Tue Jun 21 13:15:41 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
-0.302779	96.489418	0.000000
-0.290031	104.699219	0.005005
-0.148291	95.160523	0.010010
0.012691	93.538655	0.015014
-0.478898	87.694938	0.020019
-0.564485	72.319458	0.025024
-0.844625	67.288088	0.030029
-0.969852	79.695914	0.035034
-1.068685	64.896877	0.040038
-1.398722	54.611470	0.045043
-1.191108	46.889799	0.050048
-1.692346	46.084244	0.055053
-1.773795	29.873794	0.060058
-1.915919	14.193382	0.065062
-2.590293	16.855228	0.070067
-2.678879	10.819304	0.075072
-3.241288	8.426862	0.080077
-4.163966	3.495595	0.085082
-4.271738	4.798514	0.090086
-4.712531	7.338997	0.095091
-4.937120	7.951847	0.100096
-4.826818	3.216767	0.105101
-4.906727	13.437294	0.110106
-4.735459	1.336920	0.115110
-5.370313	10.928283	0.120115
-5.930723	11.592005	0.125120
-5.819355	16.106940	0.130125
-6.488770	10.637835	0.135130
-6.376409	2.141245	0.140134
-6.145624	22.580732	0.145139
-6.964845	-3.579406	0.150144
-7.601812	6.349744	0.155149
-7.882204	14.500688	0.160154
-7.716574	6.465125	0.165158
-7.834365	-4.212362	0.170163
-7.671340	7.358342	0.175168
-8.560774	7.060084	0.180173
-9.199909	5.583345	0.185178
-9.193820	4.068437	0.190182
-9.375652	5.100051	0.195187
-9.121593	6.247151	0.200192
-9.194487	9.037909	0.205197
-9.828560	3.409825	0.210202
-10.087799	0.927914	0.215206
-10.760698	11.629065	0.220211
-10.603504	3.588191	0.225216
-10.989663	7.420645	0.230221
-11.739127	5.670123	0.235226
-12.001734	-0.972786	0.240230
-12.264082	12.445935	0.245235
-11.870318	2.919633	0.250240
-12.143082	9.110977	0.255245
-12.602309	-1.931082	0.260250
-12.252247	3.307410	0.265254
-12.800419	11.348774	0.270259
-13.310302	-3.788635	0.275264
-13.776169	1.945494	0.280269
-14.049823	7.252340	0.285274
-14.044114	2.159845	0.290278
-14.523434	14.220141	0.295283
-14.306105	7.094011	0.300288
-14.266769	-0.376785	0.305293
-15.079426	12.791084	0.310298
-15.286510	3.519381	0.315302
-15.585199	10.651759	0.320307
-15.522344	10.368281	0.325312
-15.804702	9.054464	0.330317
-16.815889	15.302573	0.335322
-16.978262	6.994540	0.340326
-17.238225	11.059080	0.345331
-17.285881	1.180227	0.350336
-17.245781	9.168972	0.355341
-17.562230	17.011141	0.360346
-17.132413	8.125724	0.365350
-17.400393	7.081057	0.370355
-17.986848	-1.305338	0.375360
-18.639969	1.526246	0.380365
-19.012460	13.437624	0.385370
-18.811424	-0.966608	0.390374
-19.176184	11.694736	0.395379
-19.961824	9.209023	0.400384
-20.263531	5.267762	0.405389
-20.022739	8.916874	0.410394
-20.142149	5.181437	0.415398
-20.342573	7.237725	0.420403
-20.239891	4.445862	0.425408
-20.472233	10.126327	0.430413
-21.354183	8.497004	0.435418
-21.606055	1.591443	0.440422
-21.642533	8.650208	0.445427
-21.793826	0.179124	0.450432
-22.554122	1.170960	0.455437
-23.027693	10.307601	0.460442
-23.374206	1.406887	0.465446
-23.373575	12.315397	0.470451
-23.306581	0.642745	0.475456
-23.583102	3.287648	0.480461
-23.454953	6.324143	0.485466
-23.625121	0.569318	0.490470
-24.605106	3.069243	0.495475
-25.084639	7.508173	0.500480
-25.373176	5.036443	0.505485
-25.180643	9.896686	0.510490
-25.080155	6.591134	0.515494
-25.379061	6.409001	0.520499
-25.194663	-0.052579	0.525504
-25.655101	5.175480	0.530509
-26.225495	11.162932	0.535514
-26.407669	4.432111	0.540518
-26.810229	3.133069	0.545523
-27.074161	1.091201	0.550528
-27.832933	1.087438	0.555533
-28.215505	-0.773563	0.560538
-27.579057	3.789590	0.565542
-28.215887	3.722221	0.570547
-28.584088	10.442830	0.575552
-28.437947	4.106772	0.580557
-28.676387	13.930467	0.585562
-28.344533	-2.822377	0.590566
-29.055279	5.897894	0.595571
-29.779034	1.421896	0.600576
-29.661686	5.797110	0.605581
-30.086709	8.190142	0.610586
-30.146001	9.557257	0.615590
-30.884950	15.007658	0.620595
-31.197298	4.213597	0.625600
-31.357482	10.504896	0.630605
-31.731209	13.787103	0.635610
-31.492925	0.760402	0.640614
-31.838735	13.508001	0.645619
-31.502064	12.773266	0.650624
-31.870848	4.092319	0.655629
-32.646960	11.223639	0.660634
-32.848558	9.329512	0.665638
-33.174950	12.469891	0.670643
-33.285117	6.566995	0.675648
-33.222071	12.694444	0.680653
-34.191174	16.363942	0.685658
-34.534825	11.789084	0.690662
-34.719705	14.923789	0.695667
-34.632652	14.391216	0.700672
-34.429425	10.701018	0.705677
-34.628660	13.857834	0.710682
-34.605031	3.979017	0.715686
-35.762736	16.714051	0.720691
-36.020771	2.884103	0.725696
-35.968898	15.392985	0.730701
-36.321598	14.628748	0.735706
-36.436916	-3.916028	0.740710
-37.313988	6.042819	0.745715
-37.817288	11.079264	0.750720
-37.501371	9.181135	0.755725
-37.608614	14.827664	0.760730
-37.367541	10.024752	0.765734
-38.236959	16.062119	0.770739
-38.164342	14.713596	0.775744
-38.052395	9.370062	0.780749
-39.176112	9.306361	0.785754
-39.235448	5.312338	0.790758
-39.493671	16.696268	0.795763
-39.621889	10.352362	0.800768
-39.818049	10.456517	0.805773
-39.832449	5.795960	0.810778
-39.800735	6.991519	0.815782
-40.773194	7.176669	0.820787
-40.963670	9.214339	0.825792
-41.236715	12.706214	0.830797
-41.200495	18.576049	0.835802
-41.242168	4.756843	0.840806
-42.190937	13.153245	0.845811
-42.724375	14.351619	0.850816
-42.937013	7.157177	0.855821
-43.037839	7.879577	0.860826
-42.417758	6.802896	0.865830
-43.123973	16.415948	0.870835
-42.901687	4.920635	0.875840
-42.880675	3.478045	0.880845
-44.002814	14.810860	0.885850
-44.176847	8.874733	0.890854
-44.780467	8.746219	0.895859
-44.418727	6.093004	0.900864
-44.262559	7.228290	0.905869
-45.426684	9.982490	0.910874
-45.899048	2.689967	0.915878
-46.114678	10.899250	0.920883
-46.221490	6.634455	0.925888
-46.302937	2.598905	0.930893
-46.552130	7.665691	0.935898
-46.081523	3.322445	0.940902
-45.954410	11.736437	0.945907
-46.622677	7.645129	0.950912
-47.181192	9.160429	0.955917
-47.613350	15.081382	0.960922
-47.452911	7.503704	0.965926
-48.450017	12.511812	0.970931
-48.888547	17.867870	0.975936
-48.857425	14.205777	0.980941
-49.202213	20.664796	0.985946
-48.463380	8.960608	0.990950
-49.111635	13.224622	0.995955
-49.072751	9.303133	1.000960
-49.968531	15.117539	1.005965
-50.372861	15.945649	1.010970
-50.356119	7.553891	1.015974
-50.700053	12.724378	1.020979
-50.542965	16.290065	1.025984
-51.034109	13.831759	1.030989
-51.948917	19.098956	1.035994
-51.758469	7.900769	1.040998
-51.887899	13.311015	1.046003
-51.914903	15.289647	1.051008
-52.185327	11.962045	1.056013
-52.488080	5.859572	1.061018
-52.470839	6.297007	1.066022
-53.347224	12.464189	1.071027
-53.766450	8.398142	1.076032
-54.113631	14.664761	1.081037
-54.121157	18.440439	1.086042
-53.603759	14.417211	1.091046
-53.931051	14.189264	1.096051
-54.798620	8.288857	1.101056
-55.269580	7.215844	1.106061
-55.291187	15.713665	1.111066
-55.267052	4.105930	1.116070
-55.631063	16.389062	1.121075
-55.529757	7.662633	1.126080
-55.598894	17.250106	1.131085
-56.886989	17.863252	1.136090
-56.730754	14.087299	1.141094
-57.164517	19.601619	1.146099
-56.815310	17.687319	1.151104
-56.718265	11.263486	1.156109
-57.544162	17.641547	1.161114
-58.081079	16.517098	1.166118
-58.313919	16.641339	1.171123
-58.697945	14.531152	1.176128
-58.403912	15.700242	1.181133
-58.563353	15.152840	1.186138
-59.012341	10.516101	1.191142
-59.576472	13.254615	1.196147
-59.810200	15.684248	1.201152
-59.853408	16.337906	1.206157
-60.115372	10.434299	1.211162
-60.170595	7.888612	1.216166
-61.027362	15.700674	1.221171
-61.797948	8.270663	1.226176
-60.751372	12.614342	1.231181
-61.227744	6.667112	1.236186
-61.531546	11.763663	1.241190
-61.879770	18.676328	1.246195
-61.928082	13.646452	1.251200
-62.348721	15.907337	1.256205
-63.300760	18.894597	1.261210
-63.492076	16.493003	1.266214
-63.603303	20.215012	1.271219
-63.686021	17.159034	1.276224
-63.428042	15.118748	1.281229
-63.620958	20.572859	1.286234
-63.912413	18.468653	1.291238
-64.117771	17.857421	1.296243
-64.420361	16.332851	1.301248
-64.779060	5.900092	1.306253
-65.380375	20.919476	1.311258
-65.243726	15.181130	1.316262
-65.158226	14.741955	1.321267
-65.868296	16.921124	1.326272
-66.310201	14.359749	1.331277
-66.684350	18.078134	1.336282
-66.501028	10.307029	1.341286
-66.747084	11.304290	1.346291
-67.309972	11.238889	1.351296
-67.853333	16.411225	1.356301
-67.903507	11.648848	1.361306
-67.837010	11.888489	1.366310
-68.355057	24.710990	1.371315
-68.326964	14.452945	1.376320
-68.481361	11.069032	1.381325
-68.691060	18.640937	1.386330
-68.701463	6.330693	1.391334
-69.509905	11.589155	1.396339
-69.496840	13.876884	1.401344
-69.784639	11.680512	1.406349
-69.899186	14.047982	1.411354
-70.216692	5.750849	1.416358
-70.977015	13.184043	1.421363
-71.402643	15.371558	1.426368
-71.454810	6.283182	1.431373
-71.601005	9.325246	1.436378
-71.635545	2.601753	1.441382
-71.586441	9.064604	1.446387
-71.950433	15.938834	1.451392
-71.892996	5.943519	1.456397
-72.786085	15.209429	1.461402
-73.103200	15.272640	1.466406
-73.122240	20.202847	1.471411
-73.200781	20.409082	1.476416
-73.839519	14.548927	1.481421
-74.145232	14.908420	1.486426
-74.333903	12.032396	1.491430
-74.615552	19.058356	1.496435
-74.800713	14.378717	1.501440
-74.626126	8.648102	1.506445
-75.110205	13.480285	1.511450
-75.442615	14.362396	1.516454
-76.288279	18.565966	1.521459
-76.214054	10.603162	1.526464
-76.142717	13.405357	1.531469
-76.608033	18.565560	1.536474
-76.236052	5.404831	1.541478
-76.251782	17.140109	1.546483
-77.134399	15.686141	1.551488
-77.563275	15.790751	1.556493
-77.881431	9.457978	1.561498
-77.875399	15.693928	1.566502
-77.971928	16.644128	1.571507
-78.415831	20.993100	1.576512
-79.049433	15.366329	1.581517
-79.775919	25.576127	1.586522
-79.344844	16.783638	1.591526
-79.558370	11.965039	1.596531
-79.979463	24.244013	1.601536
-79.824075	13.095636	1.606541
-79.538821	28.787927	1.611546
-79.962928	21.356184	1.616550
-80.601944	20.107948	1.621555
-80.943418	17.170994	1.626560
-80.948355	9.039953	1.631565
-81.204715	15.778945	1.636570
-81.653213	9.853346	1.641574
-82.472524	17.937448	1.646579
-82.796159	19.599941	1.651584
-82.816816	9.094033	1.656589
-82.748791	20.105242	1.661594
-82.704391	19.954467	1.666598
-82.799577	3.543083	1.671603
-83.202532	11.032140	1.676608
-83.641811	4.881636	1.681613
-84.726814	20.089062	1.686618
-84.284607	18.687422	1.691622
-84.491242	11.103440	1.696627
-84.409170	18.078834	1.701632
-84.374704	9.981128	1.706637
-85.001988	18.453354	1.711642
-85.549378	8.734816	1.716646
-86.029943	14.357920	1.721651
-85.976402	6.107282	1.726656
-85.881754	1.054132	1.731661
-86.386327	18.140340	1.736666
-87.023766	13.262889	1.741670
-87.438340	18.247152	1.746675
-87.732231	17.341954	1.751680
-87.975067	12.550311	1.756685
-87.626816	18.695251	1.761690
-87.847591	2.196924	1.766694
-87.975181	7.096953	1.771699
-87.985264	11.554639	1.776704
-88.415659	11.128676	1.781709
-89.364017	14.829479	1.786714
-89.436181	15.606529	1.791718
-89.457373	12.939767	1.796723
-89.631280	11.678049	1.801728
-89.588587	11.874666	1.806733
-90.429795	11.030706	1.811738
-90.743482	6.906931	1.816742
-91.061397	12.066204	1.821747
-91.193051	5.559087	1.826752
-91.412955	12.344333	1.831757
-91.265519	10.352742	1.836762
-91.131470	7.883850	1.841766
-91.272453	10.721207	1.846771
-92.278442	13.288206	1.851776
-92.511119	12.276572	1.856781
-93.005020	14.820728	1.861786
-92.907507	8.933961	1.866790
-92.785749	6.880122	1.871795
-93.636592	10.436903	1.876800
-93.933225	8.272189	1.881805
-94.680030	16.145569	1.886810
-94.236522	6.026528	1.891814
-94.519228	9.273732	1.896819
-94.541732	13.067476	1.901824
-94.383870	6.455976	1.906829
-95.270646	11.126535	1.911834
-95.774216	9.487254	1.916838
-95.787949	13.407022	1.921843
-95.998852	12.950828	1.926848
-95.868765	12.967014	1.931853
-96.461351	25.146320	1.936858
-96.733754	12.148937	1.941862
-97.048351	11.659201	1.946867
-97.569950	16.263760	1.951872
-97.473961	11.406139	1.956877
-97.886573	23.677787	1.961882
-97.487351	9.098455	1.966886
-98.283265	14.427269	1.971891
-98.546468	10.811553	1.976896
-98.556734	14.589853	1.981901
-99.052194	16.646460	1.986906
-99.054451	15.317243	1.991910
-98.836374	4.661494	1.996915
-99.817008	12.532913	2.006912
-99.719600	15.656102	2.016909
-99.049110	21.000286	2.026906
-98.531502	15.249464	2.036902
-97.853036	9.795452	2.046899
-97.728796	3.927607	2.056896
-97.135828	6.170873	2.066893
-96.595451	9.105113	2.076890
-95.951126	10.936998	2.086886
-95.080948	4.141246	2.096883
-95.092653	12.362629	2.106880
-94.695311	15.828946	2.116877
-93.569656	8.301902	2.126874
-93.576381	11.854894	2.136870
-93.146366	14.115665	2.146867
-92.191884	12.336087	2.156864
-91.758136	5.427079	2.166861
-91.682349	9.015605	2.176858
-90.939267	14.120740	2.186854
-90.451686	13.283318	2.196851
-90.252134	3.976073	2.206848
-89.386466	9.495199	2.216845
-88.856388	9.201806	2.226842
-88.585150	15.375976	2.236838
-87.451982	16.997093	2.246835
-87.379607	17.120927	2.256832
-87.434645	12.319501	2.266829
-86.301800	11.881828	2.276826
-85.823047	8.450383	2.286822
-85.790129	16.225145	2.296819
-84.632335	12.226798	2.306816
-84.400146	17.126290	2.316813
-84.172048	11.273843	2.326810
-83.475160	6.460320	2.336806
-82.734758	11.202737	2.346803
-82.517506	16.029818	2.356800
-81.712068	15.634315	2.366797
-81.231058	18.718083	2.376794
-81.117475	23.577747	2.386790
-80.316844	15.122130	2.396787
-79.820222	12.789266	2.406784
-79.377419	11.399105	2.416781
-79.249994	17.677709	2.426778
-78.312600	14.081000	2.436774
-78.109250	11.833652	2.446771
-77.356651	11.244770	2.456768
-76.454139	11.896795	2.466765
-76.610236	9.877515	2.476762
-76.214145	8.268262	2.486758
-75.243379	9.148458	2.496755
-75.037409	15.410892	2.506752
-74.296204	10.037382	2.516749
-73.575511	10.797960	2.526746
-73.582264	15.993687	2.536742
-73.063286	14.681998	2.546739
-72.432667	7.987566	2.556736
-71.972681	12.259936	2.566733
-71.250709	11.416894	2.576730
-70.572012	21.450609	2.586726
-70.535811	8.584229	2.596723
-70.230854	8.176176	2.606720
-68.888870	9.304317	2.616717
-68.820770	8.561261	2.626714
-68.800060	8.291367	2.636710
-67.868269	5.274714	2.646707
-67.400191	4.340349	2.656704
-66.938755	5.155716	2.666701
-65.767363	7.937449	2.676698
-65.574566	6.028734	2.686694
-65.464929	6.648068	2.696691
-65.245009	2.988599	2.706688
-64.480717	2.683294	2.716685
-63.879254	9.505788	2.726682
-63.298068	5.789851	2.736678
-62.251638	2.497749	2.746675
-62.209003	1.956891	2.756672
-62.369821	6.110573	2.766669
-61.896851	11.542598	2.776666
-61.081942	6.862464	2.786662
-59.880335	9.348547	2.796659
-59.416231	9.991179	2.806656
-59.169741	6.711218	2.816653
-59.315811	3.550010	2.826650
-58.585726	9.050894	2.836646
-57.877380	9.107743	2.846643
-57.490845	8.607740	2.856640
-56.434674	5.966651	2.866637
-56.096812	8.522467	2.876634
-55.950133	11.247859	2.886630
-55.770714	3.713921	2.896627
-54.800644	6.145680	2.906624
-54.447975	8.025277	2.916621
-53.676310	13.897062	2.926618
-53.279484	11.255896	2.936614
-53.200704	12.894153	2.946611
-52.240930	13.674221	2.956608
-51.527565	13.204267	2.966605
-51.581104	10.910744	2.976602
-50.812949	13.163340	2.986598
-50.055417	7.205438	2.996595
-49.709850	8.663181	3.006592
-49.657146	11.744971	3.016589
-48.889776	10.402426	3.026586
-48.616362	11.458966	3.036582
-47.827565	6.448843	3.046579
-47.042037	5.438991	3.056576
-47.166855	4.931790	3.066573
-46.349319	7.894828	3.076570
-45.718710	8.084289	3.086566
-45.631490	4.298408	3.096563
-44.529540	12.065671	3.106560
-44.004073	5.855749	3.116557
-44.053343	6.047148	3.126554
-43.219018	11.428228	3.136550
-42.522097	7.778089	3.146547
-42.334466	12.137057	3.156544
-42.246419	12.218780	3.166541
-41.420430	7.209612	3.176538
-40.836475	8.371611	3.186534
-39.826918	8.370482	3.196531
-39.712284	7.203012	3.206528
-39.434306	6.805553	3.216525
-39.133558	9.978848	3.226522
-38.061992	4.981375	3.236518
-37.411309	9.033871	3.246515
-37.329607	6.257183	3.256512
-37.069564	4.246641	3.266509
-35.853576	11.437238	3.276506
-35.828847	9.561294	3.286502
-35.534236	0.288297	3.296499
-34.617939	-1.051442	3.306496
-34.343288	2.644243	3.316493
-33.995717	8.152954	3.326490
-33.134046	5.450225	3.336486
-32.556839	3.761390	3.346483
-32.576561	0.131331	3.356480
-31.697616	5.499095	3.366477
-31.391026	4.961948	3.376474
-30.811207	2.525214	3.386470
-30.013247	3.273399	3.396467
-29.417119	-0.511199	3.406464
-29.501122	3.988578	3.416461
-29.167822	-1.177485	3.426458
-28.340238	1.730346	3.436454
-27.755800	3.188448	3.446451
-26.923624	-6.610228	3.456448
-26.296642	7.822999	3.466445
-26.800953	-2.584028	3.476442
-26.138239	0.583663	3.486438
-24.654767	1.914230	3.496435
-24.562299	-2.447493	3.506432
-24.293933	4.076290	3.516429
-24.441719	7.308844	3.526426
-23.455692	9.832810	3.536422
-22.816426	12.392069	3.546419
-21.849287	10.272340	3.556416
-21.781858	11.215395	3.566413
-21.585145	10.807289	3.576410
-20.671143	8.579192	3.586406
-20.302770	10.768971	3.596403
-19.709850	8.697379	3.606400
-18.844790	6.086760	3.616397
-18.685665	10.481471	3.626394
-18.482301	8.000181	3.636390
-17.877101	6.209697	3.646387
-17.165708	6.068265	3.656384
-16.843130	13.022112	3.666381
-16.270955	16.802893	3.676378
-15.627517	16.923253	3.686374
-15.293581	15.312046	3.696371
-14.729338	7.760813	3.706368
-13.606126	11.136975	3.716365
-13.791905	11.125139	3.726362
-13.804443	16.124241	3.736358
-12.579459	3.537584	3.746355
-11.823727	5.363483	3.756352
-11.847520	3.097636	3.766349
-11.300070	5.008409	3.776346
-10.457855	14.999844	3.786342
-10.373660	9.743435	3.796339
-10.083018	2.710333	3.806336
-9.100737	4.955932	3.816333
-8.750782	8.212168	3.826330
-8.122612	5.910284	3.836326
-7.369805	5.157383	3.846323
-7.110764	6.974246	3.856320
-6.968732	9.444536	3.866317
-6.296317	4.752046	3.876314
-5.425992	8.987696	3.886310
-5.383825	9.817173	3.896307
-4.926354	8.895832	3.906304
-3.982618	9.110508	3.916301
-4.187550	12.183392	3.926298
-3.071170	10.977290	3.936294
-2.818241	17.903947	3.946291
-2.433098	23.222691	3.956288
-2.028816	40.185578	3.966285
-1.784093	53.467194	3.976282
-1.529430	71.530749	3.986278
-1.066764	92.193123	3.996275
-0.600935	115.427586	4.006272
0.000000	148.048631	4.011277
0.170164	145.937623	4.016282
0.134425	171.045986	4.021286
0.205183	178.610998	4.026291
0.113728	184.910722	4.031296
0.292348	213.131750	4.036301
0.699203	196.597348	4.041306
0.764005	215.425310	4.046310
0.853611	209.134247	4.051315
0.860461	209.982683	4.056320
1.050487	206.221611	4.061325
1.273451	197.939060	4.066330
0.835992	209.787741	4.071334
0.869714	218.499111	4.076339
1.287622	221.653037	4.081344
1.003930	221.998424	4.086349
1.150437	229.527040	4.091354
1.041318	243.093455	4.096358
1.303871	243.219728	4.101363
1.477483	239.401376	4.106368
1.029429	240.456960	4.111373
1.460642	234.958853	4.116378
1.295506	236.882439	4.121382
1.364447	229.943778	4.126387
1.366187	223.833614	4.131392
0.900851	223.269760	4.136397
1.294888	226.479144	4.141402
1.004466	236.701327	4.146406
1.366653	244.703956	4.151411
1.185631	240.976295	4.156416
1.251270	244.792208	4.161421
1.445099	242.622212	4.166426
1.259357	251.797174	4.171430
1.561949	248.146116	4.176435
1.590606	243.757784	4.181440
1.109848	248.343011	4.186445
1.253099	244.825492	4.191450
1.506686	251.186510	4.196454
1.429065	247.070338	4.201459
1.363522	251.499787	4.206464
1.469149	251.295656	4.211469
1.304366	245.334418	4.216474
1.577669	258.256564	4.221478
1.194299	251.749574	4.226483
1.596499	256.334626	4.231488
1.271490	259.835949	4.236493
1.553824	248.207964	4.241498
1.392603	260.180059	4.246502
1.410182	255.958728	4.251507
1.565209	252.814789	4.256512
1.532515	263.401023	4.261517
1.656533	256.426392	4.266522
1.254353	259.563384	4.271526
1.388958	258.279958	4.276531
1.924944	258.626964	4.281536
1.590904	254.718026	4.286541
1.689685	255.939599	4.291546
1.355706	265.042025	4.296550
1.228254	257.807504	4.301555
1.551051	270.843419	4.306560
1.271457	294.701583	4.311565
1.579725	292.037049	4.316570
1.498886	289.920421	4.321574
1.765877	285.561285	4.326579
1.556481	292.223947	4.331584
1.620238	285.789131	4.336589
1.659042	289.357303	4.341594
1.825550	296.622550	4.346598
1.954383	286.188188	4.351603
2.051468	285.504364	4.356608
2.135206	295.455256	4.361613
2.016304	289.648615	4.366618
1.631242	295.290929	4.371622
1.777422	286.057056	4.376627
2.108860	287.919537	4.381632
1.900326	298.708569	4.386637
2.162742	293.612148	4.391642
1.859386	299.140490	4.396646
1.724978	294.774409	4.401651
1.940035	297.514183	4.406656
1.559957	297.203995	4.411661
1.933426	290.351438	4.416666
1.941191	293.009305	4.421670
1.839826	297.383918	4.426675
1.798946	281.064859	4.431680
1.577829	299.734051	4.436685
1.449299	305.318696	4.441690
1.961934	322.829016	4.446694
1.900627	320.520100	4.451699
2.364677	333.347181	4.456704
2.100433	335.862429	4.461709
2.326556	323.113940	4.466714
2.281804	329.279495	4.471718
2.410109	327.634993	4.476723
2.342751	323.947691	4.481728
2.277186	315.945910	4.486733
2.052752	307.362641	4.491738
1.808768	298.038457	4.496742
2.044878	323.210192	4.501747
2.363299	316.351347	4.506752
2.333622	327.161300	4.511757
2.643074	326.541372	4.516762
2.276965	310.817629	4.521766
2.221467	303.223070	4.526771
2.424806	303.582731	4.531776
1.851325	306.754017	4.536781
2.060994	321.173293	4.541786
1.819366	327.774015	4.546790
2.129538	329.578849	4.551795
2.514236	326.808115	4.556800
2.208558	332.658118	4.561805
2.507788	325.474077	4.566810
2.198943	333.565173	4.571814
2.325491	330.747593	4.576819
2.270246	327.243980	4.581824
2.185231	342.320658	4.586829
2.288293	332.901296	4.591834
2.231049	336.581486	4.596838
2.287164	336.291027	4.601843
2.050817	330.417187	4.606848
2.124256	333.281849	4.611853
2.715307	343.522327	4.616858
2.606406	346.210572	4.621862
2.496025	341.873652	4.626867
2.404361	338.259834	4.631872
2.060215	336.239884	4.636877
2.601402	349.163925	4.641882
2.469689	363.085644	4.646886
2.448204	369.791423	4.651891
2.591434	367.265502	4.656896
2.414127	370.370608	4.661901
2.615648	361.981406	4.666906
2.853616	368.359859	4.671910
2.643646	362.787512	4.676915
2.650037	363.052899	4.681920
2.579492	372.184782	4.686925
2.678459	372.804256	4.691930
2.686235	362.982297	4.696934
2.566709	364.830265	4.701939
2.510203	370.268028	4.706944
2.448910	377.526633	4.711949
2.625436	368.015951	4.716954
2.481910	372.671669	4.721958
2.627997	369.970829	4.726963
2.941419	366.214150	4.731968
2.634486	373.964345	4.736973
2.920333	364.687564	4.741978
2.283888	371.852552	4.746982
2.596597	362.144285	4.751987
2.592690	374.176655	4.756992
2.909532	391.124302	4.761997
2.927391	385.839237	4.767002
2.955145	380.903008	4.772006
2.671625	376.189613	4.777011
2.862798	381.241815	4.782016
2.638152	392.152180	4.787021
2.961595	400.058097	4.792026
3.036311	400.349863	4.797030
3.146000	405.499237	4.802035
3.416601	399.508274	4.807040
2.761645	372.395173	4.812045
2.719269	368.889617	4.817050
2.771859	381.930703	4.822054
2.738928	395.433919	4.827059
3.068149	401.616514	4.832064
2.830278	408.915226	4.837069
3.050719	406.054853	4.842074
2.882393	406.098157	4.847078
3.069938	402.265618	4.852083
3.161349	398.036167	4.857088
2.979200	405.600938	4.862093
3.047217	397.824259	4.867098
3.196489	405.000846	4.872102
2.949327	406.561317	4.877107
3.198090	404.255905	4.882112
2.751029	404.438508	4.887117
3.422102	403.058739	4.892122
3.127668	410.086598	4.897126
2.819166	401.677041	4.902131
3.109559	399.575692	4.907136
3.100608	412.539968	4.912141
3.169213	408.667132	4.917146
3.032676	404.010890	4.922150
3.150356	405.681250	4.927155
3.437033	407.611741	4.932160
3.364431	415.385118	4.937165
3.203166	404.730334	4.942170
3.176302	410.317916	4.947174
3.377459	401.841332	4.952179
3.192200	401.653397	4.957184
2.967537	407.476003	4.962189
3.444132	423.032243	4.967194
3.582673	433.683186	4.972198
3.342431	429.552453	4.977203
3.661632	420.556651	4.982208
3.421409	416.716795	4.987213
3.726868	402.654841	4.992218
3.387707	413.530704	4.997222
3.317206	412.048369	5.002227
3.345609	401.334552	5.007232
3.337526	397.963224	5.012237
3.337494	411.794705	5.017242
3.511700	432.648648	5.022246
3.373373	437.094148	5.027251
3.793720	430.810589	5.032256
3.486006	435.268152	5.037261
3.464203	429.672122	5.042266
3.802357	440.539255	5.047270
3.609299	424.042380	5.052275
3.566222	413.287308	5.057280
3.475447	424.306560	5.062285
3.346607	427.163491	5.067290
3.645976	431.595911	5.072294
3.458646	441.896078	5.077299
3.417225	431.829234	5.082304
3.366509	424.018526	5.087309
3.433624	419.527870	5.092314
3.529199	434.237483	5.097318
3.628715	429.871899	5.102323
3.269580	428.186539	5.107328
3.232173	432.491596	5.112333
3.447643	439.081403	5.117338
3.756918	459.508473	5.122342
3.673075	468.333186	5.127347
4.041769	464.568517	5.132352
4.029645	459.968619	5.137357
3.688864	442.935150	5.142362
3.900468	442.601380	5.147366
3.507944	442.285552	5.152371
3.777015	455.872412	5.157376
3.810439	468.551865	5.162381
3.928372	466.323758	5.167386
3.960588	466.772145	5.172390
3.976674	468.327118	5.177395
4.126032	455.560249	5.182400
3.615076	449.000103	5.187405
3.766368	459.189350	5.192410
4.029874	471.619949	5.197414
4.125995	470.161918	5.202419
4.036527	465.138312	5.207424
4.044164	451.051825	5.212429
3.874116	444.113568	5.217434
3.849759	446.544118	5.222438
4.130909	462.603415	5.227443
3.903917	471.633188	5.232448
3.302222	480.473011	5.237453
3.685365	470.155076	5.242458
3.739505	473.496969	5.247462
3.639921	475.811315	5.252467
4.094562	466.146577	5.257472
3.781094	471.010832	5.262477
3.681914	478.784695	5.267482
3.892156	484.029929	5.272486
3.997827	494.948226	5.277491
4.391348	497.991989	5.282496
4.148569	498.342644	5.287501
4.395041	500.469250	5.292506
4.093144	500.903697	5.297510
3.849469	501.014338	5.302515
4.123309	499.066681	5.307520
3.864144	501.553487	5.312525
4.230353	505.709637	5.317530
4.300243	502.447922	5.322534
4.203038	505.949270	5.327539
4.317690	494.631852	5.332544
4.129271	504.022703	5.337549
4.253643	497.793060	5.342554
4.307768	503.715766	5.347558
3.901563	503.353657	5.352563
4.290492	495.458274	5.357568
4.158719	498.282945	5.362573
4.305342	500.845234	5.367578
4.156984	501.313656	5.372582
4.238314	491.904110	5.377587
4.786325	502.170370	5.382592
4.514038	507.277847	5.387597
4.668144	500.420672	5.392602
4.465180	500.209816	5.397606
4.519822	504.711594	5.402611
4.504953	496.919581	5.407616
4.544266	509.304847	5.412621
4.511210	502.222714	5.417626
4.471797	502.535550	5.422630
4.380198	507.130810	5.427635
4.687302	502.084939	5.432640
4.323723	506.171106	5.437645
4.405927	502.468074	5.442650
4.658312	509.060087	5.447654
4.437736	507.727706	5.452659
4.500362	502.049193	5.457664
4.325390	508.005298	5.462669
4.469287	500.955237	5.467674
4.736494	503.307324	5.472678
4.569326	504.789436	5.477683
4.662303	499.466634	5.482688
4.632283	509.836705	5.487693
4.597692	499.326250	5.492698
4.691087	508.711683	5.497702
4.015743	516.637015	5.502707
4.746640	528.811082	5.507712
4.539114	529.759169	5.512717
4.891491	536.338188	5.517722
4.983974	539.433780	5.522726
5.049720	537.977616	5.527731
5.216439	529.908054	5.532736
5.017711	523.916216	5.537741
4.533583	507.385159	5.542746
4.856616	509.846209	5.547750
4.334526	508.647229	5.552755
4.879632	520.758911	5.557760
4.840719	534.375130	5.562765
5.170180	532.849841	5.567770
4.964069	531.972102	5.572774
4.595566	517.311220	5.577779
4.791743	518.938205	5.582784
4.899009	534.791535	5.587789
4.968505	528.931308	5.592794
4.820619	528.363816	5.597798
5.029859	541.520788	5.602803
5.136860	536.363390	5.607808
5.022507	547.309869	5.612813
4.719015	541.850429	5.617818
4.533379	542.231881	5.622822
4.776516	542.700995	5.627827
5.198872	538.492089	5.632832
4.629538	542.076360	5.637837
4.835965	540.638736	5.642842
4.674859	537.411119	5.647846
4.577106	537.268684	5.652851
4.774575	539.495567	5.657856
4.834532	556.078820	5.662861
5.018084	561.814746	5.667866
5.154547	568.267713	5.672870
4.797094	575.533811	5.677875
5.166512	564.923260	5.682880
5.108711	568.166489	5.687885
5.178051	572.130665	5.692890
5.307429	576.534047	5.697894
5.125973	580.488446	5.702899
5.259041	575.144376	5.707904
4.981176	577.518451	5.712909
5.166487	564.928671	5.717914
5.109721	573.956366	5.722918
4.856037	575.167259	5.727923
5.054443	575.655424	5.732928
5.208129	578.703790	5.737933
5.327394	573.500342	5.742938
5.271711	570.340711	5.747942
5.151003	579.729868	5.752947
5.233608	570.306052	5.757952
5.398128	577.074068	5.762957
5.199016	576.778506	5.767962
5.079848	571.051134	5.772966
4.938680	599.615120	5.777971
5.333596	601.827474	5.782976
5.379677	605.875433	5.787981
5.509678	605.500114	5.792986
5.679482	601.066601	5.797990
5.470665	609.721260	5.802995
5.611713	606.989836	5.808000
5.714341	612.613475	5.813005
5.449556	615.302516	5.818010
5.850642	613.280296	5.823014
5.205751	610.533966	5.828019
5.379336	599.732034	5.833024
5.514148	612.521904	5.838029
5.522011	602.886069	5.843034
5.700554	611.738262	5.848038
5.710321	616.156922	5.853043
5.487817	614.548574	5.858048
5.465592	612.788461	5.863053
5.843196	615.025983	5.868058
5.580883	618.762101	5.873062
5.260950	620.314119	5.878067
5.563936	615.438212	5.883072
5.470041	623.831318	5.888077
5.281882	612.693017	5.893082
5.404604	613.119317	5.898086
5.312187	614.478354	5.903091
5.459615	611.349020	5.908096
5.387951	623.452400	5.913101
5.630065	628.989799	5.918106
5.802272	634.018781	5.923110
5.706794	640.336524	5.928115
5.968089	643.018974	5.933120
5.945383	628.563585	5.938125
5.615397	618.181492	5.943130
5.946734	612.537182	5.948134
5.482665	617.065484	5.953139
5.978371	624.769135	5.958144
5.926147	635.542976	5.963149
6.050110	631.852339	5.968154
5.486911	622.302565	5.973158
5.792342	628.423476	5.978163
6.008536	627.849765	5.983168
5.972769	635.742267	5.988173
5.745832	632.539542	5.993178
6.056402	633.431841	5.998182
5.884126	636.259099	6.003187
6.188073	628.010864	6.008192
5.900597	636.954249	6.013197
6.009626	642.786218	6.018202
6.147138	630.392564	6.023206
6.087234	630.110063	6.028211
6.184542	626.855425	6.033216
5.957173	628.462962	6.038221
5.656703	601.803255	6.043226
5.969447	611.225840	6.048230
5.893208	620.674162	6.053235
5.983803	621.198533	6.058240
5.660766	629.050586	6.063245
5.619778	627.274436	6.068250
5.922954	627.225063	6.073254
5.781605	628.895714	6.078259
6.177461	625.851736	6.083264
5.908608	623.836646	6.088269
5.996650	632.063070	6.093274
6.213053	628.297924	6.098278
5.962104	631.754307	6.103283
6.288367	621.014501	6.108288
6.109583	632.743904	6.113293
6.070853	622.112687	6.118298
6.159013	615.460368	6.123302
5.829190	622.088449	6.128307
5.984500	603.500690	6.133312
5.775871	607.396248	6.138317
6.116687	620.629184	6.143322
6.314751	614.287437	6.148326
6.138849	615.897699	6.153331
5.949083	609.748642	6.158336
5.703253	607.366436	6.163341
5.523197	602.487833	6.168346
5.761984	614.023951	6.173350
5.690480	630.999066	6.178355
6.171996	621.852341	6.183360
6.010741	632.270273	6.188365
5.831129	621.284278	6.193370
6.008103	617.811808	6.198374
5.927461	630.414571	6.203379
6.138995	619.324736	6.208384
6.241135	630.801202	6.213389
5.999185	629.890910	6.218394
6.057502	624.989011	6.223398
6.303448	621.844940	6.228403
5.689254	618.607870	6.233408
5.998128	607.048238	6.238413
5.819584	612.980109	6.243418
6.102044	611.080741	6.248422
5.754182	618.833888	6.253427
6.265792	616.505248	6.258432
6.048371	621.256752	6.263437
5.897474	609.908231	6.268442
5.896337	604.640643	6.273446
5.843193	609.457494	6.278451
5.933750	615.472486	6.283456
6.260994	630.093603	6.288461
5.929769	625.102082	6.293466
5.766380	609.991153	6.298470
5.675599	618.141209	6.303475
6.087248	620.889535	6.308480
6.114161	628.412691	6.313485
5.988248	627.151061	6.318490
6.258499	630.327549	6.323494
5.545563	622.652050	6.328499
5.637193	624.163152	6.333504
5.510061	628.583962	6.338509
5.851530	633.476774	6.343514
6.195927	637.128616	6.348518
6.046417	634.546141	6.353523
6.314422	636.330760	6.358528
6.387570	638.041081	6.363533
5.749079	636.141464	6.368538
5.909238	634.496392	6.373542
6.021520	639.235340	6.378547
6.151670	629.366110	6.383552
5.514058	637.641258	6.388557
5.829169	631.973579	6.393562
6.105624	625.748500	6.398566
6.209072	629.170473	6.403571
6.320073	626.582752	6.408576
6.020666	622.281394	6.413581
5.792609	617.899350	6.418586
6.085257	614.305899	6.423590
6.179625	624.135061	6.428595
5.728872	626.064547	6.433600
5.899942	611.723515	6.438605
5.951160	624.929221	6.443610
6.492760	618.389686	6.448614
5.896303	620.557018	6.453619
5.920988	610.042790	6.458624
5.855166	611.058194	6.463629
5.922162	611.862157	6.468634
6.055287	614.104837	6.473638
5.978003	607.877164	6.478643
5.715585	608.255938	6.483648
5.606730	620.140505	6.488653
5.905566	626.027671	6.493658
6.154057	621.583294	6.498662
6.185779	629.811741	6.503667
5.878102	622.700234	6.508672
6.461045	622.553622	6.513677
6.039342	619.458534	6.518682
6.042253	609.015995	6.523686
5.746875	619.066577	6.528691
5.964703	597.479350	6.533696
5.960931	603.235654	6.538701
6.108474	607.602687	6.543706
6.377921	602.408897	6.548710
5.682524	613.861709	6.553715
6.108116	605.072955	6.558720
6.223424	606.826219	6.563725
5.974555	609.686679	6.568730
5.844979	610.779340	6.573734
5.860518	614.762698	6.578739
6.068645	606.276955	6.583744
6.161973	608.733037	6.588749
6.178040	610.637912	6.593754
5.919838	599.195078	6.598758
5.480370	610.235298	6.603763
5.989821	604.144912	6.608768
6.137408	612.599459	6.613773
5.755085	607.687251	6.618778
6.117267	602.290829	6.623782
5.676486	612.442248	6.628787
5.727921	601.348546	6.633792
5.717083	607.263893	6.638797
5.762156	614.118405	6.643802
6.172281	615.341143	6.648806
5.678393	624.139909	6.653811
6.347460	624.858782	6.658816
6.101504	621.069949	6.663821
5.590768	610.970978	6.668826
6.095962	612.929250	6.673830
5.910619	632.679872	6.678835
5.837963	630.945079	6.683840
6.086165	635.567585	6.688845
6.124593	627.881140	6.693850
6.035320	619.683615	6.698854
5.643628	611.069460	6.703859
6.208928	611.445959	6.708864
5.897572	612.785007	6.713869
5.761683	619.606929	6.718874
6.316040	623.781292	6.723878
5.854640	620.749020	6.728883
5.837962	612.820492	6.733888
5.805929	616.333570	6.738893
6.239470	625.225049	6.743898
6.149241	621.990217	6.748902
5.833647	623.039481	6.753907
5.874114	604.593287	6.758912
5.876171	615.261626	6.763917
6.143641	622.969916	6.768922
6.454666	614.545080	6.773926
5.922051	623.852096	6.778931
6.040663	601.102576	6.783936
5.871186	621.421265	6.788941
5.888279	609.626565	6.793946
5.918919	603.193352	6.798950
6.149789	609.468095	6.803955
5.870056	601.245480	6.808960
6.153241	605.598933	6.813965
5.848762	608.343092	6.818970
5.981939	603.796055	6.823974
5.745530	616.862499	6.828979
6.120012	604.015605	6.833984
5.873520	612.864176	6.838989
5.992809	610.502224	6.843994
6.305883	606.642337	6.848998
5.911135	616.399348	6.854003
6.103493	607.836884	6.859008
5.994377	611.486655	6.864013
6.175346	613.788509	6.869018
6.071080	613.285425	6.874022
5.958284	617.397782	6.879027
6.019531	614.129384	6.884032
5.831648	604.169365	6.889037
5.953883	620.673502	6.894042
6.054704	612.415890	6.899046
6.145294	613.587342	6.904051
6.063854	602.469463	6.909056
5.870470	618.741690	6.914061
6.071003	612.493864	6.919066
5.975229	609.033208	6.924070
6.174444	612.453133	6.929075
6.345739	606.080696	6.934080
6.386478	608.636657	6.939085
6.086123	616.956592	6.944090
6.186403	604.405725	6.949094
5.975744	598.272368	6.954099
6.013187	594.955028	6.959104
5.873806	592.685838	6.964109
5.992903	596.367478	6.969114
5.983456	588.670232	6.974118
5.796102	591.332042	6.979123
6.022975	595.991616	6.984128
5.794909	592.901571	6.989133
6.007002	604.934269	6.994138
6.158337	608.350281	6.999142
6.111468	606.215552	7.004147
6.142635	586.200087	7.009152
5.886941	581.186997	7.014157
5.814046	573.741217	7.019162
6.075012	582.036862	7.024166
5.706874	575.446697	7.029171
6.134859	585.084230	7.034176
5.799700	590.209841	7.039181
6.051155	604.605292	7.044186
6.117414	605.887337	7.049190
5.584446	606.142973	7.054195
6.458519	595.712485	7.059200
6.212171	585.806561	7.064205
5.764236	576.434478	7.069210
6.300187	574.617859	7.074214
5.739337	575.571369	7.079219
5.849545	570.667998	7.084224
5.756536	577.398932	7.089229
5.869528	582.980389	7.094234
6.329341	592.335196	7.099238
5.885451	577.793303	7.104243
5.706051	579.269948	7.109248
5.708668	579.181146	7.114253
5.812068	594.180890	7.119258
6.204606	599.999051	7.124262
5.775792	601.287294	7.129267
6.143699	598.721172	7.134272
6.078459	605.565727	7.139277
6.208854	603.635101	7.144282
6.128351	587.901869	7.149286
5.790125	584.250872	7.154291
5.872044	578.424288	7.159296
5.715263	585.260706	7.164301
5.935779	604.345948	7.169306
6.223197	599.408884	7.174310
6.045972	615.487405	7.179315
5.633509	603.506901	7.184320
5.922003	603.970677	7.189325
6.029205	608.735322	7.194330
6.364435	605.184354	7.199334
5.870289	604.785693	7.204339
5.951456	593.706412	7.209344
6.198242	587.372198	7.214349
5.932256	582.929152	7.219354
5.985031	580.033361	7.224358
5.714957	587.218690	7.229363
5.914080	593.973287	7.234368
5.787252	606.881466	7.239373
6.083695	613.519116	7.244378
5.885837	615.795881	7.249382
5.719700	609.002738	7.254387
5.899158	608.478723	7.259392
6.054714	617.323675	7.264397
5.718998	614.344003	7.269402
6.318416	608.092489	7.274406
6.123304	615.796660	7.279411
6.209719	613.705180	7.284416
5.939089	611.185784	7.289421
5.648911	608.562865	7.294426
6.113953	605.838573	7.299430
5.957265	613.811868	7.304435
5.637755	608.970168	7.309440
5.793995	618.376837	7.314445
5.757476	627.408117	7.319450
5.771027	612.989167	7.324454
5.778966	616.023785	7.329459
5.991341	610.369179	7.334464
6.074790	607.339243	7.339469
5.843990	620.536190	7.344474
5.808518	616.475499	7.349478
5.855024	617.325086	7.354483
5.735258	613.460104	7.359488
5.891546	615.124095	7.364493
5.834057	618.535022	7.369498
6.122258	606.018159	7.374502
6.029837	610.581024	7.379507
6.279642	606.702999	7.384512
5.951099	599.884456	7.389517
6.109849	611.881591	7.394522
6.514726	609.551286	7.399526
5.931034	618.265854	7.404531
6.001004	614.883724	7.409536
6.079034	612.392241	7.414541
5.935333	616.989056	7.419546
6.231341	614.377609	7.424550
5.801449	614.421600	7.429555
5.864774	612.797892	7.434560
6.103595	612.459020	7.439565
5.817227	617.485191	7.444570
5.726050	608.338581	7.449574
5.663035	616.286302	7.454579
5.871198	615.096244	7.459584
5.902033	614.120260	7.464589
5.537634	618.805916	7.469594
5.997893	610.864326	7.474598
5.899452	614.958715	7.479603
5.922920	612.041920	7.484608
6.383067	605.229536	7.489613
6.305543	611.829649	7.494618
6.386145	603.844563	7.499622
6.054069	612.926550	7.504627
5.859334	612.709594	7.509632
6.338076	611.282522	7.514637
6.082489	617.610783	7.519642
6.354491	613.978717	7.524646
6.277174	604.284363	7.529651
5.790028	584.331834	7.534656
5.883043	577.993288	7.539661
5.672710	596.934960	7.544666
6.185103	599.172065	7.549670
5.982499	622.702436	7.554675
5.710743	611.662242	7.559680
6.043592	608.841829	7.564685
6.194450	611.061838	7.569690
6.162482	595.619336	7.574694
5.932399	593.988170	7.579699
5.957490	578.064988	7.584704
5.794943	573.821891	7.589709
5.866908	592.346207	7.594714
6.096977	596.956707	7.599718
5.799794	598.555475	7.604723
5.888326	609.875516	7.609728
6.028544	614.154566	7.614733
5.988292	617.336091	7.619738
5.988583	611.183388	7.624742
5.890085	622.396467	7.629747
5.974545	616.236534	7.634752
6.017985	614.698607	7.639757
5.638225	617.089165	7.644762
6.061927	609.245788	7.649766
6.110017	614.726309	7.654771
6.038139	609.895703	7.659776
5.918866	611.996057	7.664781
5.377136	622.972704	7.669786
6.098684	607.772867	7.674790
5.793099	615.070653	7.679795
6.037680	612.075606	7.684800
5.990784	614.137334	7.689805
5.656724	620.792954	7.694810
5.941560	607.303362	7.699814
5.696740	614.577469	7.704819
5.908490	611.469256	7.709824
6.002487	608.755292	7.714829
5.562452	612.025117	7.719834
5.958772	605.719220	7.724838
6.113286	617.102344	7.729843
5.786470	603.194042	7.734848
5.995399	608.835600	7.739853
6.411210	613.908108	7.744858
6.317126	614.596856	7.749862
6.131044	621.404396	7.754867
6.416069	616.257555	7.759872
6.475206	611.711132	7.764877
5.859683	606.652236	7.769882
6.104396	590.993422	7.774886
5.648360	592.617901	7.779891
5.686994	601.558180	7.784896
6.056154	607.961186	7.789901
5.877987	614.281165	7.794906
6.205344	608.275198	7.799910
5.889812	612.106957	7.804915
5.980084	607.047227	7.809920
6.404324	608.937600	7.814925
5.618941	606.200523	7.819930
6.001977	608.197375	7.824934
6.006850	612.361684	7.829939
6.218037	616.817048	7.834944
5.920128	604.494724	7.839949
5.775984	586.431177	7.844954
5.958958	602.312889	7.849958
5.973974	609.644020	7.854963
6.143734	609.753299	7.859968
6.339316	589.913866	7.864973
5.588754	589.708629	7.869978
5.801018	590.295538	7.874982
5.981979	612.423622	7.879987
6.211448	608.355965	7.884992
5.929800	603.035169	7.889997
5.747679	596.810454	7.895002
5.765791	597.213819	7.900006
5.920400	608.772356	7.905011
5.778132	609.598933	7.910016
5.625414	614.753347	7.915021
5.674525	612.933271	7.920026
6.060151	608.130118	7.925030
5.980231	615.163595	7.930035
5.746899	611.104290	7.935040
5.791097	616.089933	7.940045
5.856763	617.311493	7.945050
6.190191	614.252398	7.950054
6.060161	615.392891	7.955059
6.124047	616.754266	7.960064
5.825007	613.815292	7.965069
5.758842	614.711164	7.970074
5.807214	613.690835	7.975078
5.795878	617.804152	7.980083
5.461428	624.413660	7.985088
5.678135	614.433016	7.990093
5.636470	624.867845	7.995098
6.125346	633.013492	8.000102
6.327082	634.211930	8.005107
6.061147	636.723558	8.010112
6.024488	622.571614	8.015130
5.874414	629.718482	8.020147
5.888132	619.177959	8.025165
5.892686	615.827069	8.030182
5.866979	622.303778	8.035200
6.124393	624.113828	8.040218
5.997157	629.492463	8.045235
5.789001	628.049507	8.050253
6.183227	626.909928	8.055270
6.092855	631.584867	8.060288
6.310944	624.439018	8.065306
5.842624	622.527364	8.070323
6.226221	604.338107	8.075341
6.033755	618.652148	8.080358
6.039198	620.330113	8.085376
6.082870	619.873344	8.090394
5.949612	622.900766	8.095411
6.006580	615.687118	8.100429
5.991917	628.382460	8.105446
5.866069	621.138455	8.110464
6.168264	626.505820	8.115482
6.063037	633.923593	8.120499
6.365089	629.944737	8.125517
5.964496	622.645445	8.130534
6.125984	624.750495	8.135552
5.925531	612.911077	8.140570
6.114085	616.406042	8.145587
6.099950	628.300758	8.150605
6.144775	632.473420	8.155622
6.075738	629.687040	8.160640
6.503885	625.608570	8.165658
5.998303	621.496143	8.170675
5.982300	619.326927	8.175693
6.097063	625.281590	8.180710
6.062176	624.628394	8.185728
6.076661	624.401246	8.190746
6.111146	643.284124	8.195763
6.467201	632.397947	8.200781
6.268620	631.430540	8.205798
5.916417	620.945094	8.210816
6.140441	621.703263	8.215834
6.233533	635.627143	8.220851
6.233289	634.764680	8.225869
6.278733	631.623538	8.230886
6.077956	636.214011	8.235904
6.298579	627.142668	8.240922
5.976836	644.783830	8.245939
6.083902	644.548438	8.250957
6.125161	634.678498	8.255974
6.177611	648.336302	8.260992
6.111042	637.985427	8.266010
5.918454	651.846791	8.271027
6.030777	639.821515	8.276045
5.971396	637.387843	8.281062
5.975111	655.710512	8.286080
6.569021	652.954896	8.291098
5.821659	648.571886	8.296115
6.308098	644.157008	8.301133
6.266269	647.327159	8.306150
6.401215	651.391996	8.311168
6.212598	639.791330	8.316186
6.427593	645.940414	8.321203
6.698665	639.171982	8.326221
6.240369	642.154022	8.331238
5.906985	648.742314	8.336256
6.423545	647.463587	8.341274
6.304013	646.907078	8.346291
6.175502	639.871760	8.351309
6.342137	642.147604	8.356326
6.478791	647.132964	8.361344
6.299334	633.128184	8.366362
6.194687	643.811010	8.371379
6.187856	644.958958	8.376397
6.357617	648.554673	8.381414
6.218335	647.956949	8.386432
6.323220	639.231908	8.391450
6.355433	655.500384	8.396467
6.202692	647.878954	8.401485
6.064853	646.369238	8.406502
6.022677	653.571869	8.411520
6.407965	667.887918	8.416538
6.710209	669.357894	8.421555
6.624625	668.051715	8.426573
6.347427	647.208809	8.431590
6.407502	649.314909	8.436608
6.532174	640.257085	8.441626
6.152991	642.598112	8.446643
6.254215	651.851274	8.451661
6.779040	661.642529	8.456678
6.107481	668.326588	8.461696
6.540797	667.254939	8.466714
6.230796	674.117305	8.471731
6.499923	682.408883	8.476749
6.487056	674.851281	8.481766
6.371192	683.719175	8.486784
6.940723	677.099718	8.491802
6.639965	661.348965	8.496819
6.088722	653.737223	8.501837
6.510286	654.532364	8.506854
6.801589	669.073806	8.511872
6.865774	658.894561	8.516890
6.496006	649.200539	8.521907
6.386407	646.983435	8.526925
6.723541	649.782981	8.531942
6.445513	652.513534	8.536960
6.535617	651.519975	8.541978
6.222769	648.031491	8.546995
6.341635	645.220686	8.552013
6.659103	644.344194	8.557030
6.470299	662.672374	8.562048
6.874965	647.948456	8.567066
6.449941	637.497891	8.572083
6.433890	634.444485	8.577101
6.566347	638.137708	8.582119
6.765829	648.345795	8.587136
6.718794	631.988134	8.592154
6.452881	639.632504	8.597171
6.262625	644.860173	8.602189
6.313699	646.576842	8.607207
6.473291	665.263057	8.612224
6.631141	661.723005	8.617242
7.007995	672.561933	8.622259
6.557925	674.874155	8.627277
6.831652	678.110163	8.632295
6.816419	670.628542	8.637312
6.738400	650.847858	8.642330
6.275962	649.585185	8.647347
6.405889	669.224682	8.652365
6.551262	665.461906	8.657383
6.676025	677.305906	8.662400
6.789438	673.512596	8.667418
6.869653	677.300693	8.672435
6.685873	679.090898	8.677453
6.865859	663.370768	8.682471
6.518824	671.194324	8.687488
6.803834	673.273023	8.692506
7.043445	655.836046	8.697523
6.753757	647.540093	8.702541
6.994558	639.137407	8.707559
6.555853	643.675946	8.712576
6.649206	631.384543	8.717594
6.879236	636.751657	8.722611
6.585216	640.758396	8.727629
6.558387	638.733481	8.732647
6.486707	647.920789	8.737664
7.075066	659.636045	8.742682
7.023652	650.550289	8.747699
6.579120	644.790055	8.752717
6.881804	638.261648	8.757735
6.825308	640.700414	8.762752
6.772850	630.965278	8.767770
6.674568	638.377573	8.772787
6.451084	643.581611	8.777805
6.889134	639.802659	8.782823
6.436062	651.126612	8.787840
6.636965	658.226006	8.792858
6.962573	676.578071	8.797875
7.003537	674.167145	8.802893
7.089711	664.144482	8.807911
6.480652	670.808744	8.812928
6.840476	669.196936	8.817946
6.933364	669.722506	8.822963
6.535546	667.461398	8.827981
6.803611	670.668816	8.832999
6.476406	669.486892	8.838016
6.843230	673.207846	8.843034
7.136453	670.495324	8.848051
6.876022	671.108924	8.853069
7.121949	669.604160	8.858087
6.944509	670.394951	8.863104
6.812912	670.903759	8.868122
7.127910	680.146341	8.873139
6.770174	672.942285	8.878157
6.904992	672.740484	8.883175
6.563740	675.946442	8.888192
6.792276	670.824701	8.893210
7.087513	673.985497	8.898227
6.777957	671.884172	8.903245
6.806828	681.102879	8.908263
6.685575	680.921827	8.913280
6.774899	676.327436	8.918298
6.967203	663.303132	8.923315
6.934125	678.715568	8.928333
7.092735	670.200498	8.933351
7.056107	675.690122	8.938368
6.555682	671.731148	8.943386
7.001293	673.073849	8.948403
6.608776	672.662535	8.953421
7.058397	661.871861	8.958439
6.719571	678.297069	8.963456
6.845630	693.278076	8.968474
7.135073	698.843235	8.973491
7.213537	712.616466	8.978509
7.486894	700.475507	8.983527
6.833558	696.121006	8.988544
6.494484	688.376089	8.993562
7.173760	694.634524	8.998579
7.078801	700.201528	9.003597
7.395957	698.844011	9.008615
7.074811	699.318856	9.013632
6.686737	694.088592	9.018650
7.061429	700.872632	9.023667
7.011136	708.258905	9.028685
7.160795	699.277612	9.033703
6.937437	709.071533	9.038720
6.937262	701.410249	9.043738
7.203703	703.571155	9.048755
7.259979	713.984484	9.053773
7.318737	713.623634	9.058791
7.576709	703.113864	9.063808
7.461623	701.557858	9.068826
7.447158	683.988128	9.073843
7.283143	682.289054	9.078861
7.078665	675.590689	9.083879
7.004211	669.535322	9.088896
6.973029	671.873451	9.093914
7.318729	677.317089	9.098931
7.055882	678.085017	9.103949
7.244364	672.126653	9.108967
6.998643	679.142935	9.113984
6.878349	678.465298	9.119002
7.117979	685.862998	9.124019
7.281231	703.786496	9.129037
7.686166	690.252973	9.134055
7.154920	689.315057	9.139072
6.902229	675.969963	9.144090
7.026529	692.978301	9.149107
7.161595	708.022000	9.154125
7.372320	699.922275	9.159143
7.327872	708.653562	9.164160
7.063806	706.484466	9.169178
7.274088	702.562517	9.174195
7.433403	708.918472	9.179213
7.371162	699.340415	9.184231
7.414584	707.552064	9.189248
6.954880	714.258145	9.194266
7.346026	709.181116	9.199283
7.207735	707.717922	9.204301
7.430192	701.607473	9.209319
7.395981	693.872306	9.214336
7.300898	695.800966	9.219354
7.449195	702.591394	9.224371
6.858983	705.563008	9.229389
7.414622	695.766113	9.234407
7.315144	696.064891	9.239424
7.148687	703.486537	9.244442
7.349801	703.891438	9.249459
7.337437	704.815910	9.254477
7.401998	697.255319	9.259495
7.130613	696.295239	9.264512
6.877327	704.571763	9.269530
7.248947	706.446766	9.274547
7.229168	715.099567	9.279565
7.228354	702.986683	9.284583
7.209050	704.543369	9.289600
7.162126	727.865156	9.294618
7.337155	731.770237	9.299635
7.572523	737.657338	9.304653
7.542845	734.848674	9.309671
7.849092	728.661746	9.314688
7.218952	727.413844	9.319706
7.620095	730.144935	9.324723
7.574868	721.885624	9.329741
7.450356	711.340762	9.334759
7.407655	708.180344	9.339776
7.493042	717.840475	9.344794
7.929078	717.754535	9.349811
7.785519	707.695085	9.354829
7.747380	698.260273	9.359847
7.803693	703.515238	9.364864
7.261477	701.028838	9.369882
7.445546	697.294290	9.374899
7.322399	697.431249	9.379917
7.441035	694.332697	9.384935
7.566929	691.075078	9.389952
7.481149	698.034571	9.394970
7.760313	694.947230	9.399987
7.924983	706.577964	9.405005
7.565826	707.263422	9.410023
7.430994	705.021355	9.415040
7.342964	701.682629	9.420058
7.519099	699.130820	9.425075
7.377563	703.221375	9.430093
7.657265	697.087276	9.435111
7.595324	693.429290	9.440128
7.700278	704.366803	9.445146
7.592434	683.549740	9.450163
7.321452	701.422310	9.455181
7.580463	716.755712	9.460199
7.935144	732.503577	9.465216
7.418689	723.817991	9.470234
7.783626	721.475847	9.475251
7.500405	736.852994	9.480269
7.744378	733.847058	9.485287
7.765128	726.677937	9.490304
7.652274	731.942027	9.495322
7.791777	729.743109	9.500339
7.426999	738.625087	9.505357
7.719907	723.958183	9.510375
7.830941	729.507622	9.515392
7.765492	734.672924	9.520410
8.070541	726.795348	9.525427
7.609961	723.668297	9.530445
7.453651	713.802282	9.535463
7.850589	721.631011	9.540480
7.608788	739.282270	9.545498
7.682813	726.309780	9.550515
7.546772	736.101463	9.555533
7.403335	722.989798	9.560551
7.601711	732.963099	9.565568
7.668904	730.022655	9.570586
7.936368	730.954727	9.575603
7.887328	730.066089	9.580621
7.700405	731.197410	9.585639
7.969269	732.559147	9.590656
7.656349	727.262888	9.595674
7.715296	726.934287	9.600691
7.894493	732.814153	9.605709
7.469439	735.156098	9.610727
8.010862	739.568588	9.615744
7.696185	734.066723	9.620762
8.149231	726.378802	9.625779
7.989311	734.095426	9.630797
7.548255	735.497948	9.635815
7.588395	734.654775	9.640832
7.388410	741.869406	9.645850
7.542851	749.233607	9.650867
7.946488	758.707215	9.655885
7.843822	764.155445	9.660903
8.310701	766.113102	9.665920
8.090976	768.805676	9.670938
8.315232	755.827576	9.675955
8.100799	733.605340	9.680973
7.716923	739.544589	9.685991
7.942556	727.347735	9.691008
7.915500	731.724442	9.696026
8.065901	727.357703	9.701043
8.023889	726.340743	9.706061
8.050545	739.552532	9.711079
8.196386	717.230903	9.716096
8.206293	737.968250	9.721114
8.237045	726.802034	9.726131
8.200023	732.570467	9.731149
8.016477	734.322453	9.736167
8.082169	725.049949	9.741184
8.002059	736.488180	9.746202
8.155012	721.880671	9.751219
8.338491	721.272410	9.756237
7.814040	729.802498	9.761255
7.927012	719.026980	9.766272
8.025785	729.765153	9.771290
8.137872	737.226121	9.776307
8.208660	728.840121	9.781325
8.135064	733.278468	9.786343
8.046900	729.504350	9.791360
7.836146	731.994656	9.796378
8.049526	729.437463	9.801395
8.070511	722.868663	9.806413
7.906872	732.713336	9.811431
8.398071	724.601406	9.816448
8.210673	727.726389	9.821466
8.107938	728.815031	9.826483
8.425494	728.130636	9.831501
7.849035	732.255028	9.836519
8.246616	731.778234	9.841536
8.326149	723.529757	9.846554
8.432941	729.769622	9.851571
8.081235	728.408297	9.856589
7.618450	730.215575	9.861607
8.256693	720.869132	9.866624
8.387270	730.600130	9.871642
8.101415	733.070590	9.876659
8.324660	723.855458	9.881677
8.095199	733.010679	9.886695
8.034542	721.351758	9.891712
7.983833	738.931613	9.896730
8.162306	742.719991	9.901747
8.273708	750.581843	9.906765
8.199681	763.006432	9.911783
8.398940	762.716405	9.916800
8.204376	767.455091	9.921818
8.235222	767.941728	9.926835
8.471819	758.898764	9.931853
8.159281	755.892066	9.936871
8.233750	758.505217	9.941888
8.404597	754.403181	9.946906
8.167501	759.187095	9.951923
8.442613	758.097544	9.956941
8.391773	764.079288	9.961959
8.583609	758.780536	9.966976
8.509196	760.312103	9.971994
8.346146	761.611904	9.977011
8.291964	754.806732	9.982029
7.994235	761.880085	9.987047
8.462418	750.705589	9.992064
8.358421	754.023843	9.997082
8.329502	757.715864	10.002099
8.145651	753.235972	10.007117
8.347733	762.059137	10.012135
8.614602	764.212108	10.017152
8.318461	761.227496	10.022170
8.417217	765.297962	10.027187
8.629054	765.396775	10.032205
8.834150	762.322079	10.037223
8.420639	760.560771	10.042240
8.427432	752.222755	10.047258
8.590790	758.192650	10.052275
8.484202	756.830102	10.057293
8.405752	760.971639	10.062311
8.552643	748.854733	10.067328
8.626615	753.178498	10.072346
8.562738	764.887275	10.077363
8.702546	758.720021	10.082381
8.268600	771.024302	10.087399
8.299483	757.110558	10.092416
8.650986	769.704834	10.097434
8.065363	767.948404	10.102451
8.632878	755.465403	10.107469
8.320412	769.244759	10.112487
8.387672	756.321787	10.117504
8.300041	767.998675	10.122522
8.454976	765.370842	10.127539
8.486575	756.110657	10.132557
8.460373	761.741884	10.137575
8.335064	766.111249	10.142592
8.613659	778.232986	10.147610
8.600365	782.797575	10.152627
8.932919	789.994515	10.157645
8.455736	778.545853	10.162663
8.540466	786.016098	10.167680
8.555724	790.674775	10.172698
8.492305	798.821490	10.177715
8.924755	792.058551	10.182733
8.701320	799.733366	10.187751
8.817458	802.014445	10.192768
8.962343	787.197985	10.197786
8.604575	783.224809	10.202803
8.874832	773.231826	10.207821
8.433406	771.366484	10.212839
8.444537	777.178533	10.217856
8.725221	781.990883	10.222874
8.681433	790.359922	10.227891
8.803876	786.275341	10.232909
8.777087	780.363604	10.237927
8.821822	785.629964	10.242944
8.767762	791.709097	10.247962
8.715134	796.575463	10.252979
9.071582	787.015419	10.257997
8.634850	784.411543	10.263015
8.445633	785.510573	10.268032
8.479251	790.405566	10.273050
8.446751	794.104095	10.278067
8.765639	786.618663	10.283085
8.355809	784.060724	10.288103
8.876041	788.388159	10.293120
9.013692	784.533725	10.298138
8.813218	781.965528	10.303155
9.005715	785.866548	10.308173
9.148752	786.602310	10.313191
8.811067	791.091883	10.318208
8.901022	792.557656	10.323226
8.833809	790.830730	10.328243
9.096430	789.540501	10.333261
9.076955	789.761469	10.338279
8.968727	788.333052	10.343296
9.016516	783.553391	10.348314
8.726129	796.395702	10.353331
8.954777	784.733708	10.358349
9.084927	795.112420	10.363367
9.253125	789.604983	10.368384
9.417548	783.441517	10.373402
9.179963	786.096503	10.378419
9.256874	777.040602	10.383437
8.923101	782.934565	10.388455
8.829238	792.257514	10.393472
9.259546	786.827930	10.398490
8.797673	786.293459	10.403507
9.077548	776.394153	10.408525
8.957061	774.731559	10.413543
9.052658	781.675228	10.418560
9.066213	784.132731	10.423578
8.636380	785.741262	10.428595
8.857334	791.473693	10.433613
8.776299	781.362112	10.438631
9.114451	783.582805	10.443648
8.916858	784.619839	10.448666
8.783342	783.889666	10.453683
8.908101	784.903636	10.458701
9.176620	805.918313	10.463719
9.472017	808.205142	10.468736
9.605461	795.742019	10.473754
9.234673	788.540463	10.478771
9.522917	784.450867	10.483789
9.531148	786.369124	10.488807
9.305398	782.886265	10.493824
9.500570	778.908140	10.498842
9.311103	781.660269	10.503859
9.379341	780.325854	10.508877
9.183770	776.704541	10.513895
9.194033	781.600250	10.518912
9.323038	779.369994	10.523930
9.207032	775.061528	10.528947
9.410719	773.485012	10.533965
9.192394	783.617892	10.538983
9.517824	776.105793	10.544000
9.348335	776.002802	10.549018
9.363551	781.044927	10.554035
9.637867	775.743927	10.559053
9.051027	757.017780	10.564071
9.262007	769.575092	10.569088
9.419582	766.455905	10.574106
9.189275	765.096126	10.579123
9.302631	771.591994	10.584141
9.286856	782.784580	10.589159
9.132268	774.133135	10.594176
9.366913	772.511732	10.599194
9.200286	785.926028	10.604211
9.390736	780.495221	10.609229
9.439087	784.427983	10.614247
9.488549	777.111966	10.619264
9.532595	778.640848	10.624282
9.065926	786.646467	10.629299
9.198261	780.962698	10.634317
9.338131	782.034793	10.639335
9.311855	784.909499	10.644352
9.240220	775.856937	10.649370
9.357283	775.460842	10.654387
9.620291	775.497642	10.659405
9.190972	784.931642	10.664423
9.111873	776.349582	10.669440
9.284183	776.088425	10.674458
9.176029	776.460684	10.679475
9.041520	778.189989	10.684493
9.259070	795.457393	10.689511
9.333451	810.956886	10.694528
9.738352	812.464994	10.699546
9.481508	811.462736	10.704563
9.241522	813.609882	10.709581
9.273224	815.670312	10.714599
9.174378	815.648138	10.719616
9.617641	807.487413	10.724634
9.396929	816.454629	10.729651
9.622152	817.633846	10.734669
9.541164	810.637430	10.739687
9.380497	817.570796	10.744704
9.337530	807.161965	10.749722
9.358869	817.909871	10.754739
9.537620	812.033770	10.759757
9.636954	824.793463	10.764775
9.534985	850.541352	10.769792
9.722287	842.550544	10.774810
9.678862	847.498862	10.779827
9.892726	838.154908	10.784845
9.855611	826.848290	10.789863
9.667808	823.889425	10.794880
9.733222	812.488680	10.799898
9.516800	815.593685	10.804915
9.691481	810.784344	10.809933
9.651540	807.266774	10.814951
9.505947	819.732785	10.819968
9.961743	826.057017	10.824986
9.850872	846.167298	10.830003
10.104477	831.122175	10.835021
9.930317	817.055724	10.840039
10.116499	818.731144	10.845056
9.724682	811.829894	10.850074
9.435872	819.730492	10.855091
9.420748	812.084620	10.860109
9.657924	804.717036	10.865127
9.743245	827.550171	10.870144
9.843547	836.291811	10.875162
9.812628	853.215009	10.880179
10.112237	837.646934	10.885197
9.996565	830.599955	10.890215
9.558098	829.665170	10.895232
9.850997	831.276073	10.900250
10.004278	852.196514	10.905267
9.859083	847.163764	10.910285
10.201975	845.394121	10.915303
9.646526	836.166531	10.920320
10.013370	836.680207	10.925338
10.226648	841.294693	10.930355
9.658946	822.897957	10.935373
10.076372	822.324179	10.940391
9.611039	826.071945	10.945408
10.008880	834.134035	10.950426
10.128694	850.293332	10.955443
10.172298	848.346092	10.960461
9.954462	827.451777	10.965479
9.801825	826.681857	10.970496
10.205620	829.547953	10.975514
10.117885	824.804106	10.980531
9.921382	824.506779	10.985549
10.150368	828.591916	10.990567
10.205302	833.070817	10.995584
10.009881	816.468647	11.000602
9.813580	824.473215	11.005619
10.030842	837.716121	11.010637
10.208736	832.502325	11.015655
10.184398	851.887297	11.020672
10.098621	842.900815	11.025690
10.415603	841.177586	11.030707
10.124760	826.972974	11.035725
10.112223	809.668517	11.040743
9.789784	817.834512	11.045760
10.360505	823.773591	11.050778
10.068099	829.152087	11.055795
9.809863	843.329595	11.060813
10.087474	842.280961	11.065831
10.313895	848.659719	11.070848
10.413066	847.320963	11.075866
10.436930	848.824849	11.080883
9.994030	842.171402	11.085901
9.924768	843.548588	11.090919
9.963105	861.377998	11.095936
10.348695	849.428564	11.100954
10.310818	858.405291	11.105971
10.437248	854.656236	11.110989
10.565877	853.953515	11.116007
10.185545	856.108553	11.121024
10.242742	857.794706	11.126042
10.376877	854.486478	11.131059
10.275021	858.067772	11.136077
10.172506	852.125636	11.141095
10.237749	846.722625	11.146112
10.352922	855.249620	11.151130
10.302405	858.828319	11.156147
9.988472	860.800718	11.161165
9.908503	853.534441	11.166183
9.854767	856.253085	11.171200
9.937595	850.027911	11.176218
10.312223	854.050358	11.181235
10.309460	857.004644	11.186253
10.434521	855.012027	11.191271
9.982635	859.423683	11.196288
10.199155	874.428073	11.201306
10.486673	880.368401	11.206323
10.579274	895.679144	11.211341
10.314848	882.890906	11.216359
10.351597	894.519342	11.221376
10.508828	888.096014	11.226394
10.579349	890.317734	11.231411
10.526436	892.108340	11.236429
10.786013	884.593708	11.241447
10.486369	883.403660	11.246464
10.640257	884.597845	11.251482
10.731268	884.782411	11.256499
10.626370	887.234349	11.261517
10.810656	860.541003	11.266535
10.463358	861.418982	11.271552
10.465246	858.602313	11.276570
10.420459	857.325581	11.281587
10.121571	862.322897	11.286605
10.509441	874.654164	11.291623
10.460872	887.397456	11.296640
10.825682	888.126421	11.301658
10.859338	883.718737	11.306675
10.861716	897.692518	11.311693
10.804192	875.227966	11.316711
10.682106	886.505550	11.321728
10.649437	879.301898	11.326746
10.486524	874.333881	11.331763
10.385622	882.208121	11.336781
10.552358	882.743516	11.341799
10.699104	885.512823	11.346816
10.674967	885.147586	11.351834
10.924747	879.406147	11.356851
10.784647	889.606060	11.361869
10.681650	882.482159	11.366887
10.558927	887.073953	11.371904
10.506687	892.308770	11.376922
10.674436	884.614472	11.381939
10.563674	897.862928	11.386957
10.397707	884.453690	11.391975
10.777828	883.660901	11.396992
10.519411	892.053330	11.402010
10.781865	884.006752	11.407027
10.224183	897.605970	11.412045
10.654830	896.768595	11.417063
10.585204	909.855534	11.422080
10.645605	918.482967	11.427098
10.983515	923.308720	11.432115
11.196551	918.727235	11.437133
11.041866	913.406285	11.442151
11.297506	913.134477	11.447168
10.972550	911.720676	11.452186
11.183094	897.207005	11.457203
10.746478	896.332536	11.462221
11.035731	875.415998	11.467239
11.129058	883.251778	11.472256
10.578774	878.625842	11.477274
11.123613	885.211719	11.482291
10.779157	890.389416	11.487309
11.192375	893.008700	11.492327
11.318699	892.291792	11.497344
11.044737	884.706065	11.502362
11.098363	885.109410	11.507379
10.866065	878.792317	11.512397
10.940699	878.288683	11.517415
10.970005	887.804276	11.522432
11.012483	886.607969	11.527450
10.990318	895.049071	11.532467
10.928515	913.815944	11.537485
11.109583	911.127464	11.542503
11.315640	908.194700	11.547520
11.220475	909.925378	11.552538
10.984092	896.409290	11.557555
10.883169	902.719838	11.562573
11.147583	915.294798	11.567591
11.121284	913.740997	11.572608
11.096684	909.931901	11.577626
11.243088	907.801103	11.582643
11.229987	913.028266	11.587661
11.060737	908.416783	11.592679
11.406398	918.395341	11.597696
11.342622	920.386953	11.602714
11.363232	905.460649	11.607731
11.270958	908.548659	11.612749
11.061706	914.177182	11.617767
11.377295	912.973443	11.622784
11.214050	914.884679	11.627802
11.304079	909.225584	11.632819
11.100323	910.352619	11.637837
11.291559	914.573158	11.642855
11.336838	902.439494	11.647872
11.298121	911.730550	11.652890
11.599318	907.786015	11.657907
11.356463	910.769044	11.662925
11.010782	902.182633	11.667943
11.116226	902.178598	11.672960
10.982532	915.104504	11.677978
10.865740	907.202990	11.682995
11.234161	916.169952	11.688013
11.534588	918.811460	11.693031
11.296693	917.467884	11.698048
11.301395	921.544517	11.703066
11.348667	913.084363	11.708083
11.128565	915.386097	11.713101
11.220040	925.390215	11.718119
11.670193	931.983524	11.723136
11.433453	948.973583	11.728154
11.907472	945.548430	11.733171
11.667170	928.722874	11.738189
11.535760	924.160235	11.743207
11.444888	914.922991	11.748224
11.451940	922.451831	11.753242
11.520424	909.589156	11.758259
11.328419	915.543548	11.763277
11.515888	929.617413	11.768295
11.779596	937.524609	11.773312
11.440240	924.773546	11.778330
11.747450	923.513716	11.783347
11.884961	915.092553	11.788365
11.492724	916.472047	11.793383
11.463911	914.901340	11.798400
11.227587	922.655117	11.803418
11.682618	924.725381	11.808435
12.039185	936.035156	11.813453
11.695067	926.033969	11.818471
11.984568	913.033517	11.823488
11.840350	911.617346	11.828506
12.013174	907.713753	11.833523
11.733539	911.271349	11.838541
11.797295	907.483449	11.843559
11.658722	902.935388	11.848576
11.438952	904.415451	11.853594
11.497499	904.375483	11.858611
11.637415	905.380259	11.863629
11.789102	909.591991	11.868647
11.795851	901.958593	11.873664
11.613144	911.998261	11.878682
11.730839	923.718035	11.883699
11.785062	934.055871	11.888717
11.828683	944.198628	11.893735
11.879715	939.924266	11.898752
11.527025	937.811149	11.903770
12.130440	937.262080	11.908787
11.966906	948.854038	11.913805
11.917234	944.778231	11.918823
12.071194	933.111172	11.923840
11.909330	940.899870	11.928858
12.086218	932.749330	11.933875
12.030115	923.433099	11.938893
11.841598	922.509279	11.943911
11.691075	915.344416	11.948928
11.789103	939.648772	11.953946
12.019252	940.701599	11.958963
12.223470	944.701896	11.963981
12.087151	951.401772	11.968999
11.842987	947.440449	11.974016
11.968815	947.794834	11.979034
11.952157	939.285411	11.984051
11.937066	944.340481	11.989069
12.034474	950.136339	11.994087
12.386757	944.983783	11.999104
12.394963	945.983600	12.004122
12.396042	934.190680	12.009139
12.152812	915.742861	12.014157
11.897521	907.919003	12.019175
12.174207	914.334344	12.024192
12.039565	917.538815	12.029210
11.954973	915.044316	12.034227
12.184910	923.751155	12.039245
11.949873	944.216359	12.044263
12.259085	941.200369	12.049280
12.246315	937.958180	12.054298
12.096794	937.244822	12.059315
11.999049	946.708658	12.064333
11.955316	950.529550	12.069351
12.227658	936.111510	12.074368
12.270735	952.180476	12.079386
12.246634	939.006743	12.084403
12.273495	942.026609	12.089421
12.123688	946.848092	12.094439
12.456523	938.644562	12.099456
12.274818	950.034422	12.104474
12.613301	935.505435	12.109491
12.464611	944.691104	12.114509
12.502088	947.884797	12.119527
12.570983	936.311738	12.124544
12.361853	950.041073	12.129562
12.524168	943.888522	12.134579
12.308743	937.507196	12.139597
12.302252	940.052685	12.144615
12.536560	938.948620	12.149632
12.147504	949.214597	12.154650
12.180323	945.756992	12.159667
12.227928	942.851640	12.164685
12.187854	949.416293	12.169703
12.353655	945.314649	12.174720
12.227522	946.145774	12.179738
12.366311	937.701160	12.184755
12.450682	938.704113	12.189773
12.281844	945.580623	12.194791
12.386004	936.046517	12.199808
12.314037	945.345854	12.204826
12.285609	947.973714	12.209843
12.390959	937.275288	12.214861
12.377160	947.067728	12.219879
12.382774	958.369886	12.224896
12.598136	979.278251	12.229914
12.227733	976.263769	12.234931
12.708297	975.039795	12.239949
12.232837	975.948843	12.244967
12.794525	958.927074	12.249984
12.710657	974.781660	12.255002
12.816126	974.422124	12.260019
12.715420	967.969823	12.265037
12.622318	976.455784	12.270055
12.825943	976.573282	12.275072
12.362229	987.100848	12.280090
12.965904	976.916705	12.285107
12.684011	978.155498	12.290125
12.430095	983.549325	12.295143
12.652172	972.924062	12.300160
12.541776	979.239359	12.305178
12.145576	975.144943	12.310195
12.764122	970.162847	12.315213
12.665785	974.465995	12.320231
12.712906	964.961000	12.325248
12.482532	981.548089	12.330266
12.656604	995.519118	12.335283
12.767351	1001.827726	12.340301
12.818357	1010.983124	12.345319
12.961865	1003.997083	12.350336
12.950343	1004.282483	12.355354
12.891974	1007.643627	12.360371
13.043631	999.788557	12.365389
12.862101	1000.708382	12.370407
12.733142	997.532268	12.375424
12.956748	1005.632353	12.380442
13.319210	998.767533	12.385459
13.581327	993.788152	12.390477
12.914282	990.083840	12.395495
12.935869	975.273051	12.400512
12.914792	983.021137	12.405530
12.828274	981.213138	12.410547
13.013599	982.597785	12.415565
13.082375	999.896745	12.420583
12.936952	993.293183	12.425600
13.068402	999.476320	12.430618
12.888443	1000.248254	12.435635
12.874684	997.546351	12.440653
13.014705	1006.044906	12.445671
13.010159	989.703847	12.450688
13.186085	994.490699	12.455706
13.270112	1001.435202	12.460723
13.411458	1000.912645	12.465741
12.893525	997.948964	12.470759
13.076647	992.470874	12.475776
13.408943	995.926376	12.480794
13.168050	992.743995	12.485811
13.350871	988.041121	12.490829
13.493091	996.396793	12.495847
13.211040	989.265485	12.500864
13.359224	1003.567172	12.505882
12.991781	997.342484	12.510899
13.352347	987.613533	12.515917
13.474678	999.961311	12.520935
13.260694	991.076677	12.525952
13.130792	992.197787	12.530970
13.105425	993.058291	12.535987
13.523101	996.263444	12.541005
12.914833	1004.563476	12.546023
13.284908	995.728579	12.551040
13.576881	991.419424	12.556058
13.403308	998.774675	12.561075
13.301326	995.211039	12.566093
13.183364	998.962742	12.571111
13.461986	1001.811804	12.576128
13.502330	995.242045	12.581146
13.316196	1000.587255	12.586163
13.755182	989.359552	12.591181
13.624714	995.482125	12.596199
13.322182	998.022708	12.601216
13.640046	998.798427	12.606234
13.393921	1000.993070	12.611251
13.746643	996.773063	12.616269
13.521272	1000.677979	12.621287
13.521686	999.775231	12.626304
13.576856	1002.303434	12.631322
13.615003	1000.337787	12.636339
13.697282	992.396575	12.641357
13.525350	1004.277749	12.646375
13.722465	995.132529	12.651392
13.695143	1002.778906	12.656410
13.759995	997.332602	12.661427
13.871184	998.190967	12.666445
13.717121	1001.168758	12.671463
13.669117	996.476938	12.676480
13.722362	995.226480	12.681498
13.745318	1007.989916	12.686515
13.866684	1000.122933	12.691533
13.956308	1004.325284	12.696551
13.802571	988.637644	12.701568
13.353038	977.675179	12.706586
13.495039	995.608832	12.711603
13.859955	997.781033	12.716621
13.524438	998.970441	12.721639
13.700099	1002.247165	12.726656
13.652246	1000.513467	12.731674
13.420469	1007.748444	12.736691
13.568447	998.134212	12.741709
13.553824	994.511231	12.746727
13.276262	998.430694	12.751744
13.591368	1008.485234	12.756762
13.882099	1021.362209	12.761779
13.822891	1029.181983	12.766797
13.566351	1034.086124	12.771815
13.613003	1036.448820	12.776832
13.969253	1025.290694	12.781850
13.753957	1037.521187	12.786867
13.948023	1024.068746	12.791885
13.927115	1022.316411	12.796903
13.909756	1034.634594	12.801920
14.023333	1029.961676	12.806938
13.850714	1034.594451	12.811955
14.105234	1032.200075	12.816973
13.998854	1041.993338	12.821991
13.929626	1025.463747	12.827008
13.954999	1019.899174	12.832026
13.808136	1036.835471	12.837043
13.798850	1024.488709	12.842061
13.826388	1041.146930	12.847079
13.938926	1050.800017	12.852096
13.957772	1054.488137	12.857114
13.925538	1059.375616	12.862131
14.250129	1051.554087	12.867149
14.390239	1052.587186	12.872167
14.236861	1057.716370	12.877184
14.440759	1062.523020	12.882202
14.400177	1063.163220	12.887219
14.449205	1053.000399	12.892237
14.381756	1053.221836	12.897255
14.232889	1049.921847	12.902272
14.175529	1046.651980	12.907290
14.279084	1054.296002	12.912307
14.476667	1055.281791	12.917325
14.297487	1048.496007	12.922343
14.485436	1045.588656	12.927360
14.450856	1032.352014	12.932378
14.184208	1028.340852	12.937395
14.335948	1018.129158	12.942413
14.527127	1035.193724	12.947431
13.974662	1031.943246	12.952448
14.425013	1039.204653	12.957466
14.447678	1057.827404	12.962483
14.634795	1045.023316	12.967501
14.543506	1054.586539	12.972519
14.260991	1052.299981	12.977536
14.542502	1053.642725	12.982554
14.182347	1055.499183	12.987571
14.638476	1052.730882	12.992589
14.687749	1054.311680	12.997607
14.495503	1053.294379	13.002624
14.782522	1051.712698	13.007642
14.421584	1052.841361	13.012659
14.691283	1051.041690	13.017677
14.416119	1053.238393	13.022695
14.301667	1054.221128	13.027712
14.180329	1052.885404	13.032730
14.556312	1061.563414	13.037747
14.327700	1059.219900	13.042765
14.541295	1055.073700	13.047783
14.289422	1059.279464	13.052800
14.460847	1053.672586	13.057818
14.381401	1057.725787	13.062835
14.352269	1060.144735	13.067853
14.872682	1083.036118	13.072871
14.720926	1087.298932	13.077888
15.049919	1089.388515	13.082906
14.846996	1091.796482	13.087923
14.784436	1074.727563	13.092941
14.851199	1065.429089	13.097959
14.473555	1057.120709	13.102976
15.084509	1074.494143	13.107994
15.103554	1088.081491	13.113011
15.180919	1056.663948	13.118029
15.034700	1055.726030	13.123047
15.036243	1051.199212	13.128064
14.951708	1050.209743	13.133082
14.667717	1051.434322	13.138099
14.901339	1050.418549	13.143117
14.586107	1047.650025	13.148135
14.813790	1053.719615	13.153152
14.964441	1044.521826	13.158170
14.768847	1044.114112	13.163187
14.630510	1061.520661	13.168205
14.835470	1064.401222	13.173223
14.753006	1080.676534	13.178240
15.298098	1072.235040	13.183258
15.025098	1075.931727	13.188275
15.154057	1082.067280	13.193293
15.261808	1073.151765	13.198311
15.239373	1086.464494	13.203328
15.576009	1075.061557	13.208346
14.889065	1059.414500	13.213363
14.956080	1058.979837	13.218381
14.996010	1061.327509	13.223399
14.929143	1072.461443	13.228416
15.423491	1072.362305	13.233434
15.220609	1080.763749	13.238451
15.473905	1077.676286	13.243469
15.410878	1074.067994	13.248487
14.789156	1062.891075	13.253504
14.636938	1067.855115	13.258522
14.617874	1083.392794	13.263539
14.511452	1084.961187	13.268557
15.051124	1081.860162	13.273575
14.797735	1087.088983	13.278592
15.033874	1089.273860	13.283610
15.254715	1094.553682	13.288627
15.604945	1098.579446	13.293645
15.583714	1097.316116	13.298663
15.548589	1093.511867	13.303680
15.299138	1105.205173	13.308698
15.617497	1094.716242	13.313715
15.369266	1096.591179	13.318733
15.319213	1101.377689	13.323751
14.836661	1106.964530	13.328768
15.561975	1090.384012	13.333786
15.510380	1096.870716	13.338803
15.335131	1103.573561	13.343821
15.345276	1105.779720	13.348839
15.109767	1097.942253	13.353856
15.526141	1095.797042	13.358874
15.792382	1099.239097	13.363891
15.657567	1096.004485	13.368909
15.531845	1103.542801	13.373927
15.437475	1108.846082	13.378944
15.686156	1094.261347	13.383962
15.388923	1100.244257	13.388979
15.082821	1092.249985	13.393997
15.535467	1091.893194	13.399015
15.143105	1101.100012	13.404032
15.403339	1113.961643	13.409050
15.771448	1125.329092	13.414067
16.036499	1125.792313	13.419085
16.274826	1120.838484	13.424103
16.139266	1114.588343	13.429120
16.078892	1095.482888	13.434138
16.138438	1091.381084	13.439155
15.816510	1082.496554	13.444173
15.964973	1093.510994	13.449191
15.608759	1085.246292	13.454208
15.953484	1082.311006	13.459226
16.169393	1089.008522	13.464243
16.094370	1086.039592	13.469261
15.814881	1083.946616	13.474279
15.554748	1093.333497	13.479296
16.016619	1094.303478	13.484314
15.918700	1096.696815	13.489331
16.083132	1101.687958	13.494349
16.273248	1091.992284	13.499367
16.021369	1096.523639	13.504384
16.034062	1080.842205	13.509402
16.135768	1085.549646	13.514419
15.870806	1082.486582	13.519437
15.746121	1087.815348	13.524455
15.877319	1083.861912	13.529472
15.729593	1084.569459	13.534490
16.079613	1084.132027	13.539507
15.818531	1085.392577	13.544525
15.920655	1083.409634	13.549543
15.825095	1092.111413	13.554560
16.036785	1083.840468	13.559578
16.289515	1084.162033	13.564595
16.059439	1084.989511	13.569613
16.092297	1084.980961	13.574631
15.906140	1086.212964	13.579648
16.377691	1084.951105	13.584666
16.153134	1091.761712	13.589683
16.284736	1085.922842	13.594701
16.436358	1081.312111	13.599719
16.321997	1087.893453	13.604736
16.358853	1084.697345	13.609754
16.329535	1086.122661	13.614771
16.270226	1088.356459	13.619789
16.589290	1082.539303	13.624807
16.211743	1085.236017	13.629824
16.007539	1089.900809	13.634842
16.164611	1088.829207	13.639859
16.355376	1108.437929	13.644877
16.631149	1107.640362	13.649895
16.837249	1113.897795	13.654912
16.695502	1098.211602	13.659930
16.660717	1087.516592	13.664947
16.410786	1093.878268	13.669965
16.498563	1087.810441	13.674983
16.694767	1078.455488	13.680000
16.677532	1082.295646	13.685018
16.678252	1077.422512	13.690035
16.611355	1079.675281	13.695053
16.569187	1081.760575	13.700071
16.393104	1082.393687	13.705088
16.443247	1078.193446	13.710106
16.440713	1075.699507	13.715123
16.204812	1087.583857	13.720141
16.127686	1080.150473	13.725159
16.509062	1104.893193	13.730176
16.548955	1110.485257	13.735194
16.533007	1117.156218	13.740211
16.360048	1117.837238	13.745229
16.911313	1117.265304	13.750247
16.531200	1126.718133	13.755264
16.935115	1118.269676	13.760282
16.885516	1117.267332	13.765299
16.381414	1119.472426	13.770317
16.707888	1117.095255	13.775335
16.680891	1116.916700	13.780352
16.575187	1123.133251	13.785370
16.755297	1110.746791	13.790387
16.647798	1112.351979	13.795405
16.267886	1117.993873	13.800423
16.436373	1126.404713	13.805440
16.544998	1132.744434	13.810458
16.713314	1144.285133	13.815475
16.590961	1151.818190	13.820493
17.213126	1139.145524	13.825511
17.371732	1138.619317	13.830528
17.311446	1149.666000	13.835546
17.530864	1144.035394	13.840563
17.424164	1149.528521	13.845581
17.522929	1122.987070	13.850599
17.044960	1119.069928	13.855616
17.304253	1121.883632	13.860634
17.400846	1105.646959	13.865651
17.102712	1112.672114	13.870669
17.330060	1107.459092	13.875687
17.325544	1109.243677	13.880704
17.086833	1113.905529	13.885722
17.203684	1100.449667	13.890739
16.772041	1117.840674	13.895757
16.952667	1102.121963	13.900775
17.002343	1104.687312	13.905792
16.691763	1120.049682	13.910810
16.883016	1113.415517	13.915827
17.097551	1127.615390	13.920845
17.354524	1136.496608	13.925863
17.391576	1145.116617	13.930880
17.312910	1144.478915	13.935898
17.313091	1135.640622	13.940915
17.322977	1147.803601	13.945933
17.441471	1132.814022	13.950951
17.139982	1141.733779	13.955968
17.335493	1144.590330	13.960986
17.389691	1133.927403	13.966003
17.169487	1144.980091	13.971021
17.389856	1142.688987	13.976039
17.700404	1145.316655	13.981056
17.379033	1152.159854	13.986074
17.344768	1139.083694	13.991091
17.390707	1148.903770	13.996109
17.485138	1142.957257	14.001127
17.201296	1147.136450	14.006144
17.323959	1138.903052	14.011162
17.519508	1135.005087	14.016179
17.397133	1142.889707	14.021197
17.541666	1146.151537	14.026215
17.717422	1137.175513	14.031232
17.045128	1145.863374	14.036250
17.712153	1160.228502	14.041267
17.639520	1175.317677	14.046285
17.919425	1173.044663	14.051303
18.013096	1169.844641	14.056320
17.764729	1162.674211	14.061338
17.840804	1149.789214	14.066355
17.738503	1142.241469	14.071373
17.620821	1145.883322	14.076391
17.954407	1148.036324	14.081408
17.835046	1155.177561	14.086426
17.843281	1137.642534	14.091443
17.563652	1144.683536	14.096461
17.786847	1160.110313	14.101479
17.977617	1164.092816	14.106496
17.698057	1177.405287	14.111514
18.183842	1174.032072	14.116531
17.756635	1173.220986	14.121549
17.964650	1172.115747	14.126567
17.952454	1172.784322	14.131584
17.784875	1166.586705	14.136602
18.135158	1174.684012	14.141619
17.820376	1182.702871	14.146637
17.984905	1173.203110	14.151655
18.008714	1177.659706	14.156672
17.866906	1187.888442	14.161690
18.160789	1174.321709	14.166707
18.103487	1174.788704	14.171725
18.042390	1171.121409	14.176743
18.306976	1171.019766	14.181760
17.988046	1178.308228	14.186778
18.074583	1174.119652	14.191795
18.180494	1175.646597	14.196813
18.004668	1163.772562	14.201831
18.327667	1171.765334	14.206848
17.917650	1176.469349	14.211866
18.070611	1164.412135	14.216883
18.236381	1169.292453	14.221901
18.050692	1176.824986	14.226919
18.445144	1167.098580	14.231936
18.037316	1170.397942	14.236954
18.315449	1176.550563	14.241971
18.089593	1170.659042	14.246989
18.174269	1193.520381	14.252007
18.674110	1196.271041	14.257024
18.263766	1191.905687	14.262042
18.581351	1185.147032	14.267059
18.634686	1190.458167	14.272077
18.593067	1177.682789	14.277095
18.818034	1169.385980	14.282112
18.473783	1164.347111	14.287130
18.538011	1160.167351	14.292147
18.531480	1171.699621	14.297165
18.373727	1168.786106	14.302183
18.690786	1162.825162	14.307200
18.317090	1176.576829	14.312218
18.701909	1172.519566	14.317235
18.649372	1174.055031	14.322253
18.880438	1165.444231	14.327271
18.618583	1163.086126	14.332288
18.606181	1171.398994	14.337306
18.717009	1166.432405	14.342323
18.605847	1169.440525	14.347341
18.664389	1181.845860	14.352359
18.899411	1189.557942	14.357376
18.720900	1190.358778	14.362394
18.990850	1186.912641	14.367411
18.651394	1173.971236	14.372429
18.598120	1188.738329	14.377447
19.188358	1194.802271	14.382464
19.005219	1185.717541	14.387482
18.697577	1169.205226	14.392499
18.822621	1177.450852	14.397517
18.733000	1190.540156	14.402535
18.879992	1183.064889	14.407552
19.010732	1192.881188	14.412570
19.048186	1185.272881	14.417587
19.048146	1193.346318	14.422605
19.197167	1189.173769	14.427623
19.379749	1181.653634	14.432640
18.914072	1185.565317	14.437658
19.039181	1165.656643	14.442675
18.902774	1174.714039	14.447693
18.906214	1182.934923	14.452711
18.992468	1189.378368	14.457728
18.962361	1186.578355	14.462746
19.494078	1191.726029	14.467763
19.575469	1190.235074	14.472781
19.309714	1186.452850	14.477799
19.252159	1168.173585	14.482816
18.946028	1177.108304	14.487834
19.210535	1173.620946	14.492851
19.325472	1189.528263	14.497869
19.107564	1189.447065	14.502887
19.298077	1189.676182	14.507904
19.068462	1195.537305	14.512922
18.825306	1194.178040	14.517939
19.180604	1187.028899	14.522957
19.150386	1198.424564	14.527975
19.196307	1185.957905	14.532992
19.141722	1189.958994	14.538010
19.126765	1193.216536	14.543027
19.365371	1192.310162	14.548045
19.300372	1193.918557	14.553063
19.409367	1187.585768	14.558080
19.231399	1193.300153	14.563098
19.256671	1212.439179	14.568115
19.552263	1223.065973	14.573133
19.359752	1232.643703	14.578151
19.615611	1218.668671	14.583168
19.522300	1220.771114	14.588186
19.741866	1220.978491	14.593203
19.674257	1220.800754	14.598221
19.424757	1218.213830	14.603239
19.809453	1214.027053	14.608256
19.692099	1218.763721	14.613274
19.881182	1220.204459	14.618291
19.489372	1215.169906	14.623309
19.578450	1216.379178	14.628327
20.015249	1215.502582	14.633344
19.857304	1221.167601	14.638362
20.196265	1222.833122	14.643379
19.809289	1210.155454	14.648397
19.697357	1221.980404	14.653415
19.815854	1217.828648	14.658432
19.977554	1215.807085	14.663450
19.610523	1212.122724	14.668467
20.144943	1208.396182	14.673485
20.036166	1218.628525	14.678503
19.977711	1206.494477	14.683520
20.022375	1219.843060	14.688538
19.996531	1213.134173	14.693555
20.342029	1214.143117	14.698573
20.027557	1209.570156	14.703591
20.403691	1211.344085	14.708608
20.107520	1213.154535	14.713626
20.241568	1197.876105	14.718643
20.215026	1186.485586	14.723661
19.867083	1190.225417	14.728679
20.231378	1188.257710	14.733696
19.895010	1198.369461	14.738714
20.136582	1203.172673	14.743731
20.085209	1209.639703	14.748749
19.667464	1208.193208	14.753767
19.885636	1214.338844	14.758784
20.180168	1208.719399	14.763802
20.203831	1203.195986	14.768819
20.171719	1198.014086	14.773837
19.771777	1210.083167	14.778855
19.978040	1209.723865	14.783872
20.040700	1214.934254	14.788890
20.132839	1235.096854	14.793907
20.557618	1235.538750	14.798925
20.519768	1239.050085	14.803943
20.782480	1233.504009	14.808960
20.850915	1238.574083	14.813978
20.693871	1232.988459	14.818995
20.412065	1220.046917	14.824013
20.490373	1212.068849	14.829031
20.632507	1206.856125	14.834048
20.580423	1202.921984	14.839066
20.545999	1207.619327	14.844083
20.540725	1203.219967	14.849101
20.128952	1212.808795	14.854119
20.326137	1225.247506	14.859136
20.895553	1235.451025	14.864154
20.622065	1240.193868	14.869171
21.024576	1235.479738	14.874189
20.711374	1231.212065	14.879207
20.434286	1226.427008	14.884224
20.674191	1232.162371	14.889242
20.616756	1236.974160	14.894259
21.037729	1238.401306	14.899277
20.756711	1238.612834	14.904295
20.806617	1239.556160	14.909312
20.850436	1231.230259	14.914330
20.546035	1237.220313	14.919347
20.681191	1229.828084	14.924365
20.304796	1240.966543	14.929383
20.570771	1235.258512	14.934400
20.941862	1226.184346	14.939418
20.888591	1243.497882	14.944435
21.053481	1234.411793	14.949453
20.788654	1231.451430	14.954471
20.714620	1232.719207	14.959488
20.841903	1248.732412	14.964506
21.051513	1258.287668	14.969523
21.337514	1262.409936	14.974541
21.276823	1270.879274	14.979559
20.801162	1259.303626	14.984576
21.062748	1255.146278	14.989594
21.163036	1270.296673	14.994611
20.989501	1260.366234	14.999629
21.282643	1264.507398	15.004647
21.262681	1268.333487	15.009664
21.663829	1261.224357	15.014682
20.990853	1269.647444	15.019699
21.434459	1257.186923	15.024717
21.396693	1268.861049	15.029735
21.396362	1263.666384	15.034752
21.509877	1262.920873	15.039770
21.384950	1265.740744	15.044787
21.512058	1263.846947	15.049805
21.141518	1256.547888	15.054823
21.253804	1254.475841	15.059840
21.509497	1250.002155	15.064858
21.424362	1262.989206	15.069875
21.289594	1260.315168	15.074893
21.506741	1261.001282	15.079911
21.541798	1255.750367	15.084928
21.908132	1260.900646	15.089946
21.992317	1265.062631	15.094963
22.108537	1257.349516	15.099981
21.611670	1233.584784	15.104999
21.545797	1233.327628	15.110016
21.642818	1229.835708	15.115034
21.403620	1227.893910	15.120051
21.671920	1245.445926	15.125069
21.928291	1259.711826	15.130087
21.678246	1249.018884	15.135104
21.782756	1256.815207	15.140122
21.562024	1255.588047	15.145139
21.668276	1259.151509	15.150157
21.673872	1261.236793	15.155175
21.695861	1259.207649	15.160192
21.950907	1260.815418	15.165210
21.674524	1268.348446	15.170227
21.975699	1251.075408	15.175245
22.210693	1256.603724	15.180263
21.912954	1264.930424	15.185280
22.340180	1252.425376	15.190298
22.188376	1256.752416	15.195315
21.922565	1252.410749	15.200333
21.862545	1257.950514	15.205351
21.922056	1256.454908	15.210368
22.050141	1254.038522	15.215386
21.830720	1257.838582	15.220403
21.754123	1261.076424	15.225421
21.707496	1263.857740	15.230439
21.719812	1246.196720	15.235456
22.065805	1253.474328	15.240474
22.105874	1258.163682	15.245491
22.143086	1259.212259	15.250509
22.305383	1265.853771	15.255527
22.254907	1272.236035	15.260544
22.266643	1266.292537	15.265562
22.154070	1288.013083	15.270579
22.557194	1284.289367	15.275597
22.585716	1291.490430	15.280615
22.238255	1275.363721	15.285632
22.535323	1278.341273	15.290650
22.378232	1279.519660	15.295667
22.524680	1274.786897	15.300685
22.450628	1262.691214	15.305703
22.050966	1264.124327	15.310720
22.506973	1275.920237	15.315738
22.261293	1280.290779	15.320755
22.345176	1281.083210	15.325773
22.155211	1282.973717	15.330791
22.071401	1284.706100	15.335808
22.467537	1275.630121	15.340826
22.548009	1278.721882	15.345843
22.293563	1283.620637	15.350861
22.809519	1289.071734	15.355879
22.717416	1295.081381	15.360896
23.125355	1282.150772	15.365914
22.646285	1290.716562	15.370931
22.604499	1287.120057	15.375949
22.449118	1290.808736	15.380967
22.415072	1302.265740	15.385984
22.581570	1310.830944	15.391002
22.648838	1314.481974	15.396019
22.816742	1311.671592	15.401037
23.140684	1301.670957	15.406055
23.395366	1303.516187	15.411072
23.250233	1308.253545	15.416090
23.064211	1313.733093	15.421107
23.125163	1310.056580	15.426125
23.165333	1307.259868	15.431143
23.071718	1311.095408	15.436160
23.019125	1298.367023	15.441178
22.611751	1308.295331	15.446195
22.913293	1305.452980	15.451213
23.388938	1303.439263	15.456231
22.936785	1305.334211	15.461248
23.128137	1295.372463	15.466266
23.015393	1310.974305	15.471283
23.015856	1300.752042	15.476301
23.362130	1306.013136	15.481319
23.255057	1297.400380	15.486336
23.216858	1299.846062	15.491354
23.308622	1297.945515	15.496371
23.461839	1297.303662	15.501389
23.585301	1303.806742	15.506407
22.969646	1304.115411	15.511424
23.505681	1296.044580	15.516442
23.176061	1300.067224	15.521459
23.324155	1301.767508	15.526477
23.414165	1300.928645	15.531495
22.969831	1295.121282	15.536512
23.687936	1295.255561	15.541530
23.457698	1307.789521	15.546547
23.219259	1305.012959	15.551565
23.515125	1305.671474	15.556583
23.369401	1312.260860	15.561600
23.772812	1316.715663	15.566618
23.722568	1321.150704	15.571635
23.762953	1317.073273	15.576653
24.042850	1304.307545	15.581671
23.560837	1302.343739	15.586688
23.787682	1289.935225	15.591706
23.464713	1296.633086	15.596723
23.568760	1304.177547	15.601741
24.100775	1316.546716	15.606759
23.754228	1318.478115	15.611776
24.229651	1316.165227	15.616794
23.820946	1313.440478	15.621811
23.819937	1294.926115	15.626829
23.822753	1291.021443	15.631847
23.615354	1303.382723	15.636864
24.017826	1313.087177	15.641882
23.828570	1325.058470	15.646899
23.706008	1324.292599	15.651917
23.878080	1319.950059	15.656935
23.844398	1333.405805	15.661952
23.878724	1325.118039	15.666970
23.824815	1324.267180	15.671987
24.074875	1326.101761	15.677005
24.039572	1319.377859	15.682023
23.668447	1323.158567	15.687040
24.042792	1316.178650	15.692058
24.171723	1335.437276	15.697075
24.166420	1352.442209	15.702093
24.398345	1355.293558	15.707111
24.229065	1365.373419	15.712128
24.298356	1352.887796	15.717146
24.537232	1348.394819	15.722163
24.440337	1354.329299	15.727181
24.773198	1338.152473	15.732199
24.172648	1320.989297	15.737216
24.566901	1314.453714	15.742234
24.146527	1323.349559	15.747251
24.437171	1338.616925	15.752269
24.498889	1340.794893	15.757287
24.426594	1349.628000	15.762304
24.701553	1346.577842	15.767322
24.857912	1347.235443	15.772339
24.471448	1335.676857	15.777357
24.875428	1339.909923	15.782375
24.500937	1327.108439	15.787392
24.639017	1328.998964	15.792410
24.958887	1331.231821	15.797427
24.474524	1337.607217	15.802445
24.743333	1339.092245	15.807463
24.728635	1335.579825	15.812480
24.845858	1342.610321	15.817498
24.953157	1345.546870	15.822515
24.800891	1341.643455	15.827533
25.061424	1341.640511	15.832551
24.815843	1342.986702	15.837568
24.899115	1345.663455	15.842586
24.993407	1339.295637	15.847603
24.778603	1349.803885	15.852621
25.187309	1353.573189	15.857639
24.671646	1359.867164	15.862656
24.539598	1354.661996	15.867674
25.086948	1354.322590	15.872691
24.856078	1354.102988	15.877709
24.902869	1350.521722	15.882727
25.018902	1347.558114	15.887744
25.192148	1349.728640	15.892762
25.230422	1351.081766	15.897779
24.733861	1349.475868	15.902797
24.868067	1343.208525	15.907815
24.906349	1348.375753	15.912832
25.007938	1351.993551	15.917850
25.194282	1349.622620	15.922867
25.247554	1371.292987	15.927885
25.482297	1373.382862	15.932903
25.470269	1386.548459	15.937920
25.707700	1371.496043	15.942938
25.530036	1355.698609	15.947955
25.243006	1350.341941	15.952973
25.770048	1333.908955	15.957991
25.372750	1341.632115	15.963008
25.624343	1342.423550	15.968026
25.658532	1336.255446	15.973043
25.080003	1342.790528	15.978061
25.604791	1336.148678	15.983079
25.662588	1356.702155	15.988096
25.764458	1361.808072	15.993114
25.960743	1354.896598	15.998131
25.404698	1360.521681	16.003149
25.609893	1343.936861	16.008167
25.907261	1365.599085	16.013184
25.675103	1360.952608	16.018202
25.427160	1353.759578	16.023219
25.440066	1373.144547	16.028237
25.531756	1373.589239	16.033255
25.337487	1375.936762	16.038272
25.747560	1373.492169	16.043290
25.696543	1377.503739	16.048307
25.667167	1376.465353	16.053325
25.786200	1363.537239	16.058343
25.797792	1387.144811	16.063360
26.103399	1393.136674	16.068378
26.117421	1405.091299	16.073395
26.105756	1398.896905	16.078413
26.460596	1395.652411	16.083431
26.142624	1384.568266	16.088448
26.232761	1373.657101	16.093466
26.229740	1370.626196	16.098483
25.648480	1369.818166	16.103501
26.537308	1381.023600	16.108519
26.282770	1387.647178	16.113536
25.979876	1372.847218	16.118554
26.566962	1385.639601	16.123571
26.074204	1397.394673	16.128589
26.056720	1386.944620	16.133607
25.995219	1396.639338	16.138624
25.988079	1404.312099	16.143642
26.601813	1400.958202	16.148659
26.585521	1398.267278	16.153677
26.692409	1393.221350	16.158695
26.744784	1394.252465	16.163712
26.774676	1391.088942	16.168730
26.836147	1388.859152	16.173747
26.712142	1392.507228	16.178765
26.881002	1375.820911	16.183783
26.842428	1366.080258	16.188800
26.766673	1358.155971	16.193818
26.843691	1347.673761	16.198835
26.673541	1352.053470	16.203853
26.644541	1341.517166	16.208871
26.476567	1362.048586	16.213888
26.399497	1358.348460	16.218906
26.687962	1367.358058	16.223923
26.613902	1381.096905	16.228941
26.946431	1380.095442	16.233959
26.809826	1392.950575	16.238976
26.980533	1389.088156	16.243994
27.263147	1389.111084	16.249011
26.996193	1398.285895	16.254029
27.309593	1380.676048	16.259047
27.036518	1361.822802	16.264064
26.942857	1359.348236	16.269082
26.896834	1360.256274	16.274099
26.661587	1380.692560	16.279117
26.975451	1376.087948	16.284135
26.901691	1388.097252	16.289152
26.838924	1393.013908	16.294170
26.930589	1387.119727	16.299187
26.824308	1391.970360	16.304205
26.896809	1389.926930	16.309223
26.981779	1389.714084	16.314240
26.663456	1409.128747	16.319258
27.259310	1409.277759	16.324275
27.299036	1414.489650	16.329293
27.294614	1419.638382	16.334311
27.410601	1411.645312	16.339328
27.428332	1412.242013	16.344346
27.869540	1411.730421	16.349363
27.624650	1419.356730	16.354381
27.685646	1412.745581	16.359399
27.588173	1411.264143	16.364416
27.979732	1410.097002	16.369434
27.919315	1394.236414	16.374451
27.783792	1386.002329	16.379469
27.627258	1383.460218	16.384487
27.645587	1377.731331	16.389504
27.482630	1386.196013	16.394522
27.533981	1381.126213	16.399539
27.706947	1401.261080	16.404557
27.822410	1409.686760	16.409575
28.074744	1406.810019	16.414592
27.819133	1407.085056	16.419610
27.827932	1390.607508	16.424627
28.177251	1411.994665	16.429645
28.036782	1399.139410	16.434663
27.628427	1389.175330	16.439680
27.578609	1385.949023	16.444698
27.916410	1395.454398	16.449715
27.952464	1408.461661	16.454733
28.026819	1401.058552	16.459751
27.873876	1394.032054	16.464768
27.557088	1406.974907	16.469786
27.485762	1399.990403	16.474803
27.529682	1404.585858	16.479821
28.216729	1414.823168	16.484839
28.515050	1427.079156	16.489856
28.062534	1434.285528	16.494874
28.482214	1423.033152	16.499891
28.331321	1436.812722	16.504909
28.315992	1427.560694	16.509927
28.191147	1417.175640	16.514944
28.439270	1426.419903	16.519962
28.274055	1424.275280	16.524979
28.200270	1437.595633	16.529997
28.478655	1431.915397	16.535015
28.590703	1429.254004	16.540032
28.173610	1436.034044	16.545050
28.272588	1432.770885	16.550067
28.367632	1423.353736	16.555085
28.466743	1425.946385	16.560103
28.750930	1420.083699	16.565120
28.377604	1432.922550	16.570138
28.343654	1429.247944	16.575155
28.677047	1422.160196	16.580173
28.871403	1427.422472	16.585191
28.574352	1424.487879	16.590208
28.509879	1432.307153	16.595226
28.592056	1422.935834	16.600243
28.696506	1444.221850	16.605261
28.736148	1446.692068	16.610279
29.078771	1443.474784	16.615296
28.703006	1449.486972	16.620314
28.984747	1450.199406	16.625331
28.979227	1449.678713	16.630349
28.878464	1449.992677	16.635367
29.123050	1440.685006	16.640384
29.120532	1449.325123	16.645402
29.094923	1443.533015	16.650419
29.207056	1451.584471	16.655437
28.881814	1445.768748	16.660455
29.372802	1443.170197	16.665472
29.321551	1448.172757	16.670490
29.688764	1440.219963	16.675507
29.646860	1449.552813	16.680525
29.129095	1438.287540	16.685543
29.606133	1427.813449	16.690560
29.038508	1436.936101	16.695578
29.323063	1435.937067	16.700595
29.452413	1433.205093	16.705613
29.085375	1444.485846	16.710631
29.336023	1440.340890	16.715648
29.379316	1448.756888	16.720666
29.465891	1441.012764	16.725683
29.181375	1447.459049	16.730701
29.321478	1444.694978	16.735719
29.444299	1439.103883	16.740736
29.058252	1447.940179	16.745754
29.572504	1448.673169	16.750771
29.608951	1464.910298	16.755789
29.550302	1474.107748	16.760807
29.995088	1475.198301	16.765824
29.631333	1479.589630	16.770842
30.064294	1474.045987	16.775859
30.257071	1469.589743	16.780877
29.586738	1467.259857	16.785895
30.139667	1447.971708	16.790912
30.302889	1461.194176	16.795930
30.067820	1446.600629	16.800947
30.177735	1444.304149	16.805965
29.889046	1442.723270	16.810983
29.989570	1427.873781	16.816000
29.693489	1445.782070	16.821018
30.018277	1445.997619	16.826035
29.988077	1454.813974	16.831053
30.125003	1464.518005	16.836071
30.178785	1460.548946	16.841088
30.082036	1464.981099	16.846106
30.326478	1462.908403	16.851123
30.129446	1468.478015	16.856141
30.159988	1459.868366	16.861159
30.207372	1456.027926	16.866176
30.163946	1460.970140	16.871194
30.219734	1455.237384	16.876211
30.606100	1457.804128	16.881229
30.425669	1450.336491	16.886247
30.827206	1444.902785	16.891264
30.431137	1458.398171	16.896282
30.481114	1453.498652	16.901299
30.556339	1446.691434	16.906317
30.623103	1457.805487	16.911335
30.386442	1448.812927	16.916352
30.062477	1456.362585	16.921370
29.892469	1462.115908	16.926387
30.383351	1468.928294	16.931405
30.443199	1484.144256	16.936423
30.700887	1479.220178	16.941440
30.559769	1487.750196	16.946458
30.702553	1489.216343	16.951475
30.885149	1484.881464	16.956493
30.680054	1484.492633	16.961511
30.656405	1486.890266	16.966528
30.770541	1483.937970	16.971546
31.019181	1486.346030	16.976563
31.245715	1480.800738	16.981581
31.210119	1482.806652	16.986599
31.401719	1476.626995	16.991616
31.113987	1477.738840	16.996634
31.283989	1480.371728	17.001651
31.058323	1478.947730	17.006669
31.234195	1469.180165	17.011687
31.677489	1469.348534	17.016704
31.146771	1477.061569	17.021722
30.902732	1481.158276	17.026739
31.193475	1474.933464	17.031757
31.005129	1477.544191	17.036775
31.562017	1487.973180	17.041792
31.494964	1493.322463	17.046810
31.618286	1489.844634	17.051827
31.511052	1481.786520	17.056845
31.313811	1483.844397	17.061863
31.504576	1494.234407	17.066880
31.578948	1494.779214	17.071898
31.650468	1508.253125	17.076915
31.908774	1508.134017	17.081933
31.998729	1502.284170	17.086951
31.615100	1482.898298	17.091968
31.530826	1480.226097	17.096986
31.453602	1490.783706	17.102003
31.724873	1507.685928	17.107021
31.938297	1508.615188	17.112039
31.966133	1501.872091	17.117056
31.658691	1503.513181	17.122074
31.549475	1503.560044	17.127091
31.778624	1501.385545	17.132109
31.811986	1509.226847	17.137127
31.795543	1501.981637	17.142144
31.827355	1496.548108	17.147162
31.921308	1509.829332	17.152179
31.972457	1503.473709	17.157197
31.819662	1513.752904	17.162215
31.741644	1495.861677	17.167232
31.951165	1516.413866	17.172250
32.512758	1519.081527	17.177267
32.336851	1522.291772	17.182285
32.606936	1525.051796	17.187303
32.745648	1521.530861	17.192320
32.465338	1509.160478	17.197338
32.511026	1498.964060	17.202355
32.369716	1493.435183	17.207373
32.141818	1490.291097	17.212391
32.387210	1499.854751	17.217408
32.455689	1508.690230	17.222426
32.613943	1521.153735	17.227443
33.044509	1504.584970	17.232461
32.624539	1502.953775	17.237479
32.504716	1494.520577	17.242496
32.494656	1487.167231	17.247514
32.747491	1495.339112	17.252531
32.756831	1486.014067	17.257549
32.556629	1494.150332	17.262567
33.024735	1512.846330	17.267584
32.437039	1501.030390	17.272602
32.567768	1519.807455	17.277619
32.819721	1508.909953	17.282637
32.986538	1521.153145	17.287655
32.942087	1512.344075	17.292672
32.925628	1508.311044	17.297690
32.633544	1517.606227	17.302707
32.802122	1508.688657	17.307725
32.635684	1509.667035	17.312743
32.814548	1513.539790	17.317760
33.170464	1512.514370	17.322778
33.142593	1516.843795	17.327795
33.064390	1508.478894	17.332813
32.770235	1522.823990	17.337831
33.166290	1535.907183	17.342848
33.448738	1534.284481	17.347866
32.762481	1551.600021	17.352883
32.980329	1540.088462	17.357901
33.062528	1541.527638	17.362919
33.118885	1537.484118	17.367936
33.606957	1539.003333	17.372954
33.667135	1535.548941	17.377971
33.691056	1537.926108	17.382989
33.542103	1544.294475	17.388007
33.488465	1541.114831	17.393024
33.793260	1530.822734	17.398042
33.808494	1541.262706	17.403059
34.234799	1532.109537	17.408077
33.669684	1537.406265	17.413095
33.536433	1537.838602	17.418112
33.780206	1539.656140	17.423130
33.670769	1541.311693	17.428147
33.999553	1531.657351	17.433165
33.894344	1536.470844	17.438183
34.043941	1536.865402	17.443200
33.964522	1532.892396	17.448218
33.711498	1543.583086	17.453235
34.073408	1537.303158	17.458253
33.998576	1537.220707	17.463271
33.662937	1534.390513	17.468288
33.748929	1551.445508	17.473306
33.584339	1557.593242	17.478323
33.951810	1562.337926	17.483341
34.141442	1557.869578	17.488359
34.133962	1570.839698	17.493376
34.470010	1565.484904	17.498394
34.341010	1571.591318	17.503411
34.189669	1565.635338	17.508429
34.525697	1567.963980	17.513447
34.560882	1565.710566	17.518464
34.248219	1562.181683	17.523482
34.518780	1562.631803	17.528499
34.583000	1567.080638	17.533517
34.172245	1564.554213	17.538535
34.123269	1578.543017	17.543552
34.767744	1590.511111	17.548570
34.962395	1586.730112	17.553587
34.870124	1591.708408	17.558605
34.582642	1586.692677	17.563623
34.724936	1588.906551	17.568640
34.779374	1581.394843	17.573658
35.044078	1591.356536	17.578675
35.271037	1586.450111	17.583693
35.015282	1562.695735	17.588711
34.925898	1555.965724	17.593728
35.060064	1544.668804	17.598746
34.739590	1556.800585	17.603763
34.898246	1553.991297	17.608781
35.003034	1566.800305	17.613799
35.163852	1571.876059	17.618816
35.189068	1572.930580	17.623834
35.238524	1580.300751	17.628851
35.557845	1575.424706	17.633869
35.314657	1565.787492	17.638887
35.116286	1555.203103	17.643904
35.312929	1553.505236	17.648922
35.095647	1555.632581	17.653939
35.199953	1563.753108	17.658957
35.537225	1575.677569	17.663975
35.370289	1582.507589	17.668992
35.300529	1574.740072	17.674010
35.231397	1589.614897	17.679027
34.984987	1580.716000	17.684045
35.186958	1590.393986	17.689063
35.310948	1585.589257	17.694080
35.442446	1580.247855	17.699098
35.655472	1585.293708	17.704115
35.843206	1603.472068	17.709133
36.047527	1612.780388	17.714151
35.661364	1600.089271	17.719168
35.937471	1583.847965	17.724186
35.670078	1590.478874	17.729203
36.310771	1593.202743	17.734221
36.113786	1588.806276	17.739239
35.888617	1583.750307	17.744256
36.407225	1579.827874	17.749274
36.038216	1586.418914	17.754291
35.891248	1576.704344	17.759309
36.173879	1573.217047	17.764327
36.068852	1569.143941	17.769344
36.260852	1571.932651	17.774362
36.113271	1581.957879	17.779379
36.009644	1595.851811	17.784397
36.430802	1594.825031	17.789415
36.228750	1600.018357	17.794432
36.405181	1596.743521	17.799450
36.385002	1598.346111	17.804467
36.263307	1591.788757	17.809485
36.383250	1603.318518	17.814503
36.329553	1605.010123	17.819520
36.772648	1601.037196	17.824538
36.520850	1608.269467	17.829555
36.679101	1600.337018	17.834573
36.546399	1605.035399	17.839591
36.333221	1612.738835	17.844608
36.560195	1602.391860	17.849626
36.548153	1601.550194	17.854643
36.504444	1593.209064	17.859661
36.679482	1595.234447	17.864679
36.364319	1611.110264	17.869696
36.766600	1618.919670	17.874714
36.582127	1632.232139	17.879731
36.762519	1636.985775	17.884749
36.924501	1632.647970	17.889767
36.951199	1637.514456	17.894784
36.981162	1637.753629	17.899802
37.097623	1636.386746	17.904819
36.996424	1634.164172	17.909837
36.793317	1633.304534	17.914855
36.802381	1636.193625	17.919872
37.092848	1643.473920	17.924890
37.232596	1650.504370	17.929907
37.428854	1642.379386	17.934925
37.572380	1642.092668	17.939943
37.374317	1645.067631	17.944960
37.853035	1638.138794	17.949978
37.370512	1626.048650	17.954995
37.316029	1610.755755	17.960013
37.480921	1617.950925	17.965031
37.611648	1640.882466	17.970048
37.532574	1634.472761	17.975066
37.683323	1638.865558	17.980083
37.825685	1646.718803	17.985101
38.054092	1642.493224	17.990119
37.875804	1649.303106	17.995136
38.043844	1636.106808	18.000154
37.662835	1630.265996	18.005171
37.802312	1631.013020	18.010189
38.140771	1624.886547	18.015207
37.694903	1639.517894	18.020224
37.662777	1627.337031	18.025242
37.934691	1628.613307	18.030259
37.797170	1642.843601	18.035277
37.815173	1637.928452	18.040295
37.388652	1647.160932	18.045312
38.099165	1640.717730	18.050330
38.024349	1636.144329	18.055347
37.906734	1647.954009	18.060365
38.322846	1657.130437	18.065383
38.088998	1670.640878	18.070400
38.125493	1669.591959	18.075418
38.315254	1677.690128	18.080435
38.358351	1669.189702	18.085453
38.692353	1669.498612	18.090471
38.412228	1675.963949	18.095488
38.730053	1661.884164	18.100506
38.781924	1667.829958	18.105523
38.899868	1665.173455	18.110541
39.017525	1663.590624	18.115559
38.645775	1664.123084	18.120576
38.750028	1664.036570	18.125594
38.296861	1658.796674	18.130611
38.649063	1656.400597	18.135629
38.914883	1658.942454	18.140647
38.666952	1668.599707	18.145664
38.609096	1667.983341	18.150682
38.648926	1651.678330	18.155699
39.137910	1657.578909	18.160717
39.065510	1650.300769	18.165735
39.079212	1655.091066	18.170752
39.059556	1654.944360	18.175770
39.374898	1654.512264	18.180787
39.329914	1670.741438	18.185805
39.513360	1656.523672	18.190823
39.219962	1667.793574	18.195840
39.272306	1651.340034	18.200858
39.213686	1651.561591	18.205875
39.448997	1670.356563	18.210893
39.791884	1667.410844	18.215911
39.412704	1664.532323	18.220928
39.276861	1655.812712	18.225946
39.736322	1663.721336	18.230963
39.680328	1679.095253	18.235981
39.623471	1669.948382	18.240999
39.728217	1680.594494	18.246016
39.666020	1680.815069	18.251034
39.771617	1666.894830	18.256051
40.020096	1673.394295	18.261069
40.113558	1654.266220	18.266087
39.868497	1652.559196	18.271104
39.940283	1650.330417	18.276122
40.240626	1649.670096	18.281139
39.812957	1647.559843	18.286157
40.002831	1648.794193	18.291175
39.932685	1659.145233	18.296192
40.066540	1650.556560	18.301210
40.188549	1645.250565	18.306227
39.631929	1649.761277	18.311245
40.183845	1652.462849	18.316263
39.960682	1669.868771	18.321280
40.090990	1667.930694	18.326298
39.971171	1673.511611	18.331315
40.053200	1680.315017	18.336333
40.400353	1685.574523	18.341351
40.512741	1686.874856	18.346368
40.794278	1680.273926	18.351386
40.655750	1675.620511	18.356403
40.741947	1667.499957	18.361421
40.420972	1660.605491	18.366439
40.668363	1669.710651	18.371456
40.868822	1675.632633	18.376474
40.951741	1670.566961	18.381491
40.494165	1666.578582	18.386509
40.993635	1674.135703	18.391527
40.627639	1673.915634	18.396544
40.474720	1677.674862	18.401562
40.687209	1671.109385	18.406579
40.640785	1675.170272	18.411597
40.855013	1687.970709	18.416615
40.887047	1707.073400	18.421632
40.795028	1711.346571	18.426650
41.001945	1707.484378	18.431667
40.827724	1702.386469	18.436685
41.096014	1700.872394	18.441703
41.088982	1704.873616	18.446720
41.028661	1700.336772	18.451738
41.203898	1697.604241	18.456755
40.788102	1708.110971	18.461773
41.090517	1722.487787	18.466791
41.454296	1727.748885	18.471808
41.412450	1729.018459	18.476826
41.926382	1726.147165	18.481843
41.657475	1724.535027	18.486861
41.957230	1723.494483	18.491879
41.857825	1724.608626	18.496896
41.718125	1725.556212	18.501914
42.042518	1725.766714	18.506931
41.592999	1726.784890	18.511949
41.974614	1727.023713	18.516967
41.638725	1721.678155	18.521984
41.646074	1724.296678	18.527002
41.958968	1724.073649	18.532019
41.650196	1723.237801	18.537037
42.146234	1720.696638	18.542055
42.030821	1723.744545	18.547072
42.023485	1717.047336	18.552090
42.052551	1707.486213	18.557107
42.105027	1723.994977	18.562125
42.282371	1716.158521	18.567143
41.957665	1715.230823	18.572160
41.866811	1728.578661	18.577178
42.189945	1720.813339	18.582195
41.715045	1741.792540	18.587213
41.929361	1736.604696	18.592231
41.943790	1742.845697	18.597248
42.155690	1751.522920	18.602266
42.292791	1742.484050	18.607283
42.621972	1759.674600	18.612301
42.839749	1764.231926	18.617319
42.871805	1757.793139	18.622336
43.127970	1767.641005	18.627354
43.125229	1738.356623	18.632371
42.742680	1750.774425	18.637389
43.036953	1742.418985	18.642407
42.961614	1743.418120	18.647424
43.139461	1733.544550	18.652442
43.146251	1735.415525	18.657459
42.900041	1735.443339	18.662477
42.819728	1742.384283	18.667495
43.218915	1740.873728	18.672512
43.063707	1738.532521	18.677530
43.176271	1739.887554	18.682547
43.062285	1739.497015	18.687565
43.250053	1739.463209	18.692583
43.126057	1733.513660	18.697600
42.909598	1743.625200	18.702618
43.287080	1756.826225	18.707635
43.225661	1759.373069	18.712653
43.329033	1749.465757	18.717671
43.387170	1753.572344	18.722688
43.144592	1763.081918	18.727706
43.609569	1748.300519	18.732723
43.368189	1757.270123	18.737741
43.443293	1757.350641	18.742759
43.766198	1755.675942	18.747776
43.903095	1778.514932	18.752794
44.121516	1770.938579	18.757811
43.988769	1768.044037	18.762829
43.870076	1759.160504	18.767847
43.957111	1754.238218	18.772864
43.462145	1763.205325	18.777882
43.867842	1775.109951	18.782899
43.925616	1781.042213	18.787917
43.958344	1783.471109	18.792935
44.273717	1776.947214	18.797952
44.298951	1781.803752	18.802970
44.357272	1784.675266	18.807987
44.436359	1782.547229	18.813005
44.342075	1779.407731	18.818023
44.541513	1774.447536	18.823040
44.234843	1781.898423	18.828058
44.592347	1770.530895	18.833075
44.297941	1781.401436	18.838093
44.485351	1778.404275	18.843111
44.415206	1778.548213	18.848128
44.224085	1789.167010	18.853146
44.893357	1777.015171	18.858163
44.532268	1782.101818	18.863181
44.701855	1800.689325	18.868199
44.965645	1797.392502	18.873216
44.843085	1803.614871	18.878234
45.210146	1798.813530	18.883251
44.944446	1806.364733	18.888269
45.136535	1811.584208	18.893287
45.278302	1814.291121	18.898304
45.408339	1800.333645	18.903322
45.266174	1785.880301	18.908339
44.956836	1776.646037	18.913357
45.082659	1783.102864	18.918375
45.257083	1802.333279	18.923392
44.964508	1806.601494	18.928410
45.097883	1801.297501	18.933427
45.374091	1802.782533	18.938445
45.414018	1806.102770	18.943463
45.396924	1804.941847	18.948480
45.128474	1805.817841	18.953498
45.282886	1806.584449	18.958515
45.237731	1802.981688	18.963533
45.360831	1803.042448	18.968551
45.609570	1815.537667	18.973568
45.631446	1837.916650	18.978586
46.052076	1838.045471	18.983603
46.111624	1831.724150	18.988621
45.750550	1828.175661	18.993639
45.841350	1828.708311	18.998656
45.688539	1837.080611	19.003674
46.106381	1813.693064	19.008691
45.798858	1827.534348	19.013709
45.716018	1825.229177	19.018727
46.238741	1817.029575	19.023744
46.028725	1822.154607	19.028762
46.158814	1817.685809	19.033779
46.155175	1820.054590	19.038797
46.209336	1818.068866	19.043815
46.203255	1813.934036	19.048832
46.181047	1829.449361	19.053850
46.618763	1836.854975	19.058867
46.529144	1843.544746	19.063885
46.553816	1849.569918	19.068903
46.936081	1841.189226	19.073920
46.731204	1848.731953	19.078938
46.743479	1835.915613	19.083955
46.900028	1843.011874	19.088973
46.700574	1832.452278	19.093991
47.222167	1832.666745	19.099008
46.984729	1844.582636	19.104026
47.056951	1840.742318	19.109043
46.944569	1836.323505	19.114061
46.746672	1832.334212	19.119079
47.498689	1834.808981	19.124096
46.923774	1845.321283	19.129114
47.510092	1840.893868	19.134131
47.270919	1849.061967	19.139149
47.440423	1839.399556	19.144167
47.511747	1843.936273	19.149184
47.297449	1843.112335	19.154202
47.356077	1844.882219	19.159219
47.247945	1843.588727	19.164237
47.187641	1836.792361	19.169255
47.432450	1838.982998	19.174272
47.544188	1844.783119	19.179290
47.537602	1833.439609	19.184307
47.422626	1835.183512	19.189325
47.602513	1834.980535	19.194343
47.491305	1833.884801	19.199360
47.321531	1849.780489	19.204378
47.728528	1861.962530	19.209395
47.796160	1866.033322	19.214413
47.835048	1863.593027	19.219431
48.012493	1873.787465	19.224448
48.281452	1869.681491	19.229466
48.297277	1866.793039	19.234483
48.193640	1863.152703	19.239501
47.982375	1864.110572	19.244519
48.299984	1852.935419	19.249536
48.048236	1862.935161	19.254554
48.089123	1860.655956	19.259571
48.116666	1860.100640	19.264589
48.028934	1868.394858	19.269607
48.304607	1877.393488	19.274624
48.338618	1884.895103	19.279642
48.578068	1892.338297	19.284659
48.546289	1880.583956	19.289677
48.794564	1892.513557	19.294695
49.153317	1884.689500	19.299712
48.749970	1881.087367	19.304730
48.509553	1891.456517	19.309747
48.716948	1882.100410	19.314765
48.837754	1882.452106	19.319783
49.149151	1872.402396	19.324800
48.817795	1883.124399	19.329818
48.821195	1887.901513	19.334835
49.182387	1880.525486	19.339853
48.618135	1881.570149	19.344871
49.017748	1884.217452	19.349888
48.815601	1886.982503	19.354906
48.906775	1902.576767	19.359923
49.199434	1907.843403	19.364941
48.997207	1917.106622	19.369959
49.519706	1909.261739	19.374976
49.432208	1914.648805	19.379994
49.229260	1912.886352	19.385011
49.595725	1913.146585	19.390029
49.470136	1910.561073	19.395047
49.861795	1908.045432	19.400064
49.788865	1916.549039	19.405082
49.738441	1915.188899	19.410099
49.964637	1916.888132	19.415117
49.645521	1915.441376	19.420135
50.181691	1921.003924	19.425152
50.262281	1935.418061	19.430170
49.840065	1925.644513	19.435187
50.170291	1913.534139	19.440205
50.078842	1931.283511	19.445223
50.362031	1920.291572	19.450240
50.195647	1930.407934	19.455258
50.144463	1933.705883	19.460275
50.317688	1935.948545	19.465293
50.079711	1929.544555	19.470311
50.262696	1931.028499	19.475328
50.272753	1930.820176	19.480346
50.259794	1936.149631	19.485363
50.677079	1931.479307	19.490381
50.394316	1933.620301	19.495399
50.480303	1927.739454	19.500416
50.557629	1939.764327	19.505434
50.535464	1948.837511	19.510451
50.944736	1959.815684	19.515469
50.731274	1961.545985	19.520487
51.026829	1953.820549	19.525504
50.815945	1955.150414	19.530522
50.677822	1961.669130	19.535539
51.166786	1956.173922	19.540557
50.683648	1960.261915	19.545575
51.307272	1954.175501	19.550592
50.923373	1950.117366	19.555610
50.787775	1960.781812	19.560627
51.372374	1971.734114	19.565645
51.380196	1980.333837	19.570663
51.466115	1978.064482	19.575680
51.256341	1975.798022	19.580698
51.587872	1965.222860	19.585715
51.836518	1972.451179	19.590733
51.433906	1968.044949	19.595751
51.990609	1970.567436	19.600768
51.696112	1969.439046	19.605786
51.868167	1972.819333	19.610803
52.250126	1966.514656	19.615821
52.290437	1974.675522	19.620839
52.229243	1967.948538	19.625856
52.202206	1971.648411	19.630874
52.068894	1962.583712	19.635891
52.278456	1948.038908	19.640909
51.907081	1944.451939	19.645927
52.070232	1946.336814	19.650944
52.386557	1954.657092	19.655962
52.203616	1967.855418	19.660979
52.397137	1963.584348	19.665997
51.959835	1969.964017	19.671015
52.258380	1974.610791	19.676032
52.457207	1970.909718	19.681050
52.151476	1969.901301	19.686067
52.444241	1968.001645	19.691085
52.393927	1979.864607	19.696103
52.372344	1968.604192	19.701120
52.714205	1974.905248	19.706138
52.406080	2002.395126	19.711155
52.796703	1995.720095	19.716173
52.613039	2001.084529	19.721191
52.986409	2002.375143	19.726208
53.337607	2002.821769	19.731226
52.837737	2009.291343	19.736243
52.978158	2002.887270	19.741261
52.976100	2011.787866	19.746279
52.917342	1997.224055	19.751296
53.210486	2001.129194	19.756314
53.235080	2017.160985	19.761331
53.758965	2022.541743	19.766349
53.189704	2028.600362	19.771367
53.446591	2025.897563	19.776384
53.686143	2020.761748	19.781402
53.560813	2029.896156	19.786419
53.808712	2026.781843	19.791437
53.524262	2040.718316	19.796455
53.450876	2025.359636	19.801472
53.458477	2023.770188	19.806490
53.306670	2034.756668	19.811507
53.987141	2017.808964	19.816525
54.004733	2019.577001	19.821543
53.828827	2027.216595	19.826560
53.819828	2038.023916	19.831578
53.833700	2053.719322	19.836595
54.456807	2048.754248	19.841613
54.463481	2045.381045	19.846631
54.529024	2043.054816	19.851648
54.625233	2046.561855	19.856666
54.541455	2048.222660	19.861683
54.318440	2048.156473	19.866701
54.690359	2042.721167	19.871719
54.421404	2044.340583	19.876736
54.651130	2036.555925	19.881754
54.410399	2035.589892	19.886771
54.685760	2036.467985	19.891789
54.651794	2037.910694	19.896807
54.661837	2031.347089	19.901824
54.840273	2036.862216	19.906842
54.646078	2038.408622	19.911859
54.795391	2036.711061	19.916877
55.013326	2047.111513	19.921895
55.341712	2061.081184	19.926912
55.828574	2052.733456	19.931930
55.402201	2049.555972	19.936947
55.183540	2035.556411	19.941965
55.231287	2035.322555	19.946983
55.139676	2032.268392	19.952000
55.753476	2035.352711	19.957018
55.239929	2043.722645	19.962035
55.673603	2042.937081	19.967053
55.535729	2058.001300	19.972071
55.532380	2067.263175	19.977088
55.937965	2053.873644	19.982106
55.601312	2066.224646	19.987123
55.776438	2056.028479	19.992141
55.672486	2058.280437	19.997159
55.363862	2057.181151	20.002176
55.878718	2054.250591	20.007194
55.636473	2053.024170	20.012211
55.689873	2054.428005	20.017229
55.698585	2064.550109	20.022247
55.683962	2081.647151	20.027264
56.162958	2081.072198	20.032282
56.328834	2082.341660	20.037299
56.694210	2084.276537	20.042317
56.517801	2078.961536	20.047335
56.160490	2082.751160	20.052352
56.692822	2076.941634	20.057370
56.641493	2076.310783	20.062387
56.919914	2076.385200	20.067405
56.733015	2075.483087	20.072423
56.455859	2077.086935	20.077440
56.806624	2067.996357	20.082458
56.636443	2069.508080	20.087475
56.727681	2074.807731	20.092493
56.842471	2068.340550	20.097511
57.153750	2071.564339	20.102528
57.475124	2072.249378	20.107546
57.265372	2070.576224	20.112563
57.123919	2064.594397	20.117581
57.371901	2065.189222	20.122599
57.028661	2058.816781	20.127616
57.106000	2064.449054	20.132634
57.599799	2083.544258	20.137651
57.773120	2085.972365	20.142669
57.736644	2088.665137	20.147687
57.782568	2089.282001	20.152704
58.075514	2086.484243	20.157722
57.624422	2100.660966	20.162739
57.961236	2087.201689	20.167757
58.264203	2085.164893	20.172775
58.029172	2084.482960	20.177792
57.886561	2075.789824	20.182810
57.786162	2069.147636	20.187827
57.484739	2072.439014	20.192845
58.008669	2088.614587	20.197863
57.900890	2089.647068	20.202880
58.014967	2088.404955	20.207898
57.552096	2092.049062	20.212915
57.773402	2109.465743	20.217933
58.169756	2109.113534	20.222951
57.929415	2118.389482	20.227968
58.262918	2118.558325	20.232986
58.382053	2121.133209	20.238003
58.367272	2117.422587	20.243021
58.594117	2127.086161	20.248039
58.441052	2149.537080	20.253056
58.891020	2135.239313	20.258074
58.778468	2142.863749	20.263091
59.141711	2143.892658	20.268109
59.173662	2136.342671	20.273127
58.842175	2134.479818	20.278144
59.067790	2131.338070	20.283162
58.959645	2137.069587	20.288179
59.138552	2133.906438	20.293197
59.774565	2134.608677	20.298215
59.472015	2138.325859	20.303232
59.782006	2130.116434	20.308250
59.622193	2127.075119	20.313267
59.487667	2135.467387	20.318285
59.581652	2123.852280	20.323303
59.568623	2134.388673	20.328320
59.598108	2125.472915	20.333338
59.479097	2126.620254	20.338355
59.744933	2134.608427	20.343373
59.672243	2126.161568	20.348391
59.465782	2127.470242	20.353408
59.607223	2136.749526	20.358426
59.730308	2159.489392	20.363443
59.748113	2163.168893	20.368461
59.885666	2164.626523	20.373479
59.999179	2165.516854	20.378496
59.811131	2163.162121	20.383514
59.727993	2166.719355	20.388531
59.994911	2179.764633	20.393549
60.417473	2188.182412	20.398567
60.368645	2196.834943	20.403584
60.687981	2187.542799	20.408602
60.487290	2190.311205	20.413619
60.427226	2193.348070	20.418637
60.777080	2180.546420	20.423655
60.430351	2192.843677	20.428672
60.702993	2191.160720	20.433690
60.775968	2204.682635	20.438707
60.978861	2214.288810	20.443725
61.466417	2210.015053	20.448743
61.226095	2211.284457	20.453760
61.229477	2207.160161	20.458778
61.598418	2203.709225	20.463795
61.828490	2199.561571	20.468813
61.554243	2187.815252	20.473831
61.377738	2172.433735	20.478848
61.274300	2167.841686	20.483866
61.420080	2183.623261	20.488883
61.607800	2199.636499	20.493901
61.666722	2202.244201	20.498919
61.578440	2195.417269	20.503936
61.805695	2197.449836	20.508954
61.935913	2191.209191	20.513971
61.785404	2190.331756	20.518989
62.062237	2193.462059	20.524007
61.748487	2191.502557	20.529024
61.853636	2191.994260	20.534042
61.565088	2205.424061	20.539059
62.146527	2220.584701	20.544077
62.495139	2212.541285	20.549095
62.073507	2223.200906	20.554112
62.364937	2223.349944	20.559130
62.370558	2229.226837	20.564147
62.355559	2227.440709	20.569165
62.845797	2228.038738	20.574183
62.675492	2223.669957	20.579200
62.330528	2224.356665	20.584218
62.233293	2222.165633	20.589235
62.343885	2230.035853	20.594253
62.917914	2249.093174	20.599271
62.692548	2262.138925	20.604288
62.849557	2251.340880	20.609306
63.143603	2253.269085	20.614323
63.005387	2250.664345	20.619341
63.107227	2243.733075	20.624359
63.236559	2248.085102	20.629376
63.538732	2243.758563	20.634394
63.412526	2249.743515	20.639411
63.274440	2249.813664	20.644429
63.553846	2246.816143	20.649447
63.324757	2241.903918	20.654464
63.308877	2249.744298	20.659482
63.615135	2256.129714	20.664499
63.613213	2269.926303	20.669517
63.886717	2267.902236	20.674535
63.838526	2269.209915	20.679552
63.591289	2270.745833	20.684570
63.871799	2270.543122	20.689587
64.023715	2271.290875	20.694605
64.144852	2257.764008	20.699623
63.930057	2263.719536	20.704640
64.108649	2259.765437	20.709658
64.192508	2262.221377	20.714675
64.324811	2267.493428	20.719693
64.474876	2283.801188	20.724711
64.390152	2290.395849	20.729728
64.888338	2292.353647	20.734746
64.705091	2293.560061	20.739763
64.797604	2294.384583	20.744781
64.844761	2288.669879	20.749799
64.749983	2294.232697	20.754816
65.221762	2292.514790	20.759834
64.923145	2290.577967	20.764851
64.698294	2294.229563	20.769869
65.110629	2287.546483	20.774887
65.070946	2283.297796	20.779904
64.993153	2279.389685	20.784922
64.996052	2288.113627	20.789939
65.011695	2292.518744	20.794957
65.126525	2288.868120	20.799975
65.365780	2314.502489	20.804992
65.439984	2313.410274	20.810010
65.918300	2311.038498	20.815027
65.611959	2316.656826	20.820045
65.946177	2307.154264	20.825063
65.983220	2311.981846	20.830080
65.841043	2307.403650	20.835098
66.229877	2313.051371	20.840115
65.823055	2317.522112	20.845133
66.007245	2305.089537	20.850151
65.856912	2308.404768	20.855168
66.067093	2305.382476	20.860186
66.580971	2305.259241	20.865203
66.208753	2313.105895	20.870221
66.213383	2306.771426	20.875239
66.369934	2306.239224	20.880256
66.509720	2330.152611	20.885274
66.386088	2333.829585	20.890291
66.317776	2345.850932	20.895309
67.158520	2343.499068	20.900327
66.802737	2339.835404	20.905344
66.954701	2341.790688	20.910362
67.328756	2331.885434	20.915379
67.019151	2330.966219	20.920397
67.338268	2329.996845	20.925415
67.329272	2332.189418	20.930432
67.067952	2336.560086	20.935450
67.099374	2327.261590	20.940467
67.341301	2338.010250	20.945485
67.633275	2323.953835	20.950503
67.401837	2320.678267	20.955520
67.180672	2338.512576	20.960538
67.608492	2327.509397	20.965555
67.486546	2327.355997	20.970573
67.486015	2329.479055	20.975591
67.707053	2349.235132	20.980608
67.761062	2362.478816	20.985626
67.681208	2353.081794	20.990643
67.557454	2355.667010	20.995661
67.678057	2348.692821	21.000679
67.787933	2353.189838	21.005696
67.519887	2356.268652	21.010714
67.789106	2371.907140	21.015731
67.964049	2380.823131	21.020749
68.347100	2382.485423	21.025767
68.180591	2385.430889	21.030784
68.244797	2386.095134	21.035802
68.385720	2369.701762	21.040819
68.226106	2384.842341	21.045837
68.897937	2395.745856	21.050855
69.271169	2403.997109	21.055872
69.239625	2405.911916	21.060890
69.163154	2381.500583	21.065907
68.913014	2369.246961	21.070925
69.137719	2382.812417	21.075943
69.276630	2393.066335	21.080960
69.186950	2396.960941	21.085978
69.471259	2395.162247	21.090995
69.484902	2401.002442	21.096013
69.608062	2397.172059	21.101031
69.792472	2400.038559	21.106048
69.753998	2394.274605	21.111066
69.722756	2375.002504	21.116083
69.476331	2369.874200	21.121101
69.666327	2381.497671	21.126119
69.806964	2382.122095	21.131136
69.939207	2398.016371	21.136154
70.050382	2388.745580	21.141171
69.969138	2396.122031	21.146189
69.855380	2388.981893	21.151207
70.037458	2391.872795	21.156224
69.803409	2404.347633	21.161242
69.747565	2390.460564	21.166259
69.861108	2421.294130	21.171277
70.386549	2426.948016	21.176295
70.492476	2424.674103	21.181312
70.353321	2425.396824	21.186330
70.693256	2420.320640	21.191347
70.382147	2429.961262	21.196365
70.366616	2428.341743	21.201383
70.548294	2436.305815	21.206400
70.466748	2448.286123	21.211418
70.938983	2442.074188	21.216435
71.013337	2453.833796	21.221453
70.997506	2447.566047	21.226471
71.167357	2447.937197	21.231488
70.934119	2455.674293	21.236506
71.201152	2460.281154	21.241523
71.187218	2479.204207	21.246541
71.277330	2472.191702	21.251559
71.715519	2482.168950	21.256576
71.465454	2477.447928	21.261594
71.438961	2476.173938	21.266611
71.500933	2465.235961	21.271629
71.822753	2485.698005	21.276647
71.993827	2499.843734	21.281664
72.056059	2497.442391	21.286682
72.219197	2494.592035	21.291699
71.885236	2500.265004	21.296717
71.912471	2500.500705	21.301735
72.154781	2493.458661	21.306752
71.904560	2501.411594	21.311770
72.241530	2491.265122	21.316787
72.171587	2508.943872	21.321805
72.691419	2524.064221	21.326823
72.752403	2517.493945	21.331840
72.901889	2527.037893	21.336858
73.080384	2515.273061	21.341875
73.035025	2522.172343	21.346893
72.895787	2526.207084	21.351911
73.141480	2509.256818	21.356928
72.922864	2518.114815	21.361946
73.440421	2516.274732	21.366963
73.232115	2523.862842	21.371981
73.164497	2517.287873	21.376999
73.572176	2516.096334	21.382016
73.579567	2516.739674	21.387034
73.399338	2512.082674	21.392051
73.553164	2512.819886	21.397069
72.950052	2520.954099	21.402087
73.147270	2507.927833	21.407104
73.252771	2525.436207	21.412122
73.359631	2537.696824	21.417139
73.677126	2539.522752	21.422157
73.428074	2543.149670	21.427175
73.920269	2532.540437	21.432192
73.948094	2551.655888	21.437210
73.957009	2561.471966	21.442227
74.496934	2571.989154	21.447245
74.271419	2577.584349	21.452263
74.430008	2571.742818	21.457280
74.051064	2575.722766	21.462298
74.219184	2570.429690	21.467315
74.461340	2574.149312	21.472333
74.392970	2594.546567	21.477351
74.764552	2593.197997	21.482368
74.715864	2607.372335	21.487386
74.873478	2594.080097	21.492403
75.056061	2593.664449	21.497421
75.017128	2598.479895	21.502439
75.495738	2591.238829	21.507456
75.541475	2596.928893	21.512474
75.577882	2589.329128	21.517491
75.487810	2596.044495	21.522509
75.343918	2597.879101	21.527527
75.572758	2592.756685	21.532544
75.544156	2594.675358	21.537562
75.875791	2609.208014	21.542579
75.853634	2619.222591	21.547597
75.799334	2625.315867	21.552615
76.170147	2623.861115	21.557632
76.355797	2617.204798	21.562650
76.278412	2612.352776	21.567667
76.310254	2615.814298	21.572685
75.899786	2614.610171	21.577703
76.770761	2616.596453	21.582720
76.175473	2612.221149	21.587738
76.519704	2615.324237	21.592755
76.235736	2610.934398	21.597773
76.232899	2612.405867	21.602791
76.757187	2611.863166	21.607808
76.534637	2611.685472	21.612826
76.901474	2619.766236	21.617843
77.155056	2634.881954	21.622861
76.938950	2640.248828	21.627879
77.295783	2623.303267	21.632896
77.099282	2622.883450	21.637914
77.166511	2632.686767	21.642931
77.131816	2625.020799	21.647949
76.959400	2630.525720	21.652967
77.292633	2624.782427	21.657984
77.273669	2634.741364	21.663002
77.637720	2632.694386	21.668019
77.641515	2643.889010	21.673037
77.379212	2664.396030	21.678055
77.601054	2668.922636	21.683072
77.635250	2662.120498	21.688090
77.514508	2660.451047	21.693107
77.662957	2662.961322	21.698125
77.616706	2669.297393	21.703143
78.006992	2670.555736	21.708160
78.320671	2683.916554	21.713178
78.251368	2682.125584	21.718195
78.571786	2680.173231	21.723213
78.459989	2690.462556	21.728231
78.543530	2675.233561	21.733248
78.435293	2678.534026	21.738266
78.432279	2680.273264	21.743283
79.029999	2690.628986	21.748301
79.065550	2701.547903	21.753319
78.969907	2709.048547	21.758336
78.990980	2714.475790	21.763354
78.761017	2712.769689	21.768371
78.947910	2708.699134	21.773389
78.777991	2717.753919	21.778407
79.166475	2717.280160	21.783424
79.328218	2739.199063	21.788442
79.404462	2738.532889	21.793459
79.951674	2733.570722	21.798477
79.948845	2738.857432	21.803495
80.148778	2743.735743	21.808512
79.731782	2735.824334	21.813530
79.888369	2731.429240	21.818547
79.877363	2734.753778	21.823565
80.135557	2735.553255	21.828583
80.404488	2726.464821	21.833600
79.849038	2722.304952	21.838618
79.778238	2731.073236	21.843635
80.198340	2746.802089	21.848653
80.231348	2762.211557	21.853671
80.337643	2765.449746	21.858688
80.546998	2758.922919	21.863706
80.755138	2760.934315	21.868723
80.720454	2753.889980	21.873741
80.660298	2768.534901	21.878759
80.858852	2775.823076	21.883776
81.376572	2781.428369	21.888794
81.506481	2786.201743	21.893811
81.388915	2772.060360	21.898829
81.388941	2782.907651	21.903847
81.331466	2773.398395	21.908864
81.945199	2768.119275	21.913882
81.963443	2775.602276	21.918899
81.988061	2760.669195	21.923917
81.930902	2773.963527	21.928935
82.263728	2770.444821	21.933952
82.502016	2762.820208	21.938970
82.061043	2756.465233	21.943987
81.968012	2737.999034	21.949005
82.119800	2760.015685	21.954023
82.337235	2756.557822	21.959040
82.167777	2765.866121	21.964058
82.206944	2764.928111	21.969075
82.550602	2750.740307	21.974093
82.552354	2767.902326	21.979111
82.414903	2751.676305	21.984128
82.473304	2761.463841	21.989146
82.233250	2765.788584	21.994163
82.457401	2769.060021	21.999181
82.411555	2789.450652	22.004199
82.753726	2787.402552	22.009216
82.870402	2793.093148	22.014234
82.869515	2800.220247	22.019251
82.728463	2802.206780	22.024269
83.126798	2818.237364	22.029287
83.174536	2820.421399	22.034304
83.049691	2819.220362	22.039322
83.288666	2826.981827	22.044339
83.566785	2831.885806	22.049357
83.382322	2850.211511	22.054375
83.680046	2841.836410	22.059392
84.050040	2852.014573	22.064410
83.889372	2839.867822	22.069427
83.790297	2840.284690	22.074445
83.502659	2840.161868	22.079463
84.105083	2853.783711	22.084480
84.291550	2870.301037	22.089498
84.323381	2871.230920	22.094515
84.530497	2864.756392	22.099533
84.443148	2865.106747	22.104551
84.704713	2872.131365	22.109568
84.812448	2860.434294	22.114586
84.307134	2865.923149	22.119603
84.810682	2868.936914	22.124621
84.920759	2885.424775	22.129639
84.918419	2897.304905	22.134656
85.189927	2902.184015	22.139674
84.822030	2905.813762	22.144691
85.451026	2897.202667	22.149709
85.380037	2896.046254	22.154727
85.256462	2894.833583	22.159744
85.482974	2906.493531	22.164762
85.379144	2920.332766	22.169779
85.973304	2913.635856	22.174797
86.113831	2921.462884	22.179815
86.187137	2922.862321	22.184832
86.073593	2919.684438	22.189850
85.914301	2931.283861	22.194867
86.209895	2922.156645	22.199885
86.208762	2917.378130	22.204903
86.555916	2913.372334	22.209920
86.594167	2912.390764	22.214938
86.257382	2914.325065	22.219955
87.032028	2929.825311	22.224973
87.150802	2924.049300	22.229991
87.060543	2918.601626	22.235008
86.959150	2907.536437	22.240026
86.569745	2917.755329	22.245043
86.962643	2935.500462	22.250061
86.916425	2933.330019	22.255079
87.084019	2955.645141	22.260096
87.199414	2955.625288	22.265114
86.999955	2942.128859	22.270131
87.375497	2958.263370	22.275149
87.164592	2974.388292	22.280167
87.630339	2970.102982	22.285184
87.878054	2962.240471	22.290202
87.681224	2972.029055	22.295219
87.863478	2965.434575	22.300237
87.974810	2966.947416	22.305255
87.867753	2968.769666	22.310272
87.651811	2983.276000	22.315290
87.659945	3003.207147	22.320307
87.909558	2989.120532	22.325325
87.975900	3006.174472	22.330343
88.443655	3014.161167	22.335360
88.873183	3008.625040	22.340378
88.588885	3016.184627	22.345395
89.138320	3022.412373	22.350413
89.347706	3019.044377	22.355431
89.353241	3013.411896	22.360448
89.407091	3011.121321	22.365466
89.740434	3018.961755	22.370483
89.953987	2990.942470	22.375501
89.631730	2979.306658	22.380519
89.166087	2980.320881	22.385536
89.363943	2973.851385	22.390554
89.558041	2976.105313	22.395571
89.578314	2992.316005	22.400589
89.595943	3004.081088	22.405607
89.562280	2999.472909	22.410624
89.786706	3005.371748	22.415642
89.378578	3005.835457	22.420659
89.531694	3009.902240	22.425677
89.711557	3026.549578	22.430695
89.884774	3039.550852	22.435712
90.323996	3037.991029	22.440730
90.217918	3037.053427	22.445747
90.022573	3056.706886	22.450765
90.366841	3058.520964	22.455783
90.502348	3063.435242	22.460800
90.541748	3061.830580	22.465818
90.727821	3077.521737	22.470835
91.141196	3066.646824	22.475853
91.615477	3062.367164	22.480871
91.533737	3075.423674	22.485888
91.594304	3077.309532	22.490906
91.839966	3065.867843	22.495923
91.527133	3043.615667	22.500941
91.780916	3047.937472	22.505959
91.725294	3056.665627	22.510976
92.213140	3062.611827	22.515994
92.335233	3062.337298	22.521011
92.298372	3038.812554	22.526029
92.219635	3031.051306	22.531047
92.269715	3027.777406	22.536064
92.387731	3017.412886	22.541082
92.379999	3034.433449	22.546099
92.131671	3057.334555	22.551117
92.641750	3054.157341	22.556135
92.547016	3060.109042	22.561152
92.460779	3062.914561	22.566170
92.318802	3065.971851	22.571187
92.837174	3059.159856	22.576205
92.598475	3064.600700	22.581223
92.480068	3077.555399	22.586240
92.870445	3075.060659	22.591258
92.831161	3081.518983	22.596275
92.933927	3092.029371	22.601293
92.974619	3102.979612	22.606311
93.073857	3125.053908	22.611328
93.296381	3116.619451	22.616346
93.039660	3123.688651	22.621363
93.358287	3150.010536	22.626381
93.496724	3145.864418	22.631399
93.525718	3156.517391	22.636416
94.136150	3151.364296	22.641434
94.212513	3171.738342	22.646451
94.490759	3171.853747	22.651469
94.712819	3175.287444	22.656487
94.643565	3175.643078	22.661504
94.709259	3167.370793	22.666522
95.292122	3170.823895	22.671539
95.181928	3160.167898	22.676557
95.301947	3129.389957	22.681575
94.743272	3138.493206	22.686592
95.237405	3130.463423	22.691610
95.165177	3127.509781	22.696627
94.931317	3131.035883	22.701645
95.155676	3140.077213	22.706663
95.227607	3163.660562	22.711680
95.016509	3162.359988	22.716698
95.430649	3179.526236	22.721715
95.145250	3170.717531	22.726733
95.547084	3170.009639	22.731751
95.408612	3184.976215	22.736768
95.744956	3181.750567	22.741786
95.579170	3189.620570	22.746803
95.442636	3194.314549	22.751821
95.878399	3210.297212	22.756839
95.896437	3223.836195	22.761856
96.454058	3221.205464	22.766874
96.209646	3224.130910	22.771891
96.073896	3220.938136	22.776909
96.430406	3235.959437	22.781927
96.346585	3242.278336	22.786944
96.843506	3247.892757	22.791962
96.838408	3247.845604	22.796979
96.636154	3250.047465	22.801997
96.961241	3258.458344	22.807015
96.989912	3269.442190	22.812032
97.497342	3266.154731	22.817050
97.391915	3268.049588	22.822067
97.621523	3264.358473	22.827085
97.694381	3268.836292	22.832103
97.427333	3277.827158	22.837120
97.607198	3275.825556	22.842138
97.830545	3278.910601	22.847155
98.150301	3294.286506	22.852173
98.403073	3287.395934	22.857191
98.569831	3282.767876	22.862208
99.073580	3280.759112	22.867226
98.917390	3281.101186	22.872243
98.852042	3275.536652	22.877261
99.185492	3275.429510	22.882279
98.863796	3277.748798	22.887296
99.252292	3273.818754	22.892314
99.257156	3275.902067	22.897331
98.873456	3277.114967	22.902349
99.152418	3273.604675	22.907367
98.986797	3273.564412	22.912384
99.073600	3280.837071	22.917402
98.922181	3281.287028	22.922419
98.959132	3301.894959	22.927437
99.309914	3292.272907	22.932455
98.997970	3306.289475	22.937472
99.376380	3319.715328	22.942490
99.710209	3335.302746	22.947507
99.682031	3341.518762	22.952525
100.305271	3340.117835	22.957543
100.233265	3346.554125	22.962560
100.149805	3354.714157	22.967578
100.191874	3368.046509	22.972595
100.346946	3372.834797	22.977613
100.531040	3368.895260	22.982631
100.617895	3368.274552	22.987648
100.453905	3362.092390	22.992666
100.634361	3381.049714	22.997683
100.798065	3396.521643	23.002701
101.303663	3394.750381	23.007719
101.260611	3398.941487	23.012736
101.469807	3384.721036	23.017754
101.737693	3394.012423	23.022771
101.358935	3392.512396	23.027789
101.726576	3383.988802	23.032807
101.708063	3395.973968	23.037824
101.859960	3388.828369	23.042842
102.010343	3389.558714	23.047859
102.159789	3413.238279	23.052877
102.282335	3404.473725	23.057895
101.944799	3421.055554	23.062912
102.497320	3410.233359	23.067930
102.466554	3411.757170	23.072947
102.502453	3418.011432	23.077965
102.764381	3406.190381	23.082983
102.516535	3413.348015	23.088000
102.807152	3404.627690	23.093018
102.821646	3405.993989	23.098035
102.670124	3413.134888	23.103053
103.118620	3430.428418	23.108071
103.179674	3436.367069	23.113088
103.219717	3438.257156	23.118106
103.311711	3439.580703	23.123123
103.040908	3443.243714	23.128141
103.226473	3442.501531	23.133159
103.653126	3458.125679	23.138176
103.471443	3465.828353	23.143194
103.782991	3463.673415	23.148211
103.756207	3477.185783	23.153229
104.043178	3472.398380	23.158247
104.126745	3494.943959	23.163264
104.139296	3502.604256	23.168282
104.503626	3493.842540	23.173299
104.430599	3492.732883	23.178317
104.414813	3488.942563	23.183335
104.544535	3506.627578	23.188352
104.795522	3521.116165	23.193370
104.905468	3510.870781	23.198387
105.002402	3517.311063	23.203405
104.898467	3514.866202	23.208423
105.164879	3529.110876	23.213440
105.652849	3538.757691	23.218458
105.679068	3536.075897	23.223475
105.833125	3543.684830	23.228493
106.256066	3532.567432	23.233511
106.404493	3533.077215	23.238528
106.187526	3532.674540	23.243546
106.272786	3534.793007	23.248563
105.935172	3533.139285	23.253581
106.140761	3534.918107	23.258599
106.305588	3531.153787	23.263616
106.486455	3541.205035	23.268634
106.528468	3527.990206	23.273651
106.600412	3538.005937	23.278669
106.701397	3548.197202	23.283687
106.933226	3556.471696	23.288704
106.661849	3569.448190	23.293722
107.028943	3562.567708	23.298739
106.922296	3563.750115	23.303757
107.133435	3572.433605	23.308775
107.373018	3580.443803	23.313792
107.370021	3589.173385	23.318810
107.528029	3582.983893	23.323827
107.503273	3592.624674	23.328845
107.993915	3593.928302	23.333863
107.850067	3609.370249	23.338880
107.952662	3618.719061	23.343898
108.538184	3607.527443	23.348915
108.388092	3608.345346	23.353933
108.707377	3608.038948	23.358951
108.766262	3604.826864	23.363968
108.758541	3607.318261	23.368986
108.585623	3608.431319	23.374003
108.721196	3617.097419	23.379021
108.953593	3604.579051	23.384039
108.765281	3597.437314	23.389056
108.507102	3612.421360	23.394074
109.109152	3622.921500	23.399091
108.845174	3632.017978	23.404109
109.173234	3625.275051	23.409127
108.973962	3639.204355	23.414144
109.154553	3656.696054	23.419162
109.558571	3657.195419	23.424179
109.342271	3667.258561	23.429197
109.835663	3674.771215	23.434215
110.117128	3688.229187	23.439232
110.113658	3683.163385	23.444250
110.818086	3678.108354	23.449267
110.264976	3683.966867	23.454285
110.393666	3680.733761	23.459303
110.588324	3687.918665	23.464320
110.762802	3701.117947	23.469338
111.045368	3707.168472	23.474355
111.244248	3710.349792	23.479373
111.128429	3703.735840	23.484391
111.283948	3705.149693	23.489408
111.333199	3702.980268	23.494426
111.767911	3699.566160	23.499443
111.762947	3705.056727	23.504461
111.634754	3701.559412	23.509479
111.576942	3700.677173	23.514496
111.745983	3714.619197	23.519514
112.146823	3720.901754	23.524531
111.878917	3730.679740	23.529549
112.030509	3734.057897	23.534567
111.968386	3731.892337	23.539584
111.982077	3733.359993	23.544602
112.907203	3749.918973	23.549619
112.808863	3762.275165	23.554637
112.776692	3760.501548	23.559655
112.890013	3759.505527	23.564672
112.768663	3767.967363	23.569690
113.003408	3765.616804	23.574707
112.928852	3780.534779	23.579725
113.275774	3779.037419	23.584743
113.449747	3788.698970	23.589760
113.182057	3786.504436	23.594778
113.415174	3780.560341	23.599795
113.553387	3810.910219	23.604813
113.953453	3816.616878	23.609831
114.287015	3819.257347	23.614848
114.083963	3814.502537	23.619866
114.005194	3814.588069	23.624883
113.930088	3821.725952	23.629901
114.401581	3827.190049	23.634919
114.784253	3844.579988	23.639936
114.771986	3842.474673	23.644954
115.091440	3835.868927	23.649971
114.608596	3837.797200	23.654989
115.020987	3836.955232	23.660007
115.362563	3835.111854	23.665024
115.238853	3858.791642	23.670042
115.816394	3862.760818	23.675059
115.560011	3871.658905	23.680077
115.790069	3866.844580	23.685095
115.450485	3865.755008	23.690112
115.567432	3865.965246	23.695130
115.950191	3862.971969	23.700147
116.121703	3867.754145	23.705165
116.191073	3877.849270	23.710183
116.392909	3885.493380	23.715200
116.373524	3886.038046	23.720218
116.582211	3881.387514	23.725235
116.519603	3881.707806	23.730253
116.600800	3887.599587	23.735271
117.146781	3879.422239	23.740288
116.470590	3880.974987	23.745306
116.826434	3892.926512	23.750323
117.137086	3916.410835	23.755341
116.821921	3910.058179	23.760359
116.916968	3906.607335	23.765376
116.743421	3933.543205	23.770394
117.282227	3937.992506	23.775411
117.905244	3938.463500	23.780429
117.709245	3945.983713	23.785447
118.300972	3961.488897	23.790464
118.120241	3968.523056	23.795482
118.218489	3974.899128	23.800499
118.247536	3964.425072	23.805517
118.314396	3967.956305	23.810535
118.407726	3960.729578	23.815552
118.476515	3979.042236	23.820570
118.834583	3976.625159	23.825587
118.766831	3988.567348	23.830605
118.662242	3987.257731	23.835623
119.106772	3997.548735	23.840640
119.081787	4011.840912	23.845658
119.145432	4011.472092	23.850675
119.219233	4022.351343	23.855693
119.045266	4026.631230	23.860711
119.624492	4044.178250	23.865728
119.872398	4042.635439	23.870746
120.112862	4038.493459	23.875763
119.866317	4050.179425	23.880781
119.856816	4080.249508	23.885799
120.460327	4064.992141	23.890816
120.539140	4080.240575	23.895834
120.527316	4073.156422	23.900851
120.781685	4072.989132	23.905869
120.833053	4089.467508	23.910887
121.605487	4093.093800	23.915904
121.209403	4103.263374	23.920922
121.486191	4084.283105	23.925939
121.427051	4091.787029	23.930957
121.399448	4093.617123	23.935975
121.550735	4092.366725	23.940992
121.515692	4095.421867	23.946010
121.885989	4112.128612	23.951027
121.901503	4113.706649	23.956045
121.887144	4127.530169	23.961063
122.379950	4121.152339	23.966080
122.072432	4128.559584	23.971098
122.430035	4140.415717	23.976115
122.633865	4154.301578	23.981133
122.690460	4152.652612	23.986151
123.217920	4153.426883	23.991168
122.934767	4152.466551	23.996186
122.960427	4146.487363	24.001203
123.247637	4162.921258	24.006221
123.198366	4174.930618	24.011239
123.511494	4168.045421	24.016256
123.342073	4186.486750	24.021274
123.553201	4184.212099	24.026291
123.592644	4183.350350	24.031309
123.707794	4195.862514	24.036327
124.077807	4206.786568	24.041344
124.258236	4208.120741	24.046362
124.041467	4206.105936	24.051379
124.298837	4210.810607	24.056397
124.415050	4224.903981	24.061415
124.928544	4232.491938	24.066432
124.787192	4237.112997	24.071450
124.720071	4239.801762	24.076467
124.819983	4236.802085	24.081485
124.939352	4233.195149	24.086503
125.219229	4224.215870	24.091520
125.447203	4253.205063	24.096538
125.131173	4254.519053	24.101555
125.477699	4260.838386	24.106573
125.495284	4262.949256	24.111591
125.686989	4262.193814	24.116608
125.780861	4286.691124	24.121626
126.085788	4297.979621	24.126643
126.185023	4291.064417	24.131661
125.719929	4296.515601	24.136679
125.883346	4298.425925	24.141696
126.571869	4321.717565	24.146714
126.225626	4320.952738	24.151731
126.606320	4332.609885	24.156749
126.773175	4354.993280	24.161767
127.205528	4338.945734	24.166784
127.234549	4353.556108	24.171802
127.308916	4356.883789	24.176819
127.637953	4366.421583	24.181837
127.853593	4376.619213	24.186855
127.877508	4363.237357	24.191872
128.065579	4362.089529	24.196890
128.200965	4365.481137	24.201907
128.133198	4360.053650	24.206925
127.912049	4367.538849	24.211943
128.909256	4393.535094	24.216960
129.221388	4398.383538	24.221978
128.902210	4399.512201	24.226995
128.992093	4398.313685	24.232013
128.524292	4409.609700	24.237031
128.799405	4401.797458	24.242048
128.942453	4413.359339	24.247066
129.543248	4408.167668	24.252083
129.743507	4412.961397	24.257101
129.341124	4426.743889	24.262119
129.767595	4414.514459	24.267136
129.761453	4420.831603	24.272154
129.458688	4446.538339	24.277171
129.966717	4441.853443	24.282189
129.739714	4450.387871	24.287207
130.056509	4461.891884	24.292224
130.354342	4470.703279	24.297242
130.500554	4477.472475	24.302259
130.637427	4469.521640	24.307277
130.948741	4492.841333	24.312295
131.292198	4498.565098	24.317312
131.166863	4500.285413	24.322330
131.428888	4500.825644	24.327347
131.631673	4499.403667	24.332365
131.669731	4498.090867	24.337383
131.610795	4497.305242	24.342400
131.798422	4503.217830	24.347418
132.109341	4527.458282	24.352435
132.244520	4519.045412	24.357453
132.150792	4526.311918	24.362471
132.333561	4515.020560	24.367488
132.687080	4519.541659	24.372506
132.532806	4517.411723	24.377523
132.923826	4533.703601	24.382541
133.192199	4550.949046	24.387559
132.940733	4544.700567	24.392576
132.681553	4547.430631	24.397594
132.522375	4556.558725	24.402611
133.155925	4556.312905	24.407629
133.191202	4577.238597	24.412647
133.600910	4575.107425	24.417664
133.539931	4578.214207	24.422682
133.175149	4592.118989	24.427699
133.658845	4592.575271	24.432717
133.565116	4611.486547	24.437735
134.185971	4614.847454	24.442752
134.740035	4625.137279	24.447770
134.717341	4622.717777	24.452787
135.353502	4622.674713	24.457805
135.320871	4619.836303	24.462823
135.351173	4627.246132	24.467840
135.348125	4628.875335	24.472858
135.302563	4623.456681	24.477875
135.352146	4615.211503	24.482893
135.509433	4626.104915	24.487911
135.728483	4630.992469	24.492928
135.831816	4642.760346	24.497946
135.587773	4655.885992	24.502963
136.173292	4653.935982	24.507981
135.775779	4667.495786	24.512999
135.941652	4666.816270	24.518016
136.321079	4677.395722	24.523034
136.340062	4680.738940	24.528051
136.306048	4676.965921	24.533069
136.691220	4711.224669	24.538087
137.009391	4712.528994	24.543104
137.131099	4717.034974	24.548122
137.008873	4720.736291	24.553139
137.292128	4731.875116	24.558157
137.468433	4740.914699	24.563175
137.569442	4745.516258	24.568192
137.730644	4745.217115	24.573210
137.813819	4772.215088	24.578227
137.978370	4775.457047	24.583245
138.162038	4774.936030	24.588263
138.399370	4774.143871	24.593280
138.687120	4784.217208	24.598298
138.701349	4797.475840	24.603315
138.983201	4796.387274	24.608333
138.934390	4801.632677	24.613351
139.003370	4813.450472	24.618368
139.608054	4797.634613	24.623386
139.384468	4802.728599	24.628403
139.369545	4817.085997	24.633421
139.464137	4822.321053	24.638439
139.704520	4837.486770	24.643456
140.074086	4834.626628	24.648474
139.841643	4833.516882	24.653491
140.347788	4841.783659	24.658509
140.158748	4853.237030	24.663527
140.269047	4847.913779	24.668544
140.642148	4846.080033	24.673562
140.611278	4871.680231	24.678579
140.876752	4869.249212	24.683597
141.123212	4876.326460	24.688615
140.600835	4873.272959	24.693632
140.955907	4883.922739	24.698650
141.146677	4905.189342	24.703667
141.620105	4898.267052	24.708685
141.637866	4905.857079	24.713703
141.841050	4922.193059	24.718720
142.087867	4926.499609	24.723738
142.028280	4932.597412	24.728755
142.419061	4927.591557	24.733773
142.157300	4931.815341	24.738791
142.417293	4954.284192	24.743808
142.742774	4955.056507	24.748826
142.522602	4957.204470	24.753843
143.085642	4944.206194	24.758861
142.930229	4958.463331	24.763879
143.053279	4980.564257	24.768896
143.369765	4979.812539	24.773914
143.345819	4990.294380	24.778931
143.491325	4986.506531	24.783949
143.758221	5003.145501	24.788967
144.266426	5013.414035	24.793984
144.085646	5006.283401	24.799002
144.143945	5010.838554	24.804019
144.506028	5010.876308	24.809037
144.629718	5018.768606	24.814055
144.542451	5036.175847	24.819072
144.859081	5039.358030	24.824090
144.917761	5041.261370	24.829107
145.270052	5033.485658	24.834125
145.297782	5036.020242	24.839143
145.356581	5061.194003	24.844160
145.714267	5061.676677	24.849178
145.550354	5072.058883	24.854195
146.079186	5061.613193	24.859213
146.212382	5060.846924	24.864231
145.964909	5081.699597	24.869248
146.519214	5089.131578	24.874266
146.072197	5098.693550	24.879283
146.543465	5098.256435	24.884301
146.665701	5102.771102	24.889319
146.463854	5110.965426	24.894336
146.978603	5109.098749	24.899354
147.073865	5128.320378	24.904371
147.247137	5128.730412	24.909389
147.515674	5144.328083	24.914407
147.305607	5153.968997	24.919424
147.308236	5154.494704	24.924442
147.752207	5171.970874	24.929459
148.415961	5157.316010	24.934477
148.332602	5165.928641	24.939495
148.331182	5173.705478	24.944512
148.928287	5172.136254	24.949530
148.806253	5198.666455	24.954547
149.025541	5195.404259	24.959565
149.268859	5196.412287	24.964583
149.378335	5202.874421	24.969600
149.572985	5204.240193	24.974618
149.327597	5206.133249	24.979635
149.580570	5209.742636	24.984653
149.946617	5227.721646	24.989671
149.782245	5233.689634	24.994688
150.097275	5218.890824	24.999706
150.177986	5225.705053	25.004723
150.441918	5233.450591	25.009741
150.229225	5256.157220	25.014759
150.207936	5254.476142	25.019776
150.355071	5254.450248	25.024794
150.474028	5270.796596	25.029811
150.695623	5275.687081	25.034829
151.153781	5286.838300	25.039847
150.940669	5309.062284	25.044864
151.196982	5313.995864	25.049882
151.192697	5329.464827	25.054899
151.603142	5330.112834	25.059917
152.081641	5331.665540	25.064935
151.841707	5346.188259	25.069952
152.101015	5343.555779	25.074970
152.591526	5363.921209	25.079987
152.489224	5368.848018	25.085005
152.783179	5369.876816	25.090023
152.796592	5375.919387	25.095040
152.963268	5367.826125	25.100058
153.174403	5379.797232	25.105075
153.449556	5382.513011	25.110093
153.724132	5387.861014	25.115111
153.669101	5395.983136	25.120128
153.742936	5381.150860	25.125146
153.922242	5378.013384	25.130163
153.683382	5401.115197	25.135181
154.124394	5408.903177	25.140199
154.208523	5415.646039	25.145216
154.302251	5420.448263	25.150234
154.500240	5439.098011	25.155251
154.687410	5452.921622	25.160269
155.086130	5444.545753	25.165287
154.821094	5455.297793	25.170304
155.010872	5475.381577	25.175322
155.294376	5480.286292	25.180339
155.148302	5487.397298	25.185357
155.646986	5500.340828	25.190375
155.570350	5507.854623	25.195392
156.042691	5512.851739	25.200410
156.212645	5527.078364	25.205427
156.178758	5540.495230	25.210445
156.034971	5543.980568	25.215463
156.430091	5553.508146	25.220480
156.977688	5563.181397	25.225498
157.127507	5567.554590	25.230515
157.312275	5569.067736	25.235533
157.509077	5571.653964	25.240551
157.176127	5595.162286	25.245568
157.235842	5590.078715	25.250586
157.832266	5603.789813	25.255603
157.877640	5618.681403	25.260621
158.009778	5624.956447	25.265639
158.151383	5625.822247	25.270656
158.780126	5616.893903	25.275674
158.510731	5635.198316	25.280691
158.984100	5646.468564	25.285709
159.041262	5647.169559	25.290727
159.329613	5652.240498	25.295744
159.422433	5646.297666	25.300762
159.345431	5660.903965	25.305779
159.062398	5670.037453	25.310797
159.835933	5668.118421	25.315815
159.431406	5678.180923	25.320832
159.919309	5687.535701	25.325850
160.291160	5707.445507	25.330867
160.037742	5706.325780	25.335885
160.748224	5719.061943	25.340903
160.391519	5742.654752	25.345920
160.570966	5731.018105	25.350938
161.258717	5730.815289	25.355955
161.270840	5755.087409	25.360973
161.668198	5750.075483	25.365991
161.414982	5764.759881	25.371008
161.397589	5756.215666	25.376026
161.699241	5766.187306	25.381043
161.914117	5776.015797	25.386061
162.095629	5778.004432	25.391079
162.428188	5781.514140	25.396096
162.471751	5787.186426	25.401114
162.603445	5805.467955	25.406131
162.679191	5816.782098	25.411149
162.914531	5812.039559	25.416167
162.899924	5821.451617	25.421184
163.255503	5835.233506	25.426202
163.407783	5840.035616	25.431219
163.287035	5845.297999	25.436237
163.523439	5842.455787	25.441255
163.703736	5853.945614	25.446272
163.952665	5864.194621	25.451290
164.179829	5867.854904	25.456307
164.007546	5882.437800	25.461325
164.256723	5885.610847	25.466343
164.047117	5896.913216	25.471360
164.198091	5911.033063	25.476378
164.487932	5926.942241	25.481395
164.358220	5937.650151	25.486413
164.687326	5947.992268	25.491431
164.910850	5964.667789	25.496448
165.518030	5984.939098	25.501466
166.144784	5981.138290	25.506483
165.822147	5990.751090	25.511501
166.475619	5994.814188	25.516519
166.362795	6006.894535	25.521536
166.775311	6015.789418	25.526554
167.024680	6015.167698	25.531571
166.999483	6015.415284	25.536589
167.349890	6007.531505	25.541607
167.276241	6013.384739	25.546624
167.495459	6034.196849	25.551642
167.942174	6036.591346	25.556659
167.577732	6038.539650	25.561677
167.855339	6038.373226	25.566695
168.306657	6047.674418	25.571712
168.402482	6058.087520	25.576730
168.449337	6062.284140	25.581747
168.636429	6069.071671	25.586765
168.874709	6062.439848	25.591783
169.225383	6061.498120	25.596800
169.150969	6087.176020	25.601818
169.328106	6091.656678	25.606835
169.326870	6101.390403	25.611853
169.433189	6101.328735	25.616871
169.638490	6108.129808	25.621888
169.912127	6125.790401	25.626906
169.815527	6126.846100	25.631923
169.567800	6140.056286	25.636941
170.244643	6142.396950	25.641959
170.342095	6149.387598	25.646976
170.962734	6175.623212	25.651994
171.328354	6174.857008	25.657011
170.588790	6191.043985	25.662029
171.225242	6179.280946	25.667047
171.530316	6196.858438	25.672064
171.589907	6213.032073	25.677082
171.834682	6209.489780	25.682100
171.736722	6216.434833	25.687117
171.719588	6224.249443	25.692135
172.094110	6241.590226	25.697152
172.045246	6250.092980	25.702170
172.489344	6261.098357	25.707188
172.311185	6271.488432	25.712205
172.555476	6288.784664	25.717223
172.708179	6293.915287	25.722240
172.953012	6318.847592	25.727258
173.532698	6328.007978	25.732276
173.195333	6340.448682	25.737293
173.627199	6347.813320	25.742311
174.050251	6358.642668	25.747328
174.441308	6360.671514	25.752346
174.648577	6347.589219	25.757364
174.981283	6342.616167	25.762381
175.397059	6341.339928	25.767399
175.481094	6350.156268	25.772416
175.284001	6336.256404	25.777434
175.207643	6345.730980	25.782452
175.285409	6357.822575	25.787469
175.768165	6370.899422	25.792487
175.804706	6370.303470	25.797504
175.673793	6382.977828	25.802522
175.994445	6385.582283	25.807540
176.054420	6407.878381	25.812557
176.194993	6402.991465	25.817575
176.329478	6419.933464	25.822592
176.447033	6436.838902	25.827610
176.683864	6441.514566	25.832628
176.606577	6457.660700	25.837645
176.385811	6474.202372	25.842663
176.942670	6483.823462	25.847680
176.935472	6510.250209	25.852698
177.469876	6509.221331	25.857716
177.815632	6530.117115	25.862733
178.178847	6537.007228	25.867751
178.143935	6555.482610	25.872768
178.496972	6565.190265	25.877786
178.876767	6559.406737	25.882804
178.594889	6577.271642	25.887821
179.110349	6588.998738	25.892839
179.482651	6596.485200	25.897856
179.317612	6593.846363	25.902874
179.576893	6594.829001	25.907892
179.904451	6616.180023	25.912909
180.089852	6613.104310	25.917927
180.353446	6621.595707	25.922944
180.365998	6625.436623	25.927962
180.457373	6635.742145	25.932980
180.248162	6640.034869	25.937997
180.727423	6654.280619	25.943015
181.110801	6661.425012	25.948032
180.974823	6672.033634	25.953050
181.659593	6680.145004	25.958068
181.588745	6693.711530	25.963085
181.923030	6700.408803	25.968103
182.279079	6695.831908	25.973120
182.114141	6712.342530	25.978138
182.190960	6729.385774	25.983156
182.285310	6731.355091	25.988173
182.359085	6741.521818	25.993191
182.707409	6757.426877	25.998208
182.738402	6771.144382	26.003226
183.086115	6784.625155	26.008244
183.356795	6793.397454	26.013261
183.289029	6799.101922	26.018279
183.831069	6803.607444	26.023296
184.060757	6828.216179	26.028314
184.360844	6816.050726	26.033332
184.076733	6838.241344	26.038349
184.194096	6846.352999	26.043367
184.656495	6852.496668	26.048384
184.628371	6875.365673	26.053402
185.226060	6878.853794	26.058420
184.836458	6882.006763	26.063437
184.929760	6902.480108	26.068455
185.661727	6908.675269	26.073472
185.439994	6918.687023	26.078490
186.124369	6930.297404	26.083508
186.261622	6935.240177	26.088525
186.029866	6955.012029	26.093543
186.705048	6954.704167	26.098560
186.869593	6967.123709	26.103578
187.066374	6971.072053	26.108596
187.443443	6961.630109	26.113613
187.371557	6980.275941	26.118631
188.130294	6989.169985	26.123648
187.809068	6994.027203	26.128666
188.252473	6992.105177	26.133684
188.093996	6996.743262	26.138701
188.417622	6991.047644	26.143719
188.286475	6995.765485	26.148736
188.215001	7013.785878	26.153754
188.455331	7016.536852	26.158772
188.881422	7032.394658	26.163789
188.843423	7045.492107	26.168807
189.307028	7048.391229	26.173824
189.156365	7072.144879	26.178842
189.574655	7071.262795	26.183860
190.088373	7081.211977	26.188877
189.940706	7092.288330	26.193895
190.400843	7102.043176	26.198912
190.140588	7104.510765	26.203930
190.289264	7121.192019	26.208948
190.549243	7130.876831	26.213965
190.504379	7147.673646	26.218983
191.257777	7155.105163	26.224000
191.176793	7168.385482	26.229018
191.393547	7183.248596	26.234036
191.940544	7199.910467	26.239053
191.863551	7204.111350	26.244071
192.107890	7216.753395	26.249088
192.191807	7227.997090	26.254106
192.053046	7235.310099	26.259124
192.558904	7252.553844	26.264141
192.900443	7266.165229	26.269159
193.120580	7273.990702	26.274176
193.028612	7297.849187	26.279194
193.308665	7299.306557	26.284212
193.924966	7317.566321	26.289229
193.898275	7324.061317	26.294247
194.312774	7322.875800	26.299264
194.166932	7344.904025	26.304282
194.493666	7344.730248	26.309300
194.377332	7355.080862	26.314317
194.912797	7380.773318	26.319335
195.347962	7378.758878	26.324352
195.206341	7390.400785	26.329370
195.534828	7406.244402	26.334388
195.620254	7419.194121	26.339405
195.799513	7425.769280	26.344423
196.327912	7435.846226	26.349440
196.551707	7446.115387	26.354458
196.768925	7437.306936	26.359476
197.150359	7452.240715	26.364493
197.072708	7465.414390	26.369511
197.487092	7465.053598	26.374528
197.274667	7469.716504	26.379546
197.780513	7474.076975	26.384564
197.818298	7494.583905	26.389581
197.584306	7501.442545	26.394599
198.226941	7490.519572	26.399616
198.249904	7509.227515	26.404634
198.159008	7523.638539	26.409652
198.713876	7530.803776	26.414669
199.181612	7555.732634	26.419687
199.055364	7562.109511	26.424704
199.165751	7560.220493	26.429722
199.015677	7567.909683	26.434740
199.712673	7570.057401	26.439757
199.606268	7588.018846	26.444775
199.962013	7588.906023	26.449792
199.940070	7615.652915	26.454810
199.981531	7623.729482	26.459828
200.455369	7628.726245	26.464845
200.502814	7652.469233	26.469863
200.891974	7650.923969	26.474880
200.837555	7674.854785	26.479898
201.174977	7682.124617	26.484916
201.444070	7689.037906	26.489933
201.630189	7712.836799	26.494951
201.994074	7708.738821	26.499968
202.123400	7726.670064	26.504986
201.974227	7734.905066	26.510004
202.137352	7741.041910	26.515021
202.197502	7765.324906	26.520039
202.661338	7778.145320	26.525056
202.764381	7799.995123	26.530074
203.093556	7809.234868	26.535092
203.640757	7821.019067	26.540109
203.480056	7836.825150	26.545127
204.013864	7854.702183	26.550144
203.889698	7865.260804	26.555162
204.435270	7865.155563	26.560180
205.093541	7885.797383	26.565197
205.022625	7892.591385	26.570215
205.295629	7880.342171	26.575232
205.364139	7900.100146	26.580250
205.536716	7911.391089	26.585268
206.069390	7920.942231	26.590285
205.923007	7923.827488	26.595303
206.060407	7933.200666	26.600320
206.209074	7946.568863	26.605338
206.491474	7948.015667	26.610356
206.786364	7956.230050	26.615373
207.108433	7972.417952	26.620391
207.046568	7974.913486	26.625408
207.318856	7994.236108	26.630426
207.422051	8001.017876	26.635444
207.744108	8009.088363	26.640461
207.765157	8041.231827	26.645479
208.308186	8037.498760	26.650496
208.283021	8048.540530	26.655514
208.545454	8052.955637	26.660532
208.753994	8059.552994	26.665549
208.932933	8083.711255	26.670567
209.189696	8089.856366	26.675584
209.405179	8096.946493	26.680602
209.548206	8114.237059	26.685620
209.903072	8115.531668	26.690637
209.708618	8134.752122	26.695655
210.030594	8155.718577	26.700672
210.533159	8170.057151	26.705690
210.885417	8177.061654	26.710708
211.117787	8180.432518	26.715725
210.944732	8201.700757	26.720743
211.150259	8210.633508	26.725760
211.158209	8223.206778	26.730778
211.283959	8239.866217	26.735796
211.758646	8246.818188	26.740813
211.986715	8265.484400	26.745831
212.234749	8284.064617	26.750848
212.331223	8297.525247	26.755866
212.641094	8319.763751	26.760884
212.963898	8319.056534	26.765901
213.152795	8345.849307	26.770919
213.177638	8346.234377	26.775936
213.413055	8362.548091	26.780954
213.650353	8380.321978	26.785972
214.141613	8379.728665	26.790989
213.983500	8390.960467	26.796007
214.416090	8406.489296	26.801024
214.327449	8416.513038	26.806042
214.686887	8429.568677	26.811060
215.258715	8436.975721	26.816077
214.666482	8447.323894	26.821095
215.481511	8467.033041	26.826112
215.503899	8480.075194	26.831130
215.819192	8492.192900	26.836148
215.977212	8502.256214	26.841165
216.395042	8512.545936	26.846183
216.703421	8532.748662	26.851200
217.187104	8533.754937	26.856218
217.168666	8540.507442	26.861236
217.202251	8545.522232	26.866253
217.335900	8551.177442	26.871271
217.904633	8554.510037	26.876288
218.267291	8561.739860	26.881306
218.394403	8578.738946	26.886324
218.666267	8575.272003	26.891341
218.708158	8592.599522	26.896359
218.895476	8597.855141	26.901376
218.876464	8603.084259	26.906394
219.324534	8612.253586	26.911412
219.541640	8631.268651	26.916429
219.722554	8640.644496	26.921447
220.054467	8643.233287	26.926464
219.979963	8659.763248	26.931482
219.987302	8679.808026	26.936500
220.539729	8696.529654	26.941517
220.855326	8700.220860	26.946535
220.974081	8714.881843	26.951552
221.200329	8734.892029	26.956570
221.064321	8746.936536	26.961588
221.206331	8761.314846	26.966605
221.500429	8776.197367	26.971623
221.803748	8797.697128	26.976640
222.442548	8815.388495	26.981658
222.279123	8841.040661	26.986676
222.527645	8842.308033	26.991693
222.886779	8862.075808	26.996711
223.114340	8871.003706	27.001728
223.277733	8876.607629	27.006746
223.565317	8902.801268	27.011764
224.128634	8903.839289	27.016781
224.091393	8925.993511	27.021799
224.673018	8929.138928	27.026816
225.056511	8933.552360	27.031834
225.031831	8955.028640	27.036852
225.431144	8954.148028	27.041869
225.568135	8950.600134	27.046887
225.901172	8962.197697	27.051904
226.047668	8973.137638	27.056922
225.857900	8984.114343	27.061940
226.295121	8981.980418	27.066957
226.227503	9009.940124	27.071975
226.725562	9022.722792	27.076992
227.005602	9030.031890	27.082010
226.822476	9048.180982	27.087028
227.442783	9046.201081	27.092045
227.149763	9063.749193	27.097063
227.363478	9078.022961	27.102080
227.687361	9093.440472	27.107098
227.853675	9115.214639	27.112116
228.176689	9129.876065	27.117133
228.281363	9143.535357	27.122151
228.340555	9164.181109	27.127168
228.639603	9168.710209	27.132186
228.794277	9190.565971	27.137204
229.521968	9209.600404	27.142221
229.505138	9211.999655	27.147239
229.754672	9226.593767	27.152256
230.059612	9232.255526	27.157274
230.413119	9258.977677	27.162292
230.388033	9270.055726	27.167309
230.724316	9289.837265	27.172327
230.609285	9310.148088	27.177344
231.153195	9315.248018	27.182362
231.192496	9346.561543	27.187380
231.668019	9349.619833	27.192397
231.659851	9359.963289	27.197415
231.704212	9386.004184	27.202432
232.051749	9400.230878	27.207450
232.214311	9420.674718	27.212468
232.719511	9428.730578	27.217485
233.162944	9453.602617	27.222503
233.321330	9470.160248	27.227520
233.586293	9474.634417	27.232538
233.577479	9510.696375	27.237556
233.950155	9507.908169	27.242573
234.709051	9529.815632	27.247591
234.595412	9538.914614	27.252608
234.989663	9544.461650	27.257626
234.888970	9555.813171	27.262644
235.161891	9568.024578	27.267661
235.398702	9583.712220	27.272679
235.195640	9593.268778	27.277696
235.670825	9618.404455	27.282714
235.910947	9633.706365	27.287732
236.034893	9656.800756	27.292749
236.238597	9675.408834	27.297767
236.495883	9697.745405	27.302784
237.020080	9717.579874	27.307802
237.423854	9735.522297	27.312820
237.718226	9747.800405	27.317837
238.036147	9755.203616	27.322855
238.346424	9777.383418	27.327872
238.622398	9782.582998	27.332890
238.683905	9802.442167	27.337908
238.925545	9815.450688	27.342925
239.213464	9819.951091	27.347943
239.086760	9849.161261	27.352960
239.474286	9855.975532	27.357978
239.731754	9871.500899	27.362996
240.165163	9880.145551	27.368013
240.453660	9907.238786	27.373031
240.414494	9917.621608	27.378048
241.116679	9923.185557	27.383066
241.088478	9944.407700	27.388084
241.219672	9948.865543	27.393101
241.752728	9969.667084	27.398119
241.588647	9980.804081	27.403136
242.073973	9988.688620	27.408154
242.292724	10011.804068	27.413172
242.195243	10013.175292	27.418189
242.778678	10029.956210	27.423207
242.714191	10045.821805	27.428224
243.171784	10055.507200	27.433242
243.011994	10070.196621	27.438260
243.512002	10094.790066	27.443277
243.991425	10108.594557	27.448295
243.720946	10135.683014	27.453312
244.056923	10139.850181	27.458330
244.154807	10159.825094	27.463348
244.741811	10177.116087	27.468365
245.144313	10188.075931	27.473383
245.399710	10197.334002	27.478400
245.494211	10213.976242	27.483418
245.543655	10232.162225	27.488436
245.834286	10245.502540	27.493453
246.372760	10257.319143	27.498471
246.118955	10273.983647	27.503488
246.673263	10289.427194	27.508506
246.837974	10307.914830	27.513524
247.307131	10321.486430	27.518541
247.744460	10326.457793	27.523559
247.614661	10357.156038	27.528576
247.962081	10354.053585	27.533594
247.862432	10385.520548	27.538612
248.002800	10397.635564	27.543629
248.600221	10410.498226	27.548647
248.609960	10433.135992	27.553664
249.176755	10450.422748	27.558682
249.281912	10472.152940	27.563700
249.685087	10482.748103	27.568717
249.716366	10497.653668	27.573735
249.987477	10527.011145	27.578752
250.527766	10538.175320	27.583770
250.728140	10552.118561	27.588788
250.790779	10572.982995	27.593805
251.078865	10585.882819	27.598823
250.918818	10608.295249	27.603840
251.565557	10624.028716	27.608858
251.785268	10657.523266	27.613876
252.074834	10676.643787	27.618893
252.505846	10679.872004	27.623911
252.520708	10706.401293	27.628928
252.973746	10713.612407	27.633946
253.308931	10737.046035	27.638964
253.776813	10743.797750	27.643981
253.917265	10767.128145	27.648999
253.750297	10787.570753	27.654016
254.067666	10795.061202	27.659034
254.312050	10821.986010	27.664052
254.472566	10848.278700	27.669069
254.940358	10866.826322	27.674087
255.065555	10886.612466	27.679104
255.543358	10909.787956	27.684122
255.958611	10923.179112	27.689140
256.250263	10940.427637	27.694157
256.837589	10954.743653	27.699175
256.684859	10966.857977	27.704192
256.905706	10979.646340	27.709210
257.352554	10995.296654	27.714228
257.416027	11013.145563	27.719245
258.088248	11014.094803	27.724263
257.738386	11040.426590	27.729280
257.803634	11052.233870	27.734298
258.197771	11075.439204	27.739316
258.670297	11087.147580	27.744333
258.939329	11102.280648	27.749351
259.330369	11124.115668	27.754368
259.400905	11131.105074	27.759386
259.475685	11153.057088	27.764404
259.605363	11181.065112	27.769421
260.309580	11195.169752	27.774439
260.489306	11223.495746	27.779456
260.791127	11227.424611	27.784474
261.065658	11242.052658	27.789492
261.103017	11268.501933	27.794509
261.605498	11274.268022	27.799527
261.631867	11301.086321	27.804544
262.344920	11305.966656	27.809562
262.462011	11317.770275	27.814580
262.501888	11331.464998	27.819597
262.555884	11344.202479	27.824615
262.916376	11364.602629	27.829632
263.050853	11383.588930	27.834650
263.526354	11400.870547	27.839668
263.474798	11419.321980	27.844685
264.008373	11425.880321	27.849703
264.012583	11454.982690	27.854720
264.402036	11478.603809	27.859738
264.893964	11493.191372	27.864756
264.734617	11518.833722	27.869773
265.202094	11528.962744	27.874791
265.536674	11549.042804	27.879808
265.870076	11577.931750	27.884826
266.339115	11588.733413	27.889844
266.715034	11607.005573	27.894861
266.690203	11622.640023	27.899879
266.905404	11634.424482	27.904896
267.445166	11643.438554	27.909914
267.340350	11651.429477	27.914932
267.408644	11677.626898	27.919949
268.252737	11696.486653	27.924967
268.043673	11718.588843	27.929984
268.323738	11737.463215	27.935002
268.495558	11750.803958	27.940020
268.570267	11778.456526	27.945037
269.208148	11801.332608	27.950055
269.377597	11830.080530	27.955072
269.750164	11849.291129	27.960090
270.091560	11874.225556	27.965108
270.161362	11903.886744	27.970125
270.649228	11904.061314	27.975143
270.696138	11938.234781	27.980160
271.080337	11961.698316	27.985178
271.497536	11980.184681	27.990196
271.466831	12005.995606	27.995213
272.208179	12023.787003	28.000231
272.343218	12038.741421	28.005248
272.476745	12059.019279	28.010266
272.975031	12077.262261	28.015284
273.202422	12101.402776	28.020301
273.520440	12116.747728	28.025319
273.920947	12138.023126	28.030336
274.266171	12151.103846	28.035354
274.643164	12164.423575	28.040372
274.805756	12177.228831	28.045389
275.558985	12184.543778	28.050407
275.955663	12204.604918	28.055424
276.059095	12208.700809	28.060442
276.205924	12224.156143	28.065460
276.070931	12236.353572	28.070477
276.229102	12252.505159	28.075495
276.948568	12260.697178	28.080512
277.191052	12283.371494	28.085530
277.365814	12296.259927	28.090548
277.765809	12307.787366	28.095565
277.913273	12314.301246	28.100583
278.048643	12337.702506	28.105600
278.276152	12353.852172	28.110618
278.866852	12360.302162	28.115636
279.274995	12396.052549	28.120653
279.148813	12404.315276	28.125671
279.410979	12422.079268	28.130688
279.362716	12440.006549	28.135706
279.889230	12457.181573	28.140724
279.686393	12484.517255	28.145741
280.088111	12503.662345	28.150759
280.196127	12525.563438	28.155776
280.417087	12542.860042	28.160794
281.221050	12556.846936	28.165812
281.158129	12589.798154	28.170829
281.696422	12601.268241	28.175847
282.301696	12633.075163	28.180864
282.443004	12646.527277	28.185882
282.659496	12647.287309	28.190900
282.702070	12685.803077	28.195917
282.850682	12699.525081	28.200935
282.717799	12721.928049	28.205952
283.103350	12743.547112	28.210970
283.743947	12760.320630	28.215988
283.681969	12794.236558	28.221005
283.797028	12801.958416	28.226023
284.507941	12832.419752	28.231040
284.790131	12867.757073	28.236058
285.488074	12889.776911	28.241076
285.788756	12908.753245	28.246093
286.011687	12934.890850	28.251111
286.513476	12948.527815	28.256128
286.503932	12969.736645	28.261146
286.776844	12977.304809	28.266164
286.891726	13004.457971	28.271181
287.580513	13025.515041	28.276199
288.139952	13036.433514	28.281216
287.749770	13066.603185	28.286234
288.484490	13072.675039	28.291252
288.776186	13097.931608	28.296269
289.454545	13104.624266	28.301287
289.747585	13123.055264	28.306304
289.917486	13133.111625	28.311322
290.289053	13146.087929	28.316340
290.503607	13165.288418	28.321357
290.547653	13177.467947	28.326375
291.089766	13202.678502	28.331392
291.129843	13216.401570	28.336410
291.332590	13230.821086	28.341428
291.615009	13255.611377	28.346445
291.694732	13264.031147	28.351463
292.151591	13291.164430	28.356480
292.386374	13314.845343	28.361498
292.657627	13333.724606	28.366516
292.837845	13361.683895	28.371533
293.061804	13375.899881	28.376551
293.711919	13393.799295	28.381568
293.420323	13432.329584	28.386586
293.834189	13449.246933	28.391604
294.268581	13481.211452	28.396621
294.805707	13501.542503	28.401639
294.919338	13521.819173	28.406656
295.055181	13544.845429	28.411674
295.590795	13562.521279	28.416692
295.582679	13593.542752	28.421709
296.137620	13619.300271	28.426727
296.728565	13633.462044	28.431744
296.925827	13666.739574	28.436762
297.405568	13679.186201	28.441780
297.587954	13695.885234	28.446797
297.775543	13715.240553	28.451815
297.924778	13735.544690	28.456832
298.530803	13760.398810	28.461850
298.806811	13769.215024	28.466868
298.879726	13788.754891	28.471885
299.140401	13810.424408	28.476903
299.670493	13825.310351	28.481920
299.481944	13848.687016	28.486938
300.015083	13872.371364	28.491956
300.494767	13886.673126	28.496973
300.507019	13905.515542	28.501991
301.276787	13924.358681	28.507008
301.111331	13942.921655	28.512026
301.832016	13954.862112	28.517044
301.932663	13978.851449	28.522061
302.051229	14002.677101	28.527079
302.363113	14018.302244	28.532096
302.613684	14041.716825	28.537114
302.894258	14054.644297	28.542132
302.938331	14083.396457	28.547149
303.102514	14116.508590	28.552167
303.552708	14127.283549	28.557184
303.853534	14157.909804	28.562202
304.276465	14181.094324	28.567220
304.383047	14217.650390	28.572237
304.501736	14241.452728	28.577255
305.389295	14276.344593	28.582272
305.306604	14301.715423	28.587290
306.077689	14324.666003	28.592308
306.187443	14352.107517	28.597325
306.478779	14381.312580	28.602343
307.031017	14394.617741	28.607360
307.197267	14428.436238	28.612378
307.481537	14448.870212	28.617396
308.146072	14465.606857	28.622413
308.117340	14486.348007	28.627431
308.462559	14513.760275	28.632448
308.630394	14537.994634	28.637466
308.927598	14565.022492	28.642484
309.312739	14585.124725	28.647501
309.676503	14620.690321	28.652519
310.211341	14630.512257	28.657536
310.246178	14670.548595	28.662554
310.520139	14692.557516	28.667572
311.002910	14715.324680	28.672589
311.482487	14743.091780	28.677607
312.057211	14767.862777	28.682624
311.879135	14791.959327	28.687642
312.436942	14811.065533	28.692660
312.645693	14834.793933	28.697677
313.036442	14860.783904	28.702695
313.471320	14859.834074	28.707712
313.724630	14883.758487	28.712730
314.149273	14898.639222	28.717748
314.550944	14926.131099	28.722765
314.575905	14946.799322	28.727783
314.959875	14962.148649	28.732800
315.349465	14989.105174	28.737818
315.550018	15016.636794	28.742836
315.659453	15034.192490	28.747853
315.875892	15069.912687	28.752871
316.471974	15089.334413	28.757888
316.723201	15118.657756	28.762906
317.422612	15136.108032	28.767924
317.493749	15155.960319	28.772941
317.682259	15187.850657	28.777959
317.743932	15196.491915	28.782976
318.220120	15220.961526	28.787994
318.513536	15255.353306	28.793012
318.776271	15274.910808	28.798029
318.943161	15295.005903	28.803047
319.197042	15323.667189	28.808064
319.870644	15365.066890	28.813082
320.368009	15385.567635	28.818100
320.847923	15405.362023	28.823117
320.951554	15424.372315	28.828135
321.283057	15445.299355	28.833152
321.356754	15458.084069	28.838170
321.932115	15478.430166	28.843188
322.189268	15491.761419	28.848205
322.436262	15516.173258	28.853223
323.053176	15529.780722	28.858240
323.268764	15548.280862	28.863258
323.582429	15570.851811	28.868276
324.064845	15581.759525	28.873293
323.864302	15614.805796	28.878311
323.958056	15629.461400	28.883328
324.199104	15659.053765	28.888346
324.665923	15688.006712	28.893364
325.133496	15717.736647	28.898381
325.244848	15748.048889	28.903399
325.630621	15776.515754	28.908416
325.783294	15799.318566	28.913434
325.974467	15837.249707	28.918452
326.621261	15860.382211	28.923469
326.708587	15895.479324	28.928487
327.628381	15929.147814	28.933504
327.840681	15947.210759	28.938522
327.975975	15978.301262	28.943540
328.072174	15999.157617	28.948557
328.469869	16033.525881	28.953575
329.075730	16061.679396	28.958592
329.245141	16089.150184	28.963610
329.720799	16117.032167	28.968628
330.484414	16137.582781	28.973645
330.421960	16173.959953	28.978663
331.246720	16197.854745	28.983680
331.444057	16217.354837	28.988698
331.695167	16250.088036	28.993716
332.355180	16261.690303	28.998733
332.029914	16289.334719	29.003751
332.285074	16315.292684	29.008768
332.753756	16346.569867	29.013786
333.007164	16382.211126	29.018804
333.525460	16406.834733	29.023821
333.788886	16433.368425	29.028839
333.982686	16457.273447	29.033856
334.314030	16494.295463	29.038874
334.754538	16528.662400	29.043892
334.994134	16548.184260	29.048909
335.350835	16587.037063	29.053927
335.826167	16609.051471	29.058944
336.155611	16639.374963	29.063962
336.677814	16665.919792	29.068980
337.106354	16682.653627	29.073997
337.179990	16731.317104	29.079015
337.262590	16743.560673	29.084032
337.683979	16777.360676	29.089050
338.501137	16798.935725	29.094068
339.110869	16821.921237	29.099085
338.966141	16850.870252	29.104103
339.525659	16871.679397	29.109120
339.888170	16894.396973	29.114138
340.290767	16923.939644	29.119156
340.841429	16940.127043	29.124173
341.152023	16960.536133	29.129191
341.251992	16978.888346	29.134208
341.603876	17000.145011	29.139226
342.006581	17030.170205	29.144244
342.568967	17055.115356	29.149261
342.599498	17075.020804	29.154279
343.138100	17081.541206	29.159296
343.088650	17114.182412	29.164314
343.159527	17139.242140	29.169332
343.794068	17156.446784	29.174349
344.323861	17178.556976	29.179367
344.692094	17189.109491	29.184384
345.145595	17219.965230	29.189402
345.113992	17227.322513	29.194420
345.803427	17248.254078	29.199437
345.594110	17277.149895	29.204455
346.364681	17293.823013	29.209472
346.699641	17316.941390	29.214490
346.636962	17341.995153	29.219508
347.215863	17366.857646	29.224525
347.293038	17397.870580	29.229543
347.682893	17417.039140	29.234560
347.912636	17451.838540	29.239578
348.338841	17489.247472	29.244596
348.769187	17503.133362	29.249613
348.779113	17542.441463	29.254631
348.952983	17576.927218	29.259648
349.512378	17615.066317	29.264666
349.776319	17638.305664	29.269684
350.355180	17667.719601	29.274701
350.553084	17701.891092	29.279719
351.015670	17741.209869	29.284736
351.455585	17764.566872	29.289754
351.854907	17791.449120	29.294772
352.386995	17819.706118	29.299789
352.862962	17849.140559	29.304807
353.064931	17872.526060	29.309824
353.870154	17899.204158	29.314842
353.886142	17934.760359	29.319860
354.383567	17959.482739	29.324877
355.030084	17981.610942	29.329895
354.833593	18011.981424	29.334912
355.334120	18037.598806	29.339930
355.381665	18065.433540	29.344948
356.141580	18090.018087	29.349965
356.242587	18118.312257	29.354983
356.509412	18145.187054	29.360000
357.115768	18178.341341	29.365018
357.375838	18208.743816	29.370036
357.571352	18232.014235	29.375053
358.239532	18259.675638	29.380071
358.434364	18290.689679	29.385088
358.718687	18309.427451	29.390106
358.537833	18350.919290	29.395124
359.698451	18379.539843	29.400141
360.099258	18416.665000	29.405159
360.386835	18445.969302	29.410176
360.475586	18482.775785	29.415194
360.778093	18505.912221	29.420212
361.461488	18537.375552	29.425229
361.736500	18560.964329	29.430247
361.989946	18584.162593	29.435264
362.819328	18615.357558	29.440282
362.919519	18649.687468	29.445300
363.366494	18680.288457	29.450317
363.724483	18714.095011	29.455335
363.855763	18727.837516	29.460352
364.542129	18765.203106	29.465370
364.589391	18788.520908	29.470388
365.008449	18815.422037	29.475405
365.146241	18845.497506	29.480423
365.683379	18876.394500	29.485440
366.316086	18899.708578	29.490458
366.283965	18931.007301	29.495476
366.443048	18961.412095	29.500493
367.026884	18995.520787	29.505511
367.107465	19031.453297	29.510528
367.533373	19056.293191	29.515546
368.039669	19093.038220	29.520564
368.386268	19117.601254	29.525581
368.961204	19142.042979	29.530599
369.638663	19180.158240	29.535616
369.967986	19186.014140	29.540634
370.195888	19218.064931	29.545652
370.583160	19233.085033	29.550669
371.302738	19263.943092	29.555687
371.726934	19289.477288	29.560704
372.609866	19293.285134	29.565722
372.632935	19324.509244	29.570740
373.082604	19334.936138	29.575757
373.109620	19353.949417	29.580775
373.697124	19365.285250	29.585792
374.143053	19380.582707	29.590810
374.155866	19401.308932	29.595828
374.297328	19428.551803	29.600845
374.751997	19450.259668	29.605863
374.797026	19483.676564	29.610880
375.448154	19519.868844	29.615898
375.659783	19543.999219	29.620916
376.043607	19564.104568	29.625933
376.205450	19608.235556	29.630951
376.335521	19641.879906	29.635968
377.161681	19671.358931	29.640986
377.008620	19706.179086	29.646004
377.221999	19736.767066	29.651021
377.955014	19778.462769	29.656039
378.338298	19822.559249	29.661056
378.723661	19845.614458	29.666074
378.836014	19890.610461	29.671092
379.471871	19911.786009	29.676109
380.243415	19962.216386	29.681127
380.560828	19986.790255	29.686144
381.253127	20018.950183	29.691162
381.414830	20055.793769	29.696180
381.887985	20074.604749	29.701197
382.381425	20108.372782	29.706215
383.019608	20134.833006	29.711232
383.366632	20159.760117	29.716250
383.624670	20191.073080	29.721268
383.901470	20217.121834	29.726285
384.209396	20251.128970	29.731303
384.670901	20288.243503	29.736320
385.138125	20308.386395	29.741338
385.484916	20337.509203	29.746356
385.733337	20371.734545	29.751373
386.218799	20400.195978	29.756391
386.544426	20433.270340	29.761408
387.192066	20444.467672	29.766426
387.293592	20480.158590	29.771444
387.893358	20508.139334	29.776461
388.229002	20528.758339	29.781479
388.274611	20570.090472	29.786496
388.936663	20590.455301	29.791514
389.432114	20627.441987	29.796532
390.166398	20657.713668	29.801549
390.245801	20678.200254	29.806567
390.661438	20702.399437	29.811584
391.240259	20726.667825	29.816602
391.476305	20748.823485	29.821620
391.782092	20783.536820	29.826637
392.139087	20811.121509	29.831655
392.247508	20840.683535	29.836672
392.705919	20864.308269	29.841690
393.068217	20906.386614	29.846708
393.350463	20935.874316	29.851725
393.936965	20965.614441	29.856743
393.800337	20999.959966	29.861760
394.486041	21030.855267	29.866778
394.700850	21057.716539	29.871796
394.636264	21085.957976	29.876813
395.162144	21119.524008	29.881831
395.587732	21162.857031	29.886848
395.989425	21191.270597	29.891866
396.291713	21229.383229	29.896884
396.883724	21274.119071	29.901901
397.260730	21305.911082	29.906919
397.835031	21339.939401	29.911936
398.172586	21376.387819	29.916954
398.488474	21419.463728	29.921972
398.557961	21449.389602	29.926989
399.345022	21485.718141	29.932007
399.731603	21525.859360	29.937024
400.299024	21557.543073	29.942042
400.636140	21595.464711	29.947060
400.976163	21632.017337	29.952077
401.905949	21657.105656	29.957095
401.648949	21688.806216	29.962112
402.536114	21727.668318	29.967130
402.775845	21768.553416	29.972148
403.058815	21806.236936	29.977165
403.985608	21839.551995	29.982183
404.186243	21875.606305	29.987200
404.908381	21902.974674	29.992218
405.277235	21938.999704	29.997236
405.327070	21967.389236	30.002253
405.935874	21998.716883	30.007271
405.931763	22040.298931	30.012288
406.744399	22064.295611	30.017306
407.165601	22103.298761	30.022324
407.492236	22138.427701	30.027341
407.979319	22166.931269	30.032359
408.058551	22200.153936	30.037376
408.808994	22233.555722	30.042394
409.144438	22266.848072	30.047412
409.355693	22302.321268	30.052429
410.017702	22343.175713	30.057447
410.074845	22377.752135	30.062464
410.600795	22409.852703	30.067482
410.936979	22447.623451	30.072500
411.548619	22488.906017	30.077517
411.889958	22521.584507	30.082535
412.116375	22565.569045	30.087552
413.093426	22592.481638	30.092570
413.377578	22622.172221	30.097588
413.571199	22662.802196	30.102605
414.175016	22680.161115	30.107623
414.290954	22723.766980	30.112640
415.034403	22746.558754	30.117658
415.422490	22791.188860	30.122676
415.866592	22818.379232	30.127693
416.482016	22842.933172	30.132711
416.206673	22885.298564	30.137728
416.954562	22910.962869	30.142746
417.132391	22950.758829	30.147764
417.270178	22987.309999	30.152781
418.544251	23029.386226	30.157799
418.748362	23071.390477	30.162816
419.154042	23101.681499	30.167834
419.845316	23121.746521	30.172852
419.918608	23172.770376	30.177869
420.324843	23192.478968	30.182887
420.499490	23229.432972	30.187904
421.118151	23263.489354	30.192922
421.526550	23291.269843	30.197940
421.880185	23324.367297	30.202957
422.364255	23352.868624	30.207975
422.670642	23389.802751	30.212992
422.862158	23420.538203	30.218010
423.283059	23462.140119	30.223028
423.440067	23499.618009	30.228045
423.949036	23527.314434	30.233063
424.233141	23573.086564	30.238080
425.011956	23611.395340	30.243098
425.018446	23649.543432	30.248116
425.190218	23699.011898	30.253133
425.906553	23738.991816	30.258151
426.390881	23789.812299	30.263168
426.896609	23835.217298	30.268186
427.417345	23870.029110	30.273204
427.753963	23910.075421	30.278221
428.809373	23951.519913	30.283239
428.751686	23991.505508	30.288256
429.163244	24029.710419	30.293274
429.513953	24072.700555	30.298292
430.076564	24111.356897	30.303309
430.562515	24148.710811	30.308327
430.660649	24195.344874	30.313344
431.342059	24237.621520	30.318362
431.362002	24274.724813	30.323380
431.981212	24331.826243	30.328397
432.827083	24374.542803	30.333415
433.308877	24426.519963	30.338432
433.836620	24459.057775	30.343450
434.548953	24495.094454	30.348468
434.611985	24536.906447	30.353485
435.208425	24577.709293	30.358503
435.675230	24609.579358	30.363520
436.034278	24649.866549	30.368538
436.334922	24685.158011	30.373556
436.740787	24725.147458	30.378573
437.480888	24762.438576	30.383591
437.705217	24813.002333	30.388608
437.953816	24852.043490	30.393626
438.543980	24884.316300	30.398644
439.261130	24936.098352	30.403661
439.758614	24958.101112	30.408679
440.264017	25011.094913	30.413696
440.563280	25043.217452	30.418714
441.212081	25068.645924	30.423732
441.635726	25116.714218	30.428749
442.032280	25147.660131	30.433767
442.221244	25194.764462	30.438784
442.749175	25220.509650	30.443802
443.019467	25250.987749	30.448820
443.482306	25309.998194	30.453837
444.170112	25338.833426	30.458855
444.260810	25378.050154	30.463872
444.715140	25422.310280	30.468890
445.135592	25463.245290	30.473908
445.659273	25509.191122	30.478925
446.114317	25546.941165	30.483943
446.548617	25594.548517	30.488960
446.764688	25640.706469	30.493978
447.470604	25678.241803	30.498996
448.060659	25716.648039	30.504013
448.448088	25751.854782	30.509031
448.684874	25795.237132	30.514048
449.042739	25838.640561	30.519066
449.669725	25872.082523	30.524084
450.092492	25918.800020	30.529101
450.930536	25956.102760	30.534119
450.936421	26002.845309	30.539136
451.095754	26036.049547	30.544154
452.052911	26067.891644	30.549172
452.427989	26107.283773	30.554189
452.801421	26142.298062	30.559207
453.336063	26184.300977	30.564224
453.748391	26228.311469	30.569242
453.920893	26261.384633	30.574260
454.352022	26311.432798	30.579277
454.837047	26347.908430	30.584295
455.100316	26382.827880	30.589312
455.540894	26435.505583	30.594330
456.192429	26465.673547	30.599348
456.971114	26513.847862	30.604365
457.477822	26549.929189	30.609383
457.537432	26597.106069	30.614400
457.661425	26646.625618	30.619418
458.304885	26697.352662	30.624436
458.528626	26748.537304	30.629453
459.115971	26784.558461	30.634471
459.690404	26838.388693	30.639488
460.089330	26891.383813	30.644506
461.002481	26930.846504	30.649524
461.049003	26989.224979	30.654541
461.434030	27024.923659	30.659559
461.902878	27084.346103	30.664576
462.177592	27130.072470	30.669594
463.090871	27179.109627	30.674612
463.515730	27225.912327	30.679629
463.859193	27276.485666	30.684647
464.403379	27322.786238	30.689664
464.803673	27380.120116	30.694682
465.447108	27414.947193	30.699700
465.756777	27479.488783	30.704717
465.946062	27532.230332	30.709735
466.867325	27583.109584	30.714752
467.413968	27624.104541	30.719770
468.258853	27665.088098	30.724788
468.327151	27715.253986	30.729805
468.982184	27757.944276	30.734823
469.401598	27809.503459	30.739840
469.972526	27855.116471	30.744858
470.476305	27892.661675	30.749876
471.024961	27950.127462	30.754893
471.207942	27996.767210	30.759911
471.696419	28044.075796	30.764928
472.195778	28091.524671	30.769946
472.884990	28129.607544	30.774964
473.122670	28183.683799	30.779981
473.499654	28231.295266	30.784999
474.126616	28282.663771	30.790016
474.430196	28334.880929	30.795034
475.493116	28370.691032	30.800052
475.543625	28422.401405	30.805069
475.828825	28462.350061	30.810087
476.299779	28511.136081	30.815104
476.651658	28570.103434	30.820122
477.228421	28626.257572	30.825140
477.680853	28665.708960	30.830157
477.927737	28724.075869	30.835175
478.616294	28775.817365	30.840192
479.150353	28832.266319	30.845210
480.104843	28872.083079	30.850228
480.428222	28918.298241	30.855245
480.900562	28964.845373	30.860263
481.272725	29008.282755	30.865280
481.835799	29057.869009	30.870298
482.020551	29108.559110	30.875316
482.576558	29159.746337	30.880333
482.977990	29195.128112	30.885351
483.438577	29232.001895	30.890368
483.806561	29287.053791	30.895386
484.469740	29332.368308	30.900404
484.625165	29377.303189	30.905421
485.345071	29428.908926	30.910439
485.681215	29473.224180	30.915456
486.057235	29526.821078	30.920474
486.550745	29571.372400	30.925492
487.055781	29631.075172	30.930509
487.588024	29673.534920	30.935527
488.177486	29725.377652	30.940544
488.471904	29786.724841	30.945562
489.117089	29835.671869	30.950580
489.439913	29893.948080	30.955597
489.937366	29942.613817	30.960615
490.601667	29995.378847	30.965632
491.037064	30047.273263	30.970650
491.464278	30094.941435	30.975668
491.998019	30150.022247	30.980685
492.228027	30202.503241	30.985703
492.768811	30256.829163	30.990720
493.420184	30334.635984	30.995738
494.206989	30377.023761	31.000756
494.597900	30428.393454	31.005773
495.552051	30480.534597	31.010791
496.108283	30524.260786	31.015808
495.932021	30586.417478	31.020826
496.892635	30631.496829	31.025844
497.559834	30681.354405	31.030861
498.224428	30738.362131	31.035879
498.831669	30779.155686	31.040896
498.729189	30831.993312	31.045914
499.048888	30879.529951	31.050932
499.522475	30933.547252	31.055949
499.893647	31000.458033	31.060967
500.481126	31050.421346	31.065984
500.908716	31110.829791	31.071002
501.352324	31162.798706	31.076020
501.664879	31236.194612	31.081037
502.170766	31295.962840	31.086055
502.901345	31351.185221	31.091072
503.186609	31417.016918	31.096090
504.048816	31463.061263	31.101108
504.397870	31530.406829	31.106125
505.004744	31587.300636	31.111143
505.972010	31641.411957	31.116160
506.274567	31696.557940	31.121178
506.699391	31748.231928	31.126196
507.388701	31818.052866	31.131213
507.737756	31867.502599	31.136231
508.617203	31916.722717	31.141248
508.917401	31968.257046	31.146266
509.955553	32022.919462	31.151284
510.481990	32073.337520	31.156301
510.796063	32122.080634	31.161319
511.372438	32165.908529	31.166336
511.546969	32220.793340	31.171354
511.913288	32268.562653	31.176372
512.310719	32333.946903	31.181389
512.891713	32390.610915	31.186407
513.569196	32442.579599	31.191424
513.818392	32508.569623	31.196442
514.119186	32552.343096	31.201460
514.830257	32618.821936	31.206477
515.416255	32682.626923	31.211495
516.126287	32721.590384	31.216512
516.240822	32767.458907	31.221530
516.752467	32821.134873	31.226548
517.534489	32874.785196	31.231565
517.878264	32923.796970	31.236583
518.386687	32978.206028	31.241600
518.864618	33030.051671	31.246618
519.331774	33082.877475	31.251636
520.168678	33139.892822	31.256653
520.336418	33197.890017	31.261671
521.020898	33243.943154	31.266688
521.194909	33300.914077	31.271706
521.775304	33353.100290	31.276724
522.645751	33417.993714	31.281741
523.031083	33474.251763	31.286759
523.545062	33515.792850	31.291776
524.127572	33578.058511	31.296794
524.771102	33634.056602	31.301812
525.107780	33695.605988	31.306829
525.371735	33761.651854	31.311847
526.216881	33806.868850	31.316864
526.393978	33876.123077	31.321882
527.011210	33935.525165	31.326900
527.846421	33985.095996	31.331917
528.029944	34054.210997	31.336935
528.778835	34106.018088	31.341952
529.005371	34176.483417	31.346970
529.855482	34239.631744	31.351988
530.619284	34313.631545	31.357005
531.090596	34366.930671	31.362023
531.380001	34418.578010	31.367040
531.751159	34484.034445	31.372058
532.513185	34547.627624	31.377076
533.512946	34599.773336	31.382093
533.458012	34667.857171	31.387111
534.174816	34731.382744	31.392128
534.817418	34785.494232	31.397146
535.135143	34846.533144	31.402164
536.068280	34906.902378	31.407181
536.164350	34988.930426	31.412199
536.849371	35047.703271	31.417216
537.544584	35108.945713	31.422234
538.046773	35166.026061	31.427252
538.875059	35230.974063	31.432269
538.693799	35302.088818	31.437287
539.561673	35349.117471	31.442304
539.986176	35407.499073	31.447322
540.620973	35478.908716	31.452340
541.189068	35545.046528	31.457357
541.960515	35608.348395	31.462375
542.467145	35667.676680	31.467392
543.184275	35725.335506	31.472410
543.376277	35788.992676	31.477428
544.340812	35846.162795	31.482445
544.842777	35907.452553	31.487463
545.162781	35966.831637	31.492480
545.400271	36027.777364	31.497498
545.828968	36093.261691	31.502516
546.564493	36155.056494	31.507533
547.082524	36227.678274	31.512551
547.801542	36291.464632	31.517568
548.485451	36362.235262	31.522586
549.108376	36409.468177	31.527604
549.658301	36471.200085	31.532621
550.116091	36544.596897	31.537639
550.603179	36597.593866	31.542656
551.175330	36657.002933	31.547674
551.464614	36722.487355	31.552692
552.821009	36776.439378	31.557709
553.205664	36835.122559	31.562727
553.751603	36881.485700	31.567744
554.434632	36928.362839	31.572762
554.676783	36977.951672	31.577780
555.557565	37018.991978	31.582797
555.609482	37081.266021	31.587815
556.614412	37140.355723	31.592832
556.745731	37185.797170	31.597850
557.140854	37239.029015	31.602868
558.227823	37291.859324	31.607885
558.758057	37346.852445	31.612903
558.592909	37405.044517	31.617920
558.990688	37479.528192	31.622938
559.656619	37541.790598	31.627956
560.738019	37597.646504	31.632973
560.822365	37663.408109	31.637991
561.401095	37731.619574	31.643008
561.738079	37799.391520	31.648026
562.577983	37869.640355	31.653044
563.496233	37922.749772	31.658061
563.877995	37989.375549	31.663079
564.473371	38057.332966	31.668096
565.053105	38116.846560	31.673114
565.427508	38181.034318	31.678132
565.987869	38245.437741	31.683149
566.174824	38323.829584	31.688167
566.664240	38399.286679	31.693184
567.648070	38458.946017	31.698202
568.225747	38524.954224	31.703220
568.823836	38595.223768	31.708237
569.097568	38670.092673	31.713255
569.878814	38731.557242	31.718272
570.646869	38805.975601	31.723290
571.107548	38880.211530	31.728308
571.908524	38948.103523	31.733325
572.224515	39024.690387	31.738343
573.376309	39083.102367	31.743360
573.934118	39152.695732	31.748378
574.273602	39225.201182	31.753396
574.642478	39287.244064	31.758413
575.186934	39355.164223	31.763431
575.647687	39421.952609	31.768448
576.103866	39494.234631	31.773466
576.508947	39578.681849	31.778484
577.623299	39634.693221	31.783501
578.388337	39713.901343	31.788519
578.957126	39784.161354	31.793536
579.665032	39841.657981	31.798554
580.224454	39910.442667	31.803572
580.879995	39973.071789	31.808589
581.485092	40034.560403	31.813607
581.603648	40104.975049	31.818624
582.308279	40170.971335	31.823642
582.948339	40248.914463	31.828660
583.948760	40303.586139	31.833677
584.588354	40374.086078	31.838695
584.829740	40446.186399	31.843712
585.361055	40507.840329	31.848730
586.083583	40569.140828	31.853748
586.961639	40635.372107	31.858765
587.182518	40700.481161	31.863783
587.797074	40764.309904	31.868800
588.588054	40820.605691	31.873818
589.023241	40896.602910	31.878836
589.774334	40959.756255	31.883853
590.295197	41021.596733	31.888871
590.708005	41085.441023	31.893888
591.514645	41140.106202	31.898906
592.169884	41204.387496	31.903924
592.654285	41255.740990	31.908941
592.890004	41317.733814	31.913959
593.128453	41381.030239	31.918976
594.241189	41441.587163	31.923994
594.433230	41504.497061	31.929012
594.764120	41563.384227	31.934029
595.155604	41642.119420	31.939047
595.712726	41723.435282	31.944064
596.326091	41784.322197	31.949082
596.995788	41865.919981	31.954100
597.466965	41942.133373	31.959117
598.039822	42023.776286	31.964135
598.539794	42096.676887	31.969152
599.418211	42174.787595	31.974170
599.690623	42261.987323	31.979188
600.475433	42338.601926	31.984205
601.047097	42421.430723	31.989223
601.699884	42496.208234	31.994240
602.480865	42574.800851	31.999258
602.962387	42659.363143	32.004276
603.586471	42734.768334	32.009293
604.352444	42819.480042	32.014311
605.413805	42890.649102	32.019328
606.028543	42955.435692	32.024346
606.444743	43031.643696	32.029364
606.931049	43103.537008	32.034381
607.681649	43185.010370	32.039399
608.229013	43261.503871	32.044416
608.832340	43338.477814	32.049434
609.196392	43421.080180	32.054452
609.878686	43488.639074	32.059469
610.803808	43568.872807	32.064487
611.234942	43648.711843	32.069504
612.218249	43724.311035	32.074522
612.446942	43806.119724	32.079540
613.315979	43876.964417	32.084557
614.340231	43956.618233	32.089575
614.691126	44026.860891	32.094592
615.532630	44102.485070	32.099610
615.892419	44181.814040	32.104628
616.753133	44244.821470	32.109645
617.413584	44325.528494	32.114663
617.950036	44386.932355	32.119680
618.938375	44465.530191	32.124698
619.228063	44527.575267	32.129716
619.902833	44594.122663	32.134733
620.774179	44671.452434	32.139751
621.067174	44742.730398	32.144768
621.620992	44813.040309	32.149786
622.001631	44891.680469	32.154804
622.671358	44963.487415	32.159821
623.287768	45049.045453	32.164839
623.917849	45126.372801	32.169856
624.673299	45193.104740	32.174874
625.537164	45264.852299	32.179892
625.753349	45334.607425	32.184909
626.339874	45414.747178	32.189927
627.127332	45491.718430	32.194944
627.737970	45572.290626	32.199962
628.370791	45647.415569	32.204980
628.997059	45724.793365	32.209997
629.685894	45786.735499	32.215015
629.940217	45875.837030	32.220032
631.107335	45938.875227	32.225050
631.352978	46029.611488	32.230068
631.979090	46107.404546	32.235085
632.774947	46184.974056	32.240103
633.266683	46255.012244	32.245120
633.777278	46312.640412	32.250138
634.314178	46396.174578	32.255156
634.928267	46473.642711	32.260173
635.760238	46537.799393	32.265191
636.068083	46617.027186	32.270208
637.132251	46688.753325	32.275226
637.538570	46765.508598	32.280244
638.102010	46836.853921	32.285261
638.631853	46911.584065	32.290279
639.405691	46992.968997	32.295296
639.951247	47068.379275	32.300314
640.237070	47151.705662	32.305332
640.991014	47241.163585	32.310349
641.552795	47318.081689	32.315367
642.220214	47401.838689	32.320384
643.191289	47480.748769	32.325402
643.393326	47578.545207	32.330420
644.073630	47671.914368	32.335437
644.957725	47754.140148	32.340455
645.584078	47842.535620	32.345472
646.493826	47921.429246	32.350490
647.105466	48002.523194	32.355508
647.717456	48082.771048	32.360525
648.644288	48168.923420	32.365543
649.464050	48251.531486	32.370560
649.870242	48328.372021	32.375578
650.698622	48421.293992	32.380596
650.874462	48510.796651	32.385613
651.459336	48590.387895	32.390631
652.444612	48671.233372	32.395648
652.944028	48755.658900	32.400666
653.658613	48840.519784	32.405684
654.254113	48931.710971	32.410701
654.964860	49015.995301	32.415719
655.669804	49103.316089	32.420736
656.555920	49194.422547	32.425754
657.276962	49279.287459	32.430772
657.611778	49366.850698	32.435789
658.501363	49439.437221	32.440807
658.748026	49539.428171	32.445824
659.526949	49625.586284	32.450842
659.986375	49716.870028	32.455860
660.869288	49808.068356	32.460877
661.898231	49892.616570	32.465895
662.236518	49986.780010	32.470912
662.845796	50068.991686	32.475930
663.691125	50160.188420	32.480948
664.479294	50243.258775	32.485965
664.876356	50329.356861	32.490983
665.258143	50429.317428	32.496000
666.436517	50513.151924	32.501018
666.910177	50602.106499	32.506036
667.518349	50693.705055	32.511053
668.614398	50775.709708	32.516071
669.222245	50871.971217	32.521088
669.918845	50954.112194	32.526106
670.475989	51036.624037	32.531124
670.769241	51121.435147	32.536141
671.444949	51215.236035	32.541159
672.294185	51312.110475	32.546176
673.294404	51395.965629	32.551194
673.787269	51479.222797	32.556212
674.188386	51565.938484	32.561229
674.974348	51653.715398	32.566247
675.758605	51744.563276	32.571264
676.670295	51834.872464	32.576282
677.345006	51918.701591	32.581300
677.753842	51996.137482	32.586317
678.928269	52076.011967	32.591335
679.439137	52145.945255	32.596352
680.037930	52224.784724	32.601370
680.604417	52300.079340	32.606388
680.737376	52395.239223	32.611405
681.809782	52462.793757	32.616423
682.465414	52554.279501	32.621440
683.274554	52640.616581	32.626458
683.804444	52731.365824	32.631476
684.327702	52816.803306	32.636493
685.163603	52904.861888	32.641511
685.607899	52987.823949	32.646528
686.320019	53076.175445	32.651546
686.834177	53164.370549	32.656564
687.468328	53263.627887	32.661581
688.080339	53360.103158	32.666599
688.499045	53455.442046	32.671616
689.215740	53558.490664	32.676634
690.128582	53655.340930	32.681652
690.530242	53758.430074	32.686669
691.418282	53854.135525	32.691687
691.990728	53961.923453	32.696704
693.178714	54061.756613	32.701722
693.902077	54171.542551	32.706740
694.453491	54254.391145	32.711757
695.367360	54342.209495	32.716775
696.098738	54447.231644	32.721792
697.023614	54536.154746	32.726810
697.822616	54634.608248	32.731828
698.353772	54731.684903	32.736845
699.271759	54822.423820	32.741863
699.550803	54919.732655	32.746880
700.605776	55010.058028	32.751898
701.362102	55097.008566	32.756916
701.858284	55200.354979	32.761933
702.577662	55290.794013	32.766951
703.264796	55388.953844	32.771968
704.365545	55475.109787	32.776986
704.933162	55571.723265	32.782004
705.407124	55666.817255	32.787021
706.617378	55762.200623	32.792039
707.232475	55842.915912	32.797056
707.736699	55939.232042	32.802074
708.410245	56031.122719	32.807092
708.761822	56129.657657	32.812109
709.642898	56227.113427	32.817127
710.520177	56318.162909	32.822144
711.376915	56422.094242	32.827162
712.052120	56516.779866	32.832180
712.856174	56615.065424	32.837197
713.647843	56708.911222	32.842215
714.075642	56810.918714	32.847232
714.664429	56905.772135	32.852250
715.497924	56997.091042	32.857268
716.179933	57099.424465	32.862285
717.191645	57185.514073	32.867303
717.659463	57281.653127	32.872320
717.965517	57379.399215	32.877338
718.617923	57484.020755	32.882356
719.307401	57587.227498	32.887373
720.252859	57683.763420	32.892391
721.210411	57784.234787	32.897408
721.603478	57885.912249	32.902426
722.396596	57977.153829	32.907444
722.958370	58085.130163	32.912461
724.013915	58187.160888	32.917479
724.856811	58289.448490	32.922496
725.624059	58377.808134	32.927514
726.507647	58453.035748	32.932532
726.832997	58541.589279	32.937549
727.475921	58631.980244	32.942567
728.241729	58721.099991	32.947584
728.668546	58811.375835	32.952602
729.729481	58907.222320	32.957620
730.234063	59010.959887	32.962637
731.353947	59100.117537	32.967655
732.414719	59191.914407	32.972672
732.814313	59282.790924	32.977690
733.747603	59367.790554	32.982708
734.385095	59465.656255	32.987725
735.095172	59556.337284	32.992743
735.727423	59659.431384	32.997760
736.402810	59748.406297	33.002778
737.085233	59848.819698	33.007796
737.684021	59950.113280	33.012813
738.485964	60045.723595	33.017831
739.108942	60148.480427	33.022848
739.683819	60260.719658	33.027866
740.490640	60346.072956	33.032884
740.986898	60465.202687	33.037901
741.639362	60567.331054	33.042919
742.594072	60670.073570	33.047936
743.245058	60782.296765	33.052954
743.889572	60881.116170	33.057972
744.469943	61008.596995	33.062989
745.513826	61121.799934	33.068007
746.346131	61230.873312	33.073024
747.202023	61353.210100	33.078042
747.916853	61451.192645	33.083060
748.362799	61566.696497	33.088077
749.096909	61683.189915	33.093095
750.140961	61792.503048	33.098112
750.581927	61909.318026	33.103130
751.818385	62017.740924	33.108148
752.422026	62146.040352	33.113165
752.823179	62260.101744	33.118183
754.287696	62364.550907	33.123200
755.089898	62468.389575	33.128218
755.867596	62581.341207	33.133236
756.298802	62708.648683	33.138253
757.530200	62811.678545	33.143271
758.751448	62893.111818	33.148288
759.026541	63008.930157	33.153306
759.990600	63115.608735	33.158324
759.940506	63227.259628	33.163341
761.092592	63326.082701	33.168359
762.371243	63432.837306	33.173376
763.104954	63539.954408	33.178394
763.590632	63643.370938	33.183412
763.809239	63763.121989	33.188429
765.058627	63870.692814	33.193447
765.791125	63973.103009	33.198464
766.730984	64090.732802	33.203482
767.196859	64191.987124	33.208500
767.803314	64304.913284	33.213517
768.695366	64418.292213	33.218535
770.197468	64522.392079	33.223552
770.295989	64634.986828	33.228570
771.405752	64738.002154	33.233588
772.335162	64838.367475	33.238605
772.794356	64948.811826	33.243623
773.930040	65053.575510	33.248640
774.121096	65167.377904	33.253658
775.522804	65258.721974	33.258676
775.918077	65367.541795	33.263693
776.885712	65458.718312	33.268711
777.586321	65559.087016	33.273728
778.048915	65662.163375	33.278746
778.978947	65752.841651	33.283764
780.041209	65848.170312	33.288781
780.395040	65953.339669	33.293799
781.390197	66049.622311	33.298816
781.750252	66156.896863	33.303834
782.749393	66252.282058	33.308852
783.485522	66357.971836	33.313869
783.835826	66465.135779	33.318887
784.845964	66576.230949	33.323904
785.161702	66695.413761	33.328922
786.351667	66803.117016	33.333940
786.666583	66920.828176	33.338957
787.377370	67036.438759	33.343975
788.291543	67164.686159	33.348992
788.565067	67279.776104	33.354010
789.633812	67402.220798	33.359028
790.676850	67537.359467	33.364045
791.326555	67644.966710	33.369063
792.368701	67768.182937	33.374080
792.870712	67902.743246	33.379098
793.995766	68026.244420	33.384116
794.900717	68146.425439	33.389133
795.719304	68266.134583	33.394151
796.898606	68387.877533	33.399168
797.324597	68513.514088	33.404186
798.208352	68642.616390	33.409204
799.030398	68751.187086	33.414221
799.840757	68873.626116	33.419239
801.025382	68984.471140	33.424256
801.631175	69120.880906	33.429274
802.259521	69231.774962	33.434292
803.015684	69364.279163	33.439309
803.684484	69473.631315	33.444327
805.018904	69595.096276	33.449344
805.655692	69728.299041	33.454362
806.369717	69836.741377	33.459380
807.167591	69973.194370	33.464397
807.908528	70092.768540	33.469415
809.105299	70195.878327	33.474432
809.673880	70333.301042	33.479450
810.841666	70450.555549	33.484468
812.065844	70570.798604	33.489485
812.466322	70681.984468	33.494503
813.473104	70809.030758	33.499520
813.796732	70922.772563	33.504538
814.941106	71038.864328	33.509556
815.925155	71159.852293	33.514573
816.457745	71280.567813	33.519591
817.483051	71394.645025	33.524608
818.203124	71522.204557	33.529626
819.293895	71640.110641	33.534644
819.970585	71762.291066	33.539661
820.611929	71871.071863	33.544679
821.699099	71990.776376	33.549696
822.097293	72123.407380	33.554714
822.842819	72238.547117	33.559732
823.944552	72350.789167	33.564749
824.197787	72483.440023	33.569767
825.506655	72595.516282	33.574784
826.050978	72731.990722	33.579802
826.530233	72854.279516	33.584820
827.762178	72985.215876	33.589837
828.476458	73115.542997	33.594855
829.320175	73232.543673	33.599872
829.635327	73364.475038	33.604890
830.860921	73481.843932	33.609908
832.003850	73595.837380	33.614925
832.747932	73720.129935	33.619943
833.369130	73838.214152	33.624960
834.070976	73972.684495	33.629978
834.564678	74086.262959	33.634996
835.538742	74214.087192	33.640013
836.173584	74342.916929	33.645031
837.329115	74465.754307	33.650048
837.753937	74596.081204	33.655066
838.455623	74726.660335	33.660084
839.642353	74859.126951	33.665101
840.257569	74996.413333	33.670119
841.205191	75120.300686	33.675136
841.978882	75255.557577	33.680154
843.037994	75388.851716	33.685172
843.785192	75520.686639	33.690189
844.421150	75656.373548	33.695207
845.517714	75786.621689	33.700224
846.674144	75931.597552	33.705242
847.276675	76072.048814	33.710260
848.331360	76202.976770	33.715277
848.808654	76345.657870	33.720295
849.740733	76474.273799	33.725312
850.435487	76609.678524	33.730330
851.288066	76759.105945	33.735348
852.649854	76901.587412	33.740365
853.423370	77039.125939	33.745383
854.172377	77171.666146	33.750400
854.803478	77319.109895	33.755418
855.898346	77457.331584	33.760436
856.694086	77605.445776	33.765453
857.463082	77742.976740	33.770471
858.466727	77886.295425	33.775488
859.270620	78028.648646	33.780506
859.692781	78170.483958	33.785524
861.001738	78304.361510	33.790541
861.801098	78467.383702	33.795559
862.772683	78605.968130	33.800576
863.313351	78755.416203	33.805594
864.291043	78906.874141	33.810612
865.419440	79053.848545	33.815629
866.103132	79204.528439	33.820647
867.117296	79344.337570	33.825664
867.890261	79494.688348	33.830682
868.840121	79641.253299	33.835700
869.457528	79787.753989	33.840717
870.360734	79934.518335	33.845735
871.282041	80078.060703	33.850752
872.060796	80231.850443	33.855770
873.081350	80386.398325	33.860788
874.115838	80545.164486	33.865805
874.551791	80696.141999	33.870823
876.038339	80839.646317	33.875840
877.232494	80980.707354	33.880858
877.858854	81129.404106	33.885876
878.633451	81281.057017	33.890893
879.518173	81422.260528	33.895911
880.598226	81569.107405	33.900928
881.196807	81721.937435	33.905946
881.957402	81879.929424	33.910964
883.329875	82015.621475	33.915981
884.260742	82161.630092	33.920999
884.731211	82304.432261	33.926016
885.594244	82452.915005	33.931034
886.773872	82599.277522	33.936052
887.917887	82739.035418	33.941069
888.552749	82885.021665	33.946087
889.102775	83015.800545	33.951104
890.102175	83156.426357	33.956122
891.052966	83300.199204	33.961140
891.882628	83416.287359	33.966157
892.795970	83567.938763	33.971175
893.469033	83695.341527	33.976192
894.385380	83841.173386	33.981210
895.402090	83996.815525	33.986228
896.332675	84126.221722	33.991245
897.057238	84273.062392	33.996263
897.982490	84403.192312	34.001280
898.998046	84546.196599	34.006298
899.602568	84705.214469	34.011316
900.685310	84841.319057	34.016333
901.681636	84990.409804	34.021351
902.576201	85143.359061	34.026368
903.178540	85291.283042	34.031386
904.197617	85441.189147	34.036404
905.118134	85584.652119	34.041421
905.787551	85741.388413	34.046439
906.954596	85885.584424	34.051456
907.879091	86048.209547	34.056474
908.396907	86204.347571	34.061492
909.711456	86361.012961	34.066509
910.378643	86516.033659	34.071527
911.285703	86678.343312	34.076544
911.810896	86838.230387	34.081562
912.860227	87009.706839	34.086580
913.905902	87163.093558	34.091597
914.789576	87325.607701	34.096615
915.789605	87493.197782	34.101632
916.624193	87657.494170	34.106650
917.595319	87828.103564	34.111668
918.776136	87989.883367	34.116685
919.804169	88144.658906	34.121703
920.829177	88303.947991	34.126720
921.897369	88471.312226	34.131738
922.692312	88627.926691	34.136756
923.792154	88786.067531	34.141773
924.469657	88942.551603	34.146791
925.507095	89107.102918	34.151808
926.294685	89273.607889	34.156826
926.689155	89437.210940	34.161844
928.076482	89597.024646	34.166861
928.915297	89762.720819	34.171879
929.583962	89937.363375	34.176896
930.714843	90104.500850	34.181914
931.315298	90276.226951	34.186932
932.833448	90441.954707	34.191949
933.293254	90625.218661	34.196967
934.062057	90787.794361	34.201984
935.298473	90962.521351	34.207002
936.330847	91146.966703	34.212020
937.311526	91311.080480	34.217037
938.012069	91483.735318	34.222055
938.881602	91658.445724	34.227072
939.984192	91823.030152	34.232090
941.170281	91992.247532	34.237108
942.200132	92171.283288	34.242125
943.377759	92328.580085	34.247143
944.479328	92499.492235	34.252160
945.649162	92651.228910	34.257178
946.444830	92816.649326	34.262196
947.404356	92972.277395	34.267213
948.580315	93138.497912	34.272231
949.417148	93296.559877	34.277248
950.668266	93459.307881	34.282266
951.054756	93610.028051	34.287284
952.311514	93757.598648	34.292301
953.168712	93909.768273	34.297319
953.590374	94053.383413	34.302336
954.523082	94209.074402	34.307354
955.722939	94370.596280	34.312372
956.607699	94519.195091	34.317389
957.367813	94669.638419	34.322407
958.017705	94839.508502	34.327424
959.260295	95006.711769	34.332442
959.874772	95176.786252	34.337460
960.985915	95339.474867	34.342477
961.855333	95504.154195	34.347495
962.335303	95672.659127	34.352512
963.330799	95843.694330	34.357530
964.167789	96027.866862	34.362548
964.948039	96203.580202	34.367565
966.102400	96389.753944	34.372583
967.189708	96567.463772	34.377600
968.084954	96740.287877	34.382618
968.694087	96932.310177	34.387636
970.079151	97122.768614	34.392653
971.384424	97311.000669	34.397671
972.054218	97492.989599	34.402688
973.141556	97672.327892	34.407706
974.175811	97854.740304	34.412724
975.365626	98048.479365	34.417741
976.120142	98237.303213	34.422759
977.109431	98415.403172	34.427776
978.211400	98590.510232	34.432794
978.965342	98792.335649	34.437812
980.088594	98976.026618	34.442829
980.763499	99153.063158	34.447847
982.067301	99352.890138	34.452864
983.255465	99540.651674	34.457882
984.026955	99737.258506	34.462900
984.981894	99922.187060	34.467917
986.202637	100110.814784	34.472935
986.983482	100300.409353	34.477952
988.352050	100487.261636	34.482970
989.224890	100681.649322	34.487988
990.046127	100867.157641	34.493005
991.147083	101057.660927	34.498023
992.381563	101248.086562	34.503040
993.536504	101431.391044	34.508058
994.432984	101620.159453	34.513076
995.448877	101807.535519	34.518093
996.821097	101986.730410	34.523111
997.910432	102168.379393	34.528128
999.001672	102356.937354	34.533146
999.539173	102541.282572	34.538164
1000.470493	102716.933583	34.543181
1002.110454	102915.516937	34.548199
1002.853021	103102.782921	34.553216
1004.195753	103269.188226	34.558234
1005.039311	103458.618289	34.563252
1006.528517	103637.672246	34.568269
1007.057535	103821.685981	34.573287
1007.687675	103999.073447	34.578304
1009.072062	104170.752345	34.583322
1010.016227	104354.460550	34.588340
1011.008141	104542.012215	34.593357
1012.164570	104716.632589	34.598375
1012.972544	104906.002995	34.603392
1013.583551	105081.387204	34.608410
1014.582343	105270.424714	34.613428
1015.730095	105462.807875	34.618445
1016.555766	105649.293025	34.623463
1017.461048	105844.518066	34.628480
1018.657768	106016.391985	34.633498
1019.395461	106200.514456	34.638516
1020.447095	106380.925938	34.643533
1021.182199	106567.141192	34.648551
1021.971844	106759.263641	34.653568
1023.211803	106936.734619	34.658586
1023.931877	107131.632402	34.663604
1025.080913	107324.269454	34.668621
1026.067726	107515.300783	34.673639
1026.916126	107707.622978	34.678656
1028.006174	107905.061781	34.683674
1029.107638	108110.239316	34.688692
1030.069508	108307.828928	34.693709
1031.470305	108510.464718	34.698727
1032.069442	108706.369230	34.703744
1032.958585	108907.673923	34.708762
1034.043697	109111.139079	34.713780
1035.197295	109331.796182	34.718797
1036.400040	109525.162083	34.723815
1037.189406	109740.055871	34.728832
1038.428599	109944.312484	34.733850
1039.213231	110154.447430	34.738868
1040.396649	110359.742429	34.743885
1041.726684	110566.281481	34.748903
1042.293329	110785.261256	34.753920
1043.296051	110998.571534	34.758938
1044.605366	111209.995939	34.763956
1045.525966	111427.288154	34.768973
1046.673641	111647.838229	34.773991
1047.487356	111865.556943	34.779008
1048.724829	112076.885857	34.784026
1049.498350	112308.119044	34.789044
1050.899842	112526.353854	34.794061
1052.597377	112731.366150	34.799079
1053.285879	112954.688271	34.804096
1054.400199	113161.143034	34.809114
1055.742097	113389.529454	34.814132
1056.668822	113588.189049	34.819149
1057.822173	113805.651420	34.824167
1058.363263	114029.690627	34.829184
1059.764028	114246.912809	34.834202
1060.951925	114461.726683	34.839220
1061.922955	114681.709166	34.844237
1063.149735	114895.873782	34.849255
1063.965164	115113.072720	34.854272
1064.947113	115323.682884	34.859290
1066.362400	115547.475587	34.864308
1067.318664	115771.117887	34.869325
1068.218405	115977.970867	34.874343
1069.550918	116207.940077	34.879360
1070.869034	116429.019042	34.884378
1072.058262	116644.685471	34.889396
1073.216002	116869.329370	34.894413
1074.104191	117072.163003	34.899431
1074.916204	117294.637388	34.904448
1075.988664	117507.656122	34.909466
1077.148050	117737.476178	34.914484
1078.113953	117953.848244	34.919501
1079.483602	118166.442590	34.924519
1080.289834	118390.345535	34.929536
1081.393097	118604.330271	34.934554
1082.744035	118821.494137	34.939572
1083.774299	119054.653200	34.944589
1085.074983	119267.203661	34.949607
1085.728779	119484.082242	34.954624
1087.239626	119689.923140	34.959642
1088.011775	119916.757939	34.964660
1089.215888	120138.973896	34.969677
1090.555486	120345.430620	34.974695
1091.375769	120553.520635	34.979712
1092.157181	120750.391077	34.984730
1093.582999	120960.563459	34.989748
1094.261804	121165.449780	34.994765
1095.780506	121370.033927	34.999783
1096.751712	121587.395117	35.004800
1097.668863	121787.177360	35.009818
1098.668249	121994.677648	35.014836
1099.745558	122220.846078	35.019853
1101.039459	122423.434346	35.024871
1102.000666	122648.218532	35.029888
1103.145962	122864.330997	35.034906
1104.106589	123086.165766	35.039924
1105.008556	123301.003609	35.044941
1106.061191	123524.511939	35.049959
1107.284291	123757.993033	35.054976
1108.397026	123979.695191	35.059994
1109.567998	124200.552896	35.065012
1110.423030	124432.477843	35.070029
1111.648444	124666.764020	35.075047
1112.697686	124905.922539	35.080064
1113.959719	125126.962050	35.085082
1115.196529	125361.441810	35.090100
1116.038964	125598.865598	35.095117
1117.621523	125826.447743	35.100135
1118.497901	126062.297913	35.105152
1119.687044	126296.919472	35.110170
1120.903088	126541.031592	35.115188
1121.780863	126780.575333	35.120205
1123.361502	127013.730756	35.125223
1124.318221	127253.658036	35.130240
1125.188819	127485.413420	35.135258
1126.712970	127716.821671	35.140276
1127.784772	127963.060245	35.145293
1128.975999	128201.866031	35.150311
1129.984168	128432.997330	35.155328
1131.150609	128676.323252	35.160346
1132.415290	128914.146339	35.165364
1133.378002	129154.480215	35.170381
1135.041615	129385.941167	35.175399
1135.822300	129622.898958	35.180416
1136.664997	129864.538352	35.185434
1138.096663	130105.283646	35.190452
1138.893695	130357.468088	35.195469
1140.213631	130588.804535	35.200487
1141.256746	130840.787349	35.205504
1142.235261	131087.851733	35.210522
1143.563736	131326.443012	35.215540
1144.781145	131577.071806	35.220557
1146.047362	131814.599514	35.225575
1147.113772	132062.176641	35.230592
1148.503317	132318.423928	35.235610
1149.681508	132549.240215	35.240628
1150.710264	132805.994715	35.245645
1152.131032	133046.370977	35.250663
1153.173231	133295.787083	35.255680
1154.563193	133523.482074	35.260698
1155.807854	133760.736091	35.265716
1156.766526	134003.350987	35.270733
1157.747075	134240.842321	35.275751
1158.987825	134484.225526	35.280768
1160.624938	134721.852694	35.285786
1162.173472	134958.786266	35.290804
1163.197827	135194.578432	35.295821
1164.446199	135429.536537	35.300839
1165.744265	135665.793950	35.305856
1166.736570	135880.753450	35.310874
1168.143687	136095.176677	35.315892
1168.890400	136316.315901	35.320909
1170.016170	136540.525520	35.325927
1171.366373	136744.020814	35.330944
1172.380051	136969.684526	35.335962
1173.500532	137184.770726	35.340980
1174.325505	137414.132780	35.345997
1175.512275	137629.870178	35.351015
1176.617518	137861.420442	35.356032
1177.660919	138086.820495	35.361050
1178.678099	138325.311272	35.366068
1179.860146	138559.097839	35.371085
1181.046196	138793.658796	35.376103
1182.036511	139026.973108	35.381120
1183.136952	139273.825209	35.386138
1184.284326	139513.482007	35.391156
1185.392013	139771.380440	35.396173
1186.599030	140019.843316	35.401191
1187.415105	140261.043646	35.406208
1188.768548	140519.287476	35.411226
1189.931587	140776.626391	35.416244
1191.629424	141027.145660	35.421261
1193.071369	141268.731431	35.426279
1193.779404	141528.535036	35.431296
1194.976091	141789.388369	35.436314
1196.404163	142043.294522	35.441332
1197.473908	142301.344912	35.446349
1198.375371	142560.997430	35.451367
1199.740599	142815.756505	35.456384
1200.906761	143078.539300	35.461402
1202.279667	143336.154079	35.466420
1203.437335	143599.956643	35.471437
1204.722798	143849.029883	35.476455
1206.020272	144123.199121	35.481472
1207.082586	144391.499826	35.486490
1208.586159	144644.727444	35.491508
1209.940149	144907.911238	35.496525
1211.202827	145165.100963	35.501543
1212.527389	145419.517685	35.506560
1213.594693	145681.778052	35.511578
1215.223886	145939.090278	35.516596
1216.131272	146206.491706	35.521613
1217.576423	146467.845632	35.526631
1218.717919	146719.410252	35.531648
1219.846828	146975.607725	35.536666
1221.592358	147233.011360	35.541684
1222.765974	147506.541970	35.546701
1224.229336	147752.049022	35.551719
1225.489955	147999.303383	35.556736
1226.443318	148247.738954	35.561754
1227.768620	148499.323469	35.566772
1228.946135	148771.442365	35.571789
1230.472060	149016.769937	35.576807
1231.824216	149259.362945	35.581824
1232.464277	149519.857010	35.586842
1233.865006	149770.473753	35.591860
1235.083042	150032.271014	35.596877
1236.519369	150286.487393	35.601895
1238.046064	150537.836769	35.606912
1239.100106	150795.759940	35.611930
1240.573748	151042.809035	35.616948
1241.726701	151293.844710	35.621965
1242.802891	151546.442163	35.626983
1243.982021	151793.823873	35.632000
1245.013095	152044.212400	35.637018
1246.834556	152297.617582	35.642036
1247.954730	152540.333445	35.647053
1248.960011	152795.475026	35.652071
1250.165743	153029.694078	35.657088
1250.814822	153269.359376	35.662106
1252.432098	153506.735140	35.667124
1253.676430	153764.837154	35.672141
1255.061392	154000.224808	35.677159
1256.399929	154235.215648	35.682176
1257.181743	154489.542760	35.687194
1258.322640	154728.133662	35.692212
1259.346709	154980.305546	35.697229
1260.754867	155234.445173	35.702247
1262.217384	155488.006625	35.707264
1263.438249	155749.347622	35.712282
1264.682978	155993.662743	35.717300
1265.790597	156258.349359	35.722317
1266.844023	156526.205371	35.727335
1268.202806	156778.561727	35.732352
1269.549540	157048.148737	35.737370
1270.747647	157300.775968	35.742388
1272.065880	157579.365419	35.747405
1273.098642	157842.780929	35.752423
1274.438945	158109.090468	35.757440
1275.538024	158385.793433	35.762458
1277.620161	158656.487502	35.767476
1278.731806	158934.511480	35.772493
1279.640437	159205.504636	35.777511
1281.013331	159471.208751	35.782528
1281.933358	159762.070570	35.787546
1283.363069	160038.920366	35.792564
1284.742796	160311.758615	35.797581
1286.049381	160601.369909	35.802599
1287.196978	160872.423322	35.807616
1288.688802	161168.110299	35.812634
1290.214242	161441.566220	35.817652
1291.124978	161718.246536	35.822669
1292.185164	162011.105460	35.827687
1293.680665	162301.623457	35.832704
1295.027872	162596.253277	35.837722
1296.192137	162880.245265	35.842740
1297.880047	163175.419101	35.847757
1298.873558	163460.927616	35.852775
1300.303288	163748.776597	35.857792
1301.568751	164047.896007	35.862810
1303.088803	164327.398078	35.867828
1304.588478	164626.711174	35.872845
1305.437315	164913.293633	35.877863
1307.319075	165201.902309	35.882880
1308.270218	165504.991654	35.887898
1309.716171	165794.678640	35.892916
1311.199932	166081.937814	35.897933
1312.408558	166373.685285	35.902951
1313.847912	166658.049901	35.907968
1314.928176	166960.531563	35.912986
1316.216066	167250.622189	35.918004
1317.460077	167547.599265	35.923021
1318.721469	167844.169396	35.928039
1320.597288	168128.826546	35.933056
1321.599320	168428.196891	35.938074
1322.806699	168724.185360	35.943092
1324.207266	169018.989118	35.948109
1325.641517	169318.661897	35.953127
1326.976268	169609.940052	35.958144
1328.125065	169916.617689	35.963162
1329.292016	170213.041245	35.968180
1330.912502	170512.500704	35.973197
1332.133768	170808.183107	35.978215
1333.482070	171100.318648	35.983232
1334.737493	171401.455774	35.988250
1336.330734	171695.001201	35.993268
1337.328474	171977.631966	35.998285
1338.567275	172271.061909	36.003303
1340.032267	172543.428723	36.008320
1341.244145	172826.942875	36.013338
1342.848680	173109.112107	36.018356
1343.901319	173400.688950	36.023373
1345.018276	173686.317810	36.028391
1347.075464	173973.341231	36.033408
1348.198846	174275.191019	36.038426
1349.393678	174551.129210	36.043444
1350.945049	174846.845691	36.048461
1352.023642	175144.038091	36.053479
1353.329728	175445.661904	36.058496
1354.623077	175741.731026	36.063514
1356.154160	176043.321327	36.068532
1357.464131	176331.763920	36.073549
1358.390319	176642.278176	36.078567
1359.906232	176932.720822	36.083584
1361.053904	177257.403863	36.088602
1362.382580	177567.527383	36.093620
1363.609776	177871.412663	36.098637
1364.553664	178192.467563	36.103655
1366.619453	178518.441153	36.108672
1367.514920	178842.528784	36.113690
1368.981759	179155.355221	36.118708
1370.642278	179477.797422	36.123725
1371.795218	179812.966757	36.128743
1373.344803	180131.699924	36.133760
1374.597599	180462.897028	36.138778
1375.920756	180786.646951	36.143796
1377.759088	181114.692592	36.148813
1378.901314	181437.816429	36.153831
1380.101431	181765.032345	36.158848
1381.889333	182097.268247	36.163866
1383.226318	182424.490988	36.168884
1384.676100	182754.933731	36.173901
1386.069024	183094.983653	36.178919
1387.331080	183418.962781	36.183936
1388.671143	183748.274682	36.188954
1389.988213	184077.960472	36.193972
1391.500934	184418.493905	36.198989
1393.406272	184749.343138	36.204007
1394.636380	185078.262320	36.209024
1396.195192	185415.798680	36.214042
1397.454533	185749.540469	36.219060
1399.247609	186081.748993	36.224077
1400.310463	186426.012091	36.229095
1402.072308	186757.925116	36.234112
1403.478640	187089.949604	36.239130
1404.948933	187412.432426	36.244148
1406.188550	187740.007335	36.249165
1407.261474	188086.665236	36.254183
1409.116928	188412.542764	36.259200
1410.934236	188740.218289	36.264218
1412.110227	189077.293739	36.269236
1413.239638	189408.945698	36.274253
1414.557349	189742.967627	36.279271
1416.376970	190069.215723	36.284288
1417.704986	190405.638910	36.289306
1418.926755	190723.090579	36.294324
1420.442883	191056.173070	36.299341
1421.486552	191397.688538	36.304359
1423.142175	191725.724587	36.309376
1424.428741	192067.686077	36.314394
1425.943953	192402.248682	36.319412
1427.313314	192726.021139	36.324429
1428.480263	193079.509600	36.329447
1430.336024	193402.291172	36.334464
1431.796094	193731.169973	36.339482
1433.008633	194053.274083	36.344500
1434.532204	194369.806009	36.349517
1435.499453	194677.544724	36.354535
1437.190906	195002.926077	36.359552
1438.456868	195327.985829	36.364570
1440.159504	195641.663377	36.369588
1441.773865	195956.969367	36.374605
1443.307006	196289.822956	36.379623
1444.684788	196597.160192	36.384640
1446.549173	196928.502284	36.389658
1447.293621	197255.536773	36.394676
1449.229309	197570.772011	36.399693
1450.116027	197903.892883	36.404711
1451.824158	198240.739262	36.409728
1453.284628	198578.847063	36.414746
1454.345660	198911.664783	36.419764
1455.825396	199245.430634	36.424781
1457.090723	199599.903019	36.429799
1458.408793	199938.815526	36.434816
1459.722749	200294.997428	36.439834
1460.945856	200645.381186	36.444852
1462.532436	200999.566366	36.449869
1463.859722	201358.735123	36.454887
1465.242378	201722.213394	36.459904
1466.709652	202094.465637	36.464922
1468.111156	202452.230968	36.469940
1469.634890	202824.274483	36.474957
1471.050655	203191.804941	36.479975
1472.485171	203575.624321	36.484992
1473.935617	203946.390523	36.490010
1475.318293	204316.953913	36.495028
1477.169731	204696.685194	36.500045
1478.711627	205077.117083	36.505063
1480.120250	205448.938749	36.510080
1481.633514	205832.667716	36.515098
1483.019099	206213.181849	36.520116
1484.295503	206583.722984	36.525133
1485.971813	206978.071117	36.530151
1487.186465	207356.155714	36.535168
1488.966124	207742.732354	36.540186
1490.388689	208137.432895	36.545204
1491.803100	208523.718094	36.550221
1493.289856	208922.678292	36.555239
1494.669876	209308.109423	36.560256
1496.316015	209707.466113	36.565274
1497.954739	210100.832482	36.570292
1499.438823	210496.765851	36.575309
1500.914410	210896.588095	36.580327
1502.239953	211288.183182	36.585344
1504.151237	211680.775317	36.590362
1505.471786	212088.653984	36.595380
1507.093661	212481.373723	36.600397
1508.312322	212877.818964	36.605415
1509.848743	213269.362652	36.610432
1511.933836	213671.179381	36.615450
1513.254311	214073.860735	36.620468
1514.724695	214466.334788	36.625485
1516.131049	214874.516658	36.630503
1517.629292	215269.859404	36.635520
1519.329023	215666.821362	36.640538
1520.989682	216065.874043	36.645556
1522.268507	216458.591225	36.650573
1524.173843	216856.514649	36.655591
1525.351238	217263.474656	36.660608
1527.486923	217653.515269	36.665626
1529.011818	218063.519712	36.670644
1530.210399	218435.431488	36.675661
1531.960638	218825.235543	36.680679
1533.715425	219200.740979	36.685696
1535.307101	219554.889125	36.690714
1536.413590	219931.088470	36.695732
1538.212731	220298.615341	36.700749
1539.593495	220676.753118	36.705767
1541.092171	221047.761043	36.710784
1542.606447	221421.409154	36.715802
1543.998945	221798.634529	36.720820
1545.498341	222173.836991	36.725837
1546.891120	222555.128748	36.730855
1548.460823	222954.045113	36.735872
1549.860377	223338.919683	36.740890
1551.725514	223731.059078	36.745908
1553.052456	224135.658315	36.750925
1553.887895	224590.580758	36.755943
1555.647972	224992.698370	36.760960
1557.262004	225401.013613	36.765978
1558.817231	225814.546919	36.770996
1560.320771	226222.933927	36.776013
1562.002571	226627.838389	36.781031
1563.193965	227045.322058	36.786048
1564.797530	227456.338105	36.791066
1566.227400	227886.358217	36.796084
1568.105494	228309.523747	36.801101
1569.422328	228729.633662	36.806119
1571.023149	229154.498668	36.811136
1572.797970	229574.027485	36.816154
1574.245576	230011.290544	36.821172
1576.065969	230432.135212	36.826189
1577.985041	230859.594438	36.831207
1579.590057	231293.685646	36.836224
1581.413337	231701.350352	36.841242
1582.572129	232138.769046	36.846260
1584.209874	232556.982750	36.851277
1585.414164	232988.706447	36.856295
1587.440931	233425.248700	36.861312
1589.415555	233856.974475	36.866330
1590.908439	234288.653955	36.871348
1592.801930	234709.853735	36.876365
1594.293914	235139.452605	36.881383
1595.816060	235576.642649	36.886400
1597.756653	236005.178861	36.891418
1599.313945	236437.894498	36.896436
1600.868177	236862.838693	36.901453
1602.363303	237278.801342	36.906471
1603.835612	237713.464499	36.911488
1605.756476	238142.262865	36.916506
1607.416276	238575.042598	36.921524
1609.263716	238999.511163	36.926541
1610.947850	239430.281905	36.931559
1611.816772	239852.983270	36.936576
1614.060690	240280.945202	36.941594
1615.250845	240723.688361	36.946612
1616.976034	241144.574170	36.951629
1618.434238	241578.841103	36.956647
1620.198396	242025.302263	36.961664
1622.223340	242449.468563	36.966682
1623.357682	242896.390956	36.971700
1625.367990	243322.415503	36.976717
1626.883949	243745.575688	36.981735
1628.344546	244190.693568	36.986752
1629.847136	244621.833724	36.991770
1631.225611	245062.216212	36.996788
1632.777441	245499.903415	37.001805
1634.430494	245943.518768	37.006823
1636.166128	246389.813791	37.011840
1638.109803	246822.179670	37.016858
1639.189137	247256.517876	37.021876
1640.736306	247668.018294	37.026893
1642.602905	248099.687158	37.031911
1644.048853	248526.142165	37.036928
1646.008412	248952.004718	37.041946
1647.488036	249375.762317	37.046964
1648.873605	249800.196337	37.051981
1650.918487	250232.142763	37.056999
1652.267903	250672.816106	37.062016
1654.107012	251098.522701	37.067034
1655.227372	251539.590245	37.072052
1656.808680	251993.893245	37.077069
1658.737573	252435.869424	37.082087
1660.052199	252884.196551	37.087104
1661.769288	253321.737322	37.092122
1663.304346	253781.790269	37.097140
1664.735766	254243.842038	37.102157
1666.679426	254701.948127	37.107175
1668.189100	255169.703134	37.112192
1670.105521	255616.560450	37.117210
1671.839937	256081.408099	37.122228
1673.201475	256549.696111	37.127245
1675.201512	257019.021914	37.132263
1676.774308	257500.916797	37.137280
1678.464664	257958.405153	37.142298
1679.810696	258442.573080	37.147316
1681.732544	258921.946292	37.152333
1683.241986	259396.205332	37.157351
1684.884935	259890.002817	37.162368
1686.795536	260369.987429	37.167386
1688.320026	260865.277690	37.172404
1689.771588	261349.834274	37.177421
1691.824356	261830.125257	37.182439
1693.196977	262325.186084	37.187456
1695.421089	262812.637487	37.192474
1696.754094	263317.383017	37.197492
1698.469582	263812.411853	37.202509
1700.089101	264302.909053	37.207527
1702.056410	264808.387158	37.212544
1703.791276	265298.000886	37.217562
1705.380093	265810.450368	37.222580
1706.965421	266312.510085	37.227597
1708.795748	266813.385721	37.232615
1710.640193	267310.651285	37.237632
1712.418794	267816.869067	37.242650
1713.971166	268332.141705	37.247668
1716.059815	268835.919197	37.252685
1717.901053	269338.720800	37.257703
1719.218712	269850.651652	37.262720
1721.216499	270351.444600	37.267738
1723.008482	270859.586836	37.272756
1724.495509	271373.849934	37.277773
1726.408110	271879.633601	37.282791
1727.979583	272390.654934	37.287808
1729.650171	272895.790997	37.292826
1731.262236	273416.685460	37.297844
1733.205084	273925.610497	37.302861
1735.149156	274436.287135	37.307879
1736.821287	274948.049178	37.312896
1739.077031	275457.249746	37.317914
1740.342734	275972.937951	37.322932
1742.188799	276481.975376	37.327949
1743.851087	276992.896383	37.332967
1745.235516	277510.009437	37.337984
1747.460088	278021.012993	37.343002
1748.831522	278534.289986	37.348020
1750.563498	279051.646673	37.353037
1752.737960	279548.810603	37.358055
1754.590403	280055.780769	37.363072
1756.338824	280542.877152	37.368090
1758.260282	281025.142752	37.373108
1759.576934	281504.788985	37.378125
1761.299501	281991.555541	37.383143
1762.847266	282492.676074	37.388160
1764.816528	282976.020710	37.393178
1766.406098	283483.786584	37.398196
1768.051068	283993.116619	37.403213
1769.910388	284479.599344	37.408231
1771.233987	284990.706549	37.413248
1773.188743	285500.488576	37.418266
1774.875638	286019.940097	37.423284
1776.533530	286544.246164	37.428301
1778.229296	287054.675267	37.433319
1779.727928	287575.371591	37.438336
1781.720161	288102.741032	37.443354
1783.438489	288642.853949	37.448372
1784.939534	289178.301531	37.453389
1786.933762	289714.071922	37.458407
1788.640441	290251.792630	37.463424
1790.428619	290795.212655	37.468442
1791.956566	291339.511529	37.473460
1793.482636	291886.602322	37.478477
1795.746554	292434.203815	37.483495
1797.190811	292992.250438	37.488512
1798.965664	293552.373400	37.493530
1801.013344	294118.341278	37.498548
1802.500054	294681.554295	37.503565
1804.690700	295243.225905	37.508583
1806.392116	295812.112599	37.513600
1808.742191	296377.206384	37.518618
1809.999305	296940.014035	37.523636
1811.881159	297511.478057	37.528653
1813.814130	298076.707903	37.533671
1815.652102	298661.405460	37.538688
1817.814071	299232.661321	37.543706
1819.707478	299799.589826	37.548724
1821.202331	300379.863997	37.553741
1823.225421	300949.482035	37.558759
1825.045238	301541.861105	37.563776
1826.903140	302104.870783	37.568794
1828.457125	302686.492673	37.573812
1830.382649	303275.211537	37.578829
1832.484648	303846.043420	37.583847
1834.183459	304433.573161	37.588864
1836.028265	305020.414607	37.593882
1837.827382	305602.154999	37.598900
1839.636422	306190.746848	37.603917
1841.528173	306774.419555	37.608935
1843.448353	307366.413407	37.613952
1845.210934	307951.470669	37.618970
1847.276034	308553.057130	37.623988
1848.793255	309137.562373	37.629005
1850.727259	309727.683081	37.634023
1852.691005	310318.378602	37.639040
1854.577085	310918.757945	37.644058
1856.511926	311509.677826	37.649076
1857.819895	312107.324638	37.654093
1860.065194	312692.343431	37.659111
1862.103105	313303.395396	37.664128
1864.127118	313891.209330	37.669146
1866.232834	314488.680051	37.674164
1868.021815	315077.437469	37.679181
1869.706628	315670.498740	37.684199
1871.958915	316261.887023	37.689216
1873.538164	316852.213437	37.694234
1875.398541	317438.019368	37.699252
1877.026044	318015.174632	37.704269
1879.147080	318574.189754	37.709287
1881.209639	319139.684878	37.714304
1882.688006	319703.621264	37.719322
1884.629420	320283.168361	37.724340
1886.483532	320855.488290	37.729357
1888.025140	321418.333188	37.734375
1890.296125	322009.769777	37.739392
1891.701867	322589.918046	37.744410
1893.629527	323172.488501	37.749428
1895.444521	323769.112916	37.754445
1897.077348	324357.306904	37.759463
1898.905794	324957.015292	37.764480
1900.602147	325562.782312	37.769498
1902.595812	326154.911044	37.774516
1904.270163	326780.219155	37.779533
1906.092543	327388.308218	37.784551
1907.836641	327997.698778	37.789568
1909.768011	328626.677071	37.794586
1912.119908	329258.168691	37.799604
1913.463243	329890.149975	37.804621
1915.585852	330513.414728	37.809639
1917.418563	331149.413972	37.814656
1919.045146	331791.025122	37.819674
1921.075009	332424.971778	37.824692
1922.552519	333084.464583	37.829709
1924.652614	333725.898923	37.834727
1926.882243	334392.943600	37.839744
1928.381227	335057.638294	37.844762
1930.353788	335697.648627	37.849780
1932.322747	336366.031692	37.854797
1934.304713	337031.814906	37.859815
1936.309950	337705.987809	37.864832
1938.336896	338383.778155	37.869850
1940.815989	339044.452747	37.874868
1942.594620	339718.103486	37.879885
1944.236406	340381.360969	37.884903
1946.580871	341064.875488	37.889920
1948.671129	341739.564281	37.894938
1950.679220	342408.470387	37.899956
1952.112221	343095.584361	37.904973
1954.148560	343770.101613	37.909991
1956.155598	344439.487361	37.915008
1957.914500	345126.670665	37.920026
1960.425141	345809.862124	37.925044
1962.560534	346499.171202	37.930061
1964.352382	347185.227501	37.935079
1966.715388	347866.179704	37.940096
1968.612958	348547.300112	37.945114
1970.788975	349227.552223	37.950132
1972.627606	349913.305886	37.955149
1974.742285	350587.152388	37.960167
1976.604989	351266.054811	37.965184
1978.215981	351954.402888	37.970202
1980.393569	352634.906948	37.975220
1982.385228	353331.823531	37.980237
1984.232215	354017.892216	37.985255
1986.735852	354698.588930	37.990272
1988.714076	355386.237865	37.995290
1990.655966	356063.097720	38.000308
1992.544906	356755.027129	38.005325
1994.691982	357443.197942	38.010343
1996.491561	358129.029625	38.015360
1998.180434	358829.228686	38.020378
2000.585463	359508.264373	38.025396
2002.352530	360199.749740	38.030413
2004.809747	360888.039382	38.035431
2006.791168	361569.342730	38.040448
2008.899398	362236.355530	38.045466
2010.882420	362891.200337	38.050484
2012.651396	363547.008158	38.055501
2014.635443	364205.636046	38.060519
2016.335221	364869.601568	38.065536
2018.283305	365536.076738	38.070554
2020.367133	366201.934388	38.075572
2022.366020	366868.529985	38.080589
2024.121697	367539.009613	38.085607
2025.971121	368224.960323	38.090624
2027.668548	368909.680554	38.095642
2029.937214	369590.412937	38.100660
2031.926215	370286.346834	38.105677
2034.270896	370979.799147	38.110695
2036.037324	371677.594722	38.115712
2037.835289	372374.788220	38.120730
2039.714607	373072.588768	38.125748
2041.742393	373788.459609	38.130765
2043.665321	374500.757287	38.135783
2045.707626	375219.107453	38.140800
2047.318121	375953.947704	38.145818
2049.682708	376671.758188	38.150836
2051.897866	377405.098345	38.155853
2054.238849	378138.376673	38.160871
2056.275201	378870.852672	38.165888
2058.276586	379604.611833	38.170906
2060.396680	380334.557167	38.175924
2062.198672	381081.096959	38.180941
2064.368233	381830.170972	38.185959
2066.562262	382566.368721	38.190976
2068.246012	383321.041861	38.195994
2070.308693	384066.380663	38.201012
2072.506369	384823.292059	38.206029
2074.382049	385588.858898	38.211047
2076.987276	386349.850319	38.216064
2079.075505	387104.418802	38.221082
2081.241696	387865.344959	38.226100
2083.241683	388624.530951	38.231117
2085.329944	389395.040780	38.236135
2087.559983	390153.948764	38.241152
2089.299041	390924.681018	38.246170
2091.600082	391689.978056	38.251188
2093.870249	392468.847302	38.256205
2095.403264	393233.826775	38.261223
2098.010064	394008.672080	38.266240
2100.202227	394787.925272	38.271258
2102.164870	395566.537039	38.276276
2104.538901	396346.048898	38.281293
2106.622834	397120.113835	38.286311
2108.582685	397896.814498	38.291328
2110.448857	398676.272254	38.296346
2112.724508	399460.684447	38.301364
2114.801722	400238.924896	38.306381
2116.818121	401033.042560	38.311399
2119.286124	401811.530482	38.316416
2121.259925	402613.364939	38.321434
2123.734145	403396.698588	38.326452
2125.582373	404177.858671	38.331469
2127.513425	404965.064007	38.336487
2129.922010	405763.062626	38.341504
2132.061854	406553.633993	38.346522
2134.102707	407340.297428	38.351540
2136.493847	408128.653738	38.356557
2138.561803	408927.756349	38.361575
2140.899131	409709.970268	38.366592
2142.704730	410508.385331	38.371610
2145.222843	411295.488093	38.376628
2147.075248	412077.611437	38.381645
2149.293109	412849.468985	38.386663
2151.350759	413612.009453	38.391680
2153.459428	414368.795219	38.396698
2155.528388	415125.616211	38.401716
2158.048090	415882.745934	38.406733
2159.600646	416660.704029	38.411751
2161.709133	417415.475935	38.416768
2163.870087	418192.679281	38.421786
2166.621394	418963.101415	38.426804
2168.706452	419733.432794	38.431821
2170.861901	420505.830683	38.436839
2172.517293	421292.087181	38.441856
2174.777565	422075.028719	38.446874
2176.813866	422861.679131	38.451892
2179.103102	423647.958909	38.456909
2180.550150	424453.138229	38.461927
2183.062649	425254.013859	38.466944
2184.866814	426065.764640	38.471962
2186.888042	426877.047337	38.476980
2189.215227	427703.643284	38.481997
2191.509134	428529.659325	38.487015
2193.685878	429349.591099	38.492032
2195.502220	430186.209078	38.497050
2197.411036	431020.858550	38.502068
2199.782383	431860.362768	38.507085
2201.800418	432714.928640	38.512103
2204.258121	433563.519122	38.517120
2206.825148	434426.991598	38.522138
2208.956780	435278.761558	38.527156
2210.940214	436133.864611	38.532173
2213.155214	436994.717358	38.537191
2215.333296	437854.025363	38.542208
2217.701128	438714.332061	38.547226
2219.766777	439589.836468	38.552244
2222.340299	440459.150729	38.557261
2224.573254	441333.445908	38.562279
2226.726731	442201.091552	38.567296
2228.949522	443082.503924	38.572314
2231.153693	443957.357526	38.577332
2233.714871	444843.955325	38.582349
2235.374965	445724.847993	38.587367
2237.857262	446608.806614	38.592384
2239.783284	447505.567955	38.597402
2242.139231	448405.458050	38.602420
2244.499182	449299.189314	38.607437
2246.357757	450203.334115	38.612455
2248.653881	451098.112641	38.617472
2251.164906	452007.180458	38.622490
2253.532847	452920.278059	38.627508
2255.762149	453821.120763	38.632525
2257.724105	454740.526427	38.637543
2259.939787	455651.455493	38.642560
2262.250692	456580.985876	38.647578
2264.148650	457495.020172	38.652596
2266.641664	458415.538212	38.657613
2268.648665	459347.418961	38.662631
2270.847755	460278.466572	38.667648
2273.156584	461216.479342	38.672666
2275.553430	462147.002858	38.677684
2277.916316	463079.813454	38.682701
2279.592676	464015.574270	38.687719
2281.952220	464961.336566	38.692736
2284.158659	465910.818273	38.697754
2285.978489	466861.075533	38.702772
2288.747245	467805.722516	38.707789
2291.015096	468764.150385	38.712807
2293.133088	469724.273125	38.717824
2295.083312	470673.108008	38.722842
2297.462631	471614.448323	38.727860
2299.646242	472545.922533	38.732877
2301.846050	473499.576236	38.737895
2304.274789	474437.887875	38.742912
2306.499550	475377.802489	38.747930
2308.715116	476332.925425	38.752948
2311.180903	477259.067055	38.757965
2313.725151	478213.179921	38.762983
2315.947028	479154.014067	38.768000
2318.232581	480102.111849	38.773018
2320.318971	481063.322540	38.778036
2322.696223	482015.597579	38.783053
2324.606795	482983.552018	38.788071
2327.006078	483947.788865	38.793088
2329.299070	484931.529709	38.798106
2331.479714	485908.520318	38.803124
2333.769363	486884.277997	38.808141
2336.208911	487889.133578	38.813159
2338.568662	488869.060321	38.818176
2341.238663	489870.836627	38.823194
2343.274009	490863.272593	38.828212
2345.814591	491864.904753	38.833229
2347.572628	492870.039441	38.838247
2349.850500	493884.263918	38.843264
2352.647406	494903.085652	38.848282
2354.588242	495923.602222	38.853300
2357.443328	496943.906491	38.858317
2359.591983	497985.302808	38.863335
2361.992893	499017.159587	38.868352
2364.145793	500050.153800	38.873370
2366.555300	501090.002231	38.878388
2369.182026	502128.286930	38.883405
2371.736099	503169.140807	38.888423
2373.715391	504207.703803	38.893440
2376.308246	505258.555024	38.898458
2378.658907	506316.588942	38.903476
2381.022402	507365.123138	38.908493
2383.763654	508427.946110	38.913511
2386.011143	509481.201700	38.918528
2388.697636	510540.919260	38.923546
2390.892144	511599.185708	38.928564
2393.487020	512652.728785	38.933581
2395.419281	513727.378133	38.938599
2397.872306	514788.210653	38.943616
2400.823550	515856.800823	38.948634
2402.898839	516924.353696	38.953652
2405.439345	517988.985159	38.958669
2407.994174	519069.058812	38.963687
2410.405290	520135.528376	38.968704
2413.071594	521198.355322	38.973722
2415.295947	522288.029523	38.978740
2418.265131	523354.685751	38.983757
2420.503008	524422.243643	38.988775
2422.997339	525488.626003	38.993792
2426.091129	526559.869458	38.998810
2427.938554	527632.500599	39.003828
2430.623837	528685.782966	39.008845
2433.209082	529760.102382	39.013863
2435.681890	530823.085240	39.018880
2438.078907	531884.594221	39.023898
2440.644507	532962.055615	39.028916
2443.075674	534022.648570	39.033933
2445.769016	535083.825409	39.038951
2448.453185	536150.411313	39.043968
2450.573676	537204.078683	39.048986
2452.963767	538277.197716	39.054004
2455.281289	539326.298801	39.059021
2457.762690	540390.086683	39.064039
2460.090575	541416.995868	39.069056
2462.953267	542449.476666	39.074074
2465.120264	543476.161787	39.079092
2467.794527	544497.708790	39.084109
2470.096054	545525.026092	39.089127
2472.455628	546553.515160	39.094144
2475.025396	547577.065956	39.099162
2477.634113	548607.422875	39.104180
2480.105099	549645.769607	39.109197
2482.423162	550672.852064	39.114215
2484.423148	551719.162787	39.119232
2487.517747	552760.939929	39.124250
2489.608747	553818.785625	39.129268
2492.274170	554873.337741	39.134285
2494.298184	555926.907934	39.139303
2496.871942	556990.957486	39.144320
2499.365650	558056.543296	39.149338
2501.618998	559134.492992	39.154356
2504.398290	560209.153541	39.159373
2506.723392	561283.801535	39.164391
2508.773215	562371.868496	39.169408
2511.683443	563455.534524	39.174426
2514.134046	564567.962763	39.179444
2516.593793	565657.546396	39.184461
2519.142378	566768.414040	39.189479
2521.159393	567879.976669	39.194496
2523.857947	568991.983424	39.199514
2526.127045	570110.138943	39.204532
2529.020790	571247.117127	39.209549
2531.893897	572359.102799	39.214567
2533.996186	573506.548940	39.219584
2536.428643	574624.681146	39.224602
2539.346139	575771.083905	39.229620
2541.771842	576904.317793	39.234637
2544.006684	578042.848101	39.239655
2546.699394	579199.658406	39.244672
2549.475465	580335.230358	39.249690
2551.823918	581489.124380	39.254708
2554.637534	582637.166505	39.259725
2557.287736	583802.377363	39.264743
2559.781058	584969.658713	39.269760
2562.505909	586124.657220	39.274778
2564.932260	587287.465030	39.279796
2567.785550	588437.759611	39.284813
2570.654843	589606.034599	39.289831
2573.325825	590766.560651	39.294848
2576.284440	591917.004496	39.299866
2578.692485	593078.500936	39.304884
2581.599633	594236.644732	39.309901
2583.908986	595392.619256	39.314919
2586.606117	596550.119130	39.319936
2589.525996	597704.011886	39.324954
2591.998329	598870.935245	39.329972
2594.662309	600023.688695	39.334989
2597.435401	601180.064629	39.340007
2599.849137	602351.603749	39.345024
2602.862048	603480.573648	39.350042
2605.219721	604649.234172	39.355060
2607.979621	605804.745687	39.360077
2610.644233	606968.112640	39.365095
2613.281922	608112.399443	39.370112
2616.181731	609255.876573	39.375130
2618.352145	610418.419107	39.380148
2620.828272	611568.384586	39.385165
2623.512724	612725.800274	39.390183
2626.092958	613896.966721	39.395200
2628.960007	615041.607533	39.400218
2631.977672	616187.005033	39.405236
2634.474548	617307.270031	39.410253
2637.095582	618425.250520	39.415271
2639.786559	619537.356574	39.420288
2642.361206	620642.320748	39.425306
2644.863378	621762.677815	39.430324
2647.433135	622873.113155	39.435341
2650.083508	623986.469051	39.440359
2652.751099	625110.299034	39.445376
2655.073615	626231.020784	39.450394
2657.561776	627361.188575	39.455412
2660.150710	628494.866012	39.460429
2662.860926	629634.545249	39.465447
2665.464159	630787.102816	39.470464
2668.022002	631915.625175	39.475482
2670.611870	633076.123100	39.480500
2673.148988	634223.572027	39.485517
2675.929954	635400.154315	39.490535
2678.420395	636565.322318	39.495552
2681.307902	637735.184479	39.500570
2683.062798	638917.475593	39.505588
2685.784371	640108.851267	39.510605
2688.730986	641308.931269	39.515623
2691.237624	642516.624603	39.520640
2693.865165	643709.691640	39.525658
2696.661953	644931.962944	39.530676
2699.209158	646145.102977	39.535693
2701.903173	647373.777629	39.540711
2704.600105	648610.776221	39.545728
2707.205050	649827.351091	39.550746
2710.019520	651067.266582	39.555764
2712.708932	652313.028072	39.560781
2715.646068	653543.246281	39.565799
2718.201765	654793.301859	39.570816
2721.177388	656040.340180	39.575834
2723.525038	657296.039798	39.580852
2726.488548	658554.663975	39.585869
2729.121944	659810.790143	39.590887
2731.740916	661072.481875	39.595904
2734.883431	662333.823421	39.600922
2737.682259	663612.726491	39.605940
2740.070880	664884.410566	39.610957
2742.869779	666166.158745	39.615975
2745.992768	667433.850050	39.620992
2748.616602	668713.742434	39.626010
2751.710756	669990.151553	39.631028
2754.505464	671271.212218	39.636045
2757.348378	672540.007223	39.641063
2759.545746	673834.442590	39.646080
2762.664842	675111.296555	39.651098
2765.688376	676405.388750	39.656116
2768.773280	677680.752842	39.661133
2771.558549	678962.301781	39.666151
2774.034024	680254.207662	39.671168
2777.147313	681533.457075	39.676186
2779.999276	682815.501824	39.681204
2782.667175	684099.582413	39.686221
2785.825342	685383.053621	39.691239
2787.998556	686670.180018	39.696256
2791.111693	687961.088857	39.701274
2793.742822	689244.000251	39.706292
2796.344872	690537.800778	39.711309
2799.125299	691821.857655	39.716327
2802.231983	693121.205680	39.721344
2804.905693	694412.200556	39.726362
2807.530590	695700.982041	39.731380
2810.415502	697001.584051	39.736397
2813.435201	698291.509289	39.741415
2816.086625	699585.024279	39.746432
2819.063281	700839.281798	39.751450
2821.729203	702101.291092	39.756468
2824.624405	703356.488443	39.761485
2827.334069	704604.349985	39.766503
2830.021067	705863.281449	39.771520
2832.799114	707111.760146	39.776538
2835.245575	708373.237188	39.781556
2838.140564	709641.437004	39.786573
2841.149427	710906.656920	39.791591
2843.690285	712179.092888	39.796608
2846.363217	713460.077595	39.801626
2848.940503	714746.971527	39.806644
2851.528913	716048.264935	39.811661
2854.329653	717342.197320	39.816679
2856.968924	718665.637501	39.821696
2859.936852	719978.031395	39.826714
2863.223003	721311.776689	39.831732
2865.739179	722638.759505	39.836749
2868.768032	723961.292212	39.841767
2871.509699	725293.249267	39.846784
2874.195556	726642.494532	39.851802
2877.416015	727980.262182	39.856820
2880.344801	729332.778807	39.861837
2883.300858	730685.164926	39.866855
2885.988722	732050.951413	39.871872
2888.800072	733408.981146	39.876890
2891.781000	734777.270098	39.881908
2894.314424	736153.297746	39.886925
2897.575248	737514.360149	39.891943
2900.260831	738896.947973	39.896960
2902.897151	740284.780000	39.901978
2905.906918	741670.334374	39.906996
2908.933034	743083.360700	39.912013
2911.845763	744469.869560	39.917031
2914.766121	745885.368342	39.922048
2918.017688	747291.683672	39.927066
2921.125042	748687.173034	39.932084
2923.988415	750093.391170	39.937101
2927.536107	751496.235981	39.942119
2930.192160	752902.076101	39.947136
2932.878216	754315.337229	39.952154
2936.128260	755726.669365	39.957172
2939.006106	757140.116150	39.962189
2941.663342	758543.443741	39.967207
2944.843426	759964.831142	39.972224
2947.602327	761388.776478	39.977242
2950.949150	762816.685231	39.982260
2953.549383	764240.216176	39.987277
2956.646524	765664.968531	39.992295
2959.656753	767101.164880	39.997312
2961.957893	768541.379442	40.002330
2965.595664	769970.282187	40.007348
2968.679676	771410.056007	40.012365
2971.317843	772845.299126	40.017383
2974.334734	774281.574947	40.022400
2976.895527	775724.765083	40.027418
2980.015861	777172.193081	40.032436
2983.326971	778634.175567	40.037453
2986.562710	780067.361499	40.042471
2989.451194	781518.623274	40.047488
2992.399860	782967.522581	40.052506
2995.417946	784413.714973	40.057524
2998.325085	785868.902040	40.062541
3001.450810	787313.264392	40.067559
3004.397124	788774.323722	40.072576
3007.108365	790217.134764	40.077594
3009.961407	791674.474706	40.082612
3012.992849	793123.400887	40.087629
3015.809091	794552.227509	40.092647
3018.625485	795967.443226	40.097664
3021.384707	797390.900393	40.102682
3024.258221	798815.662986	40.107700
3027.089711	800250.906494	40.112717
3030.303701	801688.186701	40.117735
3032.925545	803127.808717	40.122752
3035.752773	804566.753100	40.127770
3038.822214	806022.371787	40.132788
3041.728421	807499.364158	40.137805
3044.255491	808971.504350	40.142823
3047.462186	810447.708956	40.147840
3050.111722	811936.043661	40.152858
3053.393182	813425.020417	40.157876
3056.296053	814919.833992	40.162893
3059.008235	816422.157195	40.167911
3062.213813	817934.165193	40.172928
3065.315769	819467.416559	40.177946
3068.418263	820984.701296	40.182964
3070.840636	822527.016900	40.187981
3074.249809	824073.734552	40.192999
3077.333061	825620.873261	40.198016
3080.194668	827177.529204	40.203034
3083.670168	828735.369759	40.208052
3086.766360	830310.438921	40.213069
3090.106448	831870.521901	40.218087
3093.287434	833444.522531	40.223104
3096.025733	835009.789382	40.228122
3099.263103	836588.366735	40.233140
3101.899550	838188.842766	40.238157
3105.357754	839773.555268	40.243175
3108.475460	841362.792534	40.248192
3111.735611	842972.758940	40.253210
3114.599967	844573.435923	40.258228
3117.528614	846189.344070	40.263245
3120.672203	847805.578097	40.268263
3123.961490	849420.399002	40.273280
3126.977440	851045.238585	40.278298
3130.313142	852663.192237	40.283316
3133.136097	854307.501878	40.288333
3136.189617	855952.888142	40.293351
3139.883114	857572.989166	40.298368
3142.758356	859217.820874	40.303386
3146.295943	860848.719295	40.308404
3149.322782	862499.622474	40.313421
3152.380654	864142.996768	40.318439
3155.638013	865793.933332	40.323456
3158.478075	867456.594093	40.328474
3161.824192	869111.255169	40.333492
3165.113653	870765.371521	40.338509
3168.387237	872423.193549	40.343527
3171.722394	874086.445274	40.348544
3174.819440	875739.403539	40.353562
3178.220763	877399.971904	40.358580
3181.257743	879062.548803	40.363597
3184.449870	880723.469443	40.368615
3187.585789	882384.120971	40.373632
3190.372075	884059.907879	40.378650
3193.743235	885727.197155	40.383668
3196.943419	887408.997174	40.388685
3200.022888	889088.686473	40.393703
3203.177485	890766.618765	40.398720
3206.102387	892446.798407	40.403738
3209.480222	894119.660036	40.408756
3212.691454	895802.660804	40.413773
3215.940982	897495.467074	40.418791
3219.105271	899177.954851	40.423808
3222.125989	900857.460349	40.428826
3225.362529	902502.346518	40.433844
3228.413593	904153.710153	40.438861
3231.547947	905802.358643	40.443879
3234.972199	907445.757634	40.448896
3237.803713	909088.094329	40.453914
3240.808795	910728.280424	40.458932
3243.550047	912401.178369	40.463949
3246.943035	914071.345941	40.468967
3250.178158	915741.606445	40.473984
3253.222515	917421.757165	40.479002
3256.305546	919101.382707	40.484020
3259.325246	920803.528267	40.489037
3262.395176	922501.963987	40.494055
3265.700231	924204.332697	40.499072
3268.926190	925942.699628	40.504090
3272.077669	927658.951443	40.509108
3275.275975	929401.085155	40.514125
3278.320378	931136.927043	40.519143
3281.446630	932882.048083	40.524160
3284.525765	934646.603313	40.529178
3288.158627	936407.127055	40.534196
3291.358851	938190.372644	40.539213
3294.245060	939956.903381	40.544231
3297.830900	941740.306388	40.549248
3300.711061	943527.990367	40.554266
3304.125233	945328.245028	40.559284
3307.525513	947153.939185	40.564301
3310.648363	948946.197424	40.569319
3314.062099	950765.163626	40.574336
3317.273539	952583.705636	40.579354
3320.636742	954468.151257	40.584372
3323.830944	956352.839940	40.589389
3327.084940	958235.338920	40.594407
3330.473799	960128.929395	40.599424
3333.874139	962022.872545	40.604442
3337.602163	963922.389463	40.609460
3340.552485	965829.511108	40.614477
3343.886088	967735.155739	40.619495
3347.283705	969642.986871	40.624512
3350.623048	971570.871893	40.629530
3353.761851	973486.147717	40.634548
3357.529589	975410.231924	40.639565
3360.464633	977332.246984	40.644583
3364.266331	979264.188117	40.649600
3367.640171	981199.246399	40.654618
3371.046400	983126.439479	40.659636
3374.097697	985071.625979	40.664653
3377.701719	986996.893148	40.669671
3381.148831	988928.439121	40.674688
3383.747642	990875.800241	40.679706
3387.694725	992830.434644	40.684724
3390.808196	994784.144440	40.689741
3393.856107	996739.910923	40.694759
3397.586203	998712.363825	40.699776
3401.117810	1000681.735778	40.704794
3404.807178	1002635.456101	40.709812
3408.340956	1004611.994708	40.714829
3411.432854	1006568.040534	40.719847
3415.327953	1008537.424244	40.724864
3418.586234	1010511.843072	40.729882
3421.968448	1012466.471055	40.734900
3425.204546	1014442.225385	40.739917
3428.828074	1016411.221060	40.744935
3432.745514	1018384.507977	40.749952
3435.721156	1020361.027079	40.754970
3439.331457	1022339.837810	40.759988
3443.251567	1024316.158395	40.765005
3446.618405	1026275.863604	40.770010
3450.412709	1028176.184855	40.775015
3453.474295	1030015.005222	40.780020
3457.095203	1031776.110737	40.785024
3460.529839	1033473.528890	40.790029
3463.520900	1035104.265424	40.795034
3466.988349	1036651.599687	40.800039
3469.842331	1038113.460838	40.805044
3472.603686	1039502.680774	40.810048
3475.583435	1040807.863915	40.815053
3478.280054	1042045.666443	40.820058
3480.771439	1043204.919934	40.825063
3482.996466	1044293.889224	40.830068
3485.756988	1045310.263582	40.835072
3488.324058	1046245.903624	40.840077
3489.968989	1047113.127742	40.845082
3492.648645	1047913.285798	40.850087
3494.398701	1048655.315396	40.855092
3496.552741	1049319.730407	40.860096
3498.096877	1049943.661887	40.865101
3499.883324	1050508.083172	40.870106
3501.477604	1050999.874500	40.875111
3502.914659	1051463.495648	40.880116
3504.297403	1051857.097070	40.885120
3505.914404	1052209.276790	40.890125
3506.771060	1052525.893785	40.895130
3508.224389	1052786.778185	40.900135
3509.189026	1053014.670797	40.905140
3510.495870	1053207.896741	40.910144
3511.373155	1053345.865312	40.915149
3512.328434	1053467.337132	40.920154
3513.426131	1053551.196472	40.925159
3514.339736	1053600.486452	40.930164
3514.985468	1053631.316310	40.935168
3515.976448	1053612.745615	40.940173
3516.691021	1053586.028527	40.945178
3517.522122	1053518.428795	40.950183
3518.065516	1053441.816158	40.955188
3518.712639	1053327.693897	40.960192
3518.902263	1053198.319972	40.965197
3519.369753	1053051.355335	40.970202
3520.059175	1052884.590893	40.975207
3520.417118	1052711.707051	40.980212
3521.033382	1052498.868309	40.985216
3521.304158	1052285.114301	40.990221
3521.770163	1052059.655280	40.995226
3522.174915	1051811.927427	41.000231
3522.689881	1051564.266718	41.005236
3522.886045	1051278.852790	41.010240
3523.361165	1050998.392008	41.015245
3523.469053	1050711.709856	41.020250
3523.894793	1050402.106483	41.025255
3523.823793	1050096.810771	41.030260
3524.112175	1049773.018694	41.035264
3524.317973	1049448.160334	41.040269
3524.438547	1049104.006322	41.045274
3524.843171	1048758.723044	41.050279
3524.791939	1048414.650883	41.055284
3525.003556	1048052.859756	41.060288
3525.253789	1047680.618990	41.065293
3525.451277	1047316.370074	41.070298
3525.687755	1046928.353994	41.075303
3525.646069	1046545.953405	41.080308
3525.396780	1046164.911652	41.085312
3525.650529	1045774.592240	41.090317
3525.659930	1045379.845735	41.095322
3526.007777	1044979.030786	41.100327
3526.072954	1044573.985987	41.105332
3526.301867	1044166.374581	41.110336
3526.465817	1043755.847503	41.115341
3526.112442	1043342.575179	41.120346
3526.312585	1042926.573710	41.125351
3526.529356	1042509.572609	41.130356
3526.216529	1042090.116431	41.135360
3526.380707	1041649.494871	41.140365
3526.323669	1041235.437151	41.145370
3526.349174	1040800.276634	41.150375
3526.230980	1040375.249228	41.155380
3526.514611	1039952.731621	41.160384
3526.610482	1039512.627931	41.165389
3526.083666	1039071.529025	41.170394
3526.364822	1038634.127401	41.175399
3526.730990	1038198.030344	41.180404
3526.549476	1037758.123253	41.185408
3526.359590	1037315.862911	41.190413
3525.968272	1036884.910488	41.195418
3526.477125	1036442.175536	41.200423
3526.172483	1036008.047307	41.205428
3526.169663	1035555.657947	41.210432
3526.187112	1035110.480725	41.215437
3526.043673	1034672.063703	41.220442
3526.221676	1034229.787419	41.225447
3526.072889	1033791.301901	41.230452
3525.884520	1033347.081449	41.235456
3526.026610	1032910.509929	41.240461
3525.762957	1032465.941388	41.245466
3525.987530	1032018.160922	41.250471
3525.935047	1031583.162201	41.255476
3525.954470	1031129.441882	41.260480
3526.211127	1030690.258386	41.265485
3525.494100	1030242.200037	41.270490
3525.937859	1029797.398865	41.275495
3525.768794	1029359.245364	41.280500
3525.772599	1028916.769582	41.285504
3525.892991	1028453.908945	41.290509
3525.593424	1028004.924410	41.295514
3525.825731	1027557.849530	41.300519
3525.637126	1027116.618335	41.305524
3525.573919	1026671.070517	41.310528
3525.609051	1026213.170868	41.315533
3525.463890	1025779.671853	41.320538
3525.708550	1025327.282907	41.325543
3525.453925	1024890.633237	41.330548
3525.188402	1024432.249704	41.335552
3525.062800	1023974.677553	41.340557
3524.937296	1023547.687619	41.345562
3525.020949	1023091.462211	41.350567
3525.043425	1022661.570022	41.355572
3525.154973	1022215.056759	41.360576
3524.866731	1021767.895242	41.365581
3524.794678	1021323.667409	41.370586
3524.767048	1020884.050310	41.375591
3524.980085	1020454.732827	41.380596
3524.786942	1020009.935995	41.385600
3524.950049	1019574.547864	41.390605
3524.772590	1019134.430302	41.395610
3524.645542	1018683.310967	41.400615
3524.597702	1018246.205734	41.405620
3524.395164	1017807.151982	41.410624
3524.344046	1017369.784994	41.415629
3524.368953	1016930.334137	41.420634
3523.922777	1016491.702626	41.425639
3524.037722	1016066.528168	41.430644
3523.896320	1015636.512030	41.435648
3523.935954	1015194.691075	41.440653
3523.864287	1014773.428166	41.445658
3524.151112	1014335.283815	41.450663
3523.690007	1013917.320792	41.455668
3523.204261	1013495.836166	41.460672
3523.671321	1013064.746341	41.465677
3523.533555	1012648.188922	41.470682
3523.362635	1012213.546759	41.475687
3523.057450	1011799.284273	41.480692
3523.183442	1011370.451177	41.485696
3523.224240	1010953.350380	41.490701
3523.002061	1010525.772766	41.495706
3523.071646	1010112.781200	41.500711
3523.003434	1009695.119471	41.505716
3522.824838	1009280.942130	41.510720
3522.891898	1008854.452800	41.515725
3522.582927	1008456.071924	41.520730
3522.760843	1008018.522161	41.525735
3522.582145	1007619.866367	41.530740
3522.641073	1007193.932896	41.535744
3522.651492	1006792.466390	41.540749
3522.398032	1006390.723187	41.545754
3522.534157	1005979.555902	41.550759
3522.316604	1005556.751938	41.555764
3522.154444	1005146.447941	41.560768
3521.937976	1004747.498055	41.565773
3521.976798	1004353.339358	41.570778
3521.801130	1003939.644059	41.575783
3521.862994	1003534.436707	41.580788
3521.881913	1003139.710347	41.585792
3521.911842	1002734.839889	41.590797
3521.579398	1002332.820758	41.595802
3521.676210	1001928.270536	41.600807
3522.035076	1001539.504423	41.605812
3521.670105	1001136.432756	41.610816
3521.379431	1000723.104514	41.615821
3521.445457	1000329.244263	41.620826
3521.237666	999931.217576	41.625831
3521.110130	999553.779740	41.630836
3521.066410	999154.600951	41.635840
3520.961361	998758.129210	41.640845
3520.844552	998379.151372	41.645850
3521.231844	997981.960171	41.650855
3520.897832	997595.081193	41.655860
3520.730257	997200.846964	41.660864
3521.023127	996813.032473	41.665869
3520.683111	996426.756175	41.670874
3520.800090	996047.875887	41.675879
3520.457720	995657.652664	41.680884
3520.276845	995278.672637	41.685888
3520.374201	994900.108394	41.690893
3520.233592	994519.610116	41.695898
3520.285969	994134.671305	41.700903
3520.448314	993765.176627	41.705908
3520.236320	993384.321709	41.710912
3520.069459	993003.726058	41.715917
3520.030926	992634.288249	41.720922
3519.988842	992247.678078	41.725927
3519.943741	991878.387028	41.730932
3519.892323	991506.246954	41.735936
3520.021850	991129.277328	41.740941
3519.476155	990765.064059	41.745946
3519.473445	990399.860759	41.750951
3519.470299	990035.316383	41.755956
3519.593362	989671.410198	41.760960
3519.771252	989299.282726	41.765965
3519.647715	988932.152747	41.770970
3519.421000	988558.581035	41.775975
3519.197668	988207.995768	41.780980
3518.515812	987835.036529	41.785984
3519.085721	987473.938977	41.790989
3518.768309	987129.934039	41.795994
3518.734382	986775.425799	41.800999
3518.742384	986425.375269	41.806004
3518.664944	986081.560030	41.811008
3518.601653	985719.577607	41.816013
3518.268717	985375.566722	41.821018
3518.788661	985023.492120	41.826023
3518.575848	984663.515979	41.831028
3518.531553	984312.953925	41.836032
3518.782166	983961.053191	41.841037
3518.269469	983612.574370	41.846042
3518.199974	983260.975897	41.851047
3518.423519	982918.383989	41.856052
3518.019751	982583.975869	41.861056
3518.086663	982230.632135	41.866061
3518.281859	981895.694545	41.871066
3518.095970	981548.207047	41.876071
3518.141822	981208.470310	41.881076
3517.912999	980865.243838	41.886080
3518.085818	980517.146291	41.891085
3517.685030	980178.886405	41.896090
3517.564036	979844.856958	41.901095
3517.436634	979513.348059	41.906100
3517.387536	979190.010524	41.911104
3517.493860	978855.397443	41.916109
3517.384033	978522.753813	41.921114
3517.369777	978184.214394	41.926119
3517.466996	977859.800680	41.931124
3517.408951	977530.411984	41.936128
3517.270393	977195.546658	41.941133
3517.279565	976871.189030	41.946138
3517.268679	976534.407635	41.951143
3517.237733	976211.680209	41.956148
3516.929556	975887.709917	41.961152
3517.274450	975558.336654	41.966157
3516.603830	975237.711824	41.971162
3516.682066	974911.668023	41.976167
3516.607272	974594.916098	41.981172
3516.486225	974273.071533	41.986176
3516.778266	973946.644304	41.991181
3516.320844	973630.488541	41.996186
3516.259793	973322.657470	42.001191
3516.386894	973016.049816	42.006196
3516.357495	972698.501116	42.011200
3516.335388	972386.898009	42.016205
3516.280691	972084.474853	42.021210
3516.230839	971758.370358	42.026215
3516.214878	971462.948729	42.031220
3516.073594	971144.647788	42.036224
3516.326261	970837.022661	42.041229
3515.816223	970526.083372	42.046234
3515.909220	970211.995634	42.051239
3515.942686	969911.301753	42.056244
3515.846110	969617.754703	42.061248
3515.869681	969307.541844	42.066253
3515.417079	969006.000112	42.071258
3515.373871	968702.516127	42.076263
3515.453333	968412.204945	42.081268
3515.300881	968109.196805	42.086272
3515.557740	967806.985936	42.091277
3515.619498	967516.045222	42.096282
3515.352982	967213.302166	42.101287
3515.162738	966930.300363	42.106292
3515.350862	966626.668524	42.111296
3515.227238	966329.336336	42.116301
3515.175060	966041.080318	42.121306
3514.943876	965744.616553	42.126311
3515.266116	965463.611650	42.131316
3514.889022	965174.484630	42.136320
3514.788072	964893.129954	42.141325
3515.032109	964602.501171	42.146330
3514.725128	964307.150655	42.151335
3514.739148	964029.063854	42.156340
3514.418197	963744.751637	42.161344
3514.785798	963457.765774	42.166349
3514.621986	963185.053564	42.171354
3514.345346	962892.759287	42.176359
3514.403015	962622.726221	42.181364
3513.935556	962344.049616	42.186368
3514.151943	962065.246855	42.191373
3514.076977	961807.931271	42.196378
3514.220316	961528.037002	42.201383
3514.129785	961260.315523	42.206388
3513.884892	960988.884122	42.211392
3514.049117	960708.064818	42.216397
3513.980404	960449.119864	42.221402
3513.987045	960177.314835	42.226407
3513.984359	959917.355252	42.231412
3513.552973	959632.074103	42.236416
3513.422016	959374.953011	42.241421
3513.364369	959119.180411	42.246426
3513.712621	958847.452383	42.251431
3513.291030	958594.068621	42.256436
3513.483487	958333.221338	42.261440
3513.471300	958073.278158	42.266445
3513.414706	957822.446911	42.271450
3513.263311	957554.465220	42.276455
3513.517322	957303.952376	42.281460
3513.405634	957035.940055	42.286464
3513.465860	956774.455836	42.291469
3513.090972	956526.463911	42.296474
3513.256094	956260.625056	42.301479
3512.984269	956013.672680	42.306484
3513.095758	955758.507605	42.311488
3513.117258	955502.757692	42.316493
3512.716781	955259.226484	42.321498
3512.912269	955003.916155	42.326503
3512.780309	954755.513889	42.331508
3512.821704	954504.914589	42.336512
3512.853573	954253.717474	42.341517
3512.679652	954017.256807	42.346522
3512.741111	953761.423196	42.351527
3512.303975	953512.331081	42.356532
3512.379505	953274.719847	42.361536
3512.833122	953039.096792	42.366541
3512.315003	952799.307367	42.371546
3512.538333	952547.564977	42.376551
3512.648728	952318.242193	42.381556
3512.372893	952086.199443	42.386560
3512.360880	951842.339636	42.391565
3512.047122	951606.647169	42.396570
3511.583179	951376.611487	42.401575
3512.038446	951160.378494	42.406580
3512.080618	950927.561054	42.411584
3512.359263	950705.407486	42.416589
3511.917049	950488.528638	42.421594
3511.979629	950250.606993	42.426599
3511.993063	950026.362969	42.431604
3511.561616	949800.364617	42.436608
3511.783910	949567.838220	42.441613
3511.441091	949344.484074	42.446618
3511.709104	949128.961425	42.451623
3511.392387	948910.176913	42.456628
3511.209473	948701.408804	42.461632
3511.677502	948485.443362	42.466637
3511.112812	948269.830361	42.471642
3511.158842	948055.351846	42.476647
3511.670486	947843.563229	42.481652
3511.601475	947632.148676	42.486656
3511.646561	947414.197857	42.491661
3511.530840	947197.412938	42.496666
3511.572884	946975.902342	42.501671
3511.519220	946758.227147	42.506676
3511.244522	946548.333558	42.511680
3511.210697	946328.052092	42.516685
3510.912274	946124.368043	42.521690
3511.335657	945908.397396	42.526695
3511.236524	945701.121204	42.531700
3510.739135	945486.816562	42.536704
3511.041509	945275.435477	42.541709
3510.934428	945069.092752	42.546714
3510.846703	944862.834350	42.551719
3510.770045	944665.951182	42.556724
3510.601308	944467.734869	42.561728
3510.769883	944261.697548	42.566733
3510.547944	944053.896535	42.571738
3510.370350	943848.187099	42.576743
3510.527777	943653.812956	42.581748
3510.016182	943465.289164	42.586752
3510.221773	943260.355340	42.591757
3510.103257	943073.955804	42.596762
3510.149510	942883.977768	42.601767
3509.642653	942699.065735	42.606772
3510.129421	942515.803762	42.611776
3510.146800	942315.653988	42.616781
3510.028967	942122.992368	42.621786
3509.851080	941934.070423	42.626791
3509.980316	941749.403007	42.631796
3510.027304	941561.580328	42.636800
3510.068363	941369.343691	42.641805
3510.058723	941183.337424	42.646810
3509.678315	940994.414662	42.651815
3509.877227	940807.114708	42.656820
3509.448813	940629.495656	42.661824
3509.860984	940434.096335	42.666829
3509.569160	940259.317538	42.671834
3509.671896	940076.895487	42.676839
3509.373012	939901.051443	42.681844
3509.415897	939721.406637	42.686848
3509.376168	939538.509911	42.691853
3509.189985	939364.450590	42.696858
3509.415101	939178.621628	42.701863
3509.252108	939012.887403	42.706868
3509.104876	938853.664859	42.711872
3509.121029	938667.468625	42.716877
3509.193186	938501.967080	42.721882
3509.028775	938328.253147	42.726887
3508.990958	938154.224918	42.731892
3509.308001	937992.502434	42.736896
3509.248388	937807.055163	42.741901
3508.782200	937638.642241	42.746906
3508.844340	937462.177075	42.751911
3508.923936	937299.129670	42.756916
3508.880695	937140.509147	42.761920
3508.758470	936961.372086	42.766925
3508.754834	936800.912463	42.771930
3508.631088	936635.192327	42.776935
3508.924548	936473.906424	42.781940
3508.997470	936314.762182	42.786945
3509.099025	936139.684830	42.791949
3508.777070	935986.063409	42.796954
3508.961320	935801.368336	42.801959
3508.589016	935639.399024	42.806964
3508.302500	935477.506519	42.811969
3508.565132	935321.754673	42.816973
3508.465674	935164.330892	42.821978
3508.484947	934999.878779	42.826983
3508.483428	934836.864186	42.831988
3508.393566	934684.509759	42.836993
3508.558547	934522.801335	42.841997
3508.053972	934370.410182	42.847002
3508.183615	934212.248470	42.852007
3508.583686	934060.658924	42.857012
3508.134203	933900.280140	42.862017
3508.334278	933746.507289	42.867021
3508.223306	933602.282387	42.872026
3508.079601	933441.647329	42.877031
3508.238868	933288.923582	42.882036
3507.917404	933135.218834	42.887041
3507.922102	932985.007238	42.892045
3508.073190	932842.062143	42.897050
3508.053748	932691.174271	42.902055
3508.210545	932541.212963	42.907060
3507.758879	932384.148122	42.912065
3508.114527	932237.121233	42.917069
3508.025490	932084.499574	42.922074
3507.845872	931941.680615	42.927079
3507.897598	931804.195924	42.932084
3507.288807	931660.384027	42.937089
3507.684673	931510.258102	42.942093
3507.618019	931376.334154	42.947098
3507.454439	931231.765181	42.952103
3507.718086	931090.482480	42.957108
3507.211733	930958.444729	42.962113
3507.302681	930820.351922	42.967117
3507.431555	930682.633371	42.972122
3507.465231	930537.532843	42.977127
3507.556253	930404.230548	42.982132
3507.265197	930270.795787	42.987137
3507.696526	930122.161242	42.992141
3507.415476	929994.479962	42.997146
3507.183626	929855.646937	43.002151
3507.257767	929712.630067	43.007156
3507.297040	929589.112118	43.012161
3507.424639	929444.830660	43.017165
3507.281324	929312.692141	43.022170
3507.187679	929169.015944	43.027175
3507.491292	929034.491641	43.032180
3506.909219	928901.838870	43.037185
3507.351665	928766.420411	43.042189
3506.944854	928642.377613	43.047194
3507.107045	928504.501068	43.052199
3507.088679	928361.463116	43.057204
3507.072137	928246.377036	43.062209
3507.051582	928108.616423	43.067213
3506.879033	927978.947457	43.072218
3506.845162	927846.658446	43.077223
3507.012646	927718.080025	43.082228
3506.424435	927597.021186	43.087233
3506.747751	927464.663857	43.092237
3506.507909	927353.630764	43.097242
3506.412986	927235.749332	43.102247
3506.500079	927114.280024	43.107252
3506.679604	926996.540277	43.112257
3507.032341	926871.562410	43.117261
3506.907215	926752.714362	43.122266
3506.786632	926621.754617	43.127271
3506.699115	926490.690116	43.132276
3506.452335	926382.328775	43.137281
3506.508826	926253.637290	43.142285
3506.451360	926133.899398	43.147290
3506.791408	926009.191793	43.152295
3506.535386	925886.405593	43.157300
3506.124540	925771.427242	43.162305
3506.532053	925649.391309	43.167309
3506.129432	925547.766800	43.172314
3506.043354	925424.653658	43.177319
3506.369607	925311.370262	43.182324
3506.175421	925202.399636	43.187329
3506.391095	925082.497114	43.192333
3505.749136	924959.560991	43.197338
3505.927890	924853.117270	43.202343
3506.419618	924750.849657	43.207348
3506.298483	924634.453336	43.212353
3506.436529	924520.415178	43.217357
3506.360778	924414.004677	43.222362
3506.207386	924289.626783	43.227367
3506.209033	924180.314711	43.232372
3505.889373	924067.688324	43.237377
3506.160520	923944.770799	43.242381
3506.204886	923847.847715	43.247386
3506.054089	923731.629003	43.252391
3506.083631	923622.204833	43.257396
3506.550636	923508.379457	43.262401
3506.107640	923394.413125	43.267405
3506.084226	923292.683418	43.272410
3506.454179	923173.962928	43.277415
3506.492231	923056.544601	43.282420
3505.893579	922947.402520	43.287425
3505.872800	922838.740014	43.292429
3506.167019	922742.621347	43.297434
3506.021011	922621.761839	43.302439
3506.027414	922509.818459	43.307444
3506.036696	922402.007734	43.312449
3506.142780	922278.887017	43.317453
3506.162694	922177.513808	43.322458
3505.841996	922070.712593	43.327463
3506.202854	921956.294843	43.332468
3506.195343	921853.669709	43.337473
3506.008587	921727.891530	43.342477
3506.133625	921624.085968	43.347482
3505.989682	921516.763728	43.352487
3506.273737	921403.693569	43.357492
3505.984642	921294.755578	43.362497
3506.010349	921181.338554	43.367501
3505.776206	921075.080540	43.372506
3505.779113	920968.107990	43.377511
3505.909781	920861.978082	43.382516
3505.602939	920762.940959	43.387521
3505.925821	920658.026015	43.392525
3505.901315	920554.032124	43.397530
3505.443709	920444.238887	43.402535
3505.836738	920346.425749	43.407540
3505.673673	920248.798670	43.412545
3505.748434	920131.310648	43.417549
3505.885464	920032.860525	43.422554
3505.586595	919941.023195	43.427559
3505.901811	919836.286025	43.432564
3505.453433	919735.713905	43.437569
3505.506800	919631.689464	43.442573
3505.633837	919534.001703	43.447578
3505.250564	919430.526456	43.452583
3505.429336	919325.032076	43.457588
3505.493765	919243.130773	43.462593
3505.635586	919147.550664	43.467597
3505.215323	919043.592967	43.472602
3505.441479	918946.359457	43.477607
3505.399029	918856.482429	43.482612
3505.335899	918754.481317	43.487617
3505.257489	918658.640164	43.492621
3505.206316	918567.604910	43.497626
3505.433084	918472.383883	43.502631
3505.265041	918378.381170	43.507636
3504.848783	918278.161692	43.512641
3505.182748	918182.917933	43.517645
3505.197611	918096.387572	43.522650
3505.065254	918010.072590	43.527655
3505.069379	917918.247332	43.532660
3505.084137	917838.739354	43.537665
3505.298429	917731.379331	43.542669
3505.003209	917648.069377	43.547674
3504.665858	917551.481289	43.552679
3504.855565	917468.955037	43.557684
3504.517353	917384.781782	43.562689
3505.011587	917302.876682	43.567693
3504.786904	917227.057238	43.572698
3504.858721	917137.229216	43.577703
3504.868537	917047.891268	43.582708
3504.803242	916962.896378	43.587713
3504.573769	916874.076350	43.592717
3504.645164	916790.115231	43.597722
3505.121089	916715.039692	43.602727
3505.119037	916623.097327	43.607732
3505.327977	916537.569245	43.612737
3505.224930	916442.463315	43.617741
3504.832780	916361.267773	43.622746
3504.789679	916268.459664	43.627751
3505.056243	916185.805038	43.632756
3504.689144	916101.616705	43.637761
3504.647320	916014.388598	43.642765
3504.184112	915936.953620	43.647770
3504.486019	915858.910044	43.652775
3504.906777	915781.808682	43.657780
3504.334866	915696.877517	43.662785
3504.743672	915612.072341	43.667789
3504.220811	915536.471085	43.672794
3504.353732	915457.968147	43.677799
3504.446281	915381.492987	43.682804
3504.175594	915302.187622	43.687809
3504.644353	915223.914892	43.692813
3504.463365	915144.303556	43.697818
3504.077288	915059.139245	43.702823
3504.292228	914985.431182	43.707828
3504.023062	914919.506365	43.712833
3504.163323	914839.356132	43.717837
3504.321537	914768.928948	43.722842
3504.345143	914698.234105	43.727847
3504.439144	914621.844392	43.732852
3504.305012	914553.581446	43.737857
3504.584180	914468.490963	43.742861
3504.377664	914387.042841	43.747866
3503.923805	914323.549149	43.752871
3504.180666	914250.691134	43.757876
3504.411174	914189.009489	43.762881
3504.072335	914108.734851	43.767885
3504.038552	914028.601421	43.772890
3503.988675	913962.725266	43.777895
3504.368185	913888.975332	43.782900
3504.058992	913829.786660	43.787905
3504.193044	913743.360270	43.792909
3504.154626	913685.281347	43.797914
3504.196109	913611.679700	43.802919
3504.612584	913526.359311	43.807924
3504.290839	913463.315526	43.812929
3504.216586	913387.321645	43.817933
3503.886641	913312.524845	43.822938
3503.839482	913248.084667	43.827943
3503.955682	913182.171772	43.832948
3503.704645	913119.497729	43.837953
3503.940329	913046.049174	43.842957
3503.986702	912988.237917	43.847962
3503.679336	912918.441696	43.852967
3503.711148	912850.997268	43.857972
3503.647585	912788.866615	43.862977
3503.675699	912726.045745	43.867981
3503.778512	912671.593914	43.872986
3503.382711	912615.874837	43.877991
3504.118751	912537.134335	43.882996
3503.849939	912492.569425	43.888001
3503.802862	912421.471471	43.893005
3503.962087	912364.213154	43.898010
3503.620092	912287.091938	43.903015
3503.631873	912236.601235	43.908020
3503.801147	912179.146628	43.913025
3503.876438	912107.253617	43.918029
3504.187070	912042.451282	43.923034
3503.825951	911976.987990	43.928039
3503.860155	911902.979209	43.933044
3503.206925	911844.885743	43.938049
3503.349014	911780.589890	43.943053
3503.500472	911734.118727	43.948058
3503.356936	911674.879513	43.953063
3503.641069	911616.243751	43.958068
3503.314488	911564.453525	43.963073
3503.672706	911509.562653	43.968077
3503.556946	911455.616621	43.973082
3503.098513	911383.705717	43.978087
3503.724921	911332.527251	43.983092
3503.483949	911283.033126	43.988097
3503.585451	911214.882561	43.993101
3503.662316	911153.674006	43.998106
3503.582140	911095.478210	44.003111
3503.844817	911040.598409	44.008116
3503.479389	910984.279539	44.013121
3503.635267	910923.922791	44.018125
3503.356157	910856.408753	44.023130
3503.241808	910810.455477	44.028135
3503.653172	910749.861977	44.033140
3503.307766	910693.922355	44.038145
3503.610995	910637.393399	44.043149
3503.451139	910578.048692	44.048154
3503.386607	910527.844036	44.053159
3503.536336	910467.001386	44.058164
3503.182538	910422.144545	44.063169
3503.367038	910363.511877	44.068173
3503.664464	910310.546807	44.073178
3503.183876	910252.600852	44.078183
3503.663418	910193.917776	44.083188
3503.689305	910144.273067	44.088193
3503.848676	910085.159635	44.093197
3503.492628	910024.106255	44.098202
3503.134243	909971.824331	44.103207
3502.997102	909906.492303	44.108212
3503.202100	909869.732381	44.113217
3503.344834	909819.487134	44.118221
3503.358301	909758.273541	44.123226
3503.455126	909706.685282	44.128231
3503.642166	909649.104983	44.133236
3503.315134	909607.803846	44.138241
3503.465431	909539.238950	44.143245
3503.351895	909490.093331	44.148250
3503.201111	909434.976485	44.153255
3503.678661	909384.864933	44.158260
3503.414150	909331.501044	44.163265
3503.361816	909270.003672	44.168269
3503.547869	909218.492562	44.173274
3503.011751	909171.823877	44.178279
3503.182405	909100.840023	44.183284
3503.401429	909062.433491	44.188289
3503.269591	909000.174947	44.193293
3503.261102	908951.971335	44.198298
3503.205377	908905.414077	44.203303
3503.455316	908850.225383	44.208308
3503.296207	908798.574404	44.213313
3503.422362	908744.369180	44.218317
3503.484006	908689.884809	44.223322
3503.250724	908647.693311	44.228327
3503.413732	908588.948949	44.233332
3503.168719	908544.926680	44.238337
3503.449025	908475.748682	44.243341
3503.337125	908429.678771	44.248346
3503.338836	908377.129587	44.253351
3503.548127	908318.181888	44.258356
3503.123793	908273.029940	44.263361
3503.255877	908212.454656	44.268365
3503.155816	908171.973204	44.273370
3502.996231	908125.619347	44.278375
3503.215125	908067.149521	44.283380
3502.805654	908025.946568	44.288385
3502.984929	907967.385790	44.293389
3503.167558	907929.555969	44.298394
3503.297557	907889.130979	44.303399
3503.661551	907830.056175	44.308404
3503.496695	907780.903830	44.313409
3503.243670	907725.497507	44.318413
3503.395970	907675.134792	44.323418
3503.271705	907623.949280	44.328423
3503.310468	907559.042717	44.333428
3503.174429	907513.933516	44.338433
3503.224696	907467.539582	44.343437
3503.384474	907420.548596	44.348442
3502.803839	907374.354259	44.353447
3503.167708	907315.466876	44.358452
3502.846900	907277.811992	44.363457
3503.215321	907214.968768	44.368461
3503.185893	907168.103257	44.373466
3503.032416	907121.643557	44.378471
3503.255134	907069.142011	44.383476
3503.101391	907027.985948	44.388481
3502.998065	906976.115901	44.393485
3503.067105	906926.435226	44.398490
3502.880944	906876.892596	44.403495
3503.168213	906824.281656	44.408500
3502.878188	906785.075194	44.413505
3502.987902	906741.076602	44.418509
3502.885702	906701.549259	44.423514
3502.762725	906645.146223	44.428519
3503.010004	906604.113852	44.433524
3502.708403	906563.171605	44.438529
3502.622343	906528.270068	44.443533
3502.708559	906491.121504	44.448538
3502.863347	906452.996854	44.453543
3502.836234	906400.337244	44.458548
3502.906226	906362.611765	44.463553
3502.724690	906321.744413	44.468557
3502.829369	906272.630760	44.473562
3502.908707	906231.526853	44.478567
3503.072620	906177.290335	44.483572
3502.862215	906155.332399	44.488577
3502.817128	906107.688851	44.493581
3502.947126	906060.401893	44.498586
3502.807584	906019.621862	44.503591
3502.770892	905968.406662	44.508596
3502.865233	905934.629226	44.513601
3502.807417	905894.510055	44.518605
3503.025721	905844.119875	44.523610
3502.639949	905803.282359	44.528615
3503.238762	905767.105631	44.533620
3502.764580	905725.606849	44.538625
3503.126692	905683.101775	44.543629
3503.290296	905642.076101	44.548634
3503.121306	905577.952374	44.553639
3503.065373	905536.286805	44.558644
3503.217109	905492.657299	44.563649
3503.035197	905442.232948	44.568653
3502.964103	905400.665333	44.573658
3503.023793	905355.023998	44.578663
3503.161409	905301.748016	44.583668
3502.849055	905256.842486	44.588673
3503.146659	905214.055041	44.593677
3503.119712	905164.085019	44.598682
3502.816358	905121.878253	44.603687
3502.976544	905069.368149	44.608692
3503.176711	905028.814328	44.613697
3503.143309	904978.168352	44.618701
3503.313179	904933.856130	44.623706
3502.745129	904895.068063	44.628711
3502.847710	904850.766266	44.633716
3502.610700	904816.843681	44.638721
3502.819114	904766.734840	44.643725
3502.923642	904725.036770	44.648730
3502.948907	904692.999900	44.653735
3502.975496	904639.349945	44.658740
3502.872936	904601.351511	44.663745
3502.656825	904546.872276	44.668749
3502.980143	904510.539827	44.673754
3503.109508	904465.844612	44.678759
3503.521664	904417.435862	44.683764
3502.974211	904372.272466	44.688769
3502.934466	904323.068937	44.693773
3503.213421	904272.268602	44.698778
3503.066944	904233.502965	44.703783
3503.139377	904182.928826	44.708788
3502.936230	904130.373254	44.713793
3503.098196	904082.678282	44.718797
3503.306508	904038.931596	44.723802
3502.984654	904000.579216	44.728807
3503.249451	903950.646759	44.733812
3502.993287	903907.844043	44.738817
3503.009019	903869.338647	44.743821
3503.365982	903824.504308	44.748826
3503.021796	903760.195540	44.753831
3502.787655	903713.431180	44.758836
3502.773000	903681.105578	44.763841
3502.721039	903647.145393	44.768845
3503.047738	903595.559024	44.773850
3502.423806	903559.762469	44.778855
3502.572302	903516.793585	44.783860
3502.741745	903486.849149	44.788865
3502.990634	903441.740033	44.793869
3503.162615	903402.723151	44.798874
3503.168167	903353.503622	44.803879
3503.191774	903294.243798	44.808884
3502.971824	903259.633374	44.813889
3503.045111	903213.972297	44.818893
3503.337778	903166.247979	44.823898
3502.838723	903128.787401	44.828903
3502.911428	903078.782300	44.833908
3503.037609	903036.295965	44.838913
3502.635199	902990.614922	44.843917
3502.769780	902965.788676	44.848922
3502.361268	902924.451238	44.853927
3502.666547	902880.486490	44.858932
3502.422822	902846.939101	44.863937
3502.637016	902802.120098	44.868941
3502.714538	902771.607879	44.873946
3502.440996	902730.632843	44.878951
3502.706476	902687.831361	44.883956
3502.934279	902657.679840	44.888961
3502.728031	902615.052038	44.893965
3502.613648	902571.443566	44.898970
3502.517451	902543.082186	44.903975
3502.866653	902489.744539	44.908980
3502.463699	902457.958455	44.913985
3502.818094	902420.931666	44.918989
3503.049667	902381.801334	44.923994
3502.534462	902337.774454	44.928999
3502.742939	902292.469694	44.934004
3502.430164	902263.563423	44.939009
3502.649022	902221.152166	44.944013
3502.706955	902191.894872	44.949018
3502.778008	902148.638669	44.954023
3502.716436	902102.121992	44.959028
3502.409270	902077.461118	44.964033
3502.606116	902044.222453	44.969037
3502.591124	902012.080329	44.974042
3502.281395	901970.719570	44.979047
3502.706594	901937.828780	44.984052
3502.654253	901906.078330	44.989057
3502.646638	901863.412083	44.994061
3502.872934	901820.513908	44.999066
3502.743561	901780.666577	45.004071
3502.910333	901733.530016	45.009076
3502.718839	901709.717284	45.014081
3502.746467	901658.741581	45.019085
3502.962868	901620.380735	45.024090
3502.644910	901582.011122	45.029095
3502.878918	901535.923745	45.034100
3502.741763	901494.144882	45.039105
3502.692889	901461.715569	45.044109
3502.496510	901417.532387	45.049114
3502.273815	901379.242234	45.054119
3502.302429	901342.455092	45.059124
3502.452910	901304.971831	45.064129
3502.416888	901289.337839	45.069133
3502.669424	901245.562062	45.074138
3502.836404	901214.447374	45.079143
3502.650682	901174.701567	45.084148
3502.588306	901135.610978	45.089153
3502.879025	901105.537305	45.094157
3502.511712	901070.068709	45.099162
3502.610263	901026.316594	45.104167
3502.958878	900997.391376	45.109172
3502.592096	900954.584299	45.114177
3502.505945	900903.813586	45.119181
3502.409259	900875.540403	45.124186
3502.731825	900836.094662	45.129191
3502.663231	900789.761367	45.134196
3502.518530	900764.971398	45.139201
3501.905214	900732.051549	45.144205
3502.564085	900694.383910	45.149210
3502.536657	900673.243243	45.154215
3502.634798	900631.419197	45.159220
3502.095101	900606.210830	45.164225
3501.970646	900574.271620	45.169229
3502.344039	900536.553403	45.174234
3502.205538	900521.320380	45.179239
3502.607127	900477.803743	45.184244
3502.512485	900457.542352	45.189249
3502.347059	900419.719007	45.194253
3502.391813	900387.557743	45.199258
3502.359118	900359.367979	45.204263
3502.532846	900321.294980	45.209268
3502.138772	900281.287498	45.214273
3502.227697	900258.001771	45.219277
3502.324472	900215.305809	45.224282
3501.891144	900196.547698	45.229287
3502.082313	900151.325091	45.234292
3502.279014	900141.829574	45.239297
3501.995698	900111.748601	45.244301
3502.253841	900093.455608	45.249306
3501.976519	900065.401237	45.254311
3502.306405	900022.375716	45.259316
3502.425666	900002.463705	45.264321
3502.242041	899971.303340	45.269325
3502.314216	899937.783068	45.274330
3502.142780	899915.601049	45.279335
3502.093189	899875.437359	45.284340
3502.159580	899841.531197	45.289345
3502.281393	899828.860747	45.294349
3502.287626	899783.182812	45.299354
3501.923605	899772.137377	45.304359
3502.106428	899731.065245	45.309364
3502.131982	899709.043098	45.314369
3502.087019	899689.639888	45.319373
3502.228903	899656.685883	45.324378
3502.273599	899631.473430	45.329383
3502.185458	899598.750126	45.334388
3501.994001	899573.576319	45.339393
3502.155806	899539.845768	45.344397
3502.519390	899504.246872	45.349402
3502.640613	899482.014930	45.354407
3502.422960	899448.829220	45.359412
3502.517652	899404.389113	45.364417
3502.386063	899379.011422	45.369421
3502.650697	899343.041508	45.374426
3502.396193	899317.007752	45.379431
3502.323746	899287.949981	45.384436
3502.544323	899247.833886	45.389441
3502.279885	899218.227916	45.394445
3502.577982	899168.150872	45.399450
3502.265776	899151.783802	45.404455
3502.286127	899115.756105	45.409460
3502.156788	899104.284370	45.414465
3502.282880	899063.892792	45.419469
3502.243856	899036.470100	45.424474
3502.203573	899010.303052	45.429479
3502.521271	898975.287875	45.434484
3502.202135	898944.916818	45.439489
3502.100034	898906.879710	45.444493
3502.122622	898881.184625	45.449498
3502.057699	898871.440323	45.454503
3502.439871	898835.447812	45.459508
3502.227141	898806.893599	45.464513
3502.271790	898769.990420	45.469517
3502.351398	898741.870648	45.474522
3502.198859	898710.987949	45.479527
3502.452422	898689.503781	45.484532
3502.369912	898654.455962	45.489537
3502.188070	898630.725183	45.494541
3502.438024	898588.571201	45.499546
3502.137305	898571.138066	45.504551
3502.435649	898535.060864	45.509556
3502.386154	898517.296402	45.514561
3502.331889	898477.026930	45.519565
3502.332805	898449.208440	45.524570
3502.118006	898413.987738	45.529575
3502.400613	898387.378237	45.534580
3502.399421	898360.139212	45.539585
3502.282722	898333.112274	45.544589
3502.319423	898283.746611	45.549594
3502.568722	898262.841093	45.554599
3502.503064	898219.577216	45.559604
3502.217405	898209.385158	45.564609
3502.160418	898175.199522	45.569613
3502.286647	898144.074602	45.574618
3502.050677	898116.100303	45.579623
3502.290463	898083.797172	45.584628
3501.888615	898065.702947	45.589633
3502.269621	898044.871525	45.594637
3502.618361	898003.662896	45.599642
3502.166879	897975.820006	45.604647
3502.362674	897946.131535	45.609652
3502.101307	897925.598704	45.614657
3502.306621	897894.555983	45.619661
3502.058241	897867.741713	45.624666
3502.270914	897843.846028	45.629671
3502.129181	897814.888690	45.634676
3502.256983	897776.806093	45.639681
3502.205962	897745.997993	45.644685
3502.549063	897721.500681	45.649690
3502.276668	897691.211775	45.654695
3502.325959	897652.175226	45.659700
3502.290479	897636.047977	45.664705
3501.889970	897597.954609	45.669709
3502.153301	897562.649827	45.674714
3501.856486	897547.145020	45.679719
3502.245721	897509.597198	45.684724
3502.140310	897505.653679	45.689729
3502.056053	897467.700546	45.694733
3502.266002	897443.030750	45.699738
3501.994548	897416.218139	45.704743
3502.011205	897378.924051	45.709748
3502.138311	897362.479406	45.714753
3501.779934	897338.965501	45.719757
3502.103492	897316.305262	45.724762
3502.027405	897289.170029	45.729767
3502.210006	897253.007113	45.734772
3502.561108	897244.157586	45.739777
3502.336076	897209.414122	45.744781
3502.362635	897181.295330	45.749786
3502.138907	897154.377000	45.754791
3502.352033	897121.299861	45.759796
3502.535213	897093.734519	45.764801
3502.424569	897070.275297	45.769805
3502.450226	897035.682696	45.774810
3502.277517	896985.374043	45.779815
3502.200127	896882.778828	45.784820
3502.085722	896740.863242	45.789825
3501.855470	896542.824700	45.794829
3502.111714	896283.340135	45.799834
3501.685312	895974.093207	45.804839
3502.173855	895601.476213	45.809844
3501.717053	895165.783207	45.814849
3501.598931	894665.531599	45.819853
3501.621207	894103.830392	45.824858
3501.208691	893493.227476	45.829863
3501.362264	892806.759837	45.834868
3501.171500	892064.373861	45.839873
3501.139169	891247.589392	45.844877
3500.684988	890369.819015	45.849882
3500.539837	889428.302417	45.854887
3500.111168	888419.429262	45.859892
3500.133081	887346.334056	45.864897
3499.534372	886195.218878	45.869901
3499.423130	884980.184347	45.874906
3498.961665	883688.449142	45.879911
3498.353331	882325.547432	45.884916
3497.901829	880901.456411	45.889921
3497.428751	879397.360873	45.894925
3497.157691	877818.495189	45.899930
3496.566768	876177.395046	45.904935
3496.483390	874460.876634	45.909940
3496.063120	872665.134423	45.914945
3495.542815	870794.912198	45.919949
3495.257408	868840.281432	45.924954
3494.445167	866820.808249	45.929959
3494.113695	864715.182295	45.934964
3493.580827	862546.559512	45.939969
3492.830006	860285.809187	45.944973
3492.787458	857962.344265	45.949978
3491.802749	855564.402220	45.954983
3490.925233	853080.533991	45.959988
3490.455489	850538.441483	45.964993
3489.606971	847918.607811	45.969997
3489.094603	845216.437853	45.975002
3487.801453	842458.341790	45.980007
3487.370848	839613.109639	45.985012
3486.537733	836710.459467	45.990017
3485.674706	833735.273041	45.995021
3485.056482	830677.645320	46.000026
3484.108436	827557.353937	46.005031
3483.105338	824355.598688	46.010036
3482.376418	821095.156986	46.015041
3481.347378	817765.624859	46.020045
3480.546625	814352.869792	46.025050
3479.400422	810880.288305	46.030055
3478.699705	807327.870655	46.035060
3477.591883	803716.635741	46.040065
3476.597816	800019.680125	46.045069
3475.830421	796249.775335	46.050074
3474.579783	792409.098825	46.055079
3473.320099	788507.451375	46.060084
3472.446073	784543.752408	46.065089
3471.196675	780501.660814	46.070093
3470.133085	776381.268962	46.075098
3468.534359	772213.321231	46.080103
3467.351011	767959.506433	46.085108
3466.490375	763649.501907	46.090113
3465.248201	759259.421694	46.095117
3464.241672	754814.131640	46.100122
3462.627952	750290.484478	46.105127
3461.191633	745692.147008	46.110132
3459.790542	741048.419146	46.115137
3458.155349	736319.112991	46.120141
3457.275930	731525.832359	46.125146
3455.623107	726660.970760	46.130151
3454.197600	721744.051318	46.135156
3452.991457	716756.416928	46.140161
3451.221408	711706.347448	46.145165
3449.837819	706569.724675	46.150170
3448.361861	701382.591357	46.155175
3446.430223	696119.947492	46.160180
3445.143826	690803.312046	46.165185
3443.243857	685427.165577	46.170189
3441.895685	679962.961737	46.175194
3439.747250	674459.760299	46.180199
3438.142027	668857.671802	46.185204
3436.332354	663225.160972	46.190209
3434.240294	657510.310408	46.195213
3433.030488	651747.410006	46.200218
3430.725736	645932.358008	46.205223
3428.843751	640039.960666	46.210228
3426.850001	634095.905071	46.215233
3424.976732	628092.262113	46.220237
3423.421419	622027.405772	46.225242
3420.899180	615900.755214	46.230247
3419.102640	609739.229008	46.235252
3417.134064	603499.620866	46.240257
3414.937331	597207.940495	46.245261
3412.562572	590862.656486	46.250266
3410.151243	584469.359698	46.255271
3408.360031	578007.215747	46.260276
3406.158877	571504.237853	46.265281
3403.960241	564930.564169	46.270285
3401.405183	558319.216277	46.275290
3399.214547	551653.515848	46.280295
3396.965125	544936.304796	46.285300
3394.463880	538164.240892	46.290305
3391.671200	531331.177227	46.295309
3389.213489	524464.224758	46.300314
3386.578448	517562.041784	46.305319
3384.032411	510591.924980	46.310324
3381.566207	503585.373433	46.315329
3378.630987	496544.695223	46.320333
3376.518552	489440.527300	46.325338
3373.563204	482314.112683	46.330343
3370.733324	475131.073215	46.335348
3368.109489	467909.510955	46.340353
3364.898750	460644.490583	46.345357
3362.241698	453344.036506	46.350362
3359.266336	446011.193905	46.355367
3356.293592	438635.728306	46.360372
3353.325350	431224.245130	46.365377
3349.920242	423795.820881	46.370381
3346.887926	416311.257680	46.375386
3343.716414	408820.347741	46.380391
3340.787907	401285.402355	46.385396
3337.474103	393717.421441	46.390401
3333.957366	386131.860415	46.395405
3330.779819	378495.370380	46.400410
3327.363024	370862.285372	46.405415
3324.127395	363195.413251	46.410420
3320.834109	355504.169482	46.415425
3317.187935	347796.334283	46.420429
3313.757136	340047.361377	46.425434
3310.154505	332296.044226	46.430439
3306.423917	324542.565512	46.435444
3302.751575	316764.961904	46.440449
3299.265887	308965.916094	46.445453
3295.898155	301143.613898	46.450458
3291.895178	293328.160346	46.455463
3288.059012	285489.262544	46.460468
3284.248663	277637.600796	46.465473
3280.208641	269785.405662	46.470477
3276.426357	261920.974235	46.475482
3272.420321	254062.535751	46.480487
3268.324301	246191.289628	46.485492
3264.252939	238319.815609	46.490497
3260.027241	230432.932001	46.495501
3256.137674	222493.935073	46.500506
3251.526569	214623.389828	46.505511
3247.250502	206756.277247	46.510516
3242.907873	198913.224071	46.515521
3238.280050	191079.295344	46.520525
3233.895608	183240.953371	46.525530
3229.401144	175444.206382	46.530535
3224.791318	167642.809210	46.535540
3220.118995	159871.417362	46.540545
3215.027730	152110.491255	46.545549
3210.560121	144374.754731	46.550554
3205.187275	136664.698493	46.555559
3200.303805	128978.384679	46.560564
3195.305558	121331.216635	46.565569
3190.334037	113726.491989	46.570573
3185.164467	106141.505741	46.575578
3179.525677	98601.968263	46.580583
3173.949474	91092.745618	46.585588
3168.567279	83650.540247	46.590593
3162.604589	76239.699323	46.595597
3156.864785	68888.891416	46.600602
3150.812912	61598.555340	46.605607
3143.943307	54371.438978	46.610612
3137.270771	47231.345984	46.615617
3129.226759	40183.985805	46.620621
3117.408657	33329.354690	46.625626
3095.071956	26914.781268	46.630631
3070.500621	20806.904394	46.635636
3040.977892	15189.385567	46.640641
3006.708122	10168.741334	46.645645
2971.137244	5760.791604	46.650650
2935.749976	2040.088025	46.655655
2852.052418	342.675241	46.660660
2748.113846	326.461282	46.665665
2703.223926	330.535079	46.670669
2709.313454	329.777390	46.675674
2744.047096	316.944371	46.680679
2785.333414	320.541495	46.685684
2818.575883	300.799747	46.690689
2837.193412	303.824958	46.695693
2843.171885	302.463725	46.700698
2840.442714	309.349374	46.705703
2833.887421	315.467491	46.710708
2827.528922	302.291284	46.715713
2822.044011	297.283051	46.720717
2818.101409	292.147855	46.725722
2815.356929	295.987090	46.730727
2813.113277	300.491628	46.735732
2811.149236	305.649420	46.740737
2809.058260	304.016273	46.745741
2806.932480	284.225439	46.750746
2804.116134	286.993124	46.755751
2801.143386	285.623868	46.760756
2797.876850	287.527269	46.765761
2794.794903	287.680179	46.770765
2791.443255	282.381990	46.775770
2788.402228	280.411850	46.780775
2785.151397	283.516458	46.785780
2782.546756	281.316843	46.790785
2778.978999	287.663985	46.795789
2776.200385	271.370457	46.800794
2772.911941	280.336823	46.805799
2769.611963	276.520063	46.810804
2766.617473	271.419513	46.815809
2763.024254	275.254351	46.820813
2759.521955	271.404674	46.825818
2756.140361	282.723349	46.830823
2753.028034	266.317557	46.835828
2750.138411	272.438759	46.840833
2746.923605	276.298396	46.845837
2743.415402	266.752037	46.850842
2739.761742	275.374126	46.855847
2736.256010	274.450831	46.860852
2733.351644	276.362005	46.865857
2729.902033	277.057923	46.870861
2726.645043	269.746273	46.875866
2722.796301	263.434517	46.880871
2719.292304	279.334774	46.885876
2716.331639	267.168556	46.890881
2712.912244	276.892647	46.895885
2709.443593	271.956808	46.900890
2706.538679	274.340919	46.905895
2702.924194	275.120501	46.910900
2699.415120	267.634179	46.915905
2695.862992	274.219942	46.920909
2692.535171	259.293915	46.925914
2689.010332	263.169220	46.930919
2685.313172	259.956805	46.935924
2682.162265	263.697397	46.940929
2678.942594	264.575641	46.945933
2676.121071	250.874075	46.950938
2672.014271	259.124584	46.955943
2668.563166	258.735015	46.960948
2664.874941	262.210248	46.965953
2661.396107	268.919707	46.970957
2657.567943	266.020207	46.975962
2654.910253	264.206341	46.980967
2651.954808	267.216895	46.985972
2647.826111	257.782482	46.990977
2643.880916	253.749435	46.995981
2640.915487	250.579313	47.000986
2637.275925	250.293486	47.005991
2633.935020	250.017185	47.010996
2630.299362	254.395881	47.016001
2626.842996	256.799201	47.021005
2624.074933	253.504164	47.026010
2620.740393	256.662149	47.031015
2617.457151	250.525946	47.036020
2613.672043	241.047110	47.041025
2609.730556	248.439965	47.046029
2606.721583	242.496901	47.051034
2603.132998	241.841157	47.056039
2598.899867	245.118632	47.061044
2595.855138	244.164355	47.066049
2592.232647	247.123988	47.071053
2589.531582	243.268912	47.076058
2585.999329	237.190014	47.081063
2582.317200	238.877564	47.086068
2578.816921	237.647209	47.091073
2575.033130	244.765806	47.096077
2571.907388	240.779143	47.101082
2568.133674	236.160572	47.106087
2564.147779	243.702871	47.111092
2561.614885	231.220310	47.116097
2558.020148	238.503084	47.121101
2554.898520	235.597581	47.126106
2551.147277	236.993837	47.131111
2547.478410	237.035763	47.136116
2544.019557	238.517962	47.141121
2540.558101	234.803013	47.146125
2537.115875	237.947245	47.151130
2533.492433	233.509927	47.156135
2529.625863	238.333320	47.161140
2526.523931	223.310587	47.166145
2522.955819	236.393192	47.171149
2519.695195	233.070581	47.176154
2516.054462	239.861700	47.181159
2512.855147	232.875790	47.186164
2509.229954	235.117208	47.191169
2505.653798	232.764716	47.196173
2502.145214	230.381340	47.201178
2498.575876	229.730784	47.206183
2495.318119	228.373237	47.211188
2491.778301	220.538540	47.216193
2488.103870	232.291658	47.221197
2484.545188	230.802626	47.226202
2480.929966	223.376643	47.231207
2477.451124	226.040707	47.236212
2474.420921	224.988991	47.241217
2470.764895	235.369931	47.246221
2467.744914	221.828383	47.251226
2464.156779	225.690990	47.256231
2460.453054	228.125378	47.261236
2457.132903	219.831550	47.266241
2453.341498	220.943231	47.271245
2450.138397	218.468033	47.276250
2446.349705	215.277434	47.281255
2443.022002	226.091626	47.286260
2439.684266	217.288615	47.291265
2435.837011	238.758164	47.296269
2432.304306	227.911303	47.301274
2428.890866	224.600562	47.306279
2425.336768	219.233658	47.311284
2422.142248	221.402864	47.316289
2418.567442	223.875994	47.321293
2414.858929	212.973913	47.326298
2411.611517	222.343553	47.331303
2407.409570	222.187825	47.336308
2404.476252	213.791312	47.341313
2401.258530	223.228087	47.346317
2397.873862	216.933758	47.351322
2394.534970	223.323268	47.356327
2390.480348	221.500767	47.361332
2387.177777	208.197557	47.366337
2383.172462	220.570139	47.371341
2380.372795	215.502232	47.376346
2376.816439	213.000736	47.381351
2373.014645	218.616327	47.386356
2369.601169	209.701552	47.391361
2366.025826	221.299058	47.396365
2362.419655	209.434276	47.401370
2359.021567	222.267284	47.406375
2355.456820	222.971017	47.411380
2352.465846	214.513212	47.416385
2348.435385	214.858691	47.421389
2345.392125	213.822631	47.426394
2341.720862	202.905789	47.431399
2337.702104	208.859149	47.436404
2334.960838	206.995326	47.441409
2331.224708	208.948118	47.446413
2327.873366	210.734577	47.451418
2324.438230	210.384450	47.456423
2320.792695	215.421531	47.461428
2317.141463	209.690474	47.466433
2313.264270	210.448579	47.471437
2309.895874	209.017464	47.476442
2306.796360	207.073476	47.481447
2303.411593	208.851458	47.486452
2300.151109	199.821894	47.491457
2295.992921	212.243842	47.496461
2292.556924	200.648229	47.501466
2289.179596	203.764539	47.506471
2285.529649	199.933689	47.511476
2282.491020	200.467539	47.516481
2279.013271	206.056535	47.521485
2275.498500	200.345810	47.526490
2271.866020	199.100602	47.531495
2268.082995	207.736224	47.536500
2264.364776	198.809687	47.541505
2261.022823	206.063339	47.546509
2257.771011	207.266059	47.551514
2254.334406	198.303892	47.556519
2250.634717	200.312297	47.561524
2247.521010	193.928955	47.566529
2243.565891	207.975464	47.571533
2240.844271	190.567110	47.576538
2237.474894	207.159107	47.581543
2233.475287	201.878147	47.586548
2229.812204	188.691042	47.591553
2225.720699	200.534274	47.596557
2222.481957	200.055295	47.601562
2219.077886	199.411996	47.606567
2215.546378	202.728457	47.611572
2212.477717	197.216261	47.616577
2208.643558	196.846845	47.621581
2205.689600	195.193848	47.626586
2201.780374	193.179568	47.631591
2197.835779	202.774936	47.636596
2195.081389	198.578235	47.641601
2191.140737	202.494886	47.646605
2188.062324	188.464352	47.651610
2184.297566	188.406740	47.656615
2180.633254	202.648789	47.661620
2177.519047	189.611860	47.666625
2174.071808	197.504566	47.671629
2170.447314	189.814369	47.676634
2166.871139	193.940819	47.681639
2162.700495	202.259052	47.686644
2159.708075	196.337256	47.691649
2156.607390	198.887787	47.696653
2153.329327	190.011617	47.701658
2149.565900	192.759199	47.706663
2145.994019	190.421277	47.711668
2142.177491	187.404449	47.716673
2138.379151	191.396902	47.721677
2135.055527	190.421873	47.726682
2131.931492	205.359762	47.731687
2128.116769	201.662808	47.736692
2124.992836	197.498554	47.741697
2121.267669	198.451150	47.746701
2118.030078	191.012459	47.751706
2114.559354	194.433211	47.756711
2110.755422	193.036265	47.761716
2107.723058	191.699786	47.766721
2103.524065	195.616535	47.771725
2100.198361	192.430877	47.776730
2096.992183	196.929638	47.781735
2093.371141	188.631128	47.786740
2089.823620	184.082967	47.791745
2086.282033	197.324418	47.796749
2082.844848	184.334191	47.801754
2079.413034	182.137379	47.806759
2075.604528	193.571665	47.811764
2072.474933	180.893960	47.816769
2068.884041	185.434162	47.821773
2065.451492	183.328652	47.826778
2061.909352	184.247517	47.831783
2058.368980	188.330633	47.836788
2054.890529	183.119280	47.841793
2051.334581	184.655541	47.846797
2047.607185	178.654307	47.851802
2044.217810	183.541719	47.856807
2040.875348	187.474156	47.861812
2037.446642	177.502860	47.866817
2033.756510	185.411881	47.871821
2030.180733	186.248310	47.876826
2027.017231	186.671313	47.881831
2022.991411	189.251562	47.886836
2019.995887	181.707457	47.891841
2016.478715	182.598156	47.896845
2012.737007	182.617188	47.901850
2009.275929	181.939448	47.906855
2005.689208	194.395882	47.911860
2002.463444	184.056012	47.916865
1998.805710	191.666857	47.921869
1995.469078	182.755493	47.926874
1991.800465	184.374143	47.931879
1988.067237	185.026241	47.936884
1984.752287	172.684706	47.941889
1981.144469	183.305821	47.946893
1977.649757	183.743693	47.951898
1974.315295	188.847840	47.956903
1971.216140	192.716854	47.961908
1967.565715	187.058184	47.966913
1963.807784	180.113254	47.971917
1960.302942	186.419718	47.976922
1956.714988	177.097198	47.981927
1953.101701	189.057200	47.986932
1949.819931	181.801963	47.991937
1946.423641	184.689756	47.996941
1943.139727	182.883227	48.001946
1939.687745	179.201119	48.006951
1935.587219	198.011541	48.011956
1932.399641	188.556996	48.016961
1928.322033	181.630360	48.021965
1925.369170	185.662120	48.026970
1922.108008	176.443132	48.031975
1917.886882	179.073089	48.036980
1915.148176	176.857040	48.041985
1911.120903	181.815164	48.046989
1908.007990	183.866228	48.051994
1904.315208	172.262065	48.056999
1900.490763	182.141296	48.062004
1897.409601	174.958941	48.067009
1893.917325	186.505891	48.072013
1890.350571	182.988019	48.077018
1886.815148	174.872494	48.082023
1882.898567	182.513143	48.087028
1879.536256	175.727516	48.092033
1876.365224	177.073436	48.097037
1872.760141	167.295206	48.102042
1869.340923	178.537641	48.107047
1865.600883	182.848052	48.112052
1862.145196	177.100868	48.117057
1858.412767	176.388925	48.122061
1855.294116	180.965729	48.127066
1852.201481	187.865265	48.132071
1848.394504	183.440665	48.137076
1844.807496	183.205954	48.142081
1841.104551	187.956639	48.147085
1838.036051	183.963801	48.152090
1834.376882	184.896636	48.157095
1831.150375	191.905918	48.162100
1827.258406	177.571773	48.167105
1823.190623	184.059328	48.172109
1820.022017	181.155183	48.177114
1816.867403	183.734958	48.182119
1813.157349	184.394218	48.187124
1810.099366	182.483762	48.192129
1806.551615	185.340822	48.197133
1802.579475	181.813021	48.202138
1799.054244	177.103144	48.207143
1795.297058	176.152613	48.212148
1792.597083	171.655315	48.217153
1788.872533	177.833998	48.222157
1785.263022	178.459304	48.227162
1781.949221	175.246458	48.232167
1778.139381	170.659787	48.237172
1774.914499	174.161718	48.242177
1770.704579	180.695882	48.247181
1767.529213	172.249243	48.252186
1764.462793	173.612883	48.257191
1760.711716	167.417286	48.262196
1757.367278	167.135269	48.267201
1753.770692	176.473941	48.272205
1750.305904	166.820645	48.277210
1746.823356	165.010959	48.282215
1742.883402	174.779529	48.287220
1739.535324	165.781270	48.292225
1736.084529	168.497643	48.297229
1732.587564	170.888142	48.302234
1729.357316	165.455088	48.307239
1725.735055	171.503643	48.312244
1722.531150	172.969551	48.317249
1718.876476	175.849862	48.322253
1715.488494	169.708379	48.327258
1711.774173	168.762280	48.332263
1707.966309	166.666354	48.337268
1704.785251	166.094922	48.342273
1700.854492	170.966420	48.347277
1697.583469	167.171526	48.352282
1694.512728	168.126841	48.357287
1690.952795	166.090808	48.362292
1687.336041	164.483707	48.367297
1683.488521	168.291033	48.372301
1680.052163	164.813555	48.377306
1676.371088	171.616026	48.382311
1672.712722	167.635510	48.387316
1669.471892	164.149221	48.392321
1666.315136	171.006169	48.397325
1662.692698	163.003489	48.402330
1659.472881	164.504825	48.407335
1655.654123	173.531373	48.412340
1652.372667	163.060884	48.417345
1648.745458	169.078538	48.422349
1645.316069	166.436652	48.427354
1641.484556	160.479021	48.432359
1637.699665	167.996263	48.437364
1634.490856	161.975221	48.442369
1631.104921	168.696200	48.447373
1627.590426	154.790094	48.452378
1624.267115	161.653666	48.457383
1620.569671	162.344539	48.462388
1617.196835	166.988939	48.467393
1613.808827	166.613778	48.472397
1610.161553	170.471549	48.477402
1606.821500	172.018442	48.482407
1602.963951	165.959569	48.487412
1599.552581	162.922629	48.492417
1596.114088	181.649128	48.497421
1592.505726	169.011059	48.502426
1589.213342	158.283523	48.507431
1585.453026	176.024210	48.512436
1582.211790	159.543107	48.517441
1578.614691	163.232962	48.522445
1575.027855	158.816827	48.527450
1571.101135	167.570789	48.532455
1567.930233	176.194343	48.537460
1565.043623	160.886050	48.542465
1561.207774	164.425331	48.547469
1557.532542	169.196899	48.552474
1554.047859	169.230065	48.557479
1550.580706	164.568022	48.562484
1546.831689	161.198159	48.567489
1543.463633	170.708186	48.572493
1540.182135	168.693948	48.577498
1536.619416	159.758558	48.582503
1532.716039	159.952294	48.587508
1529.855886	153.123441	48.592513
1525.982936	162.280985	48.597517
1522.740399	159.059124	48.602522
1518.982112	154.086655	48.607527
1515.296311	162.264479	48.612532
1512.372368	156.563309	48.617537
1508.401029	160.632773	48.622541
1505.092128	157.465307	48.627546
1501.639727	158.908093	48.632551
1497.909025	169.050751	48.637556
1494.301924	161.900552	48.642561
1490.847950	169.987792	48.647565
1487.420663	159.091608	48.652570
1483.990544	153.432864	48.657575
1480.479897	171.500387	48.662580
1476.989571	159.568736	48.667585
1473.491001	165.143543	48.672589
1469.935352	164.164709	48.677594
1466.656563	162.364190	48.682599
1463.126063	165.378883	48.687604
1459.508264	162.238028	48.692609
1455.923177	164.144222	48.697613
1452.749470	162.343318	48.702618
1449.026207	165.478088	48.707623
1445.215143	164.570295	48.712628
1442.024956	167.600989	48.717633
1438.420051	166.831209	48.722637
1434.904216	165.178819	48.727642
1431.728677	158.576008	48.732647
1428.029908	170.527765	48.737652
1424.839207	167.184924	48.742657
1420.704807	172.292572	48.747661
1417.112326	167.882232	48.752666
1414.008339	164.374697	48.757671
1410.645002	173.091322	48.762676
1407.441862	154.872042	48.767681
1403.416653	161.299212	48.772685
1399.871519	168.065007	48.777690
1396.431818	167.003523	48.782695
1392.944058	165.407305	48.787700
1389.357048	157.090767	48.792705
1385.718944	165.011760	48.797709
1382.110564	156.031955	48.802714
1378.978862	162.897760	48.807719
1375.469266	169.533967	48.812724
1371.994585	166.050827	48.817729
1368.501257	160.081156	48.822733
1364.626259	161.591719	48.827738
1361.454949	158.151000	48.832743
1357.628832	163.046716	48.837748
1354.648235	159.413057	48.842753
1351.181257	164.515037	48.847757
1347.390907	169.012148	48.852762
1343.870206	154.599180	48.857767
1340.154638	169.368797	48.862772
1336.686576	160.515024	48.867777
1333.780880	157.842863	48.872781
1329.847030	151.033155	48.877786
1326.378752	156.815983	48.882791
1322.678849	158.138782	48.887796
1319.255389	153.462601	48.892801
1315.942980	165.057324	48.897805
1312.345349	158.900498	48.902810
1308.881067	159.945583	48.907815
1305.203620	155.078536	48.912820
1301.994900	157.750072	48.917825
1298.528954	162.422905	48.922829
1294.849872	159.147469	48.927834
1291.615798	156.968495	48.932839
1287.626332	155.901076	48.937844
1284.826887	145.085808	48.942849
1280.881450	157.139603	48.947853
1277.163410	153.479104	48.952858
1273.773586	140.847063	48.957863
1270.030018	158.383874	48.962868
1266.650641	153.386484	48.967873
1262.853978	148.985560	48.972877
1259.822987	150.457137	48.977882
1256.290602	155.793181	48.982887
1252.691914	159.413090	48.987892
1249.483241	158.042979	48.992897
1246.165899	157.493999	48.997901
1242.499656	159.006267	49.002906
1238.931991	144.204914	49.007911
1235.032459	160.892340	49.012916
1231.918099	152.284683	49.017921
1228.171624	161.627561	49.022925
1224.772939	152.244211	49.027930
1221.384655	153.106495	49.032935
1216.850910	147.953649	49.037940
1213.953253	152.458395	49.042945
1210.678530	152.777588	49.047949
1207.489799	148.964527	49.052954
1204.173447	139.327037	49.057959
1200.426690	155.447928	49.062964
1196.968896	150.505393	49.067969
1193.108476	161.283622	49.072973
1189.878413	150.665312	49.077978
1186.440640	152.621357	49.082983
1182.706141	168.266832	49.087988
1179.285706	146.575026	49.092993
1175.521880	145.267542	49.097997
1171.921122	153.681179	49.103002
1168.635893	142.450399	49.108007
1165.013788	143.843935	49.113012
1162.226762	150.023180	49.118017
1158.237093	151.144383	49.123021
1154.801200	145.947842	49.128026
1151.337223	139.892007	49.133031
1147.468526	151.434734	49.138036
1144.186283	145.612697	49.143041
1140.462765	150.864980	49.148045
1137.123438	155.247823	49.153050
1133.782881	153.710354	49.158055
1130.158471	160.392351	49.163060
1126.974618	144.053932	49.168065
1123.153497	149.770320	49.173069
1119.419718	141.079277	49.178074
1116.610664	139.577874	49.183079
1112.377478	145.347006	49.188084
1109.222635	146.246357	49.193089
1105.762035	155.876344	49.198093
1101.817993	148.236364	49.203098
1098.789486	148.799094	49.208103
1095.213481	161.530976	49.213108
1091.942174	151.614983	49.218113
1088.255463	157.746477	49.223117
1084.741142	150.982879	49.228122
1081.170913	141.402267	49.233127
1077.289127	150.804720	49.238132
1074.051253	145.320544	49.243137
1070.647719	147.019211	49.248141
1066.921105	151.253802	49.253146
1064.028010	148.598092	49.258151
1059.996298	153.330697	49.263156
1056.780498	147.516488	49.268161
1052.940383	151.257570	49.273165
1049.497261	155.112788	49.278170
1046.179118	151.527857	49.283175
1042.502791	149.312079	49.288180
1039.530283	149.589515	49.293185
1036.121034	149.456679	49.298189
1032.103161	147.843615	49.303194
1028.206439	157.228252	49.308199
1024.870430	153.669775	49.313204
1021.453485	150.434897	49.318209
1017.994555	156.585415	49.323213
1014.481480	149.963951	49.328218
1010.947307	148.091544	49.333223
1007.258341	147.889936	49.338228
1003.894471	154.034019	49.343233
1000.472188	154.438346	49.348237
997.379355	157.931384	49.353242
994.064207	145.261584	49.358247
990.287316	153.941082	49.363252
986.735014	154.876247	49.368257
982.887149	152.490167	49.373261
979.333707	145.334311	49.378266
976.284136	145.948165	49.383271
972.322130	150.529601	49.388276
969.241372	144.668069	49.393281
965.842802	147.679664	49.398285
962.043164	147.869361	49.403290
958.488451	136.687670	49.408295
954.386168	158.789993	49.413300
951.480105	147.237587	49.418305
948.320133	141.604663	49.423309
944.850023	150.631884	49.428314
941.582955	141.639253	49.433319
937.570061	150.196001	49.438324
933.722644	143.853286	49.443329
930.380230	141.695457	49.448333
926.931883	147.518878	49.453338
923.656306	143.730259	49.458343
919.923278	149.433226	49.463348
916.164732	147.494005	49.468353
912.644283	136.239595	49.473357
909.217675	136.476576	49.478362
906.265016	134.649575	49.483367
902.415372	143.639144	49.488372
899.075992	138.265827	49.493377
895.523596	145.093555	49.498381
891.723342	149.073268	49.503386
888.707792	143.075901	49.508391
885.354963	150.122238	49.513396
881.754531	139.727656	49.518401
877.843008	138.084713	49.523405
873.890409	154.644994	49.528410
870.963975	134.698754	49.533415
867.307169	148.977643	49.538420
864.022793	140.447538	49.543425
860.633492	140.032108	49.548429
856.830187	143.430604	49.553434
853.449890	138.896260	49.558439
849.663849	139.013552	49.563444
846.294510	141.209543	49.568449
842.997516	144.685337	49.573453
839.739146	139.349582	49.578458
836.170479	141.172034	49.583463
832.358917	143.430718	49.588468
828.921508	145.219824	49.593473
825.165875	138.599573	49.598477
821.745846	137.709727	49.603482
818.552420	143.427320	49.608487
814.905970	139.167715	49.613492
811.528157	135.624415	49.618497
807.742209	138.094176	49.623501
804.287977	146.194934	49.628506
800.968743	135.437983	49.633511
797.035096	144.515726	49.638516
793.793864	141.637368	49.643521
790.633445	145.147638	49.648525
786.979432	138.939229	49.653530
783.791430	141.248932	49.658535
779.685967	143.012216	49.663540
776.392560	142.465745	49.668545
772.708019	140.588015	49.673549
769.095900	141.773206	49.678554
765.930752	138.357567	49.683559
762.409398	142.028398	49.688564
759.390290	142.381611	49.693569
755.564817	142.403680	49.698573
751.594586	137.355852	49.703578
748.118510	138.659849	49.708583
744.289509	146.005866	49.713588
740.936915	139.694751	49.718593
738.040353	141.249812	49.723597
734.399745	145.119179	49.728602
731.149157	136.188727	49.733607
727.494737	146.760349	49.738612
723.786965	142.647919	49.743617
720.294150	129.554481	49.748621
716.820491	138.247755	49.753626
713.575688	130.834473	49.758631
709.624566	130.850727	49.763636
706.434730	129.567885	49.768641
702.798434	129.826097	49.773645
699.126201	131.221979	49.778650
696.026656	138.624567	49.783655
692.215750	147.553427	49.788660
688.510734	140.399026	49.793665
685.366987	129.227751	49.798669
681.709039	146.593487	49.803674
678.419477	131.465077	49.808679
674.994784	131.715735	49.813684
671.464473	133.282538	49.818689
667.770710	136.856456	49.823693
664.212319	142.531321	49.828698
660.462501	134.382879	49.833703
657.147052	134.382424	49.838708
653.885408	137.167351	49.843713
650.516704	139.450405	49.848717
646.587792	140.054853	49.853722
643.123514	141.083077	49.858727
639.603331	130.366421	49.863732
635.958360	131.604910	49.868737
632.891588	130.662690	49.873741
629.375297	138.740878	49.878746
625.889786	137.657579	49.883751
621.956705	143.977792	49.888756
618.751318	139.177306	49.893761
615.395514	137.215920	49.898765
611.679020	139.344802	49.903770
608.311670	140.171324	49.908775
604.461281	132.928180	49.913780
600.867773	140.209889	49.918785
597.561752	132.773874	49.923789
594.348298	135.105679	49.928794
590.837979	132.427303	49.933799
587.113166	135.770014	49.938804
583.162464	137.566284	49.943809
579.818500	146.283192	49.948813
576.964510	151.679567	49.953818
573.872194	134.418562	49.958823
570.024082	141.556924	49.963828
566.374513	138.662830	49.968833
562.420146	134.541419	49.973837
559.019442	146.149625	49.978842
555.685382	143.930321	49.983847
552.250243	141.864104	49.988852
548.480103	132.578726	49.993857
545.053284	130.787608	49.998861
541.590467	141.161895	50.003866
538.264648	133.054711	50.008871
534.407717	143.208079	50.013876
531.100095	141.240168	50.018881
527.780887	129.672600	50.023885
524.206846	138.869447	50.028890
520.821371	133.504462	50.033895
517.172251	129.094404	50.038900
513.761827	136.254910	50.043905
510.285134	138.306703	50.048909
506.483252	140.357448	50.053914
503.121808	128.113716	50.058919
499.588572	132.183751	50.063924
496.109398	137.304933	50.068929
492.689010	135.189555	50.073933
488.836577	136.696140	50.078938
485.685560	135.130175	50.083943
481.885278	137.977519	50.088948
478.167722	140.275805	50.093953
475.146199	134.123844	50.098957
471.734718	138.370104	50.103962
468.156863	142.597129	50.108967
464.146744	141.586368	50.113972
461.014703	138.707365	50.118977
457.864511	129.769216	50.123981
454.222468	135.394142	50.128986
450.806076	125.916925	50.133991
446.937975	135.594061	50.138996
443.136117	136.671596	50.144001
439.903634	121.385770	50.149005
436.096201	130.183016	50.154010
433.039029	129.499636	50.159015
429.732647	138.521225	50.164020
426.372606	135.868239	50.169025
422.853988	136.823932	50.174029
418.871321	135.217847	50.179034
415.590766	132.427789	50.184039
411.983590	135.108651	50.189044
408.371866	126.212588	50.194049
405.251329	123.133208	50.199053
401.295158	134.693721	50.204058
398.113159	127.713522	50.209063
394.206810	137.547400	50.214068
391.104891	128.108767	50.219073
387.505574	135.992877	50.224077
383.818785	127.262786	50.229082
380.437174	126.936837	50.234087
376.634974	134.276338	50.239092
373.851173	135.761270	50.244097
370.067422	131.861437	50.249101
366.211651	138.405672	50.254106
362.926657	127.686462	50.259111
359.698006	129.215426	50.264116
355.951562	137.154694	50.269121
352.466124	129.886716	50.274125
349.002987	137.612155	50.279130
345.749231	131.620092	50.284135
341.879166	126.221799	50.289140
338.388301	129.368914	50.294145
335.090459	130.758584	50.299149
331.078240	133.775321	50.304154
327.924167	122.954555	50.309159
324.355317	123.497921	50.314164
320.918475	128.899545	50.319169
317.791061	130.479273	50.324173
313.928851	127.902194	50.329178
310.501434	118.698465	50.334183
307.073102	129.396748	50.339188
303.104957	130.175930	50.344193
299.745754	123.434714	50.349197
296.267091	129.079883	50.354202
292.934613	121.427494	50.359207
289.484846	130.397524	50.364212
285.916021	126.029833	50.369217
282.191263	122.272465	50.374221
279.022157	125.829119	50.379226
275.389445	120.319182	50.384231
271.468771	125.024610	50.389236
268.554148	127.248773	50.394241
265.164064	131.194653	50.399245
261.291598	134.427885	50.404250
257.911302	134.962591	50.409255
254.676832	135.014752	50.414260
250.949800	128.049509	50.419265
247.411693	133.244765	50.424269
243.584231	128.426585	50.429274
240.568247	120.607003	50.434279
236.690583	128.557821	50.439284
233.500223	132.308454	50.444289
229.770949	124.320421	50.449293
226.140231	120.732046	50.454298
222.921388	119.937247	50.459303
219.028102	137.283427	50.464308
215.732557	127.947637	50.469313
212.072434	131.607920	50.474317
208.720360	130.052160	50.479322
205.490438	121.580110	50.484327
201.551804	126.164251	50.489332
198.162361	120.429407	50.494337
194.964364	121.641826	50.499341
191.227645	127.648094	50.504346
187.900830	122.834115	50.509351
184.410978	132.554020	50.514356
180.868360	125.551409	50.519361
177.394336	119.343563	50.524365
173.038676	125.900457	50.529370
170.200695	119.468329	50.534375
166.907269	123.068138	50.539380
163.522282	128.737366	50.544385
160.008583	128.639081	50.549389
156.308146	122.095180	50.554394
152.807540	120.456311	50.559399
149.097799	130.325914	50.564404
145.737167	125.697734	50.569409
142.268506	127.961410	50.574413
138.645027	135.736239	50.579418
135.296056	127.345720	50.584423
131.604312	129.393157	50.589428
128.323201	128.574008	50.594433
124.858825	128.881398	50.599437
121.125598	135.917631	50.604442
117.719006	117.652952	50.609447
114.112317	126.842276	50.614452
110.636200	119.472532	50.619457
107.328108	121.292682	50.624461
103.658064	134.390660	50.629466
100.400350	130.755635	50.634471
96.540943	136.966015	50.639476
93.010693	130.461086	50.644481
89.953956	128.629984	50.649485
86.228649	136.017375	50.654490
82.882841	135.908525	50.659495
79.367142	135.125294	50.664500
75.475712	135.744575	50.669505
72.290755	130.116086	50.674509
68.770872	134.565103	50.679514
65.257342	131.097968	50.684519
61.782437	134.755728	50.689524
58.434963	127.670399	50.694529
54.700228	130.407008	50.699533
50.785756	134.505391	50.704538
47.492305	124.537341	50.709543
44.014607	124.667231	50.714548
40.907923	128.243713	50.719553
37.290791	127.269914	50.724557
33.480337	134.199025	50.729562
30.133825	129.059677	50.734567
26.496943	133.107381	50.739572
23.017608	120.067439	50.744577
20.028810	115.651700	50.749581
16.263328	130.457488	50.754586
12.553704	119.563027	50.759591
9.132041	121.530522	50.764596
5.521627	124.507068	50.769601
1.883929	120.043291	50.774605