Tue Jun 21 13:27:14 2022

Number of Points = 9928

Depth (nm)	Load (N)	Time (s)
-0.200239	102.848942	0.000000
0.098977	120.909402	0.005005
0.507536	119.027102	0.010010
0.544727	128.232953	0.015014
0.642755	127.712965	0.020019
0.294723	113.712526	0.025024
0.082727	109.951548	0.030029
0.220736	89.119645	0.035034
-0.034146	91.536016	0.040038
-0.183077	72.436093	0.045043
-0.578809	60.404705	0.050048
-0.979532	57.213910	0.055053
-1.301387	42.545765	0.060058
-1.926898	34.168188	0.065062
-1.883638	31.300914	0.070067
-2.478614	14.051713	0.075072
-2.766495	21.732862	0.080077
-2.827663	19.541186	0.085082
-3.106640	19.483821	0.090086
-3.859057	15.492082	0.095091
-4.596485	20.750617	0.100096
-4.870052	26.882108	0.105101
-4.414434	13.758439	0.110106
-4.569933	22.511879	0.115110
-4.349403	25.882163	0.120115
-4.735116	21.693540	0.125120
-5.235362	26.783943	0.130125
-5.876948	20.096631	0.135130
-6.514588	17.019470	0.140134
-6.280651	14.133650	0.145139
-6.036319	19.783924	0.150144
-6.445760	16.720678	0.155149
-6.223566	12.772387	0.160154
-7.198879	27.598744	0.165158
-7.455167	20.976884	0.170163
-7.924363	21.856185	0.175168
-8.035560	22.929778	0.180173
-7.730862	16.044926	0.185178
-8.411233	22.757436	0.190182
-8.788238	24.244650	0.195187
-9.100685	28.897450	0.200192
-9.104297	17.476046	0.205197
-9.391071	23.495466	0.210202
-9.842822	24.474492	0.215206
-9.550066	17.464337	0.220211
-10.354744	18.881078	0.225216
-10.559871	18.473058	0.230221
-10.650792	16.309595	0.235226
-10.953129	27.060289	0.240230
-10.854970	18.982223	0.245235
-10.903008	21.506215	0.250240
-11.514878	18.718222	0.255245
-12.102333	14.732321	0.260250
-12.814260	25.505452	0.265254
-12.722242	24.494116	0.270259
-12.683976	26.633621	0.275264
-12.854942	20.486230	0.280269
-12.588760	17.302622	0.285274
-13.729362	21.868581	0.290278
-13.692559	15.360399	0.295283
-14.043520	22.780069	0.300288
-14.435537	19.868054	0.305293
-14.074332	15.865762	0.310298
-14.667417	21.380807	0.315302
-14.656562	19.995546	0.320307
-15.085610	21.745937	0.325312
-15.574822	17.195379	0.330317
-15.508968	12.684727	0.335322
-15.958746	19.646172	0.340326
-16.032314	22.188995	0.345331
-16.185547	18.897632	0.350336
-17.068551	27.197698	0.355341
-17.122410	25.443681	0.360346
-17.363442	22.251907	0.365350
-17.425794	21.224497	0.370355
-17.329594	23.458599	0.375360
-17.787013	19.955549	0.380365
-18.116800	17.353700	0.385370
-18.889820	24.869110	0.390374
-18.679451	16.764177	0.395379
-18.806507	17.590770	0.400384
-19.275253	13.043534	0.405389
-19.240477	8.963874	0.410394
-19.552441	20.583436	0.415398
-19.860433	12.126460	0.420403
-20.277464	19.016178	0.425408
-20.498828	13.191685	0.430413
-20.157008	16.172868	0.435418
-20.646942	10.181506	0.440422
-20.945695	10.415129	0.445427
-21.575624	19.388024	0.450432
-22.096733	15.583735	0.455437
-21.803604	12.131042	0.460442
-21.915719	14.608220	0.465446
-22.595446	11.484160	0.470451
-23.313696	15.928086	0.475456
-23.401689	20.202921	0.480461
-23.314872	14.280431	0.485466
-23.673238	16.333470	0.490470
-23.500795	19.351778	0.495475
-23.509195	25.092249	0.500480
-23.794560	26.777409	0.505485
-24.550175	17.865306	0.510490
-24.993936	24.693346	0.515494
-25.014114	15.046939	0.520499
-24.997236	22.109696	0.525504
-25.314054	18.731167	0.530509
-25.318811	14.478677	0.535514
-26.230414	18.893449	0.540518
-26.604620	18.754175	0.545523
-26.489452	14.608119	0.550528
-26.786742	23.503832	0.555533
-26.580843	11.294520	0.560538
-26.864536	23.873374	0.565542
-27.200989	18.618301	0.570547
-28.104213	21.854989	0.575552
-28.242283	27.559115	0.580557
-27.928230	14.433433	0.585562
-28.296761	19.760531	0.590566
-28.324656	21.489092	0.595571
-29.268939	21.444220	0.600576
-29.743694	27.322499	0.605581
-29.679027	11.820389	0.610586
-29.995768	25.593649	0.615590
-29.771246	19.030306	0.620595
-29.949215	12.657345	0.625600
-29.962500	22.923668	0.630605
-30.380860	13.653210	0.635610
-31.212656	17.326410	0.640614
-31.194268	16.348382	0.645619
-31.131558	13.396393	0.650624
-31.360241	22.519123	0.655629
-31.966389	18.842187	0.660634
-32.708434	19.140337	0.665638
-32.628691	28.082546	0.670643
-32.853200	20.658990	0.675648
-32.827529	19.189186	0.680653
-32.835282	21.073462	0.685658
-33.474031	15.997505	0.690662
-34.075099	24.126564	0.695667
-34.209807	21.548059	0.700672
-34.673465	23.413112	0.705677
-34.032057	20.065543	0.710682
-34.781573	24.987855	0.715686
-34.693791	19.512558	0.720691
-34.933534	21.434856	0.725696
-35.380027	19.981672	0.730701
-35.660613	18.290262	0.735706
-36.302526	23.775112	0.740710
-35.989499	21.768533	0.745715
-36.005900	17.586248	0.750720
-36.743589	20.576091	0.755725
-37.229433	22.520199	0.760730
-37.898498	20.907920	0.765734
-37.403051	19.513650	0.770739
-37.667437	19.481893	0.775744
-37.543704	9.375948	0.780749
-37.713946	13.034317	0.785754
-38.522491	22.749954	0.790758
-38.708420	13.115211	0.795763
-38.920880	19.398393	0.800768
-39.341652	19.247887	0.805773
-39.228164	16.355766	0.810778
-40.177953	25.383212	0.815782
-40.558999	14.568167	0.820787
-40.597704	22.454521	0.825792
-41.248101	15.263702	0.830797
-40.498909	18.862564	0.835802
-40.985686	24.790785	0.840806
-40.744584	17.686570	0.845811
-40.736270	23.663242	0.850816
-41.644065	17.320561	0.855821
-42.324104	11.916177	0.860826
-42.744115	17.334481	0.865830
-42.743538	13.307252	0.870835
-42.803225	16.562318	0.875840
-42.654719	13.326762	0.880845
-42.683807	15.268047	0.885850
-43.860378	18.727406	0.890854
-44.096527	18.739319	0.895859
-44.126508	10.532506	0.900864
-44.282252	15.239076	0.905869
-44.052285	21.803009	0.910874
-44.225261	15.556106	0.915878
-44.844657	16.367537	0.920883
-45.207434	21.978237	0.925888
-45.401778	16.479213	0.930893
-45.238495	18.965250	0.935898
-45.969966	24.736857	0.940902
-46.733328	15.254567	0.945907
-47.359638	26.555004	0.950912
-47.119848	19.508035	0.955917
-47.143087	10.991674	0.960922
-47.364010	25.959308	0.965926
-47.424906	18.587792	0.970931
-47.276804	16.277992	0.975936
-47.607934	13.243617	0.980941
-48.114915	15.630094	0.985946
-48.596236	16.521274	0.990950
-48.783063	5.390309	0.995955
-49.146067	11.038536	1.000960
-48.952802	16.334168	1.005965
-49.313266	11.743550	1.010970
-50.280382	12.286569	1.015974
-50.315840	5.991639	1.020979
-50.229805	11.137688	1.025984
-50.203469	16.964163	1.030989
-50.191357	6.960768	1.035994
-51.151939	16.780316	1.040998
-51.698882	14.878458	1.046003
-51.678779	14.813009	1.051008
-52.098644	16.849988	1.056013
-51.937900	6.560317	1.061018
-52.019247	28.261126	1.066022
-52.096352	13.505327	1.071027
-52.383971	20.914703	1.076032
-53.261935	15.153955	1.081037
-53.400043	10.402986	1.086042
-53.848599	12.468001	1.091046
-54.134812	19.349081	1.096051
-54.038404	13.569057	1.101056
-54.348409	16.244963	1.106061
-54.115264	10.304953	1.111066
-54.791190	16.635086	1.116070
-54.925592	11.062400	1.121075
-55.356420	20.138486	1.126080
-55.690979	15.296320	1.131085
-55.236405	10.259538	1.136090
-55.964574	13.327923	1.141094
-56.155320	15.815952	1.146099
-56.294980	14.057202	1.151104
-56.743170	16.220430	1.156109
-56.704196	1.937174	1.161114
-57.871376	15.914008	1.166118
-57.939843	11.076520	1.171123
-57.918583	12.450423	1.176128
-58.149484	16.361558	1.181133
-58.205562	8.086253	1.186138
-58.587218	13.272851	1.191142
-58.888611	17.928357	1.196147
-58.868762	12.495097	1.201152
-58.933827	21.351760	1.206157
-59.625545	6.273682	1.211162
-60.140985	19.616501	1.216166
-60.165884	17.452368	1.221171
-60.332506	19.812477	1.226176
-60.564274	19.611533	1.231181
-60.233121	14.350298	1.236186
-60.905610	19.983279	1.241190
-61.155010	21.259925	1.246195
-61.621938	16.692069	1.251200
-61.859182	17.122313	1.256205
-61.957100	13.782131	1.261210
-62.239777	16.603090	1.266214
-62.537533	15.118372	1.271219
-63.180517	16.630889	1.276224
-63.592444	19.142917	1.281229
-63.397210	14.720557	1.286234
-63.610749	17.572494	1.291238
-64.065315	18.244348	1.296243
-64.089258	17.188280	1.301248
-63.890977	16.774434	1.306253
-64.045626	16.332996	1.311258
-64.793576	25.791542	1.316262
-65.057074	20.645752	1.321267
-65.277230	21.706409	1.326272
-65.358031	19.588632	1.331277
-65.426577	7.208499	1.336282
-66.527898	18.283700	1.341286
-66.540678	16.925442	1.346291
-66.971240	17.655679	1.351296
-67.245785	13.600605	1.356301
-67.047855	10.517888	1.361306
-67.088154	20.188393	1.366310
-67.319745	3.759350	1.371315
-67.262738	13.581075	1.376320
-68.175028	20.975104	1.381325
-68.276027	14.962556	1.386330
-68.439004	21.715682	1.391334
-68.790477	18.580880	1.396339
-68.654137	12.659664	1.401344
-69.564583	14.397034	1.406349
-69.516190	13.311621	1.411354
-70.406809	12.805584	1.416358
-69.956988	13.951833	1.421363
-70.104644	11.230437	1.426368
-70.483925	9.664699	1.431373
-70.508039	16.536313	1.436378
-71.267719	17.616067	1.441382
-71.325914	31.083072	1.446387
-71.503665	18.698322	1.451392
-71.640071	24.807098	1.456397
-71.772494	7.632088	1.461402
-72.769593	18.022454	1.466406
-72.812244	10.814274	1.471411
-72.828056	14.369714	1.476416
-73.352620	17.639211	1.481421
-73.327425	13.686248	1.486426
-73.151101	16.815796	1.491430
-73.312140	15.849130	1.496435
-74.294662	12.150864	1.501440
-74.558121	21.663558	1.506445
-74.564317	21.190432	1.511450
-74.890657	19.605862	1.516454
-74.887906	21.229891	1.521459
-74.896290	11.615677	1.526464
-75.814717	20.064678	1.531469
-75.935617	10.350699	1.536474
-76.529499	17.081646	1.541478
-76.493356	12.833436	1.546483
-76.433639	9.599956	1.551488
-76.736336	19.792644	1.556493
-76.576871	7.573861	1.561498
-77.615129	20.315557	1.566502
-77.908115	19.310753	1.571507
-78.161607	13.091002	1.576512
-77.911546	22.678691	1.581517
-77.935785	13.448744	1.586522
-78.173218	14.839440	1.591526
-78.982916	25.315993	1.596531
-79.610101	25.664394	1.601536
-79.879146	21.930850	1.606541
-79.530312	19.850062	1.611546
-80.010743	17.292505	1.616550
-79.938953	21.319668	1.621555
-79.814132	21.340082	1.626560
-79.969965	20.798991	1.631565
-80.523196	14.510676	1.636570
-81.361427	27.668974	1.641574
-81.240731	13.814204	1.646579
-81.222825	14.835831	1.651584
-82.291583	20.488460	1.656589
-82.479900	11.035864	1.661594
-82.832470	14.717916	1.666598
-82.913150	12.110341	1.671603
-82.832140	16.858806	1.676608
-83.034477	16.191822	1.681613
-82.892102	14.844574	1.686618
-83.089990	17.977486	1.691622
-83.954884	12.779350	1.696627
-84.042667	12.949820	1.701632
-84.513764	10.322837	1.706637
-84.103239	2.278302	1.711642
-84.592549	17.664120	1.716646
-85.328054	16.389242	1.721651
-85.441015	9.990722	1.726656
-85.908554	19.227596	1.731661
-85.972177	11.219350	1.736666
-86.081806	10.633706	1.741670
-86.156857	11.636391	1.746675
-86.178024	14.044635	1.751680
-87.181371	17.100581	1.756685
-87.122635	9.918828	1.761690
-87.964785	17.245397	1.766694
-87.804388	20.847433	1.771699
-87.848489	19.994601	1.776704
-88.120397	25.091200	1.781709
-87.703137	17.368379	1.786714
-88.223669	20.986094	1.791718
-88.760984	14.580889	1.796723
-89.048992	12.771328	1.801728
-89.374626	18.143813	1.806733
-89.286984	9.324738	1.811738
-90.333163	21.090161	1.816742
-90.907162	16.296927	1.821747
-90.764369	17.821198	1.826752
-90.930076	24.589774	1.831757
-90.948625	13.130798	1.836762
-91.032182	20.956693	1.841766
-91.067785	16.173752	1.846771
-90.886524	9.558774	1.851776
-91.676909	14.500882	1.856781
-92.307069	13.997694	1.861786
-92.501778	11.052226	1.866790
-92.704789	19.089315	1.871795
-92.564122	14.568841	1.876800
-92.866556	16.102121	1.881805
-93.313263	12.969479	1.886810
-94.039222	15.814518	1.891814
-94.447321	14.556262	1.896819
-94.455090	19.981877	1.901824
-94.256636	24.681492	1.906829
-94.220445	14.285363	1.911834
-94.485837	21.022889	1.916838
-95.041752	12.806092	1.921843
-95.425977	14.344235	1.926848
-96.036958	17.383155	1.931853
-95.793023	12.576614	1.936858
-96.000162	16.971818	1.941862
-96.197548	25.434810	1.946867
-96.572360	20.062371	1.951872
-97.165517	21.972161	1.956877
-96.834705	14.245898	1.961882
-97.383651	29.018425	1.966886
-97.265412	14.718287	1.971891
-97.503647	14.489803	1.976896
-98.367657	12.537256	1.981901
-98.709542	17.327538	1.986906
-98.859097	21.035368	1.991910
-98.815809	26.394316	1.996915
-98.947920	20.429120	2.006912
-99.413660	10.471353	2.016909
-98.316981	19.548276	2.026906
-97.664112	16.700116	2.036902
-97.564918	21.912081	2.046899
-96.605823	11.448443	2.056896
-96.640314	13.582429	2.066893
-96.099468	16.415624	2.076890
-95.129142	23.805348	2.086886
-94.949499	17.781125	2.096883
-94.582234	15.947050	2.106880
-93.819790	18.514941	2.116877
-93.301580	16.963114	2.126874
-92.303813	18.938399	2.136870
-92.620992	16.044016	2.146867
-92.189785	19.354559	2.156864
-91.157183	16.532623	2.166861
-90.890610	21.438668	2.176858
-90.321912	17.919814	2.186854
-89.387427	24.656725	2.196851
-89.341316	14.360882	2.206848
-88.881394	19.911638	2.216845
-88.470656	21.309386	2.226842
-87.632213	23.265020	2.236838
-87.370013	21.052383	2.246835
-87.184930	16.713455	2.256832
-86.116028	18.104160	2.266829
-86.081192	17.216448	2.276826
-84.724322	21.742371	2.286822
-84.825422	23.091513	2.296819
-84.362796	17.846532	2.306816
-84.094209	14.920937	2.316813
-82.899981	17.711528	2.326810
-82.751387	15.252941	2.336806
-82.623630	17.821025	2.346803
-82.163271	21.137214	2.356800
-81.308727	16.974906	2.366797
-80.783687	17.286565	2.376794
-79.765525	16.938425	2.386790
-79.608243	21.470759	2.396787
-79.586956	21.924921	2.406784
-79.000016	20.887686	2.416781
-77.939534	21.042111	2.426778
-77.899493	22.506980	2.436774
-77.548283	19.147239	2.446771
-76.370631	30.170619	2.456768
-76.134706	17.580981	2.466765
-76.029501	15.624927	2.476762
-75.453057	12.920228	2.486758
-74.813774	18.955795	2.496755
-74.573128	20.325203	2.506752
-73.431270	14.607935	2.516749
-72.943820	13.058834	2.526746
-73.204451	18.463957	2.536742
-72.321745	15.520240	2.546739
-71.666694	18.473429	2.556736
-71.625563	15.089958	2.566733
-70.697346	13.888721	2.576730
-70.358781	17.236145	2.586726
-69.847537	18.989897	2.596723
-68.807523	17.618401	2.606720
-68.693327	15.160571	2.616717
-68.509096	16.300243	2.626714
-67.761257	15.906180	2.636710
-67.190533	14.872620	2.646707
-66.854472	19.786722	2.656704
-66.044940	14.851210	2.666701
-65.594116	19.889556	2.676698
-65.536856	19.257758	2.686694
-64.956876	20.524934	2.696691
-63.969664	18.275813	2.706688
-63.857113	23.432222	2.716685
-63.411108	21.067632	2.726682
-62.602148	14.784483	2.736678
-62.289629	15.717970	2.746675
-61.730479	22.013004	2.756672
-60.788799	21.287696	2.766669
-60.294554	12.696899	2.776666
-60.422974	20.231046	2.786662
-60.389824	19.666665	2.796659
-59.378978	19.714715	2.806656
-58.909670	21.083206	2.816653
-57.885139	17.682106	2.826650
-57.649060	20.891400	2.836646
-57.565498	28.074111	2.846643
-56.781347	20.077850	2.856640
-55.803311	18.368079	2.866637
-55.862550	18.641152	2.876634
-55.331662	20.767264	2.886630
-54.583337	23.564726	2.896627
-54.504609	23.998904	2.906624
-53.721994	11.953580	2.916621
-53.030389	19.770812	2.926618
-53.063748	19.855844	2.936614
-52.285900	16.322117	2.946611
-51.506508	20.691563	2.956608
-51.188300	13.995917	2.966605
-50.862403	17.083443	2.976602
-50.088831	15.886480	2.986598
-50.191658	13.102415	2.996595
-49.155110	22.283563	3.006592
-48.523458	22.438866	3.016589
-48.054265	11.231441	3.026586
-48.005014	13.466752	3.036582
-47.426448	17.287367	3.046579
-46.552707	22.371468	3.056576
-45.832913	19.511243	3.066573
-45.471583	13.714980	3.076570
-45.457359	18.479064	3.086566
-45.138968	16.000460	3.096563
-44.165973	15.954013	3.106560
-43.998239	13.018249	3.116557
-42.528136	15.401389	3.126554
-42.564037	6.858869	3.136550
-42.348594	17.053467	3.146547
-42.103915	15.902201	3.156544
-41.028207	13.490834	3.166541
-40.772937	10.372628	3.176538
-40.189899	13.532764	3.186534
-39.338420	15.614088	3.196531
-39.120504	16.949325	3.206528
-38.971932	16.821662	3.216525
-38.117073	12.511911	3.226522
-37.156999	15.467351	3.236518
-37.393746	9.554365	3.246515
-37.022868	13.951549	3.256512
-36.088342	12.437089	3.266509
-35.792823	17.767305	3.276506
-35.353600	14.911853	3.286502
-34.397486	16.852952	3.296499
-34.124250	18.199579	3.306496
-33.867529	14.497067	3.316493
-32.851078	8.850763	3.326490
-32.387738	19.374787	3.336486
-32.285248	9.095094	3.346483
-32.073749	9.291128	3.356480
-31.504552	12.352394	3.366477
-30.529633	18.146858	3.376474
-29.665461	14.826656	3.386470
-29.653637	15.870796	3.396467
-29.517675	20.145061	3.406464
-28.664276	15.558734	3.416461
-28.020262	10.537816	3.426458
-27.974570	12.735583	3.436454
-26.997883	7.562760	3.446451
-26.565209	14.025350	3.456448
-26.357658	13.494329	3.466445
-25.610845	3.739032	3.476442
-25.032772	10.341540	3.486438
-24.780554	15.722198	3.496435
-24.035690	15.329426	3.506432
-23.187948	20.316673	3.516429
-22.820089	18.137520	3.526426
-22.654444	14.239859	3.536422
-22.965558	16.992454	3.546419
-21.950692	20.245874	3.556416
-20.747935	14.298422	3.566413
-20.403106	16.944966	3.576410
-20.200400	21.846580	3.586406
-20.006784	17.805779	3.596403
-18.984248	17.781957	3.606400
-18.643719	23.430543	3.616397
-18.416037	25.688077	3.626394
-17.329808	20.681065	3.636390
-17.125076	20.599426	3.646387
-17.053144	19.518852	3.656384
-15.895422	12.108031	3.666381
-15.569458	14.878424	3.676378
-15.302790	14.703938	3.686374
-14.126389	18.364312	3.696371
-13.904849	24.177235	3.706368
-13.489613	20.636379	3.716365
-13.556281	14.226156	3.726362
-12.900991	18.121406	3.736358
-11.978190	16.015147	3.746355
-11.725981	16.640315	3.756352
-11.032050	15.114723	3.766349
-10.535437	13.072122	3.776346
-10.185221	13.348524	3.786342
-9.072017	18.425187	3.796339
-9.133059	10.846499	3.806336
-8.796662	9.027026	3.816333
-8.462465	10.222286	3.826330
-7.626686	11.696268	3.836326
-7.400889	20.671241	3.846323
-5.877782	19.060312	3.856320
-5.815336	18.281442	3.866317
-5.610245	19.275600	3.876314
-5.651981	18.600721	3.886310
-4.558391	23.363707	3.896307
-3.947218	32.400538	3.906304
-3.717703	25.511121	3.916301
-3.161287	20.885060	3.926298
-2.575237	23.837044	3.936294
-2.275021	32.700119	3.946291
-1.701317	43.165188	3.956288
-1.657334	43.484199	3.966285
-1.303268	63.873064	3.976282
-0.543483	84.547467	3.986278
-0.455215	107.363101	3.996275
0.000000	122.534688	4.001280
0.272927	143.994669	4.006285
0.529822	138.295964	4.011290
0.421602	149.869848	4.016294
0.651243	148.393094	4.021299
1.184083	164.654891	4.026304
0.804175	177.537518	4.031309
1.383330	180.192115	4.036314
1.008712	180.586302	4.041318
1.529418	177.844184	4.046323
1.031099	188.295919	4.051328
0.922288	185.106290	4.056333
1.187661	179.984161	4.061338
0.855652	181.652393	4.066342
0.780900	184.382118	4.071347
0.964791	190.545274	4.076352
1.083030	180.814864	4.081357
1.327856	183.176526	4.086362
0.840523	185.612853	4.091366
1.035117	189.302217	4.096371
1.131693	203.125992	4.101376
1.120845	214.171912	4.106381
1.449476	209.080345	4.111386
1.217168	221.392737	4.116390
1.555367	215.863471	4.121395
1.660920	221.200540	4.126400
1.250497	222.473473	4.131405
1.645855	213.751322	4.136410
1.384881	212.290878	4.141414
1.601650	216.258372	4.146419
1.443215	226.896378	4.151424
1.431171	219.621062	4.156429
1.441479	221.942234	4.161434
1.387207	219.526596	4.166438
1.292365	221.055511	4.171443
1.527906	211.919767	4.176448
1.556274	216.278990	4.181453
1.552743	222.950352	4.186458
1.340302	224.014872	4.191462
1.675343	221.673890	4.196467
1.803922	221.524963	4.201472
1.756527	223.070293	4.206477
1.689386	217.782591	4.211482
1.207331	217.013909	4.216486
1.641957	213.350076	4.221491
1.374258	222.398872	4.226496
1.268110	218.369724	4.231501
1.334509	221.671247	4.236506
1.345133	218.399279	4.241510
1.375437	217.587790	4.246515
1.546800	227.393485	4.251520
1.674690	228.288381	4.256525
1.792946	238.985363	4.261530
1.683501	248.579455	4.266534
1.643813	242.920744	4.271539
1.566100	243.425611	4.276544
1.685496	257.188428	4.281549
1.612148	249.480624	4.286554
1.443683	257.419767	4.291558
1.631698	243.912983	4.296563
1.921057	246.233536	4.301568
1.648820	249.055766	4.306573
1.838605	247.248749	4.311578
1.549594	256.949738	4.316582
1.800868	243.151671	4.321587
1.751002	247.163127	4.326592
1.950650	244.794240	4.331597
1.768783	242.677773	4.336602
1.631343	256.019970	4.341606
1.700041	248.167087	4.346611
1.807943	251.543244	4.351616
1.849071	263.413548	4.356621
2.021337	268.017336	4.361626
2.181257	278.865316	4.366630
1.948437	274.693734	4.371635
2.005745	280.903541	4.376640
2.058794	273.433504	4.381645
2.369134	272.088418	4.386650
1.853600	255.570341	4.391654
2.114740	252.071190	4.396659
2.023692	252.325280	4.401664
1.911244	256.243303	4.406669
2.274811	267.888537	4.411674
2.012841	281.677426	4.416678
2.412271	278.612599	4.421683
2.123093	256.289092	4.426688
1.858563	253.504120	4.431693
2.317648	261.998848	4.436698
2.248817	278.126156	4.441702
2.272568	267.429194	4.446707
2.010098	266.637568	4.451712
2.215641	272.274625	4.456717
2.535378	270.753735	4.461722
2.153949	262.289242	4.466726
2.059203	263.991603	4.471731
2.080462	271.771661	4.476736
1.962386	277.824617	4.481741
2.450631	279.529112	4.486746
2.081777	290.040780	4.491750
2.562620	285.702674	4.496755
2.466868	280.300891	4.501760
2.773356	290.547006	4.506765
2.570325	274.155752	4.511770
2.583698	260.967167	4.516774
2.388512	253.783731	4.521779
2.184991	257.950875	4.526784
2.150793	260.912674	4.531789
2.263352	267.138586	4.536794
2.423238	276.759138	4.541798
2.580492	274.709256	4.546803
2.481321	273.848951	4.551808
2.595935	278.880049	4.556813
2.484636	274.982968	4.561818
2.296593	271.677581	4.566822
2.514670	285.808692	4.571827
2.334835	288.602801	4.576832
2.555574	293.267242	4.581837
2.665740	290.336745	4.586842
2.481133	293.329772	4.591846
2.476543	283.707845	4.596851
2.205565	287.177729	4.601856
2.242024	288.226101	4.606861
2.391954	287.045317	4.611866
2.602494	300.452279	4.616870
2.638620	281.550563	4.621875
2.456383	289.581593	4.626880
2.461802	283.970850	4.631885
2.656983	279.103628	4.636890
2.343363	296.367101	4.641894
2.522112	285.718068	4.646899
2.442740	285.858730	4.651904
2.460351	297.246914	4.656909
2.991868	309.450262	4.661914
3.016268	303.203707	4.666918
3.000465	285.644187	4.671923
2.723423	294.465859	4.676928
2.323411	292.424382	4.681933
2.706665	285.106866	4.686938
2.463683	306.558371	4.691942
3.139200	308.308032	4.696947
2.889373	305.934826	4.701952
3.017873	303.988369	4.706957
2.964266	290.656928	4.711962
2.704494	299.837066	4.716966
2.872495	288.853548	4.721971
2.860242	294.039651	4.726976
2.829600	310.467922	4.731981
3.003680	311.366620	4.736986
2.765644	312.860448	4.741990
3.012455	317.652007	4.746995
3.210568	311.858186	4.752000
2.379593	311.802040	4.757005
2.825397	304.948159	4.762010
2.946609	313.723828	4.767014
2.908803	303.616218	4.772019
2.881137	310.743120	4.777024
2.836130	313.463600	4.782029
2.796394	306.600133	4.787034
2.536117	316.864929	4.792038
2.635876	306.692110	4.797043
2.794772	316.535842	4.802048
2.587572	323.719120	4.807053
2.932090	333.548702	4.812058
2.927173	349.351142	4.817062
3.311646	344.983393	4.822067
3.391069	352.200920	4.827072
3.303047	352.024118	4.832077
3.749556	345.064922	4.837082
3.082402	335.198653	4.842086
3.507278	323.623978	4.847091
3.355449	314.023256	4.852096
3.201371	319.017163	4.857101
3.365298	315.804842	4.862106
2.995304	315.896735	4.867110
3.100410	311.365485	4.872115
3.261795	310.406976	4.877120
3.070447	320.735546	4.882125
3.476770	323.210794	4.887130
3.202532	327.781381	4.892134
3.436023	332.302627	4.897139
3.567531	319.088117	4.902144
2.982481	315.852208	4.907149
3.346008	327.879736	4.912154
3.665740	344.906764	4.917158
3.571233	328.988260	4.922163
3.440196	326.555124	4.927168
3.195237	322.237339	4.932173
3.611500	316.042913	4.937178
3.530626	314.944153	4.942182
3.120014	316.495764	4.947187
3.427952	313.680517	4.952192
3.086409	318.602060	4.957197
3.596782	334.720543	4.962202
3.662290	342.570271	4.967206
3.555929	340.138769	4.972211
3.619160	327.787265	4.977216
3.307088	332.797865	4.982221
3.294778	335.511948	4.987226
3.434850	344.155846	4.992230
3.762961	346.569851	4.997235
3.811370	349.645666	5.002240
3.554510	351.215037	5.007245
3.601149	348.663280	5.012250
3.573527	349.970518	5.017254
3.310598	346.674949	5.022259
3.469482	353.021691	5.027264
3.679395	348.845451	5.032269
3.815586	352.504072	5.037274
3.857270	349.150761	5.042278
3.537630	353.801493	5.047283
3.907338	357.746068	5.052288
3.802376	356.071121	5.057293
3.703722	357.621598	5.062298
3.357128	353.896859	5.067302
3.524946	346.387260	5.072307
3.853283	354.849816	5.077312
3.428329	349.689005	5.082317
3.923428	355.395759	5.087322
3.560070	358.534628	5.092326
3.668251	351.901805	5.097331
3.330516	347.857295	5.102336
3.694089	347.673204	5.107341
3.862259	349.218768	5.112346
3.209093	362.899440	5.117350
3.702706	368.939157	5.122355
3.611129	378.623513	5.127360
3.851557	386.057121	5.132365
4.328832	387.773313	5.137370
4.097915	377.198564	5.142374
4.479992	383.815814	5.147379
4.253424	362.815987	5.152384
3.966401	365.664563	5.157389
3.948570	353.415065	5.162394
3.777316	358.543452	5.167398
3.853725	366.493608	5.172403
3.647447	372.599094	5.177408
4.118428	377.458733	5.182413
4.120866	374.126716	5.187418
3.938254	379.845846	5.192422
4.069502	384.603675	5.197427
4.141195	382.760548	5.202432
3.977430	375.584481	5.207437
4.071297	385.527037	5.212442
3.772129	385.683967	5.217446
4.220708	378.147004	5.222451
4.163276	378.919066	5.227456
4.033624	383.973281	5.232461
4.033673	382.024404	5.237466
3.917124	392.791553	5.242470
4.066841	391.298212	5.247475
4.074804	383.749154	5.252480
4.188924	390.488724	5.257485
4.646006	385.409575	5.262490
4.063153	389.066103	5.267494
4.096060	382.074341	5.272499
4.339352	385.807589	5.277504
4.267096	389.546911	5.282509
4.237583	378.378964	5.287514
4.103495	391.751310	5.292518
4.131986	387.296464	5.297523
4.206837	381.947700	5.302528
4.016832	386.725177	5.307533
4.228438	382.220277	5.312538
4.108713	397.480549	5.317542
4.521673	406.841218	5.322547
4.632569	419.106409	5.327552
4.210147	406.270083	5.332557
4.148360	409.806589	5.337562
4.516412	407.313096	5.342566
4.523790	420.784984	5.347571
4.234503	418.433687	5.352576
4.399077	418.717480	5.357581
4.750343	414.493544	5.362586
4.679824	414.640832	5.367590
4.597745	408.015414	5.372595
4.667123	402.649985	5.377600
4.277294	411.058821	5.382605
4.505471	405.418056	5.387610
4.205271	420.560230	5.392614
4.285828	422.864472	5.397619
4.629076	418.006236	5.402624
4.254798	416.593937	5.407629
4.479274	413.683562	5.412634
4.279402	419.987318	5.417638
4.439398	423.373633	5.422643
4.398804	417.169763	5.427648
4.287567	422.125429	5.432653
4.453698	420.050969	5.437658
4.570783	436.039712	5.442662
4.551289	437.815277	5.447667
4.828004	443.001533	5.452672
4.574295	441.711943	5.457677
4.806814	442.915135	5.462682
4.976749	456.809082	5.467686
4.794863	446.407323	5.472691
4.823300	452.899043	5.477696
4.763438	445.848020	5.482701
4.849200	438.349004	5.487706
4.447091	447.467154	5.492710
4.808285	450.890807	5.497715
4.773773	454.008592	5.502720
4.617321	449.813069	5.507725
5.062499	455.101875	5.512730
4.960456	456.034463	5.517734
4.949373	451.456501	5.522739
4.974858	448.040335	5.527744
4.574488	449.728005	5.532749
4.837519	445.288574	5.537754
4.511797	451.800654	5.542758
4.648500	449.571416	5.547763
4.926068	445.795794	5.552768
4.845406	448.528911	5.557773
4.879191	446.598910	5.562778
5.053488	450.687362	5.567782
5.202530	458.206785	5.572787
5.045833	445.752085	5.577792
4.642210	458.120856	5.582797
5.034847	450.657454	5.587802
5.254103	456.616930	5.592806
5.146865	455.831756	5.597811
5.174773	457.054029	5.602816
5.066947	456.840642	5.607821
4.910295	455.503800	5.612826
4.954483	446.120567	5.617830
4.691679	449.343841	5.622835
4.969129	455.973117	5.627840
4.988960	472.628036	5.632845
5.115480	474.963353	5.637850
5.188941	483.865428	5.642854
5.204171	481.924286	5.647859
5.221702	470.426228	5.652864
4.849113	480.196056	5.657869
5.530759	483.859702	5.662874
5.080540	480.538678	5.667878
5.244405	483.816816	5.672883
5.205330	479.784979	5.677888
5.071333	484.071310	5.682893
5.418180	474.719049	5.687898
5.508021	475.422526	5.692902
5.452818	484.962000	5.697907
5.671572	476.341567	5.702912
5.431111	476.710388	5.707917
5.133456	480.003574	5.712922
5.135222	483.122660	5.717926
5.449629	474.665573	5.722931
5.638191	476.318284	5.727936
5.423773	484.844144	5.732941
5.626498	483.892001	5.737946
5.417815	489.162793	5.742950
5.497259	484.527205	5.747955
5.379022	478.675986	5.752960
5.419644	489.395864	5.757965
5.509768	479.443771	5.762970
5.724022	484.353256	5.767974
5.467209	482.332245	5.772979
5.483299	481.005475	5.777984
5.263440	485.313326	5.782989
5.439192	481.765707	5.787994
5.389384	481.852140	5.792998
5.451406	484.117624	5.798003
5.429274	481.260701	5.803008
5.047024	489.688452	5.808013
5.550745	478.504758	5.813018
5.461941	486.222041	5.818022
5.260622	479.376570	5.823027
5.565645	484.179065	5.828032
5.197785	486.463634	5.833037
5.483178	492.565900	5.838042
5.627178	502.930233	5.843046
5.669409	503.224025	5.848051
5.661014	507.996923	5.853056
5.630187	506.808559	5.858061
5.692182	511.352532	5.863066
5.643931	508.121037	5.868070
5.719399	509.508506	5.873075
5.637338	510.206507	5.878080
5.802216	507.474511	5.883085
5.732133	501.528480	5.888090
5.533359	516.072986	5.893094
5.464362	510.400284	5.898099
5.744026	508.244456	5.903104
5.579361	505.944144	5.908109
5.603459	506.866899	5.913114
5.553049	520.648595	5.918118
5.921409	533.992923	5.923123
6.218887	528.816621	5.928128
5.714735	528.271812	5.933133
6.235536	529.882932	5.938138
5.728401	522.032117	5.943142
5.880386	519.341129	5.948147
5.762163	523.054745	5.953152
5.649445	543.356619	5.958157
5.739255	539.632390	5.963162
6.217085	545.310698	5.968166
6.198754	547.878994	5.973171
5.953592	547.379115	5.978176
6.048506	546.148614	5.983181
5.973395	542.707643	5.988186
6.051348	547.040988	5.993190
6.139915	546.160040	5.998195
6.258263	541.062928	6.003200
5.826117	546.469214	6.008205
5.958306	541.492358	6.013210
5.901246	548.413478	6.018214
6.316854	539.386258	6.023219
6.358016	539.382639	6.028224
5.926446	544.235488	6.033229
6.262590	544.391415	6.038234
6.109026	543.488201	6.043238
6.061202	546.639981	6.048243
6.395126	546.645903	6.053248
6.294363	544.039980	6.058253
6.394798	525.495554	6.063258
6.245807	526.932033	6.068262
5.926149	511.148503	6.073267
5.724905	511.859925	6.078272
5.905255	520.200848	6.083277
6.257169	535.134116	6.088282
5.960115	528.886628	6.093286
5.886209	532.566858	6.098291
5.957901	542.232964	6.103296
6.053609	549.707784	6.108301
6.174802	534.866151	6.113306
6.036930	545.341322	6.118310
5.919141	549.037506	6.123315
6.334816	548.219810	6.128320
6.073556	548.460056	6.133325
6.425191	546.239814	6.138330
6.191464	530.329552	6.143334
5.847629	522.736457	6.148339
6.096176	516.914475	6.153344
5.853668	531.248572	6.158349
6.008422	530.754305	6.163354
5.750668	549.332957	6.168358
6.019656	541.621604	6.173363
6.314343	544.190166	6.178368
6.025092	545.294856	6.183373
6.279785	551.255014	6.188378
6.160342	548.828210	6.193382
6.034905	557.399762	6.198387
6.261612	549.194755	6.203392
6.077521	552.039740	6.208397
6.079278	553.574004	6.213402
6.030806	552.915061	6.218406
6.289349	551.762449	6.223411
6.158638	524.861261	6.228416
5.511739	531.271250	6.233421
5.832429	542.378147	6.238426
5.884593	537.848493	6.243430
6.041712	551.347008	6.248435
6.253145	548.707347	6.253440
5.956223	549.929147	6.258445
6.327177	543.364819	6.263450
6.188298	552.170271	6.268454
6.373452	551.636040	6.273459
6.609525	546.818008	6.278464
5.900218	529.534470	6.283469
6.122705	521.970543	6.288474
6.210982	520.250359	6.293478
5.870466	519.132810	6.298483
6.010268	524.993183	6.303488
5.728977	524.265835	6.308493
6.186643	528.215820	6.313498
6.175702	548.031574	6.318502
6.086203	553.924599	6.323507
6.085022	543.293145	6.328512
5.940702	547.878988	6.333517
6.035588	546.370242	6.338522
6.258079	547.111354	6.343526
6.359430	542.519089	6.348531
6.269125	525.984776	6.353536
6.133336	524.036666	6.358541
5.923814	512.041187	6.363546
5.706420	521.881051	6.368550
6.047104	530.498348	6.373555
6.147191	537.409426	6.378560
6.205913	548.510371	6.383565
6.195046	528.905711	6.388570
5.686738	519.316923	6.393574
5.710981	540.154191	6.398579
6.062862	541.393276	6.403584
6.088246	548.995973	6.408589
6.281574	546.623746	6.413594
6.235464	555.807729	6.418598
6.027555	540.090128	6.423603
6.301391	549.323351	6.428608
5.913481	561.849645	6.433613
6.130912	553.637094	6.438618
6.282953	560.769086	6.443622
5.962398	547.304415	6.448627
6.294245	547.580247	6.453632
5.879951	538.401542	6.458637
5.734671	538.369593	6.463642
6.051120	550.469423	6.468646
6.104869	554.403810	6.473651
6.554994	560.194064	6.478656
6.197168	548.230415	6.483661
6.149129	534.130979	6.488666
5.811309	522.536811	6.493670
5.823253	536.122500	6.498675
6.335528	549.692843	6.503680
5.905522	545.784331	6.508685
6.155899	552.849715	6.513690
5.992610	562.525538	6.518694
6.130055	553.102525	6.523699
6.229796	560.217918	6.528704
6.318969	553.943960	6.533709
6.147882	532.930966	6.538714
5.694236	523.294446	6.543718
5.868204	540.347602	6.548723
6.025307	549.077203	6.553728
5.961974	552.717404	6.558733
5.951480	545.650267	6.563738
6.239788	556.924158	6.568742
5.837524	559.241076	6.573747
6.240843	550.936372	6.578752
6.389109	558.675020	6.583757
6.386362	554.569657	6.588762
5.966095	543.575621	6.593766
6.097684	541.746633	6.598771
6.225785	530.819675	6.603776
6.000462	538.291011	6.608781
5.865126	529.584926	6.613786
6.009790	541.180969	6.618790
6.129064	554.175629	6.623795
6.500797	556.978702	6.628800
5.588797	542.240063	6.633805
6.189935	547.404604	6.638810
6.105576	550.304708	6.643814
6.033508	545.769180	6.648819
6.196691	536.018081	6.653824
6.017182	554.930708	6.658829
6.312288	551.430405	6.663834
6.041285	533.195926	6.668838
5.747357	534.038731	6.673843
6.218354	543.036832	6.678848
5.946738	560.246873	6.683853
6.282453	553.383881	6.688858
6.074803	550.696591	6.693862
6.128196	544.944409	6.698867
6.163145	530.063977	6.703872
6.136158	531.366981	6.708877
6.239992	525.251636	6.713882
5.923397	523.044166	6.718886
5.745106	534.677893	6.723891
6.073497	538.271974	6.728896
5.892816	562.475484	6.733901
6.238845	552.448607	6.738906
6.306894	557.407979	6.743910
5.769264	549.741581	6.748915
6.206675	546.030243	6.753920
6.141866	563.093164	6.758925
6.182062	553.686452	6.763930
6.180340	543.235259	6.768934
5.941874	536.743824	6.773939
6.201662	542.653010	6.778944
6.132898	537.264231	6.783949
6.048542	529.934043	6.788954
6.002287	532.307450	6.793958
5.693877	536.555383	6.798963
6.145649	545.919380	6.803968
5.714890	550.502530	6.808973
6.005719	550.287463	6.813978
6.040208	553.362268	6.818982
5.739159	560.518767	6.823987
6.000692	560.269082	6.828992
5.990634	560.850375	6.833997
5.828982	558.457990	6.839002
5.689802	558.771561	6.844006
5.694330	567.294365	6.849011
6.028916	565.975235	6.854016
5.878690	553.623375	6.859021
6.316686	564.046223	6.864026
6.190297	553.606983	6.869030
5.832812	565.737510	6.874035
5.958928	561.014051	6.879040
5.989202	566.640178	6.884045
5.954030	560.530274	6.889050
6.335056	570.025391	6.894054
6.335245	578.410584	6.899059
6.579590	570.007673	6.904064
6.142064	559.275788	6.909069
6.199079	550.272813	6.914074
6.153679	556.782723	6.919078
6.197906	561.402669	6.924083
6.414191	555.566281	6.929088
6.409367	566.433849	6.934093
6.271670	556.827874	6.939098
6.255424	567.743906	6.944102
6.219709	559.260287	6.949107
6.243105	560.608035	6.954112
5.969451	563.647827	6.959117
5.908557	555.923008	6.964122
5.943498	557.673588	6.969126
5.950414	563.856134	6.974131
6.167986	556.708997	6.979136
6.053291	568.501142	6.984141
6.097564	557.390114	6.989146
6.275232	567.560061	6.994150
5.962778	556.841410	6.999155
5.927597	555.858997	7.004160
5.620921	562.592936	7.009165
5.786142	561.898016	7.014170
5.958927	566.041412	7.019174
5.970568	559.632088	7.024179
6.252137	555.870183	7.029184
5.951625	566.047081	7.034189
6.079366	553.430739	7.039194
6.044554	557.320786	7.044198
5.642624	557.853300	7.049203
6.035487	554.525664	7.054208
5.975994	559.059575	7.059213
6.138498	570.471922	7.064218
5.970403	559.305874	7.069222
6.070451	564.998396	7.074227
6.593123	554.827613	7.079232
6.147493	566.281256	7.084237
6.176454	559.834529	7.089242
6.274990	559.828712	7.094246
5.582613	567.071325	7.099251
6.052124	567.455396	7.104256
5.984784	562.466381	7.109261
5.991940	563.810701	7.114266
6.202720	561.520241	7.119270
5.844363	555.155806	7.124275
6.155829	552.754741	7.129280
5.985174	554.098507	7.134285
6.360390	560.570345	7.139290
6.495297	557.229772	7.144294
5.950375	562.848723	7.149299
6.201738	562.028436	7.154304
5.908230	560.953620	7.159309
5.933572	560.630956	7.164314
5.916849	567.155461	7.169318
5.906335	569.386791	7.174323
6.193575	563.742306	7.179328
6.022234	563.567852	7.184333
5.866605	558.441901	7.189338
5.811885	567.889187	7.194342
5.978651	569.647936	7.199347
6.419589	570.181192	7.204352
5.918225	573.399986	7.209357
6.053740	569.138916	7.214362
6.144525	578.318202	7.219366
5.979862	574.097956	7.224371
6.208274	562.030316	7.229376
6.433441	578.211081	7.234381
6.406244	572.162014	7.239386
6.356633	566.197767	7.244390
5.875546	571.611968	7.249395
6.173341	556.687988	7.254400
6.151195	569.192599	7.259405
6.371528	570.324803	7.264410
6.136025	555.509653	7.269414
5.766160	568.818971	7.274419
5.973142	566.851395	7.279424
6.116560	565.634568	7.284429
6.289080	568.582522	7.289434
6.518045	559.193687	7.294438
6.250237	573.510501	7.299443
6.292243	569.031066	7.304448
5.852143	569.871239	7.309453
6.137821	558.924484	7.314458
6.351573	559.481939	7.319462
6.130337	571.306331	7.324467
5.892786	557.037954	7.329472
6.003201	556.929724	7.334477
5.991056	568.662460	7.339482
6.143124	564.247290	7.344486
6.079424	564.288860	7.349491
6.406375	566.550942	7.354496
5.906533	569.381908	7.359501
6.036127	556.513252	7.364506
6.250041	562.897146	7.369510
6.184627	561.701677	7.374515
6.181980	568.312260	7.379520
5.903584	565.753508	7.384525
6.102234	567.141109	7.389530
6.193201	560.705427	7.394534
6.109909	564.546867	7.399539
6.305970	563.146085	7.404544
5.956560	562.401203	7.409549
6.067934	549.015185	7.414554
6.177540	551.089865	7.419558
5.653002	549.475691	7.424563
6.098232	553.091080	7.429568
6.009365	567.615856	7.434573
5.973813	572.627909	7.439578
6.499720	568.101105	7.444582
6.107737	574.654598	7.449587
5.988087	563.911911	7.454592
6.051478	566.661058	7.459597
6.037261	564.913834	7.464602
6.352468	565.473829	7.469606
5.989263	551.114372	7.474611
5.927191	544.216609	7.479616
5.919097	554.925260	7.484621
6.087953	559.908000	7.489626
6.034510	558.791261	7.494630
6.095944	565.144162	7.499635
6.411488	570.626358	7.504640
6.334895	565.594670	7.509645
5.760763	546.121541	7.514650
5.811689	550.498436	7.519654
6.222356	561.740821	7.524659
6.608237	553.972809	7.529664
6.323746	548.184218	7.534669
6.128310	537.218475	7.539674
5.918847	535.680006	7.544678
5.807024	536.728280	7.549683
6.071345	540.882759	7.554688
5.971825	537.990884	7.559693
5.940680	538.883715	7.564698
6.361229	549.855678	7.569702
5.919735	542.579096	7.574707
6.245378	538.193407	7.579712
6.125739	540.856821	7.584717
5.938634	532.928143	7.589722
5.797342	539.957140	7.594726
5.868422	559.177766	7.599731
6.284385	555.366966	7.604736
6.055168	563.624372	7.609741
6.108411	568.645204	7.614746
6.202572	569.195032	7.619750
5.929805	579.201382	7.624755
6.315449	573.708733	7.629760
6.226783	560.444040	7.634765
6.081754	548.205978	7.639770
6.024547	533.616092	7.644774
5.903321	541.561963	7.649779
6.328476	548.110975	7.654784
5.748045	550.006076	7.659789
5.594051	556.466478	7.664794
6.230290	568.211438	7.669798
6.158096	568.658567	7.674803
6.239487	572.897219	7.679808
6.215848	572.962546	7.684813
6.144503	574.042207	7.689818
6.275534	561.553190	7.694822
6.060378	556.496693	7.699827
6.467599	538.126223	7.704832
6.105333	538.323597	7.709837
5.630868	540.736929	7.714842
5.882752	541.683538	7.719846
5.549678	560.611140	7.724851
5.966741	561.841604	7.729856
5.998060	571.957640	7.734861
6.099508	577.445491	7.739866
6.116029	578.661963	7.744870
6.238277	568.295605	7.749875
6.205141	569.646992	7.754880
6.085319	570.990236	7.759885
6.342073	568.713869	7.764890
6.521616	567.732605	7.769894
5.929190	551.687140	7.774899
5.721782	542.881879	7.779904
6.134738	557.048064	7.784909
6.266109	572.167075	7.789914
6.502362	562.282693	7.794918
6.346912	544.741661	7.799923
6.200530	539.667073	7.804928
5.782456	543.247410	7.809933
5.814086	543.942769	7.814938
6.055813	531.196862	7.819942
6.077949	536.370839	7.824947
5.964996	534.655952	7.829952
5.751548	537.238795	7.834957
5.797081	556.499366	7.839962
6.117344	559.624536	7.844966
5.962225	565.550731	7.849971
6.464039	567.806355	7.854976
6.171969	570.945894	7.859981
6.144422	562.870599	7.864986
6.350185	551.564307	7.869990
6.126680	541.898350	7.874995
6.278278	531.804616	7.880000
5.818569	534.230896	7.885005
5.824454	530.789541	7.890010
6.016544	540.518790	7.895014
6.000546	560.966688	7.900019
6.464067	562.757207	7.905024
5.861811	556.492754	7.910029
5.858881	557.459456	7.915034
6.212999	560.423713	7.920038
6.036573	566.354620	7.925043
6.250168	560.440134	7.930048
6.230175	554.021842	7.935053
6.202731	536.522970	7.940058
6.142743	538.930226	7.945062
5.998266	536.722276	7.950067
6.002350	535.051751	7.955072
5.818600	540.255677	7.960077
5.421282	552.017645	7.965082
6.195466	550.342543	7.970086
5.871495	569.538807	7.975091
6.136953	563.979232	7.980096
6.426516	556.734529	7.985101
6.292114	565.788093	7.990106
6.417002	562.286570	7.995110
5.995040	561.530218	8.000115
6.318547	531.917606	8.005133
6.034923	541.234224	8.010150
5.784882	528.994654	8.015168
6.157780	544.845396	8.020186
6.197868	558.105778	8.025203
6.216786	553.393763	8.030221
5.867911	544.268164	8.035238
6.091527	552.961465	8.040256
5.966334	556.848697	8.045274
6.268211	562.997923	8.050291
6.353480	554.981056	8.055309
6.172244	556.755472	8.060326
5.935214	549.985396	8.065344
5.848822	552.779664	8.070362
6.058400	562.979718	8.075379
6.241475	568.070741	8.080397
6.351014	566.315361	8.085414
6.445515	570.449859	8.090432
6.303016	546.364156	8.095450
5.804436	540.604057	8.100467
6.191437	551.982710	8.105485
6.374737	557.688610	8.110502
6.240229	558.473467	8.115520
6.173911	547.430343	8.120538
6.044774	561.117343	8.125555
6.061808	564.679865	8.130573
6.231942	568.338485	8.135590
6.234216	569.718762	8.140608
6.322326	565.366717	8.145626
6.226258	571.664513	8.150643
6.189782	566.089482	8.155661
6.462762	570.120810	8.160678
6.345666	560.145067	8.165696
6.329355	541.230831	8.170714
6.205631	536.834349	8.175731
6.047560	532.519141	8.180749
6.369911	546.537638	8.185766
6.457403	563.842646	8.190784
6.432906	537.886561	8.195802
6.083219	546.883634	8.200819
6.444048	533.524476	8.205837
5.987192	532.763807	8.210854
6.054870	545.023421	8.215872
6.214064	556.969290	8.220890
6.316767	562.384621	8.225907
6.598526	567.458516	8.230925
6.235270	568.006467	8.235942
6.100444	576.605800	8.240960
6.059153	565.576628	8.245978
6.128227	570.940251	8.250995
6.043427	567.497092	8.256013
6.028746	568.109166	8.261030
5.798616	565.865777	8.266048
6.257802	565.417367	8.271066
6.175329	565.780645	8.276083
6.326188	563.260996	8.281101
6.467806	565.498058	8.286118
5.939430	561.848054	8.291136
6.422156	575.461702	8.296154
6.420477	600.044600	8.301171
6.306659	595.302586	8.306189
6.568383	599.812919	8.311206
6.332056	607.277775	8.316224
6.605652	593.161015	8.321242
6.079518	581.332056	8.326259
6.350594	595.579546	8.331277
6.344984	598.067748	8.336294
6.246147	597.403294	8.341312
6.716042	595.393963	8.346330
6.142387	590.855447	8.351347
6.295415	600.349978	8.356365
6.609918	604.903537	8.361382
6.443790	607.056534	8.366400
6.182971	598.714890	8.371418
5.935018	601.800665	8.376435
6.396755	600.674711	8.381453
6.633610	607.161472	8.386470
6.463820	610.081954	8.391488
7.079021	593.842231	8.396506
6.791727	611.903989	8.401523
6.802404	604.379141	8.406541
6.774988	604.202236	8.411558
6.538451	599.233905	8.416576
6.403358	577.954612	8.421594
6.480618	582.391553	8.426611
6.377007	594.379393	8.431629
6.186600	595.067019	8.436646
6.165580	608.153127	8.441664
6.445449	599.832771	8.446682
6.663014	605.901297	8.451699
6.415389	598.925685	8.456717
6.436431	591.953419	8.461734
6.330547	597.823156	8.466752
6.647479	596.783381	8.471770
6.733232	597.596331	8.476787
6.584494	599.221679	8.481805
6.787706	591.653342	8.486822
6.685243	607.002978	8.491840
6.871575	599.190402	8.496858
6.421263	598.394593	8.501875
6.367449	603.469345	8.506893
6.582855	605.477281	8.511910
6.473319	604.129408	8.516928
6.242702	604.536901	8.521946
6.571044	612.348583	8.526963
6.494824	611.524685	8.531981
6.635422	597.775984	8.536998
6.626788	608.032475	8.542016
6.639524	597.068936	8.547034
6.735638	600.033765	8.552051
6.367210	610.012258	8.557069
6.702381	601.740024	8.562087
6.608277	603.148269	8.567104
6.655443	602.178556	8.572122
6.631324	603.383296	8.577139
6.685194	604.049567	8.582157
7.036415	602.380731	8.587175
6.753213	600.536256	8.592192
7.038823	598.502916	8.597210
6.954503	596.881201	8.602227
6.541861	601.489027	8.607245
6.627084	594.497866	8.612263
5.952468	603.307846	8.617280
6.487174	607.336787	8.622298
6.838812	611.411987	8.627315
7.029698	617.101102	8.632333
6.748718	609.339525	8.637351
6.362327	608.918932	8.642368
6.902300	619.952445	8.647386
7.010906	631.724083	8.652403
6.818526	614.042378	8.657421
6.802155	595.537902	8.662439
6.570979	610.818113	8.667456
6.586741	613.438794	8.672474
6.643973	625.587610	8.677491
7.037944	630.871080	8.682509
6.913413	635.027692	8.687527
6.972087	633.516538	8.692544
7.146741	614.707985	8.697562
6.966033	599.424796	8.702579
6.651621	610.439944	8.707597
6.527290	600.587216	8.712615
6.634471	603.360659	8.717632
6.963374	617.975143	8.722650
7.044261	629.030354	8.727667
6.690853	624.855528	8.732685
6.852958	623.148915	8.737703
6.924613	623.007570	8.742720
7.183802	627.534865	8.747738
7.144236	611.978703	8.752755
6.890489	610.770055	8.757773
6.966906	596.400922	8.762791
6.415314	609.117829	8.767808
6.601540	605.928385	8.772826
7.212779	618.960789	8.777843
6.653799	628.525207	8.782861
7.208134	628.957044	8.787879
6.936447	629.109938	8.792896
6.977182	613.337342	8.797914
7.243338	606.033163	8.802931
7.010184	603.908175	8.807949
7.340977	596.532278	8.812967
7.174781	604.527019	8.817984
6.893551	600.968750	8.823002
6.912114	602.852204	8.828019
6.833524	605.619009	8.833037
6.801150	593.829927	8.838055
6.823464	596.086355	8.843072
6.807478	604.093622	8.848090
6.734835	603.588402	8.853107
7.411444	627.235856	8.858125
7.340228	604.486596	8.863143
7.197318	600.149962	8.868160
7.046941	597.563857	8.873178
7.027271	599.677445	8.878195
7.167926	604.331833	8.883213
7.163685	601.238294	8.888231
6.980265	605.683370	8.893248
7.041229	601.976712	8.898266
6.987482	595.792564	8.903283
6.534391	602.075480	8.908301
6.912510	596.629215	8.913319
6.817324	605.096811	8.918336
6.907133	628.454450	8.923354
7.079905	626.842914	8.928371
6.809473	635.295256	8.933389
6.781404	635.790069	8.938407
7.037690	639.296654	8.943424
7.200461	635.623914	8.948442
6.949455	641.421050	8.953459
7.009427	638.898330	8.958477
7.021756	634.607236	8.963495
7.007969	645.659238	8.968512
6.955510	638.799116	8.973530
7.360065	622.627508	8.978547
6.946288	637.239800	8.983565
6.866798	634.039431	8.988583
6.725656	641.688332	8.993600
6.862456	639.112735	8.998618
7.388687	646.425161	9.003635
7.460013	667.184905	9.008653
7.376795	651.142262	9.013671
7.380772	651.536893	9.018688
7.327821	642.871848	9.023706
7.416302	635.407325	9.028723
7.044030	633.038063	9.033741
7.487767	632.092242	9.038759
7.416802	639.564966	9.043776
7.383096	631.386078	9.048794
7.651189	626.248161	9.053811
7.400353	631.786424	9.058829
7.290805	633.642672	9.063847
6.980419	629.633348	9.068864
7.108449	644.170693	9.073882
7.405447	636.677153	9.078899
7.132866	645.516643	9.083917
7.172461	634.022680	9.088935
7.261260	646.159199	9.093952
6.942379	640.674208	9.098970
7.257171	636.823550	9.103987
7.180920	629.670934	9.109005
7.447834	625.362291	9.114023
7.409189	627.218215	9.119040
7.342604	627.733972	9.124058
7.486457	629.137657	9.129075
6.918032	638.346385	9.134093
7.236493	638.179920	9.139111
7.264866	640.182218	9.144128
7.109006	636.021329	9.149146
7.475055	647.909198	9.154163
7.032280	647.803433	9.159181
7.591127	658.615358	9.164199
7.719162	658.801270	9.169216
7.190428	654.412374	9.174234
7.360312	650.482170	9.179251
7.491168	654.044959	9.184269
7.454372	650.866649	9.189287
7.268006	646.705690	9.194304
7.112457	660.244405	9.199322
7.452915	651.613418	9.204339
7.351424	663.896807	9.209357
7.314324	663.410108	9.214375
7.463350	658.249969	9.219392
7.281690	665.128475	9.224410
7.865315	655.931663	9.229427
7.722545	663.176540	9.234445
7.569668	659.914700	9.239463
7.811263	663.049338	9.244480
7.223637	661.821173	9.249498
7.583701	647.073944	9.254515
7.459001	651.805354	9.259533
7.639636	663.464899	9.264551
7.598033	655.774677	9.269568
7.288529	657.759702	9.274586
7.606067	660.268023	9.279603
7.383386	663.948799	9.284621
7.483133	656.629241	9.289639
7.687263	658.510319	9.294656
7.268237	669.918005	9.299674
7.723619	656.430888	9.304691
7.378297	658.492312	9.309709
7.689528	665.457302	9.314727
7.802882	669.397771	9.319744
7.571903	664.613920	9.324762
7.930330	667.967780	9.329779
7.746866	666.421133	9.334797
7.499647	658.190584	9.339815
7.656913	648.833681	9.344832
7.604709	656.250948	9.349850
7.519573	654.910053	9.354867
7.854098	655.270028	9.359885
7.646082	655.858020	9.364903
7.623817	654.572852	9.369920
7.434773	659.887718	9.374938
7.707858	652.285932	9.379955
7.414398	661.200143	9.384973
7.601250	660.570855	9.389991
7.823303	656.973722	9.395008
7.686389	667.140673	9.400026
7.919032	661.524196	9.405043
7.887481	673.670036	9.410061
7.710439	660.162053	9.415079
7.607888	649.503769	9.420096
7.865959	660.188740	9.425114
7.869861	651.132804	9.430131
7.568819	646.989259	9.435149
7.355778	643.079160	9.440167
7.945658	652.138417	9.445184
7.589746	664.825330	9.450202
7.866432	663.245006	9.455219
7.920455	671.650138	9.460237
7.665040	664.998009	9.465255
8.008280	660.761556	9.470272
7.654858	661.387010	9.475290
7.645484	670.533696	9.480307
7.901745	662.284732	9.485325
7.859100	660.636820	9.490343
8.121780	658.920241	9.495360
7.493906	656.831080	9.500378
7.630696	659.372086	9.505395
7.311623	665.972184	9.510413
6.916479	671.160954	9.515431
7.245749	659.079276	9.520448
7.066688	667.120271	9.525466
7.510207	674.795598	9.530483
7.566921	686.454421	9.535501
7.549690	693.479323	9.540519
7.802627	691.541533	9.545536
7.677124	698.764277	9.550554
7.716791	694.493048	9.555571
7.807332	691.877860	9.560589
7.922214	693.822930	9.565607
7.938847	690.660173	9.570624
7.928575	705.312990	9.575642
7.900461	693.123938	9.580659
8.408413	692.113941	9.585677
8.140584	693.114570	9.590695
8.075860	679.971807	9.595712
7.568551	695.079334	9.600730
8.044882	683.962596	9.605747
8.128407	692.933292	9.610765
8.003920	696.066746	9.615783
7.586785	688.987870	9.620800
7.603651	697.267287	9.625818
7.826551	697.487489	9.630835
8.087145	714.550432	9.635853
7.706879	727.796120	9.640871
8.203374	728.526104	9.645888
7.791753	725.204739	9.650906
8.372104	726.070828	9.655923
8.084504	728.654955	9.660941
7.913913	721.629722	9.665959
8.190374	714.971779	9.670976
7.994634	719.911812	9.675994
8.049086	723.204608	9.681011
7.939896	718.460412	9.686029
7.924892	727.850175	9.691047
8.233758	714.491594	9.696064
8.179047	733.357057	9.701082
7.972720	731.703959	9.706099
8.297127	733.687957	9.711117
8.207298	730.531797	9.716135
8.275045	720.374368	9.721152
8.095095	733.904196	9.726170
8.293536	722.092150	9.731187
8.092313	722.269989	9.736205
8.022889	711.467209	9.741223
8.126054	712.357985	9.746240
8.257173	727.317706	9.751258
8.147983	726.718540	9.756275
8.337781	725.770276	9.761293
8.113695	725.523186	9.766311
8.285806	730.971963	9.771328
8.243268	725.974223	9.776346
8.269919	721.021324	9.781363
8.247407	709.908433	9.786381
8.008166	706.483729	9.791399
8.319718	713.281769	9.796416
8.291259	712.136590	9.801434
8.243176	725.740632	9.806451
8.373456	712.644287	9.811469
7.955346	711.186092	9.816487
8.384552	712.815747	9.821504
8.394676	723.979587	9.826522
8.260451	723.058601	9.831539
8.424654	718.175440	9.836557
8.168187	715.667312	9.841575
8.391542	718.386109	9.846592
8.254605	701.172064	9.851610
8.339472	710.979899	9.856627
8.550273	713.593693	9.861645
8.230726	707.520242	9.866663
8.392024	700.981368	9.871680
7.921271	699.910215	9.876698
8.287035	708.724743	9.881715
8.421790	728.696161	9.886733
8.277922	728.359414	9.891751
8.437020	728.660256	9.896768
8.696797	728.793254	9.901786
8.251726	730.248799	9.906803
8.438558	723.594277	9.911821
8.373191	716.526428	9.916839
8.456240	721.119135	9.921856
8.517312	722.987690	9.926874
8.262933	728.153171	9.931891
8.828435	726.975383	9.936909
8.342096	727.840160	9.941927
8.627939	723.224634	9.946944
8.241272	713.971932	9.951962
8.416207	723.429054	9.956979
8.527354	719.558556	9.961997
8.278332	717.245640	9.967015
8.106943	711.428346	9.972032
8.149484	718.104012	9.977050
8.174942	725.160441	9.982067
8.378818	717.226797	9.987085
8.279871	719.597805	9.992103
8.431280	723.898501	9.997120
8.480212	716.108618	10.002138
7.984067	721.312948	10.007155
8.377173	727.273129	10.012173
8.338512	745.090734	10.017191
8.719367	748.576718	10.022208
8.623706	748.199313	10.027226
8.628368	756.162297	10.032243
8.768127	753.886961	10.037261
8.628865	752.627851	10.042279
8.710268	748.876831	10.047296
8.853197	747.217471	10.052314
8.306431	733.166350	10.057331
8.861313	730.546705	10.062349
8.729668	729.541438	10.067367
8.620100	722.502557	10.072384
8.524231	714.150860	10.077402
8.370297	730.023480	10.082419
8.837543	732.992428	10.087437
8.474189	734.957247	10.092455
9.067112	742.599995	10.097472
8.913990	732.375987	10.102490
8.554018	734.316625	10.107507
8.903602	729.713770	10.112525
8.460520	720.504262	10.117543
8.501990	723.064999	10.122560
8.513298	731.796903	10.127578
8.596204	746.170172	10.132595
8.914227	750.177554	10.137613
8.718488	761.809342	10.142631
8.860099	753.222248	10.147648
8.903272	766.271877	10.152666
8.647895	747.128291	10.157683
8.793799	749.249323	10.162701
8.820142	756.559148	10.167719
9.193593	753.732153	10.172736
8.822577	737.657159	10.177754
8.624749	730.139217	10.182771
8.931819	717.908816	10.187789
8.354240	729.824268	10.192807
8.765608	742.543633	10.197824
8.995085	753.840454	10.202842
8.829757	758.603819	10.207859
8.787574	748.923997	10.212877
8.772275	759.078745	10.217895
8.930719	763.240500	10.222912
9.005448	759.081157	10.227930
8.758906	764.485495	10.232947
9.201952	762.362683	10.237965
8.959672	764.497210	10.242983
8.988094	761.962765	10.248000
9.002634	740.613198	10.253018
8.827389	740.956805	10.258035
8.718172	729.560636	10.263053
8.552749	746.900051	10.268071
8.879449	761.351856	10.273088
8.980367	765.328266	10.278106
8.665246	754.460634	10.283123
8.911857	748.084375	10.288141
8.642984	755.126566	10.293159
9.054283	756.477317	10.298176
8.893425	752.874279	10.303194
8.570133	764.269331	10.308211
9.232081	756.905056	10.313229
8.989155	757.467732	10.318247
8.854388	755.773649	10.323264
9.091522	753.555414	10.328282
8.993523	763.095547	10.333299
9.278960	748.260586	10.338317
8.987293	758.279610	10.343335
8.981203	756.393364	10.348352
9.216521	759.157821	10.353370
9.160873	761.910227	10.358387
9.204577	755.666771	10.363405
9.122123	763.330816	10.368423
8.961854	768.079174	10.373440
8.832020	755.724249	10.378458
8.861471	762.787908	10.383475
9.111300	754.404929	10.388493
9.222135	758.657632	10.393511
9.091897	761.895589	10.398528
9.210912	751.523363	10.403546
8.987270	761.439792	10.408563
8.940046	754.935424	10.413581
9.234127	761.111216	10.418599
9.432847	779.481253	10.423616
9.412765	760.859681	10.428634
8.798223	770.121198	10.433651
9.078426	777.559461	10.438669
9.056601	787.720426	10.443687
9.081324	785.689712	10.448704
9.641195	785.397450	10.453722
9.169315	796.866339	10.458739
9.163502	792.328219	10.463757
9.463497	794.326110	10.468775
9.181113	796.655855	10.473792
9.499627	792.908079	10.478810
9.071461	792.655806	10.483827
9.222285	786.048163	10.488845
9.423475	790.156786	10.493863
9.097353	782.885641	10.498880
9.599440	787.899111	10.503898
9.230948	789.995095	10.508915
9.471126	792.092255	10.513933
9.264245	790.957324	10.518951
9.464604	797.599019	10.523968
9.566066	782.901175	10.528986
9.045571	797.578725	10.534003
9.274934	791.834405	10.539021
9.604095	799.052378	10.544039
9.345499	801.041588	10.549056
9.446622	798.651784	10.554074
9.355642	803.295378	10.559091
9.290423	794.726762	10.564109
9.440375	806.018287	10.569127
9.596681	799.075102	10.574144
9.425275	795.832443	10.579162
9.473195	800.415242	10.584179
9.192073	792.544153	10.589197
9.492641	801.961230	10.594215
9.105364	800.642402	10.599232
9.599011	791.984397	10.604250
9.135225	805.854183	10.609267
9.168171	795.509565	10.614285
9.303801	799.809352	10.619303
9.356260	800.064470	10.624320
9.977435	787.539891	10.629338
9.516762	800.515506	10.634355
9.452325	792.677037	10.639373
9.544200	792.504392	10.644391
9.655207	800.641118	10.649408
9.833340	796.648885	10.654426
9.425799	800.847678	10.659443
9.480079	796.431883	10.664461
9.567421	799.620829	10.669479
9.430847	792.376164	10.674496
9.724748	787.987619	10.679514
9.443855	803.038469	10.684531
9.241293	790.579030	10.689549
9.627450	789.221498	10.694567
9.508997	799.149665	10.699584
9.591950	819.190010	10.704602
9.571573	821.736596	10.709619
9.796354	818.472421	10.714637
9.747095	821.744618	10.719655
9.667655	833.129655	10.724672
9.958942	808.156798	10.729690
9.619485	800.049708	10.734707
9.889283	801.579004	10.739725
9.889508	786.299133	10.744743
9.442047	796.152650	10.749760
9.386141	798.020507	10.754778
9.220409	815.508860	10.759795
9.603426	817.634731	10.764813
9.921215	820.725290	10.769831
9.819212	828.043016	10.774848
10.022921	816.859914	10.779866
9.936662	822.956198	10.784883
9.856122	821.344463	10.789901
9.740861	812.727433	10.794919
9.802285	821.396368	10.799936
9.523862	813.578755	10.804954
9.869781	810.069732	10.809971
9.740062	818.897868	10.814989
10.117829	820.371888	10.820007
9.864792	822.862516	10.825024
10.034169	816.836402	10.830042
9.956725	822.008834	10.835059
9.885202	821.399096	10.840077
10.108684	823.928924	10.845095
9.902278	822.073871	10.850112
10.257894	822.043765	10.855130
10.330601	817.124152	10.860147
9.649531	796.800272	10.865165
9.836543	805.175582	10.870183
9.676134	814.917410	10.875200
10.216972	815.730996	10.880218
10.009845	820.706015	10.885235
9.722660	816.281799	10.890253
10.265480	812.816545	10.895271
9.801456	819.393468	10.900288
10.196822	816.516773	10.905306
9.847931	825.573320	10.910323
10.079655	817.208659	10.915341
10.110080	819.290557	10.920359
10.147550	818.666709	10.925376
10.161738	818.891552	10.930394
10.359383	826.459251	10.935411
9.827724	807.044820	10.940429
10.377908	807.086034	10.945447
9.721218	792.220034	10.950464
10.158699	798.851992	10.955482
9.996656	814.894930	10.960499
10.098523	818.391695	10.965517
10.177979	820.459176	10.970535
9.933151	825.176280	10.975552
10.335636	810.239599	10.980570
10.246452	818.855522	10.985587
9.994689	824.834731	10.990605
10.381946	818.943789	10.995623
9.868290	820.068591	11.000640
10.095373	816.185958	11.005658
10.099921	820.496433	11.010675
10.140296	818.021808	11.015693
10.256484	812.572190	11.020711
10.015363	819.960583	11.025728
10.194443	818.996767	11.030746
10.218455	820.595108	11.035763
10.092983	815.335102	11.040781
10.181780	814.088614	11.045799
10.155376	823.218526	11.050816
10.183797	825.148403	11.055834
10.606120	812.988603	11.060851
10.220666	819.422995	11.065869
10.347670	810.655227	11.070887
10.284129	818.351598	11.075904
10.071599	813.342610	11.080922
10.241973	821.107725	11.085939
10.084144	818.332079	11.090957
10.140596	820.507301	11.095975
10.335991	826.065636	11.100992
10.516867	820.150603	11.106010
10.468848	824.093425	11.111027
10.253484	819.552202	11.116045
10.261653	816.783714	11.121063
10.226761	828.890466	11.126080
10.604961	831.303343	11.131098
10.618182	826.616793	11.136115
10.228561	830.120538	11.141133
10.528248	822.706381	11.146151
10.348318	811.974975	11.151168
10.483481	826.547922	11.156186
10.466537	830.587564	11.161203
10.226908	838.266649	11.166221
10.735323	841.985061	11.171239
10.664717	849.547586	11.176256
10.715793	847.755795	11.181274
10.528717	827.768952	11.186291
10.192586	825.459420	11.191309
10.834548	830.854446	11.196327
10.717514	825.880426	11.201344
10.212674	829.265461	11.206362
10.305163	825.931857	11.211379
10.621229	842.155090	11.216397
11.042126	841.721281	11.221415
10.781703	833.405822	11.226432
10.851729	824.578587	11.231450
10.689803	823.864927	11.236467
10.606747	824.471601	11.241485
10.322135	813.915788	11.246503
10.406888	818.477534	11.251520
10.748509	828.816127	11.256538
10.764262	827.625826	11.261555
10.357272	836.086913	11.266573
10.809426	838.341883	11.271591
10.798464	850.213599	11.276608
10.454809	851.014206	11.281626
10.636601	850.724314	11.286643
10.675321	862.553170	11.291661
10.549506	852.393849	11.296679
10.524395	860.838170	11.301696
10.666678	851.554096	11.306714
10.927183	854.414395	11.311731
10.519597	849.751064	11.316749
10.623876	850.549543	11.321767
10.558769	856.476598	11.326784
10.501046	855.677575	11.331802
10.399865	853.142530	11.336819
10.143698	855.913195	11.341837
10.597307	869.669318	11.346855
10.593710	893.016052	11.351872
10.840799	883.368558	11.356890
11.133026	880.882927	11.361907
10.954436	875.771847	11.366925
11.282403	877.470643	11.371943
10.891560	882.504842	11.376960
10.878156	879.906047	11.381978
11.132135	881.816298	11.386995
10.902533	883.545612	11.392013
10.864549	878.340780	11.397031
11.262255	878.617468	11.402048
10.681656	870.867578	11.407066
11.133488	869.468458	11.412083
10.804401	881.030294	11.417101
11.021623	872.962872	11.422119
11.199795	876.565906	11.427136
11.047478	870.537924	11.432154
10.857385	851.932977	11.437171
10.957297	859.030679	11.442189
11.010744	864.484586	11.447207
10.908314	873.086591	11.452224
10.739593	877.568679	11.457242
11.236813	879.124495	11.462259
11.036623	875.499989	11.467277
11.214634	872.012850	11.472295
11.045931	875.511913	11.477312
10.985962	886.722514	11.482330
10.986873	878.055111	11.487347
10.705054	884.942425	11.492365
11.156082	874.560414	11.497383
10.965474	884.151387	11.502400
10.996435	876.176220	11.507418
11.077062	869.776611	11.512435
10.719204	878.070145	11.517453
10.946983	868.991183	11.522471
11.044170	873.841424	11.527488
10.889293	885.718888	11.532506
11.350474	886.731487	11.537523
11.121743	899.253050	11.542541
11.375238	903.490831	11.547559
11.281616	908.948241	11.552576
11.331166	901.499091	11.557594
11.508412	889.927817	11.562611
10.871028	886.924494	11.567629
11.445775	897.892215	11.572647
11.624679	905.167007	11.577664
11.077970	895.798577	11.582682
11.335109	880.806371	11.587699
11.069041	890.606685	11.592717
11.092027	891.846559	11.597735
11.363071	903.923970	11.602752
11.205777	917.231712	11.607770
11.839192	905.936451	11.612787
11.535140	911.760579	11.617805
11.259035	906.165660	11.622823
11.350849	902.899076	11.627840
11.341284	910.741273	11.632858
11.696801	907.997532	11.637875
11.309554	907.900678	11.642893
11.466307	901.556558	11.647911
11.337609	908.516554	11.652928
11.360534	910.167838	11.657946
11.374961	909.392691	11.662963
11.285786	907.472942	11.667981
11.339395	907.581422	11.672999
11.296997	902.052525	11.678016
11.592346	912.688193	11.683034
11.639213	911.854920	11.688051
11.238077	914.631491	11.693069
11.433150	907.927103	11.698087
11.462033	904.376465	11.703104
11.200035	911.516402	11.708122
11.457804	905.133902	11.713139
11.160237	908.466523	11.718157
11.512728	909.031394	11.723175
11.529294	916.811002	11.728192
11.523156	934.443920	11.733210
12.065775	928.742557	11.738227
11.461255	923.123669	11.743245
11.747171	912.348913	11.748263
11.595483	913.337805	11.753280
11.450769	908.540380	11.758298
11.658190	927.119772	11.763315
11.538176	937.817148	11.768333
11.527797	936.692186	11.773351
11.718883	939.854928	11.778368
11.822922	942.293141	11.783386
12.017348	932.426394	11.788403
11.928299	940.837647	11.793421
11.927765	921.287885	11.798439
12.083391	916.653709	11.803456
11.610615	903.966887	11.808474
11.830322	892.137018	11.813491
11.658287	893.032431	11.818509
11.685328	892.908708	11.823527
12.051193	889.152282	11.828544
11.766858	898.256446	11.833562
11.969755	902.332535	11.838579
11.868751	899.527781	11.843597
11.680211	897.696137	11.848615
11.815198	901.061458	11.853632
11.434932	918.439394	11.858650
12.261148	919.141169	11.863667
12.329539	920.443209	11.868685
11.984752	893.307928	11.873703
12.026337	899.839744	11.878720
12.141853	902.103224	11.883738
11.995591	897.421015	11.888755
11.679656	900.210245	11.893773
11.601063	899.472154	11.898791
11.967582	903.011725	11.903808
12.105445	921.784509	11.908826
12.116566	912.311890	11.913843
12.307793	892.627266	11.918861
11.750158	893.753056	11.923879
12.131863	891.816360	11.928896
11.999164	892.405668	11.933914
11.799130	888.861838	11.938931
12.018237	904.399651	11.943949
12.099869	921.660952	11.948967
12.363835	928.207923	11.953984
11.975871	928.875719	11.959002
12.008175	930.979762	11.964019
12.105252	937.272100	11.969037
12.120913	930.803307	11.974055
12.516263	925.727483	11.979072
12.015644	926.853677	11.984090
12.515679	919.369293	11.989107
12.199360	917.638723	11.994125
12.109860	900.591397	11.999143
12.171678	898.780892	12.004160
12.095928	909.675241	12.009178
12.564332	915.687197	12.014195
12.302311	898.951104	12.019213
11.817671	896.269714	12.024231
11.958815	908.477295	12.029248
12.329325	917.765151	12.034266
12.501714	925.350465	12.039283
12.310118	920.178534	12.044301
12.289172	928.367884	12.049319
12.601458	923.228654	12.054336
12.269743	934.623650	12.059354
12.633024	930.958189	12.064371
12.436843	906.911127	12.069389
12.184519	898.434850	12.074407
12.442416	901.423931	12.079424
12.190652	907.400809	12.084442
12.684090	912.781484	12.089459
12.491254	903.112339	12.094477
12.287696	898.850227	12.099495
12.075277	895.263566	12.104512
12.034428	909.382295	12.109530
12.358881	918.960048	12.114547
12.592365	924.192441	12.119565
12.421380	925.089257	12.124583
12.554934	923.931015	12.129600
12.512123	929.227663	12.134618
12.647489	921.818621	12.139635
12.726317	931.534687	12.144653
12.566989	930.071414	12.149671
12.590854	922.965467	12.154688
12.635952	927.999932	12.159706
12.570873	926.232484	12.164723
12.609539	925.391907	12.169741
12.579560	923.996976	12.174759
12.722390	922.174630	12.179776
12.759732	926.527339	12.184794
12.790012	921.816284	12.189811
12.554645	907.730762	12.194829
12.440988	914.214671	12.199847
12.738238	910.178671	12.204864
12.435095	926.419095	12.209882
12.308326	925.354743	12.214899
12.326494	931.344412	12.219917
11.988341	937.193881	12.224935
12.249488	925.057926	12.229952
12.147864	931.480010	12.234970
12.427087	948.063770	12.239987
12.940442	955.464300	12.245005
12.827494	952.267436	12.250023
13.040397	949.153620	12.255040
12.912250	960.059042	12.260058
13.155822	948.732242	12.265075
12.700001	935.854406	12.270093
12.780486	935.408855	12.275111
12.784243	933.267032	12.280128
12.742008	945.023139	12.285146
12.996678	952.904277	12.290163
13.091492	950.832409	12.295181
12.962733	936.204429	12.300199
12.679378	917.043613	12.305216
12.277632	930.303659	12.310234
12.959549	948.174220	12.315251
13.358761	943.945745	12.320269
13.202979	936.788440	12.325287
12.743198	948.081823	12.330304
13.078349	948.784601	12.335322
13.137432	955.582822	12.340339
13.230354	942.987329	12.345357
13.136115	928.656382	12.350375
13.136803	919.689006	12.355392
12.903356	926.602579	12.360410
12.765446	921.377666	12.365427
13.262641	923.937382	12.370445
13.144708	924.146704	12.375463
13.392933	919.797968	12.380480
12.979420	926.018556	12.385498
12.872209	921.141693	12.390515
13.085769	912.251272	12.395533
12.917401	926.078942	12.400551
13.124674	932.451846	12.405568
13.184125	953.038751	12.410586
12.744971	946.467316	12.415603
12.984025	935.929034	12.420621
12.875742	949.251915	12.425639
13.106936	942.335241	12.430656
13.037655	952.034114	12.435674
12.982950	946.978871	12.440691
13.144632	948.472543	12.445709
12.974682	962.783163	12.450727
13.151233	952.585913	12.455744
13.329506	953.169005	12.460762
13.171678	957.719781	12.465779
13.192399	950.915116	12.470797
13.168794	953.890192	12.475815
13.174943	951.312557	12.480832
13.102612	960.531253	12.485850
13.295990	978.076068	12.490867
13.687120	982.586738	12.495885
13.276002	973.063531	12.500903
13.855411	974.749049	12.505920
13.508899	958.510325	12.510938
13.328988	956.991798	12.515955
13.634804	950.818243	12.520973
13.351891	958.081738	12.525991
13.510613	948.121685	12.531008
13.275766	948.866486	12.536026
13.538333	952.434305	12.541043
13.572169	952.218121	12.546061
13.415621	947.815540	12.551079
13.269862	947.150770	12.556096
13.222003	956.268958	12.561114
13.201333	970.099374	12.566131
13.398471	972.383600	12.571149
13.344221	985.447970	12.576167
13.648272	976.849209	12.581184
13.530726	980.296912	12.586202
13.490416	983.398770	12.591219
13.528984	977.286779	12.596237
13.376942	981.997621	12.601255
13.587216	977.450043	12.606272
13.568589	977.663394	12.611290
13.263320	984.689669	12.616307
13.538863	976.885752	12.621325
13.725196	980.559110	12.626343
13.620004	978.360521	12.631360
13.806270	976.078240	12.636378
13.485804	975.208942	12.641395
14.000223	970.482664	12.646413
13.639327	989.108992	12.651431
13.831030	982.095301	12.656448
14.058453	986.313014	12.661466
13.931411	985.023122	12.666483
14.006828	982.692662	12.671501
13.623562	974.004964	12.676519
13.802220	971.136961	12.681536
13.955781	973.777600	12.686554
13.725367	981.513494	12.691571
13.916312	972.779533	12.696589
13.768006	975.972891	12.701607
13.449388	979.634984	12.706624
13.842858	975.818850	12.711642
13.829341	982.953894	12.716659
13.910752	975.049846	12.721677
13.550968	989.759625	12.726695
13.842172	1000.944835	12.731712
14.412167	1003.187404	12.736730
13.814440	1000.971553	12.741747
14.118703	1001.934949	12.746765
14.176369	1002.910045	12.751783
13.806115	1001.922617	12.756800
14.223473	1000.168579	12.761818
14.028596	989.763922	12.766835
14.062493	977.022275	12.771853
14.063200	982.051510	12.776871
14.225573	1001.945482	12.781888
13.953949	983.178294	12.786906
13.928991	983.101368	12.791923
14.432893	997.501219	12.796941
14.199983	988.614608	12.801959
14.038957	979.838141	12.806976
14.139189	975.933167	12.811994
13.816840	987.798285	12.817011
14.158360	989.692873	12.822029
14.216625	1000.918230	12.827047
14.153777	1007.564623	12.832064
14.612776	1002.013688	12.837082
14.048451	1011.987869	12.842099
14.537402	1003.454142	12.847117
14.411329	1006.750907	12.852135
14.188746	991.144358	12.857152
14.532091	975.609856	12.862170
14.262138	982.681460	12.867187
13.983457	975.562991	12.872205
14.121803	979.260435	12.877223
14.656763	996.016459	12.882240
14.562009	1001.271735	12.887258
13.838773	1003.048156	12.892275
14.545897	1004.096019	12.897293
14.614960	1005.336147	12.902311
14.273750	998.915787	12.907328
14.412099	995.595418	12.912346
14.311344	1000.062350	12.917363
14.471900	1001.988873	12.922381
14.423154	1005.757459	12.927399
14.385963	1012.101194	12.932416
14.672190	1007.557565	12.937434
13.950944	1018.750205	12.942451
14.473527	1013.134409	12.947469
14.253270	1009.622639	12.952487
14.212233	1009.999931	12.957504
14.588584	1005.663812	12.962522
14.487813	1008.879619	12.967539
14.425852	1010.993770	12.972557
14.210387	1003.409720	12.977575
14.114376	1010.251756	12.982592
14.385533	1005.588581	12.987610
14.855325	1027.041064	12.992627
15.033281	1031.614605	12.997645
14.737370	1025.414678	13.002663
14.472189	1013.779568	13.007680
14.870292	1013.149145	13.012698
14.577049	1014.701617	13.017715
14.981526	1019.715579	13.022733
15.018925	1005.493861	13.027751
14.799113	1007.046378	13.032768
14.849261	993.272936	13.037786
14.480795	994.355992	13.042803
14.584456	994.501065	13.047821
14.966238	998.833374	13.052839
14.783816	1011.636324	13.057856
14.960546	995.112897	13.062874
14.665979	1002.498022	13.067891
14.831877	1007.170399	13.072909
15.283012	1010.030657	13.077927
14.936715	1003.663892	13.082944
15.350166	991.893594	13.087962
15.050500	996.801712	13.092979
15.061802	991.517818	13.097997
15.112765	997.230046	13.103015
14.949353	993.981690	13.108032
15.367746	990.663768	13.113050
15.136438	990.824151	13.118067
15.341432	993.003933	13.123085
15.603736	988.367819	13.128103
15.014997	985.597749	13.133120
15.086829	975.948510	13.138138
14.865013	993.288483	13.143155
15.032610	985.502436	13.148173
15.247039	989.008552	13.153191
14.930628	996.016205	13.158208
15.198663	988.115893	13.163226
14.972251	989.466359	13.168243
15.280562	987.804785	13.173261
14.894089	978.552679	13.178279
14.989874	996.051867	13.183296
14.913489	984.633539	13.188314
14.827046	992.599132	13.193331
14.892048	999.993612	13.198349
15.139856	993.091487	13.203367
15.083009	988.094851	13.208384
15.295912	977.334502	13.213402
15.105518	988.507721	13.218419
14.846842	975.622403	13.223437
15.002767	982.653015	13.228455
15.002811	1006.221749	13.233472
15.353037	1016.605891	13.238490
15.157615	1019.776746	13.243507
15.310488	1013.261183	13.248525
15.381591	1011.729826	13.253543
15.178817	1029.227309	13.258560
15.157677	1014.440496	13.263578
15.147817	1025.917298	13.268595
15.553301	1027.175341	13.273613
15.688979	1020.254370	13.278631
15.336106	1031.182093	13.283648
15.539949	1012.471568	13.288666
15.362074	1025.716671	13.293683
15.157396	1022.190115	13.298701
15.727103	1015.950397	13.303719
15.296121	1016.432808	13.308736
15.768063	1015.504342	13.313754
15.644322	1013.672584	13.318771
15.340315	1023.883578	13.323789
15.791452	1019.091782	13.328807
15.291724	1022.679153	13.333824
15.678051	1015.983206	13.338842
15.493176	1023.256874	13.343859
15.497975	1024.637560	13.348877
15.439404	1020.338022	13.353895
15.505457	1020.403499	13.358912
15.557063	1017.810058	13.363930
15.397095	1035.163851	13.368947
15.787862	1046.288516	13.373965
16.290759	1047.873724	13.378983
15.742285	1043.704509	13.384000
15.871379	1009.142418	13.389018
15.628596	1024.774944	13.394035
15.785468	1030.053128	13.399053
15.988058	1037.471299	13.404071
15.577171	1024.721376	13.409088
16.038055	1028.752418	13.414106
15.938826	1027.398864	13.419123
16.018464	1019.312810	13.424141
16.117088	1007.963514	13.429159
15.983244	1016.976690	13.434176
16.167308	1017.398595	13.439194
15.686751	1016.164481	13.444211
15.674449	1012.532059	13.449229
16.178951	1013.278449	13.454247
16.080496	1013.940828	13.459264
15.956676	1010.954012	13.464282
15.834513	1014.063131	13.469299
15.638585	1015.448708	13.474317
16.107019	1012.823254	13.479335
16.010692	1014.086831	13.484352
15.841919	1035.536406	13.489370
16.149212	1045.302504	13.494387
16.051793	1053.640404	13.499405
16.118485	1052.736128	13.504423
16.209287	1050.688926	13.509440
16.240648	1052.628581	13.514458
16.341571	1039.709649	13.519475
16.074489	1023.298655	13.524493
16.224106	1019.805556	13.529511
15.940709	1021.420569	13.534528
15.956377	1027.054404	13.539546
16.455169	1035.496319	13.544563
16.230739	1049.781395	13.549581
16.678657	1042.220153	13.554599
16.336737	1030.810328	13.559616
15.851793	1019.964329	13.564634
16.175472	1031.045369	13.569651
16.173383	1042.224846	13.574669
16.255778	1046.538635	13.579687
16.269297	1052.558253	13.584704
16.330258	1047.268479	13.589722
16.280018	1047.561866	13.594739
16.111179	1061.458629	13.599757
16.411686	1045.165825	13.604775
16.207346	1045.907547	13.609792
16.370683	1049.997706	13.614810
16.416960	1060.260560	13.619827
16.335909	1053.043585	13.624845
16.697657	1045.975331	13.629863
16.445998	1042.856533	13.634880
16.538289	1043.972744	13.639898
16.235961	1050.360396	13.644915
16.445780	1055.115275	13.649933
16.576162	1048.886088	13.654951
16.302778	1057.963730	13.659968
16.231376	1056.209911	13.664986
16.340128	1059.163091	13.670003
16.368357	1070.311978	13.675021
16.813255	1080.716314	13.680039
16.635052	1087.123584	13.685056
17.008075	1084.650920	13.690074
17.131956	1085.721746	13.695091
16.678510	1059.665545	13.700109
16.416925	1045.446055	13.705127
16.662452	1065.912538	13.710144
16.946574	1075.085665	13.715162
16.988367	1070.465174	13.720179
16.522667	1063.612268	13.725197
16.957785	1071.302176	13.730215
16.845116	1067.996192	13.735232
17.051855	1060.840217	13.740250
17.003790	1058.794749	13.745267
16.700483	1044.030221	13.750285
16.561967	1043.544555	13.755303
16.704516	1053.948545	13.760320
16.660908	1060.450836	13.765338
16.996070	1073.581503	13.770355
16.576221	1073.768382	13.775373
16.972081	1072.080492	13.780391
16.819124	1072.434587	13.785408
16.906970	1080.285542	13.790426
17.239792	1071.140253	13.795443
17.221902	1076.292672	13.800461
17.187106	1079.007824	13.805479
17.088846	1087.343913	13.810496
16.986300	1079.857659	13.815514
17.271779	1071.352469	13.820531
16.922088	1077.454285	13.825549
16.895589	1072.698257	13.830567
17.300661	1074.268171	13.835584
17.248686	1073.046154	13.840602
17.293403	1079.615321	13.845619
16.858720	1086.337491	13.850637
17.188100	1073.801159	13.855655
17.191009	1076.131734	13.860672
17.026454	1076.842461	13.865690
17.416517	1060.349386	13.870707
17.186064	1077.381446	13.875725
17.020241	1074.274805	13.880743
17.370550	1072.745240	13.885760
17.223338	1077.146267	13.890778
17.460461	1068.905769	13.895795
17.169251	1075.979361	13.900813
17.259070	1074.465764	13.905831
16.984479	1072.618427	13.910848
16.905849	1077.670673	13.915866
17.335843	1072.722919	13.920883
17.225187	1080.711857	13.925901
17.580290	1077.339045	13.930919
17.431807	1089.403001	13.935936
17.128943	1097.875333	13.940954
17.896302	1089.927327	13.945971
17.381390	1101.209084	13.950989
17.762321	1090.583427	13.956007
17.369949	1082.927454	13.961024
17.171820	1096.572021	13.966042
17.656798	1088.969975	13.971059
17.980521	1092.656830	13.976077
17.873857	1089.496298	13.981095
17.622053	1083.407543	13.986112
17.668635	1079.181912	13.991130
17.245834	1067.900408	13.996147
17.124116	1083.724356	14.001165
17.446160	1078.476770	14.006183
17.830892	1089.189488	14.011200
17.930901	1089.132812	14.016218
17.759322	1084.226006	14.021235
17.166478	1092.445968	14.026253
17.324519	1084.477209	14.031271
17.515890	1085.943538	14.036288
17.744305	1095.679425	14.041306
17.922771	1086.095135	14.046323
18.091487	1092.239852	14.051341
17.807912	1087.425209	14.056359
17.876292	1092.891291	14.061376
17.841972	1096.159890	14.066394
17.963910	1084.874391	14.071411
17.765342	1092.168863	14.076429
17.770625	1093.772301	14.081447
17.740021	1093.962048	14.086464
17.763555	1113.818919	14.091482
18.235988	1115.025333	14.096499
18.392832	1119.712629	14.101517
18.615544	1101.429566	14.106535
18.347969	1087.992103	14.111552
18.168585	1092.998441	14.116570
18.304838	1079.788990	14.121587
18.292150	1086.942448	14.126605
18.374764	1090.925910	14.131623
18.295255	1086.790050	14.136640
18.078370	1086.451213	14.141658
18.019442	1083.966611	14.146675
17.936007	1083.547017	14.151693
17.755558	1083.791889	14.156711
18.232562	1088.911578	14.161728
18.136278	1081.181382	14.166746
18.331109	1079.957865	14.171763
18.076696	1079.733112	14.176781
18.086429	1079.694927	14.181799
18.462170	1079.804398	14.186816
18.094213	1089.986261	14.191834
18.230533	1082.414393	14.196851
18.213356	1085.849831	14.201869
18.182837	1085.271086	14.206887
18.102714	1088.440579	14.211904
18.089463	1106.330768	14.216922
18.223905	1103.835010	14.221939
18.419836	1118.158808	14.226957
18.528714	1123.155217	14.231975
18.820490	1114.677701	14.236992
18.459667	1115.006375	14.242010
18.398279	1111.786768	14.247027
18.549166	1120.398932	14.252045
18.262177	1116.611583	14.257063
18.480154	1104.864513	14.262080
18.351196	1121.454238	14.267098
18.430269	1113.269414	14.272115
18.171085	1123.781308	14.277133
18.755126	1117.516738	14.282151
18.815490	1116.000928	14.287168
18.682353	1119.476045	14.292186
18.658727	1112.599522	14.297203
18.625075	1111.987045	14.302221
18.479298	1116.122893	14.307239
18.601075	1112.413918	14.312256
18.763648	1114.796799	14.317274
18.853450	1114.903618	14.322291
18.727514	1116.076046	14.327309
19.016145	1112.365033	14.332327
19.109700	1113.480251	14.337344
18.711290	1120.706255	14.342362
18.667682	1109.675307	14.347379
18.926043	1116.122109	14.352397
18.629556	1111.104092	14.357415
19.105845	1114.123586	14.362432
18.949496	1114.512494	14.367450
19.164339	1112.935280	14.372467
19.141113	1116.608725	14.377485
18.653064	1126.394764	14.382503
18.972078	1112.353869	14.387520
18.929458	1116.082886	14.392538
19.043569	1116.976599	14.397555
18.791632	1118.419095	14.402573
18.799031	1133.712282	14.407591
18.882085	1138.305112	14.412608
19.207676	1147.454881	14.417626
19.648511	1136.609044	14.422643
19.354212	1131.780809	14.427661
18.902525	1138.117641	14.432679
19.274279	1138.531306	14.437696
19.356294	1137.048521	14.442714
19.479111	1133.995646	14.447731
19.828239	1115.772734	14.452749
19.101940	1113.548628	14.457767
19.116739	1105.833883	14.462784
18.993485	1109.000286	14.467802
19.111268	1105.923054	14.472819
19.385100	1121.447694	14.477837
19.315294	1128.750782	14.482855
19.517148	1132.507824	14.487872
19.448209	1127.338742	14.492890
19.288066	1122.955209	14.497907
19.547031	1117.330666	14.502925
19.414998	1129.652157	14.507943
19.512633	1119.803681	14.512960
19.515422	1110.840571	14.517978
19.239623	1119.426146	14.522995
19.552538	1131.523574	14.528013
19.601826	1141.051362	14.533031
19.640642	1135.204219	14.538048
19.859922	1134.237272	14.543066
19.388783	1126.689197	14.548083
19.347803	1119.962783	14.553101
19.482678	1130.202353	14.558119
19.459905	1139.884587	14.563136
19.725790	1140.990563	14.568154
19.549297	1130.774492	14.573171
19.577028	1133.753700	14.578189
19.469527	1143.335797	14.583207
19.594606	1131.437166	14.588224
19.382359	1141.921222	14.593242
19.736324	1144.423199	14.598259
19.462781	1133.012211	14.603277
19.571264	1135.100912	14.608295
19.909754	1131.084010	14.613312
19.677840	1143.311818	14.618330
19.265162	1138.043354	14.623347
19.864924	1151.958595	14.628365
19.724601	1166.640469	14.633383
20.141492	1165.934490	14.638400
20.168102	1162.322361	14.643418
20.153710	1173.970097	14.648435
20.013604	1169.513157	14.653453
19.938152	1168.473360	14.658471
20.381049	1166.939872	14.663488
20.200403	1151.858483	14.668506
20.169404	1143.399358	14.673523
20.382232	1126.706040	14.678541
19.999016	1127.804145	14.683559
20.201924	1113.706492	14.688576
20.431941	1123.252767	14.693594
20.237206	1115.808138	14.698611
20.062095	1123.582975	14.703629
19.905950	1126.530032	14.708647
20.089744	1118.760134	14.713664
20.142418	1116.782227	14.718682
20.011568	1131.773512	14.723699
20.293189	1142.194296	14.728717
20.206176	1154.845350	14.733735
20.891814	1151.187483	14.738752
20.387706	1147.997870	14.743770
20.464748	1139.704710	14.748787
20.249733	1122.499975	14.753805
20.050654	1127.695405	14.758823
20.221974	1136.274275	14.763840
20.415900	1151.090152	14.768858
20.649840	1156.924105	14.773875
20.875667	1152.096745	14.778893
20.386338	1143.729653	14.783911
20.544038	1121.299985	14.788928
20.543424	1132.157246	14.793946
20.614142	1126.751266	14.798963
20.360666	1124.782714	14.803981
20.339013	1136.913105	14.808999
20.303158	1151.113114	14.814016
20.597890	1159.202285	14.819034
20.382727	1154.018036	14.824051
20.693540	1149.538011	14.829069
20.300986	1166.059230	14.834087
20.442011	1164.748950	14.839104
20.380654	1156.062175	14.844122
20.440019	1153.191845	14.849139
20.640965	1152.269663	14.854157
20.617612	1164.743653	14.859175
21.080298	1151.400565	14.864192
20.845399	1155.716137	14.869210
20.492758	1159.581536	14.874227
20.680609	1162.241725	14.879245
20.631589	1177.580518	14.884263
20.819731	1188.406957	14.889280
20.757560	1192.428985	14.894298
20.794385	1185.773909	14.899315
21.282361	1184.804198	14.904333
21.085748	1182.116795	14.909351
20.977821	1181.822904	14.914368
21.021651	1178.262249	14.919386
20.969090	1191.952085	14.924403
20.986735	1172.913546	14.929421
21.046060	1186.999799	14.934439
20.738669	1178.731299	14.939456
20.971328	1174.392943	14.944474
20.615491	1180.549359	14.949491
21.133726	1166.567550	14.954509
20.997119	1173.066391	14.959527
21.397795	1176.848788	14.964544
21.270651	1174.428616	14.969562
21.263640	1179.358409	14.974579
21.605330	1179.424308	14.979597
20.981377	1178.010779	14.984615
20.950406	1179.074184	14.989632
21.203046	1172.834939	14.994650
21.272629	1170.422348	14.999667
21.152887	1174.003131	15.004685
20.854482	1198.982164	15.009703
20.995213	1204.814247	15.014720
21.431830	1203.236128	15.019738
21.339288	1208.005294	15.024755
21.982721	1208.685778	15.029773
21.962736	1205.216390	15.034791
21.730142	1203.168388	15.039808
21.959766	1198.010473	15.044826
21.566043	1185.373319	15.049843
21.716849	1181.997305	15.054861
21.732504	1176.174454	15.059879
21.814030	1175.433457	15.064896
21.705335	1164.508127	15.069914
21.153965	1178.090393	15.074931
21.219566	1175.335558	15.079949
21.711526	1190.008819	15.084967
21.703560	1206.267193	15.089984
22.128688	1209.985316	15.095002
21.690497	1194.905586	15.100019
21.556754	1180.806137	15.105037
21.752539	1194.082030	15.110055
21.773247	1201.326071	15.115072
21.819562	1202.925482	15.120090
21.705000	1203.758642	15.125107
21.885061	1198.138868	15.130125
22.026590	1200.213051	15.135143
21.946523	1200.424768	15.140160
21.934453	1196.760769	15.145178
21.842784	1203.393516	15.150195
22.098691	1194.756151	15.155213
22.001261	1203.424045	15.160231
22.040299	1189.908166	15.165248
22.467919	1194.952212	15.170266
21.931093	1202.754700	15.175283
22.090033	1197.575419	15.180301
22.231364	1199.630737	15.185319
22.015719	1206.649357	15.190336
22.531167	1192.434530	15.195354
22.079609	1194.099845	15.200371
22.394776	1182.070489	15.205389
22.216579	1163.592721	15.210407
22.177212	1168.131817	15.215424
22.043975	1155.495648	15.220442
22.099820	1178.681007	15.225459
22.227383	1181.831878	15.230477
22.361791	1202.346074	15.235495
22.441957	1194.739750	15.240512
22.512683	1190.915984	15.245530
22.001721	1206.393497	15.250547
22.176793	1197.174651	15.255565
21.900727	1195.319276	15.260583
22.070621	1197.135226	15.265600
22.103774	1193.492479	15.270618
21.841215	1194.444235	15.275635
22.519680	1206.127267	15.280653
22.423672	1209.770661	15.285671
22.232215	1231.150248	15.290688
22.337571	1223.633830	15.295706
22.259756	1226.809662	15.300723
22.699019	1225.372831	15.305741
22.605068	1231.638261	15.310759
22.202394	1217.257333	15.315776
22.632840	1216.427064	15.320794
22.339622	1223.342398	15.325811
22.755136	1215.805729	15.330829
22.629725	1217.772938	15.335847
22.492559	1221.290870	15.340864
22.936627	1223.412596	15.345882
22.624353	1227.000469	15.350899
23.084307	1237.891382	15.355917
23.184899	1232.492229	15.360935
22.951474	1227.873957	15.365952
23.464866	1211.039050	15.370970
23.013071	1210.191090	15.375987
23.086375	1230.515841	15.381005
23.210817	1219.904221	15.386023
22.781704	1221.671725	15.391040
23.207184	1215.614862	15.396058
22.974351	1215.518812	15.401075
23.148487	1219.836356	15.406093
23.314959	1216.637264	15.411111
22.999743	1218.942586	15.416128
23.551604	1217.465852	15.421146
23.010761	1220.508908	15.426163
22.942549	1213.918061	15.431181
22.845063	1217.249900	15.436199
22.914046	1210.009189	15.441216
23.436143	1212.184133	15.446234
22.870976	1220.201947	15.451251
23.100933	1210.078360	15.456269
23.171391	1209.849023	15.461287
22.957627	1219.118062	15.466304
23.618412	1229.859970	15.471322
23.555800	1241.243308	15.476339
23.696997	1231.070233	15.481357
23.652763	1211.738751	15.486375
23.350482	1214.849782	15.491392
23.477750	1206.014821	15.496410
23.319392	1209.760662	15.501427
23.226882	1205.870617	15.506445
23.246715	1212.209716	15.511463
23.702311	1227.792159	15.516480
23.862767	1226.694399	15.521498
23.502536	1230.574064	15.526515
23.540610	1218.200809	15.531533
23.478776	1228.406088	15.536551
23.514160	1234.772541	15.541568
23.776379	1238.573549	15.546586
23.997038	1241.583430	15.551603
23.820188	1228.713091	15.556621
23.977200	1210.518729	15.561639
23.631606	1214.536119	15.566656
23.654904	1195.539529	15.571674
23.754639	1210.248622	15.576691
23.748335	1229.090138	15.581709
23.778474	1235.753909	15.586727
23.514296	1245.848219	15.591744
24.120244	1236.068253	15.596762
23.828327	1243.559350	15.601779
24.101195	1234.732152	15.606797
24.119405	1235.241761	15.611815
23.742604	1247.329079	15.616832
24.051101	1236.802323	15.621850
24.062912	1241.267220	15.626867
23.984261	1234.871001	15.631885
24.318884	1224.291896	15.636903
24.132954	1233.149653	15.641920
24.472386	1235.370201	15.646938
24.450407	1240.660750	15.651955
24.260253	1235.833347	15.656973
24.442708	1223.085010	15.661991
24.421475	1219.593778	15.667008
24.177959	1197.425704	15.672026
24.422782	1203.355902	15.677043
23.881307	1200.019319	15.682061
24.238340	1211.596528	15.687079
24.142665	1233.862596	15.692096
24.180628	1237.279095	15.697114
24.492536	1238.483755	15.702131
24.513589	1231.495452	15.707149
24.621417	1227.249404	15.712167
24.508644	1234.295096	15.717184
24.611608	1225.941300	15.722202
23.877860	1225.407341	15.727219
24.145999	1231.397073	15.732237
24.297446	1231.198024	15.737255
24.323392	1241.027369	15.742272
24.252889	1230.573215	15.747290
24.196209	1232.649514	15.752307
24.632063	1237.022149	15.757325
24.948360	1248.793134	15.762343
24.759742	1261.403620	15.767360
25.195305	1252.192001	15.772378
24.821310	1242.169972	15.777395
24.768242	1231.760567	15.782413
24.577900	1228.492998	15.787431
24.410604	1232.071039	15.792448
24.799175	1240.816351	15.797466
25.069234	1259.520413	15.802483
24.975754	1259.331999	15.807501
24.837991	1260.563875	15.812519
24.599864	1261.791898	15.817536
24.632897	1251.318224	15.822554
24.684572	1255.637552	15.827571
24.985771	1250.432729	15.832589
25.228599	1245.360405	15.837607
24.783259	1247.477046	15.842624
24.961768	1253.777684	15.847642
25.203607	1250.203910	15.852659
25.117825	1249.189833	15.857677
25.569135	1244.814072	15.862695
25.413910	1250.503844	15.867712
25.356229	1245.170263	15.872730
25.829529	1239.039726	15.877747
25.285726	1248.150445	15.882765
25.403712	1247.003811	15.887783
25.120545	1249.522723	15.892800
25.355008	1252.661419	15.897818
25.629707	1244.571689	15.902835
25.024502	1240.553935	15.907853
25.353358	1242.541989	15.912871
25.486688	1248.115872	15.917888
25.424456	1242.345655	15.922906
25.130142	1244.537680	15.927923
25.005147	1246.508367	15.932941
25.455503	1240.707211	15.937959
25.521349	1248.424890	15.942976
25.613129	1249.046331	15.947994
25.376303	1235.229642	15.953011
25.322489	1248.585886	15.958029
25.338199	1251.924972	15.963047
25.308730	1252.305867	15.968064
25.597043	1254.512441	15.973082
25.758921	1269.434917	15.978099
25.589382	1281.510383	15.983117
26.141508	1274.544359	15.988135
26.105253	1260.975532	15.993152
26.085893	1252.734100	15.998170
26.029035	1245.196501	16.003187
25.414175	1241.777574	16.008205
25.678748	1233.726533	16.013223
25.415927	1245.588683	16.018240
25.683734	1264.837599	16.023258
25.953173	1258.978206	16.028275
26.010502	1270.991690	16.033293
26.052673	1269.309196	16.038311
26.029824	1274.322742	16.043328
25.724837	1267.818715	16.048346
25.928475	1271.116845	16.053363
25.685725	1272.969635	16.058381
26.040683	1267.930705	16.063399
26.132356	1274.134708	16.068416
25.877167	1272.199884	16.073434
26.311520	1273.114199	16.078451
26.141902	1278.294959	16.083469
26.354370	1283.198286	16.088487
26.391125	1279.519490	16.093504
26.510349	1274.586124	16.098522
26.743722	1261.207686	16.103539
26.237318	1266.571369	16.108557
26.467375	1257.578417	16.113575
26.587444	1255.191311	16.118592
26.514866	1262.862628	16.123610
26.966455	1252.329884	16.128627
26.441743	1257.377313	16.133645
26.546434	1253.104612	16.138663
26.548107	1252.525649	16.143680
26.288648	1257.377979	16.148698
26.543815	1252.742181	16.153715
26.397858	1266.705810	16.158733
26.529848	1255.183095	16.163751
26.511757	1260.639539	16.168768
26.601503	1273.908256	16.173786
26.753945	1275.711751	16.178803
26.864393	1282.801998	16.183821
26.973932	1289.354222	16.188839
26.838031	1273.734608	16.193856
26.689983	1272.057233	16.198874
26.762458	1264.947412	16.203891
26.843547	1283.045013	16.208909
26.950563	1284.813512	16.213927
27.091181	1287.316588	16.218944
26.838509	1287.941917	16.223962
27.322995	1280.170573	16.228979
27.001748	1277.893938	16.233997
26.950692	1266.666085	16.239015
26.859966	1260.708852	16.244032
26.842049	1279.292910	16.249050
27.128423	1285.078861	16.254067
27.180530	1280.774702	16.259085
27.102853	1285.652058	16.264103
27.089074	1288.720058	16.269120
27.166873	1276.732295	16.274138
27.337530	1278.037511	16.279155
27.011629	1288.551508	16.284173
27.124266	1285.948704	16.289191
27.074032	1288.140083	16.294208
27.232165	1288.335193	16.299226
27.473319	1287.717757	16.304243
26.974073	1293.072784	16.309261
27.109714	1286.857591	16.314279
27.074226	1288.067416	16.319296
27.262286	1309.870480	16.324314
27.768466	1307.807221	16.329331
27.679787	1317.876062	16.334349
27.514221	1304.800251	16.339367
27.496952	1309.331400	16.344384
27.675222	1314.724247	16.349402
28.072257	1312.250722	16.354419
27.658304	1297.086564	16.359437
27.519789	1274.587614	16.364455
27.861074	1289.952440	16.369472
27.588037	1291.143333	16.374490
28.077542	1296.494876	16.379507
27.388925	1305.029225	16.384525
27.833334	1306.654067	16.389543
27.914016	1304.965193	16.394560
27.790733	1316.135015	16.399578
27.902344	1308.073044	16.404595
27.745409	1309.018340	16.409613
28.089737	1312.440032	16.414631
27.900529	1321.795222	16.419648
27.789875	1310.004382	16.424666
27.835854	1304.784717	16.429683
27.948551	1309.741973	16.434701
28.103974	1320.740061	16.439719
28.239318	1307.005775	16.444736
27.829023	1309.253626	16.449754
28.102397	1307.321827	16.454771
28.245186	1307.811992	16.459789
27.927607	1307.307936	16.464807
28.355990	1302.611947	16.469824
27.905459	1310.667516	16.474842
28.107566	1304.173600	16.479859
28.426736	1326.905352	16.484877
28.341522	1323.753030	16.489895
28.429622	1330.591493	16.494912
28.279668	1339.450440	16.499930
28.676675	1337.659973	16.504947
28.674750	1328.823893	16.509965
28.526678	1327.818550	16.514983
28.960694	1325.747159	16.520000
28.451135	1324.085151	16.525018
28.915219	1305.468186	16.530035
28.504520	1302.586294	16.535053
28.360819	1298.464156	16.540071
28.656908	1310.576716	16.545088
28.605170	1311.859311	16.550106
28.798285	1321.541738	16.555123
28.656122	1329.435630	16.560141
28.405834	1326.763781	16.565159
28.664507	1325.427709	16.570176
28.507709	1333.816929	16.575194
28.840002	1324.868819	16.580211
28.810882	1326.631125	16.585229
28.688403	1329.249817	16.590247
28.751163	1320.920737	16.595264
28.438255	1326.410666	16.600282
28.327148	1324.551582	16.605299
28.288885	1350.050371	16.610317
28.896095	1351.455352	16.615335
28.863955	1358.431451	16.620352
28.926009	1354.679552	16.625370
29.237331	1351.365899	16.630387
29.260949	1359.939822	16.635405
29.551234	1357.575697	16.640423
29.693123	1355.286536	16.645440
29.612863	1361.206450	16.650458
29.798391	1345.404409	16.655475
29.736856	1352.920402	16.660493
29.295378	1335.778124	16.665511
29.787809	1318.530045	16.670528
29.344524	1317.833028	16.675546
29.164154	1309.330436	16.680563
29.567504	1325.032257	16.685581
29.511515	1331.797730	16.690599
29.652611	1312.538976	16.695616
29.279338	1324.682855	16.700634
29.724746	1335.641599	16.705651
29.516022	1337.261602	16.710669
29.558598	1345.168612	16.715687
29.954805	1356.072527	16.720704
29.700273	1349.943173	16.725722
29.748774	1348.554105	16.730739
29.183475	1339.523907	16.735757
29.329350	1351.920422	16.740775
29.804573	1339.703422	16.745792
29.818292	1346.059729	16.750810
30.001346	1341.976781	16.755827
29.890092	1352.772597	16.760845
29.800343	1343.420351	16.765863
30.037254	1344.772081	16.770880
29.857255	1347.821947	16.775898
29.991646	1350.518187	16.780915
30.090588	1345.075568	16.785933
29.956291	1345.194693	16.790951
30.400399	1343.140133	16.795968
29.867398	1349.253510	16.800986
29.873230	1338.229960	16.806003
29.883500	1341.205013	16.811021
30.015950	1346.523177	16.816039
29.946133	1347.459562	16.821056
30.128647	1377.032786	16.826074
30.420456	1375.230601	16.831091
30.417809	1371.314611	16.836109
30.394162	1375.624397	16.841127
30.557408	1369.673100	16.846144
30.591192	1372.727728	16.851162
29.969152	1376.655503	16.856179
30.430805	1368.423338	16.861197
30.157205	1379.390146	16.866215
30.501713	1374.256456	16.871232
30.543562	1373.701151	16.876250
30.599262	1377.663947	16.881267
30.358606	1371.232686	16.886285
30.424226	1379.295738	16.891303
30.557906	1374.143415	16.896320
30.298729	1377.921345	16.901338
30.263181	1378.264273	16.906355
30.700203	1392.368488	16.911373
30.799762	1406.394737	16.916391
31.288954	1397.568635	16.921408
30.759726	1383.295513	16.926426
30.415945	1389.645286	16.931443
30.889399	1400.837225	16.936461
30.552377	1404.598130	16.941479
31.055854	1398.994810	16.946496
31.088940	1410.759665	16.951514
31.060588	1402.749559	16.956531
31.129038	1404.292966	16.961549
30.837882	1405.191989	16.966567
30.985044	1399.061063	16.971584
30.977468	1407.715374	16.976602
30.840550	1407.340059	16.981619
31.232492	1396.972998	16.986637
30.812741	1397.914967	16.991655
30.918376	1398.590812	16.996672
30.937031	1408.310055	17.001690
31.248233	1419.847765	17.006707
31.518337	1421.284950	17.011725
31.691938	1420.367675	17.016743
31.953948	1412.070120	17.021760
31.820660	1407.469070	17.026778
31.662539	1393.946682	17.031795
31.814782	1390.639677	17.036813
31.771552	1389.868934	17.041831
31.639554	1384.270843	17.046848
31.493636	1389.560706	17.051866
31.602864	1392.126870	17.056883
31.712146	1383.770762	17.061901
31.676648	1388.182906	17.066919
31.807169	1382.716542	17.071936
31.834519	1386.913952	17.076954
31.822908	1386.059235	17.081971
32.088927	1381.888918	17.086989
31.598396	1386.453570	17.092007
31.917930	1378.674452	17.097024
31.875714	1385.931361	17.102042
31.993016	1382.003381	17.107059
32.036167	1382.343908	17.112077
31.850931	1392.369731	17.117095
32.118771	1378.109121	17.122112
32.076308	1389.885288	17.127130
31.965144	1386.196314	17.132147
32.186917	1385.621059	17.137165
31.964885	1399.749369	17.142183
32.409686	1405.898891	17.147200
32.117454	1403.961916	17.152218
32.282887	1405.539263	17.157235
32.327773	1399.426453	17.162253
32.121121	1414.480562	17.167271
32.171729	1406.074316	17.172288
32.446928	1409.357478	17.177306
32.475623	1408.008298	17.182323
32.952175	1405.269628	17.187341
32.640358	1416.107359	17.192359
32.393492	1409.516876	17.197376
32.156532	1411.192741	17.202394
32.196358	1412.745612	17.207411
32.711592	1398.899918	17.212429
31.893787	1407.707284	17.217447
32.569318	1406.045099	17.222464
32.794032	1407.072482	17.227482
32.544471	1410.303560	17.232499
32.713025	1402.050618	17.237517
32.644469	1410.002046	17.242535
32.488976	1398.235493	17.247552
32.717295	1418.987967	17.252570
32.795589	1436.861805	17.257587
32.918320	1425.983796	17.262605
32.701753	1434.698316	17.267623
32.803998	1431.905873	17.272640
32.957982	1428.511171	17.277658
32.957034	1439.237996	17.282675
32.920721	1421.929322	17.287693
32.755450	1429.440876	17.292711
32.881791	1426.484209	17.297728
33.071847	1427.737801	17.302746
32.782859	1430.767147	17.307763
32.851406	1435.989231	17.312781
32.944909	1452.181063	17.317799
33.409549	1453.782100	17.322816
33.335865	1455.793529	17.327834
33.405124	1454.198655	17.332851
33.633446	1444.660613	17.337869
33.556888	1446.562675	17.342887
33.656633	1438.630552	17.347904
33.896776	1442.107713	17.352922
33.619399	1450.816958	17.357939
33.919316	1441.202103	17.362957
33.887946	1443.503764	17.367975
33.732945	1427.801725	17.372992
33.820788	1412.715386	17.378010
33.590361	1407.996564	17.383027
33.709720	1408.603996	17.388045
33.450294	1427.737269	17.393063
33.776191	1431.364792	17.398080
34.348761	1427.257482	17.403098
33.672928	1434.239018	17.408115
34.220388	1420.352930	17.413133
33.991610	1419.829835	17.418151
33.749631	1416.351882	17.423168
33.892974	1424.937907	17.428186
33.837512	1439.831576	17.433203
34.275372	1432.593855	17.438221
33.988709	1447.082512	17.443239
34.148469	1441.316407	17.448256
34.435630	1435.089059	17.453274
34.092946	1448.692910	17.458291
34.454617	1435.103317	17.463309
34.397282	1445.499723	17.468327
34.314967	1441.459114	17.473344
34.547324	1438.241981	17.478362
34.404016	1439.256681	17.483379
34.459537	1437.434166	17.488397
34.232051	1440.054516	17.493415
34.054507	1433.639156	17.498432
34.134877	1434.658552	17.503450
34.015114	1436.981541	17.508467
34.427619	1427.033096	17.513485
34.431456	1431.785192	17.518503
34.193439	1431.550236	17.523520
34.512845	1445.652716	17.528538
34.479355	1461.686847	17.533555
34.633065	1463.493698	17.538573
34.631433	1470.474639	17.543591
34.717566	1478.384347	17.548608
35.064425	1468.109348	17.553626
34.859793	1473.403449	17.558643
34.915747	1469.650958	17.563661
35.102072	1457.431702	17.568679
34.854359	1466.465962	17.573696
35.040708	1463.137545	17.578714
34.958099	1471.336605	17.583731
35.410194	1460.708362	17.588749
35.272623	1460.680788	17.593767
34.857111	1466.661765	17.598784
35.182277	1467.255988	17.603802
34.767000	1469.693267	17.608819
35.091903	1461.759677	17.613837
35.080401	1463.608450	17.618855
35.115131	1461.406308	17.623872
35.322518	1461.910191	17.628890
35.266401	1463.447064	17.633907
35.252072	1461.290840	17.638925
35.159433	1462.688486	17.643943
34.935292	1490.845814	17.648960
35.605556	1489.529765	17.653978
35.501379	1495.017474	17.658995
35.548741	1491.211283	17.664013
35.835546	1498.599984	17.669031
35.799879	1497.527199	17.674048
36.054497	1485.772200	17.679066
35.426943	1491.329639	17.684083
35.734909	1491.523172	17.689101
35.642932	1497.975782	17.694119
35.720212	1486.141486	17.699136
35.703344	1490.382466	17.704154
35.404577	1491.961882	17.709171
35.738052	1483.474898	17.714189
35.782501	1491.097817	17.719207
35.796874	1491.681692	17.724224
35.955797	1485.910986	17.729242
35.775432	1493.013262	17.734259
35.476698	1513.035029	17.739277
36.025467	1517.898100	17.744295
36.127309	1519.544256	17.749312
36.491447	1518.802118	17.754330
36.198766	1521.678944	17.759347
36.298528	1513.404263	17.764365
35.962381	1516.780407	17.769383
36.430565	1521.952490	17.774400
36.577963	1515.470695	17.779418
36.285620	1508.908959	17.784435
36.527603	1516.937369	17.789453
36.897429	1508.853798	17.794471
36.367291	1516.336044	17.799488
36.567804	1509.404122	17.804506
36.428803	1518.236160	17.809523
36.809044	1518.283869	17.814541
36.920319	1512.333642	17.819559
36.866391	1516.929975	17.824576
36.887129	1522.855275	17.829594
36.827490	1514.105416	17.834611
36.839026	1512.612613	17.839629
36.866436	1507.792407	17.844647
36.732109	1520.701984	17.849664
36.952813	1509.640766	17.854682
36.850636	1510.184098	17.859699
36.872119	1516.575803	17.864717
36.923176	1513.229227	17.869735
36.757750	1511.085810	17.874752
36.920075	1520.248662	17.879770
37.161413	1534.038167	17.884787
37.074189	1541.257325	17.889805
37.162839	1539.617106	17.894823
37.097200	1538.363456	17.899840
37.226461	1537.364934	17.904858
37.117254	1539.312964	17.909875
37.144194	1541.900652	17.914893
37.155340	1529.839086	17.919911
37.434700	1540.858936	17.924928
37.580596	1540.161594	17.929946
37.363422	1529.063418	17.934963
37.379159	1538.104490	17.939981
37.204216	1542.727561	17.944999
37.174683	1542.245486	17.950016
37.680381	1564.870720	17.955034
37.464943	1567.083192	17.960051
37.658179	1571.497279	17.965069
37.776141	1569.764015	17.970087
38.011989	1562.540392	17.975104
37.986730	1572.798896	17.980122
38.029359	1565.005299	17.985139
37.990862	1557.062148	17.990157
38.174942	1560.683657	17.995175
38.179314	1562.393200	18.000192
38.379162	1554.238933	18.005210
38.151261	1542.813391	18.010227
37.975285	1538.479604	18.015245
38.231295	1522.070442	18.020263
38.126188	1537.892496	18.025280
38.177933	1531.272990	18.030298
37.957822	1539.289736	18.035315
38.222243	1555.411250	18.040333
38.273396	1544.587135	18.045351
38.113854	1551.382055	18.050368
38.377182	1562.464417	18.055386
38.457472	1555.636238	18.060403
38.419721	1551.344127	18.065421
38.649443	1559.462384	18.070439
38.151988	1563.966816	18.075456
38.454313	1556.136129	18.080474
38.346787	1552.986274	18.085491
38.454123	1553.642553	18.090509
38.451259	1550.055686	18.095527
38.077137	1560.905802	18.100544
38.501020	1574.863542	18.105562
38.813801	1579.885393	18.110579
38.638690	1593.689576	18.115597
39.148936	1584.879962	18.120615
38.653449	1587.995104	18.125632
39.016373	1583.360658	18.130650
39.048562	1581.184116	18.135667
38.855008	1585.947289	18.140685
38.903675	1582.077474	18.145703
38.516535	1587.462463	18.150720
38.941836	1590.664511	18.155738
39.413339	1599.427793	18.160755
39.692284	1609.488708	18.165773
39.797341	1593.832416	18.170791
39.176611	1586.476992	18.175808
39.296469	1580.597365	18.180826
39.303561	1573.403346	18.185843
39.038117	1576.772914	18.190861
39.516552	1588.106684	18.195879
39.477058	1607.816358	18.200896
39.609148	1597.750851	18.205914
40.108380	1605.314666	18.210931
39.771785	1599.792105	18.215949
39.615193	1570.550068	18.220967
39.473834	1580.082135	18.225984
39.766551	1582.986058	18.231002
39.804499	1596.315204	18.236019
39.738193	1605.316750	18.241037
40.103364	1591.862267	18.246055
39.984026	1604.056442	18.251072
39.871650	1585.935773	18.256090
39.854862	1592.604712	18.261107
39.936032	1590.821238	18.266125
40.247798	1603.125527	18.271143
39.872646	1602.458158	18.276160
39.925947	1601.452918	18.281178
40.072066	1588.304393	18.286195
40.163578	1603.693173	18.291213
40.360697	1594.894455	18.296231
40.291017	1593.065881	18.301248
40.301576	1597.198412	18.306266
40.184888	1598.683123	18.311283
40.128249	1591.762246	18.316301
40.690036	1596.692086	18.321319
40.170045	1595.798306	18.326336
40.171350	1597.053638	18.331354
40.393829	1598.613686	18.336371
40.306487	1604.095890	18.341389
40.492968	1597.388692	18.346407
40.531943	1608.842093	18.351424
40.589175	1614.634220	18.356442
40.558295	1620.655899	18.361459
40.463466	1625.047619	18.366477
40.862033	1616.791518	18.371495
40.631069	1626.262466	18.376512
40.308046	1621.218753	18.381530
40.516574	1623.829143	18.386547
40.543723	1620.362093	18.391565
40.606528	1633.013927	18.396583
40.840851	1646.281860	18.401600
40.833014	1644.809181	18.406618
40.947958	1640.955542	18.411635
40.991917	1650.597912	18.416653
41.711414	1640.085509	18.421671
41.154795	1643.987555	18.426688
41.292681	1639.807284	18.431706
41.452879	1641.677255	18.436723
41.694428	1645.592418	18.441741
41.688796	1635.358745	18.446759
41.777618	1641.112974	18.451776
41.275587	1635.638660	18.456794
41.749238	1637.652005	18.461811
41.765837	1637.734336	18.466829
41.788729	1631.469958	18.471847
41.675618	1644.111952	18.476864
41.419476	1643.903615	18.481882
41.916329	1634.994223	18.486899
41.470366	1638.624796	18.491917
41.947330	1637.212790	18.496935
41.886575	1640.033913	18.501952
41.994355	1629.818866	18.506970
42.039848	1635.224363	18.511987
41.739738	1640.416219	18.517005
41.980848	1630.967284	18.522023
41.861754	1630.355941	18.527040
41.740109	1654.333605	18.532058
42.556661	1656.194507	18.537075
42.229561	1670.393609	18.542093
42.005883	1670.416905	18.547111
42.042671	1665.417144	18.552128
42.167086	1671.445807	18.557146
42.612558	1662.274040	18.562163
42.429336	1666.360328	18.567181
42.325711	1660.484210	18.572199
42.603477	1662.455978	18.577216
42.502635	1670.218003	18.582234
42.639391	1654.041046	18.587251
42.460160	1666.748731	18.592269
42.462854	1656.971539	18.597287
42.360701	1654.604633	18.602304
42.128799	1666.768676	18.607322
42.698939	1664.793208	18.612339
42.608011	1683.678423	18.617357
42.662057	1687.284091	18.622375
42.693008	1690.810513	18.627392
43.062640	1690.055647	18.632410
43.084969	1690.703566	18.637427
42.668748	1693.585130	18.642445
43.020114	1685.433265	18.647463
43.300097	1685.002693	18.652480
43.021666	1692.416180	18.657498
43.319089	1686.604357	18.662515
43.309349	1684.826870	18.667533
43.477945	1680.671424	18.672551
43.379064	1688.012266	18.677568
43.280772	1689.359294	18.682586
43.799198	1679.655750	18.687603
43.563108	1681.263389	18.692621
43.817444	1687.809130	18.697639
43.666336	1688.193640	18.702656
43.373324	1695.698913	18.707674
43.839377	1684.363088	18.712691
43.542076	1680.192264	18.717709
43.812644	1673.302212	18.722727
43.727183	1676.571527	18.727744
43.620811	1679.957298	18.732762
43.751012	1673.396394	18.737779
43.898382	1681.633864	18.742797
43.792724	1682.343526	18.747815
43.949645	1683.123097	18.752832
43.651690	1679.624036	18.757850
43.971498	1680.710496	18.762867
44.164404	1699.346764	18.767885
44.274598	1703.649441	18.772903
44.124378	1699.500322	18.777920
44.017739	1706.796788	18.782938
44.330720	1707.706427	18.787955
44.429705	1712.413720	18.792973
44.327195	1707.077559	18.797991
44.316869	1709.057270	18.803008
43.897184	1710.487436	18.808026
44.377243	1711.092244	18.813043
44.477617	1703.172087	18.818061
44.539398	1704.943007	18.823079
44.792778	1702.417618	18.828096
44.750992	1705.512778	18.833114
44.526970	1696.167197	18.838131
44.607705	1704.612563	18.843149
44.540761	1700.229181	18.848167
44.601320	1715.968868	18.853184
44.270212	1728.902539	18.858202
44.997111	1736.529511	18.863219
45.157957	1736.785204	18.868237
45.042130	1731.220530	18.873255
45.408078	1732.547780	18.878272
45.119913	1732.385296	18.883290
45.233097	1726.101205	18.888307
45.102582	1731.631154	18.893325
45.209911	1719.869657	18.898343
45.489962	1719.661122	18.903360
45.058924	1731.272751	18.908378
45.328676	1729.769063	18.913395
45.183855	1723.176903	18.918413
45.027874	1726.160660	18.923431
45.507120	1721.624237	18.928448
45.240307	1725.777532	18.933466
45.546979	1730.510679	18.938483
45.522540	1750.365680	18.943501
45.209984	1745.707990	18.948519
45.644411	1739.252986	18.953536
45.504587	1750.916019	18.958554
45.798455	1739.657090	18.963571
45.670621	1742.080673	18.968589
45.609010	1737.588523	18.973607
45.969861	1744.727680	18.978624
45.553229	1742.164010	18.983642
45.569597	1753.118895	18.988659
46.123503	1765.234400	18.993677
45.884230	1776.125330	18.998695
46.358897	1761.632090	19.003712
46.200322	1774.282505	19.008730
46.067543	1771.763563	19.013747
46.082696	1768.298467	19.018765
46.226488	1773.988525	19.023783
46.489141	1770.170634	19.028800
46.185239	1761.964627	19.033818
46.644292	1758.376820	19.038835
46.759795	1756.551423	19.043853
46.740609	1758.881822	19.048871
47.016715	1764.653907	19.053888
46.966457	1762.091382	19.058906
46.935735	1754.798028	19.063923
46.725305	1755.143935	19.068941
46.625444	1763.329863	19.073959
47.076003	1755.394217	19.078976
46.772427	1765.506017	19.083994
46.718045	1767.277674	19.089011
46.639077	1760.068291	19.094029
46.949238	1759.837840	19.099047
47.302259	1757.800672	19.104064
46.816408	1763.178049	19.109082
47.015842	1770.971508	19.114099
47.079841	1783.094128	19.119117
47.225319	1772.839281	19.124135
47.535337	1776.971490	19.129152
47.338020	1783.912924	19.134170
47.849374	1780.161727	19.139187
47.677301	1781.057589	19.144205
47.730549	1786.513429	19.149223
48.019153	1771.119483	19.154240
47.253717	1763.600529	19.159258
47.516801	1768.698389	19.164275
47.684596	1775.008494	19.169293
47.793018	1778.174468	19.174311
47.617766	1773.366082	19.179328
47.701585	1778.096772	19.184346
47.938444	1769.363818	19.189363
48.147458	1773.484797	19.194381
47.838619	1779.769492	19.199399
47.836650	1771.955617	19.204416
47.703228	1780.612075	19.209434
47.919457	1776.671160	19.214451
48.101513	1765.519702	19.219469
48.122676	1775.906088	19.224487
48.229234	1779.982221	19.229504
47.952112	1794.647182	19.234522
48.334393	1801.209976	19.239539
48.423804	1807.991346	19.244557
48.428488	1807.952814	19.249575
48.874497	1800.542314	19.254592
48.619538	1804.582642	19.259610
48.874136	1802.453891	19.264627
48.893909	1801.234896	19.269645
48.347745	1805.840375	19.274663
48.774090	1793.150008	19.279680
48.456730	1808.517320	19.284698
48.361396	1806.972104	19.289715
48.810704	1797.751197	19.294733
48.534268	1807.867979	19.299751
48.831721	1795.011155	19.304768
48.871644	1804.713739	19.309786
48.577828	1798.755672	19.314803
48.930088	1815.094806	19.319821
49.038314	1820.472263	19.324839
49.728057	1824.802244	19.329856
49.386947	1828.642273	19.334874
49.319044	1826.665737	19.339891
49.516583	1825.218485	19.344909
49.093615	1825.864156	19.349927
49.271539	1825.758356	19.354944
49.102256	1828.484095	19.359962
49.599345	1823.076569	19.364979
49.592020	1820.189599	19.369997
49.478521	1827.036071	19.375015
49.806966	1824.936428	19.380032
49.508149	1823.046158	19.385050
49.043737	1819.207693	19.390067
49.282998	1837.446684	19.395085
49.486892	1865.909413	19.400103
49.824569	1856.837272	19.405120
49.813907	1856.454820	19.410138
49.776100	1850.329933	19.415155
50.047930	1854.936603	19.420173
49.845943	1853.964167	19.425191
50.569423	1859.793318	19.430208
50.127880	1863.069661	19.435226
50.501276	1867.795740	19.440243
50.523607	1862.703426	19.445261
50.351380	1861.278025	19.450279
50.521805	1853.724544	19.455296
50.662761	1857.021370	19.460314
50.684483	1863.053331	19.465331
50.617141	1856.719156	19.470349
50.335548	1857.428034	19.475367
50.919572	1864.111391	19.480384
50.890473	1872.851810	19.485402
50.548732	1877.324642	19.490419
50.936606	1877.016755	19.495437
51.090397	1877.448030	19.500455
51.050772	1876.627453	19.505472
50.882196	1873.497089	19.510490
51.161274	1878.602967	19.515507
50.997617	1872.481980	19.520525
50.922315	1871.831486	19.525543
50.862715	1877.999754	19.530560
50.693745	1880.249459	19.535578
50.622714	1871.851683	19.540595
51.249193	1880.215051	19.545613
51.526777	1905.441193	19.550631
51.292394	1894.562930	19.555648
51.713638	1904.597721	19.560666
51.524147	1902.544061	19.565683
51.905156	1899.886877	19.570701
51.689612	1894.580391	19.575719
51.417199	1896.680687	19.580736
51.981196	1900.872060	19.585754
51.917384	1894.608939	19.590771
52.212233	1889.852209	19.595789
52.002194	1897.885975	19.600807
51.835072	1887.767065	19.605824
51.951997	1885.068568	19.610842
52.104552	1881.316519	19.615859
52.388318	1889.844906	19.620877
52.035470	1892.329786	19.625895
52.092353	1887.177805	19.630912
52.050052	1885.310803	19.635930
52.207799	1892.503737	19.640947
52.196706	1879.064062	19.645965
52.238598	1883.233215	19.650983
52.159136	1884.740135	19.656000
52.277393	1887.675759	19.661018
52.277886	1890.480487	19.666035
52.358918	1902.945268	19.671053
52.387935	1918.332897	19.676071
52.701450	1918.775523	19.681088
52.591366	1918.530793	19.686106
52.690520	1914.699387	19.691123
52.986456	1908.615676	19.696141
52.761128	1913.347594	19.701159
52.724846	1910.651232	19.706176
52.886294	1913.194663	19.711194
52.751843	1917.983191	19.716211
52.949035	1913.879642	19.721229
53.018323	1942.225427	19.726247
53.160668	1940.232962	19.731264
53.428679	1942.981593	19.736282
53.430687	1940.620625	19.741299
53.658835	1933.937093	19.746317
53.564062	1945.249105	19.751335
53.561993	1934.397703	19.756352
53.820074	1936.568045	19.761370
53.497694	1938.481735	19.766387
53.660841	1939.089813	19.771405
53.313075	1934.509551	19.776423
53.685516	1927.938353	19.781440
53.947016	1937.364958	19.786458
53.572268	1935.719139	19.791475
53.936124	1924.620933	19.796493
53.559984	1929.548696	19.801511
53.882812	1925.769624	19.806528
53.887553	1934.892277	19.811546
53.968883	1952.645733	19.816563
54.246899	1945.339753	19.821581
54.206731	1951.718224	19.826599
54.364589	1950.136977	19.831616
54.236334	1948.405855	19.836634
54.106892	1962.502809	19.841651
54.590861	1961.691992	19.846669
54.321694	1956.636101	19.851687
54.586106	1954.317511	19.856704
54.813316	1951.288532	19.861722
54.732552	1953.490177	19.866739
54.891970	1945.402244	19.871757
54.624062	1963.308026	19.876775
54.383490	1955.422146	19.881792
54.667662	1950.904965	19.886810
54.412411	1968.130298	19.891827
54.754179	1977.427492	19.896845
54.809321	1986.392615	19.901863
55.013552	1981.193764	19.906880
55.253799	1979.778011	19.911898
55.094842	1987.893918	19.916915
55.250439	1969.969774	19.921933
55.364211	1982.575264	19.926951
55.441388	1977.606118	19.931968
55.639043	1975.037549	19.936986
55.294805	1976.902105	19.942003
55.347118	1974.850526	19.947021
55.336573	1984.494254	19.952039
55.816021	1999.786124	19.957056
55.571433	2001.807415	19.962074
55.800782	1998.091443	19.967091
55.769273	1997.089590	19.972109
55.897420	1989.828877	19.977127
55.764587	1997.900700	19.982144
55.933930	1995.820291	19.987162
55.780179	2001.149454	19.992179
55.849615	1996.111897	19.997197
55.714648	1995.301981	20.002215
55.620796	2002.027557	20.007232
55.695168	1999.715229	20.012250
55.864993	2019.543134	20.017267
56.175682	2020.132692	20.022285
56.530616	2022.559851	20.027303
56.474845	2027.707835	20.032320
56.789543	2014.572378	20.037338
56.665588	2016.526452	20.042355
56.987084	2019.876099	20.047373
57.030836	2015.489654	20.052391
56.681773	2018.282989	20.057408
56.783854	2016.715695	20.062426
56.742278	2019.488828	20.067443
56.911901	2009.969215	20.072461
56.788279	2019.391131	20.077479
56.781629	2019.945041	20.082496
56.814890	2016.148930	20.087514
56.721754	2015.730522	20.092531
56.981737	2031.289081	20.097549
57.351548	2037.325288	20.102567
57.500482	2033.326945	20.107584
57.607422	2027.587088	20.112602
57.363483	2044.245657	20.117619
57.667468	2034.271094	20.122637
57.649986	2034.335841	20.127655
57.522047	2031.165251	20.132672
57.769346	2034.695301	20.137690
57.736731	2042.384008	20.142707
57.818670	2041.042888	20.147725
57.820762	2036.004657	20.152743
57.852917	2041.536522	20.157760
58.079905	2028.967164	20.162778
57.801083	2033.746953	20.167795
57.992169	2024.235589	20.172813
58.216963	2027.107142	20.177831
57.861526	2041.150246	20.182848
57.962943	2030.705275	20.187866
57.755702	2043.098999	20.192883
57.894057	2055.766228	20.197901
58.558311	2065.609310	20.202919
58.445518	2063.084649	20.207936
58.559650	2062.392544	20.212954
58.638424	2069.674229	20.217971
58.503615	2060.649886	20.222989
58.774063	2070.240843	20.228007
58.664598	2068.095562	20.233024
58.715665	2054.539929	20.238042
58.669310	2054.029126	20.243059
58.860484	2059.692547	20.248077
58.716063	2059.809414	20.253095
58.430656	2074.885469	20.258112
58.973307	2071.275090	20.263130
59.261161	2075.221674	20.268147
58.768030	2075.953775	20.273165
59.296561	2071.099636	20.278183
59.194287	2076.234862	20.283200
59.358518	2074.889169	20.288218
59.360010	2079.369009	20.293235
59.427074	2077.609076	20.298253
59.508715	2075.445538	20.303271
59.113525	2077.968166	20.308288
59.689182	2092.911512	20.313306
59.747170	2107.453562	20.318323
59.715674	2108.664364	20.323341
59.714044	2108.308364	20.328359
59.597338	2109.479730	20.333376
59.802419	2109.697003	20.338394
59.726420	2113.604232	20.343411
59.811908	2109.438416	20.348429
59.966099	2102.579651	20.353447
60.147306	2117.926136	20.358464
60.325845	2116.906033	20.363482
60.613742	2116.326105	20.368499
60.596261	2112.245450	20.373517
60.555926	2098.467110	20.378535
60.308340	2097.369133	20.383552
60.420219	2096.903392	20.388570
60.682366	2106.321725	20.393587
60.610323	2120.814842	20.398605
60.971691	2117.973861	20.403623
60.545458	2121.608363	20.408640
60.810042	2112.346595	20.413658
61.170960	2123.898651	20.418675
61.023818	2119.207553	20.423693
61.028991	2114.603052	20.428711
60.856216	2123.238656	20.433728
60.778549	2123.294864	20.438746
61.277769	2117.581364	20.443763
60.991639	2117.164985	20.448781
61.070935	2119.192116	20.453799
61.218697	2142.804263	20.458816
61.436754	2142.177234	20.463834
61.506998	2152.819534	20.468851
61.431811	2142.421447	20.473869
61.562368	2139.485603	20.478887
61.814586	2149.283177	20.483904
61.634974	2144.680521	20.488922
61.656745	2147.771939	20.493939
61.777404	2148.991018	20.498957
61.974957	2146.907887	20.503975
61.486974	2151.624308	20.508992
61.841699	2159.169017	20.514010
62.126278	2170.955408	20.519027
62.230963	2181.710140	20.524045
62.604881	2174.845671	20.529063
62.564416	2176.569793	20.534080
62.307220	2177.273070	20.539098
62.418269	2171.051360	20.544115
62.202034	2172.511267	20.549133
62.889088	2163.139755	20.554151
62.641840	2168.220666	20.559168
62.693013	2165.984204	20.564186
62.838228	2170.498150	20.569203
62.734645	2176.336406	20.574221
62.624227	2164.470858	20.579239
63.086952	2159.213400	20.584256
62.770146	2160.308449	20.589274
62.881369	2168.173410	20.594291
62.519219	2178.978662	20.599309
62.956284	2175.291250	20.604327
62.939550	2197.818868	20.609344
63.124171	2184.400463	20.614362
63.459562	2195.094958	20.619379
63.291635	2203.717599	20.624397
63.273055	2197.792942	20.629415
63.213019	2196.325704	20.634432
63.608947	2206.498353	20.639450
63.574989	2206.016596	20.644467
63.621888	2226.839564	20.649485
63.902222	2218.595243	20.654503
63.910764	2224.828747	20.659520
64.218918	2214.613607	20.664538
64.456365	2218.096903	20.669555
64.030454	2211.664466	20.674573
64.725166	2210.472275	20.679591
64.207900	2191.304116	20.684608
64.140135	2186.559696	20.689626
64.220962	2183.400967	20.694643
63.766819	2199.655908	20.699661
64.096644	2202.203794	20.704679
63.911855	2211.500121	20.709696
63.911339	2211.051805	20.714714
64.410745	2223.564112	20.719731
64.228852	2238.038518	20.724749
64.650570	2237.839594	20.729767
64.447317	2251.832884	20.734784
64.643384	2248.816092	20.739802
64.737103	2238.241937	20.744819
64.774994	2252.305148	20.749837
65.183925	2260.003142	20.754855
65.151954	2268.945448	20.759872
65.329207	2266.374698	20.764890
65.309242	2270.521124	20.769907
65.511747	2271.143567	20.774925
65.849079	2262.005498	20.779943
65.745889	2257.359839	20.784960
65.392900	2238.014022	20.789978
65.465646	2236.575978	20.794995
65.537953	2261.315409	20.800013
66.126952	2252.569158	20.805031
65.922821	2258.960728	20.810048
65.711955	2264.396685	20.815066
65.992695	2255.860533	20.820083
65.843262	2260.054772	20.825101
65.947307	2250.419094	20.830119
65.926368	2263.693599	20.835136
65.773949	2268.265909	20.840154
65.951966	2251.783850	20.845171
66.039511	2264.914011	20.850189
66.344604	2280.069272	20.855207
66.547977	2291.816050	20.860224
66.357177	2289.807831	20.865242
66.625256	2288.658714	20.870259
66.416434	2296.416094	20.875277
66.956508	2286.547563	20.880295
66.790583	2287.665278	20.885312
66.695507	2284.437617	20.890330
67.050671	2285.595044	20.895347
66.734696	2294.348158	20.900365
67.078466	2284.706233	20.905383
67.017256	2283.101380	20.910400
66.675870	2289.858222	20.915418
67.055593	2292.388412	20.920435
66.891089	2313.039402	20.925453
67.399577	2312.124506	20.930471
67.389358	2310.113552	20.935488
67.416141	2310.713908	20.940506
67.466781	2302.272918	20.945523
67.212816	2306.358881	20.950541
67.451279	2303.207494	20.955559
67.642519	2327.280853	20.960576
67.733029	2333.689420	20.965594
67.672732	2340.268241	20.970611
67.681297	2339.771959	20.975629
67.909760	2334.234319	20.980647
68.341301	2331.282464	20.985664
68.339253	2334.112103	20.990682
68.221150	2329.418889	20.995699
68.171592	2336.307755	21.000717
68.350550	2332.434686	21.005735
68.194448	2331.104212	21.010752
68.322496	2334.528874	21.015770
68.644697	2326.002749	21.020787
68.506661	2332.376712	21.025805
68.439499	2347.443668	21.030823
68.883361	2355.483186	21.035840
68.949605	2366.451900	21.040858
69.032583	2351.745002	21.045875
69.110081	2362.563418	21.050893
69.133926	2357.729759	21.055911
69.306729	2355.529040	21.060928
69.183130	2359.800528	21.065946
69.490305	2349.169695	21.070963
69.079309	2353.283244	21.075981
69.389192	2347.796294	21.080999
69.623325	2351.209694	21.086016
69.371507	2348.848956	21.091034
69.511302	2352.654371	21.096051
69.430970	2350.683762	21.101069
69.032080	2352.081404	21.106087
69.177522	2364.230759	21.111104
69.216734	2388.412459	21.116122
69.522754	2381.763089	21.121139
69.717751	2383.247451	21.126157
69.719476	2388.650220	21.131175
69.919870	2397.581687	21.136192
69.807242	2409.466705	21.141210
70.480732	2413.358189	21.146227
70.424222	2416.111028	21.151245
70.590461	2415.567376	21.156263
70.974036	2406.854266	21.161280
70.650793	2417.361493	21.166298
71.007939	2405.322279	21.171315
70.980662	2408.109255	21.176333
70.908626	2402.815055	21.181351
70.863961	2403.884747	21.186368
71.024371	2402.287678	21.191386
71.059063	2401.747302	21.196403
70.910817	2401.266744	21.201421
70.843177	2407.808225	21.206439
71.398847	2394.101423	21.211456
71.032049	2399.484500	21.216474
71.445619	2395.074120	21.221491
71.170556	2394.125954	21.226509
71.231678	2402.013502	21.231527
71.425970	2415.411564	21.236544
71.685204	2431.820692	21.241562
72.009985	2423.220462	21.246579
71.804271	2423.709309	21.251597
71.765657	2430.598374	21.256615
72.033562	2420.477957	21.261632
71.622500	2427.551527	21.266650
71.972789	2422.716557	21.271667
71.864163	2430.128656	21.276685
71.727779	2428.257087	21.281703
71.961626	2430.515375	21.286720
71.920146	2443.659570	21.291738
71.951140	2449.360679	21.296755
71.877322	2451.868740	21.301773
72.176035	2451.833102	21.306791
72.374523	2461.425980	21.311808
72.755224	2472.061980	21.316826
72.825292	2477.557014	21.321843
72.955843	2470.180713	21.326861
72.841450	2473.254974	21.331879
72.958689	2473.290724	21.336896
73.132727	2474.009626	21.341914
73.151117	2473.934176	21.346931
73.173918	2479.612242	21.351949
72.821195	2476.101592	21.356967
73.362494	2466.319365	21.361984
73.156710	2470.419047	21.367002
73.555221	2466.511168	21.372019
73.202073	2456.308507	21.377037
73.285386	2475.219379	21.382055
73.794591	2480.583828	21.387072
74.065126	2486.892176	21.392090
74.309764	2482.371546	21.397107
74.220073	2481.183615	21.402125
73.908619	2475.412861	21.407143
74.196806	2468.371111	21.412160
74.035325	2478.052341	21.417178
74.148954	2473.354182	21.422195
74.352588	2485.677866	21.427213
74.419048	2483.565213	21.432231
74.335158	2470.718608	21.437248
73.849865	2478.002139	21.442266
74.314078	2476.914635	21.447283
74.263418	2482.282407	21.452301
74.204454	2497.042227	21.457319
74.853055	2496.258857	21.462336
74.744557	2506.345134	21.467354
74.727222	2502.677762	21.472371
75.049641	2504.043395	21.477389
74.720789	2497.523896	21.482407
75.071282	2508.016490	21.487424
75.212893	2504.930708	21.492442
75.368536	2520.448370	21.497459
75.572683	2522.430471	21.502477
75.573853	2538.559586	21.507495
75.342156	2530.255776	21.512512
75.344988	2539.083414	21.517530
75.459624	2518.511331	21.522547
75.592707	2537.595544	21.527565
75.283795	2532.115704	21.532583
75.578228	2536.661353	21.537600
75.532064	2551.799049	21.542618
76.081724	2546.901501	21.547635
76.442295	2554.246606	21.552653
76.476759	2556.924168	21.557671
76.700340	2551.147482	21.562688
76.516073	2562.822812	21.567706
76.323760	2550.331514	21.572723
76.657672	2555.974634	21.577741
76.397813	2557.808749	21.582759
76.916894	2545.672138	21.587776
76.925965	2542.175985	21.592794
76.862467	2542.439308	21.597811
76.768228	2550.371948	21.602829
76.541499	2548.887784	21.607847
76.816007	2538.341764	21.612864
76.659653	2560.023287	21.617882
76.833298	2567.402497	21.622899
77.072167	2576.731658	21.627917
76.946936	2583.785928	21.632935
77.362676	2575.152444	21.637952
77.114176	2587.519570	21.642970
77.710880	2601.283869	21.647987
77.386107	2605.797012	21.653005
77.557714	2605.741078	21.658023
77.936789	2600.043360	21.663040
77.752765	2600.822340	21.668058
77.948501	2607.260058	21.673075
78.064945	2608.188515	21.678093
77.907872	2592.689193	21.683111
78.204200	2589.585653	21.688128
78.046700	2600.245887	21.693146
78.237518	2592.131946	21.698163
78.399893	2604.470430	21.703181
78.547224	2624.613087	21.708199
78.877062	2621.765426	21.713216
78.732192	2625.088873	21.718234
78.340212	2624.273835	21.723251
78.788789	2622.659744	21.728269
78.612664	2625.821032	21.733287
78.506776	2622.699822	21.738304
78.584353	2621.605847	21.743322
78.583378	2625.997271	21.748339
78.989346	2634.408981	21.753357
79.063221	2657.419930	21.758375
79.210144	2646.611085	21.763392
78.934477	2645.601580	21.768410
79.436902	2653.609903	21.773427
79.459361	2658.532137	21.778445
79.442466	2680.029309	21.783463
79.637150	2668.929844	21.788480
79.948862	2670.905573	21.793498
80.184590	2675.114110	21.798515
80.157989	2667.626325	21.803533
80.226592	2677.260134	21.808551
80.344104	2667.004605	21.813568
80.402128	2670.342504	21.818586
80.774040	2665.620028	21.823603
80.338293	2662.546338	21.828621
80.085281	2666.435766	21.833639
80.238607	2667.612073	21.838656
80.191373	2670.018517	21.843674
80.144922	2684.633521	21.848691
80.828902	2687.684701	21.853709
80.785239	2702.220513	21.858727
81.135270	2700.675490	21.863744
80.986653	2696.915626	21.868762
80.681402	2697.672947	21.873779
80.929711	2695.259272	21.878797
81.131502	2713.577157	21.883815
81.135925	2713.617018	21.888832
81.068319	2728.710795	21.893850
81.308984	2727.993775	21.898867
81.850492	2714.429207	21.903885
81.614167	2725.241169	21.908903
81.776685	2728.438935	21.913920
81.802982	2719.573768	21.918938
81.950229	2727.730312	21.923955
82.206744	2720.858665	21.928973
81.803925	2727.844779	21.933991
82.301104	2734.247208	21.939008
82.266688	2747.209768	21.944026
82.347690	2750.495450	21.949043
82.740475	2743.495712	21.954061
82.235817	2750.105361	21.959079
82.778640	2750.817946	21.964096
82.588585	2750.203738	21.969114
82.177721	2746.095128	21.974131
82.507934	2743.009177	21.979149
82.396001	2756.379883	21.984167
82.848212	2766.177415	21.989184
82.900383	2767.222830	21.994202
82.992035	2770.318945	21.999219
83.462048	2771.962944	22.004237
83.307526	2776.190448	22.009255
83.395911	2773.713076	22.014272
83.445442	2779.078536	22.019290
83.327880	2778.970472	22.024307
83.534167	2767.517809	22.029325
83.632264	2766.590911	22.034343
83.888455	2768.824683	22.039360
83.916767	2770.939874	22.044378
83.776525	2788.612064	22.049395
84.024744	2792.719344	22.054413
84.009059	2809.192500	22.059431
84.072828	2794.260790	22.064448
84.211687	2809.389757	22.069466
83.942547	2807.090087	22.074483
84.040798	2795.086745	22.079501
84.415004	2804.440884	22.084519
84.736091	2817.103286	22.089536
84.791819	2819.457270	22.094554
84.504719	2823.957544	22.099571
84.960883	2821.714964	22.104589
84.796294	2824.609795	22.109607
84.896718	2817.605276	22.114624
85.311787	2810.974681	22.119642
84.740508	2818.054085	22.124659
85.363761	2807.262334	22.129677
85.536393	2823.524785	22.134695
85.504604	2835.057740	22.139712
85.961185	2840.160536	22.144730
85.399367	2846.615110	22.149747
85.678212	2846.103198	22.154765
85.251988	2841.338000	22.159783
85.302053	2846.532515	22.164800
85.635418	2833.258231	22.169818
85.955746	2853.769423	22.174835
86.217235	2859.462443	22.179853
86.208232	2860.071895	22.184871
86.110903	2861.197585	22.189888
86.156827	2858.635097	22.194906
86.346054	2862.511594	22.199923
86.526207	2860.045394	22.204941
86.666647	2867.360160	22.209959
86.648163	2887.117586	22.214976
87.027397	2887.907267	22.219994
87.126924	2894.064553	22.225011
87.299910	2888.744975	22.230029
87.343245	2885.001714	22.235047
87.254132	2887.392289	22.240064
87.413498	2882.298215	22.245082
87.402795	2890.584942	22.250099
87.497602	2885.078293	22.255117
87.477265	2879.259188	22.260135
87.488674	2877.962748	22.265152
87.602255	2885.790671	22.270170
87.537918	2881.577010	22.275187
87.455682	2881.839504	22.280205
87.822512	2899.830652	22.285223
87.831101	2904.083158	22.290240
88.069564	2907.035692	22.295258
87.966434	2910.890521	22.300275
88.396860	2911.619361	22.305293
88.370431	2908.333745	22.310311
88.352139	2909.940881	22.315328
88.638625	2914.124542	22.320346
88.575130	2925.219076	22.325363
89.033235	2928.344715	22.330381
88.750150	2932.171071	22.335399
88.488395	2936.530949	22.340416
88.799621	2926.192386	22.345434
88.818124	2931.371288	22.350451
88.848535	2931.582058	22.355469
88.940936	2938.650853	22.360487
88.852596	2953.902624	22.365504
89.220384	2958.327582	22.370522
89.425424	2964.084717	22.375539
89.496955	2962.909823	22.380557
89.557335	2959.812989	22.385575
89.517668	2960.636201	22.390592
89.853467	2976.218198	22.395610
89.771213	2985.116479	22.400627
90.138600	2980.106447	22.405645
90.390538	2986.088522	22.410663
90.161898	2989.864142	22.415680
90.318689	2984.050713	22.420698
89.957431	2981.616650	22.425715
90.053574	2980.466028	22.430733
90.204762	2990.158017	22.435751
90.699395	3004.761300	22.440768
90.820454	3005.885885	22.445786
90.617422	3013.119780	22.450803
90.978909	3003.975707	22.455821
90.851996	3007.342721	22.460839
91.097686	2999.830563	22.465856
91.151458	2996.541099	22.470874
91.169948	3015.931511	22.475891
91.647180	3017.836177	22.480909
91.493424	3024.718581	22.485927
91.718316	3030.379925	22.490944
91.794076	3022.639568	22.495962
91.482396	3027.526287	22.500979
91.674499	3031.201938	22.505997
91.910836	3029.569399	22.511015
91.820827	3026.137184	22.516032
92.130290	3039.370246	22.521050
92.310313	3058.478825	22.526067
92.509732	3054.737243	22.531085
92.478884	3052.405958	22.536103
92.349868	3052.101738	22.541120
92.532056	3046.719948	22.546138
92.811231	3054.655591	22.551155
92.841758	3049.431206	22.556173
92.707915	3045.915290	22.561191
92.798311	3053.793204	22.566208
92.927036	3052.394641	22.571226
92.922816	3075.258099	22.576243
93.289239	3087.825019	22.581261
93.554677	3077.825464	22.586279
93.393204	3071.999337	22.591296
93.538202	3079.114611	22.596314
93.574535	3074.500729	22.601331
93.855361	3068.137158	22.606349
93.457386	3076.831441	22.611367
93.462075	3083.165148	22.616384
93.688284	3103.102828	22.621402
93.704800	3092.793656	22.626419
93.722176	3102.390536	22.631437
94.152220	3110.260674	22.636455
94.170406	3130.432061	22.641472
94.644150	3131.095862	22.646490
94.708850	3130.386698	22.651507
94.700351	3135.492965	22.656525
94.486409	3129.429416	22.661543
94.330188	3132.548136	22.666560
94.604846	3127.238025	22.671578
94.721436	3145.344125	22.676595
95.073779	3146.559180	22.681613
95.229568	3152.637168	22.686631
95.251554	3157.482464	22.691648
95.609223	3153.181535	22.696666
95.289018	3153.751963	22.701683
95.505172	3156.076287	22.706701
95.686311	3141.445316	22.711719
95.845250	3150.565200	22.716736
95.937264	3142.439379	22.721754
95.928683	3151.178299	22.726771
95.761972	3146.427918	22.731789
95.827523	3157.986338	22.736807
95.915551	3177.587900	22.741824
96.187290	3180.372363	22.746842
96.234631	3186.191126	22.751859
95.622195	3184.927861	22.756877
96.044674	3187.681068	22.761895
96.113062	3206.900447	22.766912
96.686893	3203.278355	22.771930
96.784606	3223.674908	22.776947
97.169022	3226.695474	22.781965
97.238046	3222.465940	22.786983
96.837757	3230.348010	22.792000
97.376592	3217.877264	22.797018
97.463112	3221.107402	22.802035
97.522996	3226.101185	22.807053
97.667357	3211.384103	22.812071
97.357091	3221.607013	22.817088
97.732586	3231.288002	22.822106
97.725602	3241.276442	22.827123
97.926302	3244.694789	22.832141
98.216512	3232.734534	22.837159
98.095353	3249.543367	22.842176
98.007983	3240.672311	22.847194
98.388583	3244.534150	22.852211
98.312878	3247.969911	22.857229
98.941581	3257.382199	22.862247
98.690483	3272.841562	22.867264
98.996298	3265.147651	22.872282
98.900094	3274.764229	22.877299
98.937863	3269.572433	22.882317
99.275819	3270.272110	22.887335
98.867455	3273.318418	22.892352
99.080325	3266.432498	22.897370
99.421448	3272.701131	22.902387
99.659632	3271.635250	22.907405
99.391438	3263.558766	22.912423
99.565158	3280.747989	22.917440
99.545581	3281.588760	22.922458
99.967624	3289.324867	22.927475
99.961813	3291.794240	22.932493
100.459329	3293.303417	22.937511
100.174821	3292.081922	22.942528
100.140644	3297.660653	22.947546
100.446150	3288.526077	22.952563
100.467088	3285.392398	22.957581
100.815388	3281.269383	22.962599
100.679660	3281.556095	22.967616
100.867582	3289.827867	22.972634
100.928803	3304.281514	22.977651
100.875530	3318.061142	22.982669
101.223697	3306.645232	22.987687
101.046554	3321.042679	22.992704
101.333209	3310.170867	22.997722
101.125053	3316.536758	23.002739
100.858979	3319.756389	23.007757
101.193636	3321.474835	23.012775
101.230287	3339.027797	23.017792
101.670023	3341.651784	23.022810
101.521014	3345.792692	23.027827
101.209682	3354.592087	23.032845
101.648946	3355.218296	23.037863
101.738813	3373.793310	23.042880
102.092360	3380.224515	23.047898
102.273527	3384.220206	23.052915
101.887006	3388.448092	23.057933
102.380431	3384.203374	23.062951
102.135744	3406.047955	23.067968
102.112243	3400.713486	23.072986
102.530559	3406.611085	23.078003
102.767689	3428.998438	23.083021
103.001271	3430.926173	23.088039
102.981969	3438.687388	23.093056
103.285246	3428.789626	23.098074
103.311366	3430.882432	23.103091
103.219598	3427.873696	23.108109
103.631773	3424.102315	23.113127
103.489665	3436.763161	23.118144
103.660371	3457.250308	23.123162
104.170595	3446.857982	23.128179
103.844796	3460.821848	23.133197
104.170705	3452.998520	23.138215
104.413952	3449.217301	23.143232
104.252074	3444.945218	23.148250
104.690460	3448.987722	23.153267
104.190787	3445.553939	23.158285
104.316104	3439.763272	23.163303
104.466786	3458.534247	23.168320
104.900573	3466.836675	23.173338
104.961987	3459.948577	23.178355
105.048506	3474.188719	23.183373
105.201028	3473.589030	23.188391
105.063610	3471.487555	23.193408
105.228638	3471.234655	23.198426
105.725161	3470.764648	23.203443
105.463505	3473.657950	23.208461
105.755077	3484.054255	23.213479
105.534268	3494.751172	23.218496
105.851076	3485.571299	23.223514
106.163936	3487.956444	23.228531
105.939692	3495.563800	23.233549
105.956814	3494.864072	23.238567
106.137576	3502.351222	23.243584
106.169333	3522.856342	23.248602
106.561402	3522.286290	23.253619
106.596809	3522.747847	23.258637
106.348517	3521.499075	23.263655
106.465665	3521.549807	23.268672
106.205357	3541.377234	23.273690
107.105820	3544.321875	23.278707
106.982712	3552.273189	23.283725
107.465866	3547.664729	23.288743
107.497611	3551.761196	23.293760
107.454629	3557.442671	23.298778
107.503818	3548.665774	23.303795
107.462405	3568.076239	23.308813
107.711978	3574.492845	23.313831
107.704574	3588.146991	23.318848
107.987500	3582.145903	23.323866
107.753666	3577.966416	23.328883
107.648051	3587.640656	23.333901
108.124196	3591.741521	23.338919
108.403679	3607.224405	23.343936
108.417716	3609.604705	23.348954
108.762556	3601.658075	23.353971
108.721424	3602.462269	23.358989
108.941004	3598.984184	23.364007
109.033717	3597.305673	23.369024
109.080000	3596.599930	23.374042
108.933530	3592.579618	23.379059
109.038003	3609.444012	23.384077
109.260327	3618.395783	23.389095
109.410060	3615.807715	23.394112
109.207479	3627.585700	23.399130
109.863308	3613.505307	23.404147
109.279059	3620.971514	23.409165
109.585096	3630.034251	23.414183
109.842397	3642.289722	23.419200
109.914705	3647.126839	23.424218
110.009809	3650.757272	23.429235
110.102535	3650.017063	23.434253
110.053566	3669.234784	23.439271
110.615774	3674.840912	23.444288
110.629745	3679.713685	23.449306
110.740092	3676.517087	23.454323
110.770356	3677.435859	23.459341
110.736272	3677.767962	23.464359
111.047976	3686.701430	23.469376
111.119983	3704.117829	23.474394
111.460245	3695.939202	23.479411
111.276299	3704.040053	23.484429
111.275444	3690.866450	23.489447
111.565730	3700.676422	23.494464
111.459159	3716.420206	23.499482
111.869761	3725.269204	23.504499
111.861671	3733.424431	23.509517
112.152725	3728.036591	23.514535
112.237443	3719.335618	23.519552
112.171478	3727.621700	23.524570
112.743583	3734.192875	23.529587
112.640668	3741.366822	23.534605
112.692532	3741.137773	23.539623
113.078005	3740.857035	23.544640
113.094049	3752.158307	23.549658
113.192698	3749.144365	23.554675
113.063082	3747.172681	23.559693
112.797602	3750.740378	23.564711
113.406583	3742.909023	23.569728
113.366774	3764.035838	23.574746
113.727100	3771.874937	23.579763
113.663795	3786.337045	23.584781
113.827287	3771.838348	23.589799
113.687679	3770.972009	23.594816
113.890257	3783.374860	23.599834
114.299071	3778.993632	23.604851
114.431864	3790.276390	23.609869
114.329968	3793.352383	23.614887
114.361579	3798.292754	23.619904
114.146853	3802.787229	23.624922
114.661264	3799.175630	23.629939
114.731406	3811.445289	23.634957
114.557601	3826.505731	23.639975
114.944453	3823.981930	23.644992
114.792697	3828.760516	23.650010
115.272264	3827.229380	23.655027
115.098692	3831.887547	23.660045
115.199384	3854.646573	23.665063
115.529118	3851.587658	23.670080
115.472125	3855.049986	23.675098
115.848995	3847.877568	23.680115
115.850825	3855.196452	23.685133
116.155959	3882.393567	23.690151
116.315994	3879.196971	23.695168
116.363320	3878.030741	23.700186
116.474708	3873.899545	23.705203
116.822168	3871.100329	23.710221
116.917900	3884.470691	23.715239
117.114008	3874.306888	23.720256
116.902947	3876.432721	23.725274
117.003863	3877.164192	23.730291
117.055711	3878.875580	23.735309
116.527063	3876.860478	23.740327
117.003754	3878.737783	23.745344
117.044605	3899.343086	23.750362
117.023601	3903.141641	23.755379
117.313279	3915.801081	23.760397
117.382961	3926.695903	23.765415
117.946469	3935.314951	23.770432
117.968785	3936.157878	23.775450
117.882673	3925.044556	23.780467
118.128160	3934.804604	23.785485
118.088051	3954.790613	23.790503
118.486859	3949.475817	23.795520
118.648662	3963.699215	23.800538
118.813492	3952.604180	23.805555
118.851178	3959.824250	23.810573
118.859329	3965.700193	23.815591
119.430756	3977.002605	23.820608
118.981183	3992.330548	23.825626
119.453730	3995.552064	23.830643
119.652209	3981.960510	23.835661
119.214747	3988.826910	23.840679
119.611207	3982.288686	23.845696
119.433253	3995.333532	23.850714
119.886126	3992.162064	23.855731
120.303958	3996.308525	23.860749
120.323767	4004.138753	23.865767
120.434747	4002.864323	23.870784
120.345137	4005.501643	23.875802
120.119672	3997.866196	23.880819
120.233001	4017.433909	23.885837
120.515603	4027.266622	23.890855
121.068919	4024.390377	23.895872
120.817734	4033.871243	23.900890
120.871816	4042.247869	23.905907
121.340826	4045.891305	23.910925
121.208424	4056.745647	23.915943
121.811218	4048.446197	23.920960
121.650596	4051.495343	23.925978
121.451498	4044.577666	23.930995
121.779522	4063.108162	23.936013
121.789421	4081.807115	23.941031
122.183975	4074.976996	23.946048
122.254606	4088.584796	23.951066
122.289047	4082.698685	23.956083
122.350394	4091.233214	23.961101
122.436630	4102.249059	23.966119
122.795812	4100.368873	23.971136
122.821645	4113.108382	23.976154
122.861199	4114.948623	23.981171
122.842096	4103.104282	23.986189
123.011564	4129.327673	23.991207
123.338320	4117.245718	23.996224
123.375287	4143.580847	24.001242
123.625736	4129.247374	24.006259
124.068860	4126.029455	24.011277
123.846726	4128.491066	24.016295
123.858949	4128.358353	24.021312
123.810561	4143.979136	24.026330
123.976431	4162.735841	24.031347
124.494691	4159.240866	24.036365
124.362273	4160.544138	24.041383
124.776712	4145.923615	24.046400
124.704569	4156.864916	24.051418
124.760250	4155.802812	24.056435
124.648841	4163.074435	24.061453
124.777158	4184.341724	24.066471
125.138204	4185.067945	24.071488
124.995033	4188.307960	24.076506
125.339488	4182.911520	24.081523
125.535718	4185.814983	24.086541
125.526435	4197.053041	24.091559
126.001347	4196.720871	24.096576
126.036076	4206.987713	24.101594
126.353212	4202.312441	24.106611
126.207370	4201.623911	24.111629
126.144893	4211.316988	24.116647
126.278799	4199.714216	24.121664
126.270808	4210.589018	24.126682
126.789614	4222.706754	24.131699
126.748142	4230.081022	24.136717
126.828137	4237.637579	24.141735
126.846184	4234.901106	24.146752
126.395016	4242.088834	24.151770
126.979672	4251.729138	24.156787
126.910534	4255.244360	24.161805
126.924509	4268.886109	24.166823
127.608996	4281.348964	24.171840
127.820694	4295.433673	24.176858
127.936041	4288.983603	24.181875
127.997268	4282.390501	24.186893
127.966839	4283.879294	24.191911
128.112565	4296.636904	24.196928
128.432461	4313.147439	24.201946
128.396036	4309.525330	24.206963
128.587142	4313.977962	24.211981
128.628205	4328.366588	24.216999
129.052409	4339.799169	24.222016
129.014534	4342.680779	24.227034
129.043999	4334.446960	24.232051
129.480951	4339.645648	24.237069
129.594387	4349.970431	24.242087
129.755413	4364.113206	24.247104
129.679365	4368.366733	24.252122
129.619869	4367.639486	24.257139
130.004735	4371.367810	24.262157
130.289654	4368.465062	24.267175
129.958386	4364.323150	24.272192
130.207307	4386.292920	24.277210
130.172469	4390.951514	24.282227
130.573932	4392.345189	24.287245
130.525074	4401.019414	24.292263
130.978641	4393.810032	24.297280
130.940262	4407.662967	24.302298
131.160083	4403.384918	24.307315
131.385082	4405.298447	24.312333
131.333686	4404.100483	24.317351
131.791774	4420.032248	24.322368
131.686306	4444.613981	24.327386
131.960891	4450.833467	24.332403
132.100711	4444.313128	24.337421
132.125549	4446.600018	24.342439
132.113335	4447.605410	24.347456
132.041372	4445.666619	24.352474
132.022577	4464.299111	24.357491
132.557088	4458.390711	24.362509
132.571595	4475.374099	24.367527
132.290197	4477.810136	24.372544
133.047827	4494.648465	24.377562
132.932879	4503.926710	24.382579
132.870719	4500.215099	24.387597
132.994393	4508.429244	24.392615
133.212499	4515.845726	24.397632
133.389571	4531.202754	24.402650
133.586880	4538.069831	24.407667
133.796183	4524.213765	24.412685
133.511916	4543.913325	24.417703
133.523621	4560.357011	24.422720
134.119434	4560.150516	24.427738
134.022454	4576.974485	24.432755
134.310183	4587.528885	24.437773
134.341691	4593.268887	24.442791
134.454538	4594.602469	24.447808
134.733926	4598.813752	24.452826
135.150103	4607.918284	24.457843
135.402351	4619.278732	24.462861
135.205734	4620.220945	24.467879
135.723814	4609.873418	24.472896
135.855078	4610.100593	24.477914
136.042373	4617.789204	24.482931
136.326278	4611.491445	24.487949
136.043530	4624.736873	24.492967
135.794129	4630.046139	24.497984
136.517045	4643.837824	24.503002
136.701078	4647.376587	24.508019
136.732880	4631.617157	24.513037
136.890321	4637.165428	24.518055
136.717890	4637.509035	24.523072
137.193137	4651.231473	24.528090
136.984731	4675.934567	24.533107
137.511827	4668.843622	24.538125
137.389991	4664.306257	24.543143
137.199053	4671.475510	24.548160
137.436996	4683.140006	24.553178
137.790627	4694.823161	24.558195
137.650694	4701.594931	24.563213
137.963280	4706.400078	24.568231
137.826266	4720.233390	24.573248
138.356298	4713.960998	24.578266
138.135443	4734.873374	24.583283
138.586221	4721.394563	24.588301
138.847764	4748.029024	24.593319
138.758061	4755.418610	24.598336
138.956485	4755.182610	24.603354
139.012615	4762.220432	24.608371
139.425837	4767.842174	24.613389
139.324037	4778.567513	24.618407
139.371240	4786.210094	24.623424
139.993989	4778.560636	24.628442
139.841139	4787.195585	24.633459
140.249602	4785.515867	24.638477
140.288892	4806.423859	24.643495
140.399060	4803.368038	24.648512
140.500473	4808.792547	24.653530
140.412422	4803.628162	24.658547
140.903162	4812.876407	24.663565
141.052467	4828.365908	24.668583
140.803483	4831.117957	24.673600
141.090196	4835.732900	24.678618
141.238713	4832.476196	24.683635
141.355142	4833.813143	24.688653
141.564306	4843.468725	24.693671
141.438834	4855.443959	24.698688
141.877914	4846.940442	24.703706
141.751065	4855.576637	24.708723
141.811302	4861.656934	24.713741
142.176100	4880.042910	24.718759
142.374796	4879.242967	24.723776
142.555113	4875.660451	24.728794
142.407026	4884.093835	24.733811
142.687145	4895.194698	24.738829
143.035064	4901.671571	24.743847
143.291421	4895.977599	24.748864
143.483992	4895.525985	24.753882
143.622893	4896.792274	24.758899
143.397298	4897.759777	24.763917
143.626790	4904.216090	24.768935
143.775347	4926.107149	24.773952
144.012592	4922.253725	24.778970
144.033045	4928.795061	24.783987
144.355856	4928.333698	24.789005
144.251925	4930.000109	24.794023
144.699231	4947.328191	24.799040
144.768547	4946.035382	24.804058
144.671011	4953.643727	24.809075
144.684975	4953.427236	24.814093
145.008852	4953.906841	24.819111
145.075270	4974.232490	24.824128
145.216594	4974.861240	24.829146
145.124138	4988.651183	24.834163
145.366876	4987.005968	24.839181
145.292478	5000.075455	24.844199
145.443383	5013.944840	24.849216
146.230265	5025.158005	24.854234
146.301235	5038.746882	24.859251
146.281997	5031.728110	24.864269
146.335164	5038.633446	24.869287
146.663649	5051.596111	24.874304
146.979378	5056.131496	24.879322
147.114158	5073.058601	24.884339
147.379100	5056.917555	24.889357
147.441174	5067.077259	24.894375
147.328427	5067.740987	24.899392
147.732232	5081.601642	24.904410
147.777521	5091.829510	24.909427
147.757479	5090.973623	24.914445
148.122592	5078.115124	24.919463
147.966972	5094.924939	24.924480
148.442079	5103.644332	24.929498
148.280802	5110.678923	24.934515
148.415285	5113.541591	24.939533
149.160708	5129.368230	24.944551
148.859376	5145.214599	24.949568
149.291857	5148.015338	24.954586
148.943875	5156.696969	24.959603
148.973041	5148.601388	24.964621
149.401872	5166.343886	24.969639
149.475906	5167.317719	24.974656
150.014061	5169.372456	24.979674
150.030747	5176.836773	24.984691
150.161396	5183.596245	24.989709
150.366317	5191.403507	24.994727
150.616441	5203.624768	24.999744
150.714744	5203.082430	25.004762
150.792528	5205.871018	25.009779
150.928904	5199.488765	25.014797
151.084299	5214.857138	25.019815
150.849757	5224.418657	25.024832
151.030416	5224.959785	25.029850
151.289156	5230.828581	25.034867
151.551789	5245.793316	25.039885
152.276624	5255.185789	25.044903
151.999662	5252.924848	25.049920
152.233707	5256.968974	25.054938
151.962764	5256.275115	25.059955
152.388307	5265.133543	25.064973
152.641720	5274.129946	25.069991
152.751644	5277.358998	25.075008
152.876767	5272.393868	25.080026
152.895255	5269.790244	25.085043
152.782372	5280.067259	25.090061
153.599092	5285.686185	25.095079
153.439100	5295.233042	25.100096
153.541489	5299.829807	25.105114
153.280992	5303.725055	25.110131
153.372159	5310.806940	25.115149
153.761423	5321.196172	25.120167
153.665751	5326.930719	25.125184
154.026427	5348.891210	25.130202
153.986498	5365.882995	25.135219
154.106560	5370.342177	25.140237
154.448842	5386.194862	25.145255
154.225888	5399.569654	25.150272
154.724236	5405.806033	25.155290
155.083948	5420.616247	25.160307
155.429684	5414.328413	25.165325
155.530331	5422.841408	25.170343
155.906465	5440.689814	25.175360
155.987223	5439.136741	25.180378
156.165455	5440.331981	25.185395
156.079168	5438.864843	25.190413
156.455984	5433.187754	25.195431
156.401543	5452.863000	25.200448
156.576056	5462.406561	25.205466
156.840775	5476.138586	25.210483
157.007625	5469.854354	25.215501
157.133783	5482.468886	25.220519
157.065402	5494.550142	25.225536
157.425793	5494.459802	25.230554
157.494488	5498.104488	25.235571
157.603979	5510.767483	25.240589
157.693357	5511.470226	25.245607
157.606254	5530.860353	25.250624
158.198248	5530.507207	25.255642
158.377845	5547.506162	25.260659
158.372762	5547.114820	25.265677
158.851473	5552.016379	25.270695
158.939488	5575.044628	25.275712
159.402824	5574.208716	25.280730
159.767893	5580.438877	25.285747
159.485722	5590.358195	25.290765
159.739800	5570.926255	25.295783
159.817255	5581.399571	25.300800
159.961288	5584.005562	25.305818
160.092266	5603.838536	25.310835
159.971197	5608.325104	25.315853
160.454145	5608.089247	25.320871
160.303087	5613.981136	25.325888
160.635204	5636.320079	25.330906
160.834014	5642.080811	25.335923
160.609740	5643.242675	25.340941
160.875640	5648.974976	25.345959
160.922280	5665.935424	25.350976
161.370641	5668.015335	25.355994
161.636740	5681.902469	25.361011
161.658410	5700.801446	25.366029
162.010448	5699.823283	25.371047
162.240116	5708.445028	25.376064
161.999577	5695.322421	25.381082
162.360505	5699.700079	25.386099
162.306163	5716.033826	25.391117
162.763189	5719.826929	25.396135
162.893041	5715.683926	25.401152
162.958830	5727.882554	25.406170
163.423652	5742.042435	25.411187
163.121600	5753.358424	25.416205
163.462684	5749.037887	25.421223
163.237579	5761.506016	25.426240
163.317033	5770.069963	25.431258
163.782547	5775.366008	25.436275
163.767796	5788.665705	25.441293
164.307312	5804.363292	25.446311
164.213289	5817.161826	25.451328
164.582878	5815.125352	25.456346
164.728710	5818.840041	25.461363
164.601626	5841.527808	25.466381
165.211112	5841.991667	25.471399
164.944183	5842.204445	25.476416
165.154622	5870.077153	25.481434
165.480574	5873.534416	25.486451
165.647054	5875.162461	25.491469
166.058223	5875.700108	25.496487
166.264956	5894.830956	25.501504
166.377092	5890.415176	25.506522
166.763343	5888.824874	25.511539
166.779483	5883.079742	25.516557
167.152228	5892.382817	25.521575
167.556044	5905.184068	25.526592
167.664703	5919.916597	25.531610
168.044268	5918.091114	25.536627
167.713249	5922.870078	25.541645
167.742046	5911.190512	25.546663
167.920819	5917.009007	25.551680
168.132023	5915.012130	25.556698
168.353500	5910.371887	25.561715
168.202739	5930.640208	25.566733
168.292090	5928.680829	25.571751
168.586218	5943.192860	25.576768
168.517172	5955.796768	25.581786
168.802244	5960.259518	25.586803
168.761048	5966.881588	25.591821
169.215572	5980.236078	25.596839
168.771185	5992.133435	25.601856
169.108542	6010.071607	25.606874
169.582596	6021.916181	25.611891
169.587513	6034.611873	25.616909
169.674603	6054.744886	25.621927
170.060020	6061.131758	25.626944
170.240710	6075.058581	25.631962
170.299305	6092.736610	25.636979
170.243221	6111.386670	25.641997
170.641146	6116.532558	25.647015
170.820542	6125.560605	25.652032
171.160201	6145.759827	25.657050
171.646325	6146.823813	25.662067
171.636511	6152.484585	25.667085
172.072902	6160.140591	25.672103
172.105359	6164.613714	25.677120
172.575997	6175.265711	25.682138
173.035911	6174.407498	25.687156
172.855666	6174.887113	25.692173
173.053069	6165.250125	25.697191
172.773439	6170.010415	25.702208
172.973165	6192.591812	25.707226
173.557715	6191.157686	25.712244
173.470542	6197.878828	25.717261
173.591589	6198.633069	25.722279
173.718986	6208.914229	25.727296
173.725211	6227.286316	25.732314
174.321991	6224.715185	25.737332
174.441547	6224.700158	25.742349
174.739475	6231.715936	25.747367
175.042351	6246.074784	25.752384
175.242375	6248.585765	25.757402
175.383702	6247.973259	25.762420
175.127209	6252.131930	25.767437
175.439557	6243.365891	25.772455
175.817015	6251.779950	25.777472
175.686408	6254.107013	25.782490
175.936658	6251.358530	25.787508
175.916952	6272.164810	25.792525
176.031275	6273.220257	25.797543
176.076606	6276.216830	25.802560
176.032259	6296.706655	25.807578
176.361959	6298.985090	25.812596
176.484952	6310.994329	25.817613
176.868021	6332.928856	25.822631
176.867315	6336.594676	25.827648
177.016516	6349.900784	25.832666
177.765391	6362.289272	25.837684
177.724168	6365.758596	25.842701
177.935127	6367.979510	25.847719
178.178238	6371.745963	25.852736
178.588756	6389.271547	25.857754
178.476733	6390.562170	25.862772
178.298902	6395.990134	25.867789
178.443650	6408.387304	25.872807
178.857732	6426.417217	25.877824
179.001929	6436.139668	25.882842
179.251394	6442.883949	25.887860
179.208318	6453.628267	25.892877
179.552119	6458.962023	25.897895
179.924008	6469.606151	25.902912
180.042974	6477.670088	25.907930
180.539848	6472.538286	25.912948
180.470664	6489.970900	25.917965
180.624350	6505.102156	25.922983
181.093376	6502.597027	25.928000
180.946172	6508.525628	25.933018
181.334556	6524.497063	25.938036
181.375452	6528.314358	25.943053
181.535728	6532.026037	25.948071
181.436400	6539.926081	25.953088
181.674899	6563.131706	25.958106
182.103955	6554.019302	25.963124
182.126410	6580.512130	25.968141
182.351489	6592.142364	25.973159
182.785301	6598.483636	25.978176
182.652828	6599.641398	25.983194
182.885825	6608.529310	25.988212
183.258118	6620.647169	25.993229
183.252046	6628.455416	25.998247
183.617583	6639.481934	26.003264
183.475228	6657.046567	26.008282
184.015130	6652.473120	26.013300
184.378233	6662.243751	26.018317
184.320986	6667.172952	26.023335
184.730632	6677.907064	26.028352
184.556985	6686.239303	26.033370
184.994031	6695.827580	26.038388
184.743599	6707.854043	26.043405
185.139412	6711.147910	26.048423
185.721065	6710.655470	26.053440
185.533804	6736.902870	26.058458
185.577195	6724.175856	26.063476
185.802333	6735.405269	26.068493
185.753747	6758.642952	26.073511
186.222487	6766.167874	26.078528
186.438765	6764.974252	26.083546
187.058940	6782.711316	26.088564
186.765484	6787.162164	26.093581
187.009207	6786.030949	26.098599
187.500500	6794.013719	26.103616
186.859535	6803.392990	26.108634
187.252171	6816.613507	26.113652
187.622684	6822.349398	26.118669
187.608494	6830.968805	26.123687
188.281493	6842.711750	26.128704
188.180036	6844.577229	26.133722
187.827625	6850.434380	26.138740
188.321365	6866.359576	26.143757
188.765726	6869.346916	26.148775
188.969778	6891.628494	26.153792
188.933896	6907.426375	26.158810
189.482431	6908.466696	26.163828
189.505679	6919.878530	26.168845
189.483482	6935.045615	26.173863
190.104134	6938.355084	26.178880
190.017501	6959.085125	26.183898
190.293113	6963.575721	26.188916
190.688400	6973.590908	26.193933
190.871511	6981.650785	26.198951
191.331400	6989.523066	26.203968
191.367524	6994.190371	26.208986
191.569037	6992.242226	26.214004
191.744499	7002.957828	26.219021
192.108394	7022.883988	26.224039
192.133672	7023.721076	26.229056
191.851338	7028.858575	26.234074
192.482391	7036.368573	26.239092
192.504504	7057.639200	26.244109
192.426675	7054.974823	26.249127
192.692517	7067.573011	26.254144
193.014810	7074.103862	26.259162
193.394445	7072.420024	26.264180
193.494898	7087.486607	26.269197
193.561325	7103.366993	26.274215
193.825444	7101.984262	26.279232
193.838765	7127.959648	26.284250
193.794261	7126.500401	26.289268
194.331364	7138.823739	26.294285
194.591588	7165.045816	26.299303
195.017971	7171.363345	26.304320
194.637177	7166.587712	26.309338
194.879307	7190.546675	26.314356
195.551435	7193.282912	26.319373
195.688393	7213.517054	26.324391
195.795959	7211.905809	26.329408
195.936335	7235.258628	26.334426
196.468191	7231.128241	26.339444
196.582072	7250.745557	26.344461
197.142497	7255.671151	26.349479
197.339774	7248.342228	26.354496
197.120233	7254.865177	26.359514
197.153542	7275.290634	26.364532
196.965950	7282.074543	26.369549
197.227112	7301.137429	26.374567
197.526953	7308.509404	26.379584
197.866035	7318.499456	26.384602
198.197272	7335.109743	26.389620
198.287712	7346.045237	26.394637
198.413505	7356.711011	26.399655
198.850398	7361.001731	26.404672
198.949395	7377.322042	26.409690
199.002505	7378.596435	26.414708
199.434868	7397.252218	26.419725
199.185070	7410.202276	26.424743
199.389052	7418.249468	26.429760
199.629329	7435.452296	26.434778
199.680980	7439.575229	26.439796
200.433105	7458.047392	26.444813
200.429629	7474.367437	26.449831
200.568828	7467.915279	26.454848
200.656839	7489.873471	26.459866
201.121960	7489.701204	26.464884
201.265237	7499.092053	26.469901
201.552907	7503.214529	26.474919
201.707519	7521.123227	26.479936
201.955294	7538.460409	26.484954
202.011043	7531.907035	26.489972
202.279558	7540.001108	26.494989
202.392777	7548.819580	26.500007
202.512770	7548.650881	26.505024
202.616796	7571.398959	26.510042
202.773909	7580.253505	26.515060
203.187085	7592.889161	26.520077
203.535044	7600.138303	26.525095
203.612979	7605.610197	26.530112
203.905181	7630.000282	26.535130
204.136972	7632.623595	26.540148
204.349339	7637.072865	26.545165
204.389781	7666.798827	26.550183
204.625737	7660.879604	26.555200
204.858494	7685.497809	26.560218
205.283005	7700.916209	26.565236
205.592357	7688.473658	26.570253
205.745754	7715.730466	26.575271
205.912328	7727.807608	26.580288
205.621312	7737.608416	26.585306
206.027777	7743.827071	26.590324
206.370322	7753.863299	26.595341
206.602894	7773.181187	26.600359
207.053559	7776.585933	26.605376
207.391245	7782.496967	26.610394
207.409078	7773.713466	26.615412
207.906563	7779.427113	26.620429
208.155749	7799.429165	26.625447
208.316944	7804.181557	26.630464
208.630146	7808.574797	26.635482
208.627679	7803.899398	26.640500
209.168295	7797.728038	26.645517
208.779931	7809.161385	26.650535
209.037036	7812.537526	26.655552
209.289640	7828.320861	26.660570
209.453548	7833.113773	26.665588
209.666249	7848.076635	26.670605
209.730354	7862.059776	26.675623
209.894209	7866.933841	26.680640
210.060120	7878.108488	26.685658
210.656084	7887.664095	26.690676
210.948244	7880.699643	26.695693
211.331489	7903.129424	26.700711
211.236048	7918.040958	26.705728
211.166761	7918.378582	26.710746
211.357852	7926.830688	26.715764
211.579351	7934.373468	26.720781
211.993110	7949.350405	26.725799
212.041450	7956.104209	26.730816
212.187452	7974.945925	26.735834
212.205118	7987.798610	26.740852
212.749068	7999.414903	26.745869
212.684974	8000.023432	26.750887
212.895278	8011.602801	26.755904
213.171994	8021.980152	26.760922
213.237073	8039.437924	26.765940
213.690270	8049.884544	26.770957
213.756429	8063.948656	26.775975
213.841983	8075.917378	26.780992
213.983589	8086.102875	26.786010
214.433582	8100.130264	26.791028
214.804319	8109.608281	26.796045
214.792770	8130.182473	26.801063
215.017540	8125.753733	26.806080
215.186170	8147.178799	26.811098
215.124548	8153.454620	26.816116
215.542005	8172.739238	26.821133
215.522818	8180.788311	26.826151
215.801754	8201.214468	26.831168
216.184395	8219.152373	26.836186
216.419539	8237.307708	26.841204
217.353294	8239.072880	26.846221
217.539825	8248.540510	26.851239
217.415139	8254.454213	26.856256
217.882636	8269.743953	26.861274
217.812651	8269.698861	26.866292
218.353846	8270.036265	26.871309
218.076247	8297.936519	26.876327
218.235728	8299.396614	26.881344
218.741127	8315.033028	26.886362
218.994071	8339.900190	26.891380
219.164862	8333.959997	26.896397
219.111907	8345.454787	26.901415
219.433780	8358.127437	26.906432
219.768985	8369.910109	26.911450
220.120901	8396.752378	26.916468
220.602632	8396.870397	26.921485
220.375114	8404.261646	26.926503
220.756334	8424.528576	26.931520
220.938421	8423.499619	26.936538
221.072955	8431.003463	26.941556
221.766162	8448.564093	26.946573
221.828249	8453.963279	26.951591
222.037345	8450.315334	26.956608
222.288864	8456.601670	26.961626
222.435001	8472.062174	26.966644
222.806165	8472.301691	26.971661
222.605946	8490.674328	26.976679
222.714478	8502.467050	26.981696
222.925729	8515.025795	26.986714
223.040614	8536.024656	26.991732
223.582176	8543.174437	26.996749
223.546284	8563.287658	27.001767
223.826157	8567.472361	27.006784
224.149645	8581.383260	27.011802
224.292171	8601.838025	27.016820
224.539693	8614.345155	27.021837
224.599567	8634.589922	27.026855
224.740735	8643.537504	27.031872
225.886812	8652.121806	27.036890
225.926517	8667.654472	27.041908
226.255419	8659.802895	27.046925
226.360116	8675.973131	27.051943
226.601631	8684.339306	27.056960
226.969069	8688.483550	27.061978
226.984707	8705.052194	27.066996
227.297063	8704.716937	27.072013
227.509230	8714.301915	27.077031
227.637754	8716.237463	27.082048
227.610933	8737.288405	27.087066
227.783990	8750.750125	27.092084
227.859758	8746.754725	27.097101
228.138814	8769.744950	27.102119
228.442580	8774.607951	27.107136
228.672697	8792.429166	27.112154
228.863535	8812.467356	27.117172
229.044504	8810.912337	27.122189
228.986575	8834.409035	27.127207
229.282186	8842.214118	27.132224
229.558338	8850.136651	27.137242
229.653351	8871.087250	27.142260
230.000446	8884.998445	27.147277
230.200332	8897.394730	27.152295
230.603117	8923.645732	27.157312
231.147734	8940.409076	27.162330
231.022489	8944.282811	27.167348
231.525833	8947.611347	27.172365
231.753599	8961.658952	27.177383
231.644342	8967.961095	27.182400
232.024757	8988.052416	27.187418
232.182257	9004.983105	27.192436
232.149565	9021.044087	27.197453
232.872355	9016.995086	27.202471
233.057519	9052.820642	27.207488
233.299082	9060.173144	27.212506
233.127344	9075.433975	27.217524
233.549370	9081.960965	27.222541
234.042408	9101.873868	27.227559
234.247814	9123.472192	27.232576
234.532814	9121.034158	27.237594
234.832544	9150.385154	27.242612
234.954975	9147.515541	27.247629
235.323002	9164.042083	27.252647
235.231257	9192.965598	27.257664
235.774309	9182.276979	27.262682
235.812861	9211.691803	27.267700
236.251653	9211.818517	27.272717
236.387490	9232.371304	27.277735
236.619569	9251.706031	27.282752
236.963069	9258.476913	27.287770
237.000936	9269.458665	27.292788
237.484204	9288.390266	27.297805
237.689687	9295.193462	27.302823
237.682492	9316.034728	27.307840
237.996697	9317.398405	27.312858
238.222228	9340.911158	27.317876
238.327673	9336.968208	27.322893
238.657435	9361.685594	27.327911
238.792851	9381.921952	27.332928
239.475075	9387.507919	27.337946
239.746029	9395.831781	27.342964
239.941904	9414.165116	27.347981
240.216206	9430.664120	27.352999
240.375597	9435.644182	27.358016
240.572562	9439.876715	27.363034
240.454490	9446.598034	27.368052
240.465345	9468.182547	27.373069
240.827517	9483.863513	27.378087
240.982549	9507.262133	27.383104
241.420460	9509.860306	27.388122
241.620891	9540.767016	27.393140
241.862486	9549.845799	27.398157
242.345715	9569.337073	27.403175
242.767189	9574.660604	27.408192
243.244228	9590.926114	27.413210
243.189158	9616.629318	27.418228
243.419312	9618.783705	27.423245
243.879610	9632.005608	27.428263
244.017417	9651.020820	27.433280
244.193417	9650.473353	27.438298
244.373630	9674.668455	27.443316
244.650630	9677.355528	27.448333
244.694007	9683.821759	27.453351
244.611115	9701.401160	27.458368
245.132356	9706.566416	27.463386
245.122744	9735.539548	27.468404
245.213486	9740.312058	27.473421
245.468314	9762.229213	27.478439
245.963669	9781.721103	27.483456
246.354154	9791.233881	27.488474
246.622417	9812.591113	27.493492
246.844772	9827.049246	27.498509
247.194868	9830.880750	27.503527
247.286448	9851.465289	27.508544
247.748856	9856.399264	27.513562
247.916114	9870.859466	27.518580
248.248440	9891.564920	27.523597
248.365825	9896.515051	27.528615
248.563234	9915.253641	27.533632
249.018559	9919.751571	27.538650
249.255414	9943.849467	27.543668
249.374951	9943.625676	27.548685
249.827360	9966.751214	27.553703
249.993333	9978.533150	27.558720
250.190310	9983.403957	27.563738
250.456757	9997.784042	27.568756
250.788501	10009.482627	27.573773
251.280277	10022.289977	27.578791
251.032156	10051.418966	27.583808
251.665709	10054.366940	27.588826
251.884265	10074.432056	27.593844
251.877698	10080.276456	27.598861
252.268951	10086.252752	27.603879
252.525597	10102.399274	27.608896
253.081092	10115.402561	27.613914
252.742188	10138.257540	27.618932
253.299975	10159.122976	27.623949
253.562786	10167.526582	27.628967
253.555655	10184.760719	27.633984
254.183565	10190.047923	27.639002
254.239983	10201.183231	27.644020
254.140064	10225.876957	27.649037
254.682449	10238.639076	27.654055
254.833578	10262.864299	27.659072
255.002252	10279.021622	27.664090
255.453089	10292.741184	27.669108
255.621240	10306.340529	27.674125
256.343091	10310.095646	27.679143
256.591631	10335.500785	27.684160
256.687573	10350.283630	27.689178
256.936256	10357.275510	27.694196
257.189112	10377.101340	27.699213
257.668245	10394.408840	27.704231
257.689902	10398.672221	27.709248
257.848255	10412.593928	27.714266
258.018616	10429.713073	27.719284
258.213892	10441.964778	27.724301
258.925895	10453.155614	27.729319
258.822544	10468.520680	27.734336
259.201818	10480.062051	27.739354
259.955076	10480.949783	27.744372
259.498508	10502.003263	27.749389
260.138410	10511.023752	27.754407
260.313597	10535.200495	27.759424
260.421372	10541.475995	27.764442
260.819662	10547.197613	27.769460
260.904994	10574.707691	27.774477
261.219089	10577.900090	27.779495
261.146656	10600.691918	27.784512
261.837427	10614.859719	27.789530
262.159525	10631.630156	27.794548
262.077667	10643.319668	27.799565
262.344657	10664.092082	27.804583
262.325502	10676.716660	27.809600
262.671934	10692.057122	27.814618
262.970901	10699.180279	27.819636
262.880105	10726.965579	27.824653
263.745312	10741.998045	27.829671
263.729877	10757.286592	27.834688
264.194039	10767.455070	27.839706
264.411914	10792.089967	27.844724
264.608816	10803.326919	27.849741
265.176591	10820.294820	27.854759
265.137246	10833.658722	27.859776
265.307147	10853.082879	27.864794
265.851949	10860.322987	27.869812
265.819961	10878.343536	27.874829
266.494784	10878.551748	27.879847
266.629865	10919.287093	27.884864
266.766145	10926.438855	27.889882
267.638484	10934.366949	27.894900
267.645944	10954.714705	27.899917
268.054560	10965.410917	27.904935
268.148524	10970.908884	27.909952
268.265918	10981.933792	27.914970
268.898447	11001.060949	27.919988
269.104038	11009.357863	27.925005
269.170428	11023.750708	27.930023
269.676545	11038.220475	27.935040
269.437571	11052.652859	27.940058
270.265469	11064.880687	27.945076
270.186353	11084.064283	27.950093
270.732138	11096.704404	27.955111
270.733156	11117.874394	27.960128
271.016799	11129.719635	27.965146
271.618744	11129.430949	27.970164
271.520814	11168.180658	27.975181
272.037386	11172.247294	27.980199
272.017551	11184.624987	27.985216
272.157463	11201.925688	27.990234
272.723869	11221.645506	27.995252
272.655952	11247.327432	28.000269
273.047800	11255.670856	28.005287
273.167806	11286.211317	28.010304
273.438851	11300.707624	28.015322
273.774614	11312.452978	28.020340
273.899225	11338.891063	28.025357
274.452392	11361.916050	28.030375
274.695019	11392.174837	28.035392
275.122650	11408.730068	28.040410
275.389740	11421.561546	28.045428
275.209657	11439.506383	28.050445
275.843235	11452.616015	28.055463
276.337366	11468.834115	28.060480
276.242958	11489.153707	28.065498
276.792090	11504.574848	28.070516
276.873642	11529.526530	28.075533
277.395696	11536.329492	28.080551
277.603940	11558.822509	28.085568
277.596118	11576.305642	28.090586
277.967350	11591.636553	28.095604
278.201608	11619.895896	28.100621
278.487061	11634.446846	28.105639
278.665034	11659.225189	28.110656
278.870043	11675.926273	28.115674
279.406211	11692.645047	28.120692
279.439396	11719.837938	28.125709
279.856876	11740.296879	28.130727
280.347769	11758.088460	28.135744
280.405712	11776.347251	28.140762
280.787625	11788.595875	28.145780
280.919106	11807.028474	28.150797
281.378137	11823.288984	28.155815
281.421853	11835.324158	28.160832
281.708835	11859.541107	28.165850
282.227061	11869.294774	28.170868
282.338377	11896.728735	28.175885
282.672623	11908.087122	28.180903
283.087981	11922.675136	28.185920
283.521298	11949.007965	28.190938
284.229938	11956.840753	28.195956
284.346207	11965.915644	28.200973
284.536980	11972.267785	28.205991
284.708720	11987.181405	28.211008
284.740621	12002.431775	28.216026
284.907916	12012.746305	28.221044
285.269685	12041.803135	28.226061
285.422974	12044.920017	28.231079
286.043962	12066.147786	28.236096
285.972223	12089.631809	28.241114
286.454717	12106.446568	28.246132
286.613714	12134.924126	28.251149
286.835325	12143.568809	28.256167
287.361653	12161.985308	28.261184
287.219085	12185.816848	28.266202
287.780720	12200.711829	28.271220
288.313586	12234.611638	28.276237
288.381944	12251.624315	28.281255
288.836535	12260.433784	28.286272
288.855878	12285.932717	28.291290
289.218756	12300.870143	28.296308
289.674277	12330.148351	28.301325
290.069823	12344.445338	28.306343
290.480637	12367.544173	28.311360
290.720674	12383.882468	28.316378
291.132327	12395.174806	28.321396
291.078488	12419.794119	28.326413
291.581150	12438.006835	28.331431
291.789819	12453.338681	28.336448
292.106009	12475.479441	28.341466
292.673885	12488.129606	28.346484
292.726794	12503.165801	28.351501
292.842840	12521.849179	28.356519
293.124353	12544.485872	28.361536
293.427807	12564.373772	28.366554
293.987559	12578.163142	28.371572
293.796046	12609.405344	28.376589
294.554799	12623.921393	28.381607
294.858073	12640.574113	28.386624
294.798110	12667.765096	28.391642
295.181636	12682.092737	28.396660
295.586997	12705.489224	28.401677
295.861000	12722.427382	28.406695
296.370033	12743.302658	28.411712
296.629667	12757.904593	28.416730
296.816358	12774.135493	28.421748
296.922664	12792.094301	28.426765
297.194228	12813.848932	28.431783
297.797894	12834.407663	28.436800
297.898466	12847.962811	28.441818
298.335536	12870.747561	28.446836
298.252508	12893.766565	28.451853
298.867177	12909.794385	28.456871
299.125871	12925.827561	28.461888
299.111558	12948.674524	28.466906
299.670828	12970.408535	28.471924
300.138158	13001.640145	28.476941
300.336427	13010.872249	28.481959
300.854685	13016.355840	28.486976
300.739019	13036.931454	28.491994
301.163137	13041.510292	28.497012
301.336281	13063.424957	28.502029
301.514705	13086.602677	28.507047
302.099730	13097.907784	28.512064
302.258062	13117.517802	28.517082
302.782759	13126.027744	28.522100
302.564562	13160.643199	28.527117
302.838916	13184.413495	28.532135
303.420511	13196.770395	28.537152
303.459098	13226.008910	28.542170
303.342902	13240.200698	28.547188
303.704267	13276.799152	28.552205
304.398388	13302.292001	28.557223
305.345939	13316.958661	28.562240
305.609219	13342.505548	28.567258
305.918692	13358.418852	28.572276
306.377134	13379.512923	28.577293
306.432288	13391.794781	28.582311
306.696972	13403.239802	28.587328
306.884858	13437.318992	28.592346
306.969827	13450.253139	28.597364
307.526141	13471.238147	28.602381
307.917351	13494.408020	28.607399
308.202754	13518.375546	28.612416
308.196624	13541.598643	28.617434
308.812188	13551.698117	28.622452
308.654354	13580.750715	28.627469
308.825095	13602.488415	28.632487
309.603078	13625.977423	28.637504
309.894533	13654.193010	28.642522
310.380015	13677.925928	28.647540
310.671275	13698.296334	28.652557
311.110855	13720.364781	28.657575
311.442962	13741.760759	28.662592
311.471750	13761.419783	28.667610
311.901721	13778.408874	28.672628
312.226531	13799.686359	28.677645
312.109576	13825.717730	28.682663
312.767145	13848.204160	28.687680
312.882240	13880.487064	28.692698
313.318813	13895.624945	28.697716
313.815889	13921.606847	28.702733
313.906849	13938.563958	28.707751
314.203641	13963.337174	28.712768
314.729287	13998.731192	28.717786
315.228454	14008.137854	28.722804
315.817409	14030.330143	28.727821
316.278548	14061.432423	28.732839
316.577289	14059.945678	28.737856
316.510166	14084.084280	28.742874
317.016413	14087.403183	28.747892
317.071278	14108.591787	28.752909
317.226093	14127.647259	28.757927
317.708569	14149.420772	28.762944
317.691324	14176.870392	28.767962
318.243688	14191.760858	28.772980
318.817585	14211.555575	28.777997
318.961267	14232.151230	28.783015
319.293676	14246.088395	28.788032
319.326179	14264.113046	28.793050
320.101451	14274.539574	28.798068
320.678047	14310.375009	28.803085
320.479430	14320.880801	28.808103
321.015509	14346.407748	28.813120
321.076513	14363.567264	28.818138
321.558359	14380.244217	28.823156
322.160677	14387.654495	28.828173
322.088953	14423.233412	28.833191
322.647392	14429.580824	28.838208
322.591263	14446.160909	28.843226
322.956702	14464.838331	28.848244
323.457496	14483.635217	28.853261
323.580663	14498.753032	28.858279
323.581751	14517.906901	28.863296
323.845807	14553.662208	28.868314
324.532503	14568.978392	28.873332
324.895343	14595.751133	28.878349
324.937624	14619.084374	28.883367
325.391916	14639.521958	28.888384
325.491883	14663.283866	28.893402
325.747463	14685.696136	28.898420
326.434445	14706.818718	28.903437
326.176424	14734.660589	28.908455
326.814789	14757.105744	28.913472
327.046515	14789.634342	28.918490
327.407807	14812.853591	28.923508
328.225761	14836.600938	28.928525
328.304858	14864.199675	28.933543
328.764476	14889.675504	28.938560
329.137617	14916.506956	28.943578
329.192414	14940.202663	28.948596
329.823399	14954.365258	28.953613
329.923495	14991.031279	28.958631
330.303533	15007.096850	28.963648
330.550115	15040.121539	28.968666
330.719382	15067.163507	28.973684
331.418870	15094.281680	28.978701
331.474034	15121.894267	28.983719
331.834529	15152.244547	28.988736
332.084988	15175.087042	28.993754
332.396881	15203.382298	28.998772
333.101127	15231.607936	29.003789
333.488015	15262.858758	29.008807
333.857671	15277.101136	29.013824
333.882924	15314.101797	29.018842
334.394427	15329.821239	29.023860
335.086364	15350.836654	29.028877
335.072737	15387.817121	29.033895
335.774984	15412.381990	29.038912
336.056424	15424.705150	29.043930
336.256652	15444.771258	29.048948
336.241244	15478.700774	29.053965
336.564789	15500.373142	29.058983
337.334150	15523.874191	29.064000
337.722109	15544.254531	29.069018
338.071473	15568.176642	29.074036
338.466159	15570.223431	29.079053
339.233404	15595.186046	29.084071
339.256648	15606.964163	29.089088
339.478232	15636.044285	29.094106
339.675644	15659.585023	29.099124
340.267336	15670.739506	29.104141
340.365434	15697.028261	29.109159
340.786351	15710.925229	29.114176
341.290499	15737.022326	29.119194
340.978934	15757.799268	29.124212
341.600081	15784.063066	29.129229
342.116473	15817.485994	29.134247
342.687014	15830.035869	29.139264
342.755487	15854.898591	29.144282
342.737752	15881.334483	29.149300
343.248520	15899.486677	29.154317
343.199110	15926.162738	29.159335
343.755965	15958.816371	29.164352
344.358675	15980.767869	29.169370
344.398567	16011.086103	29.174388
344.474976	16022.009288	29.179405
344.831975	16046.523488	29.184423
345.026025	16082.355174	29.189440
345.278267	16102.528539	29.194458
345.656542	16138.251046	29.199476
346.403547	16168.058479	29.204493
346.382404	16204.608555	29.209511
347.326781	16225.094677	29.214528
347.977704	16248.603756	29.219546
348.162255	16273.441591	29.224564
348.723011	16292.864277	29.229581
348.368716	16318.629923	29.234599
348.843959	16346.075730	29.239616
349.375951	16371.390557	29.244634
349.607343	16397.929482	29.249652
349.979212	16416.701058	29.254669
350.092551	16453.128544	29.259687
350.850246	16480.348134	29.264704
350.842618	16504.885532	29.269722
351.026011	16543.301901	29.274740
351.660693	16562.212993	29.279757
352.105114	16596.763833	29.284775
352.589551	16618.440993	29.289792
353.094648	16647.151261	29.294810
353.110237	16681.234165	29.299828
353.698587	16696.887028	29.304845
353.856218	16729.939279	29.309863
354.382402	16751.781520	29.314880
355.060749	16776.268840	29.319898
355.011188	16803.806993	29.324916
355.351705	16827.295762	29.329933
355.876837	16861.280518	29.334951
356.407981	16882.646070	29.339968
356.722002	16901.561757	29.344986
356.727096	16936.532803	29.350004
357.347723	16947.385446	29.355021
357.522630	16984.136510	29.360039
357.827774	17004.046858	29.365056
358.284299	17039.450980	29.370074
358.321371	17076.444169	29.375092
358.953459	17093.100590	29.380109
359.236839	17130.497656	29.385127
359.588243	17163.699979	29.390144
360.349464	17187.400217	29.395162
360.658668	17205.800014	29.400180
360.766985	17233.079453	29.405197
361.208992	17270.527822	29.410215
361.402053	17298.468015	29.415232
361.923314	17324.932078	29.420250
362.052199	17346.925981	29.425268
362.689015	17373.690995	29.430285
362.955547	17401.965999	29.435303
363.418538	17434.144685	29.440320
363.738742	17459.686969	29.445338
363.942126	17489.241537	29.450356
364.665680	17509.028073	29.455373
364.787483	17539.518402	29.460391
365.267235	17571.867981	29.465408
365.794843	17600.554108	29.470426
365.948467	17617.974388	29.475444
366.566096	17650.194109	29.480461
366.477157	17665.993087	29.485479
366.810303	17695.734628	29.490496
367.379794	17715.917357	29.495514
367.264357	17754.133764	29.500532
368.099074	17777.228389	29.505549
368.412653	17817.774773	29.510567
368.474794	17833.402302	29.515584
368.885913	17861.297895	29.520602
369.549788	17899.019935	29.525620
369.933026	17918.366718	29.530637
369.988349	17943.048731	29.535655
370.345453	17972.763156	29.540672
371.074994	17987.195811	29.545690
371.357746	18030.210158	29.550708
371.572696	18048.646981	29.555725
371.902686	18082.548305	29.560743
372.108473	18115.029410	29.565760
372.849715	18144.491398	29.570778
372.954480	18183.556716	29.575796
373.551811	18195.774491	29.580813
373.802544	18232.999728	29.585831
374.089067	18264.559740	29.590848
374.500246	18294.942080	29.595866
374.714040	18332.068030	29.600884
375.183531	18351.416807	29.605901
375.419868	18386.975322	29.610919
375.546475	18425.856302	29.615936
376.510340	18458.925169	29.620954
376.793974	18493.432475	29.625972
377.135696	18520.118907	29.630989
377.317518	18560.167096	29.636007
377.480783	18591.431258	29.641024
378.379095	18624.318975	29.646042
378.650355	18663.682613	29.651060
379.224951	18692.807412	29.656077
379.752587	18729.349459	29.661095
379.886140	18764.262093	29.666112
380.368302	18787.758568	29.671130
380.724697	18823.214589	29.676148
381.144793	18851.455604	29.681165
381.668864	18891.492088	29.686183
381.719402	18917.680304	29.691200
382.478482	18939.032853	29.696218
382.785273	18972.336028	29.701236
383.098716	19002.272342	29.706253
383.621327	19029.673759	29.711271
384.033820	19061.936470	29.716288
384.050103	19083.156740	29.721306
384.574065	19126.089848	29.726324
385.010945	19147.445540	29.731341
385.590412	19180.727651	29.736359
385.385500	19212.798021	29.741376
386.278975	19237.426791	29.746394
386.639500	19269.044245	29.751412
386.791018	19305.022340	29.756429
387.318189	19341.829084	29.761447
387.675870	19375.201889	29.766464
388.306569	19400.686304	29.771482
388.426599	19433.895182	29.776500
389.073723	19467.727916	29.781517
389.541705	19491.662855	29.786535
389.783022	19528.657630	29.791552
390.323508	19542.268439	29.796570
390.635527	19593.714935	29.801588
391.261353	19613.662045	29.806605
391.578624	19625.361238	29.811623
391.795078	19662.010426	29.816640
392.321632	19672.937187	29.821658
392.903399	19702.136659	29.826676
393.286762	19734.000308	29.831693
393.453930	19755.064027	29.836711
393.425191	19782.835401	29.841728
393.888139	19812.021620	29.846746
394.354891	19833.048470	29.851764
394.562004	19864.525319	29.856781
395.104602	19900.521953	29.861799
395.178357	19927.967595	29.866816
396.005516	19945.797535	29.871834
396.193845	19977.299776	29.876852
396.559395	20013.480459	29.881869
396.930021	20036.377547	29.886887
396.903299	20075.311378	29.891904
397.713882	20105.009730	29.896922
398.012070	20142.608168	29.901940
398.015682	20185.587537	29.906957
398.659927	20207.864115	29.911975
398.884086	20255.062441	29.916992
399.798124	20272.452665	29.922010
399.959099	20316.651855	29.927028
400.334294	20350.053657	29.932045
401.020910	20378.603152	29.937063
400.957487	20415.948297	29.942080
401.607437	20452.926358	29.947098
402.178803	20490.586000	29.952116
402.629658	20521.517641	29.957133
403.162621	20558.414389	29.962151
403.156844	20592.773679	29.967168
403.859131	20617.729382	29.972186
404.429729	20648.737617	29.977204
404.665199	20693.029525	29.982221
405.236614	20714.815876	29.987239
405.146353	20756.074755	29.992256
406.009578	20779.570879	29.997274
406.561919	20815.884772	30.002292
406.792596	20840.922008	30.007309
407.586472	20880.830299	30.012327
407.624849	20911.720551	30.017344
408.241644	20932.828010	30.022362
408.724627	20963.357823	30.027380
408.964251	20995.775842	30.032397
409.109797	21027.258748	30.037415
409.450844	21061.785485	30.042432
410.082299	21097.758942	30.047450
410.128600	21134.857320	30.052468
410.802053	21176.066520	30.057485
411.691357	21203.393464	30.062503
411.777603	21242.923057	30.067520
412.461306	21269.569884	30.072538
412.786233	21310.796096	30.077556
412.677558	21331.858558	30.082573
413.385666	21353.649920	30.087591
413.840049	21396.860506	30.092608
414.365813	21425.868845	30.097626
414.391870	21458.811881	30.102644
414.502035	21495.017512	30.107661
415.521550	21529.286291	30.112679
415.575807	21569.034798	30.117696
416.140169	21605.559687	30.122714
416.741774	21641.104061	30.127732
416.991432	21681.985713	30.132749
417.795471	21712.165745	30.137767
417.987109	21752.119000	30.142784
418.481171	21774.536036	30.147802
419.069032	21805.193502	30.152820
419.260126	21849.008565	30.157837
419.784311	21873.248219	30.162855
420.031773	21915.865244	30.167872
420.288952	21943.443062	30.172890
420.731252	21975.750580	30.177908
420.801732	22014.250215	30.182925
421.486549	22044.221938	30.187943
421.793635	22082.310452	30.192960
422.447754	22111.022790	30.197978
422.900510	22140.440213	30.202996
423.168355	22181.583385	30.208013
423.551758	22211.103862	30.213031
423.966247	22243.698741	30.218048
424.210643	22288.097419	30.223066
424.532401	22318.982762	30.228084
424.786255	22358.160819	30.233101
425.258213	22390.292347	30.238119
425.569933	22441.664005	30.243136
426.097920	22480.467423	30.248154
426.580097	22517.096181	30.253172
427.316079	22564.977863	30.258189
427.831386	22596.955965	30.263207
428.178024	22631.863421	30.268224
428.698721	22668.142380	30.273242
429.201082	22709.355247	30.278260
429.427123	22740.670331	30.283277
429.868391	22779.055149	30.288295
430.387837	22815.640540	30.293312
430.917753	22860.972692	30.298330
431.108617	22891.738821	30.303348
431.753141	22936.645378	30.308365
432.176296	22967.969260	30.313383
432.405201	23020.518524	30.318400
432.737240	23056.786957	30.323418
433.262942	23088.702766	30.328436
433.646305	23132.382092	30.333453
433.998648	23177.362867	30.338471
434.650476	23220.968033	30.343488
435.100192	23255.525411	30.348506
435.766405	23296.838738	30.353524
436.231956	23340.325231	30.358541
436.788021	23374.354333	30.363559
436.980623	23415.121867	30.368576
437.370155	23453.944113	30.373594
438.116990	23492.969087	30.378612
438.452092	23533.724362	30.383629
439.099429	23559.075124	30.388647
439.432528	23598.394306	30.393664
439.743858	23634.900783	30.398682
440.611170	23669.585435	30.403700
440.776749	23711.034652	30.408717
441.387774	23730.370929	30.413735
441.756358	23770.745918	30.418752
441.829482	23795.510814	30.423770
442.354928	23830.416369	30.428788
442.905097	23874.849008	30.433805
443.415555	23906.899760	30.438823
443.624487	23952.183854	30.443840
444.243066	23991.732669	30.448858
444.945300	24015.923844	30.453876
445.035696	24067.737577	30.458893
445.775404	24086.772264	30.463911
446.079275	24132.523679	30.468928
446.525463	24174.712919	30.473946
447.124179	24203.781747	30.478964
447.174170	24247.140617	30.483981
447.966062	24288.124883	30.488999
448.298420	24319.966181	30.494016
448.587380	24353.798582	30.499034
449.173949	24391.057511	30.504052
449.322525	24432.874000	30.509069
450.075687	24467.352078	30.514087
450.246308	24506.452646	30.519104
450.544916	24548.364442	30.524122
451.593856	24582.825348	30.529140
451.602469	24613.768246	30.534157
452.071760	24647.347449	30.539175
452.504747	24685.111848	30.544192
452.601807	24726.518089	30.549210
453.423735	24756.235351	30.554228
453.639842	24805.213927	30.559245
454.320674	24843.833421	30.564263
454.695013	24881.768817	30.569280
454.774560	24918.229649	30.574298
455.535771	24955.574454	30.579316
455.814431	24999.919317	30.584333
456.828508	25031.797371	30.589351
456.761615	25076.297390	30.594368
457.644599	25103.516546	30.599386
458.269941	25145.848855	30.604404
458.648918	25190.196534	30.609421
458.975367	25224.472337	30.614439
459.640434	25259.843445	30.619456
459.570561	25294.475154	30.624474
460.578870	25329.054684	30.629492
460.868198	25374.190445	30.634509
461.632111	25411.002739	30.639527
462.009801	25450.919669	30.644544
462.033966	25488.668324	30.649562
462.747823	25520.937623	30.654580
462.858495	25561.709626	30.659597
463.596523	25608.187994	30.664615
464.264993	25638.111973	30.669632
464.505066	25679.733410	30.674650
465.104346	25724.512839	30.679668
465.421654	25770.263240	30.684685
465.986466	25802.062513	30.689703
466.232983	25863.012644	30.694720
466.591363	25906.791500	30.699738
467.295377	25942.498231	30.704756
467.433116	25997.407454	30.709773
467.931407	26037.144917	30.714791
468.603497	26080.793445	30.719808
468.996861	26131.352007	30.724826
469.688614	26174.783026	30.729844
469.748002	26218.145307	30.734861
470.182638	26263.076399	30.739879
470.870524	26303.745177	30.744896
471.288679	26356.069886	30.749914
472.209373	26398.999895	30.754932
472.509427	26454.132906	30.759949
472.786601	26496.141316	30.764967
473.086819	26539.679050	30.769984
473.524484	26578.276436	30.775002
474.343892	26628.598770	30.780020
475.041285	26667.516135	30.785037
475.100642	26706.933469	30.790055
475.772637	26752.690870	30.795072
476.401790	26800.546876	30.800090
477.283962	26838.430938	30.805108
477.503890	26883.913347	30.810125
477.976138	26929.272107	30.815143
478.433441	26965.469715	30.820160
478.513951	27014.559017	30.825178
479.281228	27056.153312	30.830196
479.403346	27099.264523	30.835213
480.125719	27136.652035	30.840231
480.505965	27189.070707	30.845248
480.912711	27235.065700	30.850266
481.547141	27278.313399	30.855284
481.931413	27321.280837	30.860301
482.480005	27352.170835	30.865319
482.947914	27398.692413	30.870336
483.246002	27437.816386	30.875354
483.915118	27470.084120	30.880372
484.270000	27527.539542	30.885389
484.951915	27560.243812	30.890407
485.359413	27593.927309	30.895424
485.605841	27652.186581	30.900442
486.090066	27682.154057	30.905460
486.846393	27728.726588	30.910477
487.014043	27778.469252	30.915495
487.520093	27827.487282	30.920512
487.892784	27871.558964	30.925530
488.583297	27908.682115	30.930548
488.775504	27956.389634	30.935565
489.392817	28012.992489	30.940583
489.697960	28049.917872	30.945600
490.166149	28108.678271	30.950618
490.595081	28156.744657	30.955636
491.304240	28208.316996	30.960653
491.743062	28272.095620	30.965671
492.106862	28305.036905	30.970688
492.588372	28358.171084	30.975706
493.384857	28414.281852	30.980724
493.999285	28464.094508	30.985741
494.267144	28517.879702	30.990759
494.833740	28569.994081	30.995776
495.261024	28621.216784	31.000794
495.890041	28660.765118	31.005812
496.536666	28714.563958	31.010829
496.841159	28768.962202	31.015847
497.352851	28809.959411	31.020864
497.655655	28875.071990	31.025882
498.356975	28926.900138	31.030900
498.935832	28981.080128	31.035917
499.319383	29030.162823	31.040935
499.676308	29088.414916	31.045952
500.049908	29146.181750	31.050970
500.817809	29189.547774	31.055988
501.403596	29249.229550	31.061005
501.993075	29315.469949	31.066023
502.497765	29352.876163	31.071040
502.824582	29399.366485	31.076058
503.380120	29460.928007	31.081076
503.910978	29507.769755	31.086093
504.569829	29575.548731	31.091111
505.166452	29617.874632	31.096128
505.607880	29662.898566	31.101146
506.322960	29713.597294	31.106164
506.971988	29767.657684	31.111181
507.404476	29799.697562	31.116199
508.000606	29849.340515	31.121216
508.344509	29899.858263	31.126234
509.020689	29941.408272	31.131252
509.914070	29988.005174	31.136269
510.036885	30044.011792	31.141287
510.796550	30074.351111	31.146304
510.827940	30131.549963	31.151322
511.129441	30177.096867	31.156340
511.647836	30229.754213	31.161357
512.142393	30285.277310	31.166375
512.591952	30324.726586	31.171392
512.825053	30378.630514	31.176410
513.522804	30427.176090	31.181428
514.376041	30481.397350	31.186445
514.844949	30532.789129	31.191463
515.640367	30572.462539	31.196480
515.945605	30623.553532	31.201498
516.413742	30667.326189	31.206516
517.182332	30715.845066	31.211533
517.352608	30766.302532	31.216551
517.949380	30811.515102	31.221568
518.073465	30856.976379	31.226586
518.832859	30899.294213	31.231604
519.426850	30954.645210	31.236621
519.754094	31002.143051	31.241639
520.641130	31045.175277	31.246656
520.611276	31091.410413	31.251674
521.086487	31146.712252	31.256692
521.734212	31189.569873	31.261709
522.144437	31241.333124	31.266727
522.579760	31291.685131	31.271744
522.715640	31361.491690	31.276762
523.394921	31413.147820	31.281780
524.114897	31475.578970	31.286797
524.503851	31536.556881	31.291815
525.249866	31583.365401	31.296832
525.724686	31644.077051	31.301850
526.342171	31707.680824	31.306868
527.145150	31755.972845	31.311885
527.868705	31810.607757	31.316903
528.043671	31866.611527	31.321920
528.922389	31920.397558	31.326938
528.933089	31966.426325	31.331956
529.675017	32028.253117	31.336973
530.168206	32087.697940	31.341991
530.791766	32134.288370	31.347008
531.357403	32197.173583	31.352026
531.752741	32255.382459	31.357044
532.486282	32307.073243	31.362061
533.169705	32366.269798	31.367079
533.552761	32419.590311	31.372096
534.421990	32475.809297	31.377114
534.350706	32526.936530	31.382132
535.297054	32570.407581	31.387149
535.437384	32639.890263	31.392167
536.012663	32695.546417	31.397184
536.564217	32757.732267	31.402202
537.508868	32803.955778	31.407220
538.015297	32870.081266	31.412237
538.064414	32926.342707	31.417255
538.590308	32979.448777	31.422272
539.026999	33039.313198	31.427290
539.631476	33107.676417	31.432308
540.413921	33173.432338	31.437325
541.279038	33221.228953	31.442343
541.750819	33275.108511	31.447360
542.362095	33341.022753	31.452378
542.859940	33401.149654	31.457396
543.634201	33452.306886	31.462413
543.849930	33510.060461	31.467431
544.417090	33558.238622	31.472448
544.868240	33619.248100	31.477466
545.393052	33675.947570	31.482484
546.281724	33727.752510	31.487501
546.245181	33789.240876	31.492519
547.265148	33848.405613	31.497536
547.458474	33907.650515	31.502554
548.284583	33964.076992	31.507572
548.534438	34019.870018	31.512589
548.954173	34085.638822	31.517607
550.033787	34138.410577	31.522624
550.420033	34200.717171	31.527642
550.755871	34258.964524	31.532660
551.414837	34312.803619	31.537677
551.964924	34373.619420	31.542695
552.976130	34423.086592	31.547712
553.355573	34474.283675	31.552730
553.824201	34525.642873	31.557748
554.749377	34576.103009	31.562765
554.706168	34621.304931	31.567783
555.637613	34669.151256	31.572800
555.847501	34722.832352	31.577818
556.148775	34773.658207	31.582836
556.902487	34822.146586	31.587853
557.215503	34885.411281	31.592871
557.945519	34931.909356	31.597888
558.232046	34999.969487	31.602906
558.434879	35059.387038	31.607924
559.420916	35117.946183	31.612941
559.696062	35187.422761	31.617959
560.229974	35246.883988	31.622976
560.871494	35311.225658	31.627994
561.356647	35388.277289	31.633012
562.179424	35440.268510	31.638029
562.811522	35508.822530	31.643047
563.438971	35570.989820	31.648064
564.089528	35639.250929	31.653082
564.537567	35701.385233	31.658100
565.166467	35758.806264	31.663117
565.438967	35825.912399	31.668135
566.231520	35891.424141	31.673152
567.008671	35956.929201	31.678170
567.333788	36021.404660	31.683188
567.948800	36082.613166	31.688205
568.232090	36147.771399	31.693223
569.001107	36207.705031	31.698240
569.872593	36279.195434	31.703258
570.269247	36340.526158	31.708276
570.730669	36399.523445	31.713293
571.081554	36474.708237	31.718311
571.924992	36543.452151	31.723328
572.835588	36608.009579	31.728346
573.402510	36677.822358	31.733364
574.136840	36737.570958	31.738381
574.277443	36804.626796	31.743399
574.943181	36855.713837	31.748416
575.725866	36929.055272	31.753434
576.286737	36999.416322	31.758452
577.010713	37056.800496	31.763469
577.396147	37123.804381	31.768487
577.774713	37182.982054	31.773504
578.753630	37251.393768	31.778522
579.269598	37325.989799	31.783540
579.739899	37384.692131	31.788557
580.646781	37446.949047	31.793575
580.941650	37507.079055	31.798592
581.781175	37563.281022	31.803610
581.872544	37629.293826	31.808628
582.653992	37692.566593	31.813645
583.015406	37760.318546	31.818663
583.855320	37825.545375	31.823680
584.546517	37891.702933	31.828698
584.733915	37962.410421	31.833716
585.280970	38021.285180	31.838733
585.806359	38092.679015	31.843751
586.679501	38158.766406	31.848768
587.533976	38231.870800	31.853786
587.865889	38298.114527	31.858804
588.448459	38359.178255	31.863821
588.501964	38432.185545	31.868839
589.385276	38497.603303	31.873856
589.913798	38558.831311	31.878874
590.612375	38638.162542	31.883892
591.248526	38701.715374	31.888909
591.535967	38762.734583	31.893927
592.140812	38821.902237	31.898944
592.786091	38878.831689	31.903962
593.069606	38947.724679	31.908980
594.145675	39007.285303	31.913997
594.636518	39077.801697	31.919015
595.326615	39144.260697	31.924032
595.775830	39205.876474	31.929050
596.572605	39280.424565	31.934068
597.697712	39333.383898	31.939085
598.103659	39393.703764	31.944103
598.710514	39456.582224	31.949120
599.203136	39508.431383	31.954138
599.638477	39566.609875	31.959156
600.320163	39641.847698	31.964173
600.604992	39702.693691	31.969191
601.127493	39770.066570	31.974208
601.763545	39834.955492	31.979226
602.174233	39916.262343	31.984244
603.219448	39984.114587	31.989261
604.083990	40050.263900	31.994279
604.203139	40121.404547	31.999296
604.876085	40187.519758	32.004314
605.274587	40257.550870	32.009332
606.097940	40326.457579	32.014349
606.579622	40411.394695	32.019367
607.275745	40479.682187	32.024384
607.966026	40543.709128	32.029402
608.307686	40622.132511	32.034420
608.772924	40698.401722	32.039437
609.283109	40772.640236	32.044455
610.130927	40847.063115	32.049472
610.618275	40920.876661	32.054490
611.747988	41007.963360	32.059508
612.161377	41081.701390	32.064525
612.734912	41170.835029	32.069543
613.079651	41235.650797	32.074560
614.348080	41314.959284	32.079578
614.947384	41385.378175	32.084596
615.504219	41455.037203	32.089613
616.225786	41525.628978	32.094631
616.324650	41603.206403	32.099648
617.026554	41680.081387	32.104666
617.688662	41759.984593	32.109684
618.351757	41841.917988	32.114701
618.570170	41905.541518	32.119719
619.363320	41992.963200	32.124736
620.342711	42066.014812	32.129754
620.708407	42144.380676	32.134772
621.503960	42213.778903	32.139789
622.201749	42294.205749	32.144807
622.597537	42378.499934	32.149824
623.613666	42447.275305	32.154842
623.951620	42531.210358	32.159860
624.763192	42598.441528	32.164877
625.369190	42675.579603	32.169895
626.019331	42745.673204	32.174912
626.876612	42818.059695	32.179930
627.264146	42895.200091	32.184948
628.144531	42960.267928	32.189965
628.606675	43034.602368	32.194983
628.942981	43120.892527	32.200000
629.648647	43184.316680	32.205018
630.075424	43266.165988	32.210036
630.978758	43342.086260	32.215053
632.004690	43417.209849	32.220071
632.161735	43495.132831	32.225088
632.852139	43557.705130	32.230106
633.201134	43639.344765	32.235124
633.616742	43718.454126	32.240141
634.620158	43785.001093	32.245159
635.273797	43854.015281	32.250176
635.967739	43919.887718	32.255194
636.631815	43996.137553	32.260212
636.931275	44072.845860	32.265229
637.612250	44139.175887	32.270247
638.198154	44221.239854	32.275264
638.965292	44292.548162	32.280282
639.314454	44364.838409	32.285300
639.626701	44454.182531	32.290317
640.646003	44533.359647	32.295335
641.096727	44614.336239	32.300352
641.812885	44695.869206	32.305370
642.259775	44787.140854	32.310388
642.902233	44866.425922	32.315405
643.646156	44947.503849	32.320423
644.115254	45042.098023	32.325440
644.943586	45123.617443	32.330458
645.518885	45213.313195	32.335476
646.469657	45307.099595	32.340493
647.228459	45388.382206	32.345511
647.659143	45473.672887	32.350528
648.304832	45550.178363	32.355546
649.213767	45645.296446	32.360564
649.767086	45722.395764	32.365581
650.095864	45810.411007	32.370599
650.855886	45900.594177	32.375616
651.860906	45974.162037	32.380634
652.490773	46063.306499	32.385652
653.230864	46142.902871	32.390669
654.021777	46233.028832	32.395687
654.749124	46308.102842	32.400704
655.821383	46382.883252	32.405722
656.541707	46470.211532	32.410740
656.679438	46554.402923	32.415757
657.613992	46627.902876	32.420775
658.237424	46708.111445	32.425792
659.066363	46784.348433	32.430810
659.471242	46866.065413	32.435828
660.074734	46936.652875	32.440845
661.342185	47013.383511	32.445863
661.498059	47107.859813	32.450880
662.257584	47179.840293	32.455898
662.897850	47264.498023	32.460916
663.334118	47337.397866	32.465933
664.038003	47423.924795	32.470951
664.483040	47510.747580	32.475968
665.711962	47573.098834	32.480986
666.467119	47659.090955	32.486004
666.941786	47742.799203	32.491021
667.745960	47815.182090	32.496039
667.984791	47904.800948	32.501056
668.907843	47977.587970	32.506074
669.791679	48063.393244	32.511092
670.180692	48142.790777	32.516109
670.538188	48213.291016	32.521127
671.102678	48310.554324	32.526144
672.198928	48381.002451	32.531162
672.655694	48470.256294	32.536180
673.077392	48561.436546	32.541197
674.035698	48645.188747	32.546215
674.620777	48731.921268	32.551232
675.687634	48822.455976	32.556250
676.341796	48897.028016	32.561268
676.789556	48980.104995	32.566285
677.458286	49048.134416	32.571303
677.831537	49136.242920	32.576320
678.636409	49204.935727	32.581338
679.572302	49280.609120	32.586356
680.393820	49357.062893	32.591373
681.546178	49416.375552	32.596391
681.987132	49508.987848	32.601408
682.299143	49562.827556	32.606426
682.946122	49635.363338	32.611444
683.469798	49722.356838	32.616461
684.412696	49790.662530	32.621479
684.583150	49873.337583	32.626496
685.261270	49954.400325	32.631514
686.188794	50049.537280	32.636532
686.243099	50128.947847	32.641549
687.386242	50205.490754	32.646567
688.073308	50298.306168	32.651584
688.711307	50389.765668	32.656602
689.580011	50482.027605	32.661620
690.059618	50564.607093	32.666637
690.888712	50638.790545	32.671655
691.560719	50729.159482	32.676672
692.305542	50825.562318	32.681690
692.938283	50908.212697	32.686708
693.206234	51006.116683	32.691725
694.729075	51086.036835	32.696743
695.302843	51174.345723	32.701760
695.680814	51267.697024	32.706778
696.057907	51365.262583	32.711796
697.059685	51458.593736	32.716813
697.827689	51545.046458	32.721831
698.546629	51647.421279	32.726848
699.092365	51733.090338	32.731866
699.945483	51817.205365	32.736884
700.581194	51916.531389	32.741901
701.162252	52008.235361	32.746919
701.887812	52103.807489	32.751936
702.851057	52197.957211	32.756954
703.757053	52291.301882	32.761972
703.981348	52379.035959	32.766989
705.089383	52473.276777	32.772007
705.184982	52566.649417	32.777024
706.375537	52663.126611	32.782042
707.252618	52751.493554	32.787060
707.558573	52846.923921	32.792077
708.021036	52939.883856	32.797095
709.086488	53034.500858	32.802112
709.674916	53133.657668	32.807130
710.837995	53230.199064	32.812148
711.341824	53325.327355	32.817165
711.861966	53414.470263	32.822183
712.432182	53514.826112	32.827200
712.991933	53617.755658	32.832218
714.167404	53710.607618	32.837236
714.537721	53813.872794	32.842253
715.483449	53909.714263	32.847271
716.500674	54006.567920	32.852288
716.755184	54103.301808	32.857306
717.498955	54196.208515	32.862324
718.730867	54301.083879	32.867341
719.300886	54382.729436	32.872359
719.966059	54482.847052	32.877376
721.022423	54575.672248	32.882394
721.719923	54665.562321	32.887412
722.428814	54760.928997	32.892429
722.539761	54852.363863	32.897447
723.352457	54949.420260	32.902464
724.162399	55048.733302	32.907482
725.303898	55143.720656	32.912500
725.979672	55230.059542	32.917517
726.836314	55307.143721	32.922535
727.316904	55389.541186	32.927552
727.734365	55472.499158	32.932570
728.498816	55555.608597	32.937588
729.248599	55653.582423	32.942605
729.577696	55736.758314	32.947623
730.584836	55834.147049	32.952640
731.269659	55927.463398	32.957658
732.090870	56019.373801	32.962676
732.629061	56113.460899	32.967693
733.277193	56210.512773	32.972711
734.181420	56309.696468	32.977728
734.755905	56404.518252	32.982746
735.497962	56504.159428	32.987764
736.215988	56599.394405	32.992781
737.039887	56697.999331	32.997799
737.790618	56799.245584	33.002816
738.426333	56897.054823	33.007834
739.311066	57000.845490	33.012852
739.696268	57108.719362	33.017869
740.713397	57209.967864	33.022887
741.286492	57312.857498	33.027904
741.933957	57416.582141	33.032922
743.208503	57517.517892	33.037940
743.855239	57622.520221	33.042957
744.574839	57720.553421	33.047975
745.278070	57826.583849	33.052992
745.781609	57941.387648	33.058010
746.792740	58036.094379	33.063028
747.246179	58144.840939	33.068045
748.264529	58241.752952	33.073063
749.123948	58346.041372	33.078080
749.965622	58445.682045	33.083098
751.119188	58541.410330	33.088116
752.023037	58649.655380	33.093133
752.671360	58740.463012	33.098151
753.463898	58839.968410	33.103168
754.238273	58938.339747	33.108186
755.219684	59038.453177	33.113204
755.752725	59135.670955	33.118221
756.527619	59221.745236	33.123239
757.659655	59324.710698	33.128256
757.946101	59419.613316	33.133274
758.843413	59510.604421	33.138292
759.620892	59610.880816	33.143309
760.446763	59703.009555	33.148327
761.541713	59796.080130	33.153344
762.108539	59896.424380	33.158362
762.779484	59981.684839	33.163380
763.566368	60078.789314	33.168397
764.282997	60177.947277	33.173415
764.978014	60273.987137	33.178432
766.077299	60368.064525	33.183450
766.836117	60458.400208	33.188468
767.303811	60557.816086	33.193485
768.240935	60643.332345	33.198503
769.176436	60743.487069	33.203520
769.795148	60838.600487	33.208538
770.318927	60931.517922	33.213556
771.150884	61028.606832	33.218573
771.936729	61116.463366	33.223591
772.703020	61210.574442	33.228608
773.154646	61311.304982	33.233626
774.110133	61410.688575	33.238644
774.637057	61516.318714	33.243661
775.514920	61614.028547	33.248679
776.068756	61715.401511	33.253696
776.965938	61806.270166	33.258714
777.790887	61904.103907	33.263732
778.350808	62000.275362	33.268749
779.031470	62093.342782	33.273767
779.548882	62192.594043	33.278784
780.369695	62296.877515	33.283802
781.194385	62383.601638	33.288820
781.953964	62477.865023	33.293837
782.762514	62587.455189	33.298855
783.515583	62692.876992	33.303872
784.290383	62808.295476	33.308890
785.047687	62901.385480	33.313908
785.621096	63015.757549	33.318925
786.397787	63116.316754	33.323943
787.148189	63224.364947	33.328960
787.697139	63339.615164	33.333978
788.590764	63453.114947	33.338996
789.669196	63580.807445	33.344013
790.437268	63689.013175	33.349031
791.227209	63788.113255	33.354048
791.635169	63913.295381	33.359066
792.403097	64025.099701	33.364084
793.098487	64149.761615	33.369101
794.323126	64265.139113	33.374119
794.868656	64387.374540	33.379136
795.532600	64510.532998	33.384154
796.515666	64621.679122	33.389172
797.842214	64751.335383	33.394189
798.135077	64863.393469	33.399207
799.408381	64976.206629	33.404224
800.369122	65099.913717	33.409242
801.153027	65211.924068	33.414260
801.874645	65331.506092	33.419277
802.917322	65434.396856	33.424295
803.826901	65547.406022	33.429312
804.583388	65663.987658	33.434330
805.625632	65769.004272	33.439348
806.259801	65886.738991	33.444365
807.183128	65999.931663	33.449383
808.069377	66101.239492	33.454400
808.468236	66228.757173	33.459418
809.280967	66319.419350	33.464436
810.000443	66442.308163	33.469453
811.158000	66560.225623	33.474471
812.214716	66672.053255	33.479488
812.935870	66789.538410	33.484506
813.796497	66883.109612	33.489524
814.196168	66999.492149	33.494541
814.888695	67114.075629	33.499559
816.186574	67226.707182	33.504576
816.739913	67355.179769	33.509594
817.469678	67463.335507	33.514612
818.318864	67572.199122	33.519629
819.036920	67690.739326	33.524647
820.010449	67814.966090	33.529664
820.331007	67937.676696	33.534682
821.583257	68053.038878	33.539700
822.491362	68160.605980	33.544717
822.935413	68286.832496	33.549735
824.227563	68397.675618	33.554752
825.021616	68511.800970	33.559770
826.074349	68630.613535	33.564788
826.533193	68749.822155	33.569805
827.247577	68868.382193	33.574823
828.181522	68962.639649	33.579840
829.078671	69098.400385	33.584858
829.881693	69212.433170	33.589876
830.867930	69323.919745	33.594893
831.425801	69434.560923	33.599911
832.105818	69543.393070	33.604928
833.167257	69649.570258	33.609946
833.944509	69752.861085	33.614964
834.771296	69859.280460	33.619981
835.402159	69981.578461	33.624999
836.190201	70084.078714	33.630016
836.877926	70201.291089	33.635034
837.868238	70312.921258	33.640052
838.775939	70439.671884	33.645069
839.323147	70551.136294	33.650087
840.400156	70665.839718	33.655104
840.900587	70791.477319	33.660122
841.786981	70908.888339	33.665140
842.940842	71028.127495	33.670157
843.576705	71149.153989	33.675175
844.677945	71267.720243	33.680192
845.190370	71396.034219	33.685210
846.161480	71509.766863	33.690228
846.604209	71649.488916	33.695245
847.600298	71774.892182	33.700263
848.829133	71898.676767	33.705280
849.163377	72027.675298	33.710298
850.384885	72156.812426	33.715316
851.218267	72288.784330	33.720333
852.471683	72418.626006	33.725351
853.319523	72538.803123	33.730368
853.885066	72662.145269	33.735386
854.671063	72795.127262	33.740404
855.895120	72917.906631	33.745421
856.363597	73040.375296	33.750439
857.478954	73163.970854	33.755456
858.489258	73307.359865	33.760474
859.105831	73440.734293	33.765492
860.332668	73565.603812	33.770509
860.862057	73697.944421	33.775527
861.898525	73820.633416	33.780544
862.980021	73962.269469	33.785562
863.445254	74077.591744	33.790580
864.417781	74207.142698	33.795597
865.149419	74342.141597	33.800615
866.462070	74462.682499	33.805632
866.968807	74603.582929	33.810650
867.762150	74731.952321	33.815668
869.072025	74858.175246	33.820685
870.018199	74991.978947	33.825703
870.619978	75116.119509	33.830720
871.266115	75251.568206	33.835738
872.074023	75387.547552	33.840756
873.041979	75520.585576	33.845773
874.266437	75663.492869	33.850791
875.033907	75778.407240	33.855808
875.549082	75904.489294	33.860826
876.449919	76047.439939	33.865844
877.395972	76164.515186	33.870861
878.064802	76318.024253	33.875879
879.431316	76451.185386	33.880896
880.124168	76583.054572	33.885914
880.969848	76716.841059	33.890932
881.719190	76862.320407	33.895949
882.773718	76999.046849	33.900967
883.651950	77123.918288	33.905984
884.186458	77263.540729	33.911002
885.486830	77403.416903	33.916020
886.373200	77533.608828	33.921037
887.005318	77674.223416	33.926055
887.859773	77810.640029	33.931072
888.788643	77950.815109	33.936090
889.331325	78076.000381	33.941108
890.464379	78202.961062	33.946125
891.174150	78338.924085	33.951143
892.110078	78463.629006	33.956160
892.848523	78603.592964	33.961178
893.653218	78743.021811	33.966196
894.709529	78874.932976	33.971213
895.223219	79011.229801	33.976231
896.279011	79146.507918	33.981248
897.162861	79295.681392	33.986266
898.034878	79430.099667	33.991284
898.863504	79563.121579	33.996301
899.312010	79726.729595	34.001319
900.247590	79863.259114	34.006336
901.230811	80013.996059	34.011354
902.370829	80170.287632	34.016372
903.057027	80318.178399	34.021389
903.915209	80464.637293	34.026407
904.749955	80606.868814	34.031424
905.737170	80773.716526	34.036442
906.728366	80922.522372	34.041460
908.036672	81075.837997	34.046477
908.653243	81241.599049	34.051495
909.271363	81388.831118	34.056512
910.400433	81551.068124	34.061530
911.286093	81704.843781	34.066548
912.332641	81862.959149	34.071565
913.082126	82014.083296	34.076583
914.000285	82173.455714	34.081600
915.078111	82339.825392	34.086618
916.229655	82502.217263	34.091636
917.145792	82648.977936	34.096653
917.968783	82812.021039	34.101671
919.203055	82972.998015	34.106688
920.502819	83131.409241	34.111706
920.900367	83279.537714	34.116724
922.083919	83425.879505	34.121741
922.933105	83583.096631	34.126759
923.958840	83740.817100	34.131776
925.202844	83893.535813	34.136794
925.706710	84047.535784	34.141812
927.090859	84192.862231	34.146829
927.455558	84357.934457	34.151847
928.773594	84497.104743	34.156864
929.819861	84659.522863	34.161882
930.882062	84812.556090	34.166900
932.046690	84955.152249	34.171917
932.586978	85107.463819	34.176935
933.261144	85252.730803	34.181952
934.428469	85420.442918	34.186970
935.512995	85566.871528	34.191988
936.268277	85722.302653	34.197005
937.096317	85874.337517	34.202023
937.935434	86037.489189	34.207040
938.790987	86193.697814	34.212058
939.836102	86356.127920	34.217076
940.932493	86502.674314	34.222093
941.660697	86661.906470	34.227111
942.647916	86810.137045	34.232128
943.666834	86967.576710	34.237146
944.605979	87134.725005	34.242164
945.722495	87281.209637	34.247181
946.675029	87456.305925	34.252199
947.374793	87604.089107	34.257216
948.278123	87759.812951	34.262234
949.332093	87928.567863	34.267252
950.412984	88084.599872	34.272269
950.865653	88240.407720	34.277287
951.985729	88388.866692	34.282304
953.067356	88533.953636	34.287322
953.897820	88686.392232	34.292340
954.846399	88823.877290	34.297357
955.628241	88984.913449	34.302375
956.485828	89130.667586	34.307392
957.420085	89298.534382	34.312410
958.229683	89459.221080	34.317428
959.258020	89612.816309	34.322445
959.927555	89782.128887	34.327463
961.354798	89939.837150	34.332480
962.161288	90093.402526	34.337498
962.638515	90261.845280	34.342516
963.486298	90420.032238	34.347533
964.756397	90602.256978	34.352551
965.690549	90768.121494	34.357568
966.957985	90933.729514	34.362586
967.605631	91102.915766	34.367604
968.727517	91269.588109	34.372621
969.776749	91437.090064	34.377639
971.057524	91616.048560	34.382656
971.892787	91781.417390	34.387674
972.725796	91959.667645	34.392692
973.688496	92116.188444	34.397709
974.859242	92289.309217	34.402727
975.503614	92479.866970	34.407744
976.717514	92645.748707	34.412762
977.970931	92820.714094	34.417780
978.855628	92993.178267	34.422797
979.825767	93156.768207	34.427815
980.656412	93338.832970	34.432832
982.155480	93516.129970	34.437850
982.734306	93687.079862	34.442868
983.880858	93850.790845	34.447885
984.780912	94026.177733	34.452903
986.021547	94209.472425	34.457920
987.105936	94373.203493	34.462938
987.611682	94554.375174	34.467956
988.857759	94729.140161	34.472973
989.744329	94906.725692	34.477991
991.009526	95086.623645	34.483008
991.811477	95254.458459	34.488026
992.575104	95435.948434	34.493044
993.753536	95612.167770	34.498061
995.313748	95792.034720	34.503079
996.082860	95969.653610	34.508096
997.149206	96134.538742	34.513114
997.881833	96316.299805	34.518132
999.235761	96491.913960	34.523149
1000.284189	96673.479807	34.528167
1001.037386	96845.827997	34.533184
1002.301329	97014.383251	34.538202
1003.288960	97190.518671	34.543220
1004.262969	97363.808815	34.548237
1004.933624	97532.801169	34.553255
1005.916276	97714.182844	34.558272
1007.090003	97881.897864	34.563290
1007.731917	98063.186453	34.568308
1009.299653	98244.386573	34.573325
1010.130889	98426.944285	34.578343
1011.170088	98602.327676	34.583360
1012.248823	98772.906892	34.588378
1013.304999	98961.319038	34.593396
1014.296469	99137.847272	34.598413
1015.445783	99311.140779	34.603431
1016.438410	99475.673786	34.608448
1017.588535	99648.405987	34.613466
1018.116945	99821.159848	34.618484
1019.162955	99987.111849	34.623501
1020.465996	100144.538513	34.628519
1021.620818	100308.277655	34.633536
1022.433609	100469.174633	34.638554
1022.907269	100641.594862	34.643572
1023.881688	100806.848565	34.648589
1025.274427	100971.736587	34.653607
1026.278126	101153.037995	34.658624
1027.412523	101313.228607	34.663642
1027.967741	101500.437987	34.668660
1029.079902	101671.885785	34.673677
1029.916489	101850.364149	34.678695
1030.897944	102022.513376	34.683712
1031.879230	102211.208734	34.688730
1032.797104	102396.148508	34.693748
1034.018675	102586.332839	34.698765
1035.041518	102755.643408	34.703783
1035.799381	102954.651486	34.708800
1037.068916	103149.353029	34.713818
1037.889992	103341.622677	34.718836
1039.009394	103532.210732	34.723853
1040.337192	103718.155911	34.728871
1041.215547	103910.686224	34.733888
1042.250150	104105.003140	34.738906
1043.198260	104309.518126	34.743924
1044.418944	104493.320868	34.748941
1045.499288	104689.749547	34.753959
1046.232648	104887.072942	34.758976
1047.326866	105084.477464	34.763994
1048.574366	105284.568441	34.769012
1049.860439	105487.909501	34.774029
1050.759490	105677.485655	34.779047
1051.626250	105885.116619	34.784064
1052.987991	106073.947843	34.789082
1053.569853	106281.350365	34.794100
1054.590262	106484.236358	34.799117
1056.093910	106693.351533	34.804135
1056.805533	106900.598093	34.809152
1058.010311	107101.216441	34.814170
1059.245097	107319.589097	34.819188
1059.787369	107522.688681	34.824205
1061.059410	107721.856615	34.829223
1062.233355	107934.354540	34.834240
1063.072509	108140.690284	34.839258
1064.128449	108351.209713	34.844276
1065.517226	108563.588415	34.849293
1066.520041	108771.206581	34.854311
1067.503056	108990.305741	34.859328
1068.792533	109191.394325	34.864346
1069.970344	109399.976392	34.869364
1070.906536	109611.766782	34.874381
1072.132551	109822.902876	34.879399
1072.832907	110034.596203	34.884416
1074.378270	110241.679875	34.889434
1075.419074	110447.746463	34.894452
1076.244924	110671.154066	34.899469
1077.578243	110861.847625	34.904487
1078.520701	111087.405510	34.909504
1079.606237	111299.627643	34.914522
1080.819616	111508.283242	34.919540
1081.667678	111721.751343	34.924557
1082.929717	111927.944462	34.929575
1083.884732	112137.660983	34.934592
1084.788119	112352.049584	34.939610
1086.020109	112569.717320	34.944628
1087.091111	112780.382325	34.949645
1088.414310	112990.893214	34.954663
1089.180438	113208.237566	34.959680
1090.296909	113411.019858	34.964698
1091.311825	113603.862629	34.969716
1092.314560	113798.165679	34.974733
1093.393520	114000.375669	34.979751
1094.422622	114208.423192	34.984768
1095.594281	114415.257773	34.989786
1096.448889	114619.270338	34.994804
1097.777578	114824.802358	34.999821
1098.781991	115033.240140	35.004839
1099.600087	115254.975407	35.009856
1101.010785	115457.204353	35.014874
1102.100327	115676.136031	35.019892
1103.176476	115895.477049	35.024909
1104.621899	116099.782706	35.029927
1105.463200	116311.766449	35.034944
1106.781419	116523.660253	35.039962
1107.943375	116748.720600	35.044980
1108.639441	116957.413514	35.049997
1110.190264	117177.420794	35.055015
1111.045026	117396.581867	35.060032
1112.287808	117614.210658	35.065050
1113.177235	117836.714422	35.070068
1114.205540	118061.515721	35.075085
1115.104620	118277.356383	35.080103
1116.493741	118503.039120	35.085120
1117.552033	118736.925896	35.090138
1118.774352	118960.853130	35.095156
1119.649678	119197.004007	35.100173
1121.338551	119423.151197	35.105191
1122.434127	119650.754085	35.110208
1123.719044	119874.665321	35.115226
1124.823559	120086.747289	35.120244
1125.746377	120336.699115	35.125261
1127.108055	120544.737558	35.130279
1127.973642	120779.597597	35.135296
1129.341892	120999.296498	35.140314
1130.483897	121239.462167	35.145332
1131.335887	121458.844319	35.150349
1132.714915	121687.860763	35.155367
1133.632714	121929.931952	35.160384
1134.994367	122151.845527	35.165402
1136.083036	122387.669908	35.170420
1137.256925	122617.728577	35.175437
1138.440145	122856.937367	35.180455
1139.507231	123092.200593	35.185472
1140.705829	123312.312152	35.190490
1141.949100	123554.634185	35.195508
1142.868525	123789.040152	35.200525
1144.396246	124008.975668	35.205543
1145.281799	124246.736587	35.210560
1146.366334	124480.841814	35.215578
1147.619848	124722.727955	35.220596
1148.913106	124959.387821	35.225613
1150.228811	125174.576133	35.230631
1151.505530	125421.001272	35.235648
1152.525565	125648.332860	35.240666
1153.742341	125879.271125	35.245684
1154.828102	126115.150436	35.250701
1155.892658	126340.071676	35.255719
1156.974393	126579.187199	35.260736
1158.264334	126815.063481	35.265754
1159.483458	127040.674070	35.270772
1160.719087	127273.558926	35.275789
1161.994017	127498.200344	35.280807
1163.306637	127734.536192	35.285824
1164.373682	127961.484157	35.290842
1165.338190	128189.857675	35.295860
1166.593093	128420.022779	35.300877
1167.444570	128625.197051	35.305895
1168.850241	128848.647796	35.310912
1169.808533	129075.089467	35.315930
1170.975739	129285.121310	35.320948
1171.422578	129510.573237	35.325965
1172.911370	129733.281347	35.330983
1173.956281	129966.103727	35.336000
1175.265620	130191.126397	35.341018
1176.311356	130423.368911	35.346036
1176.906520	130666.690539	35.351053
1178.410663	130907.163723	35.356071
1179.193214	131145.843872	35.361088
1180.451309	131397.529325	35.366106
1181.822487	131639.323013	35.371124
1182.787321	131888.500137	35.376141
1184.128941	132134.815347	35.381159
1184.789098	132384.959414	35.386176
1185.897372	132632.293124	35.391194
1187.371986	132904.567356	35.396212
1188.539266	133165.523254	35.401229
1189.710047	133423.438127	35.406247
1190.979464	133680.109038	35.411264
1191.790424	133941.447004	35.416282
1193.197547	134200.153001	35.421300
1194.307012	134475.086975	35.426317
1195.830514	134739.812583	35.431335
1196.695335	135016.325545	35.436352
1198.053212	135272.170261	35.441370
1199.767765	135536.819993	35.446388
1200.727427	135811.371519	35.451405
1201.850161	136081.549706	35.456423
1202.994239	136348.785175	35.461440
1204.094614	136617.221794	35.466458
1206.037304	136882.186869	35.471476
1207.083481	137161.083997	35.476493
1208.485105	137426.345681	35.481511
1209.555894	137684.842892	35.486528
1210.827285	137959.994511	35.491546
1212.482099	138216.155081	35.496564
1213.528439	138490.866423	35.501581
1214.553057	138754.184879	35.506599
1215.916556	139021.684288	35.511616
1217.256540	139290.952140	35.516634
1218.714035	139547.028580	35.521652
1219.951378	139817.369960	35.526669
1221.390277	140064.006966	35.531687
1222.478632	140324.144373	35.536704
1223.594667	140593.180528	35.541722
1224.997822	140839.752927	35.546740
1226.105978	141108.794405	35.551757
1227.407696	141365.366625	35.556775
1228.792974	141628.482683	35.561792
1229.629408	141892.452279	35.566810
1231.198539	142152.054778	35.571828
1232.504430	142417.231485	35.576845
1233.622965	142676.823594	35.581863
1234.991903	142941.423212	35.586880
1236.160941	143190.853414	35.591898
1237.634594	143448.680597	35.596916
1238.636466	143713.093060	35.601933
1239.973656	143969.817979	35.606951
1241.364467	144227.791342	35.611968
1242.041273	144490.906427	35.616986
1243.313658	144749.106044	35.622004
1244.731477	145019.369042	35.627021
1246.003192	145275.809830	35.632039
1247.471875	145545.979618	35.637056
1248.449533	145804.387729	35.642074
1249.752387	146046.143262	35.647092
1250.984515	146300.315136	35.652109
1252.026330	146538.249080	35.657127
1253.357339	146786.624971	35.662144
1254.516009	147043.566229	35.667162
1255.868874	147295.886176	35.672180
1256.852809	147555.878328	35.677197
1258.387774	147802.730889	35.682215
1259.375163	148062.256804	35.687232
1260.379146	148330.139733	35.692250
1261.829136	148582.198810	35.697268
1262.955336	148845.157018	35.702285
1264.086823	149107.266454	35.707303
1265.647290	149369.167323	35.712320
1267.026279	149646.560839	35.717338
1268.572916	149904.244249	35.722356
1269.124338	150183.592237	35.727373
1270.331336	150444.937578	35.732391
1271.862188	150726.271224	35.737408
1273.068559	150998.401533	35.742426
1274.195365	151268.454133	35.747444
1275.724763	151550.047823	35.752461
1276.788405	151821.941271	35.757479
1277.987653	152101.234395	35.762496
1279.355192	152390.458772	35.767514
1281.009344	152668.983228	35.772532
1282.133159	152953.546292	35.777549
1283.601643	153233.906695	35.782567
1284.619172	153508.369275	35.787584
1285.729528	153802.847398	35.792602
1287.172125	154083.611452	35.797620
1288.594111	154372.651401	35.802637
1289.628265	154662.467940	35.807655
1291.353328	154939.525540	35.812672
1292.465047	155242.627371	35.817690
1293.915290	155530.707121	35.822708
1294.897103	155827.352811	35.827725
1295.787784	156115.326335	35.832743
1297.229974	156403.210796	35.837760
1298.644572	156711.956875	35.842778
1300.074308	157002.689276	35.847796
1301.461577	157311.596726	35.852813
1302.743592	157600.937075	35.857831
1303.940180	157895.773923	35.862848
1305.327559	158195.414745	35.867866
1306.718959	158494.689221	35.872884
1308.130955	158789.370103	35.877901
1309.446189	159093.545740	35.882919
1310.896823	159398.094538	35.887936
1312.115749	159693.980987	35.892954
1313.591662	159980.515175	35.897972
1314.819302	160276.011079	35.902989
1316.172099	160583.464665	35.908007
1317.787080	160877.923964	35.913024
1319.087660	161176.966526	35.918042
1320.231134	161472.154975	35.923060
1321.172580	161765.184025	35.928077
1322.396617	162072.669843	35.933095
1324.201495	162373.096603	35.938112
1325.195259	162672.949055	35.943130
1326.921689	162967.632940	35.948148
1328.551485	163269.680911	35.953165
1329.928725	163570.516684	35.958183
1331.545148	163866.404898	35.963200
1332.649336	164158.725721	35.968218
1334.142462	164444.335802	35.973236
1335.055029	164724.625958	35.978253
1336.527061	165017.005980	35.983271
1337.925524	165294.123627	35.988288
1338.983096	165576.641102	35.993306
1340.487118	165850.103314	35.998324
1341.556098	166130.072124	36.003341
1342.733598	166412.765482	36.008359
1344.318210	166701.991401	36.013376
1345.444865	166984.899832	36.018394
1346.841670	167272.980469	36.023412
1347.888257	167552.200639	36.028429
1349.137575	167849.470656	36.033447
1350.861209	168134.888927	36.038464
1351.859253	168439.208660	36.043482
1353.259802	168727.742128	36.048500
1354.424136	169031.302393	36.053517
1356.163203	169329.998538	36.058535
1357.180394	169626.785640	36.063552
1358.298094	169934.673997	36.068570
1359.775541	170241.845110	36.073588
1361.208660	170556.131772	36.078605
1362.568451	170873.935042	36.083623
1363.928805	171174.913751	36.088640
1365.285267	171487.595094	36.093658
1366.916336	171805.588303	36.098676
1368.294363	172118.511401	36.103693
1369.369391	172433.732800	36.108711
1370.806741	172748.350744	36.113728
1372.071119	173067.847046	36.118746
1373.662059	173387.811830	36.123764
1375.109928	173709.947084	36.128781
1376.382547	174032.329199	36.133799
1378.093376	174339.539218	36.138816
1379.348093	174669.517536	36.143834
1380.565670	174987.308386	36.148852
1382.192764	175311.353687	36.153869
1383.571896	175630.149983	36.158887
1384.929397	175951.439365	36.163904
1386.065451	176284.519413	36.168922
1387.711347	176607.504086	36.173940
1389.606793	176937.099856	36.178957
1390.983403	177260.755139	36.183975
1392.386571	177566.094362	36.188992
1393.565383	177891.195146	36.194010
1395.200268	178224.726036	36.199028
1396.796749	178536.613438	36.204045
1398.031843	178857.522858	36.209063
1399.875475	179161.415500	36.214080
1400.874912	179485.451915	36.219098
1402.574973	179803.840876	36.224116
1403.788018	180117.882739	36.229133
1405.141680	180432.994790	36.234151
1406.886403	180752.321406	36.239168
1408.309283	181083.024697	36.244186
1409.691080	181383.148194	36.249204
1411.320699	181698.856866	36.254221
1412.333297	182027.564998	36.259239
1414.053942	182341.142791	36.264256
1415.163963	182656.524147	36.269274
1416.689770	182981.942090	36.274292
1418.430274	183293.085152	36.279309
1419.447947	183615.874612	36.284327
1421.044695	183932.198418	36.289344
1422.156676	184260.738731	36.294362
1423.669062	184586.308117	36.299380
1425.263417	184901.990563	36.304397
1426.402827	185221.786450	36.309415
1427.826919	185542.679539	36.314432
1429.018251	185870.188133	36.319450
1430.590952	186199.717356	36.324468
1432.239191	186514.156053	36.329485
1433.531156	186829.950121	36.334503
1435.088501	187123.005728	36.339520
1436.272690	187435.101703	36.344538
1437.324164	187751.473749	36.349556
1438.492966	188061.988941	36.354573
1440.151705	188386.591338	36.359591
1441.701492	188704.193736	36.364608
1442.810831	189023.774762	36.369626
1444.142227	189342.051418	36.374644
1445.729467	189672.588266	36.379661
1447.172032	189998.200073	36.384679
1448.716189	190325.256735	36.389696
1450.022896	190663.055869	36.394714
1451.528064	190992.306067	36.399732
1453.258194	191325.608559	36.404749
1454.510699	191660.362830	36.409767
1455.718298	191997.157522	36.414784
1456.932781	192337.850240	36.419802
1458.639841	192677.181269	36.424820
1459.938778	193024.769851	36.429837
1461.277215	193389.606413	36.434855
1462.912189	193736.191306	36.439872
1464.133988	194091.834571	36.444890
1465.867139	194447.496907	36.449908
1467.224557	194800.874679	36.454925
1468.574376	195156.096492	36.459943
1470.044454	195511.478134	36.464960
1471.657801	195874.061818	36.469978
1472.794620	196244.267454	36.474996
1474.528787	196594.253828	36.480013
1476.252450	196974.421598	36.485031
1477.358144	197334.024858	36.490048
1478.839989	197707.914264	36.495066
1480.151108	198074.178300	36.500084
1481.889772	198440.652996	36.505101
1483.484832	198807.229577	36.510119
1485.165393	199189.740387	36.515136
1486.793579	199566.142394	36.520154
1488.096178	199930.234045	36.525172
1489.872350	200300.914950	36.530189
1491.197762	200675.608192	36.535207
1492.687234	201033.224912	36.540224
1494.066765	201410.134995	36.545242
1495.631365	201790.101774	36.550260
1497.707803	202162.964718	36.555277
1499.135722	202537.498438	36.560295
1500.702706	202912.493589	36.565312
1502.298098	203271.018087	36.570330
1503.702135	203634.515062	36.575348
1505.190368	204002.101043	36.580365
1506.597952	204375.834849	36.585383
1508.441572	204738.553528	36.590400
1509.931722	205112.785225	36.595418
1511.386922	205488.776757	36.600436
1512.741366	205859.606263	36.605453
1514.213733	206227.269109	36.610471
1515.973020	206592.308702	36.615488
1517.359654	206962.541358	36.620506
1518.698487	207344.325738	36.625524
1520.871792	207706.787957	36.630541
1521.969910	208089.326734	36.635559
1523.514416	208459.260891	36.640576
1524.976763	208821.870973	36.645594
1526.601903	209198.601180	36.650612
1528.273455	209558.437205	36.655629
1529.703056	209941.094925	36.660647
1530.826343	210307.678498	36.665664
1532.427918	210657.346981	36.670682
1533.890628	211021.845868	36.675700
1535.627627	211367.152119	36.680717
1536.922698	211725.916707	36.685735
1538.491401	212088.650225	36.690752
1539.988983	212448.323994	36.695770
1541.354820	212807.843214	36.700788
1543.136291	213165.720608	36.705805
1544.496091	213519.732560	36.710823
1546.296505	213891.349479	36.715840
1547.618230	214260.354892	36.720858
1548.788921	214624.485059	36.725876
1550.609265	214996.103145	36.730893
1552.078277	215371.285606	36.735911
1553.580950	215744.432188	36.740928
1555.085204	216129.491494	36.745946
1556.215134	216520.379485	36.750964
1557.518238	216902.884529	36.755981
1559.290775	217297.606147	36.760999
1561.161032	217688.376491	36.766016
1562.616679	218085.312433	36.771034
1563.979892	218483.357336	36.776052
1565.663725	218870.861285	36.781069
1567.324147	219272.644521	36.786087
1568.552976	219683.821901	36.791104
1570.483618	220086.655769	36.796122
1572.072012	220487.998383	36.801140
1573.549105	220891.672187	36.806157
1574.989049	221307.316555	36.811175
1576.812028	221702.122774	36.816192
1578.584667	222111.111455	36.821210
1579.861039	222532.121271	36.826228
1581.922133	222925.292315	36.831245
1583.341018	223339.423748	36.836263
1584.802233	223744.126441	36.841280
1586.740159	224157.997241	36.846298
1588.270726	224562.462691	36.851316
1589.845846	225036.542997	36.856333
1591.195706	225467.380932	36.861351
1592.778599	225872.019893	36.866368
1594.476037	226285.607465	36.871386
1596.005592	226716.470826	36.876404
1598.065081	227118.393429	36.881421
1599.586688	227550.937307	36.886439
1601.275533	227958.740398	36.891456
1602.914313	228373.715940	36.896474
1604.158763	228794.904831	36.901492
1605.836546	229210.943306	36.906509
1607.683622	229632.060601	36.911527
1609.535150	230047.717252	36.916544
1611.154857	230454.777119	36.921562
1612.421299	230884.681111	36.926580
1614.231388	231291.381645	36.931597
1616.072026	231720.634381	36.936615
1617.366937	232140.783272	36.941632
1619.013699	232562.577062	36.946650
1620.335403	232981.275927	36.951668
1622.230589	233401.481440	36.956685
1623.844675	233830.472560	36.961703
1625.485615	234252.043132	36.966720
1627.541686	234678.321675	36.971738
1628.145496	235110.327928	36.976756
1630.305843	235525.389241	36.981773
1631.957186	235953.312671	36.986791
1633.521791	236381.429258	36.991808
1635.339868	236809.327158	36.996826
1636.862596	237236.639776	37.001844
1638.682227	237648.485325	37.006861
1640.327716	238062.722895	37.011879
1641.849564	238462.121555	37.016896
1643.442698	238864.074837	37.021914
1644.874627	239267.732071	37.026932
1646.323141	239673.648131	37.031949
1648.051284	240080.179223	37.036967
1649.392601	240504.048518	37.041984
1651.098110	240912.667853	37.047002
1652.881820	241342.638395	37.052020
1654.301004	241751.154079	37.057037
1656.185224	242174.174650	37.062055
1657.354596	242611.869663	37.067072
1659.439160	243032.292927	37.072090
1660.935495	243476.641667	37.077108
1662.241829	243891.961906	37.082125
1663.776544	244334.298889	37.087143
1664.974560	244772.475321	37.092160
1667.105650	245226.527411	37.097178
1668.386538	245668.324054	37.102196
1670.339823	246120.882655	37.107213
1672.182799	246582.020867	37.112231
1673.334873	247048.074974	37.117248
1675.048993	247501.945064	37.122266
1676.593056	247967.554566	37.127284
1678.362054	248432.238373	37.132301
1680.295601	248899.308823	37.137319
1681.944368	249375.444912	37.142336
1683.888635	249832.582014	37.147354
1685.349995	250316.548786	37.152372
1687.147628	250773.761812	37.157389
1688.609922	251245.916869	37.162407
1690.207790	251733.571263	37.167424
1692.212933	252216.459196	37.172442
1693.938479	252708.462619	37.177460
1695.465004	253181.777094	37.182477
1697.152719	253669.062422	37.187495
1698.679458	254152.310106	37.192512
1700.540725	254647.620143	37.197530
1702.040317	255133.946593	37.202548
1703.594001	255631.365541	37.207565
1705.663106	256116.328135	37.212583
1707.344144	256609.077571	37.217600
1709.186355	257097.100894	37.222618
1710.733693	257598.738373	37.227636
1712.389302	258095.150353	37.232653
1714.390286	258587.542402	37.237671
1716.036354	259082.965260	37.242688
1718.163778	259582.855774	37.247706
1719.669226	260076.752169	37.252724
1721.612538	260566.435417	37.257741
1723.326988	261068.095895	37.262759
1724.823678	261565.245001	37.267776
1727.297189	262054.306769	37.272794
1728.706894	262556.702928	37.277812
1730.863387	263044.267020	37.282829
1732.868454	263529.620380	37.287847
1734.322012	264019.586318	37.292864
1736.189271	264498.712653	37.297882
1737.787582	264986.596368	37.302900
1739.520237	265479.563557	37.307917
1741.352779	265972.894886	37.312935
1742.802693	266450.767670	37.317952
1744.990958	266944.547415	37.322970
1746.673957	267436.885931	37.327988
1748.432605	267919.126423	37.333005
1750.337084	268410.233350	37.338023
1751.761724	268897.227459	37.343040
1753.943482	269374.519014	37.348058
1755.430045	269841.509593	37.353076
1757.344445	270300.172975	37.358093
1759.122725	270760.153781	37.363111
1760.449615	271227.295892	37.368128
1762.413174	271683.815430	37.373146
1764.064252	272152.121972	37.378164
1765.621484	272619.757414	37.383181
1767.810975	273089.573922	37.388199
1769.131696	273559.329909	37.393216
1771.102648	274029.231724	37.398234
1772.638191	274509.772064	37.403252
1774.114484	274995.630406	37.408269
1775.965383	275470.655306	37.413287
1777.543012	275959.695709	37.418304
1779.392461	276441.399740	37.423322
1780.747973	276938.019253	37.428340
1782.726549	277434.560159	37.433357
1784.744786	277941.381247	37.438375
1786.361325	278441.916939	37.443392
1788.247202	278940.171556	37.448410
1789.782092	279443.487088	37.453428
1791.788409	279948.323789	37.458445
1793.715227	280461.300870	37.463463
1795.223426	280981.483569	37.468480
1797.074895	281493.200140	37.473498
1798.992917	282007.673027	37.478516
1800.522415	282522.919805	37.483533
1802.524296	283037.502781	37.488551
1804.313692	283565.048561	37.493568
1806.383952	284086.322941	37.498586
1808.128589	284602.340551	37.503604
1809.752732	285131.711951	37.508621
1811.735737	285656.043665	37.513639
1813.680469	286182.132543	37.518656
1815.610293	286701.998807	37.523674
1817.627299	287239.807148	37.528692
1819.490643	287768.926411	37.533709
1821.050533	288281.456420	37.538727
1822.768957	288821.771851	37.543744
1824.900376	289347.716513	37.548762
1826.383728	289893.171918	37.553780
1828.010245	290421.837298	37.558797
1830.309229	290952.142052	37.563815
1832.002533	291496.768568	37.568832
1833.961105	292021.384623	37.573850
1835.896765	292561.775435	37.578868
1837.709966	293102.996830	37.583885
1839.859556	293640.807466	37.588903
1841.442068	294178.404476	37.593920
1843.238387	294713.601530	37.598938
1845.369755	295243.686294	37.603956
1846.803791	295799.054109	37.608973
1849.155508	296335.878785	37.613991
1850.702064	296873.392532	37.619008
1852.748961	297407.493727	37.624026
1854.800355	297949.541198	37.629044
1856.471506	298500.690443	37.634061
1858.387634	299037.598662	37.639079
1860.078064	299583.633812	37.644096
1862.193852	300117.938071	37.649114
1864.274085	300665.731534	37.654132
1866.095288	301203.811978	37.659149
1868.072784	301735.387226	37.664167
1869.679686	302279.897154	37.669184
1871.519346	302806.333444	37.674202
1873.428844	303358.457048	37.679220
1875.228817	303895.357241	37.684237
1877.660479	304421.940421	37.689255
1879.145096	304944.410241	37.694272
1881.280484	305448.103090	37.699290
1883.040323	305959.778697	37.704308
1884.822685	306470.787248	37.709325
1886.736049	306975.777642	37.714343
1888.554871	307502.214744	37.719360
1890.515307	308012.448073	37.724378
1892.331373	308522.092597	37.729396
1893.977980	309050.732288	37.734413
1895.796231	309566.210850	37.739431
1897.802893	310097.730059	37.744448
1899.602571	310623.769190	37.749466
1901.493051	311152.100722	37.754484
1903.217237	311691.553534	37.759501
1905.014475	312218.902782	37.764519
1906.863429	312770.592863	37.769536
1908.630132	313319.042055	37.774554
1910.422853	313868.752610	37.779572
1911.912180	314416.122170	37.784589
1914.280376	314973.398311	37.789607
1916.016285	315540.754104	37.794624
1917.942553	316100.709999	37.799642
1919.864713	316661.728653	37.804660
1921.597553	317235.140296	37.809677
1923.632332	317813.448880	37.814695
1925.535067	318386.162740	37.819712
1927.330149	318963.663263	37.824730
1929.711496	319532.073367	37.829748
1931.443699	320115.363711	37.834765
1933.836932	320691.887255	37.839783
1935.651691	321274.188862	37.844800
1937.711718	321854.337322	37.849818
1939.813381	322434.727598	37.854836
1941.780808	323022.142519	37.859853
1943.636206	323598.094136	37.864871
1945.447428	324182.375662	37.869888
1947.373286	324768.613170	37.874906
1949.387026	325349.194137	37.879924
1951.064319	325935.740828	37.884941
1953.243114	326523.011485	37.889959
1955.211202	327114.855769	37.894976
1957.318249	327708.930801	37.899994
1959.488879	328304.411096	37.905012
1961.200095	328902.322266	37.910029
1963.547101	329488.215479	37.915047
1965.404569	330083.526126	37.920064
1967.171385	330678.718595	37.925082
1969.430601	331276.971480	37.930100
1971.267194	331882.015218	37.935117
1973.012543	332470.566329	37.940135
1974.808739	333076.873017	37.945152
1976.840246	333682.042554	37.950170
1979.152677	334285.077358	37.955188
1981.015022	334887.824332	37.960205
1983.166717	335494.070629	37.965223
1985.107438	336104.990216	37.970240
1986.392190	336715.274869	37.975258
1988.335564	337318.742266	37.980276
1990.716065	337939.696008	37.985293
1992.984350	338541.318603	37.990311
1994.756183	339156.722958	37.995328
1996.562292	339770.464292	38.000346
1998.789367	340390.499636	38.005364
2000.495764	341005.638324	38.010381
2002.763183	341627.631375	38.015399
2004.521006	342244.700517	38.020416
2006.604465	342866.962002	38.025434
2008.807454	343472.063642	38.030452
2010.618868	344071.410154	38.035469
2012.688237	344662.229538	38.040487
2014.357465	345247.016427	38.045504
2016.256970	345844.879304	38.050522
2018.523644	346437.420397	38.055540
2020.266103	347049.049329	38.060557
2022.172047	347644.147036	38.065575
2024.467604	348254.577321	38.070592
2026.419016	348867.797047	38.075610
2028.734929	349473.081206	38.080628
2030.209912	350081.236776	38.085645
2032.287705	350701.972991	38.090663
2034.281474	351317.943577	38.095680
2036.192601	351936.735935	38.100698
2038.634732	352563.958146	38.105716
2039.927352	353201.460499	38.110733
2042.156221	353825.502304	38.115751
2044.264272	354460.491463	38.120768
2046.092472	355112.010660	38.125786
2048.368939	355743.197389	38.130804
2049.983000	356393.641020	38.135821
2052.285043	357034.851954	38.140839
2054.109641	357694.831507	38.145856
2056.120028	358352.410168	38.150874
2058.847608	359008.540503	38.155892
2060.496947	359659.180374	38.160909
2062.922473	360325.157997	38.165927
2065.157076	360983.646335	38.170944
2066.869279	361654.362378	38.175962
2068.912403	362306.720754	38.180980
2070.527631	362977.683983	38.185997
2072.900191	363646.531876	38.191015
2075.154367	364328.021307	38.196032
2077.662343	365013.109788	38.201050
2079.807252	365685.004037	38.206068
2082.053049	366354.180840	38.211085
2084.085106	367015.517388	38.216103
2086.688509	367696.838077	38.221120
2088.528030	368368.227564	38.226138
2090.708649	369033.765290	38.231156
2092.692555	369708.759221	38.236173
2094.575059	370381.931220	38.241191
2096.938363	371059.729108	38.246208
2099.181315	371735.682637	38.251226
2101.326147	372414.049152	38.256244
2103.239366	373090.538847	38.261261
2105.075015	373767.358183	38.266279
2107.420507	374449.659941	38.271296
2109.207340	375131.736336	38.276314
2111.901741	375817.326880	38.281332
2113.827562	376502.422116	38.286349
2115.967755	377191.500538	38.291367
2118.136523	377876.908705	38.296384
2120.256199	378565.607816	38.301402
2122.798524	379247.275081	38.306420
2124.597183	379939.549330	38.311437
2127.001276	380628.565087	38.316455
2128.864454	381304.419823	38.321472
2130.884755	381995.194851	38.326490
2133.271088	382676.488134	38.331508
2135.305339	383369.412554	38.336525
2137.517661	384055.548603	38.341543
2139.648368	384739.731362	38.346560
2141.606059	385433.638461	38.351578
2143.851623	386117.468710	38.356596
2145.999591	386807.156757	38.361613
2147.838045	387497.235821	38.366631
2150.521836	388178.845115	38.371648
2152.299699	388849.282809	38.376666
2154.585287	389510.470961	38.381684
2156.459219	390171.865084	38.386701
2158.713629	390830.647361	38.391719
2160.988283	391500.413363	38.396736
2162.722220	392167.516391	38.401754
2164.645599	392832.368321	38.406772
2166.903567	393509.722378	38.411789
2169.221108	394185.327841	38.416807
2171.683513	394874.479363	38.421824
2173.496416	395550.365387	38.426842
2176.015866	396228.577803	38.431860
2177.671445	396914.064171	38.436877
2179.848674	397605.353407	38.441895
2182.107879	398294.078509	38.446912
2183.739630	398998.020020	38.451930
2186.069552	399699.269700	38.456948
2188.089860	400410.157539	38.461965
2190.224342	401123.745623	38.466983
2192.338255	401831.389809	38.472000
2194.086429	402564.440850	38.477018
2196.344184	403289.837978	38.482036
2198.983670	404026.808598	38.487053
2200.671394	404770.555101	38.492071
2203.173136	405501.276594	38.497088
2205.286395	406248.536271	38.502106
2207.587361	406978.897048	38.507124
2209.986083	407720.546537	38.512141
2212.388362	408469.800586	38.517159
2214.740931	409212.100962	38.522176
2216.471155	409961.525907	38.527194
2218.961463	410713.261598	38.532212
2221.387308	411473.852446	38.537229
2223.475272	412229.436637	38.542247
2225.705456	412980.745789	38.547264
2227.585908	413759.851080	38.552282
2229.967366	414516.587514	38.557300
2232.005342	415281.944446	38.562317
2234.229830	416058.923319	38.567335
2236.520461	416820.925892	38.572352
2238.634654	417613.527047	38.577370
2241.181178	418389.521114	38.582388
2243.472877	419174.421899	38.587405
2245.606135	419951.246654	38.592423
2247.935830	420737.054744	38.597440
2250.069596	421520.743551	38.602458
2252.565110	422300.575326	38.607476
2255.072827	423089.470077	38.612493
2257.178222	423889.495365	38.617511
2259.955056	424666.344909	38.622528
2261.919581	425453.936767	38.627546
2264.031748	426234.339681	38.632564
2266.860894	427023.813733	38.637581
2268.854959	427807.071168	38.642599
2271.267323	428582.083076	38.647616
2273.325716	429379.453814	38.652634
2275.859894	430159.912324	38.657652
2278.111511	430951.123450	38.662669
2280.398500	431749.591370	38.667687
2282.666489	432529.458327	38.672704
2284.650580	433328.782735	38.677722
2286.795628	434115.652431	38.682740
2289.228276	434925.527337	38.687757
2291.481181	435710.705111	38.692775
2293.999108	436504.365182	38.697792
2296.236221	437306.647222	38.702810
2298.443811	438105.211503	38.707828
2300.556271	438885.950582	38.712845
2302.785904	439654.549224	38.717863
2305.255297	440422.069869	38.722880
2307.232147	441197.994146	38.727898
2309.746191	441956.043037	38.732916
2312.101097	442731.395765	38.737933
2314.151396	443497.108039	38.742951
2316.632002	444273.599750	38.747968
2318.989061	445053.321938	38.752986
2321.347578	445820.065302	38.758004
2323.320122	446604.196271	38.763021
2325.785518	447394.945073	38.768039
2328.126278	448178.350781	38.773056
2330.295048	448973.996643	38.778074
2332.812533	449763.333968	38.783092
2335.165593	450555.551858	38.788109
2336.883514	451361.500021	38.793127
2339.224674	452170.652201	38.798144
2341.766653	452985.252143	38.803162
2344.026012	453791.270067	38.808180
2346.514706	454606.523130	38.813197
2348.199838	455442.911638	38.818215
2351.153237	456258.781028	38.823232
2353.294205	457088.100024	38.828250
2355.787516	457922.433549	38.833268
2357.975496	458762.091584	38.838285
2360.427022	459602.126196	38.843303
2362.807900	460434.908332	38.848320
2364.922605	461292.924423	38.853338
2367.371314	462143.013477	38.858356
2370.190877	462985.018625	38.863373
2372.301604	463840.195736	38.868391
2374.801299	464697.697497	38.873408
2376.960166	465571.137904	38.878426
2379.009690	466427.172435	38.883444
2381.753470	467292.252057	38.888461
2384.023505	468160.200985	38.893479
2386.301258	469032.050898	38.898496
2388.559978	469920.184898	38.903514
2391.262424	470784.861465	38.908532
2394.129299	471676.350058	38.913549
2396.309253	472566.899592	38.918567
2399.190813	473442.943987	38.923584
2401.640350	474325.636419	38.928602
2403.876620	475196.754667	38.933620
2406.507906	476067.312373	38.938637
2408.999715	476955.429412	38.943655
2411.460797	477822.700011	38.948672
2413.623182	478702.150547	38.953690
2416.289998	479577.435464	38.958708
2419.084959	480457.202182	38.963725
2421.341606	481335.954664	38.968743
2423.883145	482206.942271	38.973760
2426.305251	483090.177074	38.978778
2428.927947	483964.903530	38.983796
2431.416398	484836.933499	38.988813
2433.592144	485719.978014	38.993831
2436.346903	486585.971477	38.998848
2438.942608	487468.405109	39.003866
2441.144631	488338.542989	39.008884
2443.590550	489212.584923	39.013901
2445.664844	490089.117536	39.018919
2448.368050	490977.614899	39.023936
2450.812468	491855.763635	39.028954
2453.486072	492729.388981	39.033972
2455.902944	493612.196325	39.038989
2458.056274	494494.093353	39.044007
2460.733953	495368.087936	39.049024
2463.083916	496238.206651	39.054042
2465.439373	497099.097549	39.059060
2467.942664	497942.616105	39.064077
2470.036346	498794.937557	39.069095
2472.480967	499640.398229	39.074112
2474.977505	500502.453085	39.079130
2477.182228	501350.539849	39.084148
2479.708732	502206.347667	39.089165
2481.841236	503081.744239	39.094183
2484.639594	503951.890826	39.099200
2486.693170	504818.785786	39.104218
2489.190776	505695.192662	39.109236
2491.533091	506579.494240	39.114253
2494.065340	507473.497631	39.119271
2496.512685	508373.011351	39.124288
2498.541026	509262.259369	39.129306
2500.772507	510170.177513	39.134324
2503.423084	511077.369948	39.139341
2505.800273	512006.230073	39.144359
2508.138095	512914.981988	39.149376
2510.688457	513856.859843	39.154394
2513.095572	514794.673152	39.159412
2515.544907	515741.292577	39.164429
2517.757367	516691.622514	39.169447
2520.476960	517627.248712	39.174464
2522.853123	518579.703362	39.179482
2525.537472	519553.510699	39.184500
2528.051618	520511.616834	39.189517
2530.050810	521480.175503	39.194535
2532.546885	522462.241348	39.199552
2535.492304	523449.558943	39.204570
2537.913358	524427.077417	39.209588
2540.472693	525420.423943	39.214605
2543.134696	526401.299637	39.219623
2545.779386	527395.860749	39.224640
2548.418331	528396.297880	39.229658
2550.619129	529410.082090	39.234676
2553.780977	530392.424476	39.239693
2556.044474	531409.836753	39.244711
2558.767385	532415.877326	39.249728
2561.242899	533420.429728	39.254746
2563.720321	534437.394534	39.259764
2566.172918	535449.611654	39.264781
2568.782474	536466.412051	39.269799
2571.205627	537487.599510	39.274816
2573.866493	538507.165496	39.279834
2576.183019	539548.651937	39.284852
2578.956006	540583.496918	39.289869
2581.484579	541628.971407	39.294887
2584.102973	542658.961257	39.299904
2586.659102	543691.199634	39.304922
2588.812533	544733.939903	39.309940
2591.708785	545778.642215	39.314957
2594.076481	546848.597180	39.319975
2596.364224	547887.156365	39.324992
2599.486403	548937.818116	39.330010
2602.046088	550018.305541	39.335028
2604.820074	551070.671208	39.340045
2607.103655	552146.310359	39.345063
2609.993282	553203.971116	39.350080
2612.484411	554268.450223	39.355098
2615.054551	555331.575855	39.360116
2617.572036	556390.957650	39.365133
2619.940903	557462.038008	39.370151
2622.971867	558538.047925	39.375168
2625.696802	559619.597690	39.380186
2628.077179	560684.990334	39.385204
2630.941499	561755.491314	39.390221
2633.703084	562808.844723	39.395239
2636.267606	563846.978421	39.400256
2638.931534	564887.072032	39.405274
2641.346340	565915.774814	39.410292
2644.160088	566943.928345	39.415309
2646.550139	567985.826558	39.420327
2649.069446	569018.331415	39.425344
2651.869345	570071.137746	39.430362
2654.433614	571109.590542	39.435380
2656.772268	572147.343264	39.440397
2659.156672	573214.713929	39.445415
2661.899548	574281.985422	39.450432
2664.377202	575347.453886	39.455450
2666.795726	576409.881296	39.460468
2669.082300	577496.120780	39.465485
2671.825245	578583.243669	39.470503
2674.188773	579682.873989	39.475520
2676.787912	580785.928685	39.480538
2679.361538	581901.627265	39.485556
2682.129789	583007.012433	39.490573
2684.674874	584132.090556	39.495591
2687.241011	585265.233719	39.500608
2690.108989	586386.440007	39.505626
2693.165991	587538.440321	39.510644
2695.904274	588667.175806	39.515661
2698.526045	589804.745492	39.520679
2701.334919	590950.895930	39.525696
2703.867850	592095.177670	39.530714
2706.469722	593253.116416	39.535732
2709.283505	594396.327898	39.540749
2712.033570	595572.300962	39.545767
2714.449482	596736.640666	39.550784
2717.900817	597905.301466	39.555802
2719.974264	599084.939514	39.560820
2722.734210	600260.588927	39.565837
2725.272577	601439.660232	39.570855
2727.814843	602633.178898	39.575872
2730.833629	603820.037330	39.580890
2733.540784	605008.275563	39.585908
2736.618996	606205.687763	39.590925
2739.724352	607409.925190	39.595943
2742.201060	608608.383764	39.600960
2744.811483	609809.144458	39.605978
2747.914168	611018.400286	39.610996
2750.932930	612210.431868	39.616013
2753.645661	613411.839530	39.621031
2756.187560	614616.746207	39.626048
2758.974474	615820.281182	39.631066
2761.427045	617024.639943	39.636084
2764.334660	618237.190719	39.641101
2767.176128	619460.865580	39.646119
2770.097341	620669.245112	39.651136
2772.951366	621882.699048	39.656154
2775.576529	623109.047477	39.661172
2778.156798	624331.166704	39.666189
2781.230377	625555.813504	39.671207
2783.632648	626783.578160	39.676224
2786.644693	628003.209093	39.681242
2789.379461	629242.073973	39.686260
2792.656676	630465.373768	39.691277
2795.391677	631692.416063	39.696295
2797.857834	632932.040781	39.701312
2801.073131	634153.623903	39.706330
2803.762898	635388.178433	39.711348
2806.562001	636619.074967	39.716365
2809.125716	637847.369156	39.721383
2812.042884	639084.689945	39.726400
2814.745952	640310.672092	39.731418
2817.352567	641540.763901	39.736436
2820.055544	642742.410838	39.741453
2822.885255	643940.503901	39.746471
2825.256892	645152.743227	39.751488
2828.442762	646357.224062	39.756506
2830.817732	647561.993960	39.761524
2833.769018	648769.365896	39.766541
2836.162022	649988.846073	39.771559
2838.714817	651214.729472	39.776576
2841.753621	652438.438396	39.781594
2844.389958	653682.191733	39.786612
2847.089933	654911.729469	39.791629
2849.791505	656161.337078	39.796647
2852.580397	657424.467727	39.801664
2855.648583	658671.055266	39.806682
2857.981212	659941.654494	39.811700
2860.703637	661211.176996	39.816717
2863.390464	662488.802332	39.821735
2866.186862	663788.936808	39.826752
2869.269511	665083.772217	39.831770
2871.985568	666389.639168	39.836788
2874.953535	667693.395447	39.841805
2877.808903	669011.567089	39.846823
2880.130836	670340.635657	39.851840
2883.379576	671664.043244	39.856858
2886.247760	673007.913455	39.861876
2888.720525	674335.647444	39.866893
2891.903680	675697.425450	39.871911
2894.430841	677049.420513	39.876928
2897.428744	678400.246548	39.881946
2900.084088	679776.719967	39.886964
2902.752973	681153.879848	39.891981
2906.152425	682518.393789	39.896999
2908.713739	683905.341047	39.902016
2911.972999	685291.118078	39.907034
2914.828665	686683.453084	39.912052
2917.596868	688073.503351	39.917069
2920.911752	689465.482849	39.922087
2923.603287	690869.309744	39.927104
2926.721727	692268.231554	39.932122
2929.624390	693682.795802	39.937140
2932.843911	695084.036887	39.942157
2936.121064	696480.087189	39.947175
2939.145247	697891.777056	39.952192
2942.182058	699295.007927	39.957210
2945.167042	700698.617536	39.962228
2948.044681	702100.978396	39.967245
2951.348895	703507.007452	39.972263
2954.333667	704911.622469	39.977280
2957.704954	706303.659434	39.982298
2960.344180	707715.157281	39.987316
2963.356385	709124.033829	39.992333
2966.515475	710528.098549	39.997351
2969.345108	711939.857936	40.002368
2972.501020	713332.419984	40.007386
2975.531025	714756.547033	40.012404
2978.927127	716153.800847	40.017421
2981.920237	717556.281484	40.022439
2984.971168	718967.916318	40.027456
2988.051709	720363.233599	40.032474
2990.901597	721775.810561	40.037492
2994.145375	723168.503069	40.042509
2997.438228	724560.557181	40.047527
3000.053694	725960.741459	40.052544
3003.141558	727355.963783	40.057562
3006.104895	728753.982417	40.062580
3009.177118	730158.362749	40.067597
3012.309230	731547.179228	40.072615
3015.206755	732932.684988	40.077632
3018.278809	734271.561897	40.082650
3021.005388	735642.064371	40.087668
3023.914338	736993.694763	40.092685
3027.037565	738332.230421	40.097703
3030.232223	739683.703280	40.102720
3033.037192	741032.050347	40.107738
3035.753748	742388.863234	40.112756
3038.693595	743745.257984	40.117773
3041.951680	745117.933335	40.122791
3044.467770	746488.272152	40.127808
3047.347836	747860.183611	40.132826
3050.346293	749250.905452	40.137844
3052.934517	750642.726794	40.142861
3056.135809	752050.699737	40.147879
3058.907483	753462.968496	40.152896
3061.885116	754877.898494	40.157914
3064.610839	756302.800427	40.162932
3067.516191	757736.464483	40.167949
3070.862112	759186.913305	40.172967
3073.824352	760640.100431	40.177984
3076.674056	762084.810715	40.183002
3079.511605	763553.249942	40.188020
3082.303487	765025.491390	40.193037
3085.013349	766500.701914	40.198055
3088.103221	768003.578764	40.203072
3091.321817	769501.068192	40.208090
3094.280500	771002.720281	40.213108
3097.152739	772519.409480	40.218125
3100.624566	774044.528619	40.223143
3103.173391	775583.331274	40.228160
3106.096208	777111.192158	40.233178
3109.331770	778652.670985	40.238196
3112.277250	780215.366050	40.243213
3115.992176	781773.082487	40.248231
3118.708763	783335.924781	40.253248
3121.839440	784896.396930	40.258266
3124.960664	786468.396743	40.263284
3127.647214	788053.358081	40.268301
3130.907093	789621.354177	40.273319
3134.286897	791222.402560	40.278336
3137.022181	792821.675219	40.283354
3140.367826	794416.222391	40.288372
3143.550963	796022.675559	40.293389
3146.653371	797628.331851	40.298407
3149.714223	799250.902266	40.303424
3152.702561	800869.973172	40.308442
3156.143035	802489.030477	40.313460
3159.227273	804128.601813	40.318477
3162.346230	805752.127852	40.323495
3165.090073	807397.085138	40.328512
3168.397464	809030.359827	40.333530
3171.697825	810664.024514	40.338548
3174.843417	812317.984584	40.343565
3178.310317	813951.363736	40.348583
3181.193310	815609.246604	40.353600
3184.371753	817263.936439	40.358618
3187.566468	818919.481954	40.363636
3190.507362	820581.097380	40.368653
3194.080567	822235.655252	40.373671
3196.910132	823900.308205	40.378688
3199.963850	825568.988270	40.383706
3202.787993	827235.916446	40.388724
3205.966246	828911.034637	40.393741
3209.251102	830587.116787	40.398759
3212.315832	832286.813223	40.403776
3215.807290	833964.762604	40.408794
3218.939774	835649.927687	40.413812
3221.704499	837333.786041	40.418829
3224.689770	838989.772648	40.423847
3228.027931	840642.546735	40.428864
3230.802528	842293.913565	40.433882
3234.230443	843944.061097	40.438900
3237.253437	845615.325838	40.443917
3240.526858	847275.317859	40.448935
3243.735898	848946.441677	40.453952
3246.839590	850620.146257	40.458970
3250.277316	852296.840956	40.463988
3253.090567	853986.192907	40.469005
3256.354469	855663.265661	40.474023
3259.788844	857376.721472	40.479040
3262.920396	859080.824975	40.484058
3266.014241	860784.265591	40.489076
3268.744823	862510.652108	40.494093
3272.055620	864226.082360	40.499111
3275.408208	865976.963216	40.504128
3278.773922	867705.831150	40.509146
3282.139828	869460.925841	40.514164
3285.040326	871215.969628	40.519181
3288.754461	872975.298098	40.524199
3291.961528	874742.025231	40.529216
3295.258543	876513.239403	40.534234
3298.723498	878279.833377	40.539252
3301.747162	880058.920883	40.544269
3304.781581	881846.259170	40.549287
3308.129968	883649.612803	40.554304
3311.718895	885451.015673	40.559322
3315.360806	887251.753240	40.564340
3318.479484	889060.797335	40.569357
3321.871813	890860.062426	40.574375
3325.269102	892673.132150	40.579392
3328.476220	894487.971633	40.584410
3332.206518	896300.507720	40.589428
3335.567880	898131.699235	40.594445
3338.764657	899938.244337	40.599463
3342.696154	901769.798050	40.604480
3345.599122	903597.842995	40.609498
3349.087223	905418.361713	40.614516
3352.471582	907257.830043	40.619533
3355.792774	909080.159132	40.624551
3359.617976	910916.032103	40.629568
3362.651353	912759.207873	40.634586
3366.264537	914591.966703	40.639604
3369.358930	916430.919451	40.644621
3372.931152	918267.445154	40.649639
3376.518529	920113.424226	40.654656
3379.639050	921963.071853	40.659674
3383.423223	923796.535370	40.664692
3386.679735	925649.880762	40.669709
3390.047158	927497.870448	40.674727
3393.424594	929353.649253	40.679744
3396.508859	931203.273956	40.684762
3400.132147	933053.983170	40.689780
3403.416329	934910.798690	40.694797
3406.973403	936768.348904	40.699815
3410.143616	938625.495849	40.704832
3413.493368	940485.394575	40.709850
3417.002571	942352.438914	40.714868
3420.405560	944224.847151	40.719885
3423.827484	946085.018576	40.724903
3427.336563	947954.050019	40.729920
3430.488853	949828.185143	40.734938
3433.843687	951691.106665	40.739956
3437.266550	953591.548106	40.744973
3440.397876	955509.298427	40.749991
3443.954703	957446.582415	40.755008
3447.141027	959353.877219	40.760013
3450.598283	961216.072441	40.765018
3453.562241	963023.783622	40.770023
3456.989039	964763.196979	40.775028
3459.861895	966436.401027	40.780032
3463.099101	968049.075089	40.785037
3465.929792	969576.646901	40.790042
3468.745961	971043.667400	40.795047
3471.504817	972418.901280	40.800052
3474.325851	973731.721019	40.805056
3476.828017	974974.902072	40.810061
3479.557058	976136.478723	40.815066
3481.777804	977241.240628	40.820071
3484.135845	978254.048309	40.825076
3486.178711	979201.686541	40.830080
3487.855478	980107.045136	40.835085
3490.060988	980935.142508	40.840090
3492.185036	981694.898359	40.845095
3494.042023	982414.578687	40.850100
3496.102234	983056.449674	40.855104
3497.508738	983647.319430	40.860109
3499.159341	984185.689867	40.865114
3500.164492	984690.260119	40.870119
3501.701063	985131.187351	40.875124
3503.195849	985527.603521	40.880128
3503.935709	985884.805363	40.885133
3505.605692	986184.770207	40.890138
3506.615108	986470.197602	40.895143
3507.887412	986703.095188	40.900148
3508.941298	986901.884175	40.905152
3509.553042	987070.213463	40.910157
3510.793329	987200.009957	40.915162
3511.461662	987304.834590	40.920167
3512.409553	987364.556702	40.925172
3513.312130	987425.943488	40.930176
3513.961581	987429.639817	40.935181
3514.376499	987423.622788	40.940186
3514.944856	987408.023497	40.945191
3515.506395	987349.808653	40.950196
3516.219005	987282.986363	40.955200
3516.589372	987196.422354	40.960205
3517.134054	987085.641971	40.965210
3517.751502	986961.681194	40.970215
3518.270160	986810.913173	40.975220
3518.920074	986653.779886	40.980224
3519.146311	986472.815722	40.985229
3519.581303	986280.496837	40.990234
3519.843310	986084.883498	40.995239
3520.214558	985860.371673	41.000244
3520.455169	985631.482741	41.005248
3520.320701	985400.890416	41.010253
3521.157294	985145.251289	41.015258
3520.881521	984905.198941	41.020263
3521.422963	984637.878091	41.025268
3521.417985	984367.317260	41.030272
3521.888280	984089.151856	41.035277
3522.095312	983787.596552	41.040282
3521.984330	983491.347401	41.045287
3522.280853	983184.280546	41.050292
3522.386323	982882.010922	41.055296
3522.472196	982573.481911	41.060301
3522.588256	982248.630621	41.065306
3522.695234	981927.081206	41.070311
3522.702786	981596.353794	41.075316
3523.057675	981261.644972	41.080320
3523.008424	980937.234367	41.085325
3523.082418	980575.780625	41.090330
3523.011971	980238.055089	41.095335
3522.966387	979898.938392	41.100340
3523.382421	979541.854685	41.105344
3523.209513	979201.838669	41.110349
3523.600450	978831.139811	41.115354
3523.489296	978466.848383	41.120359
3523.609080	978111.189152	41.125364
3523.642363	977744.092826	41.130368
3523.405587	977369.788202	41.135373
3523.809162	977000.531588	41.140378
3523.535053	976635.075547	41.145383
3523.492533	976251.774590	41.150388
3523.502141	975873.813825	41.155392
3523.289509	975501.825861	41.160397
3523.769492	975124.324436	41.165402
3523.790513	974743.452933	41.170407
3523.913699	974362.050534	41.175412
3523.814390	973977.531378	41.180416
3523.922070	973592.170242	41.185421
3523.652314	973202.152716	41.190426
3523.419236	972827.159125	41.195431
3523.453715	972435.377176	41.200436
3523.473521	972055.695932	41.205440
3523.536951	971667.768038	41.210445
3523.906832	971273.406658	41.215450
3523.537676	970888.235560	41.220455
3523.353254	970494.107491	41.225460
3523.584438	970090.591320	41.230464
3523.195894	969701.137555	41.235469
3523.419291	969316.937157	41.240474
3523.103140	968927.614605	41.245479
3523.068275	968539.589091	41.250484
3523.062419	968149.771275	41.255488
3522.933474	967766.699327	41.260493
3523.143198	967368.573048	41.265498
3522.520992	966989.347135	41.270503
3522.753302	966597.525177	41.275508
3522.476673	966209.773521	41.280512
3522.573324	965835.247097	41.285517
3522.840203	965444.319695	41.290522
3522.718791	965049.513586	41.295527
3522.878422	964677.936346	41.300532
3522.577121	964295.542463	41.305536
3522.503488	963909.070854	41.310541
3522.649716	963522.830839	41.315546
3522.675198	963133.255002	41.320551
3522.227862	962754.798054	41.325556
3522.300173	962370.745525	41.330560
3522.115340	961989.354499	41.335565
3522.275140	961608.371230	41.340570
3521.966044	961228.321705	41.345575
3522.092891	960840.729265	41.350580
3522.273794	960454.571547	41.355584
3521.829539	960080.935269	41.360589
3521.679102	959677.828329	41.365594
3521.678363	959314.260593	41.370599
3521.739763	958935.958767	41.375604
3521.922889	958563.100771	41.380608
3521.665294	958176.274544	41.385613
3521.747496	957798.482773	41.390618
3521.391224	957428.483014	41.395623
3521.616567	957063.559723	41.400628
3521.639862	956685.802825	41.405632
3521.331917	956320.037964	41.410637
3521.381434	955938.501900	41.415642
3521.227006	955567.270893	41.420647
3521.114486	955197.578226	41.425652
3521.088076	954821.276603	41.430656
3520.941203	954452.326492	41.435661
3520.694516	954076.110688	41.440666
3520.680853	953724.944312	41.445671
3520.740231	953353.633874	41.450676
3521.004180	952997.864934	41.455680
3520.741013	952620.477888	41.460685
3520.706940	952270.170809	41.465690
3520.498088	951916.374867	41.470695
3520.537170	951550.654152	41.475700
3520.478094	951196.400979	41.480704
3520.292538	950845.874512	41.485709
3520.512774	950493.917880	41.490714
3519.989573	950143.207467	41.495719
3519.980932	949807.313167	41.500724
3520.379219	949456.499507	41.505728
3519.958731	949122.063248	41.510733
3520.053204	948763.597311	41.515738
3519.867606	948420.655632	41.520743
3519.816141	948071.543792	41.525748
3519.622908	947722.527261	41.530752
3519.640796	947397.094542	41.535757
3519.514298	947052.520209	41.540762
3519.506939	946727.432138	41.545767
3519.289398	946379.955826	41.550772
3519.604940	946047.974332	41.555776
3519.039555	945709.892882	41.560781
3519.081979	945368.529185	41.565786
3518.909460	945037.807846	41.570791
3518.622263	944706.988433	41.575796
3518.633577	944380.408462	41.580800
3518.798102	944051.100775	41.585805
3518.779148	943721.036055	41.590810
3518.597180	943399.406826	41.595815
3518.507496	943071.611340	41.600820
3519.043761	942748.003169	41.605824
3518.611185	942420.797822	41.610829
3518.591270	942082.389167	41.615834
3518.426876	941764.200754	41.620839
3518.444219	941445.483761	41.625844
3518.445091	941119.370718	41.630848
3518.254076	940799.690108	41.635853
3518.213937	940471.338866	41.640858
3518.004477	940152.484146	41.645863
3517.924975	939842.599108	41.650868
3517.988871	939521.647738	41.655872
3517.676616	939204.956832	41.660877
3518.108103	938897.615800	41.665882
3517.742641	938585.402184	41.670887
3517.535294	938268.253648	41.675892
3517.377087	937957.694334	41.680896
3517.580206	937658.468883	41.685901
3517.710569	937340.728982	41.690906
3517.517807	937036.450316	41.695911
3517.014265	936726.929870	41.700916
3517.131275	936415.370505	41.705920
3516.877863	936120.640699	41.710925
3516.986817	935800.700621	41.715930
3516.842338	935512.154261	41.720935
3516.755335	935213.316766	41.725940
3516.754403	934921.644186	41.730944
3516.539767	934632.869230	41.735949
3516.477003	934317.568886	41.740954
3516.527229	934030.732403	41.745959
3516.527993	933741.393261	41.750964
3516.626464	933451.062403	41.755968
3516.133987	933158.125491	41.760973
3516.390253	932865.624876	41.765978
3516.215315	932587.289674	41.770983
3516.254992	932294.217170	41.775988
3516.324951	931997.091401	41.780992
3515.472974	931727.654547	41.785997
3515.897774	931435.335070	41.791002
3515.766474	931161.142120	41.796007
3515.773369	930890.945095	41.801012
3515.904188	930606.502048	41.806016
3515.532089	930331.825746	41.811021
3515.524009	930046.415249	41.816026
3515.513536	929777.700976	41.821031
3515.181315	929492.602243	41.826036
3515.346283	929225.367881	41.831040
3514.985464	928949.945905	41.836045
3515.099383	928689.801192	41.841050
3515.303407	928428.091881	41.846055
3514.860134	928152.450097	41.851060
3515.308120	927889.040929	41.856064
3514.880714	927617.788337	41.861069
3515.008987	927345.373470	41.866074
3514.929028	927084.894132	41.871079
3514.902036	926829.774642	41.876084
3514.704252	926565.157321	41.881088
3514.312737	926299.982193	41.886093
3514.560039	926029.883248	41.891098
3514.641573	925773.061620	41.896103
3514.371848	925513.209772	41.901108
3514.163247	925257.468513	41.906112
3514.342220	925004.631135	41.911117
3513.862327	924749.198700	41.916122
3514.125154	924501.322623	41.921127
3513.814754	924261.605327	41.926132
3513.961711	924000.746281	41.931136
3513.714587	923759.265530	41.936141
3513.919808	923500.968659	41.941146
3513.831366	923265.112647	41.946151
3513.409347	923013.819096	41.951156
3514.169049	922773.474498	41.956160
3514.036848	922529.419272	41.961165
3513.603143	922276.554500	41.966170
3513.617226	922040.243249	41.971175
3513.409740	921790.011424	41.976180
3513.432555	921552.234591	41.981184
3513.536400	921310.297642	41.986189
3513.432728	921065.498124	41.991194
3513.159489	920835.819093	41.996199
3513.036872	920597.831807	42.001204
3513.439884	920359.747454	42.006208
3513.208243	920127.818672	42.011213
3513.302621	919878.988043	42.016218
3513.192142	919650.386491	42.021223
3512.812862	919425.187505	42.026228
3512.894782	919185.757280	42.031232
3512.643096	918950.220843	42.036237
3512.713272	918721.069168	42.041242
3512.698842	918493.654134	42.046247
3512.724027	918266.993027	42.051252
3512.477396	918040.463494	42.056256
3512.088079	917828.193752	42.061261
3512.086030	917602.279447	42.066266
3512.042314	917384.930006	42.071271
3512.204913	917163.109636	42.076276
3512.330678	916950.046906	42.081280
3512.129839	916742.035899	42.086285
3512.266248	916516.438826	42.091290
3512.200806	916306.848455	42.096295
3512.155419	916083.863041	42.101300
3511.849927	915862.548286	42.106304
3511.749724	915655.634730	42.111309
3511.880762	915436.541823	42.116314
3511.855097	915235.955689	42.121319
3511.838553	915021.878099	42.126324
3511.732387	914803.087791	42.131328
3511.451941	914597.415865	42.136333
3511.820978	914394.133408	42.141338
3511.417470	914195.208712	42.146343
3511.444961	913974.533200	42.151348
3511.350287	913767.739946	42.156352
3511.291821	913573.070495	42.161357
3511.363054	913364.211759	42.166362
3511.151694	913170.516541	42.171367
3510.951429	912967.853001	42.176372
3511.063211	912759.638957	42.181376
3510.768290	912571.331625	42.186381
3511.295348	912376.619618	42.191386
3511.247448	912180.646481	42.196391
3511.114255	911986.800279	42.201396
3510.974094	911782.926832	42.206400
3510.505725	911590.470935	42.211405
3510.512053	911395.328163	42.216410
3510.903410	911209.848551	42.221415
3510.410548	911022.484502	42.226420
3510.846167	910821.564583	42.231424
3510.222018	910628.907982	42.236429
3510.568543	910450.253275	42.241434
3510.259352	910269.194732	42.246439
3510.123435	910097.451606	42.251444
3510.502736	909901.808961	42.256448
3510.401358	909724.457681	42.261453
3510.428927	909530.787788	42.266458
3510.329506	909361.907793	42.271463
3509.964701	909167.422176	42.276468
3509.857353	908983.106785	42.281472
3510.063686	908810.688818	42.286477
3510.493900	908627.429979	42.291482
3509.869673	908461.694280	42.296487
3509.750200	908277.453805	42.301492
3509.639450	908103.523299	42.306496
3509.559683	907930.353656	42.311501
3509.641849	907757.537652	42.316506
3509.568814	907583.970356	42.321511
3509.549480	907412.028219	42.326516
3510.010671	907242.605483	42.331520
3509.709570	907068.577438	42.336525
3510.138279	906898.378007	42.341530
3509.741987	906734.289137	42.346535
3509.423585	906552.821182	42.351540
3509.581595	906374.548300	42.356544
3509.444063	906217.346325	42.361549
3509.824047	906047.128866	42.366554
3509.805472	905878.611755	42.371559
3509.658042	905706.348555	42.376564
3509.479987	905525.595698	42.381568
3509.100924	905358.279867	42.386573
3509.520409	905195.844200	42.391578
3509.181783	905033.914613	42.396583
3508.998191	904870.700519	42.401588
3509.132767	904706.367903	42.406592
3509.071900	904551.614872	42.411597
3508.770746	904391.397218	42.416602
3508.736008	904226.788904	42.421607
3508.645055	904073.185477	42.426612
3508.672643	903916.084368	42.431616
3508.663519	903768.538456	42.436621
3508.821695	903619.417038	42.441626
3508.862636	903472.144566	42.446631
3508.707530	903309.555682	42.451636
3508.880688	903154.725402	42.456640
3508.785746	903001.286202	42.461645
3508.577021	902835.314386	42.466650
3508.995672	902696.356218	42.471655
3508.567587	902537.650643	42.476660
3508.838779	902372.165167	42.481664
3508.595292	902232.725441	42.486669
3508.594731	902073.839767	42.491674
3508.641693	901911.563122	42.496679
3508.344872	901762.756824	42.501684
3508.571160	901621.197258	42.506688
3508.390530	901479.315002	42.511693
3508.544159	901311.597192	42.516698
3508.524562	901173.059668	42.521703
3508.342171	901024.697677	42.526708
3508.456869	900883.620647	42.531712
3507.979935	900727.382201	42.536717
3508.156447	900581.845978	42.541722
3508.041460	900439.830099	42.546727
3508.029470	900303.490722	42.551732
3507.964370	900161.363035	42.556736
3507.716647	900034.229416	42.561741
3507.978522	899896.579722	42.566746
3508.041945	899756.738260	42.571751
3507.896699	899608.622506	42.576756
3507.973482	899469.447717	42.581760
3507.927002	899333.090530	42.586765
3507.927209	899196.239457	42.591770
3508.063131	899056.658422	42.596775
3507.667522	898924.888215	42.601780
3507.734604	898780.482493	42.606784
3507.777099	898648.826835	42.611789
3507.560252	898503.011962	42.616794
3507.667136	898370.180106	42.621799
3507.687454	898237.166198	42.626804
3507.557756	898106.009233	42.631808
3507.359869	897979.497261	42.636813
3507.475037	897841.628414	42.641818
3507.603507	897720.853027	42.646823
3507.277177	897580.828656	42.651828
3507.683797	897465.315364	42.656832
3507.373006	897330.499109	42.661837
3507.312817	897202.497903	42.666842
3507.377414	897076.888631	42.671847
3507.091884	896946.599993	42.676852
3507.480976	896803.733236	42.681856
3506.967962	896699.563756	42.686861
3507.108885	896566.780578	42.691866
3506.713941	896452.634810	42.696871
3506.805412	896328.453911	42.701876
3507.181367	896200.261583	42.706880
3507.015571	896086.553845	42.711885
3507.098394	895966.328370	42.716890
3506.881408	895843.927104	42.721895
3506.850168	895725.648051	42.726900
3507.083399	895605.583436	42.731904
3506.732525	895481.843453	42.736909
3506.932635	895361.972432	42.741914
3507.128716	895237.750445	42.746919
3506.775380	895122.314650	42.751924
3506.949322	894996.351359	42.756928
3506.543054	894884.012271	42.761933
3506.943810	894767.575163	42.766938
3506.820421	894659.534499	42.771943
3506.801163	894540.745533	42.776948
3506.798759	894413.735153	42.781952
3506.393100	894303.414371	42.786957
3506.690783	894182.729129	42.791962
3506.543483	894086.087939	42.796967
3506.259874	893973.807335	42.801972
3506.608568	893853.590061	42.806977
3505.915582	893750.942854	42.811981
3506.189157	893639.337240	42.816986
3506.364890	893527.648886	42.821991
3506.001455	893422.621252	42.826996
3506.589782	893310.473963	42.832001
3506.396841	893218.949599	42.837005
3506.440679	893090.161847	42.842010
3506.289508	892990.892282	42.847015
3506.306135	892890.916539	42.852020
3506.507838	892771.570870	42.857025
3506.227843	892670.479874	42.862029
3506.414318	892552.969263	42.867034
3506.267089	892450.015337	42.872039
3506.095595	892356.056254	42.877044
3506.421786	892246.735453	42.882049
3506.070565	892143.132724	42.887053
3506.026737	892029.227161	42.892058
3505.952990	891926.348399	42.897063
3506.044193	891830.016522	42.902068
3506.289825	891723.503428	42.907073
3506.055945	891621.806048	42.912077
3506.089872	891520.449579	42.917082
3506.102747	891420.932301	42.922087
3506.145529	891323.149203	42.927092
3506.275781	891215.678544	42.932097
3506.155228	891108.247190	42.937101
3506.047275	890991.526760	42.942106
3506.004291	890888.430844	42.947111
3505.832674	890797.928132	42.952116
3506.169281	890686.544679	42.957121
3506.054845	890594.675205	42.962125
3505.665975	890481.472783	42.967130
3505.938961	890389.052553	42.972135
3505.863036	890283.919891	42.977140
3505.808552	890181.587010	42.982145
3505.476489	890092.744054	42.987149
3505.808643	889989.086504	42.992154
3505.778686	889894.676781	42.997159
3505.541670	889796.430067	43.002164
3505.360258	889709.007434	43.007169
3505.472461	889614.182719	43.012173
3505.409197	889525.480184	43.017178
3505.804953	889426.735928	43.022183
3505.129083	889338.034681	43.027188
3505.821437	889242.721277	43.032193
3505.529300	889163.628924	43.037197
3505.095744	889062.596308	43.042202
3505.336334	888978.092321	43.047207
3505.207716	888882.230936	43.052212
3505.545696	888800.127147	43.057217
3505.445606	888716.255978	43.062221
3505.440049	888621.144027	43.067226
3505.487896	888532.020836	43.072231
3504.740422	888428.319514	43.077236
3505.008657	888355.510008	43.082241
3505.124320	888275.370630	43.087245
3505.160373	888183.534588	43.092250
3505.533025	888107.705007	43.097255
3505.277277	888010.398547	43.102260
3505.170925	887924.581506	43.107265
3505.035374	887849.025791	43.112269
3505.071984	887761.247335	43.117274
3505.464022	887677.279965	43.122279
3505.265137	887604.247613	43.127284
3505.510003	887506.075963	43.132289
3505.466817	887414.724622	43.137293
3505.321515	887320.291686	43.142298
3505.458784	887233.553207	43.147303
3505.301114	887147.733066	43.152308
3505.257261	887056.085811	43.157313
3505.066383	886975.494961	43.162317
3504.947772	886879.501839	43.167322
3505.276776	886805.114166	43.172327
3504.908029	886726.775297	43.177332
3505.152218	886631.589400	43.182337
3505.006217	886555.534519	43.187341
3505.087000	886467.148359	43.192346
3505.247368	886377.102203	43.197351
3504.574941	886300.840309	43.202356
3505.356217	886219.110776	43.207361
3504.888420	886150.363491	43.212365
3504.858084	886064.699890	43.217370
3505.162566	885984.013607	43.222375
3504.677560	885909.651730	43.227380
3504.941038	885819.870331	43.232385
3504.949122	885743.295358	43.237389
3504.655545	885657.572295	43.242394
3504.985181	885582.878391	43.247399
3504.704743	885508.284034	43.252404
3504.826989	885430.911639	43.257409
3504.534085	885358.544083	43.262413
3504.841009	885280.364747	43.267418
3504.774219	885205.828112	43.272423
3504.344924	885128.736181	43.277428
3504.575182	885047.468189	43.282433
3504.601361	884988.888468	43.287437
3504.659238	884895.350669	43.292442
3504.705484	884824.663350	43.297447
3504.581791	884750.420703	43.302452
3504.371721	884669.510434	43.307457
3504.478557	884605.685018	43.312461
3504.501291	884536.644104	43.317466
3504.594688	884461.490553	43.322471
3504.110183	884399.115884	43.327476
3504.528944	884339.012488	43.332481
3504.439063	884272.020416	43.337485
3504.187184	884199.244308	43.342490
3504.451773	884141.100918	43.347495
3504.267443	884061.049429	43.352500
3504.276293	883986.581509	43.357505
3504.069372	883928.997859	43.362509
3504.073024	883854.238588	43.367514
3504.525709	883791.412472	43.372519
3504.285005	883729.474638	43.377524
3504.584308	883643.236768	43.382529
3504.229137	883578.314084	43.387533
3504.099922	883499.698427	43.392538
3504.557623	883446.261644	43.397543
3504.597203	883373.911409	43.402548
3504.464714	883300.910690	43.407553
3504.377213	883233.906263	43.412557
3504.241799	883169.911300	43.417562
3504.094094	883103.302686	43.422567
3504.194545	883035.102795	43.427572
3504.433763	882961.164909	43.432577
3504.413614	882888.818486	43.437581
3504.148003	882834.236151	43.442586
3504.292105	882763.604508	43.447591
3504.311338	882699.869471	43.452596
3504.369475	882636.321044	43.457601
3504.083402	882565.370435	43.462605
3504.245262	882492.989112	43.467610
3504.440350	882436.583653	43.472615
3504.182206	882373.956230	43.477620
3504.491733	882294.767709	43.482625
3504.276760	882231.744189	43.487629
3503.930005	882163.220313	43.492634
3504.066551	882104.690228	43.497639
3504.087225	882042.691383	43.502644
3504.390350	881963.402554	43.507649
3504.178409	881910.158896	43.512653
3504.080022	881833.840574	43.517658
3504.202524	881771.434585	43.522663
3503.905175	881713.650174	43.527668
3503.976394	881650.863849	43.532673
3504.101905	881592.717950	43.537677
3504.082523	881526.070172	43.542682
3504.037142	881463.204163	43.547687
3504.056210	881410.499157	43.552692
3504.210394	881339.945502	43.557697
3503.682891	881282.291618	43.562701
3504.350544	881216.205285	43.567706
3504.111739	881151.720794	43.572711
3504.022364	881096.705626	43.577716
3503.906495	881031.521365	43.582721
3503.820178	880967.300372	43.587725
3504.134717	880913.185795	43.592730
3504.253222	880851.933293	43.597735
3504.155488	880794.882009	43.602740
3504.105877	880722.416697	43.607745
3503.987448	880668.952536	43.612749
3503.814857	880608.036112	43.617754
3504.050205	880547.148739	43.622759
3503.858462	880485.846624	43.627764
3504.156781	880422.331434	43.632769
3503.834442	880366.475719	43.637773
3504.032906	880307.239165	43.642778
3504.097332	880240.369132	43.647783
3503.722604	880168.822613	43.652788
3504.014976	880102.882452	43.657793
3503.859370	880063.275650	43.662797
3503.823783	880002.233448	43.667802
3503.886893	879946.504027	43.672807
3503.851087	879890.693468	43.677812
3503.892037	879821.496823	43.682817
3503.958208	879765.377555	43.687821
3503.654362	879701.759951	43.692826
3503.842645	879644.553428	43.697831
3503.932482	879589.494568	43.702836
3503.649304	879529.844963	43.707841
3503.944181	879472.522292	43.712845
3503.533160	879411.535790	43.717850
3503.771389	879351.507733	43.722855
3503.641474	879300.746537	43.727860
3503.839131	879250.900081	43.732865
3503.650366	879194.235861	43.737869
3503.703616	879131.231642	43.742874
3503.941741	879083.121594	43.747879
3503.677982	879035.869184	43.752884
3503.636963	878974.235666	43.757889
3503.611073	878920.061864	43.762893
3503.574684	878863.175502	43.767898
3503.765689	878814.586413	43.772903
3503.395460	878766.283232	43.777908
3503.520860	878699.482508	43.782913
3503.561013	878658.283182	43.787917
3503.310149	878599.006484	43.792922
3503.459791	878541.214026	43.797927
3503.550540	878500.780672	43.802932
3503.412791	878436.734272	43.807937
3503.406197	878387.301853	43.812941
3503.208998	878338.191210	43.817946
3503.534209	878287.830922	43.822951
3503.533137	878244.406083	43.827956
3503.610254	878185.749699	43.832961
3503.311654	878138.689671	43.837965
3503.452405	878094.367962	43.842970
3503.740072	878043.720971	43.847975
3503.753916	877987.496398	43.852980
3503.645290	877933.230195	43.857985
3503.290525	877881.427473	43.862989
3502.950320	877830.106587	43.867994
3503.397568	877783.017770	43.872999
3503.135688	877749.907762	43.878004
3503.449565	877694.503415	43.883009
3503.533596	877643.014063	43.888013
3503.798032	877582.478923	43.893018
3503.603208	877527.156810	43.898023
3502.985025	877485.379128	43.903028
3503.280895	877435.694994	43.908033
3503.152662	877401.009890	43.913037
3503.120818	877345.077543	43.918042
3503.357002	877304.805904	43.923047
3503.259387	877257.705712	43.928052
3503.270695	877219.700333	43.933057
3503.323119	877180.815395	43.938061
3503.305944	877128.465680	43.943066
3503.748895	877077.106150	43.948071
3503.140016	877030.379223	43.953076
3503.061038	876980.849965	43.958081
3503.084673	876932.660725	43.963085
3503.298243	876890.063111	43.968090
3503.474077	876838.648559	43.973095
3503.488245	876793.368374	43.978100
3503.333415	876739.195732	43.983105
3503.192200	876695.103864	43.988109
3503.294141	876644.572406	43.993114
3503.535226	876595.568927	43.998119
3503.428695	876561.650972	44.003124
3503.568824	876501.610012	44.008129
3503.242825	876454.250146	44.013133
3503.189962	876401.415052	44.018138
3503.425962	876358.809909	44.023143
3503.497386	876316.619425	44.028148
3503.570711	876259.786789	44.033153
3503.628684	876212.167792	44.038157
3503.196057	876156.484129	44.043162
3503.330284	876112.245559	44.048167
3503.081205	876067.584972	44.053172
3503.207372	876017.916864	44.058177
3503.116662	875973.423409	44.063181
3503.220683	875929.867230	44.068186
3503.183512	875881.679427	44.073191
3503.126022	875841.737102	44.078196
3503.054784	875790.935958	44.083201
3503.176776	875754.454452	44.088205
3503.122059	875707.043892	44.093210
3503.168453	875653.119047	44.098215
3502.961091	875622.024546	44.103220
3503.033515	875568.191612	44.108225
3502.868378	875531.271156	44.113229
3502.773483	875495.405638	44.118234
3502.798683	875466.405485	44.123239
3503.156180	875423.967543	44.128244
3502.879924	875380.954859	44.133249
3502.890265	875336.246001	44.138253
3503.023108	875303.251170	44.143258
3503.151102	875258.328380	44.148263
3502.911182	875212.205108	44.153268
3503.326647	875170.143722	44.158273
3503.147558	875126.919217	44.163277
3502.825221	875083.814980	44.168282
3502.841396	875037.454187	44.173287
3502.832396	875011.269973	44.178292
3502.957793	874961.787091	44.183297
3502.723452	874926.813965	44.188301
3503.066745	874888.253956	44.193306
3503.105408	874850.616768	44.198311
3502.954662	874804.960564	44.203316
3502.861620	874765.307788	44.208321
3502.440172	874733.855930	44.213325
3502.492664	874687.680393	44.218330
3503.193209	874655.364341	44.223335
3502.911775	874611.377008	44.228340
3502.722778	874575.327433	44.233345
3502.473445	874542.488319	44.238349
3502.510509	874513.481542	44.243354
3502.553904	874473.901329	44.248359
3502.500060	874442.484351	44.253364
3503.057861	874414.749212	44.258369
3502.869494	874379.377299	44.263373
3502.586540	874339.655965	44.268378
3503.169063	874303.865611	44.273383
3502.709361	874259.808039	44.278388
3502.975295	874222.808397	44.283393
3503.050229	874190.980880	44.288397
3502.887835	874150.559431	44.293402
3502.907873	874103.899700	44.298407
3502.653268	874078.721819	44.303412
3502.721090	874038.067675	44.308417
3502.606219	873990.653275	44.313421
3502.431706	873953.239510	44.318426
3502.817253	873918.934316	44.323431
3502.577145	873888.127100	44.328436
3502.905640	873845.197623	44.333441
3502.934947	873813.569606	44.338445
3502.785247	873771.882430	44.343450
3503.061887	873733.034882	44.348455
3502.679012	873706.518477	44.353460
3502.697449	873658.691437	44.358465
3502.857137	873627.817002	44.363469
3502.657857	873591.666127	44.368474
3502.627126	873562.471853	44.373479
3502.630715	873538.122210	44.378484
3502.850666	873499.573501	44.383489
3502.632192	873459.835645	44.388493
3502.734701	873420.529693	44.393498
3502.553028	873398.538250	44.398503
3502.198514	873362.702587	44.403508
3502.582143	873334.894099	44.408513
3502.718972	873300.432288	44.413517
3503.024431	873265.942496	44.418522
3502.949629	873221.522750	44.423527
3502.675850	873192.075656	44.428532
3502.933743	873145.369202	44.433537
3502.812387	873117.254833	44.438541
3502.533666	873071.121280	44.443546
3502.853121	873039.926420	44.448551
3502.880565	873006.548111	44.453556
3502.949980	872977.528496	44.458561
3502.814573	872924.967026	44.463565
3502.596571	872897.255612	44.468570
3502.824537	872857.343152	44.473575
3502.242296	872825.810627	44.478580
3502.794237	872782.448583	44.483585
3502.686363	872754.815382	44.488589
3502.423731	872728.080744	44.493594
3502.783276	872684.167552	44.498599
3502.419573	872673.360984	44.503604
3502.707976	872622.570446	44.508609
3502.562220	872586.016534	44.513613
3502.539796	872563.510640	44.518618
3502.555556	872530.519680	44.523623
3502.139594	872511.668348	44.528628
3502.438263	872474.070275	44.533633
3502.488904	872449.320315	44.538637
3502.344926	872420.527192	44.543642
3502.584285	872394.387537	44.548647
3502.208946	872358.743296	44.553652
3502.226377	872320.608422	44.558657
3502.453374	872293.597106	44.563661
3502.244250	872264.522873	44.568666
3502.998763	872237.327364	44.573671
3502.207485	872215.431970	44.578676
3502.472987	872167.649257	44.583681
3502.575079	872142.695484	44.588685
3502.252504	872109.757932	44.593690
3502.539865	872077.204872	44.598695
3502.371887	872054.721033	44.603700
3502.263849	872021.456549	44.608705
3502.203393	871989.930648	44.613709
3502.453614	871969.221229	44.618714
3502.917255	871942.363402	44.623719
3502.608328	871915.535701	44.628724
3502.493123	871874.508771	44.633729
3502.339139	871851.730752	44.638733
3502.234428	871816.038669	44.643738
3502.744959	871793.927243	44.648743
3502.428013	871777.289114	44.653748
3502.506333	871740.984204	44.658753
3502.542972	871708.373400	44.663757
3502.337927	871682.594955	44.668762
3502.521537	871648.795146	44.673767
3502.205249	871626.916360	44.678772
3502.479293	871582.523938	44.683777
3502.575263	871560.965151	44.688781
3502.200257	871539.192757	44.693786
3502.325954	871502.975633	44.698791
3502.441351	871474.523367	44.703796
3502.682471	871447.020678	44.708801
3502.102580	871414.218710	44.713805
3502.158002	871388.104948	44.718810
3502.306871	871350.427426	44.723815
3502.235089	871344.228459	44.728820
3502.507446	871302.066247	44.733825
3502.411803	871280.732106	44.738829
3502.408010	871251.230912	44.743834
3502.320258	871229.701197	44.748839
3502.439615	871193.289145	44.753844
3502.541464	871167.069720	44.758849
3502.506076	871133.497166	44.763853
3502.239117	871110.055588	44.768858
3502.708989	871073.099815	44.773863
3502.211475	871053.674995	44.778868
3502.436975	871011.615501	44.783873
3502.385967	870996.484168	44.788877
3502.371838	870968.924280	44.793882
3502.487446	870929.696775	44.798887
3502.284231	870909.640692	44.803892
3502.563197	870888.825739	44.808897
3502.112671	870849.496875	44.813901
3502.007862	870841.070620	44.818906
3502.559002	870806.429070	44.823911
3502.210815	870776.691109	44.828916
3501.976522	870749.166478	44.833921
3502.209453	870728.843823	44.838925
3502.381564	870700.378523	44.843930
3502.477226	870664.258313	44.848935
3502.242558	870658.861911	44.853940
3502.329912	870615.075386	44.858945
3502.346025	870598.864368	44.863949
3502.219267	870564.236043	44.868954
3501.983897	870550.104521	44.873959
3502.235510	870524.342886	44.878964
3502.369406	870491.709408	44.883969
3502.394242	870470.449577	44.888973
3502.004797	870446.054980	44.893978
3502.394173	870432.402606	44.898983
3501.934505	870406.272350	44.903988
3502.385699	870364.947598	44.908993
3502.405387	870354.753060	44.913997
3502.214798	870322.754481	44.919002
3502.493673	870290.969569	44.924007
3502.354590	870271.094895	44.929012
3502.151381	870235.021329	44.934017
3502.437621	870198.284530	44.939021
3502.254560	870176.766717	44.944026
3502.395398	870143.741943	44.949031
3502.143092	870128.156253	44.954036
3502.329650	870092.502932	44.959041
3502.112070	870085.064834	44.964045
3502.171288	870055.159090	44.969050
3502.356307	870031.638806	44.974055
3502.389525	870012.705541	44.979060
3502.348407	869979.321572	44.984065
3502.287436	869953.803113	44.989069
3502.028220	869943.459690	44.994074
3502.331779	869917.395683	44.999079
3501.949625	869886.202865	45.004084
3502.134982	869861.517041	45.009089
3502.066347	869834.543308	45.014093
3502.252579	869811.798512	45.019098
3502.276023	869791.992536	45.024103
3502.248896	869764.526301	45.029108
3502.183150	869747.549901	45.034113
3502.040612	869723.111668	45.039117
3502.341158	869694.426279	45.044122
3502.497762	869678.674975	45.049127
3502.188489	869650.089843	45.054132
3502.147069	869629.905729	45.059137
3502.005792	869597.021487	45.064141
3502.226789	869574.852500	45.069146
3502.195416	869537.484462	45.074151
3502.083507	869521.194540	45.079156
3502.054251	869504.793882	45.084161
3501.987503	869469.081506	45.089165
3501.776017	869453.390253	45.094170
3502.294483	869437.869924	45.099175
3502.301048	869411.949725	45.104180
3502.417707	869391.059231	45.109185
3502.205749	869358.767781	45.114189
3501.878362	869339.988874	45.119194
3502.309112	869311.668510	45.124199
3501.983586	869300.849509	45.129204
3502.105412	869275.395117	45.134209
3502.011836	869249.296555	45.139213
3501.858578	869230.974009	45.144218
3502.128292	869213.067116	45.149223
3502.025163	869183.474999	45.154228
3501.905754	869164.175878	45.159233
3502.049328	869150.852326	45.164237
3501.984921	869123.680532	45.169242
3502.346117	869103.719553	45.174247
3502.025419	869078.725554	45.179252
3501.900143	869045.447320	45.184257
3502.098053	869038.327789	45.189261
3501.782161	869023.040934	45.194266
3502.000992	868989.123203	45.199271
3501.585166	868989.677163	45.204276
3501.841918	868967.888371	45.209281
3501.715465	868936.065966	45.214285
3501.802726	868927.702449	45.219290
3502.018009	868919.414912	45.224295
3502.138099	868892.017503	45.229300
3501.714458	868870.437537	45.234305
3502.128959	868860.855000	45.239309
3502.102085	868835.617408	45.244314
3502.132175	868809.011128	45.249319
3502.067556	868796.206516	45.254324
3501.671066	868768.116963	45.259329
3501.591875	868762.693223	45.264333
3501.802915	868751.687739	45.269338
3501.817186	868723.239042	45.274343
3501.366011	868708.750365	45.279348
3501.689686	868692.386423	45.284353
3501.756880	868682.084122	45.289357
3502.037876	868682.037867	45.294362
3502.253805	868638.798223	45.299367
3501.666402	868633.069741	45.304372
3501.845607	868614.108002	45.309377
3501.995182	868587.772320	45.314381
3501.858490	868573.425681	45.319386
3502.323395	868555.096312	45.324391
3501.914476	868532.444714	45.329396
3502.100751	868509.306610	45.334401
3501.906852	868498.658648	45.339405
3501.797191	868465.568801	45.344410
3502.420029	868443.814886	45.349415
3502.282672	868430.147653	45.354420
3502.129559	868403.763941	45.359425
3501.857714	868376.622934	45.364429
3501.930376	868343.987840	45.369434
3501.689579	868326.647877	45.374439
3501.912954	868329.621006	45.379444
3502.130466	868301.622292	45.384449
3502.340525	868278.382286	45.389453
3502.176435	868262.097533	45.394458
3501.979818	868233.681259	45.399463
3501.952529	868221.160552	45.404468
3502.314575	868195.662001	45.409473
3502.165375	868174.131402	45.414477
3502.045636	868153.372641	45.419482
3502.519292	868113.290921	45.424487
3502.586733	868111.435011	45.429492
3502.287636	868081.481350	45.434497
3502.585325	868057.449275	45.439501
3502.246511	868027.890280	45.444506
3502.484433	867998.041923	45.449511
3502.188463	867985.564991	45.454516
3501.986617	867944.816647	45.459521
3502.009500	867924.227794	45.464525
3501.825619	867904.935237	45.469530
3502.035540	867890.724058	45.474535
3501.985884	867873.545493	45.479540
3501.848464	867856.381339	45.484545
3502.015399	867847.517687	45.489549
3501.808938	867813.760484	45.494554
3502.081327	867781.672038	45.499559
3501.911593	867780.146407	45.504564
3501.785012	867747.540896	45.509569
3502.059937	867728.269284	45.514573
3502.032539	867722.447657	45.519578
3502.145772	867687.471837	45.524583
3502.198666	867679.889074	45.529588
3501.815661	867655.870435	45.534593
3501.820361	867627.223911	45.539597
3501.854797	867612.652569	45.544602
3501.892054	867608.179646	45.549607
3501.936868	867576.904440	45.554612
3501.627693	867559.282204	45.559617
3501.566301	867555.311023	45.564621
3501.282095	867544.287818	45.569626
3501.812658	867529.051900	45.574631
3501.548620	867508.703106	45.579636
3501.836618	867490.205430	45.584641
3501.894250	867485.243525	45.589645
3501.717954	867475.367698	45.594650
3501.875118	867437.858403	45.599655
3501.693250	867426.623906	45.604660
3501.944825	867425.417204	45.609665
3502.031922	867397.047331	45.614669
3501.725726	867383.405527	45.619674
3501.876586	867358.715092	45.624679
3501.897205	867352.011214	45.629684
3501.686976	867318.737392	45.634689
3501.632985	867304.859639	45.639693
3501.337963	867305.976492	45.644698
3501.655982	867298.835118	45.649703
3501.569663	867287.875949	45.654708
3501.659557	867258.533860	45.659713
3501.723215	867244.442364	45.664717
3501.841061	867244.617210	45.669722
3502.134392	867223.592956	45.674727
3501.787190	867196.944579	45.679732
3501.726270	867181.805234	45.684737
3501.752565	867168.787946	45.689741
3501.686009	867155.980151	45.694746
3501.900232	867143.417408	45.699751
3501.716267	867138.300796	45.704756
3501.718644	867128.200735	45.709761
3501.824932	867099.826298	45.714765
3501.844093	867080.303411	45.719770
3501.926762	867072.035182	45.724775
3501.736036	867054.294834	45.729780
3501.920833	867028.820543	45.734785
3501.759212	867020.883835	45.739789
3501.656640	867014.296990	45.744794
3501.879301	866981.435554	45.749799
3501.579913	866959.439764	45.754804
3501.528376	866948.377130	45.759809
3501.805436	866935.997833	45.764813
3501.827593	866908.995978	45.769818
3501.872728	866830.518177	45.774823
3501.799264	866698.157751	45.779828
3501.663606	866503.549300	45.784833
3501.521533	866266.394328	45.789837
3501.268244	865967.764485	45.794842
3501.789792	865605.853329	45.799847
3501.390399	865175.780251	45.804852
3501.278563	864695.498997	45.809857
3501.242969	864153.276037	45.814861
3500.715796	863566.290260	45.819866
3500.863054	862899.254462	45.824871
3500.454432	862186.556771	45.829876
3500.504872	861393.117565	45.834881
3500.116234	860539.080436	45.839885
3499.529535	859642.465680	45.844890
3499.701687	858651.555634	45.849895
3499.163491	857614.498704	45.854900
3498.930746	856494.234395	45.859905
3498.770213	855321.406073	45.864909
3497.984923	854074.688518	45.869914
3497.825888	852760.450671	45.874919
3497.446695	851384.534235	45.879924
3496.973153	849927.498536	45.884929
3496.831931	848398.471291	45.889933
3496.152365	846808.067264	45.894938
3495.723311	845143.538656	45.899943
3495.132452	843406.358421	45.904948
3494.346069	841593.402116	45.909953
3494.099682	839717.166206	45.914957
3493.251728	837780.663492	45.919962
3492.842970	835753.949478	45.924967
3492.560859	833666.674450	45.929972
3491.615492	831505.825111	45.934977
3491.002730	829264.376572	45.939981
3490.110197	826971.622472	45.944986
3489.785286	824591.001846	45.949991
3488.712417	822164.600455	45.954996
3488.124236	819654.156391	45.960001
3487.368718	817068.398618	45.965005
3486.342410	814425.280021	45.970010
3485.942436	811705.243580	45.975015
3484.703487	808925.545841	45.980020
3483.987574	806066.385402	45.985025
3483.453441	803150.335080	45.990029
3482.186084	800151.624786	45.995034
3481.347577	797083.217252	46.000039
3480.050754	793959.810061	46.005044
3479.111249	790764.697573	46.010049
3477.986082	787502.846921	46.015053
3476.945206	784191.737696	46.020058
3476.138138	780792.914081	46.025063
3474.780652	777342.867401	46.030068
3473.734924	773817.954939	46.035073
3472.724993	770222.562443	46.040077
3471.743081	766570.109620	46.045082
3470.219615	762841.979591	46.050087
3468.858091	759056.019588	46.055092
3467.920012	755206.834668	46.060097
3466.626188	751285.535599	46.065101
3465.244560	747319.117787	46.070106
3464.159682	743256.788480	46.075111
3462.654188	739149.838184	46.080116
3461.419990	734978.356373	46.085121
3460.304663	730742.785087	46.090125
3458.566983	726435.638009	46.095130
3457.534922	722068.604424	46.100135
3455.698707	717634.870155	46.105140
3454.104344	713129.964627	46.110145
3452.949759	708566.381054	46.115149
3451.291346	703951.214581	46.120154
3449.963095	699258.029397	46.125159
3448.038522	694507.224530	46.130164
3446.261716	689696.576190	46.135169
3444.588959	684831.604413	46.140173
3442.763505	679895.610475	46.145178
3441.237595	674901.199936	46.150183
3439.742852	669864.965506	46.155188
3438.026570	664743.561062	46.160193
3436.124001	659559.646842	46.165197
3434.011156	654321.857711	46.170202
3432.455563	649019.927646	46.175207
3430.655731	643665.979622	46.180212
3428.487083	638248.439168	46.185217
3426.148447	632777.729430	46.190221
3424.158408	627264.645206	46.195226
3422.613576	621684.800574	46.200231
3420.223435	616054.044702	46.205236
3418.198123	610366.732540	46.210241
3416.410229	604628.922063	46.215245
3413.838769	598834.230431	46.220250
3411.717200	592985.235440	46.225255
3409.786565	587083.411486	46.230260
3407.552763	581139.126319	46.235265
3405.342386	575125.709270	46.240269
3402.798967	569075.691845	46.245274
3400.836782	562957.560286	46.250279
3397.663529	556809.862911	46.255284
3395.736802	550596.531905	46.260289
3393.608545	544347.984131	46.265293
3390.927138	538056.576754	46.270298
3388.587721	531699.712832	46.275303
3385.944941	525307.421628	46.280308
3382.942565	518854.075736	46.285313
3380.687923	512363.589899	46.290317
3377.989079	505841.443790	46.295322
3375.624259	499259.980489	46.300327
3372.638377	492650.121512	46.305332
3370.022151	485977.176913	46.310337
3367.305692	479282.037864	46.315341
3364.168199	472554.882590	46.320346
3361.660477	465766.295412	46.325351
3358.705487	458956.459648	46.330356
3355.455056	452100.463660	46.335361
3352.603982	445212.277879	46.340365
3349.742227	438287.557194	46.345370
3346.811492	431327.934337	46.350375
3343.234701	424349.548849	46.355380
3340.270774	417329.970542	46.360385
3337.415611	410279.341067	46.365389
3334.184752	403199.022489	46.370394
3331.076993	396090.726245	46.375399
3327.885041	388948.328843	46.380404
3323.989958	381788.065010	46.385409
3320.613627	374598.701402	46.390413
3317.054297	367389.938858	46.395418
3313.734952	360154.514212	46.400423
3310.287977	352902.488626	46.405428
3306.716387	345645.448063	46.410433
3303.514786	338358.743388	46.415437
3299.945355	331054.846051	46.420442
3296.480469	323726.486850	46.425447
3292.669589	316394.193916	46.430452
3288.805339	309029.167953	46.435457
3285.224235	301656.547801	46.440461
3281.087527	294282.552105	46.445466
3277.379844	286900.266118	46.450471
3273.766312	279499.324234	46.455476
3269.635720	272108.906082	46.460481
3265.860422	264694.661919	46.465485
3261.269895	257286.426248	46.470490
3257.530629	249868.615602	46.475495
3253.362456	242479.003724	46.480500
3249.168261	235055.864470	46.485505
3245.333951	227641.561200	46.490509
3240.834863	220164.960859	46.495514
3236.804155	212748.156380	46.500519
3232.303977	205360.480760	46.505524
3228.031546	197959.460631	46.510529
3223.761957	190576.914067	46.515533
3219.197288	183227.273122	46.520538
3214.736929	175871.775433	46.525543
3210.331141	168520.834075	46.530548
3205.243273	161193.198475	46.535553
3200.302258	153888.372250	46.540557
3195.416005	146626.429340	46.545562
3191.043903	139362.897095	46.550567
3185.970902	132134.776329	46.555572
3180.837275	124931.587584	46.560577
3175.639113	117771.954256	46.565581
3170.518498	110638.729697	46.570586
3165.076211	103542.271354	46.575591
3159.062183	96505.186159	46.580596
3153.394265	89496.722281	46.585601
3147.436584	82559.436752	46.590605
3140.192551	75686.635333	46.595610
3133.463966	68890.386679	46.600615
3124.531839	62217.299858	46.605620
3108.510453	55842.384426	46.610625
3089.434806	49706.376784	46.615629
3071.347745	43799.946825	46.620634
3054.071712	38178.958091	46.625639
3037.527580	32854.096464	46.630644
3021.112616	27841.040345	46.635649
3005.823487	23146.900881	46.640653
2989.951751	18789.189089	46.645658
2974.165317	14777.373279	46.650663
2954.655479	11204.890830	46.655668
2932.926800	8056.024591	46.660673
2911.621128	5313.702268	46.665677
2891.716619	2971.749956	46.670682
2871.660759	1029.960024	46.675687
2823.916044	319.794460	46.680692
2773.027648	317.045681	46.685697
2752.571778	322.807876	46.690701
2756.724166	307.250246	46.695706
2773.570847	301.574885	46.700711
2792.817160	298.128326	46.705716
2807.342973	293.006497	46.710721
2815.490881	288.853283	46.715725
2816.929032	306.008653	46.720730
2814.604493	303.652296	46.725735
2810.483452	293.102258	46.730740
2806.517982	292.527097	46.735745
2803.288456	287.252959	46.740749
2799.735493	291.415037	46.745754
2796.657118	287.420795	46.750759
2794.692951	289.892379	46.755764
2791.654756	286.648518	46.760769
2789.491411	279.887736	46.765773
2786.845852	287.491742	46.770778
2784.150253	281.066246	46.775783
2780.642043	288.708388	46.780788
2777.309338	282.376172	46.785793
2774.586434	271.280149	46.790797
2771.513533	284.919538	46.795802
2768.473637	279.131046	46.800807
2765.457232	275.468005	46.805812
2761.998619	284.904893	46.810817
2759.004207	267.869470	46.815821
2755.492511	277.920956	46.820826
2752.198985	264.161442	46.825831
2749.328373	270.056112	46.830836
2745.712259	269.527159	46.835841
2742.797184	263.276048	46.840845
2739.506257	264.568196	46.845850
2736.356275	263.137844	46.850855
2732.820664	266.737434	46.855860
2729.198108	270.926824	46.860865
2726.029151	257.623561	46.865869
2722.145277	264.225360	46.870874
2719.112734	272.981782	46.875879
2716.142404	265.088840	46.880884
2712.859677	270.549885	46.885889
2709.042602	256.804572	46.890893
2705.675410	267.795662	46.895898
2702.432374	261.891153	46.900903
2699.180273	260.395976	46.905908
2695.761154	262.090568	46.910913
2692.455060	260.665481	46.915917
2689.281749	263.725776	46.920922
2685.477996	261.002601	46.925927
2681.973976	264.063004	46.930932
2678.604516	260.156347	46.935937
2675.330520	257.095931	46.940941
2671.645495	255.736543	46.945946
2668.562268	249.976986	46.950951
2664.999570	257.758816	46.955956
2661.147579	259.772327	46.960961
2658.224279	249.293597	46.965965
2654.362315	261.598162	46.970970
2651.598305	254.309822	46.975975
2648.632762	256.327833	46.980980
2644.234065	267.474963	46.985985
2640.909356	247.693086	46.990989
2637.164990	254.799217	46.995994
2633.775230	251.313124	47.000999
2630.850114	252.330661	47.006004
2627.216877	255.365850	47.011009
2623.727501	253.265361	47.016013
2620.303579	248.478119	47.021018
2617.046407	244.955162	47.026023
2613.921137	243.034958	47.031028
2610.131432	248.059133	47.036033
2606.497599	239.141058	47.041037
2602.882848	249.405781	47.046042
2599.539329	245.766051	47.051047
2596.027342	246.431702	47.056052
2592.445094	245.684933	47.061057
2589.078088	247.757784	47.066061
2585.520940	243.464597	47.071066
2581.900530	246.209580	47.076071
2578.557738	242.272155	47.081076
2574.849873	246.100377	47.086081
2572.213661	242.584302	47.091085
2568.405443	243.689200	47.096090
2564.976487	242.450639	47.101095
2561.844729	243.147102	47.106100
2558.038467	236.418810	47.111105
2554.696721	236.476605	47.116109
2550.898354	243.043880	47.121114
2547.501114	244.229369	47.126119
2543.677205	235.583080	47.131124
2540.512125	243.299359	47.136129
2536.950108	236.419473	47.141133
2533.276844	239.618809	47.146138
2530.075165	237.174107	47.151143
2526.437912	231.549900	47.156148
2523.423053	233.137232	47.161153
2519.895417	234.612644	47.166157
2516.466447	238.855866	47.171162
2513.024137	234.885579	47.176167
2509.560118	233.357621	47.181172
2505.268612	233.856767	47.186177
2501.910292	231.433201	47.191181
2498.774734	226.748837	47.196186
2495.701929	240.321994	47.201191
2492.099701	228.242133	47.206196
2488.397366	231.520102	47.211201
2484.757357	230.153033	47.216205
2481.645487	231.162405	47.221210
2478.406646	234.258897	47.226215
2474.798464	223.520181	47.231220
2470.727220	232.918805	47.236225
2467.241875	223.889713	47.241229
2463.734818	231.816399	47.246234
2460.482150	221.011914	47.251239
2456.937081	226.540671	47.256244
2453.516354	229.825467	47.261249
2450.290475	221.382687	47.266253
2446.422647	228.076938	47.271258
2442.901205	223.719559	47.276263
2439.424749	223.059835	47.281268
2435.594824	230.325061	47.286273
2432.790794	225.989386	47.291277
2429.480323	227.284759	47.296282
2426.023981	224.869533	47.301287
2421.956900	221.696687	47.306292
2418.388890	231.254026	47.311297
2415.325581	219.944110	47.316301
2411.470907	228.685205	47.321306
2407.821231	221.215246	47.326311
2404.709753	225.900272	47.331316
2401.241798	217.880133	47.336321
2397.990056	220.507947	47.341325
2393.927234	223.782732	47.346330
2390.470818	221.334786	47.351335
2387.320687	212.712407	47.356340
2383.971474	221.451584	47.361345
2380.181702	207.558840	47.366349
2376.217726	221.715069	47.371354
2373.134922	206.495539	47.376359
2369.863282	214.666401	47.381364
2366.204310	217.647207	47.386369
2363.065294	205.997978	47.391373
2359.437589	216.046118	47.396378
2356.249392	216.748474	47.401383
2352.954564	220.424993	47.406388
2349.010840	222.413029	47.411393
2345.256395	210.624647	47.416397
2341.290232	222.004480	47.421402
2337.927790	210.986343	47.426407
2334.834034	217.686487	47.431412
2331.463165	212.893673	47.436417
2327.602257	217.166677	47.441421
2324.438248	212.230591	47.446426
2320.776952	210.441300	47.451431
2317.261439	205.764141	47.456436
2313.471698	223.166317	47.461441
2310.529761	209.746810	47.466445
2306.669374	213.478240	47.471450
2303.067642	215.199487	47.476455
2299.808595	220.623110	47.481460
2296.148745	213.728594	47.486465
2293.035857	201.334491	47.491469
2289.294843	214.194141	47.496474
2286.273931	212.812439	47.501479
2282.706293	213.643790	47.506484
2278.835627	208.973588	47.511489
2275.640719	208.484772	47.516493
2272.007363	213.792006	47.521498
2268.112685	218.488794	47.526503
2265.007696	212.231086	47.531508
2261.372930	209.870699	47.536513
2257.972833	210.586788	47.541517
2254.317607	217.912294	47.546522
2250.706900	208.056703	47.551527
2247.497289	205.572459	47.556532
2243.791053	209.587323	47.561537
2240.512081	204.043131	47.566541
2236.918973	211.938374	47.571546
2233.709360	210.827826	47.576551
2230.072594	202.349060	47.581556
2226.547075	211.125918	47.586561
2223.391672	196.871064	47.591565
2219.469803	201.908443	47.596570
2215.546186	212.349096	47.601575
2211.996460	201.390603	47.606580
2208.743670	209.480297	47.611585
2205.380280	210.428355	47.616589
2201.900994	203.935101	47.621594
2198.607262	199.745947	47.626599
2195.031542	205.122454	47.631604
2191.536824	199.899669	47.636609
2188.144087	203.398863	47.641613
2184.289718	192.655083	47.646618
2180.947323	197.116093	47.651623
2177.169438	205.011292	47.656628
2173.623433	202.788074	47.661633
2170.203443	198.536510	47.666637
2167.056601	208.545431	47.671642
2163.719245	201.351305	47.676647
2160.319386	201.729970	47.681652
2156.181874	208.188135	47.686657
2153.123221	192.609199	47.691661
2149.432755	204.761802	47.696666
2145.823514	197.501481	47.701671
2142.584894	201.515970	47.706676
2138.817181	205.121514	47.711681
2135.579766	202.642729	47.716685
2132.085304	203.248386	47.721690
2128.875865	195.024957	47.726695
2125.043099	202.935569	47.731700
2121.391764	199.490486	47.736705
2118.019999	192.675251	47.741709
2113.832408	202.131218	47.746714
2110.607631	196.807287	47.751719
2107.700940	196.404590	47.756724
2103.897509	200.546705	47.761729
2100.518458	194.984215	47.766733
2096.985804	199.562736	47.771738
2093.754063	191.367884	47.776743
2090.456141	200.187753	47.781748
2086.258053	200.053374	47.786753
2082.912670	206.574580	47.791757
2079.254313	199.706250	47.796762
2075.754501	198.098480	47.801767
2072.283120	196.114624	47.806772
2068.709371	199.591493	47.811777
2065.738101	197.719240	47.816781
2062.161034	194.896389	47.821786
2058.714314	196.507358	47.826791
2055.444147	191.978744	47.831796
2051.219197	198.707376	47.836801
2048.129110	198.063067	47.841805
2044.334974	203.264393	47.846810
2040.917354	202.059067	47.851815
2037.708792	194.089737	47.856820
2034.250610	194.279401	47.861825
2030.475135	196.607149	47.866829
2026.630660	193.409929	47.871834
2023.332388	198.017679	47.876839
2020.284738	191.963415	47.881844
2016.120642	190.793371	47.886849
2012.820254	193.962672	47.891853
2009.262166	199.122475	47.896858
2005.632071	196.160223	47.901863
2002.750923	192.779266	47.906868
1999.168771	192.109885	47.911873
1995.634066	184.499343	47.916877
1991.827501	191.354488	47.921882
1988.606846	189.143395	47.926887
1985.379664	183.776344	47.931892
1981.392126	194.637975	47.936897
1977.658193	186.575880	47.941901
1974.087978	186.350930	47.946906
1971.045384	189.862889	47.951911
1967.649317	186.691517	47.956916
1964.355996	197.305503	47.961921
1960.646407	183.740536	47.966925
1957.023091	186.980571	47.971930
1953.608828	188.443971	47.976935
1949.857142	184.404245	47.981940
1946.112952	197.979781	47.986945
1943.163869	177.449443	47.991949
1939.821235	190.986483	47.996954
1936.330714	180.509244	48.001959
1932.592338	177.229658	48.006964
1928.519002	191.389024	48.011969
1924.995386	181.687477	48.016973
1921.686051	191.042734	48.021978
1918.381240	188.080307	48.026983
1915.517706	181.983082	48.031988
1911.610113	191.990694	48.036993
1907.865373	183.507153	48.041997
1904.452621	187.259868	48.047002
1900.787458	188.727250	48.052007
1897.530461	184.015224	48.057012
1893.709401	199.571952	48.062017
1890.727231	181.775928	48.067021
1886.808420	190.690571	48.072026
1883.380583	184.226771	48.077031
1880.096183	186.668888	48.082036
1876.424419	183.632122	48.087041
1872.838886	184.868510	48.092045
1869.513169	183.340479	48.097050
1866.073821	181.917655	48.102055
1862.305082	184.677774	48.107060
1858.605099	179.166907	48.112065
1855.244103	174.440914	48.117069
1852.039557	181.500421	48.122074
1848.243409	175.393499	48.127079
1845.155618	179.206638	48.132084
1841.138253	184.531020	48.137089
1837.996256	176.313259	48.142093
1834.623081	185.839349	48.147098
1831.310196	184.407896	48.152103
1827.451884	181.549397	48.157108
1823.544840	190.320847	48.162113
1820.589150	189.394986	48.167117
1816.900543	188.519545	48.172122
1813.467189	188.145613	48.177127
1809.697516	180.299146	48.182132
1806.229816	176.061469	48.187137
1803.093540	179.872579	48.192141
1799.249876	184.620487	48.197146
1795.698735	183.475682	48.202151
1792.526611	181.705065	48.207156
1788.812763	184.221734	48.212161
1785.483530	176.284773	48.217165
1781.707470	176.783276	48.222170
1778.422484	185.790237	48.227175
1774.846653	177.798311	48.232180
1771.222324	188.577000	48.237185
1768.092565	181.532815	48.242189
1764.323623	187.264575	48.247194
1760.963576	179.241748	48.252199
1757.507313	186.710935	48.257204
1753.954611	184.680367	48.262209
1750.603161	178.645701	48.267213
1746.644661	188.545803	48.272218
1743.042803	188.151016	48.277223
1739.824913	177.658509	48.282228
1736.315741	183.400655	48.287233
1732.767405	181.207762	48.292237
1729.005474	190.368339	48.297242
1725.954172	186.507918	48.302247
1722.669508	183.713793	48.307252
1719.073164	177.271255	48.312257
1715.339298	168.861085	48.317261
1711.843238	183.154534	48.322266
1707.986477	172.155456	48.327271
1704.811920	169.872617	48.332276
1701.377196	179.770281	48.337281
1698.066719	177.208761	48.342285
1694.511261	173.966641	48.347290
1690.520123	177.884913	48.352295
1687.582690	169.726616	48.357300
1683.666741	174.249154	48.362305
1680.504740	166.771092	48.367309
1676.493631	185.662793	48.372314
1673.127429	171.892972	48.377319
1669.800491	169.481803	48.382324
1666.052565	176.180276	48.387329
1663.186129	165.254040	48.392333
1659.221315	174.360360	48.397338
1655.739908	179.308224	48.402343
1652.520943	168.204614	48.407348
1648.602082	187.917021	48.412353
1645.070770	166.669320	48.417357
1642.006559	170.846524	48.422362
1638.402009	170.017922	48.427367
1635.052622	165.808590	48.432372
1631.329606	174.332695	48.437377
1627.994819	157.231396	48.442381
1624.138053	166.390534	48.447386
1620.450074	173.247661	48.452391
1617.156010	160.544830	48.457396
1613.641865	164.587805	48.462401
1610.459403	163.711389	48.467405
1606.669584	166.090178	48.472410
1602.975279	170.692191	48.477415
1600.404846	168.880309	48.482420
1596.352594	177.090803	48.487425
1592.912772	171.199135	48.492429
1589.235704	170.545555	48.497434
1585.525058	171.137798	48.502439
1582.023127	160.220525	48.507444
1578.669260	174.129816	48.512449
1575.142867	165.370735	48.517453
1571.537780	175.343988	48.522458
1567.697863	167.133616	48.527463
1564.461176	163.826892	48.532468
1561.588011	167.058111	48.537473
1558.103231	163.180637	48.542477
1554.177189	168.150928	48.547482
1550.698187	169.758314	48.552487
1547.392662	157.199522	48.557492
1543.682674	167.561317	48.562497
1540.128047	163.321443	48.567501
1536.675739	161.281563	48.572506
1532.925115	166.408973	48.577511
1529.747095	167.271613	48.582516
1526.155490	163.904175	48.587521
1522.598574	167.119542	48.592525
1519.161377	166.383755	48.597530
1515.401343	172.537316	48.602535
1512.569403	161.506625	48.607540
1508.948264	160.572724	48.612545
1505.443517	157.901764	48.617549
1501.923157	158.763569	48.622554
1498.042078	175.049546	48.627559
1494.559531	161.422058	48.632564
1490.821209	167.561785	48.637569
1487.726490	162.500408	48.642573
1484.262672	158.989934	48.647578
1480.755644	168.071844	48.652583
1477.038450	163.258386	48.657588
1473.444808	165.851730	48.662593
1470.266317	158.858851	48.667597
1466.874725	162.154486	48.672602
1463.113910	169.323716	48.677607
1459.664280	167.346994	48.682612
1456.226617	164.496458	48.687617
1452.515532	154.051761	48.692621
1448.851233	161.930856	48.697626
1445.460975	169.332104	48.702631
1442.099137	156.889665	48.707636
1438.589758	159.011679	48.712641
1435.384939	157.599558	48.717645
1431.571266	170.452791	48.722650
1427.552792	164.452053	48.727655
1424.715922	166.324799	48.732660
1421.372469	161.085532	48.737665
1417.740026	161.846732	48.742669
1414.221797	162.269174	48.747674
1410.301660	165.517815	48.752679
1407.041318	164.103838	48.757684
1403.540850	161.368312	48.762689
1400.201066	160.911732	48.767693
1396.853284	166.304391	48.772698
1393.153450	171.670976	48.777703
1389.561320	160.370747	48.782708
1385.694451	169.727885	48.787713
1382.619780	169.519363	48.792717
1378.978387	162.638185	48.797722
1375.232383	161.614124	48.802727
1372.091387	167.794338	48.807732
1368.352292	164.652493	48.812737
1365.401774	160.127022	48.817741
1361.586290	157.956083	48.822746
1357.944475	155.419192	48.827751
1354.395150	154.566096	48.832756
1350.839536	166.972385	48.837761
1348.067442	154.449920	48.842765
1344.243559	166.770902	48.847770
1340.720141	165.075045	48.852775
1337.148706	156.775324	48.857780
1332.990956	162.804126	48.862785
1329.842152	156.572317	48.867789
1326.513196	160.699539	48.872794
1322.830652	158.724718	48.877799
1319.520383	156.390386	48.882804
1315.995462	159.639096	48.887809
1312.803558	155.007138	48.892813
1308.786567	155.409288	48.897818
1305.336631	166.667589	48.902823
1302.071686	156.034829	48.907828
1298.543465	159.168852	48.912833
1295.463523	156.005142	48.917837
1291.654177	164.654657	48.922842
1287.891387	156.570133	48.927847
1284.505627	151.442955	48.932852
1280.893257	168.473411	48.937857
1277.579976	153.688190	48.942861
1274.123185	162.397645	48.947866
1270.401891	155.738358	48.952871
1266.993942	155.518306	48.957876
1263.275499	150.798780	48.962881
1259.695301	154.496336	48.967885
1256.529895	156.380272	48.972890
1253.035488	159.047363	48.977895
1249.898650	143.735916	48.982900
1245.620310	149.741307	48.987905
1242.278020	157.289071	48.992909
1239.106972	154.186639	48.997914
1235.428794	154.112318	49.002919
1231.885158	141.634413	49.007924
1228.124341	153.065114	49.012929
1224.983871	153.816770	49.017933
1221.353859	154.980093	49.022938
1218.063739	152.314532	49.027943
1214.579784	156.293007	49.032948
1210.698142	163.005430	49.037953
1207.353456	152.806065	49.042957
1204.062256	152.007111	49.047962
1200.531292	161.174661	49.052967
1197.315278	153.478571	49.057972
1193.244569	155.295733	49.062977
1189.767391	154.243566	49.067981
1186.450993	142.320739	49.072986
1183.164757	152.522537	49.077991
1179.419713	142.328413	49.082996
1175.499902	160.010445	49.088001
1172.295279	158.019294	49.093005
1168.613282	147.879084	49.098010
1165.201486	152.245470	49.103015
1162.054737	151.640723	49.108020
1158.383367	162.474743	49.113025
1155.108360	159.420343	49.118029
1151.596670	151.627538	49.123034
1147.595027	156.135659	49.128039
1144.381577	148.817288	49.133044
1140.932067	154.977408	49.138049
1137.692253	154.332415	49.143053
1133.642405	152.579307	49.148058
1129.851758	155.321910	49.153063
1126.854277	156.990108	49.158068
1123.413999	155.142542	49.163073
1120.047884	145.642609	49.168077
1116.322744	152.093014	49.173082
1112.475419	161.829559	49.178087
1109.352123	146.720432	49.183092
1105.540171	153.422003	49.188097
1102.418242	140.046467	49.193101
1099.131942	144.727621	49.198106
1095.259019	154.497416	49.203111
1092.072183	150.015355	49.208116
1088.180844	153.108337	49.213121
1084.846333	147.705059	49.218125
1081.185518	151.066001	49.223130
1077.333460	156.019899	49.228135
1074.853305	144.529402	49.233140
1071.103468	154.702940	49.238145
1067.482139	147.297753	49.243149
1063.752605	141.976978	49.248154
1060.033558	145.643569	49.253159
1056.693527	147.398249	49.258164
1052.915100	150.670124	49.263169
1049.708452	142.072160	49.268173
1046.530161	145.012344	49.273178
1043.053843	149.412375	49.278183
1039.100304	147.507070	49.283188
1035.545703	146.242665	49.288193
1032.070266	147.141997	49.293197
1028.706234	142.337829	49.298202
1025.014179	156.931471	49.303207
1021.980136	146.436005	49.308212
1018.159406	152.640622	49.313217
1014.768742	152.505914	49.318221
1011.395547	144.243167	49.323226
1007.871880	150.148447	49.328231
1004.360779	148.853982	49.333236
1000.356235	146.304750	49.338241
997.115551	149.258048	49.343245
993.836489	151.470775	49.348250
990.706184	142.280457	49.353255
987.258747	144.514716	49.358260
983.035627	150.005630	49.363265
979.773576	147.247004	49.368269
976.054487	152.521176	49.373274
972.314893	146.160205	49.378279
969.331324	142.025683	49.383284
965.759819	142.948254	49.388289
961.757351	148.782374	49.393293
958.499512	141.924382	49.398298
955.467098	153.025840	49.403303
951.737619	142.923682	49.408308
948.180736	146.490924	49.413313
944.981692	138.490312	49.418317
941.319074	144.700412	49.423322
937.169421	142.394872	49.428327
934.173897	140.728866	49.433332
930.357849	141.989094	49.438337
927.058474	139.023362	49.443341
923.708838	134.872847	49.448346
920.122616	132.504339	49.453351
916.633609	132.984295	49.458356
912.739079	144.341026	49.463361
909.421673	139.478923	49.468365
906.374554	135.262802	49.473370
902.648020	139.622025	49.478375
899.064348	137.974377	49.483380
895.573963	141.815417	49.488385
892.471515	146.466701	49.493389
889.155078	150.190771	49.498394
885.187906	144.525043	49.503399
881.434397	137.434143	49.508404
877.883585	147.117869	49.513409
874.453379	142.641100	49.518413
871.244282	148.689617	49.523418
867.372467	145.615742	49.528423
864.184727	140.056352	49.533428
860.477656	151.927562	49.538433
857.179984	140.173411	49.543437
853.834342	140.498080	49.548442
849.846672	141.245862	49.553447
846.630775	134.352019	49.558452
843.209762	143.845774	49.563457
839.765046	139.257966	49.568461
836.382441	140.212543	49.573466
832.505221	139.106251	49.578471
828.921446	140.821883	49.583476
825.458547	142.855366	49.588481
821.641278	141.024809	49.593485
818.454825	139.109653	49.598490
814.855859	130.883238	49.603495
811.788116	135.517386	49.608500
808.111896	139.077239	49.613505
804.581583	134.069874	49.618509
801.392852	142.495535	49.623514
797.251579	139.236003	49.628519
793.746456	145.994611	49.633524
790.528868	151.567822	49.638529
787.248718	145.439066	49.643533
783.750155	141.436827	49.648538
779.620260	147.892276	49.653543
776.721593	134.513439	49.658548
773.205847	140.653984	49.663553
769.485518	136.835457	49.668557
765.990872	135.781975	49.673562
762.277661	138.744924	49.678567
759.166609	127.737306	49.683572
755.572367	138.755580	49.688577
751.691977	140.824631	49.693581
748.557627	136.034203	49.698586
744.851315	145.632643	49.703591
741.863937	138.675426	49.708596
738.025003	143.545332	49.713601
734.442932	132.928030	49.718605
731.391583	132.825027	49.723610
727.062414	143.335393	49.728615
723.894648	131.436738	49.733620
720.344303	144.912507	49.738625
716.780523	133.766491	49.743629
713.597190	134.666292	49.748634
709.750502	145.003915	49.753639
706.405364	135.508568	49.758644
702.839445	137.662393	49.763649
699.366098	136.837706	49.768653
695.922706	135.012901	49.773658
692.346191	141.511067	49.778663
688.964700	133.700490	49.783668
685.604184	144.259825	49.788673
682.169306	127.378652	49.793677
678.586321	137.850469	49.798682
674.724266	133.496221	49.803687
671.486384	127.093974	49.808692
667.559300	136.651633	49.813697
664.055523	132.148928	49.818701
661.072776	136.954411	49.823706
657.669600	144.151702	49.828711
654.412667	129.400959	49.833716
650.520997	136.887850	49.838721
646.816946	137.384846	49.843725
643.460397	136.586268	49.848730
639.744488	142.447841	49.853735
636.881812	128.741114	49.858740
632.706301	141.084650	49.863745
628.917514	138.075796	49.868749
625.842359	141.234429	49.873754
622.067627	135.600069	49.878759
618.976746	135.027513	49.883764
615.533098	145.936909	49.888769
611.926674	136.267211	49.893773
608.226509	135.167543	49.898778
604.543571	140.155409	49.903783
601.329219	135.996584	49.908788
597.941736	134.652000	49.913793
594.291430	123.397678	49.918797
590.465966	125.279979	49.923802
587.207947	141.022217	49.928807
584.263016	124.031662	49.933812
580.667074	132.170417	49.938817
577.035098	134.737638	49.943821
573.304076	128.289582	49.948826
569.365649	132.572238	49.953831
566.217594	131.071637	49.958836
562.751172	137.509649	49.963841
559.057867	135.296704	49.968845
555.775975	119.970416	49.973850
552.451049	129.224682	49.978855
548.936478	124.233484	49.983860
545.333724	127.450457	49.988865
541.780144	126.482883	49.993869
538.396295	127.644107	49.998874
534.749809	128.369462	50.003879
531.798674	118.767644	50.008884
527.722062	122.438764	50.013889
523.996674	134.708298	50.018893
520.606981	134.190584	50.023898
517.007431	135.847309	50.028903
514.122369	124.836246	50.033908
510.385277	142.458489	50.038913
506.307509	129.413510	50.043917
503.325517	124.190565	50.048922
499.810701	137.428135	50.053927
496.113843	121.317089	50.058932
492.692646	132.664086	50.063937
488.727974	125.322361	50.068941
485.562425	124.183472	50.073946
482.268546	138.748478	50.078951
479.295094	125.060015	50.083956
475.200209	133.774751	50.088961
471.661227	128.891456	50.093965
468.488776	127.789044	50.098970
464.869930	136.931970	50.103975
461.163937	126.185064	50.108980
457.752622	135.458823	50.113985
454.198826	125.045495	50.118989
450.624316	122.736027	50.123994
446.893709	137.571647	50.128999
443.823894	129.193870	50.134004
440.217731	127.432321	50.139009
436.494771	117.562844	50.144013
433.335820	127.902693	50.149018
429.930629	135.136389	50.154023
426.111054	114.849587	50.159028
422.469827	139.063795	50.164033
419.527792	129.634601	50.169037
415.867869	137.536610	50.174042
411.744926	136.418869	50.179047
408.925411	131.910690	50.184052
405.342759	137.433471	50.189057
401.382975	132.772614	50.194061
398.020294	123.318335	50.199066
394.340510	129.492223	50.204071
391.326956	131.459172	50.209076
387.543515	129.791141	50.214081
383.824000	138.849555	50.219085
381.009333	129.770698	50.224090
377.551373	140.372803	50.229095
373.888737	134.358011	50.234100
369.901745	129.742735	50.239105
366.230122	129.424145	50.244109
362.971439	129.489508	50.249114
359.312698	138.698909	50.254119
356.395083	131.692948	50.259124
352.794126	131.059173	50.264129
349.281273	127.540379	50.269133
345.840095	128.569355	50.274138
342.200288	131.417093	50.279143
338.466981	120.266743	50.284148
334.808154	134.077044	50.289153
331.274012	132.953492	50.294157
328.143491	126.986639	50.299162
324.927061	128.962939	50.304167
321.300753	121.312396	50.309172
317.306775	130.092260	50.314177
314.093002	122.906445	50.319181
310.698777	126.857711	50.324186
306.857059	126.214095	50.329191
303.545479	128.897425	50.334196
300.118263	126.646191	50.339201
296.227471	128.208036	50.344205
293.214063	122.793310	50.349210
289.658925	127.409210	50.354215
286.076689	132.059989	50.359220
282.397379	137.139862	50.364225
278.505695	124.495314	50.369229
275.686241	124.967960	50.374234
271.902643	129.155782	50.379239
268.680660	120.657310	50.384244
265.036402	133.365895	50.389249
261.453945	128.727966	50.394253
257.904477	126.229811	50.399258
254.472127	124.338812	50.404263
251.324914	120.186124	50.409268
247.387969	128.546740	50.414273
244.051271	128.941041	50.419277
240.665921	131.145856	50.424282
236.745768	133.955036	50.429287
233.527114	126.375819	50.434292
229.957566	123.978693	50.439297
226.480564	127.073082	50.444301
223.161926	123.761220	50.449306
219.216333	126.525292	50.454311
215.998024	127.883731	50.459316
212.509813	129.832681	50.464321
208.952581	137.756921	50.469325
205.729704	116.253286	50.474330
201.858035	126.641602	50.479335
198.329196	122.436689	50.484340
194.757708	124.892776	50.489345
191.248479	122.391372	50.494349
188.095194	116.725392	50.499354
184.480456	126.011303	50.504359
181.177151	127.737068	50.509364
177.453752	127.694799	50.514369
174.118666	124.996451	50.519373
170.587692	120.097100	50.524378
166.648740	136.228969	50.529383
163.367170	122.819507	50.534388
159.651501	123.647601	50.539393
156.209008	122.362997	50.544397
153.017260	126.697236	50.549402
149.450207	119.871968	50.554407
145.921489	122.884602	50.559412
142.405276	126.409818	50.564417
138.451427	128.356390	50.569421
135.360675	119.774934	50.574426
131.648712	116.232066	50.579431
128.764492	127.358190	50.584436
125.102857	122.293436	50.589441
121.035491	120.795789	50.594445
117.854123	122.071619	50.599450
114.242220	126.756650	50.604455
111.021106	120.972705	50.609460
107.230180	125.634494	50.614465
103.635404	122.456854	50.619469
100.480437	125.635370	50.624474
96.797042	131.761153	50.629479
93.665066	122.197907	50.634484
90.036215	127.598339	50.639489
86.637073	123.512946	50.644493
83.158987	120.681863	50.649498
78.926765	128.774984	50.654503
76.009359	121.674683	50.659508
72.205487	115.642911	50.664513
68.964364	121.881374	50.669517
65.483530	124.721962	50.674522
61.475849	126.382106	50.679527
58.306276	120.107583	50.684532
54.460416	133.540173	50.689537
51.188186	127.325274	50.694541
48.046536	126.343978	50.699546
44.248680	128.769588	50.704551
40.901866	127.817927	50.709556
37.227786	127.058393	50.714561
33.861357	129.827572	50.719565
30.495800	121.466740	50.724570
26.393120	125.127438	50.729575
23.325590	131.115981	50.734580
19.822964	125.244930	50.739585
16.597339	122.299086	50.744589
12.909335	116.908861	50.749594
8.639487	126.177876	50.754599
5.480918	120.066545	50.759604
2.121301	130.087849	50.764609