Tue Jun 21 13:33:09 2022

Number of Points = 9930

Depth (nm)	Load (N)	Time (s)
-0.613412	90.647553	0.000000
-0.110624	73.827437	0.005005
-0.240063	84.647037	0.010010
-0.285959	81.057077	0.015014
-0.405793	73.488674	0.020019
-0.756282	76.011059	0.025024
-0.633572	59.834451	0.030029
-1.200558	50.358277	0.035034
-1.283239	41.465350	0.040038
-1.572955	27.969372	0.045043
-1.923128	19.152127	0.050048
-2.079816	11.820342	0.055053
-2.624642	15.113319	0.060058
-2.649679	-2.183687	0.065062
-2.615019	0.320298	0.070067
-3.014747	-4.035115	0.075072
-3.927516	-8.561909	0.080077
-4.404904	-5.815467	0.085082
-4.462705	-8.623179	0.090086
-4.312576	-11.383034	0.095091
-5.027683	-6.367168	0.100096
-5.460130	-12.908938	0.105101
-5.652359	-14.959324	0.110106
-5.751250	-12.390208	0.115110
-5.910673	-18.129246	0.120115
-6.048076	-0.349439	0.125120
-6.008718	-18.385841	0.130125
-6.559044	-17.285512	0.135130
-7.026665	-15.904062	0.140134
-7.007090	-17.389233	0.145139
-7.414426	-9.243126	0.150144
-7.480409	-20.422123	0.155149
-8.522735	-16.833454	0.160154
-8.736989	-7.556041	0.165158
-8.393750	-15.311192	0.170163
-8.816477	-8.765275	0.175168
-8.745256	-19.477606	0.180173
-8.857091	-11.992757	0.185178
-8.996857	-18.111955	0.190182
-9.586250	-12.127480	0.195187
-10.728922	-10.504797	0.200192
-10.357856	-19.844403	0.205197
-10.540035	-11.549496	0.210202
-10.652045	-10.188648	0.215206
-10.569574	-13.342227	0.220211
-10.839319	-17.448615	0.225216
-11.371660	-17.689575	0.230221
-12.201704	-8.483650	0.235226
-12.165840	-16.434569	0.240230
-12.213095	-15.084247	0.245235
-12.479123	-5.006165	0.250240
-12.413496	-16.830332	0.255245
-12.765843	-14.651011	0.260250
-13.313482	-15.030926	0.265254
-13.377858	-7.551171	0.270259
-13.812422	-3.183821	0.275264
-14.028936	-19.872097	0.280269
-14.023661	-12.153265	0.285274
-14.261099	-8.320771	0.290278
-14.865240	-20.866773	0.295283
-15.347577	-7.380257	0.300288
-15.299069	-14.358840	0.305293
-15.526458	-8.494889	0.310298
-15.997930	-12.425991	0.315302
-15.470381	-7.715945	0.320307
-15.767375	-12.063896	0.325312
-16.493627	-12.776339	0.330317
-17.057968	-15.951669	0.335322
-17.069974	-12.088031	0.340326
-16.833150	-17.125650	0.345331
-16.947569	-15.943977	0.350336
-17.749541	-12.162845	0.355341
-18.208528	-8.799232	0.360346
-18.457895	-10.850417	0.365350
-18.309861	-16.205642	0.370355
-18.720906	-9.429793	0.375360
-18.390751	-16.243275	0.380365
-19.131483	-6.502763	0.385370
-19.818037	-3.115278	0.390374
-19.828476	-10.251045	0.395379
-20.192947	-11.726493	0.400384
-20.054349	-12.693642	0.405389
-20.047524	-2.530699	0.410394
-20.530624	-10.872440	0.415398
-21.576165	-17.628612	0.420403
-21.649838	-12.353699	0.425408
-22.002310	-8.996476	0.430413
-21.930514	-13.557244	0.435418
-22.187726	-14.578235	0.440422
-21.707194	-18.862142	0.445427
-21.737281	-13.803423	0.450432
-21.919009	-19.274537	0.455437
-22.580241	-12.377932	0.460442
-23.170641	-10.228257	0.465446
-23.151045	-18.777753	0.470451
-24.324812	-6.327981	0.475456
-24.419349	-16.730283	0.480461
-24.387774	-17.548088	0.485466
-24.621765	-12.845730	0.490470
-24.417395	-8.347582	0.495475
-24.886769	-11.586787	0.500480
-24.888465	-15.353749	0.505485
-25.584722	-15.122578	0.510490
-26.128230	-11.474228	0.515494
-26.150560	-12.417095	0.520499
-26.610883	-4.118159	0.525504
-26.513449	-11.102081	0.530509
-26.612269	-4.787596	0.535514
-26.730656	-12.281998	0.540518
-26.808105	-11.828290	0.545523
-27.781514	-11.508797	0.550528
-28.232879	-2.717419	0.555533
-28.236016	-9.734021	0.560538
-28.097605	-9.470176	0.565542
-27.798753	-16.490015	0.570547
-28.355517	-8.083350	0.575552
-28.852212	-9.209922	0.580557
-29.293761	-11.773329	0.585562
-29.353587	-11.818043	0.590566
-29.680731	-12.943288	0.595571
-30.167618	-14.866339	0.600576
-30.767986	-26.649673	0.605581
-31.141114	-17.208614	0.610586
-30.672803	-12.919541	0.615590
-30.943978	-15.128926	0.620595
-31.344082	-14.339208	0.625600
-31.499962	-15.185171	0.630605
-31.529984	-7.665720	0.635610
-31.846746	-17.805077	0.640614
-31.845137	-20.509552	0.645619
-32.911060	-5.542303	0.650624
-32.876607	-10.403347	0.655629
-32.767411	-18.278593	0.660634
-32.694854	-9.940622	0.665638
-33.117376	-21.188050	0.670643
-34.068414	-8.061605	0.675648
-34.144994	-11.156088	0.680653
-34.635442	-15.011229	0.685658
-34.857848	-0.683108	0.690662
-34.381394	-14.499501	0.695667
-34.691892	-3.767395	0.700672
-35.208988	-15.172227	0.705677
-35.972774	-12.884516	0.710682
-36.381624	-12.883667	0.715686
-36.175667	-16.244568	0.720691
-36.357243	-4.348236	0.725696
-36.546485	-15.664490	0.730701
-36.594176	-6.293497	0.735706
-36.599375	-4.114236	0.740710
-36.875403	-15.890112	0.745715
-37.602972	-7.442139	0.750720
-37.914049	-11.799398	0.755725
-38.229747	-10.113162	0.760730
-38.475603	-3.060969	0.765734
-38.093112	-14.145709	0.770739
-38.829596	-8.476088	0.775744
-39.308766	-8.951204	0.780749
-39.636680	-9.200360	0.785754
-39.957308	-5.790590	0.790758
-39.781980	-12.272568	0.795763
-40.267126	-2.730664	0.800768
-39.841469	-6.698635	0.805773
-39.684580	-7.925741	0.810778
-40.675982	-8.029110	0.815782
-40.941599	-7.773148	0.820787
-41.232277	-6.925773	0.825792
-41.234224	-11.910041	0.830797
-41.499435	-14.504423	0.835802
-42.642684	-6.249079	0.840806
-42.408348	-13.640864	0.845811
-42.742186	-7.460720	0.850816
-42.930506	-7.382332	0.855821
-42.862311	-10.334635	0.860826
-42.847603	-9.882374	0.865830
-43.180533	-14.021315	0.870835
-43.999336	-7.235167	0.875840
-44.137376	-13.687551	0.880845
-44.643612	-16.261752	0.885850
-44.529111	-8.225148	0.890854
-44.156026	-15.301680	0.895859
-45.147110	-8.180743	0.900864
-45.315446	-8.023770	0.905869
-45.627127	-14.001032	0.910874
-45.444932	-8.532085	0.915878
-45.542642	-13.788008	0.920883
-46.140333	-14.528445	0.925888
-47.012239	-15.119280	0.930893
-46.971154	-22.046110	0.935898
-47.206212	-15.360382	0.940902
-47.031090	-20.264055	0.945907
-47.484796	-18.071500	0.950912
-47.427626	-6.878337	0.955917
-47.872910	-17.764428	0.960922
-48.628512	-13.095079	0.965926
-48.630834	-13.357303	0.970931
-48.965605	-12.773959	0.975936
-48.997566	-23.399735	0.980941
-48.725832	-11.431070	0.985946
-49.494340	-13.398256	0.990950
-50.127367	-18.723000	0.995955
-50.646558	-17.296302	1.000960
-50.693557	-13.442461	1.005965
-51.158128	-25.125142	1.010970
-51.215516	-17.989319	1.015974
-50.288834	-9.586974	1.020979
-50.886618	-14.313914	1.025984
-51.047959	-18.039835	1.030989
-51.904001	-15.792295	1.035994
-51.960571	-14.368799	1.040998
-51.910142	-20.438384	1.046003
-52.384559	-6.974099	1.051008
-52.711710	-21.438451	1.056013
-53.362497	-17.087787	1.061018
-54.200206	-7.778961	1.066022
-53.712574	-6.663835	1.071027
-53.842577	-10.904460	1.076032
-53.944697	-10.748783	1.081037
-53.840680	-14.311250	1.086042
-54.301276	-1.013232	1.091046
-54.766403	-7.046385	1.096051
-55.444786	-6.875593	1.101056
-55.276924	-1.748815	1.106061
-55.154272	-15.657773	1.111066
-55.622078	5.694601	1.116070
-55.754532	-18.151636	1.121075
-56.392287	-12.123629	1.126080
-56.618011	-18.284236	1.131085
-56.790518	-19.458766	1.136090
-57.374308	-22.032356	1.141094
-57.125128	-23.193838	1.146099
-57.514600	-10.625502	1.151104
-58.338628	-16.902714	1.156109
-58.051857	-14.324452	1.161114
-58.587501	-8.058004	1.166118
-58.232504	-20.680935	1.171123
-58.672586	-13.848380	1.176128
-58.504489	-15.473191	1.181133
-59.521429	-8.022568	1.186138
-60.048933	-19.831383	1.191142
-60.027376	-12.828215	1.196147
-60.466086	-11.262700	1.201152
-60.101348	-20.121738	1.206157
-60.263085	-18.759957	1.211162
-60.487311	-18.557221	1.216166
-61.136924	-14.022638	1.221171
-61.698046	-21.210269	1.226176
-61.750873	-7.882104	1.231181
-61.870486	-13.160249	1.236186
-62.119112	-15.277462	1.241190
-61.994508	-20.969796	1.246195
-61.966931	-10.308877	1.251200
-62.749378	-17.899317	1.256205
-63.206897	-6.351957	1.261210
-63.443217	-9.540951	1.266214
-63.407624	-19.332541	1.271219
-63.747801	-15.945188	1.276224
-64.155367	-12.356840	1.281229
-64.522792	-9.848433	1.286234
-65.029497	-4.272507	1.291238
-64.839200	-12.069820	1.296243
-65.025328	-2.815220	1.301248
-65.019217	-15.535087	1.306253
-65.035916	-13.820616	1.311258
-65.936874	-15.287529	1.316262
-66.401795	-16.472242	1.321267
-66.963733	-2.590308	1.326272
-66.848813	-14.060134	1.331277
-66.751356	-12.167629	1.336282
-66.990183	-11.230173	1.341286
-66.566957	-11.297457	1.346291
-67.513820	-8.685397	1.351296
-68.243162	-6.935788	1.356301
-68.361619	-5.652016	1.361306
-68.548425	-3.670008	1.366310
-68.367770	-14.753093	1.371315
-68.281673	-2.359016	1.376320
-68.901875	-21.577129	1.381325
-69.428782	-9.649664	1.386330
-70.041603	-13.532091	1.391334
-69.794285	-15.414319	1.396339
-70.322363	-10.972283	1.401344
-70.064962	-20.785014	1.406349
-70.164499	-16.861892	1.411354
-70.715536	-3.826152	1.416358
-71.050171	-13.604780	1.421363
-71.192645	-6.913661	1.426368
-71.337241	-9.786127	1.431373
-71.961407	-6.691154	1.436378
-72.737608	-0.994229	1.441382
-72.971081	-6.559978	1.446387
-72.919701	-13.121674	1.451392
-72.288614	-11.588282	1.456397
-72.959439	-15.095049	1.461402
-73.239034	-1.568895	1.466406
-73.047278	-17.340277	1.471411
-74.044196	-8.790469	1.476416
-74.463780	-3.245743	1.481421
-74.368667	-10.905736	1.486426
-75.077929	-5.674356	1.491430
-74.525362	-14.874709	1.496435
-74.399821	-17.527681	1.501440
-75.043810	-16.961798	1.506445
-75.608942	-20.239007	1.511450
-76.381204	-11.859802	1.516454
-76.414157	-17.777643	1.521459
-76.523662	-13.759729	1.526464
-76.316595	-13.124429	1.531469
-76.451643	-7.458698	1.536474
-77.109790	-2.998670	1.541478
-77.322811	-18.140815	1.546483
-77.918066	-2.277668	1.551488
-77.921598	-8.052977	1.556493
-78.150807	-6.651803	1.561498
-78.418680	-0.012927	1.566502
-78.380470	-6.426616	1.571507
-79.186898	-9.508171	1.576512
-79.951985	-14.851690	1.581517
-79.746193	-17.083228	1.586522
-79.292687	-8.136233	1.591526
-79.547894	-17.172029	1.596531
-79.552885	-14.986490	1.601536
-80.096172	-16.201834	1.606541
-80.733927	-15.146809	1.611546
-81.312212	-8.048644	1.616550
-81.386240	-8.907766	1.621555
-81.240715	-3.515825	1.626560
-81.189845	-10.265496	1.631565
-81.307004	-16.685220	1.636570
-82.617026	-10.232316	1.641574
-82.825000	-18.956647	1.646579
-83.109240	-9.228781	1.651584
-83.084723	-14.381412	1.656589
-82.930541	-11.248593	1.661594
-83.249793	-1.814475	1.666598
-82.905437	-10.848334	1.671603
-83.722209	-11.960371	1.676608
-84.274542	-9.351287	1.681613
-84.153670	-18.995579	1.686618
-84.524645	-11.362837	1.691622
-84.583010	-27.326033	1.696627
-85.631986	-9.747919	1.701632
-86.198605	-16.467155	1.706637
-85.839807	-16.727419	1.711642
-86.213427	-5.082854	1.716646
-86.000718	-19.403359	1.721651
-85.765378	-15.628639	1.726656
-86.074351	-12.497656	1.731661
-86.702981	-20.762787	1.736666
-87.504582	-11.933342	1.741670
-87.399449	-8.913365	1.746675
-87.543438	-15.238860	1.751680
-87.889774	-6.278002	1.756685
-87.693637	-14.657820	1.761690
-88.497256	-5.638005	1.766694
-88.625572	-9.198701	1.771699
-88.910881	-11.570909	1.776704
-89.212175	-13.039842	1.781709
-89.411848	-9.095202	1.786714
-89.440998	-4.800514	1.791718
-89.862336	-14.109335	1.796723
-90.358374	-18.831014	1.801728
-90.812655	-14.634249	1.806733
-90.695845	-9.188025	1.811738
-90.910473	-8.452895	1.816742
-90.775834	-10.536886	1.821747
-91.055984	-14.970891	1.826752
-91.807662	-13.398929	1.831757
-92.403826	-17.482627	1.836762
-92.762965	-12.104398	1.841766
-92.521488	-21.158115	1.846771
-92.837701	-19.494287	1.851776
-93.008164	-15.406092	1.856781
-92.767812	-14.448930	1.861786
-92.910867	-11.643793	1.866790
-93.425801	-16.467522	1.871795
-94.325842	-13.026125	1.876800
-94.420177	-23.030821	1.881805
-94.492685	-20.433714	1.886810
-94.674051	-8.765936	1.891814
-94.524746	-25.727889	1.896819
-94.497369	-18.288401	1.901824
-95.375937	-15.432692	1.906829
-95.611934	-18.403287	1.911834
-96.075144	-15.348783	1.916838
-96.133311	-9.248432	1.921843
-96.395677	-16.021013	1.926848
-96.790934	-8.606248	1.931853
-96.725316	-18.863974	1.936858
-97.392936	-13.665341	1.941862
-97.599490	-8.861953	1.946867
-97.601620	-18.038323	1.951872
-97.595196	-21.969227	1.956877
-97.550574	-24.049754	1.961882
-98.458163	-17.761767	1.966886
-98.769287	-18.683446	1.971891
-99.018271	-13.467119	1.976896
-99.248968	-8.172518	1.981901
-99.073515	-14.295567	1.986906
-99.941758	-14.272700	1.991910
-100.218845	-19.173310	1.996915
-100.579740	-6.306268	2.006912
-99.629461	-8.864821	2.016909
-99.226400	-11.209059	2.026906
-99.122743	-6.342818	2.036902
-98.311551	-7.619123	2.046899
-97.942002	-14.187524	2.056896
-97.591180	-10.609377	2.066893
-96.910968	-14.253984	2.076890
-96.460251	-14.599831	2.086886
-95.761829	-8.092350	2.096883
-95.309608	-12.951101	2.106880
-94.772466	-12.159140	2.116877
-94.405279	-14.177150	2.126874
-94.023203	-15.728361	2.136870
-93.411606	-10.690368	2.146867
-92.974943	-15.952579	2.156864
-91.817207	-10.728610	2.166861
-91.535041	-10.561866	2.176858
-91.557116	-16.347383	2.186854
-91.668305	-10.557811	2.196851
-90.484294	-9.950628	2.206848
-89.476737	-7.102252	2.216845
-88.965531	-14.637780	2.226842
-88.808365	-9.283869	2.236838
-88.695993	-16.653368	2.246835
-88.197491	-13.251225	2.256832
-87.370372	-15.233175	2.266829
-86.686277	-10.627649	2.276826
-86.015098	-4.996489	2.286822
-85.800380	-6.882948	2.296819
-85.795935	-8.077217	2.306816
-84.740218	-11.313164	2.316813
-83.960612	-9.722209	2.326810
-84.127404	-12.441537	2.336806
-83.469445	-5.634925	2.346803
-82.984177	-2.627142	2.356800
-82.440809	-8.649553	2.366797
-81.378096	-6.782035	2.376794
-81.122884	-8.928307	2.386790
-81.047362	-7.151991	2.396787
-80.572044	-1.211772	2.406784
-79.950028	-9.968753	2.416781
-79.566836	-13.479998	2.426778
-78.408128	-9.588701	2.436774
-78.191215	-6.791362	2.446771
-77.950614	-5.341528	2.456768
-77.500733	-0.826628	2.466765
-76.881535	-10.092715	2.476762
-76.456292	-4.385456	2.486758
-75.245880	-0.119995	2.496755
-75.170331	-4.458365	2.506752
-74.794326	-4.420969	2.516749
-74.781964	-8.652848	2.526746
-73.444591	-6.747826	2.536742
-73.116273	-9.934440	2.546739
-73.311575	-9.134001	2.556736
-72.543324	-15.206494	2.566733
-71.823485	-12.211674	2.576730
-71.024384	-12.241380	2.586726
-70.529310	-12.841750	2.596723
-70.313884	-11.294289	2.606720
-70.281020	-16.204315	2.616717
-69.658576	-11.159025	2.626714
-68.715836	-8.110622	2.636710
-67.757677	-12.741367	2.646707
-67.738982	-4.499926	2.656704
-67.049541	-8.192294	2.666701
-66.993680	-7.004490	2.676698
-66.463494	-10.888816	2.686694
-65.694331	-13.819257	2.696691
-65.725839	-10.434454	2.706688
-64.658623	-12.352231	2.716685
-63.789946	-16.032786	2.726682
-63.642549	-9.595672	2.736678
-63.732593	-12.840643	2.746675
-62.794713	-14.212412	2.756672
-62.221147	-15.033243	2.766669
-61.849932	-15.372046	2.776666
-60.770213	-12.206238	2.786662
-60.489725	-9.738527	2.796659
-60.500515	-8.639862	2.806656
-60.345629	-12.586318	2.816653
-59.475485	-14.297385	2.826650
-58.807149	-5.153665	2.836646
-57.897641	-5.719525	2.846643
-57.788930	-15.190335	2.856640
-57.687307	-5.284335	2.866637
-56.805540	-8.911339	2.876634
-56.289857	-4.849333	2.886630
-55.723808	-8.642583	2.896627
-54.647742	-11.078312	2.906624
-54.452899	-8.381049	2.916621
-54.266100	-10.770679	2.926618
-54.246473	-3.298393	2.936614
-53.175684	-11.479434	2.946611
-53.144915	-7.772802	2.956608
-52.034063	-8.509720	2.966605
-51.412777	-10.243395	2.976602
-51.300669	-11.740610	2.986598
-51.165009	-10.214910	2.996595
-50.020044	-2.478484	3.006592
-49.848586	-0.809930	3.016589
-49.613985	-10.041174	3.026586
-48.453521	-9.458531	3.036582
-48.133936	-15.975780	3.046579
-47.930816	-14.292317	3.056576
-47.090447	-7.901394	3.066573
-46.867529	-13.501250	3.076570
-46.290867	-15.412277	3.086566
-45.479416	-6.140508	3.096563
-45.282746	-6.836290	3.106560
-45.116062	-10.084062	3.116557
-44.429820	-9.109912	3.126554
-43.789243	-6.442597	3.136550
-42.657802	-6.929815	3.146547
-42.555392	-5.240145	3.156544
-42.002267	-11.776311	3.166541
-41.933376	-13.042504	3.176538
-41.483941	-4.826945	3.186534
-40.599515	-11.716130	3.196531
-40.729568	-7.144708	3.206528
-39.171887	-10.084009	3.216525
-38.745435	-7.663189	3.226522
-38.855592	-8.606515	3.236518
-38.743734	-6.512174	3.246515
-37.944192	-11.771051	3.256512
-37.369523	-9.017936	3.266509
-36.259248	-6.165019	3.276506
-35.813911	-8.352652	3.286502
-35.716079	-6.117085	3.296499
-35.648171	-7.170514	3.306496
-34.612208	-15.833621	3.316493
-33.930005	-16.034238	3.326490
-33.720912	-10.258777	3.336486
-33.723204	-15.959253	3.346483
-32.906633	-4.755743	3.356480
-32.106948	-7.312067	3.366477
-31.363237	-8.872576	3.376474
-31.064227	-8.481591	3.386470
-30.907264	-3.376794	3.396467
-30.433946	-7.947796	3.406464
-29.814329	-13.432948	3.416461
-29.180002	-11.127956	3.426458
-28.109186	-13.672074	3.436454
-27.856344	-8.906406	3.446451
-27.727678	-14.031465	3.456448
-27.827563	-10.394680	3.466445
-26.910122	-20.487645	3.476442
-26.221594	-9.109013	3.486438
-25.204331	-5.349579	3.496435
-25.004816	-6.160431	3.506432
-24.730345	-8.564183	3.516429
-24.724116	-7.659005	3.526426
-23.288337	-11.880796	3.536422
-22.664270	-13.511196	3.546419
-22.761032	-12.050543	3.556416
-22.753659	-7.760319	3.566413
-21.910370	-10.721206	3.576410
-21.156019	-15.858788	3.586406
-20.194362	-7.146947	3.596403
-20.040024	-11.167210	3.606400
-19.721716	-14.069418	3.616397
-19.674865	-14.562760	3.626394
-18.907740	-15.363081	3.636390
-17.853067	-12.546791	3.646387
-17.624134	-15.366032	3.656384
-17.312689	-4.983024	3.666381
-16.749583	-13.718784	3.676378
-15.766398	-10.711446	3.686374
-15.880872	-14.415910	3.696371
-15.601579	-12.905102	3.706368
-14.154523	-9.458680	3.716365
-13.929028	-13.458519	3.726362
-13.769830	-2.118089	3.736358
-13.395639	-10.644543	3.746355
-12.326318	-7.572432	3.756352
-12.043219	0.339328	3.766349
-11.996300	-6.972909	3.776346
-11.004677	-6.150683	3.786342
-10.376256	-9.828592	3.796339
-10.263473	-10.066704	3.806336
-9.658591	-11.033989	3.816333
-8.565943	-9.673473	3.826330
-8.796827	-10.108773	3.836326
-8.648172	-9.022480	3.846323
-7.699582	-3.122287	3.856320
-7.124225	-10.214187	3.866317
-6.585145	-11.614156	3.876314
-5.602077	-12.499826	3.886310
-5.586272	-13.623462	3.896307
-5.600660	-8.358897	3.906304
-4.895035	-4.193778	3.916301
-4.266569	-5.665452	3.926298
-3.832973	-0.496009	3.936294
-3.243280	9.426994	3.946291
-2.953726	15.581155	3.956288
-2.246189	30.945345	3.966285
-1.815020	34.041535	3.976282
-1.532288	50.535546	3.986278
-0.970622	61.018639	3.996275
-0.728531	78.295727	4.006272
-0.397935	102.908616	4.016269
0.000000	113.838514	4.021274
-0.132587	132.304204	4.026278
0.291704	141.104586	4.031283
0.651387	155.438687	4.036288
0.699856	160.989634	4.041293
0.811404	155.332943	4.046298
0.634547	164.175654	4.051302
0.741416	166.887145	4.056307
0.754492	173.333150	4.061312
0.749449	188.376909	4.066317
0.818190	191.655546	4.071322
1.032888	206.117106	4.076326
0.999730	192.813725	4.081331
1.147385	208.509672	4.086336
0.935956	204.539200	4.091341
0.988114	195.872302	4.096346
0.963232	199.431268	4.101350
0.966934	204.739817	4.106355
1.400400	222.013116	4.111360
1.031071	231.664056	4.116365
1.431487	226.469818	4.121370
1.358201	234.658418	4.126374
1.627945	223.881274	4.131379
1.504712	211.555200	4.136384
1.278278	209.227665	4.141389
1.370459	199.360651	4.146394
0.794715	216.887095	4.151398
1.525576	219.782987	4.156403
1.668725	232.079803	4.161408
1.191921	228.164911	4.166413
1.631036	224.095987	4.171418
1.256030	230.844265	4.176422
1.032533	227.581854	4.181427
1.295336	231.795510	4.186432
1.271461	229.993287	4.191437
1.612859	229.851744	4.196442
1.314195	233.101637	4.201446
1.447927	227.388558	4.206451
1.657657	239.792559	4.211456
1.103847	244.217413	4.216461
1.403030	233.576286	4.221466
1.626147	235.284228	4.226470
1.595572	240.436254	4.231475
1.229531	232.641743	4.236480
1.123681	239.038203	4.241485
0.860865	240.063905	4.246490
1.276679	263.629675	4.251494
1.504545	257.821471	4.256499
1.903212	270.617893	4.261504
1.618346	270.855928	4.266509
1.662602	266.811134	4.271514
1.980660	271.035976	4.276518
1.649826	272.853015	4.281523
2.009699	274.761109	4.286528
1.921121	273.841626	4.291533
1.897071	263.037129	4.296538
1.719645	251.328583	4.301542
1.663037	261.410838	4.306547
1.742099	256.401622	4.311552
1.859148	268.936041	4.316557
1.995910	255.437720	4.321562
1.963134	245.071584	4.326566
1.634725	234.905172	4.331571
1.695988	238.966706	4.336576
1.781642	250.494171	4.341581
2.072895	256.983739	4.346586
1.806263	257.718214	4.351590
1.805594	254.310168	4.356595
2.094088	245.484719	4.361600
1.624638	252.797042	4.366605
1.613002	259.615208	4.371610
1.896250	271.200744	4.376614
2.075566	274.081413	4.381619
2.211058	273.692958	4.386624
1.914915	278.233420	4.391629
2.192114	272.461244	4.396634
2.063881	272.184145	4.401638
2.271000	266.493433	4.406643
2.097688	246.952515	4.411648
2.009762	253.035603	4.416653
2.005985	241.873150	4.421658
1.593473	246.963903	4.426662
1.776392	260.682674	4.431667
2.176473	271.018472	4.436672
2.057853	277.906654	4.441677
2.240954	273.773746	4.446682
2.260729	273.584621	4.451686
2.181234	276.479335	4.456691
2.159347	269.429005	4.461696
1.866425	279.316361	4.466701
1.965520	275.591247	4.471706
2.063544	276.685667	4.476710
1.822906	275.745383	4.481715
2.204182	270.151140	4.486720
1.990611	279.971485	4.491725
2.101983	278.737292	4.496730
2.096121	271.694173	4.501734
1.899206	272.256472	4.506739
2.343035	275.109128	4.511744
2.116033	281.630058	4.516749
2.184534	275.364958	4.521754
2.111107	281.211023	4.526758
2.172048	280.007874	4.531763
2.726599	287.994267	4.536768
2.300923	286.823546	4.541773
2.450064	279.496246	4.546778
2.099390	273.661880	4.551782
1.944892	284.417885	4.556787
2.403296	291.714130	4.561792
2.457474	305.232649	4.566797
2.752273	297.722563	4.571802
2.887182	300.135994	4.576806
2.661664	283.953667	4.581811
2.861779	275.455023	4.586816
2.752778	266.489362	4.591821
2.667080	268.556289	4.596826
2.382226	272.609826	4.601830
1.991311	263.832734	4.606835
2.487070	264.703029	4.611840
1.817683	264.956784	4.616845
2.127899	290.011816	4.621850
2.221906	296.553599	4.626854
2.269588	304.574992	4.631859
2.443289	304.139164	4.636864
2.270220	302.445307	4.641869
2.186069	301.210336	4.646874
2.168236	311.345010	4.651878
2.096162	308.109606	4.656883
2.917820	316.934276	4.661888
2.656006	333.055727	4.666893
2.703138	333.922760	4.671898
2.821147	336.375503	4.676902
2.461309	338.033562	4.681907
2.757486	334.186603	4.686912
2.896335	343.732942	4.691917
2.930710	330.691967	4.696922
2.561735	316.473186	4.701926
2.586124	328.788166	4.706931
2.830346	341.024326	4.711936
2.936156	348.538036	4.716941
2.894498	340.763363	4.721946
2.810245	334.568526	4.726950
2.580812	335.503654	4.731955
2.779982	338.662451	4.736960
2.620726	338.411209	4.741965
2.902354	337.754645	4.746970
2.807176	343.638474	4.751974
2.479630	346.861994	4.756979
2.623384	346.739167	4.761984
2.401310	347.390490	4.766989
2.390110	342.681937	4.771994
2.433576	335.361453	4.776998
2.555693	360.990031	4.782003
2.896867	358.636566	4.787008
2.676081	373.953035	4.792013
3.145370	380.738782	4.797018
2.850017	377.688339	4.802022
3.268223	374.307602	4.807027
3.260347	370.634712	4.812032
3.476509	377.771207	4.817037
3.474237	372.318189	4.822042
3.275427	347.306227	4.827046
2.910722	350.264363	4.832051
3.135396	344.823111	4.837056
3.170120	344.674727	4.842061
3.216115	339.593998	4.847066
3.227803	344.628157	4.852070
2.969163	338.682423	4.857075
3.062600	338.738626	4.862080
3.111188	341.552547	4.867085
2.993346	341.509348	4.872090
2.919359	355.552344	4.877094
3.244745	364.975848	4.882099
3.604178	360.205129	4.887104
3.202943	354.276094	4.892109
3.031828	349.940150	4.897114
3.103867	350.779182	4.902118
3.303074	359.316218	4.907123
3.284118	365.719062	4.912128
3.366621	369.239565	4.917133
3.134152	357.196487	4.922138
3.295995	373.768603	4.927142
3.168035	374.993396	4.932147
3.322750	362.418511	4.937152
3.174156	372.856873	4.942157
3.457974	372.717958	4.947162
3.223256	370.474652	4.952166
3.181534	379.733593	4.957171
3.406919	372.895258	4.962176
3.112098	382.140461	4.967181
3.367923	364.014883	4.972186
3.389855	375.258959	4.977190
3.416593	366.119209	4.982195
3.427974	371.618356	4.987200
3.003439	373.827837	4.992205
3.187109	373.628543	4.997210
3.199856	373.542407	5.002214
3.036386	382.230878	5.007219
3.373414	387.758397	5.012224
3.426844	401.771851	5.017229
3.587617	400.152158	5.022234
3.377584	404.289246	5.027238
3.230747	410.147120	5.032243
3.354131	401.899892	5.037248
3.070224	401.001694	5.042253
3.320496	406.629428	5.047258
3.322696	407.184414	5.052262
3.279698	420.294453	5.057267
3.646815	419.221357	5.062272
3.954578	433.616214	5.067277
3.842225	423.017646	5.072282
3.572803	419.346217	5.077286
3.324622	429.191923	5.082291
3.475942	425.916149	5.087296
3.574722	431.618706	5.092301
3.793307	428.052756	5.097306
4.187045	430.748761	5.102310
3.907244	437.048401	5.107315
4.124103	429.388550	5.112320
3.789941	426.014376	5.117325
3.896259	422.853011	5.122330
3.570402	412.967859	5.127334
3.808515	417.844962	5.132339
4.278296	420.694138	5.137344
3.747590	415.346565	5.142349
3.633617	408.161047	5.147354
4.004356	413.425862	5.152358
4.014494	425.282295	5.157363
3.881919	414.005080	5.162368
4.010621	414.319482	5.167373
3.746128	400.622452	5.172378
3.988941	408.285190	5.177382
3.605421	408.109759	5.182387
4.020413	420.147994	5.187392
4.176064	423.414065	5.192397
3.877244	431.366209	5.197402
4.090664	427.317634	5.202406
3.998706	437.270285	5.207411
4.254244	418.942024	5.212416
3.896229	416.555731	5.217421
3.717123	428.161309	5.222426
4.149545	431.368725	5.227430
4.000181	427.950531	5.232435
4.258700	434.188659	5.237440
4.269412	433.031114	5.242445
4.053361	429.666587	5.247450
4.019941	434.976033	5.252454
3.854164	439.489429	5.257459
4.233154	430.655205	5.262464
4.178716	439.365516	5.267469
4.425457	429.574194	5.272474
4.421500	430.189600	5.277478
4.021472	430.418093	5.282483
4.427099	429.482282	5.287488
4.030892	437.981790	5.292493
4.077680	428.503405	5.297498
4.381646	435.232091	5.302502
4.186995	433.638293	5.307507
4.118251	431.108784	5.312512
3.745818	434.588006	5.317517
3.994272	433.064892	5.322522
4.363118	437.363464	5.327526
3.966387	443.143734	5.332531
4.180226	435.264940	5.337536
4.019872	441.467052	5.342541
3.885728	436.721995	5.347546
3.848838	446.968252	5.352550
3.932329	468.805223	5.357555
4.356152	467.145321	5.362560
4.294781	471.340495	5.367565
4.462903	468.814186	5.372570
4.264788	470.551450	5.377574
4.184327	472.031636	5.382579
4.324312	459.725716	5.387584
4.570999	472.386049	5.392589
4.285968	469.672117	5.397594
4.499183	468.491101	5.402598
4.088313	476.518261	5.407603
4.531426	465.124764	5.412608
4.175721	475.536512	5.417613
4.535738	484.904625	5.422618
4.457714	489.084209	5.427622
4.870900	499.067515	5.432627
4.710445	488.804450	5.437632
4.451198	487.930186	5.442637
4.712989	493.685894	5.447642
4.887905	483.422752	5.452646
4.754117	477.176464	5.457651
4.686738	468.104533	5.462656
4.675506	479.741948	5.467661
4.518034	465.599110	5.472666
4.183604	469.341415	5.477670
4.173693	483.452655	5.482675
4.491021	485.913859	5.487680
4.719525	498.321866	5.492685
4.979065	503.333586	5.497690
5.193960	495.454586	5.502694
4.864653	496.544793	5.507699
4.925388	492.142395	5.512704
4.906184	498.600590	5.517709
5.024332	502.763481	5.522714
4.866555	488.761968	5.527718
4.291362	479.868841	5.532723
4.503413	486.844446	5.537728
4.697399	495.304670	5.542733
4.758974	494.102387	5.547738
5.225154	488.348765	5.552742
5.122857	498.946298	5.557747
4.943337	490.723722	5.562752
4.740202	494.314246	5.567757
4.642970	498.195083	5.572762
5.085216	492.272357	5.577766
4.697529	497.448673	5.582771
5.216363	497.565469	5.587776
4.941165	502.642251	5.592781
4.895822	501.407152	5.597786
5.456797	489.767970	5.602790
5.410363	501.371368	5.607795
5.164749	495.498208	5.612800
5.131055	491.954480	5.617805
5.164927	484.469750	5.622810
5.195477	466.037984	5.627814
5.036051	473.072134	5.632819
4.922745	460.080172	5.637824
5.016774	473.941924	5.642829
4.785324	489.754016	5.647834
4.681117	494.615995	5.652838
4.417270	502.947195	5.657843
4.988553	500.614217	5.662848
4.941229	498.547069	5.667853
5.156580	500.523327	5.672858
5.356085	501.581422	5.677862
4.933544	509.710385	5.682867
5.063004	498.012406	5.687872
5.224640	499.880733	5.692877
5.094230	496.826042	5.697882
5.436043	504.697008	5.702886
4.878354	507.310211	5.707891
5.257282	510.078146	5.712896
5.182429	519.360417	5.717901
5.407614	531.684540	5.722906
5.492116	531.537186	5.727910
5.083516	537.718478	5.732915
5.086446	543.878595	5.737920
5.424881	529.703708	5.742925
5.508702	537.619383	5.747930
5.555642	533.344964	5.752934
5.560740	534.940443	5.757939
5.433660	526.520903	5.762944
5.331368	522.727644	5.767949
5.365748	524.061535	5.772954
5.599730	527.850041	5.777958
5.379146	537.743146	5.782963
5.630834	530.684693	5.787968
5.475344	529.195700	5.792973
5.282778	518.050496	5.797978
5.381217	533.218749	5.802982
5.434635	539.901744	5.807987
5.473733	534.405509	5.812992
5.526205	541.243771	5.817997
5.911948	529.534510	5.823002
5.761702	534.161792	5.828006
5.397528	528.638598	5.833011
5.857537	518.176867	5.838016
5.972830	514.840536	5.843021
5.356069	507.562594	5.848026
5.216734	513.237910	5.853030
5.377816	538.316460	5.858035
5.673677	529.205265	5.863040
5.630913	540.360911	5.868045
5.484487	541.119501	5.873050
5.602410	547.220913	5.878054
5.496133	539.558865	5.883059
5.682153	534.524744	5.888064
5.753276	542.504490	5.893069
5.453347	538.711589	5.898074
5.642486	543.012320	5.903078
5.471642	544.654498	5.908083
5.765177	539.705781	5.913088
5.537458	538.037327	5.918093
5.900848	543.577904	5.923098
5.851822	538.336817	5.928102
5.465224	534.190427	5.933107
5.470008	534.984166	5.938112
5.550632	551.260097	5.943117
5.687664	562.923937	5.948122
5.959534	568.431724	5.953126
5.920887	567.597099	5.958131
5.826391	571.167283	5.963136
5.746863	570.274699	5.968141
5.983131	567.406151	5.973146
6.076492	563.104499	5.978150
5.710000	571.957135	5.983155
5.853429	562.104493	5.988160
5.909042	560.029764	5.993165
6.173305	570.351152	5.998170
6.074770	571.092340	6.003174
5.765921	570.906122	6.008179
6.095548	569.438031	6.013184
6.132060	575.529649	6.018189
5.693754	573.027566	6.023194
5.606742	573.887618	6.028198
5.692512	575.015466	6.033203
5.769055	569.670891	6.038208
6.070227	572.967363	6.043213
5.677149	566.813506	6.048218
5.861060	581.273213	6.053222
6.134944	597.471605	6.058227
6.071896	603.248582	6.063232
6.297096	599.891073	6.068237
6.341679	594.713995	6.073242
6.598974	579.801616	6.078246
6.183071	581.702832	6.083251
6.080179	571.788551	6.088256
6.037236	573.948293	6.093261
5.853671	576.008574	6.098266
5.975731	573.284443	6.103270
5.967352	567.497482	6.108275
6.063095	572.371962	6.113280
6.005079	573.399294	6.118285
5.964587	570.247803	6.123290
5.982938	569.662059	6.128294
5.814704	571.502332	6.133299
5.835238	571.763408	6.138304
5.929663	580.550582	6.143309
6.062568	591.757495	6.148314
6.434800	589.974496	6.153318
5.835370	579.764720	6.158323
5.936513	577.734745	6.163328
5.927707	576.429849	6.168333
6.385942	588.791206	6.173338
6.314245	581.146697	6.178342
5.863869	574.880763	6.183347
6.086579	574.656847	6.188352
5.922681	574.083323	6.193357
6.040316	571.034314	6.198362
6.453920	566.329355	6.203366
6.352460	569.903256	6.208371
6.247256	559.656650	6.213376
6.232174	566.582480	6.218381
6.082229	568.836309	6.223386
5.923353	570.559588	6.228390
6.015061	568.763840	6.233395
5.829963	565.795549	6.238400
6.088570	567.109878	6.243405
5.862593	568.554769	6.248410
6.126941	574.594254	6.253414
6.071128	569.089055	6.258419
6.271512	577.764944	6.263424
5.903489	563.369948	6.268429
6.162458	567.971710	6.273434
6.126751	568.115802	6.278438
6.168382	574.442394	6.283443
6.228688	570.369603	6.288448
6.384285	567.646630	6.293453
6.114716	566.109822	6.298458
6.224386	564.262357	6.303462
5.928965	565.462402	6.308467
6.131376	570.428151	6.313472
6.662033	573.729842	6.318477
6.591694	562.749077	6.323482
6.224495	555.094705	6.328486
6.109725	549.114410	6.333491
6.075941	534.202320	6.338496
6.506870	532.328896	6.343501
6.205794	535.065377	6.348506
6.490927	533.900470	6.353510
6.179623	535.834880	6.358515
6.159779	539.747709	6.363520
6.442579	533.170152	6.368525
5.981476	533.568209	6.373530
6.153068	539.528316	6.378534
5.943136	535.837339	6.383539
6.145222	528.193305	6.388544
6.068235	530.481423	6.393549
6.206465	531.701619	6.398554
6.214756	514.398714	6.403558
5.934493	513.086084	6.408563
5.733343	503.440120	6.413568
6.130558	519.090717	6.418573
6.202583	534.652895	6.423578
6.025405	510.736270	6.428582
5.835093	515.349657	6.433587
6.147052	514.445139	6.438592
6.309432	525.095559	6.443597
5.604957	519.048145	6.448602
5.958139	522.476895	6.453606
5.922886	538.232670	6.458611
5.881319	538.946860	6.463616
5.953642	538.398160	6.468621
6.139855	540.741367	6.473626
6.323609	542.018162	6.478630
6.201316	539.446193	6.483635
6.186357	538.835378	6.488640
6.212259	528.405659	6.493645
6.138804	525.662209	6.498650
6.168587	502.001022	6.503654
6.055667	508.238721	6.508659
6.039641	499.336269	6.513664
6.057592	505.428565	6.518669
5.841063	506.938390	6.523674
6.317011	502.370539	6.528678
6.167947	508.083379	6.533683
5.931887	502.114307	6.538688
6.154414	501.848191	6.543693
6.012202	506.128395	6.548698
5.978324	493.913597	6.553702
5.840572	512.528994	6.558707
5.876865	505.209617	6.563712
5.788862	510.767304	6.568717
5.965396	530.011896	6.573722
6.264699	522.078649	6.578726
5.948851	542.722821	6.583731
6.043384	535.367343	6.588736
6.450647	533.240112	6.593741
5.871183	518.983970	6.598746
6.113082	514.613927	6.603750
5.784233	515.009423	6.608755
6.131181	529.163639	6.613760
6.226967	542.600486	6.618765
5.854710	531.744924	6.623770
6.194976	527.260708	6.628774
5.905320	530.590869	6.633779
6.136058	528.430904	6.638784
6.401141	528.562880	6.643789
5.957122	516.819538	6.648794
6.269482	507.957034	6.653798
5.956441	506.131815	6.658803
6.036721	508.867898	6.663808
6.012655	501.921031	6.668813
5.860704	503.379115	6.673818
6.100019	504.842072	6.678822
5.426572	513.142236	6.683827
5.900906	528.914659	6.688832
6.220493	532.431462	6.693837
6.008279	536.673339	6.698842
6.290198	534.624486	6.703846
5.966094	541.252379	6.708851
5.859258	538.911502	6.713856
6.180446	539.684227	6.718861
6.335279	534.604554	6.723866
6.310333	528.671951	6.728870
6.027465	511.489290	6.733875
5.915593	507.830826	6.738880
6.138823	499.469132	6.743885
5.750003	513.070067	6.748890
5.830576	514.403018	6.753894
5.712198	527.950699	6.758899
5.861642	544.778830	6.763904
5.890224	537.319420	6.768909
5.922109	537.318127	6.773914
6.301402	532.826264	6.778918
6.455313	536.493839	6.783923
6.179372	540.136292	6.788928
6.283113	541.520466	6.793933
6.076843	544.424974	6.798938
6.164737	536.263868	6.803942
6.065063	540.008956	6.808947
6.310357	527.618844	6.813952
5.951966	514.928499	6.818957
6.082907	511.853223	6.823962
6.244891	497.855587	6.828966
6.070581	508.903341	6.833971
5.842908	510.361927	6.838976
6.085790	500.346430	6.843981
5.899932	503.325105	6.848986
6.029852	499.558522	6.853990
6.121994	506.052749	6.858995
5.937599	504.257537	6.864000
6.162968	496.169990	6.869005
5.800943	505.924875	6.874010
5.883551	508.647943	6.879014
6.112029	539.952850	6.884019
5.922055	542.135749	6.889024
5.948824	539.979364	6.894029
5.849523	545.397243	6.899034
6.084639	535.325583	6.904038
6.123206	530.633006	6.909043
6.199690	534.966400	6.914048
6.365774	540.003868	6.919053
6.098826	535.773727	6.924058
6.485377	521.563449	6.929062
6.111239	505.566922	6.934067
5.923988	512.252854	6.939072
6.147337	494.762015	6.944077
5.868783	497.889834	6.949082
5.687177	496.022921	6.954086
5.770582	515.436052	6.959091
6.001040	529.359330	6.964096
5.993997	524.103600	6.969101
6.161528	531.744331	6.974106
6.064252	535.371011	6.979110
5.947238	536.306283	6.984115
5.969778	529.692294	6.989120
5.933500	537.732842	6.994125
5.733199	541.501697	6.999130
6.048490	532.352944	7.004134
6.093891	537.760082	7.009139
5.976017	539.360729	7.014144
5.978169	531.358474	7.019149
5.779749	537.070618	7.024154
6.026910	523.129503	7.029158
6.201972	536.616367	7.034163
5.758643	538.848717	7.039168
6.062067	532.340366	7.044173
5.569714	542.058638	7.049178
6.011073	536.205112	7.054182
5.817039	538.787112	7.059187
5.590276	527.361421	7.064192
5.954353	537.613174	7.069197
5.478609	557.640712	7.074202
6.202316	560.861099	7.079206
6.163319	574.299374	7.084211
5.821030	568.213280	7.089216
6.150896	565.744634	7.094221
5.796529	570.925915	7.099226
6.094515	565.627162	7.104230
6.191295	575.960104	7.109235
6.213949	578.440714	7.114240
6.032760	566.993633	7.119245
6.035584	569.480090	7.124250
6.504744	570.721073	7.129254
6.142552	563.790501	7.134259
5.862014	551.707673	7.139264
6.221516	545.243115	7.144269
5.982930	546.616090	7.149274
6.115042	544.962449	7.154278
5.940266	544.572083	7.159283
6.276919	549.078093	7.164288
5.931024	535.032303	7.169293
5.670852	546.422478	7.174298
6.162403	558.478337	7.179302
6.140857	560.816086	7.184307
6.081525	561.282992	7.189312
6.250679	540.257238	7.194317
5.595748	537.440160	7.199322
5.908671	544.983412	7.204326
6.000481	561.567720	7.209331
5.916474	559.791795	7.214336
6.466211	566.142784	7.219341
6.215116	567.293061	7.224346
6.436292	547.024365	7.229350
6.401061	540.374747	7.234355
6.016786	534.944472	7.239360
6.254777	539.691587	7.244365
5.717116	537.841199	7.249370
6.218690	531.196040	7.254374
5.844228	535.826112	7.259379
5.762745	538.854409	7.264384
6.296975	538.020635	7.269389
5.828015	543.612800	7.274394
6.041637	532.869798	7.279398
5.926489	534.173983	7.284403
5.857910	537.146071	7.289408
6.103249	535.233520	7.294413
5.961079	539.130295	7.299418
6.381466	536.611341	7.304422
6.324149	542.333867	7.309427
5.923082	531.984318	7.314432
6.038762	534.773351	7.319437
6.006901	545.069951	7.324442
5.994388	539.793612	7.329446
6.196256	536.954051	7.334451
6.084684	535.716300	7.339456
6.001550	543.482807	7.344461
5.597558	543.001335	7.349466
6.040728	531.847549	7.354470
6.286747	547.441314	7.359475
6.268313	547.619251	7.364480
6.359507	532.861113	7.369485
6.073439	541.300209	7.374490
6.076178	542.316887	7.379494
5.952658	544.161396	7.384499
6.021548	539.866171	7.389504
6.022883	544.287987	7.394509
5.858043	547.059140	7.399514
6.207244	542.140674	7.404518
6.465525	538.197520	7.409523
6.152784	535.916985	7.414528
6.032002	539.365809	7.419533
5.875637	536.966235	7.424538
6.014781	540.636849	7.429542
5.884897	547.969453	7.434547
6.101325	541.285070	7.439552
6.242964	530.309090	7.444557
5.776332	539.726106	7.449562
6.083122	533.870393	7.454566
6.114935	540.370282	7.459571
6.119686	541.853533	7.464576
6.362938	538.949101	7.469581
5.908990	542.889017	7.474586
6.338682	537.456572	7.479590
5.967455	540.699599	7.484595
6.109796	540.485045	7.489600
5.930740	534.116182	7.494605
5.991827	541.642128	7.499610
6.092950	526.539968	7.504614
5.841124	533.274293	7.509619
5.832781	540.854361	7.514624
6.016001	538.464666	7.519629
5.730043	536.192128	7.524634
6.044967	536.548121	7.529638
5.862484	537.288605	7.534643
5.871809	535.356919	7.539648
6.197494	530.274809	7.544653
6.019076	542.112824	7.549658
6.694433	537.099503	7.554662
6.504576	536.866940	7.559667
6.042026	538.499796	7.564672
6.677299	540.848173	7.569677
6.442080	539.996173	7.574682
6.037619	535.108373	7.579686
6.266470	532.611663	7.584691
6.394819	524.835783	7.589696
6.280268	522.677738	7.594701
5.942607	512.455644	7.599706
5.846725	501.187879	7.604710
5.989299	502.855906	7.609715
6.017948	499.769548	7.614720
5.724519	497.632839	7.619725
5.825704	516.951265	7.624730
5.964806	527.395571	7.629734
5.991786	533.868827	7.634739
5.984490	538.904614	7.639744
6.202138	539.639820	7.644749
5.873542	536.454344	7.649754
6.234290	539.287654	7.654758
6.163147	541.988825	7.659763
6.121603	538.513877	7.664768
6.504139	530.706560	7.669773
5.591403	523.815466	7.674778
5.606427	526.671487	7.679782
5.606491	533.018955	7.684787
5.715852	534.196768	7.689792
5.789635	545.178997	7.694797
5.488752	548.582655	7.699802
5.837383	535.257794	7.704806
5.859855	547.601682	7.709811
5.987530	570.248863	7.714816
5.970938	565.719532	7.719821
6.187140	568.005482	7.724826
6.050009	555.318723	7.729830
6.055052	556.999268	7.734835
6.099927	559.687941	7.739840
6.250921	550.197752	7.744845
5.792283	557.089473	7.749850
5.912032	549.878805	7.754854
6.005218	557.028839	7.759859
6.140691	570.415329	7.764864
6.108832	573.359242	7.769869
6.180256	579.286024	7.774874
5.859987	563.804259	7.779878
5.932462	561.747656	7.784883
6.171568	565.124065	7.789888
6.569444	573.704102	7.794893
6.276346	554.443514	7.799898
6.301740	545.742963	7.804902
6.193305	547.741070	7.809907
6.183283	550.835682	7.814912
6.179397	549.744878	7.819917
6.168201	541.515322	7.824922
6.052830	551.785497	7.829926
6.142919	545.411728	7.834931
5.653023	554.922197	7.839936
6.009482	539.964624	7.844941
5.968721	550.322890	7.849946
5.937019	548.235388	7.854950
5.722320	547.292567	7.859955
5.890754	542.377787	7.864960
6.260410	541.940883	7.869965
5.991035	549.057409	7.874970
5.947235	545.165063	7.879974
5.841019	553.709563	7.884979
5.740887	545.365671	7.889984
5.991814	537.543438	7.894989
6.003334	554.975584	7.899994
6.211762	566.484534	7.904998
6.220727	564.780043	7.910003
5.889755	550.813269	7.915008
6.107206	544.495769	7.920013
5.911550	544.422433	7.925018
6.086399	556.953632	7.930022
6.239179	565.210945	7.935027
5.963331	554.970891	7.940032
6.221138	542.156387	7.945037
5.526600	547.579094	7.950042
5.823716	552.544745	7.955046
5.948542	564.167192	7.960051
6.245425	564.693518	7.965056
6.393513	560.566332	7.970061
6.270355	567.295548	7.975066
6.016005	558.997906	7.980070
5.703519	543.868506	7.985075
5.945420	566.659968	7.990080
6.336451	571.546530	7.995085
6.169836	567.738257	8.000090
6.351349	549.399800	8.005094
6.273646	553.092707	8.010099
5.971223	552.117445	8.015104
5.810580	538.623130	8.020109
5.517041	544.820138	8.025126
5.766665	552.686170	8.030144
6.231031	562.564932	8.035162
6.094626	570.380729	8.040179
6.259716	571.490167	8.045197
6.122516	584.973239	8.050214
6.074805	574.119116	8.055232
6.212679	569.925154	8.060250
6.137853	560.307337	8.065267
6.171912	551.472228	8.070285
5.708284	550.786494	8.075302
5.913704	565.381632	8.080320
6.203934	564.960018	8.085338
6.152842	573.891141	8.090355
6.338993	571.460914	8.095373
6.268253	579.241040	8.100390
6.296564	562.858175	8.105408
6.322608	557.880229	8.110426
6.071561	557.378570	8.115443
6.255920	548.418976	8.120461
6.334147	547.891926	8.125478
6.224615	543.999746	8.130496
6.221001	550.168460	8.135514
5.766273	553.211112	8.140531
5.954605	545.882246	8.145549
5.791571	553.561508	8.150566
5.791752	559.717197	8.155584
6.576573	570.182819	8.160602
6.270134	577.741361	8.165619
6.363479	564.828789	8.170637
6.085280	573.907352	8.175654
6.036811	577.271098	8.180672
6.269852	568.504992	8.185690
5.951318	577.175894	8.190707
6.278605	570.653281	8.195725
6.217283	582.015662	8.200742
6.499289	578.434402	8.205760
6.426142	573.923632	8.210778
6.297346	580.093010	8.215795
6.221903	564.715052	8.220813
6.105490	573.799500	8.225830
6.113462	576.437806	8.230848
6.442970	566.551472	8.235866
6.442983	583.800147	8.240883
6.284941	572.440708	8.245901
6.435420	565.404104	8.250918
6.318327	561.810789	8.255936
6.302926	549.179211	8.260954
5.960920	540.179821	8.265971
6.394728	553.004771	8.270989
6.293588	562.536850	8.276006
6.075086	569.784390	8.281024
6.421848	573.919444	8.286042
5.937181	568.452281	8.291059
6.116849	580.945149	8.296077
6.003475	577.774021	8.301094
6.245157	574.723222	8.306112
6.521216	569.952478	8.311130
6.620095	567.782159	8.316147
6.525213	573.887655	8.321165
6.352818	571.524081	8.326182
6.438240	570.933835	8.331200
6.708910	572.735388	8.336218
6.349324	581.126495	8.341235
6.271978	574.688598	8.346253
6.241619	580.895806	8.351270
6.205717	573.824711	8.356288
6.630552	572.513938	8.361306
6.354264	575.508347	8.366323
6.330634	576.302405	8.371341
6.465601	575.555539	8.376358
6.218038	573.281573	8.381376
6.187529	577.484413	8.386394
6.039371	575.374879	8.391411
6.263081	576.603145	8.396429
6.598843	584.018739	8.401446
6.231688	585.706632	8.406464
6.570091	580.831473	8.411482
6.361688	578.197108	8.416499
6.448636	580.077899	8.421517
6.405678	572.222002	8.426534
6.303185	576.471799	8.431552
6.618368	582.870593	8.436570
6.405290	576.479578	8.441587
6.495567	574.910444	8.446605
6.398968	581.068783	8.451622
6.217054	581.970344	8.456640
6.801570	576.202129	8.461658
6.138088	577.404479	8.466675
6.172530	582.333721	8.471693
6.382666	590.740527	8.476710
6.489776	609.251135	8.481728
6.883287	605.992525	8.486746
6.489349	610.964759	8.491763
6.623979	593.833398	8.496781
6.860815	583.463613	8.501798
6.725726	576.534128	8.506816
6.876599	578.784624	8.511834
6.235615	582.874786	8.516851
6.435080	578.442488	8.521869
6.417795	574.085056	8.526886
6.240383	592.391199	8.531904
6.686542	598.936608	8.536922
6.642207	615.799381	8.541939
6.899504	605.985999	8.546957
6.596140	583.382265	8.551974
6.479078	588.986552	8.556992
6.373273	581.041064	8.562010
6.511765	602.367932	8.567027
6.929682	609.946694	8.572045
6.573315	603.576442	8.577063
6.452655	612.081339	8.582080
6.699507	619.687645	8.587098
6.432646	619.237025	8.592115
6.740203	625.715638	8.597133
6.770686	620.067688	8.602151
6.714279	624.938960	8.607168
6.971677	619.436102	8.612186
6.571244	598.863840	8.617203
6.584842	607.642941	8.622221
6.882120	611.525782	8.627239
6.658801	608.539378	8.632256
6.612026	606.465607	8.637274
6.531869	613.532790	8.642291
6.430078	613.848879	8.647309
6.540978	614.822224	8.652327
6.579051	624.133467	8.657344
6.719759	611.500988	8.662362
6.377017	620.828242	8.667379
6.632169	626.058922	8.672397
6.357605	615.602744	8.677415
6.566226	621.843817	8.682432
6.547695	618.416834	8.687450
6.704347	610.635731	8.692467
6.692666	615.319881	8.697485
6.669904	614.160381	8.702503
6.551548	612.160860	8.707520
6.546298	622.401657	8.712538
6.489599	643.016068	8.717555
7.033939	639.469499	8.722573
7.064250	641.095126	8.727591
6.863697	644.096692	8.732608
7.189188	638.068018	8.737626
7.192190	633.893418	8.742643
6.547613	617.286308	8.747661
6.668202	610.911480	8.752679
6.616824	619.319679	8.757696
6.736880	619.808468	8.762714
6.869603	638.401085	8.767731
6.758803	638.661190	8.772749
7.032713	626.947724	8.777767
7.006716	638.020259	8.782784
7.124866	625.140535	8.787802
6.997971	619.503686	8.792819
6.634492	618.170304	8.797837
6.781854	620.002516	8.802855
6.504814	619.355956	8.807872
6.826902	625.175512	8.812890
7.162862	632.929658	8.817907
6.918082	637.593558	8.822925
7.266538	632.789745	8.827943
6.766882	623.570757	8.832960
6.861337	627.466323	8.837978
6.743221	624.466038	8.842995
6.801264	633.483054	8.848013
6.875350	634.450686	8.853031
6.814065	641.611207	8.858048
6.937728	635.998213	8.863066
6.939363	638.995430	8.868083
7.289738	643.078530	8.873101
7.105905	636.366919	8.878119
7.058196	637.303147	8.883136
7.274274	638.622047	8.888154
7.127537	625.431483	8.893171
6.809171	618.226442	8.898189
7.082321	617.226197	8.903207
7.021061	622.756103	8.908224
7.226101	614.340058	8.913242
7.074200	613.438147	8.918259
6.587788	611.248603	8.923277
7.003550	625.918017	8.928295
7.195328	635.365222	8.933312
7.214234	639.608319	8.938330
7.135050	618.103168	8.943347
6.953345	616.774330	8.948365
7.118630	620.139695	8.953383
6.946837	620.050080	8.958400
6.978475	615.840430	8.963418
6.906481	631.576575	8.968435
7.084965	634.707882	8.973453
7.308728	631.395096	8.978471
7.045499	637.235992	8.983488
6.974450	646.121251	8.988506
7.256181	635.308395	8.993523
7.108127	638.141434	8.998541
7.185154	633.695144	9.003559
7.015465	647.312972	9.008576
7.085654	644.940122	9.013594
6.933400	650.312282	9.018611
7.045149	652.868067	9.023629
7.092424	638.991469	9.028647
7.419304	632.451970	9.033664
7.184688	638.930213	9.038682
7.129127	638.373742	9.043699
7.049325	637.570514	9.048717
7.192754	632.928989	9.053735
7.107436	631.556632	9.058752
7.126293	640.019152	9.063770
7.053687	638.512414	9.068787
6.971357	645.683115	9.073805
7.187553	640.446505	9.078823
6.954302	646.130874	9.083840
6.996583	637.908293	9.088858
7.059480	641.165821	9.093875
7.105839	646.210229	9.098893
7.193386	635.070494	9.103911
6.861134	645.077282	9.108928
7.355215	658.390339	9.113946
7.145433	656.887417	9.118963
6.945312	674.216770	9.123981
7.242187	672.972844	9.128999
7.419527	676.562983	9.134016
7.368534	673.868877	9.139034
7.338917	674.806442	9.144051
7.222499	673.695908	9.149069
7.357476	671.342639	9.154087
7.476221	671.268297	9.159104
7.443839	676.076948	9.164122
7.297713	677.262138	9.169139
7.081404	677.679076	9.174157
7.416039	673.097211	9.179175
7.541916	663.492354	9.184192
7.168622	671.610403	9.189210
7.695441	666.560917	9.194227
7.486386	675.112767	9.199245
7.475489	662.031954	9.204263
7.204719	654.114335	9.209280
7.370978	660.786821	9.214298
7.762497	668.517613	9.219315
7.478933	649.064247	9.224333
7.490325	641.739635	9.229351
7.207870	637.500892	9.234368
7.085199	638.851870	9.239386
7.381163	651.421791	9.244403
7.225421	668.133591	9.249421
7.333507	680.384274	9.254439
7.460915	670.690975	9.259456
7.655219	679.498851	9.264474
7.965283	663.056038	9.269491
7.586431	664.611632	9.274509
7.859687	638.270438	9.279527
7.840176	642.704924	9.284544
7.597836	638.888251	9.289562
7.595990	635.364806	9.294579
7.415367	640.046822	9.299597
7.304448	635.385999	9.304615
7.659390	639.564005	9.309632
7.335983	642.863061	9.314650
7.745687	623.679160	9.319667
7.238102	644.960715	9.324685
7.590765	632.507478	9.329703
7.440788	636.978920	9.334720
7.241708	632.010670	9.339738
7.653189	633.404293	9.344755
7.512363	640.585464	9.349773
7.622499	637.935152	9.354791
7.279523	639.008062	9.359808
7.111980	645.548032	9.364826
8.012899	652.891335	9.369843
7.660689	665.722918	9.374861
7.562843	656.236208	9.379879
8.084555	643.944722	9.384896
7.637482	651.320694	9.389914
7.807801	632.714575	9.394931
7.545645	640.753579	9.399949
7.720232	626.200442	9.404967
7.675781	636.226493	9.409984
7.236626	635.113894	9.415002
7.573614	628.241642	9.420019
7.242076	644.497911	9.425037
7.640113	658.610680	9.430055
8.262467	657.999825	9.435072
7.549164	653.391896	9.440090
7.503704	646.776653	9.445107
7.586930	665.773930	9.450125
7.672572	673.778194	9.455143
7.641027	672.855562	9.460160
7.578989	671.593513	9.465178
7.819030	675.177994	9.470195
7.649240	667.589295	9.475213
7.579561	670.254253	9.480231
7.740700	667.789966	9.485248
7.855975	676.160561	9.490266
7.879140	672.037728	9.495283
7.619601	676.430872	9.500301
7.912110	669.690368	9.505319
8.188213	662.625832	9.510336
7.752853	674.250006	9.515354
7.848000	666.258799	9.520371
7.948455	667.758254	9.525389
7.775669	649.726613	9.530407
8.019673	652.406552	9.535424
7.687458	641.635120	9.540442
7.904479	643.756568	9.545459
7.685026	634.590776	9.550477
7.511530	643.137508	9.555495
8.040904	653.664185	9.560512
7.765522	668.354191	9.565530
7.851286	665.653188	9.570547
7.932016	661.655069	9.575565
7.985098	664.801243	9.580583
8.143448	662.100426	9.585600
7.847779	650.784386	9.590618
7.609341	640.100570	9.595635
7.838870	655.466752	9.600653
7.679545	660.712535	9.605671
7.795211	668.172882	9.610688
7.549302	672.953114	9.615706
7.968163	668.903333	9.620723
8.076284	674.088301	9.625741
8.149594	669.538686	9.630759
8.266457	676.460682	9.635776
7.812857	666.948233	9.640794
7.813927	672.395399	9.645811
8.063359	670.038138	9.650829
7.926961	674.654183	9.655847
7.753421	668.921896	9.660864
7.772108	673.816180	9.665882
7.859589	666.601784	9.670899
7.691420	674.089055	9.675917
7.678573	676.077322	9.680935
7.684564	676.936948	9.685952
7.702281	677.880060	9.690970
7.845658	676.506836	9.695987
8.058195	688.611498	9.701005
8.263875	701.541665	9.706023
8.240656	679.079187	9.711040
7.734128	683.773845	9.716058
7.990843	693.652826	9.721075
8.201332	704.716563	9.726093
8.274454	702.044811	9.731111
8.498444	681.494823	9.736128
8.201084	676.566059	9.741146
8.087018	665.515196	9.746163
7.977547	675.236704	9.751181
7.996442	671.846422	9.756199
7.965106	669.012456	9.761216
7.664704	676.345257	9.766234
7.785627	684.766887	9.771251
8.418071	693.415219	9.776269
8.176175	696.894872	9.781287
8.147590	701.050974	9.786304
8.524698	709.580581	9.791322
8.639156	689.545146	9.796339
8.186560	689.029221	9.801357
8.004756	675.734979	9.806375
8.079089	658.796197	9.811392
7.967909	676.526547	9.816410
7.997708	691.360124	9.821427
8.144805	693.914393	9.826445
8.123764	698.434970	9.831463
8.494000	689.962792	9.836480
8.293400	702.595689	9.841498
8.320392	700.644526	9.846515
8.363004	691.603012	9.851533
8.297288	689.856166	9.856551
8.204757	687.299243	9.861568
8.084206	699.144126	9.866586
8.420694	696.218936	9.871603
8.469688	698.865430	9.876621
8.108428	700.223244	9.881639
8.270266	704.669843	9.886656
8.017941	699.724954	9.891674
8.458315	695.277927	9.896691
8.170904	697.270325	9.901709
8.213006	703.027224	9.906727
8.309888	711.853613	9.911744
8.207096	713.367043	9.916762
8.186495	701.599538	9.921779
8.610289	692.948421	9.926797
8.354435	708.650131	9.931815
8.541578	691.969782	9.936832
8.530909	704.044884	9.941850
8.195692	692.721191	9.946867
7.978483	707.569308	9.951885
7.962306	699.300077	9.956903
8.192789	693.139485	9.961920
7.827779	705.599227	9.966938
7.900381	700.209219	9.971955
8.432976	719.245532	9.976973
8.311682	728.390324	9.981991
8.293900	725.104524	9.987008
8.371060	723.328505	9.992026
8.549070	726.859887	9.997043
8.490606	732.296854	10.002061
8.659797	729.108825	10.007079
8.535790	726.425225	10.012096
8.508586	741.877703	10.017114
8.560697	731.832682	10.022131
9.059543	724.225752	10.027149
8.570299	724.087526	10.032167
8.369853	703.655031	10.037184
8.372176	725.372310	10.042202
8.437329	727.444119	10.047219
8.425350	724.927392	10.052237
8.387270	731.357383	10.057255
8.504582	729.630223	10.062272
8.472675	738.819665	10.067290
8.618618	731.645950	10.072307
8.807293	723.164844	10.077325
8.506985	727.802141	10.082343
8.575845	719.794000	10.087360
8.771453	734.597407	10.092378
9.141513	733.088222	10.097395
9.263760	716.872110	10.102413
8.869517	708.908770	10.107431
8.314805	691.611935	10.112448
8.539156	696.974109	10.117466
8.770175	694.146694	10.122483
8.715668	692.312957	10.127501
8.261656	690.435931	10.132519
8.693953	686.751616	10.137536
8.717985	690.878137	10.142554
8.707290	692.474341	10.147571
8.907136	686.830604	10.152589
8.290490	691.330519	10.157607
8.672432	703.375647	10.162624
8.755249	722.674226	10.167642
8.863792	720.845375	10.172659
9.028616	716.623880	10.177677
8.667202	705.462380	10.182695
8.439269	697.348680	10.187712
8.727665	700.986573	10.192730
8.827806	711.250526	10.197747
9.279576	717.911979	10.202765
8.933047	701.410534	10.207783
8.841378	689.257979	10.212800
8.709823	686.216209	10.217818
8.559190	693.910809	10.222835
8.733651	683.056237	10.227853
8.538824	694.275265	10.232871
9.161500	711.033796	10.237888
8.873708	695.431633	10.242906
8.624687	696.636224	10.247923
8.863171	703.855004	10.252941
8.775339	718.723045	10.257959
8.751831	725.387615	10.262976
9.027777	723.663320	10.267994
8.855602	718.731136	10.273011
9.277364	720.810820	10.278029
8.787712	720.651797	10.283047
8.651326	727.798023	10.288064
8.856843	731.733489	10.293082
8.792208	728.349547	10.298099
9.263128	725.439490	10.303117
9.104097	735.656616	10.308135
9.068592	729.258967	10.313152
8.903453	720.359705	10.318170
8.896721	718.820005	10.323187
9.199312	715.934281	10.328205
9.275560	706.933249	10.333223
9.089404	705.330353	10.338240
9.132033	693.713397	10.343258
8.978778	701.873368	10.348275
8.767540	689.503224	10.353293
8.391450	700.578266	10.358311
8.865740	710.094478	10.363328
8.859483	718.034853	10.368346
9.034262	729.970219	10.373363
9.180060	722.380414	10.378381
9.286407	724.197778	10.383399
8.990290	723.121720	10.388416
9.066821	728.037149	10.393434
8.980463	737.802898	10.398451
9.116386	725.729157	10.403469
9.101961	731.700927	10.408487
9.274714	729.493354	10.413504
9.021372	725.448179	10.418522
9.167865	730.193372	10.423539
9.427973	727.922519	10.428557
9.134574	723.683595	10.433575
9.332820	723.653172	10.438592
9.280471	724.924406	10.443610
9.173915	721.939116	10.448627
9.267979	704.113604	10.453645
9.001362	700.100553	10.458663
8.906375	712.420712	10.463680
8.953735	716.904773	10.468698
9.117363	725.653981	10.473715
9.368945	716.217241	10.478733
9.099521	724.425198	10.483751
9.335174	722.865440	10.488768
9.396128	717.911188	10.493786
9.166395	721.448278	10.498803
8.952141	717.791492	10.503821
9.048000	733.906615	10.508839
8.964022	725.400974	10.513856
9.171012	722.322823	10.518874
8.834077	735.594427	10.523891
9.207722	726.741766	10.528909
8.955394	732.956067	10.533927
9.154523	724.892103	10.538944
9.483612	741.151280	10.543962
9.070475	737.587261	10.548979
9.137005	748.092617	10.553997
9.613077	756.186202	10.559015
9.166338	754.763056	10.564032
9.607631	753.072793	10.569050
9.236876	759.248844	10.574067
9.495823	762.561332	10.579085
9.343738	770.541627	10.584103
9.510365	760.720525	10.589120
9.402712	755.890631	10.594138
9.445659	759.730589	10.599155
9.626426	747.930492	10.604173
9.351961	741.461783	10.609191
9.253406	729.542213	10.614208
9.138648	745.677658	10.619226
9.387548	757.518099	10.624243
9.744711	753.874948	10.629261
9.601439	762.529333	10.634279
9.518311	760.067292	10.639296
9.809093	753.399081	10.644314
9.314025	749.649424	10.649331
9.693582	747.460752	10.654349
9.497035	741.518873	10.659367
9.463032	736.670885	10.664384
9.699964	735.723084	10.669402
9.479182	740.999541	10.674419
9.375883	738.180628	10.679437
9.317982	739.257125	10.684455
9.357458	759.193991	10.689472
9.897101	749.706383	10.694490
9.415391	758.871112	10.699507
9.626494	750.197705	10.704525
9.495430	759.480740	10.709543
9.394471	765.548737	10.714560
9.847983	755.865556	10.719578
9.518067	758.500791	10.724595
9.696315	759.124036	10.729613
9.927519	759.525138	10.734631
9.786937	763.783261	10.739648
9.764412	760.989156	10.744666
9.855640	763.718426	10.749683
9.794490	751.866657	10.754701
9.686812	744.523526	10.759719
9.243411	731.347352	10.764736
9.623890	740.510634	10.769754
9.613146	746.007023	10.774771
9.666358	749.912599	10.779789
9.459119	758.897241	10.784807
9.616187	748.257302	10.789824
10.126808	748.636151	10.794842
9.908892	751.799659	10.799859
9.778092	761.639313	10.804877
9.879260	756.959082	10.809895
9.707810	760.490860	10.814912
9.922761	754.595400	10.819930
9.508668	766.505869	10.824947
9.546760	764.630414	10.829965
9.426126	751.097644	10.834983
9.537290	760.599611	10.840000
9.891779	754.313349	10.845018
9.896929	763.779331	10.850035
10.165674	757.667887	10.855053
9.999529	748.697519	10.860071
9.489525	763.751250	10.865088
10.029526	759.142835	10.870106
9.873814	759.547772	10.875123
9.745146	758.188093	10.880141
9.928084	757.443709	10.885159
9.745910	767.021809	10.890176
10.034071	756.036554	10.895194
9.861658	756.882421	10.900211
9.602461	751.507181	10.905229
9.718804	749.973870	10.910247
9.826109	755.760541	10.915264
9.979410	761.667543	10.920282
9.719698	758.985150	10.925299
10.058624	776.598172	10.930317
10.028562	786.499110	10.935335
9.896891	779.168990	10.940352
10.423263	787.560939	10.945370
10.078530	772.159062	10.950387
10.081612	757.981031	10.955405
9.763751	757.014865	10.960423
9.343309	771.850241	10.965440
9.923916	772.659210	10.970458
10.151268	783.679269	10.975475
9.974348	788.483151	10.980493
10.104931	782.907932	10.985511
10.064599	788.285621	10.990528
10.366288	780.713279	10.995546
10.151193	788.528830	11.000563
9.682142	791.900062	11.005581
10.231626	787.269597	11.010599
9.811109	798.072552	11.015616
10.073911	785.981692	11.020634
10.049268	791.815027	11.025651
9.837431	789.914422	11.030669
9.819524	789.048184	11.035687
9.712080	792.508350	11.040704
10.091209	791.287014	11.045722
10.061942	816.559068	11.050739
10.158700	814.417607	11.055757
10.401217	805.329541	11.060775
10.234265	818.619524	11.065792
10.327450	816.472749	11.070810
10.758892	816.961950	11.075827
10.395650	807.608065	11.080845
10.478391	787.813176	11.085863
10.170777	795.227537	11.090880
10.302487	789.538750	11.095898
9.949192	787.111205	11.100915
10.167413	791.881546	11.105933
10.553004	803.185636	11.110951
10.224223	792.942242	11.115968
10.249832	792.129818	11.120986
10.622212	800.179576	11.126003
10.239163	788.959002	11.131021
10.276349	787.182902	11.136039
10.609982	792.734483	11.141056
10.238291	790.763896	11.146074
10.078049	781.774029	11.151091
10.224175	801.103952	11.156109
10.336009	807.996920	11.161127
10.154269	807.991623	11.166144
10.328741	811.468889	11.171162
10.457072	813.768819	11.176179
10.397265	805.619349	11.181197
10.815504	805.391482	11.186215
10.766593	814.523159	11.191232
10.516056	805.907265	11.196250
10.641457	811.372080	11.201267
10.807163	812.830037	11.206285
10.743603	791.558267	11.211303
10.480296	789.538238	11.216320
10.316181	773.348619	11.221338
10.731102	770.497037	11.226355
10.177385	778.780049	11.231373
10.448667	776.793543	11.236391
10.630285	800.683875	11.241408
11.038268	803.565810	11.246426
10.766449	790.215118	11.251443
10.228849	783.642333	11.256461
10.587057	775.230365	11.261479
10.201179	787.421595	11.266496
10.926620	785.879937	11.271514
10.800551	798.112796	11.276531
10.611603	799.782226	11.281549
11.086759	784.087890	11.286567
10.898474	782.840438	11.291584
10.675353	780.181507	11.296602
10.570095	775.866537	11.301619
10.492408	775.362147	11.306637
10.966787	762.436314	11.311655
10.670701	773.422574	11.316672
10.609529	763.516362	11.321690
10.677719	770.231512	11.326707
10.603631	774.473903	11.331725
10.750304	769.067669	11.336743
10.882993	771.140899	11.341760
10.900337	765.318704	11.346778
10.811433	768.738396	11.351795
10.274388	772.800373	11.356813
10.579797	780.949788	11.361831
10.442064	795.555708	11.366848
10.599279	795.532472	11.371866
10.745263	800.095891	11.376883
10.867895	812.306083	11.381901
11.076807	804.406984	11.386919
10.447351	804.076237	11.391936
10.631729	799.876284	11.396954
10.948536	804.784233	11.401971
10.594641	808.045067	11.406989
10.970236	803.892579	11.412007
11.296133	805.229528	11.417024
11.010526	802.249856	11.422042
11.126721	794.886559	11.427059
10.893952	806.526495	11.432077
11.300722	796.583327	11.437095
11.225620	803.317887	11.442112
11.013488	797.397859	11.447130
11.079125	800.331363	11.452147
10.938604	802.584081	11.457165
11.284348	800.945066	11.462183
10.989071	814.530295	11.467200
11.267750	797.193765	11.472218
10.851673	780.864372	11.477235
10.639137	790.221149	11.482253
11.313651	789.972894	11.487271
11.071481	794.499801	11.492288
11.081415	798.629473	11.497306
10.944270	796.085824	11.502323
11.105627	801.265169	11.507341
11.119113	787.261757	11.512359
11.184604	794.560010	11.517376
11.038367	807.385554	11.522394
11.012971	793.001195	11.527411
10.548179	804.260674	11.532429
10.840128	806.345724	11.537447
11.089004	798.144357	11.542464
11.159714	797.216597	11.547482
11.284964	790.478148	11.552499
11.190403	801.832611	11.557517
11.457703	790.262235	11.562535
10.943756	793.433039	11.567552
10.957591	802.809817	11.572570
11.107867	798.000582	11.577587
10.961866	802.816670	11.582605
10.854145	797.132883	11.587623
10.606043	800.765547	11.592640
10.705382	820.216227	11.597658
11.319840	823.298216	11.602675
11.005465	834.897358	11.607693
11.609249	831.201936	11.612711
11.578052	835.170326	11.617728
11.299225	834.350439	11.622746
11.256333	836.274020	11.627763
11.441217	840.871952	11.632781
11.535987	826.123194	11.637799
11.442954	831.655679	11.642816
11.498193	828.029042	11.647834
11.667754	839.268148	11.652851
11.706857	834.587542	11.657869
11.293467	822.154314	11.662887
11.127047	808.816860	11.667904
11.105843	820.915450	11.672922
11.689792	823.047029	11.677939
11.620537	837.499924	11.682957
11.795996	822.587028	11.687975
11.587647	815.716808	11.692992
11.046337	807.428181	11.698010
11.399619	812.220650	11.703027
11.649651	827.771000	11.708045
11.414555	833.692346	11.713063
11.470416	822.746690	11.718080
11.712408	828.801229	11.723098
11.807747	820.841798	11.728115
11.500162	816.414263	11.733133
11.639958	804.850422	11.738151
11.524530	803.829080	11.743168
11.309630	803.696998	11.748186
11.655500	820.038908	11.753203
11.758875	826.680543	11.758221
11.986241	813.773918	11.763239
11.933491	802.581708	11.768256
11.586240	791.947692	11.773274
11.531954	794.877825	11.778291
11.401238	795.980949	11.783309
11.265707	793.859846	11.788327
11.698380	805.237240	11.793344
11.681125	821.553852	11.798362
12.395588	813.701345	11.803379
11.484270	804.017764	11.808397
11.456349	800.471829	11.813415
11.601448	795.856356	11.818432
11.648742	813.512199	11.823450
11.717523	826.665916	11.828467
11.258606	832.207808	11.833485
11.527366	830.539020	11.838503
11.873206	829.395236	11.843520
11.666859	830.328612	11.848538
11.664888	828.587336	11.853555
11.511596	829.149346	11.858573
11.543676	825.865503	11.863591
11.553946	832.992218	11.868608
11.634167	826.581272	11.873626
11.819926	827.940640	11.878643
11.652955	822.450503	11.883661
11.613518	833.803735	11.888679
11.766984	833.725611	11.893696
12.083306	847.978851	11.898714
12.216679	845.510866	11.903731
11.889810	835.234058	11.908749
11.854696	831.110990	11.913767
11.785022	835.041265	11.918784
12.342701	844.781143	11.923802
12.544477	835.582094	11.928819
12.424234	830.059809	11.933837
12.425008	833.086732	11.938855
12.496050	826.237958	11.943872
12.256151	824.450651	11.948890
12.357316	820.734919	11.953907
12.255804	807.234365	11.958925
11.843563	808.041210	11.963943
12.020920	795.992442	11.968960
12.198366	798.792477	11.973978
12.249255	794.743756	11.978995
12.070863	797.949150	11.984013
12.140672	795.200377	11.989031
12.152304	780.818164	11.994048
11.885538	796.787898	11.999066
12.090829	791.188495	12.004083
11.969208	796.681610	12.009101
12.155249	815.147113	12.014119
12.278917	812.082348	12.019136
12.260919	830.163173	12.024154
12.103590	830.145960	12.029171
12.321431	824.020479	12.034189
12.299626	824.598116	12.039207
12.258799	796.295773	12.044224
11.957848	805.406189	12.049242
12.366035	814.995614	12.054259
12.724285	812.901401	12.059277
12.437957	805.911034	12.064295
12.348087	794.536797	12.069312
12.102891	801.094808	12.074330
12.016717	794.002410	12.079347
12.161389	800.874191	12.084365
12.239782	809.983211	12.089383
12.588275	814.384762	12.094400
12.191552	814.311918	12.099418
12.038005	816.852214	12.104435
12.456031	817.910930	12.109453
12.318639	822.114213	12.114471
12.439371	819.354247	12.119488
12.432161	823.000568	12.124506
12.445854	820.478787	12.129523
12.346455	830.236911	12.134541
12.343789	830.187002	12.139559
12.441747	827.184755	12.144576
12.334390	827.004158	12.149594
12.551526	829.280724	12.154611
12.595449	818.252801	12.159629
12.512101	826.324494	12.164647
12.465936	815.355976	12.169664
12.248967	822.819117	12.174682
12.549427	822.213923	12.179699
12.593103	820.169042	12.184717
12.182997	822.839611	12.189735
12.753991	824.841059	12.194752
12.493007	818.977927	12.199770
12.414584	822.775403	12.204787
12.261246	811.291591	12.209805
12.197220	827.386045	12.214823
12.564543	816.007738	12.219840
12.101211	825.686364	12.224858
12.395846	831.993985	12.229875
12.795618	844.453966	12.234893
12.887095	842.346446	12.239911
12.939187	833.606020	12.244928
12.562551	834.018802	12.249946
12.739168	826.598244	12.254963
12.372511	822.094272	12.259981
12.892419	841.247398	12.264999
12.807684	839.943426	12.270016
12.514269	834.445877	12.275034
12.487781	844.349803	12.280051
12.985983	849.213164	12.285069
12.845230	851.176966	12.290087
13.135778	845.189430	12.295104
12.982710	841.265409	12.300122
12.822990	834.670579	12.305139
13.041264	815.138238	12.310157
12.890716	823.336405	12.315175
12.723822	829.522032	12.320192
12.551524	822.858033	12.325210
12.696854	837.021472	12.330227
12.948515	843.411800	12.335245
12.662350	853.386682	12.340263
12.733883	848.025145	12.345280
12.825284	846.032985	12.350298
12.850754	850.212850	12.355315
13.101844	843.442912	12.360333
12.742522	866.713504	12.365351
13.025586	843.057609	12.370368
12.814893	848.661549	12.375386
12.671912	853.044497	12.380403
12.662220	848.020409	12.385421
12.716718	856.035830	12.390439
12.936498	849.525391	12.395456
13.014860	849.436476	12.400474
12.715374	845.486307	12.405491
12.985431	859.388968	12.410509
13.115289	876.911139	12.415527
13.694281	871.580128	12.420544
13.286821	861.630411	12.425562
12.929126	848.326564	12.430579
13.177092	842.464184	12.435597
13.029543	845.160569	12.440615
13.104414	839.524480	12.445632
13.284812	848.372156	12.450650
13.143274	848.973951	12.455667
13.275701	844.434574	12.460685
13.094171	840.599120	12.465703
13.537140	841.804094	12.470720
13.492716	843.498020	12.475738
13.300787	843.622750	12.480755
13.560869	842.994322	12.485773
13.439458	847.209925	12.490791
13.502337	847.309785	12.495808
13.464785	844.968523	12.500826
13.175856	846.060842	12.505843
13.609816	844.657990	12.510861
13.430973	843.763676	12.515879
13.328027	840.085673	12.520896
13.322706	839.914163	12.525914
13.388091	840.043134	12.530931
13.668280	833.814416	12.535949
13.073131	845.883659	12.540967
13.246601	841.000890	12.545984
13.596621	852.973866	12.551002
13.486544	843.843772	12.556019
13.505930	845.447609	12.561037
13.471204	845.837239	12.566055
13.291792	843.255702	12.571072
13.466343	838.966031	12.576090
13.337622	838.638191	12.581107
13.364774	844.733428	12.586125
13.367859	846.490350	12.591143
13.300515	844.338659	12.596160
13.230058	835.428770	12.601178
13.361785	848.525629	12.606195
13.640104	841.303960	12.611213
13.618590	843.990106	12.616231
13.454010	837.743699	12.621248
13.588132	837.330607	12.626266
13.214387	848.024675	12.631283
13.028365	843.663219	12.636301
13.631946	854.949362	12.641319
13.740982	867.998816	12.646336
13.722388	872.636749	12.651354
13.553106	863.313308	12.656371
13.944860	872.942103	12.661389
13.637102	874.827267	12.666407
13.896939	865.006018	12.671424
14.120389	872.382477	12.676442
13.926504	861.762780	12.681459
13.748334	842.952316	12.686477
13.599115	843.078634	12.691495
13.474811	846.259336	12.696512
13.884402	858.508658	12.701530
13.778346	866.237692	12.706547
13.866375	873.819244	12.711565
13.840064	871.021416	12.716583
14.092907	870.203643	12.721600
14.183107	853.455712	12.726618
13.703813	857.027069	12.731635
13.855473	835.779834	12.736653
13.773138	845.502860	12.741671
13.856578	868.325750	12.746688
14.009729	866.176913	12.751706
14.079694	860.322348	12.756723
13.947440	854.827632	12.761741
13.905897	845.462185	12.766759
14.191366	845.578727	12.771776
14.019002	840.924080	12.776794
13.973427	846.912469	12.781811
14.084034	834.949129	12.786829
13.845001	840.453433	12.791847
13.737109	833.750421	12.796864
13.803966	856.194956	12.801882
13.523817	874.267668	12.806899
14.076754	863.147948	12.811917
13.968625	868.279817	12.816935
14.199661	865.756684	12.821952
14.396232	868.272476	12.826970
14.088873	867.638405	12.831987
14.277264	861.828400	12.837005
14.126388	868.288936	12.842023
14.170007	873.025618	12.847040
14.495721	867.316489	12.852058
14.381935	866.991293	12.857075
14.195492	868.686298	12.862093
14.531991	864.169027	12.867111
14.127087	863.415287	12.872128
14.298875	855.024697	12.877146
14.542990	867.432522	12.882163
14.137070	839.207876	12.887181
14.280535	834.841468	12.892199
13.915071	841.911512	12.897216
14.025009	853.594338	12.902234
13.801006	867.249697	12.907251
13.950644	856.397540	12.912269
13.905060	866.862882	12.917287
14.086056	868.111630	12.922304
14.384304	857.156522	12.927322
13.956007	869.849304	12.932339
14.133334	877.614094	12.937357
14.196856	892.361574	12.942375
14.240715	891.313457	12.947392
14.654204	891.922558	12.952410
14.702271	897.250215	12.957427
14.678885	890.022186	12.962445
14.761217	890.295194	12.967463
14.485088	891.435788	12.972480
14.541427	893.156733	12.977498
14.534437	886.588163	12.982515
14.411629	888.776547	12.987533
14.434129	893.313198	12.992551
14.444505	898.686466	12.997568
14.661869	894.564092	13.002586
14.547806	892.108727	13.007603
14.554262	890.032994	13.012621
14.487431	889.016984	13.017639
14.544397	886.919109	13.022656
14.855035	884.926073	13.027674
14.545343	891.970763	13.032691
14.624497	891.959272	13.037709
14.907688	891.704556	13.042727
14.522883	903.212660	13.047744
15.070906	886.792016	13.052762
14.470219	890.031530	13.057779
14.568800	890.231379	13.062797
14.655297	882.281648	13.067815
14.782386	892.844788	13.072832
14.496029	892.267077	13.077850
14.667632	894.997235	13.082867
14.777409	890.667097	13.087885
14.777949	895.323522	13.092903
14.529185	893.256586	13.097920
14.882807	886.386190	13.102938
14.900954	890.506259	13.107955
14.566873	883.497387	13.112973
14.420521	894.898681	13.117991
14.834895	901.499875	13.123008
15.451311	913.750820	13.128026
15.127979	912.133216	13.133043
14.698666	898.947872	13.138061
14.778508	905.544227	13.143079
14.898782	918.143458	13.148096
15.096153	915.942018	13.153114
14.995579	922.377318	13.158131
14.955253	921.369516	13.163149
15.065987	924.195580	13.168167
14.967305	929.358974	13.173184
14.981142	913.548385	13.178202
15.239403	920.783676	13.183219
15.139049	917.959125	13.188237
15.675704	912.707941	13.193255
14.985901	900.819214	13.198272
15.218490	879.686071	13.203290
15.051416	881.360548	13.208307
15.123622	879.444000	13.213325
15.045871	875.844490	13.218343
14.626768	896.283037	13.223360
15.043853	906.427319	13.228378
14.954877	915.692849	13.233395
14.675050	913.829076	13.238413
15.042234	916.696529	13.243431
14.816739	925.595711	13.248448
15.294647	909.573644	13.253466
15.243215	908.815307	13.258483
14.847659	916.210431	13.263501
15.058338	924.768110	13.268519
15.127991	945.208071	13.273536
15.720397	941.558993	13.278554
15.742537	935.483983	13.283571
15.665954	932.984612	13.288589
15.406951	919.969465	13.293607
14.881983	919.418666	13.298624
15.415851	921.895939	13.303642
15.605805	932.527433	13.308659
15.610023	931.930345	13.313677
15.934635	926.938274	13.318695
15.588679	913.692266	13.323712
15.470187	904.557625	13.328730
15.687873	909.830824	13.333747
15.567815	910.401900	13.338765
15.605099	898.595133	13.343783
15.343136	907.599552	13.348800
15.783853	901.386351	13.353818
15.585131	909.249643	13.358835
15.361230	912.226780	13.363853
15.487917	904.271958	13.368871
15.527126	904.532817	13.373888
15.552380	905.853418	13.378906
15.617567	911.066046	13.383923
15.614331	922.717666	13.388941
15.897419	914.971182	13.393959
15.951327	922.289522	13.398976
15.803193	907.060459	13.403994
15.761735	903.941131	13.409011
15.884863	906.479720	13.414029
15.976653	899.119235	13.419047
15.681757	906.057155	13.424064
16.013481	901.448149	13.429082
15.729323	900.086646	13.434099
15.497079	912.198206	13.439117
15.953073	899.415849	13.444135
15.607639	903.229606	13.449152
15.545763	902.037193	13.454170
15.584138	906.748771	13.459187
15.941609	919.235502	13.464205
16.221354	928.350619	13.469223
15.959080	932.403357	13.474240
15.979387	928.149832	13.479258
15.788137	917.360377	13.484275
16.098150	923.331252	13.489293
15.853021	926.591422	13.494311
16.010681	932.279274	13.499328
15.787283	921.104999	13.504346
16.023561	931.363484	13.509363
15.630976	924.690251	13.514381
15.956423	927.359509	13.519399
15.976340	932.940254	13.524416
16.120196	934.677419	13.529434
16.258975	927.211506	13.534451
15.601051	937.788132	13.539469
15.948268	921.818793	13.544487
15.602562	921.900880	13.549504
15.662380	926.002247	13.554522
16.075192	935.929155	13.559539
16.144610	948.757689	13.564557
16.557529	954.062746	13.569575
16.583017	949.291450	13.574592
16.450933	940.027154	13.579610
16.772211	923.513708	13.584627
16.387599	928.347298	13.589645
16.399777	915.688809	13.594663
16.566505	919.431543	13.599680
16.765211	926.049562	13.604698
16.533986	924.501347	13.609715
16.250118	927.481331	13.614733
16.261784	923.248921	13.619751
16.290469	927.660549	13.624768
16.340429	920.876639	13.629786
16.272433	918.436475	13.634803
16.234745	925.544010	13.639821
16.445087	919.949630	13.644839
16.342692	919.898125	13.649856
16.476405	921.383044	13.654874
16.476363	917.357684	13.659891
16.715300	921.357741	13.664909
16.478615	913.098138	13.669927
16.391081	916.990055	13.674944
16.577097	923.386956	13.679962
16.649693	911.955024	13.684979
16.194805	927.630859	13.689997
16.642291	918.498158	13.695015
16.515668	922.000110	13.700032
16.349098	919.401867	13.705050
16.235629	914.132748	13.710067
16.605655	927.363436	13.715085
16.586215	925.630947	13.720103
16.422339	930.109104	13.725120
16.495885	952.622354	13.730138
16.848107	952.342822	13.735155
16.709936	958.040694	13.740173
16.977768	945.995725	13.745191
16.940505	949.590362	13.750208
16.622613	948.332468	13.755226
16.978331	948.813741	13.760243
17.109299	945.850886	13.765261
17.236314	935.489012	13.770279
16.827362	922.049894	13.775296
16.914136	915.594914	13.780314
17.013460	908.932357	13.785331
16.738030	914.428148	13.790349
16.998468	911.354494	13.795367
16.960424	918.682941	13.800384
16.778454	905.306248	13.805402
16.897767	910.439444	13.810419
16.692820	918.487228	13.815437
16.889797	934.738960	13.820455
16.851893	932.928035	13.825472
16.813053	950.708135	13.830490
17.049218	944.881527	13.835507
17.048777	952.936803	13.840525
17.187503	948.421154	13.845543
17.177598	947.225643	13.850560
17.064922	942.346918	13.855578
17.292740	948.850289	13.860595
17.323052	946.332821	13.865613
17.439984	936.265517	13.870631
17.410439	925.296925	13.875648
16.869353	915.365755	13.880666
17.381328	908.943517	13.885683
17.130607	913.022682	13.890701
17.212617	905.497285	13.895719
17.263053	910.426542	13.900736
17.176763	911.157374	13.905754
17.164009	907.264430	13.910771
16.984102	928.059851	13.915789
17.309251	928.634764	13.920807
17.539791	938.983571	13.925824
17.234784	946.892432	13.930842
17.590104	938.734387	13.935859
17.597087	943.829110	13.940877
17.423481	927.660978	13.945895
17.554809	920.328973	13.950912
17.052156	914.010175	13.955930
17.152608	915.841529	13.960947
17.296807	943.200719	13.965965
17.361848	943.853347	13.970983
17.497792	944.509195	13.976000
17.448508	951.013963	13.981018
17.368715	944.131848	13.986035
17.452564	946.891505	13.991053
17.810236	942.502984	13.996071
17.548733	935.502148	14.001088
17.280123	942.777056	14.006106
17.342105	936.905281	14.011123
17.362774	948.043142	14.016141
17.474250	943.053288	14.021159
17.539152	941.365490	14.026176
17.282548	949.259252	14.031194
17.724839	934.611501	14.036211
17.545898	960.001089	14.041229
17.323371	959.936406	14.046247
17.791399	973.878040	14.051264
17.830314	981.279203	14.056282
17.950661	981.338840	14.061299
17.805221	983.384927	14.066317
17.708890	978.925514	14.071335
17.743359	976.804581	14.076352
17.667902	986.943075	14.081370
18.116334	973.512724	14.086387
17.867343	976.564891	14.091405
17.785746	976.559546	14.096423
18.172861	976.336045	14.101440
17.681279	975.556496	14.106458
17.812051	977.992261	14.111475
17.981451	981.196401	14.116493
17.961167	979.786080	14.121511
17.728250	964.859175	14.126528
17.808613	973.856159	14.131546
18.154258	974.621373	14.136563
17.913639	981.246022	14.141581
17.763428	986.056170	14.146599
17.915039	978.277491	14.151616
17.786408	982.589991	14.156634
17.680481	984.063023	14.161651
18.088709	991.699090	14.166669
18.242223	1001.439851	14.171687
18.656513	993.516886	14.176704
18.102764	985.869171	14.181722
18.237694	982.005295	14.186739
18.244035	981.697606	14.191757
17.971646	974.613519	14.196775
18.300018	965.525710	14.201792
18.203623	977.421134	14.206810
18.081231	971.324768	14.211827
18.016275	980.535180	14.216845
18.394513	992.806729	14.221863
18.774514	1001.769074	14.226880
18.238401	986.847079	14.231898
18.607731	982.968011	14.236915
18.158397	976.513198	14.241933
18.372803	986.762744	14.246951
18.244049	992.535838	14.251968
18.242069	1006.749020	14.256986
18.598069	999.476229	14.262003
18.324700	998.019627	14.267021
18.500116	1001.034594	14.272039
18.710012	996.120549	14.277056
18.793569	1007.612592	14.282074
18.736553	995.546573	14.287091
18.455351	985.873888	14.292109
18.499123	995.162365	14.297127
18.856493	999.841622	14.302144
18.866310	982.471848	14.307162
18.540096	965.763221	14.312179
18.606028	963.790223	14.317197
18.127565	971.822697	14.322215
18.853515	986.774347	14.327232
18.531119	999.987079	14.332250
18.757123	991.070136	14.337267
18.767399	988.944546	14.342285
18.781099	1001.076472	14.347303
18.726809	989.983196	14.352320
18.662924	1002.989746	14.357338
18.776593	996.592088	14.362355
18.943617	1001.804025	14.367373
19.153751	997.804864	14.372391
19.242614	986.592221	14.377408
18.818110	996.708994	14.382426
19.248087	991.161682	14.387443
18.676892	979.978815	14.392461
18.807608	978.036819	14.397479
19.271946	990.243718	14.402496
18.921489	996.557834	14.407514
18.913459	991.245641	14.412531
18.868623	993.562067	14.417549
18.739629	999.698574	14.422567
19.100308	992.031720	14.427584
18.999113	997.491997	14.432602
19.057325	994.782902	14.437619
19.135400	994.816076	14.442637
18.805438	998.769020	14.447655
18.937026	996.462719	14.452672
18.992581	994.591825	14.457690
18.937883	991.448689	14.462707
19.149381	992.077068	14.467725
18.743412	993.876150	14.472743
19.098847	994.474397	14.477760
19.168430	998.765498	14.482778
19.146208	1002.523398	14.487795
19.296676	988.507752	14.492813
19.369736	1006.978414	14.497831
19.637492	995.692050	14.502848
18.984489	991.779514	14.507866
18.887291	1000.109880	14.512883
19.309015	1002.603373	14.517901
19.508186	1013.941637	14.522919
19.627030	1005.442020	14.527936
19.377306	1019.163187	14.532954
19.180178	1001.970959	14.537971
19.441516	998.496762	14.542989
19.152423	1009.704069	14.548007
18.988605	1001.975639	14.553024
19.428207	1015.000794	14.558042
19.439012	1013.349111	14.563059
19.676301	1003.593711	14.568077
19.337929	1002.753359	14.573095
19.855086	1004.749574	14.578112
19.761227	1004.194707	14.583130
19.599231	1002.631478	14.588147
19.900357	1001.037231	14.593165
19.648540	1011.873421	14.598183
19.802975	1008.424797	14.603200
19.788813	1012.084912	14.608218
19.629515	1000.375576	14.613235
19.758798	1010.490027	14.618253
19.740694	1007.051469	14.623271
19.625065	1005.051445	14.628288
19.567382	1009.936828	14.633306
19.580892	1008.967741	14.638323
19.871985	1002.809983	14.643341
19.251599	1012.598978	14.648359
19.830487	1027.858473	14.653376
19.316745	1037.057407	14.658394
19.723078	1045.020179	14.663411
19.731655	1038.774152	14.668429
19.691959	1045.097064	14.673447
20.007532	1035.323564	14.678464
20.027728	1043.989225	14.683482
19.823389	1041.866489	14.688499
20.238711	1031.429648	14.693517
20.112208	1039.210184	14.698535
20.183162	1036.961946	14.703552
19.851306	1026.246482	14.708570
19.940555	1031.665394	14.713587
20.004990	1036.424663	14.718605
20.126192	1036.785723	14.723623
20.142838	1032.978034	14.728640
20.182523	1039.533066	14.733658
20.284730	1037.432010	14.738675
20.258725	1038.633162	14.743693
20.246309	1034.865716	14.748711
20.244016	1040.307663	14.753728
20.194519	1035.021218	14.758746
20.139256	1043.252934	14.763763
20.248573	1031.335324	14.768781
20.155527	1035.286055	14.773799
20.071532	1035.725972	14.778816
20.095836	1049.643908	14.783834
20.603295	1066.337656	14.788851
20.755299	1061.155628	14.793869
20.615105	1064.174837	14.798887
20.779773	1049.367443	14.803904
20.769913	1040.133241	14.808922
20.544246	1034.937381	14.813939
20.586442	1027.486625	14.818957
20.404700	1036.074307	14.823975
20.514855	1027.031255	14.828992
20.401902	1021.613595	14.834010
20.292890	1029.990813	14.839027
20.598016	1036.364102	14.844045
20.313357	1050.096198	14.849063
20.527050	1055.373258	14.854080
20.718592	1052.449957	14.859098
20.803759	1056.402285	14.864115
20.970443	1051.930007	14.869133
21.049453	1048.953689	14.874151
21.111901	1035.682863	14.879168
21.253892	1027.819928	14.884186
20.790434	1023.944893	14.889203
21.181860	1015.605639	14.894221
21.155555	1027.780823	14.899239
21.184639	1018.199648	14.904256
21.133080	1026.876394	14.909274
21.135709	1022.947804	14.914291
21.145523	1015.145343	14.919309
20.932237	999.160471	14.924327
21.026662	996.735918	14.929344
20.875242	986.478774	14.934362
20.791108	993.504664	14.939379
21.266088	1002.983545	14.944397
20.916140	1003.739535	14.949415
21.189389	1007.724878	14.954432
21.163668	986.497358	14.959450
20.799640	995.515185	14.964467
21.030421	988.291872	14.969485
20.719478	1016.342278	14.974503
20.850494	1021.281455	14.979520
21.222966	1016.795190	14.984538
21.440822	1019.909035	14.989555
21.188028	1022.339818	14.994573
21.423850	1022.142155	14.999591
21.317152	1026.693547	15.004608
21.347420	1017.549560	15.009626
21.280210	1019.971659	15.014643
21.382702	1012.340460	15.019661
21.093762	1014.066231	15.024679
21.160961	1015.276357	15.029696
21.488972	1012.482822	15.034714
21.292392	1024.742496	15.039731
21.521736	1019.058717	15.044749
21.304486	1020.873795	15.049767
21.069748	1019.219070	15.054784
21.325299	1023.560090	15.059802
21.080277	1026.328156	15.064819
21.201870	1011.751544	15.069837
21.378858	1029.287738	15.074855
21.250957	1031.852167	15.079872
21.418499	1039.788730	15.084890
21.333499	1057.370698	15.089907
21.662021	1052.528722	15.094925
21.357597	1055.717244	15.099943
21.400253	1041.193437	15.104960
21.650824	1053.081072	15.109978
21.531280	1062.748587	15.114995
21.907175	1051.164366	15.120013
21.701576	1053.497578	15.125031
21.654085	1051.546500	15.130048
21.650399	1051.766828	15.135066
21.633864	1058.065439	15.140083
22.034556	1050.993090	15.145101
21.832917	1055.932637	15.150119
21.872312	1058.145759	15.155136
22.044636	1048.955792	15.160154
21.739094	1050.648884	15.165171
21.946007	1041.334694	15.170189
21.962735	1047.286073	15.175207
21.691619	1053.565422	15.180224
22.032025	1047.295941	15.185242
21.821303	1054.520372	15.190259
22.201004	1049.286078	15.195277
21.855856	1049.460194	15.200295
21.972070	1057.381251	15.205312
21.850077	1053.224086	15.210330
21.628618	1072.573878	15.215347
21.968207	1077.424995	15.220365
22.357064	1073.301737	15.225383
22.204150	1079.332791	15.230400
22.670184	1069.219012	15.235418
22.373017	1077.030582	15.240435
22.502036	1069.056786	15.245453
22.269110	1054.452224	15.250471
22.216340	1044.878680	15.255488
22.444054	1029.551830	15.260506
22.253832	1041.739994	15.265523
22.916156	1045.368021	15.270541
22.407474	1042.420908	15.275559
22.563272	1045.519444	15.280576
22.733020	1037.364911	15.285594
22.359965	1035.824815	15.290611
22.424921	1034.057868	15.295629
22.205308	1038.496075	15.300647
22.329991	1037.729435	15.305664
22.610853	1033.689814	15.310682
22.546298	1033.045451	15.315699
22.563311	1027.407457	15.320717
22.660544	1035.396605	15.325735
22.693002	1038.874604	15.330752
22.674007	1032.960691	15.335770
22.353862	1039.244215	15.340787
22.556707	1032.906183	15.345805
22.571764	1030.869162	15.350823
22.402327	1051.415386	15.355840
23.175563	1066.160867	15.360858
22.665482	1068.203566	15.365875
22.607269	1060.500138	15.370893
22.742370	1065.946115	15.375911
22.393732	1073.319371	15.380928
22.880010	1058.355963	15.385946
22.699045	1073.414562	15.390963
22.880527	1068.202848	15.395981
22.966787	1065.399335	15.400999
22.820505	1067.119994	15.406016
22.979944	1058.964794	15.411034
22.927235	1067.788205	15.416051
23.023212	1067.797156	15.421069
22.974696	1066.443074	15.426087
22.813376	1074.371120	15.431104
23.224915	1067.126501	15.436122
22.755696	1068.784495	15.441139
22.642156	1068.397445	15.446157
23.062595	1066.476754	15.451175
22.873819	1068.183583	15.456192
23.004287	1071.724492	15.461210
23.053440	1100.915383	15.466227
23.228486	1093.659519	15.471245
23.664540	1093.267289	15.476263
23.244501	1106.486043	15.481280
23.357465	1099.884529	15.486298
23.395967	1092.293020	15.491315
23.431233	1091.198676	15.496333
23.606936	1088.367751	15.501351
23.382215	1089.701807	15.506368
23.621656	1067.767300	15.511386
23.326560	1068.931912	15.516403
23.069916	1058.700803	15.521421
23.136252	1079.073384	15.526439
23.232789	1089.391332	15.531456
23.569385	1086.986901	15.536474
23.522771	1091.995669	15.541491
23.513608	1088.398926	15.546509
23.524226	1091.174672	15.551527
23.480815	1096.750608	15.556544
23.614259	1087.174944	15.561562
23.694073	1100.515250	15.566579
23.534296	1090.483034	15.571597
23.556259	1085.315837	15.576615
23.608457	1100.328374	15.581632
23.413717	1091.943230	15.586650
23.640174	1094.146248	15.591667
23.422288	1097.558237	15.596685
23.294317	1091.937927	15.601703
23.586766	1108.282298	15.606720
23.708401	1113.091959	15.611738
23.979852	1114.708809	15.616755
24.137061	1112.164004	15.621773
24.427804	1106.229878	15.626791
24.066606	1099.152565	15.631808
24.285948	1084.719929	15.636826
24.204627	1088.117964	15.641843
24.146730	1078.659023	15.646861
24.089872	1076.553593	15.651879
23.616930	1079.704277	15.656896
24.044962	1077.441788	15.661914
23.815117	1075.062256	15.666931
24.204466	1093.791663	15.671949
24.236162	1099.062260	15.676967
24.095909	1093.877434	15.681984
24.074889	1092.944767	15.687002
24.231221	1110.219521	15.692019
24.471881	1120.232533	15.697037
24.479345	1096.863609	15.702055
24.366050	1091.321970	15.707072
24.225266	1081.204334	15.712090
24.350760	1087.500699	15.717107
24.202794	1089.220064	15.722125
24.353067	1096.867007	15.727143
24.346653	1108.233870	15.732160
24.256055	1111.022836	15.737178
24.644558	1108.719252	15.742195
24.143711	1110.790347	15.747213
24.277650	1109.072597	15.752231
24.001947	1124.209922	15.757248
24.262537	1116.458402	15.762266
24.260679	1115.822945	15.767283
23.957362	1116.688931	15.772301
24.687926	1118.631322	15.777319
24.576759	1141.108111	15.782336
24.910625	1140.292263	15.787354
25.148963	1139.480029	15.792371
24.633953	1121.563556	15.797389
25.079079	1105.518370	15.802407
24.929213	1117.130638	15.807424
24.932201	1109.150919	15.812442
25.094011	1110.475304	15.817459
24.736812	1103.714638	15.822477
25.007564	1091.726551	15.827495
24.650440	1112.907457	15.832512
24.725957	1104.704714	15.837530
24.923986	1108.218304	15.842547
24.711844	1107.706245	15.847565
24.847791	1103.265813	15.852583
25.058629	1106.501306	15.857600
24.716012	1114.945990	15.862618
25.129496	1127.714157	15.867635
25.017209	1130.847653	15.872653
25.483564	1133.647941	15.877671
25.035238	1124.042998	15.882688
24.864882	1121.429993	15.887706
25.292701	1125.870861	15.892723
25.220553	1121.745186	15.897741
25.458847	1125.781229	15.902759
25.297174	1128.183554	15.907776
25.394569	1119.352004	15.912794
25.528057	1101.102986	15.917811
25.264330	1100.960087	15.922829
25.326847	1088.226588	15.927847
25.385807	1091.082515	15.932864
25.110955	1092.493768	15.937882
25.207092	1104.695587	15.942899
25.140094	1117.633854	15.947917
25.339684	1117.508723	15.952935
25.319468	1123.645771	15.957952
25.051470	1130.293913	15.962970
25.272148	1127.864970	15.967987
25.145314	1130.083974	15.973005
25.357470	1123.671530	15.978023
25.378554	1134.818906	15.983040
25.444357	1138.465417	15.988058
25.761497	1149.924794	15.993075
25.552737	1147.475619	15.998093
25.741660	1142.789797	16.003111
25.806805	1155.084580	16.008128
25.790424	1147.441109	16.013146
25.861643	1150.532806	16.018163
25.838781	1150.157904	16.023181
26.175190	1150.276252	16.028199
26.007918	1135.018637	16.033216
26.017138	1131.305064	16.038234
26.278675	1119.893659	16.043251
25.928796	1111.600726	16.048269
26.114055	1108.323348	16.053287
26.095834	1114.625805	16.058304
26.157632	1117.965110	16.063322
26.121300	1113.131167	16.068339
26.097976	1117.601459	16.073357
26.039786	1111.136938	16.078375
26.162566	1121.865510	16.083392
26.098057	1109.035708	16.088410
26.032989	1110.760246	16.093427
25.944331	1122.722608	16.098445
26.003927	1123.341895	16.103463
25.963428	1119.083425	16.108480
26.197966	1141.565962	16.113498
26.306531	1140.039019	16.118515
26.113055	1153.325019	16.123533
26.269638	1148.225665	16.128551
26.263918	1145.469257	16.133568
26.185305	1152.734062	16.138586
26.414425	1155.050424	16.143603
26.307280	1154.217051	16.148621
26.393449	1147.091623	16.153639
26.317063	1152.575011	16.158656
26.155780	1149.282567	16.163674
26.472065	1147.374388	16.168691
26.531091	1153.001492	16.173709
26.624266	1138.766857	16.178727
26.263737	1147.884976	16.183744
26.257868	1151.093764	16.188762
26.430258	1162.533813	16.193779
26.093987	1168.373222	16.198797
26.719521	1166.872877	16.203815
26.629070	1175.494730	16.208832
26.661454	1173.665446	16.213850
26.849312	1177.927958	16.218867
26.945088	1180.157351	16.223885
26.604946	1166.355848	16.228903
26.918878	1176.302041	16.233920
27.010690	1172.423605	16.238938
27.236213	1167.120710	16.243955
27.516273	1168.455440	16.248973
27.316972	1161.872141	16.253991
27.550563	1162.837017	16.259008
26.833241	1152.399063	16.264026
26.966190	1136.244123	16.269043
26.926279	1149.906256	16.274061
27.066342	1152.620817	16.279079
27.577733	1162.752410	16.284096
27.356195	1148.735619	16.289114
27.257776	1134.360277	16.294131
26.992123	1138.726611	16.299149
26.973509	1136.059739	16.304167
27.472507	1142.331287	16.309184
27.297613	1158.386177	16.314202
27.197804	1150.261652	16.319219
27.270221	1158.872669	16.324237
27.268908	1165.699103	16.329255
27.488945	1157.231464	16.334272
27.325600	1162.800906	16.339290
27.509318	1153.571984	16.344307
27.434153	1159.117769	16.349325
27.354680	1155.568477	16.354343
27.699176	1151.726945	16.359360
27.374471	1160.441907	16.364378
27.587916	1155.587459	16.369395
27.914477	1157.879026	16.374413
27.647339	1159.073659	16.379431
27.727144	1150.751288	16.384448
27.605449	1153.470216	16.389466
27.820320	1164.946538	16.394483
27.309915	1170.965171	16.399501
27.655255	1160.105592	16.404519
27.911750	1159.206101	16.409536
27.457698	1159.223846	16.414554
27.636079	1158.080998	16.419571
27.614707	1161.506129	16.424589
27.449497	1154.279018	16.429607
27.745736	1167.124899	16.434624
27.799481	1188.723688	16.439642
28.052609	1178.260851	16.444659
28.149215	1191.348856	16.449677
28.037080	1196.160639	16.454695
28.074976	1191.082104	16.459712
27.803230	1190.012999	16.464730
28.108445	1186.071666	16.469747
27.851092	1194.437316	16.474765
27.942780	1185.645648	16.479783
27.899463	1186.613465	16.484800
28.176859	1188.478544	16.489818
28.225774	1189.977924	16.494835
28.075321	1188.447408	16.499853
28.228226	1193.704661	16.504871
28.483178	1194.188456	16.509888
28.157881	1194.871083	16.514906
28.461237	1185.139668	16.519923
28.129772	1187.516181	16.524941
28.652412	1203.563490	16.529959
28.652926	1205.070098	16.534976
28.410918	1198.793847	16.539994
28.614262	1192.029695	16.545011
28.278542	1193.838425	16.550029
28.559387	1209.607282	16.555047
28.880410	1207.539654	16.560064
28.968639	1216.424457	16.565082
28.842272	1191.789001	16.570099
28.829018	1185.463854	16.575117
28.603745	1177.103404	16.580135
28.900236	1181.601072	16.585152
28.389447	1187.239076	16.590170
28.429204	1186.355787	16.595187
28.494599	1199.229287	16.600205
28.548390	1211.832680	16.605223
28.860681	1207.692538	16.610240
29.040982	1217.989617	16.615258
29.341777	1215.965887	16.620275
29.070070	1217.385291	16.625293
28.842878	1224.046401	16.630311
28.951104	1208.690341	16.635328
29.156325	1214.704666	16.640346
28.918441	1209.829265	16.645363
28.805138	1215.134148	16.650381
28.698871	1211.373538	16.655399
28.954767	1206.602199	16.660416
28.838442	1210.109597	16.665434
29.164960	1208.644587	16.670451
29.206409	1209.979855	16.675469
29.111342	1210.927108	16.680487
29.442274	1226.686508	16.685504
29.145537	1239.248753	16.690522
29.726216	1225.706133	16.695539
29.252477	1232.909632	16.700557
29.236613	1229.582856	16.705575
29.624619	1230.280836	16.710592
29.468498	1242.436740	16.715610
29.314264	1232.924761	16.720627
29.567222	1234.836805	16.725645
29.420013	1227.751164	16.730663
29.796366	1228.571149	16.735680
29.645072	1240.108945	16.740698
29.804079	1231.659639	16.745715
29.997719	1239.281756	16.750733
29.672060	1235.407865	16.755751
30.115774	1232.999848	16.760768
29.839100	1228.871397	16.765786
29.858321	1218.613794	16.770803
29.835973	1202.473870	16.775821
29.692598	1218.591712	16.780839
29.823435	1218.393321	16.785856
29.731243	1221.999085	16.790874
29.773036	1228.869589	16.795891
29.908630	1227.840117	16.800909
29.586888	1226.638740	16.805927
30.087830	1225.833412	16.810944
30.260443	1238.853755	16.815962
29.910749	1228.035987	16.820979
30.297825	1229.508117	16.825997
29.801884	1239.423888	16.831015
29.897029	1226.352992	16.836032
30.020882	1237.053908	16.841050
29.969002	1229.316671	16.846067
30.042055	1223.574840	16.851085
30.008260	1247.735386	16.856103
30.184787	1254.506034	16.861120
30.105325	1264.327663	16.866138
30.473584	1259.879428	16.871155
30.231437	1260.184912	16.876173
30.275702	1259.485907	16.881191
30.660562	1255.708137	16.886208
30.549654	1263.759819	16.891226
30.684320	1259.035703	16.896243
30.452958	1252.245080	16.901261
30.370123	1260.801942	16.906279
30.836182	1253.232863	16.911296
30.563031	1253.329706	16.916314
30.624749	1251.371937	16.921331
30.800225	1250.809864	16.926349
30.434454	1254.786518	16.931367
30.347691	1246.339711	16.936384
30.532748	1250.707429	16.941402
30.764534	1246.125499	16.946419
30.608513	1253.665366	16.951437
30.886170	1266.618735	16.956455
31.367531	1274.124726	16.961472
31.140705	1266.837688	16.966490
30.934541	1257.575625	16.971507
30.789358	1246.143287	16.976525
30.727020	1253.611738	16.981543
31.027141	1261.222927	16.986560
30.911352	1272.843055	16.991578
31.422148	1284.531879	16.996595
31.070105	1290.022771	17.001613
31.397074	1289.474588	17.006631
31.412297	1279.535711	17.011648
31.378005	1279.900477	17.016666
31.288039	1268.972354	17.021683
31.147350	1255.513326	17.026701
31.155551	1269.604595	17.031719
31.353432	1269.846274	17.036736
31.516446	1281.472211	17.041754
31.366513	1278.830602	17.046771
31.664008	1269.380020	17.051789
31.131545	1277.876304	17.056807
31.297515	1283.427874	17.061824
31.496736	1271.756605	17.066842
31.622721	1274.767606	17.071859
31.483283	1274.396650	17.076877
31.351575	1272.196108	17.081895
31.735638	1275.687987	17.086912
31.834223	1275.260690	17.091930
31.800453	1270.369189	17.096947
31.787229	1264.636905	17.101965
31.571569	1278.049517	17.106983
31.900275	1271.684249	17.112000
32.012869	1279.043040	17.117018
31.799955	1269.165960	17.122035
32.008851	1268.980627	17.127053
31.782860	1262.338320	17.132071
31.889905	1269.815346	17.137088
31.741682	1279.247592	17.142106
31.658405	1281.140121	17.147123
32.001894	1284.577698	17.152141
31.582456	1303.230260	17.157159
32.004166	1298.459784	17.162176
31.842031	1308.566779	17.167194
31.921878	1306.561513	17.172211
32.139344	1302.317758	17.177229
31.988988	1300.952566	17.182247
32.387224	1297.319419	17.187264
32.396695	1308.529077	17.192282
32.072520	1299.849904	17.197299
32.319333	1307.572697	17.202317
32.512473	1321.695595	17.207335
32.950993	1314.734184	17.212352
32.989452	1304.659950	17.217370
32.762505	1291.493908	17.222387
32.762701	1295.078092	17.227405
32.626753	1297.388391	17.232423
32.675354	1294.582411	17.237440
32.897993	1293.981033	17.242458
32.775063	1296.013984	17.247475
32.997613	1285.026229	17.252493
32.800359	1291.910358	17.257511
32.755561	1290.976104	17.262528
33.076684	1290.681640	17.267546
32.838194	1279.702119	17.272563
33.055943	1287.465934	17.277581
32.805028	1286.704389	17.282599
32.662278	1285.929659	17.287616
32.882649	1288.764015	17.292634
32.999731	1285.178211	17.297651
33.093960	1286.569705	17.302669
33.015228	1291.139377	17.307687
33.098829	1293.648750	17.312704
32.958745	1287.878015	17.317722
32.975638	1284.973353	17.322739
32.876888	1284.166535	17.327757
32.530067	1284.610608	17.332775
32.528529	1288.907661	17.337792
32.949632	1312.481579	17.342810
32.740668	1317.340534	17.347827
33.032915	1319.033095	17.352845
33.027647	1333.446331	17.357863
33.248807	1326.795703	17.362880
33.360945	1328.470451	17.367898
33.184757	1329.579566	17.372915
33.396744	1333.321601	17.377933
33.212339	1342.417757	17.382951
33.474487	1352.731687	17.387968
33.505109	1342.735103	17.392986
33.341655	1346.230650	17.398003
33.737997	1345.470589	17.403021
33.806556	1346.223044	17.408039
33.536521	1345.734735	17.413056
33.501068	1340.843491	17.418074
33.876813	1340.047077	17.423091
34.124031	1340.465624	17.428109
33.763802	1340.815464	17.433127
34.170854	1338.496178	17.438144
33.833856	1344.138137	17.443162
33.617638	1338.308732	17.448179
33.762847	1331.641939	17.453197
34.021159	1342.668296	17.458215
33.857802	1361.319470	17.463232
34.302772	1352.560942	17.468250
34.017423	1370.174076	17.473267
34.449974	1365.566743	17.478285
34.410740	1360.345809	17.483303
34.205330	1352.804401	17.488320
34.516223	1343.146048	17.493338
34.035953	1345.560216	17.498355
34.017081	1349.021194	17.503373
34.051052	1353.718283	17.508391
34.198341	1361.434748	17.513408
34.634399	1365.224727	17.518426
34.053700	1362.304041	17.523443
34.390180	1356.918930	17.528461
34.409590	1361.359383	17.533479
34.587951	1362.171609	17.538496
34.677160	1356.503037	17.543514
34.503290	1353.141375	17.548531
34.793914	1350.284288	17.553549
34.585091	1354.927093	17.558567
34.443119	1359.985595	17.563584
34.507790	1351.644363	17.568602
34.528176	1375.648500	17.573619
34.860704	1383.266196	17.578637
34.805905	1384.093408	17.583655
35.004996	1390.479677	17.588672
35.454938	1382.801002	17.593690
34.937333	1383.752482	17.598707
35.007456	1365.874268	17.603725
35.174669	1364.448614	17.608743
35.144991	1353.356514	17.613760
35.157736	1348.765942	17.618778
35.087124	1349.959543	17.623795
34.975380	1351.301686	17.628813
35.363990	1358.756542	17.633831
35.346938	1377.952005	17.638848
35.420887	1373.407196	17.643866
34.650943	1372.826862	17.648883
34.996762	1370.509836	17.653901
35.072610	1376.477930	17.658919
35.211241	1383.286406	17.663936
35.486385	1379.654330	17.668954
35.254792	1382.450155	17.673971
35.335791	1377.743944	17.678989
35.782626	1379.238872	17.684007
35.508836	1376.783105	17.689024
35.622529	1378.017056	17.694042
35.135008	1380.571010	17.699059
35.610867	1389.100000	17.704077
35.718668	1398.624570	17.709095
35.640371	1407.634298	17.714112
35.743837	1408.422708	17.719130
35.896606	1415.172164	17.724147
36.163142	1415.339487	17.729165
35.949938	1408.125716	17.734183
35.737664	1404.604655	17.739200
36.062098	1401.852983	17.744218
36.218086	1407.234206	17.749235
36.021238	1404.251923	17.754253
36.164334	1400.151556	17.759271
35.949938	1397.932405	17.764288
36.464270	1403.330275	17.769306
36.162546	1402.068876	17.774323
36.219854	1394.043009	17.779341
36.279337	1400.257913	17.784359
36.026375	1408.009967	17.789376
36.281793	1394.733259	17.794394
36.338511	1396.210895	17.799411
36.659871	1393.974686	17.804429
36.662174	1399.147498	17.809447
36.741121	1399.464778	17.814464
36.815466	1388.901089	17.819482
36.247447	1401.828458	17.824499
36.352227	1394.567160	17.829517
36.403912	1391.237039	17.834535
36.452507	1393.223885	17.839552
36.445087	1397.508163	17.844570
36.653184	1403.960269	17.849587
36.461851	1402.825078	17.854605
36.692851	1386.054045	17.859623
36.331213	1403.196785	17.864640
36.705527	1409.999712	17.869658
36.793351	1425.242096	17.874675
36.639886	1420.612096	17.879693
36.704364	1419.258958	17.884711
36.756242	1430.620737	17.889728
37.096426	1419.313019	17.894746
36.984698	1418.078032	17.899763
36.938945	1418.908079	17.904781
37.324946	1424.583502	17.909799
37.247904	1414.474385	17.914816
37.260789	1416.368724	17.919834
37.294955	1421.089817	17.924851
37.189779	1414.072326	17.929869
37.396238	1413.444883	17.934887
37.060086	1422.897310	17.939904
37.673753	1414.569077	17.944922
37.402707	1417.516714	17.949939
37.306457	1413.235899	17.954957
37.477055	1417.843851	17.959975
37.388195	1420.220779	17.964992
37.279467	1418.267589	17.970010
37.385326	1433.922344	17.975027
37.391613	1446.770011	17.980045
38.147791	1451.758961	17.985063
37.820348	1452.795886	17.990080
37.849997	1450.331202	17.995098
38.065513	1455.431328	18.000115
38.094682	1451.462016	18.005133
37.563893	1436.986332	18.010151
37.393525	1446.806200	18.015168
37.562255	1442.447644	18.020186
37.965311	1450.023380	18.025203
38.254131	1451.182672	18.030221
38.309022	1444.270552	18.035239
37.769347	1451.227984	18.040256
38.073966	1446.942201	18.045274
37.847867	1440.451014	18.050291
37.496360	1449.892614	18.055309
38.140730	1455.625661	18.060327
38.149795	1474.785817	18.065344
38.255522	1481.715137	18.070362
38.453321	1491.340216	18.075379
38.374679	1480.786442	18.080397
38.665861	1473.266686	18.085415
38.771699	1484.491618	18.090432
38.802236	1480.683487	18.095450
38.760614	1470.471226	18.100467
38.533642	1461.794763	18.105485
38.616580	1454.152412	18.110503
38.245635	1461.160650	18.115520
38.544289	1461.450213	18.120538
38.800146	1459.309879	18.125555
38.679232	1470.397938	18.130573
38.869672	1466.305070	18.135591
39.057462	1471.966873	18.140608
38.878443	1465.559612	18.145626
38.966428	1465.256898	18.150643
38.900654	1462.625337	18.155661
39.259050	1463.582954	18.160679
39.223265	1460.467299	18.165696
39.376509	1463.634059	18.170714
39.264182	1467.449510	18.175731
39.145747	1472.230532	18.180749
39.193521	1456.015348	18.185767
38.899732	1463.767496	18.190784
38.947653	1469.646945	18.195802
39.203408	1458.416957	18.200819
39.283083	1465.603337	18.205837
39.294253	1466.269632	18.210855
38.902641	1458.676721	18.215872
38.945825	1465.675838	18.220890
39.208401	1479.501559	18.225907
39.194265	1486.308210	18.230925
39.524253	1494.281889	18.235943
39.538207	1495.513074	18.240960
39.442077	1498.380977	18.245978
39.742921	1486.108867	18.250995
39.589298	1492.872869	18.256013
39.906753	1483.171611	18.261031
39.515810	1496.244146	18.266048
39.750080	1494.292027	18.271066
39.952262	1487.396444	18.276083
40.069337	1494.031768	18.281101
40.167937	1486.893496	18.286119
39.880558	1497.363867	18.291136
39.916952	1490.102037	18.296154
40.009850	1482.674163	18.301171
39.741507	1498.099606	18.306189
40.077567	1501.977043	18.311207
39.909071	1513.102144	18.316224
40.068241	1515.579750	18.321242
40.217613	1510.265725	18.326259
40.225811	1516.391137	18.331277
40.655388	1511.212605	18.336295
40.704117	1510.767966	18.341312
40.329325	1513.713902	18.346330
40.696848	1508.500370	18.351347
40.510339	1516.945800	18.356365
40.559602	1505.169658	18.361383
40.836187	1517.859638	18.366400
40.808297	1517.448946	18.371418
41.162271	1500.243651	18.376435
40.833051	1513.529208	18.381453
40.960294	1509.542854	18.386471
40.885367	1486.979891	18.391488
40.817977	1476.910867	18.396506
40.868521	1478.498981	18.401523
40.634154	1495.688859	18.406541
40.932541	1499.578044	18.411559
40.530526	1501.363928	18.416576
41.004602	1503.052781	18.421594
41.023478	1497.782809	18.426611
40.758702	1500.786903	18.431629
40.898177	1501.860692	18.436647
40.662368	1507.525325	18.441664
40.840822	1513.626089	18.446682
40.957682	1523.458682	18.451699
40.976221	1537.191398	18.456717
40.946790	1533.693970	18.461735
40.862647	1539.442557	18.466752
40.782611	1540.562930	18.471770
41.402432	1545.889055	18.476787
41.448748	1559.302232	18.481805
42.166434	1554.409051	18.486823
41.979341	1554.490070	18.491840
41.899834	1542.374593	18.496858
42.191567	1533.391339	18.501875
41.694773	1528.924059	18.506893
41.926059	1533.092865	18.511911
42.054147	1529.101642	18.516928
41.660610	1526.328279	18.521946
41.976522	1525.666173	18.526963
41.979397	1531.249956	18.531981
42.298703	1517.156664	18.536999
41.640949	1524.134073	18.542016
41.629043	1527.243940	18.547034
41.978297	1527.715677	18.552051
42.243754	1554.080680	18.557069
42.374442	1553.165778	18.562087
42.273513	1553.100641	18.567104
42.474759	1560.061031	18.572122
42.517014	1542.006521	18.577139
42.442826	1529.801591	18.582157
42.443532	1519.858271	18.587175
42.510089	1514.721342	18.592192
42.457357	1524.208791	18.597210
42.640347	1523.121847	18.602227
42.238561	1527.742716	18.607245
42.196001	1536.485974	18.612263
42.544766	1542.482171	18.617280
42.508123	1558.202773	18.622298
42.890688	1549.335178	18.627315
42.577804	1555.081882	18.632333
42.628106	1555.123199	18.637351
42.752046	1556.462555	18.642368
42.411553	1558.128023	18.647386
42.580144	1552.393087	18.652403
42.530260	1552.463985	18.657421
42.654800	1556.082759	18.662439
43.017904	1574.470641	18.667456
43.278156	1588.638182	18.672474
43.125178	1582.623804	18.677491
42.707663	1590.350438	18.682509
42.961671	1586.558035	18.687527
43.314138	1579.933590	18.692544
43.254500	1584.261605	18.697562
43.273774	1569.460860	18.702579
43.197686	1584.047472	18.707597
43.261473	1585.020413	18.712615
43.326018	1579.744033	18.717632
43.302523	1581.599140	18.722650
43.429255	1574.882153	18.727667
43.434808	1593.944219	18.732685
43.331169	1611.057067	18.737703
43.747438	1596.401193	18.742720
43.857685	1610.199104	18.747738
43.846874	1601.126142	18.752755
43.836891	1608.016804	18.757773
43.875696	1602.203733	18.762791
43.949871	1609.437941	18.767808
43.773061	1601.907817	18.772826
44.060280	1589.885125	18.777843
43.889123	1598.020183	18.782861
44.179798	1596.703987	18.787879
44.346388	1590.815038	18.792896
44.238182	1595.716057	18.797914
44.374913	1591.704489	18.802931
44.018634	1595.284381	18.807949
44.170596	1590.832891	18.812967
44.248067	1588.927982	18.817984
44.437707	1593.071811	18.823002
44.301658	1595.202643	18.828019
44.283671	1596.046999	18.833037
44.348319	1594.439882	18.838055
44.253892	1594.087054	18.843072
43.847996	1607.161370	18.848090
44.870422	1623.285026	18.853107
44.528199	1627.246456	18.858125
44.652790	1632.701854	18.863143
44.592608	1628.287842	18.868160
44.559102	1630.964298	18.873178
44.852561	1624.475589	18.878195
44.776178	1629.623712	18.883213
44.825056	1613.330228	18.888231
44.861507	1618.737223	18.893248
44.758085	1630.736279	18.898266
45.128078	1648.259722	18.903283
45.106139	1654.772463	18.908301
45.502572	1653.598987	18.913319
45.500027	1651.770312	18.918336
45.387869	1640.657411	18.923354
45.258519	1624.665473	18.928371
45.338318	1621.147577	18.933389
45.192542	1633.551286	18.938407
45.457502	1644.098017	18.943424
45.078384	1651.349426	18.948442
45.427749	1648.794371	18.953459
45.398380	1640.419342	18.958477
45.282486	1650.590949	18.963495
45.402334	1643.784915	18.968512
45.381679	1655.684459	18.973530
45.469593	1647.524653	18.978547
45.571316	1646.179502	18.983565
45.509485	1665.308719	18.988583
46.014686	1669.280240	18.993600
45.778182	1675.668279	18.998618
45.893889	1680.557841	19.003635
45.958532	1674.495582	19.008653
45.991429	1678.273260	19.013671
46.097190	1679.738472	19.018688
46.070539	1682.550022	19.023706
46.331018	1673.743517	19.028723
46.216642	1681.614098	19.033741
46.108217	1680.149015	19.038759
46.118958	1668.073616	19.043776
46.199832	1675.043752	19.048794
46.340642	1671.870468	19.053811
46.583959	1677.270397	19.058829
46.439610	1677.624261	19.063847
46.585025	1670.662406	19.068864
46.415911	1677.292832	19.073882
46.720329	1663.450300	19.078899
46.399510	1667.818040	19.083917
46.748334	1693.187977	19.088935
46.885200	1688.976361	19.093952
46.579361	1690.731774	19.098970
47.051802	1688.228382	19.103987
46.844676	1683.263092	19.109005
46.735154	1689.517906	19.114023
46.867224	1683.963773	19.119040
46.680599	1697.676665	19.124058
46.998899	1685.120010	19.129075
46.942505	1687.720738	19.134093
46.962415	1694.593890	19.139111
47.449518	1686.776236	19.144128
47.141340	1695.583248	19.149146
47.003149	1709.882622	19.154163
47.033207	1717.004499	19.159181
47.371875	1719.503992	19.164199
47.523452	1716.916321	19.169216
47.225711	1724.256258	19.174234
47.398218	1719.609596	19.179251
47.761327	1716.644772	19.184269
47.300195	1719.337323	19.189287
47.648105	1710.702542	19.194304
47.331357	1719.740515	19.199322
47.642146	1729.726171	19.204339
48.117735	1732.660872	19.209357
47.832926	1741.130573	19.214375
48.321593	1728.714574	19.219392
48.151409	1730.586900	19.224410
48.200523	1737.851696	19.229427
48.480594	1727.743481	19.234445
48.232829	1715.478168	19.239463
48.364384	1693.168908	19.244480
47.878003	1698.722342	19.249498
48.040848	1716.688038	19.254515
48.217799	1722.846220	19.259533
48.343857	1735.329412	19.264551
48.570275	1729.671451	19.269568
48.357991	1730.605072	19.274586
48.358533	1719.316366	19.279603
48.391446	1709.040425	19.284621
48.560489	1725.586199	19.289639
48.551535	1721.032181	19.294656
48.452084	1722.230586	19.299674
48.786156	1727.869838	19.304691
48.913517	1727.539340	19.309709
48.646852	1733.388299	19.314727
49.084116	1720.421758	19.319744
49.110326	1730.823434	19.324762
48.626686	1725.844464	19.329779
49.260978	1722.361113	19.334797
49.063256	1720.999001	19.339815
49.113365	1721.973428	19.344832
49.081340	1722.085465	19.349850
49.035772	1722.629275	19.354867
49.321417	1734.687614	19.359885
49.135916	1740.953455	19.364903
49.378499	1744.920842	19.369920
49.178717	1756.563900	19.374938
48.987186	1762.402004	19.379955
49.378996	1748.476816	19.384973
49.250016	1766.356241	19.389991
49.226580	1755.366758	19.395008
49.235033	1760.469774	19.400026
49.501585	1772.440752	19.405043
49.582790	1779.868366	19.410061
49.431278	1783.421088	19.415079
49.612183	1773.706433	19.420096
49.087874	1786.341839	19.425114
49.328535	1791.309172	19.430131
50.055007	1800.256350	19.435149
49.814601	1801.707237	19.440167
49.793514	1815.537312	19.445184
50.257512	1808.302959	19.450202
50.578035	1803.867200	19.455219
50.237488	1799.532238	19.460237
50.432804	1808.797685	19.465255
50.680569	1795.988444	19.470272
50.630877	1795.764821	19.475290
50.522988	1799.541429	19.480307
50.532068	1792.215869	19.485325
50.401098	1805.775150	19.490343
50.937724	1797.549631	19.495360
50.880088	1799.797036	19.500378
50.822571	1796.444357	19.505395
50.993317	1796.702744	19.510413
50.641416	1798.409495	19.515431
51.070822	1797.675043	19.520448
50.749901	1799.632967	19.525466
50.840494	1805.591305	19.530483
50.705061	1799.447557	19.535501
50.791732	1799.869473	19.540519
51.112750	1791.178076	19.545536
50.820494	1798.807694	19.550554
51.125997	1814.580172	19.555571
51.311453	1820.293279	19.560589
51.544772	1830.011508	19.565607
51.639317	1821.054833	19.570624
51.554484	1821.144118	19.575642
51.544121	1822.232896	19.580659
51.727060	1819.962067	19.585677
51.703606	1821.116006	19.590695
51.456696	1812.969425	19.595712
51.879723	1812.017916	19.600730
51.770630	1813.791947	19.605747
52.047807	1814.135075	19.610765
51.480764	1807.969086	19.615783
51.559054	1815.669250	19.620800
51.707861	1806.442966	19.625818
51.314904	1820.612968	19.630835
51.627547	1806.437841	19.635853
51.641754	1827.373981	19.640871
51.910054	1828.731978	19.645888
52.206263	1838.502005	19.650906
51.960870	1851.968066	19.655923
52.421556	1847.209870	19.660941
52.434963	1857.562569	19.665959
52.547241	1856.173920	19.670976
52.355777	1850.744558	19.675994
52.270640	1860.223404	19.681011
52.421026	1854.027192	19.686029
52.288231	1848.347168	19.691047
52.467653	1854.275462	19.696064
52.702396	1846.851488	19.701082
52.496149	1849.472723	19.706099
52.416183	1844.100494	19.711117
52.298087	1854.413152	19.716135
52.500002	1876.640738	19.721152
52.802650	1873.787079	19.726170
52.802655	1876.065896	19.731187
52.830557	1875.295950	19.736205
52.825301	1881.720983	19.741223
52.688610	1871.739162	19.746240
53.126369	1880.040873	19.751258
52.885626	1906.546984	19.756275
53.259915	1903.560196	19.761293
52.947357	1906.551412	19.766311
53.250607	1903.742924	19.771328
53.337927	1902.864318	19.776346
53.473822	1902.362715	19.781363
53.657394	1903.600101	19.786381
54.159706	1903.059089	19.791399
53.865359	1906.515408	19.796416
53.985506	1896.713884	19.801434
54.077843	1898.438431	19.806451
54.352510	1894.937815	19.811469
54.021993	1897.395379	19.816487
54.009137	1899.710188	19.821504
54.114621	1896.501762	19.826522
54.317924	1902.280449	19.831539
54.376082	1895.208137	19.836557
54.402200	1894.272340	19.841575
54.182684	1898.500140	19.846592
54.274849	1897.614826	19.851610
54.270947	1898.799786	19.856627
54.105419	1903.493460	19.861645
53.823579	1899.477889	19.866663
53.789510	1897.583931	19.871680
54.083391	1891.754502	19.876698
54.005811	1913.696917	19.881715
54.161610	1918.112978	19.886733
54.431787	1925.879852	19.891751
54.405249	1919.270773	19.896768
54.812593	1935.079664	19.901786
54.973842	1944.951239	19.906803
55.289795	1947.452956	19.911821
55.186535	1932.413881	19.916839
54.862769	1929.742279	19.921856
55.166460	1921.488727	19.926874
54.629765	1927.038367	19.931891
54.869511	1941.693494	19.936909
55.115381	1946.432452	19.941927
55.143150	1952.561094	19.946944
55.338927	1951.570431	19.951962
55.120114	1962.702217	19.956979
55.395887	1942.540815	19.961997
55.358059	1956.226934	19.967015
55.382442	1957.919825	19.972032
55.385459	1948.620743	19.977050
55.247743	1963.149015	19.982067
55.350964	1967.833644	19.987085
55.293846	1976.309868	19.992103
55.486815	1970.963271	19.997120
56.009921	1963.158417	20.002138
55.835663	1971.192213	20.007155
56.070937	1971.262749	20.012173
55.962618	1968.989335	20.017191
55.900301	1963.340514	20.022208
56.257278	1964.909437	20.027226
56.031656	1974.558467	20.032243
56.286385	1984.691368	20.037261
56.473501	1986.621103	20.042279
56.550397	1995.799181	20.047296
56.625267	1982.858567	20.052314
56.609907	1992.473582	20.057331
56.530660	1974.530815	20.062349
56.723085	1979.258553	20.067367
56.744728	1990.206446	20.072384
57.307106	1981.893888	20.077402
57.111086	1963.271240	20.082419
56.759630	1961.414865	20.087437
57.030817	1952.351306	20.092455
56.699672	1947.143073	20.097472
56.977311	1952.538597	20.102490
56.487523	1957.158020	20.107507
56.494832	1976.749804	20.112525
56.879283	1981.972925	20.117543
56.816075	1983.412993	20.122560
56.951162	1981.270932	20.127578
57.034845	2001.850520	20.132595
57.215792	2005.794320	20.137613
57.552003	2008.858849	20.142631
57.734883	2005.092297	20.147648
57.577824	2003.645865	20.152666
57.591793	2018.247895	20.157683
57.559541	2012.324780	20.162701
57.795339	1998.529928	20.167719
57.748124	1998.696452	20.172736
57.892428	2004.909759	20.177754
57.898104	2003.380083	20.182771
57.744815	2008.974933	20.187789
57.751712	2002.726040	20.192807
57.779019	2016.251030	20.197824
58.364589	2020.635332	20.202842
58.401733	2039.345855	20.207859
58.297224	2033.211462	20.212877
58.502958	2039.141376	20.217895
58.202848	2041.751806	20.222912
58.437821	2035.905306	20.227930
58.425873	2040.669657	20.232947
58.342500	2038.543681	20.237965
58.577669	2042.923013	20.242983
58.534984	2043.558485	20.248000
58.804104	2030.297472	20.253018
58.591400	2039.501479	20.258035
58.735322	2031.947175	20.263053
58.567895	2034.408860	20.268071
58.537158	2030.972167	20.273088
59.104310	2036.163481	20.278106
58.776425	2050.562294	20.283123
58.970087	2059.798244	20.288141
59.470505	2057.048425	20.293159
59.182829	2057.398074	20.298176
59.252456	2044.111024	20.303194
59.266172	2060.691929	20.308211
59.273671	2053.210204	20.313229
59.217871	2045.976372	20.318247
59.342426	2051.503973	20.323264
59.687160	2043.893186	20.328282
59.657600	2045.687539	20.333299
59.662156	2046.810478	20.338317
59.855556	2048.791151	20.343335
59.956192	2062.180808	20.348352
59.565358	2038.666565	20.353370
59.830073	2044.519392	20.358387
59.425609	2056.325307	20.363405
60.334172	2064.311757	20.368423
60.094074	2080.579580	20.373440
60.451257	2069.096527	20.378458
60.103064	2075.996937	20.383475
60.231981	2087.671254	20.388493
60.129696	2072.424789	20.393511
60.369340	2075.448626	20.398528
60.500360	2064.166413	20.403546
60.680540	2071.830542	20.408563
60.514207	2078.052398	20.413581
60.326466	2065.693402	20.418599
60.038216	2068.504634	20.423616
60.412506	2072.872751	20.428634
60.409977	2091.746604	20.433651
60.802623	2101.148457	20.438669
60.896473	2096.121388	20.443687
60.778676	2102.145447	20.448704
61.267683	2099.794373	20.453722
61.401985	2089.918334	20.458739
61.355960	2089.873632	20.463757
61.399940	2093.444845	20.468775
60.991059	2082.601236	20.473792
61.414543	2091.197953	20.478810
61.335907	2093.052408	20.483827
61.382842	2095.654206	20.488845
61.591011	2092.479133	20.493863
61.361051	2102.314005	20.498880
61.594973	2108.269201	20.503898
61.584584	2124.703768	20.508915
61.322769	2122.852609	20.513933
61.589694	2118.026018	20.518951
61.691275	2127.116619	20.523968
61.839583	2118.022127	20.528986
61.781726	2122.511419	20.534003
61.737005	2137.074063	20.539021
62.019902	2141.529382	20.544039
62.055056	2152.733429	20.549056
62.411496	2152.267353	20.554074
62.441803	2154.553399	20.559091
62.245933	2161.202240	20.564109
62.608982	2138.286276	20.569127
62.414697	2146.679001	20.574144
62.653063	2144.311151	20.579162
62.624379	2147.647943	20.584179
62.537836	2144.261411	20.589197
63.080546	2135.167357	20.594215
63.019768	2147.590474	20.599232
63.146498	2132.925737	20.604250
62.866982	2146.731177	20.609267
62.842747	2142.370123	20.614285
63.104892	2139.368787	20.619303
63.121153	2145.398227	20.624320
63.143473	2151.813688	20.629338
63.137833	2161.370108	20.634355
63.002019	2164.716374	20.639373
63.467236	2171.632546	20.644391
63.249033	2177.679165	20.649408
63.576887	2173.973218	20.654426
63.287524	2176.548424	20.659443
63.222799	2174.224453	20.664461
63.480557	2167.029596	20.669479
63.333944	2169.517778	20.674496
63.336144	2182.820684	20.679514
63.805726	2188.546334	20.684531
63.717202	2194.220688	20.689549
63.613284	2194.837957	20.694567
63.722775	2204.062338	20.699584
63.890998	2204.337293	20.704602
64.094270	2204.122962	20.709619
64.030950	2218.165514	20.714637
64.319784	2226.386949	20.719655
64.426306	2227.674521	20.724672
64.431316	2232.893228	20.729690
64.460077	2221.577831	20.734707
64.385474	2224.334424	20.739725
64.704600	2224.288319	20.744743
64.288742	2222.727624	20.749760
64.460708	2219.245122	20.754778
64.636310	2234.490304	20.759795
64.585219	2253.600355	20.764813
64.991610	2246.654878	20.769831
64.999548	2244.249965	20.774848
65.033447	2245.876348	20.779866
65.426107	2249.852483	20.784883
65.366273	2244.261812	20.789901
65.565606	2233.755992	20.794919
65.288987	2228.497295	20.799936
65.465063	2236.965760	20.804954
65.717647	2235.383368	20.809971
65.106978	2248.689770	20.814989
65.462119	2236.489186	20.820007
65.271105	2248.850479	20.825024
65.535684	2257.472419	20.830042
65.698340	2260.764168	20.835059
65.673698	2271.369909	20.840077
66.069962	2271.801210	20.845095
66.058039	2268.554665	20.850112
66.277066	2259.142464	20.855130
66.156259	2270.360213	20.860147
66.010754	2271.165481	20.865165
65.899533	2264.031278	20.870183
66.175076	2267.842942	20.875200
65.976174	2263.135169	20.880218
66.469677	2284.607158	20.885235
66.507719	2295.902173	20.890253
66.595926	2289.225511	20.895271
66.505604	2297.621970	20.900288
66.825969	2295.066103	20.905306
67.059223	2283.232530	20.910323
66.884203	2288.896042	20.915341
67.045927	2282.441079	20.920359
67.137396	2289.318001	20.925376
66.585808	2286.124189	20.930394
66.906894	2279.927106	20.935411
66.984976	2292.417901	20.940429
67.471559	2296.317077	20.945447
67.611012	2320.737627	20.950464
67.506279	2311.425065	20.955482
67.570860	2310.571856	20.960499
67.417005	2317.010648	20.965517
67.370105	2310.636280	20.970535
67.609408	2319.932548	20.975552
67.565791	2322.934434	20.980570
67.853997	2312.984344	20.985587
67.553598	2326.212273	20.990605
67.722086	2316.205622	20.995623
67.598787	2315.889842	21.000640
67.268132	2317.561237	21.005658
67.742516	2332.928707	21.010675
67.694129	2346.027914	21.015693
67.962438	2341.352607	21.020711
68.404450	2341.356632	21.025728
67.740043	2345.823575	21.030746
68.533670	2362.840264	21.035763
68.463634	2374.939095	21.040781
68.673660	2367.050834	21.045799
68.736406	2377.906758	21.050816
69.014165	2376.134742	21.055834
69.003720	2361.720860	21.060851
68.679843	2373.846363	21.065869
68.696594	2373.075484	21.070887
68.746797	2360.523699	21.075904
69.005806	2370.259668	21.080922
69.219179	2366.230882	21.085939
69.144152	2379.193970	21.090957
69.093759	2371.413788	21.095975
69.409477	2367.617281	21.100992
69.069160	2376.905610	21.106010
69.356021	2376.331357	21.111027
69.283704	2401.133569	21.116045
69.535849	2397.991707	21.121063
69.519411	2399.034679	21.126080
69.549093	2406.415609	21.131098
69.844570	2396.295750	21.136115
69.571218	2399.469947	21.141133
69.943919	2388.102600	21.146151
70.017547	2403.199469	21.151168
70.244118	2419.673857	21.156186
70.517724	2425.793087	21.161203
70.134186	2430.090708	21.166221
70.282897	2428.687709	21.171239
70.504767	2421.353394	21.176256
70.273499	2427.092020	21.181274
70.436650	2421.030878	21.186291
70.418757	2421.408704	21.191309
70.468775	2419.661791	21.196327
70.724455	2426.154875	21.201344
70.578868	2428.353542	21.206362
70.495292	2419.509484	21.211379
70.608033	2425.092721	21.216397
70.924762	2435.073913	21.221415
70.903998	2437.889743	21.226432
70.850112	2444.967582	21.231450
70.864697	2435.998595	21.236467
70.989298	2452.632035	21.241485
71.001508	2458.421702	21.246503
71.563613	2467.496887	21.251520
71.517353	2471.632371	21.256538
71.650180	2463.046175	21.261555
71.445808	2464.384061	21.266573
71.787523	2458.833527	21.271591
71.629752	2464.504482	21.276608
71.431583	2469.200186	21.281626
71.916978	2454.509229	21.286643
71.700245	2460.225774	21.291661
72.293148	2485.463284	21.296679
72.248370	2494.049169	21.301696
72.259715	2497.004584	21.306714
72.369912	2488.266601	21.311731
72.278811	2483.806674	21.316749
72.346644	2488.233131	21.321767
72.442019	2482.500135	21.326784
72.285686	2486.948352	21.331802
72.618948	2482.407927	21.336819
72.479701	2482.014464	21.341837
72.265939	2480.359253	21.346855
72.803753	2494.992326	21.351872
72.433533	2512.905463	21.356890
72.729205	2516.211466	21.361907
72.603610	2513.629790	21.366925
73.044904	2516.973104	21.371943
72.933107	2511.980344	21.376960
72.752771	2522.819132	21.381978
73.480449	2531.050751	21.386995
73.458524	2542.320832	21.392013
73.535284	2526.844265	21.397031
73.767451	2530.702943	21.402048
73.707729	2536.418718	21.407066
73.676246	2536.659419	21.412083
73.943185	2534.392297	21.417101
73.871584	2525.897398	21.422119
74.331319	2522.669956	21.427136
74.537622	2537.336303	21.432154
74.771675	2531.324014	21.437171
74.513563	2523.831312	21.442189
74.415938	2516.180145	21.447207
74.390906	2500.585805	21.452224
74.141813	2502.710277	21.457242
74.321493	2522.314762	21.462259
74.338548	2523.635284	21.467277
74.075844	2529.160635	21.472295
74.338939	2527.616240	21.477312
74.300878	2539.737072	21.482330
74.609994	2545.319730	21.487347
74.844164	2554.117352	21.492365
74.927901	2562.193779	21.497383
75.267176	2563.858223	21.502400
74.897190	2567.059082	21.507418
75.286874	2559.315793	21.512435
75.454308	2554.744925	21.517453
75.534514	2558.283868	21.522471
75.666740	2553.165254	21.527488
75.335255	2556.387297	21.532506
75.877064	2550.633513	21.537523
75.757389	2551.515230	21.542541
75.535177	2549.261375	21.547559
75.892878	2556.495541	21.552576
75.861519	2561.012069	21.557594
75.543026	2564.002815	21.562611
75.763626	2566.255840	21.567629
75.788515	2584.089466	21.572647
76.094028	2586.205987	21.577664
75.876886	2588.707093	21.582682
76.224593	2583.659098	21.587699
76.100393	2587.888230	21.592717
76.107451	2619.662728	21.597735
76.195672	2610.102672	21.602752
76.122003	2611.755565	21.607770
76.277103	2611.523220	21.612787
76.619072	2621.547994	21.617805
76.757568	2633.717624	21.622823
76.941229	2629.116881	21.627840
76.827252	2645.920352	21.632858
77.374738	2641.457805	21.637875
77.589427	2633.219009	21.642893
77.138630	2639.262975	21.647911
77.236984	2626.468342	21.652928
77.157862	2640.528065	21.657946
77.434028	2639.277972	21.662963
77.463700	2628.179466	21.667981
77.327057	2638.185456	21.672999
77.441168	2625.116151	21.678016
77.479745	2657.608389	21.683034
77.800157	2659.478735	21.688051
77.997947	2656.435986	21.693069
77.998922	2666.173916	21.698087
78.015345	2662.711951	21.703104
78.279163	2661.676514	21.708122
78.132044	2663.636081	21.713139
78.184295	2663.931035	21.718157
78.021681	2674.698486	21.723175
78.213639	2662.951390	21.728192
78.342475	2669.987265	21.733210
78.524887	2686.097569	21.738227
78.604761	2685.678058	21.743245
78.663378	2690.041134	21.748263
78.660109	2682.610893	21.753280
78.894760	2688.776050	21.758298
78.801606	2685.507825	21.763315
78.891146	2684.155154	21.768333
78.733744	2686.387312	21.773351
78.834483	2708.887583	21.778368
79.095164	2711.330858	21.783386
79.274842	2712.132704	21.788403
79.563027	2703.838786	21.793421
79.482812	2707.754348	21.798439
79.758179	2708.357267	21.803456
79.817787	2708.987247	21.808474
79.748705	2705.281537	21.813491
79.614342	2705.451866	21.818509
79.781067	2734.171211	21.823527
79.806835	2737.599120	21.828544
80.162964	2741.488118	21.833562
80.487988	2735.420922	21.838579
80.659305	2734.542931	21.843597
80.349069	2735.213279	21.848615
80.922167	2730.870098	21.853632
80.769946	2736.411484	21.858650
80.653623	2730.294913	21.863667
80.726146	2723.474590	21.868685
80.611027	2732.756159	21.873703
80.955059	2728.824948	21.878720
80.798560	2726.496796	21.883738
81.076230	2717.554172	21.888755
80.847236	2717.912228	21.893773
80.720528	2726.892936	21.898791
81.289224	2732.410241	21.903808
81.056474	2742.285743	21.908826
81.018455	2753.063723	21.913843
81.243503	2749.865644	21.918861
81.094885	2751.541592	21.923879
81.554303	2750.737956	21.928896
81.401981	2778.116798	21.933914
81.726066	2775.390935	21.938931
82.204684	2775.158965	21.943949
81.850571	2780.436920	21.948967
82.126406	2776.191374	21.953984
81.963316	2780.020668	21.959002
82.002583	2778.621978	21.964019
82.423402	2782.729820	21.969037
82.002057	2783.674491	21.974055
82.405425	2789.666468	21.979072
82.444947	2804.145309	21.984090
82.446447	2802.247320	21.989107
82.904368	2805.949783	21.994125
82.642209	2805.845974	21.999143
82.777192	2812.822625	22.004160
82.896335	2797.875821	22.009178
82.658757	2811.872163	22.014195
83.222348	2800.578039	22.019213
83.094614	2799.311730	22.024231
82.976117	2804.458944	22.029248
82.891570	2811.108527	22.034266
83.010562	2822.859849	22.039283
83.093696	2818.779670	22.044301
83.080584	2823.074338	22.049319
83.233945	2833.140714	22.054336
83.353135	2853.521439	22.059354
83.617941	2858.655605	22.064371
83.660829	2854.004477	22.069389
83.624541	2854.506234	22.074407
84.002677	2851.852912	22.079424
84.394788	2864.382732	22.084442
84.301506	2870.551859	22.089459
84.315995	2877.356741	22.094477
84.305876	2886.684014	22.099495
84.605433	2876.161170	22.104512
84.591965	2867.600549	22.109530
84.604435	2877.464672	22.114547
85.182477	2870.754303	22.119565
85.020698	2873.867991	22.124583
85.217059	2863.752824	22.129600
85.175641	2876.492632	22.134618
84.952722	2868.274194	22.139635
84.993692	2863.978133	22.144653
84.906079	2868.574148	22.149671
85.227402	2863.026455	22.154688
85.313542	2880.543955	22.159706
85.259020	2897.828838	22.164723
85.675741	2899.547037	22.169741
85.792857	2899.792670	22.174759
85.818428	2906.389807	22.179776
85.665553	2901.434041	22.184794
85.804006	2904.432273	22.189811
85.888401	2897.487063	22.194829
85.715658	2907.962626	22.199847
85.693730	2925.615008	22.204864
86.162455	2924.123546	22.209882
85.942973	2927.918902	22.214899
86.133588	2918.538571	22.219917
86.134202	2939.667841	22.224935
86.636926	2953.001930	22.229952
86.734919	2953.838969	22.234970
86.536046	2965.315832	22.239987
86.540099	2957.634227	22.245005
86.912956	2963.946704	22.250023
86.768290	2955.799523	22.255040
87.098866	2959.836914	22.260058
87.187965	2976.701221	22.265075
87.517964	2977.469925	22.270093
87.418560	2984.300797	22.275111
87.949734	2982.599760	22.280128
87.824343	2978.415471	22.285146
88.020963	2985.135515	22.290163
88.486118	2964.188620	22.295181
87.973276	2963.095122	22.300199
87.863624	2975.886864	22.305216
88.050766	2966.668510	22.310234
87.881548	2968.611694	22.315251
88.033024	2974.524177	22.320269
87.742771	2967.860670	22.325287
88.065376	2967.076526	22.330304
88.580952	2981.676731	22.335322
88.383836	2999.417656	22.340339
88.648981	3000.221904	22.345357
88.825880	3005.250191	22.350375
88.810827	2998.133984	22.355392
89.083327	2999.277202	22.360410
88.794833	3005.572018	22.365427
89.164720	2999.170098	22.370445
88.913480	3006.108410	22.375463
88.650513	3005.618478	22.380480
88.931911	3006.994496	22.385498
89.295227	3025.856549	22.390515
89.220204	3033.061393	22.395533
89.085958	3028.258028	22.400551
88.792132	3034.022588	22.405568
89.266523	3043.414631	22.410586
89.513375	3062.690142	22.415603
89.919278	3052.748841	22.420621
89.881198	3059.791267	22.425639
89.801404	3054.768622	22.430656
90.154485	3067.773222	22.435674
89.940176	3081.901004	22.440691
90.257477	3080.228674	22.445709
90.306392	3086.859034	22.450727
90.253015	3084.228294	22.455744
90.678177	3075.726051	22.460762
90.688661	3081.902493	22.465779
91.054821	3089.763914	22.470797
91.131160	3087.056574	22.475815
91.326331	3094.063547	22.480832
91.293949	3092.949158	22.485850
91.118059	3104.199069	22.490867
91.151705	3107.174925	22.495885
91.233719	3101.288781	22.500903
91.424051	3106.539702	22.505920
91.535303	3096.220345	22.510938
91.137402	3108.015332	22.515955
91.658992	3104.588145	22.520973
91.412452	3120.664003	22.525991
91.233671	3128.480221	22.531008
91.784700	3120.794204	22.536026
91.762545	3140.543525	22.541043
91.862309	3148.748324	22.546061
92.125892	3159.104959	22.551079
92.344312	3164.216195	22.556096
92.340116	3159.307391	22.561114
92.319318	3163.444748	22.566131
92.570122	3171.318616	22.571149
92.777972	3176.498936	22.576167
92.929897	3190.190551	22.581184
93.259500	3194.287227	22.586202
93.318988	3192.871765	22.591219
93.207698	3185.814717	22.596237
93.435366	3189.355376	22.601255
93.145834	3189.078911	22.606272
93.537606	3186.050011	22.611290
93.178625	3182.402816	22.616307
93.510288	3179.710673	22.621325
93.487125	3185.358421	22.626343
93.507819	3193.766905	22.631360
94.091345	3195.060238	22.636378
93.963463	3212.821441	22.641395
93.980336	3208.679684	22.646413
94.134509	3207.325324	22.651431
94.057598	3215.473573	22.656448
94.398674	3209.046021	22.661466
94.189264	3202.826555	22.666483
94.272314	3204.144476	22.671501
94.671844	3218.547954	22.676519
94.517023	3232.315199	22.681536
94.846767	3220.892546	22.686554
94.610573	3225.273083	22.691571
94.900017	3233.450460	22.696589
94.951857	3227.198754	22.701607
94.890706	3235.228251	22.706624
95.056757	3223.851992	22.711642
95.092271	3239.944665	22.716659
95.301368	3256.797282	22.721677
95.514633	3254.895282	22.726695
95.575005	3256.926880	22.731712
95.529306	3257.012054	22.736730
95.607021	3255.730985	22.741747
95.541338	3258.984367	22.746765
95.769494	3266.256064	22.751783
95.539108	3276.027955	22.756800
95.742130	3275.135236	22.761818
95.909039	3291.323150	22.766835
96.035744	3303.363745	22.771853
96.266144	3308.034022	22.776871
96.364807	3314.562138	22.781888
96.628997	3309.817141	22.786906
96.657516	3321.518456	22.791923
96.694924	3311.300563	22.796941
96.781458	3313.401467	22.801959
96.859589	3336.686786	22.806976
97.285065	3329.966834	22.811994
97.461346	3333.234114	22.817011
97.443132	3337.603398	22.822029
97.622109	3320.837722	22.827047
97.346514	3334.678208	22.832064
97.760818	3332.608648	22.837082
97.537904	3329.301134	22.842099
97.670528	3338.594019	22.847117
97.754101	3344.704521	22.852135
97.969577	3357.477393	22.857152
97.837869	3358.386741	22.862170
97.865690	3359.026735	22.867187
97.865243	3360.078542	22.872205
98.341740	3371.582089	22.877223
98.211586	3387.040064	22.882240
98.371549	3381.066492	22.887258
98.613709	3378.926597	22.892275
98.823959	3380.802673	22.897293
99.128932	3393.688331	22.902311
98.816506	3409.266673	22.907328
99.065515	3406.639364	22.912346
99.014804	3411.445595	22.917363
99.278262	3405.583240	22.922381
99.705740	3401.740421	22.927399
99.473693	3405.888011	22.932416
99.736641	3403.670253	22.937434
99.812217	3412.329641	22.942451
99.759089	3410.911542	22.947469
100.204246	3414.570593	22.952487
100.174986	3433.443013	22.957504
100.428010	3431.113888	22.962522
100.536823	3433.588723	22.967539
100.306103	3436.839541	22.972557
100.454094	3433.059525	22.977575
100.316704	3425.351889	22.982592
100.504718	3435.565690	22.987610
100.235798	3432.745749	22.992627
100.480215	3432.293464	22.997645
101.320135	3445.750517	23.002663
101.124794	3456.794820	23.007680
101.029529	3460.850873	23.012698
101.327000	3466.292076	23.017715
101.079624	3461.287595	23.022733
101.473986	3451.811001	23.027751
101.217319	3466.466675	23.032768
101.197751	3466.666042	23.037786
101.489354	3467.442704	23.042803
101.116292	3484.944773	23.047821
101.523964	3491.502126	23.052839
101.644069	3487.555040	23.057856
101.899807	3486.856756	23.062874
102.059041	3501.128606	23.067891
102.101220	3520.044033	23.072909
102.406531	3509.144178	23.077927
102.460036	3516.161015	23.082944
102.576599	3517.102898	23.087962
102.775316	3507.277513	23.092979
102.802556	3512.306724	23.097997
103.127938	3508.635133	23.103015
102.824780	3518.293223	23.108032
102.962337	3517.728298	23.113050
103.348400	3536.619492	23.118067
103.304525	3541.433687	23.123085
103.563849	3539.453547	23.128103
103.366554	3548.349155	23.133120
103.344364	3542.316299	23.138138
103.549844	3541.380634	23.143155
103.272717	3544.450158	23.148173
103.638584	3555.987908	23.153191
103.351699	3566.983264	23.158208
103.675449	3561.480207	23.163226
103.970739	3585.861974	23.168243
104.150795	3601.282188	23.173261
104.352028	3597.533874	23.178279
104.465921	3607.306852	23.183296
104.392726	3603.279522	23.188314
104.969673	3612.844720	23.193331
104.812946	3629.964238	23.198349
105.118900	3622.084272	23.203367
105.116166	3625.643490	23.208384
105.086354	3623.661597	23.213402
105.221772	3626.178914	23.218419
105.392504	3615.698955	23.223437
105.359414	3620.438545	23.228455
105.192432	3624.867583	23.233472
105.388887	3635.696733	23.238490
105.547962	3643.038712	23.243507
105.364238	3650.187417	23.248525
105.919863	3651.396424	23.253543
106.011368	3670.054621	23.258560
106.136487	3674.622345	23.263578
106.439365	3671.566333	23.268595
106.570291	3678.500337	23.273613
106.814027	3664.421173	23.278631
106.701280	3668.328185	23.283648
107.109157	3660.880597	23.288666
107.349560	3656.159910	23.293683
107.192134	3666.202284	23.298701
107.203680	3662.955894	23.303719
107.068997	3661.345737	23.308736
107.301129	3678.087106	23.313754
107.519457	3683.049297	23.318771
107.505859	3685.367250	23.323789
107.728852	3682.145699	23.328807
107.450577	3687.263742	23.333824
107.525806	3685.769242	23.338842
107.973386	3682.120298	23.343859
107.900972	3719.010469	23.348877
108.273475	3717.639212	23.353895
107.961232	3721.432003	23.358912
108.023372	3721.270160	23.363930
108.280633	3703.926078	23.368947
108.161806	3722.147837	23.373965
108.576542	3729.032513	23.378983
108.474579	3740.042655	23.384000
108.545541	3743.418809	23.389018
108.661724	3733.938883	23.394035
108.821812	3756.177259	23.399053
108.881218	3764.624135	23.404071
108.891420	3781.118460	23.409088
108.819977	3778.260248	23.414106
109.245583	3787.656883	23.419123
109.276167	3810.268400	23.424141
109.750451	3812.576473	23.429159
109.687496	3807.702394	23.434176
109.530580	3804.209418	23.439194
109.995033	3830.983584	23.444211
110.187915	3832.562155	23.449229
110.460818	3833.149386	23.454247
110.630086	3837.016049	23.459264
110.406939	3837.064454	23.464282
111.029060	3830.526725	23.469299
111.264675	3832.112397	23.474317
111.103995	3833.203758	23.479335
111.249684	3828.141170	23.484352
111.128585	3831.460939	23.489370
111.158788	3824.508541	23.494387
111.232571	3825.048807	23.499405
111.339548	3829.039970	23.504423
111.532902	3843.303728	23.509440
111.190127	3847.735945	23.514458
111.497980	3851.668263	23.519475
111.434446	3859.312986	23.524493
111.511665	3868.362173	23.529511
111.739951	3869.251324	23.534528
111.980688	3880.779319	23.539546
112.012005	3879.476349	23.544563
111.899700	3891.160060	23.549581
112.623650	3906.737021	23.554599
113.110826	3900.531887	23.559616
112.974101	3910.141006	23.564634
113.052188	3905.436880	23.569651
112.877413	3910.337436	23.574669
112.741107	3905.438064	23.579687
112.986575	3907.407995	23.584704
113.165814	3931.418119	23.589722
113.541572	3926.407974	23.594739
113.434880	3929.426909	23.599757
113.465700	3930.470821	23.604775
113.831409	3926.015178	23.609792
113.712411	3937.312179	23.614810
114.291636	3941.083038	23.619827
114.263642	3945.435604	23.624845
114.151221	3952.350561	23.629863
114.389202	3952.271038	23.634880
114.479621	3953.762633	23.639898
114.582523	3956.755536	23.644915
114.816798	3951.606578	23.649933
114.898910	3949.895921	23.654951
114.790237	3953.842099	23.659968
114.799668	3977.086587	23.664986
114.884491	3971.587506	23.670003
115.039728	3987.629626	23.675021
114.739845	3982.405289	23.680039
115.338968	4005.474225	23.685056
115.275911	4012.235344	23.690074
115.679326	4009.825717	23.695091
115.583355	4022.434916	23.700109
115.581721	4023.529884	23.705127
116.021612	4028.694123	23.710144
115.985042	4036.151762	23.715162
116.294891	4035.318493	23.720179
116.245987	4051.575607	23.725197
116.072117	4047.923546	23.730215
116.674018	4042.868049	23.735232
117.044412	4052.377546	23.740250
117.108788	4057.444885	23.745267
117.112986	4051.936286	23.750285
117.192151	4045.919925	23.755303
117.306676	4045.500156	23.760320
117.011657	4049.327579	23.765338
117.244053	4054.527755	23.770355
117.082996	4051.715436	23.775373
117.263748	4071.207498	23.780391
117.643731	4071.452551	23.785408
117.585347	4086.282700	23.790426
117.672432	4080.228789	23.795443
117.840314	4092.426586	23.800461
117.824946	4102.528409	23.805479
118.196542	4106.391962	23.810496
117.900402	4119.094231	23.815514
118.511511	4126.571475	23.820531
118.156703	4137.891123	23.825549
118.641088	4141.839965	23.830567
118.395548	4148.209238	23.835584
118.389376	4155.541409	23.840602
118.921841	4160.008366	23.845619
119.187848	4168.035759	23.850637
119.178154	4161.724566	23.855655
119.781936	4188.604645	23.860672
119.882013	4188.227428	23.865690
120.351970	4185.016077	23.870707
120.219691	4189.316674	23.875725
120.106930	4197.536733	23.880743
120.259111	4197.005196	23.885760
120.178468	4189.257468	23.890778
120.696039	4184.083584	23.895795
120.546725	4186.600092	23.900813
120.844541	4184.394567	23.905831
120.830010	4180.628680	23.910848
120.958575	4194.824731	23.915866
121.151686	4199.744798	23.920883
121.143618	4211.385895	23.925901
121.141365	4220.755581	23.930919
121.547719	4208.171309	23.935936
121.527476	4206.360227	23.940954
121.578426	4199.555435	23.945971
121.544378	4208.134183	23.950989
121.762984	4220.838728	23.956007
121.879958	4228.515961	23.961024
122.011127	4238.449493	23.966042
121.926523	4241.807408	23.971059
121.867034	4246.187323	23.976077
122.064048	4250.778358	23.981095
122.248542	4257.909691	23.986112
122.234194	4268.698970	23.991130
122.379714	4280.654118	23.996147
122.683942	4287.080485	24.001165
122.762123	4289.416802	24.006183
123.200133	4288.847391	24.011200
123.272623	4306.347090	24.016218
123.518989	4315.752851	24.021235
123.775276	4322.567550	24.026253
123.835025	4317.742694	24.031271
123.852978	4314.043063	24.036288
124.131413	4315.212964	24.041306
123.557671	4314.197565	24.046323
124.064810	4320.537587	24.051341
124.272816	4340.535009	24.056359
124.417061	4341.186877	24.061376
124.480922	4344.487158	24.066394
124.855086	4343.207718	24.071411
125.010286	4342.892250	24.076429
124.549248	4346.714154	24.081447
125.002184	4345.227938	24.086464
124.937616	4342.789423	24.091482
124.872029	4353.376971	24.096499
125.207323	4361.069314	24.101517
124.885565	4383.538380	24.106535
125.377318	4376.831428	24.111552
125.661763	4398.407101	24.116570
125.777251	4398.450238	24.121587
126.140293	4395.045486	24.126605
126.181672	4411.037586	24.131623
126.464253	4396.203172	24.136640
126.478802	4399.733715	24.141658
126.197160	4397.782391	24.146675
126.550899	4413.898402	24.151693
126.462651	4428.036842	24.156711
126.711112	4423.588659	24.161728
126.654989	4423.345977	24.166746
126.769181	4444.334041	24.171763
127.006247	4454.280892	24.176781
127.015523	4453.679289	24.181799
127.407111	4451.367636	24.186816
127.276297	4460.776862	24.191834
127.659867	4476.038238	24.196851
127.930937	4474.182047	24.201869
127.526822	4478.674210	24.206887
127.805538	4487.721897	24.211904
127.933316	4498.016064	24.216922
127.963633	4501.102206	24.221939
128.399761	4502.607498	24.226957
128.431696	4527.327300	24.231975
128.839812	4526.296603	24.236992
128.743187	4526.489052	24.242010
128.800071	4528.559589	24.247027
129.187388	4535.597616	24.252045
128.918029	4556.021653	24.257063
129.477689	4547.089586	24.262080
129.268598	4553.077327	24.267098
129.617713	4572.221606	24.272115
129.825027	4574.776790	24.277133
129.695313	4590.331956	24.282151
129.981850	4583.389550	24.287168
130.453686	4582.159289	24.292186
130.458045	4577.682170	24.297203
130.493151	4599.353740	24.302221
130.426068	4608.537502	24.307239
130.520019	4606.923259	24.312256
130.579683	4613.236677	24.317274
130.496719	4624.949546	24.322291
130.894148	4637.088500	24.327309
130.820141	4627.413889	24.332327
131.231674	4636.048260	24.337344
131.665805	4656.063777	24.342362
132.033476	4664.964531	24.347379
132.054377	4658.074734	24.352397
132.161118	4672.015725	24.357415
132.166203	4660.697760	24.362432
132.512600	4653.024014	24.367450
132.536926	4666.625033	24.372467
132.676276	4655.403764	24.377485
132.597566	4659.393986	24.382503
132.574621	4662.790610	24.387520
132.807295	4680.043691	24.392538
132.731896	4687.628564	24.397555
132.958269	4683.325725	24.402573
132.935117	4689.906478	24.407591
133.190650	4687.200699	24.412608
133.204339	4707.348105	24.417626
133.319050	4715.274819	24.422643
133.764762	4717.751968	24.427661
133.660890	4723.178938	24.432679
133.678210	4712.781140	24.437696
134.093407	4731.826468	24.442714
133.906996	4748.105491	24.447731
134.025177	4759.707978	24.452749
134.190495	4766.247323	24.457767
134.402094	4780.821575	24.462784
134.479893	4781.352940	24.467802
134.481683	4792.094227	24.472819
135.136207	4789.394044	24.477837
135.015672	4803.796487	24.482855
135.099161	4814.530565	24.487872
135.261662	4803.644797	24.492890
135.286006	4817.538128	24.497907
135.552535	4821.305059	24.502925
135.724379	4837.737505	24.507943
135.580547	4837.351825	24.512960
135.892757	4844.163795	24.517978
135.959797	4867.537098	24.522995
136.268101	4865.593579	24.528013
136.253411	4868.126498	24.533031
136.413909	4879.099891	24.538048
136.754614	4886.605732	24.543066
136.994420	4885.564288	24.548083
137.185145	4884.078907	24.553101
137.247192	4898.270855	24.558119
137.738394	4903.618272	24.563136
137.713022	4907.342191	24.568154
137.740153	4905.368823	24.573171
138.272980	4906.191867	24.578189
137.934192	4901.948669	24.583207
138.202114	4904.409603	24.588224
138.552990	4901.613185	24.593242
138.581703	4905.378555	24.598259
138.719394	4913.108610	24.603277
138.648564	4936.737173	24.608295
138.580989	4938.366855	24.613312
138.877640	4928.882716	24.618330
138.767130	4937.663536	24.623347
139.017274	4945.527779	24.628365
139.045448	4957.766705	24.633383
139.318821	4966.644652	24.638400
139.595663	4973.778349	24.643418
139.673426	4973.729288	24.648435
139.784264	4988.170776	24.653453
139.665852	4990.099492	24.658471
139.920959	4997.465194	24.663488
139.958180	4998.230105	24.668506
139.844316	5017.035738	24.673523
140.346539	5012.237438	24.678541
140.737061	5025.625352	24.683559
140.850683	5048.291059	24.688576
141.128819	5049.958027	24.693594
141.040803	5056.876515	24.698611
141.306402	5044.518864	24.703629
141.489261	5057.671047	24.708647
141.423387	5072.992449	24.713664
141.824612	5078.781688	24.718682
141.664785	5084.917413	24.723699
141.879970	5081.950472	24.728717
142.077749	5092.117665	24.733735
142.269585	5103.951574	24.738752
142.395620	5101.749949	24.743770
142.213079	5109.599273	24.748787
142.371941	5109.981766	24.753805
142.780723	5122.828038	24.758823
142.796695	5132.659133	24.763840
142.788817	5136.036038	24.768858
142.748919	5146.136292	24.773875
143.169682	5137.003219	24.778893
143.051261	5155.531756	24.783911
143.398921	5165.919121	24.788928
143.424881	5172.102092	24.793946
143.611748	5191.466945	24.798963
144.155345	5187.964402	24.803981
143.912137	5200.953331	24.808999
144.105193	5200.095238	24.814016
144.588658	5206.350546	24.819034
144.451021	5222.249457	24.824051
144.796170	5231.340132	24.829069
144.939060	5222.905919	24.834087
144.911293	5224.195892	24.839104
145.311191	5242.855307	24.844122
145.390285	5251.323745	24.849139
145.706246	5244.981832	24.854157
145.857030	5239.423347	24.859175
145.806357	5247.821119	24.864192
146.037033	5245.957351	24.869210
145.702098	5258.025862	24.874227
146.109853	5270.047824	24.879245
146.300919	5275.240286	24.884263
146.478073	5273.594873	24.889280
146.750188	5284.398067	24.894298
146.764112	5295.739405	24.899315
146.865736	5293.361438	24.904333
147.268594	5301.002892	24.909351
147.252328	5308.953952	24.914368
147.456457	5323.227510	24.919386
147.428250	5332.042179	24.924403
147.645210	5334.852645	24.929421
147.805958	5326.642246	24.934439
148.034250	5348.174964	24.939456
147.792113	5354.428382	24.944474
147.902208	5357.721222	24.949491
148.343121	5367.208819	24.954509
148.357469	5384.127862	24.959527
148.555636	5375.374106	24.964544
148.862338	5373.978955	24.969562
148.706952	5402.248519	24.974579
149.208391	5410.005235	24.979597
149.815767	5412.308454	24.984615
149.204954	5411.173884	24.989632
149.806609	5419.113274	24.994650
149.824118	5436.986413	24.999667
149.882282	5435.374860	25.004685
150.165191	5438.287840	25.009703
150.118684	5446.434573	25.014720
150.408935	5460.716839	25.019738
150.325648	5461.737214	25.024755
150.461932	5462.840953	25.029773
150.937648	5477.993539	25.034791
151.087895	5487.293051	25.039808
151.341013	5485.255419	25.044826
151.595106	5486.688562	25.049843
151.569694	5488.236498	25.054861
151.589446	5492.341369	25.059879
151.377397	5492.721482	25.064896
151.768641	5509.044274	25.069914
151.862210	5516.321973	25.074931
152.118478	5514.301144	25.079949
152.067175	5532.583520	25.084967
152.400749	5553.813978	25.089984
152.681525	5550.712439	25.095002
152.613079	5562.107772	25.100019
152.677191	5559.941539	25.105037
152.990503	5564.653901	25.110055
153.134226	5583.361644	25.115072
153.420400	5568.574369	25.120090
153.620059	5579.264532	25.125107
153.431985	5585.108989	25.130125
153.469198	5590.198647	25.135143
153.582449	5603.550259	25.140160
153.802372	5605.871184	25.145178
154.198211	5630.715194	25.150195
154.172855	5628.828398	25.155213
154.343777	5637.754403	25.160231
154.387548	5658.591134	25.165248
154.902344	5662.885819	25.170266
154.929213	5670.247092	25.175283
154.955949	5666.484256	25.180301
155.431485	5683.364287	25.185319
155.716317	5688.323983	25.190336
155.653072	5691.836978	25.195354
156.027898	5688.702515	25.200371
155.839614	5692.468554	25.205389
156.239590	5710.573250	25.210407
156.274804	5714.863858	25.215424
156.445881	5721.005693	25.220442
156.794015	5728.485506	25.225459
156.748116	5737.781408	25.230477
157.020823	5747.075765	25.235495
157.170089	5762.019607	25.240512
157.547175	5754.029145	25.245530
157.652740	5758.453039	25.250547
157.628210	5760.896367	25.255565
157.885699	5778.096137	25.260583
157.729162	5786.880322	25.265600
158.079683	5784.525661	25.270618
158.149023	5781.140099	25.275635
158.424561	5796.996389	25.280653
158.309225	5793.927300	25.285671
158.514869	5801.300781	25.290688
158.890866	5800.070548	25.295706
159.108931	5814.629723	25.300723
159.323699	5820.465859	25.305741
159.415603	5821.977866	25.310759
158.853568	5833.190469	25.315776
158.945580	5839.963716	25.320794
159.349508	5854.644168	25.325811
159.573519	5871.681033	25.330829
160.017274	5891.588628	25.335847
160.382915	5898.396938	25.340864
160.235589	5902.794215	25.345882
160.526912	5919.627023	25.350899
160.926921	5913.292197	25.355917
161.135370	5910.517609	25.360935
161.011242	5912.948307	25.365952
161.426405	5930.875104	25.370970
161.671974	5939.024144	25.375987
161.652044	5935.613159	25.381005
161.997238	5926.185762	25.386023
161.797127	5941.800381	25.391040
162.120141	5945.718120	25.396058
162.156168	5954.999012	25.401075
162.136647	5966.604707	25.406093
162.561100	5954.984828	25.411111
162.759214	5980.476466	25.416128
162.455429	5991.083279	25.421146
162.839681	5990.282494	25.426163
162.853185	5994.922537	25.431181
162.999521	6003.146323	25.436199
163.183597	6026.934372	25.441216
163.265413	6029.058477	25.446234
163.459273	6036.748281	25.451251
163.666811	6053.547057	25.456269
164.096571	6046.973328	25.461287
164.172907	6064.420785	25.466304
164.550475	6072.794569	25.471322
164.756070	6085.042016	25.476339
164.880759	6084.267657	25.481357
164.887956	6079.638419	25.486375
164.923902	6093.193061	25.491392
165.276894	6105.781581	25.496410
165.297346	6117.445354	25.501427
165.321938	6115.495884	25.506445
165.919303	6119.177643	25.511463
165.812884	6132.422721	25.516480
166.349005	6140.674990	25.521498
166.368195	6137.339399	25.526515
166.392927	6136.774554	25.531533
166.697579	6157.838911	25.536551
166.831369	6171.196267	25.541568
167.082270	6157.717024	25.546586
167.057590	6165.012236	25.551603
166.968534	6180.506312	25.556621
167.159667	6187.068754	25.561639
167.444120	6200.131823	25.566656
167.529857	6209.559798	25.571674
167.658003	6221.418480	25.576691
167.889939	6235.878868	25.581709
168.189369	6239.651723	25.586727
168.316563	6258.218865	25.591744
168.760241	6250.678685	25.596762
168.692206	6256.336537	25.601779
168.983647	6277.800997	25.606797
169.538278	6276.052823	25.611815
169.477401	6279.002397	25.616832
169.722813	6273.526340	25.621850
170.004642	6268.395541	25.626867
169.820180	6289.321296	25.631885
169.984698	6289.628059	25.636903
170.153075	6307.382689	25.641920
170.203506	6295.640961	25.646938
170.535729	6310.678694	25.651955
170.264677	6321.127506	25.656973
170.601455	6329.104909	25.661991
170.542811	6338.721479	25.667008
170.733583	6354.293060	25.672026
171.225559	6365.321308	25.677044
171.462862	6390.004514	25.682061
172.113055	6389.460564	25.687079
171.836047	6393.453331	25.692096
171.612347	6395.969899	25.697114
172.124537	6396.956340	25.702132
171.960225	6416.862870	25.707149
172.723783	6418.937966	25.712167
172.413102	6431.032493	25.717184
172.554386	6445.167819	25.722202
173.184058	6454.663422	25.727220
173.089611	6478.638459	25.732237
173.722705	6474.016549	25.737255
173.267574	6481.130332	25.742272
173.531263	6489.453091	25.747290
173.855385	6506.564647	25.752308
173.813387	6509.944344	25.757325
174.309194	6507.364678	25.762343
174.248653	6520.332321	25.767360
174.436686	6531.125873	25.772378
174.679219	6528.747238	25.777396
174.595893	6537.309416	25.782413
175.017426	6545.157902	25.787431
175.089375	6560.804491	25.792448
174.929652	6563.065535	25.797466
175.544907	6580.217979	25.802484
175.830852	6593.115720	25.807501
175.955331	6591.077193	25.812519
176.155343	6598.242464	25.817536
176.548670	6618.520858	25.822554
176.721084	6618.363181	25.827572
176.806359	6622.115658	25.832589
177.006169	6615.389941	25.837607
177.060671	6621.574268	25.842624
176.925112	6645.136544	25.847642
177.469120	6641.654891	25.852660
177.288505	6652.750577	25.857677
177.595466	6659.179831	25.862695
177.942620	6672.837830	25.867712
177.873752	6677.200277	25.872730
178.443434	6678.538755	25.877748
178.382685	6695.490535	25.882765
178.487361	6702.237638	25.887783
178.945475	6709.880874	25.892800
178.944864	6713.094656	25.897818
179.147094	6720.894467	25.902836
179.204911	6732.588740	25.907853
179.654620	6733.822633	25.912871
179.767505	6744.727229	25.917888
179.804897	6759.606256	25.922906
180.088662	6756.991552	25.927924
179.881776	6766.086286	25.932941
180.049636	6791.820537	25.937959
180.230080	6790.190968	25.942976
180.442917	6813.513080	25.947994
180.901761	6816.547639	25.953012
180.790814	6828.024169	25.958029
181.396145	6838.069097	25.963047
181.629645	6848.114936	25.968064
181.364383	6850.243047	25.973082
181.788245	6866.557120	25.978100
181.924032	6882.491983	25.983117
182.219783	6882.304435	25.988135
182.506433	6904.683443	25.993152
182.372298	6910.286306	25.998170
182.986022	6906.665454	26.003188
183.197797	6924.263935	26.008205
183.549350	6926.806656	26.013223
183.882842	6932.465230	26.018240
183.444183	6938.193343	26.023258
183.863854	6932.304620	26.028276
183.837717	6943.081922	26.033293
183.895058	6952.147986	26.038311
183.959197	6958.733348	26.043328
184.176325	6977.157266	26.048346
184.836050	6987.135786	26.053364
184.845947	6993.894765	26.058381
184.816869	6998.916295	26.063399
184.928862	7015.804375	26.068416
185.249769	7022.984484	26.073434
185.695100	7028.004680	26.078452
185.356145	7051.949380	26.083469
185.639294	7055.228894	26.088487
185.785990	7065.809106	26.093504
185.862939	7096.067548	26.098522
186.286876	7083.244943	26.103540
186.553024	7104.627279	26.108557
186.495858	7119.337191	26.113575
186.880889	7117.279883	26.118592
186.950615	7135.026565	26.123610
187.165698	7144.748755	26.128628
187.251900	7139.765853	26.133645
187.474232	7158.289942	26.138663
188.056242	7171.157260	26.143680
188.101731	7179.196706	26.148698
188.450920	7174.647591	26.153716
188.602699	7196.838239	26.158733
188.728364	7192.378109	26.163751
189.013489	7194.426968	26.168768
188.760450	7194.610680	26.173786
189.522945	7212.296328	26.178804
189.410258	7229.273029	26.183821
189.568930	7224.266288	26.188839
189.815542	7234.569349	26.193856
189.730587	7257.234860	26.198874
190.075907	7260.148879	26.203892
190.027247	7269.468978	26.208909
190.124420	7281.851877	26.213927
190.510675	7288.164287	26.218944
190.563158	7319.913568	26.223962
191.220994	7323.380020	26.228980
191.058438	7332.622912	26.233997
191.351303	7343.375246	26.239015
191.643099	7345.375759	26.244032
191.725027	7373.838764	26.249050
192.010195	7373.596251	26.254068
192.442939	7381.282611	26.259085
192.560323	7389.214164	26.264103
192.882460	7399.817543	26.269120
192.887487	7412.040930	26.274138
193.197577	7398.615431	26.279156
193.309062	7423.781873	26.284173
193.469528	7431.541688	26.289191
193.792403	7430.179135	26.294208
193.605434	7441.462316	26.299226
193.886786	7452.432458	26.304244
194.173224	7467.665553	26.309261
194.275590	7479.045800	26.314279
194.617683	7493.566296	26.319296
194.499616	7504.487590	26.324314
195.150906	7512.789260	26.329332
195.200875	7522.181401	26.334349
195.827389	7521.114375	26.339367
195.998607	7539.872653	26.344384
196.024025	7549.763548	26.349402
196.454505	7549.406392	26.354420
196.243221	7549.816354	26.359437
196.446934	7548.858702	26.364455
196.655508	7568.461543	26.369472
196.935711	7579.744680	26.374490
197.150059	7579.270489	26.379508
197.183262	7590.132142	26.384525
197.128476	7605.060302	26.389543
197.637388	7605.068258	26.394560
197.313061	7625.004361	26.399578
197.698982	7630.571798	26.404596
197.830268	7643.136017	26.409613
198.135774	7665.390882	26.414631
198.338439	7666.345942	26.419648
198.596191	7686.756062	26.424666
199.009502	7691.679371	26.429684
199.031138	7693.099213	26.434701
199.258923	7721.737197	26.439719
199.857519	7721.824833	26.444736
199.612132	7731.293560	26.449754
200.067883	7731.914489	26.454772
200.401628	7749.368448	26.459789
200.081903	7759.290614	26.464807
200.524706	7750.809353	26.469824
200.335270	7767.575623	26.474842
200.500411	7773.208804	26.479860
200.595518	7786.657421	26.484877
200.778747	7808.129263	26.489895
201.296204	7811.482791	26.494912
201.368376	7832.875374	26.499930
201.702575	7845.496750	26.504948
202.112363	7853.693640	26.509965
201.942724	7873.172777	26.514983
202.549858	7872.625680	26.520000
202.539282	7894.608651	26.525018
202.727093	7902.917145	26.530036
203.422890	7902.078881	26.535053
203.737544	7898.839737	26.540071
204.404083	7889.198873	26.545088
204.258666	7893.519184	26.550106
204.611813	7904.726673	26.555124
204.896892	7909.758714	26.560141
204.872705	7921.886501	26.565159
205.178108	7908.731537	26.570176
205.101096	7917.120113	26.575194
205.421419	7916.945031	26.580212
205.596621	7919.789659	26.585229
205.376563	7920.709159	26.590247
205.714967	7934.470523	26.595264
205.798049	7945.719596	26.600282
206.239796	7934.552296	26.605300
206.130024	7950.926678	26.610317
206.395737	7968.230658	26.615335
206.897802	7959.665432	26.620352
206.996512	7985.534372	26.625370
207.161973	7998.352374	26.630388
207.307694	8013.153985	26.635405
207.232556	8016.147989	26.640423
207.652201	8022.676517	26.645440
207.649345	8037.112036	26.650458
207.715682	8039.902236	26.655476
208.117918	8057.171109	26.660493
208.379790	8073.438407	26.665511
208.489012	8083.700958	26.670528
208.410116	8093.982841	26.675546
208.095359	8105.133249	26.680564
208.700201	8133.624481	26.685581
209.041822	8151.778656	26.690599
209.666387	8156.136211	26.695616
209.818140	8188.771163	26.700634
209.813229	8194.192386	26.705652
210.400063	8204.657960	26.710669
210.173350	8215.650503	26.715687
210.423366	8227.865470	26.720704
210.780107	8241.307396	26.725722
211.110488	8250.964702	26.730740
211.855434	8259.650645	26.735757
211.437113	8271.954224	26.740775
212.163180	8280.841025	26.745792
212.026966	8300.888621	26.750810
211.952167	8292.513241	26.755828
212.282647	8307.928908	26.760845
212.570364	8323.987373	26.765863
212.985120	8335.549689	26.770880
212.837827	8354.189924	26.775898
213.074714	8359.971348	26.780916
213.632610	8375.202128	26.785933
214.080746	8383.430756	26.790951
214.337947	8384.768340	26.795968
214.516886	8392.975366	26.800986
214.305581	8403.595250	26.806004
214.651536	8400.997560	26.811021
214.565583	8419.414239	26.816039
215.023986	8422.303455	26.821056
215.166649	8447.654623	26.826074
215.106965	8458.186424	26.831092
215.454484	8454.818054	26.836109
215.336346	8469.495978	26.841127
215.804402	8479.466211	26.846144
216.130936	8495.446738	26.851162
216.415151	8512.831747	26.856180
216.267450	8520.595054	26.861197
216.458718	8556.086884	26.866215
216.646488	8557.620310	26.871232
216.937848	8570.881915	26.876250
216.832008	8588.629343	26.881268
217.538315	8590.307746	26.886285
217.679310	8617.551633	26.891303
218.109691	8624.769491	26.896320
218.471483	8649.255990	26.901338
218.465497	8662.849697	26.906356
218.614640	8669.769094	26.911373
218.728944	8683.513060	26.916391
218.681110	8697.314600	26.921408
219.191679	8710.712553	26.926426
219.575417	8741.369201	26.931444
219.973167	8749.362156	26.936461
220.125295	8763.251967	26.941479
220.660132	8759.994323	26.946496
221.016999	8775.992955	26.951514
221.061253	8787.674438	26.956532
221.513744	8789.654052	26.961549
221.559480	8807.229320	26.966567
222.018142	8812.786711	26.971584
222.077138	8819.209051	26.976602
222.100296	8824.870835	26.981620
222.814676	8830.151149	26.986637
222.455933	8848.059681	26.991655
222.724386	8844.178094	26.996672
223.348361	8852.700055	27.001690
222.924580	8877.861288	27.006708
223.278774	8868.073818	27.011725
223.586072	8890.879957	27.016743
223.977164	8910.410908	27.021760
223.988815	8912.761288	27.026778
223.900695	8933.658802	27.031796
224.200761	8935.027152	27.036813
224.346957	8957.910471	27.041831
224.665279	8966.090780	27.046848
224.943991	8981.461312	27.051866
224.894889	8997.820418	27.056884
225.606439	9021.451580	27.061901
225.708418	9037.759721	27.066919
225.817190	9037.869376	27.071936
226.186957	9051.098707	27.076954
226.354676	9061.323055	27.081972
227.035161	9084.152774	27.086989
226.876311	9092.356992	27.092007
227.061127	9097.587197	27.097024
227.639832	9106.257799	27.102042
227.483506	9114.308782	27.107060
227.838543	9127.835243	27.112077
227.867492	9153.133088	27.117095
228.397640	9159.732026	27.122112
228.867503	9175.479960	27.127130
228.398345	9186.542447	27.132148
228.880268	9176.835271	27.137165
229.142837	9204.388536	27.142183
228.896084	9214.904533	27.147200
229.317511	9218.976962	27.152218
229.475289	9234.693898	27.157236
229.884521	9248.147680	27.162253
229.678712	9264.138318	27.167271
229.873365	9278.246842	27.172288
230.311257	9295.999581	27.177306
230.609817	9327.118126	27.182324
231.068503	9337.945197	27.187341
231.193583	9352.295337	27.192359
231.668558	9357.596552	27.197376
231.998963	9362.494719	27.202394
232.346079	9381.175625	27.207412
232.595756	9391.242452	27.212429
232.576626	9401.289184	27.217447
232.783462	9411.469467	27.222464
233.326670	9421.924160	27.227482
233.180922	9428.940756	27.232500
233.509416	9446.954411	27.237517
234.011103	9458.876568	27.242535
234.110328	9467.874105	27.247552
234.311027	9479.375000	27.252570
234.138454	9495.751900	27.257588
234.527712	9512.994562	27.262605
235.001365	9528.772941	27.267623
235.229919	9533.981869	27.272640
235.415451	9546.759189	27.277658
235.413146	9561.956213	27.282676
235.579930	9579.040399	27.287693
236.117375	9587.707854	27.292711
236.338757	9607.615956	27.297728
236.560392	9612.936347	27.302746
236.829122	9632.291485	27.307764
237.099266	9644.077216	27.312781
236.897786	9651.420618	27.317799
236.881916	9678.871106	27.322816
238.027453	9693.829408	27.327834
237.385557	9709.928913	27.332852
237.945826	9728.554458	27.337869
238.525766	9737.646678	27.342887
238.826308	9759.082813	27.347904
239.276919	9771.487130	27.352922
239.453277	9771.676201	27.357940
239.684011	9787.797565	27.362957
239.796707	9800.491031	27.367975
239.843499	9812.804663	27.372992
240.192362	9827.428581	27.378010
240.094005	9840.999184	27.383028
240.446566	9854.171367	27.388045
241.023583	9868.025680	27.393063
241.079251	9887.321856	27.398080
241.565467	9891.915510	27.403098
241.479951	9910.929413	27.408116
242.060328	9922.093619	27.413133
241.974408	9931.983144	27.418151
242.374007	9951.620314	27.423168
243.080933	9945.185052	27.428186
242.906530	9964.960582	27.433204
243.252750	9989.186214	27.438221
243.491225	10002.044945	27.443239
243.546057	10019.257637	27.448256
244.201470	10024.798643	27.453274
244.258800	10035.353863	27.458292
244.539365	10045.575917	27.463309
245.092003	10054.411281	27.468327
244.812246	10060.790927	27.473344
245.111230	10065.770144	27.478362
245.298336	10069.635781	27.483380
245.432577	10080.178299	27.488397
245.495091	10099.000114	27.493415
245.686281	10104.978815	27.498432
245.858144	10118.693212	27.503450
246.168578	10143.836514	27.508468
246.280599	10157.081852	27.513485
246.802614	10170.505136	27.518503
246.785890	10190.312353	27.523520
247.692019	10203.070183	27.528538
247.922006	10215.552332	27.533556
248.167702	10221.153349	27.538573
248.498803	10240.529622	27.543591
248.538401	10240.922538	27.548608
248.749470	10248.390152	27.553626
248.781496	10269.354599	27.558644
249.145709	10280.223160	27.563661
249.396854	10296.085609	27.568679
249.230252	10311.215997	27.573696
249.848549	10326.099875	27.578714
250.016757	10337.857296	27.583732
250.179720	10360.434945	27.588749
250.675552	10364.864851	27.593767
250.622352	10386.465948	27.598784
251.373174	10396.096715	27.603802
251.106652	10415.288500	27.608820
251.455283	10437.005929	27.613837
251.981543	10446.257918	27.618855
251.908849	10460.681176	27.623872
252.087679	10479.972645	27.628890
252.380861	10496.157652	27.633908
252.683151	10522.008801	27.638925
253.012505	10535.106600	27.643943
253.398594	10548.599973	27.648960
253.645782	10572.383562	27.653978
253.607091	10579.184399	27.658996
254.137841	10604.310860	27.664013
254.621451	10610.357159	27.669031
254.630916	10624.642485	27.674048
255.093785	10648.390486	27.679066
255.224647	10662.947255	27.684084
255.552423	10676.529172	27.689101
255.853077	10684.435175	27.694119
255.775727	10709.104658	27.699136
256.326591	10720.366487	27.704154
256.431180	10744.723857	27.709172
256.767571	10749.088083	27.714189
257.111134	10759.345860	27.719207
257.163326	10788.068811	27.724224
257.635742	10791.775521	27.729242
257.908414	10811.436328	27.734260
258.028305	10831.127175	27.739277
258.245495	10838.278119	27.744295
258.455311	10856.124701	27.749312
258.679763	10863.449359	27.754330
258.886112	10894.531050	27.759348
259.569789	10906.666037	27.764365
259.701762	10922.897854	27.769383
259.842204	10926.776150	27.774400
260.108549	10945.174433	27.779418
260.476331	10965.520884	27.784436
260.272382	10979.274585	27.789453
260.881319	10998.987109	27.794471
260.913033	11016.437901	27.799488
261.243718	11029.141949	27.804506
261.796608	11049.653258	27.809524
261.749148	11054.252861	27.814541
262.446291	11068.032391	27.819559
262.202764	11083.166777	27.824576
262.460504	11091.462990	27.829594
262.661213	11110.664926	27.834612
263.290494	11125.746274	27.839629
263.648591	11145.451650	27.844647
263.829616	11158.563480	27.849664
264.461474	11148.675101	27.854682
264.456894	11178.974439	27.859700
264.684223	11180.515756	27.864717
264.780187	11188.098193	27.869735
264.578272	11206.744464	27.874752
265.224512	11224.396306	27.879770
265.356015	11243.422340	27.884788
265.366078	11272.926823	27.889805
265.814040	11280.676373	27.894823
266.079855	11308.673130	27.899840
266.187115	11324.524954	27.904858
266.596704	11347.316860	27.909876
266.800234	11368.956349	27.914893
267.023999	11388.673228	27.919911
267.125344	11412.688622	27.924928
267.688874	11435.469353	27.929946
268.119636	11455.719330	27.934964
268.183672	11486.138674	27.939981
268.853933	11496.311329	27.944999
268.872939	11515.939344	27.950016
269.081580	11521.699013	27.955034
269.331287	11548.249127	27.960052
269.565471	11566.073551	27.965069
269.859492	11576.885273	27.970087
270.387528	11603.012793	27.975104
270.540939	11610.243972	27.980122
271.036782	11631.673122	27.985140
271.717031	11643.810812	27.990157
271.662625	11657.174748	27.995175
271.776103	11672.070949	28.000192
272.188000	11685.480637	28.005210
272.485184	11694.861087	28.010228
272.703314	11709.238895	28.015245
272.823704	11720.846870	28.020263
272.894407	11748.353515	28.025280
273.255665	11762.504400	28.030298
273.819026	11789.723138	28.035316
273.890708	11804.092179	28.040333
274.536730	11813.509506	28.045351
274.755827	11830.418019	28.050368
274.980361	11854.733569	28.055386
275.227854	11858.791347	28.060404
275.343226	11876.568019	28.065421
275.855605	11891.165173	28.070439
276.033144	11911.813772	28.075456
276.358287	11928.332940	28.080474
276.693900	11941.919354	28.085492
276.752446	11956.876911	28.090509
277.086282	11975.232104	28.095527
276.789952	11995.466009	28.100544
277.078796	12016.537551	28.105562
277.774983	12033.141962	28.110580
277.626085	12065.148259	28.115597
278.618497	12077.385888	28.120615
278.813375	12095.237886	28.125632
278.879447	12110.766370	28.130650
279.107122	12118.199799	28.135668
278.968791	12140.420085	28.140685
279.491163	12163.840570	28.145703
280.064422	12189.346972	28.150720
279.953645	12200.629532	28.155738
280.339739	12218.524081	28.160756
280.661286	12241.461039	28.165773
281.176841	12258.295715	28.170791
281.646798	12273.176011	28.175808
281.943603	12294.331692	28.180826
281.990213	12291.935014	28.185844
281.994305	12311.333231	28.190861
282.540413	12319.719445	28.195879
282.773088	12347.042708	28.200896
283.053806	12353.302901	28.205914
283.347138	12366.792663	28.210932
283.649833	12379.987775	28.215949
283.859057	12397.026159	28.220967
284.104919	12418.582826	28.225984
284.504513	12444.614775	28.231002
284.977229	12444.791863	28.236020
285.011575	12468.482673	28.241037
285.297933	12483.284817	28.246055
285.491715	12501.372249	28.251072
285.881516	12525.483374	28.256090
285.951688	12543.586586	28.261108
286.259534	12568.940531	28.266125
286.651456	12584.573122	28.271143
286.750788	12604.953463	28.276160
287.082209	12628.757650	28.281178
287.569649	12641.121842	28.286196
287.610467	12673.687318	28.291213
287.948338	12683.888954	28.296231
288.002859	12708.464003	28.301248
288.271299	12735.893889	28.306266
288.407977	12758.286972	28.311284
288.748287	12797.204452	28.316301
289.372625	12809.230932	28.321319
290.025730	12843.933195	28.326336
290.060038	12867.682900	28.331354
290.958098	12874.670045	28.336372
291.011118	12890.344842	28.341389
291.181519	12912.417372	28.346407
291.405923	12933.612659	28.351424
291.737051	12958.673389	28.356442
292.491824	12969.948746	28.361460
292.185384	12998.435542	28.366477
292.689702	12998.982480	28.371495
292.950856	13023.892571	28.376512
292.869760	13046.074675	28.381530
293.500133	13058.401344	28.386548
293.667872	13084.349771	28.391565
293.918059	13099.057603	28.396583
294.331007	13109.683616	28.401600
295.067057	13138.329053	28.406618
295.000909	13148.558455	28.411636
295.030428	13173.978322	28.416653
295.256286	13182.602379	28.421671
295.895589	13205.042111	28.426688
295.847799	13239.824983	28.431706
296.611242	13241.027189	28.436724
296.684695	13273.486023	28.441741
297.133273	13300.869709	28.446759
297.190168	13316.265328	28.451776
297.310828	13338.669740	28.456794
297.834591	13345.703285	28.461812
298.045870	13382.648352	28.466829
298.272231	13406.004580	28.471847
298.795348	13431.584272	28.476864
298.650816	13445.774641	28.481882
299.172443	13461.479590	28.486900
299.808227	13487.997339	28.491917
299.610329	13505.127907	28.496935
300.362054	13519.160538	28.501952
300.690889	13544.050766	28.506970
300.990804	13550.171135	28.511988
301.046771	13570.968039	28.517005
301.640311	13577.197416	28.522023
301.773599	13596.282644	28.527040
301.752751	13623.453012	28.532058
302.309216	13652.332381	28.537076
302.340532	13664.493900	28.542093
302.907191	13679.047435	28.547111
303.116469	13697.959452	28.552128
303.341594	13717.451988	28.557146
303.998507	13736.411312	28.562164
303.906156	13751.048772	28.567181
304.562856	13772.889104	28.572199
304.629428	13777.620321	28.577216
305.045401	13808.932931	28.582234
305.140997	13832.757423	28.587252
305.527240	13854.510244	28.592269
305.991697	13879.906500	28.597287
306.080719	13899.004136	28.602304
306.299387	13919.501904	28.607322
307.024929	13942.596611	28.612340
306.874474	13970.701522	28.617357
307.319931	13987.847464	28.622375
307.756961	14010.737857	28.627392
307.601183	14033.494724	28.632410
308.221492	14053.651953	28.637428
308.276857	14083.347879	28.642445
308.736241	14113.410397	28.647463
309.607704	14129.713720	28.652480
309.371273	14160.340662	28.657498
309.864748	14172.605733	28.662516
310.199330	14200.794666	28.667533
310.522350	14219.198311	28.672551
311.231017	14232.918750	28.677568
311.312084	14258.965342	28.682586
311.986699	14267.758410	28.687604
312.349567	14299.563022	28.692621
312.616582	14308.778188	28.697639
312.765246	14320.388065	28.702656
313.124909	14337.091517	28.707674
313.444252	14349.418640	28.712692
313.721342	14379.937356	28.717709
313.883420	14397.253564	28.722727
314.239460	14418.012911	28.727744
314.680125	14433.669156	28.732762
314.812613	14454.142456	28.737780
314.772504	14476.006073	28.742797
315.184019	14498.144858	28.747815
315.948170	14520.445958	28.752832
315.835640	14549.042045	28.757850
316.496639	14557.575897	28.762868
316.837476	14578.065301	28.767885
316.927726	14596.269908	28.772903
317.593386	14618.347879	28.777920
317.762761	14650.323892	28.782938
317.938973	14661.559070	28.787956
318.407791	14683.917156	28.792973
318.689440	14700.197314	28.797991
318.754576	14715.096416	28.803008
318.791532	14746.025941	28.808026
319.582702	14755.997818	28.813044
319.677390	14783.768815	28.818061
319.824748	14811.420814	28.823079
320.357033	14828.326309	28.828096
320.567654	14846.038439	28.833114
320.979648	14877.853378	28.838132
320.947711	14896.436318	28.843149
321.389914	14915.538151	28.848167
321.815104	14938.381366	28.853184
321.685983	14969.434942	28.858202
322.409446	14994.985500	28.863220
322.343325	15021.127010	28.868237
322.613422	15048.052990	28.873255
323.292507	15074.897136	28.878272
323.342287	15098.215654	28.883290
323.669724	15111.085777	28.888308
324.263527	15144.349553	28.893325
324.342414	15175.306043	28.898343
325.251948	15192.340188	28.903360
325.159736	15222.880615	28.908378
325.559254	15253.338136	28.913396
326.027628	15266.500283	28.918413
326.513294	15292.431111	28.923431
326.909435	15309.006578	28.928448
327.059259	15337.563764	28.933466
327.582161	15354.189224	28.938484
328.033472	15378.202964	28.943501
328.290987	15404.088193	28.948519
328.565531	15416.467667	28.953536
328.670015	15440.902995	28.958554
329.265006	15457.223462	28.963572
329.486701	15485.802109	28.968589
329.661100	15512.101611	28.973607
330.261664	15523.976422	28.978624
330.277682	15553.419871	28.983642
330.509488	15582.011197	28.988660
331.228482	15606.567305	28.993677
331.326993	15627.760122	28.998695
332.116765	15640.262546	29.003712
331.909712	15674.561521	29.008730
332.445019	15694.933443	29.013748
332.675906	15721.569115	29.018765
332.785595	15749.301429	29.023783
333.291851	15772.014173	29.028800
333.569749	15806.154348	29.033818
333.886219	15831.678999	29.038836
334.432259	15848.736162	29.043853
334.653798	15877.402205	29.048871
335.052707	15899.075257	29.053888
335.343627	15934.731431	29.058906
335.682347	15954.177875	29.063924
336.091650	15978.153734	29.068941
336.295924	16005.832995	29.073959
336.850170	16032.667846	29.078976
336.936924	16063.055684	29.083994
337.272378	16093.044614	29.089012
337.742569	16110.213904	29.094029
338.246461	16143.080034	29.099047
338.616973	16156.208653	29.104064
339.140244	16193.893370	29.109082
339.090648	16204.891135	29.114100
339.655862	16225.503082	29.119117
339.822225	16255.692102	29.124135
340.514412	16274.773057	29.129152
340.751958	16297.245699	29.134170
340.900768	16315.863371	29.139188
341.948353	16339.314835	29.144205
341.909841	16359.390065	29.149223
342.388838	16375.375986	29.154240
342.370263	16392.394756	29.159258
342.243253	16416.715369	29.164276
342.931407	16444.157653	29.169293
343.022893	16469.458869	29.174311
343.689010	16487.015411	29.179328
343.940490	16516.492536	29.184346
344.301848	16532.491775	29.189364
344.538730	16553.423286	29.194381
344.974242	16577.971017	29.199399
345.260976	16591.569393	29.204416
345.720190	16621.412697	29.209434
345.721248	16640.945785	29.214452
346.085175	16659.766260	29.219469
346.330237	16686.995400	29.224487
347.133202	16708.526982	29.229504
347.257744	16729.582920	29.234522
347.490787	16758.576455	29.239540
348.062387	16783.770316	29.244557
348.367247	16805.209495	29.249575
348.510113	16835.398733	29.254592
348.805817	16862.086992	29.259610
349.260765	16885.632590	29.264628
350.085208	16907.066299	29.269645
350.009071	16935.274298	29.274663
350.645100	16956.616302	29.279680
350.773305	16978.836842	29.284698
350.756645	17000.299536	29.289716
351.331438	17026.424840	29.294733
351.267448	17057.310769	29.299751
352.165983	17094.273379	29.304768
352.276573	17116.670413	29.309786
352.751269	17143.212853	29.314804
353.032649	17175.644966	29.319821
353.516456	17209.946272	29.324839
353.869339	17234.507078	29.329856
354.176201	17264.110355	29.334874
354.471402	17301.160670	29.339892
354.606957	17333.013486	29.344909
354.848486	17364.658087	29.349927
355.489454	17392.440790	29.354944
355.903368	17423.404364	29.359962
356.608872	17450.523874	29.364980
356.876373	17470.453643	29.369997
357.451789	17500.938219	29.375015
357.955157	17527.345691	29.380032
358.226719	17547.834490	29.385050
358.388685	17560.120707	29.390068
358.955768	17585.190428	29.395085
359.052748	17617.994418	29.400103
359.388431	17641.321222	29.405120
359.779925	17663.142842	29.410138
359.850602	17697.467815	29.415156
360.163817	17725.609562	29.420173
360.363981	17771.865380	29.425191
361.254568	17804.975055	29.430208
361.295045	17824.521927	29.435226
361.706293	17862.422878	29.440244
362.230056	17878.554180	29.445261
362.636956	17914.580059	29.450279
362.833330	17937.033363	29.455296
363.558022	17962.280925	29.460314
363.974723	17996.401065	29.465332
364.308213	18016.197608	29.470349
364.699985	18044.804546	29.475367
364.949524	18066.574522	29.480384
365.220268	18089.758214	29.485402
365.523186	18108.759109	29.490420
365.990263	18139.557577	29.495437
365.954447	18168.002183	29.500455
366.592396	18195.953833	29.505472
367.068201	18228.228131	29.510490
367.361755	18253.437140	29.515508
368.004092	18279.860644	29.520525
367.958988	18310.876615	29.525543
368.355734	18335.316710	29.530560
368.834484	18347.322497	29.535578
368.809563	18374.592780	29.540596
369.527451	18399.966673	29.545613
369.689380	18432.931775	29.550631
370.136073	18456.775766	29.555648
370.175333	18479.449707	29.560666
370.924517	18518.752865	29.565684
371.652023	18546.179511	29.570701
371.436720	18571.027078	29.575719
371.754888	18599.207316	29.580736
372.595289	18624.591230	29.585754
372.566574	18661.442792	29.590772
372.782386	18677.307390	29.595789
373.273392	18710.377801	29.600807
373.759575	18744.848987	29.605824
374.106730	18773.365242	29.610842
374.167074	18809.620670	29.615860
374.529076	18842.477797	29.620877
374.721157	18879.446217	29.625895
375.203038	18922.038980	29.630912
375.739295	18953.171178	29.635930
376.354344	18995.434673	29.640948
377.035676	19021.775653	29.645965
377.198515	19056.089743	29.650983
377.700820	19092.669921	29.656000
377.849578	19116.531056	29.661018
378.191849	19151.501429	29.666036
378.905276	19176.350688	29.671053
379.220060	19208.402865	29.676071
379.652034	19239.893385	29.681088
380.072857	19269.270112	29.686106
379.961614	19296.021739	29.691124
380.688974	19320.697066	29.696141
380.947211	19367.666591	29.701159
381.031609	19404.382827	29.706176
381.330093	19433.981886	29.711194
382.133794	19478.624337	29.716212
382.614422	19503.183112	29.721229
382.670422	19551.458895	29.726247
383.108127	19572.523353	29.731264
383.489774	19609.193997	29.736282
383.906843	19646.032280	29.741300
384.429465	19668.794952	29.746317
384.657901	19718.594017	29.751335
385.412990	19746.658160	29.756352
386.245907	19775.819378	29.761370
386.217472	19812.727027	29.766388
387.060710	19831.370868	29.771405
387.094948	19871.246431	29.776423
387.365119	19886.570295	29.781440
387.816548	19911.142384	29.786458
388.104664	19958.389250	29.791476
388.654806	19979.572776	29.796493
389.138684	20010.420788	29.801511
389.311495	20043.864967	29.806528
389.966850	20075.619644	29.811546
389.892046	20113.130005	29.816564
390.375589	20136.662857	29.821581
390.733428	20167.098449	29.826599
391.089961	20202.869572	29.831616
391.581193	20230.893057	29.836634
391.765321	20272.915767	29.841652
392.448372	20294.195942	29.846669
392.588636	20328.872686	29.851687
392.990786	20365.987775	29.856704
393.701819	20387.693858	29.861722
393.515335	20423.312515	29.866740
394.075028	20449.545015	29.871757
394.438025	20489.911576	29.876775
394.660364	20512.706169	29.881792
395.307128	20545.371303	29.886810
395.653002	20581.332616	29.891828
395.607705	20610.557064	29.896845
395.867971	20643.147605	29.901863
396.448846	20687.943671	29.906880
397.042374	20724.594298	29.911898
397.247511	20760.356974	29.916916
397.716122	20799.038685	29.921933
398.171542	20835.982021	29.926951
398.278320	20874.433678	29.931968
398.950698	20907.134693	29.936986
399.514839	20953.976036	29.942004
399.754055	20981.246253	29.947021
400.076050	21027.200781	29.952039
400.436672	21060.805100	29.957056
401.014586	21097.329833	29.962074
401.229254	21130.483860	29.967092
401.309652	21180.470993	29.972109
402.469067	21214.017529	29.977127
402.842899	21260.205348	29.982144
403.563450	21292.001989	29.987162
403.708800	21333.209136	29.992180
404.062386	21364.383923	29.997197
404.751655	21397.571878	30.002215
404.367501	21432.788620	30.007232
405.165283	21471.239228	30.012250
405.630207	21508.674404	30.017268
406.047873	21549.491707	30.022285
406.542063	21585.725465	30.027303
406.789311	21622.093197	30.032320
407.495124	21655.955347	30.037338
407.767788	21688.645189	30.042356
408.485524	21724.900592	30.047373
408.921264	21747.771911	30.052391
409.121092	21794.319528	30.057408
409.568329	21833.486482	30.062426
410.011706	21866.679788	30.067444
410.300847	21897.259166	30.072461
410.776685	21935.276887	30.077479
411.317335	21980.229679	30.082496
412.038622	21998.505075	30.087514
411.888485	22039.740765	30.092532
412.794006	22069.991394	30.097549
412.749901	22101.400493	30.102567
413.046091	22141.280637	30.107584
413.368250	22172.492073	30.112602
413.704226	22211.208428	30.117620
414.232261	22252.441203	30.122637
414.562056	22286.147667	30.127655
415.123613	22331.077432	30.132672
415.574772	22362.570618	30.137690
416.110406	22400.927964	30.142708
416.454883	22443.710058	30.147725
417.043096	22477.664273	30.152743
417.378889	22519.386791	30.157760
417.911614	22545.384183	30.162778
418.368476	22586.623243	30.167796
418.797334	22614.530133	30.172813
419.147760	22654.700530	30.177831
419.685469	22672.994421	30.182848
420.261054	22711.399471	30.187866
420.409085	22750.009394	30.192884
420.973097	22773.835366	30.197901
421.912033	22801.790609	30.202919
421.714967	22835.184830	30.207936
422.204428	22853.892155	30.212954
422.401398	22891.057780	30.217972
423.018842	22913.671959	30.222989
423.417961	22947.190077	30.228007
423.607699	22976.141599	30.233024
424.283008	23006.320043	30.238042
424.522482	23043.485274	30.243060
425.165377	23076.124406	30.248077
425.550459	23103.914771	30.253095
425.812133	23145.476058	30.258112
426.013974	23168.556729	30.263130
426.054718	23205.468207	30.268148
426.480620	23242.200913	30.273165
427.283515	23279.304959	30.278183
427.425984	23318.363354	30.283200
427.871796	23345.068614	30.288218
428.077810	23396.985807	30.293236
428.766093	23440.134548	30.298253
429.468758	23475.399580	30.303271
429.905144	23520.069357	30.308288
430.899056	23559.085171	30.313306
431.344184	23597.387657	30.318324
431.361790	23632.766381	30.323341
432.034989	23658.043650	30.328359
432.158446	23693.157404	30.333376
432.748603	23725.213580	30.338394
432.883421	23766.125594	30.343412
433.345994	23806.608154	30.348429
434.058689	23848.597986	30.353447
434.229382	23882.136821	30.358464
434.866009	23915.863546	30.363482
435.193107	23963.310670	30.368500
435.853792	23995.267373	30.373517
436.449359	24020.904960	30.378535
436.399063	24076.870556	30.383552
436.733299	24110.789635	30.388570
437.396747	24151.195615	30.393588
437.410755	24188.192488	30.398605
438.321678	24227.415959	30.403623
438.674845	24272.131437	30.408640
439.135453	24308.266169	30.413658
439.736770	24349.020376	30.418676
439.720203	24391.753561	30.423693
440.641888	24432.111163	30.428711
440.935668	24483.075657	30.433728
441.131391	24512.580746	30.438746
441.878044	24551.434738	30.443764
442.288568	24608.656815	30.448781
442.848774	24641.722654	30.453799
442.955033	24693.639787	30.458816
443.528511	24728.015686	30.463834
443.804781	24770.203012	30.468852
444.570541	24801.219691	30.473869
444.741760	24845.805916	30.478887
444.802901	24900.885230	30.483904
445.332113	24944.810039	30.488922
445.879244	24990.192350	30.493940
446.151922	25042.783212	30.498957
447.042425	25077.224052	30.503975
447.467184	25113.858460	30.508992
448.022833	25153.218545	30.514010
448.442187	25201.880792	30.519028
449.039831	25246.176701	30.524045
449.628603	25284.582204	30.529063
450.068848	25323.012371	30.534080
450.346646	25352.994219	30.539098
450.788726	25390.727160	30.544116
451.152917	25433.005652	30.549133
451.881165	25460.342478	30.554151
452.285395	25491.344532	30.559168
452.570541	25519.947067	30.564186
453.400999	25552.086762	30.569204
453.582441	25585.835327	30.574221
453.868456	25621.276245	30.579239
453.967702	25654.587491	30.584256
454.942140	25695.529184	30.589274
455.199778	25736.570665	30.594292
455.413126	25780.792757	30.599309
455.883781	25815.525355	30.604327
456.479934	25849.019707	30.609344
457.082980	25888.212765	30.614362
457.694533	25927.306722	30.619380
457.640504	25976.939004	30.624397
458.393407	26006.600490	30.629415
458.878993	26059.799550	30.634432
458.892034	26097.948858	30.639450
459.608479	26143.224181	30.644468
459.908069	26192.315953	30.649485
460.244842	26235.894229	30.654503
460.868014	26283.614200	30.659520
460.836197	26322.765047	30.664538
461.470406	26378.378813	30.669556
462.156445	26430.583763	30.674573
462.458093	26470.812185	30.679591
463.095273	26517.139400	30.684608
463.639166	26576.153413	30.689626
464.091338	26618.950193	30.694644
464.207041	26672.250198	30.699661
464.993361	26716.058119	30.704679
465.498619	26771.767042	30.709696
466.133385	26813.619301	30.714714
466.804955	26856.131161	30.719732
467.088922	26899.508499	30.724749
467.691614	26942.337951	30.729767
468.080482	26989.644400	30.734784
468.686069	27031.609267	30.739802
469.399286	27068.256875	30.744820
469.589701	27117.848821	30.749837
469.685712	27161.033945	30.754855
470.409164	27214.307604	30.759872
471.138174	27262.202033	30.764890
471.669788	27304.220810	30.769908
472.240102	27352.179603	30.774925
472.860481	27378.310207	30.779943
473.158858	27422.408860	30.784960
473.485193	27463.626034	30.789978
474.138910	27501.748125	30.794996
474.629195	27551.099259	30.800013
475.151972	27581.271566	30.805031
475.326221	27628.517478	30.810048
475.529545	27666.234960	30.815066
476.031128	27719.253505	30.820084
476.112782	27773.329095	30.825101
476.551068	27806.531593	30.830119
477.325682	27864.013364	30.835136
477.807600	27917.266055	30.840154
478.474536	27960.163103	30.845172
478.855501	28022.682274	30.850189
479.486110	28062.923048	30.855207
479.824903	28116.455561	30.860224
480.232625	28171.207163	30.865242
480.648096	28214.859410	30.870260
481.108810	28264.769535	30.875277
481.712920	28311.286834	30.880295
481.952277	28363.315984	30.885312
482.387959	28408.640533	30.890330
483.212799	28449.689222	30.895348
483.561128	28501.413670	30.900365
484.019777	28542.958529	30.905383
484.128824	28588.466939	30.910400
484.282560	28640.274475	30.915418
485.402019	28685.398264	30.920436
485.658706	28738.192276	30.925453
485.968037	28789.870401	30.930471
486.432152	28837.049538	30.935488
487.175832	28888.725488	30.940506
487.952857	28944.872782	30.945524
488.658650	28990.822973	30.950541
489.113415	29037.316443	30.955559
489.640500	29075.740564	30.960576
489.923464	29125.499580	30.965594
490.627804	29169.188442	30.970612
490.843272	29220.668839	30.975629
491.648041	29258.306016	30.980647
492.306395	29300.387511	30.985664
492.611127	29359.374823	30.990682
493.397075	29406.678920	30.995700
493.595493	29442.915086	31.000717
493.997426	29492.428305	31.005735
494.575527	29542.461473	31.010752
494.843995	29585.264396	31.015770
495.460975	29632.824219	31.020788
496.051356	29691.755918	31.025805
496.534864	29735.015799	31.030823
497.112726	29783.188259	31.035840
497.645310	29831.226368	31.040858
498.088337	29880.837999	31.045876
498.592157	29929.780313	31.050893
499.310329	29964.240468	31.055911
499.466000	30016.660670	31.060928
499.754549	30068.696213	31.065946
500.953238	30119.590626	31.070964
500.762892	30168.572747	31.075981
501.515991	30218.550492	31.080999
502.023264	30258.441279	31.086016
502.354537	30322.806830	31.091034
502.833056	30359.907204	31.096052
503.549402	30422.262713	31.101069
504.315007	30479.530566	31.106087
504.655226	30527.151227	31.111104
505.137718	30572.312720	31.116122
505.797390	30620.316182	31.121140
506.244745	30675.554945	31.126157
506.666406	30707.058770	31.131175
507.215470	30755.756106	31.136192
507.744908	30809.893177	31.141210
508.022688	30864.841920	31.146228
508.531600	30916.830885	31.151245
508.816078	30973.302812	31.156263
509.545070	31020.696409	31.161280
509.882598	31086.322639	31.166298
510.865676	31132.279888	31.171316
511.221959	31182.603690	31.176333
511.783129	31232.647626	31.181351
512.416255	31275.192384	31.186368
512.780948	31327.805922	31.191386
513.296156	31379.391335	31.196404
513.943380	31422.808126	31.201421
514.053255	31475.574701	31.206439
514.662969	31529.943656	31.211456
515.147107	31594.080300	31.216474
515.882586	31635.687641	31.221492
516.239942	31686.161000	31.226509
516.865163	31732.396742	31.231527
517.248012	31772.387272	31.236544
517.708401	31831.271910	31.241562
518.160877	31878.006763	31.246580
518.420817	31913.969625	31.251597
518.636669	31973.885983	31.256615
519.663240	32026.294264	31.261632
519.793700	32078.096834	31.266650
520.349101	32128.456642	31.271668
520.703785	32198.504877	31.276685
521.469553	32244.620884	31.281703
521.952327	32307.501321	31.286720
522.394632	32363.269993	31.291738
522.954115	32423.127854	31.296756
523.522261	32481.375195	31.301773
523.806970	32542.339159	31.306791
524.536187	32595.574572	31.311808
525.093634	32654.692011	31.316826
525.577238	32715.532149	31.321844
525.945421	32775.539603	31.326861
526.255639	32837.513278	31.331879
526.962042	32904.707145	31.336896
527.725577	32975.359765	31.341914
528.570534	33032.496534	31.346932
528.972648	33090.350496	31.351949
529.535688	33143.895893	31.356967
529.850994	33195.295616	31.361984
530.357581	33257.471774	31.367002
530.809364	33311.070794	31.372020
531.477022	33386.953983	31.377037
531.766060	33448.737638	31.382055
532.560074	33508.743371	31.387072
533.030024	33581.195199	31.392090
533.565353	33650.528165	31.397108
534.208335	33705.295888	31.402125
534.465422	33771.368207	31.407143
535.094214	33835.009332	31.412160
535.806677	33903.477710	31.417178
536.039889	33960.156953	31.422196
536.752635	34030.121583	31.427213
537.391033	34092.654372	31.432231
538.017723	34159.339143	31.437248
538.346953	34227.086384	31.442266
539.008128	34291.736780	31.447284
539.686497	34355.923818	31.452301
540.545030	34414.495498	31.457319
541.245408	34466.292753	31.462336
541.658075	34536.832879	31.467354
542.141416	34589.199735	31.472372
542.750082	34648.043897	31.477389
543.179845	34705.160041	31.482407
544.344330	34760.567399	31.487424
544.391720	34816.263905	31.492442
544.906980	34875.288373	31.497460
545.717207	34931.938334	31.502477
545.983004	35001.636715	31.507495
546.932311	35045.056543	31.512512
547.210286	35104.780612	31.517530
548.199884	35156.724520	31.522548
548.367585	35204.436738	31.527565
548.753053	35264.885200	31.532583
549.237766	35305.772554	31.537600
549.839243	35378.430799	31.542618
550.324685	35436.767729	31.547636
550.888571	35485.314596	31.552653
551.467873	35548.405067	31.557671
551.883026	35617.620343	31.562688
552.320239	35681.558510	31.567706
552.940895	35731.892428	31.572724
553.471703	35786.593542	31.577741
553.917266	35839.806643	31.582759
554.510497	35884.208983	31.587776
554.965840	35948.675316	31.592794
555.339859	36009.226006	31.597812
555.967198	36064.325438	31.602829
555.914593	36125.534139	31.607847
556.798775	36194.954919	31.612864
557.638628	36261.504910	31.617882
558.226587	36325.111114	31.622900
558.552939	36384.973442	31.627917
558.721767	36452.746126	31.632935
559.719153	36507.233354	31.637952
560.267372	36574.132585	31.642970
560.920041	36651.174579	31.647988
561.440381	36712.344122	31.653005
561.707852	36770.115430	31.658023
562.294260	36847.611094	31.663040
562.870950	36925.440102	31.668058
563.357389	36985.050676	31.673076
564.167041	37059.350896	31.678093
564.423378	37132.401548	31.683111
565.292614	37206.310601	31.688128
565.802060	37279.850226	31.693146
566.239794	37352.657121	31.698164
567.121672	37426.299848	31.703181
567.895415	37494.424535	31.708199
568.548209	37559.173251	31.713216
569.001946	37624.857852	31.718234
569.545130	37684.243542	31.723252
570.459300	37748.170061	31.728269
570.784656	37817.582198	31.733287
571.296958	37885.704261	31.738304
572.153947	37957.437315	31.743322
572.323779	38020.515763	31.748340
572.943768	38094.535950	31.753357
573.538199	38168.257647	31.758375
574.197695	38220.170282	31.763392
574.960708	38298.368895	31.768410
575.607249	38360.163868	31.773428
576.172387	38425.346823	31.778445
576.328661	38496.661325	31.783463
577.299744	38565.742204	31.788480
577.685008	38629.655157	31.793498
578.132549	38699.012552	31.798516
578.690637	38774.731338	31.803533
579.169510	38847.161762	31.808551
580.007318	38913.636577	31.813568
580.589692	38993.354805	31.818586
581.188212	39054.209932	31.823604
582.132466	39116.804180	31.828621
582.548433	39179.640721	31.833639
583.083169	39251.419548	31.838656
583.917061	39311.545282	31.843674
584.163395	39381.573039	31.848692
585.141945	39447.092132	31.853709
585.554870	39518.390245	31.858727
586.388378	39576.076787	31.863744
586.918634	39641.869618	31.868762
587.453066	39711.734170	31.873780
588.248391	39774.825658	31.878797
588.547054	39838.517241	31.883815
588.932665	39889.952750	31.888832
589.658372	39965.127854	31.893850
589.949407	40034.942357	31.898868
590.897685	40094.559275	31.903885
591.356477	40164.845289	31.908903
592.241819	40222.900948	31.913920
592.321975	40283.852226	31.918938
592.735877	40346.342690	31.923956
593.688125	40398.850746	31.928973
594.043253	40466.260234	31.933991
594.142541	40526.858738	31.939008
594.867587	40600.672780	31.944026
595.313970	40673.785037	31.949044
595.546087	40747.630708	31.954061
596.240525	40828.961002	31.959079
596.876242	40906.651957	31.964096
597.367829	40983.584162	31.969114
598.007715	41069.682057	31.974132
599.106086	41136.140744	31.979149
599.342315	41224.721225	31.984167
600.012347	41294.269425	31.989184
600.825554	41374.357554	31.994202
601.766459	41448.925367	31.999220
602.398654	41518.231264	32.004237
602.542735	41594.153263	32.009255
603.511226	41665.011009	32.014272
603.984821	41734.523906	32.019290
604.423645	41814.331755	32.024308
605.268921	41884.737163	32.029325
605.885457	41965.633874	32.034343
606.591625	42037.262577	32.039360
607.139000	42117.217939	32.044378
607.563382	42194.286257	32.049396
608.719858	42274.072067	32.054413
609.049417	42345.726380	32.059431
609.755127	42417.432396	32.064448
610.228396	42498.026779	32.069466
610.369329	42572.333647	32.074484
611.271865	42652.974498	32.079501
611.814343	42732.857541	32.084519
612.374277	42812.210777	32.089536
612.944901	42905.606116	32.094554
613.561004	42989.607788	32.099572
614.345838	43059.042568	32.104589
614.814677	43154.050424	32.109607
615.531132	43217.836047	32.114624
616.433950	43298.416496	32.119642
616.825446	43383.600055	32.124660
617.832213	43463.311534	32.129677
618.353731	43537.552962	32.134695
618.739379	43610.648929	32.139712
619.984177	43696.242128	32.144730
620.295589	43770.475036	32.149748
621.128953	43830.265064	32.154765
621.813405	43920.827060	32.159783
622.436607	43993.007450	32.164800
623.058832	44062.993840	32.169818
623.503145	44126.732861	32.174836
624.388351	44202.871236	32.179853
624.704439	44279.473501	32.184871
625.361033	44357.554299	32.189888
626.134044	44422.755553	32.194906
626.784733	44499.233893	32.199924
627.045772	44572.057411	32.204941
628.061730	44651.065132	32.209959
628.511983	44721.985492	32.214976
629.189855	44789.770869	32.219994
630.007302	44872.948804	32.225012
630.818066	44944.501876	32.230029
631.191436	45019.771480	32.235047
631.864292	45092.134177	32.240064
632.327998	45159.968948	32.245082
632.723660	45238.267080	32.250100
633.136641	45300.884819	32.255117
634.198110	45367.794136	32.260135
634.388934	45444.630269	32.265152
634.931521	45519.037080	32.270170
635.705566	45592.505943	32.275188
636.549417	45667.090853	32.280205
637.223639	45734.861286	32.285223
637.749385	45800.240841	32.290240
638.728335	45865.826688	32.295258
639.183078	45946.154739	32.300276
639.774415	46012.484142	32.305293
640.260587	46093.518121	32.310311
640.767342	46169.607056	32.315328
641.358834	46248.991685	32.320346
641.968730	46328.815699	32.325364
642.579427	46407.430458	32.330381
643.023982	46489.613001	32.335399
643.687607	46570.761766	32.340416
644.398711	46662.219879	32.345434
645.120855	46749.757635	32.350452
645.639459	46825.360919	32.355469
646.509228	46913.882387	32.360487
647.057160	46999.299554	32.365504
647.916334	47077.645449	32.370522
648.381270	47155.213706	32.375540
649.326150	47244.362198	32.380557
650.006124	47319.662847	32.385575
650.534292	47409.923195	32.390592
651.382209	47485.032497	32.395610
651.854091	47571.775397	32.400628
652.492026	47653.504636	32.405645
653.477146	47741.887706	32.410663
653.839771	47819.766134	32.415680
654.563101	47902.214988	32.420698
655.286924	47983.280861	32.425716
656.316466	48057.670744	32.430733
656.854262	48146.019150	32.435751
657.346034	48220.094386	32.440768
658.001735	48307.264988	32.445786
658.636017	48403.850927	32.450804
659.132347	48473.429129	32.455821
659.745577	48560.633176	32.460839
660.210251	48643.137486	32.465856
661.249164	48726.260918	32.470874
661.691506	48817.805402	32.475892
662.721554	48903.334500	32.480909
663.352875	48990.995459	32.485927
663.726808	49064.259661	32.490944
664.317319	49151.511208	32.495962
664.804761	49243.546113	32.500980
665.678185	49324.937168	32.505997
666.735331	49408.976458	32.511015
666.865680	49518.464806	32.516032
667.850262	49599.481738	32.521050
668.509532	49688.357227	32.526068
669.347567	49773.950389	32.531085
670.031348	49847.782205	32.536103
670.519555	49946.209832	32.541120
671.060318	50025.820668	32.546138
671.866528	50119.648401	32.551156
672.864395	50203.309312	32.556173
673.280037	50297.275162	32.561191
673.833702	50380.397574	32.566208
674.788030	50458.672056	32.571226
675.336186	50548.391100	32.576244
675.767533	50629.614425	32.581261
676.791233	50704.580899	32.586279
677.321218	50787.595268	32.591296
677.898913	50870.020919	32.596314
678.637859	50955.231403	32.601332
679.376360	51027.517272	32.606349
680.152571	51109.089859	32.611367
680.482002	51193.674235	32.616384
681.853039	51262.716653	32.621402
682.378915	51339.821063	32.626420
683.102609	51412.483538	32.631437
683.344826	51478.940138	32.636455
683.966691	51584.742152	32.641472
684.271412	51660.046048	32.646490
684.964849	51749.759244	32.651508
685.661234	51847.173397	32.656525
686.147520	51927.306447	32.661543
687.032416	52027.192055	32.666560
687.720227	52100.159958	32.671578
688.280575	52214.213693	32.676596
688.992673	52302.087917	32.681613
689.766611	52393.900854	32.686631
690.178325	52496.135182	32.691648
691.093571	52585.442784	32.696666
691.543188	52684.190751	32.701684
692.350090	52779.215790	32.706701
693.300399	52872.398032	32.711719
693.649629	52971.846381	32.716736
694.792866	53060.183392	32.721754
695.161203	53167.981828	32.726772
695.767056	53264.350288	32.731789
696.697856	53363.754963	32.736807
697.271415	53463.926855	32.741824
697.808505	53564.939274	32.746842
698.717756	53664.841846	32.751860
699.366743	53772.546628	32.756877
700.260045	53864.776341	32.761895
700.873934	53969.328931	32.766912
701.810543	54067.023975	32.771930
702.517223	54163.045293	32.776948
703.309075	54255.994945	32.781965
704.304177	54361.604891	32.786983
704.819487	54458.360636	32.792000
705.726512	54546.654946	32.797018
706.289369	54641.167019	32.802036
706.877481	54736.793728	32.807053
707.864060	54823.660789	32.812071
708.682627	54924.835802	32.817088
709.181125	55006.110400	32.822106
709.966007	55105.832333	32.827124
710.585174	55213.815289	32.832141
711.331159	55305.412650	32.837159
711.879352	55399.766486	32.842176
712.820344	55493.164863	32.847194
713.467441	55584.299651	32.852212
714.317384	55678.800779	32.857229
715.026665	55774.014369	32.862247
715.538898	55872.129740	32.867264
716.600527	55953.100228	32.872282
717.128629	56054.234266	32.877300
718.102474	56147.206921	32.882317
718.726458	56237.059474	32.887335
719.397624	56334.506306	32.892352
720.266445	56423.668350	32.897370
720.772360	56532.985229	32.902388
721.081913	56622.221715	32.907405
721.901257	56711.766054	32.912423
722.533924	56815.060408	32.917440
723.611173	56912.777803	32.922458
724.105071	57010.225661	32.927476
724.754895	57106.428598	32.932493
725.534287	57196.664190	32.937511
726.089514	57293.888430	32.942528
727.131678	57376.447728	32.947546
727.188628	57472.232312	32.952564
728.164433	57565.375548	32.957581
728.958742	57659.130620	32.962599
729.344040	57758.660189	32.967616
730.047804	57849.694834	32.972634
730.932445	57953.402056	32.977652
731.403554	58060.603374	32.982669
732.469503	58151.364615	32.987687
732.826247	58269.518715	32.992704
733.941630	58358.237819	32.997722
734.704719	58461.399005	33.002740
735.345643	58559.152358	33.007757
736.324042	58664.294932	33.012775
736.742539	58766.067472	33.017792
737.610249	58860.744998	33.022810
738.585897	58961.434167	33.027828
739.284705	59067.408739	33.032845
740.058299	59171.665143	33.037863
740.994699	59275.648681	33.042880
741.780142	59371.732579	33.047898
742.346596	59474.615472	33.052916
742.965103	59586.211815	33.057933
743.813119	59672.838459	33.062951
744.482102	59783.694422	33.067968
745.194489	59883.066598	33.072986
746.164649	59986.700599	33.078004
746.716566	60097.546039	33.083021
747.613678	60195.795811	33.088039
748.059371	60311.330575	33.093056
749.093201	60404.022261	33.098074
750.015519	60511.174567	33.103092
750.322906	60622.847026	33.108109
751.560317	60718.843580	33.113127
752.299245	60832.651595	33.118144
752.895281	60935.928851	33.123162
753.690708	61048.363523	33.128180
754.303252	61154.015626	33.133197
755.222242	61254.731859	33.138215
755.683470	61358.134675	33.143232
756.488286	61469.975986	33.148250
757.166699	61580.081696	33.153268
757.856974	61694.155378	33.158285
758.722597	61805.792527	33.163303
759.418861	61920.890425	33.168320
759.976360	62031.043839	33.173338
760.970751	62139.741337	33.178356
761.368105	62269.017501	33.183373
762.515256	62379.252234	33.188391
763.028637	62496.703348	33.193408
763.937514	62611.062009	33.198426
764.931599	62723.624710	33.203444
765.700044	62846.136617	33.208461
766.647035	62942.482397	33.213479
767.460574	63060.253695	33.218496
768.050279	63168.094370	33.223514
768.885429	63279.554925	33.228532
769.492341	63382.469739	33.233549
770.346669	63486.823294	33.238567
770.762814	63605.605282	33.243584
771.690486	63721.503039	33.248602
772.487305	63831.342030	33.253620
773.339981	63956.160167	33.258637
774.173230	64060.456887	33.263655
774.754883	64174.454794	33.268672
775.557943	64280.628739	33.273690
776.582034	64371.386627	33.278708
777.140552	64488.424370	33.283725
778.233470	64591.334336	33.288743
778.827440	64692.620525	33.293760
779.402250	64800.200326	33.298778
780.451629	64889.192578	33.303796
780.651244	65002.044465	33.308813
781.624385	65110.957065	33.313831
782.424069	65228.869397	33.318848
782.976075	65346.519918	33.323866
784.186686	65448.131341	33.328884
784.535646	65565.639670	33.333901
785.773946	65674.802157	33.338919
786.268758	65777.918055	33.343936
786.768879	65900.859025	33.348954
787.753135	66019.737826	33.353972
788.523013	66133.373921	33.358989
789.108688	66251.776273	33.364007
790.325085	66369.999109	33.369024
791.118195	66486.731071	33.374042
791.752225	66608.117772	33.379060
792.307655	66737.452462	33.384077
793.194964	66853.051858	33.389095
793.889686	66985.153111	33.394112
794.700383	67097.529545	33.399130
795.970514	67222.652186	33.404148
796.432457	67346.796513	33.409165
797.006221	67475.127445	33.414183
798.197902	67593.898644	33.419200
798.518885	67728.228622	33.424218
799.783533	67843.448589	33.429236
800.520825	67976.604855	33.434253
801.709325	68094.310885	33.439271
802.191698	68219.082881	33.444288
802.729648	68339.249871	33.449306
803.829822	68460.437341	33.454324
804.675363	68593.939969	33.459341
805.334591	68712.154265	33.464359
806.248035	68848.176352	33.469376
807.233967	68974.481803	33.474394
808.133146	69091.773328	33.479412
809.260308	69220.661893	33.484429
809.974250	69338.655639	33.489447
810.374501	69454.476240	33.494464
811.139330	69592.121038	33.499482
812.188902	69712.388199	33.504500
812.931804	69841.786681	33.509517
813.737095	69971.162979	33.514535
814.287328	70087.683036	33.519552
815.153628	70222.501309	33.524570
816.206354	70351.168722	33.529588
817.057276	70479.509857	33.534605
818.159076	70609.125512	33.539623
818.899959	70726.572323	33.544640
819.534540	70856.121305	33.549658
820.886725	70971.767367	33.554676
821.593365	71104.436009	33.559693
822.110529	71223.212512	33.564711
823.064815	71339.160324	33.569728
823.883404	71458.564886	33.574746
824.957493	71583.789809	33.579764
825.599543	71693.733179	33.584781
826.360979	71826.390872	33.589799
827.534392	71944.999572	33.594816
827.906005	72064.083012	33.599834
828.854511	72183.078019	33.604852
829.557028	72302.190248	33.609869
830.562317	72419.425472	33.614887
831.381273	72535.775187	33.619904
831.997313	72649.288040	33.624922
832.849536	72759.619435	33.629940
833.379870	72880.451800	33.634957
834.204985	73003.032096	33.639975
834.815223	73129.518926	33.644992
835.467374	73248.094477	33.650010
836.480559	73361.918484	33.655028
837.310647	73506.786916	33.660045
838.048818	73632.015970	33.665063
839.115151	73761.137776	33.670080
839.544083	73888.101681	33.675098
840.543059	74021.732706	33.680116
841.036681	74156.902720	33.685133
842.081648	74285.588452	33.690151
843.033786	74420.684261	33.695168
843.712519	74557.514744	33.700186
844.785020	74687.286083	33.705204
845.647783	74820.849639	33.710221
846.428120	74963.319964	33.715239
846.944582	75107.972565	33.720256
847.787551	75246.715501	33.725274
848.848700	75382.836433	33.730292
849.714244	75524.240071	33.735309
850.730396	75657.587264	33.740327
851.949630	75793.254501	33.745344
852.682514	75939.103766	33.750362
853.653733	76063.017857	33.755380
854.539584	76197.888854	33.760397
855.189440	76332.654226	33.765415
856.497461	76463.465977	33.770432
857.166363	76614.168881	33.775450
858.335612	76744.739590	33.780468
859.098289	76882.348570	33.785485
860.052103	77000.654084	33.790503
861.335892	77131.233421	33.795520
861.882436	77281.183082	33.800538
862.582624	77396.698947	33.805556
863.639676	77529.095509	33.810573
864.344753	77663.012217	33.815591
865.325344	77794.632333	33.820608
865.911826	77933.124534	33.825626
866.791577	78072.062475	33.830644
867.610814	78206.880747	33.835661
868.514516	78338.225803	33.840679
869.653847	78484.619113	33.845696
869.995940	78612.238014	33.850714
870.794283	78754.065463	33.855732
871.837471	78903.551661	33.860749
872.727364	79045.283573	33.865767
873.785982	79179.422870	33.870784
874.668579	79324.377553	33.875802
875.462094	79458.176478	33.880820
876.383562	79603.537705	33.885837
877.089433	79750.289267	33.890855
878.162767	79876.440647	33.895872
878.992382	80021.750168	33.900890
880.346234	80154.903863	33.905908
880.827638	80287.171475	33.910925
881.848947	80434.501586	33.915943
882.693505	80565.856741	33.920960
883.647420	80713.724879	33.925978
884.460585	80845.067861	33.930996
885.511914	80987.493775	33.936013
885.909872	81121.551392	33.941031
887.341609	81252.971569	33.946048
888.291345	81401.287707	33.951066
889.007915	81530.955149	33.956084
889.924263	81659.046638	33.961101
890.603990	81788.943062	33.966119
891.655386	81904.411248	33.971136
892.350634	82046.700209	33.976154
893.072632	82168.816468	33.981172
893.849651	82290.905299	33.986189
894.624430	82428.413207	33.991207
895.251709	82569.862554	33.996224
896.017221	82705.077059	34.001242
897.027833	82846.180011	34.006260
897.971519	83004.079927	34.011277
898.529916	83138.698549	34.016295
899.626805	83285.806762	34.021312
900.451477	83444.564526	34.026330
901.124461	83592.927935	34.031348
902.019290	83750.853694	34.036365
902.937924	83907.656704	34.041383
903.892311	84050.845267	34.046400
904.357888	84217.798043	34.051418
905.529799	84374.226986	34.056436
906.627032	84529.068544	34.061453
907.361546	84694.354173	34.066471
908.177986	84854.755390	34.071488
908.930402	85021.938579	34.076506
910.177497	85183.909634	34.081524
911.417930	85347.015529	34.086541
911.869681	85499.698724	34.091559
913.159455	85664.197051	34.096576
914.067496	85827.702954	34.101594
915.213772	85991.676813	34.106612
916.333729	86144.734615	34.111629
917.189230	86309.821831	34.116647
918.186236	86463.427242	34.121664
919.286178	86617.832921	34.126682
919.925913	86771.353884	34.131700
921.009893	86928.327013	34.136717
921.884212	87091.151218	34.141735
923.120455	87240.558364	34.146752
923.919729	87392.886317	34.151770
925.115077	87550.667810	34.156788
926.275506	87711.360721	34.161805
927.126039	87864.910886	34.166823
927.888440	88000.770406	34.171840
928.802160	88161.102161	34.176858
929.689665	88315.079442	34.181876
930.966816	88468.164283	34.186893
931.151747	88618.722196	34.191911
932.156422	88768.227891	34.196928
933.112045	88935.721651	34.201946
933.905261	89100.920899	34.206964
935.434148	89257.513120	34.211981
935.920519	89426.954829	34.216999
936.989381	89576.157527	34.222016
937.785834	89740.411368	34.227034
938.733816	89904.312188	34.232052
939.774182	90065.142081	34.237069
940.601821	90229.697892	34.242087
941.677899	90382.606734	34.247104
942.418252	90549.666384	34.252122
943.277334	90714.296254	34.257140
944.412794	90875.609492	34.262157
945.126540	91054.069101	34.267175
946.357442	91208.419571	34.272192
947.350323	91364.652139	34.277210
948.216445	91533.248412	34.282228
949.087114	91689.193157	34.287245
949.944223	91866.090733	34.292263
951.024704	92012.192627	34.297280
952.141504	92167.403529	34.302298
952.971087	92325.036403	34.307316
953.832032	92467.702548	34.312333
954.683656	92624.738759	34.317351
955.808940	92771.306175	34.322368
956.454165	92933.517989	34.327386
957.254804	93091.116291	34.332404
958.320357	93239.797788	34.337421
959.190357	93413.602982	34.342439
960.211511	93572.022409	34.347456
961.210269	93738.333328	34.352474
962.052977	93896.841325	34.357492
962.774978	94062.212763	34.362509
963.765713	94229.965186	34.367527
964.713360	94394.795161	34.372544
965.887068	94573.843748	34.377562
966.468693	94745.193067	34.382580
967.352180	94911.866452	34.387597
968.442262	95087.387805	34.392615
969.562812	95257.721046	34.397632
970.676321	95445.388443	34.402650
971.280028	95626.121417	34.407668
972.732499	95801.113136	34.412685
973.382542	95971.459439	34.417703
974.246045	96149.798409	34.422720
975.408156	96338.920473	34.427738
976.328796	96517.689417	34.432756
977.576243	96697.874259	34.437773
978.070531	96879.052209	34.442791
979.457946	97059.798916	34.447808
980.502232	97242.312913	34.452826
981.290322	97428.111870	34.457844
982.640348	97599.252454	34.462861
983.610468	97797.647360	34.467879
984.423615	97966.834400	34.472896
985.748214	98150.327882	34.477914
986.378021	98328.499397	34.482932
987.567992	98498.248111	34.487949
988.511931	98689.861326	34.492967
989.758986	98876.652319	34.497984
990.737717	99055.980470	34.503002
991.853526	99234.882035	34.508020
993.103315	99416.852283	34.513037
993.693033	99605.143832	34.518055
994.894690	99770.347021	34.523072
995.775032	99953.920671	34.528090
996.985981	100140.429341	34.533108
997.991564	100319.799932	34.538125
998.543150	100502.159278	34.543143
999.887918	100676.455506	34.548160
1000.967835	100860.775091	34.553178
1001.923225	101044.717703	34.558196
1003.034319	101224.640677	34.563213
1004.046710	101416.212369	34.568231
1004.970792	101581.872016	34.573248
1006.091231	101764.108257	34.578266
1006.630296	101950.335923	34.583284
1007.878852	102127.070263	34.588301
1008.654225	102308.240335	34.593319
1010.021159	102498.887635	34.598336
1010.952843	102674.177445	34.603354
1011.648262	102864.495225	34.608372
1013.096022	103051.479679	34.613389
1014.026138	103238.316779	34.618407
1014.852543	103407.651486	34.623424
1015.985091	103602.290506	34.628442
1016.889222	103772.957140	34.633460
1018.419911	103959.706428	34.638477
1019.279983	104130.433333	34.643495
1020.107611	104295.556296	34.648512
1021.453406	104458.251659	34.653530
1022.027926	104638.248959	34.658548
1022.641216	104805.056977	34.663565
1023.882850	104976.448180	34.668583
1024.689567	105146.430600	34.673600
1026.188828	105324.544580	34.678618
1026.791739	105515.929084	34.683636
1028.289259	105692.222041	34.688653
1028.755560	105872.714252	34.693671
1029.514301	106059.213416	34.698688
1030.625558	106239.132858	34.703706
1031.650732	106446.843445	34.708724
1032.487025	106624.771789	34.713741
1033.801940	106823.520747	34.718759
1034.770898	107012.904961	34.723776
1035.593882	107204.531196	34.728794
1036.672579	107410.277194	34.733812
1038.020251	107597.145703	34.738829
1038.698943	107803.315501	34.743847
1039.603404	107997.201184	34.748864
1040.964286	108199.625983	34.753882
1041.722460	108405.293255	34.758900
1042.909161	108594.158612	34.763917
1043.881352	108812.105565	34.768935
1044.926830	109016.868647	34.773952
1046.295012	109212.320398	34.778970
1047.467245	109425.489111	34.783988
1048.738004	109627.344136	34.789005
1049.751024	109821.668281	34.794023
1050.868476	110024.602974	34.799040
1052.243122	110222.455030	34.804058
1053.070513	110419.993639	34.809076
1054.780283	110614.220893	34.814093
1055.334532	110817.292585	34.819111
1056.506781	110997.423640	34.824128
1057.520735	111201.967636	34.829146
1058.330754	111398.844764	34.834164
1059.622357	111583.140338	34.839181
1060.716449	111783.165584	34.844199
1061.595457	111988.079759	34.849216
1062.922119	112192.212015	34.854234
1063.819878	112389.031015	34.859252
1065.091213	112588.386685	34.864269
1065.748049	112796.358660	34.869287
1066.882767	113001.960152	34.874304
1067.906399	113198.852752	34.879322
1068.921359	113415.232865	34.884340
1070.085621	113615.335709	34.889357
1071.278765	113825.355064	34.894375
1071.757159	114038.382723	34.899392
1073.214404	114240.215269	34.904410
1074.190317	114451.884217	34.909428
1075.322190	114658.689255	34.914445
1076.201032	114868.971080	34.919463
1077.224500	115088.758102	34.924480
1078.615480	115294.650758	34.929498
1079.605768	115515.561513	34.934516
1080.713307	115714.700401	34.939533
1081.947424	115926.793816	34.944551
1082.907983	116151.629456	34.949568
1083.963569	116355.076572	34.954586
1085.216944	116570.123742	34.959604
1086.238395	116778.546264	34.964621
1087.240049	116980.473635	34.969639
1088.156908	117190.550934	34.974656
1089.442710	117394.790966	34.979674
1090.480691	117611.908863	34.984692
1091.131838	117807.513949	34.989709
1092.390223	118002.069653	34.994727
1093.334666	118225.923212	34.999744
1094.358869	118425.373474	35.004762
1095.574653	118625.870486	35.009780
1096.570586	118836.567580	35.014797
1097.624163	119047.307358	35.019815
1098.374765	119262.926572	35.024832
1099.802170	119467.132478	35.029850
1100.714377	119693.131488	35.034868
1101.715052	119907.370926	35.039885
1103.149970	120121.185331	35.044903
1103.838025	120348.417605	35.049920
1104.962024	120565.910821	35.054938
1105.760864	120802.378856	35.059956
1107.111767	121028.733802	35.064973
1108.147438	121252.443398	35.069991
1109.162159	121494.267015	35.075008
1110.282673	121717.585927	35.080026
1111.345659	121958.036717	35.085044
1112.548100	122183.626659	35.090061
1113.675031	122419.331016	35.095079
1114.892768	122657.962337	35.100096
1116.328641	122891.072092	35.105114
1117.808549	123131.222628	35.110132
1118.533961	123354.530402	35.115149
1119.624485	123595.319319	35.120167
1120.825882	123831.744856	35.125184
1122.078253	124055.870531	35.130202
1123.137263	124289.484333	35.135220
1124.341878	124527.980586	35.140237
1125.818856	124753.759904	35.145255
1126.526392	124998.602883	35.150272
1128.025861	125232.708787	35.155290
1129.023545	125470.156683	35.160308
1130.144007	125697.167954	35.165325
1131.340847	125935.739896	35.170343
1132.299354	126176.330299	35.175360
1133.738879	126412.837935	35.180378
1134.990918	126646.868822	35.185396
1136.351485	126886.929362	35.190413
1137.403171	127121.694082	35.195431
1138.187230	127359.267946	35.200448
1139.653233	127585.602288	35.205466
1140.492915	127825.591448	35.210484
1141.678838	128065.030892	35.215501
1142.786403	128305.879408	35.220519
1144.014113	128544.871998	35.225536
1145.273697	128774.430621	35.230554
1146.315142	129029.872403	35.235572
1147.411219	129273.176647	35.240589
1148.728796	129501.349359	35.245607
1149.545926	129752.080695	35.250624
1150.892910	129984.282958	35.255642
1151.843517	130235.528455	35.260660
1152.823125	130481.688026	35.265677
1154.457618	130724.318669	35.270695
1155.831449	130976.831079	35.275712
1156.841890	131209.947262	35.280730
1158.251646	131455.498175	35.285748
1159.126397	131685.471131	35.290765
1160.302944	131921.860964	35.295783
1161.314350	132167.609953	35.300800
1162.752277	132404.175633	35.305818
1163.446818	132651.920264	35.310836
1164.662480	132897.083266	35.315853
1166.093055	133130.232673	35.320871
1166.922029	133360.453342	35.325888
1168.303243	133590.406872	35.330906
1169.351500	133825.120398	35.335924
1170.430247	134055.951250	35.340941
1171.687878	134281.442242	35.345959
1172.735079	134514.424065	35.350976
1174.122837	134751.965968	35.355994
1175.074758	134991.838301	35.361012
1176.156292	135227.824172	35.366029
1177.894502	135457.795201	35.371047
1178.252844	135698.189170	35.376064
1179.411803	135934.420855	35.381082
1180.579899	136176.649571	35.386100
1181.659570	136420.580902	35.391117
1182.873886	136668.105146	35.396135
1184.073688	136917.649528	35.401152
1185.282412	137174.801532	35.406170
1186.302815	137428.956402	35.411188
1187.602522	137692.221207	35.416205
1188.987490	137937.342986	35.421223
1189.821869	138197.721773	35.426240
1191.446522	138451.885915	35.431258
1192.345580	138723.872215	35.436276
1193.584502	138985.153814	35.441293
1194.881897	139239.580825	35.446311
1195.858102	139504.777086	35.451328
1197.318820	139762.655211	35.456346
1198.504217	140025.703425	35.461364
1199.352479	140298.217861	35.466381
1200.777359	140558.669234	35.471399
1201.778803	140823.744718	35.476416
1203.348336	141088.170404	35.481434
1204.577033	141356.344412	35.486452
1205.975709	141628.638879	35.491469
1207.614465	141891.258633	35.496487
1207.928046	142168.390415	35.501504
1209.403652	142425.258815	35.506522
1210.643999	142693.846968	35.511540
1211.814060	142966.176968	35.516557
1213.127483	143232.626776	35.521575
1214.502364	143508.667998	35.526592
1215.584715	143783.631106	35.531610
1216.894172	144054.056963	35.536628
1218.199362	144324.625080	35.541645
1219.681641	144598.843600	35.546663
1221.021536	144863.196161	35.551680
1222.174511	145133.846299	35.556698
1223.469564	145401.380653	35.561716
1224.465773	145677.374445	35.566733
1225.585711	145938.626188	35.571751
1226.841008	146217.624948	35.576768
1227.645773	146492.007944	35.581786
1229.406022	146770.787994	35.586804
1230.255565	147041.908411	35.591821
1231.714714	147311.699889	35.596839
1232.791161	147602.723698	35.601856
1233.968672	147874.975552	35.606874
1235.767401	148155.877798	35.611892
1236.669447	148433.112879	35.616909
1237.753452	148709.292650	35.621927
1239.135948	148992.476878	35.626944
1240.479953	149267.590511	35.631962
1242.096446	149532.425829	35.636980
1242.924267	149820.362754	35.641997
1244.500226	150089.318095	35.647015
1245.362858	150361.957314	35.652032
1246.661308	150636.479738	35.657050
1247.960726	150904.573404	35.662068
1249.162451	151168.524862	35.667085
1250.951701	151423.603862	35.672103
1251.997628	151685.212796	35.677120
1253.028766	151939.849789	35.682138
1253.953836	152196.674985	35.687156
1255.314599	152463.399626	35.692173
1256.766223	152722.982567	35.697191
1257.688107	152993.829700	35.702208
1258.793695	153264.229786	35.707226
1260.352787	153527.123696	35.712244
1261.573024	153799.652253	35.717261
1262.676287	154071.935678	35.722279
1263.977979	154343.718873	35.727296
1264.966484	154615.302027	35.732314
1266.563152	154901.361537	35.737332
1267.252028	155187.382897	35.742349
1268.632149	155462.002327	35.747367
1269.970163	155760.440766	35.752384
1271.326120	156045.609658	35.757402
1272.294909	156326.747207	35.762420
1273.544831	156631.727047	35.767437
1274.936677	156928.998294	35.772455
1276.082184	157218.967454	35.777472
1277.548421	157509.989360	35.782490
1278.982963	157790.984092	35.787508
1280.328533	158097.164408	35.792525
1281.529672	158394.160838	35.797543
1282.876559	158688.103362	35.802560
1284.044082	158993.254220	35.807578
1285.666017	159284.415354	35.812596
1286.760590	159586.550658	35.817613
1288.338032	159878.662154	35.822631
1289.408745	160181.960240	35.827648
1290.482587	160486.313027	35.832666
1292.143574	160774.649093	35.837684
1293.306300	161079.156457	35.842701
1294.608037	161384.328161	35.847719
1295.787439	161699.671953	35.852736
1297.188468	162003.372737	35.857754
1298.469962	162292.276768	35.862772
1299.863232	162615.166341	35.867789
1301.561723	162919.306657	35.872807
1302.701089	163221.092864	35.877824
1303.860703	163527.965586	35.882842
1305.555556	163822.508421	35.887860
1306.822518	164130.255846	35.892877
1307.956100	164425.771027	35.897895
1309.317880	164741.969950	35.902912
1310.517237	165053.947522	35.907930
1311.879132	165347.274274	35.912948
1313.095691	165665.039164	35.917965
1314.548679	165966.767311	35.922983
1315.927505	166277.163277	35.928000
1317.062689	166577.679290	35.933018
1318.575795	166879.251479	35.938036
1319.536272	167201.751840	35.943053
1320.899148	167512.488992	35.948071
1322.544058	167818.537575	35.953088
1323.655483	168129.066782	35.958106
1324.951951	168448.246839	35.963124
1326.121686	168766.473033	35.968141
1327.544430	169076.551247	35.973159
1328.943477	169387.041546	35.978176
1330.588708	169702.911632	35.983194
1331.986123	169999.409981	35.988212
1332.997636	170318.497950	35.993229
1334.523967	170632.998224	35.998247
1336.109612	170932.783454	36.003264
1337.281167	171236.306402	36.008282
1338.849097	171523.928856	36.013300
1340.140113	171817.118971	36.018317
1341.175345	172110.568917	36.023335
1342.676068	172394.819576	36.028352
1343.856287	172685.343100	36.033370
1345.249111	172968.307944	36.038388
1346.135333	173277.297242	36.043405
1347.265532	173576.514665	36.048423
1348.685023	173883.858828	36.053440
1350.022030	174197.589260	36.058458
1351.644906	174496.197977	36.063476
1352.518949	174820.250320	36.068493
1353.782263	175130.699375	36.073511
1355.121394	175451.493655	36.078528
1356.354796	175769.490107	36.083546
1357.381534	176088.258847	36.088564
1358.614227	176427.732963	36.093581
1360.112764	176758.738479	36.098599
1361.394032	177096.178532	36.103616
1362.711894	177439.148271	36.108634
1364.077494	177765.905413	36.113652
1365.758116	178107.423693	36.118669
1367.131230	178450.327718	36.123687
1368.519124	178785.324648	36.128704
1369.747830	179132.483481	36.133722
1371.236338	179473.928437	36.138740
1372.530593	179825.409061	36.143757
1373.758258	180170.023959	36.148775
1375.247271	180517.199850	36.153792
1376.740871	180869.949195	36.158810
1378.208872	181210.913949	36.163828
1379.460167	181553.122501	36.168845
1381.015141	181910.526792	36.173863
1382.972016	182264.731999	36.178880
1383.891443	182604.387482	36.183898
1385.289276	182959.070445	36.188916
1386.676329	183310.013132	36.193933
1388.009936	183655.470887	36.198951
1389.640864	184013.206615	36.203968
1390.985835	184362.106773	36.208986
1392.450607	184717.082072	36.214004
1393.759889	185076.934172	36.219021
1395.466383	185429.119658	36.224039
1396.897565	185774.612661	36.229056
1398.039593	186139.843188	36.234074
1399.719968	186497.117105	36.239092
1401.297803	186858.459500	36.244109
1402.629915	187215.325826	36.249127
1403.932282	187560.406742	36.254144
1405.656126	187919.053323	36.259162
1407.348293	188259.364582	36.264180
1408.583829	188603.358402	36.269197
1409.913798	188953.292190	36.274215
1411.426366	189303.769133	36.279232
1412.707775	189654.768743	36.284250
1414.053488	190003.017830	36.289268
1415.728943	190352.407744	36.294285
1417.137728	190706.718451	36.299303
1418.812744	191046.578922	36.304320
1419.808716	191396.836169	36.309338
1421.514660	191739.691355	36.314356
1422.433291	192099.714963	36.319373
1423.718592	192445.461853	36.324391
1425.128950	192800.089161	36.329408
1426.374409	193153.501635	36.334426
1427.707322	193508.171169	36.339444
1429.254459	193869.446871	36.344461
1430.606513	194212.323425	36.349479
1432.312643	194543.603317	36.354496
1433.606488	194891.304666	36.359514
1435.262145	195222.571030	36.364532
1436.716538	195567.266088	36.369549
1437.680631	195913.897548	36.374567
1439.215107	196248.616986	36.379584
1440.396092	196600.980064	36.384602
1442.062863	196947.412018	36.389620
1443.530079	197299.947360	36.394637
1444.699110	197654.882578	36.399655
1446.328883	198015.075846	36.404672
1447.777801	198375.605628	36.409690
1449.063314	198726.591480	36.414708
1450.648746	199085.858257	36.419725
1451.797428	199459.177621	36.424743
1453.382423	199822.130220	36.429760
1454.378277	200186.972248	36.434778
1455.750564	200563.828278	36.439796
1457.205753	200954.537197	36.444813
1458.630651	201329.166735	36.449831
1460.343717	201704.944109	36.454848
1461.716444	202094.377847	36.459866
1463.551444	202468.818607	36.464884
1464.662954	202854.807982	36.469901
1465.978851	203241.070346	36.474919
1467.658624	203624.570157	36.479936
1469.113708	204012.299092	36.484954
1470.415435	204408.156122	36.489972
1472.299010	204793.901035	36.494989
1473.607985	205188.999127	36.500007
1475.346259	205580.714335	36.505024
1476.763781	205976.103280	36.510042
1478.163771	206365.707114	36.515060
1479.841319	206762.618871	36.520077
1481.110906	207162.660143	36.525095
1482.918261	207552.761234	36.530112
1484.426557	207952.652753	36.535130
1485.629796	208340.889349	36.540148
1487.204987	208740.735617	36.545165
1488.901162	209140.119422	36.550183
1490.310799	209526.524442	36.555200
1492.217703	209934.042015	36.560218
1493.665834	210329.498046	36.565236
1495.142726	210721.497291	36.570253
1496.382065	211123.518336	36.575271
1498.159681	211516.919126	36.580288
1499.628849	211915.147212	36.585306
1501.217230	212313.357415	36.590324
1502.853706	212709.428141	36.595341
1504.349464	213121.422327	36.600359
1506.063255	213512.582240	36.605376
1507.515634	213908.307718	36.610394
1508.762669	214298.608435	36.615412
1510.601452	214690.133697	36.620429
1511.801595	215093.829902	36.625447
1513.796782	215486.373955	36.630464
1514.948291	215882.132141	36.635482
1516.744601	216279.995037	36.640500
1518.316657	216680.944366	36.645517
1519.663622	217077.487892	36.650535
1521.152943	217466.923440	36.655552
1522.608275	217858.728159	36.660570
1524.205470	218257.190712	36.665588
1525.657680	218658.142428	36.670605
1526.795477	219059.071466	36.675623
1528.352489	219457.773922	36.680640
1529.804648	219851.872672	36.685658
1531.645445	220243.775192	36.690676
1533.422323	220618.012130	36.695693
1534.379317	221009.631692	36.700711
1536.029298	221390.521389	36.705728
1537.327793	221780.106170	36.710746
1539.276053	222171.820098	36.715764
1540.782226	222547.581492	36.720781
1541.585746	222944.770280	36.725799
1543.214414	223337.709409	36.730816
1544.379441	223737.228751	36.735834
1545.956684	224146.384007	36.740852
1547.388280	224589.092358	36.745869
1548.707705	225039.186817	36.750887
1550.150951	225454.896418	36.755904
1551.819717	225885.810153	36.760922
1553.293519	226304.540152	36.765940
1555.028659	226736.233239	36.770957
1556.391714	227152.469707	36.775975
1557.977985	227588.076475	36.780992
1559.360445	228012.516776	36.786010
1560.983247	228458.229726	36.791028
1562.409286	228894.222830	36.796045
1563.781432	229344.120374	36.801063
1565.667965	229766.908012	36.806080
1567.298478	230219.966165	36.811098
1568.483604	230662.862767	36.816116
1570.527402	231101.605501	36.821133
1571.938291	231560.571711	36.826151
1573.716810	232008.048080	36.831168
1575.303131	232459.672497	36.836186
1576.612356	232909.972327	36.841204
1578.526544	233361.849978	36.846221
1579.845144	233826.324772	36.851239
1581.585246	234269.698823	36.856256
1583.386740	234729.219279	36.861274
1584.800295	235197.517809	36.866292
1586.423287	235648.230439	36.871309
1588.405151	236105.286161	36.876327
1590.023796	236572.893981	36.881344
1591.808522	237019.341193	36.886362
1593.090130	237478.725945	36.891380
1594.996020	237928.482914	36.896397
1596.045570	238393.166358	36.901415
1597.847986	238848.048299	36.906432
1599.611731	239309.643796	36.911450
1601.191920	239777.697381	36.916468
1603.066461	240237.981060	36.921485
1604.591364	240697.662991	36.926503
1606.313299	241158.329393	36.931520
1607.720998	241618.667574	36.936538
1609.294414	242087.133450	36.941556
1610.946912	242540.167827	36.946573
1612.403715	243015.996024	36.951591
1614.246417	243476.545180	36.956608
1615.894696	243958.363845	36.961626
1617.571097	244425.318127	36.966644
1619.298294	244877.023140	36.971661
1620.653202	245343.295313	36.976679
1622.539166	245810.648994	36.981696
1624.082391	246272.776186	36.986714
1625.725770	246743.321230	36.991732
1627.579087	247202.375527	36.996749
1629.089077	247686.864659	37.001767
1630.842319	248147.689474	37.006784
1632.082695	248607.862865	37.011802
1633.522886	249072.982758	37.016820
1635.332248	249545.536073	37.021837
1637.239663	250009.868491	37.026855
1638.410060	250458.827217	37.031872
1640.008504	250917.343419	37.036890
1641.709132	251372.515325	37.041908
1643.527464	251818.091161	37.046925
1644.769730	252277.124558	37.051943
1646.594747	252732.251539	37.056960
1648.490064	253180.305110	37.061978
1649.732334	253648.509969	37.066996
1651.577436	254095.048161	37.072013
1653.091744	254567.501729	37.077031
1654.658358	255029.861779	37.082048
1656.091409	255501.389257	37.087066
1657.393164	255970.322052	37.092084
1659.227957	256438.252422	37.097101
1660.997860	256926.414650	37.102119
1662.553978	257404.374757	37.107136
1664.205807	257881.734846	37.112154
1665.711312	258378.781302	37.117172
1667.472390	258862.626644	37.122189
1668.920897	259351.959907	37.127207
1670.594174	259839.655590	37.132224
1672.444229	260345.663180	37.137242
1674.182263	260845.185921	37.142260
1675.692359	261345.965533	37.147277
1677.425796	261850.213735	37.152295
1679.067919	262352.241331	37.157312
1681.144660	262859.429976	37.162330
1682.529718	263362.490261	37.167348
1684.186838	263855.852089	37.172365
1685.959949	264375.893210	37.177383
1687.208262	264892.921443	37.182400
1688.977503	265412.378132	37.187418
1690.391983	265930.419586	37.192436
1692.552635	266454.027607	37.197453
1694.365046	266976.905125	37.202471
1695.682355	267494.529216	37.207488
1697.798661	268024.188802	37.212506
1699.538470	268553.071629	37.217524
1701.678622	269073.885714	37.222541
1702.912923	269606.381654	37.227559
1704.677578	270131.905047	37.232576
1706.507953	270651.472537	37.237594
1708.178776	271181.074291	37.242612
1710.264853	271712.054552	37.247629
1711.871213	272237.016487	37.252647
1713.381690	272765.803741	37.257664
1715.348090	273288.494296	37.262682
1716.742881	273816.333395	37.267700
1718.716851	274351.213905	37.272717
1720.403130	274875.624202	37.277735
1722.333496	275412.059240	37.282752
1724.315303	275932.100069	37.287770
1726.189482	276464.249027	37.292788
1727.872712	276982.965090	37.297805
1729.620846	277511.322056	37.302823
1731.211619	278045.952642	37.307840
1733.285641	278564.625763	37.312858
1734.702869	279104.845333	37.317876
1736.528299	279627.341677	37.322893
1738.199810	280153.367494	37.327911
1739.852978	280692.273587	37.332928
1741.594209	281218.005476	37.337946
1743.535768	281752.390108	37.342964
1745.280691	282269.862757	37.347981
1747.228298	282814.581571	37.352999
1749.022084	283339.790354	37.358016
1750.923094	283849.510353	37.363034
1752.579402	284376.719812	37.368052
1754.478107	284880.543822	37.373069
1756.258812	285382.658414	37.378087
1757.557705	285872.302838	37.383104
1759.338697	286377.208185	37.388122
1760.836504	286882.209371	37.393140
1762.435248	287388.360553	37.398157
1764.936319	287897.815391	37.403175
1766.117210	288403.523917	37.408192
1767.859235	288920.491902	37.413210
1769.592493	289434.462109	37.418228
1771.242293	289945.548477	37.423245
1773.087943	290474.024995	37.428263
1774.646577	290987.332110	37.433280
1776.567776	291515.334620	37.438298
1777.815732	292046.621049	37.443316
1779.984806	292575.289269	37.448333
1781.827860	293113.889450	37.453351
1783.226164	293651.214459	37.458368
1785.216515	294182.800553	37.463386
1786.708675	294735.141447	37.468404
1788.594601	295275.477024	37.473421
1790.390395	295824.181134	37.478439
1792.181836	296387.335173	37.483456
1794.033690	296930.538294	37.488474
1795.750582	297490.168432	37.493492
1797.592289	298043.018982	37.498509
1799.693176	298597.677855	37.503527
1801.446059	299158.461353	37.508544
1803.141140	299706.780832	37.513562
1804.740750	300288.485896	37.518580
1806.713168	300847.598133	37.523597
1808.830611	301415.978709	37.528615
1810.235515	301985.641851	37.533632
1812.355486	302546.269005	37.538650
1814.153479	303121.727085	37.543668
1816.029895	303696.965427	37.548685
1817.935811	304262.569848	37.553703
1819.667269	304839.754981	37.558720
1821.909803	305401.994993	37.563738
1823.699360	305981.753463	37.568756
1825.610147	306556.129423	37.573773
1827.605817	307126.678093	37.578791
1829.275227	307703.117808	37.583808
1831.128233	308268.958625	37.588826
1833.012915	308837.228279	37.593844
1834.785290	309405.207762	37.598861
1836.859952	309974.504647	37.603879
1838.685438	310561.208720	37.608896
1840.961074	311123.480537	37.613914
1842.531928	311689.775430	37.618932
1844.339900	312268.876537	37.623949
1846.091689	312850.267986	37.628967
1847.632827	313432.502336	37.633984
1849.938286	314001.782069	37.639002
1851.909559	314583.580826	37.644020
1853.679928	315161.446753	37.649037
1855.883121	315725.473489	37.654055
1857.390389	316306.039933	37.659072
1859.261552	316880.701190	37.664090
1861.273333	317448.224602	37.669108
1863.056413	318033.555762	37.674125
1865.163565	318603.085313	37.679143
1866.775316	319187.012928	37.684160
1868.718272	319754.376202	37.689178
1870.236267	320332.875502	37.694196
1872.338806	320912.111125	37.699213
1874.575737	321485.885757	37.704231
1875.796434	322062.311421	37.709248
1878.188524	322610.735829	37.714266
1879.887272	323171.762056	37.719284
1881.240709	323712.655180	37.724301
1883.668976	324279.187676	37.729319
1885.247880	324832.931921	37.734336
1887.349819	325378.079361	37.739354
1889.047670	325946.012000	37.744372
1890.530127	326500.594899	37.749389
1892.445882	327064.672683	37.754407
1894.125561	327646.454494	37.759424
1896.014428	328211.998343	37.764442
1897.690288	328789.961245	37.769460
1899.282718	329378.036493	37.774477
1901.674793	329955.184028	37.779495
1903.333936	330548.186829	37.784512
1905.265709	331139.818291	37.789530
1907.185364	331738.883824	37.794548
1908.869096	332326.075659	37.799565
1911.254036	332923.528405	37.804583
1912.842483	333521.893123	37.809600
1914.751104	334126.519406	37.814618
1916.868623	334740.319283	37.819636
1918.503982	335340.991547	37.824653
1920.524957	335952.432618	37.829671
1922.146693	336577.690863	37.834688
1924.150445	337183.535878	37.839706
1926.099224	337812.507536	37.844724
1927.951329	338446.361100	37.849741
1929.917618	339065.871841	37.854759
1931.970953	339694.980738	37.859776
1933.928424	340319.274912	37.864794
1936.290501	340955.119524	37.869812
1937.872983	341587.252026	37.874829
1939.863719	342212.988982	37.879847
1941.997267	342866.410629	37.884864
1944.290897	343486.268871	37.889882
1945.918457	344126.330492	37.894900
1947.673557	344763.849822	37.899917
1949.911607	345384.657005	37.904935
1951.516955	346034.569258	37.909952
1953.920073	346668.250336	37.914970
1955.827208	347320.150491	37.919988
1957.769991	347968.787070	37.925005
1959.872175	348612.134839	37.930023
1961.557534	349255.136246	37.935040
1963.749791	349904.744394	37.940058
1965.739790	350552.219438	37.945076
1967.649875	351203.149441	37.950093
1969.666565	351848.317183	37.955111
1971.427502	352510.138828	37.960128
1973.374964	353155.400142	37.965146
1975.255226	353816.192458	37.970164
1977.395004	354476.119735	37.975181
1979.314269	355127.369781	37.980199
1981.186258	355793.207594	37.985216
1983.521650	356453.071669	37.990234
1985.556508	357105.388341	37.995252
1987.413519	357776.753626	38.000269
1989.814026	358423.863778	38.005287
1991.607274	359089.737646	38.010304
1993.539686	359745.200668	38.015322
1995.412573	360402.134373	38.020340
1997.407501	361076.669744	38.025357
1999.653284	361728.014618	38.030375
2001.416615	362389.601692	38.035392
2003.778191	363055.214053	38.040410
2005.655377	363711.838313	38.045428
2007.793617	364360.823165	38.050445
2010.004900	364976.907974	38.055463
2011.795490	365614.285076	38.060480
2013.879349	366239.046294	38.065498
2015.974395	366868.133078	38.070516
2017.920346	367505.909266	38.075533
2019.779113	368129.179631	38.080551
2021.460918	368764.847151	38.085568
2023.545406	369401.806977	38.090586
2025.474691	370041.038840	38.095604
2027.388222	370694.339262	38.100621
2029.635730	371338.289660	38.105639
2031.586159	371984.611044	38.110656
2033.489112	372640.921593	38.115674
2035.496924	373303.949156	38.120692
2037.145942	373955.154196	38.125709
2039.295167	374620.416320	38.130727
2040.974599	375301.492527	38.135744
2043.472490	375968.827124	38.140762
2045.393732	376640.403106	38.145780
2047.674117	377327.198467	38.150797
2049.562342	377998.930877	38.155815
2051.312613	378688.246222	38.160832
2053.591264	379365.237802	38.165850
2055.383994	380054.568983	38.170868
2057.330690	380750.098357	38.175885
2059.626232	381439.520809	38.180903
2061.363616	382151.004544	38.185920
2063.268164	382858.870221	38.190938
2065.662380	383556.700711	38.195956
2067.686227	384282.999398	38.200973
2069.284931	384978.724830	38.205991
2071.409641	385708.194705	38.211008
2073.715252	386425.778492	38.216026
2076.177693	387151.813086	38.221044
2077.663174	387869.651714	38.226061
2080.263488	388594.971201	38.231079
2082.356506	389322.841923	38.236096
2084.164363	390045.444635	38.241114
2086.454432	390785.796517	38.246132
2088.630107	391530.053103	38.251149
2090.478629	392250.290613	38.256167
2092.704999	392978.483732	38.261184
2095.060163	393724.203176	38.266202
2097.251303	394463.341290	38.271220
2099.334452	395195.534376	38.276237
2101.443954	395936.626397	38.281255
2103.918226	396683.899605	38.286272
2106.008222	397416.948982	38.291290
2108.108239	398149.243412	38.296308
2110.050159	398892.189184	38.301325
2112.239514	399631.603286	38.306343
2114.753493	400369.018928	38.311360
2116.515336	401102.713395	38.316378
2118.853330	401852.181704	38.321396
2120.520423	402593.201787	38.326413
2122.670462	403326.318556	38.331431
2124.766778	404089.120507	38.336448
2126.852628	404825.755839	38.341466
2129.266769	405568.043396	38.346484
2131.104092	406336.552327	38.351501
2133.784794	407079.895254	38.356519
2135.575928	407830.128980	38.361536
2137.623826	408581.895639	38.366554
2139.909200	409326.711763	38.371572
2141.992138	410090.032968	38.376589
2144.214390	410845.634101	38.381607
2146.229873	411594.307416	38.386624
2148.254202	412333.991426	38.391642
2150.735710	413058.508487	38.396660
2152.498455	413800.119508	38.401677
2154.681023	414505.624349	38.406695
2156.857071	415230.435588	38.411712
2159.118683	415957.415804	38.416730
2161.194272	416686.558895	38.421748
2163.177558	417422.635491	38.426765
2165.316898	418159.500814	38.431783
2167.144699	418895.206008	38.436800
2169.146608	419634.558172	38.441818
2171.603890	420380.802291	38.446836
2173.314189	421128.337578	38.451853
2175.426715	421887.836538	38.456871
2177.725165	422647.813294	38.461888
2179.582639	423407.839470	38.466906
2181.793081	424183.075938	38.471924
2183.836371	424971.024639	38.476941
2185.878263	425741.024162	38.481959
2188.273099	426514.586420	38.486976
2190.381700	427313.789571	38.491994
2192.818174	428099.293192	38.497012
2194.931534	428895.202659	38.502029
2197.025337	429689.772507	38.507047
2199.076320	430491.258060	38.512064
2201.458421	431290.636882	38.517082
2203.583060	432088.107437	38.522100
2205.453867	432911.609967	38.527117
2207.650489	433726.424909	38.532135
2210.090176	434543.853562	38.537152
2211.919193	435380.890178	38.542170
2214.583315	436198.931445	38.547188
2216.341524	437030.706499	38.552205
2218.738117	437864.876032	38.557223
2220.864800	438691.873466	38.562240
2222.984380	439539.791141	38.567258
2225.380737	440373.867618	38.572276
2227.748938	441221.579178	38.577293
2230.137932	442062.019537	38.582311
2232.624194	442901.197547	38.587328
2234.586776	443748.474199	38.592346
2237.102065	444594.564382	38.597364
2239.570075	445450.291966	38.602381
2241.943258	446290.218228	38.607399
2244.024818	447134.307866	38.612416
2246.295645	447977.978983	38.617434
2248.600361	448829.451249	38.622452
2250.854689	449684.185370	38.627469
2253.095746	450533.627158	38.632487
2255.115348	451391.618411	38.637504
2257.419111	452251.500015	38.642522
2260.054709	453098.851031	38.647540
2262.418937	453970.889807	38.652557
2264.529020	454818.459558	38.657575
2266.950452	455675.095229	38.662592
2268.700442	456543.081329	38.667610
2271.317832	457389.601539	38.672628
2273.770473	458259.623196	38.677645
2275.792486	459120.072893	38.682663
2278.178527	459976.179256	38.687680
2280.130712	460850.215939	38.692698
2282.706394	461701.515914	38.697716
2284.944438	462585.438098	38.702733
2287.045106	463451.349503	38.707751
2289.591949	464325.539329	38.712768
2291.644177	465206.190473	38.717786
2293.892079	466070.092051	38.722804
2296.181603	466937.940741	38.727821
2298.396584	467801.720166	38.732839
2300.642099	468660.857523	38.737856
2302.713253	469507.302413	38.742874
2304.970499	470350.647533	38.747892
2307.146904	471198.162216	38.752909
2309.396965	472048.557195	38.757927
2311.758564	472916.324946	38.762944
2313.964543	473783.421635	38.767962
2316.289026	474649.498861	38.772980
2318.389722	475522.594147	38.777997
2320.831781	476385.085869	38.783015
2323.130463	477262.309501	38.788032
2325.360947	478133.189408	38.793050
2327.359823	479021.944471	38.798068
2329.683759	479903.633557	38.803085
2331.839465	480784.398741	38.808103
2333.871774	481682.108210	38.813120
2336.741184	482595.691882	38.818138
2339.237477	483498.283676	38.823156
2341.629638	484406.350407	38.828173
2343.675002	485321.092266	38.833191
2346.029652	486233.312793	38.838208
2348.365842	487140.491741	38.843226
2350.793739	488057.048235	38.848244
2353.135281	488982.707137	38.853261
2355.505993	489915.681195	38.858279
2357.623043	490844.155258	38.863296
2359.656706	491784.251266	38.868314
2362.045208	492727.517702	38.873332
2364.382945	493664.533952	38.878349
2366.782715	494622.580480	38.883367
2369.619130	495578.886508	38.888384
2371.378342	496542.228472	38.893402
2374.127916	497493.395401	38.898420
2376.378555	498464.769866	38.903437
2378.727628	499426.537790	38.908455
2381.286180	500392.805915	38.913472
2383.525520	501368.401684	38.918490
2385.960929	502333.870914	38.923508
2388.762601	503304.165572	38.928525
2390.723719	504291.334651	38.933543
2393.572277	505260.497111	38.938560
2396.064587	506242.165719	38.943578
2398.480362	507222.879959	38.948596
2401.015882	508199.431073	38.953613
2403.346249	509193.349714	38.958631
2406.089321	510165.159276	38.963648
2408.373511	511144.395362	38.968666
2410.959249	512123.823782	38.973684
2413.265749	513107.269819	38.978701
2415.732639	514093.601571	38.983719
2418.105800	515065.524060	38.988736
2420.590817	516065.486704	38.993754
2422.967569	517045.549651	38.998772
2425.312740	518049.741200	39.003789
2427.792915	519023.766698	39.008807
2430.437526	520020.475004	39.013824
2432.655028	521010.992692	39.018842
2435.106626	522004.429893	39.023860
2437.741071	522999.786832	39.028877
2440.102118	523986.359730	39.033895
2442.825726	524974.822846	39.038912
2445.193401	525979.344462	39.043930
2447.678258	526963.082883	39.048948
2450.234405	527953.491988	39.053965
2452.620054	528945.575107	39.058983
2455.204045	529943.650927	39.064000
2457.463858	530936.980448	39.069018
2459.987576	531912.731447	39.074036
2462.369676	532881.997722	39.079053
2464.552329	533836.384269	39.084071
2466.940495	534797.569383	39.089088
2469.504475	535759.567547	39.094106
2471.599407	536718.358270	39.099124
2474.195733	537688.324212	39.104141
2476.134969	538661.502773	39.109159
2478.463638	539630.777271	39.114176
2480.626771	540620.539149	39.119194
2483.452919	541608.663628	39.124212
2485.927558	542604.875545	39.129229
2488.166431	543608.650852	39.134247
2490.630080	544612.920701	39.139264
2492.989292	545625.081540	39.144282
2495.300338	546635.969758	39.149300
2497.390581	547662.810920	39.154317
2500.261825	548692.011146	39.159335
2502.682939	549715.929588	39.164352
2505.039217	550771.604709	39.169370
2508.029736	551799.295017	39.174388
2510.562379	552837.136688	39.179405
2513.076801	553889.226234	39.184423
2515.789875	554931.099352	39.189440
2518.039028	555981.059034	39.194458
2520.415736	557027.950704	39.199476
2523.108224	558098.675129	39.204493
2525.547936	559159.256589	39.209511
2528.169526	560221.129791	39.214528
2530.637169	561305.145952	39.219546
2533.640623	562359.851636	39.224564
2536.284196	563435.977777	39.229581
2538.453723	564517.617676	39.234599
2541.492751	565589.332416	39.239616
2543.733230	566671.333543	39.244634
2546.312459	567748.267721	39.249652
2548.902306	568828.473636	39.254669
2551.535359	569917.165500	39.259687
2554.038887	571005.384335	39.264704
2556.451588	572091.667994	39.269722
2559.262810	573182.159054	39.274740
2561.652678	574273.880000	39.279757
2564.292786	575372.238965	39.284775
2567.161827	576470.012363	39.289792
2569.877950	577577.798478	39.294810
2572.241809	578661.465042	39.299828
2575.088051	579776.407805	39.304845
2577.369543	580885.073633	39.309863
2580.032722	581984.649737	39.314880
2582.231057	583101.354084	39.319898
2585.304560	584202.518697	39.324916
2588.043638	585302.886803	39.329933
2590.178815	586422.355373	39.334951
2592.802871	587529.959745	39.339968
2595.510093	588654.390343	39.344986
2597.984566	589772.338750	39.350004
2600.890603	590884.949684	39.355021
2603.420301	592010.948158	39.360039
2605.869374	593127.934485	39.365056
2608.354160	594258.787376	39.370074
2610.827742	595384.173440	39.375092
2613.641373	596509.245320	39.380109
2616.136570	597628.952491	39.385127
2618.837870	598766.246764	39.390144
2621.675858	599902.505821	39.395162
2624.124721	601027.852166	39.400180
2626.989972	602157.676230	39.405197
2629.458507	603291.309412	39.410215
2631.851272	604402.067365	39.415232
2634.603841	605511.656899	39.420250
2637.093266	606599.461438	39.425268
2639.926519	607689.256726	39.430285
2642.295523	608799.388526	39.435303
2645.099644	609899.632969	39.440320
2648.013710	610992.397469	39.445338
2650.829357	612090.774003	39.450356
2653.720829	613186.528984	39.455373
2655.970799	614298.485720	39.460391
2658.414692	615385.445260	39.465408
2660.725888	616498.470908	39.470426
2663.539662	617605.001454	39.475444
2666.311407	618727.324798	39.480461
2668.801936	619857.427246	39.485479
2671.081221	620981.349543	39.490496
2673.662272	622118.249583	39.495514
2676.231998	623265.426078	39.500532
2679.087614	624411.084324	39.505549
2681.166193	625574.834327	39.510567
2683.907075	626729.956236	39.515584
2686.539808	627908.796971	39.520602
2689.189186	629083.908372	39.525620
2692.128860	630254.596883	39.530637
2694.549798	631442.667835	39.535655
2697.084417	632637.575818	39.540672
2699.768468	633829.427650	39.545690
2702.101050	635029.687308	39.550708
2705.529916	636233.920205	39.555725
2707.912714	637456.051668	39.560743
2710.558508	638665.870167	39.565760
2713.114713	639887.635495	39.570778
2715.953599	641107.662492	39.575796
2718.925987	642328.220465	39.580813
2721.305289	643568.729953	39.585831
2724.096001	644807.723730	39.590848
2727.390693	646035.363641	39.595866
2729.649746	647284.164139	39.600884
2732.917066	648516.691442	39.605901
2735.380209	649762.308831	39.610919
2738.520123	651005.815405	39.615936
2741.235893	652255.664925	39.620954
2743.897469	653495.600298	39.625972
2746.948238	654736.810643	39.630989
2749.367148	655990.222796	39.636007
2752.659342	657240.043833	39.641024
2755.291934	658482.443713	39.646042
2758.269972	659739.566476	39.651060
2761.517460	660979.952990	39.656077
2764.310047	662236.534012	39.661095
2766.884304	663474.123147	39.666112
2769.936719	664721.676714	39.671130
2772.180286	665973.679931	39.676148
2775.435577	667219.033530	39.681165
2777.983943	668473.842837	39.686183
2780.776267	669712.280093	39.691200
2783.611061	670973.426460	39.696218
2786.176998	672227.039029	39.701236
2789.116014	673490.765063	39.706253
2791.967268	674747.723034	39.711271
2794.528461	676003.615203	39.716288
2797.556640	677255.384198	39.721306
2800.039255	678522.628759	39.726324
2803.244387	679781.034167	39.731341
2805.841275	681034.499257	39.736359
2808.384836	682292.918582	39.741376
2811.593659	683552.396277	39.746394
2813.923980	684828.878631	39.751412
2817.035095	686082.957166	39.756429
2819.615915	687312.076475	39.761447
2822.160660	688539.148230	39.766464
2825.347437	689766.542578	39.771482
2827.530432	691007.036125	39.776500
2830.606597	692227.461780	39.781517
2833.375826	693468.559002	39.786535
2835.934344	694705.896546	39.791552
2838.832197	695950.296554	39.796570
2841.125104	697212.275899	39.801588
2844.028725	698463.065099	39.806605
2846.992916	699731.415053	39.811623
2849.419085	701002.247619	39.816640
2852.350841	702274.992546	39.821658
2854.813874	703566.757168	39.826676
2857.770948	704846.306646	39.831693
2860.267303	706145.063741	39.836711
2862.999636	707447.846028	39.841728
2865.928630	708755.647993	39.846746
2868.863303	710086.770476	39.851764
2871.661424	711403.003033	39.856781
2874.550620	712736.045869	39.861799
2876.843962	714076.253045	39.866816
2879.953882	715417.597563	39.871834
2883.048677	716778.572063	39.876852
2885.797559	718123.502511	39.881869
2888.625911	719483.685585	39.886887
2891.519524	720857.928472	39.891904
2894.692822	722217.805484	39.896922
2897.244654	723602.281000	39.901940
2900.269334	724966.278609	39.906957
2903.320100	726356.140651	39.911975
2906.189090	727737.890752	39.916992
2909.542796	729121.995109	39.922010
2912.128161	730515.771434	39.927028
2915.353026	731912.511964	39.932045
2918.125200	733309.234018	39.937063
2921.128204	734697.480329	39.942080
2923.962043	736107.184909	39.947098
2926.780709	737518.716658	39.952116
2929.544402	738906.470031	39.957133
2932.941266	740330.287382	39.962151
2935.744264	741748.520805	39.967168
2938.948648	743162.339981	39.972186
2941.708134	744580.465833	39.977204
2944.769816	745991.827148	39.982221
2947.538425	747424.769238	39.987239
2950.712353	748843.976106	39.992256
2953.836479	750270.717229	39.997274
2956.666659	751697.440982	40.002292
2959.846668	753120.641687	40.007309
2962.594278	754547.146863	40.012327
2965.457005	755993.111886	40.017344
2968.802761	757405.297704	40.022362
2971.612364	758853.535268	40.027380
2974.733462	760286.534679	40.032397
2977.810208	761710.512315	40.037415
2980.774302	763148.701783	40.042432
2983.891243	764587.722041	40.047450
2986.693057	766028.189676	40.052468
2989.849114	767461.634926	40.057485
2992.784769	768889.777641	40.062503
2995.360991	770342.915347	40.067520
2998.631661	771781.453317	40.072538
3001.838319	773218.984169	40.077556
3004.718444	774655.207003	40.082573
3007.738211	776096.379358	40.087591
3010.715228	777535.015797	40.092608
3014.045623	778965.112181	40.097626
3016.512584	780377.548694	40.102644
3019.834481	781768.126219	40.107661
3022.936492	783163.769802	40.112679
3025.646685	784564.160630	40.117696
3028.876033	785951.540241	40.122714
3031.620171	787352.065955	40.127732
3034.556523	788738.853244	40.132749
3037.576402	790152.604820	40.137767
3040.237213	791564.810031	40.142784
3043.647498	792968.084711	40.147802
3046.592333	794398.388632	40.152820
3049.943445	795821.869661	40.157837
3052.530309	797254.733687	40.162855
3055.540531	798685.128297	40.167872
3058.497537	800119.396785	40.172890
3061.335135	801579.809396	40.177908
3064.258086	803024.782902	40.182925
3067.286113	804485.232866	40.187943
3070.054488	805955.291839	40.192960
3073.237531	807432.397074	40.197978
3076.244223	808932.036379	40.202996
3079.227945	810420.109121	40.208013
3082.226662	811917.769741	40.213031
3085.129635	813423.417122	40.218048
3088.467787	814922.014339	40.223066
3091.239496	816432.038309	40.228084
3094.440771	817961.418619	40.233101
3097.285114	819489.725703	40.238119
3100.297489	821027.898755	40.243136
3103.154363	822559.886569	40.248154
3106.236010	824111.377787	40.253172
3109.681639	825665.270498	40.258189
3112.972716	827216.431687	40.263207
3115.678917	828789.249587	40.268224
3118.971472	830349.167431	40.273242
3121.798719	831928.074835	40.278260
3125.061129	833499.464122	40.283277
3128.223884	835078.568036	40.288295
3131.385857	836671.349792	40.293312
3134.874708	838251.954487	40.298330
3137.585399	839837.987514	40.303348
3140.703107	841432.214893	40.308365
3143.813092	843034.697331	40.313383
3147.205697	844642.657084	40.318400
3150.459120	846240.801109	40.323418
3153.958220	847839.274956	40.328436
3156.842997	849443.950229	40.333453
3160.218700	851058.911896	40.338471
3163.076352	852672.082688	40.343488
3166.643732	854283.163139	40.348506
3169.433573	855902.393999	40.353524
3172.842335	857501.013691	40.358541
3176.079942	859124.560073	40.363559
3179.246541	860751.080651	40.368576
3182.311053	862364.872059	40.373594
3185.722968	863993.780658	40.378612
3188.888571	865613.764975	40.383629
3192.279834	867230.661584	40.388647
3195.529713	868857.604975	40.393664
3198.646675	870472.317444	40.398682
3201.852599	872104.967766	40.403700
3205.151600	873725.253586	40.408717
3208.876984	875353.345511	40.413735
3211.698680	876967.599259	40.418752
3215.006368	878583.941123	40.423770
3218.140569	880209.145437	40.428788
3221.378749	881824.025735	40.433805
3224.775965	883432.057473	40.438823
3227.964229	885037.264848	40.443840
3230.686635	886589.873401	40.448858
3233.874429	888169.689540	40.453876
3236.966549	889734.807325	40.458893
3239.997886	891319.573871	40.463911
3242.969500	892897.643110	40.468928
3246.340105	894486.105119	40.473946
3248.999693	896093.903705	40.478964
3252.039848	897693.475245	40.483981
3255.490783	899305.146075	40.488999
3258.409708	900925.592620	40.494016
3261.785854	902547.036955	40.499034
3264.775448	904183.378994	40.504052
3267.563733	905839.384471	40.509069
3270.878405	907483.748573	40.514087
3273.436858	909155.540608	40.519104
3276.967146	910811.382007	40.524122
3279.759120	912495.486410	40.529140
3283.361493	914196.714639	40.534157
3286.956592	915889.924021	40.539175
3289.970572	917602.674618	40.544192
3293.358680	919303.786153	40.549210
3296.571624	921008.038957	40.554228
3299.614111	922725.211497	40.559245
3303.328372	924450.931449	40.564263
3305.972929	926197.937313	40.569280
3309.633513	927940.180441	40.574298
3312.990833	929685.257073	40.579316
3315.739417	931435.223789	40.584333
3319.568257	933192.954651	40.589351
3322.897138	934954.871851	40.594368
3326.137463	936722.814702	40.599386
3329.769686	938487.514504	40.604404
3332.979216	940257.806598	40.609421
3336.590490	942035.363166	40.614439
3339.658946	943817.463854	40.619456
3343.217807	945590.082994	40.624474
3346.770252	947379.756235	40.629492
3349.879338	949163.916023	40.634509
3353.119010	950940.563143	40.639527
3356.696362	952754.858666	40.644544
3360.078799	954586.167020	40.649562
3363.684278	956436.026464	40.654580
3366.850562	958282.138856	40.659597
3370.464849	960125.827035	40.664615
3373.360701	961977.739175	40.669632
3376.847341	963831.106944	40.674650
3380.299975	965685.347593	40.679668
3383.271978	967554.881854	40.684685
3386.868566	969410.238602	40.689703
3390.872240	971285.217815	40.694720
3393.851299	973142.882281	40.699738
3397.297951	975003.084013	40.704756
3400.346043	976875.999947	40.709773
3404.211901	978743.199126	40.714791
3407.254596	980625.894960	40.719808
3410.640878	982496.425134	40.724826
3414.407201	984378.444415	40.729844
3417.217048	986259.221112	40.734861
3420.721864	988126.909958	40.739879
3424.095414	990036.592350	40.744896
3427.454551	991913.852773	40.749914
3431.170838	993802.481643	40.754932
3434.377863	995688.622877	40.759949
3437.811435	997574.487396	40.764967
3440.976109	999465.786070	40.769984
3444.359471	1001361.559113	40.775002
3447.821629	1003242.763660	40.780007
3450.828828	1005074.903833	40.785012
3454.723756	1006850.518352	40.790016
3457.757655	1008558.191981	40.795021
3460.798360	1010190.655557	40.800026
3463.864519	1011760.496975	40.805031
3466.623197	1013262.386819	40.810036
3470.177334	1014690.471491	40.815040
3472.796919	1016043.539387	40.820045
3475.685445	1017307.186507	40.825050
3478.224558	1018499.032142	40.830055
3480.824478	1019627.587272	40.835060
3483.304838	1020672.657735	40.840064
3485.535376	1021666.880146	40.845069
3487.772106	1022567.790985	40.850074
3490.058539	1023412.734574	40.855079
3491.673213	1024199.626664	40.860084
3493.954011	1024912.674699	40.865088
3495.751454	1025579.605136	40.870093
3497.272040	1026176.768665	40.875098
3499.306446	1026731.173280	40.880103
3500.571738	1027227.549657	40.885108
3502.315291	1027667.063369	40.890112
3503.467280	1028082.822531	40.895117
3504.663992	1028433.776038	40.900122
3506.365892	1028742.319599	40.905127
3507.325630	1029012.731427	40.910132
3508.764912	1029229.908826	40.915136
3509.712787	1029427.122087	40.920141
3510.571587	1029576.914758	40.925146
3512.004567	1029696.797345	40.930151
3512.873255	1029778.345074	40.935156
3513.543207	1029831.855780	40.940160
3514.374669	1029866.852930	40.945165
3515.206803	1029859.650380	40.950170
3516.004618	1029813.254186	40.955175
3516.402240	1029774.376318	40.960180
3517.474360	1029693.186447	40.965184
3517.929326	1029586.059902	40.970189
3518.477991	1029477.851129	40.975194
3519.242353	1029331.466818	40.980199
3519.379896	1029179.664348	40.985204
3520.098277	1028994.752379	40.990208
3520.420039	1028809.318789	40.995213
3520.518464	1028598.454919	41.000218
3521.273907	1028377.987130	41.005223
3521.298857	1028147.368322	41.010228
3521.868243	1027897.285951	41.015232
3522.334420	1027637.526754	41.020237
3522.563148	1027372.081567	41.025242
3523.052112	1027079.757363	41.030247
3522.923521	1026785.292250	41.035252
3523.782801	1026476.799842	41.040256
3523.825198	1026163.194975	41.045261
3524.062381	1025836.561512	41.050266
3524.599621	1025499.204561	41.055271
3524.520811	1025161.347524	41.060276
3524.682350	1024806.477290	41.065280
3524.787501	1024451.400060	41.070285
3524.902591	1024098.914620	41.075290
3525.059263	1023734.094585	41.080295
3524.901300	1023364.166868	41.085300
3525.602635	1022984.770069	41.090304
3525.385486	1022602.203801	41.095309
3525.422086	1022207.163767	41.100314
3525.717557	1021817.384215	41.105319
3525.563698	1021434.049193	41.110324
3525.672224	1021030.384099	41.115328
3525.967847	1020625.010981	41.120333
3525.893497	1020222.868993	41.125338
3526.030952	1019810.676177	41.130343
3526.171013	1019412.513121	41.135348
3526.282823	1018990.470353	41.140352
3526.134353	1018579.688764	41.145357
3525.911403	1018148.715313	41.150362
3525.983595	1017732.112832	41.155367
3525.925129	1017313.754844	41.160372
3526.380184	1016880.923216	41.165376
3526.281338	1016464.254778	41.170381
3526.387267	1016025.302437	41.175386
3526.455794	1015593.987701	41.180391
3526.344485	1015162.863546	41.185396
3526.526858	1014720.206031	41.190400
3526.064678	1014295.090162	41.195405
3526.338289	1013854.096412	41.200410
3526.229375	1013415.752036	41.205415
3525.847182	1012996.931553	41.210420
3526.075563	1012547.979326	41.215424
3525.762044	1012118.596638	41.220429
3525.834426	1011681.446505	41.225434
3525.783815	1011235.834088	41.230439
3525.691786	1010807.868620	41.235444
3525.647708	1010367.722079	41.240448
3525.515356	1009946.593643	41.245453
3525.451806	1009504.245885	41.250458
3525.602277	1009070.377110	41.255463
3525.381716	1008640.713700	41.260468
3525.436762	1008207.279945	41.265472
3525.544400	1007775.553244	41.270477
3525.297036	1007340.742280	41.275482
3525.730498	1006892.568466	41.280487
3525.376642	1006472.674568	41.285492
3525.649746	1006015.126975	41.290496
3525.677094	1005585.092570	41.295501
3525.378245	1005147.885206	41.300506
3525.246469	1004701.380279	41.305511
3524.911965	1004264.596461	41.310516
3525.049622	1003824.978398	41.315520
3525.072416	1003397.597947	41.320525
3525.082511	1002967.561424	41.325530
3525.439577	1002521.387071	41.330535
3525.245750	1002088.496675	41.335540
3525.424813	1001644.325021	41.340544
3525.122815	1001199.808579	41.345549
3524.694023	1000767.633973	41.350554
3524.662481	1000320.279680	41.355559
3524.674220	999889.716768	41.360564
3525.014861	999457.315268	41.365568
3524.785959	999023.320103	41.370573
3524.653702	998587.037182	41.375578
3524.700653	998143.001594	41.380583
3524.157982	997724.532197	41.385588
3524.494517	997281.354758	41.390592
3524.330885	996856.333619	41.395597
3524.143952	996421.840002	41.400602
3524.307364	995994.850414	41.405607
3523.985628	995573.069710	41.410612
3524.032916	995134.738380	41.415616
3523.783524	994708.596381	41.420621
3523.984244	994297.640295	41.425626
3524.255316	993861.803547	41.430631
3523.740911	993437.460457	41.435636
3523.730365	992994.589486	41.440640
3523.589861	992573.432591	41.445645
3523.359919	992159.664502	41.450650
3523.840841	991743.507899	41.455655
3523.382416	991311.493278	41.460660
3523.730671	990872.783044	41.465664
3523.286295	990473.741400	41.470669
3523.012675	990051.639626	41.475674
3523.429201	989632.707183	41.480679
3523.231060	989219.791952	41.485684
3523.453589	988795.077897	41.490688
3523.156956	988381.045511	41.495693
3523.054689	987962.758009	41.500698
3522.940460	987547.562277	41.505703
3522.687345	987134.602187	41.510708
3522.966007	986716.355336	41.515712
3523.009385	986298.994365	41.520717
3522.763221	985894.136378	41.525722
3522.968620	985471.518120	41.530727
3522.624374	985065.251605	41.535732
3522.684247	984646.108234	41.540736
3522.509262	984245.511828	41.545741
3522.476177	983827.982342	41.550746
3522.420435	983423.210066	41.555751
3522.155031	983029.862202	41.560756
3522.465888	982612.186996	41.565760
3522.341279	982215.343668	41.570765
3522.353608	981808.102895	41.575770
3522.238050	981394.606251	41.580775
3521.954781	980989.112917	41.585780
3522.122990	980588.202954	41.590784
3521.616161	980193.625220	41.595789
3521.762714	979788.268682	41.600794
3521.957899	979378.187803	41.605799
3521.864349	978985.606950	41.610804
3522.082661	978577.418053	41.615808
3521.786940	978183.936368	41.620813
3521.543654	977778.989835	41.625818
3521.979757	977378.103424	41.630823
3521.753134	976987.458711	41.635828
3521.264815	976582.174647	41.640832
3521.539977	976183.282783	41.645837
3521.065949	975793.281210	41.650842
3521.139107	975399.449330	41.655847
3520.793911	975020.807720	41.660852
3520.792223	974625.664393	41.665856
3521.087677	974241.783286	41.670861
3520.865008	973855.615753	41.675866
3521.276283	973463.256711	41.680871
3521.065770	973075.665952	41.685876
3520.902833	972681.685955	41.690880
3520.658475	972310.083513	41.695885
3520.384592	971921.447298	41.700890
3520.403340	971533.910009	41.705895
3520.149028	971163.995115	41.710900
3520.563578	970788.566934	41.715904
3520.146799	970409.240895	41.720909
3520.258711	970027.944135	41.725914
3520.230316	969650.068967	41.730919
3520.237594	969284.489593	41.735924
3520.298038	968900.778476	41.740928
3520.065025	968530.298816	41.745933
3519.962766	968150.282339	41.750938
3519.868316	967773.468650	41.755943
3519.712121	967413.081183	41.760948
3519.821595	967027.964586	41.765952
3520.152226	966665.296894	41.770957
3519.688796	966297.843090	41.775962
3519.725187	965929.989775	41.780967
3519.439732	965555.313402	41.785972
3519.910962	965189.103110	41.790976
3519.896491	964821.187205	41.795981
3519.396276	964451.957004	41.800986
3519.494942	964088.773282	41.805991
3519.306739	963724.928412	41.810996
3519.747323	963354.493509	41.816000
3519.608546	962984.717827	41.821005
3519.531941	962625.975728	41.826010
3519.629966	962252.979830	41.831015
3519.235493	961900.023863	41.836020
3518.924934	961519.603121	41.841024
3518.772938	961169.207367	41.846029
3518.467344	960814.602711	41.851034
3518.733911	960463.703182	41.856039
3518.893129	960112.701981	41.861044
3519.044206	959757.369094	41.866048
3518.597983	959408.972556	41.871053
3518.458134	959057.172344	41.876058
3518.614906	958698.441098	41.881063
3518.348614	958354.557641	41.886068
3518.520385	957999.897128	41.891072
3518.242172	957654.797637	41.896077
3517.929287	957321.055092	41.901082
3518.186351	956963.964030	41.906087
3517.950934	956631.149204	41.911092
3518.159274	956286.770120	41.916096
3517.940193	955950.775729	41.921101
3517.673388	955614.867702	41.926106
3517.619074	955274.001712	41.931111
3517.358035	954939.818681	41.936116
3517.641961	954600.524472	41.941120
3517.474585	954278.351518	41.946125
3517.546725	953952.099420	41.951130
3517.600656	953612.588901	41.956135
3517.563330	953278.665291	41.961140
3517.430203	952938.263054	41.966144
3517.520898	952620.173760	41.971149
3517.196180	952295.879557	41.976154
3517.111684	951973.624686	41.981159
3517.382117	951654.446997	41.986164
3517.380975	951324.199376	41.991168
3517.133603	951011.474873	41.996173
3516.937683	950694.322558	42.001178
3517.180862	950379.182756	42.006183
3516.685490	950061.179489	42.011188
3516.937007	949746.477633	42.016192
3516.979794	949439.540826	42.021197
3516.745450	949128.325439	42.026202
3516.882843	948816.934200	42.031207
3516.488524	948502.357943	42.036212
3516.573092	948198.784975	42.041216
3516.457213	947893.695733	42.046221
3516.251995	947584.104521	42.051226
3516.436518	947279.407853	42.056231
3516.287448	946974.939528	42.061236
3516.538194	946662.058708	42.066240
3516.485792	946360.792953	42.071245
3516.315990	946052.443972	42.076250
3516.266058	945759.855195	42.081255
3515.718415	945454.405091	42.086260
3516.060425	945151.280058	42.091264
3515.930844	944858.461729	42.096269
3515.688039	944568.901618	42.101274
3515.793026	944260.208655	42.106279
3515.557786	943978.467799	42.111284
3515.720679	943680.074979	42.116288
3515.751805	943377.088644	42.121293
3515.310158	943094.375718	42.126298
3515.594248	942797.636418	42.131303
3515.340982	942515.435675	42.136308
3515.533692	942220.882001	42.141312
3515.458810	941947.148332	42.146317
3514.960179	941660.917143	42.151322
3515.171578	941369.090944	42.156327
3515.043422	941080.658505	42.161332
3515.064344	940796.402450	42.166336
3514.821353	940526.742743	42.171341
3514.674986	940247.276476	42.176346
3515.086062	939963.677469	42.181351
3515.012152	939698.931494	42.186356
3515.018487	939409.329833	42.191360
3514.952156	939127.873049	42.196365
3514.864541	938851.869493	42.201370
3514.947446	938573.042720	42.206375
3514.877654	938306.307801	42.211380
3514.840714	938018.553834	42.216384
3514.676608	937752.573327	42.221389
3514.114212	937470.821312	42.226394
3514.514881	937206.254408	42.231399
3514.209542	936935.652186	42.236404
3514.431127	936654.206633	42.241408
3514.129365	936396.812350	42.246413
3514.109115	936136.385378	42.251418
3514.222985	935856.065859	42.256423
3513.776292	935609.784748	42.261428
3513.944105	935341.516651	42.266432
3514.064310	935084.276324	42.271437
3513.832808	934819.117579	42.276442
3514.082195	934553.386477	42.281447
3513.515159	934301.882404	42.286452
3513.704072	934039.877739	42.291456
3513.539218	933775.039286	42.296461
3513.730269	933528.747633	42.301466
3513.638844	933264.735210	42.306471
3513.499876	933016.554469	42.311476
3513.417852	932761.825591	42.316480
3513.430712	932501.885268	42.321485
3513.294481	932250.212380	42.326490
3513.712688	932002.852194	42.331495
3513.389244	931756.754690	42.336500
3513.257159	931502.069375	42.341504
3513.283125	931255.602980	42.346509
3512.633646	931006.163803	42.351514
3512.920825	930756.366526	42.356519
3512.752611	930521.132649	42.361524
3512.635701	930286.264015	42.366528
3512.995882	930038.917760	42.371533
3512.659275	929801.662980	42.376538
3513.013099	929548.916703	42.381543
3512.717808	929319.317163	42.386548
3513.083551	929074.326332	42.391552
3512.886266	928825.958896	42.396557
3512.763923	928584.291886	42.401562
3512.735207	928335.393482	42.406567
3512.729102	928112.034617	42.411572
3512.476240	927869.780271	42.416576
3512.256628	927627.797678	42.421581
3512.426454	927402.554602	42.426586
3512.518980	927164.054649	42.431591
3512.232617	926936.945326	42.436596
3512.831410	926701.224066	42.441600
3512.414139	926470.849227	42.446605
3512.151205	926234.384447	42.451610
3512.162769	925996.999010	42.456615
3511.730398	925776.111495	42.461620
3511.654104	925540.161963	42.466624
3512.043655	925317.582255	42.471629
3511.800710	925107.689871	42.476634
3511.887353	924874.183420	42.481639
3511.497086	924655.838259	42.486644
3511.623246	924438.264362	42.491648
3511.610525	924221.665936	42.496653
3511.181275	924007.819440	42.501658
3511.359458	923788.864642	42.506663
3511.102780	923574.299421	42.511668
3511.191833	923360.341771	42.516672
3511.305872	923148.390854	42.521677
3511.128489	922943.403380	42.526682
3510.961506	922731.482343	42.531687
3511.225700	922519.770446	42.536692
3511.130396	922312.629676	42.541696
3511.117056	922103.832408	42.546701
3511.028344	921902.060771	42.551706
3511.240103	921683.207189	42.556711
3510.633591	921481.120369	42.561716
3511.077285	921276.159552	42.566720
3510.874709	921063.601674	42.571725
3511.075373	920868.092721	42.576730
3510.614536	920659.313305	42.581735
3510.653910	920459.198333	42.586740
3510.225828	920252.418171	42.591744
3510.599451	920052.329299	42.596749
3510.522512	919870.300110	42.601754
3510.570190	919670.347044	42.606759
3510.564928	919472.512279	42.611764
3510.465440	919265.832755	42.616768
3510.464666	919069.041046	42.621773
3510.090217	918884.910657	42.626778
3510.256884	918686.345237	42.631783
3510.066281	918498.129384	42.636788
3510.209933	918296.858720	42.641792
3510.092329	918107.173599	42.646797
3509.817771	917927.229247	42.651802
3509.934755	917738.262625	42.656807
3509.845430	917561.933396	42.661812
3510.007908	917358.603454	42.666816
3510.286516	917187.784727	42.671821
3509.965433	916995.013832	42.676826
3510.023318	916805.735764	42.681831
3509.721706	916613.525792	42.686836
3509.534285	916427.355823	42.691840
3509.824048	916248.129502	42.696845
3509.563834	916075.535315	42.701850
3509.780515	915887.450919	42.706855
3509.677645	915709.427056	42.711860
3509.625099	915528.018769	42.716864
3509.680872	915359.586869	42.721869
3509.580742	915171.530011	42.726874
3509.780523	914989.773381	42.731879
3509.381291	914817.066013	42.736884
3509.451673	914627.806669	42.741888
3509.519024	914466.664984	42.746893
3509.293817	914283.510197	42.751898
3509.451268	914102.501605	42.756903
3509.423673	913930.668234	42.761908
3509.511130	913763.241525	42.766912
3509.374507	913579.181655	42.771917
3509.352785	913406.945578	42.776922
3509.444612	913226.689537	42.781927
3509.047779	913054.600529	42.786932
3509.023721	912875.122739	42.791937
3509.400690	912710.795491	42.796941
3509.200772	912541.933685	42.801946
3509.268621	912350.958247	42.806951
3508.976397	912200.407804	42.811956
3508.994422	912015.980976	42.816961
3509.242209	911850.685733	42.821965
3509.125302	911676.291149	42.826970
3509.341854	911508.003513	42.831975
3508.758138	911341.673579	42.836980
3508.708736	911173.805017	42.841985
3508.595990	911007.483766	42.846989
3508.858988	910852.468114	42.851994
3508.766795	910675.917478	42.856999
3508.866491	910524.581962	42.862004
3508.837602	910359.287552	42.867009
3508.988715	910192.127149	42.872013
3508.740513	910024.545513	42.877018
3508.725543	909862.993219	42.882023
3508.351147	909700.049453	42.887028
3508.498615	909541.352909	42.892033
3508.503966	909379.397525	42.897037
3508.199458	909228.189471	42.902042
3508.607417	909061.338162	42.907047
3508.169137	908922.002001	42.912052
3508.457911	908761.910059	42.917057
3508.447908	908608.515443	42.922061
3508.296342	908454.947061	42.927066
3508.356831	908284.272815	42.932071
3508.195792	908137.543150	42.937076
3508.030216	907983.964017	42.942081
3508.276106	907833.302166	42.947085
3508.081661	907685.891038	42.952090
3508.094579	907526.194571	42.957095
3508.009960	907380.975254	42.962100
3507.879158	907238.749390	42.967105
3507.997969	907088.184685	42.972109
3508.147364	906945.519377	42.977114
3508.377128	906797.725433	42.982119
3507.918068	906649.365887	42.987124
3507.966505	906493.684790	42.992129
3507.787845	906339.676495	42.997133
3507.751372	906197.311971	43.002138
3507.545303	906043.010600	43.007143
3507.827171	905905.795059	43.012148
3507.748048	905755.516260	43.017153
3507.713832	905617.573963	43.022157
3507.812707	905475.651022	43.027162
3508.027660	905330.039359	43.032167
3507.917792	905181.583131	43.037172
3507.783563	905035.731878	43.042177
3507.543773	904890.376604	43.047181
3507.441187	904754.739751	43.052186
3507.500283	904602.187959	43.057191
3507.315415	904482.092238	43.062196
3507.197061	904339.307769	43.067201
3507.205122	904207.884972	43.072205
3507.104199	904071.362800	43.077210
3507.295170	903935.947171	43.082215
3507.235582	903804.429528	43.087220
3507.118397	903660.855524	43.092225
3507.324000	903548.685072	43.097229
3507.031732	903420.767385	43.102234
3507.232986	903277.613610	43.107239
3506.695906	903154.362577	43.112244
3506.925962	903020.172976	43.117249
3507.432721	902892.787170	43.122253
3507.020344	902763.233472	43.127258
3507.441312	902631.223006	43.132263
3506.997791	902503.116217	43.137268
3507.089762	902357.929969	43.142273
3506.860777	902239.337731	43.147277
3506.929732	902114.323000	43.152282
3506.912923	901970.592575	43.157287
3506.776228	901862.788658	43.162292
3506.672801	901736.925116	43.167297
3506.874523	901607.436591	43.172301
3506.649383	901488.248609	43.177306
3506.753634	901361.377035	43.182311
3506.547112	901253.186744	43.187316
3506.474226	901120.256654	43.192321
3506.593632	900996.560357	43.197325
3506.420529	900884.785186	43.202330
3506.456737	900767.566399	43.207335
3506.526133	900654.298413	43.212340
3506.440027	900524.735802	43.217345
3506.592569	900407.683462	43.222349
3506.529732	900290.567610	43.227354
3506.610007	900168.983883	43.232359
3506.529390	900054.956048	43.237364
3506.586979	899939.647774	43.242369
3506.730425	899813.507352	43.247373
3506.359914	899707.438836	43.252378
3506.645753	899580.207461	43.257383
3506.195816	899467.387441	43.262388
3506.428722	899343.249814	43.267393
3506.396930	899225.816977	43.272397
3506.427213	899104.508250	43.277402
3506.343846	898990.072995	43.282407
3506.166259	898884.440114	43.287412
3506.408397	898763.958421	43.292417
3506.408003	898656.456941	43.297421
3506.197254	898548.794889	43.302426
3506.455908	898418.644101	43.307431
3506.291655	898315.026803	43.312436
3505.951168	898193.856182	43.317441
3506.156370	898081.963072	43.322445
3506.018069	897987.705489	43.327450
3506.350893	897879.458130	43.332455
3506.323806	897764.698967	43.337460
3505.785588	897645.481229	43.342465
3506.175040	897527.557257	43.347469
3506.182620	897433.459617	43.352474
3506.136603	897314.057195	43.357479
3505.733943	897211.618281	43.362484
3505.689162	897106.026885	43.367489
3506.106741	897003.642305	43.372493
3505.824729	896897.119933	43.377498
3506.054114	896788.772144	43.382503
3505.852285	896691.121726	43.387508
3505.745895	896578.573880	43.392513
3505.810138	896470.826963	43.397517
3505.392241	896379.390795	43.402522
3505.736054	896268.212024	43.407527
3505.638452	896185.803076	43.412532
3505.804873	896077.452072	43.417537
3505.984110	895971.899274	43.422541
3505.569562	895878.328525	43.427546
3505.690495	895759.832209	43.432551
3505.442390	895658.789320	43.437556
3505.487508	895566.297368	43.442561
3505.789380	895461.488006	43.447565
3505.524286	895372.136564	43.452570
3505.556472	895268.527805	43.457575
3505.624873	895179.311679	43.462580
3505.499903	895067.800055	43.467585
3505.624896	894971.902543	43.472589
3505.388832	894872.873360	43.477594
3505.335015	894775.745514	43.482599
3505.445101	894681.198717	43.487604
3505.215058	894577.620571	43.492609
3505.558925	894490.861365	43.497613
3505.471953	894396.922266	43.502618
3505.368439	894293.414763	43.507623
3505.485610	894201.855375	43.512628
3505.403129	894115.160687	43.517633
3505.698076	894017.575785	43.522637
3505.333820	893909.560903	43.527642
3505.450819	893817.608694	43.532647
3504.915493	893724.409061	43.537652
3505.257399	893625.262953	43.542657
3505.500149	893530.965232	43.547661
3505.128601	893452.622169	43.552666
3505.391064	893355.901388	43.557671
3505.185442	893265.636963	43.562676
3505.317550	893162.553502	43.567681
3505.451369	893069.619649	43.572685
3505.437300	892979.899246	43.577690
3505.403725	892876.934609	43.582695
3505.400027	892779.667798	43.587700
3504.986154	892698.807460	43.592705
3505.440241	892607.747118	43.597709
3504.720136	892531.189262	43.602714
3505.184501	892436.643576	43.607719
3505.066687	892337.164069	43.612724
3504.922920	892255.769479	43.617729
3505.307876	892167.517732	43.622733
3504.810451	892080.280295	43.627738
3504.810568	891986.383852	43.632743
3504.855281	891909.208144	43.637748
3504.586899	891821.252098	43.642753
3505.088189	891728.912838	43.647757
3504.495007	891659.672031	43.652762
3504.765158	891579.069982	43.657767
3504.507250	891489.946615	43.662772
3504.609923	891413.818489	43.667777
3504.798489	891334.967249	43.672781
3504.493464	891253.198111	43.677786
3504.739269	891165.050555	43.682791
3504.674310	891088.075279	43.687796
3504.620106	891002.972875	43.692801
3504.641510	890920.274741	43.697805
3504.429117	890853.669592	43.702810
3504.865690	890765.291021	43.707815
3504.687637	890687.168327	43.712820
3504.544615	890607.587924	43.717825
3504.913488	890528.018808	43.722829
3504.370791	890459.722427	43.727834
3504.458203	890371.105128	43.732839
3504.336099	890300.996444	43.737844
3504.478782	890226.974030	43.742849
3504.435949	890151.433505	43.747853
3504.324601	890070.582912	43.752858
3504.323005	889990.390245	43.757863
3504.051373	889925.331837	43.762868
3504.137999	889854.893107	43.767873
3504.452951	889778.611571	43.772877
3504.245231	889710.154336	43.777882
3504.295540	889634.301444	43.782887
3504.082299	889575.517632	43.787892
3504.186196	889501.782492	43.792897
3504.161963	889426.809834	43.797901
3503.775324	889366.117550	43.802906
3504.273086	889287.283990	43.807911
3504.181577	889225.380633	43.812916
3503.914439	889155.475356	43.817921
3504.310939	889087.298155	43.822925
3503.899309	889021.672075	43.827930
3503.945351	888945.423794	43.832935
3504.031806	888889.292668	43.837940
3503.840418	888813.081750	43.842945
3504.105450	888761.467445	43.847949
3503.833751	888702.394067	43.852954
3504.086387	888623.495050	43.857959
3504.240563	888555.254717	43.862964
3504.251284	888486.456647	43.867969
3504.217647	888420.180868	43.872973
3503.830096	888352.704716	43.877978
3504.124100	888274.181153	43.882983
3503.684861	888214.453020	43.887988
3503.486899	888142.975804	43.892993
3503.806669	888089.120836	43.897997
3503.621699	888033.896998	43.903002
3503.606394	887962.387449	43.908007
3503.767399	887910.589127	43.913012
3503.749757	887845.562117	43.918017
3503.445255	887787.839559	43.923021
3503.157063	887730.887922	43.928026
3503.588812	887675.946144	43.933031
3503.667950	887615.545754	43.938036
3503.544132	887559.145992	43.943041
3503.837595	887500.063950	43.948045
3503.511148	887448.148230	43.953050
3503.747358	887373.880167	43.958055
3503.564975	887328.133500	43.963060
3503.692723	887254.849575	43.968065
3503.822686	887198.791606	43.973069
3503.469844	887141.457671	43.978074
3503.418214	887073.040146	43.983079
3503.534634	887032.274686	43.988084
3503.327603	886973.560071	43.993089
3503.817118	886914.730104	43.998093
3503.718399	886857.545057	44.003098
3503.685055	886798.993629	44.008103
3503.717803	886745.173419	44.013108
3503.536605	886685.870886	44.018113
3503.653010	886635.326756	44.023117
3503.323558	886581.758280	44.028122
3503.689620	886520.815213	44.033127
3503.524988	886456.667920	44.038132
3503.541676	886403.331148	44.043137
3503.715653	886349.193599	44.048141
3503.215379	886294.392249	44.053146
3503.598015	886234.798602	44.058151
3503.471435	886177.030623	44.063156
3503.563842	886118.741988	44.068161
3503.762643	886064.888092	44.073165
3503.461757	886007.243936	44.078170
3503.713808	885946.216804	44.083175
3503.527664	885898.329766	44.088180
3503.497576	885844.317920	44.093185
3503.642356	885784.758832	44.098189
3503.383308	885734.946337	44.103194
3503.276443	885672.136121	44.108199
3503.563734	885621.748604	44.113204
3503.766660	885568.179838	44.118209
3503.788251	885509.703123	44.123213
3503.484773	885451.085749	44.128218
3503.601026	885389.010197	44.133223
3503.558922	885328.702712	44.138228
3503.340355	885276.362452	44.143233
3503.810749	885217.421591	44.148237
3503.556312	885174.671028	44.153242
3503.570639	885105.638478	44.158247
3503.335045	885049.039012	44.163252
3503.519347	885001.470800	44.168257
3503.741494	884942.955327	44.173261
3503.449335	884904.759521	44.178266
3503.711920	884844.106338	44.183271
3503.496680	884784.112178	44.188276
3503.177408	884737.012052	44.193281
3503.609037	884678.653050	44.198285
3503.264391	884635.041950	44.203290
3503.880374	884578.975376	44.208295
3503.740891	884518.869166	44.213300
3503.705510	884462.424645	44.218305
3503.859845	884391.327146	44.223309
3503.567356	884341.217691	44.228314
3503.309702	884278.514052	44.233319
3503.358879	884222.343759	44.238324
3503.283419	884177.619720	44.243329
3503.547852	884123.640160	44.248333
3503.371972	884082.417940	44.253338
3503.729153	884014.671611	44.258343
3503.227881	883967.595223	44.263348
3503.122139	883908.639171	44.268353
3503.586398	883852.784271	44.273357
3503.242581	883804.324885	44.278362
3503.280689	883760.353636	44.283367
3503.088536	883711.771651	44.288372
3503.099905	883662.574683	44.293377
3503.420359	883613.229535	44.298381
3503.367085	883559.393924	44.303386
3503.379454	883508.355471	44.308391
3503.477106	883459.433102	44.313396
3503.061189	883403.912594	44.318401
3503.282831	883354.000455	44.323405
3502.911932	883313.579680	44.328410
3503.564027	883261.271502	44.333415
3503.473505	883203.758515	44.338420
3503.504982	883149.905154	44.343425
3503.654424	883099.615332	44.348429
3503.359180	883051.722772	44.353434
3503.751136	883001.198444	44.358439
3503.294439	882950.619788	44.363444
3503.096281	882891.862363	44.368449
3503.454254	882838.920876	44.373453
3503.122566	882798.877483	44.378458
3503.281349	882740.640860	44.383463
3503.033393	882705.716426	44.388468
3503.197199	882652.611522	44.393473
3503.400741	882595.818949	44.398477
3503.149124	882550.433409	44.403482
3503.238428	882500.438904	44.408487
3503.174223	882454.343715	44.413492
3502.899489	882400.533874	44.418497
3503.288593	882357.269102	44.423501
3503.185891	882313.310124	44.428506
3503.443536	882261.445427	44.433511
3503.357637	882204.115539	44.438516
3503.595514	882155.740316	44.443521
3503.512172	882113.810837	44.448525
3503.518898	882056.948577	44.453530
3503.440534	881995.062599	44.458535
3503.338369	881953.231935	44.463540
3502.993003	881897.976046	44.468545
3503.061045	881841.973425	44.473549
3503.164941	881798.945249	44.478554
3503.238865	881750.690553	44.483559
3503.163465	881709.144350	44.488564
3503.177429	881653.730074	44.493569
3503.037659	881603.862503	44.498573
3502.672577	881564.106749	44.503578
3502.938278	881524.537433	44.508583
3503.327851	881474.678426	44.513588
3502.933973	881428.241934	44.518593
3503.129479	881385.583134	44.523597
3503.031952	881354.694740	44.528602
3502.977201	881294.928799	44.533607
3502.770680	881246.231737	44.538612
3502.903505	881207.069690	44.543617
3502.868191	881170.454030	44.548621
3502.477230	881138.547127	44.553626
3502.937506	881098.845992	44.558631
3503.137997	881056.474622	44.563636
3502.794764	881013.998754	44.568641
3503.112176	880968.604042	44.573645
3503.030682	880933.350909	44.578650
3502.947285	880888.893591	44.583655
3503.039754	880837.043467	44.588660
3502.904222	880787.943338	44.593665
3502.851987	880749.196270	44.598669
3502.877235	880705.107214	44.603674
3503.089673	880668.156921	44.608679
3503.312889	880625.003556	44.613684
3503.015173	880573.021592	44.618689
3503.381175	880522.286325	44.623693
3503.183136	880479.685758	44.628698
3503.084720	880419.433593	44.633703
3502.992764	880386.310577	44.638708
3502.948043	880340.098595	44.643713
3503.280746	880294.405451	44.648717
3503.051292	880246.479017	44.653722
3503.280524	880203.030859	44.658727
3503.170516	880163.611142	44.663732
3503.462380	880121.314852	44.668737
3503.300721	880069.984302	44.673741
3503.054792	880021.864941	44.678746
3502.910269	879966.460790	44.683751
3502.883938	879939.429292	44.688756
3503.194468	879887.147220	44.693761
3503.443738	879835.553108	44.698765
3503.426877	879791.561017	44.703770
3503.391499	879740.012960	44.708775
3503.011793	879692.688184	44.713780
3503.208504	879640.035033	44.718785
3503.334734	879597.471530	44.723789
3503.259409	879544.377795	44.728794
3503.162415	879491.771702	44.733799
3503.347274	879451.523331	44.738804
3503.276948	879400.656425	44.743809
3503.085046	879341.571518	44.748813
3503.185567	879309.864398	44.753818
3503.097176	879268.399915	44.758823
3503.183883	879223.320443	44.763828
3503.093378	879178.851314	44.768833
3503.007540	879132.539669	44.773837
3503.133300	879090.360232	44.778842
3503.094681	879043.070931	44.783847
3503.280907	878992.255136	44.788852
3503.004675	878954.114611	44.793857
3503.618663	878896.152399	44.798861
3503.075492	878855.729127	44.803866
3503.299251	878803.257858	44.808871
3503.192460	878754.717482	44.813876
3502.974677	878706.098068	44.818881
3503.296978	878661.460087	44.823885
3503.145320	878619.807596	44.828890
3503.043376	878573.397269	44.833895
3503.017916	878532.304920	44.838900
3502.857600	878483.189561	44.843905
3503.354010	878432.511677	44.848909
3502.923062	878394.877646	44.853914
3502.808315	878358.063641	44.858919
3503.034662	878317.025231	44.863924
3502.935656	878274.004597	44.868929
3503.113294	878221.826529	44.873933
3502.752362	878180.690059	44.878938
3503.154078	878126.147856	44.883943
3503.024471	878088.656081	44.888948
3502.736694	878042.853781	44.893953
3503.051389	877995.691710	44.898957
3502.585440	877972.213241	44.903962
3502.648790	877928.872526	44.908967
3502.982895	877887.910307	44.913972
3502.633929	877855.106150	44.918977
3502.614384	877805.380310	44.923981
3502.567605	877770.781008	44.928986
3502.656699	877732.863178	44.933991
3502.819657	877692.800254	44.938996
3502.658890	877661.030348	44.944001
3502.956695	877612.995531	44.949005
3502.895410	877582.081282	44.954010
3502.835936	877536.334364	44.959015
3502.772505	877494.950194	44.964020
3502.629256	877461.140513	44.969025
3502.809547	877411.475366	44.974029
3502.589382	877389.989913	44.979034
3502.628661	877348.490848	44.984039
3502.770908	877318.898925	44.989044
3502.599667	877275.882891	44.994049
3502.908023	877237.344067	44.999053
3502.690772	877201.315290	45.004058
3502.894486	877163.859655	45.009063
3503.007325	877120.020091	45.014068
3502.752265	877076.919463	45.019073
3502.802430	877028.726784	45.024077
3502.720864	877002.078674	45.029082
3502.775138	876958.441459	45.034087
3502.962451	876925.252905	45.039092
3502.882605	876888.811768	45.044097
3503.153729	876842.326322	45.049101
3502.987503	876809.680134	45.054106
3502.885220	876753.656993	45.059111
3502.795947	876713.532014	45.064116
3502.808483	876677.268261	45.069121
3503.087126	876635.724743	45.074125
3503.103709	876595.290647	45.079130
3502.982106	876548.285839	45.084135
3503.069365	876506.288146	45.089140
3502.743054	876468.236701	45.094145
3502.736923	876420.727050	45.099149
3502.008037	876383.032261	45.104154
3502.437206	876354.842657	45.109159
3502.351404	876311.417657	45.114164
3502.082934	876295.172155	45.119169
3502.287557	876260.910421	45.124173
3501.927997	876225.868760	45.129178
3501.964313	876209.766736	45.134183
3502.508531	876173.218362	45.139188
3502.068533	876155.837154	45.144193
3502.107882	876120.438250	45.149197
3502.069411	876097.754555	45.154202
3501.864356	876080.819249	45.159207
3502.001757	876045.500708	45.164212
3502.163985	876020.262503	45.169217
3502.528856	875983.645539	45.174221
3502.286418	875971.079643	45.179226
3502.335846	875936.744630	45.184231
3502.205668	875911.554135	45.189236
3502.159474	875882.276964	45.194241
3502.165938	875837.572670	45.199245
3502.145945	875817.600030	45.204250
3502.088929	875788.712062	45.209255
3501.924195	875755.768880	45.214260
3502.089948	875734.989583	45.219265
3502.242172	875694.526971	45.224269
3501.716676	875680.261576	45.229274
3501.965060	875659.080507	45.234279
3501.943291	875628.731347	45.239284
3502.344827	875626.725754	45.244289
3502.551938	875577.913528	45.249293
3502.149525	875569.252124	45.254298
3501.826730	875521.302532	45.259303
3502.047654	875501.870988	45.264308
3501.960177	875480.259733	45.269313
3501.936307	875451.461631	45.274317
3502.307390	875436.466071	45.279322
3502.070098	875404.017767	45.284327
3501.973669	875381.922738	45.289332
3502.204031	875364.525728	45.294337
3502.193166	875333.009513	45.299341
3501.741282	875314.367052	45.304346
3502.292736	875291.680051	45.309351
3502.677205	875257.382874	45.314356
3502.326625	875229.316377	45.319361
3502.557337	875194.074360	45.324365
3502.278549	875172.881423	45.329370
3502.363631	875139.408740	45.334375
3502.424808	875113.407459	45.339380
3502.426576	875084.312399	45.344385
3502.655944	875044.899447	45.349389
3502.541790	875013.398547	45.354394
3502.375081	874972.013698	45.359399
3502.301046	874945.064106	45.364404
3502.443653	874907.410267	45.369409
3502.259639	874876.890007	45.374413
3502.387860	874847.966924	45.379418
3502.494430	874818.853293	45.384423
3502.526594	874785.193351	45.389428
3502.388225	874753.792045	45.394433
3502.532192	874709.832480	45.399437
3501.939786	874695.672709	45.404442
3502.176042	874666.730942	45.409447
3502.481724	874639.426431	45.414452
3502.416935	874614.801577	45.419457
3502.573537	874576.852360	45.424461
3502.644082	874552.010967	45.429466
3502.156920	874511.354632	45.434471
3502.445010	874481.627484	45.439476
3502.195434	874458.972282	45.444481
3502.258212	874436.750499	45.449485
3501.931603	874409.937076	45.454490
3502.358366	874379.507613	45.459495
3502.323768	874348.669028	45.464500
3501.942023	874331.563824	45.469505
3502.143421	874294.672368	45.474509
3502.116261	874279.351516	45.479514
3502.492812	874243.982827	45.484519
3502.253897	874216.281108	45.489524
3502.157411	874197.867557	45.494529
3502.405394	874155.729697	45.499533
3502.222532	874132.286267	45.504538
3502.344010	874094.630747	45.509543
3501.930239	874083.253046	45.514548
3502.107092	874054.803078	45.519553
3502.254907	874030.819769	45.524557
3502.058505	873998.163013	45.529562
3501.872119	873970.257487	45.534567
3502.254385	873960.203420	45.539572
3502.245659	873928.388373	45.544577
3502.265342	873901.224587	45.549581
3502.268973	873879.107462	45.554586
3502.310400	873843.500591	45.559591
3502.483985	873816.408065	45.564596
3502.246863	873798.404457	45.569601
3502.559296	873770.997837	45.574605
3502.176957	873739.437338	45.579610
3502.035591	873707.351943	45.584615
3501.974212	873679.521458	45.589620
3502.046203	873667.189872	45.594625
3502.166351	873633.508894	45.599629
3501.837505	873603.878993	45.604634
3502.076014	873582.304109	45.609639
3501.884454	873554.397477	45.614644
3502.020116	873540.988051	45.619649
3502.178791	873518.844040	45.624653
3502.174236	873497.696928	45.629658
3502.489624	873470.385444	45.634663
3502.128479	873441.342107	45.639668
3502.068417	873426.218491	45.644673
3502.160856	873379.638285	45.649677
3502.042627	873369.665680	45.654682
3502.123998	873344.429402	45.659687
3502.118181	873312.125514	45.664692
3502.057307	873294.964446	45.669697
3502.359754	873264.064694	45.674701
3502.484172	873239.596981	45.679706
3502.551574	873208.735665	45.684711
3502.583935	873180.984413	45.689716
3502.388488	873142.307911	45.694721
3502.550720	873113.467785	45.699725
3502.071842	873088.031674	45.704730
3502.047423	873063.005662	45.709735
3502.544045	873034.207077	45.714740
3502.192664	873004.092808	45.719745
3502.401900	872968.064973	45.724749
3502.450116	872950.593885	45.729754
3502.382825	872915.387432	45.734759
3502.318501	872882.217680	45.739764
3502.212788	872857.204194	45.744769
3502.515197	872820.480980	45.749773
3502.155557	872796.673313	45.754778
3502.274109	872759.203848	45.759783
3502.438842	872746.175925	45.764788
3502.312283	872722.038495	45.769793
3502.595279	872684.347424	45.774797
3502.350622	872654.892955	45.779802
3502.237030	872622.214982	45.784807
3502.253886	872587.574863	45.789812
3502.493215	872491.578198	45.794817
3502.704630	872345.421468	45.799821
3502.531768	872138.583311	45.804826
3501.938079	871876.788506	45.809831
3502.313209	871559.024529	45.814836
3501.965877	871187.599082	45.819841
3501.674629	870746.554123	45.824845
3501.680947	870253.208543	45.829850
3501.414078	869690.947298	45.834855
3501.559120	869079.539722	45.839860
3501.081426	868407.781602	45.844865
3501.633151	867651.590108	45.849869
3501.225112	866833.792490	45.854874
3501.099922	865963.775008	45.859879
3500.827561	865015.550944	45.864884
3500.342976	864011.247540	45.869889
3500.022240	862934.449041	45.874893
3499.760100	861779.983080	45.879898
3499.580823	860556.162655	45.884903
3499.377072	859262.283606	45.889908
3498.811080	857902.150932	45.894913
3498.703914	856463.912097	45.899917
3497.956854	854954.797706	45.904922
3497.550952	853370.117876	45.909927
3497.320498	851706.143583	45.914932
3496.795879	849978.958491	45.919937
3496.418732	848171.099419	45.924941
3496.110200	846286.409038	45.929946
3495.547452	844325.360911	45.934951
3495.389378	842295.382986	45.939956
3494.757864	840180.853067	45.944961
3494.454208	837993.900428	45.949965
3493.848836	835725.822289	45.954970
3492.901222	833383.817295	45.959975
3492.682612	830966.509297	45.964980
3491.989989	828476.997322	45.969985
3491.543648	825906.042807	45.974989
3490.751986	823269.446379	45.979994
3490.421019	820546.946812	45.984999
3489.548763	817758.527239	45.990004
3488.431806	814890.208067	45.995009
3488.092154	811944.860693	46.000013
3487.250832	808952.641050	46.005018
3486.360789	805854.348732	46.010023
3485.970258	802693.605693	46.015028
3484.839253	799460.530641	46.020033
3484.482223	796148.548945	46.025037
3483.000392	792777.371997	46.030042
3482.266560	789314.382683	46.035047
3481.498616	785787.218980	46.040052
3480.369634	782196.493251	46.045057
3479.519349	778530.060845	46.050061
3478.668702	774792.743428	46.055066
3477.560917	770990.895688	46.060071
3477.306314	767097.438534	46.065076
3475.506116	763148.150020	46.070081
3474.802792	759110.255809	46.075085
3473.632001	755017.661476	46.080090
3472.377901	750847.663534	46.085095
3471.564073	746598.738518	46.090100
3470.114818	742299.886902	46.095105
3469.140600	737914.156534	46.100109
3467.747349	733473.903841	46.105114
3466.971059	728943.924978	46.110119
3465.932843	724343.076229	46.115124
3464.188989	719679.325067	46.120129
3462.862199	714945.663552	46.125133
3461.515211	710139.595712	46.130138
3460.418009	705271.866103	46.135143
3459.395212	700332.344610	46.140148
3457.525933	695324.428852	46.145153
3456.522509	690239.000180	46.150157
3454.984880	685086.701060	46.155162
3453.541703	679864.265626	46.160167
3452.093839	674582.199099	46.165172
3450.256565	669220.259046	46.170177
3448.829766	663787.204251	46.175181
3446.924045	658291.794359	46.180186
3445.726890	652735.074700	46.185191
3444.305590	647113.796136	46.190196
3442.394345	641418.542491	46.195201
3440.887717	635661.654800	46.200205
3439.129431	629848.349694	46.205210
3437.342873	623961.620269	46.210215
3435.637931	618008.251500	46.215220
3433.957663	611997.831495	46.220225
3432.190378	605923.723217	46.225229
3430.261280	599792.575636	46.230234
3428.046362	593595.892889	46.235239
3426.081898	587329.980034	46.240244
3423.960020	581028.804036	46.245249
3422.280411	574639.506307	46.250253
3419.881656	568217.531035	46.255258
3417.861197	561728.676894	46.260263
3416.140503	555175.752168	46.265268
3413.728725	548568.630151	46.270273
3411.752521	541901.424558	46.275277
3409.394432	535183.294893	46.280282
3406.921465	528403.100376	46.285287
3404.595813	521571.298819	46.290292
3402.229604	514693.998143	46.295297
3399.818120	507755.857578	46.300301
3397.340479	500786.572350	46.305306
3394.866825	493748.034664	46.310311
3392.657595	486665.662688	46.315316
3389.860095	479544.647968	46.320321
3387.618114	472359.068163	46.325325
3385.124196	465141.809391	46.330330
3382.550890	457865.583159	46.335335
3379.853725	450545.946637	46.340340
3376.548811	443183.844987	46.345345
3374.344415	435775.401032	46.350349
3371.588041	428332.922805	46.355354
3368.634999	420849.848343	46.360359
3365.726724	413323.539786	46.365364
3362.752444	405754.287597	46.370369
3359.786960	398148.071783	46.375373
3356.542011	390513.050886	46.380378
3353.378507	382842.823121	46.385383
3350.522124	375136.344787	46.390388
3347.119236	367381.892820	46.395393
3344.046921	359614.153292	46.400397
3340.801602	351820.825678	46.405402
3337.675294	343990.437690	46.410407
3334.540706	336141.840394	46.415412
3330.978865	328275.951461	46.420417
3327.572676	320362.315894	46.425421
3324.270613	312447.865019	46.430426
3320.318298	304494.779402	46.435431
3317.261927	296525.706160	46.440436
3313.502354	288544.212122	46.445441
3309.812380	280544.536329	46.450445
3305.789327	272533.056224	46.455450
3302.115677	264506.320080	46.460455
3298.236823	256473.076687	46.465460
3294.388714	248422.717211	46.470465
3290.664934	240381.814826	46.475469
3286.678223	232325.042566	46.480474
3282.830038	224170.900864	46.485479
3278.738235	216092.825698	46.490484
3274.509382	208021.862680	46.495489
3270.467138	199944.630898	46.500493
3266.212495	191890.205512	46.505498
3261.980307	183820.529283	46.510503
3257.477631	175762.276369	46.515508
3252.980343	167720.040807	46.520513
3248.823841	159682.198495	46.525517
3243.775832	151659.518447	46.530522
3238.969072	143668.231363	46.535527
3234.285873	135671.143915	46.540532
3229.292148	127714.434562	46.545537
3224.282984	119780.300543	46.550541
3218.970731	111878.459655	46.555546
3213.592657	104009.197824	46.560551
3208.158527	96181.809600	46.565556
3202.282417	88400.932734	46.570561
3196.952951	80662.685734	46.575565
3190.758342	72977.786688	46.580570
3183.991087	65359.500232	46.585575
3177.280909	57813.732146	46.590580
3169.615072	50358.076788	46.595585
3160.184688	43029.175801	46.600589
3142.406161	36047.585106	46.605594
3120.462072	29377.889924	46.610599
3095.533931	23073.242110	46.615604
3064.307343	17328.621319	46.620609
3029.601281	12193.085302	46.625613
2994.512958	7670.005309	46.630618
2961.536936	3763.954846	46.635623
2920.323888	809.722929	46.640628
2818.525430	322.167351	46.645633
2747.559933	308.279416	46.650637
2730.260699	302.206806	46.655642
2750.923554	300.831324	46.660647
2788.251049	294.493410	46.665652
2823.462399	297.558197	46.670657
2848.279040	286.585801	46.675661
2860.133165	282.036317	46.680666
2860.946712	283.711382	46.685671
2856.410837	283.036099	46.690676
2849.489482	293.440487	46.695681
2843.980841	290.700460	46.700685
2839.702033	278.050251	46.705690
2836.442121	269.154340	46.710695
2833.954569	263.818161	46.715700
2831.636159	272.835222	46.720705
2830.056049	269.593514	46.725709
2827.342124	280.313382	46.730714
2824.757727	268.346287	46.735719
2822.011651	262.320626	46.740724
2818.777701	265.832112	46.745729
2815.951561	258.219612	46.750733
2812.687613	259.622906	46.755738
2809.460323	264.480358	46.760743
2806.879833	255.886408	46.765748
2803.278875	254.489371	46.770753
2799.951302	249.241288	46.775757
2796.634329	259.019078	46.780762
2793.521625	268.858292	46.785767
2790.402761	248.510661	46.790772
2787.354172	252.720957	46.795777
2784.343857	253.214511	46.800781
2781.228132	255.438784	46.805786
2777.408852	254.369854	46.810791
2774.465709	250.522246	46.815796
2770.644999	246.957178	46.820801
2767.496266	243.063772	46.825805
2764.279165	252.944292	46.830810
2760.794887	248.938510	46.835815
2757.538552	245.583057	46.840820
2754.244311	253.667078	46.845825
2751.420732	237.776886	46.850829
2747.496772	246.951519	46.855834
2744.219631	242.366515	46.860839
2740.964484	240.721045	46.865844
2737.277963	249.816252	46.870849
2733.945213	242.957576	46.875853
2730.663806	245.838342	46.880858
2727.206598	245.871660	46.885863
2724.148501	239.731389	46.890868
2720.167360	240.678418	46.895873
2717.252964	236.302756	46.900877
2713.745913	236.791089	46.905882
2710.067309	235.983567	46.910887
2707.053486	238.281450	46.915892
2703.604952	242.851034	46.920897
2700.150239	233.519688	46.925901
2696.409329	242.030681	46.930906
2692.619989	240.012398	46.935911
2689.734035	230.726931	46.940916
2686.394283	237.278041	46.945921
2683.046230	226.733222	46.950925
2679.418378	225.908665	46.955930
2676.171852	229.500057	46.960935
2672.921839	226.132572	46.965940
2668.407088	233.769566	46.970945
2665.314150	223.628657	46.975949
2662.041114	228.423480	46.980954
2658.724483	234.407972	46.985959
2655.351675	229.350992	46.990964
2651.008492	240.937706	46.995969
2648.241165	230.275374	47.000973
2644.415133	233.169101	47.005978
2640.820776	234.597424	47.010983
2637.930685	231.556174	47.015988
2634.398210	233.050463	47.020993
2631.701079	221.222905	47.025997
2628.198111	223.829283	47.031002
2624.429052	229.133424	47.036007
2621.004623	218.413788	47.041012
2616.574486	235.660815	47.046017
2613.343940	225.578173	47.051021
2610.265800	228.097485	47.056026
2606.854964	230.323987	47.061031
2603.405783	213.975928	47.066036
2599.591851	221.625591	47.071041
2596.409968	218.822364	47.076045
2592.539613	213.609945	47.081050
2589.373735	218.671691	47.086055
2586.415818	215.265536	47.091060
2582.444338	214.120049	47.096065
2579.229929	215.484132	47.101069
2575.400852	215.125039	47.106074
2571.832860	229.643455	47.111079
2568.706802	206.908235	47.116084
2565.183192	219.450644	47.121089
2561.779669	215.387881	47.126093
2558.025343	218.841730	47.131098
2554.467087	208.567339	47.136103
2551.441265	207.330539	47.141108
2547.644401	218.657834	47.146113
2544.013521	213.449742	47.151117
2540.472335	214.176297	47.156122
2536.997329	214.806680	47.161127
2534.111626	207.430370	47.166132
2530.644679	212.312921	47.171137
2527.155823	201.950141	47.176141
2523.481694	213.197594	47.181146
2519.716147	214.463622	47.186151
2516.441737	213.064609	47.191156
2512.688066	211.620372	47.196161
2509.103947	204.797249	47.201165
2505.934640	207.116367	47.206170
2502.793239	208.391486	47.211175
2499.458324	204.968082	47.216180
2495.215188	223.804686	47.221185
2492.197546	204.318233	47.226189
2488.589434	207.460669	47.231194
2484.610691	200.985686	47.236199
2481.500494	202.179297	47.241204
2478.166669	207.880975	47.246209
2474.841358	201.582126	47.251213
2471.040300	206.115704	47.256218
2467.515472	205.672535	47.261223
2463.854647	200.862162	47.266228
2460.289184	211.484104	47.271233
2456.959875	200.138536	47.276237
2453.381317	201.963405	47.281242
2449.913667	205.292259	47.286247
2446.556754	194.740031	47.291252
2442.933113	199.001417	47.296257
2440.104422	205.826087	47.301261
2436.526389	201.184018	47.306266
2432.789273	194.231894	47.311271
2429.189953	191.036107	47.316276
2425.219315	194.749535	47.321281
2422.373082	197.860785	47.326285
2418.466151	198.232393	47.331290
2415.077880	200.978838	47.336295
2412.063386	198.430899	47.341300
2408.357868	204.988861	47.346305
2404.877281	197.834371	47.351309
2401.164505	197.546598	47.356314
2397.484822	202.047761	47.361319
2394.395410	185.744724	47.366324
2390.535970	192.852238	47.371329
2387.317251	187.872847	47.376333
2383.967083	197.052447	47.381338
2380.251215	202.317580	47.386343
2376.893780	193.063603	47.391348
2373.103995	193.545562	47.396353
2369.611415	195.430102	47.401357
2366.352178	194.256024	47.406362
2362.955493	193.684424	47.411367
2359.530988	186.298118	47.416372
2355.968980	194.022779	47.421377
2352.337941	192.864303	47.426381
2348.814337	192.958574	47.431386
2345.199859	201.239922	47.436391
2341.783030	194.452076	47.441396
2338.214866	191.775154	47.446401
2334.719578	192.188794	47.451405
2331.043946	195.758279	47.456410
2327.734775	192.336276	47.461415
2324.575219	181.583440	47.466420
2320.848486	185.501582	47.471425
2317.584457	188.498922	47.476429
2313.857478	188.951811	47.481434
2310.132104	189.108230	47.486439
2306.829517	182.987710	47.491444
2303.157065	187.260602	47.496449
2299.889010	185.817866	47.501453
2296.649771	191.058244	47.506458
2292.856022	185.997231	47.511463
2289.758098	177.358422	47.516468
2286.093233	185.451371	47.521473
2282.139508	189.963713	47.526477
2278.811489	191.078753	47.531482
2275.065334	191.004188	47.536487
2271.752417	182.537443	47.541492
2268.432537	186.408583	47.546497
2265.183736	186.164495	47.551501
2261.407967	180.721056	47.556506
2258.119204	189.750673	47.561511
2254.598940	182.288693	47.566516
2250.609794	194.143626	47.571521
2247.519915	179.553706	47.576525
2243.830948	174.605683	47.581530
2240.410813	182.707592	47.586535
2237.428272	179.280473	47.591540
2233.528495	180.304242	47.596545
2229.995927	179.687680	47.601549
2226.556542	176.526427	47.606554
2222.405608	184.851028	47.611559
2219.048677	185.959435	47.616564
2215.476907	177.244397	47.621569
2212.627426	176.987500	47.626573
2209.260057	178.201438	47.631578
2205.464804	175.478047	47.636583
2202.117107	174.298756	47.641588
2198.137271	182.761285	47.646593
2194.769065	176.175306	47.651597
2191.332720	171.575166	47.656602
2187.848144	182.195149	47.661607
2184.712536	178.173886	47.666612
2180.817121	177.208775	47.671617
2177.598054	182.383335	47.676621
2174.393986	177.817278	47.681626
2170.452723	168.682766	47.686631
2166.798526	169.122763	47.691636
2163.027580	182.840328	47.696641
2159.734373	177.123115	47.701645
2156.826384	179.385879	47.706650
2153.202823	179.058898	47.711655
2149.723420	178.836190	47.716660
2145.882371	185.919524	47.721665
2142.042361	180.835887	47.726669
2138.989885	174.206896	47.731674
2135.304842	177.804712	47.736679
2131.800764	172.499654	47.741684
2128.087846	179.818582	47.746689
2125.023973	182.233402	47.751693
2121.784044	179.242354	47.756698
2118.098951	184.240320	47.761703
2114.748650	182.069294	47.766708
2111.015493	184.712844	47.771713
2107.612173	181.410545	47.776717
2104.003403	172.818141	47.781722
2100.009926	180.178482	47.786727
2096.877785	181.270772	47.791732
2093.322895	181.051689	47.796737
2090.271327	172.600937	47.801741
2086.529743	177.965437	47.806746
2082.871192	182.569495	47.811751
2079.477888	176.917613	47.816756
2075.683406	177.964772	47.821761
2072.575007	179.392778	47.826765
2068.944303	178.189863	47.831770
2065.395109	180.657432	47.836775
2062.168568	174.395874	47.841780
2058.621067	179.466868	47.846785
2055.086660	181.004308	47.851789
2051.579445	170.177474	47.856794
2047.668978	180.403136	47.861799
2044.529164	172.071975	47.866804
2040.883043	179.260344	47.871809
2037.303755	178.880948	47.876813
2033.935654	176.553667	47.881818
2030.240593	177.312902	47.886823
2026.993052	168.118820	47.891828
2023.417657	170.086541	47.896833
2019.917797	175.409985	47.901837
2016.657853	167.809307	47.906842
2012.803821	172.710327	47.911847
2009.683157	172.542144	47.916852
2006.032281	167.934160	47.921857
2002.386886	180.057307	47.926861
1998.827422	168.221270	47.931866
1995.370894	177.333401	47.936871
1991.817022	164.966000	47.941876
1988.348936	172.741291	47.946881
1984.857073	160.813001	47.951885
1981.398240	165.671864	47.956890
1977.805238	168.950097	47.961895
1974.392223	172.048038	47.966900
1970.750531	172.353504	47.971905
1967.425853	162.379301	47.976909
1964.035076	168.586803	47.981914
1960.477078	169.283987	47.986919
1957.046512	155.917259	47.991924
1953.183278	166.241345	47.996929
1950.087762	165.645163	48.001933
1946.663925	151.160790	48.006938
1942.674539	171.793217	48.011943
1939.297961	160.710273	48.016948
1935.614152	166.652420	48.021953
1932.495093	158.961052	48.026957
1929.119503	158.172755	48.031962
1925.580612	159.349896	48.036967
1922.306935	155.495288	48.041972
1918.342968	162.235383	48.046977
1914.753137	159.962376	48.051981
1911.361749	160.103012	48.056986
1907.638099	165.432903	48.061991
1904.353661	163.638135	48.066996
1900.811307	160.960054	48.072001
1897.509278	164.582398	48.077005
1894.100504	165.824505	48.082010
1890.595993	163.603928	48.087015
1887.183151	157.274016	48.092020
1883.283957	164.552437	48.097025
1879.800853	155.584265	48.102029
1876.368691	148.561147	48.107034
1872.951431	164.142741	48.112039
1869.696357	162.336439	48.117044
1866.022586	164.734343	48.122049
1862.183892	155.072466	48.127053
1858.935230	157.293200	48.132058
1855.262928	164.511865	48.137063
1851.853743	156.299748	48.142068
1848.365316	162.289407	48.147073
1844.762652	160.664663	48.152077
1841.451049	159.942230	48.157082
1837.640321	163.265999	48.162087
1834.613272	163.217645	48.167092
1830.928945	162.725708	48.172097
1827.770477	158.456670	48.177101
1824.109800	153.847893	48.182106
1820.079499	168.802012	48.187111
1816.875465	155.602822	48.192116
1813.355359	152.462519	48.197121
1809.599775	155.727273	48.202125
1806.152668	154.482395	48.207130
1802.569725	163.888244	48.212135
1799.595779	162.549029	48.217140
1795.896110	162.574906	48.222145
1792.123734	165.954931	48.227149
1789.119249	156.625379	48.232154
1785.485945	160.710221	48.237159
1781.964882	159.471263	48.242164
1778.146241	162.687256	48.247169
1774.612296	154.637896	48.252173
1771.450993	155.419469	48.257178
1767.934695	154.158027	48.262183
1764.508724	149.976248	48.267188
1760.680624	165.252803	48.272193
1757.457785	150.071939	48.277197
1754.003659	156.931782	48.282202
1750.161491	152.945064	48.287207
1746.841577	149.349437	48.292212
1743.233090	163.237162	48.297217
1739.681310	155.074742	48.302221
1736.258259	149.030610	48.307226
1733.014479	152.112990	48.312231
1729.612525	157.755334	48.317236
1726.222214	155.353607	48.322241
1722.285403	155.671905	48.327245
1718.764970	144.641733	48.332250
1714.974320	160.590774	48.337255
1711.670947	153.675371	48.342260
1708.215289	155.996706	48.347265
1704.607249	152.330702	48.352269
1701.199511	159.954513	48.357274
1697.956638	164.319273	48.362279
1694.586235	146.740509	48.367284
1690.520274	156.631955	48.372289
1687.188266	155.096218	48.377293
1683.663822	159.558615	48.382298
1680.081786	155.500760	48.387303
1676.790685	152.626235	48.392308
1673.457362	151.547762	48.397313
1669.885265	154.289749	48.402317
1666.709210	151.795835	48.407322
1662.813561	160.045331	48.412327
1659.221940	151.936727	48.417332
1655.560272	162.038865	48.422337
1651.864587	152.117143	48.427341
1648.656994	153.165747	48.432346
1645.003200	145.287069	48.437351
1641.798441	145.552960	48.442356
1638.351131	155.679680	48.447361
1634.594110	157.774981	48.452365
1631.224233	150.936343	48.457370
1627.588619	152.673745	48.462375
1624.650058	147.201659	48.467380
1620.754378	151.779902	48.472385
1617.143894	150.832514	48.477389
1613.880545	146.235817	48.482394
1609.689496	146.968594	48.487399
1606.795497	144.846280	48.492404
1603.079908	149.331632	48.497409
1599.983035	151.927461	48.502413
1596.379758	148.585380	48.507418
1592.456169	158.072119	48.512423
1589.204080	145.431641	48.517428
1585.968461	142.226554	48.522433
1581.954974	139.524943	48.527437
1578.724431	143.378012	48.532442
1574.891339	149.054004	48.537447
1571.846629	142.286208	48.542452
1568.392065	146.627022	48.547457
1564.813815	147.910193	48.552461
1561.372349	137.606739	48.557466
1557.372592	150.836568	48.562471
1553.992638	140.038686	48.567476
1550.307688	145.761455	48.572481
1547.200626	145.613236	48.577485
1543.852327	147.107071	48.582490
1539.974102	151.518110	48.587495
1536.552445	147.417295	48.592500
1533.116433	146.992506	48.597505
1529.543190	149.560732	48.602509
1526.345291	147.312860	48.607514
1522.553143	159.277418	48.612519
1518.982810	146.752735	48.617524
1515.545470	150.294480	48.622529
1511.909935	148.973214	48.627533
1508.765178	148.754090	48.632538
1505.237543	148.260001	48.637543
1501.679137	147.191615	48.642548
1498.098525	151.832148	48.647553
1494.743877	148.528589	48.652557
1491.381581	144.378336	48.657562
1487.328458	158.454150	48.662567
1484.336180	143.185299	48.667572
1480.539368	146.989337	48.672577
1476.846929	140.940993	48.677581
1473.656783	144.673986	48.682586
1469.954145	153.042491	48.687591
1467.030953	147.132646	48.692596
1463.388252	150.491886	48.697601
1459.611733	145.323172	48.702605
1456.108906	151.271467	48.707610
1452.199183	153.889833	48.712615
1448.754142	141.174011	48.717620
1445.230625	153.173159	48.722625
1441.927436	149.230838	48.727629
1438.794257	138.469233	48.732634
1434.996372	142.286902	48.737639
1432.068025	146.940257	48.742644
1427.960105	150.886330	48.747649
1424.572751	150.058312	48.752653
1421.253579	146.702375	48.757658
1417.587616	148.610322	48.762663
1414.484137	140.124858	48.767668
1410.619743	139.982111	48.772673
1406.980580	134.632876	48.777677
1403.254289	141.406501	48.782682
1399.489229	143.011547	48.787687
1396.397737	136.084074	48.792692
1393.139040	144.847344	48.797697
1389.808021	146.992213	48.802701
1386.093484	140.359532	48.807706
1381.894030	135.524435	48.812711
1378.914986	137.689085	48.817716
1375.277617	137.195670	48.822721
1372.109064	134.121937	48.827725
1369.033777	136.530228	48.832730
1365.227439	141.533375	48.837735
1361.635772	134.455345	48.842740
1358.201839	141.236331	48.847745
1354.430999	135.876738	48.852749
1351.088550	141.691638	48.857754
1347.136481	147.712681	48.862759
1343.973783	137.243947	48.867764
1340.237441	137.228689	48.872769
1337.038834	140.696170	48.877773
1333.487979	136.315735	48.882778
1329.981769	140.956719	48.887783
1326.641107	131.388073	48.892788
1322.891622	147.485262	48.897793
1319.231151	143.544666	48.902797
1315.859143	129.047175	48.907802
1312.690535	135.694348	48.912807
1309.523682	135.499930	48.917812
1305.675375	127.762047	48.922817
1301.650373	123.133422	48.927821
1298.322194	127.083522	48.932826
1294.532602	136.750988	48.937831
1291.427540	123.344486	48.942836
1287.986575	133.314863	48.947841
1284.902175	133.200372	48.952845
1281.397485	126.674791	48.957850
1277.667355	129.283147	48.962855
1273.708622	126.521851	48.967860
1269.982286	128.129677	48.972865
1266.517668	131.748132	48.977869
1263.660002	125.523114	48.982874
1259.970482	135.562422	48.987879
1256.787668	131.108978	48.992884
1252.983197	132.460171	48.997889
1249.624518	131.446586	49.002893
1245.996430	136.954945	49.007898
1242.155473	128.196657	49.012903
1238.456556	129.970475	49.017908
1235.199478	132.087243	49.022913
1232.098888	126.823378	49.027917
1228.545046	132.615285	49.032922
1225.138375	136.945460	49.037927
1221.528201	120.166350	49.042932
1217.674097	129.550696	49.047937
1214.285486	134.828073	49.052941
1210.814142	124.607224	49.057946
1207.135578	132.566202	49.062951
1204.045388	125.074673	49.067956
1200.294804	134.005411	49.072961
1196.858970	131.210034	49.077965
1193.753333	136.372169	49.082970
1189.682846	132.160048	49.087975
1186.343704	122.330196	49.092980
1182.834358	129.568956	49.097985
1179.327096	125.952836	49.102989
1175.871828	125.382905	49.107994
1172.278788	131.290853	49.112999
1169.243311	122.410327	49.118004
1165.392614	129.225213	49.123009
1161.687491	124.472793	49.128013
1158.034514	124.632557	49.133018
1154.525841	124.777544	49.138023
1151.403786	119.901703	49.143028
1147.761810	138.133578	49.148033
1144.143483	132.708109	49.153037
1140.630118	133.863854	49.158042
1137.122661	139.359652	49.163047
1133.774113	134.983824	49.168052
1130.481908	131.458088	49.173057
1127.051843	127.428060	49.178061
1123.416168	132.200906	49.183066
1119.453694	142.220718	49.188071
1116.234263	129.986701	49.193076
1112.567877	123.813603	49.198081
1109.125894	127.752062	49.203085
1105.912414	121.016470	49.208090
1102.217535	125.936268	49.213095
1098.774011	120.934828	49.218100
1095.465187	125.321731	49.223105
1091.882371	133.308969	49.228109
1088.454830	123.689770	49.233114
1084.768226	125.383923	49.238119
1081.280229	127.422550	49.243124
1077.571519	127.222770	49.248129
1073.955651	123.774867	49.253133
1070.702843	121.963641	49.258138
1067.118810	123.949484	49.263143
1063.516413	122.117132	49.268148
1060.379892	123.817440	49.273153
1056.774883	135.636119	49.278157
1053.541824	123.830858	49.283162
1049.893999	125.096129	49.288167
1046.443274	125.712528	49.293172
1042.868603	133.063817	49.298177
1039.303641	130.071266	49.303181
1035.804980	120.526036	49.308186
1032.142082	125.009221	49.313191
1028.753017	120.004162	49.318196
1025.354434	135.225943	49.323201
1021.719946	124.796813	49.328205
1018.465517	124.162022	49.333210
1014.496688	134.736295	49.338215
1011.259570	120.289007	49.343220
1007.522054	125.210204	49.348225
1003.717752	129.792177	49.353229
1000.391683	126.348709	49.358234
997.210528	130.274113	49.363239
994.192117	121.448719	49.368244
990.396975	126.164362	49.373249
986.193048	129.517705	49.378253
983.197112	123.885065	49.383258
979.398603	128.756776	49.388263
976.152384	120.315986	49.393268
972.624805	126.834076	49.398273
969.506800	126.698914	49.403277
965.633928	123.453840	49.408282
961.829470	131.563662	49.413287
958.536086	127.672589	49.418292
954.883903	123.804544	49.423297
951.483569	126.791380	49.428301
948.463279	126.176135	49.433306
944.808614	128.794772	49.438311
941.390093	118.342438	49.443316
937.493947	128.162168	49.448321
934.115969	130.717099	49.453325
930.386147	128.459158	49.458330
927.125693	123.756938	49.463335
923.472174	115.829730	49.468340
920.201630	126.769893	49.473345
916.354620	113.931407	49.478349
913.158934	117.023942	49.483354
909.310973	127.544163	49.488359
906.027895	117.235027	49.493364
902.714029	111.663515	49.498369
899.051842	123.259681	49.503373
895.959999	116.133146	49.508378
891.903000	121.756508	49.513383
888.682224	114.069556	49.518388
885.069747	120.008355	49.523393
881.497063	125.511569	49.528397
878.261239	114.093702	49.533402
874.211767	121.616974	49.538407
870.915309	121.010752	49.543412
867.830729	116.956949	49.548417
864.045154	110.247301	49.553421
860.506406	111.388515	49.558426
856.883166	116.204494	49.563431
853.659215	113.014803	49.568436
849.807759	114.578737	49.573441
846.281113	122.224145	49.578445
843.137281	109.852563	49.583450
839.769398	122.171086	49.588455
836.228828	111.076182	49.593460
832.358809	115.815582	49.598465
828.530498	117.537522	49.603469
825.495641	116.499708	49.608474
822.082304	121.938326	49.613479
818.525364	114.514037	49.618484
815.125648	112.844915	49.623489
811.361993	115.904575	49.628493
808.041960	122.462651	49.633498
804.595654	125.713933	49.638503
801.405247	108.792211	49.643508
797.500848	119.108722	49.648513
794.016786	113.582617	49.653517
790.547659	118.118988	49.658522
787.002208	123.632764	49.663527
783.544703	115.424814	49.668532
779.802662	123.196672	49.673537
776.054268	122.898922	49.678541
773.300011	107.207899	49.683546
769.516337	127.191506	49.688551
765.968896	113.252803	49.693556
762.455521	114.252156	49.698561
758.685090	114.844304	49.703565
755.343908	117.883855	49.708570
751.840285	123.848954	49.713575
748.692877	110.961613	49.718580
745.042996	119.037344	49.723585
741.436510	123.740726	49.728589
738.082279	124.423294	49.733594
734.287897	122.306050	49.738599
731.158849	116.579386	49.743604
727.314708	117.232101	49.748609
723.766634	124.323666	49.753613
720.462076	119.093533	49.758618
716.598327	123.817587	49.763623
713.136125	118.419161	49.768628
709.952813	122.481867	49.773633
706.362839	114.815880	49.778637
702.659061	119.252405	49.783642
699.428981	121.627343	49.788647
696.020847	117.927735	49.793652
692.590844	114.253653	49.798657
689.105510	115.266185	49.803661
685.474755	118.063213	49.808666
681.873537	120.176324	49.813671
678.370549	115.055619	49.818676
674.804255	115.485403	49.823681
671.160622	114.343771	49.828685
668.088863	103.414589	49.833690
664.080556	121.037787	49.838695
660.735855	114.825296	49.843700
657.461486	121.962403	49.848705
653.859456	122.813312	49.853709
650.519221	113.979861	49.858714
646.839462	121.188778	49.863719
643.062968	121.276254	49.868724
639.646573	120.213877	49.873729
636.281097	116.359259	49.878733
633.008183	108.356525	49.883738
629.678628	120.994639	49.888743
626.065966	115.088965	49.893748
622.233780	117.652570	49.898753
618.513835	127.480889	49.903757
615.276889	111.510102	49.908762
611.388325	122.884228	49.913767
608.110753	115.432059	49.918772
604.386416	114.572607	49.923777
600.863750	120.303570	49.928781
597.858365	105.772935	49.933786
594.485848	117.019460	49.938791
591.120742	118.577150	49.943796
587.547851	114.073120	49.948801
583.493585	115.791016	49.953805
580.222164	108.476386	49.958810
576.748597	115.266039	49.963815
573.217025	117.864013	49.968820
570.075324	109.723587	49.973825
566.077847	121.079851	49.978829
563.026007	118.215333	49.983834
559.292288	113.958756	49.988839
555.454249	114.473857	49.993844
552.366184	117.727225	49.998849
548.676158	118.307826	50.003853
545.225307	113.755421	50.008858
541.568409	114.544261	50.013863
538.592153	119.148847	50.018868
535.123867	116.634262	50.023873
531.030290	114.373316	50.028877
527.538678	112.489928	50.033882
524.198442	112.149722	50.038887
520.300468	123.556062	50.043892
517.172256	108.291204	50.048897
513.780454	121.636681	50.053901
510.691650	106.459044	50.058906
506.488447	119.089650	50.063911
503.124013	119.809803	50.068916
499.746619	123.920752	50.073921
495.872940	122.585267	50.078925
492.963351	124.796022	50.083930
489.326053	120.793507	50.088935
485.942745	120.651675	50.093940
482.255381	118.860903	50.098945
478.384430	122.957635	50.103949
474.867923	116.819904	50.108954
471.656886	122.225494	50.113959
468.128342	111.141571	50.118964
464.776347	112.731917	50.123969
461.076848	116.553226	50.128973
458.491074	109.342305	50.133978
454.145160	115.023718	50.138983
450.507123	109.212980	50.143988
446.850471	111.538510	50.148993
443.272588	118.147201	50.153997
440.311182	107.936989	50.159002
436.770489	117.032075	50.164007
433.555609	108.827699	50.169012
430.126262	114.421391	50.174017
426.262643	109.656588	50.179021
422.659888	110.385654	50.184026
418.890082	115.261550	50.189031
415.214660	104.273621	50.194036
411.657141	110.172305	50.199041
408.521467	115.607300	50.204045
405.280686	101.158018	50.209050
401.938597	117.615996	50.214055
397.973795	110.963085	50.219060
394.214230	110.108264	50.224065
390.479574	112.795244	50.229069
387.683036	107.834934	50.234074
384.521436	112.855883	50.239079
380.792042	108.368070	50.244084
377.381277	107.893030	50.249089
373.705554	114.237946	50.254093
370.103598	111.257610	50.259098
366.338235	121.550067	50.264103
362.699199	104.850014	50.269108
359.596505	114.184454	50.274113
355.870300	102.161084	50.279117
352.590206	100.588369	50.284122
348.943069	106.532716	50.289127
345.543080	101.412423	50.294132
342.210821	110.010522	50.299137
338.518494	110.309689	50.304141
334.912406	111.345052	50.309146
331.267661	118.234455	50.314151
328.215620	115.556821	50.319156
324.965739	112.869509	50.324161
321.065312	113.503675	50.329165
317.888696	105.830606	50.334170
314.168224	106.983191	50.339175
310.625279	107.246409	50.344180
306.715493	108.148145	50.349185
303.102821	108.805346	50.354189
299.809523	106.036045	50.359194
296.293905	113.681798	50.364199
292.987487	107.460518	50.369204
289.611614	107.814895	50.374209
285.806898	114.459474	50.379213
282.666471	109.601151	50.384218
278.621171	117.213429	50.389223
275.640754	112.902081	50.394228
272.305784	107.654460	50.399233
268.558424	107.035519	50.404237
265.346828	98.625122	50.409242
261.354258	106.017533	50.414247
257.868920	109.625166	50.419252
254.131185	104.821535	50.424257
250.855408	110.534782	50.429261
247.497243	104.358417	50.434266
243.604296	106.728753	50.439271
240.714004	105.517251	50.444276
237.008476	93.925906	50.449281
233.447712	105.203821	50.454285
230.164165	102.007903	50.459290
226.487721	108.456456	50.464295
223.005955	104.046593	50.469300
219.433614	105.305571	50.474305
215.787564	104.447509	50.479309
212.356403	101.127053	50.484314
208.656914	106.115406	50.489319
205.483665	102.260305	50.494324
202.298482	103.459154	50.499329
198.417438	108.389165	50.504333
195.399886	99.114345	50.509338
191.427852	103.455973	50.514343
187.896150	95.169478	50.519348
184.230474	95.634666	50.524353
180.646598	103.603194	50.529357
176.965988	96.542142	50.534362
173.593446	110.031456	50.539367
170.029004	106.486233	50.544372
166.607735	113.243058	50.549377
163.264844	109.465406	50.554381
159.939976	106.629613	50.559386
156.180233	106.911090	50.564391
152.890847	103.300613	50.569396
149.339567	104.298245	50.574401
145.644874	106.644529	50.579405
142.419023	98.230479	50.584410
138.514286	110.097821	50.589415
135.668648	102.451607	50.594420
131.929005	97.875738	50.599425
128.423526	105.775481	50.604429
125.006655	98.656407	50.609434
121.433703	106.186273	50.614439
118.049496	97.278484	50.619444
114.387261	106.477394	50.624449
110.691905	110.017890	50.629453
107.496216	106.152767	50.634458
103.831659	108.181716	50.639463
100.263384	110.578347	50.644468
96.392218	97.981514	50.649473
92.989048	107.050721	50.654477
89.508005	105.836886	50.659482
86.255502	105.207215	50.664487
83.065070	106.861877	50.669492
79.637003	100.983958	50.674497
75.909737	110.534661	50.679501
72.675810	106.452119	50.684506
68.671357	107.497421	50.689511
64.991234	108.963814	50.694516
61.844834	112.601124	50.699521
57.987266	106.943323	50.704525
54.794927	105.579102	50.709530
51.206969	111.387198	50.714535
47.791805	106.752548	50.719540
44.626105	101.117352	50.724545
40.494480	110.135335	50.729549
37.128134	104.738596	50.734554
33.647039	97.507298	50.739559
30.186402	95.825215	50.744564
26.747626	100.760680	50.749569
23.061902	103.459403	50.754573
19.713036	101.826309	50.759578
16.100569	93.477570	50.764583
12.782609	100.515964	50.769588
9.455596	101.873613	50.774593
5.785027	103.271973	50.779597
2.477428	90.762881	50.784602