Tue Jun 21 13:21:23 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
0.948589	116.927616	0.000000
0.454842	112.502882	0.005005
0.996713	107.003854	0.010010
0.446226	111.538628	0.015014
0.329528	96.642657	0.020019
0.168232	92.120254	0.025024
0.077257	81.390306	0.030029
0.192635	73.080242	0.035034
-0.020548	68.884738	0.040038
-0.295173	52.331900	0.045043
-0.783774	46.828694	0.050048
-1.061257	35.247383	0.055053
-1.021791	25.639422	0.060058
-1.808649	23.717490	0.065062
-2.191228	13.200256	0.070067
-2.633755	4.999980	0.075072
-2.650970	6.817741	0.080077
-2.958429	-6.951538	0.085082
-3.505773	0.828419	0.090086
-3.453594	4.231707	0.095091
-3.696012	-8.704741	0.100096
-4.422432	-0.565387	0.105101
-5.179394	-13.569361	0.110106
-5.071702	-6.722729	0.115110
-5.417792	-2.536778	0.120115
-5.068160	-2.143535	0.125120
-5.309563	2.237610	0.130125
-5.124824	-10.514222	0.135130
-5.462261	-4.739002	0.140134
-6.352405	-3.831830	0.145139
-6.912980	-4.428052	0.150144
-7.165105	-1.690299	0.155149
-6.849752	-11.036871	0.160154
-7.123892	-8.175101	0.165158
-6.977734	-11.682984	0.170163
-8.077429	-8.644250	0.175168
-8.556499	-3.630567	0.180173
-8.315939	-3.187886	0.185178
-8.739148	-0.370890	0.190182
-8.377597	-8.142108	0.195187
-8.272250	-8.929904	0.200192
-9.155505	-12.367961	0.205197
-9.653698	-7.134244	0.210202
-10.150528	3.705090	0.215206
-10.054714	-10.759470	0.220211
-10.376840	-10.912501	0.225216
-10.328635	1.065172	0.230221
-10.361494	-5.686431	0.235226
-10.577494	1.437581	0.240230
-11.662232	-6.009285	0.245235
-12.017839	-6.874472	0.250240
-12.214667	-0.038584	0.255245
-11.725944	-11.984327	0.260250
-11.997336	-1.453266	0.265254
-11.763542	-12.172991	0.270259
-12.220306	-7.390726	0.275264
-12.936290	-7.660081	0.280269
-12.971981	-4.048069	0.285274
-13.579121	4.276171	0.290278
-14.593741	-1.381445	0.295283
-14.469200	0.056063	0.300288
-14.046701	3.765658	0.305293
-14.431470	-5.946472	0.310298
-14.689362	-0.525612	0.315302
-15.136366	-2.212159	0.320307
-15.311968	1.224309	0.325312
-15.333000	3.395534	0.330317
-15.387598	-8.437941	0.335322
-16.301039	1.006367	0.340326
-16.392619	4.306378	0.345331
-16.274483	-2.764651	0.350336
-16.834074	1.269190	0.355341
-16.963439	3.668909	0.360346
-17.388804	4.032425	0.365350
-17.887447	3.276173	0.370355
-17.995191	0.714908	0.375360
-18.297558	8.349321	0.380365
-18.260228	1.971878	0.385370
-18.609381	4.450026	0.390374
-18.818039	-2.091314	0.395379
-18.406170	4.927147	0.400384
-18.906912	-3.828446	0.405389
-19.393832	-0.932819	0.410394
-19.704232	4.497724	0.415398
-19.715187	2.903939	0.420403
-20.116789	-2.052832	0.425408
-21.338325	1.365625	0.430413
-21.231318	-3.227819	0.435418
-21.269266	-0.667218	0.440422
-21.274998	0.688658	0.445427
-21.551108	-5.571164	0.450432
-21.802105	6.992410	0.455437
-21.822786	-9.899001	0.460442
-21.589409	-3.713331	0.465446
-21.812422	-8.309152	0.470451
-22.880299	-5.407896	0.475456
-23.230332	-2.860143	0.480461
-22.702718	-5.085187	0.485466
-23.636174	4.711718	0.490470
-24.127412	1.069032	0.495475
-24.180371	2.093710	0.500480
-24.590007	4.852418	0.505485
-24.040335	-2.365060	0.510490
-24.089866	-5.576507	0.515494
-24.923698	-0.700420	0.520499
-25.327941	4.433877	0.525504
-25.896184	1.812710	0.530509
-25.589644	-6.692357	0.535514
-26.318385	-4.479121	0.540518
-26.132109	-5.215595	0.545523
-26.288978	-4.265667	0.550528
-26.896644	-0.824940	0.555533
-26.957827	-5.549582	0.560538
-27.516431	0.557278	0.565542
-27.522769	1.554108	0.570547
-27.591393	0.115900	0.575552
-28.173401	-2.723407	0.580557
-28.414419	-9.739298	0.585562
-28.608196	-2.067028	0.590566
-28.540052	-2.416702	0.595571
-28.870325	-5.828916	0.600576
-29.216955	3.403131	0.605581
-29.702641	-0.001108	0.610586
-30.356138	6.764775	0.615590
-30.503194	-1.397005	0.620595
-30.578466	-1.706155	0.625600
-30.726766	7.353142	0.630605
-30.827067	2.153878	0.635610
-31.107956	2.200430	0.640614
-30.868781	2.776934	0.645619
-30.740063	3.618396	0.650624
-31.532408	2.872500	0.655629
-32.024897	-7.784181	0.660634
-32.436907	4.031324	0.665638
-32.446689	1.620189	0.670643
-32.405757	-8.939728	0.675648
-33.281124	9.727352	0.680653
-33.542579	-3.370912	0.685658
-33.828337	6.615328	0.690662
-33.949343	2.118447	0.695667
-34.035297	-2.450146	0.700672
-34.240296	2.746074	0.705677
-33.895790	-8.674957	0.710682
-34.772817	-4.412922	0.715686
-35.026105	-3.366120	0.720691
-35.173129	-3.901964	0.725696
-35.509768	-1.481142	0.730701
-35.888895	3.015557	0.735706
-36.276143	-0.308684	0.740710
-36.370693	1.119521	0.745715
-36.647394	-8.680947	0.750720
-36.973870	2.305999	0.755725
-36.806782	-12.185752	0.760730
-37.028159	-7.408129	0.765734
-37.603572	-3.577486	0.770739
-37.765923	-11.876240	0.775744
-38.569203	-2.712430	0.780749
-38.366655	-1.926411	0.785754
-38.825418	2.478298	0.790758
-38.614430	-6.967617	0.795763
-38.719183	-7.330099	0.800768
-39.516196	-6.377959	0.805773
-39.787133	-9.887613	0.810778
-40.327986	2.932933	0.815782
-40.419603	3.434766	0.820787
-40.265905	-0.677616	0.825792
-40.681491	0.612735	0.830797
-40.156478	-7.337302	0.835802
-40.694519	-0.373672	0.840806
-41.308248	-10.350390	0.845811
-41.512800	-7.415683	0.850816
-42.179409	-4.356309	0.855821
-41.797678	-3.195628	0.860826
-41.729506	-7.750276	0.865830
-42.706848	-13.725641	0.870835
-42.991001	-17.649082	0.875840
-43.180669	-8.829216	0.880845
-42.827748	-15.455259	0.885850
-43.251848	-9.562089	0.890854
-44.460868	-4.089886	0.895859
-44.595137	-7.964348	0.900864
-44.548421	-9.722588	0.905869
-45.283715	-3.526874	0.910874
-44.897388	3.118511	0.915878
-45.125364	-2.855648	0.920883
-44.982969	-9.015459	0.925888
-45.443960	-1.527055	0.930893
-44.987403	-11.841248	0.935898
-45.737081	-5.253617	0.940902
-46.246406	-6.310213	0.945907
-46.614902	-2.230662	0.950912
-46.794767	-3.787396	0.955917
-46.768204	-7.915229	0.960922
-47.509381	-7.486386	0.965926
-48.258406	-11.454006	0.970931
-47.919330	-8.938873	0.975936
-48.269775	-4.091134	0.980941
-48.488163	-14.363210	0.985946
-48.411655	-0.883398	0.990950
-48.686035	-4.905153	0.995955
-49.469207	-11.754692	1.000960
-49.838818	-0.863416	1.005965
-49.526429	-10.309150	1.010970
-49.878282	-10.670177	1.015974
-49.947685	-8.039248	1.020979
-49.484683	-10.248464	1.025984
-50.334972	-15.068959	1.030989
-51.248796	-5.719110	1.035994
-51.370234	2.918178	1.040998
-51.569860	-9.897474	1.046003
-51.550933	-4.692559	1.051008
-51.695365	-8.814965	1.056013
-51.567984	-10.124409	1.061018
-52.472852	-2.514545	1.066022
-52.748827	-4.748198	1.071027
-52.843817	-7.111872	1.076032
-53.103079	2.389274	1.081037
-53.232392	-4.193420	1.086042
-53.343035	6.618271	1.091046
-53.741697	-9.059889	1.096051
-54.370829	-7.126980	1.101056
-54.796594	2.611110	1.106061
-55.112165	-2.553487	1.111066
-55.095077	-4.145797	1.116070
-54.914559	-0.678519	1.121075
-54.886661	-10.343539	1.126080
-55.379360	0.185888	1.131085
-55.768136	-14.810933	1.136090
-56.090558	-9.912189	1.141094
-56.143650	-6.436022	1.146099
-55.844768	-1.822305	1.151104
-57.278098	2.166205	1.156109
-57.763624	-3.272559	1.161114
-57.765821	1.354512	1.166118
-57.767328	0.142779	1.171123
-57.597636	3.399521	1.176128
-57.898940	1.223539	1.181133
-57.740430	-2.857277	1.186138
-58.606728	5.141463	1.191142
-59.119677	-4.741042	1.196147
-59.205598	-9.021334	1.201152
-59.763345	-5.330366	1.206157
-59.364606	-0.610642	1.211162
-59.751216	-3.861972	1.216166
-59.720126	3.037403	1.221171
-60.390520	-6.586371	1.226176
-60.880711	-3.666520	1.231181
-61.017880	-18.460509	1.236186
-61.292964	5.448956	1.241190
-61.435372	-3.323742	1.246195
-61.053010	-0.629890	1.251200
-62.118994	4.569204	1.256205
-62.316158	-10.998861	1.261210
-62.534086	-3.092108	1.266214
-62.915143	-3.884798	1.271219
-62.576033	-2.103750	1.276224
-63.013265	-0.515786	1.281229
-62.961395	-5.298219	1.286234
-63.367148	-0.613393	1.291238
-64.223521	3.569650	1.296243
-64.480087	1.025535	1.301248
-64.541289	-3.010804	1.306253
-64.291452	-3.965991	1.311258
-64.570547	-0.804832	1.316262
-65.153562	7.339396	1.321267
-65.205513	-8.157408	1.326272
-65.685348	0.814709	1.331277
-65.534818	-9.073281	1.336282
-66.078427	-0.898485	1.341286
-67.064373	-2.884913	1.346291
-66.812353	-6.196420	1.351296
-67.229037	2.605597	1.356301
-67.081121	-10.988860	1.361306
-67.360538	3.208989	1.366310
-67.757039	7.306995	1.371315
-67.440199	-3.821350	1.376320
-68.069364	5.266668	1.381325
-68.682952	-5.090331	1.386330
-69.162208	5.573231	1.391334
-69.198970	-1.631194	1.396339
-68.998630	1.166210	1.401344
-69.220763	2.680664	1.406349
-68.929044	0.543027	1.411354
-69.525639	0.218784	1.416358
-70.018032	-2.748626	1.421363
-70.108713	-3.001352	1.426368
-70.917606	-0.114954	1.431373
-70.863542	-0.238718	1.436378
-71.099278	-1.109346	1.441382
-72.166852	-0.750172	1.446387
-71.769890	-2.328236	1.451392
-71.932111	-4.064109	1.456397
-72.086484	-11.303318	1.461402
-72.356787	3.470812	1.466406
-72.753678	7.219406	1.471411
-72.633272	-5.266223	1.476416
-73.061383	4.582171	1.481421
-73.384709	0.039078	1.486426
-74.007551	1.816240	1.491430
-74.106647	0.900487	1.496435
-74.025754	0.690189	1.501440
-74.272150	-7.657396	1.506445
-74.101896	-4.001151	1.511450
-75.018434	6.142041	1.516454
-75.669311	3.133192	1.521459
-75.356560	0.094601	1.526464
-75.582166	9.118550	1.531469
-75.487642	-2.483084	1.536474
-75.954926	5.722094	1.541478
-76.649098	1.561676	1.546483
-76.709857	2.290857	1.551488
-77.160057	6.973574	1.556493
-76.867534	-1.832475	1.561498
-77.388667	10.033468	1.566502
-77.345323	-0.681558	1.571507
-77.864469	10.730783	1.576512
-78.569415	10.130459	1.581517
-78.484476	1.230125	1.586522
-78.656940	5.121914	1.591526
-78.620804	6.604450	1.596531
-78.887388	-4.682227	1.601536
-79.659351	1.403535	1.606541
-79.704110	-6.137397	1.611546
-80.157262	6.543123	1.616550
-80.585337	5.186942	1.621555
-80.625970	5.766172	1.626560
-80.725500	11.264607	1.631565
-80.338768	6.311471	1.636570
-80.727710	3.155051	1.641574
-81.361180	8.937863	1.646579
-81.428843	-2.547123	1.651584
-81.755408	1.356767	1.656589
-81.906543	-2.150427	1.661594
-82.941239	4.709374	1.666598
-83.838837	4.752689	1.671603
-82.704960	-4.470542	1.676608
-83.274463	3.736961	1.681613
-83.459834	-5.386580	1.686618
-83.807148	4.089879	1.691622
-83.717481	-0.798073	1.696627
-83.786153	4.258945	1.701632
-84.338695	1.783779	1.706637
-84.970988	-3.776898	1.711642
-84.921687	-0.842988	1.716646
-85.252066	7.252494	1.721651
-85.148126	0.539017	1.726656
-85.279922	1.271280	1.731661
-85.504447	-4.098028	1.736666
-86.495998	-1.892169	1.741670
-86.745101	-5.152653	1.746675
-86.491717	0.923532	1.751680
-86.835747	5.114870	1.756685
-86.908811	-0.098766	1.761690
-87.791152	0.813051	1.766694
-88.346002	6.007025	1.771699
-88.203925	-7.390514	1.776704
-88.530172	-1.074677	1.781709
-88.432388	-3.254788	1.786714
-88.744506	-4.611622	1.791718
-88.723431	-1.710926	1.796723
-88.327204	-2.872300	1.801728
-89.114345	2.321861	1.806733
-89.565184	-10.180846	1.811738
-89.686938	0.252219	1.816742
-90.244116	-4.432109	1.821747
-90.961869	-10.780393	1.826752
-91.541382	0.178995	1.831757
-91.018075	-8.617911	1.836762
-91.516135	-1.624197	1.841766
-91.739435	-1.172186	1.846771
-91.771040	0.425168	1.851776
-91.824801	-5.927117	1.856781
-91.562322	-4.061551	1.861786
-91.981087	-6.067116	1.866790
-92.686925	2.119158	1.871795
-93.004488	-6.944797	1.876800
-93.077691	1.788691	1.881805
-93.301289	-3.052115	1.886810
-93.474327	-1.782393	1.891814
-94.281841	4.295445	1.896819
-94.758524	-3.201975	1.901824
-95.119951	5.336728	1.906829
-94.535985	-7.237116	1.911834
-94.893047	-2.439191	1.916838
-95.046531	3.380357	1.921843
-94.970593	-4.668765	1.926848
-95.522529	-4.493650	1.931853
-95.924080	-9.251899	1.936858
-96.438291	-0.120170	1.941862
-97.002701	-5.309260	1.946867
-96.711129	-10.490140	1.951872
-97.063476	-4.844663	1.956877
-96.913625	-11.188635	1.961882
-97.275144	-12.723765	1.966886
-97.949249	-2.125027	1.971891
-97.832591	-5.443914	1.976896
-98.446172	-3.509430	1.981901
-98.637024	-7.176592	1.986906
-98.430693	-2.649969	1.991910
-98.582069	1.255889	1.996915
-99.360360	-3.308306	2.006912
-98.800272	0.304332	2.016909
-98.473923	4.080358	2.026906
-98.331709	4.810668	2.036902
-97.397689	1.150686	2.046899
-97.235911	0.698368	2.056896
-96.134307	3.111089	2.066893
-95.733563	-3.814985	2.076890
-95.720364	4.046417	2.086886
-94.753375	-4.135833	2.096883
-94.239281	1.394484	2.106880
-94.021468	1.107155	2.116877
-93.680693	-3.848146	2.126874
-92.918060	0.537887	2.136870
-92.616159	-7.871885	2.146867
-91.762305	-2.266247	2.156864
-91.206950	-6.793154	2.166861
-91.034657	-2.381866	2.176858
-90.382543	-0.331366	2.186854
-89.786883	-1.961823	2.196851
-89.577455	-1.048813	2.206848
-88.809246	-1.245120	2.216845
-88.265540	-3.138060	2.226842
-88.296974	-6.639134	2.236838
-87.229550	2.239312	2.246835
-86.796935	0.781281	2.256832
-86.632439	3.262265	2.266829
-85.667173	2.565638	2.276826
-85.093732	1.686525	2.286822
-84.936808	7.007675	2.296819
-84.918840	6.366572	2.306816
-84.017051	1.444417	2.316813
-83.475878	-2.343345	2.326810
-82.475765	2.072121	2.336806
-82.005379	6.405000	2.346803
-82.013774	4.452737	2.356800
-81.697383	-2.217128	2.366797
-80.855172	3.524999	2.376794
-80.339698	7.028257	2.386790
-80.099955	9.680141	2.396787
-79.027131	4.378748	2.406784
-78.707489	1.426513	2.416781
-78.533772	0.821657	2.426778
-78.289688	0.737444	2.436774
-77.333269	-1.512715	2.446771
-76.780843	1.346220	2.456768
-75.949651	1.114984	2.466765
-75.965430	2.354756	2.476762
-75.766664	0.260303	2.486758
-75.035801	-2.742252	2.496755
-74.405444	0.064656	2.506752
-73.842064	0.734307	2.516749
-73.195938	-4.352574	2.526746
-72.930093	-5.094596	2.536742
-72.636535	-2.410331	2.546739
-71.491495	-7.677641	2.556736
-71.343203	-6.528269	2.566733
-71.055096	-6.774679	2.576730
-70.310136	-7.117495	2.586726
-69.756403	0.512918	2.596723
-69.674413	-4.700449	2.606720
-68.754999	-5.499533	2.616717
-68.345204	0.503890	2.626714
-68.022025	-1.701858	2.636710
-66.801917	2.474457	2.646707
-66.511974	-1.181994	2.656704
-66.310563	-6.626949	2.666701
-66.232674	-6.582672	2.676698
-65.287337	-8.252067	2.686694
-65.035021	-1.908403	2.696691
-64.492793	5.588771	2.706688
-63.238979	0.313326	2.716685
-63.133173	-1.959761	2.726682
-63.243898	-0.471905	2.736678
-63.008128	0.559248	2.746675
-62.014612	-2.754530	2.756672
-60.564655	0.902601	2.766669
-60.880505	-2.185050	2.776666
-60.506358	2.527129	2.786662
-60.194032	1.435585	2.796659
-58.762355	-1.410754	2.806656
-58.494701	-1.660889	2.816653
-58.268110	-11.978523	2.826650
-58.145218	-8.788825	2.836646
-57.364775	-7.155534	2.846643
-56.816914	-11.033115	2.856640
-56.631389	-6.144674	2.866637
-55.471997	-2.608556	2.876634
-55.434550	-4.611484	2.886630
-54.744743	-2.849372	2.896627
-54.035558	-1.337452	2.906624
-53.903449	-9.869270	2.916621
-53.723638	-5.274877	2.926618
-52.545452	-7.153545	2.936614
-52.487494	-5.368596	2.946611
-51.883623	-7.404668	2.956608
-50.662754	-8.682432	2.966605
-50.693065	-15.175929	2.976602
-50.530319	-8.390252	2.986598
-50.350234	-6.763640	2.996595
-49.500912	-1.322422	3.006592
-48.639116	-6.138363	3.016589
-47.799371	-4.725911	3.026586
-47.820682	-4.065731	3.036582
-47.860561	-2.460387	3.046579
-46.786158	-3.126077	3.056576
-46.275123	-7.452797	3.066573
-45.786734	-4.014206	3.076570
-44.820180	-5.349042	3.086566
-44.787168	-10.546590	3.096563
-44.415577	-6.386043	3.106560
-43.895448	-11.685599	3.116557
-43.210744	-4.039725	3.126554
-42.905659	-2.748962	3.136550
-42.612241	-6.809654	3.146547
-41.627540	-11.302344	3.156544
-41.165818	-10.623362	3.166541
-40.915735	-12.356628	3.176538
-39.898310	-13.635869	3.186534
-39.606384	-10.630255	3.196531
-39.770942	-7.892845	3.206528
-38.489639	-6.877753	3.216525
-38.238604	-4.291361	3.226522
-37.973932	-9.890634	3.236518
-37.215743	-6.705767	3.246515
-36.716623	-8.929584	3.256512
-36.412869	-6.243448	3.266509
-35.460090	-11.898581	3.276506
-35.028049	-7.808307	3.286502
-35.173270	-3.024937	3.296499
-34.558994	1.020145	3.306496
-33.445536	-7.508810	3.316493
-33.185021	-3.599570	3.326490
-32.861991	-8.677595	3.336486
-32.133245	-7.871327	3.346483
-31.682145	-6.733570	3.356480
-31.542179	-10.191108	3.366477
-30.329192	-6.342189	3.376474
-29.956916	0.027257	3.386470
-30.136426	-1.466723	3.396467
-29.657274	-6.673742	3.406464
-28.765086	-5.562201	3.416461
-28.128468	1.457195	3.426458
-27.238473	-8.491157	3.436454
-26.826252	-1.531222	3.446451
-26.831894	-6.060460	3.456448
-26.706730	-8.516949	3.466445
-25.962222	-8.839924	3.476442
-25.508222	-2.794419	3.486438
-24.249263	-3.592423	3.496435
-24.037408	-1.752936	3.506432
-24.062624	-5.097172	3.516429
-23.583456	-7.105082	3.526426
-22.507764	-8.212584	3.536422
-22.495889	-4.731040	3.546419
-21.417785	4.273500	3.556416
-20.660732	-5.743135	3.566413
-20.897670	-3.098854	3.576410
-20.675774	-2.071526	3.586406
-19.918586	-3.330390	3.596403
-19.318073	1.498030	3.606400
-18.262912	-2.052579	3.616397
-17.912656	-6.108457	3.626394
-17.705423	-3.652922	3.636390
-17.791185	-1.962526	3.646387
-16.758759	-7.203469	3.656384
-16.212179	-1.902582	3.666381
-15.654791	-7.538275	3.676378
-14.718641	-2.537027	3.686374
-14.608682	-4.339163	3.696371
-14.269187	-7.755649	3.706368
-14.281058	-1.888078	3.716365
-13.035838	-3.817354	3.726362
-12.755100	-9.065213	3.736358
-12.154214	-7.003451	3.746355
-11.457957	-7.708073	3.756352
-11.132391	-13.046340	3.766349
-10.890541	-11.518473	3.776346
-10.050961	-7.332081	3.786342
-9.588495	-12.128517	3.796339
-9.439304	-13.538223	3.806336
-8.765586	-9.829592	3.816333
-8.043029	-2.370373	3.826330
-7.708533	-3.630568	3.836326
-7.129978	-0.982030	3.846323
-6.491799	-1.643049	3.856320
-6.268441	-2.161873	3.866317
-5.944146	-0.759293	3.876314
-5.084310	6.687276	3.886310
-4.866336	9.529884	3.896307
-4.313719	7.661162	3.906304
-3.708936	10.263669	3.916301
-3.587340	24.754921	3.926298
-2.768424	35.349506	3.936294
-2.662162	38.520632	3.946291
-2.028410	52.271509	3.956288
-1.665634	69.292083	3.966285
-1.384760	85.942723	3.976282
-0.741325	99.428655	3.986278
-0.381688	125.048212	3.996275
0.000000	142.574900	4.001280
0.323862	147.198740	4.006285
0.378241	155.578883	4.011290
0.483154	158.971499	4.016294
0.832030	167.237367	4.021299
0.857863	188.831886	4.026304
0.805769	186.616578	4.031309
1.140902	182.792405	4.036314
0.714209	189.892982	4.041318
1.017704	187.990965	4.046323
1.132112	184.986764	4.051328
1.069772	184.873198	4.056333
1.360126	175.720095	4.061338
1.313595	191.597561	4.066342
1.209057	187.356406	4.071347
1.070320	185.082629	4.076352
1.042597	185.564808	4.081357
1.462915	188.484089	4.086362
1.128588	200.711744	4.091366
1.419006	189.863903	4.096371
1.214506	195.517923	4.101376
1.135051	189.062455	4.106381
1.393217	181.704315	4.111386
1.179221	185.449302	4.116390
1.325012	182.508775	4.121395
1.257395	187.514967	4.126400
0.738999	190.399460	4.131405
1.359524	183.961876	4.136410
1.329048	192.770100	4.141414
1.522972	189.121258	4.146419
1.429208	185.171560	4.151424
1.161529	186.212468	4.156429
1.279318	191.826142	4.161434
1.419884	189.451845	4.166438
1.088784	187.843566	4.171443
1.348514	199.526673	4.176448
1.536718	200.707581	4.181453
1.587228	190.345051	4.186458
1.435167	196.435182	4.191462
1.464966	195.082679	4.196467
1.502062	189.067506	4.201472
1.715438	190.456381	4.206477
1.598869	183.992458	4.211482
1.379216	190.875031	4.216486
1.506532	192.920090	4.221491
1.625978	194.425358	4.226496
1.319318	191.256052	4.231501
1.535062	191.294167	4.236506
1.477504	209.499275	4.241510
1.925071	208.521400	4.246515
1.695311	194.289346	4.251520
1.345192	198.807739	4.256525
1.672044	192.834173	4.261530
1.707134	216.380427	4.266534
2.077622	213.954240	4.271539
1.867253	202.615464	4.276544
1.812644	201.972941	4.281549
1.661358	186.755626	4.286554
1.728364	191.662368	4.291558
1.382463	193.305078	4.296563
1.499242	193.420755	4.301568
1.550432	201.520445	4.306573
1.902206	212.109880	4.311578
1.726358	228.355911	4.316582
1.866013	214.580870	4.321587
1.817270	220.708367	4.326592
1.698508	218.524419	4.331597
1.616571	217.426826	4.336602
1.716543	228.308191	4.341606
2.008096	224.370257	4.346611
1.926124	220.128120	4.351616
1.719736	223.849754	4.356621
1.816979	225.442766	4.361626
1.672486	223.581185	4.366630
2.092547	214.428288	4.371635
2.276766	222.288890	4.376640
1.836965	219.528208	4.381645
2.131820	222.730530	4.386650
2.004220	225.948738	4.391654
2.044699	212.569599	4.396659
1.857731	224.892062	4.401664
1.599990	229.728073	4.406669
1.816365	222.739736	4.411674
1.697381	225.046205	4.416678
2.114335	219.643995	4.421683
2.243496	228.160980	4.426688
1.772304	232.058286	4.431693
1.966648	223.299545	4.436698
1.838046	230.273422	4.441702
1.916915	215.928080	4.446707
2.081083	230.520572	4.451712
1.981067	226.777327	4.456717
2.209697	224.547298	4.461722
2.137540	225.248776	4.466726
2.253547	221.739715	4.471731
2.047541	221.365972	4.476736
1.701942	228.940557	4.481741
2.367586	234.354991	4.486746
2.046528	247.885865	4.491750
2.257523	246.492895	4.496755
2.347729	254.276531	4.501760
2.393175	247.432323	4.506765
2.729180	245.167343	4.511770
2.453423	232.879528	4.516774
2.439004	225.028766	4.521779
2.166188	222.985572	4.526784
1.861800	222.123926	4.531789
2.261356	219.434612	4.536794
2.238541	233.252347	4.541798
2.511674	241.885608	4.546803
2.209693	242.169691	4.551808
2.400579	250.474395	4.556813
2.550515	247.645849	4.561818
2.344316	248.203367	4.566822
2.498588	250.628381	4.571827
2.265389	249.274826	4.576832
2.455932	256.181658	4.581837
2.892992	249.717398	4.586842
2.265652	237.752230	4.591846
2.457622	236.423979	4.596851
2.634698	241.047488	4.601856
2.479660	238.863624	4.606861
2.193497	229.561062	4.611866
2.206346	251.016132	4.616870
2.646965	250.342514	4.621875
2.475422	261.982628	4.626880
2.507661	262.046395	4.631885
2.729809	254.301288	4.636890
2.487730	266.721120	4.641894
2.387700	256.287964	4.646899
2.406150	257.751945	4.651904
2.281158	254.780862	4.656909
2.822871	255.601114	4.661914
2.544929	261.323560	4.666918
2.641028	260.816513	4.671923
2.580970	253.410986	4.676928
2.600565	259.850024	4.681933
2.670268	253.642549	4.686938
2.244797	262.080502	4.691942
2.492557	257.070578	4.696947
2.736151	255.178473	4.701952
2.634001	263.295299	4.706957
2.720581	261.234225	4.711962
2.476797	264.093386	4.716966
3.004772	276.461488	4.721971
2.835367	273.995833	4.726976
2.708958	294.901944	4.731981
3.221964	277.863429	4.736986
2.575170	278.436285	4.741990
2.737858	286.325350	4.746995
2.936370	280.839310	4.752000
2.794648	292.991137	4.757005
3.315063	282.622564	4.762010
2.993351	280.205217	4.767014
2.948724	275.303104	4.772019
3.121549	250.577263	4.777024
2.561728	263.491741	4.782029
2.806693	270.067120	4.787034
2.858114	289.640763	4.792038
2.880512	283.526162	4.797043
3.133838	279.352215	4.802048
3.058990	282.531112	4.807053
3.245433	279.672835	4.812058
3.000917	284.279735	4.817062
2.910190	281.480181	4.822067
2.999757	281.284429	4.827072
3.223663	284.616717	4.832077
3.209182	282.291367	4.837082
2.893927	290.863034	4.842086
2.890250	286.867214	4.847091
3.330696	286.138566	4.852096
3.043231	280.085341	4.857101
3.158435	288.658938	4.862106
2.956654	290.510453	4.867110
3.274592	278.234405	4.872115
3.394164	284.663805	4.877120
2.860186	283.666518	4.882125
3.345563	276.855813	4.887130
3.295534	288.446423	4.892134
3.126287	290.853579	4.897139
3.229878	287.943899	4.902144
2.846385	293.812499	4.907149
3.001353	282.081838	4.912154
2.874828	284.310434	4.917158
2.965580	289.029751	4.922163
3.130581	284.466678	4.927168
2.663940	297.442914	4.932173
3.072549	308.842544	4.937178
2.913266	320.759708	4.942182
3.133040	325.559892	4.947187
3.025886	326.237569	4.952192
3.249101	324.227665	4.957197
3.436022	320.325978	4.962202
3.345666	322.715932	4.967206
3.053404	320.095181	4.972211
3.341129	321.321977	4.977216
3.236998	321.893381	4.982221
3.687295	321.579877	4.987226
3.536467	329.952062	4.992230
3.399105	326.230171	4.997235
3.087527	328.909350	5.002240
3.281836	345.450600	5.007245
3.826054	346.952836	5.012250
4.072297	351.276219	5.017254
3.570772	327.306230	5.022259
3.724921	328.003983	5.027264
3.257026	321.466357	5.032269
3.639745	314.255662	5.037274
3.352893	324.528427	5.042278
3.263638	324.291244	5.047283
3.274172	332.955805	5.052288
3.409325	342.302454	5.057293
3.612143	344.673267	5.062298
3.906177	345.928621	5.067302
3.937012	345.565187	5.072307
4.050191	351.455166	5.077312
3.647842	354.255745	5.082317
3.788415	346.442403	5.087322
3.379411	356.769359	5.092326
3.734905	353.420515	5.097331
3.701519	353.215718	5.102336
3.597522	355.821652	5.107341
3.758451	343.049989	5.112346
3.878768	352.825943	5.117350
3.895809	355.785197	5.122355
4.041596	353.174193	5.127360
3.848995	352.618057	5.132365
4.407017	354.299361	5.137370
3.685881	342.238147	5.142374
3.604985	329.973637	5.147379
4.005902	339.290484	5.152384
3.821315	355.351809	5.157389
3.947003	349.960093	5.162394
3.937602	357.194114	5.167398
3.989040	347.982198	5.172403
3.780623	347.423945	5.177408
3.707004	353.533315	5.182413
3.817715	355.494908	5.187418
3.496676	359.725352	5.192422
3.913592	355.664603	5.197427
3.933086	343.404179	5.202432
4.019253	354.113867	5.207437
4.352870	352.596387	5.212442
3.754108	349.411087	5.217446
4.029465	346.369350	5.222451
4.214951	349.437267	5.227456
4.148206	357.275756	5.232461
4.194817	341.636566	5.237466
3.750423	349.981794	5.242470
3.788628	348.357138	5.247475
3.812672	346.777848	5.252480
3.851513	351.860396	5.257485
4.077575	351.289398	5.262490
4.126635	348.875963	5.267494
4.214944	345.473682	5.272499
3.885154	349.541387	5.277504
3.926264	371.957123	5.282509
4.412255	369.332406	5.287514
4.558019	375.384932	5.292518
4.055886	368.951823	5.297523
4.390341	364.886769	5.302528
4.156416	362.392316	5.307533
4.287436	370.012566	5.312538
4.167134	371.437373	5.317542
4.291627	376.803726	5.322547
4.226837	375.607968	5.327552
4.544813	385.009027	5.332557
4.478272	375.280069	5.337562
4.301500	369.274587	5.342566
4.339185	366.521440	5.347571
4.362785	365.296443	5.352576
4.303634	370.894489	5.357581
4.301103	374.750534	5.362586
4.680183	382.323003	5.367590
4.473262	379.496101	5.372595
4.490808	362.838504	5.377600
3.991696	365.569661	5.382605
4.357431	376.104997	5.387610
4.228379	378.324750	5.392614
4.370528	382.185453	5.397619
4.581329	372.781764	5.402624
4.380230	388.616353	5.407629
4.584840	380.603932	5.412634
4.259344	385.833849	5.417638
4.585268	379.996332	5.422643
4.857204	387.572732	5.427648
4.605856	384.951905	5.432653
4.734650	383.802038	5.437658
4.753685	382.143454	5.442662
4.631333	380.283909	5.447667
4.833701	378.225353	5.452672
4.548417	377.810860	5.457677
4.625295	383.739226	5.462682
4.405140	384.987375	5.467686
4.331475	380.621073	5.472691
4.602650	379.443288	5.477696
4.318069	392.024774	5.482701
4.696197	379.310850	5.487706
4.122323	384.110850	5.492710
4.124475	391.735479	5.497715
4.500547	390.444022	5.502720
4.381751	406.524303	5.507725
4.596228	412.322542	5.512730
4.571888	417.264610	5.517734
4.748452	419.152159	5.522739
4.833321	411.377018	5.527744
4.615542	416.053136	5.532749
5.054845	409.394850	5.537754
5.090391	411.161100	5.542758
4.665923	411.998677	5.547763
4.767886	420.504879	5.552768
4.573903	415.969441	5.557773
4.916839	414.395947	5.562778
4.792454	413.378976	5.567782
4.773393	416.395133	5.572787
4.781816	416.116515	5.577792
4.688444	419.877893	5.582797
4.944709	409.976465	5.587802
4.903028	416.267844	5.592806
5.090299	411.519890	5.597811
4.950153	411.693900	5.602816
4.802623	420.181228	5.607821
5.146243	436.425523	5.612826
4.745414	457.050502	5.617830
5.144691	446.805876	5.622835
5.324652	445.784683	5.627840
5.185339	446.613721	5.632845
4.889836	429.725499	5.637850
4.826155	450.176039	5.642854
5.207468	450.533265	5.647859
5.325197	443.141622	5.652864
5.064454	457.949734	5.657869
5.411971	452.631563	5.662874
5.228693	451.048900	5.667878
5.058735	449.097969	5.672883
5.041786	449.233425	5.677888
4.817432	451.728469	5.682893
5.340730	453.299500	5.687898
5.002434	452.037134	5.692902
5.377822	451.784973	5.697907
5.441869	442.963223	5.702912
5.222556	452.198726	5.707917
5.341422	451.712571	5.712922
5.289532	452.699607	5.717926
5.145693	451.440168	5.722931
5.151977	446.092661	5.727936
5.085764	443.537863	5.732941
5.277259	445.810318	5.737946
4.988793	452.452400	5.742950
5.005122	458.090471	5.747955
5.479408	456.588761	5.752960
5.189398	455.663151	5.757965
5.328686	452.035924	5.762970
5.013954	455.333910	5.767974
5.496654	449.392654	5.772979
5.510237	447.366929	5.777984
5.086051	447.456152	5.782989
5.502301	460.389532	5.787994
5.667040	476.999165	5.792998
5.695605	464.736551	5.798003
5.242547	456.802605	5.803008
5.321573	464.271271	5.808013
5.539166	467.586885	5.813018
5.298427	480.526062	5.818022
5.807615	482.707632	5.823027
5.957339	476.051092	5.828032
5.642883	462.631644	5.833037
5.853730	455.078150	5.838042
5.467286	442.081501	5.843046
5.325794	439.501674	5.848051
5.491822	453.198545	5.853056
5.558015	471.802419	5.858061
5.948931	464.642789	5.863066
5.531943	468.524271	5.868070
5.833537	471.432678	5.873075
5.690828	453.121178	5.878080
5.498217	457.051147	5.883085
5.402998	462.653226	5.888090
5.628133	473.395831	5.893094
5.641812	474.419767	5.898099
5.411634	483.181500	5.903104
5.104698	485.533143	5.908109
5.804940	479.770360	5.913114
5.765502	487.775289	5.918118
5.747270	480.587497	5.923123
5.876371	481.849651	5.928128
5.593876	481.361480	5.933133
5.670675	482.617691	5.938138
5.582503	483.932401	5.943142
5.842642	489.574511	5.948147
5.974776	481.447545	5.953152
6.046051	486.600151	5.958157
6.344738	476.657713	5.963162
6.064514	487.106303	5.968166
5.650940	484.217102	5.973171
6.018761	480.733183	5.978176
5.906650	491.477180	5.983181
6.191355	480.989241	5.988186
5.996431	485.226462	5.993190
5.817081	485.361972	5.998195
5.939195	477.077612	6.003200
5.682199	486.208076	6.008205
5.819372	471.724573	6.013210
6.009021	483.188613	6.018214
5.492308	484.778531	6.023219
6.042788	500.771764	6.028224
5.897817	511.770654	6.033229
6.292402	516.309287	6.038234
6.064772	510.024647	6.043238
6.249303	506.553313	6.048243
6.296797	495.329889	6.053248
5.852006	497.237258	6.058253
6.175633	487.213919	6.063258
5.818065	491.821050	6.068262
5.811430	483.039202	6.073267
6.213908	481.370591	6.078272
5.856084	481.890471	6.083277
6.122158	483.972977	6.088282
6.026864	485.852072	6.093286
5.854334	485.879890	6.098291
6.215835	486.540354	6.103296
6.196454	477.577685	6.108301
6.279082	481.187584	6.113306
6.036644	479.124130	6.118310
5.920174	475.060307	6.123315
6.214133	483.785964	6.128320
5.950478	479.037472	6.133325
6.034837	484.817422	6.138330
6.145849	484.727640	6.143334
6.103264	481.522439	6.148339
6.171957	475.568426	6.153344
5.946992	478.986532	6.158349
6.126471	468.151342	6.163354
6.106578	477.540126	6.168358
6.196388	476.659762	6.173363
6.208146	476.440581	6.178368
6.149496	474.887995	6.183373
6.399972	478.234476	6.188378
5.988192	463.997188	6.193382
5.938052	447.953184	6.198387
6.058089	449.846545	6.203392
5.802597	455.739003	6.208397
6.074555	460.728717	6.213402
5.723266	455.183483	6.218406
5.640922	474.511523	6.223411
5.711277	472.749314	6.228416
5.688053	474.403150	6.233421
6.037654	475.836392	6.238426
5.985622	479.595675	6.243430
5.890776	477.281236	6.248435
6.068908	476.795527	6.253440
5.715504	477.648968	6.258445
6.151584	474.600128	6.263450
6.036823	480.730174	6.268454
5.716999	479.918233	6.273459
6.001218	481.031561	6.278464
6.019715	483.382793	6.283469
6.309947	474.747749	6.288474
5.956656	484.056765	6.293478
5.618643	481.085983	6.298483
5.551696	478.682660	6.303488
5.664484	473.983725	6.308493
5.856406	482.960717	6.313498
5.805036	484.120144	6.318502
5.954329	494.733435	6.323507
6.278360	509.664994	6.328512
6.061212	507.630502	6.333517
6.250126	488.889889	6.338522
6.041173	484.984054	6.343526
5.900559	482.671865	6.348531
6.125611	481.398304	6.353536
5.932272	479.719425	6.358541
6.043930	475.455613	6.363546
6.065991	484.230635	6.368550
5.966905	484.507766	6.373555
6.343942	481.440877	6.378560
6.333658	479.465869	6.383565
6.149967	486.817416	6.388570
6.092025	482.274034	6.393574
6.035978	483.808391	6.398579
6.239832	481.099145	6.403584
5.995497	478.076147	6.408589
6.338724	481.497453	6.413594
6.094112	483.047642	6.418598
5.846269	483.421237	6.423603
6.044905	478.392145	6.428608
6.023340	487.118941	6.433613
6.340326	476.933113	6.438618
5.952612	484.073545	6.443622
5.903638	482.240713	6.448627
5.935430	487.138975	6.453632
6.015185	487.751568	6.458637
6.270950	473.497665	6.463642
6.046297	471.330229	6.468646
6.149024	478.999422	6.473651
5.720691	456.928737	6.478656
5.819553	461.186372	6.483661
6.125068	470.936864	6.488666
5.955693	480.884403	6.493670
5.938185	473.238469	6.498675
6.453309	480.488306	6.503680
5.879131	466.245544	6.508685
6.033425	460.015296	6.513690
5.452509	459.818677	6.518694
5.632615	478.710953	6.523699
5.961840	481.616957	6.528704
5.732365	479.405720	6.533709
6.200197	484.490488	6.538714
6.134897	479.273227	6.543718
5.835836	482.473111	6.548723
6.285142	480.156183	6.553728
6.024375	480.938239	6.558733
6.054552	478.056467	6.563738
6.113932	483.016070	6.568742
6.200808	477.953387	6.573747
6.070457	478.943550	6.578752
5.766583	491.992651	6.583757
6.076888	472.754790	6.588762
5.938231	488.247808	6.593766
5.981833	485.796576	6.598771
6.129431	484.598793	6.603776
5.854201	487.161667	6.608781
6.099793	482.569601	6.613786
6.191824	484.075095	6.618790
5.948785	482.283279	6.623795
6.116220	478.511274	6.628800
5.781107	486.163578	6.633805
5.799746	477.117257	6.638810
5.865366	483.806492	6.643814
6.107928	481.888087	6.648819
6.253045	481.891722	6.653824
6.072087	484.462863	6.658829
6.389013	472.130983	6.663834
5.925223	459.044906	6.668838
5.910980	456.038671	6.673843
5.871405	448.272869	6.678848
5.736216	463.305094	6.683853
5.955379	466.799433	6.688858
6.138072	467.391626	6.693862
5.878971	469.804216	6.698867
6.378261	476.119115	6.703872
5.528987	465.817187	6.708877
5.566108	471.268294	6.713882
6.009919	477.596130	6.718886
5.949434	477.546192	6.723891
6.165532	468.747597	6.728896
6.102970	486.543591	6.733901
6.081787	485.745148	6.738906
6.099823	475.693681	6.743910
5.884888	485.645413	6.748915
6.091617	482.415306	6.753920
6.071145	489.805541	6.758925
6.012500	488.884834	6.763930
5.845708	489.165479	6.768934
6.106076	489.347369	6.773939
6.314130	488.583785	6.778944
5.995306	490.410501	6.783949
5.965567	473.174912	6.788954
5.737511	476.482624	6.793958
5.846477	486.841903	6.798963
6.116835	488.825426	6.803968
5.931336	489.328018	6.808973
6.166379	483.143592	6.813978
6.022104	490.211746	6.818982
6.043120	495.777815	6.823987
6.268446	480.666967	6.828992
5.852615	478.321218	6.833997
5.638220	472.436975	6.839002
5.949541	484.894205	6.844006
6.048388	486.936716	6.849011
6.199850	485.316380	6.854016
6.122050	492.008450	6.859021
6.165238	488.905869	6.864026
6.062701	475.876190	6.869030
5.678097	460.090621	6.874035
5.976527	469.710067	6.879040
6.157433	487.710052	6.884045
6.295590	479.725555	6.889050
6.128659	466.476252	6.894054
5.707066	457.841278	6.899059
5.719635	457.671298	6.904064
5.892904	473.820899	6.909069
5.973783	477.203752	6.914074
6.116519	491.041269	6.919078
6.177116	484.570775	6.924083
6.468905	469.740994	6.929088
6.192429	463.646014	6.934093
6.060067	457.778582	6.939098
6.002541	460.275209	6.944102
5.829036	460.821005	6.949107
5.866074	459.048725	6.954112
5.713771	466.137340	6.959117
5.889671	459.764587	6.964122
6.049840	466.362774	6.969126
5.536533	456.082379	6.974131
5.815641	471.649470	6.979136
5.615164	484.301565	6.984141
6.238891	488.379150	6.989146
6.188075	486.141485	6.994150
6.066268	480.578765	6.999155
6.023662	484.117047	7.004160
5.706381	486.482244	7.009165
6.084582	486.444519	7.014170
6.233598	494.282475	7.019174
6.071859	493.937704	7.024179
6.449430	484.309585	7.029184
5.939506	480.405439	7.034189
5.689050	466.524470	7.039194
5.769807	478.400427	7.044198
6.114598	485.844040	7.049203
6.364811	481.918808	7.054208
6.259399	474.204153	7.059213
6.480581	464.733173	7.064218
6.062815	462.442016	7.069222
5.672199	462.796824	7.074227
5.945544	460.252101	7.079232
6.178621	456.087578	7.084237
5.871346	462.784482	7.089242
5.890228	464.233808	7.094246
5.773790	458.525163	7.099251
6.046764	453.028508	7.104256
5.584039	462.616120	7.109261
5.858187	477.390143	7.114266
6.110928	483.695155	7.119270
6.085564	478.046016	7.124275
6.334015	470.399852	7.129280
5.869378	470.419996	7.134285
6.123023	453.625917	7.139290
6.037130	458.198906	7.144294
6.079137	461.679560	7.149299
6.348467	454.355161	7.154304
5.950629	465.649669	7.159309
5.911310	451.105621	7.164314
6.023913	456.593559	7.169318
5.694785	465.084933	7.174323
5.662206	457.586350	7.179328
5.816079	466.053394	7.184333
5.998203	473.259503	7.189338
5.905549	482.325060	7.194342
6.108735	493.089468	7.199347
6.014816	485.856188	7.204352
5.894106	489.815306	7.209357
6.022696	485.781350	7.214362
6.136219	486.998723	7.219366
5.911833	481.870361	7.224371
5.890263	482.936248	7.229376
6.073420	486.978843	7.234381
6.375984	476.915386	7.239386
6.074986	462.277508	7.244390
5.921735	464.411293	7.249395
5.907004	460.546516	7.254400
5.793108	465.366278	7.259405
5.792179	462.959327	7.264410
5.959487	487.182284	7.269414
6.267050	479.769055	7.274419
6.187893	468.383688	7.279424
5.859450	470.083724	7.284429
6.008382	455.679987	7.289434
5.528526	460.225858	7.294438
5.882107	472.245684	7.299443
6.006772	475.116492	7.304448
5.887050	487.165764	7.309453
5.932051	481.316907	7.314458
5.929802	484.104340	7.319462
6.204283	483.356397	7.324467
6.104905	484.073051	7.329472
5.894350	486.750328	7.334477
5.943313	487.041621	7.339482
6.365461	490.721795	7.344486
5.737362	493.308370	7.349491
5.951343	490.913584	7.354496
5.770940	497.437344	7.359501
5.739359	489.064958	7.364506
5.819804	494.703476	7.369510
5.781146	493.857803	7.374515
6.211357	494.588194	7.379520
6.063794	496.092712	7.384525
5.784454	493.379213	7.389530
6.105237	498.529777	7.394534
5.947997	497.760178	7.399539
6.213532	487.237520	7.404544
5.825553	495.100263	7.409549
6.213784	491.050939	7.414554
6.064984	498.583989	7.419558
5.953170	498.011707	7.424563
6.202035	492.933641	7.429568
5.928649	486.311639	7.434573
5.993227	490.746250	7.439578
5.994645	492.453038	7.444582
6.121971	495.126267	7.449587
6.018119	485.046432	7.454592
6.114861	488.682215	7.459597
5.981089	480.795831	7.464602
6.229846	488.024263	7.469606
5.917656	493.541313	7.474611
6.197749	481.731764	7.479616
5.729602	491.864554	7.484621
5.714149	494.846976	7.489626
5.743287	490.663722	7.494630
6.185777	483.333922	7.499635
6.136501	482.917445	7.504640
6.047755	488.297835	7.509645
5.774990	491.920804	7.514650
5.888360	489.854474	7.519654
5.664055	494.830074	7.524659
5.842804	483.821928	7.529664
5.859279	489.238571	7.534669
6.015290	483.281344	7.539674
6.033951	485.705368	7.544678
6.039003	483.184940	7.549683
6.364808	488.077337	7.554688
6.077237	492.082636	7.559693
6.266977	478.481804	7.564698
6.042439	485.088054	7.569702
5.788945	492.745988	7.574707
6.063043	485.865983	7.579712
5.880352	489.784845	7.584717
6.193905	487.675895	7.589722
6.206384	490.199415	7.594726
5.791740	495.962147	7.599731
6.253870	481.564738	7.604736
5.900397	497.221805	7.609741
5.989476	491.696188	7.614746
5.819552	497.681845	7.619750
5.893636	496.341322	7.624755
6.039565	485.528648	7.629760
5.718093	496.800271	7.634765
5.739703	490.601849	7.639770
5.646789	495.267773	7.644774
5.546802	487.641016	7.649779
5.994923	484.882046	7.654784
5.884762	495.227689	7.659789
5.992959	486.619624	7.664794
6.013664	483.390128	7.669798
5.939664	485.600977	7.674803
6.102854	485.704432	7.679808
6.027362	494.650329	7.684813
5.999041	481.019495	7.689818
6.103756	486.635047	7.694822
5.868820	494.296420	7.699827
6.436358	487.640152	7.704832
6.198510	493.322299	7.709837
6.075826	493.881783	7.714842
6.120085	494.589057	7.719846
6.001622	497.380344	7.724851
5.913695	493.851908	7.729856
5.801728	489.677417	7.734861
5.822281	486.357565	7.739866
5.927031	490.002481	7.744870
5.490080	498.248083	7.749875
5.848014	500.475028	7.754880
5.976006	505.016362	7.759885
5.695981	497.589124	7.764890
6.066154	509.394289	7.769894
6.116837	523.058619	7.774899
6.374223	508.265085	7.779904
5.900931	497.431800	7.784909
5.918461	494.220589	7.789914
5.842512	495.230754	7.794918
5.792199	491.592486	7.799923
5.959437	510.487327	7.804928
6.234605	526.592481	7.809933
5.979402	510.955342	7.814938
5.848728	503.168288	7.819942
5.832881	519.209930	7.824947
6.316169	517.175091	7.829952
5.952145	517.182323	7.834957
5.979603	510.111275	7.839962
6.187234	503.597678	7.844966
6.101087	498.008918	7.849971
6.005334	489.720568	7.854976
5.582027	492.311713	7.859981
6.252332	508.900811	7.864986
6.055045	494.031222	7.869990
5.950314	491.035622	7.874995
5.961804	481.635666	7.880000
5.982940	492.772999	7.885005
5.909960	489.924291	7.890010
6.124774	496.812609	7.895014
5.952324	501.192934	7.900019
6.331121	488.428884	7.905024
6.074448	495.790152	7.910029
6.120327	493.403862	7.915034
5.887928	496.901744	7.920038
5.784100	495.735134	7.925043
6.334248	491.141180	7.930048
5.797209	493.488696	7.935053
5.990843	481.018367	7.940058
6.012633	484.133349	7.945062
6.303172	488.134482	7.950067
6.183379	490.064207	7.955072
5.678103	494.139696	7.960077
5.835180	492.959287	7.965082
5.944425	487.876122	7.970086
6.104914	496.545742	7.975091
6.180472	489.456082	7.980096
5.679511	497.537835	7.985101
5.682048	493.714394	7.990106
5.715863	499.062455	7.995110
5.974985	518.067597	8.000115
6.359310	519.110856	8.005133
5.901256	507.128354	8.010150
6.088937	502.325610	8.015168
6.183107	503.740068	8.020186
5.813522	496.689222	8.025203
6.373527	492.259047	8.030221
6.079123	497.839323	8.035238
6.148784	496.543863	8.040256
6.011631	498.143662	8.045274
5.792021	491.444138	8.050291
6.315595	488.344703	8.055309
5.963612	496.697303	8.060326
5.909874	502.278276	8.065344
6.023770	495.159968	8.070362
5.840425	493.436556	8.075379
6.333014	488.196740	8.080397
6.051733	497.799745	8.085414
5.945232	492.482373	8.090432
6.138551	487.743656	8.095450
6.048923	495.429628	8.100467
5.993723	491.750886	8.105485
5.930388	504.223302	8.110502
6.184444	519.019773	8.115520
6.120654	518.155633	8.120538
6.394008	524.432593	8.125555
6.299528	503.768849	8.130573
6.188459	497.403488	8.135590
6.151844	499.034274	8.140608
6.130782	493.675984	8.145626
6.102460	496.447045	8.150643
6.243976	483.498214	8.155661
6.393541	485.447749	8.160678
6.167417	494.353874	8.165696
6.497406	484.625172	8.170714
5.923432	493.369622	8.175731
6.546915	485.835660	8.180749
6.259212	498.155474	8.185766
5.989060	492.171945	8.190784
6.547996	490.637997	8.195802
6.062293	495.048855	8.200819
6.445464	495.583627	8.205837
6.213621	494.985488	8.210854
6.233304	490.685335	8.215872
6.085064	486.770444	8.220890
5.754520	500.891318	8.225907
6.008735	487.714979	8.230925
6.091259	486.374283	8.235942
6.213738	490.795249	8.240960
6.265266	488.606401	8.245978
6.151181	497.647901	8.250995
6.107162	487.546122	8.256013
6.145358	497.907386	8.261030
6.122644	505.888363	8.266048
6.471429	514.536122	8.271066
6.415812	514.677053	8.276083
6.367553	499.525739	8.281101
6.159294	490.288496	8.286118
6.004361	493.327354	8.291136
6.249085	509.195953	8.296154
6.414508	520.905357	8.301171
6.514502	515.087872	8.306189
6.289616	500.443724	8.311206
6.126768	497.625264	8.316224
6.497461	514.836296	8.321242
6.189262	516.454973	8.326259
6.257989	514.343976	8.331277
6.546328	525.008694	8.336294
6.414367	514.597860	8.341312
6.508169	503.182790	8.346330
5.984059	507.455337	8.351347
6.508416	522.295234	8.356365
6.449481	522.681382	8.361382
5.945006	508.998222	8.366400
6.389103	511.251326	8.371418
6.185528	529.342057	8.376435
6.262072	520.486344	8.381453
6.441799	535.704953	8.386470
6.172792	531.172495	8.391488
6.265038	525.301371	8.396506
6.500433	527.254808	8.401523
6.383177	526.757369	8.406541
6.867063	529.286937	8.411558
6.841739	527.834971	8.416576
6.595749	519.665498	8.421594
6.017774	520.445643	8.426611
6.630228	520.699356	8.431629
6.357453	518.687818	8.436646
6.250677	522.711551	8.441664
6.151876	521.983711	8.446682
6.255207	528.003414	8.451699
6.319933	522.392146	8.456717
6.621628	527.165899	8.461734
6.253531	530.608344	8.466752
6.208073	527.149815	8.471770
6.399773	530.284027	8.476787
6.763439	528.497981	8.481805
6.987647	526.046495	8.486822
6.347826	530.963559	8.491840
6.510340	525.087295	8.496858
6.694329	524.923017	8.501875
6.813576	524.678520	8.506893
6.825634	522.049385	8.511910
6.662704	524.455170	8.516928
6.938193	518.891674	8.521946
6.664809	511.746943	8.526963
6.382919	500.596827	8.531981
6.413900	498.301940	8.536998
6.393190	518.864165	8.542016
6.573741	514.027758	8.547034
6.696005	531.206329	8.552051
6.795542	517.157807	8.557069
6.513775	504.226693	8.562087
6.302441	509.848331	8.567104
6.673501	521.084346	8.572122
6.535081	524.922191	8.577139
6.610653	527.421347	8.582157
6.745342	525.135462	8.587175
6.560432	527.695074	8.592192
6.663104	520.369965	8.597210
7.013914	525.633778	8.602227
6.701131	508.696467	8.607245
6.605473	496.511651	8.612263
6.359007	494.801447	8.617280
6.341609	505.565003	8.622298
6.428348	524.612701	8.627315
6.727299	533.225222	8.632333
6.773803	525.260246	8.637351
6.351269	522.253304	8.642368
6.619624	524.309936	8.647386
7.016192	527.816886	8.652403
6.509794	521.826996	8.657421
6.502867	525.650548	8.662439
6.299354	538.865247	8.667456
6.658963	523.782975	8.672474
6.371957	531.540033	8.677491
6.543725	526.623979	8.682509
6.791727	531.469613	8.687527
6.347582	533.474360	8.692544
6.573693	523.357352	8.697562
6.621356	534.355806	8.702579
6.749098	545.146534	8.707597
6.803278	538.619550	8.712615
6.888583	545.497500	8.717632
6.797673	541.737657	8.722650
6.772609	535.429294	8.727667
6.314201	530.994730	8.732685
7.060110	533.999181	8.737703
6.935685	550.737948	8.742720
7.050163	546.564199	8.747738
6.806970	540.849001	8.752755
7.183073	525.959454	8.757773
7.043148	527.614240	8.762791
6.836651	530.686249	8.767808
6.855757	527.259742	8.772826
6.750059	522.955540	8.777843
6.412968	524.044001	8.782861
6.784996	525.845687	8.787879
6.644104	527.053223	8.792896
6.890129	523.419665	8.797914
6.945512	526.227851	8.802931
6.862519	527.365568	8.807949
6.795634	522.266216	8.812967
6.487129	527.216992	8.817984
6.944341	543.069729	8.823002
6.918366	540.373665	8.828019
7.045850	542.629402	8.833037
7.336553	541.427641	8.838055
6.999065	534.829305	8.843072
6.793192	526.437254	8.848090
6.776490	521.165234	8.853107
6.412277	522.547142	8.858125
6.818043	533.792181	8.863143
6.753844	551.080385	8.868160
6.931485	545.553356	8.873178
6.757802	548.631942	8.878195
6.890990	558.502550	8.883213
7.063687	552.818080	8.888231
6.874317	548.745428	8.893248
6.993247	548.663965	8.898266
7.088156	556.289884	8.903283
7.092663	549.801434	8.908301
7.024162	552.886814	8.913319
6.832541	563.064342	8.918336
6.758867	551.676575	8.923354
6.906597	553.219955	8.928371
6.747664	563.275739	8.933389
7.177362	550.373024	8.938407
7.019967	554.591749	8.943424
7.210887	541.376833	8.948442
6.930456	548.734807	8.953459
6.742978	542.751936	8.958477
6.912375	550.672781	8.963495
6.561795	552.117980	8.968512
6.623741	558.686440	8.973530
6.847236	562.734031	8.978547
7.079501	579.312000	8.983565
7.044230	581.138031	8.988583
6.904955	576.389011	8.993600
6.949833	579.176508	8.998618
7.188860	582.959345	9.003635
7.115874	580.728902	9.008653
6.914443	582.180506	9.013671
7.067963	577.820177	9.018688
7.010521	569.569852	9.023706
7.126044	573.055837	9.028723
7.306584	575.250237	9.033741
7.062830	572.296746	9.038759
7.037255	575.049848	9.043776
7.366589	581.935237	9.048794
7.424418	577.530719	9.053811
7.292889	585.270915	9.058829
7.254431	576.624359	9.063847
6.920602	583.605981	9.068864
7.166206	582.205991	9.073882
7.222193	582.504413	9.078899
7.120306	587.406625	9.083917
7.300487	578.351250	9.088935
7.001404	581.137440	9.093952
7.272446	584.861633	9.098970
7.477222	576.153541	9.103987
7.273034	582.739115	9.109005
7.240913	574.055490	9.114023
6.985135	577.208498	9.119040
7.041464	576.988789	9.124058
7.213049	580.956994	9.129075
7.167030	591.098620	9.134093
7.524970	579.823207	9.139111
7.156972	579.606247	9.144128
7.099265	577.493739	9.149146
7.170636	578.389573	9.154163
6.987618	580.631579	9.159181
7.239301	580.858032	9.164199
7.086159	579.907903	9.169216
7.012716	577.731470	9.174234
7.238460	572.634231	9.179251
7.127592	579.351191	9.184269
7.401988	588.513835	9.189287
7.260501	607.835632	9.194304
7.199779	601.684515	9.199322
7.524044	603.501403	9.204339
7.399910	613.423119	9.209357
7.661567	607.144212	9.214375
7.142090	597.698417	9.219392
7.042260	597.253402	9.224410
7.294113	600.090284	9.229427
7.235650	613.785917	9.234445
7.650348	611.501680	9.239463
7.426583	613.005210	9.244480
7.582987	606.825223	9.249498
7.397781	606.963205	9.254515
7.366684	610.432338	9.259533
7.598108	608.205811	9.264551
7.725891	609.690495	9.269568
7.364140	594.590804	9.274586
7.341398	590.820054	9.279603
7.162314	612.600479	9.284621
7.398788	612.601119	9.289639
7.423622	613.564698	9.294656
7.239541	610.085800	9.299674
7.643823	607.006687	9.304691
7.370023	613.878783	9.309709
7.520532	608.024160	9.314727
7.764843	614.957893	9.319744
7.687274	617.121816	9.324762
7.687290	616.800218	9.329779
7.728881	615.004901	9.334797
7.643955	603.771705	9.339815
7.352225	592.864672	9.344832
7.062798	594.089920	9.349850
7.526462	603.675139	9.354867
7.274157	605.071000	9.359885
7.584885	600.304343	9.364903
7.521253	613.544759	9.369920
7.441069	613.295099	9.374938
7.668662	615.915937	9.379955
7.668528	611.677689	9.384973
7.862384	612.184961	9.389991
8.086799	610.697144	9.395008
7.758206	607.511845	9.400026
7.853968	592.169476	9.405043
7.563794	593.886744	9.410061
7.891316	587.901052	9.415079
7.586396	582.316525	9.420096
7.776473	590.141649	9.425114
7.531385	578.053555	9.430131
7.597274	582.793543	9.435149
7.808531	585.621792	9.440167
7.680331	584.493135	9.445184
7.508743	578.977470	9.450202
7.605856	581.032744	9.455219
7.650396	585.288309	9.460237
7.861291	578.785354	9.465255
7.799998	581.148925	9.470272
7.836551	586.988188	9.475290
7.486267	576.187509	9.480307
7.495895	590.946774	9.485325
7.309336	580.384318	9.490343
7.721404	600.571661	9.495360
7.867982	611.829757	9.500378
8.147874	603.741257	9.505395
7.319096	599.469768	9.510413
7.437042	597.691926	9.515431
7.589108	607.008884	9.520448
7.458204	608.382871	9.525466
8.000017	606.982251	9.530483
7.453332	618.995857	9.535501
7.818993	610.367003	9.540519
7.500563	606.446605	9.545536
7.792073	618.684774	9.550554
8.210187	612.819889	9.555571
7.505672	611.200874	9.560589
7.663741	614.611520	9.565607
7.770624	614.294665	9.570624
8.054229	618.430933	9.575642
8.290303	610.754186	9.580659
7.820871	613.772711	9.585677
7.911525	615.414321	9.590695
7.785365	615.337225	9.595712
7.674125	618.473590	9.600730
7.916643	616.013153	9.605747
7.839926	612.741462	9.610765
7.996435	606.402609	9.615783
8.208289	610.240147	9.620800
7.800189	617.869474	9.625818
8.054846	608.172656	9.630835
8.003530	619.326726	9.635853
8.141562	617.396943	9.640871
8.193065	615.565342	9.645888
7.977626	613.696453	9.650906
8.209202	613.789631	9.655923
8.002243	619.153908	9.660941
8.095932	612.691605	9.665959
7.874527	603.924747	9.670976
7.804241	612.903750	9.675994
7.906847	611.417207	9.681011
7.876387	610.414874	9.686029
7.996330	612.305161	9.691047
7.824736	610.305005	9.696064
8.195627	615.427540	9.701082
7.727825	606.734551	9.706099
7.491449	621.607213	9.711117
7.898327	615.871345	9.716135
8.121347	606.935623	9.721152
7.567570	616.624963	9.726170
8.282934	610.138059	9.731187
8.039545	622.248088	9.736205
7.866025	619.979370	9.741223
8.379550	613.309366	9.746240
8.081823	621.368027	9.751258
8.043598	607.269800	9.756275
7.919847	622.986159	9.761293
7.904253	612.209950	9.766311
8.003543	613.836352	9.771328
7.853728	613.581688	9.776346
8.051610	614.044201	9.781363
8.257319	625.918066	9.786381
8.571318	624.803577	9.791399
8.335362	620.232748	9.796416
8.070523	616.074550	9.801434
8.478022	610.994837	9.806451
8.345030	608.836527	9.811469
8.139556	618.964224	9.816487
8.218693	615.743491	9.821504
8.007591	614.315587	9.826522
8.304872	610.800481	9.831539
8.241478	609.973669	9.836557
8.218513	606.221653	9.841575
8.008046	607.656843	9.846592
7.570326	611.397430	9.851610
8.143902	613.827521	9.856627
8.665589	629.216550	9.861645
8.296383	625.726771	9.866663
8.225664	617.828793	9.871680
8.020849	615.482192	9.876698
7.960544	623.362572	9.881715
7.936598	637.991623	9.886733
7.888079	637.258009	9.891751
8.434347	646.321735	9.896768
8.186783	645.632891	9.901786
8.333207	641.824668	9.906803
8.218377	649.762119	9.911821
8.208109	649.722914	9.916839
8.463463	646.621017	9.921856
8.123222	659.808070	9.926874
8.496124	644.352834	9.931891
8.188764	645.014358	9.936909
8.207073	642.157213	9.941927
8.567007	637.107020	9.946944
8.231873	650.206217	9.951962
8.428619	641.234474	9.956979
8.333451	648.387222	9.961997
8.339351	643.931838	9.967015
8.410927	641.649301	9.972032
8.301909	654.486663	9.977050
8.355968	638.582293	9.982067
8.410872	656.779967	9.987085
8.296869	648.163202	9.992103
8.420253	643.883234	9.997120
8.463141	648.092833	10.002138
8.466953	641.382032	10.007155
8.047965	638.414635	10.012173
8.028714	649.116791	10.017191
8.386555	662.537834	10.022208
8.397802	670.699679	10.027226
8.726429	671.647993	10.032243
8.963489	668.533373	10.037261
8.699452	662.521207	10.042279
8.700927	644.369379	10.047296
8.182924	652.447998	10.052314
8.233724	642.437890	10.057331
8.613240	652.342959	10.062349
8.186697	673.570980	10.067367
8.846588	672.725570	10.072384
8.707309	669.893334	10.077402
8.619517	666.825815	10.082419
8.749138	666.165845	10.087437
8.621556	660.273595	10.092455
8.622362	641.224299	10.097472
8.166637	651.205082	10.102490
8.235295	659.718808	10.107507
8.219204	670.732247	10.112525
8.365064	674.155164	10.117543
8.519873	669.118063	10.122560
8.975567	670.385078	10.127578
8.765816	670.097821	10.132595
8.784704	674.013782	10.137613
8.731687	672.445136	10.142631
8.787114	670.405017	10.147648
8.565804	673.286802	10.152666
8.426834	678.274509	10.157683
8.763750	664.113322	10.162701
8.614476	664.951413	10.167719
9.151885	665.765948	10.172736
8.510046	673.727297	10.177754
8.666485	676.739433	10.182771
8.713596	670.724950	10.187789
8.503880	674.846865	10.192807
8.913976	666.788933	10.197824
8.826393	665.955888	10.202842
8.872062	673.281770	10.207859
8.668706	663.304287	10.212877
8.712097	666.114681	10.217895
9.071953	663.097045	10.222912
8.789888	664.637004	10.227930
8.907148	664.217255	10.232947
8.735353	663.796162	10.237965
8.523187	669.716795	10.242983
8.845520	666.177058	10.248000
8.806093	664.736469	10.253018
8.796028	667.257309	10.258035
8.771828	659.001628	10.263053
8.725309	670.857062	10.268071
8.839969	665.132558	10.273088
8.792551	666.237624	10.278106
8.798342	666.729191	10.283123
9.088699	663.505754	10.288141
8.872300	669.465669	10.293159
8.757908	663.031109	10.298176
8.922011	664.951490	10.303194
8.812444	668.420639	10.308211
8.622267	665.887759	10.313229
8.663852	668.563815	10.318247
8.833100	662.688943	10.323264
8.831936	680.730193	10.328282
8.864749	692.554003	10.333299
9.036069	698.201316	10.338317
8.995093	701.657933	10.343335
8.980617	689.825249	10.348352
8.943176	702.907476	10.353370
9.213919	707.089202	10.358387
9.392063	693.473541	10.363405
8.953141	685.960889	10.368423
9.021487	671.360340	10.373440
9.080431	679.291076	10.378458
8.963511	672.544352	10.383475
9.033868	662.865617	10.388493
8.660693	677.819841	10.393511
8.675404	687.745974	10.398528
9.047467	700.021064	10.403546
8.740450	707.491973	10.408563
9.189641	697.574511	10.413581
9.031390	701.175344	10.418599
9.108438	696.658560	10.423616
9.517662	696.936482	10.428634
9.144097	701.961469	10.433651
9.376198	695.523454	10.438669
9.057839	705.515774	10.443687
9.287819	706.435940	10.448704
9.324586	693.144066	10.453722
9.016052	702.913905	10.458739
9.392368	702.369767	10.463757
9.331786	710.349837	10.468775
9.150188	694.498998	10.473792
9.073917	696.926088	10.478810
9.136003	699.142089	10.483827
9.459967	697.912567	10.488845
9.315458	702.366978	10.493863
9.142478	689.076377	10.498880
9.033878	685.661140	10.503898
9.311421	690.698771	10.508915
9.486222	699.360681	10.513933
9.258120	693.725207	10.518951
9.130060	687.918453	10.523968
8.813633	682.553893	10.528986
8.928167	696.145955	10.534003
9.430011	692.517041	10.539021
9.554590	697.266243	10.544039
9.283428	700.772393	10.549056
9.205988	697.638590	10.554074
9.050828	700.380301	10.559091
9.437041	695.680047	10.564109
9.035683	699.782919	10.569127
9.404694	705.527018	10.574144
9.413034	701.200340	10.579162
9.323963	697.520071	10.584179
9.531425	699.089990	10.589197
8.982491	702.072880	10.594215
9.125476	711.126656	10.599232
9.440367	701.333394	10.604250
9.058179	703.166692	10.609267
9.427263	699.556216	10.614285
9.320655	711.609022	10.619303
9.465364	699.564941	10.624320
9.104336	699.300371	10.629338
9.304984	709.599642	10.634355
9.339835	723.116346	10.639373
9.536823	727.487446	10.644391
9.486327	730.386229	10.649408
9.664499	734.577780	10.654426
9.552978	732.400741	10.659443
9.763241	734.826449	10.664461
9.520102	715.318274	10.669479
9.565572	712.745577	10.674496
9.510626	703.580845	10.679514
9.175196	709.156572	10.684531
9.330337	720.830628	10.689549
9.524353	729.385443	10.694567
9.348601	725.076644	10.699584
9.642236	731.233212	10.704602
9.529379	733.628573	10.709619
9.913064	728.935026	10.714637
9.808288	737.575935	10.719655
9.877546	734.024548	10.724672
9.924576	721.758056	10.729690
9.639189	723.866255	10.734707
9.775365	700.207336	10.739725
9.714486	698.118760	10.744743
9.549744	699.758973	10.749760
9.821227	694.853715	10.754778
9.617778	699.678495	10.759795
9.646438	698.031758	10.764813
9.309304	706.188715	10.769831
9.741223	708.419457	10.774848
9.704560	711.715923	10.779866
9.630784	704.623871	10.784883
9.357284	711.672721	10.789901
9.591928	729.752141	10.794919
9.786224	724.814776	10.799936
9.744299	731.939455	10.804954
9.619944	734.225702	10.809971
9.946245	728.501167	10.814989
9.535822	726.894066	10.820007
9.771105	731.573375	10.825024
9.702239	734.573620	10.830042
9.551015	735.495104	10.835059
9.354773	730.676341	10.840077
9.862860	735.439997	10.845095
9.845737	734.311045	10.850112
9.740612	726.586415	10.855130
9.511218	734.383047	10.860147
9.906803	729.189921	10.865165
9.687252	728.129920	10.870183
9.933347	737.147348	10.875200
10.095376	737.429985	10.880218
9.732633	738.805762	10.885235
9.963134	732.562868	10.890253
9.913413	733.967515	10.895271
10.067014	737.139178	10.900288
10.181115	738.956831	10.905306
9.836731	733.235091	10.910323
9.780161	720.473974	10.915341
9.915407	724.360444	10.920359
9.863356	739.497365	10.925376
10.095237	731.162629	10.930394
9.832759	740.317814	10.935411
9.818802	726.741807	10.940429
9.853204	735.840349	10.945447
9.623778	733.804086	10.950464
10.065317	743.772562	10.955482
9.840231	762.255687	10.960499
9.895492	762.061544	10.965517
10.026021	763.852465	10.970535
9.970427	771.924649	10.975552
9.862588	760.342397	10.980570
9.808083	768.678558	10.985587
10.007914	766.510190	10.990605
9.942149	764.493276	10.995623
10.002073	772.853796	11.000640
10.092122	761.708040	11.005658
10.218413	767.370708	11.010675
10.358552	763.207217	11.015693
10.300569	769.161803	11.020711
9.944869	769.108936	11.025728
10.054688	764.028470	11.030746
10.344267	772.506463	11.035763
10.467248	769.476852	11.040781
10.208409	768.654444	11.045799
10.083264	760.342988	11.050816
10.231798	766.410612	11.055834
10.050134	768.826426	11.060851
10.203626	763.237180	11.065869
10.430699	767.926520	11.070887
10.345553	780.293918	11.075904
10.619920	756.994685	11.080922
10.319766	764.901863	11.085939
10.321655	761.423827	11.090957
10.540489	758.832651	11.095975
10.301244	764.341687	11.100992
10.501901	764.748236	11.106010
10.354581	761.347661	11.111027
10.179692	759.873986	11.116045
10.452700	761.903110	11.121063
10.260444	756.780152	11.126080
10.600251	757.688040	11.131098
10.473649	746.483687	11.136115
10.191682	737.352590	11.141133
10.565051	740.322518	11.146151
10.083241	733.399195	11.151168
10.331793	734.231647	11.156186
10.388739	748.060050	11.161203
10.674322	757.493368	11.166221
10.635870	738.955936	11.171239
10.286385	729.486438	11.176256
10.260302	723.444687	11.181274
10.151681	750.979643	11.186291
10.386679	759.280852	11.191309
10.655292	758.087260	11.196327
10.386032	757.434679	11.201344
10.451397	764.565228	11.206362
10.550138	757.461907	11.211379
10.601103	755.808321	11.216397
10.478702	759.595739	11.221415
10.217389	760.610254	11.226432
10.389771	752.218827	11.231450
10.324825	759.161121	11.236467
10.470585	760.824723	11.241485
10.096980	753.476016	11.246503
10.109506	755.555359	11.251520
10.214750	749.119825	11.256538
10.324939	759.734091	11.261555
10.807943	759.475024	11.266573
10.296989	758.137702	11.271591
10.332913	781.186034	11.276608
10.477462	788.191282	11.281626
10.618039	784.321005	11.286643
10.950466	792.268320	11.291661
10.930036	779.574788	11.296679
10.730295	786.429972	11.301696
10.727878	783.737642	11.306714
10.711444	793.041081	11.311731
10.749694	785.789898	11.316749
10.964180	778.313089	11.321767
10.697699	771.536760	11.326784
10.633154	766.077314	11.331802
10.373590	761.252492	11.336819
10.685402	779.396746	11.341837
10.980472	790.713451	11.346855
10.706744	787.584576	11.351872
10.863823	786.443308	11.356890
11.061179	790.896644	11.361907
10.776749	779.440465	11.366925
11.040320	756.243015	11.371943
10.711523	757.501762	11.376960
11.151806	758.541429	11.381978
10.693244	760.059839	11.386995
10.820755	760.048603	11.392013
10.908657	754.069063	11.397031
11.000915	766.988931	11.402048
10.857534	754.751188	11.407066
10.832115	758.222563	11.412083
10.359973	761.830901	11.417101
11.047024	766.384627	11.422119
10.810392	770.163406	11.427136
11.232238	770.450263	11.432154
10.756137	764.753472	11.437171
10.531323	777.403823	11.442189
11.043127	781.959016	11.447207
10.623549	788.482119	11.452224
11.065143	797.095969	11.457242
10.951795	792.266610	11.462259
10.938835	788.018234	11.467277
10.978582	779.137366	11.472295
10.808167	796.701686	11.477312
10.920543	776.590498	11.482330
10.931460	779.516521	11.487347
11.123276	782.481089	11.492365
11.247164	781.266582	11.497383
10.903574	786.770070	11.502400
11.031624	785.304887	11.507418
10.988595	790.596017	11.512435
10.773025	793.064297	11.517453
11.314298	781.978447	11.522471
11.164734	793.450271	11.527488
11.234100	783.999566	11.532506
11.235656	775.925375	11.537523
10.917140	791.887925	11.542541
11.299266	782.868081	11.547559
11.216489	783.356997	11.552576
11.151555	781.354116	11.557594
11.220517	784.628383	11.562611
11.165728	793.711414	11.567629
10.952089	773.173138	11.572647
11.098105	790.387826	11.577664
10.795561	782.469493	11.582682
11.333691	780.926957	11.587699
10.881182	784.110812	11.592717
11.546938	774.712135	11.597735
11.085149	784.306233	11.602752
11.183581	781.497602	11.607770
10.841854	788.003484	11.612787
11.202367	801.528137	11.617805
11.626391	808.397358	11.622823
11.393614	798.365607	11.627840
11.512487	786.899329	11.632858
11.465408	785.257251	11.637875
11.432964	786.304336	11.642893
11.571521	781.352563	11.647911
11.327926	786.436365	11.652928
11.571444	786.931088	11.657946
11.292430	783.523183	11.662963
11.298316	795.026746	11.667981
11.478361	778.215591	11.672999
11.151523	785.428809	11.678016
11.203553	783.756935	11.683034
11.580996	786.294725	11.688051
11.360839	778.499752	11.693069
11.380441	784.840688	11.698087
11.510139	793.629405	11.703104
11.276518	797.627759	11.708122
11.359779	807.923306	11.713139
11.382191	817.019550	11.718157
11.718457	813.733758	11.723175
11.676928	819.620681	11.728192
11.751894	815.072714	11.733210
11.495631	805.881417	11.738227
11.475378	812.363602	11.743245
11.516558	818.523822	11.748263
11.665221	815.472234	11.753280
11.651622	809.641757	11.758298
11.787934	816.060224	11.763315
11.445603	802.759381	11.768333
11.509613	804.610925	11.773351
11.332393	820.374132	11.778368
11.519470	813.945492	11.783386
11.666265	811.492214	11.788403
11.641659	823.932688	11.793421
11.892519	810.754072	11.798439
11.853735	813.437557	11.803456
11.950692	818.283097	11.808474
12.017536	809.784713	11.813491
11.791135	795.829673	11.818509
12.131066	788.586011	11.823527
11.857459	783.039530	11.828544
11.865335	785.792052	11.833562
11.699174	778.421579	11.838579
11.339920	782.156890	11.843597
11.610095	774.136639	11.848615
11.467496	788.444160	11.853632
11.701504	797.929741	11.858650
11.850154	807.647955	11.863667
11.513066	813.497208	11.868685
11.828201	811.627047	11.873703
11.704299	814.181327	11.878720
11.762437	811.541953	11.883738
11.788220	807.243064	11.888755
11.569890	815.485518	11.893773
11.636943	808.582293	11.898791
11.509710	810.445822	11.903808
11.563918	811.530526	11.908826
11.639331	811.722789	11.913843
11.811006	816.518557	11.918861
12.077533	827.415627	11.923879
11.871629	823.842859	11.928896
11.691447	837.717694	11.933914
11.871622	840.790102	11.938931
11.989994	848.889815	11.943949
12.225070	840.820227	11.948967
12.071422	850.192088	11.953984
12.027524	845.005166	11.959002
12.205534	843.390767	11.964019
12.118679	855.795120	11.969037
12.355943	844.091489	11.974055
11.872969	822.985179	11.979072
11.958580	815.696614	11.984090
12.156844	826.426256	11.989107
11.483603	837.642327	11.994125
12.278566	842.222693	11.999143
12.194663	849.197692	12.004160
12.231759	848.158174	12.009178
12.126627	844.904917	12.014195
12.078117	841.923767	12.019213
12.491220	843.985607	12.024231
12.705318	835.826586	12.029248
12.195559	839.681709	12.034266
12.097131	815.113479	12.039283
12.087872	822.471361	12.044301
12.173136	833.876379	12.049319
12.315118	835.529986	12.054336
12.515333	835.653948	12.059354
12.447911	824.352342	12.064371
12.178299	824.866292	12.069389
12.049444	815.160611	12.074407
12.148496	824.482739	12.079424
12.320271	837.733181	12.084442
12.664641	831.097001	12.089459
12.167278	824.778544	12.094477
12.251577	818.201575	12.099495
12.429412	835.021693	12.104512
12.303968	824.930421	12.109530
12.358979	833.403986	12.114547
12.439213	833.305702	12.119565
12.389587	829.466515	12.124583
12.271192	828.139376	12.129600
12.420905	836.247672	12.134618
12.511668	835.816166	12.139635
12.329880	842.560533	12.144653
12.213892	842.047914	12.149671
12.629204	840.445398	12.154688
12.534869	852.387625	12.159706
12.605810	836.407031	12.164723
12.491123	848.586865	12.169741
12.441520	847.262505	12.174759
12.538375	848.438571	12.179776
12.359061	846.971525	12.184794
12.927896	840.990263	12.189811
12.529960	835.433644	12.194829
12.499788	833.355712	12.199847
12.478866	835.752793	12.204864
12.118006	843.829897	12.209882
12.764323	837.753133	12.214899
12.529725	848.648558	12.219917
12.833096	841.018032	12.224935
13.018187	836.324663	12.229952
12.579588	851.577668	12.234970
12.782228	839.740805	12.239987
12.572588	845.970914	12.245005
12.824818	833.267619	12.250023
12.930955	838.867512	12.255040
12.756431	828.868613	12.260058
12.718174	814.496200	12.265075
12.712104	817.977770	12.270093
12.522740	818.987854	12.275111
12.806036	828.066887	12.280128
12.741446	849.768650	12.285146
12.695924	837.478811	12.290163
12.658738	839.972675	12.295181
13.039553	841.550516	12.300199
12.888261	842.571225	12.305216
12.773913	838.616775	12.310234
12.969346	834.829523	12.315251
12.845093	843.652840	12.320269
12.833727	847.506534	12.325287
12.910524	834.128781	12.330304
12.882245	849.902785	12.335322
12.942901	838.348870	12.340339
12.806453	845.248321	12.345357
12.992673	839.164677	12.350375
13.077241	839.831385	12.355392
13.063262	842.545805	12.360410
13.149520	831.726988	12.365427
12.648849	818.304327	12.370445
12.442540	824.907085	12.375463
12.832185	835.418832	12.380480
12.799010	841.079194	12.385498
12.812505	836.910672	12.390515
12.661331	840.940264	12.395533
12.748393	841.653014	12.400551
12.881562	845.184364	12.405568
12.680063	839.717651	12.410586
12.845042	848.922189	12.415603
12.873837	857.591437	12.420621
13.051714	871.479843	12.425639
13.294008	872.239720	12.430656
13.213892	870.288552	12.435674
13.430465	863.797923	12.440691
13.442286	854.515357	12.445709
13.264737	836.348857	12.450727
13.472142	837.055851	12.455744
12.925135	835.824093	12.460762
13.216489	832.376845	12.465779
13.214356	832.761468	12.470797
13.169209	843.810155	12.475815
13.331301	830.613546	12.480832
13.069661	831.159638	12.485850
13.253279	831.569011	12.490867
13.144250	831.350107	12.495885
12.818991	829.473394	12.500903
12.977182	840.036855	12.505920
13.375604	859.246335	12.510938
13.269833	850.903277	12.515955
13.181035	868.800209	12.520973
13.237756	870.540769	12.525991
13.480250	859.521661	12.531008
13.269844	859.580160	12.536026
13.483303	861.951031	12.541043
13.471791	852.640443	12.546061
13.541692	847.798043	12.551079
13.672319	852.312444	12.556096
13.429636	866.529922	12.561114
13.456428	860.702973	12.566131
13.386794	860.084257	12.571149
13.291791	859.650442	12.576167
13.770808	854.926112	12.581184
13.535677	858.338934	12.586202
13.473048	856.030559	12.591219
13.802857	864.127550	12.596237
13.568115	852.924493	12.601255
13.577992	858.701349	12.606272
13.544829	865.299861	12.611290
13.791456	860.769122	12.616307
13.580662	859.501766	12.621325
13.182096	862.229482	12.626343
13.771843	857.400206	12.631360
13.599940	860.002992	12.636378
13.664725	859.725385	12.641395
13.685286	855.050988	12.646413
13.638413	853.414380	12.651431
13.914339	857.406323	12.656448
13.505431	858.270095	12.661466
13.512971	846.867875	12.666483
13.514817	853.017693	12.671501
13.695050	860.150130	12.676519
13.632551	853.819491	12.681536
13.716457	858.996323	12.686554
13.696170	856.924231	12.691571
13.831930	857.805680	12.696589
13.627667	862.899529	12.701607
14.007826	857.825445	12.706624
13.792689	859.631492	12.711642
13.973473	857.960729	12.716659
13.951434	862.048467	12.721677
13.666479	860.304439	12.726695
14.002069	859.643030	12.731712
13.734454	862.227414	12.736730
13.553553	858.382794	12.741747
13.670598	865.624905	12.746765
13.528098	865.436738	12.751783
13.802159	855.996973	12.756800
13.668435	863.229429	12.761818
13.915474	866.044325	12.766835
14.120771	883.972493	12.771853
14.055502	888.532728	12.776871
14.196372	875.297865	12.781888
13.959971	869.476702	12.786906
13.890419	859.169863	12.791923
13.778825	858.054970	12.796941
13.841091	882.631299	12.801959
14.151562	878.910022	12.806976
14.106958	883.080632	12.811994
14.330780	887.922115	12.817011
14.329647	891.572561	12.822029
14.206596	877.533801	12.827047
14.327926	859.797286	12.832064
13.939860	861.594568	12.837082
13.734400	854.795106	12.842099
14.298333	863.579278	12.847117
14.390558	885.479521	12.852135
14.160561	868.679871	12.857152
14.101169	865.928853	12.862170
14.040939	867.955301	12.867187
14.327169	872.273478	12.872205
14.234229	883.377742	12.877223
14.468370	873.859542	12.882240
14.412203	879.611517	12.887258
13.770098	866.588987	12.892275
14.292715	869.758625	12.897293
14.335650	871.985696	12.902311
14.747850	866.499631	12.907328
14.563399	873.130678	12.912346
14.019871	865.029384	12.917363
14.444598	857.455522	12.922381
14.383004	868.241608	12.927399
14.480865	867.895142	12.932416
14.763068	877.998352	12.937434
14.762357	862.839400	12.942451
14.478967	850.435404	12.947469
14.559299	854.014480	12.952487
14.147003	847.259113	12.957504
14.027321	854.254605	12.962522
14.128715	858.755740	12.967539
14.326943	873.049419	12.972557
14.305484	872.752630	12.977575
14.469607	882.619503	12.982592
14.773439	869.513558	12.987610
14.721182	879.541450	12.992627
14.980078	868.856217	12.997645
14.724927	880.284964	13.002663
14.306165	870.574893	13.007680
14.170595	876.780152	13.012698
14.222559	878.077821	13.017715
14.759176	877.250846	13.022733
14.556837	877.833575	13.027751
14.800776	879.609667	13.032768
14.713002	874.598496	13.037786
14.527136	883.373773	13.042803
14.556372	869.699154	13.047821
14.183272	873.046247	13.052839
14.518342	872.536491	13.057856
14.570733	876.056423	13.062874
14.814918	881.603553	13.067891
14.777310	866.886119	13.072909
14.820940	871.885775	13.077927
14.795646	863.373486	13.082944
14.389653	882.768163	13.087962
14.849154	898.692144	13.092979
15.070876	897.153568	13.097997
14.982044	903.308580	13.103015
15.108797	889.787867	13.108032
14.844180	881.133316	13.113050
14.968308	887.527061	13.118067
14.840069	870.510567	13.123085
14.541395	882.856714	13.128103
14.681903	892.165326	13.133120
15.021506	904.871525	13.138138
14.837685	903.535135	13.143155
15.245848	902.892414	13.148173
15.240881	909.802404	13.153191
15.291281	900.718925	13.158208
15.164029	887.944178	13.163226
15.013438	877.698775	13.168243
15.215699	868.990148	13.173261
14.916295	865.865115	13.178279
14.842057	874.451832	13.183296
14.802655	882.534778	13.188314
15.040498	895.458991	13.193331
15.348683	894.886367	13.198349
15.463044	896.634314	13.203367
15.140897	890.674198	13.208384
15.321485	884.838308	13.213402
15.073598	877.930118	13.218419
15.343699	870.668849	13.223437
15.195848	873.166871	13.228455
14.919979	859.246735	13.233472
15.105699	880.380739	13.238490
15.272356	885.134842	13.243507
15.366381	889.962780	13.248525
15.274941	901.662451	13.253543
15.440961	899.731149	13.258560
15.304592	895.988195	13.263578
15.222307	895.410153	13.268595
15.451681	895.348194	13.273613
15.343523	894.763020	13.278631
15.752978	900.451285	13.283648
15.221355	902.995145	13.288666
15.038017	900.289842	13.293683
15.264833	894.220713	13.298701
15.489021	895.642220	13.303719
15.628133	890.171840	13.308736
15.503856	907.316460	13.313754
15.328617	905.407416	13.318771
15.454690	887.818108	13.323789
15.372929	898.239855	13.328807
15.321089	891.059444	13.333824
15.477784	896.244313	13.338842
15.412721	904.634655	13.343859
15.339922	894.146843	13.348877
15.141624	900.081408	13.353895
15.369465	900.111037	13.358912
15.240983	895.893965	13.363930
15.245908	898.015922	13.368947
15.869231	908.628388	13.373965
15.902554	919.681851	13.378983
15.947928	909.289416	13.384000
15.702677	902.847293	13.389018
15.711976	898.343638	13.394035
15.764785	890.391996	13.399053
15.658485	903.885383	13.404071
15.594793	900.000085	13.409088
16.051181	894.188991	13.414106
15.442708	889.807712	13.419123
15.604873	889.573820	13.424141
15.457257	894.902776	13.429159
16.001808	919.355603	13.434176
15.965588	928.990732	13.439194
15.862032	928.126854	13.444211
15.895965	928.374410	13.449229
15.794948	929.082876	13.454247
16.108362	924.732389	13.459264
15.847155	902.939670	13.464282
15.739065	904.481944	13.469299
16.200251	907.021635	13.474317
15.781989	905.792566	13.479335
15.859792	909.380342	13.484352
16.076504	912.885276	13.489370
15.975039	923.834296	13.494387
16.468296	913.803500	13.499405
16.108421	888.498954	13.504423
15.766899	895.634344	13.509440
15.893568	892.123019	13.514458
16.040868	904.531155	13.519475
16.393761	898.061638	13.524493
16.004597	894.184175	13.529511
16.112856	893.703316	13.534528
16.066230	883.085592	13.539546
15.836251	890.480843	13.544563
16.335147	907.924616	13.549581
16.393508	916.425623	13.554599
16.060454	904.036894	13.559616
16.136341	897.776624	13.564634
16.015614	913.684895	13.569651
16.279406	917.259983	13.574669
16.278915	916.112516	13.579687
16.385945	921.002088	13.584704
16.354410	908.237457	13.589722
16.138306	916.287085	13.594739
16.391235	923.251616	13.599757
16.523608	916.518226	13.604775
16.711722	910.120476	13.609792
16.445134	891.061216	13.614810
16.015156	898.976179	13.619827
16.180467	891.425180	13.624845
16.431415	904.261407	13.629863
16.312405	914.699570	13.634880
16.415584	912.671196	13.639898
16.283379	919.194010	13.644915
16.569977	909.573011	13.649933
16.407087	914.773407	13.654951
16.377362	919.349024	13.659968
16.669741	910.212478	13.664986
16.527874	917.349068	13.670003
16.489901	915.933804	13.675021
16.228400	913.393009	13.680039
16.316628	915.848797	13.685056
16.744650	916.359821	13.690074
16.411042	920.748368	13.695091
16.615443	914.218004	13.700109
16.609604	915.754371	13.705127
16.208268	917.249934	13.710144
16.897756	913.046616	13.715162
16.690964	912.721857	13.720179
16.881509	913.478888	13.725197
16.764059	909.439899	13.730215
16.501559	912.236820	13.735232
16.531811	912.962523	13.740250
16.178103	918.797639	13.745267
16.442804	913.026153	13.750285
16.930189	937.076289	13.755303
16.713311	947.571622	13.760320
16.864104	946.399496	13.765338
16.833546	938.531316	13.770355
17.068140	939.807410	13.775373
16.861651	945.717760	13.780391
16.821068	946.663059	13.785408
17.253307	935.050297	13.790426
16.942362	927.092731	13.795443
16.828653	916.429010	13.800461
16.857020	918.097108	13.805479
16.984633	934.196156	13.810496
17.153725	932.395044	13.815514
16.657305	931.958409	13.820531
17.017527	942.438095	13.825549
17.154959	941.746507	13.830567
17.113746	949.384531	13.835584
17.002885	942.055215	13.840602
16.913676	936.026983	13.845619
17.256581	948.838179	13.850637
17.319962	945.908557	13.855655
17.237943	948.750005	13.860672
17.346019	935.478790	13.865690
16.918820	917.822803	13.870707
16.913800	917.800051	13.875725
17.219662	931.907859	13.880743
17.110112	939.168629	13.885760
17.267583	942.542048	13.890778
17.178981	937.189670	13.895795
17.146529	937.608448	13.900813
17.133769	937.199986	13.905831
16.986394	944.711500	13.910848
17.450477	932.028160	13.915866
17.497223	938.682759	13.920883
17.432974	938.827288	13.925901
17.625210	930.649004	13.930919
16.979502	940.600015	13.935936
17.044777	928.104758	13.940954
17.470302	933.678570	13.945971
17.211793	935.846516	13.950989
17.440323	937.067317	13.956007
17.444928	944.774127	13.961024
17.225001	935.661771	13.966042
16.941514	934.236375	13.971059
16.939426	933.596235	13.976077
17.229664	946.193719	13.981095
17.462427	950.246374	13.986112
17.739650	950.687886	13.991130
17.790512	965.451703	13.996147
17.651686	956.821948	14.001165
17.887840	953.505856	14.006183
17.655040	952.102772	14.011200
17.584935	942.948675	14.016218
17.754864	932.867475	14.021235
17.559437	941.142815	14.026253
17.856516	937.320597	14.031271
17.486740	945.501194	14.036288
17.934263	935.277966	14.041306
17.655152	953.040375	14.046323
17.815400	953.801639	14.051341
17.970886	942.013448	14.056359
17.669068	944.772006	14.061376
17.872848	946.515387	14.066394
17.796351	936.209253	14.071411
17.624213	949.363598	14.076429
17.974864	948.845355	14.081447
17.712696	961.655971	14.086464
18.059006	956.241019	14.091482
18.034121	948.382130	14.096499
17.642358	951.306364	14.101517
17.785425	951.640569	14.106535
18.079076	947.913401	14.111552
18.221789	943.366382	14.116570
18.174258	948.462256	14.121587
17.803377	953.853792	14.126605
18.190260	948.805729	14.131623
17.802448	953.392622	14.136640
17.736341	951.570615	14.141658
17.745330	959.968015	14.146675
17.520747	953.127189	14.151693
17.836355	948.007862	14.156711
17.869017	948.907176	14.161728
17.850047	952.806642	14.166746
17.681752	962.368784	14.171763
18.162494	976.726010	14.176781
18.245176	978.022537	14.181799
18.196572	982.514295	14.186816
18.268240	967.347192	14.191834
18.970652	978.639889	14.196851
18.426988	962.115295	14.201869
18.431534	946.005038	14.206887
18.276007	945.464711	14.211904
18.941802	949.121659	14.216922
18.627926	941.137408	14.221939
18.366848	935.399435	14.226957
18.535280	933.006333	14.231975
18.125154	944.943050	14.236992
18.502965	940.890150	14.242010
18.584126	943.536474	14.247027
18.467115	944.886143	14.252045
18.462983	935.230203	14.257063
18.373649	935.447386	14.262080
18.513524	937.432441	14.267098
18.724844	932.536284	14.272115
18.575958	929.902825	14.277133
18.734876	926.942033	14.282151
18.609642	936.925750	14.287168
18.620048	934.887540	14.292186
18.634076	934.375041	14.297203
18.363093	938.226081	14.302221
19.087130	932.693473	14.307239
18.547643	939.485696	14.312256
18.397087	934.601038	14.317274
18.773610	938.237777	14.322291
18.657084	936.941026	14.327309
18.670958	929.966634	14.332327
18.816856	936.533164	14.337344
18.676243	949.735830	14.342362
18.835177	938.144307	14.347379
18.651001	936.383582	14.352397
19.038499	939.651197	14.357415
18.666313	941.917098	14.362432
18.847017	939.418423	14.367450
18.659774	935.929542	14.372467
18.601879	937.602479	14.377485
18.799022	938.247400	14.382503
18.705903	937.505804	14.387520
18.734261	948.114854	14.392538
18.958521	942.101245	14.397555
18.544214	950.489209	14.402573
18.922150	956.131143	14.407591
19.515411	970.551617	14.412608
19.136850	965.899578	14.417626
19.242297	947.049892	14.422643
18.803311	938.001367	14.427661
18.923452	945.339848	14.432679
19.054471	965.206311	14.437696
19.211814	961.764298	14.442714
19.292794	967.871926	14.447731
18.968803	973.620255	14.452749
19.104775	969.086155	14.457767
19.007162	979.297993	14.462784
19.269002	973.723800	14.467802
19.279857	975.149933	14.472819
18.853767	973.338321	14.477837
19.544410	961.025692	14.482855
19.147765	971.978350	14.487872
19.162950	959.831112	14.492890
19.457724	960.781114	14.497907
19.287928	963.051692	14.502925
19.332835	963.568680	14.507943
19.375890	961.790403	14.512960
19.290923	965.272866	14.517978
19.470466	960.709114	14.522995
19.200825	959.337326	14.528013
19.200661	960.562928	14.533031
19.380661	961.044949	14.538048
19.250870	954.343144	14.543066
19.288646	964.708924	14.548083
19.074470	964.730647	14.553101
19.395680	969.296985	14.558119
19.407751	977.486807	14.563136
19.495217	979.824625	14.568154
19.519440	993.830314	14.573171
19.616205	992.598629	14.578189
19.880210	985.021006	14.583207
19.990002	991.147494	14.588224
20.228721	987.455395	14.593242
20.125737	968.507525	14.598259
20.021842	958.908245	14.603277
19.636289	960.704335	14.608295
19.696725	962.555309	14.613312
19.761321	957.786979	14.618330
19.747203	946.684715	14.623347
19.543480	960.512380	14.628365
19.597900	956.816162	14.633383
19.627070	950.893120	14.638400
19.909730	955.535126	14.643418
20.181611	953.558730	14.648435
19.699184	952.946949	14.653453
20.149116	941.951698	14.658471
19.690785	957.108472	14.663488
19.822893	954.605638	14.668506
19.905664	950.668910	14.673523
19.788376	972.838606	14.678541
20.306124	970.344744	14.683559
20.371111	979.646624	14.688576
19.856645	971.473140	14.693594
19.719394	961.092013	14.698611
19.846108	981.743823	14.703629
20.128526	980.058974	14.708647
20.015606	987.003014	14.713664
19.846965	990.711141	14.718682
20.057816	980.789662	14.723699
20.069407	984.606914	14.728717
20.237238	981.213944	14.733735
19.978241	984.751606	14.738752
20.191366	989.236246	14.743770
20.209134	982.100563	14.748787
20.426405	984.448776	14.753805
20.359936	986.680201	14.758823
20.400919	981.029196	14.763840
20.391472	981.657937	14.768858
20.453110	980.413961	14.773875
20.089068	988.823542	14.778893
20.082246	974.637106	14.783911
20.604255	986.088810	14.788928
20.444704	991.004831	14.793946
20.499500	977.495168	14.798963
20.377848	988.105858	14.803981
20.241033	980.888690	14.808999
20.453736	993.026236	14.814016
20.360775	991.406694	14.819034
20.694787	987.099628	14.824051
20.718521	1002.164416	14.829069
20.627241	995.128671	14.834087
20.694084	991.098905	14.839104
20.542478	985.252633	14.844122
20.775303	973.277997	14.849139
20.600565	983.035306	14.854157
20.537903	978.541968	14.859175
20.325191	987.181204	14.864192
20.622863	1008.288972	14.869210
20.753728	1011.175886	14.874227
20.912121	1028.141161	14.879245
21.083977	1016.099820	14.884263
20.941320	1011.039034	14.889280
20.704341	1006.080084	14.894298
21.022696	1003.182243	14.899315
20.753034	1004.706796	14.904333
20.938983	1008.928629	14.909351
21.290319	1005.151739	14.914368
20.795306	991.090219	14.919386
21.022588	974.445432	14.924403
20.841708	986.495396	14.929421
21.082768	993.603256	14.934439
20.984709	988.548871	14.939456
20.725254	1005.530952	14.944474
21.024304	1004.787797	14.949491
21.179433	1013.308659	14.954509
21.034295	1017.426270	14.959527
21.104651	1015.086795	14.964544
20.963632	1010.413124	14.969562
21.350315	999.940884	14.974579
20.842299	1008.768001	14.979597
21.264105	1002.776381	14.984615
21.562971	1003.906410	14.989632
21.298729	1009.651157	14.994650
21.541251	998.925241	14.999667
21.499010	1010.350322	15.004685
21.150305	1002.851708	15.009703
20.829968	991.262345	15.014720
21.207706	1003.267063	15.019738
21.506804	1001.495988	15.024755
21.449374	1004.695172	15.029773
21.301433	1005.726753	15.034791
21.518022	1006.559789	15.039808
21.217098	1007.953303	15.044826
21.632046	1006.616963	15.049843
21.606882	1013.205947	15.054861
21.737243	1009.527849	15.059879
21.583520	1004.337012	15.064896
21.677253	1006.744267	15.069914
21.756218	1000.607063	15.074931
21.218699	1000.579576	15.079949
21.092404	1007.704574	15.084967
21.337690	1007.135276	15.089984
21.302749	1006.542697	15.095002
21.054929	1006.851870	15.100019
20.986122	1012.624491	15.105037
21.424447	1019.858748	15.110055
21.779381	1024.658092	15.115072
21.473367	1040.775120	15.120090
21.593644	1031.335124	15.125107
21.901285	1038.298521	15.130125
21.682464	1040.252043	15.135143
21.827718	1035.046727	15.140160
21.620704	1037.282141	15.145178
22.188919	1029.736797	15.150195
22.146060	1028.709325	15.155213
22.226573	1031.384117	15.160231
22.176234	1022.244415	15.165248
22.163116	1029.710117	15.170266
22.280788	1024.217651	15.175283
22.137969	1023.544120	15.180301
22.018525	1015.825654	15.185319
21.904318	1012.286474	15.190336
21.851750	1021.187388	15.195354
22.062488	1014.629556	15.200371
21.975716	1021.800376	15.205389
21.974050	1027.215441	15.210407
21.993997	1020.604162	15.215424
22.213319	1024.629536	15.220442
22.435338	1021.700008	15.225459
21.969080	1011.880000	15.230477
22.128844	1022.625604	15.235495
22.378166	1019.767930	15.240512
22.058596	1026.777702	15.245530
22.340608	1015.830676	15.250547
22.506830	1018.705438	15.255565
22.363054	1022.031517	15.260583
22.476602	1020.875788	15.265600
22.184137	1025.069763	15.270618
22.115942	1021.626501	15.275635
22.392380	1022.633086	15.280653
22.184343	1023.865950	15.285671
22.452283	1021.808311	15.290688
22.495738	1028.032803	15.295706
22.535379	1020.910409	15.300723
22.639233	1028.066201	15.305741
22.427698	1028.861079	15.310759
22.234331	1013.287047	15.315776
22.199111	1029.056479	15.320794
22.715395	1028.153341	15.325811
22.245391	1040.586248	15.330829
22.583584	1047.482782	15.335847
23.048364	1046.198422	15.340864
22.568648	1058.360915	15.345882
22.391648	1050.184656	15.350899
22.587566	1052.693103	15.355917
22.857422	1049.009219	15.360935
23.137712	1047.048347	15.365952
22.789635	1047.518211	15.370970
22.993897	1049.818591	15.375987
23.088725	1043.235059	15.381005
23.083966	1053.974464	15.386023
22.865648	1049.426175	15.391040
23.136464	1054.169381	15.396058
22.936021	1042.939640	15.401075
23.063981	1029.829613	15.406093
22.686090	1041.364231	15.411111
22.821607	1043.900394	15.416128
23.041472	1051.566495	15.421146
22.849355	1046.211142	15.426163
23.232964	1050.603793	15.431181
22.976984	1046.057017	15.436199
23.056084	1044.178277	15.441216
23.051112	1050.139941	15.446234
22.925172	1051.306459	15.451251
23.336049	1046.580364	15.456269
22.857401	1059.037158	15.461287
23.109591	1041.953938	15.466304
23.061750	1046.242840	15.471322
23.141177	1044.825447	15.476339
23.211870	1044.846454	15.481357
23.016358	1046.546914	15.486375
23.170721	1055.593497	15.491392
23.276785	1069.603418	15.496410
23.540135	1069.722441	15.501427
23.776164	1064.694596	15.506445
23.869688	1057.537673	15.511463
23.773114	1034.930919	15.516480
23.456041	1037.196762	15.521498
23.735977	1035.136348	15.526515
23.662468	1041.019597	15.531533
23.562162	1030.123664	15.536551
23.453251	1026.527700	15.541568
23.420579	1036.204039	15.546586
23.696377	1027.982734	15.551603
23.471005	1028.701166	15.556621
23.529654	1032.944480	15.561639
23.483155	1021.811305	15.566656
23.913939	1030.598725	15.571674
23.734897	1027.107284	15.576691
23.451682	1025.889306	15.581709
23.600152	1034.304200	15.586727
23.377658	1049.151155	15.591744
23.920021	1061.020002	15.596762
24.000575	1061.082682	15.601779
24.098896	1059.410199	15.606797
23.879198	1058.863172	15.611815
24.040552	1054.451218	15.616832
24.217940	1053.796708	15.621850
23.867981	1039.263897	15.626867
23.925595	1039.336674	15.631885
23.777479	1042.224516	15.636903
23.874974	1043.715833	15.641920
23.827540	1059.820377	15.646938
24.065961	1059.139620	15.651955
24.240767	1061.760222	15.656973
24.041268	1061.849197	15.661991
24.222714	1053.134072	15.667008
24.172365	1056.441932	15.672026
23.951625	1052.373159	15.677043
24.031091	1057.590162	15.682061
24.229092	1058.220774	15.687079
24.243348	1050.987219	15.692096
24.617728	1044.503060	15.697114
24.618043	1056.161277	15.702131
24.557163	1056.935935	15.707149
24.360862	1065.567379	15.712167
24.383728	1058.995363	15.717184
24.090626	1057.136129	15.722202
24.151275	1067.595037	15.727219
24.114740	1062.722165	15.732237
23.935943	1065.873351	15.737255
24.251036	1065.059035	15.742272
24.227008	1075.664642	15.747290
24.665157	1081.583256	15.752307
24.993982	1083.872857	15.757325
24.518008	1070.913191	15.762343
24.395350	1056.585630	15.767360
24.541857	1067.018904	15.772378
24.773610	1077.717193	15.777395
25.030371	1074.114603	15.782413
24.471972	1067.453013	15.787431
24.636889	1072.307065	15.792448
25.175436	1076.574858	15.797466
24.820047	1064.208988	15.802483
25.066435	1046.995232	15.807501
24.417102	1058.570480	15.812519
24.892728	1059.348815	15.817536
24.894914	1081.561480	15.822554
24.823800	1083.177568	15.827571
25.019740	1087.250136	15.832589
25.187620	1080.283245	15.837607
24.959321	1068.538824	15.842624
24.925537	1062.367512	15.847642
24.995781	1069.445427	15.852659
25.106930	1073.839895	15.857677
25.033712	1074.180391	15.862695
25.078456	1078.770889	15.867712
25.383031	1073.812791	15.872730
24.908076	1065.363038	15.877747
24.991437	1067.868079	15.882765
24.908781	1068.483357	15.887783
24.830085	1078.398831	15.892800
25.308391	1079.582221	15.897818
25.010947	1086.849764	15.902835
25.162621	1079.890675	15.907853
24.928030	1080.548827	15.912871
24.882812	1071.618084	15.917888
25.299181	1072.923142	15.922906
24.969610	1079.776332	15.927923
25.197807	1094.268791	15.932941
25.323658	1103.483898	15.937959
25.314487	1102.418560	15.942976
25.681093	1098.472196	15.947994
25.369396	1100.556455	15.953011
25.851238	1097.340590	15.958029
25.616211	1101.844355	15.963047
25.724163	1097.057386	15.968064
25.842537	1097.200022	15.973082
25.787863	1096.857549	15.978099
25.694532	1076.667439	15.983117
25.729479	1085.582638	15.988135
25.821036	1076.307995	15.993152
25.824978	1063.343273	15.998170
25.518269	1062.651211	16.003187
25.805423	1070.382161	16.008205
25.491389	1087.801701	16.013223
25.479271	1091.201266	16.018240
25.913150	1101.682250	16.023258
25.332826	1097.632852	16.028275
25.757751	1098.090068	16.033293
25.748362	1095.441750	16.038311
26.117875	1100.162723	16.043328
26.088494	1090.826210	16.048346
25.531063	1100.546176	16.053363
26.136066	1103.268379	16.058381
25.685944	1101.501280	16.063399
25.828690	1097.550647	16.068416
26.302304	1101.704401	16.073434
25.968825	1110.649914	16.078451
26.478472	1104.836222	16.083469
26.210046	1107.026699	16.088487
26.087830	1098.403169	16.093504
25.979601	1105.565769	16.098522
25.999414	1129.123964	16.103539
26.222732	1123.595466	16.108557
26.155183	1124.272415	16.113575
26.149774	1124.200516	16.118592
26.239752	1125.287981	16.123610
26.326727	1127.418429	16.128627
26.563007	1122.973183	16.133645
26.401872	1129.324897	16.138663
26.393841	1122.387903	16.143680
26.434355	1129.244792	16.148698
26.264336	1126.423467	16.153715
26.691439	1118.484137	16.158733
26.418734	1118.548621	16.163751
26.534003	1123.396737	16.168768
26.501433	1117.617315	16.173786
26.368431	1125.973753	16.178803
26.657861	1121.331130	16.183821
26.576030	1123.245050	16.188839
26.622888	1125.908896	16.193856
26.755536	1128.971515	16.198874
26.664285	1145.476305	16.203891
26.985226	1135.170761	16.208909
26.903166	1131.691976	16.213927
26.950367	1134.474267	16.218944
26.844198	1119.388036	16.223962
26.839398	1115.205933	16.228979
26.692114	1101.209169	16.233997
27.045356	1121.977194	16.239015
26.847547	1126.514566	16.244032
27.381414	1132.463806	16.249050
26.982521	1128.624506	16.254067
27.156638	1114.442231	16.259085
27.171072	1114.590661	16.264103
27.029064	1111.089132	16.269120
27.271052	1108.834211	16.274138
27.077219	1113.402416	16.279155
27.398098	1119.450302	16.284173
27.446398	1112.597683	16.289191
27.336559	1115.186690	16.294208
27.404642	1103.862047	16.299226
27.438087	1110.272475	16.304243
27.550868	1106.139800	16.309261
27.374975	1112.536076	16.314279
27.122884	1114.201031	16.319296
27.252010	1114.630853	16.324314
27.550202	1110.742663	16.329331
27.487676	1106.356743	16.334349
27.376106	1108.060631	16.339367
27.154578	1107.092266	16.344384
27.666166	1115.240785	16.349402
27.360212	1124.557326	16.354419
27.491840	1129.803116	16.359437
27.883423	1144.764221	16.364455
27.565903	1143.232238	16.369472
27.797560	1143.562409	16.374490
27.966951	1145.149308	16.379507
27.811791	1116.942072	16.384525
27.451991	1118.901626	16.389543
27.281548	1125.010399	16.394560
27.589578	1124.387008	16.399578
27.212919	1138.182839	16.404595
27.556997	1141.597447	16.409613
27.596814	1140.266129	16.414631
27.247428	1139.517352	16.419648
28.077991	1153.390453	16.424666
27.749341	1163.620985	16.429683
27.747169	1161.515145	16.434701
28.189664	1169.470415	16.439719
28.061172	1170.671615	16.444736
28.189145	1167.750153	16.449754
28.182846	1166.795356	16.454771
28.259762	1169.184948	16.459789
28.553853	1168.963065	16.464807
28.395561	1159.209680	16.469824
28.207326	1132.979487	16.474842
28.024723	1139.657978	16.479859
27.917035	1153.332122	16.484877
28.216378	1160.451668	16.489895
28.515305	1164.696962	16.494912
28.442683	1155.525833	16.499930
28.503653	1152.428466	16.504947
28.277531	1165.431307	16.509965
28.578760	1162.364231	16.514983
28.321473	1157.553473	16.520000
28.658283	1154.450980	16.525018
28.418736	1156.871713	16.530035
28.649593	1160.646796	16.535053
28.703614	1165.210981	16.540071
28.430436	1164.075185	16.545088
28.797852	1155.722110	16.550106
28.379713	1165.418659	16.555123
28.490069	1165.916155	16.560141
28.833141	1160.976852	16.565159
28.600283	1162.189034	16.570176
28.738335	1153.240494	16.575194
28.595565	1156.629426	16.580211
28.701444	1162.317666	16.585229
28.463198	1158.304518	16.590247
28.579490	1157.778228	16.595264
28.870928	1152.650238	16.600282
28.662442	1161.247140	16.605299
28.620721	1160.086404	16.610317
28.955129	1164.129371	16.615335
28.953488	1173.332955	16.620352
28.766138	1176.364322	16.625370
29.048552	1186.183850	16.630387
28.775369	1189.518795	16.635405
29.325185	1176.412804	16.640423
29.227755	1183.151224	16.645440
29.203843	1176.366043	16.650458
29.235032	1183.007184	16.655475
29.144439	1191.181048	16.660493
29.219171	1181.260328	16.665511
29.056562	1189.203603	16.670528
29.305917	1182.167272	16.675546
29.245738	1180.283627	16.680563
28.963999	1181.279108	16.685581
28.882366	1177.471118	16.690599
29.196916	1186.737310	16.695616
29.308445	1179.720652	16.700634
29.375051	1191.675859	16.705651
29.221609	1205.495023	16.710669
29.940970	1205.203901	16.715687
29.633561	1210.981066	16.720704
29.987659	1201.133756	16.725722
29.814095	1187.419604	16.730739
29.880970	1177.290350	16.735757
29.630870	1168.919445	16.740775
29.737076	1167.738151	16.745792
29.899287	1171.598223	16.750810
29.917099	1167.585978	16.755827
29.647817	1170.426980	16.760845
29.619370	1174.657196	16.765863
29.695198	1174.871048	16.770880
29.869962	1198.923362	16.775898
30.030854	1204.464717	16.780915
29.996448	1206.567246	16.785933
30.075373	1200.495322	16.790951
30.024174	1204.449400	16.795968
30.116454	1207.791548	16.800986
30.043752	1211.171644	16.806003
30.023121	1208.979880	16.811021
30.273299	1209.943583	16.816039
30.244828	1206.877943	16.821056
30.260467	1201.694822	16.826074
30.270177	1203.262500	16.831091
30.199866	1202.382865	16.836109
30.525655	1201.318354	16.841127
30.258415	1192.457374	16.846144
30.318444	1191.744341	16.851162
30.292633	1200.268891	16.856179
30.091181	1204.900193	16.861197
30.683555	1198.092087	16.866215
30.339504	1207.740174	16.871232
30.026421	1197.247063	16.876250
30.401011	1198.433858	16.881267
30.403353	1199.688591	16.886285
30.731168	1192.367223	16.891303
30.420589	1194.338714	16.896320
30.542201	1189.261274	16.901338
30.460739	1193.800265	16.906355
30.556664	1195.444215	16.911373
30.955316	1192.054317	16.916391
30.410609	1198.409339	16.921408
30.597861	1197.804763	16.926426
30.526073	1203.306696	16.931443
30.249884	1191.107525	16.936461
30.733938	1212.296520	16.941479
30.687858	1217.420982	16.946496
30.622306	1228.139079	16.951514
30.908054	1221.436852	16.956531
30.706209	1231.442893	16.961549
30.914434	1219.782763	16.966567
30.720042	1222.961365	16.971584
30.797216	1221.455748	16.976602
31.036369	1225.099555	16.981619
30.970481	1221.660984	16.986637
31.330198	1218.925936	16.991655
31.142314	1224.994330	16.996672
31.106268	1219.378434	17.001690
31.398121	1234.669124	17.006707
31.371087	1239.946342	17.011725
31.322100	1217.596395	17.016743
31.546024	1228.055935	17.021760
31.449608	1227.516439	17.026778
31.389658	1220.502174	17.031795
31.170844	1224.976912	17.036813
31.529626	1229.078852	17.041831
31.726633	1243.342763	17.046848
31.571616	1238.824092	17.051866
31.749090	1226.256080	17.056883
31.539351	1223.038174	17.061901
31.598399	1220.623771	17.066919
31.692406	1222.623938	17.071936
31.794960	1237.497169	17.076954
31.580129	1232.111261	17.081971
31.430766	1245.804198	17.086989
31.543821	1237.754609	17.092007
31.675626	1244.969652	17.097024
31.579255	1248.506427	17.102042
31.868295	1242.235920	17.107059
31.754333	1245.966548	17.112077
32.142402	1238.849743	17.117095
32.103396	1243.457701	17.122112
32.192599	1238.710800	17.127130
32.268309	1242.931662	17.132147
32.232451	1233.842192	17.137165
32.457987	1242.500732	17.142183
32.310172	1241.094965	17.147200
32.114115	1236.272862	17.152218
32.185502	1234.610726	17.157235
32.189795	1247.573120	17.162253
32.037377	1233.697162	17.167271
32.308232	1240.316751	17.172288
32.218194	1244.778439	17.177306
32.218639	1233.923552	17.182323
32.017906	1236.187087	17.187341
32.270915	1237.329059	17.192359
32.241049	1241.159144	17.197376
32.270359	1243.634582	17.202394
32.463964	1241.695521	17.207411
32.341431	1243.746901	17.212429
32.361876	1238.931859	17.217447
32.495432	1239.031432	17.222464
32.653202	1253.769949	17.227482
32.954561	1246.690726	17.232499
32.424158	1255.592159	17.237517
32.712785	1257.921907	17.242535
32.891702	1251.457825	17.247552
32.660431	1251.532377	17.252570
33.036056	1249.247434	17.257587
32.809314	1258.398974	17.262605
32.643133	1253.259721	17.267623
32.766963	1247.055544	17.272640
33.037190	1245.065213	17.277658
32.957064	1244.389558	17.282675
32.576253	1254.576819	17.287693
33.041770	1253.492710	17.292711
32.951333	1246.444112	17.297728
32.785654	1245.644438	17.302746
33.385679	1240.646420	17.307763
33.323244	1248.873526	17.312781
33.097238	1244.794944	17.317799
33.396266	1244.436025	17.322816
32.984332	1246.626268	17.327834
32.961430	1232.890672	17.332851
32.796560	1249.673504	17.337869
33.385783	1237.453435	17.342887
32.948292	1244.253309	17.347904
33.291019	1271.411706	17.352922
33.389197	1274.744623	17.357939
33.642417	1273.339376	17.362957
33.597318	1272.513041	17.367975
33.905851	1274.970989	17.372992
33.772662	1278.501270	17.378010
33.961296	1260.503944	17.383027
33.447296	1248.055924	17.388045
33.927915	1252.784924	17.393063
33.843804	1239.975971	17.398080
33.295713	1243.475342	17.403098
33.811669	1251.089365	17.408115
33.853242	1264.634169	17.413133
33.891453	1271.158045	17.418151
34.020477	1275.256311	17.423168
33.855842	1265.222419	17.428186
34.079469	1267.530255	17.433203
34.132492	1271.058834	17.438221
33.988364	1270.759910	17.443239
33.994324	1268.126736	17.448256
34.250874	1272.516082	17.453274
34.486972	1268.043660	17.458291
34.294168	1268.810252	17.463309
34.414832	1256.883498	17.468327
34.063455	1244.784527	17.473344
34.014703	1237.060543	17.478362
34.059527	1244.403766	17.483379
33.987702	1260.162172	17.488397
34.120521	1262.973615	17.493415
34.414961	1267.657072	17.498432
34.324615	1270.034221	17.503450
34.378784	1266.724576	17.508467
34.136060	1263.744795	17.513485
34.303826	1267.165792	17.518503
34.787993	1261.423191	17.523520
34.145755	1258.684757	17.528538
34.567979	1262.948638	17.533555
34.457430	1275.851334	17.538573
34.540605	1275.457686	17.543591
34.820473	1285.642653	17.548608
34.547398	1292.625554	17.553626
34.892621	1287.314209	17.558643
34.666690	1292.045651	17.563661
34.704719	1283.860826	17.568679
34.702327	1289.100517	17.573696
34.280486	1288.443255	17.578714
35.093968	1280.430023	17.583731
35.368627	1292.452037	17.588749
35.104854	1290.439889	17.593767
35.137676	1276.756442	17.598784
34.928389	1284.322859	17.603802
35.092747	1279.837904	17.608819
35.057355	1283.431518	17.613837
34.989518	1283.582943	17.618855
35.318364	1286.189494	17.623872
35.185278	1281.592771	17.628890
35.324518	1275.953341	17.633907
34.846581	1280.586353	17.638925
35.250845	1278.910825	17.643943
35.438946	1278.619878	17.648960
35.036902	1286.539072	17.653978
35.288466	1292.109933	17.658995
35.304066	1301.650888	17.664013
35.709557	1313.738261	17.669031
35.781366	1298.685768	17.674048
35.731223	1295.300085	17.679066
35.860959	1303.742638	17.684083
35.770206	1307.371802	17.689101
35.697588	1310.939697	17.694119
36.100799	1297.792528	17.699136
35.813457	1303.432942	17.704154
35.697189	1288.337588	17.709171
35.795351	1285.321042	17.714189
35.740151	1295.654802	17.719207
35.943015	1298.821181	17.724224
35.893406	1309.289849	17.729242
36.040018	1300.133119	17.734259
35.923980	1313.699340	17.739277
35.949708	1305.981886	17.744295
35.793171	1306.947982	17.749312
35.771056	1300.626613	17.754330
35.567471	1294.452223	17.759347
36.011866	1304.022963	17.764365
36.025583	1315.142553	17.769383
36.132512	1316.058330	17.774400
36.338724	1332.642802	17.779418
36.592697	1326.914278	17.784435
36.893948	1324.154641	17.789453
36.728659	1321.802566	17.794471
36.648693	1298.884020	17.799488
36.551527	1297.564348	17.804506
36.805802	1297.436850	17.809523
36.339097	1296.523242	17.814541
36.291943	1290.839081	17.819559
36.711714	1290.858979	17.824576
36.179190	1298.492704	17.829594
36.752350	1308.395662	17.834611
36.603178	1319.561518	17.839629
36.680975	1316.478260	17.844647
36.914715	1317.497447	17.849664
37.106284	1323.113292	17.854682
36.977129	1314.470711	17.859699
37.028041	1328.850229	17.864717
37.089138	1323.652059	17.869735
37.190855	1317.802296	17.874752
37.141998	1315.016777	17.879770
37.333396	1311.010791	17.884787
36.955424	1306.679802	17.889805
37.053881	1312.781130	17.894823
37.236896	1314.781925	17.899840
36.800818	1319.744625	17.904858
36.707365	1323.638015	17.909875
37.244768	1320.772742	17.914893
37.148220	1323.616271	17.919911
37.455014	1325.210752	17.924928
37.078267	1322.211420	17.929946
37.149804	1324.150362	17.934963
37.371866	1319.909379	17.939981
37.075348	1320.960071	17.944999
37.500792	1321.951058	17.950016
37.558889	1343.616269	17.955034
37.685612	1345.468124	17.960051
37.854903	1346.264918	17.965069
37.446569	1341.708242	17.970087
37.914433	1341.870568	17.975104
37.678934	1355.672351	17.980122
37.550170	1343.886042	17.985139
37.675178	1352.480189	17.990157
37.535287	1350.856961	17.995175
37.664825	1342.066807	18.000192
37.815028	1349.150902	18.005210
37.824643	1351.500093	18.010227
37.777744	1345.430444	18.015245
37.353167	1345.398817	18.020263
37.714621	1350.892449	18.025280
37.715165	1368.580287	18.030298
37.957328	1373.416525	18.035315
38.140319	1363.977754	18.040333
38.327829	1370.326559	18.045351
38.086624	1368.863017	18.050368
37.712066	1381.991010	18.055386
37.933115	1374.186063	18.060403
38.308679	1379.980120	18.065421
38.548861	1390.052044	18.070439
38.758572	1393.368881	18.075456
38.893219	1387.997490	18.080474
38.694342	1362.569050	18.085491
38.736793	1350.237465	18.090509
38.526041	1357.147478	18.095527
39.135835	1350.769486	18.100544
39.138275	1363.035840	18.105562
38.857801	1352.843516	18.110579
38.988639	1351.331363	18.115597
38.747526	1357.058235	18.120615
38.880202	1352.760786	18.125632
39.051110	1354.297851	18.130650
38.980973	1359.525161	18.135667
39.096458	1346.205912	18.140685
38.976320	1355.459539	18.145703
39.173113	1351.571939	18.150720
38.870742	1353.196032	18.155738
38.547403	1352.798830	18.160755
38.992417	1350.922849	18.165773
38.756026	1356.829644	18.170791
39.048617	1357.632006	18.175808
39.099677	1375.932344	18.180826
39.411821	1381.542024	18.185843
39.577507	1375.050554	18.190861
39.342494	1384.288575	18.195879
39.781363	1380.887647	18.200896
39.421349	1381.856732	18.205914
39.476499	1381.527563	18.210931
39.777430	1376.071950	18.215949
39.665125	1376.963798	18.220967
39.778026	1377.762450	18.225984
39.560019	1378.767075	18.231002
39.476415	1376.980196	18.236019
39.454873	1374.253529	18.241037
39.373220	1379.075672	18.246055
39.466383	1378.218564	18.251072
39.204620	1379.207205	18.256090
39.459773	1381.262205	18.261107
39.719045	1380.265783	18.266125
39.534084	1398.787903	18.271143
39.557957	1408.866129	18.276160
39.619068	1407.793857	18.281178
39.577726	1414.661671	18.286195
40.504014	1410.478069	18.291213
39.974531	1410.298461	18.296231
40.292331	1405.109332	18.301248
40.327453	1402.606738	18.306266
40.259225	1399.840159	18.311283
40.278842	1408.714383	18.316301
39.945790	1411.232921	18.321319
39.972585	1398.392479	18.326336
40.383818	1414.549789	18.331354
40.317108	1426.061905	18.336371
40.756085	1424.732184	18.341389
40.527365	1432.402676	18.346407
40.888873	1427.303939	18.351424
41.143367	1431.317298	18.356442
40.873824	1419.541250	18.361459
40.786277	1404.600867	18.366477
40.447862	1400.578651	18.371495
40.781103	1407.382074	18.376512
41.015169	1419.073512	18.381530
40.862412	1424.825935	18.386547
40.819922	1429.290039	18.391565
40.639639	1429.883307	18.396583
40.751032	1421.807914	18.401600
41.077905	1417.858601	18.406618
40.991060	1420.343459	18.411635
41.278062	1416.230672	18.416653
40.744911	1425.111790	18.421671
41.101244	1419.564706	18.426688
41.400573	1420.685637	18.431706
41.182596	1421.959153	18.436723
41.351956	1422.976409	18.441741
41.347229	1431.116497	18.446759
41.084182	1430.540807	18.451776
41.215067	1425.771199	18.456794
41.083682	1427.834305	18.461811
41.618658	1439.186959	18.466829
41.539968	1450.995168	18.471847
41.660150	1455.110693	18.476864
41.690500	1457.925360	18.481882
41.579610	1458.585485	18.486899
41.916737	1448.027450	18.491917
41.587113	1455.230415	18.496935
41.783351	1445.491372	18.501952
42.050629	1452.454949	18.506970
41.956094	1450.012793	18.511987
42.061288	1443.680522	18.517005
41.939683	1453.879716	18.522023
41.860934	1453.024298	18.527040
42.162315	1453.269704	18.532058
42.340190	1443.618347	18.537075
42.237186	1447.631064	18.542093
41.995928	1451.022194	18.547111
42.086090	1443.235735	18.552128
42.329372	1446.068291	18.557146
42.117728	1446.990371	18.562163
42.305454	1437.716911	18.567181
42.095677	1441.868171	18.572199
42.223357	1440.680151	18.577216
42.483004	1435.295525	18.582234
42.067233	1438.801768	18.587251
42.279633	1438.370577	18.592269
42.628422	1445.533250	18.597287
42.518688	1453.686407	18.602304
42.683339	1469.810196	18.607322
42.257067	1474.879981	18.612339
42.455111	1464.318195	18.617357
42.273152	1469.679804	18.622375
42.709721	1477.745665	18.627392
42.864373	1471.400863	18.632410
42.788380	1467.644228	18.637427
43.030060	1475.136065	18.642445
42.904728	1474.722213	18.647463
42.776833	1477.234349	18.652480
42.887457	1470.327158	18.657498
42.918688	1473.083415	18.662515
43.258082	1482.368900	18.667533
43.060330	1494.759844	18.672551
42.792770	1492.727824	18.677568
43.326978	1485.486316	18.682586
43.074187	1494.233256	18.687603
43.537604	1480.753919	18.692621
43.330671	1486.651554	18.697639
43.404305	1491.473610	18.702656
43.626085	1487.673964	18.707674
43.729887	1488.553262	18.712691
43.773507	1483.696512	18.717709
43.579026	1484.117725	18.722727
43.735776	1486.071318	18.727744
43.792765	1476.580508	18.732762
43.514338	1487.186789	18.737779
43.572580	1483.130761	18.742797
43.756207	1491.547171	18.747815
43.746945	1488.066487	18.752832
44.258634	1486.893618	18.757850
43.717627	1488.215510	18.762867
44.391902	1479.494526	18.767885
43.872974	1482.115111	18.772903
43.985652	1492.499945	18.777920
44.720725	1495.597532	18.782938
44.184791	1496.565437	18.787955
44.122833	1487.802578	18.792973
44.091815	1493.374240	18.797991
44.080175	1502.424952	18.803008
44.489563	1506.727641	18.808026
44.315835	1524.801204	18.813043
44.194326	1515.086385	18.818061
44.532003	1522.195029	18.823079
44.238166	1513.743776	18.828096
44.587071	1516.593502	18.833114
44.624678	1514.153076	18.838131
44.425944	1510.814390	18.843149
44.706619	1510.556931	18.848167
44.460924	1508.868529	18.853184
44.778646	1508.591549	18.858202
44.639225	1515.812653	18.863219
45.072691	1514.561396	18.868237
44.852309	1520.428201	18.873255
44.949076	1536.113697	18.878272
45.375193	1534.839640	18.883290
45.159192	1532.155379	18.888307
45.209372	1520.230645	18.893325
45.377062	1514.537993	18.898343
45.205962	1512.367951	18.903360
45.145623	1504.978033	18.908378
45.216501	1525.774854	18.913395
45.521909	1532.679792	18.918413
45.393598	1539.008521	18.923431
45.335846	1529.291797	18.928448
45.499278	1535.152534	18.933466
45.172188	1541.374416	18.938483
45.594529	1533.389209	18.943501
45.703016	1527.172106	18.948519
45.653014	1520.060782	18.953536
45.810968	1525.613370	18.958554
45.584621	1530.314638	18.963571
45.826194	1527.135323	18.968589
45.740215	1526.074013	18.973607
45.497240	1528.550489	18.978624
46.031187	1526.499921	18.983642
45.950798	1534.184878	18.988659
46.077327	1528.369509	18.993677
45.967679	1527.461330	18.998695
45.899097	1521.401895	19.003712
46.019103	1525.469043	19.008730
45.572923	1530.401198	19.013747
46.120464	1535.171962	19.018765
46.249973	1548.752061	19.023783
46.290318	1549.177699	19.028800
46.276468	1549.780814	19.033818
46.075419	1553.452314	19.038835
46.418351	1551.329042	19.043853
46.541385	1554.635464	19.048871
46.473291	1553.575127	19.053888
46.773296	1537.744463	19.058906
46.323939	1555.138508	19.063923
46.728892	1555.010862	19.068941
46.758221	1545.028136	19.073959
46.615102	1550.197516	19.078976
47.089256	1535.447462	19.083994
46.678760	1544.973295	19.089011
46.796213	1544.620027	19.094029
47.058799	1539.255746	19.099047
46.900171	1548.475311	19.104064
47.319904	1533.926394	19.109082
47.022627	1551.723204	19.114099
47.160504	1542.743367	19.119117
46.843689	1542.000591	19.124135
46.763752	1553.782707	19.129152
47.362398	1559.240289	19.134170
47.294113	1562.613038	19.139187
47.248403	1563.663553	19.144205
47.522529	1563.771349	19.149223
47.366589	1564.135001	19.154240
47.775700	1556.753940	19.159258
47.725054	1561.458014	19.164275
47.919042	1552.907461	19.169293
47.947633	1560.939739	19.174311
47.519051	1560.243421	19.179328
47.583714	1556.981190	19.184346
47.831098	1562.857171	19.189363
48.021210	1556.990712	19.194381
47.821889	1553.259202	19.199399
47.803896	1562.051947	19.204416
48.140057	1555.845165	19.209434
47.957898	1565.646193	19.214451
47.829455	1550.491182	19.219469
48.103029	1551.755757	19.224487
48.060074	1556.920365	19.229504
47.954362	1557.061134	19.234522
48.105247	1582.573899	19.239539
48.314820	1581.335300	19.244557
48.836192	1571.889192	19.249575
48.766779	1582.389276	19.254592
48.840061	1559.055207	19.259610
48.730516	1545.554150	19.264627
48.552980	1535.278126	19.269645
48.707520	1542.498992	19.274663
48.460852	1547.697329	19.279680
48.758809	1538.800042	19.284698
48.445854	1546.552254	19.289715
48.359544	1565.756661	19.294733
48.752632	1560.658164	19.299751
48.401400	1579.538345	19.304768
48.703269	1572.685268	19.309786
48.927905	1583.058711	19.314803
48.736213	1575.419643	19.319821
48.774763	1568.363319	19.324839
48.703244	1573.128726	19.329856
49.099588	1586.052472	19.334874
49.197369	1595.741024	19.339891
48.931297	1601.961488	19.344909
49.294461	1595.973841	19.349927
49.268028	1602.568009	19.354944
49.351113	1606.467671	19.359962
49.210433	1609.532732	19.364979
49.204766	1602.836864	19.369997
49.365947	1597.766124	19.375015
49.289138	1618.197761	19.380032
49.594218	1626.249252	19.385050
49.689045	1627.979651	19.390067
49.686131	1637.516398	19.395085
49.799121	1631.176855	19.400103
49.706562	1634.660725	19.405120
50.122553	1628.979673	19.410138
50.076467	1626.455056	19.415155
50.006233	1630.547828	19.420173
50.229062	1627.082620	19.425191
50.305989	1625.327399	19.430208
50.398690	1631.554216	19.435226
50.700875	1623.591222	19.440243
50.492545	1623.939928	19.445261
50.514863	1622.667765	19.450279
50.220627	1629.153139	19.455296
50.604206	1625.076669	19.460314
50.366842	1621.274670	19.465331
50.209016	1622.259895	19.470349
50.515885	1623.139436	19.475367
50.313004	1616.508106	19.480384
50.509666	1618.896051	19.485402
50.612342	1621.805859	19.490419
50.327722	1609.577831	19.495437
50.386556	1613.874423	19.500455
50.761807	1630.387131	19.505472
50.450961	1636.533131	19.510490
50.902345	1642.908436	19.515507
50.798630	1651.178810	19.520525
51.211302	1645.429798	19.525543
51.007861	1650.168254	19.530560
51.134307	1648.947745	19.535578
51.090250	1638.883409	19.540595
51.103998	1647.406772	19.545613
51.211889	1631.895619	19.550631
51.246927	1643.233174	19.555648
51.212251	1644.780687	19.560666
51.353102	1649.154260	19.565683
51.283660	1666.394183	19.570701
51.626104	1666.938308	19.575719
51.766008	1674.660874	19.580736
51.847221	1667.367912	19.585754
51.785952	1668.078884	19.590771
51.637514	1669.505079	19.595789
52.162749	1664.103564	19.600807
51.964215	1666.186875	19.605824
51.909597	1662.559331	19.610842
52.017759	1662.898940	19.615859
51.649155	1670.467514	19.620877
51.855420	1662.769989	19.625895
52.120328	1664.741522	19.630912
51.825937	1659.979268	19.635930
51.958055	1660.368454	19.640947
51.945248	1659.388326	19.645965
51.978439	1666.829344	19.650983
51.887775	1673.499140	19.656000
52.148037	1689.522681	19.661018
52.343761	1683.132409	19.666035
52.263730	1691.864633	19.671053
52.447589	1674.755811	19.676071
52.277959	1686.927684	19.681088
52.161838	1685.619384	19.686106
52.757103	1697.503195	19.691123
53.051120	1715.949927	19.696141
53.189919	1701.116268	19.701159
52.942663	1695.715486	19.706176
52.950231	1691.285509	19.711194
53.017321	1684.349211	19.716211
52.769634	1709.253768	19.721229
52.931582	1707.171466	19.726247
53.189382	1718.957627	19.731264
53.235508	1727.525281	19.736282
53.455324	1720.023910	19.741299
53.218712	1722.089517	19.746317
53.175471	1717.802198	19.751335
52.860341	1716.403225	19.756352
53.081510	1715.778448	19.761370
53.460686	1711.688905	19.766387
53.263166	1716.059469	19.771405
53.421094	1727.401147	19.776423
53.690899	1732.795525	19.781440
53.626980	1736.245147	19.786458
53.845318	1742.462623	19.791475
53.945021	1741.591421	19.796493
54.133008	1737.998886	19.801511
53.787105	1734.440029	19.806528
53.861151	1733.544729	19.811546
54.026996	1730.979492	19.816563
53.956012	1741.624826	19.821581
54.364294	1732.656012	19.826599
54.254444	1735.553393	19.831616
54.328259	1732.138821	19.836634
54.591473	1729.985024	19.841651
54.310181	1729.920613	19.846669
54.658475	1735.640187	19.851687
54.436062	1736.276662	19.856704
54.135061	1731.959184	19.861722
54.383634	1727.757404	19.866739
54.465270	1736.405403	19.871757
54.673152	1749.538839	19.876775
54.541453	1758.120206	19.881792
54.464835	1760.723110	19.886810
54.832852	1759.835432	19.891827
55.102061	1764.224005	19.896845
55.037771	1757.393680	19.901863
55.219702	1762.659704	19.906880
54.944998	1750.379922	19.911898
55.054169	1747.279180	19.916915
55.439699	1757.163891	19.921933
55.635405	1760.051234	19.926951
55.057979	1755.282271	19.931968
55.297768	1755.145753	19.936986
55.188527	1752.016607	19.942003
55.133695	1757.958058	19.947021
55.463878	1754.135674	19.952039
55.839256	1758.677927	19.957056
55.447870	1752.289171	19.962074
55.616615	1743.737575	19.967091
55.423131	1756.018177	19.972109
55.735715	1770.254383	19.977127
55.546764	1779.172803	19.982144
55.897163	1773.099406	19.987162
55.877245	1784.806404	19.992179
55.769214	1781.757762	19.997197
56.082145	1777.613816	20.002215
56.353346	1780.580002	20.007232
56.437947	1778.680185	20.012250
56.103030	1776.324630	20.017267
56.134140	1780.862082	20.022285
56.298135	1782.378288	20.027303
56.388772	1770.693908	20.032320
56.189753	1773.505667	20.037338
56.474571	1773.057752	20.042355
55.933696	1778.266296	20.047373
56.385295	1778.598648	20.052391
56.948281	1795.094621	20.057408
56.601707	1799.239885	20.062426
57.056930	1799.823610	20.067443
56.584824	1803.501466	20.072461
56.940392	1801.076853	20.077479
57.044214	1794.923409	20.082496
56.875217	1808.679935	20.087514
56.998944	1803.296823	20.092531
57.025838	1800.512060	20.097549
56.970635	1801.912986	20.102567
57.395433	1794.393388	20.107584
56.627808	1799.126486	20.112602
57.198070	1791.845404	20.117619
56.914901	1808.328345	20.122637
57.169045	1810.996177	20.127655
57.246160	1811.829912	20.132672
57.455641	1824.139909	20.137690
57.695550	1815.855234	20.142707
57.642131	1825.394948	20.147725
57.463429	1828.346661	20.152743
57.837646	1817.119629	20.157760
57.708341	1824.938421	20.162778
57.932740	1819.749661	20.167795
57.978071	1830.797850	20.172813
58.249287	1849.052451	20.177831
58.411172	1849.304427	20.182848
58.161439	1836.804691	20.187866
58.200762	1831.131603	20.192883
58.194707	1849.573849	20.197901
58.202442	1844.252056	20.202919
58.670583	1855.241277	20.207936
58.523031	1852.127510	20.212954
58.651755	1847.145136	20.217971
58.527300	1854.311556	20.222989
58.474307	1855.551095	20.228007
58.446556	1847.879628	20.233024
58.334112	1850.239263	20.238042
58.495860	1848.148708	20.243059
58.289922	1850.918318	20.248077
58.622979	1854.866417	20.253095
59.004158	1874.863104	20.258112
58.786469	1880.448096	20.263130
59.176129	1873.884688	20.268147
59.328603	1875.644547	20.273165
59.162597	1874.663000	20.278183
59.286351	1869.877508	20.283200
59.420147	1870.603435	20.288218
59.587068	1868.965572	20.293235
59.347585	1869.628894	20.298253
59.530129	1876.842918	20.303271
59.395584	1868.367851	20.308288
59.088854	1871.760463	20.313306
59.313387	1869.239817	20.318323
59.563069	1868.789844	20.323341
59.318094	1863.745718	20.328359
59.607698	1877.737399	20.333376
59.827483	1893.570213	20.338394
59.828042	1885.092846	20.343411
59.987534	1889.930338	20.348429
60.307984	1889.708808	20.353447
60.327135	1882.715004	20.358464
60.156147	1890.874988	20.363482
60.044906	1889.815473	20.368499
60.163787	1895.603802	20.373517
60.386863	1894.336172	20.378535
60.555635	1888.301860	20.383552
60.124124	1896.457740	20.388570
60.439798	1885.937609	20.393587
60.137350	1892.723275	20.398605
60.436184	1889.862759	20.403623
60.716273	1891.170774	20.408640
60.519239	1904.039885	20.413658
60.508551	1898.891205	20.418675
60.683358	1899.336716	20.423693
60.670639	1913.847001	20.428711
60.761878	1904.125058	20.433728
60.658151	1910.492387	20.438746
60.909993	1917.613458	20.443763
61.212710	1935.654673	20.448781
61.153962	1934.772294	20.453799
61.486233	1930.673926	20.458816
61.309950	1940.159643	20.463834
61.523943	1939.264781	20.468851
61.816952	1932.797668	20.473869
61.531358	1929.985487	20.478887
61.837868	1922.513761	20.483904
61.781667	1927.337371	20.488922
61.970868	1920.642564	20.493939
62.068175	1925.960846	20.498957
61.662037	1924.362744	20.503975
62.098314	1919.238476	20.508992
62.051428	1922.701855	20.514010
62.059889	1921.383537	20.519027
62.022418	1918.234993	20.524045
62.024443	1908.810502	20.529063
62.060833	1913.640431	20.534080
62.011925	1923.037329	20.539098
62.619812	1907.243108	20.544115
62.377412	1910.087664	20.549133
62.003027	1913.945826	20.554151
62.230887	1929.028900	20.559168
62.268539	1951.395604	20.564186
62.433726	1944.737442	20.569203
62.901634	1936.330698	20.574221
62.339889	1942.518361	20.579239
62.695623	1930.613586	20.584256
62.916099	1940.943076	20.589274
62.802214	1937.191814	20.594291
62.973023	1959.959720	20.599309
62.917667	1963.183954	20.604327
63.431169	1968.598695	20.609344
63.370848	1973.924982	20.614362
63.466733	1967.048752	20.619379
63.682934	1967.277170	20.624397
63.824542	1961.591430	20.629415
63.726639	1950.204282	20.634432
63.434297	1940.393463	20.639450
63.247455	1936.539318	20.644467
63.412840	1944.886947	20.649485
63.520248	1951.162246	20.654503
64.046211	1947.266060	20.659520
63.579715	1961.862155	20.664538
63.621990	1954.907010	20.669555
64.057591	1954.639247	20.674573
63.844143	1956.660496	20.679591
64.067839	1950.634783	20.684608
63.882243	1955.413684	20.689626
63.585717	1962.145643	20.694643
64.036522	1966.901065	20.699661
64.188913	1972.938210	20.704679
64.736895	1982.235132	20.709696
64.276324	1988.807645	20.714714
64.384059	1984.704708	20.719731
64.431635	1979.601473	20.724749
64.195183	1985.547099	20.729767
64.528119	1975.666978	20.734784
64.779878	1997.271115	20.739802
65.001067	2002.380323	20.744819
64.884953	1999.770782	20.749837
64.569489	2013.511582	20.754855
64.843100	2004.876337	20.759872
64.989103	2012.302779	20.764890
64.905267	2011.806055	20.769907
64.704228	2013.515800	20.774925
65.092851	2018.428388	20.779943
65.502688	2025.318226	20.784960
65.436559	2037.530323	20.789978
65.489416	2029.846207	20.794995
65.465005	2030.823146	20.800013
65.666197	2038.172745	20.805031
65.846151	2034.015710	20.810048
65.842451	2037.730238	20.815066
65.950801	2031.101529	20.820083
65.678482	2021.557823	20.825101
65.752343	2027.965876	20.830119
66.308421	2025.641498	20.835136
66.396761	2026.692290	20.840154
66.061423	2012.827808	20.845171
66.212680	2028.874869	20.850189
65.944081	2025.491731	20.855207
65.968599	2036.512410	20.860224
66.425799	2049.444973	20.865242
66.348710	2057.856040	20.870259
66.632425	2057.511454	20.875277
66.469508	2062.999645	20.880295
67.031302	2055.526532	20.885312
66.729317	2055.533657	20.890330
66.893786	2057.304543	20.895347
67.030759	2051.630956	20.900365
67.159312	2053.612913	20.905383
67.299235	2046.339188	20.910400
67.175694	2043.502122	20.915418
66.912850	2040.325120	20.920435
67.233688	2043.044156	20.925453
67.192077	2051.267845	20.930471
67.415067	2048.231271	20.935488
67.305922	2044.946140	20.940506
67.133934	2040.900134	20.945523
67.566185	2044.447202	20.950541
67.674821	2060.025749	20.955559
67.653904	2065.912094	20.960576
68.013853	2061.987855	20.965594
67.655226	2063.315025	20.970611
67.851161	2061.732969	20.975629
67.675640	2069.415832	20.980647
67.846927	2066.596482	20.985664
67.948112	2069.232204	20.990682
67.865612	2074.361405	20.995699
68.266995	2070.155098	21.000717
68.114686	2079.336527	21.005735
68.178849	2075.888438	21.010752
68.034786	2063.648194	21.015770
68.157381	2083.906477	21.020787
68.541900	2092.178925	21.025805
68.215693	2086.155625	21.030823
68.446270	2093.307859	21.035840
68.540269	2093.120673	21.040858
68.503802	2092.912175	21.045875
68.621342	2094.364843	21.050893
68.570747	2108.866620	21.055911
68.716933	2123.353545	21.060928
68.939516	2116.473200	21.065946
69.279095	2112.167663	21.070963
69.555280	2106.659200	21.075981
69.406168	2123.112009	21.080999
69.642458	2115.871903	21.086016
69.672328	2111.451894	21.091034
69.434662	2109.978243	21.096051
70.034474	2103.905944	21.101069
69.605265	2110.451267	21.106087
69.975178	2101.957508	21.111104
69.955283	2101.831701	21.116122
69.806807	2110.623526	21.121139
69.754536	2096.096726	21.126157
69.930457	2114.320174	21.131175
70.268756	2105.259582	21.136192
70.105805	2106.329940	21.141210
69.940949	2108.053783	21.146227
70.163341	2105.929137	21.151245
70.012156	2107.027862	21.156263
70.226262	2123.197295	21.161280
70.332701	2135.093879	21.166298
70.364346	2136.273361	21.171315
70.398606	2139.550512	21.176333
70.267877	2141.860855	21.181351
70.879400	2133.994025	21.186368
70.806870	2131.348110	21.191386
70.553597	2131.518040	21.196403
70.725095	2153.255373	21.201421
70.878777	2162.766515	21.206439
70.863854	2150.640651	21.211456
71.097861	2158.660881	21.216474
71.169345	2165.486329	21.221491
71.581737	2161.192345	21.226509
71.420684	2163.849456	21.231527
71.398844	2156.465451	21.236544
71.347247	2149.844670	21.241562
70.959220	2165.414216	21.246579
71.955426	2172.581060	21.251597
71.898245	2176.972218	21.256615
71.985996	2181.471274	21.261632
71.880638	2175.631459	21.266650
72.052014	2184.482180	21.271667
72.234539	2182.499169	21.276685
72.221576	2182.072990	21.281703
72.236898	2175.779320	21.286720
72.633267	2168.025265	21.291738
72.175270	2174.174974	21.296755
72.600856	2176.041227	21.301773
72.433014	2180.054237	21.306791
72.573216	2173.959189	21.311808
72.828402	2174.447308	21.316826
72.351846	2185.117971	21.321843
72.636417	2173.926788	21.326861
72.507321	2182.369763	21.331879
72.813557	2173.110497	21.336896
72.702749	2173.295029	21.341914
72.719371	2178.424781	21.346931
73.079263	2188.633318	21.351949
73.144058	2196.027623	21.356967
73.184620	2188.162387	21.361984
73.271122	2194.236121	21.367002
73.244177	2205.747348	21.372019
73.283376	2193.568394	21.377037
73.177642	2198.502656	21.382055
73.005334	2194.612180	21.387072
73.372181	2205.444402	21.392090
73.417306	2222.551795	21.397107
73.687993	2219.644698	21.402125
73.811113	2226.359650	21.407143
73.969733	2218.826833	21.412160
74.293295	2217.758297	21.417178
74.335565	2223.248792	21.422195
74.516545	2206.709570	21.427213
74.201325	2215.908998	21.432231
74.085220	2220.292601	21.437248
74.152604	2205.588794	21.442266
74.258649	2207.243383	21.447283
74.339919	2217.419329	21.452301
74.628398	2227.096387	21.457319
74.311317	2232.099513	21.462336
74.604037	2226.741426	21.467354
74.441594	2234.688356	21.472371
74.780879	2231.162788	21.477389
74.853747	2248.010487	21.482407
74.836173	2263.499107	21.487424
74.936209	2257.676830	21.492442
75.071194	2265.229632	21.497459
75.442895	2256.277601	21.502477
75.464637	2265.129915	21.507495
75.368206	2259.473244	21.512512
75.611128	2253.038703	21.517530
75.485317	2261.922139	21.522547
75.818042	2254.308901	21.527565
75.513581	2250.072561	21.532583
75.789207	2259.138357	21.537600
75.988890	2265.922543	21.542618
76.103613	2279.621877	21.547635
76.159572	2275.532949	21.552653
76.017028	2276.924362	21.557671
76.342736	2287.279575	21.562688
76.462271	2266.583356	21.567706
76.150520	2268.926445	21.572723
76.214612	2269.415891	21.577741
76.246476	2270.585899	21.582759
76.368309	2275.745509	21.587776
76.548138	2269.243452	21.592794
76.290436	2295.880992	21.597811
76.808917	2296.365286	21.602829
76.919207	2301.157114	21.607847
76.779508	2314.819862	21.612864
77.284378	2304.359467	21.617882
77.218000	2308.013963	21.622899
77.213256	2306.294631	21.627917
77.062983	2303.450525	21.632935
76.832360	2305.639236	21.637952
77.133051	2312.445696	21.642970
77.283622	2320.939294	21.647987
77.634334	2325.301147	21.653005
77.949299	2325.470304	21.658023
77.733930	2320.171114	21.663040
78.068835	2318.189629	21.668058
78.150068	2324.278066	21.673075
78.317418	2320.424631	21.678093
78.587616	2320.503164	21.683111
78.423975	2317.184476	21.688128
78.166957	2293.992580	21.693146
77.929535	2295.320173	21.698163
78.134167	2307.364810	21.703181
78.538085	2308.921269	21.708199
78.438980	2314.966331	21.713216
78.677423	2320.107829	21.718234
78.539289	2327.569657	21.723251
78.507839	2313.698686	21.728269
78.426176	2311.811766	21.733287
78.393194	2322.902013	21.738304
78.814835	2327.582059	21.743322
78.828164	2339.295388	21.748339
78.691344	2344.128539	21.753357
79.020197	2354.828568	21.758375
78.689492	2348.572434	21.763392
78.776176	2345.127250	21.768410
79.706474	2358.153401	21.773427
79.671473	2376.129389	21.778445
79.928304	2368.721191	21.783463
79.763086	2372.253871	21.788480
80.110077	2367.911209	21.793498
79.924670	2360.579388	21.798515
79.856219	2367.691886	21.803533
79.938778	2357.422646	21.808551
79.350369	2371.398726	21.813568
80.137665	2354.280981	21.818586
80.202276	2359.407965	21.823603
80.069166	2356.067678	21.828621
80.275987	2362.248727	21.833639
79.885875	2389.556020	21.838656
80.610811	2386.568169	21.843674
80.527775	2387.715868	21.848691
80.650166	2400.645105	21.853709
80.690701	2388.996512	21.858727
80.416230	2387.777758	21.863744
80.554198	2387.628174	21.868762
80.548045	2412.598593	21.873779
80.741851	2418.090839	21.878797
81.128336	2414.182199	21.883815
80.878013	2424.526576	21.888832
81.246866	2417.039174	21.893850
81.333395	2434.558863	21.898867
81.502969	2442.008382	21.903885
81.591992	2438.529718	21.908903
81.701763	2445.707629	21.913920
81.942954	2437.445250	21.918938
82.105248	2435.518709	21.923955
81.856142	2444.017131	21.928973
82.305747	2442.056405	21.933991
82.233587	2444.262994	21.939008
82.184997	2440.416149	21.944026
82.065400	2440.514732	21.949043
81.664733	2437.888841	21.954061
82.275511	2443.969572	21.959079
82.531070	2458.901718	21.964096
82.486323	2460.392316	21.969114
82.889888	2464.413944	21.974131
82.738640	2470.692514	21.979149
82.976759	2458.796575	21.984167
82.675530	2463.036478	21.989184
83.154182	2466.496826	21.994202
83.122701	2463.831064	21.999219
83.171553	2460.310618	22.004237
83.312390	2457.730899	22.009255
83.073299	2455.516859	22.014272
83.469103	2444.830715	22.019290
83.261053	2459.362433	22.024307
83.112859	2457.507378	22.029325
83.457547	2458.896091	22.034343
83.404137	2484.035482	22.039360
83.635536	2489.976279	22.044378
83.640663	2487.968662	22.049395
83.521696	2491.576393	22.054413
83.865588	2487.795661	22.059431
83.653872	2498.952243	22.064448
83.970629	2502.483108	22.069466
84.022385	2513.695295	22.074483
84.113120	2512.726317	22.079501
84.490296	2508.902665	22.084519
84.235045	2516.182389	22.089536
84.673529	2508.120784	22.094554
84.912807	2518.708191	22.099571
84.554441	2522.455573	22.104589
84.789998	2532.622322	22.109607
84.729177	2545.391058	22.114624
84.974940	2531.483836	22.119642
85.051442	2535.816738	22.124659
85.153259	2537.829170	22.129677
85.043558	2539.195482	22.134695
85.059384	2542.343873	22.139712
85.383700	2558.662058	22.144730
85.664062	2556.430897	22.149747
85.807083	2565.853101	22.154765
85.467044	2566.383878	22.159783
85.380876	2565.578447	22.164800
85.817104	2560.620528	22.169818
86.049032	2562.574411	22.174835
85.760259	2565.153910	22.179853
86.305380	2569.645466	22.184871
86.319904	2587.523334	22.189888
86.386114	2588.636100	22.194906
86.285013	2587.494144	22.199923
86.318625	2584.741988	22.204941
86.848095	2586.163903	22.209959
86.895002	2594.837817	22.214976
86.675399	2587.963547	22.219994
87.098438	2585.773724	22.225011
86.893315	2589.486299	22.230029
87.261676	2574.791369	22.235047
87.100932	2591.626543	22.240064
87.028289	2583.720005	22.245082
87.277374	2579.772653	22.250099
87.315590	2588.541316	22.255117
87.261316	2590.432741	22.260135
87.288209	2608.385755	22.265152
87.674915	2601.612678	22.270170
87.765492	2593.232232	22.275187
87.760662	2598.659394	22.280205
87.776049	2587.165613	22.285223
87.747481	2594.756287	22.290240
87.773899	2598.758501	22.295258
88.125664	2599.963367	22.300275
88.156025	2627.330993	22.305293
88.408454	2627.248287	22.310311
88.563038	2626.169118	22.315328
88.456969	2626.813136	22.320346
88.634493	2618.720662	22.325363
88.355738	2632.265757	22.330381
88.572010	2617.445172	22.335399
88.886903	2620.625563	22.340416
88.577401	2621.119393	22.345434
88.615433	2622.514799	22.350451
88.785382	2641.526125	22.355469
88.859400	2642.928960	22.360487
88.930290	2647.477009	22.365504
88.971056	2644.091334	22.370522
89.297765	2647.546170	22.375539
89.243515	2666.302502	22.380557
89.468093	2674.936414	22.385575
89.588810	2668.407756	22.390592
89.704215	2669.290321	22.395610
89.997145	2669.713936	22.400627
89.966576	2669.173329	22.405645
90.022042	2670.940680	22.410663
89.800152	2666.566922	22.415680
90.078022	2681.199112	22.420698
90.712705	2684.272233	22.425715
90.325788	2693.310966	22.430733
90.732636	2690.153664	22.435751
90.594814	2694.895349	22.440768
90.490943	2687.741225	22.445786
90.578404	2685.360477	22.450803
90.528731	2689.527292	22.455821
90.765070	2688.635383	22.460839
90.909417	2702.752262	22.465856
90.999292	2719.994141	22.470874
91.286393	2715.220719	22.475891
90.968459	2724.976445	22.480909
91.244058	2722.323186	22.485927
91.299427	2721.049399	22.490944
91.400331	2730.191254	22.495962
91.756410	2741.136273	22.500979
91.493319	2738.274544	22.505997
91.804795	2751.742097	22.511015
91.940241	2747.774146	22.516032
92.027415	2748.699582	22.521050
92.423007	2735.177638	22.526067
92.160176	2741.168077	22.531085
92.310625	2740.299836	22.536103
92.307900	2755.293144	22.541120
92.121893	2759.372306	22.546138
92.645152	2770.869630	22.551155
92.316154	2776.337139	22.556173
92.674655	2778.513418	22.561191
92.815231	2771.557382	22.566208
92.815926	2769.568968	22.571226
93.034106	2780.888449	22.576243
92.945394	2795.410562	22.581261
92.945273	2795.935069	22.586279
93.224948	2792.212538	22.591296
93.491954	2789.828427	22.596314
93.752890	2775.273153	22.601331
93.754392	2785.776481	22.606349
93.956117	2789.500093	22.611367
93.813131	2786.754305	22.616384
93.727439	2807.863040	22.621402
94.282676	2806.634051	22.626419
94.134656	2815.980570	22.631437
94.213937	2809.092938	22.636455
94.394052	2805.696755	22.641472
94.116170	2812.481899	22.646490
94.403959	2801.252331	22.651507
94.240435	2806.344789	22.656525
94.597420	2801.574732	22.661543
94.997627	2811.684086	22.666560
95.159357	2837.100653	22.671578
95.315412	2825.192431	22.676595
94.789530	2817.061582	22.681613
95.121745	2826.542783	22.686631
95.468477	2833.483200	22.691648
95.311207	2840.260592	22.696666
95.119986	2834.375292	22.701683
95.421899	2840.656545	22.706701
95.508085	2840.848628	22.711719
95.488802	2833.092983	22.716736
95.458934	2838.186158	22.721754
95.628208	2830.804839	22.726771
95.700687	2842.198886	22.731789
95.588258	2852.470709	22.736807
96.047814	2859.407419	22.741824
96.051231	2860.947958	22.746842
96.260096	2851.625274	22.751859
96.405445	2870.929165	22.756877
96.148968	2865.688172	22.761895
96.763043	2868.448184	22.766912
96.754931	2883.948453	22.771930
96.829227	2877.282107	22.776947
97.151473	2876.678745	22.781965
96.944758	2880.872793	22.786983
97.265146	2879.896087	22.792000
96.945984	2877.463728	22.797018
97.237787	2866.220062	22.802035
97.173018	2887.197477	22.807053
97.296686	2893.427549	22.812071
97.496236	2903.641845	22.817088
97.514420	2908.960571	22.822106
97.828580	2896.692625	22.827123
97.757929	2895.328657	22.832141
97.858615	2895.877424	22.837159
98.124722	2901.243689	22.842176
97.943063	2924.559202	22.847194
98.284176	2932.048278	22.852211
98.140872	2938.071761	22.857229
98.474006	2933.413496	22.862247
98.618280	2929.154644	22.867264
98.468960	2932.490706	22.872282
98.629334	2937.005125	22.877299
98.954507	2963.865829	22.882317
98.786358	2960.331195	22.887335
98.928348	2966.548812	22.892352
98.881709	2956.547441	22.897370
99.298964	2955.832275	22.902387
99.383242	2959.237550	22.907405
99.627118	2954.598782	22.912423
99.376612	2958.802070	22.917440
99.319775	2976.053168	22.922458
99.727813	2971.763626	22.927475
99.790006	2977.376690	22.932493
99.875781	2972.454618	22.937511
100.101594	2965.206012	22.942528
99.834946	2968.669392	22.947546
99.973747	2981.634980	22.952563
100.410245	2991.951848	22.957581
100.518861	2988.461942	22.962599
100.824506	2995.163150	22.967616
100.501373	2994.270542	22.972634
100.535556	2983.960864	22.977651
100.628563	2998.379056	22.982669
100.774099	3016.449130	22.987687
101.137192	3012.969058	22.992704
100.647242	3015.749277	22.997722
101.178881	3020.011288	23.002739
101.221383	3013.043428	23.007757
101.301621	3016.191880	23.012775
101.396661	3036.142158	23.017792
101.407132	3055.061486	23.022810
101.608939	3050.064661	23.027827
101.878924	3050.202297	23.032845
101.864034	3052.691643	23.037863
102.144054	3053.572962	23.042880
102.219100	3049.919688	23.047898
102.062358	3054.290958	23.052915
102.246151	3048.522636	23.057933
102.187227	3067.977139	23.062951
102.561857	3075.088652	23.067968
102.237888	3083.432082	23.072986
102.459847	3081.071923	23.078003
102.624799	3074.509786	23.083021
102.662385	3085.833402	23.088039
102.793725	3095.753971	23.093056
102.959724	3104.189533	23.098074
103.182965	3097.337394	23.103091
103.378067	3107.285212	23.108109
103.365891	3101.834777	23.113127
103.491958	3097.421792	23.118144
103.534207	3116.670216	23.123162
103.734240	3117.554151	23.128179
104.021684	3118.991779	23.133197
104.187966	3120.782177	23.138215
104.498336	3121.928580	23.143232
104.330202	3122.508476	23.148250
104.427968	3114.252558	23.153267
104.446000	3117.570401	23.158285
104.295929	3118.689091	23.163303
104.643191	3104.124337	23.168320
104.821078	3115.760999	23.173338
104.974326	3127.573025	23.178355
105.126062	3129.079191	23.183373
105.145365	3141.793018	23.188391
105.355766	3140.843563	23.193408
105.644147	3139.112224	23.198426
105.537393	3133.441194	23.203443
105.883776	3134.245776	23.208461
105.639301	3140.618403	23.213479
105.667310	3135.039638	23.218496
105.565395	3138.141889	23.223514
105.641589	3139.129802	23.228531
105.628200	3130.255208	23.233549
105.719435	3157.090799	23.238567
106.006475	3161.538637	23.243584
106.171038	3167.211206	23.248602
105.793863	3163.668216	23.253619
106.450021	3169.696838	23.258637
106.273943	3185.499653	23.263655
106.688024	3188.983064	23.268672
107.071214	3191.591974	23.273690
106.705034	3186.217051	23.278707
106.757525	3181.816224	23.283725
107.180262	3196.426883	23.288743
107.625161	3201.698683	23.293760
107.602809	3207.520336	23.298778
108.069488	3200.206937	23.303795
107.932652	3199.446874	23.308813
107.690666	3209.538392	23.313831
108.019013	3200.681595	23.318848
108.118368	3203.096532	23.323866
108.010336	3199.040026	23.328883
108.389274	3186.567408	23.333901
108.248204	3196.847349	23.338919
108.216453	3191.233965	23.343936
108.279708	3202.897546	23.348954
108.317314	3197.131718	23.353971
108.516229	3200.514522	23.358989
108.341736	3223.320581	23.364007
108.686327	3215.209195	23.369024
108.893888	3224.628594	23.374042
109.023800	3225.877331	23.379059
109.011819	3221.725775	23.384077
109.052796	3227.276687	23.389095
109.230230	3232.429772	23.394112
109.303985	3241.739826	23.399130
109.288473	3253.943313	23.404147
109.719643	3248.928531	23.409165
109.682185	3256.268216	23.414183
109.926208	3249.993339	23.419200
110.001672	3256.715840	23.424218
110.267581	3268.790453	23.429235
110.110103	3269.322916	23.434253
110.082317	3280.825626	23.439271
110.457891	3272.021606	23.444288
110.409470	3279.865532	23.449306
110.763607	3280.897998	23.454323
110.919810	3277.556071	23.459341
110.855047	3297.244135	23.464359
111.193877	3296.591158	23.469376
111.115079	3305.010660	23.474394
110.936808	3304.673638	23.479411
111.008068	3292.408588	23.484429
110.968901	3311.109255	23.489447
111.633959	3323.298158	23.494464
111.587437	3336.556565	23.499482
111.487175	3342.412429	23.504499
111.552414	3328.427292	23.509517
111.566031	3343.538944	23.514535
112.260868	3353.989679	23.519552
112.356993	3357.315512	23.524570
112.430426	3352.923376	23.529587
112.471385	3357.385633	23.534605
112.345552	3354.302615	23.539623
112.638666	3355.464099	23.544640
112.851424	3365.310724	23.549658
112.535034	3378.087803	23.554675
113.012208	3374.189902	23.559693
113.187797	3378.956290	23.564711
113.142037	3373.676694	23.569728
113.375469	3378.672902	23.574746
113.251247	3381.758419	23.579763
113.636153	3394.229616	23.584781
113.651918	3408.957468	23.589799
113.746880	3398.100384	23.594816
113.724800	3406.219178	23.599834
113.680536	3408.720531	23.604851
114.342957	3418.063950	23.609869
114.479136	3431.990301	23.614887
114.852430	3419.798387	23.619904
114.974044	3420.867785	23.624922
114.580993	3420.936048	23.629939
115.149299	3418.988630	23.634957
115.117873	3418.463100	23.639975
115.038470	3429.390146	23.644992
115.140004	3424.205844	23.650010
115.041110	3425.592492	23.655027
115.372434	3415.754653	23.660045
115.093751	3426.412293	23.665063
115.377597	3440.029918	23.670080
115.516585	3442.365093	23.675098
115.387946	3445.602159	23.680115
115.906318	3445.956974	23.685133
115.777645	3459.132618	23.690151
116.042321	3469.104587	23.695168
116.143522	3472.717040	23.700186
116.420025	3469.553604	23.705203
116.725922	3473.685382	23.710221
116.374671	3468.463420	23.715239
116.445880	3476.054146	23.720256
116.604201	3471.266774	23.725274
116.302478	3499.926490	23.730291
116.772102	3495.683312	23.735309
117.083288	3508.068762	23.740327
116.978871	3504.267121	23.745344
117.209392	3504.751102	23.750362
117.310649	3528.215579	23.755379
117.726520	3513.559156	23.760397
117.684006	3532.224809	23.765415
118.098687	3531.653766	23.770432
118.024359	3531.382610	23.775450
117.733579	3525.277281	23.780467
118.125306	3519.455066	23.785485
118.059024	3543.353653	23.790503
118.402155	3547.371005	23.795520
118.457874	3547.015711	23.800538
118.596890	3552.183138	23.805555
118.461558	3541.157759	23.810573
118.804957	3554.178937	23.815591
119.194157	3569.095143	23.820608
119.472724	3567.756378	23.825626
119.554938	3573.347442	23.830643
119.613485	3565.040291	23.835661
119.591337	3564.330914	23.840679
119.715725	3569.176319	23.845696
119.943890	3564.623843	23.850714
119.736634	3566.723807	23.855731
119.788480	3561.553199	23.860749
119.589930	3575.979641	23.865767
119.982899	3581.359789	23.870784
120.209670	3589.605215	23.875802
120.349981	3593.291546	23.880819
120.403307	3606.769507	23.885837
120.513060	3612.899008	23.890855
120.701700	3626.449083	23.895872
120.751309	3616.374260	23.900890
120.781971	3636.123338	23.905907
121.265034	3635.299600	23.910925
121.186541	3641.495323	23.915943
121.586905	3648.116557	23.920960
121.867541	3646.678611	23.925978
121.493333	3640.499243	23.930995
121.783353	3641.110797	23.936013
121.777869	3652.311624	23.941031
121.778873	3668.993600	23.946048
122.224366	3669.757391	23.951066
122.286712	3671.961964	23.956083
122.556227	3664.729427	23.961101
122.413208	3678.103719	23.966119
122.537115	3670.605091	23.971136
122.736748	3678.667631	23.976154
122.597597	3701.332689	23.981171
123.037816	3696.055605	23.986189
123.328637	3692.906292	23.991207
123.193810	3698.332521	23.996224
123.382783	3695.595399	24.001242
123.402547	3715.909055	24.006259
123.578326	3718.331107	24.011277
123.386516	3728.440244	24.016295
123.678650	3736.219353	24.021312
123.912602	3720.514365	24.026330
124.225400	3732.552436	24.031347
124.245091	3736.549362	24.036365
124.642394	3740.004965	24.041383
124.634923	3742.096287	24.046400
125.340482	3737.340296	24.051418
124.866775	3746.183340	24.056435
125.014852	3741.457827	24.061453
124.853149	3742.788751	24.066471
124.585745	3740.640636	24.071488
125.105504	3739.095367	24.076506
124.705622	3746.447248	24.081523
124.933239	3766.021342	24.086541
124.848394	3769.398488	24.091559
125.092521	3785.965128	24.096576
125.685317	3795.130908	24.101594
125.593886	3802.107685	24.106611
125.755402	3799.508968	24.111629
125.934140	3806.383529	24.116647
126.296809	3820.853124	24.121664
126.526564	3818.051741	24.126682
126.329302	3822.541365	24.131699
126.752290	3820.419901	24.136717
126.787984	3821.861870	24.141735
127.086120	3834.272185	24.146752
127.441153	3834.639093	24.151770
127.499487	3845.637339	24.156787
127.687441	3837.911854	24.161805
127.536694	3834.441865	24.166823
127.713076	3833.882703	24.171840
127.863772	3837.633524	24.176858
127.716006	3836.344453	24.181875
127.894844	3830.310092	24.186893
127.946904	3848.422593	24.191911
127.746127	3864.135679	24.196928
128.034190	3868.685930	24.201946
128.434374	3866.991524	24.206963
128.609706	3885.888893	24.211981
128.534562	3890.353987	24.216999
128.412333	3899.175938	24.222016
128.687456	3902.121414	24.227034
128.819240	3917.143573	24.232051
129.086750	3916.473244	24.237069
129.468969	3923.661463	24.242087
129.387771	3926.773826	24.247104
129.407519	3932.121780	24.252122
129.743253	3943.075742	24.257139
129.859020	3953.021092	24.262157
130.052047	3947.500949	24.267175
130.078847	3953.009971	24.272192
130.494837	3954.807557	24.277210
130.121325	3969.553528	24.282227
130.611650	3968.773068	24.287245
130.859098	3969.795290	24.292263
130.940225	3980.391371	24.297280
131.110281	3977.621106	24.302298
131.425069	3972.469832	24.307315
131.312915	3970.169190	24.312333
131.230259	3972.458846	24.317351
131.218146	3986.686662	24.322368
131.612816	3995.113986	24.327386
131.985930	3999.837231	24.332403
131.698700	3996.769387	24.337421
131.814907	3995.524801	24.342439
131.779601	4022.085143	24.347456
132.139238	4017.246163	24.352474
132.157093	4022.910257	24.357491
132.186474	4024.986853	24.362509
132.480867	4033.833224	24.367527
132.402774	4047.549891	24.372544
132.939361	4035.856927	24.377562
133.126349	4051.455206	24.382579
133.018996	4047.780315	24.387597
133.908228	4066.869993	24.392615
133.883789	4070.106079	24.397632
134.167276	4054.014152	24.402650
133.945923	4044.908468	24.407667
134.088897	4030.861401	24.412685
134.188547	4042.902713	24.417703
133.986848	4067.019430	24.422720
133.836395	4059.425861	24.427738
133.929535	4073.036235	24.432755
133.799621	4071.166933	24.437773
134.477294	4085.753940	24.442791
134.430801	4102.150099	24.447808
134.837177	4093.012913	24.452826
134.644400	4109.990080	24.457843
134.979723	4122.541342	24.462861
135.139222	4129.550748	24.467879
135.211738	4123.052698	24.472896
135.510800	4126.269888	24.477914
135.638127	4139.759682	24.482931
135.580389	4139.858269	24.487949
135.888875	4135.496302	24.492967
135.729022	4151.392299	24.497984
136.138399	4146.484405	24.503002
136.474004	4159.568807	24.508019
136.391847	4171.306405	24.513037
136.943628	4168.351629	24.518055
136.474064	4161.934648	24.523072
136.938609	4175.521423	24.528090
136.901172	4192.550140	24.533107
137.110857	4195.137941	24.538125
137.384962	4190.238254	24.543143
137.283208	4197.055471	24.548160
137.506458	4194.722105	24.553178
137.612608	4217.493383	24.558195
137.776549	4216.182600	24.563213
138.132296	4216.777392	24.568231
138.128035	4222.936640	24.573248
138.585006	4231.575863	24.578266
138.319253	4249.541804	24.583283
138.493713	4245.053152	24.588301
138.698772	4241.894305	24.593319
138.873104	4248.446901	24.598336
138.920342	4247.235766	24.603354
139.048810	4264.582820	24.608371
139.154160	4273.095997	24.613389
139.487523	4274.754520	24.618407
139.403930	4280.689090	24.623424
139.782396	4276.693515	24.628442
139.887137	4304.632962	24.633459
139.487114	4300.978902	24.638477
139.758588	4294.169842	24.643495
139.927465	4307.712754	24.648512
140.459349	4318.175371	24.653530
140.801087	4317.673872	24.658547
140.531575	4326.816167	24.663565
140.775038	4320.819747	24.668583
140.733985	4343.326552	24.673600
140.992848	4350.522791	24.678618
141.339510	4351.974360	24.683635
141.027895	4355.681746	24.688653
141.589833	4359.213007	24.693671
141.435968	4376.715609	24.698688
141.580545	4375.241848	24.703706
141.951893	4376.137267	24.708723
141.781020	4382.884103	24.713741
142.408355	4396.112565	24.718759
142.172217	4407.319828	24.723776
142.473800	4410.723308	24.728794
142.678065	4402.234475	24.733811
142.672623	4404.599614	24.738829
142.817029	4392.060919	24.743847
143.040770	4418.504227	24.748864
143.125557	4422.767372	24.753882
142.850541	4430.672620	24.758899
142.878521	4433.598474	24.763917
143.611954	4445.743079	24.768935
143.674720	4461.360756	24.773952
143.959608	4453.217669	24.778970
144.329371	4463.860009	24.783987
144.003927	4457.728549	24.789005
144.356189	4458.360155	24.794023
144.410745	4476.686786	24.799040
144.632159	4496.290778	24.804058
144.669011	4494.388302	24.809075
144.676330	4499.591236	24.814093
144.713825	4492.886194	24.819111
144.897076	4521.185537	24.824128
145.002764	4520.419119	24.829146
145.352255	4521.425272	24.834163
145.571034	4535.772081	24.839181
145.694269	4538.567202	24.844199
145.740371	4546.257110	24.849216
145.761246	4549.900044	24.854234
146.210395	4550.166729	24.859251
146.211310	4565.070992	24.864269
146.508423	4569.355728	24.869287
147.120380	4563.005241	24.874304
147.173779	4561.714306	24.879322
147.353483	4563.491232	24.884339
147.276322	4562.865340	24.889357
147.503734	4557.436162	24.894375
147.380062	4570.178756	24.899392
147.335040	4578.918607	24.904410
147.790932	4586.999045	24.909427
147.772581	4594.567338	24.914445
147.746132	4590.957681	24.919463
147.924375	4607.870022	24.924480
148.356552	4611.368483	24.929498
148.481982	4614.509777	24.934515
148.375531	4613.441403	24.939533
148.866266	4632.058277	24.944551
148.927725	4637.855559	24.949568
149.220579	4634.563966	24.954586
149.217242	4632.623236	24.959603
148.930924	4638.176463	24.964621
149.326159	4646.769433	24.969639
149.291671	4652.947243	24.974656
149.929819	4661.959938	24.979674
150.000439	4658.822478	24.984691
149.639373	4678.253788	24.989709
149.962392	4683.652596	24.994727
149.861078	4687.400060	24.999744
150.360315	4710.848065	25.004762
150.492880	4715.143545	25.009779
150.744340	4715.715458	25.014797
151.136901	4710.660540	25.019815
151.125689	4730.701055	25.024832
151.095657	4740.334755	25.029850
151.508263	4747.339549	25.034867
151.598609	4751.322280	25.039885
151.746005	4743.517618	25.044903
151.838415	4760.482923	25.049920
151.888345	4767.799002	25.054938
152.249162	4767.617232	25.059955
152.330154	4769.023831	25.064973
152.801154	4760.455994	25.069991
152.653628	4772.646684	25.075008
152.653064	4777.191826	25.080026
153.135333	4781.857074	25.085043
152.839447	4792.646856	25.090061
153.076298	4799.884750	25.095079
152.905483	4805.411037	25.100096
152.964555	4807.967959	25.105114
153.391325	4816.647947	25.110131
153.341880	4837.670718	25.115149
153.685399	4843.604094	25.120167
153.939138	4856.681369	25.125184
154.179007	4863.337570	25.130202
154.465018	4859.582401	25.135219
154.155318	4876.940456	25.140237
154.833807	4884.358869	25.145255
155.002898	4880.853021	25.150272
154.728947	4887.115458	25.155290
155.222017	4899.830244	25.160307
155.189338	4917.781199	25.165325
155.509685	4909.379198	25.170343
155.810561	4913.412960	25.175360
155.721588	4921.745229	25.180378
155.963199	4925.447789	25.185395
156.098519	4940.570364	25.190413
156.343298	4940.111678	25.195431
156.673257	4941.236866	25.200448
156.528978	4950.895122	25.205466
156.824458	4959.118871	25.210483
157.161739	4962.071586	25.215501
157.161956	4974.366346	25.220519
156.966342	4971.677712	25.225536
157.114932	4978.501075	25.230554
157.171303	4981.803515	25.235571
157.194102	5000.399850	25.240589
157.447783	5010.702648	25.245607
157.871728	5009.803185	25.250624
157.719280	5019.076137	25.255642
158.488759	5038.758612	25.260659
158.411296	5041.613827	25.265677
158.932075	5038.045783	25.270695
158.710824	5041.976214	25.275712
158.872023	5053.943531	25.280730
159.290616	5059.723585	25.285747
159.228604	5071.549877	25.290765
159.371494	5062.446304	25.295783
159.565151	5063.520823	25.300800
159.763400	5079.332480	25.305818
160.081993	5083.012882	25.310835
160.453301	5096.473344	25.315853
160.120002	5080.980231	25.320871
160.636935	5095.369550	25.325888
160.552565	5111.081539	25.330906
160.889002	5111.656727	25.335923
160.894021	5115.399289	25.340941
161.035112	5123.221030	25.345959
160.961663	5116.642776	25.350976
160.987324	5143.506010	25.355994
161.321602	5146.078069	25.361011
161.616542	5156.726968	25.366029
162.036038	5168.487794	25.371047
162.165333	5172.487810	25.376064
162.088936	5177.713491	25.381082
162.396747	5176.681243	25.386099
162.439829	5181.456338	25.391117
162.496049	5194.881628	25.396135
162.624561	5206.768626	25.401152
162.714822	5208.495852	25.406170
162.845955	5225.505653	25.411187
163.263703	5233.060336	25.416205
163.781524	5233.677958	25.421223
163.981149	5225.557254	25.426240
163.614605	5233.464666	25.431258
163.917125	5232.794791	25.436275
164.190946	5250.405551	25.441293
164.273387	5252.816124	25.446311
164.375941	5256.018829	25.451328
164.500088	5258.570564	25.456346
164.746229	5253.992577	25.461363
164.862288	5279.805404	25.466381
165.052187	5287.062323	25.471399
165.019770	5283.557456	25.476416
164.866008	5295.291206	25.481434
165.329115	5304.637262	25.486451
165.591530	5310.179424	25.491469
165.621870	5321.340854	25.496487
165.852271	5333.276450	25.501504
165.765879	5348.539296	25.506522
166.050944	5351.032115	25.511539
166.403801	5367.582427	25.516557
166.739395	5368.017575	25.521575
167.036925	5374.279316	25.526592
166.559806	5388.750776	25.531610
167.170590	5388.914327	25.536627
167.250259	5398.398739	25.541645
167.413426	5405.962574	25.546663
167.898764	5419.284721	25.551680
167.884955	5430.975712	25.556698
167.944649	5420.794891	25.561715
168.243167	5439.281514	25.566733
168.227343	5447.006529	25.571751
168.824796	5455.572769	25.576768
168.585430	5454.865794	25.581786
168.759992	5465.425356	25.586803
169.058608	5478.342926	25.591821
169.168011	5474.523127	25.596839
169.421993	5479.293326	25.601856
169.170345	5501.340463	25.606874
169.803996	5505.797359	25.611891
170.105253	5506.101154	25.616909
170.134190	5524.015818	25.621927
170.503622	5525.517289	25.626944
170.496595	5540.174908	25.631962
170.657973	5526.364469	25.636979
170.743684	5538.182406	25.641997
170.961159	5550.889004	25.647015
171.311754	5553.973520	25.652032
171.355659	5563.888470	25.657050
171.247605	5555.494043	25.662067
171.431241	5569.538876	25.667085
171.536904	5581.918252	25.672103
172.062670	5591.117064	25.677120
171.808603	5608.686451	25.682138
171.985510	5616.497782	25.687156
172.318685	5623.166426	25.692173
172.890168	5639.038146	25.697191
173.031052	5651.974095	25.702208
173.248377	5649.598182	25.707226
173.226802	5649.763250	25.712244
173.382864	5665.549400	25.717261
173.423582	5675.187710	25.722279
174.203120	5667.456727	25.727296
174.245769	5679.913559	25.732314
174.159098	5672.141677	25.737332
174.411450	5670.298683	25.742349
174.587338	5691.780690	25.747367
174.901241	5686.657364	25.752384
174.831253	5697.799441	25.757402
174.645178	5694.823989	25.762420
174.806046	5692.959908	25.767437
174.893109	5714.379466	25.772455
175.115492	5720.615982	25.777472
175.340932	5728.281502	25.782490
175.846177	5735.089468	25.787508
175.801770	5755.809397	25.792525
176.168005	5754.516195	25.797543
176.522826	5749.140341	25.802560
176.346961	5766.748939	25.807578
176.190153	5772.552056	25.812596
176.549893	5778.231068	25.817613
176.404289	5794.498112	25.822631
176.838216	5804.393537	25.827648
176.969233	5816.491661	25.832666
177.180537	5829.466505	25.837684
177.492501	5839.095452	25.842701
177.624801	5851.484020	25.847719
177.653077	5861.310380	25.852736
178.106649	5875.584887	25.857754
178.371067	5870.626430	25.862772
178.781542	5886.706208	25.867789
178.617129	5903.392338	25.872807
178.910642	5896.308792	25.877824
179.296753	5901.604640	25.882842
179.507534	5909.794078	25.887860
179.760474	5919.038250	25.892877
179.612422	5920.983797	25.897895
179.967576	5912.083244	25.902912
180.239242	5939.062266	25.907930
180.152222	5939.312207	25.912948
180.268083	5948.852393	25.917965
180.508762	5953.542239	25.922983
181.061254	5965.525808	25.928000
180.865296	5965.548835	25.933018
180.951161	5974.591501	25.938036
181.415950	5984.009359	25.943053
181.624075	6001.970512	25.948071
182.053052	5993.700392	25.953088
181.773129	6003.838566	25.958106
181.939443	6002.508343	25.963124
182.146831	6013.608660	25.968141
182.382011	6031.580333	25.973159
182.740036	6029.986021	25.978176
182.614843	6052.972316	25.983194
182.854093	6060.151324	25.988212
183.135654	6056.192617	25.993229
183.046424	6071.275477	25.998247
183.650042	6076.166767	26.003264
183.538314	6088.642389	26.008282
183.678653	6088.380543	26.013300
184.029933	6109.772647	26.018317
183.489918	6116.882993	26.023335
184.248741	6131.675866	26.028352
184.135918	6157.615445	26.033370
184.537879	6158.539776	26.038388
184.574136	6166.964600	26.043405
184.645294	6182.497528	26.048423
185.190932	6191.166479	26.053440
185.581770	6198.576435	26.058458
185.719627	6208.140704	26.063476
185.866698	6213.634544	26.068493
185.631040	6229.447513	26.073511
186.019936	6230.069985	26.078528
186.409001	6247.827396	26.083546
186.964103	6270.724226	26.088564
187.132024	6251.649096	26.093581
187.200078	6263.272015	26.098599
187.541626	6258.737019	26.103616
187.128333	6261.933173	26.108634
187.347766	6273.620042	26.113652
188.160672	6276.378488	26.118669
188.205824	6293.982587	26.123687
188.229769	6292.824774	26.128704
188.419906	6292.901240	26.133722
188.494818	6289.826546	26.138740
188.714746	6295.821105	26.143757
188.733400	6304.753791	26.148775
189.049942	6304.286341	26.153792
188.815029	6322.793785	26.158810
188.876266	6338.843625	26.163828
189.159067	6340.837616	26.168845
189.169709	6364.143710	26.173863
189.536070	6377.542290	26.178880
189.646725	6395.778373	26.183898
190.008437	6398.831288	26.188916
190.297722	6409.671793	26.193933
190.330612	6434.051013	26.198951
190.606097	6436.284096	26.203968
191.083958	6453.700167	26.208986
191.126794	6462.372167	26.214004
191.667307	6466.074445	26.219021
191.909307	6475.647627	26.224039
191.978151	6477.940918	26.229056
192.494354	6484.495351	26.234074
192.333884	6483.859543	26.239092
192.267462	6505.383557	26.244109
192.780675	6519.182489	26.249127
192.888010	6509.743709	26.254144
193.046766	6518.286278	26.259162
193.126608	6535.984934	26.264180
193.460909	6531.599139	26.269197
193.355986	6551.625182	26.274215
193.848944	6562.453342	26.279232
194.137133	6583.580856	26.284250
194.038663	6583.458568	26.289268
194.376241	6588.789463	26.294285
194.667960	6598.665612	26.299303
194.951534	6604.611157	26.304320
194.870821	6618.907050	26.309338
195.020785	6626.094008	26.314356
195.614692	6623.426403	26.319373
195.647556	6641.784343	26.324391
195.758435	6646.124900	26.329408
196.198037	6643.031510	26.334426
195.840184	6662.394615	26.339444
196.373552	6667.212655	26.344461
196.730486	6682.953178	26.349479
196.557466	6684.093240	26.354496
197.012557	6707.316021	26.359514
196.961300	6718.465165	26.364532
197.380836	6712.113396	26.369549
197.416766	6730.931711	26.374567
197.754686	6736.233457	26.379584
197.959453	6739.050919	26.384602
197.811201	6748.295042	26.389620
198.449322	6755.239777	26.394637
198.609915	6763.400159	26.399655
198.792556	6781.872882	26.404672
199.317810	6794.212890	26.409690
199.025615	6799.129045	26.414708
199.421257	6802.341832	26.419725
199.416030	6822.568319	26.424743
199.745635	6821.806470	26.429760
199.948287	6827.513444	26.434778
199.774383	6837.646411	26.439796
200.200750	6845.048428	26.444813
200.147070	6857.474085	26.449831
200.397141	6870.156657	26.454848
200.657243	6891.415258	26.459866
200.880626	6893.956346	26.464884
201.370045	6889.118647	26.469901
201.372306	6920.179153	26.474919
201.159575	6926.911156	26.479936
201.439179	6934.740009	26.484954
201.408395	6963.692756	26.489972
201.605568	6962.545600	26.494989
202.100052	6984.662680	26.500007
202.048545	7002.091374	26.505024
202.362760	7007.263232	26.510042
202.446392	7025.131156	26.515060
202.976112	7039.658770	26.520077
203.285182	7061.086718	26.525095
203.282696	7080.032320	26.530112
203.910986	7077.970187	26.535130
203.838787	7094.040517	26.540148
204.146912	7098.712451	26.545165
204.271269	7107.054662	26.550183
204.907771	7130.691494	26.555200
205.080433	7134.616303	26.560218
204.913828	7136.076707	26.565236
205.201967	7158.426684	26.570253
205.662730	7165.912953	26.575271
205.642007	7166.536325	26.580288
206.424536	7179.394084	26.585306
206.338319	7183.193197	26.590324
206.883864	7177.911323	26.595341
206.805284	7196.626267	26.600359
207.071306	7212.282332	26.605376
207.246957	7217.427573	26.610394
207.302638	7220.684911	26.615412
207.638945	7208.834525	26.620429
207.873236	7227.412643	26.625447
207.895603	7237.425151	26.630464
208.257963	7235.569285	26.635482
208.182598	7245.104888	26.640500
208.611580	7262.299940	26.645517
208.807981	7262.016980	26.650535
208.833509	7265.803916	26.655552
209.043620	7288.151240	26.660570
209.044525	7300.045183	26.665588
209.603851	7303.574408	26.670605
209.694046	7322.195395	26.675623
209.745042	7336.063682	26.680640
210.149925	7335.845458	26.685658
210.129978	7366.088951	26.690676
210.645884	7352.118202	26.695693
210.566141	7368.764283	26.700711
210.765553	7380.357610	26.705728
211.186792	7392.380537	26.710746
211.372253	7403.572894	26.715764
211.620450	7406.355717	26.720781
211.876867	7417.746650	26.725799
211.802458	7444.820973	26.730816
212.594486	7446.043153	26.735834
212.641120	7456.149456	26.740852
212.740804	7462.311663	26.745869
213.048598	7475.488500	26.750887
212.703246	7480.803571	26.755904
213.368020	7488.939942	26.760922
213.386356	7507.615577	26.765940
213.703070	7499.938285	26.770957
214.040130	7524.466536	26.775975
213.723814	7532.378582	26.780992
214.200428	7539.819870	26.786010
214.223747	7553.657482	26.791028
214.580267	7562.585356	26.796045
214.895449	7571.913929	26.801063
214.993273	7592.385851	26.806080
215.334649	7594.420721	26.811098
215.217732	7602.919713	26.816116
215.856850	7612.445173	26.821133
216.158124	7618.755241	26.826151
216.020741	7624.911069	26.831168
216.626521	7638.199404	26.836186
216.588864	7655.702140	26.841204
216.712183	7656.854653	26.846221
217.088532	7689.682993	26.851239
217.246583	7688.796692	26.856256
217.498859	7690.997564	26.861274
217.707306	7699.767281	26.866292
218.064514	7699.524650	26.871309
218.116410	7718.256418	26.876327
218.079064	7732.416159	26.881344
218.458249	7740.365988	26.886362
218.641546	7761.710150	26.891380
219.002507	7761.210892	26.896397
219.226091	7775.293605	26.901415
219.458573	7800.309068	26.906432
219.890322	7792.452689	26.911450
220.168365	7818.173516	26.916468
220.408842	7813.523268	26.921485
220.526935	7823.077605	26.926503
220.609474	7839.427128	26.931520
220.720253	7850.807034	26.936538
221.338360	7858.210084	26.941556
221.339049	7866.123381	26.946573
221.263989	7891.145785	26.951591
221.248864	7899.402010	26.956608
221.769576	7906.447040	26.961626
221.919610	7924.896557	26.966644
221.992253	7935.494332	26.971661
222.671454	7952.627443	26.976679
222.687533	7971.853035	26.981696
223.039273	7978.475494	26.986714
223.025475	7993.817087	26.991732
223.367983	8008.046528	26.996749
223.745851	8017.372076	27.001767
223.650917	8032.292315	27.006784
224.205262	8042.007731	27.011802
224.385175	8069.766506	27.016820
224.529965	8067.918993	27.021837
225.009196	8093.304474	27.026855
225.174968	8106.265877	27.031872
225.589199	8106.302110	27.036890
225.576570	8126.895407	27.041908
225.780035	8131.578672	27.046925
226.115033	8133.097133	27.051943
226.223065	8150.721236	27.056960
226.490092	8159.158540	27.061978
226.571254	8161.001818	27.066996
226.877714	8181.825159	27.072013
227.117193	8186.043232	27.077031
227.177289	8199.857199	27.082048
227.102534	8214.520618	27.087066
227.542627	8225.969164	27.092084
227.795693	8240.082856	27.097101
228.206559	8254.802988	27.102119
228.058470	8288.817478	27.107136
228.328193	8287.588900	27.112154
228.499205	8302.350357	27.117172
229.050141	8317.894176	27.122189
229.631528	8325.604441	27.127207
229.681017	8347.510349	27.132224
229.997065	8345.517870	27.137242
229.882367	8351.597749	27.142260
229.948298	8360.242540	27.147277
230.218920	8368.828243	27.152295
230.406784	8388.221258	27.157312
231.258038	8397.670328	27.162330
231.150426	8403.385906	27.167348
231.098297	8420.948592	27.172365
231.579971	8420.480538	27.177383
231.657543	8441.650902	27.182400
232.088544	8464.818799	27.187418
232.464937	8471.304255	27.192436
232.296548	8488.512083	27.197453
232.937830	8487.838000	27.202471
232.727401	8506.182432	27.207488
232.958238	8523.508543	27.212506
233.163349	8535.446802	27.217524
233.505920	8555.676206	27.222541
233.823378	8570.549161	27.227559
233.873948	8582.043539	27.232576
234.245542	8598.838333	27.237594
234.578505	8608.255164	27.242612
234.872383	8628.217008	27.247629
235.166251	8638.458801	27.252647
235.345576	8646.221600	27.257664
235.581953	8654.679996	27.262682
235.903615	8669.572830	27.267700
236.103247	8682.955271	27.272717
236.323623	8691.402156	27.277735
236.403700	8700.960160	27.282752
236.525578	8714.692659	27.287770
236.717746	8730.449096	27.292788
236.900097	8756.451963	27.297805
237.652297	8759.470638	27.302823
237.954080	8786.455811	27.307840
238.169884	8794.171679	27.312858
238.391585	8791.836334	27.317876
238.540677	8810.460336	27.322893
239.170888	8824.681484	27.327911
239.148628	8837.842400	27.332928
239.259607	8849.419138	27.337946
239.307521	8855.044534	27.342964
239.310409	8871.757277	27.347981
239.934789	8884.604008	27.352999
240.015242	8898.544401	27.358016
240.606430	8914.444514	27.363034
240.614752	8924.997661	27.368052
240.610982	8945.893047	27.373069
240.836269	8960.154561	27.378087
241.154129	8974.439364	27.383104
241.456082	8989.048222	27.388122
241.544778	9006.459833	27.393140
241.590553	9026.818529	27.398157
242.446213	9036.861233	27.403175
242.616976	9047.713709	27.408192
242.661149	9067.150241	27.413210
243.247144	9076.410448	27.418228
243.333629	9094.299910	27.423245
243.696342	9104.633806	27.428263
243.683112	9111.293521	27.433280
243.930413	9134.979645	27.438298
244.259370	9140.919421	27.443316
244.445476	9154.703899	27.448333
245.040283	9168.815412	27.453351
244.881572	9178.364386	27.458368
245.092988	9180.294147	27.463386
245.568095	9198.615696	27.468404
245.374777	9202.822967	27.473421
245.908232	9217.488247	27.478439
245.853052	9232.007555	27.483456
245.956514	9251.629865	27.488474
246.700532	9262.638896	27.493492
246.516734	9279.073367	27.498509
247.022481	9295.825418	27.503527
247.242611	9311.210691	27.508544
247.507663	9322.214756	27.513562
247.922164	9327.992338	27.518580
248.088829	9350.329259	27.523597
248.119223	9350.265968	27.528615
248.213199	9374.207072	27.533632
248.584921	9393.092683	27.538650
248.455921	9414.757809	27.543668
248.972979	9431.779129	27.548685
249.371377	9442.330282	27.553703
249.754363	9469.051859	27.558720
249.831182	9488.984533	27.563738
250.693487	9496.365263	27.568756
250.787937	9517.197866	27.573773
251.009011	9511.208728	27.578791
251.228698	9536.211694	27.583808
251.291879	9542.493402	27.588826
251.869690	9554.304553	27.593844
251.693968	9575.092932	27.598861
252.510614	9581.921137	27.603879
252.471822	9597.782834	27.608896
252.708287	9606.464668	27.613914
253.326771	9616.671476	27.618932
253.155001	9643.281921	27.623949
253.727165	9644.506026	27.628967
254.002086	9649.989346	27.633984
254.002109	9658.115557	27.639002
254.755335	9660.336986	27.644020
254.848771	9680.154491	27.649037
255.182940	9681.743358	27.654055
254.955393	9692.625966	27.659072
254.925860	9709.940527	27.664090
255.142640	9708.390520	27.669108
255.313323	9737.421291	27.674125
256.171293	9746.785765	27.679143
256.212268	9773.628276	27.684160
256.151113	9779.319320	27.689178
256.428907	9801.844091	27.694196
256.652734	9816.755764	27.699213
257.330389	9835.971768	27.704231
257.412852	9862.681510	27.709248
257.584886	9877.698714	27.714266
257.885450	9894.937562	27.719284
257.651174	9910.263125	27.724301
258.264643	9925.063920	27.729319
258.441048	9951.176850	27.734336
258.862707	9965.464264	27.739354
259.362087	9985.696305	27.744372
259.183842	10006.944957	27.749389
259.888671	10030.018586	27.754407
260.237482	10042.796846	27.759424
260.483316	10051.505733	27.764442
260.946372	10071.075822	27.769460
261.176031	10074.766607	27.774477
261.421877	10089.685131	27.779495
261.539804	10112.945055	27.784512
261.348911	10120.312913	27.789530
261.753649	10130.561734	27.794548
262.035716	10139.605012	27.799565
262.744086	10159.405614	27.804583
262.317525	10172.204393	27.809600
262.515618	10174.880978	27.814618
262.963394	10191.434001	27.819636
262.889788	10200.025675	27.824653
263.596676	10229.100142	27.829671
263.990444	10244.805790	27.834688
263.959591	10261.405024	27.839706
264.531861	10269.388761	27.844724
264.597052	10302.642674	27.849741
264.769705	10301.089674	27.854759
265.118077	10319.019084	27.859776
265.145650	10340.951823	27.864794
265.768750	10344.075694	27.869812
265.943534	10374.733029	27.874829
266.145420	10400.561213	27.879847
266.463110	10401.611637	27.884864
266.709650	10426.984191	27.889882
267.214686	10436.768326	27.894900
267.368727	10456.078839	27.899917
267.889126	10472.597284	27.904935
268.165043	10484.270015	27.909952
268.182383	10499.201532	27.914970
268.560355	10509.007532	27.919988
268.678386	10523.657689	27.925005
269.101509	10532.257130	27.930023
269.568944	10542.037311	27.935040
269.795975	10561.699066	27.940058
270.262161	10565.394145	27.945076
270.044537	10585.792898	27.950093
270.411763	10601.990179	27.955111
270.815965	10604.145041	27.960128
270.929467	10636.834638	27.965146
271.056220	10645.297265	27.970164
271.281938	10662.003345	27.975181
271.487168	10683.094867	27.980199
271.635549	10705.878681	27.985216
271.814653	10727.445722	27.990234
272.317631	10745.799882	27.995252
272.456053	10770.585013	28.000269
272.775232	10784.723095	28.005287
273.253195	10813.207016	28.010304
273.160884	10832.893598	28.015322
273.601776	10846.033065	28.020340
273.707786	10877.468540	28.025357
274.330041	10894.372368	28.030375
274.602724	10912.399270	28.035392
275.444461	10929.430680	28.040410
275.534502	10944.197729	28.045428
275.793701	10956.956097	28.050445
275.947430	10964.779407	28.055463
276.449656	10981.099690	28.060480
276.266633	10996.950394	28.065498
276.962643	11014.500799	28.070516
277.055690	11032.696234	28.075533
277.427798	11047.746017	28.080551
277.871736	11050.701143	28.085568
277.877944	11073.562585	28.090586
278.281553	11081.434407	28.095604
278.665731	11097.196050	28.100621
278.716554	11107.214143	28.105639
279.465130	11119.524486	28.110656
279.139498	11139.770058	28.115674
279.277630	11157.660355	28.120692
279.398885	11172.069477	28.125709
279.904027	11187.179309	28.130727
280.486447	11195.513225	28.135744
280.306593	11219.488214	28.140762
280.981401	11230.556551	28.145780
281.036279	11242.253813	28.150797
280.948582	11261.807790	28.155815
281.514715	11272.954023	28.160832
281.616026	11307.206997	28.165850
281.935413	11306.371013	28.170868
282.102986	11338.563015	28.175885
282.321250	11355.891900	28.180903
283.014806	11373.528194	28.185920
283.281241	11399.766447	28.190938
283.723095	11402.870108	28.195956
283.663409	11423.243772	28.200973
284.029962	11431.088808	28.205991
284.329779	11453.046539	28.211008
284.324599	11481.350033	28.216026
285.137935	11495.035058	28.221044
285.109339	11516.992084	28.226061
285.526273	11535.670241	28.231079
285.849680	11543.122224	28.236096
286.022743	11571.155275	28.241114
286.333721	11586.425260	28.246132
286.756905	11614.476866	28.251149
286.593043	11638.476615	28.256167
287.173710	11648.705166	28.261184
287.290726	11668.107561	28.266202
287.473795	11692.157119	28.271220
287.912254	11702.658220	28.276237
288.467541	11726.283782	28.281255
288.913966	11739.883199	28.286272
288.535887	11766.610075	28.291290
289.242160	11777.631035	28.296308
289.623872	11802.278200	28.301325
289.246132	11830.722762	28.306343
290.357155	11837.697832	28.311360
290.478001	11863.754504	28.316378
290.666545	11882.387347	28.321396
290.980170	11912.659026	28.326413
291.428963	11926.674227	28.331431
291.834507	11951.300340	28.336448
291.981611	11980.200373	28.341466
292.152629	11989.151188	28.346484
292.719660	12001.868883	28.351501
292.941897	12026.131494	28.356519
293.390026	12042.917223	28.361536
293.817297	12055.065580	28.366554
293.839619	12066.127459	28.371572
294.015895	12090.742883	28.376589
294.125150	12113.930692	28.381607
294.613685	12123.301778	28.386624
294.781686	12154.868144	28.391642
294.876856	12172.418410	28.396660
295.231164	12193.586504	28.401677
295.385074	12221.119577	28.406695
295.936945	12243.254126	28.411712
296.079706	12267.884821	28.416730
296.453078	12266.716804	28.421748
296.522288	12299.494303	28.426765
297.179634	12332.812744	28.431783
297.690923	12344.282397	28.436800
297.590031	12376.791945	28.441818
297.839573	12394.977189	28.446836
298.483715	12412.547158	28.451853
298.482246	12428.523642	28.456871
299.200782	12449.129078	28.461888
299.420840	12478.942962	28.466906
299.778020	12486.035218	28.471924
300.281113	12512.648981	28.476941
299.994839	12532.432763	28.481959
300.691718	12536.528215	28.486976
300.988852	12558.768396	28.491994
300.871645	12563.627382	28.497012
301.106594	12588.285851	28.502029
301.140592	12614.547208	28.507047
301.945536	12627.982446	28.512064
302.307126	12655.543338	28.517082
302.573047	12666.964008	28.522100
302.904820	12690.530268	28.527117
302.983400	12715.503203	28.532135
303.199140	12725.364197	28.537152
303.725139	12750.975436	28.542170
304.011360	12760.062047	28.547188
304.413022	12775.931172	28.552205
304.497151	12803.353859	28.557223
304.721770	12827.544780	28.562240
305.140907	12851.585346	28.567258
305.427253	12867.191558	28.572276
305.958259	12885.069160	28.577293
306.057648	12913.001680	28.582311
306.734667	12924.874539	28.587328
306.817809	12953.953937	28.592346
307.156275	12967.871683	28.597364
307.765668	12984.820808	28.602381
307.676726	13014.544985	28.607399
308.330042	13018.274278	28.612416
308.423981	13045.843886	28.617434
308.531411	13063.672025	28.622452
309.079485	13083.167083	28.627469
309.057912	13113.638315	28.632487
309.966167	13124.358858	28.637504
309.848195	13156.872788	28.642522
309.758274	13175.464952	28.647540
310.270075	13196.756424	28.652557
310.319081	13230.459494	28.657575
311.119500	13248.904374	28.662592
311.186630	13269.676985	28.667610
311.379488	13302.409244	28.672628
312.196937	13312.142633	28.677645
312.425682	13351.176041	28.682663
312.861867	13371.930248	28.687680
313.018282	13386.913894	28.692698
313.431640	13409.046170	28.697716
313.630072	13421.521831	28.702733
314.215072	13443.532762	28.707751
314.486444	13468.758613	28.712768
314.496097	13492.634660	28.717786
314.888458	13513.215063	28.722804
315.197777	13530.605269	28.727821
315.373924	13558.965887	28.732839
316.014185	13573.420465	28.737856
315.967623	13605.508982	28.742874
316.383444	13630.786823	28.747892
316.966239	13648.012113	28.752909
317.246238	13675.342381	28.757927
317.735297	13692.327923	28.762944
318.348569	13706.493951	28.767962
318.870712	13720.779091	28.772980
318.901044	13729.451560	28.777997
318.928284	13752.069002	28.783015
319.509850	13767.975510	28.788032
319.977485	13782.622752	28.793050
320.245775	13804.231126	28.798068
320.487761	13804.378655	28.803085
320.531221	13836.112307	28.808103
320.962888	13838.196878	28.813120
321.171829	13864.943493	28.818138
321.252234	13878.223894	28.823156
321.521353	13896.662889	28.828173
321.576159	13921.425688	28.833191
321.810958	13941.728540	28.838208
322.289984	13965.472427	28.843226
322.422907	13989.238961	28.848244
322.895443	14014.676644	28.853261
323.119483	14035.794624	28.858279
323.480185	14051.681229	28.863296
323.720466	14087.792525	28.868314
323.718590	14121.474332	28.873332
324.611074	14147.430575	28.878349
324.829479	14167.829408	28.883367
325.233366	14191.742088	28.888384
325.900732	14213.411033	28.893402
325.493418	14237.844178	28.898420
326.198191	14267.507028	28.903437
326.273083	14303.516938	28.908455
326.688058	14327.402764	28.913472
326.878421	14352.129593	28.918490
327.284463	14378.533939	28.923508
327.847402	14409.615337	28.928525
328.006597	14440.530362	28.933543
328.282237	14458.209246	28.938560
328.762177	14488.741875	28.943578
329.025480	14524.476793	28.948596
329.943196	14549.772278	28.953613
330.181537	14564.248555	28.958631
330.178559	14586.186554	28.963648
330.440620	14614.066683	28.968666
330.607319	14639.204491	28.973684
331.099428	14659.613796	28.978701
331.584325	14692.071965	28.983719
332.152876	14717.546860	28.988736
332.581077	14737.864395	28.993754
332.814498	14762.515367	28.998772
333.109187	14790.308438	29.003789
333.536454	14807.253357	29.008807
334.123026	14824.118339	29.013824
334.595375	14855.161989	29.018842
334.694097	14869.764092	29.023860
334.907588	14881.500756	29.028877
334.793172	14902.696361	29.033895
335.473567	14925.443732	29.038912
336.032659	14952.655861	29.043930
336.043920	14977.454254	29.048948
336.251207	14994.442081	29.053965
336.860869	15021.688510	29.058983
337.029082	15045.980311	29.064000
337.504087	15070.618555	29.069018
337.660182	15093.790229	29.074036
338.242207	15120.760846	29.079053
338.623165	15146.410885	29.084071
338.789839	15164.573527	29.089088
339.238399	15187.127940	29.094106
339.376416	15214.217907	29.099124
339.977767	15236.829060	29.104141
340.118269	15264.626388	29.109159
340.567558	15290.394587	29.114176
341.006358	15304.746922	29.119194
341.181657	15335.238556	29.124212
341.441904	15360.305242	29.129229
341.704529	15384.802579	29.134247
342.258984	15403.424586	29.139264
342.920158	15436.018971	29.144282
342.674173	15455.656171	29.149300
343.205216	15478.454248	29.154317
343.324074	15501.842290	29.159335
343.790786	15532.364865	29.164352
344.204778	15547.270027	29.169370
344.392140	15572.265562	29.174388
344.618895	15588.677052	29.179405
345.009697	15620.515854	29.184423
345.269404	15636.828944	29.189440
345.792406	15660.005311	29.194458
345.716123	15701.985520	29.199476
346.115903	15727.731075	29.204493
346.526031	15750.735533	29.209511
346.665325	15769.833328	29.214528
347.154578	15794.965225	29.219546
347.136323	15835.900607	29.224564
348.187297	15860.510907	29.229581
348.650787	15896.097457	29.234599
348.593057	15926.575162	29.239616
349.365928	15952.390143	29.244634
349.569007	15976.099075	29.249652
349.900998	15996.930600	29.254669
350.094406	16019.164280	29.259687
350.578762	16047.418287	29.264704
351.369561	16070.678584	29.269722
351.277523	16108.260039	29.274740
352.045161	16112.158711	29.279757
352.123677	16140.464285	29.284775
352.274151	16169.300222	29.289792
352.857938	16200.870193	29.294810
353.106379	16228.522028	29.299828
353.651166	16255.623617	29.304845
353.922539	16288.459168	29.309863
354.032560	16299.695386	29.314880
354.853618	16333.991076	29.319898
354.977331	16359.778581	29.324916
355.297364	16389.002969	29.329933
355.966645	16413.868000	29.334951
356.237649	16441.519609	29.339968
357.079079	16463.332959	29.344986
357.041955	16486.221740	29.350004
357.356194	16516.884865	29.355021
357.472199	16530.557157	29.360039
358.022149	16554.969271	29.365056
358.146156	16576.802205	29.370074
358.565275	16614.180410	29.375092
359.055274	16632.486613	29.380109
359.472719	16658.988888	29.385127
359.870224	16695.581139	29.390144
360.282530	16703.999648	29.395162
360.314084	16746.450153	29.400180
360.614991	16759.150987	29.405197
360.740618	16798.657310	29.410215
360.977079	16829.147884	29.415232
361.832939	16865.549580	29.420250
362.010408	16895.824629	29.425268
362.460949	16924.099919	29.430285
363.064156	16959.682976	29.435303
363.105061	16987.167084	29.440320
363.680930	17011.947593	29.445338
363.974186	17047.110819	29.450356
364.246290	17075.672841	29.455373
364.591502	17098.399879	29.460391
364.776682	17128.656737	29.465408
365.144027	17148.835994	29.470426
365.759127	17189.094536	29.475444
366.081686	17219.476998	29.480461
366.729841	17238.087151	29.485479
367.084910	17273.519637	29.490496
367.544920	17288.269007	29.495514
367.748947	17322.558529	29.500532
368.162014	17341.992726	29.505549
368.607933	17361.806137	29.510567
368.939744	17375.143903	29.515584
369.442329	17394.713099	29.520602
369.605779	17423.881682	29.525620
369.509433	17442.902180	29.530637
369.907986	17475.230365	29.535655
370.162092	17497.216377	29.540672
371.080974	17518.226973	29.545690
370.990538	17561.673942	29.550708
371.601551	17585.637666	29.555725
371.765979	17612.369353	29.560743
372.013921	17643.061297	29.565760
372.603737	17667.361262	29.570778
372.832757	17700.849782	29.575796
373.133936	17727.070343	29.580813
374.068382	17753.433630	29.585831
374.263188	17787.492333	29.590848
374.795406	17806.912084	29.595866
374.959610	17840.378508	29.600884
375.232154	17867.824158	29.605901
375.851944	17897.840236	29.610919
376.191432	17921.612925	29.615936
376.744023	17944.196453	29.620954
376.683223	17973.565482	29.625972
377.052190	18010.975629	29.630989
377.541064	18038.579655	29.636007
377.955995	18078.550320	29.641024
378.085336	18097.917282	29.646042
378.736273	18125.962827	29.651060
378.871500	18167.239555	29.656077
379.765306	18199.484030	29.661095
379.741810	18229.993399	29.666112
380.594679	18247.118916	29.671130
380.536996	18276.874188	29.676148
381.133142	18311.599005	29.681165
381.731318	18326.797788	29.686183
381.920680	18372.155343	29.691200
382.282251	18397.149952	29.696218
382.528335	18430.042795	29.701236
382.822434	18463.665534	29.706253
383.078913	18495.986111	29.711271
383.574478	18532.009690	29.716288
384.324287	18560.914539	29.721306
384.377274	18592.308917	29.726324
384.671354	18631.716041	29.731341
384.939026	18663.054527	29.736359
385.603377	18695.418339	29.741376
386.003496	18731.027768	29.746394
386.102170	18757.893562	29.751412
386.674955	18779.325630	29.756429
387.510315	18813.609900	29.761447
387.494448	18856.201323	29.766464
388.163299	18878.249791	29.771482
388.882158	18905.998489	29.776500
388.863273	18938.307165	29.781517
389.174295	18974.901403	29.786535
389.685263	19006.466696	29.791552
390.368785	19041.441848	29.796570
390.516193	19066.357818	29.801588
390.554397	19096.352496	29.806605
391.308922	19125.350560	29.811623
391.590378	19160.422456	29.816640
391.871838	19184.947513	29.821658
392.250001	19218.702899	29.826676
392.667035	19258.102186	29.831693
393.030753	19289.946205	29.836711
393.417321	19320.716038	29.841728
393.816241	19344.115163	29.846746
394.223318	19372.728153	29.851764
394.604611	19402.389127	29.856781
395.166747	19423.227853	29.861799
395.138054	19457.457803	29.866816
395.534509	19475.492541	29.871834
395.898825	19515.066695	29.876852
396.409146	19540.615415	29.881869
396.745002	19576.188405	29.886887
396.966627	19609.273648	29.891904
397.441821	19646.196909	29.896922
397.684111	19680.563771	29.901940
398.025739	19711.868332	29.906957
398.772580	19747.290110	29.911975
398.777054	19783.824913	29.916992
399.315847	19822.002449	29.922010
400.066705	19855.820412	29.927028
400.171554	19897.628281	29.932045
400.905662	19923.763301	29.937063
401.218118	19961.415771	29.942080
401.831959	19991.174889	29.947098
402.212693	20022.670633	29.952116
402.425167	20053.019715	29.957133
402.998947	20075.747672	29.962151
403.073547	20120.895617	29.967168
403.496237	20162.632624	29.972186
404.079124	20181.792925	29.977204
404.155079	20224.569700	29.982221
404.855924	20268.379909	29.987239
405.296344	20304.509451	29.992256
405.722113	20343.987098	29.997274
406.203264	20375.599321	30.002292
406.315055	20412.488236	30.007309
407.111535	20441.934133	30.012327
407.140996	20489.977359	30.017344
407.888012	20521.525362	30.022362
408.428523	20552.514780	30.027380
408.926999	20585.209264	30.032397
409.290733	20606.701923	30.037415
409.689866	20629.837930	30.042432
410.221737	20671.211267	30.047450
410.569740	20699.128376	30.052468
411.260359	20728.920242	30.057485
411.686045	20746.979892	30.062503
411.861074	20790.150062	30.067520
412.265585	20814.732816	30.072538
413.089934	20855.200493	30.077556
412.897065	20882.556250	30.082573
413.365804	20911.279909	30.087591
414.004311	20948.313023	30.092608
414.417166	20974.321528	30.097626
414.569847	21011.094617	30.102644
414.869265	21042.343997	30.107661
415.225249	21074.640460	30.112679
415.358112	21112.206973	30.117696
415.784658	21151.826712	30.122714
416.512970	21186.691711	30.127732
416.456483	21228.682523	30.132749
417.086446	21263.341641	30.137767
417.547866	21306.528804	30.142784
418.125202	21347.437452	30.147802
418.739347	21366.609701	30.152820
419.175801	21416.954871	30.157837
419.679903	21441.656080	30.162855
420.056394	21483.799765	30.167872
420.390369	21509.998745	30.172890
420.851452	21542.367007	30.177908
421.007042	21577.460042	30.182925
421.798648	21607.531602	30.187943
421.602662	21638.479345	30.192960
422.052188	21673.345762	30.197978
422.419204	21691.189082	30.202996
422.618648	21743.241074	30.208013
423.135755	21771.901430	30.213031
423.426779	21818.769878	30.218048
423.994601	21846.165286	30.223066
424.529095	21888.911386	30.228084
424.633527	21933.138402	30.233101
425.111937	21975.542381	30.238119
425.443929	22013.710229	30.243136
426.166309	22056.031461	30.248154
426.454126	22088.595005	30.253172
427.121407	22142.188585	30.258189
427.298783	22177.835867	30.263207
427.775943	22229.337239	30.268224
428.145301	22267.939403	30.273242
428.782088	22296.323823	30.278260
429.108766	22339.838668	30.283277
429.693674	22380.363819	30.288295
430.089266	22425.083204	30.293312
430.713741	22460.789542	30.298330
431.413339	22493.246296	30.303348
431.458461	22545.856103	30.308365
432.277661	22581.653463	30.313383
432.557451	22619.206885	30.318400
432.664597	22659.971030	30.323418
433.511406	22696.289152	30.328436
433.910487	22742.126779	30.333453
434.541204	22773.671435	30.338471
435.073195	22809.559382	30.343488
435.351179	22835.954170	30.348506
435.469129	22875.371982	30.353524
436.284035	22923.300008	30.358541
436.989314	22957.412422	30.363559
437.406161	22990.886696	30.368576
437.345864	23019.630525	30.373594
438.191622	23040.321146	30.378612
438.248227	23084.964332	30.383629
438.563448	23132.447384	30.388647
438.867905	23166.199212	30.393664
439.075118	23214.345314	30.398682
439.900842	23259.971811	30.403700
440.263610	23304.609058	30.408717
440.741022	23343.645201	30.413735
441.355068	23390.902908	30.418752
441.075868	23439.879174	30.423770
441.484969	23468.968693	30.428788
442.259075	23536.096296	30.433805
442.545534	23567.887051	30.438823
443.120477	23623.268317	30.443840
443.582992	23669.869062	30.448858
444.361626	23710.338516	30.453876
444.510928	23755.316617	30.458893
444.984931	23796.661430	30.463911
445.291364	23834.949557	30.468928
445.889243	23885.477176	30.473946
446.724160	23928.576082	30.478964
447.102471	23969.022512	30.483981
447.817584	24006.366600	30.488999
448.322990	24048.725548	30.494016
448.386956	24083.503018	30.499034
449.140782	24118.450252	30.504052
449.206546	24164.086659	30.509069
449.744695	24199.189600	30.514087
450.375468	24236.977090	30.519104
450.464707	24286.517716	30.524122
451.329250	24313.849078	30.529140
451.436462	24358.211238	30.534157
451.808186	24394.594259	30.539175
452.250266	24434.003029	30.544192
452.351116	24473.783761	30.549210
453.107733	24506.608672	30.554228
453.443180	24554.655323	30.559245
453.890112	24599.504382	30.564263
454.031334	24645.075963	30.569280
453.988838	24683.754905	30.574298
455.038387	24740.187248	30.579316
455.330857	24788.635924	30.584333
455.937935	24833.594720	30.589351
456.599747	24879.046077	30.594368
456.867307	24935.198436	30.599386
457.550940	24974.760877	30.604404
457.625904	25029.160187	30.609421
458.116435	25076.047148	30.614439
458.967861	25111.169508	30.619456
459.294915	25165.880798	30.624474
460.050738	25207.308546	30.629492
460.659840	25257.699574	30.634509
460.945577	25288.399147	30.639527
461.376604	25332.448440	30.644544
461.772826	25369.785192	30.649562
462.564344	25412.443970	30.654580
462.789707	25476.452711	30.659597
463.293369	25508.264744	30.664615
463.685712	25559.156194	30.669632
464.061357	25608.501832	30.674650
464.442626	25645.491536	30.679668
464.945883	25691.188923	30.684685
465.753872	25732.568302	30.689703
466.303778	25775.674862	30.694720
466.566352	25832.376660	30.699738
467.386983	25876.350256	30.704756
468.126690	25915.725792	30.709773
468.142518	25955.852064	30.714791
468.532257	25999.521919	30.719808
468.804363	26050.258075	30.724826
469.883430	26082.572116	30.729844
470.042229	26124.551939	30.734861
470.819834	26164.060562	30.739879
471.280111	26209.223890	30.744896
471.396459	26257.030815	30.749914
472.337961	26299.622813	30.754932
472.850557	26327.693818	30.759949
473.030806	26376.973048	30.764967
473.703942	26409.692396	30.769984
474.226210	26451.243804	30.775002
474.508274	26487.548304	30.780020
474.936993	26537.550238	30.785037
475.304485	26575.317044	30.790055
476.034937	26610.071341	30.795072
476.477670	26657.386899	30.800090
476.736123	26700.862597	30.805108
477.170779	26740.760507	30.810125
477.775732	26777.879656	30.815143
478.404721	26817.581554	30.820160
478.548282	26869.398126	30.825178
479.063741	26910.103214	30.830196
479.682850	26958.071772	30.835213
479.746008	26997.933961	30.840231
480.375220	27046.901064	30.845248
480.847393	27098.219158	30.850266
481.489197	27131.310980	30.855284
481.617774	27178.023809	30.860301
482.076220	27231.764082	30.865319
482.301044	27278.098483	30.870336
483.026756	27326.637164	30.875354
483.645173	27363.849978	30.880372
483.755045	27409.178522	30.885389
484.186309	27454.245801	30.890407
485.109958	27499.228563	30.895424
485.260027	27554.140737	30.900442
485.832817	27592.888410	30.905460
486.127059	27649.773885	30.910477
486.416921	27696.193276	30.915495
487.041431	27736.822323	30.920512
487.402431	27797.896029	30.925530
487.745615	27838.013495	30.930548
488.735852	27897.380873	30.935565
489.003304	27956.344384	30.940583
489.787171	28004.569337	30.945600
490.160538	28054.587957	30.950618
490.819652	28105.146208	30.955636
491.424914	28157.543238	30.960653
491.586905	28210.707810	30.965671
492.491592	28251.717583	30.970688
492.600286	28296.285192	30.975706
493.106474	28348.232292	30.980724
493.655719	28400.957951	30.985741
494.046860	28447.397287	30.990759
494.729018	28506.224631	30.995776
495.136352	28556.106570	31.000794
495.563724	28607.600579	31.005812
496.272520	28663.960169	31.010829
496.608599	28727.341092	31.015847
497.345750	28761.366682	31.020864
497.866654	28826.846873	31.025882
497.953894	28879.309707	31.030900
498.646678	28935.650740	31.035917
499.317648	28981.887452	31.040935
499.994067	29031.382344	31.045952
500.382505	29084.180844	31.050970
501.161389	29133.968248	31.055988
501.760751	29180.179476	31.061005
501.971620	29237.951515	31.066023
502.614488	29276.435792	31.071040
502.725078	29328.694196	31.076058
503.535289	29384.585023	31.081076
504.130040	29426.286139	31.086093
504.698283	29478.901486	31.091111
504.919047	29522.008714	31.096128
505.130458	29574.333195	31.101146
505.826202	29632.471148	31.106164
506.951658	29685.998191	31.111181
507.084454	29738.825190	31.116199
507.710231	29782.774675	31.121216
508.005813	29844.251265	31.126234
508.435432	29886.640196	31.131252
509.302312	29944.955942	31.136269
509.681237	29995.099084	31.141287
510.472530	30044.060408	31.146304
510.534420	30092.584121	31.151322
511.136836	30147.650441	31.156340
511.757631	30190.860335	31.161357
511.593922	30238.778150	31.166375
512.202069	30297.317718	31.171392
512.727596	30352.353231	31.176410
513.375751	30405.595460	31.181428
513.995809	30464.802496	31.186445
514.456688	30519.801903	31.191463
514.892069	30574.909821	31.196480
515.158332	30637.189124	31.201498
515.994917	30692.704294	31.206516
516.440001	30736.474669	31.211533
516.898402	30798.116959	31.216551
517.733757	30824.816637	31.221568
518.323345	30879.858975	31.226586
518.450098	30931.788171	31.231604
519.305905	30977.870198	31.236621
519.578070	31030.580200	31.241639
520.135408	31074.225562	31.246656
520.187196	31133.907503	31.251674
520.845893	31190.087876	31.256692
521.533255	31235.135133	31.261709
521.783265	31302.395295	31.266727
522.516842	31355.124573	31.271744
523.007598	31418.133059	31.276762
523.702604	31469.518603	31.281780
524.196047	31523.345139	31.286797
524.643776	31583.288076	31.291815
525.003621	31628.825963	31.296832
525.650235	31688.477612	31.301850
526.128979	31761.068877	31.306868
526.822991	31806.148044	31.311885
527.091109	31863.092515	31.316903
527.866192	31923.796520	31.321920
528.338380	31987.147729	31.326938
528.956640	32040.857368	31.331956
529.781372	32093.340267	31.336973
530.101177	32155.915822	31.341991
530.591562	32198.420159	31.347008
531.288047	32262.965852	31.352026
531.829848	32320.462882	31.357044
532.935513	32375.957752	31.362061
532.940393	32422.944811	31.367079
533.747428	32472.055423	31.372096
534.280871	32535.515206	31.377114
534.515342	32585.582315	31.382132
535.229012	32636.428570	31.387149
535.701092	32691.502297	31.392167
536.486508	32744.930814	31.397184
537.033417	32797.275591	31.402202
537.271775	32855.370467	31.407220
538.259712	32902.549551	31.412237
538.246594	32959.540915	31.417255
538.977745	33003.591428	31.422272
539.334583	33062.850711	31.427290
539.726670	33123.707393	31.432308
540.646528	33185.960083	31.437325
540.981245	33249.802410	31.442343
541.424818	33296.611895	31.447360
541.936899	33352.346881	31.452378
542.389562	33420.723864	31.457396
543.502199	33466.406976	31.462413
544.231644	33515.798384	31.467431
544.900062	33573.395272	31.472448
545.175899	33632.127075	31.477466
545.576540	33678.446069	31.482484
546.203466	33729.363446	31.487501
546.678718	33794.714976	31.492519
547.371997	33841.042775	31.497536
548.044468	33890.441492	31.502554
548.275219	33943.621408	31.507572
548.877185	33997.516372	31.512589
549.307599	34064.618273	31.517607
549.755590	34095.975442	31.522624
550.441835	34148.824986	31.527642
551.200361	34214.004948	31.532660
551.971360	34255.016108	31.537677
552.076851	34316.186202	31.542695
552.599052	34361.439129	31.547712
553.195385	34409.823089	31.552730
553.588560	34469.406071	31.557748
554.488664	34510.863518	31.562765
554.953239	34561.409337	31.567783
555.207590	34620.744390	31.572800
555.926546	34669.799892	31.577818
556.019560	34730.370693	31.582836
557.092961	34771.844253	31.587853
557.520025	34832.865068	31.592871
558.141144	34883.379581	31.597888
558.604168	34940.131203	31.602906
558.901160	35001.069966	31.607924
559.690000	35041.811725	31.612941
560.122538	35112.619087	31.617959
560.366074	35169.483492	31.622976
560.949307	35226.888346	31.627994
561.709511	35285.447586	31.633012
562.020842	35347.057367	31.638029
562.140770	35411.312182	31.643047
562.875075	35476.819492	31.648064
563.722356	35540.184357	31.653082
564.108065	35620.715650	31.658100
564.936133	35680.420051	31.663117
565.477950	35748.948960	31.668135
566.283280	35810.652172	31.673152
566.990387	35868.303683	31.678170
567.610184	35933.512838	31.683188
568.259435	35989.280664	31.688205
568.898908	36040.518132	31.693223
569.511014	36101.080243	31.698240
569.747760	36157.863672	31.703258
570.164484	36223.571424	31.708276
571.134196	36285.242749	31.713293
571.505477	36357.280245	31.718311
572.328872	36415.488682	31.723328
573.244865	36472.214368	31.728346
573.185375	36539.662204	31.733364
573.969550	36591.738930	31.738381
574.609014	36657.098940	31.743399
574.777178	36712.257388	31.748416
575.572151	36781.250163	31.753434
576.208945	36842.189417	31.758452
577.004676	36902.048394	31.763469
577.422767	36976.589820	31.768487
578.065935	37033.321374	31.773504
578.686225	37090.975367	31.778522
579.184559	37152.216325	31.783540
579.833543	37215.818723	31.788557
580.355348	37276.049356	31.793575
580.840366	37341.481575	31.798592
581.525947	37402.420952	31.803610
581.687517	37471.423305	31.808628
582.401085	37530.108009	31.813645
583.080231	37600.489763	31.818663
583.343387	37669.750664	31.823680
584.463432	37737.591716	31.828698
585.034094	37803.945719	31.833716
585.692017	37853.244076	31.838733
585.903041	37920.412388	31.843751
586.500740	37980.516010	31.848768
587.232536	38043.444752	31.853786
587.300682	38108.146963	31.858804
588.396294	38174.185039	31.863821
588.751671	38249.916261	31.868839
589.408950	38317.005886	31.873856
590.472719	38379.814578	31.878874
590.797690	38444.683818	31.883892
591.549960	38501.891161	31.888909
592.078428	38573.359037	31.893927
592.486458	38614.108721	31.898944
592.992345	38673.892068	31.903962
593.433000	38724.393495	31.908980
594.079543	38799.943090	31.913997
594.430447	38871.596181	31.919015
594.936812	38930.985716	31.924032
595.455251	38988.236426	31.929050
596.243206	39065.465130	31.934068
596.909018	39130.233059	31.939085
597.380808	39201.393946	31.944103
597.779534	39262.500637	31.949120
599.152001	39327.597436	31.954138
599.671020	39399.186896	31.959156
600.280670	39452.301350	31.964173
600.637442	39526.443496	31.969191
600.980068	39587.948826	31.974208
601.846288	39656.044191	31.979226
602.333578	39732.375277	31.984244
602.932023	39789.687857	31.989261
603.845025	39862.735490	31.994279
604.339959	39932.932573	31.999296
605.009902	39994.533478	32.004314
605.360598	40068.621993	32.009332
606.110082	40137.676024	32.014349
606.447366	40210.015303	32.019367
606.999083	40287.607072	32.024384
608.063449	40355.129271	32.029402
608.665165	40422.235793	32.034420
609.515069	40491.284007	32.039437
610.134147	40553.046725	32.044455
610.435615	40629.279684	32.049472
611.425956	40690.627869	32.054490
611.756584	40755.475921	32.059508
612.536263	40815.618711	32.064525
613.312053	40881.340630	32.069543
614.002172	40946.502395	32.074560
614.743600	41013.430106	32.079578
614.957431	41084.413650	32.084596
615.685352	41145.740468	32.089613
616.380521	41207.426491	32.094631
616.834363	41272.123377	32.099648
617.492197	41343.994184	32.104666
618.111466	41407.117240	32.109684
618.825681	41477.394415	32.114701
619.620782	41545.259123	32.119719
620.028930	41620.335666	32.124736
620.911838	41682.822519	32.129754
621.300135	41749.909186	32.134772
621.897436	41808.907792	32.139789
622.724457	41874.823662	32.144807
623.417098	41947.426654	32.149824
624.315175	42007.436919	32.154842
624.450276	42073.752109	32.159860
624.951051	42128.644489	32.164877
625.613767	42199.731678	32.169895
626.382571	42271.338304	32.174912
627.034082	42341.335510	32.179930
627.515686	42396.812774	32.184948
628.402761	42468.728941	32.189965
629.129055	42528.456747	32.194983
629.245070	42603.541393	32.200000
630.229606	42664.906554	32.205018
630.640473	42732.548706	32.210036
631.203329	42803.155876	32.215053
631.995193	42869.782002	32.220071
632.442936	42946.991661	32.225088
632.884306	43004.261253	32.230106
633.588676	43062.523103	32.235124
634.126500	43133.318788	32.240141
635.022119	43198.107154	32.245159
635.399682	43258.157051	32.250176
636.007971	43318.026890	32.255194
636.779820	43385.899006	32.260212
637.123521	43458.224623	32.265229
637.770556	43524.993871	32.270247
638.472590	43605.387861	32.275264
638.956931	43661.733558	32.280282
639.331918	43734.339232	32.285300
640.110889	43804.245061	32.290317
641.007113	43877.608088	32.295335
641.636545	43947.075047	32.300352
642.527476	44031.351693	32.305370
643.202298	44100.211792	32.310388
643.557639	44169.323921	32.315405
644.164938	44245.303223	32.320423
644.586616	44319.343254	32.325440
645.705978	44391.604140	32.330458
646.151289	44473.042100	32.335476
646.614552	44538.961254	32.340493
647.520794	44608.722725	32.345511
648.129663	44688.107405	32.350528
648.789125	44770.837405	32.355546
649.350411	44837.366589	32.360564
649.768832	44922.764254	32.365581
650.735155	44997.522042	32.370599
651.252675	45094.694659	32.375616
651.972690	45158.978900	32.380634
652.600793	45239.010038	32.385652
652.978703	45318.921865	32.390669
654.131533	45401.045679	32.395687
654.705857	45483.050832	32.400704
655.412160	45571.337314	32.405722
656.240962	45652.426415	32.410740
656.781857	45725.413354	32.415757
657.511240	45797.624161	32.420775
658.005566	45877.493828	32.425792
658.771968	45949.307527	32.430810
659.557962	46026.322303	32.435828
660.048751	46111.561794	32.440845
661.043975	46189.988898	32.445863
661.694823	46266.177553	32.450880
662.352275	46325.641470	32.455898
663.040251	46402.067683	32.460916
663.548606	46486.311228	32.465933
664.043680	46566.038411	32.470951
664.805028	46648.595565	32.475968
665.608603	46720.781828	32.480986
666.224385	46797.164732	32.486004
666.469906	46880.904030	32.491021
667.555108	46958.116251	32.496039
668.049966	47045.392981	32.501056
668.988615	47116.648909	32.506074
669.287019	47195.476506	32.511092
670.084412	47273.546067	32.516109
670.844098	47348.584176	32.521127
671.394021	47433.415587	32.526144
672.373432	47519.111105	32.531162
672.665926	47592.184208	32.536180
673.353112	47684.598625	32.541197
674.026148	47756.532502	32.546215
674.292376	47847.804645	32.551232
675.338983	47931.570777	32.556250
676.029897	48010.355753	32.561268
676.669814	48091.682316	32.566285
677.356248	48172.622552	32.571303
677.804190	48251.982445	32.576320
678.247753	48324.376457	32.581338
678.767035	48414.068247	32.586356
679.100188	48498.529679	32.591373
680.422196	48575.222911	32.596391
681.049937	48662.864031	32.601408
681.840329	48746.031836	32.606426
682.551972	48828.180278	32.611444
683.258363	48906.290512	32.616461
683.972816	48985.792533	32.621479
684.483612	49071.569370	32.626496
685.159335	49143.508012	32.631514
685.664372	49226.175557	32.636532
686.471202	49317.921127	32.641549
687.381003	49400.569836	32.646567
687.625615	49493.906311	32.651584
688.362657	49584.824572	32.656602
689.241818	49679.345593	32.661620
689.741784	49765.556855	32.666637
690.458409	49846.935012	32.671655
691.053061	49941.245391	32.676672
691.857396	50028.174976	32.681690
692.894645	50117.018357	32.686708
693.419566	50219.051452	32.691725
694.076977	50305.832876	32.696743
694.827842	50401.462021	32.701760
695.616518	50489.580716	32.706778
696.937127	50578.527795	32.711796
697.248982	50666.195537	32.716813
698.136435	50750.312979	32.721831
698.612012	50833.671371	32.726848
699.306324	50926.836135	32.731866
700.272091	51001.946020	32.736884
700.596790	51104.414885	32.741901
701.462989	51175.151417	32.746919
702.159566	51270.345303	32.751936
702.938215	51346.024446	32.756954
703.789110	51435.646992	32.761972
704.426723	51529.607381	32.766989
705.282087	51616.311384	32.772007
705.828471	51708.461992	32.777024
706.480297	51799.306826	32.782042
707.624833	51887.720463	32.787060
707.894814	51982.211346	32.792077
708.805628	52051.193726	32.797095
709.588717	52148.367629	32.802112
709.833959	52236.653638	32.807130
710.858811	52329.738852	32.812148
711.640577	52426.693241	32.817165
712.474102	52510.536604	32.822183
713.155519	52606.049090	32.827200
713.700698	52685.663789	32.832218
714.291326	52778.690299	32.837236
714.992024	52861.489430	32.842253
715.920701	52948.768466	32.847271
716.609163	53034.432341	32.852288
716.990868	53127.899414	32.857306
717.442712	53218.499619	32.862324
718.321447	53318.405499	32.867341
719.019913	53417.899446	32.872359
719.547768	53512.430870	32.877376
720.688547	53608.124973	32.882394
721.352548	53703.513006	32.887412
721.837677	53803.568598	32.892429
722.503972	53900.290331	32.897447
723.439273	53987.206435	32.902464
723.991446	54079.651558	32.907482
725.025655	54171.992105	32.912500
725.726301	54268.071818	32.917517
726.703053	54346.478248	32.922535
727.255038	54430.262653	32.927552
727.693494	54514.944444	32.932570
728.415904	54597.437694	32.937588
728.776510	54695.869312	32.942605
729.734900	54777.155371	32.947623
730.225868	54879.452181	32.952640
730.879583	54969.679526	32.957658
731.658829	55065.649020	32.962676
731.957762	55174.297653	32.967693
733.296942	55264.071749	32.972711
733.528404	55373.623558	32.977728
734.333629	55469.792907	32.982746
735.462704	55556.494302	32.987764
736.168747	55676.167645	32.992781
736.506626	55770.166289	32.997799
737.231546	55875.974362	33.002816
738.200974	55976.314681	33.007834
738.798102	56082.536757	33.012852
739.468993	56193.063002	33.017869
740.218916	56291.905731	33.022887
741.198442	56391.545072	33.027904
741.972383	56514.845625	33.032922
742.738212	56610.900629	33.037940
743.444391	56720.817335	33.042957
744.471849	56813.980142	33.047975
745.212745	56920.776896	33.052992
745.724930	57023.826877	33.058010
746.941691	57138.691472	33.063028
747.377431	57237.186422	33.068045
748.304908	57338.431542	33.073063
749.165948	57439.966212	33.078080
749.631981	57554.849947	33.083098
750.663217	57644.274959	33.088116
751.196562	57761.082462	33.093133
751.919499	57861.839549	33.098151
753.011863	57961.613395	33.103168
753.699169	58080.027702	33.108186
754.284928	58180.998665	33.113204
755.222920	58291.511271	33.118221
756.052622	58387.115534	33.123239
756.769127	58491.409487	33.128256
757.097018	58603.181210	33.133274
758.099742	58697.936773	33.138292
758.809071	58814.240980	33.143309
759.830292	58923.896444	33.148327
760.682502	59020.018205	33.153344
761.351923	59123.798672	33.158362
762.850039	59226.121750	33.163380
763.244159	59332.192369	33.168397
763.989174	59424.244822	33.173415
764.581349	59525.164567	33.178432
765.060175	59634.193128	33.183450
766.126980	59738.890613	33.188468
766.688103	59842.680037	33.193485
767.277786	59939.867116	33.198503
768.059004	60056.994499	33.203520
768.940374	60159.120942	33.208538
769.653162	60250.569422	33.213556
770.289027	60371.950853	33.218573
771.403137	60474.362714	33.223591
772.186014	60579.402227	33.228608
772.899529	60679.220547	33.233626
773.846639	60781.699499	33.238644
774.384050	60897.443651	33.243661
774.921198	61010.546576	33.248679
776.229334	61105.970759	33.253696
776.753242	61210.803542	33.258714
777.858404	61291.137304	33.263732
778.139440	61385.430662	33.268749
779.142190	61486.601923	33.273767
779.845127	61576.718022	33.278784
780.529427	61682.746564	33.283802
781.554232	61771.501916	33.288820
782.180058	61871.662917	33.293837
782.684721	61972.862081	33.298855
783.572273	62066.072220	33.303872
784.198652	62166.689663	33.308890
785.192483	62273.750911	33.313908
785.810418	62383.649734	33.318925
786.544095	62487.126972	33.323943
787.380123	62588.299640	33.328960
787.942726	62702.463274	33.333978
788.738748	62809.016428	33.338996
789.344597	62928.603860	33.344013
790.200959	63035.824552	33.349031
791.372792	63154.447378	33.354048
791.882591	63281.701227	33.359066
792.771267	63388.665562	33.364084
793.476436	63503.682362	33.369101
794.004300	63611.744202	33.374119
794.817533	63728.463744	33.379136
795.604750	63854.019062	33.384154
796.389082	63970.820604	33.389172
797.338473	64081.760904	33.394189
798.122903	64223.571098	33.399207
799.135277	64326.537345	33.404224
799.713939	64450.069983	33.409242
800.475678	64577.915940	33.414260
801.361616	64701.917612	33.419277
802.252039	64828.903062	33.424295
803.059748	64933.720458	33.429312
803.697386	65060.647985	33.434330
804.728150	65191.380129	33.439348
805.512125	65307.196730	33.444365
805.924620	65440.706781	33.449383
807.199903	65552.998127	33.454400
808.033367	65675.528646	33.459418
808.964367	65793.624769	33.464436
809.891480	65925.307961	33.469453
810.526996	66051.331499	33.474471
811.648064	66159.023948	33.479488
812.431755	66290.221074	33.484506
812.988128	66405.967602	33.489524
813.759805	66521.103847	33.494541
814.628766	66647.566508	33.499559
815.435837	66772.674580	33.504576
816.398094	66892.971830	33.509594
817.334335	67011.535458	33.514612
817.880539	67131.827018	33.519629
818.566517	67252.722054	33.524647
819.511982	67370.944773	33.529664
820.157138	67509.177554	33.534682
821.229122	67629.524081	33.539700
822.057763	67757.081197	33.544717
822.799026	67876.409012	33.549735
823.950099	67995.157595	33.554752
824.285383	68119.845878	33.559770
825.651312	68240.305325	33.564788
826.360193	68361.632845	33.569805
826.837299	68488.165011	33.574823
827.558470	68602.252420	33.579840
828.328614	68729.919903	33.584858
829.120301	68855.706725	33.589876
830.416018	68977.857506	33.594893
831.154353	69096.560380	33.599911
832.106608	69208.621123	33.604928
832.476389	69326.406186	33.609946
833.378861	69438.944269	33.614964
834.164326	69551.293638	33.619981
834.826479	69683.897653	33.624999
835.901306	69793.848276	33.630016
836.673224	69921.939922	33.635034
837.537913	70042.106757	33.640052
838.138707	70152.529658	33.645069
838.891538	70284.407878	33.650087
839.905697	70406.392085	33.655104
840.610600	70530.970089	33.660122
841.568169	70668.229526	33.665140
842.280726	70793.718344	33.670157
842.808324	70924.727184	33.675175
844.043310	71052.249440	33.680192
844.703319	71199.546169	33.685210
845.305675	71319.181774	33.690228
846.598617	71456.321210	33.695245
847.190650	71599.458374	33.700263
847.607970	71726.335724	33.705280
848.543326	71858.876349	33.710298
848.925654	72008.981637	33.715316
850.159218	72158.921885	33.720333
850.749282	72304.106603	33.725351
851.912522	72449.121609	33.730368
852.972282	72602.274557	33.735386
853.889793	72738.674753	33.740404
854.922869	72882.455722	33.745421
855.742352	73028.347239	33.750439
856.759255	73165.732867	33.755456
857.590796	73318.201334	33.760474
858.478701	73457.210127	33.765492
859.603223	73590.811456	33.770509
860.529162	73740.939972	33.775527
861.813239	73873.447852	33.780544
862.501734	74014.719306	33.785562
863.287299	74144.136481	33.790580
864.654495	74271.061295	33.795597
865.690458	74407.698981	33.800615
866.732977	74532.490764	33.805632
866.920120	74660.068351	33.810650
867.946300	74788.481889	33.815668
868.853878	74914.841342	33.820685
869.627182	75056.320507	33.825703
870.624769	75180.339151	33.830720
871.149713	75330.595456	33.835738
872.101356	75446.375834	33.840756
873.069368	75578.060816	33.845773
873.593060	75730.868920	33.850791
874.840682	75861.421487	33.855808
875.207189	75997.806590	33.860826
876.323768	76125.688001	33.865844
877.184328	76267.046643	33.870861
877.918847	76405.353094	33.875879
879.052275	76550.678449	33.880896
880.064170	76691.249439	33.885914
880.904893	76821.198174	33.890932
881.650791	76957.513779	33.895949
882.558009	77101.931379	33.900967
883.610241	77233.498412	33.905984
884.399667	77374.224362	33.911002
885.550662	77511.595931	33.916020
886.658276	77640.841154	33.921037
886.949192	77772.594199	33.926055
888.281917	77906.724861	33.931072
888.604427	78034.198254	33.936090
889.594010	78166.533871	33.941108
890.716192	78297.146779	33.946125
891.440478	78415.649583	33.951143
892.220433	78539.703986	33.956160
893.228802	78676.461084	33.961178
893.905590	78802.532894	33.966196
894.898599	78922.360271	33.971213
895.545100	79067.251163	33.976231
896.358454	79188.488675	33.981248
897.194712	79320.698303	33.986266
897.906055	79462.386485	33.991284
899.160318	79605.137078	33.996301
900.105790	79750.571221	34.001319
901.027963	79875.710171	34.006336
902.133724	80015.628587	34.011354
902.916564	80160.238251	34.016372
904.278673	80291.727667	34.021389
904.737180	80433.071523	34.026407
905.567554	80565.776511	34.031424
906.531860	80707.576150	34.036442
907.451277	80858.746907	34.041460
908.438158	80987.835181	34.046477
908.742344	81141.867810	34.051495
910.109225	81277.746272	34.056512
911.366754	81431.888908	34.061530
912.125327	81574.721211	34.066548
913.129607	81705.379623	34.071565
913.970038	81855.292103	34.076583
914.936318	81998.352089	34.081600
915.967265	82135.271821	34.086618
916.833628	82283.740357	34.091636
917.754269	82416.808123	34.096653
918.484888	82558.613612	34.101671
919.647292	82705.061988	34.106688
920.684163	82854.530947	34.111706
921.198256	83009.503084	34.116724
922.292240	83146.658839	34.121741
923.008167	83305.471623	34.126759
924.137313	83438.415912	34.131776
924.899638	83601.791108	34.136794
925.935992	83744.407476	34.141812
926.861176	83894.559652	34.146829
927.788601	84043.409048	34.151847
928.878272	84190.859580	34.156864
929.781649	84339.461769	34.161882
930.570194	84492.164956	34.166900
931.702299	84637.061435	34.171917
932.400634	84794.394099	34.176935
933.167390	84938.941600	34.181952
934.314964	85096.973954	34.186970
935.241764	85255.417206	34.191988
936.376441	85396.711351	34.197005
937.144724	85542.584781	34.202023
938.406667	85689.826493	34.207040
939.055665	85846.067082	34.212058
939.781745	85999.404238	34.217076
941.384488	86142.036545	34.222093
942.225186	86295.964143	34.227111
942.961670	86453.839516	34.232128
944.311078	86588.290352	34.237146
945.019521	86738.256210	34.242164
945.886349	86893.499585	34.247181
946.643201	87035.290048	34.252199
947.781531	87173.987194	34.257216
948.664465	87333.945125	34.262234
949.218193	87482.726324	34.267252
950.617136	87636.785517	34.272269
951.102769	87782.795512	34.277287
952.221427	87936.523318	34.282304
953.357390	88073.340341	34.287322
954.372914	88216.322774	34.292340
955.202047	88351.578442	34.297357
955.842336	88501.737607	34.302375
956.773626	88638.199373	34.307392
957.876939	88788.549571	34.312410
958.479335	88940.755506	34.317428
959.508255	89083.532095	34.322445
960.195029	89246.408459	34.327463
961.546688	89394.196335	34.332480
962.123951	89549.960615	34.337498
963.263348	89707.018920	34.342516
964.202476	89863.257002	34.347533
965.377278	90026.412374	34.352551
966.327151	90188.194738	34.357568
967.416016	90330.405590	34.362586
968.182014	90498.992249	34.367604
969.127237	90658.709020	34.372621
969.924913	90827.248435	34.377639
970.900914	90985.399038	34.382656
971.835337	91149.804271	34.387674
972.740340	91309.816804	34.392692
974.042026	91477.460965	34.397709
975.020573	91640.773635	34.402727
975.918296	91806.315978	34.407744
977.299583	91960.171718	34.412762
977.945685	92122.599549	34.417780
979.371896	92283.608293	34.422797
980.426645	92454.249482	34.427815
981.318392	92621.361707	34.432832
982.481430	92766.315220	34.437850
983.020631	92938.918556	34.442868
984.360750	93096.807492	34.447885
985.398739	93266.843169	34.452903
986.336678	93434.560952	34.457920
987.196454	93580.987266	34.462938
987.997284	93762.458930	34.467956
989.175206	93924.462659	34.472973
990.280231	94098.803553	34.477991
991.226313	94254.233190	34.483008
992.381670	94420.320307	34.488026
993.238937	94600.105073	34.493044
994.168948	94761.072885	34.498061
994.937459	94932.247047	34.503079
996.004089	95095.321315	34.508096
997.323761	95260.317134	34.513114
998.281959	95437.464319	34.518132
998.932631	95599.211727	34.523149
1000.148642	95775.793292	34.528167
1001.202395	95940.236232	34.533184
1002.112049	96113.205643	34.538202
1003.117574	96279.868065	34.543220
1004.386025	96449.608993	34.548237
1005.315366	96630.542330	34.553255
1005.953140	96795.926955	34.558272
1007.135845	96968.863472	34.563290
1007.745431	97149.068444	34.568308
1008.908597	97327.176381	34.573325
1009.659998	97502.669480	34.578343
1010.597920	97679.956195	34.583360
1011.853063	97856.007863	34.588378
1012.818583	98054.684148	34.593396
1014.014970	98221.005033	34.598413
1014.955433	98398.574935	34.603431
1015.627260	98575.937265	34.608448
1017.048223	98750.017831	34.613466
1017.788085	98935.683953	34.618484
1019.146871	99106.421825	34.623501
1020.211640	99265.769217	34.628519
1021.051719	99433.606790	34.633536
1021.980902	99593.858680	34.638554
1023.165196	99771.961342	34.643572
1024.277373	99931.931852	34.648589
1025.284480	100093.706157	34.653607
1025.912219	100269.143875	34.658624
1026.860861	100438.369323	34.663642
1027.958841	100609.869495	34.668660
1028.867657	100790.544695	34.673677
1030.247375	100965.324667	34.678695
1031.306021	101139.044566	34.683712
1032.412095	101310.440441	34.688730
1033.417778	101487.128290	34.693748
1034.262533	101655.536821	34.698765
1035.497560	101834.468524	34.703783
1036.256375	102019.957580	34.708800
1037.361104	102194.170837	34.713818
1038.294126	102388.219633	34.718836
1039.424837	102563.266876	34.723853
1040.509142	102754.108458	34.728871
1041.572463	102931.765415	34.733888
1042.764155	103111.732539	34.738906
1043.500028	103309.588352	34.743924
1044.700896	103492.197053	34.748941
1045.675323	103673.869320	34.753959
1046.275644	103869.180926	34.758976
1047.673204	104049.494069	34.763994
1048.867108	104253.132271	34.769012
1049.483000	104439.871633	34.774029
1050.903035	104631.329964	34.779047
1051.818314	104829.382879	34.784064
1053.025524	105020.372632	34.789082
1054.061875	105228.046545	34.794100
1055.067954	105419.845009	34.799117
1056.272034	105607.115969	34.804135
1057.310424	105815.427414	34.809152
1058.501874	106001.892670	34.814170
1060.061851	106199.925238	34.819188
1060.681401	106393.631144	34.824205
1062.191077	106576.640769	34.829223
1062.812270	106773.806898	34.834240
1064.199590	106955.116803	34.839258
1065.191579	107156.822160	34.844276
1065.864655	107341.089945	34.849293
1067.007330	107538.200816	34.854311
1068.070219	107734.376357	34.859328
1069.447164	107928.994113	34.864346
1070.554991	108120.554500	34.869364
1071.311762	108317.696886	34.874381
1072.512116	108506.166752	34.879399
1073.605956	108706.042895	34.884416
1074.906053	108893.650303	34.889434
1075.555490	109093.273442	34.894452
1076.590638	109281.446681	34.899469
1078.162118	109490.977866	34.904487
1078.885733	109688.528383	34.909504
1080.349779	109883.842485	34.914522
1081.102461	110083.012461	34.919540
1082.235016	110283.527167	34.924557
1083.567066	110475.219105	34.929575
1084.364616	110665.151286	34.934592
1085.432765	110860.854512	34.939610
1086.429633	111080.665045	34.944628
1087.754640	111269.209416	34.949645
1089.235581	111461.922394	34.954663
1089.992256	111659.367634	34.959680
1090.916332	111843.839767	34.964698
1092.390804	112024.180970	34.969716
1093.361369	112206.506905	34.974733
1094.487338	112384.817804	34.979751
1095.390354	112572.845423	34.984768
1096.616042	112746.416818	34.989786
1097.422669	112943.888285	34.994804
1098.163891	113132.567198	34.999821
1099.588526	113310.631954	35.004839
1100.699808	113509.665998	35.009856
1101.829972	113708.102893	35.014874
1102.703391	113896.118985	35.019892
1103.920517	114099.523221	35.024909
1104.870501	114295.903652	35.029927
1106.163724	114501.971433	35.034944
1107.263115	114689.816112	35.039962
1108.423335	114883.708015	35.044980
1108.807668	115089.968363	35.049997
1110.369736	115286.685267	35.055015
1111.177463	115498.579959	35.060032
1112.538734	115708.256177	35.065050
1113.646646	115917.202962	35.070068
1114.758914	116127.265528	35.075085
1116.239506	116327.981520	35.080103
1116.943991	116544.234262	35.085120
1118.387008	116737.889346	35.090138
1119.402040	116951.876520	35.095156
1120.411764	117164.852527	35.100173
1121.847680	117377.100782	35.105191
1123.071461	117581.821257	35.110208
1124.035839	117797.508310	35.115226
1125.341782	118009.516629	35.120244
1126.340683	118224.592964	35.125261
1127.975273	118424.043722	35.130279
1128.653856	118632.536394	35.135296
1129.893720	118842.825793	35.140314
1131.011459	119052.173880	35.145332
1132.054127	119261.979385	35.150349
1133.179608	119474.788536	35.155367
1134.382461	119696.038430	35.160384
1135.723829	119904.265904	35.165402
1136.820944	120112.674628	35.170420
1138.350276	120327.425367	35.175437
1139.064367	120524.406916	35.180455
1140.124988	120759.260057	35.185472
1141.748031	120955.574670	35.190490
1142.886498	121176.187408	35.195508
1143.644384	121395.762212	35.200525
1145.186134	121607.212736	35.205543
1145.953884	121817.880301	35.210560
1146.956801	122028.459791	35.215578
1148.250939	122236.762229	35.220596
1149.353926	122463.384605	35.225613
1150.416101	122682.842577	35.230631
1151.789987	122906.065206	35.235648
1152.681258	123119.028031	35.240666
1154.186059	123345.438588	35.245684
1155.020677	123558.553302	35.250701
1156.438479	123772.042033	35.255719
1157.293492	123994.965660	35.260736
1158.380856	124217.117455	35.265754
1159.461038	124438.689083	35.270772
1160.831861	124658.579371	35.275789
1161.531451	124880.280512	35.280807
1163.204638	125118.311114	35.285824
1164.148744	125336.565870	35.290842
1165.514747	125557.084482	35.295860
1166.428709	125774.967133	35.300877
1167.790760	125985.375470	35.305895
1169.077101	126200.398571	35.310912
1170.293857	126401.366016	35.315930
1171.633961	126611.934373	35.320948
1172.518615	126819.626269	35.325965
1174.141533	127018.515335	35.330983
1175.072411	127225.543237	35.336000
1176.029317	127435.039826	35.341018
1177.297998	127632.546463	35.346036
1178.464164	127854.889076	35.351053
1179.528673	128063.598942	35.356071
1180.582473	128275.544164	35.361088
1181.312264	128492.500439	35.366106
1182.965406	128704.336822	35.371124
1183.898064	128937.892798	35.376141
1184.881845	129158.614356	35.381159
1186.045020	129394.252447	35.386176
1186.836836	129616.568065	35.391194
1188.490951	129853.193201	35.396212
1189.259002	130095.645419	35.401229
1190.718673	130324.789380	35.406247
1191.736764	130558.457326	35.411264
1192.584039	130806.124458	35.416282
1194.264361	131042.234420	35.421300
1195.430355	131293.947122	35.426317
1196.482034	131527.109567	35.431335
1197.990874	131775.866464	35.436352
1198.915290	132012.995919	35.441370
1200.072387	132254.487520	35.446388
1201.369451	132508.292447	35.451405
1202.284557	132754.264723	35.456423
1203.928814	133007.940126	35.461440
1204.888855	133256.659730	35.466458
1206.479443	133502.830289	35.471476
1207.434490	133757.297380	35.476493
1208.825954	134002.401701	35.481511
1210.015771	134245.259226	35.486528
1211.394898	134498.254779	35.491546
1212.713014	134752.111785	35.496564
1213.815374	135003.496194	35.501581
1215.096317	135243.544234	35.506599
1216.631638	135491.171503	35.511616
1218.031447	135733.802471	35.516634
1219.553842	135977.860278	35.521652
1220.311276	136221.260269	35.526669
1221.686093	136465.041772	35.531687
1223.027749	136712.279108	35.536704
1224.153818	136953.075125	35.541722
1225.830328	137189.090759	35.546740
1226.906700	137439.863980	35.551757
1228.418332	137665.285365	35.556775
1229.664286	137913.422234	35.561792
1230.502079	138152.778387	35.566810
1232.134768	138389.621157	35.571828
1233.297120	138628.064843	35.576845
1234.424930	138865.463529	35.581863
1235.446852	139105.861048	35.586880
1236.342271	139348.449376	35.591898
1237.974334	139588.508536	35.596916
1239.199212	139834.824393	35.601933
1240.611699	140075.443135	35.606951
1241.586387	140318.342233	35.611968
1242.730625	140569.495055	35.616986
1244.152462	140799.935289	35.622004
1245.060075	141061.794755	35.627021
1246.749159	141302.731394	35.632039
1247.709378	141553.325808	35.637056
1248.769861	141791.897076	35.642074
1250.164754	142019.889868	35.647092
1251.162090	142261.099653	35.652109
1252.044004	142482.954078	35.657127
1253.378097	142733.495169	35.662144
1254.333411	142980.511969	35.667162
1255.814448	143214.179325	35.672180
1256.891021	143469.422133	35.677197
1258.075684	143711.955100	35.682215
1259.215149	143965.567907	35.687232
1260.469610	144227.812175	35.692250
1261.919013	144477.382791	35.697268
1262.731899	144737.598686	35.702285
1263.941985	144993.324948	35.707303
1265.281726	145250.819723	35.712320
1266.432862	145527.154590	35.717338
1267.951483	145787.667272	35.722356
1268.988308	146058.305584	35.727373
1270.131596	146317.425699	35.732391
1271.810245	146585.539596	35.737408
1272.900855	146871.583904	35.742426
1274.370283	147130.922242	35.747444
1275.462886	147405.226562	35.752461
1276.577158	147681.406370	35.757479
1278.036073	147948.298344	35.762496
1279.284161	148235.557495	35.767514
1280.823542	148508.274280	35.772532
1281.819935	148787.715984	35.777549
1283.186798	149065.094647	35.782567
1284.840921	149335.743910	35.787584
1286.015887	149624.091288	35.792602
1287.835969	149890.798045	35.797620
1288.786093	150171.107552	35.802637
1290.360286	150448.665159	35.807655
1291.654428	150719.726381	35.812672
1292.861673	151000.862052	35.817690
1294.361254	151275.229107	35.822708
1295.523842	151556.109921	35.827725
1296.928918	151832.741664	35.832743
1298.263352	152102.448929	35.837760
1299.570409	152391.645425	35.842778
1301.223085	152650.877610	35.847796
1301.963524	152929.339497	35.852813
1303.240692	153206.281350	35.857831
1304.853748	153486.087104	35.862848
1306.233187	153767.163895	35.867866
1307.693425	154043.117448	35.872884
1308.912734	154322.816724	35.877901
1310.042241	154604.765378	35.882919
1311.396417	154868.285777	35.887936
1312.644563	155161.939706	35.892954
1314.383009	155437.971277	35.897972
1315.688899	155728.042678	35.902989
1316.837069	156002.526673	35.908007
1318.255764	156277.082023	35.913024
1319.094535	156565.689132	35.918042
1320.800657	156831.929874	35.923060
1322.449741	157119.709355	35.928077
1323.330252	157403.038373	35.933095
1324.943128	157682.899288	35.938112
1326.125514	157952.735305	35.943130
1327.642115	158229.888450	35.948148
1329.266577	158513.558996	35.953165
1330.352522	158792.030387	35.958183
1331.656288	159071.127364	35.963200
1332.895702	159344.908615	35.968218
1334.062983	159619.375995	35.973236
1335.546253	159897.307147	35.978253
1336.805428	160175.708551	35.983271
1338.341186	160442.407057	35.988288
1339.158431	160705.496116	35.993306
1340.682752	160969.155071	35.998324
1341.862601	161235.448068	36.003341
1342.933475	161505.693741	36.008359
1344.122995	161766.000246	36.013376
1345.376636	162051.177295	36.018394
1346.804373	162326.571001	36.023412
1348.278601	162613.986411	36.028429
1349.336571	162892.489867	36.033447
1350.583238	163172.638710	36.038464
1351.689507	163468.545203	36.043482
1353.048260	163759.971327	36.048500
1354.287294	164053.423880	36.053517
1355.761145	164350.328783	36.058535
1356.940991	164642.615153	36.063552
1358.210815	164951.383054	36.068570
1359.888334	165245.354869	36.073588
1361.137629	165558.990015	36.078605
1362.583791	165868.547306	36.083623
1363.845551	166166.108670	36.088640
1364.982437	166471.521461	36.093658
1366.523319	166789.824610	36.098676
1367.946744	167089.839739	36.103693
1369.189195	167400.418442	36.108711
1370.935140	167713.301594	36.113728
1372.016752	168037.259936	36.118746
1373.756847	168338.487304	36.123764
1375.081938	168662.562170	36.128781
1376.355934	168978.564792	36.133799
1378.138381	169289.156094	36.138816
1379.409707	169610.010836	36.143834
1380.587509	169918.967900	36.148852
1381.880820	170237.247439	36.153869
1383.552926	170556.925881	36.158887
1385.370622	170878.219443	36.163904
1386.588565	171189.767068	36.168922
1387.667758	171500.184925	36.173940
1389.136399	171821.593431	36.178957
1390.485689	172139.610239	36.183975
1392.072315	172461.206656	36.188992
1393.660342	172787.500408	36.194010
1394.814711	173104.502624	36.199028
1396.303707	173424.040487	36.204045
1397.920685	173745.120261	36.209063
1398.997477	174060.885274	36.214080
1400.854819	174383.135187	36.219098
1402.370785	174703.501979	36.224116
1403.999252	175020.463849	36.229133
1405.082267	175339.332713	36.234151
1406.718776	175648.898545	36.239168
1408.287418	175971.498556	36.244186
1409.655508	176286.113025	36.249204
1411.349860	176591.715585	36.254221
1412.981148	176908.257642	36.259239
1413.949217	177214.707446	36.264256
1415.210355	177525.463859	36.269274
1416.949091	177836.105195	36.274292
1418.343449	178146.983034	36.279309
1419.333978	178460.379005	36.284327
1421.085993	178777.344373	36.289344
1423.027053	179082.070926	36.294362
1424.113536	179399.416654	36.299380
1425.122949	179713.769071	36.304397
1426.774387	180017.990577	36.309415
1428.105937	180334.628870	36.314432
1429.337634	180652.085196	36.319450
1430.769738	180962.961110	36.324468
1432.518893	181257.502169	36.329485
1433.629101	181557.950899	36.334503
1435.200456	181851.293485	36.339520
1436.404063	182156.781791	36.344538
1437.753138	182454.403751	36.349556
1439.167599	182760.787229	36.354573
1440.660331	183069.837699	36.359591
1441.907049	183372.025672	36.364608
1443.150877	183693.724850	36.369626
1444.607456	183997.036678	36.374644
1446.224377	184313.181786	36.379661
1447.410011	184624.703514	36.384679
1448.865230	184935.611259	36.389696
1450.189394	185265.734675	36.394714
1451.567810	185584.795155	36.399732
1453.581491	185922.830739	36.404749
1454.418538	186254.703331	36.409767
1456.080648	186580.221678	36.414784
1457.228120	186922.760295	36.419802
1458.796671	187252.512256	36.424820
1460.513313	187584.615395	36.429837
1461.807658	187932.733767	36.434855
1463.267373	188257.241513	36.439872
1464.591445	188598.694647	36.444890
1466.145301	188934.996082	36.449908
1467.770740	189283.118607	36.454925
1469.273683	189623.240656	36.459943
1470.691657	189972.835983	36.464960
1471.554572	190320.087754	36.469978
1473.369560	190667.704699	36.474996
1474.851720	191012.712795	36.480013
1476.368713	191380.757868	36.485031
1477.670255	191724.416149	36.490048
1479.243872	192089.866434	36.495066
1480.639610	192436.763016	36.500084
1482.323037	192798.289350	36.505101
1483.750265	193160.812251	36.510119
1485.110376	193527.461554	36.515136
1486.588405	193895.045653	36.520154
1488.318513	194249.526857	36.525172
1489.767072	194605.681561	36.530189
1491.083785	194970.061245	36.535207
1492.943258	195335.267391	36.540224
1494.381832	195711.209380	36.545242
1495.758095	196071.726011	36.550260
1497.277987	196441.806121	36.555277
1498.782253	196805.911211	36.560295
1500.652759	197172.331909	36.565312
1502.055170	197529.398945	36.570330
1503.292733	197907.760812	36.575348
1505.097841	198269.285004	36.580365
1506.658930	198638.875365	36.585383
1507.805789	199003.724336	36.590400
1509.546314	199367.436073	36.595418
1510.965347	199735.494189	36.600436
1512.772324	200111.590426	36.605453
1513.994095	200485.157224	36.610471
1515.866734	200852.638428	36.615488
1517.130964	201214.038852	36.620506
1518.748165	201596.027476	36.625524
1520.461193	201970.562052	36.630541
1521.981290	202342.400652	36.635559
1523.506992	202692.541395	36.640576
1524.967931	203066.767771	36.645594
1526.354591	203432.539473	36.650612
1528.002863	203796.174755	36.655629
1529.297406	204178.509532	36.660647
1530.418637	204538.972362	36.665664
1532.017805	204892.577654	36.670682
1533.546043	205253.827350	36.675700
1535.575640	205615.351440	36.680717
1536.560626	205976.046727	36.685735
1537.938449	206327.435069	36.690752
1539.770424	206697.948532	36.695770
1540.925105	207059.877835	36.700788
1542.351376	207415.440519	36.705805
1544.069292	207790.980790	36.710823
1545.382095	208163.567694	36.715840
1546.845019	208530.925427	36.720858
1548.404944	208910.992005	36.725876
1550.257910	209288.688213	36.730893
1551.549389	209679.176850	36.735911
1553.131076	210057.949906	36.740928
1554.573451	210441.242795	36.745946
1556.060999	210824.885501	36.750964
1557.772579	211214.892791	36.755981
1559.058670	211604.083268	36.760999
1560.779395	212000.365512	36.766016
1562.439773	212393.434139	36.771034
1563.938671	212794.912135	36.776052
1565.737316	213186.132860	36.781069
1567.374774	213591.451866	36.786087
1568.890901	213978.735367	36.791104
1570.305859	214379.066004	36.796122
1572.164097	214774.042493	36.801140
1573.889950	215180.547575	36.806157
1575.273170	215586.780852	36.811175
1576.542806	215993.237812	36.816192
1578.407476	216391.572492	36.821210
1579.787328	216800.909998	36.826228
1581.642574	217214.716920	36.831245
1583.035093	217623.623996	36.836263
1584.786907	218025.768267	36.841280
1586.451145	218435.141729	36.846298
1587.958392	218862.220065	36.851316
1589.474754	219257.931511	36.856333
1591.085635	219679.814811	36.861351
1592.647757	220099.294984	36.866368
1594.635838	220513.271101	36.871386
1596.177504	220925.239855	36.876404
1598.266195	221334.427510	36.881421
1599.628080	221742.111222	36.886439
1601.112226	222156.634016	36.891456
1603.023860	222562.985349	36.896474
1604.235457	222981.899479	36.901492
1606.345832	223392.818224	36.906509
1607.536984	223806.481037	36.911527
1609.497728	224224.615502	36.916544
1611.139344	224633.634858	36.921562
1612.683304	225085.013234	36.926580
1614.278344	225527.418673	36.931597
1615.731989	225946.633452	36.936615
1617.499798	226360.514518	36.941632
1619.377736	226769.451111	36.946650
1620.678818	227191.921033	36.951668
1622.017610	227598.587092	36.956685
1623.577747	228023.175927	36.961703
1625.363315	228438.838700	36.966720
1627.344541	228863.614628	36.971738
1628.915812	229291.812479	36.976756
1630.536219	229694.831415	36.981773
1631.921646	230110.539912	36.986791
1633.811186	230537.495120	36.991808
1635.693021	230949.618705	36.996826
1637.253101	231363.930278	37.001844
1639.186272	231770.510236	37.006861
1640.648307	232162.436448	37.011879
1642.373318	232566.487388	37.016896
1643.802641	232949.403556	37.021914
1645.353592	233349.040027	37.026932
1646.784103	233737.038142	37.031949
1648.388165	234137.302806	37.036967
1649.915226	234526.937915	37.041984
1651.751812	234937.402878	37.047002
1653.248346	235344.648179	37.052020
1654.740312	235744.096861	37.057037
1656.072778	236157.162715	37.062055
1657.753746	236571.594438	37.067072
1659.393009	236990.657114	37.072090
1661.079410	237416.444439	37.077108
1662.677349	237836.862098	37.082125
1664.139875	238252.857670	37.087143
1665.914129	238689.911735	37.092160
1667.537071	239116.272025	37.097178
1668.930881	239556.057982	37.102196
1670.458509	239986.906550	37.107213
1672.206190	240434.713740	37.112231
1673.366355	240888.893248	37.117248
1675.180150	241329.731035	37.122266
1677.167257	241792.717337	37.127284
1678.764990	242247.462228	37.132301
1680.743979	242699.960352	37.137319
1682.408031	243152.714514	37.142336
1684.287096	243597.838554	37.147354
1685.644983	244066.953306	37.152372
1687.237362	244519.594562	37.157389
1689.277059	244973.559785	37.162407
1690.728086	245432.195430	37.167424
1692.614496	245904.807587	37.172442
1693.982163	246379.817783	37.177460
1695.704477	246839.401329	37.182477
1697.663524	247306.846685	37.187495
1699.523736	247774.004133	37.192512
1701.379184	248241.848827	37.197530
1702.732708	248717.270867	37.202548
1704.676033	249181.850548	37.207565
1706.330104	249650.339769	37.212583
1707.960481	250129.070826	37.217600
1710.009264	250594.142583	37.222618
1711.462597	251077.628775	37.227636
1713.172870	251547.558477	37.232653
1715.116274	252017.069005	37.237671
1716.967209	252508.111664	37.242688
1718.710800	252973.997831	37.247706
1720.446172	253450.631218	37.252724
1722.431107	253930.957944	37.257741
1724.100218	254393.427807	37.262759
1725.847859	254872.498652	37.267776
1727.639044	255344.093950	37.272794
1729.234667	255823.418920	37.277812
1730.913347	256289.291986	37.282829
1732.783491	256768.800522	37.287847
1734.266518	257250.506978	37.292864
1736.161822	257725.515151	37.297882
1737.669300	258208.818100	37.302900
1739.177985	258686.100286	37.307917
1741.357582	259166.802712	37.312935
1742.825664	259651.458523	37.317952
1744.920826	260128.364306	37.322970
1746.495485	260607.261220	37.327988
1748.308197	261095.619531	37.333005
1750.037740	261568.292206	37.338023
1751.797794	262051.298808	37.343040
1753.910869	262519.741644	37.348058
1755.083688	262987.323438	37.353076
1756.510499	263453.948529	37.358093
1758.237048	263906.729906	37.363111
1759.876576	264377.561662	37.368128
1761.816385	264838.537879	37.373146
1763.505556	265315.991013	37.378164
1765.056955	265793.745962	37.383181
1766.839487	266271.055882	37.388199
1768.543051	266744.847386	37.393216
1770.541592	267214.830066	37.398234
1771.964778	267700.682599	37.403252
1773.613595	268177.098223	37.408269
1775.537937	268675.060347	37.413287
1777.297267	269168.120939	37.418304
1779.162313	269653.339339	37.423322
1780.697529	270152.532360	37.428340
1782.103940	270646.309737	37.433357
1784.164346	271159.233714	37.438375
1785.867012	271668.507160	37.443392
1787.875564	272178.059490	37.448410
1789.442214	272687.658537	37.453428
1791.040764	273197.099003	37.458445
1792.983176	273709.987306	37.463463
1794.734015	274246.302017	37.468480
1796.566305	274759.485906	37.473498
1798.260022	275281.455480	37.478516
1800.069149	275814.861353	37.483533
1801.724851	276332.008475	37.488551
1803.608606	276868.676516	37.493568
1805.760668	277387.517412	37.498586
1807.776209	277929.444760	37.503604
1809.661168	278460.571000	37.508621
1811.739151	278988.666551	37.513639
1812.983915	279533.688999	37.518656
1814.896068	280051.953141	37.523674
1816.942708	280584.164652	37.528692
1818.835589	281126.052685	37.533709
1820.967929	281652.760168	37.538727
1822.669155	282187.208558	37.543744
1824.726499	282717.405237	37.548762
1826.705961	283256.325802	37.553780
1828.470670	283790.047405	37.558797
1830.258159	284313.552187	37.563815
1832.053994	284854.529861	37.568832
1834.169576	285383.793757	37.573850
1836.166112	285915.818781	37.578868
1838.084036	286457.177019	37.583885
1840.024717	286978.285064	37.588903
1841.424518	287516.930828	37.593920
1843.648732	288047.970612	37.598938
1845.241750	288578.198180	37.603956
1847.217607	289110.087688	37.608973
1849.170589	289647.058920	37.613991
1850.937836	290187.716260	37.619008
1852.599627	290717.542914	37.624026
1854.692053	291264.187233	37.629044
1856.189118	291795.230357	37.634061
1858.628565	292330.433522	37.639079
1860.279105	292874.756076	37.644096
1861.950335	293402.918623	37.649114
1863.810672	293950.198722	37.654132
1865.424710	294489.389127	37.659149
1867.521007	295028.700530	37.664167
1869.423611	295571.393997	37.669184
1871.225256	296117.631919	37.674202
1873.052926	296652.611133	37.679220
1874.760655	297201.144977	37.684237
1876.733451	297734.875653	37.689255
1878.634964	298259.471943	37.694272
1880.611282	298775.900357	37.699290
1882.414845	299297.053331	37.704308
1883.939915	299826.757922	37.709325
1886.232304	300336.395632	37.714343
1887.700404	300863.716647	37.719360
1889.726526	301400.111171	37.724378
1891.435861	301919.614881	37.729396
1893.104771	302452.913148	37.734413
1895.384896	302984.913762	37.739431
1896.996738	303530.050325	37.744448
1899.083694	304073.987699	37.749466
1900.950452	304608.307385	37.754484
1902.300266	305148.398046	37.759501
1904.571259	305684.473013	37.764519
1906.524761	306256.253416	37.769536
1908.072248	306793.355219	37.774554
1910.346283	307346.739402	37.779572
1911.761451	307919.689490	37.784589
1914.099829	308479.099703	37.789607
1916.044385	309032.476228	37.794624
1918.107229	309602.793439	37.799642
1919.758847	310172.209478	37.804660
1921.289551	310735.267279	37.809677
1923.445468	311309.772363	37.814695
1925.388372	311889.209490	37.819712
1926.844929	312472.455498	37.824730
1929.104087	313047.412989	37.829748
1930.786660	313637.367485	37.834765
1933.280773	314224.440766	37.839783
1934.839600	314813.492115	37.844800
1937.087302	315395.365607	37.849818
1938.891993	315988.658235	37.854836
1940.914204	316590.518170	37.859853
1943.286549	317170.248949	37.864871
1945.182129	317765.822316	37.869888
1947.244537	318363.343585	37.874906
1948.891279	318950.162062	37.879924
1950.540201	319553.632074	37.884941
1952.898583	320153.450081	37.889959
1954.869664	320766.199990	37.894976
1956.811598	321353.304032	37.899994
1958.999028	321950.874036	37.905012
1960.729492	322561.513925	37.910029
1963.022846	323156.998557	37.915047
1964.921216	323754.472442	37.920064
1966.763671	324371.246144	37.925082
1969.171510	324972.229591	37.930100
1970.745808	325576.112229	37.935117
1972.958915	326175.262588	37.940135
1974.681951	326786.395284	37.945152
1976.907368	327379.539838	37.950170
1979.193411	327988.663096	37.955188
1980.685763	328596.692461	37.960205
1983.157579	329196.683546	37.965223
1985.403991	329799.498245	37.970240
1987.063383	330408.445691	37.975258
1988.854478	331001.421832	37.980276
1991.180188	331615.019029	37.985293
1993.285300	332221.309226	37.990311
1995.387327	332821.272142	37.995328
1997.134352	333417.174605	38.000346
1999.217655	334020.427631	38.005364
2000.941777	334629.851092	38.010381
2003.429980	335220.585014	38.015399
2005.746578	335825.860790	38.020416
2007.291424	336423.870169	38.025434
2009.349057	337017.041220	38.030452
2011.099968	337605.610895	38.035469
2013.221303	338180.100954	38.040487
2015.321236	338751.846705	38.045504
2017.192016	339328.700470	38.050522
2019.317122	339903.271976	38.055540
2021.153846	340488.519754	38.060557
2023.087137	341059.149976	38.065575
2025.077435	341644.967929	38.070592
2026.608009	342231.235515	38.075610
2029.236251	342818.507745	38.080628
2030.832424	343423.202269	38.085645
2032.740055	344016.264211	38.090663
2034.597150	344625.088283	38.095680
2036.597290	345223.982733	38.100698
2038.689277	345828.869371	38.105716
2040.357669	346456.278789	38.110733
2042.372156	347063.674729	38.115751
2044.730687	347691.308754	38.120768
2046.804095	348321.798226	38.125786
2048.689106	348937.463973	38.130804
2050.510269	349565.972907	38.135821
2052.591700	350204.301786	38.140839
2054.771650	350832.479884	38.145856
2056.770675	351483.416235	38.150874
2058.732895	352127.852728	38.155892
2060.869561	352767.607133	38.160909
2062.435720	353412.419832	38.165927
2064.896624	354065.651876	38.170944
2067.122967	354722.084465	38.175962
2069.503127	355368.712441	38.180980
2071.420619	356030.681876	38.185997
2073.389896	356668.882807	38.191015
2075.480304	357336.791069	38.196032
2077.722357	357997.787520	38.201050
2079.771730	358660.327448	38.206068
2081.614906	359321.469817	38.211085
2083.792262	359986.199681	38.216103
2085.904329	360651.741193	38.221120
2088.040850	361339.136913	38.226138
2090.275828	362004.965309	38.231156
2092.301781	362676.169940	38.236173
2094.157851	363350.105605	38.241191
2096.240652	364030.943187	38.246208
2098.187004	364715.520430	38.251226
2101.023612	365390.298727	38.256244
2102.890093	366085.392281	38.261261
2105.167852	366757.194480	38.266279
2106.887214	367447.036311	38.271296
2109.054382	368120.582642	38.276314
2111.359118	368808.679230	38.281332
2113.349831	369498.260645	38.286349
2115.525484	370192.059823	38.291367
2117.559470	370875.926476	38.296384
2119.852414	371574.448365	38.301402
2122.075036	372263.786879	38.306420
2124.143611	372953.949156	38.311437
2126.245667	373649.393206	38.316455
2128.319836	374343.940532	38.321472
2130.299030	375037.652901	38.326490
2132.735839	375737.463949	38.331508
2134.581774	376432.996501	38.336525
2136.718860	377126.666455	38.341543
2138.706010	377832.265904	38.346560
2140.822100	378540.086390	38.351578
2143.305290	379239.133714	38.356596
2145.336506	379947.014842	38.361613
2147.529651	380643.240815	38.366631
2149.094221	381337.781056	38.371648
2151.532845	382011.472057	38.376666
2153.880997	382696.396654	38.381684
2155.832545	383372.193949	38.386701
2157.905992	384045.954123	38.391719
2160.404861	384721.252715	38.396736
2161.861289	385405.354696	38.401754
2164.504487	386076.290954	38.406772
2166.119070	386774.382958	38.411789
2168.648782	387462.877748	38.416807
2170.636459	388147.847133	38.421824
2172.598599	388850.475087	38.426842
2174.981909	389539.734343	38.431860
2177.173226	390248.706443	38.436877
2179.547718	390944.019738	38.441895
2181.590521	391657.521353	38.446912
2183.453277	392361.708107	38.451930
2185.635474	393073.328533	38.456948
2187.533770	393788.223407	38.461965
2189.351507	394517.941875	38.466983
2192.010591	395258.300709	38.472000
2193.735676	395995.931339	38.477018
2196.174953	396733.552414	38.482036
2198.326083	397480.782305	38.487053
2200.142629	398226.122300	38.492071
2202.609001	398968.522992	38.497088
2204.587457	399719.094392	38.502106
2207.057391	400479.980105	38.507124
2209.020541	401241.005264	38.512141
2211.263490	402010.959349	38.517159
2213.318356	402777.426823	38.522176
2215.151875	403552.980943	38.527194
2217.784252	404335.172110	38.532212
2219.612647	405124.086833	38.537229
2222.157956	405901.865066	38.542247
2224.578382	406688.179867	38.547264
2226.674854	407479.212429	38.552282
2229.172413	408264.582467	38.557300
2231.427842	409052.376347	38.562317
2233.297936	409853.738151	38.567335
2235.724888	410643.661027	38.572352
2238.060902	411441.174706	38.577370
2240.090848	412243.248984	38.582388
2242.716910	413042.085052	38.587405
2244.950707	413850.257042	38.592423
2247.084349	414647.884350	38.597440
2249.152015	415461.808464	38.602458
2251.428931	416262.933516	38.607476
2253.791952	417072.098121	38.612493
2256.068483	417887.835738	38.617511
2258.622952	418698.740542	38.622528
2260.721036	419508.656483	38.627546
2262.870626	420324.159352	38.632564
2264.911868	421148.946396	38.637581
2267.188828	421956.019110	38.642599
2270.177843	422767.834703	38.647616
2272.420074	423601.723321	38.652634
2274.358665	424412.544059	38.657652
2276.956529	425238.520460	38.662669
2279.019289	426041.165184	38.667687
2281.561040	426863.956340	38.672704
2283.795322	427683.124883	38.677722
2286.161499	428498.294777	38.682740
2288.567011	429317.632198	38.687757
2290.679459	430146.253757	38.692775
2293.258694	430948.901631	38.697792
2295.626454	431777.221217	38.702810
2298.086510	432584.439170	38.707828
2300.514093	433388.141975	38.712845
2302.689598	434184.671250	38.717863
2305.268392	434956.255598	38.722880
2307.538616	435728.725331	38.727898
2309.938973	436507.979751	38.732916
2312.424486	437278.337102	38.737933
2314.240752	438046.906288	38.742951
2316.941295	438815.151554	38.747968
2318.761714	439596.773628	38.752986
2320.874259	440378.168380	38.758004
2323.484947	441159.706501	38.763021
2325.757640	441946.231360	38.768039
2328.060931	442728.827307	38.773056
2330.432061	443533.544126	38.778074
2332.741091	444326.656125	38.783092
2334.705575	445123.236210	38.788109
2336.981383	445926.210916	38.793127
2339.490370	446736.351079	38.798144
2341.242161	447554.223861	38.803162
2343.995199	448360.468613	38.808180
2345.928461	449189.022843	38.813197
2347.953793	450020.210174	38.818215
2350.320130	450851.359108	38.823232
2352.605271	451697.559693	38.828250
2355.131834	452548.743449	38.833268
2357.033837	453400.349498	38.838285
2359.159775	454261.188146	38.843303
2361.861950	455113.704175	38.848320
2364.234597	455982.116239	38.853338
2366.441848	456851.529992	38.858356
2368.968595	457720.247227	38.863373
2370.958011	458611.210534	38.868391
2373.470733	459485.061736	38.873408
2375.630517	460369.144855	38.878426
2378.217166	461254.230604	38.883444
2380.188437	462151.004681	38.888461
2382.580629	463052.622270	38.893479
2385.090695	463954.634141	38.898496
2387.182456	464862.182651	38.903514
2389.404622	465773.457983	38.908532
2392.139279	466684.757742	38.913549
2394.377684	467620.100276	38.918567
2397.038687	468528.697579	38.923584
2399.261622	469456.879051	38.928602
2401.649251	470387.817829	38.933620
2404.068762	471316.634356	38.938637
2406.517318	472254.747141	38.943655
2408.947230	473192.058596	38.948672
2411.202237	474130.716119	38.953690
2413.700995	475071.458447	38.958708
2416.006249	476014.054124	38.963725
2418.401100	476964.163471	38.968743
2421.146427	477907.751767	38.973760
2423.195691	478866.254610	38.978778
2425.554786	479812.990342	38.983796
2428.503315	480760.438092	38.988813
2430.658929	481727.105136	38.993831
2433.274239	482661.126926	38.998848
2435.490293	483634.094334	39.003866
2438.103737	484588.414251	39.008884
2440.564047	485547.302476	39.013901
2443.070597	486507.090418	39.018919
2445.733583	487455.694876	39.023936
2447.962072	488414.869550	39.028954
2450.372073	489375.677876	39.033972
2453.333695	490338.966767	39.038989
2455.510404	491298.798922	39.044007
2458.041699	492243.732822	39.049024
2460.730942	493197.066596	39.054042
2463.102315	494131.325843	39.059060
2466.000628	495048.392396	39.064077
2468.012656	495968.683923	39.069095
2470.174416	496879.869837	39.074112
2472.692135	497801.643082	39.079130
2475.004668	498726.829989	39.084148
2477.756779	499651.187026	39.089165
2479.882645	500572.670560	39.094183
2482.820477	501505.065397	39.099200
2485.182204	502450.868067	39.104218
2487.274037	503387.532716	39.109236
2490.016507	504326.255460	39.114253
2492.093613	505270.631414	39.119271
2494.599593	506213.621246	39.124288
2497.071290	507177.385636	39.129306
2499.506285	508133.535930	39.134324
2502.002825	509092.190388	39.139341
2504.458742	510063.094625	39.144359
2507.336214	511024.343039	39.149376
2509.762068	511996.596220	39.154394
2511.897105	512975.641997	39.159412
2514.897000	513956.802679	39.164429
2517.289256	514948.131911	39.169447
2519.676228	515925.843532	39.174464
2522.257170	516912.683118	39.179482
2524.593223	517907.461416	39.184500
2527.491046	518904.803717	39.189517
2529.690543	519904.715612	39.194535
2532.091492	520909.717875	39.199552
2534.783139	521912.691878	39.204570
2537.174771	522930.508380	39.209588
2540.041303	523942.184564	39.214605
2542.146542	524960.415370	39.219623
2545.154650	525993.385096	39.224640
2547.242265	527010.120001	39.229658
2549.933446	528032.929776	39.234676
2552.628324	529066.745358	39.239693
2555.288292	530105.931801	39.244711
2557.764193	531132.087050	39.249728
2560.647594	532171.241732	39.254746
2563.105110	533209.386109	39.259764
2566.101095	534243.190146	39.264781
2568.762295	535282.411138	39.269799
2571.360671	536307.577608	39.274816
2574.062577	537344.579983	39.279834
2576.511169	538380.140267	39.284852
2579.647942	539411.688128	39.289869
2581.867760	540449.349616	39.294887
2584.648778	541482.818083	39.299904
2587.556099	542516.642782	39.304922
2589.823195	543553.364120	39.309940
2593.154940	544576.404386	39.314957
2595.661736	545620.426886	39.319975
2598.416689	546632.296961	39.324992
2600.846330	547665.567688	39.330010
2603.283584	548688.351850	39.335028
2606.517891	549708.565479	39.340045
2609.108492	550744.946784	39.345063
2611.701813	551768.380170	39.350080
2614.261050	552798.176069	39.355098
2617.038282	553817.906050	39.360116
2619.739296	554835.259741	39.365133
2622.439342	555858.868588	39.370151
2625.046181	556871.158710	39.375168
2627.794188	557896.161507	39.380186
2630.089246	558919.552322	39.385204
2632.891302	559916.305041	39.390221
2635.224585	560933.455027	39.395239
2638.090953	561932.757393	39.400256
2640.808942	562909.858151	39.405274
2643.060817	563884.652520	39.410292
2645.310096	564864.095017	39.415309
2647.865061	565853.305670	39.420327
2650.449914	566846.251872	39.425344
2652.926851	567848.026195	39.430362
2655.628540	568843.510334	39.435380
2658.402557	569849.095752	39.440397
2660.798227	570851.401651	39.445415
2663.544560	571866.369689	39.450432
2666.131733	572879.475986	39.455450
2668.218219	573904.125921	39.460468
2670.950797	574921.711334	39.465485
2673.729394	575963.341097	39.470503
2676.252409	576998.454176	39.475520
2679.044061	578040.259730	39.480538
2681.443425	579096.589858	39.485556
2684.177590	580143.495294	39.490573
2686.576632	581200.147258	39.495591
2689.088004	582279.407814	39.500608
2692.060885	583348.568363	39.505626
2694.258598	584427.640919	39.510644
2697.390300	585504.207574	39.515661
2699.976136	586600.671101	39.520679
2702.509050	587690.677634	39.525696
2705.596096	588784.153049	39.530714
2708.039839	589890.615537	39.535732
2710.732401	590985.408398	39.540749
2713.311619	592101.415695	39.545767
2716.105712	593211.971547	39.550784
2719.443006	594322.383611	39.555802
2721.742353	595442.480437	39.560820
2724.668842	596552.799778	39.565837
2727.500558	597672.896204	39.570855
2730.042070	598791.129989	39.575872
2732.918488	599929.782026	39.580890
2735.624477	601049.173087	39.585908
2738.504475	602177.088241	39.590925
2741.116439	603311.194557	39.595943
2743.857670	604442.814656	39.600960
2747.165509	605587.943107	39.605978
2749.736619	606726.021295	39.610996
2752.506620	607860.399525	39.616013
2755.125082	609009.449412	39.621031
2757.894488	610152.053249	39.626048
2760.929350	611288.243715	39.631066
2763.799115	612445.704686	39.636084
2766.729306	613584.529755	39.641101
2769.429158	614727.826907	39.646119
2772.058520	615877.468178	39.651136
2775.318590	617014.685603	39.656154
2778.109429	618166.061159	39.661172
2780.933826	619292.315416	39.666189
2783.763293	620439.046093	39.671207
2786.579213	621591.155763	39.676224
2789.813202	622730.180829	39.681242
2792.240390	623875.714700	39.686260
2795.048547	625015.068296	39.691277
2797.863179	626158.496273	39.696295
2800.346644	627317.641513	39.701312
2803.474729	628460.321647	39.706330
2805.880481	629612.486832	39.711348
2808.673543	630757.671449	39.716365
2811.305719	631915.390729	39.721383
2814.018759	633085.001143	39.726400
2816.816972	634238.243142	39.731418
2819.617508	635391.307504	39.736436
2822.473167	636520.328874	39.741453
2825.138708	637642.721427	39.746471
2827.499232	638771.778668	39.751488
2830.304760	639886.020449	39.756506
2832.681589	641028.497935	39.761524
2835.392799	642169.495956	39.766541
2838.169637	643317.587607	39.771559
2840.768226	644461.639405	39.776576
2843.788013	645622.795633	39.781594
2846.069528	646790.521567	39.786612
2848.942616	647966.290209	39.791629
2851.793951	649145.912552	39.796647
2854.705461	650333.609730	39.801664
2857.367140	651518.116970	39.806682
2860.218460	652710.723486	39.811700
2863.081882	653904.081339	39.816717
2865.649003	655121.305827	39.821735
2868.435948	656322.005712	39.826752
2871.453508	657543.239383	39.831770
2874.069585	658779.724645	39.836788
2876.863427	660018.961498	39.841805
2879.660084	661257.442403	39.846823
2881.880721	662510.544726	39.851840
2885.136227	663757.241459	39.856858
2887.918687	665023.213593	39.861876
2890.680006	666289.668882	39.866893
2893.761442	667564.460972	39.871911
2896.631199	668855.433972	39.876928
2899.760854	670125.248171	39.881946
2902.258057	671434.384324	39.886964
2905.189549	672718.006345	39.891981
2908.243161	674017.342781	39.896999
2911.042512	675328.521268	39.902016
2914.503158	676628.073634	39.907034
2917.368613	677947.272436	39.912052
2920.290968	679257.478658	39.917069
2923.100662	680566.573444	39.922087
2925.935773	681889.536186	39.927104
2929.015072	683210.181584	39.932122
2932.086616	684535.553851	39.937140
2935.063595	685866.161096	39.942157
2938.357555	687187.286412	39.947175
2941.371405	688510.002224	39.952192
2944.255687	689824.405344	39.957210
2947.205313	691151.458353	39.962228
2950.631994	692480.964896	39.967245
2953.308857	693806.179873	39.972263
2956.448468	695147.093302	39.977280
2960.055214	696464.466109	39.982298
2963.034819	697789.233559	39.987316
2966.067196	699107.396820	39.992333
2968.981824	700425.777897	39.997351
2972.301712	701748.800310	40.002368
2975.514372	703062.768378	40.007386
2978.384479	704377.337276	40.012404
2981.634099	705680.050621	40.017421
2984.818470	706993.079600	40.022439
2987.900554	708304.488513	40.027456
2990.858154	709602.098881	40.032474
2993.605099	710913.163034	40.037492
2996.425522	712220.844752	40.042509
2999.736739	713523.541659	40.047527
3002.459387	714847.861293	40.052544
3005.743982	716146.149138	40.057562
3008.359515	717458.199722	40.062580
3011.645823	718782.399971	40.067597
3014.684376	720087.389062	40.072615
3017.496407	721384.347984	40.077632
3020.819368	722649.326123	40.082650
3023.228733	723922.566718	40.087668
3026.101625	725195.039975	40.092685
3029.345819	726454.949052	40.097703
3031.939251	727729.002836	40.102720
3035.187139	728995.734347	40.107738
3037.946362	730277.267658	40.112756
3040.854564	731566.476589	40.117773
3043.539619	732848.158920	40.122791
3046.297669	734141.031192	40.127808
3049.296296	735445.948313	40.132826
3052.372015	736763.671029	40.137844
3055.211926	738088.321831	40.142861
3058.097798	739406.971802	40.147879
3060.717617	740752.679051	40.152896
3063.728979	742097.353173	40.157914
3067.064026	743446.183372	40.162932
3069.932600	744812.610261	40.167949
3072.919215	746166.208143	40.172967
3075.561630	747530.521771	40.177984
3078.878424	748906.855322	40.183002
3081.747721	750294.893732	40.188020
3084.980316	751693.264632	40.193037
3088.404344	753096.522441	40.198055
3090.796240	754489.746489	40.203072
3094.410592	755902.309542	40.208090
3097.382665	757314.963479	40.213108
3100.290334	758730.073129	40.218125
3103.573263	760148.351111	40.223143
3106.538642	761584.669224	40.228160
3109.715323	763019.203252	40.233178
3112.885930	764445.841288	40.238196
3115.853389	765891.074404	40.243213
3119.244479	767333.057405	40.248231
3122.719895	768786.888140	40.253248
3125.803854	770222.118610	40.258266
3128.833129	771681.155487	40.263284
3131.513480	773139.027712	40.268301
3134.537416	774593.705368	40.273319
3137.730801	776067.806400	40.278336
3141.073499	777540.161328	40.283354
3144.263284	779015.433978	40.288372
3147.333973	780497.002148	40.293389
3150.682508	781967.426443	40.298407
3153.868424	783469.119719	40.303424
3156.954920	784944.031087	40.308442
3160.334157	786431.437254	40.313460
3163.141466	787923.775001	40.318477
3166.577706	789409.961142	40.323495
3169.531863	790913.213263	40.328512
3173.164060	792398.396033	40.333530
3176.297666	793907.104245	40.338548
3179.194509	795405.536642	40.343565
3182.399956	796897.036163	40.348583
3185.714401	798409.883925	40.353600
3188.935173	799909.007880	40.358618
3192.226443	801412.688592	40.363636
3195.536131	802922.104583	40.368653
3198.999866	804432.777896	40.373671
3202.087680	805941.664412	40.378688
3205.235222	807438.572784	40.383706
3208.303797	808952.467346	40.388724
3211.306703	810456.359806	40.393741
3214.709786	811952.279636	40.398759
3217.694692	813475.240120	40.403776
3220.641450	814991.709018	40.408794
3223.483793	816514.247545	40.413812
3226.401752	818017.000098	40.418829
3230.300328	819510.467982	40.423847
3233.510439	820997.029182	40.428864
3236.779695	822468.613346	40.433882
3239.929907	823943.058571	40.438900
3242.958388	825426.700509	40.443917
3246.571487	826889.193774	40.448935
3249.496381	828380.372082	40.453952
3252.658015	829862.107599	40.458970
3255.444330	831355.890742	40.463988
3258.907831	832855.256324	40.469005
3262.180983	834356.495786	40.474023
3265.222256	835871.101298	40.479040
3268.210429	837392.414246	40.484058
3271.501453	838909.276869	40.489076
3274.308464	840443.028791	40.494093
3277.846502	841981.298756	40.499111
3280.822684	843532.997881	40.504128
3284.054230	845090.397746	40.509146
3287.228579	846664.623765	40.514164
3290.536094	848234.448785	40.519181
3293.865778	849806.304238	40.524199
3297.161493	851391.364679	40.529216
3300.335777	852982.836710	40.534234
3303.738778	854567.067166	40.539252
3306.949858	856173.047402	40.544269
3310.096511	857785.312678	40.549287
3313.258287	859386.191472	40.554304
3316.289377	861022.451560	40.559322
3319.844226	862657.603859	40.564340
3322.919601	864295.398623	40.569357
3326.371611	865928.134122	40.574375
3329.843388	867574.371515	40.579392
3333.069154	869224.652435	40.584410
3336.663620	870884.872511	40.589428
3339.789278	872543.546468	40.594445
3343.272633	874208.664815	40.599463
3346.445511	875883.328896	40.604480
3349.894622	877555.055235	40.609498
3353.232893	879230.771769	40.614516
3356.407259	880910.772022	40.619533
3359.761146	882594.704143	40.624551
3363.247254	884292.712059	40.629568
3366.687907	885993.320758	40.634586
3370.326032	887696.099982	40.639604
3373.148640	889386.159029	40.644621
3376.538119	891083.345499	40.649639
3380.310155	892801.569106	40.654656
3383.302851	894519.596866	40.659674
3386.722865	896223.734655	40.664692
3389.919897	897941.175789	40.669709
3393.493210	899657.936759	40.674727
3397.130218	901382.252821	40.679744
3399.995906	903119.162193	40.684762
3403.640332	904839.717650	40.689780
3407.025988	906577.294306	40.694797
3410.635977	908307.366027	40.699815
3414.039051	910038.085109	40.704832
3417.445011	911775.661912	40.709850
3420.981607	913506.999302	40.714868
3424.029261	915250.933895	40.719885
3427.740128	916987.288884	40.724903
3431.362618	918733.279996	40.729920
3434.355482	920469.120879	40.734938
3437.860098	922209.308814	40.739956
3441.265742	923965.062499	40.744973
3444.595225	925708.654760	40.749991
3448.335367	927460.620282	40.755008
3451.322976	929181.346377	40.760013
3455.114191	930865.104860	40.765018
3458.266486	932500.534177	40.770023
3461.756964	934060.454932	40.775028
3464.895981	935559.148704	40.780032
3467.687915	936981.128405	40.785037
3470.962520	938334.085265	40.790042
3473.778283	939615.638608	40.795047
3476.763730	940817.590329	40.800052
3479.279596	941957.826557	40.805056
3481.507672	943022.562428	40.810061
3484.008013	944016.253389	40.815066
3486.313363	944944.762706	40.820071
3488.617667	945802.061203	40.825076
3490.893491	946600.633865	40.830080
3492.858324	947329.068131	40.835085
3494.670960	947998.660860	40.840090
3496.278931	948627.147113	40.845095
3498.579082	949185.497671	40.850100
3500.100400	949696.365586	40.855104
3501.500881	950146.263437	40.860109
3503.004321	950550.954091	40.865114
3504.274256	950919.973208	40.870119
3505.714180	951245.801704	40.875124
3507.205433	951514.790831	40.880128
3507.946912	951749.364791	40.885133
3509.393091	951941.925049	40.890138
3509.989935	952101.243394	40.895143
3511.080595	952228.631718	40.900148
3511.748750	952332.849627	40.905152
3512.567190	952409.023010	40.910157
3513.680318	952446.515213	40.915162
3514.569848	952455.835361	40.920167
3515.141047	952439.676661	40.925172
3516.073369	952396.588203	40.930176
3516.369288	952340.694889	40.935181
3516.873498	952255.791921	40.940186
3517.447494	952159.591923	40.945191
3518.204632	952029.028638	40.950196
3518.612766	951895.267980	40.955200
3518.779868	951746.337420	40.960205
3519.518328	951565.651844	40.965210
3519.789104	951394.601187	40.970215
3520.255427	951190.323379	40.975220
3520.491254	950983.014558	40.980224
3520.691556	950754.372241	40.985229
3520.908333	950513.185643	40.990234
3521.108822	950283.278636	40.995239
3521.553331	950026.438387	41.000244
3521.636091	949763.808777	41.005248
3521.655579	949490.842865	41.010253
3522.161515	949213.476500	41.015258
3521.872669	948938.426889	41.020263
3522.717729	948630.544044	41.025268
3522.832969	948332.428648	41.030272
3522.720741	948023.422966	41.035277
3522.830200	947704.982425	41.040282
3522.881375	947397.730674	41.045287
3522.910378	947078.977423	41.050292
3523.147622	946751.554467	41.055296
3523.255782	946415.802950	41.060301
3523.751664	946073.933918	41.065306
3523.326292	945743.013518	41.070311
3523.367640	945406.536976	41.075316
3523.843341	945054.070642	41.080320
3523.598078	944705.146641	41.085325
3523.562013	944336.626695	41.090330
3523.425644	943991.659065	41.095335
3523.450736	943631.124305	41.100340
3523.685103	943274.074321	41.105344
3523.529390	942914.956371	41.110349
3523.408388	942552.262943	41.115354
3523.453625	942194.211632	41.120359
3523.335358	941830.317499	41.125364
3523.418218	941463.298251	41.130368
3523.421074	941103.453808	41.135373
3523.542813	940740.593816	41.140378
3523.298040	940376.235342	41.145383
3523.507796	940001.903505	41.150388
3523.565825	939635.909685	41.155392
3523.536312	939269.233522	41.160397
3523.336968	938881.467148	41.165402
3523.443393	938517.304383	41.170407
3523.150306	938142.826121	41.175412
3523.333661	937783.010388	41.180416
3523.068831	937401.665853	41.185421
3523.119220	937028.297953	41.190426
3523.011920	936655.313090	41.195431
3523.028919	936286.789568	41.200436
3522.925853	935902.815337	41.205440
3523.019989	935544.203620	41.210445
3523.045809	935165.910443	41.215450
3522.808760	934799.339212	41.220455
3522.667377	934428.984386	41.225460
3522.618276	934045.921175	41.230464
3522.607757	933682.497618	41.235469
3522.570443	933302.161544	41.240474
3522.510729	932936.487234	41.245479
3522.240522	932555.463846	41.250484
3522.635854	932189.470884	41.255488
3522.586188	931821.317830	41.260493
3522.479493	931447.099904	41.265498
3521.890675	931084.168967	41.270503
3521.808303	930716.232523	41.275508
3522.207705	930356.161696	41.280512
3522.022429	929977.819725	41.285517
3522.018087	929613.539426	41.290522
3521.950427	929253.374747	41.295527
3521.854667	928885.793940	41.300532
3521.723881	928513.774596	41.305536
3521.318082	928155.224383	41.310541
3521.356921	927781.396692	41.315546
3521.175911	927430.254662	41.320551
3521.124276	927075.224637	41.325556
3521.088147	926718.919211	41.330560
3521.204167	926360.162410	41.335565
3521.492316	925999.719341	41.340570
3521.153596	925645.410532	41.345575
3521.031324	925279.123544	41.350580
3521.259461	924915.829894	41.355584
3520.883655	924570.011489	41.360589
3521.123532	924211.474933	41.365594
3520.815002	923853.581677	41.370599
3520.569442	923497.000358	41.375604
3520.727925	923146.771539	41.380608
3520.676935	922799.920255	41.385613
3520.783789	922445.903876	41.390618
3520.197036	922095.248585	41.395623
3520.003051	921742.870632	41.400628
3520.060875	921394.852972	41.405632
3519.971902	921065.691705	41.410637
3520.015355	920718.210002	41.415642
3519.829919	920382.288785	41.420647
3519.919709	920034.851758	41.425652
3519.589477	919690.252056	41.430656
3519.142045	919363.451802	41.435661
3519.608801	919016.657193	41.440666
3519.273853	918675.939349	41.445671
3519.169721	918357.009761	41.450676
3519.608102	918021.513172	41.455680
3519.019832	917692.132948	41.460685
3519.335424	917352.187479	41.465690
3518.950588	917033.804090	41.470695
3518.854550	916706.208453	41.475700
3519.182525	916377.560466	41.480704
3518.798600	916052.572537	41.485709
3518.523327	915726.006679	41.490714
3518.265721	915404.040641	41.495719
3518.385107	915082.667637	41.500724
3518.352619	914763.997402	41.505728
3518.244120	914458.227203	41.510733
3518.335288	914138.440711	41.515738
3517.929630	913826.134431	41.520743
3517.939670	913504.783115	41.525748
3517.961749	913199.499125	41.530752
3517.711972	912885.283179	41.535757
3517.823419	912575.614392	41.540762
3517.590084	912275.042072	41.545767
3517.727373	911963.792915	41.550772
3517.531933	911647.955530	41.555776
3517.545347	911338.811416	41.560781
3517.558919	911033.023012	41.565786
3517.421488	910738.422508	41.570791
3517.391991	910430.583814	41.575796
3517.331382	910137.866260	41.580800
3517.078631	909841.887415	41.585805
3516.939727	909532.859935	41.590810
3516.910835	909242.403295	41.595815
3517.106100	908942.639069	41.600820
3516.818718	908642.938119	41.605824
3517.004126	908346.999883	41.610829
3517.106814	908052.891562	41.615834
3516.978430	907760.927187	41.620839
3516.638610	907450.177193	41.625844
3516.751015	907164.217232	41.630848
3516.228148	906874.007114	41.635853
3516.412009	906582.700879	41.640858
3516.327961	906297.403822	41.645863
3516.117995	906009.797798	41.650868
3516.140293	905722.813905	41.655872
3515.854724	905446.188371	41.660877
3515.960840	905156.363813	41.665882
3515.866323	904881.704778	41.670887
3515.968214	904608.736599	41.675892
3515.918248	904331.920468	41.680896
3515.478436	904052.452968	41.685901
3515.730428	903774.884009	41.690906
3515.252054	903501.571305	41.695911
3515.533484	903236.902422	41.700916
3515.496171	902956.927792	41.705920
3514.882849	902696.627392	41.710925
3515.165989	902411.071102	41.715930
3515.011641	902160.419045	41.720935
3515.004904	901887.046330	41.725940
3515.285232	901617.184881	41.730944
3514.942895	901357.646482	41.735949
3515.003811	901101.022580	41.740954
3514.638509	900840.015847	41.745959
3514.605982	900568.803865	41.750964
3514.633255	900311.859812	41.755968
3514.157665	900058.849438	41.760973
3514.411859	899803.100107	41.765978
3514.222189	899555.331262	41.770983
3514.277613	899295.921896	41.775988
3514.235634	899047.526934	41.780992
3513.771545	898804.213029	41.785997
3514.023240	898540.486821	41.791002
3513.646448	898299.841310	41.796007
3513.972354	898055.012643	41.801012
3513.915237	897807.338401	41.806016
3513.617328	897575.246663	41.811021
3513.990284	897325.451729	41.816026
3513.679126	897084.357221	41.821031
3513.344402	896833.884271	41.826036
3513.365890	896598.124933	41.831040
3513.005565	896366.187157	41.836045
3513.115004	896136.674906	41.841050
3513.341649	895904.041742	41.846055
3513.154036	895660.353795	41.851060
3513.362627	895428.283951	41.856064
3512.965061	895197.560907	41.861069
3512.647111	894968.071839	41.866074
3512.862782	894737.035769	41.871079
3512.954971	894505.237392	41.876084
3512.829763	894286.901506	41.881088
3512.892641	894069.782922	41.886093
3513.164176	893832.514306	41.891098
3512.897191	893613.692624	41.896103
3512.578861	893373.021800	41.901108
3512.707560	893156.147610	41.906112
3512.335955	892936.737099	41.911117
3512.519828	892705.527235	41.916122
3512.529205	892481.588756	41.921127
3512.425598	892273.324999	41.926132
3512.388275	892044.348854	41.931136
3512.085976	891830.686476	41.936141
3512.156149	891607.090549	41.941146
3512.017250	891392.514518	41.946151
3511.780962	891186.650852	41.951156
3511.919685	890972.883798	41.956160
3511.565988	890774.375275	41.961165
3511.983693	890554.453170	41.966170
3511.598773	890347.713329	41.971175
3511.678322	890143.888227	41.976180
3511.757459	889936.766931	41.981184
3511.756527	889734.004639	41.986189
3511.873851	889525.217645	41.991194
3511.399122	889321.261189	41.996199
3511.252531	889115.405185	42.001204
3511.372541	888918.882963	42.006208
3511.136109	888716.510605	42.011213
3511.313358	888504.483723	42.016218
3511.246251	888311.164675	42.021223
3511.274790	888113.081812	42.026228
3511.085779	887911.060410	42.031232
3510.886856	887719.485097	42.036237
3511.111276	887516.026916	42.041242
3510.910686	887330.245558	42.046247
3510.753084	887140.095900	42.051252
3510.949852	886944.558350	42.056256
3510.887613	886751.379807	42.061261
3510.882883	886544.247147	42.066266
3510.666765	886371.214178	42.071271
3510.800805	886181.856108	42.076276
3510.723010	885982.846506	42.081280
3510.323081	885795.596623	42.086285
3510.411203	885608.841127	42.091290
3510.331949	885432.950103	42.096295
3510.291389	885236.329005	42.101300
3510.570100	885062.013606	42.106304
3510.123254	884886.069733	42.111309
3510.265393	884699.469688	42.116314
3510.091397	884517.176116	42.121319
3510.009213	884333.312414	42.126324
3510.191501	884161.019275	42.131328
3509.803104	883991.913794	42.136333
3509.694290	883803.970625	42.141338
3509.989517	883639.584204	42.146343
3509.722576	883470.056163	42.151348
3509.952836	883289.110130	42.156352
3510.076977	883118.345243	42.161357
3510.180622	882940.411592	42.166362
3509.833773	882770.101503	42.171367
3509.664226	882594.139404	42.176372
3509.689525	882416.977547	42.181376
3509.246203	882245.505673	42.186381
3509.693618	882081.825140	42.191386
3509.521020	881919.307740	42.196391
3509.491573	881749.303013	42.201396
3509.676543	881582.745538	42.206400
3509.414249	881420.229021	42.211405
3509.229806	881255.079363	42.216410
3509.568218	881083.735205	42.221415
3509.451145	880909.942011	42.226420
3509.537525	880749.674686	42.231424
3509.202909	880593.832480	42.236429
3509.402991	880421.038322	42.241434
3509.309171	880249.256465	42.246439
3509.200746	880090.456652	42.251444
3509.388985	879930.053207	42.256448
3508.921097	879776.536872	42.261453
3508.995570	879610.135261	42.266458
3508.656302	879457.752283	42.271463
3508.698619	879301.522851	42.276468
3509.137953	879149.100492	42.281472
3508.747197	878996.326345	42.286477
3508.859343	878836.874729	42.291482
3508.697789	878674.943857	42.296487
3508.810088	878529.634741	42.301492
3508.728709	878375.921143	42.306496
3508.390079	878224.863053	42.311501
3508.724221	878066.517135	42.316506
3508.260450	877922.451126	42.321511
3508.582171	877772.145037	42.326516
3508.482599	877623.455581	42.331520
3508.174450	877481.098064	42.336525
3508.232298	877323.553230	42.341530
3508.512799	877176.244054	42.346535
3508.151437	877033.496689	42.351540
3508.519431	876881.027322	42.356544
3508.126908	876734.205796	42.361549
3508.325927	876592.421938	42.366554
3508.300817	876444.272205	42.371559
3507.853906	876304.720985	42.376564
3507.771144	876166.173084	42.381568
3508.082654	876022.514665	42.386573
3508.056130	875889.575122	42.391578
3507.538374	875756.422604	42.396583
3507.403122	875621.943400	42.401588
3507.836361	875483.973304	42.406592
3507.561384	875349.510923	42.411597
3507.428025	875207.263684	42.416602
3507.530784	875089.801775	42.421607
3507.386732	874950.362621	42.426612
3507.731002	874826.648651	42.431616
3507.355410	874696.649410	42.436621
3507.187877	874562.733378	42.441626
3507.334308	874432.351354	42.446631
3507.563599	874307.093581	42.451636
3507.603171	874180.506452	42.456640
3507.351478	874058.135595	42.461645
3507.490737	873921.632537	42.466650
3507.339379	873789.345396	42.471655
3507.527159	873668.834182	42.476660
3507.483972	873540.888951	42.481664
3507.272059	873403.655769	42.486669
3507.579520	873276.908213	42.491674
3507.589559	873149.333825	42.496679
3507.089168	873019.609409	42.501684
3507.346736	872882.868942	42.506688
3506.956093	872770.778424	42.511693
3507.362573	872646.232583	42.516698
3507.140401	872520.623410	42.521703
3507.087178	872391.878888	42.526708
3507.149412	872274.076827	42.531712
3506.773549	872165.077374	42.536717
3506.898184	872036.683985	42.541722
3506.889605	871921.312426	42.546727
3506.596546	871798.901834	42.551732
3507.067218	871672.481353	42.556736
3506.481849	871565.349166	42.561741
3506.485985	871448.025536	42.566746
3506.645044	871342.610499	42.571751
3506.490705	871229.869752	42.576756
3506.673075	871121.147401	42.581760
3506.383586	871005.416199	42.586765
3506.798763	870888.596141	42.591770
3506.062713	870782.736374	42.596775
3506.213228	870675.564002	42.601780
3506.294672	870563.936481	42.606784
3506.062511	870455.755588	42.611789
3506.542540	870356.967290	42.616794
3506.319598	870257.031376	42.621799
3506.443604	870133.838458	42.626804
3506.449994	870025.513407	42.631808
3506.226571	869920.427472	42.636813
3506.274941	869811.218018	42.641818
3506.439848	869713.927051	42.646823
3506.014427	869604.888958	42.651828
3506.176271	869490.024751	42.656832
3506.092405	869384.518109	42.661837
3506.039458	869285.411626	42.666842
3506.069836	869180.270872	42.671847
3505.893202	869073.220760	42.676852
3506.097080	868976.008461	42.681856
3505.758441	868877.913127	42.686861
3505.958780	868762.543205	42.691866
3505.957466	868681.573262	42.696871
3505.883861	868577.507020	42.701876
3505.698546	868470.544658	42.706880
3505.692098	868374.813622	42.711885
3505.870429	868277.108740	42.716890
3505.755612	868185.179188	42.721895
3506.069585	868092.983388	42.726900
3506.206047	867992.076572	42.731904
3505.878514	867888.914104	42.736909
3506.041588	867788.193677	42.741914
3505.738663	867685.314960	42.746919
3505.714618	867595.012170	42.751924
3506.208007	867490.348135	42.756928
3505.445912	867397.833422	42.761933
3505.513935	867288.574769	42.766938
3505.269708	867206.848073	42.771943
3505.374396	867123.703206	42.776948
3505.786214	867025.356823	42.781952
3505.292915	866938.811816	42.786957
3505.308314	866833.826648	42.791962
3505.543469	866759.784258	42.796967
3505.290110	866664.455117	42.801972
3505.861621	866569.474170	42.806977
3505.358380	866467.287454	42.811981
3505.461944	866378.984962	42.816986
3505.385074	866286.728742	42.821991
3504.985510	866202.877225	42.826996
3505.122247	866115.925193	42.832001
3504.770373	866037.891238	42.837005
3505.118812	865954.884330	42.842010
3504.999654	865872.147585	42.847015
3505.211314	865783.721428	42.852020
3505.332893	865688.703603	42.857025
3505.167640	865610.147684	42.862029
3505.252856	865520.572861	42.867034
3504.997970	865445.526541	42.872039
3505.053476	865363.725437	42.877044
3505.040106	865284.363125	42.882049
3505.034361	865196.061318	42.887053
3504.743642	865106.056562	42.892058
3504.919751	865035.888527	42.897063
3504.809948	864962.172337	42.902068
3505.039267	864879.656007	42.907073
3504.869768	864803.616150	42.912077
3504.799511	864711.140437	42.917082
3504.630285	864644.813657	42.922087
3504.599935	864562.432930	42.927092
3504.860557	864482.140552	42.932097
3504.657042	864418.440119	42.937101
3504.614237	864329.451658	42.942106
3504.554776	864265.045773	42.947111
3504.373474	864194.149586	42.952116
3504.904689	864119.054424	42.957121
3504.716358	864036.595401	42.962125
3504.830431	863960.789706	42.967130
3504.863071	863882.275870	42.972135
3504.831579	863802.605591	42.977140
3504.868159	863723.020216	42.982145
3504.621312	863655.723702	42.987149
3504.609081	863580.517065	42.992154
3504.648093	863503.454808	42.997159
3504.707874	863427.262697	43.002164
3504.611187	863348.374558	43.007169
3504.704721	863277.228003	43.012173
3504.587536	863195.426020	43.017178
3504.376799	863118.497190	43.022183
3504.393092	863057.564344	43.027188
3504.493904	862980.290898	43.032193
3504.035961	862911.077305	43.037197
3504.135644	862859.360839	43.042202
3504.486665	862790.401312	43.047207
3504.585467	862715.845927	43.052212
3504.496120	862645.110820	43.057217
3504.230373	862574.112394	43.062221
3503.907657	862506.135310	43.067226
3504.348363	862442.405133	43.072231
3504.148600	862379.557320	43.077236
3504.344353	862302.162408	43.082241
3504.084574	862249.236498	43.087245
3504.048409	862175.668623	43.092250
3503.958622	862106.579574	43.097255
3503.798210	862043.235829	43.102260
3504.326399	861984.151750	43.107265
3504.273195	861921.372242	43.112269
3503.999938	861851.630149	43.117274
3504.128884	861791.832403	43.122279
3503.841414	861733.171865	43.127284
3504.249623	861652.040107	43.132289
3504.053612	861600.167237	43.137293
3504.022402	861532.811635	43.142298
3504.202876	861475.626751	43.147303
3504.281440	861416.708446	43.152308
3504.818962	861340.217023	43.157313
3504.445495	861275.636711	43.162317
3504.379874	861192.146732	43.167322
3504.359837	861125.173607	43.172327
3504.185181	861066.099210	43.177332
3504.334421	860993.847425	43.182337
3504.162611	860922.619798	43.187341
3504.234931	860864.669299	43.192346
3504.212600	860799.540015	43.197351
3504.012556	860738.425127	43.202356
3504.044236	860664.633367	43.207361
3504.178180	860602.489928	43.212365
3504.344087	860541.896078	43.217370
3503.847957	860472.077667	43.222375
3503.982970	860416.154175	43.227380
3504.158109	860347.779265	43.232385
3503.966461	860279.172352	43.237389
3504.043033	860221.312258	43.242394
3503.970134	860158.323361	43.247399
3504.089850	860096.177106	43.252404
3504.068338	860042.220479	43.257409
3503.670075	859979.283338	43.262413
3504.009568	859912.432103	43.267418
3504.269714	859853.760454	43.272423
3503.839551	859792.771224	43.277428
3504.081780	859717.474864	43.282433
3503.847068	859667.730991	43.287437
3503.884926	859594.703124	43.292442
3503.649456	859548.069860	43.297447
3503.555844	859493.925796	43.302452
3504.200024	859426.338400	43.307457
3503.494578	859367.918407	43.312461
3503.546785	859317.249274	43.317466
3503.529098	859272.522775	43.322471
3503.781201	859212.971153	43.327476
3503.873601	859154.320425	43.332481
3503.708341	859095.711586	43.337485
3503.471840	859045.087763	43.342490
3503.644098	858989.242309	43.347495
3502.980439	858933.825799	43.352500
3503.506062	858884.825470	43.357505
3503.389936	858837.680895	43.362509
3503.410602	858787.109810	43.367514
3503.552262	858730.586314	43.372519
3502.970602	858683.225507	43.377524
3503.445963	858629.369030	43.382529
3503.427499	858583.859633	43.387533
3503.292451	858533.701105	43.392538
3503.323862	858484.487248	43.397543
3503.338841	858447.432142	43.402548
3503.260458	858393.081313	43.407553
3503.271099	858346.592833	43.412557
3503.376755	858294.642133	43.417562
3503.258165	858245.353814	43.422567
3503.076601	858197.728815	43.427572
3503.538112	858150.483775	43.432577
3503.260574	858106.180583	43.437581
3503.616752	858049.323685	43.442586
3503.460636	857998.094403	43.447591
3503.388755	857958.716444	43.452596
3503.655050	857898.566144	43.457601
3503.312827	857849.700525	43.462605
3503.186000	857799.826411	43.467610
3503.257419	857752.059003	43.472615
3503.209119	857710.924842	43.477620
3503.510711	857650.863560	43.482625
3503.509582	857612.736154	43.487629
3503.196846	857565.905969	43.492634
3503.483482	857515.766892	43.497639
3503.462868	857470.249575	43.502644
3503.545502	857409.735672	43.507649
3503.363554	857361.715164	43.512653
3503.410285	857313.462065	43.517658
3503.339525	857264.547052	43.522663
3503.379068	857214.446224	43.527668
3503.620275	857168.786262	43.532673
3503.160210	857125.673310	43.537677
3503.176962	857070.905988	43.542682
3503.376134	857022.625486	43.547687
3503.294086	856975.460961	43.552692
3503.259412	856920.214394	43.557697
3503.088261	856875.106565	43.562701
3503.404660	856830.501740	43.567706
3503.263557	856779.065242	43.572711
3503.181291	856740.070280	43.577716
3503.176050	856693.474604	43.582721
3503.177121	856654.951767	43.587725
3502.899729	856603.244410	43.592730
3503.023995	856567.521866	43.597735
3502.884387	856530.480645	43.602740
3503.066151	856475.583546	43.607745
3502.906969	856443.701006	43.612749
3503.268798	856394.610506	43.617754
3503.136246	856354.064834	43.622759
3502.858646	856312.472654	43.627764
3502.988801	856254.760813	43.632769
3502.828665	856221.709843	43.637773
3503.003573	856175.566993	43.642778
3502.773042	856129.296019	43.647783
3502.684096	856104.015735	43.652788
3502.994354	856055.320180	43.657793
3503.033514	856018.538287	43.662797
3503.250670	855974.040893	43.667802
3502.950922	855922.234197	43.672807
3502.760222	855886.170423	43.677812
3502.963546	855844.009376	43.682817
3502.950625	855804.802468	43.687821
3503.129274	855769.650091	43.692826
3502.848884	855730.000304	43.697831
3502.786345	855694.108877	43.702836
3503.138356	855647.154527	43.707841
3502.922154	855616.736527	43.712845
3502.706388	855568.999459	43.717850
3502.844558	855531.809156	43.722855
3502.871343	855499.404590	43.727860
3502.806250	855452.030983	43.732865
3503.117640	855418.606112	43.737869
3502.794174	855374.971857	43.742874
3502.549105	855331.129774	43.747879
3502.697937	855291.503743	43.752884
3503.129042	855250.468724	43.757889
3502.750087	855222.313535	43.762893
3502.710263	855174.544420	43.767898
3502.852843	855134.918413	43.772903
3502.962498	855104.346889	43.777908
3502.771260	855058.645213	43.782913
3502.712949	855022.554565	43.787917
3502.588725	854986.377258	43.792922
3502.741971	854954.435522	43.797927
3502.548834	854926.637592	43.802932
3502.956485	854877.040917	43.807937
3502.693668	854846.042940	43.812941
3502.704524	854809.355796	43.817946
3502.611432	854767.820079	43.822951
3502.683347	854744.453901	43.827956
3502.793251	854702.397748	43.832961
3502.805703	854675.051363	43.837965
3502.757671	854623.386882	43.842970
3502.788139	854589.322621	43.847975
3502.468801	854560.668019	43.852980
3502.900175	854516.611377	43.857985
3502.504930	854480.475753	43.862989
3502.674412	854443.857615	43.867994
3502.682154	854409.601477	43.872999
3502.502469	854385.594185	43.878004
3502.422276	854335.295010	43.883009
3502.512706	854315.232916	43.888013
3502.595427	854273.859539	43.893018
3502.771933	854245.219094	43.898023
3502.637249	854203.005200	43.903028
3502.872280	854157.226610	43.908033
3502.423821	854134.430455	43.913037
3502.559582	854097.621181	43.918042
3502.975807	854069.329707	43.923047
3502.200309	854032.475539	43.928052
3502.480350	854003.427630	43.933057
3502.459966	853980.755021	43.938061
3502.519742	853938.215311	43.943066
3502.817137	853917.825860	43.948071
3502.271636	853886.577662	43.953076
3502.757937	853839.976735	43.958081
3502.968882	853816.973439	43.963085
3502.823315	853770.670745	43.968090
3502.859255	853730.274689	43.973095
3502.557483	853699.180037	43.978100
3502.834044	853663.318244	43.983105
3502.892081	853631.580008	43.988109
3502.736206	853589.462738	43.993114
3502.826998	853558.400027	43.998119
3502.783093	853521.714254	44.003124
3502.577151	853483.595012	44.008129
3502.839436	853451.724872	44.013133
3502.700329	853408.046316	44.018138
3502.702680	853377.386591	44.023143
3502.614048	853343.140417	44.028148
3502.823450	853307.774291	44.033153
3502.498812	853269.186618	44.038157
3502.893439	853227.560183	44.043162
3502.852362	853191.163986	44.048167
3502.546801	853165.810005	44.053172
3502.578671	853121.127903	44.058177
3502.387056	853089.720024	44.063181
3502.684561	853069.814446	44.068186
3502.779468	853027.944042	44.073191
3502.608144	852992.249492	44.078196
3502.906513	852953.070513	44.083201
3502.335266	852925.228523	44.088205
3502.424949	852896.498800	44.093210
3502.843707	852855.547265	44.098215
3502.285228	852828.286772	44.103220
3502.556312	852786.677730	44.108225
3502.627622	852757.366344	44.113229
3502.696691	852723.285439	44.118234
3502.580452	852696.243527	44.123239
3502.544851	852669.188210	44.128244
3502.559952	852625.089348	44.133249
3502.365082	852593.387455	44.138253
3502.345939	852558.054703	44.143258
3502.785781	852521.088608	44.148263
3502.582499	852498.538044	44.153268
3502.379153	852461.385526	44.158273
3502.630313	852438.857218	44.163277
3502.298334	852391.796140	44.168282
3502.440647	852372.497978	44.173287
3502.441305	852338.523575	44.178292
3502.486608	852302.886706	44.183297
3502.625742	852281.544466	44.188301
3502.467664	852251.587039	44.193306
3502.613471	852222.747598	44.198311
3502.580428	852193.450738	44.203316
3502.594968	852158.694261	44.208321
3502.242913	852135.193376	44.213325
3502.626394	852098.039346	44.218330
3502.343304	852067.712220	44.223335
3502.115094	852038.836193	44.228340
3502.403268	852009.874954	44.233345
3502.371921	851973.762057	44.238349
3502.385453	851950.005528	44.243354
3502.952456	851911.457190	44.248359
3502.493659	851879.503062	44.253364
3502.841995	851846.929010	44.258369
3502.542663	851814.753565	44.263373
3502.224363	851778.978879	44.268378
3502.924520	851743.815047	44.273383
3502.687255	851714.939003	44.278388
3502.629140	851671.040132	44.283393
3502.313804	851647.433987	44.288397
3502.286601	851622.027815	44.293402
3502.412719	851586.762955	44.298407
3502.532481	851567.660725	44.303412
3502.374805	851525.334987	44.308417
3502.308582	851500.908355	44.313421
3502.615770	851476.128020	44.318426
3502.398429	851437.316523	44.323431
3502.145084	851404.060385	44.328436
3502.650505	851379.441730	44.333441
3502.312002	851348.146582	44.338445
3502.138949	851319.647570	44.343450
3502.523293	851297.190544	44.348455
3502.437381	851271.889976	44.353460
3502.515825	851240.915051	44.358465
3502.781402	851216.140536	44.363469
3502.527844	851178.307042	44.368474
3502.644379	851145.475408	44.373479
3502.409430	851113.090979	44.378484
3502.779010	851076.419971	44.383489
3502.637656	851038.761874	44.388493
3502.524767	851012.198905	44.393498
3502.647230	850978.878571	44.398503
3502.657429	850946.452883	44.403508
3502.491544	850914.932370	44.408513
3502.677603	850879.653621	44.413517
3503.008886	850846.785030	44.418522
3502.938303	850800.545148	44.423527
3502.527986	850769.940519	44.428532
3502.901670	850729.664007	44.433537
3502.864220	850697.244870	44.438541
3502.621103	850665.151572	44.443546
3502.523138	850629.041830	44.448551
3502.414480	850593.128390	44.453556
3502.502847	850557.571786	44.458561
3502.513165	850537.705418	44.463565
3502.518305	850506.738913	44.468570
3502.612684	850475.465419	44.473575
3502.541612	850445.971825	44.478580
3502.763282	850408.347475	44.483585
3502.698403	850379.923707	44.488589
3502.563413	850347.324059	44.493594
3502.623465	850315.471143	44.498599
3502.549361	850287.632751	44.503604
3502.828730	850245.226285	44.508609
3502.792942	850223.029371	44.513613
3502.267644	850176.859769	44.518618
3502.639780	850142.520004	44.523623
3502.616588	850121.489241	44.528628
3502.683680	850086.809897	44.533633
3502.781941	850055.533655	44.538637
3502.401346	850016.155873	44.543642
3502.523950	849990.134043	44.548647
3502.235881	849963.108529	44.553652
3502.427900	849924.025363	44.558657
3502.460844	849895.680652	44.563661
3502.684660	849870.810282	44.568666
3502.941208	849836.195716	44.573671
3502.548687	849795.942021	44.578676
3502.615542	849760.968739	44.583681
3502.170477	849736.305424	44.588685
3502.536509	849701.087737	44.593690
3502.585236	849677.901063	44.598695
3502.638793	849649.357056	44.603700
3502.637351	849621.503714	44.608705
3502.421107	849580.050893	44.613709
3502.305718	849547.151651	44.618714
3502.671517	849518.166033	44.623719
3502.361869	849491.823771	44.628724
3502.412194	849453.150569	44.633729
3502.019400	849429.646142	44.638733
3502.505397	849400.153206	44.643738
3502.489059	849367.431483	44.648743
3502.523888	849351.258281	44.653748
3502.605601	849311.410292	44.658753
3502.434730	849282.219813	44.663757
3502.623421	849251.119429	44.668762
3502.592252	849218.983748	44.673767
3502.472325	849188.713074	44.678772
3502.503871	849155.300568	44.683777
3502.595328	849130.741251	44.688781
3502.463586	849089.953034	44.693786
3502.680980	849060.113153	44.698791
3502.418437	849021.196623	44.703796
3502.509061	848987.773486	44.708801
3502.591040	848970.714926	44.713805
3502.636710	848932.234063	44.718810
3502.754070	848898.806046	44.723815
3502.504794	848866.899290	44.728820
3502.587954	848821.593406	44.733825
3502.505345	848800.762782	44.738829
3502.345486	848769.912234	44.743834
3502.693750	848739.075220	44.748839
3502.582277	848719.515335	44.753844
3502.663791	848672.455358	44.758849
3502.419865	848640.936186	44.763853
3502.014867	848611.099298	44.768858
3502.120922	848597.737190	44.773863
3501.707569	848564.881856	44.778868
3502.157361	848539.287105	44.783873
3502.279632	848526.506617	44.788877
3502.175516	848502.658905	44.793882
3502.212024	848469.241910	44.798887
3502.442946	848446.994729	44.803892
3502.460114	848419.035544	44.808897
3502.468756	848388.642395	44.813901
3502.328784	848359.345096	44.818906
3502.253404	848323.315680	44.823911
3502.322519	848308.108235	44.828916
3502.323475	848269.435833	44.833921
3502.481961	848243.595635	44.838925
3502.125884	848219.009056	44.843930
3502.235718	848190.449106	44.848935
3502.077009	848166.024626	44.853940
3502.175961	848138.927432	44.858945
3501.866830	848110.825800	44.863949
3501.896649	848097.670012	44.868954
3502.016818	848076.316490	44.873959
3501.975489	848053.041204	44.878964
3501.991062	848024.885688	44.883969
3501.920772	848021.974843	44.888973
3501.897207	847986.811688	44.893978
3502.291426	847963.756558	44.898983
3502.190992	847949.355506	44.903988
3502.111109	847913.616719	44.908993
3501.917990	847906.050032	44.913997
3501.872460	847866.603460	44.919002
3501.929763	847863.087012	44.924007
3502.000982	847845.345228	44.929012
3502.064772	847813.381506	44.934017
3501.869491	847798.313801	44.939021
3501.789180	847780.207123	44.944026
3502.005328	847739.839864	44.949031
3501.592262	847735.621483	44.954036
3501.916368	847718.519614	44.959041
3502.179170	847699.576811	44.964045
3501.735454	847681.042617	44.969050
3501.833821	847647.318775	44.974055
3501.670477	847627.958860	44.979060
3501.976513	847621.576069	44.984065
3502.133275	847590.180419	44.989069
3501.841509	847569.087880	44.994074
3501.917169	847556.702782	44.999079
3501.841720	847535.477068	45.004084
3501.954797	847508.861933	45.009089
3502.021648	847498.718911	45.014093
3502.198866	847471.605932	45.019098
3502.319040	847445.671328	45.024103
3501.893500	847421.482750	45.029108
3501.814484	847397.821535	45.034113
3501.856718	847389.046343	45.039117
3501.733727	847356.234232	45.044122
3502.285918	847332.273922	45.049127
3501.628984	847317.670823	45.054132
3501.981256	847291.210208	45.059137
3502.231000	847285.518340	45.064141
3501.733552	847254.326219	45.069146
3502.189541	847225.217698	45.074151
3502.063920	847220.561893	45.079156
3502.181307	847192.970428	45.084161
3501.901461	847165.249431	45.089165
3502.395574	847154.158597	45.094170
3502.064944	847118.456580	45.099175
3502.125320	847100.811904	45.104180
3502.056575	847073.348009	45.109185
3501.993511	847054.262086	45.114189
3502.050891	847031.356458	45.119194
3502.242707	847009.890066	45.124199
3501.689673	847000.530386	45.129204
3501.596728	846970.536811	45.134209
3501.643407	846956.986121	45.139213
3502.082691	846951.555020	45.144218
3502.118980	846927.288437	45.149223
3501.931244	846905.689357	45.154228
3501.946638	846880.744007	45.159233
3501.963417	846856.967533	45.164237
3502.163509	846840.273440	45.169242
3502.191167	846814.059164	45.174247
3502.147939	846800.522950	45.179252
3501.926292	846780.000802	45.184257
3501.927158	846755.836827	45.189261
3501.734822	846737.940460	45.194266
3502.416085	846722.238566	45.199271
3501.892757	846700.206890	45.204276
3501.799666	846671.088830	45.209281
3501.781930	846642.445404	45.214285
3501.496556	846623.102484	45.219290
3501.711875	846613.713066	45.224295
3501.717974	846610.691540	45.229300
3501.663885	846581.274324	45.234305
3501.596926	846558.290016	45.239309
3501.455771	846556.267107	45.244314
3501.661934	846537.232690	45.249319
3501.690453	846527.679043	45.254324
3501.905420	846498.899183	45.259329
3502.008900	846494.010212	45.264333
3501.770463	846480.310589	45.269338
3501.659977	846446.517258	45.274343
3501.833288	846434.795935	45.279348
3502.031667	846421.024214	45.284353
3501.636003	846388.154516	45.289357
3501.929354	846373.879840	45.294362
3501.771673	846363.577093	45.299367
3501.728564	846341.367590	45.304372
3501.740129	846317.979698	45.309377
3502.108433	846311.975092	45.314381
3501.926273	846293.686011	45.319386
3501.928048	846270.104669	45.324391
3501.734728	846265.459306	45.329396
3501.720602	846238.859740	45.334401
3501.847167	846214.672970	45.339405
3501.749273	846209.816956	45.344410
3502.028846	846183.753429	45.349415
3501.970791	846166.223081	45.354420
3501.544919	846149.727730	45.359425
3501.851826	846139.737849	45.364429
3501.655809	846111.413705	45.369434
3501.889287	846091.496432	45.374439
3501.698320	846087.532667	45.379444
3501.891867	846061.482806	45.384449
3501.896746	846049.203840	45.389453
3502.013292	846038.563039	45.394458
3501.945785	846006.611736	45.399463
3502.078971	845994.603864	45.404468
3502.126430	845964.192555	45.409473
3502.254272	845952.770168	45.414477
3501.891792	845931.683758	45.419482
3502.003553	845891.711598	45.424487
3501.985773	845885.672750	45.429492
3502.069292	845869.872325	45.434497
3501.524795	845841.701826	45.439501
3501.830526	845828.593267	45.444506
3502.328487	845808.728972	45.449511
3502.292578	845785.736719	45.454516
3502.225846	845759.143788	45.459521
3502.162632	845727.872513	45.464525
3501.827864	845708.242552	45.469530
3502.079263	845677.503900	45.474535
3502.148839	845663.556838	45.479540
3502.141738	845641.338927	45.484545
3502.158009	845619.311992	45.489549
3501.951727	845595.762396	45.494554
3502.174708	845564.638062	45.499559
3501.969956	845552.490117	45.504564
3501.994462	845530.071697	45.509569
3501.989763	845504.539463	45.514573
3501.783660	845494.438174	45.519578
3502.202831	845477.996734	45.524583
3501.887762	845444.524079	45.529588
3502.224684	845435.112871	45.534593
3502.085518	845404.924514	45.539597
3501.961580	845388.572323	45.544602
3502.078925	845365.943109	45.549607
3502.269546	845341.060227	45.554612
3502.008451	845321.514374	45.559617
3501.847625	845299.320581	45.564621
3501.754358	845279.941862	45.569626
3502.210968	845260.667404	45.574631
3502.039358	845237.500585	45.579636
3502.015874	845221.813620	45.584641
3501.971450	845204.863096	45.589645
3501.812020	845193.291743	45.594650
3501.959653	845181.279940	45.599655
3501.981868	845157.106295	45.604660
3501.994096	845137.612296	45.609665
3501.676568	845127.138932	45.614669
3501.684779	845093.806065	45.619674
3502.270345	845069.246883	45.624679
3501.943696	845064.427671	45.629684
3502.009623	845024.652474	45.634689
3502.027528	845019.094224	45.639693
3501.668740	844998.296452	45.644698
3502.085425	844968.306804	45.649703
3501.796744	844957.243626	45.654708
3501.921369	844938.607660	45.659713
3501.965688	844909.361326	45.664717
3501.894503	844891.147336	45.669722
3501.676858	844854.439169	45.674727
3501.777409	844856.274467	45.679732
3501.949612	844847.864170	45.684737
3502.058741	844830.497479	45.689741
3501.853387	844800.317124	45.694746
3501.860194	844784.136749	45.699751
3501.917129	844761.905180	45.704756
3501.742933	844750.822775	45.709761
3502.041833	844738.590273	45.714765
3502.067833	844711.295366	45.719770
3502.454584	844684.525707	45.724775
3501.822050	844665.623813	45.729780
3501.673255	844630.754880	45.734785
3501.962908	844625.346446	45.739789
3502.038576	844608.374529	45.744794
3502.333760	844581.522051	45.749799
3502.010210	844562.861346	45.754804
3502.275393	844539.327582	45.759809
3502.061128	844519.381638	45.764813
3501.829726	844487.839497	45.769818
3502.063138	844405.633065	45.774823
3501.693142	844268.550047	45.779828
3501.657033	844069.804008	45.784833
3501.856216	843815.059252	45.789837
3501.510837	843516.233230	45.794842
3501.273093	843152.641660	45.799847
3501.539420	842737.370215	45.804852
3501.139012	842248.858096	45.809857
3501.067701	841712.472771	45.814861
3500.670215	841114.364421	45.819866
3500.714932	840456.729818	45.824871
3500.395580	839741.878150	45.829876
3500.125689	838953.723003	45.834881
3499.998199	838099.734798	45.839885
3499.474708	837203.932507	45.844890
3499.147037	836235.507069	45.849895
3498.717522	835193.742802	45.854900
3498.533830	834096.022785	45.859905
3498.187693	832925.004913	45.864909
3497.769465	831692.403635	45.869914
3497.480634	830394.732158	45.874919
3497.106612	829036.384268	45.879924
3496.690103	827592.835021	45.884929
3496.166908	826081.341191	45.889933
3495.797712	824511.591223	45.894938
3495.145028	822847.186950	45.899943
3494.533306	821142.296906	45.904948
3494.142643	819353.318683	45.909953
3493.437684	817494.172970	45.914957
3492.913224	815579.407385	45.919962
3492.079932	813574.780124	45.924967
3491.358083	811530.008089	45.929972
3490.410709	809398.173644	45.934977
3489.739466	807208.866277	45.939981
3488.852424	804966.429704	45.944986
3488.329740	802640.605570	45.949991
3487.414691	800249.640515	45.954996
3487.154896	797795.311033	45.960001
3485.969204	795254.444704	45.965005
3485.039585	792659.714729	45.970010
3484.297897	790001.693651	45.975015
3483.415664	787272.898943	45.980020
3482.333940	784480.690514	45.985025
3481.322346	781623.431718	45.990029
3480.569314	778694.476326	45.995034
3479.594927	775694.760016	46.000039
3478.397913	772653.657801	46.005044
3477.205706	769520.781083	46.010049
3476.112719	766334.950779	46.015053
3474.961443	763098.749029	46.020058
3473.965289	759774.194574	46.025063
3472.609076	756403.322319	46.030068
3471.218397	752963.313372	46.035073
3470.212486	749459.206026	46.040077
3469.114381	745900.940304	46.045082
3467.909360	742269.370941	46.050087
3466.386611	738583.245906	46.055092
3465.195813	734822.599150	46.060097
3463.887659	731005.144378	46.065101
3462.454428	727132.801277	46.070106
3461.550378	723185.773166	46.075111
3459.651290	719180.885381	46.080116
3457.966087	715105.718805	46.085121
3456.697688	710991.629690	46.090125
3455.368315	706797.043406	46.095130
3453.764815	702546.594119	46.100135
3451.987935	698243.685939	46.105140
3450.346825	693881.450230	46.110145
3449.193255	689455.635943	46.115149
3447.281931	684965.234822	46.120154
3445.645582	680409.558962	46.125159
3443.992766	675804.584377	46.130164
3442.428622	671128.410037	46.135169
3440.549070	666409.111757	46.140173
3438.864674	661616.875126	46.145178
3437.027422	656767.610000	46.150183
3435.411079	651871.644426	46.155188
3433.247757	646908.875632	46.160193
3431.798218	641880.631907	46.165197
3429.462734	636807.480251	46.170202
3427.429511	631677.281606	46.175207
3425.348639	626492.251812	46.180212
3423.642972	621264.256054	46.185217
3421.363748	615973.024892	46.190221
3419.333214	610620.077907	46.195226
3417.520376	605226.249009	46.200231
3415.160494	599781.960202	46.205236
3412.958790	594277.374359	46.210241
3411.255781	588726.315906	46.215245
3408.490268	583114.495110	46.220250
3406.315139	577451.361085	46.225255
3404.113152	571747.964515	46.230260
3401.710716	565988.773863	46.235265
3399.242775	560187.896097	46.240269
3396.645457	554341.660771	46.245274
3394.761537	548444.478999	46.250279
3391.976497	542509.516130	46.255284
3389.698224	536511.170282	46.260289
3387.117547	530469.741363	46.265293
3384.563290	524387.957141	46.270298
3382.063288	518256.579110	46.275303
3379.239038	512088.556705	46.280308
3376.586670	505864.262281	46.285313
3374.106068	499609.283171	46.290317
3370.854256	493314.798467	46.295322
3368.210138	486981.259423	46.300327
3365.494475	480609.763209	46.305332
3362.599001	474208.203976	46.310337
3360.219332	467755.427677	46.315341
3356.784632	461272.539344	46.320346
3354.178876	454751.004799	46.325351
3351.446289	448193.500090	46.330356
3348.032439	441591.632515	46.335361
3345.013707	434973.368155	46.340365
3341.903275	428311.285656	46.345370
3338.628502	421633.662511	46.350375
3335.800240	414913.519576	46.355380
3332.401864	408180.605224	46.360385
3329.388915	401399.440322	46.365389
3326.019981	394601.165107	46.370394
3322.882662	387770.626621	46.375399
3319.684975	380926.590217	46.380404
3316.520773	374046.609099	46.385409
3313.145686	367137.166000	46.390413
3309.013410	360202.078678	46.395418
3305.880792	353236.419771	46.400423
3302.271403	346272.000762	46.405428
3298.670120	339299.562582	46.410433
3295.418560	332303.807311	46.415437
3291.577916	325285.270154	46.420442
3287.716623	318238.308048	46.425447
3283.884963	311210.191353	46.430452
3280.408475	304158.919720	46.435457
3276.776022	297079.361008	46.440461
3272.927471	290015.762397	46.445466
3269.315861	282921.000069	46.450471
3264.898732	275838.801425	46.455476
3261.205736	268731.208076	46.460481
3257.585326	261626.835941	46.465485
3253.576347	254517.520692	46.470490
3249.432383	247404.938293	46.475495
3245.160827	240294.192649	46.480500
3241.098535	233174.645587	46.485505
3237.335307	226039.597826	46.490509
3232.956735	218868.844159	46.495514
3228.712245	211758.424332	46.500519
3224.465076	204642.750340	46.505524
3220.001534	197544.374503	46.510529
3216.132921	190457.836660	46.515533
3211.373451	183383.885103	46.520538
3206.869888	176313.239355	46.525543
3202.354891	169259.590527	46.530548
3197.884617	162227.663712	46.535553
3193.224699	155205.999928	46.540557
3188.564731	148216.314973	46.545562
3183.809079	141219.841301	46.550567
3178.743222	134272.411770	46.555572
3173.999802	127338.813690	46.560577
3169.075977	120431.019048	46.565581
3163.743810	113568.639431	46.570586
3158.933239	106731.861987	46.575591
3153.380673	99926.300491	46.580596
3147.835884	93173.810926	46.585601
3142.515295	86449.745632	46.590605
3136.399086	79767.974018	46.595610
3130.554866	73159.496227	46.600615
3124.378582	66599.383154	46.605620
3117.869090	60107.812268	46.610625
3111.435282	53685.855468	46.615629
3103.929813	47348.248204	46.620634
3095.781234	41109.155275	46.625639
3085.008889	35052.978327	46.630644
3064.885749	29379.819908	46.635649
3038.402202	24107.627956	46.640653
3008.636296	19271.861710	46.645658
2978.570397	14917.485764	46.650663
2949.032820	11093.794549	46.655668
2922.130650	7756.557690	46.660673
2898.199313	4937.832324	46.665677
2876.476883	2624.731183	46.670682
2856.149330	827.732142	46.675687
2807.566157	291.962664	46.680692
2765.300160	290.337711	46.685697
2752.292561	291.081675	46.690701
2760.756771	282.994018	46.695706
2779.266812	272.266877	46.700711
2797.587888	263.654131	46.705716
2810.494044	276.215352	46.710721
2816.967551	273.468738	46.715725
2817.589998	268.112818	46.720730
2814.548736	263.103639	46.725735
2810.076158	265.967375	46.730740
2806.238153	270.505658	46.735745
2803.140923	254.823967	46.740749
2799.585634	260.440459	46.745754
2797.191271	267.221153	46.750759
2794.569449	263.140942	46.755764
2792.146644	263.942118	46.760769
2789.992241	255.519431	46.765773
2786.951701	258.356881	46.770778
2784.216190	256.203737	46.775783
2781.310099	243.694194	46.780788
2777.460180	258.557039	46.785793
2775.052301	253.458776	46.790797
2771.446227	247.896724	46.795802
2768.636629	248.324815	46.800807
2765.337294	247.089602	46.805812
2762.020604	250.332977	46.810817
2759.009177	233.908203	46.815821
2755.953253	250.740159	46.820826
2752.508352	237.904337	46.825831
2749.443534	242.574779	46.830836
2745.978267	245.036338	46.835841
2742.668414	236.644885	46.840845
2739.670504	242.706210	46.845850
2736.216983	238.994951	46.850855
2732.711386	241.120587	46.855860
2729.390219	240.649952	46.860865
2726.343113	232.183584	46.865869
2722.506220	240.985901	46.870874
2719.011492	235.783628	46.875879
2715.986074	233.475889	46.880884
2712.474380	239.563593	46.885889
2709.298507	238.292259	46.890893
2705.781297	236.539691	46.895898
2702.479557	229.646338	46.900903
2698.930560	234.563256	46.905908
2695.546907	233.964816	46.910913
2692.739514	225.851235	46.915917
2689.350659	231.032221	46.920922
2685.803630	230.417726	46.925927
2681.976234	223.549955	46.930932
2678.469298	230.024470	46.935937
2675.661745	223.587150	46.940941
2671.906042	236.354904	46.945946
2668.042504	223.696783	46.950951
2665.073749	229.845293	46.955956
2661.746094	234.907266	46.960961
2658.731048	224.667476	46.965965
2654.336666	230.677087	46.970970
2651.426834	215.001732	46.975975
2648.153569	226.711857	46.980980
2644.354984	227.603574	46.985985
2640.785143	221.800817	46.990989
2637.548075	217.533328	46.995994
2633.527318	213.503708	47.000999
2630.295493	233.500879	47.006004
2627.367336	225.396218	47.011009
2623.861971	226.878949	47.016013
2620.180731	226.374269	47.021018
2616.912782	226.302635	47.026023
2613.671823	227.168264	47.031028
2610.052373	227.125041	47.036033
2606.233968	228.804688	47.041037
2602.557683	226.497474	47.046042
2599.826274	219.866872	47.051047
2596.356218	218.952804	47.056052
2592.253667	222.083636	47.061057
2589.317165	210.736881	47.066061
2585.689292	222.701320	47.071066
2581.865138	219.487864	47.076071
2578.430533	216.983702	47.081076
2575.248595	222.943654	47.086081
2572.191507	212.193838	47.091085
2568.376535	218.092499	47.096090
2565.070124	217.921867	47.101095
2561.327853	218.258900	47.106100
2558.029453	215.862124	47.111105
2554.529629	211.696472	47.116109
2550.953326	215.409471	47.121114
2547.448570	212.514727	47.126119
2544.240759	215.759602	47.131124
2540.507820	224.862989	47.136129
2537.242017	217.541914	47.141133
2533.446793	216.459746	47.146138
2530.013841	216.428032	47.151143
2526.383686	213.715425	47.156148
2523.204003	216.444951	47.161153
2520.131813	215.674453	47.166157
2516.122863	221.184830	47.171162
2512.478645	215.474177	47.176167
2509.575158	208.965181	47.181172
2505.693673	214.984585	47.186177
2502.376230	209.531412	47.191181
2498.637005	208.428189	47.196186
2495.001587	211.847076	47.201191
2492.111339	207.154604	47.206196
2488.303325	206.328956	47.211201
2484.890702	198.769896	47.216205
2481.180532	204.551264	47.221210
2477.499403	196.736768	47.226215
2474.632841	201.355685	47.231220
2470.793644	206.433918	47.236225
2467.607972	200.458962	47.241229
2463.969383	204.889371	47.246234
2460.103144	202.753539	47.251239
2456.910360	197.946643	47.256244
2453.753576	198.365514	47.261249
2450.431498	199.213456	47.266253
2446.887520	205.522339	47.271258
2443.190832	198.810219	47.276263
2439.516368	196.113284	47.281268
2435.826735	211.163556	47.286273
2432.451007	204.209017	47.291277
2428.900683	208.416687	47.296282
2425.545971	202.849347	47.301287
2422.248780	203.425211	47.306292
2418.291911	202.323835	47.311297
2415.542172	195.275061	47.316301
2411.413985	198.894735	47.321306
2407.958504	198.624293	47.326311
2405.057097	204.683075	47.331316
2401.076899	203.040706	47.336321
2397.529490	195.386547	47.341325
2393.900163	187.912669	47.346330
2390.575483	201.669731	47.351335
2387.190897	198.599767	47.356340
2383.533143	194.423219	47.361345
2380.392981	198.967366	47.366349
2376.276625	203.396187	47.371354
2373.457079	194.644466	47.376359
2370.197217	188.940347	47.381364
2366.453482	197.104498	47.386369
2362.962150	193.148748	47.391373
2359.331304	200.564504	47.396378
2355.487550	200.318529	47.401383
2351.857984	204.070449	47.406388
2348.411898	199.884244	47.411393
2345.379450	185.385611	47.416397
2341.733871	184.475443	47.421402
2338.173971	186.601031	47.426407
2334.603821	185.580535	47.431412
2331.265977	193.671190	47.436417
2328.126921	184.183481	47.441421
2324.380160	198.361717	47.446426
2320.875501	190.532825	47.451431
2317.235103	183.384676	47.456436
2313.336201	187.314486	47.461441
2310.609863	187.766582	47.466445
2307.035343	199.341102	47.471450
2303.585285	194.491734	47.476455
2300.042229	193.392984	47.481460
2296.433720	188.796329	47.486465
2292.996730	182.325045	47.491469
2288.986783	190.190216	47.496474
2285.491092	189.117601	47.501479
2282.390745	191.812860	47.506484
2278.730559	193.446699	47.511489
2275.163727	180.538110	47.516493
2271.904437	185.297549	47.521498
2268.336274	182.045447	47.526503
2264.950217	183.495307	47.531508
2261.193771	186.910456	47.536513
2257.379469	183.521591	47.541517
2254.553808	184.240935	47.546522
2251.012566	184.268539	47.551527
2247.609350	179.143892	47.556532
2243.795602	185.527829	47.561537
2240.680987	172.379442	47.566541
2237.206219	179.318775	47.571546
2233.249879	185.795332	47.576551
2229.997209	179.808526	47.581556
2226.088722	184.187157	47.586561
2223.077976	177.229363	47.591565
2219.633760	174.815068	47.596570
2215.527158	176.119097	47.601575
2212.461641	183.489951	47.606580
2208.780905	186.788640	47.611585
2205.599843	174.180122	47.616589
2201.771426	178.730456	47.621594
2198.234152	166.578996	47.626599
2195.191753	178.822904	47.631604
2190.997245	186.788675	47.636609
2188.045617	172.601851	47.641613
2184.345663	180.717446	47.646618
2181.118119	168.565773	47.651623
2177.824818	168.182085	47.656628
2173.900985	173.852705	47.661633
2170.176515	169.681823	47.666637
2166.780273	172.723202	47.671642
2163.340084	177.305171	47.676647
2160.204300	167.745028	47.681652
2156.399043	165.423154	47.686657
2153.008149	168.180475	47.691661
2149.279886	173.302185	47.696666
2145.768091	173.665415	47.701671
2142.491152	162.011140	47.706676
2138.531102	171.854597	47.711681
2135.491155	164.916098	47.716685
2131.973752	173.686153	47.721690
2128.669797	169.296679	47.726695
2125.311738	160.381867	47.731700
2121.249680	170.026289	47.736705
2118.080450	168.440484	47.741709
2114.415452	171.495096	47.746714
2110.887856	167.653280	47.751719
2107.475695	171.269809	47.756724
2103.521262	171.587364	47.761729
2100.362960	172.858232	47.766733
2096.937529	169.671696	47.771738
2093.689843	163.302322	47.776743
2089.988608	171.022917	47.781748
2086.050654	174.218531	47.786753
2082.791871	158.761529	47.791757
2079.378800	169.146781	47.796762
2075.935081	173.199335	47.801767
2072.538051	167.876857	47.806772
2068.867103	174.760877	47.811777
2065.635350	161.966668	47.816781
2061.927455	163.208732	47.821786
2058.478167	160.471561	47.826791
2054.986287	165.993973	47.831796
2051.335624	170.146235	47.836801
2048.116756	164.883553	47.841805
2044.484383	168.481432	47.846810
2040.766328	165.878645	47.851815
2037.110064	158.657384	47.856820
2033.429320	166.739315	47.861825
2030.542916	158.803046	47.866829
2027.099986	161.337959	47.871834
2023.600287	168.977164	47.876839
2019.993857	162.639858	47.881844
2016.158298	174.022024	47.886849
2012.660593	165.579308	47.891853
2009.610238	177.377646	47.896858
2005.922518	169.587342	47.901863
2002.443291	163.092286	47.906868
1998.517203	170.193726	47.911873
1995.637209	155.008932	47.916877
1992.230684	169.658055	47.921882
1988.612208	164.242957	47.926887
1985.159687	154.397025	47.931892
1981.021730	168.180650	47.936897
1977.847611	162.589755	47.941901
1974.459033	160.498182	47.946906
1971.087072	166.607664	47.951911
1967.753828	157.080877	47.956916
1963.948869	169.238301	47.961921
1960.253612	151.489765	47.966925
1956.748054	158.854491	47.971930
1953.781942	158.381003	47.976935
1950.061965	160.545341	47.981940
1946.057873	158.870994	47.986945
1942.873075	158.034217	47.991949
1939.328257	162.322210	47.996954
1935.747100	159.300444	48.001959
1932.805413	155.081382	48.006964
1928.657509	157.583809	48.011969
1925.447405	152.661367	48.016973
1922.067507	159.794603	48.021978
1918.306096	158.454747	48.026983
1914.934676	149.338069	48.031988
1911.204190	162.051559	48.036993
1907.494065	161.925166	48.041997
1904.299259	156.095016	48.047002
1901.174600	155.685638	48.052007
1898.028307	151.816729	48.057012
1893.850880	153.353548	48.062017
1890.259454	155.955116	48.067021
1886.898452	155.733776	48.072026
1883.257587	155.056436	48.077031
1880.014505	154.772406	48.082036
1876.236122	157.973202	48.087041
1872.991970	156.066831	48.092045
1869.374878	154.333955	48.097050
1865.624163	157.837052	48.102055
1862.398442	153.997272	48.107060
1858.800117	168.391613	48.112065
1855.214415	145.308375	48.117069
1852.020676	158.968480	48.122074
1848.446306	151.742734	48.127079
1845.190039	157.059811	48.132084
1841.034152	149.185766	48.137089
1837.618421	152.223872	48.142093
1834.342510	156.061592	48.147098
1830.867590	146.103853	48.152103
1827.641391	150.684830	48.157108
1823.830961	157.499501	48.162113
1820.555338	154.524841	48.167117
1816.633686	155.776748	48.172122
1813.380203	154.894571	48.177127
1810.074293	150.491255	48.182132
1805.900290	147.123513	48.187137
1802.732082	147.196587	48.192141
1799.386675	149.258114	48.197146
1795.869038	154.905723	48.202151
1792.735704	151.739446	48.207156
1789.073022	151.923813	48.212161
1785.498624	149.049055	48.217165
1781.642247	148.134279	48.222170
1778.141244	140.372148	48.227175
1775.054470	146.506665	48.232180
1771.204425	151.824589	48.237185
1768.127463	150.653980	48.242189
1764.198032	152.308799	48.247194
1760.593890	151.826379	48.252199
1757.338469	158.030212	48.257204
1753.717206	153.819144	48.262209
1750.447853	154.373300	48.267213
1747.069713	145.926059	48.272218
1743.278246	149.550238	48.277223
1740.091936	144.894752	48.282228
1735.974694	150.415308	48.287233
1732.542379	150.010494	48.292237
1729.154380	150.953092	48.297242
1725.766849	144.765568	48.302247
1722.453536	143.703303	48.307252
1718.776062	146.912806	48.312257
1715.666352	146.942922	48.317261
1711.560315	149.648979	48.322266
1707.870073	147.589485	48.327271
1704.599442	142.788309	48.332276
1701.229993	153.937772	48.337281
1697.614759	145.242615	48.342285
1694.165628	149.349007	48.347290
1690.609659	147.841598	48.352295
1687.609336	135.889615	48.357300
1683.918220	142.441943	48.362305
1680.682924	142.845082	48.367309
1676.875787	152.034876	48.372314
1673.110428	155.368655	48.377319
1669.666564	148.003292	48.382324
1666.176680	143.061357	48.387329
1663.146522	138.316390	48.392333
1659.396044	147.072555	48.397338
1655.557479	148.021172	48.402343
1652.290625	148.557222	48.407348
1648.175938	145.503659	48.412353
1645.033928	144.569240	48.417357
1641.592468	146.180436	48.422362
1638.106917	144.298725	48.427367
1634.985956	138.385144	48.432372
1631.274391	145.280904	48.437377
1627.878553	137.466199	48.442381
1624.368452	138.874241	48.447386
1620.424524	135.658103	48.452391
1617.128648	134.400234	48.457396
1613.665504	141.366257	48.462401
1610.358912	142.904474	48.467405
1606.779633	137.211885	48.472410
1602.974273	138.226691	48.477415
1599.764347	136.009974	48.482420
1595.511434	138.496091	48.487425
1592.719120	133.422970	48.492429
1589.278460	131.977103	48.497434
1585.516407	142.739991	48.502439
1582.330297	138.419077	48.507444
1579.061020	145.184958	48.512449
1575.446611	143.959229	48.517453
1571.330098	142.038168	48.522458
1567.966450	146.517107	48.527463
1564.535317	140.172930	48.532468
1560.950532	147.053712	48.537473
1557.921567	137.961257	48.542477
1554.183453	138.018951	48.547482
1550.590806	135.441431	48.552487
1547.357360	142.983265	48.557492
1543.655606	143.607635	48.562497
1540.217491	139.594802	48.567501
1536.452177	126.294450	48.572506
1532.900486	137.827353	48.577511
1530.126456	130.770174	48.582516
1526.114446	145.693251	48.587521
1522.551875	137.353045	48.592525
1519.199374	137.030317	48.597530
1515.562195	132.428589	48.602535
1511.946034	128.524928	48.607540
1508.542700	132.475281	48.612545
1505.224231	130.860492	48.617549
1501.475815	138.869105	48.622554
1498.009143	132.808118	48.627559
1494.713256	131.151124	48.632564
1491.117776	138.401162	48.637569
1487.642415	130.377119	48.642573
1483.659775	132.034646	48.647578
1480.479640	143.875995	48.652583
1477.448575	136.142819	48.657588
1473.550951	134.522728	48.662593
1470.085486	134.776973	48.667597
1466.795145	139.223340	48.672602
1463.260305	137.484693	48.677607
1459.683354	132.711833	48.682612
1455.720376	137.693450	48.687617
1452.500561	135.967475	48.692621
1448.963467	136.416112	48.697626
1445.745651	134.946943	48.702631
1442.322368	131.341017	48.707636
1438.461323	138.555849	48.712641
1434.830850	133.346463	48.717645
1431.431131	133.133231	48.722650
1428.070732	139.245290	48.727655
1425.030762	130.070494	48.732660
1420.985444	137.173711	48.737665
1417.601395	138.822349	48.742669
1413.675212	134.473899	48.747674
1409.982942	138.406559	48.752679
1407.295526	131.712261	48.757684
1403.682270	132.413088	48.762689
1400.190505	130.096276	48.767693
1396.847274	129.439196	48.772698
1392.919894	144.420604	48.777703
1389.057074	142.237945	48.782708
1385.740756	139.685532	48.787713
1382.671376	128.649603	48.792717
1379.119071	127.609723	48.797722
1375.608613	139.684907	48.802727
1372.322948	133.900373	48.807732
1368.843659	144.279622	48.812737
1365.019735	142.159426	48.817741
1361.801954	132.280956	48.822746
1357.947120	135.838351	48.827751
1354.529313	137.214959	48.832756
1350.138617	142.529029	48.837761
1347.403262	142.522972	48.842765
1344.481790	131.860654	48.847770
1340.602633	141.598362	48.852775
1337.050886	136.382950	48.857780
1333.034381	136.714172	48.862785
1330.195217	132.024305	48.867789
1326.721645	140.690928	48.872794
1322.805821	139.431945	48.877799
1319.317743	134.473615	48.882804
1315.920129	143.796468	48.887809
1312.305035	133.080893	48.892813
1308.806715	137.592922	48.897818
1305.228378	131.927861	48.902823
1302.069104	131.211828	48.907828
1298.435802	137.721923	48.912833
1294.924257	131.534922	48.917837
1291.397175	134.263839	48.922842
1287.933566	144.504386	48.927847
1284.566828	136.353822	48.932852
1280.908032	137.283883	48.937857
1277.355164	141.678460	48.942861
1274.096685	136.862973	48.947866
1270.218636	136.764255	48.952871
1266.972160	133.031162	48.957876
1263.485892	136.153159	48.962881
1259.982969	129.689280	48.967885
1256.581315	135.891942	48.972890
1252.748548	139.692051	48.977895
1249.291616	123.405799	48.982900
1245.616278	130.619084	48.987905
1242.067947	131.774429	48.992909
1238.841829	124.924995	48.997914
1235.235690	131.081355	49.002919
1232.019207	132.026544	49.007924
1228.478441	135.402077	49.012929
1225.173544	128.896610	49.017933
1221.722257	122.889748	49.022938
1217.862801	129.081682	49.027943
1214.327148	120.873268	49.032948
1210.995563	129.458077	49.037953
1207.300166	132.619818	49.042957
1204.047387	124.643681	49.047962
1200.008729	132.895858	49.052967
1196.643131	133.172477	49.057972
1193.496357	128.407261	49.062977
1189.603927	127.168209	49.067981
1186.092605	134.661875	49.072986
1182.582965	132.715040	49.077991
1179.382317	123.007549	49.082996
1175.831712	125.820954	49.088001
1172.586128	124.061752	49.093005
1169.111358	131.934193	49.098010
1165.389170	121.025511	49.103015
1161.836188	120.705802	49.108020
1158.288841	124.099839	49.113025
1154.713265	130.482088	49.118029
1151.563322	127.138652	49.123034
1147.692114	132.365633	49.128039
1144.373696	119.345801	49.133044
1140.466795	127.828042	49.138049
1137.149661	123.199177	49.143053
1133.630819	127.730511	49.148058
1130.279905	133.789890	49.153063
1126.979515	122.574700	49.158068
1123.066878	126.012781	49.163073
1119.890962	123.231930	49.168077
1116.414738	121.998523	49.173082
1112.721674	126.201892	49.178087
1109.234618	127.604338	49.183092
1105.400976	126.591062	49.188097
1101.912907	127.976315	49.193101
1098.953792	122.798889	49.198106
1095.397365	123.438662	49.203111
1091.906325	125.442671	49.208116
1088.357431	121.152316	49.213121
1084.747740	119.694528	49.218125
1080.948596	128.547752	49.223130
1077.799666	132.804247	49.228135
1074.606051	130.173370	49.233140
1070.524246	126.172823	49.238145
1066.991951	121.735092	49.243149
1063.954439	120.398796	49.248154
1060.080240	127.981952	49.253159
1056.898634	120.017650	49.258164
1053.279862	121.795546	49.263169
1049.739378	115.096520	49.268173
1046.287325	122.883982	49.273178
1042.688135	121.438898	49.278183
1039.369407	122.960776	49.283188
1035.520024	127.831595	49.288193
1032.001674	115.619079	49.293197
1028.626807	128.005949	49.298202
1024.932199	124.538364	49.303207
1021.712540	112.828419	49.308212
1018.351514	128.406707	49.313217
1014.951131	124.320962	49.318221
1011.519521	124.818601	49.323226
1007.465057	127.717426	49.328231
1004.362017	123.798604	49.333236
1000.445216	135.551480	49.338241
996.919840	134.079030	49.343245
993.687770	128.690868	49.348250
990.010481	127.644732	49.353255
987.075437	118.155345	49.358260
983.076301	126.048122	49.363265
979.406585	112.658314	49.368269
976.284103	123.277964	49.373274
972.469799	130.421288	49.378279
969.354270	129.085920	49.383284
965.838706	128.386618	49.388289
962.166816	123.334267	49.393293
958.812468	127.610799	49.398298
954.888570	126.580019	49.403303
951.474673	126.988735	49.408308
947.988175	126.166436	49.413313
944.592488	126.817041	49.418317
941.112739	127.059842	49.423322
937.278919	123.798089	49.428327
934.342029	125.343723	49.433332
930.548050	135.832723	49.438337
926.950304	127.980558	49.443341
923.567903	123.732070	49.448346
920.283567	129.537264	49.453351
916.987977	124.858241	49.458356
913.352080	125.519983	49.463361
909.618080	125.961148	49.468365
906.113464	125.737638	49.473370
902.325391	129.641934	49.478375
898.589527	119.130442	49.483380
895.242795	120.604761	49.488385
892.103515	121.991097	49.493389
888.735389	120.093517	49.498394
884.953982	122.012307	49.503399
881.589451	119.693416	49.508404
878.030113	123.415055	49.513409
874.351107	120.354296	49.518413
870.985209	118.807621	49.523418
867.561243	124.249952	49.528423
864.330083	111.762958	49.533428
860.468602	119.226354	49.538433
857.123695	117.910061	49.543437
853.466360	121.374221	49.548442
849.821559	127.640070	49.553447
846.402492	125.318188	49.558452
842.690487	118.671389	49.563457
839.519507	119.414952	49.568461
836.174723	120.122735	49.573466
832.341951	128.049687	49.578471
829.460429	108.880307	49.583476
825.303664	121.330323	49.588481
821.851905	115.646718	49.593485
818.721568	121.038542	49.598490
814.961326	118.214854	49.603495
811.724111	116.051378	49.608500
807.911357	117.088784	49.613505
804.393512	118.470901	49.618509
800.897799	116.764795	49.623514
797.282698	116.921167	49.628519
794.205693	110.388819	49.633524
790.508746	119.197331	49.638529
786.693761	124.635134	49.643533
783.601153	113.134666	49.648538
779.844622	123.965282	49.653543
776.829687	113.088382	49.658548
772.807229	125.827229	49.663553
769.030065	122.691233	49.668557
766.014309	111.895387	49.673562
762.212241	121.037047	49.678567
758.902169	118.566570	49.683572
755.422023	116.312685	49.688577
752.121554	120.829290	49.693581
748.497980	121.868407	49.698586
744.783849	125.759810	49.703591
741.645405	117.598192	49.708596
737.870265	116.908268	49.713601
734.433562	120.548358	49.718605
730.957810	121.360964	49.723610
727.163916	118.789393	49.728615
723.906257	121.824242	49.733620
720.461804	112.914843	49.738625
716.758380	116.245244	49.743629
713.433014	123.009116	49.748634
710.041130	130.702795	49.753639
706.509176	122.429684	49.758644
702.624071	121.856058	49.763649
699.132579	119.242576	49.768653
695.747163	110.016774	49.773658
692.211476	115.057186	49.778663
688.999235	114.108618	49.783668
685.341333	116.850556	49.788673
682.087590	112.083893	49.793677
678.270810	113.877083	49.798682
674.912886	112.374431	49.803687
671.278067	104.969490	49.808692
667.988776	107.627173	49.813697
664.312848	113.486861	49.818701
661.143237	104.861600	49.823706
657.312540	119.775023	49.828711
653.956651	109.065140	49.833716
650.083894	110.801902	49.838721
646.383137	112.833842	49.843725
643.487157	105.800227	49.848730
639.862592	113.521589	49.853735
636.588722	97.720706	49.858740
633.111397	107.238133	49.863745
629.379906	117.415477	49.868749
625.908853	116.685996	49.873754
622.063894	113.810191	49.878759
618.689052	113.605498	49.883764
614.817709	118.556660	49.888769
611.765404	111.546364	49.893773
608.424581	110.447448	49.898778
604.846515	117.604854	49.903783
601.607048	117.060065	49.908788
597.732816	104.678721	49.913793
594.118163	113.253533	49.918797
590.865408	104.927632	49.923802
586.662884	114.009188	49.928807
583.732342	106.502796	49.933812
580.337564	112.943163	49.938817
576.860395	109.177144	49.943821
573.688339	107.956990	49.948826
569.965975	109.442593	49.953831
566.201795	103.230933	49.958836
562.781311	115.637080	49.963841
559.008916	116.178825	49.968845
555.913940	108.466804	49.973850
552.184388	118.854246	49.978855
548.870554	104.566907	49.983860
545.130916	116.522077	49.988865
541.218120	116.080262	49.993869
538.503879	115.544320	49.998874
534.797377	106.960640	50.003879
531.091463	117.480939	50.008884
527.368198	117.226817	50.013889
523.976607	121.791419	50.018893
520.771274	115.725506	50.023898
517.147210	113.901157	50.028903
513.849385	112.433285	50.033908
510.309368	113.608153	50.038913
506.674340	117.029034	50.043917
503.404472	107.955963	50.048922
499.455957	123.002662	50.053927
496.104347	109.798873	50.058932
492.511589	110.196101	50.063937
489.229855	107.169791	50.068941
485.718577	113.631675	50.073946
482.074046	119.096179	50.078951
478.888913	102.508972	50.083956
475.192044	117.796824	50.088961
471.465923	111.516593	50.093965
468.095692	108.766612	50.098970
464.433417	113.962135	50.103975
461.762196	105.980756	50.108980
457.907399	122.246508	50.113985
454.137418	116.503395	50.118989
450.850294	112.817130	50.123994
446.707520	124.773380	50.128999
443.710899	118.299038	50.134004
439.942935	114.776618	50.139009
436.465951	116.285464	50.144013
433.129039	113.100594	50.149018
429.596983	116.571590	50.154023
426.287257	105.392705	50.159028
422.707100	116.125522	50.164033
419.189776	113.453992	50.169037
415.817924	114.065340	50.174042
411.668955	114.096866	50.179047
408.578573	116.238348	50.184052
404.638942	115.495622	50.189057
401.134118	109.817015	50.194061
398.084808	112.150423	50.199066
394.763140	115.981889	50.204071
391.307256	102.434336	50.209076
387.706812	115.379507	50.214081
383.979714	112.644453	50.219085
380.413835	114.282116	50.224090
376.997789	120.235181	50.229095
373.535695	111.674741	50.234100
369.987394	115.669240	50.239105
366.237986	107.930312	50.244109
363.542803	109.743959	50.249114
359.852302	113.034228	50.254119
356.757672	103.807762	50.259124
352.758700	118.883837	50.264129
348.914813	115.897399	50.269133
345.708195	106.945025	50.274138
341.798680	121.346217	50.279143
338.356415	105.269577	50.284148
334.873558	113.981425	50.289153
331.201760	111.959118	50.294157
328.411486	111.246057	50.299162
324.410061	112.146387	50.304167
320.829514	107.466469	50.309172
317.322739	112.616637	50.314177
314.087581	114.507456	50.319181
310.852788	99.291227	50.324186
306.983668	108.428939	50.329191
303.485214	117.084784	50.334196
299.780272	113.479836	50.339201
296.325304	116.329791	50.344205
293.120192	119.230154	50.349210
289.282626	107.090317	50.354215
286.143132	117.517041	50.359220
282.554061	112.238470	50.364225
278.759484	117.742376	50.369229
275.354365	110.357987	50.374234
271.607637	120.097278	50.379239
268.510693	113.270661	50.384244
265.048587	114.769090	50.389249
261.457636	110.129623	50.394253
258.312367	102.713094	50.399258
254.208872	113.691712	50.404263
250.985037	104.710695	50.409268
247.444370	108.173193	50.414273
243.768885	103.534715	50.419277
240.683419	96.880869	50.424282
236.991161	116.916199	50.429287
233.581604	99.917039	50.434292
229.948130	105.671370	50.439297
226.213285	112.668530	50.444301
222.922056	99.252146	50.449306
219.134037	108.339009	50.454311
215.661817	109.396134	50.459316
212.543548	98.343026	50.464321
209.113799	109.001364	50.469325
205.636520	106.995906	50.474330
201.648195	109.187908	50.479335
198.269846	103.241481	50.484340
194.928301	101.137785	50.489345
191.542581	108.321080	50.494349
187.689815	102.996859	50.499354
184.136403	108.721792	50.504359
180.877741	104.293594	50.509364
177.316481	107.570510	50.514369
174.015646	103.422214	50.519373
170.341062	101.731442	50.524378
166.661606	106.104791	50.529383
163.799817	98.507024	50.534388
159.883853	113.284351	50.539393
156.330795	103.837548	50.544397
152.995371	109.375850	50.549402
149.082998	105.813867	50.554407
145.878461	117.140440	50.559412
142.114353	105.216320	50.564417
138.703387	114.181033	50.569421
135.639294	104.408403	50.574426
132.050303	107.960493	50.579431
128.552156	104.937741	50.584436
124.785048	107.575080	50.589441
121.322437	104.178816	50.594445
117.641748	105.465896	50.599450
114.176214	103.361087	50.604455
110.592272	93.232723	50.609460
107.131965	107.727442	50.614465
103.540616	108.728209	50.619469
100.438055	98.730705	50.624474
96.640486	120.168263	50.629479
93.304765	106.026062	50.634484
90.006417	105.055104	50.639489
86.296778	104.555797	50.644493
82.665355	99.803216	50.649498
78.739253	112.622158	50.654503
75.719098	110.006738	50.659508
72.330129	110.354391	50.664513
68.615924	110.963890	50.669517
65.364100	101.285354	50.674522
61.646344	109.744433	50.679527
58.597957	103.057359	50.684532
54.957574	110.862097	50.689537
51.369095	112.060755	50.694541
47.910675	101.384974	50.699546
44.061274	101.486840	50.704551
40.751690	111.319090	50.709556
37.215397	118.283330	50.714561
33.451436	116.182614	50.719565
30.264293	108.283023	50.724570
26.573908	112.868854	50.729575
23.138303	108.342013	50.734580
19.684876	105.676229	50.739585
16.203456	107.182199	50.744589
12.712516	95.418212	50.749594
9.035379	107.034073	50.754599
5.862302	109.836787	50.759604
2.528565	103.708500	50.764609