Tue Jun 21 13:18:34 2022

Number of Points = 9927

Depth (nm)	Load (N)	Time (s)
0.319828	83.715956	0.000000
0.400125	81.550962	0.005005
0.173954	98.989391	0.010010
0.996313	100.633988	0.015014
0.951197	108.290969	0.020019
0.574379	95.826219	0.025024
0.640536	93.358881	0.030029
0.066188	81.453343	0.035034
0.056846	66.538638	0.040038
-0.024665	65.759086	0.045043
-0.238208	73.969245	0.050048
-0.553109	44.375561	0.055053
-0.828132	35.192437	0.060058
-1.581521	28.750566	0.065062
-1.533962	15.162239	0.070067
-1.979692	14.147203	0.075072
-2.289290	9.110861	0.080077
-2.642786	4.772062	0.085082
-2.480199	8.594355	0.090086
-2.834850	1.214054	0.095091
-3.549844	6.579979	0.100096
-3.731318	-9.191976	0.105101
-3.973508	1.535728	0.110106
-3.845863	-4.002415	0.115110
-4.484642	-7.397284	0.120115
-5.080260	-4.300334	0.125120
-5.324554	-15.622080	0.130125
-5.237676	-9.552459	0.135130
-5.680673	-6.707716	0.140134
-5.757271	-3.744077	0.145139
-5.891805	0.739150	0.150144
-6.043828	-14.603148	0.155149
-6.892393	-6.514803	0.160154
-6.846043	-9.645633	0.165158
-7.192102	-5.110605	0.170163
-7.192989	-5.040369	0.175168
-7.274775	-14.662364	0.180173
-7.183480	-12.411275	0.185178
-8.011368	-6.889315	0.190182
-8.202313	-6.066747	0.195187
-8.783366	-1.376572	0.200192
-8.582039	-14.408600	0.205197
-9.007301	-0.084576	0.210202
-9.514824	-4.245719	0.215206
-9.938668	-8.679029	0.220211
-10.430670	-8.560022	0.225216
-9.871462	-12.418892	0.230221
-9.952577	-14.748555	0.235226
-10.374471	-12.870293	0.240230
-10.254505	-16.045084	0.245235
-10.602674	-7.982775	0.250240
-11.424888	-10.074269	0.255245
-11.855389	-8.246479	0.260250
-11.960853	-4.671458	0.265254
-12.276612	-8.970917	0.270259
-12.225133	-8.694656	0.275264
-11.811922	-5.403653	0.280269
-12.536243	-8.212286	0.285274
-13.118921	-3.273005	0.290278
-12.934461	-11.202364	0.295283
-13.216137	-2.606622	0.300288
-14.272684	-2.642960	0.305293
-14.388827	2.738245	0.310298
-14.961506	-8.741256	0.315302
-15.111913	-0.642627	0.320307
-15.203077	-5.313563	0.325312
-14.952546	-7.929424	0.330317
-14.989567	-14.449257	0.335322
-15.010495	-13.405614	0.340326
-15.089107	-6.746187	0.345331
-16.434269	-7.456770	0.350336
-16.398519	-10.185061	0.355341
-16.529190	1.236545	0.360346
-16.693236	-2.263384	0.365350
-16.292200	-12.808147	0.370355
-17.560529	-5.647408	0.375360
-17.672696	-10.440763	0.380365
-18.185481	-10.103220	0.385370
-18.302727	-8.797552	0.390374
-18.248375	-10.960605	0.395379
-18.383898	-6.241205	0.400384
-18.182898	-10.487517	0.405389
-19.027961	-19.753210	0.410394
-19.317114	-15.785863	0.415398
-19.903334	-7.362478	0.420403
-19.689238	-3.022630	0.425408
-19.710898	-3.743417	0.430413
-20.163227	-10.340697	0.435418
-20.957984	1.622059	0.440422
-21.328584	-7.088776	0.445427
-21.641435	-7.461591	0.450432
-21.420951	-8.970963	0.455437
-21.881072	-6.950209	0.460442
-21.523121	-4.943376	0.465446
-21.486241	-13.218885	0.470451
-21.819626	9.215710	0.475456
-22.257534	-8.681874	0.480461
-23.189929	-5.069955	0.485466
-23.090035	-18.097809	0.490470
-23.059621	-2.840486	0.495475
-23.239721	-11.395795	0.500480
-24.004692	-10.040084	0.505485
-24.129274	-3.682067	0.510490
-24.379668	-4.120873	0.515494
-24.402026	-0.589412	0.520499
-24.832487	-7.716798	0.525504
-24.596881	-9.782786	0.530509
-25.570760	-2.394343	0.535514
-25.735441	-11.946764	0.540518
-25.771877	-5.612225	0.545523
-26.100934	-6.973165	0.550528
-26.185114	-4.328542	0.555533
-26.467057	-6.155689	0.560538
-27.049827	-1.004850	0.565542
-27.523099	1.797747	0.570547
-27.757126	4.040158	0.575552
-27.752040	-10.051019	0.580557
-28.047637	4.341913	0.585562
-28.304502	0.618977	0.590566
-27.950442	-11.305061	0.595571
-28.273552	-11.447665	0.600576
-28.204624	-10.784363	0.605581
-29.263231	-4.362239	0.610586
-29.333451	-5.616071	0.615590
-29.335745	-6.608833	0.620595
-29.641106	-6.168100	0.625600
-30.069800	-10.521866	0.630605
-30.839394	-9.142893	0.635610
-30.390622	-0.385539	0.640614
-30.675604	-11.333506	0.645619
-31.205421	-1.742960	0.650624
-31.302935	-7.319982	0.655629
-31.484845	-11.203329	0.660634
-31.653920	-2.908619	0.665638
-32.092112	-13.308871	0.670643
-32.725634	-5.022098	0.675648
-32.527458	-8.528338	0.680653
-32.617005	2.252624	0.685658
-33.126046	-3.653281	0.690662
-33.383761	-15.340432	0.695667
-34.012244	-2.222598	0.700672
-34.233617	-8.278361	0.705677
-34.155836	-6.976180	0.710682
-34.831394	1.127526	0.715686
-33.965002	-9.260467	0.720691
-34.410268	-4.780442	0.725696
-34.626651	-5.938634	0.730701
-35.435533	-7.927547	0.735706
-35.638513	-1.600157	0.740710
-35.736912	-2.000593	0.745715
-35.880912	-4.859350	0.750720
-36.064961	-1.979740	0.755725
-36.825379	-5.837136	0.760730
-37.265482	-7.251316	0.765734
-37.288209	-7.630343	0.770739
-37.460870	-4.754000	0.775744
-36.965838	-12.451224	0.780749
-37.239408	1.490703	0.785754
-37.859380	0.137489	0.790758
-38.265200	-6.581551	0.795763
-38.447652	-2.603849	0.800768
-38.603966	-3.092374	0.805773
-39.523773	-9.153234	0.810778
-40.126470	3.577705	0.815782
-39.991404	-7.174810	0.820787
-40.290593	-1.043619	0.825792
-40.145372	-9.934003	0.830797
-40.382818	-0.568094	0.835802
-40.293740	-3.611281	0.840806
-40.547023	-3.149769	0.845811
-40.607767	3.925640	0.850816
-40.902198	-6.414163	0.855821
-41.689499	0.787294	0.860826
-42.078166	-4.436236	0.865830
-41.837703	-5.273052	0.870835
-42.386288	6.614012	0.875840
-42.951583	-9.198758	0.880845
-43.146832	-4.990229	0.885850
-43.635627	-7.984875	0.890854
-43.309175	-8.471853	0.895859
-43.652577	-0.822755	0.900864
-43.451983	-9.610028	0.905869
-43.537568	-7.058116	0.910874
-44.518688	2.841212	0.915878
-44.856792	-0.087224	0.920883
-45.145738	-0.839323	0.925888
-45.169943	-10.476378	0.930893
-45.222225	-4.402655	0.935898
-45.432461	-1.118121	0.940902
-45.421130	-4.546453	0.945907
-46.423359	-0.338068	0.950912
-46.717349	-3.024183	0.955917
-47.094015	3.290929	0.960922
-47.063897	-1.455148	0.965926
-46.738815	-1.790347	0.970931
-47.092795	-10.044538	0.975936
-47.284220	-7.150683	0.980941
-48.028718	4.873019	0.985946
-48.419055	-1.311050	0.990950
-48.532636	-12.553207	0.995955
-48.345523	0.034889	1.000960
-48.398588	-8.993350	1.005965
-48.830161	-1.567239	1.010970
-49.613218	-7.766383	1.015974
-50.052297	-7.487219	1.020979
-50.016698	-9.039775	1.025984
-50.139208	-9.946126	1.030989
-50.049013	-7.979805	1.035994
-50.485366	-9.275021	1.040998
-50.820405	-8.844566	1.046003
-51.346031	-0.718133	1.051008
-51.650829	-13.845119	1.056013
-51.648274	-14.519793	1.061018
-51.767341	-3.711847	1.066022
-51.530128	-9.227285	1.071027
-52.379205	-0.018390	1.076032
-53.109657	-3.174293	1.081037
-53.204141	2.648113	1.086042
-53.528247	-5.494205	1.091046
-53.375049	-6.047605	1.096051
-53.569711	-6.222925	1.101056
-53.657747	-9.532580	1.106061
-53.426011	-5.156586	1.111066
-54.066309	-5.964553	1.116070
-54.542934	-10.104560	1.121075
-54.625002	0.221294	1.126080
-55.228502	-7.148565	1.131085
-56.101391	-8.144155	1.136090
-56.303667	-0.930659	1.141094
-55.814476	-7.207306	1.146099
-56.351968	-3.754121	1.151104
-56.596012	-7.354659	1.156109
-56.915419	1.029083	1.161114
-56.757786	-5.928507	1.166118
-56.388606	-11.466787	1.171123
-57.011015	2.477659	1.176128
-57.862962	-7.558067	1.181133
-58.157346	-0.356548	1.186138
-58.587732	-0.758636	1.191142
-58.063216	-5.633162	1.196147
-58.200057	-2.382885	1.201152
-58.481395	-7.599915	1.206157
-59.442457	-5.283469	1.211162
-59.845120	-2.652206	1.216166
-59.440559	-14.858700	1.221171
-59.889871	-2.869486	1.226176
-60.015491	-11.827492	1.231181
-60.339831	-10.332421	1.236186
-61.077079	-5.374839	1.241190
-61.045740	-10.375872	1.246195
-61.636212	0.555141	1.251200
-61.004039	-4.565135	1.256205
-61.359773	-1.492120	1.261210
-61.710181	-3.293323	1.266214
-61.909642	-9.277922	1.271219
-62.836782	-6.908287	1.276224
-62.894562	-9.424544	1.281229
-62.800891	-11.457751	1.286234
-63.211267	-9.584351	1.291238
-62.901011	-12.416712	1.296243
-63.558655	-0.940790	1.301248
-64.038798	-16.636817	1.306253
-64.158709	-22.103760	1.311258
-64.709349	-2.841049	1.316262
-64.430023	-8.954672	1.321267
-64.632378	-0.010355	1.326272
-65.481023	-11.796178	1.331277
-65.774094	-0.814965	1.336282
-65.777732	-0.088536	1.341286
-66.069094	-12.774930	1.346291
-66.328045	2.401062	1.351296
-66.541923	-6.002624	1.356301
-66.171514	-4.172696	1.361306
-66.354238	-6.764163	1.366310
-67.202482	-12.757934	1.371315
-67.916051	-2.433068	1.376320
-67.956683	-0.586962	1.381325
-67.718670	-11.499786	1.386330
-67.936601	-1.624637	1.391334
-67.914290	-13.069659	1.396339
-68.933613	-2.238908	1.401344
-69.216275	-8.297539	1.406349
-69.793673	-6.273144	1.411354
-69.974798	-10.962130	1.416358
-69.650016	-11.869349	1.421363
-70.034593	-6.904069	1.426368
-69.777064	-12.580539	1.431373
-69.986220	-2.901612	1.436378
-70.792898	3.842680	1.441382
-70.977839	-4.003991	1.446387
-71.202815	2.180425	1.451392
-70.911248	-5.569933	1.456397
-71.194442	4.511388	1.461402
-72.600844	-5.247408	1.466406
-72.575005	-12.457855	1.471411
-72.708135	-1.399532	1.476416
-72.809825	-2.848247	1.481421
-72.713541	-1.823029	1.486426
-73.102459	5.259765	1.491430
-72.741585	-10.102745	1.496435
-73.615872	5.528781	1.501440
-73.688244	-5.210689	1.506445
-74.120736	4.663295	1.511450
-74.257356	-1.023479	1.516454
-74.259719	-10.532723	1.521459
-75.609335	-7.612807	1.526464
-75.542976	-7.237385	1.531469
-75.807760	-1.405128	1.536474
-75.920230	-5.997150	1.541478
-75.850991	-1.362970	1.546483
-76.060071	-8.715268	1.551488
-75.877503	-6.214478	1.556493
-75.896617	-9.824442	1.561498
-77.238587	3.566274	1.566502
-77.341923	-0.812761	1.571507
-77.709722	1.112987	1.576512
-77.314571	-13.185652	1.581517
-77.625715	0.620217	1.586522
-78.541602	-6.266135	1.591526
-78.673179	-14.159723	1.596531
-78.744278	-10.857190	1.601536
-78.923050	-7.281277	1.606541
-79.295752	-6.863723	1.611546
-78.919266	-2.467699	1.616550
-79.641856	-8.100242	1.621555
-80.171678	-2.101941	1.626560
-80.588261	-5.769607	1.631565
-80.693803	-11.592751	1.636570
-81.320482	-6.693735	1.641574
-80.540682	-9.188083	1.646579
-80.720629	-14.365858	1.651584
-81.362882	-15.250063	1.656589
-82.029505	-10.180646	1.661594
-82.111481	-13.706790	1.666598
-81.979875	-17.670077	1.671603
-82.029358	-17.097079	1.676608
-82.303924	-13.673430	1.681613
-83.055746	-12.355605	1.686618
-83.744331	-13.918459	1.691622
-83.551513	-19.295708	1.696627
-83.922980	-9.877418	1.701632
-83.668008	-18.097872	1.706637
-84.095107	-10.288299	1.711642
-84.198747	-16.116294	1.716646
-84.953723	-11.603918	1.721651
-85.368416	-11.410288	1.726656
-85.558478	-11.472902	1.731661
-85.725428	-6.957669	1.736666
-85.640688	-8.570854	1.741670
-85.835028	-18.758498	1.746675
-85.893207	-3.731403	1.751680
-86.013089	-24.226625	1.756685
-86.613010	-21.519675	1.761690
-87.014151	-18.543333	1.766694
-87.043280	-14.001004	1.771699
-87.591169	-13.165491	1.776704
-87.919596	-28.390927	1.781709
-88.259764	-16.564447	1.786714
-88.639929	-8.959190	1.791718
-88.919330	-23.100908	1.796723
-89.088543	-12.596451	1.801728
-88.967653	-14.061309	1.806733
-89.027902	-12.820728	1.811738
-89.244089	-13.530805	1.816742
-88.832341	-23.638859	1.821747
-89.628078	-8.426466	1.826752
-89.621642	-9.553084	1.831757
-90.430181	-10.383895	1.836762
-91.237167	-8.452896	1.841766
-91.229461	-7.989418	1.846771
-91.801314	-3.396664	1.851776
-91.809429	-16.963101	1.856781
-91.941164	-18.853402	1.861786
-92.074362	-4.475738	1.866790
-91.630173	-27.024289	1.871795
-91.799959	-12.135006	1.876800
-92.069157	-14.904745	1.881805
-92.758661	-15.019812	1.886810
-93.111313	-11.086147	1.891814
-93.326437	-19.464356	1.896819
-94.229167	-11.350062	1.901824
-94.449117	-20.077934	1.906829
-94.814511	-9.605709	1.911834
-94.983583	-13.675879	1.916838
-94.921267	-20.597941	1.921843
-95.103809	-15.753938	1.926848
-94.845505	-12.762101	1.931853
-95.074778	-12.153406	1.936858
-95.321245	-17.105463	1.941862
-95.794754	-15.569108	1.946867
-96.866460	-13.246959	1.951872
-96.825786	-17.712985	1.956877
-96.850880	-17.048321	1.961882
-96.828950	-17.700551	1.966886
-96.729130	-16.307500	1.971891
-97.497664	-11.922327	1.976896
-98.275737	-8.405613	1.981901
-98.387504	-15.636284	1.986906
-98.501946	-14.982672	1.991910
-98.434282	-28.412860	1.996915
-98.386815	-8.331812	2.006912
-98.401220	-12.077553	2.016909
-98.339065	-16.405018	2.026906
-97.257956	-19.711586	2.036902
-96.976124	-8.384386	2.046899
-96.461488	-14.080980	2.056896
-95.699728	-13.734847	2.066893
-95.625187	-18.281707	2.076890
-95.266434	-12.553383	2.086886
-94.236984	-11.415799	2.096883
-94.125293	-11.502987	2.106880
-93.456654	-18.081816	2.116877
-92.799698	-15.907652	2.126874
-92.538015	-18.163879	2.136870
-92.108628	-10.736953	2.146867
-91.266294	-11.264056	2.156864
-90.918311	-17.659371	2.166861
-90.920156	-19.013047	2.176858
-90.284626	-16.015157	2.186854
-89.315752	-15.773666	2.196851
-88.762403	-13.586095	2.206848
-88.697840	-13.881833	2.216845
-87.963592	-13.042909	2.226842
-87.110441	-15.219072	2.236838
-86.838363	-19.143456	2.246835
-86.782236	-16.249164	2.256832
-85.557621	-14.334790	2.266829
-85.181683	-18.624521	2.276826
-85.242301	-14.062635	2.286822
-84.717771	-20.308966	2.296819
-84.105665	-17.594485	2.306816
-83.553070	-7.203631	2.316813
-82.492187	-11.697103	2.326810
-82.463745	-6.183376	2.336806
-82.163137	-13.673176	2.346803
-81.246015	-12.648774	2.356800
-81.208894	-11.650722	2.366797
-80.288605	-14.777721	2.376794
-79.305447	-7.952080	2.386790
-79.323821	-6.966966	2.396787
-79.426146	-8.282663	2.406784
-78.815826	-5.391241	2.416781
-77.881316	-1.586132	2.426778
-77.147966	-3.793233	2.436774
-76.412310	-5.969893	2.446771
-76.489171	-6.540562	2.456768
-76.081582	-1.517599	2.466765
-75.791874	-2.390232	2.476762
-74.592586	-8.666719	2.486758
-74.584533	-9.988841	2.496755
-73.894406	-1.684738	2.506752
-72.964979	-12.519482	2.516749
-73.081083	-10.871683	2.526746
-72.692539	-6.718697	2.536742
-71.721106	-8.922549	2.546739
-71.704115	-11.957243	2.556736
-70.583649	-13.560419	2.566733
-69.801391	-7.639836	2.576730
-69.787429	-8.322760	2.586726
-69.680809	-7.416635	2.596723
-69.170539	-10.850941	2.606720
-68.479366	-2.816319	2.616717
-68.263953	-5.580978	2.626714
-67.099754	-1.781502	2.636710
-66.809951	-3.412880	2.646707
-66.807332	-15.368750	2.656704
-65.672659	-5.832627	2.666701
-65.586919	-10.699853	2.676698
-64.780316	-7.413955	2.686694
-63.879737	-11.560192	2.696691
-63.643614	-5.080484	2.706688
-63.687166	-0.805943	2.716685
-63.250189	-9.883999	2.726682
-62.307192	-7.614347	2.736678
-62.166289	-7.158862	2.746675
-61.039668	-7.120724	2.756672
-60.711209	-3.987799	2.766669
-60.807532	-4.501700	2.776666
-59.782744	-9.092329	2.786662
-59.406440	-13.530904	2.796659
-59.087339	-9.005624	2.806656
-58.287536	-5.602022	2.816653
-57.582786	-6.878892	2.826650
-57.499517	-13.435066	2.836646
-56.363631	-9.477969	2.846643
-56.289013	-7.401579	2.856640
-56.179267	-6.742163	2.866637
-55.266575	-3.587443	2.876634
-54.641583	-3.605524	2.886630
-54.230895	-6.396792	2.896627
-54.271281	-9.479284	2.906624
-53.484873	-5.255063	2.916621
-53.005681	-7.578927	2.926618
-52.084699	-3.207859	2.936614
-51.651765	-4.834685	2.946611
-51.239989	-5.745909	2.956608
-51.140723	-7.751372	2.966605
-50.123680	-4.037774	2.976602
-49.637253	-5.794777	2.986598
-49.470858	-8.449164	2.996595
-49.279163	-8.500402	3.006592
-48.423928	-4.584154	3.016589
-47.476117	-4.366432	3.026586
-47.072723	-12.708647	3.036582
-46.656342	-18.020863	3.046579
-46.590690	-12.586998	3.056576
-46.036319	-6.298304	3.066573
-45.098456	-9.856573	3.076570
-44.889045	-12.116788	3.086566
-44.494467	-6.773949	3.096563
-43.748482	-8.395518	3.106560
-43.353607	-7.656275	3.116557
-43.034113	-12.634926	3.126554
-41.632627	-8.931449	3.136550
-41.694279	-5.384977	3.146547
-41.805061	-11.513647	3.156544
-41.147906	-14.132338	3.166541
-40.412925	-9.294394	3.176538
-39.755213	-10.830804	3.186534
-39.219193	-8.366304	3.196531
-38.972004	-9.965133	3.206528
-38.213292	-15.801333	3.216525
-37.649657	-12.311787	3.226522
-37.307682	-11.677988	3.236518
-37.086019	-6.901046	3.246515
-35.972157	-5.826230	3.256512
-35.536603	-8.164204	3.266509
-35.692157	-13.307804	3.276506
-34.776305	-10.615955	3.286502
-34.338999	-7.926257	3.296499
-33.780195	-9.892830	3.306496
-33.009661	-8.338124	3.316493
-32.504640	-7.488493	3.326490
-32.427490	-6.034125	3.336486
-32.267157	-11.953007	3.346483
-31.339772	-7.515618	3.356480
-30.834877	-6.468578	3.366477
-30.098428	-6.984456	3.376474
-29.393734	-7.679028	3.386470
-29.349602	-8.010109	3.396467
-29.186340	-5.887541	3.406464
-28.281765	-5.885926	3.416461
-27.904022	-2.804232	3.426458
-27.043222	-9.713435	3.436454
-26.115470	-13.145546	3.446451
-26.661997	-13.175098	3.456448
-26.100255	-15.076360	3.466445
-25.040463	-12.571947	3.476442
-24.818886	-5.401042	3.486438
-24.366600	-9.056521	3.496435
-23.587890	-5.430098	3.506432
-22.769217	-7.333208	3.516429
-22.887881	-8.575465	3.526426
-22.903211	-11.250339	3.536422
-21.591421	-15.971475	3.546419
-21.443511	-13.286013	3.556416
-20.660230	-6.009754	3.566413
-19.825182	-8.071668	3.576410
-19.801389	-3.812033	3.586406
-19.622416	-6.607999	3.596403
-18.731786	-12.590128	3.606400
-18.413170	-8.492536	3.616397
-17.767015	-5.822801	3.626394
-16.776933	-8.935068	3.636390
-16.301918	-11.810884	3.646387
-16.256480	-13.476081	3.656384
-16.409614	-12.078814	3.666381
-15.327524	-16.399141	3.676378
-14.941238	-13.100332	3.686374
-13.826759	-11.461308	3.696371
-13.541111	-7.299375	3.706368
-13.876446	-9.737697	3.716365
-12.880298	-8.571657	3.726362
-12.016086	-12.538185	3.736358
-11.892410	-9.910553	3.746355
-11.046528	-11.047187	3.756352
-10.377993	-12.815178	3.766349
-10.309556	-11.899764	3.776346
-10.069632	-12.982678	3.786342
-9.092881	-13.742059	3.796339
-8.940748	-10.402298	3.806336
-7.891872	-9.750611	3.816333
-7.574156	-8.096608	3.826330
-7.259246	-9.548187	3.836326
-6.954755	-13.126039	3.846323
-5.988541	-11.649178	3.856320
-5.917140	-13.621574	3.866317
-5.484889	-9.236738	3.876314
-4.591845	2.028785	3.886310
-4.127021	3.129886	3.896307
-4.200503	9.546082	3.906304
-3.712072	19.985932	3.916301
-2.853444	36.387504	3.926298
-2.535477	44.072992	3.936294
-1.935240	53.065799	3.946291
-1.522426	60.043245	3.956288
-1.377095	73.380455	3.966285
-0.647069	92.069111	3.976282
-0.367976	102.356965	3.986278
0.000000	129.941015	3.991283
0.103567	135.010402	3.996288
0.540045	144.628485	4.001293
1.075162	154.958998	4.006298
0.978136	169.061481	4.011302
0.965519	159.425752	4.016307
0.913768	156.687452	4.021312
1.092006	166.195182	4.026317
1.005837	162.888729	4.031322
1.073671	171.938773	4.036326
0.944577	165.616251	4.041331
0.787508	170.049979	4.046336
0.574652	169.868787	4.051341
0.728960	166.430354	4.056346
0.826772	169.677328	4.061350
0.946213	159.642030	4.066355
1.461039	178.033709	4.071360
0.968169	175.904419	4.076365
1.118257	165.442336	4.081370
1.001340	186.358565	4.086374
1.278126	194.798392	4.091379
1.420692	187.425843	4.096384
1.501765	186.641265	4.101389
1.416271	170.809028	4.106394
1.521700	172.418042	4.111398
1.302996	168.317950	4.116403
1.246112	164.410102	4.121408
1.047293	179.703400	4.126413
1.239466	166.819553	4.131418
0.789206	176.491360	4.136422
0.666297	180.925354	4.141427
1.470858	191.329869	4.146432
1.279103	195.600034	4.151437
1.541033	204.184605	4.156442
1.351046	191.718637	4.161446
1.684455	199.673905	4.166451
1.664986	202.017763	4.171456
1.515105	203.228410	4.176461
1.591343	194.112724	4.181466
1.402887	185.717147	4.186470
1.514477	182.144691	4.191475
1.177439	183.530779	4.196480
1.263579	205.101713	4.201485
1.642332	207.932758	4.206490
1.437612	206.606262	4.211494
1.302774	199.721679	4.216499
1.601858	202.813375	4.221504
1.622038	205.788655	4.226509
1.684480	199.684622	4.231514
1.561593	201.849257	4.236518
1.618565	204.033639	4.241523
1.866460	197.141719	4.246528
1.424047	198.116053	4.251533
1.732876	195.707969	4.256538
1.647577	206.417726	4.261542
1.464452	204.321991	4.266547
1.691436	196.843894	4.271552
1.528586	203.006263	4.276557
1.690882	188.425128	4.281562
1.579181	201.117937	4.286566
1.686588	197.175376	4.291571
1.724338	204.841178	4.296576
1.526130	206.427267	4.301581
1.761132	202.456865	4.306586
1.377081	203.505403	4.311590
1.275848	198.101193	4.316595
1.436837	195.404222	4.321600
1.350015	204.587247	4.326605
1.763603	202.885048	4.331610
1.899221	213.708793	4.336614
1.769079	219.197375	4.341619
1.873547	212.997576	4.346624
1.651318	221.266478	4.351629
2.091325	223.626011	4.356634
1.990158	226.109697	4.361638
1.387002	222.061811	4.366643
1.576090	225.674145	4.371648
1.367168	221.129596	4.376653
1.812765	220.451400	4.381658
1.717272	230.631239	4.386662
1.956649	226.742001	4.391667
2.001956	228.388209	4.396672
1.682988	234.343981	4.401677
1.928554	229.384353	4.406682
1.959530	228.781330	4.411686
2.243134	229.131046	4.416691
2.208500	218.029167	4.421696
1.626646	228.351708	4.426701
2.052335	219.497428	4.431706
1.963025	228.617929	4.436710
2.101917	222.659095	4.441715
2.106507	229.765625	4.446720
1.837641	222.750686	4.451725
2.190861	230.085422	4.456730
2.333162	248.355945	4.461734
2.409474	242.963956	4.466739
2.249113	229.059995	4.471744
1.718926	234.583454	4.476749
2.078500	231.970414	4.481754
2.265480	248.362989	4.486758
2.513642	248.097557	4.491763
2.370562	232.612041	4.496768
2.078787	234.427145	4.501773
1.900793	234.458827	4.506778
2.203108	240.965096	4.511782
2.370796	256.554954	4.516787
2.370374	256.559400	4.521792
2.304510	256.672168	4.526797
2.533409	252.684017	4.531802
2.207542	243.850976	4.536806
2.258448	238.612184	4.541811
2.495312	240.767570	4.546816
2.543953	241.196848	4.551821
2.526989	232.396920	4.556826
2.432896	231.509330	4.561830
2.140755	225.251870	4.566835
1.829241	231.095109	4.571840
2.180596	246.367022	4.576845
2.422927	248.866053	4.581850
2.246706	258.353999	4.586854
2.415307	254.348206	4.591859
2.463989	260.147791	4.596864
2.037625	257.570573	4.601869
2.527485	255.326284	4.606874
2.466852	264.448175	4.611878
2.644627	264.436136	4.616883
2.526733	254.240770	4.621888
2.480810	261.842311	4.626893
2.922827	252.533408	4.631898
2.666794	262.494959	4.636902
2.656213	262.236065	4.641907
2.572428	260.747258	4.646912
2.138155	260.887291	4.651917
2.682118	254.627718	4.656922
2.714732	263.046646	4.661926
2.944039	260.678361	4.666931
2.778421	258.571629	4.671936
2.512249	266.323707	4.676941
2.629976	257.608021	4.681946
2.393746	265.363034	4.686950
2.819759	261.771248	4.691955
2.760337	266.820901	4.696960
2.289179	258.945708	4.701965
2.770565	258.360646	4.706970
2.589919	259.855425	4.711974
2.724788	259.992968	4.716979
2.677101	261.958873	4.721984
2.746049	267.404635	4.726989
2.732560	255.257686	4.731994
2.484739	262.682302	4.736998
2.820293	280.490469	4.742003
2.916692	287.795538	4.747008
3.198216	286.826008	4.752013
3.057240	280.931259	4.757018
2.585862	273.068527	4.762022
2.542886	269.175124	4.767027
2.890010	279.678146	4.772032
2.637529	287.772123	4.777037
2.933631	287.717598	4.782042
2.703214	290.497786	4.787046
3.219699	298.078237	4.792051
3.412763	295.669575	4.797056
3.127664	296.950771	4.802061
3.002106	290.060861	4.807066
3.076212	284.496947	4.812070
3.378299	282.404718	4.817075
3.017629	267.191807	4.822080
2.826477	273.421051	4.827085
2.818569	264.320443	4.832090
2.753295	280.792123	4.837094
2.954902	288.442277	4.842099
3.171720	286.465994	4.847104
2.987483	301.707268	4.852109
3.507490	287.659208	4.857114
3.221859	295.816498	4.862118
3.020704	294.837112	4.867123
3.232781	298.445459	4.872128
2.993032	292.360648	4.877133
3.222889	290.437460	4.882138
3.144377	293.099745	4.887142
3.294717	292.801374	4.892147
3.406093	291.153358	4.897152
3.079526	290.087784	4.902157
3.263395	290.427574	4.907162
3.154138	291.748126	4.912166
2.956593	290.730253	4.917171
3.187590	296.664437	4.922176
2.976993	292.418123	4.927181
3.031685	292.625382	4.932186
3.201946	298.886547	4.937190
2.925470	296.050854	4.942195
2.925992	291.110078	4.947200
3.103116	306.781306	4.952205
3.493316	317.837263	4.957210
3.399175	325.328418	4.962214
3.520364	318.716728	4.967219
3.444049	324.759830	4.972224
3.300174	325.813398	4.977229
3.401132	323.656591	4.982234
3.307515	323.005524	4.987238
2.992577	324.129453	4.992243
3.512159	327.337596	4.997248
3.052995	329.403225	5.002253
3.297550	329.172726	5.007258
3.119082	333.118279	5.012262
3.302547	339.501991	5.017267
3.192967	331.086760	5.022272
3.348135	337.851677	5.027277
3.342944	348.596220	5.032282
3.645625	346.882180	5.037286
3.639731	362.206462	5.042291
3.902889	360.309719	5.047296
3.650996	360.801201	5.052301
3.699769	346.016121	5.057306
3.556854	337.946222	5.062310
3.419337	348.216966	5.067315
3.859906	345.259953	5.072320
3.613242	356.679324	5.077325
3.670201	349.618658	5.082330
3.297850	359.771810	5.087334
3.580257	361.297860	5.092339
3.866097	355.388050	5.097344
4.042719	362.876023	5.102349
3.577378	357.044828	5.107354
3.704164	364.958226	5.112358
3.830794	358.730427	5.117363
3.851009	360.055395	5.122368
3.484500	363.592821	5.127373
3.789632	357.526287	5.132378
3.511125	356.488271	5.137382
3.841845	357.021604	5.142387
3.988225	357.293406	5.147392
3.760423	363.457319	5.152397
3.860542	355.861821	5.157402
3.731968	359.292354	5.162406
3.848921	358.779875	5.167411
3.797837	351.515884	5.172416
3.630898	363.232273	5.177421
3.868498	353.732196	5.182426
3.719904	355.543928	5.187430
3.810383	356.165592	5.192435
3.929956	359.351774	5.197440
3.831619	367.129784	5.202445
3.980860	354.759655	5.207450
3.932791	367.527905	5.212454
4.354374	363.305940	5.217459
4.092720	362.611460	5.222464
3.879990	361.593729	5.227469
4.103736	358.069162	5.232474
4.236304	355.304842	5.237478
3.956643	362.403448	5.242483
3.925920	365.184916	5.247488
4.043484	368.539565	5.252493
4.286138	370.234411	5.257498
3.998003	369.083729	5.262502
4.353091	374.553383	5.267507
4.223637	366.855195	5.272512
4.000251	367.287097	5.277517
4.445467	368.154113	5.282522
4.160279	366.693320	5.287526
3.915148	374.831315	5.292531
4.353563	373.221880	5.297536
4.118721	379.189627	5.302541
4.189665	391.197381	5.307546
4.407866	392.879308	5.312550
4.315765	384.818336	5.317555
4.737356	384.419198	5.322560
3.910511	387.634042	5.327565
4.019210	368.317607	5.332570
4.013018	390.483079	5.337574
4.281202	396.946718	5.342579
4.628911	383.884195	5.347584
4.579906	403.502234	5.352589
4.308383	391.880204	5.357594
4.666229	392.852466	5.362598
4.555162	394.356456	5.367603
4.774896	371.990711	5.372608
3.969483	367.333550	5.377613
4.179712	368.632183	5.382618
4.288542	389.374152	5.387622
4.284191	388.942146	5.392627
4.443592	381.945803	5.397632
4.473170	391.130186	5.402637
4.326196	390.488939	5.407642
4.615688	388.631640	5.412646
4.629565	381.987768	5.417651
4.504739	389.962383	5.422656
4.420287	398.747691	5.427661
4.545849	392.541565	5.432666
4.684559	391.016097	5.437670
4.483726	399.449091	5.442675
4.716130	387.599358	5.447680
4.458955	395.134319	5.452685
4.761934	393.611446	5.457690
4.436322	387.898393	5.462694
4.322485	392.641555	5.467699
4.617156	389.967011	5.472704
4.480723	392.203971	5.477709
4.645907	392.741236	5.482714
4.713010	392.996961	5.487718
4.433187	389.476448	5.492723
4.568108	385.064354	5.497728
4.486889	388.632688	5.502733
4.525061	386.394113	5.507738
4.590307	404.479257	5.512742
4.771062	413.693872	5.517747
5.002712	414.169810	5.522752
4.885153	412.091014	5.527757
5.044473	412.247598	5.532762
4.555287	406.757189	5.537766
4.880146	412.659889	5.542771
4.809659	413.385765	5.547776
4.788866	420.611239	5.552781
5.149950	414.762357	5.557786
5.158448	420.422231	5.562790
4.869311	403.853662	5.567795
4.893930	395.311584	5.572800
4.418967	405.015052	5.577805
4.650820	408.058525	5.582810
4.735589	414.775341	5.587814
5.095363	419.536381	5.592819
5.040842	419.396652	5.597824
5.022831	418.892510	5.602829
5.228476	412.121750	5.607834
5.224352	410.066992	5.612838
4.929712	414.936798	5.617843
5.182801	412.004702	5.622848
4.977799	421.003773	5.627853
5.198341	409.874497	5.632858
5.342657	416.150663	5.637862
5.027687	414.441217	5.642867
5.235875	408.609763	5.647872
4.977982	416.911119	5.652877
5.191286	408.760288	5.657882
5.089580	418.447341	5.662886
5.373153	412.141038	5.667891
5.058201	407.529137	5.672896
4.989575	408.310749	5.677901
4.859160	408.778563	5.682906
4.988011	418.037692	5.687910
4.779628	415.863426	5.692915
4.854910	414.590200	5.697920
4.942361	424.911160	5.702925
5.101229	417.764912	5.707930
4.990122	423.803159	5.712934
4.911137	420.471978	5.717939
5.348943	427.457918	5.722944
5.153063	448.834549	5.727949
5.528739	452.828476	5.732954
5.560325	458.332195	5.737958
5.148436	445.632217	5.742963
5.268393	441.209562	5.747968
4.965928	460.811630	5.752973
5.454810	455.270533	5.757978
5.578880	459.312837	5.762982
5.029834	453.136901	5.767987
5.464695	455.959293	5.772992
5.226656	457.821766	5.777997
5.141825	456.957691	5.783002
5.074519	459.573747	5.788006
4.982174	457.314151	5.793011
5.390733	450.783678	5.798016
5.080568	455.851433	5.803021
5.350624	457.564642	5.808026
5.323249	478.278570	5.813030
5.284483	478.868952	5.818035
5.501596	478.047623	5.823040
5.524548	486.408676	5.828045
5.500119	482.528329	5.833050
5.673124	484.636702	5.838054
5.415916	480.715771	5.843059
5.726899	483.363120	5.848064
5.577525	494.024090	5.853069
5.681498	497.204990	5.858074
5.619639	493.164680	5.863078
5.243116	494.615153	5.868083
5.833107	496.912990	5.873088
5.539462	494.840845	5.878093
5.741945	493.822033	5.883098
5.432705	487.263198	5.888102
5.410270	493.142730	5.893107
5.745347	488.678319	5.898112
5.644800	495.011050	5.903117
5.774819	492.596814	5.908122
5.777886	498.498173	5.913126
5.924516	497.114651	5.918131
6.033745	495.207665	5.923136
5.816837	493.488286	5.928141
6.005132	473.389901	5.933146
5.641027	489.890964	5.938150
5.805803	487.214234	5.943155
5.948577	491.992485	5.948160
5.530693	498.599974	5.953165
5.646564	495.256243	5.958170
5.776061	496.826771	5.963174
5.598322	480.812153	5.968179
5.674691	493.228369	5.973184
5.688647	514.581393	5.978189
6.277868	517.088540	5.983194
5.957090	524.814268	5.988198
5.872237	527.816080	5.993203
6.296769	507.951846	5.998208
6.068356	518.231242	6.003213
6.236940	495.408266	6.008218
5.983026	493.843217	6.013222
5.718962	491.683490	6.018227
5.709869	491.086303	6.023232
5.486634	503.747509	6.028237
6.013606	520.692665	6.033242
6.019877	524.614185	6.038246
5.829129	526.393253	6.043251
6.149534	522.753183	6.048256
6.047917	537.096529	6.053261
5.964962	527.637195	6.058266
6.243836	520.786376	6.063270
5.926411	517.042160	6.068275
5.893565	503.549800	6.073280
5.761416	517.506465	6.078285
6.319234	515.513940	6.083290
5.997885	501.421097	6.088294
5.806923	497.132007	6.093299
6.011828	504.265284	6.098304
5.749692	506.532747	6.103309
5.848942	506.326901	6.108314
6.044957	517.983102	6.113318
6.081957	537.330527	6.118323
6.348741	523.556458	6.123328
5.765210	511.156785	6.128333
6.098681	493.470491	6.133338
5.969703	496.551436	6.138342
5.775305	491.080262	6.143347
5.848325	500.262054	6.148352
6.118219	514.684362	6.153357
6.145545	505.874774	6.158362
6.032103	498.516253	6.163366
5.891937	507.046217	6.168371
6.400576	493.940572	6.173376
6.282114	495.466319	6.178381
6.350551	490.825636	6.183386
6.299599	491.027699	6.188390
6.099424	496.224467	6.193395
6.330434	487.448057	6.198400
6.090084	490.893973	6.203405
5.863029	494.962661	6.208410
6.082771	493.673793	6.213414
5.934499	488.925926	6.218419
6.053914	495.228942	6.223424
6.122783	489.295613	6.228429
6.299989	485.996390	6.233434
5.885477	469.600266	6.238438
5.792203	469.067737	6.243443
5.758619	468.515258	6.248448
5.925284	490.134430	6.253453
5.853107	493.738982	6.258458
6.544732	493.495424	6.263462
5.999974	472.511412	6.268467
6.180868	466.181636	6.273472
5.860298	464.967446	6.278477
5.750351	460.301255	6.283482
5.825142	462.965611	6.288486
5.626691	470.025953	6.293491
6.174621	478.221721	6.298496
6.298666	477.829822	6.303501
6.145976	468.592041	6.308506
6.209218	457.444182	6.313510
5.690351	466.247002	6.318515
5.866407	453.508263	6.323520
5.927166	457.624594	6.328525
5.989075	451.052265	6.333530
6.067011	463.970426	6.338534
5.324962	465.220152	6.343539
5.822779	470.426239	6.348544
5.917595	491.954498	6.353549
6.128326	484.828443	6.358554
5.980917	490.594676	6.363558
6.112732	497.600140	6.368563
6.286126	487.297378	6.373568
6.122396	478.172522	6.378573
5.926877	465.132794	6.383578
6.226896	463.626784	6.388582
5.714256	464.271564	6.393587
5.983847	453.271680	6.398592
5.547604	459.898374	6.403597
5.758344	463.621241	6.408602
5.824042	486.134892	6.413606
5.945968	492.147796	6.418611
6.378406	488.420309	6.423616
6.243143	465.878581	6.428621
5.964886	464.454322	6.433626
5.643998	464.360282	6.438630
5.877398	464.423098	6.443635
6.235697	469.506851	6.448640
6.150012	465.462994	6.453645
5.782190	463.633433	6.458650
5.929674	452.648442	6.463654
5.907330	457.431332	6.468659
6.246773	457.217876	6.473664
5.933614	464.262874	6.478669
5.737859	461.486600	6.483674
5.852268	459.719463	6.488678
5.858550	470.013638	6.493683
6.138259	457.424087	6.498688
5.887353	457.373121	6.503693
5.949912	460.998767	6.508698
6.408176	456.483576	6.513702
6.186356	468.275832	6.518707
5.976869	455.951214	6.523712
5.677388	466.557298	6.528717
5.857271	460.161386	6.533722
6.092175	454.110984	6.538726
5.984009	463.680337	6.543731
5.991644	462.339175	6.548736
5.494557	464.662511	6.553741
5.978389	462.301973	6.558746
5.700615	466.536333	6.563750
6.104087	481.455886	6.568755
6.325720	461.326540	6.573760
5.991722	463.203325	6.578765
6.091467	467.038901	6.583770
5.577169	465.085592	6.588774
5.606539	468.834548	6.593779
5.921459	486.605521	6.598784
5.992050	494.995592	6.603789
5.970442	493.870819	6.608794
5.995478	501.630439	6.613798
5.652242	506.642117	6.618803
6.072157	501.119726	6.623808
5.705398	503.112057	6.628813
5.938107	498.470216	6.633818
5.878254	501.295211	6.638822
6.049941	497.094071	6.643827
6.090262	496.072117	6.648832
5.907649	497.985802	6.653837
5.950483	500.825169	6.658842
6.324540	501.204511	6.663846
5.941649	497.603359	6.668851
6.399532	498.457235	6.673856
5.952746	485.589147	6.678861
6.025926	464.177599	6.683866
6.135953	467.131735	6.688870
5.762304	470.936382	6.693875
6.027723	465.938659	6.698880
5.696064	463.952539	6.703885
5.980230	473.684065	6.708890
5.830216	482.119147	6.713894
5.585055	481.352664	6.718899
5.750963	487.503129	6.723904
5.796428	497.219339	6.728909
6.360800	502.869678	6.733914
6.269732	500.592103	6.738918
5.911970	492.145263	6.743923
5.812436	488.636905	6.748928
5.960824	494.495253	6.753933
6.029122	489.744872	6.758938
6.317599	500.612770	6.763942
5.964555	481.823974	6.768947
5.597667	470.272340	6.773952
5.693272	478.144980	6.778957
5.817244	495.755968	6.783962
5.999598	492.005760	6.788966
6.067359	502.127364	6.793971
6.270531	498.467838	6.798976
5.907642	505.458928	6.803981
6.150086	494.693608	6.808986
6.190236	499.364533	6.813990
5.925629	493.552535	6.818995
6.031616	478.346598	6.824000
5.677366	479.916917	6.829005
5.715685	488.958615	6.834010
5.646232	502.176306	6.839014
5.992883	505.097777	6.844019
6.216186	499.371139	6.849024
5.925705	502.729451	6.854029
6.041010	504.717336	6.859034
6.023378	498.526987	6.864038
5.878474	502.095236	6.869043
6.077933	496.711577	6.874048
5.845988	502.758222	6.879053
5.916724	507.733710	6.884058
5.805563	507.143953	6.889062
5.914960	501.147666	6.894067
6.285243	499.257045	6.899072
5.563310	503.256723	6.904077
5.840827	497.500190	6.909082
5.967436	505.046441	6.914086
5.727231	512.424921	6.919091
5.947924	501.388305	6.924096
5.869329	506.730116	6.929101
5.900543	504.810986	6.934106
6.232717	504.746738	6.939110
6.149216	505.380839	6.944115
6.096775	502.406574	6.949120
6.123835	506.461403	6.954125
6.186441	501.388916	6.959130
5.862225	506.657340	6.964134
5.845018	501.420662	6.969139
5.884366	502.832658	6.974144
5.656344	509.645912	6.979149
5.783731	500.994007	6.984154
5.993936	498.819677	6.989158
5.891105	495.193460	6.994163
6.049718	490.350765	6.999168
5.982103	495.991302	7.004173
5.594990	495.913754	7.009178
6.083502	490.935913	7.014182
5.737739	496.261184	7.019187
6.080810	496.299524	7.024192
5.900234	498.640506	7.029197
5.918690	496.880374	7.034202
6.245295	507.170665	7.039206
5.908300	505.282712	7.044211
5.919488	496.961059	7.049216
6.105111	507.110116	7.054221
6.031638	493.188174	7.059226
5.985108	502.666238	7.064230
5.889504	501.190218	7.069235
6.003295	503.554482	7.074240
5.812704	516.276598	7.079245
5.765577	509.725459	7.084250
5.577973	505.462846	7.089254
5.487831	507.212424	7.094259
6.133328	503.051222	7.099264
5.671052	510.460162	7.104269
6.212097	504.485142	7.109274
6.118997	501.451304	7.114278
6.395839	507.264112	7.119283
5.929239	499.496774	7.124288
5.780964	501.143495	7.129293
5.562916	501.151617	7.134298
5.796605	497.580970	7.139302
5.905829	498.876804	7.144307
6.187446	500.010689	7.149312
5.934668	505.671829	7.154317
5.983600	498.312665	7.159322
6.124921	492.195060	7.164326
5.664352	502.767854	7.169331
6.171595	503.917459	7.174336
5.886052	516.088737	7.179341
5.831657	506.490101	7.184346
6.136149	500.442562	7.189350
5.478721	505.115340	7.194355
6.078007	497.483683	7.199360
5.979841	498.930686	7.204365
6.232587	500.993098	7.209370
6.002179	498.321423	7.214374
5.763753	503.645300	7.219379
6.234265	505.491479	7.224384
6.281824	500.533770	7.229389
6.109179	495.651010	7.234394
5.783110	507.880104	7.239398
5.854600	501.487719	7.244403
5.835961	505.130769	7.249408
5.926484	501.852804	7.254413
5.998378	499.641387	7.259418
6.172647	494.403985	7.264422
6.074665	506.434672	7.269427
6.367419	509.224957	7.274432
5.958511	503.507895	7.279437
6.022318	507.798972	7.284442
6.020404	503.993630	7.289446
5.979584	509.612962	7.294451
6.308694	500.451866	7.299456
6.103120	498.812505	7.304461
6.060172	507.017138	7.309466
6.097360	509.465131	7.314470
6.019864	507.709442	7.319475
6.210927	499.072253	7.324480
6.148886	506.811169	7.329485
5.974448	488.668676	7.334490
5.877395	474.691059	7.339494
5.499192	486.034033	7.344499
6.023034	486.953750	7.349504
6.036876	499.214166	7.354509
6.101762	503.148274	7.359514
6.272540	491.696834	7.364518
5.863434	495.227530	7.369523
5.818756	474.740485	7.374528
5.952960	487.391819	7.379533
5.753728	491.482146	7.384538
6.287737	493.292549	7.389542
5.962471	492.163399	7.394547
6.116852	474.563815	7.399552
5.802355	469.259357	7.404557
5.815906	474.293244	7.409562
5.564169	488.921499	7.414566
5.760785	497.749318	7.419571
6.125362	497.794161	7.424576
5.895014	500.461694	7.429581
5.837511	499.727874	7.434586
5.928286	507.888063	7.439590
5.885169	505.486117	7.444595
6.132909	498.199607	7.449600
6.133169	498.447655	7.454605
5.857534	492.731615	7.459610
5.969457	501.122146	7.464614
5.974645	498.377119	7.469619
6.014711	498.061881	7.474624
5.609574	502.928107	7.479629
6.196884	505.133836	7.484634
6.282351	499.931266	7.489638
5.647656	506.265037	7.494643
5.751196	499.238424	7.499648
5.309803	505.361591	7.504653
5.692674	499.732063	7.509658
5.757068	502.175746	7.514662
5.710977	504.278569	7.519667
5.901201	494.993458	7.524672
5.595831	497.268473	7.529677
5.969534	501.378183	7.534682
5.692356	507.904554	7.539686
5.623458	530.824779	7.544691
5.952932	529.418474	7.549696
5.933318	532.941315	7.554701
6.212391	533.136877	7.559706
6.197918	529.508255	7.564710
6.265386	532.725401	7.569715
6.111583	508.559219	7.574720
5.857133	509.725635	7.579725
5.891097	508.111728	7.584730
6.240934	508.443378	7.589734
5.905671	505.847281	7.594739
5.951146	501.489632	7.599744
5.759865	502.797736	7.604749
6.035099	501.780492	7.609754
6.047275	497.074332	7.614758
6.261006	499.781598	7.619763
6.457483	492.845569	7.624768
5.879763	497.841807	7.629773
5.825843	496.469789	7.634778
5.853530	490.947629	7.639782
5.959289	505.800866	7.644787
6.125185	489.286109	7.649792
5.852930	497.618302	7.654797
5.864713	496.384593	7.659802
5.920300	495.557451	7.664806
5.956868	495.110377	7.669811
6.237040	496.835730	7.674816
5.989862	499.762591	7.679821
6.014707	503.019745	7.684826
6.293680	498.893785	7.689830
5.936936	494.656816	7.694835
6.169784	500.667537	7.699840
5.942808	511.326766	7.704845
5.920855	504.654438	7.709850
6.108233	493.292997	7.714854
5.861023	498.505844	7.719859
6.037998	494.599048	7.724864
5.723133	502.632820	7.729869
6.037936	488.629217	7.734874
6.208165	499.737125	7.739878
5.952202	506.069944	7.744883
5.991333	491.516025	7.749888
5.944922	494.103959	7.754893
5.956044	504.733030	7.759898
5.929219	500.011225	7.764902
5.988983	494.452572	7.769907
6.232210	495.282004	7.774912
6.023249	496.219076	7.779917
5.929962	488.996150	7.784922
5.771415	501.093301	7.789926
5.545747	499.547650	7.794931
5.531043	500.103460	7.799936
5.757373	502.251353	7.804941
5.529839	503.533097	7.809946
5.521988	494.345515	7.814950
5.775593	510.122489	7.819955
6.114830	521.722218	7.824960
5.978797	539.006892	7.829965
6.008308	542.543110	7.834970
6.405255	524.853374	7.839974
6.170876	520.849124	7.844979
6.135521	510.519149	7.849984
5.990634	507.032505	7.854989
5.967646	501.927818	7.859994
6.080137	497.315358	7.864998
6.119654	508.056356	7.870003
6.350657	500.250062	7.875008
6.043032	498.910783	7.880013
6.214223	498.015951	7.885018
5.926312	498.439400	7.890022
5.808468	505.738806	7.895027
6.203917	498.946444	7.900032
5.631325	501.924432	7.905037
5.882650	507.737124	7.910042
6.423932	500.766291	7.915046
6.234128	516.129469	7.920051
6.305785	500.539252	7.925056
5.951531	501.795409	7.930061
5.734319	505.649146	7.935066
6.024897	502.469677	7.940070
5.905616	505.876602	7.945075
6.005298	503.418052	7.950080
5.884244	500.883179	7.955085
5.730868	502.589157	7.960090
6.109687	503.100718	7.965094
5.508032	511.774005	7.970099
5.608009	500.880322	7.975104
5.840899	507.146988	7.980109
5.604611	506.356142	7.985114
6.208008	500.163987	7.990118
5.928072	508.703671	7.995136
6.406708	505.342987	8.000154
6.057582	499.559529	8.005171
6.198463	507.601005	8.010189
5.942473	506.663976	8.015206
6.046857	512.638617	8.020224
6.351690	502.045822	8.025242
6.036888	519.468394	8.030259
5.981385	516.565821	8.035277
6.001968	509.924341	8.040294
5.890048	505.498545	8.045312
5.662311	506.372061	8.050330
5.770042	504.407152	8.055347
6.091041	507.881531	8.060365
6.071945	505.269760	8.065382
5.923407	518.082846	8.070400
6.258231	501.885878	8.075418
6.271093	504.393444	8.080435
5.906392	509.142316	8.085453
6.332520	501.841991	8.090470
6.345854	505.865906	8.095488
6.215301	500.032472	8.100506
5.930586	506.287672	8.105523
6.300096	501.274709	8.110541
6.243891	501.666702	8.115558
6.202930	510.513434	8.120576
6.089336	490.458343	8.125594
6.039691	490.790788	8.130611
5.666591	492.011777	8.135629
6.194456	505.526755	8.140646
6.084323	509.867355	8.145664
6.191100	507.754584	8.150682
5.961495	505.721335	8.155699
5.909468	515.079904	8.160717
6.049701	512.311441	8.165734
6.048105	513.779352	8.170752
6.357346	503.519069	8.175770
6.393495	512.173518	8.180787
6.002042	509.332485	8.185805
6.444999	508.721213	8.190822
6.369275	516.698178	8.195840
6.495663	509.411662	8.200858
6.091754	497.716444	8.205875
6.299206	492.852162	8.210893
6.129742	484.468279	8.215910
5.841015	493.296784	8.220928
6.021834	493.410172	8.225946
6.246722	509.612143	8.230963
6.065079	509.484003	8.235981
6.060309	515.122613	8.240998
6.260275	519.689205	8.246016
6.270634	507.185272	8.251034
6.062975	510.143894	8.256051
5.664711	512.205409	8.261069
6.210490	502.402574	8.266086
5.913942	523.079962	8.271104
6.045296	509.543858	8.276122
5.978359	508.031465	8.281139
6.094876	516.337986	8.286157
6.122101	515.886695	8.291174
5.840261	532.125954	8.296192
6.348891	533.992803	8.301210
6.200985	530.869522	8.306227
6.182507	555.047899	8.311245
6.602870	536.087314	8.316262
6.005501	553.953738	8.321280
6.068081	543.275253	8.326298
6.351917	545.374789	8.331315
6.119580	546.844302	8.336333
6.385978	546.363441	8.341350
6.040911	551.639549	8.346368
6.154230	541.526836	8.351386
6.348559	539.655055	8.356403
6.085007	547.306866	8.361421
6.374290	538.922963	8.366438
6.107680	547.702761	8.371456
6.524236	549.806695	8.376474
6.519381	546.333563	8.381491
6.299491	549.338310	8.386509
6.445580	541.203104	8.391526
6.454347	547.683716	8.396544
6.329703	545.327392	8.401562
6.552658	544.700390	8.406579
6.479637	545.394753	8.411597
6.808632	536.436599	8.416614
6.589285	545.630980	8.421632
6.032269	543.785597	8.426650
6.548687	540.545609	8.431667
6.360565	546.408674	8.436685
6.358362	534.455186	8.441702
6.028388	538.852474	8.446720
6.297650	542.955071	8.451738
6.400546	544.492879	8.456755
6.196535	538.417677	8.461773
6.745724	536.516263	8.466790
6.300465	547.635719	8.471808
6.494072	545.901843	8.476826
6.443931	541.567571	8.481843
6.278278	546.849397	8.486861
6.276501	544.767195	8.491878
6.532629	555.705156	8.496896
6.532088	539.000931	8.501914
6.366014	536.317241	8.506931
6.367414	545.673083	8.511949
6.626364	542.774924	8.516966
6.417372	551.258194	8.521984
6.556571	564.715943	8.527002
6.684768	556.919298	8.532019
6.296493	560.735146	8.537037
6.678173	563.736725	8.542054
6.427521	568.733048	8.547072
6.813355	560.977786	8.552090
6.724567	548.592003	8.557107
6.159141	551.522878	8.562125
6.220048	552.622593	8.567143
6.649527	561.917791	8.572160
6.365065	577.985890	8.577178
6.690227	577.386053	8.582195
6.381990	574.023190	8.587213
6.482009	575.140247	8.592231
6.484509	582.193526	8.597248
6.385701	575.747368	8.602266
6.605997	572.775294	8.607283
6.268679	579.376810	8.612301
6.707529	575.110754	8.617319
6.577883	567.904010	8.622336
6.659938	570.104283	8.627354
6.759646	573.603906	8.632371
6.328560	576.953061	8.637389
6.638356	560.434805	8.642407
6.574170	577.699019	8.647424
6.700740	578.422926	8.652442
6.833310	570.375764	8.657459
6.587212	578.032770	8.662477
6.440616	576.429436	8.667495
6.914082	572.301143	8.672512
6.720869	573.766738	8.677530
6.700006	565.864271	8.682547
6.743547	575.110010	8.687565
6.643629	572.258676	8.692583
6.788333	578.332367	8.697600
6.605813	572.520110	8.702618
6.929104	571.249762	8.707635
6.392468	568.163093	8.712653
6.569204	566.178286	8.717671
6.434661	569.259448	8.722688
6.569110	565.374884	8.727706
6.752841	572.231229	8.732723
6.563085	595.548526	8.737741
6.621063	599.492241	8.742759
7.040788	605.720977	8.747776
7.046861	604.491741	8.752794
6.987830	577.933638	8.757811
6.596543	579.938498	8.762829
6.749231	573.277870	8.767847
6.852370	585.282062	8.772864
6.746037	585.457963	8.777882
7.022582	580.759562	8.782899
6.744774	584.832694	8.787917
6.683088	576.638380	8.792935
6.829351	589.592652	8.797952
6.843437	598.850566	8.802970
7.142566	606.781642	8.807987
7.062858	589.561766	8.813005
7.064857	578.889352	8.818023
7.027427	577.604728	8.823040
6.908173	580.784142	8.828058
6.846721	567.136224	8.833075
6.772357	573.689862	8.838093
6.708396	579.140279	8.843111
6.999381	580.925862	8.848128
6.673541	577.782828	8.853146
6.818151	568.064298	8.858163
6.609980	578.490228	8.863181
6.803105	586.729773	8.868199
7.108361	603.224221	8.873216
6.844938	608.129765	8.878234
7.232485	593.318959	8.883251
6.955659	582.519499	8.888269
6.662761	572.170710	8.893287
6.910741	574.101003	8.898304
7.143745	599.362136	8.903322
7.266940	592.770947	8.908339
7.123316	578.378410	8.913357
6.983567	577.873671	8.918375
6.859889	568.953652	8.923392
7.022846	574.142686	8.928410
7.056645	567.235231	8.933427
6.746566	573.674764	8.938445
6.724520	565.334924	8.943463
6.885393	576.230804	8.948480
7.075915	595.743649	8.953498
7.289335	602.554936	8.958515
7.223023	598.501064	8.963533
6.903192	581.472133	8.968551
6.956557	572.328122	8.973568
6.899458	591.283582	8.978586
7.135840	597.402725	8.983603
7.214733	612.682193	8.988621
7.197591	598.823183	8.993639
7.015186	588.692093	8.998656
6.865058	586.066183	9.003674
7.281606	589.461376	9.008691
7.213492	597.380236	9.013709
7.031407	589.314310	9.018727
7.003803	577.283702	9.023744
6.921859	590.222226	9.028762
7.345653	596.661294	9.033779
6.935224	604.083535	9.038797
7.030702	599.013762	9.043815
7.043759	598.358135	9.048832
7.231034	610.681069	9.053850
7.402182	593.899537	9.058867
7.363294	602.472177	9.063885
6.791366	592.304022	9.068903
7.426803	597.404388	9.073920
7.175596	600.052544	9.078938
7.118833	587.904717	9.083955
7.106408	585.383357	9.088973
6.936922	599.339468	9.093991
7.174355	597.811307	9.099008
7.122453	605.068868	9.104026
7.404742	603.140391	9.109043
7.336531	604.194370	9.114061
7.331489	603.872033	9.119079
7.431760	595.683563	9.124096
7.116024	586.791205	9.129114
7.448657	582.521872	9.134131
7.031136	585.711706	9.139149
6.963876	591.698465	9.144167
7.203570	594.074787	9.149184
7.307961	601.315716	9.154202
7.422591	602.602391	9.159219
7.275844	599.634209	9.164237
7.361881	607.594275	9.169255
7.316174	595.267457	9.174272
7.090945	599.029938	9.179290
7.266060	597.588863	9.184307
7.275364	606.444647	9.189325
7.322200	602.731265	9.194343
7.302019	600.487940	9.199360
7.059936	602.697213	9.204378
7.272459	605.449075	9.209395
7.472205	610.032659	9.214413
7.242613	603.194985	9.219431
7.227424	606.136713	9.224448
7.204428	613.258004	9.229466
7.191575	597.043715	9.234483
7.149037	599.673849	9.239501
6.950191	606.487469	9.244519
7.317879	598.501941	9.249536
6.985003	602.194262	9.254554
7.351143	601.652593	9.259571
7.556837	613.796310	9.264589
7.264256	616.986719	9.269607
7.544652	614.103103	9.274624
7.248693	622.412243	9.279642
7.461225	627.381879	9.284659
7.727235	628.767298	9.289677
7.626960	624.542874	9.294695
7.201600	604.553239	9.299712
7.451454	611.612811	9.304730
7.471021	608.104717	9.309747
7.711796	606.612613	9.314765
7.720778	602.252196	9.319783
7.614989	599.689803	9.324800
7.233664	601.895364	9.329818
7.278022	612.452911	9.334835
7.450265	607.078317	9.339853
7.399575	613.455227	9.344871
7.633899	608.672084	9.349888
7.504508	617.968335	9.354906
7.482098	612.727935	9.359923
7.491387	610.769670	9.364941
7.590787	626.528402	9.369959
7.657930	622.004224	9.374976
7.308883	613.547260	9.379994
7.681273	628.396473	9.385011
7.609688	633.924939	9.390029
7.404212	632.616174	9.395047
7.702128	614.343248	9.400064
7.552291	630.077710	9.405082
7.517518	629.548106	9.410099
7.724683	631.813293	9.415117
7.447612	636.361680	9.420135
7.725528	635.643688	9.425152
7.459403	630.299950	9.430170
7.643182	639.635095	9.435187
7.626263	633.724136	9.440205
7.668710	640.804092	9.445223
7.886008	628.034704	9.450240
7.452221	636.109606	9.455258
7.727459	631.799374	9.460275
7.699159	628.471632	9.465293
7.377604	631.582595	9.470311
7.645212	635.327836	9.475328
7.701498	630.362175	9.480346
7.695456	631.554473	9.485363
7.951059	630.543345	9.490381
7.714581	639.239075	9.495399
7.847219	629.176842	9.500416
7.492707	635.054504	9.505434
7.576091	640.023878	9.510451
7.895874	635.784215	9.515469
7.635049	636.114433	9.520487
7.813395	625.317121	9.525504
7.658228	633.193923	9.530522
7.824875	640.759972	9.535539
7.949242	635.582260	9.540557
7.345157	639.077786	9.545575
7.685595	633.818233	9.550592
7.308406	637.086825	9.555610
7.546189	641.403112	9.560627
7.718461	629.611197	9.565645
7.357848	645.053041	9.570663
7.761012	638.770171	9.575680
7.211368	642.959787	9.580698
7.419544	653.891193	9.585715
7.912484	657.548339	9.590733
7.701812	672.397305	9.595751
8.174692	668.844049	9.600768
7.958919	668.793995	9.605786
7.571985	664.837883	9.610803
7.705510	664.266628	9.615821
7.296031	673.754759	9.620839
8.217305	657.846512	9.625856
7.848923	664.979160	9.630874
7.786944	657.547008	9.635891
7.784884	660.035419	9.640909
7.830564	664.766572	9.645927
8.286878	660.818053	9.650944
7.901065	664.722292	9.655962
7.917947	666.874911	9.660979
8.039462	649.444491	9.665997
7.963609	657.296754	9.671015
7.676134	662.630681	9.676032
7.774365	668.688089	9.681050
7.939821	668.178865	9.686067
7.885540	668.841392	9.691085
7.458901	664.809971	9.696103
7.746533	660.206751	9.701120
7.865996	677.755605	9.706138
7.674528	687.728476	9.711155
7.991592	689.521957	9.716173
8.082573	691.586722	9.721191
8.013759	682.399103	9.726208
8.397256	698.268135	9.731226
8.048355	704.247643	9.736243
8.229331	684.367719	9.741261
8.230494	701.095690	9.746279
8.272797	681.622963	9.751296
8.397845	669.676643	9.756314
8.099943	673.278942	9.761331
8.224762	659.767409	9.766349
7.865545	666.080087	9.771367
8.237242	664.132859	9.776384
8.089230	666.585995	9.781402
8.273409	660.018928	9.786419
8.541294	665.894706	9.791437
7.904379	659.852565	9.796455
8.026782	666.254373	9.801472
8.107662	663.226241	9.806490
7.974428	661.771660	9.811507
7.970762	660.001547	9.816525
7.826065	670.817789	9.821543
8.412073	668.591385	9.826560
8.275903	667.124692	9.831578
8.173228	669.404189	9.836595
8.363717	665.067828	9.841613
8.066782	666.567340	9.846631
8.320785	664.794317	9.851648
8.300339	667.415293	9.856666
8.241561	665.648794	9.861683
7.973525	658.738136	9.866701
8.292326	657.263026	9.871719
8.356482	662.045839	9.876736
8.394428	664.153633	9.881754
8.233432	665.882192	9.886771
8.622032	665.096660	9.891789
8.213759	673.710236	9.896807
8.313323	671.375028	9.901824
8.335692	669.356523	9.906842
7.896500	666.497186	9.911859
8.419687	664.483142	9.916877
8.215975	663.368952	9.921895
8.189135	666.115782	9.926912
8.231410	669.950705	9.931930
8.240253	667.712800	9.936947
8.406988	670.365767	9.941965
8.448690	684.630072	9.946983
8.134814	665.905283	9.952000
8.119619	681.283663	9.957018
8.021752	697.632384	9.962035
8.088092	699.105203	9.967053
8.357796	701.906469	9.972071
8.540413	702.805735	9.977088
8.543896	704.544854	9.982106
8.499147	701.601294	9.987123
8.619689	698.075671	9.992141
8.172409	699.183573	9.997159
8.362674	696.142832	10.002176
8.561788	693.716730	10.007194
8.165205	702.464992	10.012211
8.441528	700.337896	10.017229
8.476931	697.056674	10.022247
8.567966	692.983609	10.027264
8.699395	696.227039	10.032282
8.242648	690.006240	10.037299
8.213831	693.199438	10.042317
8.546881	696.906693	10.047335
8.478373	698.728201	10.052352
8.726333	694.639385	10.057370
8.675131	707.845932	10.062387
8.815987	695.213944	10.067405
8.612304	695.647292	10.072423
8.836573	697.815962	10.077440
8.723951	701.461990	10.082458
8.365552	700.797404	10.087475
9.037356	697.015935	10.092493
8.701361	681.845758	10.097511
8.872238	680.135709	10.102528
8.675020	674.919118	10.107546
8.554080	668.222272	10.112563
8.721030	661.626956	10.117581
8.412928	670.802646	10.122599
8.447334	667.438530	10.127616
8.441786	660.234419	10.132634
8.199190	678.197933	10.137651
8.827935	684.841075	10.142669
8.804723	690.058419	10.147687
8.619359	693.012596	10.152704
9.160529	694.669366	10.157722
8.607581	681.229504	10.162739
8.702246	672.613207	10.167757
8.265843	664.250599	10.172775
8.247982	679.208184	10.177792
8.808244	687.310218	10.182810
8.596135	693.819004	10.187827
8.420778	699.459160	10.192845
8.628192	705.492597	10.197863
8.381195	699.847653	10.202880
8.563328	691.282606	10.207898
8.556173	700.216361	10.212915
8.692841	694.248057	10.217933
8.277658	700.264129	10.222951
8.269339	697.256667	10.227968
8.710063	715.974731	10.232986
8.648084	725.113238	10.238003
8.937908	726.115217	10.243021
8.690746	728.686351	10.248039
8.711445	723.463577	10.253056
8.868832	728.169951	10.258074
8.471940	737.385579	10.263091
8.784095	724.628749	10.268109
8.549850	732.170291	10.273127
8.492741	727.876095	10.278144
9.176244	723.579327	10.283162
8.877840	739.731787	10.288179
9.004556	738.644364	10.293197
9.108699	739.250740	10.298215
8.945452	736.102006	10.303232
8.757953	721.257967	10.308250
8.774583	731.440879	10.313267
9.060745	730.342012	10.318285
8.960928	731.477803	10.323303
8.694688	739.372265	10.328320
9.072768	726.483657	10.333338
8.463356	736.450578	10.338355
9.099303	728.676057	10.343373
8.883071	737.607845	10.348391
8.772733	731.738302	10.353408
9.054891	726.506872	10.358426
8.585004	737.006955	10.363443
8.964678	729.032367	10.368461
8.877534	729.770807	10.373479
9.106002	744.379807	10.378496
9.063128	737.319235	10.383514
8.817269	736.323824	10.388531
8.997015	749.859070	10.393549
8.936131	756.701874	10.398567
8.902612	761.282402	10.403584
9.418688	760.485597	10.408602
9.004606	766.424745	10.413619
8.918439	763.770300	10.418637
9.069149	756.923317	10.423655
8.841181	751.127574	10.428672
9.206981	754.932957	10.433690
8.987315	762.693347	10.438707
9.068207	752.316393	10.443725
9.317270	753.886904	10.448743
9.239095	759.519649	10.453760
9.334624	749.913852	10.458778
9.013195	767.169305	10.463795
9.141178	761.293747	10.468813
9.161967	754.021455	10.473831
8.890656	768.642773	10.478848
9.147685	749.538317	10.483866
9.169886	760.842309	10.488883
9.075101	754.354074	10.493901
9.190639	759.048885	10.498919
8.839798	761.590740	10.503936
9.181770	754.331398	10.508954
9.248533	754.846332	10.513971
8.982026	755.494798	10.518989
9.417682	754.805007	10.524007
9.158230	755.918420	10.529024
9.212759	752.660789	10.534042
8.912113	759.781475	10.539059
9.046316	754.997742	10.544077
9.391463	754.720161	10.549095
9.208777	765.408122	10.554112
9.133066	755.834615	10.559130
9.305920	771.209107	10.564147
9.637023	775.001738	10.569165
9.557527	768.293655	10.574183
9.065344	759.031620	10.579200
9.464999	759.666221	10.584218
9.521095	763.275663	10.589235
9.366120	751.737049	10.594253
9.470333	752.556394	10.599271
9.084321	763.131970	10.604288
9.254760	756.349433	10.609306
9.836704	760.926459	10.614323
9.268687	751.832097	10.619341
9.099659	760.948197	10.624359
9.248808	775.906957	10.629376
9.584422	784.336779	10.634394
9.567229	787.764279	10.639411
9.389299	790.608983	10.644429
9.597000	786.968124	10.649447
9.215769	787.430876	10.654464
9.478384	790.457729	10.659482
9.363527	807.370373	10.664499
9.452963	793.291386	10.669517
9.487802	800.108122	10.674535
9.535563	794.674553	10.679552
9.684788	785.934992	10.684570
9.245932	795.945356	10.689587
9.360279	796.388636	10.694605
9.764677	800.354559	10.699623
9.729554	798.123916	10.704640
9.888507	792.173930	10.709658
9.659855	796.654899	10.714675
9.351835	798.375145	10.719693
9.551573	797.237044	10.724711
9.210130	799.242732	10.729728
9.667571	797.734414	10.734746
9.451329	796.162471	10.739763
9.569998	798.980498	10.744781
9.470646	804.830141	10.749799
9.141396	803.341082	10.754816
9.389365	798.920365	10.759834
9.460686	792.528222	10.764851
9.384406	792.740879	10.769869
9.355726	786.802283	10.774887
9.546153	813.157962	10.779904
9.844896	821.043151	10.784922
9.611891	830.847017	10.789939
9.579643	822.028044	10.794957
9.869729	825.821181	10.799975
9.844434	825.589985	10.804992
10.051003	815.377601	10.810010
9.764366	805.730730	10.815027
9.419161	799.732348	10.820045
9.865893	813.813563	10.825063
9.953899	810.824377	10.830080
9.652661	809.597593	10.835098
9.645757	804.129375	10.840115
9.923728	819.586109	10.845133
9.921072	820.108998	10.850151
9.748938	821.501641	10.855168
9.883655	820.721139	10.860186
9.966839	833.962622	10.865203
9.733588	811.312301	10.870221
9.897554	803.503311	10.875239
9.380904	824.617725	10.880256
9.973833	814.463401	10.885274
9.822317	822.541258	10.890291
9.847616	828.514354	10.895309
9.692888	821.382115	10.900327
9.942588	824.857153	10.905344
9.893489	813.523783	10.910362
9.799877	825.655226	10.915379
9.671957	826.346883	10.920397
9.900155	817.782406	10.925415
9.739423	829.307283	10.930432
9.966317	823.674363	10.935450
9.864730	815.381023	10.940467
9.973603	823.800780	10.945485
10.194250	824.128431	10.950503
9.947420	826.513315	10.955520
9.895265	821.086048	10.960538
9.627105	832.524785	10.965555
9.817513	833.732202	10.970573
10.051336	825.569524	10.975591
9.628432	830.848773	10.980608
10.047725	839.018324	10.985626
10.194429	850.990312	10.990643
10.018498	857.497506	10.995661
10.268914	855.745527	11.000679
10.284392	852.697482	11.005696
10.204032	830.726109	11.010714
10.110635	823.088855	11.015731
9.921743	833.937332	11.020749
9.874320	828.669506	11.025767
10.074600	845.515045	11.030784
10.355351	860.585158	11.035802
10.309467	862.865908	11.040819
10.022982	853.307955	11.045837
10.182041	851.022315	11.050855
10.499482	858.943795	11.055872
10.462336	853.084918	11.060890
10.694461	824.549928	11.065907
9.914420	839.350041	11.070925
9.899414	823.847450	11.075943
9.830166	832.845105	11.080960
9.735754	847.781279	11.085978
10.461965	847.624048	11.090995
10.117034	860.967551	11.096013
10.270032	865.315657	11.101031
10.431555	867.581746	11.106048
9.945895	857.356414	11.111066
10.553068	866.418049	11.116083
10.034081	868.123241	11.121101
10.147555	854.274064	11.126119
10.419706	871.220715	11.131136
10.549725	860.031263	11.136154
10.492130	859.658572	11.141171
10.094559	861.610572	11.146189
10.213737	855.692345	11.151207
10.466610	871.251312	11.156224
10.662244	859.761245	11.161242
10.640364	866.784637	11.166259
10.341267	869.004569	11.171277
10.694000	864.886155	11.176295
10.351844	859.682480	11.181312
10.583812	861.024742	11.186330
10.339966	861.436794	11.191347
10.371954	866.517503	11.196365
10.443698	863.946727	11.201383
10.380851	863.883552	11.206400
10.086636	864.124032	11.211418
10.366488	851.236628	11.216435
10.353930	870.588576	11.221453
10.660311	856.386995	11.226471
10.248517	867.459013	11.231488
10.051892	875.681369	11.236506
10.121040	858.879042	11.241523
10.594097	873.551198	11.246541
10.756296	867.146731	11.251559
10.565206	867.937823	11.256576
10.393442	874.823843	11.261594
10.778346	874.547944	11.266611
10.415808	873.454528	11.271629
10.768561	863.887163	11.276647
10.605429	862.794189	11.281664
10.397624	856.723033	11.286682
10.661756	866.060362	11.291699
10.486992	864.424066	11.296717
10.286271	856.862833	11.301735
10.727716	868.439980	11.306752
10.630847	890.603810	11.311770
10.736241	885.811422	11.316787
10.632053	892.294152	11.321805
10.742590	883.850693	11.326823
10.821383	896.735100	11.331840
10.632395	901.671714	11.336858
10.836465	891.103805	11.341875
10.629517	900.306184	11.346893
10.405306	897.101374	11.351911
10.961915	894.496362	11.356928
10.970206	895.325300	11.361946
10.950398	896.978144	11.366963
10.584415	900.466972	11.371981
11.047054	902.561553	11.376999
10.983754	890.754910	11.382016
10.770351	883.285524	11.387034
10.909424	874.312566	11.392051
10.775583	875.369361	11.397069
10.521993	865.366211	11.402087
10.803951	872.235752	11.407104
10.997219	885.046471	11.412122
11.091544	890.968793	11.417139
10.483649	889.384143	11.422157
10.772497	900.474403	11.427175
11.070611	893.700583	11.432192
10.645109	890.483048	11.437210
10.919328	893.780822	11.442227
10.623653	900.694066	11.447245
10.791467	900.760007	11.452263
11.016495	898.913808	11.457280
10.857580	898.761034	11.462298
11.168378	889.023444	11.467315
10.688431	902.325959	11.472333
10.760243	904.115199	11.477351
10.762083	897.827822	11.482368
10.815082	898.163159	11.487386
10.706319	892.773980	11.492403
10.447575	901.416459	11.497421
10.870694	906.341863	11.502439
10.980804	919.899812	11.507456
11.003962	928.479877	11.512474
11.317335	919.622117	11.517491
11.216898	924.244481	11.522509
11.272747	919.624847	11.527527
11.350157	927.273921	11.532544
11.035260	918.374147	11.537562
11.287499	907.489209	11.542579
10.656262	910.992046	11.547597
10.849771	919.932853	11.552615
10.798678	919.906706	11.557632
10.735057	927.388986	11.562650
11.063538	921.453788	11.567667
10.837528	920.019271	11.572685
11.042681	937.451083	11.577703
10.893566	934.878290	11.582720
10.702356	943.498979	11.587738
11.230061	940.389713	11.592755
11.357317	956.972281	11.597773
11.473981	956.776233	11.602791
11.797104	952.587505	11.607808
11.288943	942.665042	11.612826
11.417324	929.495977	11.617843
11.596630	935.735331	11.622861
11.350127	931.247256	11.627879
11.406658	930.374189	11.632896
11.443975	936.942948	11.637914
11.206272	918.484360	11.642931
11.047952	932.089134	11.647949
10.928305	927.255658	11.652967
11.432344	928.134779	11.657984
11.084234	934.181564	11.663002
11.567922	940.080369	11.668019
11.470032	952.636223	11.673037
11.442305	935.691201	11.678055
11.548889	929.733694	11.683072
11.558752	932.961479	11.688090
11.301292	930.414896	11.693107
11.316237	935.184684	11.698125
11.252381	942.704804	11.703143
11.679980	947.538932	11.708160
11.357006	966.810521	11.713178
11.527685	963.173391	11.718195
11.512733	963.524313	11.723213
11.629476	961.615333	11.728231
11.722980	954.759627	11.733248
11.269262	944.254551	11.738266
11.679281	951.821786	11.743283
11.778521	944.881674	11.748301
11.638879	936.239863	11.753319
11.782937	928.320332	11.758336
11.372444	928.813129	11.763354
10.989584	930.462716	11.768371
11.300578	945.288150	11.773389
11.248921	957.908396	11.778407
11.290778	947.716902	11.783424
11.466616	963.991052	11.788442
11.550895	958.045889	11.793459
11.819777	951.265469	11.798477
11.439707	965.896714	11.803495
11.768503	956.300584	11.808512
11.702004	965.274240	11.813530
11.410862	960.855750	11.818547
11.624399	966.861111	11.823565
11.363109	979.359797	11.828583
11.763922	971.873297	11.833600
11.656272	971.170717	11.838618
11.676166	967.804608	11.843635
11.969942	973.980928	11.848653
11.655931	971.066947	11.853671
11.837789	966.746497	11.858688
11.525616	977.938704	11.863706
11.597164	983.316037	11.868723
11.922458	997.190767	11.873741
12.077443	999.169387	11.878759
12.196912	993.129410	11.883776
11.719345	979.876009	11.888794
11.845934	965.917085	11.893811
11.696789	976.774039	11.898829
11.720023	987.469783	11.903847
12.237831	998.404486	11.908864
12.138680	992.792823	11.913882
12.109606	977.251071	11.918899
12.000512	971.406427	11.923917
11.843298	959.750711	11.928935
11.794600	963.107092	11.933952
11.714934	974.821006	11.938970
12.069263	978.805896	11.943987
12.351967	981.681042	11.949005
11.937781	984.260192	11.954023
11.978533	967.776610	11.959040
11.861471	969.223529	11.964058
11.947828	978.295103	11.969075
12.116580	978.217982	11.974093
12.062167	992.463842	11.979111
12.148609	991.528734	11.984128
12.210349	992.644090	11.989146
12.301646	980.527143	11.994163
11.797899	972.202290	11.999181
11.851764	985.567650	12.004199
11.898925	996.024408	12.009216
12.167493	999.599901	12.014234
12.388873	991.172672	12.019251
12.337986	994.658552	12.024269
11.836354	996.832517	12.029287
12.048895	987.773709	12.034304
12.029204	992.436263	12.039322
12.429000	995.099115	12.044339
12.040698	997.340923	12.049357
12.188451	992.747386	12.054375
12.421802	984.030788	12.059392
12.257874	1000.712014	12.064410
12.283629	997.070924	12.069427
12.209768	988.835496	12.074445
11.985050	992.450944	12.079463
12.215906	991.975366	12.084480
12.094106	997.096152	12.089498
12.390074	993.577631	12.094515
12.367842	998.584688	12.099533
11.973887	995.688271	12.104551
12.244263	993.018836	12.109568
11.862790	991.608088	12.114586
12.162443	997.485425	12.119603
12.415210	998.549857	12.124621
12.069560	998.315805	12.129639
12.353148	1015.786290	12.134656
12.527617	1029.355723	12.139674
12.350962	1032.176638	12.144691
12.810392	1031.173068	12.149709
12.252211	1020.863185	12.154727
12.420490	1017.678784	12.159744
12.360162	1023.994469	12.164762
12.637123	1030.153912	12.169779
12.664946	1032.303194	12.174797
12.501579	1032.199973	12.179815
12.694627	995.629324	12.184832
12.390963	1000.938882	12.189850
12.308225	1003.602512	12.194867
12.528369	1016.489988	12.199885
12.262527	1026.002969	12.204903
12.751245	1022.056082	12.209920
12.592950	1032.433900	12.214938
12.517400	1029.625294	12.219955
12.825247	1019.901103	12.224973
12.375910	1026.338687	12.229991
12.651842	1027.364247	12.235008
12.489485	1025.729422	12.240026
12.601948	1028.393801	12.245043
12.604878	1025.234812	12.250061
12.323426	1031.628455	12.255079
12.625786	1025.756597	12.260096
12.809684	1028.227657	12.265114
12.693271	1025.502588	12.270131
13.106964	1025.915987	12.275149
12.835810	1023.716918	12.280167
12.679958	1023.062080	12.285184
12.820750	1025.510358	12.290202
12.722545	1026.431739	12.295219
12.760814	1022.952344	12.300237
12.615704	1025.783387	12.305255
12.575936	1021.664971	12.310272
12.566683	1025.490406	12.315290
12.576150	1021.031567	12.320307
12.758756	1024.504770	12.325325
12.381140	1029.040788	12.330343
12.834672	1038.566533	12.335360
12.811511	1056.773269	12.340378
12.829772	1052.057068	12.345395
12.939122	1061.670138	12.350413
12.707460	1063.057700	12.355431
12.752661	1060.229093	12.360448
12.948584	1063.285548	12.365466
12.530110	1055.148489	12.370483
12.971919	1057.898092	12.375501
12.794445	1069.607802	12.380519
13.174800	1059.977481	12.385536
13.064508	1067.101822	12.390554
13.148264	1057.488336	12.395571
13.085790	1060.045081	12.400589
12.839024	1074.118546	12.405607
13.182303	1052.142845	12.410624
13.068603	1059.968115	12.415642
12.574513	1064.415167	12.420659
13.239382	1053.957054	12.425677
13.044926	1063.349972	12.430695
13.054243	1062.305983	12.435712
13.129217	1057.712668	12.440730
12.863110	1063.801432	12.445747
13.663703	1051.675628	12.450765
13.322377	1064.008902	12.455783
13.075182	1058.334333	12.460800
13.218797	1060.011705	12.465818
13.249581	1061.499502	12.470835
13.339083	1052.742123	12.475853
13.004121	1053.202337	12.480871
12.884537	1051.776166	12.485888
12.984478	1054.291448	12.490906
13.082378	1062.767480	12.495923
12.788534	1055.747143	12.500941
13.065576	1075.806086	12.505959
13.406802	1074.789412	12.510976
13.543945	1086.592699	12.515994
13.474850	1092.806718	12.521011
13.380526	1088.165842	12.526029
13.044260	1083.590621	12.531047
13.461337	1092.581511	12.536064
13.482682	1092.116217	12.541082
13.180606	1090.236421	12.546099
13.250535	1092.330315	12.551117
13.318000	1096.883195	12.556135
13.442997	1084.063761	12.561152
13.214112	1086.660665	12.566170
13.178822	1091.372681	12.571187
13.448970	1096.700630	12.576205
13.065257	1093.899740	12.581223
13.233906	1092.067184	12.586240
13.438049	1087.449320	12.591258
13.418223	1089.765945	12.596275
13.416275	1084.118861	12.601293
13.373661	1089.730089	12.606311
13.425809	1089.762433	12.611328
13.475012	1087.244958	12.616346
13.303173	1105.395272	12.621363
13.322705	1119.788841	12.626381
13.490460	1122.816902	12.631399
13.623447	1113.507817	12.636416
13.940120	1126.108936	12.641434
14.066450	1129.117875	12.646451
13.864922	1117.035928	12.651469
13.468261	1098.792813	12.656487
13.778085	1121.133710	12.661504
13.861479	1115.576023	12.666522
13.441804	1097.781194	12.671539
13.522325	1105.181030	12.676557
13.906105	1113.949107	12.681575
13.788909	1113.684308	12.686592
14.179883	1107.729636	12.691610
13.711336	1103.427882	12.696627
14.040682	1085.355098	12.701645
13.708295	1090.199380	12.706663
13.842277	1085.437629	12.711680
13.907919	1080.004543	12.716698
13.773799	1082.754252	12.721715
13.804232	1083.181910	12.726733
13.772237	1086.725309	12.731751
13.498664	1072.574298	12.736768
13.993388	1092.996414	12.741786
13.732145	1111.473340	12.746803
14.207797	1108.525412	12.751821
13.803272	1116.539024	12.756839
13.882926	1116.327844	12.761856
13.963428	1112.920566	12.766874
13.735428	1128.516906	12.771891
14.008809	1119.705812	12.776909
13.849289	1122.696340	12.781927
13.945684	1120.704886	12.786944
13.919187	1120.380580	12.791962
13.919450	1118.075923	12.796979
13.790130	1123.113352	12.801997
13.765574	1118.575082	12.807015
13.518088	1117.165361	12.812032
13.657911	1118.851241	12.817050
13.945017	1127.171571	12.822067
13.992222	1122.582835	12.827085
13.788162	1132.183284	12.832103
14.029477	1141.043471	12.837120
14.137401	1145.487306	12.842138
13.638013	1149.669913	12.847155
13.957368	1139.085501	12.852173
13.777994	1150.803854	12.857191
13.916453	1155.831988	12.862208
14.478947	1147.834786	12.867226
14.236529	1153.404718	12.872243
14.326900	1148.748985	12.877261
14.466917	1155.879552	12.882279
14.235044	1148.341445	12.887296
14.274816	1142.903567	12.892314
14.426533	1146.329552	12.897331
14.592881	1147.986240	12.902349
14.697484	1157.461577	12.907367
14.612128	1153.573897	12.912384
14.696753	1147.743956	12.917402
14.385478	1154.380769	12.922419
14.486335	1149.453229	12.927437
14.294373	1140.723514	12.932455
14.089960	1145.441506	12.937472
14.653021	1146.465588	12.942490
14.386962	1155.664914	12.947507
14.253347	1153.825321	12.952525
14.392851	1148.984292	12.957543
14.215347	1153.088400	12.962560
14.327274	1146.048069	12.967578
14.410923	1148.390479	12.972595
14.713992	1147.505313	12.977613
14.354702	1151.995419	12.982631
14.280610	1151.756944	12.987648
14.677746	1139.653398	12.992666
14.321607	1147.975145	12.997683
14.315493	1143.539716	13.002701
14.518751	1145.681615	13.007719
14.355351	1150.725878	13.012736
14.656130	1151.396949	13.017754
14.396250	1151.234908	13.022771
14.356279	1157.940965	13.027789
14.804339	1163.017829	13.032807
14.728411	1175.760772	13.037824
14.882219	1170.283134	13.042842
14.383080	1164.523873	13.047859
14.575761	1168.988324	13.052877
14.800911	1180.668450	13.057895
14.817170	1189.184842	13.062912
14.933424	1180.052106	13.067930
14.858196	1190.778074	13.072947
14.996121	1170.801118	13.077965
14.820294	1156.427550	13.082983
14.622388	1152.878184	13.088000
14.915645	1155.067383	13.093018
14.459898	1158.779394	13.098035
14.747610	1173.193954	13.103053
14.655115	1182.672419	13.108071
14.341301	1190.288381	13.113088
14.902787	1182.225582	13.118106
14.712840	1191.794991	13.123123
15.079254	1189.591102	13.128141
15.055358	1185.644813	13.133159
14.803449	1180.735130	13.138176
15.220655	1178.063790	13.143194
14.681359	1180.559362	13.148211
14.684513	1184.072948	13.153229
15.296517	1177.554497	13.158247
14.925729	1191.177360	13.163264
15.057245	1186.328981	13.168282
14.829508	1190.051271	13.173299
14.542568	1187.544171	13.178317
14.963715	1187.505960	13.183335
14.919108	1201.235441	13.188352
15.194962	1192.186895	13.193370
14.850375	1194.795497	13.198387
15.070411	1210.081511	13.203405
15.321724	1209.213180	13.208423
15.268013	1216.339243	13.213440
15.313566	1209.474043	13.218458
15.220709	1201.334559	13.223475
15.027627	1183.144637	13.228493
15.173720	1197.005916	13.233511
15.094795	1225.123781	13.238528
15.334181	1218.423325	13.243546
15.745254	1218.991884	13.248563
15.293879	1209.063389	13.253581
15.515441	1195.586551	13.258599
15.198983	1186.488460	13.263616
15.217256	1180.798624	13.268634
15.305682	1185.464985	13.273651
15.327053	1186.872465	13.278669
15.326314	1181.305852	13.283687
15.118905	1190.241163	13.288704
15.529760	1203.567672	13.293722
15.328952	1211.107845	13.298739
15.578309	1214.160206	13.303757
15.477609	1212.803331	13.308775
15.428822	1217.886508	13.313792
15.732553	1203.252779	13.318810
15.351010	1205.441924	13.323827
15.389423	1207.800888	13.328845
15.323437	1202.609630	13.333863
15.765912	1207.548461	13.338880
15.768516	1209.345261	13.343898
15.462344	1198.049063	13.348915
15.386828	1203.153983	13.353933
15.773996	1207.751195	13.358951
15.814933	1212.024258	13.363968
15.798530	1197.680943	13.368986
15.484312	1186.144360	13.374003
15.506358	1190.354405	13.379021
15.706678	1191.852327	13.384039
15.766865	1197.553654	13.389056
15.582642	1188.251387	13.394074
15.696754	1193.199709	13.399091
15.692437	1207.396132	13.404109
15.606755	1204.000213	13.409127
15.527636	1219.027122	13.414144
15.728997	1210.979852	13.419162
15.701645	1219.600330	13.424179
15.571393	1226.048540	13.429197
15.645741	1221.768264	13.434215
15.424237	1224.650575	13.439232
15.815553	1212.763679	13.444250
15.741890	1227.492457	13.449267
15.543830	1220.669169	13.454285
15.736975	1216.145212	13.459303
15.559248	1215.485721	13.464320
15.682672	1213.975199	13.469338
15.677408	1224.506539	13.474355
15.543379	1243.051923	13.479373
15.666926	1243.904312	13.484391
15.806644	1254.358514	13.489408
16.109848	1245.940826	13.494426
16.196292	1248.193814	13.499443
15.956839	1254.685315	13.504461
15.897259	1255.404648	13.509479
16.040009	1254.890899	13.514496
16.423717	1257.722206	13.519514
16.090570	1242.992335	13.524531
15.944138	1250.690447	13.529549
16.383562	1245.275326	13.534567
16.049057	1252.045945	13.539584
16.096970	1253.715959	13.544602
16.182509	1242.996184	13.549619
15.968494	1254.290048	13.554637
16.193060	1253.474174	13.559655
16.033534	1255.513570	13.564672
15.830886	1247.354055	13.569690
15.878186	1237.841375	13.574707
15.821807	1241.997887	13.579725
16.091859	1241.422900	13.584743
15.935413	1251.226950	13.589760
16.079588	1262.577249	13.594778
16.300171	1270.025228	13.599795
16.327533	1271.281333	13.604813
16.523924	1261.523088	13.609831
16.437414	1267.986118	13.614848
16.250812	1267.067076	13.619866
16.456024	1262.747796	13.624883
16.248731	1268.638322	13.629901
16.509366	1266.077932	13.634919
16.425786	1268.740566	13.639936
16.635488	1267.497241	13.644954
16.554838	1260.621029	13.649971
16.321727	1266.745746	13.654989
16.512677	1265.868904	13.660007
16.596006	1263.279610	13.665024
16.483304	1263.852626	13.670042
16.627684	1260.868192	13.675059
16.296520	1269.269724	13.680077
16.947799	1262.851819	13.685095
16.732029	1256.406636	13.690112
16.772673	1269.728763	13.695130
16.610510	1255.365045	13.700147
16.271654	1261.078147	13.705165
16.742009	1260.748723	13.710183
16.769367	1253.723529	13.715200
16.267303	1267.048125	13.720218
16.871861	1263.215457	13.725235
16.840114	1269.251712	13.730253
16.869601	1266.013081	13.735271
16.817754	1267.127188	13.740288
16.894092	1266.205942	13.745306
17.103068	1265.109191	13.750323
16.537606	1262.621430	13.755341
16.808428	1258.969616	13.760359
16.478476	1261.390377	13.765376
16.506102	1266.070374	13.770394
16.583102	1274.025979	13.775411
16.734719	1272.825343	13.780429
16.729519	1269.873158	13.785447
16.504063	1273.324230	13.790464
16.641992	1270.553062	13.795482
16.818081	1264.147313	13.800499
16.462940	1273.179181	13.805517
16.632665	1285.977201	13.810535
16.623034	1292.606640	13.815552
16.737748	1300.789080	13.820570
17.023938	1301.899179	13.825587
16.985101	1298.279737	13.830605
17.201782	1303.037885	13.835623
17.090789	1299.426849	13.840640
16.645723	1307.663015	13.845658
17.466999	1293.229711	13.850675
17.073206	1298.674765	13.855693
17.361203	1297.366505	13.860711
17.207407	1299.646292	13.865728
17.099533	1292.585208	13.870746
17.328066	1299.464574	13.875763
16.924204	1294.668993	13.880781
17.123698	1292.321869	13.885799
17.097025	1298.319895	13.890816
16.934684	1293.149680	13.895834
17.066046	1285.349391	13.900851
17.073088	1290.621374	13.905869
16.862022	1286.609599	13.910887
17.115544	1293.554114	13.915904
16.844104	1304.526822	13.920922
17.521319	1314.908986	13.925939
17.439644	1327.113645	13.930957
17.567749	1323.613006	13.935975
17.526915	1323.976096	13.940992
17.600575	1312.770849	13.946010
17.466590	1295.869407	13.951027
17.354151	1293.812910	13.956045
17.162484	1293.554928	13.961063
17.521035	1309.963747	13.966080
17.399696	1317.886079	13.971098
17.591214	1315.193035	13.976115
17.461658	1326.641071	13.981133
17.705483	1324.693286	13.986151
17.798265	1332.641978	13.991168
17.531247	1324.801343	13.996186
17.888924	1309.390485	14.001203
17.331942	1306.162745	14.006221
17.376042	1310.422713	14.011239
17.653194	1312.479959	14.016256
17.898939	1324.197728	14.021274
18.199194	1317.387151	14.026291
17.629376	1308.106934	14.031309
17.617066	1302.542194	14.036327
17.576225	1295.903857	14.041344
17.321547	1300.282589	14.046362
17.488092	1315.668902	14.051379
17.655385	1324.502870	14.056397
18.010416	1326.805484	14.061415
17.753521	1329.125183	14.066432
17.599633	1335.048621	14.071450
17.701060	1329.898887	14.076467
17.527029	1334.152464	14.081485
17.764492	1335.471025	14.086503
17.632108	1335.267397	14.091520
17.225506	1333.984790	14.096538
17.701693	1324.824254	14.101555
17.694421	1350.189982	14.106573
18.233306	1358.221502	14.111591
18.462282	1352.001444	14.116608
18.002733	1340.743139	14.121626
18.007790	1325.437115	14.126643
18.081843	1332.440894	14.131661
18.149382	1330.191599	14.136679
18.053241	1327.024545	14.141696
18.123590	1323.066945	14.146714
17.964311	1316.760804	14.151731
17.779418	1325.998757	14.156749
18.117510	1334.844998	14.161767
18.124908	1341.489747	14.166784
18.172398	1353.681305	14.171802
18.394050	1357.602047	14.176819
18.016012	1349.052632	14.181837
17.982733	1355.817901	14.186855
18.338937	1357.619941	14.191872
18.307832	1366.189155	14.196890
18.324061	1353.715457	14.201907
18.383618	1365.792036	14.206925
18.209330	1364.378044	14.211943
18.235482	1359.181318	14.216960
17.992933	1373.865368	14.221978
18.199680	1363.079771	14.226995
18.421555	1369.850036	14.232013
18.281476	1361.863167	14.237031
18.555618	1357.647011	14.242048
18.281984	1360.149010	14.247066
18.104485	1353.082499	14.252083
18.010724	1365.113996	14.257101
18.238131	1362.546101	14.262119
18.266716	1363.861853	14.267136
18.153301	1361.688975	14.272154
18.265494	1369.229359	14.277171
18.317687	1383.857130	14.282189
18.619898	1388.427127	14.287207
18.814186	1379.946301	14.292224
18.406497	1393.054592	14.297242
18.744091	1385.446476	14.302259
18.376816	1386.404168	14.307277
18.714715	1384.708904	14.312295
18.738100	1374.780028	14.317312
18.505357	1394.366331	14.322330
18.887064	1386.850908	14.327347
18.737203	1385.079331	14.332365
18.873912	1382.884715	14.337383
18.978880	1382.888233	14.342400
18.880689	1388.244210	14.347418
18.856426	1382.304261	14.352435
18.877202	1390.989698	14.357453
18.903080	1387.481959	14.362471
19.266554	1371.897641	14.367488
18.518519	1375.114806	14.372506
18.805523	1369.578428	14.377523
19.039626	1383.957574	14.382541
18.793894	1384.659316	14.387559
18.842882	1384.383133	14.392576
18.602108	1381.715602	14.397594
18.831013	1382.935979	14.402611
18.827153	1388.470820	14.407629
18.639277	1384.059516	14.412647
18.916358	1384.633343	14.417664
18.730220	1392.250700	14.422682
18.890165	1388.634934	14.427699
19.091027	1387.723768	14.432717
19.095021	1380.403177	14.437735
19.067462	1376.906651	14.442752
18.680909	1391.137013	14.447770
19.119909	1410.278638	14.452787
19.537885	1410.600397	14.457805
19.226511	1400.798986	14.462823
19.475503	1400.589287	14.467840
18.931497	1391.396082	14.472858
19.248415	1407.149311	14.477875
19.267402	1415.994111	14.482893
19.199344	1428.283207	14.487911
19.154168	1418.970373	14.492928
18.678312	1418.392132	14.497946
18.696798	1424.808706	14.502963
19.352427	1428.388706	14.507981
19.197837	1425.494694	14.512999
19.579092	1417.710043	14.518016
19.088979	1421.838823	14.523034
19.414060	1420.443312	14.528051
19.405630	1426.528128	14.533069
19.030045	1433.063899	14.538087
19.270669	1425.451350	14.543104
19.066935	1447.936029	14.548122
19.340739	1447.102149	14.553139
19.852212	1455.561484	14.558157
19.631509	1451.166227	14.563175
19.933686	1443.041513	14.568192
19.509380	1451.044398	14.573210
19.669765	1445.806516	14.578227
19.839345	1454.367348	14.583245
19.606526	1445.063131	14.588263
19.991417	1438.783362	14.593280
19.433181	1441.268725	14.598298
19.647479	1437.211668	14.603315
19.622616	1444.290933	14.608333
19.748912	1451.820361	14.613351
20.141774	1445.256201	14.618368
19.902446	1448.362762	14.623386
20.002147	1431.487435	14.628403
19.942182	1423.226641	14.633421
19.519032	1423.104625	14.638439
19.623832	1416.031888	14.643456
19.589851	1435.651470	14.648474
19.982433	1432.061736	14.653491
19.935522	1439.400945	14.658509
19.797957	1447.043356	14.663527
20.095689	1443.103976	14.668544
20.041138	1447.039377	14.673562
19.930927	1443.833685	14.678579
19.921807	1434.390856	14.683597
19.721189	1447.690097	14.688615
20.194295	1445.439371	14.693632
20.404690	1437.417653	14.698650
20.162331	1445.115999	14.703667
20.011418	1437.287970	14.708685
20.175229	1439.290381	14.713703
20.379048	1440.593263	14.718720
20.218271	1440.698268	14.723738
20.483447	1436.047360	14.728755
20.132192	1431.850103	14.733773
20.156695	1439.031819	14.738791
20.135254	1441.883009	14.743808
20.157999	1438.341919	14.748826
20.397880	1435.683759	14.753843
20.408699	1438.101658	14.758861
20.200805	1436.608186	14.763879
20.246528	1431.717246	14.768896
19.925073	1436.870450	14.773914
20.409933	1438.801981	14.778931
20.661952	1434.007585	14.783949
20.135294	1443.464405	14.788967
20.003986	1443.220833	14.793984
20.170819	1438.414165	14.799002
19.910915	1441.780822	14.804019
20.096957	1454.719979	14.809037
20.176101	1477.598010	14.814055
20.526315	1466.172841	14.819072
20.555526	1472.914428	14.824090
20.405270	1475.882230	14.829107
20.529469	1465.871641	14.834125
20.508961	1479.738321	14.839143
20.561855	1474.183194	14.844160
20.493519	1474.780367	14.849178
20.307247	1475.904939	14.854195
20.960938	1473.505014	14.859213
20.530514	1483.125054	14.864231
20.671358	1474.349488	14.869248
20.438976	1472.668337	14.874266
20.650373	1477.152613	14.879283
20.617553	1488.000502	14.884301
20.408497	1495.598083	14.889319
20.778540	1506.718245	14.894336
20.789525	1518.127007	14.899354
20.903826	1508.453461	14.904371
21.355832	1507.580227	14.909389
20.831470	1507.816700	14.914407
21.074047	1503.305734	14.919424
21.008359	1507.222916	14.924442
21.037960	1504.767675	14.929459
21.369128	1492.880684	14.934477
20.885772	1475.927060	14.939495
21.202002	1470.417302	14.944512
21.115310	1474.284805	14.949530
21.032415	1475.268243	14.954547
20.969082	1461.593079	14.959565
21.384723	1489.362597	14.964583
21.234760	1469.893950	14.969600
20.886985	1472.851547	14.974618
20.922221	1492.137300	14.979635
21.275059	1492.356463	14.984653
20.900774	1498.508979	14.989671
21.267540	1491.647943	14.994688
21.201810	1490.209663	14.999706
21.178601	1498.925278	15.004723
21.333968	1500.656658	15.009741
21.348186	1498.561836	15.014759
21.557018	1499.602871	15.019776
21.500915	1506.844817	15.024794
21.294441	1501.603889	15.029811
21.284213	1492.563567	15.034829
21.171782	1504.195117	15.039847
21.398051	1490.928659	15.044864
21.481999	1495.373416	15.049882
20.975239	1502.086843	15.054899
21.291268	1494.012564	15.059917
20.995750	1496.836316	15.064935
21.265431	1498.749157	15.069952
21.280090	1509.690773	15.074970
21.083203	1530.084689	15.079987
21.702151	1524.553129	15.085005
21.683854	1520.409766	15.090023
21.532404	1531.239929	15.095040
21.577449	1528.334885	15.100058
21.607576	1522.532725	15.105075
21.763311	1530.718729	15.110093
21.811802	1535.339841	15.115111
21.826735	1517.499723	15.120128
22.083282	1526.884771	15.125146
21.861645	1528.362051	15.130163
21.838064	1530.948652	15.135181
21.937012	1528.601608	15.140199
21.949472	1522.158677	15.145216
22.008969	1521.260677	15.150234
21.747736	1526.636614	15.155251
22.024417	1530.693562	15.160269
21.901638	1531.549751	15.165287
21.917008	1523.565008	15.170304
21.769702	1531.623638	15.175322
21.615850	1525.695251	15.180339
21.996611	1519.624007	15.185357
21.736000	1517.364852	15.190375
21.997865	1522.515582	15.195392
21.848059	1525.117967	15.200410
21.873320	1524.140204	15.205427
22.322352	1525.863113	15.210445
22.147403	1525.127164	15.215463
22.084614	1527.837973	15.220480
22.001409	1528.333280	15.225498
21.947169	1538.488693	15.230515
22.043345	1545.442055	15.235533
22.162292	1557.097533	15.240551
22.394992	1550.661033	15.245568
22.420439	1552.908025	15.250586
22.341609	1556.336846	15.255603
22.585819	1547.442547	15.260621
22.147002	1554.792379	15.265639
22.457311	1554.433155	15.270656
22.282644	1556.456594	15.275674
22.319446	1554.565898	15.280691
22.451607	1548.748407	15.285709
22.443996	1552.955194	15.290727
22.520654	1554.422056	15.295744
22.584439	1553.400510	15.300762
22.453826	1557.201291	15.305779
22.594251	1549.381652	15.310797
22.439985	1557.466251	15.315815
22.435787	1547.258369	15.320832
22.657550	1546.239797	15.325850
22.558663	1559.021894	15.330867
22.850264	1550.992182	15.335885
22.287839	1553.435342	15.340903
22.390336	1561.010890	15.345920
22.639239	1552.018174	15.350938
22.815188	1552.844580	15.355955
22.821156	1546.038543	15.360973
22.823842	1553.129437	15.365991
22.647442	1548.215795	15.371008
22.864851	1543.276704	15.376026
22.834146	1551.875875	15.381043
22.983631	1543.398443	15.386061
23.120765	1548.533617	15.391079
23.075552	1544.374232	15.396096
23.059426	1545.545435	15.401114
22.634606	1553.678772	15.406131
22.444986	1543.935060	15.411149
22.992355	1573.877392	15.416167
23.027382	1577.226734	15.421184
23.069824	1576.352815	15.426202
22.730805	1580.061341	15.431219
23.038493	1572.199820	15.436237
23.138597	1580.851754	15.441255
23.094674	1579.519697	15.446272
23.266402	1577.499175	15.451290
23.175030	1578.893865	15.456307
23.018363	1578.184807	15.461325
22.973945	1572.502059	15.466343
23.021438	1581.505225	15.471360
23.202442	1572.761535	15.476378
22.932899	1572.240066	15.481395
23.264602	1576.120986	15.486413
23.434202	1594.536587	15.491431
23.060035	1599.864715	15.496448
23.572477	1599.542884	15.501466
23.821543	1597.317427	15.506483
23.605100	1582.634442	15.511501
23.590103	1572.852740	15.516519
23.314449	1570.433471	15.521536
23.751750	1567.945746	15.526554
23.455838	1573.908935	15.531571
23.664862	1571.157043	15.536589
23.662821	1561.506667	15.541607
23.387352	1563.906640	15.546624
23.696490	1562.455489	15.551642
23.524831	1562.468596	15.556659
23.182430	1565.883587	15.561677
23.344262	1579.175674	15.566695
23.587350	1580.588994	15.571712
24.240870	1587.073310	15.576730
24.159869	1593.153674	15.581747
24.049334	1572.586638	15.586765
23.896914	1566.078867	15.591783
23.818146	1564.951794	15.596800
23.887228	1556.861290	15.601818
23.778898	1553.989514	15.606835
24.001028	1550.505538	15.611853
24.007054	1555.723054	15.616871
23.955465	1557.079658	15.621888
24.048827	1545.349329	15.626906
24.064530	1551.523111	15.631923
23.958352	1552.084428	15.636941
23.908039	1544.815666	15.641959
24.117723	1554.132507	15.646976
24.308740	1556.353656	15.651994
24.217304	1551.789720	15.657011
24.150857	1548.248808	15.662029
24.037705	1554.595110	15.667047
24.244587	1554.133723	15.672064
24.322697	1544.159062	15.677082
24.147649	1557.912034	15.682099
24.253686	1552.475637	15.687117
24.617963	1548.759462	15.692135
24.342517	1553.353120	15.697152
24.197497	1546.151615	15.702170
23.880963	1554.993001	15.707187
24.205579	1571.527008	15.712205
24.482160	1580.522946	15.717223
24.428107	1587.842936	15.722240
24.926888	1580.815512	15.727258
24.583793	1567.746423	15.732275
24.033697	1558.512000	15.737293
24.702767	1570.124421	15.742311
24.277841	1586.380992	15.747328
24.790886	1588.337796	15.752346
24.496506	1589.746026	15.757363
24.783335	1583.215115	15.762381
24.460747	1583.059909	15.767399
24.550375	1584.955334	15.772416
24.720307	1589.165013	15.777434
24.728324	1590.409387	15.782451
24.605601	1591.178563	15.787469
24.735530	1586.833471	15.792487
24.450496	1590.336604	15.797504
24.751378	1588.967920	15.802522
24.776717	1575.759860	15.807539
24.605641	1583.813004	15.812557
24.700731	1584.765400	15.817575
24.761385	1582.433351	15.822592
24.927317	1576.448446	15.827610
24.727498	1594.264988	15.832627
24.824867	1584.752072	15.837645
24.996484	1576.846940	15.842663
24.705276	1588.428236	15.847680
24.848221	1600.061269	15.852698
24.730491	1609.837479	15.857715
25.068296	1609.258741	15.862733
25.192981	1597.242872	15.867751
25.263932	1618.194518	15.872768
25.297463	1609.468536	15.877786
25.328922	1610.255487	15.882803
24.803729	1607.270449	15.887821
25.363334	1605.299472	15.892839
25.152334	1610.414363	15.897856
25.293141	1605.207229	15.902874
25.007674	1615.420668	15.907891
25.235731	1615.707347	15.912909
25.176391	1604.903047	15.917927
25.320326	1610.892626	15.922944
25.443896	1606.940707	15.927962
25.122487	1618.384508	15.932979
25.436601	1609.080566	15.937997
25.457728	1606.717264	15.943015
25.405694	1616.716063	15.948032
25.699468	1606.994625	15.953050
25.794322	1613.086821	15.958067
25.304408	1613.060898	15.963085
25.677370	1616.269642	15.968103
25.538576	1610.469044	15.973120
25.544492	1607.247631	15.978138
25.329800	1611.582427	15.983155
25.303114	1608.355782	15.988173
25.845667	1615.011242	15.993191
25.636206	1634.367614	15.998208
25.761714	1640.547658	16.003226
26.097568	1640.698770	16.008243
25.569286	1637.609513	16.013261
26.241001	1629.287288	16.018279
25.658224	1630.038159	16.023296
26.072773	1626.653011	16.028314
26.072569	1622.823947	16.033331
25.935254	1619.564046	16.038349
25.947119	1601.910953	16.043367
25.569580	1613.934517	16.048384
25.895463	1627.915621	16.053402
25.782927	1633.009490	16.058419
25.736924	1630.363993	16.063437
26.246890	1633.485880	16.068455
25.909016	1633.856827	16.073472
25.791771	1640.347936	16.078490
25.808357	1638.490105	16.083507
25.961203	1636.716797	16.088525
26.388474	1628.399225	16.093543
25.995642	1636.500535	16.098560
26.184205	1644.356360	16.103578
26.239129	1656.124483	16.108595
26.416644	1666.059318	16.113613
26.532939	1654.006999	16.118631
26.656931	1660.254230	16.123648
26.473064	1650.392176	16.128666
26.177089	1637.002626	16.133683
26.134348	1653.638105	16.138701
26.590470	1658.342933	16.143719
26.398921	1667.451481	16.148736
26.858374	1662.328570	16.153754
26.702410	1659.593796	16.158771
26.885189	1665.058065	16.163789
26.412895	1643.431941	16.168807
26.322860	1657.778798	16.173824
26.538612	1662.369887	16.178842
26.911602	1661.395556	16.183859
26.663689	1672.076830	16.188877
26.853248	1659.938752	16.193895
26.792277	1668.178825	16.198912
26.809326	1664.026420	16.203930
27.074259	1654.341619	16.208947
26.764693	1661.541750	16.213965
26.957704	1652.459806	16.218983
26.736585	1653.461027	16.224000
26.731908	1643.660248	16.229018
26.979469	1653.922059	16.234035
27.099276	1663.323928	16.239053
27.058317	1652.716945	16.244071
26.856764	1667.420073	16.249088
26.981056	1655.682965	16.254106
26.984087	1666.395120	16.259123
26.974031	1666.656270	16.264141
26.928267	1648.667391	16.269159
26.919074	1666.745757	16.274176
26.755005	1654.616636	16.279194
27.235088	1663.497820	16.284211
26.971123	1649.734454	16.289229
27.206561	1657.965595	16.294247
26.939413	1656.672858	16.299264
27.184733	1655.987780	16.304282
27.333198	1654.478188	16.309299
27.511338	1675.898778	16.314317
27.484233	1669.480448	16.319335
27.045091	1668.061073	16.324352
27.325763	1675.646936	16.329370
27.408136	1669.731739	16.334387
27.775485	1673.165047	16.339405
27.836298	1672.187687	16.344423
27.620110	1672.729035	16.349440
27.507420	1668.491421	16.354458
27.714609	1669.483133	16.359475
27.412324	1674.574973	16.364493
27.555640	1669.073701	16.369511
27.488995	1684.954902	16.374528
27.847428	1677.034925	16.379546
28.005104	1678.145075	16.384563
27.539093	1677.593144	16.389581
27.893877	1668.508811	16.394599
27.691623	1681.723876	16.399616
27.860744	1684.615995	16.404634
28.143457	1671.581770	16.409651
27.528169	1674.728979	16.414669
27.904532	1672.472195	16.419687
27.737620	1673.574283	16.424704
27.613253	1673.323259	16.429722
27.654112	1670.386992	16.434739
27.616754	1676.316066	16.439757
28.010915	1668.130334	16.444775
27.592466	1676.791814	16.449792
27.631406	1692.381523	16.454810
27.827319	1700.577499	16.459827
27.862636	1701.894921	16.464845
28.377136	1703.576301	16.469863
28.294020	1704.569632	16.474880
28.209203	1706.229391	16.479898
28.100491	1704.569467	16.484915
27.817433	1702.202585	16.489933
28.145769	1707.373866	16.494951
28.105980	1713.162805	16.499968
28.098988	1720.255377	16.504986
28.358917	1733.454581	16.510003
28.590120	1730.893872	16.515021
28.876409	1737.621743	16.520039
28.673649	1726.740320	16.525056
28.522822	1728.968496	16.530074
28.474107	1719.912761	16.535091
28.373178	1729.728391	16.540109
28.998568	1728.822103	16.545127
29.009614	1717.828509	16.550144
28.771325	1699.898224	16.555162
29.108582	1696.019559	16.560179
28.195844	1697.556967	16.565197
28.411220	1697.302438	16.570215
28.664979	1704.232533	16.575232
28.399141	1714.657747	16.580250
29.158038	1725.021939	16.585267
29.034200	1728.749198	16.590285
29.318622	1721.732406	16.595303
29.070774	1717.329756	16.600320
28.749942	1700.476925	16.605338
28.887387	1695.587249	16.610355
28.773717	1712.594381	16.615373
29.306350	1718.361366	16.620391
29.195561	1720.166373	16.625408
29.243400	1711.753713	16.630426
29.057549	1696.607678	16.635443
28.734169	1709.751485	16.640461
29.041939	1712.300569	16.645479
29.151843	1716.309200	16.650496
29.478455	1733.978490	16.655514
29.257926	1733.763074	16.660531
29.043183	1729.880927	16.665549
29.208101	1718.744921	16.670567
29.159627	1734.185366	16.675584
29.073072	1726.365037	16.680602
29.288354	1723.066410	16.685619
29.257920	1723.604953	16.690637
29.241547	1734.075091	16.695655
29.404075	1723.054440	16.700672
29.267009	1733.436296	16.705690
29.552666	1719.131062	16.710707
29.311196	1728.332952	16.715725
29.375689	1742.179098	16.720743
29.757804	1759.901038	16.725760
29.538887	1752.779785	16.730778
30.050858	1746.825703	16.735795
29.752730	1745.293205	16.740813
29.909680	1754.837405	16.745831
30.073755	1736.055403	16.750848
29.956362	1726.509459	16.755866
29.955502	1716.343039	16.760883
29.801905	1720.217745	16.765901
29.759873	1719.840880	16.770919
29.811431	1717.587483	16.775936
29.956936	1734.591091	16.780954
30.150147	1718.519265	16.785971
29.594958	1725.897896	16.790989
29.861664	1738.714090	16.796007
29.862072	1742.563298	16.801024
30.035047	1746.632753	16.806042
30.083463	1752.009459	16.811059
29.865354	1753.544443	16.816077
29.723557	1756.112862	16.821095
30.029559	1750.507455	16.826112
29.922832	1755.400401	16.831130
29.988135	1744.114730	16.836147
29.990407	1757.890484	16.841165
30.078978	1779.241795	16.846183
30.109505	1778.254876	16.851200
30.317768	1776.031820	16.856218
30.595221	1770.334283	16.861235
30.396210	1773.849196	16.866253
30.445044	1773.493110	16.871271
30.624954	1773.430675	16.876288
30.496697	1770.146013	16.881306
30.714393	1769.248180	16.886323
30.617857	1776.868998	16.891341
30.739839	1768.953877	16.896359
30.610636	1766.783162	16.901376
30.386407	1774.402682	16.906394
30.792135	1764.956311	16.911411
30.754907	1770.369253	16.916429
30.535590	1761.302375	16.921447
31.018324	1764.907938	16.926464
30.865948	1765.337147	16.931482
31.258868	1755.855894	16.936499
31.075955	1762.709505	16.941517
30.729903	1763.981423	16.946535
31.051046	1756.792390	16.951552
30.850638	1769.117058	16.956570
30.852783	1763.322986	16.961587
30.647803	1767.913699	16.966605
30.860293	1761.198173	16.971623
30.943995	1755.823278	16.976640
30.603718	1763.964771	16.981658
30.871753	1761.700716	16.986675
31.364519	1776.882678	16.991693
31.186243	1791.372224	16.996711
31.583501	1786.475323	17.001728
30.956894	1794.322116	17.006746
31.245676	1787.080554	17.011763
31.032999	1799.188378	17.016781
31.296472	1787.262766	17.021799
31.669968	1786.813547	17.026816
31.359555	1795.283972	17.031834
31.586443	1787.473913	17.036851
31.273890	1791.856853	17.041869
31.543499	1793.584309	17.046887
31.407034	1796.040039	17.051904
31.235146	1791.289747	17.056922
31.627444	1783.707419	17.061939
31.855803	1785.462965	17.066957
31.471307	1786.013684	17.071975
31.548565	1792.633672	17.076992
31.539971	1793.548133	17.082010
31.636011	1788.604653	17.087027
31.571407	1790.552415	17.092045
31.698350	1797.114965	17.097063
31.951993	1811.241270	17.102080
31.764938	1817.675902	17.107098
31.925191	1820.306126	17.112115
32.417089	1817.682942	17.117133
32.317116	1810.747480	17.122151
31.997441	1791.494723	17.127168
31.902829	1788.230076	17.132186
32.299013	1802.174500	17.137203
32.486578	1809.003397	17.142221
31.950160	1795.580297	17.147239
32.090098	1784.684998	17.152256
31.852882	1792.854321	17.157274
32.215884	1805.757381	17.162291
32.554547	1817.606990	17.167309
32.425595	1821.747721	17.172327
32.833728	1823.327831	17.177344
32.205090	1806.832551	17.182362
32.268473	1789.533317	17.187379
32.279871	1808.924200	17.192397
32.568366	1821.245116	17.197415
32.873761	1808.278282	17.202432
32.677660	1806.424942	17.207450
32.543156	1788.059253	17.212467
32.582801	1789.196043	17.217485
32.384882	1788.820974	17.222503
32.684026	1795.525876	17.227520
32.171211	1811.681486	17.232538
32.424530	1812.594703	17.237555
32.505690	1822.545988	17.242573
32.414722	1816.947631	17.247591
32.748470	1812.339983	17.252608
32.735466	1818.979260	17.257626
32.748849	1821.975542	17.262643
32.750109	1813.379200	17.267661
32.469709	1811.752420	17.272679
32.619005	1816.960079	17.277696
32.742965	1836.330782	17.282714
33.047046	1840.975015	17.287731
33.180362	1840.752184	17.292749
33.085050	1846.196819	17.297767
33.359783	1839.527646	17.302784
33.228232	1844.736545	17.307802
33.583744	1835.842942	17.312819
33.572280	1832.181442	17.317837
33.192206	1820.288750	17.322855
33.128071	1804.951584	17.327872
33.181341	1826.880861	17.332890
33.780961	1831.258826	17.337907
33.399560	1817.234045	17.342925
33.193075	1813.580433	17.347943
33.593408	1819.012668	17.352960
33.317378	1827.656946	17.357978
33.282877	1842.324309	17.362995
33.465128	1828.519570	17.368013
33.575233	1830.953373	17.373031
33.858334	1825.313149	17.378048
33.772296	1822.124242	17.383066
33.547395	1827.567100	17.388083
33.837389	1822.957639	17.393101
33.546812	1827.505062	17.398119
34.036934	1824.074681	17.403136
33.796468	1828.875621	17.408154
33.810748	1823.182667	17.413171
34.190597	1826.822211	17.418189
33.891125	1823.489117	17.423207
34.186748	1818.957859	17.428224
34.084996	1829.697322	17.433242
33.773291	1828.006825	17.438259
33.831203	1821.547188	17.443277
33.913696	1825.655663	17.448295
34.175324	1827.688385	17.453312
34.303275	1830.176714	17.458330
33.984467	1829.366145	17.463347
34.240998	1824.460252	17.468365
33.865359	1827.839857	17.473383
33.716677	1821.710104	17.478400
33.993189	1833.385368	17.483418
34.073806	1845.117490	17.488435
34.044352	1846.718489	17.493453
34.174307	1857.326686	17.498471
34.328973	1857.906630	17.503488
34.291008	1862.203962	17.508506
33.999490	1858.932930	17.513523
34.557067	1854.024421	17.518541
34.435741	1863.500988	17.523559
34.610713	1853.077405	17.528576
34.530861	1862.508914	17.533594
34.615476	1886.670914	17.538611
35.047123	1883.230911	17.543629
34.781771	1882.386684	17.548647
34.882243	1867.861188	17.553664
34.983086	1856.597897	17.558682
34.442586	1862.416263	17.563699
34.993706	1862.193144	17.568717
35.113939	1871.276954	17.573735
35.249421	1859.486657	17.578752
34.941757	1864.101488	17.583770
34.941943	1849.800887	17.588787
35.152931	1846.962794	17.593805
34.933568	1851.981904	17.598823
35.174513	1844.873435	17.603840
34.817389	1861.634427	17.608858
34.943821	1869.931764	17.613875
35.095908	1875.376780	17.618893
34.759966	1885.862144	17.623911
35.188826	1879.632793	17.628928
34.833834	1876.268723	17.633946
35.248582	1887.279394	17.638963
35.245601	1872.038730	17.643981
35.063248	1884.093566	17.648999
35.443227	1892.003255	17.654016
35.486058	1906.800788	17.659034
35.816155	1915.703019	17.664051
35.871371	1899.621572	17.669069
35.544382	1881.558518	17.674087
35.886821	1873.035569	17.679104
35.538020	1873.678019	17.684122
35.711842	1869.779131	17.689139
36.047974	1886.431650	17.694157
35.576761	1880.339141	17.699175
35.323095	1882.187117	17.704192
35.626314	1889.420133	17.709210
35.793026	1898.843119	17.714227
35.944706	1893.112426	17.719245
35.687595	1897.948034	17.724263
35.685066	1906.248241	17.729280
35.822322	1904.520793	17.734298
35.980325	1902.596993	17.739315
36.408539	1890.338505	17.744333
36.388959	1901.204963	17.749351
36.068184	1893.806019	17.754368
36.010439	1896.834566	17.759386
36.024732	1900.685058	17.764403
36.289025	1893.903415	17.769421
36.049493	1900.471576	17.774439
36.585308	1914.520541	17.779456
36.438168	1912.427186	17.784474
36.353091	1907.142394	17.789491
36.641729	1905.233182	17.794509
36.288380	1923.600337	17.799527
36.452432	1931.955259	17.804544
36.635676	1930.357203	17.809562
36.740714	1931.546561	17.814579
36.971462	1926.823649	17.819597
36.953410	1917.205625	17.824615
36.616848	1906.630883	17.829632
36.851599	1897.118255	17.834650
36.654660	1900.989158	17.839667
36.615783	1901.567295	17.844685
36.749382	1919.088835	17.849703
36.596270	1926.999808	17.854720
37.012894	1928.478915	17.859738
37.048259	1932.914126	17.864755
36.843909	1924.743904	17.869773
36.817541	1929.638558	17.874791
36.925852	1929.693887	17.879808
36.869436	1925.290187	17.884826
36.757148	1924.895817	17.889843
36.816898	1922.666231	17.894861
36.883192	1932.832257	17.899879
37.037712	1942.562806	17.904896
37.289918	1941.028528	17.909914
37.464889	1957.385362	17.914931
37.532983	1942.831693	17.919949
37.461803	1956.015836	17.924967
37.559233	1944.506979	17.929984
37.429489	1940.599285	17.935002
37.644001	1941.989024	17.940019
37.700127	1919.750197	17.945037
37.623036	1923.720553	17.950055
37.567106	1923.680243	17.955072
37.485766	1919.425950	17.960090
37.309152	1930.431821	17.965107
37.815984	1935.169677	17.970125
37.563549	1946.303864	17.975143
37.543037	1949.974695	17.980160
37.682353	1941.942441	17.985178
37.615035	1937.798421	17.990195
37.859249	1939.450177	17.995213
37.802626	1941.734831	18.000231
37.691041	1945.056561	18.005248
37.987885	1932.946963	18.010266
37.977212	1936.692541	18.015283
38.152635	1935.471377	18.020301
38.042105	1941.337865	18.025319
38.140945	1935.026131	18.030336
38.506197	1929.558884	18.035354
38.174801	1943.984162	18.040371
38.201603	1934.617759	18.045389
38.673607	1940.809051	18.050407
38.508238	1943.381404	18.055424
38.507666	1932.778172	18.060442
38.439879	1936.358007	18.065459
38.606809	1933.344514	18.070477
38.608771	1933.244616	18.075495
38.531520	1937.139411	18.080512
38.638112	1931.831927	18.085530
38.613871	1940.834581	18.090547
38.526401	1931.524112	18.095565
38.345732	1946.759883	18.100583
38.890234	1954.352196	18.105600
38.742080	1969.728277	18.110618
38.973849	1982.907160	18.115635
39.058276	1972.933147	18.120653
39.000498	1959.434187	18.125671
39.097483	1954.977517	18.130688
38.998429	1938.992050	18.135706
38.345204	1944.733440	18.140723
38.560304	1960.854889	18.145741
38.801343	1963.174116	18.150759
38.967198	1964.019934	18.155776
39.142109	1960.707864	18.160794
38.721122	1968.392344	18.165811
38.774273	1960.222771	18.170829
39.124763	1969.793324	18.175847
39.395013	1984.593825	18.180864
39.618074	1981.642289	18.185882
39.314654	1994.796417	18.190899
39.549743	1987.963269	18.195917
39.695940	1997.876338	18.200935
39.529210	1988.165170	18.205952
39.607406	1987.633347	18.210970
39.699710	1992.499708	18.215987
40.014195	1973.429907	18.221005
39.608140	1965.817092	18.226023
39.409703	1963.346389	18.231040
39.588437	1966.992498	18.236058
39.738252	1981.942864	18.241075
39.737226	1980.634378	18.246093
39.747062	1983.905694	18.251111
39.749939	1981.782370	18.256128
39.944126	1982.416800	18.261146
39.672303	1990.408488	18.266163
39.897521	1981.958436	18.271181
39.821513	1979.824158	18.276199
39.924476	1983.841488	18.281216
40.061779	1982.367179	18.286234
39.790477	1978.094325	18.291251
39.803162	1977.050111	18.296269
39.924533	1983.457359	18.301287
40.249649	2003.744984	18.306304
40.285282	2004.906076	18.311322
40.378466	2011.627854	18.316339
40.575845	2009.339244	18.321357
40.114087	1999.420224	18.326375
40.180708	2008.456692	18.331392
40.690200	2004.076585	18.336410
40.483954	2002.917043	18.341427
40.785678	2001.909218	18.346445
40.946495	2007.841430	18.351463
40.615899	2007.659590	18.356480
40.967050	2004.121864	18.361498
40.454181	2007.890382	18.366515
40.732067	2006.024672	18.371533
40.933356	1999.725082	18.376551
40.748541	2008.807122	18.381568
41.136343	1999.145857	18.386586
40.870520	2000.912787	18.391603
40.793673	2001.324770	18.396621
40.980386	2001.809254	18.401639
40.971799	2007.812432	18.406656
40.986610	1997.489686	18.411674
40.858382	1999.567697	18.416691
40.984387	1997.043658	18.421709
40.971749	2002.808916	18.426727
40.547161	2013.710235	18.431744
41.031495	2016.212023	18.436762
40.968290	2017.629647	18.441779
40.738643	2017.179509	18.446797
41.275745	2024.201414	18.451815
41.365157	2042.377278	18.456832
41.513429	2040.542082	18.461850
41.308780	2051.942848	18.466867
41.409066	2053.641285	18.471885
41.799152	2046.897015	18.476903
41.825996	2051.175793	18.481920
42.010640	2036.627146	18.486938
41.731444	2036.021822	18.491955
41.556937	2044.466727	18.496973
41.678806	2047.891556	18.501991
41.584562	2048.522569	18.507008
42.181216	2045.646956	18.512026
41.868861	2054.162332	18.517043
41.821200	2045.734990	18.522061
42.171948	2045.041888	18.527079
41.920429	2050.316392	18.532096
42.161754	2035.954034	18.537114
42.037723	2038.366010	18.542131
41.974626	2042.806927	18.547149
42.305614	2050.696463	18.552167
42.256317	2065.149157	18.557184
42.900567	2052.639015	18.562202
42.385109	2051.076329	18.567219
42.021505	2045.119482	18.572237
42.522506	2049.787078	18.577255
42.475897	2058.890752	18.582272
42.894185	2058.191583	18.587290
42.565421	2053.633333	18.592307
42.841908	2051.024522	18.597325
42.449079	2033.243460	18.602343
42.308653	2058.582393	18.607360
42.635841	2059.482212	18.612378
42.794629	2061.158757	18.617395
42.866274	2054.934551	18.622413
42.663761	2058.315065	18.627431
42.615616	2069.745835	18.632448
42.492351	2063.983835	18.637466
43.049708	2067.100328	18.642483
43.148495	2062.466946	18.647501
43.074357	2052.078576	18.652519
42.741235	2059.541853	18.657536
43.162635	2050.621470	18.662554
43.141909	2067.047835	18.667571
43.169393	2069.400473	18.672589
43.377106	2073.772932	18.677607
43.380705	2083.943534	18.682624
43.319961	2078.762531	18.687642
43.150577	2088.367275	18.692659
43.594053	2081.064527	18.697677
43.638750	2088.893613	18.702695
43.683284	2084.221175	18.707712
43.868023	2082.281114	18.712730
43.773640	2089.178872	18.717747
43.896249	2091.484264	18.722765
44.050248	2086.394081	18.727783
44.006713	2067.570464	18.732800
44.291620	2052.526052	18.737818
43.946826	2048.662997	18.742835
43.337408	2045.698116	18.747853
43.974463	2055.252766	18.752871
44.246093	2058.731148	18.757888
44.326479	2050.100312	18.762906
44.130717	2045.481457	18.767923
43.905458	2044.752237	18.772941
44.281438	2035.799619	18.777959
44.025666	2032.213566	18.782976
44.509720	2047.903945	18.787994
44.214705	2054.684906	18.793011
44.070534	2066.251658	18.798029
44.474520	2075.752393	18.803047
44.373950	2081.184594	18.808064
44.613671	2078.183036	18.813082
44.319579	2073.364701	18.818099
44.109414	2076.860661	18.823117
44.595670	2072.321781	18.828135
44.562368	2072.100159	18.833152
44.393850	2070.191823	18.838170
44.403330	2074.003391	18.843187
44.398834	2074.764429	18.848205
44.763855	2072.536241	18.853223
44.685956	2094.302178	18.858240
44.921502	2097.627090	18.863258
45.307341	2104.024454	18.868275
44.884451	2109.785244	18.873293
45.183346	2097.776362	18.878311
44.936299	2104.236400	18.883328
44.584296	2111.295729	18.888346
44.961331	2104.891008	18.893363
44.815733	2103.000134	18.898381
45.181344	2103.704217	18.903399
44.965752	2106.814851	18.908416
45.271236	2098.848310	18.913434
45.542387	2106.242649	18.918451
44.997442	2110.456673	18.923469
45.387151	2116.090386	18.928487
45.360746	2134.745393	18.933504
45.388620	2134.595532	18.938522
45.585821	2132.584502	18.943539
45.389588	2131.226829	18.948557
45.719988	2122.167926	18.953575
45.554087	2141.474801	18.958592
45.595413	2123.811118	18.963610
45.735621	2121.129190	18.968627
45.641632	2132.209319	18.973645
45.954598	2120.557944	18.978663
45.640403	2125.794425	18.983680
45.959860	2137.779354	18.988698
45.828635	2149.174333	18.993715
45.819391	2156.809622	18.998733
45.745249	2150.888662	19.003751
46.010540	2156.005573	19.008768
46.059041	2158.072844	19.013786
46.346370	2154.346829	19.018803
46.118613	2153.253832	19.023821
46.452596	2143.230117	19.028839
46.339929	2149.776587	19.033856
46.453421	2150.917711	19.038874
46.432938	2148.805319	19.043891
46.436581	2169.111352	19.048909
46.872804	2172.172727	19.053927
46.806579	2177.843771	19.058944
46.904766	2174.121905	19.063962
46.871578	2150.456935	19.068979
46.599193	2143.345930	19.073997
46.854633	2149.683801	19.079015
46.876564	2167.783188	19.084032
46.840155	2173.861906	19.089050
46.956837	2170.169656	19.094067
46.716080	2179.846907	19.099085
46.966355	2168.829127	19.104103
46.956679	2175.844791	19.109120
46.815270	2170.153081	19.114138
47.344558	2172.468705	19.119155
47.055902	2171.201139	19.124173
47.369575	2164.539553	19.129191
47.186317	2172.845027	19.134208
47.149227	2170.713334	19.139226
47.425816	2171.466021	19.144243
47.365136	2183.719059	19.149261
47.641601	2188.804208	19.154279
47.567993	2198.967196	19.159296
47.528786	2188.884379	19.164314
47.991794	2185.158007	19.169331
47.713506	2186.667563	19.174349
48.142455	2183.541340	19.179367
48.424884	2176.725469	19.184384
47.982289	2164.833808	19.189402
48.286799	2145.598908	19.194419
48.024431	2153.271780	19.199437
48.202231	2146.553565	19.204455
47.896625	2155.026144	19.209472
48.094687	2151.715318	19.214490
48.227540	2143.287166	19.219507
47.941200	2144.564973	19.224525
48.275934	2154.767406	19.229543
48.522303	2159.553188	19.234560
48.312026	2174.368085	19.239578
48.443059	2154.669756	19.244595
48.298150	2176.594941	19.249613
48.376104	2172.290578	19.254631
48.219035	2179.805864	19.259648
48.193870	2182.555834	19.264666
48.185128	2182.099821	19.269683
48.102202	2189.485507	19.274701
48.697080	2179.452821	19.279719
48.149849	2188.070944	19.284736
48.130440	2201.864462	19.289754
48.808556	2198.004825	19.294771
48.829630	2200.508156	19.299789
49.144325	2200.591125	19.304807
49.083926	2205.722218	19.309824
49.014763	2208.510582	19.314842
49.119471	2199.373648	19.319859
49.323128	2198.426540	19.324877
49.305327	2208.189729	19.329895
49.267168	2206.081043	19.334912
49.317749	2199.897670	19.339930
49.696568	2196.545486	19.344947
49.544117	2202.479645	19.349965
49.318236	2193.119494	19.354983
49.494922	2203.391833	19.360000
49.398733	2198.675338	19.365018
49.431995	2193.868114	19.370035
49.279077	2199.237368	19.375053
49.718667	2193.063601	19.380071
49.875172	2193.429861	19.385088
49.871283	2199.964638	19.390106
49.892025	2191.494787	19.395123
49.640657	2198.116608	19.400141
49.822803	2195.653716	19.405159
50.065910	2198.371864	19.410176
49.773681	2217.492657	19.415194
50.294641	2221.920772	19.420211
49.999330	2223.397716	19.425229
49.979171	2221.112025	19.430247
50.314646	2226.691765	19.435264
49.754738	2224.544666	19.440282
50.153597	2223.343965	19.445299
50.181509	2223.456706	19.450317
50.046956	2211.198633	19.455335
50.160477	2226.644634	19.460352
49.986205	2246.514858	19.465370
50.423975	2242.144594	19.470387
50.267081	2258.637412	19.475405
50.293704	2257.513702	19.480423
50.864615	2246.828616	19.485440
50.741938	2252.279105	19.490458
51.034827	2241.415248	19.495475
50.815913	2254.011091	19.500493
51.140485	2244.234156	19.505511
51.051813	2254.905208	19.510528
50.836616	2252.942372	19.515546
51.060832	2244.119888	19.520563
50.860675	2257.303202	19.525581
51.244959	2265.439545	19.530599
51.232293	2279.854876	19.535616
50.826894	2279.813769	19.540634
51.448327	2269.408109	19.545651
51.270445	2278.806888	19.550669
51.628539	2272.752495	19.555687
51.603928	2270.837234	19.560704
51.260754	2276.930568	19.565722
51.588780	2276.266417	19.570739
51.414833	2280.659613	19.575757
51.600240	2282.184131	19.580775
51.598422	2286.220465	19.585792
51.590056	2278.498725	19.590810
51.830622	2276.463959	19.595827
51.809521	2277.200591	19.600845
51.652093	2282.703697	19.605863
52.014928	2293.056692	19.610880
51.992191	2298.822551	19.615898
52.279151	2304.277277	19.620915
52.104391	2314.681510	19.625933
52.208825	2305.324865	19.630951
52.435102	2297.207553	19.635968
52.201275	2300.835833	19.640986
52.505157	2301.373369	19.646003
52.490035	2300.380984	19.651021
52.663286	2297.055337	19.656039
52.289859	2282.676435	19.661056
52.045155	2291.309088	19.666074
52.297902	2292.815369	19.671091
52.356581	2297.316118	19.676109
52.490223	2293.114710	19.681127
52.737670	2288.306638	19.686144
52.990669	2295.170980	19.691162
52.855770	2284.708260	19.696179
52.727192	2293.041358	19.701197
52.445877	2294.663635	19.706215
52.937942	2293.153782	19.711232
53.021870	2320.605295	19.716250
53.102542	2316.967795	19.721267
53.388935	2316.590077	19.726285
53.117732	2330.623838	19.731303
53.477856	2310.978719	19.736320
53.299184	2320.935553	19.741338
53.513488	2315.020313	19.746355
53.463794	2321.782421	19.751373
53.622029	2310.923490	19.756391
53.567821	2317.510746	19.761408
53.336636	2313.946935	19.766426
53.271107	2307.083503	19.771443
53.345918	2300.850013	19.776461
53.521499	2311.527348	19.781479
53.885597	2308.177971	19.786496
53.451096	2326.080275	19.791514
54.228018	2329.709311	19.796531
54.178611	2342.730327	19.801549
54.117968	2338.026408	19.806567
54.326702	2346.291867	19.811584
54.069030	2345.241213	19.816602
54.321546	2343.913942	19.821619
54.358935	2343.056172	19.826637
54.167067	2350.370600	19.831655
54.491384	2348.959782	19.836672
54.478430	2348.509579	19.841690
54.424690	2340.996906	19.846707
54.482826	2346.322207	19.851725
54.470567	2347.368415	19.856743
54.875399	2337.772629	19.861760
54.517332	2342.829824	19.866778
54.632490	2338.903917	19.871795
54.610645	2335.666083	19.876813
54.639513	2341.343882	19.881831
54.758231	2340.312402	19.886848
54.600961	2339.516001	19.891866
54.762029	2333.294594	19.896883
54.654339	2337.711088	19.901901
54.573302	2354.343422	19.906919
55.363291	2362.728005	19.911936
54.960209	2369.681729	19.916954
54.767838	2359.904491	19.921971
55.068540	2374.510156	19.926989
54.504922	2368.716625	19.932007
55.247285	2381.996347	19.937024
55.294127	2392.638753	19.942042
55.173683	2397.889307	19.947059
55.544268	2396.831078	19.952077
55.598723	2385.099078	19.957095
55.552234	2383.815410	19.962112
55.632905	2390.063417	19.967130
55.636858	2390.773857	19.972147
55.612448	2388.234108	19.977165
55.807944	2392.970510	19.982183
56.073900	2401.886793	19.987200
56.093978	2407.494415	19.992218
56.152531	2408.043444	19.997235
56.414836	2403.365167	20.002253
56.142950	2400.574649	20.007271
56.353361	2386.219057	20.012288
56.445740	2386.523890	20.017306
56.251457	2396.855816	20.022323
56.329626	2387.130618	20.027341
56.112181	2406.415252	20.032359
56.764766	2403.353535	20.037376
56.455067	2408.122807	20.042394
56.549511	2401.791139	20.047411
56.716093	2396.142838	20.052429
56.534300	2400.939355	20.057447
56.986501	2401.191299	20.062464
56.781851	2398.857781	20.067482
56.667150	2394.130512	20.072499
56.556716	2396.007587	20.077517
56.594385	2400.783512	20.082535
56.858641	2417.378029	20.087552
56.637053	2429.551600	20.092570
56.614164	2432.358720	20.097587
56.925827	2438.012957	20.102605
56.969084	2431.772828	20.107623
57.094932	2440.343416	20.112640
57.361756	2452.730240	20.117658
57.495365	2459.743566	20.122675
57.825254	2459.144852	20.127693
57.748057	2460.712872	20.132711
57.703607	2444.542636	20.137728
57.533035	2450.825971	20.142746
57.931109	2449.250561	20.147763
58.251016	2450.388238	20.152781
57.907687	2452.231046	20.157799
58.118261	2447.196736	20.162816
58.132121	2450.747813	20.167834
58.010790	2449.050920	20.172851
58.295714	2446.767436	20.177869
57.620551	2443.554687	20.182887
58.238156	2442.175221	20.187904
58.542845	2443.737487	20.192922
58.499827	2434.641807	20.197939
58.443375	2440.800330	20.202957
58.501392	2443.439323	20.207975
58.565639	2444.607916	20.212992
58.848901	2445.163047	20.218010
58.482132	2446.814056	20.223027
58.723524	2442.267583	20.228045
58.407907	2437.508999	20.233063
58.230732	2440.405846	20.238080
58.642112	2456.607126	20.243098
58.481463	2464.750340	20.248115
58.984147	2458.017567	20.253133
59.099858	2467.604865	20.258151
59.108306	2463.735576	20.263168
58.797842	2474.120258	20.268186
59.064722	2467.936397	20.273203
59.131883	2469.791948	20.278221
59.178771	2469.207416	20.283239
59.203122	2461.008883	20.288256
59.151388	2462.570324	20.293274
59.416532	2483.245300	20.298291
59.419106	2485.089105	20.303309
59.581128	2491.454005	20.308327
59.868024	2487.143699	20.313344
60.071858	2495.830152	20.318362
59.918446	2493.962178	20.323379
60.186843	2488.671415	20.328397
59.909424	2495.210662	20.333415
60.126686	2481.319623	20.338432
59.983779	2487.126318	20.343450
60.141579	2486.500584	20.348467
60.154560	2487.559159	20.353485
59.978385	2487.345440	20.358503
60.095348	2481.008436	20.363520
60.272388	2479.605459	20.368538
60.287045	2475.892627	20.373555
60.401675	2468.309097	20.378573
60.241951	2483.655709	20.383591
60.618057	2473.929944	20.388608
60.317266	2469.655929	20.393626
60.370154	2474.646298	20.398643
60.715657	2486.104322	20.403661
60.796492	2498.165267	20.408679
60.853862	2497.321110	20.413696
60.869216	2508.812165	20.418714
61.164411	2507.869568	20.423731
61.004005	2502.570667	20.428749
60.884370	2501.807397	20.433767
61.181210	2506.661706	20.438784
60.901059	2510.005956	20.443802
60.906992	2505.483886	20.448819
61.201740	2500.755717	20.453837
61.180842	2512.340578	20.458855
61.226543	2522.165105	20.463872
61.282851	2529.306624	20.468890
61.204653	2532.388684	20.473907
61.445849	2532.288935	20.478925
61.506171	2534.942916	20.483943
61.471799	2536.975927	20.488960
61.440140	2541.273583	20.493978
61.630606	2545.669900	20.498995
61.563744	2544.966004	20.504013
61.638625	2557.441391	20.509031
61.967842	2557.553851	20.514048
62.125964	2560.907040	20.519066
62.289807	2556.865531	20.524083
62.560923	2552.879493	20.529101
62.147485	2563.064343	20.534119
62.829220	2552.213446	20.539136
62.598833	2549.652658	20.544154
62.517187	2554.132226	20.549171
62.382977	2549.946754	20.554189
62.419528	2558.650312	20.559207
62.545327	2559.968968	20.564224
62.909141	2568.237609	20.569242
63.219695	2573.678680	20.574259
62.819529	2572.359854	20.579277
62.862419	2573.052436	20.584295
63.215688	2574.346026	20.589312
63.479216	2561.137454	20.594330
62.998576	2582.598693	20.599347
63.394059	2569.028479	20.604365
63.213847	2569.505233	20.609383
63.313984	2572.407762	20.614400
63.158874	2567.688706	20.619418
62.970549	2570.895315	20.624435
63.233828	2560.612159	20.629453
63.411349	2569.642402	20.634471
63.207425	2567.790657	20.639488
63.257474	2562.419483	20.644506
63.365337	2582.627298	20.649523
64.044520	2588.401846	20.654541
63.661455	2598.469872	20.659559
63.692095	2587.438164	20.664576
63.831190	2594.436469	20.669594
64.040546	2594.125836	20.674611
64.358146	2590.488019	20.679629
63.830114	2597.994849	20.684647
63.906497	2592.255502	20.689664
64.371976	2593.778165	20.694682
64.248415	2612.987268	20.699699
64.300739	2611.502956	20.704717
64.467490	2617.724201	20.709735
64.804517	2614.619810	20.714752
64.905184	2612.575882	20.719770
64.557832	2616.988042	20.724787
65.088802	2603.449305	20.729805
64.783584	2605.231879	20.734823
65.054483	2609.232588	20.739840
65.145313	2609.022295	20.744858
64.810936	2609.395042	20.749875
65.183789	2606.526862	20.754893
65.017305	2610.111382	20.759911
65.334666	2611.302253	20.764928
65.063212	2608.790776	20.769946
64.667161	2614.620144	20.774963
64.985287	2609.549073	20.779981
65.251160	2630.409569	20.784999
65.715493	2644.195823	20.790016
65.680224	2640.253409	20.795034
65.313356	2653.509153	20.800051
65.728919	2639.170937	20.805069
65.673895	2639.656099	20.810087
65.471840	2644.851347	20.815104
65.763495	2648.647435	20.820122
65.476986	2644.078861	20.825139
65.922387	2654.988544	20.830157
65.875076	2671.204581	20.835175
66.191994	2672.431359	20.840192
66.259048	2669.033056	20.845210
66.136242	2668.605364	20.850227
66.422905	2667.852373	20.855245
66.526800	2670.162920	20.860263
66.341246	2666.296176	20.865280
66.541562	2658.647573	20.870298
66.574718	2676.641355	20.875315
66.667173	2689.272610	20.880333
66.931757	2698.381430	20.885351
66.797429	2703.933225	20.890368
67.084105	2696.786481	20.895386
67.008140	2691.380220	20.900403
67.181718	2690.450664	20.905421
67.131294	2689.702698	20.910439
67.075022	2698.774091	20.915456
67.765707	2685.551379	20.920474
67.298912	2687.294178	20.925491
67.475053	2686.944158	20.930509
67.330681	2684.440369	20.935527
67.750336	2690.689456	20.940544
67.770157	2678.197171	20.945562
67.346918	2688.229777	20.950579
67.378080	2683.102256	20.955597
67.420445	2685.549774	20.960615
67.526923	2688.730428	20.965632
67.887435	2688.629820	20.970650
67.469918	2698.598489	20.975667
67.642375	2701.599704	20.980685
67.911794	2699.559321	20.985703
68.114575	2701.886178	20.990720
68.427521	2699.891346	20.995738
67.987043	2704.797330	21.000755
68.232124	2701.058102	21.005773
68.441810	2697.068419	21.010791
68.394213	2707.021118	21.015808
68.467494	2711.086862	21.020826
68.605412	2722.105386	21.025843
68.783394	2722.475584	21.030861
69.063549	2729.996301	21.035879
68.597729	2731.530266	21.040896
69.101699	2717.156078	21.045914
69.058494	2727.469112	21.050931
69.087920	2724.973154	21.055949
69.384635	2721.749424	21.060967
69.012750	2721.553146	21.065984
68.920742	2725.150559	21.071002
69.056965	2727.898313	21.076019
69.435691	2714.233892	21.081037
69.248605	2714.594850	21.086055
68.920141	2727.995884	21.091072
69.438644	2735.280271	21.096090
69.063091	2754.669473	21.101107
69.334091	2746.411837	21.106125
69.416050	2754.864267	21.111143
69.633803	2767.665403	21.116160
69.780546	2780.618081	21.121178
69.931630	2786.356520	21.126195
70.184872	2782.689943	21.131213
70.296633	2781.057179	21.136231
70.055194	2786.936998	21.141248
70.431586	2771.710199	21.146266
70.272092	2777.129168	21.151283
70.244500	2772.075525	21.156301
70.287652	2765.361230	21.161319
70.205374	2782.906891	21.166336
71.023493	2784.809799	21.171354
70.696952	2800.392628	21.176371
71.146618	2797.210491	21.181389
71.314820	2795.186067	21.186407
71.271058	2794.545269	21.191424
71.119782	2771.891895	21.196442
71.093074	2770.916359	21.201459
71.194254	2763.000636	21.206477
71.164353	2770.371124	21.211495
71.193659	2788.142034	21.216512
71.443705	2793.147106	21.221530
71.348533	2790.058731	21.226547
71.565061	2792.286468	21.231565
71.928767	2793.735053	21.236583
71.352385	2791.251202	21.241600
71.393539	2786.290116	21.246618
71.220439	2784.904929	21.251635
71.356770	2791.000563	21.256653
71.560608	2805.760481	21.261671
71.835541	2811.635520	21.266688
72.211753	2813.584043	21.271706
71.991047	2816.101916	21.276723
72.124280	2811.587421	21.281741
72.423430	2816.161110	21.286759
71.947161	2823.948474	21.291776
72.498515	2809.848661	21.296794
72.705750	2815.319525	21.301811
72.376801	2814.778709	21.306829
72.393236	2817.619547	21.311847
72.574232	2833.514068	21.316864
73.198394	2826.428322	21.321882
73.022295	2839.468368	21.326899
73.049555	2831.965669	21.331917
73.434272	2828.684823	21.336935
73.414385	2824.389001	21.341952
73.461464	2801.523591	21.346970
73.079961	2797.077009	21.351987
72.872969	2798.261012	21.357005
73.222809	2814.664998	21.362023
73.056219	2829.238618	21.367040
73.293174	2828.895457	21.372058
73.416515	2840.328715	21.377075
73.308724	2838.184619	21.382093
73.603884	2828.720089	21.387111
73.273492	2840.246196	21.392128
73.827457	2844.513899	21.397146
73.871268	2869.959875	21.402163
73.904982	2866.388689	21.407181
73.913210	2859.346645	21.412199
73.961324	2870.303366	21.417216
74.113335	2858.701719	21.422234
74.177550	2858.333613	21.427251
73.851764	2859.691634	21.432269
74.410731	2869.455015	21.437287
73.867700	2890.712028	21.442304
74.618707	2886.245624	21.447322
74.359555	2890.897606	21.452339
74.278820	2892.393414	21.457357
74.731625	2898.498504	21.462375
74.762140	2914.758211	21.467392
75.040203	2915.579204	21.472410
74.867213	2911.472896	21.477427
75.262567	2917.267795	21.482445
75.212219	2917.358457	21.487463
75.268299	2922.620905	21.492480
75.380299	2908.516188	21.497498
75.466611	2918.667340	21.502515
75.267831	2916.331589	21.507533
75.169984	2905.815855	21.512551
75.478956	2918.470110	21.517568
75.782201	2935.977306	21.522586
75.908705	2938.156580	21.527603
75.912596	2940.874311	21.532621
76.052432	2951.229631	21.537639
75.604047	2942.578762	21.542656
76.023794	2935.329160	21.547674
76.031971	2946.219707	21.552691
75.929742	2946.804434	21.557709
75.958040	2941.236714	21.562727
76.105583	2953.942928	21.567744
76.789988	2955.392762	21.572762
76.831600	2959.623278	21.577779
76.848663	2963.426720	21.582797
76.847866	2950.610437	21.587815
76.998848	2968.310219	21.592832
77.149525	2955.225522	21.597850
77.362976	2961.171434	21.602867
77.007404	2950.261299	21.607885
77.024780	2947.851166	21.612903
76.977161	2952.095667	21.617920
77.197367	2947.487592	21.622938
77.340397	2948.221882	21.627955
76.998067	2944.985803	21.632973
77.561845	2947.476169	21.637991
77.539057	2958.734875	21.643008
77.356296	2946.790136	21.648026
77.748567	2946.425586	21.653043
77.712953	2949.060088	21.658061
78.093260	2947.693496	21.663079
77.656776	2947.146069	21.668096
77.937019	2952.962404	21.673114
78.073778	2964.155716	21.678131
78.174455	2978.368657	21.683149
78.309072	2974.316131	21.688167
77.799652	2976.193981	21.693184
78.142136	2972.513370	21.698202
78.304256	2966.643931	21.703219
78.145493	2972.221128	21.708237
78.546181	2971.858333	21.713255
78.112935	2979.157506	21.718272
78.047400	2990.779643	21.723290
78.337317	3001.386547	21.728307
78.292368	3007.962324	21.733325
78.986173	3027.065730	21.738343
78.750687	3029.008079	21.743360
79.084786	3028.153115	21.748378
79.190390	3037.451860	21.753395
78.958404	3033.453329	21.758413
79.257730	3026.617756	21.763431
79.154252	3034.832516	21.768448
79.141966	3049.307555	21.773466
79.556218	3046.253686	21.778483
79.635542	3063.168911	21.783501
79.964698	3058.645922	21.788519
79.858244	3057.021307	21.793536
79.881295	3060.998207	21.798554
80.052197	3054.897338	21.803571
79.847445	3061.601970	21.808589
79.964573	3058.223640	21.813607
80.467510	3070.015510	21.818624
80.466888	3080.210298	21.823642
80.592542	3078.261788	21.828659
80.630271	3079.129674	21.833677
80.864640	3072.519030	21.838695
80.623992	3075.581634	21.843712
80.924106	3077.762105	21.848730
81.086323	3069.835333	21.853747
80.715377	3067.221740	21.858765
80.823008	3067.073626	21.863783
80.698312	3068.537356	21.868800
80.805384	3071.787682	21.873818
80.938530	3063.590898	21.878835
81.190013	3088.439799	21.883853
81.446441	3096.232758	21.888871
81.592063	3088.900119	21.893888
81.112918	3098.136655	21.898906
81.457179	3091.456621	21.903923
81.531752	3098.674518	21.908941
81.500203	3095.467663	21.913959
81.444583	3112.471041	21.918976
81.810389	3124.161631	21.923994
82.358916	3121.088663	21.929011
81.917593	3132.319149	21.934029
82.282757	3120.753280	21.939047
82.292967	3131.751110	21.944064
82.223498	3124.782447	21.949082
82.394110	3119.124164	21.954099
82.318258	3122.461881	21.959117
82.481229	3131.887811	21.964135
82.691530	3150.588312	21.969152
82.909108	3145.508520	21.974170
82.825804	3136.224988	21.979187
82.853322	3147.144759	21.984205
83.131924	3155.460899	21.989223
83.163152	3155.339217	21.994240
82.996897	3152.492090	21.999258
83.116126	3148.803520	22.004275
83.085999	3155.557630	22.009293
83.076598	3143.343460	22.014311
83.050752	3151.900186	22.019328
83.298149	3171.785631	22.024346
83.416590	3175.349482	22.029363
83.605986	3172.478898	22.034381
83.411085	3169.673129	22.039399
83.474281	3175.318380	22.044416
83.826420	3191.143192	22.049434
83.916333	3192.018586	22.054451
83.816437	3204.684865	22.059469
84.110621	3195.451796	22.064487
84.260265	3203.710960	22.069504
84.095410	3197.784148	22.074522
84.337919	3204.036396	22.079539
84.507424	3220.463584	22.084557
84.729770	3224.425244	22.089575
85.220466	3216.843261	22.094592
84.783766	3219.782435	22.099610
85.082261	3215.499541	22.104627
85.265563	3215.805874	22.109645
85.170026	3208.156381	22.114663
85.142740	3218.895493	22.119680
85.569557	3213.086080	22.124698
85.753270	3209.901832	22.129715
85.296468	3210.138152	22.134733
85.679840	3212.762383	22.139751
85.523666	3205.797410	22.144768
85.499735	3204.438671	22.149786
85.862290	3205.763066	22.154803
85.911102	3207.059088	22.159821
86.107806	3198.858797	22.164839
85.959121	3208.285586	22.169856
85.989169	3208.359000	22.174874
86.390598	3224.757634	22.179891
86.326728	3238.317673	22.184909
86.128889	3242.827309	22.189927
86.218988	3240.551955	22.194944
86.412500	3245.160982	22.199962
86.875494	3237.790290	22.204979
86.577358	3242.492536	22.209997
86.805523	3234.134245	22.215015
86.904531	3233.985195	22.220032
86.300188	3239.671703	22.225050
87.005381	3253.689514	22.230067
87.049545	3264.577867	22.235085
87.096253	3259.815732	22.240103
87.205812	3265.043059	22.245120
87.012910	3273.868090	22.250138
87.305005	3268.128213	22.255155
87.399790	3288.088689	22.260173
87.395828	3299.836307	22.265191
87.411070	3289.820148	22.270208
87.218608	3282.036652	22.275226
87.777517	3301.522220	22.280243
87.754285	3320.784091	22.285261
87.778466	3316.675346	22.290279
87.761805	3310.039232	22.295296
87.877403	3314.408790	22.300314
88.452697	3332.028490	22.305331
88.342793	3345.188326	22.310349
88.518913	3338.526578	22.315367
88.959921	3347.260074	22.320384
88.755152	3344.727590	22.325402
88.935456	3341.930536	22.330419
89.107628	3339.338789	22.335437
89.090118	3344.831305	22.340455
89.400322	3340.992157	22.345472
89.351928	3343.216985	22.350490
89.628557	3333.494168	22.355507
89.297210	3343.232416	22.360525
89.324907	3335.070276	22.365543
89.420810	3333.251871	22.370560
89.572160	3338.614052	22.375578
89.622936	3331.515925	22.380595
89.558762	3329.909087	22.385613
89.644494	3332.342045	22.390631
89.520012	3324.543334	22.395648
89.672103	3344.726308	22.400666
89.864610	3358.195569	22.405683
90.203846	3357.880744	22.410701
90.450047	3362.058593	22.415719
90.596670	3356.091169	22.420736
90.151781	3361.851723	22.425754
90.231765	3358.964966	22.430771
90.149264	3378.430445	22.435789
90.077389	3396.464104	22.440807
90.473764	3394.390405	22.445824
90.093784	3392.996893	22.450842
90.636360	3412.373481	22.455859
90.878350	3425.165239	22.460877
91.065663	3427.057316	22.465895
91.370822	3419.389015	22.470912
91.425875	3430.042977	22.475930
91.349187	3431.454691	22.480947
91.716696	3446.974821	22.485965
91.849645	3446.423253	22.490983
92.067152	3447.846500	22.496000
91.634014	3457.796971	22.501018
92.145275	3444.914790	22.506035
92.248554	3449.459281	22.511053
92.207515	3447.555258	22.516071
92.162033	3441.860190	22.521088
92.035739	3455.934750	22.526106
92.145912	3445.889385	22.531123
92.665130	3439.446407	22.536141
92.403560	3445.168762	22.541159
92.710664	3455.601852	22.546176
92.623328	3458.158773	22.551194
92.811876	3454.674033	22.556211
92.823854	3457.894905	22.561229
92.793342	3460.766471	22.566247
92.988463	3456.570323	22.571264
92.814921	3469.851050	22.576282
93.200520	3479.969548	22.581299
93.320810	3489.670904	22.586317
93.483621	3492.022612	22.591335
93.455436	3493.918092	22.596352
93.405072	3490.198068	22.601370
93.364054	3483.797831	22.606387
93.795492	3500.672946	22.611405
94.001098	3505.463928	22.616423
94.189905	3505.098408	22.621440
94.050755	3512.502691	22.626458
94.215726	3517.641785	22.631475
94.179159	3521.076638	22.636493
94.022598	3515.322761	22.641511
94.409446	3529.611670	22.646528
94.399400	3540.055593	22.651546
94.273742	3534.989196	22.656563
94.566181	3536.398862	22.661581
94.767025	3535.651381	22.666599
95.010112	3538.819040	22.671616
94.853349	3545.167857	22.676634
95.230171	3564.127143	22.681651
95.299569	3571.544172	22.686669
95.244840	3561.363025	22.691687
95.530695	3559.040249	22.696704
95.230076	3567.481261	22.701722
95.377250	3561.004157	22.706739
95.659908	3565.119324	22.711757
95.394464	3568.095173	22.716775
95.791762	3578.034217	22.721792
95.478348	3600.440537	22.726810
95.748205	3596.209927	22.731827
96.040402	3589.061866	22.736845
96.059719	3601.570914	22.741863
96.502824	3611.939064	22.746880
96.533102	3616.131866	22.751898
96.576232	3615.199445	22.756915
96.915534	3607.470668	22.761933
96.754277	3608.508556	22.766951
97.071226	3611.372231	22.771968
96.852548	3613.637105	22.776986
96.989522	3619.427014	22.782003
97.415899	3615.605577	22.787021
97.157869	3607.662280	22.792039
97.427367	3604.937825	22.797056
97.255570	3613.972964	22.802074
97.515804	3629.429926	22.807091
97.897588	3644.069429	22.812109
97.912630	3639.778624	22.817127
98.012727	3638.627294	22.822144
97.790940	3636.991395	22.827162
97.966201	3640.256144	22.832179
97.943497	3636.715780	22.837197
97.776883	3645.550841	22.842215
98.404205	3649.762525	22.847232
98.440911	3663.347623	22.852250
98.725754	3661.609723	22.857267
98.410298	3657.765813	22.862285
98.567038	3670.598664	22.867303
98.675955	3656.403615	22.872320
98.523678	3661.371241	22.877338
98.487971	3681.040792	22.882355
98.855430	3685.501053	22.887373
98.853338	3686.125533	22.892391
99.442376	3689.038670	22.897408
99.387654	3705.630678	22.902426
99.607389	3711.665614	22.907443
99.980479	3708.236494	22.912461
99.613598	3709.284023	22.917479
99.920896	3704.456555	22.922496
99.902557	3714.709422	22.927514
100.110018	3708.411670	22.932531
100.201927	3711.696928	22.937549
100.122680	3711.557703	22.942567
100.183392	3699.931963	22.947584
100.467551	3723.787358	22.952602
100.514864	3736.927003	22.957619
100.602116	3733.238078	22.962637
100.819573	3740.493646	22.967655
100.902902	3736.691575	22.972672
100.904676	3733.690124	22.977690
100.911402	3734.983315	22.982707
101.180554	3730.558665	22.987725
100.879471	3729.165839	22.992743
101.334502	3735.833962	22.997760
101.449476	3754.236361	23.002778
101.184114	3754.522100	23.007795
101.417195	3752.456888	23.012813
101.376178	3757.211213	23.017831
101.614951	3758.638055	23.022848
101.775428	3761.669418	23.027866
101.647180	3770.403695	23.032883
101.984121	3776.153465	23.037901
101.854187	3787.441926	23.042919
101.997038	3778.594253	23.047936
101.999087	3786.018598	23.052954
102.146668	3797.427675	23.057971
102.543981	3813.427949	23.062989
102.738626	3823.364085	23.068007
102.853585	3810.860261	23.073024
102.944380	3807.864137	23.078042
102.872903	3818.591290	23.083059
103.297963	3803.712964	23.088077
103.030348	3809.002532	23.093095
103.413710	3820.634040	23.098112
103.549270	3840.692815	23.103130
103.363739	3840.553467	23.108147
103.803540	3831.723535	23.113165
103.536679	3835.232026	23.118183
103.699638	3838.331113	23.123200
103.735129	3837.496808	23.128218
103.748576	3843.913639	23.133235
104.121457	3854.207740	23.138253
103.719362	3859.806641	23.143271
104.237443	3862.475619	23.148288
104.346013	3859.015846	23.153306
104.374592	3866.102323	23.158323
104.935709	3886.159601	23.163341
104.833517	3887.937049	23.168359
104.885626	3887.434684	23.173376
105.245673	3881.781774	23.178394
104.898349	3891.764773	23.183411
105.192570	3889.865429	23.188429
105.014158	3887.228477	23.193447
105.294673	3885.686573	23.198464
105.626607	3907.962064	23.203482
105.540430	3911.942304	23.208499
105.986199	3907.152879	23.213517
105.673989	3904.427825	23.218535
105.987639	3907.212563	23.223552
105.899466	3906.563321	23.228570
105.963543	3908.337260	23.233587
106.052214	3923.549258	23.238605
106.208305	3934.825904	23.243623
106.379440	3934.151051	23.248640
106.694187	3934.957366	23.253658
106.509685	3934.210671	23.258675
106.707555	3930.656950	23.263693
106.325060	3953.744996	23.268711
106.910865	3954.263088	23.273728
106.958661	3959.977325	23.278746
107.038847	3962.855067	23.283763
107.354919	3960.059838	23.288781
107.267106	3962.691341	23.293799
107.678348	3982.159293	23.298816
107.770503	3986.673888	23.303834
107.457960	3997.522586	23.308851
107.931050	3977.175079	23.313869
107.842669	3981.303755	23.318887
107.899237	3981.062106	23.323904
107.707016	3991.052955	23.328922
108.242429	4013.080305	23.333939
108.276473	4003.596878	23.338957
108.315820	4012.546097	23.343975
108.710800	4003.404544	23.348992
108.908335	4008.015888	23.354010
108.641259	4008.010531	23.359027
108.963442	4004.253506	23.364045
108.947989	4020.657033	23.369063
108.885240	4025.809193	23.374080
109.206441	4042.036511	23.379098
109.177680	4043.206055	23.384115
109.443811	4036.683071	23.389133
109.338445	4043.904029	23.394151
109.559057	4041.613644	23.399168
109.663261	4054.021188	23.404186
109.297266	4066.131735	23.409203
109.552098	4063.653763	23.414221
109.841910	4066.214094	23.419239
109.743210	4085.018460	23.424256
110.078812	4098.242978	23.429274
110.117060	4096.740381	23.434291
110.506823	4090.407173	23.439309
110.147309	4099.072821	23.444327
110.697135	4110.436394	23.449344
110.907430	4117.402725	23.454362
110.970789	4126.644931	23.459379
111.089959	4124.669016	23.464397
110.918210	4123.726467	23.469415
111.339146	4124.376606	23.474432
111.475362	4133.247639	23.479450
111.406042	4146.759752	23.484467
111.719305	4144.089386	23.489485
111.595372	4148.187765	23.494503
111.528136	4155.353634	23.499520
111.921961	4146.379147	23.504538
111.898377	4169.999517	23.509555
111.931996	4167.539255	23.514573
112.193134	4177.516585	23.519591
112.606697	4174.353938	23.524608
112.523311	4164.850481	23.529626
112.574200	4175.129594	23.534643
112.719957	4188.998321	23.539661
113.070794	4201.153300	23.544679
113.098013	4202.968027	23.549696
113.400215	4191.231061	23.554714
112.770110	4199.132772	23.559731
113.356394	4197.365380	23.564749
113.346858	4205.439979	23.569767
113.520661	4214.447379	23.574784
113.824865	4211.157926	23.579802
113.504933	4215.646315	23.584819
113.863602	4216.893480	23.589837
114.026538	4222.594260	23.594855
114.176030	4215.499078	23.599872
114.220694	4232.659142	23.604890
114.036006	4247.488298	23.609907
114.385242	4256.971483	23.614925
114.710367	4250.366977	23.619943
114.804998	4255.280520	23.624960
114.655243	4247.158312	23.629978
114.696468	4254.539378	23.634995
114.972411	4263.139276	23.640013
115.412819	4263.002601	23.645031
115.439817	4273.764555	23.650048
115.332720	4273.716170	23.655066
115.306661	4277.807040	23.660083
115.462130	4278.240467	23.665101
115.769866	4283.955884	23.670119
115.572336	4302.613854	23.675136
115.855501	4299.316054	23.680154
115.560106	4313.181544	23.685171
116.019876	4300.613545	23.690189
115.979394	4316.670285	23.695207
115.889012	4323.825100	23.700224
116.063499	4323.826958	23.705242
116.397606	4331.681704	23.710259
116.592242	4341.019643	23.715277
116.750151	4353.703621	23.720295
117.114337	4356.168207	23.725312
117.224979	4350.218966	23.730330
117.273308	4359.596104	23.735347
117.513214	4350.093347	23.740365
117.526816	4350.217136	23.745383
117.342473	4351.763707	23.750400
117.441089	4346.495317	23.755418
117.609065	4368.802943	23.760435
117.663614	4371.943318	23.765453
117.888826	4375.138917	23.770471
117.872248	4372.197872	23.775488
118.016775	4377.414270	23.780506
118.093782	4396.597074	23.785523
118.654746	4393.995122	23.790541
118.608691	4403.507620	23.795559
118.553572	4401.558166	23.800576
119.017456	4409.875802	23.805594
118.913930	4411.111306	23.810611
118.957695	4423.257448	23.815629
119.492404	4421.533223	23.820647
119.253873	4433.104743	23.825664
119.733275	4426.205280	23.830682
119.283469	4429.412637	23.835699
119.604598	4424.093991	23.840717
119.737846	4430.138406	23.845735
119.752021	4454.908278	23.850752
120.180125	4456.529863	23.855770
120.089715	4461.172479	23.860787
120.137699	4459.910011	23.865805
120.290205	4467.072715	23.870823
120.039888	4478.003582	23.875840
120.731861	4481.017963	23.880858
120.650276	4486.957000	23.885875
120.772556	4472.946044	23.890893
121.227042	4485.625127	23.895911
120.864544	4508.663422	23.900928
121.446454	4506.550988	23.905946
121.120590	4511.075882	23.910963
121.123018	4510.591174	23.915981
121.628295	4516.477944	23.920999
121.431552	4525.642168	23.926016
121.839231	4533.023331	23.931034
121.791809	4541.417033	23.936051
121.984721	4539.343014	23.941069
122.209149	4542.778191	23.946087
122.201235	4561.790184	23.951104
122.278959	4563.943112	23.956122
122.263785	4558.875416	23.961139
122.626399	4563.421789	23.966157
122.932038	4569.782662	23.971175
123.046871	4592.890105	23.976192
123.331016	4582.067036	23.981210
123.398499	4592.722486	23.986227
123.565396	4593.712404	23.991245
123.804927	4587.341657	23.996263
123.253989	4586.536680	24.001280
123.534594	4575.018795	24.006298
123.831905	4582.838807	24.011315
123.947994	4607.231346	24.016333
124.100801	4606.928075	24.021351
124.252597	4614.533569	24.026368
124.224598	4606.891898	24.031386
124.301096	4610.265740	24.036403
124.260212	4606.200902	24.041421
124.536195	4615.402678	24.046439
124.725630	4634.229298	24.051456
124.652764	4638.117735	24.056474
124.798961	4633.158755	24.061491
124.709036	4631.640314	24.066509
124.797698	4648.158779	24.071527
125.075871	4660.421441	24.076544
125.544335	4660.551826	24.081562
125.589079	4655.271777	24.086579
125.655720	4671.349732	24.091597
125.977228	4669.940365	24.096615
125.901485	4679.145285	24.101632
125.939470	4683.467437	24.106650
126.085657	4686.498984	24.111667
126.275370	4682.902343	24.116685
126.429881	4689.905731	24.121703
126.334747	4710.629529	24.126720
126.603302	4714.507921	24.131738
126.733819	4707.794474	24.136755
126.869122	4712.328912	24.141773
127.303193	4722.797745	24.146791
127.288941	4741.208522	24.151808
127.692704	4732.857380	24.156826
127.539140	4735.590466	24.161843
127.869470	4729.750406	24.166861
128.057484	4727.454295	24.171879
127.807536	4735.895022	24.176896
128.136174	4740.910945	24.181914
128.319530	4765.127992	24.186931
128.412543	4766.445178	24.191949
128.570062	4763.153910	24.196967
128.250074	4758.117717	24.201984
128.343317	4759.405725	24.207002
128.473885	4773.666539	24.212019
128.491304	4789.377886	24.217037
128.610705	4784.520166	24.222055
128.582072	4807.497317	24.227072
129.053541	4814.252178	24.232090
129.539728	4816.888017	24.237107
129.750092	4822.830034	24.242125
129.861893	4830.446192	24.247143
129.936359	4839.455435	24.252160
130.294479	4840.950039	24.257178
130.658408	4845.445874	24.262195
130.523421	4851.919195	24.267213
130.794153	4842.302354	24.272231
130.684469	4837.867666	24.277248
130.718334	4842.055870	24.282266
130.800349	4840.266370	24.287283
130.883804	4845.862404	24.292301
130.755312	4854.296472	24.297319
130.714653	4880.504734	24.302336
130.834151	4873.270099	24.307354
131.259220	4886.232388	24.312371
131.374505	4910.736578	24.317389
131.624869	4897.857036	24.322407
131.319062	4905.929070	24.327424
131.717246	4920.717481	24.332442
132.064374	4931.059087	24.337459
132.035079	4938.612814	24.342477
132.457940	4923.669614	24.347495
132.483412	4934.036914	24.352512
132.316060	4940.431360	24.357530
132.492442	4957.680666	24.362547
133.032037	4958.666393	24.367565
133.154117	4957.090766	24.372583
133.068703	4967.228363	24.377600
133.135525	4954.334272	24.382618
133.428580	4966.873510	24.387635
133.624714	4987.686483	24.392653
133.796652	4985.359131	24.397671
133.810986	4993.786953	24.402688
133.930354	4988.027407	24.407706
133.634036	4973.263878	24.412723
133.363858	4984.118050	24.417741
134.125946	5000.742756	24.422759
134.195474	5014.686266	24.427776
134.327753	5016.634118	24.432794
134.491025	5023.611002	24.437811
134.421199	5036.762466	24.442829
134.744581	5039.077192	24.447847
135.065437	5041.074157	24.452864
135.174079	5053.482545	24.457882
135.305351	5057.595610	24.462899
135.456398	5069.222803	24.467917
135.922579	5064.723421	24.472935
135.615034	5066.167596	24.477952
136.060453	5066.813727	24.482970
136.032309	5083.148794	24.487987
135.759663	5096.780445	24.493005
136.213328	5101.517458	24.498023
136.165062	5100.498485	24.503040
136.355954	5110.123393	24.508058
136.653159	5120.849065	24.513075
136.628063	5122.997829	24.518093
136.581789	5126.615782	24.523111
137.032559	5138.454877	24.528128
137.284180	5139.949030	24.533146
137.328182	5144.089956	24.538163
137.171619	5152.787945	24.543181
137.357398	5158.041090	24.548199
137.711273	5166.470279	24.553216
137.762212	5173.017696	24.558234
137.932712	5178.457672	24.563251
137.655394	5207.296012	24.568269
138.432762	5199.523860	24.573287
138.340213	5203.085698	24.578304
138.772072	5213.603269	24.583322
139.438072	5225.470589	24.588339
139.085341	5233.174093	24.593357
139.374901	5218.173140	24.598375
139.796790	5221.155994	24.603392
139.428702	5225.813305	24.608410
139.896887	5218.932685	24.613427
139.475887	5223.224655	24.618445
140.013355	5217.739187	24.623463
139.945688	5231.122793	24.628480
139.556859	5243.923216	24.633498
140.183316	5245.538037	24.638515
140.005808	5251.521597	24.643533
140.265129	5271.655825	24.648551
140.647363	5291.825647	24.653568
140.419032	5277.691670	24.658586
140.203777	5280.744584	24.663603
140.902326	5301.511805	24.668621
140.897605	5304.843326	24.673639
141.172930	5306.154000	24.678656
141.457556	5322.397363	24.683674
141.782806	5330.035917	24.688691
141.695789	5339.566000	24.693709
142.138469	5336.095086	24.698727
142.099057	5333.938142	24.703744
142.014151	5334.209776	24.708762
142.267847	5348.360152	24.713779
142.580486	5357.885508	24.718797
142.586626	5356.401496	24.723815
142.967151	5361.627979	24.728832
142.937940	5361.238269	24.733850
143.185525	5359.770987	24.738867
142.923011	5359.946802	24.743885
143.247110	5367.101197	24.748903
143.368454	5384.352995	24.753920
143.357671	5386.184389	24.758938
143.666341	5388.807977	24.763955
143.817448	5392.702047	24.768973
143.989252	5393.145404	24.773991
143.897332	5418.554979	24.779008
143.620784	5430.902999	24.784026
143.968341	5422.292233	24.789043
144.313993	5434.431702	24.794061
144.582916	5451.192097	24.799079
144.613253	5448.290339	24.804096
144.466412	5457.399584	24.809114
144.783602	5468.329322	24.814131
144.788158	5485.831332	24.819149
145.077498	5490.157770	24.824167
145.298749	5499.091893	24.829184
145.584774	5518.330456	24.834202
145.677754	5526.410812	24.839219
145.629266	5532.740924	24.844237
146.158597	5540.730927	24.849255
145.955673	5549.808555	24.854272
146.349905	5560.114425	24.859290
146.607496	5557.049793	24.864307
146.726011	5564.877059	24.869325
146.847689	5555.951562	24.874343
147.210557	5568.808151	24.879360
147.042042	5583.958798	24.884378
147.311033	5588.024786	24.889395
147.116099	5596.954625	24.894413
147.646465	5592.379885	24.899431
148.087793	5609.321405	24.904448
147.817604	5628.449780	24.909466
148.176497	5619.102985	24.914483
148.152036	5620.286899	24.919501
148.280294	5623.720123	24.924519
148.577790	5637.866659	24.929536
148.628665	5647.388273	24.934554
148.805637	5638.892270	24.939571
148.689704	5652.040853	24.944589
149.100792	5668.553474	24.949607
149.010132	5667.968365	24.954624
149.006291	5669.646634	24.959642
149.663952	5674.754879	24.964659
149.562870	5698.254114	24.969677
149.818116	5691.413273	24.974695
150.021383	5702.725910	24.979712
149.908886	5711.145972	24.984730
150.519376	5723.456833	24.989747
150.766441	5721.358732	24.994765
150.818570	5736.636817	24.999783
151.085138	5722.693014	25.004800
150.868492	5729.107754	25.009818
151.195872	5723.979030	25.014835
151.222050	5751.941913	25.019853
151.526762	5757.874177	25.024871
151.864823	5754.426796	25.029888
151.305741	5763.426470	25.034906
151.521968	5760.050454	25.039923
151.531880	5777.252610	25.044941
151.988404	5778.842068	25.049959
152.038084	5789.697391	25.054976
152.096878	5804.286854	25.059994
152.397611	5801.577334	25.065011
152.331972	5816.507180	25.070029
152.495675	5819.669154	25.075047
152.782630	5828.427975	25.080064
152.848764	5841.146464	25.085082
153.095550	5847.611328	25.090099
153.060660	5857.098437	25.095117
153.018203	5869.917627	25.100135
153.554324	5882.967108	25.105152
153.712675	5889.615181	25.110170
154.016247	5895.368110	25.115187
154.033698	5903.063417	25.120205
153.841424	5909.386769	25.125223
154.305722	5926.957284	25.130240
154.275853	5936.173456	25.135258
154.489243	5933.272807	25.140275
154.686241	5960.792703	25.145293
154.935940	5970.023254	25.150311
155.277571	5972.182302	25.155328
155.150903	5988.351102	25.160346
155.531855	5987.870626	25.165363
155.596747	5994.020688	25.170381
155.720667	6001.803169	25.175399
156.139659	6015.299043	25.180416
156.212249	6022.385112	25.185434
156.478182	6012.765208	25.190451
156.587968	6016.923826	25.195469
156.516332	6033.920803	25.200487
156.990177	6040.865622	25.205504
157.014517	6046.575048	25.210522
157.177539	6040.249468	25.215539
157.293011	6057.006771	25.220557
157.566831	6060.797201	25.225575
158.385695	6063.978348	25.230592
158.340726	6066.408562	25.235610
158.382683	6060.737843	25.240627
158.202691	6057.855045	25.245645
158.492505	6059.266565	25.250663
158.649130	6054.820522	25.255680
158.695962	6066.485396	25.260698
159.140593	6084.049892	25.265715
159.021280	6090.984247	25.270733
158.856035	6089.521454	25.275751
159.100773	6087.300033	25.280768
159.314336	6108.868509	25.285786
159.476555	6120.827795	25.290803
159.709564	6119.472340	25.295821
159.598704	6122.531759	25.300839
159.965891	6140.848722	25.305856
159.739555	6151.242759	25.310874
160.063163	6150.100714	25.315891
160.294508	6178.859756	25.320909
160.444000	6189.849266	25.325927
160.716959	6184.108752	25.330944
160.736277	6204.924251	25.335962
160.927920	6207.394075	25.340979
161.120707	6211.480719	25.345997
161.103457	6232.359018	25.351015
161.312309	6234.114764	25.356032
161.575279	6241.277317	25.361050
162.018998	6263.903497	25.366067
162.134513	6268.319577	25.371085
162.171222	6277.460339	25.376103
162.493055	6274.388873	25.381120
162.856150	6292.536561	25.386138
162.932252	6297.974437	25.391155
162.468769	6297.325796	25.396173
162.799459	6309.385716	25.401191
163.415390	6316.715918	25.406208
163.341247	6335.275517	25.411226
163.336346	6329.946418	25.416243
163.728437	6333.510185	25.421261
163.908492	6339.507416	25.426279
164.348763	6348.387645	25.431296
164.601342	6353.278056	25.436314
164.360602	6358.531332	25.441331
164.685117	6362.728529	25.446349
164.655735	6353.499935	25.451367
164.541672	6351.996350	25.456384
164.810680	6361.981643	25.461402
165.157745	6382.573771	25.466419
165.531018	6377.971260	25.471437
165.406804	6378.768474	25.476455
165.278677	6389.481153	25.481472
165.793718	6411.881499	25.486490
165.446666	6406.271124	25.491507
166.049354	6428.258435	25.496525
165.920621	6444.354790	25.501543
166.164378	6439.169582	25.506560
166.580104	6459.090397	25.511578
166.489393	6456.017098	25.516595
166.831789	6469.971850	25.521613
166.791103	6500.838570	25.526631
166.974756	6494.369981	25.531648
167.209439	6513.782876	25.536666
167.365409	6528.045796	25.541683
167.802528	6528.157771	25.546701
167.697753	6535.705853	25.551719
168.099746	6559.852437	25.556736
167.950195	6566.337532	25.561754
168.463491	6572.732578	25.566771
168.983263	6590.532520	25.571789
168.806523	6594.667840	25.576807
168.766025	6585.214109	25.581824
169.148102	6609.714571	25.586842
168.909282	6624.010646	25.591859
169.741082	6616.609239	25.596877
169.680539	6630.190547	25.601895
170.041482	6626.261875	25.606912
170.107476	6639.205509	25.611930
170.205938	6637.087784	25.616947
170.683775	6647.613671	25.621965
170.624399	6667.560635	25.626983
170.803205	6667.167170	25.632000
170.995052	6677.958607	25.637018
171.189683	6679.267795	25.642035
171.654369	6679.577635	25.647053
171.650836	6698.333909	25.652071
171.541123	6699.164970	25.657088
171.760574	6700.831585	25.662106
171.666746	6701.678132	25.667123
172.091971	6724.295431	25.672141
172.261768	6740.745153	25.677159
172.313038	6731.655005	25.682176
172.423094	6744.512664	25.687194
172.540413	6754.819480	25.692212
173.168739	6757.302948	25.697229
173.092036	6766.654957	25.702247
173.433543	6785.327428	25.707264
173.608371	6787.296813	25.712282
173.672578	6785.244603	25.717300
174.054300	6793.072223	25.722317
173.974273	6818.147316	25.727335
174.157103	6817.724038	25.732352
174.229675	6823.413944	25.737370
174.299933	6816.341745	25.742388
174.453407	6831.845920	25.747405
174.557645	6842.194341	25.752423
174.768918	6832.332516	25.757440
174.904246	6862.091699	25.762458
174.824470	6873.067655	25.767476
175.360242	6879.257464	25.772493
174.942469	6896.867187	25.777511
175.375961	6897.880069	25.782528
175.899835	6918.431807	25.787546
176.215295	6931.117769	25.792564
176.178045	6931.575305	25.797581
176.140907	6942.708084	25.802599
176.863229	6953.849827	25.807616
176.810661	6966.509317	25.812634
176.748781	6964.884396	25.817652
177.295737	6974.077349	25.822669
177.347110	6996.735665	25.827687
177.669963	6993.600094	25.832704
177.773050	7007.771380	25.837722
177.505935	7024.883698	25.842740
177.898838	7017.060903	25.847757
178.202165	7039.363285	25.852775
178.488232	7053.045892	25.857792
178.251865	7058.341994	25.862810
178.581785	7073.851851	25.867828
178.967862	7081.957730	25.872845
178.895470	7094.504028	25.877863
179.035184	7112.519502	25.882880
179.152147	7120.981089	25.887898
179.570311	7135.504402	25.892916
180.200077	7147.969151	25.897933
179.506550	7158.426226	25.902951
180.013997	7168.634850	25.907968
180.597521	7177.470564	25.912986
180.607323	7190.379052	25.918004
180.681752	7197.886751	25.923021
180.876229	7210.295224	25.928039
181.232250	7216.732326	25.933056
181.582714	7234.940687	25.938074
181.970944	7227.513193	25.943092
182.203498	7230.244218	25.948109
182.189409	7242.344603	25.953127
182.268483	7244.410243	25.958144
182.765162	7252.601873	25.963162
182.591105	7261.742650	25.968180
182.760692	7261.459400	25.973197
182.814880	7262.628839	25.978215
183.089669	7274.268676	25.983232
183.160797	7284.387350	25.988250
183.041693	7298.795752	25.993268
183.454751	7304.481448	25.998285
183.861303	7320.186020	26.003303
183.948339	7328.054817	26.008320
184.237255	7336.637711	26.013338
184.501182	7347.351504	26.018356
184.728844	7338.518525	26.023373
184.814189	7356.128953	26.028391
184.780523	7369.496917	26.033408
185.199665	7388.302968	26.038426
185.307820	7385.072897	26.043444
185.918976	7384.132073	26.048461
185.987334	7401.639813	26.053479
185.976294	7403.057945	26.058496
186.339545	7405.417628	26.063514
186.068514	7409.301741	26.068532
186.257835	7408.474077	26.073549
186.053520	7430.115897	26.078567
186.698604	7432.809380	26.083584
186.901297	7448.890476	26.088602
186.643707	7467.024117	26.093620
186.878272	7470.387369	26.098637
186.654510	7486.716338	26.103655
186.934001	7489.647589	26.108672
187.585722	7503.665471	26.113690
187.692582	7527.124319	26.118708
187.568221	7530.352446	26.123725
187.928201	7560.165540	26.128743
188.096962	7559.546074	26.133760
188.323845	7572.478798	26.138778
188.420360	7590.874548	26.143796
189.076693	7598.393225	26.148813
188.971091	7625.838500	26.153831
189.225674	7621.688522	26.158848
190.114921	7631.887014	26.163866
189.948153	7653.581998	26.168884
190.504602	7652.286299	26.173901
190.374536	7643.257160	26.178919
190.310732	7664.480608	26.183936
190.713016	7670.246203	26.188954
190.497738	7687.273453	26.193972
191.158021	7683.554911	26.198989
191.193184	7708.608395	26.204007
191.242560	7711.809371	26.209024
191.458505	7722.338373	26.214042
191.679158	7733.391217	26.219060
191.979372	7726.152147	26.224077
192.059218	7747.474806	26.229095
192.107700	7758.890159	26.234112
192.645359	7764.219829	26.239130
192.804182	7796.852007	26.244148
193.115616	7788.888722	26.249165
193.039509	7799.559077	26.254183
193.054090	7809.536206	26.259200
193.857482	7820.472940	26.264218
193.706671	7829.470768	26.269236
193.783311	7839.541619	26.274253
194.161059	7860.321213	26.279271
194.246205	7860.693919	26.284288
194.630110	7874.859660	26.289306
194.447697	7882.124264	26.294324
194.730395	7888.511550	26.299341
194.785916	7899.313784	26.304359
195.092934	7908.097222	26.309376
195.563570	7914.010708	26.314394
195.143503	7943.794543	26.319412
195.718089	7949.184331	26.324429
196.036627	7957.904447	26.329447
196.325201	7973.579572	26.334464
196.376335	7981.616907	26.339482
196.503298	7993.611012	26.344500
197.181069	7994.698536	26.349517
197.507578	8006.979430	26.354535
197.268441	8024.728603	26.359552
197.703811	8028.409267	26.364570
197.801191	8043.749036	26.369588
197.944606	8037.996223	26.374605
198.045679	8053.643390	26.379623
198.052394	8061.660548	26.384640
198.475690	8072.471332	26.389658
198.565973	8096.811288	26.394676
199.040248	8095.789898	26.399693
198.960869	8104.872944	26.404711
198.970735	8123.590079	26.409728
199.165924	8123.946149	26.414746
199.407017	8141.375690	26.419764
199.990645	8147.126404	26.424781
199.916533	8158.916816	26.429799
199.634552	8163.564656	26.434816
200.310230	8176.777262	26.439834
200.175720	8181.010766	26.444852
200.586636	8198.461094	26.449869
200.826035	8213.515988	26.454887
201.006099	8216.849824	26.459904
201.438883	8226.218382	26.464922
201.479237	8245.166931	26.469940
201.768916	8244.344668	26.474957
202.232023	8263.609240	26.479975
202.189061	8272.553225	26.484992
202.323061	8272.455454	26.490010
202.415124	8285.327578	26.495028
202.899454	8288.392854	26.500045
202.971862	8309.029014	26.505063
202.748289	8313.234761	26.510080
203.321171	8320.769176	26.515098
203.108164	8343.265213	26.520116
203.680608	8358.324187	26.525133
203.927998	8371.647247	26.530151
203.912071	8379.512341	26.535168
204.400222	8391.951103	26.540186
204.495971	8404.184644	26.545204
204.690770	8416.946912	26.550221
204.754054	8422.212760	26.555239
205.379778	8440.152426	26.560256
205.547202	8452.274882	26.565274
205.375019	8460.774022	26.570292
205.846290	8479.968182	26.575309
205.842930	8484.745654	26.580327
206.194606	8500.241486	26.585344
206.372644	8507.771250	26.590362
206.391733	8523.524616	26.595380
206.839287	8527.925744	26.600397
207.336509	8543.544043	26.605415
207.247680	8557.527123	26.610432
207.594851	8566.612287	26.615450
208.062156	8581.137455	26.620468
208.294084	8578.012694	26.625485
208.132923	8597.567716	26.630503
208.223864	8615.016330	26.635520
208.459135	8611.613721	26.640538
209.107857	8641.155739	26.645556
209.074183	8640.810012	26.650573
209.005811	8648.045053	26.655591
209.284215	8666.082650	26.660608
209.578987	8666.339533	26.665626
209.647530	8675.607168	26.670644
209.761592	8699.346988	26.675661
210.167981	8704.389123	26.680679
210.414940	8731.624315	26.685696
210.986518	8734.632698	26.690714
210.782034	8737.181105	26.695732
211.134883	8760.011799	26.700749
211.525111	8765.774277	26.705767
211.738515	8778.120181	26.710784
212.121795	8786.115537	26.715802
211.543326	8793.711595	26.720820
212.109580	8813.089736	26.725837
212.525553	8831.381248	26.730855
212.431876	8829.411633	26.735872
212.551076	8832.925832	26.740890
212.774254	8844.663594	26.745908
213.130314	8848.754613	26.750925
213.607301	8876.714525	26.755943
213.349401	8890.469862	26.760960
213.507983	8892.389421	26.765978
214.060072	8907.234076	26.770996
213.859493	8906.731637	26.776013
214.280649	8928.026150	26.781031
214.164451	8946.457888	26.786048
214.638726	8947.259343	26.791066
215.038575	8967.974489	26.796084
215.039734	8975.476249	26.801101
215.191732	8992.959283	26.806119
215.196705	8994.203958	26.811136
215.701443	9021.449749	26.816154
215.684556	9021.991415	26.821172
215.844043	9047.592822	26.826189
216.242613	9066.101759	26.831207
216.482853	9089.649533	26.836224
216.697714	9093.576502	26.841242
216.923106	9109.307319	26.846260
217.061514	9135.099058	26.851277
217.387256	9146.368666	26.856295
217.501862	9172.803293	26.861312
217.844794	9176.857182	26.866330
218.027808	9199.522827	26.871348
218.414879	9211.848981	26.876365
218.990284	9209.421142	26.881383
218.990334	9220.359496	26.886400
219.658866	9237.659600	26.891418
219.704475	9253.282460	26.896436
219.607747	9259.121006	26.901453
220.309651	9258.729118	26.906471
220.266307	9288.667356	26.911488
220.296879	9285.909026	26.916506
220.543609	9295.804533	26.921524
220.624612	9315.079276	26.926541
220.960344	9319.521196	26.931559
220.956291	9334.283429	26.936576
221.216577	9341.191800	26.941594
221.078645	9361.751484	26.946612
221.416120	9381.424220	26.951629
221.937651	9393.148443	26.956647
221.742457	9406.490491	26.961664
222.317278	9439.109145	26.966682
222.825357	9437.075286	26.971700
222.851012	9462.029888	26.976717
223.332931	9467.722297	26.981735
223.621695	9479.674188	26.986752
223.798763	9495.563065	26.991770
223.841460	9503.952341	26.996788
223.990293	9519.700962	27.001805
224.715893	9528.430180	27.006823
224.214128	9533.185697	27.011840
224.701661	9550.961210	27.016858
225.153853	9570.430055	27.021876
225.381479	9575.136525	27.026893
225.708263	9589.800895	27.031911
225.619964	9606.157648	27.036928
225.961172	9615.242823	27.041946
226.255612	9628.972737	27.046964
226.084483	9637.756719	27.051981
226.866333	9638.341068	27.056999
226.766159	9660.403522	27.062016
226.856264	9665.573954	27.067034
227.105281	9696.750245	27.072052
226.958190	9705.333333	27.077069
227.717598	9715.193859	27.082087
227.697585	9732.916519	27.087104
228.057494	9763.934353	27.092122
228.763138	9768.143420	27.097140
228.493747	9777.255716	27.102157
229.038967	9789.341851	27.107175
228.785946	9799.659160	27.112192
229.518386	9804.438901	27.117210
229.912214	9820.928766	27.122228
229.874099	9826.507291	27.127245
230.310755	9823.903018	27.132263
230.207496	9829.415911	27.137280
230.549500	9841.457734	27.142298
230.499033	9839.104268	27.147316
230.659982	9856.768745	27.152333
231.093221	9864.450703	27.157351
230.990607	9883.346074	27.162368
231.175167	9901.618823	27.167386
231.499845	9911.512836	27.172404
231.950940	9929.161661	27.177421
232.192618	9939.876943	27.182439
232.600679	9960.981984	27.187456
232.308172	9971.121590	27.192474
232.714185	9980.489312	27.197492
232.807183	10012.716208	27.202509
233.095219	10030.901857	27.207527
233.252642	10044.020615	27.212544
233.571168	10060.690211	27.217562
233.627341	10080.738108	27.222580
233.931681	10093.370920	27.227597
234.096281	10113.010936	27.232615
234.152792	10136.534726	27.237632
234.636458	10154.949688	27.242650
234.742957	10171.030540	27.247668
235.076243	10193.902757	27.252685
235.703983	10210.720640	27.257703
235.941102	10230.266070	27.262720
236.476634	10231.857892	27.267738
236.574674	10251.023003	27.272756
236.412289	10261.702185	27.277773
236.859358	10274.782635	27.282791
237.335015	10298.641433	27.287808
237.540385	10300.554206	27.292826
238.031916	10310.896696	27.297844
238.223326	10326.463372	27.302861
238.592922	10333.106696	27.307879
238.858449	10349.350480	27.312896
238.718529	10353.435760	27.317914
239.078894	10356.993093	27.322932
238.980631	10375.831597	27.327949
239.403020	10386.900938	27.332967
239.232471	10415.053453	27.337984
239.575005	10426.481115	27.343002
239.814645	10444.610641	27.348020
239.672787	10468.066911	27.353037
240.271572	10486.494710	27.358055
240.507458	10493.878748	27.363072
240.738683	10510.717680	27.368090
241.057260	10527.810036	27.373108
241.212079	10551.908254	27.378125
241.798209	10566.701546	27.383143
241.806698	10585.280752	27.388160
241.887349	10597.447558	27.393178
242.631224	10613.075108	27.398196
242.476194	10635.422147	27.403213
243.045705	10650.667342	27.408231
243.281549	10653.013946	27.413248
243.652866	10678.450524	27.418266
243.723191	10676.904182	27.423284
244.168249	10702.475131	27.428301
244.642392	10706.959920	27.433319
244.510894	10717.904523	27.438336
244.582614	10732.754763	27.443354
244.908595	10739.438565	27.448372
245.261103	10747.102799	27.453389
245.228447	10762.436755	27.458407
245.657077	10774.448394	27.463424
245.655230	10788.422162	27.468442
245.984085	10800.967172	27.473460
246.048876	10821.848905	27.478477
246.214473	10825.475616	27.483495
246.580801	10848.269234	27.488512
246.608077	10857.372418	27.493530
246.868940	10872.884792	27.498548
246.993940	10890.787986	27.503565
247.544845	10912.227531	27.508583
248.099592	10931.358027	27.513600
248.095234	10940.838366	27.518618
248.490697	10946.303745	27.523636
248.255249	10979.261355	27.528653
249.125886	10985.270500	27.533671
249.586379	11009.501584	27.538688
249.593941	11019.273083	27.543706
250.303782	11022.529262	27.548724
250.603738	11040.257116	27.553741
250.647695	11044.195524	27.558759
250.822945	11048.203592	27.563776
250.724514	11064.892830	27.568794
251.327754	11081.101931	27.573812
250.875888	11091.518372	27.578829
251.319864	11096.099658	27.583847
251.885143	11118.443151	27.588864
252.008318	11142.946153	27.593882
252.383409	11146.259349	27.598900
252.638922	11178.349791	27.603917
252.770655	11177.759173	27.608935
253.075976	11192.950921	27.613952
253.454769	11211.404941	27.618970
253.858915	11223.840120	27.623988
253.907677	11246.193660	27.629005
254.232974	11256.815614	27.634023
254.419955	11263.640828	27.639040
254.327999	11282.806313	27.644058
254.753636	11288.695422	27.649076
255.130170	11320.471444	27.654093
255.449325	11332.742716	27.659111
255.751389	11351.441235	27.664128
255.892902	11374.977183	27.669146
255.992393	11370.578529	27.674164
256.397463	11397.104238	27.679181
256.635182	11405.736405	27.684199
256.969944	11423.249339	27.689216
257.075426	11443.608284	27.694234
257.388069	11462.880340	27.699252
257.283932	11475.762285	27.704269
257.988432	11498.173078	27.709287
258.309828	11510.407871	27.714304
258.519733	11531.182981	27.719322
258.670219	11528.838547	27.724340
258.913709	11553.946266	27.729357
259.206923	11568.029441	27.734375
259.485633	11582.545220	27.739392
259.534570	11593.304541	27.744410
259.690541	11617.122089	27.749428
260.007613	11639.107141	27.754445
260.177894	11654.329557	27.759463
260.668933	11676.853149	27.764480
261.111172	11698.310153	27.769498
261.381085	11720.254272	27.774516
261.423267	11728.482482	27.779533
261.882865	11762.740123	27.784551
262.608838	11760.946473	27.789568
262.391488	11766.614429	27.794586
262.755307	11778.264081	27.799604
262.720639	11791.057562	27.804621
263.145029	11803.656874	27.809639
263.401504	11818.516922	27.814656
263.579400	11823.166102	27.819674
263.910091	11845.114511	27.824692
264.472247	11862.681677	27.829709
264.299544	11862.622056	27.834727
264.640303	11877.777066	27.839744
264.524233	11892.293866	27.844762
265.048506	11896.561109	27.849780
265.469932	11921.802253	27.854797
265.555037	11936.336217	27.859815
265.573664	11957.912541	27.864832
265.829583	11984.473358	27.869850
266.303175	12001.220146	27.874868
266.567403	12026.205400	27.879885
266.655836	12045.274163	27.884903
267.108467	12054.681080	27.889920
267.488822	12077.521386	27.894938
267.693984	12091.775602	27.899956
268.280460	12119.276276	27.904973
268.387174	12133.312024	27.909991
268.492969	12141.876600	27.915008
268.919686	12169.807223	27.920026
269.406412	12174.646486	27.925044
269.512235	12204.237654	27.930061
269.707021	12212.672498	27.935079
270.161346	12226.387617	27.940096
270.427407	12245.732926	27.945114
270.368262	12260.658234	27.950132
270.796142	12278.375724	27.955149
271.040644	12299.265856	27.960167
271.216249	12317.293047	27.965184
271.351444	12344.518966	27.970202
271.491617	12366.435009	27.975220
271.976770	12379.097202	27.980237
272.098945	12401.790023	27.985255
272.693393	12423.621488	27.990272
272.987802	12440.401544	27.995290
273.198606	12454.258023	28.000308
273.576063	12476.404410	28.005325
274.135550	12491.522212	28.010343
274.422732	12503.933616	28.015360
274.649545	12524.979827	28.020378
275.184012	12527.735857	28.025396
275.570261	12544.867999	28.030413
275.537127	12561.079926	28.035431
276.280483	12559.691472	28.040448
276.161900	12586.464978	28.045466
276.357999	12585.420831	28.050484
276.733751	12606.809676	28.055501
276.758268	12614.357323	28.060519
277.160750	12620.783407	28.065536
277.413299	12652.001060	28.070554
277.284918	12660.261129	28.075572
277.605723	12673.291152	28.080589
278.024304	12691.559046	28.085607
278.202309	12710.432533	28.090624
278.335457	12729.595554	28.095642
278.953895	12748.630988	28.100660
278.870728	12769.464077	28.105677
279.018770	12791.598440	28.110695
279.470543	12803.316219	28.115712
279.598109	12828.065305	28.120730
280.096835	12848.608333	28.125748
280.450383	12857.365510	28.130765
280.735102	12881.667893	28.135783
281.057583	12891.530221	28.140800
281.447641	12906.263567	28.145818
281.460820	12917.584407	28.150836
281.478546	12938.295423	28.155853
281.970906	12957.159709	28.160871
282.369406	12971.874382	28.165888
282.228111	12986.607506	28.170906
282.277624	13009.913632	28.175924
282.781671	13032.941254	28.180941
283.168023	13061.915481	28.185959
283.634236	13071.404268	28.190976
283.777616	13106.675260	28.195994
283.986090	13121.850180	28.201012
284.362882	13134.986349	28.206029
284.706639	13167.531019	28.211047
285.020251	13182.543605	28.216064
285.141676	13206.709606	28.221082
285.713253	13226.873858	28.226100
286.256087	13247.016102	28.231117
286.178053	13277.783796	28.236135
286.914997	13284.747340	28.241152
286.924758	13306.196112	28.246170
286.855505	13322.703175	28.251188
287.384399	13338.911092	28.256205
287.353088	13365.767563	28.261223
287.827913	13381.218555	28.266240
287.951666	13416.386299	28.271258
288.474234	13440.590257	28.276276
288.893913	13452.290179	28.281293
289.113295	13487.182210	28.286311
289.353377	13495.178406	28.291328
289.922131	13526.028620	28.296346
290.323984	13544.152100	28.301364
290.343696	13554.834028	28.306381
290.697314	13579.003119	28.311399
291.290227	13591.769775	28.316416
291.169982	13615.461037	28.321434
291.504405	13634.396381	28.326452
292.141758	13643.206291	28.331469
292.261596	13670.583534	28.336487
292.365387	13687.476806	28.341504
292.596743	13713.650513	28.346522
293.176123	13728.577057	28.351540
293.665528	13745.110269	28.356557
293.589089	13762.763141	28.361575
294.173667	13776.522627	28.366592
294.319263	13808.612817	28.371610
294.395491	13821.138947	28.376628
294.726947	13839.633738	28.381645
295.019561	13864.303490	28.386663
295.732298	13876.877174	28.391680
295.831695	13906.658464	28.396698
295.889628	13924.078080	28.401716
296.437968	13944.710418	28.406733
296.290360	13957.338322	28.411751
297.077480	13973.587658	28.416768
296.930319	13994.636206	28.421786
297.039664	14012.376795	28.426804
297.719814	14048.638969	28.431821
298.077670	14067.210026	28.436839
298.688480	14080.517834	28.441856
298.584183	14107.813132	28.446874
298.557424	14123.938870	28.451892
299.110385	14149.235772	28.456909
299.329739	14170.463434	28.461927
300.089164	14185.437821	28.466944
300.440329	14209.524722	28.471962
300.576342	14219.588935	28.476980
300.973171	14230.200999	28.481997
300.986546	14253.680364	28.487015
301.627545	14276.655554	28.492032
301.724705	14281.895639	28.497050
301.905513	14302.469488	28.502068
302.270146	14308.710231	28.507085
302.534126	14339.751125	28.512103
302.950811	14339.442626	28.517120
302.884588	14362.683153	28.522138
303.093530	14392.511812	28.527156
303.618113	14403.359740	28.532173
303.956057	14440.946586	28.537191
304.191382	14454.428755	28.542208
304.713046	14473.696574	28.547226
304.662259	14487.437325	28.552244
305.322002	14505.979398	28.557261
305.030894	14536.157447	28.562279
305.864069	14555.324940	28.567296
305.836144	14574.972274	28.572314
306.205630	14611.707935	28.577332
306.640977	14625.280070	28.582349
306.859023	14654.732591	28.587367
307.326161	14679.206040	28.592384
307.597509	14698.138873	28.597402
307.666447	14727.788000	28.602420
308.501019	14740.548655	28.607437
308.289377	14771.479964	28.612455
308.651958	14783.566982	28.617472
309.141657	14818.722869	28.622490
309.381640	14841.601319	28.627508
309.739958	14862.386054	28.632525
309.783814	14890.449334	28.637543
310.532130	14914.028644	28.642560
311.337128	14930.751964	28.647578
311.153204	14961.508821	28.652596
311.774550	14978.722816	28.657613
311.706751	14991.097156	28.662631
312.352655	15007.344106	28.667648
312.357335	15026.917233	28.672666
312.598504	15044.974409	28.677684
313.045134	15063.189883	28.682701
313.410813	15094.384016	28.687719
313.710137	15104.470600	28.692736
314.344967	15129.367739	28.697754
314.330413	15151.423456	28.702772
314.668378	15166.982330	28.707789
314.828431	15199.548840	28.712807
315.256575	15214.013176	28.717824
315.670497	15244.280718	28.722842
315.946147	15261.826483	28.727860
316.231471	15283.233803	28.732877
316.331599	15307.937589	28.737895
316.723594	15322.738996	28.742912
317.174230	15353.421495	28.747930
317.176456	15386.132710	28.752948
317.544411	15397.610895	28.757965
317.908579	15430.153532	28.762983
318.378036	15448.767577	28.768000
318.599626	15482.933725	28.773018
318.780289	15504.235715	28.778036
319.143005	15524.773103	28.783053
319.123285	15560.404214	28.788071
319.731784	15587.232490	28.793088
320.051404	15605.858906	28.798106
320.387785	15635.490617	28.803124
320.575573	15654.622797	28.808141
321.109300	15678.843983	28.813159
321.469531	15691.501064	28.818176
321.741128	15715.362189	28.823194
321.801419	15745.831046	28.828212
322.779057	15748.525318	28.833229
323.021122	15775.945735	28.838247
323.377366	15786.028045	28.843264
323.794809	15799.178545	28.848282
323.990457	15827.481520	28.853300
324.276868	15844.390916	28.858317
324.399043	15858.848147	28.863335
324.834461	15882.925134	28.868352
325.151616	15897.797767	28.873370
325.167484	15930.756845	28.878388
325.697470	15956.678214	28.883405
325.640311	15976.391953	28.888423
325.959197	15998.064180	28.893440
326.208044	16031.821866	28.898458
326.569909	16063.094125	28.903476
326.975843	16089.704556	28.908493
327.228040	16120.303113	28.913511
327.412770	16137.853827	28.918528
328.216558	16171.226763	28.923546
328.107745	16201.190107	28.928564
328.649486	16231.827638	28.933581
328.990228	16258.871564	28.938599
329.291730	16288.373089	28.943616
329.829181	16312.903536	28.948634
330.356088	16342.875400	28.953652
330.778458	16357.688474	28.958669
330.531203	16386.339985	28.963687
331.208413	16419.931408	28.968704
331.530905	16432.325765	28.973722
331.743570	16475.573115	28.978740
332.203158	16501.218537	28.983757
332.211620	16530.712254	28.988775
332.730304	16553.037815	28.993792
333.295208	16582.611334	28.998810
333.788736	16613.998402	29.003828
334.044653	16621.734996	29.008845
334.471312	16660.401429	29.013863
334.940584	16666.595807	29.018880
335.462608	16676.848259	29.023898
336.042282	16710.562029	29.028916
336.244788	16726.422226	29.033933
336.624363	16730.418369	29.038951
336.814559	16755.831351	29.043968
337.200256	16770.351372	29.048986
337.292545	16788.274320	29.054004
337.698140	16798.675376	29.059021
337.795919	16824.406408	29.064039
338.143012	16849.840854	29.069056
338.502240	16872.218461	29.074074
338.645572	16895.512986	29.079092
339.081352	16928.041994	29.084109
339.338207	16955.126166	29.089127
339.683344	16985.286913	29.094144
339.978154	17003.244353	29.099162
340.519977	17037.650751	29.104180
340.415206	17061.159970	29.109197
340.908110	17079.634838	29.114215
341.202371	17114.555269	29.119232
341.807340	17139.195569	29.124250
342.034912	17165.468395	29.129268
342.536644	17180.634781	29.134285
342.927571	17205.774049	29.139303
343.047037	17233.620716	29.144320
343.463841	17261.547473	29.149338
344.007898	17282.209938	29.154356
344.304672	17301.674356	29.159373
344.324428	17314.218794	29.164391
344.646862	17337.599368	29.169408
345.163554	17365.397847	29.174426
345.085494	17389.469017	29.179444
345.438618	17412.177821	29.184461
345.706173	17450.530365	29.189479
345.996312	17474.942685	29.194496
346.633463	17503.542739	29.199514
346.702879	17531.541637	29.204532
347.015813	17562.137534	29.209549
347.542882	17596.101423	29.214567
347.483118	17623.265889	29.219584
348.475026	17648.162905	29.224602
348.730538	17690.239813	29.229620
349.051025	17714.667955	29.234637
349.520673	17745.586630	29.239655
349.825570	17775.113886	29.244672
350.421453	17783.710634	29.249690
350.656361	17823.319516	29.254708
350.874315	17841.988926	29.259725
351.641296	17872.548075	29.264743
351.596549	17891.328807	29.269760
352.331623	17913.710243	29.274778
352.630597	17947.909654	29.279796
352.839844	17962.053216	29.284813
353.410791	17991.041829	29.289831
353.204754	18022.823227	29.294848
354.213214	18044.092361	29.299866
354.389782	18072.301437	29.304884
354.764684	18096.536693	29.309901
355.348162	18110.701989	29.314919
355.333826	18149.514248	29.319936
355.837702	18167.881318	29.324954
356.243908	18189.403235	29.329972
356.496071	18211.664799	29.334989
356.315959	18246.316156	29.340007
356.648076	18274.703187	29.345024
357.650713	18299.239982	29.350042
357.894967	18328.855503	29.355060
358.396234	18352.307221	29.360077
358.742735	18377.430393	29.365095
358.669899	18414.656015	29.370112
359.664924	18445.154827	29.375130
359.931257	18466.075980	29.380148
360.102806	18494.713818	29.385165
360.407085	18515.787975	29.390183
360.512984	18541.696882	29.395200
360.880366	18564.412782	29.400218
361.519065	18599.859458	29.405236
361.869257	18617.963971	29.410253
362.644887	18641.886189	29.415271
362.524290	18678.336799	29.420288
363.025440	18693.044338	29.425306
363.180197	18728.287622	29.430324
363.799801	18749.562118	29.435341
364.029410	18772.640049	29.440359
364.673127	18811.521493	29.445376
365.160094	18826.170015	29.450394
365.341423	18847.983818	29.455412
365.906750	18869.108227	29.460429
366.184989	18882.065090	29.465447
366.457043	18908.546131	29.470464
366.910687	18931.213571	29.475482
366.999905	18957.650857	29.480500
367.158486	18979.919475	29.485517
367.846678	18996.469206	29.490535
367.852402	19035.070525	29.495552
368.334345	19053.513147	29.500570
368.808375	19079.795496	29.505588
368.892558	19102.204289	29.510605
369.461587	19128.278656	29.515623
369.253040	19158.246483	29.520640
369.744349	19185.661230	29.525658
370.066721	19213.045652	29.530676
370.264748	19252.528449	29.535693
371.059112	19272.399960	29.540711
371.161902	19311.655874	29.545728
371.653826	19347.249824	29.550746
372.026769	19377.549038	29.555764
372.203799	19406.846524	29.560781
372.594487	19437.092460	29.565799
372.926929	19481.808163	29.570816
373.274888	19511.479560	29.575834
374.049165	19541.208149	29.580852
374.202505	19571.908245	29.585869
374.961326	19600.627351	29.590887
375.034984	19634.837554	29.595904
375.667676	19663.820434	29.600922
376.165562	19694.555169	29.605940
376.258651	19722.962151	29.610957
376.702393	19750.932767	29.615975
376.851538	19788.313888	29.620992
377.432607	19822.380581	29.626010
378.008956	19858.012094	29.631028
378.081370	19886.602505	29.636045
378.614963	19921.061943	29.641063
378.691460	19959.278446	29.646080
379.159541	19992.066651	29.651098
379.691351	20019.649486	29.656116
380.036803	20051.863728	29.661133
380.802317	20082.143386	29.666151
380.849754	20117.118833	29.671168
381.145403	20147.816924	29.676186
381.817225	20175.684282	29.681204
382.246796	20219.080440	29.686221
382.896153	20243.940295	29.691239
383.072595	20280.217511	29.696256
383.289958	20306.560034	29.701274
383.966633	20333.157669	29.706292
384.246277	20359.366989	29.711309
384.717953	20390.405320	29.716327
384.633344	20422.298870	29.721344
384.892682	20452.286158	29.726362
385.453778	20479.924816	29.731380
386.104551	20516.713699	29.736397
386.938253	20541.147746	29.741415
387.104261	20577.748967	29.746432
387.699639	20591.789853	29.751450
388.104320	20616.544128	29.756468
388.087499	20647.625945	29.761485
388.562871	20673.721374	29.766503
388.731072	20700.774264	29.771520
389.252731	20727.175870	29.776538
389.940126	20765.039250	29.781556
390.119172	20797.225702	29.786573
390.597631	20826.478926	29.791591
390.743109	20855.861416	29.796608
390.883050	20885.328437	29.801626
391.571771	20911.770481	29.806644
391.721049	20945.299166	29.811661
391.845599	20974.608069	29.816679
392.531602	21022.744370	29.821696
392.848129	21049.954589	29.826714
393.357198	21086.028702	29.831732
393.498205	21126.182817	29.836749
394.108865	21149.527325	29.841767
394.305120	21173.216377	29.846784
394.851533	21219.799639	29.851802
395.428006	21233.618723	29.856820
395.520436	21261.285778	29.861837
396.105363	21281.145464	29.866855
396.441452	21332.074584	29.871872
396.815481	21357.304883	29.876890
397.344105	21383.257001	29.881908
397.388064	21418.880602	29.886925
398.068514	21452.467440	29.891943
398.276190	21490.804454	29.896960
398.583423	21515.342822	29.901978
398.742144	21550.867293	29.906996
399.393783	21590.578501	29.912013
400.339436	21619.437276	29.917031
400.759305	21658.925265	29.922048
401.098227	21691.999898	29.927066
401.483192	21716.970338	29.932084
401.413944	21750.656621	29.937101
402.373858	21773.579960	29.942119
402.659381	21807.223407	29.947136
402.720012	21838.833847	29.952154
403.168658	21866.835550	29.957172
403.447552	21902.539543	29.962189
404.225853	21935.497784	29.967207
404.454696	21976.918144	29.972224
404.769381	22016.859567	29.977242
405.144157	22048.654923	29.982260
405.800596	22078.100034	29.987277
406.146848	22109.670014	29.992295
406.387815	22157.802789	29.997312
406.577188	22193.541133	30.002330
407.281006	22225.004845	30.007348
407.579231	22275.358074	30.012365
408.079232	22297.131489	30.017383
408.483798	22337.154976	30.022400
408.960574	22373.834795	30.027418
409.604586	22394.977427	30.032436
410.246865	22431.688322	30.037453
410.760969	22466.129383	30.042471
411.056145	22498.271467	30.047488
411.297775	22523.049216	30.052506
411.690230	22551.244264	30.057524
411.752547	22585.418167	30.062541
412.844026	22616.435277	30.067559
412.823528	22656.761663	30.072576
413.387129	22693.695867	30.077594
413.646769	22723.458491	30.082612
413.753562	22761.969605	30.087629
414.017483	22798.505808	30.092647
414.620196	22838.483492	30.097664
414.884410	22882.405835	30.102682
415.341997	22911.129988	30.107700
415.792177	22938.778414	30.112717
416.532959	22992.253682	30.117735
417.026375	23029.637026	30.122752
417.357172	23066.771411	30.127770
418.056489	23096.182812	30.132788
418.264566	23127.564674	30.137805
418.989150	23157.038228	30.142823
419.246004	23192.154093	30.147840
419.445797	23229.062942	30.152858
420.420293	23259.286914	30.157876
420.464079	23284.484856	30.162893
420.746802	23315.714366	30.167911
421.323498	23345.629026	30.172928
421.322321	23372.496598	30.177946
422.176932	23400.991872	30.182964
422.245800	23438.827991	30.187981
422.816782	23472.775990	30.192999
423.326528	23496.790133	30.198016
423.458895	23526.117917	30.203034
423.952820	23554.936490	30.208052
424.382468	23584.976830	30.213069
424.576538	23619.064769	30.218087
425.006351	23653.809189	30.223104
425.672232	23688.402648	30.228122
425.959888	23723.833051	30.233140
426.067041	23761.176272	30.238157
426.520021	23805.555452	30.243175
426.979243	23838.563892	30.248192
427.556520	23880.573039	30.253210
427.782884	23923.728467	30.258228
428.268579	23968.071115	30.263245
428.823642	24002.369736	30.268263
429.435757	24041.768366	30.273280
429.622323	24078.767973	30.278298
430.018984	24115.836971	30.283316
430.803608	24164.334878	30.288333
431.255535	24193.875853	30.293351
432.063277	24220.774889	30.298368
432.221884	24255.729425	30.303386
432.959744	24287.869431	30.308404
433.283207	24326.263057	30.313421
433.551675	24359.155835	30.318439
433.802671	24394.559002	30.323456
434.494273	24430.655746	30.328474
434.982800	24449.492703	30.333492
435.424042	24498.758042	30.338509
436.276635	24535.216309	30.343527
436.336372	24566.289459	30.348544
436.535337	24605.126956	30.353562
437.228567	24631.585101	30.358580
437.648560	24666.563451	30.363597
438.238590	24701.772365	30.368615
438.620516	24733.401231	30.373632
439.048616	24770.800775	30.378650
439.395454	24792.648468	30.383668
440.144727	24833.587493	30.388685
440.493616	24859.361768	30.393703
440.851830	24883.630036	30.398720
440.879322	24930.012856	30.403738
441.675645	24954.953087	30.408756
442.171739	24998.785721	30.413773
442.302362	25020.716799	30.418791
442.861384	25069.541633	30.423808
443.404141	25106.585443	30.428826
444.159450	25144.799040	30.433844
444.069178	25176.450094	30.438861
444.229636	25216.449765	30.443879
444.498583	25251.362834	30.448896
444.975007	25301.684454	30.453914
445.767456	25340.674575	30.458932
445.765353	25391.318522	30.463949
446.570886	25421.355078	30.468967
446.761087	25460.710093	30.473984
447.227240	25507.592783	30.479002
448.003300	25546.027787	30.484020
448.670706	25594.593301	30.489037
448.798842	25635.321611	30.494055
449.352798	25665.974301	30.499072
449.532692	25713.441146	30.504090
450.056834	25736.065030	30.509108
450.448243	25793.473989	30.514125
451.355640	25832.499826	30.519143
451.726052	25863.728932	30.524160
452.210104	25894.538694	30.529178
452.340007	25924.924516	30.534196
452.244325	25962.690914	30.539213
453.171839	26009.438686	30.544231
453.984155	26039.481511	30.549248
453.726424	26085.662298	30.554266
454.273651	26125.896576	30.559284
454.710713	26167.038702	30.564301
455.085022	26209.153383	30.569319
455.665102	26257.618508	30.574336
456.231944	26294.348610	30.579354
456.414150	26340.883110	30.584372
457.050071	26395.824750	30.589389
457.477026	26431.840172	30.594407
457.974210	26474.897251	30.599424
458.365301	26521.795121	30.604442
458.985635	26567.929668	30.609460
459.390502	26600.189048	30.614477
459.663456	26643.453994	30.619495
460.281359	26692.321000	30.624512
460.490732	26740.523923	30.629530
461.428155	26789.909280	30.634548
461.929007	26831.900440	30.639565
462.266482	26879.517904	30.644583
463.100903	26920.078731	30.649600
463.082612	26972.405011	30.654618
463.885284	27007.548754	30.659636
464.286942	27057.474630	30.664653
464.957643	27089.009560	30.669671
465.713124	27130.473513	30.674688
466.258193	27171.805198	30.679706
466.666708	27207.516145	30.684724
466.738430	27248.096708	30.689741
467.195444	27277.597975	30.694759
468.229606	27317.091993	30.699776
468.468021	27367.970058	30.704794
468.866121	27396.140595	30.709812
469.595449	27437.628540	30.714829
469.984594	27477.453641	30.719847
470.530753	27504.211841	30.724864
470.865239	27555.588753	30.729882
471.097520	27588.282323	30.734900
471.427396	27628.108114	30.739917
471.670368	27669.213374	30.744935
472.548086	27710.245234	30.749952
473.224986	27749.859301	30.754970
473.602564	27788.046628	30.759988
473.908887	27837.040982	30.765005
474.115690	27880.859403	30.770023
474.953523	27927.371680	30.775040
475.105867	27977.161645	30.780058
475.587677	28010.679091	30.785076
475.912219	28057.163091	30.790093
476.176429	28103.335422	30.795111
476.888879	28153.989069	30.800128
477.100015	28212.183537	30.805146
478.102886	28246.290314	30.810164
478.233623	28295.425429	30.815181
478.892506	28336.166892	30.820199
479.525780	28378.319699	30.825216
479.644244	28437.262151	30.830234
480.284147	28470.016110	30.835252
481.019715	28515.234509	30.840269
481.132105	28569.799613	30.845287
482.013450	28605.255363	30.850304
482.092336	28655.131978	30.855322
482.871638	28701.539285	30.860340
483.265632	28741.738742	30.865357
483.377938	28779.173977	30.870375
484.280494	28816.071546	30.875392
484.692288	28856.315644	30.880410
485.402494	28899.561166	30.885428
485.795358	28941.641546	30.890445
486.129366	28989.000351	30.895463
486.222012	29020.908922	30.900480
486.635487	29075.712870	30.905498
487.267946	29117.230317	30.910516
487.803263	29167.379895	30.915533
487.934271	29220.912306	30.920551
488.704681	29267.092282	30.925568
489.115675	29320.711169	30.930586
489.230055	29370.833186	30.935604
489.801201	29418.166529	30.940621
490.192001	29481.771416	30.945639
491.178271	29534.125278	30.950656
491.492405	29595.951261	30.955674
492.060204	29644.853781	30.960692
492.552152	29692.655285	30.965709
493.005197	29753.376681	30.970727
493.669708	29794.316225	30.975744
493.910038	29858.019940	30.980762
494.561487	29902.934041	30.985780
495.584563	29955.819425	30.990797
495.285848	30015.104397	30.995815
496.103272	30062.345089	31.000832
496.633697	30107.487974	31.005850
497.134820	30164.265342	31.010868
497.880640	30215.966921	31.015885
498.399552	30270.252345	31.020903
498.896585	30319.651182	31.025920
499.312730	30377.973517	31.030938
499.603255	30431.167708	31.035956
500.303145	30477.999876	31.040973
500.717628	30532.454834	31.045991
501.787002	30582.539012	31.051008
502.045637	30629.876856	31.056026
502.642447	30681.071244	31.061044
503.070171	30722.986061	31.066061
503.700543	30782.151416	31.071079
504.342184	30822.169523	31.076096
504.627620	30875.416381	31.081114
505.137028	30923.038497	31.086132
505.818732	30961.980684	31.091149
505.939863	31012.765697	31.096167
506.639258	31063.906359	31.101184
507.055161	31114.797492	31.106202
507.290703	31164.213572	31.111220
508.002267	31207.316265	31.116237
508.556283	31265.684982	31.121255
509.260725	31314.951320	31.126272
509.707114	31369.851631	31.131290
509.936764	31419.250468	31.136308
510.860933	31470.462393	31.141325
511.193253	31515.827831	31.146343
511.682498	31558.548518	31.151360
512.281254	31616.122163	31.156378
512.696472	31658.325249	31.161396
513.208428	31706.920896	31.166413
513.603099	31754.365455	31.171431
514.296919	31806.174966	31.176448
514.965748	31858.130756	31.181466
515.381977	31910.800591	31.186484
516.020860	31954.750152	31.191501
516.419937	31994.571249	31.196519
516.665279	32034.436808	31.201536
517.190903	32086.161378	31.206554
517.580266	32123.122428	31.211572
518.230355	32172.005723	31.216589
518.528725	32222.480889	31.221607
518.978527	32264.897421	31.226624
519.223179	32328.192814	31.231642
519.925541	32379.724911	31.236660
520.428059	32427.633054	31.241677
520.819353	32494.129648	31.246695
521.224745	32548.059044	31.251712
522.127644	32598.510974	31.256730
522.033581	32652.160452	31.261748
522.552413	32712.284746	31.266765
523.111667	32770.951017	31.271783
524.051868	32834.754752	31.276800
524.700002	32886.959956	31.281818
525.037186	32943.864888	31.286836
525.811844	32997.153920	31.291853
526.063502	33053.369666	31.296871
526.759580	33109.515203	31.301888
527.466157	33176.612225	31.306906
527.894171	33230.981729	31.311924
528.786734	33279.408254	31.316941
529.228511	33326.836595	31.321959
529.804674	33383.258444	31.326976
530.431956	33439.280714	31.331994
530.626222	33491.666930	31.337012
531.227289	33540.416941	31.342029
531.580710	33606.952357	31.347047
532.080785	33661.977096	31.352064
532.869449	33718.715121	31.357082
533.262685	33775.925845	31.362100
533.704579	33829.111489	31.367117
534.177590	33892.062233	31.372135
534.968144	33948.191622	31.377152
535.706115	34008.703737	31.382170
536.360826	34067.165978	31.387188
536.976888	34110.013820	31.392205
537.113083	34169.991752	31.397223
537.968388	34236.102482	31.402240
538.227986	34282.399025	31.407258
538.339881	34332.996226	31.412276
539.180040	34390.093935	31.417293
539.436250	34458.791393	31.422311
540.432192	34516.943017	31.427328
541.063780	34579.775263	31.432346
541.375774	34639.094507	31.437364
542.157929	34693.457195	31.442381
542.679722	34751.119984	31.447399
543.191068	34810.384715	31.452416
543.824585	34875.108047	31.457434
544.096463	34931.430490	31.462452
545.149237	34977.057918	31.467469
545.302598	35041.574114	31.472487
545.824402	35105.470975	31.477504
546.325660	35164.369300	31.482522
546.925933	35214.894484	31.487540
547.567043	35266.217822	31.492557
548.011120	35324.154098	31.497575
548.642300	35386.692574	31.502592
549.279062	35442.536494	31.507610
549.665648	35510.528392	31.512628
550.335852	35555.198051	31.517645
550.824703	35621.727996	31.522663
551.485624	35673.595209	31.527680
552.012250	35731.017325	31.532698
552.477510	35788.374034	31.537716
553.215407	35825.304005	31.542733
553.763312	35880.551712	31.547751
554.213456	35924.046772	31.552768
554.987248	35977.269073	31.557786
555.036273	36034.414547	31.562804
555.922152	36075.934750	31.567821
556.295257	36132.083234	31.572839
556.821718	36177.150642	31.577856
557.607082	36229.327099	31.582874
558.056931	36293.271639	31.587892
558.505296	36347.634591	31.592909
559.030573	36399.463213	31.597927
559.462298	36452.503650	31.602944
559.966834	36505.065081	31.607962
560.395891	36564.390227	31.612980
561.067461	36628.163547	31.617997
561.879134	36694.233720	31.623015
561.985653	36756.526042	31.628032
562.799330	36811.410685	31.633050
563.310110	36875.154668	31.638068
564.008441	36935.815750	31.643085
564.324171	36998.822318	31.648103
564.828113	37052.947784	31.653120
565.491647	37121.253414	31.658138
565.905036	37187.233473	31.663156
566.762395	37248.715174	31.668173
567.281957	37311.326125	31.673191
567.558831	37376.294188	31.678208
568.417700	37442.857979	31.683226
569.123597	37514.475388	31.688244
569.945294	37570.857111	31.693261
570.479886	37638.052888	31.698279
570.872377	37693.505442	31.703296
571.828966	37744.748896	31.708314
572.303429	37804.723955	31.713332
573.253732	37858.149841	31.718349
574.088028	37916.740039	31.723367
574.271004	37971.776740	31.728384
574.625818	38025.008100	31.733402
575.225731	38098.630743	31.738420
575.586901	38157.426258	31.743437
576.244490	38205.068461	31.748455
576.844541	38271.775962	31.753472
577.872281	38336.635836	31.758490
577.910976	38395.059348	31.763508
578.638956	38452.472547	31.768525
579.211888	38516.631814	31.773543
579.765588	38578.111435	31.778560
580.193552	38634.220695	31.783578
580.992379	38703.115931	31.788596
581.195420	38766.620740	31.793613
581.999695	38827.589412	31.798631
582.313706	38898.377476	31.803648
583.132901	38962.494404	31.808666
583.762938	39036.100057	31.813684
584.409533	39083.342325	31.818701
585.034589	39154.269309	31.823719
585.280220	39219.135461	31.828736
586.158273	39273.571791	31.833754
586.398844	39349.307594	31.838772
586.990784	39416.052177	31.843789
587.890062	39467.287859	31.848807
588.152630	39541.202564	31.853824
589.120449	39604.375392	31.858842
589.456392	39676.977938	31.863860
590.312098	39736.204930	31.868877
590.674471	39804.747209	31.873895
591.181520	39861.494273	31.878912
591.940612	39915.680713	31.883930
592.312461	39986.662279	31.888948
592.854630	40038.340613	31.893965
593.582418	40097.750932	31.898983
593.878177	40165.529006	31.904000
594.818476	40229.033688	31.909018
594.908892	40296.581048	31.914036
595.860608	40351.911241	31.919053
596.359549	40424.647609	31.924071
596.883714	40483.477279	31.929088
597.535804	40547.744197	31.934106
597.882760	40613.766542	31.939124
598.362936	40676.243989	31.944141
598.986063	40749.541958	31.949159
599.475673	40827.316720	31.954176
600.373357	40886.035361	31.959194
600.820691	40969.819037	31.964212
601.373319	41034.962797	31.969229
602.368814	41107.023030	31.974247
602.723429	41188.007023	31.979264
603.777983	41249.122267	31.984282
604.321700	41333.699833	31.989300
604.618399	41391.932317	31.994317
605.466924	41453.369614	31.999335
606.014752	41529.969598	32.004352
606.993440	41595.875139	32.009370
607.412797	41662.425945	32.014388
608.117220	41729.993757	32.019405
608.515206	41801.101093	32.024423
608.892914	41872.707721	32.029440
609.550623	41936.855410	32.034458
610.036321	42016.773174	32.039476
610.716306	42092.599063	32.044493
611.786738	42163.804900	32.049511
612.196957	42246.779629	32.054528
613.083895	42300.939287	32.059546
613.280349	42374.339536	32.064564
613.696795	42454.283267	32.069581
614.564272	42522.587868	32.074599
614.735728	42611.956028	32.079616
615.545624	42677.947012	32.084634
616.509632	42760.589298	32.089652
617.283509	42839.424180	32.094669
617.922226	42907.452316	32.099687
618.668534	42976.728970	32.104704
618.762589	43038.792035	32.109722
619.479780	43121.003161	32.114740
620.475746	43191.887422	32.119757
621.129694	43259.251284	32.124775
621.537617	43344.785559	32.129792
622.061991	43419.265991	32.134810
622.538384	43485.195031	32.139828
623.333296	43563.394859	32.144845
624.217054	43638.463966	32.149863
624.909723	43708.604706	32.154880
625.746260	43773.019609	32.159898
625.839908	43855.062434	32.164916
626.708906	43928.843759	32.169933
627.152900	44000.217090	32.174951
627.715244	44085.176642	32.179968
628.481472	44151.855757	32.184986
629.033211	44231.137417	32.190004
629.171672	44298.069318	32.195021
630.200802	44366.306553	32.200039
630.663587	44453.532395	32.205056
631.486524	44522.126380	32.210074
632.203031	44605.465062	32.215092
632.717460	44672.197158	32.220109
633.624963	44733.285016	32.225127
633.836408	44811.049792	32.230144
634.167827	44889.388669	32.235162
634.962150	44948.740324	32.240180
635.717084	45023.788924	32.245197
636.473381	45088.619480	32.250215
637.203366	45165.330531	32.255232
637.510191	45238.395337	32.260250
637.965649	45306.045684	32.265268
638.753804	45386.928773	32.270285
639.720987	45458.262123	32.275303
639.810806	45539.886630	32.280320
640.739195	45609.543910	32.285338
641.500343	45685.617218	32.290356
642.322480	45764.630080	32.295373
642.922507	45839.770710	32.300391
643.416738	45909.807230	32.305408
644.251930	45981.852791	32.310426
644.626890	46067.202793	32.315444
645.216201	46148.835704	32.320461
646.353070	46219.401768	32.325479
647.077900	46302.714990	32.330496
647.608869	46380.297568	32.335514
648.512796	46447.255702	32.340532
648.778369	46517.272298	32.345549
649.242443	46594.317349	32.350567
650.023714	46674.840767	32.355584
650.498926	46754.373051	32.360602
651.434654	46831.884193	32.365620
652.018238	46907.679150	32.370637
652.605681	46980.189500	32.375655
653.238058	47055.329592	32.380672
653.999324	47134.200335	32.385690
654.812258	47220.379923	32.390708
655.256224	47300.563889	32.395725
655.780707	47373.300897	32.400743
656.282969	47459.709815	32.405760
657.021119	47554.111011	32.410778
657.924205	47635.704710	32.415796
658.495586	47709.070010	32.420813
659.157488	47795.826691	32.425831
659.819155	47877.985610	32.430848
660.609821	47952.196674	32.435866
661.175714	48038.212393	32.440884
661.702579	48131.208133	32.445901
662.481085	48203.700998	32.450919
663.019901	48298.435717	32.455936
663.476369	48383.874198	32.460954
664.229362	48472.798026	32.465972
664.904057	48565.329268	32.470989
666.029310	48640.435112	32.476007
666.525454	48733.928385	32.481024
667.096248	48810.153053	32.486042
667.970160	48902.283446	32.491060
668.314482	48985.832408	32.496077
669.133482	49069.818004	32.501095
669.848985	49159.591325	32.506112
670.744395	49240.930996	32.511130
671.279305	49318.752256	32.516148
671.576985	49410.746702	32.521165
672.713722	49485.484426	32.526183
673.292973	49579.170193	32.531200
673.984691	49654.291719	32.536218
674.433420	49740.309178	32.541236
674.878029	49823.292460	32.546253
676.202371	49902.776300	32.551271
676.823123	50000.642174	32.556288
677.408809	50075.482829	32.561306
678.098671	50149.125271	32.566324
678.087335	50234.785175	32.571341
679.066483	50308.525656	32.576359
679.830405	50392.529287	32.581376
680.330319	50463.102690	32.586394
681.084999	50551.997940	32.591412
681.437876	50628.875449	32.596429
682.525607	50711.734038	32.601447
682.893664	50800.978664	32.606464
683.678436	50887.501541	32.611482
684.132833	50974.098413	32.616500
685.030401	51065.897253	32.621517
685.837500	51145.329638	32.626535
686.377791	51231.401748	32.631552
686.929121	51310.510719	32.636570
687.653233	51416.490727	32.641588
688.294915	51503.520141	32.646605
689.173382	51584.294435	32.651623
689.490439	51688.113217	32.656640
690.169718	51780.595926	32.661658
691.182085	51862.366337	32.666676
692.221432	51963.432693	32.671693
693.176219	52048.776504	32.676711
693.671733	52135.365423	32.681728
694.251116	52226.097846	32.686746
695.458621	52312.279152	32.691764
695.996791	52403.537265	32.696781
696.623924	52480.661013	32.701799
697.445534	52567.166310	32.706816
697.899277	52646.176809	32.711834
698.483460	52731.742860	32.716852
699.115828	52830.714035	32.721869
699.994705	52914.482097	32.726887
700.884738	53006.638807	32.731904
701.392892	53096.041342	32.736922
702.064024	53188.146668	32.741940
702.603751	53266.842184	32.746957
703.800422	53360.895762	32.751975
704.258114	53456.999039	32.756992
704.768946	53545.240660	32.762010
705.491375	53635.501048	32.767028
706.273568	53738.432402	32.772045
706.672702	53825.493319	32.777063
707.582302	53925.510868	32.782080
707.850057	54017.200312	32.787098
708.888189	54109.558833	32.792116
709.634422	54213.711721	32.797133
710.764029	54295.517126	32.802151
711.324459	54397.465049	32.807168
711.665430	54494.736312	32.812186
712.566041	54588.895287	32.817204
713.451204	54688.383687	32.822221
714.183357	54781.737418	32.827239
714.787747	54872.951809	32.832256
715.506774	54972.601811	32.837274
716.303961	55055.457363	32.842292
716.749035	55160.176861	32.847309
717.817846	55247.594516	32.852327
718.540778	55343.429309	32.857344
719.079962	55436.963381	32.862362
720.332890	55524.876249	32.867380
720.592243	55620.852259	32.872397
721.273017	55719.286513	32.877415
721.931510	55810.034996	32.882432
722.604818	55908.427190	32.887450
723.496954	55989.438484	32.892468
724.046368	56097.109190	32.897485
724.678959	56188.868385	32.902503
725.428019	56284.058866	32.907520
725.976402	56364.654635	32.912538
726.967437	56458.137717	32.917556
727.220248	56546.921959	32.922573
728.226518	56635.259683	32.927591
729.126692	56726.389417	32.932608
729.867855	56813.090915	32.937626
730.520477	56906.549932	32.942644
731.172828	57000.584474	32.947661
731.922241	57098.489695	32.952679
732.859504	57192.996182	32.957696
733.339921	57281.859781	32.962714
734.270544	57373.316028	32.967732
735.291443	57468.050111	32.972749
735.919499	57562.432552	32.977767
736.549098	57659.924304	32.982784
737.206167	57751.490723	32.987802
738.089610	57832.036978	32.992820
738.929882	57936.225393	32.997837
739.695943	58024.172944	33.002855
740.283097	58115.891618	33.007872
740.580716	58204.208145	33.012890
741.405603	58303.237956	33.017908
742.067410	58406.706303	33.022925
742.870127	58506.366419	33.027943
743.481939	58609.724006	33.032960
744.339301	58726.641468	33.037978
745.080235	58823.248322	33.042996
745.579597	58937.571945	33.048013
746.321809	59043.457043	33.053031
747.015611	59152.106145	33.058048
747.904662	59264.900958	33.063066
748.841542	59376.146434	33.068084
749.577076	59477.768984	33.073101
750.395361	59588.156773	33.078119
750.997955	59689.682298	33.083136
751.703177	59802.352513	33.088154
752.773703	59904.351548	33.093172
753.460130	60025.020981	33.098189
753.973735	60123.251666	33.103207
754.856401	60229.296689	33.108224
755.442215	60342.027570	33.113242
756.780379	60448.996982	33.118260
757.220097	60553.062892	33.123277
758.145123	60663.628476	33.128295
758.397791	60779.772964	33.133312
759.440264	60888.329436	33.138330
760.239091	60991.143630	33.143348
761.173638	61102.361019	33.148365
761.984309	61211.096602	33.153383
762.947964	61317.765938	33.158400
763.362754	61429.216455	33.163418
764.513684	61536.785072	33.168436
765.098734	61648.012678	33.173453
765.869736	61749.647017	33.178471
766.742394	61848.389145	33.183488
767.282471	61968.057685	33.188506
767.863958	62066.931199	33.193524
768.445041	62179.868940	33.198541
769.372539	62298.160599	33.203559
770.320366	62397.828414	33.208576
770.974798	62521.956408	33.213594
771.920234	62618.376764	33.218612
772.519891	62733.615279	33.223629
773.386943	62853.557251	33.228647
774.038425	62951.917762	33.233664
774.392301	63071.661444	33.238682
775.498176	63176.060300	33.243700
776.152665	63278.043838	33.248717
777.019092	63380.555402	33.253735
778.370672	63496.621966	33.258752
778.575947	63599.623251	33.263770
779.298607	63693.601253	33.268788
780.401541	63804.110071	33.273805
780.639456	63909.054441	33.278823
781.667334	64004.576332	33.283840
782.455953	64115.834150	33.288858
783.226252	64214.509720	33.293876
783.943825	64332.398938	33.298893
784.965064	64453.544714	33.303911
785.900349	64556.512172	33.308928
786.379685	64666.977022	33.313946
787.229000	64774.049800	33.318964
788.313375	64883.145084	33.323981
788.771709	64994.222015	33.328999
789.747918	65093.980303	33.334016
790.262520	65211.073612	33.339034
790.777532	65326.106630	33.344052
791.794213	65442.220502	33.349069
792.579692	65558.638777	33.354087
793.183755	65675.498628	33.359104
793.819086	65790.779816	33.364122
794.778875	65922.672486	33.369140
795.604647	66043.233958	33.374157
796.165735	66174.309090	33.379175
797.282838	66279.549848	33.384192
797.691249	66416.354195	33.389210
798.528904	66533.666986	33.394228
799.967946	66661.938344	33.399245
800.379369	66788.907399	33.404263
801.747222	66896.967390	33.409280
802.465812	67018.898816	33.414298
802.848520	67135.746504	33.419316
803.968193	67254.622521	33.424333
804.552893	67384.398889	33.429351
805.653839	67497.722040	33.434368
806.622298	67624.762046	33.439386
807.638075	67744.170120	33.444404
808.100182	67865.320617	33.449421
809.273359	67981.011664	33.454439
810.290214	68094.491018	33.459456
810.508707	68219.502655	33.464474
811.143751	68335.335228	33.469492
812.316516	68454.089075	33.474509
813.027071	68576.745268	33.479527
813.781429	68699.976614	33.484544
814.613106	68830.808496	33.489562
815.719521	68944.283902	33.494580
816.506200	69059.880367	33.499597
816.946853	69174.345993	33.504615
817.842600	69298.290869	33.509632
818.684533	69423.067348	33.514650
819.599675	69555.274596	33.519668
820.241147	69676.481613	33.524685
820.983653	69792.424472	33.529703
822.218550	69910.841043	33.534720
822.690468	70044.585260	33.539738
823.657768	70169.067139	33.544756
824.412783	70292.667990	33.549773
825.047507	70423.972182	33.554791
826.065979	70537.887932	33.559808
826.693179	70662.827295	33.564826
827.460458	70793.814627	33.569844
828.305567	70910.821529	33.574861
828.727182	71042.980466	33.579879
829.710753	71182.268657	33.584896
830.497267	71293.906067	33.589914
831.288248	71415.117137	33.594932
832.409768	71535.679802	33.599949
833.175036	71663.675384	33.604967
834.113372	71778.173750	33.609984
834.947822	71910.908404	33.615002
835.781049	72022.921277	33.620020
836.804566	72141.315528	33.625037
837.766287	72263.660360	33.630055
838.098660	72388.057712	33.635072
839.072728	72511.407386	33.640090
839.597348	72642.907702	33.645108
840.879377	72763.659347	33.650125
841.636981	72889.880091	33.655143
842.350548	73007.552486	33.660160
843.379323	73146.877456	33.665178
843.852864	73275.392450	33.670196
845.648092	73400.881693	33.675213
846.182557	73534.801575	33.680231
846.743472	73648.670247	33.685248
847.687718	73780.613957	33.690266
848.621952	73905.470631	33.695284
850.004482	74030.070466	33.700301
850.406977	74157.988945	33.705319
851.468827	74280.442380	33.710336
852.065424	74409.152387	33.715354
852.711051	74537.260542	33.720372
853.777784	74665.634992	33.725389
854.495890	74793.340536	33.730407
855.312155	74935.064758	33.735424
856.338765	75062.429909	33.740442
856.876077	75200.748754	33.745460
858.018885	75340.606409	33.750477
858.968186	75482.299498	33.755495
859.563577	75607.120691	33.760512
860.384327	75747.059488	33.765530
861.228535	75880.455425	33.770548
862.108435	76018.729056	33.775565
862.630540	76145.684236	33.780583
863.906076	76292.268302	33.785600
865.060805	76439.455217	33.790618
865.423494	76580.499687	33.795636
866.431156	76706.726292	33.800653
867.087855	76862.050176	33.805671
868.240021	76995.218456	33.810688
869.169320	77141.688291	33.815706
869.914265	77286.032679	33.820724
871.068929	77418.652785	33.825741
871.583315	77565.845530	33.830759
872.908138	77697.300595	33.835776
873.239499	77838.427783	33.840794
874.252619	77981.777182	33.845812
875.182844	78126.583414	33.850829
875.741269	78264.905184	33.855847
876.651330	78411.120849	33.860864
877.439068	78564.859836	33.865882
878.359611	78708.026771	33.870900
879.580748	78851.050018	33.875917
880.188736	79008.984057	33.880935
881.225674	79145.315415	33.885952
882.385013	79298.061744	33.890970
882.944064	79441.887757	33.895988
884.149594	79580.097935	33.901005
884.517158	79730.821023	33.906023
885.497192	79868.507254	33.911040
886.668982	80018.941103	33.916058
887.326818	80177.495014	33.921076
888.241687	80313.493026	33.926093
889.045402	80457.221765	33.931111
889.918282	80590.527133	33.936128
890.745700	80729.920267	33.941146
891.288907	80866.242431	33.946164
892.522268	81001.641507	33.951181
893.233432	81144.725641	33.956199
894.364305	81280.503925	33.961216
895.110110	81421.825346	33.966234
896.019623	81566.973355	33.971252
897.077661	81709.959380	33.976269
897.635621	81852.004112	33.981287
898.614047	81993.062839	33.986304
899.637548	82151.392863	33.991322
900.084118	82293.193035	33.996340
901.409873	82439.802454	34.001357
902.188309	82604.641982	34.006375
903.177648	82753.725844	34.011392
904.102556	82899.980601	34.016410
904.768849	83054.820274	34.021428
906.017901	83211.797994	34.026445
906.861494	83364.959115	34.031463
907.608563	83518.725621	34.036480
908.401213	83676.180578	34.041498
909.310629	83830.415813	34.046516
910.767141	83990.382513	34.051533
911.121627	84151.424698	34.056551
911.996880	84305.694056	34.061568
913.143490	84464.956022	34.066586
913.582661	84623.804587	34.071604
914.625403	84776.378974	34.076621
915.493871	84946.408682	34.081639
916.492821	85115.038680	34.086656
917.597824	85279.710366	34.091674
918.214892	85449.943506	34.096692
919.549703	85613.364662	34.101709
920.260819	85778.282173	34.106727
921.585881	85949.933135	34.111744
922.411848	86099.173067	34.116762
923.130976	86279.696784	34.121780
924.168274	86443.989210	34.126797
925.284298	86612.401815	34.131815
926.331446	86773.651247	34.136832
927.166174	86923.280960	34.141850
928.147010	87102.173079	34.146868
929.213103	87257.025154	34.151885
929.902899	87426.437945	34.156903
931.017825	87579.594478	34.161920
932.384646	87745.493098	34.166938
932.753329	87916.690072	34.171956
933.836349	88072.228121	34.176973
934.708126	88233.738000	34.181991
935.687904	88393.800928	34.187008
937.006882	88553.726569	34.192026
937.533082	88730.681105	34.197044
938.852295	88882.584558	34.202061
939.709650	89047.241228	34.207079
940.427797	89209.036265	34.212096
941.542259	89367.184909	34.217114
942.330839	89539.431592	34.222132
943.487706	89696.176783	34.227149
944.228217	89858.573729	34.232167
945.148895	90023.017794	34.237184
946.294646	90186.862504	34.242202
946.925456	90346.091201	34.247220
947.981853	90522.414357	34.252237
948.935405	90689.654886	34.257255
949.713872	90851.805433	34.262272
950.387836	91012.025032	34.267290
951.382717	91187.673366	34.272308
952.323031	91320.832451	34.277325
953.183600	91503.024199	34.282343
953.957559	91652.807496	34.287360
955.042426	91813.160647	34.292378
955.732898	91989.441087	34.297396
956.762238	92153.324709	34.302413
957.927729	92326.028955	34.307431
958.988199	92486.207030	34.312448
960.310982	92653.267128	34.317466
960.644881	92813.263693	34.322484
962.087247	92980.844259	34.327501
963.142002	93158.383109	34.332519
963.809511	93319.587390	34.337536
965.071140	93482.637670	34.342554
965.671200	93660.698423	34.347572
966.643623	93823.089871	34.352589
967.644688	93992.585943	34.357607
968.484477	94177.472226	34.362624
969.505473	94352.854180	34.367642
970.378812	94529.002393	34.372660
971.567072	94699.592759	34.377677
972.250494	94878.667643	34.382695
972.946515	95057.172037	34.387712
974.233136	95230.326110	34.392730
974.983927	95428.611866	34.397748
976.250546	95608.855272	34.402765
976.960441	95782.880848	34.407783
977.899659	95971.334310	34.412800
979.463981	96150.361316	34.417818
979.996286	96347.981533	34.422836
980.685302	96515.520754	34.427853
982.040402	96711.583450	34.432871
983.151221	96904.833034	34.437888
984.071979	97080.681282	34.442906
985.046126	97268.784238	34.447924
986.268916	97453.929074	34.452941
987.100205	97651.946941	34.457959
988.577335	97834.741830	34.462976
989.529987	98012.256296	34.467994
990.343029	98200.677740	34.473012
991.262014	98382.809200	34.478029
992.319827	98575.440959	34.483047
993.616926	98760.152593	34.488064
994.651858	98941.787749	34.493082
995.249952	99124.553723	34.498100
996.287629	99317.840214	34.503117
997.018946	99515.199099	34.508135
998.404732	99701.954200	34.513152
999.348705	99885.345874	34.518170
1000.065094	100076.247393	34.523188
1001.306796	100265.638925	34.528205
1002.288776	100459.291493	34.533223
1003.059778	100651.080988	34.538240
1004.433309	100847.995734	34.543258
1005.239936	101049.076891	34.548276
1006.482815	101230.820563	34.553293
1007.383551	101411.583712	34.558311
1008.227896	101604.203953	34.563328
1009.385409	101798.204809	34.568346
1010.320702	101987.324107	34.573364
1011.280381	102181.031296	34.578381
1012.547470	102367.939370	34.583399
1013.293476	102567.788665	34.588416
1014.585393	102761.438918	34.593434
1015.870141	102949.374028	34.598452
1016.842785	103140.249502	34.603469
1017.914788	103317.445354	34.608487
1018.783780	103496.069040	34.613504
1019.658310	103668.234242	34.618522
1020.563478	103848.184101	34.623540
1021.836996	104025.313435	34.628557
1022.516264	104191.106142	34.633575
1023.593007	104382.188759	34.638592
1024.379247	104562.619109	34.643610
1025.487596	104748.810580	34.648628
1026.441957	104941.031993	34.653645
1027.485875	105118.155993	34.658663
1028.433994	105311.115701	34.663680
1029.223881	105493.438907	34.668698
1030.026145	105693.176053	34.673716
1031.408253	105884.700330	34.678733
1032.584571	106086.974987	34.683751
1033.248369	106281.901253	34.688768
1034.482516	106473.631557	34.693786
1035.387004	106683.542409	34.698804
1036.318490	106878.454104	34.703821
1037.475089	107071.620099	34.708839
1038.474108	107278.087525	34.713856
1039.753118	107485.143550	34.718874
1040.730316	107677.469613	34.723892
1041.741991	107892.299367	34.728909
1043.071126	108101.631789	34.733927
1043.758042	108308.196732	34.738944
1045.021669	108507.359271	34.743962
1045.805684	108708.907919	34.748980
1046.611952	108928.466556	34.753997
1047.869705	109144.747596	34.759015
1048.372191	109363.207294	34.764032
1049.584328	109574.774511	34.769050
1050.803957	109793.689106	34.774068
1051.974557	110016.021068	34.779085
1053.025069	110225.859309	34.784103
1053.958797	110454.681709	34.789120
1055.371743	110661.815859	34.794138
1056.044774	110883.743105	34.799156
1057.322973	111105.660756	34.804173
1058.450987	111317.698732	34.809191
1059.217679	111543.289500	34.814208
1060.653602	111762.602092	34.819226
1061.581489	111978.542008	34.824244
1062.469653	112205.600276	34.829261
1063.864891	112415.474217	34.834279
1064.881533	112644.769811	34.839296
1066.146454	112865.031534	34.844314
1067.393828	113084.069037	34.849332
1068.123829	113306.145635	34.854349
1068.859462	113523.864964	34.859367
1070.108037	113747.455606	34.864384
1071.486883	113969.126129	34.869402
1072.726292	114205.758452	34.874420
1073.524343	114423.259065	34.879437
1074.722541	114638.389365	34.884455
1075.659512	114869.984177	34.889472
1076.880196	115088.446271	34.894490
1078.226731	115308.726353	34.899508
1078.962325	115530.680216	34.904525
1080.452975	115746.695490	34.909543
1081.261507	115974.050806	34.914560
1082.475446	116186.846315	34.919578
1083.684433	116419.511097	34.924596
1084.605403	116632.295017	34.929613
1085.804982	116848.442789	34.934631
1086.716250	117078.032567	34.939648
1087.619219	117302.722035	34.944666
1088.723325	117523.844883	34.949684
1089.843552	117747.906386	34.954701
1091.061442	117948.651738	34.959719
1091.510326	118167.264983	34.964736
1092.720000	118376.149428	34.969754
1093.883452	118592.759754	34.974772
1094.853382	118813.281098	34.979789
1096.157686	119029.947427	34.984807
1097.097034	119254.557347	34.989824
1097.783687	119462.192904	34.994842
1099.328899	119698.186481	34.999860
1100.197723	119935.675014	35.004877
1101.402473	120149.806426	35.009895
1102.053531	120379.401993	35.014912
1103.565175	120614.268025	35.019930
1104.604893	120851.482270	35.024948
1105.614442	121083.723223	35.029965
1106.912979	121318.021829	35.034983
1107.388302	121557.793491	35.040000
1108.733608	121790.161891	35.045018
1109.931854	122032.390390	35.050036
1111.022086	122278.655978	35.055053
1112.122396	122517.926525	35.060071
1112.911105	122773.687322	35.065088
1114.462245	123018.919670	35.070106
1115.469490	123266.233635	35.075124
1116.231575	123512.867794	35.080141
1117.739996	123749.317930	35.085159
1118.574838	124017.058021	35.090176
1119.955973	124263.494588	35.095194
1120.993626	124518.227846	35.100212
1121.902611	124772.338154	35.105229
1123.345737	125019.885919	35.110247
1124.475202	125282.924490	35.115264
1125.770865	125532.756778	35.120282
1126.803231	125784.256940	35.125300
1128.158972	126046.428181	35.130317
1129.809236	126295.282846	35.135335
1130.483039	126545.834583	35.140352
1131.825415	126795.415951	35.145370
1132.795247	127045.618619	35.150388
1133.798445	127308.822181	35.155405
1135.319766	127553.208754	35.160423
1136.778246	127810.675612	35.165440
1137.835866	128065.840623	35.170458
1139.264798	128310.590659	35.175476
1139.996292	128561.504062	35.180493
1141.332382	128802.052409	35.185511
1142.543934	129051.027081	35.190528
1143.735668	129298.029604	35.195546
1144.848513	129545.186544	35.200564
1145.430153	129795.247282	35.205581
1147.153435	130045.704354	35.210599
1148.005410	130307.753933	35.215616
1149.081274	130556.674195	35.220634
1150.526609	130808.197341	35.225652
1151.712889	131057.230033	35.230669
1153.318237	131294.634470	35.235687
1154.244596	131549.557819	35.240704
1155.218179	131791.355064	35.245722
1156.646554	132038.821508	35.250740
1157.562500	132287.249277	35.255757
1158.860398	132526.298271	35.260775
1159.770717	132786.165411	35.265792
1160.983505	133035.437261	35.270810
1162.396408	133287.416229	35.275828
1163.443213	133536.161572	35.280845
1164.804077	133776.667284	35.285863
1165.932503	134011.470286	35.290880
1167.173367	134247.093111	35.295898
1168.063004	134483.333517	35.300916
1169.355287	134721.486796	35.305933
1170.365086	134943.486179	35.310951
1170.956238	135186.703110	35.315968
1172.262976	135431.565787	35.320986
1173.320822	135675.495209	35.326004
1174.057269	135917.755320	35.331021
1175.859055	136167.359339	35.336039
1176.721200	136411.313850	35.341056
1177.433644	136669.507528	35.346074
1178.961323	136922.065908	35.351092
1180.003797	137177.888769	35.356109
1181.146241	137438.831980	35.361127
1182.301856	137708.003664	35.366144
1183.129553	137958.631584	35.371162
1184.519072	138227.439097	35.376180
1185.622918	138506.553467	35.381197
1186.996645	138766.822081	35.386215
1188.305776	139039.909586	35.391232
1189.473253	139305.808052	35.396250
1190.780908	139571.216272	35.401268
1191.999615	139847.330263	35.406285
1193.283993	140115.536093	35.411303
1194.511516	140386.834639	35.416320
1195.663349	140653.240668	35.421338
1197.015885	140924.256500	35.426356
1197.518140	141203.796643	35.431373
1198.989855	141469.243104	35.436391
1200.518893	141745.942330	35.441408
1201.517117	142028.450420	35.446426
1203.315833	142296.955866	35.451444
1204.144945	142573.092602	35.456461
1205.634319	142851.138615	35.461479
1207.037697	143119.195799	35.466496
1208.133700	143394.178945	35.471514
1209.708673	143646.461954	35.476532
1210.659454	143929.437004	35.481549
1211.844581	144201.393561	35.486567
1213.392322	144480.228981	35.491584
1214.310349	144753.311824	35.496602
1215.469584	145012.128131	35.501620
1216.440428	145298.724985	35.506637
1218.147609	145570.542252	35.511655
1219.612519	145849.757116	35.516672
1220.398018	146126.068139	35.521690
1221.740146	146399.334332	35.526708
1222.337746	146682.605074	35.531725
1223.986504	146955.710627	35.536743
1225.213201	147231.969811	35.541760
1226.339704	147520.372085	35.546778
1227.788285	147797.245666	35.551796
1228.809177	148088.510758	35.556813
1230.247796	148366.950243	35.561831
1231.185447	148649.254130	35.566848
1232.456982	148939.000604	35.571866
1233.936720	149211.313776	35.576884
1234.913640	149505.691949	35.581901
1236.133373	149788.236888	35.586919
1237.482191	150063.241401	35.591936
1238.850199	150366.833225	35.596954
1240.255379	150648.085643	35.601972
1241.285708	150923.111041	35.606989
1242.363525	151204.637339	35.612007
1243.803468	151485.940978	35.617024
1244.722846	151773.839596	35.622042
1246.536302	152055.123754	35.627060
1247.500156	152334.597071	35.632077
1248.771007	152604.013856	35.637095
1250.181422	152872.990880	35.642112
1251.146995	153143.958654	35.647130
1252.760065	153407.654584	35.652148
1253.753800	153683.111777	35.657165
1254.981719	153950.540899	35.662183
1256.444452	154222.803976	35.667200
1257.531900	154499.316974	35.672218
1259.102373	154767.443478	35.677236
1259.668157	155053.116313	35.682253
1261.153272	155322.618011	35.687271
1262.590400	155600.932986	35.692288
1263.350909	155886.605041	35.697306
1264.858750	156155.055782	35.702324
1265.873282	156447.400428	35.707341
1267.699692	156721.510779	35.712359
1269.029769	157007.870550	35.717376
1270.282641	157283.069028	35.722394
1271.480875	157565.103373	35.727412
1272.900711	157861.590334	35.732429
1273.817653	158142.330504	35.737447
1275.354907	158432.636860	35.742464
1276.531811	158722.484720	35.747482
1277.849599	159013.300879	35.752500
1279.261357	159306.628154	35.757517
1280.267778	159594.886526	35.762535
1281.720859	159887.957394	35.767552
1282.974043	160182.776075	35.772570
1284.246901	160465.389013	35.777588
1285.555916	160767.522843	35.782605
1287.027091	161057.998206	35.787623
1288.641904	161353.564690	35.792640
1289.256529	161650.579972	35.797658
1290.791049	161943.842158	35.802676
1292.384505	162252.397435	35.807693
1293.536300	162543.570220	35.812711
1295.034103	162836.476738	35.817728
1296.075837	163141.044331	35.822746
1297.429667	163420.986676	35.827764
1298.913323	163737.158042	35.832781
1299.972127	164039.280484	35.837799
1301.133940	164336.820394	35.842816
1302.414514	164644.784891	35.847834
1303.917078	164942.107697	35.852852
1305.336301	165251.918721	35.857869
1306.626236	165549.534579	35.862887
1308.244189	165850.003861	35.867904
1309.296377	166156.481491	35.872922
1310.847539	166456.268093	35.877940
1311.988391	166767.315842	35.882957
1313.222178	167061.423774	35.887975
1314.879326	167370.334851	35.892992
1315.595652	167684.796308	35.898010
1317.012103	167969.591823	35.903028
1318.558483	168286.394634	35.908045
1319.869253	168591.590051	35.913063
1321.150729	168897.896323	35.918080
1322.106325	169215.209332	35.923098
1323.529826	169524.770172	35.928116
1325.063439	169837.170024	35.933133
1326.338783	170150.832881	35.938151
1327.627043	170459.242251	35.943168
1328.602605	170765.738463	35.948186
1330.107688	171082.250221	35.953204
1331.472203	171398.165561	35.958221
1332.778492	171712.671389	35.963239
1334.334876	172020.209247	35.968256
1335.450871	172331.146704	35.973274
1336.887142	172633.619690	35.978292
1338.311578	172929.624535	35.983309
1339.403618	173230.635387	35.988327
1340.929175	173525.624685	35.993344
1341.925673	173828.266769	35.998362
1343.445576	174119.250458	36.003380
1344.593191	174432.607580	36.008397
1345.769617	174734.223047	36.013415
1347.788971	175034.812716	36.018432
1349.091999	175332.844852	36.023450
1350.751788	175621.771189	36.028468
1351.612919	175932.748634	36.033485
1353.154302	176240.074791	36.038503
1354.522291	176534.486500	36.043520
1355.741050	176849.421012	36.048538
1357.170758	177149.423009	36.053556
1358.173613	177458.368653	36.058573
1359.581202	177780.473852	36.063591
1361.358117	178093.915176	36.068608
1362.434874	178410.735912	36.073626
1363.875147	178718.538176	36.078644
1365.005282	179046.916221	36.083661
1365.961023	179364.384774	36.088679
1367.260931	179686.494436	36.093696
1368.469488	180030.844999	36.098714
1369.962810	180358.727150	36.103732
1371.626439	180693.475095	36.108749
1373.201658	181028.620561	36.113767
1374.648954	181350.944614	36.118784
1375.943387	181695.215781	36.123802
1377.416210	182026.919465	36.128820
1378.904545	182350.892846	36.133837
1380.092263	182689.654095	36.138855
1381.660779	183023.290128	36.143872
1382.545867	183365.710392	36.148890
1384.329873	183697.017561	36.153908
1386.240584	184038.206360	36.158925
1387.227543	184379.854584	36.163943
1388.472470	184709.276853	36.168960
1390.114007	185055.695269	36.173978
1391.614889	185386.907101	36.178996
1393.030303	185731.755049	36.184013
1394.115823	186068.040766	36.189031
1395.800871	186400.472123	36.194048
1396.954509	186740.952164	36.199066
1398.384979	187089.474389	36.204084
1399.935514	187443.881513	36.209101
1401.009532	187775.139807	36.214119
1402.954443	188121.717296	36.219136
1404.184739	188480.321944	36.224154
1405.989398	188836.091958	36.229172
1407.573494	189163.529126	36.234189
1409.260388	189502.452109	36.239207
1410.683462	189824.562596	36.244224
1412.103985	190167.075116	36.249242
1413.020525	190507.057835	36.254260
1414.582358	190840.740916	36.259277
1415.609443	191186.586775	36.264295
1417.357888	191517.399170	36.269312
1418.437546	191878.105734	36.274330
1419.947148	192213.417229	36.279348
1421.267707	192548.672929	36.284365
1422.677057	192895.265058	36.289383
1423.799862	193235.076554	36.294400
1425.135548	193596.423675	36.299418
1426.432847	193936.616386	36.304436
1428.128096	194284.895505	36.309453
1429.254186	194637.726642	36.314471
1430.681773	194976.227618	36.319488
1432.499430	195306.439281	36.324506
1433.803481	195641.333281	36.329524
1435.226628	195975.942723	36.334541
1436.291013	196322.800973	36.339559
1438.138006	196652.887676	36.344576
1439.415847	196993.975742	36.349594
1440.686647	197338.354946	36.354612
1442.054891	197685.677970	36.359629
1443.370856	198027.945748	36.364647
1444.880608	198378.080166	36.369664
1446.429040	198723.817156	36.374682
1447.536421	199078.224076	36.379700
1448.995855	199422.506553	36.384717
1450.261375	199790.742583	36.389735
1452.002236	200149.989182	36.394752
1453.426802	200512.806803	36.399770
1454.767887	200873.380119	36.404788
1456.222110	201240.069008	36.409805
1457.514546	201617.515157	36.414823
1459.074178	201988.951704	36.419840
1460.978582	202354.111789	36.424858
1462.033871	202728.060548	36.429876
1463.715539	203098.428773	36.434893
1464.540670	203475.212687	36.439911
1466.313940	203848.946926	36.444928
1467.925362	204234.771994	36.449946
1469.449640	204611.636575	36.454964
1470.979734	204985.302381	36.459981
1472.307092	205371.446830	36.464999
1474.163759	205747.703430	36.470016
1475.480987	206134.932655	36.475034
1476.945268	206515.892366	36.480052
1478.799260	206887.329894	36.485069
1480.366626	207275.805870	36.490087
1482.052183	207655.096529	36.495104
1483.673330	208031.618835	36.500122
1485.055745	208403.128643	36.505140
1486.865039	208779.090028	36.510157
1488.032692	209153.673514	36.515175
1489.759117	209543.276886	36.520192
1491.161442	209917.888537	36.525210
1492.807446	210302.467644	36.530228
1494.280368	210676.512292	36.535245
1495.917637	211055.204342	36.540263
1497.066648	211429.889921	36.545280
1498.533731	211814.099047	36.550298
1500.111834	212203.624810	36.555316
1501.942777	212584.602615	36.560333
1503.352764	212969.511932	36.565351
1504.316754	213350.560072	36.570368
1505.669529	213741.450431	36.575386
1507.245877	214127.048313	36.580404
1508.543202	214516.833674	36.585421
1510.157569	214925.463941	36.590439
1511.997571	215315.721722	36.595456
1513.242426	215710.320854	36.600474
1514.767890	216104.265711	36.605492
1516.568404	216497.988951	36.610509
1517.977128	216899.728070	36.615527
1519.325628	217280.220656	36.620544
1521.060141	217672.613432	36.625562
1522.643379	218078.569991	36.630580
1524.223149	218457.555756	36.635597
1525.625892	218861.767397	36.640615
1527.106017	219255.249674	36.645632
1528.578501	219653.255655	36.650650
1530.097907	220044.219956	36.655668
1531.329850	220420.120921	36.660685
1532.600656	220812.526052	36.665703
1534.420764	221193.971092	36.670720
1535.794944	221575.186355	36.675738
1537.050924	221962.289666	36.680756
1539.167889	222347.194727	36.685773
1540.384163	222738.320357	36.690791
1541.722473	223126.074445	36.695808
1543.190005	223515.764248	36.700826
1544.603797	223925.504497	36.705844
1546.038079	224341.287906	36.710861
1547.232473	224800.698379	36.715879
1548.897322	225203.137203	36.720896
1550.878620	225602.273878	36.725914
1552.233003	226021.911628	36.730932
1553.520986	226433.230521	36.735949
1555.254318	226844.934368	36.740967
1556.745292	227267.855689	36.745984
1558.102336	227684.882231	36.751002
1559.747119	228112.378322	36.756020
1561.669065	228532.895648	36.761037
1562.894606	228958.838056	36.766055
1564.059940	229384.690125	36.771072
1565.984735	229815.244152	36.776090
1567.189117	230248.712600	36.781108
1568.966857	230685.059527	36.786125
1570.834518	231127.260520	36.791143
1572.400106	231555.973984	36.796160
1574.418087	231991.446819	36.801178
1576.185523	232430.112031	36.806196
1578.032939	232860.535256	36.811213
1579.783859	233292.575875	36.816231
1581.153893	233709.515951	36.821248
1582.677346	234138.751442	36.826266
1584.426105	234565.105842	36.831284
1585.952920	234998.356406	36.836301
1587.411777	235424.887846	36.841319
1589.055881	235858.730805	36.846336
1590.800780	236307.113369	36.851354
1592.475073	236736.076299	36.856372
1594.404046	237171.170796	36.861389
1595.993456	237606.881227	36.866407
1597.529392	238029.976677	36.871424
1599.524576	238456.172412	36.876442
1601.078809	238884.499462	36.881460
1602.835382	239309.034451	36.886477
1604.313717	239750.838951	36.891495
1605.911203	240172.201255	36.896512
1607.804281	240591.534145	36.901530
1609.360703	241025.402767	36.906548
1611.082919	241437.957603	36.911565
1612.531172	241867.781266	36.916583
1613.895455	242291.827792	36.921600
1615.922973	242714.241313	36.926618
1617.415828	243151.172514	36.931636
1619.004416	243576.174799	36.936653
1620.547976	244003.954076	36.941671
1621.836443	244433.706752	36.946688
1623.903590	244864.042702	36.951706
1625.089101	245290.663707	36.956724
1626.874992	245718.075216	36.961741
1628.582101	246156.575948	36.966759
1630.265744	246591.245311	36.971776
1632.091645	247014.943081	36.976794
1633.317417	247455.735057	36.981812
1635.310127	247883.292940	36.986829
1637.041312	248307.007852	36.991847
1638.776582	248737.225710	36.996864
1640.600817	249136.717055	37.001882
1641.814854	249541.644215	37.006900
1643.396179	249937.543777	37.011917
1645.370423	250356.978237	37.016935
1646.920692	250749.708208	37.021952
1648.531479	251153.783679	37.026970
1650.034074	251567.987774	37.031988
1651.664522	251973.965820	37.037005
1653.390150	252393.036454	37.042023
1654.751325	252798.754669	37.047040
1656.677348	253219.291496	37.052058
1658.052361	253637.633289	37.057076
1659.829987	254051.107571	37.062093
1661.504265	254479.358407	37.067111
1663.141557	254898.876814	37.072128
1664.837712	255328.750192	37.077146
1666.312759	255758.990485	37.082164
1668.076282	256179.606214	37.087181
1669.320228	256607.446203	37.092199
1670.852269	257049.820182	37.097216
1672.652809	257486.383331	37.102234
1673.978418	257939.613345	37.107252
1675.860427	258368.897775	37.112269
1677.393340	258826.589971	37.117287
1678.967120	259274.571343	37.122304
1680.856540	259723.186429	37.127322
1682.428482	260192.633800	37.132340
1684.264620	260634.957534	37.137357
1685.859265	261100.463455	37.142375
1687.403297	261567.832044	37.147392
1689.323989	262025.993076	37.152410
1690.871766	262491.785704	37.157428
1692.447887	262964.889577	37.162445
1694.252010	263428.505545	37.167463
1695.803200	263895.490862	37.172480
1697.485663	264361.869937	37.177498
1699.172421	264844.048775	37.182516
1701.129975	265319.603107	37.187533
1702.725508	265798.798710	37.192551
1704.417604	266277.444491	37.197568
1706.246643	266750.910392	37.202586
1707.958286	267239.662484	37.207604
1709.626839	267715.872083	37.212621
1711.650960	268198.119166	37.217639
1713.026509	268677.856327	37.222656
1715.167644	269154.113268	37.227674
1716.523507	269641.498803	37.232692
1718.461365	270122.970298	37.237709
1720.115396	270594.834935	37.242727
1721.059899	271100.728883	37.247744
1723.479874	271576.530063	37.252762
1725.293830	272078.290614	37.257780
1726.979381	272574.076508	37.262797
1729.135190	273068.183517	37.267815
1730.910609	273549.371760	37.272832
1732.584910	274032.633465	37.277850
1734.317361	274524.369123	37.282868
1736.230656	275008.300812	37.287885
1737.658735	275492.514925	37.292903
1739.098455	275983.279955	37.297920
1741.220299	276463.389330	37.302938
1742.770263	276968.816598	37.307956
1744.460353	277450.849549	37.312973
1746.577771	277946.350185	37.317991
1748.398474	278434.151033	37.323008
1749.971488	278908.782586	37.328026
1751.714803	279409.447299	37.333044
1753.605601	279884.024032	37.338061
1755.390853	280336.365019	37.343079
1756.910822	280811.254703	37.348096
1759.004402	281266.412898	37.353114
1760.881985	281723.891768	37.358132
1762.619584	282192.975691	37.363149
1764.604763	282652.745901	37.368167
1766.091780	283123.189545	37.373184
1767.595732	283577.143578	37.378202
1769.339633	284059.379158	37.383220
1770.650066	284527.282395	37.388237
1772.527021	285003.422244	37.393255
1774.080211	285493.152864	37.398272
1776.015617	285963.641041	37.403290
1777.468221	286461.310228	37.408308
1779.084178	286952.829152	37.413325
1781.093962	287448.294664	37.418343
1782.699376	287945.120662	37.423360
1784.446535	288433.158291	37.428378
1786.272977	288940.383818	37.433396
1788.073374	289441.388651	37.438413
1789.925124	289952.644807	37.443431
1791.156243	290474.034518	37.448448
1793.262888	290974.449468	37.453466
1795.061896	291498.916187	37.458484
1796.903377	292021.570286	37.463501
1798.564646	292541.610342	37.468519
1800.274911	293064.637212	37.473536
1802.277536	293589.543849	37.478554
1803.515893	294129.788579	37.483572
1805.315979	294654.469846	37.488589
1807.251122	295199.369490	37.493607
1809.031407	295743.352286	37.498624
1810.693490	296288.164676	37.503642
1812.287210	296836.287456	37.508660
1814.140040	297382.408934	37.513677
1815.949105	297946.491541	37.518695
1817.744845	298505.138035	37.523712
1819.496276	299055.508979	37.528730
1821.367887	299626.861279	37.533748
1823.313299	300196.979010	37.538765
1825.365601	300761.183492	37.543783
1826.829570	301332.796368	37.548800
1828.761370	301890.842503	37.553818
1830.664067	302457.931588	37.558836
1832.567732	303022.147180	37.563853
1834.596501	303596.599037	37.568871
1836.217432	304171.571756	37.573888
1838.054769	304744.752674	37.578906
1840.011476	305323.243433	37.583924
1841.914306	305899.732948	37.588941
1844.073254	306463.808376	37.593959
1845.633133	307043.013446	37.598976
1847.536437	307619.415070	37.603994
1849.935133	308198.168873	37.609012
1851.572216	308758.480291	37.614029
1853.819650	309330.445079	37.619047
1855.134340	309903.245509	37.624064
1857.497780	310470.942001	37.629082
1859.780561	311044.513905	37.634100
1861.049999	311609.944909	37.639117
1863.266881	312173.793210	37.644135
1865.102554	312750.422781	37.649152
1867.117147	313313.508789	37.654170
1869.330380	313869.091964	37.659188
1871.177608	314425.442423	37.664205
1873.194493	314987.855051	37.669223
1874.855451	315547.071756	37.674240
1876.935836	316090.547338	37.679258
1878.837944	316638.238016	37.684276
1880.584134	317166.575597	37.689293
1882.358569	317701.531936	37.694311
1884.414555	318222.979745	37.699328
1886.246260	318764.317202	37.704346
1888.129005	319292.412758	37.709364
1889.680446	319823.199608	37.714381
1892.258257	320347.210964	37.719399
1893.640729	320889.798817	37.724416
1895.541827	321423.384282	37.729434
1897.169535	321969.121930	37.734452
1898.820018	322516.222285	37.739469
1900.740546	323066.117080	37.744487
1902.514917	323619.890537	37.749504
1904.217912	324181.262484	37.754522
1906.153232	324739.747354	37.759540
1907.797022	325311.477832	37.764557
1909.929429	325877.866709	37.769575
1911.621827	326458.591567	37.774592
1913.321097	327029.179574	37.779610
1915.419514	327605.637116	37.784628
1917.034109	328191.791077	37.789645
1919.455991	328777.298110	37.794663
1921.407099	329359.982782	37.799680
1923.167790	329952.213311	37.804698
1925.249416	330539.231106	37.809716
1926.571965	331129.871569	37.814733
1929.127309	331716.722739	37.819751
1931.040032	332322.586721	37.824768
1932.991573	332919.476358	37.829786
1935.263559	333520.038308	37.834804
1936.733987	334121.665258	37.839821
1938.947532	334710.749394	37.844839
1940.684140	335322.904621	37.849856
1942.642799	335921.892240	37.854874
1944.610322	336523.384651	37.859892
1946.612151	337135.043518	37.864909
1948.645756	337747.882973	37.869927
1950.330668	338367.270897	37.874944
1952.261286	338976.305163	37.879962
1954.227801	339603.221137	37.884980
1956.421085	340219.659617	37.889997
1958.634059	340828.904057	37.895015
1960.455779	341452.495658	37.900032
1962.200498	342080.356186	37.905050
1964.447288	342698.886947	37.910068
1966.288037	343314.786477	37.915085
1968.503536	343932.316752	37.920103
1970.424338	344565.268180	37.925120
1972.024589	345186.132459	37.930138
1974.491400	345808.774321	37.935156
1976.506384	346438.030354	37.940173
1978.546570	347050.929640	37.945191
1980.461913	347678.307207	37.950208
1982.169650	348307.689958	37.955226
1984.686066	348942.945033	37.960244
1986.349510	349572.165253	37.965261
1988.370148	350178.858828	37.970279
1990.535903	350825.615610	37.975296
1992.610470	351449.361513	37.980314
1994.820374	352073.583730	37.985332
1996.547597	352700.363530	37.990349
1998.736522	353323.556223	37.995367
2000.686286	353950.027379	38.000384
2002.566784	354568.863019	38.005402
2004.915958	355190.200434	38.010420
2006.516950	355818.807670	38.015437
2008.837367	356424.196783	38.020455
2010.540140	357042.365657	38.025472
2012.542939	357645.556565	38.030490
2014.686069	358241.839533	38.035508
2016.132994	358834.702038	38.040525
2018.243891	359438.077003	38.045543
2020.586719	360049.117534	38.050560
2022.223904	360648.290205	38.055578
2024.449903	361259.737482	38.060596
2026.131535	361877.176453	38.065613
2028.354606	362492.233090	38.070631
2030.347374	363113.863386	38.075648
2032.192386	363728.303388	38.080666
2034.474499	364351.819513	38.085684
2036.084293	364971.910379	38.090701
2038.231337	365597.990746	38.095719
2040.449595	366238.483030	38.100736
2042.061854	366871.378371	38.105754
2044.415347	367495.871236	38.110772
2045.993201	368147.724789	38.115789
2048.269813	368793.338456	38.120807
2050.038959	369448.308242	38.125824
2052.104355	370106.565570	38.130842
2054.441747	370762.102888	38.135860
2056.452390	371419.812862	38.140877
2058.572150	372061.311082	38.145895
2060.559133	372719.939637	38.150912
2062.839565	373389.286566	38.155930
2065.308926	374043.550101	38.160948
2066.915244	374712.171702	38.165965
2069.414307	375367.394786	38.170983
2071.719281	376032.883196	38.176000
2073.692639	376696.080462	38.181018
2076.348930	377358.974701	38.186036
2077.815461	378019.009463	38.191053
2080.292165	378680.005801	38.196071
2082.452731	379342.360048	38.201088
2084.460587	380012.384434	38.206106
2087.007298	380673.406181	38.211124
2088.772304	381341.694379	38.216141
2091.129221	382000.844681	38.221159
2093.077070	382670.774672	38.226176
2094.792236	383336.241574	38.231194
2097.645308	383993.697898	38.236212
2099.548567	384681.367356	38.241229
2101.432331	385333.632159	38.246247
2103.752265	386006.372818	38.251264
2105.939270	386675.521223	38.256282
2108.354029	387343.654562	38.261300
2110.338175	388019.298101	38.266317
2112.440255	388676.807287	38.271335
2114.923932	389346.787951	38.276352
2116.722130	390008.983627	38.281370
2119.202484	390677.339076	38.286388
2121.222802	391349.380784	38.291405
2123.168582	392014.424029	38.296423
2125.542507	392677.886586	38.301440
2127.539562	393355.210839	38.306458
2129.423026	394018.167328	38.311476
2131.516404	394688.120617	38.316493
2133.659437	395357.341018	38.321511
2135.713697	396041.691676	38.326528
2138.203223	396710.418818	38.331546
2140.439536	397391.818890	38.336564
2142.542757	398051.328926	38.341581
2144.657524	398723.113092	38.346599
2146.866574	399386.554085	38.351616
2148.707356	400067.373870	38.356634
2151.139233	400721.903293	38.361652
2152.791630	401375.152706	38.366669
2155.549080	402021.540481	38.371687
2157.455927	402674.008502	38.376704
2159.234696	403303.652931	38.381722
2161.552458	403944.976221	38.386740
2163.176217	404598.941141	38.391757
2165.327770	405252.170157	38.396775
2167.361667	405908.620824	38.401792
2169.217873	406569.113477	38.406810
2171.437248	407238.220028	38.411828
2173.575342	407918.673190	38.416845
2175.519255	408589.134739	38.421863
2177.763706	409268.953811	38.426880
2179.868199	409951.286698	38.431898
2182.183057	410637.544522	38.436916
2184.130493	411334.610890	38.441933
2186.421730	412025.675004	38.446951
2188.436878	412720.895320	38.451968
2190.364690	413431.283569	38.456986
2192.616694	414129.694905	38.462004
2194.845469	414846.478994	38.467021
2196.849440	415561.988750	38.472039
2199.350489	416280.435759	38.477056
2201.311338	417011.386528	38.482074
2203.791494	417722.680248	38.487092
2205.906620	418464.681411	38.492109
2207.998625	419187.723101	38.497127
2210.350656	419917.867375	38.502144
2212.419180	420653.734582	38.507162
2214.823180	421389.524779	38.512180
2217.012877	422139.685064	38.517197
2219.223640	422874.627628	38.522215
2221.242307	423623.479869	38.527232
2223.119378	424380.333055	38.532250
2225.840831	425131.200557	38.537268
2227.857863	425892.793943	38.542285
2230.348201	426648.007068	38.547303
2232.403458	427409.647622	38.552320
2234.742184	428178.001310	38.557338
2237.063253	428940.207483	38.562356
2239.439647	429707.290654	38.567373
2241.399171	430478.619454	38.572391
2243.713130	431240.955242	38.577408
2245.591119	432019.080809	38.582426
2247.965190	432793.403503	38.587444
2250.303203	433577.981384	38.592461
2252.512329	434356.125952	38.597479
2254.913987	435133.048383	38.602496
2257.245724	435924.177649	38.607514
2259.438132	436704.320366	38.612532
2261.658276	437499.715109	38.617549
2263.862298	438286.785276	38.622567
2266.277589	439069.238754	38.627584
2268.150575	439871.236161	38.632602
2270.853973	440661.632108	38.637620
2273.011880	441459.578520	38.642637
2275.096518	442250.677747	38.647655
2277.937317	443054.727772	38.652672
2279.733289	443849.864670	38.657690
2282.366537	444636.992855	38.662708
2284.417195	445436.734785	38.667725
2286.374745	446240.357760	38.672743
2289.232030	447034.595770	38.677760
2290.930784	447846.750365	38.682778
2293.675596	448643.021209	38.687796
2296.110327	449458.230188	38.692813
2298.180187	450251.213868	38.697831
2300.504027	451044.935042	38.702848
2302.541801	451834.425241	38.707866
2305.174867	452596.023402	38.712884
2307.552908	453375.638775	38.717901
2309.663017	454144.953164	38.722919
2312.001409	454920.825436	38.727936
2314.009499	455688.885491	38.732954
2316.826685	456460.878815	38.737972
2319.052168	457237.036011	38.742989
2320.904774	458019.898871	38.748007
2323.322818	458808.148848	38.753024
2325.575228	459598.821991	38.758042
2328.120834	460386.433030	38.763060
2330.443221	461177.689565	38.768077
2332.690988	461976.964251	38.773095
2334.857183	462773.035788	38.778112
2336.798618	463573.762479	38.783130
2339.504427	464378.525512	38.788148
2341.615038	465190.429416	38.793165
2344.016517	466020.142148	38.798183
2346.217150	466834.034834	38.803200
2348.737033	467664.314752	38.808218
2351.244431	468482.938693	38.813236
2353.266863	469312.067453	38.818253
2355.527899	470156.228652	38.823271
2358.166588	470969.722393	38.828288
2360.466655	471824.261896	38.833306
2362.847703	472668.089561	38.838324
2365.423697	473514.777336	38.843341
2367.562757	474357.760809	38.848359
2370.210586	475218.352683	38.853376
2372.394863	476079.486375	38.858394
2374.630513	476927.136143	38.863412
2377.449106	477782.277342	38.868429
2379.479233	478649.175422	38.873447
2382.376533	479501.445772	38.878464
2384.488380	480371.632322	38.883482
2386.945431	481224.096670	38.888500
2389.156087	482095.699104	38.893517
2391.475287	482971.381866	38.898535
2394.301614	483837.446111	38.903552
2396.687883	484721.009710	38.908570
2399.019753	485587.171601	38.913588
2401.108224	486461.509543	38.918605
2403.245724	487345.740707	38.923623
2406.040147	488221.793125	38.928640
2408.288275	489108.491648	38.933658
2410.914196	489994.022886	38.938676
2413.261267	490891.516390	38.943693
2415.599903	491776.297526	38.948711
2418.015916	492663.796079	38.953728
2420.540397	493570.658766	38.958746
2422.886668	494462.365033	38.963764
2425.409191	495352.280062	38.968781
2427.842624	496256.391196	38.973799
2430.177906	497139.230212	38.978816
2432.950310	498052.371397	38.983834
2435.286820	498948.383235	38.988852
2437.476268	499839.125241	38.993869
2439.760658	500742.716729	38.998887
2442.565971	501650.006334	39.003904
2444.989729	502555.695180	39.008922
2447.697036	503457.757179	39.013940
2450.192865	504365.250843	39.018957
2452.194367	505263.144199	39.023975
2454.743900	506168.057801	39.028992
2456.902240	507085.590706	39.034010
2459.306540	507988.661769	39.039028
2461.896373	508900.222156	39.044045
2464.350728	509785.538609	39.049063
2466.700868	510657.111762	39.054080
2468.898431	511543.381203	39.059098
2470.961739	512427.254288	39.064116
2474.155355	513315.679577	39.069133
2476.095588	514201.489621	39.074151
2478.715308	515097.267064	39.079168
2480.979403	515992.799895	39.084186
2483.408020	516893.242688	39.089204
2485.698216	517787.559278	39.094221
2487.720463	518708.672588	39.099239
2490.376519	519626.653804	39.104256
2492.886760	520551.657079	39.109274
2495.549049	521474.765841	39.114292
2497.824414	522410.676930	39.119309
2500.375483	523343.009422	39.124327
2502.687133	524274.266286	39.129344
2505.237307	525228.341105	39.134362
2507.131685	526180.197355	39.139380
2509.929914	527134.160308	39.144397
2512.229726	528096.905790	39.149415
2514.933676	529061.133368	39.154432
2517.455251	530038.367809	39.159450
2519.440296	531006.312597	39.164468
2522.056389	531999.309475	39.169485
2524.625364	532982.179562	39.174503
2527.155126	533979.535918	39.179520
2529.705396	534968.566439	39.184538
2531.899914	535980.838417	39.189556
2534.685009	536986.148409	39.194573
2537.083808	537998.798222	39.199591
2539.601343	539012.161792	39.204608
2542.201170	540025.439719	39.209626
2544.553480	541049.653213	39.214644
2547.362024	542069.743252	39.219661
2549.732912	543106.933725	39.224679
2552.800649	544141.266874	39.229696
2555.453024	545168.953365	39.234714
2557.496371	546205.666256	39.239732
2560.358150	547237.691292	39.244749
2562.795644	548284.642896	39.249767
2565.532297	549319.549743	39.254784
2568.147283	550362.040235	39.259802
2570.686167	551419.997221	39.264820
2573.341103	552461.566641	39.269837
2576.177863	553506.142362	39.274855
2578.800418	554566.504074	39.279872
2581.535655	555607.013711	39.284890
2584.126481	556650.029245	39.289908
2586.837437	557699.324892	39.294925
2589.573990	558758.682644	39.299943
2592.208555	559789.788765	39.304960
2595.140837	560855.025406	39.309978
2597.552434	561905.845603	39.314996
2600.747321	562945.955084	39.320013
2602.964613	564001.712085	39.325031
2605.647668	565042.241151	39.330048
2608.151114	566084.624590	39.335066
2610.667520	567124.461578	39.340084
2613.197354	568181.132008	39.345101
2615.796664	569224.149435	39.350119
2618.691243	570275.918213	39.355136
2621.180014	571329.122797	39.360154
2623.814495	572388.289012	39.365172
2626.840158	573432.095850	39.370189
2629.118085	574486.979582	39.375207
2631.593646	575523.427506	39.380224
2634.049704	576565.362122	39.385242
2636.482101	577593.969083	39.390260
2639.524121	578605.685552	39.395277
2642.079770	579627.080721	39.400295
2644.863123	580634.259898	39.405312
2647.450506	581646.955971	39.410330
2650.054434	582664.480315	39.415348
2652.999268	583666.920827	39.420365
2655.259463	584704.389618	39.425383
2658.233070	585709.765838	39.430400
2660.860884	586729.202638	39.435418
2663.201008	587759.879473	39.440436
2665.932095	588788.949985	39.445453
2668.204165	589831.489846	39.450471
2670.744940	590875.848930	39.455488
2673.352112	591917.249256	39.460506
2675.680445	592978.646426	39.465524
2678.355763	594040.291986	39.470541
2681.041255	595105.898114	39.475559
2683.842497	596183.410582	39.480576
2686.319598	597260.076008	39.485594
2688.956712	598347.383500	39.490612
2691.425171	599430.661056	39.495629
2694.289312	600527.992918	39.500647
2696.869819	601615.103485	39.505664
2699.787792	602725.886042	39.510682
2701.943046	603838.138595	39.515700
2704.982690	604949.386327	39.520717
2707.580063	606067.054968	39.525735
2709.651146	607193.107829	39.530752
2712.384093	608326.145134	39.535770
2715.254697	609465.500299	39.540788
2718.367524	610603.349255	39.545805
2720.707133	611763.470673	39.550823
2723.344779	612902.514683	39.555840
2726.154299	614068.670958	39.560858
2728.457213	615234.538072	39.565876
2731.279619	616396.596280	39.570893
2733.904036	617575.013598	39.575911
2736.661070	618751.032813	39.580928
2739.273880	619941.545356	39.585946
2741.609289	621130.574062	39.590964
2744.545491	622326.769812	39.595981
2747.046114	623517.608270	39.600999
2749.968574	624718.288434	39.606016
2752.694167	625930.357345	39.611034
2755.045877	627148.944440	39.616052
2758.157162	628355.379526	39.621069
2761.139758	629594.110982	39.626087
2764.074566	630810.983299	39.631104
2766.684081	632030.614903	39.636122
2769.439807	633259.566500	39.641140
2772.400553	634472.965232	39.646157
2775.327716	635713.680342	39.651175
2778.076512	636945.493307	39.656192
2781.350999	638162.601978	39.661210
2783.709347	639390.844824	39.666228
2786.729201	640610.101469	39.671245
2789.321815	641847.191562	39.676263
2792.288052	643080.429300	39.681280
2795.074147	644313.098571	39.686298
2797.545987	645547.265624	39.691316
2800.683810	646786.357546	39.696333
2803.245239	648010.835264	39.701351
2805.989508	649256.667182	39.706368
2809.308019	650495.969485	39.711386
2811.721055	651738.107651	39.716404
2814.783827	652965.433780	39.721421
2817.525170	654199.237295	39.726439
2819.691713	655403.889250	39.731456
2823.055798	656598.881914	39.736474
2825.915164	657811.193519	39.741492
2828.639250	659000.321031	39.746509
2831.102750	660203.287872	39.751527
2833.555046	661407.252609	39.756544
2836.741861	662625.780488	39.761562
2838.859777	663850.651785	39.766580
2841.638296	665076.203693	39.771597
2844.788600	666300.890697	39.776615
2847.174606	667546.194213	39.781632
2849.927554	668782.071242	39.786650
2852.466524	670039.161035	39.791668
2855.438898	671295.514932	39.796685
2857.955957	672560.677501	39.801703
2860.349273	673834.440789	39.806720
2863.640897	675122.746854	39.811738
2866.159659	676409.461558	39.816756
2869.565629	677692.223867	39.821773
2872.741725	678992.536958	39.826791
2874.884147	680292.986455	39.831808
2877.991110	681595.378379	39.836826
2880.892686	682906.907734	39.841844
2883.909128	684217.832655	39.846861
2886.897724	685540.391831	39.851879
2889.772918	686862.528779	39.856896
2892.727243	688178.651320	39.861914
2895.303886	689521.149096	39.866932
2898.146904	690854.866453	39.871949
2901.678604	692194.226017	39.876967
2904.545963	693540.638287	39.881984
2907.416574	694875.089768	39.887002
2909.966613	696231.464109	39.892020
2912.783577	697577.122679	39.897037
2915.964397	698946.215871	39.902055
2918.792611	700302.809442	39.907072
2922.159085	701658.211528	39.912090
2924.550869	703039.135897	39.917108
2927.906837	704397.879141	39.922125
2931.101173	705766.592020	39.927143
2933.568201	707157.349865	39.932160
2936.513527	708538.145922	39.937178
2939.243703	709915.635062	39.942196
2942.601365	711301.017277	39.947213
2945.468669	712694.521672	39.952231
2948.442062	714078.226883	39.957248
2951.623593	715461.671071	39.962266
2954.099389	716861.925976	39.967284
2957.253891	718249.863376	39.972301
2960.483220	719652.990223	39.977319
2962.929638	721051.460050	39.982336
2966.109957	722454.715678	39.987354
2968.831810	723869.772680	39.992372
2972.160751	725265.357860	39.997389
2975.158596	726677.365807	40.002407
2977.859496	728090.562786	40.007424
2980.986145	729499.591442	40.012442
2984.205588	730919.178109	40.017460
2987.136676	732331.797838	40.022477
2990.363236	733731.925660	40.027495
2993.143488	735153.260202	40.032512
2996.162862	736565.961760	40.037530
2999.290055	737990.338960	40.042548
3002.496174	739393.034027	40.047565
3005.370363	740813.148214	40.052583
3008.189752	742229.021412	40.057600
3011.073045	743641.572441	40.062618
3014.260379	745050.318839	40.067636
3017.282856	746428.619393	40.072653
3020.718789	747803.207643	40.077671
3023.409311	749162.152619	40.082688
3026.080937	750529.682590	40.087706
3029.384964	751901.940795	40.092724
3032.415205	753270.207366	40.097741
3035.625415	754639.481177	40.102759
3038.494024	756016.838525	40.107776
3041.464365	757394.176942	40.112794
3044.509823	758773.813294	40.117812
3047.411926	760157.946754	40.122829
3050.505663	761548.339246	40.127847
3053.531031	762946.751025	40.132864
3056.347487	764338.002357	40.137882
3059.176239	765747.286128	40.142900
3062.181646	767161.338908	40.147917
3065.676751	768566.833550	40.152935
3068.589060	769997.566525	40.157952
3071.529852	771410.279973	40.162970
3074.196776	772855.388195	40.167988
3077.429475	774294.519770	40.173005
3080.598356	775743.053377	40.178023
3083.650971	777197.897947	40.183040
3086.479590	778642.376633	40.188058
3089.391306	780113.007107	40.193076
3092.390131	781570.566560	40.198093
3095.689928	783056.039071	40.203111
3098.588179	784538.327805	40.208128
3101.673324	786024.250988	40.213146
3105.069340	787518.736565	40.218164
3107.663017	789014.608989	40.223181
3110.871243	790521.973163	40.228199
3114.045093	792036.370897	40.233216
3117.442826	793535.465578	40.238234
3120.226687	795055.547484	40.243252
3123.414100	796561.816465	40.248269
3126.868413	798079.954544	40.253287
3129.857928	799613.254656	40.258304
3133.130375	801140.639470	40.263322
3136.493820	802666.839747	40.268340
3139.735030	804194.042269	40.273357
3143.085351	805734.236287	40.278375
3146.032652	807283.047380	40.283392
3149.251110	808813.914820	40.288410
3152.042904	810356.675146	40.293428
3155.346286	811896.996465	40.298445
3158.905023	813438.486975	40.303463
3162.105052	814987.740537	40.308480
3165.505528	816523.811720	40.313498
3168.656203	818063.573222	40.318516
3171.755498	819608.794109	40.323533
3175.174324	821155.212470	40.328551
3178.105462	822708.324550	40.333568
3181.439062	824242.035033	40.338586
3184.664131	825795.930383	40.343604
3187.490402	827340.164408	40.348621
3190.892159	828896.559294	40.353639
3194.237223	830447.280905	40.358656
3197.363754	831999.128885	40.363674
3200.389938	833553.201645	40.368692
3203.364914	835121.561537	40.373709
3206.768004	836680.220343	40.378727
3209.831057	838251.352950	40.383744
3213.240279	839806.863679	40.388762
3216.005184	841372.313464	40.393780
3219.287557	842944.633438	40.398797
3222.299870	844513.787148	40.403815
3225.584873	846069.383194	40.408832
3228.627492	847611.417982	40.413850
3231.655491	849136.365293	40.418868
3234.669910	850669.974752	40.423885
3238.082257	852207.218636	40.428903
3240.842944	853738.363898	40.433920
3243.976320	855286.343922	40.438938
3246.682352	856841.961694	40.443956
3249.641505	858405.582996	40.448973
3253.321520	859971.013480	40.453991
3256.298742	861546.241293	40.459008
3259.625579	863128.757759	40.464026
3262.779793	864714.281081	40.469044
3265.700461	866311.149060	40.474061
3269.254508	867916.883904	40.479079
3271.923193	869527.757321	40.484096
3275.234819	871158.419122	40.489114
3278.291954	872779.096314	40.494132
3281.530047	874408.202498	40.499149
3284.719351	876056.696371	40.504167
3287.760245	877708.235386	40.509184
3291.056146	879382.951991	40.514202
3294.359764	881051.004276	40.519220
3297.532625	882725.944485	40.524237
3300.915656	884399.595851	40.529255
3304.672876	886093.945093	40.534272
3307.814775	887783.362865	40.539290
3310.449142	889486.747546	40.544308
3314.028723	891192.269317	40.549325
3317.705168	892908.743661	40.554343
3320.574161	894626.473926	40.559360
3324.096264	896352.830636	40.564378
3327.175214	898091.260498	40.569396
3330.328584	899823.845572	40.574413
3333.961310	901580.662065	40.579431
3337.285388	903325.427970	40.584448
3340.169120	905079.249104	40.589466
3343.481532	906843.607158	40.594484
3346.716677	908613.187742	40.599501
3350.000026	910382.483081	40.604519
3353.395521	912169.549247	40.609536
3356.711409	913952.684823	40.614554
3360.109041	915744.639007	40.619572
3363.127399	917544.516702	40.624589
3366.624787	919338.344926	40.629607
3369.877363	921145.724616	40.634624
3373.217639	922964.954522	40.639642
3376.192684	924786.410453	40.644660
3379.674496	926607.068544	40.649677
3383.036817	928428.850918	40.654695
3386.848505	930262.292719	40.659712
3389.558919	932101.315101	40.664730
3392.949986	933940.255986	40.669748
3396.301297	935784.877111	40.674765
3400.287047	937634.389331	40.679783
3402.969683	939490.633983	40.684800
3406.909796	941324.312801	40.689818
3409.975161	943167.999306	40.694836
3413.253557	945049.296750	40.699853
3416.454577	946908.246477	40.704871
3419.871764	948770.115470	40.709888
3423.546449	950646.245220	40.714906
3427.175917	952511.582808	40.719924
3429.879127	954436.107048	40.724941
3433.610608	956358.949513	40.729959
3437.318764	958289.954087	40.734976
3440.816064	960215.166673	40.739994
3444.577845	962131.094443	40.745012
3447.769768	964042.580943	40.750016
3451.302763	965882.391270	40.755021
3454.683715	967677.699653	40.760026
3458.123419	969412.566562	40.765031
3461.542184	971052.242717	40.770036
3464.206042	972630.466388	40.775040
3467.620237	974124.460413	40.780045
3470.309308	975549.387251	40.785050
3473.246045	976895.465691	40.790055
3476.231455	978164.639779	40.795060
3478.911414	979365.515088	40.800064
3481.471461	980479.943192	40.805069
3483.742645	981520.497895	40.810074
3485.646853	982485.280291	40.815079
3488.327591	983391.901564	40.820084
3490.443526	984231.048018	40.825088
3492.498834	984996.129766	40.830093
3494.620731	985719.834644	40.835098
3496.429043	986360.982604	40.840103
3498.623578	986954.791410	40.845108
3499.888985	987486.084612	40.850112
3501.521991	987955.446202	40.855117
3502.991114	988384.624817	40.860122
3504.355143	988756.752933	40.865127
3505.803945	989082.144560	40.870132
3506.568222	989371.657966	40.875136
3507.852642	989600.437190	40.880141
3508.989757	989820.750822	40.885146
3510.347871	989999.007678	40.890151
3511.257630	990131.520531	40.895156
3512.230211	990231.269582	40.900160
3513.337962	990289.277354	40.905165
3514.172557	990332.124256	40.910170
3514.837741	990332.014705	40.915175
3515.833204	990312.161800	40.920180
3516.414932	990264.012996	40.925184
3516.930520	990184.391194	40.930189
3517.759602	990100.330314	40.935194
3517.942692	989971.925731	40.940199
3518.554040	989842.960303	40.945204
3519.068521	989701.627884	40.950208
3519.652450	989523.041861	40.955213
3520.210751	989336.558022	40.960218
3520.273227	989135.038771	40.965223
3520.966082	988917.224530	40.970228
3521.253357	988695.666353	40.975232
3522.116262	988436.856453	40.980237
3522.229612	988178.840820	40.985242
3522.709136	987908.466738	40.990247
3522.972319	987624.073130	40.995252
3522.951316	987335.323675	41.000256
3523.214098	987035.199769	41.005261
3523.464007	986714.385447	41.010266
3524.002507	986386.677884	41.015271
3524.346262	986057.325316	41.020276
3524.308417	985720.895504	41.025280
3524.694637	985368.376971	41.030285
3524.682891	985016.585113	41.035290
3524.396106	984658.670117	41.040295
3524.691550	984289.123061	41.045300
3524.569310	983924.694997	41.050304
3524.857203	983558.419512	41.055309
3525.281747	983182.143573	41.060314
3525.448467	982799.150963	41.065319
3525.698481	982400.404408	41.070324
3525.335101	982010.516153	41.075328
3525.302737	981617.422894	41.080333
3525.466854	981211.578805	41.085338
3525.473110	980808.660849	41.090343
3525.848191	980402.431567	41.095348
3525.468676	980008.894128	41.100352
3525.510861	979598.268370	41.105357
3525.841490	979178.678435	41.110362
3525.706810	978771.342824	41.115367
3526.049348	978345.145961	41.120372
3525.833948	977935.615207	41.125376
3525.911528	977509.595043	41.130381
3526.022165	977089.692565	41.135386
3525.553103	976658.325699	41.140391
3525.921258	976230.892223	41.145396
3525.519026	975812.641541	41.150400
3526.009056	975379.945329	41.155405
3526.023502	974943.385427	41.160410
3526.153998	974511.366909	41.165415
3526.007192	974073.398841	41.170420
3525.528371	973656.176095	41.175424
3525.756368	973216.614403	41.180429
3525.952001	972783.281599	41.185434
3525.807707	972348.700911	41.190439
3525.969709	971912.081095	41.195444
3525.732924	971487.913333	41.200448
3525.637919	971040.414506	41.205453
3525.619616	970608.712893	41.210458
3526.024910	970167.812229	41.215463
3525.874687	969716.404387	41.220468
3525.449517	969285.550598	41.225472
3525.600284	968846.351237	41.230477
3525.671388	968399.108114	41.235482
3525.447566	967969.687855	41.240487
3525.721326	967517.645764	41.245492
3525.377626	967086.221973	41.250496
3525.442823	966635.514947	41.255501
3525.306031	966203.305617	41.260506
3525.236937	965764.591896	41.265511
3525.506739	965317.565473	41.270516
3525.200251	964885.970294	41.275520
3525.228058	964436.369693	41.280525
3524.953083	964004.409398	41.285530
3524.830249	963568.376576	41.290535
3525.059488	963122.361294	41.295540
3524.953738	962686.258798	41.300544
3525.145002	962249.094822	41.305549
3524.925784	961814.022370	41.310554
3524.963422	961380.246217	41.315559
3524.875591	960924.512339	41.320564
3524.551472	960493.178266	41.325568
3524.644371	960068.798231	41.330573
3524.486734	959625.711346	41.335578
3524.520192	959197.945163	41.340583
3524.364671	958761.455579	41.345588
3524.406691	958335.094089	41.350592
3524.216297	957909.621574	41.355597
3524.682101	957475.382855	41.360602
3524.441240	957026.718213	41.365607
3524.238253	956593.209550	41.370612
3523.925442	956173.511886	41.375616
3523.872546	955733.148230	41.380621
3523.781148	955311.586324	41.385626
3523.839103	954892.126675	41.390631
3523.939722	954461.938608	41.395636
3523.840534	954044.012569	41.400640
3523.767258	953605.451795	41.405645
3523.796847	953189.110344	41.410650
3523.662983	952761.973649	41.415655
3523.647268	952331.610582	41.420660
3523.083155	951933.601002	41.425664
3523.279598	951515.063646	41.430669
3523.157804	951115.387019	41.435674
3523.203145	950709.816558	41.440679
3523.614809	950292.578281	41.445684
3523.131831	949892.865437	41.450688
3523.217060	949482.407426	41.455693
3522.833902	949072.280714	41.460698
3522.354560	948669.026936	41.465703
3522.800627	948266.641666	41.470708
3522.428282	947860.722740	41.475712
3522.401180	947454.810538	41.480717
3522.231694	947067.938725	41.485722
3522.547011	946681.340842	41.490727
3522.380468	946273.347970	41.495732
3522.024287	945885.747829	41.500736
3522.296542	945477.811129	41.505741
3522.577249	945094.642709	41.510746
3522.396612	944694.283709	41.515751
3522.454312	944289.927619	41.520756
3522.157177	943898.145852	41.525760
3522.545968	943495.301364	41.530765
3522.092689	943095.054987	41.535770
3521.724839	942701.948935	41.540775
3521.845415	942311.127886	41.545780
3521.695318	941927.891675	41.550784
3521.660846	941529.563437	41.555789
3521.730269	941146.329205	41.560794
3521.512535	940754.488403	41.565799
3521.640548	940366.778414	41.570804
3521.272226	939985.831153	41.575808
3521.577645	939601.485735	41.580813
3521.417341	939215.750691	41.585818
3521.270732	938830.176622	41.590823
3521.399966	938439.638604	41.595828
3521.069501	938062.763519	41.600832
3521.323463	937673.394280	41.605837
3520.983775	937295.794175	41.610842
3520.676738	936910.872227	41.615847
3520.760472	936539.286128	41.620852
3520.681476	936177.388888	41.625856
3520.739290	935794.435217	41.630861
3520.712937	935421.061323	41.635866
3520.487140	935043.088399	41.640871
3520.533710	934676.845519	41.645876
3520.182477	934313.809323	41.650880
3520.457390	933939.417019	41.655885
3520.154294	933574.018748	41.660890
3519.941757	933212.227420	41.665895
3519.815312	932838.590933	41.670900
3519.734405	932489.398423	41.675904
3520.050662	932122.933751	41.680909
3520.095305	931764.840864	41.685914
3519.732968	931394.789385	41.690919
3519.824605	931034.431094	41.695924
3519.512373	930690.727057	41.700928
3519.488198	930327.459071	41.705933
3519.637757	929976.046216	41.710938
3519.400181	929607.770215	41.715943
3519.565007	929255.442794	41.720948
3519.241220	928901.155349	41.725952
3519.049415	928545.861940	41.730957
3519.069448	928199.252230	41.735962
3519.160622	927846.459424	41.740967
3519.290603	927498.248819	41.745972
3518.981752	927156.621783	41.750976
3518.972441	926804.160982	41.755981
3518.806089	926453.432617	41.760986
3518.455652	926112.418366	41.765991
3518.826233	925766.554052	41.770996
3518.553647	925438.267030	41.776000
3518.693756	925084.514902	41.781005
3518.643916	924740.864534	41.786010
3518.602019	924399.882694	41.791015
3519.023148	924049.957697	41.796020
3518.184489	923710.986258	41.801024
3518.200403	923371.275699	41.806029
3518.052107	923040.898443	41.811034
3517.868114	922713.968822	41.816039
3518.199503	922364.429810	41.821044
3517.971709	922041.794441	41.826048
3518.021036	921712.553502	41.831053
3517.939300	921387.835062	41.836058
3517.933923	921053.272407	41.841063
3517.828017	920719.763835	41.846068
3517.349833	920405.056764	41.851072
3517.751589	920075.658018	41.856077
3517.599108	919742.481732	41.861082
3517.140250	919422.999566	41.866087
3517.310879	919102.721229	41.871092
3517.107176	918785.084070	41.876096
3517.326260	918466.203744	41.881101
3517.157904	918141.401101	41.886106
3517.014655	917837.365875	41.891111
3517.070086	917511.622440	41.896116
3516.714310	917200.944701	41.901120
3517.000057	916886.581503	41.906125
3517.068086	916568.866354	41.911130
3516.877591	916258.011323	41.916135
3517.163006	915943.497518	41.921140
3516.663158	915630.924540	41.926144
3516.596444	915317.106715	41.931149
3516.166321	915015.850291	41.936154
3516.495102	914715.993178	41.941159
3516.813014	914398.303179	41.946164
3516.148022	914096.167959	41.951168
3516.118704	913794.296633	41.956173
3516.174797	913487.481728	41.961178
3515.912052	913187.445731	41.966183
3516.052917	912886.459753	41.971188
3515.775188	912594.101104	41.976192
3515.724427	912284.538845	41.981197
3515.845928	911997.863819	41.986202
3515.557513	911718.757631	41.991207
3515.706802	911404.680231	41.996212
3515.442179	911126.118273	42.001216
3515.683913	910835.315250	42.006221
3515.616726	910539.535889	42.011226
3515.296852	910255.830762	42.016231
3515.332711	909971.184903	42.021236
3515.441428	909685.259198	42.026240
3515.426003	909392.398160	42.031245
3515.655074	909113.267622	42.036250
3515.052750	908827.607515	42.041255
3515.276212	908546.521057	42.046260
3515.165768	908260.750650	42.051264
3515.015162	907980.950611	42.056269
3515.095184	907693.094575	42.061274
3515.031886	907415.276681	42.066279
3514.938940	907132.724106	42.071284
3514.665656	906856.841695	42.076288
3515.153546	906581.495333	42.081293
3515.030781	906304.596189	42.086298
3514.632126	906015.478126	42.091303
3514.799131	905745.448622	42.096308
3514.524722	905462.455181	42.101312
3514.660837	905191.535672	42.106317
3514.546840	904925.854140	42.111322
3514.462503	904643.656124	42.116327
3514.577517	904371.059984	42.121332
3514.157379	904101.433542	42.126336
3514.385910	903832.266200	42.131341
3514.063495	903567.133324	42.136346
3513.891793	903308.525602	42.141351
3514.430055	903034.925980	42.146356
3514.102755	902774.581984	42.151360
3513.831631	902509.487048	42.156365
3514.032460	902248.645502	42.161370
3513.799984	901989.021584	42.166375
3513.969392	901721.886198	42.171380
3513.840500	901473.226382	42.176384
3513.766389	901203.306783	42.181389
3514.013858	900942.686486	42.186394
3513.812399	900686.376420	42.191399
3513.711585	900421.637556	42.196404
3513.661741	900168.851563	42.201408
3513.570397	899902.831421	42.206413
3513.718003	899650.762171	42.211418
3513.643709	899388.964079	42.216423
3513.952702	899134.430761	42.221428
3513.400227	898892.197503	42.226432
3513.317015	898626.598709	42.231437
3513.302082	898377.107210	42.236442
3513.170330	898140.954334	42.241447
3513.267013	897881.762869	42.246452
3513.082944	897627.532674	42.251456
3513.004257	897391.339742	42.256461
3513.047907	897142.267148	42.261466
3512.720897	896903.389576	42.266471
3513.227075	896656.828120	42.271476
3512.922969	896412.321974	42.276480
3512.876001	896165.637043	42.281485
3513.031592	895920.744074	42.286490
3512.876947	895689.227820	42.291495
3513.025006	895437.453892	42.296500
3512.535559	895201.334041	42.301504
3512.284420	894955.306694	42.306509
3512.574164	894731.893567	42.311514
3512.566615	894491.798648	42.316519
3512.255638	894250.196982	42.321524
3512.324877	894025.729178	42.326528
3512.522901	893790.694181	42.331533
3512.246156	893548.187062	42.336538
3511.934223	893324.044451	42.341543
3511.922720	893092.882371	42.346548
3511.758681	892867.440578	42.351552
3512.210192	892631.832647	42.356557
3511.843758	892410.563862	42.361562
3511.610312	892190.328277	42.366567
3512.056087	891962.429550	42.371572
3511.929197	891738.194215	42.376576
3511.701645	891514.256808	42.381581
3511.735523	891291.428127	42.386586
3511.513420	891082.753628	42.391591
3511.802180	890848.743292	42.396596
3511.792094	890636.342219	42.401600
3511.701814	890410.211110	42.406605
3511.621188	890185.133549	42.411610
3511.271448	889961.445803	42.416615
3511.571007	889746.348912	42.421620
3511.474907	889550.270754	42.426624
3511.531825	889320.299510	42.431629
3511.260872	889096.468361	42.436634
3511.142244	888898.920449	42.441639
3511.102706	888680.840218	42.446644
3510.883402	888473.812081	42.451648
3511.388629	888250.884538	42.456653
3511.526919	888044.943251	42.461658
3511.247202	887838.966709	42.466663
3511.504121	887618.571694	42.471668
3511.118205	887412.790980	42.476672
3511.049518	887200.659825	42.481677
3510.958021	886990.750706	42.486682
3510.759194	886796.144309	42.491687
3511.395514	886576.130953	42.496692
3510.816995	886370.151237	42.501696
3510.904119	886153.212959	42.506701
3510.885205	885951.578919	42.511706
3510.843952	885743.939537	42.516711
3511.038233	885540.707162	42.521716
3510.700396	885335.909506	42.526720
3510.695987	885133.857360	42.531725
3510.521920	884934.730727	42.536730
3510.502880	884746.028628	42.541735
3510.619103	884531.058117	42.546740
3510.785962	884338.342240	42.551744
3510.275077	884129.850973	42.556749
3510.531564	883941.464666	42.561754
3510.255988	883746.865335	42.566759
3510.709599	883539.743425	42.571764
3510.278105	883345.543726	42.576768
3510.094458	883148.197516	42.581773
3510.334581	882957.167093	42.586778
3509.999570	882771.939674	42.591783
3510.619009	882576.185175	42.596788
3510.139708	882392.034905	42.601792
3510.053563	882192.315551	42.606797
3510.219827	881996.906875	42.611802
3509.935322	881812.899957	42.616807
3510.435443	881620.232953	42.621812
3510.071399	881429.348910	42.626816
3510.024216	881238.212657	42.631821
3510.086017	881045.598927	42.636826
3510.082277	880864.422409	42.641831
3509.932513	880669.312062	42.646836
3509.793192	880492.021983	42.651840
3509.773603	880303.176076	42.656845
3510.079892	880109.231580	42.661850
3509.941443	879934.540781	42.666855
3509.855487	879740.745618	42.671860
3509.626219	879558.306059	42.676864
3509.556363	879371.473500	42.681869
3509.709250	879192.739186	42.686874
3509.563384	879021.123683	42.691879
3509.530862	878828.355670	42.696884
3509.540562	878644.782197	42.701888
3509.435443	878462.385034	42.706893
3509.537479	878285.570039	42.711898
3509.075538	878120.862354	42.716903
3509.184232	877945.393095	42.721908
3509.269971	877776.611159	42.726912
3509.014261	877592.757751	42.731917
3508.974119	877430.481722	42.736922
3508.817482	877261.143274	42.741927
3508.517769	877097.252727	42.746932
3508.279740	876932.668788	42.751936
3509.010790	876765.399749	42.756941
3509.122775	876597.355346	42.761946
3508.482840	876443.974155	42.766951
3508.683104	876273.481966	42.771956
3508.526110	876126.897358	42.776960
3508.367125	875953.934020	42.781965
3508.591788	875781.096349	42.786970
3508.103321	875620.008029	42.791975
3508.899602	875463.649453	42.796980
3508.358527	875314.004701	42.801985
3508.573375	875144.932237	42.806989
3508.685509	874994.298933	42.811994
3508.141147	874832.325499	42.816999
3508.205553	874669.083450	42.822004
3508.390741	874521.432759	42.827009
3507.872203	874360.509071	42.832013
3508.267750	874202.146330	42.837018
3507.923835	874060.488167	42.842023
3508.012723	873896.735810	42.847028
3508.006087	873759.476991	42.852033
3508.011347	873608.438047	42.857037
3508.338240	873456.760209	42.862042
3508.049790	873318.276495	42.867047
3508.034010	873156.655224	42.872052
3508.050180	873010.644026	42.877057
3508.193271	872853.936203	42.882061
3508.486891	872699.430954	42.887066
3507.951251	872558.544704	42.892071
3508.319697	872398.780006	42.897076
3507.947354	872257.083492	42.902081
3507.823961	872091.278735	42.907085
3508.060741	871953.647004	42.912090
3507.674291	871809.807412	42.917095
3507.632199	871655.718527	42.922100
3507.570857	871515.117575	42.927105
3507.567998	871376.056366	42.932109
3507.722590	871233.278232	42.937114
3507.456865	871085.519426	42.942119
3507.711024	870949.317366	42.947124
3507.681322	870808.791597	42.952129
3507.710546	870654.762149	42.957133
3507.454716	870515.528450	42.962138
3507.132291	870389.987886	42.967143
3507.668734	870245.473198	42.972148
3507.238285	870114.412110	42.977153
3507.313250	869977.635033	42.982157
3507.241305	869829.910287	42.987162
3507.252733	869702.844249	42.992167
3507.327646	869563.533872	42.997172
3507.116936	869431.062573	43.002177
3507.065264	869296.717669	43.007181
3507.298818	869174.748914	43.012186
3506.853913	869045.996688	43.017191
3507.382463	868912.130047	43.022196
3507.323684	868781.366843	43.027201
3507.211346	868649.444557	43.032205
3507.272836	868502.053412	43.037210
3507.211465	868372.932257	43.042215
3507.129618	868230.412662	43.047220
3506.824132	868105.015552	43.052225
3507.102737	867971.945887	43.057229
3506.933354	867838.267379	43.062234
3506.562177	867722.583182	43.067239
3506.743623	867583.209228	43.072244
3506.850540	867465.304991	43.077249
3506.972731	867341.569393	43.082253
3507.032424	867214.539772	43.087258
3506.612072	867079.623288	43.092263
3506.976083	866956.616830	43.097268
3506.356180	866843.481676	43.102273
3506.463277	866714.199986	43.107277
3506.551384	866589.191977	43.112282
3506.354827	866472.192363	43.117287
3506.635603	866352.489456	43.122292
3506.540438	866223.619057	43.127297
3506.605070	866101.518603	43.132301
3506.659733	865985.050907	43.137306
3506.550924	865870.647680	43.142311
3506.618628	865738.340425	43.147316
3506.453571	865619.667771	43.152321
3506.715053	865502.088167	43.157325
3506.362273	865393.155837	43.162330
3506.421945	865272.690802	43.167335
3506.368218	865148.647711	43.172340
3506.336581	865030.330058	43.177345
3506.461977	864914.801509	43.182349
3506.312301	864803.202067	43.187354
3506.307695	864679.529845	43.192359
3506.204611	864571.804523	43.197364
3506.032194	864471.472502	43.202369
3505.759033	864352.306968	43.207373
3506.442294	864227.346276	43.212378
3505.846060	864117.556611	43.217383
3505.869431	864010.286253	43.222388
3505.683765	863906.837842	43.227393
3505.880963	863802.061424	43.232397
3505.933250	863683.314917	43.237402
3505.860845	863588.879012	43.242407
3505.795041	863475.297857	43.247412
3505.768363	863376.575574	43.252417
3505.613136	863267.183677	43.257421
3506.114071	863167.302136	43.262426
3505.544213	863068.178444	43.267431
3505.926620	862948.974444	43.272436
3505.621385	862854.565457	43.277441
3505.864487	862748.499908	43.282445
3505.993977	862647.018897	43.287450
3505.499862	862547.777028	43.292455
3505.597980	862441.244068	43.297460
3505.636620	862343.174515	43.302465
3505.585711	862242.299596	43.307469
3505.814605	862130.977290	43.312474
3505.663076	862040.806791	43.317479
3505.493292	861923.423135	43.322484
3505.546583	861830.591476	43.327489
3505.462849	861726.214284	43.332493
3505.459156	861632.514197	43.337498
3505.172050	861542.650245	43.342503
3505.600349	861439.155783	43.347508
3505.445144	861349.656061	43.352513
3505.476584	861249.431532	43.357517
3505.598791	861145.593686	43.362522
3505.423088	861044.038985	43.367527
3505.658219	860947.761541	43.372532
3505.520721	860850.377413	43.377537
3505.217895	860754.282758	43.382541
3505.352740	860650.239953	43.387546
3505.363077	860557.493168	43.392551
3505.409876	860461.433505	43.397556
3505.214757	860364.148316	43.402561
3505.032518	860272.498353	43.407565
3505.292844	860177.565705	43.412570
3505.029979	860090.495811	43.417575
3505.242188	859991.387506	43.422580
3505.105350	859911.294620	43.427585
3505.044175	859808.339258	43.432589
3505.148769	859714.202900	43.437594
3505.052534	859634.974778	43.442599
3505.072578	859541.238615	43.447604
3504.917220	859443.154311	43.452609
3505.056077	859357.855249	43.457613
3505.318224	859263.102559	43.462618
3505.322489	859173.350126	43.467623
3505.272203	859068.921906	43.472628
3505.018630	858988.349938	43.477633
3505.288213	858896.702115	43.482637
3505.145859	858806.676723	43.487642
3504.970290	858721.906823	43.492647
3504.945269	858616.105246	43.497652
3505.069321	858530.699836	43.502657
3504.852582	858446.905408	43.507661
3505.183999	858363.797539	43.512666
3504.893515	858267.953456	43.517671
3504.986662	858175.156848	43.522676
3504.753364	858094.569763	43.527681
3505.037777	858018.661973	43.532685
3505.162884	857927.412478	43.537690
3504.819405	857842.949847	43.542695
3504.778977	857758.533380	43.547700
3504.740081	857674.407289	43.552705
3504.929006	857592.285073	43.557709
3504.906166	857502.123539	43.562714
3504.836906	857411.092916	43.567719
3504.786740	857327.061185	43.572724
3504.908634	857243.291764	43.577729
3504.637214	857163.963237	43.582733
3505.089643	857070.604356	43.587738
3504.833325	856997.788498	43.592743
3504.497369	856906.502507	43.597748
3504.567650	856816.996492	43.602753
3504.645786	856751.515678	43.607757
3504.999481	856667.311093	43.612762
3504.709760	856582.724963	43.617767
3504.891135	856497.670918	43.622772
3504.826698	856416.644828	43.627777
3504.950366	856323.328763	43.632781
3504.824021	856243.672585	43.637786
3504.996954	856169.122306	43.642791
3504.715467	856083.165914	43.647796
3504.537283	855995.829235	43.652801
3504.828235	855917.851305	43.657805
3504.311332	855831.930187	43.662810
3504.192376	855759.368893	43.667815
3504.300831	855675.385727	43.672820
3504.128324	855611.782683	43.677825
3504.167416	855539.484645	43.682829
3504.452335	855456.928887	43.687834
3504.069645	855386.158025	43.692839
3504.210100	855317.051572	43.697844
3504.010534	855242.843352	43.702849
3504.478480	855173.000210	43.707853
3504.809990	855099.870408	43.712858
3504.221752	855021.442162	43.717863
3504.629892	854941.291838	43.722868
3504.445475	854869.606608	43.727873
3504.198342	854792.676176	43.732877
3504.606669	854705.711106	43.737882
3504.507303	854639.069335	43.742887
3504.675291	854555.353032	43.747892
3504.219510	854476.117514	43.752897
3504.345824	854410.798492	43.757901
3504.480836	854342.752488	43.762906
3504.167254	854267.870101	43.767911
3504.169988	854190.890992	43.772916
3504.397644	854119.323784	43.777921
3503.610520	854045.684560	43.782925
3504.099021	853976.700390	43.787930
3503.899558	853908.218096	43.792935
3504.268710	853838.473463	43.797940
3504.340625	853770.334225	43.802945
3504.289574	853707.567451	43.807949
3504.065284	853621.177978	43.812954
3504.013440	853559.285778	43.817959
3504.514485	853478.809187	43.822964
3504.142108	853415.605741	43.827969
3504.284751	853345.795543	43.832973
3504.159113	853263.764764	43.837978
3504.075698	853194.184768	43.842983
3504.109898	853117.868451	43.847988
3504.117151	853051.678662	43.852993
3504.306981	852985.166069	43.857997
3504.437843	852917.202396	43.863002
3503.918248	852848.761109	43.868007
3504.049999	852771.937754	43.873012
3504.439975	852700.035359	43.878017
3504.173871	852628.337571	43.883021
3503.977370	852554.388560	43.888026
3503.937641	852485.572156	43.893031
3503.903396	852423.471005	43.898036
3504.077994	852363.379120	43.903041
3503.809120	852298.492294	43.908045
3503.860352	852225.764074	43.913050
3503.614964	852172.651365	43.918055
3503.970421	852093.933086	43.923060
3503.761228	852030.396544	43.928065
3503.810843	851967.303477	43.933069
3503.977278	851908.474129	43.938074
3503.891136	851838.781999	43.943079
3504.094773	851767.678345	43.948084
3504.090485	851712.769546	43.953089
3503.612189	851644.794932	43.958093
3503.717741	851584.804241	43.963098
3503.653623	851522.893712	43.968103
3503.742127	851453.460561	43.973108
3503.737015	851391.636363	43.978113
3503.606098	851336.550374	43.983117
3503.893324	851272.047998	43.988122
3503.934596	851218.003599	43.993127
3504.190272	851150.681562	43.998132
3503.758060	851074.611675	44.003137
3503.646254	851016.696033	44.008141
3503.895083	850950.930860	44.013146
3503.610467	850897.813698	44.018151
3503.799514	850836.730952	44.023156
3503.910988	850768.746938	44.028161
3503.722297	850708.114657	44.033165
3503.613049	850642.405219	44.038170
3503.442521	850594.427514	44.043175
3503.424444	850523.833035	44.048180
3503.288355	850473.316934	44.053185
3503.462556	850413.498381	44.058189
3503.538889	850360.219774	44.063194
3503.269043	850306.608229	44.068199
3503.446675	850247.469175	44.073204
3503.772090	850194.342870	44.078209
3503.576676	850133.121800	44.083213
3503.558456	850068.949427	44.088218
3503.464411	850013.845641	44.093223
3503.737108	849952.740438	44.098228
3503.705079	849901.326079	44.103233
3503.646302	849840.469163	44.108237
3503.536679	849776.308835	44.113242
3503.216214	849726.888321	44.118247
3503.128586	849669.248317	44.123252
3503.105802	849622.115279	44.128257
3503.073877	849563.685995	44.133261
3503.365661	849515.136839	44.138266
3503.220348	849474.353360	44.143271
3503.055607	849411.074887	44.148276
3503.170713	849364.696334	44.153281
3503.184432	849318.431536	44.158285
3503.409187	849262.684207	44.163290
3502.882852	849208.715881	44.168295
3503.203427	849157.042492	44.173300
3503.193183	849102.014232	44.178305
3502.840811	849056.197402	44.183309
3502.991144	849004.453400	44.188314
3502.914651	848965.213653	44.193319
3502.819914	848924.223440	44.198324
3502.899239	848873.269262	44.203329
3502.882682	848823.888914	44.208333
3503.184144	848774.066162	44.213338
3502.910395	848733.883424	44.218343
3503.076217	848690.024014	44.223348
3502.837524	848639.509947	44.228353
3503.092297	848596.414472	44.233357
3503.323750	848543.581815	44.238362
3503.059079	848498.136064	44.243367
3503.038292	848447.000087	44.248372
3503.014305	848393.526387	44.253377
3502.862446	848353.515935	44.258381
3503.192786	848300.762344	44.263386
3503.200516	848265.205942	44.268391
3502.903461	848223.757407	44.273396
3502.643543	848163.599158	44.278401
3502.652896	848129.502915	44.283405
3503.097746	848069.812126	44.288410
3502.830502	848032.838487	44.293415
3502.842923	847989.194267	44.298420
3502.997984	847954.780817	44.303425
3502.936179	847904.718743	44.308429
3503.020607	847862.035945	44.313434
3502.935436	847823.862054	44.318439
3503.018485	847769.878291	44.323444
3502.968650	847732.379956	44.328449
3502.764215	847675.033042	44.333453
3503.032212	847639.332778	44.338458
3503.170199	847598.782631	44.343463
3502.943866	847542.607175	44.348468
3502.861926	847503.456567	44.353473
3502.690606	847463.541048	44.358477
3503.001091	847409.516704	44.363482
3502.951821	847367.242260	44.368487
3503.126114	847321.325921	44.373492
3502.960244	847280.336645	44.378497
3502.502387	847230.724142	44.383501
3502.709897	847189.672753	44.388506
3502.871935	847152.525748	44.393511
3503.043942	847094.721775	44.398516
3502.702029	847064.087650	44.403521
3502.646982	847021.422102	44.408525
3502.801220	846973.557898	44.413530
3502.643500	846949.615653	44.418535
3502.651558	846902.457016	44.423540
3502.743706	846859.181514	44.428545
3502.869390	846813.756634	44.433549
3502.953569	846772.430531	44.438554
3502.663232	846744.319649	44.443559
3502.798766	846692.461531	44.448564
3502.887323	846663.118622	44.453569
3502.712808	846620.859778	44.458573
3503.111829	846571.490615	44.463578
3502.671717	846527.326140	44.468583
3502.387375	846475.437969	44.473588
3502.519298	846438.194256	44.478593
3502.960814	846407.720157	44.483597
3502.884145	846364.176733	44.488602
3502.580424	846330.219720	44.493607
3502.581554	846279.841963	44.498612
3502.975549	846247.231179	44.503617
3502.789626	846203.314867	44.508621
3502.903451	846162.467082	44.513626
3502.572100	846124.323394	44.518631
3502.863052	846086.174387	44.523636
3502.856094	846046.417648	44.528641
3502.860703	846003.832794	44.533645
3502.828323	845962.423115	44.538650
3502.636776	845912.658843	44.543655
3502.921127	845867.200970	44.548660
3503.168906	845836.658578	44.553665
3503.020866	845793.805102	44.558669
3502.850819	845733.998502	44.563674
3502.689059	845700.501943	44.568679
3502.744748	845660.537536	44.573684
3502.917879	845625.523616	44.578689
3502.804363	845579.349595	44.583693
3502.940301	845536.350120	44.588698
3502.703704	845499.648833	44.593703
3503.023801	845442.487430	44.598708
3502.991615	845406.336652	44.603713
3502.935146	845367.460880	44.608717
3502.941338	845326.722853	44.613722
3502.864585	845288.532136	44.618727
3502.783721	845233.384056	44.623732
3503.063012	845194.939189	44.628737
3502.862997	845145.267692	44.633741
3502.372042	845101.393931	44.638746
3502.244105	845073.151337	44.643751
3502.713903	845035.746183	44.648756
3503.045207	844995.244828	44.653761
3502.800220	844956.884891	44.658765
3502.772953	844909.034863	44.663770
3502.829342	844877.154856	44.668775
3502.422565	844831.803377	44.673780
3502.293160	844790.109567	44.678785
3502.635712	844766.856290	44.683789
3502.855640	844723.642491	44.688794
3502.507060	844700.502844	44.693799
3502.404749	844657.926490	44.698804
3502.711682	844607.972286	44.703809
3502.515230	844583.929928	44.708813
3502.179238	844541.391287	44.713818
3502.480806	844523.407218	44.718823
3502.064887	844476.885048	44.723828
3502.410090	844453.532709	44.728833
3502.554167	844412.571105	44.733837
3502.856634	844380.160680	44.738842
3502.221482	844347.709630	44.743847
3502.209685	844302.874093	44.748852
3502.341732	844261.523596	44.753857
3502.407605	844228.664006	44.758861
3502.535191	844206.808726	44.763866
3502.490292	844177.183783	44.768871
3502.617886	844132.129115	44.773876
3502.559325	844104.260645	44.778881
3502.319271	844075.739618	44.783885
3502.698916	844031.227560	44.788890
3502.286106	843997.958251	44.793895
3502.429079	843967.813979	44.798900
3502.640709	843930.639770	44.803905
3502.523449	843896.346437	44.808909
3502.610010	843848.469598	44.813914
3502.675493	843827.305598	44.818919
3502.411236	843781.240701	44.823924
3502.571510	843748.070609	44.828929
3502.405208	843707.740457	44.833933
3502.847420	843671.306589	44.838938
3502.717351	843642.375547	44.843943
3502.338513	843601.397349	44.848948
3502.270778	843569.141242	44.853953
3501.912016	843542.489565	44.858957
3501.938766	843503.588574	44.863962
3502.374241	843483.239828	44.868967
3502.227870	843446.024266	44.873972
3502.456594	843414.303440	44.878977
3502.022359	843387.371082	44.883981
3502.483445	843354.344334	44.888986
3502.501332	843327.239737	44.893991
3502.499463	843284.345090	44.898996
3502.539081	843251.094779	44.904001
3502.412746	843223.038603	44.909005
3502.535068	843185.972216	44.914010
3502.286732	843161.835487	44.919015
3502.434433	843120.279953	44.924020
3502.592289	843085.546917	44.929025
3502.235095	843056.845596	44.934029
3502.510638	843017.218169	44.939034
3502.491631	842993.432983	44.944039
3502.262591	842956.715624	44.949044
3502.464131	842918.172203	44.954049
3502.160992	842899.015721	44.959053
3502.238482	842863.904729	44.964058
3502.576680	842840.060110	44.969063
3502.463487	842802.542801	44.974068
3502.617013	842761.958916	44.979073
3502.188511	842733.852855	44.984077
3502.501938	842702.796987	44.989082
3502.435287	842664.978698	44.994087
3502.222687	842638.299116	44.999092
3502.272797	842595.683726	45.004097
3502.219099	842576.777664	45.009101
3502.211271	842543.238947	45.014106
3502.089524	842519.663906	45.019111
3502.612397	842487.402463	45.024116
3502.224848	842463.871009	45.029121
3502.163237	842437.360704	45.034125
3502.138202	842402.459047	45.039130
3501.886732	842374.907234	45.044135
3502.004719	842343.101780	45.049140
3502.217327	842326.978692	45.054145
3502.101598	842291.018823	45.059149
3502.334257	842261.826682	45.064154
3502.179065	842228.505586	45.069159
3501.931678	842210.117867	45.074164
3502.034127	842186.504644	45.079169
3502.063359	842153.640296	45.084173
3502.158109	842128.955557	45.089178
3502.152328	842098.193086	45.094183
3502.013790	842074.911675	45.099188
3502.041552	842043.948398	45.104193
3501.901353	842027.102614	45.109197
3502.347367	841995.680155	45.114202
3502.066822	841972.665537	45.119207
3502.142184	841942.083956	45.124212
3501.949918	841913.008975	45.129217
3501.845276	841898.789763	45.134221
3502.137106	841858.323563	45.139226
3502.147328	841839.892321	45.144231
3502.197053	841817.456544	45.149236
3502.158804	841778.409381	45.154241
3501.617669	841770.405061	45.159245
3501.899837	841731.841135	45.164250
3501.906721	841707.364256	45.169255
3502.116856	841689.435961	45.174260
3502.223068	841659.140472	45.179265
3501.898579	841639.349842	45.184269
3502.248626	841609.306483	45.189274
3502.047789	841586.033538	45.194279
3501.958709	841557.378739	45.199284
3502.348943	841521.964987	45.204289
3501.980480	841506.423136	45.209293
3502.559184	841462.396554	45.214298
3502.023415	841446.589570	45.219303
3502.208389	841413.549447	45.224308
3502.109096	841393.184594	45.229313
3501.857233	841359.045946	45.234317
3501.843292	841327.257129	45.239322
3501.816942	841325.701200	45.244327
3502.004344	841289.636938	45.249332
3502.157319	841264.256600	45.254337
3501.865174	841243.142880	45.259341
3502.030278	841204.936361	45.264346
3501.987850	841193.777224	45.269351
3501.744389	841168.461822	45.274356
3502.175605	841133.331715	45.279361
3502.092466	841132.906599	45.284365
3502.122616	841088.528960	45.289370
3502.133680	841080.579061	45.294375
3501.957531	841037.210282	45.299380
3502.312375	841010.674149	45.304385
3502.284858	840993.904573	45.309389
3502.142905	840949.017931	45.314394
3502.116486	840939.074770	45.319399
3501.826256	840905.915251	45.324404
3501.979736	840886.628666	45.329409
3501.564473	840874.067509	45.334413
3501.810725	840844.525265	45.339418
3501.852017	840827.353805	45.344423
3501.947818	840803.687765	45.349428
3502.074427	840766.655278	45.354433
3502.053691	840753.980113	45.359437
3502.161861	840717.779366	45.364442
3501.950357	840705.769472	45.369447
3501.831399	840679.602609	45.374452
3502.069688	840650.694715	45.379457
3501.747392	840635.094349	45.384461
3501.947522	840605.217239	45.389466
3501.850279	840591.871645	45.394471
3502.185929	840573.188041	45.399476
3502.007404	840534.400157	45.404481
3501.843154	840529.501923	45.409485
3502.034382	840496.455998	45.414490
3501.985445	840474.909516	45.419495
3502.192614	840452.004075	45.424500
3502.497608	840414.452480	45.429505
3501.979117	840408.393355	45.434509
3502.157588	840365.936890	45.439514
3502.071663	840345.566470	45.444519
3501.940679	840309.207731	45.449524
3502.297054	840289.495767	45.454529
3502.006751	840270.816877	45.459533
3502.045321	840236.868170	45.464538
3501.714763	840225.949876	45.469543
3502.143206	840193.058362	45.474548
3502.117791	840168.532101	45.479553
3502.171222	840147.991781	45.484557
3502.134676	840106.690691	45.489562
3502.127924	840095.036054	45.494567
3501.771320	840067.735369	45.499572
3502.387242	840029.691350	45.504577
3502.130161	840008.031271	45.509581
3502.187941	839981.881182	45.514586
3502.262429	839956.215934	45.519591
3501.926109	839932.471539	45.524596
3502.015649	839915.679828	45.529601
3501.395168	839889.104637	45.534605
3502.027109	839866.956202	45.539610
3501.924316	839864.632177	45.544615
3501.669958	839826.437712	45.549620
3502.425997	839801.439881	45.554625
3502.118148	839779.299673	45.559629
3502.122744	839744.573593	45.564634
3501.526795	839729.162399	45.569639
3501.929674	839696.467621	45.574644
3502.060543	839684.984646	45.579649
3501.817506	839669.807793	45.584653
3501.925769	839634.771398	45.589658
3502.102249	839622.110254	45.594663
3501.670281	839594.039585	45.599668
3501.781224	839561.148350	45.604673
3501.903550	839558.689574	45.609677
3502.131013	839527.242158	45.614682
3502.517553	839513.424400	45.619687
3501.829238	839481.200950	45.624692
3502.327524	839450.586461	45.629697
3502.126067	839434.134070	45.634701
3502.354459	839388.541318	45.639706
3501.877506	839380.620926	45.644711
3502.205354	839350.570560	45.649716
3502.213397	839314.866072	45.654721
3502.245226	839289.497814	45.659725
3502.480863	839262.974041	45.664730
3502.280449	839238.082822	45.669735
3502.326999	839204.127290	45.674740
3502.613123	839173.936639	45.679745
3502.199947	839158.542716	45.684749
3502.216129	839111.812320	45.689754
3501.869712	839098.797303	45.694759
3501.699309	839063.706129	45.699764
3501.710654	839036.389161	45.704769
3501.897375	839027.480987	45.709773
3502.020170	839007.657217	45.714778
3501.795151	838987.061475	45.719783
3501.776209	838975.260463	45.724788
3502.121361	838938.912993	45.729793
3501.903529	838921.144970	45.734797
3501.743833	838902.489312	45.739802
3501.880730	838876.321646	45.744807
3501.977289	838863.916058	45.749812
3501.926743	838839.583928	45.754817
3501.928761	838799.292350	45.759821
3501.980323	838715.285994	45.764826
3501.723338	838580.158703	45.769831
3501.739702	838384.884225	45.774836
3501.623630	838136.841511	45.779841
3501.170152	837831.764982	45.784845
3501.404695	837463.330079	45.789850
3501.628989	837049.352565	45.794855
3501.486958	836557.823358	45.799860
3501.256715	835991.265214	45.804865
3500.974924	835390.794948	45.809869
3501.202296	834709.257940	45.814874
3500.790417	833968.540788	45.819879
3500.827298	833166.100440	45.824884
3500.731476	832301.179767	45.829889
3500.262554	831369.642473	45.834893
3500.397649	830356.353077	45.839898
3500.177341	829287.518242	45.844903
3499.672213	828141.112493	45.849908
3499.497740	826931.654566	45.854913
3498.991098	825650.079021	45.859917
3498.821800	824291.393908	45.864922
3498.583115	822859.873457	45.869927
3498.047742	821357.024804	45.874932
3497.928915	819778.866943	45.879937
3497.379537	818126.808225	45.884941
3497.185283	816396.162475	45.889946
3496.564927	814592.727363	45.894951
3495.819871	812712.772298	45.899956
3495.578975	810763.528846	45.904961
3495.105614	808732.222311	45.909965
3494.546276	806622.875053	45.914970
3494.194585	804449.392809	45.919975
3493.580693	802181.777218	45.924980
3493.511897	799844.535233	45.929985
3492.543750	797444.023000	45.934989
3491.738189	794946.763456	45.939994
3491.137588	792395.973472	45.944999
3490.544544	789762.593089	45.950004
3489.905918	787058.243668	45.955009
3489.011865	784288.736986	45.960013
3488.531228	781431.953550	45.965018
3487.808618	778508.574873	45.970023
3486.918889	775508.373824	45.975028
3486.396257	772440.780894	45.980033
3485.365294	769296.207216	45.985037
3484.727216	766064.753718	45.990042
3484.228430	762775.753943	45.995047
3483.089655	759401.986665	46.000052
3482.254684	755972.812762	46.005057
3481.145870	752464.362944	46.010061
3480.295232	748878.875501	46.015066
3479.363458	745229.017830	46.020071
3478.098861	741509.959303	46.025076
3477.645455	737706.091086	46.030081
3476.453929	733856.918504	46.035085
3475.467014	729906.422390	46.040090
3474.429012	725893.066297	46.045095
3473.127004	721818.597381	46.050100
3472.156405	717671.340570	46.055105
3470.466685	713450.141651	46.060109
3469.532473	709157.896467	46.065114
3468.674334	704806.307376	46.070119
3467.540101	700382.594364	46.075124
3466.557535	695877.055579	46.080129
3464.889689	691315.949717	46.085133
3463.982636	686669.164873	46.090138
3462.597869	681955.877066	46.095143
3461.298140	677174.924773	46.100148
3459.933936	672323.418081	46.105153
3458.576864	667409.050253	46.110157
3457.166198	662408.312218	46.115162
3455.609180	657358.320357	46.120167
3453.842000	652225.573847	46.125172
3452.549325	647033.862220	46.130177
3450.631905	641796.317940	46.135181
3449.439464	636461.251857	46.140186
3448.157551	631079.202708	46.145191
3446.255121	625631.947994	46.150196
3444.882580	620112.227718	46.155201
3442.901358	614533.252175	46.160205
3441.467260	608883.402039	46.165210
3439.975683	603178.278619	46.170215
3437.752459	597400.989156	46.175220
3436.315126	591563.889001	46.180225
3433.949357	585668.081428	46.185229
3432.696395	579704.751294	46.190234
3430.774373	573680.893815	46.195239
3428.681651	567599.217573	46.200244
3426.837670	561446.235898	46.205249
3424.672466	555242.712420	46.210253
3422.682524	548984.627090	46.215258
3420.891935	542666.116526	46.220263
3418.962960	536281.974433	46.225268
3417.051213	529819.184042	46.230273
3414.364575	523326.774519	46.235277
3412.182359	516761.779469	46.240282
3410.392871	510158.363589	46.245287
3407.600856	503500.908153	46.250292
3405.479781	496777.412802	46.255297
3403.246484	490006.475265	46.260301
3400.591859	483176.528115	46.265306
3397.997887	476305.280339	46.270311
3395.373139	469391.720160	46.275316
3392.965443	462416.030601	46.280321
3390.469937	455402.615304	46.285325
3387.928085	448339.193390	46.290330
3385.068280	441233.102785	46.295335
3382.639075	434087.821382	46.300340
3379.972408	426890.723254	46.305345
3377.058133	419658.206004	46.310349
3374.103594	412372.421923	46.315354
3371.446661	405071.265799	46.320359
3368.448369	397713.843847	46.325364
3365.072303	390325.581070	46.330369
3362.310144	382897.621899	46.335373
3359.363131	375429.714560	46.340378
3356.330042	367927.005835	46.345383
3353.083378	360389.319866	46.350388
3349.920350	352827.734258	46.355393
3346.944511	345243.190826	46.360397
3343.457718	337620.300638	46.365402
3340.194006	329977.105029	46.370407
3336.856817	322301.128184	46.375412
3334.043828	314605.099358	46.380417
3330.250744	306890.950198	46.385421
3326.747730	299133.166264	46.390426
3323.268517	291372.460291	46.395431
3319.848156	283585.358517	46.400436
3316.365022	275769.521785	46.405441
3312.359993	267958.043666	46.410445
3308.605336	260119.231160	46.415450
3304.912431	252272.944552	46.420455
3301.052480	244410.426019	46.425460
3297.209308	236552.418566	46.430465
3293.318896	228662.100392	46.435469
3289.417486	220697.269486	46.440474
3285.155513	212813.031458	46.445479
3281.279905	204939.821391	46.450484
3277.039841	197041.642014	46.455489
3272.291303	189152.384685	46.460493
3268.434808	181272.711912	46.465498
3263.703613	173403.552777	46.470503
3258.888954	165548.351937	46.475508
3254.439884	157693.907833	46.480513
3249.560340	149876.863576	46.485517
3244.788452	142073.694186	46.490522
3240.113916	134293.801253	46.495527
3235.289828	126528.609301	46.500532
3230.221076	118794.881739	46.505537
3224.704292	111095.956328	46.510541
3219.148207	103432.397416	46.515546
3213.468433	95802.270608	46.520551
3207.598230	88236.134961	46.525556
3201.833781	80707.308508	46.530561
3195.117948	73255.284008	46.535565
3188.175497	65857.558392	46.540570
3180.933627	58555.709719	46.545575
3172.811425	51343.497740	46.550580
3159.166675	44378.858138	46.555585
3137.719137	37767.630186	46.560589
3116.611328	31419.068732	46.565594
3092.061121	25508.074866	46.570599
3061.930369	20122.653811	46.575604
3029.985265	15316.885880	46.580609
2998.642801	11071.483233	46.585613
2970.224317	7381.408798	46.590618
2943.919326	4270.039572	46.595623
2919.777327	1729.234714	46.600628
2875.578203	334.380945	46.605633
2808.543529	305.828764	46.610637
2778.232536	295.259371	46.615642
2780.353834	285.842275	46.620647
2800.725837	280.938482	46.625652
2826.038088	274.797738	46.630657
2846.777862	281.077642	46.635661
2859.033335	282.820569	46.640666
2862.947196	275.287209	46.645671
2861.382527	271.926918	46.650676
2856.970737	270.630107	46.655681
2851.689150	279.071610	46.660685
2847.178237	266.978361	46.665690
2843.988269	279.012551	46.670695
2841.305991	272.650366	46.675700
2839.351502	262.161657	46.680705
2836.674831	274.666479	46.685709
2834.508352	260.228798	46.690714
2831.689994	258.210089	46.695719
2828.378995	268.691034	46.700724
2825.493459	254.350690	46.705729
2822.955231	259.579937	46.710733
2820.112332	254.758680	46.715738
2817.093470	245.946597	46.720743
2813.416503	259.276768	46.725748
2810.459004	251.438511	46.730753
2807.071889	248.480376	46.735757
2804.253119	251.591863	46.740762
2801.121620	246.212003	46.745767
2797.548719	250.952856	46.750772
2794.510620	240.026483	46.755777
2790.873823	251.395556	46.760781
2787.782678	248.480561	46.765786
2784.859700	238.261421	46.770791
2781.182374	244.310131	46.775796
2778.224752	238.875550	46.780801
2774.760881	246.167426	46.785805
2771.188327	243.016524	46.790810
2768.118164	238.804701	46.795815
2764.708844	245.158495	46.800820
2761.661070	236.380828	46.805825
2757.873290	232.831695	46.810829
2754.608711	230.875218	46.815834
2751.142866	228.504778	46.820839
2747.886350	232.674838	46.825844
2744.515145	231.459418	46.830849
2740.997081	227.709104	46.835853
2737.212515	239.212306	46.840858
2734.204752	219.949997	46.845863
2730.672358	232.765352	46.850868
2727.792826	222.435686	46.855873
2724.199236	225.161977	46.860877
2720.442954	220.831731	46.865882
2716.991594	231.838306	46.870887
2713.898118	227.536434	46.875892
2710.730647	220.764217	46.880897
2706.841684	232.989566	46.885901
2702.582011	229.194707	46.890906
2699.914686	225.568081	46.895911
2697.297879	231.240152	46.900916
2693.903394	228.869818	46.905921
2690.218459	226.721077	46.910925
2686.618191	221.503518	46.915930
2682.384084	224.900328	46.920935
2679.139435	227.703259	46.925940
2675.975126	215.477206	46.930945
2672.749342	222.291746	46.935949
2669.113072	218.778859	46.940954
2665.460651	220.546346	46.945959
2661.677431	219.226895	46.950964
2658.449682	211.713979	46.955969
2655.134040	220.557819	46.960973
2652.129676	219.031300	46.965978
2649.071330	217.251623	46.970983
2645.386052	221.884026	46.975988
2641.215421	215.202421	46.980993
2637.849414	206.297796	46.985997
2634.486595	218.672766	46.991002
2631.205184	220.783204	46.996007
2627.480389	213.108029	47.001012
2624.339974	211.617796	47.006017
2620.629171	214.152739	47.011021
2617.178424	213.998419	47.016026
2613.760271	213.669797	47.021031
2610.231605	221.541589	47.026036
2607.026361	217.320597	47.031041
2603.612392	205.743227	47.036045
2599.926606	209.239845	47.041050
2596.447534	216.671675	47.046055
2592.845241	212.515828	47.051060
2589.527668	211.268379	47.056065
2586.104167	216.476085	47.061069
2582.381181	214.373176	47.066074
2578.953923	215.176452	47.071079
2575.232051	206.736736	47.076084
2572.241089	204.486972	47.081089
2568.235297	213.910488	47.086093
2565.005210	201.007456	47.091098
2561.836550	206.364535	47.096103
2557.973197	215.506427	47.101108
2554.807026	200.661278	47.106113
2551.430434	205.988742	47.111117
2547.717576	217.363388	47.116122
2544.288974	202.520511	47.121127
2540.795282	208.372899	47.126132
2537.341224	205.716499	47.131137
2533.674955	209.866299	47.136141
2529.959154	206.055244	47.141146
2526.615998	200.278938	47.146151
2523.097542	207.368608	47.151156
2520.091201	200.667427	47.156161
2516.337845	196.486650	47.161165
2512.993658	191.179410	47.166170
2509.583626	191.602969	47.171175
2505.830817	199.706981	47.176180
2502.632007	197.733904	47.181185
2498.861315	202.685787	47.186189
2495.436732	201.486062	47.191194
2492.178967	201.224393	47.196199
2488.098048	202.474262	47.201204
2484.929029	191.210795	47.206209
2481.391797	201.116090	47.211213
2478.042214	195.934682	47.216218
2474.514059	196.817437	47.221223
2470.966250	203.201754	47.226228
2467.716899	193.342616	47.231233
2464.141353	193.112305	47.236237
2460.585966	201.150805	47.241242
2456.967042	188.298634	47.246247
2453.357044	201.546874	47.251252
2449.914390	195.048600	47.256257
2446.366583	199.620355	47.261261
2443.000175	205.165649	47.266266
2439.614572	192.192685	47.271271
2436.251545	204.053318	47.276276
2432.948153	193.744703	47.281281
2429.184077	194.021722	47.286285
2425.439987	192.792300	47.291290
2422.766691	190.607612	47.296295
2418.844840	196.095812	47.301300
2415.102647	191.819933	47.306305
2411.464974	191.133403	47.311309
2408.141706	192.899821	47.316314
2404.754637	188.847525	47.321319
2400.929537	195.006315	47.326324
2397.546446	194.271652	47.331329
2393.977921	190.766351	47.336333
2390.759038	187.436592	47.341338
2387.450286	185.085877	47.346343
2383.884281	187.767587	47.351348
2380.027491	180.740390	47.356353
2376.732892	185.563636	47.361357
2373.125251	185.506035	47.366362
2369.970612	183.805585	47.371367
2366.250118	189.165661	47.376372
2363.038386	192.962091	47.381377
2359.345144	181.600360	47.386381
2355.818081	181.448363	47.391386
2352.471446	179.641286	47.396391
2348.905536	189.416409	47.401396
2345.611922	178.844980	47.406401
2341.943332	191.594996	47.411405
2338.037103	198.061262	47.416410
2334.943321	186.138216	47.421415
2331.307059	191.979340	47.426420
2327.518550	185.020047	47.431425
2323.939544	190.106960	47.436429
2320.647467	190.821000	47.441434
2317.557764	192.088916	47.446439
2313.870717	195.600939	47.451444
2310.471556	187.607648	47.456449
2306.773929	189.318520	47.461453
2303.133138	186.019601	47.466458
2300.073992	186.090152	47.471463
2296.434866	190.175837	47.476468
2292.702448	181.343632	47.481473
2289.187060	184.900543	47.486477
2285.753656	185.458754	47.491482
2282.455804	183.196893	47.496487
2278.873412	174.694949	47.501492
2275.544212	173.877867	47.506497
2271.812734	176.348586	47.511501
2268.352173	175.982412	47.516506
2265.057463	174.602946	47.521511
2261.164688	188.434348	47.526516
2257.730535	167.931960	47.531521
2254.192946	171.906183	47.536525
2250.791148	183.387506	47.541530
2247.542198	166.449499	47.546535
2243.830271	177.394743	47.551540
2240.473592	166.015843	47.556545
2236.641943	161.572546	47.561549
2233.245651	176.558907	47.566554
2230.259013	168.029289	47.571559
2226.356097	186.191237	47.576564
2222.941183	173.179893	47.581569
2219.185924	175.707663	47.586573
2215.829724	177.296315	47.591578
2212.673897	174.055730	47.596583
2208.819972	187.367073	47.601588
2205.359186	170.915392	47.606593
2201.891403	183.521821	47.611597
2198.413101	176.660807	47.616602
2195.034739	172.527902	47.621607
2191.288018	176.554857	47.626612
2187.831188	168.755510	47.631617
2184.499209	175.418925	47.636621
2180.971827	164.818154	47.641626
2177.327385	167.050788	47.646631
2173.633408	175.067745	47.651636
2170.770483	174.844303	47.656641
2167.174751	169.716409	47.661645
2163.726598	168.329395	47.666650
2159.811862	166.118376	47.671655
2156.345454	164.421007	47.676660
2152.722783	164.434134	47.681665
2149.523300	170.303894	47.686669
2145.679530	174.531420	47.691674
2142.420020	176.501400	47.696679
2138.686434	176.540746	47.701684
2135.511219	169.450749	47.706689
2131.864671	168.340827	47.711693
2128.372361	168.401514	47.716698
2125.112211	167.396516	47.721703
2121.113752	178.000199	47.726708
2117.987213	162.807495	47.731713
2114.403371	166.594282	47.736717
2110.797576	171.376330	47.741722
2107.520170	172.248921	47.746727
2104.009007	170.976157	47.751732
2100.587000	165.171960	47.756737
2096.874276	170.157767	47.761741
2092.944358	171.342764	47.766746
2090.187356	165.593337	47.771751
2086.672612	166.767401	47.776756
2083.009522	170.960793	47.781761
2078.712672	165.332661	47.786765
2075.569989	164.939982	47.791770
2072.347645	160.063091	47.796775
2068.937510	173.645385	47.801780
2065.530520	165.102619	47.806785
2062.165977	167.654980	47.811789
2058.382690	168.152334	47.816794
2055.124318	170.944892	47.821799
2051.480144	168.995945	47.826804
2047.920229	166.394496	47.831809
2044.303142	173.334391	47.836813
2040.681865	166.528695	47.841818
2037.530307	166.298930	47.846823
2033.565077	168.559388	47.851828
2030.337886	165.268358	47.856833
2027.283107	165.070965	47.861837
2023.496756	170.321776	47.866842
2019.884911	163.477638	47.871847
2016.413353	167.144517	47.876852
2012.883932	159.029721	47.881857
2009.296362	166.919886	47.886861
2005.643251	167.944780	47.891866
2002.467406	166.036138	47.896871
1999.100235	167.745941	47.901876
1995.677541	164.753633	47.906881
1992.001838	162.511958	47.911885
1988.346362	168.123426	47.916890
1984.962516	160.168924	47.921895
1981.152120	164.432697	47.926900
1977.850293	157.241384	47.931905
1974.149717	164.954672	47.936909
1970.735652	164.229178	47.941914
1967.735987	170.238519	47.946919
1963.626298	164.468877	47.951924
1960.310188	164.312125	47.956929
1956.502605	161.208575	47.961933
1953.354621	164.282132	47.966938
1950.225392	157.130809	47.971943
1946.654190	161.587961	47.976948
1942.967936	157.956629	47.981953
1939.591958	157.987780	47.986957
1935.593257	166.846361	47.991962
1932.302897	159.790338	47.996967
1928.398337	161.790830	48.001972
1925.478563	150.623216	48.006977
1922.076582	157.472008	48.011981
1918.389185	157.863844	48.016986
1914.745439	157.511411	48.021991
1911.156908	154.959394	48.026996
1907.889330	146.556345	48.032001
1904.404697	157.724544	48.037005
1900.791605	155.885435	48.042010
1897.506570	151.808188	48.047015
1893.909630	162.385366	48.052020
1890.544845	160.047224	48.057025
1887.014004	154.253676	48.062029
1883.084956	156.578925	48.067034
1880.088474	156.585912	48.072039
1876.575533	157.959932	48.077044
1872.866945	159.897311	48.082049
1869.379259	157.084955	48.087053
1865.657461	156.680527	48.092058
1862.242173	159.793165	48.097063
1858.614534	166.136596	48.102068
1855.479319	155.764769	48.107073
1851.957738	162.148108	48.112077
1848.140850	153.067602	48.117082
1844.696227	153.988713	48.122087
1841.487001	159.163461	48.127092
1837.549957	160.096064	48.132097
1834.170663	158.410791	48.137101
1830.744263	160.489256	48.142106
1827.491054	149.748584	48.147111
1823.891304	166.467069	48.152116
1820.218756	158.016722	48.157121
1816.700192	167.931366	48.162125
1813.259572	157.700997	48.167130
1810.072787	146.957458	48.172135
1806.067776	167.988453	48.177140
1802.696063	161.970356	48.182145
1799.391583	164.669857	48.187149
1795.490923	159.817608	48.192154
1792.328093	152.848572	48.197159
1788.640519	154.138824	48.202164
1785.403652	160.217644	48.207169
1782.182388	153.817923	48.212173
1778.117725	156.869371	48.217178
1775.056384	150.528881	48.222183
1770.840050	161.681685	48.227188
1767.806661	165.698455	48.232193
1764.243554	155.778847	48.237197
1760.562844	156.259686	48.242202
1757.580853	158.374108	48.247207
1753.580098	162.407831	48.252212
1750.481730	155.959412	48.257217
1746.797798	162.106197	48.262221
1742.942768	157.520165	48.267226
1739.832271	153.145422	48.272231
1735.811928	155.362931	48.277236
1732.871145	158.026858	48.282241
1729.505091	160.486550	48.287245
1725.659356	157.213471	48.292250
1722.537304	149.256386	48.297255
1718.668239	161.331445	48.302260
1715.288287	154.856362	48.307265
1711.455294	146.465384	48.312269
1708.028752	151.020559	48.317274
1705.102092	136.977057	48.322279
1701.229682	148.892235	48.327284
1697.649313	150.908614	48.332289
1694.154623	158.401593	48.337293
1690.801534	153.530008	48.342298
1687.241563	158.620325	48.347303
1683.414319	162.453555	48.352308
1680.110506	149.507813	48.357313
1676.855541	153.927309	48.362317
1673.387707	154.455728	48.367322
1670.005108	148.751926	48.372327
1666.110510	154.672299	48.377332
1662.818948	149.162836	48.382337
1659.402464	155.709109	48.387341
1655.464917	157.501553	48.392346
1652.344515	148.427509	48.397351
1648.667031	145.728976	48.402356
1645.087254	142.973651	48.407361
1641.470631	147.332944	48.412365
1638.109418	144.067699	48.417370
1634.615610	147.299043	48.422375
1630.901686	160.450860	48.427380
1627.787953	144.813831	48.432385
1624.534535	148.427765	48.437389
1620.506333	152.803381	48.442394
1617.085249	147.086444	48.447399
1613.344148	157.096594	48.452404
1610.073603	146.041841	48.457409
1606.885568	146.109862	48.462413
1602.814302	146.199115	48.467418
1600.293832	144.352564	48.472423
1596.282452	154.885932	48.477428
1592.819235	148.049173	48.482433
1589.182126	157.215307	48.487437
1585.463136	150.110011	48.492442
1581.833715	139.831520	48.497447
1578.312757	151.182734	48.502452
1574.939525	148.479372	48.507457
1572.061926	157.088035	48.512461
1567.950174	152.208119	48.517466
1564.711872	142.642325	48.522471
1560.984283	149.649745	48.527476
1557.630973	136.349591	48.532481
1554.189462	139.770279	48.537485
1550.444061	140.368338	48.542490
1547.256178	145.663274	48.547495
1543.444361	150.492987	48.552500
1540.262881	139.825951	48.557505
1536.574682	140.410425	48.562509
1532.665142	145.182885	48.567514
1529.717509	140.217980	48.572519
1526.216321	144.981768	48.577524
1522.819763	146.339773	48.582529
1519.364595	145.994570	48.587533
1515.526561	141.524534	48.592538
1512.047461	137.810388	48.597543
1508.140776	141.196094	48.602548
1504.809974	145.431683	48.607553
1501.921709	141.313434	48.612557
1497.501103	145.036083	48.617562
1494.415474	145.364912	48.622567
1490.990260	139.408205	48.627572
1487.728332	135.913741	48.632577
1484.469263	137.599720	48.637581
1480.679311	149.406506	48.642586
1476.792952	142.917432	48.647591
1473.370668	142.614782	48.652596
1469.970409	139.324743	48.657601
1466.874117	136.426902	48.662605
1463.049350	141.374849	48.667610
1459.730122	131.709644	48.672615
1455.900166	142.009867	48.677620
1452.435057	142.157729	48.682625
1449.251194	140.153908	48.687629
1445.504564	135.198375	48.692634
1442.188427	134.549045	48.697639
1438.448500	144.947674	48.702644
1434.907923	139.954737	48.707649
1431.551425	147.925694	48.712653
1427.914432	136.458054	48.717658
1424.554104	132.632191	48.722663
1421.010872	142.786775	48.727668
1417.467271	136.131189	48.732673
1413.999146	133.916655	48.737677
1410.304216	143.053191	48.742682
1406.955694	139.230125	48.747687
1403.368388	141.079343	48.752692
1399.781883	136.671636	48.757697
1396.353350	142.698309	48.762701
1392.995189	146.306226	48.767706
1389.887181	141.346219	48.772711
1386.343493	134.707053	48.777716
1382.442643	133.698564	48.782721
1378.603645	134.987523	48.787725
1374.875377	144.775679	48.792730
1372.017870	131.710268	48.797735
1368.318720	146.371412	48.802740
1365.270287	129.720757	48.807745
1361.775349	132.547742	48.812749
1357.989343	139.624362	48.817754
1354.295717	129.690196	48.822759
1350.788208	138.443741	48.827764
1347.310515	134.083410	48.832769
1344.086834	125.363151	48.837773
1340.410964	134.840541	48.842778
1337.302060	129.560248	48.847783
1333.481555	124.977958	48.852788
1329.873194	133.747396	48.857793
1326.083912	134.574106	48.862797
1322.555240	139.929857	48.867802
1319.412369	125.097932	48.872807
1315.989443	135.577443	48.877812
1312.477553	137.213768	48.882817
1309.096344	127.418826	48.887821
1305.067989	132.947964	48.892826
1302.013872	135.075378	48.897831
1298.419492	130.541381	48.902836
1294.872877	132.285089	48.907841
1291.534753	126.755794	48.912845
1287.724332	134.042717	48.917850
1284.441396	131.196186	48.922855
1280.900834	132.475555	48.927860
1277.449147	139.609648	48.932865
1273.907660	122.948232	48.937869
1270.170840	135.148545	48.942874
1267.086957	118.749729	48.947879
1263.614642	135.818443	48.952884
1259.938746	131.419711	48.957889
1256.632413	129.316690	48.962893
1252.603340	127.907801	48.967898
1249.367843	117.394989	48.972903
1245.714864	136.801639	48.977908
1242.156222	131.000005	48.982913
1238.837490	128.553311	48.987917
1234.968018	135.145346	48.992922
1231.837932	134.492447	48.997927
1228.064023	130.534617	49.002932
1224.697536	136.411038	49.007937
1221.430222	132.803998	49.012941
1217.547974	136.803368	49.017946
1214.433007	125.207399	49.022951
1210.635319	133.626965	49.027956
1207.448536	137.085116	49.032961
1204.295114	129.089419	49.037965
1200.045042	138.103970	49.042970
1196.776779	137.585041	49.047975
1193.164806	128.013649	49.052980
1189.684736	131.177328	49.057985
1186.563286	134.246395	49.062989
1182.420027	130.838277	49.067994
1179.183114	125.368116	49.072999
1175.641035	128.409841	49.078004
1172.198462	133.338239	49.083009
1168.827228	122.753210	49.088013
1165.491598	137.364637	49.093018
1162.217353	127.732698	49.098023
1158.563146	136.258825	49.103028
1155.163732	125.019950	49.108033
1151.404083	134.885477	49.113037
1147.639239	129.344955	49.118042
1144.187740	125.059593	49.123047
1140.165329	130.191630	49.128052
1136.828859	132.334657	49.133057
1133.665008	123.468118	49.138061
1130.310602	126.682301	49.143066
1127.305104	129.295526	49.148071
1122.968077	127.893864	49.153076
1119.713424	132.937453	49.158081
1116.152256	121.194130	49.163085
1112.436279	129.001141	49.168090
1109.348744	123.410627	49.173095
1105.957023	127.670569	49.178100
1102.190061	132.747376	49.183105
1098.667696	126.810018	49.188109
1094.810486	136.233107	49.193114
1091.778850	135.150606	49.198119
1088.460395	133.800780	49.203124
1084.640013	127.385626	49.208129
1081.321456	127.518812	49.213133
1077.458449	131.669037	49.218138
1074.143764	125.414378	49.223143
1070.652584	134.233690	49.228148
1066.971137	130.542904	49.233153
1063.684285	132.644626	49.238157
1060.009618	131.679529	49.243162
1057.201653	122.895495	49.248167
1053.388649	125.930804	49.253172
1049.810699	129.423748	49.258177
1046.295660	120.553193	49.263181
1042.386004	124.542041	49.268186
1039.171803	131.118815	49.273191
1035.799431	129.629351	49.278196
1032.244101	132.813682	49.283201
1028.646040	122.749168	49.288205
1024.775145	136.974992	49.293210
1021.323100	122.277333	49.298215
1017.690762	122.384705	49.303220
1014.543001	125.386997	49.308225
1011.371132	121.135028	49.313229
1007.712892	130.187238	49.318234
1004.119993	122.459546	49.323239
1000.786087	124.114824	49.328244
997.356317	129.080300	49.333249
993.647093	122.632837	49.338253
989.671105	139.716930	49.343258
986.347627	126.948517	49.348263
982.755729	132.823899	49.353268
979.509256	132.745139	49.358273
976.432728	129.577186	49.363277
972.537853	130.216224	49.368282
969.139305	120.514431	49.373287
965.612067	127.422844	49.378292
962.123218	129.765248	49.383297
958.423873	122.805673	49.388301
954.749264	124.266319	49.393306
951.711799	121.356751	49.398311
948.178589	120.975361	49.403316
944.577180	127.016329	49.408321
941.383042	126.849613	49.413325
937.386278	140.731838	49.418330
934.114283	117.789944	49.423335
930.594245	126.252599	49.428340
926.975043	122.213801	49.433345
923.364359	116.465848	49.438349
919.870390	128.795155	49.443354
916.379744	122.385218	49.448359
913.000292	127.950623	49.453364
909.620743	128.622689	49.458369
906.238728	130.880766	49.463373
902.550434	126.140438	49.468378
899.320842	128.256486	49.473383
895.561246	129.801488	49.478388
892.023062	135.933472	49.483393
888.485723	133.988918	49.488397
884.547593	135.672389	49.493402
881.597052	127.014084	49.498407
877.811073	125.596706	49.503412
874.489383	131.466745	49.508417
870.835933	122.627525	49.513421
867.399035	125.525001	49.518426
864.355089	121.716515	49.523431
860.186831	126.279915	49.528436
856.723182	126.516793	49.533441
853.891181	129.682456	49.538445
850.081366	135.103403	49.543450
846.630346	122.286752	49.548455
842.897223	124.117306	49.553460
839.054807	123.432535	49.558465
836.005825	117.886961	49.563469
832.284883	120.546098	49.568474
829.179751	117.748453	49.573479
825.723029	122.382839	49.578484
821.709185	122.139267	49.583489
818.430734	118.676267	49.588493
814.833824	122.084119	49.593498
811.272474	118.109458	49.598503
807.681519	125.236912	49.603508
804.318634	125.396778	49.608513
801.303320	120.311571	49.613517
797.567527	124.920904	49.618522
794.409561	112.273100	49.623527
790.365431	125.143818	49.628532
786.833192	126.279716	49.633537
783.855119	122.355410	49.638541
779.696430	118.045252	49.643546
775.957689	121.241371	49.648551
772.657722	123.596284	49.653556
769.294349	117.652447	49.658561
766.082509	117.766832	49.663565
762.338596	117.847680	49.668570
758.927762	121.218676	49.673575
755.251782	118.722920	49.678580
751.762250	123.453760	49.683585
748.849917	127.845013	49.688589
744.958134	128.073870	49.693594
741.402056	132.546759	49.698599
737.732971	124.654897	49.703604
734.077649	122.819186	49.708609
731.211075	121.371591	49.713613
726.842048	122.743454	49.718618
723.651366	114.280901	49.723623
720.378524	122.592299	49.728628
716.617011	116.333909	49.733633
713.626024	115.824326	49.738637
709.808276	119.920595	49.743642
706.190524	108.405079	49.748647
702.863426	123.065479	49.753652
699.447527	122.236463	49.758657
695.873327	120.283762	49.763661
692.535804	126.658568	49.768666
688.910928	118.460673	49.773671
685.256282	118.753952	49.778676
681.591323	114.262750	49.783681
678.088153	108.687854	49.788685
674.325241	124.377652	49.793690
671.215888	112.182296	49.798695
667.931662	129.127687	49.803700
664.472195	119.655282	49.808705
661.012786	119.180018	49.813709
657.172272	121.510585	49.818714
654.061597	119.320597	49.823719
650.432776	128.578559	49.828724
646.936192	127.285577	49.833729
643.369755	119.533309	49.838733
639.788994	126.861075	49.843738
636.316143	125.208182	49.848743
632.846292	120.718879	49.853748
628.888061	118.286508	49.858753
625.630834	110.601501	49.863757
622.280466	118.435409	49.868762
619.051567	111.304970	49.873767
615.238302	121.848725	49.878772
611.775308	120.434774	49.883777
608.312739	108.219773	49.888781
604.483824	122.793159	49.893786
601.063513	121.795834	49.898791
597.813252	119.897558	49.903796
594.269569	109.817746	49.908801
591.049095	107.062847	49.913805
586.878467	112.108183	49.918810
583.687179	114.230351	49.923815
580.092407	117.720321	49.928820
576.611688	113.769816	49.933825
573.438862	116.252429	49.938829
569.606911	115.753831	49.943834
566.291767	115.287727	49.948839
562.606715	122.604981	49.953844
559.100760	124.728916	49.958849
555.837584	115.062315	49.963853
551.794794	120.651897	49.968858
548.827994	116.156583	49.973863
545.110979	120.060888	49.978868
541.744352	117.061636	49.983873
538.273425	115.307075	49.988877
534.690336	125.437867	49.993882
531.014258	115.527625	49.998887
527.341298	118.479022	50.003892
524.006071	116.018840	50.008897
521.000086	116.015472	50.013901
516.998579	119.731260	50.018906
513.696548	117.266777	50.023911
510.412414	115.821140	50.028916
506.819387	122.334063	50.033921
503.194228	114.840679	50.038925
499.396963	121.018980	50.043930
496.139708	116.586570	50.048935
492.671543	119.244805	50.053940
489.065877	123.358653	50.058945
485.883322	115.298107	50.063949
481.651788	122.744539	50.068954
478.628170	118.374316	50.073959
475.251733	114.900373	50.078964
471.569527	115.393162	50.083969
468.220268	112.118181	50.088973
464.451254	113.496973	50.093978
460.921342	106.398919	50.098983
457.427223	117.095993	50.103988
454.101159	113.689311	50.108993
450.627073	105.775714	50.113997
446.762991	113.396980	50.119002
443.855776	118.734191	50.124007
440.590109	112.782354	50.129012
436.391280	115.118341	50.134017
433.120187	109.273181	50.139021
429.202005	115.220933	50.144026
425.943940	112.744903	50.149031
422.584259	109.788802	50.154036
419.076273	113.205729	50.159041
415.653638	115.041294	50.164045
411.912175	117.091643	50.169050
408.913283	109.137717	50.174055
405.192137	111.210165	50.179060
401.321926	117.011078	50.184065
397.883573	113.092983	50.189069
394.083357	116.843841	50.194074
390.906313	114.303120	50.199079
387.542055	112.913464	50.204084
384.093093	111.878432	50.209089
380.812762	115.614689	50.214093
377.040501	116.645007	50.219098
373.706724	110.629117	50.224103
370.353443	114.731278	50.229108
366.160296	118.577981	50.234113
363.023629	107.029146	50.239117
359.488228	106.599264	50.244122
356.070796	102.827522	50.249127
352.178297	113.016360	50.254132
348.801244	115.194506	50.259137
345.780966	112.183275	50.264141
341.942786	121.256282	50.269146
338.580595	117.228738	50.274151
334.903150	112.535473	50.279156
331.094386	112.779967	50.284161
327.991168	111.064961	50.289165
324.436424	116.708934	50.294170
321.105674	106.534931	50.299175
317.432652	115.234096	50.304180
314.022184	108.742546	50.309185
310.664479	110.910019	50.314189
306.703290	109.747112	50.319194
303.255723	108.259030	50.324199
299.948239	115.308165	50.329204
296.231544	111.652708	50.334209
293.069580	108.049482	50.339213
289.549917	108.042507	50.344218
285.988551	113.083562	50.349223
282.532654	111.568657	50.354228
278.659286	114.816085	50.359233
275.337959	107.557572	50.364237
271.625721	116.998140	50.369242
268.543738	108.901198	50.374247
265.088014	118.378440	50.379252
261.144775	115.135058	50.384257
257.839024	102.709920	50.389261
254.346256	117.124901	50.394266
250.936202	112.391790	50.399271
247.510387	112.604932	50.404276
243.897086	109.194072	50.409281
240.557720	98.457392	50.414285
236.820585	107.411134	50.419290
233.743891	107.129985	50.424295
230.079141	108.691027	50.429300
226.216415	116.808547	50.434305
222.845182	104.174252	50.439309
219.106957	106.887668	50.444314
215.880873	109.829275	50.449319
212.297270	106.261185	50.454324
208.551887	112.973014	50.459329
205.261685	110.683828	50.464333
201.760954	120.075622	50.469338
198.241311	104.972787	50.474343
194.822726	103.829478	50.479348
191.399328	116.958430	50.484353
188.301307	102.734986	50.489357
184.454148	107.728517	50.494362
180.838912	111.511879	50.499367
177.141787	112.195055	50.504372
173.518160	109.738306	50.509377
170.144917	106.688358	50.514381
166.577458	107.301531	50.519386
163.325621	110.152719	50.524391
160.086134	117.090053	50.529396
156.224991	114.176741	50.534401
152.922644	107.035959	50.539405
149.074773	115.278561	50.544410
145.681904	104.005387	50.549415
142.491979	111.821545	50.554420
138.904970	116.075255	50.559425
135.652887	107.309006	50.564429
131.694108	117.758430	50.569434
128.225165	103.814507	50.574439
124.482637	114.433555	50.579444
121.008975	112.978755	50.584449
117.583351	109.823069	50.589453
114.191720	111.536322	50.594458
110.846757	106.265276	50.599463
107.279845	103.936147	50.604468
103.724956	107.481657	50.609473
100.263814	110.079045	50.614477
96.661441	107.151557	50.619482
93.026447	111.889613	50.624487
89.293293	105.001374	50.629492
86.352221	103.854270	50.634497
83.193164	92.956850	50.639501
79.340607	112.605236	50.644506
76.011452	104.239763	50.649511
72.224259	104.045596	50.654516
68.593120	118.757120	50.659521
65.231650	103.422802	50.664525
61.248480	118.313590	50.669530
58.242572	112.907114	50.674535
54.915393	112.723419	50.679540
50.823315	116.579929	50.684545
47.936649	106.555819	50.689549
44.192867	113.122870	50.694554
41.051549	108.177902	50.699559
37.522861	107.040522	50.704564
33.749147	108.179126	50.709569
30.203042	101.388238	50.714573
26.495780	112.010202	50.719578
23.162029	97.805620	50.724583
19.790882	110.965299	50.729588
15.948019	106.598487	50.734593
12.825521	103.009075	50.739597
9.148184	104.333219	50.744602
5.771679	107.819076	50.749607
2.148683	101.163690	50.754612