Tue Jun 21 13:12:57 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.241303	102.431701	0.000000
0.215551	89.086153	0.005005
0.246780	87.186614	0.010010
-0.267727	77.183942	0.015014
-0.246602	68.545351	0.020019
-0.558254	76.486406	0.025024
-0.752862	58.234117	0.030029
-0.933995	55.674541	0.035034
-1.176593	55.812631	0.040038
-1.149512	44.540242	0.045043
-2.096912	36.974718	0.050048
-1.954695	28.601244	0.055053
-1.889157	38.307322	0.060058
-2.436512	25.679275	0.065062
-2.815800	17.874448	0.070067
-3.410394	18.987635	0.075072
-3.955672	13.445293	0.080077
-4.154195	2.410389	0.085082
-4.627461	18.773117	0.090086
-4.450596	21.166923	0.095091
-4.512781	32.030590	0.100096
-4.624932	16.985571	0.105101
-5.071477	17.148356	0.110106
-5.597781	27.280597	0.115110
-5.938829	22.578816	0.120115
-6.365163	19.605195	0.125120
-6.407735	19.603997	0.130125
-6.197192	18.580138	0.135130
-6.619833	22.792188	0.140134
-6.169149	20.271257	0.145139
-7.044813	18.131973	0.150144
-7.476675	12.353981	0.155149
-7.726106	24.456327	0.160154
-8.176096	22.822569	0.165158
-8.112226	18.116884	0.170163
-7.989754	20.481019	0.175168
-8.561776	18.736046	0.180173
-9.049786	12.082708	0.185178
-9.444672	23.780138	0.190182
-9.516831	15.567478	0.195187
-9.728489	26.361369	0.200192
-9.611279	16.564929	0.205197
-9.912575	20.983818	0.210202
-10.602564	27.038241	0.215206
-10.820843	18.468726	0.220211
-10.778036	20.752320	0.225216
-10.800317	20.365329	0.230221
-11.444771	27.090644	0.235226
-12.255400	28.702749	0.240230
-12.132137	24.111152	0.245235
-12.530839	22.429632	0.250240
-12.705140	23.916433	0.255245
-12.993093	19.629536	0.260250
-12.839808	24.187057	0.265254
-12.619785	21.249272	0.270259
-13.024472	27.358867	0.275264
-13.646656	23.680441	0.280269
-14.068392	13.449331	0.285274
-14.411910	17.628545	0.290278
-14.210655	12.129525	0.295283
-14.702122	20.964449	0.300288
-14.818365	16.603140	0.305293
-15.564584	20.658021	0.310298
-16.039927	18.808042	0.315302
-16.204132	21.297597	0.320307
-15.961664	22.367286	0.325312
-16.060760	14.074235	0.330317
-16.118577	12.892746	0.335322
-16.277667	22.011451	0.340326
-16.468666	4.709975	0.345331
-17.380501	15.600862	0.350336
-17.533113	18.739103	0.355341
-17.478854	13.893721	0.360346
-18.346934	19.203495	0.365350
-17.521272	11.150593	0.370355
-18.665373	15.154344	0.375360
-19.050304	10.205275	0.380365
-18.953915	12.137030	0.385370
-19.423795	23.111221	0.390374
-19.601253	22.042685	0.395379
-19.419838	22.631717	0.400384
-19.657098	18.875343	0.405389
-20.311186	9.895326	0.410394
-21.118163	15.943465	0.415398
-20.631064	15.060881	0.420403
-21.067918	26.486431	0.425408
-21.026240	29.198623	0.430413
-21.078684	15.085002	0.435418
-21.958249	19.613069	0.440422
-22.052281	17.710997	0.445427
-22.613047	19.751971	0.450432
-22.740095	21.227592	0.455437
-22.524067	15.695144	0.460442
-22.546714	23.532664	0.465446
-22.563342	17.137917	0.470451
-23.403861	17.470531	0.475456
-23.535930	9.621221	0.480461
-23.510890	4.313198	0.485466
-24.116446	19.271115	0.490470
-24.421617	14.583131	0.495475
-25.263598	22.895350	0.500480
-25.512572	21.245277	0.505485
-25.350131	19.261661	0.510490
-25.108570	29.034683	0.515494
-24.985332	31.816447	0.520499
-25.753920	26.059484	0.525504
-26.338879	27.393869	0.530509
-26.649018	26.404137	0.535514
-26.924004	25.829693	0.540518
-26.670237	18.063300	0.545523
-26.859034	23.323340	0.550528
-27.884382	19.064035	0.555533
-28.032168	16.502892	0.560538
-28.306423	20.894215	0.565542
-28.472046	13.090716	0.570547
-28.848187	18.178723	0.575552
-28.477197	18.423587	0.580557
-28.532849	23.872528	0.585562
-28.706612	22.332150	0.590566
-29.039772	15.014601	0.595571
-29.675745	29.761683	0.600576
-29.735204	18.934820	0.605581
-30.594488	25.069375	0.610586
-31.338513	22.709977	0.615590
-30.808819	26.255400	0.620595
-30.621564	23.409670	0.625600
-31.253932	34.300664	0.630605
-31.108800	17.640692	0.635610
-31.436378	24.237361	0.640614
-31.975195	30.448695	0.645619
-32.790557	33.949870	0.650624
-33.054330	35.889963	0.655629
-33.018828	24.632182	0.660634
-32.971678	26.716540	0.665638
-32.955874	27.414495	0.670643
-33.255357	24.035663	0.675648
-33.269075	30.485639	0.680653
-33.877732	23.676653	0.685658
-34.413231	27.110367	0.690662
-34.384919	23.231870	0.695667
-34.511066	28.786615	0.700672
-34.742860	22.212405	0.705677
-35.428534	20.286358	0.710682
-36.371497	27.696520	0.715686
-36.523326	21.687255	0.720691
-35.540374	29.169006	0.725696
-36.085886	24.778341	0.730701
-36.028749	17.480222	0.735706
-36.384032	27.092389	0.740710
-36.920944	19.898170	0.745715
-37.756299	26.892491	0.750720
-38.131718	22.932065	0.755725
-37.830649	24.298309	0.760730
-38.117609	27.516225	0.765734
-37.837913	21.970271	0.770739
-38.150157	21.007726	0.775744
-38.574987	23.226484	0.780749
-39.052323	8.840467	0.785754
-39.639992	25.850651	0.790758
-39.768908	13.563388	0.795763
-39.527707	24.807779	0.800768
-39.676268	25.673455	0.805773
-39.746742	20.998108	0.810778
-40.806853	25.121157	0.815782
-40.915619	20.323096	0.820787
-41.116838	29.732940	0.825792
-41.198463	25.660713	0.830797
-41.315971	17.495624	0.835802
-41.882284	28.037249	0.840806
-42.391580	15.766406	0.845811
-42.725388	23.210665	0.850816
-42.735049	26.709640	0.855821
-42.751314	26.476758	0.860826
-43.178921	31.324455	0.865830
-42.973534	17.596153	0.870835
-42.876364	28.867162	0.875840
-43.200224	24.114192	0.880845
-43.587243	14.745999	0.885850
-44.156719	24.980899	0.890854
-44.400087	25.420840	0.895859
-45.351277	16.301180	0.900864
-45.904996	21.518644	0.905869
-45.067375	15.588047	0.910874
-45.525374	26.877584	0.915878
-45.818505	12.312074	0.920883
-46.160731	18.464602	0.925888
-46.134567	20.713852	0.930893
-45.902893	15.711020	0.935898
-46.644314	15.257827	0.940902
-46.974448	23.217109	0.945907
-47.437150	20.558343	0.950912
-47.228853	16.470272	0.955917
-47.167231	14.191566	0.960922
-48.184294	24.719232	0.965926
-48.562511	11.934537	0.970931
-49.077178	26.680669	0.975936
-49.421124	24.906810	0.980941
-48.844122	15.467772	0.985946
-49.213339	17.161097	0.990950
-49.108579	25.871436	0.995955
-49.747187	24.916566	1.000960
-50.408635	26.308021	1.005965
-50.438443	19.124152	1.010970
-50.706460	29.771680	1.015974
-50.591481	21.718851	1.020979
-50.647594	32.987225	1.025984
-50.950239	21.031042	1.030989
-51.605476	21.005406	1.035994
-52.196943	30.099419	1.040998
-52.000248	32.080670	1.046003
-52.254479	18.650286	1.051008
-52.419084	23.076929	1.056013
-52.174187	19.109878	1.061018
-53.435103	27.959752	1.066022
-53.356646	28.280884	1.071027
-53.556518	26.407785	1.076032
-53.806132	28.027630	1.081037
-53.308227	23.087858	1.086042
-54.526860	33.052967	1.091046
-54.779501	23.927141	1.096051
-55.220233	24.748061	1.101056
-55.219261	23.316485	1.106061
-55.206317	21.636260	1.111066
-55.478493	21.666574	1.116070
-55.266256	22.135454	1.121075
-56.085211	21.347007	1.126080
-56.642159	18.412980	1.131085
-56.658987	14.244187	1.136090
-57.035390	24.616819	1.141094
-56.889336	16.431764	1.146099
-57.026129	13.863870	1.151104
-57.434392	15.649502	1.156109
-58.177114	17.245829	1.161114
-58.719024	16.453534	1.166118
-58.548208	16.426667	1.171123
-58.492994	13.628261	1.176128
-59.014089	9.091086	1.181133
-58.735758	6.199492	1.186138
-59.051351	23.786806	1.191142
-59.263372	14.457715	1.196147
-59.661577	22.095566	1.201152
-60.145571	18.847342	1.206157
-60.341733	13.282122	1.211162
-60.469394	23.075827	1.216166
-60.416407	13.749420	1.221171
-61.306791	11.020194	1.226176
-61.720993	25.334300	1.231181
-61.600683	8.234453	1.236186
-62.134028	21.952609	1.241190
-61.948481	13.655640	1.246195
-62.117397	17.282218	1.251200
-62.181039	12.811759	1.256205
-62.599879	15.309541	1.261210
-63.249380	20.397434	1.266214
-63.314010	13.910593	1.271219
-63.739582	18.626922	1.276224
-63.915611	24.408767	1.281229
-63.525831	17.467988	1.286234
-64.150830	17.698615	1.291238
-64.777895	23.937981	1.296243
-64.954677	26.069289	1.301248
-65.082232	23.251619	1.306253
-64.915115	17.958742	1.311258
-65.453295	23.685911	1.316262
-66.022139	21.893060	1.321267
-66.430622	18.296273	1.326272
-66.678934	21.165613	1.331277
-66.591499	13.304817	1.336282
-66.796844	19.428165	1.341286
-67.008237	16.828028	1.346291
-66.791227	18.029012	1.351296
-67.487404	22.312413	1.356301
-67.868232	8.440656	1.361306
-68.461152	17.586209	1.366310
-68.480494	16.270478	1.371315
-68.263120	14.361434	1.376320
-68.677053	13.600634	1.381325
-69.066550	17.660184	1.386330
-69.598373	19.204024	1.391334
-69.676817	12.570288	1.396339
-69.822879	16.716803	1.401344
-69.916289	18.065888	1.406349
-69.984095	13.202638	1.411354
-70.670265	21.826892	1.416358
-71.173511	14.258094	1.421363
-71.580521	12.600849	1.426368
-71.824166	15.117175	1.431373
-71.491710	14.831474	1.436378
-71.744907	17.127383	1.441382
-71.841811	13.551813	1.446387
-71.700978	15.493374	1.451392
-72.724265	23.537652	1.456397
-73.045833	12.525301	1.461402
-73.389475	21.863611	1.466406
-73.323488	10.081810	1.471411
-73.431167	11.653877	1.476416
-73.526373	21.477527	1.481421
-74.339466	9.386262	1.486426
-74.768376	6.107411	1.491430
-74.818597	7.500255	1.496435
-75.020647	13.758425	1.501440
-75.007621	15.144742	1.506445
-75.138112	17.744745	1.511450
-75.166985	20.011397	1.516454
-75.919351	11.422997	1.521459
-76.249876	15.589602	1.526464
-76.818910	19.888848	1.531469
-76.429409	15.561792	1.536474
-76.669784	21.119663	1.541478
-76.519730	24.736239	1.546483
-77.096189	20.804771	1.551488
-77.921303	18.011064	1.556493
-77.441832	15.023404	1.561498
-78.246214	12.121283	1.566502
-78.018430	14.543551	1.571507
-78.497253	16.635686	1.576512
-79.389337	21.418817	1.581517
-79.297098	14.574873	1.586522
-79.659962	16.644843	1.591526
-79.414447	9.446760	1.596531
-79.661820	9.963339	1.601536
-79.777344	16.081480	1.606541
-80.541611	16.294918	1.611546
-80.790971	23.977383	1.616550
-81.282969	16.020741	1.621555
-81.151690	15.180107	1.626560
-81.215455	18.573389	1.631565
-81.168850	16.990598	1.636570
-81.681167	20.978730	1.641574
-82.242498	25.452527	1.646579
-82.623696	26.566299	1.651584
-82.815963	35.261303	1.656589
-82.557982	19.067890	1.661594
-83.067848	34.680116	1.666598
-83.240272	25.447078	1.671603
-83.780116	28.991628	1.676608
-84.205523	24.273438	1.681613
-84.252378	23.447308	1.686618
-84.397130	26.584644	1.691622
-84.960300	24.916557	1.696627
-84.656423	25.094585	1.701632
-85.058850	32.511338	1.706637
-84.753938	16.430135	1.711642
-85.395440	19.427344	1.716646
-85.820345	19.703374	1.721651
-86.252762	26.253077	1.726656
-86.329367	29.621058	1.731661
-86.438448	17.041224	1.736666
-86.856072	24.174160	1.741670
-87.287549	18.764733	1.746675
-87.301078	24.933078	1.751680
-87.849470	22.287325	1.756685
-87.759136	11.934130	1.761690
-87.581691	24.177117	1.766694
-88.506676	19.478914	1.771699
-88.597345	25.313716	1.776704
-88.951763	25.156569	1.781709
-89.081282	10.330727	1.786714
-89.027554	11.686228	1.791718
-89.654884	6.329173	1.796723
-90.562323	16.263261	1.801728
-90.581410	20.313564	1.806733
-90.465663	15.528646	1.811738
-90.820433	13.357184	1.816742
-90.577287	21.859498	1.821747
-90.591422	11.061057	1.826752
-91.412445	23.568663	1.831757
-92.005715	7.498680	1.836762
-92.206699	22.072087	1.841766
-92.454752	24.604932	1.846771
-92.606419	20.665275	1.851776
-92.668331	21.896665	1.856781
-92.932574	21.175999	1.861786
-92.831613	18.031985	1.866790
-93.214527	23.699698	1.871795
-93.362946	20.588104	1.876800
-94.181381	22.806539	1.881805
-94.160894	23.744859	1.886810
-94.180504	24.117159	1.891814
-94.147475	22.339480	1.896819
-94.956543	9.732910	1.901824
-95.610729	24.661195	1.906829
-96.087748	22.179248	1.911834
-96.093359	27.529521	1.916838
-95.878004	20.642294	1.921843
-95.459074	19.565173	1.926848
-95.828193	24.779104	1.931853
-96.635164	13.157468	1.936858
-97.285925	20.671387	1.941862
-97.504183	22.144552	1.946867
-97.406706	21.720561	1.951872
-97.725022	21.183885	1.956877
-97.209388	7.072499	1.961882
-97.841898	23.981967	1.966886
-98.606954	21.682305	1.971891
-98.807354	19.734114	1.976896
-99.441305	32.129443	1.981901
-99.380856	26.170668	1.986906
-99.336323	23.887688	1.991910
-99.056626	29.046853	1.996915
-99.752315	28.522354	2.006912
-99.679324	28.972103	2.016909
-98.982245	18.517075	2.026906
-99.214525	27.746321	2.036902
-98.158752	25.422407	2.046899
-97.705239	18.517038	2.056896
-96.581480	26.076758	2.066893
-96.410065	22.578843	2.076890
-96.276888	20.417605	2.086886
-96.139350	26.359425	2.096883
-94.989991	24.886031	2.106880
-94.749614	25.307662	2.116877
-93.855147	24.396330	2.126874
-93.579990	27.124547	2.136870
-93.295766	23.150143	2.146867
-92.890468	25.362250	2.156864
-91.987709	27.251310	2.166861
-91.452106	20.387867	2.176858
-91.029126	23.636544	2.186854
-90.309121	25.506870	2.196851
-90.120727	22.195035	2.206848
-89.998602	29.112123	2.216845
-89.287186	27.693082	2.226842
-88.838111	29.146323	2.236838
-87.580633	32.781980	2.246835
-87.342040	36.561089	2.256832
-87.252439	25.924709	2.266829
-86.918454	30.036362	2.276826
-86.142649	29.894521	2.286822
-85.779360	31.183946	2.296819
-84.852743	32.479857	2.306816
-84.280250	31.477612	2.316813
-84.273289	29.647288	2.326810
-83.891944	25.331375	2.336806
-83.204135	25.181189	2.346803
-82.766784	22.676754	2.356800
-81.242376	23.932939	2.366797
-81.670755	18.760236	2.376794
-81.185390	23.783176	2.386790
-80.911317	22.429453	2.396787
-79.634586	17.450545	2.406784
-79.630936	23.515900	2.416781
-79.580672	17.159226	2.426778
-78.238439	21.045415	2.436774
-78.203981	25.846060	2.446771
-77.651040	16.123843	2.456768
-77.145659	15.782771	2.466765
-76.641796	15.185287	2.476762
-76.285023	10.387388	2.486758
-75.313017	19.746760	2.496755
-75.088422	21.735095	2.506752
-74.594763	20.297585	2.516749
-74.102104	19.096949	2.526746
-73.777325	26.324078	2.536742
-72.728250	27.031849	2.546739
-72.116166	20.794141	2.556736
-72.097417	22.853119	2.566733
-72.018031	15.550127	2.576730
-71.090651	20.922304	2.586726
-70.497915	25.138109	2.596723
-70.021157	20.544398	2.606720
-69.266480	22.787956	2.616717
-69.035097	24.099819	2.626714
-69.033589	26.054957	2.636710
-67.808269	26.827198	2.646707
-67.195661	25.257958	2.656704
-67.192383	23.572878	2.666701
-66.636623	18.269397	2.676698
-65.937172	24.254496	2.686694
-65.662777	26.287142	2.696691
-65.025699	20.278248	2.706688
-64.256411	18.330175	2.716685
-63.939195	17.534995	2.726682
-63.721866	20.640498	2.736678
-63.046614	19.171336	2.746675
-62.418912	16.508530	2.756672
-62.241800	13.705571	2.766669
-61.261168	14.595393	2.776666
-61.120540	18.778585	2.786662
-60.896153	27.187504	2.796659
-59.827741	27.504018	2.806656
-59.328463	30.413455	2.816653
-59.120902	28.498341	2.826650
-58.578619	22.224574	2.836646
-57.822998	25.674634	2.846643
-57.737383	23.976906	2.856640
-56.426499	24.129380	2.866637
-56.574486	23.580967	2.876634
-56.267087	21.050043	2.886630
-55.560632	23.843962	2.896627
-54.817585	21.417138	2.906624
-54.675713	25.002033	2.916621
-54.362343	24.304506	2.926618
-53.031025	26.800323	2.936614
-52.890669	18.290652	2.946611
-52.742279	19.040100	2.956608
-52.026063	16.983254	2.966605
-51.912377	20.096042	2.976602
-50.798450	19.986731	2.986598
-50.546299	19.617060	2.996595
-50.245574	26.574520	3.006592
-48.951821	19.824209	3.016589
-48.728869	23.076379	3.026586
-48.855974	15.508437	3.036582
-48.035185	19.763142	3.046579
-47.365366	26.939457	3.056576
-47.175397	26.750798	3.066573
-46.796893	20.147908	3.076570
-45.970651	19.674867	3.086566
-45.641786	17.594045	3.096563
-44.565022	19.478208	3.106560
-44.285786	16.786964	3.116557
-43.899184	18.076483	3.126554
-43.968174	18.410644	3.136550
-42.847613	16.325961	3.146547
-42.702178	16.446588	3.156544
-41.849571	23.718298	3.166541
-40.610505	18.355207	3.176538
-41.163046	18.818645	3.186534
-41.076585	16.172169	3.196531
-39.935310	19.837159	3.206528
-39.094137	19.823800	3.216525
-38.989193	14.763519	3.226522
-38.794349	14.560420	3.236518
-37.663284	17.084266	3.246515
-37.326736	19.702737	3.256512
-37.273143	18.234968	3.266509
-36.410940	19.965773	3.276506
-35.983323	19.916970	3.286502
-35.532946	21.531627	3.296499
-34.798581	25.674984	3.306496
-34.414750	18.399815	3.316493
-34.226533	21.207045	3.326490
-33.207246	13.039663	3.336486
-32.874243	19.122004	3.346483
-32.660367	21.443469	3.356480
-31.607711	20.311331	3.366477
-31.244827	21.752573	3.376474
-31.483660	20.300233	3.386470
-30.412996	27.722556	3.396467
-29.451520	23.687768	3.406464
-29.595603	20.068224	3.416461
-29.423157	21.826712	3.426458
-28.464405	12.969902	3.436454
-27.995683	21.690064	3.446451
-27.178852	23.457232	3.456448
-26.735204	14.509673	3.466445
-26.821892	18.615911	3.476442
-26.060842	24.932444	3.486438
-25.458400	30.358644	3.496435
-25.027656	24.654020	3.506432
-24.014643	17.117383	3.516429
-23.896996	15.858129	3.526426
-23.555202	22.405319	3.536422
-23.065560	24.082236	3.546419
-22.187825	17.744624	3.556416
-21.847835	24.792599	3.566413
-21.691732	19.973000	3.576410
-20.752774	16.219948	3.586406
-20.263450	21.589597	3.596403
-20.171158	25.160379	3.606400
-18.981944	30.946625	3.616397
-18.638839	26.884425	3.626394
-18.849926	25.276533	3.636390
-18.150658	25.120705	3.646387
-17.235583	31.989280	3.656384
-17.054671	17.741516	3.666381
-16.012353	24.741554	3.676378
-15.542709	22.520055	3.686374
-15.446063	25.894900	3.696371
-15.350868	23.790337	3.706368
-14.342047	20.132610	3.716365
-13.611259	22.797041	3.726362
-13.688038	16.998637	3.736358
-12.897853	25.651346	3.746355
-12.209790	14.995885	3.756352
-12.032048	20.596540	3.766349
-11.570205	23.811130	3.776346
-10.743022	21.211718	3.786342
-10.291967	25.102060	3.796339
-9.975025	26.154556	3.806336
-9.250047	18.453212	3.816333
-9.018218	26.571246	3.826330
-8.544555	25.007635	3.836326
-7.848458	19.164035	3.846323
-7.368143	20.963815	3.856320
-7.052330	18.296351	3.866317
-5.726141	12.171376	3.876314
-5.859385	17.691541	3.886310
-5.603992	23.068516	3.896307
-4.908196	10.980070	3.906304
-4.327472	17.752264	3.916301
-4.307930	17.340499	3.926298
-3.416999	32.749774	3.936294
-3.306830	40.922145	3.946291
-2.664157	45.986433	3.956288
-2.234620	49.236807	3.966285
-1.705785	61.373188	3.976282
-1.411016	81.008220	3.986278
-0.948022	95.960669	3.996275
-0.065603	118.855834	4.006272
0.000000	121.465997	4.011277
0.177290	139.520618	4.016282
0.358273	144.950546	4.021286
0.343158	146.165513	4.026291
0.544873	150.860292	4.031296
1.085728	143.078660	4.036301
0.219013	144.897790	4.041306
0.521602	159.083658	4.046310
0.793651	163.621950	4.051315
0.922592	173.449632	4.056320
1.506935	168.162600	4.061325
1.078244	174.163548	4.066330
1.271181	165.956243	4.071334
1.109023	153.816447	4.076339
0.771650	152.152777	4.081344
0.912435	137.325449	4.086349
0.602318	152.843942	4.091354
1.055172	171.028004	4.096358
1.202750	170.193742	4.101363
0.870426	179.733727	4.106368
1.104118	171.768312	4.111373
0.977191	181.982127	4.116378
1.093062	172.307368	4.121382
1.227177	179.409591	4.126387
1.065398	177.879248	4.131392
1.145389	173.039223	4.136397
1.013042	178.361601	4.141402
1.250853	181.732214	4.146406
1.183711	173.259142	4.151411
1.104467	178.970160	4.156416
1.415300	177.471866	4.161421
0.723603	165.275497	4.166426
1.342017	174.191937	4.171430
1.145261	175.168807	4.176435
1.307003	183.869213	4.181440
1.547824	177.246074	4.186445
0.890200	179.890374	4.191450
1.396741	182.559755	4.196454
1.497399	182.834788	4.201459
1.091996	188.381763	4.206464
1.335665	180.000288	4.211469
1.463179	185.918609	4.216474
1.301375	181.549996	4.221478
1.326369	171.843321	4.226483
1.178680	187.309692	4.231488
1.089703	172.616479	4.236493
0.824649	179.612725	4.241498
1.208007	182.945423	4.246502
1.518806	173.829996	4.251507
1.183015	178.716800	4.256512
1.111489	183.596746	4.261517
1.109003	182.932178	4.266522
0.949694	173.825727	4.271526
1.593990	188.904023	4.276531
1.547474	200.309069	4.281536
1.549747	185.722884	4.286541
1.304023	179.087170	4.291546
1.335912	187.692653	4.296550
1.794380	198.972242	4.301555
1.852875	204.015173	4.306560
1.575837	186.347077	4.311565
1.442009	188.482344	4.316570
1.149078	182.751730	4.321574
1.356692	187.457778	4.326579
1.623497	200.263329	4.331584
1.629591	209.605013	4.336589
1.838085	218.091086	4.341594
1.703217	215.410157	4.346598
1.832065	214.515255	4.351603
1.459066	207.712149	4.356608
2.087243	199.604041	4.361613
1.697185	198.834929	4.366618
1.438135	189.702756	4.371622
1.836631	196.942755	4.376627
1.621218	202.221472	4.381632
1.893509	200.323442	4.386637
1.874779	201.583215	4.391642
1.573226	198.051748	4.396646
1.837862	196.247537	4.401651
1.670388	208.777894	4.406656
1.978700	204.709522	4.411661
1.460130	206.288080	4.416666
1.649021	206.767150	4.421670
1.902366	203.539058	4.426675
1.552057	205.816341	4.431680
1.891734	205.671134	4.436685
1.719051	212.354122	4.441690
1.802285	200.044401	4.446694
2.002117	203.758750	4.451699
1.892920	216.825492	4.456704
2.110847	206.226858	4.461709
2.180953	216.044378	4.466714
1.873190	216.169777	4.471718
2.364429	202.723917	4.476723
2.042094	211.825564	4.481728
2.025216	210.279116	4.486733
1.693629	210.072002	4.491738
1.881742	207.897038	4.496742
2.055968	202.796901	4.501747
1.619166	207.344644	4.506752
1.888580	202.775956	4.511757
1.706592	216.846165	4.516762
1.692287	212.998555	4.521766
1.967592	218.037556	4.526771
2.128693	212.691538	4.531776
2.029537	204.153895	4.536781
2.114327	209.937612	4.541786
1.831672	220.592829	4.546790
2.051905	219.920189	4.551795
2.296490	232.200980	4.556800
2.126962	221.959341	4.561805
2.080533	231.314078	4.566810
2.183224	240.972099	4.571814
2.480086	247.862499	4.576819
2.039018	240.018257	4.581824
2.283615	238.861069	4.586829
2.228884	237.467508	4.591834
2.395731	238.754176	4.596838
2.417120	232.591819	4.601843
2.214549	231.513021	4.606848
1.895080	226.685649	4.611853
2.430906	239.312101	4.616858
2.316892	243.379763	4.621862
2.599394	241.671651	4.626867
2.495444	231.128273	4.631872
2.587940	221.402890	4.636877
2.430453	219.439667	4.641882
2.238243	210.330355	4.646886
2.177635	211.770324	4.651891
2.244389	236.891601	4.656896
2.556648	236.432237	4.661901
2.527556	254.669367	4.666906
2.433089	247.334674	4.671910
2.664856	238.774181	4.676915
2.032875	236.749616	4.681920
2.455088	240.652114	4.686925
2.506719	250.022197	4.691930
2.456888	252.068970	4.696934
2.520770	243.836226	4.701939
2.136593	250.132545	4.706944
2.148207	236.093952	4.711949
2.447159	242.054355	4.716954
2.421679	242.036512	4.721958
2.647017	244.175656	4.726963
2.617132	243.163180	4.731968
2.680830	232.972307	4.736973
2.556638	239.998337	4.741978
2.891639	244.386318	4.746982
2.844216	243.104225	4.751987
2.662462	249.147784	4.756992
2.702447	240.694232	4.761997
2.580414	239.335496	4.767002
2.276835	245.263459	4.772006
2.396870	246.856844	4.777011
2.131781	248.470589	4.782016
2.638111	246.672920	4.787021
2.437967	257.574193	4.792026
2.787072	266.475490	4.797030
2.921182	268.792744	4.802035
2.993696	273.045609	4.807040
2.870263	265.819305	4.812045
3.022758	272.555626	4.817050
2.752199	256.891314	4.822054
2.775123	255.113900	4.827059
2.915104	272.822215	4.832064
2.738237	266.030019	4.837069
2.716601	272.970409	4.842074
2.949643	271.425787	4.847078
3.147652	275.349633	4.852083
2.713498	274.283131	4.857088
2.848697	270.156778	4.862093
2.867873	266.389254	4.867098
3.045627	269.366870	4.872102
3.204248	273.213172	4.877107
2.936859	282.144340	4.882112
2.934360	269.994986	4.887117
2.916843	268.137833	4.892122
2.852193	271.547303	4.897126
3.029281	269.141693	4.902131
3.073327	268.594921	4.907136
3.085402	263.444062	4.912141
3.001446	276.611657	4.917146
2.872360	276.033170	4.922150
2.982625	272.938475	4.927155
2.842187	271.664481	4.932160
3.304874	272.085585	4.937165
3.169976	278.713997	4.942170
3.050937	280.489057	4.947174
3.324016	275.484219	4.952179
3.087486	276.963193	4.957184
3.397352	273.100960	4.962189
3.110515	276.347321	4.967194
2.969285	275.954170	4.972198
3.186364	272.394426	4.977203
3.043064	285.683154	4.982208
3.087554	279.350796	4.987213
3.352397	274.681018	4.992218
3.064211	276.457446	4.997222
3.151791	276.097842	5.002227
3.408946	276.046418	5.007232
3.131095	286.129397	5.012237
2.901842	276.264264	5.017242
3.149201	277.634496	5.022246
3.324529	277.896376	5.027251
3.176123	293.169385	5.032256
3.278036	306.242684	5.037261
3.445788	313.511279	5.042266
3.495083	307.247971	5.047270
3.912416	301.294123	5.052275
3.893599	290.221756	5.057280
3.768285	279.773842	5.062285
3.499546	270.935874	5.067290
3.410687	277.152123	5.072294
3.591020	266.316160	5.077299
3.386727	281.904677	5.082304
3.577026	273.224342	5.087309
3.441441	265.237148	5.092314
3.795279	281.349327	5.097318
3.817432	277.226299	5.102323
3.436078	285.632481	5.107328
3.886218	268.955275	5.112333
3.543571	287.098337	5.117338
3.287346	284.227723	5.122342
3.505075	272.652260	5.127347
3.175013	276.202573	5.132352
3.102769	265.234385	5.137357
3.305728	276.037740	5.142362
3.207168	281.933544	5.147366
3.554743	285.805195	5.152371
3.545200	305.099832	5.157376
3.979118	302.777984	5.162381
4.009817	307.753721	5.167386
3.610164	302.982820	5.172390
3.819052	303.845362	5.177395
3.581043	311.399796	5.182400
3.642175	306.695463	5.187405
3.700071	311.048245	5.192410
3.557369	307.772047	5.197414
3.737530	309.340090	5.202419
3.618352	306.849148	5.207424
3.578465	311.085116	5.212429
3.635402	316.571363	5.217434
3.705766	307.146189	5.222438
4.005951	301.976025	5.227443
3.830070	307.428399	5.232448
3.822086	305.506910	5.237453
3.723587	317.061944	5.242458
3.891284	318.980746	5.247462
3.738427	309.041569	5.252467
3.557507	315.419304	5.257472
3.704516	309.058512	5.262477
3.814010	306.493196	5.267482
3.941699	311.190415	5.272486
3.843685	308.588814	5.277491
3.660332	311.941974	5.282496
4.091797	321.963958	5.287501
3.991355	338.380530	5.292506
4.049359	337.137804	5.297510
4.244886	331.082537	5.302515
3.971819	338.069328	5.307520
4.029379	326.633619	5.312525
3.977249	330.884842	5.317530
3.752578	336.763660	5.322534
4.018261	333.060481	5.327539
3.932657	342.653643	5.332544
4.233392	337.927977	5.337549
4.327207	350.810251	5.342554
4.163231	347.812064	5.347558
4.416569	337.569196	5.352563
4.086889	338.938883	5.357568
4.111087	350.571109	5.362573
4.299467	342.242905	5.367578
3.918323	334.032696	5.372582
4.133771	336.459827	5.377587
4.235946	340.190973	5.382592
4.199841	340.293884	5.387597
4.104525	339.676452	5.392602
3.955135	346.851549	5.397606
4.164514	342.816890	5.402611
3.928196	340.459795	5.407616
4.176229	334.419118	5.412621
4.170327	340.527130	5.417626
4.051617	342.120987	5.422630
4.193515	336.795077	5.427635
3.819965	345.518699	5.432640
4.169619	359.343920	5.437645
4.546395	357.003110	5.442650
4.649806	367.169630	5.447654
4.813490	359.193018	5.452659
4.231716	359.695318	5.457664
4.457883	358.666088	5.462669
4.577450	362.888098	5.467674
4.378777	365.484846	5.472678
4.692462	364.786464	5.477683
4.426599	360.858124	5.482688
4.382316	338.520392	5.487693
4.641817	344.823827	5.492698
4.234015	352.715230	5.497702
4.621305	352.658242	5.502707
4.373575	363.755334	5.507712
4.437805	363.624559	5.512717
4.605674	365.284629	5.517722
4.527929	363.928020	5.522726
4.705362	368.351995	5.527731
4.711122	380.437818	5.532736
4.525375	369.521898	5.537741
4.908824	376.884259	5.542746
4.567746	374.750921	5.547750
4.612415	369.107798	5.552755
4.654263	371.571969	5.557760
4.904857	368.683325	5.562765
4.916125	373.062395	5.567770
4.492243	363.456570	5.572774
4.626180	361.883555	5.577779
4.612554	364.356122	5.582784
4.841950	364.506238	5.587789
4.805032	370.315104	5.592794
4.552398	372.543873	5.597798
4.794161	368.974298	5.602803
4.684320	373.107806	5.607808
4.792325	372.480384	5.612813
4.377194	370.385753	5.617818
4.326110	369.856310	5.622822
4.411693	370.286779	5.627827
4.545044	375.033994	5.632832
4.508612	380.745692	5.637837
4.629900	392.905735	5.642842
4.739563	393.920482	5.647846
5.033667	394.769905	5.652851
4.962503	406.450919	5.657856
4.924585	404.506945	5.662861
4.669050	395.473920	5.667866
4.709727	414.412075	5.672870
5.016710	398.305063	5.677875
4.915386	401.997105	5.682880
4.992516	402.133165	5.687885
5.465010	402.722755	5.692890
4.972571	403.037592	5.697894
5.299640	408.905983	5.702899
5.201781	403.192713	5.707904
5.532147	403.425963	5.712909
5.292722	389.156869	5.717914
4.813468	383.556492	5.722918
4.770743	386.978735	5.727923
4.913307	393.425087	5.732928
5.030035	400.033196	5.737933
5.146779	399.265598	5.742938
4.900521	408.131375	5.747942
5.180260	395.597145	5.752947
4.842524	405.656176	5.757952
4.939292	404.157985	5.762957
5.279989	399.284784	5.767962
5.309264	409.295673	5.772966
5.264242	404.694138	5.777971
4.981062	401.435263	5.782976
4.985537	396.295682	5.787981
5.019061	407.537847	5.792986
5.067586	407.235620	5.797990
5.348415	401.357225	5.802995
5.098407	400.247393	5.808000
5.059638	400.870929	5.813005
4.965769	405.729188	5.818010
5.102439	429.735883	5.823014
5.663967	428.041340	5.828019
5.374795	436.737029	5.833024
5.517304	431.446112	5.838029
5.052668	432.455318	5.843034
5.184265	434.110351	5.848038
5.229842	429.966236	5.853043
5.079814	427.562475	5.858048
5.480299	428.925519	5.863053
5.486076	430.122249	5.868058
5.289407	435.113181	5.873062
5.603965	427.342832	5.878067
5.309876	429.748382	5.883072
5.330070	429.551884	5.888077
5.566840	425.240340	5.893082
5.351889	436.521896	5.898086
5.497898	427.205485	5.903091
5.446240	440.007531	5.908096
5.388362	440.503594	5.913101
5.264142	433.508623	5.918106
5.225478	438.128049	5.923110
5.738994	443.031970	5.928115
5.348619	451.998006	5.933120
5.484301	463.120482	5.938125
5.836153	462.117794	5.943130
5.898907	466.141442	5.948134
6.083063	449.837643	5.953139
5.509891	454.555452	5.958144
5.536098	448.443717	5.963149
5.686392	447.333704	5.968154
5.765971	453.347288	5.973158
5.817288	445.620126	5.978163
5.438059	447.283576	5.983168
5.648559	453.696405	5.988173
5.622002	462.660220	5.993178
5.691733	465.699768	5.998182
5.796079	469.338429	6.003187
5.968081	472.406826	6.008192
5.661381	478.899587	6.013197
6.118952	462.477286	6.018202
5.731264	464.493600	6.023206
5.842601	462.652976	6.028211
5.932981	468.599262	6.033216
5.974022	466.214966	6.038221
6.058967	451.954264	6.043226
5.537886	449.967350	6.048230
5.912479	439.754657	6.053235
5.336624	434.158416	6.058240
5.620755	453.317581	6.063245
5.784732	456.081824	6.068250
5.717744	469.742685	6.073254
5.773715	454.963830	6.078259
5.647529	471.399014	6.083264
5.752266	472.207376	6.088269
5.864983	467.636142	6.093274
5.950813	465.776061	6.098278
5.863430	467.837764	6.103283
5.823663	469.334494	6.108288
6.008767	467.251360	6.113293
6.203620	466.695397	6.118298
5.880755	461.568952	6.123302
5.900604	443.360816	6.128307
5.531781	441.720279	6.133312
5.502351	455.675850	6.138317
5.734952	451.930957	6.143322
6.031139	463.368448	6.148326
6.264353	470.518530	6.153331
6.062129	461.236280	6.158336
5.585254	445.317235	6.163341
6.047454	440.735696	6.168346
5.749618	439.229829	6.173350
5.757554	439.390570	6.178355
5.509417	433.846032	6.183360
5.608699	425.345264	6.188365
5.783899	436.350865	6.193370
5.532590	462.134162	6.198374
5.689733	461.832300	6.203379
5.696475	473.389362	6.208384
5.447723	473.889209	6.213389
6.273202	471.400275	6.218394
6.053185	472.780429	6.223398
6.171547	460.935336	6.228403
5.629631	457.601680	6.233408
5.748984	451.604763	6.238413
5.993397	454.887119	6.243418
6.016180	452.684835	6.248422
5.961717	436.823134	6.253427
5.801867	436.517325	6.258432
5.891057	436.916612	6.263437
5.800448	427.567157	6.268442
5.880178	432.393916	6.273446
5.793924	434.660659	6.278451
5.658483	438.594968	6.283456
5.680133	435.234103	6.288461
6.327927	431.938673	6.293466
5.888672	434.115472	6.298470
6.037909	436.205478	6.303475
5.925890	438.205543	6.308480
5.806217	435.504693	6.313485
5.904508	428.824732	6.318490
5.840350	443.628876	6.323494
5.959789	437.502496	6.328499
5.855043	439.347433	6.333504
5.572031	434.874495	6.338509
5.846057	435.151807	6.343514
5.773048	446.111687	6.348518
5.988020	431.688177	6.353523
5.743483	437.624591	6.358528
5.696793	433.632311	6.363533
5.791634	423.551993	6.368538
5.319101	440.680716	6.373542
5.799246	439.264673	6.378547
5.885386	435.337029	6.383552
5.687685	437.418575	6.388557
6.300494	425.135437	6.393562
5.783197	438.506355	6.398566
5.573066	441.525343	6.403571
5.609886	436.269489	6.408576
5.501126	435.888323	6.413581
5.700690	434.264768	6.418586
5.644353	439.457035	6.423590
5.768391	436.266686	6.428595
5.743713	442.383768	6.433600
5.407065	441.205201	6.438605
5.893501	446.876518	6.443610
5.973331	468.487523	6.448614
5.845585	448.299055	6.453619
5.540994	434.979845	6.458624
5.950987	444.948631	6.463629
5.804119	440.631148	6.468634
5.679184	438.553969	6.473638
5.842518	451.239712	6.478643
5.855934	460.034299	6.483648
5.653558	457.375755	6.488653
5.765761	449.108654	6.493658
5.842769	467.965672	6.498662
5.715972	463.596116	6.503667
5.894534	470.146852	6.508672
5.610647	474.030367	6.513677
6.055408	472.542429	6.518682
6.005669	475.727271	6.523686
5.962459	450.164682	6.528691
5.810694	447.834813	6.533696
5.876613	445.145854	6.538701
6.011950	439.854938	6.543706
5.967478	446.562973	6.548710
5.851145	441.039628	6.553715
6.025479	442.171939	6.558720
5.895468	435.961951	6.563725
6.026217	431.232436	6.568730
5.985155	438.845687	6.573734
6.028684	429.176827	6.578739
5.812690	444.592999	6.583744
5.833447	443.862803	6.588749
5.875008	438.774888	6.593754
5.431003	436.645363	6.598758
5.722523	434.382203	6.603763
6.015601	430.398190	6.608768
5.828093	434.611473	6.613773
5.746471	434.333954	6.618778
5.386496	445.812005	6.623782
5.366471	439.446851	6.628787
5.725317	443.824231	6.633792
5.728143	446.295666	6.638797
5.940873	436.546883	6.643802
5.502892	443.185494	6.648806
5.626572	449.805300	6.653811
5.545884	445.556779	6.658816
5.579362	457.189126	6.663821
6.004168	459.093787	6.668826
5.820587	471.096183	6.673830
6.005433	458.539530	6.678835
5.404591	454.054095	6.683840
5.650461	468.869481	6.688845
6.090603	459.041783	6.693850
5.866423	472.481806	6.698854
5.539460	470.369996	6.703859
5.876444	475.277308	6.708864
5.789455	471.948436	6.713869
6.339035	467.909507	6.718874
5.758850	451.297537	6.723878
5.643378	439.674707	6.728883
5.411321	450.990088	6.733888
5.839775	459.190237	6.738893
6.041647	460.141569	6.743898
5.905236	471.936644	6.748902
6.021878	455.346827	6.753907
5.673555	451.725560	6.758912
5.678835	449.200961	6.763917
5.956672	446.579329	6.768922
5.717460	443.489980	6.773926
5.687207	436.643040	6.778931
5.763418	452.870637	6.783936
5.928728	467.037289	6.788941
6.004247	461.307325	6.793946
5.749511	446.267344	6.798950
5.964372	441.280382	6.803955
5.927768	444.055735	6.808960
6.100992	439.200781	6.813965
6.318273	435.660306	6.818970
5.929233	443.240997	6.823974
6.101418	438.043241	6.828979
5.693018	431.817390	6.833984
5.752253	445.646971	6.838989
5.828443	437.301774	6.843994
5.621870	437.166112	6.848998
5.812404	439.637050	6.854003
5.704973	443.314917	6.859008
5.841828	443.393529	6.864013
6.044535	440.523853	6.869018
5.824153	444.693642	6.874022
5.896359	442.704195	6.879027
5.892234	434.297113	6.884032
5.823897	436.260935	6.889037
6.285259	439.659511	6.894042
5.756216	445.261387	6.899046
5.839472	444.105049	6.904051
5.897519	436.407562	6.909056
5.717762	441.018384	6.914061
5.519195	431.628392	6.919066
5.329989	444.805665	6.924070
5.395052	440.217663	6.929075
5.552422	447.239985	6.934080
5.765247	442.141074	6.939085
5.601637	443.698369	6.944090
5.472998	447.553210	6.949094
5.847478	443.261878	6.954099
5.571274	444.133911	6.959104
5.822686	456.304820	6.964109
6.026099	446.612237	6.969114
5.469106	443.115315	6.974118
5.674789	450.435909	6.979123
5.848800	466.757045	6.984128
5.929817	468.355336	6.989133
6.209160	462.494134	6.994138
5.668514	452.442856	6.999142
5.788594	451.415400	7.004147
5.734959	444.205674	7.009152
6.043049	441.123971	7.014157
5.856899	444.556163	7.019162
5.448125	444.010958	7.024166
5.886482	434.329602	7.029171
5.929310	434.032067	7.034176
5.828445	442.460561	7.039181
5.929394	435.906453	7.044186
5.656338	443.512142	7.049190
5.791347	440.636113	7.054195
5.903622	447.279908	7.059200
5.722507	442.765823	7.064205
6.041268	437.255484	7.069210
5.779198	440.998425	7.074214
6.008986	436.401697	7.079219
5.901445	443.121358	7.084224
6.145628	439.722853	7.089229
5.782382	444.331105	7.094234
6.037734	439.987669	7.099238
5.874912	446.102171	7.104243
5.627523	440.064358	7.109248
5.503307	443.288561	7.114253
5.773734	429.844142	7.119258
5.672853	444.686928	7.124262
5.687211	438.952694	7.129267
5.756330	437.487101	7.134272
5.560952	442.438156	7.139277
5.871618	440.246813	7.144282
5.796997	440.547126	7.149286
5.874331	438.777849	7.154291
5.633977	441.252847	7.159296
5.199440	441.076196	7.164301
5.650360	454.222071	7.169306
5.988501	468.561983	7.174310
5.973257	467.732961	7.179315
5.992080	468.975289	7.184320
5.588459	460.621124	7.189325
6.111901	463.269602	7.194330
5.634507	443.982268	7.199334
5.719616	437.143458	7.204339
6.023800	451.484241	7.209344
5.577543	458.199020	7.214349
5.799909	453.662322	7.219354
5.880635	465.606738	7.224358
5.503421	468.053489	7.229363
5.772067	468.492918	7.234368
5.879614	471.755317	7.239373
5.946836	476.039110	7.244378
5.653914	478.591887	7.249382
6.301683	462.872784	7.254387
6.062845	451.226564	7.259392
5.562753	449.073568	7.264397
5.817565	443.631636	7.269402
5.725067	440.020304	7.274406
5.832979	444.328333	7.279411
5.883547	452.435354	7.284416
5.709814	449.198010	7.289421
5.786922	447.769178	7.294426
5.541342	461.359555	7.299430
5.682433	463.327775	7.304435
5.996509	467.793682	7.309440
5.956816	478.765631	7.314445
6.135068	456.705634	7.319450
6.013369	452.920346	7.324454
6.067237	444.843472	7.329459
5.969252	448.907153	7.334464
5.934798	446.188243	7.339469
5.869360	447.274219	7.344474
5.703036	445.593638	7.349478
5.872679	456.390204	7.354483
5.860435	442.389515	7.359488
5.558972	438.710170	7.364493
5.533099	442.164761	7.369498
5.770802	442.830332	7.374502
5.542642	444.405816	7.379507
5.386437	439.217247	7.384512
5.623778	442.350992	7.389517
5.826082	452.553289	7.394522
5.965691	468.912488	7.399526
5.902062	457.989308	7.404531
6.010304	442.624199	7.409536
5.664340	453.004508	7.414541
5.994790	436.175850	7.419546
5.970944	441.032195	7.424550
6.005387	438.099804	7.429555
6.121744	448.465913	7.434560
6.077046	437.940407	7.439565
5.980336	435.917560	7.444570
5.617281	439.598682	7.449574
5.839159	446.667551	7.454579
6.195737	431.793946	7.459584
5.664639	456.488672	7.464589
5.875411	435.326540	7.469594
5.744885	438.205063	7.474598
5.829585	437.098809	7.479603
5.773706	441.596566	7.484608
5.763912	445.614068	7.489613
5.869098	431.362267	7.494618
5.547552	439.258967	7.499622
5.758882	442.495885	7.504627
5.649752	440.119885	7.509632
5.531205	447.855691	7.514637
5.668448	436.801581	7.519642
5.499081	447.721176	7.524646
5.362468	447.998602	7.529651
5.702242	439.730132	7.534656
5.889374	446.718715	7.539661
5.766532	441.788068	7.544666
5.351584	450.917425	7.549670
5.758950	472.215486	7.554675
6.081624	472.281089	7.559680
5.729902	483.397263	7.564685
5.955048	474.650264	7.569690
5.945681	479.298005	7.574694
5.677723	461.921730	7.579699
5.878775	466.033382	7.584704
5.698776	456.950911	7.589709
5.847081	458.216593	7.594714
5.739942	465.604584	7.599718
5.943909	473.927757	7.604723
6.096909	469.356956	7.609728
5.645629	465.787269	7.614733
5.860097	443.498696	7.619738
6.082928	446.568144	7.624742
5.787538	451.901629	7.629747
5.556158	448.130163	7.634752
5.566596	451.211496	7.639757
6.173505	459.691127	7.644762
5.961313	454.967677	7.649766
5.675318	452.138666	7.654771
5.760158	447.623757	7.659776
5.736236	447.162038	7.664781
5.971970	442.184841	7.669786
5.699623	454.788216	7.674790
5.668063	445.767211	7.679795
5.859871	443.750854	7.684800
6.019363	443.086488	7.689805
6.017142	440.103136	7.694810
5.634738	449.132775	7.699814
5.421021	448.957841	7.704819
5.669633	450.671053	7.709824
5.672487	463.006660	7.714829
5.840465	465.781095	7.719834
5.676456	462.509775	7.724838
5.565411	465.589914	7.729843
6.140428	466.469393	7.734848
5.949312	475.828501	7.739853
6.146906	457.696886	7.744858
5.779429	450.821715	7.749862
5.733965	455.198165	7.754867
5.881254	440.107602	7.759872
5.840651	447.664539	7.764877
6.045627	439.439507	7.769882
5.462842	440.827829	7.774886
5.680772	439.818113	7.779891
5.994135	441.528298	7.784896
5.935699	447.663996	7.789901
5.644790	446.848653	7.794906
5.866206	443.432210	7.799910
5.949580	444.015788	7.804915
5.851922	445.027374	7.809920
5.895975	450.222755	7.814925
6.118193	445.592151	7.819930
6.037497	449.345909	7.824934
5.844948	444.258672	7.829939
5.844133	450.009689	7.834944
5.522778	448.029762	7.839949
5.938519	436.825340	7.844954
5.564829	448.311979	7.849958
5.772277	449.124052	7.854963
5.963368	446.917185	7.859968
5.829957	447.135865	7.864973
6.212980	440.448218	7.869978
5.639805	456.035635	7.874982
5.982779	448.672811	7.879987
6.139483	441.365896	7.884992
5.521077	458.059981	7.889997
5.835844	448.375796	7.895002
5.479167	448.466275	7.900006
5.706049	450.507905	7.905011
6.055965	449.882455	7.910016
5.793759	454.150935	7.915021
5.818309	447.034034	7.920026
5.670477	446.734918	7.925030
5.444919	451.077843	7.930035
5.466022	439.278078	7.935040
5.242490	453.654744	7.940045
5.773834	459.347836	7.945050
6.025032	474.080646	7.950054
5.813714	468.672281	7.955059
5.701655	455.074695	7.960064
5.714946	465.975503	7.965069
5.983464	476.835435	7.970074
5.995529	461.153520	7.975078
5.508143	458.924218	7.980083
5.699905	453.143040	7.985088
5.795596	463.504293	7.990093
6.087859	474.816539	7.995098
5.892507	457.039687	8.000102
5.964912	459.542227	8.005107
5.810013	454.291868	8.010112
5.483835	464.560169	8.015130
5.781708	453.464877	8.020147
5.815736	454.225168	8.025165
6.080069	459.842814	8.030182
5.811646	447.760083	8.035200
5.688229	457.258965	8.040218
5.876248	456.425373	8.045235
5.728236	456.654237	8.050253
5.635209	458.676024	8.055270
5.876623	465.870969	8.060288
6.126674	474.959621	8.065306
6.048402	459.407660	8.070323
5.613539	453.755738	8.075341
5.668927	453.069099	8.080358
5.848850	462.909063	8.085376
5.701987	488.490356	8.090394
5.828462	480.819040	8.095411
6.015927	484.969613	8.100429
6.083276	489.110356	8.105446
5.963284	486.090138	8.110464
6.024063	475.004959	8.115482
5.965668	464.079276	8.120499
5.966496	463.823883	8.125517
5.817952	461.989410	8.130534
6.118560	448.982986	8.135552
5.535757	461.894103	8.140570
5.760670	472.415153	8.145587
5.966480	487.654770	8.150605
5.940241	487.294221	8.155622
6.143989	473.785154	8.160640
6.075670	479.487614	8.165658
6.199486	460.229236	8.170675
5.895125	454.786198	8.175693
5.677139	452.663248	8.180710
6.144386	453.322276	8.185728
6.045570	469.214634	8.190746
6.001883	458.634131	8.195763
6.064867	451.858314	8.200781
5.791346	461.524761	8.205798
5.916878	468.351328	8.210816
5.715342	470.948522	8.215834
6.329407	478.333322	8.220851
6.274551	477.662575	8.225869
6.034803	473.769146	8.230886
5.989234	461.896136	8.235904
5.921077	463.209528	8.240922
6.011942	472.201910	8.245939
6.466223	476.571665	8.250957
6.019740	466.211781	8.255974
6.006475	445.873055	8.260992
5.811075	446.821916	8.266010
6.152394	462.335896	8.271027
5.982867	469.344974	8.276045
5.844854	478.010129	8.281062
6.426475	482.278884	8.286080
6.166940	477.447069	8.291098
5.705698	470.326785	8.296115
6.139044	472.308454	8.301133
5.834691	476.096406	8.306150
5.860740	475.559889	8.311168
5.841048	484.084203	8.316186
5.695091	482.155015	8.321203
5.936723	484.237521	8.326221
5.797227	477.300159	8.331238
6.265575	483.623935	8.336256
6.235666	481.491292	8.341274
6.263222	483.452173	8.346291
5.958092	474.710880	8.351309
6.282229	485.659767	8.356326
6.304819	482.074837	8.361344
6.412917	481.849709	8.366362
6.395340	479.838834	8.371379
6.454250	477.005708	8.376397
6.210552	489.614060	8.381414
6.323871	477.653314	8.386432
6.296878	481.620519	8.391450
6.606253	475.731184	8.396467
6.568905	473.077176	8.401485
6.066931	479.220315	8.406502
6.278279	467.265981	8.411520
5.850028	481.876194	8.416538
6.314081	476.538762	8.421555
6.531895	477.736105	8.426573
5.856735	475.351676	8.431590
5.722277	473.531404	8.436608
6.059407	479.772191	8.441626
5.994298	486.030970	8.446643
6.102769	479.503298	8.451661
6.067715	483.573011	8.456678
6.313587	475.407750	8.461696
6.251620	479.773038	8.466714
6.180972	473.706690	8.471731
6.833979	473.408061	8.476749
6.461328	482.502988	8.481766
6.409100	481.038558	8.486784
6.255748	476.289153	8.491802
6.014586	480.912641	8.496819
6.261615	473.225106	8.501837
5.884858	477.387618	8.506854
6.404221	466.976254	8.511872
6.250599	485.584980	8.516890
6.125661	478.263935	8.521907
6.071154	477.065611	8.526925
6.053773	484.000686	8.531942
6.614524	499.173272	8.536960
6.522211	493.739001	8.541978
6.549044	497.750442	8.546995
5.923907	481.409946	8.552013
6.528264	504.461342	8.557030
6.359118	494.954464	8.562048
6.202728	494.170027	8.567066
6.181090	510.105942	8.572083
6.734010	510.689177	8.577101
6.453480	515.991586	8.582119
6.523556	507.077128	8.587136
6.364651	497.035128	8.592154
6.390537	505.032457	8.597171
6.634637	503.376446	8.602189
6.457020	489.810840	8.607207
6.340179	483.928305	8.612224
6.347200	497.876933	8.617242
6.725419	496.052268	8.622259
6.450722	488.373369	8.627277
6.248324	484.943599	8.632295
6.043257	497.032213	8.637312
6.490155	501.751203	8.642330
6.734840	515.146553	8.647347
6.976537	505.020889	8.652365
6.303545	494.887260	8.657383
6.624190	490.409138	8.662400
6.306412	481.705759	8.667418
6.269942	486.964792	8.672435
6.249594	492.977006	8.677453
6.101165	516.149531	8.682471
6.405047	511.569659	8.687488
6.842385	514.517925	8.692506
6.613658	516.555301	8.697523
6.802738	517.621195	8.702541
6.885215	524.660610	8.707559
6.665653	514.723320	8.712576
6.534329	500.503629	8.717594
6.336565	503.440141	8.722611
6.728090	512.689626	8.727629
6.587304	511.531568	8.732647
6.699665	515.366265	8.737664
6.675856	500.484919	8.742682
6.752809	486.250633	8.747699
6.518917	483.044567	8.752717
6.457944	489.411906	8.757735
6.271126	491.061658	8.762752
6.722762	499.120757	8.767770
6.711269	515.303601	8.772787
6.770974	508.078336	8.777805
6.500702	509.314185	8.782823
6.466446	514.086478	8.787840
6.760991	516.961547	8.792858
6.444471	513.364068	8.797875
6.922409	514.722459	8.802893
6.663168	519.006064	8.807911
6.637051	514.634762	8.812928
6.624478	513.646601	8.817946
6.474455	525.527317	8.822963
6.934009	511.709932	8.827981
6.600717	516.630556	8.832999
6.469484	515.022524	8.838016
6.781991	517.456461	8.843034
6.848939	526.987245	8.848051
6.908845	510.851762	8.853069
6.469765	516.048152	8.858087
6.862776	524.004776	8.863104
6.753246	518.518233	8.868122
6.488240	527.073548	8.873139
6.779695	511.044200	8.878157
6.717123	524.933122	8.883175
6.273804	517.109899	8.888192
6.822454	518.744158	8.893210
6.595856	516.917289	8.898227
6.827549	512.068879	8.903245
6.757279	523.914342	8.908263
6.884771	520.123070	8.913280
6.920703	521.824516	8.918298
6.491334	515.495136	8.923315
6.490253	515.264269	8.928333
6.719058	514.471357	8.933351
6.815196	514.199984	8.938368
7.012071	509.193770	8.943386
6.790502	515.366273	8.948403
7.112210	513.741304	8.953421
6.777085	511.557237	8.958439
6.572034	513.102735	8.963456
6.810398	519.182938	8.968474
6.187770	523.263351	8.973491
6.868785	519.097764	8.978509
6.727142	522.425350	8.983527
6.697598	535.358093	8.988544
6.884311	532.998247	8.993562
6.768321	544.313146	8.998579
7.088460	546.339947	9.003597
7.016362	535.775315	9.008615
6.948648	540.880299	9.013632
7.041095	537.275916	9.018650
6.950058	527.675577	9.023667
6.781138	528.344684	9.028685
6.854721	530.690638	9.033703
7.036274	541.249424	9.038720
7.072660	536.207380	9.043738
6.835193	540.966879	9.048755
6.670061	529.521854	9.053773
6.896158	536.975847	9.058791
6.702747	538.415687	9.063808
6.746394	540.857341	9.068826
6.750638	542.758511	9.073843
6.636449	544.651343	9.078861
7.130254	540.774606	9.083879
6.993238	547.927538	9.088896
7.091639	542.634098	9.093914
6.906584	545.436632	9.098931
7.251509	542.741356	9.103949
7.000496	546.669890	9.108967
7.090542	546.702457	9.113984
7.374878	539.547452	9.119002
7.127487	546.912742	9.124019
7.042756	547.201989	9.129037
6.897866	537.597965	9.134055
6.833873	542.802720	9.139072
7.166129	533.801528	9.144090
7.170216	538.809588	9.149107
7.075540	538.229679	9.154125
6.804056	540.344015	9.159143
7.032734	538.469507	9.164160
7.316230	530.035800	9.169178
6.825032	537.062350	9.174195
6.912164	542.147599	9.179213
7.308629	539.772702	9.184231
7.235138	538.649559	9.189248
7.315400	539.164420	9.194266
6.898290	541.033402	9.199283
7.322089	539.954084	9.204301
7.323827	541.826734	9.209319
7.066930	549.570146	9.214336
7.200111	536.523072	9.219354
6.934000	530.177084	9.224371
7.089793	539.286893	9.229389
7.226868	536.594345	9.234407
6.778505	539.917611	9.239424
6.623067	538.009670	9.244442
6.877914	549.076563	9.249459
7.038414	562.847090	9.254477
7.333693	562.699619	9.259495
7.107501	575.237232	9.264512
7.651107	577.187863	9.269530
7.338814	574.196715	9.274547
7.201543	570.261097	9.279565
7.309728	573.410720	9.284583
7.043808	580.482854	9.289600
7.548183	570.155394	9.294618
7.380624	569.717858	9.299635
7.090216	550.461035	9.304653
7.072761	562.290302	9.309671
6.909832	573.643111	9.314688
7.465731	579.279247	9.319706
7.546628	576.282041	9.324723
7.273281	575.480159	9.329741
7.669207	573.923204	9.334759
7.366271	579.066364	9.339776
7.259015	563.439576	9.344794
7.463344	567.540927	9.349811
7.073862	562.292051	9.354829
7.222819	567.414704	9.359847
7.358762	572.495423	9.364864
7.806056	560.362783	9.369882
7.358741	565.283407	9.374899
6.953466	563.245782	9.379917
7.613245	565.760401	9.384935
7.416098	582.421665	9.389952
7.503469	564.833645	9.394970
7.363009	572.104276	9.399987
7.268674	567.183468	9.405005
7.508465	573.970887	9.410023
7.285200	575.699513	9.415040
7.545014	562.668453	9.420058
7.515114	579.966540	9.425075
7.546441	572.706379	9.430093
7.369622	549.324537	9.435111
7.527384	560.231544	9.440128
7.735463	556.100957	9.445146
7.667197	545.467578	9.450163
7.386932	543.991104	9.455181
7.621644	528.194347	9.460199
7.126666	547.320269	9.465216
7.163077	540.008498	9.470234
7.109115	545.633610	9.475251
7.150539	568.017741	9.480269
7.285100	571.685795	9.485287
7.181484	567.119451	9.490304
7.416609	566.633737	9.495322
7.551780	568.738411	9.500339
7.590930	564.607845	9.505357
7.722003	565.591228	9.510375
7.439697	575.814870	9.515392
7.820258	569.488349	9.520410
7.608936	577.663961	9.525427
7.390872	565.774557	9.530445
7.739262	566.435754	9.535463
7.155390	565.657735	9.540480
7.388190	564.232510	9.545498
7.487210	566.606735	9.550515
7.374763	570.321596	9.555533
7.936745	565.149007	9.560551
7.711394	561.430719	9.565568
7.515204	564.210298	9.570586
7.818106	563.987751	9.575603
7.733743	570.412339	9.580621
7.936554	563.744610	9.585639
7.303794	570.102145	9.590656
7.534930	567.054867	9.595674
7.576176	564.848032	9.600691
7.535064	565.983148	9.605709
7.819292	560.586101	9.610727
7.385093	568.264991	9.615744
7.390260	580.243271	9.620762
7.690221	581.607125	9.625779
7.625370	585.561138	9.630797
8.191197	590.502572	9.635815
7.922426	584.679407	9.640832
7.411997	577.170592	9.645850
7.563092	569.175099	9.650867
7.718392	589.550188	9.655885
7.998542	599.895457	9.660903
7.803514	595.813896	9.665920
7.632701	583.093284	9.670938
7.751584	590.752445	9.675955
7.698642	599.294139	9.680973
8.191684	593.391275	9.685991
7.500370	594.116772	9.691008
7.617061	603.184672	9.696026
7.679863	590.311007	9.701043
7.860758	599.319261	9.706061
8.095228	597.595548	9.711079
7.758422	604.969569	9.716096
7.789967	602.160636	9.721114
8.086798	604.125561	9.726131
7.574040	601.420933	9.731149
8.175968	596.923956	9.736167
8.080138	603.509895	9.741184
7.678521	583.815572	9.746202
7.620027	591.844240	9.751219
7.739307	596.671247	9.756237
7.965540	597.227485	9.761255
7.803872	604.118992	9.766272
8.299038	594.360522	9.771290
7.948721	598.617501	9.776307
7.870136	604.574642	9.781325
8.131865	592.468375	9.786343
7.798358	599.624145	9.791360
7.974278	593.858827	9.796378
7.989906	592.535108	9.801395
7.830605	606.678293	9.806413
7.992546	602.329956	9.811431
7.985458	597.813954	9.816448
7.939846	604.491964	9.821466
7.813210	599.105069	9.826483
7.796541	610.378964	9.831501
7.958941	600.553555	9.836519
8.090235	609.171630	9.841536
7.979833	597.674975	9.846554
8.192022	604.848449	9.851571
8.084487	609.407724	9.856589
8.244741	598.690408	9.861607
7.973327	603.883471	9.866624
8.089944	593.940262	9.871642
8.031074	598.075362	9.876659
8.069547	600.706845	9.881677
7.834556	607.451844	9.886695
8.074595	606.215365	9.891712
7.898412	601.312232	9.896730
8.213745	600.106196	9.901747
7.909061	597.696618	9.906765
8.108638	599.754413	9.911783
7.951587	605.069278	9.916800
8.231712	598.240513	9.921818
8.372108	599.122755	9.926835
8.277995	609.164479	9.931853
8.472615	604.071212	9.936871
8.228113	597.175197	9.941888
7.815206	600.323325	9.946906
8.190065	590.524153	9.951923
7.803874	601.005156	9.956941
7.795429	599.181716	9.961959
8.232782	607.852252	9.966976
8.148801	602.859053	9.971994
7.972532	594.580573	9.977011
7.911161	605.373908	9.982029
7.912114	603.655401	9.987047
8.285578	607.446294	9.992064
8.131833	604.244055	9.997082
8.191915	598.998277	10.002099
8.188142	605.395953	10.007117
8.046185	600.910353	10.012135
8.373360	616.186885	10.017152
8.651246	621.994263	10.022170
8.459276	607.860495	10.027187
8.198654	610.089176	10.032205
8.247235	597.724322	10.037223
8.151831	601.433611	10.042240
8.102614	598.593371	10.047258
8.481022	609.237709	10.052275
8.223295	621.742198	10.057293
8.697600	621.599922	10.062311
8.386211	609.267700	10.067328
8.284756	610.350413	10.072346
8.245362	598.363685	10.077363
8.410870	602.636226	10.082381
8.122529	602.238767	10.087399
8.202555	605.025170	10.092416
8.362574	623.351628	10.097434
8.712034	618.250432	10.102451
8.256134	614.819307	10.107469
8.241270	614.753899	10.112487
8.911057	620.918401	10.117504
8.091057	616.444096	10.122522
8.653076	616.638453	10.127539
8.438989	614.021757	10.132557
8.462690	601.104955	10.137575
8.390044	606.668227	10.142592
8.547070	608.812395	10.147610
8.660575	596.252355	10.152627
8.172306	600.747517	10.157645
8.685340	605.355595	10.162663
8.434453	600.482745	10.167680
8.277553	608.119280	10.172698
8.427771	618.026069	10.177715
8.423237	627.171336	10.182733
8.841182	622.536916	10.187751
8.757614	615.962450	10.192768
8.373852	601.724235	10.197786
8.521336	604.299678	10.202803
8.510051	607.097659	10.207821
8.644976	628.383790	10.212839
8.563975	614.413715	10.217856
8.336924	628.888197	10.222874
8.848814	621.205742	10.227891
8.807970	629.584437	10.232909
8.780328	609.354760	10.237927
8.302465	595.851179	10.242944
8.268108	609.063108	10.247962
8.575738	617.298074	10.252979
8.666099	621.637391	10.257997
8.496049	625.609228	10.263015
8.591265	629.604458	10.268032
8.287043	637.650220	10.273050
8.493390	625.944804	10.278067
8.558668	622.070115	10.283085
8.088495	628.471021	10.288103
8.965509	631.116007	10.293120
8.603023	635.958831	10.298138
8.780312	624.294250	10.303155
8.520373	624.850488	10.308173
8.623207	631.009473	10.313191
8.834958	620.360381	10.318208
8.590195	633.621542	10.323226
8.872455	629.296971	10.328243
8.844749	626.056535	10.333261
8.741537	633.627700	10.338279
8.914158	632.542531	10.343296
8.698198	633.399932	10.348314
9.050059	622.750077	10.353331
8.725049	633.285336	10.358349
8.718867	627.076765	10.363367
8.786377	624.919704	10.368384
8.672045	624.794984	10.373402
8.845332	613.776307	10.378419
8.469820	619.549370	10.383437
8.568866	621.885216	10.388455
8.830439	643.484822	10.393472
8.697130	649.482143	10.398490
9.231401	641.359190	10.403507
9.193663	637.381485	10.408525
9.001914	624.187171	10.413543
9.191022	620.753364	10.418560
8.942862	620.353581	10.423578
8.828263	620.315515	10.428595
8.862569	627.348781	10.433613
8.759910	618.461681	10.438631
8.630975	621.976542	10.443648
8.319407	630.313654	10.448666
8.707037	634.637015	10.453683
8.778717	639.548488	10.458701
8.543459	644.465122	10.463719
9.320171	648.954752	10.468736
9.066463	648.994442	10.473754
8.965885	649.385915	10.478771
8.813991	657.403511	10.483789
8.984685	664.019746	10.488807
9.601095	656.394175	10.493824
9.119330	657.405033	10.498842
9.698566	658.612617	10.503859
9.133210	639.969680	10.508877
9.237242	640.169408	10.513895
9.310522	626.401516	10.518912
9.030480	626.497334	10.523930
9.026216	626.307738	10.528947
9.347041	623.477866	10.533965
9.049383	620.937405	10.538983
9.115491	623.136785	10.544000
8.805086	625.567596	10.549018
8.969519	620.950552	10.554035
9.030507	628.357131	10.559053
8.718948	631.581783	10.564071
8.925365	629.970186	10.569088
8.982370	645.324357	10.574106
9.256156	652.884084	10.579123
9.158177	651.250060	10.584141
9.082062	660.157807	10.589159
9.336757	658.074068	10.594176
9.139791	659.476322	10.599194
9.432830	658.584584	10.604211
9.228826	654.713141	10.609229
8.974082	665.245644	10.614247
9.500916	657.555382	10.619264
9.131409	661.558485	10.624282
9.308224	652.844365	10.629299
9.141135	657.747746	10.634317
8.956522	662.428455	10.639335
9.288236	653.299733	10.644352
8.940032	661.044345	10.649370
9.101155	658.255675	10.654387
9.060680	660.657540	10.659405
9.041843	661.511039	10.664423
9.173563	652.909497	10.669440
9.300674	657.349228	10.674458
8.992810	661.348028	10.679475
9.108915	656.643706	10.684493
8.963747	660.845472	10.689511
9.723309	667.737009	10.694528
9.557149	678.881190	10.699546
9.601037	662.790719	10.704563
9.736993	656.060403	10.709581
9.226916	657.255073	10.714599
9.268895	657.444605	10.719616
9.602525	658.481455	10.724634
9.363515	660.792976	10.729651
9.272104	653.033057	10.734669
9.163322	652.785772	10.739687
9.360022	654.104729	10.744704
9.384425	663.393444	10.749722
9.337129	659.553922	10.754739
9.576219	667.409147	10.759757
9.458896	676.596150	10.764775
9.728804	657.201926	10.769792
9.558424	656.253470	10.774810
9.409160	650.404585	10.779827
9.484672	659.074245	10.784845
9.349424	657.170031	10.789863
9.496724	664.489308	10.794880
9.729002	660.033841	10.799898
9.541955	658.838948	10.804915
9.554023	648.566778	10.809933
9.438521	662.964163	10.814951
9.441563	667.642144	10.819968
9.185971	684.241742	10.824986
9.371240	692.362176	10.830003
9.702194	679.603866	10.835021
9.580939	691.880314	10.840039
10.090674	689.061075	10.845056
9.830965	695.321849	10.850074
9.260806	690.650058	10.855091
9.455797	681.490026	10.860109
9.473949	687.817771	10.865127
9.640109	686.004579	10.870144
9.644664	689.347359	10.875162
9.796229	694.985340	10.880179
9.953636	685.715394	10.885197
9.594285	686.442221	10.890215
9.764327	685.759025	10.895232
9.610727	685.204614	10.900250
9.632965	686.936691	10.905267
9.981623	686.242815	10.910285
9.873854	688.923134	10.915303
9.905297	684.037953	10.920320
9.957463	686.961064	10.925338
9.653681	683.499025	10.930355
9.741488	677.045948	10.935373
9.656800	692.887380	10.940391
9.606533	684.624599	10.945408
9.674345	689.979614	10.950426
9.872774	691.229394	10.955443
10.172644	683.812909	10.960461
9.727825	680.798609	10.965479
9.880792	696.744383	10.970496
9.881184	690.138070	10.975514
9.680558	694.216752	10.980531
10.025729	694.981238	10.985549
9.892478	698.019694	10.990567
9.799090	691.661572	10.995584
9.722228	690.224822	11.000602
9.518576	695.701164	11.005619
9.533784	683.858075	11.010637
9.577193	697.819360	11.015655
10.108875	683.422394	11.020672
9.705697	690.310430	11.025690
9.767523	688.797962	11.030707
10.021950	685.528117	11.035725
10.012070	688.110342	11.040743
10.109370	688.948548	11.045760
10.008252	688.882659	11.050778
9.924823	692.297093	11.055795
10.076302	690.096592	11.060813
9.674076	693.309500	11.065831
9.748834	679.215746	11.070848
9.895374	691.830110	11.075866
9.640400	689.321740	11.080883
9.802333	699.969509	11.085901
9.992512	710.852357	11.090919
10.658505	714.487953	11.095936
10.493615	712.870907	11.100954
10.094105	694.437041	11.105971
10.132412	682.976718	11.110989
10.058059	683.477229	11.116007
10.144519	683.527908	11.121024
9.949358	678.049977	11.126042
9.764415	691.197941	11.131059
9.798025	700.242649	11.136077
10.036446	709.750269	11.141095
9.882348	705.168229	11.146112
10.322624	705.592184	11.151130
10.061251	712.141412	11.156147
10.434556	702.793975	11.161165
10.122686	715.090589	11.166183
10.124918	705.696730	11.171200
10.361053	705.918282	11.176218
10.301630	715.352398	11.181235
10.312632	711.477226	11.186253
10.183704	712.428480	11.191271
9.925405	721.970331	11.196288
9.960096	717.264512	11.201306
10.149192	714.168856	11.206323
10.317599	710.546343	11.211341
10.133475	721.495510	11.216359
10.288744	710.046900	11.221376
10.518942	709.383662	11.226394
10.086150	720.019302	11.231411
10.419225	712.657144	11.236429
10.313034	712.307861	11.241447
10.149043	711.558724	11.246464
10.343527	714.007119	11.251482
10.367859	719.258721	11.256499
10.340223	716.868991	11.261517
10.181120	714.134125	11.266535
10.176296	714.474707	11.271552
10.514558	715.827704	11.276570
10.136988	716.744546	11.281587
10.490479	717.973769	11.286605
10.100892	724.030090	11.291623
10.368333	738.336575	11.296640
10.692690	739.084039	11.301658
10.304181	758.167787	11.306675
10.777962	745.121614	11.311693
10.498933	741.446421	11.316711
10.640816	739.442766	11.321728
10.426370	721.110106	11.326746
10.165172	730.580793	11.331763
10.565426	747.657649	11.336781
10.515158	749.277337	11.341799
10.467576	746.827918	11.346816
10.657615	741.985744	11.351834
10.297926	752.785275	11.356851
10.522972	742.713589	11.361869
10.972334	744.673353	11.366887
10.783810	753.045074	11.371904
10.984810	744.027703	11.376922
10.635316	734.279494	11.381939
10.561182	721.696096	11.386957
10.462189	720.003181	11.391975
10.478518	724.950223	11.396992
10.876083	728.890098	11.402010
10.775496	731.206659	11.407027
10.718695	717.542111	11.412045
10.394155	720.029605	11.417063
10.546423	732.891070	11.422080
10.738386	737.883044	11.427098
10.905302	747.358436	11.432115
10.687717	736.330188	11.437133
10.460487	741.827772	11.442151
10.799346	747.059583	11.447168
11.127278	736.015408	11.452186
10.513138	739.642921	11.457203
10.762414	729.198750	11.462221
10.911000	748.912798	11.467239
10.662617	745.024273	11.472256
11.084814	736.504893	11.477274
10.591454	729.259499	11.482291
10.876647	738.983001	11.487309
10.904946	742.687193	11.492327
10.829260	741.062066	11.497344
11.212233	719.935755	11.502362
10.696454	715.738388	11.507379
10.561617	714.804119	11.512397
11.057657	722.860117	11.517415
10.830060	729.550994	11.522432
11.129395	735.060589	11.527450
10.761665	726.485415	11.532467
10.893874	721.607945	11.537485
10.918692	731.543839	11.542503
10.979690	737.023613	11.547520
11.203857	730.516440	11.552538
11.079796	718.035795	11.557555
10.950958	708.968737	11.562573
10.832342	705.131959	11.567591
10.740812	717.951110	11.572608
10.994586	727.786100	11.577626
10.644920	738.698129	11.582643
10.845774	745.838114	11.587661
10.988582	747.852184	11.592679
10.896716	746.835605	11.597696
11.215702	742.653142	11.602714
10.899536	750.620826	11.607731
10.969307	749.500715	11.612749
11.104535	746.744268	11.617767
10.738685	755.082365	11.622784
11.069691	746.712717	11.627802
10.987051	750.204587	11.632819
10.997940	745.544431	11.637837
11.148471	746.376188	11.642855
10.855661	743.180020	11.647872
11.108936	750.901451	11.652890
11.031974	749.297005	11.657907
10.966083	749.725254	11.662925
11.102356	739.328920	11.667943
10.753224	766.961961	11.672960
11.607252	768.756300	11.677978
11.494537	763.628445	11.682995
11.361224	749.865521	11.688013
11.327561	738.437545	11.693031
11.249135	751.802161	11.698048
11.199114	746.034832	11.703066
11.284127	748.915509	11.708083
11.439494	749.114218	11.713101
11.134770	745.799163	11.718119
11.143535	739.257580	11.723136
10.943490	748.827988	11.728154
11.186926	765.084030	11.733171
11.395661	773.671853	11.738189
11.478884	777.990547	11.743207
11.135628	774.408260	11.748224
11.556612	773.147711	11.753242
11.831517	779.974679	11.758259
11.725664	769.867617	11.763277
11.720456	751.027465	11.768295
11.162128	755.832287	11.773312
11.600693	748.016055	11.778330
11.380058	749.576164	11.783347
11.054105	747.189768	11.788365
11.626041	741.297798	11.793383
11.081527	751.310659	11.798400
11.678550	753.947507	11.803418
11.210529	745.280275	11.808435
11.333849	770.447826	11.813453
11.734712	760.467481	11.818471
11.730193	773.733661	11.823488
11.869067	752.383568	11.828506
11.383359	751.707781	11.833523
11.534747	747.417250	11.838541
11.641630	738.518216	11.843559
11.109949	755.862387	11.848576
11.476087	750.682012	11.853594
11.484454	769.286694	11.858611
11.208499	775.615541	11.863629
11.412917	770.663503	11.868647
11.397590	763.647973	11.873664
11.662237	764.979702	11.878682
11.670327	772.847250	11.883699
11.598319	772.342707	11.888717
11.751631	772.467745	11.893735
11.629333	781.222194	11.898752
11.962538	769.841313	11.903770
11.790398	771.236316	11.908787
11.601998	771.132521	11.913805
11.584374	767.915976	11.918823
11.458335	772.775590	11.923840
11.927089	762.250961	11.928858
11.828148	774.184822	11.933875
11.947888	778.320313	11.938893
12.113477	770.362275	11.943911
11.709521	771.409072	11.948928
11.803177	770.438932	11.953946
11.815994	769.551466	11.958963
11.343932	777.526476	11.963981
11.725055	770.043349	11.968999
11.377931	784.113866	11.974016
11.617126	775.557449	11.979034
11.912775	774.540869	11.984051
11.961669	770.949155	11.989069
11.882213	770.253337	11.994087
11.754223	779.344535	11.999104
11.582349	772.688370	12.004122
11.785495	777.632051	12.009139
11.640653	802.055913	12.014157
12.338281	791.558716	12.019175
12.120293	801.220705	12.024192
12.035684	781.877156	12.029210
12.104231	776.238206	12.034227
11.944766	774.366726	12.039245
12.163345	759.116470	12.044263
11.749900	773.901857	12.049280
11.929557	779.055716	12.054298
12.294269	788.470035	12.059315
12.135329	775.602227	12.064333
12.268085	770.217593	12.069351
12.322552	766.467879	12.074368
11.989478	767.536795	12.079386
12.008220	763.728041	12.084403
12.089584	766.400282	12.089421
12.203473	758.044141	12.094439
11.561102	773.839821	12.099456
11.697573	778.443775	12.104474
12.260313	782.981869	12.109491
12.491938	785.577660	12.114509
12.811318	783.672554	12.119527
12.191646	769.215783	12.124544
12.120035	761.415130	12.129562
12.189387	754.556833	12.134579
11.887555	768.852500	12.139597
12.271504	762.189728	12.144615
12.105268	757.826600	12.149632
12.199051	763.039946	12.154650
12.384837	776.439568	12.159667
12.375088	773.085504	12.164685
12.556635	760.712478	12.169703
12.377883	756.187259	12.174720
12.326275	758.881518	12.179738
12.452744	757.282753	12.184755
12.541309	763.391007	12.189773
12.478358	757.768720	12.194791
12.264690	753.234717	12.199808
12.058408	750.259246	12.204826
12.448081	755.323992	12.209843
12.279954	761.477113	12.214861
12.594980	758.197613	12.219879
12.417987	750.052232	12.224896
12.270322	746.559210	12.229914
12.536305	746.186091	12.234931
12.029448	754.602259	12.239949
12.261412	748.715404	12.244967
12.079524	761.374367	12.249984
12.262889	784.816349	12.255002
12.775214	782.866695	12.260019
12.747825	779.464767	12.265037
12.764095	783.545744	12.270055
12.571889	790.161893	12.275072
12.545184	778.073324	12.280090
12.397524	772.978416	12.285107
12.324788	781.863233	12.290125
12.783902	787.860927	12.295143
12.728961	800.385915	12.300160
12.372382	801.046936	12.305178
12.076803	800.131013	12.310195
12.141151	798.623234	12.315213
12.313781	791.792698	12.320231
12.475627	795.562186	12.325248
12.495199	796.871512	12.330266
12.686558	790.670123	12.335283
12.372926	796.386354	12.340301
12.754358	785.251006	12.345319
12.768683	798.016477	12.350336
12.259986	796.468951	12.355354
12.670174	812.844666	12.360371
12.588020	815.282196	12.365389
12.898417	822.205269	12.370407
12.760447	822.827336	12.375424
12.902135	822.396849	12.380442
13.162420	811.534286	12.385459
12.775932	812.247501	12.390477
12.767859	786.591612	12.395495
12.900363	790.193920	12.400512
12.869086	795.870088	12.405530
12.723017	790.276907	12.410547
12.525310	803.953035	12.415565
13.067144	811.483414	12.420583
13.248961	812.409201	12.425600
12.634893	814.321457	12.430618
12.924110	809.347885	12.435635
12.813093	813.757805	12.440653
13.059054	817.904688	12.445671
13.130036	813.039296	12.450688
13.196087	808.951451	12.455706
13.182759	794.763522	12.460723
12.980948	803.820505	12.465741
13.141010	793.081631	12.470759
13.177303	786.267768	12.475776
12.916988	795.033662	12.480794
12.892086	780.532326	12.485811
12.763276	791.820789	12.490829
12.784534	787.068751	12.495847
13.259622	804.565539	12.500864
13.099275	803.072527	12.505882
13.030158	800.419196	12.510899
13.012793	804.778568	12.515917
13.170081	808.125215	12.520935
13.201007	818.369192	12.525952
13.131817	809.768550	12.530970
13.047398	810.218372	12.535987
13.025657	810.051549	12.541005
13.357852	811.043768	12.546023
13.564124	812.211162	12.551040
13.080392	810.447701	12.556058
13.048012	796.756599	12.561075
13.339632	813.005500	12.566093
13.251539	810.096268	12.571111
13.282679	807.583806	12.576128
13.187322	807.073680	12.581146
13.151319	811.622744	12.586163
13.063681	812.805737	12.591181
13.300541	813.209838	12.596199
13.441651	816.524129	12.601216
12.795798	825.157435	12.606234
13.474666	819.822502	12.611251
13.186536	815.585836	12.616269
13.125955	822.949060	12.621287
13.316948	814.433672	12.626304
13.221802	817.109955	12.631322
13.534362	810.238523	12.636339
13.255799	824.019392	12.641357
13.124526	808.757732	12.646375
13.170926	823.288289	12.651392
13.278227	814.395442	12.656410
13.424727	815.599897	12.661427
13.243956	824.651833	12.666445
13.443905	838.588111	12.671463
13.841475	845.717615	12.676480
13.327765	834.866671	12.681498
13.489341	841.278598	12.686515
13.735145	845.344416	12.691533
13.844875	837.235759	12.696551
13.739584	817.349950	12.701568
13.152985	818.122679	12.706586
13.454670	828.366707	12.711603
13.675401	836.952973	12.716621
13.745634	841.510437	12.721639
13.786166	839.112551	12.726656
13.449817	834.939372	12.731674
13.883264	834.567653	12.736691
13.979229	832.331445	12.741709
13.800865	820.204574	12.746727
13.846503	813.576936	12.751744
13.589656	816.448490	12.756762
13.862423	803.249738	12.761779
13.729861	812.253135	12.766797
13.909177	808.681939	12.771815
13.798490	806.216189	12.776832
13.766872	811.133799	12.781850
13.459113	800.936534	12.786867
13.604284	809.573485	12.791885
13.807144	806.030673	12.796903
13.994778	805.156774	12.801920
13.607307	811.500165	12.806938
13.858103	801.946983	12.811955
14.140059	820.089910	12.816973
13.777959	808.393057	12.821991
14.228804	808.437726	12.827008
13.877183	815.608996	12.832026
13.767868	811.702150	12.837043
13.860110	804.907752	12.842061
13.662275	804.431917	12.847079
13.670866	812.178543	12.852096
14.111986	832.376118	12.857114
14.435388	832.030889	12.862131
14.221365	827.711479	12.867149
14.316812	806.497629	12.872167
14.012056	807.050469	12.877184
13.859117	811.226004	12.882202
14.013968	806.471522	12.887219
14.387745	807.258441	12.892237
14.127945	802.172251	12.897255
13.965154	799.919450	12.902272
14.188510	804.210222	12.907290
14.024679	797.156672	12.912307
14.187574	801.572410	12.917325
14.183243	805.946159	12.922343
13.965685	796.465024	12.927360
13.559582	804.901540	12.932378
14.234766	827.784614	12.937395
14.207286	830.895340	12.942413
14.062084	835.142431	12.947431
14.345691	825.922367	12.952448
14.275960	846.510049	12.957466
14.235399	835.332737	12.962483
14.191173	836.084156	12.967501
14.404664	833.010420	12.972519
14.559194	838.625129	12.977536
14.447773	843.327234	12.982554
14.157345	836.832004	12.987571
14.087997	839.308753	12.992589
13.843457	837.876922	12.997607
14.167400	831.611439	13.002624
14.270641	838.751884	13.007642
14.203984	833.645117	13.012659
14.635299	832.999356	13.017677
14.397445	829.405901	13.022695
14.570200	835.139238	13.027712
14.420628	839.631136	13.032730
14.288699	834.605252	13.037747
14.296761	841.559895	13.042765
14.148616	836.241436	13.047783
14.190101	840.048975	13.052800
14.538541	839.381900	13.057818
14.444911	834.341801	13.062835
14.464010	840.510798	13.067853
14.365375	847.197693	13.072871
15.070605	849.424535	13.077888
14.753684	848.005475	13.082906
14.000444	842.108506	13.087923
14.892500	846.235019	13.092941
14.599968	851.533624	13.097959
14.842002	840.596114	13.102976
14.497673	827.790850	13.107994
14.439430	837.346885	13.113011
14.968550	852.675838	13.118029
14.733616	852.306927	13.123047
14.862321	830.429697	13.128064
14.570930	832.086959	13.133082
14.609380	836.668975	13.138099
14.697293	839.940114	13.143117
14.578177	855.346097	13.148135
14.972426	853.485668	13.153152
14.876684	858.338718	13.158170
15.126929	852.173221	13.163187
14.948511	842.676128	13.168205
14.661135	837.292539	13.173223
14.683836	827.804670	13.178240
14.999788	830.780185	13.183258
14.867242	845.176624	13.188275
14.894123	831.905184	13.193293
14.676759	830.733800	13.198311
14.957788	846.777414	13.203328
15.067777	849.751607	13.208346
14.958357	844.409805	13.213363
15.041188	842.631652	13.218381
15.008252	848.588808	13.223399
14.901329	830.857079	13.228416
14.779022	839.302523	13.233434
15.039721	852.360689	13.238451
15.472303	855.855845	13.243469
14.844404	844.924202	13.248487
15.007508	843.286292	13.253504
14.881425	850.439915	13.258522
14.924229	855.119242	13.263539
15.092545	859.291985	13.268557
14.941455	857.795860	13.273575
15.292485	858.624342	13.278592
15.298394	868.522906	13.283610
15.214635	861.595038	13.288627
15.388463	859.327823	13.293645
15.445724	862.822142	13.298663
15.105073	851.137059	13.303680
15.116030	854.342207	13.308698
14.917802	860.516099	13.313715
15.394313	858.016096	13.318733
14.901176	869.855864	13.323751
15.510193	856.571468	13.328768
15.340670	860.052948	13.333786
15.216022	865.352102	13.338803
15.323161	853.200762	13.343821
15.159969	863.665485	13.348839
15.295324	857.851278	13.353856
15.475495	857.130967	13.358874
15.316784	857.299800	13.363891
15.256211	857.317743	13.368909
14.717613	859.625755	13.373927
14.952627	857.092516	13.378944
15.372797	858.992566	13.383962
15.119651	861.671398	13.388979
15.394854	871.880078	13.393997
15.296733	886.712566	13.399015
15.468199	894.401161	13.404032
15.610010	883.586904	13.409050
15.668997	894.346731	13.414067
15.479942	880.883852	13.419085
15.075744	890.253124	13.424103
15.339982	888.706726	13.429120
15.789776	886.843788	13.434138
15.209326	892.314093	13.439155
15.549400	888.386748	13.444173
15.484368	880.179060	13.449191
15.459073	886.034577	13.454208
15.742334	883.079192	13.459226
15.284728	891.448303	13.464243
15.614167	881.639936	13.469261
15.564972	891.194901	13.474279
15.552439	889.189633	13.479296
15.855094	897.652137	13.484314
15.727637	904.974507	13.489331
16.292760	893.172475	13.494349
15.770798	891.625167	13.499367
15.722849	880.483690	13.504384
15.829480	882.491564	13.509402
15.882878	890.882746	13.514419
16.019387	879.814658	13.519437
15.744365	885.674520	13.524455
15.867181	876.227520	13.529472
15.870333	879.463886	13.534490
15.784604	883.489342	13.539507
15.871492	887.359056	13.544525
15.594040	891.163124	13.549543
15.781276	896.313799	13.554560
16.073048	902.777023	13.559578
16.058027	917.930803	13.564595
16.493881	904.996284	13.569613
15.898160	899.175173	13.574631
15.932882	886.773606	13.579648
16.112693	876.717197	13.584666
15.889127	889.404818	13.589683
15.642697	882.863702	13.594701
15.952879	900.639468	13.599719
16.429516	909.747153	13.604736
16.271762	918.666598	13.609754
16.054903	918.958834	13.614771
16.507121	900.356521	13.619789
16.361796	892.356208	13.624807
15.735855	888.334506	13.629824
16.194554	890.830512	13.634842
16.152174	909.503999	13.639859
16.313245	905.847617	13.644877
16.191762	913.999279	13.649895
16.283380	907.834044	13.654912
16.793179	905.267895	13.659930
16.619154	904.093658	13.664947
16.255189	892.664361	13.669965
16.135888	888.904024	13.674983
16.092523	877.512196	13.680000
16.319230	875.774386	13.685018
16.079365	887.335626	13.690035
16.253280	896.096206	13.695053
16.343484	910.879028	13.700071
16.343095	903.225165	13.705088
16.732166	897.422470	13.710106
16.697764	917.395764	13.715123
16.601706	903.599370	13.720141
16.341067	898.823114	13.725159
16.016964	898.719349	13.730176
16.536978	898.524623	13.735194
16.415826	905.219996	13.740211
16.355961	910.858028	13.745229
16.298750	911.200203	13.750247
16.584514	922.944104	13.755264
16.975677	908.234388	13.760282
16.603359	912.329354	13.765299
16.864903	903.710507	13.770317
16.894155	907.566149	13.775335
16.749432	914.910674	13.780352
16.885932	905.449974	13.785370
16.616239	913.115178	13.790387
16.984084	907.597871	13.795405
16.829574	904.588207	13.800423
16.270701	892.980957	13.805440
16.772888	895.571727	13.810458
16.481151	905.080646	13.815475
16.797435	905.007841	13.820493
16.772562	905.761570	13.825511
16.305940	903.559458	13.830528
16.477916	907.926481	13.835546
16.174087	914.399363	13.840563
16.513913	906.387207	13.845581
17.000450	908.467603	13.850599
16.640350	902.655503	13.855616
16.755649	906.830345	13.860634
16.767510	930.024582	13.865651
17.003194	943.056259	13.870669
17.391141	926.845945	13.875687
17.132444	915.936182	13.880704
17.012235	902.394958	13.885722
16.821438	906.550411	13.890739
16.794824	898.783968	13.895757
17.170880	913.341121	13.900775
17.118219	919.857844	13.905792
17.166529	915.877629	13.910810
16.903905	910.599753	13.915827
17.035775	919.312586	13.920845
17.501900	925.863085	13.925863
17.169439	916.107216	13.930880
17.186809	907.683516	13.935898
16.867235	905.815305	13.940915
17.103541	910.892509	13.945933
16.999968	919.639604	13.950951
17.119154	937.050601	13.955968
17.350743	938.756307	13.960986
16.924542	929.498607	13.966003
17.051527	940.512549	13.971021
17.274466	942.572822	13.976039
17.047514	941.261684	13.981056
17.322060	929.519158	13.986074
17.270187	935.161387	13.991091
16.954804	941.287390	13.996109
17.422337	932.955269	14.001127
17.393280	931.441686	14.006144
17.622367	931.518353	14.011162
17.519069	929.648970	14.016179
17.378582	926.110626	14.021197
17.281976	939.602817	14.026215
17.432888	939.545586	14.031232
17.337232	936.934419	14.036250
17.469156	936.321695	14.041267
17.579422	937.603811	14.046285
17.530385	929.386362	14.051303
17.735541	929.065436	14.056320
17.527477	926.549259	14.061338
17.162370	926.090882	14.066355
17.283666	927.555020	14.071373
17.465776	926.130874	14.076391
17.542903	948.935609	14.081408
17.770615	953.646549	14.086426
18.076115	947.922632	14.091443
17.743591	945.271163	14.096461
17.999418	934.797817	14.101479
17.744515	927.382927	14.106496
17.752495	923.624733	14.111514
17.782214	927.410621	14.116531
17.820222	927.244925	14.121549
18.092925	924.034600	14.126567
17.735709	934.251985	14.131584
17.799549	922.359324	14.136602
18.075662	930.558931	14.141619
17.962626	933.879899	14.146637
18.144209	919.548562	14.151655
17.827765	925.686939	14.156672
17.943142	928.469713	14.161690
17.692979	930.129606	14.166707
17.839599	923.188364	14.171725
17.881881	915.909300	14.176743
17.823563	925.897666	14.181760
17.962655	925.580986	14.186778
18.111639	915.378090	14.191795
17.796519	919.189976	14.196813
17.863603	919.278509	14.201831
17.788059	922.852703	14.206848
17.986098	914.506952	14.211866
17.979292	931.876998	14.216883
17.921447	935.410077	14.221901
17.872469	934.115531	14.226919
17.974143	949.373241	14.231936
18.378451	941.209845	14.236954
18.008575	939.048792	14.241971
18.001759	944.638290	14.246989
18.348308	937.603702	14.252007
18.252733	952.400792	14.257024
18.256446	945.863502	14.262042
18.219675	940.418301	14.267059
17.798916	947.775875	14.272077
18.488633	941.651739	14.277095
17.857628	952.622314	14.282112
18.122121	944.957244	14.287130
18.136152	951.475928	14.292147
17.888511	947.082527	14.297165
18.240063	958.924612	14.302183
18.516565	969.403996	14.307200
18.784019	975.424447	14.312218
18.590671	966.228556	14.317235
18.266968	945.749248	14.322253
18.552914	946.382223	14.327271
18.490043	948.605172	14.332288
18.268973	948.899681	14.337306
18.413042	954.749225	14.342323
18.370668	970.862662	14.347341
18.720153	958.743547	14.352359
18.592732	975.570647	14.357376
18.675078	968.154221	14.362394
18.796650	968.245149	14.367411
18.621712	976.102558	14.372429
18.991835	970.009287	14.377447
18.943424	972.954617	14.382464
18.506611	954.269541	14.387482
18.650174	951.641987	14.392499
18.728800	963.568638	14.397517
19.151200	957.322626	14.402535
18.620808	948.134134	14.407552
18.650144	945.169212	14.412570
18.756468	949.875450	14.417587
18.594223	971.651006	14.422605
19.090106	970.417801	14.427623
18.856334	970.191996	14.432640
18.729863	965.178551	14.437658
18.891520	970.201996	14.442675
18.749957	974.348920	14.447693
18.892376	974.412381	14.452711
18.652201	983.249846	14.457728
18.875117	983.436192	14.462746
19.244532	975.866327	14.467763
19.014690	977.335860	14.472781
19.067099	968.420520	14.477799
18.732951	983.527605	14.482816
18.899583	980.693479	14.487834
19.203328	970.299573	14.492851
18.557779	981.307220	14.497869
18.971450	965.973278	14.502887
18.798254	975.014992	14.507904
18.879300	974.668161	14.512922
19.186355	975.197646	14.517939
18.987696	981.060252	14.522957
19.454330	983.342371	14.527975
19.036752	983.645012	14.532992
19.521688	978.279150	14.538010
19.278013	966.918064	14.543027
18.920715	969.285435	14.548045
19.437777	986.967204	14.553063
19.485919	983.240138	14.558080
19.074906	978.696229	14.563098
19.646789	984.719815	14.568115
19.479698	986.104552	14.573133
19.396300	974.163006	14.578151
19.175933	980.721304	14.583168
19.458142	980.007318	14.588186
19.491872	965.285086	14.593203
19.110386	967.642289	14.598221
19.580719	982.489002	14.603239
19.492199	995.203558	14.608256
19.619112	995.491230	14.613274
19.757699	991.479512	14.618291
19.570348	984.672281	14.623309
19.555371	981.587530	14.628327
19.578386	986.607562	14.633344
19.487926	986.959180	14.638362
20.040789	990.882857	14.643379
19.437119	987.841651	14.648397
19.730255	983.641752	14.653415
19.681172	987.924541	14.658432
19.924270	987.178845	14.663450
19.769137	974.269691	14.668467
19.562338	971.745424	14.673485
19.986051	978.495874	14.678503
19.822170	966.090517	14.683520
19.294718	975.395214	14.688538
19.840731	979.177115	14.693555
19.417856	992.285602	14.698573
19.718206	988.629759	14.703591
19.765682	989.419542	14.708608
19.509329	997.904197	14.713626
19.900432	992.859761	14.718643
19.807370	991.097726	14.723661
19.749064	996.923319	14.728679
19.924302	990.296586	14.733696
19.759923	991.077356	14.738714
19.993499	991.370988	14.743731
20.188427	988.062510	14.748749
19.803264	990.570320	14.753767
20.136463	1000.580514	14.758784
19.962767	999.220790	14.763802
20.231980	1003.536307	14.768819
20.306825	1011.948018	14.773837
20.164329	998.061989	14.778855
20.189041	995.728112	14.783872
20.127758	996.181982	14.788890
20.221966	991.832745	14.793907
20.117023	1005.203544	14.798925
20.299688	1014.737513	14.803943
20.477694	1001.366497	14.808960
20.605650	1003.901149	14.813978
20.516782	984.945831	14.818995
20.495997	986.198472	14.824013
20.542534	983.948774	14.829031
20.327903	988.189688	14.834048
20.396189	989.007519	14.839066
20.433790	974.476361	14.844083
20.088514	984.764633	14.849101
20.313853	979.052010	14.854119
20.263954	977.557227	14.859136
20.475375	991.018930	14.864154
20.557887	979.526659	14.869171
20.151848	979.873843	14.874189
20.528383	996.903332	14.879207
20.938754	1001.558845	14.884224
20.519720	1005.016715	14.889242
20.638822	991.958204	14.894259
20.427405	985.590765	14.899277
20.804732	999.509628	14.904295
20.642312	991.264860	14.909312
20.474846	1000.229659	14.914330
20.684024	1010.714314	14.919347
20.713802	1011.223575	14.924365
20.625230	1019.235202	14.929383
20.997020	1012.216872	14.934400
20.923368	1013.241272	14.939418
20.923484	1002.908250	14.944435
20.708818	999.869947	14.949453
20.511717	1004.325670	14.954471
20.859803	1003.575973	14.959488
20.684654	1013.979788	14.964506
20.963322	1012.259736	14.969523
20.691257	1017.132584	14.974541
20.623070	1019.441066	14.979559
20.848551	1018.293971	14.984576
21.055163	1017.048036	14.989594
21.126732	1011.299055	14.994611
20.970420	1011.012393	14.999629
20.809587	1010.883165	15.004647
20.970565	1004.504840	15.009664
20.868106	1010.286571	15.014682
21.195515	1011.539428	15.019699
21.364202	1014.840928	15.024717
21.119564	1019.598216	15.029735
21.225780	1015.224937	15.034752
21.059376	1019.074031	15.039770
21.201311	1008.077391	15.044787
21.329909	1019.841485	15.049805
21.314383	1018.863820	15.054823
21.371540	1016.143481	15.059840
21.097887	1003.976734	15.064858
20.933902	1012.767349	15.069875
20.999427	1018.087425	15.074893
20.884639	1018.959587	15.079911
21.281647	1029.518267	15.084928
21.158985	1041.044860	15.089946
21.403042	1041.719420	15.094963
21.285834	1043.707296	15.099981
21.601486	1037.273819	15.104999
21.914689	1037.421201	15.110016
21.615090	1040.020751	15.115034
21.911530	1029.225668	15.120051
21.808413	1032.815083	15.125069
21.592185	1015.245724	15.130087
21.747828	1004.839312	15.135104
21.574304	1000.029702	15.140122
21.463872	997.170588	15.145139
21.733205	1009.595594	15.150157
21.698560	1014.952334	15.155175
21.871257	999.108677	15.160192
21.375672	1002.517020	15.165210
21.560728	1013.531241	15.170227
21.822034	1033.336432	15.175245
21.492101	1031.849039	15.180263
21.772926	1023.674159	15.185280
21.674837	1033.671936	15.190298
21.842179	1026.897682	15.195315
21.777343	1028.271396	15.200333
21.577789	1035.166807	15.205351
21.961794	1023.350969	15.210368
21.692180	1032.160267	15.215386
21.836521	1030.270337	15.220403
22.232673	1035.116003	15.225421
22.029440	1037.384647	15.230439
21.805408	1026.858420	15.235456
21.738036	1026.336172	15.240474
21.770778	1031.282169	15.245491
21.890967	1034.427537	15.250509
21.881586	1031.791045	15.255527
22.084189	1027.375819	15.260544
22.075964	1040.520406	15.265562
22.068238	1028.043080	15.270579
22.287046	1031.272507	15.275597
22.060323	1033.748576	15.280615
22.217046	1029.355907	15.285632
21.824146	1042.622852	15.290650
22.620547	1053.395718	15.295667
22.586338	1043.429363	15.300685
22.299350	1040.945920	15.305703
22.477262	1030.589738	15.310720
22.130827	1031.469551	15.315738
21.939381	1030.225358	15.320755
22.601484	1045.245880	15.325773
22.510271	1063.632375	15.330791
22.766679	1045.595756	15.335808
22.504271	1036.789197	15.340826
22.411283	1021.844202	15.345843
22.468090	1029.216825	15.350861
22.192066	1031.797904	15.355879
22.447281	1039.156968	15.360896
22.451306	1044.579360	15.365914
22.466078	1054.436812	15.370931
22.534352	1055.275121	15.375949
22.562846	1054.224813	15.380967
22.859954	1049.751807	15.385984
22.504163	1062.576027	15.391002
22.624809	1057.061414	15.396019
22.583100	1055.589676	15.401037
22.641511	1054.476148	15.406055
22.920296	1040.788815	15.411072
22.918042	1054.448547	15.416090
22.626822	1056.144384	15.421107
22.668035	1052.079879	15.426125
22.333611	1051.337688	15.431143
22.881476	1050.415150	15.436160
23.109979	1055.533062	15.441178
22.866147	1049.184350	15.446195
22.849280	1048.644684	15.451213
22.632634	1053.064682	15.456231
23.007734	1049.325978	15.461248
23.127322	1049.239683	15.466266
23.017269	1048.674110	15.471283
23.023721	1046.273173	15.476301
22.918787	1047.514951	15.481319
23.253534	1038.294167	15.486336
22.932483	1043.745585	15.491354
22.900789	1045.907088	15.496371
23.252072	1062.635331	15.501389
23.107447	1069.822439	15.506407
23.268569	1071.518964	15.511424
23.306999	1074.220808	15.516442
23.270340	1071.473869	15.521459
23.136514	1074.411710	15.526477
23.335515	1082.151743	15.531495
23.305136	1077.857756	15.536512
23.339213	1076.317957	15.541530
23.095816	1082.059275	15.546547
23.587210	1071.389355	15.551565
23.279202	1080.986899	15.556583
23.480201	1067.528951	15.561600
23.818440	1071.827152	15.566618
23.577653	1063.411471	15.571635
23.429852	1053.414708	15.576653
23.335886	1049.831626	15.581671
23.586756	1053.257315	15.586688
23.528228	1072.487588	15.591706
23.404298	1080.832255	15.596723
23.700143	1067.756224	15.601741
23.489959	1079.917001	15.606759
23.700096	1077.797281	15.611776
23.460633	1080.766394	15.616794
23.665627	1080.382896	15.621811
23.606242	1068.713275	15.626829
23.241536	1077.829672	15.631847
23.244813	1076.095768	15.636864
23.065769	1070.402437	15.641882
23.124450	1091.195156	15.646899
23.936799	1090.246143	15.651917
23.906860	1107.918631	15.656935
24.034496	1108.710106	15.661952
24.026008	1105.675436	15.666970
23.971284	1108.302163	15.671987
24.276514	1110.654334	15.677005
24.136110	1108.893432	15.682023
24.181792	1113.042064	15.687040
24.169538	1102.961803	15.692058
23.818671	1095.570990	15.697075
24.157727	1086.198288	15.702093
24.148888	1109.517871	15.707111
24.047479	1104.459681	15.712128
24.117100	1104.851721	15.717146
24.187805	1103.920400	15.722163
24.273917	1096.858002	15.727181
24.050623	1105.291573	15.732199
23.879459	1102.002748	15.737216
24.004819	1103.692206	15.742234
23.842327	1108.939838	15.747251
24.301905	1106.950458	15.752269
24.328060	1105.938721	15.757287
24.117482	1105.943709	15.762304
24.299533	1109.401672	15.767322
24.213961	1103.620019	15.772339
24.356675	1102.604729	15.777357
24.508067	1106.932305	15.782375
24.532333	1100.492723	15.787392
24.466933	1098.574526	15.792410
24.478938	1103.062185	15.797427
24.491194	1105.575856	15.802445
24.512074	1107.455050	15.807463
24.162701	1115.969739	15.812480
24.857098	1133.397123	15.817498
24.769481	1129.119293	15.822515
25.035988	1124.795817	15.827533
24.836772	1110.134459	15.832551
24.617036	1101.062145	15.837568
24.616166	1088.398208	15.842586
24.411759	1107.423948	15.847603
24.665425	1117.453294	15.852621
25.047080	1117.178726	15.857639
24.839919	1123.162869	15.862656
25.240480	1121.975752	15.867674
25.030627	1117.055983	15.872691
24.805465	1095.484211	15.877709
24.627873	1100.339472	15.882727
24.925194	1115.950370	15.887744
25.267228	1118.009843	15.892762
25.045746	1121.463371	15.897779
24.942448	1098.547838	15.902797
24.811130	1106.609500	15.907815
24.994061	1125.311290	15.912832
25.341506	1117.578071	15.917850
24.948917	1123.987787	15.922867
25.365556	1125.856174	15.927885
24.969627	1127.442589	15.932903
24.802895	1123.494780	15.937920
25.092407	1128.623479	15.942938
25.049792	1125.017703	15.947955
25.290019	1116.838474	15.952973
24.940681	1130.717158	15.957991
24.902211	1131.987305	15.963008
24.954444	1125.889921	15.968026
25.050913	1125.131885	15.973043
25.187697	1137.885232	15.978061
25.358321	1150.051903	15.983079
25.474686	1157.721802	15.988096
25.676464	1156.158162	15.993114
25.529226	1159.649797	15.998131
25.789447	1156.245042	16.003149
25.965505	1144.876524	16.008167
25.309091	1133.416341	16.013184
25.938900	1118.331095	16.018202
25.946221	1122.584110	16.023219
26.075177	1118.190503	16.028237
26.039017	1116.597765	16.033255
25.595753	1117.538891	16.038272
25.514191	1111.099900	16.043290
25.232822	1116.351865	16.048307
25.634208	1118.698744	16.053325
25.738162	1117.439487	16.058343
25.492125	1116.975560	16.063360
25.692990	1135.603135	16.068378
25.752657	1136.094066	16.073395
25.968824	1139.825511	16.078413
26.049504	1155.977424	16.083431
25.889242	1151.788780	16.088448
26.031154	1151.990904	16.093466
25.985392	1152.833140	16.098483
25.773784	1156.308662	16.103501
25.674612	1146.584881	16.108519
25.779506	1156.014496	16.113536
26.004180	1156.739514	16.118554
26.005378	1159.749891	16.123571
26.192076	1158.719834	16.128589
25.808317	1155.891778	16.133607
26.011684	1156.702210	16.138624
26.005429	1150.922759	16.143642
26.176395	1152.052720	16.148659
26.115231	1153.597879	16.153677
26.241909	1166.681653	16.158695
26.375878	1175.412393	16.163712
26.724124	1171.251742	16.168730
26.632625	1172.535398	16.173747
26.496982	1151.764054	16.178765
26.557942	1142.326741	16.183783
26.552445	1140.817503	16.188800
26.824668	1136.763148	16.193818
26.361406	1144.410519	16.198835
26.717138	1143.889464	16.203853
26.658117	1144.737832	16.208871
26.439682	1141.979644	16.213888
26.519639	1140.419249	16.218906
26.198647	1140.353941	16.223923
26.458581	1144.079715	16.228941
26.761558	1142.837892	16.233959
26.597644	1146.411810	16.238976
26.770097	1137.638694	16.243994
26.397747	1142.705740	16.249011
26.854626	1157.567841	16.254029
27.046892	1159.261187	16.259047
26.283919	1168.984120	16.264064
26.334198	1162.661067	16.269082
26.812749	1167.319121	16.274099
26.741027	1161.271381	16.279117
26.948659	1168.054152	16.284135
27.118309	1168.628838	16.289152
27.088221	1167.080757	16.294170
27.213636	1162.315688	16.299187
27.266226	1164.286092	16.304205
27.106497	1160.243022	16.309223
27.323956	1163.294753	16.314240
27.256722	1165.109807	16.319258
27.074080	1160.398504	16.324275
26.714505	1171.610891	16.329293
27.087289	1164.699806	16.334311
26.745896	1157.609353	16.339328
26.944729	1157.002471	16.344346
26.618808	1160.259529	16.349363
27.147949	1182.947243	16.354381
27.432186	1186.193426	16.359399
27.373489	1198.663454	16.364416
27.595804	1190.214720	16.369434
27.435251	1199.852485	16.374451
27.293941	1193.722557	16.379469
27.569199	1193.040422	16.384487
27.491020	1196.456852	16.389504
27.698196	1186.716569	16.394522
27.875480	1195.490933	16.399539
27.440749	1189.553684	16.404557
27.658815	1186.585417	16.409575
27.440932	1188.726986	16.414592
27.446800	1188.486690	16.419610
27.558739	1183.100242	16.424627
27.832864	1187.003987	16.429645
27.566304	1180.014121	16.434663
27.733812	1186.703941	16.439680
27.620144	1180.772585	16.444698
27.472797	1184.107949	16.449715
27.814171	1184.624279	16.454733
27.791891	1176.027477	16.459751
27.363203	1187.393836	16.464768
27.723039	1187.988996	16.469786
27.904364	1199.566943	16.474803
27.848297	1215.383698	16.479821
28.277515	1206.812507	16.484839
28.010358	1211.882629	16.489856
27.965069	1206.269852	16.494874
27.965365	1214.152694	16.499891
28.105113	1211.262350	16.504909
28.772116	1206.463491	16.509927
28.396484	1211.714955	16.514944
28.210538	1200.850422	16.519962
28.234194	1199.162341	16.524979
28.204142	1214.135440	16.529997
28.397997	1202.265916	16.535015
28.237202	1207.806205	16.540032
28.253427	1200.481718	16.545050
28.397162	1204.301155	16.550067
28.184590	1207.637482	16.555085
28.811831	1208.892282	16.560103
28.616039	1204.976034	16.565120
28.466646	1194.196395	16.570138
28.490685	1193.201538	16.575155
28.460902	1197.885508	16.580173
28.716952	1197.937242	16.585191
28.473608	1195.617801	16.590208
28.560827	1188.794541	16.595226
28.397001	1196.057325	16.600243
28.570294	1200.041940	16.605261
28.654559	1195.144308	16.610279
28.540725	1203.488157	16.615296
28.741149	1202.068828	16.620314
28.862827	1198.503544	16.625331
28.952590	1201.852798	16.630349
28.672142	1199.963110	16.635367
28.636826	1211.755281	16.640384
28.520473	1207.021176	16.645402
28.699058	1193.423921	16.650419
28.422886	1199.719117	16.655437
28.867651	1202.659204	16.660455
28.995543	1219.326973	16.665472
29.170244	1228.829323	16.670490
29.030501	1227.336401	16.675507
29.006236	1224.616123	16.680525
29.363233	1224.418863	16.685543
29.283234	1229.315483	16.690560
29.204379	1205.381992	16.695578
29.466901	1201.687090	16.700595
29.210770	1201.844105	16.705613
29.070756	1199.168587	16.710631
28.949313	1198.638752	16.715648
29.156312	1225.512037	16.720666
29.549166	1227.730822	16.725683
29.489999	1231.667327	16.730701
29.837468	1227.098533	16.735719
29.274270	1235.366417	16.740736
29.410163	1225.884757	16.745754
29.282115	1225.800097	16.750771
29.573532	1229.648234	16.755789
29.571904	1220.364935	16.760807
29.644814	1224.702784	16.765824
29.876632	1223.217626	16.770842
29.793258	1224.302309	16.775859
29.582405	1230.133171	16.780877
29.634239	1221.135892	16.785895
29.569605	1226.980729	16.790912
29.623421	1231.239461	16.795930
29.397834	1215.400905	16.800947
29.171320	1221.689856	16.805965
29.865657	1231.590403	16.810983
29.800686	1225.831276	16.816000
29.853980	1222.911152	16.821018
29.807513	1222.907075	16.826035
29.536378	1221.569371	16.831053
30.071118	1235.786390	16.836071
29.993645	1253.433058	16.841088
30.058391	1247.507172	16.846106
30.428211	1254.980430	16.851123
30.385754	1253.045423	16.856141
30.325798	1237.456970	16.861159
29.990446	1230.127694	16.866176
30.017859	1222.746621	16.871194
30.110430	1230.768125	16.876211
30.062754	1250.768061	16.881229
30.299812	1248.358041	16.886247
30.318946	1244.594772	16.891264
30.130851	1250.691552	16.896282
30.308719	1240.095086	16.901299
30.293627	1244.515621	16.906317
30.468660	1243.634338	16.911335
30.269097	1245.109117	16.916352
29.935409	1236.216217	16.921370
30.264246	1246.489886	16.926387
30.141243	1251.192458	16.931405
30.405936	1232.095617	16.936423
30.422540	1256.713142	16.941440
30.354549	1271.149679	16.946458
30.748290	1269.158976	16.951475
30.585659	1279.710105	16.956493
30.866722	1274.065311	16.961511
30.754077	1282.837735	16.966528
30.530753	1284.291650	16.971546
30.847634	1273.470574	16.976563
30.497480	1274.540774	16.981581
30.729002	1275.738669	16.986599
30.722094	1280.191322	16.991616
30.581626	1272.464017	16.996634
30.940286	1276.127414	17.001651
31.165616	1279.374711	17.006669
31.193685	1279.925995	17.011687
31.051760	1271.216671	17.016704
31.099028	1276.790641	17.021722
31.450468	1270.035796	17.026739
31.228699	1276.782240	17.031757
31.107780	1268.443446	17.036775
31.355302	1271.220936	17.041792
31.128045	1271.618047	17.046810
31.436965	1261.384896	17.051827
31.425580	1263.696607	17.056845
31.149435	1269.626482	17.061863
31.246403	1274.492632	17.066880
31.214958	1268.624003	17.071898
31.369449	1266.989839	17.076915
31.477813	1279.455103	17.081933
31.400283	1277.104256	17.086951
31.617172	1286.128408	17.091968
31.167060	1285.627796	17.096986
31.657719	1278.656592	17.102003
31.586086	1287.772613	17.107021
31.541043	1276.046919	17.112039
31.715661	1279.621503	17.117056
31.647602	1283.959483	17.122074
31.515529	1274.667831	17.127091
31.470748	1281.354656	17.132109
31.495796	1284.889443	17.137127
31.735296	1284.202202	17.142144
31.608706	1286.368036	17.147162
31.927498	1280.944152	17.152179
31.789581	1288.795589	17.157197
31.613845	1291.783322	17.162215
32.055248	1301.425016	17.167232
31.965288	1306.429213	17.172250
32.325472	1304.919643	17.177267
32.090602	1306.328623	17.182285
32.556390	1303.253962	17.187303
32.688347	1286.668742	17.192320
32.714733	1281.164146	17.197338
32.469992	1276.489074	17.202355
32.536245	1273.380578	17.207373
32.197966	1277.494410	17.212391
32.302778	1274.302366	17.217408
32.129470	1273.611829	17.222426
32.355000	1275.601641	17.227443
32.246972	1282.159967	17.232461
31.967040	1285.855488	17.237479
32.312475	1268.756603	17.242496
32.142814	1276.884149	17.247514
32.375291	1270.900560	17.252531
32.406512	1289.310354	17.257549
32.326523	1305.029195	17.262567
32.508705	1300.333029	17.267584
32.445917	1307.842908	17.272602
32.390353	1301.855035	17.277619
32.533307	1309.095419	17.282637
32.474627	1310.699235	17.287655
32.664699	1305.843890	17.292672
32.632340	1310.922407	17.297690
32.772787	1305.065458	17.302707
32.794285	1307.922506	17.307725
32.854749	1303.385466	17.312743
32.580586	1312.365750	17.317760
32.494200	1310.998234	17.322778
33.007731	1328.673895	17.327795
32.774901	1338.468199	17.332813
33.062176	1341.588325	17.337831
33.317309	1335.071049	17.342848
32.985168	1340.082288	17.347866
33.305779	1337.963925	17.352883
32.911891	1337.386680	17.357901
33.389352	1339.581236	17.362919
33.114281	1341.648044	17.367936
32.940554	1344.459868	17.372954
33.223574	1330.755438	17.377971
32.952274	1335.716051	17.382989
33.010887	1342.271217	17.388007
33.518206	1345.771435	17.393024
33.997626	1365.403144	17.398042
33.600209	1349.449205	17.403059
33.313787	1343.846779	17.408077
33.719661	1344.205982	17.413095
33.893649	1327.061014	17.418112
33.363851	1330.927838	17.423130
33.307676	1331.604489	17.428147
33.817769	1347.798488	17.433165
33.737349	1361.299783	17.438183
34.050587	1356.964962	17.443200
34.061140	1348.670889	17.448218
34.112714	1326.043148	17.453235
33.899212	1324.720694	17.458253
33.641607	1321.681169	17.463271
33.903921	1326.919161	17.468288
33.943558	1337.041963	17.473306
33.999408	1348.103801	17.478323
34.148973	1343.735063	17.483341
34.128774	1344.098283	17.488359
34.546389	1339.740672	17.493376
33.982366	1330.744522	17.498394
33.979505	1317.907896	17.503411
33.945746	1330.527834	17.508429
33.953768	1349.021855	17.513447
34.224919	1351.071051	17.518464
34.085086	1357.679162	17.523482
34.377308	1357.133579	17.528499
34.378419	1341.466801	17.533517
34.277871	1346.253083	17.538535
34.603284	1348.657461	17.543552
34.375287	1356.863605	17.548570
34.089690	1350.648453	17.553587
34.437493	1348.457084	17.558605
34.205593	1347.912856	17.563623
34.281491	1345.814148	17.568640
33.964106	1348.548974	17.573658
34.313258	1366.629449	17.578675
34.602431	1372.297648	17.583693
34.616254	1388.698272	17.588711
35.011310	1377.078758	17.593728
34.966894	1380.659320	17.598746
35.093671	1366.187830	17.603763
35.292532	1363.959705	17.608781
35.234721	1371.896736	17.613799
35.102704	1366.341962	17.618816
35.063018	1344.265123	17.623834
34.840103	1342.859188	17.628851
35.108147	1338.460204	17.633869
35.095936	1346.166841	17.638887
35.146456	1354.146948	17.643904
35.120061	1362.622857	17.648922
34.991110	1361.666708	17.653939
35.363189	1356.488694	17.658957
35.371774	1364.885192	17.663975
35.284751	1362.249295	17.668992
35.386283	1363.712417	17.674010
35.034301	1369.768665	17.679027
35.428921	1361.680276	17.684045
35.488077	1365.822021	17.689063
35.489956	1361.106086	17.694080
35.306595	1360.339651	17.699098
35.232945	1359.118838	17.704115
35.693642	1363.131889	17.709133
35.724188	1374.597535	17.714151
35.924935	1363.774760	17.719168
35.487352	1368.183794	17.724186
35.555447	1368.663100	17.729203
36.238751	1357.701371	17.734221
35.997389	1366.389646	17.739239
35.758587	1366.097737	17.744256
35.739570	1364.669455	17.749274
35.574981	1359.688965	17.754291
36.026143	1364.760663	17.759309
35.780988	1361.024593	17.764327
35.571916	1357.769547	17.769344
35.598764	1365.272880	17.774362
35.658133	1362.715890	17.779379
35.667884	1368.388230	17.784397
35.755236	1388.147485	17.789415
36.074607	1391.104042	17.794432
35.946698	1393.350816	17.799450
35.631263	1397.590028	17.804467
35.615872	1387.797892	17.809485
35.861876	1399.580630	17.814503
36.293953	1409.660544	17.819520
36.414755	1415.402306	17.824538
36.111647	1419.771765	17.829555
36.479320	1406.928041	17.834573
36.393667	1418.155484	17.839591
36.710847	1411.999549	17.844608
36.926980	1413.253545	17.849626
36.506545	1413.354304	17.854643
36.517843	1406.801390	17.859661
36.820484	1418.530277	17.864679
36.979540	1413.493422	17.869696
37.052558	1408.108616	17.874714
36.835548	1414.009463	17.879731
36.930585	1417.344111	17.884749
36.631903	1423.613597	17.889767
36.782438	1419.053736	17.894784
36.855702	1414.571237	17.899802
36.844579	1414.891224	17.904819
36.726729	1404.446761	17.909837
36.913331	1401.348233	17.914855
36.916714	1411.569604	17.919872
36.779880	1400.876716	17.924890
36.926080	1410.537833	17.929907
37.254958	1409.930668	17.934925
37.099977	1417.170437	17.939943
37.132692	1418.654802	17.944960
37.129737	1415.205775	17.949978
36.879625	1426.309670	17.954995
37.140641	1426.189325	17.960013
37.016635	1441.010880	17.965031
37.470342	1435.219727	17.970048
37.649677	1439.626627	17.975066
37.598054	1431.491622	17.980083
38.003190	1422.144391	17.985101
38.039777	1430.515028	17.990119
37.843631	1407.032136	17.995136
37.730480	1397.119175	18.000154
37.747958	1398.735981	18.005171
37.738219	1380.379270	18.010189
37.587139	1395.097786	18.015207
37.798176	1394.509740	18.020224
37.758241	1385.242921	18.025242
37.982157	1388.734172	18.030259
38.028562	1392.430012	18.035277
37.631241	1394.169043	18.040295
37.696350	1409.056102	18.045312
37.952973	1411.449440	18.050330
37.631912	1427.076828	18.055347
37.966662	1415.344045	18.060365
37.928563	1417.005094	18.065383
38.002980	1420.021902	18.070400
38.351253	1422.230382	18.075418
37.977463	1421.471067	18.080435
38.087245	1419.999800	18.085453
38.187051	1433.006755	18.090471
38.128190	1424.680829	18.095488
38.370778	1414.227857	18.100506
38.514005	1434.451534	18.105523
38.554510	1425.089483	18.110541
38.573778	1429.731937	18.115559
38.717146	1428.064559	18.120576
38.830600	1417.204627	18.125594
38.535525	1420.236554	18.130611
38.683604	1413.343670	18.135629
38.679098	1422.764792	18.140647
38.732696	1422.894932	18.145664
38.962300	1415.218873	18.150682
38.709424	1417.754843	18.155699
38.928225	1418.477303	18.160717
39.146704	1420.963178	18.165735
39.096139	1419.513737	18.170752
39.077132	1420.938557	18.175770
38.771609	1420.034082	18.180787
39.028813	1409.434994	18.185805
39.002959	1415.176631	18.190823
38.764684	1428.425781	18.195840
39.007523	1430.664713	18.200858
38.986559	1441.431073	18.205875
39.388253	1431.566304	18.210893
39.179248	1433.622184	18.215911
39.394479	1443.899442	18.220928
39.243102	1432.604223	18.225946
39.005189	1434.146393	18.230963
39.121545	1432.916946	18.235981
39.319243	1439.472352	18.240999
38.933499	1437.692981	18.246016
39.071666	1442.949602	18.251034
39.394132	1464.497953	18.256051
40.012885	1464.011290	18.261069
39.813631	1481.579171	18.266087
39.686256	1468.347295	18.271104
39.749003	1468.005058	18.276122
39.726775	1474.948073	18.281139
40.067979	1468.745619	18.286157
39.956694	1463.653119	18.291175
39.743590	1476.702081	18.296192
39.933553	1466.922741	18.301210
39.904956	1475.225850	18.306227
39.890029	1465.049340	18.311245
39.900450	1463.013426	18.316263
39.737585	1468.484859	18.321280
39.941869	1464.106634	18.326298
39.864539	1469.415875	18.331315
40.144243	1469.360939	18.336333
39.915701	1473.918063	18.341351
39.671860	1476.153337	18.346368
40.010433	1477.124863	18.351386
40.284446	1495.894303	18.356403
40.478962	1500.258944	18.361421
40.575617	1495.726092	18.366439
40.425337	1496.156129	18.371456
40.684218	1496.410150	18.376474
40.684916	1502.410413	18.381491
40.701157	1491.555502	18.386509
40.891009	1492.147722	18.391527
40.677772	1492.325195	18.396544
40.796965	1490.624805	18.401562
40.561842	1492.718876	18.406579
40.801728	1487.640661	18.411597
40.879817	1484.776224	18.416615
40.719892	1487.705077	18.421632
40.891644	1484.798360	18.426650
40.793561	1495.089737	18.431667
40.612461	1488.656047	18.436685
40.837743	1483.388915	18.441703
40.865475	1484.772144	18.446720
41.210875	1480.505191	18.451738
40.870744	1495.048809	18.456755
41.039025	1488.154909	18.461773
41.051670	1503.471608	18.466791
41.053251	1513.872872	18.471808
41.606152	1510.514065	18.476826
41.260927	1513.008255	18.481843
41.677783	1515.566021	18.486861
41.767406	1513.400057	18.491879
41.696933	1512.780668	18.496896
41.445822	1506.578640	18.501914
41.513264	1509.963940	18.506931
41.802323	1518.056601	18.511949
41.765826	1512.824537	18.516967
41.131986	1517.757443	18.521984
41.832500	1508.810067	18.527002
41.811564	1509.011996	18.532019
41.686898	1519.090864	18.537037
42.095244	1511.590671	18.542055
41.501954	1511.829894	18.547072
41.920592	1507.226007	18.552090
41.792175	1512.786240	18.557107
41.742994	1513.701502	18.562125
41.727701	1512.048182	18.567143
41.635201	1518.024513	18.572160
42.274324	1534.189470	18.577178
41.654221	1546.361007	18.582195
42.217402	1549.428404	18.587213
42.169438	1534.790810	18.592231
41.800651	1544.290041	18.597248
42.460471	1544.080827	18.602266
42.200674	1537.329834	18.607283
42.219546	1536.833839	18.612301
42.240791	1534.338252	18.617319
42.236256	1539.021688	18.622336
42.523910	1530.115496	18.627354
42.303061	1542.141393	18.632371
42.470394	1551.671148	18.637389
42.593069	1567.014572	18.642407
42.518977	1568.053253	18.647424
42.995294	1558.632344	18.652442
42.731693	1561.787433	18.657459
42.936693	1557.923233	18.662477
43.251890	1556.064792	18.667495
43.139348	1550.003974	18.672512
43.188661	1554.078502	18.677530
42.944497	1558.707922	18.682547
43.026030	1562.422788	18.687565
43.457279	1553.381390	18.692583
43.223747	1556.885433	18.697600
43.446247	1552.969125	18.702618
43.411973	1535.441091	18.707635
43.244957	1529.025524	18.712653
43.361428	1514.874104	18.717671
42.843083	1518.559943	18.722688
43.408283	1540.889462	18.727706
43.688145	1553.356865	18.732723
43.164059	1556.492486	18.737741
43.597812	1554.179378	18.742759
43.525237	1560.251638	18.747776
43.688338	1558.660112	18.752794
43.731804	1556.289582	18.757811
43.434885	1552.538414	18.762829
43.726136	1551.575272	18.767847
43.613184	1563.351037	18.772864
43.497253	1550.948687	18.777882
43.884450	1555.730255	18.782899
43.648028	1563.611921	18.787917
43.959161	1544.003860	18.792935
43.564133	1550.535411	18.797952
43.564670	1574.632877	18.802970
44.034634	1581.219639	18.807987
43.844044	1586.289800	18.813005
44.030808	1580.408544	18.818023
43.517562	1582.103404	18.823040
43.814192	1586.061792	18.828058
44.115315	1596.922172	18.833075
44.309845	1600.316763	18.838093
44.569088	1606.088036	18.843111
44.388359	1610.883739	18.848128
44.595802	1608.102978	18.853146
44.629160	1613.716381	18.858163
44.437936	1612.732338	18.863181
44.579344	1599.057419	18.868199
44.666541	1605.989460	18.873216
44.811569	1612.334763	18.878234
44.677715	1601.261716	18.883251
44.709529	1598.374606	18.888269
44.980140	1600.949515	18.893287
44.705073	1601.705729	18.898304
44.940988	1599.146240	18.903322
45.124377	1597.105289	18.908339
44.968518	1598.649636	18.913357
45.100397	1601.325075	18.918375
44.889641	1601.879696	18.923392
45.346997	1600.792591	18.928410
45.045844	1601.220448	18.933427
44.886181	1603.746919	18.938445
44.938233	1602.078108	18.943463
44.817913	1619.915358	18.948480
45.097548	1622.209643	18.953498
44.965545	1624.272089	18.958515
45.001750	1632.266126	18.963533
45.428458	1620.867963	18.968551
45.580803	1627.286076	18.973568
45.420762	1627.196868	18.978586
45.414330	1616.261766	18.983603
45.485026	1633.211893	18.988621
45.944664	1644.929523	18.993639
46.002448	1653.067636	18.998656
46.380679	1638.606225	19.003674
46.352264	1619.214529	19.008691
46.055142	1625.646436	19.013709
46.253502	1608.256571	19.018727
45.972278	1616.106311	19.023744
46.279662	1615.255061	19.028762
46.620529	1617.553774	19.033779
46.078805	1613.605725	19.038797
46.125450	1603.870109	19.043815
46.161642	1625.275142	19.048832
46.136513	1605.686856	19.053850
46.084292	1610.567973	19.058867
45.874683	1612.251929	19.063885
45.921056	1608.667526	19.068903
45.949006	1618.329849	19.073920
46.141038	1631.250046	19.078938
46.057117	1639.208860	19.083955
46.092525	1647.136896	19.088973
46.167851	1650.376433	19.093991
46.269268	1656.804960	19.099008
46.344766	1661.696048	19.104026
46.599310	1664.071266	19.109043
46.418176	1667.883194	19.114061
47.052040	1663.986932	19.119079
47.173873	1659.888447	19.124096
47.305089	1673.136466	19.129114
47.317287	1663.306910	19.134131
46.982409	1667.323035	19.139149
47.318913	1662.205931	19.144167
47.439079	1663.183318	19.149184
47.442070	1660.290733	19.154202
47.330882	1653.767838	19.159219
47.502358	1666.910367	19.164237
47.418711	1659.150230	19.169255
47.444539	1659.912530	19.174272
47.401500	1663.635055	19.179290
47.614012	1659.874705	19.184307
47.479675	1655.269424	19.189325
47.159821	1661.708260	19.194343
47.547653	1664.585030	19.199360
47.267180	1664.918520	19.204378
47.591514	1647.953422	19.209395
47.349991	1664.193075	19.214413
47.784403	1670.781431	19.219431
47.818855	1690.041956	19.224448
47.845122	1697.153418	19.229466
48.047223	1688.445555	19.234483
47.935173	1688.966906	19.239501
47.896047	1693.774621	19.244519
47.914546	1692.251907	19.249536
47.692676	1694.974126	19.254554
47.896827	1694.637212	19.259571
48.010481	1676.788460	19.264589
48.296785	1690.984046	19.269607
48.383102	1680.760708	19.274624
47.968406	1680.412878	19.279642
48.749718	1694.469021	19.284659
48.509997	1699.687907	19.289677
48.692437	1685.699030	19.294695
48.619892	1678.332323	19.299712
48.635628	1692.155386	19.304730
48.507075	1683.566844	19.309747
48.724849	1701.806081	19.314765
48.764911	1701.725865	19.319783
48.806077	1692.641890	19.324800
48.852832	1708.246058	19.329818
49.196997	1693.439842	19.334835
48.862714	1704.838975	19.339853
49.292453	1701.613908	19.344871
49.198245	1687.855091	19.349888
48.905087	1682.216254	19.354906
49.242865	1678.682009	19.359923
49.077543	1699.340982	19.364941
49.436502	1704.204438	19.369959
49.483284	1701.914833	19.374976
49.105906	1696.031668	19.379994
49.694684	1701.799593	19.385011
49.256255	1706.480909	19.390029
49.401929	1701.650902	19.395047
49.413949	1699.742645	19.400064
49.712866	1707.266842	19.405082
49.636118	1698.934675	19.410099
49.448452	1710.724104	19.415117
49.400820	1700.680808	19.420135
49.681171	1693.931253	19.425152
49.441419	1709.078530	19.430170
49.380895	1700.394461	19.435187
49.192985	1709.047698	19.440205
49.557422	1724.424082	19.445223
49.864379	1723.273290	19.450240
49.248006	1725.925797	19.455258
49.623126	1728.622400	19.460275
49.949342	1750.261081	19.465293
50.107203	1746.415664	19.470311
50.485624	1742.837273	19.475328
50.442185	1748.759506	19.480346
50.741706	1741.978803	19.485363
50.854056	1750.020924	19.490381
51.093000	1749.898327	19.495399
50.953808	1721.718487	19.500416
50.509138	1713.850384	19.505434
50.757863	1709.429298	19.510451
50.830534	1718.926011	19.515469
50.854575	1716.340168	19.520487
50.995156	1712.214154	19.525504
50.548003	1720.223705	19.530522
50.665448	1717.357434	19.535539
50.659772	1718.987555	19.540557
50.899845	1729.906563	19.545575
50.929969	1739.147734	19.550592
51.146762	1747.080433	19.555610
50.974866	1738.800219	19.560627
51.042963	1735.141717	19.565645
51.477017	1745.154989	19.570663
51.669947	1733.452143	19.575680
51.269040	1740.256008	19.580698
51.099188	1744.501523	19.585715
51.086866	1735.795279	19.590733
51.168372	1737.644433	19.595751
51.228428	1741.705814	19.600768
51.061426	1743.865410	19.605786
51.549142	1751.643408	19.610803
51.283417	1773.937227	19.615821
51.189627	1774.207523	19.620839
51.697280	1770.589223	19.625856
51.468264	1778.712292	19.630874
51.553646	1772.457196	19.635891
51.744308	1769.928007	19.640909
51.806465	1776.863483	19.645927
51.895664	1779.810590	19.650944
52.126162	1801.734486	19.655962
52.210523	1798.303199	19.660979
52.149201	1805.811501	19.665997
52.301741	1797.597616	19.671015
52.507938	1793.850091	19.676032
52.545445	1794.454950	19.681050
52.746212	1798.297375	19.686067
52.542057	1785.966532	19.691085
52.653195	1774.483894	19.696103
52.591324	1758.274756	19.701120
52.348826	1776.620215	19.706138
52.965442	1782.312301	19.711155
52.789885	1777.025221	19.716173
52.394853	1790.228192	19.721191
52.872110	1793.772864	19.726208
52.768484	1800.017684	19.731226
52.899622	1792.667590	19.736243
53.041390	1788.658684	19.741261
52.495554	1790.590854	19.746279
53.023868	1792.021540	19.751296
53.057673	1797.597139	19.756314
53.419138	1788.475034	19.761331
53.293135	1790.682966	19.766349
52.845049	1788.300484	19.771367
52.973128	1781.758783	19.776384
53.229668	1795.471593	19.781402
53.410421	1809.554055	19.786419
53.521396	1813.304658	19.791437
53.440043	1816.730018	19.796455
53.746531	1808.966625	19.801472
53.532093	1808.069091	19.806490
53.685355	1807.052010	19.811507
53.810456	1806.299438	19.816525
53.547206	1812.721876	19.821543
53.976155	1801.466519	19.826560
54.014227	1810.461924	19.831578
54.239992	1808.634799	19.836595
54.220410	1810.608968	19.841613
54.182533	1808.739275	19.846631
54.168436	1802.723475	19.851648
54.246073	1800.234650	19.856666
54.174518	1799.334323	19.861683
54.423001	1804.215711	19.866701
54.292569	1805.162554	19.871719
54.297696	1798.076239	19.876736
54.098575	1800.431713	19.881754
54.150796	1792.773030	19.886771
54.356172	1804.619498	19.891789
54.564117	1817.995883	19.896807
55.082134	1816.225485	19.901824
54.736093	1826.929009	19.906842
54.846502	1836.003004	19.911859
54.971119	1826.737808	19.916877
54.765524	1835.076323	19.921895
54.768209	1826.588412	19.926912
54.582916	1829.354205	19.931930
54.793036	1834.653377	19.936947
54.974193	1829.951709	19.941965
54.542543	1826.890113	19.946983
54.842444	1828.792881	19.952000
54.754925	1853.036463	19.957018
55.074556	1859.480125	19.962035
55.625501	1850.227002	19.967053
55.236725	1858.723421	19.972071
55.312562	1853.224214	19.977088
55.434703	1853.448914	19.982106
55.461547	1849.167680	19.987123
55.473652	1853.507900	19.992141
55.740676	1852.937734	19.997159
55.631323	1843.306539	20.002176
55.720085	1842.773764	20.007194
55.801697	1845.742220	20.012211
55.893247	1846.725145	20.017229
56.126299	1873.077125	20.022247
56.073182	1871.022543	20.027264
56.282040	1870.901385	20.032282
56.347537	1867.359425	20.037299
56.033312	1863.969712	20.042317
56.236496	1865.750702	20.047335
56.379859	1869.850686	20.052352
56.616902	1867.519316	20.057370
56.473344	1874.642444	20.062387
56.585222	1869.376243	20.067405
56.537256	1861.428598	20.072423
56.697216	1861.745464	20.077440
56.713735	1866.094799	20.082458
56.537221	1871.498554	20.087475
56.841521	1858.768891	20.092493
56.626270	1860.053014	20.097511
56.709766	1863.993222	20.102528
56.812456	1861.488821	20.107546
56.680925	1863.460668	20.112563
57.149218	1861.155970	20.117581
56.698718	1869.111426	20.122599
56.757176	1867.945076	20.127616
56.970578	1875.606746	20.132634
57.186004	1883.073986	20.137651
57.367378	1893.032342	20.142669
57.380378	1899.205921	20.147687
57.218810	1894.397594	20.152704
57.073234	1886.084596	20.157722
57.208075	1885.562695	20.162739
57.689946	1884.367968	20.167757
57.395314	1884.765617	20.172775
57.297811	1898.309579	20.177792
57.433685	1908.977065	20.182810
57.883885	1908.900986	20.187827
57.981700	1901.987074	20.192845
57.788636	1915.883493	20.197863
57.964426	1906.884191	20.202880
58.088222	1903.649898	20.207898
58.127093	1911.117646	20.212915
58.392720	1902.784978	20.217933
58.238356	1909.060290	20.222951
58.199257	1906.807710	20.227968
58.521504	1906.428009	20.232986
58.013729	1904.867216	20.238003
58.358199	1903.017668	20.243021
58.206787	1916.298913	20.248039
58.232876	1928.466901	20.253056
59.004227	1936.965367	20.258074
58.589803	1936.164718	20.263091
58.961186	1926.062526	20.268109
58.736812	1933.513635	20.273127
58.700179	1935.178039	20.278144
59.031346	1940.414684	20.283162
58.655681	1945.295130	20.288179
59.013403	1934.209742	20.293197
58.705492	1925.709031	20.298215
59.060675	1926.441613	20.303232
58.840688	1934.579410	20.308250
58.919521	1953.557712	20.313267
59.535353	1946.445801	20.318285
59.435439	1962.683184	20.323303
59.055570	1950.338783	20.328320
59.553077	1953.519110	20.333338
59.492590	1960.398202	20.338355
59.528894	1948.161275	20.343373
59.850152	1959.167399	20.348391
59.797149	1960.764043	20.353408
59.733383	1963.044766	20.358426
59.525266	1954.152705	20.363443
59.740893	1948.883866	20.368461
59.560980	1953.056692	20.373479
59.722926	1974.280751	20.378496
59.984766	1974.560671	20.383514
59.977111	1978.869945	20.388531
60.253488	1981.993583	20.393549
60.133802	1975.260144	20.398567
60.168243	1979.556936	20.403584
60.338092	1973.822824	20.408602
60.078710	1983.936109	20.413619
60.568589	1979.549429	20.418637
60.226649	1995.819047	20.423655
60.421261	2009.320642	20.428672
60.884932	1998.092466	20.433690
60.786810	2004.600636	20.438707
60.915439	2008.075522	20.443725
60.784597	2005.809378	20.448743
61.150151	1998.806602	20.453760
61.315975	2002.042252	20.458778
60.924941	1995.447043	20.463795
61.156104	1992.788275	20.468813
61.177561	2000.177844	20.473831
61.355140	1994.849146	20.478848
61.396700	1986.127935	20.483866
61.242406	1988.467354	20.488883
61.254542	1996.906126	20.493901
61.043622	1994.807970	20.498919
61.033675	1993.661993	20.503936
61.442704	2008.791903	20.508954
61.408044	2018.305389	20.513971
61.536234	2021.170100	20.518989
61.593424	2020.333879	20.524007
61.537170	2019.839677	20.529024
62.092588	2026.479413	20.534042
62.021390	2028.542080	20.539059
62.114293	2021.421443	20.544077
62.078355	2019.798654	20.549095
61.938089	2027.028395	20.554112
62.372321	2037.135531	20.559130
62.274377	2041.139686	20.564147
62.345248	2048.270696	20.569165
62.785402	2044.303660	20.574183
62.341275	2045.450100	20.579200
62.536074	2039.222449	20.584218
62.643483	2040.095672	20.589235
62.572336	2034.745544	20.594253
62.843418	2043.666676	20.599271
62.390337	2050.089146	20.604288
62.731191	2038.428116	20.609306
62.397367	2044.945801	20.614323
62.765535	2041.002102	20.619341
62.991934	2059.275373	20.624359
63.237499	2068.598394	20.629376
63.389229	2071.509218	20.634394
62.840288	2071.716689	20.639411
62.878501	2074.444335	20.644429
63.393197	2068.180242	20.649447
63.221559	2063.634166	20.654464
63.723906	2068.748414	20.659482
63.417874	2069.184176	20.664499
63.318725	2069.912463	20.669517
63.715192	2074.429661	20.674535
63.526229	2071.901075	20.679552
63.498406	2070.736398	20.684570
63.723799	2068.853791	20.689587
63.951497	2083.248423	20.694605
63.793529	2087.323947	20.699623
63.813849	2089.422257	20.704640
63.754746	2092.288071	20.709658
63.901150	2094.341489	20.714675
63.958557	2099.553830	20.719693
64.176069	2094.946066	20.724711
64.230378	2097.518292	20.729728
64.091433	2095.410567	20.734746
64.237721	2104.655555	20.739763
64.563240	2113.046045	20.744781
64.800252	2117.474300	20.749799
64.731448	2123.559541	20.754816
64.785901	2104.550774	20.759834
64.606664	2115.661928	20.764851
64.911349	2117.676149	20.769869
65.078860	2113.898731	20.774887
65.090323	2120.487626	20.779904
65.216710	2110.146739	20.784922
65.297583	2110.733406	20.789939
65.128893	2106.819920	20.794957
65.501828	2095.981906	20.799975
65.108642	2115.590153	20.804992
65.221514	2100.217499	20.810010
65.099764	2103.301568	20.815027
65.220152	2100.455212	20.820045
65.573863	2120.976441	20.825063
65.511544	2134.134455	20.830080
65.886431	2135.007884	20.835098
65.606008	2140.958088	20.840115
66.005302	2141.519593	20.845133
66.038647	2133.129591	20.850151
65.799300	2136.469366	20.855168
66.151232	2134.816989	20.860186
66.232511	2133.194858	20.865203
66.256516	2137.043407	20.870221
66.573194	2134.284627	20.875239
66.163012	2144.565116	20.880256
66.362652	2136.110569	20.885274
66.377143	2132.373445	20.890291
66.441360	2135.877924	20.895309
66.487662	2134.322610	20.900327
66.518121	2135.087710	20.905344
66.287085	2135.718149	20.910362
66.462887	2148.395394	20.915379
66.286220	2166.450876	20.920397
66.822785	2159.910281	20.925415
66.403370	2174.295211	20.930432
66.642599	2159.425611	20.935450
66.827490	2176.189306	20.940467
67.028014	2183.296549	20.945485
67.132107	2176.125168	20.950503
67.151628	2188.362559	20.955520
67.470558	2179.322076	20.960538
67.428850	2179.106966	20.965555
67.550236	2192.287764	20.970573
67.812574	2180.990822	20.975591
67.516720	2184.169091	20.980608
67.675652	2175.537005	20.985626
67.676146	2183.760870	20.990643
67.433364	2186.560654	20.995661
67.447941	2182.055366	21.000679
67.636056	2205.414066	21.005696
67.878418	2203.976288	21.010714
68.032471	2204.968180	21.015731
68.163062	2212.493723	21.020749
68.283854	2207.444838	21.025767
68.050675	2210.042635	21.030784
68.053166	2204.398356	21.035802
68.539096	2207.942872	21.040819
68.005946	2204.606655	21.045837
68.716141	2206.031284	21.050855
68.271054	2221.042972	21.055872
68.544040	2226.455890	21.060890
68.616592	2227.855387	21.065907
68.667112	2239.040008	21.070925
68.766369	2227.718458	21.075943
68.920483	2231.809277	21.080960
69.106453	2224.301864	21.085978
69.173878	2231.876460	21.090995
69.005662	2225.005272	21.096013
68.974631	2217.221970	21.101031
68.946678	2240.806270	21.106048
69.266168	2257.069796	21.111066
69.777850	2261.140790	21.116083
69.690212	2261.640793	21.121101
69.859091	2254.522037	21.126119
69.889359	2261.955156	21.131136
70.161864	2249.288316	21.136154
70.078517	2253.489722	21.141171
69.881980	2240.105639	21.146189
70.283159	2230.810947	21.151207
69.888365	2238.490820	21.156224
69.875228	2245.046044	21.161242
69.986984	2240.616385	21.166259
70.057437	2249.661410	21.171277
70.375039	2241.366022	21.176295
70.234860	2241.119183	21.181312
70.200244	2244.506975	21.186330
70.417548	2239.587381	21.191347
70.206446	2246.676584	21.196365
70.567257	2242.745472	21.201383
70.614186	2265.750854	21.206400
70.566961	2272.616864	21.211418
70.919073	2268.157243	21.216435
70.533433	2271.211807	21.221453
70.832936	2269.933073	21.226471
70.790029	2276.635765	21.231488
70.607672	2273.969432	21.236506
70.794730	2289.050539	21.241523
70.768231	2297.676588	21.246541
71.327773	2306.086310	21.251559
71.253156	2301.206370	21.256576
71.474143	2304.419958	21.261594
71.624040	2291.626922	21.266611
71.426626	2293.916436	21.271629
71.607122	2301.085319	21.276647
71.816928	2312.950342	21.281664
72.121437	2320.671954	21.286682
72.196346	2313.401007	21.291699
71.994018	2310.062749	21.296717
72.108200	2307.378807	21.301735
72.230259	2313.805765	21.306752
72.458187	2317.665872	21.311770
72.697201	2312.701320	21.316787
72.388442	2307.359337	21.321805
72.644295	2296.332689	21.326823
72.467199	2296.853410	21.331840
72.480415	2283.568030	21.336858
72.546430	2286.584430	21.341875
72.428163	2300.966072	21.346893
72.623457	2299.744355	21.351911
72.644055	2300.148088	21.356928
72.809233	2305.974571	21.361946
72.723852	2309.110929	21.366963
72.726828	2305.282359	21.371981
72.514281	2302.439122	21.376999
72.781966	2323.867028	21.382016
72.768548	2330.529425	21.387034
72.802679	2329.559598	21.392051
72.889123	2342.119508	21.397069
72.988145	2349.332614	21.402087
73.396204	2360.875858	21.407104
73.646472	2367.878488	21.412122
73.808741	2358.663044	21.417139
73.658157	2358.551790	21.422157
73.734139	2358.264827	21.427175
73.859032	2357.211462	21.432192
74.166507	2353.111981	21.437210
74.140340	2355.494809	21.442227
73.775161	2361.974507	21.447245
74.317927	2372.857631	21.452263
74.386699	2390.192386	21.457280
74.209665	2389.340987	21.462298
74.355416	2383.788676	21.467315
74.249107	2396.631345	21.472333
74.253350	2386.739653	21.477351
75.055063	2388.249941	21.482368
74.794526	2378.076884	21.487386
74.918702	2387.676113	21.492403
75.022348	2379.276702	21.497421
75.134355	2385.949460	21.502439
75.053252	2375.906544	21.507456
75.040296	2381.231028	21.512474
75.147925	2378.913532	21.517491
74.947728	2385.096225	21.522509
74.908592	2395.011489	21.527527
75.308908	2389.911932	21.532544
75.697157	2400.547419	21.537562
75.985200	2393.050585	21.542579
75.778804	2400.970615	21.547597
75.939495	2390.322273	21.552615
75.849801	2392.657748	21.557632
76.084970	2389.699418	21.562650
76.159722	2382.668240	21.567667
75.915631	2383.606769	21.572685
76.127610	2387.404571	21.577703
76.201091	2389.952410	21.582720
76.092080	2381.058261	21.587738
76.143712	2387.055157	21.592755
75.886578	2388.304916	21.597773
76.228878	2403.510832	21.602791
76.636632	2408.830630	21.607808
76.553445	2417.887806	21.612826
76.838445	2414.685382	21.617843
76.722629	2412.911595	21.622861
77.149791	2413.062178	21.627879
77.176944	2411.187157	21.632896
76.843883	2414.912210	21.637914
76.866319	2411.893031	21.642931
76.878478	2418.067349	21.647949
77.106315	2416.972919	21.652967
77.348667	2410.149817	21.657984
77.217642	2417.069532	21.663002
77.176772	2429.293489	21.668019
77.271618	2440.605174	21.673037
77.552617	2438.364480	21.678055
77.606024	2444.223696	21.683072
77.164278	2436.600025	21.688090
77.833285	2431.291391	21.693107
77.542770	2434.327086	21.698125
77.862514	2441.621018	21.703143
78.046302	2455.611434	21.708160
78.041316	2455.875699	21.713178
78.195852	2461.253191	21.718195
78.503417	2462.448434	21.723213
78.435708	2453.474567	21.728231
78.658041	2455.619404	21.733248
78.415626	2460.709847	21.738266
78.500360	2452.268643	21.743283
78.771583	2451.767846	21.748301
79.178196	2452.448631	21.753319
79.042416	2447.120875	21.758336
78.644104	2459.460734	21.763354
78.599837	2453.552439	21.768371
78.788329	2450.530168	21.773389
78.772889	2453.560087	21.778407
79.036935	2468.079774	21.783424
79.104890	2486.974304	21.788442
79.190908	2476.588280	21.793459
79.167344	2475.981952	21.798477
79.091407	2483.300471	21.803495
79.280199	2497.683031	21.808512
79.368996	2503.812015	21.813530
79.618257	2499.918602	21.818547
79.939907	2510.071463	21.823565
80.102956	2504.785552	21.828583
80.132934	2499.586639	21.833600
79.789112	2502.068544	21.838618
79.783400	2499.925317	21.843635
80.236950	2511.128053	21.848653
80.233700	2530.445471	21.853671
80.920880	2527.914665	21.858688
80.684934	2533.085167	21.863706
80.696899	2529.986985	21.868723
80.970226	2535.871243	21.873741
80.898367	2539.560558	21.878759
80.812453	2528.829323	21.883776
81.009084	2530.380361	21.888794
80.660816	2530.348296	21.893811
80.743756	2521.755374	21.898829
80.742118	2531.934218	21.903847
81.140961	2544.713843	21.908864
81.059266	2557.565956	21.913882
81.462026	2558.672606	21.918899
81.689959	2553.296797	21.923917
81.310872	2562.328636	21.928935
81.662039	2552.636499	21.933952
81.690856	2563.229243	21.938970
81.696446	2557.993008	21.943987
81.802433	2552.110587	21.949005
81.695086	2556.632602	21.954023
82.052654	2570.408904	21.959040
81.919291	2585.011825	21.964058
81.919522	2582.154567	21.969075
82.089532	2586.413725	21.974093
82.003663	2582.948637	21.979111
82.379013	2584.770108	21.984128
82.073949	2600.590127	21.989146
82.612484	2609.953160	21.994163
82.902466	2607.828285	21.999181
82.646014	2614.724364	22.004199
82.881044	2608.484314	22.009216
82.656278	2607.552611	22.014234
82.927770	2607.292331	22.019251
83.283835	2602.939843	22.024269
83.073894	2605.694497	22.029287
83.200949	2604.883293	22.034304
83.519531	2601.200044	22.039322
83.514456	2598.409807	22.044339
83.551259	2602.005550	22.049357
83.561388	2600.414051	22.054375
83.458607	2589.407204	22.059392
83.562548	2622.980307	22.064410
83.745194	2619.576664	22.069427
83.529561	2627.765678	22.074445
83.226477	2627.826531	22.079463
83.796352	2619.687612	22.084480
83.958639	2654.464978	22.089498
83.888572	2661.815682	22.094515
84.259097	2658.516759	22.099533
83.954253	2659.010215	22.104551
84.356407	2654.347699	22.109568
84.319450	2665.742005	22.114586
84.776087	2665.588874	22.119603
85.129418	2674.953476	22.124621
84.737126	2671.772190	22.129639
85.424255	2669.985121	22.134656
85.363278	2673.447454	22.139674
85.338728	2666.999557	22.144691
85.495428	2668.152469	22.149709
85.444886	2666.964341	22.154727
85.620153	2660.712905	22.159744
85.868610	2659.327624	22.164762
85.465241	2657.302188	22.169779
86.005742	2654.775569	22.174797
85.750831	2661.561956	22.179815
85.851086	2656.715947	22.184832
85.846802	2663.249801	22.189850
85.746953	2660.235859	22.194867
86.017905	2656.336847	22.199885
85.852921	2664.952956	22.204903
85.800084	2660.864624	22.209920
86.048263	2668.510692	22.214938
86.023064	2681.222048	22.219955
86.083429	2690.893845	22.224973
85.858357	2692.333214	22.229991
86.421195	2691.998314	22.235008
86.624621	2700.803855	22.240026
86.697775	2714.378934	22.245043
86.618270	2707.963743	22.250061
86.806737	2717.748608	22.255079
87.200029	2708.986079	22.260096
87.386355	2707.985123	22.265114
86.748952	2709.765224	22.270131
87.155122	2729.323389	22.275149
86.805929	2743.428691	22.280167
87.290174	2747.695318	22.285184
87.474786	2745.465423	22.290202
87.343528	2749.857978	22.295219
87.672660	2746.464309	22.300237
87.463393	2767.642640	22.305255
87.933323	2772.235683	22.310272
87.971616	2763.051553	22.315290
88.150498	2768.547177	22.320307
88.009170	2767.786702	22.325325
87.985697	2767.041755	22.330343
88.311168	2761.863520	22.335360
88.239127	2780.811115	22.340378
88.877718	2793.910331	22.345395
88.941292	2787.878928	22.350413
88.558373	2795.995326	22.355431
88.647913	2795.267889	22.360448
88.989509	2789.577095	22.365466
88.968154	2785.621717	22.370483
89.273470	2785.791693	22.375501
88.858316	2780.881365	22.380519
89.155446	2774.318347	22.385536
89.414969	2773.713958	22.390554
89.138440	2784.227872	22.395571
89.442300	2786.284842	22.400589
89.379920	2804.945413	22.405607
89.442282	2811.592714	22.410624
90.148583	2809.168550	22.415642
89.912238	2808.227333	22.420659
89.752023	2802.595602	22.425677
89.745596	2811.102461	22.430695
90.036562	2807.822586	22.435712
90.320880	2803.453968	22.440730
90.074965	2809.996392	22.445747
90.563859	2825.411539	22.450765
90.386280	2842.580089	22.455783
90.459907	2841.090266	22.460800
90.800202	2838.650707	22.465818
90.390960	2844.230348	22.470835
90.804918	2831.912481	22.475853
90.731579	2840.708015	22.480871
90.851242	2844.409002	22.485888
91.051369	2860.133826	22.490906
90.958919	2860.892538	22.495923
91.058016	2852.383380	22.500941
91.228720	2859.751403	22.505959
91.290896	2860.622319	22.510976
91.791451	2861.564365	22.515994
91.409393	2870.917764	22.521011
91.786357	2880.849489	22.526029
91.781918	2889.532454	22.531047
91.764274	2887.289172	22.536064
91.880168	2874.697368	22.541082
91.829766	2885.412904	22.546099
92.070573	2879.687580	22.551117
92.228195	2901.138049	22.556135
92.454075	2906.867299	22.561152
92.795239	2911.090728	22.566170
92.942008	2908.485548	22.571187
92.864960	2901.531637	22.576205
92.782992	2912.876485	22.581223
92.783842	2903.978022	22.586240
92.986283	2901.212038	22.591258
92.644253	2909.869013	22.596275
92.900794	2900.395890	22.601293
93.104080	2927.921612	22.606311
93.074074	2931.014671	22.611328
93.302511	2936.059593	22.616346
93.539448	2939.708112	22.621363
93.768148	2934.789958	22.626381
93.472393	2935.516581	22.631399
93.432421	2939.038492	22.636416
93.597237	2949.591657	22.641434
93.585981	2961.587486	22.646451
93.925808	2960.187446	22.651469
93.908012	2963.276914	22.656487
93.900475	2963.258515	22.661504
94.279999	2975.380221	22.666522
94.083293	2995.692533	22.671539
94.292604	2992.724985	22.676557
94.453078	2996.144817	22.681575
94.468781	2995.358331	22.686592
95.000791	3000.637682	22.691610
95.045508	3014.888656	22.696627
95.112427	3012.084062	22.701645
95.459232	3023.077265	22.706663
95.432159	3015.666957	22.711680
95.796573	3007.952443	22.716698
95.570818	2990.314697	22.721715
95.703818	2975.089043	22.726733
95.587194	2981.855429	22.731751
95.544560	2997.383557	22.736768
95.771421	3002.908332	22.741786
95.647613	3011.948166	22.746803
95.728979	3000.968418	22.751821
95.881434	3011.437837	22.756839
96.088223	3010.701214	22.761856
96.207464	3006.435862	22.766874
96.096913	3010.696311	22.771891
96.032762	3017.367796	22.776909
96.220748	3036.509283	22.781927
96.476598	3035.107785	22.786944
96.656415	3042.708659	22.791962
96.639326	3045.684237	22.796979
96.827946	3044.093851	22.801997
97.124771	3056.830154	22.807015
97.036246	3062.160690	22.812032
97.442670	3054.903019	22.817050
97.501505	3059.246469	22.822067
97.339439	3058.639820	22.827085
97.444879	3057.747125	22.832103
97.552759	3051.244069	22.837120
97.777748	3048.766873	22.842138
97.360802	3061.528831	22.847155
97.901600	3070.410231	22.852173
98.110587	3082.292515	22.857191
97.989859	3076.776599	22.862208
98.363942	3069.410487	22.867226
98.322901	3078.378382	22.872243
98.487173	3072.860560	22.877261
98.690163	3078.840143	22.882279
98.381867	3078.464023	22.887296
98.324736	3075.454345	22.892314
98.483627	3094.035315	22.897331
98.791479	3106.014644	22.902349
98.735576	3107.522900	22.907367
98.954216	3106.694145	22.912384
98.728980	3102.296021	22.917402
98.699876	3120.922716	22.922419
98.995047	3125.966495	22.927437
99.222804	3129.822898	22.932455
99.430719	3140.142656	22.937472
99.783905	3135.103032	22.942490
99.736306	3154.006477	22.947507
99.947061	3163.213862	22.952525
99.753303	3159.913766	22.957543
99.671843	3161.873546	22.962560
100.223889	3152.766346	22.967578
100.219748	3155.256683	22.972595
100.311896	3141.019223	22.977613
100.655643	3155.068044	22.982631
100.768709	3178.342984	22.987648
100.913325	3178.371054	22.992666
100.851594	3174.995154	22.997683
100.607262	3180.709829	23.002701
101.515147	3169.207645	23.007719
101.164779	3178.988699	23.012736
101.045325	3170.582490	23.017754
101.165137	3175.663588	23.022771
101.344634	3169.405737	23.027789
101.546112	3163.968739	23.032807
101.287993	3168.565899	23.037824
101.665787	3162.924101	23.042842
101.604091	3180.542779	23.047859
101.539455	3189.857986	23.052877
102.126850	3200.235439	23.057895
102.061601	3204.420716	23.062912
101.838256	3195.237127	23.067930
101.724693	3194.170427	23.072947
102.048750	3209.352198	23.077965
102.452938	3216.345085	23.082983
102.309036	3221.378906	23.088000
102.624380	3224.570765	23.093018
102.498279	3233.887907	23.098035
102.293364	3235.051123	23.103053
102.863928	3236.808066	23.108071
103.225332	3254.728467	23.113088
103.297124	3257.621646	23.118106
103.380427	3266.675372	23.123123
103.232715	3254.198569	23.128141
103.335872	3255.813588	23.133159
103.283480	3260.610200	23.138176
103.225403	3258.073922	23.143194
103.816411	3270.640421	23.148211
103.758313	3290.141107	23.153229
104.041991	3277.529862	23.158247
103.896726	3279.206095	23.163264
104.293382	3278.800268	23.168282
104.203348	3275.886166	23.173299
104.261020	3287.734993	23.178317
104.362462	3294.500451	23.183335
104.260083	3314.757792	23.188352
104.427196	3310.046196	23.193370
104.741380	3293.314092	23.198387
104.696406	3309.833574	23.203405
105.359942	3327.331555	23.208423
105.246048	3336.968819	23.213440
105.140557	3336.424058	23.218458
105.269973	3327.596203	23.223475
105.404986	3332.135407	23.228493
105.654749	3334.555779	23.233511
105.570359	3335.687629	23.238528
105.732712	3342.335925	23.243546
106.227071	3359.269367	23.248563
105.816922	3367.441360	23.253581
106.160347	3361.264965	23.258599
106.300807	3359.943968	23.263616
106.073628	3355.603580	23.268634
106.387143	3351.370937	23.273651
106.328970	3360.301275	23.278669
106.666397	3364.010430	23.283687
106.434624	3378.909550	23.288704
106.704460	3383.609537	23.293722
106.947836	3382.314811	23.298739
106.763455	3394.297112	23.303757
107.149908	3388.311243	23.308775
107.430007	3404.252534	23.313792
107.199677	3400.219777	23.318810
107.285638	3409.553099	23.323827
107.317221	3412.774654	23.328845
107.864713	3404.386649	23.333863
107.707418	3414.556402	23.338880
107.645302	3419.891742	23.343898
107.467593	3433.404246	23.348915
108.038361	3438.069782	23.353933
107.943301	3438.940777	23.358951
108.122330	3441.696143	23.363968
108.484737	3449.185085	23.368986
108.858425	3458.399136	23.374003
108.769469	3459.430558	23.379021
108.902893	3450.593701	23.384039
108.838372	3460.050405	23.389056
108.910148	3460.897323	23.394074
109.344851	3451.501469	23.399091
109.231477	3448.545919	23.404109
109.386110	3450.950560	23.409127
109.363475	3451.162245	23.414144
109.481827	3452.404253	23.419162
109.390692	3452.430407	23.424179
109.476710	3459.288659	23.429197
109.467870	3471.450247	23.434215
109.328890	3489.111992	23.439232
109.531891	3472.770985	23.444250
110.051026	3495.716537	23.449267
109.710267	3511.326035	23.454285
110.128448	3511.656491	23.459303
110.103793	3518.915816	23.464320
110.242332	3517.481331	23.469338
110.765197	3532.706888	23.474355
110.374757	3540.820976	23.479373
110.845366	3528.855827	23.484391
110.837947	3542.691848	23.489408
110.865526	3555.966900	23.494426
111.308943	3546.133667	23.499443
111.161563	3562.964895	23.504461
111.235828	3567.537063	23.509479
111.412146	3562.923093	23.514496
111.647902	3579.722798	23.519514
111.796681	3591.478414	23.524531
111.954634	3594.917303	23.529549
112.175417	3575.399225	23.534567
112.201456	3584.151161	23.539584
111.762794	3593.880546	23.544602
112.368218	3597.887556	23.549619
112.778891	3613.750350	23.554637
113.026456	3605.166196	23.559655
112.992530	3607.335118	23.564672
112.815761	3611.761436	23.569690
113.169673	3616.348743	23.574707
113.101638	3616.456123	23.579725
113.470582	3608.475178	23.584743
113.660110	3605.537960	23.589760
113.371316	3610.336020	23.594778
113.640096	3606.606448	23.599795
113.692093	3608.559937	23.604813
113.676092	3611.159411	23.609831
113.927814	3626.418534	23.614848
113.543952	3641.619496	23.619866
113.832485	3638.421754	23.624883
113.895188	3634.999165	23.629901
113.911729	3649.849159	23.634919
114.278825	3666.199598	23.639936
114.223794	3662.869339	23.644954
114.615310	3659.444673	23.649971
114.794666	3666.977416	23.654989
114.976381	3680.186103	23.660007
114.982340	3689.380849	23.665024
115.084749	3689.908100	23.670042
115.328076	3680.732403	23.675059
115.203797	3678.982709	23.680077
115.339882	3684.301468	23.685095
115.734290	3691.808461	23.690112
115.735546	3701.431608	23.695130
115.985133	3701.430881	23.700147
115.972625	3710.697605	23.705165
115.850246	3710.853751	23.710183
116.121148	3704.871931	23.715200
116.444809	3711.926412	23.720218
116.489597	3705.507950	23.725235
116.605192	3705.832992	23.730253
116.733753	3706.765416	23.735271
116.565703	3699.569489	23.740288
116.331743	3712.179220	23.745306
116.543439	3721.110758	23.750323
116.612538	3734.949636	23.755341
116.707037	3735.182882	23.760359
116.971511	3752.498167	23.765376
116.912035	3760.366206	23.770394
117.355579	3764.079940	23.775411
117.125805	3776.247237	23.780429
117.647583	3785.337738	23.785447
117.819385	3789.809558	23.790464
118.012523	3801.503256	23.795482
118.075417	3795.402277	23.800499
118.137663	3800.169049	23.805517
118.183796	3798.092661	23.810535
118.522508	3804.198892	23.815552
118.636012	3819.015668	23.820570
118.760340	3815.360365	23.825587
118.867388	3816.197918	23.830605
119.099078	3816.369470	23.835623
119.218617	3808.328523	23.840640
119.205352	3810.767712	23.845658
119.562489	3801.081695	23.850675
119.377101	3807.710588	23.855693
119.537154	3824.882984	23.860711
119.771207	3842.685363	23.865728
119.911962	3837.745658	23.870746
120.007956	3838.427540	23.875763
120.083521	3845.980309	23.880781
119.821837	3839.190821	23.885799
120.262393	3827.028819	23.890816
120.036555	3850.451041	23.895834
120.336750	3859.741681	23.900851
120.260093	3856.959526	23.905869
120.457123	3859.093394	23.910887
121.133218	3874.246273	23.915904
120.990797	3882.276553	23.920922
121.239152	3877.614732	23.925939
121.056186	3889.184124	23.930957
121.164988	3886.728397	23.935975
121.517144	3878.693789	23.940992
121.458635	3889.081780	23.946010
121.820877	3901.808338	23.951027
121.871604	3913.346539	23.956045
122.254241	3903.944469	23.961063
122.488523	3901.791240	23.966080
122.434612	3910.156537	23.971098
122.591796	3904.088730	23.976115
122.411896	3901.123632	23.981133
122.371002	3904.278536	23.986151
122.811626	3906.696537	23.991168
122.802830	3931.231537	23.996186
122.874736	3923.120059	24.001203
122.916746	3932.236528	24.006221
123.050735	3932.287623	24.011239
123.052631	3924.993366	24.016256
122.899070	3949.739003	24.021274
123.469897	3955.192600	24.026291
123.469736	3956.916545	24.031309
123.313938	3952.995337	24.036327
123.897474	3968.699538	24.041344
123.733092	3987.193339	24.046362
123.952431	3987.427971	24.051379
124.242018	3989.677261	24.056397
124.047268	3989.432337	24.061415
124.769681	3997.584885	24.066432
124.694219	4017.072025	24.071450
125.008532	4004.027502	24.076467
125.160539	4016.493247	24.081485
125.176586	4011.522158	24.086503
125.295294	4007.297969	24.091520
125.072420	4003.252400	24.096538
125.166687	4001.930336	24.101555
125.297795	3997.260722	24.106573
125.469071	4009.079080	24.111591
125.761366	4023.176974	24.116608
125.329965	4027.593983	24.121626
125.538427	4043.675368	24.126643
125.754119	4048.960990	24.131661
125.705095	4060.128352	24.136679
126.010475	4060.461356	24.141696
125.875442	4074.036252	24.146714
125.931723	4091.834484	24.151731
126.352541	4099.554266	24.156749
126.223004	4107.673092	24.161767
126.646988	4117.616333	24.166784
127.047207	4121.621623	24.171802
127.434104	4116.948214	24.176819
127.354874	4128.266318	24.181837
127.374858	4141.890423	24.186855
128.382237	4147.322214	24.191872
127.842171	4139.021347	24.196890
128.291193	4143.569833	24.201907
128.136947	4147.177874	24.206925
128.111141	4137.199485	24.211943
128.697459	4131.650400	24.216960
128.600620	4141.578294	24.221978
128.503690	4137.928440	24.226995
128.578315	4155.365382	24.232013
128.717985	4160.373818	24.237031
129.055612	4159.702899	24.242048
129.122782	4168.659409	24.247066
129.096559	4163.140062	24.252083
129.043044	4167.552823	24.257101
129.256968	4190.836197	24.262119
129.320605	4185.687855	24.267136
129.386557	4196.011734	24.272154
129.388631	4200.727951	24.277171
129.703141	4217.381029	24.282189
129.764027	4215.125736	24.287207
129.895452	4217.954093	24.292224
130.324603	4236.988609	24.297242
130.577291	4250.185240	24.302259
130.912296	4263.540723	24.307277
130.796431	4260.189301	24.312295
130.748923	4249.917533	24.317312
130.650867	4268.387295	24.322330
130.949185	4271.140778	24.327347
131.144104	4277.289904	24.332365
131.046451	4279.519083	24.337383
131.555274	4282.787417	24.342400
131.489655	4300.754124	24.347418
131.395998	4312.877248	24.352435
131.793205	4299.613210	24.357453
131.599944	4310.816443	24.362471
132.055254	4315.741169	24.367488
131.985284	4326.901951	24.372506
132.136776	4328.356691	24.377523
132.524524	4346.014492	24.382541
132.628802	4362.545811	24.387559
132.776906	4357.332238	24.392576
133.036236	4357.122384	24.397594
133.065870	4358.519336	24.402611
133.271063	4349.105822	24.407629
133.087602	4364.753912	24.412647
133.651383	4382.213288	24.417664
133.536358	4390.983516	24.422682
133.653529	4386.066445	24.427699
133.756804	4390.562778	24.432717
133.745621	4387.134932	24.437735
134.060288	4404.202430	24.442752
134.275544	4415.269586	24.447770
134.112648	4421.130703	24.452787
134.394074	4410.731130	24.457805
134.414410	4414.253625	24.462823
134.467179	4424.138813	24.467840
134.895826	4435.661294	24.472858
134.963193	4442.887697	24.477875
135.340590	4441.788848	24.482893
135.606363	4465.955545	24.487911
135.842541	4458.564761	24.492928
135.824767	4467.355945	24.497946
135.899909	4466.151202	24.502963
136.214217	4463.194743	24.507981
135.928770	4464.138266	24.512999
136.392167	4468.471832	24.518016
136.398651	4469.377262	24.523034
136.537648	4464.728255	24.528051
136.632228	4478.731712	24.533069
136.665727	4498.996042	24.538087
136.731593	4492.388696	24.543104
136.924736	4492.785971	24.548122
137.154171	4500.398242	24.553139
137.131015	4507.616036	24.558157
137.092050	4522.197648	24.563175
137.388392	4519.510344	24.568192
137.584750	4516.313512	24.573210
137.542428	4535.183096	24.578227
138.157992	4537.367473	24.583245
137.340389	4554.615505	24.588263
137.902618	4551.002909	24.593280
138.084507	4569.888180	24.598298
138.253900	4581.392262	24.603315
138.787685	4577.974955	24.608333
138.614586	4595.300614	24.613351
139.047020	4600.463909	24.618368
139.366272	4609.641977	24.623386
139.059018	4611.720043	24.628403
139.434061	4602.877584	24.633421
139.365457	4607.819050	24.638439
139.731739	4626.606132	24.643456
139.890628	4637.120466	24.648474
140.178569	4634.249458	24.653491
140.097240	4629.281695	24.658509
140.218845	4637.590755	24.663527
140.254072	4635.140400	24.668544
140.481524	4638.428617	24.673562
140.320234	4658.116623	24.678579
140.766955	4654.718440	24.683597
140.908825	4667.254899	24.688615
140.814455	4661.629314	24.693632
140.969792	4687.892990	24.698650
141.074063	4692.800349	24.703667
141.218526	4693.114333	24.708685
141.287606	4708.754818	24.713703
141.290162	4707.478594	24.718720
141.790890	4721.943476	24.723738
141.410411	4723.628874	24.728755
141.661651	4730.592639	24.733773
141.641466	4744.950832	24.738791
141.920664	4745.921385	24.743808
142.639791	4760.447802	24.748826
142.568065	4767.244536	24.753843
143.115603	4759.279912	24.758861
142.868999	4775.522444	24.763879
143.309723	4772.607216	24.768896
143.216733	4768.398184	24.773914
143.349324	4790.211363	24.778931
143.864652	4789.902418	24.783949
143.753467	4800.500165	24.788967
144.113262	4799.304975	24.793984
144.332266	4789.402988	24.799002
143.872764	4795.810299	24.804019
143.926124	4791.247043	24.809037
144.105870	4805.575342	24.814055
144.164033	4819.097630	24.819072
144.564238	4823.668576	24.824090
144.295575	4841.268647	24.829107
144.564912	4850.806374	24.834125
144.691456	4858.976123	24.839143
144.792388	4872.614237	24.844160
145.227905	4877.277798	24.849178
144.925020	4894.251966	24.854195
145.437277	4901.473443	24.859213
145.823755	4906.750770	24.864231
145.720949	4910.392209	24.869248
146.150985	4917.303616	24.874266
146.425924	4931.756457	24.879283
146.806613	4929.537111	24.884301
146.625222	4929.268694	24.889319
146.644476	4929.808179	24.894336
147.095570	4930.495902	24.899354
147.018648	4954.256209	24.904371
146.917555	4951.474755	24.909389
147.469391	4962.220376	24.914407
147.333651	4953.555220	24.919424
147.888789	4965.361152	24.924442
147.598492	4985.746658	24.929459
147.581320	4982.459862	24.934477
148.016708	4981.108018	24.939495
148.134297	4999.819373	24.944512
148.772332	5007.094895	24.949530
148.321899	5021.596240	24.954547
148.636840	5014.683602	24.959565
148.975988	5025.488107	24.964583
149.012226	5025.017480	24.969600
149.646846	5036.356665	24.974618
149.145633	5040.064094	24.979635
149.529342	5040.616489	24.984653
149.709723	5044.420570	24.989671
149.730297	5041.844203	24.994688
150.161585	5035.389563	24.999706
150.005290	5062.807273	25.004723
150.208669	5068.296110	25.009741
150.443854	5071.851702	25.014759
150.591544	5072.712524	25.019776
150.947865	5062.287522	25.024794
150.447045	5075.602509	25.029811
150.530239	5090.441649	25.034829
150.943435	5096.725864	25.039847
151.046819	5098.042153	25.044864
151.315715	5112.571768	25.049882
151.583648	5129.038995	25.054899
151.387823	5128.459508	25.059917
151.862876	5125.885855	25.064935
151.866858	5129.786105	25.069952
152.545762	5133.861295	25.074970
152.288864	5149.090728	25.079987
152.272651	5143.073206	25.085005
152.424389	5137.164131	25.090023
152.475597	5141.767748	25.095040
152.620755	5148.380675	25.100058
152.737369	5172.243157	25.105075
152.893077	5163.190187	25.110093
153.149650	5166.567417	25.115111
152.988377	5194.506769	25.120128
153.492740	5193.149790	25.125146
153.258544	5204.766038	25.130163
153.387052	5213.638168	25.135181
153.679755	5227.673285	25.140199
153.733130	5233.302001	25.145216
153.928751	5254.698997	25.150234
153.984303	5274.734637	25.155251
154.443968	5269.325843	25.160269
154.982331	5287.923773	25.165287
154.675377	5296.042654	25.170304
155.238974	5288.371242	25.175322
155.373012	5293.333717	25.180339
155.716958	5302.153691	25.185357
155.877772	5304.829314	25.190375
156.117197	5317.445438	25.195392
156.029289	5308.237396	25.200410
156.246684	5318.660591	25.205427
156.251132	5310.369760	25.210445
156.418433	5311.512455	25.215463
156.503578	5346.212088	25.220480
156.538381	5338.506908	25.225498
156.597002	5341.452271	25.230515
156.672186	5358.541553	25.235533
156.820078	5355.914128	25.240551
157.118063	5372.803509	25.245568
157.177106	5376.385969	25.250586
157.286557	5397.068115	25.255603
157.337970	5402.640511	25.260621
157.550937	5421.849297	25.265639
157.687133	5428.489816	25.270656
158.435673	5438.276205	25.275674
158.639886	5450.651749	25.280691
158.778163	5459.883119	25.285709
159.046628	5457.060083	25.290727
158.869702	5461.809462	25.295744
158.959026	5461.465499	25.300762
159.077957	5472.572190	25.305779
159.258483	5480.960152	25.310797
159.888619	5474.745711	25.315815
159.873121	5482.479345	25.320832
160.085677	5497.211604	25.325850
160.189152	5508.448469	25.330867
160.404814	5506.830524	25.335885
160.513294	5508.729613	25.340903
160.720505	5495.989065	25.345920
160.730569	5499.926204	25.350938
161.097925	5520.511472	25.355955
161.237456	5520.347431	25.360973
161.721088	5521.566938	25.365991
161.443669	5521.127746	25.371008
161.713154	5518.520332	25.376026
161.921735	5520.297312	25.381043
161.908164	5523.354686	25.386061
161.920711	5540.121381	25.391079
161.652118	5556.299834	25.396096
162.294907	5559.481681	25.401114
162.474328	5566.837330	25.406131
162.618200	5577.168118	25.411149
163.178897	5588.128507	25.416167
162.857173	5589.092275	25.421184
163.025686	5578.518455	25.426202
163.051893	5588.944341	25.431219
163.491991	5606.520860	25.436237
163.487453	5608.175613	25.441255
163.343857	5624.632730	25.446272
163.643615	5619.869347	25.451290
163.912027	5627.507218	25.456307
163.643936	5638.134653	25.461325
163.878722	5648.545736	25.466343
163.735647	5671.072085	25.471360
164.162841	5682.838308	25.476378
164.420234	5702.226744	25.481395
164.621056	5702.524331	25.486413
164.996394	5711.029022	25.491431
165.065526	5727.564443	25.496448
165.247764	5729.060695	25.501466
165.620740	5745.772663	25.506483
165.780950	5756.716774	25.511501
166.072223	5760.509759	25.516519
166.208320	5763.642428	25.521536
166.095321	5762.928698	25.526554
166.350010	5774.454975	25.531571
166.550132	5790.174078	25.536589
166.784905	5781.467603	25.541607
166.845973	5795.866070	25.546624
167.219576	5806.847348	25.551642
167.380681	5808.939389	25.556659
167.671125	5820.533816	25.561677
168.078365	5821.391091	25.566695
167.798822	5839.789560	25.571712
167.871568	5832.345646	25.576730
168.159140	5832.819476	25.581747
168.357580	5850.291355	25.586765
168.895550	5856.472521	25.591783
169.178970	5866.110925	25.596800
169.118181	5863.658947	25.601818
169.031903	5868.242219	25.606835
169.239863	5880.703331	25.611853
169.633851	5882.662314	25.616871
169.447308	5904.519630	25.621888
169.512276	5899.449271	25.626906
169.814347	5899.655277	25.631923
169.788670	5921.534030	25.636941
169.823774	5929.966784	25.641959
170.090601	5944.807832	25.646976
170.419016	5958.221771	25.651994
170.929415	5949.236440	25.657011
170.929916	5975.001765	25.662029
171.191034	5972.333442	25.667047
171.437574	5990.156666	25.672064
171.009117	5987.540278	25.677082
171.582473	5999.306170	25.682100
171.741260	6010.501156	25.687117
171.890296	6021.633966	25.692135
172.162718	6029.598232	25.697152
172.024527	6025.730297	25.702170
172.391591	6036.267811	25.707188
172.163481	6038.941787	25.712205
172.505757	6057.524259	25.717223
172.936346	6066.256283	25.722240
172.908985	6069.308957	25.727258
173.179830	6081.100575	25.732276
173.140952	6097.295895	25.737293
173.468675	6102.036743	25.742311
173.647489	6115.913504	25.747328
173.730722	6121.140630	25.752346
174.243665	6125.704324	25.757364
174.455516	6147.436948	25.762381
175.085028	6137.470098	25.767399
175.341980	6149.098665	25.772416
175.071197	6142.080875	25.777434
175.169525	6141.987449	25.782452
175.082493	6138.772624	25.787469
175.478451	6137.289383	25.792487
175.404496	6155.739246	25.797504
175.506783	6169.748442	25.802522
175.681705	6170.222818	25.807540
175.667402	6186.194412	25.812557
176.157885	6190.657876	25.817575
176.192392	6208.133661	25.822592
176.422082	6211.456497	25.827610
176.660383	6225.981966	25.832628
176.717988	6230.158732	25.837645
177.101985	6232.763698	25.842663
176.862914	6257.301057	25.847680
177.256628	6262.414606	25.852698
177.960333	6256.989498	25.857716
178.139409	6289.462401	25.862733
177.982074	6279.973073	25.867751
178.246487	6284.772504	25.872768
178.286484	6283.721518	25.877786
178.586457	6298.455806	25.882804
178.679662	6317.773726	25.887821
178.887543	6313.463273	25.892839
178.987397	6319.516307	25.897856
179.237811	6348.399290	25.902874
179.458613	6342.540557	25.907892
179.548660	6348.617280	25.912909
179.763181	6355.945434	25.917927
180.260926	6360.591265	25.922944
180.166649	6373.295773	25.927962
180.468071	6366.216234	25.932980
180.409665	6388.546853	25.937997
180.774153	6394.878250	25.943015
180.674851	6401.954350	25.948032
180.513907	6420.265331	25.953050
180.830981	6421.859838	25.958068
181.161931	6451.728405	25.963085
181.829750	6458.741332	25.968103
181.858156	6463.128569	25.973120
181.580568	6472.946860	25.978138
182.086696	6482.289637	25.983156
182.058867	6479.347706	25.988173
182.254398	6503.807195	25.993191
182.651535	6510.614486	25.998208
182.518939	6518.675981	26.003226
183.320263	6523.481905	26.008244
183.349260	6544.524649	26.013261
183.251968	6544.085535	26.018279
183.714367	6559.864378	26.023296
183.742799	6573.626235	26.028314
184.184923	6567.796943	26.033332
184.176649	6587.874744	26.038349
184.433782	6597.017790	26.043367
184.673384	6597.784717	26.048384
185.205661	6594.962705	26.053402
185.211051	6600.240684	26.058420
185.062872	6612.606165	26.063437
185.454157	6622.068070	26.068455
185.709580	6620.882154	26.073472
185.752098	6628.936769	26.078490
185.723728	6640.854743	26.083508
185.638869	6654.123451	26.088525
185.949239	6648.978358	26.093543
186.301747	6674.118648	26.098560
186.460178	6689.703770	26.103578
186.829441	6683.078365	26.108596
187.220657	6693.609171	26.113613
187.223504	6710.079401	26.118631
187.200581	6717.732163	26.123648
187.172785	6724.153053	26.128666
187.238144	6721.053871	26.133684
187.491005	6737.314970	26.138701
187.741494	6747.439836	26.143719
188.253401	6762.253682	26.148736
188.011584	6775.932065	26.153754
188.661639	6770.814190	26.158772
188.321088	6787.784802	26.163789
188.646968	6801.107722	26.168807
188.938310	6805.335739	26.173824
189.206747	6827.836563	26.178842
189.435428	6833.832234	26.183860
189.632051	6839.421268	26.188877
189.917761	6854.260044	26.193895
190.253209	6866.811889	26.198912
190.315104	6874.386884	26.203930
190.729511	6882.020887	26.208948
190.439135	6888.377403	26.213965
190.730879	6892.321030	26.218983
191.114411	6908.284989	26.224000
191.452355	6917.855935	26.229018
191.652275	6916.219191	26.234036
191.773210	6928.155197	26.239053
191.705253	6935.594972	26.244071
192.179699	6942.250235	26.249088
192.051403	6947.935630	26.254106
192.341714	6960.276838	26.259124
192.505288	6969.834148	26.264141
192.547692	6977.426597	26.269159
192.762680	6993.327175	26.274176
192.944763	7003.082296	26.279194
193.696043	7014.383914	26.284212
193.399512	7035.801781	26.289229
193.281017	7037.485001	26.294247
193.899750	7053.689793	26.299264
193.669480	7073.952254	26.304282
194.000890	7081.783622	26.309300
194.664909	7092.560972	26.314317
194.668947	7099.569075	26.319335
195.265857	7105.767762	26.324352
194.970129	7125.964720	26.329370
195.324136	7122.059144	26.334388
195.593694	7143.996255	26.339405
195.868368	7160.254176	26.344423
196.620283	7156.414262	26.349440
196.366569	7158.742932	26.354458
196.942773	7164.252701	26.359476
196.878875	7176.388844	26.364493
197.098031	7186.460889	26.369511
197.424548	7187.197705	26.374528
197.119234	7183.461126	26.379546
197.261742	7184.099225	26.384564
197.479576	7201.281094	26.389581
197.485894	7212.016172	26.394599
197.512238	7220.328973	26.399616
197.569251	7243.124533	26.404634
197.938117	7252.136822	26.409652
198.082004	7269.831973	26.414669
198.587131	7281.566012	26.419687
198.789025	7292.747679	26.424704
199.058169	7313.724117	26.429722
199.070800	7320.955385	26.434740
199.375511	7330.325709	26.439757
199.515072	7341.175874	26.444775
199.663479	7339.579910	26.449792
200.157785	7359.420311	26.454810
200.308252	7364.756447	26.459828
200.583113	7359.203469	26.464845
200.240719	7377.176163	26.469863
200.772511	7397.343598	26.474880
200.491598	7403.695600	26.479898
201.024234	7409.979879	26.484916
201.420921	7429.664024	26.489933
201.291739	7435.723105	26.494951
201.535584	7441.745642	26.499968
201.580126	7468.440302	26.504986
201.861443	7478.160384	26.510004
202.273634	7491.428638	26.515021
202.375768	7512.079311	26.520039
202.899055	7521.529355	26.525056
203.117467	7522.690536	26.530074
203.402655	7532.612448	26.535092
203.739929	7544.673794	26.540109
203.655095	7556.774307	26.545127
203.819477	7554.914162	26.550144
203.929222	7571.852809	26.555162
204.584040	7573.812944	26.560180
204.847291	7579.798449	26.565197
204.925440	7592.116195	26.570215
205.199181	7597.366622	26.575232
205.200041	7604.564522	26.580250
205.367130	7611.689219	26.585268
205.340972	7624.559105	26.590285
205.467816	7637.133492	26.595303
205.749990	7641.256912	26.600320
206.099532	7660.267786	26.605338
206.235385	7667.489841	26.610356
206.279300	7686.520620	26.615373
206.381524	7701.614272	26.620391
207.004436	7716.828121	26.625408
207.076815	7723.528220	26.630426
207.341123	7728.558120	26.635444
207.448869	7746.774157	26.640461
207.440396	7758.060295	26.645479
208.029501	7760.198327	26.650496
208.591305	7772.429056	26.655514
208.861140	7774.991741	26.660532
209.204697	7770.051115	26.665549
209.265171	7802.608975	26.670567
209.596066	7803.451439	26.675584
209.685363	7812.762396	26.680602
209.384224	7806.655544	26.685620
209.881454	7821.153003	26.690637
209.597392	7836.880246	26.695655
210.004532	7835.491894	26.700672
210.320253	7854.700013	26.705690
209.974283	7878.698288	26.710708
210.581567	7877.081447	26.715725
210.538337	7898.584572	26.720743
210.632562	7905.218902	26.725760
211.135103	7922.046422	26.730778
211.137401	7942.543246	26.735796
211.622111	7946.338612	26.740813
211.711538	7958.646897	26.745831
212.213284	7982.908306	26.750848
212.275891	7986.228456	26.755866
212.708277	7995.905730	26.760884
213.052769	8008.389239	26.765901
212.983695	8026.444239	26.770919
213.462096	8034.382508	26.775936
213.957627	8048.759935	26.780954
213.720753	8051.702731	26.785972
214.290837	8049.822632	26.790989
214.224654	8048.017140	26.796007
214.545932	8052.754133	26.801024
214.626269	8076.604148	26.806042
214.431388	8066.822993	26.811060
215.376456	8084.331281	26.816077
215.408353	8094.768109	26.821095
215.576661	8098.305528	26.826112
215.492926	8091.977460	26.831130
215.714892	8107.885088	26.836148
215.796435	8117.461395	26.841165
216.180371	8135.296583	26.846183
216.538417	8155.021109	26.851200
216.552025	8160.776396	26.856218
216.601705	8168.365057	26.861236
217.067004	8177.820369	26.866253
217.594432	8194.470759	26.871271
217.448161	8196.882620	26.876288
217.798022	8217.203313	26.881306
217.720375	8222.873687	26.886324
217.998203	8231.380128	26.891341
218.307894	8250.491257	26.896359
218.922316	8255.340480	26.901376
218.856777	8272.184427	26.906394
219.064490	8281.289363	26.911412
219.528517	8280.554830	26.916429
219.139470	8296.707161	26.921447
219.452613	8308.519432	26.926464
220.010145	8334.941565	26.931482
219.875995	8345.474579	26.936500
220.264805	8353.068632	26.941517
220.089705	8372.508297	26.946535
220.499587	8378.334341	26.951552
220.905327	8396.980735	26.956570
221.025531	8407.507919	26.961588
221.756308	8415.760661	26.966605
221.860138	8428.915320	26.971623
221.753775	8443.621187	26.976640
222.499955	8460.936734	26.981658
222.424502	8469.181961	26.986676
222.893860	8476.023049	26.991693
222.840519	8494.650237	26.996711
223.263160	8498.070019	27.001728
223.423637	8510.933356	27.006746
223.076718	8532.978372	27.011764
223.695983	8538.175853	27.016781
223.741552	8554.072164	27.021799
224.282644	8560.743864	27.026816
225.011267	8583.772045	27.031834
224.697834	8583.163049	27.036852
224.977177	8582.051023	27.041869
225.060210	8610.122931	27.046887
225.240042	8616.641766	27.051904
225.481276	8625.716929	27.056922
225.616593	8649.416115	27.061940
225.815658	8650.093753	27.066957
226.040841	8677.744434	27.071975
226.164096	8681.418632	27.076992
226.837800	8689.367439	27.082010
226.907366	8708.802459	27.087028
227.480720	8711.770376	27.092045
227.219481	8726.545468	27.097063
227.483939	8734.268999	27.102080
227.692854	8751.464259	27.107098
227.872140	8768.389514	27.112116
228.376661	8765.222753	27.117133
228.743761	8787.548526	27.122151
228.301561	8794.996762	27.127168
228.773085	8806.401122	27.132186
228.977915	8827.712395	27.137204
229.254233	8829.120111	27.142221
229.349195	8839.920385	27.147239
229.696228	8844.138945	27.152256
230.033062	8848.333198	27.157274
229.977835	8868.538230	27.162292
230.401705	8877.625843	27.167309
230.275720	8896.042586	27.172327
230.741535	8909.720663	27.177344
230.932534	8924.704670	27.182362
231.468131	8942.930021	27.187380
231.642943	8944.297832	27.192397
231.420211	8962.959119	27.197415
231.824542	8980.112822	27.202432
232.178120	8983.359806	27.207450
232.593786	9003.289328	27.212468
233.343639	9006.495926	27.217485
233.461952	9020.061465	27.222503
233.430108	9026.221623	27.227520
233.733094	9031.759162	27.232538
233.768460	9052.746653	27.237556
234.299665	9049.872412	27.242573
234.358791	9059.276533	27.247591
234.249259	9090.904077	27.252608
234.847885	9083.707973	27.257626
234.941195	9111.059034	27.262644
235.033653	9118.955387	27.267661
235.192202	9131.725010	27.272679
235.407672	9148.739211	27.277696
235.733382	9165.016729	27.282714
236.017490	9175.065890	27.287732
236.316352	9190.371034	27.292749
236.422865	9204.582298	27.297767
236.476160	9223.301393	27.302784
237.043815	9230.806390	27.307802
236.882013	9248.266011	27.312820
237.515031	9264.142984	27.317837
237.878830	9283.841169	27.322855
238.017475	9306.504841	27.327872
238.563791	9307.726106	27.332890
238.551287	9322.087159	27.337908
238.765645	9333.611671	27.342925
239.067918	9341.521457	27.347943
239.045761	9358.538978	27.352960
239.685295	9376.047278	27.357978
239.830560	9386.448064	27.362996
239.993118	9400.491090	27.368013
240.252825	9406.666942	27.373031
240.319601	9432.253569	27.378048
240.278619	9437.255770	27.383066
240.798486	9452.869633	27.388084
241.025162	9471.427968	27.393101
241.453220	9480.278107	27.398119
241.519332	9493.625016	27.403136
242.031671	9498.945295	27.408154
242.350342	9523.994060	27.413172
242.294054	9515.637830	27.418189
242.577344	9540.031518	27.423207
242.359970	9558.691821	27.428224
243.052296	9571.882352	27.433242
243.557372	9588.054192	27.438260
243.455599	9601.853605	27.443277
243.751050	9619.474276	27.448295
243.664335	9636.790325	27.453312
244.189018	9645.921563	27.458330
244.615533	9655.845039	27.463348
244.774549	9667.442764	27.468365
245.678739	9684.908381	27.473383
245.348846	9690.506796	27.478400
245.782526	9687.023861	27.483418
245.759504	9704.394040	27.488436
246.072878	9718.166585	27.493453
245.986668	9716.681704	27.498471
245.751497	9745.703219	27.503488
246.359913	9749.592780	27.508506
246.911455	9771.188247	27.513524
247.131842	9784.925034	27.518541
247.284505	9800.087159	27.523559
247.372126	9810.376439	27.528576
247.852779	9820.639268	27.533594
247.995533	9837.090349	27.538612
248.300132	9858.899342	27.543629
248.400549	9858.419526	27.548647
248.624531	9880.757910	27.553664
249.046765	9887.449059	27.558682
249.409381	9915.842517	27.563700
249.533424	9929.363759	27.568717
250.160489	9945.078531	27.573735
249.885946	9965.435479	27.578752
250.129019	9971.459892	27.583770
250.331339	9990.712986	27.588788
250.647928	10013.036224	27.593805
251.159110	10019.833242	27.598823
251.599754	10039.020158	27.603840
251.856674	10055.352511	27.608858
252.442211	10064.572393	27.613876
252.110923	10088.064963	27.618893
252.445099	10088.535163	27.623911
252.523687	10112.991968	27.628928
253.367132	10109.080292	27.633946
253.510015	10117.682558	27.638964
253.629343	10143.299433	27.643981
253.884651	10147.554008	27.648999
254.101517	10184.517607	27.654016
254.349003	10173.971012	27.659034
254.646642	10188.147569	27.664052
255.007230	10198.246165	27.669069
255.218269	10204.296452	27.674087
255.078421	10232.360821	27.679104
255.271724	10238.629921	27.684122
255.510214	10256.081095	27.689140
255.524302	10275.000135	27.694157
256.000795	10290.326560	27.699175
256.161265	10307.080868	27.704192
256.557740	10328.091396	27.709210
256.814205	10359.010883	27.714228
257.242989	10358.523180	27.719245
257.639028	10385.145607	27.724263
257.574370	10401.273920	27.729280
257.978289	10420.587122	27.734298
258.347241	10438.135074	27.739316
258.292141	10453.029676	27.744333
258.750219	10468.976198	27.749351
258.950867	10492.534932	27.754368
259.137408	10501.075816	27.759386
259.550357	10518.844259	27.764404
260.166027	10530.016426	27.769421
260.330638	10547.525052	27.774439
260.520388	10558.707866	27.779456
260.495431	10576.613463	27.784474
261.028704	10587.815067	27.789492
261.114976	10608.139885	27.794509
261.536767	10607.091598	27.799527
261.540526	10634.161478	27.804544
261.873555	10645.336391	27.809562
262.064320	10648.758785	27.814580
262.493327	10670.619981	27.819597
262.761260	10680.668038	27.824615
263.101025	10701.274032	27.829632
263.403191	10701.753491	27.834650
263.931526	10715.023325	27.839668
263.678999	10727.527425	27.844685
264.214103	10737.885827	27.849703
264.230470	10760.218830	27.854720
264.459308	10765.179143	27.859738
264.938544	10769.685172	27.864756
264.851318	10792.708196	27.869773
265.367871	10798.298450	27.874791
265.222611	10820.664594	27.879808
265.312039	10832.699333	27.884826
265.753344	10856.849838	27.889844
265.415526	10889.877757	27.894861
266.052272	10896.763879	27.899879
266.634059	10922.279440	27.904896
266.733770	10948.583918	27.909914
267.440187	10965.642472	27.914932
267.779522	10995.214818	27.919949
268.439327	10992.078658	27.924967
268.323679	11012.032445	27.929984
268.456381	11026.025107	27.935002
268.750907	11040.808801	27.940020
269.051336	11056.705580	27.945037
269.664788	11070.812518	27.950055
269.628361	11097.634556	27.955072
269.427963	11116.223724	27.960090
270.328537	11120.379628	27.965108
270.582863	11146.435079	27.970125
270.479736	11160.983739	27.975143
270.592262	11185.275824	27.980160
270.818407	11201.832676	27.985178
271.305876	11210.174427	27.990196
271.637383	11236.136883	27.995213
271.996212	11253.267460	28.000231
272.261667	11278.426251	28.005248
272.253693	11293.105825	28.010266
273.039722	11313.287336	28.015284
273.237813	11334.522684	28.020301
273.581485	11342.218605	28.025319
273.642197	11367.600518	28.030336
273.728792	11381.701968	28.035354
274.519972	11393.450783	28.040372
274.842477	11418.056707	28.045389
275.250849	11419.516075	28.050407
275.327171	11441.520211	28.055424
275.409292	11442.288243	28.060442
275.989823	11465.606665	28.065460
276.019347	11475.828624	28.070477
276.671152	11484.543564	28.075495
276.287297	11505.722613	28.080512
276.646993	11519.638734	28.085530
277.294183	11524.974404	28.090548
277.292075	11562.372925	28.095565
277.841341	11571.613866	28.100583
278.305464	11590.936629	28.105600
278.183759	11604.254917	28.110618
278.719893	11613.764365	28.115636
278.837711	11633.399779	28.120653
279.354318	11641.209041	28.125671
279.714517	11652.618103	28.130688
279.706052	11669.797313	28.135706
280.331497	11678.406417	28.140724
279.858570	11695.966664	28.145741
280.398296	11696.848059	28.150759
280.718036	11716.722765	28.155776
280.659925	11731.381094	28.160794
280.843448	11740.383269	28.165812
281.354936	11759.789791	28.170829
281.929874	11784.431703	28.175847
281.824644	11798.325746	28.180864
282.071999	11807.194479	28.185882
282.504531	11827.945713	28.190900
282.705940	11838.585404	28.195917
283.118215	11848.047732	28.200935
283.144944	11875.120612	28.205952
283.570790	11884.615383	28.210970
284.050037	11905.472443	28.215988
283.995994	11916.838376	28.221005
284.306887	11937.039437	28.226023
284.652370	11954.319519	28.231040
284.990343	11970.207831	28.236058
285.497036	11988.917331	28.241076
285.575112	12012.582876	28.246093
285.898202	12032.665426	28.251111
286.141553	12044.577887	28.256128
286.530520	12076.277676	28.261146
286.829064	12086.301057	28.266164
286.698541	12099.881225	28.271181
287.391993	12122.665030	28.276199
287.598863	12141.323480	28.281216
287.899303	12163.483752	28.286234
288.351312	12180.131863	28.291252
288.380309	12201.374274	28.296269
288.735938	12223.249718	28.301287
288.688999	12239.017632	28.306304
289.129488	12270.250698	28.311322
289.655591	12284.954652	28.316340
289.396734	12306.671905	28.321357
290.018471	12336.600226	28.326375
290.418772	12349.386751	28.331392
290.915157	12379.430453	28.336410
291.272748	12389.081799	28.341428
291.336256	12409.921651	28.346445
291.501022	12421.658293	28.351463
292.104201	12444.274693	28.356480
292.162531	12463.700337	28.361498
292.856103	12489.691546	28.366516
293.164779	12504.496301	28.371533
293.269733	12517.777819	28.376551
293.414130	12536.273717	28.381568
293.591245	12564.745873	28.386586
294.066414	12584.323289	28.391604
294.507232	12604.703814	28.396621
294.961937	12620.967415	28.401639
295.631386	12642.655954	28.406656
295.357332	12665.993066	28.411674
295.810315	12666.190757	28.416692
295.922604	12697.576675	28.421709
296.565131	12703.866933	28.426727
296.877149	12724.793703	28.431744
296.648382	12741.616535	28.436762
296.978509	12746.122593	28.441780
297.235811	12768.213611	28.446797
297.513447	12783.922024	28.451815
297.640101	12806.157640	28.456832
298.047325	12834.984582	28.461850
298.560380	12855.772658	28.466868
298.679552	12877.691276	28.471885
299.040455	12892.249776	28.476903
299.256155	12909.048065	28.481920
299.452100	12931.989426	28.486938
299.735226	12953.435022	28.491956
299.922959	12970.939289	28.496973
300.268735	12998.523833	28.501991
300.866138	13018.447155	28.507008
300.998890	13043.421050	28.512026
301.412816	13059.712328	28.517044
301.654938	13086.453718	28.522061
301.970859	13099.407667	28.527079
302.368276	13119.164071	28.532096
302.679256	13144.715358	28.537114
302.780148	13148.673221	28.542132
303.192227	13171.442038	28.547149
303.285681	13193.377945	28.552167
304.294043	13200.703128	28.557184
304.297286	13234.152132	28.562202
304.675131	13250.041402	28.567220
304.841831	13269.087599	28.572237
305.081693	13283.136965	28.577255
305.456810	13299.809984	28.582272
305.579313	13325.630721	28.587290
305.893141	13340.331371	28.592308
306.234276	13367.143511	28.597325
306.527497	13385.926205	28.602343
306.853457	13398.851940	28.607360
306.964003	13420.118688	28.612378
307.764276	13450.266939	28.617396
307.836949	13470.643295	28.622413
308.179106	13481.542866	28.627431
308.550015	13505.401658	28.632448
308.792164	13518.867737	28.637466
309.279988	13544.406139	28.642484
309.819882	13562.423257	28.647501
309.628179	13582.455820	28.652519
310.264562	13596.060011	28.657536
310.485685	13624.622870	28.662554
310.746134	13651.239226	28.667572
311.180249	13672.106028	28.672589
311.295935	13690.699395	28.677607
312.012114	13697.092902	28.682624
312.054904	13723.950282	28.687642
312.363550	13742.050003	28.692660
313.201188	13761.129138	28.697677
313.231667	13784.288206	28.702695
313.511906	13799.767072	28.707712
313.584200	13811.461710	28.712730
314.068113	13826.024326	28.717748
314.336905	13843.520841	28.722765
314.602904	13875.469857	28.727783
314.924950	13882.855369	28.732800
315.426043	13914.184000	28.737818
315.602646	13925.268873	28.742836
315.844535	13948.405789	28.747853
315.955456	13969.115279	28.752871
316.419086	13981.208616	28.757888
316.694731	14002.858561	28.762906
316.948339	14027.561793	28.767924
317.299294	14050.549992	28.772941
317.579285	14074.558627	28.777959
318.022703	14092.054874	28.782976
317.908756	14120.402981	28.787994
318.549134	14137.582989	28.793012
318.837631	14161.642355	28.798029
319.224448	14191.612974	28.803047
319.545618	14204.809645	28.808064
319.950493	14227.062611	28.813082
320.069940	14245.397515	28.818100
320.438832	14270.439795	28.823117
320.576772	14291.731512	28.828135
321.195919	14304.689817	28.833152
321.427124	14328.060718	28.838170
321.648101	14347.447497	28.843188
322.165883	14363.423440	28.848205
322.018628	14389.541097	28.853223
322.634446	14404.678150	28.858240
323.036070	14436.021093	28.863258
322.910921	14447.485662	28.868276
323.821305	14467.880635	28.873293
323.733062	14488.574889	28.878311
324.155482	14503.581709	28.883328
324.711090	14531.236556	28.888346
324.586598	14554.797468	28.893364
325.099233	14571.718537	28.898381
325.332431	14600.541153	28.903399
325.781621	14620.183633	28.908416
325.822631	14651.501567	28.913434
326.157576	14667.161330	28.918452
326.671939	14692.968223	28.923469
326.843627	14731.319261	28.928487
327.129695	14751.256833	28.933504
327.595765	14786.528443	28.938522
328.256287	14806.300082	28.943540
328.695888	14832.179460	28.948557
328.857588	14859.000104	28.953575
329.271607	14867.595475	28.958592
329.557970	14896.832208	28.963610
330.209533	14919.012186	28.968628
330.289800	14942.750962	28.973645
330.325792	14974.169636	28.978663
330.830956	14995.094142	28.983680
331.248994	15014.212674	28.988698
331.386285	15030.755029	28.993716
332.037591	15055.572088	28.998733
332.138117	15085.821842	29.003751
332.552968	15094.445565	29.008768
332.609401	15126.513664	29.013786
332.732469	15149.757054	29.018804
333.804692	15178.126587	29.023821
333.935006	15200.134733	29.028839
334.351017	15220.580951	29.033856
334.625184	15252.182970	29.038874
334.539167	15277.481763	29.043892
335.045107	15300.283720	29.048909
335.670730	15329.223920	29.053927
336.134865	15340.637284	29.058944
336.479658	15372.706996	29.063962
336.760195	15399.773646	29.068980
337.142295	15409.492082	29.073997
337.150117	15434.892220	29.079015
337.683875	15448.135092	29.084032
338.166358	15474.074584	29.089050
338.067495	15497.435581	29.094068
338.597580	15521.836811	29.099085
338.858526	15552.724439	29.104103
339.375632	15565.654928	29.109120
339.911027	15588.884282	29.114138
339.959445	15616.331737	29.119156
340.700899	15636.199741	29.124173
340.718212	15665.584824	29.129191
341.325892	15679.107242	29.134208
341.227719	15692.796937	29.139226
341.487450	15730.640808	29.144244
342.063483	15750.117063	29.149261
342.015594	15782.955548	29.154279
342.520912	15804.979669	29.159296
342.688961	15835.936793	29.164314
343.275287	15864.258689	29.169332
343.981361	15871.162271	29.174349
344.029506	15902.539722	29.179367
344.719887	15914.541794	29.184384
344.717388	15938.651926	29.189402
344.878172	15960.659197	29.194420
344.926261	15979.825899	29.199437
345.033946	16005.153643	29.204455
346.079221	16028.803617	29.209472
346.407849	16063.679865	29.214490
346.494485	16084.649811	29.219508
347.415101	16098.685070	29.224525
347.188104	16124.063660	29.229543
347.251169	16150.243868	29.234560
348.161223	16176.616518	29.239578
348.207066	16201.584383	29.244596
348.666652	16220.104779	29.249613
348.930481	16258.625388	29.254631
349.140360	16277.800335	29.259648
349.749898	16311.550888	29.264666
350.123830	16339.282985	29.269684
350.642749	16362.776240	29.274701
350.841704	16387.324982	29.279719
350.773390	16410.863481	29.284736
351.427100	16437.427145	29.289754
351.745165	16470.917319	29.294772
352.649664	16496.162798	29.299789
352.902705	16524.049197	29.304807
353.051183	16549.862817	29.309824
353.346244	16567.906429	29.314842
353.697648	16590.335379	29.319860
354.075443	16613.344789	29.324877
354.416814	16646.506749	29.329895
354.632600	16674.949688	29.334912
355.660599	16698.836778	29.339930
355.479005	16719.609175	29.344948
356.161737	16748.543996	29.349965
356.398413	16770.412105	29.354983
356.886731	16794.305112	29.360000
357.084676	16811.613173	29.365018
357.484155	16847.458226	29.370036
357.827680	16870.021268	29.375053
358.020858	16900.943125	29.380071
358.132762	16926.120255	29.385088
358.877158	16945.809658	29.390106
358.879666	16987.570384	29.395124
359.650771	17010.877803	29.400141
359.980539	17039.278858	29.405159
360.068698	17064.341904	29.410176
360.574675	17089.126186	29.415194
360.836592	17123.069917	29.420212
361.425298	17151.079941	29.425229
362.093056	17184.374965	29.430247
362.370732	17198.757181	29.435264
363.090343	17213.704681	29.440282
362.941635	17234.149130	29.445300
363.436513	17250.528912	29.450317
363.664009	17280.254088	29.455335
363.474506	17309.164006	29.460352
364.247624	17334.404141	29.465370
364.274509	17367.662156	29.470388
364.511809	17392.756185	29.475405
364.962794	17429.170915	29.480423
365.285007	17453.383990	29.485440
365.980653	17481.821406	29.490458
366.152922	17519.363842	29.495476
367.013521	17545.281842	29.500493
367.158262	17573.585174	29.505511
367.338441	17593.553166	29.510528
367.732025	17613.134332	29.515546
368.404078	17642.835448	29.520564
368.843032	17663.955586	29.525581
368.806601	17684.058848	29.530599
369.116179	17725.671295	29.535616
369.707640	17744.921932	29.540634
369.914514	17764.698122	29.545652
370.436524	17784.244048	29.550669
370.756033	17812.252452	29.555687
371.143900	17833.319781	29.560704
372.029540	17851.845584	29.565722
371.920304	17882.272311	29.570740
372.355487	17904.487397	29.575757
372.685713	17931.277250	29.580775
372.794327	17952.353114	29.585792
373.209294	17978.369193	29.590810
373.625758	18020.007250	29.595828
374.231144	18039.268536	29.600845
374.630543	18075.300694	29.605863
374.466309	18104.559349	29.610880
375.218645	18128.944990	29.615898
375.206710	18162.884146	29.620916
375.613633	18193.270154	29.625933
376.038007	18222.294450	29.630951
376.145239	18254.093777	29.635968
376.647826	18294.953699	29.640986
376.790621	18326.379969	29.646004
377.490622	18361.871148	29.651021
377.957911	18390.412550	29.656039
378.777566	18429.744778	29.661056
378.813278	18458.578426	29.666074
379.172170	18485.881502	29.671092
379.231397	18519.180602	29.676109
379.880551	18554.259693	29.681127
380.234754	18592.345114	29.686144
380.717219	18619.627958	29.691162
380.860731	18663.229775	29.696180
381.692433	18700.465523	29.701197
381.932767	18736.817083	29.706215
382.196217	18760.988186	29.711232
382.733537	18783.753497	29.716250
383.301372	18826.738476	29.721268
383.607582	18858.163925	29.726285
384.085422	18887.997151	29.731303
384.337932	18919.322825	29.736320
384.902811	18944.751219	29.741338
384.989870	18973.421183	29.746356
385.433841	19005.379037	29.751373
385.581253	19035.412250	29.756391
386.004876	19071.206075	29.761408
386.505629	19106.906809	29.766426
386.721315	19142.918076	29.771444
387.547980	19184.476961	29.776461
388.165507	19206.668335	29.781479
388.205198	19239.221677	29.786496
388.872604	19259.483087	29.791514
389.259058	19282.598812	29.796532
389.472787	19322.539492	29.801549
389.841845	19344.540422	29.806567
390.247296	19382.327503	29.811584
390.969964	19404.490704	29.816602
390.906699	19441.605059	29.821620
391.373029	19464.471335	29.826637
391.905121	19490.252826	29.831655
392.248679	19527.416706	29.836672
392.764590	19556.475470	29.841690
392.584405	19583.521139	29.846708
393.325491	19604.152300	29.851725
393.487670	19635.626694	29.856743
393.625945	19666.737765	29.861760
394.278621	19693.056138	29.866778
394.958597	19729.933036	29.871796
395.173965	19755.102041	29.876813
395.318501	19784.396085	29.881831
395.435228	19812.854467	29.886848
396.129011	19851.343761	29.891866
396.351237	19885.452609	29.896884
396.958935	19920.191430	29.901901
397.543070	19949.100844	29.906919
397.554666	19979.817240	29.911936
398.420541	20009.339147	29.916954
398.520542	20050.044532	29.921972
398.655946	20081.678700	29.926989
399.292097	20116.611870	29.932007
399.912386	20150.822500	29.937024
400.234231	20182.730287	29.942042
400.819263	20215.250450	29.947060
400.859798	20247.811914	29.952077
401.363739	20283.226107	29.957095
401.586147	20318.191908	29.962112
402.092042	20363.269071	29.967130
402.804218	20398.376288	29.972148
403.122356	20429.042772	29.977165
403.759122	20457.160766	29.982183
404.019323	20487.906317	29.987200
404.397141	20532.790708	29.992218
404.457642	20559.064971	29.997236
405.140215	20586.481876	30.002253
405.955257	20621.514200	30.007271
405.951513	20657.424708	30.012288
406.604895	20683.069712	30.017306
406.823183	20719.336193	30.022324
407.369447	20747.848050	30.027341
408.023716	20784.938064	30.032359
407.750221	20824.414266	30.037376
408.265814	20865.213663	30.042394
408.734837	20892.863494	30.047412
409.310907	20931.980190	30.052429
409.756191	20959.656134	30.057447
409.946816	20999.500559	30.062464
410.493944	21026.399794	30.067482
411.090650	21061.420292	30.072500
411.285497	21114.361878	30.077517
411.803666	21136.097668	30.082535
412.109255	21166.154235	30.087552
412.511847	21208.680733	30.092570
413.145576	21240.338668	30.097588
413.742754	21269.707019	30.102605
414.240142	21294.983019	30.107623
414.873076	21322.582779	30.112640
415.236639	21351.083322	30.117658
415.643776	21381.782536	30.122676
415.864288	21414.540360	30.127693
416.183210	21429.997874	30.132711
416.568973	21469.760660	30.137728
416.855006	21492.714722	30.142746
417.243156	21536.371799	30.147764
417.240265	21572.589996	30.152781
418.060116	21604.903696	30.157799
418.555310	21648.702599	30.162816
418.936502	21676.546424	30.167834
419.551578	21712.859746	30.172852
420.057624	21755.081952	30.177869
420.241749	21768.687321	30.182887
420.603805	21810.034742	30.187904
420.974106	21833.777893	30.192922
421.630509	21853.341026	30.197940
422.312378	21885.928806	30.202957
422.693260	21905.308964	30.207975
422.853856	21937.153728	30.212992
423.291730	21952.628301	30.218010
423.961900	21978.507441	30.223028
423.909475	22012.606126	30.228045
424.675228	22042.258551	30.233063
424.774766	22072.191574	30.238080
425.324685	22099.891490	30.243098
425.719193	22127.077909	30.248116
425.886667	22159.850683	30.253133
426.075056	22183.143508	30.258151
426.460294	22239.716852	30.263168
426.797370	22269.082682	30.268186
427.290488	22312.874187	30.273204
427.663583	22355.895684	30.278221
428.150865	22391.116805	30.283239
428.565630	22433.478801	30.288256
428.971091	22479.073355	30.293274
429.447709	22511.125496	30.298292
429.611008	22556.621573	30.303309
430.110641	22594.070710	30.308327
430.373048	22644.071405	30.313344
430.977431	22692.818829	30.318362
431.610157	22739.371461	30.323380
432.297295	22773.787645	30.328397
433.073535	22807.903744	30.333415
433.560680	22850.548097	30.338432
433.893088	22881.899449	30.343450
434.581400	22917.588259	30.348468
434.864147	22950.524821	30.353485
435.145434	22979.282980	30.358503
435.577952	23015.225627	30.363520
435.968480	23050.079369	30.368538
436.552444	23085.057282	30.373556
436.672282	23119.878696	30.378573
437.505186	23156.534363	30.383591
437.772400	23195.756288	30.388608
438.021163	23232.256484	30.393626
438.757423	23268.348089	30.398644
438.938722	23309.598192	30.403661
439.225468	23342.560081	30.408679
439.681080	23385.075378	30.413696
440.226499	23429.580175	30.418714
440.496669	23462.573423	30.423732
440.334857	23512.202179	30.428749
441.323184	23552.604972	30.433767
442.010453	23593.280029	30.438784
442.407026	23637.215499	30.443802
443.200763	23668.223876	30.448820
443.374516	23717.559580	30.453837
443.677444	23743.752923	30.458855
443.937854	23795.698542	30.463872
444.722330	23832.762648	30.468890
445.332060	23871.095238	30.473908
445.360429	23919.238175	30.478925
446.007673	23958.902014	30.483943
446.309997	24005.034964	30.488960
446.907312	24050.841674	30.493978
447.139462	24081.696155	30.498996
447.618350	24119.502168	30.504013
448.510123	24146.948576	30.509031
448.961885	24194.539667	30.514048
449.158505	24236.085943	30.519066
449.622338	24272.901286	30.524084
449.940609	24313.897752	30.529101
450.343506	24359.469374	30.534119
451.127344	24392.273754	30.539136
451.578328	24421.878343	30.544154
452.108810	24449.448107	30.549172
452.313368	24491.277550	30.554189
452.826777	24520.748974	30.559207
453.208238	24550.229668	30.564224
453.300896	24587.901928	30.569242
453.904238	24627.975148	30.574260
454.431557	24665.462103	30.579277
455.018119	24710.190520	30.584295
455.543780	24743.164460	30.589312
455.628482	24791.455074	30.594330
456.018049	24820.969587	30.599348
456.671539	24871.531861	30.604365
456.927960	24908.461746	30.609383
457.385129	24945.661284	30.614400
457.766339	24991.679750	30.619418
458.522184	25033.873479	30.624436
459.083370	25080.638315	30.629453
459.423085	25117.939670	30.634471
459.752707	25168.297774	30.639488
460.452999	25211.097266	30.644506
461.054894	25250.367871	30.649524
461.171481	25300.534517	30.654541
461.783910	25330.400990	30.659559
462.242441	25370.831098	30.664576
462.292410	25423.652330	30.669594
463.109556	25462.014089	30.674612
463.422092	25502.314110	30.679629
463.916422	25552.437905	30.684647
464.509201	25589.878197	30.689664
464.771090	25649.228987	30.694682
465.253863	25688.261659	30.699700
465.664457	25736.775414	30.704717
466.210844	25789.222274	30.709735
466.660244	25837.594258	30.714752
466.969419	25884.276811	30.719770
467.671308	25931.736697	30.724788
468.267122	25982.980494	30.729805
468.922760	26014.862908	30.734823
469.642754	26059.515979	30.739840
470.074966	26105.658311	30.744858
470.411373	26137.142711	30.749876
470.846342	26187.262404	30.754893
471.585565	26227.884650	30.759911
471.907222	26269.096558	30.764928
472.166347	26322.586195	30.769946
472.454716	26353.025384	30.774964
473.053448	26405.948074	30.779981
473.656648	26450.826520	30.784999
474.327678	26492.186181	30.790016
474.496801	26532.774155	30.795034
475.276153	26578.469161	30.800052
475.542103	26613.956408	30.805069
475.897190	26665.421867	30.810087
476.541564	26702.751944	30.815104
476.712649	26750.440715	30.820122
477.142642	26796.619958	30.825140
477.633719	26850.779439	30.830157
477.928959	26899.432263	30.835175
478.415000	26946.842335	30.840192
478.804900	26998.634242	30.845210
479.393838	27040.541906	30.850228
480.001289	27101.392506	30.855245
480.158337	27148.778709	30.860263
481.044144	27190.334778	30.865280
481.270293	27248.902035	30.870298
481.791140	27296.335693	30.875316
481.969333	27339.977644	30.880333
482.518502	27393.091363	30.885351
483.481878	27443.404854	30.890368
483.853057	27489.538893	30.895386
484.207734	27526.313008	30.900404
484.687886	27574.044380	30.905421
485.137817	27625.052197	30.910439
486.130938	27668.042767	30.915456
486.274281	27713.028972	30.920474
486.611480	27750.560405	30.925492
487.313763	27793.880174	30.930509
487.296377	27842.962775	30.935527
488.194852	27886.483754	30.940544
488.320020	27940.789206	30.945562
489.208976	27986.753710	30.950580
489.453502	28042.112311	30.955597
489.890966	28097.325593	30.960615
490.583109	28141.326163	30.965632
491.069882	28189.925669	30.970650
491.510114	28237.914691	30.975668
492.385055	28285.320848	30.980685
492.581610	28344.319420	30.985703
493.208788	28385.589905	30.990720
493.365978	28431.506318	30.995738
494.122135	28486.273755	31.000756
494.752375	28535.541375	31.005773
494.957988	28588.333868	31.010791
495.454370	28638.538811	31.015808
496.000333	28702.339129	31.020826
496.585078	28749.580045	31.025844
497.008252	28803.618034	31.030861
497.570110	28849.257211	31.035879
498.328866	28904.113865	31.040896
498.591833	28959.686852	31.045914
499.463517	29005.215228	31.050932
499.827672	29044.947066	31.055949
500.285346	29105.390933	31.060967
500.925344	29136.874704	31.065984
501.605852	29191.066911	31.071002
502.074679	29241.492678	31.076020
502.419194	29284.137113	31.081037
502.661433	29327.328599	31.086055
503.711673	29384.649829	31.091072
503.792910	29434.247448	31.096090
504.731766	29477.311413	31.101108
505.408843	29518.342855	31.106125
505.340448	29577.575569	31.111143
505.796192	29612.195151	31.116160
506.162372	29670.302514	31.121178
507.201053	29719.275575	31.126196
507.792805	29766.354020	31.131213
508.097028	29818.433499	31.136231
508.633470	29865.874723	31.141248
508.858431	29919.595595	31.146266
509.256006	29956.042765	31.151284
510.051721	30010.458225	31.156301
510.439764	30066.307441	31.161319
510.999337	30112.764290	31.166336
511.561832	30172.061830	31.171354
512.251893	30216.326686	31.176372
513.026061	30258.331329	31.181389
512.861522	30300.655464	31.186407
513.184484	30351.853157	31.191424
513.769080	30398.618974	31.196442
514.466043	30446.827134	31.201460
514.984966	30504.700590	31.206477
515.509054	30558.746221	31.211495
516.278537	30604.516526	31.216512
516.453267	30650.593603	31.221530
516.926579	30697.971795	31.226548
517.555892	30738.234674	31.231565
518.226497	30796.030352	31.236583
518.557424	30833.578900	31.241600
518.957864	30885.068219	31.246618
519.584522	30923.770149	31.251636
520.215530	30971.552089	31.256653
520.343295	31022.130903	31.261671
520.778022	31074.113623	31.266688
521.435661	31131.912548	31.271706
521.773717	31185.208387	31.276724
522.549275	31231.733418	31.281741
522.793295	31299.934749	31.286759
523.334271	31338.027025	31.291776
523.801611	31397.842967	31.296794
524.685355	31456.643626	31.301812
525.040400	31508.031838	31.306829
525.258544	31570.682030	31.311847
526.160319	31619.922846	31.316864
526.532044	31686.810859	31.321882
526.843994	31740.510262	31.326900
527.785933	31788.703643	31.331917
527.982457	31849.105485	31.336935
528.692531	31908.561143	31.341952
529.100326	31969.729899	31.346970
529.508506	32033.356845	31.351988
530.827114	32093.621184	31.357005
530.825825	32160.367604	31.362023
531.345317	32204.034593	31.367040
532.086887	32264.076295	31.372058
532.409515	32324.477821	31.377076
533.185867	32383.308796	31.382093
533.392123	32439.050443	31.387111
533.888029	32489.686127	31.392128
534.550511	32558.299532	31.397146
534.968722	32632.810207	31.402164
535.764003	32677.530837	31.407181
536.321477	32747.932583	31.412199
537.351554	32813.122375	31.417216
537.762243	32854.912499	31.422234
538.026977	32911.437988	31.427252
538.619204	32974.283676	31.432269
539.360472	33037.874883	31.437287
539.500002	33080.729651	31.442304
540.347277	33138.002006	31.447322
541.031987	33195.522335	31.452340
541.896943	33237.850378	31.457357
542.497758	33298.420606	31.462375
543.008999	33346.332903	31.467392
543.513182	33396.947712	31.472410
544.285385	33444.880207	31.477428
544.755959	33489.662920	31.482445
544.971135	33544.705998	31.487463
545.815447	33600.276279	31.492480
546.081148	33639.207960	31.497498
546.430063	33699.322633	31.502516
547.318287	33749.452037	31.507533
547.504110	33803.724471	31.512551
548.066863	33864.274515	31.517568
548.882716	33914.861313	31.522586
549.174797	33970.435760	31.527604
549.649202	34014.553297	31.532621
549.853641	34084.116192	31.537639
550.327690	34132.134580	31.542656
551.154861	34194.532289	31.547674
551.667561	34251.311319	31.552692
552.305836	34310.666964	31.557709
552.757764	34378.460680	31.562727
553.213505	34427.047777	31.567744
553.669477	34479.604982	31.572762
553.770040	34544.585671	31.577780
554.624016	34592.782275	31.582797
555.182624	34663.011500	31.587815
555.940829	34709.374937	31.592832
556.103148	34775.293000	31.597850
556.735494	34836.144090	31.602868
557.483169	34891.118977	31.607885
558.042755	34951.726871	31.612903
558.167033	35019.959087	31.617920
558.872796	35076.083914	31.622938
559.226448	35146.816019	31.627956
559.860735	35211.142740	31.632973
560.364087	35281.011122	31.637991
561.425438	35348.149060	31.643008
561.931488	35401.303466	31.648026
562.353555	35467.692356	31.653044
563.268637	35527.637422	31.658061
563.809068	35594.912968	31.663079
564.207164	35656.692433	31.668096
564.710865	35713.420765	31.673114
565.571901	35784.753127	31.678132
565.856084	35841.950563	31.683149
566.622480	35915.322131	31.688167
567.172192	35972.072069	31.693184
567.981669	36033.431277	31.698202
568.388327	36101.125356	31.703220
569.276924	36156.475305	31.708237
569.739087	36228.030065	31.713255
570.225836	36284.725125	31.718272
571.051379	36332.479772	31.723290
571.595217	36392.236648	31.728308
572.287020	36447.537990	31.733325
572.883435	36518.153244	31.738343
573.502668	36570.512793	31.743360
574.251308	36617.750680	31.748378
574.665536	36682.317899	31.753396
575.245804	36736.312975	31.758413
575.223545	36798.547794	31.763431
575.654552	36857.526350	31.768448
576.585024	36918.739140	31.773466
577.077117	36988.000521	31.778484
577.947930	37046.222016	31.783501
578.429224	37122.416853	31.788519
578.696199	37180.457778	31.793536
579.444423	37240.038445	31.798554
579.919117	37307.848871	31.803572
580.570633	37364.753616	31.808589
581.522676	37423.714088	31.813607
581.740242	37500.010957	31.818624
582.727281	37559.054456	31.823642
583.059835	37625.058899	31.828660
583.608400	37690.674328	31.833677
584.505330	37742.006525	31.838695
585.160407	37808.737899	31.843712
585.812867	37872.401923	31.848730
585.927436	37922.282713	31.853748
586.476716	37978.672861	31.858765
587.240675	38045.336584	31.863783
587.720805	38103.509321	31.868800
588.340522	38170.099517	31.873818
588.490633	38236.022725	31.878836
588.957988	38303.481393	31.883853
589.725196	38372.759343	31.888871
590.300365	38433.767722	31.893888
590.915920	38490.047478	31.898906
591.675879	38559.766093	31.903924
592.272879	38616.017742	31.908941
592.822106	38676.362039	31.913959
593.407247	38741.792118	31.918976
594.488827	38796.212259	31.923994
594.704198	38852.837122	31.929012
595.507061	38909.879482	31.934029
595.708330	38964.840347	31.939047
596.451881	39032.906269	31.944064
597.093758	39085.007312	31.949082
597.509451	39154.169612	31.954100
598.255764	39207.506906	31.959117
598.748481	39265.854875	31.964135
598.837201	39327.726411	31.969152
599.955240	39394.140762	31.974170
600.492085	39465.610658	31.979188
601.115294	39529.067483	31.984205
601.863624	39600.168305	31.989223
602.095448	39662.910640	31.994240
603.330958	39729.398316	31.999258
603.632977	39804.311335	32.004276
604.204545	39863.178489	32.009293
604.906158	39920.471191	32.014311
605.364870	39992.786293	32.019328
606.155174	40053.265703	32.024346
607.020464	40132.099135	32.029364
607.368732	40191.493588	32.034381
608.133931	40256.116392	32.039399
608.222718	40325.097267	32.044416
608.907789	40389.885324	32.049434
609.481615	40464.235179	32.054452
610.179194	40527.357989	32.059469
610.940309	40592.430923	32.064487
611.444185	40668.804104	32.069504
612.173809	40732.973561	32.074522
612.249613	40815.870874	32.079540
613.159463	40888.986161	32.084557
613.874793	40959.949319	32.089575
614.818931	41041.592741	32.094592
615.496782	41103.448535	32.099610
615.941320	41177.134432	32.104628
616.614060	41246.262063	32.109645
617.530427	41314.980277	32.114663
617.945660	41377.088797	32.119680
618.485828	41448.739468	32.124698
619.232489	41515.939565	32.129716
619.540015	41582.881069	32.134733
620.186919	41663.345165	32.139751
620.696076	41729.205695	32.144768
621.302658	41791.426013	32.149786
622.215956	41869.955842	32.154804
622.637098	41937.208164	32.159821
623.394060	42017.466161	32.164839
624.266725	42085.272585	32.169856
624.815178	42145.685202	32.174874
625.287211	42218.546675	32.179892
625.813181	42300.233256	32.184909
626.386500	42365.371908	32.189927
626.953212	42443.882574	32.194944
627.681108	42509.182430	32.199962
628.456290	42579.469402	32.204980
628.733439	42650.713586	32.209997
629.437643	42727.927184	32.215015
629.688396	42803.653283	32.220032
630.587377	42875.155375	32.225050
631.324854	42954.599749	32.230068
632.127931	43031.763518	32.235085
632.870939	43100.280224	32.240103
633.355583	43172.950747	32.245120
634.039766	43226.938230	32.250138
634.654386	43298.978376	32.255156
634.697455	43364.470303	32.260173
635.966085	43430.599557	32.265191
636.389175	43505.040202	32.270208
637.294208	43570.630207	32.275226
637.365916	43638.486389	32.280244
638.154558	43707.493483	32.285261
638.647034	43782.561547	32.290279
639.303548	43863.788177	32.295296
639.936569	43937.899013	32.300314
640.574758	44004.181960	32.305332
641.366545	44077.727159	32.310349
642.274323	44145.282667	32.315367
642.669426	44228.398091	32.320384
643.493270	44298.184595	32.325402
644.185000	44372.483201	32.330420
645.072750	44448.650503	32.335437
645.706670	44512.795150	32.340455
646.302244	44581.606903	32.345472
646.673219	44655.536581	32.350490
647.209612	44726.505798	32.355508
647.751051	44802.311869	32.360525
648.769190	44881.585366	32.365543
649.272014	44951.588444	32.370560
649.528836	45031.774769	32.375578
650.698966	45113.891224	32.380596
651.022834	45200.174048	32.385613
652.101419	45272.694446	32.390631
652.624754	45350.678192	32.395648
653.263897	45429.356740	32.400666
654.147310	45508.175194	32.405684
654.335048	45590.806755	32.410701
655.377075	45665.311444	32.415719
655.786373	45744.733504	32.420736
656.198461	45816.570503	32.425754
656.986541	45891.215985	32.430772
657.564305	45976.519334	32.435789
658.531948	46053.036733	32.440807
658.934842	46138.976040	32.445824
659.841622	46226.439709	32.450842
660.748779	46303.261805	32.455860
660.907349	46382.099606	32.460877
661.646148	46462.966988	32.465895
662.108769	46553.628773	32.470912
662.721664	46629.095613	32.475930
663.833797	46712.513872	32.480948
663.925974	46803.307606	32.485965
665.144177	46885.717492	32.490983
665.774284	46977.209390	32.496000
666.278511	47062.135040	32.501018
667.137551	47141.033795	32.506036
667.568952	47224.620603	32.511053
668.493494	47301.573339	32.516071
669.226713	47385.508832	32.521088
669.632263	47464.430262	32.526106
670.535957	47556.186010	32.531124
670.931799	47633.180179	32.536141
671.758702	47716.324747	32.541159
672.442355	47809.618199	32.546176
673.117892	47890.249464	32.551194
674.058361	47971.604662	32.556212
674.648107	48041.096302	32.561229
675.311185	48127.977403	32.566247
676.014422	48208.425414	32.571264
676.623056	48280.513958	32.576282
677.404660	48367.051247	32.581300
677.796606	48443.095551	32.586317
678.796653	48509.435462	32.591335
679.076843	48589.506594	32.596352
679.815195	48657.103064	32.601370
680.853239	48732.782659	32.606388
681.085099	48813.914415	32.611405
682.080944	48873.210222	32.616423
682.317876	48962.183733	32.621440
683.184745	49039.118265	32.626458
684.023039	49107.666227	32.631476
684.535337	49195.341417	32.636493
685.538543	49275.365283	32.641511
685.878896	49372.162552	32.646528
686.401837	49436.841193	32.651546
687.062225	49523.397430	32.656564
687.477926	49609.258631	32.661581
688.555084	49686.726318	32.666599
689.193189	49776.812149	32.671616
689.862767	49874.429198	32.676634
690.565019	49958.551634	32.681652
691.052844	50046.695878	32.686669
691.610785	50124.627073	32.691687
692.294533	50222.237220	32.696704
693.076777	50317.690103	32.701722
694.012973	50405.543874	32.706740
694.635883	50506.526177	32.711757
695.548261	50588.712003	32.716775
695.902836	50672.961392	32.721792
696.878021	50772.187502	32.726810
697.480447	50854.450999	32.731828
698.204525	50958.053180	32.736845
699.184575	51035.845569	32.741863
699.801957	51131.152851	32.746880
700.150707	51232.405391	32.751898
701.119035	51309.253221	32.756916
701.598367	51405.677583	32.761933
702.523103	51504.252460	32.766951
702.920692	51595.378366	32.771968
703.958210	51693.057423	32.776986
704.428572	51779.560419	32.782004
705.090103	51889.634369	32.787021
705.819173	51972.285966	32.792039
706.949083	52067.652037	32.797056
707.433207	52160.686810	32.802074
708.364548	52253.471153	32.807092
709.058441	52345.429698	32.812109
709.968910	52433.360073	32.817127
710.420833	52538.866767	32.822144
711.156019	52635.179070	32.827162
711.987009	52715.504659	32.832180
712.489739	52813.347287	32.837197
712.985705	52905.593919	32.842215
713.699437	52999.378111	32.847232
714.692295	53092.168894	32.852250
715.759482	53186.792655	32.857268
716.129914	53284.868013	32.862285
716.793194	53376.046718	32.867303
717.741408	53455.837876	32.872320
718.735009	53545.301088	32.877338
719.224980	53641.861078	32.882356
719.678106	53733.745922	32.887373
720.614184	53825.229081	32.892391
721.341542	53913.790293	32.897408
721.923622	54016.307545	32.902426
722.701458	54093.223106	32.907444
723.527805	54189.963915	32.912461
724.415577	54294.807710	32.917479
725.172481	54369.042541	32.922496
725.256710	54456.600556	32.927514
726.122202	54533.749751	32.932532
726.645943	54634.567591	32.937549
727.208527	54717.675308	32.942567
727.892970	54801.034909	32.947584
728.481770	54899.012673	32.952602
729.571948	54988.561240	32.957620
730.109253	55087.256126	32.962637
730.660860	55184.293673	32.967655
731.433699	55281.175047	32.972672
732.142571	55383.577319	32.977690
732.889148	55479.920605	32.982708
733.340374	55580.673113	32.987725
734.445089	55689.551332	32.992743
735.268783	55772.481268	32.997760
735.830797	55888.356746	33.002778
736.667473	55984.605433	33.007796
737.333785	56087.978837	33.012813
737.917171	56185.894340	33.017831
738.816953	56286.917446	33.022848
739.339138	56397.368207	33.027866
740.366086	56498.952696	33.032884
740.891638	56612.955363	33.037901
741.549641	56715.019036	33.042919
742.687265	56817.989672	33.047936
743.429239	56924.110015	33.052954
744.133832	57019.955848	33.057972
744.967060	57129.183844	33.062989
745.766237	57233.179438	33.068007
746.816937	57340.306230	33.073024
747.032768	57435.015284	33.078042
748.230780	57542.447392	33.083060
748.867723	57651.976118	33.088077
749.756406	57744.300368	33.093095
750.903661	57841.416618	33.098112
751.460845	57943.092466	33.103130
752.283426	58039.056365	33.108148
753.101343	58139.691603	33.113165
753.745743	58248.040598	33.118183
754.950488	58330.621102	33.123200
755.598584	58435.463139	33.128218
756.488540	58523.196415	33.133236
756.949364	58620.088711	33.138253
758.027808	58722.920927	33.143271
758.865052	58817.856005	33.148288
759.160368	58906.479273	33.153306
760.170878	59004.034538	33.158324
760.816564	59107.439558	33.163341
761.667211	59195.220178	33.168359
762.419502	59295.619248	33.173376
762.959500	59395.542020	33.178394
763.678194	59490.657866	33.183412
763.817470	59594.610494	33.188429
764.655520	59702.303263	33.193447
765.717173	59810.806501	33.198464
766.412712	59919.250798	33.203482
767.031358	60018.676987	33.208500
767.843037	60126.003482	33.213517
768.621447	60240.035411	33.218535
769.415063	60339.358385	33.223552
770.300717	60448.304954	33.228570
771.115228	60549.287715	33.233588
772.074613	60655.094671	33.238605
772.954196	60762.855714	33.243623
773.629480	60858.168431	33.248640
774.612715	60963.890881	33.253658
774.996564	61069.099942	33.258676
775.398397	61164.674214	33.263693
776.564076	61265.709885	33.268711
777.545351	61355.216360	33.273728
777.909723	61449.116905	33.278746
778.871663	61548.556978	33.283764
779.989926	61645.095809	33.288781
780.182978	61743.020652	33.293799
781.418449	61828.037435	33.298816
781.847082	61940.518631	33.303834
782.486008	62040.861494	33.308852
783.542137	62144.953569	33.313869
784.221038	62229.255020	33.318887
785.189003	62337.882007	33.323904
785.960238	62446.428333	33.328922
786.517264	62544.865670	33.333940
787.332360	62649.259324	33.338957
787.894531	62756.242676	33.343975
788.891661	62852.902040	33.348992
789.553613	62967.404571	33.354010
790.517714	63068.166414	33.359028
791.185730	63188.705752	33.364045
791.603663	63295.507163	33.369063
792.962824	63396.148373	33.374080
793.441513	63512.270840	33.379098
794.114959	63620.599317	33.384116
795.083702	63735.030073	33.389133
795.541310	63857.643548	33.394151
796.549080	63969.325714	33.399168
797.147772	64084.925838	33.404186
798.125937	64203.687740	33.409204
798.940394	64313.949821	33.414221
799.332655	64440.787605	33.419239
800.363776	64556.205041	33.424256
801.518276	64674.788756	33.429274
802.338712	64798.441393	33.434292
803.165239	64914.634280	33.439309
803.567283	65034.033551	33.444327
804.384245	65141.347402	33.449344
805.313056	65275.384072	33.454362
806.090944	65395.311162	33.459380
807.233123	65521.260232	33.464397
807.590476	65629.436510	33.469415
809.070819	65753.282782	33.474432
809.974556	65873.786055	33.479450
810.578800	65982.821031	33.484468
811.551764	66099.185943	33.489485
812.159916	66223.451098	33.494503
813.290137	66332.672743	33.499520
813.891462	66452.236802	33.504538
814.912950	66568.627903	33.509556
815.735547	66683.674321	33.514573
816.357749	66807.340004	33.519591
817.049991	66917.781442	33.524608
817.883843	67034.692964	33.529626
818.546295	67147.517691	33.534644
819.575527	67264.556230	33.539661
820.279134	67383.748289	33.544679
821.440939	67506.070679	33.549696
822.223606	67623.050829	33.554714
822.943979	67739.763742	33.559732
823.994381	67851.680859	33.564749
824.591033	67973.429244	33.569767
825.507178	68085.685930	33.574784
826.335213	68208.921132	33.579802
827.401566	68333.224091	33.584820
828.288013	68447.257936	33.589837
828.921860	68560.088603	33.594855
829.765309	68665.443366	33.599872
830.375921	68779.853399	33.604890
831.136104	68880.676945	33.609908
832.123767	68992.913954	33.614925
832.905666	69102.656449	33.619943
833.652525	69210.552702	33.624960
834.194807	69321.998873	33.629978
834.792982	69434.776846	33.634996
835.645324	69547.532346	33.640013
836.271629	69676.645518	33.645031
837.110226	69793.900254	33.650048
838.134849	69920.198492	33.655066
839.112095	70034.832830	33.660084
839.727913	70152.467826	33.665101
840.716103	70272.963193	33.670119
841.478426	70401.381657	33.675136
842.015380	70527.353120	33.680154
842.719003	70659.020345	33.685172
843.796515	70781.331228	33.690189
844.814112	70912.897493	33.695207
845.747938	71036.839732	33.700224
846.616966	71173.908241	33.705242
847.304889	71309.053616	33.710260
848.323772	71433.262301	33.715277
848.904111	71560.819840	33.720295
849.779453	71688.190222	33.725312
850.759334	71811.123840	33.730330
851.640436	71952.691406	33.735348
852.702188	72086.964064	33.740365
853.180231	72221.839994	33.745383
854.253507	72343.635561	33.750400
854.926983	72488.870828	33.755418
855.650047	72625.302348	33.760436
856.657876	72752.568542	33.765453
857.302130	72893.397253	33.770471
858.436672	73038.237415	33.775488
859.334396	73176.319365	33.780506
859.980920	73317.732255	33.785524
861.195760	73445.714507	33.790541
861.832023	73582.982194	33.795559
862.808925	73723.046619	33.800576
863.859226	73863.896657	33.805594
864.754870	74014.632731	33.810612
865.963225	74134.556636	33.815629
866.249824	74277.919909	33.820647
867.198393	74417.860655	33.825664
868.341330	74561.311833	33.830682
869.224773	74692.284400	33.835700
870.384886	74819.107383	33.840717
870.974224	74961.526968	33.845735
871.824829	75091.811646	33.850752
872.820118	75228.151133	33.855770
873.740365	75366.047095	33.860788
874.462832	75501.604862	33.865805
875.220438	75634.077499	33.870823
876.191337	75776.964200	33.875840
876.910034	75907.838417	33.880858
877.638734	76049.679065	33.885876
878.909953	76179.457859	33.890893
879.554324	76323.629122	33.895911
880.663918	76458.300160	33.900928
881.532898	76593.675935	33.905946
882.292992	76737.495522	33.910964
883.506838	76866.136662	33.915981
884.053597	77001.372132	33.920999
885.157746	77146.427791	33.926016
886.104714	77276.323547	33.931034
886.679686	77420.582976	33.936052
887.918541	77550.963382	33.941069
888.757970	77683.909112	33.946087
889.503486	77805.169239	33.951104
890.270838	77930.044541	33.956122
891.303037	78061.765137	33.961140
892.217718	78180.551380	33.966157
892.879986	78314.042515	33.971175
893.517164	78437.803585	33.976192
894.555243	78574.909261	33.981210
895.196926	78713.327476	33.986228
896.316487	78844.291798	33.991245
897.069311	78987.709568	33.996263
897.774259	79123.709755	34.001280
898.781942	79257.402398	34.006298
899.361062	79408.916935	34.011316
900.466243	79541.526076	34.016333
901.427807	79695.927138	34.021351
902.011036	79842.996803	34.026368
903.158288	79981.117783	34.031386
903.851963	80132.643528	34.036404
904.754966	80286.387745	34.041421
905.642724	80435.517472	34.046439
906.704934	80590.837928	34.051456
907.820720	80742.076521	34.056474
908.122302	80889.009758	34.061492
909.516100	81047.555483	34.066509
910.156804	81193.650145	34.071527
911.109412	81352.264626	34.076544
911.949516	81511.797163	34.081562
912.499047	81666.241795	34.086580
913.635018	81829.593079	34.091597
914.585357	82002.738068	34.096615
915.535960	82162.351767	34.101632
916.999217	82316.567436	34.106650
917.301254	82476.467720	34.111668
918.882942	82629.963651	34.116685
919.366423	82799.908299	34.121703
920.145423	82962.187864	34.126720
921.722755	83118.161553	34.131738
922.264141	83284.367362	34.136756
923.318394	83432.856400	34.141773
924.196447	83594.940556	34.146791
925.410958	83760.114735	34.151808
926.274988	83911.251362	34.156826
927.087217	84076.291857	34.161844
928.166862	84230.115562	34.166861
928.996716	84397.477490	34.171879
929.904659	84553.274179	34.176896
931.236260	84716.132694	34.181914
931.847509	84874.473546	34.186932
932.723142	85032.771753	34.191949
933.827564	85197.202422	34.196967
934.560621	85347.471554	34.201984
935.975484	85514.067727	34.207002
936.689687	85670.960615	34.212020
937.976603	85827.165056	34.217037
938.608442	85981.283183	34.222055
939.761016	86148.718201	34.227072
940.937277	86290.295488	34.232090
941.361044	86450.019479	34.237108
942.312847	86617.060751	34.242125
943.377630	86767.125931	34.247143
944.601078	86929.739314	34.252160
945.324352	87080.008502	34.257178
946.457836	87238.380205	34.262196
947.611130	87391.915102	34.267213
948.576311	87541.552393	34.272231
949.433819	87691.322340	34.277248
950.636265	87831.411129	34.282266
951.602809	87981.259801	34.287284
952.273855	88128.563725	34.292301
953.197807	88264.815615	34.297319
954.115496	88399.664447	34.302336
955.058305	88546.717190	34.307354
955.728451	88694.689242	34.312372
956.563032	88825.478776	34.317389
957.632085	88977.968370	34.322407
958.509477	89123.820435	34.327424
959.269765	89276.147825	34.332442
960.529887	89433.329793	34.337460
961.465389	89582.377289	34.342477
962.335273	89733.069348	34.347495
963.040978	89896.389868	34.352512
964.403489	90043.565953	34.357530
964.839128	90204.015692	34.362548
965.833991	90361.918458	34.367565
966.833024	90521.448080	34.372583
967.524833	90692.953154	34.377600
968.990024	90854.388834	34.382618
970.053380	91018.853995	34.387636
970.832593	91176.747126	34.392653
971.848564	91344.171650	34.397671
972.567602	91511.171750	34.402688
973.861953	91671.894309	34.407706
974.899777	91833.976820	34.412724
975.712751	91992.540576	34.417741
976.942759	92163.258199	34.422759
977.482665	92330.122661	34.427776
979.067948	92500.695294	34.432794
979.804563	92669.016945	34.437812
980.577772	92842.903607	34.442829
981.619155	93004.316070	34.447847
982.687790	93182.808462	34.452864
983.889942	93339.303833	34.457882
984.746034	93511.820687	34.462900
985.674728	93679.357973	34.467917
986.907288	93849.302078	34.472935
987.533776	94023.170736	34.477952
988.902912	94191.271656	34.482970
989.832198	94364.687551	34.487988
990.676280	94532.206656	34.493005
991.981643	94707.670621	34.498023
992.544200	94884.562630	34.503040
993.895175	95050.988642	34.508058
994.885773	95215.335808	34.513076
995.921335	95390.532726	34.518093
997.112412	95566.458452	34.523111
997.512339	95739.977842	34.528128
998.744916	95902.991862	34.533146
999.681021	96083.090705	34.538164
1000.820577	96255.427902	34.543181
1001.992203	96429.457521	34.548199
1002.716636	96615.298851	34.553216
1003.844022	96779.735013	34.558234
1004.813051	96961.392032	34.563252
1005.824821	97134.022295	34.568269
1007.073864	97306.829752	34.573287
1007.549788	97480.304336	34.578304
1008.680397	97655.868603	34.583322
1009.723449	97829.891218	34.588340
1010.860929	98010.306140	34.593357
1012.188194	98178.675127	34.598375
1013.183155	98354.963079	34.603392
1014.209692	98526.555858	34.608410
1015.030742	98698.082482	34.613428
1016.291705	98871.791353	34.618445
1017.558974	99037.004159	34.623463
1018.292990	99201.875702	34.628480
1019.641964	99357.017051	34.633498
1020.444973	99518.561750	34.638516
1021.468638	99673.176352	34.643533
1022.302873	99830.001146	34.648551
1023.245628	99987.188835	34.653568
1024.266964	100142.395470	34.658586
1025.683686	100310.035697	34.663604
1026.078224	100475.421125	34.668621
1027.479831	100631.751816	34.673639
1028.315557	100794.470479	34.678656
1029.340170	100957.032311	34.683674
1029.930667	101129.759396	34.688692
1030.675890	101306.697874	34.693709
1032.192685	101490.322805	34.698727
1032.881573	101665.709153	34.703744
1034.058495	101839.483728	34.708762
1035.038222	102020.719207	34.713780
1036.295592	102197.807052	34.718797
1037.591656	102368.488234	34.723815
1038.624474	102556.329109	34.728832
1039.363196	102727.630349	34.733850
1040.495793	102899.836383	34.738868
1041.147204	103091.252088	34.743885
1042.570933	103270.415631	34.748903
1043.440464	103469.060901	34.753920
1044.462880	103642.733775	34.758938
1045.703744	103832.442756	34.763956
1046.487711	104018.492641	34.768973
1047.433288	104201.477635	34.773991
1048.530933	104392.493466	34.779008
1049.167848	104584.600040	34.784026
1050.736072	104773.995740	34.789044
1051.609656	104973.715571	34.794061
1052.845766	105165.828630	34.799079
1053.966713	105358.012787	34.804096
1055.101771	105549.841382	34.809114
1056.431681	105747.287865	34.814132
1057.172833	105935.182147	34.819149
1058.574322	106120.929440	34.824167
1059.271944	106320.257888	34.829184
1060.636309	106508.065842	34.834202
1061.681876	106696.333133	34.839220
1062.639125	106884.806341	34.844237
1064.021760	107086.205775	34.849255
1064.805623	107274.976383	34.854272
1065.863558	107463.880332	34.859290
1067.263779	107655.604243	34.864308
1068.235359	107846.805078	34.869325
1069.571071	108037.085755	34.874343
1069.929221	108229.822030	34.879360
1071.278441	108431.021743	34.884378
1072.905737	108616.052345	34.889396
1073.730543	108814.010288	34.894413
1075.132753	109002.513434	34.899431
1075.836361	109195.148802	34.904448
1077.050202	109374.552838	34.909466
1078.104897	109562.407976	34.914484
1079.167728	109764.817645	34.919501
1080.524491	109942.124377	34.924519
1081.247161	110145.948510	34.929536
1082.318720	110327.548462	34.934554
1083.733889	110510.980271	34.939572
1084.734261	110700.359656	34.944589
1086.058243	110882.732283	34.949607
1086.804363	111082.835208	34.954624
1088.049828	111262.031053	34.959642
1089.416280	111452.938585	34.964660
1090.079810	111639.428495	34.969677
1090.989504	111810.322514	34.974695
1092.214897	111989.982461	34.979712
1093.182379	112169.521527	34.984730
1094.708886	112345.016805	34.989748
1095.392537	112516.142579	34.994765
1096.424364	112690.556331	34.999783
1097.161579	112880.652939	35.004800
1098.501783	113072.792162	35.009818
1099.531063	113253.265496	35.014836
1100.702920	113444.915696	35.019853
1101.996683	113627.564773	35.024871
1102.695337	113820.055913	35.029888
1103.604637	114017.821910	35.034906
1105.140657	114206.262504	35.039924
1106.055412	114397.150893	35.044941
1107.008062	114596.497456	35.049959
1107.842594	114789.656918	35.054976
1108.980155	114987.886103	35.059994
1110.225548	115188.658119	35.065012
1111.147148	115410.542199	35.070029
1112.383202	115611.774871	35.075047
1113.272978	115818.919723	35.080064
1114.436132	116026.172928	35.085082
1115.634669	116232.623576	35.090100
1116.776514	116449.728064	35.095117
1117.953210	116650.787842	35.100135
1119.307164	116860.334229	35.105152
1120.614356	117076.883987	35.110170
1121.677105	117279.500147	35.115188
1122.474759	117491.601207	35.120205
1123.569017	117697.686868	35.125223
1124.958855	117918.093883	35.130240
1125.957369	118135.602273	35.135258
1127.177291	118344.940888	35.140276
1128.146934	118567.462360	35.145293
1129.421366	118776.643030	35.150311
1130.439566	118989.326838	35.155328
1131.397351	119212.197337	35.160346
1132.832250	119426.069919	35.165364
1133.554868	119656.877047	35.170381
1135.065463	119881.105830	35.175399
1136.039417	120097.581201	35.180416
1137.105716	120311.204400	35.185434
1138.458421	120527.569641	35.190452
1139.695120	120763.166535	35.195469
1140.763818	120973.676816	35.200487
1141.639505	121201.644882	35.205504
1142.687109	121424.720095	35.210522
1144.113924	121646.276964	35.215540
1145.375153	121871.423854	35.220557
1146.105152	122096.609581	35.225575
1147.734711	122324.715108	35.230592
1148.645964	122553.992975	35.235610
1149.927575	122785.074301	35.240628
1151.025953	123010.117314	35.245645
1152.304777	123252.354993	35.250663
1153.452773	123474.554505	35.255680
1154.757078	123696.995959	35.260698
1155.767245	123916.674181	35.265716
1157.059489	124138.563259	35.270733
1158.421925	124367.514241	35.275751
1159.659242	124580.772240	35.280768
1160.324352	124819.005004	35.285786
1161.680286	125027.037597	35.290804
1162.769067	125259.056935	35.295821
1164.228530	125478.798945	35.300839
1165.331240	125702.023541	35.305856
1166.603643	125923.688129	35.310874
1167.913743	126128.782709	35.315892
1168.872392	126338.461535	35.320909
1169.924197	126550.585249	35.325927
1171.119770	126770.418174	35.330944
1172.090330	126979.820560	35.335962
1173.317984	127185.024536	35.340980
1174.471260	127398.037216	35.345997
1175.575408	127614.709871	35.351015
1176.692370	127839.430578	35.356032
1177.861554	128046.601884	35.361050
1178.829577	128267.142158	35.366068
1179.733012	128492.447912	35.371085
1180.806621	128723.912761	35.376103
1182.174635	128942.908662	35.381120
1182.905008	129185.093756	35.386138
1184.249012	129415.378209	35.391156
1185.078811	129663.051798	35.396173
1186.186027	129895.673225	35.401191
1187.648011	130144.703818	35.406208
1188.336272	130402.420629	35.411226
1190.107404	130651.847771	35.416244
1191.242987	130886.259127	35.421261
1192.075249	131137.493195	35.426279
1193.439858	131382.924152	35.431296
1194.489538	131639.970090	35.436314
1195.681671	131891.581602	35.441332
1196.795168	132148.126677	35.446349
1198.623131	132405.924798	35.451367
1199.918735	132657.106862	35.456384
1200.660062	132908.534630	35.461402
1202.191334	133161.101490	35.466420
1203.715890	133424.751369	35.471437
1204.949097	133675.660074	35.476455
1206.067390	133925.372672	35.481472
1207.379786	134180.278257	35.486490
1208.457683	134420.100134	35.491508
1209.895638	134671.527790	35.496525
1211.063520	134925.803825	35.501543
1212.140720	135188.882643	35.506560
1213.657302	135444.144636	35.511578
1214.913223	135688.307591	35.516596
1216.043400	135945.184063	35.521613
1217.204843	136206.887808	35.526631
1218.775934	136450.370363	35.531648
1219.721580	136714.243751	35.536666
1221.369858	136957.793328	35.541684
1222.049957	137219.001369	35.546701
1223.230668	137472.141032	35.551719
1224.761688	137714.536363	35.556736
1225.857185	137975.187145	35.561754
1227.157373	138227.995771	35.566772
1228.443937	138491.509797	35.571789
1229.485953	138751.985224	35.576807
1230.719001	139011.429400	35.581824
1232.095195	139279.055535	35.586842
1232.923760	139525.282363	35.591860
1234.072927	139796.969520	35.596877
1235.471100	140063.380916	35.601895
1237.182881	140316.973890	35.606912
1238.292931	140574.675074	35.611930
1239.039383	140840.591578	35.616948
1240.537601	141102.353570	35.621965
1241.763070	141361.867494	35.626983
1243.194508	141622.959723	35.632000
1244.276236	141889.120501	35.637018
1245.531415	142155.140516	35.642036
1246.950161	142408.860643	35.647053
1248.313680	142670.720099	35.652071
1249.527981	142915.702611	35.657088
1250.659396	143165.354430	35.662106
1251.697335	143408.898537	35.667124
1253.418740	143648.603110	35.672141
1254.078838	143904.323538	35.677159
1255.290254	144150.862201	35.682176
1256.511078	144397.857549	35.687194
1257.956203	144663.814364	35.692212
1258.847543	144920.049170	35.697229
1260.090271	145184.496164	35.702247
1261.431715	145438.960942	35.707264
1262.423168	145710.339525	35.712282
1263.439841	145977.809948	35.717300
1265.163369	146252.977644	35.722317
1266.081776	146522.484778	35.727335
1267.354369	146781.612050	35.732352
1268.175350	147072.191835	35.737370
1269.495405	147351.873348	35.742388
1271.029630	147636.264858	35.747405
1271.933838	147912.810714	35.752423
1273.651743	148196.415247	35.757440
1274.431782	148482.269640	35.762458
1275.700946	148767.030766	35.767476
1276.942610	149067.373343	35.772493
1277.926158	149358.375518	35.777511
1279.475253	149654.993927	35.782528
1280.611731	149966.902851	35.787546
1282.219061	150270.023047	35.792564
1283.524616	150559.028092	35.797581
1284.757391	150868.049426	35.802599
1286.221361	151166.456862	35.807616
1287.395620	151472.613604	35.812634
1288.511782	151772.757557	35.817652
1290.233490	152074.681023	35.822669
1291.518132	152389.464696	35.827687
1292.784041	152681.485890	35.832704
1294.177312	152987.301462	35.837722
1295.492336	153301.009413	35.842740
1297.051662	153602.984411	35.847757
1297.935142	153907.838708	35.852775
1299.537210	154203.570485	35.857792
1300.737140	154512.055774	35.862810
1302.147552	154816.119731	35.867828
1303.786759	155115.657739	35.872845
1304.996243	155424.021771	35.877863
1306.126706	155729.953029	35.882880
1307.391780	156033.086323	35.887898
1308.870909	156340.778667	35.892916
1310.137136	156637.624424	35.897933
1311.070802	156960.241038	35.902951
1312.802038	157255.137057	35.907968
1314.193945	157573.369732	35.912986
1315.646499	157867.453666	35.918004
1317.080250	158178.402503	35.923021
1318.298650	158483.401492	35.928039
1319.859367	158785.022416	35.933056
1320.915461	159094.328041	35.938074
1322.372032	159409.265988	35.943092
1324.158529	159708.369878	35.948109
1325.222136	160013.012569	35.953127
1326.411879	160304.341066	35.958144
1327.572280	160614.275199	35.963162
1328.525860	160916.633731	35.968180
1330.166892	161222.712286	35.973197
1331.159414	161531.133175	35.978215
1333.102536	161836.772995	35.983232
1333.888565	162147.008723	35.988250
1335.398198	162448.766220	35.993268
1336.815345	162745.174395	35.998285
1338.129615	163040.206020	36.003303
1339.340593	163323.596906	36.008320
1340.677890	163632.344052	36.013338
1341.920683	163918.423395	36.018356
1343.597878	164207.109973	36.023373
1344.700904	164510.636702	36.028391
1345.965135	164806.031299	36.033408
1347.084579	165096.604993	36.038426
1348.547046	165408.896799	36.043444
1350.124313	165710.462988	36.048461
1351.092717	166023.234163	36.053479
1352.471533	166326.499549	36.058496
1353.844857	166636.860801	36.063514
1355.245020	166957.040766	36.068532
1356.413010	167262.605973	36.073549
1357.582563	167581.166318	36.078567
1359.026946	167902.627328	36.083584
1360.508089	168216.103210	36.088602
1361.675427	168526.181713	36.093620
1362.961442	168860.047539	36.098637
1364.526025	169186.586167	36.103655
1365.941369	169509.243489	36.108672
1367.415372	169840.039992	36.113690
1368.953020	170160.816348	36.118708
1370.497384	170472.888775	36.123725
1371.717320	170811.411437	36.128743
1373.275713	171125.097527	36.133760
1374.765433	171450.040283	36.138778
1375.655829	171783.040931	36.143796
1377.562070	172106.104743	36.148813
1378.604998	172430.798183	36.153831
1379.704464	172767.806694	36.158848
1381.359355	173092.175110	36.163866
1382.423396	173423.864201	36.168884
1384.146981	173763.708088	36.173901
1385.635329	174094.405294	36.178919
1387.228312	174437.092822	36.183936
1388.792140	174776.805272	36.188954
1389.877058	175098.895547	36.193972
1391.746587	175434.995949	36.198989
1392.718758	175771.868809	36.204007
1394.076089	176109.809830	36.209024
1395.754882	176442.750486	36.214042
1397.188135	176796.192247	36.219060
1398.765694	177117.160917	36.224077
1400.033387	177455.455872	36.229095
1401.053495	177790.202324	36.234112
1402.747522	178119.077648	36.239130
1404.092205	178460.983725	36.244148
1405.942129	178796.653106	36.249165
1407.099822	179136.817771	36.254183
1408.667099	179468.032661	36.259200
1409.926045	179803.565145	36.264218
1411.084744	180132.211877	36.269236
1412.612479	180467.260015	36.274253
1414.133640	180815.308255	36.279271
1415.209979	181150.714594	36.284288
1416.798179	181491.927765	36.289306
1418.105504	181838.761558	36.294324
1419.831908	182175.970852	36.299341
1421.167199	182522.398315	36.304359
1422.574718	182873.842407	36.309376
1423.954763	183209.858860	36.314394
1424.947587	183555.283363	36.319412
1426.741830	183894.142287	36.324429
1428.063572	184242.271171	36.329447
1429.521832	184582.865366	36.334464
1430.768198	184912.275878	36.339482
1431.794764	185250.952694	36.344500
1433.407465	185582.908778	36.349517
1434.927334	185922.536323	36.354535
1436.014424	186271.300613	36.359552
1437.608875	186611.085007	36.364570
1439.101165	186950.964483	36.369588
1440.686069	187290.716441	36.374605
1441.986533	187631.418681	36.379623
1442.963228	187975.083345	36.384640
1444.660049	188326.069729	36.389658
1445.647096	188672.694519	36.394676
1447.056181	189021.714291	36.399693
1448.654934	189386.813750	36.404711
1449.981548	189750.284793	36.409728
1451.260996	190103.470731	36.414746
1452.250069	190477.576404	36.419764
1454.040364	190849.647841	36.424781
1455.591196	191229.428685	36.429799
1456.982469	191598.600136	36.434816
1458.593733	191974.351442	36.439834
1459.942301	192356.191202	36.444852
1461.657243	192730.939810	36.449869
1462.855622	193105.331716	36.454887
1464.126057	193479.802832	36.459904
1465.958193	193865.304315	36.464922
1466.972907	194263.740007	36.469940
1469.037795	194645.069144	36.474957
1470.373656	195024.794453	36.479975
1471.768137	195420.381635	36.484992
1473.553343	195805.737561	36.490010
1474.785593	196207.221687	36.495028
1476.433000	196585.990585	36.500045
1477.935751	196976.249831	36.505063
1479.191683	197367.288517	36.510080
1481.170452	197752.357251	36.515098
1482.204613	198155.853785	36.520116
1483.865497	198551.898161	36.525133
1485.616476	198941.302582	36.530151
1487.428686	199338.532656	36.535168
1489.115695	199720.220085	36.540186
1490.451849	200125.024139	36.545204
1492.039446	200502.377443	36.550221
1493.248022	200893.114006	36.555239
1494.289107	201285.429380	36.560256
1496.279357	201672.854246	36.565274
1497.788278	202076.383957	36.570292
1499.400796	202480.330496	36.575309
1500.868173	202871.136648	36.580327
1502.621028	203263.218194	36.585344
1504.284883	203651.482048	36.590362
1505.312067	204050.721784	36.595380
1507.079835	204443.340372	36.600397
1508.731433	204842.214507	36.605415
1510.272110	205236.652337	36.610432
1511.687626	205626.910077	36.615450
1513.043135	206022.207863	36.620468
1514.341753	206416.894886	36.625485
1515.920064	206813.531195	36.630503
1517.338655	207214.868587	36.635520
1518.917561	207607.521747	36.640538
1520.267862	208007.807814	36.645556
1521.985957	208423.577134	36.650573
1523.524514	208823.632964	36.655591
1524.763761	209219.791162	36.660608
1526.522641	209633.540918	36.665626
1527.844049	210036.457434	36.670644
1529.553144	210441.114950	36.675661
1530.995796	210827.939482	36.680679
1532.488697	211210.008350	36.685696
1534.067571	211596.102742	36.690714
1535.327689	211982.734050	36.695732
1536.971498	212373.646502	36.700749
1538.348802	212770.268198	36.705767
1539.879708	213157.266257	36.710784
1541.463504	213544.765184	36.715802
1542.938605	213942.798131	36.720820
1544.316063	214343.083898	36.725837
1545.898879	214748.518530	36.730855
1547.345560	215155.958419	36.735872
1548.977008	215553.312118	36.740890
1550.713712	215971.272990	36.745908
1552.092962	216383.250075	36.750925
1553.776383	216783.444842	36.755943
1554.930467	217208.390143	36.760960
1556.625200	217614.148588	36.765978
1557.895611	218037.554338	36.770996
1559.626276	218451.285272	36.776013
1561.162072	218881.330461	36.781031
1562.572561	219304.819937	36.786048
1564.208037	219732.058361	36.791066
1565.499970	220175.331074	36.796084
1567.268623	220608.494340	36.801101
1569.060924	221036.982044	36.806119
1570.622329	221472.570512	36.811136
1572.175717	221913.292652	36.816154
1573.766250	222349.260746	36.821172
1575.206689	222787.287271	36.826189
1576.768380	223239.290526	36.831207
1577.929742	223681.836868	36.836224
1579.911064	224144.797710	36.841242
1581.552405	224644.468325	36.846260
1583.041659	225100.884841	36.851277
1584.548268	225542.339649	36.856295
1586.348405	225995.761743	36.861312
1588.014546	226447.963011	36.866330
1589.642480	226904.490232	36.871348
1591.546143	227351.346816	36.876365
1593.139271	227791.245731	36.881383
1594.316230	228262.965414	36.886400
1596.130751	228712.178151	36.891418
1597.547141	229168.392506	36.896436
1599.642383	229621.092518	36.901453
1601.335980	230071.142455	36.906471
1602.910575	230529.519547	36.911488
1604.768102	230989.502403	36.916506
1606.358177	231427.609797	36.921524
1607.867516	231882.902942	36.926541
1609.595605	232329.626514	36.931559
1611.098205	232786.777726	36.936576
1612.648548	233231.196316	36.941594
1614.195273	233691.568796	36.946612
1615.772713	234154.528443	36.951629
1617.313783	234609.722515	36.956647
1618.670091	235071.603542	36.961664
1620.026410	235538.743939	36.966682
1622.288931	235999.614050	36.971700
1623.430688	236470.602582	36.976717
1625.397212	236930.101441	36.981735
1626.940879	237392.059053	36.986752
1628.655403	237854.624599	36.991770
1630.425021	238317.867984	36.996788
1631.742394	238785.607108	37.001805
1633.772514	239245.227875	37.006823
1634.814588	239711.490424	37.011840
1636.657561	240161.542048	37.016858
1638.322178	240615.383591	37.021876
1639.962477	241071.567075	37.026893
1641.550468	241512.417043	37.031911
1642.861812	241963.779332	37.036928
1644.572897	242408.878209	37.041946
1645.778697	242858.582991	37.046964
1647.355129	243319.429865	37.051981
1649.294715	243776.966008	37.056999
1650.608641	244257.697288	37.062016
1652.247139	244719.018899	37.067034
1653.976799	245185.711556	37.072052
1655.315987	245664.713574	37.077069
1657.529692	246126.247132	37.082087
1658.955601	246604.982196	37.087104
1660.695169	247072.184013	37.092122
1662.418778	247543.936207	37.097140
1663.771918	248036.529819	37.102157
1665.804178	248509.756411	37.107175
1667.448257	249011.905509	37.112192
1669.174600	249491.712330	37.117210
1671.347132	249979.244704	37.122228
1672.812223	250458.943269	37.127245
1674.493411	250924.965120	37.132263
1676.279035	251414.518843	37.137280
1677.869838	251900.421709	37.142298
1679.604739	252389.070108	37.147316
1681.034119	252881.401995	37.152333
1683.057892	253372.619910	37.157351
1684.791159	253869.576444	37.162368
1686.434889	254357.199659	37.167386
1688.094813	254848.859565	37.172404
1689.855707	255336.692523	37.177421
1691.653788	255832.089707	37.182439
1693.459735	256335.386182	37.187456
1694.889657	256823.274302	37.192474
1696.948057	257323.785767	37.197492
1698.348618	257822.703951	37.202509
1700.202216	258318.600567	37.207527
1702.020924	258816.814664	37.212544
1703.848655	259318.761543	37.217562
1705.596758	259814.904175	37.222580
1707.081149	260310.455211	37.227597
1708.874867	260806.742552	37.232615
1710.575344	261314.806882	37.237632
1712.273522	261818.425848	37.242650
1714.293841	262315.589782	37.247668
1715.622191	262824.070621	37.252685
1717.747900	263326.246503	37.257703
1719.608700	263830.472704	37.262720
1721.545943	264332.247246	37.267738
1722.764181	264841.913570	37.272756
1724.272972	265337.559765	37.277773
1726.285940	265835.738803	37.282791
1727.929810	266355.825049	37.287808
1729.611374	266872.144897	37.292826
1731.603820	267372.713763	37.297844
1733.278377	267887.992150	37.302861
1735.120360	268394.249616	37.307879
1736.688136	268902.863428	37.312896
1738.257499	269414.118232	37.317914
1740.132510	269920.342891	37.322932
1741.841602	270440.184781	37.327949
1743.826775	270937.752811	37.332967
1745.353414	271457.928104	37.337984
1747.041963	271968.117927	37.343002
1749.037454	272476.503414	37.348020
1750.433282	272994.563872	37.353037
1752.400418	273496.042727	37.358055
1754.215056	273982.431324	37.363072
1755.839179	274484.574657	37.368090
1757.330098	274967.331523	37.373108
1759.108295	275460.175574	37.378125
1760.746487	275955.759800	37.383143
1762.255957	276456.901948	37.388160
1764.035886	276954.010173	37.393178
1766.212440	277456.894288	37.398196
1767.395789	277964.945496	37.403213
1769.520461	278473.525867	37.408231
1770.814433	278986.433511	37.413248
1772.425745	279502.970713	37.418266
1774.131474	280027.873576	37.423284
1775.845574	280548.226688	37.428301
1777.808077	281079.053638	37.433319
1779.443388	281606.961083	37.438336
1781.213421	282148.104333	37.443354
1783.228248	282675.133034	37.448372
1784.855036	283213.781833	37.453389
1786.784285	283743.386856	37.458407
1788.328430	284287.583274	37.463424
1789.736342	284830.149254	37.468442
1791.778380	285379.162092	37.473460
1793.513761	285930.662095	37.478477
1795.380369	286475.737367	37.483495
1797.390987	287040.980457	37.488512
1799.229491	287589.256686	37.493530
1801.213841	288137.455894	37.498548
1802.750342	288703.558037	37.503565
1804.621402	289262.338055	37.508583
1807.055105	289821.226011	37.513600
1808.476157	290381.599629	37.518618
1810.672168	290935.823006	37.523636
1811.914818	291503.841168	37.528653
1813.687319	292063.666683	37.533671
1815.993504	292620.556725	37.538688
1817.881979	293194.988085	37.543706
1819.583865	293756.874732	37.548724
1821.130817	294327.394624	37.553741
1823.124239	294899.006300	37.558759
1825.031692	295463.441330	37.563776
1826.754225	296037.047646	37.568794
1828.598451	296611.062629	37.573812
1830.451841	297183.320524	37.578829
1832.286338	297763.451993	37.583847
1834.081591	298334.087715	37.588864
1836.202689	298907.714249	37.593882
1838.404749	299487.546702	37.598900
1840.006067	300070.598946	37.603917
1842.019675	300632.982028	37.608935
1844.019449	301209.561433	37.613952
1845.759561	301786.408829	37.618970
1847.742929	302356.939388	37.623988
1849.225837	302943.854106	37.629005
1851.024790	303510.776221	37.634023
1852.979974	304086.608702	37.639040
1854.910965	304670.644622	37.644058
1856.824524	305251.631988	37.649076
1859.057184	305820.169372	37.654093
1860.748082	306406.315865	37.659111
1862.543577	306976.949485	37.664128
1864.560512	307547.034763	37.669146
1866.307545	308127.649133	37.674164
1868.550369	308701.142986	37.679181
1870.451909	309273.114652	37.684199
1872.540787	309847.692417	37.689216
1873.890648	310425.054547	37.694234
1876.035703	310985.266634	37.699252
1877.964272	311539.390347	37.704269
1879.972180	312088.037179	37.709287
1881.810061	312632.873615	37.714304
1883.298177	313170.958276	37.719322
1885.139155	313716.294232	37.724340
1886.733577	314283.937136	37.729357
1888.481355	314830.626100	37.734375
1890.361983	315392.880485	37.739392
1891.856696	315960.958428	37.744410
1893.402835	316523.513091	37.749428
1895.456657	317108.223408	37.754445
1897.010418	317683.971687	37.759463
1898.974530	318279.021685	37.764480
1901.002043	318868.368226	37.769498
1902.735383	319453.035341	37.774516
1904.362857	320053.356049	37.779533
1906.348560	320654.246962	37.784551
1908.385610	321254.641476	37.789568
1909.953628	321868.590456	37.794586
1912.013028	322466.456361	37.799604
1914.059637	323085.164290	37.804621
1915.773612	323701.864495	37.809639
1918.163246	324315.247943	37.814656
1920.039800	324937.037851	37.819674
1921.825085	325548.401515	37.824692
1923.848588	326172.998219	37.829709
1925.883178	326796.088691	37.834727
1927.705043	327405.828016	37.839744
1929.578631	328043.175024	37.844762
1931.725581	328668.436051	37.849780
1934.037116	329293.155433	37.854797
1935.616208	329930.505027	37.859815
1937.441794	330552.523722	37.864832
1939.417139	331189.768410	37.869850
1941.712411	331822.561159	37.874868
1943.977072	332459.769000	37.879885
1945.447595	333106.138051	37.884903
1947.483338	333731.107500	37.889920
1949.463715	334373.950261	37.894938
1951.274340	335006.963937	37.899956
1953.237329	335658.577429	37.904973
1955.433324	336297.122163	37.909991
1957.265705	336948.487434	37.915008
1959.206235	337598.252897	37.920026
1961.428174	338235.678064	37.925044
1963.352943	338899.619110	37.930061
1965.527015	339533.888433	37.935079
1967.651332	340169.782476	37.940096
1969.308642	340819.045860	37.945114
1971.600833	341465.048559	37.950132
1973.366727	342130.140507	37.955149
1974.879289	342775.848552	37.960167
1977.298295	343419.773951	37.965184
1979.077072	344083.542531	37.970202
1981.034355	344728.161085	37.975220
1982.821731	345400.767552	37.980237
1985.042967	346053.268315	37.985255
1987.477116	346700.674337	37.990272
1989.168250	347360.578839	37.995290
1991.415649	348007.489768	38.000308
1993.941489	348653.355802	38.005325
1995.700916	349312.713218	38.010343
1997.977576	349953.906891	38.015360
2000.167464	350602.211234	38.020378
2002.247109	351243.114320	38.025396
2004.331528	351888.371997	38.030413
2006.324968	352520.794974	38.035431
2008.493532	353135.696097	38.040448
2010.295909	353770.111644	38.045466
2012.307667	354374.033498	38.050484
2014.170314	354994.642391	38.055501
2015.902230	355596.537714	38.060519
2018.117391	356221.333184	38.065536
2019.878131	356832.898721	38.070554
2021.688454	357447.897773	38.075572
2023.871300	358075.563163	38.080589
2025.099338	358708.780837	38.085607
2027.334752	359341.543259	38.090624
2029.078351	359988.356588	38.095642
2030.974953	360637.189292	38.100660
2033.263129	361279.020655	38.105677
2035.110068	361921.599474	38.110695
2036.764571	362578.152920	38.115712
2038.719291	363248.142244	38.120730
2041.038537	363915.421499	38.125748
2042.782993	364579.714563	38.130765
2044.391382	365249.878604	38.135783
2047.142556	365920.451041	38.140800
2048.991887	366616.781211	38.145818
2050.943829	367295.223529	38.150836
2053.044907	367971.980146	38.155853
2054.634697	368660.603891	38.160871
2056.615324	369356.582291	38.165888
2058.711372	370060.315415	38.170906
2061.149572	370760.123143	38.175924
2063.103990	371460.529885	38.180941
2065.136057	372175.316502	38.185959
2067.354105	372878.467419	38.190976
2069.295816	373594.077546	38.195994
2071.274926	374305.380914	38.201012
2073.615273	375026.019252	38.206029
2075.550639	375747.115364	38.211047
2077.908853	376457.754429	38.216064
2079.939555	377185.550645	38.221082
2081.907136	377909.816946	38.226100
2084.503170	378631.834011	38.231117
2085.981076	379353.690630	38.236135
2088.434034	380075.599044	38.241152
2090.772959	380814.854807	38.246170
2092.920119	381533.080098	38.251188
2095.140305	382261.420044	38.256205
2097.214825	382992.607692	38.261223
2099.490663	383710.054275	38.266240
2101.904406	384437.426403	38.271258
2104.049616	385153.239957	38.276276
2106.288302	385875.968837	38.281293
2107.952374	386603.466409	38.286311
2110.239913	387320.754414	38.291328
2113.099421	388044.370914	38.296346
2114.982287	388763.340704	38.301364
2117.290297	389482.908221	38.306381
2119.417730	390210.144405	38.311399
2121.718447	390919.159763	38.316416
2124.167542	391638.577742	38.321434
2126.034148	392340.204851	38.326452
2128.057541	393057.327632	38.331469
2130.128270	393776.833506	38.336487
2132.798388	394486.743879	38.341504
2134.764528	395202.506979	38.346522
2136.828764	395916.107721	38.351540
2138.981211	396623.467416	38.356557
2141.095281	397329.346536	38.361575
2143.169509	398036.203594	38.366592
2145.519920	398750.043047	38.371610
2147.422547	399460.416363	38.376628
2149.896671	400159.933296	38.381645
2151.682938	400851.817922	38.386663
2153.766634	401528.762280	38.391680
2155.814809	402220.646457	38.396698
2157.970930	402902.411173	38.401716
2160.395021	403582.645549	38.406733
2161.563447	404269.303640	38.411751
2163.908833	404954.433049	38.416768
2165.984764	405665.660763	38.421786
2167.855621	406365.680456	38.426804
2170.364480	407068.895856	38.431821
2172.090198	407780.836013	38.436839
2174.151371	408486.596840	38.441856
2176.553376	409210.851895	38.446874
2178.677023	409929.991038	38.451892
2180.758130	410659.757086	38.456909
2182.666578	411390.164953	38.461927
2184.756079	412117.331286	38.466944
2187.032635	412854.553112	38.471962
2188.771503	413588.778282	38.476980
2191.372307	414332.566479	38.481997
2193.482173	415094.295389	38.487015
2195.640087	415847.990877	38.492032
2197.925279	416602.479089	38.497050
2199.951505	417369.346396	38.502068
2202.625128	418131.525504	38.507085
2204.688553	418900.239925	38.512103
2206.912025	419663.409592	38.517120
2208.920196	420423.679667	38.522138
2211.287399	421202.377069	38.527156
2213.704914	421969.470529	38.532173
2215.641012	422741.177237	38.537191
2218.019161	423524.813225	38.542208
2220.401729	424305.537278	38.547226
2222.517854	425095.698317	38.552244
2224.796795	425873.401924	38.557261
2226.961919	426668.870738	38.562279
2229.110199	427446.444054	38.567296
2231.061868	428252.629101	38.572314
2233.319785	429046.586250	38.577332
2236.067589	429835.120519	38.582349
2238.363729	430630.132085	38.587367
2240.663696	431429.267074	38.592384
2242.923262	432232.785330	38.597402
2245.532720	433036.066320	38.602420
2247.803557	433826.924042	38.607437
2250.044076	434624.339481	38.612455
2251.867453	435422.960208	38.617472
2254.489597	436226.937763	38.622490
2256.642503	437026.510883	38.627508
2259.213154	437827.909939	38.632525
2261.065734	438621.858978	38.637543
2263.578540	439428.271154	38.642560
2265.946122	440234.374645	38.647578
2268.020926	441052.438716	38.652596
2270.232690	441852.993938	38.657613
2272.273780	442657.747743	38.662631
2275.016995	443464.430564	38.667648
2277.159120	444276.596178	38.672666
2279.304818	445088.983890	38.677684
2281.800211	445898.399958	38.682701
2283.963012	446709.408755	38.687719
2286.141004	447530.197795	38.692736
2288.489520	448337.219444	38.697754
2290.872610	449145.924569	38.702772
2293.255434	449959.707344	38.707789
2295.542638	450772.918224	38.712807
2297.746209	451589.702267	38.717824
2300.115027	452398.790751	38.722842
2302.308353	453195.082465	38.727860
2304.630316	453965.178425	38.732877
2306.960647	454759.364702	38.737895
2309.260280	455540.378581	38.742912
2311.383459	456323.616625	38.747930
2313.831343	457110.967632	38.752948
2316.145061	457897.349703	38.757965
2318.135387	458694.068273	38.762983
2320.343486	459496.432188	38.768000
2322.841372	460292.700463	38.773018
2324.478344	461106.418129	38.778036
2326.952936	461909.804053	38.783053
2329.103572	462730.497960	38.788071
2331.554537	463557.527440	38.793088
2333.180973	464379.149127	38.798106
2335.317690	465211.720569	38.803124
2338.089460	466060.222907	38.808141
2340.064588	466903.968244	38.813159
2342.395906	467758.634441	38.818176
2344.824050	468608.345246	38.823194
2347.239817	469470.652850	38.828212
2349.566654	470327.378299	38.833229
2351.998027	471195.213952	38.838247
2354.414461	472066.346863	38.843264
2356.778035	472950.027835	38.848282
2359.133244	473822.352729	38.853300
2361.753463	474693.481949	38.858317
2363.650012	475587.723824	38.863335
2366.201298	476456.761416	38.868352
2369.126873	477338.373984	38.873370
2371.430895	478227.218748	38.878388
2373.735350	479106.576285	38.883405
2376.401029	480001.739672	38.888423
2378.478921	480884.381940	38.893440
2381.163409	481773.445608	38.898458
2383.688155	482670.368813	38.903476
2386.049764	483554.399026	38.908493
2388.486887	484453.267200	38.913511
2390.774248	485339.190414	38.918528
2392.914141	486240.390209	38.923546
2395.603027	487138.222744	38.928564
2398.367655	488044.830689	38.933581
2400.815181	488940.440452	38.938599
2403.117255	489834.514130	38.943616
2405.861592	490740.884603	38.948634
2407.909821	491639.146786	38.953652
2410.079800	492545.870747	38.958669
2412.961482	493440.167119	38.963687
2415.091985	494349.880500	38.968704
2417.904028	495253.579914	38.973722
2420.180105	496165.846485	38.978740
2423.093822	497063.731331	38.983757
2425.432368	497976.646588	38.988775
2427.551473	498867.553901	38.993792
2430.313025	499770.817764	38.998810
2432.601207	500679.659255	39.003828
2435.218626	501580.730100	39.008845
2437.939276	502496.209721	39.013863
2439.677766	503398.183766	39.018880
2442.449489	504308.611669	39.023898
2445.158029	505215.973681	39.028916
2447.324782	506105.776539	39.033933
2449.583545	507015.330979	39.038951
2451.945219	507934.598426	39.043968
2454.710896	508845.529012	39.048986
2457.073581	509753.701659	39.054004
2459.527138	510675.922437	39.059021
2461.941689	511577.681462	39.064039
2464.034455	512459.129487	39.069056
2466.642347	513354.102099	39.074074
2468.882313	514234.569820	39.079092
2471.026145	515115.558349	39.084109
2473.632663	516011.538707	39.089127
2475.416477	516892.284773	39.094144
2477.945407	517803.493176	39.099162
2480.344800	518718.246520	39.104180
2482.396660	519618.291683	39.109197
2485.084376	520541.353032	39.114215
2487.270612	521472.501391	39.119232
2489.540620	522392.698754	39.124250
2491.989386	523334.821982	39.129268
2494.530203	524276.619537	39.134285
2497.200945	525218.185731	39.139303
2498.937308	526179.638197	39.144320
2501.736123	527130.329237	39.149338
2504.116117	528113.556551	39.154356
2506.431316	529076.186959	39.159373
2508.840051	530053.087928	39.164391
2511.309465	531044.664539	39.169408
2513.990455	532023.554490	39.174426
2516.359527	533039.729230	39.179444
2518.935745	534024.190281	39.184461
2521.686229	535023.855815	39.189479
2523.883056	536042.314951	39.194496
2526.654377	537044.906942	39.199514
2528.600819	538061.201238	39.204532
2531.280528	539071.918687	39.209549
2533.950840	540097.608991	39.214567
2536.264414	541129.974903	39.219584
2538.672805	542163.205570	39.224602
2541.520618	543213.490543	39.229620
2544.032405	544257.515597	39.234637
2547.067391	545295.341262	39.239655
2549.581402	546336.494559	39.244672
2552.186182	547373.330801	39.249690
2554.729338	548433.329283	39.254708
2556.879662	549491.450693	39.259725
2559.640444	550536.570065	39.264743
2562.351844	551599.915713	39.269760
2565.200285	552652.348585	39.274778
2567.902724	553725.733190	39.279796
2570.211680	554781.658022	39.284813
2573.091476	555839.667247	39.289831
2575.669468	556900.205487	39.294848
2578.372981	557962.598388	39.299866
2581.238716	559025.030426	39.304884
2583.681139	560088.100228	39.309901
2586.325094	561143.968286	39.314919
2588.983227	562209.544041	39.319936
2591.472577	563282.594840	39.324954
2593.882556	564339.901532	39.329972
2596.575874	565407.018600	39.334989
2599.579043	566474.097155	39.340007
2601.931586	567536.374827	39.345024
2604.480789	568613.443211	39.350042
2607.173270	569678.299176	39.355060
2609.709113	570753.583275	39.360077
2612.407817	571823.931255	39.365095
2615.250837	572904.001933	39.370112
2617.553857	573975.036349	39.375130
2620.026621	575041.234837	39.380148
2622.923662	576116.856185	39.385165
2625.531174	577193.436172	39.390183
2627.772202	578280.117183	39.395200
2630.654452	579346.181409	39.400218
2633.172356	580413.919217	39.405236
2635.424313	581471.627905	39.410253
2638.661119	582507.167948	39.415271
2640.764826	583556.948123	39.420288
2643.817196	584593.244416	39.425306
2646.358179	585647.986852	39.430324
2648.590030	586697.324372	39.435341
2651.287738	587737.922085	39.440359
2653.511633	588804.321379	39.445376
2656.386728	589859.291896	39.450394
2658.890898	590931.319415	39.455412
2661.331577	591999.302282	39.460429
2664.189810	593075.237239	39.465447
2666.711513	594159.847344	39.470464
2669.415862	595239.618546	39.475482
2672.030574	596324.815351	39.480500
2674.762450	597426.921705	39.485517
2677.168052	598521.315270	39.490535
2679.544618	599622.821751	39.495552
2682.426529	600733.553793	39.500570
2685.247041	601856.205320	39.505588
2687.697616	602973.401598	39.510605
2690.533891	604097.483573	39.515623
2692.932784	605224.580343	39.520640
2695.819071	606363.046217	39.525658
2698.520042	607497.074743	39.530676
2701.073449	608636.568080	39.535693
2703.760940	609780.827292	39.540711
2706.338851	610931.841757	39.545728
2709.314757	612085.623524	39.550746
2712.173059	613250.709200	39.555764
2715.111233	614408.857959	39.560781
2717.807294	615562.174907	39.565799
2720.565379	616732.511543	39.570816
2723.063355	617893.967248	39.575834
2726.003859	619053.527204	39.580852
2728.662952	620236.803450	39.585869
2731.661310	621407.500094	39.590887
2734.275337	622594.875171	39.595904
2737.456795	623770.833177	39.600922
2740.136137	624946.195973	39.605940
2742.806053	626127.176771	39.610957
2745.828143	627303.473361	39.615975
2748.305732	628485.124185	39.620992
2751.067130	629665.298276	39.626010
2754.045818	630846.203790	39.631028
2756.418049	632045.201749	39.636045
2759.519980	633232.410082	39.641063
2762.322700	634423.027517	39.646080
2765.385775	635616.461012	39.651098
2768.401327	636806.920720	39.656116
2770.754830	637995.656265	39.661133
2773.919173	639179.680622	39.666151
2776.476226	640381.330075	39.671168
2779.053028	641573.257818	39.676186
2782.169362	642766.603684	39.681204
2784.709244	643970.378137	39.686221
2787.596965	645157.845678	39.691239
2790.450518	646358.093532	39.696256
2793.473502	647548.947538	39.701274
2796.272544	648740.993537	39.706292
2798.800998	649944.057387	39.711309
2801.749102	651140.478200	39.716327
2804.899150	652330.991382	39.721344
2807.667078	653525.161629	39.726362
2810.705319	654719.342408	39.731380
2813.484107	655912.674122	39.736397
2816.357093	657097.876279	39.741415
2819.022515	658281.624620	39.746432
2821.582971	659433.377981	39.751450
2824.689677	660592.821431	39.756468
2827.119035	661744.471821	39.761485
2830.338109	662883.958088	39.766503
2833.103787	664036.673377	39.771520
2835.468529	665195.139068	39.776538
2838.671644	666345.663515	39.781556
2841.366885	667509.815258	39.786573
2844.172072	668664.553553	39.791591
2846.965526	669838.950262	39.796608
2849.329512	670997.854198	39.801626
2852.148870	672174.244128	39.806644
2854.651072	673357.251718	39.811661
2857.439005	674542.498995	39.816679
2860.421134	675745.360028	39.821696
2863.115409	676942.397294	39.826714
2866.249809	678141.642818	39.831732
2868.874472	679362.879558	39.836749
2871.626103	680572.307698	39.841767
2874.455071	681793.685303	39.846784
2877.321507	683022.344600	39.851802
2880.304053	684252.259803	39.856820
2883.071981	685494.855867	39.861837
2885.956237	686736.269687	39.866855
2888.758948	687982.689592	39.871872
2891.410741	689234.521469	39.876890
2894.273510	690491.107257	39.881908
2897.374011	691761.272768	39.886925
2900.049733	693038.670817	39.891943
2903.182121	694316.752890	39.896960
2905.748441	695600.051568	39.901978
2908.971059	696868.921596	39.906996
2911.663083	698168.291574	39.912013
2914.752368	699451.588119	39.917031
2917.261418	700743.963188	39.922048
2920.012805	702037.296591	39.927066
2923.520330	703338.589222	39.932084
2926.038057	704663.732856	39.937101
2929.390146	705971.542850	39.942119
2932.205001	707284.097335	39.947136
2935.101520	708608.274773	39.952154
2938.114440	709920.838730	39.957172
2940.868763	711248.790133	39.962189
2944.198567	712578.320475	39.967207
2947.357120	713900.345062	39.972224
2949.883162	715231.719379	39.977242
2953.057431	716560.203373	39.982260
2955.828124	717904.325461	39.987277
2959.112184	719232.664491	39.992295
2961.987559	720572.184936	39.997312
2965.048982	721912.497270	40.002330
2968.201302	723248.375300	40.007348
2970.565344	724588.962171	40.012365
2973.751187	725932.902109	40.017383
2976.689158	727271.029243	40.022400
2979.715166	728619.941029	40.027418
2982.766281	729968.773648	40.032436
2985.960583	731327.187769	40.037453
2988.995821	732674.980245	40.042471
2991.839317	734032.898791	40.047488
2994.833420	735391.106378	40.052506
2997.852006	736738.813258	40.057524
3000.513901	738108.904923	40.062541
3003.476185	739460.109561	40.067559
3006.907286	740817.469750	40.072576
3009.771900	742175.085191	40.077594
3012.829815	743532.336586	40.082612
3015.412747	744876.069587	40.087629
3018.540816	746199.220245	40.092647
3021.238537	747516.253599	40.097664
3023.854996	748851.558977	40.102682
3027.082459	750172.293748	40.107700
3030.114562	751500.126894	40.112717
3032.974512	752836.922000	40.117735
3036.002294	754169.418837	40.122752
3038.493208	755514.132164	40.127770
3042.126711	756865.460924	40.132788
3044.884984	758208.572637	40.137805
3047.750904	759568.555921	40.142823
3050.443175	760928.520593	40.147840
3053.355199	762312.458133	40.152858
3056.170470	763688.729985	40.157876
3058.686378	765077.831152	40.162893
3061.881850	766484.214189	40.167911
3065.305556	767886.017518	40.172928
3068.048988	769315.192943	40.177946
3071.139671	770722.118670	40.182964
3074.002181	772153.428991	40.187981
3076.984861	773588.371062	40.192999
3080.125688	775028.408890	40.198016
3083.193205	776470.434070	40.203034
3086.314371	777924.585738	40.208052
3089.151697	779381.143753	40.213069
3092.480132	780851.117509	40.218087
3096.011758	782302.359890	40.223104
3098.874891	783792.024570	40.228122
3102.118785	785259.493136	40.233140
3105.344189	786735.930768	40.238157
3108.358752	788201.655480	40.243175
3111.760313	789693.970812	40.248192
3114.396689	791192.614991	40.253210
3117.625629	792676.243800	40.258228
3120.928900	794168.657934	40.263245
3123.928482	795669.080485	40.268263
3127.375109	797167.932155	40.273280
3130.545724	798678.695204	40.278298
3133.724841	800175.082603	40.283316
3136.784608	801683.349225	40.288333
3139.996999	803193.315391	40.293351
3143.435386	804712.840703	40.298368
3146.606228	806244.737118	40.303386
3149.728943	807750.828789	40.308404
3152.798947	809270.573895	40.313421
3155.932056	810791.092022	40.318439
3159.356386	812313.760559	40.323456
3162.305820	813835.430742	40.328474
3165.421430	815367.569125	40.333492
3168.917166	816894.021864	40.338509
3171.634614	818429.966435	40.343527
3175.160614	819955.078340	40.348544
3177.957088	821492.838906	40.353562
3181.569946	823027.473372	40.358580
3184.131015	824569.237975	40.363597
3187.307510	826107.614128	40.368615
3190.685907	827656.707934	40.373632
3193.856863	829213.508092	40.378650
3197.206108	830757.288695	40.383668
3200.381690	832308.328029	40.388685
3203.349178	833856.643300	40.393703
3206.599733	835401.375353	40.398720
3209.572007	836970.992017	40.403738
3212.673492	838523.561550	40.408756
3215.996027	840096.925903	40.413773
3219.338255	841662.067558	40.418791
3222.731403	843224.383039	40.423808
3225.414794	844773.596102	40.428826
3228.945775	846311.499591	40.433844
3232.089022	847826.643498	40.438861
3234.872757	849357.897467	40.443879
3238.384652	850872.435747	40.448896
3241.185269	852400.801579	40.453914
3244.104324	853919.354528	40.458932
3247.552662	855465.203651	40.463949
3250.636157	857003.641739	40.468967
3253.985051	858541.650433	40.473984
3257.207618	860101.986165	40.479002
3260.424324	861655.718614	40.484020
3263.826476	863207.181732	40.489037
3266.708056	864783.722102	40.494055
3269.987518	866353.100869	40.499072
3272.967441	867941.006196	40.504090
3276.144130	869522.843042	40.509108
3279.534023	871112.454606	40.514125
3282.586173	872714.665956	40.519143
3286.041116	874320.249031	40.524160
3289.035976	875940.851692	40.529178
3292.289610	877563.674494	40.534196
3295.329695	879188.598487	40.539213
3298.850472	880830.098916	40.544231
3302.417525	882460.889758	40.549248
3305.692465	884109.624126	40.554266
3308.763472	885744.888572	40.559284
3312.068171	887413.921887	40.564301
3315.267411	889079.787802	40.569319
3318.874165	890747.226644	40.574336
3322.097979	892424.660054	40.579354
3325.355466	894107.862822	40.584372
3328.779333	895781.672722	40.589389
3331.992077	897474.681881	40.594407
3335.515013	899154.320903	40.599424
3338.579354	900855.300126	40.604442
3341.881776	902548.312084	40.609460
3345.189311	904259.772070	40.614477
3348.520572	905964.738015	40.619495
3352.102112	907676.835259	40.624512
3355.385824	909387.395215	40.629530
3358.481853	911108.607494	40.634548
3361.717437	912828.874570	40.639565
3365.065618	914566.260421	40.644583
3368.425458	916300.787771	40.649600
3371.893174	918056.346907	40.654618
3375.093595	919790.748361	40.659636
3378.570061	921525.220534	40.664653
3382.112763	923299.216052	40.669671
3385.454466	925035.937129	40.674688
3389.218438	926804.615100	40.679706
3392.400081	928554.214752	40.684724
3395.894362	930298.973429	40.689741
3398.885759	932060.573058	40.694759
3402.269228	933810.991850	40.699776
3405.884686	935588.254592	40.704794
3409.268037	937347.640052	40.709812
3412.935902	939107.726200	40.714829
3416.142665	940879.913072	40.719847
3419.780810	942637.472959	40.724864
3423.245726	944408.126076	40.729882
3426.256106	946178.915610	40.734900
3429.923778	947947.937712	40.739917
3432.993173	949721.792546	40.744935
3436.668613	951494.359859	40.749952
3439.911450	953301.879932	40.754970
3443.427707	955121.451691	40.759988
3447.154149	956934.547916	40.765005
3449.883694	958748.256081	40.770010
3453.183519	960505.835843	40.775015
3456.696182	962218.766537	40.780020
3459.632038	963857.742851	40.785024
3463.236745	965421.056004	40.790029
3465.936849	966923.511279	40.795034
3468.847595	968357.829659	40.800039
3471.659827	969719.025999	40.805044
3474.475850	971003.027576	40.810048
3477.262380	972200.797913	40.815053
3479.634124	973347.843914	40.820058
3482.269760	974409.776510	40.825063
3484.540801	975403.066680	40.830068
3486.615277	976335.148362	40.835072
3488.941028	977199.920534	40.840077
3490.365942	978013.818552	40.845082
3492.487923	978750.230455	40.850087
3494.389278	979431.798441	40.855092
3496.248633	980063.980881	40.860096
3497.981097	980629.331251	40.865101
3499.205571	981154.975041	40.870106
3500.760925	981634.830268	40.875111
3502.187521	982043.800292	40.880116
3503.423328	982425.540479	40.885120
3504.736099	982754.733839	40.890125
3505.793818	983052.427115	40.895130
3507.131033	983296.579311	40.900135
3508.232693	983519.876277	40.905140
3509.057943	983702.517724	40.910144
3510.090094	983852.722356	40.915149
3511.067391	983965.461737	40.920154
3511.814705	984043.987019	40.925159
3512.897299	984100.793938	40.930164
3513.717634	984129.151236	40.935168
3514.522280	984119.846523	40.940173
3515.155480	984097.104428	40.945178
3515.786230	984048.992466	40.950183
3516.317158	983976.306669	40.955188
3516.800438	983883.331055	40.960192
3517.671623	983763.747588	40.965197
3518.333831	983638.243371	40.970202
3518.882298	983479.185104	40.975207
3519.346348	983302.277256	40.980212
3519.469451	983115.465531	40.985216
3519.997676	982907.011969	40.990221
3520.086286	982695.987986	40.995226
3520.856257	982473.228990	41.000231
3520.955351	982229.000279	41.005236
3521.123652	981976.647813	41.010240
3521.672864	981712.214455	41.015245
3521.837452	981438.362835	41.020250
3521.993219	981154.346290	41.025255
3522.425252	980873.003801	41.030260
3522.390728	980572.392152	41.035264
3522.809577	980266.905500	41.040269
3522.721688	979951.721202	41.045274
3523.220847	979628.805829	41.050279
3523.586124	979306.773189	41.055284
3523.365290	978961.965422	41.060288
3523.552272	978620.195116	41.065293
3523.840521	978276.629506	41.070298
3523.930123	977921.940158	41.075303
3523.782729	977557.694339	41.080308
3523.741000	977198.390344	41.085312
3523.907673	976831.506440	41.090317
3523.903318	976473.420842	41.095322
3524.301452	976100.296330	41.100327
3524.253878	975723.702983	41.105332
3524.230664	975351.380799	41.110336
3524.216086	974964.666207	41.115341
3524.065120	974584.594248	41.120346
3524.295087	974195.343893	41.125351
3524.225203	973827.719831	41.130356
3523.935356	973441.729705	41.135360
3524.081603	973047.624916	41.140365
3524.124172	972664.851703	41.145370
3524.101714	972266.223413	41.150375
3524.444166	971872.885502	41.155380
3524.472988	971468.130516	41.160384
3524.308344	971069.246801	41.165389
3524.183660	970665.047192	41.170394
3524.216902	970277.127890	41.175399
3524.192303	969872.269030	41.180404
3523.889431	969481.514501	41.185408
3524.076431	969069.129261	41.190413
3523.582975	968680.210386	41.195418
3524.138052	968276.806725	41.200423
3524.179835	967888.039533	41.205428
3523.977047	967486.172982	41.210432
3523.978322	967086.887107	41.215437
3523.613944	966688.025208	41.220442
3523.602989	966273.612139	41.225447
3523.745477	965869.520067	41.230452
3523.534230	965475.247365	41.235456
3523.937603	965060.189057	41.240461
3523.679676	964671.938865	41.245466
3523.652879	964258.655919	41.250471
3523.365813	963854.101265	41.255476
3523.247203	963464.571520	41.260480
3523.241626	963051.492117	41.265485
3522.733069	962649.533502	41.270490
3522.931837	962253.307267	41.275495
3523.191199	961866.251692	41.280500
3522.817690	961466.539151	41.285504
3523.231892	961063.827953	41.290509
3522.847231	960678.072218	41.295514
3523.217746	960277.174780	41.300519
3522.715817	959874.335384	41.305524
3522.732872	959475.988180	41.310528
3523.211422	959066.952987	41.315533
3522.851812	958685.077833	41.320538
3522.619438	958277.083825	41.325543
3522.779386	957881.837496	41.330548
3522.161160	957488.554868	41.335552
3522.591160	957102.425539	41.340557
3522.470855	956706.654671	41.345562
3522.621923	956306.889912	41.350567
3522.726179	955915.636196	41.355572
3522.303626	955510.517611	41.360576
3522.031260	955125.548514	41.365581
3522.190226	954742.248085	41.370586
3522.414679	954344.689229	41.375591
3522.493141	953950.364072	41.380596
3522.129869	953551.179890	41.385600
3522.317167	953155.016768	41.390605
3521.948258	952761.763350	41.395610
3521.910358	952374.147451	41.400615
3521.967507	951991.529760	41.405620
3521.762697	951618.586004	41.410624
3521.915233	951231.304842	41.415629
3521.839417	950860.292926	41.420634
3521.723926	950475.868165	41.425639
3521.736153	950093.019770	41.430644
3521.295239	949724.568506	41.435648
3521.497931	949347.564712	41.440653
3521.166847	948984.591567	41.445658
3521.015231	948604.912193	41.450663
3520.766802	948239.575957	41.455668
3520.499377	947889.625918	41.460672
3520.979808	947513.015671	41.465677
3520.786448	947152.474464	41.470682
3520.666105	946789.789895	41.475687
3520.838584	946429.807843	41.480692
3520.562519	946066.810753	41.485696
3520.369609	945696.114431	41.490701
3520.520183	945338.932222	41.495706
3520.427817	944972.093270	41.500711
3520.444328	944614.787255	41.505716
3520.397352	944262.830435	41.510720
3520.617850	943899.694803	41.515725
3520.116097	943544.698965	41.520730
3519.929966	943188.573014	41.525735
3520.172049	942827.370295	41.530740
3519.698892	942482.643581	41.535744
3519.758243	942115.002133	41.540749
3519.784138	941771.583177	41.545754
3519.439478	941412.869998	41.550759
3519.177013	941074.052199	41.555764
3519.135217	940731.246475	41.560768
3519.241027	940386.668592	41.565773
3519.258894	940052.147040	41.570778
3519.106620	939707.470886	41.575783
3519.317940	939366.738425	41.580788
3518.721922	939033.690644	41.585792
3519.066878	938690.782840	41.590797
3518.874086	938367.309857	41.595802
3518.765756	938019.446672	41.600807
3518.529771	937681.362904	41.605812
3518.497653	937355.595230	41.610816
3518.631659	937026.135373	41.615821
3518.323832	936688.095214	41.620826
3518.566041	936351.861072	41.625831
3518.391293	936022.293086	41.630836
3518.080483	935698.578770	41.635840
3518.142730	935374.591163	41.640845
3517.822162	935058.802000	41.645850
3517.659169	934729.726668	41.650855
3517.969614	934403.815303	41.655860
3517.744489	934082.290343	41.660864
3517.549961	933768.322252	41.665869
3517.543118	933445.762814	41.670874
3517.633771	933147.354604	41.675879
3517.966043	932825.949162	41.680884
3517.219799	932504.893833	41.685888
3517.446931	932180.394715	41.690893
3517.051479	931882.667146	41.695898
3517.050646	931570.936580	41.700903
3516.784582	931263.744025	41.705908
3516.913944	930955.700352	41.710912
3516.925800	930649.578647	41.715917
3516.833650	930348.450012	41.720922
3516.839669	930044.310995	41.725927
3516.916899	929742.063664	41.730932
3516.314760	929443.176668	41.735936
3516.689215	929139.213290	41.740941
3516.408774	928836.493140	41.745946
3516.326197	928537.853903	41.750951
3516.557545	928251.731203	41.755956
3516.324919	927955.966125	41.760960
3516.415396	927646.392055	41.765965
3516.133594	927353.580134	41.770970
3516.072325	927060.235365	41.775975
3515.670149	926771.735413	41.780980
3515.809466	926488.800594	41.785984
3516.208807	926199.080585	41.790989
3515.915350	925916.090668	41.795994
3515.643015	925622.990148	41.800999
3515.876140	925336.134304	41.806004
3515.905844	925053.622299	41.811008
3515.837645	924756.403452	41.816013
3515.775708	924472.241688	41.821018
3515.495853	924185.312675	41.826023
3515.594675	923904.267042	41.831028
3515.492802	923633.239544	41.836032
3515.289832	923348.753130	41.841037
3515.494769	923067.357803	41.846042
3515.144999	922780.172985	41.851047
3515.263811	922503.474548	41.856052
3514.917709	922231.647330	41.861056
3515.284945	921947.762372	41.866061
3515.201748	921681.442637	41.871066
3514.905500	921399.754258	41.876071
3514.830385	921121.189230	41.881076
3514.895114	920854.227147	41.886080
3514.730396	920583.345240	41.891085
3514.637147	920316.575050	41.896090
3514.708608	920040.720317	41.901095
3514.894812	919768.104123	41.906100
3514.463391	919507.604107	41.911104
3514.437762	919236.728128	41.916109
3514.125698	918978.685001	41.921114
3513.749532	918715.828205	41.926119
3514.075677	918462.178606	41.931124
3513.995818	918208.776551	41.936128
3514.151128	917948.008734	41.941133
3514.002178	917688.529883	41.946138
3513.988280	917430.267806	41.951143
3513.843028	917179.235089	41.956148
3513.534864	916932.934898	41.961152
3513.583140	916663.458796	41.966157
3513.845479	916425.128788	41.971162
3513.464340	916170.140968	41.976167
3513.653541	915924.676114	41.981172
3513.532485	915678.480996	41.986176
3513.368747	915424.096546	41.991181
3513.103759	915185.895600	41.996186
3513.064645	914936.764507	42.001191
3513.105429	914692.039169	42.006196
3512.934250	914471.801628	42.011200
3513.088845	914224.532468	42.016205
3513.002029	913987.887409	42.021210
3513.088635	913736.465549	42.026215
3513.418366	913507.437271	42.031220
3513.047612	913267.436298	42.036224
3513.148472	913017.616832	42.041229
3512.828232	912787.991228	42.046234
3513.042009	912546.128222	42.051239
3512.989696	912302.949480	42.056244
3512.530428	912079.772761	42.061248
3512.707579	911829.693996	42.066253
3512.686515	911596.018515	42.071258
3512.743900	911359.140024	42.076263
3512.631864	911133.265745	42.081268
3512.389710	910903.934083	42.086272
3512.506709	910669.521910	42.091277
3512.467608	910451.414502	42.096282
3512.224101	910216.946103	42.101287
3512.391548	909981.243323	42.106292
3512.088835	909754.476445	42.111296
3511.979489	909525.836785	42.116301
3511.873431	909311.165784	42.121306
3511.849583	909096.087269	42.126311
3511.659144	908873.025641	42.131316
3511.610804	908661.405095	42.136320
3511.594454	908442.154047	42.141325
3511.838960	908225.936892	42.146330
3511.463185	908012.513450	42.151335
3511.432435	907796.132020	42.156340
3511.406472	907597.003121	42.161344
3511.505831	907377.883779	42.166349
3511.594661	907171.777162	42.171354
3511.300650	906952.416507	42.176359
3511.345890	906740.803681	42.181364
3511.544749	906533.304959	42.186368
3511.650920	906305.172066	42.191373
3511.314976	906113.082367	42.196378
3511.225255	905905.028988	42.201383
3511.542898	905691.691484	42.206388
3511.052596	905476.356555	42.211392
3511.080743	905272.022473	42.216397
3511.318162	905069.479507	42.221402
3511.102816	904866.521370	42.226407
3510.984293	904658.329693	42.231412
3510.831333	904464.416248	42.236416
3510.964949	904263.308444	42.241421
3511.067665	904068.181209	42.246426
3511.046515	903858.496229	42.251431
3510.680496	903650.886753	42.256436
3510.306361	903462.765122	42.261440
3510.550808	903261.989048	42.266445
3510.333207	903074.214595	42.271450
3510.300384	902882.542764	42.276455
3510.616352	902685.787907	42.281460
3510.155058	902491.856830	42.286464
3510.395582	902303.884544	42.291469
3510.342663	902119.139762	42.296474
3509.974515	901935.020019	42.301479
3510.216747	901744.132725	42.306484
3510.177656	901558.691456	42.311488
3509.893474	901370.195099	42.316493
3509.802783	901186.487790	42.321498
3509.915851	901001.485777	42.326503
3510.048110	900822.364148	42.331508
3509.841495	900640.492563	42.336512
3509.786649	900446.906611	42.341517
3509.951500	900278.190513	42.346522
3509.304807	900092.704410	42.351527
3509.659654	899915.448511	42.356532
3509.712286	899743.934451	42.361536
3509.869488	899552.503914	42.366541
3509.760093	899374.921207	42.371546
3509.493874	899205.278231	42.376551
3509.634092	899024.552834	42.381556
3509.484351	898852.562085	42.386560
3509.585418	898667.775136	42.391565
3509.394995	898498.291589	42.396570
3509.349181	898330.228040	42.401575
3509.629009	898140.854479	42.406580
3509.372966	897981.605542	42.411584
3508.984719	897798.223165	42.416589
3508.934061	897633.907228	42.421594
3508.631209	897467.502675	42.426599
3508.892713	897306.217273	42.431604
3508.758300	897150.209675	42.436608
3509.046920	896977.896427	42.441613
3508.701208	896817.953183	42.446618
3508.470606	896657.406721	42.451623
3508.617793	896503.363988	42.456628
3508.551653	896347.806172	42.461632
3508.612478	896175.312803	42.466637
3508.514975	896022.843427	42.471642
3508.555637	895860.973490	42.476647
3508.419860	895710.628027	42.481652
3508.446446	895562.571224	42.486656
3508.603268	895391.971064	42.491661
3508.766712	895235.185203	42.496666
3508.393287	895080.319809	42.501671
3508.476227	894929.531045	42.506676
3508.288410	894778.976201	42.511680
3508.388817	894613.484668	42.516685
3508.515432	894464.802855	42.521690
3508.136231	894318.037080	42.526695
3507.950543	894167.852365	42.531700
3507.823966	894024.807340	42.536704
3508.231179	893863.593499	42.541709
3508.393195	893722.040051	42.546714
3508.259709	893579.661701	42.551719
3508.272610	893411.829481	42.556724
3508.149795	893273.212152	42.561728
3508.011422	893121.251823	42.566733
3508.099035	892977.758513	42.571738
3507.577982	892825.079863	42.576743
3507.873831	892682.318323	42.581748
3507.828636	892533.904543	42.586752
3507.832113	892404.527802	42.591757
3507.542790	892250.635278	42.596762
3507.321890	892118.194702	42.601767
3507.747285	891972.879915	42.606772
3507.413877	891834.165657	42.611776
3507.453419	891694.903056	42.616781
3507.342469	891568.040621	42.621786
3507.651217	891433.175913	42.626791
3507.842857	891296.393054	42.631796
3507.381658	891158.553897	42.636800
3507.598692	891008.123019	42.641805
3507.697894	890873.859984	42.646810
3507.246271	890735.235298	42.651815
3507.641666	890606.623863	42.656820
3507.166979	890478.443078	42.661824
3507.439359	890333.015196	42.666829
3507.387173	890208.918160	42.671834
3507.312930	890067.603401	42.676839
3507.525034	889925.947777	42.681844
3507.007624	889800.757726	42.686848
3507.082985	889657.860416	42.691853
3507.082287	889524.356205	42.696858
3506.490939	889403.716618	42.701863
3506.799637	889266.962855	42.706868
3506.633955	889147.892479	42.711872
3506.924586	889018.585517	42.716877
3506.886009	888907.519631	42.721882
3506.634921	888781.295954	42.726887
3506.582025	888662.196946	42.731892
3506.599194	888533.311171	42.736896
3506.849368	888415.318248	42.741901
3506.674681	888290.619421	42.746906
3506.601975	888166.578455	42.751911
3506.626158	888045.034834	42.756916
3506.962642	887927.598320	42.761920
3506.499950	887807.387916	42.766925
3506.574430	887694.247796	42.771930
3506.340485	887570.801224	42.776935
3506.926490	887445.765247	42.781940
3506.361883	887334.271814	42.786945
3506.377036	887214.647791	42.791949
3506.628530	887102.821869	42.796954
3506.456523	886989.418194	42.801959
3506.757087	886858.125439	42.806964
3506.192114	886750.782685	42.811969
3506.352894	886625.799027	42.816973
3506.374438	886511.192575	42.821978
3506.510304	886403.050338	42.826983
3506.187872	886273.202085	42.831988
3506.015022	886165.977460	42.836993
3506.268149	886052.001355	42.841997
3506.418324	885942.105719	42.847002
3506.577461	885831.044856	42.852007
3506.364789	885702.811412	42.857012
3506.304331	885605.625863	42.862017
3506.598174	885480.595559	42.867021
3506.642702	885374.288572	42.872026
3506.113722	885264.685606	42.877031
3506.637652	885142.224099	42.882036
3505.981090	885036.123233	42.887041
3506.053085	884909.761712	42.892045
3506.429259	884799.807186	42.897050
3506.048595	884692.202232	42.902055
3506.100092	884571.743012	42.907060
3505.836456	884474.668808	42.912065
3505.957542	884354.290440	42.917069
3505.741972	884254.299732	42.922074
3505.486600	884149.278522	42.927079
3506.019810	884042.479293	42.932084
3505.850706	883949.835159	42.937089
3505.698119	883832.493009	42.942093
3505.962515	883735.416295	42.947098
3505.852690	883642.466975	42.952103
3505.921513	883532.345426	42.957108
3505.796785	883425.062201	42.962113
3505.936489	883315.021708	42.967117
3506.113355	883208.459581	42.972122
3505.891153	883110.677823	42.977127
3505.730391	882994.288619	42.982132
3505.917744	882893.723867	42.987137
3506.071351	882784.833318	42.992141
3505.864027	882680.843094	42.997146
3505.839015	882584.182302	43.002151
3505.744195	882472.421061	43.007156
3505.483243	882376.183136	43.012161
3505.549191	882265.844390	43.017165
3505.686107	882169.828104	43.022170
3505.228622	882075.070583	43.027175
3505.487090	881970.312867	43.032180
3505.519588	881889.420819	43.037185
3505.632155	881783.908829	43.042189
3505.552716	881691.310862	43.047194
3505.657960	881589.380912	43.052199
3505.774461	881481.828421	43.057204
3505.294020	881381.347623	43.062209
3505.455502	881287.637889	43.067213
3505.693622	881194.107793	43.072218
3505.355791	881089.238757	43.077223
3505.504171	880996.107816	43.082228
3505.124444	880908.003653	43.087233
3505.169664	880817.309042	43.092237
3505.195813	880716.636459	43.097242
3505.029209	880621.516748	43.102247
3505.150805	880530.417539	43.107252
3505.216613	880447.077702	43.112257
3505.227613	880350.083315	43.117261
3505.149481	880251.260942	43.122266
3504.629885	880171.889559	43.127271
3505.089827	880088.867288	43.132276
3505.089028	880002.237465	43.137281
3505.005020	879904.476133	43.142285
3504.993657	879817.845325	43.147290
3505.097519	879733.035480	43.152295
3505.130331	879645.135054	43.157300
3504.922444	879558.338972	43.162305
3504.691490	879466.312206	43.167309
3505.063617	879378.158053	43.172314
3504.861171	879291.938606	43.177319
3505.063464	879203.034492	43.182324
3504.938087	879116.993608	43.187329
3505.015398	879036.151656	43.192333
3504.706156	878950.041698	43.197338
3504.825694	878866.961306	43.202343
3505.213982	878779.473953	43.207348
3504.847610	878700.542006	43.212353
3504.953006	878608.834072	43.217357
3505.029701	878516.838655	43.222362
3504.693754	878434.602607	43.227367
3505.073305	878351.859808	43.232372
3504.536794	878277.215099	43.237377
3504.771254	878183.346786	43.242381
3505.038974	878102.460618	43.247386
3504.913466	878014.658803	43.252391
3505.059275	877928.361961	43.257396
3504.998067	877840.159201	43.262401
3505.087484	877747.180270	43.267405
3504.897451	877660.450133	43.272410
3504.636841	877576.444731	43.277415
3504.797967	877493.725858	43.282420
3504.602798	877418.044562	43.287425
3504.378479	877327.728207	43.292429
3504.298397	877255.709826	43.297434
3504.229823	877191.735409	43.302439
3504.374494	877108.141296	43.307444
3504.138431	877039.539219	43.312449
3504.446623	876954.170861	43.317453
3504.633992	876882.976433	43.322458
3504.381803	876796.340763	43.327463
3504.557302	876729.412462	43.332468
3504.417590	876652.354806	43.337473
3504.488903	876577.006632	43.342477
3504.527314	876501.856837	43.347482
3504.379396	876422.858334	43.352487
3504.345058	876351.112249	43.357492
3504.476477	876283.022599	43.362497
3504.649076	876198.926184	43.367501
3504.779164	876109.987257	43.372506
3504.712592	876041.345643	43.377511
3504.475337	875949.070949	43.382516
3504.315822	875882.091269	43.387521
3504.277826	875801.514818	43.392525
3504.594398	875728.927588	43.397530
3504.206310	875657.425301	43.402535
3504.479013	875573.885341	43.407540
3504.611466	875507.823068	43.412545
3504.390635	875416.798045	43.417549
3504.213979	875349.330261	43.422554
3504.263090	875276.587588	43.427559
3504.170718	875199.018265	43.432564
3504.541271	875127.287593	43.437569
3504.201598	875046.459605	43.442573
3504.393348	874976.793230	43.447578
3504.188523	874901.372201	43.452583
3504.446926	874825.776903	43.457588
3504.298791	874759.849496	43.462593
3504.201690	874680.625351	43.467597
3504.438757	874622.004169	43.472602
3504.317517	874547.340784	43.477607
3504.587857	874463.785550	43.482612
3504.254981	874398.466516	43.487617
3504.306322	874313.199339	43.492621
3504.359999	874247.911954	43.497626
3504.169651	874172.770250	43.502631
3503.920132	874093.854362	43.507636
3503.924001	874034.780798	43.512641
3504.154628	873964.029107	43.517645
3503.881323	873900.246789	43.522650
3504.273488	873828.108827	43.527655
3504.093008	873757.616415	43.532660
3503.941054	873693.229846	43.537665
3504.095789	873613.658929	43.542669
3503.623766	873546.510288	43.547674
3503.852292	873489.722485	43.552679
3503.849513	873419.487805	43.557684
3503.999273	873356.600043	43.562689
3503.866797	873289.489561	43.567693
3503.837810	873224.010503	43.572698
3503.866815	873150.371925	43.577703
3503.838894	873082.950838	43.582708
3503.825328	873024.161136	43.587713
3503.315819	872960.892718	43.592717
3503.674645	872900.391131	43.597722
3503.542430	872852.485392	43.602727
3503.789062	872781.328898	43.607732
3503.446089	872722.493462	43.612737
3503.626940	872661.824728	43.617741
3503.538502	872591.691398	43.622746
3503.332729	872538.944049	43.627751
3503.541029	872468.372276	43.632756
3503.406883	872421.433641	43.637761
3503.409163	872358.559619	43.642765
3503.312192	872302.008156	43.647770
3503.407059	872251.731472	43.652775
3503.643081	872186.197322	43.657780
3503.615763	872140.403236	43.662785
3503.318557	872085.726302	43.667789
3503.620534	872026.098488	43.672794
3503.448204	871962.860922	43.677799
3503.646705	871899.949728	43.682804
3503.775681	871845.685550	43.687809
3503.475607	871787.513046	43.692813
3503.821959	871717.491854	43.697818
3503.363490	871669.339222	43.702823
3503.648511	871607.963316	43.707828
3503.456869	871552.099607	43.712833
3503.481546	871490.571304	43.717837
3503.562256	871427.771576	43.722842
3503.419372	871375.779898	43.727847
3503.357983	871315.622582	43.732852
3503.199677	871259.556547	43.737857
3503.475957	871206.523876	43.742861
3503.391006	871153.647297	43.747866
3503.214338	871108.743313	43.752871
3503.149687	871047.322201	43.757876
3503.379090	870994.101268	43.762881
3503.267731	870945.303291	43.767885
3503.542949	870884.406813	43.772890
3503.166988	870837.010270	43.777895
3502.983308	870784.437840	43.782900
3502.984894	870732.416749	43.787905
3503.228239	870680.937705	43.792909
3503.224864	870621.734385	43.797914
3502.870974	870572.585093	43.802919
3502.928492	870526.958748	43.807924
3503.410987	870479.320870	43.812929
3503.187686	870424.713572	43.817933
3503.310520	870362.769231	43.822938
3503.308330	870320.062951	43.827943
3503.526425	870264.702042	43.832948
3503.316906	870220.573281	43.837953
3503.113761	870171.687039	43.842957
3503.320136	870110.891084	43.847962
3502.968900	870075.035062	43.852967
3502.986308	870011.454345	43.857972
3502.804764	869968.386837	43.862977
3503.099425	869919.513582	43.867981
3503.232474	869879.985103	43.872986
3503.330611	869826.387126	43.877991
3503.104779	869769.735808	43.882996
3503.083550	869716.350652	43.888001
3503.159726	869671.200055	43.893005
3503.326127	869613.803137	43.898010
3503.102457	869567.924583	43.903015
3502.968040	869516.497754	43.908020
3503.104587	869477.548485	43.913025
3502.962827	869424.180579	43.918029
3503.090886	869372.612194	43.923034
3503.064745	869336.795255	43.928039
3503.040571	869287.872299	43.933044
3503.228730	869233.768795	43.938049
3503.034926	869181.183926	43.943053
3503.284673	869131.437926	43.948058
3503.037787	869082.841227	43.953063
3502.938730	869034.025615	43.958068
3503.227982	868984.854381	43.963073
3503.268905	868939.218660	43.968077
3503.066913	868876.827036	43.973082
3502.997089	868830.432057	43.978087
3503.073415	868784.400984	43.983092
3503.216795	868748.164253	43.988097
3503.010602	868679.072290	43.993101
3503.098000	868627.698369	43.998106
3502.894797	868588.702210	44.003111
3502.803710	868545.124107	44.008116
3502.613836	868506.513576	44.013121
3503.001437	868464.797832	44.018125
3502.903958	868419.472230	44.023130
3502.655813	868372.132164	44.028135
3503.163361	868315.928814	44.033140
3503.234738	868281.642997	44.038145
3502.754976	868227.543363	44.043149
3503.174711	868179.606267	44.048154
3502.932040	868138.671768	44.053159
3502.966433	868085.942592	44.058164
3502.789475	868047.035682	44.063169
3503.063707	867995.140074	44.068173
3502.979856	867953.012957	44.073178
3502.966802	867901.940670	44.078183
3502.892093	867849.227390	44.083188
3503.110973	867814.234895	44.088193
3502.849306	867769.416940	44.093197
3503.044500	867711.511558	44.098202
3502.835736	867657.750547	44.103207
3502.802370	867620.467983	44.108212
3502.745852	867576.780047	44.113217
3502.898571	867529.658604	44.118221
3502.906523	867485.959386	44.123226
3502.645319	867460.366183	44.128231
3502.944805	867401.566666	44.133236
3502.758415	867364.210615	44.138241
3502.630027	867319.658670	44.143245
3502.834088	867283.597323	44.148250
3502.617361	867242.555326	44.153255
3502.742034	867192.522536	44.158260
3502.800646	867150.463430	44.163265
3502.840704	867102.871643	44.168269
3502.513925	867072.431932	44.173274
3502.423942	867035.349293	44.178279
3502.977725	866997.286329	44.183284
3502.874461	866949.619827	44.188289
3502.682625	866906.143542	44.193293
3502.915365	866855.701682	44.198298
3502.788244	866817.069942	44.203303
3502.883974	866769.077871	44.208308
3502.807750	866735.972976	44.213313
3502.643730	866696.083991	44.218317
3502.621552	866643.157238	44.223322
3502.571087	866612.184068	44.228327
3502.994779	866561.514042	44.233332
3502.949192	866524.129572	44.238337
3502.497783	866485.549131	44.243341
3502.513525	866445.725993	44.248346
3502.606127	866404.433062	44.253351
3502.708641	866365.760591	44.258356
3502.336301	866330.856879	44.263361
3502.480541	866289.069022	44.268365
3502.306168	866244.613816	44.273370
3502.547871	866218.155447	44.278375
3502.430969	866175.147169	44.283380
3502.480203	866143.378137	44.288385
3501.934473	866109.861509	44.293389
3502.294604	866070.561925	44.298394
3502.252697	866031.522584	44.303399
3502.595118	866005.338079	44.308404
3502.573740	865970.471584	44.313409
3502.151105	865940.236194	44.318413
3502.276669	865897.671647	44.323418
3502.302247	865883.777504	44.328423
3502.604151	865842.543373	44.333428
3502.613049	865804.271257	44.338433
3502.408451	865767.393958	44.343437
3502.546113	865725.117604	44.348442
3502.343490	865694.067647	44.353447
3502.462120	865656.456465	44.358452
3502.613801	865633.118728	44.363457
3502.360929	865596.539748	44.368461
3502.730183	865549.949964	44.373466
3502.467415	865520.851786	44.378471
3502.653353	865481.868486	44.383476
3502.623954	865439.229097	44.388481
3502.457748	865407.880245	44.393485
3502.410892	865362.620398	44.398490
3502.324995	865329.800792	44.403495
3502.394804	865287.435410	44.408500
3501.947073	865257.006437	44.413505
3502.044215	865239.213304	44.418509
3502.459325	865198.927560	44.423514
3502.624803	865167.425668	44.428519
3502.543536	865122.363978	44.433524
3502.281282	865092.486486	44.438529
3502.052001	865063.283435	44.443533
3502.614763	865025.983737	44.448538
3502.272526	865001.656324	44.453543
3502.641915	864963.028039	44.458548
3502.498657	864917.489296	44.463553
3502.326788	864887.207302	44.468557
3502.398108	864848.433096	44.473562
3502.387160	864815.404046	44.478567
3502.334329	864788.016441	44.483572
3502.195806	864755.882437	44.488577
3502.151042	864721.498331	44.493581
3502.378063	864698.338875	44.498586
3502.353316	864665.311277	44.503591
3502.377664	864617.022387	44.508596
3502.251193	864588.188711	44.513601
3502.029130	864569.280353	44.518605
3502.295198	864534.649665	44.523610
3501.878735	864507.806472	44.528615
3501.738072	864485.775485	44.533620
3501.973951	864439.393428	44.538625
3502.254938	864423.316413	44.543629
3502.287617	864387.557460	44.548634
3502.202197	864369.694690	44.553639
3502.297517	864330.816053	44.558644
3502.654347	864301.415594	44.563649
3502.245333	864268.837773	44.568653
3502.475281	864221.969235	44.573658
3502.373884	864200.222215	44.578663
3502.099024	864151.881746	44.583668
3502.277426	864132.808882	44.588673
3502.278180	864090.543648	44.593677
3502.370781	864062.642988	44.598682
3501.997916	864031.806848	44.603687
3502.150489	863997.969090	44.608692
3502.384441	863972.473803	44.613697
3502.467999	863942.922300	44.618701
3502.480222	863900.265193	44.623706
3502.266629	863880.284471	44.628711
3502.466376	863834.098061	44.633716
3502.475859	863810.290891	44.638721
3502.503419	863772.488659	44.643725
3502.535447	863739.349484	44.648730
3502.357375	863697.888310	44.653735
3502.594416	863657.913155	44.658740
3502.958513	863632.200658	44.663745
3502.463824	863589.624878	44.668749
3502.426583	863553.969691	44.673754
3502.220238	863526.601665	44.678759
3502.375221	863476.047220	44.683764
3502.397155	863461.467909	44.688769
3502.329141	863421.152766	44.693773
3502.384542	863380.039638	44.698778
3502.246731	863358.587111	44.703783
3502.335730	863310.665838	44.708788
3502.654233	863286.417000	44.713793
3502.336070	863247.502358	44.718797
3502.589498	863211.117037	44.723802
3502.327366	863186.283231	44.728807
3502.631903	863131.911409	44.733812
3502.488468	863099.380704	44.738817
3502.648013	863070.006781	44.743821
3502.681755	863026.756910	44.748826
3502.323618	862987.652826	44.753831
3502.529926	862949.816013	44.758836
3502.654672	862928.415885	44.763841
3502.637696	862891.781660	44.768845
3502.611281	862852.136144	44.773850
3502.383296	862821.950235	44.778855
3502.229125	862785.435153	44.783860
3502.240377	862749.475695	44.788865
3502.177572	862718.581775	44.793869
3502.045955	862678.272170	44.798874
3502.238522	862666.481177	44.803879
3502.388822	862622.043003	44.808884
3502.284017	862595.334335	44.813889
3502.017804	862568.846514	44.818893
3502.289286	862533.523205	44.823898
3502.364740	862507.756318	44.828903
3502.337899	862460.916475	44.833908
3502.514739	862435.715705	44.838913
3502.118465	862396.905656	44.843917
3502.008659	862374.181576	44.848922
3502.197408	862342.369593	44.853927
3502.295337	862309.989266	44.858932
3502.548528	862285.066863	44.863937
3502.339303	862246.710987	44.868941
3502.606135	862224.313058	44.873946
3502.025167	862185.726469	44.878951
3501.986889	862160.462807	44.883956
3502.262371	862122.998217	44.888961
3502.024649	862097.767154	44.893965
3502.332158	862061.754813	44.898970
3502.087004	862041.578833	44.903975
3502.338678	862011.115472	44.908980
3502.299404	861985.073686	44.913985
3502.389555	861961.537554	44.918989
3502.548222	861912.913399	44.923994
3502.175101	861888.675739	44.928999
3502.285504	861842.294498	44.934004
3502.294846	861831.115261	44.939009
3502.159032	861791.286446	44.944013
3502.329163	861761.224062	44.949018
3502.151770	861731.801984	44.954023
3502.289036	861700.578322	44.959028
3501.954655	861667.293798	44.964033
3502.119027	861640.730983	44.969037
3502.618672	861596.810962	44.974042
3502.141429	861580.073738	44.979047
3502.298690	861546.318744	44.984052
3502.038746	861510.007820	44.989057
3502.060543	861485.509078	44.994061
3502.431807	861448.607776	44.999066
3501.857953	861420.804773	45.004071
3502.135566	861390.236827	45.009076
3502.361134	861360.454945	45.014081
3502.097685	861337.946711	45.019085
3502.143726	861302.847811	45.024090
3501.969347	861276.047597	45.029095
3502.242948	861249.270664	45.034100
3502.015430	861212.174961	45.039105
3502.074163	861203.902664	45.044109
3502.286173	861162.651515	45.049114
3502.057375	861140.234048	45.054119
3502.054772	861100.767597	45.059124
3502.235217	861083.823435	45.064129
3501.904924	861052.187432	45.069133
3502.246459	861020.148945	45.074138
3502.054927	860999.085768	45.079143
3502.252065	860966.973581	45.084148
3502.398720	860929.036811	45.089153
3502.231603	860909.524697	45.094157
3501.874803	860868.073631	45.099162
3501.759508	860850.399839	45.104167
3502.034340	860823.718048	45.109172
3502.444660	860796.236104	45.114177
3501.964259	860773.178236	45.119181
3502.134978	860739.610983	45.124186
3501.924989	860714.175173	45.129191
3501.886571	860678.017214	45.134196
3501.962223	860668.283159	45.139201
3502.063507	860637.351624	45.144205
3502.066451	860610.713697	45.149210
3501.747726	860580.823247	45.154215
3501.995453	860557.644598	45.159220
3502.060396	860520.690931	45.164225
3501.903040	860511.869984	45.169229
3502.013080	860485.311083	45.174234
3501.962671	860464.708902	45.179239
3502.172404	860432.786266	45.184244
3502.068866	860403.831695	45.189249
3501.866316	860390.643090	45.194253
3501.885083	860346.890516	45.199258
3502.198932	860334.588925	45.204263
3502.094838	860294.064531	45.209268
3501.987499	860276.096094	45.214273
3501.900544	860243.249121	45.219277
3502.118941	860222.699057	45.224282
3502.017529	860196.076512	45.229287
3501.854635	860175.394661	45.234292
3502.128086	860164.849421	45.239297
3501.769783	860136.130000	45.244301
3502.098469	860099.713679	45.249306
3502.071267	860076.286822	45.254311
3501.804423	860042.593373	45.259316
3501.848974	860018.571115	45.264321
3501.666608	859993.419423	45.269325
3502.064882	859975.366797	45.274330
3501.684381	859956.761832	45.279335
3501.595003	859946.859361	45.284340
3501.887742	859922.115237	45.289345
3501.745921	859886.164074	45.294349
3502.102708	859863.353738	45.299354
3501.838017	859841.423545	45.304359
3501.875957	859814.679146	45.309364
3502.198603	859790.026791	45.314369
3501.946122	859773.442010	45.319373
3501.880618	859735.532773	45.324378
3502.106556	859714.007444	45.329383
3502.322227	859691.705875	45.334388
3502.330583	859664.382300	45.339393
3502.073463	859634.574288	45.344397
3502.247990	859594.582738	45.349402
3501.970464	859563.027535	45.354407
3501.740269	859531.950543	45.359412
3502.108975	859520.805094	45.364417
3501.782816	859486.826641	45.369421
3502.211082	859464.489218	45.374426
3501.860588	859444.516444	45.379431
3501.711453	859411.480765	45.384436
3502.183180	859387.969065	45.389441
3501.644866	859367.735274	45.394445
3501.991215	859340.160088	45.399450
3502.160528	859313.294611	45.404455
3502.069310	859289.194615	45.409460
3502.264438	859263.394288	45.414465
3502.009516	859254.101399	45.419469
3502.103794	859209.939279	45.424474
3501.994962	859203.053233	45.429479
3501.912314	859168.254969	45.434484
3501.995470	859141.597413	45.439489
3502.101193	859117.658774	45.444493
3502.154042	859084.004599	45.449498
3501.924717	859058.467822	45.454503
3501.844744	859023.862779	45.459508
3501.899274	859019.672402	45.464513
3501.972751	858993.307522	45.469517
3501.910792	858969.298686	45.474522
3501.633816	858939.198818	45.479527
3501.683517	858913.907196	45.484532
3501.867259	858900.457231	45.489537
3501.789952	858876.839539	45.494541
3501.978951	858849.871539	45.499546
3501.970269	858829.743190	45.504551
3501.683224	858799.547046	45.509556
3501.972334	858781.606136	45.514561
3501.877472	858748.655177	45.519565
3501.928783	858721.903792	45.524570
3501.260913	858714.720310	45.529575
3501.514877	858692.214295	45.534580
3501.723763	858666.798177	45.539585
3501.524879	858657.203399	45.544589
3501.799778	858638.583674	45.549594
3501.882482	858616.202845	45.554599
3501.834001	858600.845501	45.559604
3502.129444	858572.983501	45.564609
3501.910275	858551.332919	45.569613
3502.064981	858517.853347	45.574618
3501.935570	858508.830394	45.579623
3501.978945	858481.690264	45.584628
3501.893175	858442.803833	45.589633
3501.821867	858428.714091	45.594637
3501.860645	858400.699091	45.599642
3501.446162	858384.915244	45.604647
3501.685074	858370.190741	45.609652
3501.807632	858353.734815	45.614657
3501.807268	858332.436420	45.619661
3502.213977	858306.499948	45.624666
3502.026580	858283.092609	45.629671
3501.973630	858262.094397	45.634676
3502.225730	858228.694454	45.639681
3501.879522	858198.310576	45.644685
3501.970364	858168.827101	45.649690
3501.915159	858153.858769	45.654695
3502.081150	858130.392622	45.659700
3501.794559	858104.083237	45.664705
3501.945814	858078.771433	45.669709
3501.904555	858045.613341	45.674714
3501.638435	858025.524761	45.679719
3501.465357	858002.308505	45.684724
3502.058959	857989.469827	45.689729
3502.280851	857973.093772	45.694733
3502.149186	857940.047263	45.699738
3502.169922	857908.337110	45.704743
3501.948805	857884.739282	45.709748
3502.092230	857858.552514	45.714753
3502.055631	857838.911811	45.719757
3502.077371	857805.352993	45.724762
3502.097352	857777.727289	45.729767
3501.701272	857746.474021	45.734772
3501.757341	857713.492621	45.739777
3501.387098	857700.909406	45.744781
3501.853989	857688.966353	45.749786
3501.643465	857666.630367	45.754791
3501.837598	857648.215472	45.759796
3501.903820	857636.435594	45.764801
3501.612321	857607.109675	45.769805
3501.780630	857581.112153	45.774810
3501.546404	857544.384316	45.779815
3501.745634	857466.635444	45.784820
3502.285312	857331.343519	45.789825
3501.447197	857134.605113	45.794829
3501.672816	856883.599610	45.799834
3501.332649	856581.118172	45.804839
3501.125959	856216.530981	45.809844
3501.527193	855779.143797	45.814849
3500.941580	855304.037944	45.819853
3501.179196	854751.982488	45.824858
3501.038062	854147.290240	45.829863
3500.821506	853475.588263	45.834868
3500.646410	852747.932526	45.839873
3500.132662	851956.869782	45.844877
3499.908240	851089.030425	45.849882
3499.560430	850164.803444	45.854887
3499.320739	849183.249248	45.859892
3499.500440	848125.781144	45.864897
3498.992099	847014.952753	45.869901
3498.688795	845813.947814	45.874906
3498.461898	844561.529339	45.879911
3497.836569	843223.624079	45.884916
3497.532280	841820.001081	45.889921
3497.049395	840357.429785	45.894925
3496.835103	838813.553637	45.899930
3496.040149	837211.435407	45.904935
3495.457687	835522.546816	45.909940
3495.089227	833761.905304	45.914945
3494.331298	831951.234343	45.919949
3494.155354	830057.998187	45.924954
3493.399395	828084.028446	45.929959
3492.598894	826047.592047	45.934964
3492.587850	823940.820157	45.939969
3491.801040	821776.573240	45.944973
3491.165100	819504.938760	45.949978
3490.539880	817198.804695	45.954983
3489.655413	814795.957839	45.959988
3489.323544	812325.305964	45.964993
3488.051560	809792.855884	45.969997
3487.345306	807189.031784	45.975002
3486.745399	804508.047517	45.980007
3485.939331	801769.147923	45.985012
3485.340369	798951.297756	45.990017
3483.834362	796076.192451	45.995021
3483.297563	793113.647879	46.000026
3482.334277	790101.478114	46.005031
3481.169730	787016.832354	46.010036
3480.649865	783858.994621	46.015041
3479.283758	780643.966326	46.020045
3478.343850	777348.485375	46.025050
3477.395195	773999.068311	46.030055
3476.163943	770580.622576	46.035060
3475.322068	767079.695074	46.040065
3474.168069	763524.456904	46.045069
3473.199318	759903.464794	46.050074
3471.672219	756208.814643	46.055079
3470.495830	752456.957692	46.060084
3469.562614	748631.242864	46.065089
3468.265856	744749.524362	46.070093
3467.065550	740786.090748	46.075098
3465.583222	736773.115185	46.080103
3464.273630	732695.070512	46.085108
3463.360745	728547.532413	46.090113
3461.752115	724323.459907	46.095117
3460.352612	720038.922543	46.100122
3458.960763	715695.918058	46.105127
3457.335514	711285.932264	46.110132
3456.584325	706808.455757	46.115137
3454.848741	702277.381014	46.120141
3453.539374	697666.666525	46.125146
3451.937019	693008.468014	46.130151
3450.410509	688272.072592	46.135156
3448.866195	683482.201253	46.140161
3447.126252	678618.803328	46.145165
3445.694792	673700.056867	46.150170
3443.596175	668710.459655	46.155175
3441.811613	663668.835693	46.160180
3440.422595	658559.699594	46.165185
3438.358101	653396.647226	46.170189
3436.817078	648166.091470	46.175194
3435.136590	642884.678421	46.180199
3433.003016	637531.309420	46.185204
3431.624429	632117.880506	46.190209
3428.984406	626658.198222	46.195213
3427.282309	621137.944384	46.200218
3425.341946	615567.494764	46.205223
3423.521520	609940.191430	46.210228
3421.815678	604239.990165	46.215233
3419.364874	598493.635543	46.220237
3417.513294	592686.221148	46.225242
3415.287484	586834.406328	46.230247
3413.496420	580920.800544	46.235252
3411.227098	574939.735811	46.240257
3408.666211	568926.122688	46.245261
3406.512057	562841.941626	46.250266
3404.372709	556711.803525	46.255271
3401.957379	550536.964216	46.260276
3399.990236	544311.860510	46.265281
3397.227704	538045.673605	46.270285
3394.740365	531716.082225	46.275290
3392.515717	525327.970253	46.280295
3389.659304	518888.752237	46.285300
3387.393331	512423.043638	46.290305
3384.466858	505910.715961	46.295309
3381.917767	499348.376801	46.300314
3379.268360	492746.996418	46.305319
3376.334753	486112.302842	46.310324
3374.338693	479418.361096	46.315329
3371.473927	472691.210301	46.320333
3368.841962	465919.817503	46.325338
3365.856675	459102.234034	46.330343
3363.081459	452248.439312	46.335348
3360.440768	445339.218716	46.340353
3357.266772	438425.801576	46.345357
3354.365749	431440.840931	46.350362
3351.628130	424440.470586	46.355367
3348.286310	417401.328796	46.360372
3345.617879	410325.342376	46.365377
3342.230756	403230.302444	46.370381
3338.947870	396088.299512	46.375386
3335.833948	388925.734506	46.380391
3332.457461	381741.916754	46.385396
3329.157982	374512.306493	46.390401
3325.656995	367264.302102	46.395405
3322.547186	359988.452413	46.400410
3318.946982	352701.366121	46.405415
3315.543862	345383.198148	46.410420
3311.946967	338042.161629	46.415425
3308.590790	330703.596809	46.420429
3305.162377	323323.030699	46.425434
3301.319348	315940.240934	46.430439
3297.912121	308538.101375	46.435444
3294.405969	301113.585695	46.440449
3290.675105	293679.796074	46.445453
3286.924757	286221.874277	46.450458
3283.044947	278765.606482	46.455463
3278.932389	271295.244903	46.460468
3275.422134	263811.694823	46.465473
3271.175392	256327.197890	46.470477
3267.491023	248845.182475	46.475482
3263.663808	241345.416821	46.480487
3259.522579	233853.347171	46.485492
3255.639238	226325.715985	46.490497
3251.455430	218764.634949	46.495501
3246.821064	211250.444562	46.500506
3242.972647	203758.529373	46.505511
3238.923800	196265.894482	46.510516
3234.759628	188777.732641	46.515521
3230.267208	181302.273474	46.520525
3225.866351	173834.736056	46.525530
3221.469717	166367.003287	46.530535
3216.737454	158912.842992	46.535540
3212.525409	151475.451864	46.540545
3207.366451	144068.678790	46.545549
3202.718426	136675.803117	46.550554
3197.870061	129299.714834	46.555559
3192.910478	121951.668135	46.560564
3188.070377	114637.076611	46.565569
3183.088677	107349.719139	46.570573
3177.995712	100087.742700	46.575578
3172.649261	92858.962184	46.580583
3166.857603	85690.455829	46.585588
3161.499230	78546.083277	46.590593
3155.741023	71458.828434	46.595597
3149.858286	64416.056548	46.600602
3143.712509	57444.406492	46.605607
3136.603302	50529.447311	46.610612
3129.626020	43706.025136	46.615617
3119.947699	37020.351192	46.620621
3102.487544	30660.485762	46.625626
3076.834017	24722.836837	46.630631
3047.211436	19196.803981	46.635636
3014.307834	14222.143485	46.640641
2979.968012	9835.625759	46.645645
2947.666852	6026.157849	46.650650
2917.052024	2846.595343	46.655655
2876.355516	617.525568	46.660660
2793.102631	324.194294	46.665665
2741.570729	336.850255	46.670669
2733.579300	330.206513	46.675674
2754.007277	313.662466	46.680679
2784.394289	314.919497	46.685684
2812.462790	299.947315	46.690689
2830.506340	308.037780	46.695693
2838.209405	305.121488	46.700698
2837.992022	297.897151	46.705703
2833.003001	309.122635	46.710708
2827.862352	308.456397	46.715713
2822.840622	298.229020	46.720717
2819.389474	290.829758	46.725722
2816.601792	292.915834	46.730727
2813.799296	299.007255	46.735732
2811.715070	299.325908	46.740737
2809.056254	294.904863	46.745741
2806.496514	291.347227	46.750746
2803.990494	283.529577	46.755751
2801.058436	296.989838	46.760756
2798.110816	278.599605	46.765761
2794.709942	291.281933	46.770765
2791.878261	293.396199	46.775770
2788.705188	288.224073	46.780775
2785.478286	277.877436	46.785780
2782.875704	278.049947	46.790785
2779.303473	278.988683	46.795789
2775.863185	276.444265	46.800794
2772.825106	279.366178	46.805799
2769.439414	287.408465	46.810804
2766.462135	272.186559	46.815809
2763.136847	275.681585	46.820813
2760.092367	276.601536	46.825818
2756.784463	283.126851	46.830823
2753.454814	278.882047	46.835828
2749.887439	271.022878	46.840833
2746.551717	278.269928	46.845837
2743.081392	278.814161	46.850842
2739.748709	278.554209	46.855847
2736.179124	280.759081	46.860852
2733.134738	273.426178	46.865857
2730.210441	273.037672	46.870861
2726.742281	259.233208	46.875866
2723.343327	266.383346	46.880871
2719.591174	273.158406	46.885876
2716.348942	270.293627	46.890881
2713.036873	268.702574	46.895885
2709.580950	268.785435	46.900890
2705.998331	261.586759	46.905895
2702.287970	264.676477	46.910900
2699.726197	256.958879	46.915905
2696.473567	256.816782	46.920909
2692.493622	259.291869	46.925914
2688.689331	258.322378	46.930919
2685.455442	264.128635	46.935924
2682.570806	250.002168	46.940929
2678.854290	261.973302	46.945933
2675.336280	258.465731	46.950938
2671.863404	249.916921	46.955943
2667.899560	257.558540	46.960948
2665.273779	248.279899	46.965953
2662.117100	260.052094	46.970957
2658.167688	256.025673	46.975962
2654.443530	251.513726	46.980967
2651.324945	257.807746	46.985972
2647.710489	254.781839	46.990977
2644.051663	249.771290	46.995981
2640.916537	251.874533	47.000986
2637.883900	245.425835	47.005991
2633.990813	248.509836	47.010996
2630.890995	244.224834	47.016001
2627.497306	245.495740	47.021005
2623.870704	251.345128	47.026010
2620.127090	238.257586	47.031015
2616.426827	251.602723	47.036020
2613.488205	235.832689	47.041025
2610.064791	243.704455	47.046029
2606.023726	237.364579	47.051034
2602.647308	239.563314	47.056039
2599.382369	246.725344	47.061044
2596.473858	241.576802	47.066049
2592.873828	242.023348	47.071053
2589.023930	237.473400	47.076058
2585.689581	235.798495	47.081063
2581.938985	237.269629	47.086068
2578.829872	228.743360	47.091073
2575.095071	236.150288	47.096077
2571.262288	242.928087	47.101082
2568.098583	236.505807	47.106087
2564.835684	239.529664	47.111092
2561.788526	232.776357	47.116097
2557.879603	234.339945	47.121101
2554.291033	239.195602	47.126106
2550.636849	227.044163	47.131111
2547.114161	234.546348	47.136116
2543.717460	232.279082	47.141121
2540.635325	237.874079	47.146125
2537.096768	230.809181	47.151130
2533.675312	231.642688	47.156135
2530.043979	232.304022	47.161140
2526.584832	230.319801	47.166145
2523.033587	231.048832	47.171149
2519.546605	234.973660	47.176154
2516.211025	225.349707	47.181159
2512.388951	232.288384	47.186164
2508.888751	235.230668	47.191169
2505.421506	232.491191	47.196173
2502.202633	232.500339	47.201178
2498.916546	225.230209	47.206183
2495.459030	233.059319	47.211188
2491.465961	224.858791	47.216193
2487.959665	229.038238	47.221197
2484.761719	236.266828	47.226202
2481.600219	229.830237	47.231207
2477.719168	230.794698	47.236212
2474.306819	221.320209	47.241217
2470.676711	228.089287	47.246221
2467.117499	224.661499	47.251226
2463.499042	218.846392	47.256231
2460.147498	226.650728	47.261236
2457.218108	229.816745	47.266241
2453.438723	230.411598	47.271245
2449.810465	221.621426	47.276250
2446.592883	223.540264	47.281255
2443.033016	231.431096	47.286260
2439.734680	221.686995	47.291265
2436.098482	231.239411	47.296269
2431.867640	225.404637	47.301274
2428.743529	220.590966	47.306279
2425.106424	221.636762	47.311284
2421.994277	223.239239	47.316289
2418.472021	223.594532	47.321293
2414.977594	227.228986	47.326298
2411.680543	221.870597	47.331303
2407.811095	233.425669	47.336308
2404.406674	220.984879	47.341313
2400.727543	233.140031	47.346317
2397.500055	224.373930	47.351322
2393.994492	218.752977	47.356327
2390.342099	229.484839	47.361332
2387.282427	218.192909	47.366337
2383.392051	219.388292	47.371341
2379.842377	225.867282	47.376346
2376.733218	221.566237	47.381351
2373.084213	229.291458	47.386356
2370.116425	215.616285	47.391361
2366.140416	219.272053	47.396365
2362.347527	225.368302	47.401370
2358.909566	210.435154	47.406375
2355.488809	222.955577	47.411380
2351.938639	217.383462	47.416385
2348.397584	219.311556	47.421389
2345.281170	217.160772	47.426394
2341.631660	224.308676	47.431399
2337.776070	221.174813	47.436404
2334.783114	209.412112	47.441409
2331.298285	217.694380	47.446413
2327.599573	224.449814	47.451418
2324.247333	214.469608	47.456423
2320.620919	217.430484	47.461428
2316.964724	215.766471	47.466433
2313.685233	217.810662	47.471437
2309.988903	211.852637	47.476442
2306.747247	209.278935	47.481447
2303.098745	220.241880	47.486452
2299.485791	219.128821	47.491457
2296.216879	213.376126	47.496461
2292.894535	219.722917	47.501466
2289.377459	222.045326	47.506471
2285.409500	213.666591	47.511476
2282.024594	213.785388	47.516481
2278.648071	210.278448	47.521485
2275.291100	215.916198	47.526490
2272.167232	203.922169	47.531495
2268.177376	218.350941	47.536500
2264.465660	213.684127	47.541505
2260.973407	215.613696	47.546509
2257.393728	218.066051	47.551514
2254.325322	209.181645	47.556519
2250.410194	217.065730	47.561524
2247.256133	199.915467	47.566529
2243.523814	215.123458	47.571533
2240.232160	217.886247	47.576538
2236.928652	208.482986	47.581543
2233.546433	205.982272	47.586548
2229.451752	213.880622	47.591553
2226.203334	213.433447	47.596557
2222.452612	218.169668	47.601562
2219.514704	201.836643	47.606567
2215.615282	205.793650	47.611572
2211.826456	205.776912	47.616577
2208.687985	202.637439	47.621581
2205.051281	208.443570	47.626586
2201.661157	200.232566	47.631591
2198.152954	205.137742	47.636596
2194.745747	205.610758	47.641601
2191.096597	209.214861	47.646605
2187.792435	203.455637	47.651610
2184.645891	199.776407	47.656615
2181.159549	207.545732	47.661620
2177.505249	197.033770	47.666625
2173.696344	205.727023	47.671629
2170.052541	199.062651	47.676634
2166.587480	202.253929	47.681639
2162.988571	207.432029	47.686644
2159.688224	209.102645	47.691649
2155.949413	205.780730	47.696653
2153.014843	196.617369	47.701658
2149.547297	192.288442	47.706663
2145.969849	195.244511	47.711668
2141.971552	193.389462	47.716673
2138.599206	193.862681	47.721677
2135.103129	206.447356	47.726682
2131.512688	206.386476	47.731687
2128.094095	203.400863	47.736692
2124.684312	201.877469	47.741697
2121.535917	202.416928	47.746701
2117.959664	205.025700	47.751706
2114.277637	190.628409	47.756711
2110.505270	204.569847	47.761716
2107.253474	198.277706	47.766721
2103.843024	200.243999	47.771725
2100.389425	192.784573	47.776730
2096.946944	191.940516	47.781735
2092.941465	200.543734	47.786740
2089.544708	197.560860	47.791745
2086.269893	195.338528	47.796749
2082.372348	198.859599	47.801754
2079.233682	196.979670	47.806759
2075.381723	203.913317	47.811764
2072.301696	199.123207	47.816769
2069.008348	203.903199	47.821773
2065.240874	204.304567	47.826778
2062.077633	189.544983	47.831783
2058.098064	195.389479	47.836788
2054.800115	194.834959	47.841793
2051.441123	198.283101	47.846797
2047.665723	205.212610	47.851802
2044.070807	193.927846	47.856807
2040.420112	198.571107	47.861812
2037.384525	201.391986	47.866817
2033.834846	191.889831	47.871821
2030.107642	198.298505	47.876826
2026.433729	190.660423	47.881831
2022.882755	199.821699	47.886836
2019.757582	195.874224	47.891841
2016.438049	193.120392	47.896845
2012.767734	200.056448	47.901850
2009.298609	194.012611	47.906855
2005.796781	187.886955	47.911860
2002.329998	199.661128	47.916865
1998.894734	188.259659	47.921869
1994.820025	200.438731	47.926874
1991.854153	189.632477	47.931879
1988.116301	190.752658	47.936884
1984.992304	185.711952	47.941889
1981.335035	189.053897	47.946893
1977.747281	199.189424	47.951898
1974.314761	183.070912	47.956903
1970.481518	187.347321	47.961908
1967.186416	193.366956	47.966913
1963.285222	191.692177	47.971917
1960.058433	192.325006	47.976922
1956.822964	187.190641	47.981927
1953.613540	191.266153	47.986932
1949.736775	184.150650	47.991937
1946.238687	188.771927	47.996941
1942.574641	188.219144	48.001946
1939.077553	190.662818	48.006951
1935.399188	199.300533	48.011956
1932.199332	185.465920	48.016961
1928.955371	192.789439	48.021965
1925.109356	187.579518	48.026970
1921.973218	182.259852	48.031975
1918.322011	186.648713	48.036980
1914.775869	179.257614	48.041985
1911.035605	184.944092	48.046989
1907.495930	185.813937	48.051994
1904.087833	177.103527	48.056999
1900.571601	187.140059	48.062004
1897.159658	178.777804	48.067009
1893.762253	177.212674	48.072013
1890.275347	180.438925	48.077018
1887.014966	184.296546	48.082023
1883.130116	184.207915	48.087028
1879.699477	178.929031	48.092033
1876.225665	185.205574	48.097037
1872.451841	184.875026	48.102042
1869.324163	179.595246	48.107047
1865.572891	182.175877	48.112052
1862.230191	177.025750	48.117057
1858.740898	183.542062	48.122061
1854.952934	184.866383	48.127066
1851.536590	181.729053	48.132071
1847.964936	191.620850	48.137076
1844.915511	183.052525	48.142081
1841.643831	189.435814	48.147085
1838.082336	189.145406	48.152090
1834.497373	180.276400	48.157095
1830.378942	182.581244	48.162100
1826.880788	180.970051	48.167105
1823.563457	188.035397	48.172109
1819.943999	188.987751	48.177114
1816.825953	180.649040	48.182119
1813.137051	190.943263	48.187124
1809.324013	184.488113	48.192129
1806.223384	183.537673	48.197133
1802.663337	189.248334	48.202138
1799.553341	170.207994	48.207143
1795.506835	182.017658	48.212148
1791.989490	181.498776	48.217153
1788.693541	179.861115	48.222157
1784.988719	179.189288	48.227162
1781.808681	178.810058	48.232167
1777.920498	186.580301	48.237172
1774.702787	190.167105	48.242177
1770.961556	183.742751	48.247181
1767.571711	184.761605	48.252186
1764.164771	187.045072	48.257191
1760.509235	184.868700	48.262196
1756.977650	185.503669	48.267201
1753.525288	184.920206	48.272205
1750.034656	180.146261	48.277210
1746.690287	184.699259	48.282215
1743.189426	185.960055	48.287220
1739.756321	184.949143	48.292225
1736.228699	187.446155	48.297229
1732.349936	189.025735	48.302234
1729.127915	180.773336	48.307239
1725.253672	193.762710	48.312244
1722.255359	185.653131	48.317249
1718.812504	180.224439	48.322253
1714.913255	175.086648	48.327258
1711.037333	174.258242	48.332263
1707.852926	177.808601	48.337268
1704.746040	174.980598	48.342273
1701.425596	174.202313	48.347277
1697.597164	175.859842	48.352282
1694.352248	175.802001	48.357287
1690.313760	184.953253	48.362292
1686.916448	173.500204	48.367297
1683.512430	172.708705	48.372301
1680.005212	185.155168	48.377306
1676.797023	180.554451	48.382311
1673.060834	182.173868	48.387316
1669.719013	180.685956	48.392321
1666.152890	182.316155	48.397325
1662.296430	184.719351	48.402330
1658.987211	177.277480	48.407335
1655.459618	178.991900	48.412340
1652.251189	180.188264	48.417345
1648.473015	177.641318	48.422349
1644.706236	189.960389	48.427354
1641.342052	182.099386	48.432359
1638.048688	187.498901	48.437364
1634.385882	186.540424	48.442369
1631.206014	172.521218	48.447373
1627.396547	181.645726	48.452378
1624.116046	178.258000	48.457383
1620.947367	180.131398	48.462388
1616.983319	180.909562	48.467393
1613.558836	177.227327	48.472397
1609.992071	187.304165	48.477402
1606.491235	174.142365	48.482407
1603.015497	180.053738	48.487412
1599.352123	179.817051	48.492417
1596.076019	178.798261	48.497421
1592.020024	183.876058	48.502426
1588.640739	173.128165	48.507431
1585.323879	181.009574	48.512436
1581.995033	175.525252	48.517441
1579.067094	168.757308	48.522445
1575.036231	180.301693	48.527450
1571.629008	184.152012	48.532455
1567.891729	179.491588	48.537460
1564.473439	182.218911	48.542465
1560.918804	177.025889	48.547469
1557.390571	187.389047	48.552474
1554.249885	173.115572	48.557479
1550.156812	181.022456	48.562484
1546.667165	183.004394	48.567489
1543.778770	178.799876	48.572493
1539.928676	178.593104	48.577498
1536.351923	169.202425	48.582503
1532.663946	182.051027	48.587508
1529.099636	174.532813	48.592513
1526.111887	173.172783	48.597517
1522.749259	175.073166	48.602522
1518.983897	167.432488	48.607527
1515.376074	176.293261	48.612532
1511.929732	173.506885	48.617537
1508.501045	174.529382	48.622541
1504.596198	185.176224	48.627546
1501.865986	172.156338	48.632551
1497.916997	170.658776	48.637556
1494.078176	174.550476	48.642561
1491.116241	169.238648	48.647565
1487.120901	171.856549	48.652570
1484.106763	167.420064	48.657575
1480.201659	172.445187	48.662580
1476.822170	173.390903	48.667585
1473.764438	176.779776	48.672589
1470.141841	177.446972	48.677594
1466.390450	170.359539	48.682599
1462.617345	171.559365	48.687604
1459.176397	177.794049	48.692609
1455.859033	165.036214	48.697613
1452.352827	168.805880	48.702618
1449.060767	170.821540	48.707623
1445.261783	180.728472	48.712628
1441.549430	162.678591	48.717633
1438.463357	179.304877	48.722637
1434.679326	168.987112	48.727642
1431.498046	170.769376	48.732647
1427.536181	166.064694	48.737652
1424.531627	173.705339	48.742657
1421.105410	160.935532	48.747661
1417.288013	170.678573	48.752666
1413.946847	161.089028	48.757671
1410.137798	172.265145	48.762676
1406.432526	168.302689	48.767681
1403.418232	164.900536	48.772685
1399.792595	172.072353	48.777690
1396.478118	171.014859	48.782695
1392.882972	170.370805	48.787700
1389.389514	172.059257	48.792705
1385.863951	167.498190	48.797709
1382.216200	177.148691	48.802714
1378.766433	162.230644	48.807719
1375.270283	161.811192	48.812724
1371.746819	170.191412	48.817729
1368.357951	167.816177	48.822733
1364.791487	167.962084	48.827738
1361.275643	167.199767	48.832743
1357.861814	177.662147	48.837748
1353.996388	176.545969	48.842753
1351.146553	179.295123	48.847757
1347.437474	167.968889	48.852762
1343.846565	169.233023	48.857767
1340.087434	166.431190	48.862772
1336.632472	175.184134	48.867777
1333.411017	161.655539	48.872781
1329.417948	162.989315	48.877786
1326.362552	162.482444	48.882791
1322.607453	166.360833	48.887796
1319.476456	172.555625	48.892801
1315.975825	165.702165	48.897805
1312.354402	171.010479	48.902810
1308.617395	166.273473	48.907815
1304.995529	171.270861	48.912820
1301.398128	162.651449	48.917825
1297.896322	165.197597	48.922829
1294.789764	162.137167	48.927834
1291.288079	158.821382	48.932839
1287.993791	168.274984	48.937844
1284.125724	164.910047	48.942849
1280.799531	161.097964	48.947853
1276.841942	162.597210	48.952858
1273.767582	154.357873	48.957863
1270.221437	159.238178	48.962868
1266.697064	166.000054	48.967873
1263.533766	154.939289	48.972877
1259.452030	169.217545	48.977882
1256.150046	171.826203	48.982887
1252.737843	162.012519	48.987892
1248.996500	170.236633	48.992897
1245.853790	157.101418	48.997901
1241.997475	167.965778	49.002906
1238.937016	162.262717	49.007911
1235.361025	162.883121	49.012916
1231.718837	166.401522	49.017921
1228.139061	152.700191	49.022925
1224.227286	159.920221	49.027930
1220.887114	155.647148	49.032935
1217.839034	157.077785	49.037940
1214.213826	168.634109	49.042945
1210.819035	163.256495	49.047949
1206.993320	164.296304	49.052954
1203.798205	164.275370	49.057959
1200.439735	166.989114	49.062964
1196.570705	167.311469	49.067969
1193.447018	157.159462	49.072973
1189.467958	165.081721	49.077978
1185.957845	152.245487	49.082983
1182.591996	164.880222	49.087988
1178.848106	158.676870	49.092993
1175.926477	166.814259	49.097997
1172.147449	163.716499	49.103002
1168.644744	160.760726	49.108007
1164.937016	164.309944	49.113012
1161.614756	160.397845	49.118017
1158.422343	150.436810	49.123021
1154.462567	164.824233	49.128026
1150.943803	160.834911	49.133031
1147.568672	166.096705	49.138036
1144.109467	155.864442	49.143041
1140.363271	157.759247	49.148045
1136.976720	160.605354	49.153050
1133.947346	155.004783	49.158055
1130.239192	162.864932	49.163060
1126.751940	164.925126	49.168065
1123.061269	162.764559	49.173069
1119.075206	162.290537	49.178074
1116.185317	154.211448	49.183079
1112.677794	159.020755	49.188084
1109.044328	154.726406	49.193089
1105.600620	159.775785	49.198093
1101.882390	164.583827	49.203098
1098.428143	162.096077	49.208103
1095.175383	165.784628	49.213108
1091.543686	163.612560	49.218113
1087.928740	153.859975	49.223117
1084.232543	165.475285	49.228122
1080.975443	158.608400	49.233127
1077.301044	169.166925	49.238132
1074.058635	162.662688	49.243137
1070.780956	155.107351	49.248141
1067.035068	157.350069	49.253146
1063.351815	154.913633	49.258151
1059.820872	158.127038	49.263156
1056.557153	161.245939	49.268161
1053.136900	155.205469	49.273165
1049.451082	165.694463	49.278170
1046.109956	164.625059	49.283175
1042.442893	164.115920	49.288180
1039.050307	162.619507	49.293185
1035.980043	160.911534	49.298189
1031.872599	155.082198	49.303194
1028.582953	151.492589	49.308199
1024.734954	152.857895	49.313204
1021.003956	156.031000	49.318209
1017.800411	147.650619	49.323213
1014.504153	155.119303	49.328218
1011.237194	144.081814	49.333223
1007.785426	153.452496	49.338228
1004.000970	154.037302	49.343233
1000.521181	147.422014	49.348237
996.924670	157.710183	49.353242
993.722368	160.961843	49.358247
990.038280	158.888707	49.363252
986.121123	164.030476	49.368257
982.841363	154.465676	49.373261
979.333788	158.847262	49.378266
975.907055	158.461830	49.383271
972.360313	153.146640	49.388276
968.952276	156.289072	49.393281
965.637894	147.449113	49.398285
961.965703	147.758456	49.403290
958.573151	154.253456	49.408295
954.895330	155.602913	49.413300
951.209476	156.709792	49.418305
947.935241	148.754775	49.423309
944.140288	159.395288	49.428314
940.702881	147.141243	49.433319
937.556580	147.727130	49.438324
933.868365	155.691672	49.443329
930.494719	157.809989	49.448333
926.863156	156.781407	49.453338
923.279693	138.886788	49.458343
919.910266	163.831745	49.463348
916.316321	159.544442	49.468353
912.928256	143.703758	49.473357
909.351887	153.716132	49.478362
906.132899	152.372662	49.483367
902.520161	152.491856	49.488372
898.845238	155.077785	49.493377
895.330402	151.949205	49.498381
891.518429	155.240986	49.503386
888.259326	155.750842	49.508391
885.041013	149.953781	49.513396
881.439249	153.855305	49.518401
877.655388	145.839593	49.523405
874.237226	154.571752	49.528410
870.728366	152.287594	49.533415
867.135038	151.558216	49.538420
863.714067	155.380912	49.543425
860.570406	151.160083	49.548429
856.857899	155.819956	49.553434
853.987972	143.746826	49.558439
849.917807	153.606478	49.563444
845.835904	161.003345	49.568449
842.407176	144.613750	49.573453
839.055377	150.643678	49.578458
835.914082	150.091162	49.583463
832.287516	154.242314	49.588468
828.594501	147.610935	49.593473
825.534819	146.497713	49.598477
822.259520	150.283123	49.603482
818.526918	146.160728	49.608487
814.640225	146.395163	49.613492
810.783236	146.060307	49.618497
808.096272	142.040447	49.623501
804.457763	152.797067	49.628506
800.784888	147.037767	49.633511
797.269247	147.462052	49.638516
793.430070	148.483517	49.643521
790.274393	145.118606	49.648525
786.708920	144.965644	49.653530
783.241510	148.978222	49.658535
779.795414	143.911378	49.663540
776.166645	142.083247	49.668545
773.026748	143.526209	49.673549
769.032154	146.203403	49.678554
765.395172	140.788077	49.683559
762.257022	140.357838	49.688564
758.711212	142.890946	49.693569
755.491970	143.228543	49.698573
751.847903	146.727888	49.703578
748.230853	144.550530	49.708583
744.812598	146.485538	49.713588
741.075345	156.564901	49.718593
737.595162	150.490603	49.723597
734.127067	155.248079	49.728602
730.701207	146.339142	49.733607
727.537634	150.714721	49.738612
723.521997	146.254425	49.743617
720.222226	146.206750	49.748621
716.328663	137.695083	49.753626
713.157634	146.703781	49.758631
709.761537	135.036117	49.763636
706.403675	148.959403	49.768641
703.026470	142.876983	49.773645
699.108139	143.438017	49.778650
695.658751	146.033763	49.783655
692.154000	148.558158	49.788660
688.435450	141.307156	49.793665
685.146898	140.505011	49.798669
681.594678	146.137024	49.803674
678.131513	136.126070	49.808679
674.588485	147.455635	49.813684
670.938619	148.342878	49.818689
667.628936	141.561797	49.823693
664.002920	143.904597	49.828698
660.606252	143.376104	49.833703
657.212411	139.786858	49.838708
653.566677	146.833081	49.843713
650.316234	135.957555	49.848717
646.501181	141.082114	49.853722
643.034912	134.107329	49.858727
639.519557	135.858184	49.863732
636.091884	138.288368	49.868737
632.704073	135.428881	49.873741
628.884736	138.327620	49.878746
625.505029	133.503502	49.883751
622.211122	141.974320	49.888756
618.578276	138.779262	49.893761
615.456678	135.550533	49.898765
611.443395	145.547979	49.903770
607.890732	146.110360	49.908775
604.703540	137.056278	49.913780
601.354704	148.379813	49.918785
597.908011	142.608928	49.923789
594.028465	147.788406	49.928794
590.571374	140.676771	49.933799
587.228769	144.574517	49.938804
583.028568	152.123391	49.943809
579.597864	143.838182	49.948813
576.075608	142.919287	49.953818
572.736736	140.621852	49.958823
569.606445	139.949899	49.963828
566.139333	146.035997	49.968833
562.891258	139.984622	49.973837
559.083682	143.096571	49.978842
555.783232	142.867188	49.983847
552.288172	138.500301	49.988852
548.530008	145.637826	49.993857
544.897361	132.937328	49.998861
541.468243	143.110098	50.003866
538.280892	141.596893	50.008871
534.291902	133.031539	50.013876
530.860763	137.286746	50.018881
527.784208	139.840265	50.023885
524.285856	141.799744	50.028890
520.809061	134.921330	50.033895
516.872042	135.721238	50.038900
513.235693	137.811700	50.043905
509.910950	132.927670	50.048909
506.326550	145.785654	50.053914
502.969241	139.007264	50.058919
499.777668	133.427501	50.063924
495.981173	138.355131	50.068929
492.264105	131.540972	50.073933
488.779342	136.910559	50.078938
485.160308	134.969768	50.083943
482.256177	151.005182	50.088948
478.440641	135.215921	50.093953
475.423860	129.362162	50.098957
471.605435	139.969209	50.103962
467.651280	142.474806	50.108967
464.338736	135.015931	50.113972
460.978950	143.160118	50.118977
457.425180	127.481686	50.123981
453.840083	132.947428	50.128986
450.699446	144.160234	50.133991
447.035986	138.336156	50.138996
443.140844	135.897237	50.144001
440.035447	136.779420	50.149005
436.344038	134.400723	50.154010
432.771190	132.221846	50.159015
429.585870	129.386636	50.164020
425.765758	132.069592	50.169025
422.642151	127.221613	50.174029
418.621212	132.673276	50.179034
415.181047	134.219067	50.184039
411.887713	133.615060	50.189044
408.375418	131.265354	50.194049
404.870654	135.709652	50.199053
401.390033	142.278025	50.204058
398.006251	146.995550	50.209063
394.405256	134.540377	50.214068
390.776313	139.404448	50.219073
387.244447	137.253952	50.224077
383.399213	140.029905	50.229082
380.372822	139.089093	50.234087
376.793966	135.602133	50.239092
373.408804	141.222910	50.244097
370.136483	129.205127	50.249101
366.463951	129.315320	50.254106
363.063977	132.067718	50.259111
359.360413	134.754135	50.264116
355.696731	137.814417	50.269121
352.403032	131.162976	50.274125
348.785803	134.507829	50.279130
345.120307	135.214407	50.284135
341.927305	130.788038	50.289140
338.424628	133.319270	50.294145
334.846826	126.197456	50.299149
331.131735	132.062902	50.304154
327.964085	131.237862	50.309159
324.379638	132.595470	50.314164
320.643986	135.381162	50.319169
317.159750	129.196216	50.324173
313.724509	135.158227	50.329178
310.482391	139.770077	50.334183
306.681635	132.655588	50.339188
302.805810	135.533565	50.344193
299.978188	136.637850	50.349197
296.127224	133.446421	50.354202
293.169436	132.361707	50.359207
289.128292	137.318755	50.364212
285.477913	137.535857	50.369217
282.172644	137.014833	50.374221
278.777394	135.617343	50.379226
275.113148	129.653250	50.384231
271.808225	141.554233	50.389236
268.301297	136.370613	50.394241
265.153940	135.681184	50.399245
261.281504	132.286534	50.404250
257.710467	147.598711	50.409255
253.933144	134.116725	50.414260
250.473570	125.104285	50.419265
247.334706	130.923154	50.424269
243.907563	135.855169	50.429274
240.341993	135.432718	50.434279
236.711933	131.077795	50.439284
233.187371	134.985396	50.444289
229.855495	132.150524	50.449293
226.139138	130.420443	50.454298
222.421973	137.714633	50.459303
219.495135	132.778983	50.464308
215.704052	135.827713	50.469313
212.308236	130.087421	50.474317
208.367657	134.653744	50.479322
205.123470	132.621146	50.484327
201.861783	130.644729	50.489332
198.245890	137.255772	50.494337
195.063684	131.498286	50.499341
191.122384	129.601430	50.504346
187.601237	130.558738	50.509351
184.209081	130.196426	50.514356
180.217492	128.103665	50.519361
177.175242	130.077500	50.524365
173.815766	133.293390	50.529370
170.328323	134.261905	50.534375
167.032808	129.532372	50.539380
163.079084	128.569613	50.544385
159.766697	130.905300	50.549389
155.840038	140.523312	50.554394
152.465181	127.541946	50.559399
149.422939	131.693390	50.564404
145.444091	136.794963	50.569409
141.814630	124.997936	50.574413
138.325725	124.857500	50.579418
135.189728	135.530014	50.584423
131.684550	130.989143	50.589428
127.974762	130.539949	50.594433
124.691983	123.424737	50.599437
121.250002	127.545490	50.604442
117.295486	118.840082	50.609447
114.126183	126.683208	50.614452
110.438356	131.910478	50.619457
106.989436	129.074366	50.624461
103.558762	126.038691	50.629466
99.814266	134.824025	50.634471
96.981594	129.964242	50.639476
93.343078	129.619903	50.644481
89.853208	125.413979	50.649485
85.909587	136.158281	50.654490
82.534980	133.056506	50.659495
79.139977	125.153604	50.664500
75.421901	135.643107	50.669505
72.324594	125.410518	50.674509
68.306404	128.917497	50.679514
64.625934	121.786292	50.684519
61.455700	126.770624	50.689524
58.265063	129.196340	50.694529
54.689111	127.052837	50.699533
51.108515	129.823738	50.704538
47.484536	127.800279	50.709543
44.520418	123.020318	50.714548
40.342622	128.679044	50.719553
36.872078	130.082558	50.724557
33.591494	124.069963	50.729562
30.023779	118.864262	50.734567
26.507576	126.488422	50.739572
22.866617	131.814959	50.744577
19.474902	113.712333	50.749581
15.974755	125.143383	50.754586
12.527062	119.843033	50.759591
8.958077	126.502694	50.764596
5.107106	133.604512	50.769601
2.257231	120.141297	50.774605