Tue Jun 21 13:10:02 2022

Number of Points = 9930

Depth (nm)	Load (N)	Time (s)
0.012082	103.379416	0.000000
0.031683	110.131559	0.005005
0.047738	100.842968	0.010010
-0.097659	88.173548	0.015014
-0.294819	78.509229	0.020019
-0.332944	71.413525	0.025024
-0.706063	57.976123	0.030029
-1.365957	45.680042	0.035034
-0.981574	26.740482	0.040038
-1.962502	5.813145	0.045043
-2.354873	8.129529	0.050048
-2.507257	-5.455072	0.055053
-3.098068	-2.566124	0.060058
-3.092708	-14.185944	0.065062
-3.834593	-5.785136	0.070067
-4.292656	5.946234	0.075072
-4.800574	-2.018646	0.080077
-4.772204	1.673730	0.085082
-4.919233	1.070594	0.090086
-4.855104	-1.160776	0.095091
-5.137386	1.506983	0.100096
-4.852534	-3.742048	0.105101
-5.663532	-5.663731	0.110106
-6.381000	-0.684968	0.115110
-6.655272	-1.842063	0.120115
-6.801324	0.871809	0.125120
-6.608653	-9.165241	0.130125
-6.708443	-5.598263	0.135130
-6.790293	-10.997913	0.140134
-7.528089	-8.448113	0.145139
-8.454977	-1.900211	0.150144
-8.161144	2.564178	0.155149
-8.155284	5.845882	0.160154
-8.092273	2.111413	0.165158
-8.029829	-9.711446	0.170163
-9.037131	2.033318	0.175168
-9.384813	-6.770907	0.180173
-9.962711	1.836196	0.185178
-9.592544	-0.385665	0.190182
-9.702999	-1.749459	0.195187
-9.971263	0.463692	0.200192
-10.847026	-2.679414	0.205197
-11.164454	-1.074000	0.210202
-11.317743	3.023587	0.215206
-11.560186	-0.327597	0.220211
-11.652578	4.498721	0.225216
-11.328519	5.340792	0.230221
-11.861601	-2.813108	0.235226
-11.437275	-3.371933	0.240230
-12.155735	1.228510	0.245235
-12.715776	2.925998	0.250240
-12.481587	0.279695	0.255245
-13.309951	4.911757	0.260250
-13.767132	-4.148432	0.265254
-13.951888	-5.418029	0.270259
-14.212520	1.538534	0.275264
-14.201736	-3.597822	0.280269
-14.270291	2.820973	0.285274
-14.476871	-0.214891	0.290278
-15.221629	-4.003064	0.295283
-15.807500	0.735658	0.300288
-15.616171	-7.283242	0.305293
-16.000234	-4.084774	0.310298
-16.032548	3.667714	0.315302
-16.091623	2.755790	0.320307
-16.076135	2.314788	0.325312
-16.593218	0.301812	0.330317
-17.265708	-0.164385	0.335322
-17.194582	-1.819319	0.340326
-17.230439	-1.161159	0.345331
-17.420939	3.401981	0.350336
-17.857251	-3.707473	0.355341
-18.678377	-2.332014	0.360346
-18.897204	-0.544804	0.365350
-18.863494	-3.031221	0.370355
-19.088323	2.098424	0.375360
-19.042634	-2.877953	0.380365
-19.361820	1.734518	0.385370
-19.345100	7.734661	0.390374
-19.983369	-3.342083	0.395379
-20.796078	2.551108	0.400384
-20.680138	-5.330989	0.405389
-20.959149	0.409494	0.410394
-20.796833	5.025506	0.415398
-20.643885	-1.410151	0.420403
-21.615093	7.848560	0.425408
-21.817717	-0.529571	0.430413
-22.388407	0.735155	0.435418
-22.422940	-1.567493	0.440422
-22.320701	-0.196740	0.445427
-22.416693	1.144087	0.450432
-23.135812	-1.175436	0.455437
-23.544559	-4.651223	0.460442
-23.871469	-3.659522	0.465446
-23.934031	1.993417	0.470451
-24.313035	0.430584	0.475456
-23.768077	-10.714218	0.480461
-24.199844	-1.996536	0.485466
-24.623096	-5.858667	0.490470
-24.857182	-12.575364	0.495475
-25.239622	-3.176765	0.500480
-25.474892	-8.098721	0.505485
-25.762131	4.368236	0.510490
-26.179825	4.872560	0.515494
-26.477277	-2.653962	0.520499
-27.065136	3.239292	0.525504
-26.892679	0.149740	0.530509
-27.033250	1.294301	0.535514
-26.923228	-4.656898	0.540518
-27.062670	-5.861181	0.545523
-27.510889	8.942417	0.550528
-28.130384	-0.814909	0.555533
-28.537904	1.539702	0.560538
-28.575492	0.030840	0.565542
-28.461843	-8.861615	0.570547
-28.817423	-1.163539	0.575552
-29.511837	-11.796648	0.580557
-30.098596	-1.802604	0.585562
-30.348674	-4.726676	0.590566
-30.105397	-7.441182	0.595571
-30.403044	-3.477163	0.600576
-30.347673	-3.637058	0.605581
-30.386669	7.214864	0.610586
-30.905056	-2.022852	0.615590
-31.510344	-4.848833	0.620595
-31.723815	-5.399328	0.625600
-31.830705	-7.349987	0.630605
-32.087202	-7.894936	0.635610
-32.039970	-8.504586	0.640614
-32.093313	-1.477567	0.645619
-32.733688	-1.301038	0.650624
-33.335777	-5.767584	0.655629
-33.779784	1.082396	0.660634
-33.508423	-8.082842	0.665638
-33.482582	-5.999301	0.670643
-33.930130	-1.452006	0.675648
-34.188188	-10.491290	0.680653
-34.787160	-5.294363	0.685658
-34.976957	-9.117006	0.690662
-35.079006	-4.977784	0.695667
-35.333323	-3.386964	0.700672
-35.361545	1.046690	0.705677
-35.765132	4.178537	0.710682
-36.324661	-0.532449	0.715686
-36.563242	-4.247559	0.720691
-36.995741	-0.443545	0.725696
-36.753195	2.090142	0.730701
-36.882796	-3.148272	0.735706
-37.028798	-2.388795	0.740710
-36.787855	1.295609	0.745715
-38.092452	3.631634	0.750720
-38.296722	-7.332662	0.755725
-38.530454	5.254489	0.760730
-38.730903	3.518234	0.765734
-38.719070	10.848620	0.770739
-38.876030	6.805836	0.775744
-39.172868	1.897428	0.780749
-39.503638	8.463444	0.785754
-39.887070	8.868955	0.790758
-39.530115	0.046514	0.795763
-40.071695	10.015916	0.800768
-40.552634	-0.957625	0.805773
-41.076135	-2.719710	0.810778
-41.154312	-2.153800	0.815782
-41.062806	-2.750852	0.820787
-41.307298	0.582175	0.825792
-41.591115	-5.195665	0.830797
-42.868039	-3.195742	0.835802
-43.007840	1.915679	0.840806
-42.900342	-6.617796	0.845811
-42.813493	3.035204	0.850816
-42.700965	-6.090313	0.855821
-43.146638	4.279181	0.860826
-43.050795	-3.210052	0.865830
-43.972258	-9.698465	0.870835
-44.620651	8.445581	0.875840
-44.542594	-3.089983	0.880845
-44.641289	6.199671	0.885850
-45.067842	11.890197	0.890854
-44.713261	3.773613	0.895859
-44.647773	11.921149	0.900864
-44.849175	2.055124	0.905869
-45.637235	4.331661	0.910874
-46.123595	1.274248	0.915878
-46.467746	-7.970213	0.920883
-47.370130	-1.802874	0.925888
-46.928637	-4.543497	0.930893
-46.819814	-1.030009	0.935898
-47.656474	3.964551	0.940902
-47.711836	4.153921	0.945907
-48.459959	11.755392	0.950912
-48.204916	1.401353	0.955917
-48.222495	6.645666	0.960922
-48.456792	3.175328	0.965926
-48.113181	-4.306786	0.970931
-49.119740	-0.356991	0.975936
-49.034416	0.738520	0.980941
-49.184126	0.741840	0.985946
-49.734402	4.764075	0.990950
-50.355563	-7.776940	0.995955
-51.151498	-0.239188	1.000960
-51.277616	-4.029556	1.005965
-51.027514	0.123969	1.010970
-51.037453	2.101745	1.015974
-51.049356	0.024454	1.020979
-51.280682	8.352565	1.025984
-50.997852	-1.297647	1.030989
-51.921285	-1.862192	1.035994
-52.284547	0.614740	1.040998
-52.192952	0.513768	1.046003
-53.144351	-4.632559	1.051008
-53.512306	-9.738949	1.056013
-53.963377	0.865277	1.061018
-53.762032	3.167408	1.066022
-54.059810	-7.943609	1.071027
-54.448263	7.786434	1.076032
-54.141740	1.208129	1.081037
-54.385001	3.024448	1.086042
-54.251594	4.427926	1.091046
-54.897492	4.791853	1.096051
-55.535959	-3.222042	1.101056
-55.484763	3.570205	1.106061
-55.704095	-1.154688	1.111066
-55.884174	7.172237	1.116070
-56.549750	1.259099	1.121075
-57.330718	-2.335800	1.126080
-57.198240	-4.961116	1.131085
-57.222788	7.011433	1.136090
-57.411470	6.330146	1.141094
-57.442173	0.150454	1.146099
-57.786152	3.140811	1.151104
-57.518767	-3.571315	1.156109
-58.184723	3.561693	1.161114
-58.834002	-7.221359	1.166118
-58.981198	-1.429495	1.171123
-59.118631	5.225073	1.176128
-59.021660	0.167586	1.181133
-59.338414	-1.347140	1.186138
-60.211041	6.162665	1.191142
-60.843726	0.918172	1.196147
-60.922443	4.871986	1.201152
-61.174995	3.209283	1.206157
-61.016063	2.667763	1.211162
-61.131272	-1.664512	1.216166
-60.875336	2.892777	1.221171
-61.077239	6.276373	1.226176
-61.370633	0.681666	1.231181
-62.340658	11.055909	1.236186
-62.390455	4.097939	1.241190
-62.172380	-0.114495	1.246195
-62.591444	6.115284	1.251200
-63.046666	-5.069115	1.256205
-63.638587	1.738662	1.261210
-64.119290	9.358798	1.266214
-64.001899	2.111083	1.271219
-64.024883	1.489380	1.276224
-63.901775	-3.238744	1.281229
-64.462139	2.721789	1.286234
-65.191444	10.357638	1.291238
-65.566854	13.712546	1.296243
-65.829718	8.515932	1.301248
-65.751979	0.005933	1.306253
-65.612562	4.108524	1.311258
-65.435498	5.161412	1.316262
-66.091656	-2.184933	1.321267
-66.909631	6.590989	1.326272
-67.245528	-4.232712	1.331277
-67.272841	3.303851	1.336282
-67.243422	1.236294	1.341286
-67.317915	4.543340	1.346291
-67.625880	8.266154	1.351296
-68.067641	0.666842	1.356301
-68.544355	0.664129	1.361306
-68.989702	0.738707	1.366310
-68.766747	0.300446	1.371315
-68.767894	-1.139069	1.376320
-68.880046	-3.386237	1.381325
-69.918535	-1.346859	1.386330
-70.479710	-2.752237	1.391334
-70.349278	-3.250557	1.396339
-70.857586	10.124631	1.401344
-70.477577	-1.778445	1.406349
-70.651745	-1.108232	1.411354
-70.864715	9.156819	1.416358
-71.382979	1.520251	1.421363
-71.736706	1.752915	1.426368
-71.949368	-1.224711	1.431373
-72.053764	8.420099	1.436378
-72.142205	4.431684	1.441382
-72.558618	-2.899701	1.446387
-73.719800	8.094645	1.451392
-73.878367	2.064197	1.456397
-73.109331	2.251426	1.461402
-73.506789	3.261128	1.466406
-73.372649	2.250904	1.471411
-73.885805	5.096020	1.476416
-74.348175	-1.280359	1.481421
-75.382870	7.200922	1.486426
-75.615819	4.301247	1.491430
-74.826570	-4.105172	1.496435
-75.267637	0.688902	1.501440
-75.273639	-2.657821	1.506445
-75.449729	1.890500	1.511450
-76.160937	-0.251737	1.516454
-76.844054	0.728313	1.521459
-77.044404	4.662408	1.526464
-76.944319	2.219069	1.531469
-77.016288	6.179658	1.536474
-77.334874	-4.007154	1.541478
-77.248305	-1.625437	1.546483
-77.909913	3.828339	1.551488
-78.215183	6.370458	1.556493
-78.195813	2.275784	1.561498
-78.560741	3.209257	1.566502
-78.581826	2.909682	1.571507
-79.131326	8.775672	1.576512
-79.401875	-2.314397	1.581517
-79.657486	4.213912	1.586522
-80.106196	5.274529	1.591526
-80.205202	3.246197	1.596531
-80.245870	6.743001	1.601536
-80.785710	-1.700437	1.606541
-81.247381	-6.232654	1.611546
-81.944862	6.001504	1.616550
-81.715436	-0.115100	1.621555
-81.768684	5.192541	1.626560
-81.642886	-0.755547	1.631565
-81.888393	0.050800	1.636570
-82.086700	1.536838	1.641574
-82.276979	-5.626965	1.646579
-83.449701	6.662613	1.651584
-83.279712	-11.619786	1.656589
-83.178561	-5.782819	1.661594
-83.296629	1.906511	1.666598
-83.439212	-4.369694	1.671603
-84.583283	-3.216612	1.676608
-84.924893	-5.968838	1.681613
-85.248605	-4.533072	1.686618
-85.395839	-2.481648	1.691622
-85.097488	-5.387218	1.696627
-85.397398	5.983085	1.701632
-85.260050	2.015294	1.706637
-85.443207	-3.155047	1.711642
-85.965997	-4.504423	1.716646
-86.724502	-4.235902	1.721651
-87.055742	-4.485296	1.726656
-86.976443	-3.873636	1.731661
-87.039287	-4.148337	1.736666
-87.335452	5.386938	1.741670
-87.382994	0.455011	1.746675
-88.139034	4.665641	1.751680
-88.693689	5.291714	1.756685
-88.700289	5.088210	1.761690
-88.959541	4.056308	1.766694
-88.643353	2.546085	1.771699
-88.950831	8.781263	1.776704
-88.921684	-3.739767	1.781709
-89.529975	6.286858	1.786714
-90.060704	-4.735452	1.791718
-90.031235	-4.969202	1.796723
-90.127734	7.740260	1.801728
-90.325236	2.270374	1.806733
-90.942516	3.564727	1.811738
-91.355166	3.378741	1.816742
-91.177787	-0.877470	1.821747
-91.789422	-2.702504	1.826752
-92.421901	-5.202319	1.831757
-92.695507	-4.281010	1.836762
-92.640926	1.197817	1.841766
-92.759615	-1.980073	1.846771
-92.702076	-3.220331	1.851776
-93.052605	0.859797	1.856781
-93.446221	-2.605068	1.861786
-93.527368	4.093457	1.866790
-93.330896	0.291304	1.871795
-94.276664	4.853035	1.876800
-94.379003	-9.681507	1.881805
-94.744283	2.378838	1.886810
-95.006246	-5.389757	1.891814
-95.454385	-9.284262	1.896819
-96.073880	2.101669	1.901824
-96.315699	1.505552	1.906829
-96.199535	-9.347028	1.911834
-96.119416	-6.790592	1.916838
-96.351600	-4.737136	1.921843
-96.427743	0.450764	1.926848
-96.273077	-9.006734	1.931853
-97.094381	1.838577	1.936858
-97.788883	-1.522388	1.941862
-97.741461	-3.405854	1.946867
-98.283881	8.116302	1.951872
-97.938731	4.539152	1.956877
-98.178643	-2.135925	1.961882
-99.163266	1.927660	1.966886
-99.304440	-8.060805	1.971891
-99.649579	4.162360	1.976896
-99.673037	-1.482177	1.981901
-99.454362	1.629500	1.986906
-99.854719	5.526469	1.991910
-99.677130	-5.130468	1.996915
-100.165521	1.749518	2.006912
-100.461703	-5.511826	2.016909
-99.936199	-0.881427	2.026906
-99.211134	-0.864507	2.036902
-98.322652	2.613724	2.046899
-98.414952	2.734199	2.056896
-97.810332	1.357934	2.066893
-97.174066	8.324621	2.076890
-96.952496	1.101809	2.086886
-95.810486	5.211228	2.096883
-95.752883	10.714798	2.106880
-95.576075	4.153209	2.116877
-94.221427	-2.071541	2.126874
-93.924929	1.595224	2.136870
-93.788693	2.458315	2.146867
-93.558985	-4.936162	2.156864
-92.551183	0.102204	2.166861
-92.223105	1.341142	2.176858
-91.849474	-10.148221	2.186854
-91.281578	-7.978460	2.196851
-90.671745	-7.940281	2.206848
-89.736581	-0.922724	2.216845
-89.685946	-4.048147	2.226842
-89.461824	-8.087879	2.236838
-88.808576	-12.090005	2.246835
-88.295962	-8.343642	2.256832
-87.539436	-6.983014	2.266829
-86.949567	-9.299119	2.276826
-86.598981	-6.324168	2.286822
-86.320096	-15.290673	2.296819
-85.478942	-8.766727	2.306816
-85.189334	-4.232606	2.316813
-84.931110	-8.117151	2.326810
-84.090676	-7.208662	2.336806
-83.570953	-3.655923	2.346803
-83.321403	-3.351798	2.356800
-82.462008	-6.531333	2.366797
-82.068147	-7.380111	2.376794
-81.908576	-1.237644	2.386790
-80.954165	-6.356411	2.396787
-80.543710	-0.676349	2.406784
-80.337703	-1.560208	2.416781
-79.449840	-5.309355	2.426778
-78.924166	1.721883	2.436774
-78.909486	-4.814829	2.446771
-77.851240	-5.385971	2.456768
-77.486240	-1.831713	2.466765
-77.306934	-3.513940	2.476762
-76.896552	-3.467624	2.486758
-75.990659	5.473936	2.496755
-75.619204	0.533906	2.506752
-75.308260	1.555375	2.516749
-74.417138	-5.173508	2.526746
-74.120279	0.239264	2.536742
-73.723121	-0.457128	2.546739
-72.674220	-8.572120	2.556736
-72.536545	-3.465722	2.566733
-72.354587	-2.761554	2.576730
-71.847267	-0.194687	2.586726
-70.990121	-4.996422	2.596723
-70.831219	1.215116	2.606720
-70.014098	0.127704	2.616717
-69.244243	2.207712	2.626714
-69.513590	2.504313	2.636710
-68.397021	4.817750	2.646707
-68.001145	1.286018	2.656704
-67.875634	4.674846	2.666701
-67.138811	0.840460	2.676698
-66.498402	-4.051046	2.686694
-66.109321	-3.998238	2.696691
-65.313417	-3.613284	2.706688
-64.983574	-0.488878	2.716685
-64.962467	-0.449029	2.726682
-64.164964	-7.276610	2.736678
-63.533869	-7.316438	2.746675
-63.458691	2.285309	2.756672
-62.174485	-3.341925	2.766669
-61.921646	0.664215	2.776666
-61.771860	-1.370754	2.786662
-61.133505	0.398101	2.796659
-60.380726	2.501093	2.806656
-60.186294	0.319631	2.816653
-59.841292	-4.154852	2.826650
-58.679506	-1.797134	2.836646
-58.619765	-10.708976	2.846643
-58.460685	1.330123	2.856640
-57.650653	-0.122437	2.866637
-57.316170	-0.808448	2.876634
-56.006512	2.735392	2.886630
-55.659453	-4.203721	2.896627
-55.620092	4.649775	2.906624
-55.416264	4.555633	2.916621
-54.867778	0.489451	2.926618
-54.119020	2.329926	2.936614
-53.352304	3.198862	2.946611
-52.605629	-2.351407	2.956608
-52.361811	6.067726	2.966605
-52.414434	2.976195	2.976602
-51.904409	0.256409	2.986598
-50.963607	6.735219	2.996595
-50.731304	4.774116	3.006592
-49.747518	5.639312	3.016589
-49.668757	6.303074	3.026586
-49.082475	-0.295896	3.036582
-48.438443	-0.017182	3.046579
-47.952164	-1.290857	3.056576
-47.482780	0.322030	3.066573
-47.403371	-5.112600	3.076570
-46.307253	-1.343319	3.086566
-45.972074	2.709649	3.096563
-45.783775	-4.871407	3.106560
-45.135394	-7.643938	3.116557
-44.932902	-5.695613	3.126554
-43.595499	-4.694353	3.136550
-43.134625	-3.285942	3.146547
-43.016283	0.756897	3.156544
-42.758803	-4.143708	3.166541
-42.270347	-1.333646	3.176538
-41.692691	-5.381341	3.186534
-40.887926	5.427170	3.196531
-40.372784	-8.833060	3.206528
-40.185275	-0.809656	3.216525
-39.606713	2.738090	3.226522
-38.864305	-1.375615	3.236518
-38.569631	-4.394447	3.246515
-38.145657	-3.044337	3.256512
-37.408918	1.763103	3.266509
-37.069199	-0.396183	3.276506
-36.621450	-6.589288	3.286502
-35.951127	-8.321211	3.296499
-35.492623	-2.330592	3.306496
-35.308049	-2.009776	3.316493
-34.003633	2.055973	3.326490
-33.638058	-4.395007	3.336486
-33.518696	-1.568872	3.346483
-33.436464	-3.912347	3.356480
-32.363041	2.386832	3.366477
-31.803299	2.495949	3.376474
-31.828740	3.321599	3.386470
-30.687476	1.230723	3.396467
-30.017730	2.327533	3.406464
-30.039680	7.141863	3.416461
-30.214351	-3.647553	3.426458
-28.939316	5.001718	3.436454
-28.600568	-2.700478	3.446451
-27.586888	-0.541693	3.456448
-27.186453	0.681119	3.466445
-27.225674	-8.649818	3.476442
-26.970014	-1.159719	3.486438
-25.739164	-6.796285	3.496435
-25.588617	1.902269	3.506432
-25.099503	0.272670	3.516429
-24.215946	2.205429	3.526426
-24.251300	0.131569	3.536422
-23.472747	-2.973121	3.546419
-22.533557	-2.129777	3.556416
-22.331780	0.623831	3.566413
-21.997221	-1.671922	3.576410
-21.907067	-0.652614	3.586406
-20.919682	1.413908	3.596403
-20.722743	2.220912	3.606400
-20.025007	0.324603	3.616397
-19.475544	1.351432	3.626394
-19.033666	-5.795039	3.636390
-17.756560	2.402804	3.646387
-18.043698	4.252211	3.656384
-17.291279	7.832226	3.666381
-17.400185	3.928649	3.676378
-16.795038	4.110667	3.686374
-16.075467	-0.126499	3.696371
-14.776180	-1.823471	3.706368
-14.987878	-2.932364	3.716365
-14.565122	-2.847388	3.726362
-14.282776	0.397117	3.736358
-13.143426	1.384751	3.746355
-13.102492	4.032414	3.756352
-12.893301	2.928315	3.766349
-11.737510	-0.181146	3.776346
-11.501842	-3.641492	3.786342
-10.808265	2.740351	3.796339
-9.823624	0.102812	3.806336
-10.325294	1.235928	3.816333
-9.824431	2.989821	3.826330
-8.575480	3.073925	3.836326
-8.124691	5.827596	3.846323
-7.767415	-4.284856	3.856320
-7.941709	3.518488	3.866317
-7.510183	-1.017940	3.876314
-6.267874	-1.402989	3.886310
-5.522395	-4.508917	3.896307
-5.204405	1.710861	3.906304
-5.019843	3.698910	3.916301
-4.797130	7.402405	3.926298
-4.161851	4.878238	3.936294
-3.626133	9.848394	3.946291
-3.022442	19.672259	3.956288
-2.859610	35.387454	3.966285
-2.659773	51.036076	3.976282
-1.928292	69.803709	3.986278
-1.291731	80.072668	3.996275
-1.109364	98.193869	4.006272
-0.742443	126.610249	4.016269
0.000000	145.359992	4.021274
-0.217336	168.181715	4.026278
-0.338137	155.638606	4.031283
0.199723	179.653689	4.036288
0.564838	182.562968	4.041293
0.781994	197.122972	4.046298
0.523516	194.709770	4.051302
0.728178	192.403795	4.056307
0.778767	203.020797	4.061312
0.569143	207.765555	4.066317
0.976629	200.489047	4.071322
0.772889	202.390801	4.076326
0.980156	200.292779	4.081331
1.009826	199.779369	4.086336
0.974867	199.072615	4.091341
0.820095	201.884464	4.096346
0.975586	204.727620	4.101350
1.278767	189.939439	4.106355
0.993616	201.094322	4.111360
0.958853	197.852364	4.116365
1.160560	199.066162	4.121370
1.014618	195.530035	4.126374
0.930990	195.376974	4.131379
0.715353	210.509297	4.136384
0.883395	203.605342	4.141389
0.854214	195.740266	4.146394
0.707829	207.258361	4.151398
0.944163	199.471863	4.156403
1.356017	213.064665	4.161408
1.363561	224.342188	4.166413
1.029585	203.687127	4.171418
0.799115	208.055269	4.176422
0.989486	205.031580	4.181427
0.956536	219.817528	4.186432
0.952876	211.636822	4.191437
1.241917	217.954263	4.196442
1.090552	231.263630	4.201446
1.283194	218.726387	4.206451
0.728004	225.153631	4.211456
1.101823	231.494731	4.216461
1.109592	219.740345	4.221466
0.944389	226.212731	4.226470
1.180153	219.929030	4.231475
1.013336	226.290189	4.236480
1.276642	227.813670	4.241485
1.270579	233.181661	4.246490
1.293854	226.698313	4.251494
1.600976	225.435062	4.256499
1.259797	229.114881	4.261504
1.054551	225.306771	4.266509
1.091276	231.682180	4.271514
1.097537	247.460775	4.276518
1.402475	250.464492	4.281523
1.874537	262.003161	4.286528
1.283481	239.034030	4.291533
1.110509	236.503061	4.296538
1.046514	255.180326	4.301542
1.430607	260.019387	4.306547
1.503306	253.756558	4.311552
1.604017	264.495544	4.316557
1.684060	266.600734	4.321562
1.655315	267.983335	4.326566
1.794159	259.296913	4.331571
1.567950	263.280150	4.336576
1.493306	240.245239	4.341581
1.580406	241.245161	4.346586
1.501748	243.468784	4.351590
1.470083	247.998195	4.356595
1.531461	264.639710	4.361600
1.537367	262.100824	4.366605
1.958578	270.147368	4.371610
1.398461	263.580440	4.376614
1.668549	258.025724	4.381619
1.563288	261.564857	4.386624
1.776102	268.961743	4.391629
2.014345	267.553997	4.396634
1.601692	267.348067	4.401638
1.590768	251.956288	4.406643
1.597761	260.872996	4.411648
1.723434	257.441855	4.416653
1.675178	267.932199	4.421658
1.288610	265.278726	4.426662
1.571413	259.633892	4.431667
1.472553	267.856932	4.436672
1.590784	266.431763	4.441677
1.669263	258.123173	4.446682
1.315358	266.063432	4.451686
1.902870	258.961133	4.456691
1.381742	273.220173	4.461696
1.507368	271.457912	4.466701
1.934933	285.536979	4.471706
1.887627	292.991552	4.476710
2.089398	286.759236	4.481715
2.091431	290.726590	4.486720
1.549229	286.098875	4.491725
1.822356	282.331914	4.496730
1.587606	300.853788	4.501734
2.115837	291.528225	4.506739
1.969788	303.493896	4.511744
1.970646	299.654600	4.516749
2.258035	295.372592	4.521754
1.610352	308.661594	4.526758
2.399803	299.212653	4.531763
1.778476	307.403629	4.536768
1.827645	299.399231	4.541773
2.147074	306.656329	4.546778
1.700189	304.944070	4.551782
1.711617	299.470059	4.556787
1.889436	302.043723	4.561792
2.046192	299.455974	4.566797
2.416318	308.523139	4.571802
2.239512	304.447447	4.576806
2.174183	302.136039	4.581811
2.134113	310.450404	4.586816
1.777463	303.691502	4.591821
2.063858	306.988978	4.596826
1.745637	299.853116	4.601830
1.934294	297.829599	4.606835
2.015292	331.086479	4.611840
2.229698	326.484232	4.616845
2.594992	326.252689	4.621850
2.177319	337.166366	4.626854
2.342780	329.700371	4.631859
2.210011	335.286912	4.636864
2.376214	332.129656	4.641869
2.225331	334.161796	4.646874
2.414280	329.779059	4.651878
2.548443	314.762800	4.656883
1.949233	321.084101	4.661888
2.622906	324.380995	4.666893
2.438300	318.381763	4.671898
2.240121	324.319341	4.676902
2.661835	323.297197	4.681907
2.092509	323.648836	4.686912
2.443123	325.523536	4.691917
2.589789	335.349184	4.696922
2.386634	329.649420	4.701926
2.453309	333.153193	4.706931
2.390498	350.994653	4.711936
2.104505	342.967191	4.716941
2.552956	336.270718	4.721946
2.257996	339.272160	4.726950
2.733450	335.127921	4.731955
2.702781	343.261761	4.736960
2.615666	337.203162	4.741965
2.753948	332.884857	4.746970
2.423276	334.065657	4.751974
2.923195	331.526062	4.756979
2.385948	336.005423	4.761984
2.392385	333.301069	4.766989
2.471268	340.360026	4.771994
2.523878	344.399730	4.776998
2.675740	328.134736	4.782003
2.383228	339.571945	4.787008
2.486516	344.490882	4.792013
2.312825	346.242634	4.797018
2.142327	340.920886	4.802022
2.569643	342.276125	4.807027
2.469361	348.818128	4.812032
2.712360	338.926048	4.817037
2.596808	343.994691	4.822042
2.063468	357.896873	4.827046
2.740264	361.257590	4.832051
2.788203	365.343855	4.837056
2.617089	365.108189	4.842061
2.350681	374.067472	4.847066
2.671497	364.843898	4.852070
2.868735	371.872417	4.857075
2.983937	370.244679	4.862080
2.920730	367.912782	4.867085
3.012526	366.273133	4.872090
2.573005	374.812534	4.877094
3.212500	371.411529	4.882099
2.819068	366.687916	4.887104
2.864303	367.201237	4.892109
3.001913	366.458599	4.897114
2.954516	366.058784	4.902118
2.941111	359.221314	4.907123
2.687327	371.424711	4.912128
3.029540	362.699228	4.917133
3.072398	366.494867	4.922138
3.038750	373.068274	4.927142
3.087710	372.731636	4.932147
2.940114	364.667827	4.937152
2.963300	370.783076	4.942157
2.475353	370.878119	4.947162
2.481476	374.720298	4.952166
3.040574	379.994952	4.957171
3.029445	396.874173	4.962176
2.768075	396.600367	4.967181
2.879690	401.047883	4.972186
3.069935	400.455385	4.977190
3.281933	396.307986	4.982195
3.330626	396.056444	4.987200
3.344190	403.645640	4.992205
3.105072	398.101191	4.997210
3.064872	400.540276	5.002214
3.212601	396.612106	5.007219
3.358755	396.986959	5.012224
3.132427	398.270466	5.017229
3.097123	393.930765	5.022234
3.113374	405.120543	5.027238
3.286035	391.859277	5.032243
3.233761	397.891323	5.037248
3.286185	395.182106	5.042253
3.580700	398.644811	5.047258
3.119949	395.243254	5.052262
3.159389	394.627577	5.057267
3.223277	409.385831	5.062272
3.086041	397.450484	5.067277
3.157934	401.677441	5.072282
3.007753	405.520448	5.077286
3.308643	400.281058	5.082291
3.251614	394.980759	5.087296
3.541555	399.619765	5.092301
3.040589	407.932552	5.097306
3.009817	419.097567	5.102310
3.617000	419.593418	5.107315
3.795023	426.973249	5.112320
3.725680	421.153611	5.117325
3.941728	420.140061	5.122330
3.374003	411.666460	5.127334
3.379502	399.517045	5.132339
3.325366	405.811665	5.137344
3.041910	415.351009	5.142349
3.743163	427.684619	5.147354
3.494363	427.860045	5.152358
3.849901	433.146323	5.157363
3.716303	427.843101	5.162368
3.607236	428.197858	5.167373
3.682065	418.388435	5.172378
3.609060	428.345436	5.177382
3.928509	426.628814	5.182387
3.496885	418.725083	5.187392
3.459246	423.035700	5.192397
3.708355	428.497866	5.197402
3.811379	426.467200	5.202406
3.772789	419.754052	5.207411
3.869235	427.689086	5.212416
3.520151	417.452170	5.217421
3.902677	420.519048	5.222426
3.495115	426.655522	5.227430
3.363699	423.478857	5.232435
3.463410	427.105647	5.237440
3.482618	429.661590	5.242445
3.739409	424.761813	5.247450
3.605169	426.824165	5.252454
3.428753	433.022812	5.257459
3.510657	439.980276	5.262464
3.396845	433.781411	5.267469
3.900834	441.699289	5.272474
3.791858	459.174561	5.277478
3.978464	457.705096	5.282483
4.081461	464.344126	5.287488
4.215301	449.180181	5.292493
3.918930	445.366386	5.297498
3.700833	449.518828	5.302502
4.304842	453.549941	5.307507
4.245708	448.560188	5.312512
4.068882	434.605093	5.317517
3.892055	428.642419	5.322522
3.770503	434.170897	5.327526
3.669557	434.685930	5.332531
3.712133	444.980789	5.337536
3.998855	454.180253	5.342541
3.995440	459.371265	5.347546
3.940381	464.507484	5.352550
3.984348	464.705473	5.357555
4.128383	470.528620	5.362560
3.817853	466.754855	5.367565
3.947062	465.318575	5.372570
3.730152	474.384966	5.377574
4.148805	467.459525	5.382579
4.042968	465.157168	5.387584
4.101720	465.644968	5.392589
4.067442	463.905020	5.397594
4.000519	471.996188	5.402598
4.269491	471.974972	5.407603
4.350198	466.043445	5.412608
4.115929	466.573648	5.417613
4.456736	465.097199	5.422618
3.852433	466.020995	5.427622
3.904314	465.093630	5.432627
4.527773	480.243958	5.437632
4.356488	484.420626	5.442637
4.124810	480.384957	5.447642
4.398578	493.231840	5.452646
4.714106	484.035712	5.457651
4.242414	483.463031	5.462656
4.098765	479.645447	5.467661
4.375223	494.168481	5.472666
4.432862	499.857940	5.477670
5.020062	495.162536	5.482675
4.301293	476.155859	5.487680
4.226739	468.323220	5.492685
4.348328	470.442674	5.497690
4.238000	475.265794	5.502694
4.526265	490.437299	5.507699
4.691587	482.225508	5.512704
4.651098	497.247804	5.517709
4.465860	466.632906	5.522714
4.256706	461.710024	5.527718
4.250801	473.549412	5.532723
4.181428	484.714156	5.537728
4.836466	482.062812	5.542733
4.831705	490.571331	5.547738
4.454924	499.604810	5.552742
4.614889	481.292298	5.557747
4.793556	480.987264	5.562752
4.483043	494.125277	5.567757
4.668796	484.041101	5.572762
4.740475	503.615405	5.577766
4.959067	483.407998	5.582771
4.295811	478.728833	5.587776
4.387629	487.922701	5.592781
4.796951	486.828203	5.597786
4.657982	495.095105	5.602790
4.519698	488.260495	5.607795
4.632528	495.342910	5.612800
4.852564	492.122637	5.617805
4.820763	483.434351	5.622810
4.637102	491.659317	5.627814
4.426808	495.174454	5.632819
4.637864	500.126904	5.637824
4.478727	499.319532	5.642829
4.600789	490.497031	5.647834
4.690432	491.800451	5.652838
4.529146	485.940758	5.657843
5.064902	487.599915	5.662848
5.166439	495.492502	5.667853
4.988842	491.652712	5.672858
4.611120	495.720102	5.677862
4.825049	483.216220	5.682867
4.981862	493.969757	5.687872
5.131736	491.268264	5.692877
4.906924	488.654075	5.697882
4.813905	500.167695	5.702886
4.833607	495.263346	5.707891
5.026095	493.513077	5.712896
5.123175	490.261067	5.717901
5.055445	499.255803	5.722906
5.145689	496.133983	5.727910
5.245255	490.714182	5.732915
5.174073	495.668372	5.737920
5.069460	497.264447	5.742925
5.025870	485.342929	5.747930
4.795722	491.453011	5.752934
5.193605	488.835170	5.757939
4.944161	490.941866	5.762944
4.836540	495.816049	5.767949
5.167673	492.061535	5.772954
4.922253	501.175287	5.777958
5.302084	492.669061	5.782963
5.295036	499.210687	5.787968
5.022101	501.114068	5.792973
5.280696	490.929417	5.797978
5.119463	496.492707	5.802982
5.047253	491.500962	5.807987
5.092968	485.534175	5.812992
4.784670	495.953277	5.817997
5.313652	514.908399	5.823002
5.070927	516.423940	5.828006
5.255757	530.431928	5.833011
5.068954	529.354242	5.838016
5.130364	520.063020	5.843021
5.359915	518.726945	5.848026
5.250205	525.168756	5.853030
5.371125	523.189778	5.858035
5.269443	530.890474	5.863040
5.613940	532.137291	5.868045
5.461981	522.690177	5.873050
4.942584	535.588709	5.878054
5.344383	519.366787	5.883059
5.105327	525.549202	5.888064
5.202967	533.595590	5.893069
5.299152	531.379162	5.898074
5.585728	530.895229	5.903078
5.472135	529.157553	5.908083
5.368233	519.768197	5.913088
5.447299	532.623673	5.918093
5.474249	535.274062	5.923098
5.116414	542.126190	5.928102
5.295982	527.672125	5.933107
5.393916	537.189437	5.938112
5.450120	555.920373	5.943117
5.735704	557.259239	5.948122
5.839963	557.514144	5.953126
6.080917	543.377287	5.958131
5.300719	535.937538	5.963136
5.274246	541.546810	5.968141
5.527954	538.447447	5.973146
5.593181	558.529066	5.978150
5.695180	547.506550	5.983155
5.784219	560.913148	5.988160
6.088388	554.867819	5.993165
5.771937	534.171130	5.998170
5.641662	535.655422	6.003174
5.749531	524.366923	6.008179
5.442982	525.104661	6.013184
5.535140	534.424799	6.018189
5.909976	537.324446	6.023194
5.705451	547.756592	6.028198
5.885812	547.443383	6.033203
5.921249	538.831946	6.038208
5.795424	537.409868	6.043213
5.706582	530.130142	6.048218
5.630535	531.589667	6.053222
5.823457	524.070289	6.058227
5.910378	524.705970	6.063232
5.484311	529.787412	6.068237
5.848315	526.407917	6.073242
5.550652	530.300240	6.078246
5.698730	522.010375	6.083251
5.768719	532.640177	6.088256
5.671140	544.352517	6.093261
5.839154	545.806757	6.098266
5.556386	551.100694	6.103270
5.936048	554.998875	6.108275
6.126935	543.532034	6.113280
5.984158	536.153489	6.118285
5.812638	526.301315	6.123290
5.927628	532.028848	6.128294
5.811916	531.903593	6.133299
5.683396	525.934461	6.138304
5.657878	527.221038	6.143309
5.749667	519.202956	6.148314
5.784101	524.895281	6.153318
5.923350	520.075718	6.158323
5.461832	517.826330	6.163328
5.623148	523.676237	6.168333
5.826346	522.958646	6.173338
5.509919	525.558342	6.178342
5.732522	519.729793	6.183347
5.961970	522.067412	6.188352
5.507314	519.648359	6.193357
5.738573	528.830214	6.198362
5.787004	529.934636	6.203366
5.759395	530.553564	6.208371
5.745661	528.368165	6.213376
5.584878	523.982503	6.218381
6.138684	524.825241	6.223386
5.915762	527.654155	6.228390
5.850123	524.211219	6.233395
5.870675	526.966663	6.238400
5.862887	535.588192	6.243405
6.080915	521.350364	6.248410
5.805549	525.976058	6.253414
5.706899	521.412765	6.258419
6.024516	522.796842	6.263424
6.073143	524.563701	6.268429
6.021031	530.348505	6.273434
5.703157	522.355237	6.278438
5.633617	518.750734	6.283443
5.806989	529.346445	6.288448
5.507477	529.648277	6.293453
5.913425	531.431748	6.298458
5.665466	533.523995	6.303462
5.806937	528.853251	6.308467
5.752942	526.304309	6.313472
5.618956	526.699899	6.318477
5.744939	527.278593	6.323482
5.425687	532.240521	6.328486
5.638730	525.555913	6.333491
5.420788	526.912440	6.338496
5.570144	530.748502	6.343501
5.824260	528.949544	6.348506
5.477318	531.440625	6.353510
5.595285	524.987059	6.358515
5.825400	525.035624	6.363520
5.910260	530.712496	6.368525
5.771989	522.259090	6.373530
5.359534	529.090063	6.378534
5.901140	527.960830	6.383539
5.892267	529.277804	6.388544
5.867854	526.012356	6.393549
5.835214	524.027428	6.398554
5.397554	528.137904	6.403558
5.213796	531.396455	6.408563
5.764698	532.802487	6.413568
5.735762	530.956859	6.418573
5.916307	525.251900	6.423578
5.703652	530.423117	6.428582
5.879023	521.371342	6.433587
5.549881	522.140843	6.438592
5.790122	529.858725	6.443597
5.910185	525.662380	6.448602
5.823836	537.937247	6.453606
5.787346	526.764611	6.458611
5.635557	534.318695	6.463616
5.825975	535.066496	6.468621
6.028980	527.930457	6.473626
5.749862	530.890435	6.478630
5.656307	525.958456	6.483635
5.654525	530.273032	6.488640
5.585291	529.400450	6.493645
5.646367	526.687409	6.498650
5.813953	535.182609	6.503654
5.743822	532.792632	6.508659
5.999650	525.524509	6.513664
5.798925	527.960199	6.518669
5.829739	524.117663	6.523674
5.593474	535.978469	6.528678
5.566370	531.677628	6.533683
5.919553	539.260186	6.538688
5.709174	525.961391	6.543693
5.789911	523.182736	6.548698
5.454395	537.446014	6.553702
5.588750	530.453361	6.558707
5.692883	530.577845	6.563712
5.589775	537.563029	6.568717
5.856488	521.790122	6.573722
5.411928	531.881928	6.578726
5.690244	519.303023	6.583731
5.214716	530.612214	6.588736
5.333965	548.743051	6.593741
5.903305	550.017958	6.598746
5.648469	554.861084	6.603750
5.772990	553.179095	6.608755
5.933207	560.374268	6.613760
6.048523	559.536247	6.618765
6.059694	554.134219	6.623770
5.774436	548.499475	6.628774
5.972392	542.620730	6.633779
5.737219	530.133947	6.638784
5.637406	530.848503	6.643789
5.739535	526.019890	6.648794
5.631214	529.397180	6.653798
5.483507	529.168883	6.658803
5.554003	537.112612	6.663808
5.483035	553.888441	6.668813
5.802837	564.107479	6.673818
5.878037	562.365967	6.678822
5.736572	560.990483	6.683827
6.071462	561.132801	6.688832
5.699022	558.152115	6.693837
6.324423	550.234710	6.698842
5.585709	540.025525	6.703846
6.064193	531.944590	6.708851
6.026557	529.219477	6.713856
5.605612	533.251210	6.718861
5.883818	524.676150	6.723866
5.841417	528.530545	6.728870
6.114150	519.299647	6.733875
5.599072	519.897268	6.738880
5.599929	529.162663	6.743885
5.702830	526.360208	6.748890
5.656132	525.859630	6.753894
5.672347	526.877426	6.758899
5.731208	529.118575	6.763904
5.394095	535.254871	6.768909
5.561874	522.682032	6.773914
5.613979	533.881557	6.778918
5.795312	524.105542	6.783923
5.483008	524.931851	6.788928
5.633171	532.979014	6.793933
6.237269	538.162994	6.798938
5.792607	533.384861	6.803942
5.686745	534.314730	6.808947
5.864482	530.307357	6.813952
5.919825	527.011731	6.818957
6.030985	518.407896	6.823962
5.470418	532.956491	6.828966
5.431596	529.472605	6.833971
5.630652	523.523827	6.838976
5.449677	528.957785	6.843981
5.613832	526.350618	6.848986
5.781472	548.508253	6.853990
6.113788	553.510302	6.858995
5.890199	537.854680	6.864000
5.734372	537.463540	6.869005
5.817731	527.515681	6.874010
5.519447	535.865030	6.879014
5.796212	526.915458	6.884019
5.581212	535.320677	6.889024
5.676499	526.477132	6.894029
5.812210	520.304798	6.899034
5.520859	527.418634	6.904038
5.886945	534.307574	6.909043
5.755440	530.623935	6.914048
5.797461	523.862662	6.919053
5.794685	524.889720	6.924058
5.355599	528.285075	6.929062
5.634081	540.384681	6.934067
5.990661	554.645461	6.939072
5.905548	555.139918	6.944077
5.966973	533.360804	6.949082
5.860671	537.513900	6.954086
5.924399	529.185308	6.959091
5.782641	521.220699	6.964096
5.822886	533.130242	6.969101
6.177220	532.898143	6.974106
5.852169	527.469310	6.979110
6.014628	531.587373	6.984115
5.792316	529.977223	6.989120
5.485835	538.601049	6.994125
5.784205	532.393093	6.999130
5.918278	537.013747	7.004134
5.845125	530.573472	7.009139
5.758873	531.194611	7.014144
5.686804	535.576478	7.019149
5.624485	532.856044	7.024154
5.694756	546.253699	7.029158
6.279052	533.819285	7.034163
6.121040	537.378661	7.039168
5.969970	541.285589	7.044173
6.180520	522.718766	7.049178
5.817788	510.781005	7.054182
5.700532	505.963269	7.059187
5.878429	507.146106	7.064192
5.582050	507.175288	7.069197
5.912208	501.062724	7.074202
5.411732	499.674270	7.079206
5.584925	489.764842	7.084211
5.638954	503.482866	7.089216
5.545445	526.925571	7.094221
5.681064	522.810915	7.099226
5.600277	537.205672	7.104230
5.731570	535.491186	7.109235
5.707214	534.058226	7.114240
5.575203	540.729888	7.119245
5.622334	533.577623	7.124250
5.416620	539.418650	7.129254
5.844929	528.097611	7.134259
5.974438	532.601799	7.139264
5.870939	527.714485	7.144269
5.979666	530.146690	7.149274
5.822692	532.134279	7.154278
5.897696	533.566424	7.159283
6.165531	526.962335	7.164288
5.746143	511.695952	7.169293
5.521191	498.106742	7.174298
5.636321	515.767173	7.179302
6.040690	514.830773	7.184307
5.829854	502.863327	7.189312
5.359678	497.753361	7.194317
5.766219	509.185056	7.199322
5.484894	524.438479	7.204326
5.791318	518.172757	7.209331
5.994922	521.634164	7.214336
5.699907	519.595986	7.219341
5.537952	528.171207	7.224346
5.283530	533.665085	7.229350
5.640689	532.347149	7.234355
5.952725	530.041698	7.239360
5.373916	535.157117	7.244365
5.614483	527.038222	7.249370
5.755572	536.689684	7.254374
5.670122	525.549034	7.259379
5.887749	533.971417	7.264384
5.367995	527.913735	7.269389
5.811242	538.063374	7.274394
5.614494	534.474209	7.279398
5.870726	534.583177	7.284403
5.436573	532.740512	7.289408
5.583458	535.527137	7.294413
5.908711	526.939351	7.299418
5.945636	527.579561	7.304422
6.080284	526.853785	7.309427
6.048190	532.031810	7.314432
5.769507	539.765964	7.319437
5.870465	530.958379	7.324442
5.701616	535.916125	7.329446
5.990729	531.909254	7.334451
6.083486	536.487413	7.339456
5.965772	534.279961	7.344461
5.848301	516.044724	7.349466
5.573074	515.027661	7.354470
5.668835	506.424211	7.359475
5.987630	509.539747	7.364480
5.733127	509.721643	7.369485
6.366458	502.574349	7.374490
5.559183	502.920201	7.379494
5.545095	504.148049	7.384499
5.746150	503.481137	7.389504
5.603846	498.262215	7.394509
5.873686	499.165983	7.399514
5.677928	495.996010	7.404518
5.771945	501.540717	7.409523
5.738629	494.506973	7.414528
5.745292	499.768753	7.419533
5.688002	490.387681	7.424538
5.660832	496.734114	7.429542
5.560279	500.806326	7.434547
5.861877	490.986934	7.439552
5.850330	501.468003	7.444557
5.831994	495.387494	7.449562
5.386490	500.197449	7.454566
5.523011	507.499729	7.459571
5.979273	521.262070	7.464576
5.714551	521.585966	7.469581
6.070582	515.266248	7.474586
5.613087	501.488009	7.479590
5.766810	502.542630	7.484595
5.719273	502.674468	7.489600
5.540589	500.801345	7.494605
5.646932	509.083086	7.499610
5.920118	518.659380	7.504614
6.127871	509.123504	7.509619
5.945976	506.042009	7.514624
5.643421	507.119496	7.519629
6.012592	500.386351	7.524634
6.164349	504.100844	7.529638
5.740452	499.502019	7.534643
6.020557	501.792568	7.539648
5.723686	499.369888	7.544653
5.994016	489.943644	7.549658
5.497231	503.096131	7.554662
5.632183	495.518086	7.559667
6.029172	501.288110	7.564672
5.887263	505.697714	7.569677
5.813731	491.522006	7.574682
5.618093	499.355859	7.579686
5.591306	500.008395	7.584691
5.812622	496.768767	7.589696
5.848408	503.609178	7.594701
5.858390	499.368116	7.599706
5.832715	498.016287	7.604710
6.032766	493.117991	7.609715
6.063882	502.241011	7.614720
5.771988	503.464736	7.619725
5.820952	497.689812	7.624730
5.872915	488.968511	7.629734
5.685606	478.110381	7.634739
5.428778	484.691190	7.639744
5.349691	487.242107	7.644749
5.750994	495.424677	7.649754
5.534550	504.099881	7.654758
5.341464	499.118677	7.659763
5.425694	496.161251	7.664768
5.199516	501.688330	7.669773
5.723997	503.174513	7.674778
5.591185	496.357938	7.679782
5.543985	502.051536	7.684787
5.605296	503.137247	7.689792
5.431740	509.474575	7.694797
5.901662	517.560347	7.699802
5.690797	523.216722	7.704806
5.834376	532.929733	7.709811
5.945157	532.570422	7.714816
5.902121	521.087275	7.719821
5.737017	505.029493	7.724826
5.591141	512.255003	7.729830
5.386790	510.598071	7.734835
5.807491	519.752695	7.739840
5.622300	533.811104	7.744845
5.657201	532.723347	7.749850
5.425008	534.899023	7.754854
5.503804	532.183442	7.759859
6.150769	525.471975	7.764864
5.869408	530.870854	7.769869
6.079996	531.102429	7.774874
5.613334	535.049378	7.779878
5.763468	534.510089	7.784883
5.891981	525.182494	7.789888
5.831195	528.129605	7.794893
5.690657	505.212761	7.799898
5.693188	509.066224	7.804902
5.635397	518.661014	7.809907
5.880491	519.984874	7.814912
5.370755	524.634575	7.819917
5.965327	527.950533	7.824922
5.816895	534.573405	7.829926
5.820267	527.244074	7.834931
5.711558	513.631853	7.839936
5.470030	523.877902	7.844941
5.829414	522.064867	7.849946
5.667411	530.713311	7.854950
5.703563	536.359769	7.859955
5.611067	530.781719	7.864960
5.317918	534.227307	7.869965
5.587528	527.807831	7.874970
5.584812	538.332457	7.879974
5.712409	543.815968	7.884979
5.919152	536.449405	7.889984
5.415195	537.776527	7.894989
5.792814	531.666354	7.899994
5.726022	534.763848	7.904998
5.717486	533.332215	7.910003
5.909664	525.021232	7.915008
5.723094	534.137494	7.920013
5.795728	535.964317	7.925018
5.517376	540.320943	7.930022
5.522698	539.305968	7.935027
5.897827	541.443243	7.940032
5.593319	540.685201	7.945037
5.277197	534.832973	7.950042
5.686785	545.482329	7.955046
5.324626	539.709753	7.960051
5.672864	537.844096	7.965056
6.164350	544.581045	7.970061
5.801484	542.754005	7.975066
5.579215	536.923533	7.980070
5.338185	544.819391	7.985075
5.676090	549.980555	7.990080
5.910334	561.351424	7.995085
5.975905	546.713550	8.000090
5.742396	543.852143	8.005094
5.839414	541.973619	8.010099
5.786354	540.244665	8.015104
5.636629	546.589903	8.020109
5.743118	541.886209	8.025126
5.490046	544.392152	8.030144
5.576064	547.335417	8.035162
5.985337	555.261421	8.040179
5.820916	557.657811	8.045197
5.796627	543.153428	8.050214
5.971141	546.222580	8.055232
5.566636	543.542348	8.060250
5.750650	541.143182	8.065267
5.541344	541.733154	8.070285
5.732432	560.494538	8.075302
5.632131	576.042604	8.080320
5.889609	578.692934	8.085338
6.078617	570.960227	8.090355
5.648229	580.716702	8.095373
6.175284	565.756852	8.100390
5.923297	554.503722	8.105408
5.526310	555.097412	8.110426
5.809574	555.338516	8.115443
5.600877	569.669374	8.120461
6.045168	569.488565	8.125478
6.141971	569.799126	8.130496
5.444023	561.914690	8.135514
5.819234	563.110778	8.140531
5.852516	580.286026	8.145549
5.819428	565.404364	8.150566
5.892136	572.255279	8.155584
5.941046	582.966374	8.160602
5.680815	566.034472	8.165619
5.617077	575.595201	8.170637
5.485610	572.693189	8.175654
5.932835	569.659924	8.180672
5.790609	580.189689	8.185690
6.013364	569.781300	8.190707
5.951799	575.730694	8.195725
5.844504	574.778288	8.200742
6.080441	574.999475	8.205760
5.831442	575.797385	8.210778
5.919722	569.573777	8.215795
6.020617	581.218718	8.220813
5.931812	571.058755	8.225830
6.105183	572.671705	8.230848
5.992061	574.809227	8.235866
6.118447	569.826468	8.240883
5.675805	570.096638	8.245901
5.927822	575.921869	8.250918
6.138802	576.978235	8.255936
6.032357	567.722905	8.260954
6.103920	572.484980	8.265971
5.888000	573.849223	8.270989
5.825344	577.309205	8.276006
6.154411	569.679479	8.281024
5.811014	581.843826	8.286042
6.067675	573.299182	8.291059
5.623329	583.803589	8.296077
5.832661	577.153661	8.301094
5.898759	580.313208	8.306112
6.152664	577.219438	8.311130
6.186921	583.353546	8.316147
6.163689	578.086329	8.321165
6.249870	576.638728	8.326182
5.996892	574.538280	8.331200
5.883645	581.645763	8.336218
6.245059	573.463078	8.341235
5.844003	577.033028	8.346253
5.972796	565.853245	8.351270
6.356330	570.698100	8.356288
5.894322	568.431099	8.361306
6.191109	558.704308	8.366323
5.902512	567.536373	8.371341
5.932198	570.075612	8.376358
5.869074	574.244087	8.381376
5.887840	574.838811	8.386394
6.142779	589.307270	8.391411
6.102003	606.476898	8.396429
6.247253	602.879299	8.401446
6.511582	608.222220	8.406464
6.185848	598.723084	8.411482
6.217881	578.579597	8.416499
6.062642	583.640433	8.421517
6.040413	575.578357	8.426534
6.263960	576.401358	8.431552
6.237234	578.021459	8.436570
6.307148	572.210312	8.441587
6.149652	573.997726	8.446605
6.279935	574.267705	8.451622
6.340202	569.366166	8.456640
5.998353	576.951825	8.461658
6.363237	564.149199	8.466675
6.180763	582.103628	8.471693
6.166085	572.800425	8.476710
6.328915	574.764900	8.481728
6.192380	577.309619	8.486746
6.275875	570.048684	8.491763
6.137257	566.822683	8.496781
6.012465	575.165849	8.501798
6.291996	570.226034	8.506816
6.086421	575.363308	8.511834
6.463383	570.719346	8.516851
6.161967	581.440225	8.521869
6.164446	576.107928	8.526886
6.531926	572.761707	8.531904
6.450855	584.356079	8.536922
6.472508	574.521305	8.541939
5.750949	580.093210	8.546957
5.869932	569.432140	8.551974
6.494194	593.363605	8.556992
6.228478	606.418198	8.562010
6.586685	599.589091	8.567027
6.392356	600.755483	8.572045
6.317621	588.724602	8.577063
6.367143	580.655956	8.582080
6.046190	582.721602	8.587098
6.639270	588.228961	8.592115
6.393918	593.063400	8.597133
6.069671	580.354991	8.602151
6.155617	591.377458	8.607168
6.556134	600.458598	8.612186
6.760684	592.129645	8.617203
6.302318	592.950611	8.622221
6.265692	588.212148	8.627239
6.231043	591.634032	8.632256
6.260095	606.292854	8.637274
6.456167	603.476946	8.642291
6.610442	607.245872	8.647309
6.436078	605.899675	8.652327
6.333197	606.545643	8.657344
6.393972	619.363912	8.662362
6.234832	611.527034	8.667379
6.541270	605.988303	8.672397
6.477461	602.267655	8.677415
6.842830	605.626848	8.682432
6.242595	601.752326	8.687450
6.395654	597.481433	8.692467
6.616420	602.519184	8.697485
6.441510	601.043165	8.702503
6.553233	606.801487	8.707520
6.513104	609.282416	8.712538
6.532178	606.860555	8.717555
6.349294	605.352197	8.722573
6.247764	604.908643	8.727591
6.614820	604.435723	8.732608
6.209257	609.414010	8.737626
6.598570	601.040286	8.742643
6.356477	611.775377	8.747661
6.413202	612.240005	8.752679
6.772186	605.827472	8.757696
6.469803	614.187075	8.762714
6.489519	606.967194	8.767731
6.849461	611.216992	8.772749
6.620864	604.373050	8.777767
6.621497	598.968418	8.782784
6.537327	612.709048	8.787802
6.340006	608.527862	8.792819
6.531998	600.099416	8.797837
6.697268	603.466744	8.802855
6.517759	603.538432	8.807872
6.787910	605.480218	8.812890
6.523221	605.501842	8.817907
6.489609	608.629483	8.822925
6.097815	605.815648	8.827943
6.526384	604.271391	8.832960
6.274781	614.751383	8.837978
6.386937	602.001006	8.842995
6.548175	601.596810	8.848013
6.100554	610.046204	8.853031
6.811152	597.211893	8.858048
6.310434	605.775385	8.863066
6.716995	627.377162	8.868083
7.330038	630.374700	8.873101
6.867193	616.619989	8.878119
6.711652	599.186298	8.883136
6.309169	617.985216	8.888154
6.376964	612.197829	8.893171
6.542038	610.443873	8.898189
6.729135	630.153184	8.903207
6.855812	630.469625	8.908224
6.777330	619.014107	8.913242
6.700471	611.155927	8.918259
6.591053	611.506737	8.923277
6.521855	614.675310	8.928295
7.271531	623.925798	8.933312
6.629972	624.003331	8.938330
6.479164	608.323850	8.943347
6.901403	613.822897	8.948365
6.882432	628.239708	8.953383
7.077191	617.850684	8.958400
6.604006	616.576013	8.963418
6.812938	599.696299	8.968435
6.751356	603.440539	8.973453
6.351639	611.992624	8.978471
6.663406	618.781929	8.983488
6.533342	638.299886	8.988506
6.715347	641.814836	8.993523
6.935021	629.700528	8.998541
6.613021	636.539277	9.003559
7.118155	638.538214	9.008576
6.974302	631.128688	9.013594
6.770030	636.203566	9.018611
7.319317	637.295250	9.023629
7.027667	637.677417	9.028647
7.173946	621.682998	9.033664
7.007552	619.098946	9.038682
6.677821	608.640685	9.043699
6.935957	603.602047	9.048717
6.634717	608.634118	9.053735
6.958936	613.135485	9.058752
6.846121	607.793530	9.063770
6.889806	609.843482	9.068787
7.061628	617.630896	9.073805
6.699982	617.911668	9.078823
6.865190	618.824839	9.083840
7.260250	640.957639	9.088858
7.022079	620.883838	9.093875
7.401649	610.378986	9.098893
6.765627	609.718249	9.103911
7.093538	610.537159	9.108928
6.981440	602.833037	9.113946
6.645427	608.906822	9.118963
6.829473	605.505344	9.123981
6.662603	617.031276	9.128999
7.328614	617.241482	9.134016
6.864783	613.587858	9.139034
6.811390	607.474892	9.144051
7.032109	614.179475	9.149069
7.128732	627.514616	9.154087
7.257765	622.668007	9.159104
6.718613	618.690655	9.164122
7.029281	610.250230	9.169139
7.304243	617.017874	9.174157
6.613836	610.133872	9.179175
6.615443	615.687611	9.184192
6.775989	626.531225	9.189210
6.814096	635.440521	9.194227
7.115799	630.062988	9.199245
6.842464	631.070036	9.204263
7.012330	633.850426	9.209280
6.534368	636.944769	9.214298
6.776540	631.227903	9.219315
6.888465	637.637736	9.224333
6.822200	649.751916	9.229351
7.435487	656.843650	9.234368
7.320001	650.128193	9.239386
6.884278	643.098860	9.244403
7.064218	654.845131	9.249421
7.225208	664.060847	9.254439
7.100647	652.607029	9.259456
7.049057	654.918613	9.264474
7.192188	660.909141	9.269491
6.935670	669.270036	9.274509
7.094271	669.673706	9.279527
7.276245	667.817344	9.284544
7.233024	667.332049	9.289562
7.353108	675.726251	9.294579
7.380160	673.331010	9.299597
7.184469	657.751425	9.304615
7.057693	646.465291	9.309632
7.556243	659.716583	9.314650
7.427507	650.123185	9.319667
6.884480	636.077028	9.324685
6.540558	645.846389	9.329703
6.911326	658.240942	9.334720
7.289647	659.830987	9.339738
7.201338	663.582422	9.344755
7.194090	664.063551	9.349773
7.209288	661.775780	9.354791
7.474881	656.597512	9.359808
7.517422	663.888869	9.364826
7.081333	672.396817	9.369843
7.097881	667.745975	9.374861
6.695782	668.747969	9.379879
6.788723	664.389972	9.384896
7.402913	670.752080	9.389914
7.093531	670.267159	9.394931
7.408730	667.076221	9.399949
7.391296	675.019207	9.404967
7.100360	673.364374	9.409984
7.436344	675.981053	9.415002
7.460772	679.792560	9.420019
7.494215	672.815045	9.425037
7.360500	665.347134	9.430055
7.121400	663.256580	9.435072
7.373721	665.116686	9.440090
7.371780	664.251744	9.445107
7.333890	674.178703	9.450125
7.607250	692.619753	9.455143
7.596129	675.695493	9.460160
7.590839	670.977405	9.465178
7.518385	669.834392	9.470195
7.387094	661.562982	9.475213
7.328532	665.511841	9.480231
7.651687	657.600983	9.485248
7.163646	659.067180	9.490266
7.403468	661.374603	9.495283
7.411399	668.824046	9.500301
7.217302	673.464207	9.505319
7.969125	675.003035	9.510336
8.000937	664.757491	9.515354
7.550825	661.037020	9.520371
7.606276	657.694225	9.525389
7.372674	669.906991	9.530407
7.548041	662.441442	9.535424
7.565635	665.132099	9.540442
7.296274	666.172740	9.545459
7.237597	651.169650	9.550477
7.260062	667.838550	9.555495
7.391518	664.102876	9.560512
7.660773	660.390052	9.565530
7.331852	668.786162	9.570547
7.672690	675.844678	9.575565
7.711827	671.079078	9.580583
7.302111	662.578590	9.585600
7.766258	676.950880	9.590618
7.779513	682.071244	9.595635
7.795461	666.532585	9.600653
7.479345	671.787402	9.605671
7.428789	676.039250	9.610688
7.563164	665.649171	9.615706
7.423417	667.000219	9.620723
7.970189	677.644490	9.625741
7.714394	684.908884	9.630759
7.534685	674.443256	9.635776
7.564694	676.494104	9.640794
7.847894	692.459266	9.645811
7.898405	674.603598	9.650829
7.533815	665.953520	9.655847
7.422100	663.087195	9.660864
7.797952	668.100665	9.665882
7.722025	681.783696	9.670899
7.800265	663.995886	9.675917
7.658551	668.009299	9.680935
7.580936	654.602157	9.685952
7.835176	663.438675	9.690970
7.376931	674.909951	9.695987
7.658970	685.301626	9.701005
7.782035	685.034056	9.706023
7.916356	692.260231	9.711040
8.075458	687.442086	9.716058
7.621152	680.192205	9.721075
7.476527	668.214564	9.726093
7.763353	692.712460	9.731111
7.927361	690.662627	9.736128
7.795274	693.478855	9.741146
7.849584	699.515994	9.746163
7.928980	699.423361	9.751181
8.037895	691.265694	9.756199
7.529303	684.019682	9.761216
7.707649	688.935950	9.766234
7.915150	691.442025	9.771251
8.005561	688.686312	9.776269
7.749885	688.756243	9.781287
7.683481	692.474138	9.786304
8.002557	691.698943	9.791322
7.681112	697.057400	9.796339
7.795531	691.718731	9.801357
7.780975	698.488883	9.806375
7.498952	696.717617	9.811392
8.043982	685.453668	9.816410
8.018656	703.123767	9.821427
8.261410	689.515129	9.826445
8.412520	690.430244	9.831463
7.780892	690.438420	9.836480
7.978337	680.126071	9.841498
7.815905	677.275228	9.846515
7.926811	683.315192	9.851533
7.983899	687.693699	9.856551
7.654058	694.934140	9.861568
8.294996	692.334495	9.866586
7.771881	701.352114	9.871603
7.786590	692.474263	9.876621
7.826763	690.920497	9.881639
8.078720	690.464271	9.886656
7.985455	691.843055	9.891674
7.806285	693.949013	9.896691
8.128347	693.432756	9.901709
8.260502	695.333629	9.906727
8.010350	698.191455	9.911744
7.797071	692.681471	9.916762
8.257053	685.949837	9.921779
8.174360	684.698683	9.926797
8.226300	692.733334	9.931815
7.857925	693.003806	9.936832
7.992570	687.624390	9.941850
7.896132	696.679615	9.946867
8.016846	693.598430	9.951885
8.142115	696.686986	9.956903
7.868118	703.156025	9.961920
7.849816	692.012910	9.966938
7.455978	695.159472	9.971955
7.950298	691.869581	9.976973
7.761647	700.690093	9.981991
8.314631	710.849135	9.987008
8.628546	708.650862	9.992026
8.302263	693.920769	9.997043
8.279149	698.357045	10.002061
8.520876	694.273597	10.007079
8.013478	696.374854	10.012096
8.437542	686.680448	10.017114
7.947209	695.761529	10.022131
8.147689	694.559148	10.027149
8.214972	692.415888	10.032167
7.883614	697.809843	10.037184
8.199034	679.621739	10.042202
8.248757	688.783458	10.047219
8.422927	690.465181	10.052237
8.601353	685.379679	10.057255
8.006175	695.830008	10.062272
8.291078	679.886586	10.067290
8.151640	694.158456	10.072307
8.153518	692.288609	10.077325
8.095818	687.599271	10.082343
8.143341	694.994142	10.087360
8.403880	694.925842	10.092378
8.116969	706.935273	10.097395
8.437409	720.034624	10.102413
8.618673	708.417532	10.107431
8.051502	702.255164	10.112448
8.314217	708.453848	10.117466
8.588374	722.182482	10.122483
8.421799	714.768411	10.127501
8.385644	690.824679	10.132519
8.365649	690.215072	10.137536
8.583246	685.075843	10.142554
8.364658	690.160195	10.147571
8.353024	684.534546	10.152589
8.521686	687.867081	10.157607
8.337669	681.694815	10.162624
8.690776	686.106977	10.167642
8.225561	685.501412	10.172659
8.214053	685.103772	10.177677
8.685456	688.803868	10.182695
8.494060	689.667831	10.187712
8.628256	691.025879	10.192730
8.359608	684.289314	10.197747
8.340833	686.933245	10.202765
8.548783	681.107467	10.207783
8.508134	688.520085	10.212800
8.672910	686.902776	10.217818
8.333090	687.900364	10.222835
8.007414	694.885013	10.227853
8.444430	701.273323	10.232871
8.731940	723.142571	10.237888
8.625498	716.112220	10.242906
8.390357	715.672481	10.247923
8.365097	727.822843	10.252941
8.853687	724.291782	10.257959
8.388397	726.349065	10.262976
8.819748	719.006052	10.267994
8.681806	731.010518	10.273011
8.377621	717.866809	10.278029
8.451015	710.609449	10.283047
8.572084	721.017567	10.288064
8.875131	716.477922	10.293082
8.979525	715.490650	10.298099
8.476452	706.572159	10.303117
8.497159	695.619420	10.308135
8.719885	712.039078	10.313152
9.224105	703.955308	10.318170
8.757905	689.218863	10.323187
8.736933	681.483078	10.328205
8.609690	678.872062	10.333223
8.752072	687.911751	10.338240
8.666409	686.058762	10.343258
8.355515	686.586235	10.348275
8.440034	686.701402	10.353293
8.699771	696.457052	10.358311
8.590165	712.391222	10.363328
8.599461	717.452808	10.368346
8.915843	726.501894	10.373363
8.680236	733.462198	10.378381
8.683372	728.728524	10.383399
8.769531	726.678192	10.388416
8.717253	716.005225	10.393434
8.691565	718.920762	10.398451
8.768061	716.848017	10.403469
8.862509	712.758244	10.408487
8.603285	723.941498	10.413504
8.648309	709.937656	10.418522
8.939358	714.331757	10.423539
8.838345	721.071748	10.428557
8.698062	715.902798	10.433575
8.481647	716.418170	10.438592
8.463316	721.895332	10.443610
8.691515	720.777330	10.448627
8.547521	718.680074	10.453645
8.974612	713.965962	10.458663
8.986046	721.208563	10.463680
8.958432	722.897720	10.468698
8.908254	720.838076	10.473715
8.744837	718.203124	10.478733
9.154214	716.418938	10.483751
8.968323	716.274963	10.488768
9.068843	713.825034	10.493786
8.770046	718.975036	10.498803
8.797994	714.266390	10.503821
9.166263	715.471120	10.508839
9.043323	722.598972	10.513856
9.048445	719.957370	10.518874
9.026183	712.581211	10.523891
8.769343	712.500163	10.528909
8.987483	708.132838	10.533927
8.895345	722.467370	10.538944
8.744665	719.662601	10.543962
8.885665	722.506839	10.548979
9.093592	726.919826	10.553997
9.293572	711.493948	10.559015
8.830730	719.404024	10.564032
9.027917	717.772683	10.569050
9.167205	723.213117	10.574067
8.987399	720.542691	10.579085
9.383645	718.252048	10.584103
9.228859	724.217132	10.589120
9.236930	713.601493	10.594138
9.156077	713.068100	10.599155
9.132045	713.474454	10.604173
9.209513	709.609135	10.609191
9.106519	716.163637	10.614208
9.096621	714.920110	10.619226
9.245601	721.934830	10.624243
8.868892	719.526523	10.629261
8.868046	713.495164	10.634279
9.141804	714.121484	10.639296
9.273342	725.883303	10.644314
9.213135	723.397785	10.649331
9.054540	730.671695	10.654349
9.236187	727.082804	10.659367
9.419425	738.936067	10.664384
9.109507	732.244109	10.669402
9.520935	724.166640	10.674419
9.102452	718.424106	10.679437
9.289415	712.200241	10.684455
9.348456	720.951405	10.689472
9.121661	720.617364	10.694490
9.375294	715.393029	10.699507
9.163683	722.338332	10.704525
9.481103	721.845282	10.709543
9.182297	727.327553	10.714560
9.239847	726.861000	10.719578
9.290945	724.375554	10.724595
9.213631	733.145761	10.729613
9.575466	728.160576	10.734631
9.381987	742.699692	10.739648
9.369368	737.928469	10.744666
9.460576	735.880842	10.749683
9.027095	730.864761	10.754701
9.265888	732.185809	10.759719
9.377060	739.737475	10.764736
9.372891	737.147406	10.769754
9.697483	735.033576	10.774771
9.342446	738.043808	10.779789
9.565285	737.715230	10.784807
9.759759	737.009088	10.789824
9.633825	723.805151	10.794842
9.806809	706.883834	10.799859
9.088122	718.603768	10.804877
9.374431	711.690658	10.809895
9.278668	713.026159	10.814912
9.639427	726.249935	10.819930
9.607178	717.746752	10.824947
9.134721	712.808387	10.829965
9.536808	712.189120	10.834983
9.800978	730.213258	10.840000
9.488279	728.370301	10.845018
9.729617	716.910175	10.850035
9.381813	707.686460	10.855053
9.577029	716.694191	10.860071
9.500849	723.426922	10.865088
9.452285	722.748032	10.870106
10.076665	724.524098	10.875123
9.300990	722.804259	10.880141
9.512194	726.077793	10.885159
9.875199	732.709460	10.890176
10.052663	733.547777	10.895194
9.756862	720.129072	10.900211
9.285928	712.563049	10.905229
9.110480	709.346266	10.910247
9.705441	717.439036	10.915264
9.919921	728.820610	10.920282
9.969329	712.637425	10.925299
9.696553	710.558739	10.930317
9.868645	706.146681	10.935335
9.596241	708.285008	10.940352
9.385505	709.122254	10.945370
9.824689	722.112581	10.950387
9.545737	718.234235	10.955405
9.698592	722.245733	10.960423
9.943873	725.534095	10.965440
9.890167	730.094336	10.970458
9.825276	715.897284	10.975475
9.541914	714.236074	10.980493
9.857211	720.467786	10.985511
9.777301	719.143731	10.990528
9.534000	726.920613	10.995546
9.626827	725.925808	11.000563
9.915358	735.731830	11.005581
9.791565	735.862202	11.010599
9.643623	741.020301	11.015616
9.762027	736.660428	11.020634
9.945357	730.202525	11.025651
9.741097	739.078790	11.030669
9.950110	734.834616	11.035687
9.776209	729.273613	11.040704
9.684064	738.835210	11.045722
9.527542	727.984625	11.050739
9.621878	739.367992	11.055757
9.424210	736.024575	11.060775
9.344763	731.130569	11.065792
9.483719	753.332709	11.070810
9.882773	760.815851	11.075827
10.005734	770.910320	11.080845
9.915578	765.344098	11.085863
10.171238	765.340776	11.090880
9.996623	766.279518	11.095898
10.147249	766.019194	11.100915
10.344733	762.027301	11.105933
10.029246	769.190995	11.110951
10.337523	761.830548	11.115968
10.275411	750.755271	11.120986
10.250299	734.945406	11.126003
9.795336	739.840188	11.131021
9.909765	724.604830	11.136039
10.246268	723.255521	11.141056
9.907157	730.188083	11.146074
10.086034	719.320941	11.151091
10.205489	726.119305	11.156109
10.131332	733.294200	11.161127
10.223620	719.407712	11.166144
9.762982	729.712957	11.171162
9.747866	741.476633	11.176179
10.346979	757.309242	11.181197
10.396966	763.840400	11.186215
10.285034	755.562585	11.191232
10.083385	743.266787	11.196250
10.073041	722.933881	11.201267
10.218168	743.119747	11.206285
10.365266	753.623571	11.211303
10.426420	745.785183	11.216320
10.091625	729.281370	11.221338
10.075068	719.000494	11.226355
10.289543	734.215708	11.231373
10.302204	741.511262	11.236391
10.182511	732.240312	11.241408
9.958956	739.428138	11.246426
10.461689	748.905409	11.251443
10.656692	752.180449	11.256461
10.306974	738.521063	11.261479
10.561995	723.864361	11.266496
10.110827	729.384065	11.271514
10.605534	720.099570	11.276531
10.415080	727.821641	11.281549
10.062988	730.193625	11.286567
10.373618	722.776905	11.291584
10.055250	728.884426	11.296602
10.638470	738.831013	11.301619
10.442853	734.292444	11.306637
10.202108	735.963353	11.311655
10.392354	731.143581	11.316672
10.354751	747.967781	11.321690
10.601263	741.740342	11.326707
10.473918	754.265089	11.331725
10.394566	742.848990	11.336743
10.622172	737.532506	11.341760
10.300556	737.722799	11.346778
10.293285	741.743889	11.351795
10.710215	750.837360	11.356813
10.317843	757.173669	11.361831
10.899185	748.607448	11.366848
10.335969	739.311122	11.371866
10.715769	737.077921	11.376883
10.671576	737.107716	11.381901
10.267132	730.492430	11.386919
10.567033	726.260766	11.391936
10.619388	730.158994	11.396954
10.719200	726.233281	11.401971
10.594906	723.614682	11.406989
10.254153	727.933888	11.412007
10.822182	747.190727	11.417024
10.503937	740.996966	11.422042
10.814528	747.347965	11.427059
10.729911	731.795186	11.432077
10.297748	727.009190	11.437095
10.588858	737.372234	11.442112
10.107058	766.031542	11.447130
10.338064	750.781187	11.452147
10.634119	756.839338	11.457165
10.687323	763.278236	11.462183
10.703397	752.332523	11.467200
10.463001	761.125419	11.472218
10.718097	750.499163	11.477235
10.784371	761.682874	11.482253
10.612214	757.622276	11.487271
10.720148	753.505458	11.492288
10.538929	759.669017	11.497306
10.842162	763.778453	11.502323
10.795975	753.440260	11.507341
10.443443	763.809906	11.512359
10.896440	749.499510	11.517376
10.468953	767.914189	11.522394
10.656614	760.634736	11.527411
10.840557	758.989050	11.532429
10.759551	764.744700	11.537447
10.676535	756.329819	11.542464
10.797534	774.817456	11.547482
11.257567	770.571074	11.552499
11.300976	758.376411	11.557517
10.765724	753.890138	11.562535
10.772379	757.853811	11.567552
10.745427	755.351365	11.572570
10.974426	744.736127	11.577587
10.975689	753.680725	11.582605
10.593844	756.180074	11.587623
11.198351	763.843752	11.592640
11.097662	766.904781	11.597658
10.965428	755.275001	11.602675
10.960656	753.596789	11.607693
10.870093	755.660526	11.612711
11.112095	757.862097	11.617728
10.840847	757.609821	11.622746
11.266871	770.461825	11.627763
11.161266	758.016655	11.632781
11.193857	759.662778	11.637799
11.441977	750.044314	11.642816
11.112010	758.102083	11.647834
11.269607	755.570259	11.652851
11.328145	759.028518	11.657869
10.887854	758.584561	11.662887
11.204894	748.471249	11.667904
10.985266	758.313795	11.672922
11.268631	751.721214	11.677939
11.314051	752.102291	11.682957
11.038651	751.445214	11.687975
11.090829	753.381384	11.692992
10.856098	756.459488	11.698010
10.855498	750.054867	11.703027
10.875654	749.501597	11.708045
10.970327	767.708167	11.713063
11.670985	772.832446	11.718080
11.017108	763.494822	11.723098
11.370281	758.250053	11.728115
11.194910	749.812282	11.733133
11.211041	754.400728	11.738151
11.686430	753.668934	11.743168
11.320192	760.572539	11.748186
11.079189	748.606858	11.753203
11.280121	749.275552	11.758221
10.870875	752.164455	11.763239
11.201545	764.437394	11.768256
11.695429	770.431299	11.773274
11.488669	771.615509	11.778291
11.501752	757.231895	11.783309
11.184751	759.990570	11.788327
11.318743	754.647852	11.793344
11.565131	760.725252	11.798362
11.242393	766.755956	11.803379
11.457362	755.083645	11.808397
11.318477	764.369941	11.813415
11.340272	768.346464	11.818432
11.472120	774.541255	11.823450
11.658115	774.569939	11.828467
11.502273	760.772924	11.833485
11.163577	755.913965	11.838503
11.444828	756.351655	11.843520
11.781762	765.192648	11.848538
11.549031	767.470468	11.853555
11.080778	754.559002	11.858573
11.278567	767.959791	11.863591
11.048186	771.141109	11.868608
11.332983	771.306181	11.873626
11.428824	767.659446	11.878643
11.799131	772.798665	11.883661
11.497759	782.800817	11.888679
11.477393	775.101891	11.893696
11.638632	777.889248	11.898714
11.310950	778.978921	11.903731
11.691255	773.751307	11.908749
11.563703	775.112155	11.913767
11.710972	774.837820	11.918784
11.732922	767.740912	11.923802
11.501330	770.206328	11.928819
11.568136	772.932948	11.933837
11.389773	777.317398	11.938855
11.457962	775.079888	11.943872
11.716600	779.493547	11.948890
11.582885	790.828892	11.953907
11.644560	776.463984	11.958925
11.776248	785.770447	11.963943
11.766255	795.828290	11.968960
11.828433	794.090565	11.973978
11.593804	787.130223	11.978995
11.996275	798.690158	11.984013
11.738130	798.347527	11.989031
11.811948	801.290302	11.994048
12.043731	789.965948	11.999066
11.840652	794.816676	12.004083
11.946987	772.719989	12.009101
11.762782	777.348307	12.014119
11.649665	778.515831	12.019136
11.819630	780.516353	12.024154
12.077869	797.650656	12.029171
11.938057	791.762349	12.034189
11.906086	784.751130	12.039207
11.998897	775.493389	12.044224
12.101916	769.897540	12.049242
11.691722	768.800997	12.054259
11.920003	770.114340	12.059277
12.082508	784.057176	12.064295
12.240169	787.485644	12.069312
12.036062	775.403602	12.074330
11.564764	779.218483	12.079347
12.086699	784.795172	12.084365
11.806189	803.674113	12.089383
11.952559	800.936671	12.094400
12.579680	800.805701	12.099418
12.336290	796.915541	12.104435
12.261476	770.972682	12.109453
11.887372	777.997275	12.114471
11.965110	773.405163	12.119488
12.134461	770.917057	12.124506
11.961368	779.750391	12.129523
12.331577	772.288351	12.134541
11.924465	776.085516	12.139559
12.025033	776.433841	12.144576
12.006277	772.672230	12.149594
11.730827	793.130154	12.154611
12.297562	793.631985	12.159629
12.420111	799.890134	12.164647
12.430630	796.723637	12.169664
11.999622	782.528883	12.174682
11.933461	796.396608	12.179699
12.291197	807.195100	12.184717
12.312431	805.646427	12.189735
12.155895	806.606586	12.194752
12.360564	803.847680	12.199770
12.041946	802.359219	12.204787
12.346802	793.174224	12.209805
12.499808	803.657420	12.214823
12.334417	804.326542	12.219840
12.756109	801.112037	12.224858
12.204211	804.943026	12.229875
12.584005	797.943535	12.234893
12.261266	789.626596	12.239911
12.391992	799.754049	12.244928
12.498981	790.374666	12.249946
12.586692	786.613925	12.254963
12.360611	778.495542	12.259981
12.098076	778.108759	12.264999
12.383547	789.051087	12.270016
12.467155	796.925439	12.275034
12.504547	801.500536	12.280051
12.709819	792.726498	12.285069
12.611947	795.024115	12.290087
12.287435	776.641090	12.295104
12.349226	782.185710	12.300122
12.552754	797.414215	12.305139
12.706462	790.891904	12.310157
12.672412	806.477064	12.315175
12.431957	790.807518	12.320192
12.758156	792.005836	12.325210
12.285218	784.913705	12.330227
12.680448	792.144361	12.335245
12.637834	791.055450	12.340263
12.462593	803.142128	12.345280
12.734117	796.959735	12.350298
12.608389	806.075777	12.355315
12.690135	801.151121	12.360333
12.703149	801.217897	12.365351
12.709279	802.149152	12.370368
12.731992	796.128820	12.375386
12.649132	802.460351	12.380403
13.086594	796.075688	12.385421
12.650769	773.875083	12.390439
12.568153	771.866470	12.395456
12.768058	788.758467	12.400474
12.858071	796.493970	12.405491
12.837526	789.065131	12.410509
12.598017	778.338089	12.415527
12.752666	788.563143	12.420544
13.279152	785.017920	12.425562
12.830708	780.661351	12.430579
12.768772	765.490982	12.435597
12.555104	763.431240	12.440615
12.836412	780.044016	12.445632
12.680659	784.282212	12.450650
12.651734	788.594286	12.455667
13.290880	789.693542	12.460685
13.062047	796.264191	12.465703
12.862174	787.649364	12.470720
13.090299	781.232445	12.475738
12.450665	779.953432	12.480755
13.019633	785.046769	12.485773
12.866016	788.596855	12.490791
12.611746	791.308143	12.495808
12.951006	788.976929	12.500826
12.538215	793.725382	12.505843
12.834865	790.599691	12.510861
12.865155	791.270660	12.515879
12.720796	792.590201	12.520896
13.151615	791.808308	12.525914
12.829341	796.175651	12.530931
12.623199	798.015238	12.535949
12.621008	797.209381	12.540967
12.779980	817.460371	12.545984
13.440653	814.318491	12.551002
13.476503	814.535021	12.556019
13.322871	805.675137	12.561037
13.195347	792.007650	12.566055
13.034094	794.375995	12.571072
13.432776	782.670486	12.576090
12.998043	787.824910	12.581107
13.152363	784.839318	12.586125
13.500935	784.979263	12.591143
13.289327	794.142981	12.596160
13.399011	780.363001	12.601178
13.115102	795.780873	12.606195
13.438565	787.737621	12.611213
13.463362	783.340483	12.616231
13.267804	785.721199	12.621248
13.562607	778.700359	12.626266
13.166940	796.076788	12.631283
13.417902	792.039421	12.636301
13.326462	789.372460	12.641319
13.244983	788.510445	12.646336
13.318336	785.144580	12.651354
13.398744	786.709957	12.656371
13.385657	780.096378	12.661389
13.289341	783.861766	12.666407
13.099751	788.676402	12.671424
13.497625	786.803568	12.676442
13.304882	789.700720	12.681459
13.399225	783.542160	12.686477
13.641885	787.622265	12.691495
13.323093	798.507579	12.696512
13.614306	799.158570	12.701530
13.821602	797.203125	12.706547
13.537189	789.793176	12.711565
13.582051	778.266724	12.716583
13.514204	791.500901	12.721600
13.689210	782.359066	12.726618
13.607062	784.103714	12.731635
13.419900	779.820410	12.736653
13.371052	787.220654	12.741671
13.123179	787.890441	12.746688
13.781112	796.233442	12.751706
13.314624	806.781426	12.756723
13.565681	819.815978	12.761741
13.689326	817.719665	12.766759
13.721180	822.077980	12.771776
14.022839	821.248186	12.776794
13.588041	815.659884	12.781811
13.626890	810.695480	12.786829
14.280769	811.794660	12.791847
13.469450	814.956047	12.796864
13.818975	807.594260	12.801882
13.885392	813.143637	12.806899
13.497223	813.738630	12.811917
13.961813	822.681740	12.816935
13.798635	815.852461	12.821952
13.929652	811.194432	12.826970
13.619442	818.321843	12.831987
13.759282	804.758884	12.837005
13.817247	811.956029	12.842023
13.509224	812.900331	12.847040
13.924160	811.638022	12.852058
13.616670	814.006176	12.857075
13.588451	818.843311	12.862093
13.567853	808.945702	12.867111
13.515491	810.192533	12.872128
13.831098	810.865075	12.877146
13.089803	816.963925	12.882163
13.722573	836.334952	12.887181
14.007837	830.060119	12.892199
13.985600	845.599663	12.897216
14.099348	847.340619	12.902234
14.275491	844.767129	12.907251
14.171510	847.392914	12.912269
14.343721	841.530477	12.917287
14.074487	840.769230	12.922304
14.079645	820.538741	12.927322
13.966327	829.979890	12.932339
14.144942	841.193479	12.937357
14.482827	835.212671	12.942375
13.811409	824.698840	12.947392
14.025528	830.896565	12.952410
14.279585	842.255922	12.957427
14.142162	835.935336	12.962445
14.288524	844.370945	12.967463
14.354214	844.326641	12.972480
14.062901	834.298655	12.977498
14.043249	826.474394	12.982515
14.090137	838.021194	12.987533
14.300812	838.278851	12.992551
14.304564	846.321955	12.997568
14.415337	850.339668	13.002586
14.463652	846.972030	13.007603
14.157918	846.040852	13.012621
14.293107	843.988684	13.017639
14.221763	846.898420	13.022656
14.334121	843.414279	13.027674
14.174786	842.555704	13.032691
13.911575	845.101955	13.037709
14.200893	845.757593	13.042727
14.099998	844.981463	13.047744
14.118770	837.598843	13.052762
14.372197	838.437187	13.057779
14.402993	846.949411	13.062797
14.385289	839.679518	13.067815
14.079007	851.375354	13.072832
14.512162	852.797293	13.077850
14.239475	859.817334	13.082867
14.633686	870.512197	13.087885
15.030137	856.135480	13.092903
14.646932	848.247792	13.097920
14.742659	839.037953	13.102938
14.578852	839.853263	13.107955
14.635338	833.351757	13.112973
15.078407	828.043263	13.117991
14.739875	829.940994	13.123008
14.721445	828.552028	13.128026
15.025253	838.179611	13.133043
14.751492	835.347959	13.138061
14.996988	833.220444	13.143079
14.905866	824.651365	13.148096
14.886513	820.198537	13.153114
14.918944	830.696206	13.158131
14.636229	819.116491	13.163149
14.883496	820.362919	13.168167
14.599986	819.551678	13.173184
14.733609	821.785377	13.178202
14.924938	820.113660	13.183219
14.620673	827.475906	13.188237
14.791725	822.096714	13.193255
14.889533	818.340592	13.198272
14.795368	817.251948	13.203290
14.778705	825.620452	13.208307
14.935775	828.353393	13.213325
15.157097	826.190908	13.218343
14.891274	816.434288	13.223360
14.830533	815.711744	13.228378
14.782912	817.745151	13.233395
14.669270	822.255504	13.238413
14.831281	821.328367	13.243431
14.678309	826.449928	13.248448
14.657095	822.904842	13.253466
14.874278	814.260702	13.258483
14.742420	821.503457	13.263501
14.870263	821.337451	13.268519
14.897889	823.493431	13.273536
14.675816	817.906516	13.278554
15.129181	816.444546	13.283571
14.811898	830.460572	13.288589
15.011909	823.923100	13.293607
15.237323	836.282814	13.298624
15.007434	831.697531	13.303642
15.326933	835.722015	13.308659
15.052910	840.621116	13.313677
15.145768	830.975559	13.318695
14.917298	849.743975	13.323712
15.206337	854.012472	13.328730
15.140947	843.436465	13.333747
15.369765	854.145712	13.338765
15.318985	851.720420	13.343783
15.355486	845.531652	13.348800
15.472949	851.209985	13.353818
15.541477	832.520484	13.358835
14.825946	836.553370	13.363853
14.988849	838.099581	13.368871
15.599932	842.200581	13.373888
15.403376	849.596574	13.378906
15.601946	844.287617	13.383923
15.507829	848.862852	13.388941
15.335872	825.683093	13.393959
15.240324	830.832939	13.398976
15.230798	833.807630	13.403994
15.512706	847.286287	13.409011
15.432111	853.371807	13.414029
15.606990	852.716146	13.419047
15.491636	845.791930	13.424064
15.532202	839.181646	13.429082
15.905510	837.556168	13.434099
15.501918	828.992766	13.439117
15.276322	821.728567	13.444135
15.543253	827.294350	13.449152
15.320074	846.653195	13.454170
15.664316	840.289855	13.459187
15.522004	857.313393	13.464205
15.670735	855.786121	13.469223
15.782393	856.233788	13.474240
15.435559	853.171331	13.479258
15.847371	848.678989	13.484275
15.168511	856.447354	13.489293
15.672695	853.229021	13.494311
15.781152	856.930599	13.499328
15.539260	847.576670	13.504346
15.414903	847.917755	13.509363
15.496955	855.282184	13.514381
15.992672	847.042277	13.519399
16.061450	852.521595	13.524416
15.160843	850.997615	13.529434
15.623022	846.067821	13.534451
15.396559	852.231035	13.539469
15.711929	852.949285	13.544487
15.870188	857.070942	13.549504
15.625499	853.548287	13.554522
15.793937	854.042454	13.559539
15.765902	854.454593	13.564557
15.856836	850.594489	13.569575
15.785694	854.153373	13.574592
15.885955	865.173665	13.579610
16.270925	883.180735	13.584627
16.067571	875.370727	13.589645
15.873355	854.033105	13.594663
15.912547	850.143381	13.599680
15.853130	856.340744	13.604698
15.993447	864.692330	13.609715
16.154755	886.830727	13.614733
16.338655	881.752523	13.619751
16.027007	855.663707	13.624768
16.069346	848.600392	13.629786
16.090391	841.281170	13.634803
16.233706	851.467593	13.639821
16.524681	862.050025	13.644839
16.409796	852.501842	13.649856
16.449953	847.469103	13.654874
16.302742	834.933521	13.659891
16.060556	834.948858	13.664909
15.773740	835.318812	13.669927
16.242950	850.024661	13.674944
15.850196	837.154163	13.679962
15.852319	842.244535	13.684979
15.817626	861.034419	13.689997
16.179775	862.609055	13.695015
16.192814	873.477662	13.700032
16.475752	872.964336	13.705050
16.429264	872.325251	13.710067
16.123881	882.971014	13.715085
16.366774	873.951736	13.720103
16.562585	869.954975	13.725120
16.582070	879.027330	13.730138
16.582421	873.413013	13.735155
16.567699	873.420606	13.740173
16.365844	873.221007	13.745191
16.586452	870.548422	13.750208
16.313101	871.238573	13.755226
16.762083	864.628363	13.760243
16.526336	873.060334	13.765261
16.216113	870.955545	13.770279
16.732944	869.938945	13.775296
16.475481	871.422095	13.780314
16.744891	866.859632	13.785331
16.815480	865.133497	13.790349
16.582389	866.671270	13.795367
16.877986	869.614340	13.800384
16.675835	874.964521	13.805402
16.810495	878.497994	13.810419
16.638552	874.741645	13.815437
16.498666	870.236719	13.820455
16.522163	875.142469	13.825472
16.265866	882.510970	13.830490
16.685967	869.288537	13.835507
16.668773	879.099607	13.840525
16.752114	882.599455	13.845543
16.960768	871.578858	13.850560
16.528496	885.106124	13.855578
17.092247	866.880223	13.860595
16.560776	874.173425	13.865613
16.455091	875.870802	13.870631
16.812022	867.500329	13.875648
16.461673	872.311296	13.880666
16.551210	869.612386	13.885683
16.568090	878.168268	13.890701
16.679139	891.653603	13.895719
17.013813	894.369352	13.900736
17.027399	903.771423	13.905754
16.863323	895.427367	13.910771
17.185092	900.801428	13.915789
17.169760	901.733488	13.920807
17.165074	898.011640	13.925824
16.688588	900.101506	13.930842
17.050029	895.100586	13.935859
17.183817	899.000333	13.940877
16.995079	896.460483	13.945895
17.138138	896.197079	13.950912
17.073326	899.409272	13.955930
17.530206	894.863394	13.960947
17.329538	900.834175	13.965965
17.062160	894.385484	13.970983
17.150831	887.897916	13.976000
17.213073	896.904937	13.981018
17.403663	887.430948	13.986035
17.423233	877.244767	13.991053
17.008737	870.531877	13.996071
17.231315	878.903707	14.001088
17.268586	888.126265	14.006106
17.360340	898.009854	14.011123
17.366822	900.641371	14.016141
17.138351	895.814901	14.021159
17.458611	897.099640	14.026176
17.529236	897.549771	14.031194
17.653624	896.563509	14.036211
17.607419	885.611873	14.041229
16.830493	877.765742	14.046247
17.320840	879.260493	14.051264
17.403436	889.628248	14.056282
17.366208	897.275821	14.061299
17.314450	904.620306	14.066317
17.336091	900.542146	14.071335
17.533687	890.972905	14.076352
17.315490	899.911802	14.081370
17.738543	888.915925	14.086387
17.722325	885.769191	14.091405
17.483780	886.324451	14.096423
17.396282	899.041525	14.101440
17.542455	899.798030	14.106458
17.653827	895.898312	14.111475
17.459646	891.401975	14.116493
17.680300	891.850098	14.121511
17.681532	880.118600	14.126528
17.467663	892.382996	14.131546
17.558188	888.505234	14.136563
17.708000	882.474451	14.141581
17.523772	885.534376	14.146599
17.739101	887.354969	14.151616
17.935919	889.805762	14.156634
18.007285	879.570454	14.161651
17.901764	895.683655	14.166669
17.619434	893.714395	14.171687
17.798739	887.311027	14.176704
17.592434	899.272222	14.181722
17.810545	905.168543	14.186739
17.649823	910.551245	14.191757
17.905072	917.563417	14.196775
18.307204	905.430100	14.201792
18.274912	918.349063	14.206810
18.280110	897.421648	14.211827
18.096684	884.280633	14.216845
17.770563	889.999362	14.221863
18.039167	875.502071	14.226880
17.814836	886.081267	14.231898
17.931206	895.012005	14.236915
17.894655	902.588999	14.241933
18.114702	907.783853	14.246951
18.411658	908.034311	14.251968
18.179011	921.968297	14.256986
18.309554	912.294403	14.262003
18.445538	895.333340	14.267021
18.163604	881.923614	14.272039
18.201939	878.057646	14.277056
17.848355	889.040511	14.282074
18.070238	903.886967	14.287091
18.467551	903.838537	14.292109
18.331662	914.952689	14.297127
18.390915	914.144132	14.302144
18.115035	916.109842	14.307162
18.306888	913.968365	14.312179
18.259727	918.493327	14.317197
18.077738	926.766826	14.322215
17.960931	920.447908	14.327232
17.987164	917.702388	14.332250
18.264296	928.222986	14.337267
18.651741	910.606124	14.342285
18.416324	917.258618	14.347303
18.190516	910.946336	14.352320
18.477483	910.392580	14.357338
18.130171	915.060939	14.362355
18.693696	907.067634	14.367373
18.381327	915.221777	14.372391
18.789531	910.149334	14.377408
18.445733	918.420489	14.382426
18.246524	922.178539	14.387443
18.549007	926.171220	14.392461
18.771286	950.620375	14.397479
19.105880	934.017311	14.402496
18.794243	921.932882	14.407514
18.798405	915.644721	14.412531
18.955250	912.985836	14.417549
18.901363	919.092155	14.422567
18.813970	902.638130	14.427584
18.954107	904.571564	14.432602
18.848316	912.167902	14.437619
18.931482	904.139184	14.442637
18.511412	915.749191	14.447655
18.721268	904.822067	14.452672
18.672042	912.474390	14.457690
18.560028	904.313432	14.462707
19.026922	903.411787	14.467725
18.642113	911.331478	14.472743
18.679921	907.306936	14.477760
18.756391	921.856242	14.482778
18.907294	934.896453	14.487795
19.278389	939.505307	14.492813
19.080713	933.925727	14.497831
19.332443	925.868692	14.502848
19.186376	921.798613	14.507866
19.133406	907.067151	14.512883
18.971521	902.095800	14.517901
18.796477	904.947525	14.522919
18.825950	913.870616	14.527936
18.894344	920.891291	14.532954
19.084389	933.924232	14.537971
19.453003	927.944993	14.542989
18.815030	931.127696	14.548007
19.329283	937.537173	14.553024
19.329738	935.592339	14.558042
19.216868	932.551359	14.563059
19.380210	928.658380	14.568077
19.320472	933.427151	14.573095
19.442777	935.917454	14.578112
19.782866	935.220261	14.583130
19.229265	921.832256	14.588147
19.509705	902.157231	14.593165
19.206160	904.908586	14.598183
19.170505	894.549263	14.603200
19.115007	913.298564	14.608218
18.921623	923.534094	14.613235
19.352869	921.491159	14.618253
19.568753	929.807828	14.623271
19.292844	922.249170	14.628288
19.313981	927.225403	14.633306
19.202536	926.489990	14.638323
19.571409	924.263691	14.643341
19.115711	931.829005	14.648359
19.570818	922.964709	14.653376
19.527903	923.285223	14.658394
19.326932	932.901178	14.663411
19.415156	929.642263	14.668429
19.478863	951.735501	14.673447
19.795791	961.262174	14.678464
19.801787	958.572357	14.683482
19.665225	959.547327	14.688499
20.026394	959.430082	14.693517
19.802576	960.939164	14.698535
19.638970	944.546137	14.703552
19.937922	940.822031	14.708570
19.619458	945.772223	14.713587
19.774127	951.195624	14.718605
19.789346	962.587532	14.723623
19.657806	959.140207	14.728640
19.833635	958.645795	14.733658
20.126162	957.641136	14.738675
20.372663	949.219616	14.743693
20.084664	950.733026	14.748711
19.653390	941.374966	14.753728
19.881201	942.142364	14.758746
19.996581	958.951698	14.763763
20.273956	961.777730	14.768781
19.923761	964.112822	14.773799
19.868187	957.790836	14.778816
19.963805	947.475093	14.783834
20.047730	955.194362	14.788851
20.533249	948.077302	14.793869
20.480960	955.587640	14.798887
20.320156	934.947886	14.803904
20.420459	919.128088	14.808922
19.823357	922.229615	14.813939
20.157124	915.809321	14.818957
19.843827	933.335249	14.823975
20.243402	933.371480	14.828992
20.375799	947.991468	14.834010
20.317024	955.126912	14.839027
20.396321	947.540525	14.844045
20.193598	955.345052	14.849063
20.329336	949.279962	14.854080
20.513542	944.701271	14.859098
20.392429	953.511924	14.864115
20.564037	951.124199	14.869133
20.642552	952.694631	14.874151
20.311651	944.287230	14.879168
20.534215	943.759490	14.884186
20.357496	945.321399	14.889203
20.330842	936.625839	14.894221
20.448927	946.468487	14.899239
20.302366	951.434703	14.904256
20.549167	949.572693	14.909274
20.309485	953.437448	14.914291
20.538186	948.712418	14.919309
20.700123	946.312909	14.924327
20.723757	948.460907	14.929344
20.835775	949.641950	14.934362
20.679356	949.458841	14.939379
20.721039	940.838180	14.944397
20.554962	943.173489	14.949415
20.561111	942.801264	14.954432
20.523717	943.047246	14.959450
20.400189	953.285402	14.964467
20.533337	946.043233	14.969485
20.541246	955.439584	14.974503
20.426553	946.233422	14.979520
20.616267	958.815672	14.984538
20.738834	974.300267	14.989555
21.167223	969.897269	14.994573
21.047077	964.490658	14.999591
21.069400	975.640071	15.004608
21.432108	972.876620	15.009626
21.117324	962.046564	15.014643
21.143138	943.993895	15.019661
20.816553	936.060173	15.024679
21.075832	933.467391	15.029696
21.021761	936.981737	15.034714
21.101855	937.116930	15.039731
21.207836	931.823275	15.044749
21.111708	933.064765	15.049767
20.810157	942.355663	15.054784
21.056529	942.421200	15.059802
21.016296	961.314087	15.064819
21.465400	963.466042	15.069837
21.582325	964.865555	15.074855
21.169727	958.767640	15.079872
21.278257	953.120421	15.084890
21.172803	971.041879	15.089907
21.589811	965.393181	15.094925
21.397737	950.046943	15.099943
21.084125	953.063348	15.104960
21.227398	948.653237	15.109978
21.344475	966.719724	15.114995
21.036324	961.780447	15.120013
20.967461	963.158364	15.125031
21.143214	964.693012	15.130048
21.681104	955.384693	15.135066
21.601488	956.157723	15.140083
21.394643	958.409631	15.145101
21.578024	954.125943	15.150119
21.479063	953.601051	15.155136
21.943862	956.205505	15.160154
21.724840	962.877744	15.165171
21.738695	959.757903	15.170189
21.601131	965.435989	15.175207
21.514821	966.149894	15.180224
21.538579	959.821070	15.185242
21.817024	961.985536	15.190259
21.770857	962.768775	15.195277
21.788229	961.653778	15.200295
21.866444	959.215771	15.205312
22.091706	958.428934	15.210330
21.814985	962.297856	15.215347
21.673224	961.264718	15.220365
22.028694	964.050656	15.225383
21.901113	960.979824	15.230400
21.690226	960.108126	15.235418
21.620176	961.052006	15.240435
21.783943	955.242890	15.245453
21.706084	967.062795	15.250471
21.356455	964.072429	15.255488
21.818181	969.738287	15.260506
21.972106	982.028857	15.265523
22.239180	991.858674	15.270541
22.228578	985.304043	15.275559
22.158520	984.028331	15.280576
22.015058	964.209648	15.285594
22.331702	980.869937	15.290611
22.325923	970.835131	15.295629
22.181915	958.219787	15.300647
22.079505	961.645690	15.305664
21.886532	964.559054	15.310682
22.329747	966.390738	15.315699
22.400370	978.644314	15.320717
22.639117	984.845110	15.325735
22.070458	977.996682	15.330752
22.438912	960.154965	15.335770
22.314143	953.780267	15.340787
22.413109	961.666727	15.345805
22.400440	963.026284	15.350823
22.299455	969.714413	15.355840
22.610523	975.056022	15.360858
22.460710	972.511682	15.365875
22.106907	980.308562	15.370893
22.708915	978.110972	15.375911
22.436925	987.563531	15.380928
22.588098	983.939865	15.385946
22.448947	992.021667	15.390963
22.376907	985.141002	15.395981
22.750161	982.025817	15.400999
22.584650	983.818148	15.406016
22.470575	976.542495	15.411034
22.588034	997.538360	15.416051
22.412804	982.494013	15.421069
22.547906	983.770838	15.426087
22.220484	978.057220	15.431104
22.828103	981.388392	15.436122
22.851879	980.454216	15.441139
22.614355	980.086907	15.446157
22.676849	980.108090	15.451175
22.267363	982.364030	15.456192
22.994191	991.586245	15.461210
22.867457	1005.403954	15.466227
22.895346	1012.266423	15.471245
22.978961	1004.834799	15.476263
22.814417	1014.407373	15.481280
23.322479	1002.796969	15.486298
23.047038	1007.273540	15.491315
23.172835	1002.247041	15.496333
23.267879	1008.105909	15.501351
23.185853	1002.007173	15.506368
23.352081	975.892959	15.511386
23.186609	976.987280	15.516403
22.993259	973.773406	15.521421
23.227541	960.598198	15.526439
23.170225	965.202805	15.531456
23.202829	961.731843	15.536474
22.917023	957.363646	15.541491
23.171352	983.317718	15.546509
23.545868	990.727481	15.551527
23.039656	991.918773	15.556544
23.049199	992.463665	15.561562
23.413772	992.939139	15.566579
23.488986	996.642713	15.571597
23.074036	987.406720	15.576615
23.223254	995.035279	15.581632
23.722940	999.625616	15.586650
23.318177	997.908495	15.591667
23.400609	989.719624	15.596685
23.781334	990.273917	15.601703
23.172505	995.822182	15.606720
23.387191	993.209216	15.611738
23.470167	994.717105	15.616755
23.132242	1004.275863	15.621773
23.603184	993.753066	15.626791
23.297835	998.590871	15.631808
23.607735	992.315436	15.636826
23.388915	999.315991	15.641843
23.201270	1009.137652	15.646861
23.632949	1013.787283	15.651879
23.874025	1022.201795	15.656896
23.889999	1018.103284	15.661914
24.061213	1015.680970	15.666931
24.200991	1016.890097	15.671949
24.007993	995.605618	15.676967
23.709332	991.901717	15.681984
23.780972	990.500972	15.687002
23.941460	988.705610	15.692019
23.767091	1014.120507	15.697037
24.228812	1010.556040	15.702055
23.910898	1023.907803	15.707072
24.075656	1016.919807	15.712090
24.422337	1010.393796	15.717107
24.027010	997.565714	15.722125
24.131128	983.300667	15.727143
24.075932	986.286886	15.732160
24.170414	985.985070	15.737178
24.319347	993.090469	15.742195
23.942166	991.347916	15.747213
24.108763	987.629967	15.752231
24.008691	1009.829932	15.757248
23.864936	1018.509731	15.762266
24.053377	1010.388725	15.767283
24.023512	1016.761567	15.772301
24.596376	1016.328965	15.777319
24.339296	1008.286850	15.782336
24.326928	1019.392828	15.787354
24.699543	1015.021099	15.792371
24.462564	1020.200725	15.797389
24.564302	1012.412567	15.802407
24.669346	1018.425289	15.807424
24.266035	1022.476992	15.812442
24.701110	1009.231882	15.817459
24.537809	1021.701384	15.822477
24.594916	1012.987187	15.827495
24.653733	1020.812611	15.832512
24.795060	1022.544690	15.837530
24.783052	1018.758280	15.842547
24.615397	1011.999336	15.847565
24.946406	1011.366634	15.852583
24.621135	1011.633120	15.857600
24.483386	1015.038116	15.862618
24.522502	1008.715390	15.867635
24.755121	1020.061107	15.872653
25.052173	999.780082	15.877671
24.937146	1014.030488	15.882688
24.869435	1011.746945	15.887706
24.730330	1007.961112	15.892723
24.709628	1004.913123	15.897741
24.942223	1007.049363	15.902759
24.683492	1010.435809	15.907776
24.783949	1014.152923	15.912794
24.884275	1003.082849	15.917811
24.934787	1018.708943	15.922829
25.026964	1013.929731	15.927847
24.758715	1014.838718	15.932864
24.849811	1005.957880	15.937882
25.062980	1008.514642	15.942899
24.838310	1021.826557	15.947917
24.842603	1012.790409	15.952935
24.816979	1022.938781	15.957952
24.820450	1033.957898	15.962970
25.207650	1027.893657	15.967987
25.217117	1021.220731	15.973005
25.316697	1032.962488	15.978023
25.172583	1036.764196	15.983040
25.028410	1030.454489	15.988058
25.483146	1034.609776	15.993075
25.428051	1034.891367	15.998093
25.584070	1026.160391	16.003111
25.193617	1032.088241	16.008128
25.296353	1032.033079	16.013146
25.385108	1024.787201	16.018163
25.235285	1028.631191	16.023181
25.711270	1035.026181	16.028199
25.437795	1036.518296	16.033216
25.310295	1032.363619	16.038234
25.941017	1020.793519	16.043251
25.517012	1024.949433	16.048269
25.633303	1025.081783	16.053287
25.573217	1027.823947	16.058304
25.727140	1042.674703	16.063322
25.800844	1038.465844	16.068339
25.555482	1042.953585	16.073357
25.764139	1047.248832	16.078375
25.724191	1051.043138	16.083392
25.646842	1056.029028	16.088410
26.108654	1051.379143	16.093427
26.101045	1057.506592	16.098445
26.102842	1051.614028	16.103463
25.934332	1049.017655	16.108480
25.798722	1054.600965	16.113498
26.262250	1047.670566	16.118515
26.305757	1042.984440	16.123533
25.675780	1025.722521	16.128551
25.928816	1036.107033	16.133568
26.016337	1051.136109	16.138586
26.417616	1051.482678	16.143603
26.248014	1048.308948	16.148621
25.956197	1046.982159	16.153639
26.290456	1048.124048	16.158656
26.234775	1047.380183	16.163674
26.612262	1049.342442	16.168691
26.344224	1032.711111	16.173709
26.582867	1022.180697	16.178727
26.000754	1014.973470	16.183744
26.003107	1020.673682	16.188762
26.101486	1033.916761	16.193779
26.426329	1044.224036	16.198797
26.349918	1049.064498	16.203815
26.452621	1040.134083	16.208832
26.263360	1042.515370	16.213850
26.311618	1043.065269	16.218867
26.469698	1050.662075	16.223885
26.259675	1037.951696	16.228903
26.354508	1040.627267	16.233920
26.363947	1043.241391	16.238938
26.599345	1039.541170	16.243955
26.168862	1046.814973	16.248973
26.066335	1047.863051	16.253991
26.326802	1061.017112	16.259008
26.789645	1072.344037	16.264026
26.818584	1069.644102	16.269043
26.848244	1076.374422	16.274061
26.817951	1073.509891	16.279079
27.020596	1068.105699	16.284096
26.957080	1068.391440	16.289114
27.097624	1059.516557	16.294131
26.726830	1068.172562	16.299149
26.777102	1068.222540	16.304167
27.308959	1065.850341	16.309184
26.830437	1063.011214	16.314202
27.046564	1062.685317	16.319219
27.090111	1065.272538	16.324237
26.956854	1065.694625	16.329255
27.294447	1056.367052	16.334272
27.162530	1066.555886	16.339290
27.061897	1054.532079	16.344307
27.113033	1059.967544	16.349325
27.240735	1068.955953	16.354343
27.102044	1064.220464	16.359360
26.831482	1071.179227	16.364378
27.027085	1060.182309	16.369395
27.095368	1061.956408	16.374413
27.238805	1065.278243	16.379431
27.390639	1061.614687	16.384448
27.059830	1071.859292	16.389466
27.183657	1065.038281	16.394483
27.311112	1085.241301	16.399501
27.543442	1096.712708	16.404519
27.859179	1094.039294	16.409536
27.409895	1083.881794	16.414554
27.602754	1081.189754	16.419571
27.920225	1080.352605	16.424589
27.652892	1068.070573	16.429607
27.887628	1061.231199	16.434624
27.593301	1060.195759	16.439642
27.249481	1055.082837	16.444659
27.449732	1064.782038	16.449677
27.589498	1080.042247	16.454695
28.067618	1084.807041	16.459712
27.811645	1092.933829	16.464730
27.921785	1082.620709	16.469747
28.069810	1097.164238	16.474765
27.854425	1094.169727	16.479783
28.212994	1080.482516	16.484800
27.983555	1073.912903	16.489818
28.056851	1056.932517	16.494835
28.158259	1053.472975	16.499853
27.712291	1058.057715	16.504871
27.890898	1058.786024	16.509888
27.714457	1069.479459	16.514906
28.386557	1077.169505	16.519923
28.208053	1092.263142	16.524941
27.967101	1079.543283	16.529959
28.199131	1081.587111	16.534976
28.022123	1089.312252	16.539994
28.254215	1082.335517	16.545011
28.435807	1078.541838	16.550029
28.183691	1080.185139	16.555047
28.474144	1082.345666	16.560064
27.990276	1082.182131	16.565082
28.407098	1078.433751	16.570099
28.065511	1081.730392	16.575117
28.294044	1085.884568	16.580135
28.344159	1074.057430	16.585152
28.411119	1078.473389	16.590170
28.273495	1079.133593	16.595187
28.432756	1086.538102	16.600205
28.284934	1087.346447	16.605223
28.367734	1076.690232	16.610240
28.238964	1084.978230	16.615258
28.633530	1092.315828	16.620275
28.695137	1100.698292	16.625293
28.785445	1102.578981	16.630311
28.686389	1098.685315	16.635328
28.826976	1105.689790	16.640346
28.693304	1103.868715	16.645363
28.846762	1106.355856	16.650381
29.142706	1105.936824	16.655399
28.952901	1087.139008	16.660416
28.649910	1089.345440	16.665434
28.953037	1085.375341	16.670451
29.126393	1105.221980	16.675469
28.824815	1099.228455	16.680487
29.017750	1094.191598	16.685504
29.068703	1096.716182	16.690522
29.192655	1095.766592	16.695539
29.272370	1093.929476	16.700557
29.211186	1096.421843	16.705575
29.156952	1088.381923	16.710592
29.179469	1098.283011	16.715610
29.176394	1096.903683	16.720627
29.306482	1092.076044	16.725645
29.086315	1110.672935	16.730663
29.385001	1097.809377	16.735680
29.344495	1100.216040	16.740698
29.417270	1102.200022	16.745715
29.359457	1098.945963	16.750733
29.178547	1103.336832	16.755751
29.115648	1100.455255	16.760768
29.339735	1106.245944	16.765786
29.650403	1098.823134	16.770803
29.528612	1094.304121	16.775821
29.616575	1108.029681	16.780839
29.480066	1094.244519	16.785856
29.405380	1092.963266	16.790874
29.066447	1099.567627	16.795891
29.417721	1097.895381	16.800909
29.280534	1104.269100	16.805927
29.751755	1106.739057	16.810944
29.635772	1122.115275	16.815962
29.873004	1132.541050	16.820979
29.737629	1126.284568	16.825997
29.875511	1128.142817	16.831015
30.050473	1120.687351	16.836032
29.885910	1127.409302	16.841050
29.707454	1123.935458	16.846067
30.119958	1126.098222	16.851085
29.769732	1117.928957	16.856103
29.823665	1116.258700	16.861120
29.561549	1121.892114	16.866138
29.323636	1117.637197	16.871155
29.742480	1122.946840	16.876173
29.924462	1143.433417	16.881191
30.400087	1145.929816	16.886208
30.393714	1148.590669	16.891226
30.668398	1141.808817	16.896243
30.508206	1126.602789	16.901261
30.440088	1122.063071	16.906279
30.449100	1107.471543	16.911296
30.345097	1112.665007	16.916314
30.413891	1113.667793	16.921331
30.662642	1108.555155	16.926349
30.147015	1109.950764	16.931367
30.393947	1113.970015	16.936384
30.281475	1112.548565	16.941402
30.218013	1115.621214	16.946419
30.317088	1119.523222	16.951437
30.248119	1136.679800	16.956455
30.802150	1134.523598	16.961472
30.582608	1138.140977	16.966490
30.611948	1144.400134	16.971507
30.841489	1137.148214	16.976525
30.700878	1142.650496	16.981543
30.616082	1143.612970	16.986560
30.747454	1140.987792	16.991578
30.731239	1146.761988	16.996595
30.788507	1137.170163	17.001613
30.518112	1142.911251	17.006631
31.004140	1135.386162	17.011648
31.018021	1147.851623	17.016666
31.001310	1135.885113	17.021683
31.021997	1127.197355	17.026701
31.063047	1139.627603	17.031719
31.011506	1135.478431	17.036736
31.170131	1130.459053	17.041754
31.014516	1136.055940	17.046771
30.954662	1133.342352	17.051789
30.950896	1143.213176	17.056807
31.190926	1136.329981	17.061824
31.047028	1134.377135	17.066842
30.944138	1143.305347	17.071859
31.359342	1143.932282	17.076877
31.339211	1158.829293	17.081895
31.462962	1161.693398	17.086912
31.649277	1172.748479	17.091930
31.501566	1162.544535	17.096947
31.500281	1159.726364	17.101965
31.708130	1168.444482	17.106983
31.963907	1140.574662	17.112000
31.527885	1143.465313	17.117018
31.368621	1134.185319	17.122035
31.869354	1124.471254	17.127053
31.496089	1128.884926	17.132071
31.380829	1130.729974	17.137088
31.576868	1148.733208	17.142106
31.823826	1156.860609	17.147123
31.752289	1162.602635	17.152141
31.895281	1169.473673	17.157159
31.975611	1160.011870	17.162176
31.885925	1161.686156	17.167194
31.965275	1164.231246	17.172211
31.860528	1151.740341	17.177229
31.765639	1165.761575	17.182247
31.960405	1159.550019	17.187264
31.713152	1156.049370	17.192282
31.821808	1162.973334	17.197299
31.918502	1156.138667	17.202317
31.634553	1169.020771	17.207335
31.866551	1165.062824	17.212352
32.174911	1159.231266	17.217370
32.041793	1165.813386	17.222387
32.179716	1169.843615	17.227405
31.968134	1185.629414	17.232423
32.371869	1182.594574	17.237440
32.587012	1183.131806	17.242458
32.141221	1184.880807	17.247475
32.557130	1179.344416	17.252493
32.403851	1187.457792	17.257511
32.605794	1186.314580	17.262528
32.742783	1183.789249	17.267546
32.614257	1182.774770	17.272563
32.799209	1171.347266	17.277581
32.667246	1161.192682	17.282599
33.022241	1151.342107	17.287616
32.822690	1148.579602	17.292634
32.644252	1148.899334	17.297651
32.969837	1137.057636	17.302669
32.752094	1147.830402	17.307687
32.662325	1140.702217	17.312704
32.502326	1145.925830	17.317722
32.153193	1146.295478	17.322739
32.368120	1166.927415	17.327757
32.888566	1165.611390	17.332775
32.573379	1178.315610	17.337792
33.033412	1175.432862	17.342810
32.811779	1172.329531	17.347827
33.030142	1170.859201	17.352845
32.882838	1173.426861	17.357863
32.938396	1177.904183	17.362880
32.974831	1177.878109	17.367898
32.739927	1184.361346	17.372915
32.983655	1178.893622	17.377933
33.211141	1201.224263	17.382951
33.436752	1210.135127	17.387968
33.399584	1208.757103	17.392986
33.287707	1202.284895	17.398003
33.543282	1198.318705	17.403021
33.596318	1207.893558	17.408039
33.608633	1198.817786	17.413056
33.715045	1190.013045	17.418074
33.137893	1198.208817	17.423091
33.427850	1193.162161	17.428109
33.425864	1197.146669	17.433127
33.520535	1200.390783	17.438144
33.752806	1198.574850	17.443162
33.560149	1199.712269	17.448179
33.673049	1197.019275	17.453197
33.590856	1201.369417	17.458215
33.527454	1198.928051	17.463232
33.788664	1190.569712	17.468250
33.683865	1203.343050	17.473267
33.824804	1201.211539	17.478285
33.971296	1195.130399	17.483303
33.900845	1196.993232	17.488320
34.079499	1195.746398	17.493338
33.932887	1197.582865	17.498355
33.934881	1197.450686	17.503373
34.019720	1196.143404	17.508391
33.415032	1193.130659	17.513408
33.715349	1198.533181	17.518426
33.726009	1216.196727	17.523443
34.150950	1219.937719	17.528461
34.362484	1222.759349	17.533479
34.445056	1224.887784	17.538496
34.434320	1221.723145	17.543514
34.265588	1225.828181	17.548531
34.396073	1220.404783	17.553549
34.433554	1221.345440	17.558567
34.505869	1226.260934	17.563584
34.361254	1218.375673	17.568602
33.859863	1218.909112	17.573619
34.078973	1213.757255	17.578637
34.390277	1210.486146	17.583655
34.284617	1229.665778	17.588672
35.089130	1231.584913	17.593690
35.217029	1232.632249	17.598707
34.852568	1219.549270	17.603725
35.207602	1205.502308	17.608743
35.105709	1209.726978	17.613760
34.913690	1200.968889	17.618778
34.973111	1206.927429	17.623795
34.964449	1206.041523	17.628813
34.992295	1199.898926	17.633831
35.143059	1193.404099	17.638848
35.099216	1199.269895	17.643866
35.227197	1204.657255	17.648883
35.189271	1198.370042	17.653901
35.063432	1206.035590	17.658919
35.286464	1214.076435	17.663936
35.176012	1198.427465	17.668954
34.806739	1201.884223	17.673971
35.072811	1202.741360	17.678989
34.898106	1200.908958	17.684007
35.143736	1196.389312	17.689024
35.545907	1199.562038	17.694042
35.115365	1198.282614	17.699059
35.174402	1202.272767	17.704077
35.362038	1197.941852	17.709095
35.296389	1203.050258	17.714112
35.537350	1191.257176	17.719130
35.501661	1204.857631	17.724147
34.948731	1203.763034	17.729165
35.022986	1218.813368	17.734183
35.003409	1236.696899	17.739200
35.568489	1231.852701	17.744218
35.605603	1238.770435	17.749235
35.560259	1231.925396	17.754253
35.544326	1232.808757	17.759271
35.495382	1240.665128	17.764288
35.747489	1247.377979	17.769306
35.777254	1263.197909	17.774323
35.985060	1261.784829	17.779341
36.128503	1255.225048	17.784359
36.283738	1257.581214	17.789376
36.332932	1253.209036	17.794394
36.585276	1253.188943	17.799411
36.164591	1228.997424	17.804429
35.702028	1226.172551	17.809447
35.761696	1229.525221	17.814464
36.150237	1246.018385	17.819482
36.009402	1246.433071	17.824499
36.089344	1251.272903	17.829517
36.204454	1254.161291	17.834535
36.091107	1256.290675	17.839552
36.544919	1249.776354	17.844570
36.541187	1259.912594	17.849587
36.439287	1246.610530	17.854605
36.578147	1246.037982	17.859623
36.195438	1249.122181	17.864640
36.450039	1244.404190	17.869658
36.293202	1253.759105	17.874675
36.320006	1249.196151	17.879693
36.442691	1266.754200	17.884711
36.442856	1282.146383	17.889728
37.040171	1285.861999	17.894746
36.839255	1287.390941	17.899763
36.809346	1283.942068	17.904781
37.061380	1282.159860	17.909799
37.345883	1281.241942	17.914816
37.045420	1267.479048	17.919834
36.696066	1247.764169	17.924851
36.685934	1244.958865	17.929869
37.161273	1262.585679	17.934887
36.762726	1280.417840	17.939904
37.155428	1275.303753	17.944922
37.050216	1287.744952	17.949939
37.092806	1275.843711	17.954957
37.422568	1280.005981	17.959975
37.145485	1278.008636	17.964992
37.236219	1269.685175	17.970010
37.135951	1277.185897	17.975027
37.094674	1279.163985	17.980045
37.498655	1274.180705	17.985063
37.375395	1271.559872	17.990080
37.392166	1268.168233	17.995098
37.350039	1274.942021	18.000115
37.386152	1272.534951	18.005133
37.598654	1271.345104	18.010151
37.343181	1271.358702	18.015168
37.236229	1269.537514	18.020186
37.621323	1280.417242	18.025203
37.889066	1296.285988	18.030221
37.919572	1302.056049	18.035239
37.799836	1294.095765	18.040256
37.937012	1288.423209	18.045274
37.877907	1282.657961	18.050291
37.711739	1300.089864	18.055309
38.286318	1293.622849	18.060327
38.004781	1301.559888	18.065344
38.027000	1299.479518	18.070362
38.110143	1299.470118	18.075379
38.212655	1302.955864	18.080397
38.309801	1300.223337	18.085415
37.790478	1292.517008	18.090432
38.089491	1300.863814	18.095450
37.972395	1301.656452	18.100467
37.951582	1307.064548	18.105485
38.076919	1294.140951	18.110503
37.886507	1305.580152	18.115520
38.406094	1302.083990	18.120538
38.215250	1296.321653	18.125555
38.229958	1305.303320	18.130573
38.489755	1314.399131	18.135591
38.312849	1330.246263	18.140608
38.399035	1324.031360	18.145626
38.599109	1334.977982	18.150643
38.595912	1333.463616	18.155661
38.820668	1319.447571	18.160679
38.912602	1326.844053	18.165696
38.798099	1313.822753	18.170714
38.763339	1321.231943	18.175731
38.879181	1318.551040	18.180749
39.221301	1308.776512	18.185767
39.108655	1313.985254	18.190784
39.426478	1318.068411	18.195802
39.356802	1309.188430	18.200819
39.344983	1305.113341	18.205837
39.332714	1284.183963	18.210855
39.038086	1285.807947	18.215872
39.172616	1280.957862	18.220890
38.931399	1275.311352	18.225907
38.701597	1295.413963	18.230925
39.060017	1310.684651	18.235943
39.179741	1314.875016	18.240960
39.379354	1315.679779	18.245978
39.636762	1305.123233	18.250995
39.316961	1321.610934	18.256013
39.361397	1318.072973	18.261031
39.361321	1315.975427	18.266048
39.526483	1313.498165	18.271066
39.766622	1310.612433	18.276083
39.505872	1308.732849	18.281101
39.268358	1310.866660	18.286119
39.659850	1318.437548	18.291136
39.499704	1311.118973	18.296154
39.704337	1309.739091	18.301171
39.467322	1320.682093	18.306189
39.848138	1325.935507	18.311207
39.967659	1331.072742	18.316224
39.862039	1331.694587	18.321242
40.098873	1328.397596	18.326259
39.701113	1324.619079	18.331277
40.083274	1331.662002	18.336295
39.956113	1336.543634	18.341312
39.634228	1323.664536	18.346330
39.702900	1330.276697	18.351347
39.466344	1341.481050	18.356365
40.222645	1337.409081	18.361383
40.007480	1352.550773	18.366400
40.406432	1354.879198	18.371418
40.326337	1363.378179	18.376435
40.330389	1362.040560	18.381453
40.597180	1354.487101	18.386471
40.716481	1365.699083	18.391488
40.436039	1358.260249	18.396506
40.673251	1353.754156	18.401523
40.430183	1359.516782	18.406541
40.650948	1348.363923	18.411559
41.073484	1353.224225	18.416576
40.853841	1353.467319	18.421594
40.849886	1347.679530	18.426611
40.800470	1371.235774	18.431629
40.924234	1354.321113	18.436647
40.976914	1354.554943	18.441664
41.184477	1355.753268	18.446682
41.130061	1351.809234	18.451699
40.797814	1354.945726	18.456717
41.402422	1357.201124	18.461735
41.463974	1351.326504	18.466752
41.379281	1348.935882	18.471770
41.207634	1348.836389	18.476787
41.213266	1354.352326	18.481805
41.207437	1345.346007	18.486823
41.285237	1343.549729	18.491840
40.930065	1352.724161	18.496858
41.214026	1344.347013	18.501875
41.147320	1349.458791	18.506893
41.327982	1350.282836	18.511911
41.281661	1353.206240	18.516928
41.242770	1346.784877	18.521946
41.137506	1356.111629	18.526963
41.625231	1364.238643	18.531981
41.299941	1371.179830	18.536999
41.215085	1385.298025	18.542016
41.482840	1376.924723	18.547034
41.764637	1380.117419	18.552051
41.593610	1379.717829	18.557069
41.519415	1368.435056	18.562087
41.864063	1378.436133	18.567104
41.936200	1395.423572	18.572122
42.293568	1400.181295	18.577139
42.007542	1393.865399	18.582157
42.356957	1380.382194	18.587175
42.019636	1364.100160	18.592192
42.058169	1375.246784	18.597210
42.180491	1378.055262	18.602227
42.217775	1399.066524	18.607245
42.150328	1394.140399	18.612263
42.021456	1389.175628	18.617280
42.198873	1389.497858	18.622298
42.559749	1397.231333	18.627315
42.281655	1400.260050	18.632333
42.330153	1396.946987	18.637351
42.194648	1388.320377	18.642368
42.355735	1401.588427	18.647386
42.593940	1393.986140	18.652403
42.658496	1395.996718	18.657421
42.904546	1387.350237	18.662439
42.689676	1389.285823	18.667456
42.396582	1387.939529	18.672474
42.923107	1390.213766	18.677491
42.764694	1395.889162	18.682509
43.221773	1388.276620	18.687527
43.012671	1387.849476	18.692544
42.563951	1401.965731	18.697562
42.857116	1393.358295	18.702579
43.027268	1415.212527	18.707597
43.446275	1414.906180	18.712615
43.618273	1412.919497	18.717632
43.319064	1406.166808	18.722650
43.122224	1395.450378	18.727667
43.068402	1409.738258	18.732685
43.584566	1409.219370	18.737703
43.542800	1415.762061	18.742720
42.936511	1424.369461	18.747738
43.227603	1417.310368	18.752755
43.630093	1421.304731	18.757773
43.682016	1420.135162	18.762791
43.539914	1420.865411	18.767808
43.579776	1415.331756	18.772826
43.675217	1413.912072	18.777843
43.833263	1413.932002	18.782861
43.858853	1413.761268	18.787879
44.088930	1414.651149	18.792896
43.809594	1420.515472	18.797914
43.983534	1418.136739	18.802931
43.695097	1426.628913	18.807949
43.764395	1424.643092	18.812967
44.106536	1418.679074	18.817984
43.544128	1417.874214	18.823002
44.049494	1415.862646	18.828019
43.711734	1427.342869	18.833037
43.750301	1443.221761	18.838055
43.855173	1444.093006	18.843072
44.244965	1448.196958	18.848090
44.469375	1448.428338	18.853107
44.713650	1448.852883	18.858125
44.477309	1442.502363	18.863143
44.551057	1441.746496	18.868160
44.503951	1440.116950	18.873178
44.846096	1438.294215	18.878195
44.768387	1442.220065	18.883213
44.571755	1436.286982	18.888231
44.916156	1433.916242	18.893248
44.665649	1434.042008	18.898266
44.827003	1433.516122	18.903283
44.829447	1437.484210	18.908301
44.784527	1425.528447	18.913319
45.068855	1428.721915	18.918336
44.843969	1440.090547	18.923354
44.955111	1429.230580	18.928371
44.899375	1424.415891	18.933389
44.893694	1428.895552	18.938407
45.341759	1415.819205	18.943424
45.160949	1428.960428	18.948442
45.425819	1425.922551	18.953459
45.266912	1432.024808	18.958477
44.951620	1428.271980	18.963495
45.104606	1429.902570	18.968512
45.009408	1440.556036	18.973530
45.345576	1446.516089	18.978547
45.275963	1454.116151	18.983565
45.454504	1462.626692	18.988583
45.535334	1456.561440	18.993600
45.093261	1462.509022	18.998618
45.788328	1449.535448	19.003635
45.767279	1453.386566	19.008653
45.376070	1460.389887	19.013671
45.415112	1454.503994	19.018688
45.450941	1451.573721	19.023706
45.940485	1464.295713	19.028723
45.867620	1475.867937	19.033741
45.773847	1483.723192	19.038759
45.837712	1473.389522	19.043776
45.916618	1479.805567	19.048794
45.900293	1479.688230	19.053811
45.815784	1476.377094	19.058829
45.811043	1488.362059	19.063847
45.970951	1470.578302	19.068864
46.242941	1484.815847	19.073882
46.726554	1500.787642	19.078899
46.672638	1491.939198	19.083917
46.302256	1486.514389	19.088935
46.635515	1471.057026	19.093952
46.520155	1473.674564	19.098970
46.743925	1467.865559	19.103987
46.715501	1468.221480	19.109005
46.399907	1471.938303	19.114023
46.707105	1480.342513	19.119040
46.814396	1498.915963	19.124058
47.084470	1495.650442	19.129075
47.072864	1492.846912	19.134093
46.990189	1492.176785	19.139111
46.996636	1487.211231	19.144128
46.969359	1485.829182	19.149146
47.107921	1486.359814	19.154163
47.325653	1491.930838	19.159181
47.261103	1486.120353	19.164199
47.290759	1473.092372	19.169216
47.135872	1475.651888	19.174234
47.201078	1477.635204	19.179251
47.403849	1494.077112	19.184269
47.452715	1502.325684	19.189287
47.600483	1489.225377	19.194304
47.074509	1497.930148	19.199322
47.383319	1493.690111	19.204339
47.290980	1491.081049	19.209357
47.196407	1490.263682	19.214375
47.514599	1488.071681	19.219392
47.736383	1500.897094	19.224410
47.391351	1495.324385	19.229427
47.641264	1496.141302	19.234445
47.675907	1509.358335	19.239463
47.811784	1516.825978	19.244480
47.431454	1529.339696	19.249498
47.671226	1521.926850	19.254515
48.160316	1522.911252	19.259533
47.824704	1518.370039	19.264551
47.606220	1511.422442	19.269568
47.935669	1518.322212	19.274586
48.260843	1530.107308	19.279603
48.387086	1529.214793	19.284621
48.068558	1527.167191	19.289639
48.505908	1530.655814	19.294656
48.499995	1537.081990	19.299674
48.784868	1528.937267	19.304691
48.289828	1521.057905	19.309709
48.257400	1522.060155	19.314727
48.777093	1527.699303	19.319744
48.688755	1540.710742	19.324762
48.878914	1530.347462	19.329779
49.115110	1533.774905	19.334797
48.446612	1530.423839	19.339815
48.735771	1519.291816	19.344832
48.306757	1537.010418	19.349850
48.367782	1534.806268	19.354867
48.550028	1530.373399	19.359885
48.654367	1542.260818	19.364903
48.857516	1532.304438	19.369920
48.885452	1556.959173	19.374938
49.162413	1572.601482	19.379955
49.427277	1568.625786	19.384973
49.498909	1569.803722	19.389991
49.804235	1564.790230	19.395008
49.442787	1543.906900	19.400026
49.457899	1536.015500	19.405043
49.557178	1526.233015	19.410061
49.225923	1546.017711	19.415079
49.434835	1548.694561	19.420096
49.594609	1561.091710	19.425114
49.421343	1566.303881	19.430131
49.502181	1563.418496	19.435149
49.374552	1568.679016	19.440167
49.700640	1559.632181	19.445184
49.434089	1558.865333	19.450202
49.562236	1564.016178	19.455219
49.804615	1572.428415	19.460237
49.989144	1577.611267	19.465255
50.290655	1579.018857	19.470272
50.493911	1584.526563	19.475290
50.284516	1587.400634	19.480307
50.266862	1583.554785	19.485325
50.057368	1585.940291	19.490343
50.140697	1581.831265	19.495360
50.114381	1576.761264	19.500378
49.917103	1576.582943	19.505395
50.220175	1580.726093	19.510413
50.615011	1577.209582	19.515431
50.701638	1559.494944	19.520448
50.754858	1569.437313	19.525466
50.487479	1570.880042	19.530483
50.679061	1564.102318	19.535501
51.065016	1580.422255	19.540519
50.966086	1565.476122	19.545536
50.990803	1570.454726	19.550554
50.530648	1577.630538	19.555571
50.547870	1568.136809	19.560589
50.523442	1596.557745	19.565607
51.082755	1597.979343	19.570624
51.109471	1605.031639	19.575642
51.148202	1603.765816	19.580659
51.246494	1604.409026	19.585677
50.947683	1602.773108	19.590695
51.305953	1600.772882	19.595712
51.279026	1606.193906	19.600730
51.086975	1602.557242	19.605747
51.398470	1596.173823	19.610765
50.904205	1608.792296	19.615783
51.291989	1614.370640	19.620800
51.717133	1628.393195	19.625818
51.930593	1626.735840	19.630835
52.228705	1623.731004	19.635853
52.056688	1626.728027	19.640871
52.405134	1605.495182	19.645888
52.176659	1592.631494	19.650906
51.925549	1587.277451	19.655923
52.165186	1586.773244	19.660941
51.965188	1582.420186	19.665959
52.366347	1573.795164	19.670976
52.339046	1584.246935	19.675994
51.941585	1585.711992	19.681011
52.256186	1576.538309	19.686029
52.250815	1577.042383	19.691047
52.291212	1578.034941	19.696064
52.449981	1581.435845	19.701082
52.567305	1578.118434	19.706099
52.313394	1586.891198	19.711117
52.275171	1580.092070	19.716135
52.412327	1591.049292	19.721152
52.243362	1601.538311	19.726170
52.411174	1614.516849	19.731187
52.607875	1606.363457	19.736205
52.499834	1612.554999	19.741223
52.575851	1608.365681	19.746240
52.589752	1611.876406	19.751258
52.455057	1623.693229	19.756275
52.507111	1634.129533	19.761293
52.928627	1648.552707	19.766311
52.945531	1640.815289	19.771328
53.321293	1645.164138	19.776346
52.931473	1649.716916	19.781363
53.371082	1642.467381	19.786381
53.237789	1639.404839	19.791399
53.296885	1644.591554	19.796416
53.427598	1639.164036	19.801434
53.398695	1636.417674	19.806451
53.565962	1636.193165	19.811469
53.524908	1634.319683	19.816487
53.591502	1648.555168	19.821504
53.610986	1651.897260	19.826522
53.794445	1652.331094	19.831539
53.747858	1651.506560	19.836557
53.662337	1655.143205	19.841575
53.871211	1659.799612	19.846592
54.002674	1659.295598	19.851610
53.646858	1658.881714	19.856627
54.125056	1651.522242	19.861645
54.134278	1652.875479	19.866663
54.148988	1650.375831	19.871680
54.288858	1654.353504	19.876698
53.838075	1660.390398	19.881715
54.255562	1652.542552	19.886733
54.138247	1672.463639	19.891751
54.271027	1683.677164	19.896768
54.758467	1679.536634	19.901786
54.606992	1684.569251	19.906803
54.978405	1677.335717	19.911821
54.705898	1679.522220	19.916839
54.825826	1678.000426	19.921856
55.169445	1670.786851	19.926874
55.289270	1684.410009	19.931891
55.356120	1658.078817	19.936909
54.958784	1651.371007	19.941927
55.083309	1646.392543	19.946944
54.906119	1638.726633	19.951962
54.729185	1648.850861	19.956979
54.821981	1654.956411	19.961997
54.970972	1668.393230	19.967015
55.074151	1668.970672	19.972032
55.562243	1668.949342	19.977050
55.212416	1674.443146	19.982067
55.480027	1683.540638	19.987085
55.416812	1676.020012	19.992103
55.260245	1677.606214	19.997120
55.624029	1671.410957	20.002138
55.459254	1674.589862	20.007155
55.442054	1676.115193	20.012173
55.309543	1675.691893	20.017191
55.735559	1680.757237	20.022208
55.781030	1696.703356	20.027226
55.612098	1696.933727	20.032243
55.704217	1697.368907	20.037261
55.865239	1709.798253	20.042279
55.729270	1697.074674	20.047296
55.654586	1696.408333	20.052314
55.866154	1704.321411	20.057331
56.050638	1714.048436	20.062349
55.761382	1716.735359	20.067367
56.087514	1716.887697	20.072384
56.634953	1717.832924	20.077402
56.261191	1712.394814	20.082419
56.805740	1721.227969	20.087437
56.373787	1720.407395	20.092455
56.307564	1719.039648	20.097472
56.602319	1718.901117	20.102490
56.742963	1720.752287	20.107507
56.994430	1729.121766	20.112525
56.942107	1733.797035	20.117543
56.810745	1730.355412	20.122560
57.265410	1732.835697	20.127578
57.024522	1742.913882	20.132595
57.333684	1746.459608	20.137613
56.830143	1730.376363	20.142631
56.915768	1738.738661	20.147648
57.277309	1737.859538	20.152666
57.428895	1736.527380	20.157683
57.413412	1745.973359	20.162701
57.512395	1746.214096	20.167719
57.412039	1738.843684	20.172736
57.905530	1729.374936	20.177754
57.697873	1743.951982	20.182771
57.641104	1734.954658	20.187789
57.557536	1736.905554	20.192807
57.666865	1736.458351	20.197824
57.710384	1733.998409	20.202842
57.522685	1739.061844	20.207859
57.538201	1724.819448	20.212877
57.443240	1758.382709	20.217895
57.297353	1767.381392	20.222912
57.848634	1765.382258	20.227930
57.977728	1774.211398	20.232947
58.133172	1766.396647	20.237965
58.283261	1778.494390	20.242983
58.261048	1791.440760	20.248000
58.515485	1777.455216	20.253018
58.561894	1789.431551	20.258035
58.833065	1783.895292	20.263053
58.787195	1789.635661	20.268071
58.766012	1782.206057	20.273088
59.006128	1779.398592	20.278106
58.685344	1784.565574	20.283123
58.963141	1774.730146	20.288141
58.996489	1779.388881	20.293159
58.920006	1780.489781	20.298176
59.360124	1761.969919	20.303194
58.945581	1767.926049	20.308211
58.938310	1767.480829	20.313229
59.088234	1768.667865	20.318247
59.211982	1771.568306	20.323264
59.161617	1773.277092	20.328282
59.022516	1776.455703	20.333299
59.280638	1766.774326	20.338317
59.246002	1768.250191	20.343335
59.102799	1772.222795	20.348352
59.453629	1764.300496	20.353370
59.489364	1775.867954	20.358387
59.502975	1782.368559	20.363405
59.587729	1788.545179	20.368423
59.395676	1806.900450	20.373440
59.468033	1799.970315	20.378458
59.282432	1804.084988	20.383475
59.406710	1805.544780	20.388493
59.606548	1813.698442	20.393511
59.527190	1836.056003	20.398528
60.233419	1820.609376	20.403546
59.918493	1826.145879	20.408563
60.125141	1828.765672	20.413581
60.197012	1824.485643	20.418599
60.214760	1830.459985	20.423616
60.669456	1834.501721	20.428634
60.689122	1840.758431	20.433651
60.655387	1837.040379	20.438669
60.657322	1831.894750	20.443687
60.693061	1839.947641	20.448704
60.882964	1858.055082	20.453722
61.039616	1854.153139	20.458739
61.269775	1838.692010	20.463757
61.233934	1821.262709	20.468775
60.899066	1813.640930	20.473792
61.209846	1802.627568	20.478810
61.416324	1811.567933	20.483827
61.003478	1817.176159	20.488845
60.889166	1823.294807	20.493863
61.201874	1835.509766	20.498880
61.495712	1840.280903	20.503898
61.559059	1854.019075	20.508915
61.502963	1846.232616	20.513933
61.692263	1843.251268	20.518951
61.810944	1839.800110	20.523968
61.726128	1835.346805	20.528986
61.287376	1843.215660	20.534003
61.463444	1847.525189	20.539021
61.655465	1841.377597	20.544039
61.782359	1834.731335	20.549056
61.896255	1841.718122	20.554074
62.034114	1867.248864	20.559091
61.726286	1869.678254	20.564109
62.058335	1868.217384	20.569127
61.857706	1871.817626	20.574144
62.449723	1870.305444	20.579162
62.412602	1875.225092	20.584179
62.251859	1868.139819	20.589197
62.259014	1861.463764	20.594215
62.312058	1868.809464	20.599232
62.578498	1870.131548	20.604250
62.949732	1881.052974	20.609267
62.893236	1876.423706	20.614285
62.804145	1876.853462	20.619303
63.297590	1877.365507	20.624320
63.323224	1859.590940	20.629338
63.282156	1853.271303	20.634355
63.249087	1858.110746	20.639373
63.078835	1852.356996	20.644391
62.915597	1850.963961	20.649408
63.386795	1849.467849	20.654426
63.206032	1845.288306	20.659443
63.411988	1852.470882	20.664461
63.223246	1843.480779	20.669479
63.115728	1854.290114	20.674496
63.334301	1867.229750	20.679514
63.396941	1884.590959	20.684531
63.174586	1891.131466	20.689549
63.304929	1878.942000	20.694567
63.256636	1891.859700	20.699584
63.646172	1898.333937	20.704602
63.794101	1915.624365	20.709619
63.956196	1915.917648	20.714637
63.937475	1908.903330	20.719655
63.916463	1913.650241	20.724672
63.968760	1914.795184	20.729690
64.141255	1920.377397	20.734707
63.980200	1920.459613	20.739725
64.124858	1903.481839	20.744743
64.380324	1911.231453	20.749760
64.219101	1918.264221	20.754778
64.307878	1930.147034	20.759795
64.333042	1943.701053	20.764813
64.686558	1934.277405	20.769831
64.553872	1943.356289	20.774848
64.842453	1940.156905	20.779866
65.056529	1935.995428	20.784883
64.760310	1936.453968	20.789901
64.827818	1942.295309	20.794919
64.947842	1936.813157	20.799936
65.159213	1944.403549	20.804954
65.009420	1944.960288	20.809971
65.210339	1964.880241	20.814989
65.396762	1965.626594	20.820007
65.185259	1964.968721	20.825024
65.479393	1963.561760	20.830042
65.513844	1961.131236	20.835059
65.648487	1958.373487	20.840077
65.764230	1954.594043	20.845095
65.815591	1962.259364	20.850112
66.092496	1952.198376	20.855130
65.986017	1952.182578	20.860147
65.772905	1956.512087	20.865165
66.011703	1946.149532	20.870183
65.854502	1952.187928	20.875200
65.824511	1950.768097	20.880218
65.858732	1955.064922	20.885235
66.148259	1970.207117	20.890253
66.268689	1973.996749	20.895271
66.272597	1977.979300	20.900288
66.283830	1974.052978	20.905306
66.725379	1977.949681	20.910323
66.825458	1975.262615	20.915341
67.051709	1976.895701	20.920359
66.913942	1968.795137	20.925376
66.978563	1973.591275	20.930394
67.239216	1970.936285	20.935411
67.209827	1970.198258	20.940429
67.423687	1957.759069	20.945447
67.163474	1948.303563	20.950464
66.958941	1934.849392	20.955482
67.020318	1940.732300	20.960499
66.903200	1964.809720	20.965517
67.458893	1961.593271	20.970535
67.614839	1969.294430	20.975552
67.424111	1974.148989	20.980570
67.738245	1971.783576	20.985587
67.626845	1962.001840	20.990605
67.369720	1975.611682	20.995623
67.285568	1974.614606	21.000640
67.686523	1971.774177	21.005658
67.564995	1974.466837	21.010675
67.298040	1975.545350	21.015693
67.686001	1967.517979	21.020711
68.173943	1979.258359	21.025728
67.528671	1987.481960	21.030746
67.744459	1983.601296	21.035763
67.777449	1995.185121	21.040781
68.138202	1985.968911	21.045799
68.151697	1986.907287	21.050816
67.961132	2007.776386	21.055834
68.520311	2010.447687	21.060851
68.137155	2024.622153	21.065869
68.251195	2003.973260	21.070887
68.486271	2018.706791	21.075904
68.197577	2022.423620	21.080922
68.645923	2027.829092	21.085939
68.648627	2037.463975	21.090957
68.920518	2033.092501	21.095975
69.057090	2043.680446	21.100992
69.130288	2037.076453	21.106010
69.521752	2042.564186	21.111027
69.373652	2045.653000	21.116045
69.478401	2046.097517	21.121063
69.399457	2033.059881	21.126080
69.018747	2044.164981	21.131098
69.331182	2035.449275	21.136115
69.639558	2031.291452	21.141133
69.452482	2032.841007	21.146151
69.677083	2047.503464	21.151168
69.839167	2060.258122	21.156186
70.208208	2062.729017	21.161203
70.101537	2071.291842	21.166221
70.382867	2065.699076	21.171239
70.422414	2054.590677	21.176256
70.108478	2052.538698	21.181274
70.356028	2040.722623	21.186291
69.999487	2056.981744	21.191309
69.836494	2059.354109	21.196327
70.334746	2057.396794	21.201344
70.253699	2059.026830	21.206362
70.450850	2048.629370	21.211379
70.382611	2063.063548	21.216397
70.617145	2055.343435	21.221415
70.781936	2073.247012	21.226432
70.719204	2072.639701	21.231450
71.339264	2077.477768	21.236467
71.083523	2089.939415	21.241485
71.193182	2073.378680	21.246503
71.174775	2077.049982	21.251520
71.119827	2074.216120	21.256538
71.427628	2062.004215	21.261555
71.276987	2068.300632	21.266573
71.652945	2071.138505	21.271591
71.540076	2054.011074	21.276608
71.411203	2064.958741	21.281626
71.832045	2057.195180	21.286643
71.859671	2055.540596	21.291661
71.545135	2053.436352	21.296679
71.829431	2054.514546	21.301696
72.018897	2069.158431	21.306714
71.988755	2067.326791	21.311731
72.119358	2070.060401	21.316749
71.797044	2070.492949	21.321767
72.110262	2078.777195	21.326784
72.362040	2087.349186	21.331802
72.233610	2092.521824	21.336819
72.357481	2094.931346	21.341837
72.530322	2095.856337	21.346855
72.414543	2088.877301	21.351872
72.182922	2097.639968	21.356890
72.757149	2091.882158	21.361907
72.596303	2103.434770	21.366925
72.447248	2103.818946	21.371943
72.605923	2102.609210	21.376960
72.461537	2118.882482	21.381978
72.586149	2134.519875	21.386995
72.667286	2137.256963	21.392013
72.611710	2121.979088	21.397031
73.075751	2150.822147	21.402048
73.450445	2162.278651	21.407066
73.825305	2157.857022	21.412083
73.969525	2160.054123	21.417101
73.961480	2152.169001	21.422119
73.781781	2142.215383	21.427136
73.530532	2130.004646	21.432154
73.688413	2136.377571	21.437171
73.859960	2150.428811	21.442189
73.967611	2145.204942	21.447207
73.944455	2147.459676	21.452224
73.763007	2145.896001	21.457242
74.000272	2135.958392	21.462259
74.171868	2144.513768	21.467277
73.874086	2150.822770	21.472295
74.043793	2145.018134	21.477312
74.253918	2163.765126	21.482330
74.485033	2169.205829	21.487347
74.482865	2176.974216	21.492365
74.592523	2161.373659	21.497383
74.649613	2172.163047	21.502400
74.536506	2176.441411	21.507418
74.841982	2166.167280	21.512435
74.889826	2176.614883	21.517453
74.774690	2203.738910	21.522471
75.234550	2192.682873	21.527488
75.431867	2205.961364	21.532506
75.213043	2199.153676	21.537523
75.458419	2203.400253	21.542541
75.408727	2201.531282	21.547559
75.542046	2194.093616	21.552576
75.528056	2200.000519	21.557594
75.783167	2197.151126	21.562611
75.681145	2201.535539	21.567629
75.571455	2205.419630	21.572647
75.640475	2192.712887	21.577664
75.881196	2203.693554	21.582682
76.131274	2223.141509	21.587699
76.200760	2222.485134	21.592717
76.139522	2234.281597	21.597735
76.335842	2219.413119	21.602752
75.913969	2221.741360	21.607770
75.962225	2220.083343	21.612787
76.133030	2223.143014	21.617805
76.067727	2233.444422	21.622823
76.465691	2243.460857	21.627840
76.393955	2243.735774	21.632858
76.843993	2250.756465	21.637875
76.974112	2244.979214	21.642893
76.868741	2242.317850	21.647911
77.182350	2231.846653	21.652928
76.963518	2243.864499	21.657946
77.499062	2235.828305	21.662963
77.299796	2236.060161	21.667981
77.228090	2240.754146	21.672999
77.331136	2234.538057	21.678016
77.269993	2236.622315	21.683034
77.337225	2238.425072	21.688051
77.575970	2258.463554	21.693069
77.756507	2258.899860	21.698087
78.058511	2257.721107	21.703104
77.733886	2268.972598	21.708122
77.620541	2262.445462	21.713139
77.479135	2259.207360	21.718157
78.019564	2250.787657	21.723175
78.214871	2252.764887	21.728192
78.016050	2254.234515	21.733210
78.262752	2258.392696	21.738227
78.385286	2268.893351	21.743245
78.658446	2273.787344	21.748263
78.863715	2276.298776	21.753280
78.570894	2278.269030	21.758298
78.927630	2276.767815	21.763315
79.093310	2278.029845	21.768333
79.112830	2269.840874	21.773351
78.863831	2267.285179	21.778368
78.650565	2273.418418	21.783386
78.880463	2270.825560	21.788403
79.232151	2276.655803	21.793421
79.184209	2275.322383	21.798439
79.188432	2280.423511	21.803456
79.067453	2280.040411	21.808474
79.194854	2273.919097	21.813491
79.233937	2295.090731	21.818509
79.095287	2300.113548	21.823527
79.280294	2305.579256	21.828544
79.475680	2310.310539	21.833562
79.835381	2327.921103	21.838579
80.294187	2331.238243	21.843597
79.953227	2342.355871	21.848615
80.662633	2325.893215	21.853632
80.500862	2328.790639	21.858650
80.521588	2332.328351	21.863667
80.656214	2319.089358	21.868685
80.283433	2317.025430	21.873703
80.785395	2323.528086	21.878720
80.439616	2334.292553	21.883738
80.681537	2324.648555	21.888755
80.759141	2322.379736	21.893773
80.435036	2332.516569	21.898791
80.968446	2321.669140	21.903808
80.472467	2328.462623	21.908826
80.861579	2334.843017	21.913843
81.171548	2341.857806	21.918861
81.251663	2346.469202	21.923879
81.549530	2341.362600	21.928896
81.221123	2336.167557	21.933914
81.326982	2339.566365	21.938931
81.438402	2342.672115	21.943949
81.564924	2346.497051	21.948967
81.947514	2333.740637	21.953984
81.401856	2345.317375	21.959002
81.859034	2355.093753	21.964019
81.838144	2368.265986	21.969037
81.466954	2367.455391	21.974055
82.034261	2366.809504	21.979072
81.831293	2372.482788	21.984090
81.938816	2381.812326	21.989107
82.103449	2380.358263	21.994125
82.221563	2396.287168	21.999143
82.379456	2386.547984	22.004160
82.409103	2392.995399	22.009178
82.808375	2389.729170	22.014195
82.786996	2387.057024	22.019213
82.599823	2385.541125	22.024231
82.943931	2396.329606	22.029248
83.013879	2408.214328	22.034266
82.759714	2424.799811	22.039283
83.498609	2416.457402	22.044301
83.088372	2420.902752	22.049319
83.506021	2409.091701	22.054336
83.609508	2420.870087	22.059354
83.488664	2413.419671	22.064371
83.414726	2409.052988	22.069389
83.506730	2414.470351	22.074407
83.378956	2412.417422	22.079424
83.460548	2420.373254	22.084442
83.584090	2438.762454	22.089459
84.094529	2433.871427	22.094477
83.643212	2441.553280	22.099495
83.883911	2444.931361	22.104512
84.209107	2444.989372	22.109530
83.703909	2443.729676	22.114547
84.075755	2462.887678	22.119565
84.339286	2468.509744	22.124583
84.681638	2474.788877	22.129600
84.541663	2469.692124	22.134618
84.422361	2468.516180	22.139635
85.145620	2478.613562	22.144653
85.079928	2489.978648	22.149671
85.310208	2490.168523	22.154688
85.242820	2486.083032	22.159706
85.734732	2485.827598	22.164723
86.201195	2471.988228	22.169741
85.822534	2459.677060	22.174759
85.611385	2453.180997	22.179776
85.693574	2448.912475	22.184794
85.400678	2443.642220	22.189811
85.875044	2448.762811	22.194829
85.650017	2446.231466	22.199847
85.759049	2459.975603	22.204864
86.148108	2465.179619	22.209882
85.807903	2467.003402	22.214899
86.246672	2469.767954	22.219917
85.924079	2476.641067	22.224935
86.275255	2474.497019	22.229952
86.046238	2477.053616	22.234970
86.512613	2488.703069	22.239987
86.518811	2499.423547	22.245005
86.511368	2513.271666	22.250023
86.586816	2506.778527	22.255040
87.003709	2508.882891	22.260058
86.746635	2515.833761	22.265075
87.056987	2510.962058	22.270093
86.838092	2513.647701	22.275111
86.925731	2508.936109	22.280128
87.158364	2519.280508	22.285146
87.387429	2533.435964	22.290163
87.602261	2530.404587	22.295181
87.369414	2531.105813	22.300199
87.500576	2538.751513	22.305216
87.911888	2529.540787	22.310234
87.675843	2528.230614	22.315251
87.998952	2520.138106	22.320269
87.767379	2523.213667	22.325287
88.255767	2524.642379	22.330304
87.748008	2533.783706	22.335322
87.592763	2540.177537	22.340339
87.862734	2551.680018	22.345357
88.006409	2552.965006	22.350375
88.359564	2563.139865	22.355392
88.504152	2573.569748	22.360410
88.540750	2581.128363	22.365427
89.010626	2574.247430	22.370445
89.002671	2582.651269	22.375463
89.044124	2581.578629	22.380480
89.084311	2580.829446	22.385498
89.176865	2580.314916	22.390515
89.629201	2572.902209	22.395533
89.254005	2580.685706	22.400551
89.087612	2572.871472	22.405568
89.461702	2570.946860	22.410586
89.470577	2580.003069	22.415603
89.616874	2567.431659	22.420621
89.266616	2575.226774	22.425639
89.218020	2590.029865	22.430656
89.813255	2594.312332	22.435674
90.062505	2606.914809	22.440691
90.308977	2597.572271	22.445709
89.857169	2607.568604	22.450727
90.156291	2606.803323	22.455744
90.434914	2596.272317	22.460762
90.187970	2608.756937	22.465779
90.302338	2616.973602	22.470797
90.665399	2627.296873	22.475815
90.719980	2630.416028	22.480832
90.769088	2627.153786	22.485850
90.826801	2627.760056	22.490867
90.841412	2626.531610	22.495885
90.847694	2620.699129	22.500903
90.752457	2622.444179	22.505920
90.979345	2637.035944	22.510938
90.894171	2653.515733	22.515955
91.203829	2652.099450	22.520973
91.348170	2659.397728	22.525991
91.606692	2653.968384	22.531008
91.594663	2673.010663	22.536026
91.382870	2678.481961	22.541043
91.989824	2675.387208	22.546061
91.909049	2669.890798	22.551079
91.975305	2673.022203	22.556096
92.073704	2676.571150	22.561114
92.150852	2676.116651	22.566131
92.703069	2685.629850	22.571149
92.826283	2691.611079	22.576167
92.981645	2688.591093	22.581184
93.114066	2672.328730	22.586202
92.794738	2668.333727	22.591219
92.890267	2656.776231	22.596237
93.160014	2678.518504	22.601255
93.051718	2683.939988	22.606272
93.246457	2683.774703	22.611290
93.195091	2690.493546	22.616307
93.289569	2689.617251	22.621325
93.395170	2701.073824	22.626343
93.555358	2695.527666	22.631360
93.469307	2694.676536	22.636378
93.430188	2688.898400	22.641395
93.657838	2683.043812	22.646413
93.509659	2693.395862	22.651431
94.118839	2710.382445	22.656448
94.203782	2719.171005	22.661466
93.977138	2720.028309	22.666483
94.019519	2710.374982	22.671501
94.319548	2708.885086	22.676519
94.188329	2712.038564	22.681536
93.978152	2714.579480	22.686554
94.288911	2733.191986	22.691571
94.516269	2738.626031	22.696589
94.679365	2744.942041	22.701607
94.609446	2739.742255	22.706624
95.052886	2740.566969	22.711642
94.798549	2742.713992	22.716659
94.945216	2739.475735	22.721677
95.146708	2749.655746	22.726695
95.283739	2758.784549	22.731712
95.233704	2764.600775	22.736730
95.147361	2769.135125	22.741747
95.377228	2766.144524	22.746765
95.625770	2763.087048	22.751783
95.448881	2763.671137	22.756800
95.560276	2778.470359	22.761818
95.884471	2785.343221	22.766835
96.313696	2785.064697	22.771853
96.443031	2784.007810	22.776871
96.191265	2788.635307	22.781888
96.313323	2785.525533	22.786906
96.440703	2781.530168	22.791923
96.316591	2779.335628	22.796941
96.563486	2772.396638	22.801959
96.751972	2790.482960	22.806976
97.057618	2800.105956	22.811994
96.888601	2804.548091	22.817011
97.084917	2796.896937	22.822029
97.353591	2800.977212	22.827047
97.304230	2797.480432	22.832064
97.286911	2799.975650	22.837082
97.219678	2806.173903	22.842099
97.419757	2800.475816	22.847117
97.905686	2795.147366	22.852135
97.267131	2806.097254	22.857152
98.033840	2814.079630	22.862170
97.844296	2834.312216	22.867187
98.035844	2824.158888	22.872205
98.224127	2820.546766	22.877223
98.093850	2831.837749	22.882240
98.185042	2822.389280	22.887258
98.288370	2836.018937	22.892275
97.924099	2846.039513	22.897293
98.477411	2845.312064	22.902311
98.557489	2855.094497	22.907328
98.710639	2845.069176	22.912346
98.661161	2858.173715	22.917363
98.983639	2869.411813	22.922381
99.176334	2876.660058	22.927399
99.024202	2883.265342	22.932416
99.455583	2882.604540	22.937434
99.454637	2882.620482	22.942451
99.291506	2877.662479	22.947469
99.472331	2878.334603	22.952487
99.430992	2876.875618	22.957504
99.819257	2885.405374	22.962522
99.664944	2904.086422	22.967539
99.773505	2911.543118	22.972557
100.164428	2907.113503	22.977575
99.890755	2910.317774	22.982592
100.118830	2914.676870	22.987610
100.449203	2935.168416	22.992627
100.555621	2926.415060	22.997645
100.911483	2933.008313	23.002663
100.702945	2939.590673	23.007680
100.720588	2930.420874	23.012698
100.949048	2926.544968	23.017715
100.814282	2937.935991	23.022733
101.278660	2926.359356	23.027751
101.091370	2932.644864	23.032768
101.213349	2929.341753	23.037786
101.009040	2942.434986	23.042803
101.371920	2954.025935	23.047821
101.397501	2959.143435	23.052839
101.472359	2963.919679	23.057856
101.819811	2952.637605	23.062874
101.667423	2964.092593	23.067891
101.752869	2961.280604	23.072909
101.678917	2980.206728	23.077927
101.810519	2987.362769	23.082944
102.114324	2990.061567	23.087962
102.065905	2992.629688	23.092979
102.175347	2994.127880	23.097997
102.597797	2993.772909	23.103015
102.740122	3008.926317	23.108032
103.052635	3005.609362	23.113050
103.149107	3001.880499	23.118067
102.986415	3005.183746	23.123085
103.122053	3005.110141	23.128103
102.877729	3014.236084	23.133120
103.172908	3006.560586	23.138138
103.388306	3021.523939	23.143155
103.498834	3033.339028	23.148173
103.767203	3027.850833	23.153191
103.370492	3037.883202	23.158208
103.550377	3032.491946	23.163226
103.824907	3034.893603	23.168243
103.414482	3040.345939	23.173261
104.083445	3055.643717	23.178279
103.985197	3062.098803	23.183296
104.220198	3056.132220	23.188314
104.301682	3059.324573	23.193331
104.541512	3083.044594	23.198349
104.903485	3077.998407	23.203367
104.946636	3078.027130	23.208384
105.330547	3082.966042	23.213402
105.415979	3071.723326	23.218419
105.334497	3068.245190	23.223437
105.880350	3064.182437	23.228455
105.829342	3070.991157	23.233472
105.676261	3051.913592	23.238490
105.622682	3044.276130	23.243507
105.817281	3058.061358	23.248525
105.885531	3052.596837	23.253543
105.615271	3066.724022	23.258560
105.923339	3063.291638	23.263578
105.988674	3060.490836	23.268595
106.209021	3059.985844	23.273613
106.237709	3059.440136	23.278631
106.154676	3067.880685	23.283648
106.309550	3079.494748	23.288666
106.226449	3082.137924	23.293683
105.964151	3087.390538	23.298701
106.177703	3086.335832	23.303719
106.400556	3107.233238	23.308736
106.281533	3108.800372	23.313754
106.919250	3124.885750	23.318771
107.033127	3143.115161	23.323789
107.321476	3138.622143	23.328807
107.005226	3145.553557	23.333824
107.397642	3136.974408	23.338842
107.639796	3138.519546	23.343859
107.650087	3149.580771	23.348877
107.823306	3164.661099	23.353895
107.979256	3169.863000	23.358912
108.199252	3161.760460	23.363930
108.334411	3166.884298	23.368947
108.274378	3164.399145	23.373965
108.349639	3157.883323	23.378983
108.407393	3169.441084	23.384000
108.581870	3163.957363	23.389018
108.799620	3164.680085	23.394035
108.736400	3169.894254	23.399053
108.825077	3174.632445	23.404071
108.892158	3194.067814	23.409088
108.971441	3187.200491	23.414106
108.750492	3185.460553	23.419123
108.785916	3196.878710	23.424141
109.446861	3208.728012	23.429159
108.933023	3219.964262	23.434176
109.340123	3226.943685	23.439194
109.530179	3216.836418	23.444211
109.616510	3234.060550	23.449229
109.843815	3237.694200	23.454247
110.052539	3242.844470	23.459264
110.018914	3245.004629	23.464282
110.111154	3240.517276	23.469299
110.180018	3248.161039	23.474317
110.436275	3258.328379	23.479335
110.370387	3268.063184	23.484352
110.684640	3278.718626	23.489370
111.277030	3269.725154	23.494387
111.328768	3274.767553	23.499405
111.712153	3266.330002	23.504423
111.705430	3265.210561	23.509440
111.811639	3260.613397	23.514458
111.942057	3259.846882	23.519475
111.567695	3267.090364	23.524493
111.836238	3246.523314	23.529511
111.579313	3258.455322	23.534528
111.800025	3254.218376	23.539546
111.992135	3255.995458	23.544563
111.907811	3281.540895	23.549581
111.873439	3286.586136	23.554599
111.834900	3286.142899	23.559616
112.275185	3297.241711	23.564634
112.428103	3297.792870	23.569651
112.537164	3310.245882	23.574669
112.520011	3300.686702	23.579687
112.572351	3311.198108	23.584704
112.883433	3315.499870	23.589722
112.957016	3328.595847	23.594739
113.123003	3337.418981	23.599757
113.125366	3331.943222	23.604775
113.410351	3339.102774	23.609792
113.392569	3338.629718	23.614810
113.754906	3343.109636	23.619827
113.861906	3359.166182	23.624845
114.160107	3362.572352	23.629863
114.116349	3362.700120	23.634880
114.399205	3366.707323	23.639898
114.380732	3354.999663	23.644915
114.394437	3359.455014	23.649933
114.633850	3352.407940	23.654951
114.693070	3349.944357	23.659968
114.436670	3364.423884	23.664986
114.715576	3371.545871	23.670003
114.893858	3384.710004	23.675021
115.328928	3380.594640	23.680039
115.288114	3383.916769	23.685056
115.201265	3379.152692	23.690074
115.218559	3385.824636	23.695091
115.328948	3398.981121	23.700109
115.586816	3404.645810	23.705127
115.812585	3408.226599	23.710144
115.650720	3411.214404	23.715162
116.070624	3409.505756	23.720179
116.043515	3405.778751	23.725197
116.268223	3410.009791	23.730215
116.309559	3403.383328	23.735232
116.138847	3413.873458	23.740250
116.287715	3419.929076	23.745267
116.537088	3436.872866	23.750285
116.433500	3427.323981	23.755303
116.530524	3429.788951	23.760320
116.641887	3439.716195	23.765338
117.243086	3449.625741	23.770355
117.257206	3459.033602	23.775373
117.307098	3462.410817	23.780391
117.302216	3461.372957	23.785408
117.357467	3454.717000	23.790426
117.807202	3460.131808	23.795443
117.723277	3484.271831	23.800461
118.052141	3482.540843	23.805479
118.146952	3478.150645	23.810496
117.838596	3480.906387	23.815514
118.119108	3473.003535	23.820531
118.122254	3477.028333	23.825549
118.186413	3500.579231	23.830567
118.598980	3512.069053	23.835584
118.418176	3509.455396	23.840602
119.125562	3503.793159	23.845619
118.808109	3511.396667	23.850637
118.989668	3530.768221	23.855655
119.176660	3534.251116	23.860672
119.223541	3544.424564	23.865690
119.574620	3533.123755	23.870707
119.438478	3531.266574	23.875725
119.567178	3535.663168	23.880743
120.010853	3546.282404	23.885760
120.217109	3553.597234	23.890778
120.764914	3548.085826	23.895795
120.943508	3541.966174	23.900813
120.942576	3544.194592	23.905831
121.126535	3517.822757	23.910848
120.866462	3516.957080	23.915866
120.929575	3506.685581	23.920883
121.160827	3512.018455	23.925901
121.198771	3520.740042	23.930919
121.274550	3526.527060	23.935936
121.084422	3533.410594	23.940954
121.369807	3527.544560	23.945971
121.638115	3537.981775	23.950989
121.413128	3531.009540	23.956007
121.595741	3529.646503	23.961024
121.462894	3542.094469	23.966042
121.850821	3547.225803	23.971059
121.618976	3560.054392	23.976077
121.987652	3549.533432	23.981095
122.126855	3549.665166	23.986112
122.121162	3568.996107	23.991130
122.332238	3581.133983	23.996147
122.566027	3595.544774	24.001165
122.844841	3580.497546	24.006183
122.865679	3589.138135	24.011200
122.660625	3593.592364	24.016218
122.931750	3592.587156	24.021235
122.876727	3619.986796	24.026253
123.133200	3623.796834	24.031271
123.106374	3618.681758	24.036288
123.547721	3640.658415	24.041306
123.841642	3635.103173	24.046323
123.921771	3638.290358	24.051341
124.028242	3649.256869	24.056359
124.262335	3649.652851	24.061376
124.122706	3642.066356	24.066394
124.413478	3635.860763	24.071411
124.588531	3642.290528	24.076429
124.460804	3654.632604	24.081447
124.837327	3657.115518	24.086464
124.335507	3667.779548	24.091482
124.625052	3669.015675	24.096499
124.719677	3669.859213	24.101517
124.924096	3681.720674	24.106535
125.332470	3698.154502	24.111552
125.056602	3695.529777	24.116570
125.031375	3698.041017	24.121587
125.254147	3713.997648	24.126605
125.303868	3728.005512	24.131623
125.686816	3719.001968	24.136640
125.930212	3733.538872	24.141658
126.257447	3739.246143	24.146675
126.288228	3750.209506	24.151693
126.539843	3744.320238	24.156711
126.655478	3747.943753	24.161728
127.050407	3745.516273	24.166746
127.094068	3741.272284	24.171763
127.305531	3739.433917	24.176781
127.342667	3742.204561	24.181799
127.409029	3746.474115	24.186816
127.277441	3741.055827	24.191834
127.738491	3755.208244	24.196851
127.727329	3762.728482	24.201869
127.697541	3772.628513	24.206887
127.644029	3756.901389	24.211904
127.835640	3769.991190	24.216922
128.067378	3761.362309	24.221939
128.091693	3773.988011	24.226957
127.800446	3805.186265	24.231975
127.987585	3803.197565	24.236992
128.305069	3807.413353	24.242010
128.321757	3822.185145	24.247027
129.048015	3811.758769	24.252045
128.672256	3824.251900	24.257063
129.117361	3821.096709	24.262080
129.281981	3853.389436	24.267098
129.301346	3851.024511	24.272115
129.719968	3852.745655	24.277133
129.243925	3859.423482	24.282151
129.771568	3853.718429	24.287168
130.051540	3874.259718	24.292186
130.009178	3876.253276	24.297203
130.383011	3868.953370	24.302221
130.238128	3871.393883	24.307239
130.168078	3867.643164	24.312256
130.519266	3874.555749	24.317274
130.614220	3897.874948	24.322291
130.645302	3894.187019	24.327309
130.568731	3896.009839	24.332327
130.973269	3895.625532	24.337344
131.039747	3909.132287	24.342362
131.240966	3917.240364	24.347379
131.212546	3916.613517	24.352397
131.355327	3916.278846	24.357415
131.593929	3937.455900	24.362432
131.821499	3946.314859	24.367450
131.983984	3955.527957	24.372467
132.121645	3956.093480	24.377485
132.171693	3953.499018	24.382503
132.414007	3964.746455	24.387520
132.580637	3981.558450	24.392538
132.588531	3982.057256	24.397555
132.612772	3977.569925	24.402573
133.030370	3973.515972	24.407591
133.268036	3976.016415	24.412608
132.610192	3975.152775	24.417626
133.034083	3993.468881	24.422643
133.318302	4006.945972	24.427661
133.260737	4010.597041	24.432679
133.435243	4001.120287	24.437696
133.364669	4015.389306	24.442714
133.823930	4027.493921	24.447731
134.320324	4028.002419	24.452749
133.986966	4031.586537	24.457767
134.396207	4037.009433	24.462784
134.189206	4048.540012	24.467802
134.705092	4065.937683	24.472819
135.168607	4061.551646	24.477837
135.037215	4053.115423	24.482855
135.204701	4055.234522	24.487872
135.407914	4055.066249	24.492890
135.166113	4055.514256	24.497907
135.418510	4057.392491	24.502925
135.475304	4076.960995	24.507943
135.792223	4072.802407	24.512960
135.630190	4080.642309	24.517978
135.703199	4082.820368	24.522995
136.115257	4094.511524	24.528013
136.031406	4105.925679	24.533031
136.503846	4110.355304	24.538048
136.466781	4115.008676	24.543066
136.489603	4109.321350	24.548083
136.929643	4117.699491	24.553101
136.915566	4135.218054	24.558119
137.270522	4133.571669	24.563136
137.127622	4132.360519	24.568154
137.496012	4128.704501	24.573171
137.267014	4127.934446	24.578189
137.334150	4148.584967	24.583207
137.830360	4159.437697	24.588224
137.669381	4158.020843	24.593242
137.954460	4163.506867	24.598259
138.485426	4179.609044	24.603277
138.526243	4185.101651	24.608295
138.605916	4194.732603	24.613312
138.337833	4191.444978	24.618330
138.361911	4191.991513	24.623347
139.109841	4189.950875	24.628365
138.921335	4213.330072	24.633383
139.058309	4212.871927	24.638400
138.867966	4208.883912	24.643418
139.142878	4217.335908	24.648435
139.569677	4227.123621	24.653453
139.471126	4245.653309	24.658471
139.475315	4242.356036	24.663488
139.720363	4258.888372	24.668506
140.077889	4270.426457	24.673523
140.401385	4269.716920	24.678541
140.330840	4272.452721	24.683559
140.708157	4273.307769	24.688576
140.744318	4275.168278	24.693594
140.758006	4292.572953	24.698611
140.850136	4292.902678	24.703629
140.672172	4300.785491	24.708647
140.529303	4296.969153	24.713664
140.950608	4319.074907	24.718682
141.062164	4330.649820	24.723699
141.397523	4340.523621	24.728717
141.442316	4350.362053	24.733735
141.772707	4352.929110	24.738752
142.000338	4363.791796	24.743770
141.899569	4380.575247	24.748787
142.703122	4375.640617	24.753805
142.590719	4382.930625	24.758823
142.902381	4377.984499	24.763840
142.835303	4371.477170	24.768858
142.993003	4376.950493	24.773875
143.467724	4372.849181	24.778893
143.257917	4369.471541	24.783911
143.434973	4385.020604	24.788928
143.911350	4405.372960	24.793946
143.708903	4408.709464	24.798963
143.826773	4389.344816	24.803981
143.539212	4398.965025	24.808999
143.668721	4397.540222	24.814016
143.981997	4419.345049	24.819034
144.216523	4425.508158	24.824051
144.404541	4426.682796	24.829069
144.150125	4443.034188	24.834087
144.567606	4448.933117	24.839104
144.699562	4461.030041	24.844122
144.592839	4465.616294	24.849139
144.801538	4468.797325	24.854157
144.905964	4495.646409	24.859175
145.164775	4494.210429	24.864192
145.897835	4506.930841	24.869210
145.785003	4509.444507	24.874227
146.079241	4512.720855	24.879245
145.993044	4512.846207	24.884263
145.961506	4521.085274	24.889280
146.684570	4528.696174	24.894298
146.471101	4538.518415	24.899315
146.831970	4538.312224	24.904333
146.887748	4546.186390	24.909351
147.050340	4542.656491	24.914368
147.186400	4551.729406	24.919386
146.569757	4573.226895	24.924403
147.307635	4564.298388	24.929421
147.210646	4582.847904	24.934439
147.375551	4600.702778	24.939456
147.916863	4607.556256	24.944474
147.892904	4604.471480	24.949491
148.116520	4612.817201	24.954509
148.525113	4617.999418	24.959527
148.599182	4616.984638	24.964544
148.780098	4619.196886	24.969562
149.120299	4621.597765	24.974579
149.430863	4615.622417	24.979597
149.445021	4618.916017	24.984615
149.477587	4613.463949	24.989632
149.252494	4629.405878	24.994650
149.697102	4643.199550	24.999667
149.884089	4641.318667	25.004685
149.926206	4646.281983	25.009703
149.955246	4641.066756	25.014720
150.229415	4643.492747	25.019738
150.180747	4658.861299	25.024755
150.549028	4667.379987	25.029773
150.324136	4672.008702	25.034791
150.555518	4677.525849	25.039808
150.535587	4692.745553	25.044826
150.485556	4705.074408	25.049843
150.493150	4703.636684	25.054861
150.828125	4721.940012	25.059879
151.200638	4723.089642	25.064896
151.374285	4722.121375	25.069914
151.282556	4743.546370	25.074931
151.654977	4744.679478	25.079949
152.106790	4752.989857	25.084967
151.847770	4759.229293	25.089984
152.138649	4772.557092	25.095002
152.309179	4778.545859	25.100019
152.393076	4780.511934	25.105037
152.529203	4796.827389	25.110055
152.440813	4804.259315	25.115072
152.994188	4796.689053	25.120090
153.108051	4807.335401	25.125107
153.395931	4816.755064	25.130125
153.639074	4829.345780	25.135143
153.275405	4833.808502	25.140160
153.706948	4844.440873	25.145178
153.791744	4848.076443	25.150195
154.190746	4854.729922	25.155213
153.967692	4855.767880	25.160231
154.395197	4863.427089	25.165248
154.421759	4873.135768	25.170266
154.512358	4894.781230	25.175283
155.134265	4886.446667	25.180301
155.071184	4893.021511	25.185319
154.779875	4905.580270	25.190336
155.417746	4913.263744	25.195354
155.780113	4921.984381	25.200371
156.246439	4920.288765	25.205389
155.749857	4917.927977	25.210407
155.612928	4926.790343	25.215424
156.302325	4930.274648	25.220442
156.639081	4940.951129	25.225459
156.946846	4937.161626	25.230477
156.848987	4936.602152	25.235495
156.466179	4944.685375	25.240512
156.905986	4959.559877	25.245530
157.067640	4968.157042	25.250547
157.286791	4965.895125	25.255565
157.151666	4972.979674	25.260583
157.030072	4991.788916	25.265600
157.939402	4996.287445	25.270618
158.007142	4999.762847	25.275635
157.982354	5021.225179	25.280653
158.265012	5026.445708	25.285671
158.389853	5028.280599	25.290688
158.646497	5025.373746	25.295706
158.644994	5037.560152	25.300723
158.866224	5039.650800	25.305741
159.325242	5040.425425	25.310759
159.116075	5054.394637	25.315776
159.638761	5041.666004	25.320794
159.371112	5059.845033	25.325811
159.994224	5074.441213	25.330829
160.109177	5071.796443	25.335847
159.930637	5081.638440	25.340864
160.139279	5067.544928	25.345882
160.382773	5088.714852	25.350899
160.423042	5100.470675	25.355917
160.598699	5102.532648	25.360935
160.352930	5112.607103	25.365952
161.004166	5126.397709	25.370970
160.935364	5140.998237	25.375987
161.371036	5139.821175	25.381005
161.332387	5137.133304	25.386023
161.589199	5153.762296	25.391040
161.902326	5154.627237	25.396058
161.827868	5157.533955	25.401075
161.897520	5157.957205	25.406093
162.035207	5167.455499	25.411111
162.252823	5186.196215	25.416128
162.858540	5180.419093	25.421146
162.723785	5177.680969	25.426163
162.620741	5181.142942	25.431181
162.486182	5198.849602	25.436199
162.752780	5214.694182	25.441216
163.228885	5219.590558	25.446234
163.261185	5234.806077	25.451251
163.254660	5241.838739	25.456269
163.732842	5238.165869	25.461287
163.925082	5257.865423	25.466304
164.256541	5259.519645	25.471322
164.092268	5269.276701	25.476339
164.242550	5271.661869	25.481357
164.691780	5278.992414	25.486375
164.383615	5285.634772	25.491392
164.872597	5288.258428	25.496410
164.972500	5288.957842	25.501427
165.344776	5315.882908	25.506445
165.644475	5314.607844	25.511463
165.625705	5326.313753	25.516480
165.784739	5322.299117	25.521498
165.644523	5339.958041	25.526515
166.060269	5347.131918	25.531533
166.180573	5349.150319	25.536551
166.348875	5357.578839	25.541568
166.443977	5376.881927	25.546586
166.694558	5378.392821	25.551603
166.709906	5379.886739	25.556621
167.137555	5397.588758	25.561639
166.889523	5408.844376	25.566656
167.395558	5412.604876	25.571674
167.118459	5430.885920	25.576691
167.300349	5432.289264	25.581709
167.788104	5444.763582	25.586727
168.223783	5464.822404	25.591744
168.311079	5465.798783	25.596762
168.477434	5466.172166	25.601779
168.954194	5478.397088	25.606797
169.081298	5490.059279	25.611815
169.245531	5492.213769	25.616832
169.417351	5488.934952	25.621850
169.249392	5485.601334	25.626867
169.461181	5498.030019	25.631885
170.077592	5510.392517	25.636903
170.229155	5523.448669	25.641920
170.071274	5516.173026	25.646938
170.240859	5520.750071	25.651955
170.309722	5530.031574	25.656973
170.733169	5533.532480	25.661991
170.489738	5543.232712	25.667008
170.933434	5551.476341	25.672026
171.289659	5552.962675	25.677044
171.152857	5575.016100	25.682061
171.794123	5569.833106	25.687079
171.796551	5573.830599	25.692096
171.902999	5569.883676	25.697114
172.243949	5562.765649	25.702132
172.087518	5569.086869	25.707149
172.474840	5574.995157	25.712167
172.543702	5590.661774	25.717184
172.312664	5583.018587	25.722202
172.441246	5593.560642	25.727220
172.796814	5612.004155	25.732237
173.075027	5618.891398	25.737255
173.045742	5630.252727	25.742272
173.289928	5640.032178	25.747290
173.562051	5642.107395	25.752308
173.488572	5645.597654	25.757325
173.429357	5667.843929	25.762343
173.448248	5685.192573	25.767360
173.752882	5701.032921	25.772378
174.410476	5705.110224	25.777396
174.525874	5712.816007	25.782413
174.531514	5716.574360	25.787431
174.764683	5741.773907	25.792448
174.893882	5740.056046	25.797466
175.091247	5749.619635	25.802484
175.333978	5758.895331	25.807501
175.956612	5767.287451	25.812519
175.823164	5760.000561	25.817536
176.149248	5763.772036	25.822554
176.428339	5784.655825	25.827572
176.352524	5791.842761	25.832589
176.642712	5783.148365	25.837607
176.630898	5800.269086	25.842624
176.752325	5800.118277	25.847642
176.629403	5818.846024	25.852660
177.161661	5821.053837	25.857677
177.411711	5831.373526	25.862695
177.133431	5848.226516	25.867712
177.136786	5853.054860	25.872730
177.949024	5865.693177	25.877748
177.999962	5880.917259	25.882765
178.299821	5877.199730	25.887783
178.385259	5892.328323	25.892800
178.750924	5903.469306	25.897818
178.959640	5905.893730	25.902836
178.934511	5909.042094	25.907853
179.280699	5921.453589	25.912871
179.596347	5934.345872	25.917888
179.713693	5931.126390	25.922906
179.932040	5934.596757	25.927924
179.879324	5956.408384	25.932941
180.206974	5960.849911	25.937959
180.226712	5970.214630	25.942976
180.169771	5973.216262	25.947994
180.800240	5983.806237	25.953012
180.701148	5997.857297	25.958029
181.057070	5996.962746	25.963047
181.277194	6018.326029	25.968064
181.344692	6023.780204	25.973082
181.589655	6019.635387	25.978100
181.922821	6035.192530	25.983117
182.109454	6038.849323	25.988135
182.117250	6051.149177	25.993152
182.280536	6049.173601	25.998170
182.451145	6051.579152	26.003188
182.251595	6061.466191	26.008205
182.796421	6068.435515	26.013223
182.937587	6092.475716	26.018240
183.017181	6103.697279	26.023258
183.329749	6109.937135	26.028276
183.558485	6127.991895	26.033293
184.318318	6118.435879	26.038311
184.505441	6126.460006	26.043328
184.474101	6124.020435	26.048346
184.901599	6117.290311	26.053364
184.719754	6133.377030	26.058381
184.977010	6138.059461	26.063399
185.007149	6146.506551	26.068416
184.875528	6156.864433	26.073434
185.193169	6155.902962	26.078452
185.199155	6175.572272	26.083469
185.604545	6185.748333	26.088487
185.393362	6188.840126	26.093504
185.714881	6198.281042	26.098522
185.960786	6205.325904	26.103540
186.065560	6225.628719	26.108557
186.579318	6242.829103	26.113575
186.458951	6245.548286	26.118592
186.725235	6249.802359	26.123610
187.125303	6255.121221	26.128628
187.089723	6277.454229	26.133645
187.464138	6272.175776	26.138663
187.457788	6278.943438	26.143680
187.905263	6292.220611	26.148698
187.909819	6298.580055	26.153716
187.708054	6305.272172	26.158733
188.116158	6312.620251	26.163751
188.352235	6327.061920	26.168768
188.689290	6324.458939	26.173786
189.041549	6345.257319	26.178804
188.705502	6359.292004	26.183821
189.398360	6359.018239	26.188839
189.407922	6379.014868	26.193856
189.403492	6392.288171	26.198874
189.784958	6391.494915	26.203892
189.978312	6410.353735	26.208909
190.087790	6420.024434	26.213927
190.287036	6422.137813	26.218944
190.509389	6447.484415	26.223962
191.104752	6441.113100	26.228980
190.890300	6448.670634	26.233997
191.201682	6463.593027	26.239015
191.354447	6479.805074	26.244032
191.323916	6483.476655	26.249050
191.899743	6485.486744	26.254068
191.739076	6498.835622	26.259085
191.893060	6494.212677	26.264103
192.331300	6518.468996	26.269120
192.173851	6533.643924	26.274138
192.338872	6539.744545	26.279156
192.403439	6565.285225	26.284173
193.149003	6571.186571	26.289191
193.189227	6586.854977	26.294208
193.352221	6598.582146	26.299226
193.912014	6597.131603	26.304244
194.246618	6614.377803	26.309261
194.115331	6613.368537	26.314279
194.331356	6617.832669	26.319296
194.343712	6642.054133	26.324314
194.647467	6644.447187	26.329332
194.465449	6653.439279	26.334349
195.092290	6677.748112	26.339367
195.444887	6675.396128	26.344384
195.122270	6692.840216	26.349402
195.644001	6712.205059	26.354420
195.644397	6716.251224	26.359437
195.947779	6723.520737	26.364455
196.305370	6737.540960	26.369472
196.381007	6748.703772	26.374490
196.796494	6758.783226	26.379508
196.659506	6773.270520	26.384525
197.032873	6775.836382	26.389543
197.218586	6784.743256	26.394560
197.129722	6795.571798	26.399578
197.934115	6805.404952	26.404596
197.700459	6828.481996	26.409613
198.333273	6829.557194	26.414631
198.382842	6831.866329	26.419648
198.126950	6837.887088	26.424666
198.917645	6846.140907	26.429684
198.646459	6855.225853	26.434701
198.646047	6871.506981	26.439719
199.102376	6886.577489	26.444736
199.065274	6889.989533	26.449754
199.556669	6903.155190	26.454772
199.756232	6919.646652	26.459789
200.034112	6927.427738	26.464807
200.103603	6936.097157	26.469824
200.249104	6943.700098	26.474842
200.686575	6949.208347	26.479860
200.813422	6949.329165	26.484877
200.888528	6962.737073	26.489895
201.436285	6963.124548	26.494912
201.146821	6976.918126	26.499930
201.759737	6987.734598	26.504948
201.880696	7003.799638	26.509965
202.212906	7008.739305	26.514983
202.404933	7007.291320	26.520000
202.343104	7012.101663	26.525018
202.436599	7026.373807	26.530036
202.549804	7035.996217	26.535053
202.758262	7040.612167	26.540071
203.353461	7059.929041	26.545088
203.283715	7064.447695	26.550106
203.792653	7070.520733	26.555124
203.730825	7090.969599	26.560141
204.165223	7087.264178	26.565159
204.402789	7099.166840	26.570176
204.756622	7109.971147	26.575194
204.789550	7120.102346	26.580212
204.859047	7116.478592	26.585229
204.940288	7128.892363	26.590247
205.170807	7141.259378	26.595264
205.171491	7156.519785	26.600282
205.640689	7163.608454	26.605300
205.690638	7184.016881	26.610317
205.880942	7193.802277	26.615335
206.309765	7200.308462	26.620352
206.572302	7208.532540	26.625370
206.933892	7228.497170	26.630388
207.137527	7239.151564	26.635405
207.150487	7236.290166	26.640423
207.731677	7246.855283	26.645440
207.685124	7260.595504	26.650458
208.140706	7263.270717	26.655476
208.393875	7260.476676	26.660493
208.167208	7277.411642	26.665511
208.429576	7290.365052	26.670528
208.529214	7293.259881	26.675546
208.887986	7304.894512	26.680564
209.048590	7321.383388	26.685581
208.868704	7326.485120	26.690599
209.424477	7338.065897	26.695616
209.465156	7365.661382	26.700634
209.791079	7357.328854	26.705652
209.863423	7376.683044	26.710669
209.693521	7397.776407	26.715687
210.525714	7403.882710	26.720704
210.784076	7416.208308	26.725722
210.991851	7422.034378	26.730740
211.430857	7432.761791	26.735757
211.304463	7442.829772	26.740775
211.634277	7434.512314	26.745792
211.648380	7459.764250	26.750810
211.789908	7475.157610	26.755828
212.256470	7473.980004	26.760845
212.155999	7499.830712	26.765863
212.678074	7491.307317	26.770880
212.540161	7514.838184	26.775898
212.893098	7529.740525	26.780916
213.052637	7530.296260	26.785933
213.188144	7558.485271	26.790951
213.441945	7559.853275	26.795968
213.570582	7567.970524	26.800986
213.711217	7590.146235	26.806004
214.248628	7580.738030	26.811021
213.956930	7616.715748	26.816039
214.277215	7617.896306	26.821056
214.303384	7635.239574	26.826074
214.676978	7655.876240	26.831092
215.003748	7662.873708	26.836109
215.062633	7682.195838	26.841127
215.638416	7688.707830	26.846144
215.749229	7723.194986	26.851162
216.022575	7724.161977	26.856180
215.930432	7738.189004	26.861197
216.401742	7747.550124	26.866215
216.646651	7747.395402	26.871232
216.848945	7772.710417	26.876250
217.122228	7783.191379	26.881268
217.337680	7797.666160	26.886285
217.717608	7800.895147	26.891303
217.830135	7813.635900	26.896320
217.932208	7831.843540	26.901338
218.046670	7841.173988	26.906356
218.630642	7856.520471	26.911373
218.856843	7860.936008	26.916391
219.211695	7872.320424	26.921408
219.467349	7896.430265	26.926426
219.751016	7896.610995	26.931444
219.854169	7898.820040	26.936461
219.965733	7916.852121	26.941479
220.196132	7912.198001	26.946496
220.151635	7929.521778	26.951514
220.538283	7947.954993	26.956532
220.787940	7952.427327	26.961549
220.882424	7960.748935	26.966567
221.312952	7978.457310	26.971584
221.609494	7989.938113	26.976602
221.599551	8001.668951	26.981620
222.082211	8013.010256	26.986637
221.911864	8019.437939	26.991655
222.148611	8028.152738	26.996672
222.552114	8041.166108	27.001690
222.724387	8054.521039	27.006708
223.008381	8059.162594	27.011725
222.929636	8070.280208	27.016743
223.416672	8090.319682	27.021760
223.554364	8109.467012	27.026778
224.010043	8125.626658	27.031796
224.389527	8124.765122	27.036813
224.362266	8142.146144	27.041831
224.787475	8148.775417	27.046848
224.914682	8154.923095	27.051866
225.126527	8180.145800	27.056884
225.200901	8196.117351	27.061901
225.536365	8203.541357	27.066919
225.901587	8213.919158	27.071936
226.182401	8224.822964	27.076954
225.822129	8230.283327	27.081972
226.458608	8246.717232	27.086989
226.179936	8263.246714	27.092007
226.564777	8275.662325	27.097024
226.777580	8289.860709	27.102042
227.185496	8306.261614	27.107060
227.478354	8316.636494	27.112077
227.471706	8329.759746	27.117095
228.045307	8337.090040	27.122112
228.054424	8354.896951	27.127130
228.168511	8374.223385	27.132148
228.685696	8375.740071	27.137165
228.800577	8388.436780	27.142183
229.484856	8390.083355	27.147200
229.633755	8390.981975	27.152218
229.396660	8392.391139	27.157236
229.930064	8401.899917	27.162253
229.931927	8416.491754	27.167271
230.612655	8419.535586	27.172288
230.713403	8431.940842	27.177306
230.740042	8448.099364	27.182324
231.322442	8454.085156	27.187341
230.780102	8459.263000	27.192359
231.467575	8473.160831	27.197376
231.619400	8485.270146	27.202394
231.703099	8500.525974	27.207412
231.807826	8505.946481	27.212429
231.947300	8522.884387	27.217447
232.388939	8541.200478	27.222464
232.521847	8546.858960	27.227482
232.584296	8579.627653	27.232500
233.030720	8582.715029	27.237517
232.878456	8606.099416	27.242535
233.404607	8622.943485	27.247552
233.839683	8645.780899	27.252570
233.995158	8650.769244	27.257588
233.921289	8681.306951	27.262605
234.299985	8694.601465	27.267623
234.572489	8705.189510	27.272640
235.296631	8718.300032	27.277658
235.170698	8746.479275	27.282676
235.615633	8746.564787	27.287693
235.527889	8775.779962	27.292711
236.476829	8773.109968	27.297728
236.571208	8784.478286	27.302746
236.753734	8795.569696	27.307764
236.788148	8802.822456	27.312781
236.854070	8824.267816	27.317799
237.448527	8839.472505	27.322816
237.792857	8840.204094	27.327834
237.769057	8862.875148	27.332852
238.388800	8863.714761	27.337869
238.477893	8861.705435	27.342887
238.757318	8879.216100	27.347904
238.981797	8893.146825	27.352922
239.010103	8892.256729	27.357940
239.286065	8896.979424	27.362957
239.207668	8919.531977	27.367975
239.434706	8927.989701	27.372992
239.720360	8949.953444	27.378010
239.984714	8961.411916	27.383028
240.553220	8977.165380	27.388045
240.328029	8996.589691	27.393063
240.521895	9014.447894	27.398080
240.722316	9031.633063	27.403098
241.203768	9046.966945	27.408116
241.187816	9052.638431	27.413133
241.435275	9076.609612	27.418151
241.493847	9094.030239	27.423168
242.114613	9113.135046	27.428186
242.194947	9137.328562	27.433204
242.746059	9150.717022	27.438221
243.032416	9179.604738	27.443239
243.074383	9186.749283	27.448256
243.793060	9197.820760	27.453274
243.397443	9200.270105	27.458292
243.803578	9216.558014	27.463309
243.883339	9233.640478	27.468327
244.477471	9247.621400	27.473344
244.753665	9262.382086	27.478362
245.275095	9271.271807	27.483380
245.423291	9268.150539	27.488397
245.495995	9286.029888	27.493415
245.623229	9292.160669	27.498432
246.294854	9299.676071	27.503450
246.023634	9322.744808	27.508468
246.601411	9326.558197	27.513485
246.456821	9336.703643	27.518503
246.697171	9351.026032	27.523520
247.272972	9363.744117	27.528538
247.245626	9377.261607	27.533556
247.633256	9379.940558	27.538573
247.624029	9399.046790	27.543591
247.918231	9418.296614	27.548608
248.267198	9423.528899	27.553626
248.106693	9451.878962	27.558644
248.155983	9467.722796	27.563661
248.403558	9480.680437	27.568679
248.713979	9511.115144	27.573696
249.024570	9533.311898	27.578714
249.103176	9563.961544	27.583732
249.372172	9576.231908	27.588749
249.881866	9606.119378	27.593767
249.986459	9628.203043	27.598784
250.888346	9635.814416	27.603802
251.003353	9653.294059	27.608820
251.512450	9676.112027	27.613837
252.026263	9677.581348	27.618855
251.848495	9694.888127	27.623872
252.497821	9717.072393	27.628890
252.294976	9729.752644	27.633908
252.869298	9739.472886	27.638925
253.273638	9743.512038	27.643943
253.409808	9756.228366	27.648960
253.677197	9774.295831	27.653978
253.867168	9779.404868	27.658996
254.190475	9798.473075	27.664013
254.258915	9802.865635	27.669031
254.555060	9816.794754	27.674048
255.095935	9825.962816	27.679066
255.032414	9852.465872	27.684084
255.405163	9855.211181	27.689101
255.565821	9867.860519	27.694119
255.519951	9896.353103	27.699136
255.874898	9886.323819	27.704154
256.085875	9906.382121	27.709172
256.344282	9916.833860	27.714189
256.662538	9936.378906	27.719207
256.713469	9955.329307	27.724224
257.347982	9967.901075	27.729242
257.256169	9987.941847	27.734260
257.810808	10008.673699	27.739277
258.015647	10016.964716	27.744295
258.040214	10033.237835	27.749312
258.580549	10047.870437	27.754330
258.631771	10070.213283	27.759348
258.893350	10083.049343	27.764365
259.122231	10107.435595	27.769383
259.119956	10120.797509	27.774400
259.775176	10131.542953	27.779418
259.712402	10158.666406	27.784436
260.416960	10188.369080	27.789453
260.770029	10188.543871	27.794471
260.761877	10219.432082	27.799488
261.326198	10208.112143	27.804506
261.456259	10239.512450	27.809524
261.290733	10256.774474	27.814541
261.957865	10262.733536	27.819559
262.249879	10270.812509	27.824576
262.714416	10273.876739	27.829594
262.574355	10290.387719	27.834612
262.715005	10303.830121	27.839629
263.212227	10314.205561	27.844647
263.542049	10331.253315	27.849664
263.734107	10339.604127	27.854682
263.843899	10362.126763	27.859700
263.909061	10373.567220	27.864717
264.099653	10388.929264	27.869735
264.541803	10409.317848	27.874752
264.937755	10418.287281	27.879770
264.835059	10445.232683	27.884788
265.162770	10452.233588	27.889805
265.469246	10479.437484	27.894823
265.856094	10497.414295	27.899840
266.155361	10512.552840	27.904858
266.296077	10527.497048	27.909876
266.756953	10549.215743	27.914893
267.022398	10563.877774	27.919911
267.315609	10587.239358	27.924928
267.837450	10593.380164	27.929946
268.347847	10615.906963	27.934964
268.418669	10623.564199	27.939981
268.587289	10637.101518	27.944999
268.959300	10651.708173	27.950016
269.276233	10665.473079	27.955034
269.373479	10681.149448	27.960052
269.668046	10684.102443	27.965069
270.137138	10706.637781	27.970087
269.875399	10723.906775	27.975104
270.274740	10746.278811	27.980122
270.458516	10756.173831	27.985140
270.592266	10775.611775	27.990157
271.119603	10794.355884	27.995175
271.262683	10815.144295	28.000192
271.586256	10838.652487	28.005210
272.091226	10848.185557	28.010228
272.227765	10872.819883	28.015245
272.738654	10882.966526	28.020263
272.628111	10906.948484	28.025280
272.969975	10915.359888	28.030298
273.255849	10935.006051	28.035316
273.435842	10963.569494	28.040333
273.769204	10979.596275	28.045351
273.825600	10999.215896	28.050368
274.267077	11015.237423	28.055386
274.528046	11045.799823	28.060404
274.876072	11061.006449	28.065421
275.274370	11074.282363	28.070439
275.417241	11104.812423	28.075456
276.024805	11110.271124	28.080474
276.487103	11126.843978	28.085492
276.899495	11145.434191	28.090509
277.198998	11151.145593	28.095527
277.136946	11171.421631	28.100544
277.511213	11178.168543	28.105562
277.663013	11193.896258	28.110580
277.866677	11202.568627	28.115597
278.287283	11228.037322	28.120615
278.407555	11237.731997	28.125632
279.023088	11260.029568	28.130650
279.019301	11267.860187	28.135668
278.684259	11281.541293	28.140685
279.196042	11303.296700	28.145703
279.425427	11322.333410	28.150720
280.192959	11342.327377	28.155738
280.188606	11365.865404	28.160756
280.277275	11382.732004	28.165773
280.852097	11385.938138	28.170791
281.192155	11413.076595	28.175808
281.328405	11419.002632	28.180826
281.624342	11428.852711	28.185844
282.007253	11449.022355	28.190861
282.170173	11452.698505	28.195879
282.052819	11476.932982	28.200896
282.559816	11490.627739	28.205914
282.974453	11513.184249	28.210932
282.786946	11536.418773	28.215949
283.467616	11548.661897	28.220967
282.995588	11576.533845	28.225984
283.723313	11591.085625	28.231002
284.060724	11617.934917	28.236020
284.296668	11643.171674	28.241037
284.911901	11655.580139	28.246055
284.635152	11681.666080	28.251072
285.704446	11715.329495	28.256090
286.365057	11727.487830	28.261108
286.727660	11751.142168	28.266125
286.464874	11749.360915	28.271143
286.834812	11765.574672	28.276160
287.278795	11785.036542	28.281178
287.632918	11799.190214	28.286196
287.759851	11827.702507	28.291213
288.079808	11828.480039	28.296231
288.448256	11858.930061	28.301248
288.702860	11866.442431	28.306266
288.765563	11886.894116	28.311284
288.849718	11905.180246	28.316301
289.436450	11921.840478	28.321319
289.380007	11938.400752	28.326336
289.431848	11958.386304	28.331354
289.899430	11981.223080	28.336372
290.437856	12007.051700	28.341389
290.960666	12019.341798	28.346407
291.136483	12043.727150	28.351424
291.211706	12061.816379	28.356442
291.758098	12072.868734	28.361460
292.035046	12111.040230	28.366477
292.664728	12117.088134	28.371495
292.683146	12133.588941	28.376512
292.968277	12147.867798	28.381530
293.526327	12168.888673	28.386548
293.822822	12185.751650	28.391565
294.197955	12189.807292	28.396583
294.212036	12206.652426	28.401600
294.503091	12231.918799	28.406618
294.869451	12241.445699	28.411636
295.274303	12263.388716	28.416653
295.583654	12272.433403	28.421671
295.381773	12291.400807	28.426688
295.636349	12306.635106	28.431706
296.075097	12338.377630	28.436724
296.640904	12358.678873	28.441741
296.803653	12372.215465	28.446759
296.907422	12393.363827	28.451776
297.468308	12410.906601	28.456794
297.828906	12425.021928	28.461812
297.718733	12440.756393	28.466829
298.157322	12456.622243	28.471847
298.316457	12477.873438	28.476864
298.448267	12499.170156	28.481882
298.842262	12524.163076	28.486900
298.965057	12553.052388	28.491917
299.436364	12563.580130	28.496935
299.683729	12587.355618	28.501952
300.080839	12611.944730	28.506970
300.622740	12625.376228	28.511988
300.801084	12643.872952	28.517005
301.025818	12654.996280	28.522023
301.037821	12677.545413	28.527040
301.602986	12698.685566	28.532058
302.275217	12710.420381	28.537076
302.037114	12727.570970	28.542093
302.368606	12748.757746	28.547111
302.869275	12773.255894	28.552128
303.071578	12790.425057	28.557146
303.386756	12820.204906	28.562164
303.427823	12840.395042	28.567181
303.984002	12853.127811	28.572199
304.150419	12889.702542	28.577216
304.393580	12904.529552	28.582234
305.053440	12931.193694	28.587252
305.279262	12954.888185	28.592269
305.487882	12974.628406	28.597287
305.956543	12995.261712	28.602304
305.984962	13015.454157	28.607322
306.493281	13027.260459	28.612340
306.333427	13057.901031	28.617357
306.656713	13073.969377	28.622375
307.255917	13102.330091	28.627392
307.521375	13132.403986	28.632410
308.084534	13155.340064	28.637428
308.338484	13190.238360	28.642445
308.662050	13203.173805	28.647463
308.602500	13228.266515	28.652480
308.932823	13261.784397	28.657498
309.451261	13279.511645	28.662516
309.678705	13314.491815	28.667533
310.331723	13333.511196	28.672551
310.776658	13351.471323	28.677568
311.131319	13374.467436	28.682586
311.580388	13385.049825	28.687604
312.171158	13409.448916	28.692621
312.673612	13423.623583	28.697639
312.473495	13434.138521	28.702656
312.636272	13451.809778	28.707674
313.049941	13466.848627	28.712692
313.277092	13493.818556	28.717709
313.884153	13503.445046	28.722727
314.273109	13523.835330	28.727744
314.373124	13537.276108	28.732762
314.587441	13561.496611	28.737780
314.453668	13573.688535	28.742797
315.044237	13599.047719	28.747815
315.460021	13620.792185	28.752832
315.455843	13640.395074	28.757850
315.959113	13659.896662	28.762868
316.082932	13685.019610	28.767885
316.428013	13701.311912	28.772903
317.040896	13730.240391	28.777920
317.223667	13748.606828	28.782938
317.793240	13760.279022	28.787956
318.034044	13790.047737	28.792973
318.397071	13802.310477	28.797991
318.719320	13819.826505	28.803008
318.799664	13845.030968	28.808026
319.368508	13855.581231	28.813044
319.697594	13889.890190	28.818061
320.016541	13910.656605	28.823079
320.155311	13929.421380	28.828096
320.411825	13949.766349	28.833114
320.813033	13964.391651	28.838132
321.021389	13980.571324	28.843149
321.493534	13993.279498	28.848167
321.805419	14019.161421	28.853184
321.944211	14041.250162	28.858202
322.335002	14045.793829	28.863220
322.509946	14070.280071	28.868237
322.858965	14091.963719	28.873255
323.081413	14106.278311	28.878272
323.206407	14132.186617	28.883290
323.953215	14148.121308	28.888308
324.094677	14173.034049	28.893325
324.195220	14191.115144	28.898343
324.569867	14223.321123	28.903360
324.772908	14251.552402	28.908378
325.302225	14268.205637	28.913396
325.605965	14296.059410	28.918413
325.699721	14326.501197	28.923431
326.326197	14351.816207	28.928448
326.713089	14374.901382	28.933466
326.935488	14408.143178	28.938484
327.669959	14427.304813	28.943501
327.970012	14439.033136	28.948519
328.337928	14459.893013	28.953536
328.597110	14487.234383	28.958554
328.783266	14498.255030	28.963572
329.195514	14521.099804	28.968589
329.597394	14555.183762	28.973607
330.130935	14565.139845	28.978624
330.210515	14592.470138	28.983642
330.615096	14600.586234	28.988660
331.022856	14637.424384	28.993677
331.217565	14640.282737	28.998695
331.704078	14662.090960	29.003712
331.856406	14686.841921	29.008730
332.084543	14713.476413	29.013748
332.692815	14726.005020	29.018765
332.863341	14757.681591	29.023783
333.324424	14778.898413	29.028800
333.088887	14800.400779	29.033818
333.654560	14826.851926	29.038836
334.035686	14850.714169	29.043853
334.552165	14878.238989	29.048871
335.076871	14902.564563	29.053888
335.030149	14928.015527	29.058906
335.606230	14947.011702	29.063924
336.088903	14964.756160	29.068941
336.009049	15000.158027	29.073959
336.129405	15020.493763	29.078976
336.407043	15055.666360	29.083994
337.452669	15075.559016	29.089012
337.827628	15108.780134	29.094029
338.132765	15118.104502	29.099047
338.678431	15136.563742	29.104064
338.490372	15168.850525	29.109082
338.876690	15180.073347	29.114100
339.712744	15199.847956	29.119117
339.842101	15223.000592	29.124135
340.410412	15231.594270	29.129152
340.462249	15262.317401	29.134170
341.041195	15274.127832	29.139188
341.463272	15299.697223	29.144205
341.615223	15314.811038	29.149223
342.284085	15326.151118	29.154240
342.087452	15359.125319	29.159258
342.414389	15373.604983	29.164276
342.754911	15396.570027	29.169293
343.002030	15424.496557	29.174311
343.345778	15434.590186	29.179328
343.266719	15457.445076	29.184346
343.814180	15486.947029	29.189364
344.178668	15506.027735	29.194381
344.330474	15530.471123	29.199399
344.895834	15542.282420	29.204416
345.056276	15582.071661	29.209434
345.376183	15605.932525	29.214452
345.664941	15627.637634	29.219469
345.978296	15652.004027	29.224487
346.312033	15680.630667	29.229504
346.461163	15707.853578	29.234522
346.757676	15731.387496	29.239540
347.274515	15764.977351	29.244557
347.506834	15798.089492	29.249575
347.923580	15818.983996	29.254592
348.119811	15862.372757	29.259610
348.664242	15887.706873	29.264628
349.213470	15919.351373	29.269645
349.268123	15946.771578	29.274663
349.757096	15981.227099	29.279680
350.204605	16008.549286	29.284698
350.824687	16039.865472	29.289716
351.021428	16067.312800	29.294733
351.140034	16094.790444	29.299751
352.243619	16115.339943	29.304768
352.323160	16150.894434	29.309786
352.571075	16170.929909	29.314804
352.992355	16193.759752	29.319821
353.454009	16220.748941	29.324839
353.892167	16236.538150	29.329856
354.095643	16266.725775	29.334874
354.490220	16292.485680	29.339892
355.200801	16316.246661	29.344909
355.504349	16343.842277	29.349927
355.992072	16359.136339	29.354944
355.960788	16386.428058	29.359962
356.506322	16395.115965	29.364980
356.898097	16422.894144	29.369997
357.190030	16445.569203	29.375015
357.550338	16461.606375	29.380032
357.985347	16495.602175	29.385050
358.081252	16516.112462	29.390068
358.630168	16533.264434	29.395085
358.627609	16566.710174	29.400103
358.940220	16586.174293	29.405120
359.204892	16621.409120	29.410138
359.497063	16649.960778	29.415156
360.083274	16674.505778	29.420173
360.099513	16705.347823	29.425191
360.723908	16736.735551	29.430208
361.142347	16767.577351	29.435226
361.631914	16799.430450	29.440244
362.017607	16824.782820	29.445261
362.349803	16849.084810	29.450279
362.660587	16869.252593	29.455296
363.239257	16897.733617	29.460314
363.521990	16935.485055	29.465332
364.070724	16957.413706	29.470349
364.398027	16985.622798	29.475367
364.767730	17009.813204	29.480384
364.977668	17031.509559	29.485402
365.238793	17053.124961	29.490420
365.868357	17079.586495	29.495437
366.099881	17104.521863	29.500455
366.538410	17127.149949	29.505472
366.732100	17146.792042	29.510490
367.124855	17170.247452	29.515508
367.720022	17193.885353	29.520525
367.809085	17227.648291	29.525543
368.195353	17240.489848	29.530560
368.576524	17266.805207	29.535578
369.126718	17284.950842	29.540596
369.040477	17302.218191	29.545613
369.260566	17332.185897	29.550631
369.832783	17354.666062	29.555648
369.871890	17384.728446	29.560666
370.240913	17411.564664	29.565684
371.107479	17439.349517	29.570701
371.052122	17467.011134	29.575719
371.344644	17496.022910	29.580736
371.725552	17527.542289	29.585754
372.125141	17559.671841	29.590772
372.944040	17592.121423	29.595789
373.130587	17626.911017	29.600807
373.620118	17651.049424	29.605824
373.814294	17677.156773	29.610842
374.017419	17710.153035	29.615860
374.311593	17735.553472	29.620877
374.944109	17773.252079	29.625895
375.057370	17801.509016	29.630912
375.879380	17835.178684	29.635930
376.320014	17865.041489	29.640948
377.060174	17885.188315	29.645965
377.059010	17917.003395	29.650983
377.632478	17945.617924	29.656000
377.765258	17979.130809	29.661018
378.101346	18004.776946	29.666036
378.653966	18033.034078	29.671053
378.959831	18059.583854	29.676071
379.359981	18085.140692	29.681088
379.595683	18116.396734	29.686106
380.148171	18149.815279	29.691124
380.548604	18179.100450	29.696141
380.780440	18217.654588	29.701159
381.202553	18247.644108	29.706176
381.619906	18272.384948	29.711194
381.789755	18302.138862	29.716212
382.522215	18325.203904	29.721229
382.801265	18358.206224	29.726247
383.447963	18382.297613	29.731264
383.656611	18415.732609	29.736282
383.957409	18453.648455	29.741300
384.482342	18466.054983	29.746317
384.395804	18508.843233	29.751335
384.988902	18546.737715	29.756352
385.231482	18567.426468	29.761370
385.798107	18603.897188	29.766388
386.320639	18631.293261	29.771405
386.640024	18665.657887	29.776423
386.770940	18697.695372	29.781440
386.826640	18735.376537	29.786458
387.421518	18773.622794	29.791476
387.853284	18806.586539	29.796493
388.500955	18848.565225	29.801511
388.837352	18872.819032	29.806528
389.461370	18907.504215	29.811546
389.494245	18936.794792	29.816564
390.212589	18969.320460	29.821581
390.687794	19001.024083	29.826599
390.887339	19030.213145	29.831616
391.266868	19057.822766	29.836634
391.715080	19091.607288	29.841652
392.236313	19121.640306	29.846669
392.405400	19151.607111	29.851687
392.975092	19180.276412	29.856704
393.456411	19203.207664	29.861722
393.468102	19236.319026	29.866740
394.060432	19265.522321	29.871757
394.350667	19283.366328	29.876775
394.673852	19314.717339	29.881792
395.486210	19338.079562	29.886810
395.223385	19380.509809	29.891828
395.754080	19396.862151	29.896845
396.139600	19435.223398	29.901863
396.825171	19467.280921	29.906880
397.247097	19487.712534	29.911898
396.830209	19526.627722	29.916916
397.522873	19551.777367	29.921933
398.363583	19590.520838	29.926951
398.524480	19620.924968	29.931968
399.135364	19635.306188	29.936986
399.415189	19681.719646	29.942004
399.376829	19701.034234	29.947021
400.175134	19740.292725	29.952039
400.405755	19775.462605	29.957056
401.092002	19805.724948	29.962074
401.075402	19843.196694	29.967092
401.820490	19883.531673	29.972109
402.270522	19922.113539	29.977127
402.515589	19957.607763	29.982144
402.844124	19991.902650	29.987162
403.256077	20028.908163	29.992180
404.013471	20057.483263	29.997197
404.076764	20097.732938	30.002215
404.447190	20140.941624	30.007232
405.840406	20162.758396	30.012250
405.451239	20190.798230	30.017268
406.063851	20232.798804	30.022285
406.462101	20259.261106	30.027303
406.868360	20284.456098	30.032320
407.613628	20323.120886	30.037338
407.727799	20355.471750	30.042356
408.046367	20382.675836	30.047373
408.167678	20408.842076	30.052391
408.691695	20446.722338	30.057408
409.405059	20485.165743	30.062426
409.225338	20526.281241	30.067444
409.690037	20566.960674	30.072461
410.306405	20607.610375	30.077479
410.824275	20645.386465	30.082496
411.344583	20670.684565	30.087514
411.996157	20708.813916	30.092532
411.997400	20739.544478	30.097549
412.213376	20773.441770	30.102567
412.337377	20816.150598	30.107584
413.367078	20854.842065	30.112602
413.636926	20897.079186	30.117620
413.792898	20929.857820	30.122637
414.377942	20966.381089	30.127655
415.013582	21010.295466	30.132672
415.341025	21044.367212	30.137690
415.558630	21088.428230	30.142708
416.129224	21114.896468	30.147725
416.414410	21153.716563	30.152743
416.936840	21189.728789	30.157760
417.480914	21225.067409	30.162778
417.676050	21275.214002	30.167796
418.600094	21306.420414	30.172813
419.046423	21334.229273	30.177831
418.940295	21366.733633	30.182848
419.951237	21398.597518	30.187866
420.320153	21440.475877	30.192884
420.818999	21466.060958	30.197901
421.333281	21484.559259	30.202919
421.674506	21517.743555	30.207936
422.657439	21529.270857	30.212954
422.878993	21553.143897	30.217972
423.195331	21570.987591	30.222989
423.329447	21596.628499	30.228007
423.439844	21620.176298	30.233024
423.659704	21645.337949	30.238042
424.382718	21684.123073	30.243060
424.820075	21712.126404	30.248077
425.300243	21748.454284	30.253095
425.489065	21774.625659	30.258112
426.054410	21808.941818	30.263130
425.958915	21842.906991	30.268148
426.754713	21872.264053	30.273165
427.208378	21903.852154	30.278183
427.463234	21945.512547	30.283200
428.012224	21979.849104	30.288218
428.240262	22009.568414	30.293236
428.958912	22044.611806	30.298253
429.377577	22080.819705	30.303271
429.373265	22124.125443	30.308288
430.371775	22157.825056	30.313306
430.310686	22205.657919	30.318324
430.688767	22234.007782	30.323341
431.672277	22271.590618	30.328359
431.768584	22316.176330	30.333376
432.327421	22341.369644	30.338394
432.758899	22389.820040	30.343412
433.035647	22431.244634	30.348429
433.843711	22462.204319	30.353447
433.983272	22500.225344	30.358464
434.684189	22527.017979	30.363482
435.005217	22563.522164	30.368500
435.527337	22601.535298	30.373517
436.027049	22644.577617	30.378535
436.311317	22673.658048	30.383552
436.714460	22708.803909	30.388570
436.630683	22765.440910	30.393588
437.222998	22801.303086	30.398605
437.814909	22840.338045	30.403623
438.279637	22882.062192	30.408640
438.749248	22914.950451	30.413658
439.428835	22965.461817	30.418676
439.806223	23003.206502	30.423693
440.502751	23047.234354	30.428711
440.712562	23088.138640	30.433728
441.292202	23115.901558	30.438746
441.683246	23154.375993	30.443764
442.155095	23203.706663	30.448781
442.516952	23228.074485	30.453799
442.396103	23267.523254	30.458816
443.496131	23307.028692	30.463834
443.528204	23353.381264	30.468852
443.792747	23397.027359	30.473869
444.395953	23438.643225	30.478887
444.676011	23485.633193	30.483904
445.592947	23520.334592	30.488922
445.932637	23568.872920	30.493940
446.391044	23609.981742	30.498957
446.756732	23652.533132	30.503975
447.301091	23688.715771	30.508992
447.889180	23723.850469	30.514010
448.223366	23771.784739	30.519028
448.480499	23809.409184	30.524045
449.173408	23844.596171	30.529063
449.451962	23884.128502	30.534080
449.871758	23935.489982	30.539098
450.558579	23971.438333	30.544116
451.131381	23998.748080	30.549133
451.710441	24023.129982	30.554151
451.547662	24068.084849	30.559168
452.012629	24110.308710	30.564186
452.581694	24147.762431	30.569204
453.180460	24173.942199	30.574221
453.574484	24203.792415	30.579239
453.647258	24244.901924	30.584256
454.088999	24276.614680	30.589274
454.545458	24317.995195	30.594292
454.742137	24373.873581	30.599309
455.383649	24414.413127	30.604327
455.953436	24470.450867	30.609344
456.075574	24510.609792	30.614362
456.630181	24553.050156	30.619380
456.953917	24597.988983	30.624397
457.584704	24651.276357	30.629415
457.873024	24700.170186	30.634432
458.443728	24749.399069	30.639450
459.212389	24796.463177	30.644468
459.657183	24841.155515	30.649485
460.387148	24878.770301	30.654503
460.704221	24926.622321	30.659520
461.006196	24966.664238	30.664538
461.542764	25007.853378	30.669556
462.076626	25060.817419	30.674573
462.966041	25096.450739	30.679591
463.135333	25151.166003	30.684608
463.272555	25183.665745	30.689626
464.012106	25228.357627	30.694644
464.609991	25267.446036	30.699661
465.522385	25323.748440	30.704679
465.691482	25353.987993	30.709696
466.481286	25389.209437	30.714714
466.774427	25436.581092	30.719732
467.195169	25470.756652	30.724749
467.789201	25504.831057	30.729767
467.999163	25543.968516	30.734784
468.668308	25586.518652	30.739802
468.923130	25629.935475	30.744820
469.161490	25675.758662	30.749837
469.903181	25707.181552	30.754855
470.079483	25757.841224	30.759872
470.661627	25800.194949	30.764890
471.083508	25847.366637	30.769908
471.364047	25893.703878	30.774925
471.907716	25937.773929	30.779943
472.299195	25990.575136	30.784960
472.811305	26042.025425	30.789978
473.403666	26084.419165	30.794996
473.883697	26139.404732	30.800013
474.688934	26177.839496	30.805031
474.822013	26223.186328	30.810048
475.186268	26266.734898	30.815066
475.724646	26319.960722	30.820084
475.963657	26365.933888	30.825101
476.785982	26416.539060	30.830119
477.011207	26461.981673	30.835136
477.407210	26515.301055	30.840154
477.959767	26553.929880	30.845172
478.322907	26614.683620	30.850189
479.314453	26659.239732	30.855207
479.806240	26697.878936	30.860224
479.877548	26746.830254	30.865242
480.718223	26790.922733	30.870260
481.111324	26838.742242	30.875277
482.039464	26886.198911	30.880295
482.329666	26919.686034	30.885312
482.855145	26967.077067	30.890330
483.188897	26992.450124	30.895348
483.302172	27037.922236	30.900365
483.965715	27076.111162	30.905383
484.201231	27122.604253	30.910400
485.115497	27152.423971	30.915418
485.661133	27195.506389	30.920436
485.613521	27248.321002	30.925453
486.551984	27276.979220	30.930471
486.754472	27327.001936	30.935488
487.190122	27368.405840	30.940506
488.053513	27402.597150	30.945524
488.276133	27459.367665	30.950541
488.840024	27491.113448	30.955559
488.426868	27543.544651	30.960576
488.983528	27602.392854	30.965594
489.684941	27659.813507	30.970612
490.314994	27710.258694	30.975629
491.047670	27751.494487	30.980647
491.659770	27806.129102	30.985664
491.632337	27864.336660	30.990682
492.434451	27909.880039	30.995700
493.005340	27964.616611	31.000717
493.665676	28013.802115	31.005735
494.328085	28059.529892	31.010752
494.472519	28115.198729	31.015770
495.329372	28157.758834	31.020788
495.417384	28207.793561	31.025805
496.240188	28261.823741	31.030823
496.533954	28313.452554	31.035840
497.201298	28360.994271	31.040858
497.880296	28407.669792	31.045876
498.218140	28454.868790	31.050893
498.890923	28497.378162	31.055911
499.027177	28545.304808	31.060928
499.455619	28599.760934	31.065946
500.402375	28648.591670	31.070964
500.437349	28693.620465	31.075981
501.156959	28749.287639	31.080999
501.771643	28805.824150	31.086016
501.899787	28861.406572	31.091034
502.287343	28914.513873	31.096052
502.855740	28967.805940	31.101069
503.631720	29029.051897	31.106087
504.183714	29079.706412	31.111104
504.434109	29121.930698	31.116122
505.373364	29165.385078	31.121140
505.728461	29229.474513	31.126157
506.647034	29281.094292	31.131175
506.919434	29322.760161	31.136192
507.276868	29380.596749	31.141210
508.557940	29408.835830	31.146228
509.364724	29445.034433	31.151245
510.174318	29480.658450	31.156263
510.617439	29513.241876	31.161280
511.014108	29546.659645	31.166298
511.843841	29575.125115	31.171316
512.025568	29610.133959	31.176333
512.685645	29633.131669	31.181351
512.837281	29676.320121	31.186368
513.167532	29715.248306	31.191386
513.730043	29751.298665	31.196404
514.032158	29786.972572	31.201421
514.596324	29839.065945	31.206439
515.010630	29874.396502	31.211456
515.036562	29917.943932	31.216474
515.580740	29957.957286	31.221492
515.827062	30015.016133	31.226509
516.414583	30063.231935	31.231527
516.736545	30114.571133	31.236544
517.372335	30158.728134	31.241562
517.690196	30199.495683	31.246580
517.884922	30259.908225	31.251597
518.474508	30313.800344	31.256615
519.063613	30358.031828	31.261632
519.433633	30414.112355	31.266650
520.204055	30468.233744	31.271668
520.452062	30527.549876	31.276685
521.026616	30584.086144	31.281703
521.858785	30626.369232	31.286720
522.008317	30694.186380	31.291738
522.794504	30749.385086	31.296756
522.840914	30813.395704	31.301773
523.601035	30873.076295	31.306791
524.254557	30930.064419	31.311808
524.808284	30990.836549	31.316826
525.406710	31045.445676	31.321844
525.818017	31101.354331	31.326861
526.335467	31155.219943	31.331879
526.882846	31208.831503	31.336896
527.093824	31276.460871	31.341914
527.853962	31330.072303	31.346932
528.335897	31406.258577	31.351949
528.980112	31464.265965	31.356967
529.648302	31523.209853	31.361984
529.777355	31583.694586	31.367002
530.704834	31640.261036	31.372020
531.257533	31710.621665	31.377037
531.786430	31765.560055	31.382055
532.554682	31827.700537	31.387072
533.002680	31898.404237	31.392090
533.582291	31945.591537	31.397108
534.551746	32007.670961	31.402125
535.077403	32065.456972	31.407143
535.308525	32120.013443	31.412160
535.708423	32172.781436	31.417178
536.383748	32237.109653	31.422196
536.966489	32285.329163	31.427213
537.766209	32340.767260	31.432231
537.795214	32393.262799	31.437248
538.091206	32457.156017	31.442266
539.071751	32514.789339	31.447284
539.329209	32580.623681	31.452301
539.875133	32643.068868	31.457319
540.621035	32698.356056	31.462336
541.183613	32766.115945	31.467354
541.774629	32813.660241	31.472372
542.576470	32877.114696	31.477389
543.054227	32935.078705	31.482407
543.704109	32986.832689	31.487424
543.754108	33051.658610	31.492442
544.641625	33099.817280	31.497460
545.081366	33161.817987	31.502477
545.569692	33215.132981	31.507495
546.169427	33277.956475	31.512512
546.360101	33338.654718	31.517530
547.141840	33407.655656	31.522548
547.898744	33459.759360	31.527565
548.417557	33529.744653	31.532583
548.880086	33574.345927	31.537600
549.206931	33642.542610	31.542618
549.727559	33696.352293	31.547636
550.347096	33766.299758	31.552653
550.737659	33824.476737	31.557671
551.668875	33882.766416	31.562688
551.560469	33947.883720	31.567706
552.583852	33998.632126	31.572724
553.078036	34058.780834	31.577741
553.201652	34121.622958	31.582759
553.945495	34171.171582	31.587776
554.651120	34239.768611	31.592794
555.319887	34296.888091	31.597812
556.249625	34342.906667	31.602829
556.400406	34407.774475	31.607847
557.530924	34451.854004	31.612864
558.028981	34507.759012	31.617882
558.749191	34551.726794	31.622900
558.978424	34611.283718	31.627917
559.158487	34663.615763	31.632935
559.985628	34716.541499	31.637952
560.583908	34781.497566	31.642970
561.343218	34839.970290	31.647988
561.871965	34888.256264	31.653005
561.817294	34947.119640	31.658023
562.686004	34997.217952	31.663040
562.866256	35062.547167	31.668058
563.362659	35121.622904	31.673076
563.971763	35192.909467	31.678093
564.724443	35259.533301	31.683111
565.184760	35332.192625	31.688128
565.561730	35398.869671	31.693146
566.220974	35468.410083	31.698164
566.904504	35524.028774	31.703181
567.395646	35596.854490	31.708199
568.146460	35653.857408	31.713216
568.590188	35732.154594	31.718234
569.445362	35794.023080	31.723252
570.097314	35859.602212	31.728269
570.418763	35935.888010	31.733287
571.036439	35992.150257	31.738304
571.488225	36061.130780	31.743322
572.248437	36127.115890	31.748340
572.696379	36199.206342	31.753357
572.798338	36266.582254	31.758375
574.092854	36331.706457	31.763392
574.159376	36400.474277	31.768410
574.643702	36479.345559	31.773428
575.577232	36544.583911	31.778445
576.007988	36621.457345	31.783463
576.676292	36686.456033	31.788480
577.479678	36763.839692	31.793498
577.961699	36828.465715	31.798516
578.808768	36890.058392	31.803533
579.296253	36956.328367	31.808551
579.981306	37019.646354	31.813568
580.637657	37097.024200	31.818586
581.228022	37151.861623	31.823604
581.705321	37220.141644	31.828621
582.145419	37286.726826	31.833639
583.211261	37351.662127	31.838656
583.368658	37410.713057	31.843674
584.091237	37467.906276	31.848692
584.813094	37532.914919	31.853709
585.218120	37601.628126	31.858727
585.945589	37661.021129	31.863744
586.437487	37728.319011	31.868762
586.914526	37789.341529	31.873780
587.735034	37861.339068	31.878797
588.221438	37938.729676	31.883815
589.067525	37988.776901	31.888832
589.125015	38053.490143	31.893850
589.754125	38116.057346	31.898868
590.676604	38181.060363	31.903885
591.206692	38248.584270	31.908903
592.030794	38290.697430	31.913920
592.230127	38359.327578	31.918938
592.691506	38414.351127	31.923956
593.238717	38475.298044	31.928973
593.674372	38537.150604	31.933991
594.525608	38599.916300	31.939008
595.131938	38671.756769	31.944026
595.741631	38733.066681	31.949044
596.254656	38796.397214	31.954061
596.517929	38856.622176	31.959079
597.357794	38916.164815	31.964096
597.707366	38989.447380	31.969114
598.432466	39060.518455	31.974132
598.918043	39118.579940	31.979149
599.261540	39202.991471	31.984167
600.328676	39269.022433	31.989184
600.731074	39343.702384	31.994202
601.277665	39413.791073	31.999220
601.906949	39483.528583	32.004237
602.305597	39556.536976	32.009255
603.263926	39629.405712	32.014272
603.399911	39697.899830	32.019290
604.045242	39784.290713	32.024308
604.937097	39853.430601	32.029325
605.413849	39942.972147	32.034343
606.230162	40011.717906	32.039360
606.677560	40088.789434	32.044378
607.115583	40157.831927	32.049396
608.087780	40225.252090	32.054413
608.428386	40319.998328	32.059431
609.005888	40385.369301	32.064448
610.116361	40462.790435	32.069466
610.927068	40533.029105	32.074484
611.364095	40603.759200	32.079501
611.665045	40691.249926	32.084519
612.366503	40756.806906	32.089536
613.102974	40837.792500	32.094554
613.747270	40905.177850	32.099572
614.329109	40975.847529	32.104589
614.586294	41063.426180	32.109607
615.489967	41128.190197	32.114624
616.155069	41204.223293	32.119642
616.467680	41294.379435	32.124660
617.415659	41376.023777	32.129677
617.841825	41454.121073	32.134695
618.657545	41528.665723	32.139712
619.432815	41601.307351	32.144730
619.727882	41679.499897	32.149748
620.552944	41757.983939	32.154765
620.858718	41835.316646	32.159783
621.707144	41914.248948	32.164800
622.504149	42002.620401	32.169818
623.362065	42083.506109	32.174836
623.638584	42158.455052	32.179853
624.024855	42225.509034	32.184871
624.448433	42296.358315	32.189888
625.327988	42386.233376	32.194906
625.784237	42463.423827	32.199924
626.801492	42544.029444	32.204941
627.191290	42627.672278	32.209959
628.096251	42704.517973	32.214976
628.895919	42781.226699	32.219994
629.379728	42854.436075	32.225012
630.205891	42920.611526	32.230029
630.751918	42997.637787	32.235047
631.129366	43076.649781	32.240064
631.838628	43146.678336	32.245082
632.708170	43219.629577	32.250100
633.418377	43283.757453	32.255117
633.616132	43349.435336	32.260135
634.405905	43423.739286	32.265152
634.863331	43488.149642	32.270170
635.750833	43560.474084	32.275188
636.288694	43633.424981	32.280205
636.267963	43704.214185	32.285223
636.945844	43779.425290	32.290240
637.771849	43857.902235	32.295258
638.196380	43942.887115	32.300276
639.445597	44006.580978	32.305293
639.990945	44096.049098	32.310311
640.438364	44162.206351	32.315328
641.268252	44244.908986	32.320346
641.676909	44325.319855	32.325364
642.450211	44390.400966	32.330381
643.019487	44479.314387	32.335399
643.601987	44553.316093	32.340416
644.410270	44629.415249	32.345434
645.285007	44720.205387	32.350452
646.202449	44792.542261	32.355469
646.646437	44865.207188	32.360487
647.174438	44944.514745	32.365504
648.026256	45015.808690	32.370522
648.359811	45102.986310	32.375540
649.044626	45180.895346	32.380557
649.865817	45264.844863	32.385575
650.552215	45337.165213	32.390592
651.311293	45415.223973	32.395610
651.919146	45496.626822	32.400628
652.391034	45566.410007	32.405645
653.154094	45653.812784	32.410663
653.510152	45723.236782	32.415680
654.256520	45805.533792	32.420698
654.674281	45903.090197	32.425716
655.394769	45970.680146	32.430733
656.213196	46063.671252	32.435751
656.563091	46150.124702	32.440768
657.308066	46227.835475	32.445786
658.182079	46324.314380	32.450804
658.946017	46405.310059	32.455821
659.731821	46490.148754	32.460839
660.289673	46580.469733	32.465856
660.996610	46661.750673	32.470874
661.124273	46749.033089	32.475892
662.004906	46824.794379	32.480909
662.940070	46918.761954	32.485927
663.484732	46996.600592	32.490944
664.425679	47079.098313	32.495962
664.957999	47169.884221	32.500980
665.661162	47246.033401	32.505997
666.416850	47337.345279	32.511015
666.980996	47420.089976	32.516032
667.928502	47493.322763	32.521050
668.217410	47581.804478	32.526068
669.328757	47668.789422	32.531085
669.966243	47745.895726	32.536103
670.149822	47819.369830	32.541120
671.042328	47901.067494	32.546138
671.858056	47995.874930	32.551156
672.681207	48065.359689	32.556173
673.288304	48153.001878	32.561191
674.215757	48232.509740	32.566208
675.041032	48300.715949	32.571226
675.193666	48376.275387	32.576244
675.842538	48455.372324	32.581261
676.458953	48547.641536	32.586279
676.840049	48626.110775	32.591296
677.881269	48698.606288	32.596314
678.042563	48782.977375	32.601332
679.330635	48864.623190	32.606349
679.944588	48940.958110	32.611367
680.453927	49005.991335	32.616384
680.928988	49074.305606	32.621402
681.289077	49162.694412	32.626420
682.238476	49256.080519	32.631437
683.087712	49337.504059	32.636455
683.474230	49418.347550	32.641472
684.349698	49502.609967	32.646490
684.624143	49593.052064	32.651508
685.341134	49672.717569	32.656525
686.179979	49755.824863	32.661543
686.542548	49858.884112	32.666560
687.545839	49934.687960	32.671578
687.592130	50030.545512	32.676596
688.435703	50122.516228	32.681613
689.474499	50223.131447	32.686631
690.007790	50328.751760	32.691648
690.908021	50419.087886	32.696666
691.435045	50518.683821	32.701684
691.908777	50614.997874	32.706701
692.525969	50713.234351	32.711719
693.243121	50805.358727	32.716736
694.245813	50913.349319	32.721754
694.810467	51016.934057	32.726772
695.297902	51106.267744	32.731789
696.332141	51209.377841	32.736807
696.948144	51324.491105	32.741824
697.769678	51405.274093	32.746842
698.581605	51511.985561	32.751860
699.155244	51613.348269	32.756877
700.063320	51707.087870	32.761895
700.638441	51804.452379	32.766912
701.749173	51904.729595	32.771930
702.044426	51996.354513	32.776948
702.619458	52097.068798	32.781965
703.848086	52191.136758	32.786983
704.566724	52296.459126	32.792000
705.484738	52381.273496	32.797018
705.919382	52481.975084	32.802036
706.579322	52559.232719	32.807053
707.523842	52655.769605	32.812071
708.071325	52759.998222	32.817088
708.863003	52852.492703	32.822106
709.715418	52942.772643	32.827124
710.054765	53047.334157	32.832141
711.167376	53141.508015	32.837159
711.542986	53232.272508	32.842176
712.489495	53328.723931	32.847194
713.501887	53419.011191	32.852212
714.112379	53521.773974	32.857229
715.199418	53614.715999	32.862247
715.535789	53702.197439	32.867264
716.934975	53786.774030	32.872282
717.068402	53868.142244	32.877300
717.761020	53955.515335	32.882317
718.432892	54045.830212	32.887335
719.206815	54147.059174	32.892352
719.582233	54236.545728	32.897370
720.054023	54333.541839	32.902388
720.915160	54434.075471	32.907405
721.793362	54526.689884	32.912423
722.176003	54617.731287	32.917440
723.688682	54707.183494	32.922458
724.299934	54805.978561	32.927476
724.977811	54898.766861	32.932493
725.706221	54972.629630	32.937511
726.293990	55062.350173	32.942528
727.082783	55137.909573	32.947546
727.722081	55226.731421	32.952564
728.113778	55314.482548	32.957581
729.207484	55396.033091	32.962599
729.487665	55487.531426	32.967616
730.261869	55569.849544	32.972634
730.912312	55670.784476	32.977652
731.437115	55759.400173	32.982669
732.451207	55857.868458	32.987687
732.715340	55963.285606	32.992704
733.560918	56059.804976	32.997722
734.170523	56162.600581	33.002740
734.754050	56261.843483	33.007757
735.704835	56370.447677	33.012775
736.066357	56474.012604	33.017792
737.109092	56577.162074	33.022810
737.820281	56685.049333	33.027828
738.468078	56784.442179	33.032845
739.285710	56892.932223	33.037863
739.797698	57008.215944	33.042880
740.642716	57109.808444	33.047898
741.720460	57221.764393	33.052916
742.542548	57327.374494	33.057933
743.620531	57432.102360	33.062951
744.318858	57537.430714	33.067968
745.334949	57630.118921	33.072986
745.863961	57731.811082	33.078004
746.539625	57844.273054	33.083021
747.843594	57925.274654	33.088039
748.606643	58036.806931	33.093056
749.193785	58140.747599	33.098074
750.203858	58230.273501	33.103092
750.447005	58331.036450	33.108109
751.527131	58420.753838	33.113127
751.734803	58530.756581	33.118144
752.617244	58627.629811	33.123162
753.682339	58733.579968	33.128180
753.951302	58843.435243	33.133197
755.088733	58937.474466	33.138215
755.609772	59042.334440	33.143232
756.271162	59149.592234	33.148250
757.106948	59262.591779	33.153268
757.643788	59376.026916	33.158285
758.683196	59477.877295	33.163303
759.295994	59591.686591	33.168320
759.819511	59687.050598	33.173338
760.982529	59788.667216	33.178356
761.423951	59911.386282	33.183373
762.493858	60006.617174	33.188391
763.160908	60127.126113	33.193408
763.780826	60238.662613	33.198426
764.121071	60343.192648	33.203444
764.971710	60468.343864	33.208461
766.412088	60564.369324	33.213479
767.099232	60687.766619	33.218496
767.615939	60804.701865	33.223514
768.424464	60914.264204	33.228532
769.290549	61014.608786	33.233549
770.114599	61128.366453	33.238567
771.094181	61240.601076	33.243584
771.768327	61349.777149	33.248602
772.455134	61455.469093	33.253620
773.104478	61565.560576	33.258637
774.053477	61671.956099	33.263655
774.895677	61783.717098	33.268672
775.778320	61878.728563	33.273690
776.788287	61979.092002	33.278708
776.934452	62083.384924	33.283725
778.020441	62169.148479	33.288743
778.653091	62279.107497	33.293760
779.035589	62381.491887	33.298778
779.949312	62475.091429	33.303796
780.759906	62589.788597	33.308813
781.461658	62695.162089	33.313831
782.264855	62801.220966	33.318848
782.861990	62905.923855	33.323866
783.536261	63018.035389	33.328884
784.174446	63128.775512	33.333901
785.243531	63236.865956	33.338919
785.871142	63346.180429	33.343936
786.468775	63466.967008	33.348954
787.535215	63582.133068	33.353972
788.133793	63707.105519	33.358989
788.751378	63819.938756	33.364007
789.576953	63945.323908	33.369024
790.214835	64055.443232	33.374042
791.365904	64176.957864	33.379060
792.120551	64312.774588	33.384077
793.133036	64437.038193	33.389095
793.483320	64550.494863	33.394112
794.366175	64678.504705	33.399130
795.390886	64796.440593	33.404148
795.835433	64923.885961	33.409165
797.108369	65042.768357	33.414183
797.750054	65163.190857	33.419200
798.648595	65289.096740	33.424218
799.454586	65404.037821	33.429236
800.029298	65530.169404	33.434253
801.257654	65652.103421	33.439271
802.057127	65774.058511	33.444288
803.102401	65891.029939	33.449306
804.105756	66017.226321	33.454324
804.755720	66142.451432	33.459341
805.909269	66256.214399	33.464359
806.785764	66362.418402	33.469376
807.429708	66480.926211	33.474394
808.463560	66591.233655	33.479412
808.792079	66712.741038	33.484429
809.832978	66824.559532	33.489447
810.559028	66941.861467	33.494464
811.084584	67059.247794	33.499482
812.312303	67183.403599	33.504500
812.503596	67307.971802	33.509517
813.630808	67427.770628	33.514535
814.608583	67554.068974	33.519552
815.271464	67669.406494	33.524570
816.130040	67788.587942	33.529588
816.832323	67921.446180	33.534605
817.605941	68037.532413	33.539623
819.055980	68163.237840	33.544640
819.876784	68285.058518	33.549658
820.580395	68387.419228	33.554676
821.006165	68513.163359	33.559693
822.132759	68630.629706	33.564711
822.876608	68745.087152	33.569728
823.550485	68862.243966	33.574746
824.509429	68980.808525	33.579764
825.439507	69103.071061	33.584781
826.042517	69218.528064	33.589799
826.624825	69349.815384	33.594816
827.472421	69467.952140	33.599834
828.515479	69587.909860	33.604852
829.458516	69725.178285	33.609869
830.040168	69841.622258	33.614887
831.067513	69946.004555	33.619904
831.877789	70060.970243	33.624922
832.506041	70163.054753	33.629940
833.265020	70286.547436	33.634957
834.086530	70401.171639	33.639975
834.693113	70515.275553	33.644992
835.378705	70636.234110	33.650010
836.377376	70752.557149	33.655028
836.950078	70881.642275	33.660045
837.891162	70999.202907	33.665063
838.551663	71132.568610	33.670080
839.252622	71268.881515	33.675098
840.118072	71385.230006	33.680116
840.748967	71519.089906	33.685133
841.778218	71653.700498	33.690151
842.609871	71786.833258	33.695168
843.465960	71922.681978	33.700186
844.392288	72057.217248	33.705204
845.097498	72196.425238	33.710221
846.217739	72330.841604	33.715239
847.204311	72463.124484	33.720256
848.063004	72604.681148	33.725274
849.043534	72724.906992	33.730292
849.909604	72872.769124	33.735309
850.876282	72989.166405	33.740327
851.725603	73121.564527	33.745344
852.195280	73252.552734	33.750362
853.224931	73387.477570	33.755380
854.321521	73528.981928	33.760397
855.100362	73659.567295	33.765415
855.768522	73804.040766	33.770432
856.540970	73953.936812	33.775450
857.667824	74088.078339	33.780468
858.329320	74216.871363	33.785485
859.285171	74362.255914	33.790503
860.242484	74492.456242	33.795520
861.196617	74629.406069	33.800538
861.815073	74763.989981	33.805556
862.934624	74911.020760	33.810573
863.875622	75047.229066	33.815591
864.618477	75172.649560	33.820608
864.913230	75329.350740	33.825626
866.020626	75465.831374	33.830644
867.043358	75609.303044	33.835661
867.682703	75758.746400	33.840679
868.772061	75902.398699	33.845696
869.361493	76039.828715	33.850714
870.398834	76188.601967	33.855732
871.307275	76337.998405	33.860749
872.204964	76479.978411	33.865767
873.015185	76617.647469	33.870784
873.691974	76772.252691	33.875802
874.688232	76912.492415	33.880820
875.874004	77068.463971	33.885837
876.843497	77207.615729	33.890855
877.779184	77341.751709	33.895872
878.588354	77485.226550	33.900890
879.314158	77629.867307	33.905908
880.374127	77782.923393	33.910925
881.233191	77923.097281	33.915943
882.269600	78054.823560	33.920960
882.834175	78203.720083	33.925978
883.942618	78342.343564	33.930996
884.767811	78482.267206	33.936013
885.599453	78639.029401	33.941031
886.480488	78774.966828	33.946048
887.212095	78915.844841	33.951066
887.999527	79049.870077	33.956084
888.993528	79180.376458	33.961101
889.912324	79325.799600	33.966119
891.156544	79454.457011	33.971136
891.686889	79596.137986	33.976154
892.292206	79726.155126	33.981172
893.362379	79855.400285	33.986189
894.354817	79998.746998	33.991207
895.036015	80137.692570	33.996224
895.815976	80288.230984	34.001242
896.795264	80427.647774	34.006260
897.809938	80571.475216	34.011277
898.393069	80708.542657	34.016295
899.182641	80847.430367	34.021312
900.416560	81001.270310	34.026330
901.367232	81145.947036	34.031348
902.110367	81295.758033	34.036365
903.081120	81439.035176	34.041383
903.849935	81592.101959	34.046400
904.515052	81753.721323	34.051418
905.375756	81893.552609	34.056436
906.531494	82052.771121	34.061453
907.591977	82216.087149	34.066471
908.585300	82362.567601	34.071488
909.188557	82525.467964	34.076506
910.286593	82683.846297	34.081524
911.221648	82830.965719	34.086541
912.121951	82988.594330	34.091559
913.244458	83145.510301	34.096576
914.146192	83302.033620	34.101594
915.148486	83454.783170	34.106612
915.792429	83608.415497	34.111629
916.847797	83770.769043	34.116647
917.944072	83911.225317	34.121664
918.658716	84068.835058	34.126682
919.984388	84230.805467	34.131700
920.942145	84382.492888	34.136717
921.665275	84528.070031	34.141735
922.903905	84682.028727	34.146752
923.677488	84841.019635	34.151770
924.686500	84983.369711	34.156788
925.829075	85137.518144	34.161805
926.329905	85290.381682	34.166823
927.543301	85437.028697	34.171840
928.086764	85600.966632	34.176858
929.185949	85758.460942	34.181876
930.431461	85910.022132	34.186893
931.286232	86068.052495	34.191911
932.030011	86214.883285	34.196928
933.074397	86374.017009	34.201946
933.998276	86537.892258	34.206964
934.869214	86687.090542	34.211981
935.699059	86849.585064	34.216999
937.079707	87001.751081	34.222016
937.840305	87165.145135	34.227034
938.585471	87320.506330	34.232052
939.506458	87469.100126	34.237069
940.747437	87629.665264	34.242087
941.787012	87782.797629	34.247104
942.721856	87938.720031	34.252122
943.640701	88090.678329	34.257140
944.541542	88234.173407	34.262157
945.535403	88402.264608	34.267175
946.186174	88550.093513	34.272192
947.177693	88712.612052	34.277210
948.155228	88860.977390	34.282228
949.029132	89016.391678	34.287245
949.819691	89187.395145	34.292263
950.883175	89336.223861	34.297280
951.702185	89492.511001	34.302298
952.708557	89638.674061	34.307316
953.710108	89783.414867	34.312333
954.431700	89940.233657	34.317351
955.599436	90080.417441	34.322368
956.211868	90226.206212	34.327386
956.662261	90381.832292	34.332404
957.731684	90537.850664	34.337421
958.862177	90715.504719	34.342439
959.968283	90875.208950	34.347456
960.680116	91029.466904	34.352474
961.455922	91199.835246	34.357492
962.756478	91350.580234	34.362509
963.514791	91533.200528	34.367527
964.632314	91689.528511	34.372544
965.680508	91855.514635	34.377562
966.414947	92027.914646	34.382580
967.654150	92197.289303	34.387597
968.598159	92369.644423	34.392615
969.292745	92532.623922	34.397632
970.282536	92712.752678	34.402650
971.472848	92882.817431	34.407668
972.533604	93056.221443	34.412685
972.935693	93227.317715	34.417703
974.322497	93391.365772	34.422720
975.307037	93574.533610	34.427738
976.185982	93752.226120	34.432756
977.659562	93919.694045	34.437773
978.366958	94099.651821	34.442791
979.738164	94268.810108	34.447808
980.404520	94446.504804	34.452826
981.345636	94616.958256	34.457844
982.333504	94786.417684	34.462861
983.011131	94975.919658	34.467879
984.287290	95146.359339	34.472896
985.220516	95327.282529	34.477914
986.080467	95507.149364	34.482932
987.607360	95685.793113	34.487949
988.686545	95869.620656	34.492967
989.771000	96037.857260	34.497984
990.457020	96221.113051	34.503002
991.787529	96388.279497	34.508020
993.013819	96559.984191	34.513037
993.538770	96728.723111	34.518055
995.112174	96908.615027	34.523072
996.060469	97070.822837	34.528090
996.812665	97241.901581	34.533108
998.186440	97414.562654	34.538125
999.181135	97583.957674	34.543143
1000.399665	97747.226702	34.548160
1001.642536	97915.728277	34.553178
1002.593276	98076.701349	34.558196
1003.443618	98229.911484	34.563213
1004.430733	98404.270292	34.568231
1005.535145	98567.386233	34.573248
1006.277689	98733.519604	34.578266
1007.285140	98902.756757	34.583284
1008.621518	99061.177924	34.588301
1009.465034	99231.039488	34.593319
1010.392839	99401.742947	34.598336
1011.367031	99561.993499	34.603354
1012.352953	99738.723185	34.608372
1013.450973	99893.250948	34.613389
1014.202272	100072.326303	34.618407
1015.188410	100240.258965	34.623424
1016.450569	100418.619146	34.628442
1017.051708	100587.700405	34.633460
1018.335944	100747.793162	34.638477
1018.851847	100911.065725	34.643495
1019.859634	101071.586098	34.648512
1021.045099	101232.685923	34.653530
1022.113169	101400.131428	34.658548
1023.196671	101550.783980	34.663565
1024.095599	101717.658008	34.668583
1024.884163	101886.311578	34.673600
1025.770984	102054.785375	34.678618
1026.923358	102217.334125	34.683636
1028.049060	102385.662937	34.688653
1029.078862	102564.411971	34.693671
1029.887124	102729.167331	34.698688
1031.219239	102911.439969	34.703706
1031.805280	103089.702440	34.708724
1033.090275	103258.783072	34.713741
1033.683774	103432.094989	34.718759
1034.849723	103620.206582	34.723776
1035.912980	103802.156300	34.728794
1036.600438	103989.602463	34.733812
1038.026727	104168.113292	34.738829
1038.956653	104364.197248	34.743847
1039.510299	104550.048463	34.748864
1040.856918	104739.835284	34.753882
1041.985068	104929.482285	34.758900
1043.406055	105117.068499	34.763917
1044.449075	105298.816612	34.768935
1045.543364	105496.097656	34.773952
1046.942501	105678.422756	34.778970
1047.964394	105863.825834	34.783988
1048.908868	106047.913137	34.789005
1050.003486	106236.245171	34.794023
1050.974550	106419.368069	34.799040
1052.354138	106596.256488	34.804058
1053.208334	106798.779832	34.809076
1054.653606	106981.980178	34.814093
1055.510359	107169.902159	34.819111
1056.134816	107345.628459	34.824128
1057.743497	107538.609121	34.829146
1058.577602	107727.184724	34.834164
1059.544100	107911.458546	34.839181
1060.570781	108100.815573	34.844199
1061.856641	108290.865736	34.849216
1062.963528	108484.582138	34.854234
1063.985473	108674.893971	34.859252
1065.102499	108860.492054	34.864269
1065.884454	109048.173502	34.869287
1067.027517	109245.043410	34.874304
1068.450384	109433.837588	34.879322
1069.232951	109638.990853	34.884340
1070.320713	109806.498928	34.889357
1071.549322	110003.765533	34.894375
1072.420336	110199.116574	34.899392
1073.829969	110381.408471	34.904410
1074.579439	110582.204018	34.909428
1075.939111	110763.290633	34.914445
1076.931312	110959.019754	34.919463
1077.536802	111148.391617	34.924480
1078.939981	111327.941956	34.929498
1080.096455	111535.213813	34.934516
1081.330309	111728.830903	34.939533
1082.058685	111926.992118	34.944551
1083.125335	112119.334764	34.949568
1084.435568	112314.476186	34.954586
1085.455414	112513.657550	34.959604
1086.550591	112714.804180	34.964621
1087.740880	112897.731728	34.969639
1088.741711	113096.236303	34.974656
1089.943863	113280.152560	34.979674
1090.581882	113472.879482	34.984692
1092.165116	113650.666783	34.989709
1093.294996	113836.777712	34.994727
1093.631872	114021.665383	34.999744
1095.258769	114197.371198	35.004762
1095.868925	114394.403922	35.009780
1097.212335	114577.481835	35.014797
1098.225543	114762.629973	35.019815
1099.052001	114953.853573	35.024832
1100.237422	115146.400113	35.029850
1101.480077	115351.494196	35.034868
1102.402747	115542.921256	35.039885
1103.423708	115750.639519	35.044903
1104.200749	115949.708010	35.049920
1105.747463	116148.625309	35.054938
1106.717554	116360.841645	35.059956
1107.554966	116555.203749	35.064973
1108.846463	116760.692694	35.069991
1110.090707	116967.584676	35.075008
1111.195759	117166.011907	35.080026
1112.047712	117384.362558	35.085044
1113.424717	117593.555829	35.090061
1114.639592	117799.267609	35.095079
1115.640178	118019.055645	35.100096
1117.068584	118218.868488	35.105114
1118.247503	118426.706740	35.110132
1118.894753	118637.029230	35.115149
1120.481843	118850.758498	35.120167
1121.551073	119056.959463	35.125184
1122.878571	119264.665110	35.130202
1123.646257	119482.969493	35.135220
1124.514538	119689.296853	35.140237
1126.200558	119901.281461	35.145255
1126.911909	120116.457299	35.150272
1128.662066	120325.519858	35.155290
1129.494426	120544.670482	35.160308
1130.628144	120756.549824	35.165325
1132.243601	120965.208350	35.170343
1133.012849	121183.715206	35.175360
1134.411405	121389.928826	35.180378
1135.296138	121620.306497	35.185396
1136.678929	121822.432529	35.190413
1137.745095	122040.845931	35.195431
1138.774197	122254.033226	35.200448
1140.592921	122465.836901	35.205466
1141.236236	122678.355982	35.210484
1142.248401	122885.784415	35.215501
1143.523450	123108.479924	35.220519
1144.662640	123322.670492	35.225536
1145.923820	123529.491921	35.230554
1146.628332	123747.242522	35.235572
1147.987699	123971.780803	35.240589
1149.139209	124181.083488	35.245607
1149.832061	124408.421989	35.250624
1151.569339	124624.487351	35.255642
1152.780618	124838.144464	35.260660
1153.622178	125056.262046	35.265677
1154.962424	125276.884250	35.270695
1155.938811	125501.991462	35.275712
1157.395696	125719.771266	35.280730
1158.702331	125938.718145	35.285748
1159.929022	126160.417469	35.290765
1160.590125	126368.041848	35.295783
1161.767851	126595.810801	35.300800
1163.261454	126812.869850	35.305818
1164.326503	127041.066310	35.310836
1165.246341	127243.913470	35.315853
1166.646001	127455.187500	35.320871
1167.747320	127671.734385	35.325888
1168.804856	127865.132659	35.330906
1169.974760	128077.805142	35.335924
1171.040525	128284.285425	35.340941
1172.659078	128489.889827	35.345959
1173.477553	128693.561749	35.350976
1174.756213	128902.938950	35.355994
1175.646835	129116.843497	35.361012
1176.801313	129327.929915	35.366029
1177.936274	129541.467397	35.371047
1178.972525	129761.208451	35.376064
1179.817469	129989.374122	35.381082
1180.913160	130213.240849	35.386100
1182.032934	130445.344648	35.391117
1183.084071	130662.807805	35.396135
1184.158900	130905.316879	35.401152
1185.383708	131132.933608	35.406170
1186.518135	131376.044881	35.411188
1187.606985	131612.523011	35.416205
1188.967006	131849.984874	35.421223
1189.714277	132094.014933	35.426240
1191.599882	132342.637854	35.431258
1192.643381	132583.985876	35.436276
1193.956329	132826.368712	35.441293
1194.908044	133073.059924	35.446311
1195.993864	133307.243762	35.451328
1197.593626	133572.568618	35.456346
1198.681850	133813.981799	35.461364
1199.664552	134061.702268	35.466381
1201.155217	134303.394842	35.471399
1202.431234	134556.813545	35.476416
1203.796018	134803.893301	35.481434
1205.184542	135054.685622	35.486452
1206.135529	135308.861141	35.491469
1207.430599	135550.100781	35.496487
1208.463106	135805.876770	35.501504
1209.507498	136046.869871	35.506522
1211.172836	136304.598988	35.511540
1212.054615	136561.648200	35.516557
1213.477092	136808.733397	35.521575
1214.733449	137060.716496	35.526592
1215.972245	137313.629947	35.531610
1217.014258	137570.115238	35.536628
1218.187179	137824.349350	35.541645
1219.951544	138075.837695	35.546663
1220.822876	138339.089640	35.551680
1222.113723	138585.246045	35.556698
1223.356384	138848.301100	35.561716
1224.720395	139105.049126	35.566733
1226.189403	139358.269500	35.571751
1227.290413	139611.565261	35.576768
1228.379026	139864.547955	35.581786
1229.383896	140119.879446	35.586804
1230.870322	140374.486564	35.591821
1232.232071	140636.939743	35.596839
1233.443598	140894.626669	35.601856
1234.429565	141141.156179	35.606874
1235.896911	141397.929636	35.611892
1237.059491	141659.561235	35.616909
1238.315746	141908.968013	35.621927
1239.695438	142168.437229	35.626944
1241.004763	142428.376506	35.631962
1242.704781	142681.976160	35.636980
1243.528339	142934.720728	35.641997
1245.013063	143183.376013	35.647015
1245.959961	143444.333784	35.652032
1247.022466	143691.642162	35.657050
1248.297436	143933.388141	35.662068
1249.521506	144185.695021	35.667085
1250.937537	144426.089503	35.672103
1251.713127	144666.058840	35.677120
1253.091662	144916.075378	35.682138
1254.440326	145159.808503	35.687156
1254.960119	145405.810816	35.692173
1256.589114	145656.437886	35.697191
1257.785832	145913.111330	35.702208
1258.958109	146160.570824	35.707226
1260.439464	146407.587780	35.712244
1261.486675	146678.558711	35.717261
1262.986093	146930.775936	35.722279
1263.992673	147187.921024	35.727296
1265.149675	147448.403908	35.732314
1266.595731	147720.407344	35.737332
1267.861659	147985.517852	35.742349
1269.075217	148243.650745	35.747367
1270.147590	148512.183320	35.752384
1271.146917	148779.677238	35.757402
1272.752667	149044.675769	35.762420
1273.820282	149325.200452	35.767437
1275.366114	149592.191351	35.772455
1276.658484	149877.845099	35.777472
1277.997493	150140.726667	35.782490
1279.507301	150419.956193	35.787508
1280.765557	150704.581828	35.792525
1282.229693	150963.973175	35.797543
1283.389662	151253.527761	35.802560
1284.473405	151520.748242	35.807578
1286.060820	151796.081168	35.812596
1287.421493	152080.497261	35.817613
1288.518048	152348.114629	35.822631
1290.041689	152616.678014	35.827648
1291.457854	152896.600791	35.832666
1293.666322	153154.970746	35.837684
1294.864556	153428.147264	35.842701
1296.340526	153690.954585	35.847719
1297.494671	153955.694202	35.852736
1298.605249	154227.330623	35.857754
1300.011493	154487.389580	35.862772
1301.113038	154750.570369	35.867789
1302.753205	155023.380596	35.872807
1304.024795	155290.291654	35.877824
1305.190694	155558.046521	35.882842
1306.705415	155830.109273	35.887860
1307.524703	156098.204156	35.892877
1308.507676	156359.563214	35.897895
1310.001136	156635.935353	35.902912
1311.455978	156920.992726	35.907930
1313.169467	157187.374130	35.912948
1314.136546	157467.974536	35.917965
1315.322523	157735.486986	35.922983
1316.317879	158009.946543	35.928000
1317.676980	158286.263431	35.933018
1319.417431	158567.504813	35.938036
1320.441367	158848.803125	35.943053
1322.039572	159130.972623	35.948071
1323.244132	159392.809456	35.953088
1324.501935	159681.737400	35.958106
1326.006849	159957.242240	35.963124
1327.216299	160239.280610	35.968141
1328.725785	160519.672791	35.973159
1330.055579	160798.231604	35.978176
1331.247638	161080.519611	35.983194
1332.842716	161343.585616	35.988212
1334.018788	161635.991517	35.993229
1335.208650	161914.669701	35.998247
1336.619475	162186.741238	36.003264
1337.682448	162461.561719	36.008282
1339.196501	162714.753596	36.013300
1340.219296	162978.482622	36.018317
1341.483213	163244.279561	36.023335
1343.046916	163512.908696	36.028352
1344.211361	163795.701516	36.033370
1345.472370	164053.383837	36.038388
1346.565834	164342.180602	36.043405
1347.574241	164619.396585	36.048423
1349.334188	164903.874561	36.053440
1350.367664	165191.113582	36.058458
1351.768632	165477.989244	36.063476
1352.926356	165775.057597	36.068493
1354.188484	166065.157491	36.073511
1355.773032	166368.275098	36.078528
1356.625099	166662.113643	36.083546
1357.940482	166951.499999	36.088564
1359.288567	167260.753318	36.093581
1360.946939	167565.541808	36.098599
1362.239853	167869.263461	36.103616
1363.374822	168173.419317	36.108634
1364.620925	168494.536788	36.113652
1365.835087	168806.322620	36.118669
1367.567314	169123.862017	36.123687
1368.708076	169437.110875	36.128704
1370.035309	169763.451891	36.133722
1371.580208	170072.222399	36.138740
1373.022941	170395.604859	36.143757
1374.642341	170721.993215	36.148775
1376.392029	171032.931612	36.153792
1377.623983	171347.498107	36.158810
1379.034475	171664.727476	36.163828
1380.574609	171996.581826	36.168845
1381.877916	172304.049236	36.173863
1383.636261	172623.587942	36.178880
1384.571419	172940.955210	36.183898
1386.220372	173262.838610	36.188916
1387.445423	173583.296761	36.193933
1388.675181	173898.971954	36.198951
1390.453779	174222.718570	36.203968
1391.795724	174545.016634	36.208986
1393.191373	174872.054309	36.214004
1394.304231	175189.813141	36.219021
1395.736882	175515.288040	36.224039
1397.433347	175827.319794	36.229056
1398.631132	176170.516422	36.234074
1400.101949	176491.448051	36.239092
1401.627315	176831.968052	36.244109
1402.739233	177157.367153	36.249127
1404.154104	177483.225964	36.254144
1405.625419	177808.519133	36.259162
1407.163908	178137.407712	36.264180
1408.765304	178473.306529	36.269197
1409.792010	178803.540470	36.274215
1411.497347	179134.667057	36.279232
1412.998733	179457.084749	36.284250
1414.443245	179783.334150	36.289268
1416.247544	180114.983751	36.294285
1417.405861	180443.226486	36.299303
1419.472323	180765.952400	36.304320
1420.572995	181088.598741	36.309338
1421.884690	181405.322918	36.314356
1423.220630	181726.335043	36.319373
1424.546378	182053.481296	36.324391
1425.726451	182386.860326	36.329408
1427.158490	182718.867063	36.334426
1428.783916	183032.858218	36.339444
1430.029446	183359.378362	36.344461
1431.324737	183679.507703	36.349479
1432.980454	183990.211930	36.354496
1434.427346	184309.596418	36.359514
1435.536840	184616.573839	36.364532
1436.939678	184915.025426	36.369549
1438.687280	185237.069254	36.374567
1439.943789	185561.125488	36.379584
1441.060443	185889.446322	36.384602
1442.535446	186223.015753	36.389620
1444.010795	186549.250205	36.394637
1445.346318	186871.625382	36.399655
1447.138947	187206.760222	36.404672
1448.427769	187538.908373	36.409690
1449.697800	187863.280202	36.414708
1451.393539	188201.965762	36.419725
1452.257366	188533.428228	36.424743
1454.081653	188861.623822	36.429760
1455.233938	189213.619626	36.434778
1456.720135	189549.237556	36.439796
1458.015608	189890.867932	36.444813
1459.489693	190251.677382	36.449831
1461.174715	190588.690107	36.454848
1462.647726	190948.323350	36.459866
1464.020761	191296.410458	36.464884
1465.405136	191649.169337	36.469901
1466.533565	192001.756738	36.474919
1468.083093	192362.439369	36.479936
1469.292366	192727.560079	36.484954
1471.226438	193094.708634	36.489972
1472.906220	193464.326128	36.494989
1474.229117	193833.204978	36.500007
1475.849388	194190.382647	36.505024
1477.334480	194552.865903	36.510042
1478.916489	194916.033453	36.515060
1480.352852	195278.808177	36.520077
1481.611544	195645.791119	36.525095
1483.371002	196005.913962	36.530112
1484.751281	196382.554997	36.535130
1486.103676	196745.326386	36.540148
1487.796308	197125.106686	36.545165
1489.609869	197490.764083	36.550183
1491.276193	197866.071320	36.555200
1492.470169	198232.292190	36.560218
1493.781692	198604.665908	36.565236
1495.469124	198971.837620	36.570253
1496.842459	199344.471781	36.575271
1498.684690	199718.871443	36.580288
1499.905217	200095.762760	36.585306
1501.202453	200471.475369	36.590324
1502.864955	200838.953108	36.595341
1504.329807	201230.906256	36.600359
1506.169928	201605.075091	36.605376
1507.461369	201975.260903	36.610394
1509.292125	202350.831804	36.615412
1510.594138	202726.745945	36.620429
1511.803046	203110.130467	36.625447
1514.113671	203471.762863	36.630464
1515.112703	203862.143887	36.635482
1516.609581	204230.110560	36.640500
1518.178962	204602.726903	36.645517
1519.628900	204990.741114	36.650535
1521.135533	205369.224994	36.655552
1522.692150	205754.482850	36.660570
1524.122239	206140.525375	36.665588
1525.582970	206512.648356	36.670605
1526.975165	206898.167594	36.675623
1528.734059	207273.939886	36.680640
1530.155183	207667.571831	36.685658
1531.638775	208035.647641	36.690676
1533.128521	208397.260963	36.695693
1534.372167	208769.925543	36.700711
1536.182427	209129.724162	36.705728
1537.340216	209513.745482	36.710746
1538.951483	209876.284875	36.715764
1540.517032	210257.372505	36.720781
1541.790917	210637.189442	36.725799
1543.303741	211000.435621	36.730816
1544.975260	211392.583602	36.735834
1546.275583	211784.769290	36.740852
1547.925900	212170.676747	36.745869
1549.363109	212558.475067	36.750887
1551.136088	212944.721195	36.755904
1552.526860	213340.429007	36.760922
1554.128086	213733.843447	36.765940
1555.522345	214122.163552	36.770957
1557.131420	214533.231166	36.775975
1558.801448	214917.496290	36.780992
1559.970533	215331.002075	36.786010
1561.543414	215735.249026	36.791028
1563.122105	216149.351044	36.796045
1564.283587	216562.025300	36.801063
1566.074018	216976.705428	36.806080
1567.859983	217397.381984	36.811098
1569.440835	217825.485071	36.816116
1571.285273	218231.551556	36.821133
1572.520529	218657.175450	36.826151
1574.311225	219075.039018	36.831168
1575.482678	219501.591292	36.836186
1577.193208	219926.176747	36.841204
1578.689461	220354.507529	36.846221
1580.732126	220782.521168	36.851239
1582.821293	221205.245837	36.856256
1584.370744	221628.620084	36.861274
1585.811691	222048.737388	36.866292
1587.598162	222455.159789	36.871309
1588.881044	222892.044465	36.876327
1590.809973	223309.850695	36.881344
1592.495984	223728.739946	36.886362
1593.934753	224161.488935	36.891380
1595.486304	224587.997939	36.896397
1597.065135	225089.103206	36.901415
1598.528488	225504.200091	36.906432
1600.421027	225943.586065	36.911450
1602.171826	226367.121945	36.916468
1603.992570	226786.456658	36.921485
1605.754996	227219.772512	36.926503
1606.814255	227647.440095	36.931520
1608.644702	228071.044599	36.936538
1610.288482	228501.717218	36.941556
1611.846827	228924.683542	36.946573
1613.683139	229365.080896	36.951591
1615.258370	229781.519075	36.956608
1617.214680	230209.300486	36.961626
1618.632274	230636.410137	36.966644
1620.238699	231047.512641	36.971661
1622.154122	231486.836580	36.976679
1623.494959	231913.175153	36.981696
1624.744671	232326.499167	36.986714
1626.560118	232755.225576	36.991732
1628.529476	233191.014686	36.996749
1630.119912	233624.530646	37.001767
1631.842244	234048.348019	37.006784
1633.156129	234465.781961	37.011802
1634.723389	234902.073841	37.016820
1636.427703	235327.116664	37.021837
1638.059877	235754.992020	37.026855
1639.310403	236162.356029	37.031872
1641.271506	236577.198708	37.036890
1643.195224	236992.023088	37.041908
1644.247912	237384.282953	37.046925
1645.806102	237807.247294	37.051943
1647.528632	238218.043232	37.056960
1649.147540	238641.304143	37.061978
1650.633722	239058.567551	37.066996
1652.267191	239483.605928	37.072013
1653.691633	239921.685618	37.077031
1655.299818	240345.027915	37.082048
1657.195246	240777.951044	37.087066
1658.788185	241211.839442	37.092084
1660.568910	241633.631475	37.097101
1662.255889	242066.820033	37.102119
1663.622352	242509.943868	37.107136
1665.441267	242942.096044	37.112154
1667.286514	243394.896892	37.117172
1668.995419	243821.530911	37.122189
1670.421012	244262.768115	37.127207
1671.790686	244714.430349	37.132224
1673.465220	245163.832879	37.137242
1675.258619	245625.308164	37.142260
1677.074119	246066.788454	37.147277
1678.615589	246530.262672	37.152295
1680.268569	246981.220882	37.157312
1682.189007	247439.578548	37.162330
1683.539983	247907.328331	37.167348
1685.592434	248368.612071	37.172365
1686.976329	248836.713169	37.177383
1688.748448	249299.695459	37.182400
1690.328971	249760.271189	37.187418
1691.854414	250241.280559	37.192436
1693.904989	250700.915853	37.197453
1695.783673	251191.622579	37.202471
1697.087308	251659.993737	37.207488
1699.345735	252131.535373	37.212506
1700.878282	252605.102499	37.217524
1702.949916	253077.234539	37.222541
1704.778569	253545.342497	37.227559
1706.227135	254029.339726	37.232576
1708.275954	254492.254982	37.237594
1709.998778	254963.048503	37.242612
1711.754035	255430.890085	37.247629
1713.282000	255906.949235	37.252647
1715.198985	256378.498702	37.257664
1717.002490	256845.977102	37.262682
1718.597760	257318.062584	37.267700
1720.799250	257788.625420	37.272717
1722.445490	258259.534044	37.277735
1724.034216	258730.579201	37.282752
1725.933710	259190.649600	37.287770
1727.391019	259667.762408	37.292788
1728.927704	260140.899131	37.297805
1730.696143	260614.530959	37.302823
1732.341934	261091.485361	37.307840
1734.320352	261566.454034	37.312858
1735.631253	262049.865067	37.317876
1737.620845	262525.237988	37.322893
1739.659889	263007.918658	37.327911
1741.223064	263484.682510	37.332928
1743.228983	263960.636271	37.337946
1744.781443	264446.267038	37.342964
1746.143408	264916.864843	37.347981
1747.719457	265396.216440	37.352999
1749.495884	265883.968401	37.358016
1751.507634	266372.646388	37.363034
1753.088137	266850.624235	37.368052
1754.700984	267314.472172	37.373069
1756.222403	267778.639586	37.378087
1757.825221	268253.894189	37.383104
1759.842955	268718.004027	37.388122
1761.480000	269187.231394	37.393140
1762.878873	269655.379797	37.398157
1764.574145	270136.154696	37.403175
1765.876715	270619.635696	37.408192
1767.989622	271097.596776	37.413210
1769.460623	271588.110534	37.418228
1771.230318	272088.481262	37.423245
1773.101825	272591.374617	37.428263
1774.307659	273093.640369	37.433280
1776.399584	273587.274411	37.438298
1778.296623	274101.896854	37.443316
1780.070134	274606.377690	37.448333
1781.669804	275125.467248	37.453351
1783.190714	275634.966615	37.458368
1785.151939	276156.966340	37.463386
1786.666633	276683.865073	37.468404
1788.288211	277210.363890	37.473421
1790.413544	277737.845138	37.478439
1791.988550	278277.456564	37.483456
1794.072330	278807.685417	37.488474
1795.854562	279349.545976	37.493492
1797.498776	279886.753887	37.498509
1799.553827	280420.082170	37.503527
1801.383824	280964.800682	37.508544
1803.192708	281495.448529	37.513562
1804.942588	282050.693284	37.518580
1806.872827	282583.984977	37.523597
1808.945233	283129.825230	37.528615
1810.524541	283696.193209	37.533632
1812.528992	284224.666533	37.538650
1814.160571	284776.467157	37.543668
1815.994787	285327.800546	37.548685
1817.872593	285874.730375	37.553703
1819.946555	286430.846335	37.558720
1822.052669	286981.341301	37.563738
1823.778386	287544.165519	37.568756
1825.529748	288080.058621	37.573773
1827.360410	288633.716904	37.578791
1829.421083	289189.519380	37.583808
1831.393521	289740.127055	37.588826
1833.513086	290301.147592	37.593844
1835.166596	290854.749632	37.598861
1836.780849	291402.488343	37.603879
1838.606187	291964.413697	37.608896
1840.597700	292511.805785	37.613914
1842.442514	293073.163995	37.618932
1844.224202	293627.341913	37.623949
1846.218433	294180.135931	37.628967
1848.033104	294742.100665	37.633984
1850.005434	295297.128008	37.639002
1851.857952	295839.599869	37.644020
1853.715807	296405.104930	37.649037
1855.745589	296950.005670	37.654055
1857.331477	297509.352529	37.659072
1859.548173	298062.953779	37.664090
1861.206676	298617.888761	37.669108
1863.067762	299181.524246	37.674125
1865.378998	299730.503762	37.679143
1867.148487	300292.598825	37.684160
1868.968293	300832.916477	37.689178
1871.389993	301381.462132	37.694196
1872.950963	301930.603923	37.699213
1875.021121	302476.458368	37.704231
1877.094016	303011.642348	37.709248
1879.267562	303528.266764	37.714266
1881.040256	304044.141736	37.719284
1883.063071	304557.331181	37.724301
1885.001280	305065.706280	37.729319
1886.447422	305578.172330	37.734336
1888.241884	306102.056961	37.739354
1889.940652	306610.335579	37.744372
1891.808630	307136.487381	37.749389
1893.695169	307653.185582	37.754407
1894.989709	308193.977226	37.759424
1896.878854	308712.522265	37.764442
1898.942245	309261.128690	37.769460
1900.832315	309804.807945	37.774477
1902.879727	310334.490273	37.779495
1904.175564	310886.488208	37.784512
1906.047744	311432.470124	37.789530
1908.059286	311989.928850	37.794548
1909.770507	312552.842076	37.799565
1911.643636	313107.547491	37.804583
1913.351436	313678.096478	37.809600
1915.265406	314244.797977	37.814618
1917.454080	314811.983000	37.819636
1918.632718	315388.065658	37.824653
1920.706774	315968.414239	37.829671
1922.719997	316554.760845	37.834688
1924.619087	317144.016175	37.839706
1926.574272	317741.281268	37.844724
1928.314192	318328.318284	37.849741
1930.551776	318916.461506	37.854759
1932.066557	319532.903817	37.859776
1934.262242	320129.574985	37.864794
1936.579502	320733.914273	37.869812
1938.144589	321342.409374	37.874829
1940.127555	321943.872699	37.879847
1942.059475	322549.680625	37.884864
1943.798307	323158.333009	37.889882
1946.202725	323772.201554	37.894900
1948.221133	324382.268557	37.899917
1950.290867	324989.680567	37.904935
1952.056011	325616.356595	37.909952
1953.826251	326225.024476	37.914970
1955.963663	326840.150518	37.919988
1957.566559	327476.481762	37.925005
1959.559104	328084.941667	37.930023
1961.456263	328719.459121	37.935040
1963.475576	329353.568670	37.940058
1965.498313	329969.670973	37.945076
1967.669514	330611.789367	37.950093
1969.962571	331231.463739	37.955111
1971.719010	331867.594237	37.960128
1973.747918	332495.802721	37.965146
1975.534409	333114.600477	37.970164
1977.338242	333768.725320	37.975181
1979.863112	334391.194528	37.980199
1981.985417	335022.557028	37.985216
1984.003995	335651.974551	37.990234
1985.951432	336283.325561	37.995252
1987.521972	336920.417271	38.000269
1989.571321	337551.761522	38.005287
1991.812402	338183.751757	38.010304
1994.042325	338823.021042	38.015322
1996.151423	339453.240515	38.020340
1998.307217	340080.626929	38.025357
2000.095080	340697.710230	38.030375
2002.223590	341337.725730	38.035392
2004.302577	341958.247960	38.040410
2006.508198	342584.909082	38.045428
2008.513363	343204.082422	38.050445
2010.774914	343799.855217	38.055463
2012.689693	344386.033289	38.060480
2014.820877	344982.599622	38.065498
2016.662182	345566.719422	38.070516
2018.245031	346166.305323	38.075533
2020.475324	346763.847797	38.080551
2022.382253	347369.481012	38.085568
2024.481939	347978.094452	38.090586
2026.740635	348571.421268	38.095604
2028.077064	349181.362756	38.100621
2030.603989	349782.674124	38.105639
2032.531572	350395.902075	38.110656
2033.941830	351011.922274	38.115674
2036.538648	351623.652379	38.120692
2038.201652	352249.967064	38.125709
2040.301894	352854.732742	38.130727
2042.246027	353489.357088	38.135744
2044.219355	354120.313247	38.140762
2046.390730	354752.496106	38.145780
2048.349880	355391.225729	38.150797
2050.293256	356018.707681	38.155815
2052.343219	356667.577766	38.160832
2054.530958	357310.528437	38.165850
2056.817834	357949.925935	38.170868
2058.549460	358599.097307	38.175885
2060.564941	359246.486192	38.180903
2062.507439	359895.196083	38.185920
2064.435950	360549.885368	38.190938
2066.879008	361206.889184	38.195956
2068.628099	361883.658533	38.200973
2071.164194	362543.440877	38.205991
2073.078128	363201.361385	38.211008
2074.751909	363875.546472	38.216026
2077.301349	364543.867369	38.221044
2079.498957	365216.826323	38.226061
2081.438288	365877.715762	38.231079
2083.604730	366555.856532	38.236096
2085.601335	367235.027809	38.241114
2087.630143	367899.849601	38.246132
2089.861074	368591.057191	38.251149
2091.942903	369263.658437	38.256167
2094.361742	369951.993978	38.261184
2095.944880	370628.381133	38.266202
2098.558449	371303.190592	38.271220
2100.539899	371995.262743	38.276237
2102.105917	372681.886402	38.281255
2104.597328	373369.485395	38.286272
2106.641667	374059.604953	38.291290
2108.802726	374751.390942	38.296308
2110.853624	375438.540428	38.301325
2113.302333	376127.614155	38.306343
2115.502268	376838.194991	38.311360
2117.223288	377526.397247	38.316378
2119.813992	378213.148805	38.321396
2121.274031	378921.576942	38.326413
2123.546776	379612.663550	38.331431
2125.796768	380309.774722	38.336448
2127.488935	381017.283603	38.341466
2129.651346	381711.514612	38.346484
2132.169746	382433.157735	38.351501
2134.055088	383145.736337	38.356519
2136.632783	383852.378932	38.361536
2138.280696	384561.340064	38.366554
2140.835693	385265.344116	38.371572
2143.225519	385973.974206	38.376589
2145.248905	386682.649055	38.381607
2147.631173	387369.978782	38.386624
2149.655882	388074.413882	38.391642
2151.920686	388735.798974	38.396660
2153.606531	389427.102633	38.401677
2155.710092	390092.668295	38.406695
2157.937005	390768.972568	38.411712
2159.815087	391461.719943	38.416730
2162.006249	392134.704722	38.421748
2163.894604	392821.107944	38.426765
2165.681027	393513.519592	38.431783
2167.921675	394201.024601	38.436800
2169.836543	394916.143489	38.441818
2172.280500	395620.234261	38.446836
2174.293239	396329.270936	38.451853
2175.976020	397034.492801	38.456871
2178.297474	397763.034609	38.461888
2179.833152	398482.057830	38.466906
2182.224676	399215.468161	38.471924
2184.478800	399956.839660	38.476941
2186.427329	400699.230753	38.481959
2188.471779	401446.857412	38.486976
2190.310152	402196.677595	38.491994
2192.941282	402953.315127	38.497012
2195.127531	403715.808082	38.502029
2197.281141	404479.248460	38.507047
2199.244778	405247.943884	38.512064
2201.080186	406025.937317	38.517082
2203.435632	406806.533782	38.522100
2205.725711	407596.061763	38.527117
2207.753543	408383.735479	38.532135
2210.132008	409175.381669	38.537152
2212.169512	409975.420437	38.542170
2214.695246	410773.961542	38.547188
2216.860094	411570.993146	38.552205
2219.039028	412361.691395	38.557223
2221.330098	413171.242822	38.562240
2223.405968	413989.644319	38.567258
2226.064716	414804.783383	38.572276
2228.284447	415612.143426	38.577293
2230.127080	416418.172896	38.582311
2232.243451	417236.617114	38.587328
2234.903132	418059.351868	38.592346
2237.131394	418883.448026	38.597364
2239.137232	419704.591331	38.602381
2241.562013	420533.893568	38.607399
2243.943831	421359.174749	38.612416
2245.895859	422186.449166	38.617434
2248.548374	423018.213767	38.622452
2250.958683	423848.218008	38.627469
2253.067490	424678.345200	38.632487
2255.696072	425501.573552	38.637504
2258.080794	426324.561089	38.642522
2260.236201	427149.178594	38.647540
2262.142331	427987.630373	38.652557
2264.390998	428826.097497	38.657575
2267.245394	429654.006519	38.662592
2269.322641	430483.634781	38.667610
2271.326358	431325.698685	38.672628
2273.894719	432164.753902	38.677645
2276.148836	433007.576480	38.682663
2278.852394	433829.491432	38.687680
2280.825300	434664.556012	38.692698
2282.883557	435503.422680	38.697716
2285.451866	436330.787244	38.702733
2287.867595	437170.394058	38.707751
2290.296091	438004.552832	38.712768
2292.441259	438849.506216	38.717786
2294.798095	439672.633916	38.722804
2297.205591	440508.980253	38.727821
2299.115856	441324.682427	38.732839
2301.987050	442136.553028	38.737856
2303.932249	442949.406658	38.742874
2306.231077	443742.541772	38.747892
2308.235826	444549.204462	38.752909
2310.532837	445350.628919	38.757927
2313.559518	446156.456176	38.762944
2315.731583	446963.456646	38.767962
2318.281465	447759.741896	38.772980
2320.469986	448564.656007	38.777997
2322.256409	449368.897927	38.783015
2324.741643	450174.460779	38.788032
2326.879664	450992.744726	38.793050
2329.567368	451809.490037	38.798068
2331.328892	452636.622399	38.803085
2333.948140	453464.389506	38.808103
2336.387879	454289.169698	38.813120
2338.791444	455124.592312	38.818138
2341.246294	455949.505825	38.823156
2343.253576	456779.971190	38.828173
2345.735769	457621.902525	38.833191
2348.346234	458453.312363	38.838208
2350.311858	459299.758828	38.843226
2352.584005	460144.956394	38.848244
2354.822595	460986.787476	38.853261
2357.080931	461842.278577	38.858279
2359.734868	462696.504990	38.863296
2361.741920	463574.456145	38.868314
2363.928653	464430.807481	38.873332
2366.510038	465306.362647	38.878349
2368.614612	466183.220683	38.883367
2371.464547	467064.413855	38.888384
2373.817900	467943.122192	38.893402
2376.068294	468828.730206	38.898420
2378.183052	469705.376177	38.903437
2380.766479	470599.235123	38.908455
2383.504104	471499.645264	38.913472
2385.679915	472390.607280	38.918490
2388.122946	473288.858917	38.923508
2390.528012	474185.810951	38.928525
2392.693301	475076.243202	38.933543
2395.262155	475978.234528	38.938560
2397.739966	476882.166873	38.943578
2399.959552	477793.926143	38.948596
2402.414043	478695.147051	38.953613
2404.436386	479613.161523	38.958631
2407.286448	480518.923876	38.963648
2409.577304	481439.478364	38.968666
2412.283579	482360.018427	38.973684
2414.608215	483269.668206	38.978701
2416.984931	484195.470215	38.983719
2419.237188	485118.468001	38.988736
2421.580219	486040.746604	38.993754
2424.150789	486961.273742	38.998772
2426.887229	487878.343388	39.003789
2429.069023	488816.454588	39.008807
2431.520140	489731.758119	39.013824
2434.093634	490670.663990	39.018842
2436.160245	491598.499760	39.023860
2438.570884	492531.325887	39.028877
2441.205761	493468.252786	39.033895
2443.702264	494396.573147	39.038912
2446.088510	495332.429688	39.043930
2449.003874	496271.780057	39.048948
2451.287406	497196.047169	39.053965
2453.698745	498139.917364	39.058983
2456.270623	499052.835318	39.064000
2459.175329	499990.718566	39.069018
2461.282644	500904.973764	39.074036
2464.035852	501803.688651	39.079053
2466.020806	502702.733568	39.084071
2468.789393	503593.682308	39.089088
2471.179420	504491.200856	39.094106
2473.364786	505390.317493	39.099124
2475.633858	506280.849084	39.104141
2478.198943	507186.610800	39.109159
2480.852636	508091.601250	39.114176
2483.017460	508994.907342	39.119194
2485.313866	509912.457863	39.124212
2488.051784	510814.407202	39.129229
2490.051571	511747.931126	39.134247
2493.113387	512678.855905	39.139264
2495.532802	513606.555751	39.144282
2497.533494	514532.909236	39.149300
2500.078322	515469.398647	39.154317
2502.052496	516416.457805	39.159335
2505.003324	517355.840718	39.164352
2507.381663	518310.023961	39.169370
2509.731562	519263.649090	39.174388
2512.454417	520222.745600	39.179405
2514.741956	521185.178663	39.184423
2517.372556	522145.278039	39.189440
2520.183025	523118.433486	39.194458
2522.700836	524089.761491	39.199476
2525.197102	525061.584498	39.204493
2527.552173	526049.029760	39.209511
2530.423400	527015.175142	39.214528
2532.953347	527998.232815	39.219546
2535.540967	528986.301234	39.224564
2538.495748	529964.274572	39.229581
2541.334629	530950.810786	39.234599
2543.581276	531931.488722	39.239616
2546.433697	532914.366811	39.244634
2548.457323	533900.737980	39.249652
2551.432531	534882.556882	39.254669
2554.227036	535877.977273	39.259687
2556.720811	536872.523062	39.264704
2559.388206	537854.995458	39.269722
2562.113385	538850.271610	39.274740
2564.634531	539845.059132	39.279757
2567.219631	540833.578512	39.284775
2569.944941	541824.219129	39.289792
2572.641712	542819.472873	39.294810
2574.821661	543816.401189	39.299828
2577.955156	544805.406213	39.304845
2580.294941	545800.557180	39.309863
2582.816259	546802.295104	39.314880
2585.771784	547796.849267	39.319898
2588.076963	548796.869207	39.324916
2590.821435	549789.303090	39.329933
2593.647360	550803.419539	39.334951
2596.172852	551791.471053	39.339968
2598.968405	552789.408957	39.344986
2601.132368	553797.681095	39.350004
2603.997049	554798.475031	39.355021
2606.398992	555800.024649	39.360039
2609.066491	556807.937887	39.365056
2611.777433	557813.959047	39.370074
2614.252265	558806.578649	39.375092
2617.042376	559809.973747	39.380109
2619.507448	560816.410609	39.385127
2622.302987	561831.205088	39.390144
2624.660528	562834.139775	39.395162
2627.159614	563853.447412	39.400180
2630.009445	564864.030000	39.405197
2632.892236	565878.897248	39.410215
2635.331808	566876.485308	39.415232
2637.870944	567855.051545	39.420250
2640.052837	568827.678175	39.425268
2642.649424	569802.973781	39.430285
2645.041794	570784.051339	39.435303
2647.705338	571773.290271	39.440320
2650.420036	572757.073476	39.445338
2652.701765	573754.150407	39.450356
2655.421310	574751.176602	39.455373
2657.947983	575750.714454	39.460391
2660.394295	576754.901952	39.465408
2663.146717	577768.339605	39.470426
2665.414623	578784.784421	39.475444
2668.184461	579804.423808	39.480461
2670.428051	580841.971445	39.485479
2673.232730	581873.671960	39.490496
2675.837914	582917.404113	39.495514
2678.309528	583977.014661	39.500532
2681.324672	585008.967424	39.505549
2683.792424	586076.869097	39.510567
2686.246573	587143.575913	39.515584
2688.756805	588206.118961	39.520602
2691.413738	589293.053015	39.525620
2693.965568	590369.581773	39.530637
2696.850816	591454.627781	39.535655
2699.586578	592556.635892	39.540672
2702.582728	593639.058785	39.545690
2705.130139	594735.934783	39.550708
2708.229796	595825.003292	39.555725
2710.738241	596937.159006	39.560743
2713.569145	598040.441130	39.565760
2716.251760	599143.442876	39.570778
2719.125550	600254.420300	39.575796
2722.161054	601369.219817	39.580813
2724.343416	602485.203688	39.585831
2726.855686	603597.270256	39.590848
2730.190017	604723.859375	39.595866
2732.642924	605859.891936	39.600884
2735.480455	606976.930679	39.605901
2738.005739	608120.231724	39.610919
2740.615632	609257.699060	39.615936
2743.620734	610386.931418	39.620954
2746.799369	611537.481956	39.625972
2749.516938	612675.084998	39.630989
2752.111095	613819.744190	39.636007
2754.771804	614951.721996	39.641024
2757.714008	616105.089220	39.646042
2760.515283	617257.508958	39.651060
2763.743784	618398.688708	39.656077
2766.384795	619542.245748	39.661095
2769.023765	620692.230982	39.666112
2771.752524	621838.781187	39.671130
2774.283308	622995.037259	39.676148
2777.043231	624148.083693	39.681165
2779.842030	625307.045478	39.686183
2782.506347	626474.396703	39.691200
2785.646938	627621.161900	39.696218
2788.535360	628789.821141	39.701236
2791.183567	629952.997773	39.706253
2794.094028	631130.484182	39.711271
2796.708238	632287.117510	39.716288
2799.880511	633449.372476	39.721306
2802.368545	634619.398387	39.726324
2805.035306	635783.972938	39.731341
2807.747530	636953.899281	39.736359
2810.833170	638134.759861	39.741376
2813.602882	639303.612581	39.746394
2815.948819	640494.353813	39.751412
2818.683805	641643.638896	39.756429
2821.512176	642795.772096	39.761447
2823.901927	643945.852484	39.766464
2826.917522	645082.883692	39.771482
2829.746184	646242.006310	39.776500
2832.035130	647376.805167	39.781517
2834.988022	648525.573796	39.786535
2837.356894	649697.484658	39.791552
2840.511531	650869.876152	39.796570
2843.050159	652036.450709	39.801588
2845.850723	653202.695576	39.806605
2848.616829	654403.234731	39.811623
2851.119558	655588.278585	39.816640
2853.852134	656781.708807	39.821658
2856.452237	657983.631380	39.826676
2859.263111	659203.546932	39.831693
2862.110264	660427.187280	39.836711
2864.569734	661658.254586	39.841728
2867.164853	662896.659206	39.846746
2869.851507	664138.323833	39.851764
2872.672461	665398.965073	39.856781
2875.530041	666661.026548	39.861799
2878.348106	667935.017109	39.866816
2881.028538	669213.933615	39.871834
2883.694880	670504.716343	39.876852
2886.429505	671797.648758	39.881869
2889.419930	673095.781290	39.886887
2892.261842	674416.131214	39.891904
2895.023905	675726.564690	39.896922
2897.844117	677065.880299	39.901940
2901.079883	678391.764846	39.906957
2903.884692	679720.710429	39.911975
2906.618172	681063.834019	39.916992
2909.609891	682402.347335	39.922010
2912.329280	683756.801759	39.927028
2915.203449	685111.774416	39.932045
2918.458679	686473.830683	39.937063
2921.227008	687835.960941	39.942080
2924.340052	689196.290040	39.947098
2926.835335	690572.098749	39.952116
2929.844093	691954.757073	39.957133
2932.873075	693327.027148	39.962151
2935.702021	694717.522404	39.967168
2938.903792	696104.762237	39.972186
2941.578372	697497.970777	39.977204
2944.728913	698885.128807	39.982221
2948.306075	700281.763364	39.987239
2951.158783	701667.686914	39.992256
2954.548870	703062.717561	39.997274
2957.299013	704450.642832	40.002292
2960.014169	705847.021205	40.007309
2963.671028	707239.550697	40.012327
2966.500333	708633.575711	40.017344
2969.688677	710029.592389	40.022362
2972.893751	711414.683546	40.027380
2975.386744	712801.300005	40.032397
2978.561258	714196.387201	40.037415
2981.394621	715591.646515	40.042432
2984.546643	716986.621933	40.047450
2987.416458	718371.221015	40.052468
2990.412330	719781.141535	40.057485
2993.629867	721170.461564	40.062503
2996.522682	722589.269452	40.067520
2999.997745	723969.919153	40.072538
3002.829639	725376.492232	40.077556
3005.671905	726774.767389	40.082573
3008.842329	728162.669770	40.087591
3011.694171	729562.097053	40.092608
3014.639613	730922.493543	40.097626
3017.770523	732295.570305	40.102644
3020.529519	733650.304006	40.107661
3023.473542	734988.981063	40.112679
3026.441513	736345.102257	40.117696
3029.561819	737694.750029	40.122714
3032.467822	739053.678870	40.127732
3034.996284	740422.058178	40.132749
3038.141244	741785.068184	40.137767
3040.770968	743165.633389	40.142784
3043.872482	744541.243594	40.147802
3046.816275	745930.886789	40.152820
3049.293504	747319.374162	40.157837
3052.663646	748721.069437	40.162855
3055.326416	750133.173291	40.167872
3058.410212	751550.517353	40.172890
3061.432967	752965.887267	40.177908
3064.333361	754408.152435	40.182925
3067.141472	755840.510876	40.187943
3070.157120	757295.113582	40.192960
3073.301195	758748.334538	40.197978
3076.298987	760200.169614	40.202996
3079.268782	761673.575807	40.208013
3082.466234	763138.294159	40.213031
3085.617362	764624.571182	40.218048
3088.968753	766098.178250	40.223066
3092.043606	767586.829309	40.228084
3094.810736	769075.331546	40.233101
3098.037916	770556.775860	40.238119
3101.065106	772059.819927	40.243136
3104.104265	773562.407925	40.248154
3107.585230	775060.932119	40.253172
3110.487846	776588.263780	40.258189
3113.499325	778100.333751	40.263207
3116.657516	779627.918078	40.268224
3120.125153	781142.321649	40.273242
3123.584448	782665.288706	40.278260
3126.474601	784194.894043	40.283277
3129.825791	785712.523629	40.288295
3133.030506	787248.338880	40.293312
3136.176705	788773.440517	40.298330
3139.552871	790303.077209	40.303348
3142.849603	791833.865991	40.308365
3146.053265	793361.741285	40.313383
3149.049983	794902.150008	40.318400
3152.406273	796423.113020	40.323418
3155.715568	797974.446608	40.328436
3158.517030	799507.310770	40.333453
3161.749545	801050.676806	40.338471
3165.198561	802593.026263	40.343488
3168.302132	804152.499211	40.348506
3171.607102	805694.811912	40.353524
3174.754283	807256.455835	40.358541
3177.737224	808790.593159	40.363559
3180.811336	810348.704277	40.368576
3183.964082	811900.678883	40.373594
3187.379422	813454.060370	40.378612
3190.445682	815008.849604	40.383629
3193.505542	816565.329631	40.388647
3196.655838	818130.657023	40.393664
3199.989025	819693.585448	40.398682
3203.191029	821250.459251	40.403700
3205.905314	822833.287791	40.408717
3209.082028	824400.104526	40.413735
3212.325225	825970.436671	40.418752
3215.557522	827542.782171	40.423770
3218.871392	829132.228671	40.428788
3221.820395	830712.724049	40.433805
3225.371296	832269.015836	40.438823
3228.344663	833812.854668	40.443840
3231.524662	835348.305605	40.448858
3234.667295	836882.908674	40.453876
3237.348170	838421.550276	40.458893
3240.831246	839962.218065	40.463911
3243.695277	841511.903552	40.468928
3246.686492	843059.049709	40.473946
3249.870384	844622.895922	40.478964
3252.820839	846193.973418	40.483981
3256.252926	847775.169901	40.488999
3259.321784	849349.031904	40.494016
3262.342177	850933.965001	40.499034
3265.632297	852541.267251	40.504052
3268.783801	854146.524989	40.509069
3271.692076	855755.578371	40.514087
3275.243085	857375.844596	40.519104
3278.245410	859006.054590	40.524122
3281.194290	860637.293120	40.529140
3284.597533	862293.419027	40.534157
3287.788100	863929.163399	40.539175
3291.150252	865596.411035	40.544192
3294.098290	867266.559291	40.549210
3298.024673	868932.111946	40.554228
3301.225355	870605.840184	40.559245
3304.729496	872278.952354	40.564263
3307.941190	873961.027352	40.569280
3311.069698	875646.217761	40.574298
3314.901883	877343.672622	40.579316
3318.269892	879048.835008	40.584333
3321.602053	880735.532263	40.589351
3324.829212	882430.069323	40.594368
3327.876575	884132.449893	40.599386
3331.883852	885834.076889	40.604404
3334.985651	887551.956061	40.609421
3338.789949	889266.795505	40.614439
3342.012035	890980.833551	40.619456
3345.412832	892689.314435	40.624474
3348.916915	894408.836958	40.629492
3352.276826	896123.237258	40.634509
3355.939843	897843.910760	40.639527
3359.557745	899554.627932	40.644544
3362.699862	901279.348670	40.649562
3366.318731	902980.453094	40.654580
3369.712701	904705.907026	40.659597
3373.488558	906418.641953	40.664615
3376.763920	908138.145013	40.669632
3380.175719	909853.342094	40.674650
3383.625741	911559.637684	40.679668
3387.046959	913292.794408	40.684685
3390.289912	915007.277696	40.689703
3393.953638	916724.130814	40.694720
3397.181960	918452.610397	40.699738
3401.016190	920166.524603	40.704756
3404.435378	921887.255583	40.709773
3407.859846	923595.256567	40.714791
3411.370206	925307.494551	40.719808
3414.571267	927029.491795	40.724826
3417.743666	928745.860347	40.729844
3421.233855	930469.573138	40.734861
3424.769893	932186.207131	40.739879
3428.328660	933903.428703	40.744896
3431.352641	935636.733193	40.749914
3434.842431	937352.553139	40.754932
3438.217036	939084.373184	40.759949
3441.605223	940805.865518	40.764967
3445.152793	942536.604820	40.769984
3448.566046	944263.444779	40.775002
3451.799399	945965.689848	40.780007
3455.218863	947637.027752	40.785012
3458.560978	949242.100352	40.790016
3461.767337	950792.934590	40.795021
3464.706390	952272.865403	40.800026
3468.006539	953713.217221	40.805031
3470.733470	955086.423150	40.810036
3474.050508	956381.844649	40.815040
3476.841862	957600.795920	40.820045
3479.274649	958758.293167	40.825050
3482.306195	959827.856048	40.830055
3484.803151	960837.642633	40.835060
3486.924442	961755.625890	40.840064
3489.461118	962620.407126	40.845069
3491.246743	963421.625980	40.850074
3493.655200	964135.386655	40.855079
3495.858841	964807.580345	40.860084
3497.523351	965404.208983	40.865088
3498.810308	965948.077141	40.870093
3500.514288	966454.240024	40.875098
3502.285060	966886.357474	40.880103
3503.968893	967279.311221	40.885108
3505.229132	967618.975340	40.890112
3506.228568	967909.344467	40.895117
3507.151939	968169.867606	40.900122
3508.629586	968386.061761	40.905127
3509.773846	968569.134328	40.910132
3510.722107	968719.750726	40.915136
3511.606009	968828.010239	40.920141
3512.123160	968907.270829	40.925146
3513.383171	968955.198528	40.930151
3513.988847	968977.796561	40.935156
3514.813644	968972.671133	40.940160
3515.474659	968935.286970	40.945165
3516.029094	968890.093205	40.950170
3516.391934	968810.981005	40.955175
3517.050631	968717.632270	40.960180
3517.389790	968594.982268	40.965184
3518.503211	968468.288350	40.970189
3518.591028	968317.592616	40.975194
3519.353040	968136.350788	40.980199
3519.858901	967944.479515	40.985204
3520.131772	967751.661658	40.990208
3520.331126	967525.772930	40.995213
3520.798450	967300.124764	41.000218
3521.251670	967055.973080	41.005223
3521.228678	966807.778851	41.010228
3521.648635	966535.912704	41.015232
3522.045205	966255.032467	41.020237
3522.178154	965974.181932	41.025242
3522.677112	965676.420101	41.030247
3522.632493	965380.592429	41.035252
3522.619909	965073.485585	41.040256
3522.859255	964749.089212	41.045261
3522.846011	964426.968141	41.050266
3523.438368	964102.085471	41.055271
3523.520302	963772.372361	41.060276
3523.493112	963420.722122	41.065280
3523.520088	963071.979532	41.070285
3523.532065	962725.372990	41.075290
3523.513030	962375.420467	41.080295
3523.576956	962019.066021	41.085300
3523.881373	961657.849876	41.090304
3524.215593	961289.062791	41.095309
3524.098816	960923.461501	41.100314
3524.054275	960540.580876	41.105319
3524.220075	960171.064106	41.110324
3524.316654	959781.250817	41.115328
3524.035394	959390.983413	41.120333
3523.751269	959023.035115	41.125338
3523.809846	958637.854961	41.130343
3524.179589	958243.678206	41.135348
3524.141575	957857.775734	41.140352
3523.925879	957468.837754	41.145357
3523.690074	957083.896393	41.150362
3524.180265	956695.476248	41.155367
3523.969347	956306.164961	41.160372
3523.486282	955922.951789	41.165376
3523.797447	955530.266269	41.170381
3523.774463	955134.666978	41.175386
3523.831772	954733.436950	41.180391
3523.697398	954353.004438	41.185396
3523.918717	953955.910988	41.190400
3523.600540	953557.211473	41.195405
3523.347897	953162.495913	41.200410
3523.647104	952769.624696	41.205415
3523.673226	952376.756800	41.210420
3523.529778	951989.487750	41.215424
3523.332408	951602.867599	41.220429
3523.176962	951224.628046	41.225434
3523.088242	950833.531936	41.230439
3523.300463	950453.165901	41.235444
3522.945687	950072.673614	41.240448
3523.102068	949690.633667	41.245453
3522.760595	949315.153555	41.250458
3523.132494	948923.261283	41.255463
3522.976967	948544.823376	41.260468
3522.779366	948170.001172	41.265472
3523.013229	947785.605200	41.270477
3522.448255	947403.322112	41.275482
3522.524332	947017.458876	41.280487
3522.548043	946635.117375	41.285492
3522.262401	946261.989326	41.290496
3522.232807	945881.323895	41.295501
3522.136311	945501.694637	41.300506
3521.932896	945125.885423	41.305511
3522.119332	944759.752788	41.310516
3521.657853	944384.410922	41.315520
3521.992964	944006.420259	41.320525
3522.035590	943650.002265	41.325530
3521.689171	943269.292189	41.330535
3521.672748	942889.266157	41.335540
3521.438241	942533.774983	41.340544
3521.506307	942156.459722	41.345549
3521.471351	941789.482712	41.350554
3521.508141	941426.876036	41.355559
3521.338193	941066.386478	41.360564
3521.117308	940695.816964	41.365568
3520.985450	940328.273533	41.370573
3520.899825	939961.271667	41.375578
3520.681886	939610.753949	41.380583
3520.905584	939253.525014	41.385588
3520.546353	938899.435645	41.390592
3520.849791	938530.543263	41.395597
3520.618069	938177.055077	41.400602
3520.569761	937824.759396	41.405607
3520.476042	937472.639274	41.410612
3520.144352	937116.698382	41.415616
3520.406600	936760.539540	41.420621
3520.194208	936414.698159	41.425626
3520.000435	936060.581229	41.430631
3519.840258	935708.833198	41.435636
3519.965770	935363.442480	41.440640
3519.613900	935005.730721	41.445645
3519.226053	934672.468343	41.450650
3519.557565	934328.031172	41.455655
3519.447182	933989.402144	41.460660
3519.441585	933649.198566	41.465664
3519.442580	933313.386883	41.470669
3518.899830	932970.060767	41.475674
3519.064908	932634.658790	41.480679
3519.243988	932306.144860	41.485684
3518.776017	931974.357087	41.490688
3518.786739	931636.229180	41.495693
3518.535431	931319.629764	41.500698
3518.593118	930984.524920	41.505703
3518.824493	930656.188048	41.510708
3518.499519	930344.343751	41.515712
3518.619459	930007.726485	41.520717
3518.059039	929673.216866	41.525722
3518.149346	929345.878672	41.530727
3518.000479	929030.278362	41.535732
3518.010233	928717.803176	41.540736
3518.262091	928389.803196	41.545741
3517.627522	928079.414080	41.550746
3517.705438	927763.989576	41.555751
3517.752165	927447.782896	41.560756
3517.647697	927143.016905	41.565760
3517.522760	926817.961076	41.570765
3517.251973	926513.570947	41.575770
3517.121988	926202.701247	41.580775
3517.069846	925913.425530	41.585780
3517.049703	925610.961063	41.590784
3516.985974	925300.028022	41.595789
3516.964026	925007.814778	41.600794
3517.200603	924690.548684	41.605799
3517.085787	924394.279761	41.610804
3516.694351	924100.155200	41.615808
3516.893010	923795.244863	41.620813
3516.595567	923503.475858	41.625818
3516.606446	923209.236256	41.630823
3516.376087	922904.057595	41.635828
3515.901155	922618.809014	41.640832
3516.444072	922318.085882	41.645837
3516.250522	922032.952278	41.650842
3516.137470	921733.362586	41.655847
3516.211085	921455.175939	41.660852
3515.958910	921167.697706	41.665856
3516.011412	920881.308382	41.670861
3515.852101	920606.387209	41.675866
3515.973941	920315.915897	41.680871
3516.044004	920034.289345	41.685876
3515.939814	919742.188822	41.690880
3515.783800	919456.720658	41.695885
3515.627339	919170.948838	41.700890
3515.599768	918892.165931	41.705895
3515.721135	918616.135139	41.710900
3515.405968	918342.087141	41.715904
3515.543855	918058.999394	41.720909
3515.328753	917796.072402	41.725914
3515.112391	917521.004165	41.730919
3515.209415	917236.436431	41.735924
3515.086668	916976.053744	41.740928
3515.333514	916693.550890	41.745933
3515.051909	916431.724239	41.750938
3514.955893	916153.389880	41.755943
3514.966349	915885.615558	41.760948
3514.812113	915618.047819	41.765952
3514.767450	915356.997194	41.770957
3514.658067	915092.381556	41.775962
3514.732716	914818.188341	41.780967
3514.608627	914557.883099	41.785972
3514.615592	914302.263404	41.790976
3514.638195	914029.483997	41.795981
3514.325604	913769.846590	41.800986
3514.129471	913517.402486	41.805991
3514.401585	913257.066479	41.810996
3514.208562	912997.950828	41.816000
3514.200374	912727.712899	41.821005
3513.742690	912477.479955	41.826010
3513.909521	912228.963433	41.831015
3513.915984	911975.740579	41.836020
3513.819155	911727.726629	41.841024
3513.563494	911475.294817	41.846029
3513.422643	911248.563439	41.851034
3513.676776	910978.870944	41.856039
3513.540600	910742.769596	41.861044
3513.305914	910505.614148	41.866048
3513.362488	910255.870138	41.871053
3513.304110	910012.013673	41.876058
3512.865569	909775.920753	41.881063
3513.228142	909536.022550	41.886068
3512.874617	909295.942699	41.891072
3513.159595	909067.412652	41.896077
3513.071599	908837.392017	41.901082
3513.130903	908586.125904	41.906087
3513.408748	908344.550912	41.911092
3512.669119	908110.461321	41.916096
3512.909917	907880.250331	41.921101
3512.821522	907650.180452	41.926106
3512.863710	907410.146491	41.931111
3512.890144	907176.662754	41.936116
3512.601978	906948.332628	41.941120
3512.614727	906718.593248	41.946125
3512.470022	906493.789421	41.951130
3512.574420	906265.366552	41.956135
3512.918515	906030.914226	41.961140
3512.378406	905805.279558	41.966144
3512.463579	905576.252778	41.971149
3512.116134	905352.786811	41.976154
3512.392746	905132.682230	41.981159
3511.896958	904906.232011	41.986164
3511.737829	904695.444088	41.991168
3511.843839	904476.017086	41.996173
3511.733270	904267.134743	42.001178
3511.577513	904049.277959	42.006183
3511.764843	903833.093141	42.011188
3511.739337	903626.681811	42.016192
3511.896817	903394.948004	42.021197
3511.611436	903185.281963	42.026202
3511.574334	902975.856702	42.031207
3511.439949	902754.374921	42.036212
3511.296456	902556.823188	42.041216
3511.144850	902349.999455	42.046221
3510.991916	902152.048905	42.051226
3510.908093	901945.778258	42.056231
3510.977299	901741.598588	42.061236
3510.897667	901554.137189	42.066240
3510.929717	901351.687148	42.071245
3510.890254	901153.682679	42.076250
3510.685803	900955.698412	42.081255
3510.563260	900763.004039	42.086260
3510.611877	900563.226317	42.091264
3510.484089	900367.043240	42.096269
3510.584835	900174.871283	42.101274
3510.427752	899985.825336	42.106279
3510.526119	899798.565760	42.111284
3510.439486	899616.159026	42.116288
3510.589744	899414.971807	42.121293
3510.319831	899225.339475	42.126298
3510.390499	899040.183991	42.131303
3510.282954	898856.790316	42.136308
3510.539525	898665.410483	42.141312
3510.307204	898469.468324	42.146317
3509.959186	898291.987986	42.151322
3510.116059	898113.452915	42.156327
3510.081976	897919.390964	42.161332
3510.188517	897736.408642	42.166336
3510.076101	897550.268441	42.171341
3509.501160	897373.859332	42.176346
3509.527064	897194.447338	42.181351
3509.610142	897021.203673	42.186356
3509.416614	896851.768422	42.191360
3509.411139	896673.504523	42.196365
3509.568993	896499.362986	42.201370
3509.354295	896331.944804	42.206375
3509.665741	896164.918151	42.211380
3509.452474	895986.183725	42.216384
3509.596323	895818.884599	42.221389
3509.201832	895651.379317	42.226394
3509.453260	895476.611143	42.231399
3509.258252	895304.520570	42.236404
3509.001421	895130.695300	42.241408
3509.041488	894959.232079	42.246413
3508.737239	894806.281323	42.251418
3509.132034	894640.065998	42.256423
3509.161997	894482.605272	42.261428
3508.429344	894320.046081	42.266432
3508.762448	894151.893428	42.271437
3508.940832	893999.904800	42.276442
3508.583884	893841.523414	42.281447
3508.925314	893674.805369	42.286452
3508.659699	893517.560009	42.291456
3508.953947	893355.674191	42.296461
3508.958265	893192.961418	42.301466
3508.526949	893051.199466	42.306471
3508.673589	892885.553973	42.311476
3508.108651	892741.389177	42.316480
3508.492563	892583.817698	42.321485
3508.588348	892431.510828	42.326490
3508.316265	892276.552999	42.331495
3507.999989	892111.444812	42.336500
3507.573438	891976.521054	42.341504
3508.154582	891822.667478	42.346509
3508.093680	891685.258999	42.351514
3507.974500	891535.187930	42.356519
3508.097378	891388.554669	42.361524
3508.012802	891255.975371	42.366528
3508.270318	891098.770684	42.371533
3508.331943	890960.647619	42.376538
3507.863090	890810.421731	42.381543
3508.050580	890657.375499	42.386548
3507.594692	890523.776472	42.391552
3507.888216	890371.478955	42.396557
3507.510576	890230.412075	42.401562
3507.758056	890092.334213	42.406567
3507.719977	889952.365360	42.411572
3507.644085	889823.620954	42.416576
3507.593030	889681.422661	42.421581
3507.461960	889546.102770	42.426586
3507.571740	889402.323189	42.431591
3507.793344	889263.262222	42.436596
3507.274869	889119.288826	42.441600
3507.362750	888986.144933	42.446605
3507.708494	888861.566614	42.451610
3507.532202	888722.558134	42.456615
3507.489450	888583.137261	42.461620
3507.293069	888452.350070	42.466624
3507.377637	888318.997775	42.471629
3507.372246	888192.237275	42.476634
3507.221186	888066.949499	42.481639
3507.199833	887919.283783	42.486644
3506.858818	887796.247130	42.491648
3507.356234	887659.134216	42.496653
3507.306156	887543.882974	42.501658
3506.938435	887414.261774	42.506663
3506.959264	887287.960973	42.511668
3506.775750	887169.046563	42.516672
3507.023755	887028.862729	42.521677
3506.929211	886915.638757	42.526682
3506.868072	886791.663495	42.531687
3507.248988	886655.610639	42.536692
3506.780823	886536.052556	42.541696
3506.923092	886410.680506	42.546701
3506.705076	886288.172222	42.551706
3506.395127	886173.614040	42.556711
3506.696744	886054.790378	42.561716
3506.501978	885934.303597	42.566720
3506.652706	885816.371132	42.571725
3506.625714	885709.598373	42.576730
3506.439404	885583.488084	42.581735
3506.267409	885467.053814	42.586740
3506.292907	885364.719361	42.591744
3506.600046	885242.102422	42.596749
3506.460190	885123.041943	42.601754
3506.534672	885002.685061	42.606759
3506.340377	884890.309273	42.611764
3506.227826	884781.500277	42.616768
3506.452916	884667.211444	42.621773
3506.061190	884560.574437	42.626778
3506.442797	884449.934940	42.631783
3506.621373	884330.321592	42.636788
3506.174883	884216.812350	42.641792
3506.581752	884095.994583	42.646797
3506.491544	883988.619558	42.651802
3506.246997	883876.910282	42.656807
3506.283335	883744.428885	42.661812
3506.095862	883633.480247	42.666816
3505.885722	883522.242695	42.671821
3506.218145	883413.915835	42.676826
3506.177250	883317.754350	42.681831
3506.035803	883187.710739	42.686836
3505.815115	883086.248344	42.691840
3506.071387	882990.710454	42.696845
3505.650779	882883.078896	42.701850
3505.830769	882776.024391	42.706855
3505.645264	882672.224440	42.711860
3505.792632	882576.697705	42.716864
3505.720174	882475.103382	42.721869
3506.083186	882363.555543	42.726874
3505.668491	882269.181862	42.731879
3505.918918	882150.480526	42.736884
3505.735076	882062.458643	42.741888
3505.695166	881957.943912	42.746893
3505.840298	881859.596585	42.751898
3505.492008	881750.866616	42.756903
3505.574830	881640.416723	42.761908
3505.320178	881550.558160	42.766912
3505.421626	881447.173512	42.771917
3505.646516	881351.807714	42.776922
3505.239744	881270.592186	42.781927
3505.485230	881169.504039	42.786932
3505.353949	881077.970875	42.791937
3505.505325	880971.469293	42.796941
3505.502384	880885.434466	42.801946
3505.341697	880792.060810	42.806951
3505.496948	880689.816573	42.811956
3504.717530	880603.421069	42.816961
3504.935614	880496.802963	42.821965
3505.386128	880420.279068	42.826970
3505.549952	880333.142801	42.831975
3505.514538	880238.480017	42.836980
3505.175987	880148.323026	42.841985
3505.173214	880049.291323	42.846989
3505.147411	879956.075909	42.851994
3505.332573	879869.607551	42.856999
3505.185664	879771.370131	42.862004
3505.037853	879684.953906	42.867009
3505.201143	879594.705715	42.872013
3505.301397	879495.744594	42.877018
3505.105822	879423.868926	42.882023
3505.109520	879323.854786	42.887028
3505.139795	879242.054526	42.892033
3504.624412	879148.325440	42.897037
3505.114370	879070.517531	42.902042
3505.271411	878971.441296	42.907047
3505.246205	878884.508484	42.912052
3504.840203	878792.984869	42.917057
3505.107776	878712.010427	42.922061
3505.401313	878616.201104	42.927066
3504.923378	878537.285574	42.932071
3504.938237	878446.171847	42.937076
3504.770917	878361.871760	42.942081
3504.895021	878278.394825	42.947085
3504.772021	878188.366048	42.952090
3504.585545	878111.529281	42.957095
3505.050872	878011.901414	42.962100
3504.540608	877937.539087	42.967105
3504.857824	877852.570254	42.972109
3504.596494	877775.450614	42.977114
3504.524883	877701.982426	42.982119
3504.697212	877618.294302	42.987124
3504.433337	877549.606010	42.992129
3504.628026	877462.422057	42.997133
3504.993734	877372.591114	43.002138
3504.557292	877291.907007	43.007143
3504.821183	877207.034595	43.012148
3504.675464	877140.648819	43.017153
3504.354547	877050.247441	43.022157
3504.760108	876966.026874	43.027162
3504.463537	876899.178469	43.032167
3504.763889	876818.851260	43.037172
3504.320126	876741.748135	43.042177
3504.629616	876660.641620	43.047181
3504.473419	876582.034673	43.052186
3504.103967	876509.958106	43.057191
3504.608501	876426.392249	43.062196
3504.373924	876351.867506	43.067201
3504.591685	876277.752114	43.072205
3504.650208	876209.673829	43.077210
3504.580091	876126.101434	43.082215
3504.464960	876041.468633	43.087220
3504.371479	875974.673255	43.092225
3504.639022	875898.314629	43.097229
3504.848092	875814.497890	43.102234
3504.574380	875743.074978	43.107239
3504.555097	875653.378271	43.112244
3504.418317	875589.785804	43.117249
3504.434943	875509.390556	43.122253
3504.424017	875433.168777	43.127258
3504.477311	875347.528515	43.132263
3504.530387	875258.298786	43.137268
3504.302046	875194.911115	43.142273
3504.524773	875123.398924	43.147277
3504.307672	875051.473413	43.152282
3504.084487	874978.966122	43.157287
3504.360492	874905.793785	43.162292
3504.191235	874829.008392	43.167297
3503.918425	874752.627016	43.172301
3504.258878	874687.006447	43.177306
3504.125233	874620.299375	43.182311
3504.024556	874537.291499	43.187316
3504.137282	874471.706066	43.192321
3504.111326	874406.821713	43.197325
3504.222802	874332.020498	43.202330
3503.769981	874275.837610	43.207335
3504.084737	874207.985061	43.212340
3503.735009	874143.927149	43.217345
3504.036130	874078.112326	43.222349
3503.970494	874009.641182	43.227354
3503.804183	873939.827810	43.232359
3503.891075	873873.852013	43.237364
3503.541488	873814.155636	43.242369
3503.598230	873754.003694	43.247373
3503.953332	873697.876227	43.252378
3503.802200	873627.280629	43.257383
3503.908675	873558.096870	43.262388
3503.678928	873504.683145	43.267393
3503.679194	873422.613119	43.272397
3503.822180	873369.330788	43.277402
3503.629019	873307.857343	43.282407
3503.896153	873235.053905	43.287412
3503.932104	873183.533780	43.292417
3503.903298	873113.494002	43.297421
3503.907180	873045.873422	43.302426
3503.498471	872986.566520	43.307431
3503.838239	872926.553603	43.312436
3503.792750	872857.289700	43.317441
3504.235543	872798.325730	43.322445
3503.798934	872729.997964	43.327450
3503.278435	872674.102109	43.332455
3503.810264	872607.650853	43.337460
3503.576873	872543.750541	43.342465
3503.691827	872486.875011	43.347469
3503.944966	872435.603698	43.352474
3503.642478	872367.928855	43.357479
3503.796950	872302.797724	43.362484
3503.673224	872249.161182	43.367489
3503.581617	872193.578262	43.372493
3503.836202	872132.601073	43.377498
3503.625879	872070.341403	43.382503
3504.016953	872000.219337	43.387508
3503.706038	871945.640566	43.392513
3503.669389	871871.803120	43.397517
3503.807924	871815.790614	43.402522
3503.295803	871760.272927	43.407527
3503.418903	871692.035092	43.412532
3503.526336	871641.654296	43.417537
3503.573591	871589.342189	43.422541
3503.590436	871523.642972	43.427546
3503.633127	871469.098615	43.432551
3503.872112	871416.074105	43.437556
3503.282670	871351.928526	43.442561
3503.654698	871287.138625	43.447565
3503.551312	871229.801840	43.452570
3503.453281	871180.033270	43.457575
3503.393564	871106.190137	43.462580
3503.310676	871057.000333	43.467585
3503.423775	871001.954860	43.472589
3503.290159	870945.008515	43.477594
3502.962326	870887.317212	43.482599
3503.129227	870831.776048	43.487604
3503.207295	870791.583401	43.492609
3503.317026	870745.562044	43.497613
3503.299531	870700.531838	43.502618
3503.363310	870651.605691	43.507623
3503.370338	870590.653524	43.512628
3503.124993	870539.642149	43.517633
3503.280109	870478.761499	43.522637
3503.527466	870432.326822	43.527642
3503.359836	870380.524813	43.532647
3503.393476	870325.971498	43.537652
3503.219304	870266.113539	43.542657
3503.028860	870217.516905	43.547661
3503.170900	870158.479331	43.552666
3503.406311	870115.441376	43.557671
3503.253421	870058.295620	43.562676
3503.135575	870007.841085	43.567681
3502.956255	869951.863454	43.572685
3503.201720	869906.007402	43.577690
3502.616903	869867.859102	43.582695
3503.185074	869816.901660	43.587700
3503.248231	869774.472046	43.592705
3502.974381	869713.071855	43.597709
3503.324788	869658.169046	43.602714
3502.869780	869618.056334	43.607719
3502.778441	869561.089827	43.612724
3502.811125	869524.973206	43.617729
3502.884582	869484.578384	43.622733
3502.901168	869446.716606	43.627738
3502.543656	869403.285841	43.632743
3502.743911	869352.093836	43.637748
3502.863300	869304.506573	43.642753
3502.710038	869265.895017	43.647757
3502.871913	869212.087037	43.652762
3502.326934	869181.208681	43.657767
3502.660030	869133.584851	43.662772
3502.710303	869089.113821	43.667777
3502.581708	869053.312168	43.672781
3502.757294	869005.519109	43.677786
3502.457752	868975.861321	43.682791
3502.624766	868929.622389	43.687796
3502.702252	868905.338796	43.692801
3502.796860	868853.480351	43.697805
3502.812520	868808.527519	43.702810
3502.961346	868767.630019	43.707815
3502.784331	868730.378124	43.712820
3502.832262	868683.574395	43.717825
3502.693322	868641.558398	43.722829
3503.058517	868595.284238	43.727834
3502.733948	868560.094455	43.732839
3502.737093	868503.393587	43.737844
3502.644104	868460.689120	43.742849
3502.488380	868417.315044	43.747853
3502.670987	868370.972144	43.752858
3502.773605	868340.953677	43.757863
3502.877119	868302.390697	43.762868
3502.729165	868263.577617	43.767873
3502.579408	868212.142262	43.772877
3502.698471	868166.682109	43.777882
3502.418980	868132.453343	43.782887
3502.931381	868079.742607	43.787892
3502.399702	868047.011357	43.792897
3502.253482	868012.759951	43.797901
3502.239860	867974.602555	43.802906
3502.034636	867943.176335	43.807911
3502.354648	867906.225828	43.812916
3502.421014	867872.326996	43.817921
3502.639763	867846.365137	43.822925
3502.862529	867797.001066	43.827930
3502.485644	867764.631176	43.832935
3502.620835	867714.989554	43.837940
3502.656505	867679.249733	43.842945
3502.258282	867634.453395	43.847949
3502.529717	867602.170024	43.852954
3502.165540	867570.476725	43.857959
3502.512724	867529.926535	43.862964
3502.271436	867500.543161	43.867969
3502.512290	867460.689767	43.872973
3502.475672	867420.784715	43.877978
3502.539909	867397.953821	43.882983
3502.278133	867347.015048	43.887988
3502.350628	867320.492362	43.892993
3502.562272	867289.285365	43.897997
3502.387578	867253.092119	43.903002
3502.370894	867210.754628	43.908007
3502.764998	867176.215208	43.913012
3502.651641	867141.176522	43.918017
3502.502545	867105.075279	43.923021
3502.431164	867071.777302	43.928026
3502.414428	867027.884719	43.933031
3502.562289	866997.269401	43.938036
3502.335947	866974.970348	43.943041
3502.434366	866931.058086	43.948045
3502.606547	866885.482375	43.953050
3502.453280	866858.315032	43.958055
3502.446418	866806.649862	43.963060
3502.483310	866783.432671	43.968065
3502.511383	866742.541280	43.973069
3502.482829	866712.633410	43.978074
3502.265015	866673.821563	43.983079
3502.395980	866630.581586	43.988084
3502.618280	866603.156973	43.993089
3502.177145	866568.168950	43.998093
3502.379309	866516.369729	44.003098
3502.268648	866502.402374	44.008103
3502.542313	866460.206010	44.013108
3502.372472	866423.521354	44.018113
3502.603946	866386.770357	44.023117
3502.659140	866347.911429	44.028122
3502.155539	866306.619046	44.033127
3502.609460	866271.287581	44.038132
3502.420136	866243.540644	44.043137
3502.313090	866202.862102	44.048141
3502.430582	866170.887805	44.053146
3502.299832	866136.720284	44.058151
3502.217399	866108.080956	44.063156
3502.084324	866081.683809	44.068161
3502.258554	866046.397107	44.073165
3502.444925	866007.417242	44.078170
3502.268506	865973.839103	44.083175
3502.125081	865940.255342	44.088180
3502.670659	865895.096279	44.093185
3502.484471	865872.397992	44.098189
3502.274180	865828.722820	44.103194
3502.470068	865808.972479	44.108199
3502.164199	865768.323759	44.113204
3502.259995	865735.573654	44.118209
3501.699480	865703.417176	44.123213
3502.309132	865663.102589	44.128218
3501.822723	865647.058161	44.133223
3502.117861	865607.280700	44.138228
3502.278145	865590.838166	44.143233
3502.226976	865554.031524	44.148237
3502.586394	865520.751132	44.153242
3502.498059	865496.481093	44.158247
3502.369749	865447.835578	44.163252
3502.305747	865417.732841	44.168257
3502.043964	865389.022504	44.173261
3502.581819	865357.848906	44.178266
3502.367454	865343.215960	44.183271
3502.519611	865294.328717	44.188276
3502.690667	865268.752181	44.193281
3502.397507	865225.183432	44.198285
3502.488846	865189.711092	44.203290
3502.116986	865158.880634	44.208295
3502.105989	865113.807430	44.213300
3502.291860	865088.324834	44.218305
3502.168999	865067.361695	44.223309
3502.497554	865022.037574	44.228314
3502.328214	864992.435801	44.233319
3502.390489	864950.360857	44.238324
3502.163887	864922.905422	44.243329
3502.354334	864898.004157	44.248333
3502.371038	864862.250746	44.253338
3502.038275	864838.504075	44.258343
3502.177349	864797.678355	44.263348
3502.273054	864767.351761	44.268353
3502.287979	864740.827210	44.273357
3502.833051	864708.191815	44.278362
3502.443944	864670.172492	44.283367
3502.571659	864630.221881	44.288372
3502.610936	864597.183457	44.293377
3502.253809	864559.061011	44.298381
3502.450561	864513.171869	44.303386
3502.197698	864489.896434	44.308391
3502.535175	864458.168288	44.313396
3502.113181	864419.667028	44.318401
3502.553044	864409.878985	44.323405
3502.622910	864367.410108	44.328410
3502.044652	864323.590349	44.333415
3502.252743	864291.882649	44.338420
3502.324549	864256.602368	44.343425
3502.077761	864231.964716	44.348429
3502.394702	864191.494237	44.353434
3502.181513	864167.239424	44.358439
3502.163091	864138.968844	44.363444
3502.403943	864107.934907	44.368449
3502.100158	864071.646656	44.373453
3502.099199	864042.401131	44.378458
3501.862305	864024.659508	44.383463
3502.102763	863988.669742	44.388468
3501.996208	863960.315684	44.393473
3501.886546	863935.362740	44.398477
3502.319618	863903.518777	44.403482
3502.048696	863878.203508	44.408487
3502.125761	863842.142627	44.413492
3502.222773	863817.349476	44.418497
3501.911189	863789.611392	44.423501
3502.206810	863757.594976	44.428506
3501.973862	863720.807114	44.433511
3501.963998	863691.658529	44.438516
3502.543126	863678.639832	44.443521
3502.203078	863647.310570	44.448525
3502.251667	863612.904878	44.453530
3502.235587	863594.153921	44.458535
3502.013679	863556.974567	44.463540
3502.144750	863518.473613	44.468545
3501.944580	863504.222548	44.473549
3501.907589	863467.498032	44.478554
3501.891701	863452.050427	44.483559
3501.976494	863420.941512	44.488564
3501.901038	863400.353468	44.493569
3501.780320	863364.711019	44.498573
3502.439584	863333.507010	44.503578
3502.248712	863315.950071	44.508583
3502.158454	863274.665994	44.513588
3502.351790	863245.384610	44.518593
3501.820247	863220.303874	44.523597
3502.214117	863180.882902	44.528602
3502.242518	863164.649860	44.533607
3502.327515	863135.191441	44.538612
3502.347206	863111.574262	44.543617
3502.049243	863074.307297	44.548621
3502.159010	863043.581043	44.553626
3501.896708	863012.721575	44.558631
3501.684616	862979.618558	44.563636
3501.712009	862948.905395	44.568641
3501.952803	862941.480104	44.573645
3502.324890	862912.847924	44.578650
3502.251705	862885.552318	44.583655
3502.271115	862850.272479	44.588660
3502.185599	862819.771627	44.593665
3501.819073	862788.053551	44.598669
3502.576116	862761.592426	44.603674
3502.262771	862745.997663	44.608679
3502.229617	862696.925608	44.613684
3502.387882	862681.252979	44.618689
3501.859721	862655.294686	44.623693
3501.785150	862626.831931	44.628698
3501.798360	862593.106574	44.633703
3501.890124	862566.462653	44.638708
3501.915648	862548.381907	44.643713
3501.566324	862511.508685	44.648717
3501.960877	862501.433485	44.653722
3502.061736	862469.831113	44.658727
3501.888438	862451.782835	44.663732
3501.769752	862416.328850	44.668737
3501.805110	862394.455686	44.673741
3501.732615	862378.528729	44.678746
3501.815974	862341.097241	44.683751
3501.714178	862333.630463	44.688756
3501.766460	862314.864286	44.693761
3501.799888	862294.934876	44.698765
3501.980648	862268.372175	44.703770
3501.915619	862241.461089	44.708775
3501.692544	862222.059655	44.713780
3501.571558	862183.883334	44.718785
3501.525599	862169.895295	44.723789
3501.831107	862150.989700	44.728794
3501.868517	862129.601206	44.733799
3501.926233	862106.848587	44.738804
3502.113953	862079.214789	44.743809
3501.587908	862049.074222	44.748813
3501.805813	862032.223766	44.753818
3501.786770	862003.262967	44.758823
3501.657313	861996.869473	44.763828
3501.845994	861971.373314	44.768833
3501.829068	861939.204415	44.773837
3502.172582	861910.086244	44.778842
3501.690897	861888.199245	44.783847
3501.691623	861870.120565	44.788852
3501.834122	861845.992245	44.793857
3501.790585	861837.154495	44.798861
3502.061376	861806.492651	44.803866
3501.699439	861792.652999	44.808871
3501.562907	861762.349634	44.813876
3501.940237	861753.539622	44.818881
3501.750259	861729.076820	44.823885
3501.810508	861700.198712	44.828890
3501.685979	861676.210912	44.833895
3501.940895	861656.534518	44.838900
3502.112944	861629.776064	44.843905
3501.958973	861604.334819	44.848909
3501.941369	861578.093389	44.853914
3501.801639	861558.190092	44.858919
3501.983372	861535.706510	44.863924
3502.388521	861503.368565	44.868929
3501.786480	861483.832800	44.873933
3502.022321	861442.093718	44.878938
3501.891216	861433.950235	44.883943
3501.917609	861396.911134	44.888948
3501.746810	861385.857991	44.893953
3501.825037	861363.390826	44.898957
3502.064021	861328.649205	44.903962
3501.785604	861311.100881	44.908967
3501.966665	861283.756185	44.913972
3501.921545	861261.308965	44.918977
3501.948275	861226.698939	44.923981
3502.093704	861197.804413	44.928986
3502.088303	861174.961500	44.933991
3501.936786	861160.502489	44.938996
3502.245040	861114.569277	44.944001
3501.957926	861099.743625	44.949005
3501.956465	861067.664778	44.954010
3501.938167	861044.434660	44.959015
3501.655174	861009.971639	44.964020
3501.996425	860996.694792	44.969025
3501.696242	860977.496504	44.974029
3501.954205	860950.915335	44.979034
3501.719922	860939.677416	44.984039
3501.589846	860918.215044	44.989044
3502.074912	860893.832088	44.994049
3501.545213	860872.824245	44.999053
3501.857167	860837.290098	45.004058
3501.810317	860825.632234	45.009063
3501.731552	860794.050749	45.014068
3501.747669	860762.453468	45.019073
3501.736666	860764.107966	45.024077
3501.621786	860729.421229	45.029082
3501.942815	860704.967330	45.034087
3501.875858	860691.757073	45.039092
3502.109350	860665.664772	45.044097
3501.551054	860652.049298	45.049101
3501.720897	860615.565109	45.054106
3501.753177	860601.949440	45.059111
3501.837155	860582.200526	45.064116
3501.974019	860552.234959	45.069121
3501.681109	860545.866865	45.074125
3501.713934	860517.376538	45.079130
3501.654047	860495.415019	45.084135
3501.406662	860477.567517	45.089140
3501.818886	860449.208802	45.094145
3501.603172	860438.258554	45.099149
3501.801276	860420.045829	45.104154
3501.452840	860389.673317	45.109159
3501.628228	860385.950076	45.114164
3501.852606	860365.496784	45.119169
3501.847086	860332.053639	45.124173
3501.959920	860312.687984	45.129178
3501.941294	860296.163366	45.134183
3501.848802	860270.025858	45.139188
3502.028405	860247.829545	45.144193
3501.953526	860220.813919	45.149197
3502.024054	860193.676993	45.154202
3501.928213	860174.248055	45.159207
3501.729662	860146.766355	45.164212
3501.696198	860121.687954	45.169217
3501.775295	860108.355145	45.174221
3501.977106	860081.584991	45.179226
3501.947969	860051.255411	45.184231
3501.719169	860036.612008	45.189236
3501.988268	860015.372368	45.194241
3501.720804	860008.999517	45.199245
3501.988819	859970.453537	45.204250
3501.868010	859951.611366	45.209255
3501.661154	859927.241325	45.214260
3502.073569	859902.185790	45.219265
3502.077626	859885.267408	45.224269
3501.949999	859849.313790	45.229274
3501.663289	859836.818489	45.234279
3501.927650	859808.383933	45.239284
3502.087178	859782.300043	45.244289
3501.528971	859764.307198	45.249293
3501.797354	859725.856844	45.254298
3501.619360	859723.747121	45.259303
3501.504144	859693.818870	45.264308
3501.924411	859673.525453	45.269313
3501.311191	859658.847244	45.274317
3501.737709	859642.150283	45.279322
3501.533478	859616.417312	45.284327
3501.628286	859605.414405	45.289332
3501.864151	859579.317071	45.294337
3501.563970	859563.711957	45.299341
3501.545219	859543.782141	45.304346
3501.741092	859510.981953	45.309351
3501.537492	859490.499010	45.314356
3502.218144	859482.413642	45.319361
3501.508944	859455.693603	45.324365
3501.676647	859433.885236	45.329370
3501.582392	859416.301102	45.334375
3501.394439	859390.078313	45.339380
3502.069305	859364.296681	45.344385
3501.607128	859355.329827	45.349389
3501.976980	859331.056862	45.354394
3501.971220	859304.511978	45.359399
3501.654638	859282.393907	45.364404
3501.986654	859259.585465	45.369409
3501.801173	859248.239140	45.374413
3502.015581	859213.489528	45.379418
3502.058811	859194.715233	45.384423
3501.854789	859171.605819	45.389428
3502.207239	859147.237754	45.394433
3501.858473	859127.166469	45.399437
3501.926791	859097.496779	45.404442
3502.110627	859067.905154	45.409447
3501.954397	859050.135692	45.414452
3501.891137	859017.278308	45.419457
3501.577424	859015.968636	45.424461
3501.700241	858971.022274	45.429466
3501.981335	858950.554906	45.434471
3501.675533	858940.200266	45.439476
3501.879772	858898.643483	45.444481
3501.504376	858903.567580	45.449485
3501.459874	858874.304371	45.454490
3501.647840	858855.116208	45.459495
3501.412399	858840.082044	45.464500
3501.339778	858831.536460	45.469505
3501.425254	858808.864204	45.474509
3501.525251	858775.297901	45.479514
3501.486869	858774.331799	45.484519
3501.645809	858771.680000	45.489524
3501.682756	858734.331254	45.494529
3501.405514	858721.540362	45.499533
3501.764574	858703.490502	45.504538
3501.639133	858680.560778	45.509543
3501.695163	858676.369928	45.514548
3501.824932	858641.144772	45.519553
3501.725259	858622.295015	45.524557
3501.578808	858606.370375	45.529562
3501.586390	858586.724846	45.534567
3501.606380	858560.366987	45.539572
3501.894660	858540.772314	45.544577
3501.516872	858529.067334	45.549581
3501.808137	858507.235308	45.554586
3501.475704	858500.968828	45.559591
3501.779398	858476.314376	45.564596
3501.943314	858447.501042	45.569601
3501.722403	858439.854605	45.574605
3501.652169	858400.576448	45.579610
3501.792065	858388.883160	45.584615
3501.678506	858374.411283	45.589620
3501.917370	858348.016449	45.594625
3501.778031	858331.117390	45.599629
3501.558332	858303.339113	45.604634
3501.763219	858282.687564	45.609639
3501.832376	858269.060621	45.614644
3502.027088	858240.630258	45.619649
3501.513511	858237.019227	45.624653
3501.644143	858209.960846	45.629658
3501.847520	858176.568740	45.634663
3501.617036	858173.300053	45.639668
3501.715765	858140.022244	45.644673
3501.422528	858132.192824	45.649677
3501.579035	858113.299291	45.654682
3501.262481	858091.468669	45.659687
3501.763199	858065.904793	45.664692
3501.872936	858060.051296	45.669697
3501.816349	858037.010558	45.674701
3501.913552	858021.725058	45.679706
3501.868280	858009.964298	45.684711
3501.553226	857973.446970	45.689716
3502.091166	857956.824329	45.694721
3501.915411	857923.882346	45.699725
3501.798803	857899.003042	45.704730
3501.792487	857898.128777	45.709735
3501.334359	857857.549400	45.714740
3502.038314	857844.205971	45.719745
3501.476478	857819.302434	45.724749
3501.423169	857800.442506	45.729754
3501.432750	857796.064184	45.734759
3501.901679	857786.649823	45.739764
3501.881976	857748.234514	45.744769
3501.565256	857748.870306	45.749773
3501.644850	857718.122186	45.754778
3501.900978	857685.496819	45.759783
3501.504664	857681.282552	45.764788
3501.818286	857641.255437	45.769793
3501.922935	857635.596903	45.774797
3502.025386	857613.014690	45.779802
3502.095586	857588.006080	45.784807
3501.692565	857545.275720	45.789812
3501.836008	857458.295898	45.794817
3501.710208	857324.183777	45.799821
3501.729616	857137.323466	45.804826
3501.715268	856886.941985	45.809831
3501.403817	856578.717259	45.814836
3501.502681	856197.639120	45.819841
3501.453331	855776.184989	45.824845
3501.099982	855288.392807	45.829850
3501.067755	854739.398596	45.834855
3500.993946	854140.048319	45.839860
3500.825068	853471.746160	45.844865
3500.218145	852747.472791	45.849869
3500.337183	851953.289988	45.854874
3499.987698	851109.133480	45.859879
3499.379018	850182.715292	45.864884
3499.410926	849199.758368	45.869889
3498.765172	848151.491490	45.874893
3498.494107	847057.876883	45.879898
3498.059277	845884.093429	45.884903
3497.581740	844652.201966	45.889908
3497.224948	843339.622353	45.894913
3496.686364	841963.419003	45.899917
3496.172913	840515.178227	45.904922
3495.674472	839012.852256	45.909927
3495.068575	837430.321848	45.914932
3494.543425	835789.165781	45.919937
3493.487078	834082.021489	45.924941
3493.031193	832312.118392	45.929946
3492.720734	830463.656926	45.934951
3492.256946	828544.731434	45.939956
3491.848285	826552.755123	45.944961
3490.717164	824494.245025	45.949965
3490.113279	822376.759864	45.954970
3489.569597	820176.254956	45.959975
3488.520751	817913.835502	45.964980
3488.417886	815586.706457	45.969985
3487.572651	813198.118944	45.974989
3486.359117	810737.564777	45.979994
3485.679622	808192.667967	45.984999
3484.679793	805592.306766	45.990004
3483.854641	802928.200741	45.995009
3483.212117	800198.416286	46.000013
3482.205992	797388.934489	46.005018
3481.258339	794518.353921	46.010023
3479.769807	791595.695576	46.015028
3479.217258	788593.285770	46.020033
3478.073803	785537.538306	46.025037
3477.335530	782396.995801	46.030042
3476.191724	779202.151215	46.035047
3474.375374	775951.362461	46.040052
3473.712637	772612.003724	46.045057
3472.111019	769245.709234	46.050061
3471.175155	765794.264012	46.055066
3469.922504	762281.152867	46.060071
3468.218496	758713.727004	46.065076
3467.405435	755076.151707	46.070081
3465.918062	751381.195174	46.075085
3464.579809	747627.913675	46.080090
3463.290888	743804.241762	46.085095
3461.928140	739920.798637	46.090100
3460.657108	735980.456620	46.095105
3459.040215	731983.767286	46.100109
3457.570273	727905.271081	46.105114
3456.318600	723777.615804	46.110119
3454.393142	719582.201179	46.115124
3453.050738	715332.085966	46.120129
3451.673901	711030.787105	46.125133
3450.011925	706649.784836	46.130138
3448.226168	702214.595721	46.135143
3446.703094	697735.091970	46.140148
3445.281947	693179.972188	46.145153
3443.342912	688563.284391	46.150157
3441.141668	683888.406007	46.155162
3439.553330	679169.630202	46.160167
3437.796937	674389.703741	46.165172
3436.082221	669553.666431	46.170177
3433.830497	664659.714303	46.175181
3431.897357	659702.010373	46.180186
3430.382039	654702.152305	46.185191
3428.451124	649642.259631	46.190196
3426.535599	644504.758040	46.195201
3424.573300	639329.345754	46.200205
3422.350620	634100.625557	46.205210
3420.542264	628809.233065	46.210215
3418.062980	623479.341697	46.215220
3416.192059	618088.070525	46.220225
3413.915242	612648.678196	46.225229
3411.578622	607153.656279	46.230234
3409.479776	601619.033338	46.235239
3407.154975	596033.877319	46.240244
3404.878750	590384.853967	46.245249
3402.536648	584708.032693	46.250253
3400.153867	578962.634240	46.255258
3397.870705	573179.132041	46.260263
3395.617355	567358.242290	46.265268
3393.208897	561463.738545	46.270273
3390.780384	555542.510694	46.275277
3388.242845	549564.653160	46.280282
3385.896549	543547.193655	46.285287
3383.216085	537479.278257	46.290292
3380.378539	531372.480506	46.295297
3377.938950	525225.003593	46.300301
3375.550257	519020.297582	46.305306
3372.676241	512783.254741	46.310311
3369.796352	506503.306257	46.315316
3367.289100	500169.784205	46.320321
3364.305887	493826.036568	46.325325
3361.737287	487429.004850	46.330330
3358.758523	480997.110238	46.335335
3355.767065	474522.569643	46.340340
3353.061643	468017.365603	46.345345
3349.817936	461476.554653	46.350349
3346.667931	454896.570564	46.355354
3343.895889	448288.101141	46.360359
3340.525859	441648.208790	46.365364
3337.160879	434979.934794	46.370369
3334.190269	428286.970098	46.375373
3331.002203	421571.551763	46.380378
3327.948230	414811.156954	46.385383
3324.572497	408033.205903	46.390388
3320.940207	401238.692458	46.395393
3318.050426	394409.781701	46.400397
3314.475684	387558.201700	46.405402
3311.289457	380693.780264	46.410407
3307.553803	373805.607433	46.415412
3304.266857	366874.791511	46.420417
3300.674052	359933.462865	46.425421
3296.808127	352983.066969	46.430426
3293.547865	346007.100299	46.435431
3289.718044	339029.444179	46.440436
3286.214702	332025.804126	46.445441
3282.545005	325025.353670	46.450445
3278.876531	317996.049125	46.455450
3275.377060	310960.394117	46.460455
3271.622348	303925.671480	46.465460
3267.835661	296856.229910	46.470465
3263.572903	289784.969824	46.475469
3259.427436	282716.056092	46.480474
3256.045484	275639.995072	46.485479
3252.049449	268570.343096	46.490484
3247.914046	261477.973050	46.495489
3243.858495	254389.600439	46.500493
3239.607590	247302.479802	46.505498
3235.859467	240207.109168	46.510503
3231.505605	233129.200080	46.515508
3227.423787	226027.311877	46.520513
3222.863613	218895.038987	46.525517
3218.237743	211820.810344	46.530522
3214.411751	204757.788155	46.535527
3209.721938	197721.986097	46.540532
3205.289781	190673.219307	46.545537
3200.700961	183651.387959	46.550541
3196.100980	176651.517388	46.555546
3191.724771	169647.806227	46.560551
3187.100555	162691.158208	46.565556
3182.368086	155735.992579	46.570561
3177.631350	148812.205022	46.575565
3172.793944	141895.848979	46.580570
3167.704757	135020.353891	46.585575
3162.617607	128168.031936	46.590580
3158.146898	121341.337158	46.595585
3152.904248	114556.348990	46.600589
3147.446945	107801.303325	46.605594
3142.220716	101073.585620	46.610599
3136.670334	94402.687338	46.615604
3131.553720	87762.425096	46.620609
3125.943924	81185.652000	46.625613
3119.960644	74648.354140	46.630618
3113.985519	68159.037037	46.635623
3107.570362	61755.011241	46.640628
3100.944056	55414.745949	46.645633
3093.450257	49140.887822	46.650637
3082.017710	43079.749223	46.655642
3064.491144	37307.876448	46.660647
3045.417175	31768.207850	46.665652
3027.114541	26487.417398	46.670657
3007.135789	21578.773262	46.675661
2983.931034	17100.141177	46.680666
2958.540773	13081.884962	46.685671
2932.144020	9566.849843	46.690676
2907.610952	6507.049233	46.695681
2884.984042	3906.442548	46.700685
2864.308137	1776.182099	46.705690
2834.372827	388.579210	46.710695
2776.711938	283.305781	46.715700
2746.148810	288.747228	46.720705
2743.198935	287.737738	46.725709
2757.152832	287.526852	46.730714
2777.388932	272.825060	46.735719
2794.137032	283.130633	46.740724
2804.653980	279.578762	46.745729
2808.315520	277.418843	46.750733
2806.964484	275.674277	46.755738
2803.719998	270.211975	46.760743
2799.011592	265.405626	46.765748
2795.729279	257.573573	46.770753
2792.376171	261.501786	46.775757
2789.302815	264.739719	46.780762
2786.687455	269.197051	46.785767
2784.051385	271.981575	46.790772
2781.561092	265.725075	46.795777
2778.936318	254.421043	46.800781
2776.567346	249.932457	46.805786
2773.546546	249.059375	46.810791
2770.473730	262.972264	46.815796
2767.367700	251.340331	46.820801
2764.355482	246.608588	46.825805
2761.094351	252.044335	46.830810
2757.636339	240.428262	46.835815
2754.358385	254.326845	46.840820
2751.427171	253.084174	46.845825
2748.170679	246.144624	46.850829
2745.296603	246.738073	46.855834
2742.148128	244.872923	46.860839
2738.759060	242.403348	46.865844
2735.036321	236.302089	46.870849
2731.875838	243.964232	46.875853
2728.308746	239.916490	46.880858
2725.423756	239.814344	46.885863
2722.084401	242.776509	46.890868
2718.802266	241.867251	46.895873
2715.487832	247.314580	46.900877
2711.960385	254.067550	46.905882
2709.109444	249.469867	46.910887
2705.030636	245.015591	46.915892
2701.618888	239.948027	46.920897
2698.926409	239.460495	46.925901
2694.921072	240.968830	46.930906
2691.785350	241.801641	46.935911
2688.270003	240.777748	46.940916
2684.799533	241.117584	46.945921
2681.715016	229.821214	46.950925
2678.765921	234.409437	46.955930
2675.227197	235.513993	46.960935
2671.227093	233.496564	46.965940
2667.725639	236.406968	46.970945
2664.352560	231.904951	46.975949
2661.068415	242.031418	46.980954
2657.803771	227.075288	46.985959
2653.737934	240.309820	46.990964
2651.142761	234.178068	46.995969
2648.102045	230.969061	47.000973
2643.901648	236.119005	47.005978
2640.502662	240.129868	47.010983
2636.928457	233.881036	47.015988
2633.989416	233.446856	47.020993
2630.166890	226.293349	47.025997
2626.153209	234.767302	47.031002
2623.164881	231.188137	47.036007
2620.241254	233.662605	47.041012
2616.083867	216.003441	47.046017
2612.934041	217.633913	47.051021
2609.218674	227.758151	47.056026
2605.943486	225.590756	47.061031
2602.520052	220.895414	47.066036
2599.578089	218.153631	47.071041
2595.752802	218.177923	47.076045
2592.040199	228.594965	47.081050
2588.688697	221.319164	47.086055
2585.702973	223.925856	47.091060
2582.131147	211.338471	47.096065
2578.061631	218.325028	47.101069
2574.710968	219.392302	47.106074
2571.378348	214.444793	47.111079
2567.999734	213.786396	47.116084
2564.572381	216.958941	47.121089
2560.914484	217.055884	47.126093
2556.905501	213.816500	47.131098
2553.962250	211.423070	47.136103
2550.582085	218.042098	47.141108
2546.786505	208.831084	47.146113
2543.852963	208.660488	47.151117
2540.320662	213.721163	47.156122
2537.364410	207.510547	47.161127
2533.185350	213.858068	47.166132
2529.842677	205.477330	47.171137
2526.138732	209.506620	47.176141
2522.686577	214.695376	47.181146
2519.419824	214.730162	47.186151
2516.068665	213.742050	47.191156
2512.059246	214.870333	47.196161
2509.226422	216.210950	47.201165
2505.336649	208.695878	47.206170
2502.141359	207.776775	47.211175
2498.573472	209.758908	47.216180
2494.449961	212.554820	47.221185
2491.580131	202.065233	47.226189
2487.428941	210.005467	47.231194
2484.896847	205.239669	47.236199
2481.115379	211.236647	47.241204
2477.831809	206.407805	47.246209
2474.690642	191.912597	47.251213
2470.624884	205.121950	47.256218
2467.123197	196.163252	47.261223
2463.756677	204.137386	47.266228
2459.843171	207.511604	47.271233
2456.428491	202.463861	47.276237
2452.716898	204.786675	47.281242
2449.956702	196.331174	47.286247
2446.124262	197.028510	47.291252
2442.613880	201.528338	47.296257
2439.482840	197.363070	47.301261
2435.315947	202.804044	47.306266
2431.964495	195.040539	47.311271
2428.689721	198.103523	47.316276
2425.557777	201.167404	47.321281
2421.700901	195.175583	47.326285
2417.853111	205.340732	47.331290
2414.972974	199.438709	47.336295
2411.486150	196.089582	47.341300
2407.736649	194.991862	47.346305
2404.349509	196.535138	47.351309
2400.493369	192.435122	47.356314
2397.543441	192.026168	47.361319
2394.165906	203.100805	47.366324
2390.450111	199.635167	47.371329
2387.043750	193.848840	47.376333
2382.980378	196.500326	47.381338
2379.871957	196.813171	47.386343
2376.788330	191.943310	47.391348
2372.769480	189.411999	47.396353
2369.511942	188.806375	47.401357
2365.380776	195.163676	47.406362
2362.434115	188.694071	47.411367
2359.232517	200.756185	47.416372
2355.489648	194.344999	47.421377
2351.823917	181.677233	47.426381
2347.817335	189.783137	47.431386
2344.571323	199.650072	47.436391
2341.815830	194.247318	47.441396
2338.390561	186.305246	47.446401
2334.815079	193.316588	47.451405
2331.124217	196.591985	47.456410
2327.743730	189.576540	47.461415
2324.342236	196.675599	47.466420
2320.299276	196.191378	47.471425
2317.084308	187.019313	47.476429
2313.494178	199.110266	47.481434
2310.359821	188.253818	47.486439
2306.482003	192.401949	47.491444
2302.724533	194.733037	47.496449
2299.453218	188.839035	47.501453
2295.931184	190.366763	47.506458
2292.801260	181.899394	47.511463
2288.704888	185.840889	47.516468
2285.477775	189.094223	47.521473
2282.380633	181.721425	47.526477
2278.431623	190.864175	47.531482
2275.307481	184.599760	47.536487
2271.482300	186.321216	47.541492
2268.224119	183.687699	47.546497
2264.695215	183.648319	47.551501
2261.181741	180.964797	47.556506
2257.896334	180.285702	47.561511
2253.912854	187.170073	47.566516
2250.405802	190.680604	47.571521
2247.101130	187.354415	47.576525
2243.274899	192.592276	47.581530
2239.984510	184.887911	47.586535
2236.422936	184.020182	47.591540
2232.939624	185.390201	47.596545
2230.072475	176.410221	47.601549
2226.353889	178.901104	47.606554
2222.843351	184.268409	47.611559
2218.774104	185.145919	47.616564
2215.340005	180.971051	47.621569
2212.100381	172.574745	47.626573
2208.310538	179.944207	47.631578
2205.081518	175.971507	47.636583
2201.844993	180.096321	47.641588
2198.357411	171.722021	47.646593
2194.671742	177.550827	47.651597
2190.724309	177.802019	47.656602
2187.325519	179.877616	47.661607
2184.170727	183.616171	47.666612
2180.607961	188.149881	47.671617
2177.480094	179.048007	47.676621
2173.633613	187.846908	47.681626
2170.461135	174.007561	47.686631
2166.696563	176.475690	47.691636
2163.124850	176.428455	47.696641
2159.418213	178.605222	47.701645
2155.942745	176.777288	47.706650
2152.280050	173.811822	47.711655
2148.817389	173.036956	47.716660
2145.671637	168.028725	47.721665
2142.596727	180.018316	47.726669
2138.773234	173.957097	47.731674
2135.397553	178.194522	47.736679
2131.635234	171.328522	47.741684
2127.720164	183.594989	47.746689
2124.716921	171.014394	47.751693
2121.111690	182.258594	47.756698
2117.957272	170.026605	47.761703
2114.311188	168.374684	47.766708
2110.446245	172.835787	47.771713
2107.119789	169.971523	47.776717
2103.337151	177.011494	47.781722
2100.129823	168.598694	47.786727
2096.539303	178.324316	47.791732
2092.980224	173.461335	47.796737
2089.555635	163.159766	47.801741
2086.343681	178.163881	47.806746
2082.660767	167.165738	47.811751
2079.289491	166.351757	47.816756
2075.807603	166.453545	47.821761
2072.298366	166.299364	47.826765
2068.859940	169.660741	47.831770
2064.981379	168.824568	47.836775
2061.590818	167.283430	47.841780
2057.889210	166.116310	47.846785
2054.758099	156.695781	47.851789
2051.187188	173.966429	47.856794
2047.684992	170.477245	47.861799
2043.987892	164.759726	47.866804
2040.593048	163.702004	47.871809
2036.746806	159.083044	47.876813
2033.407936	165.592343	47.881818
2030.210637	159.333683	47.886823
2026.761252	164.155631	47.891828
2023.260640	161.512793	47.896833
2019.978935	159.438456	47.901837
2015.884062	173.051136	47.906842
2012.538181	168.609852	47.911847
2009.494262	168.124106	47.916852
2005.724350	173.843815	47.921857
2002.220848	163.918060	47.926861
1998.648122	175.083159	47.931866
1994.814598	164.515106	47.936871
1991.595026	173.824714	47.941876
1987.966232	170.240054	47.946881
1985.080959	165.988736	47.951885
1981.398437	171.265408	47.956890
1977.491872	160.308838	47.961895
1974.080117	164.482859	47.966900
1970.627252	174.827178	47.971905
1967.035268	157.641741	47.976909
1963.400502	160.241521	47.981914
1960.170775	166.515767	47.986919
1957.143830	165.976140	47.991924
1952.908426	166.762119	47.996929
1949.690868	166.348109	48.001933
1945.958246	169.091546	48.006938
1942.409934	164.902599	48.011943
1939.057083	163.849657	48.016948
1935.894999	171.956095	48.021953
1932.449322	158.010520	48.026957
1928.765359	164.253639	48.031962
1925.072451	160.958066	48.036967
1921.628271	159.751693	48.041972
1917.937083	167.917901	48.046977
1914.978224	161.077653	48.051981
1911.251856	162.396279	48.056986
1907.620871	166.403295	48.061991
1904.052274	162.225820	48.066996
1900.243500	168.946021	48.072001
1897.256188	163.934295	48.077005
1893.597678	164.616753	48.082010
1890.347780	164.386519	48.087015
1886.842241	158.215384	48.092020
1882.959774	156.260896	48.097025
1879.649108	153.008987	48.102029
1876.152746	160.547076	48.107034
1872.330404	160.254523	48.112039
1869.089662	150.353372	48.117044
1865.557095	148.059305	48.122049
1862.088894	152.172864	48.127053
1858.419051	160.194288	48.132058
1855.361657	162.599320	48.137063
1851.757465	154.555975	48.142068
1847.983767	160.078488	48.147073
1844.347211	161.940998	48.152077
1840.741298	165.198767	48.157082
1837.575787	147.950516	48.162087
1834.404886	166.779106	48.167092
1830.660328	159.599231	48.172097
1827.369308	146.656744	48.177101
1823.413001	160.202852	48.182106
1820.015347	150.415673	48.187111
1816.491210	150.734202	48.192116
1812.705687	155.003223	48.197121
1809.731947	148.077302	48.202125
1806.283125	152.922983	48.207130
1802.693307	150.416020	48.212135
1799.144443	157.441461	48.217140
1795.186923	162.491363	48.222145
1792.151662	154.193057	48.227149
1788.519102	157.356398	48.232154
1784.921114	157.701161	48.237159
1781.692138	159.695701	48.242164
1778.167278	161.196438	48.247169
1774.696363	149.805193	48.252173
1771.243304	158.451555	48.257178
1767.487788	154.384400	48.262183
1764.139516	147.673518	48.267188
1760.497663	157.536687	48.272193
1756.853551	157.817852	48.277197
1753.374005	161.973223	48.282202
1749.567384	156.037240	48.287207
1746.612382	154.587380	48.292212
1743.117040	156.282578	48.297217
1739.705083	158.967867	48.302221
1735.937234	164.816094	48.307226
1732.577992	161.985148	48.312231
1729.101970	154.138989	48.317236
1725.516532	157.585074	48.322241
1722.420467	149.968411	48.327245
1718.579387	151.149450	48.332250
1714.910714	148.983758	48.337255
1711.346638	151.381217	48.342260
1707.672433	154.449868	48.347265
1704.344641	152.656881	48.352269
1700.965773	159.286071	48.357274
1697.596661	151.771566	48.362279
1694.265857	157.058809	48.367284
1690.300021	154.030328	48.372289
1686.946313	146.747531	48.377293
1683.121390	142.891426	48.382298
1679.986943	148.962427	48.387303
1676.817792	151.193232	48.392308
1673.292336	150.870340	48.397313
1669.581086	149.038314	48.402317
1665.942503	155.181369	48.407322
1662.416169	142.452941	48.412327
1659.072293	152.527429	48.417332
1655.411016	147.683270	48.422337
1652.254073	147.508885	48.427341
1648.760572	145.217214	48.432346
1644.939151	148.478564	48.437351
1641.375507	153.944421	48.442356
1637.669251	156.134737	48.447361
1634.468574	146.902843	48.452365
1630.796491	148.254749	48.457370
1627.326974	142.988399	48.462375
1624.152739	152.333144	48.467380
1620.096019	153.845702	48.472385
1617.215000	140.645023	48.477389
1613.395831	147.544550	48.482394
1609.865754	151.888144	48.487399
1606.639019	154.398271	48.492404
1602.954207	156.010027	48.497409
1599.907376	148.411369	48.502413
1596.079364	150.269585	48.507418
1592.326220	141.411404	48.512423
1588.705455	142.003596	48.517428
1585.127210	146.446533	48.522433
1581.871311	148.419012	48.527437
1578.266030	148.681071	48.532442
1574.830825	145.751499	48.537447
1571.481731	143.452406	48.542452
1567.677850	145.208778	48.547457
1564.386271	147.985792	48.552461
1560.925624	151.636539	48.557466
1557.307270	151.478668	48.562471
1554.024691	151.584215	48.567476
1550.496340	150.182848	48.572481
1546.694360	150.611033	48.577485
1543.324001	155.363216	48.582490
1539.839288	156.309485	48.587495
1536.380320	148.494416	48.592500
1532.944898	153.542708	48.597505
1529.395398	154.501861	48.602509
1525.881309	152.085811	48.607514
1522.515437	153.284979	48.612519
1518.745031	145.487646	48.617524
1515.251929	146.118986	48.622529
1511.890187	142.406915	48.627533
1508.032038	150.229599	48.632538
1505.188061	147.754137	48.637543
1501.719204	141.058260	48.642548
1497.296091	148.163451	48.647553
1494.291102	150.288312	48.652557
1490.879551	150.232481	48.657562
1487.572949	151.614679	48.662567
1483.777221	143.965421	48.667572
1479.973480	150.633982	48.672577
1477.257027	154.388151	48.677581
1473.226853	152.197737	48.682586
1469.715995	145.570790	48.687591
1466.043476	148.321036	48.692596
1462.543090	156.051480	48.697601
1459.322045	150.443061	48.702605
1456.017813	144.556136	48.707610
1452.168159	155.007188	48.712615
1449.055939	149.905908	48.717620
1445.562846	152.279795	48.722625
1442.314498	146.649459	48.727629
1438.370851	142.384765	48.732634
1434.937333	147.648104	48.737639
1431.299307	140.812704	48.742644
1427.374402	154.752516	48.747649
1424.078370	136.724815	48.752653
1420.591766	135.918927	48.757658
1416.960453	146.578020	48.762663
1413.912601	145.916695	48.767668
1409.812426	142.389695	48.772673
1406.849104	152.170162	48.777677
1403.006889	155.552556	48.782682
1399.708734	150.841197	48.787687
1396.625688	148.172852	48.792692
1393.021609	150.513023	48.797697
1389.467392	149.813647	48.802701
1385.886510	143.557893	48.807706
1382.349984	148.964985	48.812711
1378.887298	144.227754	48.817716
1375.021298	148.877063	48.822721
1371.826899	146.135180	48.827725
1367.864467	143.237655	48.832730
1364.669773	144.599271	48.837735
1361.361966	141.485412	48.842740
1357.430936	151.506562	48.847745
1354.367200	140.728218	48.852749
1351.185578	145.190623	48.857754
1347.058410	150.065067	48.862759
1343.757219	139.270133	48.867764
1340.018389	138.609006	48.872769
1337.130728	135.967217	48.877773
1333.316911	142.132563	48.882778
1329.650064	146.092643	48.887783
1326.009744	144.026776	48.892788
1322.260047	147.751121	48.897793
1318.915381	144.427499	48.902797
1315.842306	148.233006	48.907802
1312.206618	145.289415	48.912807
1309.152810	142.535588	48.917812
1305.274535	141.488852	48.922817
1301.596846	144.549701	48.927821
1297.923203	149.241277	48.932826
1294.472041	144.321646	48.937831
1291.497087	134.916161	48.942836
1287.329561	145.465060	48.947841
1284.243592	137.510207	48.952845
1280.526709	143.302586	48.957850
1277.353116	137.660418	48.962855
1273.662372	139.879630	48.967860
1270.077343	151.052739	48.972865
1266.533121	139.217816	48.977869
1262.906666	144.885147	48.982874
1259.785726	133.415000	48.987879
1256.219593	134.486040	48.992884
1252.390869	140.008223	48.997889
1249.137575	140.402389	49.002893
1245.569453	138.289528	49.007898
1242.074697	143.735792	49.012903
1238.730754	138.688369	49.017908
1235.234561	148.445716	49.022913
1231.799445	142.286768	49.027917
1227.894830	137.661001	49.032922
1224.467851	139.422832	49.037927
1221.324327	137.039106	49.042932
1217.463657	147.199296	49.047937
1214.114161	141.125667	49.052941
1210.791517	141.207691	49.057946
1207.228462	143.358092	49.062951
1203.890718	134.331940	49.067956
1200.137609	136.153426	49.072961
1196.210995	136.221642	49.077965
1192.626133	140.477697	49.082970
1189.496914	141.644690	49.087975
1186.235463	138.596316	49.092980
1182.665930	132.237038	49.097985
1179.441642	135.733338	49.102989
1175.815414	140.592400	49.107994
1171.776242	137.706159	49.112999
1168.629008	134.707787	49.118004
1164.867882	139.181263	49.123009
1161.577775	134.546317	49.128013
1157.940519	140.579202	49.133018
1154.488356	138.455334	49.138023
1151.204336	134.700501	49.143028
1147.182095	139.576314	49.148033
1144.014815	130.936440	49.153037
1140.507619	144.485333	49.158042
1137.044998	137.327354	49.163047
1133.620898	140.584790	49.168052
1129.910471	141.576774	49.173057
1126.897910	135.488952	49.178061
1123.305055	133.216687	49.183066
1119.257675	139.181245	49.188071
1115.998642	126.776570	49.193076
1112.203227	134.709550	49.198081
1109.155123	128.088495	49.203085
1105.364699	134.550296	49.208090
1101.806686	129.758212	49.213095
1098.419536	129.516301	49.218100
1094.985806	127.907443	49.223105
1091.600075	125.792967	49.228109
1088.393777	131.058835	49.233114
1084.424999	136.112936	49.238119
1080.787870	135.252079	49.243124
1077.400620	135.127023	49.248129
1074.239279	127.652487	49.253133
1070.673407	132.255370	49.258138
1066.996226	140.815708	49.263143
1063.512372	130.618958	49.268148
1059.790667	138.534069	49.273153
1056.546856	130.365334	49.278157
1053.070139	131.851546	49.283162
1049.280707	134.520211	49.288167
1045.774129	136.613640	49.293172
1042.295964	128.877355	49.298177
1038.950042	133.719177	49.303181
1034.992495	126.804154	49.308186
1031.686759	128.996402	49.313191
1028.601888	130.428693	49.318196
1024.980444	129.881225	49.323201
1021.449872	132.326150	49.328205
1017.797158	121.754209	49.333210
1014.471519	140.203420	49.338215
1011.040202	123.334554	49.343220
1007.593683	132.252252	49.348225
1003.926155	124.307354	49.353229
1000.472918	133.005546	49.358234
996.829151	132.998746	49.363239
993.266878	132.577287	49.368244
989.842156	129.803522	49.373249
986.673166	125.923235	49.378253
982.689501	118.166799	49.383258
979.243980	119.657973	49.388263
976.182667	122.374617	49.393268
972.275236	132.447596	49.398273
969.037824	129.950324	49.403277
965.249697	126.453840	49.408282
961.767608	130.999731	49.413287
958.355762	121.613278	49.418292
954.792429	132.327150	49.423297
951.259462	126.381762	49.428301
947.678797	127.581543	49.433306
944.350856	123.871432	49.438311
941.050785	130.247530	49.443316
937.340071	135.524493	49.448321
933.858619	131.744265	49.453325
930.116655	126.441453	49.458330
926.723535	135.879633	49.463335
923.201994	126.486681	49.468340
919.830281	134.052546	49.473345
916.524979	133.143657	49.478349
912.713053	124.521781	49.483354
909.096527	129.515993	49.488359
905.646270	129.112192	49.493364
902.148887	138.209072	49.498369
898.777643	134.429195	49.503373
895.361464	133.134907	49.508378
891.859516	127.532936	49.513383
888.686319	124.982283	49.518388
884.915190	133.359372	49.523393
881.183211	136.024198	49.528397
877.648673	125.220506	49.533402
873.931307	133.120629	49.538407
870.844347	131.287647	49.543412
867.352328	128.325603	49.548417
863.726584	133.757490	49.553421
860.239091	132.983758	49.558426
856.958979	133.661675	49.563431
853.578200	120.267201	49.568436
849.868291	125.507194	49.573441
846.175395	130.779898	49.578445
842.895263	128.353329	49.583450
838.853959	130.076746	49.588455
835.639700	135.310156	49.593460
831.872766	132.146348	49.598465
828.724399	123.158066	49.603469
825.712037	127.995580	49.608474
821.687574	132.097093	49.613479
818.399770	124.646637	49.618484
814.662443	132.093469	49.623489
811.065366	128.487573	49.628493
807.397460	128.437955	49.633498
803.804571	120.478132	49.638503
800.713006	117.536341	49.643508
797.199101	128.655168	49.648513
793.981340	126.703768	49.653517
790.405412	119.308297	49.658522
786.675482	134.106682	49.663527
783.189046	112.858792	49.668532
780.003427	126.162896	49.673537
776.826217	119.429064	49.678541
772.737258	121.022090	49.683546
768.861596	127.826419	49.688551
765.527606	130.221460	49.693556
762.034954	130.588475	49.698561
758.480577	130.209510	49.703565
755.268251	123.506959	49.708570
751.571187	127.835184	49.713575
748.344901	126.106837	49.718580
744.968734	133.776961	49.723585
740.921000	128.439057	49.728589
737.590093	114.289723	49.733594
733.649401	129.167997	49.738599
730.691102	116.667936	49.743604
727.276674	128.585550	49.748609
723.762093	125.784239	49.753613
720.381898	121.180728	49.758618
716.623302	126.466373	49.763623
713.160725	123.499783	49.768628
709.560910	122.709628	49.773633
705.744443	130.991145	49.778637
702.556551	127.083809	49.783642
699.246216	122.666094	49.788647
696.033049	127.711945	49.793652
691.857890	125.593794	49.798657
688.203626	127.908868	49.803661
685.037750	128.028496	49.808666
681.348977	129.422594	49.813671
678.336202	120.914225	49.818676
674.651236	124.614558	49.823681
671.248514	132.322672	49.828685
667.708147	125.382402	49.833690
664.294642	131.184853	49.838695
660.787455	119.422126	49.843700
657.191875	125.399153	49.848705
653.311088	123.151431	49.853709
649.733044	120.275827	49.858714
646.568316	124.847195	49.863719
642.963647	120.980638	49.868724
639.446345	123.590409	49.873729
635.746435	130.969027	49.878733
632.604506	129.928932	49.883738
628.865799	132.157384	49.888743
625.688798	124.944701	49.893748
622.052739	127.435209	49.898753
618.529248	130.279469	49.903757
615.300206	123.781670	49.908762
611.793456	122.155280	49.913767
608.353596	126.730359	49.918772
604.475716	126.536468	49.923777
600.827476	125.384015	49.928781
597.340267	127.464123	49.933786
594.055978	125.255898	49.938791
590.666576	127.509667	49.943796
587.085330	128.551173	49.948801
583.425692	137.042658	49.953805
580.102384	125.889340	49.958810
576.172553	135.938707	49.963815
573.031397	125.898229	49.968820
569.367358	119.862378	49.973825
566.231360	130.890813	49.978829
562.671988	117.828080	49.983834
558.976694	131.585270	49.988839
555.546576	126.828732	49.993844
551.645727	131.479735	49.998849
548.595887	126.748688	50.003853
545.198805	129.477565	50.008858
541.433527	132.172844	50.013863
538.203252	126.829726	50.018868
534.359181	130.839084	50.023873
530.883713	122.600383	50.028877
527.014187	135.771531	50.033882
523.792694	133.398257	50.038887
520.916935	117.613272	50.043892
517.386732	119.627936	50.048897
513.530073	122.734609	50.053901
509.837698	122.430778	50.058906
506.121830	127.552048	50.063911
503.101420	127.524599	50.068916
499.221316	128.011189	50.073921
495.662878	119.788224	50.078925
491.969101	116.416465	50.083930
488.649102	122.619945	50.088935
485.845575	116.224905	50.093940
482.085662	114.024434	50.098945
478.318705	115.731193	50.103949
475.003134	111.935346	50.108954
471.116389	126.964727	50.113959
467.836415	110.463260	50.118964
464.413093	111.765066	50.123969
461.056871	115.970220	50.128973
457.719404	121.338329	50.133978
453.719467	126.446659	50.138983
450.164554	110.618432	50.143988
446.886383	125.314855	50.148993
443.604993	121.110021	50.153997
440.079732	112.899183	50.159002
436.074130	116.956269	50.164007
432.819813	116.739656	50.169012
429.373345	113.631318	50.174017
425.836678	114.651763	50.179021
422.117225	115.121309	50.184026
418.532734	113.058019	50.189031
415.684522	113.780425	50.194036
411.681581	116.425750	50.199041
408.291112	110.480740	50.204045
404.888185	110.378134	50.209050
401.116067	117.967989	50.214055
397.843436	114.625678	50.219060
394.168356	118.287106	50.224065
390.963505	110.626541	50.229069
387.512740	114.496730	50.234074
383.379371	113.634321	50.239079
380.536956	104.531055	50.244084
376.807368	119.113770	50.249089
373.140456	108.356341	50.254093
369.883459	110.796352	50.259098
366.515165	118.941401	50.264103
363.183225	108.453751	50.269108
359.242963	113.094663	50.274113
355.969837	107.544681	50.279117
352.452826	107.965783	50.284122
348.286911	117.018383	50.289127
345.080605	117.822599	50.294132
341.689278	112.442561	50.299137
337.914069	117.203188	50.304141
334.820481	112.747924	50.309146
331.371946	120.704997	50.314151
327.524682	116.987008	50.319156
324.202393	119.920346	50.324161
320.818912	127.452652	50.329165
317.470208	108.167646	50.334170
314.053449	112.690769	50.339175
310.620988	102.688677	50.344180
306.419311	109.190555	50.349185
302.804787	113.220917	50.354189
299.645530	111.735394	50.359194
296.250689	106.797811	50.364199
293.192270	118.062993	50.369204
289.386242	124.552290	50.374209
285.365574	114.485759	50.379213
281.911029	110.964280	50.384218
278.330339	117.331036	50.389223
275.412999	120.352091	50.394228
271.821545	114.745150	50.399233
268.148710	112.520984	50.404237
264.902373	115.266559	50.409242
261.465141	111.903257	50.414247
257.849925	111.374341	50.419252
254.225542	114.768784	50.424257
250.044592	113.880834	50.429261
247.323239	104.729411	50.434266
243.486932	111.271113	50.439271
240.464798	111.706687	50.444276
236.674376	102.243046	50.449281
233.098089	112.330646	50.454285
229.781421	114.636189	50.459290
225.781108	120.972795	50.464295
222.331054	108.786626	50.469300
219.279594	112.140918	50.474305
215.792391	114.360839	50.479309
212.526282	101.687009	50.484314
208.881045	117.012657	50.489319
205.036330	111.198270	50.494324
201.715353	111.258282	50.499329
197.698650	105.346082	50.504333
194.664392	113.858247	50.509338
190.856105	116.205540	50.514343
187.631738	103.239277	50.519348
184.153059	109.199281	50.524353
180.637755	106.771118	50.529357
176.919891	107.756050	50.534362
173.556238	110.118747	50.539367
169.909798	107.089317	50.544372
166.449645	106.159675	50.549377
163.407399	113.059378	50.554381
160.262428	104.701776	50.559386
156.244840	109.286794	50.564391
152.730427	108.939799	50.569396
148.883845	112.829325	50.574401
145.241686	103.471864	50.579405
142.180527	96.258762	50.584410
138.494856	108.587908	50.589415
134.956106	97.531850	50.594420
131.572274	105.656738	50.599425
127.971878	116.100060	50.604429
124.714569	107.837650	50.609434
120.988599	103.760165	50.614439
117.676662	106.031659	50.619444
114.213656	110.709602	50.624449
110.282436	113.836662	50.629453
106.817176	109.207098	50.634458
103.186716	109.710926	50.639463
100.094551	99.139616	50.644468
96.756031	103.290600	50.649473
93.079009	107.677602	50.654477
89.552105	97.534865	50.659482
85.615086	100.718158	50.664487
82.605627	99.131828	50.669492
79.082442	102.068219	50.674497
75.159652	102.924170	50.679501
71.929347	105.476408	50.684506
68.125590	112.784642	50.689511
64.835774	107.556558	50.694516
61.715296	108.970745	50.699521
58.236039	103.551244	50.704525
54.766758	92.074295	50.709530
50.680794	114.196012	50.714535
47.259011	102.596744	50.719540
43.726447	105.828153	50.724545
40.574536	110.702495	50.729549
37.194947	101.331065	50.734554
33.773550	107.460877	50.739559
30.190269	107.409352	50.744564
26.492657	111.291879	50.749569
22.715723	106.030035	50.754573
19.809806	107.945869	50.759578
15.726326	107.119566	50.764583
12.217738	100.266986	50.769588
8.785963	99.231346	50.774593
5.462880	106.520421	50.779597
2.310268	110.017707	50.784602