734.494923	123.433160	49.748596
731.012557	117.345233	49.753601
727.515861	118.309719	49.758605
723.858812	130.932332	49.763610
720.207993	125.726942	49.768615
717.120984	123.770180	49.773620
713.503702	127.817482	49.778625
709.782826	121.415204	49.783629
706.313612	125.670874	49.788634
703.080764	124.424386	49.793639
699.502604	123.388750	49.798644
696.036648	129.596138	49.803649
692.877548	117.179076	49.808653
689.295135	127.556110	49.813658
685.866878	122.193162	49.818663
682.041349	120.906801	49.823668
678.463034	122.523407	49.828673
674.871880	122.688365	49.833677
671.160663	122.952122	49.838682
667.776023	121.347151	49.843687
664.654793	120.668117	49.848692
661.227221	131.684580	49.853697
658.086196	126.846214	49.858701
653.913671	128.005249	49.863706
650.170368	128.314589	49.868711
646.373496	126.338563	49.873716
643.354777	129.557933	49.878721
640.044839	128.347334	49.883725
636.744310	125.486042	49.888730
633.326617	124.448974	49.893735
629.659924	129.804371	49.898740
625.548983	130.907660	49.903745
622.977976	122.074269	49.908749
619.231790	127.918603	49.913754
615.363913	123.246110	49.918759
611.931752	120.230001	49.923764
608.189937	125.903713	49.928769
605.025129	120.382792	49.933773
600.921046	119.673818	49.938778
597.862453	131.581224	49.943783
594.553399	128.256056	49.948788
590.848423	125.823434	49.953793
587.493854	120.307283	49.958797
584.350663	120.605992	49.963802
580.887354	115.040943	49.968807
576.906204	129.200262	49.973812
573.471316	134.190167	49.978817
569.678528	121.025562	49.983821
566.305201	123.705925	49.988826
562.980031	123.905701	49.993831
559.367095	120.115993	49.998836
555.634246	122.736067	50.003841
552.201414	121.560671	50.008845
548.848059	125.115098	50.013850
545.353680	120.728972	50.018855
541.932031	116.062440	50.023860
538.351076	121.551326	50.028865
535.427268	113.809234	50.033869
531.148670	126.413265	50.038874
527.840947	122.677669	50.043879
524.363812	126.946429	50.048884
520.643727	126.113606	50.053889
517.344986	121.252902	50.058893
513.737702	123.324360	50.063898
510.377946	119.109970	50.068903
506.854067	118.763686	50.073908
502.947522	121.979097	50.078913
499.787092	114.175347	50.083917
496.384946	116.421260	50.088922
492.863747	114.527431	50.093927
489.676763	115.023687	50.098932
485.774427	124.309255	50.103937
482.407489	111.446257	50.108941
478.746705	116.355798	50.113946
475.299540	120.615490	50.118951
471.946406	123.041569	50.123956
468.337628	130.570635	50.128961
465.093960	121.173186	50.133965
461.404972	124.182527	50.138970
458.040947	120.606281	50.143975
454.184722	112.217564	50.148980
450.823473	119.707452	50.153985
447.632922	115.405518	50.158989
443.401312	122.420995	50.163994
439.738289	117.712203	50.168999
436.710610	118.798216	50.174004
433.489083	122.092529	50.179009
430.391295	114.701162	50.184013
426.174953	115.402148	50.189018
422.534721	114.524228	50.194023
419.538582	112.492261	50.199028
415.417421	117.718593	50.204033
412.107880	111.119660	50.209037
408.527536	114.940662	50.214042
405.273704	110.473212	50.219047
401.563164	111.071176	50.224052
398.049376	110.006194	50.229057
394.897211	115.494673	50.234061
391.186883	112.425524	50.239066
387.609713	110.814160	50.244071
384.418476	113.967331	50.249076
380.859049	120.600084	50.254081
377.603944	113.088373	50.259085
373.903888	119.362363	50.264090
370.200351	117.579721	50.269095
366.508002	115.941655	50.274100
362.770356	120.599778	50.279105
360.139130	118.446678	50.284109
356.445694	120.703809	50.289114
352.610895	124.449359	50.294119
349.403146	116.132201	50.299124
345.831805	126.379378	50.304129
342.413449	106.057846	50.309133
338.593525	116.721694	50.314138
335.404902	114.247645	50.319143
331.874470	111.304472	50.324148
327.887683	111.443042	50.329153
324.759517	115.814822	50.334157
321.184570	116.127955	50.339162
317.443399	110.165909	50.344167
313.993179	104.240961	50.349172
310.592558	115.485451	50.354177
307.166611	116.857107	50.359181
303.679487	107.608240	50.364186
300.209613	112.830475	50.369191
296.642239	108.207612	50.374196
292.930492	110.500188	50.379201
289.720670	109.894503	50.384205
286.155511	113.931144	50.389210
282.581836	105.050446	50.394215
279.242591	110.836962	50.399220
275.568502	108.502518	50.404225
272.089976	114.248948	50.409229
268.237120	117.633671	50.414234
264.609982	118.940983	50.419239
261.602908	109.956844	50.424244
258.303015	118.834633	50.429249
254.947736	113.300724	50.434253
251.053271	118.216173	50.439258
247.367056	107.643831	50.444263
243.907650	122.574652	50.449268
240.849363	115.721938	50.454273
237.480637	104.996805	50.459277
233.661431	114.262692	50.464282
230.161308	110.174188	50.469287
226.644660	116.830364	50.474292
223.077684	116.324897	50.479297
219.444944	109.167100	50.484301
215.796723	111.183613	50.489306
212.619523	105.580797	50.494311
209.169478	104.828655	50.499316
205.452543	110.810554	50.504321
202.224659	106.456783	50.509325
198.449273	110.994202	50.514330
195.016045	103.114308	50.519335
191.740333	103.533513	50.524340
188.142111	109.558723	50.529345
184.743007	105.961279	50.534349
180.758653	112.555202	50.539354
177.579701	112.194317	50.544359
174.237592	108.141864	50.549364
170.390002	105.602789	50.554369
167.104874	105.965949	50.559373
163.661746	113.243050	50.564378
160.000226	106.819425	50.569383
156.655178	106.622807	50.574388
152.748187	108.635246	50.579393
149.670571	105.392303	50.584397
146.172749	106.823543	50.589402
142.589396	117.841667	50.594407
138.817078	108.211949	50.599412
135.444876	112.523224	50.604417
131.879954	108.270893	50.609421
128.378911	107.618626	50.614426
124.615682	106.603260	50.619431
121.301268	120.851649	50.624436
117.890003	125.385687	50.629441
114.608332	122.044336	50.634445
110.924242	114.797063	50.639450
107.627292	118.496792	50.644455
104.217907	115.320256	50.649460
99.718699	118.305777	50.654465
96.540672	116.113532	50.659469
93.396199	117.854933	50.664474
89.960992	109.465545	50.669479
86.806178	113.949644	50.674484
82.976769	110.517067	50.679489
79.810425	106.445261	50.684493
76.162615	113.158983	50.689498
72.213017	111.218236	50.694503
69.166571	108.197128	50.699508
65.146505	123.590506	50.704513
61.940660	117.846325	50.709517
58.336818	110.315073	50.714522
54.877647	114.212198	50.719527
51.483958	114.272951	50.724532
47.811551	115.374818	50.729537
44.412416	109.514461	50.734541
40.777334	107.683680	50.739546
37.314808	119.762875	50.744551
33.930198	102.122789	50.749556
30.294700	119.482495	50.754561
27.184336	107.841170	50.759565
23.498407	112.007931	50.764570
19.901770	112.057914	50.769575
16.222014	109.987883	50.774580
12.422429	113.161147	50.779585
9.278339	109.969178	50.784589
6.005921	111.766165	50.789594
2.516530	105.215912	50.794599