Mon Mar 08 19:15:17 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.124009	99.548438	0.000000
-1.258653	78.475916	0.005005
-1.947809	47.545116	0.010010
-3.859551	-3.960785	0.015014
-7.350792	-40.516866	0.020019
-12.655348	-40.041767	0.025024
-17.879315	-43.605177	0.030029
-22.696852	-40.872444	0.035034
-26.876947	-36.100037	0.040038
-30.486020	-48.921600	0.045043
-34.511312	-40.421003	0.050048
-38.009863	-42.573961	0.055053
-41.497691	-33.853178	0.060058
-45.369117	-29.897896	0.065062
-48.962074	-38.158640	0.070067
-52.726313	-25.842707	0.075072
-56.257403	-30.672651	0.080077
-60.047884	-34.672790	0.085082
-63.894490	-34.386009	0.090086
-67.847682	-41.614768	0.095091
-71.882062	-29.853337	0.100096
-75.298503	-37.203981	0.105101
-78.790064	-43.380504	0.110106
-82.691924	-44.341616	0.115110
-86.242588	-42.793240	0.120115
-90.783997	-29.263674	0.125120
-94.353414	-35.739970	0.130125
-97.904830	-33.795670	0.135130
-101.902595	-27.073294	0.140134
-105.232335	-38.351435	0.145139
-109.228879	-34.363479	0.150144
-112.952894	-44.809202	0.155149
-116.731923	-42.819099	0.160154
-120.587445	-42.407813	0.165158
-124.183912	-44.642785	0.170163
-128.211960	-44.727469	0.175168
-131.893746	-39.905094	0.180173
-134.911715	-44.515610	0.185178
-139.394159	-47.906930	0.190182
-143.114252	-48.277251	0.195187
-147.192195	-36.808357	0.200192
-151.019645	-40.800872	0.205197
-154.799711	-26.981123	0.210202
-158.548190	-27.775791	0.215206
-161.582059	-40.430331	0.220211
-165.673557	-34.493932	0.225216
-169.344425	-42.152315	0.230221
-173.205910	-32.783571	0.235226
-177.044298	-33.735739	0.240230
-180.680798	-25.609160	0.245235
-184.692226	-31.063952	0.250240
-188.382097	-45.856025	0.255245
-192.199027	-27.195768	0.260250
-195.990787	-20.783638	0.265254
-199.082639	-33.655943	0.270259
-203.188910	-29.257692	0.275264
-206.944646	-42.648457	0.280269
-210.702363	-19.806390	0.285274
-214.675296	-38.090097	0.290278
-218.307284	-32.747301	0.295283
-222.100463	-30.370029	0.300288
-225.900807	-42.682972	0.305293
-229.703302	-28.302917	0.310298
-233.274729	-33.268070	0.315302
-237.088215	-42.310119	0.320307
-241.070255	-28.418594	0.325312
-244.847919	-28.948292	0.330317
-248.584880	-38.338403	0.335322
-252.058903	-38.287395	0.340326
-256.074828	-32.340835	0.345331
-259.849167	-33.569578	0.350336
-263.552547	-46.662693	0.355341
-267.202628	-43.647500	0.360346
-271.190684	-31.475297	0.365350
-274.719787	-31.503768	0.370355
-278.608790	-30.751021	0.375360
-281.940159	-35.098452	0.380365
-285.989945	-35.184134	0.385370
-289.835324	-41.267595	0.390374
-293.675198	-35.934083	0.395379
-297.579043	-27.734706	0.400384
-301.111717	-38.388846	0.405389
-304.798358	-39.554251	0.410394
-308.853987	-23.577339	0.415398
-312.591939	-29.870289	0.420403
-316.406168	-26.880853	0.425408
-319.919698	-35.166464	0.430413
-323.430676	-33.713957	0.435418
-327.480868	-37.322148	0.440422
-330.944691	-33.595481	0.445427
-334.997699	-28.907494	0.450432
-338.896439	-31.436061	0.455437
-342.583616	-24.029659	0.460442
-346.772836	-37.494479	0.465446
-350.140239	-32.275727	0.470451
-353.699854	-30.498468	0.475456
-357.382755	-35.043540	0.480461
-361.299006	-35.695998	0.485466
-365.049801	-23.883198	0.490470
-368.736386	-34.583620	0.495475
-372.809302	-28.501626	0.500480
-376.194853	-31.443200	0.505485
-380.289969	-35.394184	0.510490
-384.105116	-31.636580	0.515494
-387.394972	-29.919687	0.520499
-391.640392	-29.384220	0.525504
-395.346649	-43.356529	0.530509
-398.743811	-36.362181	0.535514
-402.703651	-27.751610	0.540518
-406.147930	-39.556592	0.545523
-410.511895	-30.867293	0.550528
-414.053895	-27.563232	0.555533
-417.795846	-32.929771	0.560538
-421.641927	-28.292027	0.565542
-425.054611	-32.178450	0.570547
-428.873350	-19.736590	0.575552
-432.832932	-28.442776	0.580557
-436.739323	-30.761818	0.585562
-440.458209	-26.060783	0.590566
-443.991971	-42.539334	0.595571
-447.787111	-39.327257	0.600576
-451.463495	-38.642874	0.605581
-455.285919	-30.424721	0.610586
-459.376705	-30.989227	0.615590
-462.913407	-33.662129	0.620595
-466.898763	-32.270843	0.625600
-470.468295	-43.549556	0.630605
-474.180530	-35.218098	0.635610
-478.000081	-37.656586	0.640614
-481.556487	-43.910444	0.645619
-485.320501	-26.291055	0.650624
-489.192556	-26.879404	0.655629
-493.085493	-38.415494	0.660634
-497.012041	-29.393811	0.665638
-500.498826	-40.138534	0.670643
-504.172515	-36.349724	0.675648
-508.120444	-33.512088	0.680653
-511.833240	-31.224469	0.685658
-515.470430	-38.261673	0.690662
-519.427164	-37.434647	0.695667
-523.341356	-30.024839	0.700672
-526.859396	-31.412356	0.705677
-530.732352	-44.602506	0.710682
-534.418214	-30.820921	0.715686
-537.863286	-36.031271	0.720691
-541.965598	-29.775585	0.725696
-545.689325	-36.303795	0.730701
-549.244853	-34.916379	0.735706
-553.148464	-26.273557	0.740710
-556.822312	-39.486008	0.745715
-560.742585	-28.450043	0.750720
-564.663622	-33.171197	0.755725
-568.200372	-38.671184	0.760730
-572.278683	-33.105203	0.765734
-575.696431	-35.421650	0.770739
-579.456999	-34.696817	0.775744
-583.361064	-34.951919	0.780749
-586.669916	-32.086943	0.785754
-590.908444	-27.069302	0.790758
-594.524399	-35.990928	0.795763
-598.620563	-33.840615	0.800768
-602.497107	-35.834591	0.805773
-606.077573	-27.216505	0.810778
-609.645842	-25.940495	0.815782
-613.123839	-25.782681	0.820787
-617.352272	-44.488399	0.825792
-621.265808	-31.069258	0.830797
-624.450067	-27.505101	0.835802
-628.640798	-34.406387	0.840806
-632.040168	-32.974416	0.845811
-636.012439	-33.623778	0.850816
-639.918709	-34.006157	0.855821
-643.200481	-32.104142	0.860826
-647.158056	-32.522464	0.865830
-650.770901	-38.841153	0.870835
-654.837170	-27.980398	0.875840
-658.728134	-26.266434	0.880845
-661.820072	-35.467203	0.885850
-665.798916	-28.403206	0.890854
-669.602923	-43.231412	0.895859
-673.888939	-27.953517	0.900864
-677.233121	-27.771263	0.905869
-681.218429	-32.142931	0.910874
-684.976427	-41.552603	0.915878
-688.974695	-35.677548	0.920883
-692.328782	-32.081438	0.925888
-696.234995	-27.476231	0.930893
-699.812838	-32.247263	0.935898
-703.888790	-31.169088	0.940902
-707.343568	-32.993763	0.945907
-711.085748	-32.257470	0.950912
-714.949628	-31.145360	0.955917
-718.373922	-36.008703	0.960922
-722.786099	-24.673126	0.965926
-726.172238	-35.799400	0.970931
-729.827605	-29.151240	0.975936
-733.597634	-33.994000	0.980941
-737.764795	-30.879701	0.985946
-741.921590	-31.067347	0.990950
-745.079006	-35.530211	0.995955
-748.808001	-39.660470	1.000960
-752.061366	-30.183049	1.005965
-755.969141	-30.169212	1.010970
-760.017409	-25.612158	1.015974
-763.761430	-30.693973	1.020979
-767.754914	-28.293298	1.025984
-771.478414	-28.759859	1.030989
-774.970418	-33.558683	1.035994
-779.385130	-20.264183	1.040998
-782.811455	-35.247170	1.046003
-786.764459	-26.214501	1.051008
-790.339835	-30.831257	1.056013
-793.762999	-37.960563	1.061018
-797.809837	-42.265426	1.066022
-801.386204	-33.933127	1.071027
-805.551873	-21.153012	1.076032
-809.050826	-33.491051	1.081037
-812.747762	-35.790908	1.086042
-816.450631	-35.032350	1.091046
-819.804374	-36.578141	1.096051
-823.832603	-30.026349	1.101056
-827.663566	-24.806960	1.106061
-831.689810	-25.758000	1.111066
-835.908818	-29.350938	1.116070
-838.815041	-16.015210	1.121075
-842.718629	-25.576381	1.126080
-846.833640	-33.865934	1.131085
-850.180760	-29.595839	1.136090
-854.124280	-20.764833	1.141094
-857.549650	-31.665456	1.146099
-861.637637	-33.864879	1.151104
-865.203841	-32.092118	1.156109
-869.376052	-28.131607	1.161114
-873.653479	-22.913305	1.166118
-876.870773	-21.789191	1.171123
-880.512747	-30.032893	1.176128
-884.178439	-26.541230	1.181133
-887.782910	-31.596269	1.186138
-891.602843	-27.955367	1.191142
-895.410859	-36.103114	1.196147
-899.613923	-20.412361	1.201152
-903.236095	-29.643129	1.206157
-906.588095	-30.317092	1.211162
-910.214191	-24.770812	1.216166
-914.018057	-34.694695	1.221171
-918.218442	-25.773641	1.226176
-921.975424	-25.991780	1.231181
-925.727305	-20.371752	1.236186
-929.486547	-31.438058	1.241190
-932.927530	-37.474717	1.246195
-936.829625	-32.675835	1.251200
-940.681485	-23.446223	1.256205
-944.374273	-28.589545	1.261210
-948.231847	-27.396070	1.266214
-952.080629	-39.343648	1.271219
-955.855775	-38.502358	1.276224
-959.321572	-36.275619	1.281229
-962.678161	-36.242352	1.286234
-967.244463	-35.274534	1.291238
-970.790693	-36.084489	1.296243
-974.555896	-33.626940	1.301248
-978.399723	-34.808729	1.306253
-982.008110	-41.988543	1.311258
-985.893398	-33.559276	1.316262
-989.452692	-39.332521	1.321267
-993.534451	-37.139685	1.326272
-996.922426	-31.971952	1.331277
-1000.511075	-42.688546	1.336282
-1004.497692	-36.847954	1.341286
-1008.354444	-32.871424	1.346291
-1012.342687	-38.790482	1.351296
-1015.969226	-31.580432	1.356301
-1019.646440	-41.127023	1.361306
-1023.563208	-36.765588	1.366310
-1027.297074	-30.706780	1.371315
-1030.870403	-42.624158	1.376320
-1034.961648	-44.688722	1.381325
-1038.568445	-37.196394	1.386330
-1042.325422	-25.854672	1.391334
-1045.924148	-27.835579	1.396339
-1050.041945	-31.499498	1.401344
-1053.744157	-34.488773	1.406349
-1056.918002	-47.168529	1.411354
-1060.650776	-27.870872	1.416358
-1064.623247	-46.633974	1.421363
-1068.788571	-35.733065	1.426368
-1072.405166	-22.859006	1.431373
-1076.002964	-44.387842	1.436378
-1080.006068	-23.288760	1.441382
-1083.392430	-40.114641	1.446387
-1087.477763	-40.007202	1.451392
-1091.213833	-38.653171	1.456397
-1094.674771	-32.011920	1.461402
-1098.643462	-29.313485	1.466406
-1102.233500	-44.419552	1.471411
-1106.273353	-36.892542	1.476416
-1110.106964	-35.237474	1.481421
-1113.668294	-37.405590	1.486426
-1117.477930	-30.390008	1.491430
-1121.155755	-41.754403	1.496435
-1124.742720	-31.348006	1.501440
-1128.937028	-42.782715	1.506445
-1132.541670	-34.431228	1.511450
-1136.679977	-34.277385	1.516454
-1140.228430	-36.565781	1.521459
-1143.378673	-33.028462	1.526464
-1147.451369	-24.766058	1.531469
-1151.298422	-39.714244	1.536474
-1155.052493	-36.132342	1.541478
-1158.429537	-37.226099	1.546483
-1162.424747	-31.368102	1.551488
-1166.257011	-29.126582	1.556493
-1169.767419	-37.945891	1.561498
-1174.268835	-26.557403	1.566502
-1177.486074	-39.297845	1.571507
-1181.643392	-33.585754	1.576512
-1185.302410	-34.098239	1.581517
-1188.847211	-38.594688	1.586522
-1192.810218	-39.944693	1.591526
-1196.345896	-44.571886	1.596531
-1200.495100	-36.828546	1.601536
-1204.308202	-32.674198	1.606541
-1207.684753	-38.553600	1.611546
-1211.360770	-34.011204	1.616550
-1214.807247	-44.207766	1.621555
-1218.721543	-40.349414	1.626560
-1222.968112	-32.156829	1.631565
-1226.703586	-38.883862	1.636570
-1230.721008	-30.048323	1.641574
-1234.215326	-50.752981	1.646579
-1237.478180	-43.028423	1.651584
-1241.330253	-47.333702	1.656589
-1245.073389	-42.824666	1.661594
-1249.120902	-42.147458	1.666598
-1252.904198	-43.231254	1.671603
-1256.724077	-39.719080	1.676608
-1260.556061	-43.191830	1.681613
-1263.958792	-41.075656	1.686618
-1267.982032	-31.305651	1.691622
-1271.574042	-40.826032	1.696627
-1275.426094	-36.263250	1.701632
-1279.227792	-37.386632	1.706637
-1282.819419	-62.772947	1.711642
-1286.846580	-38.845660	1.716646
-1290.770833	-40.725201	1.721651
-1294.272235	-35.969371	1.726656
-1297.971684	-30.872782	1.731661
-1301.264780	-37.908590	1.736666
-1305.386021	-45.344809	1.741670
-1309.075665	-54.598779	1.746675
-1313.461228	-33.830779	1.751680
-1317.271352	-33.760678	1.756685
-1320.652503	-42.548394	1.761690
-1324.330449	-43.341455	1.766694
-1327.783476	-50.960268	1.771699
-1331.648769	-38.239998	1.776704
-1335.500669	-40.774384	1.781709
-1339.125421	-46.243304	1.786714
-1343.411463	-32.649913	1.791718
-1347.158995	-42.271419	1.796723
-1350.955576	-38.081639	1.801728
-1354.501871	-37.952791	1.806733
-1357.956136	-43.623998	1.811738
-1361.782314	-26.848062	1.816742
-1365.982746	-33.779531	1.821747
-1369.220867	-38.837251	1.826752
-1373.073466	-48.233750	1.831757
-1377.061996	-34.700544	1.836762
-1380.891310	-30.473938	1.841766
-1384.301268	-36.636281	1.846771
-1388.284632	-34.018581	1.851776
-1392.072157	-41.624748	1.856781
-1395.533234	-43.863660	1.861786
-1399.805760	-38.068100	1.866790
-1403.433160	-41.499251	1.871795
-1406.872073	-39.228857	1.876800
-1410.754476	-34.424475	1.881805
-1414.577327	-40.823415	1.886810
-1418.395238	-37.544663	1.891814
-1421.649440	-41.609493	1.896819
-1425.767572	-36.716889	1.901824
-1429.582551	-27.650106	1.906829
-1433.651589	-31.250179	1.911834
-1437.411653	-29.828681	1.916838
-1440.632459	-43.709758	1.921843
-1444.762485	-46.505328	1.926848
-1448.522108	-33.109573	1.931853
-1452.477316	-31.190070	1.936858
-1456.419341	-36.924942	1.941862
-1459.942211	-37.357875	1.946867
-1463.393285	-34.871004	1.951872
-1467.117636	-32.829182	1.956877
-1470.610268	-38.601295	1.961882
-1474.759475	-30.199952	1.966886
-1478.380759	-38.319825	1.971891
-1482.299921	-34.999527	1.976896
-1485.928479	-43.881396	1.981901
-1489.765675	-33.469100	1.986906
-1493.487314	-36.743103	1.991910
-1497.019138	-29.263680	1.996915
-1501.658311	-27.460050	2.006912
-1502.028773	-34.204814	2.016909
-1499.778268	-36.244399	2.026906
-1496.832308	-38.471130	2.036902
-1494.911712	-44.187077	2.046899
-1493.095185	-35.395856	2.056896
-1490.968170	-29.710963	2.066893
-1488.834015	-37.213607	2.076890
-1487.313074	-35.590302	2.086886
-1485.250486	-34.094778	2.096883
-1483.512821	-34.257097	2.106880
-1481.218259	-36.982616	2.116877
-1479.696160	-30.899294	2.126874
-1477.922925	-37.496304	2.136870
-1475.744519	-29.156137	2.146867
-1473.849983	-30.085618	2.156864
-1471.926618	-29.734545	2.166861
-1470.169552	-34.724869	2.176858
-1468.414369	-31.969144	2.186854
-1466.301996	-30.150019	2.196851
-1464.492865	-27.709221	2.206848
-1462.537595	-32.983889	2.216845
-1460.544230	-31.587777	2.226842
-1458.630887	-31.514541	2.236838
-1456.893083	-31.310573	2.246835
-1455.112383	-28.074220	2.256832
-1453.197526	-31.379923	2.266829
-1451.083496	-35.312732	2.276826
-1449.452932	-37.586142	2.286822
-1447.397812	-34.725277	2.296819
-1445.458260	-36.410308	2.306816
-1443.828755	-39.392439	2.316813
-1441.724586	-39.065553	2.326810
-1439.838304	-42.469291	2.336806
-1438.095759	-38.113743	2.346803
-1436.423927	-33.434261	2.356800
-1434.270340	-34.930936	2.366797
-1432.386891	-37.511645	2.376794
-1430.546251	-38.329837	2.386790
-1428.711538	-34.983700	2.396787
-1426.859438	-39.722384	2.406784
-1424.930906	-36.358110	2.416781
-1422.525388	-37.933000	2.426778
-1421.105607	-44.511271	2.436774
-1419.165843	-37.380120	2.446771
-1417.438598	-31.252233	2.456768
-1415.814546	-33.905076	2.466765
-1413.765445	-38.065861	2.476762
-1411.900441	-37.722761	2.486758
-1409.822494	-32.050458	2.496755
-1407.795585	-34.013108	2.506752
-1405.917356	-36.564541	2.516749
-1404.227433	-35.547664	2.526746
-1402.219719	-37.436189	2.536742
-1400.579189	-35.596724	2.546739
-1398.849994	-35.666050	2.556736
-1396.725921	-35.165479	2.566733
-1394.537775	-34.514123	2.576730
-1392.932118	-40.414820	2.586726
-1391.441054	-39.075593	2.596723
-1389.357260	-35.658780	2.606720
-1387.086454	-37.355742	2.616717
-1385.239989	-38.673742	2.626714
-1383.370733	-36.820357	2.636710
-1381.616278	-37.133697	2.646707
-1379.854039	-40.699097	2.656704
-1377.995399	-42.074299	2.666701
-1375.852776	-41.186707	2.676698
-1374.053712	-45.749503	2.686694
-1372.310361	-42.399747	2.696691
-1370.434832	-46.106423	2.706688
-1368.655454	-43.806040	2.716685
-1366.859277	-46.263785	2.726682
-1364.410599	-45.886194	2.736678
-1363.191177	-39.466991	2.746675
-1360.916544	-45.010575	2.756672
-1359.189058	-42.853445	2.766669
-1357.018704	-43.383329	2.776666
-1355.675861	-42.805033	2.786662
-1353.172525	-43.490838	2.796659
-1351.682086	-44.112395	2.806656
-1350.092476	-35.780476	2.816653
-1347.691034	-39.879191	2.826650
-1345.953209	-39.735138	2.836646
-1344.358064	-39.677185	2.846643
-1342.296805	-36.136728	2.856640
-1339.976795	-36.928955	2.866637
-1338.645561	-46.428058	2.876634
-1336.681109	-38.250859	2.886630
-1334.604012	-41.495597	2.896627
-1332.887478	-36.763195	2.906624
-1330.918527	-35.262015	2.916621
-1328.971735	-37.813309	2.926618
-1327.123903	-33.791867	2.936614
-1325.372647	-36.539214	2.946611
-1323.282031	-40.529737	2.956608
-1321.734789	-33.075160	2.966605
-1319.792408	-42.091063	2.976602
-1318.054571	-36.503174	2.986598
-1315.978920	-35.862155	2.996595
-1313.937042	-35.048373	3.006592
-1312.077518	-37.456222	3.016589
-1310.183754	-39.433791	3.026586
-1308.380702	-36.418778	3.036582
-1306.630417	-33.641615	3.046579
-1304.471674	-30.966137	3.056576
-1302.843738	-36.008301	3.066573
-1300.841894	-43.494343	3.076570
-1299.206193	-39.563656	3.086566
-1297.219852	-33.194527	3.096563
-1295.678912	-44.866493	3.106560
-1293.496397	-32.936529	3.116557
-1291.407240	-46.047713	3.126554
-1289.659394	-34.343422	3.136550
-1287.488253	-45.137365	3.146547
-1285.870655	-39.036032	3.156544
-1284.137937	-33.469398	3.166541
-1282.291934	-41.453081	3.176538
-1280.124586	-39.006310	3.186534
-1278.516116	-38.380484	3.196531
-1276.678773	-31.900654	3.206528
-1274.262280	-42.028115	3.216525
-1272.789083	-40.599114	3.226522
-1271.095021	-40.624830	3.236518
-1269.075937	-36.968616	3.246515
-1267.065955	-37.711155	3.256512
-1265.334539	-30.982274	3.266509
-1263.315509	-31.964662	3.276506
-1261.400506	-43.090200	3.286502
-1259.528412	-41.445573	3.296499
-1257.864547	-44.082575	3.306496
-1255.917184	-37.225627	3.316493
-1254.133524	-40.098097	3.326490
-1252.035429	-41.418368	3.336486
-1250.254743	-39.699109	3.346483
-1248.482412	-43.523378	3.356480
-1246.667010	-42.030709	3.366477
-1244.448026	-37.812819	3.376474
-1242.736604	-50.168830	3.386470
-1240.826542	-47.241935	3.396467
-1238.973666	-39.111522	3.406464
-1237.112949	-37.954493	3.416461
-1235.252261	-36.710623	3.426458
-1233.541382	-34.670728	3.436454
-1231.415033	-38.126929	3.446451
-1229.563515	-38.670406	3.456448
-1227.752224	-43.902900	3.466445
-1225.671109	-40.706541	3.476442
-1223.833255	-35.011429	3.486438
-1222.481272	-35.113414	3.496435
-1220.371489	-38.724838	3.506432
-1218.285440	-37.948036	3.516429
-1216.449394	-36.644948	3.526426
-1214.571969	-38.387737	3.536422
-1212.780604	-41.075108	3.546419
-1210.716809	-45.312276	3.556416
-1208.930378	-38.006406	3.566413
-1207.042426	-33.626571	3.576410
-1205.409916	-43.639575	3.586406
-1203.539293	-45.769660	3.596403
-1201.266653	-41.369275	3.606400
-1199.367015	-39.916886	3.616397
-1197.824341	-34.108210	3.626394
-1195.897081	-36.711530	3.636390
-1194.023685	-33.090353	3.646387
-1191.898890	-31.937647	3.656384
-1190.284343	-38.764838	3.666381
-1188.115282	-44.963954	3.676378
-1186.567303	-44.544686	3.686374
-1184.556670	-39.357152	3.696371
-1182.828494	-33.249747	3.706368
-1180.741399	-42.825505	3.716365
-1178.767613	-40.072950	3.726362
-1176.935781	-44.874513	3.736358
-1175.206925	-46.936107	3.746355
-1173.264665	-44.956870	3.756352
-1171.739097	-39.503836	3.766349
-1169.818455	-46.062637	3.776346
-1167.487864	-48.201551	3.786342
-1165.687875	-41.011492	3.796339
-1164.139056	-46.304570	3.806336
-1161.904073	-40.941345	3.816333
-1159.980429	-44.513461	3.826330
-1158.352058	-43.660225	3.836326
-1156.325002	-38.314251	3.846323
-1154.600905	-42.462291	3.856320
-1152.787761	-37.877824	3.866317
-1150.698116	-37.158374	3.876314
-1148.967238	-35.639472	3.886310
-1147.051258	-37.031559	3.896307
-1145.145929	-35.628978	3.906304
-1143.315743	-32.310297	3.916301
-1141.444144	-36.922422	3.926298
-1139.420478	-35.755069	3.936294
-1137.265074	-35.729763	3.946291
-1136.038998	-37.163040	3.956288
-1133.892881	-31.498218	3.966285
-1131.997186	-34.666397	3.976282
-1129.993698	-39.211197	3.986278
-1128.131117	-43.244014	3.996275
-1126.512147	-33.593551	4.006272
-1124.454851	-36.749684	4.016269
-1122.557549	-38.481370	4.026266
-1121.054013	-44.951306	4.036262
-1119.087546	-40.613955	4.046259
-1117.182623	-36.723039	4.056256
-1115.076982	-41.061551	4.066253
-1113.139112	-38.298456	4.076250
-1111.238535	-39.856985	4.086246
-1109.597374	-35.489689	4.096243
-1107.654924	-38.316405	4.106240
-1105.712420	-37.526011	4.116237
-1104.054557	-37.653175	4.126234
-1101.950564	-39.155821	4.136230
-1100.030546	-44.340882	4.146227
-1098.186299	-41.828042	4.156224
-1096.783983	-38.166164	4.166221
-1094.428662	-41.587822	4.176218
-1092.447173	-37.448624	4.186214
-1090.645568	-38.345561	4.196211
-1088.997811	-38.684241	4.206208
-1086.908195	-44.804251	4.216205
-1085.158753	-43.263009	4.226202
-1083.365999	-36.676414	4.236198
-1081.436521	-43.579171	4.246195
-1079.436393	-39.354528	4.256192
-1077.408171	-38.675709	4.266189
-1075.812603	-40.049644	4.276186
-1073.728073	-41.781240	4.286182
-1072.004257	-40.101688	4.296179
-1069.846252	-34.923408	4.306176
-1068.315015	-37.330660	4.316173
-1066.553036	-42.204648	4.326170
-1064.540960	-35.012108	4.336166
-1062.717428	-35.628340	4.346163
-1060.525103	-42.011056	4.356160
-1058.625083	-40.282314	4.366157
-1057.065776	-37.504407	4.376154
-1054.989522	-43.270173	4.386150
-1053.168324	-47.446302	4.396147
-1051.538470	-38.171707	4.406144
-1049.298926	-41.494282	4.416141
-1047.617966	-45.014865	4.426138
-1045.990919	-41.120495	4.436134
-1043.988526	-41.893205	4.446131
-1041.900295	-45.982570	4.456128
-1040.129509	-44.139992	4.466125
-1038.108229	-41.710676	4.476122
-1036.163289	-42.952578	4.486118
-1034.528825	-37.886309	4.496115
-1032.507294	-40.570885	4.506112
-1030.807544	-44.195507	4.516109
-1028.757028	-45.627960	4.526106
-1026.934320	-44.197858	4.536102
-1025.221326	-44.624289	4.546099
-1022.968275	-45.759151	4.556096
-1021.242300	-45.057206	4.566093
-1019.591677	-47.117229	4.576090
-1017.596470	-42.446512	4.586086
-1015.754661	-36.808692	4.596083
-1013.703655	-32.513182	4.606080
-1011.928646	-38.893851	4.616077
-1010.131761	-38.171661	4.626074
-1008.097835	-46.848312	4.636070
-1006.149823	-44.719861	4.646067
-1004.417087	-38.065185	4.656064
-1002.763589	-33.174027	4.666061
-1000.475741	-43.762205	4.676058
-998.681985	-39.264503	4.686054
-996.986932	-36.287224	4.696051
-995.161061	-36.502753	4.706048
-993.289181	-49.108469	4.716045
-991.358318	-47.454072	4.726042
-989.212796	-45.601912	4.736038
-987.813219	-48.100154	4.746035
-985.415430	-44.475824	4.756032
-983.684388	-43.345218	4.766029
-982.113622	-43.090497	4.776026
-979.985610	-46.153610	4.786022
-977.913690	-39.741033	4.796019
-976.336374	-37.111203	4.806016
-974.616234	-38.771813	4.816013
-972.345646	-37.050153	4.826010
-970.801662	-37.440045	4.836006
-968.883420	-35.633620	4.846003
-966.810671	-42.383949	4.856000
-965.171726	-41.495953	4.865997
-963.272231	-36.751462	4.875994
-961.187410	-42.147494	4.885990
-959.047150	-38.845088	4.895987
-957.715126	-38.432184	4.905984
-955.815675	-40.760882	4.915981
-953.719593	-41.087475	4.925978
-952.050101	-35.019442	4.935974
-949.676713	-42.139913	4.945971
-948.041367	-39.113579	4.955968
-946.112843	-34.065841	4.965965
-944.430467	-35.172534	4.975962
-942.920548	-41.941790	4.985958
-940.908468	-46.333083	4.995955
-938.812664	-36.101915	5.005952
-936.756613	-35.081656	5.015949
-934.857996	-39.319023	5.025946
-932.997762	-35.346596	5.035942
-931.178423	-35.208948	5.045939
-929.347864	-37.400304	5.055936
-927.473408	-34.123258	5.065933
-925.510527	-41.628041	5.075930
-923.845320	-32.150584	5.085926
-921.753515	-42.249487	5.095923
-920.219118	-36.914517	5.105920
-918.228484	-43.616942	5.115917
-916.295002	-38.061585	5.125914
-914.199211	-36.937141	5.135910
-912.553604	-42.651305	5.145907
-910.511390	-43.176074	5.155904
-908.693873	-36.121217	5.165901
-906.786280	-41.116262	5.175898
-904.952242	-39.496833	5.185894
-903.207051	-43.469662	5.195891
-901.375609	-41.496156	5.205888
-899.090187	-40.708311	5.215885
-897.400298	-43.696570	5.225882
-895.558718	-44.759211	5.235878
-893.764581	-47.074181	5.245875
-892.078283	-42.072930	5.255872
-890.153208	-42.678421	5.265869
-888.172293	-44.904834	5.275866
-886.112712	-43.084623	5.285862
-884.102674	-41.771191	5.295859
-882.377633	-37.944467	5.305856
-880.792826	-39.943350	5.315853
-878.686459	-35.639199	5.325850
-876.704764	-37.551539	5.335846
-874.820401	-39.541468	5.345843
-873.182834	-43.264981	5.355840
-871.081145	-43.876587	5.365837
-869.295785	-50.656675	5.375834
-867.437498	-44.685073	5.385830
-865.931756	-46.151867	5.395827
-863.576177	-39.662956	5.405824
-861.907543	-40.216378	5.415821
-859.622825	-48.243051	5.425818
-858.271845	-41.994566	5.435814
-856.135935	-45.275134	5.445811
-854.486047	-47.773844	5.455808
-852.611505	-45.355640	5.465805
-850.477685	-38.002373	5.475802
-848.253605	-46.562465	5.485798
-847.059203	-45.685422	5.495795
-844.980033	-43.232032	5.505792
-842.923811	-40.119752	5.515789
-841.135297	-40.089205	5.525786
-839.472168	-37.946648	5.535782
-837.473881	-37.209152	5.545779
-835.660750	-36.532053	5.555776
-833.471154	-40.032748	5.565773
-831.913117	-31.035420	5.575770
-830.103369	-40.972332	5.585766
-827.900548	-37.518759	5.595763
-825.997217	-36.622401	5.605760
-824.457798	-33.443283	5.615757
-822.474870	-35.917843	5.625754
-820.400194	-34.576794	5.635750
-818.572418	-31.304825	5.645747
-816.754230	-34.210913	5.655744
-815.073066	-35.713610	5.665741
-812.970472	-38.652524	5.675738
-811.036089	-46.627894	5.685734
-809.276186	-46.490124	5.695731
-807.494495	-40.272557	5.705728
-805.445956	-39.228877	5.715725
-803.872808	-41.609505	5.725722
-801.928881	-43.081564	5.735718
-799.560925	-36.424045	5.745715
-798.058943	-35.834543	5.755712
-796.387623	-44.011000	5.765709
-794.226279	-45.164142	5.775706
-792.220212	-41.691718	5.785702
-790.175697	-41.495220	5.795699
-788.935571	-48.020752	5.805696
-787.414183	-47.344352	5.815693
-784.809765	-44.542253	5.825690
-782.703543	-43.662499	5.835686
-781.046430	-39.769580	5.845683
-779.211914	-45.835934	5.855680
-777.518664	-36.808075	5.865677
-775.529582	-41.375547	5.875674
-773.514715	-47.118638	5.885670
-771.739519	-29.063413	5.895667
-770.213885	-36.945013	5.905664
-767.847613	-29.265675	5.915661
-765.923139	-35.821632	5.925658
-764.163566	-45.208936	5.935654
-762.611008	-42.466059	5.945651
-760.774055	-38.385564	5.955648
-758.456975	-34.042347	5.965645
-756.658999	-34.305334	5.975642
-754.760062	-39.758324	5.985638
-752.959425	-36.646165	5.995635
-751.300383	-42.403422	6.005632
-749.210060	-44.662994	6.015629
-747.249003	-40.278660	6.025626
-745.415743	-36.366498	6.035622
-743.509035	-38.683559	6.045619
-742.016447	-39.935030	6.055616
-739.828775	-44.144235	6.065613
-737.842178	-45.261506	6.075610
-736.116283	-33.554795	6.085606
-734.415710	-42.061131	6.095603
-732.585581	-44.111751	6.105600
-730.350845	-42.442540	6.115597
-728.589189	-44.461689	6.125594
-726.525911	-44.250767	6.135590
-724.855707	-41.965582	6.145587
-723.142288	-37.952151	6.155584
-721.185997	-39.160875	6.165581
-719.075893	-37.654882	6.175578
-717.062808	-47.873666	6.185574
-715.671176	-38.584416	6.195571
-713.458856	-37.915751	6.205568
-711.545411	-46.040851	6.215565
-710.036621	-41.948926	6.225562
-707.915748	-50.367676	6.235558
-706.272962	-40.365445	6.245555
-704.186591	-41.607572	6.255552
-702.106669	-44.020168	6.265549
-700.577225	-34.404002	6.275546
-698.605357	-44.022543	6.285542
-696.686202	-39.689885	6.295539
-694.913488	-35.758533	6.305536
-692.755523	-51.128535	6.315533
-690.875670	-43.305085	6.325530
-689.347512	-44.971128	6.335526
-687.308960	-40.524917	6.345523
-685.461090	-41.537878	6.355520
-683.830172	-39.982127	6.365517
-681.515463	-34.776402	6.375514
-679.610390	-41.697064	6.385510
-677.948590	-44.057040	6.395507
-676.212745	-42.505419	6.405504
-674.284581	-36.642701	6.415501
-672.306816	-43.576549	6.425498
-670.537674	-44.706385	6.435494
-668.441679	-47.413606	6.445491
-666.385619	-39.654600	6.455488
-665.080593	-35.136954	6.465485
-663.183351	-33.481643	6.475482
-660.953946	-40.190444	6.485478
-659.144143	-37.924357	6.495475
-657.365366	-38.709955	6.505472
-655.309219	-35.695379	6.515469
-653.712704	-37.631252	6.525466
-651.575528	-38.764616	6.535462
-649.735642	-42.769764	6.545459
-647.771631	-42.945518	6.555456
-646.130205	-40.682517	6.565453
-644.322183	-42.726381	6.575450
-642.528192	-40.580905	6.585446
-640.333661	-35.449089	6.595443
-638.270815	-42.162836	6.605440
-636.490365	-42.591867	6.615437
-634.800493	-40.178714	6.625434
-633.013079	-46.194809	6.635430
-631.181443	-44.623723	6.645427
-629.249829	-45.383194	6.655424
-626.984240	-43.674605	6.665421
-625.507015	-36.658292	6.675418
-623.614848	-49.631720	6.685414
-621.516896	-52.898124	6.695411
-619.964104	-45.385497	6.705408
-617.913480	-37.965027	6.715405
-616.136010	-41.998072	6.725402
-614.129028	-52.702086	6.735398
-612.121896	-50.139088	6.745395
-610.297891	-43.879175	6.755392
-608.376523	-40.852500	6.765389
-606.779837	-45.811858	6.775386
-605.006392	-50.843658	6.785382
-602.955488	-42.256455	6.795379
-600.787250	-40.249674	6.805376
-599.315856	-44.715359	6.815373
-597.299579	-37.311485	6.825370
-595.143023	-37.017460	6.835366
-593.340432	-40.727680	6.845363
-591.656177	-42.374390	6.855360
-589.878543	-38.759511	6.865357
-587.937388	-38.344232	6.875354
-585.999798	-36.150602	6.885350
-583.842025	-43.520481	6.895347
-581.996420	-29.017672	6.905344
-580.525142	-37.866210	6.915341
-578.744965	-37.865708	6.925338
-576.759826	-30.471048	6.935334
-574.610229	-37.441746	6.945331
-572.893733	-36.202724	6.955328
-570.926053	-34.007572	6.965325
-569.243980	-29.449047	6.975322
-567.165925	-35.435742	6.985318
-565.437595	-32.409771	6.995315
-563.202034	-34.825007	7.005312
-561.781371	-24.127209	7.015309
-559.795169	-41.171684	7.025306
-558.021484	-33.337469	7.035302
-555.771975	-40.788290	7.045299
-553.600248	-42.839659	7.055296
-552.708633	-33.866715	7.065293
-550.717979	-32.982501	7.075290
-548.590451	-40.088590	7.085286
-546.409946	-33.238234	7.095283
-544.695095	-41.156243	7.105280
-542.895173	-40.953618	7.115277
-540.937361	-35.327607	7.125274
-538.877146	-39.265242	7.135270
-537.125236	-40.801148	7.145267
-535.325099	-40.761172	7.155264
-533.644357	-35.911902	7.165261
-531.667920	-35.049084	7.175258
-529.645154	-37.059271	7.185254
-527.847827	-41.163316	7.195251
-526.308852	-31.755367	7.205248
-524.056743	-32.507525	7.215245
-522.385026	-35.773662	7.225242
-520.036269	-31.171590	7.235238
-518.467657	-42.058143	7.245235
-516.527536	-35.966683	7.255232
-514.791854	-38.134679	7.265229
-512.868661	-33.221490	7.275226
-510.782387	-31.908856	7.285222
-509.251302	-35.921422	7.295219
-507.217397	-31.022751	7.305216
-505.330337	-33.581210	7.315213
-503.529938	-38.146753	7.325210
-501.579096	-39.386004	7.335206
-499.609334	-37.437424	7.345203
-497.809086	-40.425668	7.355200
-495.871583	-33.556978	7.365197
-494.058544	-37.492993	7.375194
-492.346439	-32.836582	7.385190
-490.017614	-46.130698	7.395187
-488.471195	-32.618906	7.405184
-486.438179	-36.878976	7.415181
-484.632267	-33.483252	7.425178
-482.784728	-34.385484	7.435174
-481.005987	-37.465013	7.445171
-479.081085	-29.466996	7.455168
-477.126883	-40.121440	7.465165
-475.226377	-31.781651	7.475162
-473.479869	-33.588211	7.485158
-471.719830	-37.501537	7.495155
-469.850301	-33.501788	7.505152
-467.705211	-30.895958	7.515149
-465.615791	-36.893858	7.525146
-464.138101	-32.605755	7.535142
-462.152766	-37.459732	7.545139
-460.307793	-32.755045	7.555136
-458.430584	-41.358885	7.565133
-456.568735	-35.215402	7.575130
-454.652118	-37.355410	7.585126
-452.741958	-35.787247	7.595123
-450.605225	-28.647189	7.605120
-448.995338	-28.560979	7.615117
-447.182416	-25.185288	7.625114
-445.444696	-32.674286	7.635110
-443.399834	-34.253747	7.645107
-441.455401	-29.275996	7.655104
-439.600877	-32.465486	7.665101
-437.847898	-34.762497	7.675098
-435.778304	-33.235568	7.685094
-434.208622	-35.599618	7.695091
-432.113319	-32.538990	7.705088
-430.303295	-26.856124	7.715085
-428.454897	-32.757092	7.725082
-426.199923	-32.765977	7.735078
-424.503100	-35.391887	7.745075
-422.960214	-32.446715	7.755072
-420.860724	-31.777125	7.765069
-419.296336	-38.082708	7.775066
-417.019767	-37.510859	7.785062
-415.086562	-44.290564	7.795059
-413.266574	-37.418826	7.805056
-411.492426	-46.754551	7.815053
-409.629821	-44.384600	7.825050
-407.711903	-43.749161	7.835046
-405.830983	-48.231178	7.845043
-403.807334	-41.191439	7.855040
-402.303220	-39.114747	7.865037
-400.107306	-39.543625	7.875034
-398.373440	-38.994047	7.885030
-396.661425	-40.810834	7.895027
-394.627537	-39.267115	7.905024
-393.285560	-37.485036	7.915021
-390.989395	-35.285338	7.925018
-388.873280	-34.514170	7.935014
-387.223876	-39.235511	7.945011
-385.132162	-39.358809	7.955008
-383.229090	-42.609687	7.965005
-381.383845	-42.698368	7.975002
-379.536470	-37.401930	7.984998
-377.622791	-40.678180	7.994995
-375.727550	-40.466963	8.004992
-374.175796	-40.260901	8.014989
-372.151171	-30.260939	8.024986
-370.180163	-39.400716	8.034982
-368.138517	-42.845800	8.044979
-366.685294	-40.179944	8.054976
-365.012575	-39.374279	8.064973
-362.482303	-37.148774	8.074970
-360.673630	-38.935180	8.084966
-358.839092	-37.004363	8.094963
-357.030881	-35.561943	8.104960
-355.233207	-37.712882	8.114957
-353.504039	-38.918204	8.124954
-351.360906	-42.616304	8.134950
-349.469299	-35.081776	8.144947
-347.531377	-37.657707	8.154944
-345.994207	-41.783244	8.164941
-344.011591	-39.724485	8.174938
-341.939245	-41.276672	8.184934
-340.224946	-34.380105	8.194931
-338.351463	-30.983998	8.204928
-336.610251	-35.388405	8.214925
-334.684837	-30.968017	8.224922
-332.716960	-34.486556	8.234918
-330.872670	-35.694451	8.244915
-328.744557	-35.660889	8.254912
-327.436198	-33.342910	8.264909
-325.311076	-34.816670	8.274906
-323.067605	-33.004785	8.284902
-321.134025	-39.421347	8.294899
-319.561556	-34.063607	8.304896
-317.837512	-39.022594	8.314893
-315.751353	-40.030680	8.324890
-313.817216	-33.645998	8.334886
-312.347636	-40.117951	8.344883
-310.229418	-36.877725	8.354880
-308.296746	-40.398518	8.364877
-306.282799	-38.360517	8.374874
-304.573573	-41.428823	8.384870
-302.721420	-35.553644	8.394867
-300.859074	-38.954266	8.404864
-298.890538	-42.682870	8.414861
-297.047962	-38.102395	8.424858
-295.190060	-37.095728	8.434854
-293.394802	-42.844439	8.444851
-291.295689	-40.815283	8.454848
-289.431246	-39.789130	8.464845
-287.574011	-40.054905	8.474842
-286.078763	-49.421814	8.484838
-284.104365	-46.981191	8.494835
-282.099693	-37.664762	8.504832
-279.762631	-38.018171	8.514829
-278.201693	-35.249457	8.524826
-276.709056	-41.721913	8.534822
-274.610913	-26.777572	8.544819
-272.621586	-41.784061	8.554816
-271.054612	-33.321385	8.564813
-268.813180	-31.878574	8.574810
-266.818194	-34.487232	8.584807
-264.781669	-36.249939	8.594803
-263.234717	-36.527746	8.604800
-261.495299	-29.309879	8.614797
-259.693302	-39.649370	8.624794
-257.696392	-33.926723	8.634791
-255.858699	-29.626469	8.644787
-254.132550	-32.796910	8.654784
-251.826762	-37.701870	8.664781
-250.133733	-24.933235	8.674778
-248.236898	-21.813921	8.684775
-246.212345	-29.506456	8.694771
-244.556180	-38.002245	8.704768
-242.677179	-29.802491	8.714765
-240.782914	-33.656558	8.724762
-239.126653	-33.609184	8.734759
-236.917317	-26.823115	8.744755
-234.882428	-38.871766	8.754752
-232.724154	-35.525761	8.764749
-231.497837	-47.175375	8.774746
-229.636277	-38.006573	8.784743
-227.715527	-42.461661	8.794739
-225.574450	-47.207683	8.804736
-223.793691	-42.996209	8.814733
-222.146298	-40.214414	8.824730
-220.119756	-38.036252	8.834727
-218.039452	-37.567092	8.844723
-216.427563	-34.831728	8.854720
-214.709000	-36.739428	8.864717
-212.583376	-32.456670	8.874714
-210.708842	-35.169211	8.884711
-208.588995	-45.332035	8.894707
-206.683761	-41.743534	8.904704
-205.467170	-38.278803	8.914701
-203.671143	-37.157985	8.924698
-201.650647	-32.733711	8.934695
-199.330242	-44.865787	8.944691
-197.588716	-38.297119	8.954688
-195.844773	-46.391643	8.964685
-193.630846	-36.844855	8.974682
-191.944145	-43.976616	8.984679
-190.328628	-35.201120	8.994675
-188.301435	-45.510185	9.004672
-186.064372	-43.839245	9.014669
-184.333780	-44.959415	9.024666
-182.598938	-42.671518	9.034663
-180.710648	-44.712061	9.044659
-179.142493	-41.233948	9.054656
-176.966215	-42.890994	9.064653
-175.088368	-44.929866	9.074650
-173.098554	-46.078762	9.084647
-171.492126	-45.251330	9.094643
-169.504730	-45.105178	9.104640
-167.507533	-42.589150	9.114637
-165.879729	-45.829094	9.124634
-163.898828	-47.977553	9.134631
-161.877345	-44.098109	9.144627
-159.966625	-45.316474	9.154624
-158.236529	-41.471052	9.164621
-156.248833	-41.468612	9.174618
-154.336525	-38.831665	9.184615
-152.644062	-41.644576	9.194611
-150.974343	-46.766877	9.204608
-148.745091	-43.315286	9.214605
-147.089682	-40.174738	9.224602
-144.900547	-40.861233	9.234599
-143.109425	-39.611700	9.244595
-141.199162	-43.394036	9.254592
-139.405944	-42.787428	9.264589
-137.666386	-38.135126	9.274586
-135.924146	-36.284138	9.284583
-133.688552	-38.365849	9.294579
-131.862303	-38.566563	9.304576
-130.321668	-36.656563	9.314573
-128.225745	-39.241744	9.324570
-126.125668	-34.571168	9.334567
-124.671531	-37.702857	9.344563
-122.581917	-37.950321	9.354560
-120.614904	-35.225763	9.364557
-119.099967	-35.896241	9.374554
-116.938195	-38.578755	9.384551
-114.738444	-41.073127	9.394547
-113.250266	-40.364150	9.404544
-111.542147	-36.627283	9.414541
-109.372663	-34.849176	9.424538
-107.256165	-41.092671	9.434535
-105.731782	-39.884232	9.444531
-103.993827	-38.247261	9.454528
-101.959197	-40.587390	9.464525
-100.144091	-40.405799	9.474522
-98.274899	-41.131203	9.484519
-96.318142	-37.031385	9.494515
-94.184609	-35.623296	9.504512
-92.602754	-42.706692	9.514509
-90.944804	-34.956250	9.524506
-88.578677	-34.793088	9.534503
-86.981337	-32.096362	9.544499
-84.822538	-31.912750	9.554496
-82.967796	-32.501635	9.564493
-81.512687	-31.455802	9.574490
-79.465984	-39.276470	9.584487
-77.716381	-37.567131	9.594483
-75.537357	-35.875773	9.604480
-73.469288	-31.733695	9.614477
-72.321444	-33.897598	9.624474
-70.213532	-31.121267	9.634471
-68.334004	-38.256875	9.644467
-66.249914	-41.027999	9.654464
-64.356517	-40.854133	9.664461
-62.388870	-42.651471	9.674458
-60.404917	-40.873721	9.684455
-58.540076	-47.637522	9.694451
-57.021750	-35.148740	9.704448
-55.161925	-28.101484	9.714445
-53.313329	-33.465408	9.724442
-51.333018	-40.689707	9.734439
-49.231800	-37.073919	9.744435
-47.601098	-46.122861	9.754432
-45.710447	-38.919477	9.764429
-43.618831	-46.399930	9.774426
-41.941398	-45.110081	9.784423
-40.229580	-43.088390	9.794419
-37.894056	-45.492252	9.804416
-36.281158	-45.767802	9.814413
-34.170320	-45.304933	9.824410
-32.595475	-35.742873	9.834407
-30.899276	-40.566183	9.844403
-28.971741	-34.844896	9.854400
-26.850669	-41.111160	9.864397
-25.073689	-25.767980	9.874394
-22.906539	-41.581047	9.884391
-20.803670	-36.080342	9.894387
-19.047129	-36.309323	9.904384
-17.731258	-43.026583	9.914381
-16.044846	-47.463080	9.924378
-13.871112	-42.321022	9.934375
-11.688187	-39.995528	9.944371
-9.916609	-37.028137	9.954368
-8.371644	-32.096814	9.964365
-6.476169	-17.820871	9.974362
-5.361330	0.223612	9.984359
-3.788604	44.235298	9.994355
-2.033092	95.046583	10.004352
-0.797633	147.788284	10.014349
0.000000	216.097183	10.019354
0.691578	242.201842	10.024359
1.314894	278.511912	10.029363
1.508483	315.787858	10.034368
2.395287	336.832891	10.039373
2.643465	366.230060	10.044378
2.949896	377.286718	10.049383
3.054985	410.041907	10.054387
3.277378	425.760669	10.059392
3.636521	423.195682	10.064397
3.717245	443.800184	10.069402
4.038131	450.133383	10.074407
4.330574	457.855633	10.079411
4.023013	460.778911	10.084416
4.698554	464.601905	10.089421
4.290234	463.171685	10.094426
4.352443	457.855069	10.099431
4.385281	456.559482	10.104435
4.263335	475.110126	10.109440
4.650545	472.958531	10.114445
4.477830	480.110035	10.119450
4.709139	482.322918	10.124455
4.739288	486.327702	10.129459
4.700978	477.521673	10.134464
4.611126	463.392396	10.139469
4.568552	480.673604	10.144474
4.737869	486.039127	10.149479
4.888390	486.762116	10.154483
4.541114	497.109452	10.159488
4.723814	490.784892	10.164493
4.671491	495.848314	10.169498
4.919901	496.686573	10.174503
5.157340	492.068944	10.179507
4.911153	503.814638	10.184512
5.025835	506.091857	10.189517
5.118740	504.561189	10.194522
5.033775	496.521078	10.199527
5.128623	510.448422	10.204531
4.951836	507.820671	10.209536
5.044113	506.015723	10.214541
5.104721	525.207496	10.219546
5.086765	533.401903	10.224551
5.461002	543.550618	10.229555
5.363880	536.755021	10.234560
5.543739	545.777295	10.239565
5.536693	549.709183	10.244570
5.813473	548.046685	10.249575
6.014015	541.679834	10.254579
5.743095	556.550203	10.259584
5.949285	545.305090	10.264589
5.987483	553.061634	10.269594
5.891955	551.210944	10.274599
6.071551	556.953311	10.279603
5.946711	554.124884	10.284608
6.255592	552.895644	10.289613
6.087152	563.380079	10.294618
5.875331	557.402257	10.299623
6.257027	559.933354	10.304627
5.837405	570.711738	10.309632
6.289591	553.536070	10.314637
6.142929	558.010607	10.319642
6.255324	567.434727	10.324647
6.348108	558.729161	10.329651
6.336178	570.060665	10.334656
6.405904	568.077962	10.339661
6.728840	570.090171	10.344666
6.878862	574.025399	10.349671
6.557563	575.673598	10.354675
6.332310	571.645390	10.359680
6.769604	558.636696	10.364685
6.549544	566.366632	10.369690
6.484117	567.977174	10.374695
6.853249	572.372601	10.379699
6.460513	581.667569	10.384704
6.677082	576.778861	10.389709
6.461407	576.639349	10.394714
6.959348	598.093708	10.399719
7.000610	599.983695	10.404723
6.927699	603.118726	10.409728
6.981107	596.418938	10.414733
6.952254	606.403337	10.419738
7.128066	600.705860	10.424743
7.237731	606.907242	10.429747
7.081702	608.398202	10.434752
7.276112	611.325023	10.439757
7.057111	610.088513	10.444762
7.313474	605.018411	10.449767
7.214635	604.503883	10.454771
7.144124	617.495790	10.459776
7.549830	622.910392	10.464781
7.400747	638.411098	10.469786
7.600680	634.196789	10.474791
7.996926	642.905498	10.479795
7.894065	648.483222	10.484800
7.983899	629.528155	10.489805
7.755346	634.176622	10.494810
7.750750	627.036651	10.499815
8.054743	624.631809	10.504819
7.826877	624.558895	10.509824
7.766195	620.206389	10.514829
7.952483	637.894393	10.519834
8.064237	649.518461	10.524839
8.131560	651.177223	10.529843
7.862116	656.444060	10.534848
8.433274	649.164941	10.539853
8.144091	652.443284	10.544858
8.108994	652.260778	10.549863
7.991195	649.801784	10.554867
8.337551	662.952742	10.559872
8.410777	661.800502	10.564877
8.110882	661.680730	10.569882
8.418555	657.384576	10.574887
8.384016	657.582017	10.579891
8.453493	664.565675	10.584896
8.532004	656.633439	10.589901
8.305116	657.531747	10.594906
8.665233	673.140505	10.599911
8.903004	676.617075	10.604915
8.895370	693.708466	10.609920
9.078752	688.812398	10.614925
9.211069	685.230164	10.619930
8.996357	672.583975	10.624935
8.800850	666.415853	10.629939
8.861676	675.466655	10.634944
9.234252	683.240899	10.639949
9.204210	693.801122	10.644954
9.048735	694.448351	10.649959
9.354636	696.520064	10.654963
9.079224	699.785183	10.659968
9.378447	689.892309	10.664973
9.399279	694.521518	10.669978
9.626519	686.967658	10.674983
9.617679	693.618477	10.679987
9.309471	685.235406	10.684992
9.330667	684.405269	10.689997
9.559173	690.881040	10.695002
9.537625	699.612266	10.700007
9.801950	697.207432	10.705011
9.477824	699.445862	10.710016
9.411449	696.357353	10.715021
9.288293	708.148242	10.720026
9.892841	703.038342	10.725031
9.841776	701.287771	10.730035
9.717030	703.218441	10.735040
10.145770	698.281661	10.740045
9.782988	696.524038	10.745050
9.884397	705.423310	10.750055
9.666415	706.317046	10.755059
9.843371	702.573150	10.760064
10.066398	717.352285	10.765069
10.254081	728.024461	10.770074
10.319276	739.044182	10.775079
10.442722	730.502353	10.780083
10.491079	733.911379	10.785088
10.654895	727.996574	10.790093
10.565200	720.982090	10.795098
10.369689	707.456041	10.800103
10.326722	713.063660	10.805107
10.349106	733.742534	10.810112
10.433554	732.765114	10.815117
10.659950	731.400785	10.820122
10.770594	729.988688	10.825127
10.650141	732.774946	10.830131
10.580702	731.874108	10.835136
10.807354	725.214437	10.840141
10.741252	729.070639	10.845146
10.729211	736.890487	10.850151
11.062903	732.437201	10.855155
11.124178	734.675667	10.860160
11.510135	734.455965	10.865165
11.224982	729.163113	10.870170
10.909030	733.732512	10.875175
11.539863	729.294911	10.880179
11.248093	752.428723	10.885184
11.468628	730.503830	10.890189
11.250139	728.481921	10.895194
11.308602	730.072720	10.900199
11.533940	731.540712	10.905203
11.144974	740.007294	10.910208
11.356274	728.393802	10.915213
11.282810	738.497369	10.920218
11.157002	735.902445	10.925223
11.525627	726.365900	10.930227
11.400032	734.489281	10.935232
11.556315	728.947830	10.940237
11.267667	752.259336	10.945242
11.657748	765.420761	10.950247
11.837991	767.741181	10.955251
11.755662	782.688932	10.960256
11.952580	764.651727	10.965261
11.713137	768.614433	10.970266
12.081202	772.196400	10.975271
12.261983	763.889831	10.980275
12.313307	765.257850	10.985280
12.650583	765.194143	10.990285
12.498392	759.634073	10.995290
12.328143	761.805393	11.000295
12.576984	764.468103	11.005299
12.073206	745.694292	11.010304
12.409582	755.582696	11.015309
12.148620	760.250563	11.020314
12.293453	764.699172	11.025319
12.489239	752.059980	11.030323
12.533962	758.522516	11.035328
12.430627	768.492099	11.040333
12.599423	763.623564	11.045338
12.437350	770.581127	11.050343
12.951251	762.986237	11.055347
12.699802	777.774880	11.060352
12.890188	761.050725	11.065357
12.802029	770.108002	11.070362
12.700968	770.498978	11.075367
13.109854	756.401829	11.080371
12.685022	777.492710	11.085376
12.769594	764.062282	11.090381
13.005754	758.951196	11.095386
12.869706	765.734299	11.100391
12.938089	762.110204	11.105395
12.910116	773.214195	11.110400
12.983472	784.139610	11.115405
13.162119	808.510487	11.120410
13.499651	809.290397	11.125415
13.659774	800.389445	11.130419
13.476358	799.197704	11.135424
14.005923	798.546673	11.140429
13.681521	788.918773	11.145434
13.319641	772.284264	11.150439
13.338947	771.866002	11.155443
13.751409	800.198658	11.160448
13.885857	788.488567	11.165453
13.550050	794.915620	11.170458
13.666561	800.567222	11.175463
13.962742	801.435728	11.180467
13.564195	799.871451	11.185472
13.812126	800.236727	11.190477
13.666364	802.107684	11.195482
13.877514	799.315506	11.200487
13.345537	797.496548	11.205491
13.672202	812.289213	11.210496
13.943908	798.715368	11.215501
14.052725	798.850523	11.220506
13.781262	814.517591	11.225511
14.064396	815.525371	11.230515
14.342819	823.671095	11.235520
14.560743	826.565826	11.240525
14.937204	818.667980	11.245530
14.675835	817.811941	11.250535
14.752982	804.592392	11.255539
14.545207	809.636563	11.260544
14.555197	792.663603	11.265549
14.323793	797.932308	11.270554
14.145382	803.878528	11.275559
14.377763	811.858127	11.280563
14.777598	821.298069	11.285568
14.706699	828.739429	11.290573
14.658899	829.399451	11.295578
14.720379	814.152879	11.300583
14.954264	825.989419	11.305587
14.953909	830.825476	11.310592
15.335546	815.087877	11.315597
15.508031	821.810758	11.320602
15.147299	834.098529	11.325607
15.209326	810.664439	11.330611
15.196827	824.084089	11.335616
15.228684	821.826698	11.340621
15.154179	826.143154	11.345626
15.231629	827.186894	11.350631
15.096780	821.108377	11.355635
15.126416	829.574478	11.360640
15.394258	818.178974	11.365645
15.220753	828.959294	11.370650
15.331193	832.770021	11.375655
15.362542	827.601692	11.380659
15.383242	831.205961	11.385664
15.611872	827.696639	11.390669
15.591126	848.705828	11.395674
15.885986	845.449286	11.400679
15.893748	849.027238	11.405683
15.567078	857.550184	11.410688
16.076189	859.685704	11.415693
16.229251	851.673663	11.420698
15.545993	833.688445	11.425703
15.708898	850.019546	11.430707
15.614325	841.804158	11.435712
15.698390	862.268377	11.440717
16.056324	851.776255	11.445722
16.128171	849.042555	11.450727
16.343108	856.466726	11.455731
15.916315	862.110389	11.460736
16.189100	850.589494	11.465741
16.184963	850.113468	11.470746
15.889857	856.204476	11.475751
16.315995	858.922504	11.480755
16.369564	872.839435	11.485760
16.440359	882.741901	11.490765
16.528896	882.935484	11.495770
16.774273	876.138717	11.500775
16.766384	871.533290	11.505779
16.704975	882.997508	11.510784
16.875096	881.036598	11.515789
17.253843	870.913300	11.520794
16.903050	885.309470	11.525799
17.146818	877.271909	11.530803
17.076044	875.934463	11.535808
17.141356	865.925814	11.540813
16.824612	860.631643	11.545818
16.871233	856.859610	11.550823
17.218774	867.027005	11.555827
17.296337	886.304863	11.560832
17.455238	871.900547	11.565837
17.179104	855.375266	11.570842
16.835241	865.406932	11.575847
17.116777	877.434609	11.580851
17.057121	885.014552	11.585856
17.373420	879.950566	11.590861
17.425881	886.960701	11.595866
16.772774	891.984465	11.600871
17.350111	877.860333	11.605875
16.998509	895.937216	11.610880
17.543347	901.612006	11.615885
17.706433	911.539195	11.620890
17.832147	913.068827	11.625895
17.996849	909.506604	11.630899
17.954290	921.852511	11.635904
17.858425	895.961359	11.640909
17.813327	893.752499	11.645914
18.062048	906.430403	11.650919
18.293148	901.640193	11.655923
17.939730	893.018208	11.660928
17.811559	885.405813	11.665933
18.216961	904.830102	11.670938
18.060870	902.713060	11.675943
18.314332	900.847663	11.680947
18.092153	911.757232	11.685952
18.328422	905.270985	11.690957
18.297878	920.268967	11.695962
18.068546	912.573344	11.700967
18.359220	905.852917	11.705971
18.078207	923.707267	11.710976
18.540199	910.145545	11.715981
18.613037	912.044730	11.720986
18.165006	921.637312	11.725991
18.383227	909.371294	11.730995
18.218985	911.016556	11.736000
18.673862	909.462808	11.741005
18.608292	927.229184	11.746010
18.441975	925.883318	11.751015
18.789371	931.370416	11.756019
18.994853	944.540947	11.761024
18.962177	939.460060	11.766029
19.271952	936.926515	11.771034
18.979206	943.110222	11.776039
19.436998	933.463127	11.781043
19.197286	941.491285	11.786048
19.293124	937.988923	11.791053
19.390442	934.697637	11.796058
19.190799	931.089440	11.801063
19.367112	912.391444	11.806067
19.197152	936.193668	11.811072
19.533049	923.527250	11.816077
19.581516	925.548594	11.821082
19.688132	917.985467	11.826087
19.399809	906.424710	11.831091
19.141069	917.518309	11.836096
19.455407	925.248358	11.841101
19.332335	930.763183	11.846106
19.258981	934.560673	11.851111
19.604548	928.099561	11.856115
19.219653	936.493068	11.861120
19.570191	938.450467	11.866125
19.886239	933.776008	11.871130
19.943061	929.273781	11.876135
19.660599	932.141109	11.881139
20.020930	936.438707	11.886144
20.382946	951.678462	11.891149
20.028188	948.760471	11.896154
20.011345	957.721337	11.901159
20.428261	953.576408	11.906163
20.232819	958.323774	11.911168
20.118920	948.712655	11.916173
20.396090	961.233106	11.921178
20.208961	966.879585	11.926183
20.415856	965.644502	11.931187
20.479971	961.133217	11.936192
20.523406	962.191855	11.941197
20.758895	967.934934	11.946202
20.560541	958.690514	11.951207
20.744753	963.605988	11.956211
20.362529	950.771806	11.961216
20.434365	965.234690	11.966221
20.417177	966.129532	11.971226
20.421754	957.358949	11.976231
20.688764	959.509444	11.981235
20.732065	974.267047	11.986240
20.902224	958.761716	11.991245
20.926527	966.724126	11.996250
20.564732	976.917999	12.001255
20.805371	961.363579	12.006259
20.815361	981.196386	12.011264
21.121841	992.251934	12.016269
21.253138	993.916302	12.021274
21.184778	990.143649	12.026279
21.394339	997.141397	12.031283
20.954183	987.424592	12.036288
21.526416	982.291368	12.041293
21.270088	973.775274	12.046298
21.371615	966.563016	12.051303
21.529162	965.260110	12.056307
21.282414	958.179096	12.061312
21.112941	957.929708	12.066317
21.226390	964.551686	12.071322
21.375643	958.639110	12.076327
21.593178	960.917345	12.081331
21.354587	961.106333	12.086336
21.372992	966.962882	12.091341
21.311259	962.965253	12.096346
21.313670	958.701930	12.101351
21.376125	966.522637	12.106355
21.203470	968.639177	12.111360
21.355141	943.113735	12.116365
21.406148	951.103416	12.121370
20.954214	938.374979	12.126375
21.058100	928.815871	12.131379
20.934416	929.120573	12.136384
21.061540	943.241882	12.141389
21.402485	953.605933	12.146394
20.903039	953.976873	12.151399
21.168440	963.474620	12.156403
21.405501	963.158817	12.161408
21.185683	952.080681	12.166413
21.129317	938.723032	12.171418
21.193276	939.357350	12.176423
21.258859	925.261176	12.181427
20.931913	928.045711	12.186432
21.219182	947.351705	12.191437
21.108722	938.662558	12.196442
21.206790	946.505959	12.201447
21.147400	946.319438	12.206451
21.428869	938.835646	12.211456
21.407615	927.487741	12.216461
21.250668	934.023522	12.221466
20.893419	929.965801	12.226471
21.345389	932.832688	12.231475
21.098323	936.047606	12.236480
21.301186	934.791092	12.241485
21.338567	931.526712	12.246490
21.007266	928.641254	12.251495
21.285079	934.055873	12.256499
20.975607	933.675850	12.261504
21.091292	924.641562	12.266509
21.372933	935.300485	12.271514
21.138998	946.838002	12.276519
21.459482	929.315469	12.281523
20.931050	944.157918	12.286528
20.912079	936.712583	12.291533
21.075866	925.954906	12.296538
20.929298	932.714534	12.301543
21.215193	935.700948	12.306547
21.036223	937.570912	12.311552
21.088020	928.412770	12.316557
21.185855	943.970616	12.321562
21.083073	943.278509	12.326567
21.124894	938.193626	12.331571
21.126720	949.540580	12.336576
21.383083	940.835504	12.341581
21.380775	938.815354	12.346586
21.068304	942.978987	12.351591
21.074000	937.418897	12.356595
21.016875	949.749805	12.361600
21.253508	932.906112	12.366605
21.072477	939.125616	12.371610
20.984789	938.874223	12.376615
21.178952	937.302130	12.381619
21.232463	940.270415	12.386624
21.013039	940.864775	12.391629
21.378249	936.548326	12.396634
21.203146	946.056394	12.401639
21.453032	938.576062	12.406643
20.987435	946.548785	12.411648
21.039901	948.646765	12.416653
21.426204	938.137441	12.421658
20.893995	955.021071	12.426663
21.449097	927.996291	12.431667
20.955294	951.712997	12.436672
21.052852	939.472506	12.441677
21.194547	936.424876	12.446682
20.908054	949.076215	12.451687
20.952406	940.155796	12.456691
20.835858	970.135912	12.461696
21.338555	974.664705	12.466701
21.645994	967.093178	12.471706
21.610309	961.661104	12.476711
21.483361	946.054939	12.481715
21.353995	940.245154	12.486720
21.210721	954.281868	12.491725
21.371108	946.222874	12.496730
21.451527	952.589919	12.501735
21.251514	950.763725	12.506739
21.215250	959.705612	12.511744
21.150588	950.329489	12.516749
21.412185	953.324514	12.521754
21.177539	956.124295	12.526759
21.409898	945.756213	12.531763
21.373326	955.164922	12.536768
21.268790	944.860033	12.541773
21.375012	923.172275	12.546778
21.130212	930.314996	12.551783
20.892724	919.018932	12.556787
20.676609	929.322001	12.561792
20.802321	948.035600	12.566797
21.040834	938.156971	12.571802
20.975116	958.601062	12.576807
21.167731	958.147269	12.581811
21.389036	949.805746	12.586816
20.874832	957.811459	12.591821
20.963366	958.016083	12.596826
21.014203	955.221059	12.601831
21.193916	944.872412	12.606835
21.291685	959.302769	12.611840
21.154113	961.019477	12.616845
21.608163	948.468233	12.621850
21.118653	953.410731	12.626855
21.451680	951.237750	12.631859
21.128591	962.899885	12.636864
21.382519	950.522482	12.641869
21.386564	952.372720	12.646874
21.339746	951.540800	12.651879
21.420847	937.243444	12.656883
20.982802	936.595347	12.661888
20.985578	926.872594	12.666893
20.953695	926.722687	12.671898
21.163484	954.231693	12.676903
21.073974	943.244744	12.681907
21.031777	950.134390	12.686912
21.292011	941.698353	12.691917
21.505426	956.353113	12.696922
21.008875	948.652782	12.701927
21.451490	937.476891	12.706931
21.232177	925.633877	12.711936
21.403850	931.147424	12.716941
21.487838	923.516941	12.721946
21.109622	923.009112	12.726951
21.057576	925.189988	12.731955
21.105189	926.052416	12.736960
21.286934	921.213302	12.741965
21.224216	923.615075	12.746970
20.976362	930.477587	12.751975
21.354015	917.124852	12.756979
21.458756	916.084260	12.761984
21.339836	923.892871	12.766989
21.315782	920.469559	12.771994
21.075091	928.747022	12.776999
21.212501	916.241576	12.782003
20.737138	930.424271	12.787008
20.946210	920.985586	12.792013
21.159774	918.237155	12.797018
21.149088	926.457434	12.802023
21.336184	923.325295	12.807027
21.134091	928.330754	12.812032
20.866090	930.140800	12.817037
21.307295	930.915222	12.822042
20.955598	931.940683	12.827047
21.108427	926.745059	12.832051
20.712731	930.638112	12.837056
21.014872	918.823901	12.842061
21.087411	933.449066	12.847066
20.878531	938.923964	12.852071
21.337065	942.888936	12.857075
21.531813	946.566399	12.862080
21.329959	945.074812	12.867085
21.482863	937.313483	12.872090
21.220782	931.378212	12.877095
21.060804	930.236337	12.882099
21.071624	938.997238	12.887104
20.834295	933.594181	12.892109
21.137601	926.149489	12.897114
20.836500	940.077321	12.902119
21.079371	935.863962	12.907123
21.298943	946.097555	12.912128
21.008116	933.415967	12.917133
21.390004	927.143028	12.922138
20.916179	937.764747	12.927143
21.117595	944.834731	12.932147
21.317744	945.236018	12.937152
21.148674	949.282165	12.942157
21.519665	936.209594	12.947162
20.928941	936.238702	12.952167
21.380927	919.453718	12.957171
21.038070	925.487715	12.962176
20.927491	928.020125	12.967181
21.201575	923.136321	12.972186
20.900415	933.471880	12.977191
21.174509	939.617220	12.982195
21.285114	956.683756	12.987200
21.426418	957.908133	12.992205
21.368130	938.875359	12.997210
21.336767	947.751803	13.002215
21.672564	921.752333	13.007219
21.351472	938.976009	13.012224
21.402466	928.581671	13.017229
21.372542	940.185993	13.022234
21.235944	934.292209	13.027239
21.551991	934.536239	13.032243
21.190709	936.586666	13.037248
21.214792	936.293793	13.042253
21.272451	937.884744	13.047258
20.917377	940.345763	13.052263
21.104362	936.155510	13.057267
21.189131	939.610816	13.062272
21.356067	935.125718	13.067277
21.073997	944.754924	13.072282
21.286210	946.508882	13.077287
21.193640	938.930205	13.082291
21.021048	945.859568	13.087296
21.306052	936.700497	13.092301
21.342525	929.903907	13.097306
20.795147	921.921539	13.102311
21.291686	923.513454	13.107315
21.266801	928.709845	13.112320
21.105503	917.299129	13.117325
21.201954	926.366485	13.122330
21.107769	923.689213	13.127335
21.255483	912.748031	13.132339
21.057371	916.630068	13.137344
21.271145	918.472083	13.142349
21.014064	913.548420	13.147354
20.952627	926.278962	13.152359
21.500024	936.695229	13.157363
21.122579	917.841118	13.162368
21.139002	920.566157	13.167373
21.400078	904.721534	13.172378
21.113018	903.508466	13.177383
21.325958	909.067463	13.182387
21.287841	907.321109	13.187392
21.446110	898.790974	13.192397
21.570812	895.725562	13.197402
21.423135	899.257355	13.202407
20.895249	896.092600	13.207411
21.055369	906.841845	13.212416
20.951408	901.800725	13.217421
20.945021	897.373244	13.222426
20.983403	909.767732	13.227431
21.397151	896.937534	13.232435
21.242170	909.080590	13.237440
20.980755	910.725580	13.242445
21.340626	907.140115	13.247450
20.963530	906.160603	13.252455
21.184577	916.611558	13.257459
21.107349	907.872974	13.262464
21.213162	906.436399	13.267469
21.522831	900.394184	13.272474
21.205740	904.194270	13.277479
21.554196	900.727321	13.282483
21.497318	912.684423	13.287488
21.392637	909.959943	13.292493
21.718673	899.977495	13.297498
21.200293	908.173080	13.302503
21.303474	887.413102	13.307507
21.014097	879.894228	13.312512
21.345208	878.170991	13.317517
21.041621	870.099307	13.322522
20.813768	878.556042	13.327527
21.166390	883.498245	13.332531
21.189529	904.267130	13.337536
21.215388	909.871733	13.342541
21.404623	902.273361	13.347546
21.429240	901.171432	13.352551
21.180018	879.433197	13.357555
21.219418	870.657112	13.362560
20.806555	878.474733	13.367565
20.952531	871.394204	13.372570
20.955279	889.931800	13.377575
21.316354	884.521630	13.382579
21.010010	908.845451	13.387584
20.934547	920.742446	13.392589
21.280368	907.773263	13.397594
21.321595	904.815779	13.402599
21.126602	916.239829	13.407603
21.062739	915.468977	13.412608
21.261918	906.298382	13.417613
21.209407	909.184223	13.422618
21.064871	915.317473	13.427623
21.128544	910.251191	13.432627
21.044121	914.867297	13.437632
21.290880	912.126188	13.442637
21.310602	912.307093	13.447642
21.205618	900.228248	13.452647
21.120003	896.833683	13.457651
21.093703	893.133195	13.462656
21.057363	894.827441	13.467661
21.063370	904.746563	13.472666
21.103203	912.490425	13.477671
21.422838	909.751887	13.482675
21.199716	912.265973	13.487680
20.862876	895.687249	13.492685
20.950705	905.549168	13.497690
21.174371	913.258980	13.502695
21.392199	907.732877	13.507699
21.250291	917.245093	13.512704
21.240104	907.533882	13.517709
21.301040	920.109285	13.522714
21.282567	910.681666	13.527719
21.284615	872.616724	13.532723
20.921185	879.149142	13.537728
20.691302	896.815533	13.542733
21.083282	899.789751	13.547738
21.184238	904.485097	13.552743
21.203906	918.243477	13.557747
21.010084	914.397815	13.562752
21.280283	911.722353	13.567757
21.400702	918.827320	13.572762
21.277847	922.782512	13.577767
21.499198	910.691034	13.582771
21.121310	901.095242	13.587776
21.218358	898.215588	13.592781
21.420783	890.261884	13.597786
20.837873	883.357522	13.602791
20.971917	886.994190	13.607795
21.046566	888.607657	13.612800
21.373618	901.623144	13.617805
21.368284	895.599632	13.622810
21.194737	895.387164	13.627815
21.420566	888.779588	13.632819
21.155994	891.525784	13.637824
20.764131	893.289348	13.642829
21.231143	881.956646	13.647834
21.097813	894.422662	13.652839
21.078903	886.884303	13.657843
21.104006	893.635455	13.662848
21.395346	885.919882	13.667853
21.158835	889.090530	13.672858
20.888810	892.736451	13.677863
21.604738	880.914621	13.682867
21.315581	886.556842	13.687872
21.301398	890.261306	13.692877
21.381121	882.959528	13.697882
21.114819	884.646296	13.702887
21.403186	883.888653	13.707891
21.484150	893.111421	13.712896
20.866892	886.718734	13.717901
21.449414	880.724472	13.722906
21.010609	892.266235	13.727911
21.244114	887.524532	13.732915
21.190427	890.965640	13.737920
21.150799	889.053950	13.742925
21.235113	893.200018	13.747930
21.281111	886.695240	13.752935
21.454800	873.206343	13.757939
21.282445	889.589384	13.762944
21.239325	884.380873	13.767949
21.356529	877.954628	13.772954
21.316373	878.069390	13.777959
21.075509	868.205763	13.782963
21.220715	867.199721	13.787968
21.026742	866.036465	13.792973
20.989755	871.165381	13.797978
20.948714	889.798269	13.802983
21.225307	887.249525	13.807987
21.421406	891.335186	13.812992
21.007969	886.524777	13.817997
21.025247	884.274432	13.823002
20.992954	897.014493	13.828007
20.924205	891.377985	13.833011
21.150880	885.941942	13.838016
21.596029	885.652876	13.843021
21.715096	889.900631	13.848026
21.398420	870.984850	13.853031
21.315957	861.589546	13.858035
21.189346	865.100625	13.863040
21.002628	857.852392	13.868045
21.235015	856.031363	13.873050
21.171698	866.701098	13.878055
21.067568	858.234914	13.883059
20.723848	861.894158	13.888064
21.036004	856.991689	13.893069
21.174043	860.711291	13.898074
20.904701	863.322625	13.903079
21.463262	883.818431	13.908083
21.111305	874.193290	13.913088
21.011870	864.747075	13.918093
21.217980	878.201295	13.923098
21.117740	881.017473	13.928103
21.155747	885.393272	13.933107
21.156694	890.710108	13.938112
21.295255	880.142568	13.943117
21.263487	868.775886	13.948122
20.906272	873.252562	13.953127
21.371811	866.606764	13.958131
21.042958	866.143103	13.963136
21.093497	872.387146	13.968141
21.359304	886.181933	13.973146
21.056746	876.550489	13.978151
21.351713	869.474583	13.983155
20.929025	873.772469	13.988160
21.068078	861.233692	13.993165
21.209909	875.155473	13.998170
21.009347	891.336436	14.003175
21.403217	880.408058	14.008179
21.328059	873.438490	14.013184
21.269702	875.366478	14.018189
21.195272	858.330068	14.023207
21.238195	863.643935	14.028224
21.238029	859.593257	14.033242
21.184910	866.021909	14.038259
21.066407	856.483335	14.043277
21.126164	868.108192	14.048295
20.970946	866.473071	14.053312
21.516993	882.893270	14.058330
21.535129	880.483364	14.063347
21.114946	874.020756	14.068365
21.272121	875.104140	14.073383
21.356079	880.655271	14.078400
21.431979	875.162676	14.083418
21.356454	881.274034	14.088435
21.368327	879.788429	14.093453
21.419784	885.632588	14.098471
21.200542	897.786425	14.103488
21.689254	895.836257	14.108506
21.693894	891.847720	14.113523
21.585050	886.029107	14.118541
21.645242	870.072840	14.123559
21.403023	874.208461	14.128576
21.227237	873.141295	14.133594
21.279562	892.356673	14.138611
21.149515	899.083880	14.143629
21.628188	900.106553	14.148647
21.382502	909.494710	14.153664
21.405284	892.702873	14.158682
21.614138	899.924977	14.163699
21.572020	887.237803	14.168717
21.569496	901.445911	14.173735
21.449802	892.487910	14.178752
21.696118	901.690634	14.183770
21.685490	898.807146	14.188787
21.544610	903.591957	14.193805
21.537127	900.838518	14.198823
21.735631	917.624051	14.203840
21.483251	929.811513	14.208858
21.774312	926.288485	14.213875
22.045369	938.389325	14.218893
21.719103	937.700062	14.223911
21.776302	937.292537	14.228928
21.624670	932.669858	14.233946
21.593089	941.953107	14.238963
21.973314	937.947124	14.243981
21.648931	934.405855	14.248999
21.577866	941.101653	14.254016
21.836456	925.588705	14.259034
21.912448	935.867754	14.264051
21.771292	960.650765	14.269069
21.850988	954.303437	14.274087
22.062039	965.539325	14.279104
22.124298	972.150957	14.284122
22.165253	976.776238	14.289139
22.147127	969.345031	14.294157
22.567819	960.321250	14.299175
22.257395	980.906418	14.304192
22.125261	971.215795	14.309210
22.008669	962.450725	14.314227
21.742193	967.848581	14.319245
22.233416	966.992759	14.324263
22.258273	969.085050	14.329280
22.149265	965.962425	14.334298
22.448650	970.632999	14.339315
22.160689	968.197970	14.344333
22.542895	968.536082	14.349351
22.297447	964.099805	14.354368
22.002386	974.870614	14.359386
22.523482	966.691206	14.364403
22.410467	965.967931	14.369421
22.264312	978.744067	14.374439
22.218776	974.905073	14.379456
22.508115	972.769629	14.384474
22.504095	965.993656	14.389491
22.376621	972.492412	14.394509
22.359842	964.244644	14.399527
22.363729	972.410198	14.404544
22.143804	966.016276	14.409562
22.329179	970.878055	14.414579
22.287620	1000.173701	14.419597
22.438951	988.086329	14.424615
22.962497	995.778931	14.429632
22.779245	998.676725	14.434650
22.706516	1000.550219	14.439667
22.549143	994.833678	14.444685
22.855464	995.116258	14.449703
22.800365	1005.767027	14.454720
23.046791	991.555189	14.459738
23.214574	998.598287	14.464755
22.810526	979.916129	14.469773
22.571001	962.832586	14.474791
22.925612	970.717274	14.479808
22.766122	980.445637	14.484826
23.018181	985.845737	14.489843
22.938898	979.292533	14.494861
23.137725	963.774920	14.499879
23.101872	968.516262	14.504896
22.847477	959.277701	14.509914
23.103141	962.887230	14.514931
22.801576	967.600168	14.519949
23.035563	963.669408	14.524967
22.690666	965.504513	14.529984
23.095333	975.869588	14.535002
23.395855	982.493558	14.540019
22.699062	981.489031	14.545037
23.133242	978.956129	14.550055
23.159714	993.287110	14.555072
22.975697	999.791750	14.560090
23.321050	983.769431	14.565107
23.165323	1000.032718	14.570125
23.336958	987.778525	14.575143
23.515083	998.731844	14.580160
23.178479	979.434925	14.585178
23.444007	977.889979	14.590195
23.185990	979.033298	14.595213
23.062664	962.113683	14.600231
23.159235	974.254965	14.605248
23.170599	989.450316	14.610266
23.649348	989.147006	14.615283
23.398056	998.455895	14.620301
23.401869	994.495774	14.625319
23.400330	1002.317739	14.630336
23.234596	992.133843	14.635354
23.521949	997.907394	14.640371
23.501994	999.365082	14.645389
23.744600	998.286231	14.650407
23.198963	1004.444305	14.655424
23.160023	989.387704	14.660442
23.514175	995.523384	14.665459
23.495977	994.319398	14.670477
23.393587	998.300626	14.675495
23.383950	996.363863	14.680512
23.438469	989.004425	14.685530
23.548368	993.190879	14.690547
23.524339	993.478959	14.695565
23.339448	991.516668	14.700583
23.444544	998.085302	14.705600
23.359806	1015.705733	14.710618
23.784038	1018.459458	14.715635
23.687640	1029.270978	14.720653
23.904160	1035.898932	14.725671
24.266897	1029.029832	14.730688
24.089904	1031.009616	14.735706
24.168349	1000.860883	14.740723
23.763649	999.070493	14.745741
23.808648	990.226155	14.750759
24.146204	988.468385	14.755776
23.690800	996.194430	14.760794
23.707019	1001.584962	14.765811
24.026354	1011.524824	14.770829
24.105903	1024.983833	14.775847
24.081380	1023.571654	14.780864
24.096952	1023.825105	14.785882
24.263828	1017.558222	14.790899
23.833050	1013.670554	14.795917
24.181160	1017.951150	14.800935
24.259999	1014.128487	14.805952
23.797586	1022.683024	14.810970
24.144659	1012.624953	14.815987
24.416884	1026.636792	14.821005
24.459564	1023.754214	14.826023
24.458089	1010.673508	14.831040
24.241605	1018.639868	14.836058
24.280429	994.675939	14.841075
24.206391	989.965366	14.846093
24.219912	1010.458015	14.851111
24.506590	1007.467316	14.856128
24.288228	1014.606613	14.861146
24.332030	1005.128566	14.866163
24.188732	1009.901214	14.871181
24.151246	1020.788270	14.876199
24.403722	1016.996111	14.881216
24.089592	1016.265585	14.886234
24.186986	1016.147358	14.891251
24.162596	1016.982876	14.896269
24.179977	1018.165640	14.901287
24.165143	1022.878481	14.906304
24.103648	1032.205881	14.911322
24.403471	1032.549271	14.916339
24.562752	1042.686131	14.921357
24.624290	1040.602738	14.926375
24.581491	1044.854458	14.931392
24.674748	1039.991352	14.936410
24.995716	1045.013991	14.941427
24.940936	1047.836253	14.946445
24.858792	1048.064393	14.951463
24.914138	1032.110294	14.956480
24.166232	1026.541402	14.961498
24.722764	1033.218942	14.966515
24.744456	1036.436394	14.971533
24.977582	1042.382197	14.976551
24.839559	1042.833168	14.981568
24.756787	1050.130171	14.986586
25.029083	1034.666828	14.991603
25.067132	1037.576524	14.996621
24.817981	1043.636994	15.001639
25.269664	1025.611056	15.006656
25.073840	1045.105298	15.011674
25.313086	1028.318105	15.016691
25.223120	1031.830200	15.021709
24.954164	1015.273502	15.026727
24.943704	1012.135149	15.031744
25.158628	1026.080625	15.036762
25.205931	1038.221955	15.041779
25.131601	1035.175576	15.046797
24.942393	1034.856109	15.051815
25.295763	1042.185789	15.056832
25.251651	1041.083454	15.061850
25.605194	1034.689270	15.066867
25.266609	1023.279292	15.071885
25.132209	1012.119886	15.076903
25.272275	1028.120538	15.081920
25.169456	1032.749893	15.086938
25.401860	1033.671863	15.091955
25.601612	1037.564019	15.096973
25.368929	1035.804387	15.101991
25.373888	1019.093893	15.107008
25.489058	1040.997021	15.112026
25.611960	1040.171626	15.117043
25.775840	1021.313897	15.122061
25.451386	1006.850193	15.127079
25.428097	1012.135351	15.132096
24.962335	1009.846641	15.137114
25.146289	1021.764828	15.142131
25.480786	1024.647689	15.147149
25.041277	1040.100607	15.152167
25.653610	1029.547214	15.157184
25.438548	1036.580609	15.162202
25.395808	1027.279935	15.167219
25.266711	1028.890305	15.172237
25.262722	1030.633297	15.177255
25.693249	1044.663947	15.182272
25.711807	1064.869596	15.187290
25.662087	1066.144859	15.192307
26.032813	1069.209131	15.197325
25.775829	1074.896505	15.202343
25.782763	1063.760132	15.207360
25.786697	1080.422739	15.212378
25.844231	1068.496543	15.217395
25.821964	1078.352515	15.222413
25.766494	1073.654683	15.227431
25.826339	1071.689526	15.232448
25.880434	1071.092167	15.237466
25.908682	1069.272041	15.242483
25.983579	1061.634052	15.247501
25.694372	1074.535329	15.252519
26.379205	1069.176766	15.257536
26.181529	1073.116586	15.262554
26.119731	1075.559322	15.267571
26.338390	1058.147775	15.272589
26.181758	1062.315414	15.277607
26.325129	1065.966473	15.282624
26.289870	1061.240254	15.287642
25.975242	1067.375667	15.292659
26.194181	1070.346177	15.297677
25.924907	1061.610117	15.302695
26.225507	1060.784692	15.307712
26.316381	1066.877454	15.312730
26.431603	1067.898336	15.317747
26.249791	1064.935156	15.322765
26.425060	1076.552769	15.327783
26.577304	1063.090443	15.332800
26.315262	1071.543843	15.337818
26.557778	1064.492564	15.342835
26.476242	1062.573551	15.347853
26.009249	1068.262957	15.352871
26.083863	1056.157879	15.357888
26.136565	1067.463143	15.362906
26.504559	1079.564372	15.367923
26.721192	1089.701557	15.372941
26.951691	1099.633628	15.377959
27.195965	1069.115405	15.382976
26.785282	1078.820978	15.387994
26.758302	1061.550844	15.393011
26.897568	1054.291108	15.398029
26.730981	1063.748541	15.403047
26.934034	1062.642962	15.408064
26.902595	1064.366742	15.413082
26.633066	1058.463581	15.418099
26.947226	1056.676504	15.423117
26.813760	1056.337135	15.428135
26.976039	1064.384676	15.433152
26.895847	1057.981011	15.438170
26.468090	1069.082921	15.443187
26.708417	1061.676509	15.448205
26.395110	1068.255280	15.453223
26.698403	1067.023609	15.458240
26.947386	1075.873682	15.463258
26.904476	1086.410888	15.468275
27.008639	1087.056029	15.473293
27.032670	1084.283373	15.478311
27.369984	1090.248757	15.483328
27.257901	1083.211554	15.488346
27.072730	1089.007023	15.493363
27.369813	1077.605727	15.498381
27.202395	1090.769150	15.503399
26.900696	1083.430298	15.508416
26.663999	1088.972877	15.513434
26.966512	1086.475113	15.518451
27.250446	1085.205631	15.523469
26.827519	1086.538845	15.528487
26.933792	1085.209613	15.533504
26.890517	1095.076812	15.538522
27.170305	1108.654965	15.543539
27.628380	1111.552740	15.548557
27.413730	1127.746921	15.553575
27.551582	1111.614417	15.558592
27.624856	1128.465784	15.563610
27.579209	1110.106947	15.568627
27.551222	1121.286704	15.573645
27.375389	1117.828656	15.578663
27.713779	1119.718390	15.583680
27.830744	1115.653678	15.588698
27.500243	1109.116888	15.593715
27.837570	1113.842802	15.598733
27.757259	1118.632180	15.603751
27.717195	1105.275986	15.608768
27.617701	1106.087309	15.613786
27.611180	1112.890864	15.618803
28.037241	1109.225145	15.623821
28.126969	1117.057783	15.628839
28.052564	1090.868740	15.633856
27.853099	1075.486884	15.638874
27.538822	1087.203030	15.643891
27.799455	1077.182296	15.648909
27.686287	1085.250185	15.653927
27.881587	1097.116290	15.658944
28.043868	1107.611348	15.663962
27.973962	1103.979116	15.668979
28.058026	1108.153995	15.673997
27.799342	1115.186520	15.679015
28.091227	1115.334560	15.684032
27.922023	1112.845961	15.689050
27.802725	1109.396201	15.694067
28.267631	1114.186707	15.699085
27.980310	1114.430268	15.704103
28.352831	1106.221000	15.709120
27.846751	1113.601276	15.714138
28.086044	1105.318879	15.719155
28.434397	1099.458722	15.724173
27.906245	1113.357634	15.729191
28.364134	1100.632997	15.734208
28.617714	1107.420234	15.739226
28.278313	1113.141215	15.744243
28.394655	1105.125379	15.749261
28.297162	1102.905327	15.754279
27.995662	1112.393747	15.759296
28.359757	1102.265263	15.764314
28.055886	1103.107608	15.769331
28.234482	1103.569429	15.774349
28.222625	1118.457176	15.779367
28.567976	1129.385498	15.784384
28.720713	1128.641851	15.789402
28.772886	1143.198532	15.794419
29.175995	1121.689859	15.799437
28.948045	1118.867727	15.804455
28.822195	1097.194927	15.809472
28.543143	1103.266483	15.814490
28.713430	1100.409153	15.819507
28.850409	1095.392773	15.824525
28.870243	1094.083618	15.829543
28.676534	1096.902879	15.834560
28.733059	1096.298841	15.839578
28.459440	1103.928313	15.844595
29.249393	1110.661466	15.849613
28.943378	1111.077886	15.854631
28.797308	1098.012297	15.859648
28.826075	1105.198736	15.864666
28.758958	1112.024537	15.869683
28.777145	1127.898456	15.874701
28.765667	1133.644220	15.879719
28.917794	1124.035567	15.884736
29.461803	1131.364776	15.889754
29.057272	1128.065888	15.894771
29.263574	1123.266519	15.899789
29.025013	1126.731554	15.904807
29.084346	1126.767254	15.909824
29.310409	1120.176299	15.914842
29.285509	1130.348887	15.919859
29.426917	1121.072264	15.924877
28.828230	1128.017455	15.929895
29.155715	1129.303347	15.934912
29.399592	1123.868808	15.939930
29.218106	1131.420683	15.944947
29.275908	1127.657971	15.949965
29.269936	1132.404038	15.954983
29.353193	1119.446566	15.960000
29.394263	1123.900426	15.965018
29.255752	1131.201641	15.970035
29.592502	1112.331953	15.975053
29.258612	1124.386293	15.980071
29.290090	1127.463787	15.985088
29.528067	1141.984541	15.990106
29.703277	1157.371003	15.995123
29.802331	1147.402730	16.000141
29.783939	1159.954167	16.005159
29.787509	1145.348350	16.010176
29.769270	1125.847884	16.015194
29.302837	1131.892710	16.020211
29.439764	1147.761869	16.025229
29.779386	1152.690340	16.030247
29.678422	1148.383537	16.035264
30.341659	1151.305227	16.040282
29.837171	1158.710439	16.045299
30.270065	1150.823408	16.050317
30.280444	1151.601480	16.055335
29.852745	1139.343648	16.060352
30.160233	1135.440444	16.065370
30.090034	1124.906180	16.070387
30.243228	1107.563214	16.075405
29.815675	1123.232951	16.080423
30.106678	1124.724425	16.085440
30.375633	1129.027117	16.090458
29.943402	1135.873410	16.095475
30.008528	1117.342749	16.100493
30.137810	1130.111268	16.105511
30.008218	1147.150732	16.110528
30.295156	1147.458430	16.115546
30.158332	1150.978027	16.120563
30.400964	1151.105611	16.125581
30.528559	1159.087954	16.130599
30.321288	1150.629799	16.135616
30.486026	1153.736380	16.140634
30.344771	1149.283427	16.145651
30.448643	1150.373761	16.150669
30.396494	1143.087882	16.155687
30.447551	1149.545661	16.160704
30.373913	1150.341852	16.165722
30.064096	1160.185541	16.170739
30.128394	1145.357691	16.175757
30.284521	1145.599739	16.180775
30.227753	1155.102635	16.185792
30.695364	1153.363429	16.190810
30.387570	1169.931144	16.195827
30.396072	1167.434642	16.200845
30.645334	1172.204507	16.205863
30.629738	1174.399230	16.210880
30.826252	1172.195196	16.215898
30.660471	1170.634080	16.220915
30.977311	1167.250021	16.225933
30.553693	1176.954577	16.230951
30.973158	1168.613523	16.235968
30.954354	1180.564178	16.240986
30.966376	1172.734820	16.246003
30.808031	1172.144599	16.251021
30.915933	1180.592542	16.256039
30.893444	1176.097045	16.261056
31.089108	1169.062626	16.266074
30.846490	1181.115040	16.271091
31.015908	1174.684097	16.276109
31.025770	1171.352142	16.281127
30.785691	1173.437955	16.286144
30.949134	1189.523144	16.291162
30.977698	1199.463896	16.296179
31.127647	1204.174109	16.301197
31.290856	1215.718257	16.306215
31.523975	1204.561433	16.311232
31.674897	1207.797637	16.316250
31.293164	1202.989782	16.321267
31.385727	1204.081924	16.326285
31.898812	1190.970898	16.331303
31.473800	1205.229383	16.336320
31.681145	1191.512770	16.341338
31.578771	1204.025732	16.346355
31.515872	1202.012496	16.351373
31.570233	1191.227094	16.356391
31.631169	1186.387970	16.361408
31.969769	1189.202574	16.366426
31.655561	1194.678908	16.371443
31.705591	1169.649589	16.376461
31.877909	1158.826523	16.381479
31.803027	1165.176986	16.386496
31.718152	1154.849523	16.391514
31.646956	1159.286694	16.396531
31.839653	1160.422635	16.401549
31.986754	1164.552872	16.406567
31.573075	1175.102086	16.411584
32.240574	1183.820989	16.416602
31.696712	1183.558079	16.421619
31.974111	1187.310484	16.426637
31.994691	1188.544660	16.431655
31.554072	1194.627864	16.436672
31.958438	1193.258946	16.441690
31.635293	1196.366271	16.446707
32.103039	1195.654175	16.451725
32.204004	1190.135443	16.456743
32.012296	1193.586730	16.461760
32.154234	1189.629694	16.466778
32.163498	1193.322621	16.471795
32.072727	1195.598547	16.476813
32.194885	1189.791731	16.481831
32.258842	1198.734307	16.486848
32.247505	1193.252360	16.491866
32.312253	1189.982430	16.496883
32.017433	1194.230344	16.501901
32.352371	1195.252371	16.506919
32.173221	1218.838577	16.511936
32.968570	1206.420235	16.516954
32.631376	1216.122043	16.521971
32.569574	1201.430645	16.526989
32.770799	1184.751576	16.532007
32.465567	1193.757748	16.537024
32.258612	1186.040381	16.542042
32.361178	1200.128209	16.547059
32.354499	1208.394677	16.552077
32.675313	1222.249527	16.557095
32.429239	1216.281214	16.562112
32.637228	1215.053720	16.567130
32.420005	1214.326602	16.572147
32.117083	1223.507022	16.577165
32.393315	1219.239137	16.582183
32.678465	1234.504333	16.587200
33.250589	1244.545608	16.592218
33.064058	1243.821458	16.597235
33.257535	1246.226657	16.602253
33.390690	1224.982672	16.607271
33.180351	1226.061778	16.612288
33.406965	1213.751437	16.617306
33.312575	1210.494299	16.622323
33.053449	1209.611850	16.627341
33.277593	1203.491476	16.632359
33.041916	1209.917937	16.637376
33.325002	1208.730374	16.642394
33.212291	1208.755761	16.647411
33.606367	1210.746734	16.652429
33.350723	1200.916786	16.657447
33.192935	1205.597432	16.662464
33.564717	1207.098053	16.667482
33.306202	1206.514368	16.672499
33.068640	1213.346952	16.677517
33.462974	1205.156170	16.682535
33.012284	1215.476946	16.687552
33.173436	1200.767294	16.692570
33.277903	1222.990142	16.697587
33.531130	1235.224631	16.702605
33.577647	1231.429087	16.707623
33.482825	1245.960553	16.712640
33.770053	1233.604350	16.717658
33.773480	1233.902212	16.722675
33.512227	1254.599470	16.727693
33.884721	1239.113638	16.732711
33.742347	1242.468983	16.737728
33.803329	1231.443406	16.742746
33.667928	1246.262903	16.747763
33.706569	1244.609403	16.752781
33.786976	1240.869797	16.757799
33.631919	1246.306611	16.762816
33.647256	1240.798370	16.767834
33.886856	1232.067561	16.772851
33.979754	1249.790502	16.777869
34.110735	1229.394680	16.782887
34.180404	1244.371797	16.787904
34.171089	1245.617037	16.792922
34.105223	1235.857468	16.797939
34.150460	1240.121945	16.802957
34.552526	1233.683759	16.807975
33.841293	1240.993001	16.812992
34.325532	1236.111518	16.818010
34.155288	1232.737490	16.823027
34.148735	1240.812056	16.828045
34.378971	1251.167400	16.833063
34.470583	1257.374951	16.838080
34.303819	1253.624426	16.843098
34.365271	1252.901624	16.848115
34.498048	1253.038864	16.853133
34.705506	1255.070616	16.858151
34.219392	1254.188187	16.863168
34.723402	1260.965444	16.868186
34.465545	1253.260878	16.873203
34.348344	1266.205675	16.878221
34.592243	1257.084071	16.883239
34.357997	1255.217699	16.888256
34.347093	1257.646057	16.893274
34.365838	1257.988665	16.898291
34.469159	1263.591909	16.903309
34.412892	1260.094309	16.908327
34.347963	1291.752136	16.913344
34.716673	1293.018885	16.918362
35.108843	1291.785606	16.923379
34.567874	1294.462094	16.928397
34.911543	1300.624746	16.933415
34.983695	1288.587503	16.938432
34.902970	1301.340905	16.943450
35.372166	1288.659918	16.948467
35.264360	1298.384970	16.953485
35.518453	1284.833839	16.958503
35.035110	1296.883843	16.963520
35.068402	1294.768741	16.968538
35.586334	1289.024603	16.973555
35.050398	1299.983499	16.978573
34.811689	1281.623775	16.983591
35.223294	1287.662334	16.988608
35.311748	1293.761870	16.993626
35.321418	1291.943106	16.998643
35.064328	1291.640749	17.003661
35.342449	1279.625719	17.008679
35.341396	1308.742505	17.013696
35.507276	1307.682161	17.018714
35.848871	1304.751856	17.023731
35.566031	1321.432162	17.028749
36.127738	1309.338849	17.033767
35.645280	1304.133334	17.038784
35.644425	1282.769070	17.043802
35.924977	1286.654700	17.048819
35.442122	1288.170512	17.053837
35.724554	1292.880075	17.058855
35.384754	1304.070377	17.063872
35.646224	1320.958019	17.068890
35.783263	1314.639140	17.073907
35.514384	1315.063799	17.078925
36.157781	1305.258705	17.083943
36.034152	1323.046154	17.088960
36.019409	1309.261034	17.093978
36.221452	1312.157214	17.098995
36.210923	1317.688978	17.104013
36.122526	1305.348577	17.109031
35.920682	1315.579402	17.114048
36.095288	1309.866416	17.119066
36.149994	1304.680621	17.124083
35.855317	1308.697320	17.129101
35.992675	1308.015890	17.134119
36.075940	1309.738708	17.139136
36.031468	1314.070994	17.144154
35.981343	1303.714289	17.149171
35.905561	1313.874673	17.154189
36.211198	1318.918730	17.159207
36.298726	1342.333623	17.164224
36.086818	1345.781874	17.169242
36.667188	1338.459513	17.174259
36.660178	1348.451657	17.179277
36.884610	1345.577780	17.184295
36.347615	1339.772212	17.189312
36.772600	1334.113664	17.194330
37.114327	1338.332458	17.199347
36.889652	1351.332222	17.204365
37.285925	1331.655263	17.209383
36.949962	1341.921652	17.214400
36.941126	1346.112990	17.219418
37.081047	1326.862298	17.224435
36.749432	1335.438626	17.229453
36.725366	1333.331093	17.234471
36.892016	1336.001697	17.239488
36.826182	1340.878498	17.244506
37.068789	1343.513396	17.249523
36.896470	1345.725274	17.254541
36.886223	1334.918610	17.259559
37.218249	1341.597496	17.264576
36.991638	1340.395260	17.269594
37.159539	1330.156342	17.274611
37.015361	1339.910817	17.279629
36.871883	1329.021590	17.284647
36.907782	1340.092230	17.289664
37.112397	1342.766218	17.294682
37.205008	1356.031551	17.299699
37.346798	1366.997238	17.304717
37.317423	1358.246331	17.309735
37.255398	1378.158541	17.314752
37.022480	1384.062411	17.319770
37.577972	1371.605109	17.324787
37.157244	1367.102281	17.329805
37.168465	1373.950317	17.334823
37.392447	1366.862525	17.339840
37.589301	1378.849733	17.344858
37.786592	1379.157578	17.349875
37.591135	1387.051574	17.354893
37.982167	1393.677031	17.359911
37.891357	1387.438502	17.364928
37.607823	1383.134005	17.369946
37.833713	1382.948094	17.374963
37.804835	1399.147556	17.379981
38.113085	1397.792376	17.384999
38.000976	1400.570369	17.390016
37.700680	1399.629981	17.395034
38.178237	1396.328775	17.400051
38.222776	1404.101138	17.405069
38.203158	1385.462531	17.410087
38.261870	1397.462348	17.415104
37.857067	1403.097921	17.420122
38.058156	1390.310172	17.425139
37.939671	1390.507934	17.430157
38.151638	1395.508757	17.435175
38.367857	1391.618469	17.440192
37.991864	1391.544277	17.445210
38.447451	1393.382327	17.450227
38.200882	1397.935625	17.455245
38.196098	1384.971509	17.460263
37.964423	1390.214537	17.465280
38.054249	1397.910463	17.470298
38.564619	1412.211876	17.475315
38.590665	1419.851922	17.480333
38.466693	1423.468632	17.485351
39.010919	1413.402439	17.490368
38.881339	1418.169886	17.495386
38.951758	1407.537487	17.500403
39.100763	1425.932794	17.505421
39.055180	1414.812392	17.510439
39.343079	1392.890698	17.515456
38.994974	1394.619403	17.520474
38.914228	1375.578438	17.525491
38.902819	1393.459758	17.530509
39.023578	1387.335346	17.535527
38.941658	1379.865339	17.540544
38.858925	1384.642607	17.545562
38.881520	1371.809411	17.550579
38.817183	1401.343875	17.555597
38.920142	1413.619784	17.560615
39.159672	1417.250878	17.565632
38.997707	1419.681333	17.570650
38.888684	1410.438172	17.575667
39.070452	1418.360112	17.580685
39.215995	1415.074100	17.585703
39.084802	1416.165765	17.590720
38.679178	1418.144311	17.595738
39.072892	1425.609323	17.600755
39.259304	1443.629037	17.605773
39.322377	1442.902821	17.610791
39.730382	1442.181368	17.615808
39.550453	1451.021428	17.620826
39.804757	1443.285415	17.625843
39.479365	1450.989389	17.630861
39.470783	1452.347785	17.635879
39.666881	1453.244115	17.640896
39.605990	1459.197657	17.645914
39.564587	1439.296207	17.650931
39.701766	1442.562970	17.655949
39.731657	1448.050586	17.660967
39.913080	1434.465289	17.665984
39.490684	1450.837675	17.671002
39.890378	1459.036332	17.676019
39.802910	1469.763388	17.681037
39.755830	1467.030313	17.686055
40.174241	1475.023080	17.691072
39.988675	1483.834958	17.696090
40.266840	1470.546436	17.701107
39.935061	1473.236782	17.706125
39.776682	1482.472174	17.711143
40.306297	1473.746091	17.716160
40.240672	1478.303589	17.721178
39.923192	1483.808079	17.726195
40.011500	1493.807144	17.731213
40.276450	1504.212187	17.736231
40.388665	1509.810962	17.741248
40.449506	1505.124327	17.746266
40.744790	1503.841990	17.751283
40.756026	1511.891848	17.756301
40.743150	1505.068273	17.761319
40.891049	1495.768354	17.766336
40.814161	1506.375776	17.771354
40.889411	1503.111966	17.776371
41.045107	1489.341963	17.781389
41.020171	1479.984676	17.786407
40.856785	1469.876357	17.791424
40.611295	1478.907781	17.796442
40.576893	1488.788776	17.801459
40.849651	1503.277608	17.806477
40.933929	1503.471348	17.811495
41.153732	1496.607523	17.816512
40.761901	1500.932342	17.821530
40.873117	1493.357545	17.826547
41.104348	1503.450224	17.831565
41.039505	1490.910858	17.836583
41.001621	1488.931344	17.841600
41.091567	1487.879952	17.846618
41.513590	1486.736276	17.851635
41.662587	1489.236696	17.856653
41.259802	1483.230345	17.861671
41.708340	1489.646907	17.866688
41.649555	1499.751229	17.871706
41.419375	1497.822831	17.876723
41.370667	1487.764634	17.881741
41.170674	1489.057607	17.886759
41.451569	1492.444604	17.891776
41.671575	1495.065831	17.896794
41.646192	1482.713656	17.901811
41.661395	1492.096759	17.906829
41.661904	1501.711867	17.911847
41.790716	1488.285917	17.916864
41.860301	1494.830555	17.921882
41.812483	1505.453789	17.926899
41.882831	1502.275702	17.931917
41.746533	1512.321610	17.936935
42.038833	1516.790580	17.941952
42.162514	1524.602295	17.946970
42.110491	1519.565575	17.951987
42.500876	1511.284020	17.957005
42.230470	1513.997619	17.962023
42.265558	1490.805801	17.967040
42.052519	1482.488365	17.972058
41.952853	1484.765754	17.977075
42.016747	1502.381949	17.982093
41.782245	1505.777214	17.987111
42.150333	1514.141387	17.992128
41.996201	1521.833816	17.997146
42.100184	1509.308407	18.002163
42.209311	1515.915960	18.007181
42.077254	1526.881398	18.012199
42.416802	1524.634053	18.017216
42.615264	1545.212792	18.022234
42.778297	1544.808822	18.027251
43.171325	1541.093212	18.032269
43.100556	1543.650712	18.037287
43.171037	1524.358924	18.042304
42.664727	1525.873780	18.047322
42.628072	1514.687385	18.052339
43.089637	1507.495570	18.057357
42.411069	1515.417920	18.062375
43.002717	1520.430592	18.067392
43.304105	1524.597675	18.072410
42.982639	1527.563232	18.077427
43.178288	1529.148607	18.082445
42.906299	1519.572725	18.087463
43.287559	1522.671596	18.092480
43.292508	1547.592754	18.097498
43.143582	1537.602414	18.102515
43.673826	1525.496637	18.107533
43.105158	1540.706420	18.112551
43.291110	1531.282436	18.117568
43.170301	1531.323271	18.122586
43.244751	1542.737121	18.127603
43.267105	1540.062171	18.132621
42.840083	1548.738781	18.137639
43.070444	1536.897893	18.142656
43.156356	1539.513773	18.147674
43.054967	1543.178820	18.152691
43.543009	1559.519387	18.157709
43.456447	1571.317580	18.162727
43.690888	1564.312965	18.167744
43.677462	1579.130652	18.172762
43.917694	1573.144408	18.177779
43.805673	1561.093840	18.182797
43.585687	1559.624693	18.187815
43.949805	1555.652574	18.192832
43.848043	1566.001318	18.197850
43.801843	1565.603975	18.202867
44.033495	1556.707502	18.207885
43.973156	1561.821022	18.212903
44.207678	1560.815780	18.217920
44.185296	1553.705840	18.222938
44.020788	1564.876251	18.227955
43.939371	1576.222179	18.232973
44.225756	1590.885101	18.237991
44.629067	1592.404332	18.243008
44.372336	1590.303979	18.248026
44.533596	1595.039258	18.253043
44.580557	1593.025750	18.258061
44.338391	1600.681924	18.263079
44.386550	1591.956263	18.268096
44.610763	1588.212510	18.273114
44.620404	1592.559844	18.278131
44.658773	1598.667496	18.283149
44.511482	1600.886433	18.288167
44.862546	1588.544917	18.293184
44.886366	1594.665899	18.298202
44.845922	1602.683152	18.303219
45.111700	1593.490211	18.308237
44.723317	1602.365179	18.313255
44.822292	1593.758825	18.318272
44.849899	1591.693349	18.323290
44.670448	1597.349684	18.328307
45.028137	1585.987089	18.333325
45.021462	1590.576119	18.338343
45.046944	1579.489874	18.343360
44.938154	1600.485772	18.348378
45.034006	1619.868204	18.353395
45.229137	1616.124363	18.358413
45.404378	1620.486194	18.363431
45.332067	1625.378280	18.368448
45.377362	1622.216746	18.373466
45.364278	1615.707751	18.378483
45.278925	1617.103573	18.383501
45.264794	1624.421378	18.388519
45.462322	1617.046679	18.393536
45.426508	1621.720589	18.398554
45.381338	1622.210250	18.403571
45.848992	1624.169101	18.408589
45.368876	1636.162240	18.413607
45.595805	1640.545721	18.418624
45.985476	1644.379441	18.423642
45.901525	1635.083375	18.428659
46.219094	1652.689184	18.433677
46.085190	1646.861675	18.438695
45.941689	1648.230595	18.443712
45.843851	1650.183680	18.448730
45.821406	1646.841038	18.453747
45.890441	1648.103705	18.458765
45.994693	1642.519784	18.463783
46.339258	1641.254745	18.468800
46.124522	1645.290246	18.473818
46.108078	1642.648206	18.478835
46.449763	1648.196283	18.483853
46.105117	1636.083652	18.488871
46.402680	1642.387510	18.493888
46.562920	1631.534560	18.498906
46.372105	1649.509300	18.503923
46.263081	1642.705712	18.508941
46.569547	1645.311606	18.513959
46.626775	1659.567557	18.518976
46.841354	1660.633984	18.523994
46.946500	1662.265267	18.529011
46.786210	1659.694927	18.534029
46.672314	1670.062982	18.539047
47.005704	1662.477833	18.544064
47.162255	1663.336441	18.549082
46.803023	1668.425307	18.554099
47.133104	1647.493786	18.559117
47.071485	1658.216859	18.564135
46.905116	1656.287699	18.569152
47.230410	1656.073350	18.574170
46.897438	1656.871601	18.579187
47.322438	1656.142711	18.584205
47.347364	1661.812094	18.589223
47.164628	1657.752556	18.594240
47.283542	1650.764752	18.599258
46.880471	1668.417867	18.604275
47.319451	1655.076003	18.609293
47.113508	1660.473896	18.614311
46.860511	1658.829108	18.619328
47.195690	1669.342619	18.624346
47.159304	1692.018079	18.629363
47.579850	1679.679563	18.634381
47.952782	1680.731749	18.639399
47.819047	1690.558724	18.644416
48.245836	1676.108245	18.649434
47.846898	1678.927313	18.654451
47.960073	1683.081987	18.659469
48.247603	1676.440081	18.664487
47.952106	1679.208047	18.669504
47.973787	1682.449241	18.674522
47.879673	1683.652987	18.679539
48.329466	1675.965899	18.684557
48.184282	1688.449926	18.689575
48.029047	1688.010193	18.694592
48.010129	1685.444044	18.699610
48.028416	1691.380335	18.704627
47.786087	1688.256791	18.709645
47.840817	1686.713932	18.714663
48.187498	1696.940916	18.719680
48.594343	1711.487224	18.724698
48.304068	1702.669179	18.729715
48.695387	1707.690272	18.734733
48.358618	1715.459119	18.739751
48.442789	1699.910243	18.744768
48.581682	1705.493829	18.749786
48.592572	1710.397843	18.754803
48.704584	1706.524091	18.759821
48.852802	1710.218586	18.764839
48.574101	1712.016481	18.769856
48.598690	1704.732238	18.774874
48.691568	1709.041165	18.779891
48.981162	1729.876191	18.784909
49.097254	1739.405384	18.789927
48.870648	1739.386014	18.794944
49.490726	1727.075412	18.799962
49.472024	1738.870783	18.804979
49.230845	1726.656633	18.809997
49.452128	1718.796755	18.815015
49.548293	1713.229827	18.820032
49.584884	1704.897621	18.825050
49.428241	1699.243602	18.830067
49.844439	1692.280726	18.835085
49.773528	1684.031742	18.840103
49.439765	1689.689126	18.845120
49.601046	1695.626210	18.850138
49.453809	1689.185766	18.855155
49.568613	1690.875287	18.860173
49.433828	1704.737193	18.865191
49.769161	1704.011590	18.870208
49.813071	1718.864320	18.875226
49.902645	1723.285461	18.880243
49.907751	1734.504458	18.885261
49.727060	1727.341029	18.890279
49.736415	1727.225828	18.895296
50.032803	1723.081998	18.900314
49.850711	1718.040784	18.905331
49.760154	1729.765810	18.910349
50.108663	1721.317785	18.915367
49.947409	1727.545415	18.920384
50.268100	1740.438104	18.925402
49.865363	1751.451598	18.930419
50.205050	1747.802645	18.935437
50.329304	1753.536447	18.940455
50.286552	1751.584415	18.945472
50.674362	1753.364111	18.950490
50.735653	1751.675482	18.955507
50.767747	1752.605852	18.960525
50.699429	1747.771424	18.965543
50.629969	1747.115092	18.970560
50.666887	1745.633269	18.975578
50.430137	1751.185544	18.980595
50.606930	1749.535124	18.985613
50.876696	1745.335759	18.990631
50.536630	1759.315397	18.995648
50.695058	1764.681962	19.000666
50.731549	1774.862515	19.005683
50.922375	1776.432958	19.010701
50.966952	1779.258392	19.015719
51.164107	1776.135528	19.020736
51.245165	1777.547298	19.025754
50.992114	1780.866933	19.030771
51.100907	1775.752568	19.035789
51.714105	1765.316490	19.040807
51.246432	1770.663355	19.045824
51.360116	1774.053490	19.050842
51.339933	1775.851064	19.055859
51.875352	1769.424412	19.060877
51.636246	1771.198696	19.065895
51.402475	1768.561404	19.070912
51.533434	1771.483172	19.075930
51.572503	1793.671708	19.080947
51.652578	1791.676487	19.085965
51.878234	1791.887011	19.090983
51.839654	1803.197970	19.096000
52.094418	1794.804178	19.101018
52.111178	1799.383245	19.106035
52.291147	1790.475996	19.111053
52.156149	1796.087566	19.116071
51.970745	1797.283858	19.121088
52.436944	1783.124289	19.126106
52.181456	1793.804447	19.131123
52.397692	1789.928209	19.136141
52.156802	1790.730657	19.141159
52.079434	1794.711258	19.146176
52.383546	1786.216794	19.151194
52.496397	1792.094001	19.156211
52.349857	1784.591618	19.161229
52.449912	1787.823483	19.166247
52.137064	1799.727160	19.171264
52.382535	1795.622890	19.176282
52.624442	1822.624010	19.181299
52.679543	1820.522656	19.186317
52.824226	1818.564319	19.191335
52.538782	1820.772286	19.196352
52.752274	1818.604775	19.201370
52.773497	1820.095305	19.206387
52.787295	1819.370636	19.211405
52.925806	1818.195073	19.216423
52.972994	1841.547993	19.221440
53.498988	1833.499461	19.226458
53.595342	1852.133367	19.231475
53.437671	1837.011448	19.236493
53.709479	1817.487390	19.241511
53.394085	1801.418536	19.246528
53.882201	1804.247174	19.251546
53.671817	1805.340485	19.256563
53.603559	1804.084640	19.261581
53.636010	1806.923025	19.266599
53.069254	1809.374053	19.271616
53.659302	1807.097729	19.276634
53.370402	1816.987287	19.281651
53.591394	1830.389883	19.286669
54.008545	1825.676209	19.291687
53.719875	1841.337151	19.296704
54.164237	1837.015535	19.301722
53.948887	1838.287392	19.306739
53.900625	1834.889049	19.311757
54.150723	1831.122230	19.316775
53.911130	1834.851862	19.321792
54.325388	1827.179800	19.326810
53.848904	1838.516577	19.331827
53.852202	1829.219056	19.336845
54.079459	1836.802065	19.341863
54.012667	1848.015312	19.346880
54.379712	1842.103116	19.351898
54.180157	1872.080098	19.356915
54.721523	1859.108685	19.361933
54.807883	1863.508360	19.366951
54.537307	1878.680392	19.371968
54.506573	1867.085368	19.376986
54.812282	1862.301365	19.382003
54.652476	1868.774216	19.387021
54.607242	1855.891634	19.392039
54.882558	1867.778648	19.397056
54.902606	1857.584961	19.402074
55.093093	1858.453899	19.407091
54.774598	1855.646058	19.412109
54.929407	1857.934831	19.417127
54.746365	1865.337896	19.422144
55.047539	1866.203340	19.427162
55.284833	1875.719587	19.432179
55.133003	1895.813569	19.437197
55.129957	1892.455192	19.442215
55.158540	1890.139407	19.447232
55.339275	1881.301194	19.452250
55.578750	1877.721674	19.457267
55.526114	1884.622608	19.462285
55.769504	1882.456612	19.467303
55.255772	1881.671349	19.472320
55.493720	1882.853617	19.477338
55.848404	1883.436822	19.482355
55.701825	1898.021239	19.487373
56.108020	1908.695061	19.492391
55.962545	1902.021433	19.497408
56.102948	1902.881057	19.502426
56.338019	1908.425789	19.507443
56.183687	1899.257181	19.512461
56.190359	1893.415020	19.517479
56.125267	1902.049849	19.522496
56.270091	1899.885412	19.527514
56.570491	1901.927605	19.532531
56.402604	1909.624004	19.537549
56.328196	1898.098841	19.542567
56.244589	1902.958215	19.547584
56.541378	1890.886223	19.552602
56.473959	1909.167221	19.557619
56.472277	1891.501952	19.562637
56.764501	1885.121899	19.567655
56.852625	1896.643960	19.572672
56.466775	1889.382606	19.577690
56.842245	1886.630831	19.582707
56.493642	1893.934471	19.587725
56.597931	1888.307979	19.592743
56.532937	1894.345724	19.597760
56.623083	1895.458754	19.602778
56.744658	1919.951394	19.607795
56.854514	1930.373615	19.612813
57.123701	1919.728019	19.617831
56.830145	1920.746512	19.622848
57.206092	1925.842494	19.627866
57.285341	1915.312135	19.632883
57.346083	1919.357262	19.637901
57.444170	1921.903631	19.642919
57.312004	1936.682416	19.647936
57.445242	1947.177999	19.652954
57.596480	1940.192766	19.657971
57.580615	1946.464945	19.662989
57.983837	1935.945827	19.668007
57.656839	1941.113017	19.673024
57.998163	1938.689148	19.678042
58.204842	1940.740001	19.683059
57.910789	1943.731155	19.688077
58.082592	1931.295242	19.693095
58.176992	1941.878813	19.698112
58.070454	1937.412213	19.703130
58.243326	1934.374985	19.708147
58.150564	1942.087736	19.713165
58.192758	1941.183927	19.718183
58.290096	1928.953374	19.723200
58.187579	1941.652611	19.728218
58.533187	1935.188517	19.733235
58.564634	1935.879902	19.738253
58.428420	1928.633775	19.743271
58.407369	1936.641827	19.748288
58.652649	1948.758641	19.753306
58.770583	1967.754198	19.758323
58.614258	1971.395080	19.763341
58.925550	1965.512176	19.768359
58.538689	1974.462630	19.773376
58.874300	1963.561017	19.778394
59.117301	1958.321366	19.783411
59.081594	1967.725480	19.788429
59.261900	1958.322570	19.793447
59.100215	1963.962055	19.798464
59.060523	1961.040518	19.803482
59.340179	1960.248277	19.808499
58.761518	1969.679203	19.813517
59.161677	1955.238988	19.818535
59.327559	1986.052983	19.823552
59.368071	1991.370796	19.828570
59.563081	1980.501030	19.833587
59.348013	1996.021412	19.838605
59.706363	1988.619306	19.843623
59.935963	1992.670560	19.848640
59.816226	1992.284931	19.853658
59.970683	1992.670410	19.858675
59.729667	1987.520520	19.863693
60.155110	1988.638290	19.868711
59.993611	1984.200890	19.873728
59.907413	1992.983858	19.878746
60.029319	1987.599912	19.883763
60.009702	1990.987761	19.888781
60.243045	1985.694584	19.893799
60.023625	1980.876309	19.898816
60.563175	1979.265542	19.903834
60.205828	1983.887024	19.908851
60.042707	1989.251467	19.913869
60.490436	1987.208601	19.918887
60.606334	2011.740053	19.923904
60.230085	2007.052173	19.928922
60.629426	2002.427801	19.933939
60.031546	2012.813507	19.938957
60.464848	2010.595184	19.943975
60.473049	2014.678604	19.948992
60.703947	2026.558675	19.954010
60.981958	2034.383808	19.959027
60.719609	2037.071048	19.964045
61.003805	2037.975391	19.969063
61.293391	2041.730798	19.974080
61.251701	2040.612269	19.979098
61.096577	2030.185271	19.984115
61.283533	2031.521976	19.989133
61.359244	2020.235473	19.994151
61.211535	2029.177711	19.999168
61.541002	2032.492597	20.004186
61.573934	2027.261253	20.009203
61.497727	2044.164266	20.014221
61.773656	2051.475356	20.019239
62.112044	2046.173271	20.024256
61.999379	2053.433073	20.029274
62.366389	2024.351482	20.034291
62.066153	2025.677789	20.039309
62.352393	2017.368514	20.044327
62.405176	2002.871962	20.049344
61.971721	2011.400431	20.054362
62.287618	2007.122848	20.059379
62.229264	2006.768330	20.064397
62.366613	2009.819690	20.069415
62.146360	2012.377515	20.074432
61.892462	2009.601813	20.079450
62.551322	2024.325329	20.084467
62.201746	2037.974838	20.089485
62.101541	2037.373733	20.094503
62.610185	2038.533296	20.099520
62.607479	2034.660448	20.104538
62.622871	2044.987703	20.109555
62.590461	2053.066846	20.114573
62.551890	2034.979417	20.119591
62.657103	2040.203559	20.124608
62.807516	2035.702245	20.129626
63.271202	2053.568390	20.134643
63.117442	2059.433167	20.139661
63.227260	2057.680135	20.144679
63.246899	2056.676095	20.149696
63.095491	2067.547497	20.154714
62.951001	2065.488949	20.159731
63.063406	2070.834652	20.164749
63.144892	2069.161643	20.169767
63.160225	2082.026255	20.174784
62.970393	2076.440302	20.179802
63.545363	2098.307887	20.184819
63.403274	2097.507390	20.189837
63.662567	2099.425605	20.194855
64.002289	2098.230517	20.199872
63.910659	2096.876125	20.204890
64.204667	2101.288377	20.209907
64.031715	2101.952590	20.214925
64.052617	2088.017897	20.219943
64.304995	2093.070723	20.224960
64.115523	2094.281844	20.229978
64.100566	2084.486842	20.234995
64.248575	2092.200602	20.240013
64.078892	2094.033067	20.245031
63.926712	2093.830364	20.250048
63.862503	2097.450294	20.255066
63.968707	2099.949781	20.260083
64.266246	2121.046805	20.265101
64.525983	2111.277193	20.270119
64.526000	2119.192323	20.275136
64.484342	2122.920350	20.280154
64.808457	2136.807016	20.285171
64.752615	2135.092977	20.290189
64.993596	2145.173540	20.295207
65.405845	2143.049793	20.300224
65.209614	2143.481762	20.305242
65.306850	2151.002300	20.310259
65.785451	2148.732688	20.315277
65.719051	2131.184416	20.320295
65.514616	2122.009498	20.325312
65.353797	2109.186023	20.330330
65.666101	2105.468990	20.335347
65.522067	2117.405781	20.340365
65.403053	2102.450454	20.345383
65.108034	2109.328798	20.350400
65.196186	2133.059480	20.355418
65.597542	2135.200441	20.360435
65.650300	2135.433825	20.365453
66.022980	2140.624789	20.370471
65.930919	2130.127886	20.375488
66.294238	2132.364577	20.380506
66.434045	2129.249210	20.385523
66.222200	2137.421509	20.390541
65.900976	2130.135569	20.395559
65.631603	2136.103758	20.400576
65.951266	2138.377300	20.405594
66.379526	2152.398386	20.410611
66.690279	2158.381040	20.415629
66.600968	2154.734333	20.420647
66.796720	2159.896888	20.425664
66.761317	2170.060870	20.430682
66.931599	2166.069163	20.435699
66.756247	2156.899024	20.440717
66.929272	2149.974712	20.445735
67.069300	2151.422734	20.450752
66.528046	2161.661085	20.455770
67.038787	2149.877237	20.460787
67.041005	2155.682571	20.465805
66.951198	2155.235535	20.470823
67.262056	2151.267034	20.475840
67.132928	2151.634818	20.480858
66.972128	2154.692855	20.485875
66.943219	2155.017916	20.490893
67.174765	2173.281458	20.495911
67.395261	2174.007202	20.500928
67.231607	2181.390032	20.505946
67.659716	2179.732522	20.510963
67.685348	2181.892508	20.515981
67.450290	2181.158742	20.520999
67.822759	2181.781598	20.526016
67.772047	2175.965778	20.531034
67.841817	2203.067419	20.536051
68.393842	2207.092486	20.541069
68.303303	2200.406812	20.546087
68.525862	2195.563602	20.551104
68.089144	2195.536835	20.556122
68.555078	2196.561649	20.561139
68.548001	2199.310458	20.566157
68.492547	2197.006452	20.571175
68.668355	2198.112139	20.576192
68.508667	2206.828302	20.581210
68.767026	2194.263529	20.586227
68.715941	2202.479442	20.591245
68.904675	2206.037040	20.596263
68.957370	2195.350261	20.601280
68.906330	2201.049274	20.606298
69.214997	2202.855808	20.611315
68.973455	2205.822910	20.616333
68.889651	2203.624100	20.621351
69.493467	2195.293969	20.626368
69.227913	2205.258718	20.631386
69.043610	2197.401912	20.636403
68.967816	2194.084955	20.641421
69.107673	2204.365733	20.646439
69.005453	2192.119590	20.651456
68.897224	2211.013103	20.656474
69.178784	2220.835559	20.661491
69.624867	2233.579703	20.666509
69.130987	2233.234855	20.671527
69.007175	2237.787713	20.676544
69.609128	2249.421601	20.681562
69.907902	2258.874814	20.686579
70.173510	2253.694376	20.691597
70.312622	2267.555613	20.696615
70.369036	2257.355846	20.701632
70.259603	2268.277335	20.706650
70.018480	2266.932608	20.711667
70.494462	2253.968128	20.716685
70.271477	2253.300075	20.721703
70.434405	2243.317719	20.726720
70.678793	2242.133104	20.731738
70.766767	2246.553088	20.736755
70.712450	2241.300973	20.741773
70.821823	2242.679959	20.746791
70.992206	2243.442014	20.751808
70.471743	2251.534599	20.756826
70.638769	2241.466646	20.761843
70.825317	2248.340621	20.766861
70.962358	2276.358206	20.771879
70.911275	2267.430882	20.776896
71.054740	2267.350921	20.781914
71.400791	2266.392345	20.786931
71.431466	2269.481221	20.791949
71.301954	2271.648657	20.796967
71.574458	2260.922058	20.801984
71.534898	2276.159914	20.807002
71.503548	2272.835851	20.812019
71.703166	2270.928471	20.817037
71.500199	2269.308665	20.822055
71.717688	2286.846263	20.827072
71.777100	2295.365514	20.832090
72.045768	2289.229723	20.837107
72.161350	2302.015620	20.842125
71.719140	2298.049189	20.847143
72.085244	2296.091661	20.852160
72.210306	2294.515499	20.857178
72.268628	2297.341990	20.862195
72.637430	2298.645004	20.867213
72.184987	2290.591799	20.872231
72.432157	2282.749514	20.877248
72.734521	2306.362947	20.882266
72.537459	2311.709325	20.887283
72.895751	2313.021881	20.892301
72.653930	2324.970502	20.897319
73.110847	2315.196840	20.902336
72.655289	2316.757159	20.907354
72.810945	2322.695399	20.912371
73.012537	2319.024284	20.917389
73.213186	2319.232515	20.922407
73.238360	2314.741648	20.927424
73.497556	2309.492998	20.932442
73.475783	2303.902179	20.937459
73.650642	2308.904521	20.942477
73.292344	2323.480653	20.947495
73.616921	2315.890282	20.952512
73.442106	2313.237193	20.957530
73.526869	2310.283154	20.962547
73.938866	2306.136457	20.967565
73.733732	2310.242969	20.972583
74.115627	2323.546431	20.977600
73.822414	2330.105256	20.982618
73.864044	2338.635234	20.987635
74.099115	2340.558132	20.992653
74.292525	2344.391093	20.997671
74.484981	2334.976565	21.002688
74.770902	2335.764247	21.007706
74.482174	2335.525896	21.012723
74.834077	2334.284017	21.017741
74.593763	2337.821974	21.022759
74.758685	2335.846184	21.027776
74.516082	2342.853135	21.032794
74.772939	2332.582025	21.037811
74.772583	2328.821198	21.042829
74.639049	2337.076291	21.047847
75.095135	2329.797646	21.052864
75.107791	2330.807448	21.057882
74.911423	2333.871194	21.062899
74.920373	2329.477294	21.067917
75.009160	2327.773990	21.072935
75.326367	2341.151494	21.077952
75.071602	2353.114787	21.082970
75.105679	2347.378974	21.087987
75.479219	2347.638289	21.093005
75.375606	2350.960963	21.098023
75.526469	2353.147410	21.103040
75.644201	2350.439797	21.108058
75.789989	2359.092394	21.113075
75.757247	2372.567418	21.118093
75.733079	2384.071593	21.123111
75.978607	2375.053644	21.128128
75.989199	2365.723154	21.133146
76.231532	2375.014765	21.138163
76.180799	2375.347243	21.143181
76.003409	2375.366426	21.148199
75.890831	2377.578369	21.153216
76.210815	2405.116344	21.158234
76.393712	2397.948086	21.163251
76.504563	2393.422296	21.168269
76.501296	2397.745188	21.173287
76.509834	2398.872059	21.178304
76.883790	2409.526227	21.183322
76.825440	2403.035108	21.188339
76.750197	2431.932377	21.193357
76.893655	2424.528140	21.198375
77.073729	2415.515885	21.203392
77.322526	2429.709797	21.208410
77.193912	2420.712155	21.213427
77.047614	2410.349544	21.218445
77.187158	2435.810782	21.223463
77.413524	2412.979472	21.228480
77.415856	2419.837286	21.233498
77.503230	2453.334316	21.238515
77.804350	2439.673150	21.243533
77.920824	2440.099307	21.248551
77.795280	2437.467440	21.253568
78.114942	2445.912245	21.258586
77.847441	2444.107647	21.263603
77.869958	2435.074097	21.268621
78.077920	2438.905551	21.273639
77.952746	2435.713607	21.278656
78.274080	2440.401617	21.283674
78.199136	2452.928582	21.288691
78.586090	2461.038609	21.293709
77.758075	2484.514038	21.298727
78.619954	2479.485412	21.303744
78.580992	2471.775959	21.308762
78.598881	2477.100705	21.313779
78.820505	2476.150160	21.318797
78.852530	2478.421646	21.323815
78.857541	2493.463851	21.328832
78.845694	2498.542438	21.333850
78.985604	2501.414949	21.338867
79.511356	2496.350252	21.343885
79.427063	2499.779208	21.348903
79.141599	2498.251185	21.353920
79.419580	2500.065798	21.358938
79.462777	2506.224976	21.363955
79.510939	2492.618257	21.368973
79.496695	2492.757721	21.373991
79.655749	2516.823804	21.379008
80.118590	2523.825319	21.384026
79.953731	2528.111094	21.389043
80.668013	2521.453456	21.394061
80.178351	2520.773642	21.399079
80.092223	2528.206420	21.404096
80.377556	2525.006414	21.409114
80.442128	2535.510228	21.414131
80.173907	2512.750552	21.419149
80.524346	2521.099253	21.424167
80.377613	2515.061858	21.429184
80.870276	2509.941869	21.434202
80.701753	2509.982447	21.439219
81.390157	2509.481306	21.444237
81.020933	2516.092448	21.449255
81.211256	2511.151237	21.454272
81.264226	2504.952220	21.459290
81.237887	2513.622919	21.464307
81.469783	2502.013036	21.469325
81.445592	2511.101047	21.474343
81.310398	2503.496589	21.479360
81.226506	2496.521057	21.484378
81.082886	2506.580615	21.489395
81.326695	2502.632151	21.494413
81.358268	2509.262752	21.499431
81.276786	2518.226190	21.504448
81.473537	2521.911583	21.509466
81.376939	2534.186443	21.514483
81.430563	2530.670225	21.519501
81.732145	2534.690491	21.524519
82.145449	2528.603899	21.529536
82.038588	2549.082525	21.534554
82.148710	2555.465443	21.539571
82.500196	2558.563002	21.544589
82.668282	2557.931676	21.549607
82.653356	2556.656249	21.554624
82.863216	2556.398951	21.559642
82.594025	2549.792730	21.564659
82.868120	2552.610819	21.569677
82.572986	2560.824951	21.574695
82.936233	2549.777704	21.579712
83.129738	2547.364726	21.584730
82.818755	2556.329390	21.589747
83.157651	2549.118878	21.594765
82.949872	2554.761221	21.599783
82.730692	2549.517980	21.604800
82.918970	2566.045141	21.609818
83.207162	2581.787143	21.614835
83.208919	2580.945588	21.619853
82.962410	2592.621456	21.624871
83.214616	2596.769955	21.629888
83.452693	2602.738428	21.634906
83.164522	2615.092671	21.639923
83.556378	2604.779393	21.644941
84.104358	2628.509137	21.649959
84.413929	2636.350016	21.654976
84.508394	2630.951333	21.659994
84.554898	2637.000708	21.665011
84.621471	2621.213754	21.670029
84.597688	2606.419696	21.675047
84.475268	2606.391572	21.680064
84.849051	2618.569473	21.685082
84.783211	2625.868498	21.690099
84.842742	2619.527594	21.695117
84.889484	2622.766575	21.700135
84.845943	2634.237069	21.705152
85.342973	2621.301158	21.710170
85.108285	2630.977329	21.715187
85.427543	2631.492285	21.720205
85.030252	2631.634627	21.725223
85.034143	2625.110673	21.730240
85.245218	2624.243604	21.735258
84.988136	2633.567826	21.740275
85.273187	2627.139044	21.745293
85.536718	2648.419234	21.750311
85.409991	2652.467718	21.755328
85.749413	2645.695973	21.760346
85.811878	2655.725131	21.765363
85.640643	2648.845255	21.770381
85.768267	2644.632907	21.775399
85.947373	2653.023164	21.780416
86.235794	2665.981607	21.785434
85.983260	2678.205946	21.790451
86.027078	2685.876860	21.795469
86.583050	2674.248985	21.800487
86.310537	2675.113937	21.805504
86.536702	2678.323533	21.810522
86.768451	2676.746837	21.815539
86.787271	2675.766482	21.820557
86.687136	2661.561088	21.825575
86.530462	2676.696908	21.830592
87.027391	2684.739972	21.835610
87.002236	2702.635322	21.840627
87.075899	2701.820049	21.845645
87.328844	2695.066003	21.850663
87.202403	2697.453247	21.855680
87.584096	2700.109482	21.860698
87.485005	2701.461976	21.865715
87.567293	2704.721263	21.870733
87.363708	2696.652530	21.875751
87.565789	2714.315806	21.880768
87.999935	2703.618954	21.885786
87.810609	2711.901246	21.890803
87.783348	2720.742898	21.895821
88.060171	2720.668414	21.900839
87.499235	2728.755913	21.905856
88.108842	2725.257963	21.910874
88.583590	2746.102686	21.915891
88.914033	2737.031646	21.920909
88.787342	2745.916698	21.925927
88.603841	2750.269221	21.930944
89.010811	2732.999476	21.935962
88.691738	2738.281302	21.940979
88.939622	2744.098824	21.945997
88.973069	2728.303665	21.951015
88.693971	2735.464495	21.956032
88.959323	2734.406283	21.961050
88.966337	2753.763497	21.966067
89.166101	2756.575388	21.971085
89.099748	2765.873213	21.976103
89.134344	2772.825155	21.981120
89.251465	2763.714965	21.986138
89.215138	2781.395888	21.991155
89.194900	2810.206480	21.996173
89.891147	2792.996722	22.001191
89.850410	2791.645161	22.006208
90.137752	2795.230443	22.011226
90.205945	2801.481721	22.016243
90.380399	2793.667276	22.021261
90.733979	2792.403070	22.026279
90.560890	2789.546684	22.031296
90.451562	2799.061395	22.036314
90.346547	2795.918856	22.041331
90.439159	2789.659911	22.046349
90.840942	2802.298360	22.051367
90.774978	2811.006230	22.056384
91.045606	2809.308483	22.061402
91.211979	2823.534803	22.066419
91.374205	2819.555217	22.071437
91.584601	2808.713059	22.076455
90.970827	2796.427633	22.081472
91.528025	2803.792576	22.086490
91.453866	2818.793469	22.091507
91.284311	2805.684460	22.096525
91.696056	2794.661545	22.101543
91.587214	2793.642547	22.106560
91.728786	2797.693122	22.111578
91.588959	2799.538216	22.116595
91.693493	2792.361811	22.121613
91.997885	2804.405420	22.126631
91.833447	2826.398310	22.131648
92.144864	2832.698126	22.136666
92.163677	2832.953453	22.141683
92.205722	2831.070342	22.146701
92.309549	2831.086368	22.151719
92.352117	2841.881009	22.156736
92.570569	2833.527809	22.161754
92.346381	2855.439029	22.166771
92.569582	2859.482111	22.171789
92.862679	2854.359218	22.176807
92.685254	2856.844286	22.181824
92.953734	2862.081233	22.186842
93.237705	2862.214049	22.191859
93.186142	2880.937362	22.196877
93.764599	2879.371432	22.201895
93.433078	2890.026757	22.206912
93.563110	2885.850139	22.211930
93.517251	2882.462179	22.216947
93.897042	2885.578894	22.221965
93.837187	2885.027950	22.226983
93.686567	2893.427663	22.232000
93.965425	2880.494852	22.237018
93.846680	2882.231981	22.242035
93.957768	2905.535523	22.247053
93.912266	2912.625368	22.252071
94.186468	2912.870648	22.257088
94.479742	2907.484209	22.262106
94.429600	2904.461107	22.267123
94.282102	2910.578500	22.272141
94.761549	2924.340476	22.277159
94.612481	2935.286088	22.282176
95.198393	2931.006874	22.287194
95.026065	2939.233096	22.292211
94.804278	2941.580523	22.297229
94.950349	2936.371714	22.302247
95.182968	2935.949536	22.307264
95.344235	2935.879320	22.312282
95.329932	2936.107681	22.317299
95.398871	2948.579093	22.322317
95.978153	2954.352509	22.327335
95.739976	2959.488583	22.332352
96.236312	2956.242255	22.337370
96.017376	2955.491716	22.342387
96.044668	2950.248355	22.347405
96.279259	2939.494270	22.352423
96.086640	2945.400206	22.357440
96.309962	2954.170580	22.362458
96.289878	2944.788765	22.367475
96.195836	2944.604305	22.372493
96.429427	2946.385941	22.377511
96.304862	2963.060974	22.382528
96.823166	2960.818738	22.387546
96.879149	2980.678930	22.392563
96.577294	2973.312388	22.397581
96.927893	2974.142496	22.402599
97.039601	2974.469535	22.407616
97.320473	2969.516879	22.412634
97.200495	2966.994934	22.417651
97.205598	2974.554188	22.422669
97.891836	2977.474183	22.427687
97.568475	2990.444733	22.432704
97.692578	2995.258765	22.437722
97.847246	2991.723177	22.442739
98.026997	2991.816768	22.447757
98.219820	2981.902293	22.452775
98.149202	2991.532874	22.457792
98.038130	2997.557186	22.462810
97.846422	2993.508138	22.467827
97.679598	2989.716265	22.472845
98.509292	3006.721355	22.477863
98.548220	3016.910257	22.482880
98.858901	3024.351593	22.487898
98.709393	3021.261721	22.492915
98.740701	3025.853014	22.497933
99.031270	3027.030924	22.502951
98.854654	3022.154345	22.507968
98.889156	3019.456736	22.512986
99.141146	3030.106428	22.518003
99.334642	3046.114166	22.523021
99.414742	3042.904300	22.528039
99.210891	3047.454439	22.533056
99.343139	3044.828549	22.538074
99.714969	3044.116736	22.543091
99.404463	3052.296623	22.548109
99.506858	3064.288494	22.553127
99.978897	3068.488601	22.558144
100.347799	3072.215117	22.563162
100.610967	3073.280988	22.568179
100.388047	3081.003295	22.573197
100.544935	3071.660038	22.578215
100.552636	3064.263754	22.583232
100.652461	3069.129663	22.588250
100.852382	3058.263033	22.593267
100.454223	3062.096127	22.598285
100.541965	3060.779114	22.603303
100.522448	3065.230647	22.608320
100.777924	3082.848889	22.613338
101.148411	3085.403156	22.618355
100.974221	3093.990801	22.623373
101.051390	3086.651861	22.628391
101.224323	3092.184149	22.633408
101.128589	3105.580226	22.638426
101.389910	3105.772505	22.643443
101.383815	3116.829959	22.648461
101.737077	3113.644954	22.653479
102.028570	3122.006550	22.658496
102.101877	3108.273328	22.663514
102.105277	3113.516453	22.668531
101.874183	3137.293387	22.673549
102.057055	3138.790527	22.678567
102.302560	3132.336368	22.683584
102.270597	3136.052882	22.688602
102.446961	3137.614773	22.693619
102.232131	3153.893035	22.698637
102.674557	3165.015873	22.703655
102.784821	3161.415747	22.708672
103.090395	3170.486982	22.713690
103.535374	3164.275520	22.718707
103.167663	3166.046875	22.723725
103.347667	3165.769947	22.728743
103.485899	3171.228354	22.733760
103.321544	3171.031505	22.738778
103.519070	3187.067859	22.743795
103.697812	3193.600579	22.748813
104.142031	3179.971756	22.753831
104.011822	3195.390209	22.758848
104.123806	3190.410921	22.763866
104.292630	3191.155186	22.768883
103.739672	3194.393956	22.773901
103.885803	3184.211486	22.778919
104.150922	3209.271775	22.783936
104.222774	3218.564369	22.788954
104.676003	3208.431237	22.793971
104.987870	3212.873238	22.798989
105.458966	3198.940422	22.804007
105.327044	3201.032866	22.809024
105.480278	3202.133581	22.814042
105.475323	3201.665901	22.819059
105.629549	3197.590739	22.824077
105.724210	3205.389899	22.829095
105.819868	3192.084081	22.834112
105.764153	3193.823782	22.839130
105.885758	3195.088429	22.844147
105.632323	3195.149625	22.849165
105.627955	3185.220834	22.854183
105.738995	3195.145083	22.859200
105.553206	3199.254262	22.864218
106.051859	3198.677964	22.869235
105.840770	3221.526037	22.874253
105.922786	3215.420411	22.879271
106.369980	3221.787632	22.884288
105.963649	3225.729046	22.889306
106.557272	3241.687356	22.894323
106.668303	3236.931595	22.899341
106.986012	3254.573945	22.904359
107.018985	3248.074180	22.909376
107.057521	3250.290475	22.914394
107.327414	3246.085947	22.919411
106.922809	3257.205478	22.924429
107.061909	3251.557967	22.929447
107.275386	3256.904512	22.934464
106.826954	3279.320141	22.939482
107.224827	3284.494135	22.944499
107.407722	3293.316783	22.949517
107.616641	3305.571894	22.954535
107.617529	3312.172357	22.959552
107.731105	3315.806716	22.964570
108.042457	3310.020021	22.969587
108.289275	3332.208457	22.974605
108.228938	3337.276190	22.979623
108.341510	3330.187911	22.984640
108.442475	3335.786830	22.989658
109.114878	3340.168235	22.994675
109.066008	3337.658484	22.999693
109.145241	3339.445904	23.004711
109.249470	3347.448915	23.009728
109.539327	3363.214312	23.014746
109.682458	3347.788784	23.019763
109.702473	3357.250197	23.024781
109.857991	3346.325934	23.029799
110.184046	3339.088769	23.034816
109.666655	3337.384467	23.039834
110.013097	3348.242725	23.044851
109.986357	3347.717947	23.049869
109.845067	3349.301407	23.054887
110.022935	3354.724459	23.059904
109.876168	3351.135380	23.064922
110.228653	3339.367953	23.069939
110.188216	3351.022578	23.074957
110.555626	3368.078210	23.079975
110.801508	3370.875004	23.084992
110.365677	3375.404025	23.090010
110.813770	3366.962779	23.095027
110.884755	3380.023392	23.100045
110.866479	3396.065282	23.105063
111.035309	3401.713973	23.110080
110.888157	3410.953511	23.115098
111.369264	3400.254961	23.120115
111.341257	3410.221980	23.125133
111.442901	3430.716578	23.130151
112.375772	3431.147100	23.135168
111.874063	3432.610267	23.140186
112.167636	3429.282900	23.145203
111.873626	3424.670321	23.150221
112.235932	3428.648121	23.155239
112.805642	3420.875723	23.160256
112.442058	3428.600190	23.165274
112.556539	3424.747617	23.170291
112.434812	3423.628370	23.175309
112.165307	3417.401725	23.180327
112.696910	3418.379199	23.185344
112.646479	3447.624559	23.190362
113.118633	3444.378837	23.195379
113.065570	3451.893338	23.200397
113.369929	3449.373655	23.205415
113.234549	3445.671040	23.210432
112.848933	3462.282076	23.215450
113.354141	3451.820344	23.220467
113.581952	3472.206785	23.225485
113.618509	3467.627223	23.230503
113.710855	3471.595378	23.235520
113.667104	3476.024156	23.240538
113.842165	3490.606860	23.245555
114.001963	3498.924386	23.250573
114.183027	3492.165706	23.255591
114.442179	3495.687227	23.260608
114.548751	3508.719470	23.265626
114.926901	3513.197404	23.270643
115.207329	3502.853284	23.275661
115.299911	3512.590336	23.280679
115.426530	3508.720860	23.285696
115.259808	3515.762678	23.290714
115.457501	3500.957569	23.295731
115.463787	3504.277925	23.300749
115.352665	3509.131206	23.305767
115.660848	3513.074397	23.310784
115.369466	3517.937545	23.315802
116.000134	3499.882388	23.320819
115.938140	3513.579446	23.325837
115.969393	3531.734262	23.330855
116.026653	3539.877804	23.335872
115.892305	3541.954950	23.340890
116.096627	3542.827297	23.345907
116.302967	3551.662882	23.350925
116.602372	3556.661532	23.355943
116.977183	3557.634912	23.360960
116.465696	3564.089071	23.365978
116.694509	3567.045946	23.370995
116.917666	3563.875299	23.376013
117.001129	3588.656072	23.381031
117.454828	3592.576869	23.386048
117.094064	3604.580894	23.391066
117.441489	3580.915110	23.396083
117.429562	3597.134767	23.401101
117.380886	3610.247704	23.406119
117.566243	3604.340968	23.411136
117.473023	3613.911062	23.416154
117.635590	3621.713777	23.421171
117.978131	3622.596341	23.426189
117.946619	3653.793026	23.431207
118.095681	3644.093533	23.436224
118.377975	3645.629937	23.441242
118.628913	3651.812326	23.446259
118.883394	3650.176843	23.451277
119.029913	3666.376820	23.456295
119.148849	3669.255269	23.461312
118.940500	3668.325228	23.466330
119.272878	3673.589254	23.471347
119.358366	3668.359168	23.476365
119.193335	3666.705620	23.481383
119.406167	3668.164215	23.486400
119.577940	3685.293104	23.491418
119.787600	3691.558392	23.496435
120.150555	3697.038589	23.501453
119.830396	3692.823398	23.506471
120.369353	3679.035059	23.511488
120.323707	3687.555358	23.516506
120.285047	3696.513477	23.521523
120.730594	3698.108024	23.526541
120.756795	3712.896393	23.531559
120.984908	3713.252087	23.536576
120.692024	3724.048164	23.541594
120.945502	3711.690536	23.546611
120.826277	3707.993144	23.551629
120.896222	3716.517054	23.556647
121.311976	3733.861174	23.561664
121.085458	3745.755808	23.566682
121.377358	3748.671984	23.571699
121.874211	3743.571361	23.576717
121.574951	3749.327073	23.581735
122.082040	3755.664530	23.586752
121.992576	3765.662828	23.591770
122.106214	3769.224923	23.596787
122.497654	3781.770699	23.601805
122.311019	3782.226350	23.606823
122.797997	3766.372701	23.611840
122.412612	3777.691718	23.616858
122.436309	3788.925853	23.621875
122.749264	3800.362446	23.626893
122.865731	3802.088136	23.631911
123.082964	3791.989875	23.636928
123.058049	3811.965570	23.641946
123.134494	3822.890832	23.646963
123.656097	3825.617795	23.651981
123.597959	3833.468400	23.656999
124.158233	3819.248612	23.662016
124.197931	3825.837612	23.667034
124.254726	3828.567892	23.672051
124.012860	3829.417006	23.677069
123.568450	3832.177643	23.682087
124.279332	3843.296745	23.687104
124.748758	3849.150973	23.692122
124.686610	3845.928215	23.697139
124.947113	3848.660629	23.702157
124.692019	3859.750481	23.707175
124.923893	3854.418327	23.712192
125.429168	3847.601498	23.717210
125.128613	3852.858740	23.722227
125.191299	3850.338193	23.727245
125.290975	3849.338575	23.732263
125.129792	3855.316951	23.737280
125.434144	3867.549453	23.742298
125.524952	3867.738256	23.747315
125.713360	3852.328577	23.752333
125.625866	3875.260223	23.757351
125.929789	3888.145705	23.762368
126.037162	3893.856304	23.767386
126.215920	3889.393956	23.772403
126.319892	3891.684870	23.777421
126.348479	3907.759967	23.782439
127.055076	3904.574309	23.787456
126.851906	3909.250463	23.792474
127.261184	3909.489963	23.797491
127.457408	3904.288548	23.802509
127.216687	3913.190915	23.807527
127.485859	3911.370566	23.812544
127.625029	3921.574009	23.817562
127.693668	3933.306887	23.822579
128.029875	3940.154659	23.827597
128.125863	3941.071050	23.832615
128.267576	3942.523708	23.837632
127.970762	3929.854033	23.842650
128.061447	3936.356291	23.847667
128.164700	3939.737587	23.852685
128.414546	3959.853745	23.857703
128.457739	3959.923495	23.862720
128.469902	3960.466234	23.867738
128.552263	3969.782803	23.872755
129.037557	3996.936377	23.877773
129.413278	3989.238666	23.882791
129.390376	3985.341775	23.887808
129.310156	3987.452043	23.892826
129.203578	3997.651458	23.897843
129.838448	3989.254808	23.902861
129.780731	4009.937673	23.907879
130.096868	4019.030570	23.912896
129.827619	4016.032732	23.917914
130.039107	4013.430222	23.922931
129.980932	4017.657727	23.927949
130.044936	4029.068117	23.932967
130.489136	4042.553593	23.937984
130.404136	4040.880161	23.943002
130.610342	4049.957566	23.948019
130.757271	4060.660165	23.953037
131.163121	4062.438077	23.958055
131.158768	4058.608218	23.963072
131.581292	4064.522717	23.968090
131.518365	4073.499881	23.973107
131.955976	4071.254623	23.978125
131.890993	4069.873769	23.983143
131.968890	4071.258738	23.988160
131.939180	4064.203018	23.993178
131.960493	4066.804485	23.998195
132.127414	4060.692050	24.003213
131.936854	4070.747579	24.008231
132.291496	4077.852066	24.013248
132.485099	4093.780702	24.018266
132.340811	4105.993688	24.023283
132.541703	4098.630582	24.028301
132.996928	4118.699267	24.033319
133.024307	4129.258145	24.038336
133.031372	4127.726564	24.043354
133.175121	4137.127062	24.048371
133.361679	4129.435840	24.053389
133.289458	4142.693814	24.058407
133.720588	4155.177734	24.063424
133.838406	4153.648158	24.068442
133.891617	4159.365923	24.073459
134.012932	4157.437752	24.078477
134.250223	4173.320964	24.083495
134.378996	4182.141768	24.088512
134.386215	4187.726856	24.093530
134.449965	4186.050143	24.098547
134.798114	4185.856520	24.103565
134.714897	4202.299819	24.108583
134.770320	4213.241312	24.113600
135.291061	4201.425920	24.118618
135.111714	4215.307537	24.123635
135.484362	4212.293845	24.128653
135.689498	4227.905347	24.133671
135.853015	4223.282494	24.138688
135.959432	4228.005358	24.143706
136.234915	4232.575406	24.148723
136.570668	4225.446392	24.153741
136.433391	4229.479684	24.158759
136.319452	4234.900821	24.163776
136.641651	4222.585299	24.168794
136.677235	4256.237895	24.173811
136.924387	4260.863600	24.178829
137.259855	4255.394429	24.183847
137.196525	4255.179882	24.188864
137.205905	4252.589888	24.193882
137.031738	4262.294452	24.198899
137.396901	4257.156442	24.203917
137.910742	4263.160300	24.208935
137.735950	4267.685727	24.213952
137.931925	4256.761418	24.218970
137.967621	4253.497010	24.223987
138.167443	4264.916609	24.229005
137.772533	4274.673683	24.234023
138.027440	4283.476011	24.239040
138.166933	4298.109245	24.244058
138.390370	4301.922997	24.249075
138.600720	4292.492563	24.254093
138.702983	4316.987595	24.259111
138.893302	4323.209829	24.264128
139.103346	4326.493951	24.269146
139.141727	4324.061369	24.274163
139.690459	4320.084261	24.279181
139.541558	4350.299749	24.284199
139.539824	4349.851185	24.289216
139.760552	4344.298798	24.294234
139.717525	4352.517781	24.299251
139.883703	4338.970766	24.304269
140.342671	4359.535560	24.309287
139.900873	4366.826956	24.314304
140.522700	4359.900847	24.319322
140.980728	4367.192734	24.324339
140.632014	4377.988749	24.329357
140.926461	4386.914633	24.334375
140.952857	4394.068463	24.339392
141.257249	4396.501352	24.344410
141.094657	4403.360433	24.349427
141.687787	4408.074194	24.354445
141.722226	4417.741669	24.359463
142.067016	4426.340957	24.364480
142.153907	4419.010027	24.369498
142.087373	4417.520043	24.374515
142.118002	4421.934888	24.379533
142.246289	4425.379958	24.384551
142.494292	4439.757679	24.389568
142.566100	4443.029255	24.394586
142.356039	4454.434114	24.399603
142.744829	4452.718921	24.404621
142.935208	4462.533838	24.409639
142.891778	4482.386748	24.414656
143.232031	4472.142543	24.419674
143.127640	4480.237650	24.424691
143.278574	4491.019378	24.429709
143.691966	4512.057352	24.434727
143.767005	4517.784363	24.439744
144.342603	4511.107058	24.444762
144.131915	4533.257774	24.449779
144.285001	4533.431151	24.454797
144.393363	4542.570089	24.459815
144.345114	4545.223638	24.464832
145.006271	4533.864669	24.469850
144.777178	4554.500106	24.474867
145.358327	4551.668647	24.479885
145.351724	4564.723024	24.484903
145.874209	4562.580588	24.489920
145.436073	4560.619629	24.494938
145.324859	4555.773798	24.499955
146.026505	4556.577146	24.504973
146.042223	4560.310806	24.509991
146.039229	4578.920775	24.515008
146.479206	4582.968327	24.520026
146.173642	4576.139632	24.525043
146.222158	4580.404567	24.530061
146.548215	4579.433314	24.535079
146.610853	4583.126459	24.540096
147.050887	4583.416139	24.545114
146.847571	4607.865978	24.550131
147.252521	4602.513041	24.555149
147.206642	4606.475224	24.560167
147.416744	4604.793224	24.565184
147.176900	4602.510367	24.570202
147.304515	4620.456865	24.575219
147.406617	4635.408702	24.580237
147.503550	4644.717085	24.585255
147.788946	4661.257101	24.590272
148.609566	4665.572027	24.595290
148.287208	4667.029521	24.600307
148.268434	4671.574250	24.605325
148.729160	4677.272086	24.610343
148.509302	4685.129262	24.615360
148.852026	4689.539269	24.620378
149.066147	4698.923402	24.625395
149.384542	4705.895524	24.630413
149.585748	4715.248687	24.635431
149.606267	4712.933742	24.640448
149.933750	4709.814659	24.645466
149.951309	4713.210585	24.650483
149.818229	4729.238411	24.655501
150.323152	4729.232190	24.660519
150.320096	4727.112161	24.665536
150.553997	4732.254610	24.670554
150.667064	4745.298720	24.675571
150.889553	4753.032702	24.680589
151.120757	4756.138908	24.685607
150.996533	4764.873747	24.690624
151.552632	4758.388243	24.695642
151.289439	4758.395138	24.700659
151.323651	4772.085898	24.705677
151.347593	4784.187665	24.710695
151.707724	4792.861818	24.715712
152.103599	4787.806837	24.720730
152.085383	4813.556190	24.725747
152.555606	4813.461102	24.730765
152.727611	4811.936193	24.735783
152.515088	4818.471452	24.740800
152.688928	4814.166945	24.745818
152.663975	4817.046537	24.750835
152.837269	4839.296973	24.755853
153.172356	4832.019095	24.760871
153.087579	4844.686555	24.765888
153.585409	4862.797740	24.770906
153.980243	4875.255026	24.775923
154.136832	4868.914983	24.780941
154.558466	4859.145273	24.785959
154.415138	4872.316908	24.790976
154.551132	4866.555207	24.795994
154.696547	4873.470027	24.801011
154.477844	4875.888063	24.806029
154.672478	4863.359492	24.811047
154.546193	4870.310548	24.816064
154.885321	4881.418923	24.821082
154.851590	4900.049146	24.826099
155.181770	4892.864062	24.831117
155.241564	4899.648584	24.836135
155.168733	4900.338643	24.841152
155.448725	4910.392884	24.846170
155.421115	4919.747258	24.851187
155.467805	4948.838526	24.856205
156.035252	4953.366974	24.861223
156.187553	4953.526323	24.866240
156.461383	4955.769085	24.871258
156.439559	4980.859284	24.876275
156.840410	4981.763325	24.881293
156.991227	4984.174387	24.886311
156.828385	4987.706912	24.891328
157.235016	4992.106036	24.896346
157.324071	5009.687845	24.901363
157.283041	5018.548813	24.906381
157.885401	5014.297078	24.911399
158.017567	5032.716150	24.916416
158.373297	5041.963071	24.921434
158.518201	5048.433580	24.926451
158.621937	5035.198754	24.931469
158.804785	5024.607949	24.936487
158.414065	5038.946489	24.941504
158.718810	5033.559814	24.946522
158.865429	5037.433208	24.951539
158.723340	5056.073037	24.956557
159.019542	5062.406149	24.961575
158.962726	5082.933044	24.966592
159.391658	5090.309391	24.971610
159.326783	5098.544073	24.976627
159.906369	5107.983486	24.981645
160.260671	5103.474694	24.986663
160.141517	5119.216730	24.991680
160.082072	5114.322339	24.996698
160.683221	5122.951185	25.001715
160.554710	5133.266592	25.006733
160.994829	5133.501993	25.011751
161.038457	5132.931317	25.016768
161.234553	5143.930532	25.021786
161.691208	5168.121105	25.026803
161.634959	5157.157672	25.031821
161.982863	5163.575414	25.036839
161.876715	5158.383219	25.041856
162.229470	5158.676604	25.046874
162.270742	5166.577367	25.051891
162.026334	5198.122805	25.056909
162.467722	5200.117832	25.061927
162.538535	5197.564293	25.066944
162.743778	5200.832859	25.071962
162.802826	5209.980076	25.076979
162.846559	5219.053431	25.081997
163.152260	5222.034578	25.087015
163.093959	5228.883708	25.092032
163.261825	5234.877050	25.097050
163.864358	5245.108241	25.102067
163.898562	5252.692353	25.107085
164.089540	5251.848798	25.112103
163.952867	5257.373844	25.117120
164.164199	5266.122351	25.122138
164.318988	5284.581401	25.127155
164.436375	5280.073351	25.132173
164.807991	5275.080289	25.137191
164.866735	5298.166273	25.142208
165.023538	5304.999239	25.147226
165.479240	5306.151808	25.152243
165.430638	5315.454712	25.157261
165.623705	5316.351781	25.162279
165.808450	5317.604978	25.167296
166.254818	5325.552954	25.172314
166.283009	5325.096443	25.177331
166.421464	5325.424784	25.182349
166.719749	5331.081121	25.187367
166.812699	5343.998379	25.192384
166.990695	5342.003590	25.197402
167.310010	5339.076848	25.202419
167.405822	5346.432484	25.207437
167.531425	5346.633857	25.212455
167.577160	5342.874348	25.217472
167.688550	5348.683213	25.222490
167.802201	5365.768267	25.227507
167.776449	5366.179430	25.232525
168.190257	5368.335432	25.237543
168.360046	5377.553996	25.242560
168.351089	5391.725022	25.247578
168.645265	5404.838397	25.252595
168.539221	5416.633352	25.257613
168.896321	5421.399241	25.262631
168.749906	5431.874265	25.267648
169.212571	5423.722186	25.272666
169.468153	5435.279350	25.277683
169.611695	5453.636560	25.282701
169.882783	5460.077694	25.287719
170.064757	5461.863944	25.292736
169.965962	5472.476159	25.297754
170.040365	5485.319401	25.302771
170.287170	5486.895495	25.307789
170.485177	5498.697899	25.312807
170.492798	5514.705721	25.317824
170.778894	5515.564371	25.322842
171.039437	5528.186019	25.327859
170.935093	5543.528859	25.332877
171.489022	5538.014166	25.337895
171.555383	5539.763788	25.342912
171.506647	5550.492377	25.347930
172.232840	5533.929214	25.352947
171.813441	5556.127325	25.357965
172.066154	5564.686897	25.362983
172.477162	5564.981234	25.368000
172.531224	5568.211835	25.373018
172.844721	5580.248427	25.378035
172.461726	5588.943976	25.383053
172.915011	5597.474738	25.388071
172.998408	5608.946989	25.393088
173.078491	5624.213308	25.398106
173.414772	5620.109244	25.403123
173.483905	5631.138507	25.408141
173.785708	5641.291260	25.413159
174.119791	5652.773930	25.418176
174.142903	5660.014652	25.423194
174.660607	5665.297851	25.428211
174.560536	5683.964816	25.433229
174.821652	5683.477454	25.438247
175.064913	5678.186102	25.443264
175.014618	5686.374732	25.448282
175.486921	5707.765351	25.453299
175.553545	5711.569858	25.458317
175.841195	5705.190469	25.463335
175.782415	5702.954096	25.468352
175.946543	5733.017881	25.473370
176.204401	5732.569587	25.478387
176.339296	5738.309561	25.483405
176.830914	5732.893630	25.488423
176.781118	5752.577762	25.493440
177.074619	5767.971484	25.498458
177.450683	5752.618804	25.503475
177.692860	5753.877831	25.508493
177.324193	5755.547355	25.513511
177.887763	5758.748696	25.518528
178.033057	5779.369429	25.523546
178.345500	5780.769094	25.528563
178.283369	5777.481396	25.533581
178.488710	5770.839748	25.538599
178.860343	5769.559058	25.543616
178.783005	5778.283087	25.548634
178.925660	5782.073919	25.553651
179.207979	5794.811120	25.558669
179.525723	5796.762222	25.563687
179.240627	5795.557904	25.568704
179.510751	5810.845258	25.573722
179.719608	5822.159210	25.578739
179.672692	5836.254109	25.583757
179.966261	5830.723386	25.588775
180.287214	5846.194634	25.593792
180.417325	5859.190600	25.598810
180.828805	5858.812219	25.603827
180.814596	5863.786140	25.608845
180.970171	5877.412951	25.613863
181.660627	5879.542237	25.618880
181.615806	5892.913067	25.623898
181.688010	5880.915312	25.628915
181.796140	5881.881031	25.633933
181.661884	5884.941108	25.638951
182.040155	5885.870055	25.643968
181.897055	5910.908005	25.648986
182.124752	5904.711169	25.654003
182.369419	5912.015036	25.659021
182.580300	5928.848438	25.664039
182.653309	5945.041412	25.669056
182.703435	5945.667073	25.674074
183.070915	5955.598731	25.679092
182.911041	5965.612893	25.684109
183.354286	5974.709565	25.689127
183.744921	5974.068589	25.694144
183.575507	6000.985669	25.699162
183.870497	5994.541262	25.704180
184.238232	6015.121356	25.709197
184.595377	6016.211813	25.714215
184.578399	6030.281669	25.719232
184.541578	6037.656435	25.724250
185.216593	6055.860437	25.729268
185.197947	6058.978434	25.734285
185.304638	6057.227792	25.739303
185.958296	6071.034215	25.744320
185.947983	6077.457544	25.749338
185.870300	6073.220306	25.754356
186.050143	6078.270360	25.759373
186.498399	6092.046609	25.764391
186.829522	6094.585673	25.769408
186.714317	6105.534534	25.774426
187.230562	6091.051318	25.779444
187.290037	6103.246847	25.784461
187.127014	6126.601570	25.789479
187.537308	6123.151154	25.794496
187.638225	6133.827987	25.799514
187.911909	6137.621625	25.804532
188.205689	6152.631778	25.809549
188.387926	6161.413781	25.814567
188.704874	6148.675019	25.819584
188.502484	6164.278023	25.824602
189.088015	6174.719495	25.829620
189.140422	6187.823335	25.834637
189.354064	6183.335857	25.839655
189.453290	6176.968996	25.844672
189.408330	6194.222698	25.849690
189.961579	6192.312737	25.854708
190.017136	6209.222359	25.859725
190.211913	6203.909441	25.864743
190.473147	6215.545780	25.869760
190.226987	6241.092434	25.874778
190.505828	6234.630042	25.879796
190.704442	6246.787773	25.884813
190.594152	6272.344291	25.889831
191.021616	6266.179185	25.894848
191.178110	6279.659100	25.899866
191.474448	6293.255988	25.904884
191.664189	6296.802636	25.909901
192.053974	6296.264063	25.914919
192.233385	6301.982213	25.919936
192.167420	6315.522800	25.924954
192.653679	6315.868102	25.929972
192.551175	6335.752594	25.934989
192.445504	6335.926337	25.940007
192.745115	6342.117848	25.945024
192.997536	6345.058944	25.950042
192.957968	6356.592291	25.955060
193.259017	6392.470151	25.960077
193.531806	6382.933238	25.965095
193.956000	6400.120256	25.970112
193.733355	6414.537180	25.975130
194.247226	6412.270775	25.980148
194.686900	6442.772003	25.985165
194.446016	6457.861406	25.990183
194.929462	6450.227866	25.995200
195.301679	6464.066938	26.000218
195.820067	6481.927450	26.005236
196.017083	6468.334231	26.010253
196.180454	6454.246797	26.015271
196.133173	6465.211058	26.020288
196.100178	6468.009644	26.025306
196.703726	6480.621490	26.030324
196.914037	6491.002630	26.035341
197.030502	6498.966863	26.040359
197.051519	6479.979341	26.045376
197.114785	6486.440684	26.050394
197.483577	6501.801931	26.055412
197.751006	6508.979733	26.060429
197.851788	6519.872439	26.065447
197.956007	6520.657869	26.070464
198.212406	6534.743632	26.075482
198.447478	6540.702406	26.080500
198.731842	6551.636680	26.085517
198.528569	6555.072168	26.090535
198.880455	6561.740871	26.095552
198.822790	6568.829696	26.100570
199.083185	6573.188103	26.105588
199.170339	6598.603562	26.110605
199.176237	6607.425744	26.115623
199.921257	6612.822541	26.120640
199.676043	6641.811836	26.125658
199.863601	6645.008018	26.130676
200.176327	6665.672535	26.135693
200.254722	6677.400541	26.140711
200.771264	6680.931378	26.145728
200.815444	6683.222823	26.150746
201.263417	6687.705570	26.155764
201.605827	6706.293059	26.160781
201.697273	6710.503777	26.165799
202.252063	6698.986250	26.170816
202.355603	6715.512727	26.175834
202.492149	6718.795735	26.180852
202.711700	6702.938314	26.185869
202.579766	6715.928029	26.190887
202.890033	6724.396494	26.195904
202.991759	6730.190924	26.200922
203.279887	6726.858193	26.205940
203.251095	6744.120972	26.210957
203.305113	6759.696316	26.215975
203.900325	6764.155615	26.220992
203.897101	6765.966044	26.226010
204.120683	6766.063701	26.231028
204.389869	6784.081536	26.236045
204.407042	6792.979135	26.241063
204.622369	6811.714474	26.246080
204.583493	6824.646964	26.251098
204.945402	6830.863369	26.256116
205.207975	6841.746258	26.261133
205.260814	6843.177186	26.266151
205.558456	6851.174096	26.271168
205.905552	6873.710680	26.276186
206.025455	6891.186748	26.281204
206.286876	6895.239030	26.286221
206.261264	6911.359878	26.291239
206.599478	6911.814558	26.296256
207.105180	6940.389690	26.301274
207.258737	6946.094903	26.306292
207.399173	6948.395436	26.311309
207.255463	6962.063091	26.316327
207.880256	6958.500402	26.321344
208.103459	6973.890858	26.326362
208.055592	6993.091673	26.331380
208.709916	6988.912937	26.336397
208.948980	6997.432249	26.341415
209.080072	7012.667483	26.346432
209.155524	7015.382794	26.351450
209.393570	7025.445962	26.356468
209.733082	7044.782576	26.361485
209.893059	7065.279238	26.366503
210.462712	7057.036049	26.371520
210.411853	7057.481159	26.376538
210.455957	7064.797116	26.381556
210.835149	7068.139871	26.386573
210.976294	7082.853506	26.391591
211.330992	7091.444134	26.396608
211.536741	7087.941921	26.401626
211.649872	7083.821105	26.406644
211.668901	7099.713954	26.411661
211.872957	7119.613571	26.416679
212.025178	7110.193763	26.421696
212.168596	7127.594763	26.426714
212.148424	7140.375055	26.431732
212.171553	7143.927225	26.436749
212.599016	7173.418519	26.441767
212.675879	7169.096535	26.446784
212.899368	7181.616145	26.451802
213.026732	7203.731917	26.456820
213.455531	7215.269950	26.461837
213.395683	7236.687039	26.466855
214.078575	7235.841285	26.471872
213.877422	7245.833777	26.476890
213.935811	7279.307885	26.481908
214.434951	7273.747796	26.486925
214.949349	7283.069195	26.491943
215.043647	7298.907771	26.496960
215.042273	7306.493888	26.501978
215.503118	7314.837979	26.506996
215.920107	7320.993885	26.512013
216.006479	7323.103247	26.517031
216.160963	7334.777157	26.522048
216.378893	7349.600772	26.527066
216.584380	7363.667118	26.532084
216.909295	7369.605613	26.537101
216.950456	7362.998871	26.542119
217.295203	7369.532964	26.547136
217.785808	7391.633602	26.552154
217.519899	7400.450014	26.557172
218.232352	7397.748183	26.562189
217.836929	7404.234262	26.567207
218.311101	7416.915534	26.572224
218.633565	7432.703720	26.577242
218.588045	7433.634237	26.582260
219.261345	7452.266699	26.587277
219.353974	7457.157246	26.592295
219.452226	7457.204077	26.597312
219.564663	7474.982585	26.602330
219.912759	7488.710806	26.607348
220.055118	7491.797931	26.612365
220.087078	7508.938614	26.617383
220.364830	7523.838631	26.622400
220.548727	7521.597916	26.627418
220.945720	7555.626093	26.632436
221.113286	7549.939364	26.637453
221.479046	7567.553286	26.642471
221.980992	7574.947581	26.647488
222.017642	7575.178119	26.652506
222.384503	7583.774177	26.657524
222.272670	7594.472603	26.662541
222.488529	7618.580486	26.667559
222.738456	7614.359037	26.672576
223.295063	7623.518135	26.677594
222.889404	7644.262339	26.682612
222.980149	7634.851212	26.687629
223.516425	7655.203731	26.692647
223.520207	7659.881903	26.697664
223.941058	7676.162952	26.702682
223.849907	7693.520965	26.707700
224.470445	7701.433034	26.712717
224.618657	7716.497883	26.717735
224.831135	7722.445002	26.722752
225.408439	7726.000246	26.727770
225.411298	7746.785696	26.732788
225.745276	7750.060282	26.737805
225.964967	7747.532931	26.742823
226.451599	7740.157885	26.747840
226.216409	7752.660608	26.752858
226.368478	7764.336029	26.757876
226.744635	7762.544598	26.762893
226.677025	7776.104088	26.767911
227.010303	7786.571974	26.772928
227.061047	7785.063739	26.777946
227.441782	7813.112059	26.782964
227.417210	7822.751042	26.787981
227.691242	7839.635568	26.792999
228.300270	7855.209358	26.798016
228.379917	7862.617609	26.803034
228.781181	7869.375819	26.808052
229.215982	7869.450837	26.813069
229.290465	7893.265396	26.818087
229.295629	7884.817461	26.823104
229.898880	7896.898676	26.828122
229.686264	7908.286921	26.833140
230.014213	7915.810627	26.838157
230.228716	7933.413687	26.843175
230.529971	7938.479650	26.848192
230.811427	7960.062117	26.853210
230.684605	7967.718139	26.858228
231.118792	7967.508420	26.863245
231.348417	7995.299483	26.868263
231.504170	8002.628792	26.873280
232.104006	8014.996272	26.878298
232.192987	8035.234919	26.883316
232.401196	8035.411365	26.888333
232.646713	8042.806643	26.893351
232.634015	8057.744446	26.898368
233.088411	8051.442132	26.903386
233.157941	8075.410419	26.908404
233.727989	8083.889404	26.913421
234.116038	8098.436436	26.918439
234.000401	8113.659411	26.923456
234.371293	8116.201937	26.928474
234.384364	8119.064306	26.933492
234.778569	8136.546903	26.938509
234.974104	8153.482068	26.943527
235.112232	8156.875304	26.948544
235.473728	8166.304257	26.953562
235.499404	8184.394086	26.958580
235.972106	8181.018241	26.963597
236.434666	8197.914828	26.968615
236.115585	8217.362673	26.973632
236.524774	8219.505688	26.978650
236.586234	8239.769458	26.983668
236.991751	8243.801508	26.988685
237.052825	8253.615962	26.993703
237.336383	8267.134088	26.998720
237.591155	8261.745569	27.003738
237.519248	8292.841251	27.008756
237.937334	8299.899918	27.013773
238.181138	8306.228625	27.018791
238.313416	8325.847019	27.023808
238.636605	8335.713383	27.028826
238.904166	8352.632573	27.033844
238.953844	8357.650653	27.038861
239.287897	8371.899685	27.043879
239.460917	8392.311121	27.048896
239.900595	8400.989687	27.053914
240.074191	8427.886386	27.058932
240.415004	8430.672182	27.063949
240.975708	8448.453582	27.068967
240.830587	8460.528649	27.073984
241.461103	8458.353522	27.079002
241.246440	8470.364930	27.084020
241.481085	8475.869750	27.089037
241.423103	8495.671345	27.094055
242.060410	8518.763766	27.099072
242.713029	8523.565405	27.104090
242.498648	8533.919677	27.109108
242.907086	8553.169375	27.114125
243.004961	8561.173089	27.119143
243.181351	8587.520397	27.124160
243.448925	8601.985620	27.129178
243.682327	8615.509697	27.134196
244.194203	8619.027595	27.139213
244.235705	8632.757747	27.144231
244.634189	8638.901420	27.149248
244.903862	8628.123464	27.154266
245.216755	8641.355554	27.159284
245.692335	8660.645836	27.164301
245.868072	8652.435455	27.169319
246.001822	8664.932854	27.174336
246.602676	8672.186827	27.179354
246.660133	8686.263858	27.184372
246.778529	8685.247563	27.189389
247.306931	8688.264751	27.194407
247.313010	8711.532840	27.199424
247.853265	8706.402394	27.204442
247.673366	8712.311734	27.209460
247.669529	8706.469332	27.214477
247.969907	8728.866678	27.219495
248.280361	8732.320710	27.224512
248.515599	8756.563481	27.229530
248.605547	8761.872719	27.234548
248.920992	8773.705449	27.239565
248.953829	8789.534163	27.244583
248.946707	8800.928102	27.249600
249.498966	8816.851890	27.254618
249.950974	8840.005035	27.259636
249.989331	8856.054055	27.264653
250.006833	8884.082818	27.269671
250.442544	8889.020661	27.274688
250.652412	8900.217598	27.279706
250.751783	8913.320292	27.284724
251.095996	8914.675864	27.289741
251.440740	8940.974930	27.294759
251.417060	8954.162191	27.299776
252.077351	8957.222546	27.304794
252.172546	8990.139482	27.309812
252.291860	8997.548272	27.314829
253.045384	9006.479338	27.319847
253.165098	9013.282951	27.324864
253.535578	9033.701170	27.329882
253.865370	9043.431608	27.334900
253.888754	9052.743082	27.339917
254.119355	9057.055437	27.344935
254.262218	9074.151523	27.349952
254.784678	9077.636763	27.354970
254.809273	9096.147285	27.359988
254.752522	9106.721552	27.365005
255.544733	9128.168830	27.370023
255.596303	9151.173822	27.375040
256.114956	9150.628399	27.380058
256.360364	9170.519845	27.385076
256.789997	9167.536232	27.390093
257.190066	9181.148753	27.395111
257.059589	9197.982836	27.400128
257.335421	9184.042906	27.405146
257.483836	9191.505384	27.410164
257.927477	9206.538031	27.415181
258.090686	9219.787020	27.420199
258.235431	9236.490326	27.425216
258.203553	9249.838110	27.430234
258.643818	9265.084999	27.435252
258.859299	9271.475291	27.440269
259.096177	9281.005083	27.445287
259.309467	9306.656875	27.450304
259.637201	9317.077153	27.455322
259.929781	9330.491330	27.460340
259.970523	9353.966571	27.465357
260.439108	9371.680743	27.470375
260.907967	9385.303733	27.475392
260.984889	9399.327972	27.480410
261.435156	9416.602478	27.485428
261.779657	9418.792183	27.490445
262.310656	9427.780614	27.495463
262.242444	9436.096528	27.500480
262.574422	9453.585479	27.505498
262.705625	9462.614439	27.510516
262.688374	9469.737939	27.515533
263.257423	9488.518248	27.520551
263.285008	9496.371563	27.525568
263.776004	9510.803634	27.530586
263.722580	9522.462431	27.535604
264.228556	9547.304281	27.540621
264.604787	9552.930549	27.545639
264.639750	9558.188635	27.550656
265.073000	9568.159464	27.555674
265.836262	9582.070548	27.560692
265.533523	9596.269587	27.565709
265.901820	9589.398038	27.570727
266.002205	9608.342512	27.575744
266.349812	9611.976545	27.580762
266.507245	9618.054387	27.585780
266.735241	9632.480492	27.590797
266.898840	9640.252791	27.595815
267.095537	9666.542501	27.600832
267.411152	9664.703059	27.605850
267.666017	9685.015870	27.610868
267.689208	9698.303732	27.615885
268.204464	9700.526465	27.620903
268.625644	9727.578056	27.625920
268.855118	9740.996759	27.630938
268.864648	9755.363764	27.635956
269.492436	9772.250369	27.640973
269.726951	9779.259917	27.645991
269.582201	9796.857124	27.651008
270.019021	9813.706929	27.656026
270.384887	9830.158856	27.661044
270.589550	9851.745287	27.666061
271.090561	9865.760604	27.671079
271.182800	9879.886727	27.676096
271.165476	9884.668114	27.681114
271.391350	9914.584545	27.686132
271.823360	9922.791097	27.691149
272.308964	9941.764308	27.696167
272.430257	9965.825745	27.701184
273.044568	9974.954292	27.706202
273.041038	9978.454727	27.711220
273.620630	9996.047285	27.716237
274.107649	9999.399110	27.721255
273.997205	10025.097042	27.726272
274.485633	10033.673972	27.731290
274.961776	10038.794627	27.736308
275.100567	10055.968031	27.741325
275.468673	10058.011241	27.746343
275.562584	10076.966783	27.751360
275.862299	10095.571620	27.756378
276.472875	10089.538287	27.761396
276.407266	10108.616088	27.766413
276.973816	10111.657402	27.771431
277.056341	10127.020426	27.776448
277.533955	10120.116263	27.781466
277.578216	10137.045526	27.786484
277.664320	10149.438440	27.791501
278.001190	10158.352805	27.796519
278.246036	10175.486228	27.801536
278.078706	10190.494875	27.806554
278.776558	10206.754227	27.811572
278.692114	10213.901381	27.816589
278.889514	10236.703798	27.821607
278.952946	10256.471449	27.826624
279.295083	10279.485377	27.831642
279.479091	10285.792589	27.836660
279.784355	10315.624768	27.841677
280.414386	10324.289866	27.846695
280.394425	10347.780273	27.851712
280.617719	10373.049834	27.856730
280.978136	10372.052697	27.861748
281.241189	10410.662510	27.866765
281.789956	10414.929275	27.871783
282.190312	10444.171281	27.876800
282.691674	10441.785107	27.881818
282.982858	10468.436155	27.886836
283.132601	10475.161674	27.891853
283.471977	10487.659697	27.896871
283.885205	10501.088357	27.901888
283.913220	10503.393200	27.906906
284.281374	10517.667971	27.911924
284.525926	10527.909153	27.916941
284.406608	10544.966465	27.921959
284.746442	10560.456155	27.926976
285.200289	10585.926997	27.931994
285.619503	10592.747342	27.937012
285.791545	10627.009617	27.942029
286.435823	10634.983235	27.947047
286.595545	10641.312175	27.952064
286.856472	10656.181416	27.957082
287.224353	10663.525447	27.962100
287.042290	10679.989692	27.967117
287.577240	10691.739384	27.972135
288.057977	10703.465459	27.977152
288.465226	10707.580154	27.982170
288.447335	10746.330044	27.987188
288.392165	10750.808846	27.992205
289.178525	10771.638500	27.997223
289.444318	10788.955014	28.002240
289.472735	10798.012967	28.007258
290.114624	10809.634349	28.012276
290.510793	10828.093691	28.017293
290.563772	10846.540464	28.022311
290.602322	10863.547006	28.027328
291.050292	10872.201699	28.032346
291.389248	10889.049821	28.037364
291.456873	10913.514039	28.042381
292.147330	10925.149414	28.047399
292.275974	10936.879058	28.052416
292.120108	10957.792242	28.057434
292.792663	10970.803025	28.062452
292.845160	10999.793445	28.067469
293.287918	11007.773017	28.072487
293.380560	11026.220772	28.077504
293.717081	11041.862591	28.082522
294.515907	11053.666528	28.087540
294.610385	11070.561293	28.092557
295.048509	11083.118448	28.097575
295.468054	11084.581063	28.102592
295.474797	11097.044857	28.107610
296.043967	11107.286249	28.112628
296.264929	11111.604674	28.117645
296.615121	11117.582363	28.122663
296.994085	11133.932901	28.127680
297.048048	11145.988626	28.132698
297.482722	11146.615004	28.137716
297.278082	11171.511026	28.142733
297.594854	11168.032678	28.147751
298.070989	11186.789798	28.152768
298.258954	11203.087428	28.157786
298.556068	11213.454101	28.162804
298.652894	11234.155435	28.167821
298.697966	11253.550345	28.172839
299.103107	11268.269713	28.177856
299.495415	11295.075713	28.182874
300.005433	11306.661443	28.187892
300.037580	11335.827714	28.192909
300.597341	11349.318192	28.197927
300.803937	11372.964155	28.202944
300.830825	11394.154967	28.207962
301.068341	11400.388406	28.212980
301.783059	11430.539248	28.217997
302.147591	11451.609434	28.223015
302.620864	11458.785166	28.228032
302.689744	11492.398458	28.233050
303.195533	11488.333490	28.238068
303.314258	11511.430559	28.243085
303.481876	11519.321248	28.248103
303.987598	11541.120273	28.253120
304.387589	11553.856652	28.258138
305.042999	11573.320374	28.263156
305.070263	11598.849506	28.268173
305.177073	11605.659110	28.273191
305.816914	11620.508271	28.278208
306.093467	11636.296817	28.283226
306.696657	11629.409741	28.288244
306.954892	11644.744738	28.293261
307.428754	11659.641640	28.298279
307.512469	11659.743146	28.303296
307.368591	11682.093328	28.308314
307.969765	11688.083193	28.313332
307.957644	11703.373188	28.318349
308.256116	11716.623290	28.323367
308.629858	11738.486922	28.328384
308.927569	11757.799325	28.333402
309.337747	11761.257854	28.338420
309.488518	11786.102181	28.343437
309.693456	11803.695582	28.348455
310.237016	11813.587374	28.353472
310.327529	11831.604369	28.358490
310.787495	11847.949466	28.363508
310.973959	11873.912144	28.368525
311.417032	11888.871241	28.373543
311.603187	11901.812783	28.378560
311.357826	11916.005639	28.383578
312.406809	11921.847103	28.388596
312.617383	11956.669786	28.393613
312.909353	11960.162154	28.398631
313.483613	11973.852172	28.403648
313.538052	11980.291328	28.408666
313.904269	11998.861955	28.413684
314.108944	12008.279773	28.418701
314.503090	12020.110012	28.423719
315.055846	12040.633149	28.428736
315.021041	12055.947578	28.433754
315.353431	12059.538206	28.438772
315.325223	12078.350055	28.443789
315.916034	12107.459874	28.448807
315.907372	12116.282901	28.453824
316.207513	12136.846033	28.458842
316.316896	12156.945714	28.463860
316.604213	12188.355432	28.468877
316.915936	12196.279589	28.473895
317.487098	12229.411500	28.478912
317.748079	12256.567950	28.483930
318.111692	12263.156886	28.488948
318.582245	12300.306414	28.493965
318.523952	12327.900322	28.498983
318.815584	12336.832838	28.504000
319.204923	12363.328549	28.509018
319.849830	12386.558366	28.514036
320.095079	12410.572079	28.519053
320.815250	12422.814854	28.524071
321.425885	12441.555452	28.529088
321.922363	12461.525571	28.534106
322.801209	12456.630948	28.539124
323.049706	12472.051965	28.544141
323.217432	12481.046815	28.549159
323.498333	12469.454438	28.554176
323.965077	12474.377130	28.559194
323.941847	12467.244770	28.564212
324.400172	12497.194225	28.569229
324.644146	12491.257931	28.574247
325.192463	12501.401287	28.579264
325.180301	12511.847461	28.584282
325.165844	12513.503352	28.589300
325.612485	12528.040448	28.594317
325.644919	12556.788927	28.599335
326.210098	12556.111247	28.604352
325.985333	12577.086839	28.609370
326.304043	12590.408078	28.614388
326.408006	12619.962857	28.619405
327.116121	12629.671945	28.624423
327.465894	12651.137735	28.629440
327.384237	12681.005169	28.634458
327.963360	12687.428309	28.639476
328.481812	12719.534286	28.644493
328.445860	12741.491029	28.649511
328.766185	12749.921976	28.654528
329.118467	12770.046533	28.659546
329.501012	12774.990811	28.664564
329.669947	12816.518469	28.669581
329.687817	12825.624772	28.674599
330.225772	12847.821971	28.679616
330.599128	12878.961639	28.684634
331.065780	12893.879214	28.689652
331.679884	12908.666655	28.694669
331.483879	12946.166810	28.699687
332.308612	12962.021496	28.704704
332.620185	12975.141140	28.709722
332.977048	12998.157863	28.714740
333.022490	13017.016597	28.719757
333.328964	13039.090789	28.724775
333.991202	13042.308152	28.729792
334.081256	13078.225834	28.734810
334.795154	13097.641086	28.739828
335.019073	13103.719192	28.744845
335.047378	13133.823637	28.749863
335.696866	13136.741590	28.754880
336.051702	13154.254824	28.759898
336.765820	13168.446681	28.764916
337.062448	13188.278610	28.769933
337.043069	13203.524835	28.774951
338.023861	13211.180567	28.779968
337.645200	13233.424437	28.784986
338.281179	13234.747116	28.790004
338.829848	13240.767625	28.795021
338.876252	13280.257382	28.800039
339.258712	13279.240228	28.805056
339.609261	13306.944914	28.810074
339.873765	13312.888141	28.815092
340.102607	13332.378039	28.820109
340.167855	13351.905247	28.825127
340.757575	13371.807206	28.830144
340.727380	13398.533142	28.835162
341.412435	13421.221930	28.840180
341.807225	13439.568004	28.845197
341.942744	13464.275832	28.850215
342.832618	13476.010117	28.855232
342.964253	13485.745114	28.860250
343.171733	13500.803178	28.865268
343.490266	13526.731508	28.870285
343.845070	13543.099532	28.875303
344.433630	13554.970053	28.880320
344.756853	13577.478037	28.885338
344.926210	13595.089818	28.890356
345.515174	13608.810077	28.895373
345.532337	13636.171578	28.900391
345.640984	13640.253600	28.905408
346.036789	13675.487181	28.910426
346.567059	13691.031413	28.915444
346.592944	13705.177988	28.920461
346.983909	13729.347086	28.925479
347.550741	13748.395009	28.930496
347.857331	13764.215038	28.935514
347.878924	13781.183873	28.940532
348.611052	13785.368485	28.945549
348.892196	13825.023954	28.950567
349.246025	13826.943637	28.955584
349.634453	13845.152089	28.960602
350.009375	13858.060207	28.965620
350.717375	13865.693531	28.970637
350.511081	13888.068609	28.975655
351.071205	13900.127635	28.980672
351.145921	13917.589963	28.985690
351.298148	13945.219674	28.990708
351.699057	13962.933227	28.995725
352.027342	13991.298406	29.000743
352.270264	14020.165373	29.005760
352.776054	14037.258652	29.010778
352.965992	14060.515823	29.015796
353.377312	14091.912086	29.020813
353.509460	14122.974178	29.025831
354.312868	14127.188658	29.030848
354.858394	14171.206566	29.035866
355.126831	14193.327660	29.040884
356.030135	14198.353059	29.045901
355.613601	14227.593555	29.050919
356.336635	14244.397999	29.055936
356.641056	14262.310883	29.060954
356.853641	14283.169144	29.065972
357.179094	14297.439053	29.070989
357.520660	14329.017637	29.076007
358.172297	14344.808971	29.081024
358.435155	14369.257889	29.086042
358.904531	14386.342604	29.091060
359.310179	14398.141391	29.096077
359.701873	14428.629142	29.101095
359.923624	14450.332778	29.106112
360.121892	14470.802055	29.111130
360.632658	14488.994047	29.116148
360.978228	14507.159546	29.121165
361.338898	14531.897580	29.126183
361.826519	14544.670051	29.131200
362.035493	14577.147394	29.136218
362.337250	14596.665374	29.141236
362.548746	14602.007291	29.146253
363.038958	14640.313330	29.151271
363.476631	14653.921480	29.156288
364.013296	14670.933901	29.161306
364.281349	14694.895835	29.166324
365.050643	14690.771719	29.171341
365.266914	14728.154372	29.176359
365.372302	14735.973608	29.181376
365.902925	14752.337159	29.186394
366.149377	14763.627881	29.191412
366.741659	14788.426055	29.196429
367.081131	14804.811757	29.201447
367.234726	14824.266357	29.206464
367.726653	14823.187487	29.211482
367.800248	14852.184854	29.216500
368.292732	14861.309834	29.221517
368.346067	14890.324671	29.226535
368.792994	14891.166549	29.231552
369.127219	14917.965095	29.236570
369.054253	14934.635005	29.241588
369.580144	14958.191598	29.246605
369.820253	14991.377671	29.251623
370.089474	15009.906339	29.256640
370.748291	15034.552812	29.261658
371.110574	15055.662789	29.266676
371.537410	15075.917467	29.271693
371.589920	15123.365562	29.276711
372.207183	15141.034206	29.281728
372.128657	15169.808343	29.286746
372.303803	15192.207794	29.291764
373.062418	15215.384378	29.296781
373.341336	15256.047718	29.301799
373.890075	15292.876432	29.306816
374.221472	15312.936542	29.311834
374.515148	15348.426428	29.316852
375.039088	15368.838128	29.321869
375.310094	15412.907000	29.326887
376.204967	15423.563811	29.331904
376.840244	15447.109535	29.336922
377.161654	15474.950928	29.341940
377.657361	15489.066508	29.346957
378.163809	15504.093183	29.351975
378.274984	15521.571609	29.356992
378.505045	15539.326225	29.362010
378.901610	15576.029802	29.367028
379.405920	15591.849157	29.372045
379.292017	15612.856314	29.377063
379.673925	15643.543677	29.382080
380.428953	15662.403813	29.387098
380.478905	15689.192423	29.392116
381.360557	15718.708212	29.397133
381.613136	15739.173388	29.402151
381.768433	15754.852597	29.407168
382.448926	15770.069771	29.412186
382.854965	15794.893648	29.417204
383.459222	15820.079998	29.422221
383.472657	15849.424400	29.427239
383.920682	15853.595533	29.432256
384.582112	15876.849621	29.437274
384.638601	15897.417300	29.442292
385.200729	15923.855866	29.447309
385.396622	15950.444743	29.452327
385.508408	15968.235825	29.457344
385.961287	16000.653805	29.462362
386.202699	16031.917281	29.467380
386.542452	16051.642050	29.472397
386.693724	16074.655440	29.477415
387.412195	16094.967345	29.482432
388.137995	16110.317576	29.487450
388.314489	16131.939978	29.492468
388.580013	16157.360253	29.497485
389.079586	16176.734874	29.502503
389.538460	16187.818130	29.507520
389.930751	16222.462286	29.512538
390.013032	16235.868185	29.517556
390.665597	16248.056749	29.522573
390.650703	16268.777220	29.527591
391.071642	16299.296713	29.532608
391.780923	16318.841414	29.537626
391.908479	16348.342571	29.542644
392.524174	16373.450366	29.547661
392.886139	16393.914535	29.552679
393.215789	16426.519558	29.557696
393.450843	16452.709623	29.562714
393.651981	16487.329624	29.567732
394.287296	16503.589807	29.572749
394.411796	16538.952732	29.577767
394.833451	16573.317746	29.582784
395.708827	16585.495486	29.587802
396.124206	16622.011489	29.592820
396.633114	16649.381897	29.597837
397.089694	16667.665525	29.602855
397.598174	16690.780381	29.607872
398.183090	16713.469176	29.612890
398.404319	16740.981632	29.617908
398.942639	16752.035418	29.622925
398.922059	16777.688695	29.627943
399.470601	16802.717354	29.632960
399.841364	16814.792434	29.637978
399.969145	16840.283022	29.642996
400.523916	16862.018697	29.648013
400.871473	16889.619348	29.653031
401.547614	16916.500655	29.658048
401.950996	16929.489213	29.663066
402.158820	16971.186698	29.668084
403.194314	16972.837380	29.673101
403.372497	17004.210828	29.678119
403.193213	17019.913242	29.683136
403.806307	17040.455373	29.688154
404.365878	17068.446138	29.693172
404.912955	17090.821478	29.698189
405.358757	17109.522460	29.703207
405.500255	17137.563230	29.708224
406.095390	17155.872801	29.713242
406.102027	17184.478783	29.718260
406.515364	17203.275397	29.723277
406.905016	17222.362194	29.728295
407.030224	17254.219933	29.733312
407.859652	17280.905425	29.738330
408.170387	17305.407299	29.743348
408.520465	17329.222695	29.748365
409.150230	17357.689172	29.753383
409.698651	17378.059203	29.758400
410.117468	17399.620272	29.763418
410.115547	17420.326640	29.768436
410.489676	17445.763233	29.773453
410.891153	17455.545946	29.778471
411.063405	17482.420344	29.783488
411.357331	17505.396609	29.788506
411.636817	17534.292809	29.793524
412.344709	17548.756671	29.798541
412.819696	17599.391265	29.803559
413.302425	17622.339396	29.808576
413.930421	17644.929994	29.813594
413.828323	17675.017675	29.818612
414.507236	17687.984629	29.823629
415.360245	17720.756431	29.828647
415.459616	17752.492748	29.833664
416.129501	17764.419745	29.838682
416.524128	17789.519215	29.843700
416.943685	17823.498600	29.848717
417.130188	17837.388367	29.853735
417.758777	17846.833985	29.858752
418.262638	17874.623295	29.863770
418.490530	17899.464879	29.868788
418.808883	17914.921406	29.873805
418.934775	17946.991277	29.878823
418.978733	17989.030983	29.883840
420.280195	18008.999608	29.888858
420.579601	18044.577077	29.893876
421.014098	18060.851816	29.898893
421.524873	18079.413908	29.903911
421.652374	18122.554389	29.908928
422.390393	18130.741864	29.913946
422.736922	18161.225329	29.918964
422.936771	18190.511804	29.923981
423.349165	18204.683615	29.928999
423.730442	18238.997754	29.934016
424.246137	18270.992217	29.939034
424.800404	18296.111956	29.944052
425.134263	18329.842140	29.949069
425.764711	18352.492833	29.954087
426.029436	18374.340828	29.959104
426.810193	18402.528101	29.964122
426.761238	18425.746183	29.969140
427.282734	18441.606294	29.974157
428.055093	18466.567552	29.979175
428.030298	18504.745300	29.984192
428.743328	18511.564160	29.989210
428.854418	18551.346321	29.994228
429.723133	18578.887239	29.999245
430.375063	18594.807828	30.004263
430.506838	18630.262957	30.009280
431.254188	18644.036145	30.014298
431.400760	18665.667552	30.019316
431.867586	18685.810978	30.024333
432.559317	18712.656324	30.029351
432.495863	18744.336556	30.034368
432.664108	18751.548219	30.039386
433.176052	18775.778637	30.044404
433.753058	18802.112892	30.049421
434.065743	18831.129452	30.054439
434.122951	18855.562755	30.059456
434.961480	18877.329101	30.064474
435.148921	18902.118501	30.069492
435.566935	18918.888110	30.074509
436.191742	18944.027192	30.079527
436.507855	18986.277421	30.084544
436.667728	19003.727229	30.089562
437.002006	19041.784522	30.094580
437.487586	19077.747698	30.099597
437.954023	19112.022249	30.104615
438.357033	19138.034395	30.109632
439.072549	19176.782871	30.114650
439.195081	19200.473617	30.119668
439.599789	19236.198464	30.124685
440.182124	19274.149483	30.129703
440.647812	19308.347419	30.134720
441.322785	19334.873276	30.139738
442.005879	19374.884536	30.144756
442.269225	19398.877965	30.149773
442.724458	19420.686847	30.154791
443.208081	19463.333748	30.159808
443.339680	19475.750604	30.164826
443.965360	19494.714611	30.169844
444.216324	19538.703166	30.174861
445.278656	19553.013629	30.179879
445.784991	19582.138541	30.184896
446.349915	19610.905734	30.189914
446.746943	19631.287896	30.194932
447.328994	19652.530813	30.199949
447.740691	19665.428815	30.204967
447.547552	19702.035446	30.209984
448.556662	19714.754454	30.215002
449.026969	19750.598385	30.220020
448.967933	19778.032530	30.225037
449.550231	19797.690081	30.230055
449.997822	19842.170640	30.235072
450.303672	19858.276415	30.240090
450.367566	19902.065861	30.245108
450.707245	19938.138527	30.250125
451.501962	19966.285477	30.255143
451.940400	20006.225124	30.260160
452.452215	20033.229776	30.265178
453.139616	20069.266644	30.270196
453.345457	20106.746167	30.275213
453.899699	20141.928757	30.280231
454.522305	20152.123662	30.285248
454.873857	20193.558855	30.290266
455.251953	20223.019596	30.295284
455.442233	20255.838166	30.300301
456.021248	20271.920933	30.305319
456.439697	20318.840389	30.310336
457.030648	20334.035803	30.315354
457.868082	20355.240178	30.320372
458.075722	20392.462201	30.325389
458.672972	20415.318464	30.330407
458.889700	20427.722910	30.335424
459.130053	20458.365209	30.340442
459.651422	20501.640891	30.345460
459.896280	20531.600261	30.350477
460.423430	20559.981482	30.355495
460.820277	20596.672615	30.360512
461.077552	20626.243925	30.365530
461.567367	20659.621993	30.370548
462.003884	20693.933534	30.375565
462.417418	20728.682722	30.380583
463.197680	20770.248809	30.385600
463.931916	20802.961006	30.390618
464.341393	20838.956514	30.395636
464.824237	20866.951601	30.400653
465.139304	20890.026762	30.405671
465.401564	20924.339005	30.410688
465.888598	20959.501856	30.415706
466.938759	20990.075650	30.420724
467.025367	21022.803273	30.425741
467.654408	21057.735820	30.430759
468.297667	21088.325013	30.435776
468.798957	21121.554581	30.440794
469.529978	21133.398065	30.445812
469.649677	21173.713564	30.450829
469.694562	21188.604618	30.455847
470.386613	21228.797189	30.460864
470.832217	21264.125616	30.465882
471.620823	21288.219011	30.470900
471.760162	21334.398055	30.475917
472.385270	21354.447666	30.480935
473.242059	21384.556503	30.485952
473.660357	21414.603731	30.490970
474.026274	21444.185267	30.495988
474.479686	21473.846638	30.501005
475.415074	21494.196667	30.506023
475.418492	21528.933025	30.511040
475.913747	21541.874795	30.516058
476.334920	21581.090380	30.521076
476.710118	21606.447966	30.526093
477.088560	21636.718542	30.531111
477.382754	21670.587489	30.536128
478.003652	21708.114587	30.541146
478.418348	21735.046691	30.546164
478.869559	21779.120293	30.551181
479.562172	21803.802323	30.556199
479.967804	21842.019272	30.561216
480.347599	21872.711427	30.566234
481.193828	21896.794221	30.571252
481.475778	21940.634558	30.576269
481.979024	21959.928615	30.581287
482.344626	21992.483474	30.586304
482.840082	22007.618949	30.591322
483.132291	22037.148763	30.596340
483.514665	22078.688775	30.601357
483.921498	22102.824551	30.606375
484.240755	22140.507841	30.611392
485.038092	22176.067391	30.616410
485.708460	22195.200443	30.621428
485.713375	22238.725032	30.626445
486.462081	22265.685961	30.631463
486.724863	22298.053062	30.636480
487.215806	22329.879837	30.641498
487.681129	22373.505514	30.646516
487.991048	22405.699936	30.651533
488.982135	22431.481339	30.656551
489.451584	22481.148186	30.661568
489.612015	22515.059947	30.666586
490.435273	22540.879290	30.671604
490.316779	22587.136943	30.676621
491.269413	22631.901747	30.681639
491.773600	22664.572962	30.686656
492.160839	22702.468867	30.691674
492.508800	22745.830734	30.696692
493.032386	22789.653057	30.701709
493.897507	22817.181574	30.706727
494.051513	22858.381968	30.711744
494.205614	22888.382735	30.716762
495.161377	22928.452195	30.721780
495.960782	22972.042064	30.726797
496.165004	23013.323075	30.731815
496.676859	23052.832686	30.736832
497.397567	23074.407476	30.741850
498.009447	23113.467332	30.746868
498.505295	23163.729134	30.751885
499.149359	23181.059998	30.756903
499.695026	23218.496354	30.761920
500.019977	23252.533139	30.766938
500.316445	23275.673837	30.771956
500.998638	23310.184701	30.776973
501.761195	23345.781577	30.781991
502.217157	23379.107806	30.787008
502.702702	23411.838672	30.792026
503.387991	23426.935827	30.797044
503.533499	23462.605261	30.802061
504.326005	23492.161290	30.807079
504.340490	23519.965942	30.812096
504.817076	23563.826253	30.817114
505.533000	23587.807166	30.822132
505.594182	23630.854826	30.827149
506.493256	23675.868995	30.832167
507.184193	23730.353216	30.837184
507.426320	23751.089134	30.842202
507.984665	23782.886051	30.847220
508.343596	23829.355623	30.852237
508.899941	23854.361887	30.857255
509.373561	23890.458913	30.862272
509.745327	23922.401614	30.867290
510.340980	23956.658296	30.872308
510.531930	23987.374404	30.877325
510.983852	24026.872365	30.882343
511.246533	24068.075923	30.887360
511.889332	24102.167090	30.892378
512.539762	24139.444796	30.897396
512.940777	24178.685800	30.902413
513.484624	24222.660097	30.907431
514.308846	24258.316159	30.912448
514.708892	24300.263268	30.917466
515.237633	24333.965087	30.922484
515.677991	24382.410612	30.927501
516.381978	24415.972842	30.932519
516.625798	24455.059188	30.937536
517.190741	24492.895629	30.942554
517.958163	24524.961629	30.947572
518.360184	24572.534784	30.952589
518.581383	24613.957464	30.957607
519.302008	24641.994250	30.962624
519.793391	24683.184242	30.967642
520.145739	24728.625617	30.972660
521.180164	24772.680838	30.977677
521.537153	24807.411392	30.982695
522.101359	24850.085269	30.987712
522.657790	24888.571498	30.992730
523.539187	24927.386522	30.997748
523.409096	24972.751832	31.002765
523.886952	25012.348150	31.007783
524.941120	25044.966612	31.012800
525.134025	25091.189042	31.017818
525.887957	25130.254876	31.022836
526.144304	25173.736436	31.027853
526.535421	25214.528646	31.032871
527.286094	25264.688770	31.037888
527.698145	25310.630374	31.042906
528.819733	25335.758480	31.047924
529.196710	25384.473948	31.052941
528.995710	25437.743318	31.057959
529.810230	25467.370424	31.062976
530.246486	25512.283916	31.067994
530.866312	25555.532171	31.073012
531.614310	25586.438348	31.078029
532.269397	25631.564671	31.083047
532.741020	25690.489275	31.088064
533.414269	25730.224045	31.093082
534.199520	25756.319382	31.098100
534.492782	25804.108107	31.103117
534.530201	25838.956401	31.108135
535.233563	25884.689408	31.113152
535.544367	25935.394349	31.118170
536.231152	25974.305156	31.123188
536.523197	26022.717841	31.128205
537.358406	26061.623339	31.133223
537.669125	26096.490898	31.138240
538.301738	26138.855615	31.143258
538.891664	26180.773490	31.148276
539.714555	26202.731734	31.153293
540.157602	26247.242873	31.158311
540.549848	26287.624064	31.163328
541.025265	26324.874893	31.168346
541.643979	26360.061074	31.173364
542.318718	26397.612768	31.178381
542.550854	26428.680728	31.183399
542.809342	26465.289732	31.188416
543.265747	26528.901621	31.193434
544.376126	26558.939764	31.198452
544.712587	26603.988807	31.203469
545.018753	26656.845064	31.208487
545.923171	26690.516454	31.213504
546.121958	26741.401707	31.218522
546.672703	26789.899978	31.223540
547.046658	26834.679785	31.228557
547.654497	26885.160016	31.233575
548.646253	26927.856432	31.238592
548.943901	26981.346142	31.243610
549.628621	27017.355965	31.248628
550.282477	27064.496221	31.253645
550.513018	27109.064866	31.258663
551.467909	27153.578934	31.263680
552.124453	27197.890115	31.268698
552.498481	27248.730944	31.273716
553.203791	27292.899904	31.278733
553.495982	27338.699396	31.283751
554.503290	27377.567292	31.288768
554.570005	27427.034029	31.293786
555.513082	27463.688328	31.298804
555.825336	27515.967384	31.303821
556.372204	27555.661422	31.308839
557.319881	27593.968949	31.313856
557.783001	27649.952448	31.318874
558.376215	27682.117143	31.323892
558.657428	27721.219687	31.328909
559.442870	27768.162210	31.333927
560.056913	27810.568966	31.338944
560.074641	27865.439227	31.343962
560.886845	27905.031204	31.348980
561.611605	27959.135266	31.353997
561.653256	28001.111335	31.359015
562.647303	28051.570749	31.364032
562.979235	28096.187429	31.369050
563.550318	28133.654907	31.374068
564.302088	28197.250773	31.379085
564.795902	28231.352422	31.384103
565.289156	28267.535779	31.389120
566.054364	28329.223386	31.394138
566.363661	28366.362797	31.399156
566.875113	28418.000085	31.404173
567.386690	28464.535224	31.409191
568.223826	28502.071490	31.414208
568.741471	28549.255119	31.419226
569.137259	28594.247490	31.424244
569.742763	28638.603067	31.429261
569.870156	28676.046343	31.434279
570.697446	28728.524637	31.439296
571.257573	28777.731772	31.444314
571.717801	28813.598576	31.449332
572.435331	28854.173920	31.454349
572.530100	28914.010243	31.459367
573.742255	28954.946717	31.464384
574.258953	29012.205955	31.469402
574.861863	29048.241229	31.474420
575.378134	29100.007567	31.479437
575.631852	29143.957263	31.484455
576.688441	29179.725178	31.489472
576.978097	29245.436300	31.494490
577.449695	29302.215237	31.499508
578.198245	29342.552067	31.504525
578.292598	29399.339418	31.509543
579.246958	29452.363975	31.514560
579.727031	29497.543989	31.519578
580.440171	29542.384446	31.524596
580.906649	29606.942132	31.529613
581.491634	29664.039936	31.534631
582.359429	29705.668229	31.539648
582.880867	29760.719975	31.544666
583.360472	29812.779660	31.549684
584.170746	29856.760843	31.554701
584.889330	29911.832135	31.559719
585.506210	29958.740888	31.564736
585.920084	30003.461656	31.569754
586.771443	30041.766697	31.574772
587.141577	30086.384345	31.579789
587.607295	30143.529617	31.584807
588.904658	30183.437591	31.589824
589.395453	30228.413059	31.594842
589.710900	30282.144078	31.599860
590.394533	30322.607150	31.604877
590.992299	30369.017408	31.609895
591.458235	30414.791622	31.614912
592.392127	30457.185106	31.619930
592.795487	30511.725527	31.624948
593.365368	30557.374848	31.629965
593.931566	30595.086766	31.634983
594.744091	30630.847900	31.640000
595.267760	30683.831596	31.645018
595.674212	30730.013313	31.650036
596.294864	30765.144963	31.655053
596.648569	30817.489521	31.660071
597.189616	30873.660854	31.665088
597.573587	30918.264391	31.670106
598.228927	30967.240779	31.675124
598.921676	31024.699703	31.680141
599.285345	31082.860549	31.685159
599.828620	31127.068926	31.690176
600.549850	31181.961272	31.695194
600.843165	31227.472115	31.700212
601.919531	31265.569269	31.705229
602.094813	31323.948518	31.710247
602.698985	31360.740485	31.715264
603.432294	31408.421311	31.720282
603.907954	31473.962067	31.725300
604.575625	31514.143798	31.730317
605.215048	31573.770755	31.735335
605.990471	31611.762188	31.740352
606.418366	31671.003952	31.745370
607.165333	31711.550220	31.750388
607.971894	31772.464151	31.755405
608.525633	31811.942914	31.760423
608.988515	31863.679250	31.765440
609.438346	31922.897941	31.770458
610.227646	31965.725003	31.775476
610.872264	32007.691026	31.780493
611.333824	32072.509839	31.785511
612.058970	32125.261225	31.790528
612.602227	32173.274003	31.795546
613.379005	32235.105389	31.800564
613.802856	32286.991124	31.805581
614.258451	32341.192029	31.810599
615.145176	32401.216051	31.815616
615.862321	32459.978013	31.820634
616.555700	32501.882370	31.825652
617.245143	32553.447677	31.830669
617.677350	32609.907085	31.835687
618.244784	32661.903536	31.840704
619.019588	32710.796763	31.845722
619.643366	32769.653507	31.850740
620.393264	32826.786534	31.855757
620.723053	32884.740069	31.860775
621.280127	32930.322387	31.865792
621.923600	32987.638418	31.870810
622.480008	33039.157078	31.875828
623.365873	33074.752684	31.880845
623.827925	33140.132022	31.885863
624.591110	33198.075966	31.890880
625.498925	33244.705076	31.895898
625.876641	33301.385167	31.900916
626.719522	33352.958494	31.905933
627.217325	33403.538737	31.910951
628.013196	33440.274894	31.915968
628.700621	33502.374314	31.920986
629.106559	33548.281893	31.926004
630.069671	33613.244427	31.931021
630.030764	33666.663069	31.936039
630.738072	33713.412127	31.941056
631.369959	33764.995119	31.946074
632.220418	33812.522406	31.951092
633.165585	33872.737944	31.956109
633.297635	33921.688245	31.961127
633.904355	33967.153607	31.966144
634.421525	34029.018876	31.971162
635.035973	34078.769247	31.976180
636.030763	34104.414356	31.981197
635.923965	34172.156642	31.986215
637.033866	34227.544247	31.991232
637.504871	34259.765815	31.996250
638.360796	34318.751901	32.001268
638.809454	34379.921624	32.006285
639.196228	34425.404350	32.011303
639.749230	34487.125331	32.016320
640.383890	34553.026602	32.021338
640.711087	34601.468628	32.026356
641.959813	34667.951985	32.031373
642.423096	34735.268455	32.036391
643.021769	34790.535995	32.041408
643.788773	34850.258528	32.046426
644.271555	34899.111727	32.051444
645.054605	34966.510634	32.056461
645.540828	35021.226197	32.061479
646.238260	35090.456810	32.066496
647.117479	35147.449577	32.071514
647.827357	35212.594277	32.076532
648.534068	35269.015896	32.081549
649.248590	35335.744627	32.086567
650.000724	35379.931155	32.091584
650.592216	35423.999924	32.096602
650.791466	35519.984724	32.101620
651.703161	35554.881629	32.106637
652.591696	35618.730443	32.111655
653.044972	35672.986767	32.116672
653.837286	35733.815109	32.121690
654.337856	35797.597111	32.126708
655.128409	35850.039407	32.131725
655.897902	35918.407547	32.136743
656.549039	35968.085216	32.141760
657.263032	36029.540355	32.146778
658.058133	36093.569818	32.151796
658.510011	36145.056440	32.156813
659.260788	36195.075208	32.161831
660.014856	36249.955526	32.166848
660.596345	36308.024395	32.171866
660.916075	36372.788019	32.176884
661.996214	36417.033853	32.181901
662.311515	36473.755193	32.186919
662.795548	36546.658133	32.191936
663.721571	36609.182061	32.196954
664.417386	36668.723804	32.201972
665.132521	36727.289955	32.206989
665.750399	36790.535231	32.212007
666.179687	36857.843604	32.217024
666.730236	36903.794172	32.222042
667.158236	36971.828426	32.227060
668.163786	37035.686098	32.232077
668.646380	37105.887875	32.237095
668.786214	37166.486350	32.242112
670.103773	37221.371580	32.247130
670.900872	37282.504348	32.252148
671.711426	37334.328515	32.257165
672.213356	37391.245543	32.262183
672.795291	37442.579857	32.267200
673.324529	37496.263993	32.272218
674.001126	37560.406224	32.277236
674.834007	37615.336804	32.282253
675.321500	37662.166634	32.287271
676.045610	37730.606156	32.292288
676.664310	37792.693095	32.297306
677.182792	37857.779241	32.302324
677.941164	37933.373704	32.307341
678.394636	37998.554307	32.312359
678.910766	38053.683379	32.317376
680.058117	38127.966489	32.322394
679.909067	38210.486372	32.327412
680.864105	38269.845889	32.332429
681.434999	38340.432929	32.337447
681.820671	38422.247495	32.342464
682.847226	38496.292880	32.347482
683.524940	38580.970750	32.352500
684.533740	38656.104446	32.357517
685.097341	38726.697414	32.362535
685.857906	38795.356197	32.367552
686.978681	38857.105382	32.372570
687.345949	38945.919848	32.377588
688.539853	39002.691155	32.382605
689.171685	39064.665580	32.387623
689.675155	39137.819464	32.392640
690.512013	39200.423988	32.397658
690.957791	39265.035178	32.402676
691.590585	39344.025531	32.407693
692.132301	39421.993220	32.412711
692.853284	39490.407260	32.417728
693.752870	39557.659417	32.422746
694.101335	39631.935992	32.427764
695.219322	39699.256434	32.432781
696.244333	39772.123459	32.437799
696.590399	39841.434323	32.442816
697.575365	39911.015889	32.447834
698.291113	39982.490244	32.452852
698.573183	40049.114155	32.457869
699.560005	40104.834100	32.462887
700.271664	40178.831330	32.467904
701.322008	40252.754464	32.472922
701.449275	40326.313964	32.477940
702.135894	40386.590927	32.482957
703.082898	40453.468516	32.487975
703.366614	40531.151219	32.492992
704.341470	40597.678023	32.498010
704.841843	40674.396513	32.503028
705.730885	40745.456987	32.508045
706.307473	40816.215845	32.513063
706.813230	40882.328017	32.518080
707.915811	40939.946666	32.523098
707.967530	41011.092662	32.528116
708.979371	41079.471522	32.533133
709.752226	41148.197786	32.538151
710.603035	41218.179794	32.543168
711.138920	41275.587017	32.548186
711.783896	41344.902139	32.553204
712.371992	41421.651022	32.558221
712.989379	41490.939587	32.563239
713.436727	41566.841031	32.568256
714.564505	41636.824817	32.573274
714.969354	41724.214292	32.578292
715.745701	41793.863569	32.583309
716.543554	41861.699284	32.588327
717.385539	41947.585220	32.593344
718.110243	42017.978525	32.598362
718.628792	42088.168381	32.603380
719.412858	42164.618144	32.608397
720.264548	42244.444999	32.613415
720.669192	42333.408357	32.618432
721.527774	42397.883687	32.623450
722.177970	42491.372816	32.628468
723.016616	42570.074073	32.633485
724.153345	42638.937644	32.638503
724.571273	42722.564020	32.643520
725.467695	42797.434229	32.648538
726.054312	42876.530282	32.653556
726.749833	42949.379731	32.658573
727.329791	43029.960042	32.663591
727.960595	43123.345291	32.668608
729.133080	43200.870214	32.673626
729.543952	43286.601206	32.678644
730.156767	43361.724045	32.683661
731.542443	43437.478068	32.688679
732.281118	43513.912663	32.693696
732.840527	43596.132841	32.698714
733.533889	43668.622922	32.703732
734.089155	43749.746768	32.708749
735.061177	43819.716929	32.713767
735.871371	43913.358637	32.718784
736.968459	43979.700884	32.723802
737.620710	44062.823287	32.728820
738.001768	44135.929687	32.733837
738.944839	44205.505404	32.738855
739.814238	44290.714138	32.743872
740.442598	44368.214207	32.748890
741.415409	44443.221351	32.753908
742.187535	44513.374402	32.758925
743.059772	44578.319430	32.763943
743.603421	44654.960458	32.768960
744.354383	44716.584637	32.773978
744.777851	44793.163387	32.778996
745.354461	44871.569842	32.784013
745.970505	44944.389875	32.789031
746.599880	45022.864324	32.794048
747.333435	45092.429633	32.799066
747.959811	45171.766446	32.804084
748.680506	45227.595864	32.809101
749.747939	45318.122110	32.814119
750.222308	45403.771441	32.819136
751.263203	45474.213679	32.824154
752.256438	45557.796869	32.829172
752.454660	45638.434301	32.834189
753.419155	45701.570647	32.839207
753.850527	45789.613703	32.844224
754.928049	45863.692279	32.849242
755.680042	45947.252642	32.854260
756.162967	46031.054987	32.859277
756.943103	46097.834363	32.864295
757.718667	46187.553476	32.869312
758.711253	46254.968460	32.874330
759.437839	46338.900703	32.879348
759.730526	46431.534148	32.884365
760.640944	46512.683758	32.889383
761.197514	46606.803092	32.894400
762.002556	46691.292419	32.899418
763.199513	46782.714266	32.904436
763.591735	46867.352181	32.909453
764.667877	46958.428201	32.914471
765.160121	47049.095993	32.919488
766.080734	47135.790178	32.924506
766.846018	47222.711436	32.929524
767.405402	47321.232248	32.934541
768.136159	47396.464156	32.939559
769.166078	47485.004145	32.944576
769.903886	47584.040701	32.949594
770.670798	47670.995469	32.954612
771.661581	47759.773393	32.959629
772.440782	47842.899904	32.964647
773.282659	47945.562947	32.969664
774.011531	48023.706883	32.974682
774.890257	48102.565624	32.979700
775.417451	48205.598942	32.984717
776.390722	48296.348045	32.989735
777.096606	48379.804280	32.994752
777.900341	48466.441590	32.999770
778.679613	48559.371642	33.004788
779.514705	48650.223440	33.009805
780.821922	48729.982299	33.014823
781.286440	48824.601437	33.019840
782.077559	48892.229003	33.024858
783.003267	48975.097726	33.029876
783.428508	49076.300169	33.034893
784.352298	49152.240886	33.039911
785.143677	49244.131341	33.044928
785.820456	49327.442068	33.049946
786.357312	49417.146224	33.054964
787.069010	49515.279542	33.059981
788.062274	49599.276386	33.064999
788.797639	49686.192453	33.070016
789.473083	49772.790312	33.075034
790.283799	49851.440484	33.080052
790.706522	49936.801396	33.085069
791.556297	50011.694172	33.090087
792.374532	50108.526361	33.095104
793.307073	50184.858238	33.100122
794.084422	50271.009996	33.105140
794.638850	50345.231717	33.110157
796.198750	50441.338650	33.115175
796.554581	50530.809011	33.120192
797.490273	50611.036232	33.125210
798.488119	50716.543186	33.130228
798.644712	50800.060364	33.135245
799.888590	50878.822852	33.140263
800.563760	50970.860641	33.145280
801.259932	51060.636081	33.150298
801.946966	51140.867393	33.155316
802.634915	51248.039380	33.160333
803.471143	51344.818617	33.165351
804.165885	51450.333966	33.170368
804.832886	51544.935337	33.175386
806.173540	51631.095524	33.180404
807.072691	51721.239604	33.185421
808.057991	51820.020562	33.190439
808.584023	51915.201750	33.195456
809.411306	51993.581014	33.200474
810.472647	52100.326281	33.205492
811.384363	52177.638847	33.210509
812.082938	52278.651843	33.215527
813.002802	52357.185225	33.220544
813.527367	52462.014058	33.225562
814.734295	52550.197662	33.230580
815.247793	52645.946476	33.235597
815.922591	52728.831549	33.240615
816.713664	52836.290115	33.245632
817.738096	52923.933359	33.250650
818.739897	53020.016730	33.255668
819.333735	53112.296214	33.260685
820.209601	53202.157916	33.265703
821.257920	53295.527441	33.270720
821.641353	53397.493196	33.275738
822.793118	53490.560061	33.280756
823.860301	53584.941198	33.285773
824.731252	53662.594869	33.290791
825.641695	53751.857292	33.295808
826.383605	53832.912491	33.300826
827.525945	53920.620717	33.305844
828.052286	54021.633011	33.310861
828.873879	54105.144909	33.315879
830.021356	54198.654820	33.320896
830.515448	54288.194461	33.325914
831.570294	54359.496707	33.330932
832.024902	54446.054418	33.335949
832.841590	54527.186042	33.340967
833.569431	54619.773829	33.345984
834.322471	54711.139732	33.351002
835.214360	54784.284476	33.356020
835.846470	54872.902319	33.361037
836.576280	54955.144940	33.366055
837.582777	55038.196126	33.371072
838.410562	55140.757494	33.376090
839.215422	55210.316338	33.381108
839.733272	55305.800756	33.386125
840.588823	55400.805809	33.391143
841.337270	55502.895747	33.396160
842.026461	55599.926361	33.401178
843.156858	55686.249850	33.406196
844.025447	55803.419922	33.411213
845.009698	55879.622513	33.416231
845.906552	55974.930168	33.421248
846.671232	56075.881210	33.426266
848.017481	56161.661234	33.431284
848.310738	56258.739416	33.436301
849.368716	56352.634493	33.441319
850.289638	56453.408079	33.446336
850.973690	56538.597635	33.451354
852.029297	56633.656180	33.456372
852.852242	56733.853447	33.461389
853.592663	56822.353029	33.466407
854.719427	56918.042536	33.471424
855.412282	57015.802961	33.476442
856.375980	57107.273597	33.481460
856.984792	57204.265526	33.486477
857.917565	57295.798843	33.491495
859.086672	57396.383432	33.496512
859.945847	57493.504355	33.501530
860.950073	57585.223466	33.506548
861.502471	57682.722516	33.511565
862.426157	57773.293660	33.516583
863.740365	57866.000294	33.521600
864.201491	57963.824728	33.526618
865.101689	58048.128208	33.531636
865.877075	58145.370079	33.536653
867.023482	58248.434809	33.541671
867.898112	58333.315067	33.546688
868.558416	58434.930223	33.551706
869.643149	58524.289246	33.556724
870.203111	58619.017040	33.561741
871.270409	58722.494786	33.566759
872.269657	58807.117456	33.571776
872.805673	58907.343786	33.576794
873.979561	59004.602531	33.581812
874.935343	59098.439479	33.586829
875.375823	59207.904497	33.591847
876.692293	59291.238157	33.596864
877.553400	59386.859619	33.601882
878.667415	59465.244313	33.606900
879.322283	59560.403813	33.611917
880.035151	59652.709949	33.616935
880.986037	59735.557586	33.621952
881.549579	59831.105553	33.626970
882.632369	59913.730933	33.631988
883.553166	59995.375297	33.637005
884.386661	60081.157288	33.642023
885.019245	60170.700382	33.647040
885.723426	60263.898123	33.652058
886.579145	60350.533442	33.657076
887.383672	60446.968152	33.662093
888.263908	60537.139792	33.667111
889.378055	60638.887379	33.672128
889.803622	60735.301788	33.677146
890.671054	60839.969247	33.682164
891.486200	60947.468329	33.687181
892.621955	61054.724412	33.692199
893.669683	61156.122280	33.697216
894.162290	61264.356511	33.702234
895.075236	61369.123882	33.707252
895.586828	61475.714425	33.712269
896.639509	61588.133492	33.717287
897.884782	61700.822553	33.722304
898.573386	61810.348591	33.727322
899.404093	61920.234723	33.732340
900.823391	62035.484149	33.737357
901.662640	62132.452483	33.742375
902.580655	62239.487904	33.747392
903.435867	62348.027489	33.752410
904.386889	62455.602000	33.757428
905.541239	62568.146529	33.762445
906.313670	62667.812275	33.767463
907.577309	62776.245132	33.772480
907.923055	62881.556413	33.777498
909.196698	62982.252432	33.782516
910.027811	63084.244612	33.787533
910.926784	63194.348351	33.792551
912.170555	63300.914820	33.797568
912.739869	63419.999419	33.802586
913.886003	63510.607215	33.807604
914.675845	63622.183410	33.812621
915.417941	63730.928934	33.817639
916.722746	63835.063455	33.822656
917.385096	63946.333422	33.827674
918.246502	64045.654371	33.832692
919.272728	64160.256144	33.837709
920.492961	64263.174875	33.842727
921.393071	64360.587065	33.847744
922.536874	64468.410771	33.852762
923.444665	64570.231368	33.857780
924.415555	64666.436978	33.862797
925.187707	64771.646687	33.867815
926.271033	64871.315605	33.872832
927.405013	64979.301669	33.877850
928.279573	65069.281126	33.882868
928.843490	65181.878265	33.887885
929.727807	65279.894550	33.892903
930.669462	65372.400735	33.897920
931.320294	65470.429881	33.902938
932.397652	65564.434478	33.907956
933.862315	65640.512057	33.912973
934.392973	65740.058685	33.917991
935.660847	65827.733656	33.923008
936.376357	65907.317097	33.928026
937.414089	66009.655279	33.933044
938.392445	66090.407270	33.938061
939.190010	66183.758291	33.943079
939.858714	66280.667553	33.948096
940.744660	66373.260078	33.953114
941.774452	66484.603229	33.958132
942.707189	66575.357457	33.963149
943.372963	66676.738231	33.968167
944.933062	66767.444089	33.973184
945.650106	66883.005195	33.978202
946.456011	66974.890081	33.983220
947.291299	67086.984622	33.988237
948.176729	67184.141895	33.993255
949.238653	67290.048923	33.998272
949.596592	67404.217394	34.003290
950.745571	67514.473657	34.008308
951.780499	67618.785428	34.013325
952.510732	67736.620514	34.018343
953.817551	67849.411985	34.023360
954.559377	67958.333161	34.028378
955.607032	68073.618217	34.033396
956.662771	68184.682781	34.038413
957.263759	68312.838976	34.043431
958.811954	68416.921780	34.048448
959.350588	68541.551730	34.053466
960.204718	68650.515783	34.058484
961.383825	68762.132588	34.063501
961.908021	68892.629624	34.068519
963.270483	69001.413694	34.073536
964.331737	69123.955278	34.078554
965.061619	69239.980103	34.083572
966.125526	69348.661991	34.088589
966.969299	69476.477664	34.093607
968.432144	69579.367292	34.098624
969.657324	69702.063326	34.103642
970.838273	69806.098275	34.108660
972.245484	69915.670050	34.113677
973.312791	70012.515613	34.118695
974.324001	70112.371547	34.123712
975.370469	70209.992178	34.128730
976.150872	70305.065288	34.133748
976.785213	70405.658687	34.138765
977.607009	70524.348996	34.143783
978.810818	70609.279084	34.148800
979.759442	70728.196853	34.153818
980.557115	70827.976681	34.158836
981.767235	70947.782934	34.163853
982.592821	71049.069470	34.168871
983.513459	71135.828598	34.173888
984.031174	71246.711862	34.178906
984.886562	71334.929114	34.183924
986.322520	71437.573742	34.188941
986.891525	71546.605606	34.193959
987.858497	71642.754893	34.198976
988.647274	71748.081967	34.203994
989.260302	71861.341863	34.209012
990.436230	71974.512862	34.214029
991.039459	72091.535098	34.219047
991.617140	72216.441259	34.224064
992.717891	72325.159046	34.229082
993.821543	72469.576923	34.234100
994.712380	72582.506099	34.239117
995.848034	72704.982374	34.244135
997.091860	72833.773532	34.249152
997.938369	72973.206301	34.254170
998.664079	73093.412251	34.259188
999.883425	73222.955445	34.264205
1000.646060	73345.817272	34.269223
1001.904343	73476.215287	34.274240
1003.254891	73612.374995	34.279258
1003.726577	73720.372711	34.284276
1005.016672	73862.439353	34.289293
1005.598857	73997.283178	34.294311
1006.908183	74125.661542	34.299328
1007.850112	74262.472047	34.304346
1008.990043	74407.030920	34.309364
1010.395355	74521.393227	34.314381
1011.119274	74656.768727	34.319399
1012.414328	74777.260776	34.324416
1013.775932	74915.355001	34.329434
1014.625887	75044.204134	34.334452
1016.014319	75166.358310	34.339469
1017.215623	75284.656520	34.344487
1018.336888	75400.276049	34.349504
1019.036092	75520.134279	34.354522
1019.706681	75642.032680	34.359540
1021.463800	75761.370173	34.364557
1022.276243	75892.865995	34.369575
1023.425273	76013.982742	34.374592
1024.383755	76124.684001	34.379610
1025.537697	76246.408058	34.384628
1026.806574	76367.324592	34.389645
1027.626883	76485.109037	34.394663
1028.854162	76586.435661	34.399680
1029.827234	76715.806774	34.404698
1030.737526	76828.668330	34.409716
1032.103396	76935.327662	34.414733
1033.268005	77049.022154	34.419751
1034.151602	77167.211304	34.424768
1035.294117	77284.803791	34.429786
1036.059900	77398.936568	34.434804
1036.923094	77510.444263	34.439821
1037.568948	77628.035573	34.444839
1038.928630	77733.701498	34.449856
1040.080971	77844.495090	34.454874
1040.625583	77966.844665	34.459892
1041.751943	78070.147734	34.464909
1042.546898	78179.009084	34.469927
1043.247920	78290.787023	34.474944
1044.549771	78406.445568	34.479962
1045.586907	78525.932842	34.484980
1046.605280	78635.614357	34.489997
1047.281886	78772.086762	34.495015
1048.584451	78883.645856	34.500032
1049.984584	78996.688029	34.505050
1050.421163	79134.123835	34.510068
1051.837020	79254.838227	34.515085
1052.716391	79374.709511	34.520103
1053.789927	79505.782642	34.525120
1054.922511	79641.176983	34.530138
1055.931791	79761.674588	34.535156
1056.670277	79893.315471	34.540173
1057.865085	80033.803471	34.545191
1058.682895	80160.029035	34.550208
1060.071800	80287.795364	34.555226
1061.040920	80429.105762	34.560244
1062.538456	80561.989220	34.565261
1063.353323	80700.127527	34.570279
1064.296905	80828.347302	34.575296
1065.329700	80959.613157	34.580314
1066.658548	81102.602965	34.585332
1067.518666	81230.838508	34.590349
1068.692602	81374.120324	34.595367
1069.710391	81498.564920	34.600384
1071.177683	81635.480494	34.605402
1072.027006	81783.210161	34.610420
1073.048353	81917.733145	34.615437
1074.248594	82047.158655	34.620455
1075.089477	82172.539407	34.625472
1076.308709	82321.351952	34.630490
1077.015780	82465.006335	34.635508
1078.212730	82600.713245	34.640525
1079.133807	82745.321711	34.645543
1080.515070	82882.562618	34.650560
1081.648746	83023.485191	34.655578
1082.554825	83169.262196	34.660596
1083.917344	83309.663516	34.665613
1084.631745	83448.455596	34.670631
1085.920680	83589.926268	34.675648
1087.154175	83730.875658	34.680666
1088.214246	83882.215516	34.685684
1089.335182	84015.402197	34.690701
1090.205997	84167.185146	34.695719
1091.370861	84306.663596	34.700736
1092.968346	84436.799383	34.705754
1093.486922	84589.741471	34.710772
1094.885968	84716.338429	34.715789
1096.269970	84858.965834	34.720807
1097.232423	84996.647542	34.725824
1097.931851	85116.289667	34.730842
1099.219742	85241.048640	34.735860
1100.348328	85360.952671	34.740877
1100.905754	85492.733527	34.745895
1102.283070	85622.146601	34.750912
1103.515024	85753.347608	34.755930
1104.289680	85894.845979	34.760948
1105.516798	86023.532985	34.765965
1106.624620	86168.818108	34.770983
1107.879483	86298.090385	34.776000
1109.132416	86440.799865	34.781018
1109.956382	86580.473965	34.786036
1110.923136	86713.664209	34.791053
1111.796368	86852.162506	34.796071
1112.733584	87007.293772	34.801088
1114.170394	87155.403963	34.806106
1114.956704	87308.367300	34.811124
1116.269913	87448.747019	34.816141
1117.740004	87589.703417	34.821159
1118.949008	87744.196098	34.826176
1119.948681	87883.793857	34.831194
1121.265007	88023.854360	34.836212
1122.151621	88173.677862	34.841229
1123.064711	88314.259665	34.846247
1124.210685	88476.684571	34.851264
1125.476563	88619.798570	34.856282
1126.683181	88768.152529	34.861300
1127.523153	88928.833610	34.866317
1128.867468	89071.678867	34.871335
1129.705396	89237.332957	34.876352
1131.001961	89392.070159	34.881370
1131.900178	89547.270211	34.886388
1133.521282	89704.791098	34.891405
1134.718306	89861.634349	34.896423
1135.819356	90010.197005	34.901440
1137.174136	90154.616076	34.906458
1138.577006	90303.980159	34.911476
1139.654554	90462.895729	34.916493
1140.718357	90606.845500	34.921511
1141.813368	90751.063198	34.926528
1142.716453	90900.251554	34.931546
1144.047877	91065.980241	34.936564
1145.209962	91208.014757	34.941581
1146.394309	91365.111174	34.946599
1147.436141	91513.427870	34.951616
1148.886075	91658.347718	34.956634
1150.111966	91820.468695	34.961652
1151.109751	91958.398016	34.966669
1152.564109	92113.970613	34.971687
1153.644683	92272.822957	34.976704
1154.665025	92403.788128	34.981722
1155.758661	92561.400853	34.986740
1157.179920	92712.258425	34.991757
1158.293867	92851.484089	34.996775
1159.260237	92990.809995	35.001792
1160.474835	93115.872787	35.006810
1161.035464	93251.912701	35.011828
1162.054396	93395.609603	35.016845
1163.185235	93545.741085	35.021863
1164.341232	93683.706642	35.026880
1165.479756	93832.725650	35.031898
1166.697192	93984.459215	35.036916
1167.905734	94137.340077	35.041933
1168.623674	94275.910278	35.046951
1169.632770	94437.699104	35.051968
1170.994566	94597.396298	35.056986
1172.056553	94759.356158	35.062004
1173.218489	94915.627479	35.067021
1174.539785	95076.852626	35.072039
1175.624884	95244.600052	35.077056
1177.031899	95403.201525	35.082074
1177.912654	95581.092065	35.087092
1179.074756	95737.818217	35.092109
1180.444272	95897.719569	35.097127
1181.647161	96079.143134	35.102144
1183.088034	96229.167475	35.107162
1184.559714	96388.119872	35.112180
1185.746207	96553.691233	35.117197
1186.859553	96714.006018	35.122215
1187.971047	96864.789134	35.127232
1189.536984	97026.773799	35.132250
1190.359733	97195.121523	35.137268
1191.625584	97352.949468	35.142285
1193.199480	97514.683325	35.147303
1193.916764	97674.258156	35.152320
1195.119827	97834.016246	35.157338
1196.338829	98001.142945	35.162356
1197.746595	98165.159981	35.167373
1199.095362	98335.830185	35.172391
1200.185544	98501.171721	35.177408
1201.434881	98643.416853	35.182426
1202.534287	98817.053093	35.187444
1203.650998	98993.515836	35.192461
1205.124993	99154.910309	35.197479
1206.044897	99325.706714	35.202496
1207.278500	99488.799322	35.207514
1208.289629	99659.147174	35.212532
1209.487814	99829.612066	35.217549
1210.710431	100005.698819	35.222567
1212.429256	100172.458255	35.227584
1213.416675	100349.768147	35.232602
1213.944150	100532.751830	35.237620
1215.359969	100697.861309	35.242637
1216.892333	100871.115255	35.247655
1217.824984	101038.189427	35.252672
1219.316130	101226.378068	35.257690
1220.703421	101403.923529	35.262708
1221.964939	101565.729340	35.267725
1222.953732	101743.555879	35.272743
1223.755915	101900.198105	35.277760
1225.481862	102062.015797	35.282778
1226.425399	102228.147713	35.287796
1227.524588	102391.978203	35.292813
1229.144147	102540.237535	35.297831
1229.961562	102709.082092	35.302848
1231.053560	102869.031999	35.307866
1232.282004	103037.256761	35.312884
1233.518132	103214.865377	35.317901
1234.956566	103380.667383	35.322919
1235.758071	103552.678063	35.327936
1237.267718	103721.217385	35.332954
1237.902025	103914.278124	35.337972
1239.381782	104092.930383	35.342989
1240.971728	104257.265413	35.348007
1241.649948	104437.579062	35.353024
1243.357288	104632.310208	35.358042
1244.649507	104819.028025	35.363060
1245.828624	105000.424377	35.368077
1247.473866	105161.434658	35.373095
1248.323745	105357.915440	35.378112
1249.542092	105536.158214	35.383130
1250.798101	105712.966144	35.388148
1252.126251	105904.072304	35.393165
1253.261398	106086.091464	35.398183
1254.621689	106266.234648	35.403200
1255.894178	106468.827653	35.408218
1257.115824	106654.552227	35.413236
1258.835873	106835.313343	35.418253
1260.103392	107020.172777	35.423271
1261.185494	107214.708035	35.428288
1262.688237	107397.912846	35.433306
1263.802866	107574.719059	35.438324
1265.019094	107768.781812	35.443341
1266.510369	107945.954914	35.448359
1267.945094	108139.004942	35.453376
1269.267359	108325.732751	35.458394
1270.749834	108508.904938	35.463412
1271.685067	108678.925073	35.468429
1273.249673	108868.719802	35.473447
1274.355468	109060.304157	35.478464
1275.892039	109227.738862	35.483482
1277.222633	109411.872416	35.488500
1278.151052	109606.514665	35.493517
1279.655319	109778.471104	35.498535
1281.207234	109968.497975	35.503552
1282.189959	110127.260677	35.508570
1283.746008	110318.492213	35.513588
1284.872568	110497.311644	35.518605
1286.209863	110677.630647	35.523623
1287.209094	110860.897359	35.528640
1289.086528	111030.081549	35.533658
1290.305432	111205.663332	35.538676
1291.286917	111389.911592	35.543693
1293.136951	111547.551863	35.548711
1294.316917	111720.383709	35.553728
1295.337400	111874.030857	35.558746
1296.304158	112041.100650	35.563764
1297.886216	112203.098403	35.568781
1299.072396	112373.389180	35.573799
1299.921773	112531.061858	35.578816
1301.524662	112708.549296	35.583834
1302.299105	112883.973118	35.588852
1303.462122	113057.285429	35.593869
1304.946805	113239.625399	35.598887
1305.824964	113429.172032	35.603904
1307.116051	113616.198300	35.608922
1308.520709	113804.879143	35.613940
1309.643272	113985.180432	35.618957
1310.898818	114176.666846	35.623975
1312.011659	114380.389011	35.628992
1313.745811	114573.144459	35.634010
1315.508534	114762.832821	35.639028
1316.214003	114954.507562	35.644045
1317.665511	115151.503285	35.649063
1319.062540	115354.409498	35.654080
1320.321368	115549.735978	35.659098
1321.838434	115741.452308	35.664116
1322.847891	115941.854504	35.669133
1324.594140	116144.964800	35.674151
1325.758844	116337.703959	35.679168
1327.226239	116545.432787	35.684186
1328.551450	116734.293818	35.689204
1329.764193	116936.539240	35.694221
1331.211202	117142.465465	35.699239
1332.425851	117338.775083	35.704256
1333.959242	117539.385172	35.709274
1335.492790	117745.353156	35.714292
1336.684222	117941.664760	35.719309
1338.351138	118144.714965	35.724327
1339.408668	118349.180585	35.729344
1340.877899	118545.117082	35.734362
1342.114543	118748.449382	35.739380
1343.280046	118956.328073	35.744397
1344.800881	119153.919896	35.749415
1345.811782	119362.345626	35.754432
1347.164556	119568.515225	35.759450
1348.370436	119783.935354	35.764468
1349.832948	120001.975898	35.769485
1351.230840	120196.131642	35.774503
1352.869605	120414.324928	35.779520
1354.101303	120613.601153	35.784538
1355.603743	120825.056882	35.789556
1356.642301	121034.397110	35.794573
1358.292112	121244.629698	35.799591
1359.646432	121448.679969	35.804608
1361.225895	121670.325262	35.809626
1362.684063	121865.509667	35.814644
1363.845689	122090.099804	35.819661
1365.564063	122266.489163	35.824679
1366.674876	122474.106945	35.829696
1367.873229	122666.615587	35.834714
1369.098189	122843.568490	35.839732
1370.569184	123049.157772	35.844749
1371.818870	123238.787386	35.849767
1373.334280	123437.127997	35.854784
1374.674955	123621.920326	35.859802
1376.174894	123820.253589	35.864820
1377.142838	124019.977447	35.869837
1378.679348	124201.297579	35.874855
1379.939913	124411.072567	35.879872
1381.234892	124621.920348	35.884890
1382.561337	124811.092968	35.889908
1383.602046	125026.835482	35.894925
1384.722971	125242.908972	35.899943
1386.485877	125466.722726	35.904960
1387.952405	125680.034179	35.909978
1389.165096	125888.890986	35.914996
1390.484024	126106.295264	35.920013
1391.756167	126339.554989	35.925031
1392.819240	126565.465089	35.930048
1394.018457	126796.054925	35.935066
1396.078356	127013.019380	35.940084
1397.012029	127253.181020	35.945101
1398.581187	127472.659242	35.950119
1400.412580	127713.657671	35.955136
1401.504406	127928.300404	35.960154
1403.179881	128148.869241	35.965172
1404.713255	128384.955187	35.970189
1406.229793	128604.514179	35.975207
1407.883084	128835.289740	35.980224
1408.817873	129060.924125	35.985242
1410.712531	129287.978691	35.990260
1412.237993	129518.881625	35.995277
1413.661540	129737.184898	36.000295
1415.330729	129962.595921	36.005312
1416.587845	130193.065701	36.010330
1418.199739	130407.594392	36.015348
1419.446774	130634.205454	36.020365
1421.107041	130847.893701	36.025383
1422.690696	131070.654130	36.030400
1423.682017	131290.026433	36.035418
1425.212219	131512.773532	36.040436
1426.638341	131743.507961	36.045453
1428.206401	131964.643618	36.050471
1429.504736	132191.043726	36.055488
1430.877652	132414.608465	36.060506
1432.268716	132641.022786	36.065524
1433.719660	132872.028563	36.070541
1435.188706	133101.626979	36.075559
1436.826579	133315.552896	36.080576
1437.694082	133556.260849	36.085594
1439.461710	133775.997887	36.090612
1440.875459	134015.850040	36.095629
1442.270351	134240.363254	36.100647
1443.553518	134449.767321	36.105664
1444.769257	134662.959487	36.110682
1446.516398	134874.294898	36.115700
1447.906106	135093.151782	36.120717
1449.607797	135296.679605	36.125735
1451.038050	135519.144499	36.130752
1452.298099	135736.493669	36.135770
1454.093127	135947.233793	36.140788
1455.339951	136153.108065	36.145805
1456.614789	136372.258979	36.150823
1458.131488	136595.706772	36.155840
1459.421208	136821.447887	36.160858
1460.802546	137030.943749	36.165876
1462.037414	137269.280035	36.170893
1463.816479	137494.530434	36.175911
1465.294062	137714.875716	36.180928
1466.938422	137945.612610	36.185946
1467.923344	138178.382255	36.190964
1469.204725	138410.739142	36.195981
1470.863079	138645.737185	36.200999
1472.556049	138885.889301	36.206016
1473.898596	139111.069344	36.211034
1475.517552	139356.344084	36.216052
1476.995756	139598.880541	36.221069
1478.548061	139828.214717	36.226087
1480.156851	140055.564696	36.231104
1481.113968	140310.216391	36.236122
1483.041127	140551.092449	36.241140
1484.205089	140782.713450	36.246157
1485.627761	141029.084990	36.251175
1487.364664	141270.478633	36.256192
1488.834025	141527.885458	36.261210
1490.316810	141755.078216	36.266228
1492.081271	142010.541213	36.271245
1493.826953	142245.591672	36.276263
1495.513250	142482.744597	36.281280
1496.587194	142731.466720	36.286298
1498.377683	142963.118945	36.291316
1500.025407	143206.810850	36.296333
1501.386816	143460.867152	36.301351
1502.968865	143689.592180	36.306368
1504.512726	143944.016408	36.311386
1506.078096	144167.741174	36.316404
1507.375939	144419.153806	36.321421
1508.435758	144657.259619	36.326439
1510.091500	144897.072447	36.331456
1511.414850	145161.922568	36.336474
1513.201664	145408.157482	36.341492
1514.664892	145653.076816	36.346509
1516.246115	145906.243699	36.351527
1517.679951	146159.841664	36.356544
1519.128885	146413.502663	36.361562
1521.082321	146653.294390	36.366580
1522.367284	146915.199355	36.371597
1524.003498	147150.228453	36.376615
1525.874751	147374.713557	36.381632
1526.921886	147613.110087	36.386650
1528.618290	147835.686796	36.391668
1529.547136	148065.092747	36.396685
1531.175723	148291.397576	36.401703
1532.692292	148531.399714	36.406720
1534.179300	148775.350765	36.411738
1536.027866	148996.060644	36.416756
1537.328643	149243.556282	36.421773
1538.663745	149484.278943	36.426791
1540.741675	149706.871488	36.431808
1542.076744	149966.283564	36.436826
1543.664462	150207.706776	36.441844
1544.903199	150451.481803	36.446861
1546.356911	150686.046141	36.451879
1547.928766	150949.117585	36.456896
1549.111171	151201.515161	36.461914
1550.932267	151449.959247	36.466932
1552.319631	151717.655498	36.471949
1553.980597	151972.810153	36.476967
1555.664460	152221.801692	36.481984
1556.861195	152494.732510	36.487002
1558.259886	152769.535230	36.492020
1560.072890	153019.311011	36.497037
1561.889606	153291.376571	36.502055
1563.334634	153548.720364	36.507072
1564.592742	153822.324345	36.512090
1566.535162	154081.203429	36.517108
1568.220373	154348.873694	36.522125
1569.312988	154624.285559	36.527143
1571.529269	154890.823467	36.532160
1572.777464	155165.961488	36.537178
1574.264980	155437.196610	36.542196
1575.712305	155718.558328	36.547213
1577.221036	155977.533597	36.552231
1579.079386	156254.460116	36.557248
1580.760850	156539.861564	36.562266
1582.940070	156809.603060	36.567284
1584.313724	157081.947185	36.572301
1585.674659	157358.720765	36.577319
1587.807527	157612.714912	36.582336
1589.180230	157897.124291	36.587354
1590.801982	158157.366142	36.592372
1592.707094	158425.731026	36.597389
1594.200173	158696.991149	36.602407
1596.248806	158956.169466	36.607424
1597.723401	159226.384185	36.612442
1599.244569	159484.927424	36.617460
1601.013893	159749.811569	36.622477
1602.524171	160011.289679	36.627495
1604.017228	160265.430225	36.632512
1605.621667	160530.536668	36.637530
1607.341075	160791.264549	36.642548
1609.051240	161057.981347	36.647565
1611.090257	161316.011971	36.652583
1612.654992	161551.572314	36.657600
1614.095838	161794.547181	36.662618
1615.507767	162029.310660	36.667636
1617.081235	162268.463233	36.672653
1618.385401	162508.535212	36.677671
1620.403525	162750.131365	36.682688
1621.434458	162991.518146	36.687706
1623.353387	163238.472406	36.692724
1624.932014	163492.279983	36.697741
1625.802392	163750.792752	36.702759
1627.780355	164002.612802	36.707776
1628.834509	164269.039155	36.712794
1630.607474	164536.532768	36.717812
1632.263345	164791.833680	36.722829
1633.310276	165072.369990	36.727847
1635.195454	165342.870138	36.732864
1636.787852	165635.562931	36.737882
1638.209448	165903.832549	36.742900
1639.986575	166190.653594	36.747917
1641.543844	166469.115570	36.752935
1643.462367	166757.478562	36.757952
1645.217808	167041.950551	36.762970
1646.869362	167321.469321	36.767988
1648.455152	167600.252296	36.773005
1650.204339	167902.374521	36.778023
1652.126138	168171.735219	36.783040
1653.461850	168460.089702	36.788058
1655.435564	168744.476492	36.793076
1657.052603	169034.363467	36.798093
1658.624225	169326.149784	36.803111
1660.425221	169602.084787	36.808128
1662.125034	169891.889027	36.813146
1663.556217	170179.594461	36.818164
1665.725598	170476.507877	36.823181
1667.094021	170771.343658	36.828199
1668.823124	171060.936403	36.833216
1670.154653	171355.934704	36.838234
1672.035015	171648.907317	36.843252
1673.695178	171935.194097	36.848269
1675.425816	172237.492930	36.853287
1677.322355	172524.685174	36.858304
1678.770634	172827.705692	36.863322
1680.731445	173119.902719	36.868340
1682.796400	173414.939576	36.873357
1684.245226	173715.378986	36.878375
1685.519682	173995.449962	36.883392
1687.106405	174312.084120	36.888410
1689.323371	174601.435133	36.893428
1690.813861	174899.022524	36.898445
1692.066349	175201.952625	36.903463
1693.835651	175495.085434	36.908480
1695.688023	175793.852500	36.913498
1697.026137	176099.211446	36.918516
1699.066237	176409.408882	36.923533
1701.107141	176709.142254	36.928551
1702.992229	176987.043720	36.933568
1704.555750	177259.213040	36.938586
1706.188013	177540.127040	36.943604
1707.888994	177813.699095	36.948621
1709.190464	178092.943967	36.953639
1710.939111	178357.618566	36.958656
1712.448413	178659.391575	36.963674
1714.135127	178946.040949	36.968692
1715.982687	179220.969165	36.973709
1717.468644	179522.244597	36.978727
1719.253757	179817.448187	36.983744
1721.064876	180109.262159	36.988762
1722.649729	180424.535243	36.993780
1724.097419	180716.322265	36.998797
1725.769588	181022.171685	37.003815
1727.824934	181329.890995	37.008832
1729.435359	181636.338228	37.013850
1731.002734	181942.299639	37.018868
1732.888509	182240.993148	37.023885
1734.375272	182558.758922	37.028903
1736.389761	182869.071352	37.033920
1738.373607	183180.583553	37.038938
1740.126094	183490.980049	37.043956
1741.893019	183802.493029	37.048973
1743.521649	184120.742436	37.053991
1745.291361	184429.975439	37.059008
1747.022852	184745.053501	37.064026
1748.698077	185061.056318	37.069044
1750.641210	185368.821758	37.074061
1752.259965	185699.125809	37.079079
1754.226501	186009.366277	37.084096
1756.280533	186326.053801	37.089114
1758.423407	186645.292671	37.094132
1760.437718	186947.207764	37.099149
1761.905471	187260.835191	37.104167
1763.747885	187567.679803	37.109184
1765.775291	187874.091022	37.114202
1767.553902	188181.533568	37.119220
1769.424117	188477.415864	37.124237
1771.296224	188785.989650	37.129255
1772.842621	189104.769176	37.134272
1774.494830	189404.727370	37.139290
1776.039675	189715.998762	37.144308
1778.057619	190027.146341	37.149325
1779.687378	190342.621535	37.154343
1781.397399	190654.418549	37.159360
1783.305926	190965.196228	37.164378
1785.055316	191291.889789	37.169396
1787.223533	191596.500781	37.174413
1789.062694	191908.894591	37.179431
1790.478605	192219.111324	37.184448
1792.474004	192531.293974	37.189466
1794.030392	192844.690495	37.194484
1795.902120	193143.901117	37.199501
1797.437479	193463.168193	37.204519
1799.289046	193768.807527	37.209536
1801.150961	194053.849125	37.214554
1802.550365	194358.282040	37.219572
1804.555851	194648.672701	37.224589
1806.403971	194951.020056	37.229607
1808.062848	195247.205767	37.234624
1809.933698	195548.093562	37.239642
1811.526939	195846.983837	37.244660
1813.697829	196141.468959	37.249677
1815.016165	196458.492303	37.254695
1817.090453	196761.030299	37.259712
1818.726575	197065.860731	37.264730
1820.520402	197378.816274	37.269748
1822.460675	197689.656247	37.274765
1824.139471	198008.776868	37.279783
1826.001061	198326.575801	37.284800
1828.046240	198641.859801	37.289818
1829.453081	198953.540794	37.294836
1831.668460	199276.099758	37.299853
1833.464000	199605.390964	37.304871
1835.291606	199925.870350	37.309888
1836.999258	200246.256456	37.314906
1838.584265	200580.549956	37.319924
1840.540751	200900.811602	37.324941
1842.309116	201235.486213	37.329959
1844.134419	201567.742147	37.334976
1846.378802	201906.381725	37.339994
1848.287456	202238.476168	37.345012
1850.188567	202567.768572	37.350029
1852.154668	202902.320386	37.355047
1854.096026	203232.816211	37.360064
1855.967646	203556.648232	37.365082
1857.596356	203908.332457	37.370100
1859.487585	204226.135720	37.375117
1861.592380	204568.723243	37.380135
1863.356466	204899.206161	37.385152
1865.222045	205242.978132	37.390170
1866.888102	205582.988305	37.395188
1869.490676	205907.999747	37.400205
1871.121218	206255.966000	37.405223
1872.850969	206584.052084	37.410240
1875.220621	206905.742066	37.415258
1876.883923	207255.740126	37.420276
1878.945912	207583.563231	37.425293
1880.732252	207918.616985	37.430311
1882.757217	208252.339893	37.435328
1884.561832	208582.773617	37.440346
1886.372102	208931.387112	37.445364
1888.185688	209248.315835	37.450381
1889.705516	209599.251608	37.455399
1891.612598	209942.282450	37.460416
1893.720929	210272.334340	37.465434
1895.310052	210615.901781	37.470452
1897.353763	210966.952590	37.475469
1898.990666	211302.175497	37.480487
1900.836687	211614.985203	37.485504
1902.899507	211945.929097	37.490522
1904.903605	212282.673140	37.495540
1906.804125	212590.692815	37.500557
1908.403762	212906.810685	37.505575
1910.372048	213228.394187	37.510592
1912.266346	213553.431547	37.515610
1913.816309	213882.816323	37.520628
1915.597626	214233.152190	37.525645
1918.122785	214552.241618	37.530663
1919.797155	214889.546584	37.535680
1921.598381	215227.252089	37.540698
1923.241892	215562.318147	37.545716
1925.456180	215902.297565	37.550733
1927.350349	216247.166726	37.555751
1929.195489	216587.474759	37.560768
1931.181599	216939.747423	37.565786
1932.775459	217293.721956	37.570804
1934.975583	217639.908047	37.575821
1936.883271	218003.053993	37.580839
1938.594690	218353.612569	37.585856
1940.557472	218708.551421	37.590874
1942.577524	219073.691092	37.595892
1944.689962	219434.970846	37.600909
1946.741295	219800.045755	37.605927
1948.433962	220176.758968	37.610944
1950.738665	220514.067260	37.615962
1952.634977	220885.533354	37.620980
1954.737235	221245.744424	37.625997
1956.565130	221613.479376	37.631015
1958.892118	221964.490920	37.636032
1960.790818	222331.926109	37.641050
1962.742163	222734.602465	37.646068
1964.660760	223118.595584	37.651085
1966.693913	223489.392488	37.656103
1968.740539	223856.608328	37.661120
1970.955699	224220.205739	37.666138
1972.854436	224589.137240	37.671156
1974.693678	224954.422962	37.676173
1977.007078	225311.660944	37.681191
1979.141120	225675.976242	37.686208
1981.258948	226031.356462	37.691226
1983.198777	226409.140174	37.696244
1985.383731	226764.233565	37.701261
1987.505854	227125.712848	37.706279
1989.365387	227491.070172	37.711296
1991.339193	227843.687432	37.716314
1993.437408	228207.994137	37.721332
1995.370027	228565.319244	37.726349
1997.551901	228918.593633	37.731367
1999.276471	229283.573684	37.736384
2001.373970	229641.105632	37.741402
2003.310781	229999.121667	37.746420
2005.408476	230359.577128	37.751437
2007.558826	230709.308121	37.756455
2008.993314	231049.071363	37.761472
2011.182628	231383.382697	37.766490
2013.046850	231712.387986	37.771508
2014.561303	232065.374331	37.776525
2016.513115	232408.463781	37.781543
2018.819279	232745.606020	37.786560
2020.860436	233095.795139	37.791578
2022.481223	233451.334981	37.796596
2024.776151	233793.867053	37.801613
2026.778077	234155.165146	37.806631
2028.244327	234514.949475	37.811648
2030.503568	234865.719952	37.816666
2032.414573	235221.931346	37.821684
2034.408608	235597.255807	37.826701
2036.507810	235963.751710	37.831719
2038.452161	236343.582336	37.836736
2040.696195	236707.746653	37.841754
2042.770829	237085.527442	37.846772
2044.638683	237454.579795	37.851789
2046.701524	237837.902091	37.856807
2048.540475	238229.084170	37.861824
2050.577724	238604.031580	37.866842
2052.655295	238990.073323	37.871860
2054.909743	239376.189955	37.876877
2056.823529	239768.610204	37.881895
2058.772849	240160.721386	37.886912
2061.078777	240541.779350	37.891930
2062.919335	240946.432441	37.896948
2064.997688	241334.742602	37.901965
2067.450952	241725.966346	37.906983
2069.148705	242136.945319	37.912000
2071.620380	242524.663564	37.917018
2073.621214	242921.830340	37.922036
2075.824487	243320.185486	37.927053
2077.868599	243717.195535	37.932071
2080.292399	244127.354749	37.937088
2082.823149	244518.600442	37.942106
2084.872252	244917.569241	37.947124
2086.826188	245304.666904	37.952141
2089.294564	245690.490267	37.957159
2091.088926	246084.981662	37.962176
2093.169275	246472.291228	37.967194
2095.426187	246867.702128	37.972212
2097.521611	247260.904478	37.977229
2099.725548	247654.598722	37.982247
2101.679181	248047.520907	37.987264
2104.041547	248426.484930	37.992282
2106.188378	248824.153945	37.997300
2108.068535	249217.217884	38.002317
2110.496956	249601.432438	38.007335
2112.546594	249994.750897	38.012352
2115.022825	250390.034791	38.017370
2116.884305	250773.046653	38.022388
2118.783109	251164.258190	38.027405
2120.624268	251549.535828	38.032423
2122.654823	251922.896349	38.037440
2124.818719	252282.799049	38.042458
2126.903189	252652.977399	38.047476
2128.727499	253036.609939	38.052493
2131.338752	253404.547165	38.057511
2133.182404	253773.292728	38.062528
2135.091515	254143.705176	38.067546
2137.184735	254522.065385	38.072564
2139.299568	254903.826792	38.077581
2141.251278	255284.522529	38.082599
2142.874645	255679.877306	38.087616
2145.231731	256062.517007	38.092634
2147.441904	256475.536402	38.097652
2149.106798	256877.186650	38.102669
2151.725099	257269.363792	38.107687
2153.533961	257681.991913	38.112704
2155.356157	258091.265559	38.117722
2157.768616	258508.016267	38.122740
2159.795783	258919.875326	38.127757
2161.787046	259340.758696	38.132775
2163.749436	259770.589082	38.137792
2166.208033	260194.879940	38.142810
2168.665440	260613.583087	38.147828
2170.805805	261045.927631	38.152845
2173.443844	261474.916978	38.157863
2175.259480	261903.961183	38.162880
2177.486978	262332.077010	38.167898
2179.447059	262762.090264	38.172916
2181.925812	263191.208972	38.177933
2184.076683	263622.336275	38.182951
2186.186658	264061.955220	38.187968
2188.962336	264503.298180	38.192986
2190.802074	264937.296201	38.198004
2192.982052	265371.266179	38.203021
2195.561601	265796.891873	38.208039
2197.688018	266239.940205	38.213056
2199.770596	266669.786314	38.218074
2202.277295	267109.523636	38.223092
2204.455129	267547.078040	38.228109
2207.381409	267962.616583	38.233127
2209.405677	268403.879555	38.238144
2211.661727	268830.219820	38.243162
2214.156367	269253.753613	38.248180
2216.204393	269694.073885	38.253197
2218.803822	270113.400094	38.258215
2220.944769	270539.454923	38.263232
2223.143087	270963.951290	38.268250
2225.753541	271382.997018	38.273268
2228.009879	271809.389855	38.278285
2230.543772	272223.799281	38.283303
2232.154764	272646.128628	38.288320
2234.622673	273064.130691	38.293338
2236.865434	273479.602831	38.298356
2239.095273	273904.755821	38.303373
2241.329147	274304.555657	38.308391
2243.246000	274702.119513	38.313408
2245.764362	275094.481962	38.318426
2247.744509	275484.694275	38.323444
2250.013970	275880.652713	38.328461
2252.275342	276269.626496	38.333479
2254.240856	276665.988760	38.338496
2256.289364	277064.954389	38.343514
2258.749591	277464.235749	38.348532
2260.495838	277875.341214	38.353549
2262.732470	278278.442991	38.358567
2264.865247	278696.955596	38.363584
2266.473999	279116.592699	38.368602
2268.898342	279536.938672	38.373620
2270.994655	279976.617648	38.378637
2273.494030	280408.001845	38.383655
2275.636692	280851.712203	38.388672
2278.091335	281286.862748	38.393690
2280.830558	281716.379202	38.398708
2283.091114	282154.227350	38.403725
2285.278705	282589.317815	38.408743
2287.631753	283026.083758	38.413760
2289.633987	283464.302163	38.418778
2292.086392	283906.411749	38.423796
2294.254901	284360.708684	38.428813
2296.877022	284795.652278	38.433831
2299.041357	285255.791742	38.438848
2300.901211	285706.935479	38.443866
2303.437361	286149.004229	38.448884
2305.675058	286614.693840	38.453901
2308.215692	287064.457968	38.458919
2310.361304	287537.096053	38.463936
2313.021474	287985.976376	38.468954
2315.716344	288431.599029	38.473972
2318.159873	288902.333568	38.478989
2320.792786	289346.669222	38.484007
2322.821686	289802.709059	38.489024
2325.295629	290251.895102	38.494042
2328.237111	290691.962952	38.499060
2330.246771	291147.444827	38.504077
2332.573877	291592.511327	38.509095
2335.019244	292041.063881	38.514112
2337.681930	292489.479583	38.519130
2339.943393	292933.893665	38.524148
2341.967121	293392.061937	38.529165
2344.436821	293841.445593	38.534183
2346.761696	294290.952927	38.539200
2349.114527	294740.556531	38.544218
2351.524876	295196.576856	38.549236
2353.851315	295644.557002	38.554253
2356.007984	296099.269254	38.559271
2358.956417	296549.917664	38.564288
2360.963860	297007.725156	38.569306
2363.534852	297457.593034	38.574324
2365.631679	297897.907676	38.579341
2368.190807	298335.988843	38.584359
2370.454879	298769.263981	38.589376
2372.532492	299197.741293	38.594394
2374.911698	299615.043829	38.599412
2376.901095	300053.871488	38.604429
2379.497508	300475.735183	38.609447
2381.599294	300899.632115	38.614464
2384.164701	301324.368919	38.619482
2386.261942	301758.399484	38.624500
2388.514919	302197.179611	38.629517
2391.443995	302631.634748	38.634535
2393.658052	303075.295572	38.639552
2395.837327	303529.324223	38.644570
2398.511292	303967.753091	38.649588
2400.721789	304422.002639	38.654605
2402.821965	304865.142678	38.659623
2405.197374	305312.835236	38.664640
2407.664632	305785.429820	38.669658
2409.913959	306244.722021	38.674676
2412.308081	306711.051034	38.679693
2414.658679	307174.184859	38.684711
2416.729412	307651.102943	38.689728
2418.986870	308140.130955	38.694746
2421.640901	308611.441174	38.699764
2423.870453	309096.126475	38.704781
2426.176003	309579.858028	38.709799
2429.121225	310072.350805	38.714816
2431.358133	310571.684713	38.719834
2433.776242	311049.753750	38.724852
2435.850038	311555.002009	38.729869
2438.609642	312054.678500	38.734887
2441.498926	312551.944702	38.739904
2443.780038	313055.781835	38.744922
2446.478998	313535.980168	38.749940
2448.965926	314031.271518	38.754957
2451.328397	314545.553180	38.759975
2454.075190	315030.893177	38.764992
2456.794208	315535.335012	38.770010
2459.263569	316025.768620	38.775028
2461.652760	316526.092499	38.780045
2463.960974	317024.420264	38.785063
2466.487101	317523.904705	38.790080
2468.659712	318020.725045	38.795098
2471.570298	318524.283298	38.800116
2474.091821	319021.017795	38.805133
2476.828916	319525.614149	38.810151
2479.529827	320023.991163	38.815168
2482.200817	320514.141534	38.820186
2484.972789	321005.492339	38.825204
2487.448901	321493.484164	38.830221
2490.064458	321972.435367	38.835239
2492.776958	322461.832050	38.840256
2495.192702	322942.333442	38.845274
2497.928965	323424.609929	38.850292
2500.306856	323907.092867	38.855309
2502.640496	324370.583794	38.860327
2505.149881	324825.587468	38.865344
2507.550636	325262.422458	38.870362
2510.192397	325713.590919	38.875380
2512.450661	326159.916314	38.880397
2514.731449	326601.512140	38.885415
2517.610946	327044.077289	38.890432
2519.421570	327516.064518	38.895450
2522.168411	327958.213874	38.900468
2524.262568	328418.875398	38.905485
2526.502202	328885.732840	38.910503
2529.230994	329359.848971	38.915520
2531.550265	329826.027813	38.920538
2533.919311	330312.358897	38.925556
2536.331292	330799.873545	38.930573
2538.571893	331280.606589	38.935591
2541.365219	331781.589286	38.940608
2543.516608	332277.794688	38.945626
2546.343663	332765.306694	38.950644
2548.869484	333269.876538	38.955661
2550.895691	333790.544929	38.960679
2553.617376	334298.148968	38.965696
2556.048793	334802.418084	38.970714
2558.815921	335327.502924	38.975732
2561.208783	335841.038788	38.980749
2564.108382	336360.381456	38.985767
2566.520256	336876.496449	38.990784
2568.947203	337413.553181	38.995802
2571.620052	337937.109149	39.000820
2574.455138	338460.939942	39.005837
2576.941803	338993.937101	39.010855
2579.948677	339521.794687	39.015872
2582.654108	340055.687863	39.020890
2585.363768	340568.908101	39.025908
2588.011847	341102.471461	39.030925
2590.574611	341635.510596	39.035943
2593.274474	342148.871764	39.040960
2595.697131	342687.052755	39.045978
2598.540987	343217.850162	39.050996
2601.666469	343749.816985	39.056013
2604.176179	344270.654760	39.061031
2606.956240	344792.257600	39.066048
2609.565878	345324.241315	39.071066
2612.111629	345842.571485	39.076084
2614.716012	346373.327863	39.081101
2617.057008	346893.534409	39.086119
2620.443665	347418.394243	39.091136
2623.019997	347944.469247	39.096154
2625.450731	348458.884390	39.101172
2628.196324	348982.891936	39.106189
2630.593183	349506.949796	39.111207
2633.275309	350024.864800	39.116224
2635.693667	350558.987635	39.121242
2638.761914	351072.363636	39.126260
2641.317119	351600.463519	39.131277
2644.244107	352115.070497	39.136295
2646.755975	352590.949833	39.141312
2649.181554	353093.949627	39.146330
2651.518483	353575.787884	39.151348
2654.118183	354068.140013	39.156365
2656.948877	354552.327977	39.161383
2659.612375	355043.163102	39.166400
2662.009441	355537.919449	39.171418
2664.780402	356033.550985	39.176436
2667.022386	356532.891264	39.181453
2669.124794	357035.091604	39.186471
2671.956525	357537.628308	39.191488
2674.680987	358065.330913	39.196506
2677.274996	358580.839756	39.201524
2680.309518	359097.593302	39.206541
2682.848712	359626.983734	39.211559
2685.739473	360143.063679	39.216576
2688.046697	360672.910920	39.221594
2690.880659	361190.257706	39.226612
2693.582921	361732.898721	39.231629
2696.343325	362256.286132	39.236647
2699.201467	362791.047845	39.241664
2701.716128	363328.243539	39.246682
2704.432827	363870.020086	39.251700
2707.305363	364408.897787	39.256717
2709.759913	364949.941806	39.261735
2712.828321	365497.252207	39.266752
2715.214069	366036.466987	39.271770
2718.358270	366594.791620	39.276788
2721.030262	367138.642779	39.281805
2723.459337	367696.229466	39.286823
2726.224919	368243.478227	39.291840
2729.227949	368791.114003	39.296858
2731.835550	369351.645931	39.301876
2734.813123	369898.688210	39.306893
2737.410840	370473.138615	39.311911
2740.311652	371019.798219	39.316928
2742.971006	371580.445287	39.321946
2746.147622	372142.677791	39.326964
2749.261903	372690.703112	39.331981
2751.696854	373257.808553	39.336999
2754.435494	373808.137035	39.342016
2757.423687	374354.967961	39.347034
2760.222293	374912.808144	39.352052
2763.132719	375475.773684	39.357069
2765.929035	376017.284652	39.362087
2769.061634	376572.740440	39.367104
2771.633290	377137.208189	39.372122
2774.645711	377674.882391	39.377140
2777.396725	378235.424498	39.382157
2780.116057	378780.284776	39.387175
2783.249898	379321.926029	39.392192
2785.908612	379881.292411	39.397210
2788.595291	380412.765396	39.402228
2791.577905	380972.496146	39.407245
2794.055572	381511.902328	39.412263
2796.548963	382019.435821	39.417280
2799.417247	382548.187014	39.422298
2802.227139	383056.062537	39.427316
2805.061342	383571.613720	39.432333
2807.562589	384085.739299	39.437351
2810.187329	384606.738026	39.442368
2813.080413	385133.445164	39.447386
2815.623083	385660.758381	39.452404
2818.294051	386179.546327	39.457421
2821.127902	386719.988432	39.462439
2823.949523	387260.297695	39.467456
2826.550382	387801.775317	39.472474
2829.046752	388345.265177	39.477492
2832.080922	388895.383111	39.482509
2834.406276	389469.826773	39.487527
2837.579085	390027.184679	39.492544
2840.286833	390591.734343	39.497562
2843.446977	391160.388147	39.502580
2845.986794	391724.946314	39.507597
2848.740188	392311.982374	39.512615
2851.674743	392879.908569	39.517632
2854.145661	393472.802783	39.522650
2857.361796	394053.548256	39.527668
2860.449291	394632.858801	39.532685
2863.091838	395228.180849	39.537703
2865.933673	395827.011163	39.542720
2869.013166	396412.530947	39.547738
2872.003475	397008.147076	39.552756
2874.963531	397609.665677	39.557773
2878.099906	398206.987018	39.562791
2881.202659	398799.054177	39.567808
2884.049646	399393.255766	39.572826
2887.317780	399985.326177	39.577844
2890.442437	400578.372089	39.582861
2893.182576	401180.215396	39.587879
2896.094494	401769.115125	39.592896
2899.191493	402362.487766	39.597914
2902.125012	402965.205287	39.602932
2905.083541	403548.918342	39.607949
2907.957408	404148.352465	39.612967
2910.909807	404739.700973	39.617984
2913.911012	405332.957365	39.623002
2916.612000	405937.379050	39.628020
2919.702717	406524.818730	39.633037
2922.546457	407146.660720	39.638055
2925.704780	407740.835070	39.643072
2928.846884	408336.546808	39.648090
2931.781874	408935.042723	39.653108
2934.999459	409525.573668	39.658125
2937.862566	410123.652049	39.663143
2941.137642	410708.092867	39.668160
2943.926806	411308.237930	39.673178
2947.045380	411894.632117	39.678196
2950.092352	412484.447741	39.683213
2953.091244	413060.192900	39.688231
2955.863584	413621.769888	39.693248
2959.123288	414173.273571	39.698266
2962.243582	414706.947205	39.703284
2964.706433	415239.929514	39.708301
2967.452222	415790.799772	39.713319
2970.497241	416341.789618	39.718336
2973.140773	416900.004140	39.723354
2975.776396	417459.020007	39.728372
2978.830528	418014.689825	39.733389
2981.600667	418586.788760	39.738407
2984.437529	419164.364304	39.743424
2987.433298	419733.642423	39.748442
2990.046505	420320.225087	39.753460
2993.187054	420902.734008	39.758477
2996.204301	421494.929202	39.763495
2999.313101	422083.195454	39.768512
3002.127646	422679.578086	39.773530
3004.798006	423284.052776	39.778548
3008.189175	423892.099079	39.783565
3011.053007	424510.602535	39.788583
3013.992790	425114.994231	39.793600
3017.255861	425737.105447	39.798618
3020.208086	426349.194394	39.803636
3023.564561	426968.501193	39.808653
3026.275506	427592.430230	39.813671
3029.489187	428215.961193	39.818688
3032.782467	428844.328426	39.823706
3035.759827	429475.947659	39.828724
3039.180073	430097.046026	39.833741
3041.954007	430725.096074	39.838759
3045.013041	431349.869285	39.843776
3048.735099	431990.934859	39.848794
3051.546527	432617.667037	39.853812
3054.916349	433231.885809	39.858829
3057.933280	433872.712405	39.863847
3060.764411	434500.636630	39.868864
3063.998582	435137.167940	39.873882
3067.340676	435775.135038	39.878900
3070.804810	436400.683760	39.883917
3073.851852	437039.754551	39.888935
3076.741209	437662.779987	39.893952
3080.404023	438296.707627	39.898970
3083.253282	438929.962932	39.903988
3086.549229	439560.953923	39.909005
3089.359339	440194.208474	39.914023
3092.440384	440816.972618	39.919040
3095.903097	441450.800522	39.924058
3098.895004	442095.421044	39.929076
3102.281606	442721.987240	39.934093
3105.303732	443346.772173	39.939111
3108.257100	443988.715669	39.944128
3111.412663	444632.230219	39.949146
3114.337846	445265.081450	39.954164
3117.501252	445885.677213	39.959181
3120.129816	446514.897108	39.964199
3123.432842	447114.783547	39.969216
3126.658288	447710.718461	39.974234
3129.699780	448320.284593	39.979252
3132.804393	448914.588234	39.984269
3135.546661	449508.124195	39.989287
3138.617858	450110.653576	39.994304
3142.084100	450707.941979	39.999322
3144.809548	451317.884675	40.004340
3148.020682	451930.113265	40.009357
3151.058636	452557.789691	40.014375
3153.929210	453172.670842	40.019392
3157.498922	453798.862598	40.024410
3160.074975	454439.415162	40.029428
3163.604511	455050.244503	40.034445
3166.951333	455693.473624	40.039463
3169.645961	456332.182565	40.044480
3173.142686	456968.064521	40.049498
3176.063543	457634.278815	40.054516
3179.347339	458295.760623	40.059533
3182.430900	458948.399739	40.064551
3185.627791	459615.118045	40.069568
3188.921912	460267.634223	40.074586
3191.947028	460927.661351	40.079604
3195.180985	461598.209202	40.084621
3198.359679	462271.072295	40.089639
3201.756154	462942.817713	40.094656
3205.344401	463620.885894	40.099674
3208.286625	464300.501874	40.104692
3212.099186	464962.102571	40.109709
3215.353600	465643.902822	40.114727
3218.670492	466321.523754	40.119744
3222.238276	466987.450185	40.124762
3225.036666	467668.549411	40.129780
3228.489408	468345.932256	40.134797
3231.735342	469019.937480	40.139815
3235.025917	469706.759360	40.144832
3238.434008	470385.094687	40.149850
3241.411660	471071.920992	40.154868
3245.125583	471745.258236	40.159885
3248.380789	472431.641472	40.164903
3251.446587	473130.268265	40.169920
3254.926650	473803.827854	40.174938
3258.177992	474491.457279	40.179956
3261.553688	475168.426375	40.184973
3264.850145	475843.211411	40.189991
3268.485681	476529.093091	40.195008
3272.016986	477207.991418	40.200026
3275.107516	477894.569850	40.205044
3278.528895	478568.333639	40.210061
3282.035871	479246.256648	40.215079
3285.322529	479925.455012	40.220096
3288.620065	480589.565808	40.225114
3291.684204	481262.182472	40.230132
3295.119947	481943.157854	40.235149
3298.468796	482605.271800	40.240167
3301.566027	483248.855430	40.245184
3304.676646	483872.908410	40.250202
3307.587031	484513.548535	40.255220
3310.633854	485132.163744	40.260237
3314.365919	485772.480564	40.265255
3316.971124	486413.762694	40.270272
3320.074881	487060.755313	40.275290
3323.288299	487721.300385	40.280308
3326.723724	488365.215207	40.285325
3330.014636	489023.530177	40.290343
3332.956301	489700.620944	40.295360
3336.395372	490369.576117	40.300378
3339.428619	491047.563824	40.305396
3342.872466	491730.917810	40.310413
3346.018487	492417.274205	40.315431
3349.073214	493117.106509	40.320448
3352.942921	493810.065679	40.325466
3356.112518	494513.867863	40.330484
3359.446941	495226.203219	40.335501
3362.661590	495935.499605	40.340519
3365.975969	496648.338424	40.345536
3369.682800	497373.459996	40.350554
3373.184137	498092.272808	40.355572
3376.440611	498803.470827	40.360589
3379.898092	499514.912032	40.365607
3382.999095	500259.050174	40.370624
3387.101804	500984.469100	40.375642
3390.239025	501714.858106	40.380660
3393.717546	502451.574994	40.385677
3397.247996	503187.041493	40.390695
3400.697184	503919.511835	40.395712
3404.060710	504647.472586	40.400730
3407.424192	505385.700715	40.405748
3411.247721	506126.348822	40.410765
3414.750073	506876.909130	40.415783
3417.986583	507631.415879	40.420800
3421.844610	508352.986537	40.425818
3425.552368	509098.825568	40.430836
3428.966887	509820.354542	40.435853
3432.640496	510566.740941	40.440871
3436.078689	511315.554138	40.445888
3439.738552	512036.597749	40.450906
3443.343263	512776.641572	40.455924
3447.034333	513499.131870	40.460941
3450.538157	514228.331010	40.465959
3453.738469	514967.535639	40.470976
3457.685151	515691.657299	40.475994
3461.123652	516420.368059	40.481012
3464.763246	517143.113379	40.486029
3468.444437	517878.430996	40.491047
3471.905067	518584.143313	40.496064
3475.668849	519299.007526	40.501082
3479.128249	520032.045259	40.506100
3482.668323	520729.129821	40.511117
3486.484410	521410.914308	40.516122
3489.594069	522094.018457	40.521127
3493.118797	522657.010555	40.526132
3496.175975	523209.996890	40.531136
3499.143949	523675.119119	40.536141
3502.396090	524070.979057	40.541146
3504.691897	524445.951762	40.546151
3507.751327	524733.093120	40.551156
3509.574582	524961.839580	40.556160
3511.629933	525156.679331	40.561165
3514.030971	525271.597834	40.566170
3515.317133	525355.403227	40.571175
3517.058544	525400.670233	40.576180
3518.509576	525399.884460	40.581184
3519.535432	525351.752988	40.586189
3520.453654	525267.497223	40.591194
3521.316472	525182.087185	40.596199
3522.041824	525028.206186	40.601204
3523.088310	524888.325410	40.606208
3523.834119	524695.263011	40.611213
3524.719305	524490.246588	40.616218
3524.702955	524269.901667	40.621223
3525.246194	524035.766001	40.626228
3525.848105	523762.541155	40.631232
3525.647759	523489.994567	40.636237
3526.188135	523207.872830	40.641242
3526.368023	522905.176938	40.646247
3526.447435	522596.475193	40.651252
3526.345109	522293.306967	40.656256
3526.250039	521972.841336	40.661261
3526.343364	521653.148577	40.666266
3526.464900	521327.276865	40.671271
3526.193999	520998.983226	40.676276
3526.512611	520660.730371	40.681280
3526.019770	520323.862846	40.686285
3525.969697	519977.463065	40.691290
3525.445162	519640.080911	40.696295
3525.528132	519300.775483	40.701300
3525.414936	518966.803585	40.706304
3525.141047	518636.744046	40.711309
3524.925083	518290.790205	40.716314
3524.582669	517957.390428	40.721319
3524.312417	517623.719698	40.726324
3524.008500	517298.189644	40.731328
3523.812263	516982.245024	40.736333
3523.737978	516661.824663	40.741338
3523.269747	516344.444314	40.746343
3523.231034	516019.302572	40.751348
3522.593387	515703.302374	40.756352
3522.117598	515397.386140	40.761357
3522.587351	515091.112589	40.766362
3521.733548	514791.213305	40.771367
3521.533773	514484.427567	40.776372
3521.391665	514191.132292	40.781376
3521.158040	513904.118549	40.786381
3520.937189	513614.771102	40.791386
3520.151966	513337.698563	40.796391
3520.196369	513046.124379	40.801396
3519.771536	512785.324648	40.806400
3519.665017	512510.610014	40.811405
3519.290183	512245.291925	40.816410
3518.587118	511989.380295	40.821415
3518.722460	511732.118197	40.826420
3518.313490	511488.900856	40.831424
3518.195398	511217.860215	40.836429
3517.972752	510987.354952	40.841434
3517.478341	510746.265353	40.846439
3517.706837	510502.933246	40.851444
3517.389612	510273.900501	40.856448
3517.163449	510035.490523	40.861453
3517.098332	509812.786560	40.866458
3516.599414	509586.100690	40.871463
3516.290848	509368.539524	40.876468
3516.127789	509147.360295	40.881472
3516.006606	508933.963504	40.886477
3515.794870	508727.914995	40.891482
3515.570464	508525.306689	40.896487
3515.284058	508310.106784	40.901492
3515.207204	508112.125384	40.906496
3514.529171	507928.657631	40.911501
3514.707577	507730.327933	40.916506
3514.250137	507546.720078	40.921511
3514.286656	507359.135919	40.926516
3514.003645	507180.404950	40.931520
3513.665623	507004.969991	40.936525
3513.649872	506824.725667	40.941530
3513.498818	506664.792797	40.946535
3513.209721	506472.595046	40.951540
3513.175340	506311.122380	40.956544
3512.827633	506154.150962	40.961549
3512.701705	505992.082559	40.966554
3512.479995	505845.917981	40.971559
3512.525113	505695.104857	40.976564
3512.379745	505534.755901	40.981568
3512.192643	505387.215649	40.986573
3512.074031	505237.385997	40.991578
3511.723430	505098.674848	40.996583
3511.693123	504936.075493	41.001588
3511.417921	504816.125863	41.006592
3511.054426	504677.413426	41.011597
3511.391142	504541.777628	41.016602
3510.956570	504423.773669	41.021607
3511.229848	504280.250759	41.026612
3510.763296	504146.409003	41.031616
3510.700714	504037.757232	41.036621
3510.364766	503907.739451	41.041626
3510.094744	503803.269143	41.046631
3510.131572	503679.517210	41.051636
3510.137571	503579.152129	41.056640
3509.695211	503472.328328	41.061645
3509.700568	503362.851871	41.066650
3509.536150	503263.524190	41.071655
3509.466241	503158.411089	41.076660
3509.292519	503053.010090	41.081664
3509.219434	502960.904034	41.086669
3509.324398	502851.155604	41.091674
3509.012214	502753.215002	41.096679
3508.920802	502676.902100	41.101684
3509.202155	502567.782034	41.106688
3508.707571	502478.321458	41.111693
3508.796041	502389.780595	41.116698
3508.776960	502305.356172	41.121703
3508.665322	502218.718869	41.126708
3508.541199	502140.282958	41.131712
3508.433020	502054.707252	41.136717
3508.614181	501962.505225	41.141722
3508.086845	501888.636824	41.146727
3507.715339	501804.316340	41.151732
3507.996073	501730.167722	41.156736
3507.706128	501653.375633	41.161741
3507.981906	501577.911106	41.166746
3507.785407	501513.960588	41.171751
3507.992445	501422.257860	41.176756
3507.787360	501371.317094	41.181760
3507.504108	501294.471785	41.186765
3507.609209	501224.853890	41.191770
3507.398627	501156.399235	41.196775
3507.600297	501088.587835	41.201780
3507.665870	501020.240873	41.206784
3507.437238	500956.445297	41.211789
3507.263306	500886.667707	41.216794
3507.157343	500835.557889	41.221799
3507.148341	500775.574075	41.226804
3506.953918	500721.086360	41.231808
3506.995303	500662.916537	41.236813
3506.959693	500602.278283	41.241818
3506.954999	500549.633025	41.246823
3506.689093	500485.588558	41.251828
3507.186105	500436.710872	41.256832
3506.848220	500373.942909	41.261837
3507.012715	500318.334199	41.266842
3506.474930	500268.505925	41.271847
3506.521021	500205.727311	41.276852
3506.660493	500160.297038	41.281856
3506.253954	500113.940503	41.286861
3506.578246	500069.594476	41.291866
3506.772294	500021.522876	41.296871
3506.419539	499963.008098	41.301876
3506.497180	499914.195271	41.306880
3506.372306	499879.133071	41.311885
3506.099342	499836.500787	41.316890
3506.119656	499792.607102	41.321895
3506.358325	499736.174902	41.326900
3506.278285	499694.321760	41.331904
3505.864964	499665.177021	41.336909
3506.519627	499613.791644	41.341914
3506.325923	499572.715536	41.346919
3505.908701	499527.422270	41.351924
3506.305640	499473.849784	41.356928
3506.106634	499437.026605	41.361933
3505.976874	499406.216666	41.366938
3505.742922	499362.463365	41.371943
3505.553331	499327.764689	41.376948
3505.862008	499291.316594	41.381952
3505.867209	499274.103041	41.386957
3506.178675	499221.454553	41.391962
3505.796719	499181.976666	41.396967
3505.610332	499156.288338	41.401972
3505.641163	499119.782559	41.406976
3505.662728	499081.556924	41.411981
3505.848784	499041.178959	41.416986
3505.524912	499025.890304	41.421991
3505.945221	498989.221457	41.426996
3505.742351	498947.537870	41.432000
3505.354387	498908.971591	41.437005
3505.464400	498877.920353	41.442010
3505.558552	498847.580326	41.447015
3505.678044	498812.882436	41.452020
3505.616183	498788.237043	41.457024
3505.443681	498767.355412	41.462029
3505.357916	498726.614698	41.467034
3505.170725	498716.012388	41.472039
3505.538484	498671.352300	41.477044
3505.388766	498649.353158	41.482048
3505.058736	498634.571405	41.487053
3505.470550	498600.687554	41.492058
3505.308338	498571.146975	41.497063
3505.405361	498537.717767	41.502068
3505.614252	498502.448262	41.507072
3505.708062	498482.081105	41.512077
3505.786903	498452.249102	41.517082
3505.453006	498426.937436	41.522087
3505.357635	498381.843562	41.527092
3505.412160	498365.532633	41.532096
3505.260253	498334.876247	41.537101
3505.287888	498305.102721	41.542106
3505.052635	498282.863516	41.547111
3504.983636	498245.713598	41.552116
3505.116045	498228.630828	41.557120
3505.067983	498209.551469	41.562125
3505.276578	498179.141608	41.567130
3504.952140	498164.712979	41.572135
3504.961294	498132.056323	41.577140
3505.296373	498117.371541	41.582144
3505.129191	498098.513402	41.587149
3505.209714	498068.022341	41.592154
3505.208768	498047.517788	41.597159
3505.324449	498012.920224	41.602164
3505.138107	497990.318534	41.607168
3504.995755	497977.329189	41.612173
3505.329369	497944.064008	41.617178
3504.772986	497922.432022	41.622183
3504.940280	497909.849344	41.627188
3504.745791	497884.464259	41.632192
3504.735107	497871.150259	41.637197
3505.086830	497855.196927	41.642202
3505.012460	497829.337125	41.647207
3505.067713	497814.443181	41.652212
3504.882904	497785.107406	41.657216
3505.021573	497760.428921	41.662221
3505.172327	497735.090320	41.667226
3505.011925	497732.431903	41.672231
3504.870016	497703.646131	41.677236
3505.189475	497679.850283	41.682240
3505.119823	497669.532556	41.687245
3504.918747	497637.110751	41.692250
3504.912535	497606.936398	41.697255
3505.092363	497599.313171	41.702260
3504.779724	497572.680595	41.707264
3504.573204	497559.852980	41.712269
3504.639651	497534.932458	41.717274
3504.786611	497521.643917	41.722279
3504.849174	497505.128427	41.727284
3504.953956	497482.631983	41.732288
3504.753499	497473.853699	41.737293
3504.680471	497450.372728	41.742298
3504.951012	497436.406411	41.747303
3505.151108	497404.376453	41.752308
3504.916391	497393.932769	41.757312
3504.808346	497371.824231	41.762317
3505.273011	497344.207767	41.767322
3504.841748	497319.568129	41.772327
3504.746006	497314.114789	41.777332
3505.263018	497289.122722	41.782336
3504.781132	497276.895356	41.787341
3504.893231	497250.245810	41.792346
3505.034037	497241.869151	41.797351
3504.939580	497204.214826	41.802356
3505.269790	497186.188472	41.807360
3504.637093	497176.820165	41.812365
3504.805250	497140.238069	41.817370
3504.479561	497134.010930	41.822375
3504.698887	497116.964010	41.827380
3505.052353	497108.452419	41.832384
3504.480304	497096.694855	41.837389
3504.601995	497073.790190	41.842394
3504.547271	497057.242200	41.847399
3504.649054	497029.834504	41.852404
3504.732771	497024.757759	41.857408
3504.530604	497021.093224	41.862413
3504.873606	496986.204628	41.867418
3504.822060	496976.187432	41.872423
3504.711997	496949.572558	41.877428
3504.857513	496940.992493	41.882432
3504.502342	496938.466002	41.887437
3504.804639	496910.418866	41.892442
3504.798889	496900.343758	41.897447
3504.740399	496885.720186	41.902452
3505.130256	496859.886901	41.907456
3505.025958	496849.118504	41.912461
3504.768590	496821.311576	41.917466
3504.867819	496815.422222	41.922471
3504.911514	496785.896828	41.927476
3504.925616	496764.021404	41.932480
3504.505642	496731.733844	41.937485
3504.678245	496724.972130	41.942490
3504.389450	496718.941544	41.947495
3504.497347	496689.203321	41.952500
3504.726979	496694.989214	41.957504
3504.346681	496680.112548	41.962509
3504.630676	496656.472865	41.967514
3504.608829	496654.399971	41.972519
3504.687679	496645.982198	41.977524
3504.757704	496621.313021	41.982528
3504.502675	496620.846561	41.987533
3504.959533	496600.014866	41.992538
3504.414772	496584.100844	41.997543
3504.584331	496570.605512	42.002548
3504.974272	496538.341503	42.007552
3504.632324	496532.167359	42.012557
3504.728369	496504.000300	42.017562
3504.761014	496498.779585	42.022567
3504.687431	496496.309793	42.027572
3504.716863	496473.267059	42.032576
3504.488813	496453.353558	42.037581
3504.830316	496437.755030	42.042586
3504.328116	496418.492405	42.047591
3504.418681	496404.300582	42.052596
3504.391448	496400.304479	42.057600
3504.120441	496388.752040	42.062605
3504.241462	496373.795893	42.067610
3504.301473	496371.861927	42.072615
3504.317198	496365.175506	42.077620
3504.244408	496334.401980	42.082624
3504.248819	496332.881857	42.087629
3504.502748	496325.803347	42.092634
3504.394389	496321.820049	42.097639
3504.749648	496314.371092	42.102644
3504.825878	496296.687798	42.107648
3504.593062	496297.230472	42.112653
3504.405154	496264.399082	42.117658
3504.654089	496251.650461	42.122663
3504.418260	496241.003759	42.127668
3504.720729	496222.778310	42.132672
3504.614625	496221.680708	42.137677
3504.391159	496199.234559	42.142682
3504.147491	496182.816905	42.147687
3504.311125	496169.474112	42.152692
3504.632388	496166.891238	42.157696
3504.574316	496157.937918	42.162701
3504.708765	496125.156597	42.167706
3504.505040	496131.416224	42.172711
3504.084835	496123.431516	42.177716
3504.449287	496095.120142	42.182720
3504.268737	496079.502551	42.187725
3504.175749	496077.440835	42.192730
3504.096280	496103.427807	42.197735
3504.142987	496068.077956	42.202740
3504.341909	496075.641066	42.207744
3504.019549	496039.792523	42.212749
3504.313888	496072.961035	42.217754
3504.556274	496039.251101	42.222759
3504.320902	496049.971497	42.227764
3504.473595	496009.085744	42.232768
3504.269398	496029.927917	42.237773
3504.397602	495992.742238	42.242778
3504.668291	496008.800463	42.247783
3504.232112	495988.463647	42.252788
3504.489376	495978.852800	42.257792
3504.301509	495985.666940	42.262797
3504.334855	495937.154222	42.267802
3504.300894	495947.133974	42.272807
3504.241747	495948.003646	42.277812
3504.533664	495941.982291	42.282816
3504.331632	495919.836215	42.287821
3504.625413	495926.118551	42.292826
3504.626860	495901.357975	42.297831
3504.334293	495881.504680	42.302836
3504.534608	495885.067576	42.307840
3503.998873	495873.759184	42.312845
3504.593443	495856.044179	42.317850
3504.584372	495843.437318	42.322855
3504.615900	495839.279905	42.327860
3504.562733	495819.743145	42.332864
3504.588366	495798.674889	42.337869
3504.369315	495786.556882	42.342874
3504.351072	495787.217561	42.347879
3504.216057	495758.073191	42.352884
3504.604158	495765.150823	42.357888
3504.455420	495751.755827	42.362893
3504.391821	495725.334364	42.367898
3504.636037	495722.257264	42.372903
3504.699763	495700.828435	42.377908
3504.370534	495705.639647	42.382912
3504.123882	495673.575995	42.387917
3504.394670	495665.532513	42.392922
3504.485297	495665.112667	42.397927
3504.270444	495651.677413	42.402932
3504.427143	495636.866929	42.407936
3504.303332	495636.126532	42.412941
3504.309090	495623.112100	42.417946
3504.331827	495608.322766	42.422951
3504.695368	495578.238528	42.427956
3504.830436	495598.723764	42.432960
3504.394288	495585.272800	42.437965
3504.612120	495542.755404	42.442970
3504.348510	495552.771666	42.447975
3504.318676	495544.522469	42.452980
3504.421275	495523.441732	42.457984
3504.099244	495519.238855	42.462989
3503.986135	495494.090754	42.467994
3504.026300	495519.705202	42.472999
3504.294437	495495.509546	42.478004
3504.400806	495476.909270	42.483008
3504.384429	495482.936969	42.488013
3504.499495	495466.917690	42.493018
3504.345421	495463.498414	42.498023
3504.063559	495454.529484	42.503028
3504.406408	495438.777991	42.508032
3504.197711	495431.772253	42.513037
3504.316349	495429.879557	42.518042
3504.501750	495410.659103	42.523047
3504.289121	495393.223132	42.528052
3504.492971	495393.949994	42.533056
3504.434107	495400.693328	42.538061
3504.675862	495361.007299	42.543066
3504.276538	495378.741663	42.548071
3504.101957	495359.122331	42.553076
3504.706976	495360.241510	42.558080
3504.663288	495337.056999	42.563085
3504.452932	495316.177392	42.568090
3504.420082	495309.346356	42.573095
3504.757822	495276.126307	42.578100
3505.019255	495269.653831	42.583104
3504.696293	495258.665879	42.588109
3504.810476	495249.026629	42.593114
3504.756533	495227.514574	42.598119
3504.437604	495208.525522	42.603124
3504.616458	495197.964581	42.608128
3504.678011	495179.826809	42.613133
3504.766965	495164.925381	42.618138
3504.254601	495169.259318	42.623143
3504.176746	495141.117650	42.628148
3504.844775	495121.769981	42.633152
3504.289260	495132.237692	42.638157
3504.412579	495110.646849	42.643162
3504.525300	495088.095571	42.648167
3503.900030	495091.434649	42.653172
3504.236293	495074.316713	42.658176
3503.932728	495066.718196	42.663181
3504.295172	495059.723322	42.668186
3504.144773	495057.670564	42.673191
3503.828267	495035.642784	42.678196
3504.637492	495041.236329	42.683200
3504.356356	495046.293291	42.688205
3504.366791	495033.125795	42.693210
3504.133314	495015.135761	42.698215
3504.226558	495006.968143	42.703220
3504.283289	495005.591551	42.708224
3503.951393	495024.530869	42.713229
3504.541846	494984.687647	42.718234
3504.484826	494980.442761	42.723239
3504.498915	494957.957548	42.728244
3504.596540	494960.169672	42.733248
3504.389602	494937.263639	42.738253
3504.172112	494920.891352	42.743258
3504.157870	494919.272788	42.748263
3504.144218	494920.540410	42.753268
3504.173447	494899.065463	42.758272
3504.115194	494889.757096	42.763277
3504.318609	494867.191214	42.768282
3504.158752	494890.812685	42.773287
3504.148031	494891.421570	42.778292
3504.437862	494869.652219	42.783296
3504.148826	494849.493429	42.788301
3504.242628	494844.262578	42.793306
3504.414044	494856.944844	42.798311
3504.257448	494827.093494	42.803316
3504.651105	494810.624521	42.808321
3504.141584	494816.325282	42.813325
3504.597771	494814.784271	42.818330
3504.574202	494797.672311	42.823335
3504.557629	494790.129595	42.828340
3504.821110	494765.427349	42.833345
3504.592089	494748.246540	42.838349
3504.694141	494744.381554	42.843354
3504.634587	494730.110889	42.848359
3504.406094	494714.651624	42.853364
3504.407195	494701.130906	42.858369
3504.501609	494696.862021	42.863373
3504.434861	494666.388565	42.868378
3504.312585	494664.584504	42.873383
3504.260509	494659.781754	42.878388
3504.655014	494649.591515	42.883393
3504.026337	494621.536107	42.888397
3504.274652	494610.356204	42.893402
3504.073981	494613.881448	42.898407
3504.163822	494602.675949	42.903412
3504.549431	494595.879789	42.908417
3504.260686	494584.734113	42.913421
3504.475929	494563.786387	42.918426
3504.400858	494569.874299	42.923431
3504.214886	494553.648616	42.928436
3504.873114	494522.047594	42.933441
3504.542726	494524.833791	42.938445
3504.431239	494514.875360	42.943450
3504.672563	494498.531459	42.948455
3504.409690	494494.825371	42.953460
3504.637715	494473.419785	42.958465
3504.048112	494469.360228	42.963469
3504.500799	494445.387216	42.968474
3504.351856	494446.169875	42.973479
3504.396004	494427.932838	42.978484
3504.639775	494411.031457	42.983489
3504.259758	494410.230226	42.988493
3504.269681	494401.619768	42.993498
3504.515072	494382.895140	42.998503
3504.227444	494365.014305	43.003508
3504.291373	494354.622959	43.008513
3504.262472	494351.892625	43.013517
3504.561408	494335.235647	43.018522
3504.687906	494331.518626	43.023527
3504.449478	494322.289086	43.028532
3504.277528	494296.794182	43.033537
3504.167746	494284.252809	43.038541
3504.193412	494275.741080	43.043546
3504.404438	494280.720468	43.048551
3504.467913	494265.974255	43.053556
3504.347522	494250.598791	43.058561
3504.127590	494244.860333	43.063565
3504.296050	494237.440063	43.068570
3504.386038	494239.248374	43.073575
3504.193625	494223.327249	43.078580
3504.329426	494201.733369	43.083585
3504.313564	494207.609488	43.088589
3504.405348	494197.871952	43.093594
3504.257411	494184.526326	43.098599
3504.335488	494172.866679	43.103604
3504.281171	494154.442380	43.108609
3504.016863	494164.256950	43.113613
3503.931434	494149.483539	43.118618
3504.242981	494139.559324	43.123623
3504.086705	494132.544805	43.128628
3504.577792	494129.175231	43.133633
3504.151955	494119.013074	43.138637
3504.230657	494115.860590	43.143642
3504.427180	494106.258368	43.148647
3504.171388	494100.019145	43.153652
3504.518313	494090.696977	43.158657
3504.068812	494092.438650	43.163661
3504.028637	494075.278006	43.168666
3503.939356	494063.188991	43.173671
3503.744610	494066.561485	43.178676
3503.962182	494051.537553	43.183681
3504.044187	494051.574784	43.188685
3504.027668	494054.665918	43.193690
3504.202351	494059.245998	43.198695
3503.768114	494059.921846	43.203700
3504.151701	494061.228023	43.208705
3503.969678	494037.759906	43.213709
3504.003187	494015.473031	43.218714
3504.073338	494005.738813	43.223719
3503.862406	494030.483514	43.228724
3504.199089	494012.098556	43.233729
3504.068523	494022.854203	43.238733
3504.363462	494007.210340	43.243738
3504.284533	493994.562616	43.248743
3504.365856	493976.724371	43.253748
3504.420735	493983.197050	43.258753
3504.468123	493978.327763	43.263757
3504.157803	493952.601057	43.268762
3504.454179	493923.436242	43.273767
3504.121068	493947.997806	43.278772
3504.149107	493935.890166	43.283777
3504.254207	493919.212809	43.288781
3504.245320	493912.630665	43.293786
3503.993702	493895.655190	43.298791
3503.891964	493898.658539	43.303796
3504.087909	493905.058312	43.308801
3504.042247	493886.125985	43.313805
3503.760813	493902.982264	43.318810
3504.284650	493899.151720	43.323815
3504.259535	493864.214103	43.328820
3504.304169	493874.233195	43.333825
3504.368686	493838.369855	43.338829
3504.419302	493863.276001	43.343834
3504.096489	493824.334207	43.348839
3503.957648	493842.585910	43.353844
3504.249777	493808.509558	43.358849
3504.160256	493816.321745	43.363853
3503.715322	493816.189060	43.368858
3504.473208	493815.106681	43.373863
3503.826666	493814.752661	43.378868
3504.290332	493786.118225	43.383873
3504.471291	493772.365843	43.388877
3504.461307	493783.203851	43.393882
3504.320613	493774.009230	43.398887
3504.181653	493752.103773	43.403892
3504.357108	493718.957211	43.408897
3503.884318	493759.138146	43.413901
3504.007987	493737.646922	43.418906
3504.232862	493753.157323	43.423911
3503.904899	493734.623935	43.428916
3503.886594	493704.495714	43.433921
3503.811130	493725.674625	43.438925
3504.195307	493712.852237	43.443930
3504.094899	493710.690147	43.448935
3504.099875	493709.574837	43.453940
3504.171490	493705.815726	43.458945
3504.264148	493704.838478	43.463949
3504.331281	493679.507495	43.468954
3504.326654	493667.101003	43.473959
3503.962476	493656.169246	43.478964
3504.158458	493661.252459	43.483969
3504.118344	493669.208819	43.488973
3504.095685	493636.853020	43.493978
3504.217409	493632.174454	43.498983
3504.015342	493635.294983	43.503988
3504.228060	493624.474592	43.508993
3504.146481	493636.640642	43.513997
3504.006422	493615.140317	43.519002
3504.270081	493597.728650	43.524007
3504.049756	493595.737419	43.529012
3504.191088	493589.080779	43.534017
3504.093656	493593.754622	43.539021
3504.330185	493589.716222	43.544026
3504.108146	493575.824826	43.549031
3503.989718	493566.930423	43.554036
3504.275307	493550.325490	43.559041
3504.250189	493551.949500	43.564045
3504.304878	493560.599887	43.569050
3504.253826	493541.009736	43.574055
3504.220159	493523.442430	43.579060
3504.467627	493517.326033	43.584065
3504.242533	493518.779089	43.589069
3504.236432	493509.866907	43.594074
3503.992351	493493.446915	43.599079
3503.717687	493493.743078	43.604084
3504.040013	493485.133460	43.609089
3504.325059	493490.152004	43.614093
3504.116862	493494.995298	43.619098
3503.995533	493487.975011	43.624103
3504.170018	493485.921370	43.629108
3504.459456	493462.226091	43.634113
3504.288296	493463.265503	43.639117
3504.320327	493440.066641	43.644122
3504.446996	493440.501939	43.649127
3504.206233	493427.879404	43.654132
3504.239716	493403.110408	43.659137
3504.414094	493403.740730	43.664141
3504.287412	493400.418021	43.669146
3504.200813	493381.744852	43.674151
3504.058455	493372.550294	43.679156
3504.292558	493361.473167	43.684161
3503.680716	493377.875733	43.689165
3504.243297	493355.048680	43.694170
3504.129457	493359.370690	43.699175
3503.799979	493370.867123	43.704180
3503.950251	493345.623826	43.709185
3504.173359	493338.599686	43.714189
3504.128913	493331.060779	43.719194
3504.335414	493335.332166	43.724199
3503.983759	493338.830872	43.729204
3504.309072	493327.587387	43.734209
3504.180261	493318.036174	43.739213
3504.126030	493298.851397	43.744218
3503.815183	493306.698778	43.749223
3504.020150	493300.690309	43.754228
3504.161145	493301.477833	43.759233
3504.308615	493301.909847	43.764237
3504.152850	493278.993668	43.769242
3504.370483	493272.071650	43.774247
3503.861867	493276.405430	43.779252
3504.469682	493270.130720	43.784257
3504.067810	493277.232884	43.789261
3504.313586	493251.619878	43.794266
3504.453131	493235.696079	43.799271
3504.172634	493227.181615	43.804276
3504.444800	493220.200318	43.809281
3504.219868	493205.650766	43.814285
3504.118620	493200.348996	43.819290
3504.040375	493181.623664	43.824295
3504.037306	493183.244221	43.829300
3504.150731	493176.642485	43.834305
3503.667223	493193.987114	43.839309
3503.820004	493198.976000	43.844314
3503.849273	493187.526012	43.849319
3503.843819	493190.868747	43.854324
3503.978007	493162.893118	43.859329
3503.949312	493169.936344	43.864333
3504.256765	493154.239144	43.869338
3503.945156	493149.375737	43.874343
3503.635045	493161.780782	43.879348
3504.270383	493144.056742	43.884353
3504.075035	493148.341041	43.889357
3504.233125	493153.481023	43.894362
3503.987011	493120.602585	43.899367
3504.010252	493110.723386	43.904372
3503.845089	493121.586307	43.909377
3503.966801	493115.033880	43.914381
3504.144128	493108.675228	43.919386
3503.880986	493106.640069	43.924391
3503.655402	493110.726590	43.929396
3504.022055	493115.631055	43.934401
3503.674825	493125.661843	43.939405
3503.631156	493125.769580	43.944410
3503.923444	493129.267836	43.949415
3503.564066	493127.450455	43.954420
3503.987692	493128.598449	43.959425
3503.808791	493119.308257	43.964429
3504.055787	493109.494978	43.969434
3504.074160	493090.602359	43.974439
3503.719036	493091.164452	43.979444
3504.155594	493073.978177	43.984449
3503.627619	493086.215138	43.989453
3503.832742	493089.423328	43.994458
3503.821557	493089.475290	43.999463
3503.829190	493096.310237	44.004468
3503.967625	493095.933420	44.009473
3503.778488	493093.329508	44.014477
3503.898629	493089.157470	44.019482
3504.004775	493091.064624	44.024487
3504.022870	493082.047129	44.029492
3504.003786	493062.552703	44.034497
3504.110109	493054.736649	44.039501
3503.937796	493058.156421	44.044506
3504.071398	493048.715522	44.049511
3503.904727	493051.779912	44.054516
3503.885294	493043.527953	44.059521
3503.974023	493049.134702	44.064525
3504.142594	493043.435752	44.069530
3503.907733	493021.240738	44.074535
3503.971692	493017.735905	44.079540
3504.237537	493021.592852	44.084545
3504.341301	493018.284296	44.089549
3503.976306	493013.631856	44.094554
3504.059377	493013.314430	44.099559
3504.100384	493011.180549	44.104564
3503.931523	492994.241809	44.109569
3504.132883	492992.437076	44.114573
3504.492114	492980.225828	44.119578
3504.359991	492982.626426	44.124583
3503.933368	492974.286865	44.129588
3503.920751	492951.297016	44.134593
3504.015344	492942.976349	44.139597
3504.054939	492934.157952	44.144602
3504.127379	492938.602544	44.149607
3504.253810	492940.658433	44.154612
3504.288540	492939.842226	44.159617
3504.385636	492928.989063	44.164621
3504.332319	492915.982060	44.169626
3504.138138	492919.759807	44.174631
3503.940417	492927.640111	44.179636
3504.065213	492925.239769	44.184641
3504.268493	492921.155838	44.189645
3504.361598	492886.096410	44.194650
3503.988962	492870.962234	44.199655
3503.990154	492878.102132	44.204660
3504.336670	492877.591141	44.209665
3504.202908	492871.129647	44.214669
3504.197913	492842.263975	44.219674
3504.428524	492830.174240	44.224679
3504.053159	492838.082657	44.229684
3504.212438	492840.791714	44.234689
3504.338437	492830.896126	44.239693
3503.755443	492814.934233	44.244698
3504.146239	492803.426872	44.249703
3503.877555	492790.251250	44.254708
3504.384635	492780.295408	44.259713
3504.218821	492785.841180	44.264717
3504.285440	492783.348730	44.269722
3504.482743	492763.110799	44.274727
3504.124817	492771.067130	44.279732
3504.620527	492751.237806	44.284737
3504.275694	492743.138427	44.289741
3504.230230	492719.495130	44.294746
3504.353580	492710.460820	44.299751
3504.268788	492711.739837	44.304756
3504.803877	492701.576956	44.309761
3504.182009	492685.266597	44.314765
3504.137849	492670.991911	44.319770
3504.285140	492664.131428	44.324775
3504.083582	492669.632242	44.329780
3504.176673	492656.652561	44.334785
3504.060592	492636.008237	44.339789
3504.261313	492630.759865	44.344794
3504.158468	492636.700871	44.349799
3504.177039	492630.113933	44.354804
3504.496885	492616.440032	44.359809
3504.193209	492607.118661	44.364813
3504.144428	492596.693501	44.369818
3504.415447	492600.904219	44.374823
3504.205467	492583.870317	44.379828
3504.100863	492547.727355	44.384833
3503.838580	492565.189534	44.389837
3504.005178	492551.134661	44.394842
3504.123566	492543.316485	44.399847
3503.826512	492552.326792	44.404852
3503.993185	492552.654503	44.409857
3503.772185	492554.208272	44.414861
3503.791826	492551.672573	44.419866
3504.049004	492548.491616	44.424871
3503.709143	492542.315795	44.429876
3503.827578	492529.382664	44.434881
3503.792014	492523.513246	44.439885
3503.691312	492513.602676	44.444890
3503.739299	492514.759434	44.449895
3503.962556	492513.812127	44.454900
3504.194348	492507.495305	44.459905
3504.147263	492515.301332	44.464909
3504.099708	492512.472389	44.469914
3504.177537	492506.230543	44.474919
3504.000424	492506.207444	44.479924
3503.893463	492496.956214	44.484929
3504.140588	492482.534061	44.489933
3504.104589	492471.651023	44.494938
3504.071541	492476.466900	44.499943
3503.960331	492480.586125	44.504948
3504.259186	492486.109191	44.509953
3503.937689	492488.033350	44.514957
3503.711781	492466.140117	44.519962
3504.184831	492444.085747	44.524967
3503.912767	492448.635547	44.529972
3503.888647	492438.662190	44.534977
3503.842669	492449.202806	44.539981
3504.093183	492448.555047	44.544986
3504.054851	492433.013177	44.549991
3503.849408	492458.265536	44.554996
3504.012861	492450.237626	44.560001
3503.782767	492448.551674	44.565005
3503.559494	492442.205464	44.570010
3503.986188	492463.914168	44.575015
3503.652062	492442.747015	44.580020
3503.871984	492403.361958	44.585025
3503.740913	492416.144349	44.590029
3503.980499	492413.776443	44.595034
3504.118295	492398.611854	44.600039
3503.805859	492426.514621	44.605044
3504.152898	492411.975336	44.610049
3504.163524	492407.972385	44.615053
3503.988150	492410.987612	44.620058
3504.180350	492411.716439	44.625063
3504.106837	492385.190480	44.630068
3503.959094	492391.088017	44.635073
3503.819947	492377.030692	44.640077
3504.003572	492356.085472	44.645082
3504.000018	492381.761820	44.650087
3504.157186	492383.255835	44.655092
3504.108673	492366.753293	44.660097
3503.842050	492354.235401	44.665101
3503.797701	492342.138163	44.670106
3503.987942	492329.446762	44.675111
3504.028697	492328.325715	44.680116
3503.934913	492348.901367	44.685121
3503.559897	492334.222921	44.690125
3503.755153	492325.278347	44.695130
3504.160306	492332.354610	44.700135
3503.879328	492329.613173	44.705140
3503.970062	492337.853285	44.710145
3504.020786	492330.450862	44.715149
3503.840846	492323.996476	44.720154
3504.085839	492310.283537	44.725159
3503.908770	492295.067340	44.730164
3504.065618	492286.331392	44.735169
3503.849246	492292.847531	44.740173
3503.716321	492290.791702	44.745178
3503.939388	492280.677906	44.750183
3503.638511	492287.916415	44.755188
3503.897810	492293.496434	44.760193
3503.911044	492302.559108	44.765197
3503.829603	492301.913165	44.770202
3504.094681	492294.324919	44.775207
3504.032231	492292.004733	44.780212
3503.838383	492278.259840	44.785217
3503.589272	492270.094481	44.790221
3503.828258	492256.027946	44.795226
3504.044342	492249.561588	44.800231
3503.826503	492251.368101	44.805236
3503.971410	492263.246036	44.810241
3504.206389	492236.974973	44.815245
3503.927383	492253.933648	44.820250
3504.106984	492261.146873	44.825255
3503.966522	492264.207249	44.830260
3504.299623	492235.489777	44.835265
3503.910047	492237.829872	44.840269
3503.838381	492234.346327	44.845274
3503.920990	492203.845217	44.850279
3503.793378	492240.379159	44.855284
3504.104386	492215.514076	44.860289
3504.100678	492213.691035	44.865293
3504.077093	492214.251398	44.870298
3503.854448	492215.147084	44.875303
3503.787544	492216.423307	44.880308
3504.006670	492205.347861	44.885313
3503.833371	492192.612535	44.890317
3503.966680	492181.094841	44.895322
3503.974157	492184.385070	44.900327
3503.800487	492184.817221	44.905332
3503.854722	492183.440816	44.910337
3503.785850	492180.767123	44.915341
3503.755902	492177.732770	44.920346
3503.748633	492187.609044	44.925351
3503.609255	492183.984260	44.930356
3504.057998	492183.001300	44.935361
3503.920968	492178.970992	44.940365
3503.965850	492177.899927	44.945370
3504.222638	492165.856270	44.950375
3503.788096	492162.581994	44.955380
3503.805579	492141.257640	44.960385
3503.840282	492137.959842	44.965389
3503.942405	492149.743323	44.970394
3503.947348	492148.678569	44.975399
3503.887722	492148.383681	44.980404
3504.329408	492136.665291	44.985409
3504.002607	492148.516561	44.990413
3503.863375	492163.579397	44.995418
3504.322314	492147.148393	45.000423
3504.022327	492128.457045	45.005428
3504.024487	492105.767681	45.010433
3503.834685	492102.910513	45.015437
3503.891290	492104.876242	45.020442
3503.758904	492129.104617	45.025447
3503.732143	492117.460250	45.030452
3504.026756	492111.133366	45.035457
3504.020310	492106.525319	45.040461
3503.661075	492118.989464	45.045466
3504.228645	492114.442630	45.050471
3504.060495	492105.251521	45.055476
3504.323073	492076.241085	45.060481
3503.918010	492070.531210	45.065485
3504.059339	492070.812291	45.070490
3503.989796	492093.106299	45.075495
3503.881549	492085.171817	45.080500
3503.980740	492063.581239	45.085505
3503.786303	492080.982504	45.090509
3503.634624	492090.324566	45.095514
3503.758943	492068.476802	45.100519
3503.631361	492083.537861	45.105524
3503.702006	492092.591564	45.110529
3503.775345	492085.590624	45.115533
3504.095892	492076.524841	45.120538
3503.973099	492052.183899	45.125543
3503.977945	492038.660648	45.130548
3503.942984	492060.240209	45.135553
3503.917902	492060.547591	45.140557
3504.012662	492051.973279	45.145562
3503.912978	492046.822865	45.150567
3503.733719	492063.917881	45.155572
3504.255471	492044.336913	45.160577
3503.926467	492052.592844	45.165581
3504.080971	492031.651863	45.170586
3504.149156	492005.356191	45.175591
3503.752649	492027.651308	45.180596
3504.213201	492011.928951	45.185601
3504.125038	491993.102701	45.190605
3503.861753	492017.757064	45.195610
3504.371623	492015.548969	45.200615
3504.229526	491997.136403	45.205620
3504.188548	491964.172854	45.210625
3503.643553	491992.113026	45.215629
3503.867436	491953.030259	45.220634
3503.959572	491983.098110	45.225639
3504.169605	491974.454900	45.230644
3503.884606	491968.979241	45.235649
3504.219864	491971.660613	45.240653
3504.152711	491944.322709	45.245658
3504.064285	491935.979874	45.250663
3504.025360	491930.161445	45.255668
3503.916873	491947.802473	45.260673
3504.157944	491938.141449	45.265677
3504.139530	491923.305030	45.270682
3504.155100	491901.727481	45.275687
3503.983187	491904.539663	45.280692
3504.199430	491871.991102	45.285697
3504.342260	491888.275702	45.290701
3503.947754	491897.453659	45.295706
3504.237631	491888.848435	45.300711
3504.062107	491868.769748	45.305716
3504.048039	491858.693203	45.310721
3503.993969	491864.474812	45.315725
3503.871935	491859.783682	45.320730
3504.275306	491856.326279	45.325735
3503.971668	491857.032203	45.330740
3503.931725	491857.797741	45.335745
3504.303240	491850.293784	45.340749
3503.919375	491833.894416	45.345754
3504.170639	491815.723371	45.350759
3504.224406	491815.056041	45.355764
3504.010277	491811.240418	45.360769
3503.828090	491810.711670	45.365773
3503.927341	491814.240684	45.370778
3504.197527	491795.762760	45.375783
3503.966739	491798.280392	45.380788
3504.052309	491779.679694	45.385793
3504.260723	491778.532117	45.390797
3503.951695	491772.908262	45.395802
3504.021921	491777.556062	45.400807
3503.937192	491785.672214	45.405812
3504.222578	491770.635725	45.410817
3504.344643	491751.573425	45.415821
3504.083199	491749.487202	45.420826
3504.247190	491739.382451	45.425831
3503.774089	491742.850001	45.430836
3503.840247	491738.534259	45.435841
3504.014153	491735.467616	45.440845
3503.840523	491716.300078	45.445850
3503.947765	491719.068169	45.450855
3504.009621	491711.815677	45.455860
3504.334972	491710.598969	45.460865
3503.792933	491712.000964	45.465869
3503.783609	491718.687161	45.470874
3503.858682	491710.318385	45.475879
3503.879920	491713.555876	45.480884
3503.846129	491716.346257	45.485889
3504.016892	491712.368493	45.490893
3503.900083	491701.649713	45.495898
3504.211594	491693.040981	45.500903
3504.098407	491678.725799	45.505908
3503.997939	491662.787944	45.510913
3504.004527	491656.709010	45.515917
3503.825895	491664.029729	45.520922
3504.364553	491662.323497	45.525927
3504.194842	491663.058907	45.530932
3504.199752	491650.700209	45.535937
3504.224879	491632.919244	45.540941
3503.938569	491620.606551	45.545946
3504.134031	491627.108479	45.550951
3503.815810	491635.413534	45.555956
3504.336296	491633.507591	45.560961
3504.207668	491601.620810	45.565965
3503.956357	491594.265831	45.570970
3504.265107	491601.813419	45.575975
3503.905945	491600.299724	45.580980
3503.867952	491582.984497	45.585985
3503.926521	491584.494161	45.590989
3504.095435	491592.772891	45.595994
3504.134373	491575.496145	45.600999
3503.886940	491556.593336	45.606004
3504.081201	491540.963316	45.611009
3503.818728	491554.931914	45.616013
3503.770877	491551.292541	45.621018
3504.235563	491550.104448	45.626023
3503.853114	491556.140633	45.631028
3504.020616	491546.389743	45.636033
3503.948783	491543.159324	45.641037
3503.877453	491544.841458	45.646042
3503.999967	491525.728212	45.651047
3504.098602	491523.888929	45.656052
3504.041352	491507.387008	45.661057
3504.335067	491501.161352	45.666061
3503.668387	491519.346816	45.671066
3504.164048	491515.976057	45.676071
3504.187939	491511.413714	45.681076
3504.022730	491486.420343	45.686081
3504.376906	491478.716395	45.691085
3504.359587	491470.412760	45.696090
3504.333641	491476.443273	45.701095
3503.947555	491479.795826	45.706100
3504.177353	491450.029912	45.711105
3504.133327	491441.224025	45.716109
3504.003823	491430.203220	45.721114
3504.043163	491429.335573	45.726119
3503.807672	491435.196633	45.731124
3503.877333	491439.439439	45.736129
3504.012916	491430.149347	45.741133
3503.772255	491440.062903	45.746138
3504.163921	491421.565410	45.751143
3503.912138	491416.185630	45.756148
3503.888093	491392.233390	45.761153
3504.054187	491397.220656	45.766157
3503.595327	491396.127869	45.771162
3503.825296	491393.204248	45.776167
3503.728134	491396.207277	45.781172
3503.572967	491397.598797	45.786177
3503.838632	491405.507797	45.791181
3503.885408	491405.348019	45.796186
3504.338234	491396.919401	45.801191
3503.953720	491403.563715	45.806196
3503.879105	491401.397279	45.811201
3504.208742	491391.164869	45.816205
3503.613771	491368.771568	45.821210
3503.993535	491351.288810	45.826215
3504.151955	491357.188932	45.831220
3504.102075	491358.513168	45.836225
3504.243023	491370.088420	45.841229
3504.422634	491367.831155	45.846234
3504.277736	491334.123227	45.851239
3503.870501	491337.377855	45.856244
3504.145608	491325.938518	45.861249
3504.315268	491317.959788	45.866253
3504.286480	491322.623350	45.871258
3504.277854	491301.150225	45.876263
3503.871298	491288.248561	45.881268
3504.089484	491291.201767	45.886273
3504.312567	491287.367584	45.891277
3504.310746	491294.660503	45.896282
3504.161190	491277.463918	45.901287
3503.959565	491266.049243	45.906292
3504.039786	491244.207486	45.911297
3504.161718	491248.036902	45.916301
3504.138654	491247.179109	45.921306
3504.227998	491241.137607	45.926311
3504.113950	491236.951523	45.931316
3504.283870	491208.410205	45.936321
3504.241579	491203.908893	45.941325
3503.748174	491202.213794	45.946330
3504.240080	491185.624798	45.951335
3504.167709	491195.815765	45.956340
3503.881939	491192.771037	45.961345
3504.073481	491173.697169	45.966349
3503.789534	491167.258820	45.971354
3503.949425	491159.585447	45.976359
3503.827465	491157.932933	45.981364
3503.809675	491157.276889	45.986369
3504.211794	491166.430593	45.991373
3503.815516	491172.621027	45.996378
3503.956102	491159.531508	46.001383
3503.985394	491168.845428	46.006388
3504.153531	491158.131948	46.011393
3504.288817	491136.686537	46.016397
3503.962588	491135.066304	46.021402
3503.984736	491128.731505	46.026407
3503.884091	491116.844958	46.031412
3504.146747	491117.967876	46.036417
3504.159506	491124.600148	46.041421
3504.204354	491117.907230	46.046426
3504.071819	491090.679706	46.051431
3504.097470	491104.248574	46.056436
3504.047089	491100.660160	46.061441
3504.248776	491095.208618	46.066445
3503.929326	491097.183241	46.071450
3504.142145	491086.209424	46.076455
3504.079810	491078.672434	46.081460
3504.121980	491048.935536	46.086465
3503.845571	491054.398006	46.091469
3503.740850	491047.424819	46.096474
3504.080074	491047.877229	46.101479
3504.069193	491046.207149	46.106484
3503.976760	491048.348486	46.111489
3504.056632	491049.095120	46.116493
3503.950225	491044.046786	46.121498
3503.888493	491024.253089	46.126503
3503.956259	491016.239688	46.131508
3504.015921	491014.203926	46.136513
3503.887606	491017.769057	46.141517
3503.684770	491016.382547	46.146522
3504.294861	491016.741502	46.151527
3504.092927	491019.659855	46.156532
3504.143143	491004.204096	46.161537
3504.043102	490995.812030	46.166541
3503.784882	490972.453382	46.171546
3503.893527	490961.749193	46.176551
3503.652057	490964.066036	46.181556
3504.039153	490971.398908	46.186561
3503.943838	490980.428732	46.191565
3503.895660	490974.763410	46.196570
3504.224517	490969.494322	46.201575
3503.832377	490977.608761	46.206580
3503.976173	490982.346426	46.211585
3503.870995	490972.283803	46.216589
3503.869757	490950.961051	46.221594
3503.797747	490946.109843	46.226599
3503.581802	490954.500329	46.231604
3504.033019	490938.424019	46.236609
3504.207667	490937.383023	46.241613
3503.992399	490936.555593	46.246618
3504.414000	490930.056300	46.251623
3504.414724	490937.906077	46.256628
3504.028445	490904.995236	46.261633
3504.080867	490903.213843	46.266637
3504.091063	490898.602868	46.271642
3504.237321	490892.045784	46.276647
3503.651529	490894.822233	46.281652
3503.995456	490891.931173	46.286657
3503.521783	490903.198671	46.291661
3503.947834	490900.041396	46.296666
3504.054075	490891.717976	46.301671
3503.724377	490875.815679	46.306676
3504.093106	490859.296511	46.311681
3503.958104	490850.302135	46.316685
3503.693841	490850.596691	46.321690
3504.317572	490847.306869	46.326695
3503.788333	490864.610233	46.331700
3503.911123	490853.903747	46.336705
3504.130962	490854.982801	46.341709
3503.634423	490844.171602	46.346714
3503.790521	490841.614104	46.351719
3504.013737	490854.594805	46.356724
3503.730470	490854.689774	46.361729
3504.156146	490848.949524	46.366733
3504.106712	490828.799144	46.371738
3503.911287	490825.638782	46.376743
3503.791162	490822.466518	46.381748
3503.883311	490824.781298	46.386753
3504.118253	490816.842686	46.391757
3503.941805	490822.745253	46.396762
3504.275068	490818.994857	46.401767
3503.902905	490801.883665	46.406772
3504.186092	490793.329646	46.411777
3504.044931	490784.842688	46.416781
3503.910840	490783.293353	46.421786
3504.471499	490764.008789	46.426791
3504.004318	490785.607481	46.431796
3504.039846	490767.824052	46.436801
3504.129629	490737.167475	46.441805
3503.905594	490746.470994	46.446810
3503.974234	490730.201732	46.451815
3503.938793	490739.272856	46.456820
3504.196803	490736.091464	46.461825
3504.073829	490739.757098	46.466829
3503.863084	490745.310575	46.471834
3504.503598	490722.265406	46.476839
3504.115388	490712.449967	46.481844
3503.856054	490705.906272	46.486849
3504.294831	490698.593819	46.491853
3504.261337	490702.194671	46.496858
3503.973263	490690.033588	46.501863
3503.922615	490669.832581	46.506868
3504.142131	490650.601817	46.511873
3504.013571	490652.647612	46.516877
3504.014439	490650.823696	46.521882
3504.211995	490652.260821	46.526887
3503.702625	490664.040585	46.531892
3503.356632	490660.853343	46.536897
3503.613219	490649.112633	46.541901
3503.529742	490655.962872	46.546906
3503.523274	490653.279098	46.551911
3503.613261	490655.087760	46.556916
3503.667324	490660.903298	46.561921
3503.749433	490659.522376	46.566925
3503.924612	490658.937113	46.571930
3504.049041	490651.421082	46.576935
3503.850049	490655.554580	46.581940
3503.770475	490664.683364	46.586945
3504.235262	490651.998086	46.591949
3504.157107	490648.262030	46.596954
3504.200786	490626.324033	46.601959
3504.015946	490622.250296	46.606964
3504.161131	490607.235034	46.611969
3504.211329	490615.127775	46.616973
3503.856167	490628.351987	46.621978
3503.954954	490602.961177	46.626983
3503.852410	490591.429135	46.631988
3503.720997	490573.216071	46.636993
3503.967473	490570.492308	46.641997
3503.529624	490572.232455	46.647002
3503.812903	490571.731402	46.652007
3504.058755	490566.171431	46.657012
3503.938938	490571.356050	46.662017
3503.895656	490570.248180	46.667021
3503.653695	490569.526248	46.672026
3504.158850	490563.114921	46.677031
3504.058509	490572.196384	46.682036
3503.726864	490578.781983	46.687041
3504.277062	490568.412971	46.692045
3503.877208	490551.660466	46.697050
3503.512861	490542.246353	46.702055
3503.604174	490540.154890	46.707060
3503.609385	490533.012192	46.712065
3504.007264	490540.394179	46.717069
3503.832952	490538.648586	46.722074
3504.213118	490531.902464	46.727079
3504.047791	490541.753938	46.732084
3504.201356	490540.513659	46.737089
3504.286574	490540.094556	46.742093
3504.178595	490531.754185	46.747098
3504.099119	490496.616256	46.752103
3503.881317	490502.778701	46.757108
3503.840467	490494.832893	46.762113
3503.895463	490500.496388	46.767117
3503.592506	490502.063276	46.772122
3504.091332	490486.333596	46.777127
3504.154578	490504.708568	46.782132
3503.957306	490501.193903	46.787137
3503.848789	490500.602824	46.792141
3503.723936	490498.292277	46.797146
3503.984048	490493.185868	46.802151
3503.865651	490479.832915	46.807156
3503.931876	490469.742933	46.812161
3504.203745	490467.622926	46.817165
3503.885878	490469.090876	46.822170
3504.240042	490476.530446	46.827175
3504.291443	490471.254422	46.832180
3504.340381	490471.600780	46.837185
3504.009494	490441.111503	46.842189
3503.948485	490435.346748	46.847194
3504.235647	490427.703611	46.852199
3504.222489	490430.744165	46.857204
3504.076998	490429.449846	46.862209
3504.153071	490409.481776	46.867213
3503.742463	490405.241078	46.872218
3503.991543	490388.487163	46.877223
3503.999997	490382.103628	46.882228
3504.068952	490394.349295	46.887233
3503.842603	490386.989895	46.892237
3503.932085	490396.497281	46.897242
3504.257599	490390.620776	46.902247
3504.177773	490395.090039	46.907252
3504.035747	490363.963002	46.912257
3504.251304	490350.101338	46.917261
3504.105895	490354.986167	46.922266
3504.159795	490354.116169	46.927271
3504.188623	490345.855392	46.932276
3504.133532	490336.797491	46.937281
3504.041073	490319.439057	46.942285
3503.842680	490318.254389	46.947290
3504.311667	490308.657805	46.952295
3503.485078	490317.651574	46.957300
3503.797274	490318.716063	46.962305
3504.147757	490310.303137	46.967309
3503.586258	490308.416119	46.972314
3503.873924	490310.092274	46.977319
3503.749959	490311.478943	46.982324
3503.857898	490303.104345	46.987329
3503.900592	490310.390611	46.992333
3503.901980	490307.148407	46.997338
3504.182608	490280.411548	47.002343
3503.992580	490269.703520	47.007348
3503.981833	490267.830753	47.012353
3504.182766	490264.151811	47.017357
3503.745001	490270.804938	47.022362
3504.302078	490263.878813	47.027367
3503.986744	490269.702205	47.032372
3503.833809	490253.214303	47.037377
3503.904584	490246.314380	47.042381
3503.706481	490237.127086	47.047386
3503.768223	490223.745481	47.052391
3503.784692	490230.428132	47.057396
3503.946221	490231.617737	47.062401
3504.088293	490222.579270	47.067405
3503.955806	490229.943902	47.072410
3504.145573	490220.492702	47.077415
3504.054399	490224.507956	47.082420
3504.048682	490221.317508	47.087425
3504.127310	490198.107257	47.092429
3503.989612	490195.089612	47.097434
3504.273152	490196.715780	47.102439
3504.011348	490192.654114	47.107444
3503.990174	490193.973895	47.112449
3504.316168	490183.589458	47.117453
3503.920365	490180.865850	47.122458
3504.031585	490160.588065	47.127463
3504.337974	490150.915801	47.132468
3504.184708	490145.013589	47.137473
3504.187154	490149.621856	47.142477
3503.762888	490149.688462	47.147482
3504.232585	490142.168309	47.152487
3504.093914	490130.540395	47.157492
3504.173527	490112.141584	47.162497
3504.456956	490100.700188	47.167501
3503.944384	490109.137931	47.172506
3504.088476	490114.686161	47.177511
3503.976357	490094.342303	47.182516
3503.959422	490080.415886	47.187521
3504.154389	490068.127407	47.192525
3504.109561	490077.554882	47.197530
3504.294206	490067.040771	47.202535
3503.969837	490072.055257	47.207540
3503.906077	490068.570059	47.212545
3504.264892	490056.356977	47.217549
3504.137773	490043.612889	47.222554
3504.045151	490030.913990	47.227559
3504.228317	490019.488391	47.232564
3504.099117	490018.090168	47.237569
3504.177872	490025.573445	47.242573
3504.148738	490006.178722	47.247578
3503.873291	489984.341063	47.252583
3503.739519	489987.350101	47.257588
3503.610606	489990.560971	47.262593
3503.905200	489984.891826	47.267597
3503.729982	489985.780119	47.272602
3504.260003	489972.577577	47.277607
3503.992630	489983.255869	47.282612
3504.066603	489992.310061	47.287617
3504.117663	489978.727371	47.292621
3503.713270	489966.330952	47.297626
3504.126944	489944.738885	47.302631
3503.809274	489935.823590	47.307636
3503.797565	489932.887291	47.312641
3503.972399	489936.607314	47.317645
3503.890801	489943.761416	47.322650
3504.133686	489940.177081	47.327655
3503.846162	489939.158424	47.332660
3503.985753	489936.400814	47.337665
3503.999295	489936.803426	47.342669
3503.861667	489938.090981	47.347674
3504.095191	489925.998916	47.352679
3503.989253	489903.222672	47.357684
3503.943385	489904.141175	47.362689
3504.103258	489897.125744	47.367693
3503.905956	489892.395365	47.372698
3503.968508	489897.956547	47.377703
3503.872754	489897.566032	47.382708
3503.843237	489900.811858	47.387713
3504.108558	489890.335549	47.392717
3503.933436	489886.665317	47.397722
3504.098717	489856.957728	47.402727
3504.186409	489852.790101	47.407732
3503.740996	489857.165320	47.412737
3503.942452	489845.128922	47.417741
3503.924677	489845.080634	47.422746
3503.897787	489849.389709	47.427751
3503.681355	489859.148315	47.432756
3504.040649	489859.445635	47.437761
3503.896733	489843.158550	47.442765
3503.533422	489860.537910	47.447770
3503.676961	489856.209506	47.452775
3503.975942	489864.063243	47.457780
3503.879519	489859.013011	47.462785
3503.907163	489840.571499	47.467789
3503.658011	489834.988246	47.472794
3504.040669	489823.834902	47.477799
3503.840964	489832.831124	47.482804
3503.959850	489825.518241	47.487809
3504.450605	489827.061043	47.492813
3504.034265	489830.874519	47.497818
3503.816801	489823.918696	47.502823
3503.994811	489822.826458	47.507828
3504.133548	489804.975157	47.512833
3503.956659	489791.377708	47.517837
3504.153687	489785.420022	47.522842
3504.238055	489774.313792	47.527847
3503.827855	489783.951110	47.532852
3503.846151	489797.319482	47.537857
3504.247190	489777.856538	47.542861
3504.118027	489775.141379	47.547866
3504.217899	489765.754809	47.552871
3504.017653	489749.729798	47.557876
3504.169479	489751.123570	47.562881
3504.184812	489753.855827	47.567885
3503.843260	489750.870329	47.572890
3504.232843	489733.637773	47.577895
3503.877337	489711.457896	47.582900
3503.811077	489697.893546	47.587905
3504.044768	489696.893802	47.592909
3503.821814	489700.778042	47.597914
3503.740246	489709.147843	47.602919
3503.906440	489702.637847	47.607924
3503.694674	489699.024020	47.612929
3503.624495	489705.264695	47.617933
3503.787603	489695.868096	47.622938
3503.767264	489701.594389	47.627943
3503.750125	489694.910762	47.632948
3503.749964	489697.797428	47.637953
3503.925110	489691.589917	47.642957
3504.289868	489695.583876	47.647962
3504.105178	489686.242240	47.652967
3504.047446	489675.512965	47.657972
3503.785884	489674.236937	47.662977
3503.895732	489667.381278	47.667981
3503.806475	489664.710447	47.672986
3503.778356	489657.015527	47.677991
3503.688731	489660.574798	47.682996
3503.559409	489666.926135	47.688001
3503.677381	489659.106825	47.693005
3503.566476	489661.504492	47.698010
3503.698511	489664.522222	47.703015
3503.734786	489664.516042	47.708020
3503.687466	489667.004960	47.713025
3503.692227	489665.585539	47.718029
3503.651659	489674.860589	47.723034
3503.875518	489667.328452	47.728039
3503.761767	489669.625266	47.733044
3503.827205	489661.358403	47.738049
3504.056643	489663.651629	47.743053
3503.838614	489667.636399	47.748058
3503.863062	489671.684148	47.753063
3503.910886	489666.155210	47.758068
3503.969522	489673.236600	47.763073
3504.130227	489649.202290	47.768077
3503.700390	489636.910976	47.773082
3503.990479	489624.201969	47.778087
3504.116946	489624.941297	47.783092
3503.780770	489622.005579	47.788097
3503.819641	489621.847035	47.793101
3503.824885	489625.999130	47.798106
3503.725198	489622.114321	47.803111
3503.606205	489635.504506	47.808116
3503.808950	489632.230361	47.813121
3503.937246	489622.636625	47.818125
3503.801245	489630.913762	47.823130
3503.933555	489636.666600	47.828135
3504.145241	489626.147971	47.833140
3503.617329	489628.206341	47.838145
3504.140868	489612.218775	47.843149
3503.736215	489603.367720	47.848154
3503.892559	489596.656640	47.853159
3503.890158	489597.264383	47.858164
3503.909305	489604.301389	47.863169
3504.009107	489584.936506	47.868173
3503.976232	489598.313107	47.873178
3503.970284	489599.883778	47.878183
3503.952729	489587.527274	47.883188
3503.880179	489590.425397	47.888193
3504.221183	489579.987606	47.893197
3503.910043	489568.741159	47.898202
3504.014458	489553.731503	47.903207
3503.975566	489553.534598	47.908212
3503.922236	489545.590361	47.913217
3504.084460	489542.575861	47.918221
3503.751878	489561.926031	47.923226
3503.892201	489553.647285	47.928231
3504.057827	489547.998393	47.933236
3503.796108	489554.522645	47.938241
3503.729306	489549.974160	47.943245
3503.938151	489532.415428	47.948250
3504.042666	489511.580843	47.953255
3504.269660	489507.492426	47.958260
3504.017291	489503.631723	47.963265
3504.163349	489508.723962	47.968269
3504.029762	489516.494255	47.973274
3504.294767	489500.192897	47.978279
3504.285202	489487.075295	47.983284
3504.099041	489479.962444	47.988289
3504.243959	489459.678580	47.993293
3504.280468	489470.663694	47.998298
3503.954837	489463.724833	48.003303
3503.825178	489443.484347	48.008308
3503.871063	489429.547520	48.013313
3503.847732	489417.748982	48.018317
3503.813152	489433.709191	48.023322
3503.934861	489422.748807	48.028327
3504.062878	489423.032036	48.033332
3504.040541	489429.265241	48.038337
3504.032365	489424.758111	48.043341
3503.802175	489421.957565	48.048346
3503.884191	489412.522991	48.053351
3503.890753	489420.980294	48.058356
3503.806374	489417.852794	48.063361
3503.956801	489397.416039	48.068365
3503.871065	489396.973278	48.073370
3503.580214	489384.609182	48.078375
3503.896345	489383.495090	48.083380
3503.668517	489386.569740	48.088385
3503.908504	489383.593576	48.093389
3503.770123	489380.981120	48.098394
3503.848665	489381.221517	48.103399
3503.765162	489379.917327	48.108404
3503.796757	489381.330129	48.113409
3503.816235	489377.780996	48.118413
3503.763335	489387.463349	48.123418
3504.047611	489376.629200	48.128423
3504.177811	489381.166812	48.133428
3504.066040	489377.942332	48.138433
3503.986601	489364.177219	48.143437
3503.970821	489359.215411	48.148442
3503.680624	489350.903316	48.153447
3503.636818	489352.479991	48.158452
3503.685949	489349.382031	48.163457
3504.110054	489346.022201	48.168461
3503.699237	489355.963743	48.173466
3503.824177	489360.907405	48.178471
3503.722302	489359.707420	48.183476
3503.933755	489349.543236	48.188481
3503.972326	489344.167621	48.193485
3503.870980	489360.442354	48.198490
3503.898204	489354.612672	48.203495
3503.908707	489358.358781	48.208500
3503.868470	489362.720729	48.213505
3504.183775	489331.975573	48.218509
3503.961638	489323.905967	48.223514
3503.893113	489305.580435	48.228519
3503.971532	489313.570564	48.233524
3504.281123	489307.240376	48.238529
3503.815060	489305.084911	48.243533
3504.006736	489302.825494	48.248538
3503.954223	489311.292183	48.253543
3503.863346	489304.772027	48.258548
3503.655411	489300.397742	48.263553
3504.032442	489278.861358	48.268557
3503.533882	489281.826858	48.273562
3503.529406	489269.822641	48.278567
3503.715320	489280.075127	48.283572
3503.956039	489271.577784	48.288577
3503.842778	489271.240674	48.293581
3503.562193	489281.769494	48.298586
3503.739287	489258.745133	48.303591
3503.925134	489263.425934	48.308596
3503.788041	489263.903020	48.313601
3503.977117	489268.735266	48.318605
3503.741949	489277.889311	48.323610
3503.660514	489280.383672	48.328615
3503.675795	489283.825131	48.333620
3503.763312	489276.770253	48.338625
3503.664398	489270.453962	48.343629
3503.637585	489282.208970	48.348634
3503.720608	489269.988317	48.353639
3503.963061	489277.142108	48.358644
3503.652288	489282.357259	48.363649
3503.919784	489278.667606	48.368653
3503.555322	489280.143010	48.373658
3503.631851	489285.955423	48.378663
3504.024924	489286.753932	48.383668
3503.832627	489278.223725	48.388673
3503.843836	489273.966755	48.393677
3503.436215	489284.110437	48.398682
3503.571007	489272.236166	48.403687
3503.885652	489278.416162	48.408692
3503.606939	489274.762182	48.413697
3503.801683	489281.720904	48.418701
3503.624187	489281.647205	48.423706
3504.002250	489282.498739	48.428711
3503.818715	489282.122084	48.433716
3503.771257	489280.406976	48.438721
3504.158273	489281.561006	48.443725
3504.066910	489265.062508	48.448730
3503.994573	489252.511835	48.453735
3503.722343	489240.296657	48.458740
3503.849939	489241.846252	48.463745
3503.804235	489243.777800	48.468749
3503.817483	489247.776757	48.473754
3503.645207	489249.880264	48.478759
3503.901196	489249.130233	48.483764
3504.020056	489245.008198	48.488769
3504.103287	489235.623995	48.493773
3503.761088	489248.745819	48.498778
3503.650800	489239.493506	48.503783
3503.846235	489249.187334	48.508788
3503.492214	489248.077844	48.513793
3504.004052	489244.146960	48.518797
3503.705202	489252.095437	48.523802
3503.873485	489237.379347	48.528807
3503.729881	489228.182946	48.533812
3503.708965	489215.877381	48.538817
3503.976008	489213.504739	48.543821
3503.670506	489220.187981	48.548826
3503.851663	489207.394607	48.553831
3503.945238	489217.003245	48.558836
3503.458523	489215.256249	48.563841
3503.575382	489207.234321	48.568845
3503.948118	489214.266241	48.573850
3503.786736	489212.467828	48.578855
3503.789363	489234.449909	48.583860
3503.717892	489227.521443	48.588865
3503.712565	489216.175802	48.593869
3503.417987	489231.518797	48.598874
3503.459173	489213.986268	48.603879
3503.501335	489232.163204	48.608884
3503.951430	489224.088617	48.613889
3503.791542	489218.136509	48.618893
3503.798178	489223.959987	48.623898
3503.552213	489226.784269	48.628903
3503.886578	489227.034889	48.633908
3503.748309	489214.798522	48.638913
3504.154506	489223.446014	48.643917
3503.822949	489233.679004	48.648922
3503.790799	489232.721252	48.653927
3504.009726	489216.274976	48.658932
3503.837819	489239.247022	48.663937
3503.975546	489219.774468	48.668941
3503.788184	489224.564915	48.673946
3503.943941	489230.719386	48.678951
3504.205211	489194.866703	48.683956
3503.885323	489176.074252	48.688961
3503.931943	489178.041867	48.693965
3503.658289	489185.631825	48.698970
3504.013764	489182.890638	48.703975
3503.985560	489175.955316	48.708980
3503.750685	489175.840033	48.713985
3503.730808	489172.043821	48.718989
3503.767257	489191.943870	48.723994
3503.964391	489161.875591	48.728999
3503.962691	489195.457729	48.734004
3503.669042	489183.549812	48.739009
3503.886305	489172.776790	48.744013
3504.075511	489172.999699	48.749018
3503.705808	489157.203575	48.754023
3503.779834	489154.202953	48.759028
3503.707455	489149.908513	48.764033
3503.744359	489145.799409	48.769037
3503.833431	489152.774880	48.774042
3504.051671	489143.673207	48.779047
3504.187790	489133.571465	48.784052
3503.749335	489164.588771	48.789057
3504.360926	489125.489508	48.794061
3504.095572	489156.428817	48.799066
3503.614742	489128.746980	48.804071
3504.031070	489110.699196	48.809076
3503.652574	489113.899006	48.814081
3503.854446	489107.535124	48.819085
3503.504478	489114.782605	48.824090
3503.334119	489104.526676	48.829095
3503.506496	489117.010089	48.834100
3503.669580	489137.903226	48.839105
3503.992905	489151.730368	48.844109
3504.143523	489123.442204	48.849114
3503.960939	489116.581912	48.854119
3504.045873	489127.306310	48.859124
3504.102182	489117.115868	48.864129
3504.020644	489098.336322	48.869133
3503.870185	489122.216861	48.874138
3504.085144	489119.345917	48.879143
3503.925063	489099.819002	48.884148
3503.616444	489102.399943	48.889153
3503.867919	489058.697448	48.894157
3503.455809	489083.835045	48.899162
3503.511344	489076.076014	48.904167
3503.879731	489079.613661	48.909172
3503.488025	489104.089527	48.914177
3503.528205	489077.996796	48.919181
3503.780020	489120.757722	48.924186
3503.643953	489117.790298	48.929191
3503.955389	489111.814319	48.934196
3503.556285	489111.573034	48.939201
3504.000821	489087.341195	48.944205
3503.906051	489091.762476	48.949210
3503.683328	489085.212429	48.954215
3503.976366	489082.531748	48.959220
3503.823791	489079.364318	48.964225
3503.810682	489071.616134	48.969229
3503.693769	489085.006380	48.974234
3503.806345	489084.734879	48.979239
3504.102938	489078.558625	48.984244
3503.912979	489089.174534	48.989249
3503.846455	489080.421750	48.994253
3503.837892	489082.803315	48.999258
3503.495182	489083.464859	49.004263
3503.701954	489080.392593	49.009268
3504.077377	489079.573027	49.014273
3503.925889	489085.472190	49.019277
3503.994109	489087.487053	49.024282
3504.023284	489057.901025	49.029287
3504.099558	489043.300630	49.034292
3503.712916	489043.715856	49.039297
3503.865713	489032.294462	49.044301
3504.229988	489036.389943	49.049306
3504.191501	489028.645753	49.054311
3503.853043	489031.687292	49.059316
3503.830969	489050.127818	49.064321
3504.099853	489033.622836	49.069325
3503.863483	489021.908373	49.074330
3503.951978	489005.178613	49.079335
3504.030064	489002.329283	49.084340
3503.890032	489005.997949	49.089345
3503.918593	488998.141845	49.094349
3503.484289	489010.265339	49.099354
3503.505572	489009.653697	49.104359
3503.992773	489003.345990	49.109364
3503.714506	488995.234462	49.114369
3503.906152	488997.432438	49.119373
3504.024489	489001.668101	49.124378
3503.831213	489008.485639	49.129383
3504.196317	489002.501143	49.134388
3503.734312	488984.744013	49.139393
3503.874049	488966.638501	49.144397
3503.791329	488964.776979	49.149402
3503.840672	488957.576058	49.154407
3504.088208	488951.356864	49.159412
3503.798584	488968.016258	49.164417
3504.205923	488962.328991	49.169421
3503.821201	488949.118350	49.174426
3503.852665	488972.159884	49.179431
3504.119131	488951.754961	49.184436
3504.052149	488956.931671	49.189441
3503.988003	488943.315792	49.194445
3504.264535	488929.088881	49.199450
3504.058623	488921.016538	49.204455
3504.328271	488921.631960	49.209460
3504.040483	488919.752192	49.214465
3504.391169	488905.361585	49.219469
3504.182385	488906.052621	49.224474
3504.245711	488880.817058	49.229479
3504.002747	488875.941682	49.234484
3503.649323	488875.186645	49.239489
3504.019220	488863.832144	49.244493
3503.933969	488879.041035	49.249498
3503.957920	488876.909381	49.254503
3504.060363	488864.888010	49.259508
3503.644139	488852.138156	49.264513
3504.151027	488834.278409	49.269517
3504.070997	488828.972045	49.274522
3503.506552	488827.135992	49.279527
3503.790976	488822.379862	49.284532
3503.952675	488827.723078	49.289537
3503.928686	488830.157766	49.294541
3503.921100	488834.210756	49.299546
3503.952587	488832.635090	49.304551
3503.812846	488828.300570	49.309556
3503.685250	488841.490064	49.314561
3504.128222	488828.452444	49.319565
3503.950967	488836.837754	49.324570
3503.860511	488817.704767	49.329575
3504.290733	488800.667554	49.334580
3504.049785	488788.953670	49.339585
3504.119621	488790.411126	49.344589
3503.770321	488790.972414	49.349594
3503.867756	488789.690240	49.354599
3504.144614	488788.835587	49.359604
3504.251089	488797.176072	49.364609
3504.281342	488769.109015	49.369613
3504.093738	488765.440536	49.374618
3503.736348	488761.241706	49.379623
3503.933069	488752.599126	49.384628
3503.627206	488757.307112	49.389633
3504.209083	488749.363456	49.394637
3504.227150	488756.147682	49.399642
3503.968440	488741.093465	49.404647
3504.031499	488716.262952	49.409652
3504.125925	488719.540045	49.414657
3504.253872	488704.171423	49.419661
3504.084387	488712.758173	49.424666
3504.035478	488706.940324	49.429671
3504.093989	488700.345696	49.434676
3503.757078	488670.158426	49.439681
3503.805559	488678.761397	49.444685
3503.839781	488664.218010	49.449690
3503.827986	488667.714513	49.454695
3504.185339	488655.196840	49.459700
3503.551055	488668.415880	49.464705
3503.880629	488674.036528	49.469709
3504.153364	488671.865533	49.474714
3503.936776	488672.405850	49.479719
3503.931084	488671.697154	49.484724
3503.990671	488677.968312	49.489729
3504.210710	488651.643956	49.494733
3503.720389	488637.082142	49.499738
3503.697322	488620.470982	49.504743
3504.017081	488635.919979	49.509748
3503.806307	488628.912004	49.514753
3504.236153	488620.637748	49.519757
3504.179784	488621.709933	49.524762
3503.863266	488638.779095	49.529767
3504.027739	488618.491241	49.534772
3503.856668	488628.851154	49.539777
3503.781730	488629.065164	49.544781
3503.943807	488602.952514	49.549786
3503.895298	488607.873132	49.554791
3504.194392	488594.756784	49.559796
3503.723158	488608.000750	49.564801
3504.019279	488603.799908	49.569805
3503.934989	488598.646114	49.574810
3503.648401	488590.535727	49.579815
3503.928667	488612.879878	49.584820
3503.984548	488612.161449	49.589825
3504.144730	488590.810517	49.594829
3503.983360	488573.866599	49.599834
3503.987898	488574.675893	49.604839
3504.302702	488561.709001	49.609844
3503.970287	488563.787238	49.614849
3503.770219	488549.382099	49.619853
3504.076859	488555.715559	49.624858
3503.768393	488551.762218	49.629863
3504.112088	488537.878976	49.634868
3503.777120	488553.279556	49.639873
3504.070249	488537.226194	49.644877
3503.656236	488519.866272	49.649882
3503.605291	488510.198994	49.654887
3503.955399	488504.875212	49.659892
3503.834914	488505.400346	49.664897
3503.876950	488509.901448	49.669901
3503.922311	488509.995139	49.674906
3504.124107	488496.184947	49.679911
3504.048914	488520.105002	49.684916
3504.111563	488509.761271	49.689921
3503.972569	488500.513134	49.694925
3503.892520	488501.538415	49.699930
3503.981628	488491.443761	49.704935
3503.933072	488473.114268	49.709940
3503.848191	488465.073256	49.714945
3503.836159	488458.844271	49.719949
3503.829116	488459.554092	49.724954
3503.778441	488459.561654	49.729959
3503.667825	488459.629342	49.734964
3503.829387	488466.441647	49.739969
3504.082937	488458.043222	49.744973
3504.123193	488467.761975	49.749978
3503.954240	488471.131391	49.754983
3503.967312	488462.163126	49.759988
3503.781330	488439.651039	49.764993
3503.942020	488432.027088	49.769997
3503.789883	488432.607879	49.775002
3503.934764	488430.659680	49.780007
3504.158571	488429.509472	49.785012
3503.798156	488434.935316	49.790017
3503.692549	488418.590294	49.795021
3503.587688	488447.124652	49.800026
3503.740291	488444.820656	49.805031
3504.166263	488429.809943	49.810036
3503.705407	488433.630732	49.815041
3503.681058	488434.090019	49.820045
3503.790290	488433.211189	49.825050
3503.748593	488436.003304	49.830055
3503.744324	488432.508402	49.835060
3503.816188	488434.674721	49.840065
3504.119695	488426.217732	49.845069
3503.876330	488416.276892	49.850074
3503.711973	488407.640567	49.855079
3504.041776	488387.073065	49.860084
3503.891841	488396.923222	49.865089
3503.933235	488393.573058	49.870093
3503.698461	488393.305791	49.875098
3503.878247	488393.935433	49.880103
3504.110557	488387.465191	49.885108
3503.668397	488388.800979	49.890113
3503.690572	488384.947309	49.895117
3503.938527	488388.808045	49.900122
3503.867871	488392.617827	49.905127
3504.100073	488394.505539	49.910132
3504.238387	488390.532208	49.915137
3504.104785	488353.575297	49.920141
3504.214374	488355.938280	49.925146
3504.063667	488345.526870	49.930151
3504.171307	488343.280622	49.935156
3503.917368	488357.554159	49.940161
3504.238591	488334.860479	49.945165
3503.981485	488328.720838	49.950170
3504.069293	488313.662170	49.955175
3504.087152	488311.936651	49.960180
3503.705676	488309.565084	49.965185
3503.815184	488305.748250	49.970189
3503.711123	488317.313447	49.975194
3503.884736	488306.496178	49.980199
3503.842735	488305.337318	49.985204
3503.666658	488309.417050	49.990209
3503.906801	488309.986501	49.995213
3504.019871	488305.814524	50.000218
3503.807663	488305.391725	50.005223
3504.010546	488306.321647	50.010228
3504.083731	488284.426923	50.015233
3503.812778	488273.426624	50.020237
3503.965185	488258.813594	50.025242
3503.931880	488254.563430	50.030247
3503.934601	488267.580762	50.035252
3503.834850	488268.203934	50.040257
3503.837836	488259.389130	50.045261
3503.944616	488266.007548	50.050266
3503.670806	488270.052079	50.055271
3503.868898	488265.005530	50.060276
3503.761190	488272.012425	50.065281
3503.726595	488270.345847	50.070285
3503.933070	488272.136328	50.075290
3504.048971	488267.457350	50.080295
3504.380354	488236.302644	50.085300
3503.969072	488234.341014	50.090305
3504.210462	488219.156689	50.095309
3504.063361	488221.560258	50.100314
3503.975797	488231.451297	50.105319
3504.195980	488218.144543	50.110324
3504.070831	488198.003323	50.115329
3503.973588	488189.153673	50.120333
3504.128572	488186.393376	50.125338
3503.988612	488183.021183	50.130343
3504.155378	488191.403061	50.135348
3503.978338	488194.419220	50.140353
3504.231050	488177.206885	50.145357
3504.326080	488151.205521	50.150362
3504.001997	488155.156713	50.155367
3504.055854	488141.116370	50.160372
3504.188863	488147.072171	50.165377
3504.250149	488136.272558	50.170381
3504.236345	488132.728453	50.175386
3503.999493	488109.768121	50.180391
3504.239055	488093.570887	50.185396
3503.694936	488116.400497	50.190401
3503.731613	488110.113045	50.195405
3503.981965	488102.778721	50.200410
3503.709317	488107.582928	50.205415
3504.001282	488107.789611	50.210420
3503.801874	488106.250377	50.215425
3503.901104	488094.684920	50.220429
3503.644055	488086.569648	50.225434
3503.746964	488058.084817	50.230439
3504.091055	488056.206406	50.235444
3503.536025	488060.903288	50.240449
3503.765801	488055.750365	50.245453
3504.031338	488051.250305	50.250458
3503.793090	488060.658697	50.255463
3503.731901	488048.865291	50.260468
3503.758963	488057.775858	50.265473
3503.768743	488047.490886	50.270477
3503.757910	488057.724475	50.275482
3503.879371	488052.183429	50.280487
3504.068032	488045.669315	50.285492
3503.816054	488060.753246	50.290497
3504.044972	488058.791727	50.295501
3503.970384	488053.433632	50.300506
3504.063556	488042.223686	50.305511
3504.120995	488015.822837	50.310516
3503.901940	488023.252663	50.315521
3503.815276	488016.022225	50.320525
3504.083212	488016.080742	50.325530
3503.825450	488007.155066	50.330535
3504.318349	488009.862754	50.335540
3504.204427	488008.006069	50.340545
3504.119232	487982.792787	50.345549
3503.988350	487970.706415	50.350554
3503.959825	487970.558509	50.355559
3503.720454	487960.870076	50.360564
3503.880753	487967.074896	50.365569
3503.937112	487967.521439	50.370573
3504.258003	487966.761103	50.375578
3504.026657	487966.341320	50.380583
3504.340020	487951.145408	50.385588
3504.323437	487947.399085	50.390593
3504.180914	487938.455164	50.395597
3504.316731	487940.155534	50.400602
3504.489049	487928.781047	50.405607
3504.109678	487901.790556	50.410612
3503.920526	487892.904638	50.415617
3504.055668	487892.477588	50.420621
3504.320061	487880.885898	50.425626
3504.103703	487888.011417	50.430631
3504.441684	487881.524303	50.435636
3503.883662	487863.021462	50.440641
3504.110977	487852.144793	50.445645
3504.264821	487852.373309	50.450650
3503.930683	487846.346997	50.455655
3503.995969	487844.613941	50.460660
3504.000314	487848.867878	50.465665
3503.817387	487812.272300	50.470669
3503.798762	487807.209225	50.475674
3503.407714	487811.778939	50.480679
3503.856667	487796.612129	50.485684
3503.905315	487799.288748	50.490689
3503.831547	487803.403074	50.495693
3503.781047	487806.297984	50.500698
3504.029840	487818.972798	50.505703
3503.958177	487798.468111	50.510708
3503.804797	487813.536655	50.515713
3503.895599	487804.657106	50.520717
3503.868315	487807.041790	50.525722
3503.730508	487812.381972	50.530727
3503.742645	487787.811573	50.535732
3503.736724	487780.517628	50.540737
3503.664926	487738.788109	50.545741
3503.565221	487697.113566	50.550746
3503.614685	487644.980191	50.555751
3503.828681	487581.169719	50.560756
3503.645155	487501.363747	50.565761
3503.677329	487416.812271	50.570765
3503.536152	487316.330862	50.575770
3503.150680	487212.240208	50.580775
3503.254017	487098.649421	50.585780
3502.719447	486977.813379	50.590785
3502.565559	486844.910400	50.595789
3502.394681	486701.826797	50.600794
3502.045374	486566.267858	50.605799
3501.984436	486414.805995	50.610804
3501.674064	486254.922167	50.615809
3501.537670	486079.760766	50.620813
3501.229733	485908.627078	50.625818
3501.075242	485731.894882	50.630823
3501.228774	485527.755053	50.635828
3501.047704	485337.091445	50.640833
3500.574950	485118.202213	50.645837
3500.361795	484903.677183	50.650842
3499.780828	484676.693900	50.655847
3499.748365	484444.909456	50.660852
3499.414111	484214.081907	50.665857
3499.092889	483972.964388	50.670861
3499.059938	483719.233026	50.675866
3498.066150	483465.447540	50.680871
3497.820371	483198.265546	50.685876
3497.878329	482930.322523	50.690881
3497.390467	482661.246023	50.695885
3496.600674	482388.311948	50.700890
3496.239395	482106.438968	50.705895
3496.181948	481809.160466	50.710900
3495.332193	481524.366699	50.715905
3494.789758	481232.121979	50.720909
3495.010296	480937.167970	50.725914
3494.260963	480628.173981	50.730919
3493.690681	480308.809089	50.735924
3493.327108	479991.990845	50.740929
3492.776645	479676.007897	50.745933
3492.569670	479356.367502	50.750938
3492.006304	479026.541215	50.755943
3491.716921	478688.709482	50.760948
3490.923176	478356.932008	50.765953
3490.675321	478018.575550	50.770957
3490.241815	477670.359711	50.775962
3489.199861	477319.547788	50.780967
3488.877189	476965.372276	50.785972
3488.127583	476623.473010	50.790977
3487.937268	476269.162947	50.795981
3487.322788	475916.637038	50.800986
3486.843510	475552.729641	50.805991
3486.643801	475187.453616	50.810996
3485.739344	474819.950696	50.816001
3485.282520	474441.573378	50.821005
3484.913967	474063.681984	50.826010
3484.144657	473691.828586	50.831015
3483.708182	473315.404140	50.836020
3482.809524	472937.271538	50.841025
3482.487970	472550.574714	50.846029
3481.518332	472174.771245	50.851034
3481.072583	471782.807259	50.856039
3480.691545	471399.292109	50.861044
3479.792067	471014.888515	50.866049
3479.201245	470628.502418	50.871053
3479.092796	470223.932804	50.876058
3478.063442	469836.587285	50.881063
3477.776479	469430.915048	50.886068
3477.022218	469027.539746	50.891073
3476.539173	468626.598318	50.896077
3475.724769	468229.301683	50.901082
3474.879228	467825.004986	50.906087
3474.891330	467411.082700	50.911092
3473.956541	467005.922381	50.916097
3473.121459	466611.641035	50.921101
3472.622486	466197.065853	50.926106
3471.837424	465788.765284	50.931111
3471.241483	465386.918152	50.936116
3470.311904	464976.444243	50.941121
3469.919440	464561.820429	50.946125
3469.352037	464153.302059	50.951130
3468.223139	463745.574699	50.956135
3468.195670	463334.926801	50.961140
3467.308409	462923.392635	50.966145
3466.824137	462511.178312	50.971149
3466.189475	462094.973048	50.976154
3465.520001	461676.077108	50.981159
3464.850320	461253.724054	50.986164
3464.325102	460852.542139	50.991169
3463.567109	460418.469929	50.996173
3462.753624	460007.376228	51.001178
3461.850356	459588.680170	51.006183
3461.536300	459172.520807	51.011188
3460.680865	458765.164328	51.016193
3459.918673	458335.617221	51.021197
3459.606742	457918.774478	51.026202
3458.674261	457503.442464	51.031207
3457.861660	457087.931565	51.036212
3457.127960	456677.625901	51.041217
3456.442320	456253.099790	51.046221
3455.502389	455845.956967	51.051226
3454.678125	455434.932618	51.056231
3454.229924	455004.104976	51.061236
3453.531678	454605.019325	51.066241
3452.863225	454203.638726	51.071245
3452.281850	453784.986056	51.076250
3451.474234	453379.655274	51.081255
3450.767366	452965.320262	51.086260
3450.317989	452560.882395	51.091265
3449.775064	452133.770276	51.096269
3448.838407	451717.368586	51.101274
3447.878856	451320.550306	51.106279
3447.403917	450905.735536	51.111284
3446.593410	450499.187250	51.116289
3445.453221	450088.218215	51.121293
3445.039632	449677.482292	51.126298
3444.541438	449279.033717	51.131303
3443.948744	448867.550620	51.136308
3443.117922	448474.824891	51.141313
3442.235681	448058.602815	51.146317
3441.726456	447654.850234	51.151322
3440.892163	447254.187317	51.156327
3440.043667	446842.303214	51.161332
3439.326316	446445.262409	51.166337
3438.847696	446055.638325	51.171341
3437.915690	445655.674439	51.176346
3437.412508	445262.336042	51.181351
3436.517937	444846.617893	51.186356
3435.902213	444461.303943	51.191361
3435.284135	444058.776570	51.196365
3434.613026	443661.022372	51.201370
3433.519483	443263.379164	51.206375
3432.922348	442866.310864	51.211380
3432.474614	442475.304047	51.216385
3431.638683	442069.072316	51.221389
3430.924931	441686.217144	51.226394
3430.127118	441297.835802	51.231399
3429.603334	440897.373315	51.236404
3428.900300	440508.380679	51.241409
3427.958860	440115.941966	51.246413
3427.475582	439728.450714	51.251418
3426.434102	439337.081596	51.256423
3426.063948	438943.848592	51.261428
3425.357596	438556.780467	51.266433
3424.292436	438176.134955	51.271437
3423.701759	437798.988124	51.276442
3422.931372	437401.275296	51.281447
3422.703282	437021.444607	51.286452
3421.386528	436644.166723	51.291457
3420.676070	436249.523508	51.296461
3420.506650	435875.911748	51.301466
3419.521677	435497.294881	51.306471
3418.658582	435116.038022	51.311476
3418.098121	434746.076729	51.316481
3417.217877	434370.041666	51.321485
3416.720576	433988.786317	51.326490
3416.202631	433620.553961	51.331495
3415.412158	433231.335668	51.336500
3414.268816	432857.224375	51.341505
3413.726244	432484.764720	51.346509
3413.655520	432104.607483	51.351514
3412.604073	431731.100200	51.356519
3411.966099	431355.846264	51.361524
3411.315318	430989.298826	51.366529
3410.539529	430603.720840	51.371533
3409.783595	430241.598043	51.376538
3408.953709	429871.254202	51.381543
3408.296771	429490.770745	51.386548
3407.697346	429120.760855	51.391553
3406.983768	428745.507002	51.396557
3406.596300	428371.745429	51.401562
3405.590381	428006.203122	51.406567
3405.236571	427636.870232	51.411572
3404.186125	427251.286851	51.416577
3403.538964	426891.310673	51.421581
3402.808019	426534.238231	51.426586
3401.809647	426164.250453	51.431591
3401.280672	425788.951376	51.436596
3400.658944	425426.995979	51.441601
3400.079086	425065.206928	51.446605
3399.533578	424692.308193	51.451610
3398.510369	424331.671658	51.456615
3397.702893	423960.277516	51.461620
3397.022759	423609.406974	51.466625
3396.520008	423246.057653	51.471629
3395.976962	422880.169824	51.476634
3395.001247	422523.820199	51.481639
3394.561054	422152.597634	51.486644
3393.899678	421799.160976	51.491649
3393.432285	421448.381791	51.496653
3392.375987	421079.426901	51.501658
3391.473721	420708.181937	51.506663
3390.948685	420354.095769	51.511668
3389.942932	420010.598185	51.516673
3389.129475	419647.124029	51.521677
3388.857903	419296.871286	51.526682
3387.819360	418957.125881	51.531687
3387.456279	418593.795639	51.536692
3386.767403	418244.332624	51.541697
3385.821201	417898.818439	51.546701
3385.427388	417537.994743	51.551706
3384.478442	417196.029306	51.556711
3384.037660	416844.680754	51.561716
3383.373341	416495.827702	51.566721
3382.667713	416142.835640	51.571725
3381.976283	415785.339952	51.576730
3381.087523	415429.674995	51.581735
3380.616884	415078.894117	51.586740
3379.898645	414728.046537	51.591745
3378.708051	414384.002671	51.596749
3378.278601	414040.088515	51.601754
3377.510669	413695.309127	51.606759
3376.822718	413358.415365	51.611764
3376.099215	413016.848013	51.616769
3375.431011	412665.790078	51.621773
3374.914375	412328.095216	51.626778
3374.297236	411998.518366	51.631783
3373.338724	411642.259701	51.636788
3373.218178	411305.024270	51.641793
3372.158173	410963.435773	51.646797
3371.902239	410604.080567	51.651802
3371.007188	410261.873564	51.656807
3370.162676	409914.241888	51.661812
3369.642299	409574.712403	51.666817
3368.443398	409238.412184	51.671821
3368.277678	408895.362903	51.676826
3367.096924	408557.400456	51.681831
3366.933277	408219.400532	51.686836
3366.425812	407874.818209	51.691841
3365.231575	407537.177047	51.696845
3364.518889	407196.990844	51.701850
3364.020340	406852.141552	51.706855
3363.363075	406507.313523	51.711860
3362.590650	406182.755915	51.716865
3361.828377	405838.419978	51.721869
3361.258577	405498.319688	51.726874
3360.542763	405163.550777	51.731879
3360.102060	404834.326418	51.736884
3359.167199	404499.737581	51.741889
3358.371321	404154.117675	51.746893
3357.832295	403817.781520	51.751898
3357.307561	403493.157020	51.756903
3356.483506	403147.454367	51.761908
3355.601048	402819.753188	51.766913
3354.877777	402481.246122	51.771917
3354.601939	402150.900361	51.776922
3353.542199	401823.700001	51.781927
3352.974002	401479.997867	51.786932
3352.676351	401158.796281	51.791937
3351.781156	400813.944079	51.796941
3351.217236	400493.362670	51.801946
3350.568815	400152.277427	51.806951
3349.701039	399814.375443	51.811956
3349.041653	399491.181010	51.816961
3348.062576	399150.112210	51.821965
3348.221921	398820.680722	51.826970
3346.858564	398489.122533	51.831975
3346.196523	398154.247003	51.836980
3345.885367	397819.566840	51.841985
3344.818564	397496.290252	51.846989
3344.261339	397160.600085	51.851994
3343.788723	396837.070644	51.856999
3343.136720	396492.058656	51.862004
3342.169704	396171.829713	51.867009
3341.451825	395830.355202	51.872013
3341.002921	395503.021139	51.877018
3340.022635	395180.903581	51.882023
3339.545981	394840.245397	51.887028
3339.050846	394521.299197	51.892033
3338.309115	394183.905298	51.897037
3337.787313	393861.321458	51.902042
3336.893030	393526.004652	51.907047
3336.228278	393187.800654	51.912052
3335.753066	392865.759518	51.917057
3334.643176	392531.789322	51.922061
3334.211728	392199.463050	51.927066
3333.291391	391888.569061	51.932071
3332.711715	391553.030948	51.937076
3332.299115	391222.370593	51.942081
3331.431679	390910.645935	51.947085
3331.009775	390566.402865	51.952090
3329.943224	390244.253208	51.957095
3329.555331	389909.533716	51.962100
3328.727654	389582.915874	51.967105
3328.153347	389251.245625	51.972109
3327.567346	388917.794168	51.977114
3326.621287	388595.000325	51.982119
3325.803499	388265.393789	51.987124
3325.114919	387940.137635	51.992129
3324.737994	387615.897321	51.997133
3324.032181	387300.403052	52.002138
3323.071244	386973.146961	52.007143
3322.463716	386648.451357	52.012148
3321.658644	386339.906915	52.017153
3320.862986	386013.963947	52.022157
3320.446637	385699.147637	52.027162
3319.715755	385385.192179	52.032167
3319.160434	385061.974804	52.037172
3318.535157	384736.527727	52.042177
3317.943649	384417.811849	52.047181
3317.171990	384089.533959	52.052186
3316.612488	383771.417897	52.057191
3315.758145	383450.141315	52.062196
3314.955322	383142.053298	52.067201
3314.417863	382815.100651	52.072205
3314.130067	382495.582981	52.077210
3313.191893	382176.775879	52.082215
3312.480226	381850.783547	52.087220
3311.629225	381531.423195	52.092225
3310.975748	381215.437080	52.097229
3310.538918	380890.207037	52.102234
3309.604254	380581.864960	52.107239
3309.335831	380259.451626	52.112244
3308.630310	379944.328162	52.117249
3307.498796	379622.198661	52.122253
3307.213858	379302.170917	52.127258
3306.481769	378983.915441	52.132263
3305.464936	378669.263380	52.137268
3304.909169	378352.526496	52.142273
3304.328960	378035.078751	52.147277
3303.513906	377714.842221	52.152282
3302.618832	377408.275011	52.157287
3302.592762	377093.046847	52.162292
3301.671204	376781.951368	52.167297
3300.937522	376469.323011	52.172301
3300.355868	376142.779608	52.177306
3299.677558	375835.606557	52.182311
3299.017372	375510.418667	52.187316
3298.238599	375198.194667	52.192321
3297.430704	374876.001290	52.197325
3297.229402	374565.207420	52.202330
3296.526359	374241.440784	52.207335
3295.661954	373919.961147	52.212340
3295.253198	373609.574487	52.217345
3294.164327	373299.191316	52.222349
3293.737472	372975.345708	52.227354
3293.208086	372665.937798	52.232359
3292.143920	372351.498885	52.237364
3291.481962	372033.483370	52.242369
3290.595132	371720.258252	52.247373
3290.361941	371403.086033	52.252378
3289.438442	371095.738729	52.257383
3289.382514	370771.690411	52.262388
3288.620455	370455.027286	52.267393
3287.617444	370146.769904	52.272397
3287.023903	369825.165464	52.277402
3286.235429	369505.777391	52.282407
3285.479757	369201.493848	52.287412
3284.803731	368880.964000	52.292417
3284.104276	368567.635469	52.297421
3283.743073	368252.597498	52.302426
3282.928956	367945.057940	52.307431
3282.103653	367623.652077	52.312436
3281.783750	367304.555532	52.317441
3281.088315	367002.155453	52.322445
3280.126233	366682.952484	52.327450
3279.517005	366371.985793	52.332455
3278.825159	366047.189039	52.337460
3277.835393	365742.918810	52.342465
3277.349948	365433.757990	52.347469
3276.926713	365116.519640	52.352474
3275.734212	364811.868148	52.357479
3275.468698	364498.468005	52.362484
3275.207410	364188.728995	52.367489
3274.362038	363880.225270	52.372493
3273.762939	363565.294005	52.377498
3273.058299	363256.178650	52.382503
3272.595271	362932.595887	52.387508
3271.716809	362615.768593	52.392513
3271.045466	362304.656986	52.397517
3270.617899	361980.196922	52.402522
3269.624779	361671.702002	52.407527
3268.874172	361352.403253	52.412532
3268.298235	361040.174098	52.417537
3267.676151	360726.168991	52.422541
3266.830867	360405.682940	52.427546
3266.036787	360098.825836	52.432551
3265.437073	359784.912843	52.437556
3264.665432	359479.295140	52.442561
3264.145451	359170.378540	52.447565
3263.636416	358837.334621	52.452570
3262.869431	358542.296229	52.457575
3262.169497	358233.096829	52.462580
3261.663944	357907.374867	52.467585
3260.834190	357601.805586	52.472589
3260.097331	357290.086851	52.477594
3259.510295	356986.587575	52.482599
3258.658922	356664.118627	52.487604
3257.914763	356365.373781	52.492609
3257.357260	356054.255228	52.497613
3256.854742	355738.443559	52.502618
3256.065248	355440.489349	52.507623
3255.391956	355129.994239	52.512628
3254.655253	354819.990813	52.517633
3254.126207	354508.552982	52.522637
3253.479396	354200.720246	52.527642
3252.566277	353890.764612	52.532647
3252.423480	353580.863448	52.537652
3251.667942	353264.847647	52.542657
3250.772420	352955.927141	52.547661
3250.499403	352640.213029	52.552666
3249.541237	352330.637085	52.557671
3248.726127	352018.135385	52.562676
3248.293482	351719.161888	52.567681
3247.437345	351408.470103	52.572685
3247.094754	351093.801346	52.577690
3246.086587	350792.750434	52.582695
3245.600586	350469.625609	52.587700
3244.807242	350162.556254	52.592705
3243.685752	349861.569035	52.597709
3243.669224	349541.494995	52.602714
3243.014730	349245.419032	52.607719
3242.310192	348927.079166	52.612724
3241.793319	348617.437786	52.617729
3241.099442	348302.452321	52.622733
3240.671407	347981.467245	52.627738
3239.555378	347672.908069	52.632743
3238.752896	347353.353082	52.637748
3238.279349	347047.895898	52.642753
3237.663570	346745.412094	52.647757
3237.086893	346430.219554	52.652762
3236.085652	346127.004435	52.657767
3235.848510	345805.442455	52.662772
3234.789623	345492.128261	52.667777
3234.138387	345182.413196	52.672781
3233.519780	344872.309537	52.677786
3232.693823	344565.138761	52.682791
3232.157842	344260.644082	52.687796
3231.306661	343953.983215	52.692801
3230.472172	343640.903720	52.697805
3230.353049	343322.898607	52.702810
3229.594597	343025.407289	52.707815
3228.975356	342701.852622	52.712820
3228.037752	342407.975697	52.717825
3227.425642	342097.525794	52.722829
3227.103537	341788.428467	52.727834
3225.897410	341490.236861	52.732839
3225.268741	341168.432014	52.737844
3225.072042	340872.419647	52.742849
3223.872145	340566.713364	52.747853
3223.262891	340250.093614	52.752858
3222.681236	339949.504915	52.757863
3221.689745	339648.088673	52.762868
3221.219490	339342.821105	52.767873
3220.924983	339037.218815	52.772877
3220.441518	338726.197376	52.777882
3219.626143	338424.543899	52.782887
3218.961236	338109.933437	52.787892
3218.218559	337794.340967	52.792897
3217.702344	337485.813530	52.797901
3217.198665	337175.271597	52.802906
3216.203131	336862.463994	52.807911
3215.713807	336557.848338	52.812916
3215.000375	336246.393363	52.817921
3214.222311	335943.602591	52.822925
3213.502378	335612.467383	52.827930
3212.663158	335320.630119	52.832935
3212.114385	335016.220605	52.837940
3211.567843	334703.408398	52.842945
3210.708701	334402.176553	52.847949
3210.295975	334090.307810	52.852954
3209.442409	333780.645874	52.857959
3208.903784	333470.321765	52.862964
3207.990811	333168.965853	52.867969
3207.513594	332870.594723	52.872973
3207.125004	332552.987284	52.877978
3206.217828	332247.273196	52.882983
3205.294803	331938.556212	52.887988
3204.836588	331626.505682	52.892993
3203.882390	331326.065101	52.897997
3203.504844	331014.381086	52.903002
3202.787127	330708.936100	52.908007
3202.024330	330404.540813	52.913012
3201.177577	330095.982259	52.918017
3200.562826	329801.133757	52.923021
3200.188967	329497.717102	52.928026
3199.578862	329193.954716	52.933031
3198.619474	328892.028546	52.938036
3198.286886	328576.381100	52.943041
3197.584419	328264.864445	52.948045
3197.048799	327951.359737	52.953050
3196.136294	327657.008393	52.958055
3195.499679	327343.797294	52.963060
3195.089912	327039.511060	52.968065
3194.139003	326739.892121	52.973069
3193.444632	326423.071176	52.978074
3192.827900	326122.505957	52.983079
3192.196402	325817.919189	52.988084
3191.639858	325511.027965	52.993089
3190.811547	325204.840566	52.998093
3190.453854	324888.316854	53.003098
3189.493610	324585.941708	53.008103
3189.074882	324280.195330	53.013108
3188.318929	323970.631093	53.018113
3187.559384	323660.862604	53.023117
3187.279046	323347.834515	53.028122
3186.223877	323044.144894	53.033127
3185.804125	322734.319307	53.038132
3184.963281	322415.774977	53.043137
3184.463871	322113.521885	53.048141
3183.817736	321801.666413	53.053146
3183.170946	321493.323687	53.058151
3182.148515	321179.692310	53.063156
3181.817659	320872.850650	53.068161
3180.764002	320562.557595	53.073165
3180.482279	320254.814901	53.078170
3180.001230	319945.524045	53.083175
3178.864974	319631.574339	53.088180
3178.459581	319306.966486	53.093185
3177.457293	318999.970184	53.098189
3177.159419	318689.067514	53.103194
3176.375888	318386.872522	53.108199
3175.731945	318076.811950	53.113204
3175.175210	317764.088446	53.118209
3174.193893	317459.935737	53.123213
3173.593281	317145.205616	53.128218
3172.829015	316839.005068	53.133223
3172.133118	316540.457187	53.138228
3171.605587	316228.768189	53.143233
3170.995540	315931.503547	53.148237
3170.527662	315606.740493	53.153242
3169.568375	315317.041027	53.158247
3169.039097	315004.253637	53.163252
3168.707847	314693.700244	53.168257
3167.799905	314389.704957	53.173261
3166.856769	314067.405880	53.178266
3165.918444	313775.534418	53.183271
3165.086225	313463.045034	53.188276
3164.714046	313158.604996	53.193281
3163.861754	312860.835267	53.198285
3163.529076	312555.623383	53.203290
3162.497252	312259.051788	53.208295
3162.169543	311955.747294	53.213300
3161.483982	311652.345812	53.218305
3160.688749	311358.026213	53.223309
3160.294339	311038.916409	53.228314
3159.566031	310746.265319	53.233319
3158.833592	310429.091698	53.238324
3158.123871	310135.315699	53.243329
3157.466762	309835.979330	53.248333
3157.010053	309527.086660	53.253338
3156.420324	309224.325822	53.258343
3155.931310	308912.864747	53.263348
3155.000844	308606.107361	53.268353
3154.464423	308294.855952	53.273357
3153.575850	307985.594837	53.278362
3153.015604	307683.436748	53.283367
3152.427702	307370.408649	53.288372
3152.342998	307067.817365	53.293377
3151.147252	306755.265930	53.298381
3150.658094	306439.673437	53.303386
3149.743603	306145.232935	53.308391
3149.170571	305832.326158	53.313396
3148.416821	305513.641088	53.318401
3147.737283	305211.954617	53.323405
3147.391785	304901.148837	53.328410
3146.655994	304602.398509	53.333415
3145.773988	304277.644580	53.338420
3145.084905	303975.371259	53.343425
3144.480922	303660.401793	53.348429
3144.223035	303343.161348	53.353434
3143.727756	303040.677173	53.358439
3142.885560	302725.386882	53.363444
3142.143031	302404.859599	53.368449
3141.152067	302093.844390	53.373453
3140.655404	301775.263265	53.378458
3139.957656	301467.332770	53.383463
3139.357317	301161.347177	53.388468
3138.533628	300849.488128	53.393473
3137.822895	300537.381412	53.398477
3137.154842	300222.185904	53.403482
3136.616385	299911.680612	53.408487
3136.110647	299598.724778	53.413492
3135.492511	299286.448289	53.418497
3134.684377	298977.461039	53.423501
3133.868454	298658.924445	53.428506
3133.466707	298349.260600	53.433511
3132.831370	298027.892967	53.438516
3132.010809	297718.294313	53.443521
3131.454838	297413.644799	53.448525
3131.017179	297088.678897	53.453530
3130.063977	296779.048755	53.458535
3129.284023	296468.270158	53.463540
3128.653638	296143.842511	53.468545
3127.321486	295848.685242	53.473549
3126.935767	295531.119492	53.478554
3126.432856	295232.188327	53.483559
3125.819298	294922.501598	53.488564
3125.135272	294622.222996	53.493569
3124.353411	294314.395663	53.498573
3123.771605	293994.311917	53.503578
3123.251647	293704.906132	53.508583
3122.677117	293390.143063	53.513588
3122.170099	293076.744126	53.518593
3121.216647	292770.138827	53.523597
3120.414051	292459.230724	53.528602
3119.997856	292147.064112	53.533607
3119.357519	291838.447102	53.538612
3118.686797	291532.534091	53.543617
3117.927983	291222.534366	53.548621
3117.235835	290902.616804	53.553626
3116.346922	290610.107778	53.558631
3115.596168	290291.064672	53.563636
3114.909321	289983.242375	53.568641
3114.374343	289694.063605	53.573645
3113.722966	289378.365508	53.578650
3113.636528	289067.238305	53.583655
3112.855522	288758.894812	53.588660
3111.976368	288446.007793	53.593665
3111.162129	288144.698100	53.598669
3111.054113	287816.025694	53.603674
3110.325753	287522.163957	53.608679
3109.368418	287205.289677	53.613684
3108.578351	286892.514467	53.618689
3107.740887	286576.817666	53.623693
3107.177308	286260.695244	53.628698
3106.516287	285965.344458	53.633703
3105.820152	285656.628265	53.638708
3105.284831	285352.980016	53.643713
3104.698568	285042.361346	53.648717
3104.069984	284728.667508	53.653722
3103.486424	284420.874942	53.658727
3102.453931	284116.234860	53.663732
3102.214286	283801.129048	53.668737
3101.581579	283499.990876	53.673741
3101.100978	283181.306329	53.678746
3100.351729	282868.343522	53.683751
3099.610622	282546.821926	53.688756
3099.182529	282234.011709	53.693761
3098.047461	281925.337193	53.698765
3097.706640	281609.685886	53.703770
3096.777384	281291.911806	53.708775
3096.296446	280986.342372	53.713780
3095.443867	280664.200816	53.718785
3094.671293	280353.991120	53.723789
3094.278031	280048.738556	53.728794
3093.360321	279726.708838	53.733799
3093.230278	279415.785925	53.738804
3092.230160	279100.569108	53.743809
3091.354354	278784.160994	53.748813
3090.829348	278468.792436	53.753818
3090.226817	278164.132796	53.758823
3089.333692	277850.757963	53.763828
3088.931324	277534.223748	53.768833
3088.055711	277220.081997	53.773837
3087.573717	276910.538641	53.778842
3086.496310	276606.386900	53.783847
3086.430273	276295.224104	53.788852
3085.590773	275981.662316	53.793857
3084.495487	275673.234677	53.798861
3084.319541	275353.404533	53.803866
3083.282075	275045.935555	53.808871
3082.792465	274731.019535	53.813876
3081.918076	274430.808750	53.818881
3081.440763	274115.483345	53.823885
3080.746300	273803.274016	53.828890
3080.012480	273502.353452	53.833895
3079.311698	273189.686791	53.838900
3078.928282	272871.519739	53.843905
3078.071718	272569.472698	53.848909
3077.509633	272258.923634	53.853914
3077.146132	271939.480244	53.858919
3076.146543	271635.647824	53.863924
3075.671422	271316.426036	53.868929
3074.769560	270998.290620	53.873933
3074.194736	270674.424137	53.878938
3073.598797	270381.301365	53.883943
3072.714076	270063.596567	53.888948
3072.265389	269742.028134	53.893953
3071.365584	269447.196518	53.898957
3070.828267	269126.813948	53.903962
3070.134180	268822.323069	53.908967
3069.149205	268509.015434	53.913972
3068.720869	268201.222895	53.918977
3068.028149	267892.173490	53.923981
3067.673707	267582.306691	53.928986
3066.641342	267273.031259	53.933991
3065.946518	266956.520591	53.938996
3065.868232	266648.291588	53.944001
3064.582101	266348.709352	53.949005
3064.305949	266030.121100	53.954010
3063.475807	265724.660415	53.959015
3062.920142	265407.670428	53.964020
3062.264268	265107.530927	53.969025
3061.158947	264788.336303	53.974029
3060.995441	264483.051243	53.979034
3060.392991	264179.211175	53.984039
3059.744937	263865.369678	53.989044
3059.209276	263551.383342	53.994049
3058.492126	263246.186980	53.999053
3057.641470	262916.639269	54.004058
3056.878659	262610.330148	54.009063
3056.340806	262289.647340	54.014068
3055.871206	261977.307508	54.019073
3054.880184	261672.130563	54.024077
3054.643423	261349.796651	54.029082
3053.693089	261037.610311	54.034087
3052.921707	260734.920919	54.039092
3052.260537	260414.667203	54.044097
3051.320587	260109.382021	54.049101
3050.848848	259794.676490	54.054106
3050.379954	259484.453186	54.059111
3049.647476	259173.711694	54.064116
3048.950757	258862.786661	54.069121
3048.412966	258549.621205	54.074125
3047.732974	258232.200137	54.079130
3047.277463	257935.627247	54.084135
3046.609506	257620.700918	54.089140
3045.882691	257295.775682	54.094145
3045.332532	256985.059183	54.099149
3044.562286	256672.595250	54.104154
3043.932467	256361.433845	54.109159
3043.165027	256049.759867	54.114164
3042.552205	255727.925964	54.119169
3041.537166	255412.268328	54.124173
3041.571124	255092.879783	54.129178
3040.553525	254779.235453	54.134183
3039.920133	254468.510459	54.139188
3039.084608	254138.896020	54.144193
3038.306371	253839.247627	54.149197
3037.720861	253528.185528	54.154202
3037.042001	253206.035199	54.159207
3036.336757	252898.762211	54.164212
3035.909766	252589.204640	54.169217
3035.046131	252277.755783	54.174221
3034.616789	251957.962095	54.179226
3034.167003	251646.550743	54.184231
3033.130601	251340.173312	54.189236
3032.605231	251011.483317	54.194241
3032.062598	250702.049335	54.199245
3031.341806	250379.478013	54.204250
3030.537337	250073.855695	54.209255
3029.719256	249751.835827	54.214260
3029.123854	249435.765942	54.219265
3028.240997	249125.293824	54.224269
3027.985196	248803.721721	54.229274
3027.627840	248507.352326	54.234279
3026.439387	248180.403019	54.239284
3026.009379	247856.670438	54.244289
3024.965996	247547.194700	54.249293
3024.551265	247227.943099	54.254298
3023.832366	246923.306790	54.259303
3022.960261	246600.385509	54.264308
3022.602300	246284.259335	54.269313
3021.650212	245990.281153	54.274317
3021.477219	245670.689247	54.279322
3021.025415	245353.663306	54.284327
3019.799638	245035.691061	54.289332
3019.275582	244716.437105	54.294337
3018.187033	244410.235121	54.299341
3017.893590	244088.017683	54.304346
3017.239811	243776.426141	54.309351
3016.627564	243460.907153	54.314356
3016.121398	243145.957858	54.319361
3015.221570	242837.539775	54.324365
3014.924652	242512.449348	54.329370
3013.990012	242199.683860	54.334375
3013.309994	241877.686074	54.339380
3012.932389	241565.037778	54.344385
3012.303162	241243.288301	54.349389
3011.262549	240916.664674	54.354394
3010.609340	240614.324748	54.359399
3010.164666	240297.259596	54.364404
3009.753034	239965.904551	54.369409
3008.632719	239669.090420	54.374413
3008.145685	239343.427671	54.379418
3007.776025	239025.055513	54.384423
3006.601435	238700.063674	54.389428
3006.062685	238383.120650	54.394433
3005.399208	238068.159011	54.399437
3004.918157	237752.914773	54.404442
3003.881936	237432.310072	54.409447
3003.212330	237113.481698	54.414452
3002.972922	236799.857174	54.419457
3001.987419	236491.546250	54.424461
3001.314090	236177.126512	54.429466
3000.725153	235856.583147	54.434471
2999.883312	235539.594759	54.439476
2999.431748	235224.277090	54.444481
2998.614114	234908.279915	54.449485
2998.214481	234590.842568	54.454490
2997.494464	234284.456979	54.459495
2996.728818	233963.132807	54.464500
2996.306097	233640.533195	54.469505
2995.355839	233343.557335	54.474509
2994.909899	233008.461274	54.479514
2994.281154	232691.830258	54.484519
2993.541334	232378.477085	54.489524
2993.044405	232059.790318	54.494529
2992.323242	231740.147097	54.499533
2991.434329	231422.441200	54.504538
2990.658339	231103.063481	54.509543
2990.139474	230784.384579	54.514548
2990.042777	230468.568102	54.519553
2988.902441	230150.982816	54.524557
2988.319106	229825.850175	54.529562
2987.607023	229509.447015	54.534567
2986.402693	229192.868287	54.539572
2985.664494	228875.274842	54.544577
2984.941192	228566.489862	54.549581
2984.721771	228243.393319	54.554586
2983.966643	227935.786855	54.559591
2983.242952	227632.632231	54.564596
2982.922697	227304.844876	54.569601
2982.021824	226999.123536	54.574605
2981.400113	226688.916195	54.579610
2980.863130	226368.919650	54.584615
2980.028928	226058.200894	54.589620
2979.433870	225737.121182	54.594625
2978.690425	225433.837655	54.599629
2978.220552	225111.938585	54.604634
2977.381013	224801.187279	54.609639
2976.306616	224495.591857	54.614644
2976.384473	224170.694669	54.619649
2975.373107	223863.093083	54.624653
2974.475867	223549.466095	54.629658
2974.311683	223230.568717	54.634663
2973.367120	222908.359113	54.639668
2972.688402	222607.456643	54.644673
2972.230864	222295.152674	54.649677
2971.569709	221972.672995	54.654682
2971.014202	221661.392777	54.659687
2970.025690	221339.324043	54.664692
2969.825486	221021.701809	54.669697
2968.726820	220707.838320	54.674701
2968.089609	220396.168951	54.679706
2967.833493	220072.309481	54.684711
2966.700281	219766.284030	54.689716
2966.281665	219442.109379	54.694721
2965.386564	219135.412427	54.699725
2965.238163	218811.465141	54.704730
2964.376756	218500.781337	54.709735
2963.509790	218188.495907	54.714740
2962.955547	217862.835104	54.719745
2962.485292	217554.830254	54.724749
2961.674966	217227.010826	54.729754
2961.206266	216915.406275	54.734759
2960.470530	216590.009242	54.739764
2959.845270	216270.362350	54.744769
2959.169286	215956.694704	54.749773
2958.605569	215633.515211	54.754778
2957.960873	215319.501874	54.759783
2957.013661	215000.930184	54.764788
2956.467262	214675.996001	54.769793
2955.932407	214361.804279	54.774797
2954.883293	214040.847640	54.779802
2954.414465	213718.209672	54.784807
2953.377316	213400.474489	54.789812
2953.137540	213088.329532	54.794817
2952.266158	212773.485888	54.799821
2951.437088	212451.623969	54.804826
2951.295059	212137.533463	54.809831
2950.489606	211816.281922	54.814836
2950.160315	211499.284060	54.819841
2949.349479	211179.933016	54.824845
2948.527785	210854.463309	54.829850
2947.796903	210534.415584	54.834855
2947.035044	210216.779898	54.839860
2946.779972	209893.350981	54.844865
2945.626987	209580.655074	54.849869
2945.099592	209256.521681	54.854874
2944.729180	208932.874236	54.859879
2943.795426	208624.221214	54.864884
2943.130216	208295.672946	54.869889
2942.546985	207984.664079	54.874893
2941.893295	207664.390002	54.879898
2941.200900	207346.949138	54.884903
2940.306040	207029.592920	54.889908
2939.678240	206704.610962	54.894913
2938.812685	206392.420588	54.899917
2938.655663	206065.356802	54.904922
2937.719615	205750.864750	54.909927
2936.860710	205434.898634	54.914932
2936.468561	205105.993927	54.919937
2935.846479	204801.867529	54.924941
2935.158898	204480.967131	54.929946
2934.604576	204160.734649	54.934951
2933.680372	203844.036760	54.939956
2933.429584	203527.997592	54.944961
2932.653175	203215.034014	54.949965
2932.010435	202886.436295	54.954970
2931.235413	202564.491617	54.959975
2930.258453	202251.896040	54.964980
2929.861635	201921.967039	54.969985
2929.065485	201605.096100	54.974989
2928.433095	201287.195740	54.979994
2927.585300	200977.730148	54.984999
2927.193066	200653.419979	54.990004
2926.609982	200332.323293	54.995009
2925.516360	200028.501173	55.000013
2925.043284	199711.310146	55.005018
2924.656504	199386.281383	55.010023
2923.629664	199083.522951	55.015028
2922.854745	198751.497104	55.020033
2922.560680	198439.642507	55.025037
2922.158231	198117.054442	55.030042
2921.379165	197811.400980	55.035047
2920.600378	197489.029053	55.040052
2920.097902	197156.232117	55.045057
2919.052995	196845.180287	55.050061
2918.735596	196527.945600	55.055066
2918.044797	196206.483878	55.060071
2917.268699	195887.607976	55.065076
2916.973552	195565.515045	55.070081
2916.008878	195248.327139	55.075085
2915.500443	194934.008237	55.080090
2914.823662	194608.902588	55.085095
2914.056115	194280.874199	55.090100
2913.736956	193952.547941	55.095105
2912.530115	193635.523063	55.100109
2912.032937	193314.214507	55.105114
2911.600656	192989.258832	55.110119
2910.434391	192677.259463	55.115124
2909.988144	192358.430144	55.120129
2909.519172	192033.283027	55.125133
2909.083173	191716.491999	55.130138
2908.263707	191400.743430	55.135143
2907.480981	191071.975442	55.140148
2907.132948	190751.079994	55.145153
2906.240663	190427.817345	55.150157
2905.218165	190101.854825	55.155162
2904.796214	189772.593337	55.160167
2904.124771	189451.439761	55.165172
2903.549505	189130.654814	55.170177
2902.866322	188809.749192	55.175181
2902.341693	188488.744326	55.180186
2901.346510	188167.854331	55.185191
2900.519047	187851.163752	55.190196
2900.301750	187522.827083	55.195201
2899.313393	187213.570584	55.200205
2898.859662	186892.387424	55.205210
2898.187047	186567.437345	55.210215
2897.250762	186246.398723	55.215220
2896.730089	185928.858616	55.220225
2895.875902	185607.582515	55.225229
2895.437653	185279.271485	55.230234
2894.942903	184963.222458	55.235239
2893.731351	184648.675764	55.240244
2893.597530	184325.551944	55.245249
2892.783267	184008.402618	55.250253
2892.128853	183688.546115	55.255258
2891.622097	183371.912373	55.260263
2891.090158	183041.406482	55.265268
2890.274995	182720.641103	55.270273
2889.242329	182402.825531	55.275277
2888.768837	182076.566348	55.280282
2887.975898	181749.113585	55.285287
2887.328011	181444.498781	55.290292
2886.724060	181120.964150	55.295297
2886.234890	180802.183832	55.300301
2885.414942	180478.077668	55.305306
2884.755342	180165.536457	55.310311
2884.455044	179839.559341	55.315316
2883.953762	179509.062868	55.320321
2882.660036	179203.892118	55.325325
2882.469896	178866.482774	55.330330
2881.597729	178562.623634	55.335335
2880.903294	178241.478342	55.340340
2880.308045	177902.322021	55.345345
2879.763299	177588.827777	55.350349
2878.945413	177267.327961	55.355354
2878.486918	176940.380886	55.360359
2877.296284	176615.765412	55.365364
2876.978654	176295.414974	55.370369
2876.401016	175979.763247	55.375373
2875.877842	175646.159403	55.380378
2875.123617	175325.415109	55.385383
2874.516709	175006.494189	55.390388
2874.252875	174683.006468	55.395393
2873.327626	174348.752023	55.400397
2872.365240	174023.141811	55.405402
2871.663227	173692.278648	55.410407
2871.610341	173365.092650	55.415412
2870.604145	173051.986239	55.420417
2869.719877	172725.267809	55.425421
2869.075308	172400.790566	55.430426
2868.721636	172074.311443	55.435431
2867.694277	171753.829835	55.440436
2867.309661	171417.835777	55.445441
2866.510075	171100.121251	55.450445
2865.650240	170774.674184	55.455450
2865.132595	170445.335151	55.460455
2864.509389	170119.881546	55.465460
2864.032550	169787.642222	55.470465
2863.074063	169471.314198	55.475469
2862.480748	169131.303719	55.480474
2862.166577	168815.845539	55.485479
2861.088210	168501.312102	55.490484
2860.603344	168101.043967	55.495489
2859.910080	167769.606733	55.500493
2859.621814	167458.161291	55.505498
2858.811933	167122.933432	55.510503
2858.006996	166802.788609	55.515508
2857.519995	166465.951470	55.520513
2855.983963	166142.393143	55.525517
2855.642813	165823.988883	55.530522
2855.112930	165488.222768	55.535527
2854.192331	165162.884413	55.540532
2853.859442	164847.017574	55.545537
2853.388645	164527.030221	55.550541
2852.633394	164197.478308	55.555546
2852.017372	163872.560901	55.560551
2851.071282	163544.532728	55.565556
2850.491751	163208.210501	55.570561
2850.023999	162899.934268	55.575565
2848.958344	162566.975289	55.580570
2848.705026	162248.397569	55.585575
2847.647353	161924.673732	55.590580
2847.170827	161591.490660	55.595585
2846.469036	161278.777407	55.600589
2845.559930	160958.090122	55.605594
2845.111783	160633.938223	55.610599
2844.324994	160326.586512	55.615604
2843.673271	159986.924253	55.620609
2842.801200	159677.214322	55.625613
2842.366443	159362.250933	55.630618
2841.741411	159035.433879	55.635623
2841.170398	158711.370021	55.640628
2840.616925	158386.429223	55.645633
2839.945915	158077.286439	55.650637
2839.367746	157745.287347	55.655642
2838.418592	157425.859177	55.660647
2837.481333	157109.724564	55.665652
2837.046552	156789.203875	55.670657
2836.139422	156471.303392	55.675661
2835.690320	156154.947750	55.680666
2835.166097	155838.378130	55.685671
2834.298945	155509.433753	55.690676
2833.781126	155193.199645	55.695681
2833.095309	154866.470039	55.700685
2832.462370	154551.111845	55.705690
2831.990347	154220.020106	55.710695
2831.340615	153915.081009	55.715700
2830.775445	153583.527296	55.720705
2829.829227	153267.302914	55.725709
2829.019916	152949.165967	55.730714
2828.753269	152615.820556	55.735719
2827.992645	152303.503543	55.740724
2827.211710	151974.351524	55.745729
2826.389261	151659.241432	55.750733
2825.701778	151345.778014	55.755738
2825.096765	151017.637252	55.760743
2824.351034	150701.596407	55.765748
2823.984896	150385.574776	55.770753
2822.901078	150061.789934	55.775757
2822.324297	149752.302427	55.780762
2822.245715	149426.636265	55.785767
2821.227969	149096.750158	55.790772
2820.879832	148783.550078	55.795777
2819.890280	148452.318970	55.800781
2819.752879	148134.961454	55.805786
2818.820345	147806.320616	55.810791
2817.906001	147483.335599	55.815796
2817.545128	147161.892900	55.820801
2816.869987	146847.378422	55.825805
2815.927874	146520.137646	55.830810
2815.030078	146189.665412	55.835815
2814.595522	145864.613108	55.840820
2813.958841	145562.025409	55.845825
2813.085772	145232.957207	55.850829
2812.723522	144917.395915	55.855834
2811.890134	144580.220932	55.860839
2811.209131	144280.918499	55.865844
2810.735541	143946.133229	55.870849
2810.086909	143632.879530	55.875853
2809.119091	143308.357757	55.880858
2808.780004	142980.283612	55.885863
2808.236154	142656.756245	55.890868
2807.535531	142344.629406	55.895873
2806.949896	142020.530901	55.900877
2805.979276	141700.931278	55.905882
2805.504619	141372.197060	55.910887
2804.661926	141056.738850	55.915892
2804.017369	140722.346354	55.920897
2803.346879	140405.330286	55.925901
2802.552746	140090.242970	55.930906
2801.916449	139767.790262	55.935911
2801.368958	139449.850031	55.940916
2800.824924	139118.534169	55.945921
2799.900005	138804.954914	55.950925
2799.685391	138476.897319	55.955930
2798.980701	138150.991835	55.960935
2797.677470	137836.250396	55.965940
2797.587964	137497.791535	55.970945
2796.698489	137184.427132	55.975949
2795.947425	136863.053259	55.980954
2795.606097	136545.988193	55.985959
2794.547873	136224.009383	55.990964
2794.082953	135904.430092	55.995969
2793.026923	135587.920567	56.000973
2792.614684	135264.948116	56.005978
2792.050087	134942.956145	56.010983
2791.097140	134641.913250	56.015988
2790.579501	134309.542437	56.020993
2790.157750	133986.598507	56.025997
2789.291369	133678.438390	56.031002
2788.928230	133358.769558	56.036007
2787.888685	133038.665229	56.041012
2787.604308	132708.651421	56.046017
2786.777950	132396.256256	56.051021
2786.011738	132070.403573	56.056026
2785.604853	131747.520777	56.061031
2784.853409	131431.250334	56.066036
2784.579300	131105.114925	56.071041
2783.765141	130778.662387	56.076045
2782.535125	130470.416951	56.081050
2782.215561	130136.133082	56.086055
2781.297931	129817.430444	56.091060
2780.859478	129494.819906	56.096065
2780.054862	129179.637511	56.101069
2779.324699	128851.860660	56.106074
2779.043061	128544.057891	56.111079
2778.080675	128224.326522	56.116084
2777.554671	127898.497196	56.121089
2776.956982	127571.692489	56.126093
2776.448804	127255.189746	56.131098
2775.679469	126924.813195	56.136103
2774.737243	126613.415697	56.141108
2774.309684	126284.377019	56.146113
2773.564151	125964.307532	56.151117
2773.024479	125641.072548	56.156122
2772.172041	125314.538451	56.161127
2771.389971	124997.876789	56.166132
2770.587341	124679.812560	56.171137
2769.847573	124362.326266	56.176141
2769.296336	124052.267775	56.181146
2768.813739	123734.024386	56.186151
2768.154406	123426.821955	56.191156
2767.611865	123101.725973	56.196161
2767.108105	122783.002068	56.201165
2766.240917	122461.368324	56.206170
2765.842768	122129.798316	56.211175
2764.859258	121814.730015	56.216180
2764.269309	121497.000236	56.221185
2763.552794	121166.279982	56.226189
2762.861880	120852.510031	56.231194
2762.477292	120522.964200	56.236199
2761.473909	120215.517155	56.241204
2760.934394	119891.539485	56.246209
2759.982429	119575.090165	56.251213
2759.286452	119265.275901	56.256218
2758.807510	118940.964037	56.261223
2757.798634	118630.000822	56.266228
2757.344807	118317.741010	56.271233
2756.633516	117995.471015	56.276237
2756.070701	117674.286021	56.281242
2755.450199	117360.991470	56.286247
2754.706671	117051.274812	56.291252
2754.461852	116717.274011	56.296257
2753.793448	116413.964027	56.301261
2752.857893	116090.293653	56.306266
2752.347164	115761.609343	56.311271
2751.730117	115457.521937	56.316276
2751.067270	115130.171057	56.321281
2750.482876	114821.078364	56.326285
2749.365152	114484.211400	56.331290
2748.946010	114168.309449	56.336295
2748.069915	113859.807892	56.341300
2747.507249	113526.591342	56.346305
2746.878757	113222.367743	56.351309
2746.011079	112904.274391	56.356314
2745.655304	112583.172007	56.361319
2744.915724	112273.234161	56.366324
2744.426124	111942.038986	56.371329
2743.513187	111629.947212	56.376333
2743.004448	111327.764937	56.381338
2742.370158	110997.316089	56.386343
2741.398365	110681.774411	56.391348
2740.836596	110354.781193	56.396353
2740.045558	110059.011325	56.401357
2739.401311	109747.440256	56.406362
2738.812419	109418.991651	56.411367
2738.385090	109114.958152	56.416372
2737.634760	108799.488169	56.421377
2736.806937	108480.614455	56.426381
2736.428124	108158.805783	56.431386
2735.607972	107843.352955	56.436391
2734.821499	107535.728672	56.441396
2734.563887	107202.454425	56.446401
2733.659305	106898.511675	56.451405
2732.921559	106574.052720	56.456410
2732.494437	106267.250635	56.461415
2731.765396	105943.388901	56.466420
2731.008377	105623.742408	56.471425
2730.477900	105310.167664	56.476429
2729.777393	104989.423146	56.481434
2729.193778	104657.466818	56.486439
2728.046755	104367.253924	56.491444
2727.836840	104031.865719	56.496449
2726.991877	103723.449747	56.501453
2726.440250	103410.036737	56.506458
2725.883183	103076.702763	56.511463
2724.979037	102762.212344	56.516468
2724.467232	102440.438559	56.521473
2723.733704	102134.119223	56.526477
2722.850157	101814.741037	56.531482
2722.742607	101496.424175	56.536487
2721.938603	101188.618700	56.541492
2721.589278	100857.928654	56.546497
2720.839125	100530.516452	56.551501
2719.797237	100211.356671	56.556506
2719.335569	99881.269256	56.561511
2718.610802	99570.504254	56.566516
2717.680317	99252.843365	56.571521
2717.003692	98943.639540	56.576525
2716.456092	98618.594612	56.581530
2715.966489	98292.682530	56.586535
2714.906832	97989.260558	56.591540
2714.378695	97666.667935	56.596545
2713.901348	97342.860467	56.601549
2713.150124	97030.313965	56.606554
2712.371407	96715.619818	56.611559
2711.401796	96406.636378	56.616564
2711.062721	96081.150753	56.621569
2710.246827	95764.604882	56.626573
2709.636622	95463.758378	56.631578
2709.130708	95139.466993	56.636583
2708.320798	94835.787776	56.641588
2707.784830	94512.607313	56.646593
2707.165548	94199.254829	56.651597
2706.197831	93879.347982	56.656602
2706.005479	93577.560185	56.661607
2705.084414	93263.342862	56.666612
2704.663291	92933.293357	56.671617
2703.939445	92625.071462	56.676621
2702.952740	92303.319771	56.681626
2702.441948	91978.973762	56.686631
2701.784922	91670.298080	56.691636
2700.779543	91358.099496	56.696641
2700.374544	91044.960617	56.701645
2699.637433	90726.223202	56.706650
2699.256913	90425.446705	56.711655
2698.275772	90112.862595	56.716660
2698.144129	89787.347705	56.721665
2696.991695	89485.241898	56.726669
2696.343984	89165.644546	56.731674
2696.231680	88853.391026	56.736679
2695.306823	88543.191676	56.741684
2694.637974	88216.840825	56.746689
2693.955871	87912.457232	56.751693
2692.883947	87584.189191	56.756698
2692.636291	87276.151291	56.761703
2691.853374	86954.325925	56.766708
2691.238713	86637.277495	56.771713
2690.331897	86328.603274	56.776717
2689.814797	86009.558220	56.781722
2689.400519	85689.918470	56.786727
2688.621435	85377.973237	56.791732
2687.753901	85065.514143	56.796737
2687.059614	84750.262227	56.801741
2686.406307	84438.006632	56.806746
2685.778630	84115.084005	56.811751
2684.905452	83816.848669	56.816756
2684.371950	83505.811180	56.821761
2683.845023	83191.075764	56.826765
2683.077866	82883.659214	56.831770
2682.284723	82573.075966	56.836775
2681.518592	82264.749327	56.841780
2680.923936	81951.919260	56.846785
2680.427587	81640.320491	56.851789
2679.793833	81325.420917	56.856794
2679.395512	81020.483036	56.861799
2678.269809	80718.263207	56.866804
2678.072374	80403.048655	56.871809
2677.055984	80094.781151	56.876813
2675.944271	79782.040332	56.881818
2675.849796	79470.391484	56.886823
2674.895285	79170.391464	56.891828
2674.065674	78845.719420	56.896833
2673.481389	78553.546428	56.901837
2672.960427	78260.537466	56.906842
2672.475783	77946.920470	56.911847
2671.456781	77640.198299	56.916852
2671.135026	77326.932529	56.921857
2670.332316	77017.239054	56.926861
2669.646254	76710.383088	56.931866
2669.138969	76395.437618	56.936871
2668.339116	76096.459353	56.941876
2667.735995	75795.344485	56.946881
2666.928849	75478.655059	56.951885
2666.280047	75174.819622	56.956890
2665.816432	74871.320555	56.961895
2664.933023	74565.098624	56.966900
2664.250868	74269.904745	56.971905
2663.808262	73953.358960	56.976909
2662.336576	73651.982984	56.981914
2662.166617	73347.776239	56.986919
2661.519112	73045.784687	56.991924
2660.810595	72746.778454	56.996929
2659.883135	72451.067500	57.001933
2659.441047	72140.657162	57.006938
2659.300779	71837.773735	57.011943
2658.106234	71543.873311	57.016948
2657.843275	71241.088129	57.021953
2657.176435	70926.526366	57.026957
2656.063574	70630.890980	57.031962
2655.771961	70321.486169	57.036967
2654.971366	70011.299105	57.041972
2654.046256	69707.736638	57.046977
2653.407050	69415.781518	57.051981
2653.066176	69107.841431	57.056986
2652.774725	68802.590163	57.061991
2651.574903	68506.797917	57.066996
2650.902415	68183.350753	57.072001
2650.261338	67891.140065	57.077005
2649.618430	67588.572854	57.082010
2648.959528	67293.983176	57.087015
2648.238776	66994.901804	57.092020
2647.687682	66689.614037	57.097025
2646.997739	66390.784116	57.102029
2646.292734	66084.130750	57.107034
2646.077156	65780.314578	57.112039
2644.925431	65476.828845	57.117044
2644.474633	65172.239489	57.122049
2644.032559	64871.950097	57.127053
2642.734712	64571.592045	57.132058
2642.414193	64264.162806	57.137063
2642.082266	63970.268774	57.142068
2641.177147	63661.007438	57.147073
2640.328801	63363.316774	57.152077
2639.547268	63062.609435	57.157082
2638.833845	62763.171900	57.162087
2637.834882	62465.417884	57.167092
2637.353579	62167.703663	57.172097
2636.651161	61871.007364	57.177101
2636.114235	61580.646098	57.182106
2635.695663	61282.973883	57.187111
2634.721456	60983.412795	57.192116
2634.054082	60684.314343	57.197121
2633.545090	60397.939595	57.202125
2632.538450	60103.769436	57.207130
2632.261954	59797.884098	57.212135
2631.308717	59512.887911	57.217140
2630.879610	59212.452147	57.222145
2630.191371	58921.871188	57.227149
2629.133204	58620.766015	57.232154
2628.692735	58336.937819	57.237159
2628.068625	58056.165673	57.242164
2627.549127	57757.619300	57.247169
2626.737224	57464.317735	57.252173
2625.938945	57174.148739	57.257178
2625.505693	56877.536664	57.262183
2624.786354	56586.608011	57.267188
2624.207452	56301.798125	57.272193
2623.783831	55996.236200	57.277197
2622.728227	55706.991911	57.282202
2622.521971	55402.940274	57.287207
2621.445707	55117.502905	57.292212
2620.899142	54811.249226	57.297217
2620.320380	54531.270531	57.302221
2619.350529	54238.482249	57.307226
2618.603325	53946.071597	57.312231
2618.048527	53656.071653	57.317236
2617.296597	53368.335196	57.322241
2616.524173	53075.388829	57.327245
2615.718238	52783.196082	57.332250
2615.204200	52491.502860	57.337255
2614.374777	52209.900610	57.342260
2614.072805	51922.093723	57.347265
2613.441132	51635.428906	57.352269
2612.790108	51355.577216	57.357274
2612.214045	51054.707062	57.362279
2611.113023	50774.435860	57.367284
2610.199654	50493.136410	57.372289
2609.844505	50200.256147	57.377293
2609.355243	49912.976232	57.382298
2608.823410	49635.173086	57.387303
2607.911243	49349.585848	57.392308
2607.241179	49058.621732	57.397313
2606.818898	48779.935133	57.402317
2605.876707	48493.594537	57.407322
2605.517170	48202.392793	57.412327
2604.719829	47926.714598	57.417332
2604.384754	47630.972769	57.422337
2603.629066	47348.477110	57.427341
2602.763635	47060.936065	57.432346
2602.285199	46778.576414	57.437351
2601.116528	46485.294942	57.442356
2600.650531	46203.486596	57.447361
2600.102368	45921.120147	57.452365
2599.112269	45643.689589	57.457370
2598.829885	45352.563875	57.462375
2598.126846	45076.026696	57.467380
2597.464442	44789.202355	57.472385
2596.417791	44505.584136	57.477389
2595.557263	44218.841698	57.482394
2595.151609	43939.438586	57.487399
2594.256735	43673.491692	57.492404
2593.814674	43392.989946	57.497409
2593.289730	43116.775109	57.502413
2592.524860	42841.450210	57.507418
2591.971913	42556.406845	57.512423
2591.005674	42279.838921	57.517428
2590.231394	42001.916894	57.522433
2589.462873	41724.659329	57.527437
2588.745443	41457.529477	57.532442
2588.033473	41174.007731	57.537447
2587.501933	40919.093897	57.542452
2586.770453	40643.264501	57.547457
2586.325649	40368.856494	57.552461
2585.490164	40101.202097	57.557466
2584.855538	39823.070347	57.562471
2583.939529	39559.904813	57.567476
2583.383906	39284.624382	57.572481
2582.648938	39024.758207	57.577485
2581.871417	38757.479329	57.582490
2581.112988	38493.789986	57.587495
2580.109060	38237.603197	57.592500
2579.880235	37970.472656	57.597505
2579.060202	37717.000835	57.602509
2578.027955	37452.487500	57.607514
2577.515579	37196.134270	57.612519
2576.609650	36945.931138	57.617524
2576.099299	36689.646937	57.622529
2574.966159	36441.766540	57.627533
2574.224244	36188.771602	57.632538
2573.781458	35952.039426	57.637543
2573.016674	35717.454217	57.642548
2571.982979	35459.602716	57.647553
2571.146367	35217.594967	57.652557
2570.097573	35003.278930	57.657562
2569.067222	34776.034865	57.662567
2568.367292	34557.010189	57.667572
2567.281737	34344.045472	57.672577
2566.742865	34128.553603	57.677581
2565.419535	33917.697560	57.682586
2564.514541	33718.116700	57.687591
2563.305226	33533.327541	57.692596
2562.583366	33335.084488	57.697601
2561.922636	33151.742357	57.702605
2561.105507	32979.722675	57.707610
2560.280106	32802.116803	57.712615
2559.123793	32628.972512	57.717620
2558.500185	32461.924197	57.722625
2557.649335	32313.531349	57.727629
2556.713639	32151.187716	57.732634
2555.725260	31984.296861	57.737639
2554.669038	31839.579930	57.742644
2554.229858	31695.030359	57.747649
2553.445387	31534.239490	57.752653
2552.386950	31411.035194	57.757658
2552.059764	31267.446553	57.762663
2551.117735	31134.143351	57.767668
2550.757175	31001.749255	57.772673
2550.139868	30868.978205	57.777677
2549.488254	30742.565414	57.782682
2548.615233	30595.988087	57.787687
2547.892950	30481.034204	57.792692
2547.453269	30335.411217	57.797697
2546.866399	30208.425070	57.802701
2545.842862	30084.305671	57.807706
2545.450581	29953.127437	57.812711
2544.923079	29824.330551	57.817716
2543.963174	29699.448778	57.822721
2543.560316	29578.680692	57.827725
2542.874501	29451.645016	57.832730
2542.672228	29317.586875	57.837735
2541.942190	29197.565464	57.842740
2541.230021	29073.600316	57.847745
2540.648424	28931.800887	57.852749
2539.788393	28810.014536	57.857754
2539.262762	28674.674806	57.862759
2538.431490	28546.203166	57.867764
2537.834190	28410.093408	57.872769
2537.262310	28292.969943	57.877773
2536.288154	28172.898427	57.882778
2536.000212	28045.548436	57.887783
2535.491726	27924.878885	57.892788
2534.501780	27803.757328	57.897793
2534.232162	27676.148256	57.902797
2533.201989	27549.123597	57.907802
2532.788846	27418.377484	57.912807
2531.831971	27286.552000	57.917812
2531.363533	27165.850961	57.922817
2530.965288	27043.165102	57.927821
2530.088386	26931.424936	57.932826
2529.680835	26802.223890	57.937831
2529.148146	26675.774915	57.942836
2528.548864	26540.868306	57.947841
2527.787898	26419.096897	57.952845
2527.258543	26294.485112	57.957850
2526.693078	26159.597663	57.962855
2526.053197	26023.107234	57.967860
2525.341193	25889.667688	57.972865
2524.585227	25769.100881	57.977869
2523.716892	25638.828350	57.982874
2523.269228	25507.950003	57.987879
2522.648368	25378.913458	57.992884
2521.902957	25246.755275	57.997889
2521.165425	25120.163053	58.002893
2520.668521	24993.296770	58.007898
2520.237556	24859.632508	58.012903
2519.292390	24739.589126	58.017908
2519.006406	24603.722011	58.022913
2518.467301	24478.323535	58.027917
2517.235632	24347.492079	58.032922
2517.015051	24216.890758	58.037927
2516.472399	24081.259879	58.042932
2515.668759	23941.784686	58.047937
2514.870153	23809.686313	58.052941
2514.023979	23679.686051	58.057946
2513.709089	23551.398343	58.062951
2512.657630	23433.148927	58.067956
2511.964335	23292.730925	58.072961
2511.861779	23161.400967	58.077965
2510.814935	23034.933558	58.082970
2510.757667	22901.220962	58.087975
2509.806620	22766.458825	58.092980
2508.985505	22634.162177	58.097985
2508.671977	22498.209224	58.102989
2507.926401	22366.438198	58.107994
2507.325227	22239.566966	58.112999
2506.466297	22113.356651	58.118004
2505.812744	21966.514427	58.123009
2505.422996	21836.096885	58.128013
2504.356832	21710.247158	58.133018
2504.148500	21562.381155	58.138023
2503.319019	21433.447599	58.143028
2502.656942	21301.423512	58.148033
2501.906395	21175.369327	58.153037
2501.147074	21040.747065	58.158042
2500.549451	20903.551311	58.163047
2499.733821	20779.287070	58.168052
2499.495658	20642.898381	58.173057
2498.821373	20510.036501	58.178061
2497.547703	20377.547873	58.183066
2497.185113	20251.633819	58.188071
2496.818031	20121.907433	58.193076
2495.865701	19994.257691	58.198081
2495.449979	19853.892608	58.203085
2494.282391	19729.411417	58.208090
2493.908729	19590.926106	58.213095
2492.739899	19470.222021	58.218100
2492.163886	19342.210846	58.223105
2491.822338	19212.556234	58.228109
2491.104019	19095.876926	58.233114
2490.785151	18959.977893	58.238119
2490.151895	18825.628217	58.243124
2489.251567	18694.236189	58.248129
2488.695360	18563.105303	58.253133
2488.020700	18432.782524	58.258138
2487.107700	18291.877588	58.263143
2486.587604	18176.018011	58.268148
2485.911885	18057.313738	58.273153
2485.551533	17914.950282	58.278157
2484.547911	17790.813017	58.283162
2483.854033	17664.656189	58.288167
2483.285238	17526.402294	58.293172
2482.654885	17404.582962	58.298177
2482.065850	17265.770404	58.303181
2481.057544	17141.901732	58.308186
2480.498097	17014.492178	58.313191
2480.147226	16894.024159	58.318196
2479.544501	16758.482206	58.323201
2478.756229	16624.845484	58.328205
2477.797878	16497.792704	58.333210
2477.308487	16362.334922	58.338215
2476.405242	16243.007931	58.343220
2475.855158	16114.564210	58.348225
2475.269341	15988.418914	58.353229
2474.580080	15872.842533	58.358234
2474.278320	15737.336715	58.363239
2473.330667	15609.121437	58.368244
2472.769129	15482.440029	58.373249
2472.118728	15354.230562	58.378253
2471.254845	15230.915892	58.383258
2470.607245	15089.104637	58.388263
2469.498775	14972.231750	58.393268
2469.159075	14850.509820	58.398273
2468.714124	14735.849341	58.403277
2467.464109	14611.723465	58.408282
2467.247915	14482.770953	58.413287
2466.364483	14361.022101	58.418292
2465.551673	14229.719276	58.423297
2465.012269	14105.787976	58.428301
2464.424174	13988.799358	58.433306
2463.845114	13868.746394	58.438311
2463.220818	13760.396394	58.443316
2462.564683	13627.215899	58.448321
2461.897177	13505.022362	58.453325
2461.217195	13384.249491	58.458330
2460.897031	13257.951559	58.463335
2459.821996	13134.275516	58.468340
2459.126077	13008.936070	58.473345
2458.713784	12879.208554	58.478349
2458.022187	12765.444935	58.483354
2457.647813	12641.351499	58.488359
2456.684235	12526.223232	58.493364
2456.087921	12391.774274	58.498369
2455.692435	12270.950138	58.503373
2454.806623	12143.568661	58.508378
2454.272593	12009.697333	58.513383
2453.344146	11883.851272	58.518388
2452.605072	11768.373388	58.523393
2452.213476	11635.428283	58.528397
2451.671142	11521.028936	58.533402
2450.765772	11398.344205	58.538407
2449.926056	11281.116549	58.543412
2449.352465	11149.141157	58.548417
2448.790883	11028.951928	58.553421
2447.763735	10905.951018	58.558426
2447.415296	10781.963166	58.563431
2446.615692	10660.202249	58.568436
2445.626553	10544.591880	58.573441
2445.532748	10427.002485	58.578445
2444.622982	10315.419778	58.583450
2444.463745	10183.935479	58.588455
2443.452995	10064.873303	58.593460
2442.768000	9938.119617	58.598465
2441.926459	9810.004025	58.603469
2441.136042	9699.984891	58.608474
2440.346102	9574.887602	58.613479
2440.022452	9463.961088	58.618484
2439.379847	9344.203657	58.623489
2438.679428	9230.240822	58.628493
2438.104003	9107.998550	58.633498
2437.419875	8981.853166	58.638503
2436.659859	8878.273239	58.643508
2435.916297	8754.765100	58.648513
2435.333212	8631.660912	58.653517
2434.412318	8523.943133	58.658522
2434.095106	8394.547118	58.663527
2433.430096	8284.430921	58.668532
2432.808273	8171.957825	58.673537
2432.590143	8051.681143	58.678541
2431.691341	7916.767053	58.683546
2431.331903	7791.414847	58.688551
2430.338088	7671.214112	58.693556
2429.436719	7550.829694	58.698561
2428.917001	7432.924231	58.703565
2427.691810	7320.508245	58.708570
2427.196368	7197.054501	58.713575
2426.445085	7089.083540	58.718580
2425.813941	6979.548234	58.723585
2424.760532	6861.665645	58.728589
2424.213018	6747.817402	58.733594
2423.536288	6640.558057	58.738599
2422.574715	6532.793279	58.743604
2422.479214	6422.814307	58.748609
2421.807758	6307.579524	58.753613
2420.799277	6217.834726	58.758618
2420.398062	6097.766122	58.763623
2419.824099	5986.560824	58.768628
2419.035076	5880.269717	58.773633
2418.386010	5779.842860	58.778637
2417.757962	5673.798255	58.783642
2417.004550	5557.903183	58.788647
2416.120524	5457.597005	58.793652
2415.292541	5350.433286	58.798657
2414.613591	5237.247676	58.803661
2413.564309	5154.465252	58.808666
2412.984943	5052.745880	58.813671
2412.746086	4963.315736	58.818676
2411.853667	4860.786838	58.823681
2411.228815	4764.937524	58.828685
2410.104091	4668.513471	58.833690
2409.928503	4568.767459	58.838695
2408.969382	4486.792361	58.843700
2408.113162	4387.520650	58.848705
2407.606331	4302.055949	58.853709
2406.480511	4217.953334	58.858714
2405.869867	4126.840306	58.863719
2405.217350	4047.355394	58.868724
2404.310072	3958.057834	58.873729
2403.823177	3881.117003	58.878733
2402.901235	3812.178562	58.883738
2402.306523	3722.549752	58.888743
2401.768731	3635.335161	58.893748
2401.120167	3558.633796	58.898753
2400.864527	3476.568572	58.903757
2399.615150	3405.583049	58.908762
2399.179053	3322.874598	58.913767
2398.487937	3241.370258	58.918772
2397.716155	3162.228441	58.923777
2396.762927	3084.574747	58.928781
2396.099589	3014.066793	58.933786
2395.795113	2932.970510	58.938791
2395.032289	2869.621386	58.943796
2393.935654	2787.038830	58.948801
2393.376700	2715.712187	58.953805
2392.525220	2661.859234	58.958810
2392.135332	2583.462778	58.963815
2391.375512	2513.723265	58.968820
2390.510118	2439.769334	58.973825
2389.947325	2372.409928	58.978829
2389.251367	2320.791253	58.983834
2389.151870	2243.771576	58.988839
2388.018835	2178.960644	58.993844
2387.324415	2109.421663	58.998849
2387.098902	2031.696035	59.003853
2386.319868	1971.137761	59.008858
2385.422296	1905.414635	59.013863
2384.840010	1831.418112	59.018868
2384.123891	1768.564723	59.023873
2383.320940	1713.060327	59.028877
2382.491505	1651.498107	59.033882
2381.975910	1578.846991	59.038887
2381.213453	1515.689786	59.043892
2380.270134	1461.282579	59.048897
2379.914839	1400.445804	59.053901
2378.996487	1354.413836	59.058906
2378.309995	1289.165466	59.063911
2377.644308	1234.845979	59.068916
2376.803035	1173.172542	59.073921
2376.435155	1122.054901	59.078925
2375.703867	1076.637572	59.083930
2375.282786	1014.375408	59.088935
2374.568549	961.234773	59.093940
2373.646155	910.149032	59.098945
2373.330568	840.358928	59.103949
2372.296051	792.513142	59.108954
2371.814685	725.487498	59.113959
2371.084002	684.810078	59.118964
2370.628115	627.247335	59.123969
2369.990007	569.898217	59.128973
2369.018691	527.449061	59.133978
2368.477109	459.926417	59.138983
2367.727049	410.562358	59.143988
2366.832535	370.982534	59.148993
2366.215109	322.271092	59.153997
2365.604127	270.665155	59.159002
2364.745823	223.677961	59.164007
2363.959331	183.359300	59.169012
2363.237256	147.802236	59.174017
2362.626270	100.593307	59.179021
2361.695503	74.800541	59.184026
2361.123391	21.752781	59.189031
2360.179711	-10.671745	59.194036
2359.173046	-34.407061	59.199041
2358.335009	-70.225882	59.204045
2356.089278	-67.044464	59.209050
2351.031933	56.009677	59.214055
2351.327671	55.468766	59.219060
2352.310775	63.800827	59.224065
2353.434607	45.524202	59.229069
2353.102560	40.692780	59.234074
2353.262011	41.326187	59.239079
2352.723452	34.228411	59.244084
2351.364609	55.516982	59.249089
2350.587811	45.557078	59.254093
2349.271849	59.943122	59.259098
2348.818720	49.490362	59.264103
2348.295789	51.190724	59.269108
2347.753687	61.344683	59.274113
2347.308537	56.908069	59.279117
2346.696684	54.178856	59.284122
2346.205317	56.118632	59.289127
2345.398824	59.991187	59.294132
2344.092811	62.493790	59.299137
2344.239074	55.011456	59.304141
2343.408868	72.363883	59.309146
2342.832488	67.709966	59.314151
2342.437995	63.924459	59.319156
2342.133755	70.043287	59.324161
2341.449849	57.950882	59.329165
2340.151829	68.366636	59.334170
2339.405917	65.368534	59.339175
2338.502268	67.985524	59.344180
2338.113905	68.658494	59.349185
2337.745839	69.157942	59.354189
2336.752471	71.066944	59.359194
2336.075466	63.533814	59.364199
2335.870557	65.816083	59.369204
2335.433054	67.944432	59.374209
2334.854923	60.375125	59.379213
2333.905701	70.308234	59.384218
2332.964193	64.818124	59.389223
2332.259063	73.093061	59.394228
2332.048843	74.070507	59.399233
2331.594720	66.453148	59.404237
2330.650766	70.932535	59.409242
2329.721098	75.614653	59.414247
2329.025475	67.638215	59.419252
2328.231775	70.367078	59.424257
2328.007665	64.318523	59.429261
2327.460836	69.269499	59.434266
2326.865510	66.584975	59.439271
2326.196373	70.913553	59.444276
2325.133067	74.082549	59.449281
2324.790449	65.398877	59.454285
2323.509683	74.854733	59.459290
2323.321751	68.287950	59.464295
2322.874779	62.981184	59.469300
2322.211772	76.766986	59.474305
2321.618480	61.675159	59.479309
2320.658372	76.376942	59.484314
2320.156846	67.636472	59.489319
2319.562940	72.829874	59.494324
2318.693509	73.079261	59.499329
2317.918522	67.505981	59.504333
2317.094448	70.801038	59.509338
2316.745566	67.271642	59.514343
2316.464438	73.393115	59.519348
2315.761839	79.201398	59.524353
2315.583560	68.006483	59.529357
2314.502836	73.351201	59.534362
2313.669753	74.102585	59.539367
2312.889164	68.948071	59.544372
2312.106603	73.651018	59.549377
2311.596582	69.715109	59.554381
2310.842091	76.195492	59.559386
2310.259485	68.691550	59.564391
2309.289951	70.336596	59.569396
2308.350457	73.892801	59.574401
2308.159321	72.210159	59.579405
2307.883239	72.581487	59.584410
2307.611977	71.890802	59.589415
2306.254816	73.171561	59.594420
2306.132337	75.399761	59.599425
2305.045365	63.491131	59.604429
2304.347356	76.777880	59.609434
2303.926006	65.804437	59.614439
2303.235783	64.808050	59.619444
2302.703653	68.214500	59.624449
2301.859041	69.693085	59.629453
2300.835573	78.901575	59.634458
2300.559087	73.668694	59.639463
2300.170414	78.706555	59.644468
2299.321059	75.540371	59.649473
2298.719667	70.370057	59.654477
2297.863515	77.514669	59.659482
2296.836927	74.024947	59.664487
2296.606093	73.247430	59.669492
2296.076598	67.709339	59.674497
2295.606260	65.493836	59.679501
2294.350280	72.094753	59.684506
2294.204037	62.309237	59.689511
2293.273291	65.234878	59.694516
2292.235222	63.593521	59.699521
2292.185129	56.599625	59.704525
2291.489864	64.574967	59.709530
2290.661117	62.700148	59.714535
2290.151525	67.585302	59.719540
2288.600711	68.087837	59.724545
2288.979505	62.528697	59.729549
2288.352354	67.757334	59.734554
2287.490851	62.516320	59.739559
2286.492896	68.778284	59.744564
2286.131817	73.236203	59.749569
2285.752102	68.502227	59.754573
2284.350890	67.596528	59.759578
2283.763501	61.889435	59.764583
2283.732189	70.109550	59.769588
2282.730931	72.682117	59.774593
2281.860962	67.842975	59.779597
2281.306599	72.618543	59.784602
2281.010521	67.809805	59.789607
2280.172765	65.952186	59.794612
2278.932696	77.342758	59.799617
2279.302941	63.488949	59.804621
2278.230911	70.417074	59.809626
2277.215206	73.103893	59.814631
2276.807389	59.837094	59.819636
2276.149124	71.119619	59.824641
2275.434596	63.485231	59.829645
2274.994190	61.553558	59.834650
2273.868326	65.265481	59.839655
2273.630091	67.649228	59.844660
2273.273905	70.354446	59.849665
2272.079722	67.821683	59.854669
2271.065696	81.128599	59.859674
2270.907026	65.258256	59.864679
2270.688108	60.211789	59.869684
2269.553297	68.797723	59.874689
2269.119110	67.450089	59.879693
2268.426907	59.100988	59.884698
2267.834769	61.935087	59.889703
2267.439047	61.568487	59.894708
2266.626700	73.725396	59.899713
2266.162072	60.508609	59.904718
2264.994053	71.438340	59.909722
2263.897805	59.709395	59.914727
2263.613272	57.420278	59.919732
2263.137462	71.764570	59.924737
2262.403582	70.472354	59.929742
2261.513938	70.682390	59.934746
2260.701025	72.520222	59.939751
2260.309920	71.424366	59.944756
2259.968580	72.890950	59.949761
2259.470404	61.265837	59.954766
2258.287411	71.264426	59.959770
2257.675247	65.835647	59.964775
2257.163880	67.348120	59.969780
2256.550885	68.799444	59.974785
2256.066124	64.932080	59.979790
2255.548661	68.829777	59.984794
2254.784793	62.515196	59.989799
2253.778680	69.003959	59.994804
2252.672605	76.661288	59.999809
2252.424906	70.359449	60.004814
2251.950598	71.880238	60.009818
2251.329301	66.609021	60.014823
2250.387349	57.618323	60.019828
2249.767352	64.731791	60.024833
2249.216362	69.571480	60.029838
2248.280571	68.104721	60.034842
2247.982356	67.883500	60.039847
2247.277678	66.741193	60.044852
2246.799606	62.141093	60.049857
2246.386921	61.994797	60.054862
2245.848996	67.636627	60.059866
2244.694966	67.595301	60.064871
2243.556245	68.694793	60.069876
2242.666189	70.328832	60.074881
2242.799334	62.613620	60.079886
2242.158281	64.884649	60.084890
2241.378163	65.216086	60.089895
2240.844560	67.455881	60.094900
2240.197478	66.403784	60.099905
2239.335406	63.707977	60.104910
2238.853885	71.233130	60.109914
2238.299144	66.227316	60.114919
2237.347381	70.985502	60.119924
2236.241533	74.121855	60.124929
2235.873647	70.373145	60.129934
2235.498965	66.944046	60.134938
2234.729181	67.261230	60.139943
2234.232146	60.276731	60.144948
2233.343941	69.793349	60.149953
2232.740959	59.966755	60.154958
2232.009479	65.872666	60.159962
2231.415539	67.920191	60.164967
2231.118641	68.250675	60.169972
2230.522896	71.167353	60.174977
2230.099778	64.450239	60.179982
2228.781627	66.341411	60.184986
2227.831100	68.696224	60.189991
2227.100559	73.841930	60.194996
2226.525472	67.931057	60.200001
2225.792933	62.395231	60.205006
2225.317946	78.171214	60.210010
2225.157470	64.493047	60.215015
2225.089794	62.975327	60.220020
2224.004935	66.253428	60.225025
2222.955139	63.805014	60.230030
2221.995116	65.018089	60.235034
2221.405430	70.035802	60.240039
2220.911534	67.093951	60.245044
2220.096303	65.931341	60.250049
2219.716597	62.070975	60.255054
2219.166591	68.085294	60.260058
2218.352504	63.956376	60.265063
2217.824851	68.532180	60.270068
2216.692670	65.653731	60.275073
2216.383434	61.030012	60.280078
2215.489681	59.167106	60.285082
2214.765656	69.496589	60.290087
2214.588631	61.583007	60.295092
2214.018246	61.717187	60.300097
2213.767631	58.689443	60.305102
2212.182318	63.450362	60.310106
2211.002668	70.214237	60.315111
2210.573711	62.455730	60.320116
2210.073486	65.418758	60.325121
2209.803279	55.924149	60.330126
2208.904121	67.922953	60.335130
2208.427509	70.655165	60.340135
2208.418395	59.600593	60.345140
2207.674982	65.068451	60.350145
2206.525504	67.322370	60.355150
2205.616562	68.614077	60.360154
2204.621016	65.843264	60.365159
2204.197584	57.224481	60.370164
2203.639257	65.960253	60.375169
2203.337139	51.840965	60.380174
2202.837254	56.820778	60.385178
2202.195582	60.921103	60.390183
2201.509541	56.817610	60.395188
2200.155690	63.943420	60.400193
2199.661717	58.735599	60.405198
2198.925556	60.764691	60.410202
2198.436824	66.949058	60.415207
2198.224439	59.026896	60.420212
2197.628266	64.668510	60.425217
2197.058715	61.147334	60.430222
2195.606577	62.649785	60.435226
2194.692700	69.652192	60.440231
2194.251674	62.799161	60.445236
2193.679176	67.503504	60.450241
2193.238947	55.083934	60.455246
2192.767788	60.853943	60.460250
2192.056770	64.113752	60.465255
2191.857278	54.751427	60.470260
2190.631756	64.567554	60.475265
2189.646110	54.434265	60.480270
2188.772718	60.621305	60.485274
2188.241087	62.037660	60.490279
2188.080863	59.886522	60.495284
2187.198321	62.497056	60.500289
2187.071618	58.804711	60.505294
2186.559340	63.945760	60.510298
2185.415768	61.868615	60.515303
2184.926524	61.415942	60.520308
2184.095391	70.317992	60.525313
2183.443940	58.192116	60.530318
2182.858811	56.542027	60.535322
2181.659195	59.012057	60.540327
2180.923843	63.072057	60.545332
2180.067348	67.424078	60.550337
2180.293456	53.411803	60.555342
2179.713779	59.727285	60.560346
2178.646863	58.150472	60.565351
2178.325432	64.648908	60.570356
2177.672015	66.762647	60.575361
2177.110387	70.679978	60.580366
2175.968033	73.104661	60.585370
2175.497081	65.554665	60.590375
2174.903216	63.477049	60.595380
2174.475327	70.470173	60.600385
2174.060723	57.336942	60.605390
2172.727746	64.390069	60.610394
2171.897235	64.975514	60.615399
2171.385812	62.668788	60.620404
2170.760768	55.499620	60.625409
2170.438751	54.184671	60.630414
2169.760950	60.886290	60.635418
2168.577130	53.924034	60.640423
2168.064630	59.500339	60.645428
2167.241687	66.734322	60.650433
2166.810491	57.580637	60.655438
2166.208778	67.447618	60.660442
2165.460036	60.749062	60.665447
2165.594645	51.333742	60.670452
2164.081203	58.319309	60.675457
2163.355167	53.384847	60.680462
2162.564029	65.448520	60.685466
2162.290543	60.434377	60.690471
2162.372759	58.721001	60.695476
2161.053859	65.800284	60.700481
2159.959459	60.578920	60.705486
2159.490510	60.045764	60.710490
2158.484283	70.826863	60.715495
2158.344407	60.956786	60.720500
2157.765021	63.847228	60.725505
2157.573614	67.860363	60.730510
2156.712444	60.184631	60.735514
2155.423727	60.251439	60.740519
2154.737656	60.269949	60.745524
2153.598232	70.364158	60.750529
2153.665281	57.969772	60.755534
2153.062181	61.917337	60.760538
2152.754533	56.342515	60.765543
2152.159497	57.426750	60.770548
2150.692536	65.247010	60.775553
2150.275817	59.787258	60.780558
2149.852518	60.558832	60.785562
2148.998768	63.522763	60.790567
2148.844312	63.917387	60.795572
2147.618071	64.155630	60.800577
2147.009817	60.995406	60.805582
2146.610959	57.778309	60.810586
2146.072370	59.999988	60.815591
2145.432243	56.532598	60.820596
2144.295633	59.358486	60.825601
2143.642005	60.155564	60.830606
2142.577754	64.917430	60.835610
2142.114491	60.218816	60.840615
2141.872253	60.266259	60.845620
2140.999425	73.512952	60.850625
2140.973678	63.364582	60.855630
2140.750066	70.714792	60.860634
2139.423213	53.377246	60.865639
2138.555746	64.131600	60.870644
2137.591121	69.429574	60.875649
2137.495863	56.796024	60.880654
2135.770298	63.458884	60.885658
2135.480685	67.378795	60.890663
2135.180139	58.578113	60.895668
2134.145708	58.757547	60.900673
2133.626882	52.292178	60.905678
2133.306392	57.513186	60.910682
2132.726849	67.647878	60.915687
2132.233988	54.252699	60.920692
2131.439470	54.868714	60.925697
2130.979531	49.548285	60.930702
2129.840691	62.157536	60.935706
2128.917944	55.188571	60.940711
2128.665327	57.286038	60.945716
2128.090520	65.880936	60.950721
2127.527844	59.215950	60.955726
2126.593164	67.856907	60.960730
2125.658881	58.458211	60.965735
2125.166939	48.068441	60.970740
2124.711399	60.416325	60.975745
2124.566407	51.493203	60.980750
2123.428745	60.525891	60.985754
2122.133971	59.005752	60.990759
2121.766865	55.763123	60.995764
2120.897900	62.715845	61.000769
2120.370413	61.346773	61.005774
2120.290050	57.317513	61.010778
2119.972733	61.513044	61.015783
2119.132323	61.357361	61.020788
2117.807727	64.580501	61.025793
2117.478362	56.509765	61.030798
2116.920273	59.155571	61.035802
2116.316133	56.188660	61.040807
2115.006169	50.990483	61.045812
2114.162385	66.582127	61.050817
2113.740681	60.112388	61.055822
2113.324101	62.081336	61.060826
2112.811095	56.879710	61.065831
2112.528489	50.876741	61.070836
2112.004964	56.010120	61.075841
2111.267107	53.810294	61.080846
2110.537065	50.366643	61.085850
2109.809249	55.393669	61.090855
2108.762395	59.096271	61.095860
2107.749962	62.369230	61.100865
2107.372071	57.455238	61.105870
2106.723958	57.627003	61.110874
2106.335756	53.386401	61.115879
2106.151593	62.100661	61.120884
2104.850996	69.016223	61.125889
2103.984949	61.112637	61.130894
2103.250539	60.604264	61.135898
2102.809335	60.678549	61.140903
2102.063297	59.730494	61.145908
2101.610661	57.818139	61.150913
2101.136174	54.127370	61.155918
2100.079564	60.247312	61.160922
2099.362749	56.785795	61.165927
2099.118027	56.343224	61.170932
2098.219982	73.299609	61.175937
2098.126325	60.774613	61.180942
2097.048915	69.163847	61.185946
2096.081201	56.511044	61.190951
2095.556741	57.546248	61.195956
2094.926476	71.872474	61.200961
2094.630704	57.835778	61.205966
2093.231438	66.142043	61.210970
2092.441204	64.953431	61.215975
2091.921917	61.908410	61.220980
2091.223706	73.925819	61.225985
2091.140382	63.818129	61.230990
2090.933761	61.734282	61.235994
2089.984227	70.814404	61.240999
2089.326680	60.479296	61.246004
2088.154081	59.326125	61.251009
2087.593366	66.124297	61.256014
2087.073597	61.966071	61.261018
2086.715928	60.134840	61.266023
2085.975119	56.997242	61.271028
2084.942844	59.429723	61.276033
2084.628645	53.412848	61.281038
2083.913102	54.367991	61.286042
2082.761373	59.659398	61.291047
2081.883877	60.583472	61.296052
2081.297718	64.857932	61.301057
2080.912538	64.240539	61.306062
2080.847843	61.422997	61.311066
2079.913523	68.729864	61.316071
2079.514186	60.291783	61.321076
2078.334067	62.556922	61.326081
2077.504257	56.052606	61.331086
2077.084687	53.988359	61.336090
2076.261849	56.863830	61.341095
2076.096175	63.159367	61.346100
2075.560970	63.142920	61.351105
2074.300380	59.690426	61.356110
2073.556442	55.785385	61.361114
2072.839861	57.152263	61.366119
2072.720686	54.665053	61.371124
2072.240508	59.742677	61.376129
2071.562945	50.585539	61.381134
2070.429808	52.147819	61.386138
2069.860549	50.816924	61.391143
2069.314514	49.804029	61.396148
2068.431475	57.383441	61.401153
2067.504976	54.831955	61.406158
2066.842018	60.328073	61.411162
2066.165712	51.796760	61.416167
2066.224580	53.608272	61.421172
2065.169660	60.046489	61.426177
2065.185959	52.860740	61.431182
2064.319694	56.239824	61.436186
2063.275751	59.770099	61.441191
2062.545127	51.349905	61.446196
2061.868074	54.569660	61.451201
2061.565528	47.789308	61.456206
2060.605139	52.432220	61.461210
2059.712971	52.748374	61.466215
2059.787163	46.907986	61.471220
2058.771746	52.732833	61.476225
2058.348370	48.422133	61.481230
2057.128152	45.688611	61.486234
2056.343426	53.894216	61.491239
2056.200045	52.602974	61.496244
2055.519660	54.066610	61.501249
2054.527613	51.307920	61.506254
2052.958715	60.010108	61.511258
2053.149084	56.256424	61.516263
2053.006525	55.592651	61.521268
2051.788774	60.400981	61.526273
2051.243076	58.982776	61.531278
2050.842440	58.240113	61.536282
2050.382417	60.914522	61.541287
2049.409126	55.948372	61.546292
2048.447152	61.247526	61.551297
2047.780105	55.633563	61.556302
2047.350362	54.791445	61.561306
2046.796130	56.988816	61.566311
2046.616612	58.152211	61.571316
2045.304585	65.763439	61.576321
2044.574172	57.786318	61.581326
2043.824406	66.060498	61.586330
2043.357222	62.803802	61.591335
2043.018297	46.437033	61.596340
2042.442574	62.538055	61.601345
2041.722378	51.558504	61.606350
2040.432099	51.817996	61.611354
2040.016902	56.371247	61.616359
2040.035623	54.229571	61.621364
2039.049571	58.118082	61.626369
2038.030652	51.411990	61.631374
2037.415512	59.388850	61.636378
2036.834887	58.663712	61.641383
2036.910729	56.533471	61.646388
2035.641710	55.783539	61.651393
2034.778805	53.717115	61.656398
2033.783357	62.556962	61.661402
2033.582073	56.249376	61.666407
2033.508570	52.485529	61.671412
2032.194459	55.964075	61.676417
2030.985948	52.020813	61.681422
2030.761242	63.770701	61.686426
2030.227712	63.339276	61.691431
2029.960689	57.013739	61.696436
2028.885726	56.239322	61.701441
2027.927889	49.873610	61.706446
2027.175280	60.095694	61.711450
2026.741099	56.108397	61.716455
2026.377504	55.388244	61.721460
2025.782659	56.973925	61.726465
2025.498204	52.787835	61.731470
2024.612332	53.233883	61.736474
2023.647928	52.503422	61.741479
2023.213480	51.428676	61.746484
2022.588015	52.729070	61.751489
2021.559169	63.108529	61.756494
2020.866970	56.568203	61.761498
2019.843718	56.624487	61.766503
2019.486840	50.734242	61.771508
2019.021633	60.790875	61.776513
2018.671420	56.635720	61.781518
2018.006550	53.539707	61.786522
2017.110738	49.816476	61.791527
2016.507211	46.557773	61.796532
2015.531542	64.846330	61.801537
2015.497544	49.806219	61.806542
2014.388658	57.011496	61.811546
2013.414507	53.720149	61.816551
2013.179112	49.952035	61.821556
2012.539600	54.545617	61.826561
2012.067445	49.014275	61.831566
2010.736390	63.521096	61.836570
2010.081025	50.437167	61.841575
2009.688016	43.915599	61.846580
2008.761660	54.797585	61.851585
2008.543710	48.268734	61.856590
2008.066772	55.607101	61.861594
2007.428248	54.380249	61.866599
2006.804720	47.868456	61.871604
2005.596637	57.923139	61.876609
2005.434528	48.972792	61.881614
2004.537337	54.307406	61.886618
2003.495324	52.460221	61.891623
2003.301433	55.559158	61.896628
2002.134832	60.704729	61.901633
2002.058601	43.044240	61.906638
2001.791426	56.327283	61.911642
2000.417540	56.185343	61.916647
1999.871296	53.400077	61.921652
1999.125459	64.787988	61.926657
1998.678301	52.577727	61.931662
1998.246832	60.799822	61.936666
1997.078177	59.157232	61.941671
1996.521433	62.963434	61.946676
1996.035913	66.556493	61.951681
1995.470337	59.470976	61.956686
1994.815703	51.611155	61.961690
1993.754781	56.109202	61.966695
1993.249999	55.285309	61.971700
1992.619964	59.349136	61.976705
1992.186493	53.822696	61.981710
1991.101042	62.522304	61.986714
1990.020231	52.998701	61.991719
1989.769054	57.637885	61.996724
1988.891088	59.514501	62.001729
1989.081795	59.477478	62.006734
1988.468702	60.933605	62.011738
1987.557164	53.926653	62.016743
1986.700377	54.237216	62.021748
1986.119334	61.927987	62.026753
1985.695381	55.081762	62.031758
1984.598144	63.661823	62.036762
1983.718703	64.707657	62.041767
1983.458591	52.399909	62.046772
1982.751074	65.614080	62.051777
1982.511167	62.534204	62.056782
1981.630862	54.327019	62.061786
1980.332383	71.567736	62.066791
1979.976519	62.424218	62.071796
1979.722498	57.082178	62.076801
1979.154636	53.557636	62.081806
1978.054597	61.479006	62.086810
1977.172655	52.680751	62.091815
1976.946397	51.965615	62.096820
1976.181031	56.397838	62.101825
1975.494105	58.386057	62.106830
1974.586606	62.815609	62.111834
1973.872679	60.910057	62.116839
1973.785132	52.327908	62.121844
1972.892911	52.921631	62.126849
1972.541273	47.984579	62.131854
1971.489879	51.367840	62.136858
1970.435970	55.461100	62.141863
1970.369938	55.365479	62.146868
1969.889209	59.924409	62.151873
1968.802558	54.514257	62.156878
1967.561001	54.772359	62.161882
1967.264366	63.614849	62.166887
1967.260448	50.323468	62.171892
1966.788678	58.752224	62.176897
1966.018611	49.226623	62.181902
1965.083215	50.579374	62.186906
1963.934086	60.221033	62.191911
1963.910957	46.784478	62.196916
1962.127422	60.416999	62.201921
1961.732009	57.740260	62.206926
1961.164552	53.711056	62.211930
1960.627813	53.556110	62.216935
1960.183607	41.414785	62.221940
1959.283101	69.004494	62.226945
1959.302491	49.028157	62.231950
1958.987935	57.663762	62.236954
1957.985788	59.399255	62.241959
1957.422977	54.576141	62.246964
1956.737589	56.237706	62.251969
1955.668270	57.081883	62.256974
1955.031865	57.355901	62.261978
1954.107759	52.292102	62.266983
1953.830395	50.025543	62.271988
1952.517301	63.028339	62.276993
1951.877014	49.912079	62.281998
1951.374518	54.561193	62.287002
1950.568192	60.270892	62.292007
1950.665189	55.888657	62.297012
1950.248047	58.799114	62.302017
1949.533102	52.396460	62.307022
1948.362704	55.868002	62.312026
1947.884457	51.799412	62.317031
1947.471170	44.525749	62.322036
1946.269565	59.833597	62.327041
1945.483258	53.923220	62.332046
1945.138845	55.566935	62.337050
1944.784067	55.491915	62.342055
1944.057244	49.081688	62.347060
1942.544343	58.159801	62.352065
1942.026488	54.390798	62.357070
1941.623502	53.938672	62.362074
1941.084549	54.137303	62.367079
1941.005249	48.027982	62.372084
1939.917088	52.085689	62.377089
1939.277043	55.491977	62.382094
1938.488270	52.133391	62.387098
1937.865918	49.897939	62.392103
1937.259699	54.960892	62.397108
1936.373545	54.796760	62.402113
1935.669790	59.548782	62.407118
1934.884061	57.831249	62.412122
1934.406402	57.917655	62.417127
1934.262480	49.539995	62.422132
1933.195910	48.341683	62.427137
1932.285405	47.774581	62.432142
1931.677331	43.860639	62.437146
1931.272811	51.376743	62.442151
1931.085829	50.999138	62.447156
1930.198610	48.772614	62.452161
1929.093785	54.558080	62.457166
1928.494987	47.810585	62.462170
1927.769872	52.004626	62.467175
1927.436676	51.651806	62.472180
1926.555207	59.415501	62.477185
1925.649049	52.325724	62.482190
1925.206236	53.174542	62.487194
1924.934049	55.593659	62.492199
1924.343060	52.597905	62.497204
1923.277405	53.236519	62.502209
1922.512660	44.094853	62.507214
1921.959790	51.800078	62.512218
1921.482310	61.015033	62.517223
1920.690683	47.818735	62.522228
1919.546200	47.227280	62.527233
1919.050223	53.368670	62.532238
1918.529444	50.426425	62.537242
1918.068173	56.876107	62.542247
1917.958450	47.728234	62.547252
1916.998323	53.429237	62.552257
1915.856750	48.474088	62.557262
1915.723965	52.493689	62.562266
1914.782194	56.537631	62.567271
1913.653715	54.790936	62.572276
1913.020315	50.794289	62.577281
1912.576060	52.643081	62.582286
1912.167950	50.124480	62.587290
1911.889126	48.326492	62.592295
1910.720512	52.672935	62.597300
1909.835651	43.334308	62.602305
1909.452527	43.410443	62.607310
1908.983213	52.758132	62.612314
1908.261481	50.111128	62.617319
1907.709746	49.958573	62.622324
1906.633821	49.547043	62.627329
1906.188261	52.159254	62.632334
1906.187884	49.061868	62.637338
1904.685913	52.141380	62.642343
1903.812272	42.034611	62.647348
1903.300187	40.313074	62.652353
1902.914481	44.328669	62.657358
1902.509076	45.218858	62.662362
1901.133416	46.725092	62.667367
1900.871205	42.808294	62.672372
1900.337551	47.031870	62.677377
1899.928707	50.655342	62.682382
1898.675614	43.172819	62.687386
1897.779985	49.640990	62.692391
1897.329992	50.300150	62.697396
1896.998891	51.856605	62.702401
1896.815075	40.528635	62.707406
1895.992111	47.027847	62.712410
1895.016335	56.757120	62.717415
1894.632221	43.463034	62.722420
1893.222066	52.557971	62.727425
1892.694292	46.672805	62.732430
1892.067209	53.776408	62.737434
1891.321188	47.624703	62.742439
1891.411251	47.466460	62.747444
1890.562499	53.894079	62.752449
1889.420687	55.221278	62.757454
1888.977143	43.038869	62.762458
1888.186674	42.673492	62.767463
1888.033678	48.115493	62.772468
1887.070337	47.173613	62.777473
1886.022020	52.445521	62.782478
1885.663702	46.758950	62.787482
1884.789067	50.155182	62.792487
1884.578427	49.013394	62.797492
1883.579543	55.304006	62.802497
1882.981624	49.382670	62.807502
1882.533654	55.756130	62.812506
1881.818227	56.200398	62.817511
1881.334249	49.335345	62.822516
1880.006300	51.639802	62.827521
1879.242397	51.528818	62.832526
1878.963050	49.998987	62.837530
1878.500999	57.822261	62.842535
1878.037859	51.125780	62.847540
1877.104671	50.005660	62.852545
1876.182446	54.677262	62.857550
1875.985357	50.439482	62.862554
1875.314351	55.782378	62.867559
1874.687905	50.838509	62.872564
1873.735032	42.879428	62.877569
1872.985899	48.431835	62.882574
1872.269835	45.560025	62.887578
1871.936867	53.142042	62.892583
1871.406069	42.006348	62.897588
1870.161082	49.368888	62.902593
1869.568958	57.766297	62.907598
1869.323124	39.697548	62.912602
1868.649060	55.319040	62.917607
1867.870638	31.894609	62.922612
1867.080613	50.314542	62.927617
1866.624996	40.983483	62.932622
1866.327292	48.023760	62.937626
1865.010911	47.940567	62.942631
1864.379403	40.162276	62.947636
1863.639801	46.274540	62.952641
1863.468324	53.635387	62.957646
1862.951549	51.154545	62.962650
1861.617561	52.917523	62.967655
1861.034672	59.815432	62.972660
1860.620475	58.035786	62.977665
1860.223935	46.298486	62.982670
1859.115917	61.473236	62.987674
1858.036695	64.126132	62.992679
1857.303505	47.512943	62.997684
1856.996327	59.607057	63.002689
1856.662590	49.750467	63.007694
1856.265197	51.139263	63.012698
1855.530558	59.745372	63.017703
1854.631439	50.765404	63.022708
1853.707678	57.362630	63.027713
1853.414204	43.729328	63.032718
1853.153297	50.408968	63.037722
1851.617254	56.829021	63.042727
1851.293363	50.107286	63.047732
1850.511146	49.994488	63.052737
1850.343174	52.067497	63.057742
1849.579986	43.029687	63.062746
1848.375216	55.045535	63.067751
1848.055659	40.525441	63.072756
1847.597989	52.433716	63.077761
1847.343685	52.855245	63.082766
1846.031408	49.929870	63.087770
1845.317245	48.735567	63.092775
1845.216231	48.867843	63.097780
1843.829996	52.931909	63.102785
1843.017128	48.949583	63.107790
1842.560833	46.981092	63.112794
1841.803745	59.238093	63.117799
1841.945515	43.495209	63.122804
1841.169443	50.937850	63.127809
1840.022423	43.966774	63.132814
1839.340862	38.817213	63.137818
1838.692513	52.376793	63.142823
1838.342840	47.453646	63.147828
1837.293788	55.627149	63.152833
1836.826161	54.067292	63.157838
1836.343264	48.906688	63.162842
1835.592950	54.057188	63.167847
1834.985500	44.849584	63.172852
1833.846736	49.074628	63.177857
1833.384925	56.131503	63.182862
1833.244633	54.847670	63.187866
1832.226437	61.097213	63.192871
1831.390145	43.582664	63.197876
1830.728983	56.089350	63.202881
1830.416513	51.414175	63.207886
1830.017963	50.934555	63.212890
1828.779912	55.798234	63.217895
1828.064963	45.978523	63.222900
1827.359340	53.744281	63.227905
1827.040626	52.944494	63.232910
1826.407195	47.095043	63.237914
1825.066713	49.890348	63.242919
1824.821852	42.282483	63.247924
1823.979083	55.789361	63.252929
1823.694126	56.083301	63.257934
1823.589826	41.319312	63.262938
1822.053720	55.158610	63.267943
1821.544488	58.265045	63.272948
1821.177283	47.637953	63.277953
1820.412387	42.049064	63.282958
1819.416042	47.039940	63.287962
1818.331501	57.587558	63.292967
1817.967710	44.908404	63.297972
1817.441725	46.685035	63.302977
1816.898123	52.152786	63.307982
1816.666460	46.952298	63.312986
1816.004444	46.555510	63.317991
1815.273121	44.856185	63.322996
1814.616016	51.950375	63.328001
1813.812548	51.388397	63.333006
1813.059000	39.236311	63.338010
1812.157152	52.208545	63.343015
1812.201728	50.013885	63.348020
1810.909228	50.568717	63.353025
1809.936518	58.395809	63.358030
1809.457472	50.027224	63.363034
1808.910568	56.190906	63.368039
1808.833246	47.197169	63.373044
1807.984343	61.436701	63.378049
1806.965717	43.120099	63.383054
1806.301646	41.553595	63.388058
1805.411874	52.458201	63.393063
1805.378247	41.921648	63.398068
1804.621204	44.458755	63.403073
1803.417257	45.855776	63.408078
1803.389789	46.503055	63.413082
1802.574586	42.680380	63.418087
1802.364651	38.788411	63.423092
1801.083487	46.547786	63.428097
1800.641671	41.497359	63.433102
1799.986987	45.025841	63.438106
1799.072400	41.990042	63.443111
1798.451167	47.687729	63.448116
1797.843240	45.041611	63.453121
1797.014747	50.835284	63.458126
1796.964060	51.850509	63.463130
1795.771138	49.074935	63.468135
1795.080533	49.248792	63.473140
1794.254834	50.210462	63.478145
1793.784359	50.071835	63.483150
1793.531956	46.514600	63.488154
1791.764934	47.674617	63.493159
1791.635638	42.226080	63.498164
1791.180893	44.376161	63.503169
1790.899094	51.795522	63.508174
1790.405261	44.793294	63.513178
1788.895248	46.369800	63.518183
1788.496505	45.737260	63.523188
1788.133002	48.281267	63.528193
1787.582321	44.750894	63.533198
1786.724694	47.532624	63.538202
1785.833698	54.261854	63.543207
1785.469452	46.751794	63.548212
1784.854755	49.474452	63.553217
1783.829362	54.097811	63.558222
1783.332740	54.467940	63.563226
1782.178452	52.381642	63.568231
1782.094063	46.659481	63.573236
1781.507262	53.136992	63.578241
1780.373057	58.561341	63.583246
1779.960403	39.260756	63.588250
1778.795265	49.926829	63.593255
1778.682497	50.532461	63.598260
1778.216895	48.062436	63.603265
1777.389827	50.624861	63.608270
1776.794147	41.992548	63.613274
1775.946472	50.927260	63.618279
1775.587361	45.001152	63.623284
1775.139071	48.637209	63.628289
1774.040766	51.335741	63.633294
1773.443669	45.491575	63.638298
1772.893062	54.989372	63.643303
1772.395457	56.905002	63.648308
1771.459723	48.265184	63.653313
1770.307198	54.220699	63.658318
1770.175446	39.470542	63.663322
1769.557599	48.930130	63.668327
1768.892996	43.464098	63.673332
1767.968438	54.596577	63.678337
1767.384151	48.651034	63.683342
1767.110563	53.022562	63.688346
1766.034348	59.016423	63.693351
1765.174692	37.722689	63.698356
1764.732445	47.789875	63.703361
1763.960746	54.216329	63.708366
1764.077416	43.450920	63.713370
1762.920010	53.784628	63.718375
1762.254775	47.459298	63.723380
1761.415586	49.883311	63.728385
1760.891831	46.112137	63.733390
1760.380853	39.763892	63.738394
1759.266343	52.894479	63.743399
1758.734447	47.175575	63.748404
1758.283730	47.732375	63.753409
1757.568175	50.559360	63.758414
1757.044857	43.661166	63.763418
1755.677914	52.118549	63.768423
1755.473233	52.178985	63.773428
1754.916322	43.985201	63.778433
1754.519308	47.092748	63.783438
1753.874764	43.659287	63.788442
1752.784241	40.408604	63.793447
1752.358572	37.845516	63.798452
1751.645960	38.123798	63.803457
1751.021290	53.693301	63.808462
1750.423918	38.469911	63.813466
1749.423363	53.689115	63.818471
1749.245149	41.628612	63.823476
1748.167775	50.204009	63.828481
1747.314723	48.279618	63.833486
1746.892925	39.255444	63.838490
1745.995664	48.395146	63.843495
1745.846967	40.090814	63.848500
1745.416869	49.862774	63.853505
1744.329395	53.899944	63.858510
1743.755736	49.398718	63.863514
1742.953079	54.431401	63.868519
1742.973622	46.980089	63.873524
1741.620102	53.946774	63.878529
1740.463002	49.801538	63.883534
1740.394846	48.728596	63.888538
1740.045227	51.549511	63.893543
1739.294590	46.150764	63.898548
1738.195267	51.433975	63.903553
1737.699490	50.143524	63.908558
1737.495841	39.979318	63.913562
1736.161113	50.866293	63.918567
1735.220954	44.324446	63.923572
1734.422005	46.295818	63.928577
1733.933355	50.382970	63.933582
1733.822525	54.320242	63.938586
1733.451821	51.207557	63.943591
1733.019545	40.101994	63.948596
1731.921005	53.592735	63.953601
1731.390056	49.079999	63.958606
1731.065531	36.282683	63.963610
1729.609530	48.324268	63.968615
1729.087592	45.084221	63.973620
1728.654332	49.780714	63.978625
1727.975347	57.077082	63.983630
1726.855856	50.798670	63.988634
1725.966372	50.210957	63.993639
1725.608477	44.499122	63.998644
1725.258694	43.273794	64.003649
1724.996306	41.982552	64.008654
1724.085856	43.353498	64.013658
1723.086499	43.368257	64.018663
1722.573214	46.316085	64.023668
1722.013987	36.238313	64.028673
1721.380851	42.461425	64.033678
1720.439084	50.310432	64.038682
1719.557254	49.992729	64.043687
1719.382561	41.974789	64.048692
1718.942885	52.710169	64.053697
1718.075037	41.162873	64.058702
1717.500342	43.984842	64.063706
1716.619535	44.009160	64.068711
1715.875229	37.284841	64.073716
1714.853959	42.629775	64.078721
1714.138242	44.791353	64.083726
1713.858514	36.252382	64.088730
1713.106762	45.181333	64.093735
1713.154975	41.153765	64.098740
1712.170074	47.341286	64.103745
1711.342775	39.034348	64.108750
1711.194505	41.943131	64.113754
1710.237025	45.743635	64.118759
1708.856211	38.002397	64.123764
1708.422554	47.741808	64.128769
1707.794461	48.900769	64.133774
1707.820907	42.438804	64.138778
1707.034409	40.691507	64.143783
1706.244638	39.559712	64.148788
1705.519258	48.352020	64.153793
1704.684877	44.001017	64.158798
1704.119800	35.439561	64.163802
1703.364919	42.352183	64.168807
1702.877624	42.063288	64.173812
1702.420071	48.275866	64.178817
1701.237387	46.107388	64.183822
1700.516412	48.263497	64.188826
1699.954565	48.502081	64.193831
1699.660688	42.185601	64.198836
1698.776587	49.853575	64.203841
1697.703905	48.795097	64.208846
1697.405769	45.831736	64.213850
1696.541618	53.734653	64.218855
1696.586920	47.897289	64.223860
1695.691250	52.623072	64.228865
1694.745255	53.469843	64.233870
1694.271734	45.401598	64.238874
1693.749579	53.871491	64.243879
1692.870722	43.089162	64.248884
1691.702977	42.012670	64.253889
1691.266158	53.515537	64.258894
1690.907789	48.034006	64.263898
1690.265081	44.122477	64.268903
1689.878413	43.007087	64.273908
1688.734675	43.487892	64.278913
1688.154404	43.136498	64.283918
1687.875771	37.366355	64.288922
1686.874015	45.130283	64.293927
1685.874445	40.275693	64.298932
1685.375606	50.113764	64.303937
1684.927141	48.853655	64.308942
1684.653240	42.756345	64.313946
1683.357027	40.142305	64.318951
1683.031728	41.732552	64.323956
1682.556836	41.392807	64.328961
1681.758072	37.944439	64.333966
1680.959516	36.050839	64.338970
1679.921009	43.047935	64.343975
1679.765231	35.640406	64.348980
1679.153828	42.140758	64.353985
1678.289943	40.490912	64.358990
1677.702733	37.053098	64.363994
1676.695459	48.938286	64.368999
1676.342953	42.705235	64.374004
1676.116712	41.442949	64.379009
1674.638330	43.526979	64.384014
1674.065402	37.727890	64.389018
1673.391873	39.013917	64.394023
1673.044871	36.876722	64.399028
1672.804205	40.706884	64.404033
1671.886252	50.229919	64.409038
1671.113683	43.208918	64.414042
1670.503319	43.221836	64.419047
1669.631682	51.534358	64.424052
1668.739754	49.606707	64.429057
1667.934312	46.457432	64.434062
1667.739966	50.925184	64.439066
1667.203579	53.156058	64.444071
1666.876090	43.214950	64.449076
1665.556151	45.120863	64.454081
1664.879115	50.540446	64.459086
1664.504255	40.335641	64.464090
1663.875618	50.066603	64.469095
1663.188989	46.433280	64.474100
1662.265026	45.903102	64.479105
1661.544908	51.409950	64.484110
1660.934151	45.869170	64.489114
1660.474946	49.199484	64.494119
1660.254235	43.943667	64.499124
1659.086166	45.631506	64.504129
1658.348814	49.947395	64.509134
1658.008590	38.838272	64.514138
1657.169577	41.311168	64.519143
1656.258746	38.333172	64.524148
1655.629777	45.517530	64.529153
1655.190141	54.001126	64.534158
1655.122667	40.156951	64.539162
1653.812622	48.975904	64.544167
1652.974748	37.960017	64.549172
1652.828972	44.633987	64.554177
1652.215719	57.216659	64.559182
1651.125324	40.680808	64.564186
1650.074448	48.119829	64.569191
1649.726794	43.951722	64.574196
1649.175791	47.936831	64.579201
1648.898649	41.888926	64.584206
1648.013158	42.205733	64.589210
1646.937635	45.414756	64.594215
1646.648128	40.098910	64.599220
1645.845978	42.711027	64.604225
1645.494783	50.133529	64.609230
1644.488259	45.704239	64.614234
1643.641917	57.540227	64.619239
1643.514231	47.994719	64.624244
1642.778652	53.474067	64.629249
1641.743690	54.281373	64.634254
1641.461174	38.389880	64.639258
1640.563886	49.199524	64.644263
1640.188725	47.002153	64.649268
1639.763392	43.201184	64.654273
1638.610643	52.362572	64.659278
1637.898059	52.224585	64.664282
1637.367655	54.875541	64.669287
1636.888034	40.198013	64.674292
1635.698415	45.024115	64.679297
1634.920351	47.873673	64.684302
1634.632168	46.176550	64.689306
1634.144273	53.363736	64.694311
1633.799122	51.052794	64.699316
1633.026231	49.183515	64.704321
1632.053804	46.628452	64.709326
1631.815744	39.163039	64.714330
1630.333459	46.001995	64.719335
1629.951716	40.158357	64.724340
1629.176564	48.576981	64.729345
1628.674271	50.908097	64.734350
1628.650989	47.743400	64.739354
1627.222231	54.250599	64.744359
1626.402640	43.717495	64.749364
1625.920745	46.203058	64.754369
1625.632252	45.623990	64.759374
1625.488295	40.269259	64.764378
1624.006173	58.758163	64.769383
1623.329209	49.468632	64.774388
1622.660408	55.755777	64.779393
1622.065106	50.649346	64.784398
1621.852013	43.255657	64.789402
1620.339894	59.445511	64.794407
1619.862191	44.434959	64.799412
1619.444926	53.960474	64.804417
1619.260239	53.204076	64.809422
1618.719266	47.139738	64.814426
1617.484512	46.699944	64.819431
1616.797261	36.901150	64.824436
1616.370976	45.825726	64.829441
1614.862350	53.706462	64.834446
1614.453700	42.130423	64.839450
1613.898168	43.872361	64.844455
1613.779718	47.694153	64.849460
1613.427163	46.120792	64.854465
1612.740623	44.587870	64.859470
1612.032826	41.120344	64.864474
1610.980454	43.195083	64.869479
1610.679127	49.070633	64.874484
1609.330349	51.391144	64.879489
1608.872212	51.493430	64.884494
1608.527992	44.759206	64.889498
1607.843440	53.909308	64.894503
1606.655412	44.279944	64.899508
1606.105279	46.579240	64.904513
1605.593810	46.797226	64.909518
1605.434179	45.975351	64.914522
1603.944540	58.788703	64.919527
1603.375190	47.386416	64.924532
1602.611214	45.299699	64.929537
1602.179210	43.089289	64.934542
1602.325821	41.394061	64.939546
1601.191636	55.792474	64.944551
1600.305156	40.058430	64.949556
1600.077417	46.215590	64.954561
1598.852742	53.101948	64.959566
1598.234126	49.330112	64.964570
1597.200108	46.720195	64.969575
1597.133976	48.269282	64.974580
1596.477881	42.321006	64.979585
1596.255478	50.334879	64.984590
1595.414222	46.208924	64.989594
1593.966656	53.168536	64.994599
1593.712365	44.942496	64.999604
1593.198674	45.490404	65.004609
1592.265161	55.159429	65.009614
1591.768038	36.198750	65.014618
1590.543251	47.088812	65.019623
1590.729163	50.387615	65.024628
1590.474712	43.033615	65.029633
1589.180539	50.438770	65.034638
1588.456623	45.502585	65.039642
1587.815785	50.019191	65.044647
1587.416931	39.239504	65.049652
1586.465737	41.615131	65.054657
1585.760531	44.355361	65.059662
1585.337990	44.023086	65.064666
1584.499642	48.626258	65.069671
1583.333070	31.616882	65.074676
1582.577194	45.977269	65.079681
1582.309608	49.236155	65.084686
1582.073453	39.635357	65.089690
1581.534022	46.348209	65.094695
1581.058044	35.136101	65.099700
1580.050847	49.806062	65.104705
1579.156075	44.357732	65.109710
1579.036211	34.225979	65.114714
1577.348159	43.324196	65.119719
1576.881889	39.767852	65.124724
1576.659497	41.603523	65.129729
1575.876109	45.564062	65.134734
1575.641418	40.588009	65.139738
1574.450991	44.939625	65.144743
1573.799027	39.720794	65.149748
1573.211463	44.307781	65.154753
1572.869256	53.278929	65.159758
1572.352808	40.739211	65.164762
1571.062510	46.869641	65.169767
1570.486237	44.298974	65.174772
1570.039028	33.000303	65.179777
1569.486363	35.008285	65.184782
1568.561270	36.501451	65.189786
1567.735242	39.967319	65.194791
1567.611020	40.798694	65.199796
1566.988180	55.428102	65.204801
1565.980703	47.089921	65.209806
1565.550942	37.926719	65.214810
1564.624246	53.679827	65.219815
1564.213465	49.900212	65.224820
1563.181881	53.293090	65.229825
1562.679433	42.559826	65.234830
1562.198161	37.604027	65.239834
1561.485690	40.984051	65.244839
1560.991248	47.300270	65.249844
1559.997978	44.808469	65.254849
1559.213204	46.665681	65.259854
1559.134037	42.544819	65.264858
1558.000240	43.225940	65.269863
1557.089407	43.707645	65.274868
1556.457757	35.760754	65.279873
1556.171705	50.937443	65.284878
1555.854171	41.204505	65.289882
1554.753971	45.633253	65.294887
1554.275477	45.197914	65.299892
1553.498520	35.258863	65.304897
1552.835879	49.467257	65.309902
1552.222591	44.136636	65.314906
1551.349777	51.612053	65.319911
1550.504207	42.019774	65.324916
1550.320764	40.135719	65.329921
1549.630639	44.500896	65.334926
1548.377629	32.305283	65.339930
1548.059298	39.322037	65.344935
1547.539082	43.180850	65.349940
1547.177686	37.258308	65.354945
1546.440355	51.737179	65.359950
1545.739699	40.439353	65.364954
1544.641152	43.724608	65.369959
1544.392446	44.548955	65.374964
1543.759677	38.384113	65.379969
1542.705622	37.576618	65.384974
1542.308084	37.410680	65.389978
1541.801101	39.868704	65.394983
1541.250197	44.341068	65.399988
1540.037021	48.850846	65.404993
1539.545898	52.113713	65.409998
1539.083304	46.281360	65.415002
1538.192401	44.055565	65.420007
1537.307497	43.918176	65.425012
1536.466733	43.926731	65.430017
1535.895757	48.436977	65.435022
1535.961596	41.191365	65.440026
1535.396571	45.375829	65.445031
1534.776636	39.683590	65.450036
1533.736993	48.167908	65.455041
1532.949863	49.472019	65.460046
1532.619542	37.476728	65.465050
1531.241933	43.662044	65.470055
1530.844363	35.526591	65.475060
1530.482213	41.981058	65.480065
1529.859430	40.017004	65.485070
1529.232184	34.270740	65.490074
1528.150870	45.767200	65.495079
1527.594360	44.543209	65.500084
1526.878751	40.532929	65.505089
1526.474939	44.357483	65.510094
1525.558994	40.484684	65.515098
1524.813566	42.581646	65.520103
1524.458055	38.380121	65.525108
1523.877708	47.855858	65.530113
1523.516037	42.442693	65.535118
1522.477071	33.273800	65.540122
1521.730244	44.340244	65.545127
1521.467369	40.015196	65.550132
1520.424457	43.673224	65.555137
1519.436602	48.924611	65.560142
1519.162649	40.296455	65.565146
1518.379615	46.065627	65.570151
1518.008621	43.632660	65.575156
1517.197709	51.322167	65.580161
1516.549640	46.191038	65.585166
1516.211757	46.332577	65.590170
1515.208584	53.743565	65.595175
1514.429514	42.992770	65.600180
1514.250792	45.195226	65.605185
1513.227174	53.203945	65.610190
1512.143792	51.268925	65.615194
1511.027378	49.761756	65.620199
1510.579041	46.048042	65.625204
1510.636702	44.351175	65.630209
1510.042992	50.583831	65.635214
1510.096009	33.588870	65.640218
1508.617457	41.676174	65.645223
1507.970816	35.682275	65.650228
1507.349165	43.321208	65.655233
1506.646106	42.787525	65.660238
1505.859005	46.139999	65.665242
1505.326726	45.558681	65.670247
1504.888002	45.918085	65.675252
1503.893177	40.181347	65.680257
1502.935021	44.037216	65.685262
1502.429591	33.189340	65.690266
1501.716021	46.138022	65.695271
1501.437878	33.984648	65.700276
1501.392003	34.064023	65.705281
1500.141617	49.568964	65.710286
1499.349795	35.934526	65.715290
1498.925088	41.758723	65.720295
1497.715865	42.074983	65.725300
1496.998146	37.771750	65.730305
1496.519009	49.774907	65.735310
1496.107471	40.001729	65.740314
1495.876696	47.285261	65.745319
1494.963177	43.763731	65.750324
1494.124718	36.942494	65.755329
1493.287952	48.035851	65.760334
1492.531840	42.387337	65.765338
1491.434117	45.675636	65.770343
1490.892168	38.737903	65.775348
1490.409793	45.753922	65.780353
1489.779144	43.570365	65.785358
1489.680072	38.653197	65.790362
1489.548368	44.720985	65.795367
1488.428401	47.629639	65.800372
1487.714934	40.679738	65.805377
1486.389295	45.087565	65.810382
1485.876828	43.754089	65.815386
1484.740013	44.941898	65.820391
1484.680857	40.961357	65.825396
1484.437451	49.421668	65.830401
1483.760599	49.673841	65.835406
1483.293649	43.898962	65.840410
1481.971658	46.563767	65.845415
1481.583569	45.368215	65.850420
1480.983639	46.322489	65.855425
1479.599244	45.570664	65.860430
1479.738677	38.428475	65.865434
1478.650409	42.429598	65.870439
1478.474519	40.407162	65.875444
1477.674132	35.596704	65.880449
1476.679539	44.690436	65.885454
1476.210768	44.192069	65.890458
1475.635984	44.916856	65.895463
1475.170369	48.325481	65.900468
1474.058762	39.362107	65.905473
1473.043516	43.813654	65.910478
1473.026863	36.224783	65.915482
1472.371553	41.134772	65.920487
1471.726438	39.284663	65.925492
1471.111652	39.864427	65.930497
1470.674960	37.927586	65.935502
1469.725968	38.784373	65.940506
1468.657005	47.765354	65.945511
1468.244546	38.273016	65.950516
1468.162238	39.610218	65.955521
1466.667177	49.193469	65.960526
1465.984818	45.513798	65.965530
1465.202443	48.253705	65.970535
1464.713409	39.442129	65.975540
1464.442399	39.541511	65.980545
1463.946303	45.156296	65.985550
1463.155476	36.529867	65.990554
1462.138677	44.693623	65.995559
1462.117232	39.406171	66.000564
1461.414966	46.077108	66.005569
1459.981157	49.168103	66.010574
1459.824313	44.372074	66.015578
1459.171076	48.714064	66.020583
1458.562684	40.930656	66.025588
1457.604955	41.506575	66.030593
1456.448571	37.963733	66.035598
1456.240452	39.544844	66.040602
1455.669430	51.438032	66.045607
1455.117074	32.572918	66.050612
1454.288708	38.111199	66.055617
1453.566637	53.764004	66.060622
1453.505937	34.778184	66.065626
1452.829618	53.052364	66.070631
1452.019856	45.305686	66.075636
1451.381529	38.895763	66.080641
1450.583404	45.156180	66.085646
1449.517906	28.643315	66.090650
1448.924041	42.321992	66.095655
1448.337572	39.216840	66.100660
1447.732421	48.918867	66.105665
1447.274299	46.074002	66.110670
1445.939720	40.422818	66.115674
1445.076242	45.291782	66.120679
1444.620712	44.114838	66.125684
1444.541950	40.101148	66.130689
1443.876486	50.054022	66.135694
1443.781121	36.469773	66.140698
1442.981592	46.784555	66.145703
1442.117207	45.614239	66.150708
1441.497852	39.671213	66.155713
1439.977481	38.426958	66.160718
1439.883587	34.399906	66.165722
1439.244457	42.312849	66.170727
1438.828211	37.450820	66.175732
1437.992075	38.783244	66.180737
1436.924169	39.707823	66.185742
1436.653649	34.185581	66.190746
1436.120469	40.329782	66.195751
1435.567677	43.326510	66.200756
1434.466691	33.632957	66.205761
1433.866257	46.199411	66.210766
1433.741706	41.503904	66.215770
1432.391677	39.616026	66.220775
1431.493562	44.388001	66.225780
1431.117890	40.710063	66.230785
1430.531070	41.971332	66.235790
1430.274135	40.687141	66.240794
1429.412663	45.763937	66.245799
1428.362179	40.231611	66.250804
1428.144928	33.388947	66.255809
1427.566873	45.570241	66.260814
1426.948945	36.943156	66.265818
1426.046354	34.288775	66.270823
1425.660706	40.168270	66.275828
1425.270226	33.531323	66.280833
1423.854810	47.756862	66.285838
1423.397105	36.338480	66.290842
1422.849426	44.686302	66.295847
1421.918389	44.250371	66.300852
1421.081279	44.113311	66.305857
1420.391992	46.929894	66.310862
1420.008656	38.790628	66.315866
1419.466290	46.546280	66.320871
1418.833332	39.668760	66.325876
1417.882079	42.624742	66.330881
1417.102762	40.516869	66.335886
1416.844254	35.453167	66.340890
1416.212369	48.666410	66.345895
1415.672543	45.156480	66.350900
1414.501961	38.854811	66.355905
1413.892970	52.114879	66.360910
1413.898199	39.282584	66.365914
1412.864008	52.638610	66.370919
1412.000430	39.988542	66.375924
1411.628986	41.764338	66.380929
1410.918852	48.960059	66.385934
1410.539530	41.597553	66.390938
1408.921363	46.450856	66.395943
1408.737519	42.354525	66.400948
1408.209085	37.127152	66.405953
1407.720486	44.700804	66.410958
1407.166873	35.472178	66.415962
1405.660198	47.520376	66.420967
1405.345693	38.682657	66.425972
1405.033058	33.830976	66.430977
1404.332792	42.863759	66.435982
1403.471292	42.024142	66.440986
1402.730428	43.149058	66.445991
1402.402309	42.551084	66.450996
1401.724886	46.748703	66.456001
1400.415157	46.882295	66.461006
1399.926844	48.482711	66.466010
1399.434604	42.399652	66.471015
1399.133767	49.448328	66.476020
1398.878459	41.446405	66.481025
1397.768095	42.063950	66.486030
1397.157271	38.372932	66.491034
1396.299027	48.165649	66.496039
1395.577953	36.100041	66.501044
1394.872448	35.784386	66.506049
1394.066480	41.399543	66.511054
1393.750229	29.666973	66.516058
1393.057203	42.692821	66.521063
1392.030192	41.062693	66.526068
1391.656767	39.101620	66.531073
1390.633223	48.351359	66.536078
1390.577641	38.395488	66.541082
1389.759548	41.342931	66.546087
1388.853036	38.176703	66.551092
1388.550691	35.146253	66.556097
1387.734419	37.211934	66.561102
1387.338981	30.809162	66.566106
1386.141577	38.856570	66.571111
1385.100791	43.919302	66.576116
1385.062598	39.232151	66.581121
1384.478076	43.501736	66.586126
1384.222353	42.368737	66.591130
1383.397350	35.387719	66.596135
1382.575461	38.570720	66.601140
1381.997487	36.033487	66.606145
1380.837893	44.505376	66.611150
1380.622157	37.960506	66.616154
1379.873917	45.485546	66.621159
1379.118991	42.074466	66.626164
1378.317373	35.036120	66.631169
1377.228612	40.978488	66.636174
1377.216525	34.549478	66.641178
1376.807245	38.009082	66.646183
1375.743698	44.813147	66.651188
1375.022375	39.487136	66.656193
1374.297995	47.473563	66.661198
1373.893232	29.846527	66.666202
1373.617249	42.085462	66.671207
1372.503895	39.481944	66.676212
1372.112449	32.055150	66.681217
1371.030829	39.027658	66.686222
1370.842605	35.446090	66.691226
1369.217889	40.384028	66.696231
1368.512173	37.491806	66.701236
1368.313524	39.793625	66.706241
1367.642569	39.398372	66.711246
1367.725663	32.542672	66.716250
1366.767054	36.636763	66.721255
1365.865595	35.956467	66.726260
1365.454755	31.293859	66.731265
1364.714576	40.982661	66.736270
1364.333989	29.531546	66.741274
1362.988941	37.851575	66.746279
1362.866944	33.100482	66.751284
1362.205055	30.784739	66.756289
1361.049775	34.208384	66.761294
1360.882177	30.382278	66.766298
1360.089323	36.873675	66.771303
1359.461695	34.724365	66.776308
1358.402795	34.688807	66.781313
1357.732526	36.426954	66.786318
1357.301823	40.825051	66.791322
1356.792813	42.408265	66.796327
1355.836834	45.107988	66.801332
1354.990404	33.046555	66.806337
1354.305681	38.737063	66.811342
1354.155565	36.321054	66.816346
1353.753137	33.218213	66.821351
1352.571610	34.376916	66.826356
1351.980098	26.513599	66.831361
1351.077994	44.309604	66.836366
1351.263417	38.557215	66.841370
1350.404366	48.758481	66.846375
1349.173022	37.444168	66.851380
1348.874213	31.666254	66.856385
1348.091694	46.768882	66.861390
1347.294611	33.132198	66.866394
1346.467783	41.642664	66.871399
1345.632970	43.668730	66.876404
1345.357611	41.411393	66.881409
1345.132565	43.479302	66.886414
1344.216947	35.960797	66.891418
1343.197602	41.233012	66.896423
1342.709971	36.527423	66.901428
1342.290191	43.654925	66.906433
1341.226586	50.946267	66.911438
1340.452497	41.566633	66.916442
1339.952873	50.089746	66.921447
1339.504581	40.943740	66.926452
1339.164062	39.529350	66.931457
1338.277913	41.948334	66.936462
1337.461887	30.454483	66.941466
1336.744159	39.810155	66.946471
1336.350678	33.761878	66.951476
1336.043348	44.654419	66.956481
1335.175675	40.797675	66.961486
1334.816924	37.900772	66.966490
1333.456605	40.666351	66.971495
1332.511417	39.032703	66.976500
1332.146648	38.448449	66.981505
1331.596441	41.247675	66.986510
1331.232198	35.533778	66.991514
1330.104005	42.915806	66.996519
1329.161386	33.088333	67.001524
1328.626444	38.799189	67.006529
1328.108509	42.911550	67.011534
1327.926814	36.339201	67.016538
1326.818807	32.385055	67.021543
1326.014321	35.108012	67.026548
1325.870659	31.014768	67.031553
1325.183408	36.413961	67.036558
1324.321070	34.489618	67.041562
1323.408199	45.322306	67.046567
1322.894045	35.679024	67.051572
1322.333401	32.664414	67.056577
1321.722775	35.990459	67.061582
1320.803147	26.108879	67.066586
1320.137865	29.238618	67.071591
1319.594435	32.374218	67.076596
1319.512640	28.105569	67.081601
1318.290628	31.568222	67.086606
1317.519822	31.040630	67.091610
1316.871455	28.390031	67.096615
1316.614861	31.861638	67.101620
1315.877975	25.180442	67.106625
1315.063764	29.103367	67.111630
1314.324870	29.813277	67.116634
1314.008061	29.740192	67.121639
1312.900407	30.994396	67.126644
1312.437683	31.458566	67.131649
1311.771612	26.551130	67.136654
1311.542287	25.890158	67.141658
1310.254499	33.095720	67.146663
1309.330434	36.867387	67.151668
1309.080825	29.157879	67.156673
1308.376513	36.371610	67.161678
1308.594017	25.290615	67.166682
1307.066313	28.685178	67.171687
1306.186555	26.686345	67.176692
1305.903562	26.202630	67.181697
1305.197813	38.096738	67.186702
1303.942272	36.178141	67.191706
1303.400146	41.150592	67.196711
1302.941639	32.796236	67.201716
1302.787494	28.515437	67.206721
1302.180755	41.570154	67.211726
1301.710598	24.853937	67.216730
1300.761630	32.992761	67.221735
1299.976856	27.139155	67.226740
1298.975714	23.284724	67.231745
1298.139831	34.797417	67.236750
1297.738611	27.632380	67.241754
1297.388003	34.225365	67.246759
1296.614025	28.149281	67.251764
1295.820036	21.426712	67.256769
1294.811065	36.294114	67.261774
1294.709849	28.023306	67.266778
1294.192777	33.494794	67.271783
1293.325699	39.663711	67.276788
1292.424731	32.149210	67.281793
1291.642422	44.310949	67.286798
1291.478533	25.081399	67.291802
1290.822852	33.697122	67.296807
1289.881946	43.359506	67.301812
1289.308825	32.815756	67.306817
1288.536052	34.272187	67.311822
1288.016474	25.612175	67.316826
1286.927834	34.298304	67.321831
1286.186819	28.538665	67.326836
1286.462116	30.184854	67.331841
1285.686043	38.523268	67.336846
1284.899629	27.232882	67.341850
1283.765888	23.768525	67.346855
1283.353251	33.346922	67.351860
1282.979543	27.919955	67.356865
1281.422799	31.765403	67.361870
1281.028266	29.407181	67.366874
1280.666378	34.571740	67.371879
1279.852620	34.405784	67.376884
1279.681443	28.717974	67.381889
1278.792489	40.297456	67.386894
1278.003537	35.387486	67.391898
1277.370880	39.562245	67.396903
1276.697228	34.629215	67.401908
1276.298955	26.810892	67.406913
1274.969897	36.344181	67.411918
1274.374942	37.299286	67.416922
1273.798284	34.069625	67.421927
1273.595638	37.054868	67.426932
1273.356795	26.137881	67.431937
1272.182482	30.406634	67.436942
1271.422966	28.644150	67.441946
1270.831132	32.325166	67.446951
1270.304603	32.439960	67.451956
1269.359870	20.860959	67.456961
1268.758934	30.294258	67.461966
1268.657457	34.215845	67.466970
1267.654489	32.235036	67.471975
1266.451100	32.944692	67.476980
1266.335729	28.812265	67.481985
1265.435533	34.637965	67.486990
1264.782257	35.458849	67.491994
1263.597229	30.682814	67.496999
1262.982321	25.404580	67.502004
1262.653803	24.667925	67.507009
1262.139447	31.777350	67.512014
1261.953068	26.243340	67.517018
1261.498431	30.812397	67.522023
1260.244728	32.283798	67.527028
1260.067079	30.865603	67.532033
1258.651190	35.953320	67.537038
1257.544325	31.729380	67.542042
1256.929592	31.799857	67.547047
1256.371798	29.823967	67.552052
1256.433875	33.658053	67.557057
1255.918978	32.951029	67.562062
1255.447785	34.149799	67.567066
1254.405161	39.760040	67.572071
1253.663480	40.227572	67.577076
1253.543299	24.821301	67.582081
1252.341618	34.895712	67.587086
1251.906427	28.625441	67.592090
1250.986173	31.545010	67.597095
1250.236887	28.082620	67.602100
1249.097912	26.787304	67.607105
1248.337740	33.021230	67.612110
1248.285287	27.705612	67.617114
1247.847618	33.878804	67.622119
1247.221810	33.457483	67.627124
1246.735105	26.621424	67.632129
1245.674886	31.125924	67.637134
1245.159599	21.782461	67.642138
1244.537838	36.301322	67.647143
1243.758020	33.329462	67.652148
1243.373202	33.133164	67.657153
1242.723824	36.873795	67.662158
1241.818940	34.555721	67.667162
1240.830177	26.824981	67.672167
1239.991872	29.529686	67.677172
1240.101113	30.621982	67.682177
1238.933127	36.256889	67.687182
1238.127095	38.377754	67.692186
1237.440389	31.841561	67.697191
1237.107234	33.888818	67.702196
1237.085696	28.795355	67.707201
1235.534032	30.058688	67.712206
1235.034235	30.738489	67.717210
1234.320259	27.155378	67.722215
1234.053758	26.670626	67.727220
1233.514322	30.455275	67.732225
1231.855755	38.344263	67.737230
1231.714443	28.980761	67.742234
1231.272417	34.404058	67.747239
1230.952038	37.548362	67.752244
1230.308494	34.395576	67.757249
1228.918641	41.978506	67.762254
1228.776016	33.370531	67.767258
1227.912208	36.440398	67.772263
1226.761104	30.892630	67.777268
1226.276085	35.233148	67.782273
1225.280073	31.226552	67.787278
1225.462953	30.930533	67.792282
1225.073819	34.254494	67.797287
1223.562785	26.786565	67.802292
1223.246211	19.858813	67.807297
1222.448099	30.548695	67.812302
1221.911408	28.383388	67.817306
1221.347564	30.836313	67.822311
1220.544403	28.142548	67.827316
1220.252015	27.915789	67.832321
1219.503424	34.795974	67.837326
1218.578478	21.624367	67.842330
1217.756287	29.216381	67.847335
1217.237324	36.744416	67.852340
1216.889637	24.356185	67.857345
1215.725988	41.052140	67.862350
1214.824736	32.878586	67.867354
1214.509114	25.775649	67.872359
1214.247195	28.931158	67.877364
1213.914849	26.741246	67.882369
1212.304143	38.613686	67.887374
1211.768691	23.487909	67.892378
1211.161771	28.743470	67.897383
1211.029697	33.893570	67.902388
1210.563687	31.802177	67.907393
1209.251896	30.982188	67.912398
1208.708360	28.124151	67.917402
1208.443925	27.060363	67.922407
1207.182298	35.693605	67.927412
1206.642656	33.757415	67.932417
1205.860558	37.659498	67.937422
1205.593731	27.846051	67.942426
1204.591737	33.749452	67.947431
1203.856838	36.106584	67.952436
1203.281583	28.721673	67.957441
1202.484461	30.655060	67.962446
1202.801361	21.627117	67.967450
1202.082967	31.181598	67.972455
1201.029358	19.996814	67.977460
1200.425428	25.125751	67.982465
1199.082761	30.998170	67.987470
1198.574617	34.002031	67.992474
1198.113353	26.020287	67.997479
1197.766174	32.125481	68.002484
1196.899343	36.972968	68.007489
1196.125650	36.890549	68.012494
1195.325903	29.864594	68.017498
1194.953248	41.773561	68.022503
1194.036315	38.377265	68.027508
1193.043044	32.425969	68.032513
1192.175646	36.321119	68.037518
1191.913803	25.187046	68.042522
1191.594476	35.539046	68.047527
1191.123121	29.884786	68.052532
1190.901536	29.558468	68.057537
1189.550417	30.427260	68.062542
1189.117955	33.941032	68.067546
1188.310794	36.353810	68.072551
1187.291336	38.576432	68.077556
1186.950324	31.663606	68.082561
1185.925846	29.747749	68.087566
1186.166300	28.792904	68.092570
1184.954430	35.379353	68.097575
1184.044001	37.084773	68.102580
1183.461743	24.342788	68.107585
1183.110383	33.744299	68.112590
1182.718532	25.270577	68.117594
1181.305587	32.048264	68.122599
1181.026489	26.046486	68.127604
1180.638939	25.301884	68.132609
1179.426742	39.266549	68.137614
1179.067502	33.387893	68.142618
1178.171549	36.117553	68.147623
1177.908653	32.191509	68.152628
1177.155662	25.659572	68.157633
1176.010689	23.223593	68.162638
1175.578158	25.050128	68.167642
1174.947484	36.208533	68.172647
1174.422785	30.389305	68.177652
1173.637057	28.307762	68.182657
1172.426798	32.620118	68.187662
1172.284340	33.752435	68.192666
1171.983619	36.403213	68.197671
1171.367715	25.208759	68.202676
1170.490637	26.645541	68.207681
1169.527838	37.908799	68.212686
1169.116273	25.945454	68.217690
1168.568818	21.839173	68.222695
1167.413704	29.925662	68.227700
1167.263587	22.865800	68.232705
1166.661087	27.907788	68.237710
1166.135720	26.242137	68.242714
1165.177317	30.271607	68.247719
1164.251666	33.576819	68.252724
1163.734321	27.816346	68.257729
1163.168185	34.098280	68.262734
1162.638381	31.130842	68.267738
1161.417820	33.252996	68.272743
1160.996216	28.492801	68.277748
1160.612988	26.235299	68.282753
1159.915213	29.630423	68.287758
1159.118861	28.299586	68.292762
1158.169780	27.562286	68.297767
1157.814218	34.141876	68.302772
1157.701523	35.375111	68.307777
1156.307883	35.566323	68.312782
1155.773097	28.430443	68.317786
1155.068399	31.831401	68.322791
1154.693932	26.226396	68.327796
1154.505370	24.220198	68.332801
1153.166654	34.682269	68.337806
1153.047990	27.019772	68.342810
1152.164504	29.678074	68.347815
1150.838598	32.523421	68.352820
1150.445191	26.549288	68.357825
1149.798220	37.820670	68.362830
1149.519493	37.541287	68.367834
1148.193294	34.061869	68.372839
1147.541316	38.703325	68.377844
1147.387774	26.965443	68.382849
1146.735994	41.213139	68.387854
1146.433610	35.948310	68.392858
1145.544050	30.549792	68.397863
1144.397642	31.305633	68.402868
1144.124359	32.695286	68.407873
1143.506661	36.165986	68.412878
1142.876689	30.391891	68.417882
1142.355054	37.440994	68.422887
1141.301206	34.739815	68.427892
1140.484621	27.722868	68.432897
1139.536454	43.118354	68.437902
1139.002799	33.129744	68.442906
1138.939346	37.737528	68.447911
1137.996340	36.048418	68.452916
1137.183367	35.962802	68.457921
1136.737462	31.630653	68.462926
1136.304586	23.026281	68.467930
1135.884913	34.018677	68.472935
1134.699021	33.467271	68.477940
1134.318801	24.906562	68.482945
1133.677545	33.201488	68.487950
1132.781801	23.685187	68.492954
1132.042138	33.219411	68.497959
1131.092869	29.954434	68.502964
1131.150329	32.647594	68.507969
1129.666103	35.002495	68.512974
1129.256059	28.341921	68.517978
1128.581835	31.558276	68.522983
1127.738194	31.004480	68.527988
1127.951570	28.849211	68.532993
1126.670540	37.056663	68.537998
1125.893062	32.788286	68.543002
1125.198455	32.265980	68.548007
1124.731711	25.538737	68.553012
1124.481545	28.463736	68.558017
1124.005572	30.773402	68.563022
1123.000106	32.312615	68.568026
1122.492247	30.975331	68.573031
1121.487320	34.807223	68.578036
1120.821149	31.448344	68.583041
1119.801592	35.194259	68.588046
1119.305880	38.360151	68.593050
1119.012174	28.699222	68.598055
1118.174675	34.393573	68.603060
1117.403776	34.457382	68.608065
1116.366850	30.533030	68.613070
1116.329679	38.020722	68.618074
1115.823025	24.995516	68.623079
1115.159154	23.760312	68.628084
1114.579925	26.054863	68.633089
1113.350541	35.383142	68.638094
1113.092330	26.400931	68.643098
1112.326775	27.690693	68.648103
1111.333737	32.179827	68.653108
1111.174223	22.130152	68.658113
1110.572768	34.617945	68.663118
1109.821017	24.910028	68.668122
1108.918822	22.312473	68.673127
1108.608186	34.626287	68.678132
1107.884845	25.811088	68.683137
1106.911444	30.289216	68.688142
1106.092586	29.499687	68.693146
1105.891546	39.695690	68.698151
1104.957751	32.435636	68.703156
1104.151362	24.526154	68.708161
1103.264177	29.551934	68.713166
1102.775408	26.617407	68.718170
1102.590050	28.524484	68.723175
1101.758059	37.775373	68.728180
1101.003958	20.568261	68.733185
1100.361092	31.534656	68.738190
1100.084148	26.849233	68.743194
1099.282858	32.906816	68.748199
1097.875151	26.854332	68.753204
1097.598356	23.807250	68.758209
1096.940877	32.814351	68.763214
1096.645670	32.923927	68.768218
1096.368136	27.905879	68.773223
1095.044967	32.365528	68.778228
1094.485346	26.725333	68.783233
1093.722617	28.219643	68.788238
1092.843424	29.898047	68.793242
1092.334248	27.012497	68.798247
1091.591137	32.819568	68.803252
1091.607330	23.787412	68.808257
1090.451730	21.214400	68.813262
1089.778518	23.803009	68.818266
1088.858399	20.728946	68.823271
1088.653290	33.415460	68.828276
1088.008027	27.687968	68.833281
1086.942057	37.799199	68.838286
1086.409501	31.405687	68.843290
1085.987790	23.446068	68.848295
1085.363468	35.489671	68.853300
1084.747434	28.175934	68.858305
1083.612953	28.945673	68.863310
1083.071573	26.662879	68.868314
1082.890121	34.443159	68.873319
1081.762476	36.011282	68.878324
1080.713978	22.195536	68.883329
1080.166344	35.592507	68.888334
1079.890046	31.845218	68.893338
1079.252361	27.687081	68.898343
1078.949617	33.707949	68.903348
1078.115810	21.187355	68.908353
1077.326039	32.867787	68.913358
1076.731325	35.361918	68.918362
1076.148677	32.565323	68.923367
1075.301796	34.932415	68.928372
1075.022412	34.638953	68.933377
1073.936916	34.905770	68.938382
1072.767668	29.118130	68.943386
1072.350815	37.979738	68.948391
1071.554400	35.657090	68.953396
1071.267363	22.852423	68.958401
1070.905540	31.213292	68.963406
1070.408513	33.543661	68.968410
1069.643641	28.592095	68.973415
1069.050518	26.869437	68.978420
1068.203007	25.928368	68.983425
1066.751421	29.949588	68.988430
1066.591249	19.122634	68.993434
1065.789479	28.674630	68.998439
1065.468812	40.250495	69.003444
1065.293106	20.805286	69.008449
1064.052912	37.281653	69.013454
1063.518073	26.443329	69.018458
1063.396024	25.265452	69.023463
1062.097858	24.478064	69.028468
1061.191675	29.016473	69.033473
1060.522602	32.969997	69.038478
1060.078536	26.228124	69.043482
1059.003473	20.143255	69.048487
1058.149041	37.821333	69.053492
1057.919106	26.967626	69.058497
1057.735803	35.744779	69.063502
1057.190815	31.663361	69.068506
1056.118788	30.288103	69.073511
1055.397452	39.880928	69.078516
1054.801772	26.666487	69.083521
1054.263134	30.296506	69.088526
1053.877307	33.662535	69.093530
1052.855825	31.799871	69.098535
1051.997075	31.962824	69.103540
1051.781761	27.417408	69.108545
1050.668924	35.378952	69.113550
1049.972651	26.827537	69.118554
1049.807900	22.349768	69.123559
1048.932092	28.600555	69.128564
1048.247381	27.277226	69.133569
1047.242499	31.861300	69.138574
1046.775068	35.234004	69.143578
1046.245884	27.677819	69.148583
1045.618182	33.364047	69.153588
1045.247358	23.929859	69.158593
1044.072404	33.959093	69.163598
1043.398986	21.745721	69.168602
1043.257141	29.565426	69.173607
1042.406610	28.495544	69.178612
1041.631566	20.024470	69.183617
1040.923135	34.292219	69.188622
1040.611453	17.500440	69.193626
1039.631226	22.528421	69.198631
1038.428150	31.341637	69.203636
1038.025603	23.629702	69.208641
1037.830117	32.973308	69.213646
1037.033726	32.154998	69.218650
1035.900802	22.506168	69.223655
1035.169443	28.896398	69.228660
1035.295613	20.777105	69.233665
1034.874768	32.148137	69.238670
1034.112488	26.660037	69.243674
1033.150278	29.810266	69.248679
1032.312070	26.237520	69.253684
1031.653481	29.356797	69.258689
1030.829584	27.609361	69.263694
1030.119254	29.998897	69.268698
1029.867203	29.854048	69.273703
1029.215228	32.243763	69.278708
1028.172952	26.306647	69.283713
1027.303435	29.415326	69.288718
1027.100997	19.020856	69.293722
1026.670469	14.188002	69.298727
1025.934207	24.989496	69.303732
1025.208861	19.877128	69.308737
1024.501432	35.224872	69.313742
1023.949084	23.949403	69.318746
1023.203465	28.549009	69.323751
1022.078146	34.134638	69.328756
1021.755921	25.966830	69.333761
1020.942246	26.748638	69.338766
1020.621405	30.086987	69.343770
1019.553619	34.465048	69.348775
1018.776041	26.320794	69.353780
1018.638750	22.950350	69.358785
1018.155483	29.446189	69.363790
1017.862729	21.767254	69.368794
1016.483392	30.871853	69.373799
1015.877448	41.505983	69.378804
1015.479164	27.435454	69.383809
1014.195215	36.084938	69.388814
1013.723473	35.032073	69.393818
1013.116226	27.258095	69.398823
1012.610005	38.270574	69.403828
1012.030056	30.561633	69.408833
1010.950101	38.024404	69.413838
1010.434181	31.599884	69.418842
1009.994591	24.504094	69.423847
1009.228821	35.023304	69.428852
1008.390005	33.831728	69.433857
1007.744427	35.337387	69.438862
1007.202622	34.770306	69.443866
1006.997495	33.441653	69.448871
1006.149545	36.837053	69.453876
1005.347898	34.370188	69.458881
1004.330857	36.217200	69.463886
1004.149709	20.815956	69.468890
1002.690354	29.597418	69.473895
1002.181330	30.698176	69.478900
1002.090923	25.546302	69.483905
1001.612125	31.538413	69.488910
1001.195471	27.439749	69.493914
1000.154384	28.680340	69.498919
998.917923	36.059208	69.503924
998.809742	23.845812	69.508929
998.256971	36.239145	69.513934
997.201226	26.962810	69.518938
996.651026	28.052774	69.523943
996.242824	33.423410	69.528948
995.733660	25.499800	69.533953
994.371762	25.824814	69.538958
993.767108	30.941289	69.543962
993.428485	27.323771	69.548967
992.699595	28.459509	69.553972
992.426773	18.476766	69.558977
991.383238	27.852786	69.563982
990.763389	30.671036	69.568986
989.977318	30.082898	69.573991
988.974529	32.140524	69.578996
988.449923	23.550785	69.584001
987.666520	27.591893	69.589006
987.614687	31.995985	69.594010
987.342562	29.008095	69.599015
986.301186	35.789837	69.604020
985.502151	27.688431	69.609025
984.665600	36.880150	69.614030
984.413974	33.743927	69.619034
983.304775	35.782217	69.624039
982.073002	36.906504	69.629044
982.293136	20.457462	69.634049
981.444675	39.072834	69.639054
981.336675	24.134591	69.644058
980.285255	31.988622	69.649063
979.272546	32.497773	69.654068
978.601087	23.365305	69.659073
977.873743	32.165933	69.664078
978.080014	32.386541	69.669082
976.990592	29.875589	69.674087
976.132843	28.004255	69.679092
976.051776	27.885822	69.684097
975.009834	31.327860	69.689102
974.026182	24.950960	69.694106
973.865546	21.175827	69.699111
973.028080	23.826863	69.704116
972.312195	20.873309	69.709121
971.301978	25.111347	69.714126
970.989356	27.912259	69.719130
970.528688	25.137285	69.724135
969.331506	24.699711	69.729140
968.852599	23.613305	69.734145
968.027093	34.145179	69.739150
967.602557	24.222843	69.744154
967.396657	27.244883	69.749159
965.990701	37.280939	69.754164
965.751572	23.913619	69.759169
965.284882	27.199487	69.764174
964.175111	26.631320	69.769178
963.078917	24.044187	69.774183
962.581671	24.206422	69.779188
962.495556	20.624426	69.784193
961.785604	31.010189	69.789198
961.199348	17.735948	69.794202
960.541714	27.957276	69.799207
959.505417	39.091940	69.804212
959.425620	27.794921	69.809217
958.625559	36.935112	69.814222
957.768709	30.169056	69.819226
957.355977	31.453187	69.824231
956.453099	33.264707	69.829236
955.455067	26.633074	69.834241
954.859451	34.998034	69.839246
954.104308	34.821279	69.844250
953.828286	21.155499	69.849255
953.453943	32.262107	69.854260
952.480117	26.679969	69.859265
951.582347	33.776322	69.864270
951.125916	24.680611	69.869274
950.861373	34.412073	69.874279
949.504953	21.552089	69.879284
948.953321	25.102195	69.884289
948.196372	24.622972	69.889294
947.947996	27.167674	69.894298
947.348382	21.866602	69.899303
946.344304	33.147518	69.904308
946.317830	25.099818	69.909313
945.434350	27.288279	69.914318
944.480514	21.162102	69.919322
943.748832	24.450713	69.924327
942.968998	28.414000	69.929332
942.499849	31.217744	69.934337
942.062876	30.995100	69.939342
940.981149	23.438557	69.944346
940.351120	28.432930	69.949351
939.968773	23.300707	69.954356
939.652968	22.382310	69.959361
937.998695	29.118089	69.964366
937.584643	25.697075	69.969370
937.054249	26.796514	69.974375
936.599459	18.995154	69.979380
936.194070	22.842096	69.984385
935.033911	23.603370	69.989390
934.282740	33.639327	69.994394
934.182335	23.316941	69.999399
933.563088	35.498518	70.004404
933.049516	22.253717	70.009409
931.920388	29.787409	70.014414
931.188833	39.164274	70.019418
930.995213	27.984712	70.024423
929.547158	33.180205	70.029428
928.887744	28.410593	70.034433
928.471753	39.088620	70.039438
928.368045	33.778027	70.044442
927.729845	28.998732	70.049447
926.745730	33.106485	70.054452
926.111635	20.885327	70.059457
925.581555	32.696343	70.064462
924.571585	30.286307	70.069466
923.643522	28.575981	70.074471
922.939072	25.366748	70.079476
922.773136	30.331432	70.084481
922.252734	33.674738	70.089486
921.846970	27.652161	70.094490
920.743805	21.934509	70.099495
919.862020	27.981289	70.104500
919.640793	27.770049	70.109505
918.690256	32.980996	70.114510
917.755517	30.325617	70.119514
917.486711	29.314594	70.124519
916.846463	28.952420	70.129524
916.250804	24.044944	70.134529
915.108370	38.358116	70.139534
914.916916	27.640234	70.144538
914.532556	31.225229	70.149543
913.347966	31.600915	70.154548
912.516234	26.125487	70.159553
911.919257	24.479172	70.164558
911.583560	24.765513	70.169562
911.414506	24.590124	70.174567
910.417301	40.061260	70.179572
909.633578	23.642652	70.184577
909.018166	36.356600	70.189582
907.966644	31.614696	70.194586
907.479846	28.602632	70.199591
906.805383	35.677658	70.204596
906.550287	25.045595	70.209601
905.365101	33.840246	70.214606
904.585246	30.136843	70.219610
904.054531	23.268458	70.224615
903.603493	31.569420	70.229620
903.027335	25.614960	70.234625
901.806627	25.275773	70.239630
901.095851	26.881712	70.244634
900.880006	19.796079	70.249639
900.272734	31.354466	70.254644
900.131617	25.931567	70.259649
898.911869	29.118091	70.264654
898.413177	30.587787	70.269658
897.975508	21.131160	70.274663
897.063528	37.326705	70.279668
896.108220	22.827644	70.284673
895.353911	37.320320	70.289678
895.207656	29.807318	70.294682
894.806610	31.583156	70.299687
893.203976	43.044490	70.304692
892.985277	30.419787	70.309697
892.127286	36.508521	70.314702
891.752160	34.845830	70.319706
890.684433	30.153818	70.324711
889.770575	30.740309	70.329716
889.583982	27.533830	70.334721
889.089308	31.614172	70.339726
888.965954	27.705387	70.344730
887.965511	33.506148	70.349735
886.859343	37.694836	70.354740
886.642238	21.435220	70.359745
886.187458	29.315756	70.364750
885.028393	27.211721	70.369754
884.380109	33.079438	70.374759
883.795767	32.236895	70.379764
883.273231	30.392671	70.384769
882.189312	21.926659	70.389774
881.398368	25.342981	70.394778
881.109675	26.162709	70.399783
880.606658	34.284300	70.404788
880.308542	25.915578	70.409793
879.311904	29.752542	70.414798
878.533366	27.983748	70.419802
877.743808	23.157598	70.424807
876.847597	34.191147	70.429812
876.490211	26.710169	70.434817
875.926672	33.923657	70.439822
875.311027	36.102635	70.444826
874.588474	31.059251	70.449831
873.410088	38.616576	70.454836
873.543893	35.379610	70.459841
872.607857	36.395389	70.464846
871.487600	36.183726	70.469850
870.819983	31.918455	70.474855
869.997985	49.140428	70.479860
869.998460	40.426157	70.484865
869.417782	42.771450	70.489870
868.494095	37.469931	70.494874
867.887180	24.001900	70.499879
866.805719	34.227617	70.504884
867.012178	29.581991	70.509889
866.224255	29.790502	70.514894
865.370787	30.514040	70.519898
864.903220	31.940944	70.524903
864.106388	37.020223	70.529908
863.352589	28.774479	70.534913
862.571014	32.980902	70.539918
861.942893	30.689887	70.544922
861.280090	30.317126	70.549927
859.847481	30.516276	70.554932
859.624880	35.002731	70.559937
858.832808	39.090985	70.564942
858.653206	30.296575	70.569946
858.379448	28.319731	70.574951
857.517973	37.545406	70.579956
856.772715	31.234691	70.584961
856.414456	37.505666	70.589966
855.575602	29.765442	70.594970
854.575897	27.408993	70.599975
853.492824	35.296487	70.604980
853.242889	28.112210	70.609985
852.586683	33.861353	70.614990
852.198310	33.911671	70.619994
851.802643	37.605701	70.624999
850.675403	32.180477	70.630004
850.382551	27.051373	70.635009
848.944077	35.075849	70.640014
848.125360	32.706367	70.645018
847.600776	31.701367	70.650023
847.268693	36.627844	70.655028
847.243326	33.728429	70.660033
846.777341	45.199697	70.665038
845.722734	40.921906	70.670042
844.758738	32.726965	70.675047
844.114711	36.137264	70.680052
843.403844	29.693356	70.685057
842.541516	36.648490	70.690062
841.447122	24.790759	70.695066
841.585488	30.648401	70.700071
841.043708	33.511026	70.705076
840.672801	34.312306	70.710081
839.693597	33.163629	70.715086
838.880960	32.778451	70.720090
838.245139	22.561791	70.725095
837.125166	33.460658	70.730100
836.874419	30.023135	70.735105
836.451480	22.010161	70.740110
835.457520	23.509807	70.745114
834.576107	23.651210	70.750119
833.869560	31.726352	70.755124
833.321329	28.358250	70.760129
832.877258	32.626078	70.765134
832.622461	26.691452	70.770138
831.630548	20.192939	70.775143
830.694967	29.597557	70.780148
830.199584	17.787999	70.785153
829.730335	23.179401	70.790158
829.113540	21.241388	70.795162
828.366010	34.660727	70.800167
827.419814	35.488916	70.805172
827.130607	22.443397	70.810177
826.343544	30.340554	70.815182
825.124876	26.718056	70.820186
825.255062	33.830604	70.825191
824.726113	37.104328	70.830196
823.827553	22.588389	70.835201
822.929099	28.910647	70.840206
822.217263	22.867426	70.845210
821.829533	19.604664	70.850215
820.442898	33.496282	70.855220
819.909705	25.942379	70.860225
819.467402	35.005160	70.865230
819.123076	33.892633	70.870234
818.789844	30.788343	70.875239
817.347955	40.789187	70.880244
817.017030	25.553739	70.885249
816.484300	28.430695	70.890254
816.202974	29.406944	70.895258
815.319618	24.039113	70.900263
814.158948	26.516146	70.905268
813.845348	20.844760	70.910273
813.155116	31.522282	70.915278
812.278111	26.438852	70.920282
811.638112	27.681910	70.925287
810.975653	30.861773	70.930292
810.807552	19.553608	70.935297
809.594355	26.370637	70.940302
808.708725	24.513261	70.945306
808.390019	21.658960	70.950311
807.724773	30.320433	70.955316
807.640925	28.390635	70.960321
806.614009	31.997492	70.965326
805.632516	33.454167	70.970330
805.074505	20.386787	70.975335
804.384792	31.578284	70.980340
803.737816	23.697164	70.985345
802.901306	31.416128	70.990350
802.057947	26.067166	70.995354
801.968559	20.191372	71.000359
801.649069	30.893460	71.005364
800.779894	25.168584	71.010369
799.832472	35.552752	71.015374
799.538561	30.959957	71.020378
798.432673	33.341551	71.025383
797.280071	31.219184	71.030388
797.291781	25.234262	71.035393
796.979015	29.467002	71.040398
796.078002	30.059366	71.045402
795.090080	33.965933	71.050407
794.384671	35.687733	71.055412
794.220909	24.008315	71.060417
793.204053	38.446606	71.065422
792.064697	37.306093	71.070426
791.861393	17.654060	71.075431
791.310254	33.760650	71.080436
791.020064	26.026160	71.085441
790.283677	30.282175	71.090446
789.095060	30.989700	71.095450
788.875947	31.596526	71.100455
788.105962	31.231382	71.105460
787.200924	26.901433	71.110465
786.786269	34.963240	71.115470
786.063682	31.920929	71.120474
785.545964	27.046812	71.125479
784.238842	25.933006	71.130484
783.880902	23.367212	71.135489
783.167654	32.116749	71.140494
783.085208	30.554138	71.145498
782.067236	27.060557	71.150503
780.780867	36.517874	71.155508
780.594765	26.623865	71.160513
779.847950	23.312617	71.165518
779.589236	35.808962	71.170522
779.022737	27.126609	71.175527
777.947780	33.499052	71.180532
777.374130	24.554504	71.185537
776.873696	25.631860	71.190542
775.962379	25.994073	71.195546
775.375554	25.916728	71.200551
774.474735	30.134269	71.205556
774.431926	22.825581	71.210561
774.007696	30.642921	71.215566
772.909550	31.482701	71.220570
772.255719	23.109127	71.225575
771.338045	26.979288	71.230580
770.210682	17.816973	71.235585
769.329397	27.045816	71.240590
768.936024	16.517797	71.245594
768.881469	22.073418	71.250599
768.275150	26.896903	71.255604
768.228583	15.413295	71.260609
767.313407	25.410731	71.265614
766.083346	26.279396	71.270618
766.080929	28.119525	71.275623
764.834473	31.632040	71.280628
764.070834	21.858352	71.285633
763.885431	31.919392	71.290638
763.040858	28.776664	71.295642
762.095205	29.472334	71.300647
761.243795	33.003965	71.305652
760.878775	32.618520	71.310657
760.452063	39.322998	71.315662
759.248442	32.309464	71.320666
758.726464	24.173511	71.325671
758.049885	26.925151	71.330676
757.279359	25.175621	71.335681
756.994885	31.105292	71.340686
756.206456	26.875058	71.345690
755.503114	30.706377	71.350695
754.607337	29.951284	71.355700
754.460984	14.181891	71.360705
754.192069	23.694857	71.365710
753.286331	30.641154	71.370714
752.686287	29.763297	71.375719
751.313651	24.739866	71.380724
750.620862	32.365006	71.385729
750.262962	28.637064	71.390734
749.749630	29.666020	71.395738
749.527437	23.928058	71.400743
748.166368	27.340560	71.405748
747.399129	33.036439	71.410753
746.850788	39.001810	71.415758
746.750823	34.400226	71.420762
746.174520	25.974896	71.425767
744.918286	28.538131	71.430772
744.355060	26.224204	71.435777
743.987325	41.125272	71.440782
742.858594	40.552336	71.445786
742.336774	31.039760	71.450791
741.535945	29.686119	71.455796
741.184898	29.184919	71.460801
740.440169	31.680923	71.465806
739.799521	30.716498	71.470810
739.112926	27.810390	71.475815
738.601543	29.651120	71.480820
737.787254	33.917973	71.485825
736.900286	31.098952	71.490830
736.078161	23.811830	71.495834
736.085870	26.348894	71.500839
735.373681	33.871477	71.505844
734.627056	26.950782	71.510849
733.395473	25.638909	71.515854
732.508535	30.220084	71.520858
732.584393	26.970266	71.525863
731.943367	26.635071	71.530868
731.438386	24.985194	71.535873
730.745101	22.409718	71.540878
730.196414	22.830907	71.545882
729.571047	17.294319	71.550887
728.064569	35.289115	71.555892
727.597742	19.033030	71.560897
727.061975	23.339118	71.565902
726.950435	26.428144	71.570906
725.753796	22.860536	71.575911
724.720601	29.514912	71.580916
724.622779	25.393934	71.585921
724.357941	32.515740	71.590926
723.191586	27.511522	71.595930
722.802591	22.894458	71.600935
721.555433	29.305370	71.605940
721.433702	21.935140	71.610945
720.526090	33.284333	71.615950
719.506880	33.613283	71.620954
719.438615	18.023839	71.625959
718.663738	25.666781	71.630964
718.320129	23.855608	71.635969
717.180210	24.520723	71.640974
716.537447	25.694861	71.645978
715.951132	17.832502	71.650983
715.402837	28.853272	71.655988
714.439110	19.193455	71.660993
713.545735	25.079721	71.665998
713.232227	33.193235	71.671002
713.133329	29.480834	71.676007
712.304897	31.969672	71.681012
711.232948	28.415333	71.686017
710.489951	27.301640	71.691022
710.188226	28.673784	71.696026
709.961657	21.031681	71.701031
708.574621	22.447303	71.706036
708.270523	21.254278	71.711041
707.566067	28.382995	71.716046
706.806544	20.267531	71.721050
705.820788	26.808710	71.726055
705.162807	35.085869	71.731060
705.281804	23.194307	71.736065
704.234032	23.799029	71.741070
703.278013	18.617845	71.746074
702.809581	17.261760	71.751079
702.227610	27.578305	71.756084
701.104470	21.529649	71.761089
700.422609	25.316562	71.766094
699.826327	27.727445	71.771098
699.384355	18.369325	71.776103
698.818938	20.895135	71.781108
698.497155	21.860491	71.786113
697.371696	29.240728	71.791118
696.795675	25.642134	71.796122
696.732026	24.046575	71.801127
695.359991	26.375971	71.806132
694.453209	25.630536	71.811137
694.197970	25.695951	71.816142
693.585876	23.736726	71.821146
693.084541	22.947242	71.826151
691.935775	31.171657	71.831156
691.483383	21.605474	71.836161
690.808586	27.097425	71.841166
690.403744	26.898092	71.846170
689.682487	17.685358	71.851175
688.481480	32.337479	71.856180
688.146607	19.871668	71.861185
687.654407	25.004984	71.866190
687.115122	27.479332	71.871194
686.453485	22.930911	71.876199
685.802940	33.649441	71.881204
685.245627	20.282391	71.886209
684.074136	28.505695	71.891214
683.269630	23.379239	71.896218
683.159481	20.712514	71.901223
682.420318	27.589734	71.906228
681.548511	24.550715	71.911233
680.987882	28.567475	71.916238
680.080408	19.149440	71.921242
679.948317	21.365004	71.926247
678.802511	32.674864	71.931252
678.115159	25.218083	71.936257
677.339325	29.734280	71.941262
676.976768	28.424417	71.946266
676.851811	23.536679	71.951271
675.697088	26.195741	71.956276
674.809640	19.787895	71.961281
674.226728	26.777425	71.966286
673.861993	17.681389	71.971290
673.525517	17.565786	71.976295
672.199369	29.654942	71.981300
671.823948	29.357894	71.986305
671.285210	24.931828	71.991310
670.167931	25.192837	71.996314
669.527908	16.386623	72.001319
668.972730	30.716739	72.006324
668.743686	20.763364	72.011329
667.843785	34.527088	72.016334
666.763940	27.440288	72.021338
666.164582	22.404171	72.026343
665.897677	26.661155	72.031348
665.665896	23.329440	72.036353
664.427344	26.129579	72.041358
663.421930	20.994121	72.046362
663.325637	18.322038	72.051367
662.723742	23.319867	72.056372
661.855783	25.740900	72.061377
661.120134	26.236024	72.066382
660.568347	30.547829	72.071386
660.864556	18.921354	72.076391
659.148239	29.226138	72.081396
658.807754	27.841805	72.086401
657.490775	25.023477	72.091406
656.523780	33.275731	72.096410
656.261298	28.394123	72.101415
655.424383	23.299644	72.106420
655.153752	24.602192	72.111425
654.613513	25.018899	72.116430
654.215417	22.158340	72.121434
653.528337	20.646278	72.126439
652.598161	24.944219	72.131444
652.094675	21.477583	72.136449
650.864260	20.769502	72.141454
650.020333	21.419056	72.146458
649.692964	13.759902	72.151463
648.982423	26.869038	72.156468
648.513409	22.979046	72.161473
648.267545	17.602817	72.166478
647.442895	26.059473	72.171482
646.607385	18.919592	72.176487
646.089075	23.151956	72.181492
645.636799	19.809623	72.186497
644.628471	24.235121	72.191502
643.998625	22.387539	72.196506
643.409536	17.974230	72.201511
642.671756	29.249091	72.206516
641.827075	17.555133	72.211521
640.962816	14.573273	72.216526
640.746180	19.183353	72.221530
640.470026	19.034497	72.226535
639.139269	20.100594	72.231540
638.553233	17.258927	72.236545
638.050647	26.071133	72.241550
637.349139	26.816278	72.246554
637.302432	18.085902	72.251559
635.899243	20.448672	72.256564
635.615091	12.706951	72.261569
634.786810	16.919289	72.266574
633.944927	28.183921	72.271578
633.111171	13.583659	72.276583
632.230521	15.793845	72.281588
632.242062	16.209424	72.286593
631.972280	24.926217	72.291598
630.748307	23.365618	72.296602
629.765427	12.825857	72.301607
629.320587	32.819820	72.306612
629.001330	15.412825	72.311617
628.349744	26.889992	72.316622
627.496648	26.850349	72.321626
626.984554	25.472848	72.326631
626.268506	18.749165	72.331636
625.177341	26.854051	72.336641
624.336717	21.509455	72.341646
623.792296	14.886172	72.346650
623.661634	19.950889	72.351655
623.345933	24.297642	72.356660
622.580799	21.706833	72.361665
621.396990	19.827626	72.366670
620.572791	31.546735	72.371674
620.431260	27.194619	72.376679
619.402005	20.465622	72.381684
618.847875	19.954203	72.386689
618.267821	15.578885	72.391694
617.976694	23.393961	72.396698
617.067980	25.129258	72.401703
616.354793	28.943254	72.406708
615.946261	13.713929	72.411713
614.887253	21.299640	72.416718
614.154786	21.059456	72.421722
613.684014	12.620526	72.426727
613.202323	20.729280	72.431732
612.399709	19.541538	72.436737
611.359108	12.839584	72.441742
611.066469	18.035742	72.446746
610.424418	15.195118	72.451751
609.241171	10.160542	72.456756
608.478140	16.831852	72.461761
607.978374	17.839751	72.466766
607.734630	14.293922	72.471770
607.285482	12.572109	72.476775
606.627785	26.068625	72.481780
605.488618	19.626779	72.486785
604.775503	22.191896	72.491790
604.311996	18.819825	72.496794
604.303742	23.338380	72.501799
603.029659	26.592032	72.506804
602.518161	14.591164	72.511809
601.893470	18.790014	72.516814
600.471119	19.930638	72.521818
599.792576	19.456380	72.526823
599.466613	25.876757	72.531828
599.026760	17.508594	72.536833
598.795126	15.361085	72.541838
598.125046	18.100688	72.546842
597.163746	18.365275	72.551847
596.191159	19.719689	72.556852
595.597489	23.798492	72.561857
595.679432	19.838122	72.566862
594.439234	21.176809	72.571866
593.739689	18.058357	72.576871
593.212663	14.849359	72.581876
592.392483	12.109642	72.586881
591.463914	24.469806	72.591886
590.656706	21.811596	72.596890
590.553505	12.429523	72.601895
589.738770	23.648838	72.606900
589.613986	17.389220	72.611905
588.595100	18.724204	72.616910
587.751266	13.660817	72.621914
587.196692	15.251423	72.626919
586.452510	29.293117	72.631924
585.736828	14.946871	72.636929
585.346348	19.343378	72.641934
584.812498	16.663715	72.646938
584.127300	17.765800	72.651943
582.918653	29.383722	72.656948
582.119894	23.860597	72.661953
582.245828	17.322948	72.666958
581.338054	26.625437	72.671962
580.579376	17.079681	72.676967
579.665810	15.457062	72.681972
579.170768	14.398535	72.686977
578.992044	13.472548	72.691982
577.905952	20.632103	72.696986
577.435051	13.814211	72.701991
576.740502	20.515622	72.706996
576.079816	12.884336	72.712001
574.858352	16.919624	72.717006
574.378496	18.758516	72.722010
574.046883	10.417278	72.727015
573.200192	12.284628	72.732020
572.911991	17.041715	72.737025
571.650755	20.996613	72.742030
570.905592	23.096939	72.747034
570.633964	20.003381	72.752039
570.362488	29.002704	72.757044
569.419564	21.443170	72.762049
568.401433	14.471170	72.767054
567.769064	29.310294	72.772058
567.893339	19.103565	72.777063
566.689221	27.775205	72.782068
565.914120	23.522419	72.787073
565.310104	21.297030	72.792078
564.761962	23.140491	72.797082
564.481630	24.627508	72.802087
563.259894	26.769043	72.807092
562.364748	23.292267	72.812097
562.384676	19.614570	72.817102
561.615223	26.556560	72.822106
560.461915	24.869632	72.827111
559.462585	28.946819	72.832116
559.405077	15.676829	72.837121
558.806605	23.578699	72.842126
558.422385	30.929242	72.847130
557.709855	21.893352	72.852135
556.863992	21.429985	72.857140
556.450329	24.112993	72.862145
555.418641	32.903827	72.867150
554.396051	30.385579	72.872154
554.333936	20.404065	72.877159
553.544950	28.670572	72.882164
553.136197	14.072045	72.887169
551.992092	21.961471	72.892174
551.343863	12.891696	72.897178
551.348428	17.703077	72.902183
550.206321	15.195984	72.907188
549.244536	20.410412	72.912193
548.697369	19.644026	72.917198
548.247235	27.105985	72.922202
548.112453	24.965131	72.927207
546.847629	23.619225	72.932212
545.986552	21.669734	72.937217
545.652238	24.920389	72.942222
544.709259	27.564706	72.947226
544.077545	15.702844	72.952231
543.289826	20.908474	72.957236
542.599143	19.553127	72.962241
542.462209	18.216813	72.967246
541.915460	23.018236	72.972250
541.434001	17.607011	72.977255
540.170221	18.470116	72.982260
539.788201	13.943439	72.987265
538.656832	23.652109	72.992270
537.850255	21.750707	72.997274
537.655020	15.123872	73.002279
537.060719	27.938560	73.007284
536.923036	17.890243	73.012289
535.212485	15.684990	73.017294
534.709333	23.466032	73.022298
534.427550	13.694542	73.027303
533.770517	20.557133	73.032308
533.410752	10.671917	73.037313
532.176742	14.590957	73.042318
531.427215	26.097926	73.047322
531.129945	16.395130	73.052327
530.467515	24.067509	73.057332
529.573201	15.965700	73.062337
528.751902	15.511046	73.067342
528.495491	22.751350	73.072346
528.348369	12.236216	73.077351
527.134339	19.214327	73.082356
526.506526	17.582483	73.087361
526.235306	20.167119	73.092366
524.892848	24.658490	73.097370
523.973193	18.052424	73.102375
523.681428	29.598445	73.107380
523.234710	20.923907	73.112385
523.025702	9.329026	73.117390
521.852786	21.838502	73.122394
521.360099	21.229014	73.127399
520.440158	21.253668	73.132404
519.560871	13.890594	73.137409
519.204042	15.631057	73.142414
517.964469	18.321044	73.147418
518.016697	19.893859	73.152423
517.255308	17.464906	73.157428
516.580301	15.965153	73.162433
515.806458	23.794043	73.167438
515.006467	25.672897	73.172442
514.894005	15.631606	73.177447
513.460734	23.625448	73.182452
512.962611	18.981658	73.187457
512.454460	25.839464	73.192462
511.784188	19.665161	73.197466
511.723237	15.341224	73.202471
510.658050	19.976084	73.207476
510.250140	15.387308	73.212481
509.657331	12.573561	73.217486
508.113011	14.000151	73.222490
507.741720	9.367701	73.227495
507.071118	13.583342	73.232500
506.465192	12.189276	73.237505
506.162997	13.727085	73.242510
505.077954	15.258708	73.247514
504.390559	14.144107	73.252519
503.963951	18.207353	73.257524
503.330205	20.804006	73.262529
503.041284	15.789451	73.267534
501.802206	19.187374	73.272538
501.515418	17.105428	73.277543
500.644011	23.857102	73.282548
500.227737	20.901703	73.287553
499.089352	19.573528	73.292558
498.427362	32.974558	73.297562
498.332754	21.769856	73.302567
497.135544	25.842315	73.307572
496.483523	14.300655	73.312577
495.854694	24.279355	73.317582
495.017403	27.430371	73.322586
495.029663	19.343435	73.327591
494.231518	22.306877	73.332596
493.192753	22.834562	73.337601
492.763083	21.737256	73.342606
492.048197	16.803167	73.347610
491.701014	16.353424	73.352615
490.437661	18.512659	73.357620
490.024252	17.422225	73.362625
489.521157	22.907365	73.367630
488.863704	25.810553	73.372634
487.999736	14.026707	73.377639
487.318865	20.402703	73.382644
486.936286	12.023873	73.387649
486.349503	11.320579	73.392654
485.298399	19.553160	73.397658
484.396619	15.833061	73.402663
483.743036	26.457487	73.407668
483.539490	18.997825	73.412673
483.231071	17.728253	73.417678
482.250997	26.748989	73.422682
481.922600	18.809353	73.427687
481.344322	22.493088	73.432692
480.282569	12.437447	73.437697
479.762951	14.687939	73.442702
478.879782	21.003126	73.447706
477.953986	26.643905	73.452711
476.960977	24.534115	73.457716
476.404149	20.379049	73.462721
476.412622	25.418450	73.467726
475.575982	22.839080	73.472730
475.414763	14.070199	73.477735
474.473089	20.408898	73.482740
473.776085	21.777804	73.487745
473.186691	21.421836	73.492750
472.007297	22.238419	73.497754
471.380733	17.873704	73.502759
470.728314	23.135066	73.507764
470.514760	24.712373	73.512769
469.719469	17.414781	73.517774
468.430786	21.325216	73.522778
468.148076	16.864729	73.527783
467.778898	23.976352	73.532788
467.269642	16.756192	73.537793
466.556968	22.222683	73.542798
465.281049	25.309546	73.547802
465.100031	26.856441	73.552807
464.447010	19.531457	73.557812
463.432056	22.502637	73.562817
463.090139	21.574273	73.567822
462.117108	32.457738	73.572826
461.945699	10.832818	73.577831
460.775978	21.768106	73.582836
460.056384	19.302553	73.587841
459.548064	10.708810	73.592846
459.219198	17.109155	73.597850
458.876142	16.691874	73.602855
457.359957	19.471683	73.607860
456.898515	18.668009	73.612865
456.574843	17.208493	73.617870
455.650450	28.344390	73.622874
454.968627	25.328806	73.627879
454.316694	23.819087	73.632884
453.521802	24.681653	73.637889
453.362292	24.444854	73.642894
452.582291	26.147089	73.647898
451.821842	14.239543	73.652903
451.113488	26.826419	73.657908
450.647481	19.429072	73.662913
449.641473	18.854067	73.667918
448.740612	32.575412	73.672922
448.359589	29.395224	73.677927
447.774063	28.273871	73.682932
447.449857	35.044043	73.687937
446.479944	37.680072	73.692942
445.880502	30.570466	73.697946
445.671094	23.461804	73.702951
444.295020	23.475577	73.707956
443.575387	24.895401	73.712961
443.120661	23.838364	73.717966
442.070886	21.950508	73.722970
442.239816	14.087764	73.727975
441.306988	28.304600	73.732980
440.423850	18.949028	73.737985
439.830456	23.645942	73.742990
439.318046	25.061139	73.747994
438.754262	14.446826	73.752999
437.862919	22.474212	73.758004
437.324649	21.225494	73.763009
437.122551	20.296935	73.768014
435.829067	23.339304	73.773018
435.386906	15.592834	73.778023
434.299953	22.117106	73.783028
434.048601	19.496547	73.788033
433.310871	20.107178	73.793038
432.239563	20.185939	73.798042
431.750531	18.229255	73.803047
431.084658	20.777429	73.808052
430.838611	22.438757	73.813057
430.568062	13.215822	73.818062
429.289172	22.553818	73.823066
429.110443	17.012397	73.828071
427.864493	31.857827	73.833076
426.988047	13.729163	73.838081
426.534028	19.070882	73.843086
425.668712	28.409224	73.848090
425.328514	12.711789	73.853095
424.766489	17.988719	73.858100
423.921201	17.924250	73.863105
423.476806	22.239483	73.868110
422.801057	17.655552	73.873114
422.400529	14.598320	73.878119
421.474756	20.795739	73.883124
421.072886	12.391615	73.888129
420.424582	14.247907	73.893134
419.161798	16.563194	73.898138
418.624454	14.026045	73.903143
417.777419	20.359145	73.908148
417.623364	16.844781	73.913153
416.937603	13.935488	73.918158
415.654655	16.078958	73.923162
415.479377	12.720931	73.928167
414.998095	20.041214	73.933172
414.292204	8.265338	73.938177
413.223153	7.616819	73.943182
412.373875	18.631948	73.948186
412.126873	10.714055	73.953191
411.657558	14.691082	73.958196
410.754327	12.693167	73.963201
410.277208	6.344638	73.968206
409.241061	16.202169	73.973210
409.227387	12.936660	73.978215
408.272832	12.416548	73.983220
407.285348	16.258525	73.988225
407.199367	13.007689	73.993230
406.184903	23.279637	73.998234
405.244570	22.167518	74.003239
404.640187	20.363250	74.008244
403.874574	20.388589	74.013249
403.753822	20.593445	74.018254
403.042276	29.782722	74.023258
402.445893	25.720703	74.028263
401.504107	21.926591	74.033268
401.061210	15.468535	74.038273
400.718830	14.251691	74.043278
399.176026	15.287045	74.048282
398.729592	9.277383	74.053287
398.006701	14.775475	74.058292
397.651336	14.782759	74.063297
397.361072	12.151060	74.068302
395.736508	18.975451	74.073306
395.473330	8.538753	74.078311
395.010164	13.131350	74.083316
394.687374	9.331657	74.088321
393.812353	12.761507	74.093326
393.155302	20.688501	74.098330
392.750277	17.195203	74.103335
391.727939	17.409672	74.108340
390.739856	17.421578	74.113345
390.287385	16.911359	74.118350
389.817782	20.208813	74.123354
388.935057	7.054571	74.128359
387.945482	13.050864	74.133364
387.391618	11.121866	74.138369
386.937455	8.268718	74.143374
386.410624	13.380783	74.148378
385.954613	14.563090	74.153383
384.788866	16.787244	74.158388
384.272015	20.327178	74.163393
383.923917	16.763314	74.168398
383.314195	21.964278	74.173402
382.645663	23.983066	74.178407
381.448213	13.986942	74.183412
381.167883	7.432035	74.188417
380.631868	16.648531	74.193422
379.345065	25.161539	74.198426
378.769309	19.539889	74.203431
378.258931	19.458341	74.208436
378.230497	15.181268	74.213441
377.603330	14.859725	74.218446
376.110134	26.042115	74.223450
375.869170	17.692782	74.228455
375.107671	16.656253	74.233460
374.545303	14.156216	74.238465
373.701890	19.115313	74.243470
372.799388	21.324336	74.248474
372.645281	11.814797	74.253479
371.681975	13.875822	74.258484
371.404568	16.458301	74.263489
370.887402	7.017651	74.268494
369.987355	15.380730	74.273498
369.506664	10.975460	74.278503
368.322529	20.359878	74.283508
367.251513	19.555583	74.288513
367.326144	19.081223	74.293518
366.432582	22.573958	74.298522
366.214082	14.667298	74.303527
365.253457	16.428297	74.308532
364.274626	16.254248	74.313537
364.050377	17.063762	74.318542
363.569240	23.210852	74.323546
362.742243	15.705480	74.328551
361.488370	21.340225	74.333556
361.185392	14.713238	74.338561
361.118406	12.255689	74.343566
359.811838	11.627693	74.348570
359.407475	12.207303	74.353575
358.861117	27.382798	74.358580
358.109197	23.052281	74.363585
357.139810	14.800097	74.368590
356.425440	24.951709	74.373594
356.325710	19.205333	74.378599
355.581495	10.605057	74.383604
354.605280	21.337672	74.388609
353.929166	19.067062	74.393614
353.283572	28.384602	74.398618
352.931935	19.232944	74.403623
351.645579	22.550167	74.408628
350.954964	27.510156	74.413633
350.930403	23.525760	74.418638
349.908186	20.351573	74.423642
349.978541	17.727069	74.428647
349.095994	23.162312	74.433652
348.220197	15.917019	74.438657
347.835949	8.216538	74.443662
346.765662	10.247313	74.448666
346.029889	16.002919	74.453671
345.464191	19.965355	74.458676
344.839215	16.557573	74.463681
343.671054	6.990444	74.468686
343.083221	13.749006	74.473690
342.608503	13.975577	74.478695
342.402562	19.085401	74.483700
341.812757	9.156471	74.488705
341.014878	14.329079	74.493710
340.073137	19.737488	74.498714
339.649496	17.630065	74.503719
338.705966	15.922432	74.508724
337.701567	20.337949	74.513729
337.511495	13.716629	74.518734
336.689555	19.708306	74.523738
336.436574	14.915119	74.528743
335.196027	17.953832	74.533748
334.157119	13.189694	74.538753
333.995941	10.772386	74.543758
333.659615	22.785940	74.548762
333.629793	9.554157	74.553767
332.495654	18.705131	74.558772
331.548901	17.037436	74.563777
331.073508	10.966176	74.568782
329.921435	23.951758	74.573786
329.251618	8.639599	74.578791
328.851466	18.968207	74.583796
328.448971	10.707701	74.588801
327.897605	11.518885	74.593806
326.941372	19.343765	74.598810
326.275948	14.619457	74.603815
325.768954	19.554919	74.608820
325.060039	16.773914	74.613825
323.799257	16.190677	74.618830
322.939445	29.262149	74.623834
323.076333	14.370179	74.628839
322.343324	19.825751	74.633844
322.054417	28.914580	74.638849
321.149495	21.789047	74.643854
320.061740	28.472753	74.648858
320.013882	15.513483	74.653863
319.386228	23.725948	74.658868
318.259596	13.075222	74.663873
317.788245	9.562550	74.668878
316.977255	23.745801	74.673882
316.334938	9.916234	74.678887
315.411301	17.677579	74.683892
314.635637	21.406992	74.688897
314.282693	26.691622	74.693902
313.691286	30.451596	74.698906
313.473422	15.564123	74.703911
312.580888	20.505836	74.708916
311.731887	19.763950	74.713921
311.497343	15.395156	74.718926
310.082661	15.736832	74.723930
309.089535	18.157424	74.728935
308.996733	15.497424	74.733940
308.441063	13.111446	74.738945
308.224120	15.291660	74.743950
307.256688	13.239365	74.748954
306.658012	7.151492	74.753959
305.753393	18.175463	74.758964
305.485108	23.129655	74.763969
304.281217	11.652366	74.768974
303.444165	26.092071	74.773978
303.072609	14.116309	74.778983
302.971359	27.951511	74.783988
301.885105	27.665303	74.788993
301.250059	14.000149	74.793998
300.762981	22.108217	74.799002
299.783423	23.753995	74.804007
298.888960	18.230464	74.809012
298.090538	16.003014	74.814017
297.940567	15.118198	74.819022
297.227450	29.997020	74.824026
296.823065	14.907479	74.829031
295.728622	23.415096	74.834036
295.338966	22.910653	74.839041
295.009558	20.895446	74.844046
293.969046	23.957490	74.849050
293.257040	16.277714	74.854055
292.722237	22.955302	74.859060
292.254929	20.832771	74.864065
291.389531	19.308235	74.869070
290.275969	26.108020	74.874074
290.017184	17.944457	74.879079
289.548827	21.115580	74.884084
288.725704	17.048733	74.889089
287.997747	22.512969	74.894094
287.092789	19.484116	74.899098
286.680196	16.878235	74.904103
285.426222	20.059451	74.909108
284.760955	21.562111	74.914113
284.547972	16.568605	74.919118
283.907936	22.887675	74.924122
283.465186	8.195319	74.929127
283.169440	24.083032	74.934132
282.152678	25.731592	74.939137
281.661134	27.186068	74.944142
280.684428	24.722126	74.949146
279.997149	11.656626	74.954151
279.004980	16.656802	74.959156
278.342829	17.175013	74.964161
278.335789	10.024672	74.969166
277.674260	23.132352	74.974170
276.832290	19.453263	74.979175
276.192886	19.950504	74.984180
275.610274	27.854622	74.989185
274.614834	14.497634	74.994190
273.525495	11.859272	74.999194
272.999075	17.021750	75.004199
272.688092	22.831093	75.009204
272.383146	15.805494	75.014209
271.830811	19.664895	75.019214
270.812775	23.373028	75.024218
270.166836	14.143726	75.029223
269.603160	15.527704	75.034228
268.591478	14.553158	75.039233
267.864052	15.690438	75.044238
267.088568	23.254734	75.049242
266.999081	15.616093	75.054247
266.389144	4.736408	75.059252
265.753893	16.231509	75.064257
265.308486	10.576506	75.069262
264.236909	21.715403	75.074266
263.261702	18.404462	75.079271
262.408029	14.154849	75.084276
261.857799	7.508948	75.089281
261.621340	9.864150	75.094286
261.034499	10.747230	75.099290
260.876508	19.618082	75.104295
259.832058	20.444794	75.109300
258.975340	17.152814	75.114305
258.437890	10.836015	75.119310
256.988589	20.228046	75.124314
256.895189	18.530022	75.129319
256.098086	15.917626	75.134324
255.698443	11.048486	75.139329
255.460508	16.885607	75.144334
254.214889	17.689194	75.149338
253.451534	18.061126	75.154343
253.240671	18.537377	75.159348
251.993816	21.245996	75.164353
251.249302	13.989283	75.169358
250.626136	18.345645	75.174362
250.408084	18.657473	75.179367
250.028041	8.704604	75.184372
249.140188	21.950853	75.189377
248.718601	17.170361	75.194382
247.877452	24.819239	75.199386
247.244275	11.175888	75.204391
246.063581	16.986663	75.209396
244.987225	19.619228	75.214401
244.966140	10.397572	75.219406
244.818494	12.226144	75.224410
243.742300	10.940214	75.229415
242.819386	22.053846	75.234420
242.509289	13.103742	75.239425
241.804408	11.028550	75.244430
240.870228	19.564253	75.249434
240.388439	10.155847	75.254439
239.855455	19.315111	75.259444
239.261114	13.267563	75.264449
238.780105	16.208912	75.269454
237.938798	9.440689	75.274458
236.994976	21.562107	75.279463
236.806337	19.136568	75.284468
235.441003	9.834300	75.289473
234.699350	11.905774	75.294478
234.140847	25.345523	75.299482
233.895730	16.307796	75.304487
233.371155	12.765782	75.309492
232.656625	16.780342	75.314497
231.784144	15.512407	75.319502
230.744738	16.418745	75.324506
230.706124	11.633983	75.329511
230.163645	15.570661	75.334516
228.796923	25.684359	75.339521
228.484105	14.760475	75.344526
227.825665	14.954853	75.349530
227.748119	19.993756	75.354535
226.621139	17.202153	75.359540
225.822256	20.020718	75.364545
225.593397	13.413482	75.369550
224.382770	20.621395	75.374554
223.478583	10.938145	75.379559
223.067520	5.085305	75.384564
222.716825	24.532834	75.389569
222.508296	20.317589	75.394574
221.029005	21.661453	75.399578
220.594995	19.861614	75.404583
220.019942	26.510940	75.409588
219.291530	16.023860	75.414593
218.479786	16.272637	75.419598
217.625256	19.904268	75.424602
217.489782	16.855286	75.429607
216.744487	23.367754	75.434612
215.847642	22.302390	75.439617
215.502129	16.719777	75.444622
214.816096	28.092111	75.449626
214.343588	23.203054	75.454631
213.327314	17.534983	75.459636
212.053438	24.882287	75.464641
211.919315	19.794224	75.469646
211.395869	22.046953	75.474650
210.831115	13.151640	75.479655
209.811768	15.866588	75.484660
209.069540	21.484495	75.489665
209.240691	14.729926	75.494670
208.121244	29.028596	75.499674
207.090283	19.879608	75.504679
206.630195	22.021321	75.509684
205.871032	22.600743	75.514689
205.911458	19.735021	75.519694
204.489715	34.938113	75.524698
203.981229	18.255229	75.529703
203.186210	27.714874	75.534708
202.572359	23.214179	75.539713
202.899782	16.850987	75.544718
201.443051	26.129123	75.549722
201.001116	11.856103	75.554727
200.406220	13.059004	75.559732
198.989452	22.042205	75.564737
198.086375	8.482898	75.569742
197.904067	23.584598	75.574746
197.332734	12.455943	75.579751
197.085777	16.142107	75.584756
196.355205	22.638041	75.589761
195.589831	17.970704	75.594766
194.700866	27.303410	75.599770
194.225319	13.609722	75.604775
193.969028	22.846304	75.609780
193.047294	21.631961	75.614785
192.693541	20.022748	75.619790
191.381516	31.403417	75.624794
190.478295	24.285554	75.629799
189.687649	21.096601	75.634804
188.891923	24.384575	75.639809
188.705080	15.654515	75.644814
188.404066	27.542604	75.649818
188.236635	20.121385	75.654823
187.020851	22.140730	75.659828
186.174518	24.717729	75.664833
185.889177	12.867021	75.669838
184.659413	28.730171	75.674842
184.034018	16.047478	75.679847
183.480417	18.691347	75.684852
182.993232	25.151640	75.689857
182.569737	19.895257	75.694862
181.414640	20.969859	75.699866
180.898175	22.656969	75.704871
180.181824	18.798631	75.709876
179.913287	23.282969	75.714881
179.204659	11.419321	75.719886
177.678462	19.445483	75.724890
177.308712	21.249545	75.729895
176.981472	20.079202	75.734900
176.676855	22.721226	75.739905
176.253607	19.579359	75.744910
175.286040	24.107328	75.749914
174.562479	17.703530	75.754919
173.471499	16.342723	75.759924
172.591502	15.996886	75.764929
172.547561	13.166691	75.769934
171.721134	23.809252	75.774938
171.604418	23.125709	75.779943
170.778288	16.128025	75.784948
170.147167	25.735001	75.789953
168.997420	12.724349	75.794958
167.951317	23.296282	75.799962
167.488953	21.720155	75.804967
167.158251	22.146136	75.809972
166.731920	22.492751	75.814977
165.847374	19.279355	75.819982
165.049848	21.823350	75.824986
164.594135	18.786003	75.829991
164.257691	26.693468	75.834996
162.795780	29.720247	75.840001
162.351151	19.727230	75.845006
161.466361	26.755504	75.850010
161.323103	15.930753	75.855015
160.518342	23.337325	75.860020
159.450450	21.567592	75.865025
159.189767	17.901530	75.870030
158.696773	25.925408	75.875034
158.216750	33.955108	75.880039
156.727973	22.505971	75.885044
156.308242	32.560193	75.890049
156.465798	21.731634	75.895054
155.359648	22.697527	75.900058
154.552243	20.651319	75.905063
154.023193	29.278574	75.910068
153.206422	29.151307	75.915073
152.687307	21.505480	75.920078
151.176844	23.354215	75.925082
150.976434	19.293793	75.930087
150.570817	16.589062	75.935092
149.829621	32.197731	75.940097
149.599740	23.655872	75.945102
148.959517	25.094654	75.950106
147.765259	18.387463	75.955111
147.226826	28.988850	75.960116
146.708311	25.384391	75.965121
145.801641	19.042910	75.970126
144.637032	26.416976	75.975130
144.435720	18.824559	75.980135
144.313172	22.099835	75.985140
143.578320	25.691911	75.990145
142.589918	22.841987	75.995150
141.633632	21.704131	76.000154
141.665052	21.397493	76.005159
140.878833	24.228256	76.010164
140.042054	25.058177	76.015169
139.465043	20.460171	76.020174
138.757722	22.914105	76.025178
138.243066	13.512544	76.030183
137.270279	20.228443	76.035188
136.388404	26.776897	76.040193
136.055854	21.521793	76.045198
135.517789	25.495632	76.050202
134.775011	12.921556	76.055207
133.948816	22.340455	76.060212
133.304160	20.783937	76.065217
133.190081	16.154704	76.070222
131.977024	19.723680	76.075226
131.334049	18.091206	76.080231
130.951406	15.059563	76.085236
130.360716	14.051070	76.090241
129.399029	12.633402	76.095246
128.378017	18.822441	76.100250
127.911577	13.804716	76.105255
127.580336	22.566002	76.110260
126.965087	20.716234	76.115265
126.307458	13.076735	76.120270
125.636377	20.909826	76.125274
125.125541	19.308322	76.130279
123.929465	15.682595	76.135284
123.194928	20.198657	76.140289
122.937652	18.846868	76.145294
122.262827	21.325585	76.150298
121.538829	16.027248	76.155303
120.429021	16.837630	76.160308
119.564714	17.817016	76.165313
119.535692	19.427999	76.170318
119.033053	17.724272	76.175322
118.763927	24.514058	76.180327
117.746662	10.411639	76.185332
116.963586	22.204704	76.190337
116.686330	11.844422	76.195342
115.205779	14.435833	76.200346
114.630147	18.964405	76.205351
114.005657	15.242821	76.210356
113.738423	13.041124	76.215361
113.558204	9.176174	76.220366
112.138927	17.226320	76.225370
111.422271	14.397736	76.230375
110.928946	19.506080	76.235380
110.565945	16.275780	76.240385
109.717209	9.724822	76.245390
108.656004	13.184446	76.250394
108.172086	16.334424	76.255399
107.666846	16.181155	76.260404
106.817645	17.732109	76.265409
106.244049	2.038885	76.270414
105.583751	12.107798	76.275418
104.952768	14.606335	76.280423
104.709126	9.841657	76.285428
103.630192	11.979559	76.290433
103.260195	9.557722	76.295438
102.242464	17.219020	76.300442
101.800281	11.202445	76.305447
101.064791	8.750580	76.310452
100.001385	15.649660	76.315457
99.775935	11.579048	76.320462
98.666206	26.055958	76.325466
98.587821	12.824069	76.330471
97.771961	17.975957	76.335476
96.762468	18.131732	76.340481
96.672365	14.061615	76.345486
96.120109	17.676623	76.350490
95.281628	8.008189	76.355495
94.764929	15.468184	76.360500
93.583451	19.612422	76.365505
92.892814	6.982751	76.370510
92.041112	16.150273	76.375514
91.662519	18.204897	76.380519
90.951700	18.980059	76.385524
90.760440	15.928946	76.390529
90.353439	8.233731	76.395534
89.222534	16.849725	76.400538
88.635598	7.981644	76.405543
87.997859	11.014235	76.410548
86.622548	19.167764	76.415553
86.504465	13.301351	76.420558
85.975050	15.523517	76.425562
85.308048	11.345128	76.430567
84.338366	16.400129	76.435572
83.366043	18.100023	76.440577
83.315668	4.190365	76.445582
82.822139	15.904149	76.450586
82.188389	14.164570	76.455591
81.349434	9.032803	76.460596
80.773189	12.257426	76.465601
80.549678	5.299305	76.470606
79.140524	15.736773	76.475610
78.474332	9.156722	76.480615
77.899668	14.916662	76.485620
77.199309	19.599161	76.490625
76.512865	9.341980	76.495630
75.900218	12.504605	76.500634
74.952492	16.318284	76.505639
74.883818	14.179542	76.510644
73.821502	13.607363	76.515649
73.106798	11.819198	76.520654
72.462272	26.477387	76.525658
72.043058	16.502422	76.530663
71.677124	22.790440	76.535668
70.737210	27.090124	76.540673
69.997281	19.350231	76.545678
69.331141	23.811249	76.550682
68.822393	18.149046	76.555687
68.010706	12.345929	76.560692
67.289591	22.774613	76.565697
66.596050	19.666408	76.570702
66.038951	22.214670	76.575706
65.799879	10.637294	76.580711
64.674096	16.720066	76.585716
63.973425	13.387511	76.590721
63.568674	18.369782	76.595726
62.356602	18.959971	76.600730
61.662559	17.879672	76.605735
61.333531	19.850708	76.610740
61.046722	15.551781	76.615745
60.607841	13.334887	76.620750
59.331001	23.715003	76.625754
58.961213	10.114880	76.630759
58.288650	17.025763	76.635764
57.022470	12.515603	76.640769
56.391730	7.629746	76.645774
55.720145	17.989034	76.650778
55.282122	15.726275	76.655783
54.868991	16.260025	76.660788
54.582270	10.622344	76.665793
53.676508	12.461436	76.670798
52.805717	20.244390	76.675802
52.414282	13.694644	76.680807
51.629319	17.881319	76.685812
50.475492	19.994919	76.690817
50.328746	6.051751	76.695822
49.635389	21.212852	76.700826
49.432316	17.737878	76.705831
48.220092	17.528637	76.710836
47.454473	19.447879	76.715841
47.252139	11.176024	76.720846
46.040199	13.021368	76.725850
45.253077	20.535533	76.730855
45.148086	15.755060	76.735860
44.062314	14.264180	76.740865
43.397228	7.505782	76.745870
42.624073	17.203225	76.750874
42.311230	16.817452	76.755879
41.972910	13.300974	76.760884
41.048163	18.262097	76.765889
40.284933	9.259730	76.770894
39.406096	19.548000	76.775898
38.972588	14.209676	76.780903
38.844568	17.326564	76.785908
37.796788	14.809410	76.790913
37.299794	5.025050	76.795918
36.722778	13.390318	76.800922
35.283896	16.802974	76.805927
34.765012	13.198605	76.810932
33.960219	15.679146	76.815937
34.011640	15.709916	76.820942
32.855396	9.446132	76.825946
32.103104	1.126380	76.830951
31.559680	8.950162	76.835956
31.096669	12.759092	76.840961
30.705740	11.677770	76.845966
29.465473	12.491652	76.850970
29.160946	5.688375	76.855975
28.572021	11.288181	76.860980
27.556233	20.557577	76.865985
26.790772	7.692301	76.870990
25.421780	14.602295	76.875994
25.068880	14.834729	76.880999
24.871691	12.320696	76.886004
24.625421	16.672189	76.891009
24.488114	11.791224	76.896014
23.649078	17.159702	76.901018
22.705192	9.587967	76.906023
22.280461	9.442375	76.911028
20.936175	13.350850	76.916033
20.349346	12.149394	76.921038
19.424057	16.932428	76.926042
19.058250	14.656583	76.931047
18.803616	4.699547	76.936052
17.662393	12.695933	76.941057
17.076166	9.375103	76.946062
16.370019	13.498758	76.951066
16.017037	5.301396	76.956071
15.301803	4.792155	76.961076
14.298445	12.564720	76.966081
13.929115	11.965625	76.971086
13.215142	12.017539	76.976090
12.466820	13.807884	76.981095
11.861661	10.983627	76.986100
10.774720	20.270683	76.991105
10.815192	14.787394	76.996110
10.302772	15.034232	77.001114
9.232057	9.572049	77.006119
8.724518	11.021241	77.011124
7.942259	21.320924	77.016129
7.344543	8.479363	77.021134
6.178331	15.221419	77.026139
5.744546	6.787804	77.031143
5.331492	13.573736	77.036148
4.796370	23.707860	77.041153
3.926200	17.540381	77.046158