Mon Mar 08 19:18:49 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.386000	116.536396	0.000000
0.283974	93.845928	0.005005
-0.446784	62.770756	0.010010
-1.752826	8.620421	0.015014
-6.141324	-9.409375	0.020019
-11.858298	-9.861504	0.025024
-16.659645	-8.075489	0.030029
-21.743847	-11.862628	0.035034
-25.740163	-9.534850	0.040038
-29.045125	-28.699285	0.045043
-32.957647	-10.657471	0.050048
-36.622387	-15.716448	0.055053
-40.124030	-1.483571	0.060058
-43.805350	-5.655289	0.065062
-47.596785	-9.686440	0.070067
-51.519746	-0.750746	0.075072
-54.936186	-2.140580	0.080077
-58.819959	-11.762649	0.085082
-62.913844	1.495642	0.090086
-66.286364	-7.104188	0.095091
-69.937509	-1.900057	0.100096
-73.704982	-4.284039	0.105101
-77.498085	-2.013825	0.110106
-81.298880	-3.867391	0.115110
-85.094374	-8.678370	0.120115
-89.353454	-0.214082	0.125120
-92.664264	-12.969226	0.130125
-96.636566	-2.030892	0.135130
-100.602183	-9.624632	0.140134
-103.831953	-8.604807	0.145139
-107.894854	-10.717688	0.150144
-111.626972	-12.273101	0.155149
-115.533425	-16.843990	0.160154
-119.327043	-7.041074	0.165158
-122.983782	-9.499411	0.170163
-126.546165	-13.757777	0.175168
-129.793685	-14.294579	0.180173
-133.540913	-16.522433	0.185178
-138.103565	-10.368581	0.190182
-141.854205	-15.645482	0.195187
-145.854494	-16.421668	0.200192
-149.449017	-1.680281	0.205197
-153.041322	-2.408024	0.210202
-157.030032	-11.625278	0.215206
-160.844128	-5.734320	0.220211
-164.620271	5.336814	0.225216
-168.312691	-3.639144	0.230221
-172.241772	-10.562126	0.235226
-175.676041	1.485718	0.240230
-179.258244	-17.123359	0.245235
-182.877779	1.371785	0.250240
-186.763594	-14.058810	0.255245
-190.456059	-8.526237	0.260250
-194.697897	-0.121292	0.265254
-198.489581	-10.579350	0.270259
-201.983763	6.290600	0.275264
-205.653945	-10.254511	0.280269
-209.309384	-9.765814	0.285274
-213.309248	-1.905619	0.290278
-216.825023	-15.428896	0.295283
-221.014184	0.238480	0.300288
-224.541314	-8.016341	0.305293
-228.095571	-9.327165	0.310298
-232.416614	-7.688339	0.315302
-235.726727	-15.950967	0.320307
-239.956972	-10.614747	0.325312
-243.301597	-14.070389	0.330317
-246.990941	3.876206	0.335322
-250.773871	-6.494862	0.340326
-254.075503	-9.744479	0.345331
-258.315217	3.499546	0.350336
-262.328514	-7.637343	0.355341
-265.724222	-11.206217	0.360346
-269.675174	-14.798416	0.365350
-273.564792	-2.132184	0.370355
-277.355950	-6.200853	0.375360
-281.107486	-15.023690	0.380365
-284.628444	-9.319675	0.385370
-288.608392	-9.736198	0.390374
-292.295221	-16.912090	0.395379
-295.815388	-3.371313	0.400384
-299.946349	-9.563314	0.405389
-303.797201	-12.621119	0.410394
-307.412168	-15.371245	0.415398
-310.982930	-12.704110	0.420403
-314.811087	-5.571282	0.425408
-318.620696	-0.660014	0.430413
-322.017361	-17.671172	0.435418
-326.155772	-10.075670	0.440422
-329.472711	-10.468666	0.445427
-333.761609	-0.974268	0.450432
-337.346562	-5.080490	0.455437
-340.893742	-12.404746	0.460442
-345.034916	-0.928178	0.465446
-348.627274	-6.802409	0.470451
-352.670631	-9.741100	0.475456
-356.107003	-5.614706	0.480461
-360.004643	-7.447634	0.485466
-363.845663	-14.111554	0.490470
-367.390537	-16.478569	0.495475
-371.485341	-6.658734	0.500480
-375.095032	-10.847672	0.505485
-378.686320	-14.621680	0.510490
-382.353923	-12.747895	0.515494
-385.979278	-18.438612	0.520499
-390.283362	-17.346220	0.525504
-393.787040	-13.726231	0.530509
-397.508706	-8.817848	0.535514
-401.525944	-8.622726	0.540518
-405.216099	-21.755178	0.545523
-408.629348	-10.159795	0.550528
-412.705206	-12.375733	0.555533
-416.205324	-5.881712	0.560538
-419.928823	-6.999659	0.565542
-423.592830	-22.246057	0.570547
-428.225519	0.339071	0.575552
-431.595448	-6.294315	0.580557
-434.893934	-17.065670	0.585562
-439.104227	-7.588380	0.590566
-442.747039	-12.528803	0.595571
-446.747335	-10.169743	0.600576
-450.629370	-8.236383	0.605581
-454.288039	-13.114336	0.610586
-457.719099	-15.363782	0.615590
-461.086613	-24.476280	0.620595
-465.284556	-3.059572	0.625600
-469.009017	-9.117505	0.630605
-472.951568	-8.629861	0.635610
-476.792679	-10.026958	0.640614
-480.272214	-21.062619	0.645619
-484.058526	-4.888358	0.650624
-487.700046	-4.954929	0.655629
-491.482739	-14.716963	0.660634
-495.495826	-13.899497	0.665638
-499.000091	-14.814230	0.670643
-502.845522	-13.367567	0.675648
-506.626135	-7.263828	0.680653
-510.457992	-1.587102	0.685658
-514.376006	-7.000661	0.690662
-517.876573	-2.953668	0.695667
-522.002943	-7.707934	0.700672
-525.573180	-9.018914	0.705677
-529.190886	-7.927101	0.710682
-533.041640	1.738910	0.715686
-536.716395	-6.968047	0.720691
-540.498077	-9.948209	0.725696
-544.845209	-7.869453	0.730701
-548.152969	-6.264189	0.735706
-551.896951	-9.633524	0.740710
-555.282077	-15.181011	0.745715
-559.125291	-10.858473	0.750720
-562.874945	-8.812048	0.755725
-566.706065	-7.804350	0.760730
-570.901178	-4.983490	0.765734
-574.313413	-16.345122	0.770739
-578.390967	-7.986279	0.775744
-582.267188	-10.024095	0.780749
-585.879188	-9.030871	0.785754
-589.822165	-6.095726	0.790758
-593.226807	-8.644063	0.795763
-596.730003	2.664768	0.800768
-600.487024	-16.655198	0.805773
-604.474714	-10.030990	0.810778
-608.451732	-5.950328	0.815782
-611.745307	-11.119728	0.820787
-615.857790	1.894833	0.825792
-619.521288	-11.692497	0.830797
-623.162674	-8.543727	0.835802
-627.122261	-16.553793	0.840806
-630.816152	-11.688918	0.845811
-634.694459	-8.144338	0.850816
-638.317126	-14.380669	0.855821
-641.764143	-10.595926	0.860826
-645.889189	-8.828414	0.865830
-649.317726	-19.301144	0.870835
-653.557672	-7.921836	0.875840
-657.516300	-6.179317	0.880845
-660.908240	-5.686304	0.885850
-664.755317	-5.333437	0.890854
-668.211654	-14.423551	0.895859
-672.223157	-8.793561	0.900864
-676.084596	-11.797026	0.905869
-679.657476	-9.878005	0.910874
-683.589987	-8.625279	0.915878
-687.141231	-13.531063	0.920883
-691.167520	-15.109515	0.925888
-694.788416	-14.259773	0.930893
-698.421810	-10.184992	0.935898
-702.304030	-7.347674	0.940902
-705.996626	-8.454339	0.945907
-710.184907	-9.019779	0.950912
-713.818507	-16.170378	0.955917
-717.298647	-15.235870	0.960922
-721.243439	-8.250928	0.965926
-724.591787	-10.200989	0.970931
-728.405290	-7.751473	0.975936
-732.235271	-14.331386	0.980941
-736.189978	-8.704061	0.985946
-740.219280	-11.896618	0.990950
-743.597964	-17.151562	0.995955
-747.391570	2.387615	1.000960
-751.161364	-1.778304	1.005965
-754.852958	-13.224310	1.010970
-758.759565	-0.097358	1.015974
-762.526771	-8.890084	1.020979
-766.183399	-0.828420	1.025984
-770.102165	-11.449681	1.030989
-773.642539	-7.183089	1.035994
-777.745808	-8.727014	1.040998
-781.002469	-10.699532	1.046003
-784.882671	-9.521226	1.051008
-788.956765	-14.461546	1.056013
-792.878625	-4.684441	1.061018
-796.868181	1.729085	1.066022
-799.879692	-18.438171	1.071027
-803.609775	-2.335516	1.076032
-807.341594	-6.609905	1.081037
-811.367439	-1.843071	1.086042
-815.247872	-4.996221	1.091046
-818.607575	-1.819646	1.096051
-823.247052	-2.112507	1.101056
-826.727402	-4.829736	1.106061
-830.138599	-10.965533	1.111066
-833.783984	1.317173	1.116070
-837.488842	-16.847005	1.121075
-841.535456	2.559297	1.126080
-845.087454	-6.666628	1.131085
-848.923833	-6.717263	1.136090
-853.017873	-8.778152	1.141094
-856.328145	-20.450504	1.146099
-860.062827	-2.169440	1.151104
-864.192176	-7.479234	1.156109
-867.875561	-9.273035	1.161114
-871.811365	-5.127573	1.166118
-875.166269	-11.813153	1.171123
-879.224444	-8.409723	1.176128
-882.681757	-10.774186	1.181133
-886.462955	-11.029107	1.186138
-890.411676	-1.058335	1.191142
-894.142075	-15.769811	1.196147
-897.967005	-1.649695	1.201152
-901.872631	-8.895263	1.206157
-905.475229	-16.864149	1.211162
-909.191547	-4.702453	1.216166
-912.832090	-10.916565	1.221171
-917.004405	-3.332005	1.226176
-920.304568	-7.047648	1.231181
-923.603325	-1.792955	1.236186
-927.853118	-5.435595	1.241190
-931.750858	-15.908550	1.246195
-935.697301	-15.761686	1.251200
-939.396116	-6.836812	1.256205
-943.035830	-16.631972	1.261210
-946.823542	-11.571859	1.266214
-950.130288	-15.086147	1.271219
-954.262605	-15.062483	1.276224
-958.187462	-6.348998	1.281229
-961.849344	-15.834678	1.286234
-965.679372	-5.485411	1.291238
-969.044447	-16.095510	1.296243
-973.228079	-5.587194	1.301248
-976.961671	-6.847711	1.306253
-980.559827	-15.835814	1.311258
-984.252517	-9.314931	1.316262
-988.331884	-17.175904	1.321267
-992.400694	-5.511185	1.326272
-996.046202	-12.713034	1.331277
-999.366379	-10.955363	1.336282
-1003.235745	-6.243195	1.341286
-1006.951634	-0.090694	1.346291
-1010.780458	-8.961445	1.351296
-1014.505296	-13.263414	1.356301
-1018.110099	-12.977100	1.361306
-1021.690339	-2.264027	1.366310
-1025.715755	-7.222749	1.371315
-1029.738660	-8.484215	1.376320
-1033.438856	-13.960097	1.381325
-1036.926730	-22.007033	1.386330
-1041.391824	2.055048	1.391334
-1044.790151	-11.077267	1.396339
-1048.312112	0.137415	1.401344
-1051.803848	-11.166602	1.406349
-1055.294073	-12.437534	1.411354
-1059.402106	-1.340394	1.416358
-1062.932013	-13.978585	1.421363
-1067.309028	-2.687034	1.426368
-1071.205078	-9.126504	1.431373
-1074.572359	-14.513654	1.436378
-1078.956293	-1.857026	1.441382
-1082.329957	-8.208160	1.446387
-1085.818713	-9.193877	1.451392
-1089.541436	-3.568395	1.456397
-1093.325828	-4.120490	1.461402
-1097.535500	-8.701132	1.466406
-1100.921805	-9.737904	1.471411
-1104.871963	-3.170922	1.476416
-1108.100595	-7.977857	1.481421
-1112.005883	-2.133917	1.486426
-1116.702725	2.398595	1.491430
-1119.978160	-16.191712	1.496435
-1123.893290	2.695708	1.501440
-1127.779184	-6.712868	1.506445
-1130.889423	-9.960311	1.511450
-1134.807764	-8.802135	1.516454
-1138.368364	-4.531774	1.521459
-1142.534238	1.036964	1.526464
-1146.011031	-7.002120	1.531469
-1150.146192	-1.361019	1.536474
-1153.912350	-1.204786	1.541478
-1157.035314	-15.801686	1.546483
-1161.008463	-5.755625	1.551488
-1164.604881	-8.103716	1.556493
-1168.359943	-13.149586	1.561498
-1172.073700	-12.505009	1.566502
-1176.197704	-18.806903	1.571507
-1180.330256	-9.515835	1.576512
-1184.440936	-7.620387	1.581517
-1187.607760	-11.744871	1.586522
-1191.444814	-2.151006	1.591526
-1194.948324	-13.834495	1.596531
-1198.666815	-10.890116	1.601536
-1202.626570	-14.260131	1.606541
-1206.468928	-8.083940	1.611546
-1210.457913	-11.769360	1.616550
-1213.463084	-14.245091	1.621555
-1217.547557	-6.629926	1.626560
-1221.357960	-15.350301	1.631565
-1224.622166	-17.581158	1.636570
-1228.973071	-0.773060	1.641574
-1232.910423	-8.661043	1.646579
-1236.734783	-5.239231	1.651584
-1240.075701	-12.167749	1.656589
-1243.624435	-9.147971	1.661594
-1247.627870	-0.061935	1.666598
-1251.271623	-21.675762	1.671603
-1255.510887	2.394684	1.676608
-1259.350331	-5.513652	1.681613
-1262.823602	-5.411997	1.686618
-1266.501152	-12.806953	1.691622
-1269.730534	-6.454392	1.696627
-1273.960795	-2.360486	1.701632
-1277.856096	-6.175889	1.706637
-1281.856316	-10.004452	1.711642
-1285.575825	-10.068342	1.716646
-1288.582010	-13.103582	1.721651
-1292.663204	-5.487238	1.726656
-1296.633342	-12.862122	1.731661
-1300.259145	-9.665936	1.736666
-1304.332501	-4.838639	1.741670
-1308.025257	-7.970532	1.746675
-1311.637344	-0.755637	1.751680
-1315.367707	-8.523650	1.756685
-1319.123050	-14.712415	1.761690
-1322.967231	-11.227373	1.766694
-1326.827764	-11.935618	1.771699
-1330.423224	0.068591	1.776704
-1334.276917	-7.006349	1.781709
-1337.767416	-10.397628	1.786714
-1341.731839	-7.227595	1.791718
-1345.580246	-12.059548	1.796723
-1349.457022	4.415846	1.801728
-1353.141875	-9.855876	1.806733
-1356.653899	-7.751628	1.811738
-1360.498987	-1.120629	1.816742
-1364.137814	-19.057906	1.821747
-1368.288890	-1.338625	1.826752
-1371.752733	-8.445946	1.831757
-1375.394174	-13.419779	1.836762
-1379.458453	-19.798659	1.841766
-1383.120144	-11.954458	1.846771
-1387.173174	-3.427910	1.851776
-1390.810000	-7.416948	1.856781
-1394.386660	-15.002865	1.861786
-1398.306463	-8.698864	1.866790
-1401.561290	-15.618841	1.871795
-1405.595711	-8.878622	1.876800
-1408.940672	-6.383185	1.881805
-1413.081819	-13.558607	1.886810
-1417.012884	-5.067305	1.891814
-1420.452575	-15.131787	1.896819
-1424.192246	-5.007576	1.901824
-1428.088189	-9.144286	1.906829
-1431.975641	-11.396476	1.911834
-1436.064476	-10.497477	1.916838
-1439.614404	-5.621302	1.921843
-1443.755645	-6.230795	1.926848
-1447.174696	-7.602406	1.931853
-1450.663802	-9.459491	1.936858
-1454.903454	-8.419626	1.941862
-1457.950945	-6.903647	1.946867
-1462.198148	-1.321332	1.951872
-1465.771395	-6.069416	1.956877
-1469.304451	-7.257174	1.961882
-1473.229602	-8.639163	1.966886
-1476.969402	-9.229304	1.971891
-1481.065033	-12.742640	1.976896
-1484.525471	-21.395598	1.981901
-1488.708771	-6.925512	1.986906
-1492.422222	-0.630745	1.991910
-1495.762303	-18.924681	1.996915
-1499.596381	-14.392794	2.006912
-1500.984919	-4.047077	2.016909
-1498.633130	-8.988201	2.026906
-1495.370064	-8.893518	2.036902
-1493.231915	-10.598552	2.046899
-1491.513929	-7.176143	2.056896
-1489.696826	-2.078672	2.066893
-1487.656051	-6.698424	2.076890
-1485.663448	-5.080383	2.086886
-1484.084223	-8.659978	2.096883
-1482.153005	-5.039616	2.106880
-1480.419764	-11.133691	2.116877
-1478.011427	-12.488846	2.126874
-1476.196364	-7.640494	2.136870
-1474.336812	-11.853874	2.146867
-1472.532148	-3.314120	2.156864
-1470.850823	-9.496184	2.166861
-1468.680820	-5.367770	2.176858
-1466.588385	-14.845950	2.186854
-1464.804626	-9.686284	2.196851
-1462.951732	-12.054511	2.206848
-1461.315095	-4.995630	2.216845
-1459.313618	-12.526749	2.226842
-1457.561096	-20.619536	2.236838
-1455.556244	-18.594514	2.246835
-1453.425696	-10.159028	2.256832
-1451.619871	-13.842772	2.266829
-1450.070162	-10.914402	2.276826
-1447.727742	-14.759844	2.286822
-1445.948752	-16.535213	2.296819
-1444.147953	-13.653358	2.306816
-1442.216590	-6.867424	2.316813
-1440.516726	-13.780277	2.326810
-1438.565656	-13.680699	2.336806
-1436.828687	-13.554734	2.346803
-1434.864961	-17.961591	2.356800
-1432.861960	-14.998424	2.366797
-1431.009518	-11.090690	2.376794
-1429.152604	-13.914239	2.386790
-1427.076083	-20.134281	2.396787
-1425.407841	-10.410627	2.406784
-1423.475233	-13.568372	2.416781
-1421.594153	-10.304642	2.426778
-1419.862879	-16.982526	2.436774
-1417.859636	-10.369120	2.446771
-1416.227738	-18.303632	2.456768
-1413.907068	-1.584399	2.466765
-1412.146430	-5.192992	2.476762
-1410.321582	-8.827651	2.486758
-1408.576350	-10.892830	2.496755
-1406.235445	-7.596921	2.506752
-1404.973604	-14.884856	2.516749
-1402.951115	-13.970952	2.526746
-1400.856932	-17.110337	2.536742
-1398.911413	-12.505423	2.546739
-1397.210416	-11.720032	2.556736
-1395.258957	-17.242708	2.566733
-1393.589125	-20.209949	2.576730
-1391.508103	-16.537709	2.586726
-1389.505174	-13.607648	2.596723
-1387.981016	-18.179343	2.606720
-1386.103114	-12.921008	2.616717
-1384.057753	-10.940297	2.626714
-1381.998484	-16.608107	2.636710
-1380.289104	-6.287883	2.646707
-1378.263652	-11.678719	2.656704
-1376.314722	-20.208654	2.666701
-1374.532361	-17.014339	2.676698
-1372.799203	-17.034547	2.686694
-1371.084013	-11.675946	2.696691
-1369.097033	-12.038341	2.706688
-1367.096125	-4.276697	2.716685
-1365.246942	-18.237640	2.726682
-1363.449644	-22.843570	2.736678
-1361.329653	-11.788594	2.746675
-1359.340990	-18.108193	2.756672
-1358.086911	-11.692155	2.766669
-1355.937672	-15.629733	2.776666
-1353.979019	-17.687985	2.786662
-1351.988141	-16.241644	2.796659
-1350.488511	-14.558783	2.806656
-1348.354813	-10.557062	2.816653
-1346.501534	-23.004541	2.826650
-1344.510058	-16.201304	2.836646
-1342.810895	-16.359722	2.846643
-1340.826440	-20.714561	2.856640
-1338.962893	-10.853161	2.866637
-1336.732504	-25.366115	2.876634
-1335.275625	-15.782229	2.886630
-1333.267647	-11.815630	2.896627
-1331.406278	-19.153705	2.906624
-1329.827863	-16.068805	2.916621
-1327.617041	-12.846723	2.926618
-1325.703456	-23.769212	2.936614
-1324.059931	-19.501132	2.946611
-1322.375271	-16.715844	2.956608
-1320.226655	-18.766581	2.966605
-1318.141069	-17.692186	2.976602
-1316.390770	-20.588575	2.986598
-1314.535676	-19.248354	2.996595
-1312.546040	-22.250937	3.006592
-1310.908824	-17.887106	3.016589
-1308.860008	-10.729879	3.026586
-1306.941578	-13.959466	3.036582
-1305.347815	-22.705640	3.046579
-1303.270237	-11.549085	3.056576
-1301.227366	-17.087896	3.066573
-1299.319756	-12.257367	3.076570
-1297.848790	-12.395018	3.086566
-1296.081209	-10.628699	3.096563
-1293.784577	-13.640931	3.106560
-1291.911432	-5.075666	3.116557
-1290.006855	-6.378422	3.126554
-1288.328843	-13.496084	3.136550
-1286.439191	-12.783432	3.146547
-1284.744167	-9.106151	3.156544
-1282.851769	-12.470491	3.166541
-1280.476401	-21.264377	3.176538
-1278.676537	-14.503038	3.186534
-1277.065314	-12.654843	3.196531
-1275.103432	-15.272455	3.206528
-1273.545626	-9.067592	3.216525
-1271.552179	-15.626292	3.226522
-1269.328161	-16.212839	3.236518
-1267.702462	-16.645214	3.246515
-1265.855160	-16.989903	3.256512
-1263.562513	-7.029746	3.266509
-1261.832746	-14.146200	3.276506
-1260.083972	-13.521500	3.286502
-1258.203068	-1.332434	3.296499
-1256.398252	-5.230596	3.306496
-1254.513227	-16.236884	3.316493
-1252.710840	-12.723593	3.326490
-1250.460647	-13.514822	3.336486
-1249.130330	-11.405353	3.346483
-1247.237748	-10.571566	3.356480
-1245.031921	-17.006348	3.366477
-1243.265278	-12.671070	3.376474
-1241.241957	-13.858587	3.386470
-1239.242763	-6.431262	3.396467
-1237.758261	-10.172370	3.406464
-1235.870284	-9.400991	3.416461
-1233.941825	-15.153528	3.426458
-1231.962296	-9.395040	3.436454
-1229.956005	-16.143644	3.446451
-1228.011668	-19.037864	3.456448
-1226.368604	-13.312367	3.466445
-1224.516474	-10.299609	3.476442
-1222.852564	-11.745366	3.486438
-1220.646360	-8.356660	3.496435
-1218.699471	-14.896817	3.506432
-1216.941170	-7.088317	3.516429
-1214.875461	-14.638995	3.526426
-1212.984614	-16.468402	3.536422
-1211.364223	-8.952020	3.546419
-1209.679895	-10.634703	3.556416
-1207.500136	-13.077137	3.566413
-1205.645376	-11.187338	3.576410
-1203.886506	-13.698203	3.586406
-1201.874869	-13.249719	3.596403
-1200.144228	-6.996672	3.606400
-1198.487120	-7.378765	3.616397
-1196.703891	-4.034453	3.626394
-1194.192788	-6.586731	3.636390
-1192.487432	-11.774630	3.646387
-1190.587681	-5.880188	3.656384
-1188.433578	-11.553540	3.666381
-1187.252847	-7.025002	3.676378
-1185.113629	-8.321008	3.686374
-1183.324132	-4.440883	3.696371
-1181.217749	-11.892261	3.706368
-1179.318184	-10.323797	3.716365
-1177.568611	-9.141831	3.726362
-1175.491494	-18.372606	3.736358
-1173.876382	-20.377324	3.746355
-1172.133205	-11.822736	3.756352
-1170.093669	-16.334662	3.766349
-1168.122605	-5.942447	3.776346
-1166.017481	-9.877537	3.786342
-1164.342335	-12.543914	3.796339
-1162.706908	-9.794834	3.806336
-1160.765675	-3.952788	3.816333
-1158.893321	-9.391578	3.826330
-1156.711781	-8.310282	3.836326
-1154.741131	-11.579681	3.846323
-1153.250908	-9.059978	3.856320
-1151.311488	-6.335840	3.866317
-1149.397157	-8.178428	3.876314
-1147.678402	-13.248448	3.886310
-1145.766378	-6.639137	3.896307
-1143.794919	-8.435599	3.906304
-1141.885459	-16.119105	3.916301
-1140.041146	-11.526187	3.926298
-1137.829037	-13.629546	3.936294
-1136.031964	-11.667307	3.946291
-1134.423575	-7.579761	3.956288
-1132.535518	-6.977246	3.966285
-1130.582013	-10.485445	3.976282
-1128.816902	-15.968629	3.986278
-1126.907634	-7.178484	3.996275
-1124.792389	-9.555263	4.006272
-1123.302550	-9.563200	4.016269
-1121.546893	-5.437628	4.026266
-1119.176344	-11.996541	4.036262
-1117.346001	-16.179715	4.046259
-1115.594866	-3.857659	4.056256
-1113.824408	-17.119053	4.066253
-1111.884752	-10.165210	4.076250
-1110.065062	-15.099781	4.086246
-1107.946099	-10.493933	4.096243
-1106.243077	-6.696222	4.106240
-1104.614319	-8.519932	4.116237
-1102.439067	-2.557383	4.126234
-1100.278620	-15.529073	4.136230
-1098.757770	-14.561495	4.146227
-1097.378565	-8.514235	4.156224
-1095.011024	-12.254413	4.166221
-1092.848843	-13.037728	4.176218
-1091.056341	-15.348642	4.186214
-1089.362866	-16.230652	4.196211
-1087.804716	-13.090235	4.206208
-1085.579248	-15.748276	4.216205
-1083.599743	-13.668345	4.226202
-1081.849049	-13.358005	4.236198
-1079.775232	-13.950344	4.246195
-1078.320441	-13.655824	4.256192
-1076.201015	-18.679364	4.266189
-1074.068753	-11.412108	4.276186
-1072.402728	-13.004930	4.286182
-1070.376363	-19.456639	4.296179
-1068.806965	-26.904126	4.306176
-1066.859006	-15.620818	4.316173
-1064.777053	-22.068781	4.326170
-1063.340629	-16.834283	4.336166
-1061.306435	-15.424614	4.346163
-1059.082188	-16.735685	4.356160
-1057.472315	-14.604504	4.366157
-1055.927616	-9.977803	4.376154
-1053.510897	-23.659867	4.386150
-1051.666238	-24.914954	4.396147
-1049.748488	-18.642771	4.406144
-1048.050696	-17.902395	4.416141
-1046.576582	-17.069403	4.426138
-1044.390822	-16.956506	4.436134
-1042.349296	-12.780286	4.446131
-1040.267858	-15.389987	4.456128
-1038.634583	-14.217735	4.466125
-1036.867142	-11.507044	4.476122
-1034.894196	-5.628907	4.486118
-1033.091441	-10.020752	4.496115
-1031.326477	-15.628573	4.506112
-1029.254978	-16.312069	4.516109
-1027.592418	-19.061595	4.526106
-1025.684673	-17.794292	4.536102
-1023.555211	-14.726255	4.546099
-1021.792044	-16.186167	4.556096
-1020.054047	-17.267866	4.566093
-1018.040932	-16.985237	4.576090
-1016.193289	-18.310244	4.586086
-1014.051010	-18.566128	4.596083
-1012.558594	-19.250150	4.606080
-1010.572583	-19.173167	4.616077
-1008.656323	-9.684606	4.626074
-1006.768165	-18.536105	4.636070
-1004.929513	-18.178200	4.646067
-1002.992750	-14.018345	4.656064
-1000.885474	-14.546496	4.666061
-999.565041	-6.816199	4.676058
-997.304145	-14.432652	4.686054
-995.736550	-14.099281	4.696051
-993.960226	-5.635098	4.706048
-991.753026	-9.783717	4.716045
-989.826261	-14.553758	4.726042
-988.079127	-15.390596	4.736038
-986.011148	-13.312097	4.746035
-984.039212	-4.683410	4.756032
-982.366663	-8.242872	4.766029
-980.706519	-17.362607	4.776026
-978.750723	-12.203210	4.786022
-976.705823	-15.166990	4.796019
-974.656814	-15.769479	4.806016
-972.825713	-16.670256	4.816013
-971.075128	-16.277715	4.826010
-969.491705	-15.035867	4.836006
-967.439968	-22.031514	4.846003
-965.505992	-21.305162	4.856000
-963.514009	-16.945696	4.865997
-961.563487	-13.144823	4.875994
-959.891626	-22.525346	4.885990
-958.271163	-21.082585	4.895987
-956.237393	-21.313172	4.905984
-954.254678	-10.006889	4.915981
-952.260419	-17.362785	4.925978
-950.418595	-19.375185	4.935974
-948.466589	-19.951087	4.945971
-946.783344	-12.160360	4.955968
-944.844668	-19.291059	4.965965
-943.086259	-11.862850	4.975962
-941.410269	-13.706631	4.985958
-938.969023	-13.628171	4.995955
-937.299224	-8.449846	5.005952
-935.453267	-11.511248	5.015949
-933.692475	-1.391479	5.025946
-931.965707	-12.882211	5.035942
-929.982684	-2.677980	5.045939
-927.873752	-9.951150	5.055936
-925.849375	-12.283227	5.065933
-924.152207	-11.705280	5.075930
-922.270394	-16.337037	5.085926
-920.517752	-9.447849	5.095923
-918.939026	-7.441054	5.105920
-916.817677	-12.505818	5.115917
-914.723484	-8.093178	5.125914
-912.870636	-12.551362	5.135910
-911.130057	-15.250130	5.145907
-909.068436	-11.372243	5.155904
-907.282239	-7.455054	5.165901
-905.291369	-14.647752	5.175898
-903.609909	-8.151353	5.185894
-901.643575	-12.248750	5.195891
-900.032357	-15.179443	5.205888
-897.979675	-14.565164	5.215885
-896.017701	-14.364248	5.225882
-894.066608	-11.052848	5.235878
-892.470507	-11.679166	5.245875
-890.685762	-13.745549	5.255872
-888.452168	-13.635416	5.265869
-886.727609	-9.855190	5.275866
-884.522576	-9.078952	5.285862
-882.983953	-20.072232	5.295859
-881.254632	-22.173955	5.305856
-879.389120	-13.338699	5.315853
-877.199051	-18.987533	5.325850
-875.291183	-14.428237	5.335846
-873.523542	-14.622522	5.345843
-871.635010	-17.300706	5.355840
-869.742615	-16.022926	5.365837
-867.840673	-12.080002	5.375834
-866.220862	-15.168353	5.385830
-864.429204	-12.496132	5.395827
-862.171168	-16.973266	5.405824
-860.282816	-9.354193	5.415821
-858.562199	-13.663312	5.425818
-856.488568	-18.126749	5.435814
-854.745992	-9.240239	5.445811
-852.919231	-13.117930	5.455808
-851.190484	-10.061456	5.465805
-849.297554	-1.803670	5.475802
-847.182398	-12.794369	5.485798
-845.296491	-19.441327	5.495795
-843.636180	-16.306018	5.505792
-841.640058	-14.059597	5.515789
-840.050194	-13.993348	5.525786
-837.950843	-16.675209	5.535782
-836.018278	-20.550853	5.545779
-834.158773	-19.907217	5.555776
-832.238714	-20.620014	5.565773
-830.261677	-18.485788	5.575770
-828.371458	-17.851794	5.585766
-826.717473	-13.340288	5.595763
-824.805256	-11.767237	5.605760
-822.907344	-11.674432	5.615757
-820.913390	-19.075964	5.625754
-819.129764	-24.014031	5.635750
-817.279585	-25.958195	5.645747
-815.552805	-15.513971	5.655744
-813.516850	-19.213504	5.665741
-811.648380	-20.660095	5.675738
-809.880719	-17.085634	5.685734
-807.671493	-19.398214	5.695731
-806.095642	-16.989856	5.705728
-804.100672	-16.980440	5.715725
-802.353927	-18.192845	5.725722
-800.321522	-10.083620	5.735718
-798.330998	-11.748644	5.745715
-796.671230	-12.956615	5.755712
-794.699027	-20.971978	5.765709
-793.075457	-10.010740	5.775706
-790.964010	-11.511939	5.785702
-788.932596	-12.616685	5.795699
-787.383426	-13.398052	5.805696
-785.582807	-16.493144	5.815693
-783.545593	-6.711095	5.825690
-781.410758	-18.979012	5.835686
-779.785873	-8.527939	5.845683
-777.535632	-13.553189	5.855680
-775.837763	-15.886637	5.865677
-774.117163	-13.537704	5.875674
-772.645329	-14.136186	5.885670
-769.963079	-10.216844	5.895667
-768.409064	-11.878390	5.905664
-766.687324	-15.988691	5.915661
-765.047086	-10.186602	5.925658
-762.705735	-20.924451	5.935654
-761.012436	-23.361361	5.945651
-759.200286	-20.146054	5.955648
-757.262017	-21.063792	5.965645
-755.501184	-24.311965	5.975642
-753.410855	-27.074410	5.985638
-751.402411	-25.445630	5.995635
-749.761737	-24.890105	6.005632
-747.978616	-20.209718	6.015629
-746.145737	-20.018044	6.025626
-743.775736	-21.096340	6.035622
-742.254461	-21.536926	6.045619
-740.323976	-16.374852	6.055616
-738.271475	-17.647124	6.065613
-736.739177	-12.694552	6.075610
-735.262261	-21.552765	6.085606
-732.617938	-18.839873	6.095603
-730.716113	-10.354475	6.105600
-729.263868	-14.720085	6.115597
-727.079264	-13.026282	6.125594
-725.237530	-19.681882	6.135590
-723.341911	-21.176950	6.145587
-721.838589	-16.039749	6.155584
-719.800887	-12.765722	6.165581
-717.888401	-14.029812	6.175578
-715.862440	-14.866799	6.185574
-713.851762	-24.272896	6.195571
-712.211444	-18.772343	6.205568
-710.011403	-25.355722	6.215565
-708.608177	-23.532304	6.225562
-706.603447	-23.753298	6.235558
-704.639918	-26.275979	6.245555
-702.909735	-24.754262	6.255552
-701.005029	-21.176354	6.265549
-699.389619	-22.906083	6.275546
-697.232853	-24.698633	6.285542
-695.034469	-19.822470	6.295539
-693.530745	-23.338970	6.305536
-691.185618	-19.460400	6.315533
-689.704992	-19.692364	6.325530
-687.787815	-16.373789	6.335526
-685.797454	-24.882991	6.345523
-684.375940	-14.910896	6.355520
-682.223541	-18.256321	6.365517
-680.611771	-12.885382	6.375514
-678.291069	-21.756818	6.385510
-676.376727	-19.992944	6.395507
-674.746600	-21.541862	6.405504
-672.825602	-16.334005	6.415501
-670.895023	-14.594824	6.425498
-669.011408	-16.230028	6.435494
-667.139094	-23.929353	6.445491
-665.420651	-8.731336	6.455488
-663.283477	-15.418311	6.465485
-661.315723	-15.990179	6.475482
-659.688770	-23.438730	6.485478
-657.743242	-23.263407	6.495475
-655.986585	-21.755357	6.505472
-654.189841	-21.036818	6.515469
-652.239552	-15.719946	6.525466
-650.270051	-26.014622	6.535462
-648.408521	-14.510275	6.545459
-646.545461	-15.065403	6.555456
-644.467363	-18.578912	6.565453
-642.993768	-17.112463	6.575450
-640.855186	-9.463706	6.585446
-638.756161	-20.086948	6.595443
-637.079280	-15.924725	6.605440
-635.369420	-20.119874	6.615437
-633.250419	-20.516947	6.625434
-631.182916	-22.323596	6.635430
-629.896332	-24.660703	6.645427
-627.807460	-22.072095	6.655424
-626.142939	-20.977170	6.665421
-624.388001	-22.315482	6.675418
-621.972917	-17.314404	6.685414
-620.172271	-26.671087	6.695411
-618.314783	-24.269701	6.705408
-616.512594	-16.316146	6.715405
-614.626867	-12.589877	6.725402
-612.764999	-16.701933	6.735398
-610.777306	-21.835078	6.745395
-608.733445	-21.512802	6.755392
-607.264833	-19.207167	6.765389
-605.495630	-23.418089	6.775386
-603.329921	-15.546278	6.785382
-601.310191	-21.292390	6.795379
-599.642485	-19.604308	6.805376
-597.610086	-23.661494	6.815373
-595.856778	-19.487768	6.825370
-594.050888	-20.327388	6.835366
-592.134844	-17.992173	6.845363
-590.124787	-21.046374	6.855360
-588.567151	-21.180058	6.865357
-586.450239	-17.230188	6.875354
-584.407311	-19.795455	6.885350
-582.594502	-25.978993	6.895347
-581.090221	-12.418693	6.905344
-578.938473	-23.135566	6.915341
-577.406053	-25.227723	6.925338
-575.252521	-25.096611	6.935334
-573.127539	-25.696679	6.945331
-571.744269	-25.595670	6.955328
-569.544732	-21.613197	6.965325
-567.778826	-12.692284	6.975322
-565.759004	-18.948352	6.985318
-564.165666	-13.992778	6.995315
-561.979948	-23.133057	7.005312
-560.019092	-21.888064	7.015309
-558.409298	-19.732836	7.025306
-556.485400	-17.469894	7.035302
-554.399953	-21.323953	7.045299
-552.523887	-17.469782	7.055296
-551.105668	-19.812086	7.065293
-549.087320	-24.657991	7.075290
-547.244064	-17.473521	7.085286
-545.144880	-17.436325	7.095283
-543.183762	-24.761350	7.105280
-541.616932	-18.374248	7.115277
-539.490369	-16.847830	7.125274
-537.737189	-19.830960	7.135270
-535.798799	-19.472829	7.145267
-533.723492	-18.463975	7.155264
-532.053673	-19.856516	7.165261
-530.075362	-18.658493	7.175258
-528.385121	-20.324276	7.185254
-526.533518	-20.436982	7.195251
-524.513088	-20.504025	7.205248
-522.893074	-22.138063	7.215245
-520.831728	-21.689038	7.225242
-518.763564	-20.505357	7.235238
-517.313571	-27.581368	7.245235
-515.144066	-21.958359	7.255232
-513.267751	-22.501291	7.265229
-511.254261	-21.528331	7.275226
-509.882309	-15.501635	7.285222
-507.765330	-21.908954	7.295219
-505.410296	-20.493201	7.305216
-503.890325	-25.644712	7.315213
-502.048950	-13.393374	7.325210
-500.192942	-11.031125	7.335206
-498.461052	-21.338271	7.345203
-496.352581	-19.464735	7.355200
-494.590500	-20.346228	7.365197
-492.546285	-23.855776	7.375194
-490.955056	-22.884831	7.385190
-488.922016	-16.718979	7.395187
-487.089503	-22.544042	7.405184
-484.901713	-18.136478	7.415181
-483.287640	-17.352322	7.425178
-481.452219	-18.889689	7.435174
-479.503078	-18.831631	7.445171
-477.431389	-23.198134	7.455168
-476.074232	-12.568283	7.465165
-473.976326	-22.288116	7.475162
-472.029780	-18.126206	7.485158
-470.424090	-19.086911	7.495155
-468.119019	-20.517702	7.505152
-466.286801	-13.198774	7.515149
-464.441632	-21.790410	7.525146
-462.469798	-22.659589	7.535142
-460.968479	-23.267325	7.545139
-459.089524	-16.806856	7.555136
-456.878163	-17.995318	7.565133
-455.126183	-12.543977	7.575130
-453.305682	-16.579841	7.585126
-451.413085	-12.249833	7.595123
-449.243399	-13.774243	7.605120
-447.516406	-18.066732	7.615117
-445.730896	-16.686280	7.625114
-444.191531	-10.957836	7.635110
-442.037469	-8.220003	7.645107
-439.956382	-17.332426	7.655104
-438.174056	-23.215753	7.665101
-436.670345	-19.666742	7.675098
-434.553696	-12.716869	7.685094
-432.356379	-16.479751	7.695091
-430.665014	-20.338671	7.705088
-428.883282	-20.226999	7.715085
-426.835669	-13.820273	7.725082
-425.130131	-14.545854	7.735078
-423.329471	-18.498006	7.745075
-421.544742	-20.320900	7.755072
-419.439969	-10.921897	7.765069
-417.659979	-18.958392	7.775066
-415.733782	-14.512148	7.785062
-413.973867	-10.429327	7.795059
-412.097749	-24.348177	7.805056
-410.012816	-18.953125	7.815053
-408.158119	-21.153474	7.825050
-406.202197	-14.976811	7.835046
-404.583307	-21.209786	7.845043
-402.630341	-23.946843	7.855040
-400.511629	-16.818859	7.865037
-398.804786	-23.891612	7.875034
-397.121294	-18.827163	7.885030
-394.907114	-22.665330	7.895027
-393.235653	-13.997596	7.905024
-391.370476	-19.456778	7.915021
-389.518308	-24.768625	7.925018
-387.811883	-22.410825	7.935014
-385.741717	-27.124356	7.945011
-383.792124	-19.415179	7.955008
-382.043647	-18.166126	7.965005
-380.065612	-15.480654	7.975002
-378.188572	-16.569879	7.984998
-376.480379	-14.210772	7.994995
-374.412856	-14.642027	8.004992
-372.422898	-16.365028	8.014989
-370.683735	-14.247690	8.024986
-368.887988	-13.274578	8.034982
-366.895211	-15.462208	8.044979
-365.266373	-11.509992	8.054976
-363.252075	-19.258615	8.064973
-361.240124	-18.501584	8.074970
-359.462886	-16.245061	8.084966
-357.691389	-12.606124	8.094963
-355.441412	-12.051289	8.104960
-353.483560	-16.156375	8.114957
-351.960831	-12.952953	8.124954
-350.133963	-14.613586	8.134950
-348.180455	-10.788975	8.144947
-346.226945	-13.050841	8.154944
-344.131875	-16.486288	8.164941
-342.592771	-19.539310	8.174938
-340.993101	-13.825157	8.184934
-338.961690	-18.736138	8.194931
-336.916522	-18.702766	8.204928
-335.069726	-19.589773	8.214925
-333.276117	-15.848565	8.224922
-330.952146	-10.308449	8.234918
-329.443838	-21.621842	8.244915
-327.898133	-16.023796	8.254912
-325.673067	-21.063568	8.264909
-323.483780	-19.643277	8.274906
-321.874555	-21.916474	8.284902
-320.143743	-13.463406	8.294899
-317.974353	-20.982557	8.304896
-316.184044	-19.234901	8.314893
-314.471145	-23.981338	8.324890
-312.465787	-19.433966	8.334886
-310.601199	-9.968095	8.344883
-309.080280	-13.059245	8.354880
-306.941929	-21.081823	8.364877
-305.124724	-15.714983	8.374874
-303.307737	-18.562880	8.384870
-301.397096	-18.594841	8.394867
-299.003061	-22.701619	8.404864
-297.289790	-16.631381	8.414861
-296.082877	-23.130087	8.424858
-293.798513	-16.641037	8.434854
-291.711817	-18.358890	8.444851
-290.117291	-19.829242	8.454848
-288.026860	-16.080117	8.464845
-286.338222	-19.060663	8.474842
-284.616884	-16.373607	8.484838
-282.556257	-17.607319	8.494835
-280.610128	-21.892044	8.504832
-278.732500	-19.218879	8.514829
-276.722219	-18.834119	8.524826
-275.057529	-13.510800	8.534822
-273.130949	-16.210389	8.544819
-271.035914	-20.245733	8.554816
-269.335161	-19.170547	8.564813
-267.762987	-19.467387	8.574810
-265.727431	-19.099282	8.584807
-263.536244	-20.240140	8.594803
-262.074889	-18.091010	8.604800
-260.040569	-14.487631	8.614797
-258.039975	-21.059319	8.624794
-256.229202	-22.071562	8.634791
-254.704566	-22.463431	8.644787
-252.399292	-24.464016	8.654784
-250.727239	-24.915724	8.664781
-248.832461	-24.263047	8.674778
-246.713763	-21.849372	8.684775
-244.918574	-19.860875	8.694771
-243.199056	-23.389446	8.704768
-240.978193	-23.527710	8.714765
-239.309828	-18.167060	8.724762
-237.388418	-19.583766	8.734759
-235.796769	-24.265013	8.744755
-233.785856	-23.823479	8.754752
-231.797600	-20.899527	8.764749
-229.806683	-30.548411	8.774746
-227.796821	-23.464467	8.784743
-226.390687	-26.590927	8.794739
-224.306500	-30.215576	8.804736
-222.190301	-28.313029	8.814733
-220.881514	-20.029360	8.824730
-218.663652	-28.533472	8.834727
-216.886752	-31.368592	8.844723
-214.884286	-32.405080	8.854720
-213.076085	-24.922647	8.864717
-211.299214	-25.143176	8.874714
-209.300218	-20.790476	8.884711
-207.467921	-31.293452	8.894707
-205.289512	-31.207026	8.904704
-204.107321	-27.169210	8.914701
-202.100167	-30.099482	8.924698
-200.004906	-25.370582	8.934695
-198.011931	-25.126670	8.944691
-196.028000	-27.086973	8.954688
-194.382038	-26.165613	8.964685
-192.356052	-31.632943	8.974682
-190.474790	-25.156828	8.984679
-188.676279	-29.470026	8.994675
-186.997559	-27.728148	9.004672
-184.777394	-27.799937	9.014669
-183.366870	-28.277755	9.024666
-181.466722	-28.127958	9.034663
-179.165689	-25.405443	9.044659
-177.319075	-25.048164	9.054656
-175.671047	-25.671240	9.064653
-173.979533	-18.512762	9.074650
-171.739056	-14.656429	9.084647
-169.893853	-25.500898	9.094643
-167.921921	-20.900700	9.104640
-166.209079	-22.584051	9.114637
-164.374989	-17.699763	9.124634
-162.601442	-13.097899	9.134631
-160.468428	-17.957061	9.144627
-158.724612	-14.869310	9.154624
-156.690159	-17.590759	9.164621
-154.975029	-18.833967	9.174618
-152.984358	-17.730752	9.184615
-151.107091	-19.061404	9.194611
-149.202864	-14.554588	9.204608
-147.544309	-18.310197	9.214605
-145.646508	-26.082694	9.224602
-143.531459	-21.713720	9.234599
-141.873416	-14.763019	9.244595
-139.930535	-19.512883	9.254592
-137.898039	-17.593745	9.264589
-136.259899	-19.661449	9.274586
-134.436814	-10.964020	9.284583
-132.568696	-20.124326	9.294579
-130.389034	-18.797052	9.304576
-128.465387	-12.559733	9.314573
-126.754797	-13.724833	9.324570
-124.981281	-9.522384	9.334567
-123.135458	-9.251774	9.344563
-121.232705	-14.165739	9.354560
-119.168288	-13.511605	9.364557
-117.643799	-14.915412	9.374554
-115.545580	-15.049781	9.384551
-113.736816	-18.590927	9.394547
-111.605387	-16.149161	9.404544
-109.820545	-17.742914	9.414541
-107.889903	-15.501201	9.424538
-106.263338	-8.051266	9.434535
-104.316617	-5.534235	9.444531
-102.540602	-10.791104	9.454528
-100.345219	-10.416782	9.464525
-98.733908	-11.640230	9.474522
-96.777154	-11.872006	9.484519
-94.742800	-10.516779	9.494515
-93.412468	-13.266359	9.504512
-91.351118	-20.804402	9.514509
-89.271121	-12.335806	9.524506
-87.180997	-9.334827	9.534503
-85.400973	-12.943996	9.544499
-83.644589	-7.717260	9.554496
-81.950897	-14.315642	9.564493
-79.930144	-20.247817	9.574490
-77.915781	-13.994929	9.584487
-76.226056	-9.558034	9.594483
-74.171761	-13.364100	9.604480
-72.340599	-15.577813	9.614477
-70.476697	-15.772652	9.624474
-68.466646	-22.416754	9.634471
-66.847151	-20.701653	9.644467
-64.950038	-17.050953	9.654464
-63.042417	-13.310352	9.664461
-61.292900	-16.875165	9.674458
-59.395223	-18.868966	9.684455
-57.581091	-20.761021	9.694451
-55.247315	-18.866191	9.704448
-53.596216	-15.649893	9.714445
-51.545377	-7.535007	9.724442
-50.004502	-5.538946	9.734439
-48.069837	-15.417144	9.744435
-46.089289	-17.375210	9.754432
-44.281141	-16.062798	9.764429
-42.495085	-9.495577	9.774426
-40.413685	-15.478449	9.784423
-38.872879	-14.406002	9.794419
-36.751536	-13.249328	9.804416
-34.726250	-15.160841	9.814413
-32.882288	-15.041435	9.824410
-31.078708	-11.443675	9.834407
-29.405320	-13.275368	9.844403
-27.383731	-14.325806	9.854400
-25.196229	-17.287865	9.864397
-23.604636	-15.486183	9.874394
-21.591324	-8.773626	9.884391
-19.979012	-12.493359	9.894387
-18.036778	-12.275939	9.904384
-16.272048	-8.484086	9.914381
-14.004022	-12.748909	9.924378
-12.363890	-14.240567	9.934375
-10.422570	-7.552830	9.944371
-8.422071	-19.211401	9.954368
-6.810296	-10.810138	9.964365
-5.153743	-7.552044	9.974362
-3.602712	16.754895	9.984359
-2.523480	53.005464	9.994355
-0.963023	107.320600	10.004352
0.000000	156.309983	10.009357
0.535556	178.924980	10.014362
1.223402	227.321117	10.019367
1.762215	253.600349	10.024371
2.248549	274.709553	10.029376
2.887627	290.228061	10.034381
2.879657	307.904459	10.039386
3.195199	307.951839	10.044391
3.281560	312.804246	10.049395
2.912736	318.769995	10.054400
3.194976	318.951991	10.059405
3.594769	339.862215	10.064410
3.592800	349.672238	10.069415
3.895320	354.725137	10.074419
3.853743	359.495468	10.079424
3.825344	362.712048	10.084429
3.927407	365.866820	10.089434
3.876708	367.275121	10.094439
3.981103	365.670494	10.099443
4.104078	370.280548	10.104448
3.858051	364.475809	10.109453
3.962153	370.678370	10.114458
3.899671	380.121190	10.119463
4.503318	373.237949	10.124467
4.110474	376.315550	10.129472
4.331922	379.011334	10.134477
4.564557	379.486659	10.139482
4.345045	372.782018	10.144487
4.470332	377.573047	10.149491
4.280947	392.728665	10.154496
4.294587	394.844189	10.159501
4.490130	381.559233	10.164506
4.247271	395.499722	10.169511
4.277888	389.078440	10.174515
4.636098	384.624896	10.179520
4.505922	398.441764	10.184525
4.541216	389.843634	10.189530
4.652345	403.811244	10.194535
4.586762	403.222432	10.199539
4.432969	411.091913	10.204544
4.906963	417.774791	10.209549
5.339801	425.446638	10.214554
5.029285	430.203121	10.219559
5.159821	429.494720	10.224563
5.390228	427.212425	10.229568
5.199834	418.118864	10.234573
4.932320	410.499383	10.239578
4.779302	417.193964	10.244583
5.217483	430.270531	10.249587
5.163578	436.536167	10.254592
5.403300	434.868949	10.259597
5.424021	437.303458	10.264602
5.176120	444.153528	10.269607
5.283773	436.385888	10.274611
5.316069	443.375763	10.279616
5.254897	434.876567	10.284621
5.671704	441.063973	10.289626
5.575777	443.491859	10.294631
5.787814	445.722396	10.299635
5.601642	442.505218	10.304640
5.626927	438.024338	10.309645
5.888411	450.026861	10.314650
5.572960	452.439302	10.319655
5.955294	455.626659	10.324659
6.007844	461.388067	10.329664
5.873280	460.985289	10.334669
6.062861	467.782938	10.339674
6.310684	477.163713	10.344679
6.239177	473.275405	10.349683
6.030707	471.930395	10.354688
6.056172	478.224389	10.359693
6.412185	483.245147	10.364698
6.266813	488.170842	10.369703
6.404926	480.895042	10.374707
6.570034	498.998214	10.379712
6.382878	484.996794	10.384717
6.724690	495.578376	10.389722
6.322711	498.985454	10.394727
6.328284	487.548863	10.399731
6.725846	505.717465	10.404736
6.466780	496.339928	10.409741
6.677803	502.563337	10.414746
6.694211	511.533207	10.419751
6.780722	496.523065	10.424755
6.944554	503.059919	10.429760
6.916406	491.165096	10.434765
7.055222	502.463434	10.439770
6.726335	509.272837	10.444775
6.903409	489.607451	10.449779
6.739117	504.787567	10.454784
6.813418	500.913841	10.459789
7.535185	502.877012	10.464794
7.048302	504.815351	10.469799
7.138555	498.865461	10.474803
7.119409	511.381134	10.479808
7.035416	509.227817	10.484813
7.102256	519.113710	10.489818
7.104793	522.096740	10.494823
7.633275	532.156583	10.499827
7.699938	537.400124	10.504832
7.761033	532.670662	10.509837
7.520328	523.700172	10.514842
7.370218	512.482352	10.519847
7.553884	538.064992	10.524851
7.501445	538.424948	10.529856
7.882133	542.888300	10.534861
8.246160	539.457191	10.539866
7.972419	551.081558	10.544871
8.019141	538.670146	10.549875
7.625126	541.050978	10.554880
7.961372	541.659589	10.559885
8.052401	544.354129	10.564890
8.366716	543.826138	10.569895
8.162428	543.503863	10.574899
8.017477	558.835488	10.579904
7.956077	550.680025	10.584909
8.397416	547.943035	10.589914
8.199194	549.475805	10.594919
8.434902	547.760330	10.599923
8.666252	544.057078	10.604928
8.154328	549.561636	10.609933
8.487676	548.426657	10.614938
8.139467	559.957255	10.619943
8.376506	547.633748	10.624947
8.236857	552.478130	10.629952
8.427671	541.455060	10.634957
8.619287	554.995255	10.639962
8.304895	557.019625	10.644967
8.398781	563.977658	10.649971
8.417173	576.080558	10.654976
8.790078	586.203099	10.659981
9.043492	573.618345	10.664986
8.799291	588.353993	10.669991
9.009374	575.140656	10.674995
9.229925	570.617553	10.680000
9.213356	575.546388	10.685005
9.367060	582.703040	10.690010
9.347779	579.465519	10.695015
9.499139	574.217036	10.700019
9.286348	562.227029	10.705024
9.429107	554.053194	10.710029
9.225955	558.144486	10.715034
9.213553	559.213971	10.720039
9.511769	565.898148	10.725043
9.679760	584.549729	10.730048
9.545407	569.092207	10.735053
9.632402	561.944364	10.740058
9.391852	562.553514	10.745063
9.528682	581.774593	10.750067
9.261250	585.064039	10.755072
9.596598	595.632534	10.760077
9.499165	599.109328	10.765082
9.488920	596.911121	10.770087
9.538009	590.734377	10.775091
9.329269	600.836163	10.780096
9.475063	602.793448	10.785101
9.811538	616.566054	10.790106
9.870684	611.106768	10.795111
10.053575	630.505064	10.800115
10.206315	621.940101	10.805120
10.175236	634.123478	10.810125
10.172267	623.355176	10.815130
10.079157	632.557048	10.820135
10.540153	624.597336	10.825139
10.145168	639.481661	10.830144
10.439390	627.672500	10.835149
10.534468	621.780136	10.840154
10.681841	627.483910	10.845159
10.431390	634.500052	10.850163
10.409547	633.916868	10.855168
10.888084	627.613267	10.860173
11.137713	614.633277	10.865178
11.019337	632.655678	10.870183
10.879949	624.824841	10.875187
10.570704	626.408442	10.880192
10.741773	634.260921	10.885197
10.995330	619.011126	10.890202
10.689371	635.254735	10.895207
10.607468	634.838822	10.900211
11.016940	627.619013	10.905216
10.841554	636.278939	10.910221
11.063472	634.598769	10.915226
11.020634	629.002781	10.920231
11.069145	626.156549	10.925235
10.884887	629.847467	10.930240
10.879036	638.176009	10.935245
11.031837	634.430071	10.940250
11.190653	655.938994	10.945255
11.313248	654.998467	10.950259
11.838735	649.983590	10.955264
11.635941	660.890271	10.960269
11.715985	658.138349	10.965274
11.535097	653.040599	10.970279
11.584875	650.730311	10.975283
11.771214	658.769597	10.980288
11.765824	660.262161	10.985293
12.144378	655.704369	10.990298
11.513695	650.867591	10.995303
11.900268	652.570442	11.000307
11.972488	661.673425	11.005312
12.012341	649.851202	11.010317
12.003637	634.271070	11.015322
11.696686	631.145650	11.020327
12.177369	647.374189	11.025331
12.249916	657.210382	11.030336
12.218880	658.281269	11.035341
12.420324	654.483414	11.040346
12.288211	652.812402	11.045351
12.177642	638.137891	11.050355
11.995028	657.747481	11.055360
12.084328	653.246863	11.060365
12.419057	669.675321	11.065370
11.986641	668.843816	11.070375
12.387010	665.602419	11.075379
12.361809	671.335312	11.080384
12.128825	678.884840	11.085389
12.513801	668.280127	11.090394
12.444057	659.260208	11.095399
12.448670	660.326986	11.100403
12.742131	682.818967	11.105408
12.992318	694.776189	11.110413
13.338846	679.828463	11.115418
12.579034	685.284301	11.120423
12.765271	673.842401	11.125427
12.796408	673.999800	11.130432
13.043091	682.672857	11.135437
13.547679	692.150012	11.140442
13.290399	687.408202	11.145447
13.089288	669.985343	11.150451
13.532088	668.744590	11.155456
13.555290	666.194116	11.160461
13.676942	656.866135	11.165466
12.834197	666.455668	11.170471
12.912384	659.154645	11.175475
13.265462	671.106475	11.180480
13.044763	678.452198	11.185485
13.626569	681.404370	11.190490
13.592520	690.723013	11.195495
13.942251	688.109416	11.200499
14.050026	683.850265	11.205504
14.021828	684.302550	11.210509
13.565927	673.630105	11.215514
13.118847	669.235533	11.220519
13.598627	673.337778	11.225523
13.676350	683.923774	11.230528
13.359656	683.280386	11.235533
13.871162	684.731509	11.240538
13.965838	694.182584	11.245543
14.147888	690.313698	11.250547
14.068595	682.258783	11.255552
14.204516	696.728914	11.260557
14.351394	690.914990	11.265562
14.020383	694.777561	11.270567
14.040502	691.989459	11.275571
14.238141	685.367945	11.280576
14.335836	703.747048	11.285581
14.257229	684.833367	11.290586
14.053056	699.051821	11.295591
14.397001	701.523129	11.300595
14.336285	705.828283	11.305600
14.494117	722.698168	11.310605
14.926112	730.469661	11.315610
14.495662	734.013794	11.320615
14.615108	721.891818	11.325619
14.670657	725.568165	11.330624
14.789192	720.965094	11.335629
15.045672	728.302542	11.340634
14.784242	724.936457	11.345639
15.181479	711.723107	11.350643
14.968005	725.301264	11.355648
14.913446	727.642176	11.360653
15.219637	721.036447	11.365658
14.931318	728.949633	11.370663
15.058417	717.507670	11.375667
15.261508	724.724324	11.380672
15.083694	729.689967	11.385677
15.100422	719.765258	11.390682
14.974607	734.324479	11.395687
15.062379	727.231623	11.400691
15.000796	731.623653	11.405696
14.898364	736.531545	11.410701
15.186114	728.405448	11.415706
15.189809	752.957484	11.420711
15.684854	747.445969	11.425715
15.468147	758.556788	11.430720
15.968168	757.783134	11.435725
16.012942	758.146513	11.440730
15.968218	754.178164	11.445735
15.783243	740.532533	11.450739
15.957468	733.794885	11.455744
15.358406	732.573647	11.460749
15.782123	733.253470	11.465754
15.511079	756.724987	11.470759
15.938021	753.745834	11.475763
16.184567	754.043916	11.480768
16.051437	752.680554	11.485773
16.001035	746.267304	11.490778
15.880707	758.649521	11.495783
16.169373	746.685034	11.500787
16.496540	750.035796	11.505792
16.273498	751.104199	11.510797
16.792907	743.053106	11.515802
16.566856	746.224027	11.520807
16.598611	740.537253	11.525811
16.426192	752.055735	11.530816
16.186102	735.990436	11.535821
16.743794	736.221545	11.540826
16.249130	744.986074	11.545831
16.688997	753.114285	11.550835
16.556208	740.185715	11.555840
16.585464	748.105030	11.560845
16.594702	737.252695	11.565850
16.918710	738.027268	11.570855
16.782768	751.971546	11.575859
16.685514	750.260270	11.580864
17.045480	765.293966	11.585869
17.146997	765.610449	11.590874
17.226079	760.638350	11.595879
17.081540	748.326648	11.600883
17.133613	753.589941	11.605888
17.207168	755.765347	11.610893
17.412163	752.736439	11.615898
17.077121	756.557092	11.620903
17.460135	748.947212	11.625907
17.284873	750.041109	11.630912
17.251522	770.576353	11.635917
17.777430	755.139476	11.640922
17.583375	767.522422	11.645927
17.447991	748.704443	11.650931
17.842103	761.105535	11.655936
17.401977	751.061285	11.660941
17.896587	751.132149	11.665946
17.631890	762.526587	11.670951
17.639836	759.770376	11.675955
17.774855	768.246833	11.680960
17.883750	774.571804	11.685965
17.923098	772.110198	11.690970
17.755240	774.261033	11.695975
18.017349	769.396933	11.700979
17.989657	770.308025	11.705984
18.161241	774.941995	11.710989
18.130897	777.416244	11.715994
17.947243	786.315694	11.720999
18.099843	768.155067	11.726003
18.150477	780.510036	11.731008
18.149437	774.183516	11.736013
18.558107	768.214269	11.741018
17.669469	773.638647	11.746023
17.879293	773.114700	11.751027
17.936605	779.033169	11.756032
18.325628	789.328323	11.761037
18.774450	799.858371	11.766042
18.526273	796.039153	11.771047
18.852126	782.979047	11.776051
18.916214	793.362299	11.781056
18.966523	784.113422	11.786061
18.902376	776.428194	11.791066
18.856705	759.161781	11.796071
18.809265	769.127572	11.801075
18.656849	756.471772	11.806080
18.839444	765.290717	11.811085
18.780964	782.163635	11.816090
18.967639	783.573539	11.821095
19.112693	779.303683	11.826099
19.132435	781.998600	11.831104
19.212754	798.477245	11.836109
19.671657	790.054160	11.841114
19.431631	794.752209	11.846119
19.523407	779.141702	11.851123
19.425281	777.520446	11.856128
19.155684	766.873408	11.861133
19.243322	759.987135	11.866138
19.238596	782.569409	11.871143
19.098865	780.153710	11.876147
19.329419	787.506362	11.881152
19.139039	802.910145	11.886157
19.588261	785.832845	11.891162
19.468207	794.111885	11.896167
19.286754	788.624675	11.901171
19.643500	790.136763	11.906176
19.701287	800.246639	11.911181
19.832196	824.775354	11.916186
19.806570	831.150190	11.921191
20.133744	824.684569	11.926195
20.232075	813.874736	11.931200
19.808997	827.089033	11.936205
20.077694	818.387191	11.941210
20.106219	822.504682	11.946215
19.951011	820.214446	11.951219
20.258080	819.662372	11.956224
19.988962	826.698930	11.961229
20.283579	814.325013	11.966234
20.194225	822.734788	11.971239
20.211005	820.097003	11.976243
20.415586	817.703651	11.981248
19.859997	827.919261	11.986253
20.150288	814.732337	11.991258
20.543132	824.158018	11.996263
20.341763	840.252713	12.001267
20.595887	853.631834	12.006272
20.486425	843.407048	12.011277
21.144735	849.568731	12.016282
21.093540	845.580888	12.021287
20.855822	829.590799	12.026291
21.188008	816.764616	12.031296
20.878714	819.611366	12.036301
20.928719	815.735122	12.041306
20.664815	816.097273	12.046311
20.674537	830.291203	12.051315
20.690613	823.810547	12.056320
20.617203	825.247745	12.061325
20.905106	811.999703	12.066330
20.687833	822.729046	12.071335
20.529693	813.831936	12.076339
20.559841	817.946014	12.081344
20.284172	825.087693	12.086349
21.001881	808.765472	12.091354
20.630843	822.917622	12.096359
20.450490	816.988685	12.101363
20.708533	826.886871	12.106368
20.645000	820.724837	12.111373
20.764274	822.375728	12.116378
20.618053	826.107935	12.121383
20.659518	826.579076	12.126387
20.820645	820.054786	12.131392
20.589447	832.240286	12.136397
20.865052	827.806094	12.141402
21.027083	840.780427	12.146407
20.687308	825.979858	12.151411
21.088682	824.938087	12.156416
20.983884	828.513880	12.161421
21.011127	827.210087	12.166426
20.567425	818.883638	12.171431
20.892357	797.406011	12.176435
20.799463	785.401425	12.181440
20.532484	803.925550	12.186445
20.948587	790.389004	12.191450
20.746340	789.397778	12.196455
20.540641	802.232035	12.201459
20.441590	808.148647	12.206464
20.618250	794.047899	12.211469
20.792772	793.006042	12.216474
20.695609	804.656064	12.221479
20.598192	799.503947	12.226483
20.827490	796.486924	12.231488
20.471185	792.002142	12.236493
20.725682	794.997082	12.241498
20.690891	796.842850	12.246503
20.963266	788.709710	12.251507
20.808006	802.455271	12.256512
20.783399	796.236578	12.261517
21.049644	793.708818	12.266522
20.799954	792.176388	12.271527
20.950756	797.613182	12.276531
20.950180	795.493826	12.281536
20.781939	805.584563	12.286541
20.840838	794.369456	12.291546
21.107737	801.899242	12.296551
20.855143	792.490517	12.301555
20.766836	773.534111	12.306560
20.485071	780.091701	12.311565
20.784510	764.094857	12.316570
20.580870	767.670630	12.321575
20.545938	772.186153	12.326579
20.587446	766.453659	12.331584
20.514058	777.678828	12.336589
20.873680	784.657662	12.341594
20.902855	790.246314	12.346599
20.583550	771.435562	12.351603
20.601973	778.583928	12.356608
20.312831	780.361453	12.361613
20.883921	783.641781	12.366618
20.578783	804.743962	12.371623
20.497458	803.444871	12.376627
20.824376	796.141954	12.381632
20.794896	804.673055	12.386637
20.855687	797.956623	12.391642
20.604644	794.792287	12.396647
20.711132	783.897599	12.401651
20.696320	773.887997	12.406656
20.624015	774.878744	12.411661
21.122164	770.833267	12.416666
20.849779	784.045567	12.421671
20.822178	787.274730	12.426675
20.814662	778.484503	12.431680
20.591578	779.603376	12.436685
20.694887	779.664112	12.441690
20.284210	776.542587	12.446695
20.324553	778.712255	12.451699
20.603727	779.916597	12.456704
20.303347	790.127746	12.461709
20.837950	795.907020	12.466714
20.667672	796.809317	12.471719
20.533952	803.696537	12.476723
20.569592	797.034578	12.481728
20.831193	808.906499	12.486733
21.051964	795.487833	12.491738
20.947159	801.529937	12.496743
20.868981	786.867454	12.501747
20.619939	778.216673	12.506752
20.318545	796.101315	12.511757
20.660181	775.090981	12.516762
20.466216	789.787283	12.521767
20.577468	779.040069	12.526771
20.721960	794.038778	12.531776
20.607967	782.084868	12.536781
20.794878	796.644736	12.541786
20.936472	789.027610	12.546791
20.823450	784.196528	12.551795
20.713430	785.863485	12.556800
20.577392	801.175022	12.561805
21.032269	775.535687	12.566810
20.516205	788.466740	12.571815
20.727080	788.813090	12.576819
20.972179	783.951698	12.581824
20.759421	789.066435	12.586829
20.965552	779.415823	12.591834
20.634701	789.146137	12.596839
20.876072	782.569643	12.601843
20.742426	795.482286	12.606848
20.695094	785.641864	12.611853
20.725996	791.069395	12.616858
20.798207	791.600284	12.621863
20.720579	793.292037	12.626867
20.627381	787.885367	12.631872
20.441806	791.097149	12.636877
20.793867	787.436084	12.641882
20.437221	785.920713	12.646887
20.733378	790.854936	12.651891
21.103042	778.937427	12.656896
20.934783	797.647646	12.661901
21.085175	779.156203	12.666906
20.977748	769.530377	12.671911
20.700753	762.721182	12.676915
20.555393	757.784881	12.681920
20.159547	755.515689	12.686925
20.379683	779.883443	12.691930
20.445151	795.541298	12.696935
20.766173	799.627901	12.701939
20.657808	792.651450	12.706944
20.394136	804.938300	12.711949
20.678574	793.256719	12.716954
20.717681	787.478869	12.721959
20.778297	804.351741	12.726963
20.628110	800.591008	12.731968
20.963393	799.028355	12.736973
20.777976	794.634587	12.741978
20.588097	801.910803	12.746983
20.575190	798.834639	12.751987
20.821542	788.392296	12.756992
20.442579	802.277613	12.761997
20.843137	797.561729	12.767002
20.527023	805.834200	12.772007
20.290162	799.594166	12.777011
20.721976	807.671654	12.782016
20.431272	803.220560	12.787021
20.768492	801.178212	12.792026
20.248832	812.193891	12.797031
20.389589	797.250478	12.802035
20.787419	799.123439	12.807040
20.761054	802.934294	12.812045
20.992401	807.863090	12.817050
20.837102	805.708486	12.822055
20.549452	795.403346	12.827059
21.006792	799.178052	12.832064
20.821914	801.331606	12.837069
20.933618	802.176314	12.842074
20.616901	803.994509	12.847079
21.082851	803.316173	12.852083
20.901029	793.475118	12.857088
20.499563	789.897966	12.862093
20.606337	788.392260	12.867098
20.838812	776.879827	12.872103
20.487800	782.786153	12.877107
20.689011	776.906760	12.882112
20.757461	792.958368	12.887117
20.825536	788.708672	12.892122
20.311369	780.352484	12.897127
20.950034	779.451062	12.902131
21.193866	777.738997	12.907136
20.412226	779.371149	12.912141
20.782812	772.193741	12.917146
20.639690	771.230933	12.922151
20.672601	768.702546	12.927155
20.566434	775.580627	12.932160
20.474319	777.126458	12.937165
20.861399	775.647007	12.942170
20.572947	775.150495	12.947175
20.335595	777.020683	12.952179
20.758062	780.845100	12.957184
20.686631	798.926453	12.962189
20.785588	781.029828	12.967194
20.626121	777.827237	12.972199
20.730408	780.087629	12.977203
20.664631	767.506309	12.982208
20.725099	780.920980	12.987213
21.013744	765.321665	12.992218
20.707477	778.312287	12.997223
20.719137	769.929008	13.002227
20.762933	768.094310	13.007232
20.750197	780.716425	13.012237
20.878191	771.609704	13.017242
21.079152	773.476215	13.022247
20.819100	769.228396	13.027251
20.570289	772.502298	13.032256
20.596875	790.605854	13.037261
20.804031	779.401804	13.042266
20.727416	775.875344	13.047271
20.510179	784.094185	13.052275
20.847971	777.502314	13.057280
20.618192	778.945525	13.062285
20.609530	775.575381	13.067290
20.608240	772.082639	13.072295
20.793408	784.371999	13.077299
20.982164	777.723475	13.082304
20.799548	782.588980	13.087309
21.051958	786.292291	13.092314
20.517488	780.462425	13.097319
20.439728	783.581317	13.102323
21.036825	783.058680	13.107328
20.657378	785.400956	13.112333
20.849235	785.100645	13.117338
20.721973	788.342549	13.122343
20.758055	771.189236	13.127347
20.670076	760.330312	13.132352
20.497371	773.503051	13.137357
20.874937	771.708156	13.142362
20.625398	767.490200	13.147367
20.499313	762.811017	13.152371
21.022968	747.125354	13.157376
20.607174	767.713707	13.162381
20.700625	747.111999	13.167386
20.577111	759.404840	13.172391
20.504282	753.824626	13.177395
20.511261	763.581465	13.182400
20.648975	785.166486	13.187405
21.073788	774.391342	13.192410
20.607174	770.091315	13.197415
20.498242	759.063849	13.202419
20.851713	776.590135	13.207424
20.927685	771.424567	13.212429
20.706286	758.942190	13.217434
20.752474	754.711764	13.222439
20.721570	756.806060	13.227443
20.992198	746.410337	13.232448
20.617447	749.002589	13.237453
20.643429	749.608658	13.242458
20.695903	755.493196	13.247463
20.535303	749.097521	13.252467
20.713494	748.635390	13.257472
20.734938	752.433876	13.262477
20.812135	746.638929	13.267482
20.798752	750.420892	13.272487
21.209809	754.351200	13.277491
20.831024	750.779901	13.282496
20.381743	760.727778	13.287501
20.568233	752.602049	13.292506
20.962744	743.545876	13.297511
20.683830	762.969122	13.302515
20.936145	754.539585	13.307520
20.984977	747.530199	13.312525
20.958860	749.737270	13.317530
20.796677	758.015124	13.322535
20.899510	739.156009	13.327539
20.953410	719.557262	13.332544
20.219760	730.725279	13.337549
20.654152	725.075216	13.342554
20.643870	735.206942	13.347559
20.176585	745.428911	13.352563
20.560402	748.892061	13.357568
20.515246	750.485592	13.362573
20.939706	751.293029	13.367578
20.694672	764.800565	13.372583
20.697494	767.353101	13.377587
20.801711	766.038613	13.382592
20.521533	760.370044	13.387597
20.642118	762.489065	13.392602
20.749877	753.352468	13.397607
20.691499	760.248150	13.402611
21.032809	765.512625	13.407616
20.393769	754.859865	13.412621
20.523623	762.573912	13.417626
20.216199	767.500317	13.422631
20.427813	760.587963	13.427635
20.838441	761.484338	13.432640
20.575309	760.677863	13.437645
20.630685	752.345969	13.442650
20.574820	760.345097	13.447655
20.614969	767.718646	13.452659
20.549895	771.256551	13.457664
20.746706	764.679287	13.462669
20.813187	759.162006	13.467674
20.692440	763.579251	13.472679
20.771395	758.804289	13.477683
21.075800	761.062722	13.482688
20.686386	771.141404	13.487693
20.759672	760.223644	13.492698
20.874225	761.662396	13.497703
20.968811	770.030188	13.502707
20.613023	750.028396	13.507712
20.335451	755.143998	13.512717
20.677865	763.644144	13.517722
20.680869	764.693840	13.522727
20.652773	773.582664	13.527731
21.025766	759.075327	13.532736
20.699827	767.502305	13.537741
20.833752	756.773568	13.542746
20.416312	756.532591	13.547751
20.696684	751.011160	13.552755
21.050263	748.734401	13.557760
20.535617	746.012658	13.562765
20.549172	728.621719	13.567770
20.482584	739.363235	13.572775
20.597587	756.077570	13.577779
20.888006	758.658349	13.582784
20.659324	749.846645	13.587789
20.674877	746.612992	13.592794
20.588089	747.451509	13.597799
20.579061	755.682857	13.602803
20.720239	757.289246	13.607808
20.578448	771.496245	13.612813
21.111367	767.554032	13.617818
20.720689	754.996157	13.622823
20.681424	742.754399	13.627827
20.632646	731.422475	13.632832
20.678438	733.928728	13.637837
20.475734	734.858270	13.642842
20.272509	748.854277	13.647847
20.557991	760.142040	13.652851
20.890508	763.998146	13.657856
20.952077	779.426374	13.662861
20.627334	759.034848	13.667866
20.604159	754.329792	13.672871
20.673730	758.861758	13.677875
20.535414	765.347577	13.682880
20.605129	779.483004	13.687885
20.801217	772.771813	13.692890
21.252966	766.604888	13.697895
21.055065	761.484581	13.702899
20.911793	743.563559	13.707904
20.350548	751.296365	13.712909
20.612850	742.466280	13.717914
20.864121	733.163306	13.722919
20.221617	742.489143	13.727923
20.821972	737.028644	13.732928
20.575505	735.522513	13.737933
20.513137	742.327362	13.742938
20.556934	740.491090	13.747943
20.452296	745.052414	13.752947
20.608495	745.995676	13.757952
20.463732	761.023139	13.762957
20.750241	767.072201	13.767962
20.760284	778.325064	13.772967
20.906214	769.048330	13.777971
20.987337	756.077743	13.782976
20.561369	747.888853	13.787981
20.841364	746.622023	13.792986
20.607330	736.098643	13.797991
20.538538	747.725171	13.802995
20.819483	735.198963	13.808000
20.636699	745.228902	13.813005
20.407485	753.181559	13.818010
20.745687	737.375677	13.823015
20.764957	753.061354	13.828019
20.583355	749.024953	13.833024
20.776739	753.776863	13.838029
20.754447	746.506013	13.843034
20.728256	758.646140	13.848039
20.676632	751.625966	13.853043
20.720040	741.786870	13.858048
20.441298	749.901964	13.863053
20.855591	737.878024	13.868058
20.864421	748.514480	13.873063
20.493715	742.522895	13.878067
20.457981	748.254345	13.883072
20.613711	749.907297	13.888077
20.434045	742.937512	13.893082
20.792477	745.583133	13.898087
20.820168	744.826468	13.903091
21.026006	742.984851	13.908096
20.619892	752.588376	13.913101
20.605793	743.952182	13.918106
20.692690	735.735116	13.923111
20.758647	749.426421	13.928115
20.678367	748.997630	13.933120
20.986531	749.243308	13.938125
21.105124	739.650838	13.943130
20.645971	738.776283	13.948135
20.552745	750.597517	13.953139
20.848906	749.388032	13.958144
20.861009	748.927161	13.963149
20.714408	747.097601	13.968154
20.860933	740.602483	13.973159
20.773438	748.650804	13.978163
20.951899	742.869669	13.983168
20.670944	754.337656	13.988173
20.811074	745.255824	13.993178
20.640936	748.400481	13.998183
20.627576	760.740408	14.003187
21.142971	755.115260	14.008192
20.387441	743.907627	14.013210
20.631796	749.030856	14.018227
20.586956	755.210014	14.023245
20.570216	751.874932	14.028263
21.098036	742.586078	14.033280
21.099408	753.437243	14.038298
20.644592	739.194760	14.043315
20.799943	726.121157	14.048333
20.658505	726.832588	14.053351
21.192512	726.536592	14.058368
20.800762	733.060485	14.063386
20.437983	721.401769	14.068403
20.842317	741.262705	14.073421
20.689089	745.145411	14.078439
20.677298	751.451421	14.083456
20.884027	758.485438	14.088474
20.936964	749.981698	14.093491
21.072153	758.884722	14.098509
20.738232	752.478017	14.103527
20.851971	753.475914	14.108544
20.896674	754.997587	14.113562
20.434632	755.379512	14.118579
20.950649	748.055518	14.123597
20.750387	761.980839	14.128615
20.865162	756.510799	14.133632
20.811401	768.860307	14.138650
21.015362	772.742676	14.143667
21.147139	783.143662	14.148685
21.059848	793.645658	14.153703
21.250224	782.603330	14.158720
21.145946	787.009882	14.163738
21.426572	789.829327	14.168755
21.114254	784.973193	14.173773
21.162460	797.105130	14.178791
21.329326	788.625666	14.183808
21.380649	798.482686	14.188826
21.269685	792.203986	14.193843
21.373278	786.534386	14.198861
21.125448	791.720402	14.203879
21.159684	782.164207	14.208896
21.305177	788.924883	14.213914
21.106046	802.359316	14.218931
21.166099	790.419191	14.223949
20.997662	785.510223	14.228967
20.981441	789.957783	14.233984
21.597840	811.758989	14.239002
21.395302	818.111179	14.244019
21.869283	815.712341	14.249037
21.454819	817.466118	14.254055
21.767796	811.676603	14.259072
21.536129	816.858477	14.264090
21.614921	816.932364	14.269107
21.804116	815.027225	14.274125
21.557933	801.798962	14.279143
21.919337	799.775131	14.284160
21.413074	798.583339	14.289178
21.709812	808.827482	14.294195
21.529400	800.021183	14.299213
21.538312	816.590281	14.304231
21.430488	814.123800	14.309248
21.622874	823.300864	14.314266
21.720614	821.603779	14.319283
22.070774	813.353023	14.324301
21.825838	820.273505	14.329319
21.648797	813.704909	14.334336
21.837406	821.259333	14.339354
21.789283	822.618080	14.344371
21.830230	812.689588	14.349389
21.576214	828.470140	14.354407
21.622604	826.211851	14.359424
21.816130	827.539922	14.364442
21.430982	819.159493	14.369459
21.923087	813.788113	14.374477
21.789185	831.241960	14.379495
21.643848	841.533040	14.384512
22.202758	853.714123	14.389530
21.581650	852.658611	14.394547
22.068336	856.723982	14.399565
22.162835	856.263719	14.404583
22.243104	843.080872	14.409600
22.446240	860.460550	14.414618
22.172994	852.724450	14.419635
22.608734	851.945512	14.424653
22.295778	861.520927	14.429671
22.503400	839.045453	14.434688
22.204879	827.974109	14.439706
22.335065	822.419794	14.444723
22.552445	802.300611	14.449741
22.025181	817.007968	14.454759
22.044363	819.241527	14.459776
22.387375	837.739227	14.464794
22.217733	843.224227	14.469811
22.191394	847.085149	14.474829
22.694794	851.542654	14.479847
22.291833	846.883413	14.484864
22.700625	850.201489	14.489882
22.612027	835.746357	14.494899
22.698329	826.891211	14.499917
22.739293	829.181068	14.504935
22.640964	814.774695	14.509952
23.012823	812.832559	14.514970
22.636116	817.370653	14.519987
22.678290	809.257104	14.525005
22.805056	816.231549	14.530023
22.884188	823.138095	14.535040
22.484615	814.569647	14.540058
22.387583	816.565357	14.545075
22.950001	822.210423	14.550093
22.746637	824.913600	14.555111
22.474029	803.966568	14.560128
22.532962	815.763354	14.565146
22.640171	808.290617	14.570163
22.488145	805.452117	14.575181
22.319526	815.509384	14.580199
22.537727	819.859793	14.585216
22.541681	813.329965	14.590234
22.534056	845.160518	14.595251
23.060615	841.468222	14.600269
23.004484	848.836769	14.605287
22.893962	851.679289	14.610304
23.135106	844.534358	14.615322
22.741232	827.328141	14.620339
23.102225	840.626086	14.625357
22.971895	844.094637	14.630375
22.926584	837.517603	14.635392
22.868075	832.572212	14.640410
22.938579	848.878285	14.645427
23.108448	846.870840	14.650445
22.988106	858.471327	14.655463
23.033487	850.396566	14.660480
23.117772	850.719670	14.665498
23.042112	848.495000	14.670515
23.127432	861.943891	14.675533
23.014321	856.466118	14.680551
23.030643	847.115643	14.685568
23.200091	844.521570	14.690586
22.860095	855.883402	14.695603
23.467070	845.447788	14.700621
23.480540	847.765628	14.705639
23.428607	854.894425	14.710656
23.338422	841.617651	14.715674
23.357130	850.691881	14.720691
23.519581	847.680529	14.725709
23.181101	856.742523	14.730727
23.105127	852.545471	14.735744
23.101679	847.435574	14.740762
23.153971	852.153777	14.745779
23.323292	844.855145	14.750797
23.499142	839.910122	14.755815
23.546190	840.328821	14.760832
23.914727	840.974649	14.765850
23.682101	840.258270	14.770867
23.736851	838.803977	14.775885
23.413785	846.550126	14.780903
23.757099	838.883998	14.785920
23.714283	835.872356	14.790938
23.788826	844.835438	14.795955
24.007324	842.617332	14.800973
23.807363	845.058867	14.805991
23.906760	839.628998	14.811008
24.064903	845.594936	14.816026
23.600008	847.831780	14.821043
23.944534	840.778893	14.826061
24.104023	847.153574	14.831079
23.679727	845.426497	14.836096
23.529926	841.662763	14.841114
23.446093	838.352517	14.846131
23.565594	847.766148	14.851149
23.837876	835.074889	14.856167
23.837623	849.613287	14.861184
23.821465	833.149006	14.866202
23.696562	840.638621	14.871219
24.004512	840.026346	14.876237
23.958871	841.295043	14.881255
24.078094	842.559467	14.886272
24.213118	839.475418	14.891290
23.684988	844.463929	14.896307
23.803690	850.190786	14.901325
23.925309	842.926503	14.906343
23.764005	850.469116	14.911360
24.027634	870.478504	14.916378
24.225473	870.176353	14.921395
24.220114	863.064436	14.926413
24.552180	866.320827	14.931431
24.321444	873.758130	14.936448
24.520105	848.945146	14.941466
24.189149	849.052926	14.946483
24.455358	844.340438	14.951501
24.000141	838.034832	14.956519
24.135563	849.039282	14.961536
24.701185	860.862250	14.966554
24.317735	859.691760	14.971571
24.612082	851.528530	14.976589
24.073141	848.405691	14.981607
24.027449	861.996591	14.986624
24.561763	853.911483	14.991642
24.353590	866.345472	14.996659
24.716171	863.774071	15.001677
24.679319	861.522762	15.006695
24.684069	857.460687	15.011712
24.709070	865.571301	15.016730
24.604996	863.541483	15.021747
24.742081	852.436821	15.026765
24.656500	850.548763	15.031783
24.656718	860.700247	15.036800
25.091830	851.091081	15.041818
24.611177	839.238726	15.046835
24.640765	842.848499	15.051853
24.643389	826.090241	15.056871
24.282317	851.012340	15.061888
24.364139	851.395608	15.066906
24.874988	858.047711	15.071923
24.731655	851.829200	15.076941
24.972125	868.973289	15.081959
24.483063	869.864430	15.086976
24.834501	860.913497	15.091994
24.669370	866.905837	15.097011
24.768480	858.237379	15.102029
24.847588	867.632298	15.107047
24.871542	858.961670	15.112064
25.097101	864.415105	15.117082
24.924901	867.648110	15.122099
25.055856	863.383447	15.127117
24.994643	862.532770	15.132135
24.539053	867.808573	15.137152
25.245162	871.260120	15.142170
25.106307	888.867399	15.147187
25.019236	896.583800	15.152205
25.638887	881.652317	15.157223
25.192682	894.745596	15.162240
25.581467	862.272051	15.167258
25.339326	858.823466	15.172275
25.280777	862.508644	15.177293
25.497316	851.016957	15.182311
25.305746	862.782954	15.187328
25.513496	849.914798	15.192346
25.699075	846.149479	15.197363
25.159853	858.140794	15.202381
25.433799	864.972247	15.207399
25.139056	846.941718	15.212416
25.357039	855.303098	15.217434
25.518919	861.732456	15.222451
25.288997	850.791715	15.227469
25.259942	851.419165	15.232487
25.011586	854.941147	15.237504
25.584042	863.763484	15.242522
25.590090	878.549427	15.247539
25.682763	888.208019	15.252557
26.103254	876.266961	15.257575
25.959213	876.016190	15.262592
25.687570	856.044135	15.267610
25.428799	859.426216	15.272627
25.650155	855.331168	15.277645
25.930745	843.527273	15.282663
25.522399	851.908326	15.287680
25.729511	854.701760	15.292698
25.809092	874.400760	15.297715
25.779364	887.067410	15.302733
25.586229	879.162799	15.307751
25.683279	891.985401	15.312768
26.135498	887.073357	15.317786
25.826035	887.668458	15.322803
25.859051	892.207290	15.327821
26.412457	874.796454	15.332839
26.068769	884.392514	15.337856
26.198003	886.408771	15.342874
25.869373	880.537529	15.347891
26.021111	885.191121	15.352909
26.179831	871.920235	15.357927
26.031780	893.662605	15.362944
26.251041	876.825695	15.367962
26.445440	876.841820	15.372979
25.987809	877.855355	15.377997
26.296664	883.226303	15.383015
25.912239	888.423128	15.388032
26.224196	876.848568	15.393050
26.167261	881.760367	15.398067
26.015204	880.184908	15.403085
26.120282	888.191533	15.408103
26.279335	887.884557	15.413120
26.261452	886.278260	15.418138
26.157719	888.627382	15.423155
26.182464	889.779472	15.428173
26.596148	879.583861	15.433191
26.328797	887.391927	15.438208
26.226194	880.682448	15.443226
26.588994	881.461319	15.448243
26.140779	895.146335	15.453261
26.303352	883.383251	15.458279
26.089805	891.711238	15.463296
26.457440	894.960390	15.468314
26.338357	916.893216	15.473331
26.459133	917.031188	15.478349
26.960790	911.911490	15.483367
26.287904	920.701265	15.488384
26.720835	905.834142	15.493402
26.759622	916.322410	15.498419
27.001913	918.470068	15.503437
26.800019	922.609104	15.508455
26.593108	912.309543	15.513472
26.939433	907.439548	15.518490
26.721489	913.857153	15.523507
26.731709	914.976958	15.528525
26.784102	901.177200	15.533543
26.823979	919.809864	15.538560
26.615804	919.997156	15.543578
26.453659	911.666042	15.548595
26.508156	928.962552	15.553613
26.960077	936.751875	15.558631
26.880580	948.909026	15.563648
27.163138	957.392292	15.568666
27.396172	942.954963	15.573683
27.360723	959.392883	15.578701
27.293818	929.204969	15.583719
26.967607	934.356348	15.588736
27.025971	929.876743	15.593754
27.611646	933.377400	15.598771
27.186893	927.427094	15.603789
27.209425	922.136860	15.608807
27.383415	929.813216	15.613824
27.414695	923.513344	15.618842
27.267565	923.042857	15.623859
27.047721	920.092462	15.628877
27.329617	928.355607	15.633895
27.413238	948.057209	15.638912
27.830883	951.457263	15.643930
27.648676	930.662358	15.648947
27.195098	924.304546	15.653965
27.294103	936.615676	15.658983
27.505774	938.628230	15.664000
27.467210	940.193089	15.669018
27.639907	933.909981	15.674035
27.320902	952.632958	15.679053
27.729180	933.489816	15.684071
27.622609	942.585658	15.689088
27.607539	944.064978	15.694106
27.901052	942.073978	15.699123
27.755557	944.023955	15.704141
27.792205	936.938334	15.709159
27.524090	944.675771	15.714176
27.761729	947.750626	15.719194
28.158110	950.309412	15.724211
27.861992	944.148260	15.729229
27.923140	942.798321	15.734247
27.979968	939.421576	15.739264
28.175560	937.634944	15.744282
28.363339	932.991561	15.749299
28.006063	917.860372	15.754317
27.945006	910.648784	15.759335
27.834583	905.990053	15.764352
28.067935	913.112703	15.769370
28.195870	913.427273	15.774387
28.221395	914.623283	15.779405
28.019076	901.035597	15.784423
28.020766	913.856125	15.789440
28.099018	919.652378	15.794458
28.164052	932.005099	15.799475
28.254425	936.580412	15.804493
28.228990	941.518666	15.809511
27.967688	942.604704	15.814528
28.175057	948.688668	15.819546
28.092921	947.699760	15.824563
28.225993	946.354079	15.829581
28.367222	937.548303	15.834599
28.431172	942.972491	15.839616
28.154184	950.683034	15.844634
28.161451	942.807770	15.849651
28.377672	942.826707	15.854669
28.423800	943.417004	15.859687
28.758160	946.888538	15.864704
28.645824	942.676811	15.869722
28.699580	948.854483	15.874739
28.395168	939.339612	15.879757
28.803788	941.724996	15.884775
28.705170	949.789310	15.889792
28.558253	940.422341	15.894810
28.607387	941.358201	15.899827
28.676424	935.401491	15.904845
28.517157	938.624585	15.909863
28.353739	938.340726	15.914880
28.945976	935.581685	15.919898
28.795855	946.987232	15.924915
28.689546	953.236049	15.929933
28.711428	951.381173	15.934951
28.909965	961.051242	15.939968
28.983258	965.791299	15.944986
29.254197	960.049327	15.950003
29.296670	964.954737	15.955021
28.919727	936.760390	15.960039
28.725575	943.858435	15.965056
29.068055	949.721089	15.970074
29.021038	945.727017	15.975091
28.580917	963.053694	15.980109
29.134989	960.569705	15.985127
29.200268	946.838630	15.990144
29.217785	956.495098	15.995162
29.267484	956.573626	16.000179
29.177175	961.846256	16.005197
29.218565	961.045272	16.010215
29.163935	960.012652	16.015232
29.163001	963.337905	16.020250
29.505339	952.275932	16.025267
29.178733	958.017228	16.030285
29.102391	960.494118	16.035303
29.367342	956.478600	16.040320
29.413681	962.872952	16.045338
29.732835	957.551126	16.050355
29.381477	950.590298	16.055373
29.465483	957.464673	16.060391
29.745611	951.271382	16.065408
29.648096	958.890389	16.070426
29.818505	946.281344	16.075443
29.663906	951.001118	16.080461
29.632407	951.657275	16.085479
29.876264	951.440585	16.090496
29.180134	963.589137	16.095514
29.448667	962.718894	16.100531
29.413278	953.349857	16.105549
29.686764	962.117699	16.110567
29.661599	964.197916	16.115584
29.566895	984.698741	16.120602
30.181679	986.971033	16.125619
29.810894	993.524728	16.130637
29.843530	992.517512	16.135655
30.083656	990.607374	16.140672
29.983947	985.630751	16.145690
30.294270	986.342497	16.150707
30.163933	984.912990	16.155725
30.214582	981.104665	16.160743
30.349382	974.695459	16.165760
30.037706	974.955883	16.170778
30.198846	954.351560	16.175795
30.070541	960.864994	16.180813
30.096803	979.311156	16.185831
29.985506	980.871890	16.190848
29.938810	987.410071	16.195866
30.492049	983.748090	16.200883
29.959065	989.929702	16.205901
30.378774	982.867902	16.210919
30.225670	977.975297	16.215936
30.141771	988.226798	16.220954
30.442052	975.991819	16.225971
30.097691	976.793823	16.230989
29.794770	988.280398	16.236007
30.592205	980.754113	16.241024
30.310855	980.372666	16.246042
30.357753	988.369752	16.251059
30.643443	998.243010	16.256077
30.368502	1013.865088	16.261095
30.801299	1004.117773	16.266112
30.629008	1009.927281	16.271130
31.210971	986.015563	16.276147
30.658050	993.010413	16.281165
30.782970	992.999870	16.286183
31.031209	971.453604	16.291200
30.603857	977.994293	16.296218
30.820771	973.295917	16.301235
30.536840	975.598292	16.306253
30.626115	987.961352	16.311271
31.069505	990.330188	16.316288
30.608957	1005.535149	16.321306
30.901797	998.452680	16.326323
30.856329	1004.355210	16.331341
30.980547	1009.080867	16.336359
31.442604	1001.535707	16.341376
31.237115	998.866133	16.346394
31.250721	996.081397	16.351411
31.140534	1003.304497	16.356429
31.216304	1005.518050	16.361447
31.068299	1003.916763	16.366464
31.068766	1001.445562	16.371482
31.065160	999.023771	16.376499
31.655909	1007.110297	16.381517
31.195761	998.439720	16.386535
31.280683	991.684552	16.391552
31.474635	999.736837	16.396570
31.581850	986.143746	16.401587
31.720128	997.731410	16.406605
31.457155	989.095455	16.411623
31.668511	990.370365	16.416640
31.291429	991.764291	16.421658
31.703361	985.471318	16.426675
31.626449	996.157411	16.431693
31.362809	999.551311	16.436711
31.417864	987.843040	16.441728
31.700801	984.747954	16.446746
31.808695	999.514631	16.451763
31.616904	990.783957	16.456781
31.374445	996.371857	16.461799
31.697990	989.301798	16.466816
31.537550	997.970565	16.471834
31.312172	986.250396	16.476851
31.305040	991.619876	16.481869
31.275938	1009.459892	16.486887
32.003358	1018.641406	16.491904
32.250361	1029.582584	16.496922
32.266769	1029.899215	16.501939
32.060702	1025.653652	16.506957
31.993421	1025.420521	16.511975
31.913032	1016.882837	16.516992
31.685115	1035.950021	16.522010
31.968937	1030.289332	16.527027
31.989047	1018.872883	16.532045
31.878866	1030.984663	16.537063
32.072034	1025.531905	16.542080
32.325340	1022.026283	16.547098
32.192709	1024.070168	16.552115
32.313962	1018.597423	16.557133
32.178042	1017.052406	16.562151
32.124871	1021.155167	16.567168
31.836266	1012.167803	16.572186
32.187107	1022.518296	16.577203
32.656797	1029.129857	16.582221
32.310685	1038.699666	16.587239
32.443629	1031.431909	16.592256
32.781095	1041.234022	16.597274
32.923784	1030.222706	16.602291
32.415979	1021.504663	16.607309
32.066650	1022.478912	16.612327
32.765991	1027.677532	16.617344
32.740609	1044.779294	16.622362
33.080332	1038.917789	16.627379
32.800520	1026.400927	16.632397
32.544218	1023.571149	16.637415
32.719981	1029.797034	16.642432
33.043351	1040.140909	16.647450
32.957226	1031.722101	16.652467
32.880551	1023.679293	16.657485
32.962908	1018.362181	16.662503
32.717768	1001.069115	16.667520
32.604942	1015.963815	16.672538
32.772754	1034.236471	16.677555
33.114080	1050.436662	16.682573
32.854635	1051.143334	16.687591
32.967237	1039.185185	16.692608
32.929596	1039.349998	16.697626
32.820517	1042.443994	16.702643
33.077383	1044.567326	16.707661
32.913894	1055.404115	16.712679
33.187961	1046.158687	16.717696
32.998748	1043.315059	16.722714
32.828456	1054.662563	16.727731
33.524510	1056.277003	16.732749
33.453104	1073.313783	16.737767
33.477364	1075.202099	16.742784
33.516951	1072.237036	16.747802
33.659470	1062.709001	16.752819
33.829462	1045.843576	16.757837
33.450479	1042.759669	16.762855
33.390991	1040.513515	16.767872
33.586743	1032.373774	16.772890
33.367905	1041.353884	16.777907
33.715259	1044.749443	16.782925
33.486470	1068.804580	16.787943
33.802948	1062.654206	16.792960
33.822037	1074.827199	16.797978
34.210110	1052.041058	16.802995
33.706701	1047.676180	16.808013
33.325247	1053.235936	16.813031
33.741534	1052.600084	16.818048
33.960634	1069.088762	16.823066
33.843765	1075.411671	16.828083
34.020854	1071.059370	16.833101
34.045343	1073.826921	16.838119
33.958350	1072.845070	16.843136
34.089278	1083.328202	16.848154
34.087188	1076.160606	16.853171
34.114438	1064.947464	16.858189
33.995910	1071.335126	16.863207
34.229196	1072.453971	16.868224
33.898517	1067.204288	16.873242
34.176843	1069.879447	16.878259
34.440985	1063.430697	16.883277
34.097704	1069.928133	16.888295
34.484848	1064.471163	16.893312
34.227120	1069.919963	16.898330
34.183813	1061.524193	16.903347
34.142531	1058.633375	16.908365
34.142018	1073.566847	16.913383
34.244746	1061.877653	16.918400
34.410771	1063.268332	16.923418
34.557179	1073.564954	16.928435
34.505854	1069.971060	16.933453
34.173696	1075.533973	16.938471
34.325955	1062.270235	16.943488
34.347466	1081.794746	16.948506
34.740914	1091.278096	16.953523
34.953116	1083.933182	16.958541
34.613414	1086.228740	16.963559
34.674374	1087.617302	16.968576
35.087986	1083.694437	16.973594
35.425958	1081.719922	16.978611
35.456798	1071.190430	16.983629
35.219592	1065.136225	16.988647
35.027952	1062.291408	16.993664
35.041250	1050.176065	16.998682
34.949558	1055.088747	17.003699
35.203963	1059.722877	17.008717
34.851775	1060.118744	17.013735
35.130071	1048.146744	17.018752
34.990807	1057.787389	17.023770
34.604144	1063.885923	17.028787
35.055491	1059.117099	17.033805
34.851096	1079.272205	17.038823
34.816825	1074.330729	17.043840
35.297974	1092.984471	17.048858
35.325918	1079.496738	17.053875
35.477980	1087.351271	17.058893
35.139750	1082.516469	17.063911
35.384448	1087.164739	17.068928
35.458603	1077.133247	17.073946
35.200495	1085.603724	17.078963
35.525215	1087.788596	17.083981
35.437817	1082.520554	17.088999
35.226655	1090.886025	17.094016
35.624388	1082.858753	17.099034
35.390531	1092.547538	17.104051
35.633247	1079.381036	17.109069
35.545461	1090.619460	17.114087
35.319700	1111.308099	17.119104
35.838662	1113.082916	17.124122
35.824549	1116.783093	17.129139
36.214068	1105.285639	17.134157
35.891388	1119.748324	17.139175
36.187419	1109.074269	17.144192
35.805648	1102.857498	17.149210
35.713044	1101.802612	17.154227
36.550350	1108.621408	17.159245
36.151407	1100.255596	17.164263
36.027104	1089.675332	17.169280
36.038057	1090.909858	17.174298
35.932616	1086.037927	17.179315
36.156841	1109.460917	17.184333
36.078586	1108.707319	17.189351
36.283090	1120.377324	17.194368
36.059130	1112.619065	17.199386
36.034542	1113.821510	17.204403
36.519092	1112.635251	17.209421
36.217701	1120.555830	17.214439
36.493270	1105.373847	17.219456
36.532075	1108.493032	17.224474
36.291065	1114.321406	17.229491
36.515565	1109.164051	17.234509
36.428460	1113.247083	17.239527
36.547067	1101.992601	17.244544
36.609264	1112.529186	17.249562
36.341730	1114.460898	17.254579
36.691934	1115.999951	17.259597
36.483661	1104.066183	17.264615
36.556807	1116.381592	17.269632
36.923807	1113.291947	17.274650
36.899389	1117.910792	17.279667
36.634432	1114.712735	17.284685
36.822401	1117.147498	17.289703
36.810738	1107.340446	17.294720
36.915424	1123.300050	17.299738
36.799333	1130.890651	17.304755
37.281663	1124.499880	17.309773
36.894461	1136.303590	17.314791
37.087381	1143.483137	17.319808
37.164096	1130.799217	17.324826
36.905840	1132.142745	17.329843
37.111958	1131.571869	17.334861
37.624178	1133.775606	17.339879
37.407019	1140.201050	17.344896
37.333600	1127.220197	17.349914
37.035498	1131.380927	17.354931
37.559382	1122.034264	17.359949
37.641725	1127.765457	17.364967
37.240307	1120.694559	17.369984
37.750897	1115.573367	17.375002
37.430383	1116.951990	17.380019
37.675791	1115.632421	17.385037
37.435718	1106.566475	17.390055
37.431013	1121.728741	17.395072
37.652195	1124.051248	17.400090
37.263890	1135.076528	17.405107
37.881596	1123.179317	17.410125
37.408625	1121.658157	17.415143
37.423932	1129.765747	17.420160
37.704280	1124.490947	17.425178
37.591371	1133.380290	17.430195
37.546596	1127.208858	17.435213
37.851929	1130.611140	17.440231
37.792789	1132.732976	17.445248
37.759355	1115.500386	17.450266
37.541771	1145.836190	17.455283
37.808402	1149.098365	17.460301
38.301658	1156.772685	17.465319
37.759374	1157.403354	17.470336
38.182667	1158.419547	17.475354
38.104571	1163.547164	17.480371
38.356117	1149.254535	17.485389
38.295475	1160.999891	17.490407
38.183274	1157.796337	17.495424
38.494260	1145.287389	17.500442
38.344064	1158.015959	17.505459
38.434957	1152.016351	17.510477
38.444648	1157.612860	17.515495
38.325465	1150.292451	17.520512
38.599402	1149.835021	17.525530
38.494330	1156.646843	17.530547
38.466610	1150.348417	17.535565
38.343648	1149.979454	17.540583
38.223225	1145.761092	17.545600
38.410960	1138.758236	17.550618
38.161696	1157.088127	17.555635
38.731425	1166.458475	17.560653
39.143254	1168.929899	17.565671
38.677745	1178.136614	17.570688
38.908398	1172.235825	17.575706
38.976816	1184.369583	17.580723
39.088968	1178.000077	17.585741
39.081385	1171.806964	17.590759
38.762913	1176.210044	17.595776
39.165845	1161.547210	17.600794
38.812927	1176.503960	17.605811
38.973164	1164.630914	17.610829
39.048554	1167.426543	17.615847
39.040635	1165.415951	17.620864
39.100634	1169.488120	17.625882
39.384536	1168.629572	17.630899
39.906900	1156.703498	17.635917
39.537455	1164.858313	17.640935
39.520158	1167.259757	17.645952
39.929471	1162.525918	17.650970
39.495117	1147.792150	17.655987
39.335934	1127.600444	17.661005
39.355758	1136.212231	17.666023
39.070304	1146.917538	17.671040
39.709185	1156.833672	17.676058
39.297058	1163.530882	17.681075
39.423512	1158.760362	17.686093
39.591742	1167.840831	17.691111
39.333838	1166.194136	17.696128
39.863258	1165.618885	17.701146
39.862117	1164.360653	17.706163
39.672041	1153.012225	17.711181
40.104661	1164.398932	17.716199
39.817861	1163.670726	17.721216
39.740814	1154.960976	17.726234
39.786049	1166.708327	17.731251
39.813636	1158.659826	17.736269
40.146919	1161.359270	17.741287
39.874622	1164.373935	17.746304
40.121827	1171.359231	17.751322
40.137421	1194.954052	17.756339
40.357238	1189.555182	17.761357
40.691352	1188.547059	17.766375
40.406951	1171.936418	17.771392
40.104513	1164.285023	17.776410
40.201984	1167.915511	17.781427
40.368431	1177.251087	17.786445
40.543427	1182.206219	17.791463
40.429899	1182.233706	17.796480
40.529228	1172.028256	17.801498
40.591305	1191.321514	17.806515
40.918177	1181.694790	17.811533
40.751336	1190.248294	17.816551
40.435154	1185.051308	17.821568
41.110058	1171.012019	17.826586
40.715722	1172.789365	17.831603
40.364147	1155.089966	17.836621
40.746807	1173.599080	17.841639
40.477374	1173.495710	17.846656
41.025046	1177.114171	17.851674
40.826267	1186.297227	17.856691
40.622447	1182.301357	17.861709
40.934957	1182.188542	17.866727
40.650706	1173.920792	17.871744
41.044815	1187.330177	17.876762
40.669741	1178.292009	17.881779
40.818977	1183.090809	17.886797
41.238914	1190.432365	17.891815
40.694594	1211.272620	17.896832
41.051179	1197.038693	17.901850
41.024225	1217.746110	17.906867
41.041167	1213.581322	17.911885
41.450561	1211.181714	17.916903
41.161899	1212.045629	17.921920
41.329929	1206.738378	17.926938
41.713410	1208.088099	17.931955
41.375890	1209.500901	17.936973
41.663570	1205.374730	17.941991
41.104595	1209.229465	17.947008
41.538931	1195.980389	17.952026
41.812739	1209.199780	17.957043
41.647888	1202.489067	17.962061
42.059273	1195.851617	17.967079
41.703711	1211.128133	17.972096
41.460086	1212.332488	17.977114
41.615320	1219.065073	17.982131
42.141028	1235.151128	17.987149
42.483521	1236.151901	17.992167
42.130131	1226.092543	17.997184
42.087853	1213.683919	18.002202
41.937372	1206.019278	18.007219
41.886880	1202.382748	18.012237
42.204399	1214.280186	18.017255
42.247730	1233.812433	18.022272
42.058559	1237.007329	18.027290
42.263167	1224.041820	18.032307
42.200282	1233.060094	18.037325
42.428926	1238.783728	18.042343
42.337169	1243.787716	18.047360
42.308872	1226.115320	18.052378
42.602583	1221.428212	18.057395
42.157754	1237.245931	18.062413
42.417013	1225.975213	18.067431
42.304925	1228.717387	18.072448
42.371822	1228.464427	18.077466
42.228777	1230.351133	18.082483
42.181612	1224.123413	18.087501
42.920016	1242.473639	18.092519
42.829806	1259.826656	18.097536
42.748221	1253.091630	18.102554
43.190783	1250.655266	18.107571
42.589274	1257.714616	18.112589
43.403925	1246.267221	18.117607
42.867081	1256.990679	18.122624
42.834957	1261.038243	18.127642
42.998254	1248.209857	18.132659
42.673823	1260.401614	18.137677
43.402192	1246.201150	18.142695
42.889153	1268.617317	18.147712
43.097168	1250.491943	18.152730
43.075274	1257.408518	18.157747
42.777317	1261.328599	18.162765
43.298691	1249.698323	18.167783
43.324950	1239.988948	18.172800
43.251783	1256.011669	18.177818
43.316612	1250.321331	18.182835
43.273792	1274.248053	18.187853
43.502197	1269.316526	18.192871
43.698368	1281.382802	18.197888
43.701736	1283.088869	18.202906
43.994426	1277.503746	18.207923
43.700186	1274.563568	18.212941
43.693161	1273.647598	18.217959
44.001914	1271.891641	18.222976
44.021357	1263.937185	18.227994
43.908690	1251.634132	18.233011
43.682215	1234.194670	18.238029
43.936037	1255.659569	18.243047
43.943213	1268.740648	18.248064
44.295024	1273.999507	18.253082
44.051636	1265.039377	18.258099
44.347192	1275.932103	18.263117
43.965724	1258.196448	18.268135
43.952382	1266.851354	18.273152
44.557670	1257.899018	18.278170
44.396003	1270.851303	18.283187
44.177485	1263.398821	18.288205
44.477236	1263.036368	18.293223
44.344019	1272.072174	18.298240
44.341760	1271.282853	18.303258
44.140120	1265.199297	18.308275
44.242414	1257.851376	18.313293
44.280564	1269.315235	18.318311
44.378415	1263.802088	18.323328
44.482239	1270.056853	18.328346
44.505506	1268.555630	18.333363
44.201646	1272.841582	18.338381
44.725467	1275.881879	18.343399
44.673680	1297.475800	18.348416
44.505953	1290.218116	18.353434
44.914788	1285.007707	18.358451
44.828905	1290.905788	18.363469
45.081037	1284.317291	18.368487
45.123280	1284.681715	18.373504
44.839500	1290.381705	18.378522
44.920855	1290.268005	18.383539
44.917426	1287.577161	18.388557
44.981726	1276.565577	18.393575
44.904812	1287.242446	18.398592
44.682883	1305.775796	18.403610
45.294332	1309.536698	18.408627
45.013012	1324.980810	18.413645
45.491678	1319.290509	18.418663
45.531008	1322.842222	18.423680
45.383476	1316.827091	18.428698
45.666266	1315.224701	18.433715
45.387653	1308.195468	18.438733
45.897107	1319.541733	18.443751
45.760865	1309.889686	18.448768
45.472063	1306.052047	18.453786
46.028081	1305.629847	18.458803
45.881130	1313.428376	18.463821
45.866815	1300.288510	18.468839
46.003288	1310.962825	18.473856
45.987398	1298.984056	18.478874
46.287590	1308.982627	18.483891
45.826148	1315.662603	18.488909
46.048667	1295.162832	18.493927
46.193984	1308.358763	18.498944
45.910329	1305.292627	18.503962
46.436145	1299.198428	18.508979
45.898380	1313.749088	18.513997
46.161713	1308.561876	18.519015
46.098118	1297.834930	18.524032
46.116059	1295.831206	18.529050
45.886052	1292.308223	18.534067
46.019255	1301.814344	18.539085
46.430745	1315.858127	18.544103
46.392463	1320.661712	18.549120
46.541022	1332.619226	18.554138
46.635686	1324.589822	18.559155
47.003048	1330.791573	18.564173
46.504781	1336.928467	18.569191
46.627911	1329.855601	18.574208
46.606840	1325.728302	18.579226
46.864293	1322.105549	18.584243
46.806042	1325.323627	18.589261
46.682771	1324.183956	18.594279
46.823494	1318.623054	18.599296
46.832206	1325.704661	18.604314
46.659435	1317.513426	18.609331
46.735281	1324.522980	18.614349
46.702914	1352.205974	18.619367
47.159579	1357.814643	18.624384
47.332942	1351.787643	18.629402
47.248198	1354.731538	18.634419
47.236744	1355.626753	18.639437
47.491935	1354.209652	18.644455
47.728503	1354.066479	18.649472
47.317646	1364.922501	18.654490
47.317265	1349.041832	18.659507
47.425416	1353.642756	18.664525
47.323189	1357.358620	18.669543
47.502094	1351.506909	18.674560
47.566826	1356.987755	18.679578
47.872758	1343.598582	18.684595
47.647307	1347.865758	18.689613
47.923407	1349.059593	18.694631
48.044752	1354.490512	18.699648
47.845395	1349.837955	18.704666
47.825840	1347.086754	18.709683
47.845524	1342.441737	18.714701
47.813180	1350.495704	18.719719
47.625910	1353.246745	18.724736
47.999868	1369.055143	18.729754
48.321065	1370.502900	18.734771
47.852267	1388.317555	18.739789
48.070291	1374.634072	18.744807
48.038975	1378.679967	18.749824
47.768946	1374.557753	18.754842
48.150621	1383.571285	18.759859
48.434903	1379.719305	18.764877
48.520598	1371.807704	18.769895
48.414528	1380.120402	18.774912
48.330173	1376.350807	18.779930
48.675917	1376.125730	18.784947
48.450787	1382.352785	18.789965
48.569852	1398.587243	18.794983
49.014226	1410.582585	18.800000
48.697598	1415.826982	18.805018
48.963192	1410.898914	18.810035
48.862895	1412.912528	18.815053
49.002101	1405.980202	18.820071
49.088746	1408.877899	18.825088
48.819704	1409.380058	18.830106
49.021261	1403.502692	18.835123
48.912942	1398.075855	18.840141
49.050131	1408.896415	18.845159
49.097305	1390.768203	18.850176
48.884078	1415.700724	18.855194
49.321845	1404.640491	18.860211
48.869482	1402.447499	18.865229
49.114405	1401.895593	18.870247
49.532735	1408.040487	18.875264
49.470073	1427.737759	18.880282
49.532759	1432.646397	18.885299
49.792611	1442.542959	18.890317
49.258290	1439.606430	18.895335
49.953968	1428.454712	18.900352
49.704487	1438.508003	18.905370
49.674356	1432.184672	18.910387
50.011966	1430.815766	18.915405
49.783421	1433.641042	18.920423
49.908268	1436.219630	18.925440
49.580862	1435.746415	18.930458
50.058928	1427.316046	18.935475
49.788139	1429.238879	18.940493
49.960548	1440.582365	18.945511
50.169752	1432.918440	18.950528
49.879590	1442.149263	18.955546
49.779870	1443.288215	18.960563
49.688651	1445.017250	18.965581
49.898346	1458.654496	18.970599
50.030741	1465.716445	18.975616
50.121066	1477.735275	18.980634
50.249244	1463.020005	18.985651
50.172637	1467.104607	18.990669
50.383296	1471.933033	18.995687
50.574959	1484.722983	19.000704
50.588903	1492.450332	19.005722
50.977871	1497.777278	19.010739
50.955400	1495.768961	19.015757
50.499977	1490.853611	19.020775
51.059686	1486.097256	19.025792
50.928129	1485.259333	19.030810
50.819516	1492.523322	19.035827
51.007262	1496.553189	19.040845
51.064741	1497.105520	19.045863
51.184985	1493.186865	19.050880
50.894549	1499.153831	19.055898
51.017560	1499.617063	19.060915
51.188464	1485.075849	19.065933
51.127905	1488.113439	19.070951
51.190975	1483.868859	19.075968
50.981527	1498.170720	19.080986
51.165629	1489.351481	19.086003
51.478626	1492.214669	19.091021
51.024244	1493.068849	19.096039
51.455681	1494.060176	19.101056
51.733118	1512.836612	19.106074
51.932825	1524.465239	19.111091
51.729050	1526.496944	19.116109
51.742242	1529.239643	19.121127
51.953640	1520.705462	19.126144
51.707060	1522.682647	19.131162
51.569866	1518.138096	19.136179
51.656800	1524.274545	19.141197
51.804084	1525.926228	19.146215
52.189903	1509.085618	19.151232
52.003098	1520.920598	19.156250
51.818879	1517.816535	19.161267
51.928385	1513.023435	19.166285
51.845220	1513.569883	19.171303
52.368656	1534.388173	19.176320
52.424685	1545.710977	19.181338
52.434497	1543.777727	19.186355
52.625571	1543.994157	19.191373
52.468661	1547.275208	19.196391
52.599319	1537.377529	19.201408
52.921375	1539.992323	19.206426
52.573127	1536.794869	19.211443
52.739455	1536.538630	19.216461
52.721601	1539.781773	19.221479
52.969655	1524.699693	19.226496
52.937068	1545.366006	19.231514
52.623831	1543.009234	19.236531
52.730054	1539.517509	19.241549
52.803515	1529.326944	19.246567
53.165582	1537.454964	19.251584
52.910314	1530.546165	19.256602
52.953673	1542.695232	19.261619
53.095076	1534.889487	19.266637
53.017040	1531.339062	19.271655
53.145278	1528.784474	19.276672
52.939391	1536.461964	19.281690
53.246927	1558.628164	19.286707
53.693332	1550.424565	19.291725
53.324515	1572.266079	19.296743
53.545840	1570.739531	19.301760
53.696374	1565.021244	19.306778
53.610480	1559.903796	19.311795
53.687282	1561.797953	19.316813
53.496319	1567.683018	19.321831
53.676068	1561.791763	19.326848
53.905691	1563.614360	19.331866
54.013129	1555.832896	19.336883
54.127013	1559.106942	19.341901
53.998610	1558.383339	19.346919
54.161917	1554.133765	19.351936
54.333772	1556.530276	19.356954
54.219609	1556.276299	19.361971
54.313846	1553.801059	19.366989
54.086299	1560.000261	19.372007
54.332743	1553.484908	19.377024
53.867034	1565.362830	19.382042
53.789306	1556.445311	19.387059
54.548509	1564.206424	19.392077
54.605744	1574.928177	19.397095
54.274832	1582.199349	19.402112
54.538820	1584.620497	19.407130
54.882157	1578.269001	19.412147
54.704994	1595.085739	19.417165
54.503614	1586.132867	19.422183
54.847125	1583.191588	19.427200
54.528234	1580.821554	19.432218
54.886589	1582.334193	19.437235
54.650863	1588.677853	19.442253
54.511551	1588.561590	19.447271
54.992504	1594.155469	19.452288
54.713851	1610.426852	19.457306
54.747257	1616.836140	19.462323
54.752268	1619.728022	19.467341
54.766206	1620.117419	19.472359
55.147770	1619.534276	19.477376
55.366551	1631.664879	19.482394
55.083494	1647.259044	19.487411
55.785385	1635.313389	19.492429
55.596582	1651.394313	19.497447
55.939777	1645.261458	19.502464
55.881892	1641.795880	19.507482
55.782027	1651.720066	19.512499
55.973863	1638.542298	19.517517
55.842525	1643.488242	19.522535
56.157528	1634.756576	19.527552
55.990050	1633.221243	19.532570
56.160500	1634.074881	19.537587
55.965104	1617.278075	19.542605
55.885193	1634.936632	19.547623
56.060754	1625.596438	19.552640
55.848973	1650.771372	19.557658
55.758451	1644.089498	19.562675
56.222680	1643.186437	19.567693
56.093039	1639.438153	19.572711
56.154231	1629.468121	19.577728
56.428866	1636.584547	19.582746
56.145752	1640.013158	19.587763
56.450891	1642.553592	19.592781
56.494497	1658.004439	19.597799
56.675915	1663.062532	19.602816
57.049492	1662.342238	19.607834
56.910455	1661.804366	19.612851
57.340779	1660.839072	19.617869
56.716292	1649.946489	19.622887
56.244315	1655.385629	19.627904
56.532482	1659.146275	19.632922
56.593752	1669.880038	19.637939
56.765941	1658.301981	19.642957
56.905008	1666.289462	19.647975
57.076343	1663.353603	19.652992
57.629219	1678.792467	19.658010
57.536856	1674.898231	19.663027
57.633399	1668.932115	19.668045
57.209460	1671.393775	19.673063
57.295707	1665.103691	19.678080
57.551574	1678.614233	19.683098
57.589359	1685.740142	19.688115
57.850019	1685.865254	19.693133
57.705489	1694.874813	19.698151
57.736950	1693.208647	19.703168
57.627010	1695.126312	19.708186
57.756952	1688.771049	19.713203
57.703751	1690.454724	19.718221
57.729578	1685.078745	19.723239
57.805692	1683.119172	19.728256
57.912384	1682.597167	19.733274
57.855612	1688.467172	19.738291
58.371928	1680.917732	19.743309
58.175001	1698.278854	19.748327
58.079828	1705.990685	19.753344
58.647641	1707.377126	19.758362
58.353096	1713.421912	19.763379
58.584473	1715.049195	19.768397
58.641003	1712.145793	19.773415
58.361498	1708.874416	19.778432
58.723240	1699.147411	19.783450
58.148544	1730.382945	19.788467
58.486015	1720.686537	19.793485
58.623710	1719.733302	19.798503
58.784246	1717.241169	19.803520
58.802552	1712.237608	19.808538
58.764864	1716.135178	19.813555
59.031929	1731.056542	19.818573
59.103396	1743.489155	19.823591
59.011612	1742.390046	19.828608
59.538452	1739.724663	19.833626
59.074708	1751.045577	19.838643
59.292259	1735.656688	19.843661
59.450489	1740.333118	19.848679
59.363300	1738.398009	19.853696
59.396762	1730.027361	19.858714
59.394362	1735.574112	19.863731
59.624220	1732.158577	19.868749
59.355058	1729.135654	19.873767
59.384680	1740.055413	19.878784
59.223740	1737.181968	19.883802
59.188426	1731.359550	19.888819
59.443520	1755.845164	19.893837
59.684114	1770.457761	19.898855
59.770398	1764.114147	19.903872
60.056771	1773.055035	19.908890
59.828157	1764.933799	19.913907
60.223607	1760.481977	19.918925
60.334490	1760.961308	19.923943
60.135108	1766.114772	19.928960
60.132855	1760.417629	19.933978
60.041653	1767.010449	19.938995
60.290913	1775.842427	19.944013
60.457110	1786.822237	19.949031
60.310173	1794.575404	19.954048
60.402356	1792.768983	19.959066
60.102745	1802.806923	19.964083
60.292152	1777.396083	19.969101
60.342553	1794.802819	19.974119
60.701946	1821.713230	19.979136
61.141185	1812.157834	19.984154
61.058274	1811.087192	19.989171
61.418190	1805.363734	19.994189
61.624077	1806.427235	19.999207
61.736717	1799.347950	20.004224
61.452766	1788.105227	20.009242
61.496666	1782.292177	20.014259
61.531831	1767.666937	20.019277
61.610585	1772.735148	20.024295
61.431039	1785.800854	20.029312
61.406373	1771.193017	20.034330
61.457194	1776.940507	20.039347
61.340525	1770.676446	20.044365
61.494736	1791.245680	20.049383
61.674463	1804.999716	20.054400
62.097162	1791.114888	20.059418
62.047305	1808.551787	20.064435
61.994216	1811.286234	20.069453
61.744724	1805.398842	20.074471
61.753993	1809.188274	20.079488
62.028843	1797.625195	20.084506
61.802194	1804.894006	20.089523
61.975787	1813.245721	20.094541
61.639137	1808.360082	20.099559
61.917789	1802.059705	20.104576
61.987580	1815.809261	20.109594
61.871208	1833.590277	20.114611
62.196914	1834.384562	20.119629
62.330208	1833.981004	20.124647
62.475171	1850.192963	20.129664
62.811184	1825.575056	20.134682
62.606213	1831.841557	20.139699
62.720562	1824.623562	20.144717
62.565705	1834.573945	20.149735
62.716259	1850.888833	20.154752
62.913657	1862.367090	20.159770
63.046318	1865.373944	20.164787
63.371860	1860.297740	20.169805
63.231276	1857.194510	20.174823
63.247146	1863.232325	20.179840
63.467259	1859.893820	20.184858
63.318682	1861.551827	20.189875
63.101310	1870.684796	20.194893
63.230938	1859.914034	20.199911
62.963598	1873.715836	20.204928
63.340412	1854.645718	20.209946
62.922663	1873.420231	20.214963
63.415444	1875.839548	20.219981
63.901497	1892.130865	20.224999
63.602214	1891.862359	20.230016
63.927978	1885.227244	20.235034
64.088590	1891.204234	20.240051
64.288516	1880.483595	20.245069
64.103730	1876.986289	20.250087
63.943092	1876.096350	20.255104
64.479825	1882.968181	20.260122
64.293937	1884.814612	20.265139
64.384931	1879.914232	20.270157
64.200625	1875.688539	20.275175
64.302229	1884.108404	20.280192
64.486723	1880.847935	20.285210
64.227386	1880.071264	20.290227
64.300062	1882.102975	20.295245
65.050325	1891.256248	20.300263
64.581084	1903.526689	20.305280
65.098900	1899.870139	20.310298
64.568814	1906.342677	20.315315
65.075211	1918.762709	20.320333
64.918936	1896.562282	20.325351
64.917019	1913.626720	20.330368
64.842741	1914.170192	20.335386
65.142257	1911.787998	20.340403
65.062003	1912.810623	20.345421
65.334307	1902.666737	20.350439
65.355300	1903.391644	20.355456
65.365427	1909.556235	20.360474
65.261141	1907.796863	20.365491
65.583279	1904.210843	20.370509
65.735085	1903.936466	20.375527
65.238063	1911.751816	20.380544
65.215094	1910.493855	20.385562
65.653615	1917.972823	20.390579
65.414457	1939.286121	20.395597
65.795162	1926.579769	20.400615
65.590147	1928.006110	20.405632
65.785777	1922.574649	20.410650
66.055026	1934.208247	20.415667
66.240405	1938.185133	20.420685
66.474216	1932.472299	20.425703
66.131802	1944.876707	20.430720
66.314211	1948.452947	20.435738
66.451619	1960.195680	20.440755
66.666945	1954.319044	20.445773
66.609840	1964.362466	20.450791
66.617590	1968.004318	20.455808
66.993930	1939.868777	20.460826
66.914335	1948.467015	20.465843
67.157111	1942.645781	20.470861
67.269867	1921.923531	20.475879
67.025103	1918.656004	20.480896
67.557810	1912.049222	20.485914
67.413542	1907.172194	20.490931
67.023378	1912.304224	20.495949
67.540893	1911.568831	20.500967
67.146214	1911.291941	20.505984
67.097776	1906.978505	20.511002
67.428174	1915.382351	20.516019
67.226346	1915.652008	20.521037
67.587104	1917.252391	20.526055
67.383612	1922.491508	20.531072
67.252046	1937.564747	20.536090
67.501629	1952.053399	20.541107
67.683246	1947.034725	20.546125
67.879661	1944.093238	20.551143
67.428003	1959.104288	20.556160
67.477812	1955.365056	20.561178
67.800057	1960.199447	20.566195
67.966185	1971.300532	20.571213
68.308239	1974.296039	20.576231
67.723768	1982.309417	20.581248
67.953287	1970.854104	20.586266
67.982492	1979.960402	20.591283
67.870862	1978.301293	20.596301
68.162455	1989.159012	20.601319
68.396499	2006.371548	20.606336
68.581632	2004.602189	20.611354
68.531580	2002.731908	20.616371
68.626630	2003.938943	20.621389
68.888519	1999.786777	20.626407
69.039342	1998.557722	20.631424
69.343172	1999.453034	20.636442
69.162391	2000.900686	20.641459
69.003071	1996.777940	20.646477
69.247858	1991.591873	20.651495
69.339715	1995.188858	20.656512
69.169533	2002.623369	20.661530
69.396595	1988.772699	20.666547
69.087374	2002.317031	20.671565
69.590871	1997.110154	20.676583
69.405750	2001.457605	20.681600
69.427252	1994.063994	20.686618
69.832791	1995.193200	20.691635
69.531021	1997.446664	20.696653
69.512469	1995.620124	20.701671
69.601898	2018.819119	20.706688
69.816454	2017.792259	20.711706
70.363136	2013.302087	20.716723
70.167862	2020.783081	20.721741
70.437303	2006.417544	20.726759
70.452074	2012.896047	20.731776
69.963122	2024.380068	20.736794
70.344789	2009.011909	20.741811
70.069276	2015.576032	20.746829
70.222105	2001.510670	20.751847
70.378572	2021.129757	20.756864
70.167669	2013.093647	20.761882
70.749740	2024.804847	20.766899
70.838070	2044.771463	20.771917
70.832543	2040.358334	20.776935
70.805915	2044.642769	20.781952
70.975732	2042.811353	20.786970
71.080310	2043.058890	20.791987
70.836238	2046.080242	20.797005
71.087464	2040.941895	20.802023
70.920172	2036.645801	20.807040
71.266039	2033.877093	20.812058
71.389538	2032.403853	20.817075
71.297854	2028.691886	20.822093
71.469033	2030.921843	20.827111
71.719451	2031.909047	20.832128
71.750824	2047.530575	20.837146
71.676706	2041.701635	20.842163
71.591099	2049.604034	20.847181
71.883857	2056.260024	20.852199
71.897787	2054.214363	20.857216
71.727816	2053.977141	20.862234
72.085044	2047.470644	20.867251
71.504937	2050.070527	20.872269
72.024877	2044.463032	20.877287
72.120375	2052.344416	20.882304
72.129698	2073.203001	20.887322
72.237103	2077.742927	20.892339
72.345836	2090.070793	20.897357
72.387788	2076.189784	20.902375
72.417021	2077.905976	20.907392
72.768808	2084.546274	20.912410
72.750061	2069.540785	20.917427
72.683777	2093.486758	20.922445
72.809271	2077.970614	20.927463
73.037146	2077.594440	20.932480
72.808091	2068.881637	20.937498
72.730661	2079.093549	20.942515
72.752509	2084.649151	20.947533
73.391534	2086.032144	20.952551
73.432567	2091.918174	20.957568
73.404672	2098.121944	20.962586
73.753793	2094.106853	20.967603
73.593094	2101.865523	20.972621
73.661701	2094.146595	20.977639
73.761502	2089.386314	20.982656
73.727662	2097.247449	20.987674
74.114245	2089.145902	20.992691
73.774098	2099.308488	20.997709
73.752137	2086.722841	21.002727
73.540292	2091.129636	21.007744
73.756578	2088.716642	21.012762
74.022366	2092.145913	21.017779
73.633342	2099.195369	21.022797
74.011970	2112.944721	21.027815
74.397753	2118.305443	21.032832
74.388218	2112.615616	21.037850
74.329848	2117.221317	21.042867
74.095417	2127.673808	21.047885
74.648059	2106.832382	21.052903
74.605553	2116.799648	21.057920
74.457011	2117.161485	21.062938
74.684786	2127.966564	21.067955
74.955401	2147.359977	21.072973
75.163589	2140.070230	21.077991
75.395225	2142.576860	21.083008
75.688332	2149.943857	21.088026
75.607444	2140.892772	21.093043
75.376794	2149.288697	21.098061
75.439109	2141.304901	21.103079
75.342523	2143.789939	21.108096
75.455617	2142.164187	21.113114
76.186187	2143.282472	21.118131
75.806004	2146.726679	21.123149
75.679637	2152.685049	21.128167
75.978963	2140.829926	21.133184
75.854941	2143.235967	21.138202
75.694413	2136.031764	21.143219
75.757711	2147.383768	21.148237
76.142126	2145.024179	21.153255
75.938524	2129.587202	21.158272
75.415665	2155.665211	21.163290
76.027498	2163.969266	21.168307
76.174936	2180.130863	21.173325
76.133385	2175.176014	21.178343
75.908213	2180.170137	21.183360
75.858324	2173.149624	21.188378
76.461017	2195.304340	21.193395
76.063277	2193.500492	21.198413
76.324975	2211.709327	21.203431
76.897548	2199.881370	21.208448
76.521876	2216.087100	21.213466
77.156024	2213.862285	21.218483
77.358503	2225.028555	21.223501
77.405978	2229.730673	21.228519
77.681483	2217.224894	21.233536
77.686251	2215.586522	21.238554
77.618043	2189.772440	21.243571
77.323046	2196.435706	21.248589
77.587646	2189.427956	21.253607
77.735572	2197.502409	21.258624
77.637731	2215.361163	21.263642
77.794750	2210.884308	21.268659
78.057572	2220.046313	21.273677
78.138814	2220.135549	21.278695
78.389934	2217.630461	21.283712
78.300913	2217.224593	21.288730
78.377994	2204.018995	21.293747
78.246650	2199.141380	21.298765
78.317758	2207.235955	21.303783
78.576565	2211.457617	21.308800
78.348513	2212.234839	21.313818
78.514962	2205.720942	21.318835
78.233189	2209.495543	21.323853
78.309934	2217.623832	21.328871
78.464926	2219.894154	21.333888
78.394324	2219.755915	21.338906
78.231929	2232.525123	21.343923
78.561619	2246.946240	21.348941
78.575737	2239.715707	21.353959
78.960681	2235.344073	21.358976
78.612125	2245.980020	21.363994
79.254273	2252.474989	21.369011
79.427578	2261.298929	21.374029
79.190205	2260.271761	21.379047
79.343616	2256.363344	21.384064
79.529488	2263.297604	21.389082
79.725923	2255.452810	21.394099
79.592424	2264.862092	21.399117
79.817272	2281.341801	21.404135
80.190871	2279.465275	21.409152
80.173486	2290.567554	21.414170
80.412138	2280.008765	21.419187
80.422614	2279.522533	21.424205
80.364974	2285.466850	21.429223
80.571671	2279.224936	21.434240
80.632899	2281.466174	21.439258
80.677282	2274.930813	21.444275
80.525489	2269.183383	21.449293
80.651198	2277.851324	21.454311
80.494440	2272.274576	21.459328
80.595825	2282.272494	21.464346
80.904286	2285.993890	21.469363
81.115974	2281.991227	21.474381
80.918312	2289.389366	21.479399
81.194192	2284.901399	21.484416
80.872560	2282.909218	21.489434
80.835327	2281.209894	21.494451
81.265895	2293.470880	21.499469
81.149786	2283.879468	21.504487
81.051775	2277.492658	21.509504
81.146100	2301.863259	21.514522
81.246590	2318.117442	21.519539
81.113465	2313.482325	21.524557
81.162998	2318.744157	21.529575
81.459694	2320.693014	21.534592
81.545219	2330.221572	21.539610
82.333807	2331.686924	21.544627
81.980988	2336.517406	21.549645
82.074753	2340.912508	21.554663
82.565028	2328.865544	21.559680
82.142247	2334.348209	21.564698
81.959323	2334.115406	21.569715
81.976183	2341.105757	21.574733
82.326937	2357.928069	21.579751
82.693461	2356.981562	21.584768
82.680719	2372.074056	21.589786
82.776786	2358.281679	21.594803
82.822392	2354.793135	21.599821
82.959718	2358.113964	21.604839
83.274371	2354.912074	21.609856
83.104456	2353.340082	21.614874
82.994375	2349.313992	21.619891
83.655537	2357.658273	21.624909
83.424383	2372.920882	21.629927
83.901120	2351.993681	21.634944
83.817949	2356.194413	21.639962
83.871683	2346.517671	21.644979
83.942263	2345.617572	21.649997
83.706960	2347.564750	21.655015
83.994572	2332.661150	21.660032
83.918815	2344.002448	21.665050
84.027519	2358.841174	21.670067
84.289085	2373.600480	21.675085
84.229544	2372.622813	21.680103
84.308883	2364.577189	21.685120
84.535162	2374.001531	21.690138
84.598622	2365.513258	21.695155
84.319632	2368.726653	21.700173
84.411930	2372.896262	21.705191
84.766727	2368.901429	21.710208
84.416018	2368.074803	21.715226
84.487261	2373.521175	21.720243
84.751104	2377.482526	21.725261
84.444661	2394.113943	21.730279
84.759441	2389.498614	21.735296
84.781350	2401.091018	21.740314
84.979728	2403.790194	21.745331
85.029885	2404.433394	21.750349
84.822856	2426.016782	21.755367
85.435842	2416.715657	21.760384
85.126013	2432.349537	21.765402
85.311364	2419.260977	21.770419
85.527673	2424.193433	21.775437
85.639357	2427.167570	21.780455
85.850798	2433.350620	21.785472
85.881448	2446.400702	21.790490
85.829692	2442.201683	21.795507
85.849972	2441.562080	21.800525
85.745988	2451.570841	21.805543
85.686249	2442.317200	21.810560
85.867925	2462.973461	21.815578
86.473507	2468.572982	21.820595
86.684381	2468.267941	21.825613
87.044189	2466.491123	21.830631
86.989364	2463.267115	21.835648
87.015866	2472.801247	21.840666
87.325467	2461.342218	21.845683
87.599716	2460.570876	21.850701
87.191614	2462.163364	21.855719
87.639542	2454.279932	21.860736
87.588211	2459.236203	21.865754
87.903882	2450.833509	21.870771
87.734331	2425.425294	21.875789
87.483979	2424.438723	21.880807
87.699230	2415.053941	21.885824
87.347806	2427.549859	21.890842
87.864757	2442.493462	21.895859
87.449974	2438.280760	21.900877
87.613667	2456.787115	21.905895
87.552310	2447.532942	21.910912
87.644032	2450.130367	21.915930
87.821752	2465.758896	21.920947
87.904670	2478.018847	21.925965
88.009280	2477.014209	21.930983
87.999070	2476.019229	21.936000
87.878189	2494.475054	21.941018
88.212443	2502.019722	21.946035
88.455340	2507.102917	21.951053
88.446471	2511.426344	21.956071
88.404275	2512.343050	21.961088
88.861016	2524.188695	21.966106
89.222682	2537.982059	21.971123
89.304998	2537.681786	21.976141
89.199631	2537.529424	21.981159
89.573184	2527.187268	21.986176
89.624159	2540.071378	21.991194
89.706483	2525.056380	21.996211
89.628431	2525.170235	22.001229
89.697123	2530.811350	22.006247
89.529050	2523.985699	22.011264
89.927892	2531.683685	22.016282
89.891726	2523.462116	22.021299
90.014675	2525.300276	22.026317
89.970179	2529.700966	22.031335
90.156172	2520.549668	22.036352
90.277550	2525.994395	22.041370
90.017383	2533.745559	22.046387
90.369614	2549.587821	22.051405
90.595452	2553.571012	22.056423
90.441549	2557.127100	22.061440
90.554241	2554.905951	22.066458
90.826606	2539.848048	22.071475
90.329683	2557.169151	22.076493
90.754666	2559.564795	22.081511
90.654278	2548.193101	22.086528
91.022732	2572.535387	22.091546
91.250114	2576.630815	22.096563
91.505524	2576.240015	22.101581
91.209170	2581.236186	22.106599
91.307317	2574.101418	22.111616
91.444728	2576.081218	22.116634
91.456832	2576.806003	22.121651
91.848001	2571.635717	22.126669
91.732209	2579.925479	22.131687
91.713466	2560.006695	22.136704
92.130147	2590.914509	22.141722
91.983171	2598.673614	22.146739
92.527025	2599.836662	22.151757
92.212306	2603.254015	22.156775
92.192757	2606.607784	22.161792
92.405830	2600.533825	22.166810
92.778111	2593.359266	22.171827
92.701225	2589.253879	22.176845
92.570689	2603.954818	22.181863
93.079057	2595.183096	22.186880
92.992996	2593.952440	22.191898
92.576440	2598.527317	22.196915
93.005709	2600.565977	22.201933
93.007340	2619.608854	22.206951
92.651985	2620.886978	22.211968
92.922554	2624.484725	22.216986
92.981162	2625.804596	22.222003
93.331844	2642.781415	22.227021
93.376985	2652.254487	22.232039
93.627340	2652.178327	22.237056
93.664125	2655.935277	22.242074
93.639183	2653.984612	22.247091
94.004539	2637.705207	22.252109
94.164213	2652.513295	22.257127
93.994595	2660.271323	22.262144
94.342120	2669.785069	22.267162
94.517634	2670.394133	22.272179
94.557498	2670.711780	22.277197
94.452340	2680.037369	22.282215
94.607580	2667.261718	22.287232
94.589139	2673.837052	22.292250
94.511850	2667.888810	22.297267
95.097417	2667.124446	22.302285
94.919756	2665.014865	22.307303
94.731329	2658.390608	22.312320
95.288740	2678.234528	22.317338
95.442771	2685.668025	22.322355
95.331027	2692.719954	22.327373
95.463073	2691.808460	22.332391
95.662677	2697.575064	22.337408
95.732361	2693.142665	22.342426
96.070110	2699.097251	22.347443
96.004773	2682.391732	22.352461
95.816561	2691.366397	22.357479
95.694269	2693.571679	22.362496
95.938292	2692.068930	22.367514
96.401792	2690.041158	22.372531
95.985176	2683.663287	22.377549
96.142683	2684.607150	22.382567
96.378175	2709.508086	22.387584
96.559459	2707.504078	22.392602
96.455692	2720.847203	22.397619
96.467056	2723.917627	22.402637
96.255580	2724.033881	22.407655
96.401072	2727.255174	22.412672
96.544307	2737.571580	22.417690
96.745600	2748.132795	22.422707
96.683287	2742.769693	22.427725
97.059273	2754.502556	22.432743
97.361891	2765.912055	22.437760
97.663755	2769.888689	22.442778
97.710987	2787.223185	22.447795
98.139505	2764.698500	22.452813
98.397716	2773.559554	22.457831
98.183131	2768.580968	22.462848
98.184143	2770.184546	22.467866
98.168590	2767.482777	22.472883
98.546292	2765.595313	22.477901
98.222036	2769.962816	22.482919
98.123629	2770.281277	22.487936
98.192255	2758.876961	22.492954
98.059913	2759.155212	22.497971
98.639574	2758.785853	22.502989
98.660184	2771.126778	22.508007
98.531081	2776.297704	22.513024
98.709592	2780.950789	22.518042
98.801961	2783.804590	22.523059
98.782585	2783.220062	22.528077
99.179459	2796.393755	22.533095
99.275516	2815.712072	22.538112
99.451600	2801.991465	22.543130
99.473319	2820.003365	22.548147
99.797333	2818.605832	22.553165
99.871527	2814.693381	22.558183
99.682888	2813.279277	22.563200
99.809444	2814.567879	22.568218
99.869040	2814.395501	22.573235
99.960776	2805.958309	22.578253
100.093066	2820.612049	22.583271
100.249902	2823.804025	22.588288
100.807251	2829.077880	22.593306
100.404713	2841.778941	22.598323
100.599520	2832.771557	22.603341
100.985518	2831.803828	22.608359
100.484635	2842.813730	22.613376
100.917790	2830.428590	22.618394
100.883877	2832.265847	22.623411
100.945518	2835.121412	22.628429
100.737692	2823.571566	22.633447
100.649177	2838.302222	22.638464
101.354599	2848.336353	22.643482
101.273520	2861.603624	22.648499
101.451753	2855.656247	22.653517
101.267063	2855.606985	22.658535
101.309241	2859.772928	22.663552
101.586208	2870.857029	22.668570
102.102045	2876.551255	22.673587
102.217131	2878.069009	22.678605
102.160081	2873.304383	22.683623
102.449240	2884.296882	22.688640
102.778966	2868.129089	22.693658
102.739323	2868.845623	22.698675
102.573604	2873.130456	22.703693
102.496247	2868.504359	22.708711
102.543297	2871.415744	22.713728
102.827886	2874.629834	22.718746
102.699782	2879.507248	22.723763
103.008657	2892.482689	22.728781
103.475490	2896.470808	22.733799
103.152348	2905.257106	22.738816
103.477280	2895.131673	22.743834
103.467375	2904.700210	22.748851
103.432564	2900.545550	22.753869
103.584816	2898.437600	22.758887
103.355162	2905.250439	22.763904
104.399523	2886.950339	22.768922
104.659974	2907.140823	22.773939
104.854525	2885.053625	22.778957
104.963284	2883.909863	22.783975
104.619541	2878.571136	22.788992
105.052572	2874.971922	22.794010
104.913938	2870.069285	22.799027
104.860279	2879.769847	22.804045
104.776019	2878.249423	22.809063
104.432993	2876.726213	22.814080
104.811626	2874.681275	22.819098
104.523918	2883.686081	22.824115
104.850123	2878.987763	22.829133
104.915331	2896.046584	22.834151
104.996175	2904.117185	22.839168
105.194467	2906.993449	22.844186
105.445754	2910.439389	22.849203
105.163045	2906.966883	22.854221
105.427197	2922.775619	22.859239
105.556996	2936.313734	22.864256
105.544046	2930.891564	22.869274
105.844595	2947.916065	22.874291
105.600579	2942.177566	22.879309
106.155139	2944.359906	22.884327
105.592535	2969.215505	22.889344
106.103500	2961.487720	22.894362
105.902483	2980.039526	22.899379
105.778340	2976.458342	22.904397
106.358161	2989.378866	22.909415
106.594365	3002.204746	22.914432
106.835355	2990.625674	22.919450
107.125021	3000.864646	22.924467
106.679565	2998.923568	22.929485
107.084705	3017.989933	22.934503
107.046190	3024.346812	22.939520
107.525478	3018.062692	22.944538
107.442910	3027.453331	22.949555
107.666956	3029.296674	22.954573
107.935894	3018.259793	22.959591
107.481750	3029.477115	22.964608
107.772520	3047.849121	22.969626
108.097751	3045.864589	22.974643
108.379048	3045.508194	22.979661
108.991735	3029.478376	22.984679
108.727116	3043.919544	22.989696
109.032013	3026.187894	22.994714
109.240819	3036.423266	22.999731
109.272768	3032.811672	23.004749
109.504289	3023.334238	23.009767
109.107319	3007.954689	23.014784
109.294401	2992.293247	23.019802
109.398309	3004.631313	23.024819
109.048221	2996.634938	23.029837
109.539913	3008.326749	23.034855
109.491643	3023.335914	23.039872
109.735019	3027.754563	23.044890
109.718997	3024.536042	23.049907
109.799511	3028.209818	23.054925
109.907138	3031.238214	23.059943
109.368921	3032.598230	23.064960
109.755112	3033.827361	23.069978
109.851037	3057.036417	23.074995
109.888162	3063.961745	23.080013
110.093695	3047.301497	23.085031
109.907852	3072.260802	23.090048
110.100965	3086.670713	23.095066
110.282955	3084.853747	23.100083
110.126259	3097.507175	23.105101
110.423408	3113.573574	23.110119
110.424629	3119.762910	23.115136
110.777736	3129.464849	23.120154
111.011764	3149.275245	23.125171
111.028851	3151.029685	23.130189
111.614800	3148.574094	23.135207
111.479506	3143.502504	23.140224
111.441109	3150.903998	23.145242
111.949891	3142.841383	23.150259
112.276934	3158.957340	23.155277
112.244892	3150.604185	23.160295
112.438412	3152.151152	23.165312
112.630723	3137.150236	23.170330
112.409865	3141.638225	23.175347
112.398402	3148.666517	23.180365
113.035761	3144.294486	23.185383
112.830388	3164.530502	23.190400
112.884226	3158.388888	23.195418
112.939213	3159.081694	23.200435
113.063649	3162.378021	23.205453
113.142829	3168.075919	23.210471
113.261746	3156.453256	23.215488
113.227917	3155.708195	23.220506
113.175121	3156.743831	23.225523
113.316673	3163.512544	23.230541
113.445034	3169.438575	23.235559
113.321836	3176.669544	23.240576
113.679597	3175.655957	23.245594
113.802963	3179.347322	23.250611
113.907987	3202.253898	23.255629
114.340052	3202.615207	23.260647
114.125743	3219.233655	23.265664
114.487830	3207.992999	23.270682
114.395519	3206.407750	23.275699
114.223178	3213.350818	23.280717
114.656272	3223.184010	23.285735
114.695440	3241.720661	23.290752
115.075177	3236.823340	23.295770
115.024813	3237.849156	23.300787
115.123776	3235.631667	23.305805
115.262562	3231.891293	23.310823
115.672273	3251.426042	23.315840
115.585086	3245.752872	23.320858
115.418115	3258.035235	23.325875
115.914759	3248.782034	23.330893
116.420116	3242.259260	23.335911
116.273272	3241.201063	23.340928
115.894513	3252.110777	23.345946
116.471130	3239.322499	23.350963
116.397148	3246.724209	23.355981
116.797511	3262.046724	23.360999
116.899942	3275.407817	23.366016
116.858226	3268.231299	23.371034
116.943673	3265.662784	23.376051
116.634942	3281.972285	23.381069
117.063255	3272.104628	23.386087
116.801115	3265.609046	23.391104
116.817288	3274.876338	23.396122
117.285045	3291.019560	23.401139
117.325144	3302.019840	23.406157
117.686680	3300.204896	23.411175
117.494715	3309.917571	23.416192
117.695088	3305.994309	23.421210
117.684186	3302.368243	23.426227
117.756189	3327.523631	23.431245
118.063283	3318.747394	23.436263
117.960700	3336.398256	23.441280
118.091867	3333.179008	23.446298
118.288651	3329.792766	23.451315
118.571705	3345.190708	23.456333
118.914684	3350.665698	23.461351
118.801924	3353.101603	23.466368
118.831873	3354.975938	23.471386
119.579599	3352.529917	23.476403
119.347262	3353.562732	23.481421
119.577473	3350.998650	23.486439
119.630703	3351.908057	23.491456
119.551428	3348.946540	23.496474
119.887519	3340.356021	23.501491
120.014210	3327.991800	23.506509
119.859868	3351.765100	23.511527
120.064133	3364.008023	23.516544
120.336437	3378.544037	23.521562
120.333587	3377.421966	23.526579
120.320850	3377.801505	23.531597
120.114348	3377.673911	23.536615
120.721149	3368.195410	23.541632
120.590252	3399.333847	23.546650
120.743873	3393.956524	23.551667
120.689875	3407.836663	23.556685
121.043940	3395.299262	23.561703
121.474092	3401.048265	23.566720
121.493567	3399.185595	23.571738
121.930462	3383.690777	23.576755
121.400725	3394.182604	23.581773
121.678739	3407.423003	23.586791
121.869601	3414.243752	23.591808
121.683270	3423.989427	23.596826
121.744374	3421.548262	23.601843
122.114089	3425.740801	23.606861
122.059643	3434.173077	23.611879
122.212458	3452.075969	23.616896
121.816774	3460.419511	23.621914
122.782169	3446.804490	23.626931
122.678086	3474.074262	23.631949
122.845616	3481.938645	23.636967
123.066860	3474.588734	23.641984
123.209146	3481.488840	23.647002
123.338671	3470.962327	23.652019
123.438910	3480.299724	23.657037
123.753017	3470.721522	23.662055
123.607390	3480.060365	23.667072
123.755934	3483.606207	23.672090
124.435367	3491.547865	23.677107
124.141226	3496.754798	23.682125
124.260899	3486.450093	23.687143
124.344520	3487.881685	23.692160
124.247862	3490.421235	23.697178
124.855564	3489.411039	23.702195
124.908483	3483.441701	23.707213
124.879836	3485.868935	23.712231
125.106166	3478.172109	23.717248
124.603076	3491.160351	23.722266
125.011144	3472.792658	23.727283
124.853411	3486.991465	23.732301
125.119179	3486.937233	23.737319
125.302398	3501.670066	23.742336
125.421604	3516.583813	23.747354
125.784439	3501.806259	23.752371
125.518853	3523.789971	23.757389
125.461241	3510.057195	23.762407
125.791846	3531.858544	23.767424
125.727190	3532.475266	23.772442
126.343539	3523.274388	23.777459
126.110775	3539.640496	23.782477
126.190265	3553.460944	23.787495
126.660231	3554.055350	23.792512
126.737324	3570.281627	23.797530
126.788398	3557.305493	23.802547
126.883086	3568.931272	23.807565
127.004441	3567.112118	23.812583
127.387002	3589.853913	23.817600
127.351099	3584.891390	23.822618
127.716638	3580.730909	23.827635
127.760588	3576.100189	23.832653
127.817666	3577.311054	23.837671
127.920583	3586.273669	23.842688
128.075515	3599.755691	23.847706
128.043124	3613.981832	23.852723
128.321297	3608.622329	23.857741
128.429244	3616.091971	23.862759
128.641985	3611.837068	23.867776
128.433598	3630.475826	23.872794
129.009646	3612.505155	23.877811
128.891444	3632.977273	23.882829
128.846003	3638.790405	23.887847
129.270316	3636.269266	23.892864
129.032324	3639.714737	23.897882
129.210588	3636.230693	23.902899
129.568161	3660.077831	23.907917
129.381550	3659.202144	23.912935
130.206678	3662.120988	23.917952
129.916774	3668.241344	23.922970
130.383973	3660.793129	23.927987
130.171062	3656.872743	23.933005
130.095260	3668.245753	23.938023
130.386548	3687.138433	23.943040
130.436548	3694.175279	23.948058
130.626055	3692.040039	23.953075
130.481484	3698.542339	23.958093
130.503797	3694.832218	23.963111
130.564013	3714.575919	23.968128
130.777216	3723.105702	23.973146
131.274488	3708.089402	23.978163
131.184696	3724.727112	23.983181
131.528675	3740.995192	23.988199
132.073948	3732.909134	23.993216
132.085986	3734.964935	23.998234
132.457576	3737.587190	24.003251
132.214849	3729.817139	24.008269
132.200585	3730.056913	24.013287
132.561492	3729.259896	24.018304
132.222227	3736.630998	24.023322
132.673339	3733.963193	24.028339
133.052547	3747.105174	24.033357
133.007355	3748.862536	24.038375
133.264568	3749.541218	24.043392
133.233212	3763.423590	24.048410
133.195693	3754.779916	24.053427
133.295869	3761.774184	24.058445
133.271130	3760.729516	24.063463
133.424264	3761.014968	24.068480
133.402168	3784.151179	24.073498
133.848928	3775.827516	24.078515
134.047093	3781.415436	24.083533
133.888906	3791.384985	24.088551
133.981710	3800.971557	24.093568
134.125400	3818.018156	24.098586
134.446565	3811.266493	24.103603
134.566521	3817.704643	24.108621
134.602686	3842.028886	24.113639
135.266808	3825.461398	24.118656
135.280444	3828.773184	24.123674
135.354173	3843.978486	24.128691
135.635177	3830.676760	24.133709
135.653469	3831.834833	24.138727
135.848794	3829.475246	24.143744
135.924077	3831.296791	24.148762
136.453435	3838.774083	24.153779
136.227157	3840.384914	24.158797
136.304304	3862.666104	24.163815
136.694219	3846.121075	24.168832
136.269367	3859.376415	24.173850
136.501326	3857.884916	24.178867
136.640793	3851.922866	24.183885
136.412432	3864.040895	24.188903
136.624686	3875.250144	24.193920
136.836620	3886.944010	24.198938
137.062763	3875.885779	24.203955
137.225371	3899.814740	24.208973
137.314510	3911.281206	24.213991
137.867333	3906.500809	24.219008
137.602088	3915.674932	24.224026
137.835221	3909.959083	24.229043
138.283636	3907.729827	24.234061
138.125151	3910.789038	24.239079
138.343491	3927.487975	24.244096
138.287465	3926.049467	24.249114
138.279762	3927.378457	24.254131
138.222764	3931.088546	24.259149
138.568220	3945.146996	24.264167
139.158177	3947.839881	24.269184
138.929429	3955.636339	24.274202
139.110606	3966.141078	24.279219
139.180853	3951.084064	24.284237
139.014103	3977.694562	24.289255
139.572510	3969.366363	24.294272
139.774639	3976.316160	24.299290
140.109736	3972.987168	24.304307
140.225432	3979.759597	24.309325
140.389253	3987.152084	24.314343
140.818568	3993.040692	24.319360
140.500036	4008.185208	24.324378
140.616259	4003.130637	24.329395
141.094678	3998.351061	24.334413
140.964904	4009.378173	24.339431
141.327903	3991.965690	24.344448
141.113652	4002.303809	24.349466
141.410116	3993.783734	24.354483
141.708407	4003.332956	24.359501
141.489405	4033.123564	24.364519
142.076100	4015.040579	24.369536
141.815391	4022.231745	24.374554
142.014971	4019.567025	24.379571
142.258263	4024.207823	24.384589
142.108591	4023.712457	24.389607
142.337044	4049.610320	24.394624
142.282324	4049.866776	24.399642
142.754419	4046.099011	24.404659
143.042436	4049.157856	24.409677
142.775580	4060.757504	24.414695
143.383689	4062.940141	24.419712
143.241812	4073.918100	24.424730
143.239627	4082.818328	24.429747
143.514643	4078.614720	24.434765
143.500423	4088.590621	24.439783
143.806937	4096.718725	24.444800
143.658765	4108.654257	24.449818
143.827854	4101.942443	24.454835
144.173908	4111.441642	24.459853
144.123576	4132.012191	24.464871
144.461104	4120.114772	24.469888
144.509657	4129.352270	24.474906
144.814513	4141.221104	24.479923
145.356982	4148.499809	24.484941
145.366986	4152.413236	24.489959
145.398448	4143.425588	24.494976
145.482909	4155.861338	24.499994
145.537792	4148.155314	24.505011
145.798559	4141.035547	24.510029
145.557265	4155.567698	24.515047
145.814652	4160.923704	24.520064
146.097115	4179.761793	24.525082
146.107656	4176.733867	24.530099
146.208432	4180.385039	24.535117
146.486690	4176.181673	24.540135
146.730191	4195.225013	24.545152
146.617599	4202.273082	24.550170
146.875538	4208.021549	24.555187
147.751519	4192.892458	24.560205
147.326034	4197.246624	24.565223
147.365758	4203.929008	24.570240
147.569244	4194.134344	24.575258
147.600311	4212.708130	24.580275
148.126336	4213.053708	24.585293
147.973865	4227.819558	24.590311
148.269817	4225.000988	24.595328
148.144597	4231.569661	24.600346
148.284821	4234.283177	24.605363
148.638541	4245.669175	24.610381
148.334640	4260.677889	24.615399
148.655127	4263.584501	24.620416
149.063429	4254.780559	24.625434
148.919654	4282.106936	24.630451
149.219950	4278.840064	24.635469
149.497243	4276.107843	24.640487
149.802689	4272.393339	24.645504
149.723631	4270.300050	24.650522
150.092980	4298.457935	24.655539
150.320714	4297.277790	24.660557
150.382333	4302.657196	24.665575
150.445529	4312.999282	24.670592
150.372439	4305.540132	24.675610
150.361963	4303.715161	24.680627
150.807413	4319.527190	24.685645
150.688076	4329.434271	24.690663
150.894162	4320.609826	24.695680
151.212104	4320.028880	24.700698
151.410385	4337.739962	24.705715
151.943226	4344.940065	24.710733
151.838510	4347.401596	24.715751
151.448770	4355.182240	24.720768
151.794493	4345.605511	24.725786
151.928185	4360.673566	24.730803
152.112484	4373.830670	24.735821
152.428448	4382.380643	24.740839
152.532709	4378.306440	24.745856
152.733648	4387.090296	24.750874
152.311809	4396.926869	24.755891
153.155752	4397.301216	24.760909
152.754642	4413.724243	24.765927
153.210195	4400.759179	24.770944
153.608365	4425.712631	24.775962
153.689402	4428.637788	24.780979
153.908718	4429.191178	24.785997
153.840588	4436.276322	24.791015
154.089600	4420.027657	24.796032
154.511287	4411.805182	24.801050
154.408288	4421.467432	24.806067
154.813508	4434.518570	24.811085
154.882800	4440.531629	24.816103
155.278560	4445.857026	24.821120
155.326347	4444.003869	24.826138
155.478514	4445.795140	24.831155
155.255597	4449.615986	24.836173
155.294936	4440.953359	24.841191
155.680571	4444.461635	24.846208
155.662776	4439.016078	24.851226
155.482089	4465.878265	24.856243
155.883016	4470.730070	24.861261
156.319823	4465.348114	24.866279
156.281116	4474.428253	24.871296
156.813271	4470.441559	24.876314
156.543444	4496.305594	24.881331
157.183891	4493.716030	24.886349
156.963985	4497.873095	24.891367
157.057147	4494.687974	24.896384
157.305711	4486.480474	24.901402
157.441351	4509.639094	24.906419
157.638574	4515.484683	24.911437
157.530190	4527.173495	24.916455
157.589000	4529.459520	24.921472
157.901771	4533.062034	24.926490
158.304997	4561.409328	24.931507
158.115245	4561.550443	24.936525
158.268104	4562.297725	24.941543
158.613341	4575.547351	24.946560
159.070437	4578.661952	24.951578
159.115506	4588.284184	24.956595
159.500469	4578.118921	24.961613
159.528328	4575.818957	24.966631
159.489526	4575.235881	24.971648
159.845331	4581.057786	24.976666
160.166449	4594.084717	24.981683
160.251703	4602.884788	24.986701
160.346787	4607.822374	24.991719
160.224917	4606.845838	24.996736
160.198304	4603.728563	25.001754
160.245519	4616.228855	25.006771
160.773117	4628.979033	25.011789
160.926460	4636.351493	25.016807
160.743127	4629.213406	25.021824
161.158318	4645.574983	25.026842
161.583543	4643.059042	25.031859
161.732097	4651.561132	25.036877
161.789310	4656.268775	25.041895
161.929010	4651.219679	25.046912
162.187521	4651.245273	25.051930
162.024032	4653.261535	25.056947
162.534320	4671.411794	25.061965
162.506670	4672.316087	25.066983
162.426468	4673.170546	25.072000
162.700429	4674.304444	25.077018
162.909726	4676.578300	25.082035
163.017710	4675.455766	25.087053
163.044100	4702.351449	25.092071
163.192420	4705.081069	25.097088
163.434786	4706.282940	25.102106
163.188386	4711.341873	25.107123
163.619096	4715.234789	25.112141
163.876928	4722.423861	25.117159
163.792254	4732.502686	25.122176
164.516216	4741.945194	25.127194
164.718407	4756.216070	25.132211
165.029260	4751.717066	25.137229
164.735484	4750.103194	25.142247
165.078511	4744.662930	25.147264
164.959303	4751.905050	25.152282
164.884698	4784.726426	25.157299
165.163803	4778.075432	25.162317
165.526393	4784.674352	25.167335
165.750007	4817.972178	25.172352
166.052823	4808.493244	25.177370
165.726255	4818.559560	25.182387
166.319426	4823.926784	25.187405
166.304874	4830.728242	25.192423
166.327921	4835.720657	25.197440
166.966322	4851.013979	25.202458
166.923077	4871.869996	25.207475
167.227055	4858.182932	25.212493
167.480811	4864.204516	25.217511
167.474315	4863.702025	25.222528
167.889272	4868.193005	25.227546
167.756940	4890.413182	25.232563
168.271265	4881.642315	25.237581
168.073467	4892.726560	25.242599
168.232918	4890.859478	25.247616
168.686926	4897.478488	25.252634
168.407419	4913.457878	25.257651
168.730223	4908.027859	25.262669
169.169460	4910.061343	25.267687
169.058136	4926.190934	25.272704
169.083415	4935.158889	25.277722
169.433995	4939.132295	25.282739
169.766025	4943.018193	25.287757
169.840112	4951.585824	25.292775
169.596043	4970.257141	25.297792
169.959860	4960.305819	25.302810
170.367918	4977.714400	25.307827
170.518381	4998.050399	25.312845
170.752260	4994.970178	25.317863
170.771711	5005.414128	25.322880
171.317795	4986.543460	25.327898
170.958015	5001.554754	25.332915
171.338286	5002.228043	25.337933
171.429295	5021.933196	25.342951
171.430457	5020.860708	25.347968
171.691604	5016.921013	25.352986
171.700983	5030.367774	25.358003
172.228068	5045.192878	25.363021
172.504312	5040.447568	25.368039
172.947184	5046.800164	25.373056
173.084298	5044.461468	25.378074
172.860476	5047.156081	25.383091
173.086334	5040.298695	25.388109
173.371949	5045.875520	25.393127
173.274849	5073.549146	25.398144
173.655649	5066.076245	25.403162
173.769123	5068.908252	25.408179
173.778920	5075.592658	25.413197
174.193565	5075.684618	25.418215
174.268985	5094.494748	25.423232
174.145221	5103.724145	25.428250
174.272986	5105.745168	25.433267
175.025092	5103.281668	25.438285
174.896872	5116.809447	25.443303
174.959283	5133.265575	25.448320
175.153183	5136.832912	25.453338
175.127301	5135.055135	25.458355
175.020376	5145.738033	25.463373
175.646151	5140.999900	25.468391
175.559742	5148.793959	25.473408
175.857557	5164.089989	25.478426
176.033155	5174.548499	25.483443
176.116008	5175.970155	25.488461
176.210175	5198.251448	25.493479
176.297919	5214.329164	25.498496
176.753256	5217.752570	25.503514
177.036877	5234.945290	25.508531
177.084494	5245.622501	25.513549
177.417478	5255.447864	25.518567
177.600378	5270.784353	25.523584
177.693610	5272.418344	25.528602
177.752587	5283.046570	25.533619
177.995588	5288.232214	25.538637
178.364570	5303.590993	25.543655
178.506960	5322.688108	25.548672
178.762548	5328.420088	25.553690
178.807432	5334.656893	25.558707
179.050897	5336.690970	25.563725
179.404526	5338.538344	25.568743
179.567768	5365.274963	25.573760
179.646217	5362.338238	25.578778
179.909235	5361.719599	25.583795
180.169726	5350.219744	25.588813
180.177809	5371.759794	25.593831
180.138885	5377.482104	25.598848
181.213561	5375.484784	25.603866
181.706018	5366.828044	25.608883
181.858317	5363.561719	25.613901
182.189943	5349.720321	25.618919
182.334486	5325.105831	25.623936
182.420596	5313.016249	25.628954
182.195001	5315.922028	25.633971
182.284170	5304.101015	25.638989
182.574575	5304.904292	25.644007
182.434869	5307.626450	25.649024
182.519884	5307.003937	25.654042
182.509156	5308.009415	25.659059
182.639153	5302.982099	25.664077
182.832320	5311.356309	25.669095
182.791518	5328.504097	25.674112
182.746065	5333.082000	25.679130
183.230297	5336.894964	25.684148
183.084149	5357.960030	25.689165
183.733931	5368.397365	25.694183
183.292070	5371.638151	25.699200
183.563611	5392.444721	25.704218
183.929064	5399.688561	25.709236
183.931959	5409.476182	25.714253
184.506765	5425.632246	25.719271
184.558970	5428.136595	25.724288
184.534840	5453.125298	25.729306
184.821019	5468.920698	25.734324
184.864192	5471.623958	25.739341
184.975838	5487.049916	25.744359
185.388828	5512.998044	25.749376
185.082509	5522.960910	25.754394
185.772809	5525.967739	25.759412
185.709679	5547.521759	25.764429
186.103144	5560.146237	25.769447
186.277042	5568.299454	25.774464
186.724400	5577.736260	25.779482
186.638294	5580.156479	25.784500
187.013996	5595.179353	25.789517
187.655347	5601.258244	25.794535
187.834394	5615.099382	25.799552
187.585206	5603.470534	25.804570
188.214226	5614.749990	25.809588
187.963422	5638.670600	25.814605
188.160645	5636.006757	25.819623
188.364973	5647.099049	25.824640
188.559115	5661.365796	25.829658
189.044736	5653.299230	25.834676
188.713854	5673.493408	25.839693
189.455877	5676.628126	25.844711
189.435832	5688.070119	25.849728
189.601665	5679.024709	25.854746
189.902696	5685.821092	25.859764
189.807419	5700.908147	25.864781
190.199023	5711.467919	25.869799
190.581098	5705.818109	25.874816
191.051908	5698.135438	25.879834
190.908746	5706.080448	25.884852
190.634326	5725.315340	25.889869
191.303720	5729.392337	25.894887
191.330124	5736.663648	25.899904
191.769962	5731.774031	25.904922
191.851898	5733.374472	25.909940
191.785417	5737.931464	25.914957
192.205888	5751.355043	25.919975
192.158686	5765.935719	25.924992
192.228877	5769.393124	25.930010
192.735153	5753.347437	25.935028
192.668467	5788.865878	25.940045
192.967505	5776.624749	25.945063
193.132969	5792.666319	25.950080
193.047878	5794.768575	25.955098
193.454703	5809.255671	25.960116
193.328233	5818.880094	25.965133
193.759781	5840.048857	25.970151
194.167485	5848.303419	25.975168
194.325181	5845.464894	25.980186
194.357618	5854.631308	25.985204
194.259203	5870.790556	25.990221
194.920726	5874.560453	25.995239
195.257784	5877.059591	26.000256
195.458752	5896.937987	26.005274
195.876550	5902.168363	26.010292
195.776576	5897.391498	26.015309
196.042711	5901.908102	26.020327
196.182472	5907.857032	26.025344
196.282170	5918.106315	26.030362
196.705749	5924.389995	26.035380
196.692193	5925.999387	26.040397
196.613008	5928.958256	26.045415
196.821926	5950.283039	26.050432
196.669856	5948.419859	26.055450
197.259218	5969.584105	26.060468
197.502422	5983.102241	26.065485
197.737074	5993.638463	26.070503
197.947841	5994.998109	26.075520
197.820264	6014.877117	26.080538
198.366760	6012.718468	26.085556
198.348858	6035.625466	26.090573
198.761140	6038.192100	26.095591
198.884906	6047.536038	26.100608
198.931005	6061.752821	26.105626
199.496764	6061.068586	26.110644
199.636295	6064.919389	26.115661
199.648065	6069.843215	26.120679
200.388578	6097.433221	26.125696
200.243439	6102.227871	26.130714
200.687980	6090.259102	26.135732
200.444892	6102.453692	26.140749
200.981533	6106.660532	26.145767
201.042967	6124.619809	26.150784
200.962156	6120.229253	26.155802
201.222946	6131.635474	26.160820
201.592417	6140.226728	26.165837
201.552886	6144.407420	26.170855
201.812367	6156.572287	26.175872
202.046584	6165.326731	26.180890
202.282122	6169.630369	26.185908
202.060359	6187.520791	26.190925
202.314805	6186.471566	26.195943
202.563766	6208.448057	26.200960
202.825136	6223.885535	26.205978
202.845159	6229.793890	26.210996
203.028193	6240.080464	26.216013
203.418922	6259.385457	26.221031
203.698656	6283.786629	26.226048
203.551831	6278.869200	26.231066
204.417877	6294.087624	26.236084
204.488647	6304.035742	26.241101
204.665951	6309.519388	26.246119
204.971561	6325.373191	26.251136
204.735916	6340.993089	26.256154
205.267980	6336.222322	26.261172
205.677100	6354.649641	26.266189
205.921683	6359.972310	26.271207
205.756321	6362.291211	26.276224
206.145083	6380.912202	26.281242
206.379943	6377.670259	26.286260
206.470876	6401.212692	26.291277
206.650842	6400.214664	26.296295
206.934233	6411.729219	26.301312
207.157805	6418.235391	26.306330
207.386858	6439.734692	26.311348
207.543442	6455.772892	26.316365
207.990958	6456.500840	26.321383
208.087062	6459.949556	26.326400
208.177432	6472.084997	26.331418
208.843592	6465.259830	26.336436
208.275936	6478.714142	26.341453
208.699302	6486.608595	26.346471
209.287144	6497.900809	26.351488
208.938026	6500.278135	26.356506
209.690384	6512.457563	26.361524
209.667835	6533.821662	26.366541
210.149450	6528.265822	26.371559
209.977972	6541.070111	26.376576
210.099566	6561.080070	26.381594
210.110098	6553.166648	26.386612
210.596779	6570.594486	26.391629
211.025790	6584.662613	26.396647
211.357039	6591.123373	26.401664
211.289218	6592.791055	26.406682
211.716047	6616.299953	26.411700
211.855243	6614.547608	26.416717
211.838237	6621.382539	26.421735
212.032787	6638.764976	26.426752
211.952538	6658.036998	26.431770
212.806495	6648.740470	26.436788
212.618082	6661.446068	26.441805
213.089687	6679.658487	26.446823
213.648126	6679.123309	26.451840
213.663590	6688.264623	26.456858
213.694364	6690.149482	26.461876
213.679213	6688.041724	26.466893
213.656607	6707.040266	26.471911
213.739704	6717.939478	26.476928
213.860805	6728.891647	26.481946
214.663769	6733.109716	26.486964
214.498543	6754.825750	26.491981
214.876804	6774.682573	26.496999
215.205152	6776.970828	26.502016
215.561667	6786.860345	26.507034
215.985241	6795.702209	26.512052
215.848644	6808.374496	26.517069
216.346415	6809.033872	26.522087
216.529537	6817.990397	26.527104
216.460761	6835.817086	26.532122
216.825335	6828.596877	26.537140
216.794110	6853.295609	26.542157
216.858183	6857.459199	26.547175
217.508359	6874.920343	26.552192
217.283980	6885.700323	26.557210
217.558810	6896.733539	26.562228
218.015034	6917.431784	26.567245
217.876332	6923.480589	26.572263
218.351598	6927.592025	26.577280
218.332069	6946.831926	26.582298
218.629894	6952.458677	26.587316
219.322258	6967.329408	26.592333
219.272059	6983.986512	26.597351
219.941421	6990.792450	26.602368
219.638414	6999.293139	26.607386
220.022399	7005.596974	26.612404
220.247298	7011.354177	26.617421
220.283995	7033.699330	26.622439
220.563101	7028.452539	26.627456
220.739615	7048.657394	26.632474
221.108752	7057.842479	26.637492
221.531751	7067.583112	26.642509
221.434635	7091.556309	26.647527
222.034010	7094.048463	26.652544
222.198081	7098.772112	26.657562
222.227562	7113.657394	26.662580
222.300055	7123.462592	26.667597
222.798778	7133.754542	26.672615
223.191240	7139.492165	26.677632
223.098676	7151.660472	26.682650
223.579999	7152.756012	26.687668
223.742071	7158.058292	26.692685
223.957002	7186.287240	26.697703
224.299159	7175.045977	26.702720
224.248329	7186.525507	26.707738
224.362256	7183.834543	26.712756
224.740182	7207.925754	26.717773
224.466489	7214.917536	26.722791
225.047154	7212.667517	26.727808
225.154236	7239.971962	26.732826
225.207667	7238.192304	26.737844
225.608137	7258.788190	26.742861
225.673129	7273.831627	26.747879
226.147987	7271.246766	26.752896
226.258308	7285.060300	26.757914
226.502825	7299.128622	26.762932
226.245916	7305.212947	26.767949
226.856332	7324.122386	26.772967
227.473250	7317.244104	26.777984
227.675094	7346.914507	26.783002
227.832432	7350.813952	26.788020
227.878423	7355.403079	26.793037
227.982786	7375.793766	26.798055
228.371925	7387.816240	26.803072
228.587010	7394.974887	26.808090
229.204763	7405.239399	26.813108
229.416418	7407.786333	26.818125
229.480719	7416.521399	26.823143
229.705258	7413.037755	26.828160
229.799705	7442.323410	26.833178
229.887486	7440.011090	26.838196
230.316688	7450.209698	26.843213
230.585133	7472.187323	26.848231
230.925955	7465.446616	26.853248
230.893709	7476.972977	26.858266
230.848525	7498.291718	26.863284
231.263784	7516.130188	26.868301
231.274164	7536.657246	26.873319
231.600263	7527.700041	26.878336
231.827689	7559.093848	26.883354
232.217329	7549.526160	26.888372
233.065716	7566.043825	26.893389
233.216466	7579.933804	26.898407
233.368464	7585.801206	26.903424
233.862605	7578.572573	26.908442
233.877165	7571.918446	26.913460
233.812098	7587.792567	26.918477
233.992781	7612.749905	26.923495
234.588721	7609.497350	26.928512
234.781631	7611.024443	26.933530
234.720133	7641.113512	26.938548
235.063649	7637.668290	26.943565
235.122178	7647.793937	26.948583
235.248505	7661.898754	26.953600
235.366359	7676.576168	26.958618
235.658465	7681.118296	26.963636
235.935292	7695.317965	26.968653
235.931686	7712.509006	26.973671
236.538597	7724.537169	26.978688
236.632618	7729.946496	26.983706
236.812301	7753.971844	26.988724
237.136606	7750.206272	26.993741
237.089862	7765.300277	26.998759
237.588124	7781.285449	27.003776
237.604242	7789.439868	27.008794
238.177680	7799.458362	27.013812
238.263291	7796.762360	27.018829
238.244076	7821.657494	27.023847
238.878028	7825.847755	27.028864
239.088006	7849.356201	27.033882
239.320775	7845.694896	27.038900
239.733132	7859.386857	27.043917
239.794878	7874.454237	27.048935
239.952992	7869.841743	27.053952
240.183142	7875.055534	27.058970
240.390698	7896.106376	27.063988
240.864115	7895.787724	27.069005
240.442572	7918.234005	27.074023
240.985068	7922.411332	27.079040
241.449643	7935.492325	27.084058
241.674525	7956.051864	27.089076
242.009704	7959.133139	27.094093
242.312491	7973.272284	27.099111
242.435903	7993.030525	27.104128
242.753229	7985.142973	27.109146
242.956100	8009.618257	27.114164
243.483636	8013.174032	27.119181
243.207667	8029.687321	27.124199
243.729472	8041.929169	27.129216
243.963578	8041.159246	27.134234
244.016302	8062.540692	27.139252
244.649766	8063.832372	27.144269
244.775033	8078.332749	27.149287
244.735476	8086.212942	27.154304
245.251700	8106.919815	27.159322
245.239275	8108.035124	27.164340
245.721296	8119.238447	27.169357
245.763580	8136.813725	27.174375
246.120057	8135.853547	27.179392
246.217435	8155.814439	27.184410
246.414471	8167.061651	27.189428
246.907351	8172.857639	27.194445
247.163165	8193.175735	27.199463
247.491123	8199.860409	27.204480
247.528857	8208.385366	27.209498
247.746930	8215.973556	27.214516
247.885149	8221.893765	27.219533
248.251724	8242.439771	27.224551
248.846453	8257.069286	27.229568
249.173543	8251.581513	27.234586
249.224607	8271.802523	27.239604
249.577507	8277.502050	27.244621
249.631250	8280.171878	27.249639
249.951062	8295.529028	27.254656
250.222171	8289.002075	27.259674
250.466476	8307.143362	27.264692
250.971736	8305.245132	27.269709
250.811672	8311.717297	27.274727
251.224792	8316.950864	27.279744
251.443266	8321.488404	27.284762
251.287308	8334.002194	27.289780
251.799893	8344.317177	27.294797
251.698172	8360.519001	27.299815
251.566254	8358.689281	27.304832
252.039192	8384.917746	27.309850
252.197327	8404.827584	27.314868
252.806767	8410.688495	27.319885
252.669891	8434.769336	27.324903
253.186208	8454.157112	27.329920
253.266351	8464.667793	27.334938
253.426024	8488.383559	27.339956
253.735872	8499.225116	27.344973
254.247214	8508.985672	27.349991
254.534540	8524.515053	27.355008
255.153425	8535.710255	27.360026
255.001522	8545.753599	27.365044
255.717903	8563.791625	27.370061
255.652287	8574.350797	27.375079
255.930298	8584.372066	27.380096
256.570033	8605.693379	27.385114
256.442598	8608.101789	27.390132
256.691042	8622.443787	27.395149
257.103948	8634.165264	27.400167
257.460595	8644.035549	27.405184
257.471501	8653.959377	27.410202
257.669976	8675.321224	27.415220
258.331907	8681.424890	27.420237
258.207562	8698.777951	27.425255
258.373444	8703.283074	27.430272
258.837233	8712.745250	27.435290
258.919630	8727.207454	27.440308
259.542471	8738.573718	27.445325
259.850125	8760.123660	27.450343
259.953481	8760.003261	27.455360
260.480117	8771.162985	27.460378
260.537616	8790.229320	27.465396
260.784827	8789.278651	27.470413
260.853787	8804.474084	27.475431
261.172687	8804.082477	27.480448
261.805517	8812.597122	27.485466
261.504786	8832.224214	27.490484
262.051611	8823.844038	27.495501
262.530406	8846.167085	27.500519
262.530205	8863.107894	27.505536
262.695319	8860.196800	27.510554
262.494818	8888.659658	27.515572
263.174166	8896.627133	27.520589
263.537083	8910.517588	27.525607
263.891780	8922.142735	27.530624
264.276995	8915.744865	27.535642
264.499183	8937.997214	27.540660
264.909694	8942.344991	27.545677
265.123390	8949.249268	27.550695
265.076867	8945.595625	27.555712
265.379615	8948.837297	27.560730
265.719816	8978.752905	27.565748
265.952662	8977.499201	27.570765
266.233492	8990.645040	27.575783
266.287734	9003.611004	27.580800
266.834786	8997.371437	27.585818
266.766343	9018.340382	27.590836
266.682643	9037.889871	27.595853
266.890078	9042.018241	27.600871
267.190746	9066.819613	27.605888
267.612143	9085.356972	27.610906
267.607569	9108.924820	27.615924
268.613047	9122.101636	27.620941
268.598896	9138.097947	27.625959
268.521249	9149.702084	27.630976
268.921358	9162.469843	27.635994
269.320980	9184.565226	27.641012
269.644090	9195.001892	27.646029
269.717802	9204.231863	27.651047
270.131496	9228.319867	27.656064
270.645083	9245.819363	27.661082
270.544252	9260.652412	27.666100
271.438664	9271.618548	27.671117
271.196400	9281.142870	27.676135
271.523703	9288.913681	27.681152
271.914986	9307.707534	27.686170
272.250176	9315.800521	27.691188
272.413056	9340.831268	27.696205
272.608095	9350.259965	27.701223
272.918015	9363.517959	27.706240
273.597713	9373.493836	27.711258
273.665906	9397.224446	27.716276
273.955175	9401.290691	27.721293
274.438929	9400.220446	27.726311
274.248936	9428.685802	27.731328
274.707199	9444.155061	27.736346
274.766819	9448.977949	27.741364
274.936647	9461.033525	27.746381
275.322006	9483.912247	27.751399
275.576354	9499.180743	27.756416
276.436320	9503.503479	27.761434
276.307423	9524.047995	27.766452
276.585722	9528.795135	27.771469
276.910414	9550.357669	27.776487
277.214045	9568.254960	27.781504
277.505927	9578.188915	27.786522
277.752269	9579.830461	27.791540
278.079598	9588.816040	27.796557
278.285620	9611.062919	27.801575
279.000824	9610.227259	27.806592
279.865267	9588.169275	27.811610
279.909301	9604.342131	27.816628
280.442462	9589.791477	27.821645
280.619269	9582.694706	27.826663
280.569674	9591.047871	27.831680
280.873529	9580.398747	27.836698
281.176816	9596.377611	27.841716
281.357630	9600.388013	27.846733
281.212936	9611.734460	27.851751
281.356620	9616.791099	27.856768
281.825124	9610.649184	27.861786
281.649075	9635.148579	27.866804
281.757053	9647.683959	27.871821
281.885522	9667.205961	27.876839
281.953104	9689.416789	27.881856
282.525275	9693.068956	27.886874
282.934917	9719.680900	27.891892
283.117573	9734.399590	27.896909
283.374646	9750.472941	27.901927
283.556398	9776.378051	27.906944
284.105347	9783.326862	27.911962
284.393693	9810.911671	27.916980
284.494140	9838.541824	27.921997
284.780693	9838.171878	27.927015
285.099657	9867.221120	27.932032
285.706873	9887.733406	27.937050
285.685359	9897.705720	27.942068
285.951202	9911.541365	27.947085
286.544858	9925.611614	27.952103
286.615728	9957.569366	27.957120
287.116086	9960.860822	27.962138
287.570197	9985.146639	27.967156
287.533524	9996.002418	27.972173
288.276544	10005.860034	27.977191
288.272873	10015.790629	27.982208
288.915997	10038.362344	27.987226
289.171518	10043.308050	27.992244
289.345353	10046.867584	27.997261
289.516186	10062.336868	28.002279
289.567256	10078.899441	28.007296
290.038019	10100.055457	28.012314
290.433719	10114.698070	28.017332
290.481705	10135.933324	28.022349
290.793481	10139.085683	28.027367
290.880904	10165.599468	28.032384
291.477870	10184.505657	28.037402
291.953921	10196.433538	28.042420
292.049876	10202.658741	28.047437
292.464088	10212.577951	28.052455
292.693725	10237.119515	28.057472
293.167551	10246.290293	28.062490
293.858965	10254.630784	28.067508
294.074685	10259.771382	28.072525
294.207306	10263.207296	28.077543
294.407032	10282.765960	28.082560
294.749822	10285.568720	28.087578
295.106857	10291.330932	28.092596
295.369887	10308.232208	28.097613
295.390805	10314.038163	28.102631
295.398020	10324.654244	28.107648
296.074093	10340.305349	28.112666
296.092213	10346.669718	28.117684
295.917155	10361.051769	28.122701
296.333563	10373.797903	28.127719
296.096427	10397.568530	28.132736
296.646850	10419.544911	28.137754
297.140494	10430.614744	28.142772
297.438592	10458.196042	28.147789
298.223934	10471.506346	28.152807
298.300367	10502.409832	28.157824
298.874672	10507.848289	28.162842
299.342489	10518.795994	28.167860
299.278730	10535.101538	28.172877
299.898282	10545.616248	28.177895
299.850087	10565.335594	28.182912
300.316564	10575.865672	28.187930
300.485486	10591.800516	28.192948
300.826665	10606.886713	28.197965
301.086594	10623.596423	28.202983
301.454398	10635.155896	28.208000
301.931358	10654.353708	28.213018
302.318507	10659.923177	28.218036
302.074776	10693.670678	28.223053
302.988542	10702.647280	28.228071
302.799757	10705.908264	28.233088
303.092606	10719.375192	28.238106
303.691258	10740.725399	28.243124
304.036514	10741.055938	28.248141
304.122276	10757.832512	28.253159
304.154885	10776.605107	28.258176
304.595798	10791.532757	28.263194
305.299201	10812.480748	28.268212
305.261356	10837.376783	28.273229
305.684795	10845.652500	28.278247
305.635155	10870.012955	28.283264
306.081403	10895.271861	28.288282
306.325257	10904.448612	28.293300
306.487510	10936.637849	28.298317
306.998122	10949.054270	28.303335
307.427575	10981.360778	28.308352
307.622438	10986.231076	28.313370
308.335571	11003.506447	28.318388
308.114351	11023.993353	28.323405
308.736901	11036.167712	28.328423
308.908904	11058.497319	28.333440
309.142478	11075.896030	28.338458
309.642166	11088.926595	28.343476
309.681643	11124.294430	28.348493
310.341334	11121.932505	28.353511
310.616772	11154.443761	28.358528
310.650053	11162.385184	28.363546
311.055963	11177.612351	28.368564
310.960529	11201.405732	28.373581
311.740030	11206.512289	28.378599
311.984486	11219.702090	28.383616
311.983827	11238.569494	28.388634
312.647069	11248.025114	28.393652
312.721382	11266.204169	28.398669
313.674069	11281.367911	28.403687
313.598220	11292.665298	28.408704
314.074639	11311.525624	28.413722
314.391445	11316.962134	28.418740
314.467418	11343.671655	28.423757
314.947705	11349.313899	28.428775
315.043671	11367.822533	28.433792
315.567064	11381.789273	28.438810
315.583923	11404.797343	28.443828
316.161097	11419.506756	28.448845
316.852215	11440.757833	28.453863
316.655474	11447.451649	28.458880
316.848659	11459.796701	28.463898
317.446498	11477.568324	28.468916
317.688348	11508.223603	28.473933
318.113034	11514.673207	28.478951
318.098482	11536.183267	28.483968
318.826593	11554.173476	28.488986
318.960015	11565.026888	28.494004
319.280957	11586.306472	28.499021
319.702845	11604.366399	28.504039
319.967268	11624.146704	28.509056
319.821757	11636.668656	28.514074
320.595690	11660.111711	28.519092
320.883340	11679.065152	28.524109
320.725434	11701.774514	28.529127
321.438791	11717.596632	28.534144
321.939498	11729.158594	28.539162
322.403620	11756.879913	28.544180
322.257054	11772.223276	28.549197
323.117242	11770.549838	28.554215
323.379966	11803.961350	28.559232
323.565428	11823.113063	28.564250
324.022500	11821.024556	28.569268
324.157166	11854.548278	28.574285
324.535740	11849.893929	28.579303
324.725459	11883.463248	28.584320
325.041850	11892.023808	28.589338
325.270890	11920.019398	28.594356
325.522027	11931.718883	28.599373
325.999348	11951.736826	28.604391
326.316823	11973.387421	28.609408
326.815739	11987.692336	28.614426
327.554432	12005.681795	28.619444
327.256647	12016.937567	28.624461
327.944282	12025.148618	28.629479
328.399004	12045.054985	28.634496
328.338063	12063.209724	28.639514
328.846828	12081.013967	28.644532
328.876842	12089.004409	28.649549
329.480846	12092.612757	28.654567
329.794742	12103.743566	28.659584
329.597334	12133.512666	28.664602
330.327981	12139.168833	28.669620
330.287649	12167.827223	28.674637
330.507689	12181.246070	28.679655
330.984837	12218.739070	28.684672
330.875854	12223.764840	28.689690
331.741488	12248.294314	28.694708
331.924129	12266.830968	28.699725
332.465338	12287.050896	28.704743
332.921570	12292.419499	28.709760
333.136436	12323.504175	28.714778
333.719782	12332.667444	28.719796
334.165128	12358.220165	28.724813
334.575810	12361.423353	28.729831
334.723695	12376.164733	28.734848
335.135156	12397.828901	28.739866
335.337668	12403.450487	28.744884
335.641739	12433.172921	28.749901
336.209484	12432.849808	28.754919
336.039537	12452.910767	28.759936
336.214739	12471.680257	28.764954
336.886371	12484.572872	28.769972
337.429833	12507.549465	28.774989
337.578056	12527.921677	28.780007
337.758140	12545.436470	28.785024
337.837204	12568.716203	28.790042
338.586523	12585.433533	28.795060
338.651557	12614.014386	28.800077
339.318418	12626.790019	28.805095
339.609106	12651.028466	28.810112
339.704143	12677.113935	28.815130
340.299024	12687.258258	28.820148
340.577412	12701.903008	28.825165
341.092672	12723.445042	28.830183
341.129064	12743.871572	28.835200
341.110250	12755.881539	28.840218
341.592220	12783.676281	28.845236
341.822401	12821.039922	28.850253
342.471492	12833.761302	28.855271
342.948452	12865.472187	28.860288
343.311584	12879.387939	28.865306
343.676268	12911.821262	28.870324
343.878723	12926.142437	28.875341
344.189022	12940.323455	28.880359
344.851633	12970.631292	28.885376
344.918224	12985.812829	28.890394
345.180372	13000.528934	28.895412
345.741999	13016.905733	28.900429
345.902990	13036.361981	28.905447
346.807676	13059.572882	28.910464
346.600933	13078.898487	28.915482
347.374686	13083.224829	28.920500
347.611785	13112.578704	28.925517
347.785348	13117.900954	28.930535
348.083991	13136.254106	28.935552
348.453442	13149.211387	28.940570
348.776988	13165.435610	28.945588
348.887130	13184.604593	28.950605
349.298701	13197.581768	28.955623
349.743115	13216.038906	28.960640
350.147554	13237.370284	28.965658
350.351025	13258.760675	28.970676
350.431953	13273.093476	28.975693
350.985942	13291.256574	28.980711
351.186516	13321.949655	28.985728
351.544554	13343.620543	28.990746
352.095810	13349.975208	28.995764
352.561508	13391.439821	29.000781
352.919966	13408.797903	29.005799
353.655527	13424.399859	29.010816
353.341995	13442.238750	29.015834
353.856557	13463.690448	29.020852
354.276759	13486.939265	29.025869
354.284600	13508.893281	29.030887
354.485091	13536.037258	29.035904
355.072191	13555.622264	29.040922
356.168230	13584.863791	29.045940
356.171489	13608.850659	29.050957
356.258076	13631.802195	29.055975
356.947304	13648.886461	29.060992
356.939627	13666.118403	29.066010
357.325256	13691.432976	29.071028
357.906891	13725.456149	29.076045
358.282791	13736.051490	29.081063
358.505828	13763.420944	29.086080
358.852775	13787.196685	29.091098
359.377756	13792.896102	29.096116
359.714020	13829.178544	29.101133
359.624324	13841.776065	29.106151
360.523586	13872.128876	29.111168
360.737033	13884.569893	29.116186
361.228069	13904.883028	29.121204
361.516061	13924.691513	29.126221
361.864294	13952.669993	29.131239
362.276673	13969.397489	29.136256
362.169520	14001.077194	29.141274
362.885518	14013.252958	29.146292
363.286774	14044.383579	29.151309
363.368444	14076.021346	29.156327
363.847945	14088.046825	29.161344
364.238957	14124.880917	29.166362
364.748736	14143.826254	29.171380
364.879555	14157.473602	29.176397
364.960943	14189.539668	29.181415
365.506615	14215.493583	29.186432
365.599039	14244.344042	29.191450
366.342658	14261.354900	29.196468
366.499083	14296.366223	29.201485
367.109703	14317.230566	29.206503
367.784099	14317.591017	29.211520
367.911208	14354.051992	29.216538
368.091282	14366.740678	29.221556
368.513241	14391.083292	29.226573
369.052064	14401.654614	29.231591
369.678942	14426.144304	29.236608
369.485354	14451.268269	29.241626
369.802057	14473.033649	29.246644
370.112231	14493.641965	29.251661
370.428273	14528.687129	29.256679
370.874385	14545.915254	29.261696
371.196051	14572.442231	29.266714
371.437869	14608.225874	29.271732
371.925072	14629.499379	29.276749
372.172663	14656.538660	29.281767
372.517321	14687.524440	29.286784
372.749052	14720.177635	29.291802
373.424677	14756.783403	29.296820
374.113432	14774.728040	29.301837
374.365648	14799.677630	29.306855
374.962772	14827.543568	29.311872
375.326930	14848.642154	29.316890
375.944997	14868.112042	29.321908
376.289511	14894.422215	29.326925
376.372973	14914.765827	29.331943
376.788327	14924.604429	29.336960
377.216737	14963.774933	29.341978
377.536793	14979.262467	29.346996
378.411887	14989.947997	29.352013
378.272129	15031.720684	29.357031
378.704213	15048.143128	29.362048
379.490581	15080.311274	29.367066
379.658763	15095.080690	29.372084
380.064730	15116.702187	29.377101
380.416403	15133.410230	29.382119
380.870508	15148.404644	29.387136
381.034242	15176.055406	29.392154
381.443658	15197.369355	29.397172
382.021061	15217.103589	29.402189
382.244146	15248.152091	29.407207
382.600289	15264.235204	29.412224
382.769625	15294.453683	29.417242
382.975421	15316.091121	29.422260
383.423026	15349.542861	29.427277
383.603518	15367.770715	29.432295
383.827646	15400.926068	29.437312
384.311262	15433.849045	29.442330
385.155640	15460.447685	29.447348
385.928030	15492.981841	29.452365
385.912110	15530.070834	29.457383
386.200424	15540.885384	29.462400
386.581312	15561.244653	29.467418
386.935302	15591.661017	29.472436
387.183285	15603.418453	29.477453
387.314331	15644.999689	29.482471
387.525976	15663.926722	29.487488
387.645586	15689.681505	29.492506
387.898919	15731.400938	29.497524
388.701410	15763.788677	29.502541
389.040140	15797.688087	29.507559
389.777329	15824.652010	29.512576
389.974233	15865.919178	29.517594
390.153770	15884.382792	29.522612
390.990940	15913.367162	29.527629
391.427939	15950.654341	29.532647
391.943898	15964.089206	29.537664
392.407550	15992.925703	29.542682
392.703400	16026.727747	29.547700
393.461480	16036.807780	29.552717
393.365695	16070.878584	29.557735
393.997870	16099.808979	29.562752
394.430404	16116.862728	29.567770
394.753396	16147.615783	29.572788
395.177321	16180.173367	29.577805
395.336897	16206.787459	29.582823
395.857657	16224.025070	29.587840
396.115344	16264.086386	29.592858
396.530299	16283.225546	29.597876
397.547494	16318.272319	29.602893
397.764827	16343.343938	29.607911
397.830644	16362.202563	29.612928
398.422219	16394.964757	29.617946
398.725037	16426.828692	29.622964
399.407888	16449.018487	29.627981
399.453907	16473.315181	29.632999
400.277136	16487.902938	29.638016
400.297859	16511.228479	29.643034
400.520653	16548.910634	29.648052
400.928055	16564.777924	29.653069
401.348557	16614.833782	29.658087
401.695231	16635.524882	29.663104
402.258896	16659.023746	29.668122
402.574999	16695.336468	29.673140
403.302082	16719.313252	29.678157
403.327340	16749.277271	29.683175
403.811408	16775.491971	29.688192
404.437578	16802.550494	29.693210
404.807943	16840.166940	29.698228
405.309701	16856.780225	29.703245
405.661694	16887.850374	29.708263
406.027130	16901.011464	29.713280
406.600188	16933.642342	29.718298
406.763228	16963.629700	29.723316
407.046045	16981.617997	29.728333
407.301555	17029.929267	29.733351
407.676840	17050.279596	29.738368
408.194805	17082.883746	29.743386
408.179637	17112.695678	29.748404
408.926236	17135.400266	29.753421
409.170839	17154.801782	29.758439
409.532364	17193.553248	29.763456
410.235828	17214.076480	29.768474
410.343358	17253.261042	29.773492
411.066372	17269.961359	29.778509
411.279957	17311.803305	29.783527
412.372617	17317.436837	29.788544
412.625298	17349.173478	29.793562
412.809858	17371.130645	29.798580
413.699690	17400.387167	29.803597
413.651070	17420.703962	29.808615
413.478428	17456.985532	29.813632
414.132467	17476.281276	29.818650
414.410315	17521.474862	29.823668
415.049723	17545.751133	29.828685
415.338529	17586.627983	29.833703
415.756618	17617.082427	29.838720
416.295746	17648.379980	29.843738
416.642946	17679.390877	29.848756
417.103356	17708.369581	29.853773
417.915518	17739.899977	29.858791
418.477907	17766.672939	29.863808
418.909055	17797.010509	29.868826
418.918743	17827.236953	29.873844
419.576821	17852.738998	29.878861
419.680222	17880.997793	29.883879
420.035112	17918.797275	29.888896
420.533489	17952.910623	29.893914
420.373057	17979.277495	29.898932
421.195884	18016.791060	29.903949
421.363608	18056.908565	29.908967
421.956366	18095.420343	29.913984
422.976700	18122.344176	29.919002
423.425188	18168.193335	29.924020
423.913500	18181.956585	29.929037
424.179498	18224.260342	29.934055
424.539051	18242.732940	29.939072
425.011267	18272.291505	29.944090
424.902148	18290.917569	29.949108
426.063032	18322.333363	29.954125
426.323454	18343.613115	29.959143
426.996837	18390.204239	29.964160
427.397085	18402.304604	29.969178
427.868189	18447.077002	29.974196
428.224960	18464.866863	29.979213
428.589289	18487.174325	29.984231
428.834479	18525.400825	29.989248
429.386304	18546.145070	29.994266
429.605068	18569.137244	29.999284
429.922574	18612.033447	30.004301
430.028995	18635.731402	30.009319
430.591371	18669.977864	30.014336
431.481206	18706.793067	30.019354
433.905015	18672.261984	30.024372
435.301936	18644.670462	30.029389
435.522766	18639.979781	30.034407
436.124274	18632.171020	30.039424
436.418462	18604.779665	30.044442
436.333882	18604.638362	30.049460
436.347780	18601.468824	30.054477
436.758254	18604.260014	30.059495
436.782316	18605.345081	30.064512
437.011350	18604.197924	30.069530
436.687933	18608.461526	30.074548
437.151005	18620.007182	30.079565
437.205323	18648.954713	30.084583
437.173292	18683.435671	30.089600
437.714652	18695.521660	30.094618
437.906251	18732.671004	30.099636
438.013813	18749.737520	30.104653
438.665460	18793.734133	30.109671
438.629705	18832.627803	30.114688
439.172997	18876.193882	30.119706
439.145191	18936.212541	30.124724
439.934780	18971.451036	30.129741
440.312247	19020.585312	30.134759
440.081883	19076.713125	30.139776
441.009366	19118.011164	30.144794
441.279617	19169.900043	30.149812
441.806954	19226.602969	30.154829
442.888018	19267.402912	30.159847
443.134705	19288.664495	30.164864
444.021589	19331.313701	30.169882
444.327297	19365.118719	30.174900
445.098004	19400.761997	30.179917
445.612470	19435.222121	30.184935
446.033359	19476.332522	30.189952
446.736251	19504.177095	30.194970
447.342235	19531.434375	30.199988
447.683626	19564.012436	30.205005
448.067486	19589.985857	30.210023
448.431557	19620.143776	30.215040
448.950263	19651.887040	30.220058
449.155537	19684.315769	30.225076
449.569575	19721.083983	30.230093
450.215155	19758.396924	30.235111
450.448236	19789.239068	30.240128
451.163308	19830.609067	30.245146
451.440593	19862.049074	30.250164
451.859211	19883.289985	30.255181
452.084241	19923.878797	30.260199
452.735264	19962.792650	30.265216
453.268738	19999.216879	30.270234
453.475113	20041.046852	30.275252
454.308978	20071.997794	30.280269
455.404165	20086.649600	30.285287
455.278463	20124.222917	30.290304
455.932072	20145.729923	30.295322
456.142735	20168.784419	30.300340
456.609675	20206.522596	30.305357
456.728152	20227.965349	30.310375
457.019197	20248.405356	30.315392
457.792050	20278.460445	30.320410
457.936190	20322.452067	30.325428
458.404803	20355.207986	30.330445
458.789808	20389.327031	30.335463
458.912831	20424.770691	30.340480
459.518017	20457.014861	30.345498
460.036879	20492.279065	30.350516
460.815419	20533.403392	30.355533
461.470229	20567.879100	30.360551
461.890986	20595.759155	30.365568
462.496694	20632.148942	30.370586
462.192430	20671.186430	30.375604
463.011552	20712.278776	30.380621
463.552539	20742.302004	30.385639
463.915854	20782.277636	30.390656
464.635530	20802.045680	30.395674
465.377174	20822.939523	30.400692
465.604886	20879.165411	30.405709
465.920745	20902.586956	30.410727
466.405739	20947.432842	30.415744
467.198442	20970.845463	30.420762
467.647760	21010.773720	30.425780
468.086215	21031.532655	30.430797
468.575419	21068.782685	30.435815
469.021833	21097.145836	30.440832
469.435184	21130.143712	30.445850
469.967347	21163.749987	30.450868
470.149522	21198.058248	30.455885
470.807129	21230.828027	30.460903
471.011654	21279.195656	30.465920
471.693726	21303.167035	30.470938
472.474380	21349.801902	30.475956
472.965070	21370.082811	30.480973
473.645740	21408.479713	30.485991
473.928707	21435.077493	30.491008
474.217164	21474.246602	30.496026
474.664641	21497.344475	30.501044
474.860873	21532.484438	30.506061
475.255831	21571.262743	30.511079
475.558805	21606.873353	30.516096
476.669762	21633.546690	30.521114
476.890961	21682.472058	30.526132
477.150045	21714.548325	30.531149
478.040304	21748.768615	30.536167
478.661876	21791.964151	30.541184
478.947963	21813.851750	30.546202
479.559067	21852.024556	30.551220
479.773775	21892.361792	30.556237
480.130731	21923.615652	30.561255
480.370445	21964.160154	30.566272
481.237686	21997.655377	30.571290
481.476587	22029.604767	30.576308
482.049832	22055.114625	30.581325
482.516402	22089.879629	30.586343
482.977127	22124.900024	30.591360
483.333879	22149.104087	30.596378
483.833856	22178.727461	30.601396
484.307214	22220.420692	30.606413
485.001065	22248.774468	30.611431
485.170233	22288.081954	30.616448
485.642034	22318.624452	30.621466
486.103927	22367.869590	30.626484
486.416883	22414.205661	30.631501
486.812484	22450.838304	30.636519
487.537143	22496.438802	30.641536
487.926345	22537.856448	30.646554
488.894742	22568.094287	30.651572
488.923207	22623.969868	30.656589
489.313186	22653.157218	30.661607
489.816721	22695.860529	30.666624
489.987940	22734.529274	30.671642
490.991511	22777.859625	30.676660
491.272945	22824.046764	30.681677
491.894859	22852.079145	30.686695
492.589209	22905.549853	30.691712
493.014902	22947.008441	30.696730
494.123037	22991.711274	30.701748
494.310108	23018.660162	30.706765
494.806621	23058.516790	30.711783
495.032237	23094.658970	30.716800
495.800152	23131.327611	30.721818
496.316052	23163.940088	30.726836
496.750576	23211.701259	30.731853
497.562493	23239.477229	30.736871
497.912557	23276.338000	30.741888
498.628469	23315.627109	30.746906
499.610642	23355.841894	30.751924
499.609057	23378.598984	30.756941
500.280706	23412.453669	30.761959
500.771175	23440.610428	30.766976
501.218348	23471.690734	30.771994
501.538196	23510.103771	30.777012
501.760329	23541.712332	30.782029
502.526579	23571.132868	30.787047
502.724065	23615.506798	30.792064
503.060566	23652.046097	30.797082
503.732692	23692.582076	30.802100
504.113396	23730.980442	30.807117
504.611453	23774.702815	30.812135
505.165121	23816.516641	30.817152
505.866458	23857.057841	30.822170
506.327395	23889.435610	30.827188
506.829951	23931.272059	30.832205
507.563581	23963.458463	30.837223
508.085173	24002.270618	30.842240
508.522548	24031.029204	30.847258
508.889432	24059.661230	30.852276
509.165111	24096.198638	30.857293
509.906351	24121.792205	30.862311
510.080350	24156.295659	30.867328
510.556861	24195.827519	30.872346
511.496213	24229.777579	30.877364
511.525509	24279.494560	30.882381
512.116015	24298.728345	30.887399
512.366220	24351.749309	30.892416
512.934335	24382.791658	30.897434
513.513328	24431.770934	30.902452
514.140676	24470.177487	30.907469
514.766063	24506.642806	30.912487
515.352513	24546.796051	30.917504
515.694203	24589.048185	30.922522
516.156883	24617.611608	30.927540
516.640190	24665.320550	30.932557
516.969103	24713.418142	30.937575
517.562554	24757.729825	30.942592
517.971573	24808.605750	30.947610
518.438595	24847.813060	30.952628
518.971513	24897.807791	30.957645
519.681294	24950.258928	30.962663
519.940955	25001.271112	30.967680
520.825614	25035.839722	30.972698
521.442433	25087.797259	30.977716
521.757828	25130.581998	30.982733
522.326976	25166.270862	30.987751
523.135542	25217.817027	30.992768
523.554089	25249.370127	30.997786
524.154491	25293.033900	31.002804
524.909798	25333.098428	31.007821
525.236787	25365.706925	31.012839
525.461058	25426.107129	31.017856
525.943813	25462.416181	31.022874
526.798665	25496.728227	31.027892
527.494645	25556.637079	31.032909
527.785785	25595.631621	31.037927
528.365530	25644.809079	31.042944
528.707993	25674.885525	31.047962
529.625815	25714.619483	31.052980
530.062536	25764.154880	31.057997
530.695974	25803.298646	31.063015
531.204713	25845.755949	31.068032
532.032084	25879.962126	31.073050
532.501078	25916.263374	31.078068
532.929316	25968.833603	31.083085
533.585798	26006.275009	31.088103
534.250291	26031.584535	31.093120
534.306392	26080.044799	31.098138
535.224164	26107.624606	31.103156
535.573880	26157.475216	31.108173
536.456335	26183.257586	31.113191
536.628854	26226.211388	31.118208
536.875723	26262.241571	31.123226
537.714178	26288.318656	31.128244
537.982758	26328.337953	31.133261
538.590188	26371.296135	31.138279
539.274864	26393.113177	31.143296
539.625443	26429.380094	31.148314
540.337346	26462.817347	31.153332
540.504261	26508.125106	31.158349
541.177049	26538.134807	31.163367
541.411234	26579.874426	31.168384
542.005432	26615.860325	31.173402
542.797887	26660.047908	31.178420
542.828727	26709.907696	31.183437
543.349937	26743.383786	31.188455
544.257374	26794.099199	31.193472
544.416713	26843.519040	31.198490
545.360082	26885.295392	31.203508
545.704152	26930.221614	31.208525
546.376209	26976.134837	31.213543
546.877886	27022.015455	31.218560
547.321283	27070.138924	31.223578
548.069501	27103.947518	31.228596
548.431844	27160.542893	31.233613
549.252282	27198.052360	31.238631
550.196566	27243.415636	31.243648
550.694532	27275.271271	31.248666
551.422873	27320.784969	31.253684
551.797185	27361.721206	31.258701
552.560009	27396.801213	31.263719
552.780205	27440.099673	31.268736
553.148434	27473.044656	31.273754
554.019567	27507.563266	31.278772
554.170356	27558.893215	31.283789
555.008203	27597.133527	31.288807
555.259261	27637.941195	31.293824
555.767370	27696.265024	31.298842
556.165394	27739.412273	31.303860
556.624075	27792.709227	31.308877
557.533411	27841.927592	31.313895
558.217114	27886.280048	31.318912
558.380410	27938.341910	31.323930
559.278604	27973.721485	31.328948
559.887405	28025.830853	31.333965
560.632744	28073.954141	31.338983
561.309512	28111.624136	31.344000
561.897597	28159.478065	31.349018
562.785840	28197.677114	31.354036
562.964135	28244.239858	31.359053
563.694467	28269.631466	31.364071
564.419002	28317.341224	31.369088
564.579545	28352.684693	31.374106
565.235236	28382.974748	31.379124
565.989192	28425.469149	31.384141
566.405881	28462.521146	31.389159
566.988370	28507.824279	31.394176
567.522327	28551.652475	31.399194
567.883379	28580.785945	31.404212
568.321792	28618.132658	31.409229
568.767499	28654.269679	31.414247
569.521773	28684.018291	31.419264
569.475862	28741.974793	31.424282
570.263999	28776.989172	31.429300
571.090222	28824.397441	31.434317
571.602103	28866.041234	31.439335
572.105280	28912.268940	31.444352
572.385866	28968.650457	31.449370
573.076680	29010.962631	31.454388
573.233825	29058.853188	31.459405
573.797905	29109.963079	31.464423
574.718015	29165.184478	31.469440
575.167539	29216.478411	31.474458
575.700286	29256.047671	31.479476
576.341620	29309.410357	31.484493
576.871048	29373.692714	31.489511
577.484771	29413.559904	31.494528
578.020910	29476.289390	31.499546
578.656817	29526.826576	31.504564
579.174966	29577.469346	31.509581
579.897598	29635.579261	31.514599
580.770413	29681.362628	31.519616
580.666737	29738.294957	31.524634
581.415545	29794.883703	31.529652
582.139088	29851.634258	31.534669
582.703479	29899.876894	31.539687
583.239847	29954.917833	31.544704
584.197995	30011.645768	31.549722
584.865001	30052.007178	31.554740
585.561445	30105.573298	31.559757
585.995220	30151.276623	31.564775
586.754292	30203.432101	31.569792
587.428062	30253.243744	31.574810
587.901921	30287.417889	31.579828
588.417967	30344.997481	31.584845
588.863215	30401.620923	31.589863
589.738954	30443.070556	31.594880
590.561308	30494.082207	31.599898
591.037892	30536.445083	31.604916
591.716808	30590.795690	31.609933
592.082630	30646.017417	31.614951
593.434356	30673.517042	31.619968
593.028755	30729.139273	31.624986
593.970582	30765.205134	31.630004
594.730730	30813.345231	31.635021
595.190412	30864.124241	31.640039
595.669094	30900.877219	31.645056
596.085576	30961.768663	31.650074
596.734529	31006.210839	31.655092
597.111591	31060.417233	31.660109
597.979598	31113.670936	31.665127
598.783817	31151.653933	31.670144
599.085755	31207.765572	31.675162
599.380459	31236.709486	31.680180
600.421570	31290.927519	31.685197
600.886439	31338.800984	31.690215
601.477195	31377.980037	31.695232
601.937175	31432.037343	31.700250
602.472813	31471.094586	31.705268
602.903228	31523.212061	31.710285
603.108918	31577.568814	31.715303
604.125567	31624.616073	31.720320
604.401342	31683.490036	31.725338
605.013385	31733.494121	31.730356
606.122117	31786.191578	31.735373
606.591108	31846.304096	31.740391
607.272438	31889.749011	31.745408
607.390808	31952.184162	31.750426
608.282401	32003.024011	31.755444
609.077035	32051.942431	31.760461
609.348235	32110.385225	31.765479
610.150652	32162.283152	31.770496
610.556989	32233.703056	31.775514
611.318959	32287.850637	31.780532
611.812822	32334.912265	31.785549
612.463845	32399.719898	31.790567
613.251997	32446.199095	31.795584
613.579938	32510.945135	31.800602
614.457162	32561.483231	31.805620
614.931256	32627.445308	31.810637
615.631940	32694.533197	31.815655
616.616035	32738.166992	31.820672
617.153827	32793.742118	31.825690
617.457187	32850.234269	31.830708
618.364790	32900.302022	31.835725
618.652922	32960.188918	31.840743
619.539813	33026.889138	31.845760
619.780622	33079.751029	31.850778
620.673830	33143.042972	31.855796
621.524121	33193.869442	31.860813
622.141166	33258.569228	31.865831
622.962660	33316.135832	31.870848
623.427826	33373.535555	31.875866
624.015516	33426.138408	31.880884
624.873191	33476.882611	31.885901
625.329407	33544.162629	31.890919
625.801821	33589.364985	31.895936
626.449905	33637.825975	31.900954
626.942608	33700.272760	31.905972
627.677739	33758.333842	31.910989
628.040678	33823.019556	31.916007
629.128402	33868.495117	31.921024
629.523520	33942.253936	31.926042
629.896427	33993.075343	31.931060
630.714325	34050.019293	31.936077
631.464922	34111.748759	31.941095
632.554958	34159.918647	31.946112
632.790435	34225.822643	31.951130
633.496569	34263.897819	31.956148
634.279624	34304.771403	31.961165
634.518321	34365.803053	31.966183
635.198176	34405.567826	31.971200
635.900940	34462.302961	31.976218
636.268489	34510.199563	31.981236
637.258968	34569.017301	31.986253
637.693133	34625.489955	31.991271
638.422398	34676.543608	31.996288
638.776613	34732.353102	32.001306
639.532203	34785.362308	32.006324
640.532026	34841.135573	32.011341
640.674003	34893.705292	32.016359
641.593590	34938.179624	32.021376
642.128077	34998.934773	32.026394
642.631038	35066.855113	32.031412
643.113020	35121.040805	32.036429
643.833702	35178.997241	32.041447
644.664075	35241.790160	32.046464
644.925409	35312.853919	32.051482
645.813396	35378.185658	32.056500
646.537076	35437.775687	32.061517
646.729736	35496.004899	32.066535
647.512882	35560.248971	32.071552
648.307768	35615.326002	32.076570
648.937643	35694.020997	32.081588
649.546463	35752.943111	32.086605
649.767954	35824.098942	32.091623
650.693271	35890.757280	32.096640
651.096913	35962.791165	32.101658
652.044270	36037.907508	32.106676
652.894653	36088.927293	32.111693
653.360169	36171.815781	32.116711
654.241834	36218.520853	32.121728
654.969728	36292.722660	32.126746
655.336359	36363.020551	32.131764
656.056300	36427.132985	32.136781
656.886260	36499.293635	32.141799
657.723275	36555.852146	32.146816
658.300589	36625.661977	32.151834
658.917054	36690.301117	32.156852
659.927361	36748.890074	32.161869
660.292127	36810.963726	32.166887
661.093702	36879.414603	32.171904
661.768446	36938.223192	32.176922
662.391481	37006.472837	32.181940
663.144816	37061.893910	32.186957
663.736086	37138.902299	32.191975
664.746868	37183.295583	32.196992
665.610748	37248.455593	32.202010
666.180112	37304.526362	32.207028
666.786353	37353.952371	32.212045
667.174768	37414.685955	32.217063
668.373552	37473.318386	32.222080
668.884881	37518.887830	32.227098
669.306067	37577.975527	32.232116
669.919700	37622.378027	32.237133
670.279174	37677.750329	32.242151
671.037235	37732.237921	32.247168
671.951809	37793.267490	32.252186
672.234122	37851.105905	32.257204
673.083872	37895.912996	32.262221
673.454570	37965.061258	32.267239
674.150746	38025.964049	32.272256
674.760459	38087.420048	32.277274
675.412309	38146.573921	32.282292
676.368499	38214.751777	32.287309
676.970197	38282.215349	32.292327
677.579906	38335.084027	32.297344
678.355319	38402.734854	32.302362
678.557569	38467.443626	32.307380
679.231274	38521.822645	32.312397
679.946401	38600.831462	32.317415
680.736584	38660.895378	32.322432
681.508432	38729.055786	32.327450
682.087121	38796.958680	32.332468
683.005291	38864.974931	32.337485
683.626527	38929.965646	32.342503
684.109081	39000.770117	32.347520
684.873262	39065.809550	32.352538
685.384054	39144.301573	32.357556
686.616987	39219.159619	32.362573
686.837281	39284.863589	32.367591
687.471767	39345.809344	32.372608
688.474588	39407.483495	32.377626
689.025628	39481.636066	32.382644
689.790741	39551.465961	32.387661
690.412861	39628.709439	32.392679
691.065409	39700.475276	32.397696
691.903015	39763.881574	32.402714
692.690205	39835.984487	32.407732
693.807293	39896.916884	32.412749
694.345417	39967.292373	32.417767
695.037177	40032.607226	32.422784
695.791692	40089.009400	32.427802
696.506931	40163.077308	32.432820
697.191018	40225.265625	32.437837
697.847658	40293.349748	32.442855
698.626721	40355.668493	32.447872
699.448341	40416.293422	32.452890
699.700326	40490.646236	32.457908
700.898129	40551.246445	32.462925
701.494540	40614.601282	32.467943
702.491958	40676.019139	32.472960
703.222224	40731.072737	32.477978
704.133229	40788.029467	32.482996
704.618757	40847.072595	32.488013
705.176813	40907.017423	32.493031
705.929914	40970.582023	32.498048
706.793903	41015.097071	32.503066
707.190151	41077.708063	32.508084
708.085752	41124.810869	32.513101
708.451035	41187.565965	32.518119
708.578644	41249.737806	32.523136
709.128246	41300.362350	32.528154
710.175591	41367.478650	32.533172
710.846617	41428.646827	32.538189
711.292631	41498.357314	32.543207
712.065372	41564.231284	32.548224
712.649222	41635.623539	32.553242
712.927968	41713.795330	32.558260
713.840209	41777.607265	32.563277
714.832137	41865.964108	32.568295
715.313424	41933.961261	32.573312
716.194414	41994.675391	32.578330
716.567297	42073.038847	32.583348
717.503078	42138.160476	32.588365
718.119127	42227.288693	32.593383
718.704138	42304.354636	32.598400
719.488172	42379.045716	32.603418
719.852712	42476.223619	32.608436
720.779098	42565.468200	32.613453
721.537362	42643.520571	32.618471
722.207807	42732.753145	32.623488
723.239268	42799.483311	32.628506
724.106877	42889.177365	32.633524
725.186445	42965.533538	32.638541
725.701789	43043.557003	32.643559
726.525038	43121.692671	32.648576
727.602904	43184.653898	32.653594
728.050734	43272.644070	32.658612
728.875084	43338.056103	32.663629
729.737914	43412.890535	32.668647
730.080652	43486.517963	32.673664
731.076777	43566.255764	32.678682
731.689675	43651.650792	32.683700
732.498320	43719.962484	32.688717
733.297757	43789.922506	32.693735
733.841923	43868.658005	32.698752
734.858315	43928.818006	32.703770
735.391872	44008.861761	32.708788
736.191242	44082.646154	32.713805
736.930980	44164.291810	32.718823
737.550660	44234.531450	32.723840
738.375320	44305.729253	32.728858
739.251137	44391.773757	32.733876
740.192449	44446.319879	32.738893
741.150874	44527.894582	32.743911
741.835185	44599.983433	32.748928
742.830610	44667.385862	32.753946
743.478217	44737.225621	32.758964
744.071995	44799.970119	32.763981
744.876396	44861.293295	32.768999
745.374607	44939.548859	32.774016
746.294749	45002.844666	32.779034
747.032038	45068.592565	32.784052
747.685710	45125.584131	32.789069
748.177055	45187.169655	32.794087
749.100680	45248.913718	32.799104
750.160464	45305.093571	32.804122
750.312826	45368.020802	32.809140
751.485295	45439.432885	32.814157
752.069803	45496.578639	32.819175
752.501811	45572.976851	32.824192
753.393423	45638.942100	32.829210
753.872326	45713.257650	32.834228
754.669095	45773.929075	32.839245
755.231772	45866.639943	32.844263
756.038838	45938.815757	32.849280
756.741886	46014.664837	32.854298
757.234519	46085.440103	32.859316
757.974780	46172.650732	32.864333
758.807216	46254.446034	32.869351
759.672738	46332.917545	32.874368
760.751941	46407.844026	32.879386
761.247069	46493.338014	32.884404
761.890108	46570.252790	32.889421
762.751718	46644.833180	32.894439
763.271978	46740.293895	32.899456
764.561804	46821.283943	32.904474
765.183089	46904.090772	32.909492
766.007949	46983.893603	32.914509
766.818511	47053.347567	32.919527
767.644172	47146.733225	32.924544
768.231071	47225.010152	32.929562
768.887359	47307.772300	32.934580
769.694012	47380.714490	32.939597
770.784596	47469.323976	32.944615
771.406327	47557.664637	32.949632
772.781449	47633.946959	32.954650
773.534737	47716.348531	32.959668
773.984015	47795.031671	32.964685
774.856382	47862.068487	32.969703
775.224535	47942.970635	32.974720
775.910128	48018.342117	32.979738
776.573700	48102.450942	32.984756
777.717477	48195.548586	32.989773
778.516647	48277.456427	32.994791
779.214046	48371.919689	32.999808
779.957358	48448.558532	33.004826
780.738850	48531.407470	33.009844
781.514861	48618.873821	33.014861
782.592438	48696.558567	33.019879
783.084991	48782.404859	33.024896
784.440114	48864.551927	33.029914
785.123398	48933.648624	33.034932
786.015765	49009.922248	33.039949
786.869512	49079.434128	33.044967
787.298698	49170.164244	33.049984
788.522374	49237.207165	33.055002
789.031551	49317.613543	33.060020
789.440980	49390.248628	33.065037
790.273283	49454.101447	33.070055
790.682359	49534.669890	33.075072
791.835049	49602.148321	33.080090
792.289675	49688.853856	33.085108
793.127540	49766.483637	33.090125
793.807180	49839.945307	33.095143
794.587547	49923.403635	33.100160
795.598597	49998.586601	33.105178
796.210170	50075.417541	33.110196
796.530024	50155.693759	33.115213
797.562894	50240.956223	33.120231
798.392221	50340.202263	33.125248
799.663660	50417.586011	33.130266
800.719107	50498.248430	33.135284
801.330405	50584.160269	33.140301
802.421201	50656.868792	33.145319
802.885442	50742.621775	33.150336
803.697439	50822.598614	33.155354
804.673815	50897.456398	33.160372
804.921066	50987.984911	33.165389
806.059256	51075.172196	33.170407
806.901654	51157.168500	33.175424
807.685616	51237.776494	33.180442
808.655366	51332.578219	33.185460
809.216600	51420.487014	33.190477
810.391475	51495.274687	33.195495
810.794046	51585.809904	33.200512
811.781489	51666.163381	33.205530
812.746558	51755.789420	33.210548
813.495787	51845.958351	33.215565
814.165142	51931.485568	33.220583
815.057174	52017.217597	33.225600
815.670039	52107.030840	33.230618
816.504092	52198.077999	33.235636
817.596431	52284.672544	33.240653
818.405417	52364.435840	33.245671
819.086619	52470.250046	33.250688
819.957919	52546.791482	33.255706
820.880815	52636.343421	33.260724
821.716022	52729.393976	33.265741
822.668084	52812.974176	33.270759
823.040292	52897.830559	33.275776
824.025742	52985.054603	33.280794
824.758955	53090.974640	33.285812
825.518966	53178.478516	33.290829
826.746409	53261.341569	33.295847
827.398604	53354.500226	33.300864
828.013884	53439.522460	33.305882
829.041522	53536.819936	33.310900
829.931790	53621.698266	33.315917
831.036744	53706.615419	33.320935
831.679035	53803.726325	33.325952
832.541445	53892.643958	33.330970
832.856650	53975.197825	33.335988
833.505284	54051.623276	33.341005
834.608049	54128.816331	33.346023
835.439012	54223.516504	33.351040
836.168731	54305.264185	33.356058
837.429683	54385.579958	33.361076
838.103983	54479.842430	33.366093
838.881438	54560.763029	33.371111
839.368329	54655.558093	33.376128
840.394765	54730.177671	33.381146
840.800668	54825.690375	33.386164
841.725319	54923.920723	33.391181
843.142381	54999.476656	33.396199
844.095498	55098.969131	33.401216
844.552228	55187.736726	33.406234
845.256479	55279.814337	33.411252
846.301288	55371.039633	33.416269
847.255435	55451.756160	33.421287
847.797823	55563.576251	33.426304
848.875103	55645.072628	33.431322
849.746867	55748.353612	33.436340
850.193208	55844.269250	33.441357
851.220297	55924.202910	33.446375
851.988128	56040.787993	33.451392
852.925758	56134.275325	33.456410
853.922252	56219.928563	33.461428
854.752426	56320.959278	33.466445
855.656595	56422.041908	33.471463
856.485594	56522.407873	33.476480
857.458074	56628.468277	33.481498
858.386988	56724.134952	33.486516
859.169219	56830.065808	33.491533
860.181581	56922.569851	33.496551
861.098075	57003.807456	33.501568
862.012437	57116.635338	33.506586
863.007152	57200.168949	33.511604
863.867809	57301.948370	33.516621
864.894282	57395.317509	33.521639
865.701737	57482.818733	33.526656
866.486458	57586.284924	33.531674
867.500899	57672.033636	33.536692
868.170054	57766.961025	33.541709
869.041816	57854.437997	33.546727
869.813677	57951.537708	33.551744
870.649500	58051.576306	33.556762
871.777118	58136.002206	33.561780
872.722851	58243.951397	33.566797
873.714823	58332.390159	33.571815
874.335670	58430.921270	33.576832
875.359814	58523.639845	33.581850
875.680561	58607.849035	33.586868
876.608401	58712.138524	33.591885
877.827937	58815.163564	33.596903
878.556363	58914.062129	33.601920
879.599332	59004.200800	33.606938
880.336857	59087.480808	33.611956
880.862666	59184.600891	33.616973
882.133653	59253.498237	33.621991
882.798590	59360.491502	33.627008
883.746174	59442.347381	33.632026
884.234836	59535.986564	33.637044
885.037989	59628.973152	33.642061
885.991505	59709.882112	33.647079
886.676023	59811.280311	33.652096
887.633353	59911.085451	33.657114
888.686615	60005.473817	33.662132
889.553056	60117.266795	33.667149
890.221324	60214.347482	33.672167
891.071547	60318.061613	33.677184
892.238340	60418.006632	33.682202
893.242597	60515.818437	33.687220
893.750641	60614.057023	33.692237
894.692132	60715.138241	33.697255
895.807943	60831.972858	33.702272
896.570005	60931.243042	33.707290
898.051602	61024.024436	33.712308
898.495271	61132.297624	33.717325
899.378620	61227.830626	33.722343
900.732717	61345.552508	33.727360
901.154841	61438.403505	33.732378
902.256036	61540.486793	33.737396
903.083866	61652.986587	33.742413
904.206638	61749.529289	33.747431
905.121703	61853.172144	33.752448
906.029872	61957.410291	33.757466
907.445132	62047.305503	33.762484
908.283584	62148.082456	33.767501
908.778263	62255.577230	33.772519
909.654465	62351.574942	33.777536
911.060512	62457.343875	33.782554
911.957151	62550.143801	33.787572
912.477004	62657.128474	33.792589
913.399814	62754.064969	33.797607
914.537427	62852.928729	33.802624
915.289037	62965.754794	33.807642
916.530960	63056.418161	33.812660
916.951645	63168.186560	33.817677
918.290053	63265.590059	33.822695
919.528921	63368.943418	33.827712
920.058389	63465.112487	33.832730
920.955538	63557.860442	33.837748
921.692783	63671.551933	33.842765
922.765961	63770.746531	33.847783
923.441009	63864.011320	33.852800
924.149537	63989.175584	33.857818
925.266013	64076.443783	33.862836
926.193275	64190.215515	33.867853
927.256702	64297.464018	33.872871
928.213327	64414.864079	33.877888
929.024358	64519.185490	33.882906
930.211786	64610.622886	33.887924
930.596647	64708.924496	33.892941
931.510362	64801.356926	33.897959
932.672896	64898.487306	33.902976
933.145515	64993.324658	33.907994
934.267711	65102.883218	33.913012
935.158604	65210.205368	33.918029
935.975840	65315.063867	33.923047
937.143257	65417.808113	33.928064
938.182084	65519.929105	33.933082
939.143476	65615.443419	33.938100
939.853943	65715.002725	33.943117
940.568313	65833.937570	33.948135
941.883049	65941.704862	33.953152
942.447020	66053.587400	33.958170
943.604887	66154.865377	33.963188
944.520305	66268.919832	33.968205
945.548109	66375.506642	33.973223
946.034904	66482.865476	33.978240
947.120555	66605.428632	33.983258
948.278397	66712.978868	33.988276
949.376241	66834.366634	33.993293
949.808656	66938.423520	33.998311
950.975031	67066.387103	34.003328
951.779311	67182.410241	34.008346
952.751225	67292.368439	34.013364
953.442083	67431.632092	34.018381
954.696208	67537.090174	34.023399
955.824426	67664.969043	34.028416
956.680938	67787.629865	34.033434
957.944868	67903.568411	34.038452
958.757357	68023.262373	34.043469
959.606645	68148.883058	34.048487
960.791535	68258.809710	34.053504
961.648388	68381.625853	34.058522
962.687085	68497.837529	34.063540
963.774611	68622.109377	34.068557
964.983962	68739.445106	34.073575
965.745074	68859.961027	34.078592
966.432693	68977.115864	34.083610
967.919094	69087.965814	34.088628
968.724754	69211.945131	34.093645
969.596740	69325.490691	34.098663
970.558161	69443.552408	34.103680
971.690123	69562.288967	34.108698
972.681406	69670.289615	34.113716
973.594977	69794.274418	34.118733
974.497737	69911.211106	34.123751
975.817171	70033.395473	34.128768
976.670231	70141.155366	34.133786
977.659554	70259.590328	34.138804
978.555377	70377.832391	34.143821
979.280486	70496.285546	34.148839
980.643829	70613.089974	34.153856
981.520221	70729.966248	34.158874
982.596238	70826.909580	34.163892
983.373227	70943.904031	34.168909
984.484384	71041.297734	34.173927
985.486902	71144.774632	34.178944
986.204062	71261.767856	34.183962
987.545979	71353.168338	34.188980
988.365726	71465.881655	34.193997
989.335547	71579.468939	34.199015
990.302150	71680.054268	34.204032
990.967474	71807.155666	34.209050
991.953055	71910.468686	34.214068
992.963446	72029.258470	34.219085
993.679115	72141.177122	34.224103
995.020206	72259.865135	34.229120
995.814860	72379.215779	34.234138
996.849139	72505.662709	34.239156
997.852820	72611.238568	34.244173
998.837527	72752.979722	34.249191
1000.000979	72854.026247	34.254208
1000.803495	72983.110079	34.259226
1001.829470	73099.995547	34.264244
1002.630983	73231.235854	34.269261
1003.856416	73349.481201	34.274279
1005.126281	73468.908135	34.279296
1005.714861	73587.793315	34.284314
1007.218772	73713.566612	34.289332
1008.412158	73827.377658	34.294349
1008.868446	73956.699815	34.299367
1010.327349	74076.687995	34.304384
1011.109362	74209.182706	34.309402
1012.161971	74323.486593	34.314420
1013.087828	74453.388140	34.319437
1014.210098	74579.404544	34.324455
1015.573893	74697.977118	34.329472
1016.402211	74827.005586	34.334490
1017.313350	74950.258449	34.339508
1018.456103	75063.812859	34.344525
1019.345191	75198.287693	34.349543
1020.762207	75301.101005	34.354560
1021.715469	75443.883706	34.359578
1022.602466	75552.564979	34.364596
1023.832594	75681.901558	34.369613
1025.062893	75804.211509	34.374631
1025.833847	75916.591235	34.379648
1026.870767	76044.374640	34.384666
1027.983016	76168.494058	34.389684
1029.095119	76284.828289	34.394701
1029.862950	76406.299089	34.399719
1030.736706	76533.283648	34.404736
1032.014030	76658.504755	34.409754
1032.943706	76781.626839	34.414772
1034.030778	76908.187983	34.419789
1035.141281	77022.712882	34.424807
1036.569322	77152.299161	34.429824
1037.237017	77270.668970	34.434842
1038.202250	77388.733015	34.439860
1039.331478	77481.118131	34.444877
1040.017036	77603.304411	34.449895
1041.367797	77713.680549	34.454912
1041.896460	77833.535723	34.459930
1043.063673	77946.179693	34.464948
1043.987299	78061.321643	34.469965
1044.649485	78181.315632	34.474983
1046.023963	78284.226734	34.480000
1046.540741	78431.998243	34.485018
1047.481240	78554.326645	34.490036
1048.851523	78682.775214	34.495053
1049.695462	78813.185520	34.500071
1050.896334	78936.049964	34.505088
1052.025868	79071.972307	34.510106
1052.922852	79211.541654	34.515124
1053.948272	79333.658946	34.520141
1055.108812	79476.961655	34.525159
1056.334651	79602.815852	34.530176
1057.466767	79736.757455	34.535194
1058.434710	79881.212409	34.540212
1059.594873	80017.129818	34.545229
1060.553639	80150.210434	34.550247
1061.413659	80286.013012	34.555264
1062.526111	80426.984889	34.560282
1063.895501	80566.924449	34.565300
1064.872838	80700.315395	34.570317
1065.760301	80843.968145	34.575335
1067.270244	80969.766544	34.580352
1067.891773	81100.953667	34.585370
1068.914092	81257.597016	34.590388
1070.350510	81384.364149	34.595405
1071.726933	81527.981802	34.600423
1072.662215	81659.141518	34.605440
1073.743215	81796.075683	34.610458
1074.880196	81928.456672	34.615476
1076.369208	82067.622444	34.620493
1077.169216	82210.577909	34.625511
1078.221582	82326.759976	34.630528
1079.324766	82457.322751	34.635546
1080.324550	82597.025034	34.640564
1081.732858	82730.784037	34.645581
1082.524352	82866.323600	34.650599
1083.643541	83009.739519	34.655616
1084.778169	83132.247481	34.660634
1085.994777	83265.762235	34.665652
1087.153882	83400.608278	34.670669
1088.337553	83545.787766	34.675687
1089.690260	83664.534172	34.680704
1091.007277	83794.780476	34.685722
1091.634921	83921.223833	34.690740
1093.066789	84046.035371	34.695757
1094.228118	84160.945862	34.700775
1095.543004	84282.148468	34.705792
1096.276572	84404.961571	34.710810
1097.580177	84514.888388	34.715828
1098.383635	84626.292559	34.720845
1099.268293	84744.335536	34.725863
1100.646955	84857.900214	34.730880
1101.933032	84970.993401	34.735898
1102.624978	85082.221718	34.740916
1103.553268	85206.443716	34.745933
1104.362763	85328.523027	34.750951
1105.406551	85445.716360	34.755968
1106.204506	85577.889782	34.760986
1107.016179	85700.400826	34.766004
1108.613205	85827.795250	34.771021
1109.305828	85975.725089	34.776039
1110.484529	86109.630604	34.781056
1111.631028	86250.971394	34.786074
1112.588953	86393.386385	34.791092
1113.380873	86542.189569	34.796109
1114.476087	86684.091483	34.801127
1115.635038	86835.032403	34.806144
1116.903114	86981.202113	34.811162
1117.949061	87142.842789	34.816180
1118.926629	87287.069021	34.821197
1119.955510	87441.866726	34.826215
1120.924792	87594.967759	34.831232
1122.202786	87753.370271	34.836250
1123.412512	87915.186749	34.841268
1124.851865	88065.668093	34.846285
1125.729570	88221.722196	34.851303
1126.944679	88380.379622	34.856320
1127.973625	88543.216033	34.861338
1128.992525	88706.466303	34.866356
1130.582742	88845.856592	34.871373
1131.193885	89010.609461	34.876391
1132.818393	89177.757199	34.881408
1133.583063	89335.949447	34.886426
1134.635677	89498.220160	34.891444
1135.975898	89652.737615	34.896461
1137.148869	89818.583516	34.901479
1138.311723	89987.423506	34.906496
1139.431006	90142.624624	34.911514
1140.652698	90304.495041	34.916532
1141.863317	90462.162927	34.921549
1143.010962	90617.679127	34.926567
1144.560195	90789.803026	34.931584
1145.767780	90928.040667	34.936602
1146.689738	91098.205063	34.941620
1148.173745	91240.138348	34.946637
1149.314070	91405.603094	34.951655
1150.686657	91555.189606	34.956672
1151.759327	91713.868745	34.961690
1152.773210	91860.952996	34.966708
1154.386521	92009.688477	34.971725
1155.416229	92163.096739	34.976743
1156.674058	92306.913345	34.981760
1157.885478	92453.736145	34.986778
1158.890109	92592.680646	34.991796
1160.088436	92717.370959	34.996813
1161.494242	92839.669860	35.001831
1162.629210	92981.328373	35.006848
1163.598716	93100.042373	35.011866
1164.803059	93239.781420	35.016884
1165.939499	93376.167305	35.021901
1166.584357	93503.113179	35.026919
1167.708645	93642.494328	35.031936
1168.822765	93784.325750	35.036954
1169.845569	93930.473632	35.041972
1171.495671	94077.560046	35.046989
1172.245149	94228.901979	35.052007
1173.111695	94370.295800	35.057024
1174.556400	94524.084564	35.062042
1175.438764	94690.962226	35.067060
1176.543247	94835.768438	35.072077
1177.567115	95002.031347	35.077095
1178.858039	95151.047946	35.082112
1180.127377	95317.963643	35.087130
1181.122588	95491.243339	35.092148
1182.270423	95649.527557	35.097165
1183.560506	95820.903208	35.102183
1184.693664	95984.164032	35.107200
1186.067237	96142.763747	35.112218
1187.113291	96325.587246	35.117236
1188.511891	96472.261315	35.122253
1189.756704	96648.692114	35.127271
1190.500736	96814.032441	35.132288
1192.309612	96976.788169	35.137306
1193.189357	97150.934029	35.142324
1194.709736	97314.636351	35.147341
1195.892005	97479.652501	35.152359
1197.263004	97650.383941	35.157376
1198.592477	97796.932105	35.162394
1199.478131	97969.615654	35.167412
1200.684060	98140.876800	35.172429
1201.907806	98308.024320	35.177447
1203.291585	98477.418775	35.182464
1204.481587	98641.973993	35.187482
1205.537990	98815.554134	35.192500
1207.078115	98971.825392	35.197517
1208.286569	99133.819005	35.202535
1209.313737	99299.220969	35.207552
1211.518023	99442.958177	35.212570
1213.250835	99589.194353	35.217588
1214.665874	99731.818843	35.222605
1216.097578	99867.140544	35.227623
1216.788254	100015.329262	35.232640
1218.364786	100157.443562	35.237658
1219.628010	100299.045467	35.242676
1220.939922	100451.567007	35.247693
1221.779743	100582.096351	35.252711
1222.910153	100726.600743	35.257728
1224.002090	100854.630364	35.262746
1224.653547	100995.568246	35.267764
1225.943330	101133.495055	35.272781
1226.949940	101273.422780	35.277799
1227.881044	101421.462090	35.282816
1229.153730	101559.387828	35.287834
1230.068828	101713.163966	35.292852
1230.968916	101864.969403	35.297869
1231.954919	102021.969541	35.302887
1233.083410	102184.364291	35.307904
1234.168284	102364.034557	35.312922
1235.339505	102527.854900	35.317940
1236.666693	102698.909220	35.322957
1238.224495	102869.181483	35.327975
1239.423196	103040.258731	35.332992
1240.497588	103208.085613	35.338010
1241.544315	103386.320781	35.343028
1242.547384	103553.452776	35.348045
1244.030631	103747.794937	35.353063
1245.145893	103918.050263	35.358080
1246.794775	104098.846465	35.363098
1247.662045	104275.851339	35.368116
1249.180039	104462.771248	35.373133
1250.591768	104635.167773	35.378151
1251.110428	104829.191275	35.383168
1253.029272	105004.749844	35.388186
1254.254448	105193.437002	35.393204
1255.721857	105365.019993	35.398221
1257.034090	105548.576625	35.403239
1258.351909	105729.254413	35.408256
1259.693558	105907.233912	35.413274
1260.944939	106092.797850	35.418292
1262.063105	106281.776455	35.423309
1263.934012	106446.772159	35.428327
1264.604763	106633.021152	35.433344
1266.231213	106814.215015	35.438362
1267.418055	106999.372244	35.443380
1268.661438	107176.161730	35.448397
1270.132754	107348.897544	35.453415
1271.568083	107539.708969	35.458432
1273.067919	107713.803563	35.463450
1274.068512	107887.580062	35.468468
1275.376270	108057.828084	35.473485
1276.924030	108239.760386	35.478503
1277.904995	108413.651389	35.483520
1279.355589	108584.570284	35.488538
1280.882184	108762.788412	35.493556
1282.330525	108928.520239	35.498573
1283.586581	109115.410586	35.503591
1284.536554	109281.312656	35.508608
1286.622905	109449.984661	35.513626
1287.454707	109631.110826	35.518644
1288.453305	109797.590987	35.523661
1290.026519	109968.424189	35.528679
1290.892689	110143.276254	35.533696
1292.256912	110318.537771	35.538714
1293.606475	110467.801119	35.543732
1294.873320	110636.674905	35.548749
1296.027504	110800.029342	35.553767
1296.810350	110971.957298	35.558784
1298.274651	111126.789192	35.563802
1299.635246	111296.545110	35.568820
1300.467468	111472.855240	35.573837
1301.709055	111637.441994	35.578855
1302.972794	111822.288287	35.583872
1304.180752	111994.579915	35.588890
1305.526202	112181.821287	35.593908
1306.794912	112368.474923	35.598925
1308.176076	112549.889780	35.603943
1309.231286	112738.479163	35.608960
1310.868008	112926.686358	35.613978
1312.005529	113118.620535	35.618996
1312.969695	113317.186216	35.624013
1314.446081	113504.726944	35.629031
1315.690608	113696.009200	35.634048
1317.192573	113884.428639	35.639066
1318.314273	114082.494259	35.644084
1319.767025	114277.495503	35.649101
1321.144947	114479.518092	35.654119
1322.362021	114677.870796	35.659136
1324.047757	114879.303245	35.664154
1325.513216	115070.003780	35.669172
1326.717647	115276.447535	35.674189
1328.349188	115471.018128	35.679207
1329.785713	115670.382025	35.684224
1331.133333	115862.208851	35.689242
1332.668817	116064.472346	35.694260
1334.003803	116252.606859	35.699277
1335.051737	116438.357266	35.704295
1336.636587	116640.750464	35.709312
1338.274945	116820.870113	35.714330
1339.500503	117015.301834	35.719348
1340.297269	117211.145414	35.724365
1342.192071	117394.989123	35.729383
1343.576847	117599.403429	35.734400
1345.031104	117798.787534	35.739418
1346.016615	117975.961034	35.744436
1347.369286	118175.269242	35.749453
1348.889541	118365.048734	35.754471
1349.623984	118570.669497	35.759488
1351.260472	118767.505861	35.764506
1353.127070	118959.083525	35.769524
1354.091668	119150.109480	35.774541
1355.603065	119349.730799	35.779559
1356.702759	119548.925210	35.784576
1358.451102	119739.767638	35.789594
1359.636781	119942.978478	35.794612
1361.004828	120144.597928	35.799629
1362.541022	120348.857996	35.804647
1363.485984	120538.820853	35.809664
1365.214084	120730.788218	35.814682
1366.786324	120913.308867	35.819700
1367.710429	121105.229462	35.824717
1368.867281	121278.016433	35.829735
1370.333792	121462.406730	35.834752
1371.866086	121628.208826	35.839770
1373.406948	121817.567011	35.844788
1374.964598	121999.464309	35.849805
1376.369994	122173.230859	35.854823
1377.582818	122357.870396	35.859840
1378.718218	122542.270227	35.864858
1380.129040	122734.492649	35.869876
1381.320145	122932.298775	35.874893
1382.755605	123123.747528	35.879911
1384.079945	123320.838785	35.884928
1385.322000	123504.012478	35.889946
1386.939858	123704.454302	35.894964
1388.080741	123896.158085	35.899981
1389.907073	124089.590861	35.904999
1390.936504	124292.397801	35.910016
1392.251625	124482.558195	35.915034
1394.113974	124680.929275	35.920052
1395.177622	124891.980954	35.925069
1396.640576	125089.683889	35.930087
1398.188636	125290.288024	35.935104
1399.414096	125502.547423	35.940122
1400.682887	125706.112328	35.945140
1401.800844	125907.384736	35.950157
1403.551159	126109.862831	35.955175
1404.993058	126322.296947	35.960192
1405.966816	126546.536740	35.965210
1407.654162	126743.012761	35.970228
1408.826694	126966.299735	35.975245
1410.008033	127171.928963	35.980263
1411.413189	127393.117704	35.985280
1413.432225	127605.837490	35.990298
1414.831703	127843.739181	35.995316
1416.116325	128049.573951	36.000333
1417.974931	128256.041121	36.005351
1419.399910	128483.860771	36.010368
1420.620843	128689.089730	36.015386
1422.264517	128900.675752	36.020404
1423.625307	129128.029545	36.025421
1425.191353	129340.923432	36.030439
1426.608526	129542.327072	36.035456
1428.255472	129759.607247	36.040474
1429.596368	129972.022355	36.045492
1430.878322	130184.005050	36.050509
1432.955664	130388.122370	36.055527
1434.041986	130598.188317	36.060544
1435.203806	130802.834214	36.065562
1436.802519	131012.897877	36.070580
1438.478121	131230.311661	36.075597
1439.732634	131440.686608	36.080615
1440.934021	131655.429818	36.085632
1442.535311	131846.229289	36.090650
1443.834674	132053.104938	36.095668
1445.325566	132252.121866	36.100685
1446.972625	132443.006794	36.105703
1448.093429	132646.228287	36.110720
1449.270436	132842.321852	36.115738
1450.763739	133035.933889	36.120756
1452.015747	133248.451256	36.125773
1453.660560	133448.453068	36.130791
1454.742094	133659.885625	36.135808
1455.927595	133866.121073	36.140826
1457.673199	134080.669492	36.145844
1458.704720	134303.543462	36.150861
1461.067845	134522.444423	36.155879
1461.958113	134731.520547	36.160896
1463.074021	134960.341433	36.165914
1464.676851	135178.988076	36.170932
1465.949216	135403.618904	36.175949
1467.709378	135626.057905	36.180967
1469.361121	135860.477438	36.185984
1470.800137	136083.477828	36.191002
1472.579082	136299.241254	36.196020
1473.682461	136536.059562	36.201037
1475.366518	136760.660838	36.206055
1476.806237	136993.856044	36.211072
1478.262125	137206.915098	36.216090
1479.780805	137434.475010	36.221108
1481.125907	137673.012848	36.226125
1482.634147	137903.441923	36.231143
1484.465247	138127.776886	36.236160
1485.827209	138367.483519	36.241178
1487.248913	138591.633612	36.246196
1488.767286	138829.126822	36.251213
1490.292176	139062.971204	36.256231
1492.216215	139291.596241	36.261248
1493.466764	139531.786217	36.266266
1495.080433	139756.320145	36.271284
1496.636198	140004.208559	36.276301
1497.976393	140229.423144	36.281319
1499.665320	140450.275149	36.286336
1501.256578	140697.745458	36.291354
1503.082351	140920.061955	36.296372
1504.340951	141148.236622	36.301389
1506.065768	141369.355828	36.306407
1507.503872	141611.154888	36.311424
1508.734785	141837.995764	36.316442
1510.654817	142059.519916	36.321460
1512.301943	142306.196094	36.326477
1513.442273	142534.083155	36.331495
1515.101335	142771.407780	36.336512
1516.686484	143004.918380	36.341530
1518.101130	143217.418488	36.346548
1519.483327	143458.049732	36.351565
1520.611762	143688.583572	36.356583
1522.220235	143935.190327	36.361600
1523.550397	144154.998251	36.366618
1525.430938	144380.968981	36.371636
1527.002601	144594.239506	36.376653
1528.176933	144813.582556	36.381671
1529.902024	145035.438054	36.386688
1531.294631	145253.697514	36.391706
1533.199439	145470.964523	36.396724
1534.302182	145690.451893	36.401741
1535.740230	145919.863094	36.406759
1537.105065	146141.276688	36.411776
1538.361018	146370.935609	36.416794
1540.153895	146609.890934	36.421812
1541.500034	146840.502318	36.426829
1542.708845	147079.084986	36.431847
1544.528474	147325.317456	36.436864
1545.770652	147579.071760	36.441882
1547.681742	147817.535773	36.446900
1549.007836	148056.969171	36.451917
1550.481896	148303.974016	36.456935
1552.572832	148545.178376	36.461952
1554.103364	148790.961087	36.466970
1555.538674	149041.007497	36.471988
1557.007780	149293.167512	36.477005
1558.613504	149537.891842	36.482023
1560.079231	149785.936283	36.487040
1561.861282	150034.363408	36.492058
1563.634095	150291.870759	36.497076
1564.935419	150541.848700	36.502093
1566.736226	150787.996732	36.507111
1568.185991	151056.045644	36.512128
1569.897363	151307.637771	36.517146
1571.526302	151554.642947	36.522164
1572.948487	151803.838049	36.527181
1574.471945	152075.623565	36.532199
1576.645305	152311.581639	36.537216
1577.847391	152574.560449	36.542234
1579.734804	152822.421582	36.547252
1581.480291	153074.021843	36.552269
1582.619954	153329.396962	36.557287
1584.441154	153579.150679	36.562304
1585.666668	153838.370321	36.567322
1587.345417	154087.719415	36.572340
1589.236170	154354.305118	36.577357
1590.645250	154616.874193	36.582375
1592.464459	154864.875500	36.587392
1594.304797	155132.971522	36.592410
1595.962609	155369.603756	36.597428
1597.276591	155628.861238	36.602445
1598.976392	155893.676361	36.607463
1600.835928	156143.379699	36.612480
1602.115600	156403.878466	36.617498
1604.101501	156647.542683	36.622516
1605.259853	156900.368011	36.627533
1607.112052	157156.381750	36.632551
1608.713491	157400.594238	36.637568
1610.186273	157656.900216	36.642586
1612.234032	157890.115180	36.647604
1613.770158	158134.203776	36.652621
1614.882949	158370.043108	36.657639
1617.095062	158586.841163	36.662656
1618.184773	158824.221572	36.667674
1619.899961	159062.467981	36.672692
1621.443070	159297.991671	36.677709
1622.961827	159522.704233	36.682727
1624.664203	159767.449986	36.687744
1626.445194	160017.739165	36.692762
1627.622865	160257.765647	36.697780
1629.272146	160501.840190	36.702797
1630.591149	160762.137260	36.707815
1632.353493	161000.516174	36.712832
1633.833236	161261.615671	36.717850
1635.472225	161513.358322	36.722868
1637.093131	161773.931916	36.727885
1638.550964	162029.879188	36.732903
1640.232965	162305.842358	36.737920
1641.625511	162565.900005	36.742938
1643.648144	162825.605838	36.747956
1645.245251	163087.689234	36.752973
1646.814372	163372.365637	36.757991
1648.770131	163631.834263	36.763008
1650.663484	163905.911868	36.768026
1652.020349	164181.776168	36.773044
1653.692727	164441.612644	36.778061
1655.348888	164713.032649	36.783079
1657.177738	164990.743168	36.788096
1658.640819	165256.490705	36.793114
1660.524754	165528.958608	36.798132
1662.258670	165811.712781	36.803149
1663.693802	166077.115557	36.808167
1665.726837	166339.622335	36.813184
1667.098709	166628.997375	36.818202
1669.089573	166893.467967	36.823220
1670.601207	167177.675684	36.828237
1672.237686	167451.998035	36.833255
1674.498095	167718.790780	36.838272
1675.805546	167998.014470	36.843290
1677.963381	168262.163802	36.848308
1679.676689	168540.566037	36.853325
1681.044216	168817.553897	36.858343
1683.145514	169078.191784	36.863360
1684.769390	169355.130170	36.868378
1686.408592	169623.151178	36.873396
1688.133934	169889.092856	36.878413
1689.879865	170167.298846	36.883431
1691.656152	170420.640586	36.888448
1693.013347	170696.755780	36.893466
1694.702549	170969.839348	36.898484
1696.350242	171236.995004	36.903501
1698.061688	171520.493032	36.908519
1699.717376	171799.181732	36.913536
1701.590567	172061.639211	36.918554
1703.093026	172316.977593	36.923572
1704.649910	172576.736095	36.928589
1706.170649	172826.772511	36.933607
1707.714650	173088.743655	36.938624
1709.182117	173357.515352	36.943642
1710.828597	173610.073824	36.948660
1712.765537	173882.922671	36.953677
1714.134028	174145.410703	36.958695
1715.901201	174411.262291	36.963712
1717.574729	174694.332428	36.968730
1719.215913	174968.123637	36.973748
1721.268644	175241.952850	36.978765
1722.833331	175532.454752	36.983783
1724.663499	175793.028061	36.988800
1726.148961	176088.227699	36.993818
1727.671064	176366.411321	36.998836
1729.772182	176647.816050	37.003853
1731.527089	176945.643241	37.008871
1732.874232	177226.550012	37.013888
1734.515850	177527.938954	37.018906
1736.494586	177815.003972	37.023924
1738.140462	178119.327179	37.028941
1740.028279	178417.029680	37.033959
1741.478797	178705.910133	37.038976
1743.127257	179018.219619	37.043994
1744.826914	179319.396618	37.049012
1746.870830	179615.332009	37.054029
1748.271796	179927.915902	37.059047
1750.262691	180232.288451	37.064064
1752.085059	180540.090203	37.069082
1754.008465	180859.931413	37.074100
1755.472075	181180.761530	37.079117
1757.156916	181497.219672	37.084135
1759.234147	181793.279070	37.089152
1760.980478	182114.718335	37.094170
1762.706367	182428.689921	37.099188
1764.937574	182741.733436	37.104205
1766.489822	183060.063815	37.109223
1768.373775	183366.188359	37.114240
1770.101228	183662.442863	37.119258
1772.029390	183979.882780	37.124276
1773.875265	184287.352059	37.129293
1775.695170	184605.663781	37.134311
1777.795818	184904.608107	37.139328
1779.610083	185211.073670	37.144346
1781.348450	185507.808217	37.149364
1783.457173	185807.708954	37.154381
1785.393838	186113.844004	37.159399
1786.926369	186422.748089	37.164416
1788.707262	186714.192374	37.169434
1790.375180	187019.170692	37.174452
1792.524688	187323.947694	37.179469
1794.161718	187628.008629	37.184487
1796.116117	187926.171245	37.189504
1797.825706	188219.083017	37.194522
1799.242306	188505.228705	37.199540
1801.359352	188779.970938	37.204557
1802.938103	189064.495387	37.209575
1804.574940	189336.170000	37.214592
1806.338900	189625.122657	37.219610
1808.429951	189905.916114	37.224628
1810.102014	190195.115267	37.229645
1811.546688	190480.557858	37.234663
1813.535249	190771.486925	37.239680
1815.119710	191068.725645	37.244698
1816.590781	191357.735315	37.249716
1818.586624	191651.422422	37.254733
1820.306645	191961.944965	37.259751
1822.126745	192259.965826	37.264768
1824.114581	192571.515783	37.269786
1825.699529	192883.766228	37.274804
1827.668018	193186.223725	37.279821
1828.835023	193517.022739	37.284839
1830.817160	193816.271069	37.289856
1832.859878	194142.391795	37.294874
1834.476651	194469.331059	37.299892
1836.921176	194793.488552	37.304909
1838.639710	195106.061752	37.309927
1840.184411	195436.750074	37.314944
1842.141737	195754.632568	37.319962
1843.825995	196077.649807	37.324980
1845.815728	196399.935242	37.329997
1847.553485	196739.485698	37.335015
1849.942832	197068.781332	37.340032
1851.807442	197391.993978	37.345050
1853.312964	197724.556330	37.350068
1855.278344	198041.753607	37.355085
1857.089838	198377.876165	37.360103
1859.274627	198719.881690	37.365120
1861.226496	199051.493141	37.370138
1863.073095	199370.595771	37.375156
1865.193938	199693.502670	37.380173
1866.837555	200036.376821	37.385191
1868.776827	200359.316552	37.390208
1870.856059	200679.583184	37.395226
1872.843742	201006.923545	37.400244
1874.655868	201335.677283	37.405261
1876.587568	201668.425055	37.410279
1878.476646	201988.767640	37.415296
1880.237262	202323.018939	37.420314
1882.111816	202648.686147	37.425332
1884.359831	202972.645843	37.430349
1886.088185	203311.185891	37.435367
1888.158332	203623.321836	37.440384
1890.091674	203965.108233	37.445402
1891.610591	204288.099566	37.450420
1893.574095	204617.204059	37.455437
1895.653772	204936.847760	37.460455
1897.386464	205280.260619	37.465472
1899.368301	205596.026466	37.470490
1901.365091	205916.526558	37.475508
1903.151175	206212.727141	37.480525
1904.444870	206527.413998	37.485543
1906.522983	206839.781940	37.490560
1908.497617	207150.543079	37.495578
1909.629670	207477.840770	37.500596
1911.984504	207789.890528	37.505613
1913.736285	208109.730524	37.510631
1915.448136	208445.992724	37.515648
1917.784025	208765.794287	37.520666
1919.357933	209094.896779	37.525684
1921.149085	209414.293101	37.530701
1923.377802	209751.851537	37.535719
1924.723325	210089.666235	37.540736
1926.801388	210426.274751	37.545754
1928.619659	210771.876373	37.550772
1930.638662	211117.283012	37.555789
1932.421485	211453.296451	37.560807
1934.558733	211797.393135	37.565824
1936.361313	212148.933508	37.570842
1937.999957	212515.837949	37.575860
1940.278503	212866.646563	37.580877
1942.473864	213224.846429	37.585895
1944.015400	213571.205390	37.590912
1946.327914	213932.259773	37.595930
1947.949949	214290.366016	37.600948
1950.205064	214640.299159	37.605965
1952.265100	215005.538322	37.610983
1954.191327	215351.667817	37.616000
1956.370047	215723.671726	37.621018
1958.188985	216082.035621	37.626036
1960.624805	216447.527663	37.631053
1962.574416	216805.684174	37.636071
1964.322644	217151.978022	37.641088
1966.746364	217515.484320	37.646106
1968.594006	217880.962999	37.651124
1970.536710	218228.031203	37.656141
1972.881651	218591.111191	37.661159
1974.977536	218946.170165	37.666176
1977.038435	219298.341598	37.671194
1978.976054	219657.682609	37.676212
1981.077940	219998.220688	37.681229
1982.920074	220355.612286	37.686247
1984.741207	220708.806258	37.691264
1987.138694	221061.720015	37.696282
1989.008539	221431.987220	37.701300
1991.263683	221779.352933	37.706317
1992.841364	222140.985135	37.711335
1994.943773	222477.382499	37.716352
1997.213956	222843.174449	37.721370
1998.945394	223189.601211	37.726388
2001.173565	223548.279937	37.731405
2003.107043	223900.213904	37.736423
2004.626066	224255.834013	37.741440
2006.769016	224665.448623	37.746458
2008.464846	225006.352889	37.751476
2010.424266	225347.775486	37.756493
2012.439100	225689.863720	37.761511
2014.183493	226026.345761	37.766528
2016.261136	226369.137962	37.771546
2018.105299	226718.101744	37.776564
2019.970242	227067.965256	37.781581
2022.092179	227415.326038	37.786599
2023.823993	227766.737356	37.791616
2025.785954	228112.170878	37.796634
2027.775948	228480.483534	37.801652
2029.742545	228842.630121	37.806669
2031.728445	229201.702165	37.811687
2033.676771	229581.683172	37.816704
2035.861495	229946.872740	37.821722
2037.422620	230332.683489	37.826740
2039.985251	230706.349599	37.831757
2042.092858	231084.686333	37.836775
2043.747943	231462.004346	37.841792
2045.946376	231834.082044	37.846810
2048.044419	232222.101389	37.851828
2049.946524	232615.309143	37.856845
2052.315355	233003.720524	37.861863
2054.032780	233388.833525	37.866880
2056.164329	233776.701543	37.871898
2058.177125	234182.190774	37.876916
2060.507061	234565.712806	37.881933
2062.886301	234960.454517	37.886951
2064.302820	235358.779285	37.891968
2067.177044	235749.610443	37.896986
2069.034869	236141.340897	37.902004
2070.931368	236536.114544	37.907021
2073.337101	236938.326931	37.912039
2075.266803	237322.100653	37.917056
2077.718681	237713.641193	37.922074
2080.156578	238118.977035	37.927092
2082.096912	238498.638663	37.932109
2084.646101	238890.422031	37.937127
2086.914581	239289.464708	37.942144
2089.211286	239650.786317	37.947162
2091.601136	240033.455224	37.952180
2093.642392	240414.199553	37.957197
2095.807938	240789.007325	37.962215
2097.951343	241162.575234	37.967232
2100.093127	241537.414577	37.972250
2101.746985	241920.384245	37.977268
2104.130784	242285.230816	37.982285
2106.492968	242666.718905	37.987303
2108.333659	243044.938089	37.992320
2110.382793	243422.287158	37.997338
2112.610452	243801.793464	38.002356
2114.562425	244174.613553	38.007373
2116.773949	244563.751392	38.012391
2119.133376	244939.226899	38.017408
2121.456904	245306.301601	38.022426
2123.221013	245666.480884	38.027444
2124.911121	246017.452432	38.032461
2126.917486	246359.840082	38.037479
2128.705490	246717.554480	38.042496
2131.096722	247080.686101	38.047514
2133.211295	247439.798390	38.052532
2135.264097	247791.097878	38.057549
2137.349699	248159.360902	38.062567
2139.115980	248529.072554	38.067584
2141.271434	248889.960001	38.072602
2142.733741	249286.443744	38.077620
2144.908124	249657.973122	38.082637
2147.491412	250028.803504	38.087655
2149.324348	250426.628446	38.092672
2151.544745	250815.781830	38.097690
2153.716839	251210.328929	38.102708
2155.773710	251607.689420	38.107725
2157.941263	252007.370249	38.112743
2159.850720	252409.048877	38.117760
2162.279457	252800.993411	38.122778
2164.022968	253214.512024	38.127796
2166.416745	253617.843916	38.132813
2168.821240	254026.179179	38.137831
2170.754512	254446.224178	38.142848
2172.785405	254860.996399	38.147866
2175.007611	255283.588417	38.152884
2177.357594	255693.841031	38.157901
2179.590599	256115.772641	38.162919
2181.574744	256536.855501	38.167936
2184.137538	256946.187781	38.172954
2186.272565	257376.037571	38.177972
2188.078167	257801.291801	38.182989
2190.579393	258223.794666	38.188007
2192.615411	258659.987815	38.193024
2195.161915	259077.556962	38.198042
2197.651868	259507.405244	38.203060
2199.691597	259930.695580	38.208077
2202.157703	260359.456785	38.213095
2204.410816	260792.139082	38.218112
2206.953949	261205.241369	38.223130
2209.044515	261638.331821	38.228148
2211.028083	262062.320283	38.233165
2213.653101	262482.371807	38.238183
2216.009351	262907.369290	38.243200
2218.059985	263326.471525	38.248218
2220.427279	263744.838210	38.253236
2222.940375	264170.345941	38.258253
2224.990959	264578.501061	38.263271
2227.485449	265005.562333	38.268288
2229.987830	265418.879777	38.273306
2231.671764	265837.687492	38.278324
2233.859486	266254.459717	38.283341
2236.336459	266666.613921	38.288359
2238.428004	267094.681207	38.293376
2240.469324	267504.212517	38.298394
2242.845228	267903.377414	38.303412
2244.853317	268298.587233	38.308429
2246.941383	268686.062073	38.313447
2249.264456	269090.088254	38.318464
2251.539548	269475.298480	38.323482
2253.545458	269874.040774	38.328500
2255.858665	270288.230606	38.333517
2257.978187	270678.191202	38.338535
2259.660512	271084.504855	38.343552
2262.090057	271497.076473	38.348570
2264.188422	271917.398006	38.353588
2266.325504	272337.688169	38.358605
2269.075322	272750.615972	38.363623
2271.011907	273186.942352	38.368640
2273.377510	273603.284574	38.373658
2275.495514	274031.554945	38.378676
2277.550942	274468.701112	38.383693
2279.889678	274901.026587	38.388711
2282.306795	275345.533323	38.393728
2284.412154	275782.620909	38.398746
2286.606666	276221.167765	38.403764
2288.881713	276668.008755	38.408781
2291.595621	277114.957957	38.413799
2293.549663	277569.673994	38.418816
2296.084537	278010.707043	38.423834
2298.459615	278466.448489	38.428852
2300.678074	278921.477937	38.433869
2303.000071	279372.400875	38.438887
2305.367445	279838.787098	38.443904
2307.569878	280287.137475	38.448922
2310.083592	280746.361726	38.453940
2312.308261	281204.793241	38.458957
2315.035006	281664.288040	38.463975
2317.188634	282124.533882	38.468992
2319.365836	282579.669607	38.474010
2322.020812	283042.807490	38.479028
2324.145971	283509.610844	38.484045
2326.530462	283966.313011	38.489063
2328.840636	284442.180552	38.494080
2331.545266	284894.004504	38.499098
2334.182081	285365.754818	38.504116
2336.632272	285822.978219	38.509133
2339.126338	286266.171658	38.514151
2341.527771	286737.576671	38.519168
2344.107406	287185.328040	38.524186
2346.234926	287639.831508	38.529204
2348.325493	288105.492137	38.534221
2350.922996	288560.072300	38.539239
2353.272996	289016.875703	38.544256
2355.491973	289468.999680	38.549274
2357.887164	289931.052945	38.554292
2359.826553	290396.632502	38.559309
2362.351867	290857.469719	38.564327
2364.714649	291329.559903	38.569344
2367.058440	291777.494356	38.574362
2369.540029	292218.141048	38.579380
2371.818795	292651.249155	38.584397
2374.387166	293074.683045	38.589415
2376.603123	293513.921560	38.594432
2378.964798	293941.984492	38.599450
2381.117132	294377.344869	38.604468
2383.402537	294814.461459	38.609485
2385.885687	295254.517885	38.614503
2388.148825	295705.556613	38.619520
2390.237522	296150.906521	38.624538
2392.921004	296590.775934	38.629556
2394.974606	297050.760995	38.634573
2397.204212	297497.990683	38.639591
2399.647710	297967.386674	38.644608
2402.106089	298418.057963	38.649626
2404.204449	298880.343000	38.654644
2406.798915	299367.619688	38.659661
2409.417822	299830.429368	38.664679
2411.567253	300293.515412	38.669696
2413.854581	300776.670900	38.674714
2416.714091	301245.103068	38.679732
2418.836153	301731.152274	38.684749
2421.261839	302214.510135	38.689767
2423.887748	302691.535265	38.694784
2426.409239	303174.011288	38.699802
2429.057215	303653.341386	38.704820
2431.174234	304152.998613	38.709837
2433.937194	304626.109464	38.714855
2436.266987	305119.226987	38.719872
2438.467440	305604.362056	38.724890
2441.217110	306091.008613	38.729908
2443.372568	306590.803436	38.734925
2445.871143	307081.194664	38.739943
2448.231987	307579.429173	38.744960
2451.225698	308082.920905	38.749978
2454.091955	308569.971578	38.754996
2456.260121	309077.095374	38.760013
2459.097961	309561.835257	38.765031
2461.649923	310053.603447	38.770048
2464.125633	310547.413673	38.775066
2467.003790	311030.642632	38.780084
2469.159987	311524.448569	38.785101
2471.458974	312011.041733	38.790119
2474.304561	312507.070905	38.795136
2476.830331	312996.595574	38.800154
2479.446242	313485.062423	38.805172
2481.594665	313979.773087	38.810189
2484.536096	314458.913347	38.815207
2486.717521	314949.956852	38.820224
2489.153803	315446.900927	38.825242
2491.678105	315926.659326	38.830260
2494.272119	316426.342094	38.835277
2496.770070	316911.865421	38.840295
2499.600838	317396.952673	38.845312
2501.882936	317877.603639	38.850330
2504.291447	318339.082253	38.855348
2506.659332	318807.879623	38.860365
2509.549875	319241.467037	38.865383
2511.900849	319702.338616	38.870400
2513.885050	320160.878682	38.875418
2516.264565	320605.486964	38.880436
2518.603069	321082.963386	38.885453
2520.762837	321541.011554	38.890471
2523.286231	322022.567993	38.895488
2525.741495	322503.167533	38.900506
2528.136996	322980.116807	38.905524
2529.977603	323475.589143	38.910541
2532.724474	323967.257973	38.915559
2535.527810	324466.508438	38.920576
2537.693264	324968.879117	38.925594
2540.538589	325472.129480	38.930612
2543.077415	325976.542735	38.935629
2545.271905	326492.587749	38.940647
2547.861698	327009.861993	38.945664
2550.134323	327524.440462	38.950682
2552.897821	328053.463727	38.955700
2555.177967	328576.160508	38.960717
2557.822955	329097.577020	38.965735
2561.149007	329635.743994	38.970752
2563.208604	330162.477225	38.975770
2566.386058	330689.943858	38.980788
2568.829871	331231.134108	38.985805
2571.466164	331755.580835	38.990823
2574.171349	332285.040802	38.995840
2577.000612	332817.727585	39.000858
2579.551159	333339.332366	39.005876
2582.050122	333877.345340	39.010893
2584.862017	334407.280515	39.015911
2587.569885	334936.898039	39.020928
2589.840556	335475.011032	39.025946
2592.982392	335997.568741	39.030964
2595.461735	336523.274414	39.035981
2598.189583	337066.101455	39.040999
2600.920024	337608.847494	39.046016
2603.328729	338136.887663	39.051034
2606.117805	338659.074140	39.056052
2608.810275	339204.656791	39.061069
2611.494170	339738.962696	39.066087
2614.304134	340259.787186	39.071104
2616.846830	340804.542017	39.076122
2619.686318	341327.688925	39.081140
2622.203843	341865.151556	39.086157
2624.818833	342398.734849	39.091175
2627.704428	342926.050225	39.096192
2630.497141	343452.360175	39.101210
2633.006544	343974.368895	39.106228
2635.729719	344514.999953	39.111245
2637.903733	345027.938015	39.116263
2640.724874	345555.291236	39.121280
2643.145377	346086.105170	39.126298
2645.709415	346597.622135	39.131316
2648.466506	347095.445436	39.136333
2650.912330	347591.892016	39.141351
2653.515727	348083.409575	39.146368
2656.130060	348595.941543	39.151386
2659.057760	349088.135186	39.156404
2661.446552	349595.083245	39.161421
2663.902595	350100.213581	39.166439
2666.747475	350611.928834	39.171456
2669.245720	351125.166567	39.176474
2671.843178	351636.302110	39.181492
2674.324132	352155.904565	39.186509
2676.986337	352682.251078	39.191527
2679.701169	353203.964002	39.196544
2682.053011	353748.169208	39.201562
2684.876899	354261.731300	39.206580
2687.533742	354807.197144	39.211597
2689.424589	355355.596142	39.216615
2692.616878	355897.640359	39.221632
2694.977435	356457.807240	39.226650
2697.728161	357005.798465	39.231668
2700.614287	357563.179242	39.236685
2703.307993	358117.741441	39.241703
2706.246875	358690.432186	39.246720
2708.919143	359258.919733	39.251738
2711.743733	359813.670538	39.256756
2714.190503	360385.124912	39.261773
2716.960632	360957.561927	39.266791
2719.874996	361517.278961	39.271808
2722.551417	362103.092661	39.276826
2725.613509	362671.808060	39.281844
2728.415250	363251.166504	39.286861
2730.645457	363821.116381	39.291879
2734.132349	364399.387605	39.296896
2736.743164	364978.170977	39.301914
2739.820753	365547.736885	39.306932
2742.490315	366117.131865	39.311949
2745.075789	366701.455106	39.316967
2748.354091	367264.318609	39.321984
2750.944648	367853.650726	39.327002
2753.655513	368419.025660	39.332020
2756.777892	368985.825383	39.337037
2759.807266	369561.691766	39.342055
2762.784707	370128.169709	39.347072
2765.185750	370704.272665	39.352090
2767.918140	371277.574920	39.357108
2770.579678	371849.485086	39.362125
2773.228761	372423.470222	39.367143
2776.318006	373009.988770	39.372160
2778.953866	373573.556940	39.377178
2781.708905	374152.449516	39.382196
2784.796960	374727.348462	39.387213
2787.522528	375310.441405	39.392231
2790.565004	375882.058337	39.397248
2793.274064	376454.709542	39.402266
2796.114348	376980.039208	39.407284
2798.480169	377507.974272	39.412301
2801.046319	378044.040109	39.417319
2804.070794	378577.768188	39.422336
2806.439460	379119.787507	39.427354
2808.928869	379668.528656	39.432372
2811.717603	380216.225329	39.437389
2814.390387	380782.020900	39.442407
2817.335123	381348.856027	39.447424
2819.452373	381910.537205	39.452442
2822.404874	382470.809528	39.457460
2824.980798	383043.563419	39.462477
2827.436584	383636.976673	39.467495
2830.518362	384218.841035	39.472512
2833.215782	384822.445588	39.477530
2835.974504	385411.495922	39.482548
2839.009737	386013.531104	39.487565
2841.605867	386613.190929	39.492583
2844.663705	387222.507978	39.497600
2847.138102	387834.063211	39.502618
2850.116963	388452.478028	39.507636
2853.225150	389064.089726	39.512653
2855.696171	389691.060483	39.517671
2858.485870	390320.379252	39.522688
2861.279047	390942.026945	39.527706
2864.131827	391589.903699	39.532724
2866.935190	392229.508561	39.537741
2869.909534	392856.800018	39.542759
2872.954161	393499.792466	39.547776
2875.894244	394159.197355	39.552794
2879.000307	394795.739870	39.557812
2882.059719	395429.843467	39.562829
2884.514372	396077.572394	39.567847
2887.920707	396729.702716	39.572864
2891.139466	397370.667446	39.577882
2893.809730	398028.239481	39.582900
2896.803049	398664.777582	39.587917
2900.025566	399314.198731	39.592935
2903.220818	399963.738173	39.597952
2905.940181	400608.091583	39.602970
2909.019847	401262.060645	39.607988
2912.262582	401896.392081	39.613005
2914.958803	402551.714171	39.618023
2918.116586	403173.483909	39.623040
2921.438582	403827.134316	39.628058
2924.369646	404455.126275	39.633076
2927.142634	405106.048488	39.638093
2930.251160	405752.847979	39.643111
2933.143801	406371.757483	39.648128
2936.093102	407019.544602	39.653146
2939.355357	407659.891989	39.658164
2942.498430	408289.294245	39.663181
2945.242148	408933.246035	39.668199
2948.073684	409558.869255	39.673216
2951.335771	410178.682975	39.678234
2953.811226	410778.407128	39.683252
2956.573339	411368.594472	39.688269
2959.445145	411963.695264	39.693287
2962.624121	412570.216981	39.698304
2965.230740	413173.927603	39.703322
2967.938543	413774.771343	39.708340
2970.937351	414369.575661	39.713357
2973.388172	414992.864342	39.718375
2976.183735	415597.610385	39.723392
2979.078913	416221.942870	39.728410
2981.909146	416855.192389	39.733428
2984.896929	417486.046344	39.738445
2987.700405	418131.232926	39.743463
2990.850386	418761.551623	39.748480
2993.851829	419415.293339	39.753498
2996.679873	420074.343172	39.758516
2999.953477	420716.989343	39.763533
3002.697141	421379.417220	39.768551
3005.351506	422039.385825	39.773568
3008.188392	422701.767488	39.778586
3011.183263	423391.850843	39.783604
3014.367131	424063.291075	39.788621
3017.027780	424753.013081	39.793639
3019.879821	425438.000609	39.798656
3022.998067	426141.548563	39.803674
3026.076091	426839.106098	39.808692
3029.480737	427542.065515	39.813709
3032.557650	428249.719247	39.818727
3035.648677	428942.381647	39.823744
3039.118107	429659.181340	39.828762
3041.871713	430352.493441	39.833780
3045.140881	431057.078127	39.838797
3048.041701	431779.558152	39.843815
3051.163361	432472.831766	39.848832
3054.597328	433203.950948	39.853850
3057.539316	433915.829118	39.858868
3060.481525	434625.610863	39.863885
3063.739666	435345.199345	39.868903
3066.627170	436055.355119	39.873920
3069.990639	436788.661975	39.878938
3073.207771	437498.066638	39.883956
3076.307931	438218.687094	39.888973
3079.418262	438945.969783	39.893991
3082.618910	439653.163582	39.899008
3086.024762	440366.229386	39.904026
3088.575559	441094.550231	39.909044
3092.313452	441810.205369	39.914061
3095.003729	442533.094006	39.919079
3098.034795	443261.476791	39.924096
3101.764921	443979.955332	39.929114
3104.793440	444695.536324	39.934132
3108.067097	445419.866425	39.939149
3111.055734	446142.194612	39.944167
3114.258267	446845.989028	39.949184
3117.320035	447560.618165	39.954202
3120.308863	448239.751409	39.959220
3123.661700	448914.403480	39.964237
3126.581895	449584.245139	39.969255
3129.512411	450263.025187	39.974272
3132.708284	450926.254964	39.979290
3135.566404	451608.955081	39.984308
3138.665828	452289.977185	39.989325
3141.709730	452974.328212	39.994343
3144.516780	453649.434614	39.999360
3147.784486	454345.602418	40.004378
3150.764342	455053.332724	40.009396
3154.109464	455739.121643	40.014413
3156.985190	456459.323763	40.019431
3159.810472	457160.079562	40.024448
3163.216801	457872.106541	40.029466
3166.324662	458609.862075	40.034484
3169.062637	459323.415558	40.039501
3172.411525	460068.926797	40.044519
3175.542448	460816.673324	40.049536
3178.853786	461545.950297	40.054554
3181.941396	462290.567078	40.059572
3184.954447	463045.996025	40.064589
3188.084068	463795.613244	40.069607
3191.131593	464552.400391	40.074624
3194.608166	465314.404179	40.079642
3197.887068	466073.579471	40.084660
3201.060161	466833.806553	40.089677
3203.929245	467611.706014	40.094695
3207.535833	468390.067038	40.099712
3210.538545	469155.294928	40.104730
3213.894795	469924.130659	40.109748
3217.658915	470707.184850	40.114765
3220.369591	471484.712439	40.119783
3223.400905	472280.566191	40.124800
3227.483301	473063.935786	40.129818
3230.208093	473843.040634	40.134836
3233.893797	474634.603889	40.139853
3236.617564	475420.524769	40.144871
3240.355066	476207.367058	40.149888
3243.949582	477005.121024	40.154906
3246.773263	477802.004695	40.159924
3250.490267	478589.009637	40.164941
3253.345978	479383.449219	40.169959
3256.738366	480181.057637	40.174976
3260.118234	480977.068957	40.179994
3263.072690	481768.566534	40.185012
3266.658411	482568.170404	40.190029
3269.610184	483371.531064	40.195047
3272.746398	484179.377627	40.200064
3276.740170	484959.614884	40.205082
3279.680944	485773.136102	40.210100
3283.247494	486560.501048	40.215117
3286.486166	487367.540769	40.220135
3289.679613	488163.488370	40.225152
3292.868912	488950.157466	40.230170
3296.209793	489724.594216	40.235188
3299.604374	490461.151581	40.240205
3302.757848	491229.039035	40.245223
3305.570605	491985.077746	40.250240
3308.905162	492738.881744	40.255258
3311.864861	493515.596048	40.260276
3315.247855	494288.624693	40.265293
3318.483476	495053.310588	40.270311
3321.805031	495834.920737	40.275328
3324.857652	496617.095582	40.280346
3327.742745	497404.464950	40.285364
3331.571244	498204.275647	40.290381
3334.599028	499004.379610	40.295399
3337.732950	499813.419229	40.300416
3341.371939	500612.496738	40.305434
3344.292907	501427.202831	40.310452
3347.490989	502229.912999	40.315469
3350.457714	503069.780232	40.320487
3353.869610	503900.652399	40.325504
3357.359096	504741.670114	40.330522
3360.662296	505581.717982	40.335540
3364.185763	506426.233491	40.340557
3367.428165	507283.925892	40.345575
3370.264468	508141.236421	40.350592
3374.011712	508997.805360	40.355610
3377.207186	509872.990108	40.360628
3380.842953	510733.527515	40.365645
3384.410411	511617.294452	40.370663
3387.605243	512492.648148	40.375680
3391.574024	513359.458928	40.380698
3395.001411	514233.475085	40.385716
3398.964003	515113.818853	40.390733
3402.293999	515984.883829	40.395751
3405.720815	516862.143233	40.400768
3409.633015	517726.366727	40.405786
3413.168701	518597.414014	40.410804
3416.442755	519460.840941	40.415821
3419.975298	520338.857957	40.420839
3423.509943	521206.943263	40.425856
3427.341125	522075.389502	40.430874
3430.458048	522953.079825	40.435892
3434.160072	523798.157978	40.440909
3437.691075	524678.714826	40.445927
3440.872780	525563.060115	40.450944
3445.034735	526409.693337	40.455962
3448.491423	527284.523133	40.460980
3452.146304	528147.830760	40.465997
3455.632158	529024.072675	40.471015
3459.253778	529885.930038	40.476032
3463.135707	530724.565179	40.481050
3466.238064	531591.249843	40.486068
3469.963815	532456.830558	40.491085
3473.443721	533295.744459	40.496103
3476.743166	534187.500669	40.501120
3480.377819	534982.836693	40.506125
3483.555700	535787.893307	40.511130
3487.241924	536554.944382	40.516135
3490.250563	537218.824725	40.521140
3493.383772	537835.331903	40.526144
3496.033588	538391.082864	40.531149
3498.975757	538909.445582	40.536154
3501.498519	539311.046654	40.541159
3503.914509	539685.939201	40.546164
3505.839218	540041.558870	40.551168
3508.966490	540269.724114	40.556173
3510.409591	540490.526898	40.561178
3512.515618	540658.603558	40.566183
3514.424615	540748.742263	40.571188
3515.811791	540795.788130	40.576192
3517.138979	540821.483203	40.581197
3517.973773	540791.002617	40.586202
3518.949630	540764.387945	40.591207
3520.516956	540662.792417	40.596212
3520.786627	540586.044123	40.601216
3521.351542	540423.351731	40.606221
3522.203864	540231.373421	40.611226
3523.017605	540103.532876	40.616231
3523.513313	539895.598432	40.621236
3523.133479	539660.731182	40.626240
3524.176792	539400.132148	40.631245
3524.202036	539194.838047	40.636250
3524.679779	538886.089922	40.641255
3524.891419	538628.588817	40.646260
3524.609571	538380.858299	40.651264
3524.994046	538058.269819	40.656269
3525.744704	537730.212415	40.661274
3525.113578	537455.399797	40.666279
3525.076838	537156.698625	40.671284
3524.937447	536823.054960	40.676288
3525.118685	536494.303470	40.681293
3524.749378	536215.739973	40.686298
3524.502350	535852.189117	40.691303
3525.224011	535518.229560	40.696308
3524.556926	535212.770858	40.701312
3524.136010	534900.144415	40.706317
3524.030361	534545.027206	40.711322
3523.872672	534262.454687	40.716327
3523.475602	533910.551669	40.721332
3523.234833	533601.861634	40.726336
3523.289153	533264.220487	40.731341
3522.553706	532982.271754	40.736346
3522.071522	532649.602773	40.741351
3522.593945	532328.641244	40.746356
3522.191124	532061.780723	40.751360
3521.754213	531733.682929	40.756365
3521.693474	531456.854828	40.761370
3520.732852	531139.589726	40.766375
3520.858431	530818.862134	40.771380
3520.736232	530586.595405	40.776384
3520.429657	530284.924612	40.781389
3519.899731	529991.823287	40.786394
3520.197964	529708.439596	40.791399
3520.074634	529456.448499	40.796404
3519.350799	529164.524760	40.801408
3519.474236	528864.072800	40.806413
3518.800397	528637.676234	40.811418
3518.212199	528368.558891	40.816423
3518.523821	528083.173082	40.821428
3518.031669	527864.671297	40.826432
3518.110737	527603.066933	40.831437
3517.760988	527344.760649	40.836442
3517.709802	527138.612209	40.841447
3516.828654	526872.548372	40.846452
3516.659171	526622.389738	40.851456
3516.563042	526397.942318	40.856461
3516.193792	526200.727733	40.861466
3516.168985	525933.805341	40.866471
3515.943115	525753.950098	40.871476
3515.406561	525535.271873	40.876480
3515.360636	525318.636106	40.881485
3514.941984	525106.100146	40.886490
3514.733963	524896.055509	40.891495
3514.973012	524685.937481	40.896500
3514.742867	524514.460198	40.901504
3514.388085	524349.572299	40.906509
3513.776937	524136.093533	40.911514
3513.976865	523936.688692	40.916519
3513.584207	523775.592275	40.921524
3513.616548	523566.503411	40.926528
3513.453990	523401.727134	40.931533
3513.051335	523237.492665	40.936538
3513.243241	523041.414616	40.941543
3513.090015	522861.869580	40.946548
3512.806839	522752.463049	40.951552
3512.258793	522559.428324	40.956557
3512.381210	522372.149867	40.961562
3512.244778	522237.792465	40.966567
3511.925386	522098.761068	40.971572
3511.724812	521934.835414	40.976576
3511.649992	521797.936775	40.981581
3511.329647	521642.065826	40.986586
3511.104252	521525.209834	40.991591
3510.845033	521345.462620	40.996596
3511.077166	521237.885747	41.001600
3510.619342	521086.632166	41.006605
3510.636880	520987.632231	41.011610
3510.802648	520846.288847	41.016615
3510.500581	520699.304752	41.021620
3510.539694	520569.506987	41.026624
3510.225209	520478.545212	41.031629
3510.223020	520323.673242	41.036634
3509.934494	520243.829815	41.041639
3509.835801	520080.678512	41.046644
3509.647283	519951.468040	41.051648
3509.687692	519892.858211	41.056653
3509.291507	519750.380686	41.061658
3509.275709	519657.749109	41.066663
3509.202381	519536.253551	41.071668
3508.683482	519478.185727	41.076672
3508.890937	519343.042349	41.081677
3509.279534	519256.311337	41.086682
3508.569763	519134.306617	41.091687
3508.765857	519069.348485	41.096692
3508.409957	518959.169635	41.101696
3508.592144	518864.833618	41.106701
3508.125179	518785.466432	41.111706
3508.464724	518678.462670	41.116711
3508.548494	518586.315025	41.121716
3507.926710	518526.490240	41.126720
3507.986793	518410.325531	41.131725
3508.061957	518348.872903	41.136730
3507.896074	518244.019528	41.141735
3507.874584	518196.589187	41.146740
3507.453725	518097.186066	41.151744
3508.107590	518003.276292	41.156749
3507.836363	517922.458086	41.161754
3507.742359	517837.970429	41.166759
3507.320036	517781.145635	41.171764
3507.081574	517733.293129	41.176768
3507.624852	517619.018763	41.181773
3507.327846	517533.752510	41.186778
3507.271729	517515.454594	41.191783
3506.926342	517419.626038	41.196788
3506.951133	517355.042269	41.201792
3506.658558	517300.268760	41.206797
3506.739395	517212.564271	41.211802
3506.772737	517193.038133	41.216807
3506.991721	517090.240680	41.221812
3506.703121	517068.540093	41.226816
3506.565108	516969.388961	41.231821
3506.398441	516931.940788	41.236826
3506.395299	516865.538913	41.241831
3506.633486	516789.135694	41.246836
3506.308464	516784.787128	41.251840
3506.506018	516714.458787	41.256845
3506.250239	516660.688830	41.261850
3505.891301	516608.098202	41.266855
3506.201963	516530.974314	41.271860
3505.953552	516522.163051	41.276864
3506.061409	516437.029495	41.281869
3506.179014	516416.578793	41.286874
3505.881856	516357.402934	41.291879
3506.015318	516292.747303	41.296884
3505.734708	516264.621405	41.301888
3506.222660	516210.833605	41.306893
3506.555023	516169.562298	41.311898
3505.969566	516113.364500	41.316903
3506.136030	516076.266361	41.321908
3505.826928	516021.946447	41.326912
3505.667958	515982.927086	41.331917
3505.777038	515923.685487	41.336922
3505.667562	515896.695168	41.341927
3505.690020	515826.188463	41.346932
3505.246792	515823.122732	41.351936
3505.557571	515765.365983	41.356941
3505.477687	515725.069111	41.361946
3505.593802	515699.307233	41.366951
3506.109836	515628.822843	41.371956
3505.401826	515613.913365	41.376960
3505.493272	515566.255388	41.381965
3505.731538	515513.061161	41.386970
3505.431775	515489.994702	41.391975
3505.564082	515439.699891	41.396980
3505.647458	515408.682693	41.401984
3505.555731	515371.826113	41.406989
3505.480297	515338.659049	41.411994
3505.444061	515292.133182	41.416999
3505.415151	515255.316996	41.422004
3505.280348	515211.841162	41.427008
3505.013008	515176.225781	41.432013
3505.226482	515162.485295	41.437018
3505.288007	515107.193431	41.442023
3505.311162	515067.789108	41.447028
3505.220752	515049.746805	41.452032
3505.438011	515003.787019	41.457037
3505.173017	514969.030666	41.462042
3504.846801	514946.321692	41.467047
3505.095728	514908.499837	41.472052
3505.021379	514874.320105	41.477056
3505.031303	514832.894159	41.482061
3504.887410	514828.415294	41.487066
3504.909860	514783.143225	41.492071
3505.175265	514748.100269	41.497076
3504.728455	514720.200364	41.502080
3505.069515	514702.949349	41.507085
3505.010942	514672.610763	41.512090
3504.747161	514630.974680	41.517095
3505.008958	514631.034408	41.522100
3504.857426	514596.512251	41.527104
3504.837716	514554.584505	41.532109
3504.790189	514539.670841	41.537114
3504.908646	514507.837156	41.542119
3505.000563	514477.120372	41.547124
3504.471804	514442.859842	41.552128
3504.990844	514431.498324	41.557133
3504.819546	514409.269945	41.562138
3504.753765	514369.675722	41.567143
3504.579883	514349.470896	41.572148
3504.734671	514325.015899	41.577152
3504.422004	514296.284797	41.582157
3504.308027	514274.856474	41.587162
3504.276447	514261.002241	41.592167
3504.445854	514235.836672	41.597172
3504.176924	514235.423890	41.602176
3504.227873	514201.829963	41.607181
3504.417221	514188.699470	41.612186
3504.378474	514160.481237	41.617191
3504.770792	514153.843615	41.622196
3504.275512	514130.654447	41.627200
3504.242922	514104.458400	41.632205
3504.024760	514100.901545	41.637210
3504.173480	514080.594828	41.642215
3504.106988	514057.843605	41.647220
3504.225522	514057.420163	41.652224
3504.003885	514041.471363	41.657229
3504.137462	514027.085020	41.662234
3504.014068	514002.268869	41.667239
3504.133681	514022.280250	41.672244
3504.004254	514001.562164	41.677248
3504.383445	513988.957911	41.682253
3504.190638	513957.071219	41.687258
3504.413815	513953.849234	41.692263
3504.743466	513919.199060	41.697268
3504.313248	513906.520343	41.702272
3504.149820	513878.675418	41.707277
3504.111588	513861.028253	41.712282
3504.467617	513869.014483	41.717287
3504.331452	513845.262344	41.722292
3504.060954	513818.850544	41.727296
3504.273965	513811.482394	41.732301
3504.459133	513789.550934	41.737306
3504.273117	513758.725024	41.742311
3504.042088	513763.313900	41.747316
3503.944155	513735.863048	41.752320
3503.920703	513702.128138	41.757325
3504.127824	513701.791851	41.762330
3504.133510	513703.358957	41.767335
3504.188189	513670.420958	41.772340
3504.281754	513667.472317	41.777344
3504.361859	513650.868466	41.782349
3504.164671	513630.666463	41.787354
3504.308025	513622.904578	41.792359
3504.545964	513585.334410	41.797364
3504.191983	513590.195679	41.802368
3504.246955	513560.595893	41.807373
3504.480308	513545.738124	41.812378
3504.155613	513522.622325	41.817383
3504.593303	513512.183547	41.822388
3504.084299	513512.314522	41.827392
3504.349903	513486.424470	41.832397
3504.464092	513458.534976	41.837402
3504.145057	513445.130173	41.842407
3504.297764	513430.133299	41.847412
3503.921039	513417.749259	41.852416
3504.183459	513385.334290	41.857421
3504.311622	513381.671963	41.862426
3504.307379	513368.015011	41.867431
3504.339982	513353.391137	41.872436
3504.095748	513350.242912	41.877440
3504.258019	513321.384504	41.882445
3504.196230	513312.946727	41.887450
3503.942890	513309.091761	41.892455
3504.478893	513269.501018	41.897460
3504.075920	513262.836992	41.902464
3504.201364	513253.206164	41.907469
3504.182979	513234.492946	41.912474
3504.197785	513219.720016	41.917479
3504.385436	513205.375013	41.922484
3504.270260	513203.420381	41.927488
3504.280304	513161.180971	41.932493
3504.055980	513140.476829	41.937498
3503.730929	513149.430977	41.942503
3504.138967	513129.689146	41.947508
3503.860922	513115.974098	41.952512
3504.095443	513099.345301	41.957517
3504.175719	513098.877298	41.962522
3503.854829	513080.717564	41.967527
3504.176438	513073.382515	41.972532
3504.086798	513063.633820	41.977536
3504.291621	513045.340376	41.982541
3503.995962	513031.830381	41.987546
3503.779940	513023.770929	41.992551
3504.200219	513001.244860	41.997556
3503.843848	512993.966346	42.002560
3504.160906	512980.915903	42.007565
3504.261731	512959.401379	42.012570
3504.086945	512952.549411	42.017575
3504.254567	512938.915536	42.022580
3503.902036	512916.359742	42.027584
3504.179015	512897.194790	42.032589
3503.934815	512893.995889	42.037594
3503.680411	512871.576281	42.042599
3503.956700	512856.609954	42.047604
3503.787737	512879.399892	42.052608
3504.183691	512857.788009	42.057613
3504.158669	512827.693735	42.062618
3503.820602	512825.470776	42.067623
3504.033676	512828.725082	42.072628
3503.849655	512810.644597	42.077632
3504.072639	512793.207961	42.082637
3504.077346	512793.105990	42.087642
3504.222709	512770.319554	42.092647
3504.607780	512746.281151	42.097652
3504.221824	512739.057789	42.102656
3503.705510	512723.154319	42.107661
3504.160294	512713.926403	42.112666
3504.250313	512693.020276	42.117671
3504.307134	512690.886643	42.122676
3503.765046	512693.855644	42.127680
3504.055801	512661.384229	42.132685
3504.105526	512634.060012	42.137690
3503.848081	512654.082018	42.142695
3504.231147	512624.884016	42.147700
3504.309218	512610.100557	42.152704
3503.850828	512601.016907	42.157709
3503.968241	512585.266077	42.162714
3504.063947	512568.355185	42.167719
3504.212523	512572.226767	42.172724
3503.853379	512543.297688	42.177728
3504.090524	512520.799928	42.182733
3504.473687	512511.633810	42.187738
3503.624156	512502.460167	42.192743
3504.277232	512489.153896	42.197748
3504.000906	512482.924821	42.202752
3504.128620	512460.393690	42.207757
3503.957590	512448.482294	42.212762
3504.081185	512447.956840	42.217767
3504.289168	512431.179826	42.222772
3503.584174	512399.118220	42.227776
3504.030366	512407.950863	42.232781
3503.982238	512395.210621	42.237786
3503.699205	512378.966439	42.242791
3504.039081	512350.887697	42.247796
3504.148946	512347.835079	42.252800
3504.079508	512334.592294	42.257805
3503.823946	512326.538759	42.262810
3504.322203	512324.588246	42.267815
3504.448889	512299.831251	42.272820
3504.062943	512297.008746	42.277824
3504.315160	512280.679874	42.282829
3504.607999	512256.402424	42.287834
3504.015453	512248.806807	42.292839
3504.017191	512224.828254	42.297844
3503.982092	512206.217719	42.302848
3504.021311	512188.505985	42.307853
3503.908648	512187.157883	42.312858
3503.852545	512165.060111	42.317863
3504.148199	512157.324074	42.322868
3504.047319	512158.301119	42.327872
3504.017471	512136.148572	42.332877
3504.164407	512117.913868	42.337882
3503.884472	512110.218194	42.342887
3504.101942	512103.657998	42.347892
3503.755471	512091.470556	42.352896
3504.296210	512082.532239	42.357901
3504.093272	512066.629211	42.362906
3504.237556	512059.979391	42.367911
3504.301125	512036.901376	42.372916
3503.826841	512026.049364	42.377920
3503.867735	512011.473612	42.382925
3504.182427	512017.140221	42.387930
3504.105091	511989.379762	42.392935
3504.098763	511970.056194	42.397940
3503.822475	511970.706858	42.402944
3503.816917	511948.954931	42.407949
3503.576720	511942.214068	42.412954
3503.879357	511939.029734	42.417959
3504.309315	511931.474720	42.422964
3504.035335	511926.105063	42.427968
3504.109232	511899.989957	42.432973
3504.358464	511886.291754	42.437978
3504.023983	511854.676440	42.442983
3504.136366	511840.241007	42.447988
3503.928620	511841.083196	42.452992
3504.086234	511810.452376	42.457997
3504.120512	511808.423373	42.463002
3503.749831	511807.065432	42.468007
3503.775785	511787.382436	42.473012
3503.418486	511778.990603	42.478016
3503.650577	511770.455024	42.483021
3504.044760	511769.178547	42.488026
3503.804238	511767.344736	42.493031
3503.899751	511746.942463	42.498036
3503.953529	511742.482126	42.503040
3504.095647	511718.935971	42.508045
3503.536261	511705.871309	42.513050
3503.897185	511702.020068	42.518055
3504.304817	511685.413121	42.523060
3503.837858	511692.468093	42.528064
3503.771760	511674.165408	42.533069
3503.983803	511658.803475	42.538074
3503.987405	511643.980359	42.543079
3503.800954	511652.913385	42.548084
3503.639318	511639.381099	42.553088
3503.925104	511620.112143	42.558093
3503.704556	511611.344491	42.563098
3503.562221	511621.535281	42.568103
3503.848340	511611.220476	42.573108
3503.965919	511587.020363	42.578112
3503.811718	511576.724540	42.583117
3503.913015	511579.086154	42.588122
3503.828178	511565.845205	42.593127
3503.909945	511542.308344	42.598132
3503.917318	511540.688274	42.603136
3504.321505	511531.821842	42.608141
3504.119706	511512.933362	42.613146
3503.544613	511495.925070	42.618151
3503.964286	511502.688221	42.623156
3503.938993	511493.181401	42.628160
3504.003922	511490.742802	42.633165
3504.090094	511479.447736	42.638170
3503.803329	511474.535260	42.643175
3504.080262	511444.087282	42.648180
3503.720308	511440.349917	42.653184
3504.115921	511431.231842	42.658189
3503.846135	511418.880029	42.663194
3503.667146	511399.481924	42.668199
3504.087898	511390.106907	42.673204
3503.690787	511394.115593	42.678208
3503.757853	511388.438916	42.683213
3503.714944	511362.746165	42.688218
3503.840153	511353.468428	42.693223
3503.988708	511341.606926	42.698228
3503.686717	511350.305423	42.703232
3503.689529	511339.832873	42.708237
3504.004667	511319.597736	42.713242
3503.299882	511321.277351	42.718247
3503.544955	511305.049856	42.723252
3503.630439	511314.344797	42.728256
3503.343712	511316.312466	42.733261
3503.499666	511309.002844	42.738266
3503.441615	511287.966627	42.743271
3503.677291	511275.888951	42.748276
3503.584385	511286.223898	42.753280
3503.640519	511277.564114	42.758285
3504.025593	511268.649979	42.763290
3503.887801	511270.695294	42.768295
3503.689067	511242.750448	42.773300
3503.711449	511236.676064	42.778304
3503.585973	511241.501882	42.783309
3503.601473	511238.919290	42.788314
3503.658791	511237.291297	42.793319
3503.927804	511213.167900	42.798324
3503.750246	511203.583805	42.803329
3503.804210	511188.752334	42.808333
3503.936004	511201.024832	42.813338
3503.731251	511195.441642	42.818343
3503.869100	511166.381083	42.823348
3503.752457	511157.192055	42.828353
3503.735957	511172.826961	42.833357
3503.883191	511173.056585	42.838362
3503.684952	511138.686545	42.843367
3503.879062	511115.181931	42.848372
3504.060184	511119.554603	42.853377
3503.908853	511115.632423	42.858381
3504.103569	511088.687537	42.863386
3503.716407	511078.883546	42.868391
3503.742190	511087.833914	42.873396
3504.082630	511087.274148	42.878401
3503.842645	511057.514265	42.883405
3503.756206	511054.897166	42.888410
3503.855698	511043.599707	42.893415
3503.694921	511033.810502	42.898420
3503.700544	511024.753849	42.903425
3504.010268	511015.244405	42.908429
3503.889052	511011.722165	42.913434
3504.185538	511003.985478	42.918439
3504.206568	510973.475927	42.923444
3503.747336	510971.980140	42.928449
3504.071001	510967.831081	42.933453
3504.423573	510943.845870	42.938458
3504.038302	510937.481674	42.943463
3504.203561	510914.183707	42.948468
3503.983193	510898.838844	42.953473
3503.725283	510892.454501	42.958477
3503.722231	510892.758473	42.963482
3503.583385	510880.638530	42.968487
3503.617046	510853.061045	42.973492
3503.489682	510861.378052	42.978497
3503.754444	510848.738976	42.983501
3503.720711	510874.090363	42.988506
3503.788666	510847.519270	42.993511
3503.847484	510819.027114	42.998516
3503.752887	510825.618860	43.003521
3503.490240	510823.889625	43.008525
3503.795523	510821.109397	43.013530
3503.744213	510818.233754	43.018535
3503.877053	510788.566252	43.023540
3503.405602	510804.323991	43.028545
3503.825051	510779.265565	43.033549
3503.808197	510779.672903	43.038554
3503.625508	510789.212879	43.043559
3503.916047	510730.582131	43.048564
3503.384729	510772.100378	43.053569
3503.473937	510749.269529	43.058573
3503.607688	510739.028874	43.063578
3503.447619	510759.695396	43.068583
3503.639641	510739.984948	43.073588
3503.283339	510725.673242	43.078593
3503.914420	510719.198921	43.083597
3503.862435	510721.129557	43.088602
3503.689642	510727.025418	43.093607
3503.784439	510715.273162	43.098612
3503.931002	510700.123085	43.103617
3503.871936	510670.536301	43.108621
3503.846723	510680.456181	43.113626
3503.605742	510675.536237	43.118631
3503.840381	510666.291425	43.123636
3503.699826	510651.085500	43.128641
3503.547554	510642.913659	43.133645
3503.713235	510651.133860	43.138650
3503.434790	510640.553560	43.143655
3503.870217	510617.769000	43.148660
3503.742545	510630.335874	43.153665
3503.495350	510610.239369	43.158669
3503.801093	510592.888592	43.163674
3503.374595	510599.178739	43.168679
3503.805952	510597.693936	43.173684
3503.866503	510577.295794	43.178689
3503.851979	510595.612285	43.183693
3503.769387	510549.333699	43.188698
3503.721543	510562.646886	43.193703
3504.102891	510551.810475	43.198708
3503.762190	510535.927793	43.203713
3503.834895	510532.425398	43.208717
3503.871662	510517.798433	43.213722
3503.654538	510504.476386	43.218727
3503.775135	510521.102060	43.223732
3503.820866	510493.522090	43.228737
3503.993835	510469.261050	43.233741
3504.057152	510482.506138	43.238746
3503.844671	510470.346949	43.243751
3503.862813	510435.384784	43.248756
3503.353893	510439.816099	43.253761
3503.590498	510446.507420	43.258765
3503.833236	510424.360166	43.263770
3503.931456	510416.249811	43.268775
3503.835221	510417.125035	43.273780
3503.632038	510383.310775	43.278785
3503.355275	510407.385859	43.283789
3503.809984	510383.130761	43.288794
3503.339651	510397.826254	43.293799
3503.762606	510367.454470	43.298804
3503.757307	510350.354978	43.303809
3503.782669	510361.835419	43.308813
3503.976302	510361.754167	43.313818
3503.919022	510346.484217	43.318823
3504.106657	510331.529694	43.323828
3503.632513	510336.866206	43.328833
3504.062619	510336.646394	43.333837
3504.008817	510279.535713	43.338842
3503.739486	510308.112516	43.343847
3504.042092	510286.056807	43.348852
3504.060566	510269.509998	43.353857
3503.921779	510278.739762	43.358861
3503.816557	510252.245709	43.363866
3503.819793	510263.830898	43.368871
3503.877067	510250.920620	43.373876
3503.771492	510235.051090	43.378881
3503.897343	510221.016907	43.383885
3503.633209	510213.975586	43.388890
3503.421990	510229.540942	43.393895
3503.991338	510197.425562	43.398900
3504.127948	510180.961182	43.403905
3503.862236	510171.896371	43.408909
3503.945426	510187.819978	43.413914
3504.084808	510141.302837	43.418919
3504.146018	510124.951507	43.423924
3504.131282	510140.435296	43.428929
3504.017672	510104.582603	43.433933
3504.068875	510088.890533	43.438938
3503.810047	510092.725883	43.443943
3503.806870	510079.976810	43.448948
3503.935970	510047.778953	43.453953
3503.475293	510079.371390	43.458957
3503.758951	510032.426406	43.463962
3503.384545	510082.117662	43.468967
3503.818030	510030.747371	43.473972
3503.630952	510036.848100	43.478977
3503.719929	510013.105627	43.483981
3503.888249	510007.867832	43.488986
3503.224044	510032.561205	43.493991
3503.683560	510018.676495	43.498996
3503.989355	509974.763466	43.504001
3503.609537	509990.406279	43.509005
3504.035530	509964.890290	43.514010
3503.784707	509987.494645	43.519015
3504.217937	509947.861863	43.524020
3503.713014	509925.427383	43.529025
3503.847469	509946.908428	43.534029
3504.099529	509925.770933	43.539034
3503.359870	509926.697281	43.544039
3503.784663	509884.080651	43.549044
3503.609677	509896.453164	43.554049
3503.714080	509884.648227	43.559053
3503.746158	509867.036408	43.564058
3503.735677	509877.966303	43.569063
3503.691674	509841.950279	43.574068
3503.783618	509850.283707	43.579073
3503.781896	509842.897194	43.584077
3503.853722	509855.230728	43.589082
3503.690360	509822.876297	43.594087
3503.797941	509811.930908	43.599092
3503.657879	509809.220906	43.604097
3503.648012	509821.112028	43.609101
3503.594218	509811.912345	43.614106
3503.288481	509796.023450	43.619111
3503.445974	509785.120750	43.624116
3503.467851	509782.334555	43.629121
3503.139257	509774.594921	43.634125
3503.730919	509772.983526	43.639130
3503.669283	509789.537523	43.644135
3503.403639	509780.371305	43.649140
3503.362438	509784.880646	43.654145
3503.687925	509784.272611	43.659149
3503.873633	509741.339256	43.664154
3503.481651	509746.409991	43.669159
3503.594986	509729.898264	43.674164
3503.290590	509727.113033	43.679169
3503.470428	509731.536859	43.684173
3503.550233	509749.434587	43.689178
3503.263031	509739.512840	43.694183
3503.070403	509723.757785	43.699188
3503.018765	509744.711957	43.704193
3503.527290	509740.432198	43.709197
3503.635817	509739.403103	43.714202
3503.503203	509733.605655	43.719207
3503.612708	509701.460841	43.724212
3503.439284	509715.249882	43.729217
3503.427921	509683.377109	43.734221
3503.679868	509719.158110	43.739226
3503.358746	509695.682391	43.744231
3503.809240	509723.842830	43.749236
3503.345660	509708.130584	43.754241
3503.895488	509696.761065	43.759245
3504.044759	509676.246643	43.764250
3503.361604	509660.923220	43.769255
3503.511204	509684.678955	43.774260
3503.562383	509663.977644	43.779265
3503.327081	509676.309253	43.784269
3503.689510	509667.650842	43.789274
3503.643422	509634.164441	43.794279
3503.678704	509663.402495	43.799284
3503.723156	509626.410743	43.804289
3503.700890	509644.476497	43.809293
3504.095624	509615.878660	43.814298
3503.765848	509616.234294	43.819303
3503.797419	509593.714587	43.824308
3504.117864	509600.747152	43.829313
3503.726917	509578.395394	43.834317
3503.549879	509559.197277	43.839322
3504.329388	509547.892549	43.844327
3503.812193	509561.078311	43.849332
3504.050776	509535.135954	43.854337
3503.858190	509531.928259	43.859341
3503.922339	509519.319916	43.864346
3503.914501	509523.722862	43.869351
3504.130602	509501.578631	43.874356
3503.800701	509480.684354	43.879361
3503.876416	509487.755645	43.884365
3504.317548	509476.504350	43.889370
3503.922740	509436.039955	43.894375
3504.083372	509446.234747	43.899380
3504.027371	509433.442949	43.904385
3503.863516	509406.248527	43.909389
3504.132431	509398.667264	43.914394
3503.556126	509391.067798	43.919399
3503.895303	509370.978357	43.924404
3503.738647	509366.297685	43.929409
3503.438217	509353.089100	43.934413
3503.557512	509362.227970	43.939418
3503.560384	509363.644132	43.944423
3503.618893	509366.518769	43.949428
3503.589883	509351.294063	43.954433
3503.742374	509335.990063	43.959437
3503.387910	509310.697649	43.964442
3503.414944	509318.383851	43.969447
3503.146460	509331.176311	43.974452
3503.532582	509329.496171	43.979457
3503.550905	509322.005076	43.984461
3503.707808	509323.346302	43.989466
3503.660650	509309.136339	43.994471
3503.767021	509287.413940	43.999476
3503.485236	509291.354286	44.004481
3503.713039	509277.960966	44.009485
3503.686353	509274.979981	44.014490
3503.519162	509285.631446	44.019495
3503.530314	509283.959969	44.024500
3503.604092	509259.915286	44.029505
3503.662642	509258.944657	44.034509
3503.691273	509266.731821	44.039514
3503.588729	509267.709290	44.044519
3503.960405	509247.563974	44.049524
3503.485226	509238.076413	44.054529
3503.552003	509218.333422	44.059533
3504.020881	509201.613208	44.064538
3503.496806	509200.633467	44.069543
3503.741796	509201.556014	44.074548
3503.739055	509204.541550	44.079553
3503.492420	509172.249653	44.084557
3503.574720	509157.361356	44.089562
3503.424671	509171.045944	44.094567
3503.968409	509165.748560	44.099572
3503.624871	509171.823727	44.104577
3503.449851	509167.854247	44.109581
3503.568988	509139.400372	44.114586
3503.205676	509135.713625	44.119591
3503.064204	509122.530337	44.124596
3503.696868	509121.215980	44.129601
3503.375752	509121.064292	44.134605
3503.497313	509129.292196	44.139610
3503.047995	509109.630649	44.144615
3503.911573	509124.166996	44.149620
3503.645192	509117.378559	44.154625
3503.178083	509127.824542	44.159629
3503.991336	509116.463604	44.164634
3503.712340	509099.153146	44.169639
3503.530627	509111.628477	44.174644
3503.407457	509087.108718	44.179649
3503.664013	509090.053293	44.184653
3503.681101	509100.827535	44.189658
3503.772224	509070.050547	44.194663
3503.677758	509069.508862	44.199668
3503.585866	509063.805945	44.204673
3503.599582	509053.836241	44.209677
3503.875995	509050.655524	44.214682
3503.545578	509055.767326	44.219687
3503.636506	509047.353902	44.224692
3503.658329	509038.344239	44.229697
3503.403098	509025.381241	44.234701
3503.484670	509025.469486	44.239706
3503.491890	509034.170875	44.244711
3503.612746	509028.333128	44.249716
3503.955123	509031.770113	44.254721
3503.665040	509031.259344	44.259725
3503.793413	508996.378027	44.264730
3503.596989	508997.724525	44.269735
3503.486439	508989.393513	44.274740
3503.636598	508991.494779	44.279745
3503.232827	509006.231530	44.284749
3503.601169	508987.351350	44.289754
3503.359661	508980.710718	44.294759
3503.692106	508955.056234	44.299764
3503.681303	508951.971489	44.304769
3503.414450	508956.617904	44.309773
3503.802871	508953.976030	44.314778
3503.514695	508957.512688	44.319783
3503.535027	508952.652141	44.324788
3503.654390	508935.835121	44.329793
3503.276704	508943.838439	44.334797
3503.870072	508904.329742	44.339802
3503.526132	508936.867158	44.344807
3503.547520	508912.121917	44.349812
3503.726946	508914.016180	44.354817
3503.558743	508931.245601	44.359821
3503.699756	508902.433702	44.364826
3503.839095	508886.878398	44.369831
3503.860699	508870.633331	44.374836
3503.521594	508899.628271	44.379841
3503.445900	508869.383259	44.384845
3503.638129	508887.820679	44.389850
3503.738788	508850.160620	44.394855
3503.641347	508847.190744	44.399860
3503.808858	508846.961825	44.404865
3503.725541	508832.048826	44.409869
3503.601908	508831.562340	44.414874
3503.571928	508843.659704	44.419879
3503.541927	508800.302728	44.424884
3503.235103	508796.151605	44.429889
3503.503002	508812.806247	44.434893
3503.505169	508775.566369	44.439898
3503.572871	508818.107783	44.444903
3503.597708	508774.893867	44.449908
3503.581049	508819.776081	44.454913
3503.575292	508773.733563	44.459917
3503.494783	508787.356868	44.464922
3503.342422	508749.685982	44.469927
3503.844288	508769.997286	44.474932
3503.322814	508751.206886	44.479937
3503.345979	508770.430112	44.484941
3503.937783	508763.556497	44.489946
3503.429279	508761.056352	44.494951
3503.676888	508742.245584	44.499956
3503.980279	508734.759776	44.504961
3503.551350	508734.017955	44.509965
3503.877859	508721.772342	44.514970
3503.622097	508724.747354	44.519975
3503.521863	508703.309862	44.524980
3503.938478	508688.216530	44.529985
3503.612570	508686.497073	44.534989
3503.825482	508660.355071	44.539994
3503.535110	508696.223909	44.544999
3503.754987	508675.292360	44.550004
3503.932506	508648.548763	44.555009
3503.813070	508638.549267	44.560013
3503.677980	508630.829131	44.565018
3503.683239	508637.456528	44.570023
3503.532637	508619.821711	44.575028
3503.438820	508602.532085	44.580033
3503.595951	508606.049031	44.585037
3503.866778	508598.720105	44.590042
3503.375059	508594.749949	44.595047
3503.522175	508594.524251	44.600052
3503.619839	508597.342230	44.605057
3503.516006	508593.968539	44.610061
3503.444812	508570.148200	44.615066
3503.582306	508577.564284	44.620071
3503.687930	508563.278962	44.625076
3503.350826	508565.912672	44.630081
3503.235540	508570.434040	44.635085
3503.435416	508560.890009	44.640090
3503.440617	508572.020644	44.645095
3503.557799	508571.749079	44.650100
3503.750325	508558.208984	44.655105
3503.673830	508537.374708	44.660109
3503.646101	508539.757134	44.665114
3503.651702	508525.689981	44.670119
3503.805999	508522.781457	44.675124
3503.444624	508532.553313	44.680129
3503.207415	508508.050756	44.685133
3503.451550	508502.699328	44.690138
3503.798779	508485.542270	44.695143
3503.784145	508483.217018	44.700148
3503.570069	508487.349236	44.705153
3503.650366	508500.087185	44.710157
3503.799525	508486.047908	44.715162
3503.608519	508467.204968	44.720167
3503.797397	508454.778527	44.725172
3503.601384	508450.458013	44.730177
3503.517444	508456.037016	44.735181
3503.698702	508441.284257	44.740186
3503.642977	508457.079624	44.745191
3503.664671	508429.348355	44.750196
3503.752770	508420.176101	44.755201
3503.637319	508423.685568	44.760205
3503.739513	508417.749370	44.765210
3503.754713	508423.818697	44.770215
3503.683526	508396.203251	44.775220
3503.836790	508377.204605	44.780225
3503.178381	508385.556138	44.785229
3503.738247	508381.672721	44.790234
3503.771944	508386.828367	44.795239
3503.988554	508368.325683	44.800244
3503.713315	508337.757091	44.805249
3503.650198	508345.204981	44.810253
3504.139670	508336.374033	44.815258
3503.831389	508328.124552	44.820263
3503.681760	508314.688943	44.825268
3503.584987	508294.312966	44.830273
3503.691723	508297.888539	44.835277
3503.537519	508291.385638	44.840282
3503.669595	508302.597591	44.845287
3503.706314	508287.412158	44.850292
3503.223934	508259.203700	44.855297
3503.303789	508276.394567	44.860301
3503.833547	508251.922224	44.865306
3503.374596	508262.620430	44.870311
3503.525437	508256.119902	44.875316
3503.765403	508254.563959	44.880321
3503.491902	508262.348729	44.885325
3503.658291	508248.053543	44.890330
3503.734066	508224.766085	44.895335
3503.923134	508217.095729	44.900340
3503.824260	508231.430756	44.905345
3503.675176	508228.519534	44.910349
3503.624733	508192.804680	44.915354
3503.304414	508218.559461	44.920359
3503.635153	508180.355593	44.925364
3503.562865	508187.197814	44.930369
3503.571269	508186.538644	44.935373
3504.110523	508159.028736	44.940378
3503.439124	508177.603411	44.945383
3503.385122	508139.713255	44.950388
3503.572607	508148.943188	44.955393
3503.414593	508141.277055	44.960397
3503.869914	508134.374166	44.965402
3503.405352	508145.376925	44.970407
3503.768843	508137.628367	44.975412
3503.620782	508123.079183	44.980417
3503.337981	508103.339571	44.985421
3503.186914	508109.738882	44.990426
3503.449961	508104.738536	44.995431
3503.543419	508104.470714	45.000436
3503.258258	508107.855270	45.005441
3503.240895	508121.013726	45.010445
3503.620025	508110.378536	45.015450
3503.488496	508119.962499	45.020455
3503.417366	508113.699396	45.025460
3503.527406	508113.530151	45.030465
3503.346499	508107.132600	45.035469
3503.682142	508088.610804	45.040474
3503.604908	508079.616298	45.045479
3503.494878	508061.670904	45.050484
3503.449522	508062.386406	45.055489
3503.440623	508072.811201	45.060493
3503.874725	508070.313772	45.065498
3503.463301	508074.578477	45.070503
3503.600821	508061.147887	45.075508
3503.772246	508043.006192	45.080513
3503.815075	508044.416148	45.085517
3503.613667	508040.703575	45.090522
3503.457367	508041.790808	45.095527
3503.651018	508039.786771	45.100532
3503.609816	508011.508182	45.105537
3503.320220	507993.236902	45.110541
3503.635117	507975.882052	45.115546
3503.469763	508000.145279	45.120551
3503.646753	507988.074579	45.125556
3503.971615	507991.565141	45.130561
3503.666105	507972.183166	45.135565
3503.632862	507959.589078	45.140570
3503.473158	507948.178760	45.145575
3503.386130	507949.609247	45.150580
3503.657203	507960.192258	45.155585
3503.214623	507959.958554	45.160589
3503.772721	507949.294980	45.165594
3503.540175	507956.820415	45.170599
3503.181761	507952.019448	45.175604
3503.292485	507935.051024	45.180609
3503.116800	507930.828366	45.185613
3503.184665	507933.398165	45.190618
3503.292179	507947.144212	45.195623
3503.412876	507929.567011	45.200628
3503.525146	507921.605065	45.205633
3503.635821	507912.277175	45.210637
3503.665836	507910.400186	45.215642
3503.609528	507910.054832	45.220647
3503.682174	507919.252437	45.225652
3503.685429	507912.522109	45.230657
3503.571574	507892.806155	45.235661
3503.766446	507896.519681	45.240666
3503.503962	507873.740612	45.245671
3503.625532	507868.711960	45.250676
3503.574336	507867.556199	45.255681
3503.371563	507872.850573	45.260685
3503.282004	507874.332066	45.265690
3503.634229	507872.302948	45.270695
3503.464068	507845.208265	45.275700
3503.672623	507833.233669	45.280705
3503.385357	507839.806404	45.285709
3503.770357	507840.453898	45.290714
3503.445180	507840.151037	45.295719
3503.526340	507821.314978	45.300724
3503.580855	507830.869696	45.305729
3503.104638	507834.942300	45.310733
3503.572414	507802.231332	45.315738
3503.332182	507791.137237	45.320743
3503.257612	507814.677974	45.325748
3503.647541	507805.963691	45.330753
3503.041394	507805.755836	45.335757
3503.199847	507805.376537	45.340762
3503.326674	507810.669436	45.345767
3503.562934	507805.268439	45.350772
3503.336581	507805.304158	45.355777
3503.287047	507830.004717	45.360781
3503.497909	507813.273347	45.365786
3503.587516	507807.490730	45.370791
3503.218338	507815.847421	45.375796
3503.270839	507817.104066	45.380801
3503.766942	507820.921799	45.385805
3503.502883	507770.262241	45.390810
3503.373354	507795.734493	45.395815
3503.686191	507776.456969	45.400820
3503.641043	507764.876624	45.405825
3503.420467	507780.749262	45.410829
3503.661211	507772.969342	45.415834
3503.207225	507766.058223	45.420839
3503.487942	507765.811400	45.425844
3503.687692	507752.674336	45.430849
3503.262745	507759.774864	45.435853
3503.809224	507723.205697	45.440858
3503.466364	507732.671474	45.445863
3503.492382	507748.201566	45.450868
3503.684748	507739.316074	45.455873
3503.517822	507734.434180	45.460877
3503.617945	507731.635288	45.465882
3503.771453	507715.418891	45.470887
3503.816273	507703.723085	45.475892
3503.897132	507693.539585	45.480897
3503.472015	507718.552665	45.485901
3503.780035	507693.962783	45.490906
3503.149784	507676.048610	45.495911
3503.204622	507673.762869	45.500916
3503.608418	507674.306198	45.505921
3503.448346	507671.649621	45.510925
3503.797339	507654.339662	45.515930
3503.519176	507654.687173	45.520935
3503.643338	507676.628073	45.525940
3503.721492	507662.346351	45.530945
3503.600762	507634.130316	45.535949
3503.820904	507622.254944	45.540954
3503.755516	507641.341616	45.545959
3503.667081	507614.638460	45.550964
3503.167615	507622.408629	45.555969
3503.387533	507630.419299	45.560973
3503.630445	507620.614948	45.565978
3503.228184	507597.756407	45.570983
3503.090336	507579.713710	45.575988
3503.232690	507595.529156	45.580993
3503.271629	507594.004927	45.585997
3503.318586	507570.872949	45.591002
3503.583307	507601.798649	45.596007
3503.559196	507577.261095	45.601012
3503.490799	507593.970063	45.606017
3503.796219	507562.599921	45.611021
3503.729397	507607.189599	45.616026
3503.807007	507574.185663	45.621031
3503.576749	507562.482638	45.626036
3503.903622	507518.155237	45.631041
3503.400751	507554.414226	45.636045
3503.004274	507553.060012	45.641050
3503.526538	507544.982493	45.646055
3503.275107	507555.901337	45.651060
3503.809431	507536.487340	45.656065
3502.887391	507541.996695	45.661069
3503.231452	507525.851206	45.666074
3503.258207	507547.200456	45.671079
3503.185400	507555.459829	45.676084
3503.122271	507552.838512	45.681089
3503.061752	507551.937207	45.686093
3503.351470	507562.011508	45.691098
3503.638855	507533.376602	45.696103
3503.298690	507552.000793	45.701108
3503.699593	507501.437756	45.706113
3503.493307	507530.970599	45.711117
3503.270926	507509.854540	45.716122
3503.088498	507530.983866	45.721127
3503.629271	507500.537830	45.726132
3503.934816	507521.944249	45.731137
3503.561729	507536.221988	45.736141
3503.716250	507505.229798	45.741146
3503.358851	507508.980093	45.746151
3503.526089	507470.699304	45.751156
3503.434511	507482.807352	45.756161
3503.632992	507463.395753	45.761165
3503.437455	507495.558209	45.766170
3503.583924	507478.027080	45.771175
3503.595796	507491.029590	45.776180
3503.542016	507459.108822	45.781185
3503.071529	507453.870019	45.786189
3503.608784	507433.797630	45.791194
3503.946547	507420.891509	45.796199
3503.358727	507454.077464	45.801204
3503.780466	507440.044862	45.806209
3503.194505	507427.537746	45.811213
3503.271503	507425.096667	45.816218
3503.541603	507454.807352	45.821223
3503.576991	507430.918001	45.826228
3503.625099	507423.067169	45.831233
3503.207521	507408.914190	45.836237
3503.672319	507375.039064	45.841242
3503.398163	507410.300780	45.846247
3503.387186	507394.869099	45.851252
3503.594443	507390.535183	45.856257
3503.418591	507386.565424	45.861261
3503.274009	507405.209461	45.866266
3503.512461	507394.596069	45.871271
3503.579550	507377.532795	45.876276
3503.572421	507377.078455	45.881281
3503.524180	507372.076498	45.886285
3503.920006	507353.797415	45.891290
3503.498401	507362.769824	45.896295
3503.373915	507380.601091	45.901300
3503.595824	507359.111021	45.906305
3503.474855	507366.568475	45.911309
3503.610841	507354.200208	45.916314
3503.342611	507333.192383	45.921319
3503.662891	507329.751414	45.926324
3503.743272	507333.533758	45.931329
3503.389637	507336.625676	45.936333
3503.920501	507316.149352	45.941338
3503.645072	507306.679756	45.946343
3503.680706	507317.097965	45.951348
3503.823902	507271.736337	45.956353
3503.331997	507294.534113	45.961357
3503.572081	507259.378639	45.966362
3503.295420	507290.238655	45.971367
3503.716455	507270.336252	45.976372
3503.653014	507281.427962	45.981377
3503.671950	507267.964900	45.986381
3503.403558	507236.482455	45.991386
3503.829242	507263.132778	45.996391
3503.602380	507243.130338	46.001396
3503.456270	507227.517459	46.006401
3503.417023	507261.224299	46.011405
3503.821890	507234.290788	46.016410
3503.465535	507224.479725	46.021415
3503.237679	507234.990230	46.026420
3503.378786	507201.621341	46.031425
3503.450508	507230.503533	46.036429
3503.606026	507192.325188	46.041434
3503.613524	507235.284815	46.046439
3503.717026	507208.449497	46.051444
3503.522741	507198.359795	46.056449
3503.297262	507202.747128	46.061453
3503.477679	507167.196084	46.066458
3503.575217	507174.619085	46.071463
3503.728306	507167.864787	46.076468
3503.661562	507166.306622	46.081473
3503.474777	507168.815578	46.086477
3503.779633	507168.564932	46.091482
3503.651600	507154.568391	46.096487
3503.802998	507152.267321	46.101492
3504.001531	507123.949397	46.106497
3503.661400	507117.930858	46.111501
3503.591963	507122.344151	46.116506
3503.299525	507094.508593	46.121511
3503.351962	507086.403915	46.126516
3503.852907	507082.883742	46.131521
3503.200225	507092.651842	46.136525
3503.237627	507077.060427	46.141530
3503.586955	507082.571392	46.146535
3503.580350	507094.565077	46.151540
3503.273173	507101.040032	46.156545
3503.528373	507090.272002	46.161549
3503.628600	507069.661043	46.166554
3503.478119	507066.345029	46.171559
3503.579529	507060.965115	46.176564
3503.650019	507057.664776	46.181569
3503.582926	507056.005452	46.186573
3503.406171	507046.469516	46.191578
3503.364759	507048.145878	46.196583
3503.452310	507054.305454	46.201588
3503.295993	507056.050578	46.206593
3503.380819	507043.639575	46.211597
3503.526691	507040.883943	46.216602
3503.649965	507025.076500	46.221607
3503.327426	507013.843110	46.226612
3503.424880	506997.432495	46.231617
3503.309768	507006.103633	46.236621
3503.742081	507006.946092	46.241626
3503.557910	507008.645021	46.246631
3503.862503	507007.534175	46.251636
3503.538727	506989.975673	46.256641
3503.417482	506986.503215	46.261645
3503.856089	506962.043468	46.266650
3503.562501	506975.044039	46.271655
3503.822425	506974.142660	46.276660
3503.991138	506963.894246	46.281665
3503.650195	506955.952886	46.286669
3503.797121	506934.575350	46.291674
3503.695252	506923.813049	46.296679
3503.557028	506926.516776	46.301684
3503.518794	506929.052891	46.306689
3503.127741	506937.767676	46.311693
3503.648604	506930.550339	46.316698
3503.648746	506907.728494	46.321703
3503.244243	506907.185138	46.326708
3503.617932	506894.070540	46.331713
3503.154385	506898.495576	46.336717
3503.300706	506887.491616	46.341722
3503.819231	506892.014450	46.346727
3503.534656	506893.881067	46.351732
3503.675464	506892.492484	46.356737
3503.567329	506876.721481	46.361741
3503.810233	506862.514270	46.366746
3503.844802	506848.694194	46.371751
3503.626439	506849.234678	46.376756
3503.892280	506853.240828	46.381761
3503.502308	506845.813195	46.386765
3503.641915	506821.653522	46.391770
3503.719557	506821.388180	46.396775
3503.667722	506815.526383	46.401780
3503.610685	506805.566570	46.406785
3503.229191	506820.605266	46.411789
3503.497542	506801.890327	46.416794
3503.570163	506782.750877	46.421799
3503.645442	506782.283496	46.426804
3503.658697	506778.688533	46.431809
3503.509658	506770.666155	46.436813
3503.755794	506755.345079	46.441818
3503.062410	506764.360749	46.446823
3503.534500	506762.312561	46.451828
3503.599633	506765.237187	46.456833
3503.323151	506757.993990	46.461837
3503.595573	506735.634917	46.466842
3503.754026	506727.057889	46.471847
3503.195700	506723.755665	46.476852
3503.611266	506723.487516	46.481857
3503.478166	506728.518208	46.486861
3503.712177	506731.567958	46.491866
3503.389851	506721.903042	46.496871
3503.444798	506715.670112	46.501876
3503.550086	506703.154426	46.506881
3503.511610	506709.840074	46.511885
3503.909529	506701.630011	46.516890
3503.540805	506675.880572	46.521895
3503.541919	506690.049256	46.526900
3503.738231	506689.056711	46.531905
3503.859101	506660.497293	46.536909
3503.615867	506652.692161	46.541914
3503.850668	506644.457249	46.546919
3503.757829	506646.496001	46.551924
3503.475024	506645.680385	46.556929
3503.574755	506623.297859	46.561933
3503.467313	506610.259090	46.566938
3503.368160	506606.732461	46.571943
3503.200327	506613.944626	46.576948
3503.352001	506599.245585	46.581953
3502.848506	506616.277275	46.586957
3503.333351	506604.359375	46.591962
3503.508415	506613.490881	46.596967
3503.600864	506610.338797	46.601972
3503.844942	506608.225422	46.606977
3503.435585	506611.882912	46.611981
3502.932387	506606.396003	46.616986
3503.543652	506605.337870	46.621991
3503.259861	506614.845519	46.626996
3503.438468	506617.347407	46.632001
3503.373130	506604.200773	46.637005
3503.703342	506587.601175	46.642010
3503.179070	506588.190015	46.647015
3503.277112	506577.193491	46.652020
3503.251207	506591.315921	46.657025
3503.588386	506578.662289	46.662029
3503.653262	506576.931458	46.667034
3503.601436	506598.800325	46.672039
3503.524961	506585.503626	46.677044
3503.736308	506575.602471	46.682049
3503.581651	506555.284207	46.687053
3503.551449	506546.281474	46.692058
3503.179352	506542.038915	46.697063
3503.328663	506542.268279	46.702068
3503.494436	506528.275402	46.707073
3503.487416	506547.202236	46.712077
3503.497605	506544.467971	46.717082
3503.397616	506550.404347	46.722087
3503.127892	506544.273274	46.727092
3502.964602	506544.602648	46.732097
3502.692822	506558.612155	46.737101
3503.363873	506547.676859	46.742106
3503.366162	506557.544153	46.747111
3503.195435	506555.901160	46.752116
3503.642963	506548.189221	46.757121
3503.629089	506556.692771	46.762125
3503.341977	506546.010118	46.767130
3503.527685	506520.729462	46.772135
3502.997891	506511.400842	46.777140
3503.373891	506507.394265	46.782145
3503.241893	506510.754920	46.787149
3503.503687	506507.019412	46.792154
3503.146491	506510.466264	46.797159
3503.174954	506518.507707	46.802164
3503.608457	506522.588643	46.807169
3503.261336	506532.207553	46.812173
3503.284654	506524.714461	46.817178
3503.534669	506517.387951	46.822183
3503.701057	506519.486955	46.827188
3503.839091	506515.366179	46.832193
3503.409008	506503.137380	46.837197
3503.219175	506474.323142	46.842202
3503.655275	506478.251866	46.847207
3503.203721	506479.638878	46.852212
3503.465803	506473.575540	46.857217
3503.231342	506482.113990	46.862221
3503.401955	506478.443491	46.867226
3503.552176	506473.511117	46.872231
3503.396560	506474.193506	46.877236
3503.594154	506464.952312	46.882241
3503.234311	506476.192589	46.887245
3503.312390	506474.004226	46.892250
3503.056531	506477.131444	46.897255
3502.999144	506483.465941	46.902260
3503.774175	506475.145565	46.907265
3503.574069	506470.723995	46.912269
3503.370799	506450.919331	46.917274
3503.580291	506436.261619	46.922279
3503.307002	506446.880986	46.927284
3504.083239	506435.473560	46.932289
3503.690651	506445.251515	46.937293
3503.626017	506429.776856	46.942298
3503.592301	506405.289773	46.947303
3502.963656	506417.736465	46.952308
3503.293557	506390.256857	46.957313
3503.168642	506398.018972	46.962317
3502.948245	506408.579399	46.967322
3503.598859	506402.758253	46.972327
3503.251757	506395.323650	46.977332
3503.456489	506403.640912	46.982337
3503.318418	506405.484425	46.987341
3503.616887	506402.299743	46.992346
3503.258944	506411.920429	46.997351
3503.236418	506410.203395	47.002356
3503.718918	506405.623318	47.007361
3503.327192	506409.682896	47.012365
3503.456865	506406.879121	47.017370
3503.278101	506411.107456	47.022375
3503.611761	506408.828086	47.027380
3503.632301	506376.539360	47.032385
3503.164110	506372.868594	47.037389
3503.346022	506363.427408	47.042394
3503.451000	506363.360156	47.047399
3503.318871	506365.658172	47.052404
3503.741599	506379.760471	47.057409
3503.654566	506375.523422	47.062413
3503.432695	506374.445141	47.067418
3503.381068	506364.484221	47.072423
3503.239292	506370.680283	47.077428
3503.435583	506363.412805	47.082433
3503.640456	506344.403784	47.087437
3503.599266	506327.457806	47.092442
3503.935626	506324.874373	47.097447
3503.660703	506328.510674	47.102452
3503.499849	506318.212761	47.107457
3503.521278	506322.409477	47.112461
3503.426874	506292.770187	47.117466
3503.334413	506289.191831	47.122471
3503.446359	506293.070622	47.127476
3503.818697	506281.372702	47.132481
3503.463398	506284.465066	47.137485
3503.308068	506284.084725	47.142490
3503.289310	506287.376921	47.147495
3503.447382	506285.681936	47.152500
3503.461206	506296.357225	47.157505
3503.471100	506299.746099	47.162509
3503.679304	506264.340638	47.167514
3503.329009	506247.241017	47.172519
3503.164453	506248.228456	47.177524
3503.871265	506237.337919	47.182529
3503.364348	506242.529042	47.187533
3503.184739	506244.885182	47.192538
3503.418303	506246.720579	47.197543
3502.951528	506242.796538	47.202548
3503.264247	506239.457761	47.207553
3503.548328	506246.092606	47.212557
3503.488600	506249.037053	47.217562
3503.385204	506260.135727	47.222567
3503.381376	506257.201215	47.227572
3503.909031	506234.649348	47.232577
3503.652599	506224.771323	47.237581
3503.653146	506223.404856	47.242586
3503.774540	506207.293343	47.247591
3503.696142	506213.934885	47.252596
3504.045216	506205.327473	47.257601
3503.779447	506178.700749	47.262605
3503.810802	506165.336083	47.267610
3503.760739	506171.922558	47.272615
3503.515480	506169.076794	47.277620
3503.613330	506154.588306	47.282625
3503.526878	506128.034373	47.287629
3503.495804	506129.810398	47.292634
3503.466657	506125.513534	47.297639
3503.537676	506123.933502	47.302644
3503.694803	506128.716076	47.307649
3503.336736	506126.545998	47.312653
3504.002475	506124.922575	47.317658
3503.700825	506100.325598	47.322663
3503.644453	506090.618296	47.327668
3503.693785	506079.021898	47.332673
3503.352334	506083.832679	47.337677
3503.610179	506089.864471	47.342682
3503.738169	506079.520765	47.347687
3503.461911	506053.654583	47.352692
3503.749494	506049.307640	47.357697
3503.525228	506055.010801	47.362701
3503.229599	506049.035462	47.367706
3503.684251	506050.076861	47.372711
3503.471089	506047.782660	47.377716
3503.908585	506036.985171	47.382721
3503.606509	506017.448657	47.387725
3503.616473	506003.075144	47.392730
3503.379660	505998.153202	47.397735
3503.188407	506003.648740	47.402740
3503.676887	506005.140242	47.407745
3503.483181	506005.525038	47.412749
3503.687796	505998.256093	47.417754
3503.833341	506000.409059	47.422759
3503.288953	505980.404749	47.427764
3503.813923	505975.159979	47.432769
3503.435464	505971.727971	47.437773
3503.421113	505969.604760	47.442778
3503.474256	505974.302600	47.447783
3503.228953	505961.436952	47.452788
3503.578063	505966.644676	47.457793
3503.446078	505971.877830	47.462797
3503.676928	505950.080982	47.467802
3503.620259	505939.563958	47.472807
3503.147318	505938.677147	47.477812
3503.535994	505931.227267	47.482817
3503.771655	505925.471548	47.487821
3503.353768	505925.031485	47.492826
3503.403893	505916.015731	47.497831
3503.364355	505928.723898	47.502836
3503.841331	505922.423984	47.507841
3503.363640	505907.925045	47.512845
3503.695810	505886.466343	47.517850
3503.524610	505879.864013	47.522855
3503.080452	505903.465743	47.527860
3503.511679	505888.924345	47.532865
3503.458339	505886.604863	47.537869
3503.202481	505881.534081	47.542874
3503.340440	505896.440864	47.547879
3503.555658	505890.131703	47.552884
3503.671250	505877.765615	47.557889
3503.337897	505895.530198	47.562893
3503.599688	505838.203188	47.567898
3503.413487	505855.590313	47.572903
3503.335537	505831.919109	47.577908
3503.298108	505847.106683	47.582913
3503.296374	505846.044181	47.587917
3503.146502	505831.088521	47.592922
3503.701845	505837.832466	47.597927
3503.394455	505859.135381	47.602932
3503.236722	505837.804655	47.607937
3503.204815	505855.977085	47.612941
3503.197673	505853.650297	47.617946
3503.431701	505856.042325	47.622951
3503.250210	505874.491406	47.627956
3503.774835	505843.285954	47.632961
3503.290778	505863.655278	47.637965
3503.481910	505832.047064	47.642970
3503.624419	505821.144248	47.647975
3503.441072	505811.507466	47.652980
3503.489733	505825.517518	47.657985
3503.559588	505799.849286	47.662989
3503.480362	505843.686344	47.667994
3503.799382	505805.580338	47.672999
3503.433963	505824.007936	47.678004
3503.639596	505784.300421	47.683009
3503.437990	505780.891029	47.688013
3503.834788	505775.008582	47.693018
3503.764129	505766.770930	47.698023
3503.385723	505794.157858	47.703028
3503.529184	505766.048862	47.708033
3503.077708	505770.472271	47.713037
3503.587105	505744.683882	47.718042
3503.218512	505744.590264	47.723047
3503.267691	505742.052136	47.728052
3503.590457	505727.274716	47.733057
3503.692724	505725.639104	47.738061
3503.744393	505718.697852	47.743066
3503.459088	505735.544093	47.748071
3503.393549	505739.096816	47.753076
3503.641206	505720.839447	47.758081
3503.561791	505720.194064	47.763085
3503.310197	505698.574367	47.768090
3503.784431	505689.491466	47.773095
3503.536206	505688.619732	47.778100
3503.500123	505681.591122	47.783105
3503.153324	505688.831953	47.788109
3503.181349	505683.665639	47.793114
3503.747144	505684.031615	47.798119
3503.445916	505688.431297	47.803124
3503.559738	505678.747474	47.808129
3503.467895	505666.667054	47.813133
3503.529882	505653.550187	47.818138
3503.683043	505635.965546	47.823143
3503.147092	505665.604252	47.828148
3503.785701	505636.354059	47.833153
3503.898937	505659.716201	47.838157
3503.826364	505636.094489	47.843162
3503.865713	505605.572588	47.848167
3503.488237	505594.346964	47.853172
3503.841921	505602.084396	47.858177
3503.399445	505593.500577	47.863181
3503.127461	505617.277904	47.868186
3503.331955	505588.754127	47.873191
3503.466164	505621.323374	47.878196
3503.111449	505585.701873	47.883201
3503.130638	505609.686223	47.888205
3502.977478	505590.884792	47.893210
3502.960304	505617.000349	47.898215
3503.480803	505591.412406	47.903220
3503.468052	505627.850957	47.908225
3503.268670	505588.915500	47.913229
3503.144550	505614.390081	47.918234
3503.559164	505575.205732	47.923239
3503.612644	505593.263727	47.928244
3503.378041	505559.141380	47.933249
3503.049213	505602.208787	47.938253
3502.941347	505562.702138	47.943258
3503.098366	505555.035680	47.948263
3502.897656	505592.516141	47.953268
3503.856905	505556.029024	47.958273
3503.452504	505578.663382	47.963277
3503.299471	505578.586300	47.968282
3503.277321	505564.318715	47.973287
3503.330383	505552.114100	47.978292
3503.309740	505580.963013	47.983297
3503.173054	505581.338805	47.988301
3502.979790	505562.138830	47.993306
3503.079757	505569.663343	47.998311
3503.067704	505582.974694	48.003316
3503.380593	505569.919323	48.008321
3503.158796	505581.340779	48.013325
3503.137441	505584.785337	48.018330
3503.165353	505569.700141	48.023335
3503.348149	505582.879483	48.028340
3503.502516	505577.338925	48.033345
3503.147802	505588.376532	48.038349
3503.204308	505584.825094	48.043354
3503.613553	505573.323296	48.048359
3503.265701	505582.791021	48.053364
3503.697705	505578.421138	48.058369
3503.526220	505581.079721	48.063373
3503.499738	505568.331018	48.068378
3503.304635	505544.981582	48.073383
3503.469306	505524.459829	48.078388
3503.583371	505525.757517	48.083393
3503.368103	505543.048333	48.088397
3503.556198	505538.109710	48.093402
3503.539451	505535.835005	48.098407
3503.201857	505543.631112	48.103412
3503.572407	505542.206113	48.108417
3503.545384	505549.194034	48.113421
3503.266379	505539.471007	48.118426
3503.561848	505513.716091	48.123431
3503.407204	505511.665604	48.128436
3503.322369	505507.883456	48.133441
3503.243121	505515.183284	48.138445
3502.900829	505501.725347	48.143450
3503.185646	505497.783560	48.148455
3502.822071	505510.897491	48.153460
3503.307022	505503.229787	48.158465
3503.358126	505495.883684	48.163469
3503.506701	505505.424810	48.168474
3503.278697	505507.333237	48.173479
3502.774404	505509.184118	48.178484
3503.032371	505480.348073	48.183489
3502.975139	505531.216773	48.188493
3502.818231	505537.010668	48.193498
3503.233985	505548.432593	48.198503
3503.023239	505553.830140	48.203508
3503.145361	505547.333144	48.208513
3503.245226	505539.878139	48.213517
3502.880365	505547.374915	48.218522
3502.891475	505565.945699	48.223527
3503.431377	505560.141776	48.228532
3503.412419	505540.408162	48.233537
3503.247959	505558.905490	48.238541
3503.509628	505558.509831	48.243546
3503.644499	505554.136297	48.248551
3503.071449	505555.491975	48.253556
3503.032727	505560.659905	48.258561
3503.154068	505553.454544	48.263565
3502.885047	505546.260270	48.268570
3503.053462	505565.464078	48.273575
3503.279820	505573.171040	48.278580
3503.518426	505560.431040	48.283585
3503.043371	505559.595150	48.288589
3503.144844	505563.576971	48.293594
3503.679869	505558.229276	48.298599
3503.072355	505576.492971	48.303604
3503.258855	505570.188235	48.308609
3503.327974	505577.160949	48.313613
3503.366431	505559.341328	48.318618
3503.298589	505549.989785	48.323623
3502.963793	505557.329985	48.328628
3503.487647	505551.882841	48.333633
3503.185321	505548.489323	48.338637
3502.900377	505528.848342	48.343642
3502.936796	505568.973526	48.348647
3503.160006	505561.903887	48.353652
3503.066901	505587.677243	48.358657
3503.302624	505567.954015	48.363661
3503.234335	505580.717585	48.368666
3503.183368	505581.737713	48.373671
3503.323124	505581.310717	48.378676
3503.758920	505563.630727	48.383681
3503.341242	505559.091492	48.388685
3502.900084	505542.207968	48.393690
3503.410029	505547.744643	48.398695
3503.262843	505545.743588	48.403700
3503.324602	505530.450583	48.408705
3503.367574	505549.927267	48.413709
3502.957925	505551.510153	48.418714
3503.292875	505537.186106	48.423719
3502.763445	505546.227090	48.428724
3503.076872	505569.557712	48.433729
3502.976353	505581.972129	48.438733
3503.094526	505585.242816	48.443738
3503.271694	505582.988074	48.448743
3503.283837	505593.056780	48.453748
3503.427197	505581.495798	48.458753
3503.001656	505595.176130	48.463757
3503.576235	505582.231227	48.468762
3503.460766	505571.267816	48.473767
3503.523625	505578.899404	48.478772
3503.512478	505549.852974	48.483777
3503.480622	505535.789327	48.488781
3503.560911	505551.059764	48.493786
3503.408283	505556.043272	48.498791
3503.193647	505558.506253	48.503796
3503.209575	505542.663830	48.508801
3503.531714	505548.382008	48.513805
3503.614748	505548.773680	48.518810
3503.902583	505543.414443	48.523815
3503.098664	505526.335206	48.528820
3503.703257	505507.009068	48.533825
3503.762350	505508.366053	48.538829
3503.503538	505498.943452	48.543834
3503.720378	505512.876567	48.548839
3503.662789	505527.713357	48.553844
3503.642817	505499.427338	48.558849
3503.615452	505479.188918	48.563853
3503.717729	505465.559475	48.568858
3503.897943	505479.498405	48.573863
3503.307210	505474.227398	48.578868
3503.534006	505471.812979	48.583873
3503.613339	505475.292251	48.588877
3503.591117	505440.326398	48.593882
3503.620620	505444.269014	48.598887
3503.084128	505415.457214	48.603892
3503.545403	505424.746534	48.608897
3503.667297	505416.073429	48.613901
3503.371177	505430.391325	48.618906
3503.680409	505430.443608	48.623911
3503.366738	505422.800878	48.628916
3503.703630	505419.407520	48.633921
3503.234107	505416.495863	48.638925
3503.488522	505414.481926	48.643930
3503.725299	505392.531629	48.648935
3503.636065	505413.699391	48.653940
3503.874245	505374.491874	48.658945
3503.495446	505413.822718	48.663949
3503.281225	505392.955840	48.668954
3503.742403	505354.472138	48.673959
3503.574782	505356.320430	48.678964
3503.671956	505369.968930	48.683969
3503.490865	505341.151443	48.688973
3502.841778	505369.442136	48.693978
3503.734016	505349.361864	48.698983
3503.171390	505373.387887	48.703988
3503.790525	505342.116000	48.708993
3503.577192	505357.736656	48.713997
3503.568056	505338.254299	48.719002
3503.456850	505318.939873	48.724007
3503.002921	505311.319263	48.729012
3503.531594	505325.051420	48.734017
3503.676933	505321.840139	48.739021
3503.698558	505320.065413	48.744026
3503.658982	505327.156620	48.749031
3503.646462	505309.648446	48.754036
3503.290115	505282.174350	48.759041
3503.175972	505297.576953	48.764045
3503.362966	505286.110094	48.769050
3503.728131	505280.232482	48.774055
3503.312219	505275.541072	48.779060
3503.358998	505274.116617	48.784065
3503.154369	505275.920159	48.789069
3503.207075	505274.342946	48.794074
3503.485433	505278.296875	48.799079
3503.501685	505282.140407	48.804084
3503.486946	505282.496932	48.809089
3503.640229	505277.968597	48.814093
3503.383667	505275.225687	48.819098
3503.554090	505243.467864	48.824103
3503.032124	505256.961269	48.829108
3503.744270	505249.966052	48.834113
3503.676324	505250.229771	48.839117
3503.344949	505246.081674	48.844122
3503.647756	505245.780722	48.849127
3503.277239	505250.495109	48.854132
3503.699148	505233.677308	48.859137
3503.718500	505243.542646	48.864141
3503.503620	505219.892257	48.869146
3503.881690	505197.615740	48.874151
3503.345241	505210.352357	48.879156
3503.872553	505207.232507	48.884161
3503.444380	505182.654236	48.889165
3503.485075	505208.103356	48.894170
3503.903858	505181.518743	48.899175
3503.249802	505173.828487	48.904180
3503.844170	505156.123026	48.909185
3503.983825	505148.914605	48.914189
3503.590075	505173.066032	48.919194
3503.842955	505133.653224	48.924199
3503.490792	505119.386828	48.929204
3503.360102	505118.243449	48.934209
3503.206528	505114.573296	48.939213
3503.139077	505116.608213	48.944218
3503.757968	505114.081166	48.949223
3503.183244	505112.299457	48.954228
3503.779867	505113.875162	48.959233
3503.490636	505113.971427	48.964237
3503.593634	505128.884388	48.969242
3503.912253	505091.384190	48.974247
3503.775169	505067.771908	48.979252
3503.655463	505084.035913	48.984257
3503.582675	505075.241585	48.989261
3503.623932	505063.898832	48.994266
3503.406131	505044.044264	48.999271
3503.214986	505030.460859	49.004276
3503.452280	505046.820298	49.009281
3503.539370	505034.761769	49.014285
3503.543904	505014.112907	49.019290
3503.247292	505040.526527	49.024295
3503.456817	505025.817024	49.029300
3503.746064	505021.469567	49.034305
3503.651666	505029.025032	49.039309
3503.460687	505023.387058	49.044314
3503.547167	505000.903338	49.049319
3503.107172	505001.175256	49.054324
3503.118559	504990.950554	49.059329
3503.524263	504984.813396	49.064333
3503.202419	504984.509951	49.069338
3503.256232	504986.930582	49.074343
3502.972376	504996.540331	49.079348
3502.997100	505000.787451	49.084353
3503.034606	504991.975650	49.089357
3502.724190	504981.295723	49.094362
3503.008159	505015.208847	49.099367
3502.491026	505027.689502	49.104372
3503.098469	505036.196806	49.109377
3503.249497	505027.518905	49.114381
3503.102526	505034.019908	49.119386
3503.101814	505022.582544	49.124391
3503.028358	505038.130768	49.129396
3503.161819	505015.082953	49.134401
3503.178089	505041.598945	49.139405
3503.114877	505031.537882	49.144410
3502.895284	505024.487405	49.149415
3502.712405	505053.868905	49.154420
3503.239253	505040.728717	49.159425
3503.185692	505040.635911	49.164429
3502.883198	505038.760559	49.169434
3503.457414	505085.633930	49.174439
3503.103497	505066.458803	49.179444
3503.118862	505080.474713	49.184449
3503.030105	505088.940203	49.189453
3503.448793	505083.307106	49.194458
3503.538015	505070.539754	49.199463
3503.076147	505085.035951	49.204468
3503.194040	505040.178615	49.209473
3503.615851	505060.709343	49.214477
3503.438554	505025.514134	49.219482
3503.742988	505042.925734	49.224487
3503.803273	505039.322981	49.229492
3503.283707	505051.702787	49.234497
3503.450170	505041.706646	49.239501
3503.230599	505039.666364	49.244506
3503.270746	505048.921228	49.249511
3503.219336	505062.593450	49.254516
3502.878122	505043.719939	49.259521
3502.973990	505060.607797	49.264525
3502.787841	505038.825118	49.269530
3502.843938	505039.676532	49.274535
3502.986731	505059.239201	49.279540
3503.225918	505046.245697	49.284545
3503.159810	505043.725690	49.289549
3503.148479	505054.051455	49.294554
3503.051451	505045.412768	49.299559
3503.315953	505036.312072	49.304564
3502.857246	505067.457818	49.309569
3503.224243	505053.128313	49.314573
3503.103794	505074.301417	49.319578
3503.115302	505046.870028	49.324583
3502.994713	505087.172952	49.329588
3503.348182	505070.011558	49.334593
3503.342708	505058.220715	49.339597
3502.906128	505104.393457	49.344602
3503.217342	505080.001829	49.349607
3503.321817	505073.760487	49.354612
3503.193240	505088.963123	49.359617
3503.698360	505054.520449	49.364621
3503.526577	505056.369431	49.369626
3503.132391	505067.312387	49.374631
3503.448027	505069.641017	49.379636
3503.281438	505056.053751	49.384641
3503.354523	505068.997780	49.389645
3503.066517	505057.150375	49.394650
3503.560107	505081.161684	49.399655
3503.215999	505060.365547	49.404660
3503.000165	505093.649002	49.409665
3503.450542	505076.573513	49.414669
3503.415120	505064.129505	49.419674
3503.464423	505081.581390	49.424679
3503.069218	505101.633905	49.429684
3503.329913	505058.575928	49.434689
3503.194411	505089.316297	49.439693
3503.147557	505074.647355	49.444698
3503.568386	505079.641578	49.449703
3503.574324	505071.998788	49.454708
3503.695375	505045.056163	49.459713
3503.765777	505051.978275	49.464717
3503.336476	505033.523538	49.469722
3503.681775	505037.568158	49.474727
3503.418628	505023.996128	49.479732
3503.498687	505045.289401	49.484737
3503.358914	505041.515836	49.489741
3503.317116	505029.275242	49.494746
3503.673238	505001.789317	49.499751
3503.293759	504993.600110	49.504756
3503.235081	505003.781564	49.509761
3502.894512	505002.215875	49.514765
3502.998137	504988.434025	49.519770
3503.150546	505011.082325	49.524775
3502.924311	505011.573499	49.529780
3503.418589	505009.319173	49.534785
3503.100075	505040.544025	49.539789
3502.977139	505041.524951	49.544794
3503.124416	505027.179544	49.549799
3503.324219	505043.595520	49.554804
3503.205031	505028.178852	49.559809
3503.149275	505057.894510	49.564813
3503.308357	505042.686914	49.569818
3503.504309	505038.455423	49.574823
3503.341996	505033.521433	49.579828
3503.279044	505018.652557	49.584833
3503.352030	505000.219615	49.589837
3503.266384	504994.514375	49.594842
3503.703561	504999.961511	49.599847
3503.525595	505012.439179	49.604852
3503.177111	504998.273320	49.609857
3503.334686	505003.005523	49.614861
3503.271941	505015.566195	49.619866
3503.488589	504994.478920	49.624871
3503.041182	504996.523294	49.629876
3503.373375	505025.469178	49.634881
3503.331864	504995.768726	49.639885
3502.948153	505005.343644	49.644890
3503.107600	505014.174806	49.649895
3503.131138	505012.652787	49.654900
3503.214601	504999.785078	49.659905
3503.414753	505016.302240	49.664909
3503.332880	505036.406523	49.669914
3503.524268	505009.452726	49.674919
3503.065349	505007.500878	49.679924
3503.349835	505026.130243	49.684929
3503.184762	505012.137839	49.689933
3502.935050	505014.150966	49.694938
3503.347680	504999.409340	49.699943
3503.125372	505008.452666	49.704948
3503.136172	505016.143334	49.709953
3502.934459	505016.681239	49.714957
3503.266508	505004.229717	49.719962
3503.735186	505008.609101	49.724967
3503.084893	505031.789106	49.729972
3503.518860	505020.030000	49.734977
3503.427839	505013.009806	49.739981
3502.866257	505016.539858	49.744986
3503.474590	505014.874804	49.749991
3503.224783	505006.310853	49.754996
3503.215894	504988.346311	49.760001
3503.492771	504976.257747	49.765005
3503.404023	504996.059513	49.770010
3503.672387	504979.215130	49.775015
3503.433721	504969.536019	49.780020
3503.463821	504990.229956	49.785025
3503.687886	504988.170160	49.790029
3503.568114	504981.205106	49.795034
3503.543168	504974.326277	49.800039
3503.583627	504954.734439	49.805044
3503.485755	504936.024784	49.810049
3503.509309	504935.110056	49.815053
3503.522301	504937.587754	49.820058
3503.703555	504932.295785	49.825063
3503.420412	504942.715185	49.830068
3503.335085	504942.829831	49.835073
3503.685557	504926.427895	49.840077
3502.848885	504921.144981	49.845082
3503.536560	504920.327721	49.850087
3503.672733	504913.980096	49.855092
3503.432622	504910.272969	49.860097
3503.335643	504887.058973	49.865101
3503.444431	504903.287031	49.870106
3503.615191	504884.889123	49.875111
3503.169573	504913.856907	49.880116
3503.157131	504876.054316	49.885121
3503.083428	504913.414935	49.890125
3502.953388	504881.653338	49.895130
3503.018637	504915.297573	49.900135
3503.047726	504887.711332	49.905140
3503.540910	504906.662098	49.910145
3503.006652	504900.319213	49.915149
3503.457463	504874.386984	49.920154
3503.667772	504905.781536	49.925159
3503.109950	504909.918316	49.930164
3503.220755	504886.519654	49.935169
3503.723549	504919.284992	49.940173
3503.690917	504910.180585	49.945178
3503.570212	504864.905037	49.950183
3503.786918	504894.173040	49.955188
3503.563631	504878.216001	49.960193
3502.966366	504861.407101	49.965197
3503.650946	504836.905517	49.970202
3503.797768	504848.471622	49.975207
3503.040471	504875.514996	49.980212
3503.343411	504851.681053	49.985217
3503.398601	504871.561427	49.990221
3503.078419	504857.390981	49.995226
3503.010329	504862.918017	50.000231
3503.112174	504872.011397	50.005236
3503.328333	504853.555672	50.010241
3503.286773	504885.091287	50.015245
3503.044431	504850.715743	50.020250
3503.311538	504876.129560	50.025255
3503.340713	504854.717488	50.030260
3503.150406	504885.264441	50.035265
3503.628773	504858.568706	50.040269
3503.126547	504881.877332	50.045274
3503.337003	504844.950397	50.050279
3502.940162	504867.483258	50.055284
3502.904712	504852.559286	50.060289
3503.529103	504885.204251	50.065293
3503.291973	504873.196855	50.070298
3503.509250	504853.678176	50.075303
3503.068711	504866.754141	50.080308
3503.183739	504845.783966	50.085313
3503.265627	504868.089336	50.090317
3503.565601	504838.030995	50.095322
3503.319372	504861.248579	50.100327
3503.336167	504837.156190	50.105332
3503.488155	504854.136594	50.110337
3503.682127	504841.554955	50.115341
3503.132795	504838.503989	50.120346
3503.439802	504850.753295	50.125351
3503.422006	504848.175015	50.130356
3503.457529	504832.278246	50.135361
3503.012027	504869.900155	50.140365
3502.825694	504840.829633	50.145370
3503.329611	504823.340568	50.150375
3503.159422	504858.084905	50.155380
3503.361274	504834.823610	50.160385
3502.880046	504864.151364	50.165389
3503.170217	504840.116989	50.170394
3502.887171	504859.848401	50.175399
3503.070078	504836.286450	50.180404
3503.152078	504853.379135	50.185409
3503.242972	504868.344839	50.190413
3503.330139	504835.992136	50.195418
3503.556759	504845.824938	50.200423
3503.038787	504875.968218	50.205428
3503.427979	504845.035443	50.210433
3503.732252	504867.103232	50.215437
3503.513674	504852.208204	50.220442
3503.419161	504874.440229	50.225447
3503.110225	504856.472367	50.230452
3503.469033	504833.742957	50.235457
3503.334483	504847.276661	50.240461
3503.816847	504819.568064	50.245466
3503.600615	504805.532973	50.250471
3503.402901	504835.322052	50.255476
3503.456427	504808.541562	50.260481
3503.609448	504801.887582	50.265485
3503.042287	504837.200789	50.270490
3503.116688	504803.382395	50.275495
3503.131695	504821.093003	50.280500
3503.223063	504809.489122	50.285505
3503.550808	504824.366821	50.290509
3503.045111	504836.542151	50.295514
3503.823034	504805.547868	50.300519
3503.292374	504820.864893	50.305524
3503.149433	504780.906550	50.310529
3503.838958	504802.508661	50.315533
3502.884716	504775.482530	50.320538
3503.329481	504797.173940	50.325543
3503.491217	504771.641510	50.330548
3503.253765	504785.343351	50.335553
3503.629217	504780.273688	50.340557
3503.293287	504781.136466	50.345562
3503.721870	504788.255115	50.350567
3503.510321	504771.536993	50.355572
3503.619552	504783.311517	50.360577
3503.676223	504757.441410	50.365581
3503.401425	504742.605783	50.370586
3503.513481	504733.073546	50.375591
3503.832418	504725.988443	50.380596
3503.329353	504744.894405	50.385601
3503.264553	504737.869957	50.390605
3503.450977	504735.461819	50.395610
3503.844082	504727.605861	50.400615
3503.164772	504743.047665	50.405620
3503.434320	504709.906773	50.410625
3503.309577	504714.886110	50.415629
3503.213910	504685.902220	50.420634
3503.136447	504714.457881	50.425639
3503.154713	504695.071698	50.430644
3503.302757	504695.959205	50.435649
3503.693095	504704.905857	50.440653
3503.419640	504692.448598	50.445658
3503.836203	504691.927223	50.450663
3503.082225	504715.832557	50.455668
3503.522017	504682.006788	50.460673
3503.480626	504720.223064	50.465677
3503.288073	504687.964909	50.470682
3503.270310	504708.666742	50.475687
3503.233462	504686.404548	50.480692
3503.479764	504694.159354	50.485697
3503.399519	504677.116734	50.490701
3503.275018	504662.813985	50.495706
3503.633944	504662.605373	50.500711
3503.348471	504672.772255	50.505716
3503.317295	504652.634702	50.510721
3503.448420	504678.525779	50.515725
3503.191221	504647.745430	50.520730
3503.186296	504667.281272	50.525735
3502.834940	504627.203693	50.530740
3503.608520	504571.259329	50.535745
3503.452301	504574.118088	50.540749
3502.708995	504506.823717	50.545754
3503.297706	504409.408177	50.550759
3503.015316	504387.791731	50.555764
3502.864725	504314.026096	50.560769
3502.976546	504214.053124	50.565773
3502.771226	504075.665552	50.570778
3502.880502	503990.267616	50.575783
3502.350734	503844.084795	50.580788
3502.443538	503709.240645	50.585793
3502.234650	503574.999884	50.590797
3501.885343	503446.701972	50.595802
3502.010706	503270.093892	50.600807
3501.186352	503093.583543	50.605812
3501.130541	502968.272592	50.610817
3501.184670	502784.838051	50.615821
3500.592247	502613.803246	50.620826
3500.598237	502399.902101	50.625831
3500.056808	502186.287370	50.630836
3499.884215	501969.321686	50.635841
3500.160029	501720.494723	50.640845
3498.828433	501533.874931	50.645850
3498.736142	501329.543276	50.650855
3498.839544	501059.474520	50.655860
3498.357488	500851.756891	50.660865
3497.793175	500583.305084	50.665869
3497.842446	500300.679500	50.670874
3497.797321	500070.914011	50.675879
3496.979292	499814.893239	50.680884
3496.851176	499493.353953	50.685889
3496.461552	499264.138852	50.690893
3495.920955	498955.361895	50.695898
3495.939608	498634.644740	50.700903
3495.156647	498387.305864	50.705908
3494.525268	498055.948292	50.710913
3494.048061	497784.808402	50.715917
3493.861332	497463.191669	50.720922
3493.449639	497145.756495	50.725927
3493.211292	496846.870046	50.730932
3492.562987	496527.942576	50.735937
3492.077981	496166.502629	50.740941
3491.498814	495864.514726	50.745946
3491.147127	495508.509180	50.750951
3490.622030	495178.196506	50.755956
3490.022546	494855.940888	50.760961
3489.970932	494489.133192	50.765965
3489.148982	494170.445385	50.770970
3488.914952	493781.827233	50.775975
3488.082092	493460.141164	50.780980
3487.839959	493088.221098	50.785985
3486.996116	492704.386401	50.790989
3486.393998	492367.249573	50.795994
3486.133668	491968.063765	50.800999
3484.987531	491627.454426	50.806004
3484.750361	491249.925869	50.811009
3484.338720	490880.166351	50.816013
3483.471923	490502.165130	50.821018
3483.621312	490114.524215	50.826023
3482.661214	489716.515359	50.831028
3481.799493	489350.393108	50.836033
3481.834174	488960.669901	50.841037
3480.731249	488558.455054	50.846042
3480.144148	488196.116757	50.851047
3480.204832	487765.739769	50.856052
3479.056523	487386.302408	50.861057
3478.834008	486989.132872	50.866061
3477.568811	486584.470387	50.871066
3477.562523	486196.318175	50.876071
3476.595328	485775.126986	50.881076
3475.762193	485387.849049	50.886081
3475.393135	484975.715665	50.891085
3474.511438	484583.869564	50.896090
3474.093157	484170.054856	50.901095
3473.374457	483761.345441	50.906100
3473.015615	483351.405188	50.911105
3472.382788	482956.953509	50.916109
3471.854666	482527.413952	50.921114
3471.172476	482102.500341	50.926119
3470.433901	481712.600615	50.931124
3469.719304	481275.664995	50.936129
3468.852161	480868.793423	50.941133
3468.564732	480448.392945	50.946138
3467.662905	480028.536718	50.951143
3466.946147	479636.514728	50.956148
3465.931105	479204.800492	50.961153
3465.293307	478802.208474	50.966157
3464.664447	478397.427651	50.971162
3464.425932	477952.741411	50.976167
3463.678709	477555.868527	50.981172
3463.011738	477150.865753	50.986177
3462.465451	476714.918224	50.991181
3461.552063	476318.351242	50.996186
3461.169991	475875.010176	51.001191
3460.046940	475466.497554	51.006196
3459.341645	475054.058314	51.011201
3459.102900	474629.929001	51.016205
3457.819132	474209.707148	51.021210
3457.183586	473791.199062	51.026215
3456.535213	473379.527957	51.031220
3455.817629	472981.344064	51.036225
3455.876752	472559.710049	51.041229
3454.864233	472129.415703	51.046234
3454.402310	471726.452363	51.051239
3453.479983	471294.402637	51.056244
3452.481600	470869.200271	51.061249
3452.239763	470464.301692	51.066253
3451.463613	470053.446270	51.071258
3450.955723	469616.175290	51.076263
3450.161431	469195.013299	51.081268
3449.449552	468773.779095	51.086273
3449.151291	468357.338730	51.091277
3447.661790	467945.287027	51.096282
3447.391496	467526.189068	51.101287
3446.425634	467104.758753	51.106292
3445.655961	466679.130877	51.111297
3445.166547	466263.085075	51.116301
3444.186004	465858.265203	51.121306
3443.577931	465436.745196	51.126311
3442.946061	465031.753082	51.131316
3442.079592	464636.882468	51.136321
3441.856155	464205.438873	51.141325
3440.353097	463814.102366	51.146330
3440.118102	463385.687107	51.151335
3439.359142	462958.411250	51.156340
3438.718767	462591.565086	51.161345
3438.171677	462144.510054	51.166349
3437.049646	461763.879518	51.171354
3436.811757	461337.351615	51.176359
3435.940132	460944.088185	51.181364
3435.272734	460536.937865	51.186369
3434.411156	460105.158551	51.191373
3433.342746	459733.462433	51.196378
3433.055507	459314.308872	51.201383
3432.027851	458909.873874	51.206388
3431.370380	458521.758173	51.211393
3430.753157	458123.077657	51.216397
3430.073937	457716.891741	51.221402
3429.402580	457326.525228	51.226407
3428.603285	456927.750625	51.231412
3427.565479	456511.047217	51.236417
3427.198859	456118.328461	51.241421
3426.324386	455738.975576	51.246426
3425.961292	455327.064785	51.251431
3424.955831	454959.693053	51.256436
3424.295231	454545.531910	51.261441
3423.843525	454149.443681	51.266445
3422.854987	453770.329488	51.271450
3422.586129	453380.744286	51.276455
3421.662878	452962.587389	51.281460
3420.431410	452593.082033	51.286465
3420.362344	452200.705099	51.291469
3419.350906	451814.762613	51.296474
3418.607019	451429.836985	51.301479
3418.182134	451041.048629	51.306484
3417.477589	450660.163552	51.311489
3416.690710	450250.308881	51.316493
3415.919635	449894.642853	51.321498
3415.224047	449485.724476	51.326503
3414.645380	449101.901318	51.331508
3413.598262	448722.865674	51.336513
3413.025573	448323.702301	51.341517
3412.250770	447954.203104	51.346522
3411.770900	447562.472636	51.351527
3410.933814	447184.038767	51.356532
3410.185433	446812.335120	51.361537
3409.871147	446430.558291	51.366541
3408.564055	446064.362039	51.371546
3408.114260	445678.128052	51.376551
3407.247521	445306.876399	51.381556
3406.614901	444926.140954	51.386561
3406.161582	444551.563708	51.391565
3405.182332	444177.571370	51.396570
3404.601802	443803.611707	51.401575
3404.143346	443433.687854	51.406580
3403.302575	443057.168957	51.411585
3402.805279	442666.731640	51.416589
3402.207067	442300.061415	51.421594
3401.465279	441915.336226	51.426599
3401.102150	441545.267032	51.431604
3399.685258	441174.901949	51.436609
3399.579384	440796.810514	51.441613
3398.732389	440425.379454	51.446618
3397.850952	440045.673002	51.451623
3396.711204	439675.622296	51.456628
3396.348885	439309.403192	51.461633
3395.870527	438937.586878	51.466637
3394.661350	438573.242397	51.471642
3394.263015	438192.948880	51.476647
3393.910575	437828.788094	51.481652
3392.858913	437468.337488	51.486657
3392.327022	437093.887359	51.491661
3391.491459	436729.177712	51.496666
3391.099521	436360.635238	51.501671
3390.361721	435988.283056	51.506676
3389.525862	435612.081827	51.511681
3389.086902	435262.521525	51.516685
3388.260127	434892.731633	51.521690
3387.527925	434525.790468	51.526695
3386.978080	434159.703859	51.531700
3386.057934	433787.805370	51.536705
3385.264499	433423.600277	51.541709
3384.344230	433070.810729	51.546714
3383.864209	432709.186671	51.551719
3383.039027	432350.913078	51.556724
3382.630714	431992.136955	51.561729
3382.038048	431621.069621	51.566733
3380.964682	431269.143112	51.571738
3380.527457	430910.102730	51.576743
3379.766399	430551.083232	51.581748
3379.188003	430192.436243	51.586753
3378.557240	429829.374029	51.591757
3377.495433	429475.110739	51.596762
3377.241406	429107.458774	51.601767
3376.592766	428749.463554	51.606772
3375.423055	428404.421518	51.611777
3375.191060	428037.411542	51.616781
3374.241315	427689.760468	51.621786
3373.756438	427343.148825	51.626791
3373.040915	426975.057868	51.631796
3372.161378	426616.791198	51.636801
3371.560433	426256.494687	51.641805
3370.766536	425913.342174	51.646810
3370.321878	425561.875612	51.651815
3369.246887	425203.798900	51.656820
3368.520896	424862.959041	51.661825
3368.083714	424507.744010	51.666829
3367.173721	424164.206782	51.671834
3366.471426	423812.682197	51.676839
3365.725814	423460.042345	51.681844
3365.246350	423109.718151	51.686849
3364.698005	422768.671757	51.691853
3363.893522	422422.759207	51.696858
3363.068175	422075.092925	51.701863
3362.324794	421729.822514	51.706868
3361.569549	421384.905328	51.711873
3361.199763	421034.690004	51.716877
3360.191382	420692.344551	51.721882
3359.847249	420353.649557	51.726887
3359.191282	420008.217059	51.731892
3358.615817	419670.541160	51.736897
3357.612425	419320.049008	51.741901
3356.868097	418975.024311	51.746906
3356.319105	418614.264408	51.751911
3355.563884	418284.501296	51.756916
3354.711349	417945.400596	51.761921
3354.369671	417598.618809	51.766925
3353.756188	417260.666264	51.771930
3352.734161	416925.264155	51.776935
3351.850481	416584.907395	51.781940
3351.450445	416245.969149	51.786945
3350.702995	415910.791311	51.791949
3349.787760	415575.458280	51.796954
3349.436417	415237.059512	51.801959
3348.878507	414897.444488	51.806964
3348.024663	414573.015661	51.811969
3347.214070	414225.251318	51.816973
3346.764922	413885.836046	51.821978
3345.846692	413554.469519	51.826983
3345.533641	413209.714424	51.831988
3344.772254	412882.508123	51.836993
3344.061946	412532.065355	51.841997
3343.210255	412213.886533	51.847002
3342.282694	411877.191981	51.852007
3342.108535	411531.683972	51.857012
3341.238516	411207.932347	51.862017
3340.603729	410864.624033	51.867021
3339.809602	410543.013222	51.872026
3339.264842	410194.905636	51.877031
3338.573073	409866.181478	51.882036
3337.607319	409550.279609	51.887041
3337.710120	409210.139520	51.892045
3336.489979	408872.339540	51.897050
3336.089279	408540.200504	51.902055
3335.073774	408202.132044	51.907060
3334.456961	407869.435406	51.912065
3333.704456	407532.690352	51.917069
3333.025296	407210.111327	51.922074
3332.517213	406869.457391	51.927079
3332.052707	406550.293966	51.932084
3331.145346	406219.048776	51.937089
3330.851690	405881.527031	51.942093
3329.518629	405551.892433	51.947098
3329.324451	405219.786819	51.952103
3328.680146	404889.146779	51.957108
3327.713440	404566.026752	51.962113
3327.333371	404213.403263	51.967117
3326.633729	403873.458744	51.972122
3325.791329	403547.741534	51.977127
3325.086396	403213.941831	51.982132
3324.823595	402891.405150	51.987137
3323.919745	402556.206628	51.992141
3323.574689	402218.552316	51.997146
3322.691491	401874.116487	52.002151
3321.759946	401549.435240	52.007156
3320.752182	401220.644859	52.012161
3320.327428	400889.827062	52.017165
3319.441187	400554.452470	52.022170
3319.296172	400231.006336	52.027175
3318.147976	399903.521291	52.032180
3317.802459	399580.456325	52.037185
3317.312635	399241.243347	52.042189
3316.460175	398921.455110	52.047194
3315.723947	398586.087531	52.052199
3315.303105	398256.310281	52.057204
3314.552794	397919.006146	52.062209
3313.730426	397584.506426	52.067213
3313.175498	397267.807568	52.072218
3312.365006	396926.664157	52.077223
3311.760602	396593.670857	52.082228
3310.968745	396275.296781	52.087233
3310.441152	395939.869686	52.092237
3309.738769	395621.907508	52.097242
3308.880401	395281.594036	52.102247
3308.368198	394959.375230	52.107252
3307.264113	394630.712933	52.112257
3306.610884	394313.213846	52.117261
3305.976352	393986.276262	52.122266
3305.408352	393659.248777	52.127271
3305.188621	393343.960456	52.132276
3304.206967	393019.306040	52.137281
3303.843876	392686.465372	52.142285
3302.839705	392361.960935	52.147290
3302.326136	392038.723487	52.152295
3301.803690	391696.211185	52.157300
3300.828569	391365.488858	52.162305
3300.526590	391045.819407	52.167309
3299.612141	390717.598680	52.172314
3299.030620	390386.576098	52.177319
3298.260561	390068.700925	52.182324
3297.437141	389742.313011	52.187329
3296.809783	389397.684568	52.192333
3296.057751	389089.028242	52.197338
3295.448624	388763.996089	52.202343
3294.917620	388443.958126	52.207348
3294.181089	388121.279786	52.212353
3294.100955	387782.092885	52.217357
3293.130365	387477.983781	52.222362
3292.776240	387132.273354	52.227367
3291.672231	386801.249624	52.232372
3291.054620	386469.611948	52.237377
3290.203900	386131.192799	52.242381
3289.599595	385812.135159	52.247386
3289.066851	385487.239784	52.252391
3288.691428	385165.648159	52.257396
3287.658176	384835.104251	52.262401
3287.121477	384505.521579	52.267405
3286.144030	384174.149196	52.272410
3285.750365	383848.124007	52.277415
3285.379596	383522.651886	52.282420
3284.211066	383190.716138	52.287425
3283.708238	382864.598006	52.292429
3283.068188	382536.209824	52.297434
3282.071651	382197.956297	52.302439
3281.631960	381879.398819	52.307444
3280.841651	381565.370448	52.312449
3280.049038	381234.706233	52.317453
3279.101258	380915.127489	52.322458
3278.804340	380592.340207	52.327463
3277.826509	380264.825410	52.332468
3276.959933	379943.063912	52.337473
3276.630210	379630.981811	52.342477
3275.669039	379312.867270	52.347482
3275.111374	379001.324920	52.352487
3274.739971	378683.188326	52.357492
3273.850238	378371.388309	52.362497
3273.166239	378050.549039	52.367501
3272.239427	377728.880767	52.372506
3272.226875	377411.974490	52.377511
3271.242557	377093.133621	52.382516
3270.788648	376777.335036	52.387521
3269.936687	376449.260092	52.392525
3269.336973	376133.530412	52.397530
3268.510047	375812.848524	52.402535
3267.816985	375508.321119	52.407540
3267.331704	375187.860095	52.412545
3266.957554	374857.585444	52.417549
3265.917300	374546.186729	52.422554
3265.111840	374228.261793	52.427559
3264.771872	373915.424781	52.432564
3263.910042	373602.388129	52.437569
3263.432469	373279.723380	52.442573
3262.288303	372965.378352	52.447578
3261.996096	372648.148791	52.452583
3261.236073	372333.789158	52.457588
3260.572530	371999.721734	52.462593
3260.001031	371676.576200	52.467597
3259.493879	371369.190777	52.472602
3258.976113	371048.321568	52.477607
3258.390721	370721.075138	52.482612
3257.179419	370413.539822	52.487617
3256.766080	370087.355298	52.492621
3256.044105	369765.745602	52.497626
3255.380585	369449.950274	52.502631
3255.245933	369128.090317	52.507636
3253.918419	368801.659119	52.512641
3253.455535	368478.218049	52.517645
3252.513516	368172.964935	52.522650
3251.881615	367835.094944	52.527655
3251.591586	367536.654529	52.532660
3250.777031	367210.054096	52.537665
3249.969396	366878.641540	52.542669
3248.955871	366567.282504	52.547674
3248.625404	366254.006824	52.552679
3248.124574	365923.938055	52.557684
3247.371152	365619.884376	52.562689
3246.772907	365297.764742	52.567693
3246.094506	364978.199868	52.572698
3245.580836	364651.253456	52.577703
3245.203135	364338.480930	52.582708
3244.005339	364015.760127	52.587713
3243.140699	363701.609990	52.592717
3242.502811	363384.241301	52.597722
3242.286731	363061.256797	52.602727
3241.622972	362746.610438	52.607732
3240.581668	362424.006516	52.612737
3240.165482	362093.464394	52.617741
3239.252435	361791.064758	52.622746
3238.523220	361459.880702	52.627751
3238.314706	361148.103369	52.632756
3237.082364	360831.931143	52.637761
3236.603172	360506.299014	52.642765
3235.853461	360187.959636	52.647770
3235.506398	359871.615625	52.652775
3234.810716	359541.252772	52.657780
3234.045378	359252.275000	52.662785
3233.533037	358912.107364	52.667789
3232.594022	358605.747603	52.672794
3232.097865	358275.039284	52.677799
3231.367319	357965.461675	52.682804
3230.429993	357645.252343	52.687809
3229.547071	357344.525253	52.692813
3229.311237	357012.545875	52.697818
3228.667344	356709.461413	52.702823
3228.125680	356387.985408	52.707828
3227.301186	356070.471137	52.712833
3226.937324	355751.965874	52.717837
3226.034252	355435.274422	52.722842
3225.274759	355124.971390	52.727847
3224.811394	354794.336850	52.732852
3223.746882	354488.302754	52.737857
3223.147351	354164.607878	52.742861
3222.684385	353864.837264	52.747866
3222.005429	353537.588147	52.752871
3221.021243	353220.590601	52.757876
3220.692636	352912.242194	52.762881
3220.470890	352591.048287	52.767885
3219.324208	352277.506544	52.772890
3218.612562	351960.203849	52.777895
3218.260038	351647.856204	52.782900
3216.866866	351324.167691	52.787905
3216.625979	351009.355430	52.792909
3215.867572	350706.330618	52.797914
3215.199530	350378.347808	52.802919
3214.870444	350070.135892	52.807924
3213.522821	349755.491472	52.812929
3213.051966	349436.939744	52.817933
3212.426285	349140.400876	52.822938
3212.169558	348820.055574	52.827943
3211.179256	348504.304016	52.832948
3210.458552	348183.214007	52.837953
3209.754354	347867.311806	52.842957
3209.036866	347565.892320	52.847962
3208.492143	347261.822303	52.852967
3208.073536	346938.361286	52.857972
3206.990675	346633.991272	52.862977
3206.667399	346313.260553	52.867981
3206.058021	345996.493081	52.872986
3204.866985	345697.582200	52.877991
3204.649888	345372.578818	52.882996
3204.134084	345063.096575	52.888001
3203.709909	344748.736580	52.893005
3202.422847	344440.034871	52.898010
3201.868411	344119.303270	52.903015
3201.276915	343794.986799	52.908020
3200.540553	343490.825689	52.913025
3199.779519	343183.179717	52.918029
3198.844967	342861.127010	52.923034
3198.390419	342550.069370	52.928039
3197.905416	342244.284072	52.933044
3197.215303	341938.631518	52.938049
3196.616633	341623.977414	52.943053
3196.265961	341309.613395	52.948058
3195.529300	340982.072181	52.953063
3194.642081	340675.146384	52.958068
3193.909957	340365.903568	52.963073
3193.604703	340041.852966	52.968077
3192.713771	339724.231820	52.973082
3191.939659	339413.234570	52.978087
3191.370909	339101.719662	52.983092
3190.921518	338787.944237	52.988097
3190.474932	338459.860498	52.993101
3189.379118	338150.893646	52.998106
3188.935629	337842.025789	53.003111
3188.450728	337513.536066	53.008116
3187.209922	337198.554486	53.013121
3186.426930	336881.589730	53.018125
3186.001807	336560.010075	53.023130
3185.436469	336251.561416	53.028135
3184.250274	335948.835588	53.033140
3183.931084	335630.875115	53.038145
3183.295620	335306.089712	53.043149
3182.522888	335004.439863	53.048154
3182.000774	334677.062354	53.053159
3181.714337	334375.511031	53.058164
3180.570407	334058.488430	53.063169
3180.265519	333733.974315	53.068173
3179.464888	333424.964704	53.073178
3178.752867	333106.825710	53.078183
3177.662749	332795.084218	53.083188
3177.090407	332482.241120	53.088193
3176.610771	332168.516408	53.093197
3176.076352	331859.839805	53.098202
3175.049010	331554.880469	53.103207
3174.841643	331228.506579	53.108212
3173.967213	330932.049165	53.113217
3173.409890	330609.063019	53.118221
3172.512509	330288.929777	53.123226
3172.167353	329986.503805	53.128231
3171.418931	329658.222813	53.133236
3170.390481	329349.359343	53.138241
3170.278540	329036.225174	53.143245
3169.328588	328722.865873	53.148250
3168.400527	328419.100163	53.153255
3168.226375	328102.789579	53.158260
3167.431297	327791.184202	53.163265
3166.706469	327467.447485	53.168269
3166.176036	327159.744051	53.173274
3165.394989	326837.592185	53.178279
3164.811983	326529.716415	53.183284
3163.972497	326223.203989	53.188289
3163.624062	325905.690133	53.193293
3162.422946	325587.622507	53.198298
3161.729680	325284.647908	53.203303
3161.537456	324965.578052	53.208308
3160.733709	324664.680992	53.213313
3160.127679	324341.447699	53.218317
3159.395993	324032.593124	53.223322
3158.717057	323716.116170	53.228327
3158.147799	323411.994888	53.233332
3157.490741	323094.442795	53.238337
3156.888742	322780.852818	53.243341
3156.156345	322469.344729	53.248346
3155.131860	322148.435457	53.253351
3155.035165	321837.410167	53.258356
3153.678776	321526.583089	53.263361
3153.129102	321211.069604	53.268365
3152.623195	320915.994107	53.273370
3151.885425	320594.448259	53.278375
3151.292731	320286.933467	53.283380
3150.510853	319972.521831	53.288385
3149.986654	319659.927111	53.293389
3149.382943	319345.867097	53.298394
3148.904599	319042.378620	53.303399
3148.203279	318718.452484	53.308404
3147.478203	318412.301986	53.313409
3146.876872	318095.920346	53.318413
3146.023031	317793.174804	53.323418
3145.397375	317469.665359	53.328423
3144.687623	317161.700614	53.333428
3143.848979	316868.014654	53.338433
3143.530998	316534.675622	53.343437
3142.586890	316238.636418	53.348442
3141.791107	315925.919837	53.353447
3141.431738	315611.936464	53.358452
3140.301056	315302.581210	53.363457
3140.018904	314999.202038	53.368461
3139.594126	314685.659081	53.373466
3139.110389	314370.316590	53.378471
3138.079363	314055.823667	53.383476
3137.353289	313748.793418	53.388481
3136.922047	313436.266353	53.393485
3135.974144	313116.537419	53.398490
3135.436463	312805.655085	53.403495
3134.761725	312498.180298	53.408500
3134.293804	312188.456546	53.413505
3133.656259	311861.723143	53.418509
3132.955397	311558.655244	53.423514
3132.073256	311239.903646	53.428519
3131.697393	310918.932039	53.433524
3130.908515	310620.408286	53.438529
3130.203740	310280.566763	53.443533
3129.724087	309982.374436	53.448538
3128.852837	309674.821347	53.453543
3128.382067	309361.296255	53.458548
3127.867802	309050.833030	53.463553
3127.130245	308729.276145	53.468557
3126.390252	308413.932288	53.473562
3125.389950	308092.058820	53.478567
3125.334247	307774.975318	53.483572
3124.262922	307465.207468	53.488577
3123.795494	307142.890778	53.493581
3123.230683	306834.900244	53.498586
3122.130045	306509.880995	53.503591
3121.800964	306196.656724	53.508596
3121.299768	305870.853502	53.513601
3120.498515	305548.483904	53.518605
3119.666625	305245.523249	53.523610
3118.950389	304916.899631	53.528615
3118.863816	304603.251363	53.533620
3117.773535	304278.327051	53.538625
3117.358896	303959.661572	53.543629
3116.477057	303641.935163	53.548634
3115.614805	303320.308663	53.553639
3115.096322	303003.160032	53.558644
3114.345341	302691.420875	53.563649
3113.770562	302365.952388	53.568653
3112.644894	302057.658227	53.573658
3112.224273	301745.584746	53.578663
3111.595894	301423.433385	53.583668
3111.082569	301111.704386	53.588673
3110.489138	300803.221697	53.593677
3109.873183	300483.001940	53.598682
3109.128306	300159.567713	53.603687
3108.506439	299850.833082	53.608692
3107.809799	299541.040123	53.613697
3107.378723	299202.121637	53.618701
3106.302147	298898.728852	53.623706
3105.888018	298565.561935	53.628711
3105.366896	298244.966471	53.633716
3104.291212	297944.653414	53.638721
3103.713942	297613.013110	53.643725
3102.480010	297311.221522	53.648730
3102.184261	296994.128140	53.653735
3101.969129	296676.155600	53.658740
3101.071356	296362.059690	53.663745
3100.323004	296050.282612	53.668749
3099.672717	295728.786550	53.673754
3098.852126	295412.130231	53.678759
3098.353213	295106.959181	53.683764
3097.823591	294789.262656	53.688769
3096.926885	294469.841039	53.693773
3096.430106	294145.746080	53.698778
3095.773306	293838.560841	53.703783
3095.242487	293527.102192	53.708788
3094.484380	293215.730023	53.713793
3093.936341	292893.933467	53.718797
3093.430858	292573.632327	53.723802
3092.279495	292259.392376	53.728807
3091.702460	291931.919874	53.733812
3090.904624	291631.783164	53.738817
3090.225305	291306.006906	53.743821
3089.676226	291002.162765	53.748826
3088.736727	290682.360881	53.753831
3088.307433	290363.522063	53.758836
3087.590366	290054.762715	53.763841
3086.875290	289748.651369	53.768845
3086.274646	289431.876050	53.773850
3085.809341	289124.272867	53.778855
3085.188079	288810.479896	53.783860
3084.655376	288495.068120	53.788865
3083.983337	288175.297602	53.793869
3083.327128	287866.730161	53.798874
3082.519081	287540.715446	53.803879
3082.050516	287231.175423	53.808884
3081.141130	286915.490698	53.813889
3080.396303	286584.804460	53.818893
3079.668993	286273.445409	53.823898
3078.738119	285957.686878	53.828903
3078.323564	285655.548223	53.833908
3077.630059	285343.877482	53.838913
3077.073082	285018.202908	53.843917
3076.376287	284708.391406	53.848922
3075.722557	284398.038046	53.853927
3075.632203	284078.350380	53.858932
3074.608937	283765.075316	53.863937
3073.772376	283442.805705	53.868941
3073.294127	283127.915915	53.873946
3072.425092	282810.897522	53.878951
3071.976636	282494.219889	53.883956
3071.205071	282189.716118	53.888961
3070.591371	281863.997613	53.893965
3069.789176	281547.502831	53.898970
3068.820388	281228.411038	53.903975
3068.555523	280917.510377	53.908980
3067.372430	280605.939923	53.913985
3067.173892	280295.053997	53.918989
3066.655601	279981.850011	53.923994
3065.673678	279670.145524	53.928999
3065.025824	279353.523620	53.934004
3064.681715	279045.258117	53.939009
3064.051058	278725.831805	53.944013
3063.352212	278406.721831	53.949018
3062.571490	278084.797759	53.954023
3061.738111	277764.155380	53.959028
3061.060182	277462.997131	53.964033
3060.699001	277146.711432	53.969037
3059.866698	276828.233572	53.974042
3059.128694	276520.768574	53.979047
3058.757012	276202.192303	53.984052
3057.968537	275887.680519	53.989057
3057.204900	275553.757888	53.994061
3056.777928	275236.692992	53.999066
3055.960261	274913.679402	54.004071
3055.755744	274593.701407	54.009076
3054.475824	274279.598554	54.014081
3053.866060	273953.750626	54.019085
3053.525284	273634.863978	54.024090
3052.752630	273321.572370	54.029095
3052.141607	273000.793009	54.034100
3051.296336	272678.217068	54.039105
3050.838944	272362.074249	54.044109
3050.115510	272043.324909	54.049114
3049.390956	271718.743589	54.054119
3049.052757	271392.216570	54.059124
3047.872630	271083.421524	54.064129
3047.460561	270761.439785	54.069133
3046.728341	270447.251206	54.074138
3045.770227	270129.303731	54.079143
3044.957415	269800.967808	54.084148
3044.430076	269493.521780	54.089153
3043.789760	269171.373123	54.094157
3043.320579	268859.970616	54.099162
3042.570540	268545.199981	54.104167
3041.985872	268224.163634	54.109172
3041.030854	267922.949416	54.114177
3040.251673	267604.007153	54.119181
3039.889448	267298.879254	54.124186
3039.549750	266985.368960	54.129191
3038.825752	266660.077017	54.134196
3037.864848	266347.735139	54.139201
3037.110884	266028.306071	54.144205
3036.587024	265713.781634	54.149210
3036.139019	265417.455097	54.154215
3035.732628	265083.200285	54.159220
3034.997138	264765.322850	54.164225
3034.324631	264449.982517	54.169229
3033.559534	264127.373274	54.174234
3032.484791	263797.962458	54.179239
3032.322197	263485.547503	54.184244
3031.840917	263173.743574	54.189249
3030.972974	262848.757848	54.194253
3030.184647	262536.901264	54.199258
3029.635858	262211.865686	54.204263
3029.464376	261875.259298	54.209268
3028.402155	261553.947595	54.214273
3027.607535	261230.938493	54.219277
3027.223283	260897.117439	54.224282
3026.219008	260577.835096	54.229287
3025.681285	260267.469367	54.234292
3024.865594	259948.794620	54.239297
3024.436193	259630.033659	54.244301
3023.782069	259308.940184	54.249306
3022.561944	258990.890940	54.254311
3022.501374	258653.914514	54.259316
3021.333574	258347.649281	54.264321
3021.102805	258018.035322	54.269325
3020.130646	257692.257418	54.274330
3019.444387	257379.091998	54.279335
3019.060777	257055.666728	54.284340
3018.368436	256748.589853	54.289345
3018.093749	256418.985213	54.294349
3017.210631	256095.844186	54.299354
3016.257692	255769.887859	54.304359
3015.723450	255446.183288	54.309364
3015.154435	255136.873634	54.314369
3014.313139	254809.424102	54.319373
3013.652233	254489.306526	54.324378
3013.073307	254166.782614	54.329383
3012.175728	253832.976919	54.334388
3011.653200	253519.817009	54.339393
3010.993978	253209.735285	54.344397
3010.442966	252878.219415	54.349402
3009.552317	252557.810474	54.354407
3009.322534	252229.912177	54.359412
3008.712143	251905.512736	54.364417
3007.586527	251593.343017	54.369421
3006.895179	251270.460129	54.374426
3005.932230	250947.900986	54.379431
3005.584128	250629.166984	54.384436
3004.956509	250315.214596	54.389441
3004.141367	249990.341983	54.394445
3003.500049	249680.212961	54.399450
3002.570761	249354.417474	54.404455
3002.107284	249044.159703	54.409460
3001.704929	248732.950640	54.414465
3000.996847	248412.266301	54.419469
3000.305365	248096.571360	54.424474
2999.531508	247770.729217	54.429479
2999.433017	247447.352954	54.434484
2998.381124	247135.384229	54.439489
2997.754111	246802.390591	54.444493
2997.147424	246480.039194	54.449498
2996.377795	246171.058342	54.454503
2996.070684	245843.644266	54.459508
2995.312742	245526.386692	54.464513
2994.625676	245194.654247	54.469517
2993.920460	244867.203689	54.474522
2993.163702	244545.670064	54.479527
2992.664452	244221.906451	54.484532
2991.901180	243899.586027	54.489537
2991.235198	243577.378339	54.494541
2990.398713	243257.413921	54.499546
2989.674743	242943.365862	54.504551
2989.393932	242616.948862	54.509556
2988.666044	242293.786609	54.514561
2987.817077	241953.226428	54.519565
2987.402283	241637.757668	54.524570
2986.760234	241313.234814	54.529575
2985.905738	240989.866920	54.534580
2985.367071	240671.288188	54.539585
2984.342882	240341.430021	54.544589
2983.800990	240019.594136	54.549594
2983.153611	239709.463990	54.554599
2982.423816	239382.363066	54.559604
2981.735403	239050.316489	54.564609
2981.111073	238734.786975	54.569613
2980.356351	238420.373957	54.574618
2979.877185	238097.056759	54.579623
2979.541790	237772.444570	54.584628
2978.743532	237443.679635	54.589633
2977.946969	237120.517469	54.594637
2977.265160	236799.859028	54.599642
2976.449914	236467.993248	54.604647
2976.112216	236151.916697	54.609652
2975.495970	235829.850374	54.614657
2974.508813	235496.767223	54.619661
2974.058746	235176.484556	54.624666
2973.206065	234854.942556	54.629671
2972.979220	234529.712224	54.634676
2972.153093	234210.001447	54.639681
2971.202801	233870.068333	54.644685
2970.670882	233545.806213	54.649690
2969.608818	233227.765627	54.654695
2969.529869	232906.285779	54.659700
2968.436486	232586.138881	54.664705
2967.897454	232265.777998	54.669709
2967.245911	231949.586393	54.674714
2966.474631	231622.160464	54.679719
2965.962802	231305.159602	54.684724
2965.223961	230984.452833	54.689729
2964.551570	230663.482051	54.694733
2963.977908	230334.756337	54.699738
2963.208157	230020.117824	54.704743
2962.461178	229692.949613	54.709748
2961.895664	229369.471290	54.714753
2961.665405	229051.364403	54.719757
2960.593172	228725.040587	54.724762
2959.940565	228403.642004	54.729767
2959.845027	228082.232814	54.734772
2958.613625	227761.157412	54.739777
2957.866375	227427.556087	54.744781
2957.484806	227109.060228	54.749786
2956.700686	226786.784703	54.754791
2955.978159	226453.399752	54.759796
2955.203755	226144.033819	54.764801
2954.821086	225807.771530	54.769805
2954.127037	225485.856001	54.774810
2953.377888	225163.975929	54.779815
2952.833017	224842.574009	54.784820
2952.072309	224519.399869	54.789825
2951.460737	224196.165238	54.794829
2950.588447	223870.770910	54.799834
2950.085470	223548.667438	54.804839
2949.456574	223220.958611	54.809844
2948.718477	222906.863928	54.814849
2948.386358	222580.027375	54.819853
2947.402393	222247.567024	54.824858
2946.887976	221929.023709	54.829863
2946.502673	221593.683638	54.834868
2945.544892	221269.268554	54.839873
2945.066667	220946.102824	54.844877
2944.464907	220622.512522	54.849882
2943.672092	220286.606354	54.854887
2943.229334	219959.289527	54.859892
2942.531030	219642.707227	54.864897
2942.151559	219296.684020	54.869901
2940.855057	218961.652904	54.874906
2940.042070	218636.908302	54.879911
2940.144829	218301.862409	54.884916
2939.062872	217973.077386	54.889921
2938.296206	217644.053042	54.894925
2937.643028	217326.290059	54.899930
2936.899837	216989.322252	54.904935
2936.342879	216666.951938	54.909940
2935.694936	216346.926884	54.914945
2935.256313	216002.749408	54.919949
2934.725070	215675.313676	54.924954
2933.368974	215353.559742	54.929959
2933.344352	215018.919004	54.934964
2932.528528	214688.541918	54.939969
2931.839827	214348.129146	54.944973
2931.137015	214017.813861	54.949978
2930.594010	213690.046020	54.954983
2930.032175	213354.429535	54.959988
2929.050237	213034.880465	54.964993
2928.284694	212698.014070	54.969997
2927.673512	212371.943738	54.975002
2926.821326	212048.433332	54.980007
2926.307751	211709.368475	54.985012
2925.484069	211398.521016	54.990017
2925.089146	211069.775714	54.995021
2924.451382	210746.377986	55.000026
2923.370698	210415.937348	55.005031
2922.919327	210081.147844	55.010036
2922.468846	209766.342040	55.015041
2921.519246	209441.829529	55.020045
2920.818860	209114.237451	55.025050
2920.153097	208788.143453	55.030055
2919.694222	208462.871163	55.035060
2918.833686	208132.051569	55.040065
2917.972190	207813.362777	55.045069
2917.551265	207494.593195	55.050074
2916.681129	207165.804023	55.055079
2916.591968	206844.949084	55.060084
2915.514798	206520.612464	55.065089
2915.059481	206186.226924	55.070093
2914.610786	205854.985706	55.075098
2913.595914	205537.911537	55.080103
2912.973886	205213.382832	55.085108
2912.207164	204881.026683	55.090113
2911.500550	204559.849354	55.095117
2910.860857	204239.528612	55.100122
2910.396930	203913.213269	55.105127
2909.711698	203577.224836	55.110132
2909.029439	203263.712063	55.115137
2908.592258	202938.288929	55.120141
2907.781613	202608.561843	55.125146
2906.812195	202287.960784	55.130151
2906.186268	201956.872102	55.135156
2905.540088	201631.387890	55.140161
2904.914639	201321.542040	55.145165
2904.277093	200991.771733	55.150170
2903.647144	200668.059512	55.155175
2903.600912	200324.863381	55.160180
2902.621799	200017.765989	55.165185
2902.158289	199677.096018	55.170189
2901.372486	199342.434588	55.175194
2900.472661	199022.490712	55.180199
2900.211025	198696.466988	55.185204
2899.379141	198355.761986	55.190209
2898.559927	198025.975047	55.195213
2897.972359	197698.952937	55.200218
2896.859570	197374.344640	55.205223
2896.672518	197048.230263	55.210228
2895.815936	196719.908094	55.215233
2895.041158	196391.206053	55.220237
2894.427090	196069.249998	55.225242
2893.731991	195738.999877	55.230247
2893.241298	195405.105873	55.235252
2892.453411	195088.145948	55.240257
2892.135879	194750.284379	55.245261
2891.025072	194429.677043	55.250266
2890.511913	194109.778725	55.255271
2890.249633	193775.388571	55.260276
2889.646816	193442.085198	55.265281
2888.892860	193108.884338	55.270285
2888.274849	192776.669356	55.275290
2887.302810	192445.301525	55.280295
2886.920396	192109.834735	55.285300
2886.128242	191788.138031	55.290305
2885.409657	191453.441493	55.295309
2884.657668	191112.925407	55.300314
2883.758095	190795.985278	55.305319
2883.741375	190459.568689	55.310324
2882.611587	190133.381704	55.315329
2882.172029	189801.756852	55.320333
2881.486096	189461.534684	55.325338
2880.510215	189135.470137	55.330343
2879.919888	188801.535231	55.335348
2879.623404	188476.398193	55.340353
2878.925389	188140.716647	55.345357
2878.272806	187808.948748	55.350362
2877.648470	187482.674678	55.355367
2877.342312	187140.857173	55.360372
2876.070392	186806.904584	55.365377
2875.305590	186479.654838	55.370381
2874.662251	186145.836531	55.375386
2873.969585	185814.025774	55.380391
2873.366845	185477.025553	55.385396
2872.402517	185154.905544	55.390401
2872.177984	184821.755803	55.395405
2871.377638	184494.487871	55.400410
2869.998751	184172.237025	55.405415
2869.952957	183840.414734	55.410420
2869.412800	183525.261315	55.415425
2868.603589	183192.025531	55.420429
2868.561998	182857.602172	55.425434
2867.790695	182525.255889	55.430439
2866.670709	182197.673953	55.435444
2865.876591	181866.061373	55.440449
2865.701101	181533.882711	55.445453
2864.947171	181205.347148	55.450458
2863.597585	180883.357541	55.455463
2863.378373	180549.094555	55.460468
2862.338795	180230.800458	55.465473
2861.828756	179898.305808	55.470477
2861.516423	179566.583796	55.475482
2860.953115	179252.737122	55.480487
2860.141684	178914.205185	55.485492
2859.766864	178593.159723	55.490497
2859.102576	178248.631685	55.495501
2858.351261	177917.475513	55.500506
2857.385852	177594.725099	55.505511
2856.942403	177252.294430	55.510516
2856.325806	176929.582992	55.515521
2855.563863	176597.637748	55.520525
2854.988939	176263.210845	55.525530
2854.480753	175935.504280	55.530535
2853.790970	175597.069191	55.535540
2852.928692	175268.597352	55.540545
2852.157618	174926.708578	55.545549
2851.665269	174594.469865	55.550554
2850.744804	174270.810128	55.555559
2850.409861	173928.288442	55.560564
2849.498143	173601.427777	55.565569
2848.977746	173274.724024	55.570573
2848.244601	172946.886613	55.575578
2847.478244	172611.706386	55.580583
2846.979698	172271.348716	55.585588
2845.775701	171951.695182	55.590593
2845.589090	171617.042045	55.595597
2844.930165	171294.649635	55.600602
2843.975563	170965.770129	55.605607
2843.509799	170637.210218	55.610612
2842.861319	170309.673941	55.615617
2842.102239	169972.315180	55.620621
2841.629344	169643.294325	55.625626
2841.047446	169249.375645	55.630631
2840.618168	168941.412473	55.635636
2839.468949	168590.915292	55.640641
2838.559241	168278.099641	55.645645
2838.500620	167936.362563	55.650650
2838.048283	167599.421264	55.655655
2837.305640	167271.074009	55.660660
2836.786309	166933.475343	55.665665
2835.677035	166613.418996	55.670669
2835.310288	166257.771499	55.675674
2834.401292	165921.375376	55.680679
2834.058955	165602.719398	55.685684
2833.184848	165255.477657	55.690689
2832.557350	164957.699859	55.695693
2832.253278	164593.615628	55.700698
2830.984425	164266.586216	55.705703
2830.353108	163925.726879	55.710708
2830.108308	163577.155334	55.715713
2829.347126	163271.987125	55.720717
2828.675836	162909.605328	55.725722
2827.597701	162575.733334	55.730727
2827.302945	162250.220694	55.735732
2826.555356	161915.717634	55.740737
2825.879795	161569.242532	55.745741
2825.455392	161234.592955	55.750746
2824.142402	160916.284434	55.755751
2823.780933	160577.804270	55.760756
2822.968675	160243.556020	55.765761
2822.230986	159902.255970	55.770765
2821.169643	159604.476805	55.775770
2820.724247	159240.253196	55.780775
2820.403774	158928.683216	55.785780
2819.702570	158603.586322	55.790785
2819.112592	158265.406210	55.795789
2818.275185	157953.659870	55.800794
2817.958456	157602.590549	55.805799
2816.697980	157290.103610	55.810804
2816.635916	156937.373563	55.815809
2815.713313	156629.402808	55.820813
2815.533022	156275.312688	55.825818
2814.220813	155971.693500	55.830823
2813.972529	155605.316062	55.835828
2813.340241	155309.997545	55.840833
2812.158636	154960.198280	55.845837
2811.925839	154594.185267	55.850842
2810.807239	154303.744756	55.855847
2810.063106	153984.901718	55.860852
2809.700309	153628.491287	55.865857
2808.496634	153337.894691	55.870861
2808.139748	152989.459860	55.875866
2807.658820	152678.569970	55.880871
2807.420496	152314.692807	55.885876
2806.606852	152030.401139	55.890881
2805.850257	151666.575087	55.895885
2805.129553	151358.671683	55.900890
2804.729916	150997.961330	55.905895
2804.065910	150685.632230	55.910900
2803.022300	150346.256483	55.915905
2802.344780	150015.570476	55.920909
2801.971696	149699.874883	55.925914
2800.817135	149355.062047	55.930919
2799.789878	149038.586888	55.935924
2799.399363	148702.950438	55.940929
2798.784801	148399.735291	55.945933
2798.364710	148066.308845	55.950938
2797.363603	147755.370560	55.955943
2797.197444	147433.233942	55.960948
2796.413487	147082.795180	55.965953
2795.967150	146784.143817	55.970957
2795.280667	146421.382644	55.975962
2794.217202	146126.025002	55.980967
2794.184635	145771.300884	55.985972
2793.654459	145435.530562	55.990977
2792.239015	145130.249797	55.995981
2792.086424	144788.835289	56.000986
2791.160544	144457.382478	56.005991
2790.900792	144134.849812	56.010996
2789.784687	143807.170009	56.016001
2789.149146	143465.046049	56.021005
2788.578490	143125.495094	56.026010
2787.277185	142814.678978	56.031015
2787.125027	142480.151548	56.036020
2786.622878	142158.376881	56.041025
2785.766198	141819.902244	56.046029
2785.105222	141486.914825	56.051034
2784.237119	141159.503669	56.056039
2783.872181	140827.848856	56.061044
2783.122780	140511.073409	56.066049
2782.522305	140182.309085	56.071053
2781.998991	139853.802956	56.076058
2781.064017	139527.512825	56.081063
2780.722057	139201.792999	56.086068
2779.629116	138871.151805	56.091073
2779.264544	138544.616931	56.096077
2778.707540	138222.080002	56.101082
2777.942239	137891.245388	56.106087
2777.577984	137557.352718	56.111092
2776.420515	137236.827335	56.116097
2775.961084	136904.939020	56.121101
2775.517296	136566.268054	56.126106
2774.642508	136242.863084	56.131111
2773.951293	135912.598031	56.136116
2773.311281	135579.940349	56.141121
2772.688296	135254.067410	56.146125
2771.857137	134922.235170	56.151130
2771.472991	134595.976128	56.156135
2770.930111	134260.891943	56.161140
2770.057193	133935.975401	56.166145
2769.326202	133602.135474	56.171149
2769.067931	133273.115046	56.176154
2767.988026	132951.748375	56.181159
2767.474247	132603.303378	56.186164
2766.883785	132266.433706	56.191169
2766.086640	131934.516429	56.196173
2765.192207	131611.573229	56.201178
2764.440143	131291.557961	56.206183
2764.014637	130957.865889	56.211188
2763.281884	130635.543359	56.216193
2762.962855	130301.524697	56.221197
2762.252252	129966.327349	56.226202
2761.293877	129640.724358	56.231207
2760.771797	129304.298531	56.236212
2760.214462	128977.445919	56.241217
2759.471501	128643.704823	56.246221
2759.103165	128312.384976	56.251226
2758.170958	127980.383721	56.256231
2757.413252	127653.349930	56.261236
2756.751816	127325.784095	56.266241
2756.226954	126989.234567	56.271245
2755.473041	126658.986337	56.276250
2754.449447	126335.845682	56.281255
2753.971901	126000.913685	56.286260
2753.360719	125671.785068	56.291265
2752.835675	125343.688118	56.296269
2752.102748	125021.774284	56.301274
2751.122778	124689.592158	56.306279
2750.854173	124357.555421	56.311284
2749.744467	124038.443212	56.316289
2749.253511	123715.732105	56.321293
2748.883649	123387.431295	56.326298
2748.046897	123058.776759	56.331303
2747.768732	122720.578033	56.336308
2746.479524	122392.270067	56.341313
2745.988631	122068.867868	56.346317
2745.175963	121741.343218	56.351322
2744.263127	121423.424775	56.356327
2743.757958	121094.742115	56.361332
2743.115408	120778.807458	56.366337
2742.332140	120453.122535	56.371341
2742.126670	120124.442659	56.376346
2741.056612	119808.669973	56.381351
2740.222979	119484.795289	56.386356
2739.823888	119159.516384	56.391361
2738.947716	118853.767090	56.396365
2738.552230	118523.036412	56.401370
2737.909727	118197.071817	56.406375
2737.469098	117889.030548	56.411380
2736.615913	117564.770421	56.416385
2736.136654	117238.239879	56.421389
2735.507948	116909.560010	56.426394
2734.809288	116586.049488	56.431399
2734.093479	116262.228424	56.436404
2733.412544	115920.646558	56.441409
2732.372606	115606.983543	56.446413
2732.065881	115273.335759	56.451418
2731.500480	114953.994903	56.456423
2730.802187	114617.453792	56.461428
2730.286944	114304.168112	56.466433
2729.580976	113975.513142	56.471437
2729.101880	113655.064428	56.476442
2728.250200	113328.021337	56.481447
2727.321387	112996.368196	56.486452
2726.823075	112671.867071	56.491457
2726.283085	112337.876414	56.496461
2725.615131	112021.184837	56.501466
2724.629218	111693.429302	56.506471
2724.296493	111363.537563	56.511476
2723.526982	111041.061674	56.516481
2722.722255	110721.857354	56.521485
2722.349293	110395.335564	56.526490
2721.500069	110076.565502	56.531495
2720.967041	109733.959842	56.536500
2720.446284	109409.714604	56.541505
2719.489461	109092.446587	56.546509
2719.223333	108756.240299	56.551514
2718.329533	108435.550731	56.556519
2717.552228	108099.916757	56.561524
2716.967885	107772.486446	56.566529
2716.302125	107443.189007	56.571533
2715.517131	107109.841526	56.576538
2715.171800	106782.837284	56.581543
2714.369887	106456.982090	56.586548
2713.493835	106134.518430	56.591553
2712.911956	105808.408802	56.596557
2712.397914	105473.442336	56.601562
2711.414259	105158.761864	56.606567
2710.755854	104821.518089	56.611572
2710.265806	104497.803679	56.616577
2709.190371	104182.592408	56.621581
2708.916454	103838.221675	56.626586
2708.182807	103531.110704	56.631591
2707.512091	103215.689641	56.636596
2706.857981	102880.750357	56.641601
2706.323021	102556.251386	56.646605
2705.522078	102225.290513	56.651610
2704.426761	101918.372149	56.656615
2704.131555	101581.872164	56.661620
2703.502860	101268.570382	56.666625
2702.633660	100945.275897	56.671629
2702.306004	100620.390450	56.676634
2701.253101	100298.726229	56.681639
2700.734252	99975.542020	56.686644
2699.776968	99669.925527	56.691649
2699.817024	99337.610395	56.696653
2699.093991	99022.673173	56.701658
2698.099908	98704.599215	56.706663
2697.786801	98370.850836	56.711668
2697.210224	98043.764253	56.716673
2696.348992	97733.534730	56.721677
2695.429653	97388.651756	56.726682
2695.013889	97067.724754	56.731687
2694.289917	96760.531022	56.736692
2693.594077	96418.234001	56.741697
2693.013790	96096.814103	56.746701
2692.203328	95781.713656	56.751706
2691.786792	95464.487804	56.756711
2690.748469	95132.183055	56.761716
2689.863266	94815.795279	56.766721
2689.420078	94499.532189	56.771725
2688.880878	94161.601312	56.776730
2688.132222	93841.178937	56.781735
2687.386042	93532.663182	56.786740
2686.803681	93221.963441	56.791745
2686.263173	92899.188146	56.796749
2685.661474	92572.730499	56.801754
2684.450860	92256.189733	56.806759
2684.118247	91924.550288	56.811764
2683.943564	91608.399994	56.816769
2683.103015	91290.184936	56.821773
2682.495125	90966.256589	56.826778
2681.476215	90654.146830	56.831783
2681.145627	90335.738029	56.836788
2680.397151	90008.257554	56.841793
2679.779578	89674.617729	56.846797
2679.364914	89356.540874	56.851802
2678.415855	89043.809114	56.856807
2677.865705	88703.180633	56.861812
2677.507861	88379.149713	56.866817
2676.455918	88040.811045	56.871821
2675.726215	87727.512025	56.876826
2675.016589	87395.069377	56.881831
2674.092473	87078.412698	56.886836
2673.607235	86754.020706	56.891841
2673.033505	86426.636567	56.896845
2672.675252	86110.772999	56.901850
2671.794403	85796.822520	56.906855
2671.132507	85473.479516	56.911860
2670.529107	85138.500579	56.916865
2669.804602	84822.409901	56.921869
2669.180131	84494.334578	56.926874
2668.125637	84183.788559	56.931879
2667.743667	83850.696445	56.936884
2667.046401	83529.670533	56.941889
2666.251682	83220.491961	56.946893
2665.906350	82893.240298	56.951898
2665.129852	82580.880215	56.956903
2664.415085	82244.469141	56.961908
2663.829331	81917.251809	56.966913
2662.919065	81599.185577	56.971917
2662.215968	81276.414251	56.976922
2661.329638	80957.777311	56.981927
2660.922736	80639.360816	56.986932
2660.125603	80335.174866	56.991937
2659.445034	80007.717445	56.996941
2659.021380	79696.548836	57.001946
2658.125795	79388.228962	57.006951
2657.472749	79067.911218	57.011956
2656.686955	78735.326121	57.016961
2656.152104	78418.681448	57.021965
2655.764694	78118.962367	57.026970
2654.750037	77812.744425	57.031975
2654.226321	77483.629549	57.036980
2653.629064	77168.319431	57.041985
2652.473794	76855.529383	57.046989
2652.407750	76534.518365	57.051994
2651.426466	76224.099189	57.056999
2650.830171	75919.877315	57.062004
2649.882246	75593.983882	57.067009
2649.146527	75293.265559	57.072013
2649.027298	74980.885189	57.077018
2648.052578	74674.968073	57.082023
2647.359639	74358.266082	57.087028
2646.935604	74047.152249	57.092033
2646.203300	73734.413258	57.097037
2645.508479	73421.210752	57.102042
2644.593729	73116.473598	57.107047
2643.906732	72795.189846	57.112052
2643.448302	72485.531145	57.117057
2642.592601	72181.464105	57.122061
2641.954100	71858.686472	57.127066
2641.078354	71563.734948	57.132071
2640.581987	71243.377285	57.137076
2639.709852	70940.472108	57.142081
2639.101094	70640.240902	57.147085
2638.669773	70338.358282	57.152090
2638.129142	70021.891313	57.157095
2637.215308	69710.245370	57.162100
2636.511469	69422.703051	57.167105
2635.788049	69103.518314	57.172109
2635.429436	68796.618918	57.177114
2634.503387	68491.631991	57.182119
2634.241423	68187.222286	57.187124
2633.612515	67875.034805	57.192129
2632.697217	67567.552658	57.197133
2631.847068	67267.113854	57.202138
2631.329166	66965.081798	57.207143
2630.990416	66646.265928	57.212148
2629.888024	66345.748419	57.217153
2629.338160	66033.973913	57.222157
2628.899530	65716.971901	57.227162
2627.662033	65430.991832	57.232167
2627.629431	65110.082141	57.237172
2626.830452	64817.275526	57.242177
2625.811557	64514.199351	57.247181
2625.270015	64209.254013	57.252186
2624.499639	63905.673206	57.257191
2623.724542	63600.496005	57.262196
2623.193524	63304.026123	57.267201
2622.432724	62999.726928	57.272205
2622.150558	62700.349263	57.277210
2621.154388	62401.706799	57.282215
2620.743928	62090.265879	57.287220
2620.178623	61784.464190	57.292225
2619.281340	61493.680764	57.297229
2618.736563	61184.317911	57.302234
2617.918029	60881.844202	57.307239
2617.434007	60570.528703	57.312244
2616.435425	60278.745028	57.317249
2615.786524	59977.654971	57.322253
2615.651279	59666.539797	57.327258
2614.400120	59382.122008	57.332263
2613.851312	59068.904638	57.337268
2613.395962	58779.872175	57.342273
2612.429332	58477.274121	57.347277
2612.045885	58185.033265	57.352282
2610.995042	57883.686283	57.357287
2610.326406	57574.399742	57.362292
2609.508548	57285.403717	57.367297
2609.211419	56992.516048	57.372301
2608.460845	56689.792734	57.377306
2607.982386	56405.168454	57.382311
2607.048967	56113.639349	57.387316
2606.245929	55817.245968	57.392321
2605.769356	55516.020771	57.397325
2605.124246	55216.814573	57.402330
2604.529959	54925.684172	57.407335
2603.791238	54625.078477	57.412340
2603.061062	54342.187492	57.417345
2602.417460	54035.722318	57.422349
2601.650620	53747.723319	57.427354
2600.698372	53450.414272	57.432359
2600.210351	53161.579838	57.437364
2599.674056	52871.457200	57.442369
2598.930173	52580.609569	57.447373
2598.352270	52291.616592	57.452378
2597.628583	52005.214177	57.457383
2597.209661	51712.418000	57.462388
2596.454926	51412.399713	57.467393
2595.349036	51131.542135	57.472397
2595.089215	50841.016068	57.477402
2594.254672	50553.736868	57.482407
2593.776794	50252.719683	57.487412
2593.243082	49967.502908	57.492417
2592.438638	49673.424969	57.497421
2591.518784	49377.212652	57.502426
2591.047767	49107.105534	57.507431
2590.526785	48802.627196	57.512436
2589.585243	48521.790984	57.517441
2588.715789	48234.943818	57.522445
2588.207303	47937.197253	57.527450
2587.226269	47659.316495	57.532455
2586.695534	47367.773465	57.537460
2586.071648	47089.784974	57.542465
2585.340712	46802.632302	57.547469
2584.995625	46530.029954	57.552474
2584.128322	46244.992429	57.557479
2583.425279	45955.002527	57.562484
2582.811361	45671.952096	57.567489
2582.210751	45403.769333	57.572493
2581.606556	45112.879480	57.577498
2580.771556	44830.228784	57.582503
2580.072796	44549.423883	57.587508
2579.432777	44260.929075	57.592513
2578.524095	43985.505019	57.597517
2578.047392	43701.610938	57.602522
2577.383718	43421.460688	57.607527
2576.796299	43138.975357	57.612532
2576.245499	42860.422792	57.617537
2575.244196	42591.550013	57.622541
2574.867798	42302.669714	57.627546
2573.999166	42037.923917	57.632551
2573.367414	41746.348629	57.637556
2572.719677	41475.249033	57.642561
2572.033124	41197.930644	57.647565
2571.340648	40912.709540	57.652570
2570.498354	40645.625349	57.657575
2569.809710	40367.748416	57.662580
2569.184594	40089.927588	57.667585
2568.212361	39820.265212	57.672589
2567.809370	39550.467874	57.677594
2566.935763	39278.972530	57.682599
2566.394298	39013.886521	57.687604
2565.829323	38733.150614	57.692609
2565.108349	38479.298158	57.697613
2564.785379	38194.585627	57.702618
2563.547642	37927.069316	57.707623
2562.722181	37660.222176	57.712628
2562.046805	37384.214466	57.717633
2561.013230	37142.571147	57.722637
2560.598245	36866.614412	57.727642
2559.953812	36616.907967	57.732647
2559.314184	36358.677289	57.737652
2558.285839	36104.147448	57.742657
2557.397688	35840.435382	57.747661
2557.456002	35590.221888	57.752666
2556.483655	35345.918934	57.757671
2555.737446	35077.886428	57.762676
2555.152357	34827.727840	57.767681
2554.228267	34572.868142	57.772685
2553.910848	34324.836661	57.777690
2553.186602	34079.830198	57.782695
2552.336807	33814.347194	57.787700
2551.909768	33556.096112	57.792705
2550.866093	33316.156370	57.797709
2550.456068	33066.525915	57.802714
2549.546139	32824.040528	57.807719
2548.822509	32573.773487	57.812724
2547.898193	32336.226217	57.817729
2546.872264	32101.970997	57.822733
2546.015022	31851.603350	57.827738
2545.321141	31629.450356	57.832743
2544.635789	31397.510293	57.837748
2544.180451	31162.187282	57.842753
2542.896547	30953.736662	57.847757
2542.279569	30722.007028	57.852762
2540.729038	30529.322253	57.857767
2539.969217	30300.225092	57.862772
2539.040069	30109.502341	57.867777
2537.751077	29913.847773	57.872781
2537.134444	29731.031826	57.877786
2535.690312	29550.409307	57.882791
2534.850271	29386.646989	57.887796
2534.232591	29195.438440	57.892801
2533.050097	29043.556148	57.897805
2532.344242	28877.810739	57.902810
2531.623870	28735.318254	57.907815
2530.739725	28567.158679	57.912820
2529.931488	28415.900677	57.917825
2528.868048	28283.117608	57.922829
2528.826835	28140.603259	57.927834
2527.716588	27993.111146	57.932839
2527.050594	27851.414010	57.937844
2526.286099	27720.188463	57.942849
2525.757654	27578.887382	57.947853
2525.275529	27449.300106	57.952858
2524.504072	27318.012578	57.957863
2523.486307	27184.235286	57.962868
2523.002659	27052.594677	57.967873
2522.347480	26923.307597	57.972877
2521.482391	26805.145571	57.977882
2520.979768	26672.887895	57.982887
2520.024538	26556.923463	57.987892
2519.377619	26429.524325	57.992897
2518.669112	26303.557602	57.997901
2518.404723	26187.286506	58.002906
2517.537173	26076.021991	58.007911
2517.102864	25933.422784	58.012916
2516.550679	25823.158073	58.017921
2515.905896	25697.552457	58.022925
2515.115181	25566.786144	58.027930
2514.562190	25455.255726	58.032935
2513.880160	25334.846793	58.037940
2513.583549	25216.161713	58.042945
2512.680520	25097.451229	58.047949
2512.499480	24956.802812	58.052954
2511.549773	24843.822458	58.057959
2510.732157	24712.606974	58.062964
2510.298981	24598.335040	58.067969
2509.700782	24467.206038	58.072973
2509.358263	24340.591024	58.077978
2508.400172	24207.851766	58.082983
2507.925455	24080.905194	58.087988
2507.279280	23959.982902	58.092993
2506.252769	23829.680400	58.097997
2505.863265	23709.893574	58.103002
2505.180311	23585.337191	58.108007
2504.737754	23459.061697	58.113012
2504.014296	23331.509851	58.118017
2503.490371	23201.648472	58.123021
2502.709618	23081.541473	58.128026
2502.064361	22967.396985	58.133031
2501.793990	22827.755928	58.138036
2501.094269	22711.141690	58.143041
2500.068223	22582.090645	58.148045
2499.469323	22450.856781	58.153050
2498.976838	22327.765338	58.158055
2498.039220	22191.632545	58.163060
2497.734842	22069.783753	58.168065
2497.106523	21930.644784	58.173069
2496.348345	21805.147864	58.178074
2495.415674	21692.173814	58.183079
2494.895246	21548.326306	58.188084
2494.310623	21424.875142	58.193089
2493.825147	21308.699184	58.198093
2493.364869	21159.971763	58.203098
2492.271130	21036.718044	58.208103
2491.448721	20909.842924	58.213108
2490.905320	20782.082565	58.218113
2490.752364	20655.823417	58.223117
2489.967309	20534.239545	58.228122
2488.866124	20416.689413	58.233127
2488.304843	20277.292702	58.238132
2487.796522	20150.773015	58.243137
2486.790845	20032.278229	58.248141
2486.292138	19904.326477	58.253146
2485.866841	19778.264009	58.258151
2485.476106	19641.081324	58.263156
2484.588919	19521.189655	58.268161
2484.098082	19388.828154	58.273165
2483.660920	19257.633574	58.278170
2482.310691	19136.938416	58.283175
2481.582971	19011.680438	58.288180
2481.298454	18879.812361	58.293185
2480.417578	18759.779888	58.298189
2480.332545	18621.246061	58.303194
2479.329833	18499.605545	58.308199
2478.183605	18376.086261	58.313204
2477.397132	18262.401330	58.318209
2477.078074	18137.893147	58.323213
2476.674082	18010.850095	58.328218
2476.090460	17883.525541	58.333223
2475.491237	17752.974380	58.338228
2474.598571	17611.502958	58.343233
2473.866966	17497.203956	58.348237
2473.571856	17370.797140	58.353242
2472.789093	17245.288600	58.358247
2472.610893	17117.337727	58.363252
2471.620984	16996.391320	58.368257
2471.066252	16863.450285	58.373261
2470.386932	16717.455404	58.378266
2469.354821	16603.617929	58.383271
2468.485269	16467.185981	58.388276
2467.946246	16346.707935	58.393281
2467.162779	16215.451276	58.398285
2466.894316	16096.186483	58.403290
2466.262158	15978.120590	58.408295
2465.839681	15856.027128	58.413300
2464.882410	15711.956806	58.418305
2464.068103	15597.467225	58.423309
2463.591528	15450.508917	58.428314
2462.808645	15340.280235	58.433319
2461.942848	15209.479980	58.438324
2461.577427	15070.942837	58.443329
2460.769342	14963.929696	58.448333
2459.947822	14837.293628	58.453338
2459.289236	14698.097922	58.458343
2459.027311	14578.330565	58.463348
2458.058220	14459.126105	58.468353
2457.139043	14334.282727	58.473357
2456.738140	14212.669067	58.478362
2455.641569	14087.962955	58.483367
2455.109124	13978.229070	58.488372
2454.537181	13846.498505	58.493377
2453.991173	13738.579252	58.498381
2453.342034	13614.485839	58.503386
2453.015790	13496.604893	58.508391
2452.149809	13369.316449	58.513396
2451.391484	13253.857452	58.518401
2450.818819	13136.993636	58.523405
2450.321855	13001.649470	58.528410
2449.950743	12874.920763	58.533415
2448.787064	12759.524254	58.538420
2448.031921	12616.783640	58.543425
2447.009482	12510.448126	58.548429
2446.552622	12389.334188	58.553434
2446.265728	12263.093173	58.558439
2445.386945	12148.405579	58.563444
2444.851048	12020.234327	58.568449
2444.342991	11912.358689	58.573453
2443.912954	11787.480225	58.578458
2442.941433	11664.646106	58.583463
2441.755230	11545.370550	58.588468
2441.838615	11412.244482	58.593473
2440.966986	11295.512652	58.598477
2440.559832	11171.591758	58.603482
2439.615894	11044.489217	58.608487
2439.264295	10911.991397	58.613492
2438.676199	10793.613221	58.618497
2437.908777	10675.825391	58.623501
2437.377041	10535.782758	58.628506
2436.282284	10417.341504	58.633511
2435.676331	10309.175248	58.638516
2435.211599	10171.325479	58.643521
2434.073026	10058.082359	58.648525
2433.734871	9936.476709	58.653530
2433.074934	9808.927315	58.658535
2432.521121	9674.884036	58.663540
2431.622783	9564.367506	58.668545
2430.812636	9445.171227	58.673549
2430.296384	9319.198851	58.678554
2429.888645	9194.350333	58.683559
2428.651700	9079.065554	58.688564
2428.264385	8962.009939	58.693569
2427.609819	8836.365702	58.698573
2426.805582	8717.625920	58.703578
2426.100814	8603.093118	58.708583
2425.535394	8484.190310	58.713588
2424.743950	8357.955660	58.718593
2424.015967	8261.751905	58.723597
2423.665321	8131.638176	58.728602
2422.704475	8022.860315	58.733607
2421.960583	7899.561334	58.738612
2421.641200	7783.301313	58.743617
2420.998819	7667.358859	58.748621
2420.436861	7541.999533	58.753626
2419.237714	7437.047823	58.758631
2418.922385	7314.033608	58.763636
2418.406575	7196.843769	58.768641
2417.446441	7092.047492	58.773645
2417.390030	6958.996833	58.778650
2416.562284	6852.247079	58.783655
2415.765208	6721.521493	58.788660
2414.960927	6606.718474	58.793665
2414.115769	6507.637119	58.798669
2413.532512	6373.378461	58.803674
2412.625818	6268.241923	58.808679
2412.042454	6151.018979	58.813684
2411.510801	6038.520571	58.818689
2410.373676	5943.403930	58.823693
2410.319062	5807.018162	58.828698
2409.292225	5703.453795	58.833703
2408.737440	5586.675637	58.838708
2408.024136	5486.490951	58.843713
2407.678460	5372.660386	58.848717
2406.773149	5256.750440	58.853722
2405.983410	5143.738183	58.858727
2405.841821	5046.705882	58.863732
2405.007692	4929.138020	58.868737
2403.790163	4824.161200	58.873741
2403.403091	4714.990086	58.878746
2402.782437	4594.383745	58.883751
2401.848790	4503.353191	58.888756
2400.959351	4384.694283	58.893761
2400.376029	4279.363675	58.898765
2399.672098	4175.668136	58.903770
2399.047503	4077.300775	58.908775
2398.171944	3982.607997	58.913780
2397.852840	3864.786365	58.918785
2397.141691	3775.796819	58.923789
2396.246641	3654.452257	58.928794
2395.685164	3566.018322	58.933799
2395.377552	3459.522122	58.938804
2394.745298	3349.062503	58.943809
2393.873604	3250.434665	58.948813
2393.152426	3143.578116	58.953818
2392.495474	3039.958064	58.958823
2391.656304	2958.894823	58.963828
2391.210619	2837.430565	58.968833
2390.229141	2757.804167	58.973837
2389.473014	2650.229679	58.978842
2388.987386	2544.338502	58.983847
2388.379131	2456.891787	58.988852
2387.449575	2360.450070	58.993857
2386.779829	2272.515833	58.998861
2386.441284	2166.093083	59.003866
2385.512650	2083.263589	59.008871
2384.409310	1977.906595	59.013876
2384.106750	1893.152625	59.018881
2382.917786	1814.516838	59.023885
2381.988265	1738.064008	59.028890
2381.276158	1651.291498	59.033895
2380.035171	1576.584249	59.038900
2379.673111	1510.192560	59.043905
2378.966264	1442.318233	59.048909
2377.963168	1368.739763	59.053914
2377.309775	1299.189129	59.058919
2376.732581	1240.320501	59.063924
2376.162160	1160.580878	59.068929
2375.191401	1112.967216	59.073933
2374.576813	1042.087764	59.078938
2373.724323	979.510597	59.083943
2372.918865	917.487647	59.088948
2372.371901	859.675502	59.093953
2371.328671	810.768590	59.098957
2370.895388	746.184703	59.103962
2370.072917	698.101034	59.108967
2369.159576	648.472327	59.113972
2368.663235	602.019871	59.118977
2367.844077	552.059593	59.123981
2367.431755	505.059541	59.128986
2366.739872	465.812025	59.133991
2365.844619	417.532676	59.138996
2365.206284	373.334826	59.144001
2364.402813	331.481370	59.149005
2364.204302	280.209383	59.154010
2363.606184	230.032244	59.159015
2362.665953	199.360644	59.164020
2361.974426	129.643478	59.169025
2360.937128	107.458564	59.174029
2359.954198	64.092139	59.179034
2359.065101	38.394172	59.184039
2358.654113	8.769680	59.189044
2357.725370	-33.013968	59.194049
2356.288421	-49.587797	59.199053
2352.314686	34.147176	59.204058
2351.144374	66.272594	59.209063
2351.717195	68.091313	59.214068
2352.221252	59.857222	59.219073
2352.329958	63.797921	59.224077
2351.913392	60.759028	59.229082
2351.356864	60.022515	59.234087
2350.482287	68.592785	59.239092
2349.804112	66.763854	59.244097
2348.920777	66.143820	59.249101
2348.205671	75.333753	59.254106
2347.501636	72.125989	59.259111
2347.169617	69.606677	59.264116
2347.146071	66.040275	59.269121
2346.198340	74.992720	59.274125
2345.222581	80.847868	59.279130
2344.735900	80.447194	59.284135
2344.432037	77.103432	59.289140
2343.438398	78.230742	59.294145
2342.436083	87.519845	59.299149
2342.363427	82.829018	59.304154
2341.713355	91.538735	59.309159
2340.786716	82.944916	59.314164
2340.611175	80.575822	59.319169
2339.500845	86.881231	59.324173
2338.737040	82.533392	59.329178
2337.959422	81.642715	59.334183
2337.644742	93.462490	59.339188
2337.204167	78.797821	59.344193
2336.257829	95.101530	59.349197
2336.254354	87.343711	59.354202
2335.376318	81.317254	59.359207
2334.226386	79.022268	59.364212
2333.873226	88.605801	59.369217
2333.002112	89.592263	59.374221
2332.754744	81.835282	59.379226
2332.142810	78.393727	59.384231
2331.120783	83.335314	59.389236
2330.437747	87.136663	59.394241
2329.854432	80.921547	59.399245
2329.507987	85.341271	59.404250
2328.675095	83.383922	59.409255
2327.920217	76.208883	59.414260
2327.297617	77.723615	59.419265
2326.748801	85.419099	59.424269
2326.535041	79.813979	59.429274
2326.012521	77.009502	59.434279
2324.965211	88.491318	59.439284
2324.318778	84.315673	59.444289
2323.319072	80.489358	59.449293
2322.426421	81.745734	59.454298
2321.849926	80.225523	59.459303
2321.622780	90.544404	59.464308
2321.329453	76.928676	59.469313
2320.395729	89.253462	59.474317
2319.763517	82.912068	59.479322
2319.115024	78.771444	59.484327
2318.023223	84.089940	59.489332
2317.286624	78.640278	59.494337
2316.497126	75.327811	59.499341
2315.746261	83.391218	59.504346
2316.020244	78.413615	59.509351
2315.535899	86.480484	59.514356
2315.260681	81.022301	59.519361
2313.545856	84.798065	59.524365
2312.642401	90.034656	59.529370
2312.171474	75.291237	59.534375
2311.436639	82.817536	59.539380
2311.095995	68.528106	59.544385
2309.634778	89.431264	59.549389
2309.535034	82.743659	59.554394
2309.372415	84.570204	59.559399
2308.649243	85.681438	59.564404
2308.243781	77.867538	59.569409
2307.273925	88.272673	59.574413
2306.158558	82.000027	59.579418
2305.898820	76.206668	59.584423
2304.739927	83.475385	59.589428
2304.413849	78.969829	59.594433
2303.398615	87.021555	59.599437
2303.137373	80.394257	59.604442
2303.205146	81.392663	59.609447
2302.123624	75.064193	59.614452
2301.218278	66.421294	59.619457
2300.692696	85.868814	59.624461
2300.333083	71.653353	59.629466
2299.110099	79.365880	59.634471
2298.782111	85.887829	59.639476
2298.349175	78.554510	59.644481
2296.832595	84.933826	59.649485
2296.634906	73.767621	59.654490
2296.559651	73.050977	59.659495
2295.560111	76.129853	59.664500
2295.122141	79.559615	59.669505
2293.424514	91.962991	59.674509
2293.086135	78.677678	59.679514
2292.642798	92.746004	59.684519
2291.903964	82.143420	59.689524
2291.765312	77.639678	59.694529
2290.767788	80.210478	59.699533
2290.268132	85.394067	59.704538
2289.509418	80.592870	59.709543
2288.621285	95.914415	59.714548
2287.900441	83.670587	59.719553
2287.261462	100.277208	59.724557
2287.049357	81.646699	59.729562
2286.059144	85.668658	59.734567
2284.968233	78.160593	59.739572
2284.673311	83.302248	59.744577
2284.108047	82.466212	59.749581
2284.375061	86.709796	59.754586
2283.063398	79.853308	59.759591
2281.899345	88.977278	59.764596
2281.440642	80.203616	59.769601
2280.411606	83.203602	59.774605
2280.599507	83.755615	59.779610
2279.646385	80.940602	59.784615
2278.892417	81.514277	59.789620
2278.515356	77.595531	59.794625
2277.168419	84.331134	59.799629
2277.090410	77.195405	59.804634
2276.727683	76.524358	59.809639
2275.706895	83.925716	59.814644
2275.150096	80.924845	59.819649
2274.428577	80.414781	59.824653
2273.857694	74.426362	59.829658
2273.318797	84.868799	59.834663
2272.365155	84.788199	59.839668
2271.711217	85.478469	59.844673
2271.241996	79.589036	59.849677
2270.673921	82.467027	59.854682
2270.072686	81.933155	59.859687
2269.247333	92.159270	59.864692
2268.832850	80.089201	59.869697
2267.173464	79.942356	59.874701
2267.206400	73.801396	59.879706
2266.688224	81.586639	59.884711
2265.310956	84.531483	59.889716
2265.123140	70.329783	59.894721
2264.713085	85.261689	59.899725
2264.000807	69.580479	59.904730
2262.891980	78.239968	59.909735
2262.136176	85.471571	59.914740
2262.057247	69.136414	59.919745
2261.136562	79.751366	59.924750
2260.558139	75.285845	59.929754
2259.809352	75.022951	59.934759
2258.921300	78.640799	59.939764
2258.716439	78.424088	59.944769
2258.001456	78.117988	59.949774
2257.168138	74.935489	59.954778
2256.636561	76.877327	59.959783
2256.086120	84.943647	59.964788
2255.914365	68.884979	59.969793
2254.786946	81.478606	59.974798
2254.570249	63.017586	59.979802
2253.433695	73.871771	59.984807
2252.500368	79.393800	59.989812
2252.003027	64.424377	59.994817
2250.789239	70.676836	59.999822
2250.711163	70.526745	60.004826
2250.594936	79.520781	60.009831
2249.517304	79.127133	60.014836
2249.080815	78.027838	60.019841
2247.988818	81.324815	60.024846
2247.583403	79.939905	60.029850
2247.009390	80.105014	60.034855
2246.506275	81.398968	60.039860
2245.429702	73.833459	60.044865
2244.217017	72.259646	60.049870
2243.227886	73.215972	60.054874
2243.531064	78.693246	60.059879
2243.237972	76.197735	60.064884
2242.465720	67.957932	60.069889
2240.989141	91.347151	60.074894
2240.559399	73.202179	60.079898
2239.938746	75.456181	60.084903
2239.514909	72.076276	60.089908
2238.878834	72.751105	60.094913
2238.365901	78.983859	60.099918
2237.831068	77.852859	60.104922
2237.470617	73.259732	60.109927
2236.133311	75.340422	60.114932
2235.252715	74.743644	60.119937
2235.061820	80.239368	60.124942
2234.237365	85.663713	60.129946
2233.408335	83.056105	60.134951
2232.365035	81.365545	60.139956
2232.192626	78.819353	60.144961
2231.553829	78.053339	60.149966
2230.952275	77.002307	60.154970
2230.558570	81.027428	60.159975
2229.961315	77.835875	60.164980
2229.577628	82.280436	60.169985
2228.493035	83.939435	60.174990
2227.271959	67.850117	60.179994
2226.489067	77.733617	60.184999
2226.180771	84.605669	60.190004
2225.917734	80.288814	60.195009
2224.639586	74.608136	60.200014
2223.981707	74.737670	60.205018
2223.690178	73.676883	60.210023
2223.078267	71.528405	60.215028
2222.764387	78.762447	60.220033
2222.337499	70.724898	60.225038
2221.771637	69.918933	60.230042
2220.553753	70.911554	60.235047
2219.481965	78.220095	60.240052
2218.720863	63.883858	60.245057
2218.300318	79.935436	60.250062
2217.819350	72.150885	60.255066
2217.533922	77.458186	60.260071
2216.673546	80.078215	60.265076
2216.251912	75.335531	60.270081
2214.607069	72.783233	60.275086
2214.314667	69.332023	60.280090
2213.503875	72.945510	60.285095
2212.850507	75.671467	60.290100
2212.384743	74.192061	60.295105
2212.013625	78.374443	60.300110
2211.379127	78.714728	60.305114
2210.728232	75.214735	60.310119
2210.120657	69.697338	60.315124
2209.707148	68.264835	60.320129
2208.596344	82.423268	60.325134
2207.722528	77.422748	60.330138
2206.840662	69.657644	60.335143
2206.171853	86.470828	60.340148
2205.909147	67.988730	60.345153
2205.464259	79.816532	60.350158
2204.938491	73.868282	60.355162
2204.490331	72.572158	60.360167
2203.261937	78.484772	60.365172
2202.501789	70.941625	60.370177
2201.600219	76.244172	60.375182
2200.878098	80.945844	60.380186
2200.205512	71.717303	60.385191
2199.971051	70.948652	60.390196
2199.587899	74.079581	60.395201
2198.486204	69.564631	60.400206
2198.335997	71.482247	60.405210
2197.880133	64.428552	60.410215
2197.022733	74.566716	60.415220
2196.221708	62.904920	60.420225
2195.214472	73.084199	60.425230
2194.523020	66.290220	60.430234
2194.577696	66.473870	60.435239
2193.679345	69.467343	60.440244
2192.878689	63.512249	60.445249
2191.134142	77.110503	60.450254
2191.029873	73.668872	60.455258
2191.142687	77.432297	60.460263
2190.208002	75.644103	60.465268
2189.642719	74.153683	60.470273
2188.442358	75.821601	60.475278
2188.383013	67.921288	60.480282
2187.802779	72.881136	60.485287
2186.842808	79.506502	60.490292
2186.233074	76.791584	60.495297
2185.316309	80.325703	60.500302
2184.536107	80.864144	60.505306
2184.188649	75.496289	60.510311
2183.496309	83.222444	60.515316
2183.125635	64.394801	60.520321
2182.558945	75.678976	60.525326
2180.977604	72.276143	60.530330
2180.811671	76.225710	60.535335
2179.920206	78.891681	60.540340
2179.487700	85.174761	60.545345
2178.880822	71.943120	60.550350
2178.607404	71.016655	60.555354
2178.064459	78.151427	60.560359
2176.601966	78.695616	60.565364
2176.303428	74.059564	60.570369
2175.497507	78.098049	60.575374
2174.777287	75.753886	60.580378
2174.037445	74.461467	60.585383
2173.449399	75.133422	60.590388
2173.188513	78.929327	60.595393
2172.549979	68.809185	60.600398
2172.001642	69.181539	60.605402
2170.970722	65.622007	60.610407
2170.219709	74.426597	60.615412
2169.901304	65.619678	60.620417
2169.225535	73.281702	60.625422
2168.395550	70.196472	60.630426
2167.639225	73.355072	60.635431
2166.376390	79.552273	60.640436
2165.932528	68.187044	60.645441
2165.392630	76.387309	60.650446
2165.274336	77.388422	60.655450
2164.839688	70.771319	60.660455
2163.799201	81.783754	60.665460
2163.251845	75.110416	60.670465
2162.682634	84.095896	60.675470
2161.894831	70.774700	60.680474
2161.173696	73.036776	60.685479
2160.560080	70.134832	60.690484
2160.083360	74.289819	60.695489
2159.269553	77.946376	60.700494
2158.342381	72.571158	60.705498
2157.610730	72.091118	60.710503
2156.851685	75.090886	60.715508
2156.835049	73.574926	60.720513
2156.201289	74.413403	60.725518
2155.168494	86.334488	60.730522
2154.301814	87.225690	60.735527
2153.500610	78.071182	60.740532
2152.965389	71.149929	60.745537
2151.881288	77.925881	60.750542
2151.686848	73.995531	60.755546
2151.433512	86.360629	60.760551
2150.715972	80.762925	60.765556
2150.746142	85.010951	60.770561
2149.461459	84.637579	60.775566
2148.414684	82.279004	60.780570
2147.898802	78.503728	60.785575
2147.204591	78.106056	60.790580
2146.976552	81.455223	60.795585
2145.952220	85.017460	60.800590
2144.909740	80.554635	60.805594
2144.182482	67.286920	60.810599
2143.703971	73.615143	60.815604
2143.461840	74.634327	60.820609
2142.779817	78.867620	60.825614
2142.511873	69.753089	60.830618
2141.345122	69.094517	60.835623
2140.477575	75.165935	60.840628
2139.981406	77.099022	60.845633
2139.509415	82.295586	60.850638
2138.929318	66.773227	60.855642
2138.622415	72.438737	60.860647
2137.171611	81.439520	60.865652
2136.488188	67.269181	60.870657
2135.571108	76.749805	60.875662
2135.262653	81.035788	60.880666
2135.282421	79.845198	60.885671
2134.081537	78.632249	60.890676
2133.155064	76.185210	60.895681
2132.116413	76.036151	60.900686
2131.456752	80.753157	60.905690
2131.480722	75.066194	60.910695
2130.800710	81.325472	60.915700
2130.335472	71.349727	60.920705
2129.836419	75.834677	60.925710
2128.811953	67.942429	60.930714
2128.479451	71.286093	60.935719
2127.549643	72.701383	60.940724
2127.030326	75.491241	60.945729
2126.206625	80.086049	60.950734
2125.096791	75.045742	60.955738
2124.527421	70.162524	60.960743
2123.733517	78.873011	60.965748
2123.504220	64.860849	60.970753
2122.815849	73.247094	60.975758
2122.771983	72.479747	60.980762
2121.758583	76.570089	60.985767
2120.613261	72.994037	60.990772
2119.967687	70.783120	60.995777
2119.213161	77.210334	61.000782
2118.734659	69.937907	61.005786
2118.631848	68.107629	61.010791
2117.781133	79.424264	61.015796
2116.965591	72.982720	61.020801
2116.013524	77.074371	61.025806
2115.448655	74.774958	61.030810
2114.755991	66.662920	61.035815
2114.163269	76.033738	61.040820
2114.027183	66.661759	61.045825
2113.068076	80.201658	61.050830
2111.839973	72.521492	61.055834
2111.544143	71.467709	61.060839
2110.964624	71.449225	61.065844
2110.193039	58.920240	61.070849
2109.934334	79.528566	61.075854
2109.236514	73.659678	61.080858
2108.216332	74.458560	61.085863
2107.341008	79.528323	61.090868
2107.237244	72.298934	61.095873
2106.434165	75.734615	61.100878
2106.197587	72.798089	61.105882
2105.026322	68.209070	61.110887
2103.798691	86.093331	61.115892
2103.338890	72.377929	61.120897
2102.895460	66.889710	61.125902
2102.374208	73.992663	61.130906
2102.303444	68.495770	61.135911
2101.332592	76.890576	61.140916
2100.403762	70.235213	61.145921
2099.384060	77.880866	61.150926
2098.803994	81.259087	61.155930
2098.814644	67.700843	61.160935
2098.007778	71.960261	61.165940
2096.741681	60.969946	61.170945
2095.905415	76.764222	61.175950
2095.186315	71.460088	61.180954
2094.800065	64.127303	61.185959
2094.310364	69.585287	61.190964
2094.213816	68.263351	61.195969
2093.586323	75.605506	61.200974
2092.821123	76.603620	61.205978
2092.166284	62.447691	61.210983
2090.854851	78.475058	61.215988
2090.126125	69.099355	61.220993
2089.676450	73.759393	61.225998
2089.547781	71.881183	61.231002
2088.550318	82.090483	61.236007
2087.371439	79.910585	61.241012
2087.077921	71.069771	61.246017
2086.142505	85.127870	61.251022
2085.815697	72.515691	61.256026
2085.357176	75.019953	61.261031
2084.774414	74.467424	61.266036
2084.176628	75.495744	61.271041
2083.032455	71.260389	61.276046
2082.710308	69.668337	61.281050
2082.354834	71.837716	61.286055
2081.418985	77.874259	61.291060
2080.394994	61.066246	61.296065
2079.573388	77.224036	61.301070
2078.904501	80.707814	61.306074
2078.546589	67.892428	61.311079
2078.142808	75.974913	61.316084
2077.825805	73.459566	61.321089
2076.667827	77.131337	61.326094
2075.989128	69.332472	61.331098
2075.672513	69.352698	61.336103
2074.858941	70.885173	61.341108
2073.849916	71.351151	61.346113
2072.769030	71.667691	61.351118
2071.933221	74.517243	61.356122
2071.649144	60.766092	61.361127
2070.874679	84.080201	61.366132
2070.380872	66.598297	61.371137
2070.116566	68.381065	61.376142
2069.633889	68.307800	61.381146
2069.794335	71.407671	61.386151
2068.551593	73.388282	61.391156
2068.110207	68.705534	61.396161
2067.185210	60.933146	61.401166
2065.998151	81.384450	61.406170
2065.062920	66.710074	61.411175
2064.092328	73.222045	61.416180
2063.893860	66.856058	61.421185
2063.636217	70.397573	61.426190
2063.424098	76.615726	61.431194
2062.591791	72.996337	61.436199
2061.459962	77.733094	61.441204
2060.718234	72.087224	61.446209
2060.337905	65.895171	61.451214
2058.872332	72.927222	61.456218
2058.294231	72.952677	61.461223
2057.855676	73.998308	61.466228
2057.521937	67.626981	61.471233
2056.762908	72.651492	61.476238
2056.222503	81.613489	61.481242
2056.099407	74.451826	61.486247
2054.727888	79.843186	61.491252
2054.078171	76.885499	61.496257
2053.524595	75.292331	61.501262
2053.001327	80.735152	61.506266
2052.793737	66.408915	61.511271
2051.694428	88.650263	61.516276
2050.954106	72.230881	61.521281
2050.506549	77.604918	61.526286
2049.745308	86.035862	61.531290
2048.459304	78.448491	61.536295
2047.349804	84.410107	61.541300
2046.935836	77.532713	61.546305
2046.963108	74.298866	61.551310
2046.850395	70.730859	61.556314
2045.899030	78.822980	61.561319
2045.360591	76.770114	61.566324
2044.314090	80.135638	61.571329
2043.381723	72.552074	61.576334
2042.613711	75.103881	61.581338
2042.259944	79.198373	61.586343
2041.756939	83.904729	61.591348
2041.327864	76.269676	61.596353
2040.233518	76.796514	61.601358
2039.433278	80.236494	61.606362
2039.360957	74.033406	61.611367
2038.762563	75.023986	61.616372
2037.884843	71.908532	61.621377
2036.782055	75.921629	61.626382
2035.969389	73.302032	61.631386
2036.240458	71.939103	61.636391
2035.346610	75.217327	61.641396
2034.710142	75.991610	61.646401
2033.811824	69.861267	61.651406
2032.858460	70.525000	61.656410
2032.827191	69.400856	61.661415
2031.615089	76.521999	61.666420
2030.723420	77.166480	61.671425
2030.404635	70.658748	61.676430
2029.581975	80.745708	61.681434
2029.393338	76.998947	61.686439
2028.467832	67.265007	61.691444
2027.525699	67.160593	61.696449
2026.498872	72.683332	61.701454
2026.176547	76.537879	61.706458
2025.910896	64.907877	61.711463
2025.389318	75.418540	61.716468
2025.216594	61.272854	61.721473
2023.857369	77.760392	61.726478
2023.139180	65.399576	61.731482
2022.759069	65.880874	61.736487
2021.744676	71.923589	61.741492
2021.236319	66.161854	61.746497
2020.318567	69.052808	61.751502
2019.832439	62.007116	61.756506
2019.366427	73.690045	61.761511
2018.604629	63.283608	61.766516
2017.946327	67.355471	61.771521
2016.837231	63.720107	61.776526
2015.990633	77.806693	61.781530
2015.797190	67.043558	61.786535
2015.247850	73.583301	61.791540
2015.269841	78.341949	61.796545
2014.563153	67.307048	61.801550
2013.129630	79.428952	61.806554
2012.739017	70.948901	61.811559
2012.186287	75.169585	61.816564
2011.311304	66.908330	61.821569
2010.108075	70.826995	61.826574
2009.575679	78.507293	61.831578
2009.196150	68.197875	61.836583
2008.340137	74.817829	61.841588
2008.011533	68.940838	61.846593
2007.772381	74.512028	61.851598
2007.272297	71.238883	61.856602
2006.223652	76.408716	61.861607
2005.423443	71.371364	61.866612
2004.751243	67.944196	61.871617
2003.672003	74.656348	61.876622
2002.791414	69.986553	61.881626
2002.758993	65.636288	61.886631
2001.871595	65.687191	61.891636
2001.664800	78.298768	61.896641
2000.963993	74.647491	61.901646
2000.077770	72.935251	61.906650
1999.364306	71.659196	61.911655
1998.559324	70.175327	61.916660
1998.079041	70.579491	61.921665
1997.737706	66.590478	61.926670
1996.622413	78.188814	61.931674
1995.724966	62.385738	61.936679
1995.160822	66.560928	61.941684
1995.064096	69.969679	61.946689
1994.274793	65.318515	61.951694
1993.441431	74.497315	61.956698
1992.622199	59.159627	61.961703
1991.637443	71.684948	61.966708
1991.647863	64.702371	61.971713
1991.093662	60.064355	61.976718
1990.243736	70.704400	61.981722
1989.371273	63.813069	61.986727
1988.768743	63.914953	61.991732
1988.017847	62.772572	61.996737
1987.961635	70.189639	62.001742
1987.449111	61.583876	62.006746
1986.256074	61.574491	62.011751
1985.595565	67.969460	62.016756
1985.184885	52.648936	62.021761
1983.953777	60.536317	62.026766
1982.947021	63.518675	62.031770
1982.578695	65.611261	62.036775
1981.977165	74.827380	62.041780
1981.667209	64.450160	62.046785
1981.201917	69.625176	62.051790
1980.393121	65.358718	62.056794
1979.905261	63.014002	62.061799
1978.835831	64.486194	62.066804
1978.226562	59.300283	62.071809
1978.072720	68.319190	62.076814
1976.987091	70.073063	62.081818
1976.266853	61.178588	62.086823
1975.356044	73.911364	62.091828
1975.065965	74.536067	62.096833
1974.792708	72.712352	62.101838
1973.470661	61.612725	62.106842
1972.569863	64.808494	62.111847
1971.968889	67.020006	62.116852
1971.600951	69.812668	62.121857
1971.331580	56.507048	62.126862
1970.314235	73.178443	62.131866
1969.494298	61.604899	62.136871
1968.843554	71.377585	62.141876
1968.270635	67.217187	62.146881
1967.653560	65.211514	62.151886
1967.315071	75.078135	62.156890
1967.201871	64.250238	62.161895
1965.734778	68.805288	62.166900
1965.072609	56.068198	62.171905
1964.716967	65.160132	62.176910
1963.702123	60.680393	62.181914
1963.006439	60.759224	62.186919
1962.195590	57.893372	62.191924
1962.008407	66.400351	62.196929
1961.332654	64.932250	62.201934
1959.772165	69.136291	62.206938
1959.396501	61.891739	62.211943
1958.668151	72.272807	62.216948
1958.299724	60.291725	62.221953
1957.719206	70.201491	62.226958
1957.270391	64.223750	62.231962
1957.145542	62.343366	62.236967
1955.973770	75.324143	62.241972
1955.300890	62.697556	62.246977
1954.730335	68.113201	62.251982
1954.029477	58.665327	62.256986
1953.265961	70.073796	62.261991
1952.601152	59.557380	62.266996
1951.868927	65.902240	62.272001
1951.367137	64.889054	62.277006
1950.149464	64.066770	62.282010
1949.409088	58.501151	62.287015
1948.995329	70.418626	62.292020
1948.597013	62.676223	62.297025
1947.930454	69.786489	62.302030
1947.403796	64.764083	62.307034
1946.918238	61.592722	62.312039
1945.718769	63.749436	62.317044
1945.699752	62.145555	62.322049
1944.989774	70.319225	62.327054
1943.867557	66.261795	62.332058
1943.268769	64.098692	62.337063
1942.105195	71.056051	62.342068
1942.131634	60.341607	62.347073
1941.458786	52.746863	62.352078
1940.522199	66.899773	62.357082
1939.735106	64.340802	62.362087
1938.874876	61.173727	62.367092
1938.776183	53.924640	62.372097
1938.825094	68.919282	62.377102
1937.223778	58.791218	62.382106
1937.008831	58.367986	62.387111
1936.216279	64.109018	62.392116
1935.301272	58.689390	62.397121
1934.468722	68.402633	62.402126
1933.477239	66.204100	62.407130
1933.140068	64.857294	62.412135
1932.266977	60.695673	62.417140
1932.100371	57.379073	62.422145
1931.864809	61.435884	62.427150
1931.379377	52.553041	62.432154
1930.389754	65.621591	62.437159
1929.418929	62.666031	62.442164
1928.755053	62.112223	62.447169
1927.934888	56.229709	62.452174
1927.107191	59.276698	62.457178
1926.950434	69.056123	62.462183
1926.521150	72.227519	62.467188
1926.015077	64.768719	62.472193
1925.105654	55.346081	62.477198
1924.225681	65.421651	62.482202
1923.547907	56.706529	62.487207
1922.034649	67.158585	62.492212
1921.491367	61.951176	62.497217
1921.029510	62.839685	62.502222
1920.573582	67.816110	62.507226
1920.320998	67.816728	62.512231
1919.830672	68.898983	62.517236
1919.394241	70.483593	62.522241
1918.478807	63.386234	62.527246
1917.298656	71.492629	62.532250
1917.090006	65.308044	62.537255
1916.379015	68.385395	62.542260
1915.349288	65.819220	62.547265
1914.707259	72.719027	62.552270
1914.029597	66.392864	62.557274
1913.710050	58.951767	62.562279
1913.285813	65.116861	62.567284
1912.302309	65.991992	62.572289
1911.267741	64.580866	62.577294
1910.762802	62.956358	62.582298
1910.281617	54.594793	62.587303
1909.771876	63.985569	62.592308
1909.238632	59.199175	62.597313
1908.599945	62.943108	62.602318
1907.711530	57.957643	62.607322
1907.243682	59.900463	62.612327
1906.126350	58.852546	62.617332
1905.415974	63.569758	62.622337
1904.985600	51.065546	62.627342
1904.316697	69.502932	62.632346
1904.095468	50.044581	62.637351
1902.875788	62.212989	62.642356
1902.038967	49.432696	62.647361
1902.051880	49.246095	62.652366
1901.336376	53.673973	62.657370
1899.741875	48.799030	62.662375
1898.753137	56.501315	62.667380
1898.851016	56.398992	62.672385
1898.324812	57.188915	62.677390
1897.882595	55.816215	62.682394
1897.796899	61.902335	62.687399
1896.590282	54.359229	62.692404
1895.749615	63.020408	62.697409
1895.188398	52.158005	62.702414
1894.718491	66.618441	62.707418
1893.570162	57.299973	62.712423
1892.667452	61.670846	62.717428
1892.374292	52.905717	62.722433
1891.859501	58.842347	62.727438
1891.084316	62.918598	62.732442
1891.324622	56.099801	62.737447
1889.475287	72.226812	62.742452
1888.989197	55.850737	62.747457
1888.399629	51.271980	62.752462
1887.810592	69.537423	62.757466
1887.084302	56.813697	62.762471
1886.147300	60.932984	62.767476
1885.717924	56.341410	62.772481
1885.254100	62.252605	62.777486
1884.539408	64.332384	62.782490
1884.091257	61.437360	62.787495
1882.908748	52.390821	62.792500
1882.422286	51.548673	62.797505
1882.369374	58.377028	62.802510
1881.137884	66.942571	62.807514
1880.481602	58.957302	62.812519
1879.416163	49.915833	62.817524
1879.380307	61.394856	62.822529
1879.100179	50.971936	62.827534
1878.210948	63.680798	62.832538
1877.491081	52.501405	62.837543
1876.806915	65.012139	62.842548
1875.975465	62.996372	62.847553
1875.149681	63.603637	62.852558
1874.104333	49.692724	62.857562
1873.557908	63.838892	62.862567
1873.085146	62.819536	62.867572
1872.578589	52.653329	62.872577
1872.621445	64.958758	62.877582
1871.508882	68.298561	62.882586
1871.019939	52.607316	62.887591
1870.041105	65.514902	62.892596
1869.299314	55.263043	62.897601
1868.574142	56.545010	62.902606
1867.580320	52.367892	62.907610
1867.386070	61.809502	62.912615
1866.964297	60.094533	62.917620
1866.357473	68.111496	62.922625
1865.250712	59.002476	62.927630
1864.566477	66.728967	62.932634
1864.504648	52.859019	62.937639
1863.169324	66.551724	62.942644
1862.434152	60.635239	62.947649
1861.605908	71.932582	62.952654
1861.207203	67.643632	62.957658
1861.348421	59.695747	62.962663
1860.726040	68.923073	62.967668
1859.527428	54.710083	62.972673
1859.067489	52.375153	62.977678
1858.034083	55.393323	62.982682
1857.403110	58.374406	62.987687
1856.210522	64.316159	62.992692
1855.712224	61.014383	62.997697
1855.428397	56.891693	63.002702
1854.888212	54.845459	63.007706
1854.735010	56.244767	63.012711
1853.677044	51.106481	63.017716
1852.919801	56.931805	63.022721
1852.383108	61.430650	63.027726
1851.230540	57.814881	63.032730
1850.637461	53.194116	63.037735
1849.484906	50.202793	63.042740
1848.996900	58.093660	63.047745
1848.768845	49.739232	63.052750
1848.180824	70.442372	63.057754
1848.110298	58.563827	63.062759
1847.019858	70.355365	63.067764
1846.116537	57.437423	63.072769
1845.875022	58.286229	63.077774
1844.858274	65.447381	63.082778
1844.659968	56.197289	63.087783
1843.409046	63.595884	63.092788
1843.022513	50.895504	63.097793
1842.464220	57.696870	63.102798
1841.292603	54.449968	63.107802
1840.774689	61.664374	63.112807
1840.188571	66.470677	63.117812
1839.713996	68.990138	63.122817
1839.303672	53.163425	63.127822
1837.806669	65.224508	63.132826
1837.293462	47.288501	63.137831
1836.913382	61.537561	63.142836
1836.344958	52.622192	63.147841
1836.196471	44.419132	63.152846
1835.022575	62.121447	63.157850
1834.314304	52.991751	63.162855
1833.536370	57.976735	63.167860
1833.306173	56.638189	63.172865
1832.938197	49.453949	63.177870
1831.104640	60.863604	63.182874
1830.865516	46.310645	63.187879
1830.251031	63.058433	63.192884
1830.042674	49.785744	63.197889
1829.300219	50.188989	63.202894
1828.163323	57.946357	63.207898
1827.994665	54.193298	63.212903
1827.316019	47.503069	63.217908
1826.006528	56.172471	63.222913
1825.700025	43.579238	63.227918
1824.763414	62.026011	63.232922
1824.510981	48.372410	63.237927
1824.137097	55.150803	63.242932
1823.392479	47.684188	63.247937
1822.529547	46.572261	63.252942
1821.195939	57.639197	63.257946
1821.536325	50.148528	63.262951
1820.658083	54.214352	63.267956
1819.632928	56.972617	63.272961
1819.184783	55.624526	63.277966
1818.780946	49.964519	63.282970
1817.866924	44.828626	63.287975
1817.104005	61.407602	63.292980
1816.162316	57.157575	63.297985
1815.770602	59.264931	63.302990
1814.972230	64.273666	63.307994
1814.897759	42.850908	63.312999
1813.724610	60.929982	63.318004
1812.900694	63.610568	63.323009
1812.892042	48.817598	63.328014
1812.177684	60.273467	63.333018
1811.441652	53.576584	63.338023
1810.319786	53.702627	63.343028
1809.303544	57.996939	63.348033
1809.299415	45.057666	63.353038
1808.879691	57.914325	63.358042
1808.596698	43.341533	63.363047
1807.056898	55.436225	63.368052
1806.453198	59.728106	63.373057
1806.399673	50.734143	63.378062
1804.722241	59.947658	63.383066
1804.357458	49.907188	63.388071
1803.310686	52.635776	63.393076
1803.306123	58.390479	63.398081
1802.774509	54.855898	63.403086
1802.417228	65.793047	63.408090
1801.473096	52.334435	63.413095
1800.222725	56.364742	63.418100
1799.760009	56.042364	63.423105
1799.377383	57.508065	63.428110
1798.718776	59.843874	63.433114
1797.852138	57.114665	63.438119
1797.078831	56.013744	63.443124
1796.768807	55.072637	63.448129
1796.675925	47.259701	63.453134
1795.341799	63.210328	63.458138
1794.775410	43.382647	63.463143
1794.234811	56.619604	63.468148
1793.299223	47.710519	63.473153
1792.592176	50.104480	63.478158
1791.509422	49.029047	63.483162
1791.468012	52.159363	63.488167
1790.902780	59.207832	63.493172
1790.468935	59.961033	63.498177
1789.460205	51.222826	63.503182
1788.362567	59.677263	63.508186
1788.064019	53.191603	63.513191
1787.528910	55.660761	63.518196
1787.268038	59.251686	63.523201
1786.017681	45.417533	63.528206
1784.981640	63.807567	63.533210
1784.985541	44.922185	63.538215
1784.461992	67.204576	63.543220
1783.644076	57.321213	63.548225
1782.793160	58.269949	63.553230
1782.236581	56.612670	63.558234
1781.658811	57.220001	63.563239
1780.691460	56.768036	63.568244
1779.951405	45.845770	63.573249
1779.528489	52.475841	63.578254
1779.257461	52.200294	63.583258
1778.833711	48.282756	63.588263
1777.746901	49.161725	63.593268
1776.872859	38.569811	63.598273
1776.344643	53.665516	63.603278
1774.874558	52.063421	63.608282
1774.472172	48.751167	63.613287
1773.669243	55.421086	63.618292
1773.121399	58.614480	63.623297
1773.291011	42.959045	63.628302
1772.654671	56.507660	63.633306
1772.032235	52.104457	63.638311
1770.783232	61.916977	63.643316
1770.332100	56.625594	63.648321
1769.800200	49.983039	63.653326
1768.344379	57.336932	63.658330
1767.798738	53.493943	63.663335
1767.244936	62.641004	63.668340
1766.748771	63.424605	63.673345
1766.804477	54.958898	63.678350
1766.242794	59.266191	63.683354
1765.461102	50.614938	63.688359
1764.595751	63.654328	63.693364
1764.005306	53.110409	63.698369
1762.918707	54.463991	63.703374
1761.687832	62.422381	63.708378
1761.548895	49.198605	63.713383
1760.881751	57.275616	63.718388
1760.619722	58.961856	63.723393
1760.063914	60.622214	63.728398
1758.823416	57.709550	63.733402
1758.756939	57.177604	63.738407
1757.998423	53.887216	63.743412
1757.023202	56.900913	63.748417
1756.456856	55.276728	63.753422
1756.066693	60.878209	63.758426
1755.067883	51.162355	63.763431
1754.190531	60.100613	63.768436
1753.222568	62.103957	63.773441
1753.093914	56.315109	63.778446
1752.178810	52.843019	63.783450
1751.723721	56.747050	63.788455
1751.351510	47.601865	63.793460
1750.733609	52.632411	63.798465
1749.966650	53.496865	63.803470
1749.554087	55.765227	63.808474
1748.139163	56.175946	63.813479
1747.348361	65.212423	63.818484
1746.766955	47.921187	63.823489
1746.482914	55.024347	63.828494
1745.773198	53.735156	63.833498
1745.327790	51.082567	63.838503
1744.634245	53.275710	63.843508
1743.737149	63.008700	63.848513
1743.500423	51.892975	63.853518
1742.876991	56.653180	63.858522
1741.593488	61.316373	63.863527
1740.800538	68.066719	63.868532
1740.229907	55.628980	63.873537
1739.817297	54.281568	63.878542
1739.475585	61.136859	63.883546
1739.041514	48.797282	63.888551
1737.951860	51.340325	63.893556
1737.352532	55.670946	63.898561
1736.882743	47.730227	63.903566
1735.562719	56.839710	63.908570
1734.862914	54.913467	63.913575
1734.452988	56.361435	63.918580
1733.755507	65.220675	63.923585
1733.592599	49.200174	63.928590
1732.884282	55.834577	63.933594
1732.576893	52.357439	63.938599
1731.689953	48.683776	63.943604
1731.094751	66.070298	63.948609
1730.078658	43.650717	63.953614
1729.142968	57.300492	63.958618
1728.703314	44.144986	63.963623
1727.820600	50.266216	63.968628
1726.629455	51.324195	63.973633
1726.206752	45.440136	63.978638
1725.752810	64.513557	63.983642
1725.268935	56.220276	63.988647
1724.921482	54.422570	63.993652
1724.317267	58.782354	63.998657
1723.654425	50.039706	64.003662
1723.024525	54.786750	64.008666
1722.507535	51.931078	64.013671
1721.319994	55.054197	64.018676
1720.279138	53.481730	64.023681
1719.996355	51.921324	64.028686
1719.354321	62.648243	64.033690
1719.099864	51.735602	64.038695
1718.110018	52.455700	64.043700
1717.295829	62.995506	64.048705
1716.802670	52.032472	64.053710
1716.169640	56.597096	64.058714
1715.954206	54.313245	64.063719
1714.916680	51.483480	64.068724
1713.639326	56.539927	64.073729
1713.685375	59.569625	64.078734
1712.530198	56.652895	64.083738
1711.831303	51.036619	64.088743
1711.184885	62.868050	64.093748
1710.482012	58.938087	64.098753
1710.296092	47.374354	64.103758
1709.928719	51.578256	64.108762
1709.219466	56.702165	64.113767
1708.406617	50.373894	64.118772
1707.463454	59.404613	64.123777
1707.291714	51.842319	64.128782
1705.797160	59.818954	64.133786
1705.224762	54.625691	64.138791
1705.206852	63.824834	64.143796
1704.476073	58.096933	64.148801
1703.176129	49.048647	64.153806
1702.390056	63.106735	64.158810
1701.739441	58.368997	64.163815
1701.875211	52.229091	64.168820
1701.493194	55.659497	64.173825
1700.967544	51.128985	64.178830
1699.798716	53.519046	64.183834
1699.083747	48.737920	64.188839
1698.102363	63.571316	64.193844
1697.271799	63.053503	64.198849
1696.791889	52.009527	64.203854
1695.930220	61.345835	64.208858
1696.027932	49.473715	64.213863
1695.481328	60.567083	64.218868
1694.204912	58.253062	64.223873
1693.612953	59.777256	64.228878
1692.721106	57.697031	64.233882
1692.828444	52.365848	64.238887
1691.380919	57.674828	64.243892
1690.662832	62.032206	64.248897
1690.484739	55.429664	64.253902
1689.687407	62.417246	64.258906
1689.695582	51.358824	64.263911
1688.353180	49.679732	64.268916
1687.623429	47.501228	64.273921
1687.471044	54.148260	64.278926
1686.413226	55.664451	64.283930
1685.211590	52.021866	64.288935
1684.708331	62.747247	64.293940
1684.189100	54.801776	64.298945
1684.005203	55.139997	64.303950
1683.359340	55.759742	64.308954
1682.359681	54.951841	64.313959
1681.772170	60.374949	64.318964
1681.306686	56.758934	64.323969
1680.952794	44.378259	64.328974
1679.443416	57.840060	64.333978
1678.805033	58.963219	64.338983
1678.423329	62.634842	64.343988
1677.867853	51.233885	64.348993
1677.532335	50.793559	64.353998
1676.164668	52.155552	64.359002
1675.680173	51.896577	64.364007
1675.175649	54.649465	64.369012
1674.270893	58.014679	64.374017
1674.483686	45.731642	64.379022
1673.145262	54.400970	64.384026
1672.455073	50.803304	64.389031
1672.096968	52.917953	64.394036
1670.788699	53.832143	64.399041
1669.963479	56.645432	64.404046
1669.017129	71.514276	64.409050
1669.097470	51.143964	64.414055
1668.905035	50.158965	64.419060
1668.231955	62.297396	64.424065
1667.727242	62.270281	64.429070
1666.903032	60.472621	64.434074
1666.289690	57.912950	64.439079
1665.586140	52.243814	64.444084
1664.318732	62.787815	64.449089
1664.027593	55.421102	64.454094
1663.254596	55.586406	64.459098
1662.945260	60.262044	64.464103
1661.647703	62.470730	64.469108
1660.664517	61.789524	64.474113
1660.574820	54.884377	64.479118
1659.877836	59.191103	64.484122
1659.767237	59.107694	64.489127
1658.626618	50.959754	64.494132
1657.935028	59.532652	64.499137
1657.766709	49.367976	64.504142
1656.879016	53.763338	64.509146
1655.516176	50.600516	64.514151
1655.369757	47.017401	64.519156
1654.516668	53.676392	64.524161
1654.346675	44.811333	64.529166
1653.633113	53.160648	64.534170
1652.761562	49.290614	64.539175
1651.532328	54.974925	64.544180
1651.115845	59.891501	64.549185
1651.147702	58.300045	64.554190
1650.318342	60.104797	64.559194
1649.340128	52.009907	64.564199
1648.855822	60.303888	64.569204
1648.152845	55.762134	64.574209
1647.683443	58.873707	64.579214
1646.507978	60.809128	64.584218
1646.105092	54.464641	64.589223
1645.680950	57.343531	64.594228
1644.445913	60.731259	64.599233
1644.110656	49.456175	64.604238
1642.999255	71.155465	64.609242
1642.684416	58.765431	64.614247
1642.159616	51.420072	64.619252
1642.077431	57.379474	64.624257
1640.904014	55.039658	64.629262
1640.041304	57.772184	64.634266
1639.572535	57.480757	64.639271
1639.147365	49.523515	64.644276
1638.329657	53.658619	64.649281
1637.789682	52.558527	64.654286
1637.293842	57.266946	64.659290
1636.166875	59.770229	64.664295
1635.327403	55.291160	64.669300
1634.620437	56.896710	64.674305
1634.236464	58.597601	64.679310
1633.620278	56.215000	64.684314
1632.908963	60.697466	64.689319
1632.095545	52.175878	64.694324
1631.120013	61.330025	64.699329
1630.807592	59.605612	64.704334
1630.513407	53.854112	64.709338
1629.990783	60.052206	64.714343
1628.989093	44.884035	64.719348
1627.847911	59.709712	64.724353
1627.877667	46.386631	64.729358
1626.818424	49.498869	64.734362
1625.960644	44.272123	64.739367
1625.569173	57.368712	64.744372
1624.977628	52.492312	64.749377
1624.813141	50.247684	64.754382
1623.323896	50.884732	64.759386
1622.863697	41.419262	64.764391
1622.284835	52.125112	64.769396
1621.804509	52.043672	64.774401
1621.129039	53.857100	64.779406
1620.216248	56.258558	64.784410
1619.634437	53.436860	64.789415
1619.278557	52.383218	64.794420
1618.781435	54.786450	64.799425
1617.892819	55.362777	64.804430
1616.713741	59.424415	64.809434
1616.371540	51.319962	64.814439
1616.083136	49.277938	64.819444
1614.996185	51.653451	64.824449
1614.474910	45.956956	64.829454
1613.636229	55.381086	64.834458
1613.270150	53.034449	64.839463
1612.291625	53.257649	64.844468
1611.237245	62.843777	64.849473
1611.434065	46.053413	64.854478
1610.764987	51.300263	64.859482
1610.218628	51.959408	64.864487
1608.891981	48.057615	64.869492
1608.122350	58.487864	64.874497
1607.999870	45.414465	64.879502
1607.214858	54.937297	64.884506
1606.247075	51.369560	64.889511
1605.790927	51.998606	64.894516
1605.236237	55.995746	64.899521
1604.939528	46.076972	64.904526
1603.967825	59.030787	64.909530
1603.195769	42.745992	64.914535
1602.611309	50.256407	64.919540
1601.994316	56.759640	64.924545
1600.827492	52.392511	64.929550
1599.951396	63.360047	64.934554
1599.653061	41.640193	64.939559
1599.253017	47.341018	64.944564
1598.971118	58.474337	64.949569
1598.587951	48.544068	64.954574
1597.192321	50.590177	64.959578
1596.529285	49.268383	64.964583
1595.960078	47.371893	64.969588
1594.983050	46.129944	64.974593
1594.622455	46.728043	64.979598
1593.905771	48.466027	64.984602
1593.694489	47.007813	64.989607
1592.372133	48.018891	64.994612
1591.706324	39.756137	64.999617
1591.320654	54.761397	65.004622
1591.077066	45.129063	65.009626
1590.128561	47.294942	65.014631
1589.151347	51.985230	65.019636
1588.397888	54.221044	65.024641
1587.880734	44.294721	65.029646
1587.299881	44.573017	65.034650
1587.005543	49.749297	65.039655
1585.818229	46.812505	65.044660
1585.255605	50.530224	65.049665
1585.026815	34.636930	65.054670
1584.125031	51.764658	65.059674
1583.296759	40.104322	65.064679
1582.847074	42.851664	65.069684
1582.001417	43.883202	65.074689
1581.873701	39.399883	65.079694
1580.468174	56.074664	65.084698
1579.656926	45.351439	65.089703
1579.434747	49.259486	65.094708
1578.942485	51.963135	65.099713
1577.958941	53.324072	65.104718
1576.897469	54.796733	65.109722
1576.157904	57.191184	65.114727
1576.015576	53.746191	65.119732
1575.662479	48.022986	65.124737
1575.462553	46.785308	65.129742
1574.336492	49.911336	65.134746
1573.536967	51.282460	65.139751
1572.771031	42.127339	65.144756
1571.973401	52.437465	65.149761
1571.199380	41.884942	65.154766
1570.470320	50.760255	65.159770
1570.130641	48.942416	65.164775
1570.108290	48.742494	65.169780
1569.090604	50.395849	65.174785
1568.227984	45.590920	65.179790
1567.743265	57.412441	65.184794
1567.001621	47.509174	65.189799
1565.906951	48.496706	65.194804
1564.815613	53.142059	65.199809
1564.758041	38.637597	65.204814
1564.395905	36.719254	65.209818
1563.969977	37.089629	65.214823
1562.859549	45.848923	65.219828
1561.960989	45.267846	65.224833
1561.524854	44.351537	65.229838
1560.887273	56.247805	65.234842
1560.215705	48.867445	65.239847
1559.658445	45.234503	65.244852
1558.761218	50.736797	65.249857
1558.489489	47.201985	65.254862
1557.808993	56.471692	65.259866
1556.722995	49.395287	65.264871
1556.367817	43.175703	65.269876
1555.625661	54.626561	65.274881
1555.377959	37.665578	65.279886
1554.018949	48.823376	65.284890
1553.470276	47.737300	65.289895
1552.841476	43.279984	65.294900
1552.525205	56.965414	65.299905
1552.044140	48.433631	65.304910
1550.723466	54.321737	65.309914
1550.055572	51.382854	65.314919
1550.024643	46.803737	65.319924
1549.104588	50.360644	65.324929
1548.265852	41.833658	65.329934
1547.450471	45.107442	65.334938
1547.076259	39.829125	65.339943
1547.157843	42.938316	65.344948
1546.087332	37.354339	65.349953
1545.190558	32.368778	65.354958
1544.659403	43.279927	65.359962
1543.462147	41.054330	65.364967
1542.779796	49.520124	65.369972
1542.388908	42.833154	65.374977
1542.198028	39.756985	65.379982
1541.047027	41.347959	65.384986
1539.986280	45.250481	65.389991
1539.442450	41.875595	65.394996
1538.518858	49.034647	65.400001
1538.559236	48.771145	65.405006
1538.276163	50.069681	65.410010
1537.353525	52.691916	65.415015
1536.516974	50.893109	65.420020
1535.680000	48.503041	65.425025
1535.227169	53.146295	65.430030
1534.462577	47.860624	65.435034
1533.029633	61.480649	65.440039
1532.941857	46.829604	65.445044
1532.489728	58.491416	65.450049
1532.385675	39.951237	65.455054
1531.704678	55.135879	65.460058
1530.656171	53.014378	65.465063
1530.085519	49.989090	65.470068
1529.055250	54.389799	65.475073
1528.394144	53.737889	65.480078
1527.508648	51.078003	65.485082
1526.948610	51.852874	65.490087
1526.596692	49.499272	65.495092
1525.663471	58.962099	65.500097
1525.586631	52.576871	65.505102
1524.574088	48.790786	65.510106
1524.055293	56.607734	65.515111
1523.873271	49.458667	65.520116
1522.722367	44.925055	65.525121
1522.191595	44.832727	65.530126
1521.313520	55.193492	65.535130
1520.627220	46.840979	65.540135
1519.376817	47.252487	65.545140
1518.662914	53.428949	65.550145
1518.458594	56.490535	65.555150
1517.636097	60.259022	65.560154
1517.803177	51.722024	65.565159
1517.317709	52.527624	65.570164
1516.255669	57.420641	65.575169
1515.712064	50.120883	65.580174
1514.404511	52.785365	65.585178
1513.466007	52.377801	65.590183
1512.856091	46.887795	65.595188
1512.049561	49.477397	65.600193
1511.886280	46.228119	65.605198
1511.414366	51.352200	65.610202
1510.945907	45.658378	65.615207
1510.394397	44.162776	65.620212
1509.532229	48.532048	65.625217
1509.165139	43.167455	65.630222
1508.811238	48.230207	65.635226
1507.349819	47.675513	65.640231
1506.842472	44.450949	65.645236
1506.140386	52.678625	65.650241
1505.302391	52.731308	65.655246
1504.581626	58.863136	65.660250
1503.902768	52.393809	65.665255
1503.543709	44.812433	65.670260
1502.905972	49.893482	65.675265
1502.015938	49.391491	65.680270
1501.013705	50.101023	65.685274
1500.610617	48.427304	65.690279
1500.354914	46.846855	65.695284
1499.744661	49.403693	65.700289
1498.848052	56.410246	65.705294
1497.990128	56.940737	65.710298
1497.659086	57.196702	65.715303
1497.309469	57.674804	65.720308
1496.080301	53.532089	65.725313
1495.492325	54.010223	65.730318
1495.054063	54.150769	65.735322
1494.329653	64.023527	65.740327
1493.377077	47.289673	65.745332
1492.518658	54.824717	65.750337
1492.080223	51.516668	65.755342
1491.840091	45.603650	65.760346
1491.275326	46.311474	65.765351
1490.474541	46.588472	65.770356
1489.332655	46.184852	65.775361
1489.173461	53.537824	65.780366
1487.898086	55.602725	65.785370
1487.381441	47.958087	65.790375
1487.220727	45.827985	65.795380
1486.310096	60.550836	65.800385
1485.688345	50.836694	65.805390
1484.573092	57.296129	65.810394
1484.214685	49.424506	65.815399
1483.584340	48.403462	65.820404
1482.634662	51.589802	65.825409
1482.745860	48.859852	65.830414
1481.722741	42.956151	65.835418
1480.804377	54.559596	65.840423
1480.727438	42.158620	65.845428
1479.940510	55.037367	65.850433
1479.099656	44.150165	65.855438
1478.420742	37.953661	65.860442
1477.928953	52.887477	65.865447
1477.131821	43.403053	65.870452
1475.780982	53.255513	65.875457
1475.346982	42.068706	65.880462
1475.085769	49.527770	65.885466
1474.652065	52.785074	65.890471
1474.222617	42.770737	65.895476
1473.025718	47.746695	65.900481
1472.676648	48.729312	65.905486
1471.791411	56.142475	65.910490
1470.560567	48.675991	65.915495
1470.443685	49.031960	65.920500
1469.356711	49.433289	65.925505
1469.438013	36.767487	65.930510
1468.946619	49.287045	65.935514
1467.598965	45.748197	65.940519
1466.982434	41.282649	65.945524
1466.179817	40.203836	65.950529
1466.247813	45.835023	65.955534
1464.889169	53.403840	65.960538
1463.869209	45.394518	65.965543
1463.697134	46.251243	65.970548
1463.388238	53.402512	65.975553
1463.243446	43.320864	65.980558
1462.285727	49.594428	65.985562
1461.236318	47.149842	65.990567
1460.716582	45.579819	65.995572
1459.413518	45.324823	66.000577
1459.033177	33.563402	66.005582
1458.259787	49.688352	66.010586
1457.656295	52.825992	66.015591
1457.658904	49.575585	66.020596
1456.870806	48.913915	66.025601
1456.016099	39.998443	66.030606
1455.099148	44.751731	66.035610
1454.725349	47.291500	66.040615
1453.842204	42.399995	66.045620
1452.702118	56.473375	66.050625
1452.514286	46.485295	66.055630
1452.301370	50.308301	66.060634
1451.678205	42.969172	66.065639
1450.683954	47.643289	66.070644
1449.886768	42.821699	66.075649
1449.681489	48.108405	66.080654
1448.633427	50.589761	66.085658
1447.937487	53.048271	66.090663
1447.329153	50.561976	66.095668
1446.498669	52.799031	66.100673
1446.411862	41.733664	66.105678
1445.140244	48.003505	66.110682
1444.148907	43.370460	66.115687
1443.922272	38.224821	66.120692
1443.383806	53.347396	66.125697
1442.896686	44.020288	66.130702
1441.979011	52.482501	66.135706
1441.193510	54.844865	66.140711
1440.799061	48.407628	66.145716
1440.075116	59.240633	66.150721
1438.982959	47.385764	66.155726
1438.357159	53.434706	66.160730
1437.831301	47.004163	66.165735
1437.581101	49.046498	66.170740
1437.178708	49.078856	66.175745
1436.661113	52.464609	66.180750
1435.843648	46.236522	66.185754
1434.703632	53.603457	66.190759
1433.899422	48.398231	66.195764
1432.806848	53.374972	66.200769
1432.597805	45.794999	66.205774
1432.277113	54.794662	66.210778
1431.858490	52.771782	66.215783
1430.943430	46.836736	66.220788
1430.025409	64.006505	66.225793
1429.556273	49.832383	66.230798
1429.214053	53.005770	66.235802
1427.748453	49.509342	66.240807
1427.284082	49.835389	66.245812
1426.435293	53.317934	66.250817
1426.207110	47.461371	66.255822
1425.995879	51.273073	66.260826
1424.938331	56.614816	66.265831
1424.097425	46.933953	66.270836
1423.651443	49.806881	66.275841
1423.074312	46.101442	66.280846
1421.910028	53.182094	66.285850
1421.354430	44.151290	66.290855
1420.751325	45.082830	66.295860
1420.117194	50.853992	66.300865
1419.937384	46.765301	66.305870
1418.978398	43.005443	66.310874
1418.257146	46.827245	66.315879
1417.818696	39.556538	66.320884
1417.212056	49.588767	66.325889
1415.801252	44.503612	66.330894
1415.384025	54.704427	66.335898
1414.885488	42.982296	66.340903
1414.717322	41.726971	66.345908
1413.528979	45.675049	66.350913
1413.068335	46.008391	66.355918
1412.213639	48.649828	66.360922
1411.775421	53.461077	66.365927
1411.692917	42.112771	66.370932
1410.244288	44.191053	66.375937
1409.543249	41.642237	66.380942
1408.969825	41.711245	66.385946
1408.213432	46.762287	66.390951
1407.972508	45.993165	66.395956
1406.863610	53.687884	66.400961
1406.778265	44.788911	66.405966
1405.376648	50.749866	66.410970
1404.582105	53.481089	66.415975
1404.003044	41.658227	66.420980
1403.644517	51.031313	66.425985
1403.551546	45.627902	66.430990
1402.769813	43.848812	66.435994
1401.567216	57.766572	66.440999
1401.344306	45.224813	66.446004
1400.560684	47.566389	66.451009
1399.257747	46.732691	66.456014
1398.639568	54.527603	66.461018
1397.962746	47.619620	66.466023
1397.635724	47.726733	66.471028
1397.476932	60.825765	66.476033
1396.720143	45.489494	66.481038
1395.972246	57.611462	66.486042
1395.372126	47.367241	66.491047
1394.918976	47.598475	66.496052
1393.487468	50.664320	66.501057
1392.424130	57.710018	66.506062
1392.345637	45.884859	66.511066
1391.905305	53.993685	66.516071
1391.604637	47.055876	66.521076
1390.533179	43.485786	66.526081
1389.970240	49.488475	66.531086
1389.435457	50.040175	66.536090
1388.607750	52.313073	66.541095
1387.574421	41.229439	66.546100
1386.662527	49.544097	66.551105
1386.511523	42.801687	66.556110
1386.472192	49.771346	66.561114
1385.604876	51.320449	66.566119
1384.518329	40.298890	66.571124
1383.540195	50.421711	66.576129
1383.246083	47.218471	66.581134
1383.052203	45.301796	66.586138
1381.771976	43.169886	66.591143
1380.926179	40.678780	66.596148
1380.500211	45.678884	66.601153
1380.222218	50.305403	66.606158
1378.811737	45.302216	66.611162
1377.927278	46.235913	66.616167
1377.795745	47.827328	66.621172
1377.119208	49.943743	66.626177
1376.796042	41.803209	66.631182
1376.587902	46.003907	66.636186
1375.810400	52.925330	66.641191
1375.119050	40.300354	66.646196
1374.058943	52.583906	66.651201
1372.634078	43.429530	66.656206
1372.306149	45.621413	66.661210
1371.512553	50.924371	66.666215
1371.868830	46.242719	66.671220
1371.243119	55.711894	66.676225
1370.362048	43.527061	66.681230
1369.317972	53.895323	66.686234
1368.685190	44.335937	66.691239
1368.180296	43.742813	66.696244
1366.946940	42.100175	66.701249
1366.603030	38.767668	66.706254
1366.054529	46.600387	66.711258
1365.384598	38.794085	66.716263
1364.937067	36.239678	66.721268
1364.065238	37.390556	66.726273
1363.522238	44.342507	66.731278
1363.282065	33.254232	66.736282
1361.996189	54.837789	66.741287
1361.457585	39.643468	66.746292
1360.907383	51.943736	66.751297
1360.180531	45.488397	66.756302
1359.396719	42.271546	66.761306
1358.429780	43.757649	66.766311
1358.174166	33.759870	66.771316
1357.607921	53.650588	66.776321
1357.068856	43.519674	66.781326
1355.694590	53.434252	66.786330
1354.976546	47.933097	66.791335
1354.416942	36.703221	66.796340
1354.546675	55.948749	66.801345
1354.180919	49.809729	66.806350
1353.006925	41.479614	66.811354
1352.110593	52.593908	66.816359
1351.700840	30.059283	66.821364
1350.882551	53.736707	66.826369
1349.615559	43.781429	66.831374
1349.077254	56.723174	66.836378
1348.352376	51.090650	66.841383
1348.303287	50.544915	66.846388
1347.833242	46.232724	66.851393
1347.479030	54.242713	66.856398
1346.561528	47.896527	66.861402
1345.499455	45.510772	66.866407
1345.237768	39.793585	66.871412
1343.739849	51.277886	66.876417
1343.399815	44.641221	66.881422
1342.818129	47.105246	66.886426
1342.449366	51.766696	66.891431
1342.080504	40.463924	66.896436
1340.911298	47.969564	66.901441
1340.195037	47.321741	66.906446
1339.768511	49.016818	66.911450
1339.143489	49.601796	66.916455
1338.290598	40.279253	66.921460
1337.640605	45.857418	66.926465
1336.914921	46.496243	66.931470
1336.839488	46.202265	66.936474
1335.575024	44.389555	66.941479
1335.010672	54.109163	66.946484
1334.113354	45.198937	66.951489
1333.977002	49.194270	66.956494
1333.615005	41.780548	66.961498
1331.666857	54.449700	66.966503
1331.656798	37.542462	66.971508
1330.817266	53.296343	66.976513
1330.651365	43.806246	66.981518
1329.626467	51.599595	66.986522
1328.829942	43.734583	66.991527
1328.859447	47.455981	66.996532
1328.097662	47.081889	67.001537
1327.203183	53.771197	67.006542
1326.301378	50.497423	67.011546
1325.457792	45.170771	67.016551
1325.151283	38.008416	67.021556
1324.615698	51.309251	67.026561
1324.212338	39.048501	67.031566
1323.062483	49.070909	67.036570
1322.706085	47.471797	67.041575
1321.935669	50.930874	67.046580
1320.851338	45.989408	67.051585
1320.399558	44.514263	67.056590
1320.099276	42.188755	67.061594
1318.884255	41.922987	67.066599
1318.465744	40.869886	67.071604
1317.692439	45.641378	67.076609
1317.116222	41.841212	67.081614
1316.866901	36.681853	67.086618
1316.116918	52.612301	67.091623
1315.166369	43.355751	67.096628
1314.021823	52.264051	67.101633
1314.000621	46.048188	67.106638
1313.428766	54.255196	67.111642
1312.292754	48.396325	67.116647
1311.472043	46.342779	67.121652
1310.687456	50.296095	67.126657
1310.751492	51.889536	67.131662
1310.585387	45.844936	67.136666
1309.368432	45.536905	67.141671
1308.700397	50.771034	67.146676
1308.004236	45.947625	67.151681
1307.232192	48.277926	67.156686
1306.329213	42.022487	67.161690
1305.370593	51.915158	67.166695
1305.442781	45.490495	67.171700
1305.079889	42.025404	67.176705
1304.268221	47.405363	67.181710
1303.253031	45.742264	67.186714
1302.767132	48.332987	67.191719
1302.171084	52.366714	67.196724
1301.051675	45.040298	67.201729
1300.314783	54.276435	67.206734
1300.111910	52.528345	67.211738
1299.519900	56.657620	67.216743
1299.107911	48.288382	67.221748
1298.061835	59.398116	67.226753
1297.490185	48.182780	67.231758
1297.196775	51.012547	67.236762
1295.782242	51.573251	67.241767
1295.209467	55.710507	67.246772
1294.267254	60.687050	67.251777
1293.915625	50.736075	67.256782
1293.447230	46.065685	67.261786
1293.347228	58.248659	67.266791
1292.387441	41.541300	67.271796
1291.657922	50.208590	67.276801
1290.773519	45.703683	67.281806
1289.872111	59.538903	67.286810
1288.912791	52.694790	67.291815
1288.774729	50.053350	67.296820
1288.067808	59.827171	67.301825
1288.012029	48.383172	67.306830
1287.295703	48.869144	67.311834
1286.165352	59.544449	67.316839
1285.811663	45.930736	67.321844
1284.768031	56.585945	67.326849
1283.846574	51.289033	67.331854
1283.310640	50.486406	67.336858
1282.928710	49.313960	67.341863
1282.384974	42.990377	67.346868
1281.203944	43.149708	67.351873
1280.850222	46.335976	67.356878
1280.213364	53.484205	67.361882
1279.702155	64.806938	67.366887
1278.796055	36.292909	67.371892
1277.810951	51.284660	67.376897
1277.283649	47.352153	67.381902
1277.080229	47.103756	67.386906
1276.774047	59.437775	67.391911
1275.805082	48.758677	67.396916
1274.538488	60.931599	67.401921
1273.976428	53.921834	67.406926
1274.004650	52.133851	67.411930
1273.249013	57.153271	67.416935
1272.050510	52.308821	67.421940
1271.200246	49.550395	67.426945
1270.762191	47.970581	67.431950
1270.816717	45.358444	67.436954
1269.707017	52.204981	67.441959
1269.419322	38.410486	67.446964
1268.838952	48.023840	67.451969
1267.724969	48.375933	67.456974
1266.936121	48.629026	67.461978
1266.178611	52.825619	67.466983
1265.857599	39.962043	67.471988
1264.347889	47.067711	67.476993
1263.634569	54.955038	67.481998
1263.463019	41.760207	67.487002
1262.939303	45.487564	67.492007
1262.699039	50.297316	67.497012
1262.099963	51.125755	67.502017
1261.470563	47.103834	67.507022
1260.857717	46.502666	67.512026
1259.807803	48.995426	67.517031
1258.871267	51.310895	67.522036
1258.169518	49.143840	67.527041
1257.464016	46.472783	67.532046
1257.345521	54.498911	67.537050
1256.627914	57.165906	67.542055
1255.541420	45.750186	67.547060
1254.831724	50.074789	67.552065
1254.492532	48.070850	67.557070
1254.139926	53.385718	67.562074
1253.131400	55.810403	67.567079
1252.653430	44.796221	67.572084
1251.797908	56.999976	67.577089
1250.964375	48.284636	67.582094
1250.398682	46.925383	67.587098
1249.561336	52.672121	67.592103
1249.007862	48.914084	67.597108
1248.532718	50.984316	67.602113
1248.250587	40.598132	67.607118
1247.176560	50.657393	67.612122
1246.472820	52.834932	67.617127
1246.250078	36.713696	67.622132
1245.340573	45.288192	67.627137
1244.205981	43.085891	67.632142
1243.945403	40.317288	67.637146
1242.958731	54.342679	67.642151
1242.966996	39.424129	67.647156
1242.199459	47.862519	67.652161
1241.305561	47.077398	67.657166
1240.913773	37.481320	67.662170
1239.641301	46.654397	67.667175
1238.915828	34.746076	67.672180
1238.009988	49.610119	67.677185
1237.640885	33.527929	67.682190
1237.373820	52.995780	67.687194
1237.226489	43.417595	67.692199
1236.454149	43.078324	67.697204
1235.363875	48.163575	67.702209
1234.712855	58.504072	67.707214
1233.599320	40.014101	67.712218
1232.615431	48.073756	67.717223
1232.437599	47.556380	67.722228
1231.652691	52.053788	67.727233
1231.305441	49.339965	67.732238
1231.283279	42.124529	67.737242
1230.325804	54.781290	67.742247
1229.687485	39.721140	67.747252
1228.531431	54.128262	67.752257
1228.039036	54.573912	67.757262
1227.069950	53.270924	67.762266
1226.276918	50.306304	67.767271
1226.161943	52.417036	67.772276
1225.567315	45.507080	67.777281
1225.068374	45.977425	67.782286
1224.209905	43.704420	67.787290
1223.499826	54.424871	67.792295
1222.947915	48.458975	67.797300
1221.949809	39.776130	67.802305
1221.579550	45.951621	67.807310
1221.115877	35.119676	67.812314
1219.791504	49.509410	67.817319
1219.101646	33.962329	67.822324
1218.376685	51.169223	67.827329
1217.691561	43.322810	67.832334
1217.547078	46.803800	67.837338
1217.073023	52.961108	67.842343
1216.688308	35.850133	67.847348
1215.647767	41.990290	67.852353
1215.137253	36.516108	67.857358
1214.474695	42.807460	67.862362
1213.268460	52.931909	67.867367
1213.034608	46.297307	67.872372
1212.083660	58.546206	67.877377
1211.180108	46.055956	67.882382
1210.444884	52.866620	67.887386
1209.644120	48.756852	67.892391
1209.447145	54.376541	67.897396
1209.105089	43.876897	67.902401
1208.539745	46.585918	67.907406
1207.811587	46.427277	67.912410
1206.886591	48.512283	67.917415
1206.509882	30.461808	67.922420
1205.641511	32.220858	67.927425
1204.489822	42.795497	67.932430
1204.077062	34.792247	67.937434
1203.370540	43.995182	67.942439
1203.270930	42.670628	67.947444
1202.678715	45.879060	67.952449
1201.868856	44.471918	67.957454
1201.311903	38.227729	67.962458
1199.732250	37.201608	67.967463
1199.143753	40.373180	67.972468
1198.490600	36.864386	67.977473
1197.793696	42.683413	67.982478
1197.958574	36.918917	67.987482
1197.110796	45.329076	67.992487
1197.043444	36.621230	67.997492
1195.809081	38.201955	68.002497
1194.837535	38.493584	68.007502
1194.548094	41.830478	68.012506
1193.328932	39.606959	68.017511
1192.421764	34.022407	68.022516
1191.919261	45.643352	68.027521
1191.783984	48.219334	68.032526
1191.446379	44.046959	68.037530
1190.770660	46.303630	68.042535
1190.112171	51.559918	68.047540
1189.488127	44.876990	68.052545
1188.404937	49.078086	68.057550
1187.622161	39.578888	68.062554
1186.820396	36.569945	68.067559
1186.314348	36.256147	68.072564
1185.899341	42.266877	68.077569
1185.131084	40.512522	68.082574
1184.383110	35.892929	68.087578
1183.509008	45.926720	68.092583
1183.226170	40.533027	68.097588
1182.829077	49.133281	68.102593
1181.504972	51.289650	68.107598
1181.148294	42.621506	68.112602
1180.251379	44.531753	68.117607
1180.071019	44.850522	68.122612
1179.363005	49.070802	68.127617
1178.820218	45.646957	68.132622
1178.466409	49.358346	68.137626
1177.351745	56.801764	68.142631
1176.149788	45.458064	68.147636
1175.679702	47.054443	68.152641
1175.376135	48.327890	68.157646
1174.426867	42.943991	68.162650
1173.393811	51.225938	68.167655
1173.015381	39.640897	68.172660
1172.835850	36.242861	68.177665
1172.250987	49.557848	68.182670
1171.009302	36.567919	68.187674
1170.183739	51.808697	68.192679
1169.895844	48.547733	68.197684
1169.501636	48.501565	68.202689
1168.866354	39.179181	68.207694
1168.072491	51.601787	68.212698
1166.986087	60.926651	68.217703
1166.848167	48.350927	68.222708
1166.030369	55.579989	68.227713
1164.954630	48.770217	68.232718
1164.698268	43.558386	68.237722
1163.974548	40.122322	68.242727
1163.496766	50.965100	68.247732
1162.078369	55.746192	68.252737
1161.744469	44.215567	68.257742
1161.680740	44.903698	68.262746
1161.017604	53.077937	68.267751
1160.047109	40.388639	68.272756
1159.280317	49.632708	68.277761
1158.560181	41.427628	68.282766
1158.634257	38.222636	68.287770
1157.308893	53.162880	68.292775
1156.387916	38.529317	68.297780
1156.214689	47.278461	68.302785
1155.648628	54.497449	68.307790
1154.491845	41.850396	68.312794
1153.638059	49.244444	68.317799
1153.130513	47.670974	68.322804
1152.580113	43.559255	68.327809
1152.369501	47.678358	68.332814
1151.814906	39.404379	68.337818
1150.515782	50.587507	68.342823
1150.065162	33.345121	68.347828
1149.482238	46.344425	68.352833
1148.814567	54.669190	68.357838
1148.091226	43.358193	68.362842
1147.267315	57.540640	68.367847
1147.128358	52.139834	68.372852
1146.144748	48.328814	68.377857
1144.976240	58.521404	68.382862
1144.460118	48.946694	68.387866
1144.124807	50.761328	68.392871
1143.981733	52.222129	68.397876
1143.304895	48.479009	68.402881
1142.176735	48.328814	68.407886
1141.796763	46.022312	68.412890
1140.703074	44.415918	68.417895
1139.898437	34.412469	68.422900
1139.322414	50.636948	68.427905
1138.313145	54.842076	68.432910
1138.390974	42.840720	68.437914
1137.785381	45.696497	68.442919
1136.923107	42.588390	68.447924
1136.129419	50.690360	68.452929
1135.464808	50.143184	68.457934
1135.502720	49.105827	68.462938
1134.109667	64.198773	68.467943
1133.720007	41.325152	68.472948
1133.548850	45.122605	68.477953
1132.138063	60.502205	68.482958
1131.134028	38.908955	68.487962
1130.398450	56.183781	68.492967
1129.873836	50.894775	68.497972
1129.941051	51.872724	68.502977
1129.168343	46.815558	68.507982
1128.264595	43.501173	68.512986
1127.651166	58.916371	68.517991
1127.384717	53.002863	68.522996
1126.398665	48.157816	68.528001
1125.339830	50.864923	68.533006
1124.622105	53.514624	68.538010
1124.212240	42.730912	68.543015
1123.946616	51.050078	68.548020
1122.988976	53.321645	68.553025
1121.926475	45.532133	68.558030
1121.842813	49.839191	68.563034
1121.361941	55.064090	68.568039
1120.772317	45.595693	68.573044
1119.692482	46.150565	68.578049
1118.952884	57.230525	68.583054
1118.624203	42.286741	68.588058
1117.338245	61.222826	68.593063
1116.880446	58.741057	68.598068
1116.243835	50.566856	68.603073
1115.826386	53.788508	68.608078
1115.683869	45.166735	68.613082
1114.579456	56.411947	68.618087
1113.664505	44.226318	68.623092
1113.340076	51.324881	68.628097
1112.148583	55.303550	68.633102
1111.375195	45.239945	68.638106
1110.355765	57.107119	68.643111
1110.011621	50.772334	68.648116
1109.911461	53.478344	68.653121
1109.467900	46.169102	68.658126
1109.343087	49.717925	68.663130
1108.184171	46.467787	68.668135
1107.556570	46.980694	68.673140
1106.036182	40.093455	68.678145
1105.238923	48.304802	68.683150
1104.641422	50.260486	68.688154
1104.215552	45.873520	68.693159
1104.395579	46.691606	68.698164
1103.448854	38.200909	68.703169
1102.552715	47.128112	68.708174
1101.816182	44.421040	68.713178
1101.034482	48.897472	68.718183
1100.953347	43.206796	68.723188
1099.916548	40.668905	68.728193
1099.296987	50.094559	68.733198
1098.982282	50.554545	68.738202
1097.794599	48.330797	68.743207
1097.226399	48.014288	68.748212
1096.653349	43.294363	68.753217
1095.779442	50.778355	68.758222
1095.676441	49.142126	68.763226
1094.434602	47.959841	68.768231
1093.749953	52.092850	68.773236
1092.944644	47.860852	68.778241
1092.576509	51.956131	68.783246
1092.480777	47.354237	68.788250
1091.438213	51.791746	68.793255
1090.664193	45.339275	68.798260
1090.249552	46.278757	68.803265
1089.310932	51.024567	68.808270
1088.961472	44.782093	68.813274
1088.083420	62.333468	68.818279
1087.381542	59.209323	68.823284
1086.487596	45.791986	68.828289
1085.444711	53.878417	68.833294
1085.619306	48.657966	68.838298
1084.861890	56.076128	68.843303
1084.458622	47.855361	68.848308
1083.231149	50.426892	68.853313
1082.348445	60.851571	68.858318
1082.249864	50.059350	68.863322
1081.738394	52.975857	68.868327
1080.796059	40.547036	68.873332
1080.107230	48.023667	68.878337
1079.784891	50.837554	68.883342
1078.941268	49.719659	68.888346
1077.720276	59.870162	68.893351
1077.314999	45.443168	68.898356
1076.841788	58.473921	68.903361
1076.229138	58.203908	68.908366
1075.493501	42.599512	68.913370
1074.362933	51.273872	68.918375
1073.627172	38.348597	68.923380
1073.434992	52.458945	68.928385
1073.242023	47.349001	68.933390
1072.661005	40.006446	68.938394
1071.322034	47.736300	68.943399
1070.898927	39.939719	68.948404
1070.389893	32.426455	68.953409
1069.531947	41.962565	68.958414
1069.047729	35.829840	68.963418
1068.268550	40.479332	68.968423
1067.270487	45.818043	68.973428
1066.400562	51.882231	68.978433
1065.751838	45.099196	68.983438
1065.848444	33.664116	68.988442
1064.959594	44.291604	68.993447
1064.594146	49.376729	68.998452
1063.611356	41.513071	69.003457
1062.593652	55.630168	69.008462
1062.394630	40.538051	69.013466
1061.595472	37.782612	69.018471
1060.726380	43.258495	69.023476
1060.188949	41.711875	69.028481
1059.437472	47.148551	69.033486
1059.439175	45.268600	69.038490
1058.164633	57.020260	69.043495
1057.618299	42.998893	69.048500
1057.121278	40.245852	69.053505
1056.373159	48.660692	69.058510
1055.652767	44.762111	69.063514
1054.707119	57.421765	69.068519
1054.128288	45.647870	69.073524
1053.992296	50.128824	69.078529
1052.559857	48.825501	69.083534
1052.031326	41.264879	69.088538
1050.849466	45.062277	69.093543
1050.768993	40.271891	69.098548
1050.278509	38.785611	69.103553
1049.870509	47.786553	69.108558
1049.821621	45.859460	69.113562
1048.739083	40.224020	69.118567
1048.048994	44.285367	69.123572
1047.318756	51.041658	69.128577
1046.239281	46.981018	69.133582
1045.995831	42.956109	69.138586
1045.312854	44.922248	69.143591
1044.215190	46.176963	69.148596
1043.740172	52.219333	69.153601
1043.086236	43.600087	69.158606
1042.886791	47.130822	69.163610
1041.531249	49.483062	69.168615
1040.932726	42.274181	69.173620
1040.126089	45.474180	69.178625
1039.619252	40.373176	69.183630
1039.381573	45.559394	69.188634
1038.349937	44.564459	69.193639
1037.602046	41.655800	69.198644
1037.032930	32.592584	69.203649
1036.407190	42.530130	69.208654
1036.495351	36.440389	69.213658
1035.477575	42.930203	69.218663
1034.678340	43.003680	69.223668
1033.870441	37.039145	69.228673
1032.758768	54.093127	69.233678
1032.317255	38.497155	69.238682
1031.794421	49.637251	69.243687
1031.359706	45.392049	69.248692
1031.124290	44.079648	69.253697
1029.669773	46.286799	69.258702
1028.850443	36.661027	69.263706
1028.414860	55.390887	69.268711
1027.992418	43.079643	69.273716
1027.281981	44.734783	69.278721
1026.109251	49.245059	69.283726
1025.721251	46.603983	69.288730
1025.333554	45.978091	69.293735
1024.936834	37.381009	69.298740
1023.984021	46.992146	69.303745
1022.878303	48.341186	69.308750
1022.604428	42.242812	69.313754
1022.245559	43.714296	69.318759
1021.852821	34.664023	69.323764
1020.617957	41.245145	69.328769
1020.012999	45.781783	69.333774
1019.703296	42.648884	69.338778
1018.432858	51.214636	69.343783
1017.733044	49.216069	69.348788
1017.536413	38.644458	69.353793
1016.645660	40.877035	69.358798
1016.105838	31.468565	69.363802
1015.009239	46.306228	69.368807
1014.709488	51.611128	69.373812
1014.434076	39.208695	69.378817
1013.329081	48.855085	69.383822
1012.492077	30.911022	69.388826
1011.765073	45.420241	69.393831
1011.425099	30.673829	69.398836
1011.221903	40.577266	69.403841
1010.016344	41.858622	69.408846
1009.283214	44.028280	69.413850
1008.579865	48.694109	69.418855
1008.157942	43.111273	69.423860
1007.458571	39.903185	69.428865
1006.318136	48.918163	69.433870
1006.375276	24.876037	69.438874
1005.548735	49.267528	69.443879
1004.895430	49.246838	69.448884
1004.070171	37.701399	69.453889
1003.284289	49.356406	69.458894
1002.934115	40.204751	69.463898
1002.049592	38.707059	69.468903
1001.305871	40.293388	69.473908
1000.683611	34.691970	69.478913
999.899404	38.274743	69.483918
999.577083	32.690258	69.488922
999.322271	46.007935	69.493927
998.606614	45.286001	69.498932
997.762493	33.934369	69.503937
996.919924	43.736117	69.508942
996.225055	35.648500	69.513946
995.236954	44.000612	69.518951
994.765511	35.606228	69.523956
994.306693	31.582480	69.528961
993.480758	39.088821	69.533966
992.730632	28.810276	69.538970
992.243658	35.925237	69.543975
991.675734	38.946928	69.548980
991.358342	27.777990	69.553985
990.095276	37.318650	69.558990
989.727711	32.928743	69.563994
989.204824	38.210798	69.568999
988.128451	44.367772	69.574004
987.052033	46.894813	69.579009
986.533118	40.609942	69.584014
986.294235	41.575089	69.589018
985.894227	43.079929	69.594023
985.225752	34.656976	69.599028
984.437153	45.027272	69.604033
983.829396	42.917881	69.609038
983.324395	40.298582	69.614042
981.963519	44.827773	69.619047
981.219503	38.988703	69.624052
981.070057	20.686130	69.629057
980.688162	34.954363	69.634062
980.189616	32.464920	69.639066
979.076895	38.779056	69.644071
978.438975	37.278405	69.649076
977.801619	29.979540	69.654081
976.325609	39.030569	69.659086
975.985775	32.865436	69.664090
975.290254	27.783436	69.669095
974.898267	39.438843	69.674100
975.094891	27.831752	69.679105
974.044875	34.403979	69.684110
972.985305	38.773273	69.689114
971.943253	34.539570	69.694119
972.007676	30.975015	69.699124
971.870706	35.202245	69.704129
970.369318	40.766142	69.709134
969.867369	35.453080	69.714138
969.261255	39.606731	69.719143
968.014737	32.420562	69.724148
967.503231	39.127870	69.729153
966.840934	41.880747	69.734158
966.746155	30.408325	69.739162
966.396221	32.163805	69.744167
964.971442	42.283688	69.749172
964.576463	28.845379	69.754177
964.188545	47.362650	69.759182
963.720031	31.605435	69.764186
962.576757	29.401497	69.769191
961.796419	39.814631	69.774196
961.102547	28.018091	69.779201
959.779681	43.904115	69.784206
959.504884	42.487607	69.789210
959.002120	42.179640	69.794215
958.598172	42.975523	69.799220
958.420609	35.789571	69.804225
957.126120	50.133646	69.809230
956.558607	41.626829	69.814234
955.759975	34.689503	69.819239
955.527601	35.145867	69.824244
954.872528	43.112282	69.829249
953.535537	35.986244	69.834254
953.035426	39.109109	69.839258
952.799241	52.146298	69.844263
952.360387	44.049493	69.849268
951.475495	37.427073	69.854273
950.486916	39.574319	69.859278
950.473995	28.328560	69.864282
949.136949	37.422141	69.869287
948.297960	39.160831	69.874292
947.819695	38.262375	69.879297
947.293900	42.628742	69.884302
946.992229	33.141399	69.889306
945.935629	38.891563	69.894311
945.060491	33.623698	69.899316
945.055700	38.492178	69.904321
944.055963	44.018843	69.909326
943.339446	44.421366	69.914330
942.714442	31.639370	69.919335
941.982736	42.705478	69.924340
941.746754	35.066804	69.929345
940.300820	36.837423	69.934350
939.347683	32.378287	69.939354
938.960079	43.110537	69.944359
938.904154	31.512094	69.949364
938.725525	33.398006	69.954369
937.259843	41.034543	69.959374
936.595361	36.196758	69.964378
935.606096	42.018208	69.969383
935.348692	33.482556	69.974388
935.499588	34.218536	69.979393
934.524961	45.066273	69.984398
933.904609	41.984397	69.989402
932.842184	40.644342	69.994407
931.628430	41.796158	69.999412
930.948209	36.744849	70.004417
930.503639	47.303250	70.009422
930.734069	32.585935	70.014426
929.784670	36.160321	70.019431
928.929890	36.048716	70.024436
928.040061	36.521397	70.029441
927.312164	44.406372	70.034446
927.076114	36.293075	70.039450
926.272223	41.913152	70.044455
925.294793	38.567998	70.049460
924.855800	29.580303	70.054465
924.124483	38.965415	70.059470
923.422857	38.594488	70.064474
922.491902	38.401972	70.069479
921.902474	34.276028	70.074484
921.647368	29.713708	70.079489
920.961166	37.508472	70.084494
920.694953	31.856730	70.089498
919.598651	43.070741	70.094503
919.221750	35.197467	70.099508
918.631956	37.828436	70.104513
917.258914	40.757500	70.109518
916.759277	34.094290	70.114522
916.101915	36.540481	70.119527
915.718319	48.093642	70.124532
915.192259	32.657819	70.129537
913.933054	49.155017	70.134542
913.257391	36.095679	70.139546
912.850290	38.784304	70.144551
912.447168	34.828977	70.149556
912.259243	32.313771	70.154561
911.135691	47.226711	70.159566
910.329087	33.000836	70.164570
910.009270	36.303162	70.169575
908.841733	40.650241	70.174580
908.513744	24.211563	70.179585
907.850785	40.140811	70.184590
907.082250	31.289136	70.189594
906.147825	32.815957	70.194599
905.206698	42.653908	70.199604
905.208388	29.051573	70.204609
904.678101	44.180743	70.209614
903.874572	38.329096	70.214618
902.983134	45.812772	70.219623
902.081293	34.467215	70.224628
902.011925	45.735417	70.229633
900.996721	37.484358	70.234638
900.009433	33.287702	70.239642
899.794221	35.690340	70.244647
899.293762	35.930766	70.249652
898.846390	40.385580	70.254657
897.429442	35.382143	70.259662
896.893389	40.139635	70.264666
896.388633	46.289249	70.269671
895.930418	53.595184	70.274676
895.638073	34.478042	70.279681
894.569373	54.220076	70.284686
893.727460	38.038205	70.289690
893.325251	40.817513	70.294695
891.907408	48.996789	70.299700
891.578622	36.300125	70.304705
891.119280	43.483240	70.309710
890.736368	47.927799	70.314714
890.046252	50.147412	70.319719
889.270950	43.053439	70.324724
888.537391	38.206162	70.329729
887.852438	44.977354	70.334734
887.564387	45.947180	70.339738
886.355322	41.224460	70.344743
885.719384	34.291230	70.349748
885.416367	48.059673	70.354753
884.996986	40.443885	70.359758
883.814895	35.660108	70.364762
882.948199	44.775057	70.369767
882.270670	44.047089	70.374772
882.138850	30.721456	70.379777
881.471350	38.278298	70.384782
880.309876	30.720698	70.389786
879.850799	46.209101	70.394791
879.446137	41.030378	70.399796
879.255614	30.166109	70.404801
877.983787	40.340530	70.409806
877.499534	29.740615	70.414810
876.831596	45.408905	70.419815
875.747230	37.217748	70.424820
874.861062	43.790743	70.429825
874.073489	45.537042	70.434830
873.570875	34.361338	70.439834
873.093966	46.014499	70.444839
873.103660	40.673646	70.449844
872.946165	36.613007	70.454849
871.525606	46.139362	70.459854
870.772257	40.536770	70.464858
869.707163	40.283625	70.469863
868.771640	43.863709	70.474868
868.349086	42.369809	70.479873
867.950553	46.487292	70.484878
867.683267	33.355097	70.489882
867.105719	51.743285	70.494887
866.374378	44.954543	70.499892
865.560548	43.319501	70.504897
865.300552	46.328477	70.509902
864.084781	38.478343	70.514906
863.687765	44.022643	70.519911
862.819218	43.780795	70.524916
862.256793	38.051632	70.529921
860.881696	40.632566	70.534926
860.479682	43.881752	70.539930
859.901550	39.728797	70.544935
859.611733	53.346918	70.549940
859.386942	42.562210	70.554945
858.239991	44.171756	70.559950
857.580663	39.523975	70.564954
857.192397	44.193302	70.569959
855.989887	46.008800	70.574964
855.388526	40.020922	70.579969
854.498998	51.884832	70.584974
854.119408	42.185990	70.589978
853.954546	44.380358	70.594983
852.761696	35.309246	70.599988
852.353114	38.663550	70.604993
851.171614	47.003913	70.609998
851.087608	35.398913	70.615002
850.265371	42.934662	70.620007
849.040414	43.031802	70.625012
848.741319	37.390034	70.630017
848.147711	53.055966	70.635022
848.027367	34.748778	70.640026
846.982803	38.246881	70.645031
846.252294	48.890219	70.650036
845.995685	36.940551	70.655041
844.920776	43.206145	70.660046
843.830065	41.312422	70.665050
843.153359	35.927864	70.670055
842.743429	43.837937	70.675060
842.696096	43.377086	70.680065
842.023527	50.259852	70.685070
840.638162	32.888829	70.690074
840.287632	39.743987	70.695079
839.594096	47.533631	70.700084
839.383985	38.027005	70.705089
837.965423	42.589099	70.710094
838.092711	38.169341	70.715098
837.275104	43.750626	70.720103
836.435187	38.675882	70.725108
835.803898	36.171330	70.730113
834.663011	49.891793	70.735118
834.327277	36.820957	70.740122
834.046021	44.959695	70.745127
833.058919	34.427210	70.750132
832.600978	39.785679	70.755137
831.801263	43.009865	70.760142
831.051325	32.575245	70.765146
830.232739	42.172950	70.770151
829.341029	39.064914	70.775156
829.263594	40.991492	70.780161
828.282961	40.474200	70.785166
827.669947	42.448180	70.790170
827.182009	40.176265	70.795175
826.310294	43.855010	70.800180
825.702282	32.090585	70.805185
825.675316	41.533907	70.810190
824.191431	40.309865	70.815194
823.760755	36.513474	70.820199
822.827027	42.792872	70.825204
823.012693	41.292052	70.830209
821.840040	36.615608	70.835214
820.951234	39.070277	70.840218
820.477984	38.046476	70.845223
819.718900	50.209732	70.850228
819.740661	36.462291	70.855233
818.323541	36.679915	70.860238
818.090101	32.932551	70.865242
817.619530	35.273344	70.870247
816.199155	41.691702	70.875252
815.860193	28.643468	70.880257
815.125126	43.973961	70.885262
814.939126	41.218774	70.890266
813.868586	41.236163	70.895271
812.645436	40.330151	70.900276
812.555337	36.760232	70.905281
811.969901	39.045197	70.910286
811.587016	34.522153	70.915290
810.511676	35.680378	70.920295
809.744531	37.912270	70.925300
809.249929	34.722110	70.930305
808.708921	38.867007	70.935310
807.825015	40.204483	70.940314
806.626743	36.262212	70.945319
806.670065	29.359652	70.950324
806.246626	41.849500	70.955329
805.865664	39.377645	70.960334
804.579403	32.945327	70.965338
804.258529	33.286489	70.970343
803.486099	43.580134	70.975348
803.006892	31.916632	70.980353
801.863188	36.737749	70.985358
801.213602	35.035588	70.990362
800.766997	43.135993	70.995367
800.291112	41.272149	71.000372
799.540817	39.054616	71.005377
798.355735	48.578215	71.010382
798.275897	36.885831	71.015386
797.578253	28.997417	71.020391
796.093471	43.181032	71.025396
795.519552	30.592802	71.030401
795.177342	43.538048	71.035406
795.010187	33.261396	71.040410
794.911349	36.777701	71.045415
793.264437	39.829267	71.050420
792.640156	33.185932	71.055425
791.971952	44.942083	71.060430
791.886517	36.796951	71.065434
790.612308	32.061002	71.070439
789.911806	42.146091	71.075444
789.865533	35.167911	71.080449
788.453542	33.027330	71.085454
787.594069	29.646114	71.090458
787.276808	40.624197	71.095463
786.574367	37.621659	71.100468
786.426881	40.773570	71.105473
785.847612	41.294630	71.110478
784.991175	28.399738	71.115482
784.468115	36.364087	71.120487
783.744933	43.819433	71.125492
783.102990	38.076144	71.130497
782.062265	46.392546	71.135502
781.389440	41.770590	71.140506
781.229631	40.145000	71.145511
779.666713	44.586610	71.150516
779.370129	37.843806	71.155521
778.469144	44.359266	71.160526
778.109947	38.659273	71.165530
778.019778	46.343418	71.170535
776.749959	47.501078	71.175540
776.328685	32.159009	71.180545
775.624941	42.328190	71.185550
775.185830	40.436421	71.190554
774.380831	43.535315	71.195559
773.400077	43.803341	71.200564
773.101660	34.921033	71.205569
772.532333	40.216820	71.210574
771.951062	36.453874	71.215578
771.079823	30.072198	71.220583
770.181982	46.721635	71.225588
769.955165	39.239217	71.230593
768.290048	40.707375	71.235598
767.821299	40.550141	71.240602
767.557386	33.726451	71.245607
766.937498	50.235457	71.250612
766.785111	36.156223	71.255617
765.938641	37.973426	71.260622
764.841452	39.453673	71.265626
764.175708	43.984267	71.270631
763.610627	40.434775	71.275636
763.329776	40.771147	71.280641
762.379961	42.426619	71.285646
761.931040	34.478120	71.290650
761.366856	33.287469	71.295655
760.292461	34.852393	71.300660
759.701121	34.079202	71.305665
759.084154	37.577071	71.310670
758.543470	34.126194	71.315674
757.762684	32.785533	71.320679
756.843490	39.950408	71.325684
756.486055	31.668823	71.330689
755.676063	38.798967	71.335694
755.354430	35.527671	71.340698
754.057694	32.119890	71.345703
753.502560	33.313587	71.350708
753.136164	28.746934	71.355713
752.235787	28.434503	71.360718
752.146500	36.039658	71.365722
751.333539	29.193000	71.370727
750.185440	51.208915	71.375732
750.148097	36.893762	71.380737
749.375534	29.338971	71.385742
748.528443	38.433482	71.390746
747.870636	29.827580	71.395751
747.296647	38.643661	71.400756
746.639891	38.327139	71.405761
745.475875	33.912696	71.410766
745.143286	37.404717	71.415770
744.741175	30.208819	71.420775
744.142553	47.979079	71.425780
743.553829	23.603052	71.430785
742.551145	33.985395	71.435790
741.998436	30.342483	71.440794
741.417978	39.123328	71.445799
739.773207	42.387462	71.450804
739.940912	24.728275	71.455809
739.104476	39.985030	71.460814
738.653952	35.818101	71.465818
738.264574	37.747035	71.470823
737.263956	42.591129	71.475828
736.572118	30.089499	71.480833
735.936925	36.676186	71.485838
735.272116	35.069502	71.490842
734.687536	30.392516	71.495847
733.750169	35.709058	71.500852
733.661308	40.218773	71.505857
733.154558	27.470073	71.510862
731.947196	32.137358	71.515866
731.439897	26.402614	71.520871
730.715595	37.216854	71.525876
730.023289	35.349636	71.530881
729.431512	37.908424	71.535886
728.441707	41.278013	71.540890
728.128683	28.763383	71.545895
727.480301	49.222226	71.550900
726.715777	37.090113	71.555905
725.781795	44.766679	71.560910
725.099311	34.225174	71.565914
724.907900	31.218563	71.570919
724.062702	47.548987	71.575924
723.330312	42.293173	71.580929
722.567625	42.222166	71.585934
722.420414	41.360929	71.590938
721.910879	30.429216	71.595943
720.385361	43.414631	71.600948
720.137023	36.583738	71.605953
719.523067	44.430114	71.610958
718.831182	43.245612	71.615962
718.088708	42.204774	71.620967
717.428719	39.599174	71.625972
717.221973	37.631000	71.630977
715.782814	38.315787	71.635982
714.833946	42.746396	71.640986
714.540903	33.325537	71.645991
713.993050	41.010010	71.650996
713.970823	37.129689	71.656001
713.210152	40.254657	71.661006
712.222621	34.187968	71.666010
711.689232	29.843440	71.671015
710.779506	40.411257	71.676020
710.400575	35.271053	71.681025
709.114047	40.498124	71.686030
708.530197	34.887528	71.691034
708.509684	27.178326	71.696039
707.636102	42.245473	71.701044
707.217188	40.937093	71.706049
706.064429	38.493527	71.711054
705.873163	42.712060	71.716058
705.272128	34.779911	71.721063
704.130813	32.296681	71.726068
703.469298	39.510425	71.731073
702.906211	40.729052	71.736078
702.422098	43.217092	71.741082
701.707995	42.515497	71.746087
700.627032	47.347167	71.751092
700.290950	31.619421	71.756097
699.969915	42.449882	71.761102
698.501926	34.039219	71.766106
697.933481	33.538348	71.771111
697.384562	46.639503	71.776116
697.185651	32.846799	71.781121
696.850474	37.971285	71.786126
695.739880	33.467942	71.791130
694.998109	45.127016	71.796135
694.189818	46.536066	71.801140
694.011466	41.083245	71.806145
692.702717	39.497104	71.811150
691.881320	50.913411	71.816154
691.930131	43.046516	71.821159
691.319823	45.559382	71.826164
690.848640	32.221592	71.831169
689.283749	40.001774	71.836174
688.917510	37.931272	71.841178
688.356542	27.395668	71.846183
687.884008	37.095988	71.851188
687.474051	34.646118	71.856193
686.472095	34.684178	71.861198
685.625503	31.280451	71.866202
685.079200	30.623102	71.871207
683.901907	38.497681	71.876212
683.866770	30.745079	71.881217
683.213439	39.278930	71.886222
682.618798	40.319670	71.891226
682.411736	25.339324	71.896231
681.226449	34.257476	71.901236
680.763750	27.859671	71.906241
679.539797	25.063202	71.911246
678.363253	25.706194	71.916250
678.016542	21.235766	71.921255
677.267845	29.964559	71.926260
677.213895	17.410278	71.931265
676.506459	36.416762	71.936270
676.593863	20.648411	71.941274
675.634736	29.937381	71.946279
674.796796	30.797679	71.951284
674.043279	35.755402	71.956289
672.682702	40.207429	71.961294
671.720143	38.700208	71.966298
671.398004	30.332604	71.971303
671.142367	33.465469	71.976308
671.311403	27.239873	71.981313
670.555231	32.548080	71.986318
669.502384	30.932243	71.991322
669.283434	35.230872	71.996327
667.778701	29.957723	72.001332
667.058407	42.614684	72.006337
666.361271	36.225825	72.011342
665.950015	27.210134	72.016346
665.451643	24.365943	72.021351
664.017537	30.570528	72.026356
664.038755	29.956850	72.031361
663.274235	36.873207	72.036366
662.826753	34.651654	72.041370
662.523500	34.707770	72.046375
661.451490	41.253648	72.051380
661.072941	16.010052	72.056385
659.104107	40.558208	72.061390
658.731438	38.488736	72.066394
658.443256	31.758812	72.071399
658.034324	32.828330	72.076404
657.370061	29.744066	72.081409
657.291161	31.569958	72.086414
656.410931	31.304813	72.091418
655.931542	17.020665	72.096423
654.935597	34.209245	72.101428
653.799609	35.403998	72.106433
652.960781	32.883663	72.111438
652.293196	38.570409	72.116442
652.037465	32.034003	72.121447
651.500404	33.614327	72.126452
650.957115	27.368126	72.131457
650.031774	27.677835	72.136462
649.219751	41.316018	72.141466
649.043871	28.509929	72.146471
648.198249	30.161464	72.151476
647.334433	31.018007	72.156481
646.321983	33.840906	72.161486
645.713930	33.248590	72.166490
645.776039	27.412158	72.171495
645.221750	36.633521	72.176500
644.157730	25.113661	72.181505
643.144154	38.312457	72.186510
642.715843	35.513879	72.191514
642.753015	30.457231	72.196519
641.112107	30.925043	72.201524
640.946302	20.137312	72.206529
640.322199	31.566349	72.211534
639.566921	29.616152	72.216538
639.279486	30.451872	72.221543
638.139796	30.056173	72.226548
638.105474	19.856172	72.231553
636.633563	30.748475	72.236558
635.897401	33.164704	72.241562
635.797067	29.252676	72.246567
635.106038	24.958503	72.251572
634.573402	24.871388	72.256577
633.254719	35.515383	72.261582
632.408661	35.511293	72.266586
632.548778	33.565159	72.271591
631.835130	14.236118	72.276596
631.072209	22.705423	72.281601
630.427174	20.288271	72.286606
629.880370	33.062673	72.291610
628.817207	33.995120	72.296615
627.619049	28.597487	72.301620
627.312176	26.859722	72.306625
626.882357	27.655043	72.311630
626.657833	29.403207	72.316634
626.084007	17.783226	72.321639
624.879126	38.639741	72.326644
624.453472	30.668654	72.331649
623.714788	27.142117	72.336654
622.705215	25.875780	72.341658
622.230048	23.877828	72.346663
621.425792	28.466773	72.351668
621.653051	26.420035	72.356673
620.837996	17.780884	72.361678
619.343400	33.733784	72.366682
618.842397	17.874657	72.371687
618.348666	35.393250	72.376692
618.241992	22.610843	72.381697
616.947255	31.741977	72.386702
616.290758	31.997847	72.391706
615.930363	23.841342	72.396711
615.142153	20.206010	72.401716
614.085015	24.516704	72.406721
613.380987	25.291045	72.411726
612.936479	29.912583	72.416730
612.735609	21.752751	72.421735
612.323378	31.728881	72.426740
611.336622	25.614813	72.431745
610.150278	25.981871	72.436750
609.661016	30.610537	72.441754
609.063914	28.474320	72.446759
608.061189	28.097822	72.451764
607.707603	20.755471	72.456769
607.062119	22.889200	72.461774
606.680884	30.316926	72.466778
606.368505	22.198506	72.471783
604.830643	29.968117	72.476788
604.454073	25.406268	72.481793
604.144045	26.064252	72.486798
603.593986	21.736601	72.491802
602.554692	22.575376	72.496807
601.519627	30.583440	72.501812
601.374752	25.150536	72.506817
600.746031	26.590935	72.511822
599.808885	24.349614	72.516826
599.328989	14.845017	72.521831
598.653657	35.137835	72.526836
598.246966	18.290774	72.531841
597.259099	22.648785	72.536846
596.332744	28.753618	72.541850
595.890478	26.364102	72.546855
595.269999	32.617330	72.551860
594.365836	29.776282	72.556865
593.722509	27.505515	72.561870
593.217164	34.401110	72.566874
593.106551	26.386168	72.571879
591.774780	35.281954	72.576884
591.039187	37.209280	72.581889
590.630708	34.202563	72.586894
590.230809	32.993673	72.591898
589.736177	26.142112	72.596903
588.412332	31.709472	72.601908
588.019488	35.848153	72.606913
587.568262	38.447661	72.611918
586.325631	30.720232	72.616922
585.691570	16.933799	72.621927
585.055429	32.193362	72.626932
584.626055	17.724664	72.631937
583.926794	26.303684	72.636942
583.327069	32.014324	72.641946
583.533916	23.811637	72.646951
582.005664	37.141301	72.651956
581.724165	26.704718	72.656961
580.942726	36.537817	72.661966
579.583413	33.105409	72.666970
579.326800	24.418329	72.671975
578.748785	37.948292	72.676980
578.222199	37.663119	72.681985
577.198725	25.925540	72.686990
576.469127	32.450024	72.691994
576.191783	26.830075	72.696999
575.449019	37.286182	72.702004
574.883128	31.237554	72.707009
574.060137	30.124435	72.712014
573.326469	37.911055	72.717018
573.216750	29.799782	72.722023
572.351403	23.846158	72.727028
571.511205	30.337798	72.732033
570.742186	25.139914	72.737038
570.288191	35.720329	72.742042
570.223771	23.079424	72.747047
568.695222	44.484221	72.752052
568.221644	28.042027	72.757057
567.761091	30.081662	72.762062
566.429475	30.495530	72.767066
565.718348	27.611135	72.772071
564.888104	25.247152	72.777076
564.768960	26.496018	72.782081
564.621714	21.019346	72.787086
563.996147	37.663287	72.792090
563.390114	23.482909	72.797095
562.362298	35.755225	72.802100
562.068772	30.044821	72.807105
560.980618	33.911073	72.812110
559.808408	35.725034	72.817114
559.506093	28.549554	72.822119
558.944592	38.139484	72.827124
558.193656	41.398553	72.832129
557.393248	29.644375	72.837134
556.705109	38.841339	72.842138
556.597493	37.426638	72.847143
556.121579	36.915793	72.852148
555.317169	28.777984	72.857153
554.298791	39.169191	72.862158
553.684385	45.137631	72.867162
552.957698	36.350389	72.872167
551.790335	37.089743	72.877172
551.417824	34.000039	72.882177
550.837963	33.250301	72.887182
550.359796	37.418345	72.892186
550.342441	39.757953	72.897191
549.208913	28.706503	72.902196
548.604591	37.918501	72.907201
548.192330	34.677443	72.912206
546.969341	32.254604	72.917210
546.194806	34.397866	72.922215
545.335697	38.978227	72.927220
545.121174	35.637869	72.932225
544.646104	38.841963	72.937230
543.254595	44.077948	72.942234
543.158409	37.686447	72.947239
542.316522	32.222651	72.952244
542.047802	29.666740	72.957249
540.978622	43.235523	72.962254
540.168432	34.135180	72.967258
539.997605	32.385217	72.972263
539.527734	37.598974	72.977268
538.493198	36.912199	72.982273
537.812663	34.732523	72.987278
537.027974	37.552299	72.992282
536.912604	22.029141	72.997287
535.596150	33.208949	73.002292
534.728810	33.110518	73.007297
534.043909	26.484810	73.012302
533.590237	35.529319	73.017306
533.583415	30.539603	73.022311
532.853956	29.816852	73.027316
531.951419	35.012799	73.032321
531.288566	38.134849	73.037326
530.336495	27.204308	73.042330
529.753088	28.268523	73.047335
528.845287	37.774853	73.052340
528.285642	27.492967	73.057345
528.015464	29.652085	73.062350
527.551444	27.296008	73.067354
526.955848	36.989136	73.072359
526.067322	37.034423	73.077364
525.764028	31.459613	73.082369
524.599832	40.082750	73.087374
523.465786	33.845533	73.092378
522.826434	30.997023	73.097383
522.480811	40.278199	73.102388
522.306392	29.219059	73.107393
521.756393	27.777063	73.112398
520.882334	34.297765	73.117402
520.267706	26.046169	73.122407
518.733198	38.853344	73.127412
517.814758	28.855681	73.132417
517.319463	30.810976	73.137422
516.847765	33.983000	73.142426
516.975837	31.622490	73.147431
516.286002	41.236023	73.152436
516.165029	29.304254	73.157441
515.061039	38.013991	73.162446
514.248198	40.562309	73.167450
513.636100	35.918153	73.172455
512.313986	37.535254	73.177460
511.770559	31.126697	73.182465
511.484046	42.069924	73.187470
511.003723	33.697591	73.192474
510.120992	32.516744	73.197479
509.460812	44.074548	73.202484
508.755752	34.922780	73.207489
508.218507	33.953388	73.212494
507.252196	26.368060	73.217498
506.731709	24.661186	73.222503
505.760486	33.158975	73.227508
505.374853	29.200947	73.232513
505.386308	37.182679	73.237518
503.816962	41.426787	73.242522
503.423174	39.977256	73.247527
503.004714	36.483320	73.252532
502.270141	40.066206	73.257537
501.233019	37.574359	73.262542
500.729208	35.278239	73.267546
500.165154	34.321004	73.272551
499.778184	44.733066	73.277556
499.078869	44.204206	73.282561
498.106982	34.079453	73.287566
497.749829	41.211638	73.292570
497.198567	28.284041	73.297575
495.819845	40.766810	73.302580
495.089696	26.617266	73.307585
494.642657	30.737783	73.312590
494.631316	39.992515	73.317594
493.592693	27.544654	73.322599
492.692568	39.340940	73.327604
492.050031	39.078987	73.332609
491.914773	42.665747	73.337614
490.839470	39.011537	73.342618
490.159292	30.500749	73.347623
489.326219	36.830439	73.352628
489.233983	46.689382	73.357633
488.474337	39.099518	73.362638
487.393435	34.115338	73.367642
486.944953	35.531783	73.372647
486.026613	41.733142	73.377652
485.953037	29.481611	73.382657
485.393653	31.399817	73.387662
484.084959	35.282311	73.392666
483.571851	28.690749	73.397671
482.940616	36.008511	73.402676
482.444346	38.405489	73.407681
481.631066	22.209827	73.412686
480.969058	30.587404	73.417690
480.658280	37.742160	73.422695
479.479181	37.508921	73.427700
478.888942	30.783000	73.432705
478.756653	32.355642	73.437710
477.673398	39.679189	73.442714
476.879645	38.287072	73.447719
476.136912	34.742306	73.452724
475.560345	29.496451	73.457729
475.187097	34.007314	73.462734
474.500548	32.807841	73.467738
473.728006	21.479750	73.472743
472.765999	34.853287	73.477748
472.129754	36.288608	73.482753
471.887799	37.739959	73.487758
471.030944	38.393616	73.492762
470.488004	37.661667	73.497767
469.396706	35.101201	73.502772
469.406088	36.362710	73.507777
468.862641	37.641332	73.512782
467.658016	33.131006	73.517786
466.774585	27.285955	73.522791
466.163296	45.149697	73.527796
465.751258	33.336840	73.532801
465.901570	21.839655	73.537806
464.229753	41.628961	73.542810
463.796881	29.366869	73.547815
463.524106	33.194718	73.552820
462.476209	35.168679	73.557825
461.803978	34.545634	73.562830
460.834713	33.179908	73.567834
460.505080	38.178957	73.572839
460.381622	37.482677	73.577844
459.562984	33.306653	73.582849
458.940958	35.465066	73.587854
458.019927	44.801649	73.592858
456.972702	38.432370	73.597863
455.942184	38.785713	73.602868
455.738616	31.384800	73.607873
455.218566	37.940580	73.612878
454.895570	41.527289	73.617882
454.401870	29.103014	73.622887
453.486306	38.825054	73.627892
452.634937	37.503621	73.632897
451.898645	24.405263	73.637902
450.565671	34.781966	73.642906
450.418950	28.704440	73.647911
450.158958	36.606419	73.652916
449.929536	32.675550	73.657921
448.869615	39.481335	73.662926
447.562737	38.691340	73.667930
447.307970	33.758477	73.672935
446.870319	37.442295	73.677940
445.585950	33.365706	73.682945
445.106801	34.662472	73.687950
444.251303	44.605168	73.692954
443.945928	28.921496	73.697959
443.738279	48.668349	73.702964
442.921996	32.458982	73.707969
442.102754	37.980709	73.712974
441.534901	43.156478	73.717978
441.022273	31.162549	73.722983
439.779710	40.181378	73.727988
439.114383	37.892082	73.732993
439.169070	28.384350	73.737998
438.172402	39.232573	73.743002
437.384542	31.732378	73.748007
436.670090	38.625042	73.753012
435.856474	41.838940	73.758017
435.986471	36.444255	73.763022
434.553154	41.470926	73.768026
433.931240	26.395897	73.773031
433.468009	43.042372	73.778036
432.802152	39.141618	73.783041
432.342774	33.948061	73.788046
431.113134	41.980880	73.793050
430.949253	24.994266	73.798055
430.251824	41.856238	73.803060
429.371635	31.477229	73.808065
428.518578	32.948682	73.813070
427.800795	40.034256	73.818074
427.425858	34.989663	73.823079
427.375118	34.986653	73.828084
426.332955	37.322391	73.833089
425.343817	38.135903	73.838094
424.750306	34.272508	73.843098
424.689564	30.953393	73.848103
423.508405	44.443864	73.853108
422.549367	34.160993	73.858113
421.770006	37.318977	73.863118
421.433144	37.410437	73.868122
421.318199	27.563903	73.873127
420.394953	39.417503	73.878132
419.717131	29.118215	73.883137
419.292955	32.222760	73.888142
418.013276	34.988982	73.893146
417.076141	23.594104	73.898151
416.743559	35.686306	73.903156
416.457535	32.645921	73.908161
416.024447	24.642962	73.913166
415.174674	33.580291	73.918170
414.298729	36.624364	73.923175
413.638944	37.211950	73.928180
412.997668	38.078844	73.933185
411.884975	30.480615	73.938190
411.161023	43.354226	73.943194
410.736551	42.024710	73.948199
410.490439	36.398234	73.953204
410.104687	39.195481	73.958209
409.392357	34.474291	73.963214
408.383676	39.236210	73.968218
407.932822	47.111839	73.973223
406.892788	35.370676	73.978228
406.502147	36.975024	73.983233
405.699764	34.527815	73.988238
405.056667	40.674305	73.993242
404.691699	35.397907	73.998247
403.857074	39.960217	74.003252
402.625052	37.225097	74.008257
402.544425	39.428136	74.013262
401.321153	41.922045	74.018266
400.722828	35.665760	74.023271
399.846115	33.861138	74.028276
399.656974	28.124670	74.033281
399.332038	38.545770	74.038286
398.591353	36.247995	74.043290
398.271754	29.967800	74.048295
396.982969	35.756732	74.053300
396.566419	33.572880	74.058305
396.455443	34.982867	74.063310
395.048174	29.501993	74.068314
394.505831	35.722309	74.073319
393.549750	36.051202	74.078324
393.216816	33.991213	74.083329
392.030421	28.752673	74.088334
391.486220	32.882379	74.093338
390.991583	29.624520	74.098343
390.950529	29.738231	74.103348
390.496648	48.444168	74.108353
389.303787	28.417354	74.113358
388.271087	26.714858	74.118362
388.023995	37.410541	74.123367
387.237220	36.104069	74.128372
386.294556	30.955997	74.133377
385.636045	39.672061	74.138382
385.173079	35.240707	74.143386
385.081064	26.401289	74.148391
383.779966	30.112320	74.153396
382.896939	31.889741	74.158401
383.093818	19.866358	74.163406
381.918889	33.089352	74.168410
380.847045	32.928950	74.173415
380.445245	34.322205	74.178420
380.013147	36.078234	74.183425
379.847700	25.258954	74.188430
378.501589	40.626944	74.193434
377.838813	30.013057	74.198439
377.102498	39.739667	74.203444
376.628461	41.049823	74.208449
376.339280	35.537442	74.213454
374.988806	40.338068	74.218458
374.526824	33.240102	74.223463
374.174320	36.285929	74.228468
373.898859	38.305563	74.233473
372.657028	25.005539	74.238478
372.008089	41.476614	74.243482
371.437387	25.570335	74.248487
370.756391	29.076910	74.253492
369.984740	49.322032	74.258497
369.477363	33.489227	74.263502
369.193430	32.358084	74.268506
368.166836	27.795792	74.273511
366.852470	32.168069	74.278516
366.323511	35.513233	74.283521
366.188813	34.749369	74.288526
365.023130	45.265027	74.293530
365.039357	31.218938	74.298535
364.156740	26.408215	74.303540
363.426156	31.258287	74.308545
363.258318	30.247407	74.313550
362.127182	46.304927	74.318554
361.676151	33.760347	74.323559
360.754755	33.587018	74.328564
359.880844	29.167545	74.333569
359.189187	30.455615	74.338574
358.401127	36.279881	74.343578
358.075032	23.991351	74.348583
357.870185	34.759141	74.353588
357.205920	31.482592	74.358593
356.144497	40.448937	74.363598
355.183308	37.859905	74.368602
354.951588	26.584442	74.373607
354.455284	35.906978	74.378612
353.595740	28.241634	74.383617
352.796664	26.192861	74.388622
352.023987	34.610174	74.393626
351.717916	31.390079	74.398631
350.498945	32.997134	74.403636
349.653392	47.246229	74.408641
349.411436	33.036292	74.413646
349.074323	30.092363	74.418650
348.692113	27.792669	74.423655
347.686725	36.874656	74.428660
346.694735	39.204007	74.433665
346.398611	27.084155	74.438670
345.974576	38.941791	74.443674
345.203038	40.770841	74.448679
344.021439	31.378133	74.453684
343.438616	41.406699	74.458689
343.080347	27.469179	74.463694
342.177592	28.781433	74.468698
341.355047	23.016614	74.473703
340.743620	28.410637	74.478708
340.613017	38.709312	74.483713
340.242568	29.701394	74.488718
339.065781	38.925809	74.493722
338.412221	35.570293	74.498727
337.935452	28.922522	74.503732
336.616771	43.977097	74.508737
336.348043	33.451805	74.513742
335.400126	39.273171	74.518746
335.210255	32.322651	74.523751
334.787219	14.418649	74.528756
333.231085	38.603177	74.533761
333.016333	29.980430	74.538766
332.212908	39.629440	74.543770
331.973686	38.554250	74.548775
331.071315	27.093953	74.553780
330.051527	27.433023	74.558785
329.972554	29.656297	74.563790
329.292663	33.041289	74.568794
328.324877	28.438106	74.573799
327.327819	38.666720	74.578804
326.762814	30.421471	74.583809
326.809271	30.860259	74.588814
326.268510	26.490203	74.593818
325.367373	32.906471	74.598823
324.628342	29.958794	74.603828
324.096573	34.125952	74.608833
322.914857	25.196874	74.613838
321.752768	30.839498	74.618842
321.730247	29.974186	74.623847
321.112322	37.966325	74.628852
320.270078	33.948648	74.633857
320.170272	28.372984	74.638862
319.094006	41.819964	74.643866
318.912464	27.207776	74.648871
318.227639	29.541797	74.653876
316.916775	28.126499	74.658881
316.471221	28.437132	74.663886
315.363900	25.004141	74.668890
315.050371	31.981157	74.673895
315.043041	31.477676	74.678900
313.784248	34.876091	74.683905
313.346388	28.466537	74.688910
312.416165	37.254300	74.693914
312.076427	26.128517	74.698919
311.220817	26.455621	74.703924
310.253208	35.318722	74.708929
310.010144	38.892704	74.713934
309.364934	29.253693	74.718938
309.170722	24.017909	74.723943
307.927768	31.799021	74.728948
307.143781	33.141242	74.733953
306.902964	19.787378	74.738958
305.903225	35.551165	74.743962
305.030015	35.540477	74.748967
304.801148	34.842084	74.753972
304.155610	28.199144	74.758977
303.378184	29.475669	74.763982
302.177392	34.968364	74.768986
302.089176	27.847118	74.773991
301.635188	29.939362	74.778996
300.812975	31.437478	74.784001
300.051112	17.774025	74.789006
299.199340	28.397349	74.794010
298.659776	29.765267	74.799015
298.306079	32.462807	74.804020
297.265452	29.083845	74.809025
296.685895	27.089986	74.814030
295.978879	32.466140	74.819034
295.542927	28.175574	74.824039
294.628080	12.625369	74.829044
293.629399	44.146454	74.834049
293.202949	25.470341	74.839054
292.516736	36.259661	74.844058
292.454099	24.835847	74.849063
291.988534	21.146053	74.854068
290.825887	30.505413	74.859073
290.518524	20.845681	74.864078
289.732832	28.618571	74.869082
288.589039	25.431087	74.874087
288.300314	31.823870	74.879092
287.232846	32.329819	74.884097
286.690001	23.981713	74.889102
285.647744	26.900955	74.894106
285.530273	18.611203	74.899111
285.251947	25.248314	74.904116
284.209853	27.937310	74.909121
283.358976	26.287877	74.914126
282.543891	33.146152	74.919130
282.149786	20.870061	74.924135
282.029255	22.141234	74.929140
281.020786	39.114289	74.934145
280.336571	17.448568	74.939150
279.859114	24.462747	74.944154
279.160401	30.924030	74.949159
278.152601	19.855859	74.954164
277.547474	21.062354	74.959169
277.277179	26.625928	74.964174
275.944186	38.445529	74.969178
275.272784	22.006600	74.974183
274.841987	18.618754	74.979188
274.177632	23.491403	74.984193
274.140537	11.511633	74.989198
273.021501	23.905785	74.994202
272.364268	19.231055	74.999207
271.911104	26.378550	75.004212
270.820996	22.029842	75.009217
269.838370	13.504279	75.014222
269.283686	25.663411	75.019226
269.059783	32.296582	75.024231
268.824996	25.903555	75.029236
267.508352	31.528262	75.034241
266.701657	25.822442	75.039246
266.108968	34.089668	75.044250
265.969283	23.818202	75.049255
265.441285	22.625056	75.054260
263.975840	25.001519	75.059265
263.711378	20.540135	75.064270
262.790235	22.244829	75.069274
262.605456	21.269773	75.074279
261.826162	14.678134	75.079284
260.703266	36.767380	75.084289
260.403523	24.280722	75.089294
259.879646	18.107233	75.094298
259.354779	26.966002	75.099303
258.424174	24.607089	75.104308
257.640559	34.437446	75.109313
257.280348	12.735868	75.114318
256.056176	19.850149	75.119322
255.172453	26.427651	75.124327
254.823152	18.950666	75.129332
254.368099	15.524117	75.134337
254.197686	22.314327	75.139342
253.679932	25.348660	75.144346
252.983193	20.418476	75.149351
252.139721	25.068962	75.154356
251.074057	40.501099	75.159361
250.129073	20.665104	75.164366
249.192981	26.716404	75.169370
248.864087	37.532349	75.174375
248.716939	22.610369	75.179380
248.046113	26.418106	75.184385
247.137169	25.791855	75.189390
246.103865	27.913377	75.194394
245.869772	13.155067	75.199399
245.569412	27.478096	75.204404
244.568749	36.728084	75.209409
243.924432	24.994900	75.214414
243.274693	37.468797	75.219418
242.968895	26.839060	75.224423
241.840777	26.339206	75.229428
240.709746	33.955859	75.234433
240.712965	12.555878	75.239438
239.922078	32.334153	75.244442
239.709604	20.494293	75.249447
238.499977	31.639847	75.254452
237.858789	29.966466	75.259457
237.577815	30.928924	75.264462
236.210923	23.394966	75.269466
235.272929	31.248914	75.274471
235.155245	28.270027	75.279476
234.666895	28.672646	75.284481
234.708905	23.503290	75.289486
233.331392	23.500481	75.294490
232.693836	23.740817	75.299495
232.057519	31.944043	75.304500
231.223301	32.613095	75.309505
230.762044	16.577481	75.314510
229.679059	33.920364	75.319514
229.226708	21.612575	75.324519
228.686968	26.138962	75.329524
228.211343	30.656707	75.334529
227.547747	26.124920	75.339534
226.662973	23.519034	75.344538
226.159883	25.398358	75.349543
225.564782	25.299213	75.354548
224.608735	37.260582	75.359553
223.958645	17.210453	75.364558
223.425746	27.387174	75.369562
223.027935	29.606084	75.374567
221.786677	29.892200	75.379572
220.982640	29.189316	75.384577
220.856996	25.997248	75.389582
220.478195	26.472287	75.394586
219.657734	24.847989	75.399591
218.925982	31.440699	75.404596
218.154515	24.447305	75.409601
217.759009	26.885031	75.414606
216.693160	25.801289	75.419610
215.830207	24.666281	75.424615
215.264132	26.147244	75.429620
214.612075	36.196321	75.434625
214.530090	16.038289	75.439630
213.442035	27.740018	75.444634
212.701813	31.235573	75.449639
212.568725	23.351991	75.454644
211.500791	20.573473	75.459649
210.763416	21.000026	75.464654
209.958130	22.293635	75.469658
209.444261	23.390987	75.474663
209.401372	30.056798	75.479668
208.086000	32.190188	75.484673
207.417553	29.016847	75.489678
206.489669	35.383803	75.494682
206.340553	21.061350	75.499687
205.912293	25.235677	75.504692
204.514696	29.074134	75.509697
204.112079	18.991245	75.514702
203.730064	19.492029	75.519706
203.324112	21.841540	75.524711
202.604548	31.002574	75.529716
201.531623	28.532339	75.534721
201.285355	20.051833	75.539726
200.372350	28.524660	75.544730
199.319355	37.680510	75.549735
198.822178	27.071832	75.554740
198.144951	33.584898	75.559745
197.740939	28.103472	75.564750
196.916485	24.139776	75.569754
196.019160	24.881973	75.574759
195.691379	28.061061	75.579764
195.122103	33.293863	75.584769
194.633858	21.468016	75.589774
193.256977	32.205040	75.594778
192.726812	26.131911	75.599783
192.441215	24.411315	75.604788
191.876348	24.212748	75.609793
191.320579	27.442374	75.614798
190.491534	37.871308	75.619802
190.032951	32.754951	75.624807
189.517695	20.092952	75.629812
187.987968	36.330741	75.634817
187.440078	32.562636	75.639822
186.872619	35.095585	75.644826
186.707653	34.990950	75.649831
186.355625	25.778300	75.654836
184.993963	23.418757	75.659841
184.877349	23.804698	75.664846
183.535463	25.920250	75.669850
182.817369	25.642041	75.674855
182.421453	23.943765	75.679860
181.884766	21.675037	75.684865
181.779280	29.785758	75.689870
180.274178	32.200128	75.694874
179.688456	28.037539	75.699879
179.312332	28.321359	75.704884
178.483393	31.329629	75.709889
177.368214	26.809933	75.714894
176.699439	20.683220	75.719898
176.053426	28.004964	75.724903
176.103389	32.883595	75.729908
175.356510	30.804486	75.734913
174.555070	20.452473	75.739918
173.525027	32.014091	75.744922
173.145962	26.949712	75.749927
173.030106	24.973414	75.754932
172.122633	21.672625	75.759937
171.377934	17.554308	75.764942
170.160004	18.872719	75.769946
169.932518	17.666376	75.774951
169.622881	29.092638	75.779956
168.564037	20.443664	75.784961
168.211974	26.105430	75.789966
167.738542	19.026697	75.794970
166.316220	30.217225	75.799975
165.813817	31.404215	75.804980
165.191570	24.918449	75.809985
164.740588	18.252427	75.814990
163.409215	24.412503	75.819994
162.765558	28.263234	75.824999
162.711052	13.227171	75.830004
161.775063	36.035639	75.835009
161.883498	22.359639	75.840014
160.803667	23.482583	75.845018
159.867120	31.181792	75.850023
159.490356	26.378806	75.855028
158.787254	28.160731	75.860033
158.041923	32.486537	75.865038
156.960139	30.473445	75.870042
156.583338	31.883246	75.875047
156.407605	22.342897	75.880052
155.549878	26.175723	75.885057
154.637073	24.993497	75.890062
154.041085	24.270079	75.895066
153.485627	32.184478	75.900071
152.936972	26.108001	75.905076
151.869567	29.406595	75.910081
151.417171	15.121477	75.915086
150.889521	27.613755	75.920090
150.512119	21.358599	75.925095
149.355990	21.490839	75.930100
148.496587	25.475312	75.935105
148.074447	21.890584	75.940110
147.696025	31.938614	75.945114
146.492667	31.170121	75.950119
146.130114	30.696472	75.955124
145.547246	32.270009	75.960129
145.048945	29.820138	75.965134
144.024293	29.874652	75.970138
143.273514	29.065537	75.975143
142.781470	28.207286	75.980148
142.135920	27.706225	75.985153
141.570998	31.605905	75.990158
140.526509	27.352481	75.995162
140.030680	33.473961	76.000167
139.629141	35.576792	76.005172
139.111191	30.985542	76.010177
138.661215	29.075134	76.015182
137.562042	24.161849	76.020186
136.573004	29.319671	76.025191
136.735156	22.689925	76.030196
135.597096	32.488517	76.035201
135.012078	22.646025	76.040206
133.972518	36.806242	76.045210
133.473349	39.424502	76.050215
132.753249	21.711425	76.055220
131.572349	31.354434	76.060225
131.312949	31.914521	76.065230
130.908481	32.352668	76.070234
130.278061	20.074882	76.075239
130.237776	25.287996	76.080244
128.886117	30.768551	76.085249
128.475547	25.720244	76.090254
128.084938	27.286781	76.095258
126.944448	24.909351	76.100263
126.168261	28.346012	76.105268
125.569036	32.722642	76.110273
125.371031	23.821319	76.115278
124.328305	22.007005	76.120282
123.621416	18.754672	76.125287
123.375146	9.274467	76.130292
122.301432	36.007593	76.135297
121.389549	25.178080	76.140302
120.697594	22.664483	76.145306
119.861802	24.327236	76.150311
119.728851	22.525544	76.155316
119.443292	35.729809	76.160321
118.989529	29.830585	76.165326
117.752210	23.177999	76.170330
117.223477	22.770274	76.175335
116.663428	25.590617	76.180340
115.471799	32.051690	76.185345
114.924350	29.303755	76.190350
114.399324	25.754361	76.195354
113.668220	38.389472	76.200359
113.101233	24.717102	76.205364
112.265547	31.208146	76.210369
111.989785	29.591641	76.215374
111.456125	26.857277	76.220378
110.022710	38.574695	76.225383
109.724419	29.332995	76.230388
109.031267	33.639455	76.235393
108.984298	20.735668	76.240398
107.642589	32.354887	76.245402
106.561715	28.362730	76.250407
106.678061	28.432425	76.255412
106.136924	32.146981	76.260417
105.667742	25.111737	76.265422
104.507654	23.242034	76.270426
104.043848	30.183102	76.275431
103.657366	19.465352	76.280436
102.341636	18.826757	76.285441
101.589104	23.492745	76.290446
101.205441	26.940933	76.295450
100.910019	29.351677	76.300455
100.003700	25.058895	76.305460
98.827760	35.000728	76.310465
98.541124	26.564520	76.315470
98.258717	27.689636	76.320474
97.094400	34.783408	76.325479
96.397132	25.774057	76.330484
95.459312	27.495662	76.335489
95.285717	27.127499	76.340494
94.838372	22.685843	76.345498
94.165672	30.514873	76.350503
93.289624	29.558604	76.355508
92.676758	22.894760	76.360513
92.220231	28.694608	76.365518
90.870261	34.663736	76.370522
90.102298	32.103925	76.375527
90.079488	25.595130	76.380532
89.423395	36.548402	76.385537
88.819059	30.498166	76.390542
87.914424	22.551568	76.395546
87.056433	20.091266	76.400551
86.718536	30.410360	76.405556
86.078200	39.621861	76.410561
85.469473	35.335240	76.415566
84.716916	30.358821	76.420570
84.063742	34.472845	76.425575
83.513948	37.934915	76.430580
82.649371	30.759313	76.435585
81.926769	30.776723	76.440590
81.555820	39.609398	76.445594
80.942339	35.189504	76.450599
80.671006	23.278644	76.455604
79.262805	25.545165	76.460609
78.822541	23.969090	76.465614
78.295018	30.563954	76.470618
77.030105	23.318168	76.475623
76.448288	34.816222	76.480628
75.640795	34.557032	76.485633
75.479566	27.772287	76.490638
74.833393	29.945674	76.495642
74.167024	38.161607	76.500647
73.364447	15.737486	76.505652
72.747633	27.477643	76.510657
72.343758	18.694312	76.515662
72.043697	24.548051	76.520666
70.831543	34.473593	76.525671
70.603926	27.585903	76.530676
69.451901	26.251059	76.535681
68.823572	25.993260	76.540686
67.864186	23.847158	76.545690
67.207095	32.794842	76.550695
66.901574	28.518219	76.555700
66.575101	30.200685	76.560705
65.453228	31.126962	76.565710
64.669330	22.235513	76.570714
64.288034	24.715144	76.575719
64.136718	33.634207	76.580724
62.841595	37.986220	76.585729
62.154620	28.394959	76.590734
61.349529	33.225450	76.595738
61.194491	28.139560	76.600743
60.070944	26.759181	76.605748
59.297629	27.670873	76.610753
58.892749	25.384308	76.615758
58.542370	26.479270	76.620762
57.739453	39.100614	76.625767
57.131709	15.106429	76.630772
56.329924	40.760219	76.635777
55.866338	24.291400	76.640782
54.594442	31.640448	76.645786
53.943299	40.271821	76.650791
53.509333	28.052608	76.655796
53.052789	26.715661	76.660801
52.794623	35.465697	76.665806
52.114577	31.419104	76.670810
50.947651	33.260836	76.675815
50.812419	23.971072	76.680820
49.405671	23.294985	76.685825
48.786880	24.692934	76.690830
48.266080	26.195096	76.695834
47.758011	35.421773	76.700839
47.506997	25.983328	76.705844
46.079236	37.553226	76.710849
45.849280	37.960403	76.715854
45.328612	30.684241	76.720858
44.259343	31.990043	76.725863
43.408709	27.410879	76.730868
42.612929	31.814142	76.735873
42.170376	32.663627	76.740878
41.940669	27.791484	76.745882
41.375773	32.301417	76.750887
40.769287	24.934875	76.755892
39.494774	36.470874	76.760897
39.005748	31.629050	76.765902
38.811793	22.933663	76.770906
37.669255	35.886697	76.775911
37.256272	23.880175	76.780916
36.134902	25.651574	76.785921
36.018382	24.865910	76.790926
35.391590	38.482540	76.795930
34.363010	32.280800	76.800935
33.524075	18.669183	76.805940
33.304587	37.623123	76.810945
32.711449	30.960879	76.815950
31.717489	20.217039	76.820954
30.670045	30.363890	76.825959
30.356916	25.468786	76.830964
29.959683	32.604236	76.835969
29.613959	24.306768	76.840974
28.833507	28.937808	76.845978
27.956742	34.640698	76.850983
27.533151	28.933790	76.855988
26.079370	32.377631	76.860993
25.533969	29.550550	76.865998
25.329987	22.575527	76.871002
24.718895	21.074013	76.876007
24.410776	31.933949	76.881012
22.950440	29.404169	76.886017
22.466060	24.984204	76.891022
22.101664	36.416052	76.896026
21.426672	32.319780	76.901031
20.934713	23.432246	76.906036
19.792502	37.351840	76.911041
19.401554	32.555875	76.916046
18.958608	25.527507	76.921050
17.851868	31.148814	76.926055
17.281436	17.196359	76.931060
16.557115	28.958401	76.936065
16.269344	22.520256	76.941070
15.295362	16.066990	76.946074
14.092297	33.881633	76.951079
13.833030	23.544133	76.956084
13.304349	37.197152	76.961089
13.415656	22.680251	76.966094
12.229989	23.980978	76.971098
11.038635	36.367835	76.976103
11.140136	19.521923	76.981108
10.136903	29.215481	76.986113
9.148988	37.805963	76.991118
8.665901	31.503040	76.996122
7.877553	37.239139	77.001127
7.735523	27.272421	77.006132
6.547438	27.403517	77.011137
5.818067	33.403003	77.016142
5.650079	27.174396	77.021147
5.103754	23.421861	77.026151
4.039579	29.780654	77.031156
3.188911	26.879275	77.036161