Tue Jun 21 13:24:26 2022

Number of Points = 9929

Depth (nm)	Load (N)	Time (s)
0.484991	76.301751	0.000000
0.289440	75.925703	0.005005
0.884745	67.052526	0.010010
0.339347	69.594173	0.015014
0.054484	58.852963	0.020019
0.117948	48.774740	0.025024
-0.697880	33.592869	0.030029
-0.870544	19.946712	0.035034
-1.291343	20.289752	0.040038
-1.390365	16.789328	0.045043
-1.263646	14.382044	0.050048
-2.145741	8.881680	0.055053
-2.665734	9.686133	0.060058
-3.208401	16.093863	0.065062
-3.326356	15.084946	0.070067
-3.450559	13.957678	0.075072
-3.783623	14.279480	0.080077
-3.499980	12.757099	0.085082
-3.446071	20.348902	0.090086
-4.424535	11.044521	0.095091
-4.522784	22.350663	0.100096
-4.846955	20.064024	0.105101
-4.716526	14.588188	0.110106
-4.987909	15.384228	0.115110
-5.765098	11.980323	0.120115
-5.956445	8.121640	0.125120
-6.369976	15.041179	0.130125
-5.976946	11.984771	0.135130
-6.541948	14.232671	0.140134
-6.627625	9.046986	0.145139
-7.175287	9.305067	0.150144
-7.391106	15.372144	0.155149
-7.521079	10.851110	0.160154
-7.779340	11.900327	0.165158
-7.993753	9.129019	0.170163
-8.269649	19.327939	0.175168
-8.914931	18.310641	0.180173
-9.401134	12.036489	0.185178
-9.458789	9.439317	0.190182
-9.431264	10.042989	0.195187
-9.570183	13.968108	0.200192
-9.840001	27.100961	0.205197
-9.249125	12.106088	0.210202
-10.011894	14.996300	0.215206
-10.991959	17.758908	0.220211
-11.251969	17.952384	0.225216
-11.261783	20.499656	0.230221
-11.123143	19.186978	0.235226
-11.063266	18.371993	0.240230
-11.726599	22.039808	0.245235
-12.174099	16.556274	0.250240
-12.750843	26.404039	0.255245
-12.695136	9.863084	0.260250
-12.716153	17.565761	0.265254
-12.947752	18.800398	0.270259
-12.893250	20.058498	0.275264
-13.767041	19.957964	0.280269
-13.744821	19.333524	0.285274
-13.896720	16.736370	0.290278
-14.429845	26.949870	0.295283
-14.372571	19.214644	0.300288
-14.885963	17.741768	0.305293
-15.252155	23.889201	0.310298
-15.739843	23.725320	0.315302
-15.657799	21.267220	0.320307
-15.871083	26.384117	0.325312
-16.027347	28.804881	0.330317
-15.630179	21.361660	0.335322
-16.315555	15.328481	0.340326
-16.976541	22.180075	0.345331
-17.005530	16.085358	0.350336
-17.398471	20.600737	0.355341
-17.575286	14.868533	0.360346
-18.240780	24.405591	0.365350
-18.693235	18.469012	0.370355
-18.586739	15.697051	0.375360
-19.046764	25.386366	0.380365
-18.880508	15.444669	0.385370
-19.022493	25.304894	0.390374
-19.041669	26.066669	0.395379
-19.021232	23.350003	0.400384
-19.767105	23.387732	0.405389
-20.118982	9.138419	0.410394
-20.229993	22.543534	0.415398
-20.668193	18.017105	0.420403
-20.399902	21.504001	0.425408
-21.067191	21.638434	0.430413
-21.744097	15.901826	0.435418
-22.291517	27.368589	0.440422
-22.476024	22.757720	0.445427
-22.242818	21.260266	0.450432
-22.476134	25.436439	0.455437
-22.109468	15.308818	0.460442
-22.131657	20.635800	0.465446
-22.666302	22.969843	0.470451
-22.814646	23.303878	0.475456
-23.665173	29.560332	0.480461
-23.822181	21.937748	0.485466
-24.719100	28.217079	0.490470
-24.783713	20.199526	0.495475
-25.157380	17.580095	0.500480
-24.945995	21.986712	0.505485
-24.649155	20.859179	0.510490
-24.904518	15.320346	0.515494
-25.459476	32.472344	0.520499
-25.591526	14.510501	0.525504
-26.647422	11.559855	0.530509
-26.580640	14.967443	0.535514
-26.816841	20.648559	0.540518
-27.189696	22.235543	0.545523
-26.945411	18.316161	0.550528
-27.289481	18.455084	0.555533
-27.127851	11.677604	0.560538
-28.219787	11.280298	0.565542
-28.575245	21.649866	0.570547
-28.361276	12.552158	0.575552
-28.508257	11.787217	0.580557
-28.709971	12.494564	0.585562
-28.413507	17.037260	0.590566
-28.805824	16.812990	0.595571
-29.355864	20.464018	0.600576
-30.165704	14.954456	0.605581
-30.317588	16.188521	0.610586
-30.563630	15.067025	0.615590
-30.628238	13.754459	0.620595
-31.294670	17.122843	0.625600
-31.759874	20.974915	0.630605
-31.502908	8.692631	0.635610
-31.724439	13.239216	0.640614
-31.743404	13.683249	0.645619
-31.707326	10.265831	0.650624
-31.826970	7.053381	0.655629
-32.767392	3.288165	0.660634
-33.404369	10.911693	0.665638
-33.655351	17.920544	0.670643
-33.079790	13.867369	0.675648
-33.448045	15.852599	0.680653
-33.792385	8.115612	0.685658
-33.693689	15.869896	0.690662
-34.596253	17.684315	0.695667
-34.600792	8.089010	0.700672
-35.022664	23.600236	0.705677
-34.981776	12.573646	0.710682
-34.947649	18.499481	0.715686
-35.891197	30.675746	0.720691
-35.894762	16.731643	0.725696
-36.591201	17.683720	0.730701
-36.839170	4.483595	0.735706
-36.462645	7.800221	0.740710
-36.643489	20.980888	0.745715
-36.540924	9.773590	0.750720
-37.664528	14.649138	0.755725
-37.791397	13.446931	0.760730
-38.059739	15.466527	0.765734
-38.029390	15.615865	0.770739
-37.674942	12.772453	0.775744
-39.013344	21.462897	0.780749
-38.792374	5.890325	0.785754
-39.119464	15.792446	0.790758
-39.763854	16.478384	0.795763
-39.050510	12.846192	0.800768
-39.616612	22.358897	0.805773
-40.029183	6.547687	0.810778
-40.710656	11.998845	0.815782
-41.139525	11.623158	0.820787
-40.795149	7.740088	0.825792
-41.178392	10.101548	0.830797
-41.203943	6.471943	0.835802
-41.669194	19.699116	0.840806
-41.850003	19.099617	0.845811
-42.231205	14.858569	0.850816
-42.888211	17.429351	0.855821
-42.722284	17.214851	0.860826
-42.868702	16.893421	0.865830
-43.069330	28.437927	0.870835
-43.109066	16.277195	0.875840
-44.324795	18.028631	0.880845
-44.432027	7.843930	0.885850
-44.631232	15.957361	0.890854
-44.480945	18.038065	0.895859
-44.491729	12.157009	0.900864
-44.766406	20.595911	0.905869
-44.459069	19.800526	0.910874
-45.069755	14.806374	0.915878
-46.015019	23.278584	0.920883
-46.014883	11.393637	0.925888
-46.109918	18.501179	0.930893
-46.007900	14.184053	0.935898
-46.514852	12.042538	0.940902
-47.392817	11.822921	0.945907
-47.241648	12.562601	0.950912
-47.651656	16.213133	0.955917
-47.465910	1.933011	0.960922
-47.604498	7.320309	0.965926
-47.878229	15.292556	0.970931
-48.532709	1.611765	0.975936
-48.926792	14.036631	0.980941
-49.126949	4.118132	0.985946
-49.182676	9.800732	0.990950
-49.187916	8.935161	0.995955
-49.355003	0.971690	1.000960
-50.477756	8.518984	1.005965
-50.495416	7.628633	1.010970
-50.669048	4.793349	1.015974
-50.784938	14.757974	1.020979
-50.284288	-0.762833	1.025984
-50.816934	-1.004512	1.030989
-51.165695	14.301998	1.035994
-51.753585	3.229182	1.040998
-52.190766	10.698854	1.046003
-52.123812	9.679445	1.051008
-52.693550	16.461464	1.056013
-52.215946	7.105993	1.061018
-52.966769	6.561626	1.066022
-53.582843	10.416582	1.071027
-53.989013	3.483119	1.076032
-53.915663	8.101437	1.081037
-54.060713	7.319207	1.086042
-53.827598	7.491007	1.091046
-53.799928	4.349671	1.096051
-54.175582	11.544729	1.101056
-55.305507	4.777106	1.106061
-55.232709	13.104192	1.111066
-55.478335	7.255913	1.116070
-55.470739	3.549781	1.121075
-55.667804	8.760679	1.126080
-56.743795	11.630744	1.131085
-56.887112	11.419111	1.136090
-57.199930	6.139032	1.141094
-57.410869	6.503167	1.146099
-57.232169	-2.865745	1.151104
-57.488686	14.179776	1.156109
-57.310180	11.171917	1.161114
-57.322205	10.366670	1.166118
-58.283077	15.764252	1.171123
-58.411577	6.519224	1.176128
-58.749824	10.707442	1.181133
-58.833099	1.285221	1.186138
-58.605240	6.856523	1.191142
-59.414249	8.603948	1.196147
-60.368781	5.692371	1.201152
-60.538633	12.794146	1.206157
-60.664347	11.784937	1.211162
-60.341632	7.127765	1.216166
-60.378239	10.992328	1.221171
-60.476626	7.222446	1.226176
-60.604119	15.935336	1.231181
-61.403058	14.257960	1.236186
-61.556097	8.981019	1.241190
-61.827396	17.134608	1.246195
-62.074527	8.791896	1.251200
-62.486227	6.756758	1.256205
-63.151868	7.838714	1.261210
-63.471313	9.742256	1.266214
-63.671806	13.772686	1.271219
-63.293694	4.055406	1.276224
-63.558509	11.650848	1.281229
-63.521094	13.222970	1.286234
-63.754310	11.584709	1.291238
-64.582210	19.638080	1.296243
-64.925613	14.412595	1.301248
-65.422022	10.754806	1.306253
-65.372401	6.926668	1.311258
-65.312916	8.273727	1.316262
-65.671185	13.757794	1.321267
-65.615777	10.423213	1.326272
-66.329231	11.792511	1.331277
-66.873965	14.935518	1.336282
-66.903002	5.415512	1.341286
-66.829125	15.294047	1.346291
-66.601011	8.964555	1.351296
-67.258243	12.021210	1.356301
-67.888260	2.908971	1.361306
-67.895820	8.114927	1.366310
-68.461974	9.547052	1.371315
-68.378297	15.753770	1.376320
-68.438333	8.494807	1.381325
-69.230028	3.881302	1.386330
-69.761616	11.389896	1.391334
-70.157121	8.157818	1.396339
-69.537594	6.282427	1.401344
-70.332487	13.229409	1.406349
-70.383820	10.028538	1.411354
-70.330850	13.260021	1.416358
-70.373661	16.307668	1.421363
-70.240303	17.816541	1.426368
-70.908591	14.652331	1.431373
-71.572812	5.970219	1.436378
-71.549615	8.964111	1.441382
-71.851661	8.480202	1.446387
-72.547697	2.341654	1.451392
-73.123023	11.946457	1.456397
-73.243099	4.963445	1.461402
-73.300420	9.879472	1.466406
-73.559073	19.338692	1.471411
-73.213071	12.572513	1.476416
-73.583300	16.404122	1.481421
-73.419943	11.096093	1.486426
-73.515764	11.753345	1.491430
-74.844808	12.442961	1.496435
-74.662566	5.343181	1.501440
-75.001350	13.588259	1.506445
-75.202967	13.915134	1.511450
-75.334180	12.950447	1.516454
-76.311375	12.260451	1.521459
-76.421480	6.141289	1.526464
-76.565703	12.756143	1.531469
-76.811813	4.176269	1.536474
-76.482944	5.796025	1.541478
-76.755706	13.327071	1.546483
-76.535885	6.769455	1.551488
-77.352172	9.775889	1.556493
-78.017950	16.584077	1.561498
-77.962495	9.978498	1.566502
-78.289562	11.338270	1.571507
-78.169305	10.972479	1.576512
-78.571795	8.454719	1.581517
-79.107642	6.493226	1.586522
-79.435272	5.834376	1.591526
-79.844392	18.796310	1.596531
-79.546643	1.455952	1.601536
-79.976179	13.098738	1.606541
-79.862252	8.269734	1.611546
-80.317543	5.287713	1.616550
-80.860581	15.828054	1.621555
-80.854071	3.547001	1.626560
-81.207245	13.495471	1.631565
-81.147044	13.109829	1.636570
-81.749762	15.404634	1.641574
-82.573860	9.528633	1.646579
-82.283741	4.379975	1.651584
-83.029719	11.387726	1.656589
-82.988225	11.564818	1.661594
-83.090577	9.990329	1.666598
-83.327627	18.673413	1.671603
-83.143220	8.599861	1.676608
-83.703320	14.348629	1.681613
-84.213573	12.592859	1.686618
-84.493234	10.797716	1.691622
-84.457889	18.693517	1.696627
-84.255397	17.620086	1.701632
-84.696789	13.714217	1.706637
-85.277087	10.159124	1.711642
-85.598952	4.615530	1.716646
-86.104490	13.286443	1.721651
-85.868063	5.817360	1.726656
-86.593325	10.200705	1.731661
-86.094377	13.065484	1.736666
-86.467390	6.149819	1.741670
-87.343497	20.993705	1.746675
-87.509335	16.945901	1.751680
-87.793999	17.950161	1.756685
-87.878393	18.548886	1.761690
-87.894755	9.630422	1.766694
-88.022905	20.645903	1.771699
-88.131803	6.003338	1.776704
-88.711125	12.483250	1.781709
-89.391758	6.102789	1.786714
-89.499398	3.607436	1.791718
-89.790920	15.007734	1.796723
-89.643185	5.245532	1.801728
-89.570706	9.563454	1.806733
-90.584693	12.375306	1.811738
-90.804901	14.074751	1.816742
-91.284770	16.446299	1.821747
-90.913981	9.428955	1.826752
-91.195832	2.986593	1.831757
-91.225296	5.298540	1.836762
-91.023791	-2.274472	1.841766
-92.061794	12.033426	1.846771
-92.265494	-0.738502	1.851776
-92.469607	3.719553	1.856781
-92.483116	9.957163	1.861786
-93.027857	1.422411	1.866790
-93.730479	16.891127	1.871795
-93.722107	11.368613	1.876800
-93.862117	7.151564	1.881805
-94.104823	14.208375	1.886810
-94.048748	7.933622	1.891814
-94.312738	13.393392	1.896819
-94.971666	2.580005	1.901824
-95.369548	10.702854	1.906829
-96.087171	1.338733	1.911834
-95.864598	-0.167025	1.916838
-95.564118	18.545270	1.921843
-95.936085	9.437655	1.926848
-95.934106	13.283395	1.931853
-96.145757	15.439630	1.936858
-96.749160	7.357604	1.941862
-97.512382	11.533330	1.946867
-97.190344	10.350905	1.951872
-97.314560	14.457305	1.956877
-97.715737	9.701575	1.961882
-97.633008	17.001869	1.966886
-98.408623	4.198762	1.971891
-98.917484	2.315485	1.976896
-99.236894	13.527804	1.981901
-99.237839	4.560813	1.986906
-98.974534	9.345592	1.991910
-99.383443	18.864230	1.996915
-99.679206	5.202782	2.006912
-99.504349	7.176252	2.016909
-99.149269	7.514888	2.026906
-98.894380	8.438372	2.036902
-98.159544	6.949476	2.046899
-97.476533	14.288985	2.056896
-96.577211	12.002657	2.066893
-96.283091	11.039619	2.076890
-96.760885	9.179747	2.086886
-95.674679	15.638822	2.096883
-95.052165	9.790429	2.106880
-94.531608	2.085813	2.116877
-93.700399	9.027537	2.126874
-93.650796	3.844066	2.136870
-93.156116	9.455069	2.146867
-92.269320	0.605844	2.156864
-91.701233	4.344619	2.166861
-91.988964	6.394506	2.176858
-90.673177	1.079376	2.186854
-90.549095	6.782581	2.196851
-90.351172	4.515999	2.206848
-89.537079	2.253274	2.216845
-88.914791	4.774443	2.226842
-88.435280	7.172256	2.236838
-87.792572	6.577677	2.246835
-87.282603	6.634787	2.256832
-87.281255	0.390964	2.266829
-86.527084	1.973692	2.276826
-86.154907	4.267766	2.286822
-85.724925	3.068045	2.296819
-84.591472	2.315527	2.306816
-84.167956	2.605881	2.316813
-84.511878	4.405051	2.326810
-83.312402	2.748711	2.336806
-82.567437	4.239111	2.346803
-82.528097	6.936850	2.356800
-82.517704	-0.544171	2.366797
-81.531328	3.518920	2.376794
-81.033067	2.480383	2.386790
-80.416742	6.729636	2.396787
-79.976648	3.340376	2.406784
-79.514978	2.432971	2.416781
-78.655493	6.295191	2.426778
-78.417441	9.434818	2.436774
-78.283517	4.395252	2.446771
-77.404757	3.363248	2.456768
-76.840527	0.551719	2.466765
-76.562369	1.123404	2.476762
-76.138125	3.538076	2.486758
-75.438776	-0.309048	2.496755
-75.103413	-5.511985	2.506752
-74.207514	-1.791538	2.516749
-73.744925	-1.509038	2.526746
-73.614268	6.402281	2.536742
-73.345608	-2.289638	2.546739
-72.063075	7.506153	2.556736
-72.025484	2.305702	2.566733
-71.416826	0.635183	2.576730
-70.810959	0.319771	2.586726
-70.187413	1.679130	2.596723
-70.179101	2.789271	2.606720
-69.639612	3.926239	2.616717
-68.955462	5.240589	2.626714
-68.706802	5.439574	2.636710
-67.808099	7.519402	2.646707
-67.463101	6.608005	2.656704
-67.128845	4.706311	2.666701
-66.232803	6.674155	2.676698
-66.136432	10.584319	2.686694
-65.240705	6.322145	2.696691
-64.627858	4.099076	2.706688
-64.351748	7.163839	2.716685
-64.345316	8.564348	2.726682
-63.600135	7.296225	2.736678
-62.787541	3.343606	2.746675
-62.548388	5.808693	2.756672
-61.566692	14.899935	2.766669
-61.322057	5.223468	2.776666
-61.065763	5.064943	2.786662
-60.745637	7.322393	2.796659
-59.890610	12.327994	2.806656
-59.399893	10.983463	2.816653
-58.636273	10.591542	2.826650
-58.265482	8.361535	2.836646
-57.725124	3.443748	2.846643
-57.842651	12.621797	2.856640
-57.306472	-1.312114	2.866637
-56.613881	8.713966	2.876634
-55.301101	2.296025	2.886630
-55.126347	4.176255	2.896627
-54.822432	3.191641	2.906624
-54.952088	4.840922	2.916621
-53.782429	8.066136	2.926618
-53.511355	11.754130	2.936614
-53.085572	5.529913	2.946611
-52.236573	5.016566	2.956608
-51.868780	7.990076	2.966605
-51.642252	4.983345	2.976602
-51.067273	7.762895	2.986598
-50.411919	13.165716	2.996595
-49.437428	6.417914	3.006592
-49.096976	10.851962	3.016589
-49.206436	10.677939	3.026586
-48.561576	11.524594	3.036582
-47.578890	11.565267	3.046579
-47.392705	14.046439	3.056576
-47.082372	9.115965	3.066573
-46.452659	9.579640	3.076570
-45.803585	12.692300	3.086566
-45.567066	7.991790	3.096563
-44.511535	9.300755	3.106560
-44.020976	6.664634	3.116557
-44.122515	9.835016	3.126554
-43.755593	9.357642	3.136550
-42.690245	8.922869	3.146547
-42.321677	7.875584	3.156544
-41.908914	2.232648	3.166541
-41.116040	7.846637	3.176538
-40.723199	5.846723	3.186534
-40.760471	13.981866	3.196531
-40.061822	11.094334	3.206528
-39.207254	11.837107	3.216525
-39.127875	8.254677	3.226522
-38.084240	12.296839	3.236518
-37.905107	14.285018	3.246515
-37.654758	13.913295	3.256512
-36.525631	10.289599	3.266509
-36.209448	15.073838	3.276506
-36.360292	17.783121	3.286502
-35.036252	20.127231	3.296499
-34.679688	10.107591	3.306496
-34.665895	15.709726	3.316493
-33.721754	18.943054	3.326490
-33.258062	15.803191	3.336486
-32.978133	16.039086	3.346483
-32.355259	11.913189	3.356480
-31.984796	15.064879	3.366477
-31.533286	9.600859	3.376474
-30.803984	14.380109	3.386470
-29.916651	7.128872	3.396467
-30.134679	8.315225	3.406464
-29.534902	8.175295	3.416461
-28.410223	11.053103	3.426458
-28.324466	15.405250	3.436454
-28.065715	10.639411	3.446451
-26.889221	17.544129	3.456448
-26.572634	15.987581	3.466445
-26.735479	19.914398	3.476442
-26.282530	15.809134	3.486438
-25.332951	11.194248	3.496435
-24.710764	10.071374	3.506432
-23.793695	12.506790	3.516429
-23.402957	10.555239	3.526426
-23.513664	12.245642	3.536422
-23.342191	19.786065	3.546419
-22.272551	14.961021	3.556416
-21.943048	13.359062	3.566413
-21.325611	14.971561	3.576410
-20.784955	20.334506	3.586406
-20.123498	10.913443	3.596403
-20.097090	9.237200	3.606400
-19.194864	13.409680	3.616397
-19.114705	18.255139	3.626394
-18.411935	11.818683	3.636390
-17.409493	22.812617	3.646387
-17.026105	20.186737	3.656384
-17.132669	13.992585	3.666381
-16.446546	21.596169	3.676378
-15.982318	17.076477	3.686374
-14.872814	17.175191	3.696371
-14.675688	14.648521	3.706368
-14.059428	10.409123	3.716365
-14.279159	15.103891	3.726362
-13.265705	15.848810	3.736358
-12.793386	13.157819	3.746355
-12.447884	11.971501	3.756352
-11.669595	7.267421	3.766349
-10.750232	10.173900	3.776346
-10.841217	10.438618	3.786342
-10.852005	8.824253	3.796339
-10.288086	6.179741	3.806336
-8.896197	2.955724	3.816333
-8.515183	6.514867	3.826330
-8.509693	15.422407	3.836326
-7.590148	17.439721	3.846323
-7.401347	8.027185	3.856320
-6.695120	5.382818	3.866317
-6.375393	5.842706	3.876314
-5.846175	8.136667	3.886310
-5.222851	12.754460	3.896307
-4.875561	10.483496	3.906304
-4.372406	9.408394	3.916301
-3.528331	15.445245	3.926298
-3.413353	21.926680	3.936294
-3.168452	19.009770	3.946291
-2.697537	30.964275	3.956288
-2.165247	41.416258	3.966285
-1.774387	53.110973	3.976282
-1.259848	70.948728	3.986278
-0.806608	93.376715	3.996275
-0.420622	107.983721	4.006272
0.000000	136.400685	4.011277
-0.193213	139.192654	4.016282
0.034797	151.045154	4.021286
0.452838	159.954123	4.026291
0.583789	177.654558	4.031296
0.523076	176.492096	4.036301
0.726063	196.547462	4.041306
1.170831	201.704432	4.046310
1.091990	194.460725	4.051315
0.999483	210.161700	4.056320
0.900369	202.964760	4.061325
0.928380	210.501546	4.066330
0.857307	207.143664	4.071334
1.003060	207.848535	4.076339
0.683572	205.799276	4.081344
1.052440	203.593402	4.086349
1.108969	203.704071	4.091354
1.156282	203.401072	4.096358
1.261932	203.845786	4.101363
0.717188	206.033721	4.106368
1.306353	202.630048	4.111373
1.050603	208.480429	4.116378
0.974554	201.161663	4.121382
1.063841	199.880033	4.126387
1.061611	204.675310	4.131392
1.314202	201.331122	4.136397
1.001579	206.131821	4.141402
0.952216	213.011665	4.146406
1.300395	197.744619	4.151411
1.237237	200.604257	4.156416
1.130607	201.601538	4.161421
1.497139	220.187921	4.166426
1.114189	211.096591	4.171430
1.589696	210.895352	4.176435
1.808850	206.138647	4.181440
1.729843	197.548742	4.186445
1.603801	211.981867	4.191450
1.400601	209.136835	4.196454
1.591146	196.288390	4.201459
1.358803	203.732916	4.206464
1.626905	209.156736	4.211469
1.420179	195.679853	4.216474
1.572044	205.654138	4.221478
1.562642	198.311707	4.226483
1.188699	203.689110	4.231488
1.503927	199.689854	4.236493
1.372037	209.886364	4.241498
1.148546	206.793682	4.246502
1.367407	199.285183	4.251507
1.214561	203.851431	4.256512
1.177601	204.079801	4.261517
1.679644	201.051876	4.266522
1.440604	200.113516	4.271526
1.533224	201.771041	4.276531
1.158277	205.154535	4.281536
1.397747	219.454914	4.286541
1.547414	221.898455	4.291546
1.275869	233.468673	4.296550
1.908409	226.328558	4.301555
1.486689	236.044418	4.306560
1.786230	236.004929	4.311565
1.497265	232.755151	4.316570
1.305474	241.376797	4.321574
1.704058	233.445624	4.326579
1.498187	234.327323	4.331584
1.717610	240.664593	4.336589
1.822833	236.325364	4.341594
1.634990	241.840289	4.346598
1.517045	236.018134	4.351603
1.897211	243.214233	4.356608
1.848317	238.519074	4.361613
1.751792	243.692484	4.366618
1.571239	249.345130	4.371622
1.960627	242.887799	4.376627
1.704961	244.136107	4.381632
1.908232	241.079111	4.386637
2.144795	245.408611	4.391642
1.664469	247.754410	4.396646
1.970326	236.868090	4.401651
1.423421	249.995119	4.406656
1.796050	241.134248	4.411661
1.965092	238.182180	4.416666
1.785197	246.671618	4.421670
2.101254	235.347103	4.426675
2.074223	243.215073	4.431680
2.016770	236.471997	4.436685
2.016481	241.840423	4.441690
1.902115	242.096609	4.446694
2.430463	232.443306	4.451699
2.410956	245.844317	4.456704
1.741165	243.561597	4.461709
1.877390	234.743036	4.466714
1.819169	242.262741	4.471718
1.999594	243.151315	4.476723
1.944353	245.837771	4.481728
2.178896	252.588921	4.486733
2.026102	240.461727	4.491738
1.695187	245.818600	4.496742
2.102963	240.894091	4.501747
2.002953	252.625755	4.506752
2.071587	262.830534	4.511757
2.205951	268.332566	4.516762
2.470369	271.033383	4.521766
2.528922	245.074816	4.526771
2.100374	255.547813	4.531776
2.181227	241.488881	4.536781
2.022779	240.484681	4.541786
2.120558	239.756748	4.546790
2.111194	248.650902	4.551795
2.375745	266.165920	4.556800
2.374339	265.557815	4.561805
2.375752	268.028282	4.566810
2.080567	271.006080	4.571814
2.315978	272.927091	4.576819
2.301226	279.122791	4.581824
2.088305	279.183359	4.586829
2.363357	283.023811	4.591834
2.207956	279.639226	4.596838
2.328349	271.485724	4.601843
2.295383	283.552634	4.606848
2.251463	280.587675	4.611853
2.432036	277.417607	4.616858
2.377534	281.219884	4.621862
2.214501	277.577855	4.626867
2.496586	285.139698	4.631872
2.393894	277.612579	4.636877
2.438912	285.900017	4.641882
1.894339	279.516228	4.646886
2.298843	272.521008	4.651891
2.160197	280.171860	4.656896
2.379982	283.725855	4.661901
2.544810	281.090018	4.666906
2.385228	298.415811	4.671910
2.715870	296.625925	4.676915
2.857886	297.882384	4.681920
2.650371	273.458116	4.686925
2.658987	276.834349	4.691930
2.415834	272.860250	4.696934
2.668854	279.412397	4.701939
2.436658	289.188075	4.706944
2.616879	304.124888	4.711949
2.709281	308.030521	4.716954
2.587415	314.218121	4.721958
2.708735	305.298583	4.726963
2.700270	304.524502	4.731968
2.906848	311.156578	4.736973
3.112032	306.162786	4.741978
2.734394	301.477054	4.746982
2.807062	287.998816	4.751987
2.611822	284.911504	4.756992
2.412482	286.439586	4.761997
2.450873	296.779243	4.767002
2.558091	303.156827	4.772006
2.841793	305.393478	4.777011
2.924201	310.384343	4.782016
2.730930	308.786396	4.787021
3.015384	309.246694	4.792026
2.695094	317.352116	4.797030
3.035313	315.429216	4.802035
2.974786	311.746524	4.807040
2.962044	309.784195	4.812045
2.788393	313.283960	4.817050
2.522087	312.439896	4.822054
2.647276	308.840905	4.827059
2.559827	319.751789	4.832064
2.356519	310.677026	4.837069
2.870828	323.895181	4.842074
3.010484	336.715594	4.847078
3.276144	339.773003	4.852083
3.069695	333.859497	4.857088
2.814328	322.512327	4.862093
3.021050	328.605855	4.867098
3.046398	339.859398	4.872102
3.345782	334.951429	4.877107
3.028348	325.310451	4.882112
3.029737	330.692246	4.887117
3.006766	325.698538	4.892122
3.110838	344.190792	4.897126
3.396775	344.001014	4.902131
2.994024	328.483448	4.907136
3.208431	331.561578	4.912141
3.054557	326.819247	4.917146
3.313350	336.128051	4.922150
3.286117	321.297399	4.927155
3.010280	323.393064	4.932160
3.381124	335.452938	4.937165
3.259080	324.017779	4.942170
3.057901	327.372129	4.947174
3.504524	333.561502	4.952179
3.393920	332.270733	4.957184
2.994343	315.778401	4.962189
3.461883	327.974995	4.967194
3.208935	331.491842	4.972198
3.268267	317.771088	4.977203
3.197536	333.383333	4.982208
3.467641	341.847440	4.987213
3.469929	339.796185	4.992218
3.220938	348.498601	4.997222
3.276119	340.429863	5.002227
3.361478	344.462771	5.007232
3.499851	347.087187	5.012237
3.210171	341.082083	5.017242
3.112065	348.330396	5.022246
3.218208	354.420856	5.027251
3.045677	348.874104	5.032256
3.191418	349.280017	5.037261
3.097172	345.887263	5.042266
2.918569	352.097298	5.047270
3.504151	345.507781	5.052275
3.415448	366.944685	5.057280
3.505312	369.904126	5.062285
3.668219	369.860622	5.067290
3.354923	385.259903	5.072294
3.510439	380.440865	5.077299
3.242547	381.358694	5.082304
3.383841	374.126599	5.087309
3.746624	377.314554	5.092314
3.312855	373.009288	5.097318
3.911116	379.801300	5.102323
3.695315	381.666605	5.107328
3.444649	378.209958	5.112333
4.044612	376.033281	5.117338
3.316976	380.234573	5.122342
3.699899	376.230377	5.127347
3.755447	377.508660	5.132352
3.574627	376.532625	5.137357
3.637087	382.674139	5.142362
3.300746	383.788801	5.147366
3.754900	379.207633	5.152371
3.487824	381.125830	5.157376
3.625811	372.195600	5.162381
3.753954	381.054035	5.167386
3.453113	388.444278	5.172390
3.777387	394.708205	5.177395
3.758134	405.486888	5.182400
4.055955	403.587772	5.187405
3.893961	399.326098	5.192410
3.752612	403.722171	5.197414
3.865591	409.040718	5.202419
4.040742	415.366447	5.207424
3.977903	399.212741	5.212429
4.053145	393.654937	5.217434
3.763425	394.098429	5.222438
3.900172	390.241559	5.227443
3.900929	411.596023	5.232448
4.277127	415.548029	5.237453
4.325748	391.538391	5.242458
3.893542	393.170167	5.247462
3.877674	376.774664	5.252467
3.649417	381.857452	5.257472
3.979560	399.037533	5.262477
4.222938	402.949172	5.267482
4.149151	410.731036	5.272486
3.925112	387.697401	5.277491
3.817831	395.108875	5.282496
3.956377	414.404393	5.287501
4.333030	411.595320	5.292506
4.250667	414.797994	5.297510
3.912798	410.238254	5.302515
3.913179	416.827561	5.307520
3.959488	421.561585	5.312525
4.191825	414.727227	5.317530
4.025360	417.240515	5.322534
3.921191	410.670272	5.327539
4.139436	422.630766	5.332544
4.246288	411.991983	5.337549
4.004834	416.302613	5.342554
3.904016	421.269194	5.347558
4.138236	408.066816	5.352563
4.098476	420.842810	5.357568
3.733668	419.079865	5.362573
3.840838	428.406927	5.367578
4.340319	440.775333	5.372582
4.468255	434.932909	5.377587
4.250796	447.935691	5.382592
4.033088	437.674075	5.387597
4.478000	434.957889	5.392602
4.161346	445.218697	5.397606
4.459628	438.469709	5.402611
4.264627	438.849959	5.407616
4.165194	441.399314	5.412621
4.302719	445.309548	5.417626
4.140634	445.660272	5.422630
4.426092	436.295120	5.427635
4.070247	442.996708	5.432640
4.218269	450.170764	5.437645
4.822567	440.791883	5.442650
4.469900	449.065934	5.447654
4.875107	438.777929	5.452659
4.634528	436.011467	5.457664
4.666826	443.123972	5.462669
4.684225	445.653784	5.467674
4.737454	451.406123	5.472678
4.659809	438.194978	5.477683
4.892678	440.138731	5.482688
4.404112	446.331064	5.487693
4.433415	441.367932	5.492698
4.180682	450.626731	5.497702
4.569775	440.152540	5.502707
4.605994	446.435575	5.507712
4.384393	443.030342	5.512717
4.552994	443.306373	5.517722
4.448464	447.827000	5.522726
4.627469	456.621603	5.527731
4.663004	460.748437	5.532736
4.728108	467.676731	5.537741
4.813896	476.174000	5.542746
4.711867	475.946245	5.547750
4.962024	465.434462	5.552755
4.837068	462.564585	5.557760
4.530845	447.753372	5.562765
4.504545	460.902705	5.567770
4.575607	471.584188	5.572774
4.942014	469.923143	5.577779
4.832909	475.944706	5.582784
4.562609	484.981862	5.587789
4.850375	477.552792	5.592794
4.851278	476.321100	5.597798
5.000989	475.826296	5.602803
4.079685	472.176388	5.607808
4.384288	473.101442	5.612813
4.761286	475.841670	5.617818
4.566014	475.036156	5.622822
5.076598	481.127576	5.627827
5.032706	485.467473	5.632832
4.613021	484.738785	5.637837
5.262932	501.459509	5.642842
5.166446	505.293066	5.647846
5.129501	497.829744	5.652851
4.951467	485.600961	5.657856
4.983471	483.574367	5.662861
5.178083	478.308166	5.667866
5.216891	481.947431	5.672870
4.831250	472.447900	5.677875
5.073193	486.204645	5.682880
5.144437	498.207696	5.687885
5.303140	488.563153	5.692890
4.863264	499.254867	5.697894
4.928452	484.650101	5.702899
4.899426	497.136462	5.707904
4.985808	508.568480	5.712909
5.226592	507.787056	5.717914
4.731266	520.066090	5.722918
5.186746	513.482063	5.727923
4.987109	518.969833	5.732928
5.185707	514.692815	5.737933
5.134761	504.479910	5.742938
5.129581	513.423647	5.747942
5.141837	509.369894	5.752947
4.996525	511.781025	5.757952
4.954929	513.281428	5.762957
5.162439	503.488090	5.767962
4.887076	515.084607	5.772966
5.430499	525.736648	5.777971
5.351945	537.863995	5.782976
5.486221	539.670359	5.787981
5.509338	541.203858	5.792986
5.245367	539.371906	5.797990
5.227898	533.708830	5.802995
5.423572	544.406236	5.808000
5.501962	543.984614	5.813005
5.726686	540.062224	5.818010
5.245191	532.021478	5.823014
5.459272	531.442603	5.828019
5.612347	539.270833	5.833024
5.520833	533.654553	5.838029
5.467170	511.263278	5.843034
4.993765	525.471824	5.848038
5.768786	535.705839	5.853043
5.703849	535.827547	5.858048
5.449876	544.726659	5.863053
5.494647	546.678880	5.868058
5.287903	554.308780	5.873062
5.403661	543.914712	5.878067
5.746350	548.481687	5.883072
5.507323	550.389141	5.888077
5.525893	552.422664	5.893082
5.507872	546.956817	5.898086
5.691239	539.241300	5.903091
5.465147	541.358357	5.908096
5.496470	549.629259	5.913101
5.765109	536.038431	5.918106
5.728973	542.364271	5.923110
5.701774	534.510953	5.928115
5.758980	547.655214	5.933120
5.568674	548.588622	5.938125
6.065603	547.579674	5.943130
5.690052	545.154247	5.948134
5.449938	541.681016	5.953139
5.511866	542.239149	5.958144
5.750817	542.958796	5.963149
5.723664	542.702657	5.968154
5.646856	542.598995	5.973158
5.585508	540.799204	5.978163
5.876900	545.130365	5.983168
5.695314	543.715168	5.988173
5.710726	542.866473	5.993178
5.728352	552.081745	5.998182
5.710147	553.283452	6.003187
5.884620	575.337362	6.008192
5.962953	579.476480	6.013197
6.073926	573.137739	6.018202
5.830691	565.446675	6.023206
6.066348	566.045899	6.028211
5.834196	562.967011	6.033216
5.767228	553.066748	6.038221
6.117708	556.692505	6.043226
5.963322	569.657513	6.048230
5.908694	554.158837	6.053235
5.755304	555.071134	6.058240
5.726804	553.661765	6.063245
6.153750	558.045275	6.068250
5.815254	561.459120	6.073254
6.105260	560.543047	6.078259
6.110311	548.555436	6.083264
5.649688	555.534517	6.088269
5.633462	545.751364	6.093274
5.470525	562.087558	6.098278
5.972122	567.424294	6.103283
6.218877	582.199589	6.108288
5.954856	583.955485	6.113293
6.176979	572.792115	6.118298
5.688259	566.111432	6.123302
5.763356	564.289438	6.128307
5.914524	576.923038	6.133312
5.858903	581.781147	6.138317
5.850298	585.051564	6.143322
5.759566	591.030661	6.148326
5.746229	586.455017	6.153331
5.982479	583.599108	6.158336
5.670700	579.759039	6.163341
6.091296	578.109731	6.168346
5.974534	576.879360	6.173350
6.103737	581.899862	6.178355
5.978957	573.967762	6.183360
5.806690	578.240733	6.188365
6.154031	585.983732	6.193370
5.827161	589.354414	6.198374
5.771862	583.500441	6.203379
5.892944	582.932821	6.208384
5.872712	584.650517	6.213389
6.176895	583.660658	6.218394
5.807252	587.939083	6.223398
5.676896	580.787792	6.228403
6.101715	579.450174	6.233408
5.959490	590.282503	6.238413
6.232883	580.032809	6.243418
5.887663	571.907510	6.248422
5.758503	558.791228	6.253427
5.714204	563.108324	6.258432
5.710519	577.774516	6.263437
6.024706	576.004296	6.268442
5.727623	582.487822	6.273446
6.130322	586.868054	6.278451
5.919680	582.189511	6.283456
5.881013	589.474667	6.288461
5.876780	581.329997	6.293466
5.839969	582.927298	6.298470
5.934901	576.293031	6.303475
5.822285	593.701757	6.308480
5.761886	585.350298	6.313485
6.421650	579.801407	6.318490
5.883204	588.716472	6.323494
5.845175	577.143481	6.328499
5.989984	573.215174	6.333504
5.921674	580.364530	6.338509
5.643385	562.204650	6.343514
5.620845	570.615122	6.348518
5.931403	572.106550	6.353523
5.996698	582.261969	6.358528
5.914494	585.221528	6.363533
6.228097	572.835286	6.368538
6.000056	584.615241	6.373542
5.930567	574.061988	6.378547
5.625836	571.365920	6.383552
6.073541	576.885835	6.388557
5.951489	589.102716	6.393562
5.851206	591.339649	6.398566
6.118423	589.169698	6.403571
5.837277	577.895086	6.408576
5.759606	576.543785	6.413581
5.681675	574.948023	6.418586
5.441004	582.861410	6.423590
5.756342	586.694478	6.428595
6.384214	580.903205	6.433600
5.728120	587.557484	6.438605
5.817582	574.514115	6.443610
5.758202	579.954407	6.448614
6.014733	578.320033	6.453619
5.794303	589.750622	6.458624
5.963633	590.523242	6.463629
6.108899	583.984241	6.468634
6.048476	588.450242	6.473638
5.875272	580.403017	6.478643
5.698169	586.252356	6.483648
5.948620	581.370174	6.488653
6.053332	579.405924	6.493658
6.000230	580.766944	6.498662
5.938020	578.992747	6.503667
5.720256	579.995234	6.508672
5.610812	588.765254	6.513677
5.752974	581.178101	6.518682
5.506687	581.625852	6.523686
5.683792	582.119328	6.528691
5.830506	593.514777	6.533696
5.777919	578.758528	6.538701
6.057857	577.441744	6.543706
6.023912	584.281508	6.548710
5.826227	586.171859	6.553715
5.598565	584.597733	6.558720
5.468447	587.311250	6.563725
5.840129	581.815984	6.568730
5.594360	587.548423	6.573734
5.605199	596.503961	6.578739
5.983703	608.148957	6.583744
5.911121	619.534759	6.588749
6.002379	614.632750	6.593754
5.967098	618.385749	6.598758
6.148011	607.678918	6.603763
6.283638	601.687350	6.608768
6.048347	592.501483	6.613773
5.987832	584.966046	6.618778
5.786522	586.595916	6.623782
5.550971	582.918659	6.628787
5.904718	578.716970	6.633792
6.019233	588.738536	6.638797
5.672713	575.234939	6.643802
5.836017	586.095605	6.648806
5.982300	586.643127	6.653811
6.044057	581.072294	6.658816
5.910560	585.069674	6.663821
5.783747	575.107673	6.668826
5.593341	592.487049	6.673830
5.904659	604.328272	6.678835
6.215782	617.744317	6.683840
5.874559	603.882828	6.688845
5.890134	583.616590	6.693850
5.665408	590.374873	6.698854
5.960403	601.069289	6.703859
6.126276	605.801331	6.708864
5.956371	602.023606	6.713869
6.164788	587.342927	6.718874
5.797364	599.761676	6.723878
6.076026	587.917383	6.728883
5.995104	584.463168	6.733888
5.917818	579.013834	6.738893
6.106179	580.346116	6.743898
6.145607	584.004246	6.748902
5.726201	584.126241	6.753907
5.993166	583.934472	6.758912
6.177728	589.105457	6.763917
5.946002	573.880593	6.768922
5.792759	591.821759	6.773926
5.973080	580.733191	6.778931
5.944367	581.882965	6.783936
6.108267	588.325480	6.788941
6.217624	585.075577	6.793946
5.805607	585.504989	6.798950
5.967096	582.820714	6.803955
6.126085	577.855008	6.808960
6.223654	584.477429	6.813965
6.558524	591.309206	6.818970
5.640620	572.907912	6.823974
5.735064	566.373979	6.828979
6.206633	573.117791	6.833984
5.723327	567.818579	6.838989
5.815476	563.483792	6.843994
5.819091	582.426917	6.848998
5.880078	579.299285	6.854003
5.912432	580.895591	6.859008
5.957891	585.959760	6.864013
6.071203	575.759865	6.869018
5.861099	583.046568	6.874022
5.832357	582.642094	6.879027
6.034321	585.088478	6.884032
5.948381	584.125136	6.889037
6.084101	573.839437	6.894042
5.681180	568.152954	6.899046
5.704730	575.101991	6.904051
6.124599	577.748703	6.909056
5.702831	571.865039	6.914061
5.717075	579.176160	6.919066
5.713974	579.859126	6.924070
5.860930	584.178893	6.929075
6.079512	582.852733	6.934080
6.048308	576.593382	6.939085
6.114776	583.372313	6.944090
5.720711	583.439198	6.949094
6.089472	585.246206	6.954099
6.012388	582.365616	6.959104
5.792747	583.335853	6.964109
6.147230	567.158451	6.969114
6.062207	568.958114	6.974118
5.811563	556.518304	6.979123
5.867785	548.788710	6.984128
5.725394	549.010864	6.989133
6.090258	557.998925	6.994138
5.561290	559.903678	6.999142
6.225502	569.339077	7.004147
5.752803	563.304992	7.009152
5.742364	563.285063	7.014157
6.447923	575.253386	7.019162
5.861842	561.131342	7.024166
5.990121	564.357183	7.029171
5.802900	547.196173	7.034176
5.728293	561.011325	7.039181
5.761047	552.737997	7.044186
5.828922	581.348033	7.049190
5.757941	575.930020	7.054195
5.627318	582.603252	7.059200
5.489165	584.710883	7.064205
6.169590	578.847168	7.069210
5.795554	585.307917	7.074214
5.845332	588.620963	7.079219
5.928899	579.077806	7.084224
6.069815	580.408473	7.089229
5.972399	578.940261	7.094234
6.039972	581.809697	7.099238
6.048216	583.514587	7.104243
6.201947	576.290797	7.109248
5.947281	587.836381	7.114253
6.150862	566.107131	7.119258
5.913059	564.242228	7.124262
5.911880	546.676846	7.129267
5.688977	555.145749	7.134272
5.788292	554.331310	7.139277
5.981380	568.307766	7.144282
5.997226	579.580818	7.149286
5.620767	579.490467	7.154291
5.890372	570.826050	7.159296
5.767215	581.203700	7.164301
6.221856	584.201841	7.169306
5.929627	577.259305	7.174310
5.988991	577.869173	7.179315
5.860338	562.707175	7.184320
5.693880	576.070249	7.189325
6.357287	572.988299	7.194330
5.668043	568.845661	7.199334
5.700043	554.684419	7.204339
5.896700	575.075618	7.209344
6.090193	581.730699	7.214349
5.936957	565.795444	7.219354
5.836673	571.868076	7.224358
5.732848	578.834063	7.229363
5.824724	577.149400	7.234368
5.663291	587.692055	7.239373
5.830112	587.152578	7.244378
6.018496	588.129447	7.249382
5.932186	583.253301	7.254387
6.275977	575.608291	7.259392
6.034196	578.812336	7.264397
6.119515	575.560101	7.269402
5.882007	563.025163	7.274406
5.840845	554.282960	7.279411
6.155613	552.909694	7.284416
5.965059	560.609340	7.289421
6.077846	539.062901	7.294426
5.513392	553.838707	7.299430
5.536069	545.815897	7.304435
6.029897	567.716071	7.309440
5.820585	568.690516	7.314445
5.930217	573.969811	7.319450
5.768564	584.525919	7.324454
5.659924	586.325548	7.329459
5.995675	585.430118	7.334464
5.882911	578.782290	7.339469
6.243815	579.075420	7.344474
6.081081	587.115620	7.349478
5.891217	570.764710	7.354483
5.906437	562.857978	7.359488
5.605831	567.330594	7.364493
5.647613	562.309707	7.369498
6.059445	580.010070	7.374502
5.852232	580.999955	7.379507
6.144637	581.881057	7.384512
5.887237	588.621661	7.389517
6.240990	574.828441	7.394522
5.820867	564.535335	7.399526
5.901020	551.857816	7.404531
5.700176	548.629491	7.409536
5.649249	562.349749	7.414541
6.056487	575.826409	7.419546
6.350870	570.516422	7.424550
5.791010	567.786627	7.429555
5.688889	553.959591	7.434560
5.562349	575.212220	7.439565
6.122775	565.537416	7.444570
6.121971	578.715780	7.449574
5.801318	573.943763	7.454579
5.816453	570.639410	7.459584
5.845821	579.316580	7.464589
5.858649	581.423284	7.469594
6.140287	582.643226	7.474598
6.084163	572.607161	7.479603
6.012718	570.769373	7.484608
5.782503	561.241878	7.489613
6.017413	550.831232	7.494618
5.206775	562.248238	7.499622
5.676273	566.056167	7.504627
5.667014	577.028089	7.509632
5.679117	584.706620	7.514637
5.894895	578.363349	7.519642
5.936546	581.529931	7.524646
5.800300	582.344864	7.529651
6.023782	584.456943	7.534656
5.623856	583.179726	7.539661
6.138413	581.340211	7.544666
5.944813	587.903103	7.549670
5.766791	577.892351	7.554675
6.033554	578.007874	7.559680
6.018839	581.270620	7.564685
5.952993	577.019616	7.569690
6.036855	581.725961	7.574694
5.856915	582.289219	7.579699
5.845464	577.411532	7.584704
5.908315	584.879582	7.589709
6.122870	578.153082	7.594714
5.946432	582.674604	7.599718
6.024319	586.848924	7.604723
6.202316	576.088132	7.609728
5.928935	583.400312	7.614733
6.235946	576.847751	7.619738
6.432074	560.979564	7.624742
5.774580	555.377670	7.629747
5.937890	555.684970	7.634752
5.941544	553.163200	7.639757
6.155353	545.649845	7.644762
6.135778	544.455086	7.649766
5.719622	554.669098	7.654771
5.866774	549.745421	7.659776
5.719509	551.601370	7.664781
5.953126	549.539604	7.669786
5.896730	552.696565	7.674790
6.048257	555.521112	7.679795
6.043667	555.585071	7.684800
5.842357	555.937753	7.689805
6.249486	546.257166	7.694810
5.781501	554.167529	7.699814
5.805556	552.364250	7.704819
6.220185	554.643985	7.709824
5.823539	558.620405	7.714829
6.095554	554.930935	7.719834
5.693044	560.124927	7.724838
5.665043	554.764137	7.729843
5.737511	550.854722	7.734848
5.711859	564.299848	7.739853
5.935620	557.362454	7.744858
5.883242	557.307042	7.749862
5.855396	559.698729	7.754867
5.834341	552.758660	7.759872
5.817478	560.235952	7.764877
5.843265	555.168382	7.769882
5.759350	563.598091	7.774886
5.670889	560.703603	7.779891
5.950079	565.950475	7.784896
5.781002	584.880759	7.789901
6.099700	575.317415	7.794906
5.999855	570.820631	7.799910
5.908081	561.762969	7.804915
5.812757	561.599225	7.809920
5.556096	573.291752	7.814925
5.970120	576.486657	7.819930
6.079311	576.683134	7.824934
6.010646	584.051598	7.829939
5.855986	574.107036	7.834944
5.962397	580.113671	7.839949
6.355309	570.886938	7.844954
6.210106	566.742419	7.849958
5.938573	553.362391	7.854963
5.972267	550.693562	7.859968
5.856473	557.901093	7.864973
6.043682	547.239043	7.869978
5.664389	557.194160	7.874982
5.886672	553.773414	7.879987
5.758927	549.696263	7.884992
5.580230	556.043743	7.889997
5.714558	555.215810	7.895002
5.812243	551.119088	7.900006
5.972310	567.842459	7.905011
6.039432	561.490856	7.910016
5.469741	559.281103	7.915021
6.066454	571.942351	7.920026
6.248255	576.504007	7.925030
5.924836	571.450647	7.930035
5.754577	559.901539	7.935040
5.733510	560.648457	7.940045
6.004521	563.591160	7.945050
6.084542	562.297024	7.950054
6.059550	564.836835	7.955059
6.160071	553.887799	7.960064
5.791903	558.167748	7.965069
5.917240	552.430695	7.970074
5.977706	557.760752	7.975078
5.903663	553.469276	7.980083
6.058506	540.407411	7.985088
5.822261	564.618753	7.990093
5.772570	549.628205	7.995098
5.895665	558.470014	8.000102
5.685669	558.884718	8.005107
6.028364	554.496800	8.010112
5.893374	557.041921	8.015130
5.898399	559.447861	8.020147
5.664483	554.852326	8.025165
5.760552	560.168770	8.030182
6.058064	571.621706	8.035200
5.629760	572.827446	8.040218
5.796145	582.185912	8.045235
6.279880	581.725962	8.050253
6.217618	586.970610	8.055270
5.949108	569.140960	8.060288
5.824019	569.511897	8.065306
5.946734	557.719612	8.070323
5.800200	559.990621	8.075341
5.991500	578.128992	8.080358
5.899366	573.184405	8.085376
5.837825	581.798778	8.090394
6.038976	586.922646	8.095411
6.329055	582.868831	8.100429
6.181337	578.964478	8.105446
5.871824	568.128543	8.110464
5.419766	569.634455	8.115482
5.822856	581.416151	8.120499
5.949602	589.967068	8.125517
6.000359	590.960022	8.130534
6.222410	588.319345	8.135552
5.832477	594.166645	8.140570
5.948434	590.702451	8.145587
6.068475	584.554694	8.150605
6.322778	589.772903	8.155622
6.239040	586.128408	8.160640
5.721195	595.528933	8.165658
5.946472	587.043039	8.170675
6.127468	590.518193	8.175693
5.703824	598.047932	8.180710
5.850431	594.034407	8.185728
5.838348	592.404088	8.190746
5.989363	592.866499	8.195763
5.803245	591.375623	8.200781
5.768107	588.349021	8.205798
6.151386	581.389419	8.210816
6.015626	587.731597	8.215834
5.840747	584.190772	8.220851
6.134245	599.812612	8.225869
6.527391	612.323488	8.230886
6.571743	602.944183	8.235904
6.001277	595.192379	8.240922
6.028511	591.354320	8.245939
6.115284	589.724363	8.250957
5.882172	590.601935	8.255974
6.089569	594.228219	8.260992
5.790941	596.537411	8.266010
6.104614	607.086970	8.271027
6.381039	623.720453	8.276045
6.054360	625.508738	8.281062
6.547105	618.725861	8.286080
6.064089	627.937383	8.291098
6.156086	619.347566	8.296115
6.235029	617.469116	8.301133
6.387923	628.468514	8.306150
6.296606	612.725672	8.311168
6.242050	600.558996	8.316186
6.130160	590.811110	8.321203
6.309665	594.951624	8.326221
6.167607	602.869548	8.331238
6.576415	599.934771	8.336256
6.365355	600.541780	8.341274
6.205986	597.083417	8.346291
6.033352	589.822785	8.351309
5.918305	589.000606	8.356326
6.342257	606.460960	8.361344
6.289258	621.890218	8.366362
6.131006	618.013977	8.371379
6.439315	625.536488	8.376397
6.217475	630.686718	8.381414
6.524323	618.753469	8.386432
6.417048	613.804487	8.391450
6.240137	601.231329	8.396467
6.437087	589.775719	8.401485
5.880843	593.938078	8.406502
6.123683	608.238288	8.411520
6.351767	620.357831	8.416538
6.325188	621.888756	8.421555
6.737562	618.970707	8.426573
6.428162	615.928103	8.431590
6.533567	608.056891	8.436608
6.471456	600.006743	8.441626
6.169659	592.137817	8.446643
6.399882	587.312864	8.451661
6.371332	587.370788	8.456678
6.317249	586.277507	8.461696
6.317928	588.257428	8.466714
6.292512	595.993642	8.471731
6.147228	605.611200	8.476749
6.001890	613.717455	8.481766
6.705307	630.000727	8.486784
6.654180	620.286655	8.491802
6.565367	619.551462	8.496819
6.372263	615.261335	8.501837
5.759486	610.750173	8.506854
6.686096	618.698210	8.511872
6.614627	624.825834	8.516890
6.429277	620.258849	8.521907
6.184977	617.692440	8.526925
5.953545	625.584430	8.531942
6.312903	618.541180	8.536960
6.521234	626.490063	8.541978
6.355370	626.180004	8.546995
6.524716	615.757028	8.552013
6.329990	626.035301	8.557030
6.520631	623.183101	8.562048
6.735333	618.611873	8.567066
6.353106	631.902499	8.572083
6.678216	627.992074	8.577101
6.251679	629.704579	8.582119
6.486432	618.653684	8.587136
6.326303	626.225620	8.592154
6.169245	628.824935	8.597171
6.414332	620.281415	8.602189
6.490547	625.405710	8.607207
6.570915	619.140305	8.612224
6.651109	630.344841	8.617242
6.223657	619.104216	8.622259
6.662056	621.368128	8.627277
6.369560	619.802154	8.632295
6.752358	614.849768	8.637312
6.941956	620.589496	8.642330
6.654455	618.465842	8.647347
6.958350	621.842113	8.652365
6.594430	628.109696	8.657383
6.936800	615.894601	8.662400
6.953532	627.967856	8.667418
6.542952	626.854478	8.672435
6.820982	627.672997	8.677453
6.561139	625.390639	8.682471
6.815005	618.525084	8.687488
6.690857	621.612419	8.692506
6.460036	627.622937	8.697523
6.960208	624.248841	8.702541
6.631759	629.992278	8.707559
6.940539	625.967440	8.712576
6.763869	626.094377	8.717594
6.182116	634.805752	8.722611
6.805776	617.372955	8.727629
6.489317	627.257636	8.732647
6.700197	624.015102	8.737664
6.371971	624.323032	8.742682
6.341604	619.483154	8.747699
6.715550	626.985349	8.752717
6.577091	630.405349	8.757735
6.673347	616.319520	8.762752
6.528831	626.046798	8.767770
6.745803	633.014987	8.772787
6.830277	624.032148	8.777805
6.695563	630.382044	8.782823
6.670372	631.084842	8.787840
6.881338	621.657857	8.792858
6.751402	632.879280	8.797875
6.990068	621.317138	8.802893
6.628116	633.525739	8.807911
6.755057	617.243042	8.812928
6.870182	619.821100	8.817946
6.706608	623.050782	8.822963
6.801386	626.181190	8.827981
6.851262	619.587785	8.832999
6.925523	626.079440	8.838016
7.196924	620.370746	8.843034
6.688125	627.853187	8.848051
6.627691	625.547255	8.853069
6.804639	625.597132	8.858087
6.505109	622.897161	8.863104
6.899184	620.934835	8.868122
6.197924	629.706348	8.873139
6.435969	625.139126	8.878157
6.564397	625.725152	8.883175
6.287567	641.852083	8.888192
6.825963	653.541353	8.893210
6.766378	654.730329	8.898227
6.974602	650.732765	8.903245
6.819417	660.691344	8.908263
6.547573	653.010525	8.913280
7.026990	656.226644	8.918298
6.697920	668.009578	8.923315
6.998817	658.401351	8.928333
6.943884	660.508789	8.933351
6.740171	659.543424	8.938368
7.059537	651.271428	8.943386
6.813667	658.092075	8.948403
6.683115	653.675445	8.953421
6.643592	659.521825	8.958439
6.830400	664.390236	8.963456
7.570215	659.629880	8.968474
6.972095	661.904823	8.973491
7.280736	659.365732	8.978509
6.984097	658.976744	8.983527
6.808945	663.815336	8.988544
7.103185	662.062832	8.993562
6.772143	666.635920	8.998579
7.301621	662.202108	9.003597
7.012854	660.401669	9.008615
7.153678	659.096591	9.013632
7.258805	647.185111	9.018650
7.098983	661.300884	9.023667
7.286623	661.404105	9.028685
7.243203	655.947126	9.033703
6.892327	657.745721	9.038720
6.910915	662.864021	9.043738
6.929397	667.506780	9.048755
6.907907	659.416413	9.053773
7.029386	662.563075	9.058791
6.890145	657.606577	9.063808
7.431248	662.648587	9.068826
7.015102	668.691188	9.073843
7.243051	666.357966	9.078861
6.901584	667.284585	9.083879
6.917908	667.548057	9.088896
7.269213	658.686553	9.093914
6.957882	659.843600	9.098931
7.074548	662.636357	9.103949
7.178996	661.314075	9.108967
6.852393	668.720501	9.113984
6.687071	659.939430	9.119002
6.476266	670.677650	9.124019
6.973395	681.156528	9.129037
7.593900	686.036193	9.134055
7.265023	689.237754	9.139072
7.203817	676.630612	9.144090
7.321847	672.893239	9.149107
7.268822	658.088438	9.154125
7.204040	667.150217	9.159143
7.122180	659.704846	9.164160
7.350411	659.174614	9.169178
7.481676	665.659995	9.174195
7.291174	667.304876	9.179213
7.084381	665.270797	9.184231
6.985507	667.349688	9.189248
7.304947	659.284355	9.194266
6.873623	671.116112	9.199283
6.927420	666.229607	9.204301
7.223035	673.548746	9.209319
7.052920	695.930307	9.214336
6.879684	694.678414	9.219354
7.043992	700.814658	9.224371
7.285634	697.491429	9.229389
7.487724	694.822742	9.234407
7.439542	695.305151	9.239424
7.603214	686.470372	9.244442
7.508318	694.951363	9.249459
7.712635	693.049583	9.254477
7.318043	680.137432	9.259495
7.001374	675.680360	9.264512
7.107724	685.496833	9.269530
7.193490	693.997511	9.274547
6.962395	693.729155	9.279565
7.434823	701.481991	9.284583
7.142986	695.409875	9.289600
7.261793	699.738411	9.294618
6.926237	704.137858	9.299635
6.931824	696.450050	9.304653
7.158647	684.988045	9.309671
7.412441	697.989754	9.314688
7.185494	690.798695	9.319706
7.015338	705.913009	9.324723
7.030631	717.299999	9.329741
7.396301	722.684446	9.334759
7.635118	734.797381	9.339776
7.567449	722.740058	9.344794
7.229676	734.322133	9.349811
7.435134	727.823580	9.354829
7.721412	737.180789	9.359847
7.388682	734.110924	9.364864
7.717351	726.404637	9.369882
7.234085	736.626243	9.374899
7.509880	728.403938	9.379917
7.773341	722.616999	9.384935
7.671993	733.544211	9.389952
7.517560	719.098251	9.394970
7.534743	721.247296	9.399987
7.409561	712.517418	9.405005
7.851237	708.546138	9.410023
7.123016	709.721046	9.415040
7.688674	714.525556	9.420058
7.451239	729.917160	9.425075
7.743144	717.363709	9.430093
7.552353	712.434234	9.435111
7.103241	708.832499	9.440128
7.557072	716.080184	9.445146
7.502353	732.522966	9.450163
7.512054	727.524066	9.455181
7.455376	732.912319	9.460199
7.335220	734.093615	9.465216
7.554091	723.526154	9.470234
7.456457	732.330828	9.475251
7.323413	726.271379	9.480269
7.561742	728.925111	9.485287
7.393414	733.939356	9.490304
7.502763	726.467407	9.495322
7.557158	734.696153	9.500339
7.410694	736.858127	9.505357
8.119740	729.643935	9.510375
7.591667	739.236386	9.515392
7.750354	726.800651	9.520410
8.105353	723.818072	9.525427
7.759532	727.515724	9.530445
8.082746	719.470206	9.535463
7.810044	722.646725	9.540480
7.825822	719.912828	9.545498
7.732493	727.612917	9.550515
7.956227	723.062011	9.555533
8.129712	727.086242	9.560551
7.747322	721.179891	9.565568
7.454689	705.477771	9.570586
7.755688	710.376103	9.575603
7.491080	720.093407	9.580621
7.506891	722.727296	9.585639
7.513313	728.114940	9.590656
7.803304	721.967724	9.595674
7.522863	727.308782	9.600691
7.457459	730.303738	9.605709
7.738178	719.082768	9.610727
7.809012	729.811790	9.615744
7.656137	728.621085	9.620762
7.762686	729.214479	9.625779
7.458321	728.421674	9.630797
7.430043	734.119772	9.635815
7.420962	734.952773	9.640832
7.729226	750.833526	9.645850
7.874570	757.022143	9.650867
7.891942	757.609046	9.655885
7.837080	753.234968	9.660903
8.384337	769.351739	9.665920
8.224403	749.536886	9.670938
7.951458	734.597968	9.675955
7.479930	733.088793	9.680973
7.879439	734.369851	9.685991
7.779666	742.908760	9.691008
7.956150	742.069396	9.696026
7.781151	746.994204	9.701043
7.822216	754.705513	9.706061
8.328838	754.631904	9.711079
7.933359	751.028363	9.716096
7.808965	738.234008	9.721114
7.848931	747.930813	9.726131
7.684410	770.121408	9.731149
8.023668	777.603044	9.736167
7.854078	768.276192	9.741184
8.502675	770.114790	9.746202
8.261274	750.402398	9.751219
7.721519	737.539826	9.756237
8.232014	733.827600	9.761255
7.796598	737.516077	9.766272
7.934732	732.320328	9.771290
8.311370	741.803512	9.776307
7.730785	741.409183	9.781325
8.020112	734.673129	9.786343
7.929547	749.976657	9.791360
7.870565	761.404718	9.796378
8.110756	764.426630	9.801395
8.172899	769.201945	9.806413
8.281100	760.919979	9.811431
7.891749	761.735643	9.816448
8.054262	762.625265	9.821466
8.111166	766.734162	9.826483
8.065330	771.629715	9.831501
8.254476	763.077666	9.836519
8.389961	777.194640	9.841536
8.088699	752.575505	9.846554
7.919602	752.699221	9.851571
7.636155	761.958674	9.856589
8.178198	758.886063	9.861607
8.217078	769.271604	9.866624
8.156873	772.673952	9.871642
8.169499	771.529850	9.876659
8.007450	772.766116	9.881677
8.175579	764.827354	9.886695
8.153283	766.880586	9.891712
8.181128	762.116846	9.896730
8.289366	771.306719	9.901747
7.945618	768.994929	9.906765
8.709639	763.895907	9.911783
8.673539	765.193594	9.916800
8.507638	759.836777	9.921818
8.262584	750.121274	9.926835
8.080707	741.883418	9.931853
8.005494	747.309782	9.936871
8.156463	753.899411	9.941888
8.260517	757.955225	9.946906
7.984300	768.368930	9.951923
7.923171	766.798090	9.956941
8.253123	756.829893	9.961959
7.951635	762.192163	9.966976
8.108758	769.654353	9.971994
8.193612	772.207923	9.977011
8.305959	772.302748	9.982029
8.196650	762.465945	9.987047
8.270018	773.180405	9.992064
7.933542	766.542064	9.997082
8.165909	763.890791	10.002099
7.901704	771.401493	10.007117
8.012011	781.279966	10.012135
8.158007	799.228078	10.017152
8.171309	802.158836	10.022170
8.636045	792.570637	10.027187
8.572771	801.578704	10.032205
8.380267	791.913525	10.037223
8.494813	801.742493	10.042240
8.441924	797.884189	10.047258
8.675111	788.573693	10.052275
8.434112	803.627003	10.057293
8.468181	802.180151	10.062311
8.531336	799.368321	10.067328
8.562214	799.252240	10.072346
8.561251	794.796000	10.077363
8.238443	804.097033	10.082381
8.422913	804.861375	10.087399
8.711277	801.817772	10.092416
8.486661	807.664940	10.097434
8.823077	800.651784	10.102451
8.537590	788.141924	10.107469
8.535210	776.272162	10.112487
8.399037	769.852211	10.117504
8.267299	776.789829	10.122522
8.706888	788.731378	10.127539
8.598107	798.172547	10.132557
8.417209	794.186631	10.137575
8.312796	795.733415	10.142592
8.628409	808.449798	10.147610
8.662080	795.177671	10.152627
8.734502	799.994992	10.157645
8.603202	799.576651	10.162663
8.643860	801.850159	10.167680
8.523511	806.828531	10.172698
8.654178	799.243574	10.177715
8.351572	801.199930	10.182733
8.530701	795.398585	10.187751
8.603388	800.452070	10.192768
8.436258	807.473905	10.197786
8.366030	797.381016	10.202803
8.366626	803.946358	10.207821
8.737294	802.400855	10.212839
8.705317	801.275947	10.217856
8.485962	802.017795	10.222874
8.832710	806.758196	10.227891
8.480879	809.681314	10.232909
8.355398	806.500348	10.237927
8.221686	805.275364	10.242944
8.063295	807.660964	10.247962
8.390152	813.219184	10.252979
8.525384	831.860417	10.257997
8.467756	836.776841	10.263015
8.963326	835.922032	10.268032
8.859477	830.560820	10.273050
8.824495	832.076033	10.278067
8.932117	828.814731	10.283085
9.068481	831.400724	10.288103
8.943758	840.455996	10.293120
8.773414	836.413600	10.298138
8.898083	829.630367	10.303155
8.740612	831.578440	10.308173
8.641325	829.821403	10.313191
8.765500	839.721632	10.318208
8.913743	830.045275	10.323226
9.179266	832.291393	10.328243
8.578732	838.853150	10.333261
8.766335	836.465958	10.338279
8.544746	828.163769	10.343296
8.684504	838.674376	10.348314
8.951419	830.525925	10.353331
9.044761	833.921757	10.358349
8.682303	832.229952	10.363367
8.793759	839.412745	10.368384
9.012161	834.019821	10.373402
9.051504	832.549653	10.378419
8.944195	841.352448	10.383437
8.854713	836.211679	10.388455
8.980451	835.777149	10.393472
8.715152	843.349875	10.398490
8.815101	834.186605	10.403507
8.902584	835.305967	10.408525
8.882744	839.373264	10.413543
8.807050	836.924953	10.418560
8.815279	838.936922	10.423578
8.972895	831.313237	10.428595
8.907477	834.645993	10.433613
9.153845	838.826285	10.438631
9.052073	842.107980	10.443648
9.020909	834.970255	10.448666
9.068696	840.785317	10.453683
9.142298	844.452516	10.458701
8.897519	838.143823	10.463719
8.983821	827.986019	10.468736
9.063730	845.999850	10.473754
9.335570	852.379358	10.478771
8.890019	844.648472	10.483789
8.981728	847.013922	10.488807
9.211455	857.605701	10.493824
9.249748	869.518889	10.498842
9.363256	847.141434	10.503859
9.168349	838.884818	10.508877
9.001644	846.537276	10.513895
9.221655	833.925562	10.518912
9.124601	838.026510	10.523930
9.363743	842.959142	10.528947
9.014323	839.676283	10.533965
9.140116	839.477165	10.538983
9.243183	836.744147	10.544000
9.413285	838.565145	10.549018
9.415500	827.381556	10.554035
9.493476	833.664426	10.559053
9.267085	832.318967	10.564071
9.099440	829.604403	10.569088
9.264194	841.758818	10.574106
9.435777	826.995398	10.579123
9.066988	830.751993	10.584141
9.159824	837.464664	10.589159
9.176512	827.616404	10.594176
9.016658	823.295517	10.599194
9.342833	832.757982	10.604211
9.286161	830.486827	10.609229
9.100446	836.028760	10.614247
9.414838	846.453764	10.619264
9.489848	854.362247	10.624282
9.397806	844.814250	10.629299
9.343434	836.828443	10.634317
9.273309	840.600540	10.639335
9.223776	836.436174	10.644352
9.628539	856.851214	10.649370
9.132366	843.279404	10.654387
9.278694	851.484327	10.659405
9.123717	854.751607	10.664423
9.477073	852.349562	10.669440
9.449268	860.199093	10.674458
9.449703	858.404674	10.679475
9.543686	861.149257	10.684493
9.301409	860.609142	10.689511
9.384423	859.578174	10.694528
9.118103	871.246938	10.699546
9.469346	868.221255	10.704563
9.649494	863.107871	10.709581
9.595949	861.199168	10.714599
9.974808	859.037768	10.719616
9.564783	860.578477	10.724634
9.604534	863.269839	10.729651
9.447958	859.718440	10.734669
9.272454	868.272320	10.739687
9.190025	859.775425	10.744704
9.206118	862.300635	10.749722
9.583769	871.848689	10.754739
9.606143	856.571787	10.759757
9.450315	864.314181	10.764775
9.674389	864.033830	10.769792
9.544759	868.093726	10.774810
9.631761	867.712065	10.779827
9.762660	862.326929	10.784845
9.489501	871.290663	10.789863
9.716693	859.591473	10.794880
9.444915	866.782625	10.799898
9.707625	869.150074	10.804915
9.685860	863.705576	10.809933
9.689586	861.386229	10.814951
9.611872	865.820972	10.819968
9.508374	866.936925	10.824986
9.630971	866.162774	10.830003
9.708757	872.096496	10.835021
9.719754	868.959055	10.840039
10.106682	867.957283	10.845056
9.792810	869.769851	10.850074
9.782250	864.876620	10.855091
9.748535	862.559142	10.860109
9.675215	869.261155	10.865127
9.861093	867.257295	10.870144
9.623042	868.599850	10.875162
10.133118	868.717391	10.880179
10.251829	871.601969	10.885197
9.903525	872.362418	10.890215
9.847490	866.257880	10.895232
9.700922	866.981378	10.900250
9.816982	877.706162	10.905267
10.009449	868.905879	10.910285
9.946360	866.160609	10.915303
10.052612	869.118900	10.920320
9.632576	859.694102	10.925338
9.906923	858.451931	10.930355
10.029033	867.976555	10.935373
9.917816	865.490423	10.940391
9.945281	846.962064	10.945408
9.696916	849.590905	10.950426
9.878196	867.301769	10.955443
9.674952	863.709279	10.960461
9.594674	868.842839	10.965479
10.126874	863.483763	10.970496
9.946928	861.877867	10.975514
9.996048	869.815447	10.980531
9.930346	865.610447	10.985549
9.658896	872.940123	10.990567
10.064700	865.646170	10.995584
9.699171	865.418182	11.000602
9.754502	869.680509	11.005619
9.661633	870.307718	11.010637
9.693885	879.264187	11.015655
9.929744	873.555776	11.020672
9.821661	873.969767	11.025690
9.754310	877.363480	11.030707
9.672829	882.406696	11.035725
10.097757	900.314640	11.040743
10.057267	899.658041	11.045760
9.849259	897.546970	11.050778
9.990339	908.604624	11.055795
10.273161	902.171137	11.060813
10.040523	904.872576	11.065831
10.343936	902.933102	11.070848
10.272409	911.697730	11.075866
10.088758	899.133123	11.080883
10.111033	902.489953	11.085901
10.157755	905.774629	11.090919
10.652763	902.593643	11.095936
10.447982	907.702559	11.100954
10.236915	890.465950	11.105971
10.249234	877.358304	11.110989
9.692104	878.063575	11.116007
9.816996	884.648917	11.121024
10.160295	896.850184	11.126042
10.000339	904.792090	11.131059
10.141381	896.785309	11.136077
10.142910	912.773713	11.141095
10.292137	903.839632	11.146112
10.182301	910.733922	11.151130
10.289063	906.865294	11.156147
10.295240	903.063715	11.161165
10.192876	904.373568	11.166183
10.339771	905.664978	11.171200
10.341246	904.843957	11.176218
10.227147	902.263026	11.181235
10.500773	898.291182	11.186253
10.449351	909.417326	11.191271
10.364809	902.208098	11.196288
10.454018	904.538145	11.201306
10.135655	911.560663	11.206323
10.399920	909.024550	11.211341
10.208622	912.188413	11.216359
10.523647	906.041310	11.221376
10.461418	904.223012	11.226394
10.386365	906.537743	11.231411
10.602581	900.954222	11.236429
10.277246	903.243079	11.241447
10.523621	897.537248	11.246464
10.588271	900.746910	11.251482
10.401310	910.086925	11.256499
10.351997	908.458211	11.261517
10.199603	918.964892	11.266535
10.753197	904.458990	11.271552
10.548456	919.067453	11.276570
10.173375	912.275212	11.281587
10.510129	907.943716	11.286605
10.391320	914.409986	11.291623
10.445429	909.689487	11.296640
10.698083	909.130794	11.301658
10.457747	906.603048	11.306675
10.602557	901.493141	11.311693
10.405132	910.434514	11.316711
10.578055	902.247656	11.321728
10.734741	896.990121	11.326746
10.296757	904.559978	11.331763
10.586351	909.855913	11.336781
10.357572	930.610596	11.341799
10.335445	931.450886	11.346816
10.715069	934.506827	11.351834
10.773680	938.580449	11.356851
10.865927	933.758356	11.361869
10.809230	939.173848	11.366887
11.073081	935.353606	11.371904
10.649963	915.615980	11.376922
10.302064	911.619501	11.381939
10.667310	925.942646	11.386957
10.230718	933.314658	11.391975
10.912532	935.509964	11.396992
10.779583	936.312703	11.402010
10.397215	937.692941	11.407027
10.870668	938.171256	11.412045
10.782700	940.612535	11.417063
10.958797	941.639675	11.422080
11.034865	937.111193	11.427098
10.882196	939.428152	11.432115
11.055756	932.826533	11.437133
10.847917	939.698877	11.442151
10.814570	940.010735	11.447168
11.128100	934.856342	11.452186
11.018179	947.614568	11.457203
11.078286	925.520240	11.462221
10.670201	918.379936	11.467239
10.774642	921.533803	11.472256
10.999457	929.056116	11.477274
10.904756	921.941077	11.482291
10.952909	936.123443	11.487309
10.776608	937.598291	11.492327
10.939157	932.063802	11.497344
11.059479	929.957409	11.502362
11.100166	932.826180	11.507379
11.064874	917.282008	11.512397
10.602276	925.493716	11.517415
10.733062	928.248752	11.522432
11.125884	935.528690	11.527450
10.530175	939.868926	11.532467
10.821152	932.872684	11.537485
10.929764	940.859894	11.542503
10.624034	939.894870	11.547520
10.832380	934.763014	11.552538
10.660954	939.368408	11.557555
10.775970	938.608501	11.562573
10.881263	946.526976	11.567591
11.336455	959.695939	11.572608
11.534582	960.806830	11.577626
10.964194	960.241127	11.582643
11.017408	948.590758	11.587661
11.188075	939.362175	11.592679
11.090770	943.840734	11.597696
11.196829	933.706753	11.602714
10.780870	939.134100	11.607731
11.309131	956.322274	11.612749
11.274419	971.450243	11.617767
11.041138	963.649502	11.622784
11.441228	966.612694	11.627802
11.434245	970.001941	11.632819
11.200162	948.757443	11.637837
10.916476	938.929326	11.642855
11.052591	966.435529	11.647872
11.350497	964.238703	11.652890
11.326270	961.887357	11.657907
11.625521	959.246628	11.662925
10.909022	959.527131	11.667943
11.078199	971.675798	11.672960
11.062458	968.895899	11.677978
11.075419	978.398116	11.682995
11.320602	970.994103	11.688013
11.025532	970.766650	11.693031
11.045209	972.962165	11.698048
11.286798	966.222894	11.703066
10.850935	971.531507	11.708083
11.398634	970.741285	11.713101
11.040252	974.338717	11.718119
11.275313	982.908527	11.723136
11.766717	986.468387	11.728154
11.571048	984.142671	11.733171
11.296051	976.127188	11.738189
11.176624	980.979878	11.743207
11.277792	985.588568	11.748224
11.549943	985.128215	11.753242
11.524523	990.957030	11.758259
11.305027	984.897230	11.763277
11.254649	994.122949	11.768295
11.428555	995.283128	11.773312
11.420277	988.843481	11.778330
11.200464	994.099003	11.783347
11.265655	992.347780	11.788365
11.280542	989.052196	11.793383
11.168380	993.415125	11.798400
11.273121	988.465755	11.803418
11.357706	996.208952	11.808435
11.692617	1013.156777	11.813453
11.728858	1022.443363	11.818471
11.607821	1016.668415	11.823488
11.713740	999.736659	11.828506
11.420472	1002.514294	11.833523
11.651471	1022.337879	11.838541
11.797817	1020.321256	11.843559
11.681488	1022.391274	11.848576
11.682686	1006.693733	11.853594
11.574580	1010.647350	11.858611
11.789290	1018.821748	11.863629
11.392620	1019.240620	11.868647
11.397476	1030.825229	11.873664
12.126417	1019.626273	11.878682
11.727680	1028.912849	11.883699
11.481470	1030.820919	11.888717
11.952776	1024.996301	11.893735
11.853763	1027.280767	11.898752
11.919930	1017.677332	11.903770
11.824903	1025.077073	11.908787
12.194198	1018.612684	11.913805
12.162316	1012.561566	11.918823
11.449563	1001.426171	11.923840
12.013529	988.100709	11.928858
11.802692	1006.207752	11.933875
11.410719	1012.895668	11.938893
11.406419	1017.000594	11.943911
11.517095	1015.806774	11.948928
11.589088	1010.760462	11.953946
11.422068	1030.040937	11.958963
11.624462	1016.400931	11.963981
11.878794	1019.355988	11.968999
11.853486	1031.071572	11.974016
11.845175	1029.781711	11.979034
11.931922	1041.897628	11.984051
11.789378	1053.731851	11.989069
12.003748	1052.540935	11.994087
11.914342	1044.413584	11.999104
12.156119	1053.963779	12.004122
12.130713	1053.398767	12.009139
11.798784	1047.190244	12.014157
12.248687	1052.760851	12.019175
12.322656	1055.236746	12.024192
12.427208	1046.751697	12.029210
12.296156	1030.655182	12.034227
12.082258	1022.166189	12.039245
11.915896	1016.546772	12.044263
11.923251	1021.476507	12.049280
12.141711	1018.234211	12.054298
11.909893	1028.291933	12.059315
12.051802	1043.195849	12.064333
12.081583	1044.742483	12.069351
11.933151	1049.242924	12.074368
12.098027	1044.645769	12.079386
12.471697	1052.587177	12.084403
12.372708	1049.417914	12.089421
12.516811	1038.688611	12.094439
12.267750	1036.310314	12.099456
12.320033	1031.490085	12.104474
12.417194	1025.915999	12.109491
12.377176	1023.588123	12.114509
12.547764	1014.159911	12.119527
11.915953	1024.432679	12.124544
12.182072	1014.947704	12.129562
12.453214	1023.666673	12.134579
12.258359	1022.018349	12.139597
12.309017	1015.197687	12.144615
12.272472	1021.949186	12.149632
12.242784	1012.891921	12.154650
12.038853	1032.325749	12.159667
12.636966	1039.929208	12.164685
12.660369	1044.446861	12.169703
12.504330	1040.713447	12.174720
12.559421	1020.484310	12.179738
12.435604	1020.832409	12.184755
12.453173	1018.573735	12.189773
12.301884	1014.017528	12.194791
12.206397	1018.928467	12.199808
12.375408	1017.945451	12.204826
12.035573	1037.736817	12.209843
12.172886	1041.119901	12.214861
12.520874	1045.587347	12.219879
12.444776	1047.252691	12.224896
12.405385	1048.435597	12.229914
12.481420	1051.925677	12.234931
12.267517	1060.653732	12.239949
12.382746	1043.320009	12.244967
12.284632	1044.562637	12.249984
12.516520	1044.238078	12.255002
12.610400	1050.647531	12.260019
12.314390	1051.840650	12.265037
12.646479	1050.438908	12.270055
12.550232	1051.083613	12.275072
12.490137	1049.535800	12.280090
12.588814	1050.907252	12.285107
12.744211	1061.948471	12.290125
12.876374	1050.827057	12.295143
12.577376	1054.633957	12.300160
12.815269	1046.168558	12.305178
12.500754	1052.772801	12.310195
12.378172	1065.591879	12.315213
12.785490	1073.542292	12.320231
12.875321	1086.086457	12.325248
13.031242	1082.628922	12.330266
12.865358	1067.042449	12.335283
12.557118	1051.709084	12.340301
12.975599	1063.780321	12.345319
12.808474	1069.512951	12.350336
12.718295	1065.424938	12.355354
12.905488	1069.082828	12.360371
12.693769	1075.776354	12.365389
13.116892	1077.627526	12.370407
13.178825	1072.208070	12.375424
12.876027	1053.090872	12.380442
12.538192	1055.827079	12.385459
12.530684	1068.618049	12.390477
12.973161	1080.981377	12.395495
12.695032	1087.268991	12.400512
13.115709	1083.904616	12.405530
12.895825	1080.659701	12.410547
12.783527	1081.720435	12.415565
13.157474	1073.309261	12.420583
12.722355	1072.064484	12.425600
13.108546	1074.422540	12.430618
13.152240	1080.383640	12.435635
12.884362	1082.294124	12.440653
13.214338	1081.864742	12.445671
12.927686	1085.449534	12.450688
12.990019	1081.018162	12.455706
13.116908	1079.162621	12.460723
13.095461	1084.389261	12.465741
13.261284	1074.216553	12.470759
13.103943	1080.104648	12.475776
13.140174	1076.977159	12.480794
13.272391	1079.158777	12.485811
13.077422	1084.056291	12.490829
12.957868	1077.945653	12.495847
13.007153	1084.997521	12.500864
13.022601	1072.247841	12.505882
13.271726	1076.403727	12.510899
12.842945	1077.348765	12.515917
13.233265	1067.394387	12.520935
12.942372	1075.174212	12.525952
13.125976	1074.072244	12.530970
13.349041	1078.513144	12.535987
13.026914	1087.406767	12.541005
13.165169	1082.351821	12.546023
12.994370	1088.553554	12.551040
13.085050	1079.414509	12.556058
13.203119	1078.174579	12.561075
13.308287	1099.988321	12.566093
13.532477	1094.439237	12.571111
13.805346	1106.918858	12.576128
13.222080	1094.304130	12.581146
13.709611	1084.936378	12.586163
13.285322	1084.490171	12.591181
13.619139	1078.243830	12.596199
13.588517	1077.613934	12.601216
13.388197	1071.813906	12.606234
13.312871	1076.771130	12.611251
13.054269	1081.199670	12.616269
13.270007	1080.169149	12.621287
13.591012	1091.104229	12.626304
13.421437	1099.273409	12.631322
13.862174	1092.605827	12.636339
13.449321	1090.129847	12.641357
13.648614	1071.631425	12.646375
13.594489	1078.567349	12.651392
13.741750	1069.748455	12.656410
13.712652	1070.950917	12.661427
13.521595	1071.513294	12.666445
13.677583	1074.011830	12.671463
13.326575	1068.978855	12.676480
13.226205	1081.605298	12.681498
13.668062	1094.275028	12.686515
13.811229	1097.076074	12.691533
13.851261	1089.465435	12.696551
13.830624	1079.123213	12.701568
13.282579	1080.387202	12.706586
13.747365	1079.987070	12.711603
13.358947	1095.942208	12.716621
14.133317	1090.816566	12.721639
13.951441	1100.094831	12.726656
13.479915	1101.425676	12.731674
13.790552	1097.473636	12.736691
13.775027	1109.345133	12.741709
13.933096	1093.392007	12.746727
13.754645	1107.998655	12.751744
13.580834	1106.333846	12.756762
13.765637	1117.437556	12.761779
13.381714	1110.328987	12.766797
13.701482	1097.960373	12.771815
13.841383	1103.799255	12.776832
13.703276	1108.588938	12.781850
13.810043	1095.791441	12.786867
13.941019	1096.349309	12.791885
13.874598	1101.836543	12.796903
13.832500	1118.594562	12.801920
13.604211	1103.223497	12.806938
14.056862	1102.408459	12.811955
13.944903	1107.097359	12.816973
14.148173	1096.277512	12.821991
14.068502	1107.499811	12.827008
13.414231	1101.439129	12.832026
13.838084	1103.461831	12.837043
13.808712	1104.761976	12.842061
14.183073	1125.683962	12.847079
14.230647	1134.053809	12.852096
14.435828	1122.569870	12.857114
14.135763	1106.638660	12.862131
13.620204	1115.087575	12.867149
13.691356	1109.405172	12.872167
13.869716	1126.129447	12.877184
14.054945	1136.270534	12.882202
14.091175	1142.705320	12.887219
14.225055	1137.270778	12.892237
14.204209	1141.906412	12.897255
14.299555	1147.050350	12.902272
14.267109	1141.216591	12.907290
14.765052	1133.606478	12.912307
14.308244	1140.359907	12.917325
14.570781	1133.440724	12.922343
14.442121	1108.617250	12.927360
14.154056	1107.009941	12.932378
14.394970	1102.895042	12.937395
14.232149	1093.499158	12.942413
14.130184	1098.025383	12.947431
14.147035	1097.172672	12.952448
14.582067	1122.417132	12.957466
14.663043	1108.222761	12.962483
14.539717	1098.583335	12.967501
14.604848	1101.705167	12.972519
14.422737	1099.866148	12.977536
14.053883	1094.143231	12.982554
14.234161	1092.983153	12.987571
14.234461	1100.954919	12.992589
14.514959	1110.801089	12.997607
14.517126	1124.548738	13.002624
14.429586	1133.351575	13.007642
14.726702	1130.448581	13.012659
14.267624	1115.464923	13.017677
14.504297	1126.380136	13.022695
14.653134	1130.790037	13.027712
14.770236	1128.786509	13.032730
14.549274	1102.632705	13.037747
14.531693	1102.001831	13.042765
14.733263	1110.011923	13.047783
14.574225	1099.665442	13.052800
14.557437	1111.857218	13.057818
14.630592	1113.017948	13.062835
14.368665	1115.787657	13.067853
14.368778	1127.866808	13.072871
14.601451	1128.588540	13.077888
14.588324	1133.958696	13.082906
14.515092	1128.730102	13.087923
14.379522	1133.500476	13.092941
14.245600	1130.035810	13.097959
14.646345	1124.687786	13.102976
14.237573	1129.091208	13.107994
14.357377	1137.016039	13.113011
14.377533	1149.641083	13.118029
14.608672	1155.556211	13.123047
15.039341	1152.356304	13.128064
14.845820	1162.066442	13.133082
14.856565	1158.993549	13.138099
14.791592	1156.868205	13.143117
14.710286	1161.642200	13.148135
15.122066	1160.292211	13.153152
14.863505	1160.191382	13.158170
15.091025	1152.149677	13.163187
14.863140	1150.824909	13.168205
14.749637	1155.942018	13.173223
15.209362	1158.753644	13.178240
14.887008	1156.192984	13.183258
15.008030	1159.086681	13.188275
14.747366	1158.985412	13.193293
14.864889	1154.432286	13.198311
15.050661	1142.718482	13.203328
14.984580	1159.161628	13.208346
15.086934	1152.415808	13.213363
15.019013	1149.019734	13.218381
14.867893	1153.765524	13.223399
15.243452	1153.754563	13.228416
15.080265	1155.430403	13.233434
15.191867	1151.561307	13.238451
15.068475	1156.044247	13.243469
14.985181	1158.094247	13.248487
15.467229	1148.118329	13.253504
15.175738	1161.897711	13.258522
15.078301	1155.738893	13.263539
15.234751	1160.088095	13.268557
15.344881	1153.988604	13.273575
15.278755	1158.071129	13.278592
15.188598	1162.870999	13.283610
15.199997	1157.213039	13.288627
15.161965	1151.556180	13.293645
15.000326	1157.578476	13.298663
15.198725	1155.735494	13.303680
14.917745	1145.622554	13.308698
15.115594	1151.941213	13.313715
15.197850	1159.391973	13.318733
15.498002	1171.969488	13.323751
15.668886	1175.484440	13.328768
15.348077	1169.626377	13.333786
15.716476	1150.187682	13.338803
15.275465	1158.498296	13.343821
15.306312	1153.969365	13.348839
15.492352	1147.586448	13.353856
15.467896	1161.515304	13.358874
14.927997	1154.890403	13.363891
15.291862	1172.597757	13.368909
15.577488	1189.974398	13.373927
15.636099	1178.115488	13.378944
15.531440	1176.841963	13.383962
15.847259	1179.067993	13.388979
15.951160	1176.990270	13.393997
15.734736	1176.145870	13.399015
15.549648	1164.792273	13.404032
15.334546	1158.759628	13.409050
15.835386	1172.579461	13.414067
15.909538	1185.297558	13.419085
15.136997	1170.390557	13.424103
15.572778	1177.294610	13.429120
15.521742	1188.472463	13.434138
15.837519	1183.749495	13.439155
15.989541	1183.017699	13.444173
15.764903	1184.739543	13.449191
15.971575	1177.373699	13.454208
15.704494	1179.343903	13.459226
15.565504	1178.457154	13.464243
15.935196	1172.359947	13.469261
15.650779	1186.574386	13.474279
15.941432	1182.950428	13.479296
15.655941	1179.987607	13.484314
15.845068	1182.633425	13.489331
16.175323	1178.284820	13.494349
15.625534	1182.817118	13.499367
16.282375	1178.901426	13.504384
16.170819	1179.791183	13.509402
15.650208	1168.160083	13.514419
15.820084	1160.771994	13.519437
15.652906	1179.648757	13.524455
15.907663	1181.333341	13.529472
15.821582	1183.780644	13.534490
15.829013	1174.892329	13.539507
15.834845	1174.481583	13.544525
15.935402	1186.712252	13.549543
15.739121	1171.601166	13.554560
16.144437	1178.136654	13.559578
15.987639	1178.735486	13.564595
15.807316	1175.141097	13.569613
15.728265	1175.223527	13.574631
16.169492	1175.791044	13.579648
16.009686	1185.090114	13.584666
16.005147	1179.039915	13.589683
16.430283	1184.228069	13.594701
16.312154	1186.154317	13.599719
16.321379	1171.359977	13.604736
16.126124	1180.190519	13.609754
16.280528	1180.630341	13.614771
16.493306	1175.487830	13.619789
16.204132	1177.785304	13.624807
16.490548	1171.340482	13.629824
16.308468	1179.012184	13.634842
16.109555	1179.043598	13.639859
16.648885	1169.925872	13.644877
16.082565	1173.049137	13.649895
16.192010	1175.318789	13.654912
16.274173	1187.372983	13.659930
15.872325	1184.149911	13.664947
16.221879	1190.079695	13.669965
16.424014	1200.105429	13.674983
16.407213	1196.381204	13.680000
16.398295	1200.152701	13.685018
16.310899	1201.406558	13.690035
16.438654	1209.714744	13.695053
16.482434	1210.449649	13.700071
16.480701	1205.565084	13.705088
16.380010	1206.247538	13.710106
16.261150	1205.136594	13.715123
16.255711	1203.637587	13.720141
16.279325	1204.967547	13.725159
16.407942	1204.959291	13.730176
16.402002	1212.186499	13.735194
16.298291	1203.103193	13.740211
16.532130	1226.283167	13.745229
16.647552	1237.981508	13.750247
16.680627	1237.725300	13.755264
16.804838	1245.030575	13.760282
16.746094	1230.916708	13.765299
17.061301	1242.679605	13.770317
16.869798	1233.075400	13.775335
16.582066	1216.934952	13.780352
16.599761	1225.958597	13.785370
16.713265	1228.451989	13.790387
16.665447	1236.027866	13.795405
16.800500	1234.874480	13.800423
17.283924	1235.569654	13.805440
17.025475	1238.799426	13.810458
16.588376	1230.661444	13.815475
17.139924	1234.584621	13.820493
16.887538	1232.452113	13.825511
16.717062	1214.893076	13.830528
16.553260	1226.421904	13.835546
16.636617	1235.711840	13.840563
17.105854	1232.724815	13.845581
17.126590	1232.360024	13.850599
17.137919	1235.731730	13.855616
16.922198	1232.227045	13.860634
16.796200	1239.380842	13.865651
17.213053	1240.550808	13.870669
16.870940	1231.908527	13.875687
16.955763	1232.284678	13.880704
17.131416	1226.343988	13.885722
16.789067	1237.820504	13.890739
17.026325	1232.557388	13.895757
17.114298	1231.346839	13.900775
17.259070	1238.732956	13.905792
17.445234	1235.353054	13.910810
17.082559	1233.961625	13.915827
17.199326	1228.644842	13.920845
16.897918	1237.685116	13.925863
17.261951	1228.055060	13.930880
17.040623	1234.001052	13.935898
17.153311	1237.094564	13.940915
17.086559	1239.894571	13.945933
16.978048	1232.982852	13.950951
16.883743	1229.723802	13.955968
17.361419	1238.172478	13.960986
17.142970	1258.878646	13.966003
17.299189	1258.801254	13.971021
17.318636	1261.027950	13.976039
17.651602	1269.785245	13.981056
17.860761	1264.392129	13.986074
17.324959	1262.064035	13.991091
18.133604	1249.972210	13.996109
17.302758	1247.219760	14.001127
17.146898	1226.955209	14.006144
17.466376	1239.578003	14.011162
17.263108	1245.568251	14.016179
17.371081	1257.398546	14.021197
17.711471	1267.657723	14.026215
17.986745	1265.030363	14.031232
17.472378	1251.259635	14.036250
17.552779	1261.205177	14.041267
17.809258	1253.272796	14.046285
17.432355	1253.678163	14.051303
17.786455	1255.912826	14.056320
17.811337	1262.015297	14.061338
17.435730	1249.622346	14.066355
17.676587	1245.281047	14.071373
17.760156	1262.217224	14.076391
17.844451	1257.019586	14.081408
17.920766	1256.901096	14.086426
17.781882	1257.126896	14.091443
17.855881	1240.757629	14.096461
17.553133	1242.903428	14.101479
17.708067	1254.335009	14.106496
18.289532	1252.773061	14.111514
18.080876	1250.353001	14.116531
17.963348	1234.155218	14.121549
17.464619	1231.748944	14.126567
17.621045	1240.281527	14.131584
17.642542	1248.962439	14.136602
17.767145	1265.236723	14.141619
18.048717	1253.385322	14.146637
17.748464	1269.598078	14.151655
17.767068	1261.946809	14.156672
17.788727	1264.327860	14.161690
17.533807	1261.572948	14.166707
17.771680	1257.928186	14.171725
17.613492	1258.718191	14.176743
18.004671	1269.788230	14.181760
17.945924	1286.911777	14.186778
17.822226	1294.404187	14.191795
18.459904	1286.711019	14.196813
18.124992	1292.332149	14.201831
17.727310	1293.625584	14.206848
18.518771	1289.724580	14.211866
18.114684	1296.896502	14.216883
18.428731	1296.396526	14.221901
18.724309	1293.603598	14.226919
18.081235	1287.761454	14.231936
18.314983	1276.982104	14.236954
18.194402	1272.102632	14.241971
18.236106	1272.476476	14.246989
18.142820	1286.796361	14.252007
18.103580	1295.078704	14.257024
18.313671	1300.065111	14.262042
18.438769	1296.149651	14.267059
18.466421	1297.735638	14.272077
18.435376	1291.052397	14.277095
18.541725	1300.245653	14.282112
18.835864	1291.347982	14.287130
18.287148	1291.053865	14.292147
18.301667	1289.273599	14.297165
18.272370	1288.227737	14.302183
18.406568	1294.426289	14.307200
18.575283	1288.802072	14.312218
18.449682	1303.639910	14.317235
18.499238	1295.303987	14.322253
18.465816	1294.452111	14.327271
18.335979	1295.949218	14.332288
18.355190	1296.938585	14.337306
18.074834	1294.477636	14.342323
18.480439	1286.559519	14.347341
18.676782	1289.430926	14.352359
18.444514	1297.927121	14.357376
18.766898	1298.819434	14.362394
18.611559	1317.919990	14.367411
18.689676	1315.072125	14.372429
18.565291	1319.780862	14.377447
18.616416	1326.278217	14.382464
18.920724	1315.358024	14.387482
18.598826	1322.612408	14.392499
19.126877	1321.035283	14.397517
18.902660	1321.793313	14.402535
18.785722	1322.549327	14.407552
18.916417	1325.769400	14.412570
18.731256	1333.325155	14.417587
18.849160	1324.692864	14.422605
18.976578	1317.898728	14.427623
18.857017	1329.002205	14.432640
19.028728	1319.159063	14.437658
18.974516	1319.849179	14.442675
18.809359	1324.185149	14.447693
19.166109	1305.836356	14.452711
18.713016	1315.228163	14.457728
19.321789	1316.278167	14.462746
19.053948	1326.403856	14.467763
19.279536	1316.517149	14.472781
19.446130	1318.251780	14.477799
19.057775	1320.704672	14.482816
19.351188	1321.195100	14.487834
19.091788	1328.092294	14.492851
19.385115	1314.369647	14.497869
19.494057	1325.690395	14.502887
19.015163	1322.226120	14.507904
19.214953	1314.138532	14.512922
19.034561	1321.161219	14.517939
19.144941	1329.028261	14.522957
19.476328	1318.830732	14.527975
19.320823	1321.610413	14.532992
19.530178	1315.921189	14.538010
19.302099	1322.850596	14.543027
19.520363	1311.950559	14.548045
19.353083	1315.040449	14.553063
19.309025	1320.105955	14.558080
19.662757	1313.660557	14.563098
19.678810	1321.029840	14.568115
19.239898	1316.582982	14.573133
19.390055	1313.263749	14.578151
19.177230	1314.609249	14.583168
19.477505	1305.338909	14.588186
19.340691	1321.228598	14.593203
19.327264	1311.116913	14.598221
19.602885	1310.199687	14.603239
19.422282	1319.453069	14.608256
19.552105	1315.708472	14.613274
19.378944	1310.500301	14.618291
19.755724	1313.434351	14.623309
19.654440	1312.142539	14.628327
19.665670	1315.664277	14.633344
19.766770	1313.690540	14.638362
19.388108	1325.677847	14.643379
19.608122	1332.524789	14.648397
19.554114	1339.279317	14.653415
19.658070	1352.737089	14.658432
19.880941	1349.200300	14.663450
19.556751	1358.331816	14.668467
19.762920	1347.909339	14.673485
19.869752	1342.030788	14.678503
19.853041	1345.818177	14.683520
19.531081	1344.241259	14.688538
19.872398	1354.377114	14.693555
19.421743	1345.094488	14.698573
20.041200	1345.893911	14.703591
19.891297	1352.294252	14.708608
20.221556	1345.721234	14.713626
20.077430	1343.687317	14.718643
20.008427	1335.555253	14.723661
20.074257	1335.389681	14.728679
20.061335	1352.238787	14.733696
19.923431	1342.689810	14.738714
20.097362	1343.506711	14.743731
19.637942	1349.416190	14.748749
20.059212	1362.069471	14.753767
20.317485	1379.153221	14.758784
20.200027	1367.308363	14.763802
20.378400	1370.637871	14.768819
20.301098	1374.760098	14.773837
20.359986	1354.516905	14.778855
20.186213	1350.234789	14.783872
20.231311	1354.071393	14.788890
20.173701	1367.877974	14.793907
20.251489	1367.760026	14.798925
20.528155	1371.954344	14.803943
20.406354	1372.746204	14.808960
20.475593	1375.382774	14.813978
20.529083	1371.287030	14.818995
20.019501	1376.069019	14.824013
20.476257	1371.928150	14.829031
20.066345	1378.994776	14.834048
20.443428	1367.767225	14.839066
20.446239	1375.440296	14.844083
20.407882	1372.186125	14.849101
20.496649	1375.831649	14.854119
20.402179	1373.456439	14.859136
20.308971	1383.512696	14.864154
20.220281	1377.799184	14.869171
20.593436	1375.712280	14.874189
20.621592	1380.041451	14.879207
20.229257	1376.091972	14.884224
20.599276	1372.062708	14.889242
20.578969	1388.948510	14.894259
20.825796	1400.745291	14.899277
20.757114	1394.357604	14.904295
20.585494	1398.921827	14.909312
21.064073	1399.962689	14.914330
21.048609	1393.574851	14.919347
20.562007	1381.384030	14.924365
20.506971	1383.959292	14.929383
20.728426	1403.284561	14.934400
20.746601	1400.745814	14.939418
21.048847	1406.660682	14.944435
20.663132	1420.088971	14.949453
20.657553	1402.229191	14.954471
20.976080	1415.027086	14.959488
21.135783	1412.862533	14.964506
21.060808	1406.127857	14.969523
21.184178	1400.051667	14.974541
21.221080	1401.009765	14.979559
21.022147	1415.086636	14.984576
20.901433	1398.614016	14.989594
21.089346	1403.744679	14.994611
21.104855	1407.475568	14.999629
21.477255	1402.392375	15.004647
21.162561	1407.967679	15.009664
21.027159	1403.231170	15.014682
21.427792	1404.133760	15.019699
21.424390	1401.140326	15.024717
21.456544	1398.138249	15.029735
21.102746	1407.187296	15.034752
20.957266	1399.236364	15.039770
21.042352	1397.304639	15.044787
21.362331	1400.572909	15.049805
21.349364	1391.676825	15.054823
21.242990	1404.150196	15.059840
21.049731	1396.562684	15.064858
21.242658	1398.239814	15.069875
21.007636	1407.717218	15.074893
21.486571	1393.241336	15.079911
21.289907	1400.692732	15.084928
21.332746	1408.271790	15.089946
21.633273	1419.978593	15.094963
21.390033	1424.058627	15.099981
21.875000	1420.842195	15.104999
21.759498	1423.244014	15.110016
21.492408	1410.234942	15.115034
21.645266	1406.968391	15.120051
21.386489	1423.434671	15.125069
21.610107	1411.438024	15.130087
21.390276	1422.118808	15.135104
21.840400	1421.019926	15.140122
22.047574	1420.235287	15.145139
21.884358	1425.450873	15.150157
21.748708	1420.451804	15.155175
21.607444	1420.453987	15.160192
21.909013	1422.934771	15.165210
21.523583	1418.398319	15.170227
21.394250	1431.875500	15.175245
21.749264	1417.120909	15.180263
21.551892	1417.995756	15.185280
21.432330	1412.842847	15.190298
21.690128	1415.988349	15.195315
21.298642	1424.453892	15.200333
21.816416	1431.446843	15.205351
21.806618	1445.476281	15.210368
21.958763	1453.171118	15.215386
22.362581	1452.119271	15.220403
22.184505	1452.759038	15.225421
22.254987	1452.556474	15.230439
22.121895	1458.661560	15.235456
22.193402	1455.950983	15.240474
22.413429	1445.891495	15.245491
22.076510	1434.144737	15.250509
22.196391	1421.882194	15.255527
22.118483	1432.340274	15.260544
22.079510	1446.909970	15.265562
22.448391	1441.743491	15.270579
22.298288	1445.575040	15.275597
22.587824	1443.023240	15.280615
22.001594	1433.257506	15.285632
21.987791	1431.683092	15.290650
22.218625	1450.187192	15.295667
21.930778	1443.447200	15.300685
22.679342	1443.698878	15.305703
22.150172	1441.816896	15.310720
22.330083	1443.774923	15.315738
22.244619	1439.865555	15.320755
22.254751	1449.832696	15.325773
22.544675	1442.229716	15.330791
22.553731	1446.814821	15.335808
22.262214	1444.361208	15.340826
22.519765	1438.003339	15.345843
22.229323	1447.943874	15.350861
22.739129	1447.892181	15.355879
22.802145	1444.342865	15.360896
22.396166	1447.990805	15.365914
22.712276	1458.082478	15.370931
22.601130	1472.049590	15.375949
22.881368	1470.518212	15.380967
22.653116	1466.865944	15.385984
22.838398	1477.261180	15.391002
23.365760	1465.909856	15.396019
22.975774	1451.061279	15.401037
22.583748	1447.273932	15.406055
22.791239	1439.634604	15.411072
22.706599	1446.906056	15.416090
22.926248	1456.223947	15.421107
23.153524	1463.229585	15.426125
22.922921	1459.950931	15.431143
22.885766	1450.730869	15.436160
22.873260	1464.719435	15.441178
23.052506	1472.148773	15.446195
22.801400	1474.438805	15.451213
23.083738	1465.265433	15.456231
22.870505	1476.463660	15.461248
22.886365	1476.795332	15.466266
22.992666	1472.043973	15.471283
22.636787	1476.591487	15.476301
23.250528	1466.630175	15.481319
23.294489	1463.267472	15.486336
22.788465	1476.031487	15.491354
23.167688	1473.683727	15.496371
23.076402	1478.275221	15.501389
23.009661	1473.406061	15.506407
23.311507	1482.481620	15.511424
23.309454	1497.525560	15.516442
23.370040	1499.569101	15.521459
23.595840	1497.657763	15.526477
23.709700	1484.958769	15.531495
23.384576	1470.315179	15.536512
23.334789	1467.804211	15.541530
23.679065	1455.621017	15.546547
23.219741	1462.963576	15.551565
23.140887	1466.248299	15.556583
23.490842	1486.254353	15.561600
23.608965	1500.879975	15.566618
23.893477	1496.701062	15.571635
23.543063	1478.304601	15.576653
23.469759	1470.312548	15.581671
23.668323	1475.882804	15.586688
23.672033	1494.942279	15.591706
23.882629	1497.580265	15.596723
23.611826	1496.248400	15.601741
23.440323	1490.750526	15.606759
23.705301	1498.638510	15.611776
23.707585	1506.153861	15.616794
24.019941	1496.758573	15.621811
24.041004	1504.505456	15.626829
23.829432	1494.700476	15.631847
23.923607	1495.254611	15.636864
23.766538	1509.002198	15.641882
23.705187	1492.777913	15.646899
24.107862	1496.968722	15.651917
24.077368	1494.228966	15.656935
23.873821	1491.707235	15.661952
23.664460	1500.224943	15.666970
24.004319	1494.097513	15.671987
23.865849	1498.148801	15.677005
23.890676	1485.850373	15.682023
24.408533	1485.400894	15.687040
23.790730	1497.328721	15.692058
24.085233	1489.485592	15.697075
24.140924	1498.947587	15.702093
24.009892	1490.455245	15.707111
24.036108	1495.175317	15.712128
23.924106	1501.195825	15.717146
24.290144	1493.967220	15.722163
23.890455	1501.467243	15.727181
24.381888	1511.094096	15.732199
24.661826	1525.002400	15.737216
24.338199	1518.604911	15.742234
24.604189	1506.158659	15.747251
24.353340	1502.637289	15.752269
24.127406	1496.425992	15.757287
24.367785	1499.834629	15.762304
24.249063	1521.771865	15.767322
24.595196	1521.120114	15.772339
24.401101	1523.397957	15.777357
24.452446	1525.740273	15.782375
24.716039	1520.112073	15.787392
24.450480	1524.536378	15.792410
24.626346	1519.241206	15.797427
24.155011	1519.918513	15.802445
24.217376	1533.610494	15.807463
24.446851	1521.669485	15.812480
24.305141	1532.224417	15.817498
24.725269	1523.041974	15.822515
24.853996	1533.393858	15.827533
24.820608	1535.039189	15.832551
25.039959	1529.832875	15.837568
24.600339	1524.526630	15.842586
24.752822	1526.932120	15.847603
24.850224	1545.862758	15.852621
25.237433	1550.545116	15.857639
25.070896	1531.465786	15.862656
24.753460	1525.886554	15.867674
25.080115	1527.019511	15.872691
24.970321	1523.636193	15.877709
25.007870	1524.891433	15.882727
25.425824	1518.685708	15.887744
25.226763	1523.068293	15.892762
24.892258	1513.073817	15.897779
24.736498	1519.417717	15.902797
24.595181	1537.663078	15.907815
24.978620	1542.637394	15.912832
25.215211	1551.150181	15.917850
25.511863	1549.935367	15.922867
25.783891	1549.378170	15.927885
25.328781	1542.677248	15.932903
25.355052	1535.203314	15.937920
25.210707	1545.605149	15.942938
25.127789	1546.760261	15.947955
25.415601	1548.420908	15.952973
25.522313	1543.366706	15.957991
25.796532	1542.994972	15.963008
25.471582	1540.194126	15.968026
25.608958	1526.607352	15.973043
25.358347	1523.359557	15.978061
25.435062	1531.883453	15.983079
25.784691	1540.280272	15.988096
25.524257	1527.694799	15.993114
25.346835	1522.238444	15.998131
25.766006	1538.094949	16.003149
25.378004	1533.936838	16.008167
25.784754	1534.828188	16.013184
25.596482	1546.448706	16.018202
25.442825	1543.230915	16.023219
25.541022	1539.922600	16.028237
25.668955	1537.455813	16.033255
25.815124	1544.968616	16.038272
25.651180	1549.049725	16.043290
25.580926	1544.083488	16.048307
26.025743	1551.680304	16.053325
26.032754	1552.034309	16.058343
26.192189	1540.401733	16.063360
25.522537	1550.881897	16.068378
25.658365	1539.958738	16.073395
25.869090	1539.854996	16.078413
25.488679	1543.956595	16.083431
25.860270	1549.674603	16.088448
25.906680	1563.319252	16.093466
25.832479	1568.794553	16.098483
26.123149	1568.040175	16.103501
25.857892	1579.333310	16.108519
26.122647	1568.442325	16.113536
26.258291	1572.778948	16.118554
26.207771	1566.595661	16.123571
26.216676	1568.861155	16.128589
25.822731	1568.924077	16.133607
26.194682	1565.493260	16.138624
26.042490	1576.627908	16.143642
26.009680	1578.353856	16.148659
26.007371	1576.573194	16.153677
25.981916	1600.619890	16.158695
26.571630	1601.582521	16.163712
26.280622	1598.665808	16.168730
26.646752	1600.550500	16.173747
26.789789	1604.522129	16.178765
26.690566	1605.837425	16.183783
26.604485	1603.815514	16.188800
26.625103	1605.862932	16.193818
26.841744	1603.492075	16.198835
26.817064	1599.591105	16.203853
26.828838	1595.914807	16.208871
26.699119	1570.768328	16.213888
26.447716	1566.169481	16.218906
26.411670	1581.403776	16.223923
26.954022	1581.779369	16.228941
26.829402	1592.253559	16.233959
26.910044	1594.828436	16.238976
26.872874	1591.685045	16.243994
27.014590	1586.822276	16.249011
26.751668	1585.333586	16.254029
26.882801	1587.262308	16.259047
27.060768	1582.613221	16.264064
26.917046	1595.574425	16.269082
26.839419	1592.854267	16.274099
27.063902	1588.163224	16.279117
26.919949	1590.320569	16.284135
26.895674	1589.313225	16.289152
26.706911	1601.674808	16.294170
26.911571	1594.828784	16.299187
26.794348	1599.513191	16.304205
26.733054	1604.873770	16.309223
27.281022	1595.785469	16.314240
26.923243	1602.881358	16.319258
26.818596	1603.172358	16.324275
27.397508	1611.263139	16.329293
27.269674	1623.418587	16.334311
27.852271	1614.455250	16.339328
27.387991	1605.385352	16.344346
27.320235	1588.983287	16.349363
27.155661	1588.280671	16.354381
27.500728	1613.793192	16.359399
28.081247	1610.211294	16.364416
27.759741	1604.096881	16.369434
27.381140	1593.018714	16.374451
27.481642	1588.769065	16.379469
27.398299	1591.521489	16.384487
27.861888	1587.256599	16.389504
27.570121	1588.993146	16.394522
27.839147	1584.702207	16.399539
27.637305	1579.907354	16.404557
27.111330	1586.866915	16.409575
27.572182	1599.496120	16.414592
27.721619	1611.301709	16.419610
27.904779	1613.128512	16.424627
28.019698	1616.995745	16.429645
27.567456	1621.558864	16.434663
27.812136	1606.028665	16.439680
27.921908	1611.956981	16.444698
28.114797	1619.440430	16.449715
28.178877	1614.918853	16.454733
27.753892	1624.079026	16.459751
28.100093	1613.453656	16.464768
27.993130	1610.240323	16.469786
27.999268	1616.060605	16.474803
28.185947	1613.830534	16.479821
28.140573	1613.236524	16.484839
28.109027	1613.364238	16.489856
27.994614	1616.976928	16.494874
27.975427	1618.458893	16.499891
28.301691	1614.456499	16.504909
28.136161	1627.631970	16.509927
28.195207	1610.658098	16.514944
28.303900	1603.242924	16.519962
28.127451	1613.837915	16.524979
28.514661	1603.229384	16.529997
28.159347	1613.279585	16.535015
28.340872	1607.384235	16.540032
28.171378	1616.684773	16.545050
27.839461	1621.564187	16.550067
28.497987	1626.322901	16.555085
28.487766	1649.279356	16.560103
28.399257	1638.823591	16.565120
28.490915	1638.095078	16.570138
28.404222	1651.022475	16.575155
28.853115	1639.387169	16.580173
28.506813	1643.111492	16.585191
28.902910	1639.757763	16.590208
28.572715	1642.663278	16.595226
28.477855	1642.146752	16.600243
28.957717	1641.278759	16.605261
28.850785	1640.887067	16.610279
28.884560	1633.198458	16.615296
28.697932	1634.036892	16.620314
28.544455	1653.172196	16.625331
28.595828	1640.174369	16.630349
28.937794	1641.386689	16.635367
29.003060	1638.574752	16.640384
28.931333	1642.530772	16.645402
28.517092	1641.145874	16.650419
29.396750	1647.435693	16.655437
29.328837	1649.437541	16.660455
29.312882	1644.428421	16.665472
29.200369	1638.469151	16.670490
29.074112	1635.803496	16.675507
29.357865	1630.556563	16.680525
29.258716	1637.494680	16.685543
29.537785	1634.883559	16.690560
29.484782	1627.681763	16.695578
28.739846	1642.248072	16.700595
29.236914	1630.290228	16.705613
29.272967	1634.768556	16.710631
29.336888	1640.050538	16.715648
29.527540	1628.934380	16.720666
29.175948	1639.397368	16.725683
29.361572	1654.702508	16.730701
29.438148	1663.440673	16.735719
29.363317	1663.493666	16.740736
29.478883	1667.977341	16.745754
29.323553	1673.345247	16.750771
29.608666	1654.564205	16.755789
29.637035	1667.178861	16.760807
29.623831	1660.232270	16.765824
29.633254	1661.713439	16.770842
29.539267	1662.105431	16.775859
29.721540	1667.509557	16.780877
29.642221	1669.900697	16.785895
29.417349	1659.199782	16.790912
29.882357	1667.773628	16.795930
29.703758	1678.754847	16.800947
30.001476	1689.004836	16.805965
29.869747	1686.661732	16.810983
30.017540	1688.212116	16.816000
30.428011	1686.351672	16.821018
29.992227	1684.135295	16.826035
30.322381	1660.221185	16.831053
30.015196	1663.955571	16.836071
30.012165	1658.169896	16.841088
30.009340	1661.633016	16.846106
30.212144	1679.596363	16.851123
30.449015	1682.916252	16.856141
30.525816	1684.939023	16.861159
30.352010	1677.820199	16.866176
30.249938	1654.127672	16.871194
30.098682	1657.464188	16.876211
30.267863	1676.013414	16.881229
30.254177	1676.808645	16.886247
30.155290	1683.668786	16.891264
30.423316	1688.549269	16.896282
30.335558	1686.832351	16.901299
30.210054	1689.080354	16.906317
30.258467	1688.855458	16.911335
30.155541	1686.855617	16.916352
30.484288	1683.240591	16.921370
30.420238	1681.619353	16.926387
30.174444	1677.438442	16.931405
29.963540	1689.876202	16.936423
30.673867	1699.668502	16.941440
30.821591	1710.887047	16.946458
30.822715	1714.105429	16.951475
30.980170	1713.448694	16.956493
30.911073	1710.232220	16.961511
30.889986	1701.523523	16.966528
30.986639	1700.240635	16.971546
31.106567	1709.271648	16.976563
31.493037	1704.258864	16.981581
31.177217	1702.905694	16.986599
30.858408	1686.321869	16.991616
31.227751	1684.946583	16.996634
31.185767	1682.402791	17.001651
31.037413	1678.154169	17.006669
31.037560	1679.983333	17.011687
31.183215	1691.150631	17.016704
31.321979	1696.821422	17.021722
31.164199	1693.149949	17.026739
30.952659	1695.393303	17.031757
31.232727	1705.935203	17.036775
31.046933	1702.635691	17.041792
31.288950	1700.072035	17.046810
31.075800	1703.799520	17.051827
31.316533	1703.181752	17.056845
31.360770	1699.086273	17.061863
31.141804	1699.832033	17.066880
31.541464	1695.232030	17.071898
31.432320	1701.057653	17.076915
31.235688	1689.638259	17.081933
31.434059	1705.394489	17.086951
31.493842	1712.485456	17.091968
31.780292	1728.020038	17.096986
31.536679	1735.830156	17.102003
31.763959	1729.460252	17.107021
31.703025	1728.217629	17.112039
31.666244	1737.551775	17.117056
31.827348	1727.861314	17.122074
31.708048	1735.050450	17.127091
31.861089	1731.521595	17.132109
31.897268	1735.172368	17.137127
31.758464	1733.664685	17.142144
31.826955	1731.386846	17.147162
31.735978	1735.185053	17.152179
32.046885	1721.949691	17.157197
32.314710	1729.051491	17.162215
31.925258	1732.485341	17.167232
31.999067	1729.799139	17.172250
32.087061	1725.701132	17.177267
32.077738	1724.029882	17.182285
32.272867	1717.609007	17.187303
32.388535	1720.665903	17.192320
32.393904	1723.826497	17.197338
32.326298	1725.679877	17.202355
31.901645	1725.714419	17.207373
32.391966	1722.400189	17.212391
32.457173	1738.166693	17.217408
32.636245	1727.388605	17.222426
32.535839	1725.392672	17.227443
32.132395	1713.689788	17.232461
32.449614	1722.448768	17.237479
32.430192	1745.959649	17.242496
32.582733	1740.001725	17.247514
32.496576	1755.619688	17.252531
32.596527	1746.153516	17.257549
33.009702	1748.174926	17.262567
32.857275	1746.589576	17.267584
32.971012	1734.084496	17.272602
32.688787	1743.979371	17.277619
32.781767	1739.339586	17.282637
32.821187	1741.267372	17.287655
32.505621	1743.350398	17.292672
32.766723	1737.372137	17.297690
33.096863	1741.854948	17.302707
33.050925	1737.650768	17.307725
33.085316	1743.373111	17.312743
33.010438	1744.771003	17.317760
32.951045	1745.654909	17.322778
33.110716	1738.456427	17.327795
33.152988	1738.294752	17.332813
33.411389	1743.102831	17.337831
33.332980	1749.849373	17.342848
33.733225	1745.327605	17.347866
33.548820	1748.207816	17.352883
33.078109	1742.801130	17.357901
33.255762	1741.824513	17.362919
33.217263	1742.924646	17.367936
33.892080	1746.937388	17.372954
33.570635	1745.176482	17.377971
33.346870	1751.277011	17.382989
33.272561	1746.393270	17.388007
33.384706	1747.457041	17.393024
33.362273	1748.757665	17.398042
33.157428	1745.314841	17.403059
33.045913	1751.225128	17.408077
33.218778	1745.711084	17.413095
33.141890	1750.790435	17.418112
33.531104	1766.805679	17.423130
33.335584	1772.502324	17.428147
33.104770	1777.490636	17.433165
33.627925	1768.418944	17.438183
33.302924	1775.552790	17.443200
33.790864	1779.358295	17.448218
33.954170	1785.777029	17.453235
33.639841	1795.227642	17.458253
34.152592	1788.534062	17.463271
33.981039	1789.471190	17.468288
33.949888	1785.493685	17.473306
33.805642	1791.909805	17.478323
33.962290	1791.524857	17.483341
34.235733	1779.918500	17.488359
34.055245	1795.667872	17.493376
34.163072	1782.877115	17.498394
34.248145	1787.986352	17.503411
34.307364	1793.065226	17.508429
34.337053	1793.163904	17.513447
34.353873	1791.722573	17.518464
34.011580	1787.124930	17.523482
34.495029	1787.858712	17.528499
34.330775	1779.966599	17.533517
34.488254	1795.533235	17.538535
34.562474	1805.932516	17.543552
34.954739	1812.229883	17.548570
35.177906	1797.119202	17.553587
34.804736	1790.534919	17.558605
35.300079	1777.393380	17.563623
35.109815	1782.773407	17.568640
35.006569	1783.165754	17.573658
35.150693	1789.006953	17.578675
34.840113	1785.442651	17.583693
34.686624	1774.308178	17.588711
34.774368	1777.283487	17.593728
34.911109	1769.768707	17.598746
34.677910	1782.510629	17.603763
34.644770	1778.040537	17.608781
34.983028	1764.490765	17.613799
34.671837	1782.250365	17.618816
34.818131	1773.011939	17.623834
34.911025	1776.472226	17.628851
34.976652	1782.359097	17.633869
35.345043	1774.470913	17.638887
34.930511	1785.933799	17.643904
34.828176	1776.977094	17.648922
34.952097	1786.654741	17.653939
34.758101	1807.571764	17.658957
34.946344	1810.632014	17.663975
35.212467	1819.681404	17.668992
35.510304	1818.928977	17.674010
35.413162	1816.128547	17.679027
35.336853	1808.536427	17.684045
35.706621	1807.807130	17.689063
35.643080	1807.324389	17.694080
35.590666	1816.119039	17.699098
35.531856	1809.742932	17.704115
35.580012	1810.548009	17.709133
35.749589	1804.600232	17.714151
35.276933	1804.361617	17.719168
35.599600	1806.149988	17.724186
35.701425	1833.051982	17.729203
35.693383	1837.408535	17.734221
36.146620	1828.782643	17.739239
35.937269	1842.362407	17.744256
35.867980	1835.608886	17.749274
36.229846	1834.422623	17.754291
35.993823	1834.229076	17.759309
36.268461	1835.478547	17.764327
36.136643	1836.449649	17.769344
36.325528	1827.384455	17.774362
35.909773	1832.728216	17.779379
36.076903	1840.687697	17.784397
36.498799	1822.175145	17.789415
36.459309	1829.875131	17.794432
36.095129	1833.889470	17.799450
36.321317	1820.896402	17.804467
36.207378	1835.257614	17.809485
36.345962	1819.533744	17.814503
36.255178	1831.641881	17.819520
36.282622	1817.612028	17.824538
36.361315	1814.859647	17.829555
36.286405	1824.590321	17.834573
36.656137	1819.136960	17.839591
36.171522	1816.296752	17.844608
36.267489	1825.938501	17.849626
36.231359	1832.372562	17.854643
36.346872	1847.780844	17.859661
36.922668	1854.268312	17.864679
36.721635	1861.617893	17.869696
36.984931	1859.337305	17.874714
37.231131	1854.910700	17.879731
36.855432	1870.320027	17.884749
37.038255	1855.778577	17.889767
37.017436	1867.381842	17.894784
36.656666	1848.059477	17.899802
37.139650	1858.114725	17.904819
37.267131	1859.214154	17.909837
37.098224	1858.369326	17.914855
37.334247	1852.469191	17.919872
37.157385	1851.563869	17.924890
37.103944	1845.977026	17.929907
36.876493	1846.819081	17.934925
37.305967	1842.008583	17.939943
37.090805	1849.729401	17.944960
37.188977	1851.888026	17.949978
37.126511	1838.939198	17.954995
37.024095	1855.920208	17.960013
37.517906	1849.891952	17.965031
37.462491	1873.433002	17.970048
37.412541	1870.842860	17.975066
37.968872	1871.449223	17.980083
37.503214	1877.491429	17.985101
37.897612	1875.469056	17.990119
37.493599	1867.477227	17.995136
37.474662	1880.692025	18.000154
38.074464	1871.849317	18.005171
37.777961	1874.677246	18.010189
38.147681	1870.203411	18.015207
38.124814	1879.491244	18.020224
37.931299	1864.292013	18.025242
37.929732	1856.288275	18.030259
37.481760	1875.695850	18.035277
37.667295	1866.926468	18.040295
37.800365	1866.253686	18.045312
37.799262	1872.207154	18.050330
38.033170	1879.075661	18.055347
37.898184	1869.545166	18.060365
37.829593	1868.106947	18.065383
37.839567	1880.545686	18.070400
38.041664	1888.439165	18.075418
38.383278	1892.445310	18.080435
38.174839	1904.958819	18.085453
38.529767	1890.386082	18.090471
38.698944	1897.479492	18.095488
38.554505	1892.069907	18.100506
38.788929	1887.640125	18.105523
38.766045	1899.821325	18.110541
38.683582	1889.121473	18.115559
38.706052	1891.869814	18.120576
38.636477	1889.054568	18.125594
38.956730	1887.496053	18.130611
38.884767	1892.122265	18.135629
38.985101	1888.139103	18.140647
39.136312	1895.998491	18.145664
38.713593	1898.175660	18.150682
39.052309	1884.900121	18.155699
38.927809	1889.441724	18.160717
39.022458	1892.159215	18.165735
38.974862	1890.784841	18.170752
38.875382	1896.304208	18.175770
39.103275	1891.570777	18.180787
38.762611	1897.558041	18.185805
38.649281	1893.144503	18.190823
38.863404	1892.698854	18.195840
38.737259	1887.939402	18.200858
38.943987	1892.324187	18.205875
39.269802	1912.302507	18.210893
39.066981	1915.664940	18.215911
39.248432	1922.010646	18.220928
38.767626	1925.500610	18.225946
39.129247	1910.670835	18.230963
39.339764	1917.920798	18.235981
39.342309	1922.491373	18.240999
39.639901	1933.278563	18.246016
39.319724	1948.384673	18.251034
39.725032	1951.193649	18.256051
39.647651	1950.641541	18.261069
39.688068	1946.280877	18.266087
39.729338	1947.639474	18.271104
39.626142	1942.532104	18.276122
39.802826	1943.671817	18.281139
39.662013	1946.154680	18.286157
39.801816	1943.250029	18.291175
40.018689	1939.915679	18.296192
40.027408	1951.068832	18.301210
39.910693	1942.220714	18.306227
39.927631	1945.382980	18.311245
39.941035	1938.920451	18.316263
40.088157	1944.050962	18.321280
39.936474	1939.735102	18.326298
40.553372	1944.846486	18.331315
40.312316	1938.563497	18.336333
39.968458	1946.837179	18.341351
40.413779	1951.496258	18.346368
40.167172	1954.899021	18.351386
40.210693	1961.772318	18.356403
40.491654	1973.216240	18.361421
40.442207	1969.226363	18.366439
40.744041	1957.332096	18.371456
40.764903	1970.486835	18.376474
40.586996	1963.509113	18.381491
40.557013	1965.090932	18.386509
40.455102	1970.148907	18.391527
40.600105	1960.003872	18.396544
40.575075	1963.323488	18.401562
40.613154	1962.186501	18.406579
40.527800	1974.351331	18.411597
40.751351	1986.399663	18.416615
40.962042	1989.245991	18.421632
40.795240	1994.768273	18.426650
40.938300	1989.479162	18.431667
40.898926	1995.727997	18.436685
40.862100	1992.376590	18.441703
40.953638	2000.765215	18.446720
41.240921	2007.413518	18.451738
41.197538	1994.872040	18.456755
41.466032	1992.695299	18.461773
41.311484	1993.356388	18.466791
41.351228	1992.882523	18.471808
41.212180	1993.008750	18.476826
41.573605	1984.221201	18.481843
41.536667	2003.033694	18.486861
41.478883	2005.936293	18.491879
41.869124	2013.095909	18.496896
41.970411	2006.713683	18.501914
42.187821	1990.457285	18.506931
41.838027	1994.012186	18.511949
41.923595	1992.321651	18.516967
41.956684	1984.721173	18.521984
41.635228	1984.864611	18.527002
41.861495	1979.732596	18.532019
41.672120	1982.478236	18.537037
41.604010	1988.596785	18.542055
42.068591	1993.088511	18.547072
41.905819	2011.626963	18.552090
42.077704	2010.796957	18.557107
42.171268	2013.248502	18.562125
42.117211	2014.967386	18.567143
42.361795	2015.550966	18.572160
42.166513	2020.872456	18.577178
42.384295	2009.790118	18.582195
42.087833	2010.632585	18.587213
42.405172	2014.456163	18.592231
42.618208	2006.739654	18.597248
42.490076	2014.868592	18.602266
42.589037	2007.230423	18.607283
42.639472	2010.321800	18.612301
42.473804	2004.242448	18.617319
42.751405	2000.381482	18.622336
42.682203	2013.572825	18.627354
42.557115	2010.713599	18.632371
42.762030	2015.940473	18.637389
42.739975	2019.852142	18.642407
42.789103	2004.524798	18.647424
42.626784	2010.263277	18.652442
42.812648	2010.567991	18.657459
42.909854	2013.238229	18.662477
42.959490	2007.023221	18.667495
43.127749	2002.126005	18.672512
43.046589	2006.659678	18.677530
42.904564	2002.050068	18.682547
43.032428	1998.432012	18.687565
42.778222	2006.649541	18.692583
42.834070	2005.365117	18.697600
42.720094	2028.062535	18.702618
42.978327	2031.874644	18.707635
43.146092	2041.751495	18.712653
43.170733	2045.675124	18.717671
43.493884	2036.234024	18.722688
43.223913	2042.197432	18.727706
43.499062	2038.549467	18.732723
43.470127	2036.309763	18.737741
43.450869	2041.084777	18.742759
43.925819	2047.724070	18.747776
43.679014	2056.837666	18.752794
44.022578	2060.775815	18.757811
44.108454	2048.419587	18.762829
43.759716	2039.531092	18.767847
44.073587	2028.533619	18.772864
43.935449	2044.808134	18.777882
44.046785	2036.590327	18.782899
43.984047	2037.435432	18.787917
43.781888	2039.786339	18.792935
43.946421	2048.186132	18.797952
43.993014	2061.244165	18.802970
44.025373	2058.575007	18.807987
44.132334	2060.492043	18.813005
43.829590	2063.834044	18.818023
44.264838	2052.215653	18.823040
43.961986	2061.142071	18.828058
44.179087	2060.975853	18.833075
44.398747	2063.627004	18.838093
44.264958	2085.743519	18.843111
44.907898	2091.265613	18.848128
44.585877	2089.389009	18.853146
44.645517	2088.735464	18.858163
44.818926	2090.062744	18.863181
44.566088	2086.322270	18.868199
45.025357	2089.630225	18.873216
44.784596	2100.421635	18.878234
44.786145	2088.652191	18.883251
44.923516	2089.119271	18.888269
44.824170	2092.837847	18.893287
45.086369	2085.225366	18.898304
45.022576	2086.712399	18.903322
44.940640	2090.827709	18.908339
45.228468	2083.908643	18.913357
45.177748	2085.671472	18.918375
45.411255	2086.468707	18.923392
45.360111	2089.830077	18.928410
45.026729	2086.358459	18.933427
45.234490	2074.845832	18.938445
45.372278	2081.376005	18.943463
45.363879	2074.479222	18.948480
45.128986	2075.422129	18.953498
45.066924	2086.081574	18.958515
45.239919	2075.286928	18.963533
45.202987	2093.771962	18.968551
45.399018	2098.119207	18.973568
45.714170	2106.540549	18.978586
46.007640	2090.758868	18.983603
45.841327	2088.518282	18.988621
45.923480	2098.062091	18.993639
45.995230	2083.842373	18.998656
45.719261	2101.439019	19.003674
45.959611	2094.738052	19.008691
46.354120	2088.752134	19.013709
46.199439	2092.476722	19.018727
46.597171	2088.619859	19.023744
46.328800	2102.034421	19.028762
46.304043	2088.683065	19.033779
46.536595	2078.180927	19.038797
46.374768	2065.637349	19.043815
45.978970	2059.830340	19.048832
46.294966	2079.406160	19.053850
46.571807	2085.951893	19.058867
46.481909	2094.797397	19.063885
46.190796	2095.173614	19.068903
46.596170	2082.608151	19.073920
46.217032	2091.721633	19.078938
46.312580	2091.170019	19.083955
46.738958	2086.306416	19.088973
46.491654	2095.532719	19.093991
46.349820	2091.266368	19.099008
46.281832	2093.052530	19.104026
46.544468	2111.875788	19.109043
46.869767	2120.866341	19.114061
46.502883	2128.305717	19.119079
46.615898	2121.690393	19.124096
46.734417	2122.353909	19.129114
46.754636	2120.866314	19.134131
47.057312	2128.751529	19.139149
47.033309	2138.482631	19.144167
46.945431	2141.079598	19.149184
46.901782	2149.978107	19.154202
47.366397	2148.382670	19.159219
47.442424	2148.721717	19.164237
47.082898	2147.879696	19.169255
47.339590	2140.648821	19.174272
47.176869	2143.802687	19.179290
47.141306	2152.560878	19.184307
47.736584	2174.851293	19.189325
47.880554	2177.756738	19.194343
47.956465	2181.458519	19.199360
48.104344	2179.396610	19.204378
47.818801	2182.169233	19.209395
48.105675	2176.384576	19.214413
47.910608	2183.601819	19.219431
48.309137	2166.111663	19.224448
48.202820	2155.844331	19.229466
48.043759	2151.219780	19.234483
48.263143	2132.621886	19.239501
47.928317	2127.822109	19.244519
47.983469	2141.939850	19.249536
47.781100	2156.076622	19.254554
48.159553	2160.079100	19.259571
48.305496	2159.995927	19.264589
48.089092	2161.288939	19.269607
48.004585	2155.589408	19.274624
48.252541	2153.946379	19.279642
48.252372	2158.803703	19.284659
48.485952	2158.223326	19.289677
48.432975	2169.459294	19.294695
48.321745	2185.123574	19.299712
48.480032	2190.244050	19.304730
48.247418	2194.102831	19.309747
48.431808	2191.231697	19.314765
48.379624	2194.572395	19.319783
48.870187	2184.907021	19.324800
48.843355	2188.088002	19.329818
48.960875	2207.162578	19.334835
49.478224	2203.137057	19.339853
49.411859	2201.187396	19.344871
49.338848	2185.399766	19.349888
49.307777	2189.584240	19.354906
48.848135	2183.595229	19.359923
48.922307	2183.877496	19.364941
49.026168	2198.783313	19.369959
49.012102	2207.485217	19.374976
49.398083	2213.473936	19.379994
49.209857	2217.973822	19.385011
49.683442	2216.824153	19.390029
49.285819	2218.870039	19.395047
49.738853	2214.113011	19.400064
49.638781	2211.913409	19.405082
49.545506	2215.673135	19.410099
49.428231	2202.562207	19.415117
49.298133	2224.499955	19.420135
49.645911	2235.458974	19.425152
49.834222	2241.311137	19.430170
49.972475	2244.593146	19.435187
50.172844	2235.043906	19.440205
50.248829	2238.636235	19.445223
50.442347	2239.469235	19.450240
50.320591	2233.465989	19.455258
50.334834	2234.657427	19.460275
50.745209	2228.554651	19.465293
50.155277	2230.621751	19.470311
50.159036	2237.179695	19.475328
50.618262	2229.100251	19.480346
50.241337	2236.760246	19.485363
50.402203	2232.556729	19.490381
50.341225	2237.107599	19.495399
50.428422	2238.056634	19.500416
50.349574	2229.518629	19.505434
50.451776	2236.102399	19.510451
50.719550	2253.526893	19.515469
50.931058	2263.761223	19.520487
50.997294	2265.229892	19.525504
50.905022	2261.412785	19.530522
50.706096	2263.313565	19.535539
50.901326	2266.016436	19.540557
51.338591	2261.250194	19.545575
51.022147	2263.018853	19.550592
51.357008	2261.995305	19.555610
51.280133	2265.131438	19.560627
51.260498	2253.899256	19.565645
51.314553	2255.654991	19.570663
50.921902	2251.756518	19.575680
51.491327	2258.728698	19.580698
51.458762	2256.569488	19.585715
51.761625	2246.332771	19.590733
51.593016	2251.707405	19.595751
51.631643	2254.524004	19.600768
51.949981	2251.762574	19.605786
51.641634	2251.778641	19.610803
51.796961	2249.276497	19.615821
51.429902	2243.257564	19.620839
51.322470	2246.789319	19.625856
52.158318	2260.667655	19.630874
52.085141	2270.951098	19.635891
52.427638	2260.273539	19.640909
52.093561	2253.052637	19.645927
51.950650	2245.629211	19.650944
51.942519	2253.626588	19.655962
51.808173	2263.190599	19.660979
52.068185	2272.297174	19.665997
51.959825	2266.714154	19.671015
52.051577	2275.744651	19.676032
52.327889	2268.123052	19.681050
52.112183	2274.726801	19.686067
52.650824	2272.563560	19.691085
52.245457	2270.074725	19.696103
52.287992	2288.967716	19.701120
52.920506	2296.626740	19.706138
52.682955	2307.955972	19.711155
52.907411	2298.257817	19.716173
53.272981	2301.397468	19.721191
52.805845	2302.602476	19.726208
52.892287	2295.453267	19.731226
52.897081	2302.035083	19.736243
53.545758	2302.103714	19.741261
52.839335	2302.783753	19.746279
52.733174	2302.795083	19.751296
53.176028	2298.174366	19.756314
53.155887	2304.604795	19.761331
53.427733	2297.059121	19.766349
53.409061	2299.350548	19.771367
53.005611	2301.604897	19.776384
53.393598	2291.500518	19.781402
53.142087	2317.605131	19.786419
53.450945	2321.560905	19.791437
53.384762	2323.475934	19.796455
53.035014	2333.620561	19.801472
53.380398	2330.049880	19.806490
53.779394	2335.141570	19.811507
53.722147	2329.256745	19.816525
53.817824	2339.674092	19.821543
53.901012	2357.855678	19.826560
54.122531	2355.478784	19.831578
53.886531	2367.324361	19.836595
54.254722	2367.771342	19.841613
54.352369	2360.221016	19.846631
54.266939	2358.783965	19.851648
54.028929	2362.201140	19.856666
54.348471	2360.490328	19.861683
54.268261	2351.781214	19.866701
54.522428	2352.535671	19.871719
54.161443	2365.676016	19.876736
54.572623	2349.442674	19.881754
54.491827	2350.228578	19.886771
54.739140	2352.123198	19.891789
54.772590	2355.772994	19.896807
54.763703	2360.771201	19.901824
54.874578	2348.798803	19.906842
54.802794	2348.363082	19.911859
54.824023	2360.964916	19.916877
55.038271	2366.737632	19.921895
55.047838	2380.752503	19.926912
54.954312	2380.743629	19.931930
54.966795	2378.226533	19.936947
55.310310	2370.798490	19.941965
55.713906	2373.710984	19.946983
55.203801	2370.517787	19.952000
55.424710	2374.804689	19.957018
55.281238	2376.515977	19.962035
55.255678	2380.316107	19.967053
55.440799	2366.784872	19.972071
55.497759	2377.210624	19.977088
55.533556	2377.303963	19.982106
55.346757	2378.355859	19.987123
55.356338	2384.699505	19.992141
55.578248	2375.357252	19.997159
55.278469	2392.347510	20.002176
55.558804	2399.997181	20.007194
55.889924	2411.987874	20.012211
55.980558	2400.402272	20.017229
55.587019	2401.656914	20.022247
55.752320	2407.318453	20.027264
55.943528	2410.066112	20.032282
56.152674	2424.209006	20.037299
56.348330	2429.145018	20.042317
56.464279	2423.193681	20.047335
56.585799	2436.216787	20.052352
56.577193	2427.399312	20.057370
56.535436	2421.313845	20.062387
56.454738	2433.744812	20.067405
56.619885	2429.759048	20.072423
56.415031	2440.631758	20.077440
56.481124	2422.875479	20.082458
56.303801	2417.217993	20.087475
56.593102	2418.298542	20.092493
56.408422	2429.845497	20.097511
56.506194	2444.423014	20.102528
56.759856	2446.265804	20.107546
56.775957	2451.337466	20.112563
56.978106	2458.232357	20.117581
57.068384	2453.879043	20.122599
57.034166	2455.497441	20.127616
57.162858	2472.636928	20.132634
57.175227	2479.538054	20.137651
56.963513	2484.865572	20.142669
57.484341	2480.068891	20.147687
57.669096	2485.266189	20.152704
57.776050	2482.425542	20.157722
57.786604	2476.775510	20.162739
57.264584	2474.410687	20.167757
57.972107	2475.559004	20.172775
57.539756	2481.101804	20.177792
57.940836	2478.909343	20.182810
57.825460	2468.330689	20.187827
57.905629	2475.788728	20.192845
58.161583	2472.569455	20.197863
57.884903	2490.257212	20.202880
58.434078	2493.838181	20.207898
58.400321	2501.770239	20.212915
58.538602	2506.614590	20.217933
58.577269	2498.216436	20.222951
58.207210	2491.302578	20.227968
58.626428	2488.088554	20.232986
58.856947	2499.817611	20.238003
58.867283	2496.090942	20.243021
58.682828	2474.141214	20.248039
58.395892	2480.588725	20.253056
58.772632	2489.774924	20.258074
58.855967	2494.987050	20.263091
58.913507	2498.161212	20.268109
59.107515	2495.716013	20.273127
58.683836	2505.647389	20.278144
58.811529	2493.381135	20.283162
59.005308	2500.209316	20.288179
58.791067	2493.423996	20.293197
59.170658	2496.058977	20.298215
59.371026	2498.642921	20.303232
59.234749	2500.921960	20.308250
59.244216	2494.049987	20.313267
59.069241	2502.364504	20.318285
59.123090	2499.334999	20.323303
59.144478	2502.771854	20.328320
59.129816	2509.188467	20.333338
59.454255	2515.692247	20.338355
59.704515	2527.797999	20.343373
59.683628	2516.230383	20.348391
59.271793	2520.646902	20.353408
59.394293	2518.481272	20.358426
59.489137	2541.322823	20.363443
59.209281	2559.037957	20.368461
59.953024	2541.024051	20.373479
59.973336	2556.610619	20.378496
60.170536	2566.227797	20.383514
60.098860	2573.593302	20.388531
60.170127	2575.414732	20.393549
60.463429	2569.806829	20.398567
60.354966	2577.760352	20.403584
60.896765	2580.415342	20.408602
60.703149	2580.629352	20.413619
60.799238	2572.576790	20.418637
61.018958	2561.142932	20.423655
60.589021	2575.450451	20.428672
60.801644	2577.000822	20.433690
60.714392	2576.087311	20.438707
60.849598	2576.987076	20.443725
60.944198	2566.726757	20.448743
60.999399	2579.184158	20.453760
60.967924	2569.631763	20.458778
60.776088	2563.960090	20.463795
60.689092	2569.354392	20.468813
61.214530	2590.424220	20.473831
61.379884	2598.882841	20.478848
61.319554	2593.201982	20.483866
61.599995	2599.431570	20.488883
61.385995	2597.694112	20.493901
61.452625	2608.134953	20.498919
61.360419	2599.426112	20.503936
61.471010	2604.786527	20.508954
61.809640	2588.521640	20.513971
61.536251	2600.576353	20.518989
61.843465	2597.163911	20.524007
61.955108	2614.956810	20.529024
61.647763	2625.860400	20.534042
62.068620	2624.639116	20.539059
61.701763	2630.076235	20.544077
62.222876	2625.825955	20.549095
61.990344	2633.038191	20.554112
62.135573	2632.779533	20.559130
62.529235	2623.670914	20.564147
62.027085	2632.301502	20.569165
62.424333	2643.901086	20.574183
62.419961	2658.315390	20.579200
62.761487	2656.474521	20.584218
62.871003	2646.568002	20.589235
62.942250	2658.623178	20.594253
63.010362	2644.824050	20.599271
62.862975	2648.631032	20.604288
62.723344	2655.032174	20.609306
63.150035	2642.106412	20.614323
62.774720	2650.152980	20.619341
63.237456	2639.358003	20.624359
63.175457	2653.100699	20.629376
63.058738	2649.332036	20.634394
63.298761	2640.296882	20.639411
63.043021	2646.965688	20.644429
63.270173	2656.155494	20.649447
63.569564	2667.151573	20.654464
63.625230	2672.528587	20.659482
63.794313	2677.571842	20.664499
63.578128	2681.372899	20.669517
63.498560	2672.322532	20.674535
63.770602	2678.212575	20.679552
63.665472	2671.868588	20.684570
63.985831	2670.222180	20.689587
63.730089	2682.631538	20.694605
63.741174	2677.770768	20.699623
64.012690	2673.620863	20.704640
63.870764	2678.077778	20.709658
64.505161	2679.125221	20.714675
64.474952	2687.099703	20.719693
64.318507	2679.763355	20.724711
64.206077	2670.771583	20.729728
64.504987	2695.250546	20.734746
64.440091	2692.340279	20.739763
64.406805	2703.383595	20.744781
64.821052	2696.566564	20.749799
64.673578	2702.415050	20.754816
64.580514	2704.885795	20.759834
65.142332	2699.227873	20.764851
64.940765	2690.121312	20.769869
64.711772	2700.893863	20.774887
65.005582	2693.569180	20.779904
64.722473	2702.172986	20.784922
65.015998	2717.917247	20.789939
65.025418	2730.243363	20.794957
65.323542	2732.324512	20.799975
65.263380	2725.110399	20.804992
65.230454	2727.956650	20.810010
65.463603	2724.558412	20.815027
65.515932	2720.647559	20.820045
65.473325	2724.452959	20.825063
65.777795	2752.943181	20.830080
65.760541	2753.722915	20.835098
66.028819	2754.801064	20.840115
65.689275	2754.864818	20.845133
65.835501	2756.606529	20.850151
65.996078	2754.457398	20.855168
65.875623	2755.073105	20.860186
65.870231	2749.674058	20.865203
65.939987	2755.701176	20.870221
66.202345	2768.618557	20.875239
66.356329	2778.372559	20.880256
66.117704	2788.432932	20.885274
66.179740	2774.914638	20.890291
66.212385	2779.787590	20.895309
66.251472	2776.175394	20.900327
66.523199	2794.026643	20.905344
66.659908	2804.132366	20.910362
66.925665	2808.713953	20.915379
66.891047	2812.210548	20.920397
66.987547	2816.929227	20.925415
66.971320	2810.093655	20.930432
67.197424	2806.534350	20.935450
67.061885	2807.368321	20.940467
66.691086	2801.863606	20.945485
67.157088	2803.989808	20.950503
67.763092	2814.602126	20.955520
67.269860	2818.305379	20.960538
67.635506	2820.740349	20.965555
67.959211	2823.281483	20.970573
67.571201	2825.999525	20.975591
67.813725	2816.052764	20.980608
67.866976	2829.235546	20.985626
68.083208	2815.769248	20.990643
68.075715	2825.348428	20.995661
68.003619	2819.956070	21.000679
68.279762	2821.557764	21.005696
67.872943	2824.399795	21.010714
68.221504	2818.291279	21.015731
68.172406	2821.730033	21.020749
67.988377	2826.214829	21.025767
68.442663	2822.824840	21.030784
68.096962	2827.109224	21.035802
68.342220	2820.671329	21.040819
68.180226	2822.693628	21.045837
68.219965	2824.469911	21.050855
68.898099	2828.136307	21.055872
68.646677	2852.159750	21.060890
68.759867	2850.401553	21.065907
68.643271	2851.543043	21.070925
68.945112	2853.102294	21.075943
69.011001	2850.964104	21.080960
68.662638	2854.179562	21.085978
69.050183	2838.422105	21.090995
68.937736	2851.766604	21.096013
69.196453	2873.395982	21.101031
69.594307	2871.669394	21.106048
69.593658	2879.168569	21.111066
69.510291	2870.767586	21.116083
69.307641	2884.017985	21.121101
69.474916	2879.056875	21.126119
70.071509	2877.161541	21.131136
69.881371	2883.886125	21.136154
69.932825	2883.534321	21.141171
69.704630	2878.739882	21.146189
69.813335	2887.604923	21.151207
70.037137	2887.856127	21.156224
69.933538	2901.183454	21.161242
70.250857	2903.525644	21.166259
69.991784	2908.215818	21.171277
69.934208	2916.846576	21.176295
70.300675	2905.612203	21.181312
70.127229	2918.288458	21.186330
70.279862	2909.691277	21.191347
70.479544	2926.404907	21.196365
70.537435	2922.039502	21.201383
70.909761	2935.404993	21.206400
70.446331	2933.789512	21.211418
71.064814	2923.919419	21.216435
71.348045	2920.527021	21.221453
70.945886	2929.686535	21.226471
71.102725	2920.775239	21.231488
70.619681	2929.111856	21.236506
70.929895	2946.044627	21.241523
71.324034	2957.604406	21.246541
71.077582	2959.109561	21.251559
71.319149	2946.794959	21.256576
71.398666	2949.832098	21.261594
71.677924	2946.083630	21.266611
71.871977	2943.911606	21.271629
71.951935	2955.527737	21.276647
71.991941	2940.959315	21.281664
71.843809	2954.811034	21.286682
71.993366	2959.802884	21.291699
72.476216	2973.404853	21.296717
72.312791	2984.602211	21.301735
72.457314	2963.429282	21.306752
72.306467	2972.466887	21.311770
72.339232	2969.188792	21.316787
72.493181	2968.165628	21.321805
72.178413	2974.346666	21.326823
72.913632	2970.608922	21.331840
72.468434	2971.967050	21.336858
72.528491	2962.088208	21.341875
72.759920	2966.412118	21.346893
72.559639	2967.457621	21.351911
72.451417	2966.108152	21.356928
72.855972	2968.267782	21.361946
72.479970	2967.758389	21.366963
72.558305	2991.078570	21.371981
72.922872	2999.311099	21.376999
73.034944	2998.293687	21.382016
72.904516	3014.011193	21.387034
73.091944	3007.852506	21.392051
73.480011	3032.127455	21.397069
73.579515	3039.951099	21.402087
73.694950	3022.682076	21.407104
73.628103	3027.505825	21.412122
73.648005	3030.328422	21.417139
74.341985	3016.075303	21.422157
74.368136	3026.645973	21.427175
74.501470	3018.602764	21.432192
74.101230	3017.192578	21.437210
74.040242	3015.050569	21.442227
74.150709	3011.685183	21.447245
74.424302	3017.803072	21.452263
74.383955	3015.949403	21.457280
74.161860	3016.250030	21.462298
74.174770	3016.595611	21.467315
74.358435	3015.182845	21.472333
74.219747	3036.401438	21.477351
74.522734	3036.240286	21.482368
74.613533	3050.558872	21.487386
74.614100	3049.521727	21.492403
74.957733	3045.481842	21.497421
74.913720	3055.240059	21.502439
74.928925	3066.454359	21.507456
74.951239	3076.461867	21.512474
74.947363	3078.330841	21.517491
75.099507	3076.856747	21.522509
74.923660	3077.859625	21.527527
75.091933	3083.510683	21.532544
75.580606	3094.362721	21.537562
75.682042	3102.130953	21.542579
75.905013	3101.740901	21.547597
75.839965	3106.387589	21.552615
75.843968	3099.825732	21.557632
75.793116	3107.512087	21.562650
75.879187	3102.853749	21.567667
75.967279	3099.277856	21.572685
76.251162	3093.316965	21.577703
76.604965	3088.218594	21.582720
76.343069	3086.970551	21.587738
76.506322	3096.721643	21.592755
76.188240	3097.711062	21.597773
76.832871	3117.756266	21.602791
76.853615	3117.072502	21.607808
76.851384	3108.794977	21.612826
76.943065	3113.810241	21.617843
77.348260	3113.423090	21.622861
77.250663	3108.723108	21.627879
77.246730	3103.344171	21.632896
77.306037	3089.185445	21.637914
77.039441	3088.997333	21.642931
77.325516	3099.802206	21.647949
77.454511	3104.074999	21.652967
77.441773	3109.168188	21.657984
77.095750	3110.724492	21.663002
77.156897	3109.397758	21.668019
77.479444	3104.794761	21.673037
77.498543	3106.604417	21.678055
77.657001	3102.900326	21.683072
77.486384	3107.452280	21.688090
77.598240	3123.027800	21.693107
78.100532	3134.296549	21.698125
77.935298	3149.183260	21.703143
78.125005	3132.885376	21.708160
78.122553	3148.217225	21.713178
78.217023	3150.920399	21.718195
78.469926	3137.066221	21.723213
78.159392	3136.497157	21.728231
78.290795	3130.746162	21.733248
78.308941	3148.025574	21.738266
78.286019	3165.361022	21.743283
78.406695	3169.805700	21.748301
78.442030	3168.055241	21.753319
78.516104	3172.330847	21.758336
78.814629	3180.218468	21.763354
78.827410	3185.541336	21.768371
78.759466	3191.067356	21.773389
79.043828	3197.458757	21.778407
79.332187	3196.520027	21.783424
79.024177	3187.022492	21.788442
79.047207	3206.148980	21.793459
79.589136	3209.018649	21.798477
79.246801	3213.587648	21.803495
79.489145	3217.966126	21.808512
79.972139	3217.036904	21.813530
79.910486	3217.814169	21.818547
80.445509	3211.702189	21.823565
79.537389	3221.307102	21.828583
79.751582	3221.472887	21.833600
80.181256	3235.336673	21.838618
80.034877	3245.882903	21.843635
80.202609	3241.839808	21.848653
80.219918	3248.912128	21.853671
80.223063	3238.228672	21.858688
80.196191	3247.201414	21.863706
80.369848	3268.295368	21.868723
80.799580	3270.915095	21.873741
80.521936	3273.430666	21.878759
80.624717	3270.238563	21.883776
80.967698	3265.612056	21.888794
80.962161	3271.271880	21.893811
81.394039	3280.525805	21.898829
81.350357	3290.097874	21.903847
81.825307	3298.177626	21.908864
81.952595	3283.042799	21.913882
81.448453	3268.780335	21.918899
81.896331	3265.908297	21.923917
81.794827	3265.848768	21.928935
81.562207	3260.082008	21.933952
81.507411	3263.858452	21.938970
81.801354	3285.391615	21.943987
82.056314	3282.138875	21.949005
82.075127	3285.975584	21.954023
81.981792	3280.871653	21.959040
82.235911	3268.690562	21.964058
82.431032	3279.904361	21.969075
82.644261	3275.159163	21.974093
82.558386	3282.982125	21.979111
82.331342	3270.997250	21.984128
82.728886	3283.178427	21.989146
82.386638	3282.824473	21.994163
82.708221	3288.943185	21.999181
82.622741	3296.168781	22.004199
82.585943	3301.686927	22.009216
82.921732	3302.224354	22.014234
82.533635	3303.108043	22.019251
82.979807	3302.506995	22.024269
82.975967	3320.899411	22.029287
83.211519	3318.042440	22.034304
83.436702	3328.345688	22.039322
83.574046	3326.670456	22.044339
83.553653	3321.681219	22.049357
83.861048	3335.909079	22.054375
83.535775	3337.570248	22.059392
84.149147	3324.994159	22.064410
83.654848	3330.879437	22.069427
83.941679	3312.179988	22.074445
83.733337	3326.375899	22.079463
83.946939	3337.647710	22.084480
84.049068	3346.925957	22.089498
83.825236	3362.273409	22.094515
84.125629	3346.620041	22.099533
84.245226	3360.994779	22.104551
84.319338	3383.071226	22.109568
84.709373	3384.637191	22.114586
84.847991	3380.396103	22.119603
85.010256	3382.094280	22.124621
85.029878	3391.400783	22.129639
84.838979	3379.803978	22.134656
85.234072	3376.896561	22.139674
84.804721	3393.090762	22.144691
85.250551	3381.859052	22.149709
85.282685	3394.526065	22.154727
85.282647	3410.664948	22.159744
85.503269	3409.072387	22.164762
85.712773	3415.397524	22.169779
85.832635	3412.474248	22.174797
85.587930	3417.039345	22.179815
85.560994	3413.992722	22.184832
85.665243	3402.204888	22.189850
85.749866	3427.486317	22.194867
85.931370	3437.976025	22.199885
86.163461	3444.194272	22.204903
86.043867	3441.250790	22.209920
86.103129	3447.250383	22.214938
86.395166	3449.046386	22.219955
86.281489	3454.673388	22.224973
86.369155	3457.170632	22.229991
86.484986	3466.415575	22.235008
86.812812	3456.392072	22.240026
86.480837	3471.068087	22.245043
86.599356	3470.180695	22.250061
86.769110	3481.895748	22.255079
86.935897	3493.960950	22.260096
87.166563	3494.051562	22.265114
87.167412	3504.382228	22.270131
87.332953	3495.699508	22.275149
87.345127	3503.856780	22.280167
87.668664	3520.739933	22.285184
88.165616	3514.959771	22.290202
87.820324	3511.867798	22.295219
87.797410	3523.450197	22.300237
88.011082	3524.740225	22.305255
88.088150	3516.833257	22.310272
88.703108	3518.141103	22.315290
88.330084	3522.631009	22.320307
88.374681	3512.909122	22.325325
88.351697	3508.017116	22.330343
88.616781	3512.078096	22.335360
88.631156	3507.336617	22.340378
88.689295	3507.067167	22.345395
88.694762	3505.937437	22.350413
89.028152	3506.620562	22.355431
89.003848	3515.526095	22.360448
89.138702	3507.109899	22.365466
88.977433	3515.334876	22.370483
88.693738	3504.999162	22.375501
88.790455	3520.248806	22.380519
88.934506	3539.026489	22.385536
88.864261	3534.961298	22.390554
88.836916	3538.271788	22.395571
89.567635	3560.594140	22.400589
89.234860	3572.010138	22.405607
89.402402	3566.675099	22.410624
89.969984	3564.206075	22.415642
89.832243	3573.768692	22.420659
89.876529	3568.663929	22.425677
90.301695	3586.527694	22.430695
89.811120	3593.437382	22.435712
90.233107	3603.046726	22.440730
90.202469	3595.404828	22.445747
90.279347	3601.178700	22.450765
90.127986	3587.694643	22.455783
90.336886	3611.842662	22.460800
90.526861	3620.028043	22.465818
90.254148	3622.699565	22.470835
90.656512	3618.998675	22.475853
91.122268	3629.889140	22.480871
90.995076	3648.655166	22.485888
91.418958	3645.512196	22.490906
91.503815	3647.488609	22.495923
91.502651	3649.710790	22.500941
91.495178	3648.737937	22.505959
91.461309	3651.729805	22.510976
91.530151	3646.404388	22.515994
91.718364	3644.507287	22.521011
91.567504	3647.800059	22.526029
91.756754	3653.896727	22.531047
91.628097	3666.591370	22.536064
92.009616	3666.419574	22.541082
92.072672	3659.978824	22.546099
92.054959	3678.985060	22.551117
92.133817	3683.992000	22.556135
92.353827	3700.238073	22.561152
92.662255	3696.346786	22.566170
92.699988	3695.432595	22.571187
92.952962	3700.954089	22.576205
93.085795	3696.879249	22.581223
92.594084	3708.685490	22.586240
92.838891	3698.522410	22.591258
93.392752	3697.729481	22.596275
93.256244	3707.012803	22.601293
93.903555	3722.143128	22.606311
93.295922	3713.813140	22.611328
93.694387	3716.349922	22.616346
93.568390	3725.331081	22.621363
93.743398	3721.763100	22.626381
93.954812	3716.920419	22.631399
93.707968	3718.331601	22.636416
93.959807	3715.688820	22.641434
93.967314	3709.237166	22.646451
93.914434	3709.785019	22.651469
93.833364	3738.060920	22.656487
93.975748	3753.632408	22.661504
94.269865	3750.703055	22.666522
94.094438	3746.257139	22.671539
94.359870	3758.093978	22.676557
94.607138	3771.945919	22.681575
94.393627	3771.634424	22.686592
94.599621	3766.395327	22.691610
94.623558	3771.398788	22.696627
94.572764	3786.003733	22.701645
95.165420	3800.094614	22.706663
95.040184	3806.646225	22.711680
95.344337	3794.573388	22.716698
95.154023	3800.882193	22.721715
95.056400	3812.785881	22.726733
95.440342	3810.230281	22.731751
95.484567	3819.887739	22.736768
95.739454	3829.212248	22.741786
96.073200	3823.638156	22.746803
96.091105	3822.475237	22.751821
95.945856	3820.129715	22.756839
96.105420	3827.530367	22.761856
96.487509	3837.032666	22.766874
96.326340	3843.184279	22.771891
96.400269	3853.430623	22.776909
96.559877	3851.836701	22.781927
96.332554	3857.782314	22.786944
96.541406	3856.189295	22.791962
96.358111	3856.007065	22.796979
96.839390	3872.736510	22.801997
97.271648	3876.376149	22.807015
97.158389	3881.678780	22.812032
97.300929	3879.799845	22.817050
97.705189	3874.526703	22.822067
97.593197	3880.778077	22.827085
97.972331	3872.123573	22.832103
97.542651	3883.985430	22.837120
97.500282	3874.026896	22.842138
97.520959	3895.449038	22.847155
97.626862	3908.268449	22.852173
97.745154	3894.345722	22.857191
97.800760	3903.978902	22.862208
98.197044	3912.066488	22.867226
98.198475	3933.952566	22.872243
98.200804	3942.042395	22.877261
98.589296	3937.067950	22.882279
98.746512	3945.479431	22.887296
98.539432	3931.909407	22.892314
98.718568	3943.138143	22.897331
98.857556	3967.051793	22.902349
99.082809	3966.121501	22.907367
99.101815	3970.945107	22.912384
99.185101	3965.103728	22.917402
99.452300	3959.288601	22.922419
99.239041	3962.413396	22.927437
99.495567	3968.944390	22.932455
99.764919	3989.842344	22.937472
100.000358	3996.438267	22.942490
100.138481	3993.604001	22.947507
99.822129	3995.092080	22.952525
100.177969	3998.144705	22.957543
99.918776	3993.061702	22.962560
100.208163	3984.561387	22.967578
100.443169	3983.842109	22.972595
100.097031	3991.878621	22.977613
100.526426	4010.390693	22.982631
100.502264	4020.993204	22.987648
100.745640	4018.754197	22.992666
100.840661	4014.584340	22.997683
100.685910	4025.033646	23.002701
100.906150	4017.036176	23.007719
100.690873	4027.360051	23.012736
100.727865	4036.817627	23.017754
101.336070	4044.282702	23.022771
100.985358	4052.231012	23.027789
100.994076	4046.813824	23.032807
101.353107	4071.181826	23.037824
101.696244	4067.657594	23.042842
101.976398	4078.253070	23.047859
101.743091	4080.817340	23.052877
101.977755	4065.634449	23.057895
102.348956	4071.566094	23.062912
102.151294	4081.981591	23.067930
102.572393	4067.793973	23.072947
102.609009	4076.546802	23.077965
102.664413	4075.008307	23.082983
102.698075	4082.179492	23.088000
102.581548	4096.890112	23.093018
103.139512	4098.539784	23.098035
102.679974	4102.051895	23.103053
103.296578	4095.207847	23.108071
103.180025	4098.797835	23.113088
103.159562	4099.012330	23.118106
103.606158	4103.910871	23.123123
103.034352	4100.552298	23.128141
103.348785	4114.377278	23.133159
103.515611	4130.556214	23.138176
103.821539	4122.193266	23.143194
103.993308	4126.099358	23.148211
103.610515	4135.135083	23.153229
103.937485	4125.820467	23.158247
104.233725	4134.688634	23.163264
104.050768	4149.287448	23.168282
104.294375	4147.663445	23.173299
104.309240	4148.876189	23.178317
104.405098	4143.122441	23.183335
104.518346	4156.299557	23.188352
104.773234	4165.325795	23.193370
105.150307	4165.877684	23.198387
104.759115	4171.691465	23.203405
104.948327	4171.809818	23.208423
105.030705	4161.927705	23.213440
104.924427	4174.182762	23.218458
105.381604	4193.669351	23.223475
105.222184	4195.563031	23.228493
105.437490	4196.962312	23.233511
105.315640	4201.241501	23.238528
105.338550	4226.935685	23.243546
105.810542	4230.672390	23.248563
105.889879	4228.905471	23.253581
106.177252	4233.357110	23.258599
106.233479	4241.735069	23.263616
106.353307	4256.104291	23.268634
106.394651	4254.187728	23.273651
106.633202	4267.243387	23.278669
106.826314	4249.340757	23.283687
106.938513	4258.688361	23.288704
106.714190	4263.893347	23.293722
107.177367	4255.164079	23.298739
106.958655	4270.361937	23.303757
107.484929	4276.999604	23.308775
107.349212	4284.749413	23.313792
107.508162	4286.721121	23.318810
107.643708	4284.930713	23.323827
107.451647	4293.547481	23.328845
107.523993	4282.922733	23.333863
107.771558	4291.252500	23.338880
107.488396	4301.422412	23.343898
108.185709	4317.727917	23.348915
108.130589	4314.965753	23.353933
108.088938	4317.944861	23.358951
108.517375	4323.273324	23.363968
108.453695	4331.887757	23.368986
108.650871	4336.847358	23.374003
108.735326	4353.477246	23.379021
108.828548	4349.169779	23.384039
108.650036	4346.183903	23.389056
108.633084	4347.455484	23.394074
109.009707	4345.195158	23.399091
108.624467	4362.066631	23.404109
109.190932	4369.361578	23.409127
109.242388	4374.444548	23.414144
109.072121	4380.969201	23.419162
109.290527	4387.883126	23.424179
109.519136	4402.299050	23.429197
109.773476	4399.411605	23.434215
109.925588	4395.164466	23.439232
110.078224	4395.862206	23.444250
110.019935	4405.237338	23.449267
110.382391	4428.272810	23.454285
110.548052	4429.007772	23.459303
110.696761	4426.090559	23.464320
110.591719	4426.901055	23.469338
110.778144	4424.875395	23.474355
110.847297	4437.585949	23.479373
111.087345	4442.007682	23.484391
111.209413	4455.220603	23.489408
111.464956	4463.907473	23.494426
111.423214	4452.035919	23.499443
111.594970	4452.148501	23.504461
111.686116	4460.236492	23.509479
111.861671	4454.273337	23.514496
111.766278	4450.030149	23.519514
111.822317	4451.359743	23.524531
111.998608	4462.459379	23.529549
112.003485	4471.472847	23.534567
112.422880	4486.370738	23.539584
111.862706	4491.171480	23.544602
112.077718	4479.955158	23.549619
112.341494	4498.172338	23.554637
112.217825	4507.113392	23.559655
112.444689	4516.526432	23.564672
112.243558	4531.223902	23.569690
112.616693	4535.854377	23.574707
112.847766	4543.673528	23.579725
113.167355	4555.455146	23.584743
113.162765	4555.214966	23.589760
113.368963	4579.040454	23.594778
113.548633	4573.541226	23.599795
113.394464	4583.730914	23.604813
113.915768	4576.884327	23.609831
114.107130	4575.676094	23.614848
113.797533	4591.442169	23.619866
114.394166	4589.409212	23.624883
114.620329	4592.233772	23.629901
114.661157	4593.652528	23.634919
114.820897	4586.145981	23.639936
114.791383	4589.547620	23.644954
115.099127	4580.058721	23.649971
115.061095	4590.946643	23.654989
115.063350	4585.117663	23.660007
114.797459	4578.668391	23.665024
114.661203	4597.748920	23.670042
115.043415	4603.941200	23.675059
115.306963	4610.394121	23.680077
115.246108	4620.784171	23.685095
115.753334	4626.346985	23.690112
115.649160	4651.987300	23.695130
115.767571	4641.090854	23.700147
115.943606	4646.206051	23.705165
115.862914	4660.819908	23.710183
115.738230	4644.509115	23.715200
115.727937	4661.519653	23.720218
116.191413	4671.827649	23.725235
116.190226	4678.867055	23.730253
116.549426	4685.172647	23.735271
117.028258	4692.307420	23.740288
116.932133	4707.982350	23.745306
117.257522	4697.276049	23.750323
117.099504	4700.535964	23.755341
117.016190	4700.946737	23.760359
117.202886	4691.824338	23.765376
117.175456	4703.866712	23.770394
117.722464	4707.521021	23.775411
118.009466	4717.031333	23.780429
117.756700	4721.300836	23.785447
118.121222	4715.403165	23.790464
117.858293	4730.288252	23.795482
118.034191	4719.669691	23.800499
118.097576	4720.397187	23.805517
118.508230	4737.720864	23.810535
118.896501	4752.606048	23.815552
118.550059	4751.157647	23.820570
118.610615	4757.128388	23.825587
118.657024	4755.195174	23.830605
119.026416	4751.807418	23.835623
119.153857	4767.094141	23.840640
119.311372	4776.358945	23.845658
119.415487	4778.197246	23.850675
119.523430	4784.760272	23.855693
119.198612	4790.727101	23.860711
119.704012	4782.174054	23.865728
119.619126	4803.141194	23.870746
119.703166	4806.696555	23.875763
119.792990	4796.066205	23.880781
119.934790	4810.964688	23.885799
120.127559	4828.044168	23.890816
120.253117	4836.937845	23.895834
120.434229	4833.730095	23.900851
120.591964	4839.473710	23.905869
120.707809	4846.501689	23.910887
120.982870	4852.106961	23.915904
121.169713	4860.628225	23.920922
121.335852	4864.481881	23.925939
121.296664	4859.898499	23.930957
121.334812	4859.640213	23.935975
121.742918	4852.772872	23.940992
121.513593	4868.716523	23.946010
121.633795	4880.305367	23.951027
121.812928	4889.665104	23.956045
121.925939	4897.480354	23.961063
122.253824	4897.677349	23.966080
122.174145	4899.272023	23.971098
122.277936	4908.619831	23.976115
122.450179	4913.751496	23.981133
122.575967	4916.240693	23.986151
122.647410	4911.139662	23.991168
122.734935	4920.258626	23.996186
122.963648	4938.371862	24.001203
123.058243	4945.071051	24.006221
122.772871	4944.200046	24.011239
123.006391	4940.998561	24.016256
123.120087	4962.447316	24.021274
123.107549	4971.059931	24.026291
123.215589	4979.073723	24.031309
123.534092	4998.272397	24.036327
123.717525	5010.688055	24.041344
123.828182	5013.779902	24.046362
124.100033	5005.122854	24.051379
124.797626	5014.414152	24.056397
124.677257	5020.573249	24.061415
124.711088	5019.204412	24.066432
124.914553	5013.707393	24.071450
125.023188	5019.546624	24.076467
125.124186	5015.270766	24.081485
124.932960	5017.170596	24.086503
125.289363	5013.392726	24.091520
125.374171	5016.744814	24.096538
125.602492	5016.960659	24.101555
125.551708	5012.724109	24.106573
125.517211	5031.964731	24.111591
125.736653	5033.197227	24.116608
125.758348	5049.896522	24.121626
125.615481	5047.728411	24.126643
126.410927	5051.319618	24.131661
125.967234	5072.823005	24.136679
126.143562	5069.538030	24.141696
126.098456	5077.427590	24.146714
126.313132	5089.390008	24.151731
126.828938	5101.139549	24.156749
126.612374	5119.742558	24.161767
126.749480	5113.060163	24.166784
126.705054	5117.047979	24.171802
127.090012	5133.792754	24.176819
127.338395	5128.811209	24.181837
127.313640	5139.668958	24.186855
127.782270	5148.276037	24.191872
127.780345	5166.959338	24.196890
127.998044	5161.907256	24.201907
128.347556	5156.142645	24.206925
128.406270	5167.779685	24.211943
128.438993	5162.030506	24.216960
128.287319	5170.012576	24.221978
128.179368	5183.505981	24.226995
128.814501	5184.448354	24.232013
129.000861	5197.222024	24.237031
128.727927	5191.522654	24.242048
129.066672	5207.814425	24.247066
129.086427	5211.508896	24.252083
129.337942	5217.730149	24.257101
129.438188	5219.380911	24.262119
129.659634	5227.790322	24.267136
129.746673	5234.143562	24.272154
129.926038	5235.830844	24.277171
130.352555	5235.543691	24.282189
130.338769	5238.074163	24.287207
130.646675	5243.690677	24.292224
130.533424	5238.741408	24.297242
130.352001	5240.768805	24.302259
130.921950	5247.044458	24.307277
130.760716	5268.232779	24.312295
130.988154	5267.246922	24.317312
131.042485	5273.088937	24.322330
131.112180	5269.047381	24.327347
131.407529	5287.631989	24.332365
131.230204	5293.973104	24.337383
131.404168	5289.813468	24.342400
131.712590	5299.115814	24.347418
131.726464	5317.143769	24.352435
131.812025	5325.419001	24.357453
131.912671	5333.801214	24.362471
132.008231	5327.884053	24.367488
132.264137	5328.098487	24.372506
132.536996	5338.663734	24.377523
132.805648	5339.340734	24.382541
132.602592	5363.935335	24.387559
132.872768	5353.372411	24.392576
133.111169	5351.088364	24.397594
132.975059	5369.290065	24.402611
133.413875	5367.601329	24.407629
133.689151	5376.103506	24.412647
133.676987	5374.899771	24.417664
133.527760	5375.340375	24.422682
133.793781	5373.308507	24.427699
133.740118	5362.584969	24.432717
133.980952	5395.844423	24.437735
134.086291	5391.378724	24.442752
134.126157	5394.899789	24.447770
134.236442	5395.378549	24.452787
134.888920	5406.114116	24.457805
134.728070	5428.630466	24.462823
134.805825	5436.297452	24.467840
134.774521	5434.433729	24.472858
134.757161	5428.025655	24.477875
135.090084	5441.357288	24.482893
134.942082	5447.914923	24.487911
135.101987	5454.537358	24.492928
135.506330	5470.327082	24.497946
135.422400	5484.093999	24.502963
135.972560	5472.858502	24.507981
135.739299	5494.418194	24.512999
136.024107	5505.704587	24.518016
136.122305	5498.345626	24.523034
136.329560	5508.177571	24.528051
137.124246	5529.104799	24.533069
136.999529	5535.939787	24.538087
136.886075	5545.323942	24.543104
137.211419	5536.975937	24.548122
137.063539	5539.517632	24.553139
137.293112	5542.007073	24.558157
137.412646	5551.119528	24.563175
137.659203	5566.466852	24.568192
137.548593	5569.468640	24.573210
137.530656	5570.950770	24.578227
138.176103	5583.271485	24.583245
137.935621	5604.922309	24.588263
138.034827	5598.908356	24.593280
138.096643	5602.024158	24.598298
137.869791	5613.869477	24.603315
138.606892	5631.160570	24.608333
138.584487	5629.207139	24.613351
138.078374	5647.804363	24.618368
139.134136	5657.015480	24.623386
139.278461	5665.562335	24.628403
139.944732	5672.973691	24.633421
139.792474	5679.593559	24.638439
139.891993	5687.937554	24.643456
140.442505	5685.599423	24.648474
140.234881	5688.876417	24.653491
140.221817	5682.020169	24.658509
140.503070	5682.120148	24.663527
140.517407	5681.746862	24.668544
140.474834	5682.602211	24.673562
140.614800	5696.322004	24.678579
140.659377	5704.030056	24.683597
140.847288	5719.897608	24.688615
141.134769	5709.446573	24.693632
141.471406	5726.421298	24.698650
141.635009	5739.411041	24.703667
141.690210	5731.820446	24.708685
141.727753	5748.273699	24.713703
142.032544	5745.725782	24.718720
142.301535	5740.489388	24.723738
141.747335	5740.711149	24.728755
141.933963	5744.968036	24.733773
142.079828	5765.060234	24.738791
142.318385	5761.763239	24.743808
142.681899	5770.390427	24.748826
142.610489	5765.979877	24.753843
142.989937	5776.938115	24.758861
143.173953	5791.535184	24.763879
143.382769	5789.127593	24.768896
143.770867	5790.650422	24.773914
143.321219	5798.782168	24.778931
143.677778	5790.361129	24.783949
144.039752	5796.701368	24.788967
143.665447	5796.087620	24.793984
144.099399	5807.233759	24.799002
143.994960	5828.148001	24.804019
144.092565	5817.069888	24.809037
144.370748	5830.922074	24.814055
144.105932	5846.212566	24.819072
144.353850	5853.453838	24.824090
144.571600	5864.464112	24.829107
144.742426	5878.156901	24.834125
145.005396	5881.092958	24.839143
144.666876	5895.627776	24.844160
145.264753	5890.919717	24.849178
145.268528	5901.764602	24.854195
145.732818	5907.457066	24.859213
145.952139	5928.529707	24.864231
145.836709	5933.562837	24.869248
145.797626	5934.231743	24.874266
145.939799	5948.760273	24.879283
146.393830	5954.371754	24.884301
146.531214	5953.033736	24.889319
146.213253	5973.889007	24.894336
146.959074	5993.176458	24.899354
146.889119	5993.895373	24.904371
146.884352	6000.779225	24.909389
147.171338	6018.523326	24.914407
147.138273	6021.397367	24.919424
147.695418	6023.398672	24.924442
148.199263	6048.749196	24.929459
148.189693	6048.557863	24.934477
148.474862	6058.374102	24.939495
148.434304	6051.389925	24.944512
148.926282	6038.747518	24.949530
148.752811	6052.617179	24.954547
148.564704	6058.203478	24.959565
148.931590	6067.803774	24.964583
148.744611	6073.753774	24.969600
149.222621	6064.254704	24.974618
149.257457	6078.434092	24.979635
149.745202	6097.246930	24.984653
149.614418	6105.126770	24.989671
149.895481	6111.917665	24.994688
149.896540	6106.625483	24.999706
149.905861	6120.390903	25.004723
149.910246	6133.662523	25.009741
150.346161	6135.320819	25.014759
150.227619	6145.703307	25.019776
150.770377	6151.337974	25.024794
150.664391	6166.457554	25.029811
150.812028	6155.968732	25.034829
150.980370	6176.466511	25.039847
151.035969	6199.534904	25.044864
151.288795	6198.080087	25.049882
151.114424	6213.470952	25.054899
151.362493	6225.284568	25.059917
151.567751	6231.791916	25.064935
151.537454	6234.297713	25.069952
151.917042	6245.713082	25.074970
152.194727	6254.279921	25.079987
152.337782	6256.478200	25.085005
152.671017	6263.331409	25.090023
152.632387	6290.104022	25.095040
153.171607	6288.193787	25.100058
153.435043	6287.096367	25.105075
153.516360	6283.479526	25.110093
154.132013	6281.550336	25.115111
153.665272	6279.654637	25.120128
153.966143	6275.423325	25.125146
153.993246	6279.153061	25.130163
154.060708	6278.987566	25.135181
153.832365	6289.070910	25.140199
153.912431	6304.096020	25.145216
154.410493	6307.936822	25.150234
154.333564	6322.725659	25.155251
154.366258	6337.759432	25.160269
154.457394	6342.710445	25.165287
154.847335	6356.471340	25.170304
155.097326	6355.015404	25.175322
154.892899	6364.267028	25.180339
155.166124	6384.064829	25.185357
155.619029	6387.592558	25.190375
155.617641	6398.926188	25.195392
155.780147	6400.840866	25.200410
156.397094	6412.274556	25.205427
156.483898	6409.119124	25.210445
156.566973	6407.785334	25.215463
157.107757	6422.184506	25.220480
157.127514	6422.372682	25.225498
157.219788	6418.266447	25.230515
157.307295	6431.748245	25.235533
157.475580	6442.294528	25.240551
157.521796	6443.540853	25.245568
157.752328	6443.982410	25.250586
157.742433	6440.614565	25.255603
157.420681	6461.600277	25.260621
157.697072	6466.560041	25.265639
157.783334	6480.015306	25.270656
158.108799	6491.003459	25.275674
158.406961	6502.691630	25.280691
158.768001	6504.115830	25.285709
159.090680	6514.861866	25.290727
158.889763	6533.141007	25.295744
158.814950	6534.035608	25.300762
159.039421	6539.517537	25.305779
159.190555	6561.859395	25.310797
159.763070	6554.669526	25.315815
159.645410	6576.144597	25.320832
159.996207	6573.477089	25.325850
160.072347	6590.787302	25.330867
160.371019	6595.807218	25.335885
160.897467	6588.884097	25.340903
160.420355	6593.422810	25.345920
160.939187	6610.321064	25.350938
161.112131	6626.414122	25.355955
160.927471	6625.321553	25.360973
161.309766	6613.529399	25.365991
161.334967	6624.129422	25.371008
161.646005	6641.516586	25.376026
161.930927	6653.497705	25.381043
161.773148	6655.375649	25.386061
162.167872	6643.095433	25.391079
161.775951	6675.968482	25.396096
162.111636	6680.254505	25.401114
162.362705	6676.543308	25.406131
162.796350	6691.102242	25.411149
162.488275	6700.442110	25.416167
162.479862	6707.905799	25.421184
163.054967	6713.077688	25.426202
163.275434	6732.608980	25.431219
163.390369	6739.148032	25.436237
163.429263	6736.657373	25.441255
163.583400	6753.657904	25.446272
163.901215	6768.120300	25.451290
164.311627	6765.253853	25.456307
163.942453	6770.671888	25.461325
164.251261	6783.948000	25.466343
164.195178	6802.394873	25.471360
164.645448	6803.253754	25.476378
165.010254	6806.968663	25.481395
164.641230	6827.946142	25.486413
165.220985	6814.919177	25.491431
165.493965	6823.152350	25.496448
165.515624	6838.004110	25.501466
165.580572	6835.274399	25.506483
165.797783	6845.389876	25.511501
165.961074	6861.762816	25.516519
166.414410	6872.975816	25.521536
166.412545	6870.359556	25.526554
166.507963	6878.722188	25.531571
166.586503	6897.505270	25.536589
166.860357	6902.663296	25.541607
166.842594	6913.767643	25.546624
167.199929	6914.295344	25.551642
167.360622	6929.023350	25.556659
167.408321	6933.609962	25.561677
167.764223	6945.879653	25.566695
167.870115	6969.155871	25.571712
168.119312	6969.091823	25.576730
168.453716	6966.727066	25.581747
168.251559	6974.747543	25.586765
168.718747	6979.655402	25.591783
169.089220	6987.239234	25.596800
169.253129	6986.411088	25.601818
169.518478	6988.035491	25.606835
169.147539	6999.937203	25.611853
169.542889	7011.297743	25.616871
169.637070	7034.935963	25.621888
169.786897	7021.472748	25.626906
170.030237	7028.053675	25.631923
169.943384	7049.416374	25.636941
170.271934	7041.889384	25.641959
170.545343	7045.499755	25.646976
170.378663	7073.611089	25.651994
170.482983	7077.900080	25.657011
170.767787	7078.279898	25.662029
171.294681	7106.778212	25.667047
171.120669	7117.766788	25.672064
171.389641	7108.960993	25.677082
171.987226	7130.041136	25.682100
171.566393	7149.586956	25.687117
171.908042	7131.947920	25.692135
171.955204	7150.746736	25.697152
172.451527	7159.218007	25.702170
172.604386	7169.875241	25.707188
172.556270	7179.915131	25.712205
173.121747	7181.544216	25.717223
173.127529	7198.283858	25.722240
173.320045	7201.331076	25.727258
173.222520	7195.954816	25.732276
173.305085	7220.447504	25.737293
173.651311	7228.576603	25.742311
173.655850	7229.176903	25.747328
173.797462	7244.114733	25.752346
173.900445	7261.438562	25.757364
174.214943	7265.166635	25.762381
174.569843	7265.101628	25.767399
174.777662	7276.545394	25.772416
175.155183	7277.777107	25.777434
175.563710	7271.746758	25.782452
175.237292	7280.293654	25.787469
175.253797	7288.442713	25.792487
175.899083	7290.705286	25.797504
175.609910	7304.067444	25.802522
175.727588	7305.030255	25.807540
175.708186	7336.798523	25.812557
175.705297	7347.376898	25.817575
175.840138	7353.915271	25.822592
175.889078	7368.268343	25.827610
176.649533	7377.711333	25.832628
176.692485	7402.732310	25.837645
176.986004	7403.323370	25.842663
177.410625	7428.422984	25.847680
177.588929	7437.379498	25.852698
178.120517	7427.217756	25.857716
177.801905	7440.677850	25.862733
178.015518	7443.509733	25.867751
178.179418	7465.359230	25.872768
178.094603	7468.794272	25.877786
178.574907	7479.393564	25.882804
178.691481	7502.449029	25.887821
178.967870	7497.576328	25.892839
178.922579	7505.248146	25.897856
179.338966	7525.603416	25.902874
179.610010	7521.175854	25.907892
179.698326	7535.365805	25.912909
180.068332	7541.939367	25.917927
180.089005	7546.008388	25.922944
180.017235	7559.025201	25.927962
180.887682	7566.455646	25.932980
180.989903	7572.817552	25.937997
180.856195	7583.019166	25.943015
181.181648	7574.634636	25.948032
181.329112	7605.281700	25.953050
181.346284	7604.604636	25.958068
181.128594	7614.124635	25.963085
181.535227	7616.570129	25.968103
181.886746	7639.515215	25.973120
181.706203	7653.364597	25.978138
182.143536	7660.339030	25.983156
182.045598	7679.826526	25.988173
182.412665	7679.694913	25.993191
182.815293	7695.391050	25.998208
182.288225	7710.764556	26.003226
183.238117	7724.811251	26.008244
183.009564	7746.640246	26.013261
183.562611	7735.732737	26.018279
183.907149	7746.771383	26.023296
183.915686	7757.744355	26.028314
184.212562	7756.138746	26.033332
183.926166	7775.321995	26.038349
184.343410	7779.086746	26.043367
184.604458	7779.767482	26.048384
184.529616	7786.271430	26.053402
185.262651	7805.577396	26.058420
185.041747	7815.013761	26.063437
185.273418	7815.702514	26.068455
185.625265	7828.115348	26.073472
185.763728	7832.847098	26.078490
186.306134	7836.481649	26.083508
186.399684	7850.244864	26.088525
186.449889	7860.294899	26.093543
186.697344	7862.432795	26.098560
186.863191	7872.573973	26.103578
186.995124	7858.488359	26.108596
186.899939	7866.464002	26.113613
186.998114	7881.673506	26.118631
187.447553	7892.819345	26.123648
187.357296	7901.142360	26.128666
187.781045	7910.219200	26.133684
187.683136	7916.418235	26.138701
187.564573	7915.785685	26.143719
187.913318	7948.378828	26.148736
188.193642	7960.219120	26.153754
188.649715	7960.361864	26.158772
188.804249	7976.160005	26.163789
188.731741	7975.615142	26.168807
189.057135	7996.216881	26.173824
189.326853	8004.030566	26.178842
189.736419	8009.718679	26.183860
189.501357	8027.517586	26.188877
189.558466	8036.200682	26.193895
190.155394	8050.722019	26.198912
190.289901	8079.320125	26.203930
190.473774	8073.000553	26.208948
190.561290	8088.412888	26.213965
190.989844	8099.633225	26.218983
191.413507	8101.355998	26.224000
191.562485	8106.913987	26.229018
191.735970	8126.545360	26.234036
191.828563	8135.383331	26.239053
192.046720	8143.002388	26.244071
192.316845	8132.499866	26.249088
191.957938	8159.116746	26.254106
192.647487	8164.283564	26.259124
192.788171	8164.543118	26.264141
192.978905	8181.970005	26.269159
193.213822	8189.082951	26.274176
193.261159	8199.173849	26.279194
193.413656	8200.518514	26.284212
193.495433	8221.758762	26.289229
193.500562	8230.397003	26.294247
193.918447	8247.902941	26.299264
193.849843	8256.595153	26.304282
194.139314	8269.268370	26.309300
194.362416	8284.554467	26.314317
194.469541	8298.973578	26.319335
194.831176	8313.015781	26.324352
195.465947	8322.711742	26.329370
195.438289	8340.669655	26.334388
196.008894	8341.986864	26.339405
196.055805	8345.864263	26.344423
196.366529	8344.208254	26.349440
196.407165	8364.933234	26.354458
196.557236	8368.521791	26.359476
196.779268	8372.512786	26.364493
196.691273	8382.347345	26.369511
197.011996	8392.023657	26.374528
197.226631	8405.310416	26.379546
197.588963	8408.097371	26.384564
197.482439	8426.701780	26.389581
197.626754	8437.577906	26.394599
197.856141	8454.357470	26.399616
197.820037	8473.943618	26.404634
198.106388	8467.267409	26.409652
198.260948	8488.464452	26.414669
198.780380	8515.485571	26.419687
198.920885	8512.354708	26.424704
198.986646	8534.574827	26.429722
199.135954	8534.697467	26.434740
199.529556	8548.339925	26.439757
199.574530	8568.394866	26.444775
200.021376	8571.238757	26.449792
200.110528	8572.853110	26.454810
200.390748	8577.864110	26.459828
200.699835	8583.646264	26.464845
200.756826	8587.727655	26.469863
201.055789	8588.908675	26.474880
201.094894	8619.133698	26.479898
201.211384	8616.340797	26.484916
201.289341	8627.102785	26.489933
201.825497	8641.719015	26.494951
201.816208	8642.053821	26.499968
202.089998	8651.546637	26.504986
202.374639	8668.689098	26.510004
202.502093	8682.307197	26.515021
202.563552	8685.841961	26.520039
203.072277	8694.168634	26.525056
202.710406	8707.375416	26.530074
203.386079	8708.747738	26.535092
203.620841	8727.923049	26.540109
203.559476	8737.765233	26.545127
203.800520	8746.943698	26.550144
203.631131	8761.247514	26.555162
204.226732	8772.592710	26.560180
204.325260	8791.433796	26.565197
204.486902	8803.665398	26.570215
204.639144	8816.421638	26.575232
204.719914	8836.005423	26.580250
205.070617	8855.958119	26.585268
205.544965	8866.928788	26.590285
205.598998	8876.771648	26.595303
206.020683	8885.696563	26.600320
206.211624	8905.864833	26.605338
206.335783	8913.791293	26.610356
206.953458	8923.135173	26.615373
206.963395	8933.265024	26.620391
207.482415	8936.383780	26.625408
207.573311	8943.340508	26.630426
207.809246	8947.346677	26.635444
207.951189	8950.505016	26.640461
207.989378	8965.530117	26.645479
208.347141	8966.501339	26.650496
208.273248	8984.633059	26.655514
208.580960	8991.245110	26.660532
209.244489	9002.119168	26.665549
209.264054	9014.094007	26.670567
209.498517	9010.443320	26.675584
209.246132	9021.424905	26.680602
209.593114	9036.182315	26.685620
209.601087	9047.055431	26.690637
209.326662	9057.290731	26.695655
210.201487	9065.022883	26.700672
210.312279	9093.525106	26.705690
210.462993	9109.561333	26.710708
210.913348	9119.257591	26.715725
210.843727	9136.818427	26.720743
211.383767	9140.493853	26.725760
210.702604	9142.405160	26.730778
211.289982	9165.611176	26.735796
212.032551	9181.343097	26.740813
212.005617	9196.765994	26.745831
212.311626	9198.788818	26.750848
212.199116	9215.443017	26.755866
212.584350	9229.686944	26.760884
213.037217	9243.721954	26.765901
213.122926	9250.087263	26.770919
213.534299	9254.563920	26.775936
213.765164	9265.627165	26.780954
213.991548	9279.492514	26.785972
213.991126	9281.866222	26.790989
213.853337	9286.885199	26.796007
214.416317	9296.180846	26.801024
214.471304	9311.602896	26.806042
214.566922	9312.846783	26.811060
214.731728	9323.013477	26.816077
214.612711	9348.087945	26.821095
215.352782	9349.600922	26.826112
215.536088	9374.653744	26.831130
215.760340	9391.595063	26.836148
215.879858	9402.734345	26.841165
216.088203	9407.880401	26.846183
216.548298	9427.570699	26.851200
216.650879	9441.559096	26.856218
217.220821	9441.439585	26.861236
217.346083	9456.004053	26.866253
217.279736	9473.226753	26.871271
217.718070	9467.820889	26.876288
217.917506	9485.191823	26.881306
217.817678	9501.292764	26.886324
218.059143	9517.364794	26.891341
218.198404	9527.951014	26.896359
218.534006	9535.250358	26.901376
218.644602	9558.156945	26.906394
219.280825	9569.302188	26.911412
218.985706	9583.107603	26.916429
219.075842	9596.649150	26.921447
219.553260	9610.848220	26.926464
220.034155	9628.235738	26.931482
219.993091	9650.387642	26.936500
220.558635	9657.745875	26.941517
220.458219	9674.096819	26.946535
220.783717	9681.715386	26.951552
221.008003	9699.732375	26.956570
221.106320	9710.773754	26.961588
221.523810	9713.989044	26.966605
221.763742	9739.093720	26.971623
222.352851	9746.974348	26.976640
222.575690	9751.869957	26.981658
222.486549	9770.442319	26.986676
222.751048	9767.740525	26.991693
222.963437	9789.108548	26.996711
223.410199	9806.853273	27.001728
223.438397	9802.401479	27.006746
223.409459	9825.166106	27.011764
223.969135	9838.719938	27.016781
224.012253	9839.742518	27.021799
224.277112	9856.442051	27.026816
224.742957	9866.021179	27.031834
224.601252	9874.247379	27.036852
225.028560	9889.086816	27.041869
225.172494	9903.929061	27.046887
225.375904	9903.326637	27.051904
225.518534	9932.430906	27.056922
225.605544	9935.876632	27.061940
226.049212	9950.662998	27.066957
226.040855	9972.718545	27.071975
226.493326	9986.932320	27.076992
226.659478	9986.621251	27.082010
226.393126	10017.450945	27.087028
227.177844	10020.960811	27.092045
227.308319	10041.521036	27.097063
227.750003	10057.564402	27.102080
228.053121	10069.915358	27.107098
227.895673	10082.365414	27.112116
228.162168	10087.342136	27.117133
228.601373	10114.485594	27.122151
229.005591	10122.999701	27.127168
228.745422	10125.308601	27.132186
229.036784	10143.987786	27.137204
229.284325	10151.996063	27.142221
229.083620	10159.781539	27.147239
229.615182	10176.074066	27.152256
229.768217	10195.163032	27.157274
229.845953	10211.069056	27.162292
230.589799	10225.313591	27.167309
230.489073	10243.243972	27.172327
230.514151	10258.359113	27.177344
231.272912	10260.540322	27.182362
231.352656	10278.830843	27.187380
231.712180	10292.686845	27.192397
231.861692	10302.438353	27.197415
232.390100	10320.810639	27.202432
232.590405	10329.713925	27.207450
232.270482	10340.696557	27.212468
232.673425	10352.434815	27.217485
232.885025	10365.125736	27.222503
233.438882	10388.185448	27.227520
233.755705	10392.232952	27.232538
234.043027	10408.110778	27.237556
234.266416	10419.218601	27.242573
234.386373	10431.311020	27.247591
234.470397	10444.075120	27.252608
234.892161	10458.897883	27.257626
234.861592	10461.634435	27.262644
235.455483	10479.413062	27.267661
235.484807	10491.606404	27.272679
235.698331	10510.005035	27.277696
236.062155	10518.478769	27.282714
236.028578	10522.422017	27.287732
236.380570	10541.643905	27.292749
236.698489	10556.325592	27.297767
236.963947	10572.947775	27.302784
237.284137	10581.159322	27.307802
237.150655	10597.653761	27.312820
237.743342	10604.824372	27.317837
237.838819	10624.971213	27.322855
237.574713	10638.488767	27.327872
238.394116	10650.161453	27.332890
238.275949	10674.086007	27.337908
238.733723	10679.518928	27.342925
239.178835	10699.990879	27.347943
239.199810	10705.209339	27.352960
239.751487	10729.689611	27.357978
239.790381	10742.065128	27.362996
239.863859	10747.036979	27.368013
240.050388	10767.731453	27.373031
240.587522	10785.051040	27.378048
241.067809	10790.210825	27.383066
241.042244	10807.224931	27.388084
241.597556	10823.813571	27.393101
241.641844	10831.686445	27.398119
241.546709	10839.062417	27.403136
241.979418	10843.232667	27.408154
242.161154	10868.319588	27.413172
242.273189	10882.213129	27.418189
242.811477	10894.443065	27.423207
242.833093	10910.499308	27.428224
243.209935	10922.729203	27.433242
243.491945	10940.937356	27.438260
243.799752	10944.951828	27.443277
244.136279	10960.026311	27.448295
244.222833	10980.932999	27.453312
245.001870	10988.553534	27.458330
244.439147	11000.527758	27.463348
244.728739	11006.612622	27.468365
244.869316	11014.282133	27.473383
245.358499	11026.887445	27.478400
245.767140	11039.455676	27.483418
245.541400	11052.908922	27.488436
246.066032	11064.145381	27.493453
246.206680	11084.953431	27.498471
246.124832	11097.883385	27.503488
246.636191	11108.009598	27.508506
246.324129	11129.062826	27.513524
246.714190	11146.329938	27.518541
246.987573	11164.851770	27.523559
246.907231	11189.702091	27.528576
247.514700	11202.454989	27.533594
247.742525	11231.444287	27.538612
248.154531	11248.816603	27.543629
248.599886	11270.554572	27.548647
248.703660	11288.354561	27.553664
249.418325	11287.900670	27.558682
249.408063	11311.408059	27.563700
249.503231	11322.458943	27.568717
249.583171	11337.436011	27.573735
250.217959	11351.098449	27.578752
250.741621	11362.072124	27.583770
250.722742	11387.304940	27.588788
251.040383	11402.770603	27.593805
251.225650	11405.929348	27.598823
251.268272	11432.448914	27.603840
251.924788	11440.168737	27.608858
251.906901	11456.558246	27.613876
251.932533	11484.724246	27.618893
252.277216	11482.678604	27.623911
252.627651	11516.761523	27.628928
253.014188	11530.772486	27.633946
253.075928	11548.433172	27.638964
253.722477	11551.157882	27.643981
253.921092	11572.555762	27.648999
253.859487	11598.374294	27.654016
254.156679	11601.906921	27.659034
254.651304	11625.777137	27.664052
254.776631	11638.373825	27.669069
255.183526	11655.698576	27.674087
255.473479	11666.851394	27.679104
255.933103	11673.384255	27.684122
255.591716	11691.926517	27.689140
256.149645	11706.541158	27.694157
256.521523	11712.455088	27.699175
256.554500	11729.654295	27.704192
256.813094	11743.640925	27.709210
257.051433	11760.231001	27.714228
257.318001	11783.203172	27.719245
257.499028	11800.297580	27.724263
257.863205	11817.884858	27.729280
258.282495	11830.962507	27.734298
258.390755	11848.836433	27.739316
258.343234	11866.718832	27.744333
258.332044	11879.344609	27.749351
258.834822	11908.595314	27.754368
259.350035	11934.008458	27.759386
259.388915	11955.031450	27.764404
259.506826	11970.092639	27.769421
260.227020	11982.239714	27.774439
260.051037	12004.694522	27.779456
260.408119	12022.987593	27.784474
260.694147	12044.250287	27.789492
261.340041	12060.781085	27.794509
261.647403	12081.640034	27.799527
261.512728	12085.390811	27.804544
262.122359	12101.174402	27.809562
262.354761	12113.049334	27.814580
262.541428	12131.660693	27.819597
262.702093	12141.632872	27.824615
262.634668	12168.765951	27.829632
263.065325	12165.437438	27.834650
263.274766	12193.430839	27.839668
263.408970	12210.462516	27.844685
263.925129	12223.453535	27.849703
263.990622	12245.009863	27.854720
264.779340	12261.085440	27.859738
264.502856	12277.494947	27.864756
265.161602	12287.502955	27.869773
265.449593	12304.369023	27.874791
265.328702	12323.936057	27.879808
265.857233	12348.194116	27.884826
265.996582	12364.136182	27.889844
266.223260	12379.903069	27.894861
266.899701	12395.827172	27.899879
266.970366	12410.028287	27.904896
267.627705	12426.013890	27.909914
267.321775	12432.451589	27.914932
267.583919	12458.960131	27.919949
267.980566	12479.253257	27.924967
268.069824	12502.150214	27.929984
268.471112	12519.402752	27.935002
268.979791	12537.846233	27.940020
269.310929	12554.941801	27.945037
269.699017	12571.930256	27.950055
269.655104	12584.183785	27.955072
270.131202	12595.022770	27.960090
269.994985	12612.430569	27.965108
270.433970	12638.646958	27.970125
270.770967	12644.634770	27.975143
270.822992	12674.314471	27.980160
271.055250	12696.480454	27.985178
271.647046	12707.101799	27.990196
271.776837	12727.798714	27.995213
272.172853	12745.553501	28.000231
272.210606	12763.181656	28.005248
272.217415	12778.061846	28.010266
272.788007	12800.866939	28.015284
272.983779	12823.896428	28.020301
273.777985	12843.692401	28.025319
274.038509	12865.491475	28.030336
274.213319	12874.319226	28.035354
274.427051	12888.492348	28.040372
274.742320	12905.230028	28.045389
275.247355	12921.085316	28.050407
275.345886	12935.524968	28.055424
275.637870	12952.274431	28.060442
275.645237	12966.149261	28.065460
275.816828	12986.399903	28.070477
276.410451	12996.833602	28.075495
276.644315	13018.813798	28.080512
276.991896	13026.500427	28.085530
277.213969	13054.215855	28.090548
277.237075	13075.685743	28.095565
277.538439	13084.453261	28.100583
277.526625	13107.758632	28.105600
277.677916	13125.732426	28.110618
278.169406	13156.539549	28.115636
278.454826	13179.570461	28.120653
279.189411	13194.139871	28.125671
279.116259	13225.313228	28.130688
279.585900	13227.623100	28.135706
279.900005	13253.163006	28.140724
279.886824	13263.059063	28.145741
280.430291	13275.772192	28.150759
280.420199	13291.840764	28.155776
281.014606	13308.133936	28.160794
281.466353	13318.731588	28.165812
281.457614	13349.508411	28.170829
281.701249	13351.587799	28.175847
281.892666	13372.135071	28.180864
282.304639	13388.732739	28.185882
282.440858	13413.590007	28.190900
282.469329	13431.081735	28.195917
282.977027	13442.620515	28.200935
283.435545	13471.377052	28.205952
283.637524	13481.989364	28.210970
284.024908	13490.202304	28.215988
283.599504	13526.466630	28.221005
284.279991	13543.711863	28.226023
284.837607	13580.179216	28.231040
284.650629	13593.240446	28.236058
285.171123	13610.140302	28.241076
285.094920	13637.474274	28.246093
285.835849	13664.025300	28.251111
285.972063	13680.594841	28.256128
286.343842	13712.459834	28.261146
286.819420	13723.203525	28.266164
287.370974	13748.279383	28.271181
287.871176	13761.143471	28.276199
287.994163	13782.753778	28.281216
288.141897	13790.809539	28.286234
288.505946	13812.368951	28.291252
288.727364	13825.301300	28.296269
289.242229	13834.628037	28.301287
289.305540	13855.200273	28.306304
289.435006	13873.380233	28.311322
289.955965	13890.396928	28.316340
290.226574	13905.894827	28.321357
290.546906	13917.721851	28.326375
290.962833	13937.619601	28.331392
291.341560	13945.249502	28.336410
291.703251	13965.763032	28.341428
291.466916	13993.261217	28.346445
292.410625	13997.209020	28.351463
292.427644	14020.564503	28.356480
292.473920	14035.185564	28.361498
292.858914	14053.276146	28.366516
293.067675	14068.954649	28.371533
293.375399	14092.550528	28.376551
293.386757	14109.319263	28.381568
293.843108	14133.264119	28.386586
293.924494	14152.790402	28.391604
294.140895	14169.184833	28.396621
294.482163	14196.390745	28.401639
295.018490	14221.751963	28.406656
295.098262	14245.480358	28.411674
295.538991	14270.595852	28.416692
295.550445	14294.401821	28.421709
295.826809	14315.719515	28.426727
296.281269	14337.113353	28.431744
296.694071	14363.685160	28.436762
296.918696	14383.588326	28.441780
297.018114	14411.389400	28.446797
297.452880	14424.479189	28.451815
297.743793	14450.734035	28.456832
298.172111	14479.979623	28.461850
298.799328	14495.505738	28.466868
299.006115	14513.549099	28.471885
299.305271	14532.745062	28.476903
299.422011	14556.811372	28.481920
299.669784	14576.764528	28.486938
299.851456	14585.932503	28.491956
300.055057	14623.969092	28.496973
300.670598	14631.498650	28.501991
301.253746	14652.832197	28.507008
301.446038	14675.762427	28.512026
301.904029	14680.976020	28.517044
302.016333	14700.912349	28.522061
302.466184	14711.118777	28.527079
302.303835	14721.951386	28.532096
302.680269	14747.622007	28.537114
303.024023	14762.468716	28.542132
303.303105	14780.166272	28.547149
303.501265	14804.266751	28.552167
303.966272	14823.919466	28.557184
304.081828	14844.358207	28.562202
304.315231	14869.972313	28.567220
304.637380	14887.869327	28.572237
305.189160	14912.376383	28.577255
305.388083	14938.355657	28.582272
305.485491	14960.115177	28.587290
306.314647	14972.851694	28.592308
305.970566	15012.882211	28.597325
306.682957	15032.694396	28.602343
306.837724	15054.225464	28.607360
307.020753	15083.219571	28.612378
307.344111	15112.222024	28.617396
307.683033	15133.128513	28.622413
308.133049	15155.559675	28.627431
308.466986	15180.191454	28.632448
308.371190	15205.272674	28.637466
309.210085	15225.146111	28.642484
309.191145	15255.898251	28.647501
309.467030	15284.522710	28.652519
309.987914	15306.381240	28.657536
310.267223	15327.745470	28.662554
311.075601	15349.493424	28.667572
310.978989	15375.011632	28.672589
311.253986	15392.535571	28.677607
311.482251	15418.129316	28.682624
311.737612	15431.883223	28.687642
312.222014	15456.028695	28.692660
312.244270	15483.428247	28.697677
312.944298	15518.820315	28.702695
313.217034	15535.145316	28.707712
313.324229	15562.675948	28.712730
313.656522	15586.303009	28.717748
313.771678	15614.223301	28.722765
314.477331	15632.004057	28.727783
314.825169	15661.774178	28.732800
315.042745	15694.951560	28.737818
315.689911	15703.817716	28.742836
315.942767	15737.979190	28.747853
316.255407	15751.641922	28.752871
316.613505	15766.829200	28.757888
316.894403	15799.692107	28.762906
317.238099	15808.447779	28.767924
317.478340	15831.236130	28.772941
318.073712	15847.552172	28.777959
318.550564	15867.840961	28.782976
318.368808	15882.353246	28.787994
318.592815	15896.055988	28.793012
319.102121	15927.998669	28.798029
319.441915	15941.396990	28.803047
319.593809	15964.906291	28.808064
319.843938	15986.605635	28.813082
320.364403	16003.243168	28.818100
320.332171	16024.919945	28.823117
320.759637	16053.794913	28.828135
321.516355	16079.979990	28.833152
321.477498	16094.612244	28.838170
321.855357	16102.865908	28.843188
322.249493	16128.445910	28.848205
322.036951	16145.855897	28.853223
322.549083	16167.625600	28.858240
322.747581	16194.763879	28.863258
323.101563	16216.209900	28.868276
323.324813	16246.236558	28.873293
323.413600	16275.807925	28.878311
323.885379	16304.605067	28.883328
324.417420	16341.560394	28.888346
325.027669	16358.044716	28.893364
325.138196	16390.118925	28.898381
325.395380	16412.478110	28.903399
325.887147	16437.980958	28.908416
325.782403	16464.953926	28.913434
326.273873	16485.001465	28.918452
326.373377	16511.108434	28.923469
326.710764	16540.948075	28.928487
327.242128	16563.457539	28.933504
327.384616	16609.532031	28.938522
328.020277	16630.476424	28.943540
328.085010	16670.953997	28.948557
328.529888	16697.426537	28.953575
329.162470	16727.194009	28.958592
329.286614	16759.395934	28.963610
329.549356	16780.689127	28.968628
329.851588	16808.405503	28.973645
330.496729	16834.000222	28.978663
330.695684	16868.124089	28.983680
331.261422	16885.510067	28.988698
331.743137	16916.850777	28.993716
331.989063	16946.227091	28.998733
332.189708	16963.424525	29.003751
332.689817	16989.253139	29.008768
333.013801	17021.059944	29.013786
333.442722	17029.263062	29.018804
333.779698	17054.001173	29.023821
334.076034	17075.974883	29.028839
334.735337	17090.675310	29.033856
334.401244	17120.277194	29.038874
334.672048	17150.603427	29.043892
335.035513	17173.688498	29.048909
335.230989	17206.547847	29.053927
335.675909	17228.036877	29.058944
336.171083	17268.064765	29.063962
336.344590	17292.860240	29.068980
336.922661	17323.842130	29.073997
337.250203	17351.230499	29.079015
337.783534	17366.661377	29.084032
337.529715	17397.566715	29.089050
338.326641	17422.664318	29.094068
338.544392	17448.283439	29.099085
338.844619	17475.232001	29.104103
339.416336	17508.031249	29.109120
339.369524	17536.307896	29.114138
339.812815	17557.569051	29.119156
340.286679	17583.122343	29.124173
340.608529	17613.239197	29.129191
341.256692	17638.472097	29.134208
341.164980	17661.492889	29.139226
341.604705	17685.131967	29.144244
341.961971	17709.330154	29.149261
342.189190	17731.789085	29.154279
342.775372	17754.983129	29.159296
342.939283	17799.919231	29.164314
343.299772	17817.163606	29.169332
343.581550	17847.011649	29.174349
343.887796	17874.276717	29.179367
344.462246	17895.138262	29.184384
344.284463	17917.000815	29.189402
344.569151	17944.518637	29.194420
344.982266	17967.774728	29.199437
345.317072	18007.334375	29.204455
345.856389	18028.586545	29.209472
345.959444	18065.939886	29.214490
346.532314	18085.534497	29.219508
347.000665	18111.647565	29.224525
346.758282	18154.425973	29.229543
347.751521	18179.774410	29.234560
347.819281	18206.420552	29.239578
348.171044	18234.348656	29.244596
348.265382	18259.844421	29.249613
348.638156	18287.554743	29.254631
349.160231	18328.559697	29.259648
349.533216	18363.777097	29.264666
349.690192	18392.407693	29.269684
350.627672	18419.876583	29.274701
350.828557	18463.252402	29.279719
351.463563	18490.440418	29.284736
351.603439	18519.755089	29.289754
351.656420	18535.583429	29.294772
352.031369	18581.407356	29.299789
352.347519	18607.262630	29.304807
352.799570	18630.156922	29.309824
353.311707	18663.726590	29.314842
353.616867	18690.909622	29.319860
354.288780	18718.400890	29.324877
354.704880	18748.190479	29.329895
354.950372	18776.523318	29.334912
355.419876	18801.406047	29.339930
355.985448	18820.772568	29.344948
356.556914	18849.574970	29.349965
356.612465	18873.968247	29.354983
357.125580	18887.072264	29.360000
357.223824	18920.231701	29.365018
357.585710	18940.040385	29.370036
357.845953	18977.167956	29.375053
358.209578	19006.958810	29.380071
358.363451	19027.689595	29.385088
358.825961	19055.520343	29.390106
358.871304	19090.432486	29.395124
359.180831	19110.855417	29.400141
359.431925	19152.109039	29.405159
359.891082	19189.815845	29.410176
360.253231	19219.613628	29.415194
361.009568	19252.248600	29.420212
361.387398	19281.287167	29.425229
361.325675	19312.827965	29.430247
361.979070	19336.809237	29.435264
362.166052	19377.322019	29.440282
362.291794	19402.358710	29.445300
363.228901	19435.452846	29.450317
363.459225	19460.440784	29.455335
363.774450	19495.878234	29.460352
364.042129	19520.956249	29.465370
364.369907	19549.032411	29.470388
365.095222	19579.836476	29.475405
365.427043	19608.976243	29.480423
366.010653	19645.299757	29.485440
366.279664	19667.886808	29.490458
366.361915	19700.536476	29.495476
366.784499	19724.703128	29.500493
366.884369	19766.107838	29.505511
367.309358	19789.187928	29.510528
367.729650	19817.468371	29.515546
368.172994	19841.964414	29.520564
368.312704	19866.444530	29.525581
368.370340	19901.739435	29.530599
369.070592	19933.016544	29.535616
369.128951	19952.205037	29.540634
369.805242	19985.937805	29.545652
370.155573	20013.716191	29.550669
370.279361	20045.555592	29.555687
371.279155	20083.550160	29.560704
371.568610	20107.433537	29.565722
371.643443	20136.317200	29.570740
372.080946	20160.895082	29.575757
372.227101	20201.326743	29.580775
372.817235	20222.054594	29.585792
373.081307	20263.322989	29.590810
373.480942	20298.811229	29.595828
373.919354	20326.971286	29.600845
373.818533	20361.055731	29.605863
374.397554	20404.219478	29.610880
375.135217	20436.505109	29.615898
375.439413	20470.005605	29.620916
376.136699	20490.332931	29.625933
376.188330	20525.310080	29.630951
376.526809	20550.147724	29.635968
377.182438	20588.085303	29.640986
377.385134	20627.975723	29.646004
378.055204	20647.073226	29.651021
378.295180	20687.813741	29.656039
378.460003	20718.813572	29.661056
379.074774	20752.234847	29.666074
379.138029	20789.403758	29.671092
379.478256	20805.853627	29.676109
380.035916	20846.598707	29.681127
380.361179	20868.315621	29.686144
381.082978	20913.500414	29.691162
381.125482	20952.407464	29.696180
381.490590	20976.680031	29.701197
382.063652	21019.494743	29.706215
382.617166	21047.531318	29.711232
383.004559	21077.810689	29.716250
383.025058	21117.000834	29.721268
383.552240	21143.416353	29.726285
383.715801	21178.734241	29.731303
384.340030	21208.555246	29.736320
384.553842	21248.867851	29.741338
384.932320	21283.877619	29.746356
385.744997	21307.827467	29.751373
386.129120	21357.287050	29.756391
386.261993	21387.041481	29.761408
386.608480	21413.194058	29.766426
386.978491	21446.666681	29.771444
387.331479	21470.478407	29.776461
387.514642	21519.703681	29.781479
388.105935	21561.279013	29.786496
388.536174	21600.766692	29.791514
388.880608	21624.447604	29.796532
389.206755	21648.845843	29.801549
389.766021	21695.836625	29.806567
389.985273	21724.724331	29.811584
390.381119	21755.799779	29.816602
390.373948	21800.342868	29.821620
390.793970	21832.481922	29.826637
391.382542	21879.318571	29.831655
392.075488	21909.681311	29.836672
392.588510	21953.285674	29.841690
392.830815	21984.464216	29.846708
393.394461	22017.650483	29.851725
393.728198	22046.056216	29.856743
393.999483	22080.922966	29.861760
394.716285	22098.797105	29.866778
394.448851	22143.179186	29.871796
394.998198	22169.930076	29.876813
395.234486	22203.522513	29.881831
395.750007	22236.168448	29.886848
396.329306	22259.070282	29.891866
396.174709	22293.799816	29.896884
396.462606	22332.732495	29.901901
396.880607	22381.214992	29.906919
397.452635	22414.660825	29.911936
397.809199	22451.937792	29.916954
397.782206	22509.106901	29.921972
398.573520	22551.468357	29.926989
399.192886	22584.914575	29.932007
399.648431	22638.655064	29.937024
400.266357	22668.698870	29.942042
400.526920	22710.246610	29.947060
400.818940	22739.431485	29.952077
401.377421	22781.284884	29.957095
401.776627	22816.896747	29.962112
402.240319	22849.841006	29.967130
402.491393	22888.680133	29.972148
403.353415	22921.536531	29.977165
403.454939	22958.882050	29.982183
403.546242	22993.824612	29.987200
404.044343	23032.621609	29.992218
404.686608	23076.926525	29.997236
405.142941	23114.005514	30.002253
405.476075	23156.619344	30.007271
405.748904	23195.889216	30.012288
406.398499	23235.487893	30.017306
406.672809	23267.403054	30.022324
407.123698	23300.599455	30.027341
407.645859	23340.974802	30.032359
407.791895	23386.116409	30.037376
408.348992	23418.125396	30.042394
408.836359	23458.673934	30.047412
409.492780	23488.588243	30.052429
409.603293	23530.850354	30.057447
409.955546	23576.458219	30.062464
410.648756	23603.031444	30.067482
410.590053	23654.896974	30.072500
411.186090	23694.210695	30.077517
411.559337	23741.879737	30.082535
411.667462	23787.123294	30.087552
412.157979	23825.630039	30.092570
412.490054	23876.422320	30.097588
412.909297	23909.513180	30.102605
413.487759	23949.112672	30.107623
413.988589	23997.720104	30.112640
414.369198	24036.321209	30.117658
414.626287	24083.490028	30.122676
415.252926	24116.395576	30.127693
415.869411	24153.027690	30.132711
416.059485	24205.736823	30.137728
416.577391	24228.643589	30.142746
417.189308	24288.818001	30.147764
417.779811	24315.469261	30.152781
418.251487	24363.224673	30.157799
418.199703	24392.943953	30.162816
418.849183	24431.198667	30.167834
418.984969	24472.080618	30.172852
419.791121	24512.249304	30.177869
420.068836	24549.745763	30.182887
420.291362	24587.957943	30.187904
420.834733	24621.023329	30.192922
421.316622	24660.826541	30.197940
421.503036	24688.261228	30.202957
421.768094	24721.458027	30.207975
422.199572	24760.648464	30.212992
422.871806	24797.200188	30.218010
423.113240	24845.427156	30.223028
423.530033	24883.232507	30.228045
423.748372	24925.079642	30.233063
424.061155	24960.413793	30.238080
424.764924	24996.481299	30.243098
424.724282	25057.718948	30.248116
425.255046	25095.534291	30.253133
425.748547	25145.720104	30.258151
426.025110	25190.091023	30.263168
427.002383	25221.846180	30.268186
426.936045	25274.093210	30.273204
427.451438	25320.191269	30.278221
428.243144	25356.115658	30.283239
428.713255	25405.012887	30.288256
429.001832	25442.213004	30.293274
429.883031	25479.778792	30.298292
430.109922	25524.978887	30.303309
430.601702	25579.392890	30.308327
430.956686	25612.791016	30.313344
431.521623	25645.987287	30.318362
431.951719	25690.668436	30.323380
432.066447	25727.532048	30.328397
432.836259	25768.387855	30.333415
433.190874	25809.220998	30.338432
434.069678	25849.494348	30.343450
434.245920	25897.157822	30.348468
434.508075	25927.597438	30.353485
434.715991	25967.849613	30.358503
435.264732	26017.139316	30.363520
435.839401	26064.529131	30.368538
436.298249	26102.409059	30.373556
436.416223	26142.827933	30.378573
437.098696	26189.518917	30.383591
437.381314	26239.446311	30.388608
438.046357	26280.919997	30.393626
438.353988	26322.667429	30.398644
438.804074	26371.438231	30.403661
439.684139	26412.882959	30.408679
439.912244	26451.473720	30.413696
439.953871	26485.515263	30.418714
440.524273	26532.528543	30.423732
441.088275	26577.098350	30.428749
441.616898	26614.885841	30.433767
441.648754	26661.177914	30.438784
442.354551	26701.642763	30.443802
442.795863	26758.933053	30.448820
443.033116	26795.971088	30.453837
443.693205	26836.361801	30.458855
444.320887	26892.306286	30.463872
444.803784	26927.338724	30.468890
445.114150	26974.547653	30.473908
445.711178	27010.163874	30.478925
446.027848	27050.861125	30.483943
446.415310	27092.300681	30.488960
446.927599	27123.070083	30.493978
447.029031	27174.026979	30.498996
447.361617	27222.087777	30.504013
448.054613	27270.003892	30.509031
448.565371	27316.682175	30.514048
449.051312	27363.418318	30.519066
449.412625	27406.304577	30.524084
449.984917	27453.540864	30.529101
450.784741	27483.887931	30.534119
450.693226	27524.906210	30.539136
451.083038	27564.400133	30.544154
451.682589	27607.733269	30.549172
452.186467	27631.460775	30.554189
452.662825	27682.508535	30.559207
452.732922	27726.787639	30.564224
453.533056	27763.236160	30.569242
453.919148	27817.964920	30.574260
454.243780	27862.441998	30.579277
454.257700	27898.528789	30.584295
454.855721	27955.702458	30.589312
455.486910	27998.413022	30.594330
455.856757	28050.921169	30.599348
456.415211	28096.792370	30.604365
456.964424	28134.459889	30.609383
457.270572	28204.875566	30.614400
457.706408	28238.574538	30.619418
457.942805	28291.487214	30.624436
458.461007	28340.517274	30.629453
459.265606	28386.383206	30.634471
459.373300	28442.087489	30.639488
459.958090	28486.103525	30.644506
460.276828	28541.448261	30.649524
460.547218	28588.560925	30.654541
461.716589	28644.191111	30.659559
461.959673	28691.295952	30.664576
462.517786	28738.676886	30.669594
463.320565	28794.841438	30.674612
463.714670	28841.621987	30.679629
464.746678	28883.792015	30.684647
464.893646	28922.341747	30.689664
465.029292	28941.295632	30.694682
465.596103	28987.338154	30.699700
466.225512	29044.156857	30.704717
466.825380	29079.587560	30.709735
466.750706	29127.676844	30.714752
467.052022	29173.807960	30.719770
467.769252	29230.518090	30.724788
468.365031	29274.070528	30.729805
468.935116	29326.356926	30.734823
469.104007	29378.514268	30.739840
469.439531	29428.908986	30.744858
470.079774	29473.492530	30.749876
470.292062	29528.769667	30.754893
470.996139	29576.510464	30.759911
471.329491	29631.960344	30.764928
472.163314	29670.719863	30.769946
472.635103	29714.243436	30.774964
472.957151	29771.806302	30.779981
473.644003	29817.219077	30.784999
473.833401	29871.873241	30.790016
474.450257	29914.205955	30.795034
475.037554	29974.804875	30.800052
475.157160	30016.636446	30.805069
475.774036	30059.426985	30.810087
476.373256	30123.220490	30.815104
476.789439	30167.603094	30.820122
477.887184	30210.973833	30.825140
477.871530	30260.078687	30.830157
478.521592	30300.864012	30.835175
478.686291	30350.122266	30.840192
479.427386	30400.159234	30.845210
479.771608	30444.762683	30.850228
480.032605	30494.494445	30.855245
480.815026	30530.825476	30.860263
481.160904	30595.135883	30.865280
481.534378	30634.734100	30.870298
482.280156	30684.408262	30.875316
482.619578	30733.256901	30.880333
482.921924	30767.809483	30.885351
483.583501	30815.469183	30.890368
484.040300	30847.241902	30.895386
484.744718	30888.167888	30.900404
484.934349	30937.376330	30.905421
485.322676	30982.131600	30.910439
485.531834	31030.999465	30.915456
486.152189	31079.767868	30.920474
486.695754	31129.987894	30.925492
487.123617	31176.532435	30.930509
487.814230	31230.404255	30.935527
487.915465	31280.114186	30.940544
488.627310	31331.546951	30.945562
489.337010	31383.677534	30.950580
489.604553	31442.217234	30.955597
489.840734	31475.081455	30.960615
490.424310	31537.730991	30.965632
490.982795	31592.376740	30.970650
491.683561	31649.270939	30.975668
491.903006	31705.740118	30.980685
492.578407	31743.539655	30.985703
493.053763	31816.115825	30.990720
493.517931	31863.934082	30.995738
494.127931	31918.531294	31.000756
494.403197	31960.748753	31.005773
494.933132	32008.010638	31.010791
495.784684	32068.841233	31.015808
496.152176	32119.156312	31.020826
496.801223	32172.782295	31.025844
497.077492	32222.276579	31.030861
497.624462	32273.468001	31.035879
498.012667	32332.520785	31.040896
498.364215	32391.819646	31.045914
499.118229	32444.160591	31.050932
499.586340	32503.453157	31.055949
500.264294	32556.292961	31.060967
500.769250	32605.633718	31.065984
501.219143	32657.536518	31.071002
501.917610	32710.152500	31.076020
502.308627	32761.765574	31.081037
502.787371	32810.716800	31.086055
503.496009	32858.961146	31.091072
503.537816	32913.705931	31.096090
504.415802	32968.120028	31.101108
504.602418	33021.938697	31.106125
505.256240	33077.172799	31.111143
505.876520	33142.478916	31.116160
506.479505	33186.522626	31.121178
507.201210	33238.969082	31.126196
507.493197	33288.492132	31.131213
507.929440	33332.497528	31.136231
508.414584	33385.684107	31.141248
509.045231	33437.698118	31.146266
509.673722	33488.507183	31.151284
509.736690	33540.123150	31.156301
510.133073	33602.817258	31.161319
510.732212	33653.672674	31.166336
511.446559	33712.663444	31.171354
512.142852	33758.734853	31.176372
512.483073	33819.422530	31.181389
512.949063	33870.003960	31.186407
513.585570	33926.594202	31.191424
514.089680	33970.571006	31.196442
514.447230	34019.555072	31.201460
514.895587	34081.358652	31.206477
515.600211	34124.740933	31.211495
516.326099	34176.987487	31.216512
516.637059	34224.963670	31.221530
517.565239	34266.892364	31.226548
517.713797	34319.582002	31.231565
518.358730	34361.996443	31.236583
518.616185	34413.844677	31.241600
518.967065	34461.922186	31.246618
519.687841	34499.240392	31.251636
520.011245	34548.673370	31.256653
520.493187	34602.293291	31.261671
520.985955	34651.660657	31.266688
521.348457	34714.585174	31.271706
521.757237	34756.944952	31.276724
522.230097	34818.898502	31.281741
522.831879	34877.331058	31.286759
523.430105	34940.993709	31.291776
523.659949	35002.723011	31.296794
524.655381	35051.512823	31.301812
524.757052	35121.866768	31.306829
525.500863	35170.518652	31.311847
526.197036	35234.131420	31.316864
526.278481	35286.699293	31.321882
526.848740	35341.127354	31.326900
527.709588	35409.557900	31.331917
528.497837	35468.428607	31.336935
528.764409	35525.353367	31.341952
529.031951	35581.609072	31.346970
530.257420	35638.375520	31.351988
530.546096	35711.367656	31.357005
531.508546	35761.600849	31.362023
532.112566	35811.423242	31.367040
532.674745	35863.098988	31.372058
533.000715	35915.400997	31.377076
533.709985	35971.370213	31.382093
534.304430	36027.718397	31.387111
534.493818	36064.130461	31.392128
535.164605	36126.623857	31.397146
535.769144	36181.276023	31.402164
536.472112	36237.540626	31.407181
536.811598	36299.587617	31.412199
537.658633	36349.387065	31.417216
537.783657	36395.086348	31.422234
538.618934	36451.039357	31.427252
539.322216	36508.605091	31.432269
539.906653	36553.774268	31.437287
540.052719	36606.600408	31.442304
540.487876	36668.219372	31.447322
541.070853	36709.532308	31.452340
541.359607	36763.256906	31.457357
541.849167	36828.298217	31.462375
542.299026	36890.988622	31.467392
542.922882	36955.900857	31.472410
543.653034	37005.077577	31.477428
543.904913	37066.882879	31.482445
544.894875	37120.956481	31.487463
545.302234	37173.239188	31.492480
545.720961	37238.991230	31.497498
546.558848	37292.014210	31.502516
546.904353	37349.774381	31.507533
547.391196	37401.533270	31.512551
548.141892	37463.418356	31.517568
548.388096	37526.160435	31.522586
549.214055	37580.650775	31.527604
549.868556	37635.785142	31.532621
550.569951	37690.851945	31.537639
551.227210	37741.655631	31.542656
551.171963	37794.486971	31.547674
551.989188	37849.443553	31.552692
552.517948	37912.856714	31.557709
552.880413	37953.574531	31.562727
554.220947	38006.226035	31.567744
554.343403	38063.034259	31.572762
554.569938	38100.757341	31.577780
555.161473	38157.800732	31.582797
555.602620	38205.933234	31.587815
556.481577	38255.003493	31.592832
556.735055	38312.182215	31.597850
556.963686	38367.679660	31.602868
557.678914	38425.180051	31.607885
558.237959	38487.823171	31.612903
558.773997	38542.799963	31.617920
559.048558	38604.174284	31.622938
559.695809	38664.120362	31.627956
560.250007	38740.833866	31.632973
560.550597	38807.700128	31.637991
561.390714	38858.583994	31.643008
561.415779	38940.815200	31.648026
562.490728	39004.586858	31.653044
563.008444	39072.159961	31.658061
563.376537	39144.518259	31.663079
564.190768	39201.550157	31.668096
564.773919	39268.156694	31.673114
565.299037	39344.991181	31.678132
566.161745	39394.780597	31.683149
566.328739	39472.381967	31.688167
567.176149	39537.844077	31.693184
567.637124	39604.434171	31.698202
568.264785	39669.494329	31.703220
569.217484	39735.173320	31.708237
569.528322	39801.091332	31.713255
570.345306	39856.240239	31.718272
570.832941	39919.544047	31.723290
571.550736	39980.767561	31.728308
571.941103	40054.268508	31.733325
572.403149	40120.857139	31.738343
573.363186	40170.818809	31.743360
573.534927	40248.277453	31.748378
574.223206	40316.505627	31.753396
574.987524	40369.622322	31.758413
575.694935	40446.289192	31.763431
576.583694	40488.993300	31.768448
577.051198	40555.487893	31.773466
577.158012	40614.923646	31.778484
577.972476	40686.102932	31.783501
578.446438	40748.736277	31.788519
579.210909	40796.856808	31.793536
579.986390	40870.193110	31.798554
580.357986	40923.878333	31.803572
580.984799	40985.827394	31.808589
581.613769	41040.193311	31.813607
582.563981	41101.448390	31.818624
582.666254	41164.255136	31.823642
583.340702	41213.686007	31.828660
583.876320	41278.388239	31.833677
584.614401	41345.585957	31.838695
584.924076	41403.083848	31.843712
585.073752	41472.582976	31.848730
585.798539	41535.145914	31.853748
586.486411	41606.952687	31.858765
586.920816	41675.834041	31.863783
587.723160	41741.949165	31.868800
588.460120	41808.154269	31.873818
588.943249	41871.181375	31.878836
589.439106	41927.396721	31.883853
589.877014	42006.974985	31.888871
590.722648	42061.412237	31.893888
591.278128	42129.002920	31.898906
591.687851	42189.407043	31.903924
592.726493	42251.096453	31.908941
592.439609	42314.754454	31.913959
593.122894	42368.771151	31.918976
594.118958	42432.302527	31.923994
594.641317	42499.082324	31.929012
595.229827	42556.307175	31.934029
595.799676	42616.064220	31.939047
596.291961	42683.004356	31.944064
596.780189	42760.891559	31.949082
597.305361	42817.666735	31.954100
597.864647	42891.681409	31.959117
598.289339	42959.498811	31.964135
599.143913	43016.131687	31.969152
599.567740	43104.775226	31.974170
600.364088	43180.074730	31.979188
601.201868	43236.903651	31.984205
601.397746	43307.434428	31.989223
602.225715	43379.136457	31.994240
602.914633	43453.469746	31.999258
603.355316	43522.347418	32.004276
603.840757	43597.456928	32.009293
604.231287	43672.282489	32.014311
605.203659	43745.591248	32.019328
605.365040	43817.222115	32.024346
606.276228	43891.447748	32.029364
606.898498	43969.396744	32.034381
607.079213	44052.360545	32.039399
607.685404	44119.173309	32.044416
608.557036	44210.172928	32.049434
609.400909	44290.142116	32.054452
610.434129	44362.625430	32.059469
611.213465	44435.160503	32.064487
611.979230	44498.515988	32.069504
612.510572	44569.213876	32.074522
612.925126	44637.901042	32.079540
613.616756	44700.843205	32.084557
614.083425	44774.059673	32.089575
614.671360	44842.346305	32.094592
615.491332	44916.837379	32.099610
616.240707	44995.783196	32.104628
616.752461	45061.156114	32.109645
617.023557	45129.549888	32.114663
617.853334	45189.524750	32.119680
618.484439	45266.476688	32.124698
619.392002	45346.951375	32.129716
619.826452	45414.472897	32.134733
620.037201	45481.226459	32.139751
620.922015	45558.118664	32.144768
621.780864	45638.852115	32.149786
622.382460	45710.477347	32.154804
622.742001	45777.311542	32.159821
623.269380	45850.392674	32.164839
623.997761	45923.459780	32.169856
624.456292	45997.219160	32.174874
625.356721	46074.802439	32.179892
625.582291	46146.144175	32.184909
626.374627	46225.331176	32.189927
627.027167	46303.287975	32.194944
627.960371	46377.459767	32.199962
628.793654	46457.162007	32.204980
629.281883	46527.375416	32.209997
629.803685	46597.744582	32.215015
630.730955	46668.937454	32.220032
631.176005	46732.445077	32.225050
631.816883	46806.029012	32.230068
632.460142	46866.573742	32.235085
632.710588	46944.549173	32.240103
633.260751	47006.196082	32.245120
634.231346	47070.157894	32.250138
634.461638	47129.729657	32.255156
635.268909	47201.711766	32.260173
635.543374	47276.892925	32.265191
636.476263	47344.582021	32.270208
637.285135	47411.436052	32.275226
637.480626	47488.393286	32.280244
638.372106	47553.579340	32.285261
638.636195	47640.811590	32.290279
639.316115	47716.394793	32.295296
640.039909	47782.291515	32.300314
640.706074	47865.447507	32.305332
641.651529	47928.860540	32.310349
641.849837	48014.516851	32.315367
642.715163	48092.654211	32.320384
643.228061	48168.427901	32.325402
643.907909	48257.429061	32.330420
644.418799	48329.372872	32.335437
644.924065	48416.401374	32.340455
645.827610	48484.806803	32.345472
646.551976	48574.357914	32.350490
647.013553	48655.447817	32.355508
647.837355	48730.638554	32.360525
648.297879	48816.049779	32.365543
648.951007	48891.019879	32.370560
649.882538	48981.366081	32.375578
650.336553	49057.772049	32.380596
650.914936	49140.907042	32.385613
651.669487	49232.272254	32.390631
652.508133	49311.246476	32.395648
653.175393	49393.148739	32.400666
653.460888	49480.306854	32.405684
654.624785	49552.968390	32.410701
654.993894	49639.822823	32.415719
655.461071	49724.946411	32.420736
656.625448	49810.021356	32.425754
657.262586	49898.396026	32.430772
657.854498	49974.991275	32.435789
658.578847	50059.217854	32.440807
659.199869	50144.027260	32.445824
660.279725	50222.665259	32.450842
660.438678	50307.362317	32.455860
661.135719	50379.071376	32.460877
661.725011	50469.098996	32.465895
662.666933	50542.378995	32.470912
663.180657	50620.846957	32.475930
663.651621	50717.231352	32.480948
664.383968	50797.862222	32.485965
665.247363	50893.677200	32.490983
665.666994	50966.899917	32.496000
666.229784	51053.592835	32.501018
666.957370	51149.614745	32.506036
667.916337	51220.797159	32.511053
668.677565	51307.616314	32.516071
669.092978	51382.123710	32.521088
670.082563	51471.249552	32.526106
670.756230	51566.442232	32.531124
671.339676	51630.347453	32.536141
672.262146	51717.192302	32.541159
672.876482	51799.900028	32.546176
673.636399	51873.063545	32.551194
674.321120	51959.689790	32.556212
675.095545	52023.842681	32.561229
675.625945	52105.908566	32.566247
676.165158	52188.864120	32.571264
677.206849	52265.829917	32.576282
677.435316	52342.993730	32.581300
677.977395	52419.537374	32.586317
678.564082	52492.333859	32.591335
679.565505	52564.417597	32.596352
680.131630	52629.977886	32.601370
680.387845	52706.866881	32.606388
681.026339	52780.862564	32.611405
681.458024	52860.370288	32.616423
682.178311	52955.884241	32.621440
683.372158	53033.573397	32.626458
683.475782	53126.309247	32.631476
684.426406	53208.367099	32.636493
685.021157	53291.065421	32.641511
685.695838	53377.623793	32.646528
686.807123	53463.965004	32.651546
687.160758	53545.112145	32.656564
687.593944	53631.332504	32.661581
688.363892	53722.691004	32.666599
688.865331	53811.428099	32.671616
689.915344	53905.356820	32.676634
690.343888	53997.183754	32.681652
691.027101	54074.531872	32.686669
691.699658	54181.470368	32.691687
692.425565	54266.305614	32.696704
693.159300	54356.725306	32.701722
693.824860	54455.560069	32.706740
694.680134	54549.214477	32.711757
695.403207	54651.326254	32.716775
695.983868	54737.678695	32.721792
697.133021	54830.123230	32.726810
697.889530	54930.076324	32.731828
698.676532	55002.236072	32.736845
698.888297	55101.401875	32.741863
699.662712	55203.362682	32.746880
700.422435	55285.985212	32.751898
701.062568	55387.710118	32.756916
701.889517	55474.258818	32.761933
702.413049	55573.438591	32.766951
702.890046	55669.359781	32.771968
703.943130	55761.502302	32.776986
704.530476	55856.180302	32.782004
705.359856	55955.715789	32.787021
706.489756	56047.834295	32.792039
706.883377	56141.604193	32.797056
707.582867	56221.927876	32.802074
708.190261	56326.898278	32.807092
709.131779	56422.348161	32.812109
709.925291	56516.097901	32.817127
710.276259	56608.575341	32.822144
711.670125	56707.275560	32.827162
712.488864	56793.389024	32.832180
713.250008	56880.517124	32.837197
713.705596	56968.283830	32.842215
714.194159	57066.421525	32.847232
715.052342	57153.604273	32.852250
715.390311	57244.033066	32.857268
716.397754	57339.684962	32.862285
716.852071	57433.874275	32.867303
717.191323	57535.009024	32.872320
718.499575	57615.648362	32.877338
718.872815	57724.184702	32.882356
719.956162	57819.453489	32.887373
720.600877	57915.326122	32.892391
721.173458	58021.113736	32.897408
722.306848	58101.240481	32.902426
722.895270	58194.558046	32.907444
723.574923	58280.726189	32.912461
724.017185	58370.807866	32.917479
724.598296	58463.691838	32.922496
725.708059	58556.608860	32.927514
726.335419	58647.767091	32.932532
726.693897	58737.731554	32.937549
727.481412	58823.745143	32.942567
727.908625	58930.086113	32.947584
728.979078	59015.219507	32.952602
729.462138	59106.890304	32.957620
730.071057	59199.766744	32.962637
730.882846	59303.764604	32.967655
731.150053	59405.919197	32.972672
732.146076	59494.865180	32.977690
732.937637	59607.602081	32.982708
733.392749	59707.388726	32.987725
734.368011	59800.125158	32.992743
734.998702	59912.062440	32.997760
735.773178	60014.856672	33.002778
736.181117	60128.671139	33.007796
737.121857	60232.127860	33.012813
737.867774	60333.714961	33.017831
738.515051	60441.670701	33.022848
739.392757	60548.621898	33.027866
740.295908	60666.326571	33.032884
740.668133	60774.411738	33.037901
741.553652	60886.830494	33.042919
742.693158	60998.733827	33.047936
743.372659	61109.759484	33.052954
744.183508	61217.053909	33.057972
744.823086	61319.592619	33.062989
745.729616	61422.782942	33.068007
746.302767	61536.021725	33.073024
747.523726	61637.732675	33.078042
748.070029	61753.726559	33.083060
748.758815	61858.724872	33.088077
749.734688	61967.013556	33.093095
750.473130	62070.898621	33.098112
751.225607	62175.293871	33.103130
751.881214	62278.883974	33.108148
752.761701	62391.185410	33.113165
753.946043	62494.189793	33.118183
754.462045	62597.065052	33.123200
755.489155	62700.450446	33.128218
756.090520	62798.053592	33.133236
756.391257	62898.627217	33.138253
757.321218	62998.597889	33.143271
758.118863	63120.891554	33.148288
758.993729	63220.954592	33.153306
759.475241	63331.614140	33.158324
760.098419	63443.736314	33.163341
761.498807	63545.085680	33.168359
762.192658	63658.354102	33.173376
762.739568	63755.585186	33.178394
763.326896	63867.778800	33.183412
764.150911	63979.782159	33.188429
765.274276	64077.981381	33.193447
765.744347	64191.119055	33.198464
766.487269	64300.185479	33.203482
767.188831	64409.651246	33.208500
768.234863	64518.757180	33.213517
768.959260	64623.093586	33.218535
769.875983	64728.030854	33.223552
770.753402	64836.818664	33.228570
771.338030	64930.420431	33.233588
771.767601	65039.637388	33.238605
773.161235	65143.536978	33.243623
773.445930	65251.666397	33.248640
774.339772	65356.414643	33.253658
774.932681	65465.347619	33.258676
775.440348	65562.075252	33.263693
776.620630	65665.096071	33.268711
777.332854	65767.606889	33.273728
777.969037	65860.300273	33.278746
778.697345	65963.586980	33.283764
779.303413	66075.182475	33.288781
780.305718	66167.418375	33.293799
780.796114	66272.573006	33.298816
781.444735	66383.587800	33.303834
782.131541	66497.909627	33.308852
783.019708	66610.213630	33.313869
784.178896	66718.547360	33.318887
784.576648	66836.010359	33.323904
785.400030	66931.060963	33.328922
786.087859	67041.459491	33.333940
786.916646	67158.593781	33.338957
787.725186	67269.909234	33.343975
788.681897	67382.477877	33.348992
789.248329	67504.399230	33.354010
790.328208	67617.852853	33.359028
791.088074	67730.095532	33.364045
791.944187	67834.369224	33.369063
792.416568	67955.031593	33.374080
793.432957	68076.976657	33.379098
794.480180	68188.396563	33.384116
795.019728	68314.582118	33.389133
796.104395	68412.997733	33.394151
796.798350	68528.600219	33.399168
797.436001	68639.533846	33.404186
798.331843	68771.410520	33.409204
799.438139	68888.489510	33.414221
800.021455	68996.582413	33.419239
800.747536	69115.097588	33.424256
801.632764	69226.258881	33.429274
802.908627	69347.611907	33.434292
803.123841	69470.165377	33.439309
804.297819	69580.022487	33.444327
805.027550	69702.966412	33.449344
805.888177	69807.407110	33.454362
806.562809	69924.658033	33.459380
807.488516	70040.192443	33.464397
808.025481	70158.517055	33.469415
808.870301	70271.562123	33.474432
809.918224	70403.063299	33.479450
811.002210	70521.406929	33.484468
811.495125	70636.839088	33.489485
812.078592	70746.060028	33.494503
813.018683	70871.397694	33.499520
813.773860	70994.445988	33.504538
814.536883	71119.384395	33.509556
815.408007	71239.069811	33.514573
816.462609	71356.518641	33.519591
817.250627	71491.326064	33.524608
818.138537	71603.378208	33.529626
818.896092	71712.455103	33.534644
819.233565	71843.899202	33.539661
820.455556	71969.595015	33.544679
821.129229	72095.287394	33.549696
821.953278	72212.374292	33.554714
822.877242	72338.222718	33.559732
823.555709	72462.594762	33.564749
824.600457	72583.049378	33.569767
825.258965	72705.807206	33.574784
826.061467	72826.429717	33.579802
826.955289	72949.301775	33.584820
827.606780	73079.183663	33.589837
828.516709	73210.497082	33.594855
829.534775	73322.106543	33.599872
830.240325	73446.169850	33.604890
831.241588	73560.034693	33.609908
831.979269	73677.225976	33.614925
832.873974	73782.318994	33.619943
833.542885	73900.262780	33.624960
834.236882	74006.945838	33.629978
835.072302	74126.615128	33.634996
835.839168	74243.817268	33.640013
836.763711	74347.940443	33.645031
837.592859	74473.930719	33.650048
838.280983	74600.432025	33.655066
839.099919	74717.084179	33.660084
839.842544	74829.246520	33.665101
841.096704	74948.737197	33.670119
841.786534	75078.605632	33.675136
842.964278	75196.984521	33.680154
843.906464	75323.612406	33.685172
844.877117	75443.152658	33.690189
845.469489	75555.103209	33.695207
846.452764	75685.805824	33.700224
847.311046	75800.730551	33.705242
847.801321	75921.959343	33.710260
848.273988	76058.017190	33.715277
849.294584	76170.481919	33.720295
850.152908	76310.354692	33.725312
851.084259	76443.537096	33.730330
851.830675	76566.706768	33.735348
852.617050	76694.525748	33.740365
853.327431	76831.301700	33.745383
854.337836	76974.796755	33.750400
855.208801	77105.172106	33.755418
855.974146	77233.971739	33.760436
856.348796	77378.270314	33.765453
857.573289	77508.962746	33.770471
858.521834	77658.291689	33.775488
859.102299	77793.817318	33.780506
860.144496	77931.329482	33.785524
860.864011	78081.553060	33.790541
861.865613	78213.317522	33.795559
862.524334	78364.204573	33.800576
863.305237	78505.691626	33.805594
864.186452	78647.049119	33.810612
865.116148	78803.378598	33.815629
866.178020	78936.294930	33.820647
867.414408	79089.292647	33.825664
868.004764	79231.353466	33.830682
868.970195	79366.736359	33.835700
870.157694	79505.258908	33.840717
870.849805	79641.017595	33.845735
871.701277	79774.966833	33.850752
873.069927	79922.109506	33.855770
873.919186	80053.985849	33.860788
874.661916	80202.302957	33.865805
875.279024	80325.021221	33.870823
876.493651	80464.810375	33.875840
877.235719	80606.620672	33.880858
878.208015	80739.062655	33.885876
879.120760	80889.975177	33.890893
879.841578	81023.795243	33.895911
880.652448	81157.987106	33.900928
881.527650	81304.771186	33.905946
882.476162	81434.203483	33.910964
882.862302	81593.413064	33.915981
884.011437	81720.384459	33.920999
885.043049	81870.518307	33.926016
885.526366	82013.227895	33.931034
886.654657	82160.918270	33.936052
887.746116	82295.380408	33.941069
888.678387	82430.578248	33.946087
889.321358	82568.994400	33.951104
890.223932	82688.483179	33.956122
891.505627	82821.202395	33.961140
892.119937	82959.005612	33.966157
892.795716	83086.347560	33.971175
893.633138	83216.788951	33.976192
894.467063	83350.932896	33.981210
895.528491	83493.011943	33.986228
896.283751	83630.688303	33.991245
897.092688	83765.705586	33.996263
897.914578	83911.306679	34.001280
898.400106	84058.906732	34.006298
899.612068	84197.093025	34.011316
900.533075	84349.792180	34.016333
901.357019	84501.844034	34.021351
902.114767	84642.525093	34.026368
902.919179	84790.538949	34.031386
903.754983	84940.503701	34.036404
904.710414	85086.589935	34.041421
905.901012	85250.975051	34.046439
906.727915	85409.644497	34.051456
907.664749	85558.622085	34.056474
908.634080	85709.322668	34.061492
909.273107	85866.672191	34.066509
910.324335	86016.038738	34.071527
911.486216	86173.531648	34.076544
912.212657	86337.855625	34.081562
913.101645	86477.823650	34.086580
914.407465	86646.553002	34.091597
915.287822	86787.119109	34.096615
916.194320	86940.483022	34.101632
917.059834	87100.030758	34.106650
918.267621	87263.041316	34.111668
918.964612	87413.873801	34.116685
920.037104	87572.789341	34.121703
920.909232	87725.556544	34.126720
921.640610	87884.878636	34.131738
922.595657	88040.057826	34.136756
923.678165	88200.823749	34.141773
924.767984	88351.806070	34.146791
925.516533	88508.699459	34.151808
926.168592	88666.774253	34.156826
927.266249	88828.022864	34.161844
928.235844	88981.408532	34.166861
929.333592	89146.228509	34.171879
930.435832	89299.929696	34.176896
930.995526	89472.992021	34.181914
931.858915	89622.114936	34.186932
932.681492	89798.787737	34.191949
933.875696	89959.819171	34.196967
934.936709	90117.063822	34.201984
935.792773	90284.051717	34.207002
936.699975	90436.064689	34.212020
937.877144	90599.558804	34.217037
939.024084	90758.546529	34.222055
939.948512	90916.863260	34.227072
940.868015	91076.080557	34.232090
941.848545	91220.567531	34.237108
943.033345	91380.413836	34.242125
943.687598	91539.937542	34.247143
944.862924	91680.667215	34.252160
945.628971	91848.231444	34.257178
946.458247	91993.241715	34.262196
947.137204	92148.695654	34.267213
948.254284	92319.540598	34.272231
949.431854	92466.059426	34.277248
949.952703	92634.954476	34.282266
950.969117	92783.824746	34.287284
951.852647	92924.730128	34.292301
952.712832	93089.477049	34.297319
953.886476	93229.336152	34.302336
954.867069	93388.767360	34.307354
955.698969	93539.660229	34.312372
956.818566	93687.398592	34.317389
957.380510	93847.123547	34.322407
958.619824	93992.039893	34.327424
959.183717	94158.760899	34.332442
960.070675	94310.257051	34.337460
961.162551	94461.580991	34.342477
962.167646	94628.358809	34.347495
963.075368	94785.608318	34.352512
963.690523	94959.156248	34.357530
964.792663	95113.482893	34.362548
965.651899	95282.511077	34.367565
966.573841	95452.308645	34.372583
967.577350	95623.872657	34.377600
968.145032	95804.144302	34.382618
969.736477	95970.023922	34.387636
970.437436	96150.339336	34.392653
971.356594	96321.998072	34.397671
972.507848	96491.840775	34.402688
973.235720	96683.335014	34.407706
974.147000	96850.928230	34.412724
975.577079	97026.248613	34.417741
976.195976	97212.086456	34.422759
977.391143	97388.467435	34.427776
978.278859	97574.573706	34.432794
978.932422	97750.787230	34.437812
980.080355	97925.673084	34.442829
981.636599	98117.509748	34.447847
982.534469	98287.950946	34.452864
983.653929	98479.090225	34.457882
984.666794	98643.633432	34.462900
985.641989	98812.843515	34.467917
986.822383	98998.981524	34.472935
988.203898	99171.121369	34.477952
988.670530	99339.678327	34.482970
989.392132	99509.865655	34.487988
990.784316	99687.920502	34.493005
991.835650	99866.634420	34.498023
993.062771	100038.881637	34.503040
993.858623	100218.760896	34.508058
995.077028	100389.650689	34.513076
996.150613	100569.005303	34.518093
997.015203	100749.130175	34.523111
997.959215	100925.235357	34.528128
998.976488	101104.976583	34.533146
999.481630	101270.874321	34.538164
1001.014198	101453.844181	34.543181
1001.869222	101624.700969	34.548199
1003.352678	101795.866533	34.553216
1003.988864	101973.422748	34.558234
1005.123490	102145.363792	34.563252
1006.363102	102325.228713	34.568269
1006.983994	102493.432599	34.573287
1008.232020	102669.068833	34.578304
1009.367219	102840.032943	34.583322
1010.259439	103011.202985	34.588340
1011.645725	103190.156830	34.593357
1012.181388	103353.574361	34.598375
1013.187236	103535.949479	34.603392
1014.053351	103707.748953	34.608410
1015.236613	103879.471785	34.613428
1016.374040	104057.244272	34.618445
1017.110892	104237.895732	34.623463
1018.384412	104389.305704	34.628480
1019.462819	104561.620247	34.633498
1020.409642	104716.454936	34.638516
1021.517122	104883.624878	34.643533
1022.200794	105055.982595	34.648551
1023.230743	105206.437009	34.653568
1024.027566	105373.243472	34.658586
1024.789143	105538.461002	34.663604
1025.788196	105718.838610	34.668621
1026.377290	105896.232882	34.673639
1027.727176	106071.159436	34.678656
1028.642868	106259.217087	34.683674
1029.658278	106448.044846	34.688692
1030.688402	106617.556321	34.693709
1031.686243	106811.139192	34.698727
1033.049404	106988.476076	34.703744
1033.719411	107184.433710	34.708762
1034.665559	107371.544213	34.713780
1035.910410	107548.423058	34.718797
1036.805770	107744.195527	34.723815
1037.950508	107924.538616	34.728832
1038.938557	108115.637261	34.733850
1039.626654	108311.891452	34.738868
1041.086862	108502.180109	34.743885
1041.819789	108704.294367	34.748903
1043.211535	108891.785086	34.753920
1044.082448	109102.378899	34.758938
1044.863396	109302.880988	34.763956
1046.192000	109487.941547	34.768973
1047.207760	109699.124053	34.773991
1048.601334	109899.478577	34.779008
1049.237897	110094.829474	34.784026
1050.554357	110294.262264	34.789044
1051.831282	110500.290152	34.794061
1052.743366	110708.888099	34.799079
1053.967208	110904.122333	34.804096
1055.312634	111096.056895	34.809114
1055.938428	111302.401148	34.814132
1057.383693	111497.374962	34.819149
1058.369513	111688.448350	34.824167
1059.506162	111886.440267	34.829184
1060.755007	112079.803812	34.834202
1061.440071	112288.121873	34.839220
1062.717558	112475.161945	34.844237
1063.788076	112679.580683	34.849255
1064.877507	112880.855983	34.854272
1066.435080	113067.790392	34.859290
1067.559839	113267.453722	34.864308
1068.552630	113439.572857	34.869325
1069.696641	113648.585345	34.874343
1070.592577	113831.466177	34.879360
1071.650473	114029.676396	34.884378
1072.557688	114224.276864	34.889396
1073.801486	114411.905594	34.894413
1074.859881	114606.509050	34.899431
1076.122047	114799.458467	34.904448
1077.003512	114996.146318	34.909466
1077.625357	115185.454053	34.914484
1079.125406	115385.083049	34.919501
1080.131942	115577.079129	34.924519
1081.159090	115781.565626	34.929536
1082.332882	115981.379460	34.934554
1083.532971	116176.172997	34.939572
1084.642430	116372.275207	34.944589
1085.731234	116568.166786	34.949607
1086.626516	116757.566477	34.954624
1087.972927	116954.963897	34.959642
1088.797247	117164.080531	34.964660
1090.183174	117347.511211	34.969677
1090.859138	117537.446467	34.974695
1092.097684	117716.988631	34.979712
1093.295369	117903.596330	34.984730
1094.341930	118086.352919	34.989748
1095.052211	118271.244307	34.994765
1096.068049	118469.530385	34.999783
1097.241977	118662.267048	35.004800
1098.193068	118852.000732	35.009818
1098.993209	119052.607283	35.014836
1100.090772	119249.833457	35.019853
1101.053461	119448.173016	35.024871
1102.177005	119647.285639	35.029888
1103.404244	119861.512480	35.034906
1104.205444	120074.518804	35.039924
1105.469125	120281.925272	35.044941
1106.588883	120496.212538	35.049959
1107.339410	120706.532695	35.054976
1108.793826	120908.387032	35.059994
1109.747458	121137.304748	35.065012
1110.710945	121333.413924	35.070029
1112.183324	121562.008392	35.075047
1113.107318	121786.373955	35.080064
1114.320754	122003.609368	35.085082
1115.361221	122223.510888	35.090100
1116.781905	122436.165693	35.095117
1117.607810	122659.831710	35.100135
1118.771203	122891.338879	35.105152
1120.212829	123101.675803	35.110170
1121.333927	123327.186294	35.115188
1122.618679	123540.441716	35.120205
1123.591639	123765.650483	35.125223
1124.698477	123979.597446	35.130240
1125.943651	124202.724049	35.135258
1127.009976	124424.652526	35.140276
1128.461565	124636.785511	35.145293
1129.497665	124865.629397	35.150311
1130.592581	125087.279172	35.155328
1132.140699	125304.115559	35.160346
1133.023000	125527.273872	35.165364
1134.222693	125741.040467	35.170381
1135.244244	125959.983764	35.175399
1136.298974	126186.109509	35.180416
1137.885026	126401.401137	35.185434
1138.582580	126636.651489	35.190452
1140.092402	126848.498697	35.195469
1140.905382	127077.763577	35.200487
1142.050770	127298.014099	35.205504
1143.544550	127521.706870	35.210522
1144.719983	127751.182991	35.215540
1145.793893	127968.255991	35.220557
1146.947986	128207.790369	35.225575
1148.170189	128415.791883	35.230592
1149.307025	128633.923841	35.235610
1150.346824	128864.622073	35.240628
1151.769982	129076.055161	35.245645
1152.942423	129294.363292	35.250663
1153.696129	129526.178438	35.255680
1154.800556	129743.816443	35.260698
1155.896898	129977.568369	35.265716
1157.031395	130186.660893	35.270733
1157.846851	130426.293530	35.275751
1159.428216	130664.850646	35.280768
1160.855159	130884.407988	35.285786
1161.457120	131120.810679	35.290804
1162.885372	131346.037325	35.295821
1164.172966	131587.248592	35.300839
1165.327742	131813.943520	35.305856
1166.352631	132027.934086	35.310874
1167.228385	132248.352523	35.315892
1168.544867	132465.112048	35.320909
1169.733400	132679.713742	35.325927
1170.706445	132896.634359	35.330944
1171.654378	133112.533733	35.335962
1172.760211	133343.342234	35.340980
1173.998954	133559.120444	35.345997
1175.137080	133787.733587	35.351015
1175.706083	134027.712724	35.356032
1177.357722	134247.243168	35.361050
1178.324327	134486.361257	35.366068
1179.524852	134717.506131	35.371085
1181.154085	134962.223153	35.376103
1181.956793	135194.349953	35.381120
1183.298539	135434.591981	35.386138
1184.129121	135685.176880	35.391156
1185.181082	135916.304013	35.396173
1186.848965	136156.408623	35.401191
1188.037467	136398.736871	35.406208
1189.401919	136635.801571	35.411226
1189.966785	136888.569465	35.416244
1191.314643	137131.865631	35.421261
1192.659509	137390.949161	35.426279
1193.491463	137640.990677	35.431296
1195.015351	137893.873873	35.436314
1195.864048	138140.239424	35.441332
1197.345412	138403.416208	35.446349
1198.940233	138645.439935	35.451367
1199.905035	138904.699359	35.456384
1201.199552	139161.700030	35.461402
1202.261124	139418.272004	35.466420
1203.632757	139671.713497	35.471437
1204.764715	139925.450084	35.476455
1205.729906	140187.394614	35.481472
1207.435546	140441.686858	35.486490
1208.511917	140706.812311	35.491508
1210.033562	140964.461000	35.496525
1211.173723	141223.987942	35.501543
1212.488137	141482.866688	35.506560
1213.559984	141722.880971	35.511578
1214.678772	141986.500235	35.516596
1215.994458	142249.683166	35.521613
1217.255747	142498.738100	35.526631
1218.522722	142772.749644	35.531648
1220.251129	143017.901454	35.536666
1220.918118	143281.110588	35.541684
1222.349164	143543.142858	35.546701
1223.242811	143802.019526	35.551719
1224.170401	144065.508449	35.556736
1225.370587	144328.269473	35.561754
1226.624309	144598.632449	35.566772
1228.131368	144870.008166	35.571789
1229.267405	145134.168015	35.576807
1230.220703	145411.992872	35.581824
1231.526731	145681.683247	35.586842
1232.964597	145945.989398	35.591860
1234.038734	146219.945207	35.596877
1235.694979	146488.416973	35.601895
1236.749402	146752.297792	35.606912
1238.033393	147022.876874	35.611930
1239.415285	147305.058848	35.616948
1240.511951	147566.072353	35.621965
1241.920617	147831.487726	35.626983
1242.579697	148108.062839	35.632000
1244.005650	148373.010004	35.637018
1245.272393	148639.076113	35.642036
1246.391166	148915.961777	35.647053
1248.033919	149179.965713	35.652071
1248.959939	149452.118414	35.657088
1250.503290	149696.648487	35.662106
1251.381462	149968.102598	35.667124
1252.461725	150216.783956	35.672141
1254.169471	150478.363800	35.677159
1255.154964	150744.453358	35.682176
1256.640761	150996.801806	35.687194
1257.307523	151268.921739	35.692212
1258.486606	151533.665741	35.697229
1260.106766	151794.457402	35.702247
1261.066677	152076.009540	35.707264
1262.479562	152338.640311	35.712282
1263.805279	152624.004666	35.717300
1264.646150	152898.073482	35.722317
1266.207330	153165.150261	35.727335
1267.390935	153448.692300	35.732352
1268.546811	153728.575163	35.737370
1269.797284	154017.628090	35.742388
1270.665164	154299.173614	35.747405
1272.157607	154583.535445	35.752423
1273.442549	154883.206287	35.757440
1274.673761	155171.319560	35.762458
1276.028555	155461.710520	35.767476
1277.237680	155760.918542	35.772493
1278.672803	156054.586049	35.777511
1280.081365	156355.275144	35.782528
1281.263552	156651.589374	35.787546
1282.587937	156950.089591	35.792564
1283.879899	157250.195788	35.797581
1285.164020	157536.021342	35.802599
1286.710752	157846.695185	35.807616
1288.039534	158151.863673	35.812634
1289.434066	158445.365105	35.817652
1289.935173	158744.610916	35.822669
1291.994540	159039.402219	35.827687
1293.448560	159349.722286	35.832704
1294.702046	159646.122772	35.837722
1296.092753	159937.009450	35.842740
1297.779105	160232.682912	35.847757
1299.165923	160522.280318	35.852775
1300.237048	160836.138316	35.857792
1301.313235	161124.750942	35.862810
1302.477136	161418.375103	35.867828
1303.754427	161727.422732	35.872845
1305.184440	162024.191601	35.877863
1306.271635	162323.734288	35.882880
1307.839326	162632.727867	35.887898
1309.019893	162933.553541	35.892916
1310.097956	163249.471050	35.897933
1311.664062	163556.834908	35.902951
1312.744714	163865.169345	35.907968
1313.994460	164168.631310	35.912986
1315.618412	164483.275023	35.918004
1316.882998	164798.107298	35.923021
1318.202423	165105.611780	35.928039
1319.545789	165417.022426	35.933056
1320.700573	165724.621921	35.938074
1322.190751	166037.167343	35.943092
1323.433244	166351.189712	35.948109
1325.366404	166647.323562	35.953127
1326.558844	166958.909637	35.958144
1327.619836	167267.093676	35.963162
1329.107781	167584.662416	35.968180
1330.041993	167893.227011	35.973197
1331.739768	168195.348433	35.978215
1332.413941	168517.423259	35.983232
1334.064190	168824.924212	35.988250
1335.420535	169133.858948	35.993268
1336.624264	169437.313849	35.998285
1337.918917	169736.454038	36.003303
1339.013388	170037.431167	36.008320
1340.292245	170336.920493	36.013338
1342.114876	170628.314740	36.018356
1343.133739	170935.210892	36.023373
1344.196046	171238.231504	36.028391
1345.715670	171551.457299	36.033408
1346.927740	171855.269313	36.038426
1348.485000	172175.865924	36.043444
1349.599056	172492.451743	36.048461
1350.964534	172794.531288	36.053479
1352.361841	173122.318025	36.058496
1353.655680	173428.461638	36.063514
1355.094913	173750.611231	36.068532
1356.202947	174083.756974	36.073549
1357.835529	174397.604707	36.078567
1358.750920	174715.722868	36.083584
1360.049581	175052.092592	36.088602
1361.595369	175378.486829	36.093620
1363.059981	175712.726987	36.098637
1364.171968	176048.664840	36.103655
1365.630754	176382.415552	36.108672
1366.959787	176713.283663	36.113690
1368.692361	177047.323567	36.118708
1369.956694	177392.103865	36.123725
1371.548389	177723.633283	36.128743
1372.927840	178060.517726	36.133760
1374.055866	178386.543833	36.138778
1375.556964	178731.916038	36.143796
1376.841736	179077.326332	36.148813
1378.375228	179419.905629	36.153831
1379.618663	179766.076207	36.158848
1381.299782	180107.607622	36.163866
1382.561871	180451.469737	36.168884
1383.572212	180807.116049	36.173901
1385.546406	181137.182751	36.178919
1386.776879	181491.845396	36.183936
1388.328115	181831.416804	36.188954
1389.785882	182171.323144	36.193972
1390.932413	182524.737301	36.198989
1392.503259	182865.606702	36.204007
1394.104655	183219.521432	36.209024
1395.461032	183566.002850	36.214042
1396.713582	183910.701231	36.219060
1397.948334	184263.782152	36.224077
1399.276345	184601.910102	36.229095
1400.822129	184969.566656	36.234112
1402.123177	185311.422520	36.239130
1403.670078	185654.813836	36.244148
1404.970712	186021.730865	36.249165
1406.438712	186375.941778	36.254183
1408.386355	186736.638254	36.259200
1409.604679	187075.878250	36.264218
1411.068737	187441.000355	36.269236
1412.231158	187799.599212	36.274253
1413.824738	188150.398440	36.279271
1415.162662	188503.844316	36.284288
1416.419936	188857.584937	36.289306
1418.112361	189212.969500	36.294324
1419.341169	189577.331494	36.299341
1420.909660	189929.338800	36.304359
1422.197667	190271.239024	36.309376
1423.572620	190633.653799	36.314394
1425.247925	190995.741849	36.319412
1426.249104	191343.522379	36.324429
1427.939478	191689.819985	36.329447
1429.132046	192045.532477	36.334464
1430.546668	192390.914822	36.339482
1432.405504	192728.012090	36.344500
1433.336041	193081.590339	36.349517
1434.736373	193406.491013	36.354535
1436.015560	193760.713722	36.359552
1436.903600	194106.700408	36.364570
1438.450353	194457.670932	36.369588
1439.988742	194819.410417	36.374605
1441.649742	195174.098433	36.379623
1442.736893	195533.415516	36.384640
1444.129123	195896.061195	36.389658
1446.076636	196248.917690	36.394676
1447.140204	196621.473507	36.399693
1448.695669	196981.647962	36.404711
1450.321472	197350.636350	36.409728
1451.314961	197722.829067	36.414746
1453.080816	198090.249499	36.419764
1454.343959	198458.681813	36.424781
1455.912567	198837.857339	36.429799
1457.172215	199212.832807	36.434816
1458.718230	199593.692146	36.439834
1460.254387	199960.652751	36.444852
1462.030711	200341.046463	36.449869
1463.264810	200717.557851	36.454887
1464.776908	201097.935840	36.459904
1466.178400	201482.676376	36.464922
1467.590530	201865.512728	36.469940
1468.711432	202254.506362	36.474957
1470.822135	202637.688461	36.479975
1472.377018	203022.716583	36.484992
1473.867612	203418.384671	36.490010
1475.327053	203799.572760	36.495028
1476.801833	204186.207300	36.500045
1478.340127	204570.344704	36.505063
1480.184107	204956.731742	36.510080
1481.643966	205345.190378	36.515098
1482.963892	205723.770204	36.520116
1484.453884	206114.119644	36.525133
1486.037876	206500.151081	36.530151
1487.767692	206882.008244	36.535168
1489.285662	207276.142706	36.540186
1490.921485	207659.314299	36.545204
1492.211037	208040.475219	36.550221
1493.626268	208423.013922	36.555239
1495.526813	208819.137070	36.560256
1497.085918	209212.918653	36.565274
1498.442861	209598.532658	36.570292
1499.602814	209988.117371	36.575309
1501.264409	210377.062291	36.580327
1502.923291	210762.428583	36.585344
1503.807387	211153.638804	36.590362
1505.858443	211539.502512	36.595380
1507.383870	211942.597451	36.600397
1508.732783	212334.548884	36.605415
1510.473302	212730.704010	36.610432
1511.713728	213115.540331	36.615450
1513.466735	213510.807962	36.620468
1515.124378	213901.293025	36.625485
1516.678129	214295.250943	36.630503
1518.342396	214683.884248	36.635520
1519.567694	215077.036256	36.640538
1520.900602	215466.768863	36.645556
1522.817990	215863.924201	36.650573
1524.269906	216257.450031	36.655591
1526.190223	216646.861818	36.660608
1527.208602	217042.138725	36.665626
1528.995924	217422.432319	36.670644
1530.299707	217811.315641	36.675661
1532.481023	218181.260793	36.680679
1533.759339	218538.403354	36.685696
1534.720059	218920.998052	36.690714
1536.548738	219289.049813	36.695732
1537.943875	219657.911068	36.700749
1539.104378	220039.968907	36.705767
1540.589254	220406.227290	36.710784
1541.772572	220800.043721	36.715802
1543.250882	221187.920290	36.720820
1544.669830	221576.316027	36.725837
1546.054698	221970.560563	36.730855
1547.991480	222362.073788	36.735872
1549.050986	222770.903254	36.740890
1550.476583	223168.726556	36.745908
1552.298171	223577.204393	36.750925
1553.625948	223998.465041	36.755943
1555.233312	224432.939631	36.760960
1556.510284	224888.831597	36.765978
1558.178898	225306.941770	36.770996
1559.732599	225734.902136	36.776013
1560.711397	226163.720960	36.781031
1562.506388	226586.081765	36.786048
1563.593659	227022.962813	36.791066
1565.277212	227449.789907	36.796084
1566.985153	227900.719318	36.801101
1568.132645	228350.803035	36.806119
1570.074422	228790.698409	36.811136
1571.420806	229254.747958	36.816154
1573.225648	229697.539116	36.821172
1574.994381	230148.415080	36.826189
1576.703903	230600.216674	36.831207
1578.357570	231041.843116	36.836224
1579.560397	231495.966459	36.841242
1581.426526	231950.057788	36.846260
1583.051714	232410.667569	36.851277
1584.761365	232862.653733	36.856295
1586.424400	233302.430852	36.861312
1587.716908	233776.765471	36.866330
1589.343813	234222.240953	36.871348
1591.383249	234688.834341	36.876365
1592.982787	235146.534915	36.881383
1594.810558	235603.487740	36.886400
1596.386438	236067.646643	36.891418
1597.971297	236516.538774	36.896436
1599.821105	236975.955395	36.901453
1601.505616	237429.126169	36.906471
1603.274882	237884.011340	36.911488
1604.851284	238337.456105	36.916506
1606.746440	238785.641803	36.921524
1608.737056	239238.486700	36.926541
1609.828236	239684.774982	36.931559
1611.685603	240127.254282	36.936576
1612.833600	240589.055796	36.941594
1614.663990	241027.908806	36.946612
1616.170789	241485.359851	36.951629
1617.968150	241935.778099	36.956647
1619.360210	242380.065926	36.961664
1620.935213	242851.276402	36.966682
1622.881169	243288.691827	36.971700
1624.503062	243745.721524	36.976717
1625.801850	244197.674019	36.981735
1627.602511	244649.849158	36.986752
1629.412447	245108.450356	36.991770
1631.124021	245567.932194	36.996788
1632.667027	246024.419618	37.001805
1634.151233	246473.321945	37.006823
1635.730365	246920.380182	37.011840
1637.541430	247370.398220	37.016858
1639.332454	247813.993181	37.021876
1640.956813	248236.988981	37.026893
1642.195492	248675.239942	37.031911
1644.334832	249089.412934	37.036928
1645.474591	249528.925875	37.041946
1647.293688	249960.553681	37.046964
1648.986870	250396.114758	37.051981
1650.107898	250839.823523	37.056999
1652.339474	251277.150839	37.062016
1653.949803	251718.848856	37.067034
1655.202895	252162.943308	37.072052
1656.861148	252609.943314	37.077069
1658.431689	253056.246813	37.082087
1660.115804	253508.196741	37.087104
1661.951322	253963.957802	37.092122
1663.214520	254421.972919	37.097140
1664.848955	254861.280930	37.102157
1666.582292	255337.864785	37.107175
1668.154633	255794.457631	37.112192
1669.876368	256270.662683	37.117210
1671.777224	256730.707185	37.122228
1673.857858	257189.401115	37.127245
1674.985386	257659.963484	37.132263
1676.691588	258130.887573	37.137280
1678.592150	258602.160632	37.142298
1680.415105	259077.129990	37.147316
1682.032121	259541.260727	37.152333
1683.466945	260025.769554	37.157351
1685.535686	260490.638451	37.162368
1686.992626	260969.554715	37.167386
1688.708577	261451.933714	37.172404
1690.824854	261929.114963	37.177421
1692.389185	262409.156156	37.182439
1694.023374	262884.384380	37.187456
1695.833474	263370.608315	37.192474
1697.713464	263842.010352	37.197492
1699.801082	264316.045145	37.202509
1700.781639	264804.691500	37.207527
1702.862201	265282.207028	37.212544
1704.632942	265771.738241	37.217562
1706.340200	266254.115840	37.222580
1708.340699	266737.663915	37.227597
1709.648411	267215.661073	37.232615
1711.588405	267694.594835	37.237632
1713.288781	268173.847100	37.242650
1714.846756	268670.116950	37.247668
1716.734434	269147.355723	37.252685
1718.114315	269639.132051	37.257703
1720.246315	270120.622336	37.262720
1721.684053	270618.332055	37.267738
1723.511279	271105.688570	37.272756
1725.356591	271592.304690	37.277773
1726.932368	272091.818365	37.282791
1728.694870	272577.125669	37.287808
1730.341051	273069.792749	37.292826
1731.827346	273571.681122	37.297844
1733.515713	274066.651102	37.302861
1735.008127	274567.037854	37.307879
1736.819791	275070.139765	37.312896
1738.908498	275569.816375	37.317914
1740.228908	276080.440254	37.322932
1742.002328	276581.716354	37.327949
1743.675793	277095.963002	37.332967
1745.179878	277600.151764	37.337984
1747.264387	278109.831941	37.343002
1748.821171	278624.195816	37.348020
1750.813775	279134.371287	37.353037
1752.228875	279650.076849	37.358055
1753.959882	280132.376218	37.363072
1755.800354	280620.854321	37.368090
1757.105464	281121.307572	37.373108
1759.221757	281614.436792	37.378125
1760.705711	282112.444583	37.383143
1762.603040	282598.621769	37.388160
1764.391789	283093.960021	37.393178
1765.735551	283606.973443	37.398196
1767.702222	284109.975871	37.403213
1769.493933	284624.080541	37.408231
1771.067116	285127.525751	37.413248
1772.577903	285648.506333	37.418266
1774.436161	286172.552046	37.423284
1776.136921	286686.283771	37.428301
1777.863731	287212.379550	37.433319
1779.656993	287744.710980	37.438336
1781.858176	288272.756522	37.443354
1783.002874	288804.352791	37.448372
1784.654041	289331.646861	37.453389
1786.718454	289886.480678	37.458407
1788.004508	290429.375617	37.463424
1790.063965	290974.680529	37.468442
1791.730534	291521.698971	37.473460
1793.558876	292087.077755	37.478477
1794.874374	292640.118164	37.483495
1796.685681	293200.338420	37.488512
1798.440358	293770.039370	37.493530
1800.064302	294344.305599	37.498548
1802.003979	294912.979771	37.503565
1803.618149	295502.811459	37.508583
1805.447146	296079.727263	37.513600
1807.200281	296660.411565	37.518618
1808.909703	297261.215687	37.523636
1811.164750	297840.921706	37.528653
1812.915566	298448.950764	37.533671
1814.685040	299031.346329	37.538688
1816.578798	299623.699455	37.543706
1818.351814	300230.622007	37.548724
1820.103758	300829.239217	37.553741
1821.839952	301427.906119	37.558759
1823.596598	302029.588181	37.563776
1825.617480	302632.264044	37.568794
1827.177439	303250.529748	37.573812
1829.217662	303847.962659	37.578829
1831.209841	304458.301110	37.583847
1832.753186	305073.280890	37.588864
1834.886694	305682.851052	37.593882
1836.436437	306301.706775	37.598900
1838.790249	306915.015877	37.603917
1840.635331	307532.264715	37.608935
1842.332271	308145.851080	37.613952
1844.275016	308757.335250	37.618970
1845.952753	309377.848527	37.623988
1848.221993	309995.135736	37.629005
1850.334173	310606.781024	37.634023
1851.944233	311226.935510	37.639040
1854.048813	311831.207996	37.644058
1855.681842	312450.104528	37.649076
1857.704134	313060.907193	37.654093
1859.485214	313668.773632	37.659111
1861.346770	314296.708190	37.664128
1863.156198	314902.629857	37.669146
1864.914688	315518.585203	37.674164
1867.013339	316131.965177	37.679181
1869.098365	316755.397647	37.684199
1870.768819	317369.929466	37.689216
1872.771147	317972.085755	37.694234
1874.649412	318589.797238	37.699252
1876.649914	319182.116427	37.704269
1878.461024	319768.291508	37.709287
1880.220010	320357.542414	37.714304
1882.115824	320932.749515	37.719322
1883.916138	321536.811510	37.724340
1885.602986	322127.734204	37.729357
1887.631980	322722.048075	37.734375
1889.500046	323318.947391	37.739392
1891.473669	323909.856966	37.744410
1892.852881	324516.702348	37.749428
1894.940475	325115.198593	37.754445
1896.843619	325716.436113	37.759463
1898.588776	326328.281012	37.764480
1901.054073	326931.470148	37.769498
1902.725862	327560.477415	37.774516
1904.686915	328158.405778	37.779533
1906.402766	328773.860872	37.784551
1908.056034	329402.699119	37.789568
1909.867144	330013.022379	37.794586
1911.988001	330643.216906	37.799604
1913.900280	331272.728030	37.804621
1915.619726	331901.476954	37.809639
1917.386583	332541.279382	37.814656
1919.483724	333173.327890	37.819674
1921.238875	333819.540029	37.824692
1923.217036	334455.604249	37.829709
1925.163722	335107.151065	37.834727
1927.213105	335753.773696	37.839744
1929.244571	336399.934458	37.844762
1931.232632	337056.146557	37.849780
1933.426471	337705.691212	37.854797
1935.242962	338355.391527	37.859815
1936.569267	339011.561100	37.864832
1938.879314	339664.970696	37.869850
1940.724753	340323.677328	37.874868
1943.025829	340975.751422	37.879885
1945.079563	341636.665279	37.884903
1946.954998	342306.838559	37.889920
1948.972425	342948.501493	37.894938
1950.681538	343614.902380	37.899956
1952.777811	344292.245211	37.904973
1954.795413	344952.535953	37.909991
1956.905431	345616.456890	37.915008
1959.089817	346282.767185	37.920026
1961.185368	346951.011408	37.925044
1962.922069	347614.102580	37.930061
1965.336506	348274.483662	37.935079
1967.063272	348941.465448	37.940096
1969.243955	349596.993284	37.945114
1971.311273	350270.801818	37.950132
1973.150605	350927.432319	37.955149
1975.257587	351599.843750	37.960167
1977.243827	352265.768539	37.965184
1979.500693	352923.619753	37.970202
1981.286668	353591.663428	37.975220
1983.168437	354248.998072	37.980237
1985.353258	354916.701446	37.985255
1987.205601	355582.977484	37.990272
1989.312030	356248.312929	37.995290
1991.185995	356918.420949	38.000308
1993.571727	357580.415821	38.005325
1995.559284	358242.161321	38.010343
1997.599253	358906.348547	38.015360
1999.715486	359556.887768	38.020378
2001.385895	360228.954145	38.025396
2003.171933	360892.947634	38.030413
2005.683788	361544.581711	38.035431
2007.361032	362206.135649	38.040448
2009.491076	362842.893801	38.045466
2011.464069	363477.790195	38.050484
2013.159208	364106.379914	38.055501
2015.199946	364733.887610	38.060519
2017.520544	365379.857375	38.065536
2019.612630	366016.366512	38.070554
2021.270215	366660.470699	38.075572
2023.374094	367291.147386	38.080589
2025.492812	367935.381889	38.085607
2027.423216	368587.372875	38.090624
2029.285862	369232.895432	38.095642
2031.246667	369889.829984	38.100660
2033.114136	370544.916556	38.105677
2035.286946	371200.600381	38.110695
2037.295259	371867.078924	38.115712
2039.371138	372528.714998	38.120730
2041.362615	373201.715139	38.125748
2043.125299	373873.522931	38.130765
2045.196046	374545.622146	38.135783
2047.292821	375219.656996	38.140800
2049.297080	375895.190376	38.145818
2051.100443	376580.025538	38.150836
2053.247809	377272.626403	38.155853
2055.503359	377958.018827	38.160871
2057.158469	378660.765725	38.165888
2059.296453	379345.946712	38.170906
2061.231973	380048.440963	38.175924
2063.321894	380753.684256	38.180941
2065.668526	381464.220429	38.185959
2067.601893	382173.034677	38.190976
2070.170325	382886.546323	38.195994
2072.094889	383584.023120	38.201012
2074.133522	384290.568287	38.206029
2076.456145	384988.785872	38.211047
2078.132072	385713.462244	38.216064
2080.556329	386428.440789	38.221082
2082.820083	387141.604428	38.226100
2084.400565	387862.825109	38.231117
2086.706427	388574.935350	38.236135
2088.501210	389300.245141	38.241152
2090.901537	390017.148753	38.246170
2093.593697	390746.839509	38.251188
2095.536541	391463.024582	38.256205
2097.809728	392182.078705	38.261223
2099.549541	392910.759780	38.266240
2102.117075	393630.466069	38.271258
2104.395126	394349.594637	38.276276
2106.641497	395070.282577	38.281293
2108.707823	395792.072627	38.286311
2110.792655	396514.779771	38.291328
2113.334363	397224.620648	38.296346
2115.484406	397946.977693	38.301364
2117.406681	398658.837410	38.306381
2119.863953	399365.523019	38.311399
2121.604354	400098.233522	38.316416
2124.010117	400801.293972	38.321434
2125.998017	401517.354711	38.326452
2127.794263	402236.723136	38.331469
2130.018617	402955.546507	38.336487
2132.068516	403679.397200	38.341504
2134.492073	404395.439670	38.346522
2136.479079	405121.670396	38.351540
2138.082471	405842.776915	38.356557
2140.292972	406568.654056	38.361575
2142.677223	407313.154831	38.366592
2144.571185	408037.145204	38.371610
2146.316081	408768.031504	38.376628
2148.484928	409496.269496	38.381645
2150.976121	410199.381459	38.386663
2152.922087	410915.838456	38.391680
2154.948576	411607.489753	38.396698
2156.814577	412320.831787	38.401716
2159.230910	413043.764740	38.406733
2161.324071	413753.839015	38.411751
2163.130075	414472.299549	38.416768
2165.420400	415197.346636	38.421786
2167.754968	415914.540319	38.426804
2169.604252	416643.570547	38.431821
2171.827224	417359.222857	38.436839
2173.577502	418104.764958	38.441856
2175.999930	418842.931783	38.446874
2178.074675	419587.794323	38.451892
2179.848485	420335.621856	38.456909
2182.206081	421086.014770	38.461927
2184.427705	421850.814842	38.466944
2186.349646	422602.373390	38.471962
2188.518450	423368.882389	38.476980
2190.637422	424138.413901	38.481997
2192.962661	424914.064585	38.487015
2194.962994	425702.554300	38.492032
2196.931232	426476.391309	38.497050
2199.438939	427263.581916	38.502068
2201.177951	428050.316712	38.507085
2203.498805	428844.624770	38.512103
2205.392599	429650.924174	38.517120
2207.611982	430457.800499	38.522138
2210.111703	431261.211342	38.527156
2212.333817	432057.857530	38.532173
2214.664312	432877.945157	38.537191
2216.584672	433701.462797	38.542208
2219.179742	434518.462425	38.547226
2221.626327	435340.518775	38.552244
2223.805440	436156.415339	38.557261
2226.187541	436974.830247	38.562279
2227.996546	437798.320295	38.567296
2230.220864	438624.596262	38.572314
2232.811894	439454.930785	38.577332
2235.120403	440284.673927	38.582349
2237.452877	441114.129224	38.587367
2239.677726	441952.223381	38.592384
2242.154832	442780.681590	38.597402
2244.287990	443610.683134	38.602420
2246.502978	444448.633125	38.607437
2248.968075	445276.341111	38.612455
2251.218033	446115.738715	38.617472
2253.588812	446948.709947	38.622490
2256.031629	447774.100033	38.627508
2258.205046	448622.669104	38.632525
2260.451615	449445.396682	38.637543
2262.895833	450283.334151	38.642560
2265.610703	451110.421062	38.647578
2268.142698	451947.165150	38.652596
2269.931300	452783.391590	38.657613
2272.247849	453596.184737	38.662631
2274.484822	454434.242956	38.667648
2276.734534	455273.428056	38.672666
2278.949152	456114.607221	38.677684
2281.033870	456947.531745	38.682701
2283.254371	457782.422184	38.687719
2285.771224	458622.689537	38.692736
2288.198105	459472.289476	38.697754
2290.199725	460296.293354	38.702772
2292.452232	461142.919280	38.707789
2294.496673	461985.651353	38.712807
2297.064850	462829.171072	38.717824
2298.903383	463658.723872	38.722842
2301.498043	464477.452516	38.727860
2303.739029	465304.746642	38.732877
2306.159375	466115.955557	38.737895
2308.447396	466931.852327	38.742912
2310.538113	467744.007797	38.747930
2313.382977	468556.762610	38.752948
2315.457720	469376.431636	38.757965
2317.616429	470194.889586	38.762983
2319.901400	471016.777813	38.768000
2321.879008	471845.299716	38.773018
2324.528868	472675.291064	38.778036
2326.879140	473513.075146	38.783053
2329.450487	474343.409966	38.788071
2331.445383	475188.098503	38.793088
2333.426197	476034.771516	38.798106
2336.135499	476879.366301	38.803124
2338.196961	477736.807663	38.808141
2340.487501	478574.524917	38.813159
2342.716103	479442.111522	38.818176
2345.071596	480298.222951	38.823194
2347.732875	481161.616249	38.828212
2349.929675	482031.659886	38.833229
2352.088632	482900.960895	38.838247
2354.451523	483765.137152	38.843264
2356.899195	484657.480361	38.848282
2359.101365	485528.211695	38.853300
2361.530885	486410.675770	38.858317
2364.014373	487297.731066	38.863335
2366.325574	488191.483630	38.868352
2368.753690	489081.789516	38.873370
2371.341906	489967.279180	38.878388
2373.516527	490873.030468	38.883405
2375.680282	491759.154890	38.888423
2378.554065	492667.522983	38.893440
2380.657897	493580.360314	38.898458
2383.307741	494478.072463	38.903476
2385.765781	495389.140016	38.908493
2387.934659	496287.895655	38.913511
2390.605274	497211.796835	38.918528
2392.519825	498117.812467	38.923546
2395.184638	499030.516026	38.928564
2397.750321	499954.132240	38.933581
2400.234499	500871.657861	38.938599
2402.769777	501788.922551	38.943616
2404.760653	502712.177430	38.948634
2407.633043	503627.216429	38.953652
2409.924821	504550.520070	38.958669
2412.664008	505475.513029	38.963687
2414.803799	506401.762452	38.968704
2417.207139	507324.991077	38.973722
2419.764103	508251.267436	38.978740
2422.111929	509178.986969	38.983757
2424.655747	510101.226403	38.988775
2427.447849	511026.144050	38.993792
2429.713277	511960.974299	38.998810
2432.133584	512884.181597	39.003828
2434.606117	513810.047847	39.008845
2436.984579	514740.813967	39.013863
2439.871033	515670.281891	39.018880
2442.183058	516586.486039	39.023898
2444.696014	517507.238711	39.028916
2446.719279	518435.172076	39.033933
2449.257311	519363.871576	39.038951
2451.999383	520278.677522	39.043968
2454.408281	521220.485170	39.048986
2456.695115	522140.644989	39.054004
2459.353739	523081.792607	39.059021
2461.767580	523997.235262	39.064039
2464.344065	524893.709272	39.069056
2466.220364	525785.712924	39.074074
2468.607828	526684.679556	39.079092
2471.147785	527576.668361	39.084109
2473.894912	528476.122229	39.089127
2476.203217	529374.989765	39.094144
2478.074933	530293.811376	39.099162
2480.924186	531197.060061	39.104180
2482.790706	532120.148161	39.109197
2485.783280	533030.106269	39.114215
2488.227852	533944.124578	39.119232
2490.354419	534889.392391	39.124250
2492.725982	535805.066951	39.129268
2495.164715	536742.713734	39.134285
2497.373306	537684.815755	39.139303
2500.060736	538624.110042	39.144320
2502.239994	539595.576285	39.149338
2505.008892	540536.894448	39.154356
2507.200711	541506.467008	39.159373
2509.269192	542474.534564	39.164391
2512.099796	543449.200163	39.169408
2514.726156	544430.671885	39.174426
2517.541558	545397.307872	39.179444
2520.065358	546390.577765	39.184461
2522.481970	547378.112006	39.189479
2525.071990	548367.055506	39.194496
2527.237299	549362.785532	39.199514
2530.155614	550348.465356	39.204532
2532.584672	551364.568398	39.209549
2534.876089	552362.120243	39.214567
2537.458140	553362.566604	39.219584
2540.076364	554377.106076	39.224602
2542.558097	555390.134277	39.229620
2545.398265	556414.283264	39.234637
2547.604629	557437.604196	39.239655
2550.251572	558451.227569	39.244672
2552.956770	559486.467648	39.249690
2555.825272	560506.428528	39.254708
2558.229453	561541.255827	39.259725
2560.789921	562576.126538	39.264743
2563.659489	563601.874336	39.269760
2566.416505	564625.450799	39.274778
2568.639994	565660.835509	39.279796
2571.455430	566701.663594	39.284813
2574.288185	567739.994901	39.289831
2576.844428	568767.042275	39.294848
2579.439731	569806.902337	39.299866
2582.203874	570842.082052	39.304884
2584.488993	571883.831729	39.309901
2586.972889	572919.591089	39.314919
2589.690009	573955.979853	39.319936
2592.097851	575009.947351	39.324954
2594.783478	576049.681274	39.329972
2597.167615	577097.606553	39.334989
2599.912400	578143.126727	39.340007
2602.827486	579193.296244	39.345024
2605.553061	580246.567887	39.350042
2608.320393	581287.204175	39.355060
2610.540780	582324.933889	39.360077
2613.263731	583379.040845	39.365095
2615.843087	584425.459001	39.370112
2618.628317	585490.203569	39.375130
2621.278608	586543.697348	39.380148
2623.744111	587585.149132	39.385165
2626.546613	588637.282000	39.390183
2629.301756	589677.502260	39.395200
2631.934424	590739.903318	39.400218
2634.510716	591769.045800	39.405236
2637.163539	592783.906428	39.410253
2639.562622	593811.447852	39.415271
2642.527961	594820.270294	39.420288
2645.048122	595828.177981	39.425306
2647.833229	596835.454460	39.430324
2650.134107	597844.076312	39.435341
2652.463041	598862.922817	39.440359
2655.197274	599883.365781	39.445376
2657.738317	600918.371571	39.450394
2660.091812	601945.605170	39.455412
2663.141951	602965.072705	39.460429
2665.451240	604020.713731	39.465447
2668.548221	605062.913268	39.470464
2670.977134	606111.684058	39.475482
2673.513734	607154.084730	39.480500
2675.970697	608210.914037	39.485517
2678.498348	609264.280386	39.490535
2681.356990	610330.001038	39.495552
2683.992596	611405.061935	39.500570
2686.318087	612477.619563	39.505588
2689.210369	613556.832589	39.510605
2691.999826	614643.959389	39.515623
2694.833518	615717.970574	39.520640
2697.450401	616814.713377	39.525658
2700.134154	617900.836605	39.530676
2702.928987	618994.782430	39.535693
2705.322772	620107.079651	39.540711
2708.603388	621199.174635	39.545728
2711.276949	622317.647006	39.550746
2713.754475	623409.501677	39.555764
2716.791310	624517.242422	39.560781
2719.460160	625636.320602	39.565799
2722.453093	626749.833255	39.570816
2725.093399	627873.277876	39.575834
2727.524075	628983.053533	39.580852
2730.667132	630097.839211	39.585869
2733.689500	631235.746534	39.590887
2736.613892	632346.785376	39.595904
2739.152198	633478.188999	39.600922
2741.852582	634589.476438	39.605940
2744.690191	635712.801575	39.610957
2747.271491	636848.075290	39.615975
2750.260432	637966.390480	39.620992
2752.894699	639110.938479	39.626010
2755.400234	640243.556435	39.631028
2758.756541	641377.804780	39.636045
2761.718628	642512.740602	39.641063
2764.621624	643636.936700	39.646080
2767.493909	644777.769423	39.651098
2770.410894	645906.598978	39.656116
2773.444569	647017.982621	39.661133
2776.130436	648151.933767	39.666151
2779.016585	649270.869621	39.671168
2781.491576	650404.700402	39.676186
2784.161629	651527.207127	39.681204
2787.184983	652652.468842	39.686221
2789.824048	653794.058222	39.691239
2792.820066	654919.913685	39.696256
2795.569228	656052.854173	39.701274
2798.393860	657178.429595	39.706292
2801.336686	658309.931839	39.711309
2804.131280	659450.888004	39.716327
2806.973677	660573.529472	39.721344
2809.442567	661710.838508	39.726362
2811.954687	662845.667144	39.731380
2815.141915	663974.776008	39.736397
2817.687670	665124.361507	39.741415
2820.710268	666239.844025	39.746432
2823.209292	667352.048613	39.751450
2825.493378	668445.105169	39.756468
2828.709855	669547.780963	39.761485
2831.075681	670661.211755	39.766503
2833.734717	671765.411868	39.771520
2836.398628	672889.570568	39.776538
2839.127382	674011.943196	39.781556
2841.896973	675137.107533	39.786573
2844.101090	676275.302358	39.791591
2847.046268	677410.750676	39.796608
2849.910405	678568.982602	39.801626
2852.646412	679715.065936	39.806644
2855.141748	680880.124449	39.811661
2857.883543	682050.558323	39.816679
2860.574308	683222.142486	39.821696
2863.406614	684416.596701	39.826714
2865.896142	685610.603144	39.831732
2869.139782	686803.682731	39.836749
2871.761641	688009.465869	39.841767
2874.847617	689221.612984	39.846784
2877.721182	690433.582086	39.851802
2880.261371	691659.535292	39.856820
2883.250622	692874.777214	39.861837
2885.999568	694113.904007	39.866855
2888.628776	695350.347907	39.871872
2891.776288	696592.931485	39.876890
2894.568195	697851.663764	39.881908
2897.380686	699100.246648	39.886925
2900.303284	700359.341647	39.891943
2903.554669	701615.425283	39.896960
2906.348372	702883.545486	39.901978
2909.097776	704159.317161	39.906996
2912.533416	705428.594504	39.912013
2915.240031	706717.471948	39.917031
2918.203282	707994.523792	39.922048
2921.246425	709287.318734	39.927066
2924.131554	710578.260635	39.932084
2927.252767	711851.046009	39.937101
2930.397009	713154.970802	39.942119
2932.982752	714432.159516	39.947136
2936.721055	715729.600410	39.952154
2939.402635	717020.731664	39.957172
2942.425103	718301.021246	39.962189
2945.041918	719598.592488	39.967207
2947.977668	720904.959341	39.972224
2950.975718	722204.880091	39.977242
2953.723783	723515.119098	39.982260
2957.135970	724816.785528	39.987277
2960.251081	726128.525657	39.992295
2963.222047	727423.673669	39.997312
2966.266732	728741.035535	40.002330
2968.918280	730059.385440	40.007348
2972.491495	731354.303412	40.012365
2975.070389	732665.870010	40.017383
2978.041124	733970.048783	40.022400
2981.115406	735293.647544	40.027418
2984.280661	736595.640124	40.032436
2987.188737	737903.187913	40.037453
2990.324295	739225.730907	40.042471
2993.415796	740531.188354	40.047488
2996.589654	741837.847590	40.052506
2999.463994	743160.911221	40.057524
3002.656454	744461.066424	40.062541
3005.504369	745771.120795	40.067559
3008.548103	747073.529404	40.072576
3011.546572	748386.817408	40.077594
3014.404473	749697.984984	40.082612
3017.861946	750988.335879	40.087629
3020.419236	752273.102482	40.092647
3022.749248	753536.513517	40.097664
3026.259877	754805.973337	40.102682
3028.553414	756082.759737	40.107700
3031.633875	757359.006124	40.112717
3034.395451	758649.217468	40.117735
3037.062361	759932.532389	40.122752
3040.308847	761224.144900	40.127770
3042.900251	762538.077360	40.132788
3046.204107	763850.876025	40.137805
3049.008501	765171.936734	40.142823
3051.496056	766484.949349	40.147840
3054.488030	767829.061164	40.152858
3057.146494	769173.968028	40.157876
3060.067122	770524.042512	40.162893
3062.946429	771883.703864	40.167911
3065.884639	773264.228006	40.172928
3068.905897	774648.211720	40.177946
3071.721837	776041.985216	40.182964
3074.754147	777439.188224	40.187981
3077.890354	778853.286118	40.192999
3080.460733	780256.600967	40.198016
3083.615439	781684.178996	40.203034
3086.237344	783112.003614	40.208052
3089.361819	784558.001711	40.213069
3092.308298	786010.063057	40.218087
3095.217700	787475.513887	40.223104
3098.567515	788947.256699	40.228122
3101.335559	790432.266986	40.233140
3104.405447	791909.909022	40.238157
3107.533627	793405.160672	40.243175
3110.221243	794895.513860	40.248192
3113.184245	796411.456145	40.253210
3116.059051	797928.845968	40.258228
3119.339524	799455.528759	40.263245
3122.112754	800991.500835	40.268263
3125.189854	802537.257137	40.273280
3128.709381	804084.452067	40.278298
3131.375005	805657.355882	40.283316
3134.840421	807216.272778	40.288333
3138.151052	808779.355294	40.293351
3140.967717	810345.824460	40.298368
3144.304299	811913.750783	40.303386
3147.189756	813488.078605	40.308404
3150.316376	815067.467247	40.313421
3153.409197	816672.510494	40.318439
3156.739974	818257.263598	40.323456
3160.149822	819847.872310	40.328474
3162.904740	821451.525883	40.333492
3166.068237	823043.017445	40.338509
3169.361609	824651.511018	40.343527
3172.683518	826252.683341	40.348544
3175.891781	827860.013398	40.353562
3179.061524	829484.543536	40.358580
3182.170934	831091.676537	40.363597
3185.596134	832709.608685	40.368615
3188.946080	834308.694482	40.373632
3192.143570	835917.435351	40.378650
3195.226577	837535.524352	40.383668
3198.389287	839152.022802	40.388685
3201.679802	840768.868084	40.393703
3205.005624	842389.283091	40.398720
3208.422672	843997.503071	40.403738
3211.865788	845620.375293	40.408756
3215.133603	847218.853670	40.413773
3218.635453	848837.288084	40.418791
3221.884142	850441.940545	40.423808
3225.433333	852024.086617	40.428826
3228.190179	853583.727986	40.433844
3231.551801	855138.702695	40.438861
3234.804057	856696.213887	40.443879
3237.809515	858242.602883	40.448896
3241.269971	859791.726700	40.453914
3244.326753	861351.383077	40.458932
3247.608892	862893.445197	40.463949
3250.681090	864458.310920	40.468967
3253.683459	866019.779634	40.473984
3256.903104	867578.192716	40.479002
3259.897564	869159.381637	40.484020
3262.997696	870733.843089	40.489037
3266.216100	872325.774283	40.494055
3269.623594	873921.602303	40.499072
3272.662297	875512.418593	40.504090
3275.367455	877132.646287	40.509108
3278.704014	878747.200553	40.514125
3282.291042	880364.459074	40.519143
3285.022578	882006.920123	40.524160
3288.468178	883639.914384	40.529178
3291.565981	885296.552838	40.534196
3295.063245	886941.067132	40.539213
3298.379660	888600.681643	40.544231
3301.196345	890275.530684	40.549248
3304.744746	891936.748773	40.554266
3308.087132	893629.050388	40.559284
3311.314924	895313.831369	40.564301
3314.792828	896991.518352	40.569319
3317.643574	898699.063087	40.574336
3320.710992	900409.811763	40.579354
3324.045228	902112.582389	40.584372
3327.078087	903843.087900	40.589389
3330.898486	905560.226128	40.594407
3333.672076	907291.244037	40.599424
3336.670764	909028.031800	40.604442
3340.066873	910789.491830	40.609460
3343.598696	912536.912201	40.614477
3346.799114	914306.408185	40.619495
3349.795784	916073.829128	40.624512
3353.262948	917835.031418	40.629530
3356.468799	919615.285792	40.634548
3359.331601	921416.311844	40.639565
3363.047619	923208.252043	40.644583
3365.958224	925004.522227	40.649600
3369.348958	926813.913961	40.654618
3372.809992	928622.777191	40.659636
3376.166078	930440.046943	40.664653
3379.582559	932261.376162	40.669671
3383.005735	934091.935888	40.674688
3386.754620	935904.295540	40.679706
3390.217289	937742.763660	40.684724
3393.325508	939584.660128	40.689741
3396.726580	941403.108548	40.694759
3399.876112	943245.231908	40.699776
3403.644286	945067.972126	40.704794
3407.014579	946917.251090	40.709812
3410.469955	948759.264918	40.714829
3413.830638	950598.342122	40.719847
3416.901471	952441.573597	40.724864
3420.405320	954330.160198	40.729882
3423.555357	956234.460559	40.734900
3426.853600	958136.837103	40.739917
3430.713418	960033.508808	40.744935
3433.974820	961947.730115	40.749952
3437.464199	963846.040238	40.754970
3440.790027	965741.797828	40.759988
3444.341753	967656.414419	40.765005
3448.090437	969542.581221	40.770010
3451.252251	971399.669298	40.775015
3454.769246	973168.207855	40.780020
3457.975771	974884.354373	40.785024
3460.777847	976524.525953	40.790029
3464.020346	978094.313738	40.795034
3467.254120	979598.731924	40.800039
3470.817249	981008.682407	40.805044
3473.592428	982366.682800	40.810048
3476.271168	983616.739944	40.815053
3478.956447	984794.909332	40.820058
3481.269493	985906.955452	40.825063
3484.030239	986938.932817	40.830068
3485.772253	987911.701427	40.835072
3488.404967	988816.982373	40.840077
3490.761039	989634.431343	40.845082
3492.628727	990413.343056	40.850087
3494.429656	991112.439781	40.855092
3496.443876	991756.650996	40.860096
3498.290123	992340.114575	40.865101
3499.790385	992873.108368	40.870106
3501.107516	993350.651431	40.875111
3502.413119	993779.353445	40.880116
3504.097453	994170.752312	40.885120
3504.998982	994500.405285	40.890125
3506.384258	994791.781205	40.895130
3507.573713	995056.392451	40.900135
3508.549607	995273.405266	40.905140
3509.700947	995451.038539	40.910144
3510.833951	995605.492943	40.915149
3511.624283	995709.947581	40.920154
3512.312644	995794.747089	40.925159
3513.355804	995838.978753	40.930164
3514.469878	995871.513389	40.935168
3515.092253	995864.497272	40.940173
3515.643370	995828.864471	40.945178
3516.266726	995779.197325	40.950183
3516.954666	995696.702789	40.955188
3517.628276	995601.939587	40.960192
3518.105506	995478.284829	40.965197
3518.571237	995328.919850	40.970202
3518.663227	995190.325066	40.975207
3519.389211	995014.906620	40.980212
3519.759936	994834.671639	40.985216
3520.231009	994630.162753	40.990221
3520.783390	994412.581500	40.995226
3520.886559	994185.812537	41.000231
3520.988177	993942.767620	41.005236
3521.503227	993686.006434	41.010240
3521.603630	993432.711538	41.015245
3522.101240	993164.142158	41.020250
3522.149764	992874.102834	41.025255
3522.607996	992587.098999	41.030260
3522.742310	992284.056996	41.035264
3522.881676	991979.244033	41.040269
3523.453250	991661.675365	41.045274
3523.216462	991343.832306	41.050279
3523.493829	991013.899375	41.055284
3523.674135	990675.483890	41.060288
3523.798458	990336.277712	41.065293
3523.865881	989976.103302	41.070298
3523.476392	989631.481025	41.075303
3524.069027	989269.908073	41.080308
3524.101668	988917.666366	41.085312
3524.213196	988551.447260	41.090317
3524.439142	988185.380735	41.095322
3524.361163	987822.656173	41.100327
3524.284669	987423.045783	41.105332
3524.016711	987063.229693	41.110336
3523.850467	986684.257714	41.115341
3524.622796	986293.206082	41.120346
3524.238046	985920.169129	41.125351
3524.458289	985529.741297	41.130356
3524.462820	985147.224524	41.135360
3524.100875	984766.108353	41.140365
3524.081132	984369.396318	41.145370
3523.869879	983980.201799	41.150375
3524.242567	983595.373434	41.155380
3524.336172	983203.050468	41.160384
3524.158608	982809.866784	41.165389
3524.365437	982408.393766	41.170394
3524.025748	982026.895497	41.175399
3523.958359	981621.995861	41.180404
3523.937589	981229.458332	41.185408
3523.886941	980843.635379	41.190413
3523.955843	980449.857858	41.195418
3523.984396	980033.894097	41.200423
3523.954564	979636.463811	41.205428
3523.999537	979242.021003	41.210432
3523.755372	978852.384257	41.215437
3524.072103	978441.238009	41.220442
3523.613822	978050.898149	41.225447
3523.641569	977646.286894	41.230452
3523.623546	977251.228567	41.235456
3523.742008	976848.695181	41.240461
3523.502107	976453.911411	41.245466
3523.269015	976067.111841	41.250471
3523.242834	975654.355907	41.255476
3523.182729	975265.226015	41.260480
3522.812500	974868.595171	41.265485
3522.973697	974467.646389	41.270490
3523.254519	974084.440017	41.275495
3522.990327	973684.972720	41.280500
3522.883974	973301.875511	41.285504
3522.476844	972900.715094	41.290509
3522.584746	972508.632591	41.295514
3522.567500	972125.148664	41.300519
3522.871744	971730.633820	41.305524
3522.599021	971348.020071	41.310528
3522.170344	970954.354895	41.315533
3522.353493	970558.703523	41.320538
3522.086378	970182.955470	41.325543
3522.201458	969791.761879	41.330548
3521.990253	969411.356448	41.335552
3521.922245	969024.738625	41.340557
3522.079705	968642.851820	41.345562
3521.603663	968263.783703	41.350567
3522.048004	967881.799002	41.355572
3521.639591	967504.822405	41.360576
3521.524124	967127.381322	41.365581
3521.501753	966744.810678	41.370586
3521.609477	966368.359551	41.375591
3521.331120	965990.381184	41.380596
3521.621941	965614.242032	41.385600
3520.993585	965240.187677	41.390605
3521.347827	964868.590535	41.395610
3520.859652	964496.814430	41.400615
3520.964458	964123.154061	41.405620
3521.082291	963759.161778	41.410624
3520.903332	963392.649166	41.415629
3520.871775	963018.449846	41.420634
3520.815048	962652.653448	41.425639
3520.898929	962281.619316	41.430644
3520.757493	961907.267893	41.435648
3520.724152	961548.842121	41.440653
3520.838962	961170.482098	41.445658
3520.375567	960813.452954	41.450663
3520.392282	960440.939621	41.455668
3520.525628	960082.199143	41.460672
3520.287868	959722.125567	41.465677
3520.273101	959358.758780	41.470682
3520.179804	958992.833883	41.475687
3519.862424	958628.588869	41.480692
3520.146747	958275.689769	41.485696
3520.074027	957925.964652	41.490701
3519.974969	957559.949758	41.495706
3519.761449	957220.007989	41.500711
3519.395063	956849.972626	41.505716
3519.583636	956506.883297	41.510720
3519.166790	956158.088160	41.515725
3519.335874	955808.587051	41.520730
3519.154539	955465.300632	41.525735
3519.436095	955123.780890	41.530740
3519.308209	954775.639178	41.535744
3518.652959	954425.405535	41.540749
3519.279379	954078.568781	41.545754
3519.032015	953733.718970	41.550759
3519.018288	953393.617007	41.555764
3518.940917	953046.049436	41.560768
3518.552875	952704.595102	41.565773
3518.986549	952387.434701	41.570778
3518.458608	952052.442946	41.575783
3518.733800	951725.139052	41.580788
3518.342601	951396.967494	41.585792
3518.335805	951079.041569	41.590797
3518.634197	950746.314679	41.595802
3518.058690	950425.572078	41.600807
3517.852900	950100.730392	41.605812
3517.993881	949790.544597	41.610816
3517.933349	949471.379370	41.615821
3517.994604	949149.016564	41.620826
3517.896578	948844.840976	41.625831
3517.669816	948521.720611	41.630836
3517.913803	948201.181998	41.635840
3517.333438	947890.425740	41.640845
3517.500958	947575.316011	41.645850
3517.381716	947268.657572	41.650855
3517.493165	946953.231766	41.655860
3517.091525	946645.146759	41.660864
3516.952342	946348.775750	41.665869
3517.029301	946034.639625	41.670874
3516.921988	945740.621937	41.675879
3517.032351	945438.604021	41.680884
3517.202324	945142.974498	41.685888
3516.641073	944839.212698	41.690893
3516.783139	944528.038549	41.695898
3516.586523	944231.459511	41.700903
3516.798823	943942.267077	41.705908
3516.466573	943646.347287	41.710912
3516.328352	943347.217436	41.715917
3516.217161	943053.526355	41.720922
3516.107778	942770.165121	41.725927
3516.190468	942477.080049	41.730932
3516.258803	942200.844090	41.735936
3516.057751	941911.318918	41.740941
3515.876923	941610.754399	41.745946
3515.801128	941324.529744	41.750951
3515.805193	941027.734245	41.755956
3515.535082	940756.268999	41.760960
3515.470237	940481.880394	41.765965
3515.566473	940204.862812	41.770970
3515.223458	939936.050618	41.775975
3515.364765	939654.778702	41.780980
3515.514593	939373.010879	41.785984
3515.333804	939098.856143	41.790989
3515.247080	938821.028206	41.795994
3514.978053	938541.393772	41.800999
3515.090180	938284.406652	41.806004
3514.705837	938011.570777	41.811008
3514.597277	937756.703684	41.816013
3515.088214	937488.011613	41.821018
3514.582048	937224.648938	41.826023
3514.703713	936963.663250	41.831028
3514.363900	936696.218360	41.836032
3514.276778	936436.967321	41.841037
3514.519273	936168.344454	41.846042
3514.450101	935917.506182	41.851047
3514.346645	935649.681211	41.856052
3514.360102	935394.199480	41.861056
3514.293196	935150.711526	41.866061
3514.262122	934883.315298	41.871066
3514.008400	934630.814897	41.876071
3513.682707	934370.733582	41.881076
3513.805722	934123.712338	41.886080
3513.699437	933887.945390	41.891085
3513.347895	933629.463167	41.896090
3513.423748	933402.281898	41.901095
3513.476098	933151.579690	41.906100
3513.653647	932907.851815	41.911104
3513.318808	932671.108299	41.916109
3513.474537	932421.890243	41.921114
3513.539521	932181.123184	41.926119
3513.421560	931941.815334	41.931124
3513.432817	931708.619768	41.936128
3512.705760	931457.197556	41.941133
3512.797324	931219.934783	41.946138
3512.857396	931005.231061	41.951143
3512.676140	930769.049259	41.956148
3512.804789	930534.726428	41.961152
3512.261193	930316.349200	41.966157
3512.806397	930092.501656	41.971162
3512.763330	929859.617846	41.976167
3512.507817	929631.080798	41.981172
3512.589975	929403.822959	41.986176
3512.369029	929174.204045	41.991181
3512.212261	928944.372531	41.996186
3512.276493	928734.475184	42.001191
3512.348187	928511.311524	42.006196
3512.512433	928287.738995	42.011200
3511.948177	928065.718190	42.016205
3511.975367	927839.747648	42.021210
3511.856059	927626.666391	42.026215
3511.999920	927405.558310	42.031220
3511.987109	927196.093502	42.036224
3511.531186	926987.654394	42.041229
3511.883824	926773.308225	42.046234
3512.116866	926568.006476	42.051239
3511.949431	926340.947484	42.056244
3512.083267	926133.723350	42.061248
3511.458101	925922.002934	42.066253
3511.825098	925713.666907	42.071258
3511.765984	925500.202606	42.076263
3511.463743	925287.923318	42.081268
3511.453055	925079.817115	42.086272
3511.090700	924873.683361	42.091277
3511.316244	924660.138707	42.096282
3511.096749	924460.021906	42.101287
3511.162136	924256.870357	42.106292
3511.311093	924050.909177	42.111296
3510.958226	923850.983939	42.116301
3511.275269	923651.037042	42.121306
3510.992211	923456.085475	42.126311
3511.412456	923245.144840	42.131316
3511.448405	923046.087200	42.136320
3510.983129	922849.220421	42.141325
3511.173992	922644.448637	42.146330
3510.916395	922443.589871	42.151335
3510.968573	922247.385221	42.156340
3510.842260	922058.320140	42.161344
3510.550207	921870.141382	42.166349
3510.620680	921670.065393	42.171354
3510.460475	921482.043749	42.176359
3510.665913	921286.548428	42.181364
3510.550027	921093.119106	42.186368
3510.174444	920910.307670	42.191373
3510.376060	920720.275897	42.196378
3510.302568	920539.711040	42.201383
3510.080275	920353.969331	42.206388
3510.148224	920166.537800	42.211392
3510.128871	919982.674179	42.216397
3510.472608	919790.950678	42.221402
3510.063528	919613.489251	42.226407
3510.064587	919424.503490	42.231412
3510.090063	919253.405850	42.236416
3509.863968	919069.834004	42.241421
3509.617125	918899.732398	42.246426
3509.501084	918706.217812	42.251431
3509.540502	918545.681866	42.256436
3509.569257	918373.208540	42.261440
3509.360956	918198.940077	42.266445
3509.485929	918024.418614	42.271450
3509.206348	917853.615867	42.276455
3509.247626	917690.262963	42.281460
3509.315614	917520.740099	42.286464
3509.378670	917353.138033	42.291469
3509.297482	917189.790281	42.296474
3508.857250	917021.972136	42.301479
3509.305032	916861.415457	42.306484
3509.323161	916695.244623	42.311488
3508.449843	916533.548090	42.316493
3509.049356	916364.575613	42.321498
3509.179472	916213.295128	42.326503
3508.967986	916055.615559	42.331508
3509.088044	915899.321144	42.336512
3508.599134	915740.907874	42.341517
3508.910707	915569.165757	42.346522
3508.623050	915423.998791	42.351527
3508.672379	915253.349223	42.356532
3508.891778	915105.297541	42.361536
3508.589102	914958.387225	42.366541
3508.788830	914796.366104	42.371546
3507.955574	914636.051351	42.376551
3508.476572	914489.666918	42.381556
3509.003360	914334.512827	42.386560
3508.406452	914186.859731	42.391565
3508.398368	914027.739669	42.396570
3508.450448	913874.480875	42.401575
3508.354526	913728.563046	42.406580
3508.013846	913578.154159	42.411584
3508.463604	913432.234871	42.416589
3508.124619	913280.565220	42.421594
3508.206385	913138.841162	42.426599
3508.282726	912982.470640	42.431604
3508.565234	912830.589817	42.436608
3508.047140	912693.866586	42.441613
3508.086336	912539.223777	42.446618
3508.266995	912404.786927	42.451623
3508.049581	912257.404738	42.456628
3508.381536	912108.675463	42.461632
3507.973501	911957.751488	42.466637
3508.289036	911815.280267	42.471642
3508.043441	911672.705082	42.476647
3507.982596	911530.481225	42.481652
3507.849040	911381.809000	42.486656
3508.048879	911248.689897	42.491661
3508.049896	911096.036589	42.496666
3507.651013	910963.587478	42.501671
3507.829350	910829.401656	42.506676
3507.902579	910689.832586	42.511680
3507.800046	910554.915316	42.516685
3507.699186	910403.416205	42.521690
3507.772882	910262.486849	42.526695
3507.603465	910132.871606	42.531700
3507.640931	910002.737271	42.536704
3507.659428	909870.964285	42.541709
3507.833068	909717.762419	42.546714
3507.286263	909594.173338	42.551719
3507.799350	909460.091878	42.556724
3507.621498	909319.083491	42.561728
3507.126804	909190.367357	42.566733
3507.440329	909053.223901	42.571738
3506.891487	908927.499243	42.576743
3507.161145	908806.843192	42.581748
3507.476983	908675.667620	42.586752
3506.981947	908546.165221	42.591757
3507.542052	908412.050628	42.596762
3506.982881	908293.159080	42.601767
3506.869156	908156.256644	42.606772
3507.003606	908041.198816	42.611776
3506.685443	907914.834585	42.616781
3506.627628	907795.464035	42.621786
3506.576418	907672.618241	42.626791
3506.703339	907568.641632	42.631796
3506.922902	907453.654027	42.636800
3506.722795	907331.018073	42.641805
3506.725669	907200.052029	42.646810
3506.706515	907083.842358	42.651815
3506.692504	906970.619210	42.656820
3507.102242	906842.856847	42.661824
3506.626136	906728.451078	42.666829
3506.708505	906602.473213	42.671834
3506.344621	906499.329058	42.676839
3506.508729	906381.145428	42.681844
3506.786428	906259.082273	42.686848
3506.699518	906148.844578	42.691853
3506.576306	906020.765297	42.696858
3506.199221	905910.184832	42.701863
3506.453040	905798.822964	42.706868
3506.682674	905692.093292	42.711872
3506.129129	905582.982406	42.716877
3506.653682	905459.606952	42.721882
3506.554457	905343.856471	42.726887
3506.667061	905235.111384	42.731892
3506.741989	905106.689007	42.736896
3506.262771	904999.291032	42.741901
3506.495810	904889.361607	42.746906
3506.464609	904774.745873	42.751911
3506.479207	904674.689491	42.756916
3506.452668	904549.744464	42.761920
3506.076075	904438.748756	42.766925
3506.210880	904332.298147	42.771930
3506.155584	904228.385641	42.776935
3506.277793	904119.134756	42.781940
3506.210862	904013.579762	42.786945
3506.260872	903902.985596	42.791949
3506.209002	903791.923526	42.796954
3505.852635	903690.463120	42.801959
3505.622349	903581.549306	42.806964
3506.248054	903473.457398	42.811969
3505.771302	903372.783104	42.816973
3505.737790	903270.489822	42.821978
3505.548751	903180.091134	42.826983
3505.589633	903076.141358	42.831988
3505.488129	902978.872599	42.836993
3505.521903	902886.019593	42.841997
3505.445448	902777.257804	42.847002
3505.294582	902680.957177	42.852007
3505.346917	902591.667449	42.857012
3505.406935	902503.147212	42.862017
3505.346791	902416.382806	42.867021
3505.312212	902322.566482	42.872026
3505.483327	902237.209084	42.877031
3505.150929	902139.288095	42.882036
3505.374032	902054.208933	42.887041
3505.284183	901965.415306	42.892045
3505.591280	901862.171402	42.897050
3505.408525	901771.073201	42.902055
3505.144150	901661.548441	42.907060
3505.623766	901573.909776	42.912065
3505.214655	901492.594722	42.917069
3505.401805	901392.740842	42.922074
3505.215096	901317.758352	42.927079
3505.278096	901217.535640	42.932084
3505.255276	901127.462632	42.937089
3505.006053	901053.452373	42.942093
3505.174185	900953.014527	42.947098
3504.912819	900869.638573	42.952103
3504.973980	900774.815096	42.957108
3505.021908	900689.261360	42.962113
3504.725735	900615.832392	42.967117
3504.977063	900529.470275	42.972122
3504.993341	900450.387395	42.977127
3504.881473	900363.599782	42.982132
3505.049644	900284.006742	42.987137
3504.929933	900206.487808	42.992141
3505.164372	900112.397115	42.997146
3504.768847	900031.734618	43.002151
3504.827801	899950.706386	43.007156
3505.035881	899866.175981	43.012161
3504.803917	899785.289868	43.017165
3505.070293	899706.831322	43.022170
3504.788664	899622.474514	43.027175
3504.419160	899540.931547	43.032180
3504.945809	899456.825383	43.037185
3504.439634	899390.947857	43.042189
3504.818068	899297.206133	43.047194
3504.784576	899229.510446	43.052199
3504.672503	899146.953578	43.057204
3504.749355	899067.551563	43.062209
3504.642698	898985.281179	43.067213
3504.595880	898899.232948	43.072218
3504.745052	898837.973616	43.077223
3504.629505	898752.513984	43.082228
3505.041915	898675.562428	43.087233
3504.480550	898602.827016	43.092237
3504.969250	898517.747224	43.097242
3504.717553	898437.038199	43.102247
3504.421649	898362.227510	43.107252
3504.717805	898283.068112	43.112257
3504.806410	898214.277589	43.117261
3504.922115	898118.144680	43.122266
3504.555778	898045.852945	43.127271
3504.530497	897965.389672	43.132276
3504.850583	897881.004284	43.137281
3504.556006	897815.942910	43.142285
3504.717853	897737.764037	43.147290
3504.549571	897662.633245	43.152295
3504.417536	897580.926218	43.157300
3504.651522	897506.789756	43.162305
3504.547754	897429.616468	43.167309
3504.716276	897347.856558	43.172314
3504.689685	897273.953200	43.177319
3504.510605	897194.277195	43.182324
3504.641052	897116.964443	43.187329
3504.198619	897061.000526	43.192333
3504.491950	896973.707551	43.197338
3504.354489	896903.489079	43.202343
3504.403311	896840.099034	43.207348
3504.398309	896759.615276	43.212353
3504.069304	896689.232463	43.217357
3504.459997	896617.087604	43.222362
3504.323605	896543.289427	43.227367
3504.480089	896480.747247	43.232372
3504.361907	896401.243304	43.237377
3504.227779	896329.567765	43.242381
3504.172507	896249.471560	43.247386
3504.317511	896194.851740	43.252391
3504.076249	896127.732933	43.257396
3504.559056	896053.536470	43.262401
3504.046245	895986.943900	43.267405
3504.171332	895904.687163	43.272410
3503.842169	895844.343962	43.277415
3503.938155	895783.640160	43.282420
3504.293613	895717.191283	43.287425
3504.021804	895649.975218	43.292429
3504.198175	895575.919646	43.297434
3504.270871	895507.388799	43.302439
3504.039786	895437.264238	43.307444
3504.288464	895369.282593	43.312449
3503.956845	895315.602646	43.317453
3504.380437	895249.137073	43.322458
3504.291015	895179.952462	43.327463
3503.964751	895112.932307	43.332468
3504.141721	895052.014050	43.337473
3504.240841	894989.174948	43.342477
3504.393704	894908.928893	43.347482
3503.847625	894855.183275	43.352487
3503.755413	894786.960873	43.357492
3504.054374	894711.713996	43.362497
3503.845770	894644.765590	43.367501
3503.850507	894573.045002	43.372506
3503.941404	894518.417988	43.377511
3503.805370	894467.597575	43.382516
3503.731886	894398.110847	43.387521
3503.980748	894330.503406	43.392525
3503.679592	894266.272336	43.397530
3503.801763	894203.130768	43.402535
3503.636691	894145.352422	43.407540
3503.978202	894080.433380	43.412545
3503.517919	894028.985808	43.417549
3503.466294	893958.716777	43.422554
3503.694275	893920.785077	43.427559
3503.411116	893848.232770	43.432564
3503.762363	893784.565471	43.437569
3503.614814	893737.800642	43.442573
3503.634562	893675.346808	43.447578
3503.450997	893612.925787	43.452583
3503.659209	893565.424209	43.457588
3503.931847	893506.213814	43.462593
3503.695370	893462.555015	43.467597
3503.651014	893389.764173	43.472602
3503.398733	893331.508552	43.477607
3503.538362	893274.251247	43.482612
3503.746400	893214.275026	43.487617
3503.434524	893165.308908	43.492621
3503.542687	893111.632388	43.497626
3503.793684	893060.058874	43.502631
3503.525866	893002.479238	43.507636
3503.625044	892944.451813	43.512641
3503.336172	892890.355199	43.517645
3503.502374	892824.193826	43.522650
3503.443890	892764.643546	43.527655
3503.137946	892720.410378	43.532660
3503.595329	892665.125094	43.537665
3503.542114	892613.597672	43.542669
3503.615375	892569.687625	43.547674
3503.667435	892512.823884	43.552679
3503.461123	892454.164960	43.557684
3503.480004	892394.984856	43.562689
3502.956202	892339.181213	43.567693
3503.423996	892290.659310	43.572698
3503.231489	892239.828344	43.577703
3503.299426	892198.430461	43.582708
3503.515798	892136.604289	43.587713
3503.321717	892095.345529	43.592717
3503.319974	892037.035418	43.597722
3503.573603	891982.454019	43.602727
3503.349461	891933.172770	43.607732
3503.349389	891875.924473	43.612737
3503.038927	891824.819139	43.617741
3503.307461	891778.356523	43.622746
3503.385137	891726.122599	43.627751
3503.048449	891683.723888	43.632756
3503.302428	891639.390097	43.637761
3503.441346	891593.334167	43.642765
3503.094837	891534.785616	43.647770
3503.076594	891494.944196	43.652775
3503.136363	891445.998814	43.657780
3503.199604	891394.731356	43.662785
3503.163134	891343.963431	43.667789
3503.081689	891302.873822	43.672794
3503.454083	891244.397283	43.677799
3503.175528	891197.536522	43.682804
3503.215351	891148.108305	43.687809
3502.908443	891103.379199	43.692813
3502.847686	891056.094529	43.697818
3503.138605	891010.008868	43.702823
3503.355345	890969.834926	43.707828
3503.306470	890920.225920	43.712833
3503.106161	890866.192277	43.717837
3503.212343	890816.169940	43.722842
3503.454994	890770.380473	43.727847
3503.345391	890719.038727	43.732852
3503.280881	890666.334952	43.737857
3503.032352	890613.177386	43.742861
3503.058159	890573.225576	43.747866
3503.183947	890526.486159	43.752871
3502.950155	890482.030333	43.757876
3503.204185	890433.044298	43.762881
3503.242306	890390.767712	43.767885
3503.220550	890335.345444	43.772890
3503.172822	890293.469206	43.777895
3502.977484	890237.784402	43.782900
3503.282001	890197.880792	43.787905
3502.991057	890141.050016	43.792909
3503.067997	890104.955843	43.797914
3502.946125	890052.933020	43.802919
3502.911354	890018.210991	43.807924
3503.135305	889966.130405	43.812929
3502.718149	889936.888098	43.817933
3502.849969	889889.175135	43.822938
3502.838759	889843.903794	43.827943
3502.574805	889803.994370	43.832948
3502.808759	889769.420040	43.837953
3502.636560	889721.465555	43.842957
3502.678775	889686.051653	43.847962
3502.912839	889644.124251	43.852967
3502.733489	889607.005020	43.857972
3503.260105	889560.481931	43.862977
3503.055531	889525.978389	43.867981
3502.615919	889477.195232	43.872986
3503.105955	889428.935711	43.877991
3502.687667	889395.530791	43.882996
3502.962760	889350.885615	43.888001
3502.967854	889323.699032	43.893005
3502.650449	889275.281014	43.898010
3502.969588	889233.143106	43.903015
3502.758204	889196.219995	43.908020
3502.991552	889153.418397	43.913025
3502.713084	889115.248072	43.918029
3503.007885	889065.566418	43.923034
3502.825535	889025.154382	43.928039
3502.655841	888984.836729	43.933044
3502.794796	888931.212738	43.938049
3503.021000	888902.826696	43.943053
3502.604927	888870.966421	43.948058
3502.653549	888830.418208	43.953063
3502.367346	888792.537280	43.958068
3502.933483	888748.516774	43.963073
3502.492051	888715.885765	43.968077
3502.565666	888678.622103	43.973082
3502.554992	888644.952144	43.978087
3502.756449	888604.086883	43.983092
3503.076174	888556.815709	43.988097
3502.641298	888524.376051	43.993101
3502.355544	888483.203162	43.998106
3502.846135	888441.611785	44.003111
3502.183980	888406.983393	44.008116
3502.875214	888373.970304	44.013121
3502.398945	888344.149043	44.018125
3502.663925	888306.657922	44.023130
3502.955503	888260.550123	44.028135
3502.766474	888222.746199	44.033140
3503.087582	888178.277888	44.038145
3502.580882	888144.589963	44.043149
3502.531243	888117.697003	44.048154
3502.915155	888080.958957	44.053159
3502.640918	888045.200027	44.058164
3502.915074	887998.705934	44.063169
3502.965232	887966.279985	44.068173
3502.711861	887929.936284	44.073178
3502.796140	887888.601408	44.078183
3502.608127	887840.440308	44.083188
3502.780425	887795.412935	44.088193
3502.630358	887760.309186	44.093197
3502.717233	887719.940405	44.098202
3502.750991	887685.580104	44.103207
3502.758152	887654.611103	44.108212
3502.992719	887604.733239	44.113217
3502.823281	887568.276653	44.118221
3502.858541	887519.882537	44.123226
3503.231204	887475.690654	44.128231
3502.610209	887445.985360	44.133236
3502.636326	887394.785129	44.138241
3502.509953	887372.449958	44.143245
3502.737263	887328.668017	44.148250
3502.640187	887300.811260	44.153255
3502.693351	887261.219072	44.158260
3502.621269	887213.130415	44.163265
3502.428987	887190.708617	44.168269
3502.439647	887155.090790	44.173274
3502.429306	887114.056307	44.178279
3502.508158	887083.556351	44.183284
3502.687591	887048.297197	44.188289
3502.584591	887010.471150	44.193293
3502.574563	886967.983793	44.198298
3502.780235	886932.816399	44.203303
3502.438889	886894.544926	44.208308
3502.834630	886861.765475	44.213313
3502.661562	886829.176342	44.218317
3502.749088	886794.027570	44.223322
3502.497327	886758.837694	44.228327
3502.560643	886710.722546	44.233332
3502.848802	886680.573142	44.238337
3502.704768	886652.333829	44.243341
3502.536844	886610.644193	44.248346
3502.726852	886563.281285	44.253351
3502.147880	886541.114259	44.258356
3502.903182	886491.044198	44.263361
3502.770016	886470.836133	44.268365
3502.420450	886420.850705	44.273370
3502.360293	886388.337278	44.278375
3502.350330	886358.816092	44.283380
3502.596424	886323.154351	44.288385
3502.056795	886305.722995	44.293389
3502.530919	886261.311526	44.298394
3502.498319	886229.179857	44.303399
3502.505748	886201.397380	44.308404
3502.441408	886160.849024	44.313409
3502.456709	886141.389745	44.318413
3502.429315	886113.128580	44.323418
3502.522145	886080.394615	44.328423
3502.448711	886037.620465	44.333428
3502.807342	885993.129169	44.338433
3502.651443	885974.375154	44.343437
3502.384612	885933.277747	44.348442
3502.350761	885892.916098	44.353447
3502.213023	885864.284681	44.358452
3502.637136	885833.914862	44.363457
3502.160376	885811.050550	44.368461
3502.345077	885765.521299	44.373466
3502.487868	885746.910948	44.378471
3502.422755	885711.780752	44.383476
3502.303706	885663.977371	44.388481
3502.380678	885637.632853	44.393485
3502.473445	885607.606868	44.398490
3502.421131	885582.154681	44.403495
3502.239764	885551.689524	44.408500
3502.423954	885512.160589	44.413505
3502.358887	885488.065439	44.418509
3502.395224	885459.596963	44.423514
3502.477397	885423.085387	44.428519
3502.281709	885413.339636	44.433524
3502.542030	885366.245794	44.438529
3502.605141	885337.385053	44.443533
3502.489526	885298.097681	44.448538
3502.833911	885264.736778	44.453543
3502.234522	885231.047100	44.458548
3502.538343	885196.433887	44.463553
3502.339975	885177.684287	44.468557
3502.533612	885141.152572	44.473562
3502.838736	885102.278637	44.478567
3502.225733	885069.945710	44.483572
3502.671908	885023.786648	44.488577
3502.368435	884996.727350	44.493581
3502.575877	884966.388694	44.498586
3502.688578	884932.289495	44.503591
3502.543555	884895.424748	44.508596
3502.659388	884853.966171	44.513601
3502.622873	884819.600429	44.518605
3502.634908	884784.839193	44.523610
3502.882334	884747.812027	44.528615
3502.554899	884719.496676	44.533620
3502.505546	884681.065621	44.538625
3502.416651	884645.061457	44.543629
3502.807625	884605.782756	44.548634
3502.654895	884578.309363	44.553639
3502.389337	884549.982988	44.558644
3502.805303	884513.991659	44.563649
3502.795771	884478.263867	44.568653
3502.708610	884440.612073	44.573658
3502.710282	884403.913692	44.578663
3502.326812	884372.313682	44.583668
3502.687381	884329.455422	44.588673
3502.148100	884297.783847	44.593677
3502.071669	884267.391481	44.598682
3502.414792	884240.512613	44.603687
3502.177845	884217.505655	44.608692
3502.464398	884179.984264	44.613697
3502.454887	884157.617427	44.618701
3502.851073	884106.520819	44.623706
3502.626842	884072.084746	44.628711
3502.164536	884043.981985	44.633716
3502.531150	884002.088670	44.638721
3502.472054	883977.114738	44.643725
3502.424781	883936.838525	44.648730
3502.343015	883913.223771	44.653735
3502.069145	883891.286813	44.658740
3502.302807	883855.515123	44.663745
3502.185446	883826.386092	44.668749
3502.109309	883805.675138	44.673754
3502.210723	883772.345705	44.678759
3501.708338	883754.997347	44.683764
3502.391727	883724.380115	44.688769
3502.343658	883700.662104	44.693773
3502.125609	883667.965753	44.698778
3502.287537	883645.181332	44.703783
3502.116483	883622.935895	44.708788
3502.933966	883591.327450	44.713793
3502.626607	883554.480935	44.718797
3502.687599	883510.213351	44.723802
3502.501726	883484.289747	44.728807
3502.404061	883448.182766	44.733812
3502.430783	883418.931109	44.738817
3502.488790	883389.964689	44.743821
3502.307034	883338.859718	44.748826
3502.390730	883325.190542	44.753831
3502.390574	883280.156504	44.758836
3502.752809	883251.429816	44.763841
3502.534079	883225.316774	44.768845
3502.308904	883188.067000	44.773850
3502.474583	883154.045493	44.778855
3502.397803	883128.102327	44.783860
3502.130179	883093.764456	44.788865
3502.239020	883061.591942	44.793869
3502.147290	883025.965620	44.798874
3502.471826	883001.117995	44.803879
3502.204674	882980.435573	44.808884
3502.168871	882928.334420	44.813889
3502.325391	882911.456100	44.818893
3502.485990	882883.826217	44.823898
3502.687673	882852.412088	44.828903
3502.458805	882825.330371	44.833908
3502.418381	882786.110474	44.838913
3502.365613	882773.431049	44.843917
3502.552424	882736.788502	44.848922
3502.631326	882699.679217	44.853927
3502.322495	882675.515703	44.858932
3502.560931	882634.795974	44.863937
3502.486462	882606.331778	44.868941
3502.242295	882566.175377	44.873946
3502.747871	882533.547145	44.878951
3502.102406	882519.705634	44.883956
3502.631117	882481.745968	44.888961
3502.513277	882448.445084	44.893965
3502.236128	882403.062455	44.898970
3502.781649	882378.175771	44.903975
3502.074706	882354.270241	44.908980
3502.328940	882321.294781	44.913985
3502.048799	882287.632263	44.918989
3502.183909	882264.653137	44.923994
3502.570499	882223.518670	44.928999
3502.336747	882208.736793	44.934004
3502.539271	882162.982668	44.939009
3502.357212	882138.796039	44.944013
3502.335062	882109.448994	44.949018
3502.615028	882072.108854	44.954023
3502.342214	882043.674589	44.959028
3502.327561	882004.929533	44.964033
3502.647293	881977.559749	44.969037
3502.264712	881947.883796	44.974042
3502.514538	881918.975334	44.979047
3502.336636	881899.921165	44.984052
3502.224165	881852.279086	44.989057
3502.198011	881843.371245	44.994061
3502.376690	881803.043047	44.999066
3502.086779	881779.938296	45.004071
3501.988230	881751.377020	45.009076
3502.290313	881716.452796	45.014081
3502.351035	881695.130543	45.019085
3502.313650	881669.271267	45.024090
3502.173210	881631.997580	45.029095
3501.937200	881617.698951	45.034100
3502.092859	881577.954245	45.039105
3502.233398	881557.199595	45.044109
3502.428413	881532.948327	45.049114
3502.499078	881509.298710	45.054119
3501.790995	881467.854893	45.059124
3502.090830	881440.582753	45.064129
3502.323721	881421.653097	45.069133
3501.975826	881385.477682	45.074138
3502.200315	881370.133781	45.079143
3502.107874	881333.625318	45.084148
3502.215931	881302.315158	45.089153
3502.064090	881288.195614	45.094157
3501.968804	881266.122450	45.099162
3502.012793	881229.978387	45.104167
3502.069924	881218.343175	45.109172
3502.138652	881180.644617	45.114177
3502.146963	881147.606171	45.119181
3502.155540	881132.781638	45.124186
3502.404580	881099.509492	45.129191
3502.117956	881071.750952	45.134196
3502.379079	881036.829420	45.139201
3502.168762	881015.936886	45.144205
3502.105191	880996.764044	45.149210
3502.451376	880974.713930	45.154215
3501.870088	880944.968725	45.159220
3502.214922	880912.551713	45.164225
3502.007420	880887.395215	45.169229
3502.098254	880867.808961	45.174234
3502.080845	880826.053012	45.179239
3501.822783	880811.852928	45.184244
3502.253995	880783.780972	45.189249
3501.757442	880766.422720	45.194253
3501.760468	880744.331388	45.199258
3501.900894	880716.888361	45.204263
3501.872079	880700.906207	45.209268
3502.280822	880683.689227	45.214273
3501.888883	880661.662656	45.219277
3501.970116	880635.391696	45.224282
3502.330678	880598.416439	45.229287
3502.128105	880580.815414	45.234292
3501.731332	880555.010419	45.239297
3501.798578	880535.233152	45.244301
3501.636759	880521.210291	45.249306
3501.783605	880493.183795	45.254311
3501.697265	880470.621682	45.259316
3501.978477	880458.172884	45.264321
3501.845218	880426.025741	45.269325
3501.580516	880408.822015	45.274330
3501.759716	880402.978802	45.279335
3501.821186	880377.582003	45.284340
3501.792255	880348.711712	45.289345
3501.892598	880340.846602	45.294349
3502.100972	880309.417705	45.299354
3502.320712	880293.102795	45.304359
3502.011730	880270.479695	45.309364
3502.146225	880242.550934	45.314369
3502.218624	880211.047015	45.319373
3502.004058	880186.470057	45.324378
3502.145807	880162.900186	45.329383
3502.203259	880141.960409	45.334388
3502.119810	880119.590267	45.339393
3502.233265	880091.858055	45.344397
3501.906385	880074.469787	45.349402
3502.271737	880040.687960	45.354407
3501.961238	880028.529544	45.359412
3501.810337	879992.409947	45.364417
3501.991674	879981.042521	45.369421
3501.820961	879956.651177	45.374426
3502.251406	879912.101636	45.379431
3501.842174	879900.928259	45.384436
3502.055726	879875.698036	45.389441
3502.213818	879855.128271	45.394445
3502.288631	879832.052622	45.399450
3502.094945	879800.008902	45.404455
3501.812910	879782.612377	45.409460
3501.972917	879755.549246	45.414465
3502.003072	879740.039286	45.419469
3501.945602	879705.743754	45.424474
3502.186079	879680.217533	45.429479
3501.970605	879663.875672	45.434484
3501.972043	879633.737052	45.439489
3501.976323	879623.464097	45.444493
3501.668927	879590.275061	45.449498
3502.086234	879567.917218	45.454503
3501.791110	879544.223020	45.459508
3501.830292	879516.015773	45.464513
3501.457432	879513.751406	45.469517
3501.613042	879501.515097	45.474522
3501.961036	879467.248277	45.479527
3501.919589	879454.075225	45.484532
3501.852373	879434.219486	45.489537
3501.608610	879408.481131	45.494541
3501.738222	879396.442711	45.499546
3502.016167	879376.529908	45.504551
3501.694756	879354.777528	45.509556
3501.598564	879325.913279	45.514561
3501.625876	879328.428579	45.519565
3501.902211	879297.564545	45.524570
3501.917877	879278.857592	45.529575
3501.674088	879273.082950	45.534580
3501.819496	879233.517852	45.539585
3501.984029	879217.887457	45.544589
3501.767023	879201.253811	45.549594
3501.955165	879171.082052	45.554599
3501.592218	879174.049381	45.559604
3501.854250	879153.750782	45.564609
3501.985459	879124.266577	45.569613
3501.936925	879108.767913	45.574618
3502.038383	879079.288385	45.579623
3501.566159	879062.308723	45.584628
3501.825995	879042.397773	45.589633
3501.906363	879015.150514	45.594637
3501.674636	879004.818442	45.599642
3501.829332	878988.413707	45.604647
3501.597951	878975.270873	45.609652
3501.935920	878937.901201	45.614657
3502.044167	878940.597173	45.619661
3502.017004	878905.128928	45.624666
3501.998223	878887.007924	45.629671
3501.776625	878873.087883	45.634676
3501.910458	878839.628057	45.639681
3501.752726	878829.865013	45.644685
3501.696595	878801.379271	45.649690
3501.848355	878775.379125	45.654695
3501.926694	878774.397043	45.659700
3501.869422	878737.188137	45.664705
3501.580369	878714.749585	45.669709
3501.501244	878708.365712	45.674714
3501.866546	878694.251626	45.679719
3501.867266	878668.469741	45.684724
3501.731692	878658.121214	45.689729
3501.772411	878636.403426	45.694733
3501.712464	878616.640647	45.699738
3501.738240	878597.639082	45.704743
3501.536357	878591.081456	45.709748
3501.981892	878560.573380	45.714753
3501.677439	878543.176864	45.719757
3502.148381	878529.044978	45.724762
3501.625880	878502.670083	45.729767
3501.892399	878491.576526	45.734772
3501.739726	878477.741116	45.739777
3501.842404	878443.799533	45.744781
3501.840777	878433.331613	45.749786
3502.285002	878403.501437	45.754791
3501.894429	878390.189660	45.759796
3501.716424	878364.435888	45.764801
3501.803724	878323.420297	45.769805
3501.639828	878313.851269	45.774810
3501.923155	878280.557492	45.779815
3501.648317	878204.899435	45.784820
3501.862794	878064.601902	45.789825
3501.873227	877877.126329	45.794829
3501.798537	877639.637313	45.799834
3501.758959	877323.800688	45.804839
3501.752155	876954.715013	45.809844
3501.505191	876516.416929	45.814849
3501.418666	876033.939712	45.819853
3501.150143	875491.133924	45.824858
3501.236687	874875.771182	45.829863
3500.725341	874208.355489	45.834868
3500.696088	873477.438291	45.839873
3500.630475	872695.791643	45.844877
3499.809888	871832.947705	45.849882
3499.917942	870921.106197	45.854887
3499.391157	869943.321721	45.859892
3499.261629	868887.839118	45.864897
3498.627137	867783.897096	45.869901
3498.284985	866602.493050	45.874906
3498.267918	865346.587929	45.879911
3497.556486	864032.335718	45.884916
3496.969825	862644.014575	45.889921
3496.886665	861202.509103	45.894925
3496.372506	859679.544833	45.899930
3496.044328	858091.007759	45.904935
3495.007778	856429.796596	45.909940
3494.406719	854683.890720	45.914945
3493.957312	852898.627161	45.919949
3493.588234	851040.004043	45.924954
3493.233457	849096.378106	45.929959
3492.014638	847092.954128	45.934964
3491.600193	845021.313059	45.939969
3490.710925	842883.746303	45.944973
3489.764511	840658.421031	45.949978
3489.354616	838373.590970	45.954983
3488.593187	836032.319441	45.959988
3487.870834	833602.166630	45.964993
3486.936097	831123.222625	45.969997
3486.160462	828573.389878	45.975002
3485.201399	825933.194342	45.980007
3483.857293	823253.760560	45.985012
3483.432832	820495.258581	45.990017
3482.452773	817680.351063	45.995021
3481.286224	814812.731776	46.000026
3480.861517	811859.812271	46.005031
3479.434230	808839.172198	46.010036
3478.284684	805749.440533	46.015041
3477.206470	802607.537422	46.020045
3476.165539	799391.914937	46.025050
3475.483154	796120.887102	46.030055
3473.847635	792771.028116	46.035060
3473.116968	789359.129932	46.040065
3472.035842	785899.137790	46.045069
3470.506737	782352.103742	46.050074
3469.399287	778745.771751	46.055079
3467.958793	775078.075683	46.060084
3466.715460	771355.945274	46.065089
3465.628528	767575.181207	46.070093
3464.184746	763713.013420	46.075098
3462.878657	759790.862931	46.080103
3461.296006	755828.913742	46.085108
3459.889638	751784.425442	46.090113
3458.785660	747676.194391	46.095117
3457.348043	743514.134646	46.100122
3455.935250	739276.407141	46.105127
3454.349106	734981.606650	46.110132
3453.122405	730622.446872	46.115137
3451.525083	726213.338984	46.120141
3449.641910	721730.318921	46.125146
3448.106096	717188.516873	46.130151
3446.654272	712582.598649	46.135156
3445.084838	707918.431540	46.140161
3443.326091	703201.875134	46.145165
3441.379241	698412.195078	46.150170
3439.932100	693568.141385	46.155175
3437.756479	688679.068116	46.160180
3436.170930	683719.424032	46.165185
3434.339100	678697.836773	46.170189
3432.182824	673632.599078	46.175194
3430.883232	668487.573485	46.180199
3428.699994	663310.263605	46.185204
3426.702219	658050.552410	46.190209
3425.031315	652737.549240	46.195213
3422.767634	647368.313996	46.200218
3420.565146	641947.393663	46.205223
3418.486034	636488.550869	46.210228
3416.652060	630963.867114	46.215233
3414.643064	625391.437462	46.220237
3412.364043	619767.142134	46.225242
3410.041620	614076.773334	46.230247
3407.891553	608338.856433	46.235252
3405.878321	602551.419552	46.240257
3403.665898	596716.404861	46.245261
3401.165806	590829.941528	46.250266
3398.814213	584881.531737	46.255271
3396.550532	578897.403790	46.260276
3393.857409	572857.875324	46.265281
3391.677336	566787.135286	46.270285
3389.083996	560662.941078	46.275290
3386.866724	554472.754224	46.280295
3384.257012	548268.696413	46.285300
3381.595393	541997.550476	46.290305
3378.789264	535694.978579	46.295309
3376.303619	529342.454630	46.300314
3373.829265	522943.819881	46.305319
3370.859488	516507.857329	46.310324
3368.343894	510018.867240	46.315329
3365.577479	503494.617773	46.320333
3362.517645	496944.604459	46.325338
3359.754155	490350.202641	46.330343
3356.710575	483717.706097	46.335348
3353.817469	477047.987812	46.340353
3351.329173	470332.126041	46.345357
3348.088686	463600.591950	46.350362
3345.118711	456822.053351	46.355367
3341.610391	450025.477226	46.360372
3338.872257	443186.413652	46.365377
3335.830988	436311.067648	46.370381
3332.556891	429418.103171	46.375386
3329.282287	422485.642414	46.380391
3326.144747	415539.688012	46.385396
3322.895179	408558.334212	46.390401
3319.650933	401549.189484	46.395405
3316.009254	394509.996747	46.400410
3312.835668	387463.502474	46.405415
3309.511457	380391.434617	46.410420
3306.080478	373269.396292	46.415425
3302.300644	366143.518130	46.420429
3298.759960	359008.932181	46.425434
3295.285496	351834.790300	46.430439
3291.526134	344679.516010	46.435444
3287.952677	337484.776938	46.440449
3284.264138	330289.562653	46.445453
3280.480970	323067.462318	46.450458
3276.876415	315848.350457	46.455463
3273.048555	308620.343878	46.460468
3269.197651	301379.629306	46.465473
3265.390783	294113.629789	46.470477
3261.603290	286857.911798	46.475482
3257.529343	279587.816251	46.480487
3253.608483	272320.451556	46.485492
3249.951696	265049.424609	46.490497
3245.723452	257765.696473	46.495501
3241.420037	250486.470520	46.500506
3237.522992	243209.316633	46.505511
3233.609025	235927.140654	46.510516
3229.497653	228651.399423	46.515521
3225.318151	221298.057269	46.520525
3220.994899	214015.885937	46.525530
3216.678897	206742.409856	46.530535
3212.253208	199498.119084	46.535540
3207.720387	192245.323099	46.540545
3203.364682	185016.216786	46.545549
3199.112079	177797.637935	46.550554
3194.428556	170585.640842	46.555559
3189.345790	163407.963269	46.560564
3184.869883	156235.122915	46.565569
3180.584787	149089.211280	46.570573
3175.515189	141979.427191	46.575578
3170.511807	134872.676562	46.580583
3165.449585	127799.374794	46.585588
3160.572201	120759.141051	46.590593
3155.553751	113754.963580	46.595597
3149.984317	106785.026707	46.600602
3144.760268	99851.742278	46.605607
3139.311674	92958.641061	46.610612
3133.828087	86121.613607	46.615617
3127.910817	79329.247563	46.620621
3121.443278	72606.132094	46.625626
3115.213320	65931.324277	46.630631
3107.866119	59355.982652	46.635636
3097.657838	52918.358372	46.640641
3079.089214	46818.027198	46.645645
3060.006960	40943.215360	46.650650
3042.249611	35311.594360	46.655655
3024.532682	29982.987815	46.660660
3007.686784	24954.585655	46.665665
2991.342203	20251.526061	46.670669
2974.774961	15900.817086	46.675674
2956.134200	11950.083424	46.680679
2934.083034	8472.376711	46.685684
2910.366552	5447.760533	46.690689
2887.890980	2843.937070	46.695693
2862.464553	785.384635	46.700698
2797.490114	320.418971	46.705703
2745.868341	321.489351	46.710708
2729.311176	310.828206	46.715713
2738.877786	307.887229	46.720717
2760.320308	293.854071	46.725722
2783.128083	299.769674	46.730727
2798.825308	308.927533	46.735732
2806.301504	297.538000	46.740737
2807.433050	292.724061	46.745741
2804.337330	297.770217	46.750746
2800.472665	287.755364	46.755751
2795.460232	293.853466	46.760756
2791.496702	295.189897	46.765761
2788.605115	284.013186	46.770765
2785.779360	296.132951	46.775770
2783.787375	277.202629	46.780775
2781.300075	285.220236	46.785780
2778.826805	285.170540	46.790785
2775.950166	284.081889	46.795789
2772.922719	282.493981	46.800794
2770.003651	273.636652	46.805799
2767.049979	282.239964	46.810804
2764.257393	278.650937	46.815809
2760.947206	276.837753	46.820813
2757.687022	281.591767	46.825818
2754.346391	275.469707	46.830823
2751.221014	269.979546	46.835828
2748.561652	274.781247	46.840833
2745.062659	270.243542	46.845837
2741.690692	282.089545	46.850842
2738.587027	265.102599	46.855847
2734.897120	274.538628	46.860852
2731.798974	269.630882	46.865857
2728.903614	266.111726	46.870861
2725.108035	264.672307	46.875866
2721.782839	267.087906	46.880871
2718.293217	279.910444	46.885876
2715.294456	271.679643	46.890881
2712.131184	265.383108	46.895885
2708.430630	264.966830	46.900890
2705.608013	263.827866	46.905895
2701.881439	268.081842	46.910900
2698.539081	261.761588	46.915905
2695.295401	274.178467	46.920909
2691.650657	274.667475	46.925914
2688.609024	268.386009	46.930919
2685.002853	263.161131	46.935924
2681.633249	265.575006	46.940929
2678.482509	264.730566	46.945933
2674.460300	267.532758	46.950938
2671.358018	252.951250	46.955943
2667.629336	249.416514	46.960948
2664.694181	263.166642	46.965953
2661.436432	254.807333	46.970957
2657.552607	257.301344	46.975962
2654.127196	247.651864	46.980967
2650.743968	258.890761	46.985972
2647.627721	254.953039	46.990977
2644.492405	258.018574	46.995981
2640.726431	253.262152	47.000986
2637.435751	247.193122	47.005991
2633.742617	248.598719	47.010996
2629.916480	254.268719	47.016001
2626.803485	249.569526	47.021005
2623.192206	253.620210	47.026010
2620.109966	239.689832	47.031015
2616.849397	248.353715	47.036020
2612.595238	254.373800	47.041025
2608.803640	247.098029	47.046029
2605.657209	253.548251	47.051034
2602.842672	254.069630	47.056039
2599.135197	244.266641	47.061044
2595.815273	247.539883	47.066049
2592.725181	243.751416	47.071053
2589.038322	244.339805	47.076058
2584.976875	246.580590	47.081063
2582.010466	246.895761	47.086068
2578.663787	247.081087	47.091073
2575.042256	242.043155	47.096077
2571.666258	248.672578	47.101082
2568.269483	239.960158	47.106087
2564.192497	242.353503	47.111092
2560.685333	240.838592	47.116097
2557.777776	237.065806	47.121101
2554.481731	238.879937	47.126106
2550.935761	237.128707	47.131111
2547.494018	236.756666	47.136116
2543.694730	230.711268	47.141121
2540.604141	236.339258	47.146125
2536.567184	243.228163	47.151130
2533.480898	231.656757	47.156135
2529.314048	240.190830	47.161140
2526.243554	242.539252	47.166145
2523.260392	230.102661	47.171149
2519.136087	233.324001	47.176154
2515.914710	221.685911	47.181159
2512.469116	230.384131	47.186164
2509.004264	226.882745	47.191169
2505.689896	222.511313	47.196173
2501.889694	228.845904	47.201178
2498.374319	226.782799	47.206183
2495.020606	222.776240	47.211188
2491.498799	223.605052	47.216193
2488.530619	227.207089	47.221197
2484.596978	220.812130	47.226202
2481.261389	220.736780	47.231207
2477.784360	223.677258	47.236212
2474.018038	224.881527	47.241217
2470.557828	220.681015	47.246221
2467.101839	223.462127	47.251226
2464.032090	224.434206	47.256231
2460.461529	220.001095	47.261236
2456.726862	223.730655	47.266241
2453.640241	214.974446	47.271245
2449.782073	223.674889	47.276250
2446.435607	224.900257	47.281255
2442.489511	221.623009	47.286260
2438.932259	231.975464	47.291265
2435.681637	226.406158	47.296269
2432.081677	229.763812	47.301274
2428.595641	222.221085	47.306279
2425.326385	228.315937	47.311284
2422.169557	225.833950	47.316289
2418.749795	223.486934	47.321293
2415.139257	226.765239	47.326298
2411.583101	218.751209	47.331303
2407.640879	228.281168	47.336308
2404.158750	214.453302	47.341313
2401.064015	210.961551	47.346317
2397.653115	220.539181	47.351322
2394.161821	213.674628	47.356327
2390.389838	214.414563	47.361332
2387.022373	222.505765	47.366337
2383.802811	217.376178	47.371341
2380.136396	217.294925	47.376346
2376.564045	222.440308	47.381351
2373.129604	221.979564	47.386356
2369.544250	225.174609	47.391361
2366.404274	208.373600	47.396365
2361.988779	218.990717	47.401370
2358.970750	213.802620	47.406375
2355.584239	219.958506	47.411380
2351.942591	214.506112	47.416385
2348.969222	216.111402	47.421389
2344.767464	213.383610	47.426394
2341.892166	211.592862	47.431399
2338.114521	211.011984	47.436404
2334.605488	215.143463	47.441409
2331.194660	215.353756	47.446413
2327.425636	221.862307	47.451418
2324.191915	206.884255	47.456423
2320.670421	215.160964	47.461428
2317.259091	216.919684	47.466433
2313.813950	199.927563	47.471437
2309.849213	222.079648	47.476442
2306.771558	212.464029	47.481447
2303.182739	216.276971	47.486452
2299.515663	208.258853	47.491457
2296.354689	217.532422	47.496461
2292.585800	217.859677	47.501466
2289.012276	213.312931	47.506471
2285.870164	208.718250	47.511476
2282.038298	211.544570	47.516481
2278.907958	209.152638	47.521485
2275.051662	212.078510	47.526490
2271.307847	208.396618	47.531495
2267.926273	210.158746	47.536500
2264.392245	211.926707	47.541505
2261.447314	205.717608	47.546509
2257.861031	206.115582	47.551514
2254.192934	196.462318	47.556519
2250.720348	201.061448	47.561524
2247.036180	210.552456	47.566529
2243.834035	203.108256	47.571533
2240.341562	210.791951	47.576538
2237.080355	205.332884	47.581543
2233.859802	199.225358	47.586548
2229.584809	207.692244	47.591553
2226.167001	194.164543	47.596557
2222.716931	198.556911	47.601562
2219.143113	199.596973	47.606567
2215.289203	205.265130	47.611572
2212.093800	206.144243	47.616577
2208.866490	196.980658	47.621581
2205.239534	205.100794	47.626586
2201.628779	194.642827	47.631591
2198.244364	205.696047	47.636596
2194.796185	207.196497	47.641601
2191.387425	202.843252	47.646605
2187.784070	203.414598	47.651610
2184.311104	202.658814	47.656615
2180.951079	192.434164	47.661620
2177.463025	209.637839	47.666625
2173.564972	199.082681	47.671629
2169.775928	204.235167	47.676634
2166.772430	193.017646	47.681639
2163.367860	194.452899	47.686644
2159.168115	200.704506	47.691649
2156.421675	192.379389	47.696653
2153.019068	198.605937	47.701658
2149.500011	197.646044	47.706663
2145.838888	188.507770	47.711668
2141.880912	199.822284	47.716673
2138.798932	197.410622	47.721677
2135.194682	197.850134	47.726682
2131.820269	203.375234	47.731687
2128.413354	195.713722	47.736692
2124.934720	199.851370	47.741697
2121.760761	190.071238	47.746701
2118.002405	199.712713	47.751706
2114.233619	204.338943	47.756711
2110.399285	193.214458	47.761716
2106.814929	195.303822	47.766721
2103.907002	208.339235	47.771725
2100.241910	203.020571	47.776730
2096.866274	194.268945	47.781735
2093.624816	193.533410	47.786740
2090.070169	197.409726	47.791745
2086.266988	188.536309	47.796749
2082.569692	196.941651	47.801754
2079.308035	199.430640	47.806759
2075.811257	197.178690	47.811764
2071.924422	203.936969	47.816769
2068.822289	188.769873	47.821773
2065.345759	193.029168	47.826778
2061.714975	199.572298	47.831783
2058.564806	193.084648	47.836788
2054.816926	191.136053	47.841793
2051.567176	196.869134	47.846797
2047.636695	197.626036	47.851802
2043.937982	189.346762	47.856807
2040.700046	185.528828	47.861812
2037.117433	189.726528	47.866817
2033.662622	195.387712	47.871821
2030.123453	197.591822	47.876826
2026.948625	185.029419	47.881831
2023.500066	190.634912	47.886836
2019.309006	194.804446	47.891841
2016.319295	190.938626	47.896845
2012.677454	189.940109	47.901850
2009.545766	188.892467	47.906855
2006.201762	189.977809	47.911860
2001.883907	195.304974	47.916865
1998.938178	184.780770	47.921869
1995.506844	185.556314	47.926874
1991.833315	189.029630	47.931879
1988.313326	185.881910	47.936884
1984.666020	192.830588	47.941889
1981.541253	180.440720	47.946893
1977.698346	193.811956	47.951898
1974.136953	181.983017	47.956903
1970.747082	191.204767	47.961908
1967.163012	203.177939	47.966913
1963.882395	194.028281	47.971917
1960.127629	188.625090	47.976922
1956.650352	190.024146	47.981927
1953.508719	194.270237	47.986932
1949.865482	189.402565	47.991937
1946.720686	179.567830	47.996941
1942.985178	186.095378	48.001946
1939.280810	201.439456	48.006951
1935.687604	189.842147	48.011956
1931.816140	186.707728	48.016961
1928.752667	187.762180	48.021965
1925.345299	183.880158	48.026970
1921.567080	183.935335	48.031975
1918.111118	190.113615	48.036980
1914.586594	190.099464	48.041985
1911.572931	181.479427	48.046989
1907.876882	192.490348	48.051994
1904.306974	187.711837	48.056999
1900.583102	186.026993	48.062004
1897.404216	190.587318	48.067009
1894.005742	183.474984	48.072013
1890.487189	189.630468	48.077018
1886.752512	186.319765	48.082023
1883.483597	182.048643	48.087028
1879.544518	184.813252	48.092033
1875.972834	188.070912	48.097037
1872.701905	186.301208	48.102042
1869.149769	187.935882	48.107047
1865.800439	193.780249	48.112052
1862.353347	185.255916	48.117057
1859.118312	186.203180	48.122061
1855.210961	184.669256	48.127066
1852.057843	190.062465	48.132071
1847.749196	177.406295	48.137076
1844.638985	182.745650	48.142081
1841.395221	189.486668	48.147085
1837.716155	192.459178	48.152090
1834.192028	193.243061	48.157095
1830.643409	181.020221	48.162100
1826.980480	187.911991	48.167105
1823.997747	190.195620	48.172109
1819.989817	190.408609	48.177114
1816.713225	183.465253	48.182119
1813.535121	177.100216	48.187124
1809.650985	186.871998	48.192129
1806.101646	170.259302	48.197133
1802.386549	186.946339	48.202138
1799.068982	181.460209	48.207143
1796.038600	178.379368	48.212148
1792.132064	185.070256	48.217153
1788.574716	184.295551	48.222157
1785.151691	179.201798	48.227162
1782.011848	176.493865	48.232167
1778.399536	184.624685	48.237172
1774.445734	197.060836	48.242177
1771.115071	185.199283	48.247181
1767.676483	192.740576	48.252186
1764.299689	187.509745	48.257191
1760.604410	182.815015	48.262196
1756.762555	187.684068	48.267201
1753.918106	189.304726	48.272205
1750.050766	186.513544	48.277210
1746.459701	182.405861	48.282215
1743.303176	183.011860	48.287220
1739.534080	183.458972	48.292225
1736.459268	177.643486	48.297229
1732.947956	186.599499	48.302234
1729.064676	179.697046	48.307239
1725.760283	179.479916	48.312244
1721.956363	181.962228	48.317249
1718.748353	181.348117	48.322253
1715.067968	180.910328	48.327258
1711.714146	184.269063	48.332263
1708.194014	183.215549	48.337268
1704.324828	176.222777	48.342273
1701.097872	181.396797	48.347277
1697.686010	180.239757	48.352282
1694.232391	183.112963	48.357287
1690.633606	175.635266	48.362292
1686.908911	178.681139	48.367297
1683.710899	178.309706	48.372301
1680.206039	177.373672	48.377306
1676.561527	182.063557	48.382311
1673.488176	185.484515	48.387316
1669.535671	175.204852	48.392321
1665.878982	180.485615	48.397325
1662.224365	185.925489	48.402330
1658.857081	176.161682	48.407335
1655.940235	180.114865	48.412340
1652.240783	187.915419	48.417345
1649.149320	173.160738	48.422349
1645.267186	185.817398	48.427354
1641.313318	190.061921	48.432359
1637.763797	183.942498	48.437364
1634.342427	194.577872	48.442369
1631.500143	181.160634	48.447373
1627.724590	183.450861	48.452378
1623.862024	178.597601	48.457383
1620.595597	179.654210	48.462388
1617.185617	177.369918	48.467393
1613.686385	173.719994	48.472397
1610.134844	177.486017	48.477402
1606.613336	180.426546	48.482407
1603.267197	174.004774	48.487412
1599.246218	179.394720	48.492417
1595.855023	165.559684	48.497421
1592.446645	174.589944	48.502426
1589.142773	174.563454	48.507431
1585.645600	179.293389	48.512436
1581.855335	185.411493	48.517441
1578.682336	170.938133	48.522445
1574.995038	182.329871	48.527450
1571.709480	175.910544	48.532455
1568.478708	176.993069	48.537460
1564.321993	174.244342	48.542465
1560.966240	166.932226	48.547469
1557.395641	184.053751	48.552474
1553.962096	167.925175	48.557479
1550.470271	169.205367	48.562484
1546.955146	168.785198	48.567489
1543.445038	167.271737	48.572493
1539.709276	169.058361	48.577498
1536.879536	167.092656	48.582503
1533.348653	166.936772	48.587508
1529.419964	170.245191	48.592513
1526.117332	164.079741	48.597517
1522.735755	174.289843	48.602522
1519.031969	171.258314	48.607527
1515.582049	173.795756	48.612532
1511.866510	175.864412	48.617537
1508.447617	162.695314	48.622541
1504.721211	172.186675	48.627546
1501.145308	173.323520	48.632551
1498.078972	172.630501	48.637556
1494.637540	180.958633	48.642561
1491.058984	173.125910	48.647565
1487.292062	178.332862	48.652570
1484.110054	170.886318	48.657575
1480.862205	175.849028	48.662580
1476.962275	171.626058	48.667585
1473.611506	170.861462	48.672589
1469.891720	171.410558	48.677594
1466.439031	168.692785	48.682599
1463.045377	161.680850	48.687604
1459.135362	172.316167	48.692609
1455.833415	175.962708	48.697613
1452.304293	179.446696	48.702618
1448.923393	174.855775	48.707623
1445.591657	172.460211	48.712628
1441.903794	176.452736	48.717633
1438.619269	162.959169	48.722637
1435.163723	164.512684	48.727642
1431.594434	171.004639	48.732647
1428.118285	170.237710	48.737652
1424.080100	174.098901	48.742657
1420.660373	169.633219	48.747661
1417.563870	167.524011	48.752666
1414.200678	181.460639	48.757671
1410.541174	169.789521	48.762676
1406.598103	174.179264	48.767681
1403.214586	168.576075	48.772685
1399.809388	174.422475	48.777690
1396.740134	166.674776	48.782695
1393.109091	157.668173	48.787700
1389.293004	169.257733	48.792705
1385.992315	158.850097	48.797709
1382.346454	164.734310	48.802714
1378.673158	165.365584	48.807719
1375.155989	166.312450	48.812724
1371.571355	166.381659	48.817729
1368.412440	159.574123	48.822733
1365.248282	156.044450	48.827738
1361.620212	163.462407	48.832743
1357.972911	167.850464	48.837748
1354.043909	167.241524	48.842753
1350.866563	170.876617	48.847757
1347.270589	167.613103	48.852762
1343.604320	169.390171	48.857767
1340.279843	160.241770	48.862772
1336.945391	169.682274	48.867777
1333.418735	160.648601	48.872781
1329.821109	157.924109	48.877786
1326.205741	162.150421	48.882791
1323.258507	157.101533	48.887796
1319.208529	167.511243	48.892801
1315.890606	164.410577	48.897805
1312.172354	159.733450	48.902810
1308.821265	162.017306	48.907815
1305.493145	160.978146	48.912820
1301.547251	162.760621	48.917825
1298.510545	158.460833	48.922829
1294.906194	162.482879	48.927834
1291.051582	156.425439	48.932839
1287.788058	156.180950	48.937844
1284.425472	163.300115	48.942849
1280.951608	155.182883	48.947853
1277.283626	165.151575	48.952858
1273.333722	160.355498	48.957863
1270.329894	157.896192	48.962868
1266.502235	164.179565	48.967873
1263.842661	160.989446	48.972877
1260.196770	157.085807	48.977882
1256.490281	160.073745	48.982887
1252.562185	158.167842	48.987892
1249.137105	167.738824	48.992897
1245.662810	159.949864	48.997901
1242.207440	165.820647	49.002906
1238.657195	163.347894	49.007911
1235.171482	160.619384	49.012916
1231.669566	159.296625	49.017921
1228.613985	155.072234	49.022925
1224.935556	170.268783	49.027930
1221.075855	153.458730	49.032935
1217.695251	158.329099	49.037940
1214.047860	157.240963	49.042945
1211.179214	159.142019	49.047949
1207.295484	161.660034	49.052954
1203.470394	155.963657	49.057959
1200.124821	160.778715	49.062964
1196.942219	160.514400	49.067969
1193.482185	168.126308	49.072973
1189.430873	165.947192	49.077978
1185.926213	163.951804	49.082983
1183.121802	155.901381	49.087988
1179.391695	161.636670	49.092993
1175.856455	160.036483	49.097997
1171.943702	162.423953	49.103002
1168.661111	160.515200	49.108007
1165.105034	158.566022	49.113012
1161.588126	158.888434	49.118017
1158.491956	155.188617	49.123021
1154.886388	153.356561	49.128026
1151.291162	154.135544	49.133031
1147.386570	153.337055	49.138036
1143.829530	155.582261	49.143041
1140.639236	153.462906	49.148045
1137.446040	155.586982	49.153050
1133.824427	157.729601	49.158055
1130.404828	150.871618	49.163060
1126.451969	158.864808	49.168065
1122.898813	157.789780	49.173069
1119.499691	160.018169	49.178074
1116.243057	163.255668	49.183079
1112.698108	155.440617	49.188084
1108.877135	165.078924	49.193089
1105.948916	148.079656	49.198093
1102.506183	154.904344	49.203098
1098.466136	155.036638	49.208103
1095.006739	149.311469	49.213108
1091.330860	164.657259	49.218113
1088.277282	154.462594	49.223117
1084.392064	150.842981	49.228122
1080.975374	149.864417	49.233127
1077.882652	148.938059	49.238132
1074.051455	159.210348	49.243137
1070.508779	153.811155	49.248141
1067.021546	153.477324	49.253146
1063.601249	151.400596	49.258151
1060.521255	139.846139	49.263156
1056.785783	155.760064	49.268161
1053.272234	152.959342	49.273165
1049.722919	158.250031	49.278170
1046.061861	155.612828	49.283175
1042.670986	152.799526	49.288180
1038.886839	157.940795	49.293185
1035.419847	147.649762	49.298189
1031.929532	154.239248	49.303194
1028.512744	152.532369	49.308199
1025.139699	151.897298	49.313204
1021.636973	149.398120	49.318209
1017.953986	153.873832	49.323213
1014.540353	155.107356	49.328218
1010.741455	155.470794	49.333223
1007.288512	148.029181	49.338228
1003.723747	155.229916	49.343233
1000.893712	161.938951	49.348237
997.274601	154.635725	49.353242
993.522053	156.827931	49.358247
990.108034	156.952503	49.363252
986.612660	159.307021	49.368257
983.325439	143.269258	49.373261
979.432297	153.141791	49.378266
975.763980	156.000302	49.383271
972.429782	155.381146	49.388276
968.564275	154.750006	49.393281
965.447871	156.060708	49.398285
962.048328	150.976567	49.403290
958.524801	152.174237	49.408295
955.301246	146.160156	49.413300
951.633949	160.762628	49.418305
948.194035	149.549773	49.423309
944.520291	151.655971	49.428314
940.897185	156.337333	49.433319
937.571136	149.672032	49.438324
933.871185	145.406227	49.443329
930.768268	147.286998	49.448333
927.070757	154.637617	49.453338
923.101991	154.580479	49.458343
919.884333	147.038458	49.463348
916.044835	150.821433	49.468353
912.710206	144.379381	49.473357
909.628045	144.924711	49.478362
905.839718	150.199384	49.483367
902.584443	149.068163	49.488372
899.114850	152.886076	49.493377
895.660429	145.059603	49.498381
891.916937	142.107800	49.503386
888.319631	152.048098	49.508391
884.863367	140.593511	49.513396
881.260382	146.993349	49.518401
878.043390	139.283322	49.523405
874.487098	151.892138	49.528410
870.584041	149.281102	49.533415
867.239384	146.497591	49.538420
864.130134	149.158934	49.543425
860.580206	142.597430	49.548429
857.030923	144.480249	49.553434
853.404906	158.708516	49.558439
850.275358	145.619841	49.563444
846.683425	150.796167	49.568449
842.687990	147.667430	49.573453
838.907640	143.522358	49.578458
835.678374	150.932545	49.583463
832.620810	139.370814	49.588468
829.007239	142.084419	49.593473
825.603282	147.208355	49.598477
822.056384	136.437198	49.603482
818.314516	144.478411	49.608487
814.779865	147.796834	49.613492
810.871211	143.963489	49.618497
808.266311	145.345782	49.623501
804.731228	145.130186	49.628506
800.739889	152.490824	49.633511
797.395761	142.099565	49.638516
793.718598	152.076425	49.643521
790.487760	147.241581	49.648525
786.839344	152.395130	49.653530
783.170165	151.092702	49.658535
779.928301	142.880698	49.663540
776.506224	148.499429	49.668545
772.717218	135.245619	49.673549
769.423019	137.787841	49.678554
765.620329	142.130612	49.683559
762.140066	138.140805	49.688564
758.524289	142.067857	49.693569
755.122863	133.238761	49.698573
751.426914	143.181853	49.703578
748.481172	145.562450	49.708583
745.433103	137.489708	49.713588
741.758507	142.343919	49.718593
738.132593	143.981788	49.723597
734.241639	145.766514	49.728602
730.171454	146.688934	49.733607
727.199996	137.563174	49.738612
723.793173	148.584064	49.743617
720.508411	135.978216	49.748621
716.724957	139.256374	49.753626
713.010627	140.904745	49.758631
709.827222	145.062230	49.763636
706.064148	151.817842	49.768641
702.556203	138.477937	49.773645
699.085412	148.345735	49.778650
695.739988	140.787147	49.783655
692.317486	142.331410	49.788660
688.741173	144.309016	49.793665
685.633533	144.041743	49.798669
681.886410	137.842968	49.803674
678.600945	143.378781	49.808679
674.894818	136.555962	49.813684
670.958097	131.403664	49.818689
667.479682	135.333516	49.823693
664.310134	143.327519	49.828698
660.605596	138.728033	49.833703
657.316559	140.021331	49.838708
653.247560	147.161687	49.843713
650.324668	139.079950	49.848717
646.622462	142.463125	49.853722
643.332818	150.528519	49.858727
640.026351	145.213953	49.863732
636.131648	152.790806	49.868737
632.719854	145.497814	49.873741
629.355988	145.531091	49.878746
625.717697	147.660689	49.883751
622.459201	143.919652	49.888756
618.602134	149.737355	49.893761
615.093320	139.751995	49.898765
611.568530	141.734951	49.903770
608.075911	149.588268	49.908775
604.572939	133.319564	49.913780
600.968129	144.497416	49.918785
597.525984	137.272233	49.923789
594.419937	138.983844	49.928794
590.533372	137.701763	49.933799
587.621204	135.171138	49.938804
583.671199	147.693540	49.943809
580.041605	136.173388	49.948813
576.527670	143.785753	49.953818
573.013555	150.175263	49.958823
569.622655	136.988195	49.963828
565.997820	142.422963	49.968833
562.702884	146.072907	49.973837
559.259520	147.615988	49.978842
555.737202	144.849886	49.983847
552.260036	143.970347	49.988852
548.389639	145.906545	49.993857
544.865610	140.778033	49.998861
541.779338	140.239346	50.003866
538.078216	141.639599	50.008871
534.564605	143.640302	50.013876
530.751064	147.838048	50.018881
527.779820	144.685369	50.023885
524.051441	144.095473	50.028890
520.666553	152.897973	50.033895
517.382933	139.587624	50.038900
513.608217	142.893118	50.043905
510.061892	130.804548	50.048909
506.310283	139.234584	50.053914
502.555767	142.419922	50.058919
499.843463	132.648794	50.063924
496.286042	146.612757	50.068929
492.556176	136.329410	50.073933
489.279497	129.653953	50.078938
485.469309	138.614862	50.083943
481.994072	132.950658	50.088948
478.245774	141.932117	50.093953
474.943416	135.972905	50.098957
471.596809	132.118304	50.103962
467.658092	144.838432	50.108967
464.450332	128.800443	50.113972
461.190504	138.726234	50.118977
457.556705	133.795543	50.123981
454.035638	132.435141	50.128986
450.500358	137.342500	50.133991
447.070583	124.565541	50.138996
443.470113	137.013029	50.144001
440.524276	128.872699	50.149005
436.650013	131.007363	50.154010
432.989571	139.364154	50.159015
429.400605	126.179615	50.164020
425.675262	133.657364	50.169025
422.364516	137.930644	50.174029
419.012923	134.051454	50.179034
416.039731	135.005140	50.184039
412.417373	129.075263	50.189044
408.304476	131.697595	50.194049
404.640061	136.738250	50.199053
401.383382	132.396204	50.204058
397.711933	136.308875	50.209063
394.532293	126.077041	50.214068
390.960307	140.096958	50.219073
387.681581	137.373170	50.224077
384.061770	131.851183	50.229082
380.213592	128.569262	50.234087
376.976566	129.731811	50.239092
373.098474	136.794235	50.244097
369.937920	133.074882	50.249101
366.837823	133.251976	50.254106
362.990334	127.909973	50.259111
359.265768	124.860990	50.264116
355.677145	130.460818	50.269121
352.523758	126.772854	50.274125
349.085853	127.999062	50.279130
345.035704	134.682687	50.284135
342.167022	127.283484	50.289140
338.576463	132.196327	50.294145
334.982655	135.101628	50.299149
331.365096	127.533937	50.304154
327.798968	129.702744	50.309159
324.386914	121.319797	50.314164
320.869510	128.943375	50.319169
317.228904	133.061365	50.324173
314.050627	133.750696	50.329178
310.151774	130.091239	50.334183
306.988136	123.520757	50.339188
303.134793	135.485683	50.344193
299.795494	129.948322	50.349197
296.801140	121.446332	50.354202
292.784334	127.164247	50.359207
289.439288	122.641363	50.364212
285.806328	130.586018	50.369217
282.382975	134.032654	50.374221
279.031995	127.767105	50.379226
275.466519	129.318385	50.384231
271.817153	123.689901	50.389236
268.299600	129.814586	50.394241
264.782524	121.405465	50.399245
261.127730	120.189908	50.404250
257.474804	134.179501	50.409255
254.321048	132.830292	50.414260
250.732042	131.139522	50.419265
247.176673	131.866659	50.424269
244.124106	129.461343	50.429274
240.333511	136.635292	50.434279
237.337270	133.852429	50.439284
233.600729	123.977946	50.444289
230.136411	129.012648	50.449293
226.272838	137.820982	50.454298
222.429591	133.718462	50.459303
219.032266	123.802046	50.464308
215.571682	139.139992	50.469313
212.314509	136.356534	50.474317
208.638751	130.859953	50.479322
205.172384	139.286219	50.484327
202.025950	123.990369	50.489332
198.051561	123.985342	50.494337
194.719734	127.833663	50.499341
191.173952	132.594760	50.504346
187.932048	133.450613	50.509351
184.358832	128.340628	50.514356
180.621263	133.778179	50.519361
177.383753	129.078333	50.524365
173.721102	133.807288	50.529370
170.020984	132.263250	50.534375
166.908313	120.363506	50.539380
163.328741	125.393067	50.544385
159.723766	126.176048	50.549389
156.276464	129.604841	50.554394
152.703229	126.809430	50.559399
149.317763	121.500857	50.564404
145.534244	126.578210	50.569409
141.937164	126.680277	50.574413
139.042798	122.123157	50.579418
135.362529	129.856916	50.584423
132.110112	128.267204	50.589428
128.023304	129.377051	50.594433
124.601299	130.778604	50.599437
120.878673	129.310365	50.604442
117.819512	124.658986	50.609447
114.370789	121.457205	50.614452
110.775052	129.155872	50.619457
107.119467	129.505443	50.624461
103.567537	128.923603	50.629466
99.833996	130.944885	50.634471
96.619472	132.431099	50.639476
92.872445	137.535807	50.644481
89.783864	130.278974	50.649485
86.333976	133.540318	50.654490
82.735722	129.329879	50.659495
79.437171	126.292307	50.664500
75.914546	122.779955	50.669505
72.081626	129.274322	50.674509
68.430409	130.979682	50.679514
64.798233	126.008231	50.684519
61.723394	125.552262	50.689524
58.159358	135.484485	50.694529
54.726671	128.040557	50.699533
51.433969	123.039548	50.704538
47.423508	128.058262	50.709543
44.310428	120.509132	50.714548
40.314787	124.739612	50.719553
36.934533	127.554537	50.724557
33.800560	119.042134	50.729562
29.927037	120.756514	50.734567
26.684766	118.041782	50.739572
22.897655	128.066613	50.744577
19.860452	123.820355	50.749581
16.314643	122.167629	50.754586
12.453867	125.622378	50.759591
9.061709	115.686358	50.764596
5.825883	122.662459	50.769601
1.780581	121.085159	50.774605