Mon Mar 08 19:22:20 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
0.231300	94.312189	0.000000
-0.277087	91.411605	0.005005
-1.163008	62.666749	0.010010
-2.741174	18.418451	0.015014
-6.487998	-5.410635	0.020019
-11.555115	-11.147726	0.025024
-16.748109	-6.306204	0.030029
-21.269217	3.313213	0.035034
-25.301202	3.622214	0.040038
-29.401587	4.653288	0.045043
-32.806294	-9.833912	0.050048
-36.606412	1.759837	0.055053
-39.945043	-2.100526	0.060058
-43.667411	4.912727	0.065062
-47.989180	1.083054	0.070067
-51.320606	3.927862	0.075072
-55.228960	1.167581	0.080077
-58.355062	1.202828	0.085082
-62.033248	-6.394060	0.090086
-66.404365	0.437307	0.095091
-70.153765	1.697866	0.100096
-73.880577	6.934774	0.105101
-77.710973	2.413376	0.110106
-81.633573	-2.099612	0.115110
-85.159929	-1.957902	0.120115
-88.353316	-5.623763	0.125120
-92.980444	5.226861	0.130125
-96.977628	0.330010	0.135130
-100.361999	-4.259353	0.140134
-104.499589	-5.838194	0.145139
-107.761560	-15.267467	0.150144
-111.396834	11.139727	0.155149
-115.091556	-5.926517	0.160154
-118.839631	-7.001394	0.165158
-122.874665	0.047666	0.170163
-126.536068	-11.813989	0.175168
-130.548394	6.570509	0.180173
-134.064969	-11.005056	0.185178
-137.491859	-18.384887	0.190182
-141.832406	-12.338807	0.195187
-145.393050	-3.146794	0.200192
-149.376243	-18.213233	0.205197
-153.167604	-12.289452	0.210202
-156.885953	-2.786852	0.215206
-161.169633	1.455750	0.220211
-164.540319	-4.166956	0.225216
-168.568746	-1.300653	0.230221
-171.602999	3.464792	0.235226
-175.496900	-5.906127	0.240230
-179.337175	-8.081020	0.245235
-182.936108	-14.099327	0.250240
-187.069510	-10.683273	0.255245
-190.509913	3.311586	0.260250
-194.446268	6.415535	0.265254
-198.330482	-5.560251	0.270259
-201.904221	-9.728190	0.275264
-205.787498	1.732428	0.280269
-209.134252	-4.072216	0.285274
-213.276949	6.114734	0.290278
-216.726348	9.052703	0.295283
-220.656709	-4.298568	0.300288
-224.433415	-7.618856	0.305293
-228.430642	-3.861792	0.310298
-231.919251	-5.853045	0.315302
-235.794640	1.143910	0.320307
-239.518741	-1.560323	0.325312
-243.187416	-4.754332	0.330317
-246.885826	2.952355	0.335322
-250.672170	4.367310	0.340326
-254.713427	-1.127742	0.345331
-258.293098	-6.198176	0.350336
-261.741020	2.446191	0.355341
-265.625037	-3.084975	0.360346
-269.530184	2.749923	0.365350
-273.599294	1.149406	0.370355
-276.827890	-11.963710	0.375360
-280.945889	-5.292214	0.380365
-284.745779	-2.664033	0.385370
-288.104746	-5.237250	0.390374
-292.099232	-1.425330	0.395379
-295.960087	-12.493257	0.400384
-300.178819	-1.701146	0.405389
-303.565652	-5.537669	0.410394
-307.274365	-5.323952	0.415398
-310.907297	-9.542195	0.420403
-314.542609	-12.448124	0.425408
-318.465616	-11.602561	0.430413
-322.069768	-2.616233	0.435418
-326.080270	-8.458241	0.440422
-330.004359	-5.441185	0.445427
-333.741959	-10.511519	0.450432
-337.226944	-1.435391	0.455437
-340.933040	-12.291419	0.460442
-344.653681	-13.188985	0.465446
-348.704336	-1.203157	0.470451
-352.193054	-10.346738	0.475456
-356.504679	1.958290	0.480461
-360.180581	4.962580	0.485466
-363.653429	-8.166604	0.490470
-367.494383	-10.629645	0.495475
-371.217453	-5.460700	0.500480
-375.058876	4.147016	0.505485
-378.558773	2.009557	0.510490
-382.525138	-1.939316	0.515494
-386.444022	-11.545557	0.520499
-390.225756	-6.010853	0.525504
-393.971827	5.631552	0.530509
-397.753426	5.177430	0.535514
-401.230277	-13.805837	0.540518
-404.864974	-0.314232	0.545523
-408.767566	-9.095199	0.550528
-412.597604	-7.698244	0.555533
-416.161830	-0.148345	0.560538
-420.025567	-2.424751	0.565542
-423.955837	-2.831440	0.570547
-427.507832	-8.442154	0.575552
-431.751402	-2.436280	0.580557
-435.614937	11.599658	0.585562
-438.940160	-4.320328	0.590566
-442.599677	0.676164	0.595571
-446.151901	-0.134606	0.600576
-450.445288	3.988634	0.605581
-453.517466	-5.716433	0.610586
-457.388459	8.377491	0.615590
-461.556390	6.479286	0.620595
-465.205282	3.694017	0.625600
-469.515904	4.316318	0.630605
-473.289135	1.897822	0.635610
-476.797969	-5.876817	0.640614
-480.314665	3.299182	0.645619
-484.197610	-1.187925	0.650624
-487.616917	-3.505235	0.655629
-491.501567	-2.627671	0.660634
-495.076639	-9.567018	0.665638
-499.166771	-1.519884	0.670643
-502.817098	-10.287362	0.675648
-506.497161	1.699447	0.680653
-510.354823	2.910173	0.685658
-514.119954	-6.286775	0.690662
-517.804883	2.559780	0.695667
-521.491994	0.201718	0.700672
-525.574839	5.822567	0.705677
-529.210198	-3.693105	0.710682
-532.510419	-7.339716	0.715686
-536.877869	-2.758254	0.720691
-540.646525	-5.426510	0.725696
-544.165885	-1.783101	0.730701
-547.944126	5.506302	0.735706
-551.408785	-0.078752	0.740710
-555.530476	-7.495200	0.745715
-559.221228	-7.574098	0.750720
-562.940722	-1.834623	0.755725
-567.194772	-0.041712	0.760730
-570.411278	-5.592262	0.765734
-574.560176	9.590087	0.770739
-578.195755	-1.141209	0.775744
-581.888511	-3.301169	0.780749
-585.803391	0.063308	0.785754
-589.176509	6.431839	0.790758
-593.376613	6.025960	0.795763
-596.833235	6.021674	0.800768
-600.533432	1.292696	0.805773
-604.505864	7.189329	0.810778
-607.965123	-3.024501	0.815782
-611.958646	5.854145	0.820787
-615.935289	2.787184	0.825792
-619.549859	-7.438080	0.830797
-623.408351	3.874136	0.835802
-627.287695	-0.690571	0.840806
-631.047873	4.951438	0.845811
-634.391205	5.875206	0.850816
-638.281407	1.168760	0.855821
-642.179232	-5.244166	0.860826
-645.461757	-10.500230	0.865830
-649.523229	12.722718	0.870835
-653.066601	-0.106182	0.875840
-657.093308	-5.982867	0.880845
-660.918536	-5.485078	0.885850
-664.520057	-0.562174	0.890854
-668.549149	5.051900	0.895859
-672.374312	-2.574130	0.900864
-675.957746	7.186770	0.905869
-679.612613	6.876839	0.910874
-683.288086	4.974453	0.915878
-687.258818	10.989211	0.920883
-690.686639	-4.363670	0.925888
-694.733453	0.056464	0.930893
-698.901023	5.702176	0.935898
-702.191727	5.296246	0.940902
-705.890618	6.902930	0.945907
-709.458708	0.951475	0.950912
-713.705063	2.172604	0.955917
-717.528496	0.095236	0.960922
-720.971924	-0.131733	0.965926
-725.072039	-1.384345	0.970931
-728.430897	-2.479458	0.975936
-732.285682	-1.546356	0.980941
-736.269255	1.835649	0.985946
-739.590643	-4.317595	0.990950
-743.616563	0.104012	0.995955
-747.557737	-7.731987	1.000960
-751.135320	-9.722441	1.005965
-755.096007	9.920921	1.010970
-758.465151	-3.673602	1.015974
-762.392306	8.225340	1.020979
-766.035353	7.207234	1.025984
-769.803050	-9.803630	1.030989
-773.835249	9.248840	1.035994
-777.598849	-2.634826	1.040998
-781.477051	5.544469	1.046003
-785.105879	-5.201752	1.051008
-788.524731	-5.713225	1.056013
-792.634586	6.230731	1.061018
-796.302713	7.931979	1.066022
-800.287046	9.418865	1.071027
-804.038347	8.157944	1.076032
-807.509563	-3.734558	1.081037
-811.274093	3.174613	1.086042
-814.820052	6.018484	1.091046
-818.723879	12.059027	1.096051
-822.328382	-3.421506	1.101056
-826.386221	-8.856132	1.106061
-830.405215	16.093226	1.111066
-833.689461	2.548319	1.116070
-837.354240	9.523582	1.121075
-841.181961	-2.341840	1.126080
-845.246224	-3.219956	1.131085
-849.094522	-6.713852	1.136090
-852.622075	-5.755599	1.141094
-856.525667	2.919840	1.146099
-860.530525	-0.634160	1.151104
-864.036891	-3.246057	1.156109
-867.701336	5.779070	1.161114
-871.154386	5.604317	1.166118
-875.343933	7.023218	1.171123
-879.306109	5.546990	1.176128
-882.895138	7.051238	1.181133
-886.679412	2.173751	1.186138
-890.161850	5.865372	1.191142
-893.912574	0.471643	1.196147
-897.726825	1.286579	1.201152
-901.608607	2.195890	1.206157
-905.598821	-1.866534	1.211162
-908.897004	-7.159134	1.216166
-913.160310	0.653036	1.221171
-916.735825	5.086493	1.226176
-920.377570	1.542345	1.231181
-924.190982	12.054669	1.236186
-927.741570	6.009303	1.241190
-931.866339	8.417654	1.246195
-935.557867	0.532605	1.251200
-938.994728	1.809197	1.256205
-942.991879	0.310288	1.261210
-946.657613	-3.509078	1.266214
-950.623554	0.474386	1.271219
-954.152567	5.523308	1.276224
-957.863015	-3.162857	1.281229
-962.063436	-0.384418	1.286234
-965.339558	3.356315	1.291238
-969.468059	8.419125	1.296243
-972.815723	-3.425063	1.301248
-976.586396	-6.524337	1.306253
-980.758470	1.768485	1.311258
-984.266765	-1.360119	1.316262
-988.308012	-3.296561	1.321267
-991.821767	-13.668204	1.326272
-995.780262	11.650147	1.331277
-999.984012	7.998894	1.336282
-1002.818455	-6.735641	1.341286
-1006.928960	3.382802	1.346291
-1010.635885	2.692236	1.351296
-1014.152846	-5.523345	1.356301
-1018.333675	-5.210939	1.361306
-1022.203282	7.265778	1.366310
-1025.841620	5.641825	1.371315
-1029.363607	-4.051990	1.376320
-1033.168328	4.396620	1.381325
-1036.903181	-7.596835	1.386330
-1040.875130	-8.448377	1.391334
-1044.448909	2.525650	1.396339
-1048.489293	7.098301	1.401344
-1052.090098	-1.529555	1.406349
-1055.798396	0.673641	1.411354
-1059.400377	-9.505604	1.416358
-1063.436985	5.907121	1.421363
-1066.965298	1.320130	1.426368
-1070.726280	-1.201846	1.431373
-1074.934194	2.842602	1.436378
-1078.672390	-3.405882	1.441382
-1082.335782	3.774507	1.446387
-1085.749268	-4.780759	1.451392
-1089.519715	-9.144493	1.456397
-1093.332654	8.444784	1.461402
-1096.977103	0.964025	1.466406
-1101.138316	9.837165	1.471411
-1105.277187	8.190908	1.476416
-1108.558754	-9.430074	1.481421
-1112.348166	5.034935	1.486426
-1115.642168	-11.716793	1.491430
-1119.724269	3.577149	1.496435
-1123.508794	3.850000	1.501440
-1127.033421	1.124741	1.506445
-1131.359620	10.828504	1.511450
-1134.831238	-14.687135	1.516454
-1138.615809	-11.214884	1.521459
-1142.403781	1.234759	1.526464
-1146.208297	4.858437	1.531469
-1150.222075	2.094782	1.536474
-1153.361152	-0.895527	1.541478
-1156.938785	-3.536572	1.546483
-1160.983147	-3.229974	1.551488
-1164.587116	-5.780068	1.556493
-1168.778784	1.565385	1.561498
-1172.253476	-5.537162	1.566502
-1176.464143	4.227033	1.571507
-1180.042284	-5.151649	1.576512
-1183.883935	-1.900407	1.581517
-1187.650143	11.282204	1.586522
-1191.296085	-14.068261	1.591526
-1194.922887	3.500836	1.596531
-1198.393227	14.021759	1.601536
-1202.202516	-4.146949	1.606541
-1206.406189	-1.011196	1.611546
-1209.958459	-0.851054	1.616550
-1214.258089	9.447795	1.621555
-1217.625839	-2.112122	1.626560
-1221.053922	-4.803801	1.631565
-1225.021945	-0.269239	1.636570
-1228.694528	-9.115530	1.641574
-1232.587911	-11.524595	1.646579
-1236.583038	13.967104	1.651584
-1240.267955	-4.849009	1.656589
-1244.338491	-4.534924	1.661594
-1247.494691	-13.227289	1.666598
-1251.013367	1.032183	1.671603
-1255.036908	-0.033066	1.676608
-1259.062565	-4.987982	1.681613
-1262.948168	2.925191	1.686618
-1266.237954	1.662121	1.691622
-1270.352767	7.152151	1.696627
-1274.082552	-9.002928	1.701632
-1277.369014	-8.776419	1.706637
-1281.662916	6.105438	1.711642
-1285.116434	0.890283	1.716646
-1289.217987	-4.252689	1.721651
-1293.076305	-7.080390	1.726656
-1296.193096	-7.973744	1.731661
-1300.318023	-0.231928	1.736666
-1303.907248	-4.397246	1.741670
-1307.631233	0.147277	1.746675
-1311.913635	5.271572	1.751680
-1315.394400	0.095516	1.756685
-1318.989172	-7.151569	1.761690
-1322.438623	-12.086638	1.766694
-1326.367319	3.389641	1.771699
-1330.623641	-6.935135	1.776704
-1334.018749	-5.032345	1.781709
-1338.127642	2.194505	1.786714
-1341.934985	-12.382253	1.791718
-1345.563751	-4.606248	1.796723
-1349.311066	-1.678894	1.801728
-1352.893215	7.458344	1.806733
-1356.968885	9.025442	1.811738
-1360.201090	-11.313584	1.816742
-1364.132181	-2.535183	1.821747
-1368.144661	16.800442	1.826752
-1371.650934	-21.401025	1.831757
-1375.510972	21.147754	1.836762
-1379.093367	6.307972	1.841766
-1383.198539	-1.972115	1.846771
-1387.078401	0.727380	1.851776
-1390.373052	0.920670	1.856781
-1394.285847	1.648121	1.861786
-1398.065876	-4.323493	1.866790
-1401.832406	11.923242	1.871795
-1406.078506	-5.076116	1.876800
-1409.416411	-13.849531	1.881805
-1413.350964	15.907475	1.886810
-1416.799922	-22.187970	1.891814
-1420.433690	9.860871	1.896819
-1424.492706	2.935839	1.901824
-1428.102013	-7.804541	1.906829
-1432.291110	6.737545	1.911834
-1435.542250	-11.034422	1.916838
-1439.348728	-6.564789	1.921843
-1443.223362	-15.171801	1.926848
-1446.909615	4.121158	1.931853
-1450.883164	2.532629	1.936858
-1454.963082	0.891758	1.941862
-1458.207971	6.115104	1.946867
-1461.852004	0.952804	1.951872
-1465.422980	1.759675	1.956877
-1469.537490	4.723940	1.961882
-1473.193386	-2.584063	1.966886
-1476.897234	4.683815	1.971891
-1480.881179	-2.734060	1.976896
-1484.316285	-3.107875	1.981901
-1488.428000	11.141245	1.986906
-1492.555725	-7.166724	1.991910
-1496.123858	13.739404	1.996915
-1500.204356	-3.890572	2.006912
-1500.780288	-7.795641	2.016909
-1497.783962	-0.344655	2.026906
-1495.416761	1.963771	2.036902
-1493.417309	3.936379	2.046899
-1491.437166	3.630665	2.056896
-1489.659031	6.947570	2.066893
-1487.725415	7.980267	2.076890
-1485.616479	-5.095151	2.086886
-1483.777273	-1.849598	2.096883
-1481.840567	-12.647590	2.106880
-1479.809630	2.703760	2.116877
-1478.100704	-0.638820	2.126874
-1476.434718	-3.278257	2.136870
-1474.423049	-5.982517	2.146867
-1472.418245	-4.309148	2.156864
-1470.503716	-5.537429	2.166861
-1468.713590	-2.918695	2.176858
-1467.018968	-6.225820	2.186854
-1464.913104	0.471012	2.196851
-1462.792038	-1.229248	2.206848
-1461.275961	-6.080301	2.216845
-1459.143457	0.501754	2.226842
-1457.142705	-11.965830	2.236838
-1455.587791	3.431765	2.246835
-1453.298957	-3.101321	2.256832
-1451.915023	-1.994793	2.266829
-1449.977022	-3.059459	2.276826
-1447.830722	-12.222157	2.286822
-1446.276474	-2.928222	2.296819
-1444.104320	-4.983989	2.306816
-1442.232857	1.373055	2.316813
-1440.334198	-9.125155	2.326810
-1438.550838	1.979343	2.336806
-1436.731223	-5.345384	2.346803
-1434.802405	-6.719597	2.356800
-1432.747487	-2.212314	2.366797
-1430.872151	-3.892150	2.376794
-1429.033655	-3.189939	2.386790
-1427.014189	-12.886484	2.396787
-1425.416253	-3.751096	2.406784
-1423.745018	7.399789	2.416781
-1421.602003	-4.602691	2.426778
-1419.482773	-3.605969	2.436774
-1417.664577	-3.494141	2.446771
-1416.176675	-3.713091	2.456768
-1413.845443	-2.871874	2.466765
-1412.303778	4.259524	2.476762
-1410.192064	3.514424	2.486758
-1408.317231	3.116701	2.496755
-1406.406776	-6.230825	2.506752
-1404.779265	3.482440	2.516749
-1402.688350	1.621282	2.526746
-1401.138029	-7.798050	2.536742
-1398.863905	3.409484	2.546739
-1397.017203	-3.951128	2.556736
-1395.208863	5.518476	2.566733
-1393.446967	1.507522	2.576730
-1391.414511	-9.968847	2.586726
-1389.592153	-2.160842	2.596723
-1387.639847	-8.824717	2.606720
-1385.846026	7.044661	2.616717
-1384.288554	-3.162070	2.626714
-1381.712270	1.803341	2.636710
-1380.011927	2.582966	2.646707
-1378.503225	-7.791202	2.656704
-1376.869594	-4.359505	2.666701
-1374.622911	8.977567	2.676698
-1372.717730	-1.317975	2.686694
-1370.570519	1.117371	2.696691
-1368.801512	-4.623529	2.706688
-1367.062365	-1.565530	2.716685
-1365.352268	-0.665886	2.726682
-1363.434377	6.479531	2.736678
-1361.546967	-4.600995	2.746675
-1359.612133	-4.795141	2.756672
-1357.415935	2.814116	2.766669
-1355.688306	7.755943	2.776666
-1354.050120	-6.200797	2.786662
-1352.264798	-7.114635	2.796659
-1349.992127	-5.714545	2.806656
-1348.303384	-11.022609	2.816653
-1346.321053	-6.243120	2.826650
-1344.385478	-4.766963	2.836646
-1342.864778	-5.905261	2.846643
-1340.760165	5.908906	2.856640
-1338.917680	-3.479796	2.866637
-1337.083091	-4.510449	2.876634
-1335.108675	-0.845917	2.886630
-1333.176953	0.652970	2.896627
-1331.479714	-6.232123	2.906624
-1329.365129	-0.717523	2.916621
-1327.648999	-6.951999	2.926618
-1325.968101	-5.993971	2.936614
-1323.828936	0.134026	2.946611
-1321.925920	-6.916619	2.956608
-1320.130716	-2.636064	2.966605
-1318.282659	-2.971012	2.976602
-1316.559587	-1.241360	2.986598
-1314.366711	-0.819972	2.996595
-1312.551645	-0.919125	3.006592
-1310.637499	0.978883	3.016589
-1308.862970	5.201184	3.026586
-1306.899677	3.286332	3.036582
-1305.340845	-3.830787	3.046579
-1303.474763	5.359676	3.056576
-1301.287697	1.552300	3.066573
-1299.505299	-2.294510	3.076570
-1297.621759	-9.687785	3.086566
-1295.663712	1.482035	3.096563
-1293.766306	6.020975	3.106560
-1291.995710	10.485483	3.116557
-1289.938154	6.086254	3.126554
-1288.060572	-1.793924	3.136550
-1286.210341	-3.480679	3.146547
-1284.698146	-1.603579	3.156544
-1282.677797	-2.987579	3.166541
-1280.885997	3.663390	3.176538
-1278.740598	-3.339179	3.186534
-1276.974309	1.891764	3.196531
-1275.015469	-4.679921	3.206528
-1273.021303	-5.096632	3.216525
-1271.396868	-2.654894	3.226522
-1269.758381	0.433499	3.236518
-1267.548638	-0.320843	3.246515
-1265.629373	-2.689636	3.256512
-1263.753232	-5.397292	3.266509
-1261.919935	-1.568017	3.276506
-1260.072881	-5.152006	3.286502
-1258.116107	0.329502	3.296499
-1256.334022	-0.886883	3.306496
-1254.462945	-0.576561	3.316493
-1252.645612	-0.346053	3.326490
-1250.565683	-8.441727	3.336486
-1248.914094	-1.659357	3.346483
-1246.944393	0.327703	3.356480
-1245.201970	-0.197111	3.366477
-1243.171804	-5.742887	3.376474
-1241.118868	0.518983	3.386470
-1239.308071	-3.657569	3.396467
-1237.685781	0.268646	3.406464
-1235.621411	5.169313	3.416461
-1233.752025	3.645311	3.426458
-1232.174865	-1.851652	3.436454
-1229.959221	-4.446250	3.446451
-1227.973203	-4.812675	3.456448
-1226.172333	0.253313	3.466445
-1224.710857	-3.916276	3.476442
-1222.626838	-2.893212	3.486438
-1220.581136	-4.633297	3.496435
-1218.710347	-4.289746	3.506432
-1217.000990	-1.597890	3.516429
-1214.971578	3.219975	3.526426
-1213.019516	-3.778443	3.536422
-1211.375099	0.017943	3.546419
-1209.181876	5.169579	3.556416
-1207.555197	1.824559	3.566413
-1205.748118	12.544978	3.576410
-1203.838874	7.321715	3.586406
-1201.930198	-3.083205	3.596403
-1200.000110	8.909025	3.606400
-1198.281124	3.490435	3.616397
-1196.217687	-0.161285	3.626394
-1194.326304	-1.237227	3.636390
-1192.557346	-3.097208	3.646387
-1190.185697	3.784724	3.656384
-1188.886961	2.048924	3.666381
-1186.971528	-4.852041	3.676378
-1184.910191	3.487871	3.686374
-1183.062567	-2.881225	3.696371
-1181.380672	0.754461	3.706368
-1179.464096	4.475752	3.716365
-1177.572661	1.269960	3.726362
-1175.536013	-6.335606	3.736358
-1173.854686	-4.120779	3.746355
-1171.776303	-0.572202	3.756352
-1169.883946	-4.998578	3.766349
-1168.248442	-0.229747	3.776346
-1166.179831	4.867662	3.786342
-1164.272494	-2.636687	3.796339
-1162.271423	-4.732715	3.806336
-1160.599314	-0.460754	3.816333
-1158.915641	-11.238560	3.826330
-1157.049103	-3.047447	3.836326
-1154.969882	-7.653696	3.846323
-1153.029447	0.734007	3.856320
-1151.298091	-0.519970	3.866317
-1149.392862	0.386511	3.876314
-1147.496619	-0.885948	3.886310
-1145.245825	-5.723307	3.896307
-1143.947534	0.016795	3.906304
-1141.983055	2.689998	3.916301
-1140.037685	1.471262	3.926298
-1137.923729	-4.165198	3.936294
-1135.916527	-12.471759	3.946291
-1134.407845	-8.588871	3.956288
-1132.425657	-0.842523	3.966285
-1130.860935	2.264089	3.976282
-1128.706406	-2.471020	3.986278
-1126.673402	-5.786255	3.996275
-1124.998929	-10.463509	4.006272
-1123.057056	-8.419790	4.016269
-1121.260745	2.202953	4.026266
-1119.133845	-3.067692	4.036262
-1117.427086	-0.459023	4.046259
-1115.719713	0.037061	4.056256
-1113.535107	-3.569238	4.066253
-1111.784433	0.857550	4.076250
-1109.971545	4.889152	4.086246
-1107.989224	-8.909356	4.096243
-1106.173339	-6.897570	4.106240
-1104.473069	-0.282335	4.116237
-1102.421743	-0.292810	4.126234
-1100.761221	2.035919	4.136230
-1098.602258	-6.193847	4.146227
-1096.583733	0.984656	4.156224
-1094.946348	-5.387059	4.166221
-1093.008190	-5.537307	4.176218
-1091.269545	0.489208	4.186214
-1089.141916	-11.207407	4.196211
-1087.092325	0.323734	4.206208
-1085.426672	-7.250837	4.216205
-1084.121251	-7.711947	4.226202
-1081.690651	1.959959	4.236198
-1079.742060	-7.592366	4.246195
-1078.022187	-6.971947	4.256192
-1076.130341	-10.908727	4.266189
-1074.243280	-9.991385	4.276186
-1072.547325	-2.271826	4.286182
-1070.555687	-7.350278	4.296179
-1068.558012	-10.557188	4.306176
-1066.794325	-9.043830	4.316173
-1064.697272	-5.477617	4.326170
-1063.182129	-6.420649	4.336166
-1061.084447	-15.906808	4.346163
-1059.329316	-7.366236	4.356160
-1057.406194	-5.842057	4.366157
-1055.602826	0.401488	4.376154
-1053.820423	-11.536706	4.386150
-1051.799326	-3.498106	4.396147
-1049.893743	-4.484631	4.406144
-1047.728871	-2.053383	4.416141
-1046.139512	-7.844266	4.426138
-1044.299975	-2.509594	4.436134
-1042.317743	-15.823331	4.446131
-1040.470688	-5.944378	4.456128
-1038.842023	-6.529787	4.466125
-1036.698237	-3.559929	4.476122
-1034.772757	-12.398043	4.486118
-1032.880076	-6.855562	4.496115
-1031.042135	-9.782701	4.506112
-1029.125021	-3.374181	4.516109
-1027.756607	-8.155572	4.526106
-1025.826679	-5.233601	4.536102
-1023.502864	-8.863661	4.546099
-1021.440364	-15.255948	4.556096
-1019.598111	-2.512189	4.566093
-1018.134606	-13.412583	4.576090
-1016.364907	-10.174474	4.586086
-1014.225734	-6.949664	4.596083
-1012.222018	2.782696	4.606080
-1010.467648	-5.994885	4.616077
-1008.586572	-9.142049	4.626074
-1006.807575	-11.251377	4.636070
-1004.812578	3.335745	4.646067
-1003.246431	-10.369295	4.656064
-1001.219004	-2.145355	4.666061
-999.171256	-5.147073	4.676058
-997.159715	-4.464296	4.686054
-995.435747	-4.670205	4.696051
-993.492405	-4.241765	4.706048
-991.758277	-5.128199	4.716045
-989.993796	-6.837325	4.726042
-988.062370	0.794127	4.736038
-985.942385	3.328922	4.746035
-983.915285	0.275258	4.756032
-982.561716	-3.224873	4.766029
-980.305029	0.920591	4.776026
-978.616188	0.614529	4.786022
-976.785852	-4.224913	4.796019
-975.023578	-8.369829	4.806016
-973.060688	-7.802402	4.816013
-971.002256	-4.337286	4.826010
-969.090185	0.125383	4.836006
-967.306431	-2.242029	4.846003
-965.301272	-6.976793	4.856000
-963.650818	2.384235	4.865997
-961.772381	0.636382	4.875994
-959.873645	-0.102677	4.885990
-957.774721	0.902455	4.895987
-956.002076	-6.352849	4.905984
-954.360454	10.474375	4.915981
-952.376343	-2.320173	4.925978
-950.823018	0.726813	4.935974
-948.536929	1.454149	4.945971
-946.410359	1.123905	4.955968
-944.782527	1.211281	4.965965
-942.798613	-1.295478	4.975962
-941.086650	-2.925124	4.985958
-939.306773	1.182943	4.995955
-937.392156	-4.801977	5.005952
-935.702158	-1.105825	5.015949
-933.431768	-1.801661	5.025946
-931.507409	-2.885823	5.035942
-929.636056	-4.155707	5.045939
-928.230742	-2.190232	5.055936
-926.239509	-6.848532	5.065933
-923.941762	-6.021992	5.075930
-922.097688	1.258773	5.085926
-920.403798	-9.173179	5.095923
-918.800004	-1.446654	5.105920
-916.677035	0.779854	5.115917
-914.771072	-3.776390	5.125914
-912.955822	-3.878420	5.135910
-911.069314	-5.723833	5.145907
-909.005318	1.835973	5.155904
-907.008980	-7.655971	5.165901
-905.507409	-3.460754	5.175898
-903.528377	-7.397133	5.185894
-901.450508	-3.581400	5.195891
-899.598189	-5.850783	5.205888
-898.022731	-15.820129	5.215885
-896.368439	-3.608273	5.225882
-894.248345	-7.437732	5.235878
-891.910163	-10.839452	5.245875
-890.475492	-2.665896	5.255872
-888.655116	-7.563676	5.265869
-886.775244	-11.010535	5.275866
-884.635351	-1.868209	5.285862
-882.915008	-0.347779	5.295859
-880.768843	-12.816092	5.305856
-879.027408	0.775969	5.315853
-877.407910	-7.165279	5.325850
-875.397011	-4.999760	5.335846
-873.645004	-3.648586	5.345843
-871.675270	-2.509046	5.355840
-869.773497	-4.570011	5.365837
-867.656141	-3.574060	5.375834
-866.081094	-4.992303	5.385830
-864.169835	-5.426991	5.395827
-862.314218	-13.085468	5.405824
-860.299889	0.121954	5.415821
-858.309955	-5.827580	5.425818
-856.446887	-5.108317	5.435814
-854.881228	-7.964959	5.445811
-853.054574	-6.944628	5.455808
-851.094770	-3.703621	5.465805
-849.121321	-3.993511	5.475802
-847.296229	-2.923981	5.485798
-845.257694	-7.709771	5.495795
-843.704559	-4.814251	5.505792
-841.541420	-5.358653	5.515789
-839.801585	-6.834797	5.525786
-837.716303	-0.445093	5.535782
-835.765343	-7.867757	5.545779
-834.192075	-8.431540	5.555776
-832.331673	-3.133181	5.565773
-830.252434	-2.055318	5.575770
-828.460541	-11.336112	5.585766
-826.541079	-5.016204	5.595763
-824.697049	-2.831861	5.605760
-822.740362	-7.634548	5.615757
-821.056671	-5.486149	5.625754
-819.309673	2.152832	5.635750
-817.333229	-9.252584	5.645747
-815.308588	-2.027430	5.655744
-813.308120	-11.872044	5.665741
-811.693949	0.523129	5.675738
-809.547936	-0.114816	5.685734
-807.876200	-11.345212	5.695731
-805.988564	-3.970266	5.705728
-804.099519	-3.572461	5.715725
-802.302592	-5.261375	5.725722
-800.211491	-4.305374	5.735718
-798.189950	-4.184514	5.745715
-796.529779	-6.217858	5.755712
-795.063065	-3.409537	5.765709
-792.821645	4.530945	5.775706
-791.056086	-1.921064	5.785702
-789.228063	0.867407	5.795699
-786.931722	-4.610026	5.805696
-785.266667	4.505671	5.815693
-783.670489	-0.495142	5.825690
-781.711346	-1.951036	5.835686
-779.548006	-8.523448	5.845683
-777.487841	-1.667071	5.855680
-775.957164	-7.467357	5.865677
-774.146002	-4.461457	5.875674
-771.771724	-5.424779	5.885670
-770.053701	-1.725086	5.895667
-768.513004	-5.463417	5.905664
-766.822004	-4.741844	5.915661
-764.561322	-8.118427	5.925658
-762.821927	-7.325643	5.935654
-761.004554	-1.226186	5.945651
-759.057876	3.294287	5.955648
-757.239059	-3.709333	5.965645
-755.196638	-1.190348	5.975642
-753.434786	-3.677253	5.985638
-751.567034	-4.046480	5.995635
-749.748554	-0.601231	6.005632
-747.688195	-5.523054	6.015629
-745.715627	-0.812509	6.025626
-743.903111	-5.312640	6.035622
-742.330388	-0.876066	6.045619
-740.594452	0.731972	6.055616
-738.548119	-3.491330	6.065613
-736.526421	5.216909	6.075610
-734.380257	-1.054321	6.085606
-732.564688	-2.602488	6.095603
-730.864025	-4.793827	6.105600
-729.331453	-7.725623	6.115597
-727.167961	-4.619683	6.125594
-725.486931	-3.847543	6.135590
-723.029030	-4.230533	6.145587
-721.673530	-6.421968	6.155584
-719.608307	-2.133550	6.165581
-717.929604	-1.349980	6.175578
-716.152825	-3.667149	6.185574
-714.200222	-3.412052	6.195571
-711.927872	-3.490660	6.205568
-710.047729	-0.926757	6.215565
-708.440821	0.027756	6.225562
-706.532740	-9.097853	6.235558
-704.538703	-7.827855	6.245555
-702.743033	-4.252616	6.255552
-701.052380	-2.897822	6.265549
-699.167692	-5.754821	6.275546
-697.008340	-9.045681	6.285542
-695.263602	-2.718261	6.295539
-693.368598	2.154715	6.305536
-691.412149	0.781425	6.315533
-689.827019	6.968577	6.325530
-687.873280	1.223890	6.335526
-685.861902	-3.772156	6.345523
-683.833300	-3.027103	6.355520
-682.154407	-5.483334	6.365517
-680.143385	-9.805149	6.375514
-678.517338	7.967377	6.385510
-676.483478	-3.968138	6.395507
-674.529166	3.179972	6.405504
-672.594208	-1.878060	6.415501
-670.613802	-4.827694	6.425498
-668.838474	-0.275028	6.435494
-667.443205	-0.704478	6.445491
-665.129966	-5.215087	6.455488
-663.575370	-1.182904	6.465485
-661.426194	-6.485140	6.475482
-659.585691	-6.321027	6.485478
-657.514424	-5.991690	6.495475
-655.983820	0.289454	6.505472
-654.050380	-2.041649	6.515469
-652.098895	-8.431694	6.525466
-650.095477	-12.742796	6.535462
-648.352887	-8.300142	6.545459
-646.247999	6.190845	6.555456
-644.601008	0.228374	6.565453
-642.787703	-4.508638	6.575450
-640.967145	3.042953	6.585446
-638.981102	-13.818791	6.595443
-637.301644	-1.557057	6.605440
-635.400228	-1.418445	6.615437
-633.379132	-6.430211	6.625434
-631.287603	-9.242839	6.635430
-629.538706	-9.071962	6.645427
-627.668853	-2.526070	6.655424
-625.890648	-9.987291	6.665421
-624.266361	-0.726016	6.675418
-621.986600	-9.596753	6.685414
-620.224844	-5.472908	6.695411
-618.320656	-0.585547	6.705408
-616.343983	-6.387522	6.715405
-614.351055	-2.518483	6.725402
-612.596455	-9.412275	6.735398
-611.079330	-6.357693	6.745395
-609.167228	-8.360108	6.755392
-607.075089	-2.931221	6.765389
-604.839594	-15.230445	6.775386
-603.557151	0.967658	6.785382
-601.435800	-7.137276	6.795379
-599.400890	-5.347960	6.805376
-597.694778	-8.206352	6.815373
-595.753741	1.313802	6.825370
-593.968794	-3.454960	6.835366
-591.877082	-8.012212	6.845363
-590.229806	-8.451876	6.855360
-588.397362	-1.860503	6.865357
-586.584460	-4.778576	6.875354
-584.597913	-3.996721	6.885350
-582.548409	-1.884478	6.895347
-580.750027	-8.374742	6.905344
-579.074422	1.102569	6.915341
-577.297377	-4.801691	6.925338
-574.908807	-8.387991	6.935334
-573.168270	-9.065158	6.945331
-571.611924	-3.534863	6.955328
-569.525356	-0.969083	6.965325
-567.780338	-2.204297	6.975322
-565.590710	-6.385614	6.985318
-563.884946	-6.810919	6.995315
-562.105440	-3.885052	7.005312
-560.012120	-0.300405	7.015309
-558.079523	-1.598729	7.025306
-556.863088	-0.946457	7.035302
-554.773861	-6.941615	7.045299
-552.463588	-1.416474	7.055296
-550.822877	-2.153465	7.065293
-548.945725	-11.035615	7.075290
-547.251213	-6.315219	7.085286
-545.111390	-9.170222	7.095283
-543.169534	-2.124211	7.105280
-541.426864	1.966434	7.115277
-539.371986	-6.686747	7.125274
-537.688667	-4.400721	7.135270
-535.855373	-10.195520	7.145267
-533.581477	-9.019020	7.155264
-532.267012	-5.971488	7.165261
-530.325091	-12.194134	7.175258
-528.044682	-8.495666	7.185254
-526.375379	-10.456079	7.195251
-524.412598	-4.076511	7.205248
-522.780083	-5.317406	7.215245
-520.658986	-3.664937	7.225242
-518.834054	-7.440618	7.235238
-517.058271	-13.840391	7.245235
-514.799131	-0.820136	7.255232
-513.303579	-4.944236	7.265229
-511.433999	-8.869139	7.275226
-509.585530	-5.254815	7.285222
-507.635038	-9.249476	7.295219
-505.485027	-8.171576	7.305216
-503.891743	-2.258735	7.315213
-502.260647	-2.177891	7.325210
-500.392596	-10.889618	7.335206
-498.204180	-6.590674	7.345203
-496.327247	-6.629609	7.355200
-494.502793	-6.705949	7.365197
-492.395488	-5.488593	7.375194
-490.660509	-2.167161	7.385190
-488.898746	-3.878648	7.395187
-486.925441	-8.900032	7.405184
-485.097615	-4.085622	7.415181
-483.256653	-9.340063	7.425178
-481.521037	-8.020711	7.435174
-479.340462	-9.723288	7.445171
-477.497822	-5.146487	7.455168
-476.021838	-7.134411	7.465165
-474.035388	-1.153290	7.475162
-471.986150	-4.527417	7.485158
-470.019093	-4.585460	7.495155
-468.055656	0.884637	7.505152
-466.070250	-8.512084	7.515149
-464.736589	-2.878261	7.525146
-462.422082	-1.303990	7.535142
-460.643753	-9.155098	7.545139
-458.789602	-6.913662	7.555136
-457.053015	-1.664684	7.565133
-455.076357	2.450238	7.575130
-453.160903	-7.225813	7.585126
-451.510252	-8.848481	7.595123
-449.733742	-0.239759	7.605120
-447.578066	-0.149493	7.615117
-445.578449	-2.424688	7.625114
-443.672724	-2.045047	7.635110
-442.172541	-3.357910	7.645107
-439.733819	-9.287210	7.655104
-438.175590	-5.373866	7.665101
-436.364411	-3.686042	7.675098
-434.351798	-7.013239	7.685094
-432.486861	-9.513218	7.695091
-430.861038	-3.742879	7.705088
-428.634671	-6.141104	7.715085
-427.007834	-1.834519	7.725082
-425.148694	-8.866453	7.735078
-423.392154	-11.105973	7.745075
-421.366049	-8.836704	7.755072
-419.339371	-14.739662	7.765069
-417.531032	-8.346392	7.775066
-415.884143	-9.703188	7.785062
-413.640086	-10.329593	7.795059
-411.923383	-10.786536	7.805056
-410.408069	2.295764	7.815053
-408.029468	-12.108663	7.825050
-406.109789	-9.970800	7.835046
-404.293436	-11.763569	7.845043
-402.338269	-3.265435	7.855040
-400.675408	-8.920829	7.865037
-398.820981	-10.688096	7.875034
-397.177206	-10.640782	7.885030
-395.191806	-4.894673	7.895027
-393.003780	-8.314576	7.905024
-391.067208	-5.696269	7.915021
-389.638257	-9.677039	7.925018
-387.550608	-10.385810	7.935014
-385.552204	-6.959524	7.945011
-383.962827	-5.122570	7.955008
-382.063237	1.033546	7.965005
-379.826913	-2.915080	7.975002
-378.098979	3.581059	7.984998
-376.121417	-0.411509	7.994995
-374.419938	-1.557533	8.004992
-372.532943	0.607681	8.014989
-370.628432	-4.113702	8.024986
-368.845698	-2.013940	8.034982
-366.938943	-0.246590	8.044979
-365.124095	-2.598004	8.054976
-363.249478	2.592699	8.064973
-361.288494	-4.131786	8.074970
-359.195753	-10.634158	8.084966
-357.528900	-6.785465	8.094963
-355.647506	-8.018616	8.104960
-353.753639	-10.946287	8.114957
-351.734397	-7.649607	8.124954
-349.993654	-7.729840	8.134950
-348.418950	-6.288390	8.144947
-346.146037	-4.721575	8.154944
-344.521161	-9.347772	8.164941
-342.921953	-3.249454	8.174938
-340.451298	-9.355854	8.184934
-338.288620	-6.064692	8.194931
-336.809272	-11.957576	8.204928
-335.323040	-8.637368	8.214925
-332.965413	-0.206575	8.224922
-331.533648	-0.120635	8.234918
-329.394503	-11.218542	8.244915
-327.431634	-7.759693	8.254912
-325.506222	-3.904885	8.264909
-323.682780	-0.003798	8.274906
-321.783654	-0.379277	8.284902
-319.708313	-6.525179	8.294899
-317.960415	-5.755528	8.304896
-316.701036	-2.959588	8.314893
-314.769126	-0.124168	8.324890
-312.356629	-4.362946	8.334886
-310.324351	-3.894459	8.344883
-308.519533	-4.559593	8.354880
-307.035840	-5.482922	8.364877
-305.152836	-9.267719	8.374874
-303.025991	-4.747192	8.384870
-301.121697	-3.909342	8.394867
-299.293756	-9.981000	8.404864
-297.550810	-1.291009	8.414861
-295.652976	-6.486506	8.424858
-293.569494	-8.388144	8.434854
-291.796903	-13.835208	8.444851
-290.156768	-3.752041	8.454848
-288.244879	-3.095381	8.464845
-286.127970	-5.177603	8.474842
-284.391682	-5.752837	8.484838
-282.446068	0.354967	8.494835
-280.398387	-5.855958	8.504832
-278.641433	-3.283092	8.514829
-276.872840	-6.042298	8.524826
-275.193188	-0.348325	8.534822
-272.784599	-2.454987	8.544819
-271.116574	0.083134	8.554816
-269.494198	0.672341	8.564813
-267.440192	-2.546074	8.574810
-265.631590	-5.584800	8.584807
-263.580029	-6.232444	8.594803
-262.041950	-10.266875	8.604800
-260.077083	-4.604206	8.614797
-257.978157	-3.276362	8.624794
-256.195166	-2.888035	8.634791
-254.566394	-5.572807	8.644787
-252.054753	-9.881031	8.654784
-250.608697	-4.326590	8.664781
-248.523737	-14.732140	8.674778
-246.698849	-10.147581	8.684775
-245.141585	-9.821109	8.694771
-243.273316	-5.865538	8.704768
-241.093728	-1.192327	8.714765
-239.319508	-3.112454	8.724762
-237.161834	-9.306164	8.734759
-235.183052	-14.337701	8.744755
-233.740012	-12.516762	8.754752
-231.899665	-5.272707	8.764749
-229.682454	-11.911676	8.774746
-228.038434	-10.200172	8.784743
-226.391403	-5.656680	8.794739
-223.944271	-16.929964	8.804736
-222.379849	-7.399892	8.814733
-220.580922	-16.916663	8.824730
-218.961991	-12.603933	8.834727
-216.814021	-19.536556	8.844723
-214.793909	-17.995584	8.854720
-213.459122	-10.121393	8.864717
-211.060210	-15.463103	8.874714
-209.195515	-9.029711	8.884711
-207.468637	-18.331302	8.894707
-205.659864	-10.545378	8.904704
-203.768825	-8.317520	8.914701
-201.697607	-17.628272	8.924698
-199.841138	-18.164207	8.934695
-198.185005	-10.912834	8.944691
-195.908319	-11.059536	8.954688
-194.350341	-19.483161	8.964685
-192.444948	-17.887549	8.974682
-190.569605	-8.771787	8.984679
-188.478421	-18.556213	8.994675
-186.654680	-14.634544	9.004672
-185.288327	-17.323180	9.014669
-182.890047	-19.691776	9.024666
-181.327612	-14.992658	9.034663
-179.038812	-17.088006	9.044659
-177.255549	-15.468157	9.054656
-175.604514	-18.467463	9.064653
-173.845511	-11.935077	9.074650
-171.850816	-10.154762	9.084647
-169.528727	-17.014086	9.094643
-168.269848	-12.500190	9.104640
-166.335478	-14.946316	9.114637
-164.195584	-12.008179	9.124634
-162.220556	-18.262674	9.134631
-160.400479	-20.508989	9.144627
-158.449002	-14.319917	9.154624
-156.785496	-12.527794	9.164621
-154.968538	-13.614727	9.174618
-153.059194	-13.446999	9.184615
-151.361952	-11.098182	9.194611
-149.264145	-11.547858	9.204608
-147.148993	-6.303784	9.214605
-145.736805	-13.963639	9.224602
-143.690536	-13.544610	9.234599
-141.691215	-10.704016	9.244595
-139.685063	-7.116131	9.254592
-137.962233	-1.523675	9.264589
-136.177005	-4.482794	9.274586
-134.347359	-2.254557	9.284583
-132.469326	-8.218837	9.294579
-130.649675	-1.820818	9.304576
-128.501436	2.871714	9.314573
-126.734226	-6.974661	9.324570
-124.745507	-7.326389	9.334567
-123.042476	-7.046777	9.344563
-121.280718	-10.977874	9.354560
-119.139892	-13.242178	9.364557
-117.213243	-7.795906	9.374554
-115.456029	-5.950812	9.384551
-113.586207	-3.975271	9.394547
-111.879283	-8.145494	9.404544
-110.032640	-2.905910	9.414541
-107.728709	-6.377215	9.424538
-106.078049	-6.245542	9.434535
-104.079117	-4.397954	9.444531
-102.220487	-2.412724	9.454528
-100.590290	-3.106684	9.464525
-98.981318	-6.002921	9.474522
-96.835970	-1.050968	9.484519
-94.665784	-9.112768	9.494515
-92.878024	-3.955350	9.504512
-91.190815	2.500147	9.514509
-89.219403	-1.514901	9.524506
-87.327612	0.911868	9.534503
-85.435956	-5.015082	9.544499
-83.217396	-3.778797	9.554496
-81.832058	-7.791914	9.564493
-79.997816	-5.228071	9.574490
-77.885834	-0.845481	9.584487
-76.046768	-6.735614	9.594483
-74.163664	-9.285590	9.604480
-72.572899	-2.530501	9.614477
-70.566872	-5.739522	9.624474
-68.679694	-3.285162	9.634471
-66.867481	-0.236242	9.644467
-64.695768	1.198575	9.654464
-62.945113	2.997390	9.664461
-60.879957	6.257004	9.674458
-59.382842	1.569260	9.684455
-57.411297	1.765034	9.694451
-55.318248	-5.157126	9.704448
-53.520999	-2.500523	9.714445
-51.627230	6.314027	9.724442
-50.067841	-4.097538	9.734439
-47.799475	-3.687016	9.744435
-46.141738	2.842687	9.754432
-44.135768	0.334708	9.764429
-42.514201	0.297390	9.774426
-40.503524	-1.884513	9.784423
-38.417929	-3.247884	9.794419
-36.537814	-12.736440	9.804416
-34.782513	-6.347026	9.814413
-32.869206	-3.372624	9.824410
-31.218967	-4.857586	9.834407
-29.271386	-3.347513	9.844403
-27.307615	-6.660280	9.854400
-25.332047	-1.995371	9.864397
-23.270743	-10.432882	9.874394
-21.648043	-4.420178	9.884391
-20.070955	-7.925456	9.894387
-18.057736	-8.520991	9.904384
-16.094714	-5.529244	9.914381
-14.064805	0.636398	9.924378
-12.180489	-2.398436	9.934375
-10.402985	-4.569963	9.944371
-8.619761	-7.996014	9.954368
-6.612582	-1.632541	9.964365
-4.877573	2.925502	9.974362
-3.589798	20.154201	9.984359
-2.345154	58.502394	9.994355
-1.163844	120.305468	10.004352
0.000000	167.372933	10.009357
0.926856	192.280001	10.014362
1.518281	223.313124	10.019367
1.631021	254.077328	10.024371
2.351444	272.585414	10.029376
2.644804	288.725371	10.034381
2.950670	296.964788	10.039386
3.342163	314.197664	10.044391
3.410837	324.565866	10.049395
3.602672	317.748547	10.054400
3.734413	334.458356	10.059405
3.718618	327.945372	10.064410
4.030357	339.567855	10.069415
3.711973	340.960716	10.074419
3.905765	334.860557	10.079424
3.979924	343.058113	10.084429
3.790407	344.400459	10.089434
4.152236	334.148384	10.094439
4.102019	352.779489	10.099443
4.193755	349.078268	10.104448
4.302483	358.916582	10.109453
4.078685	344.675362	10.114458
4.013988	337.365965	10.119463
4.116580	347.908538	10.124467
4.320601	347.182325	10.129472
4.389844	365.283484	10.134477
4.216569	365.341237	10.139482
4.524857	356.414382	10.144487
4.526190	365.689538	10.149491
4.329222	368.497997	10.154496
4.584239	370.305583	10.159501
4.428611	363.269285	10.164506
4.760651	365.006241	10.169511
4.575169	372.510399	10.174515
5.033702	365.518062	10.179520
4.726938	367.716435	10.184525
4.728504	372.956319	10.189530
4.807959	371.903059	10.194535
4.537727	378.908252	10.199539
4.865502	374.830346	10.204544
4.804685	375.146117	10.209549
5.057262	373.286264	10.214554
4.967850	378.868652	10.219559
4.894653	374.616592	10.224563
4.964155	372.683442	10.229568
5.052344	376.812001	10.234573
5.338526	375.598041	10.239578
5.296138	382.366631	10.244583
5.137069	386.681280	10.249587
5.297276	378.680007	10.254592
5.286208	379.735285	10.259597
5.148646	388.294628	10.264602
5.786938	397.454019	10.269607
5.144612	404.720413	10.274611
5.869900	402.383055	10.279616
5.549882	397.651560	10.284621
5.571101	409.944884	10.289626
5.729053	420.093920	10.294631
5.749755	419.665014	10.299635
5.499158	421.471252	10.304640
5.971199	425.939132	10.309645
5.994133	418.445413	10.314650
6.224212	417.528968	10.319655
5.955976	417.821054	10.324659
6.222564	421.746138	10.329664
6.095989	414.883369	10.334669
5.955025	420.000929	10.339674
6.395356	419.724281	10.344679
6.301026	418.025405	10.349683
6.207005	398.670088	10.354688
6.202785	407.764815	10.359693
6.393335	410.267057	10.364698
6.599239	410.376291	10.369703
6.147919	417.971757	10.374707
6.538581	427.883417	10.379712
6.590508	429.253490	10.384717
6.262445	433.025850	10.389722
6.629359	439.632994	10.394727
6.769612	439.768468	10.399731
6.480991	443.936647	10.404736
6.490530	445.690359	10.409741
6.540444	445.200025	10.414746
6.811239	442.750655	10.419751
6.682681	438.892166	10.424755
6.650099	445.534647	10.429760
6.695849	458.719774	10.434765
6.833127	446.175944	10.439770
7.306642	442.278193	10.444775
7.109034	450.960686	10.449779
7.170324	444.283973	10.454784
7.174677	451.439363	10.459789
6.952310	455.895010	10.464794
7.107678	461.367429	10.469799
6.800002	463.712612	10.474803
7.093268	467.732797	10.479808
7.429325	485.491941	10.484813
7.431117	490.389646	10.489818
7.637204	488.996070	10.494823
7.554715	491.453569	10.499827
7.490782	485.438607	10.504832
7.668065	493.312306	10.509837
7.618965	497.972134	10.514842
7.966340	492.446634	10.519847
7.447421	488.281400	10.524851
7.685431	487.628604	10.529856
7.891444	488.802225	10.534861
7.896204	487.975328	10.539866
7.993527	485.634041	10.544871
7.695189	494.698466	10.549875
8.096952	491.480751	10.554880
7.639118	499.118297	10.559885
7.536017	492.291169	10.564890
7.894615	485.721554	10.569895
7.960690	496.348904	10.574899
8.005446	486.486326	10.579904
7.812413	482.097235	10.584909
7.947306	501.405456	10.589914
8.250124	517.966770	10.594919
8.491058	517.797614	10.599923
8.582661	525.350694	10.604928
8.571838	529.717432	10.609933
8.835828	525.309049	10.614938
8.855504	516.614202	10.619943
8.597602	512.290639	10.624947
8.409592	502.745863	10.629952
8.708254	512.099842	10.634957
8.757247	520.372473	10.639962
9.046911	529.857204	10.644967
8.510200	526.860125	10.649971
8.885431	523.329678	10.654976
8.701845	537.775129	10.659981
8.952247	529.399854	10.664986
9.176294	533.946744	10.669991
9.276795	545.207285	10.674995
9.028595	539.688452	10.680000
9.135424	538.905194	10.685005
8.884693	538.448617	10.690010
9.311334	533.146993	10.695015
9.187688	531.664084	10.700019
9.170161	536.367773	10.705024
8.683830	534.382911	10.710029
8.838089	542.766495	10.715034
9.090629	539.746028	10.720039
8.825930	551.859580	10.725043
9.035098	556.850383	10.730048
9.297953	572.579222	10.735053
9.180502	572.758954	10.740058
9.465000	558.151032	10.745063
9.283550	577.951343	10.750067
9.424923	575.167790	10.755072
10.106209	583.058921	10.760077
9.780262	594.661898	10.765082
10.223001	582.162267	10.770087
10.208637	580.844844	10.775091
10.173654	570.252205	10.780096
10.227436	572.497178	10.785101
9.823590	568.304104	10.790106
10.055639	571.777436	10.795111
10.048604	581.456176	10.800115
10.144295	575.450408	10.805120
10.189835	576.678016	10.810125
9.962682	574.871000	10.815130
10.216341	576.297218	10.820135
10.313122	595.651067	10.825139
10.749321	591.836498	10.830144
10.566103	578.708177	10.835149
10.313123	584.111735	10.840154
11.012771	567.871722	10.845159
10.614156	575.392633	10.850163
10.560262	576.265527	10.855168
10.768768	582.264087	10.860173
10.484007	585.480817	10.865178
10.600916	573.110431	10.870183
10.381476	590.310196	10.875187
10.886212	599.287599	10.880192
11.177415	599.080464	10.885197
11.042476	601.201004	10.890202
11.104718	606.588986	10.895207
10.961048	613.342299	10.900211
10.923651	603.953202	10.905216
11.219336	611.688237	10.910221
11.054536	603.801753	10.915226
11.268197	609.357968	10.920231
11.414818	607.220105	10.925235
11.156221	600.258459	10.930240
11.360255	604.439568	10.935245
11.179573	607.113015	10.940250
11.515816	597.596521	10.945255
11.135959	603.704700	10.950259
11.522525	607.568123	10.955264
11.536375	611.383763	10.960269
11.397937	613.894360	10.965274
11.547742	608.159060	10.970279
11.012700	618.578033	10.975283
11.318977	616.403665	10.980288
11.177063	611.902304	10.985293
11.546339	638.280453	10.990298
11.772380	639.812005	10.995303
11.228771	647.248849	11.000307
12.108152	641.080213	11.005312
12.228557	646.742778	11.010317
12.138219	651.265734	11.015322
12.551109	637.348442	11.020327
12.197526	635.564736	11.025331
12.495676	637.114749	11.030336
12.290112	644.335253	11.035341
12.365204	642.532059	11.040346
12.596401	623.977679	11.045351
12.104419	615.802760	11.050355
12.301371	620.893303	11.055360
12.325107	630.603436	11.060365
12.507839	636.369593	11.065370
12.694555	639.782365	11.070375
12.598353	644.596406	11.075379
12.474266	632.726442	11.080384
12.816432	628.974169	11.085389
12.571549	633.152771	11.090394
12.707848	631.921697	11.095399
12.788261	638.017979	11.100403
12.818081	636.054855	11.105408
13.020764	623.871013	11.110413
12.844324	628.707307	11.115418
12.937411	637.699929	11.120423
12.578837	642.249895	11.125427
12.912226	643.201369	11.130432
12.961724	639.661348	11.135437
12.735880	642.002968	11.140442
13.004340	634.517285	11.145447
12.955122	650.403213	11.150451
13.163958	638.718258	11.155456
13.138978	635.068695	11.160461
13.148071	642.409498	11.165466
13.138397	636.441010	11.170471
13.044815	655.700725	11.175475
13.344772	663.110263	11.180480
13.702901	665.869667	11.185485
13.657985	669.097045	11.190490
13.935636	658.738322	11.195495
13.687673	672.490871	11.200499
13.780825	674.019969	11.205504
13.873461	671.420786	11.210509
13.850526	668.354346	11.215514
13.697128	657.922451	11.220519
13.747377	670.433712	11.225523
13.956282	663.556740	11.230528
14.005822	671.004645	11.235533
13.970452	672.046474	11.240538
14.202895	663.885293	11.245543
14.064205	669.228077	11.250547
13.980942	681.446836	11.255552
14.324515	673.113387	11.260557
13.973186	667.907413	11.265562
14.215683	660.473165	11.270567
14.151053	667.787894	11.275571
14.407442	674.912657	11.280576
14.243228	674.727697	11.285581
13.900469	671.269153	11.290586
14.197517	672.038773	11.295591
14.018830	669.227404	11.300595
14.267939	682.470185	11.305600
14.423309	687.953728	11.310605
14.420754	692.070044	11.315610
14.649553	701.709673	11.320615
14.693835	699.935040	11.325619
14.885170	698.810298	11.330624
14.785788	702.300254	11.335629
14.485968	712.360085	11.340634
14.978988	697.367112	11.345639
14.921185	698.021446	11.350643
14.668004	703.715233	11.355648
15.312390	698.801436	11.360653
14.969176	708.306802	11.365658
15.120934	699.619164	11.370663
15.053969	709.242894	11.375667
15.208900	703.114087	11.380672
15.304361	697.463112	11.385677
14.879506	701.749284	11.390682
15.189450	698.945130	11.395687
15.441905	698.526559	11.400691
15.371871	698.066386	11.405696
15.672127	711.170152	11.410701
15.456822	713.497487	11.415706
15.464254	707.393780	11.420711
15.681351	716.349326	11.425715
15.870951	709.260951	11.430720
15.941584	706.849770	11.435725
16.040528	692.238193	11.440730
16.264469	689.597564	11.445735
15.884441	689.804984	11.450739
15.987083	690.463689	11.455744
15.902347	693.863000	11.460749
16.033042	693.761888	11.465754
16.002654	694.621579	11.470759
15.820164	700.023398	11.475763
16.108697	683.006754	11.480768
16.152862	690.002950	11.485773
15.727289	694.145735	11.490778
16.223205	690.734769	11.495783
16.335165	700.602763	11.500787
16.540695	698.846566	11.505792
16.311516	682.904375	11.510797
16.555888	695.963425	11.515802
16.252073	692.426127	11.520807
16.150061	699.899795	11.525811
16.602864	720.067486	11.530816
16.946645	718.795428	11.535821
16.505213	718.724066	11.540826
16.906994	710.608389	11.545831
16.941488	716.297299	11.550835
16.628283	702.429521	11.555840
16.671673	686.044893	11.560845
16.889319	703.993501	11.565850
17.365179	697.826126	11.570855
17.139330	697.707764	11.575859
16.837064	697.959551	11.580864
16.899466	684.692612	11.585869
16.526591	692.475976	11.590874
17.233604	704.417327	11.595879
17.342854	709.799427	11.600883
17.416621	723.513326	11.605888
17.493460	711.701135	11.610893
17.092938	698.754016	11.615898
17.146848	688.531880	11.620903
17.153859	713.761606	11.625907
17.099687	716.277703	11.630912
17.718920	724.935733	11.635917
17.703071	720.956692	11.640922
17.405178	725.631043	11.645927
17.616369	723.894441	11.650931
17.909547	713.350280	11.655936
17.817936	711.201513	11.660941
17.549209	722.025928	11.665946
18.020872	719.765246	11.670951
18.128679	722.422663	11.675955
18.070430	710.242519	11.680960
17.935066	695.807077	11.685965
17.573056	701.858835	11.690970
17.753588	709.740020	11.695975
18.002312	714.983185	11.700979
17.948998	722.338713	11.705984
18.005234	712.275459	11.710989
17.615564	725.856698	11.715994
17.975209	717.743007	11.720999
17.674651	725.226278	11.726003
17.891799	737.792978	11.731008
18.038637	732.881256	11.736013
17.979934	752.085075	11.741018
18.125698	750.029328	11.746023
18.312707	762.832664	11.751027
18.137292	761.193987	11.756032
18.363534	750.160591	11.761037
18.143698	761.801969	11.766042
18.470690	754.051427	11.771047
18.660556	755.159839	11.776051
18.986412	774.917355	11.781056
19.121406	764.623887	11.786061
18.958061	752.061508	11.791066
18.870399	748.839797	11.796071
18.769636	744.596754	11.801075
19.143870	751.217069	11.806080
18.983069	743.396101	11.811085
18.788134	754.140963	11.816090
19.065461	750.428963	11.821095
19.244395	761.964163	11.826099
19.065429	753.425433	11.831104
19.655253	747.720822	11.836109
19.440008	745.035115	11.841114
19.412870	742.197984	11.846119
19.316568	741.016614	11.851123
19.288035	745.203319	11.856128
19.533961	736.273562	11.861133
19.042859	753.737619	11.866138
19.416175	754.383118	11.871143
19.507278	768.844911	11.876147
19.561865	776.014526	11.881152
19.564204	771.490108	11.886157
19.697610	779.564925	11.891162
19.782905	781.954712	11.896167
19.830071	779.495224	11.901171
19.875526	780.856902	11.906176
19.904264	775.623385	11.911181
19.909593	778.845928	11.916186
20.033451	775.603091	11.921191
19.753242	775.576976	11.926195
19.792760	783.479115	11.931200
20.176200	779.838491	11.936205
19.998882	783.534858	11.941210
20.065629	774.737733	11.946215
19.923995	779.620565	11.951219
19.984690	776.308956	11.956224
20.065425	778.240584	11.961229
20.172415	784.594460	11.966234
20.151545	782.081168	11.971239
20.241148	780.400221	11.976243
20.314209	790.276057	11.981248
20.575020	784.579753	11.986253
20.446389	794.317452	11.991258
20.752498	787.519535	11.996263
20.707685	801.638768	12.001267
20.675713	798.756665	12.006272
20.983336	787.210375	12.011277
20.836799	801.976603	12.016282
20.838608	803.165475	12.021287
20.952144	799.601008	12.026291
20.564649	813.557292	12.031296
20.768281	799.952337	12.036301
20.718856	802.642731	12.041306
20.992498	789.785122	12.046311
20.799530	785.268195	12.051315
20.842147	788.473754	12.056320
20.692982	769.159850	12.061325
20.640801	766.202131	12.066330
20.592274	769.986762	12.071335
20.764330	771.072785	12.076339
20.775035	775.972319	12.081344
20.937457	776.921110	12.086349
20.806198	773.449308	12.091354
20.983242	781.712705	12.096359
20.873802	777.106766	12.101363
20.790154	775.168028	12.106368
21.190395	771.860612	12.111373
20.636053	778.312076	12.116378
20.775131	782.705444	12.121383
20.934126	783.935475	12.126387
20.647630	784.837595	12.131392
20.834793	780.223773	12.136397
20.508972	779.317122	12.141402
20.688713	787.176399	12.146407
20.772192	787.407664	12.151411
20.612620	781.404677	12.156416
21.120378	771.129021	12.161421
21.095050	772.915142	12.166426
20.805026	784.072577	12.171431
20.864357	781.600110	12.176435
21.089380	778.560331	12.181440
20.964084	755.003860	12.186445
20.630389	748.837850	12.191450
20.513479	745.726459	12.196455
20.722293	754.965620	12.201459
20.504591	759.685539	12.206464
20.863586	763.618057	12.211469
20.532622	774.187513	12.216474
21.093631	777.770854	12.221479
20.854538	760.874539	12.226483
20.540422	750.829325	12.231488
20.892337	744.615468	12.236493
20.806949	752.679435	12.241498
20.712208	746.675584	12.246503
20.739858	744.318560	12.251507
20.653828	750.901898	12.256512
20.683959	744.785094	12.261517
20.347625	751.212815	12.266522
20.670510	748.464933	12.271527
20.569870	773.500625	12.276531
20.444656	781.744422	12.281536
20.411051	780.109933	12.286541
20.645437	793.577512	12.291546
20.663055	789.230421	12.296551
20.827356	778.738307	12.301555
21.116162	798.157994	12.306560
21.584001	778.379823	12.311565
20.955226	771.138094	12.316570
20.859196	752.353469	12.321575
20.747315	760.040050	12.326579
20.652120	753.496960	12.331584
20.776556	749.378845	12.336589
20.836329	751.148236	12.341594
20.849941	741.820298	12.346599
20.929920	752.265851	12.351603
20.772464	756.563006	12.356608
20.923469	747.798189	12.361613
20.846727	761.181322	12.366618
20.847367	755.545447	12.371623
20.719801	756.302371	12.376627
20.592114	765.836478	12.381632
20.684304	752.869072	12.386637
20.803014	752.515986	12.391642
20.739131	759.922104	12.396647
20.705535	753.362882	12.401651
20.815316	765.311231	12.406656
20.925533	753.269759	12.411661
20.804804	758.401557	12.416666
20.803526	764.268076	12.421671
20.763715	763.440387	12.426675
20.673521	755.459920	12.431680
21.047811	748.496608	12.436685
20.949062	770.666724	12.441690
20.810419	751.370088	12.446695
20.669210	747.013649	12.451699
20.656773	752.596520	12.456704
20.818951	750.232231	12.461709
20.775547	745.026001	12.466714
20.941194	736.176856	12.471719
20.966498	743.513549	12.476723
20.951550	739.395590	12.481728
21.105492	718.814448	12.486733
20.925268	734.279826	12.491738
20.795314	738.653012	12.496743
20.885007	735.608018	12.501747
20.646724	729.764260	12.506752
20.866217	722.824072	12.511757
20.851037	732.562558	12.516762
20.783867	731.442773	12.521767
20.933327	729.930477	12.526771
20.709966	734.627636	12.531776
20.703582	727.357625	12.536781
20.561279	729.569243	12.541786
20.936364	722.629470	12.546791
21.019414	729.649446	12.551795
20.624771	744.612880	12.556800
20.906336	730.801598	12.561805
20.817031	733.750647	12.566810
20.718314	733.771278	12.571815
20.744648	722.356632	12.576819
20.408878	724.247452	12.581824
20.873635	722.640716	12.586829
20.729461	742.422692	12.591834
20.584774	735.967927	12.596839
20.970030	736.945829	12.601843
20.703931	741.323384	12.606848
20.858370	724.898923	12.611853
20.336886	725.770710	12.616858
20.297425	729.325231	12.621863
20.797937	730.026135	12.626867
20.461462	737.895179	12.631872
20.714109	737.200616	12.636877
20.683106	743.902906	12.641882
20.797636	735.148645	12.646887
21.089040	728.531292	12.651891
20.521448	736.642196	12.656896
20.891072	742.886358	12.661901
20.931583	748.055513	12.666906
20.816248	735.192183	12.671911
20.730290	735.526163	12.676915
20.714308	737.886365	12.681920
21.153449	735.802752	12.686925
20.759287	724.253324	12.691930
20.587052	720.247187	12.696935
20.756618	710.370858	12.701939
20.240216	719.504893	12.706944
20.476537	726.356923	12.711949
20.483214	741.043461	12.716954
20.532302	741.811633	12.721959
21.001128	747.547975	12.726963
20.703311	744.730360	12.731968
20.973607	754.131599	12.736973
20.877721	748.634123	12.741978
20.749755	742.629265	12.746983
21.009954	742.772420	12.751987
20.670666	753.675921	12.756992
20.610328	743.432544	12.761997
20.755307	748.708038	12.767002
20.810855	750.739872	12.772007
20.588858	747.232087	12.777011
20.375017	751.013118	12.782016
20.831527	747.168463	12.787021
20.505281	764.096893	12.792026
20.629322	750.755409	12.797031
20.802896	751.995727	12.802035
20.735370	757.554270	12.807040
20.476786	750.546818	12.812045
20.776067	747.954086	12.817050
20.720496	757.500339	12.822055
21.017774	746.892423	12.827059
21.032353	754.517832	12.832064
20.939430	746.987228	12.837069
20.744668	755.011872	12.842074
20.516214	749.010423	12.847079
20.843487	748.207765	12.852083
20.581177	760.351070	12.857088
20.460977	767.136981	12.862093
20.525543	759.188599	12.867098
20.693502	752.974116	12.872103
20.770237	753.600687	12.877107
20.627727	768.404085	12.882112
20.919914	754.460202	12.887117
20.979639	756.302140	12.892122
21.004609	764.145089	12.897127
20.930911	744.675681	12.902131
20.552967	736.794734	12.907136
20.543974	729.793214	12.912141
20.545532	748.552188	12.917146
20.863574	750.685657	12.922151
21.120708	754.244918	12.927155
20.829180	745.580645	12.932160
20.721065	734.056549	12.937165
20.798196	732.853826	12.942170
20.238744	737.229283	12.947175
20.793863	733.772596	12.952179
20.995217	748.175785	12.957184
20.800001	733.559043	12.962189
20.507845	741.810520	12.967194
20.826156	726.347075	12.972199
21.091918	716.832283	12.977203
20.846589	724.119091	12.982208
20.951444	716.519114	12.987213
20.828052	728.141929	12.992218
20.563025	724.756128	12.997223
20.713650	721.477496	13.002227
20.433301	726.573241	13.007232
20.847897	728.525730	13.012237
20.671021	738.919202	13.017242
20.540901	731.266808	13.022247
21.056642	726.083368	13.027251
20.621417	747.283692	13.032256
20.596629	727.377583	13.037261
20.809034	728.720513	13.042266
20.525257	735.325921	13.047271
20.831811	724.170928	13.052275
20.809061	730.646395	13.057280
20.639578	731.064658	13.062285
20.508441	728.638347	13.067290
20.774375	727.457550	13.072295
20.790236	731.911555	13.077299
20.742384	744.496873	13.082304
20.697752	728.873696	13.087309
20.634027	731.129551	13.092314
20.539887	729.126261	13.097319
20.640460	728.012839	13.102323
20.630270	738.788148	13.107328
20.712441	733.632855	13.112333
20.677256	744.215039	13.117338
20.622069	751.950920	13.122343
21.116828	750.318895	13.127347
20.707021	744.056219	13.132352
20.605450	744.717535	13.137357
20.703046	739.520357	13.142362
20.510630	742.763392	13.147367
21.236538	733.473238	13.152371
20.841291	748.124541	13.157376
20.732144	733.252803	13.162381
20.887121	735.658277	13.167386
20.839305	735.910481	13.172391
20.879428	733.072085	13.177395
20.622517	746.857671	13.182400
20.410027	736.313720	13.187405
20.735123	743.720868	13.192410
20.918841	743.098798	13.197415
20.967848	732.940490	13.202419
20.555802	748.488587	13.207424
21.030217	731.021201	13.212429
21.239533	739.501773	13.217434
20.924612	741.725154	13.222439
21.070321	726.249815	13.227443
20.749705	740.785130	13.232448
20.996051	739.815611	13.237453
20.743424	739.744097	13.242458
20.639564	734.050782	13.247463
20.852798	725.542554	13.252467
20.661377	718.682097	13.257472
20.892769	720.725305	13.262477
20.776737	722.423386	13.267482
20.408228	721.121433	13.272487
20.767641	713.368896	13.277491
20.615911	736.003139	13.282496
20.759718	744.282854	13.287501
20.831623	739.947619	13.292506
21.036422	729.486928	13.297511
20.734604	715.540051	13.302515
20.507250	718.922691	13.307520
20.714970	713.857766	13.312525
20.586427	708.728205	13.317530
20.686058	731.142581	13.322535
21.042257	730.716926	13.327539
20.686481	723.627219	13.332544
20.796645	732.539908	13.337549
20.982309	710.550259	13.342554
20.773662	718.741096	13.347559
20.789696	713.110668	13.352563
20.440362	710.995121	13.357568
20.897172	718.974170	13.362573
20.922554	716.369936	13.367578
20.669174	723.577605	13.372583
20.729072	711.651424	13.377587
20.776946	725.309532	13.382592
20.950732	717.633906	13.387597
20.871621	708.822238	13.392602
20.939249	717.107780	13.397607
20.617555	725.911150	13.402611
20.472508	726.141015	13.407616
20.731039	715.304341	13.412621
20.846625	718.457247	13.417626
20.713580	729.971219	13.422631
21.088217	716.342222	13.427635
20.579898	723.051245	13.432640
20.806962	721.827764	13.437645
20.578253	719.896400	13.442650
20.733375	718.398971	13.447655
20.945062	709.779038	13.452659
20.844631	728.357136	13.457664
20.849191	706.960915	13.462669
20.910781	723.166712	13.467674
20.626456	719.552182	13.472679
20.837526	709.410619	13.477683
20.679558	727.991587	13.482688
20.687601	723.417389	13.487693
20.780625	725.148358	13.492698
20.840578	720.504382	13.497703
20.959652	720.829315	13.502707
20.673913	721.811733	13.507712
20.906054	723.947861	13.512717
20.778421	726.034138	13.517722
20.775287	723.661528	13.522727
21.062421	711.233913	13.527731
20.504336	707.396549	13.532736
20.635625	694.123345	13.537741
20.665093	696.380100	13.542746
20.740309	709.128682	13.547751
20.791882	691.399207	13.552755
20.753523	710.473573	13.557760
20.882515	710.503617	13.562765
20.492437	706.275190	13.567770
20.507576	702.001059	13.572775
20.777044	711.427633	13.577779
20.847873	725.913117	13.582784
20.483350	722.254608	13.587789
20.798842	723.339828	13.592794
20.658268	724.160325	13.597799
21.124398	719.246568	13.602803
20.863499	703.467104	13.607808
20.675753	694.723232	13.612813
20.968959	687.829650	13.617818
20.554757	679.632825	13.622823
20.513683	689.313913	13.627827
20.626301	695.736236	13.632832
20.587628	700.552158	13.637837
20.927113	705.804499	13.642842
20.565239	709.183361	13.647847
20.826291	712.943832	13.652851
20.414459	707.296494	13.657856
20.843128	718.621522	13.662861
21.041495	715.448815	13.667866
20.804349	720.160784	13.672871
20.831913	699.516249	13.677875
20.822395	701.905376	13.682880
20.634584	693.259284	13.687885
20.953934	700.777711	13.692890
20.759271	702.513561	13.697895
21.084662	684.918615	13.702899
20.852225	702.141086	13.707904
20.767343	702.072779	13.712909
20.989690	688.351405	13.717914
20.590302	701.912096	13.722919
20.769727	699.198143	13.727923
20.799924	701.577782	13.732928
20.643812	696.471545	13.737933
20.407029	695.724160	13.742938
20.604672	698.558052	13.747943
20.549991	692.022721	13.752947
20.301415	700.547915	13.757952
20.211694	704.127792	13.762957
20.866146	711.012472	13.767962
20.682588	714.340818	13.772967
20.666434	718.189657	13.777971
20.598672	724.106186	13.782976
20.671194	723.747852	13.787981
20.729449	730.271899	13.792986
20.987441	736.213748	13.797991
21.197419	715.450212	13.802995
20.757052	711.288150	13.808000
20.779459	702.141757	13.813005
20.709872	702.228703	13.818010
20.466788	709.798991	13.823015
20.745607	696.462833	13.828019
20.857430	697.949533	13.833024
20.331468	700.695412	13.838029
20.468070	707.612221	13.843034
20.695541	724.190522	13.848039
20.920566	726.056554	13.853043
20.885396	724.337167	13.858048
20.703881	712.291797	13.863053
21.032509	705.753671	13.868058
21.021277	704.599736	13.873063
20.946470	705.228397	13.878067
20.820996	705.270641	13.883072
20.979295	703.872053	13.888077
20.789589	696.869411	13.893082
20.619384	704.521111	13.898087
21.120630	695.515966	13.903091
20.712496	710.047863	13.908096
20.882715	713.915860	13.913101
20.989856	712.675238	13.918106
20.812472	710.331998	13.923111
20.844893	710.568250	13.928115
20.519464	705.386515	13.933120
20.874407	703.177566	13.938125
21.245149	697.906877	13.943130
20.503323	694.972435	13.948135
20.694547	691.572219	13.953139
20.694705	698.946015	13.958144
20.656772	697.730109	13.963149
20.822743	695.756300	13.968154
20.946688	694.837844	13.973159
20.763854	686.019079	13.978163
20.576996	677.156807	13.983168
20.481025	673.017097	13.988173
20.607059	695.947590	13.993178
20.501218	707.990204	13.998183
20.788498	699.022337	14.003187
20.624641	706.881179	14.008192
20.820196	715.254549	14.013210
20.731056	710.951320	14.018227
20.814691	710.629849	14.023245
20.770725	706.464123	14.028263
20.616013	719.457487	14.033280
20.672399	715.107453	14.038298
20.510291	702.566023	14.043315
20.787600	716.199856	14.048333
20.821687	702.771478	14.053351
20.590427	706.827266	14.058368
20.662194	714.688322	14.063386
20.829558	709.976126	14.068403
20.582282	705.229397	14.073421
20.614157	712.299356	14.078439
20.595820	724.413744	14.083456
20.461286	750.924554	14.088474
20.788879	737.358104	14.093491
20.748396	753.634796	14.098509
20.985123	735.680291	14.103527
21.078966	751.734225	14.108544
20.822122	739.440662	14.113562
20.794751	745.647127	14.118579
20.663356	746.580521	14.123597
20.824410	751.427836	14.128615
21.140537	757.686478	14.133632
21.209382	769.975748	14.138650
21.347300	768.239443	14.143667
21.215436	784.579504	14.148685
21.372800	777.872865	14.153703
21.182309	766.693322	14.158720
21.026791	783.356453	14.163738
21.211222	777.279378	14.168755
21.399808	785.727408	14.173773
21.410687	774.394629	14.178791
21.499579	773.457313	14.183808
21.217052	779.254637	14.188826
21.686866	775.554319	14.193843
21.532696	774.251532	14.198861
21.368388	763.816518	14.203879
21.410694	756.307185	14.208896
21.246274	760.737688	14.213914
21.642942	779.684682	14.218931
21.469627	777.998015	14.223949
21.478371	778.473366	14.228967
21.689871	774.248001	14.233984
21.045779	764.504512	14.239002
21.511213	778.460730	14.244019
21.659987	782.320657	14.249037
21.583048	781.574944	14.254055
21.774388	779.726305	14.259072
21.593873	780.374976	14.264090
21.900959	784.412559	14.269107
21.651712	785.100504	14.274125
21.737048	777.302747	14.279143
21.935061	782.490216	14.284160
21.525052	768.341436	14.289178
21.796722	763.579556	14.294195
21.505887	778.290271	14.299213
21.882520	773.705113	14.304231
22.150561	765.870358	14.309248
21.471660	780.694875	14.314266
21.790756	780.007111	14.319283
21.489666	788.210797	14.324301
21.685294	782.314391	14.329319
21.785418	787.629151	14.334336
21.916499	788.902900	14.339354
21.793825	782.744252	14.344371
21.675244	789.981380	14.349389
21.619092	781.009206	14.354407
21.713558	775.300384	14.359424
21.671482	786.641597	14.364442
21.628188	787.581390	14.369459
21.768330	798.396511	14.374477
21.877623	816.761798	14.379495
22.109734	818.050896	14.384512
22.146513	820.140299	14.389530
22.256282	812.064941	14.394547
22.105260	829.262196	14.399565
22.218467	817.203680	14.404583
22.300109	817.453490	14.409600
22.221156	816.083652	14.414618
22.242537	820.682727	14.419635
22.132366	821.299732	14.424653
22.285025	811.926175	14.429671
22.430670	814.404024	14.434688
22.352113	828.357396	14.439706
22.512680	818.023100	14.444723
22.546934	808.017246	14.449741
22.247324	804.178535	14.454759
22.662345	785.523901	14.459776
22.207843	781.222298	14.464794
22.313538	771.972653	14.469811
21.889207	794.218435	14.474829
22.323046	811.959416	14.479847
22.336842	814.579408	14.484864
22.524834	814.132760	14.489882
22.631591	819.194809	14.494899
22.683080	828.389841	14.499917
22.581996	816.461451	14.504935
22.890777	819.160229	14.509952
22.712834	820.807287	14.514970
22.659795	800.995698	14.519987
22.687082	803.994180	14.525005
22.363206	805.079390	14.530023
22.838640	805.115395	14.535040
22.528148	817.764058	14.540058
22.682289	820.841405	14.545075
22.675424	826.596355	14.550093
22.584512	820.077148	14.555111
22.672686	819.004673	14.560128
22.606869	825.899946	14.565146
22.814068	820.846331	14.570163
22.902447	817.013370	14.575181
22.800246	825.149179	14.580199
22.891886	816.373619	14.585216
22.965473	825.154596	14.590234
23.160367	813.026431	14.595251
23.038614	815.268524	14.600269
22.742217	818.807808	14.605287
22.955247	818.390197	14.610304
22.915540	816.344041	14.615322
23.009724	808.614064	14.620339
23.097813	812.568615	14.625357
22.616783	827.638452	14.630375
22.964380	810.716875	14.635392
22.671805	824.385076	14.640410
22.798553	826.103081	14.645427
22.860602	813.173472	14.650445
22.717490	819.610771	14.655463
22.966637	818.358478	14.660480
22.619457	822.909377	14.665498
23.116015	835.031393	14.670515
23.536344	845.079897	14.675533
23.524328	840.268863	14.680551
23.521364	830.316117	14.685568
23.277857	817.402207	14.690586
23.229639	814.780151	14.695603
23.375569	813.152666	14.700621
23.055595	818.120764	14.705639
23.447524	818.536575	14.710656
23.485114	824.295444	14.715674
23.560537	809.474642	14.720691
23.387553	809.732032	14.725709
23.353286	816.589238	14.730727
23.445329	809.653920	14.735744
23.167278	814.788351	14.740762
23.557405	827.732664	14.745779
23.542815	839.069534	14.750797
23.325741	848.566942	14.755815
23.799299	833.080193	14.760832
23.658268	851.057616	14.765850
23.479708	842.617697	14.770867
23.494639	838.618705	14.775885
23.551410	848.383874	14.780903
23.787658	845.858005	14.785920
23.697097	858.402419	14.790938
23.752704	838.087421	14.795955
23.752849	844.245498	14.800973
23.447827	853.500552	14.805991
24.041854	847.770224	14.811008
23.665374	848.944045	14.816026
23.866035	841.550974	14.821043
23.769415	843.678958	14.826061
23.844325	835.760146	14.831079
23.817666	854.359507	14.836096
23.683742	845.648217	14.841114
23.895532	842.213961	14.846131
24.149057	838.007042	14.851149
23.913327	841.476885	14.856167
23.988496	845.413058	14.861184
24.172481	844.915142	14.866202
24.152896	839.325151	14.871219
24.414387	842.644911	14.876237
23.989830	834.604427	14.881255
23.942455	813.558755	14.886272
23.911282	832.874482	14.891290
24.081301	841.290902	14.896307
24.164018	841.137876	14.901325
24.170939	848.049871	14.906343
24.184681	854.425992	14.911360
24.315386	848.925277	14.916378
24.257090	839.527150	14.921395
24.182662	845.997548	14.926413
23.790624	837.676616	14.931431
24.458491	837.642607	14.936448
24.459389	841.434906	14.941466
24.275964	842.812301	14.946483
24.461155	840.489616	14.951501
24.123754	854.710796	14.956519
24.072997	846.137241	14.961536
24.402388	840.883246	14.966554
24.435255	844.000387	14.971571
24.414825	840.916178	14.976589
24.311111	839.094142	14.981607
24.324237	840.279751	14.986624
24.519906	840.453178	14.991642
24.101999	840.707162	14.996659
24.711133	840.259408	15.001677
24.248022	834.295023	15.006695
24.402371	840.735222	15.011712
24.608429	832.515517	15.016730
24.643868	842.759103	15.021747
24.811674	831.259688	15.026765
24.516027	845.903604	15.031783
24.698178	833.489612	15.036800
24.642452	837.342847	15.041818
24.212937	834.364779	15.046835
24.621481	858.599680	15.051853
24.696082	881.767967	15.056871
24.959222	872.792000	15.061888
25.218614	871.947026	15.066906
24.845086	880.890576	15.071923
24.916914	869.068263	15.076941
24.909954	881.091312	15.081959
25.125074	866.490401	15.086976
25.112564	878.349177	15.091994
24.990421	870.158201	15.097011
25.329839	842.365916	15.102029
24.893603	847.118203	15.107047
24.748303	838.495242	15.112064
24.694126	851.024409	15.117082
24.778529	855.665350	15.122099
25.184158	862.276252	15.127117
25.186385	873.851123	15.132135
25.308701	861.467098	15.137152
25.267908	869.638752	15.142170
24.896840	871.181347	15.147187
25.071442	878.779143	15.152205
24.770942	875.055376	15.157223
24.895039	862.420973	15.162240
25.191828	866.150358	15.167258
25.384997	871.337059	15.172275
25.188108	864.943265	15.177293
24.993286	870.116347	15.182311
24.999229	862.589164	15.187328
25.135744	875.231074	15.192346
25.242339	889.115652	15.197363
25.382311	885.496225	15.202381
25.431245	883.866901	15.207399
25.290003	889.915422	15.212416
25.355879	893.234935	15.217434
25.340118	895.323291	15.222451
25.767862	888.024531	15.227469
25.318147	891.151014	15.232487
25.554525	898.230916	15.237504
25.909367	880.140999	15.242522
25.573666	897.904153	15.247539
25.479557	888.878196	15.252557
25.633252	886.513340	15.257575
25.522313	885.839106	15.262592
25.751029	891.056323	15.267610
25.792455	891.005830	15.272627
26.146538	885.088829	15.277645
25.982458	890.220838	15.282663
25.860307	888.162653	15.287680
25.805096	885.112294	15.292698
25.865212	902.057325	15.297715
25.991690	879.694038	15.302733
25.772446	892.472921	15.307751
25.755058	893.351965	15.312768
25.985604	885.999719	15.317786
25.731925	890.939966	15.322803
26.138651	883.644560	15.327821
26.216148	892.627860	15.332839
26.140396	882.732302	15.337856
26.325202	884.669127	15.342874
26.199047	880.105929	15.347891
26.317917	886.414963	15.352909
26.294181	895.686525	15.357927
26.196286	893.621326	15.362944
26.135283	893.220679	15.367962
26.156397	893.325999	15.372979
26.336393	893.978520	15.377997
26.101614	889.879351	15.383015
25.988522	890.017085	15.388032
26.333439	883.291495	15.393050
26.076715	897.745224	15.398067
26.371863	885.593145	15.403085
26.375195	885.696581	15.408103
26.279929	894.342520	15.413120
26.369596	889.785793	15.418138
26.328283	890.171610	15.423155
26.456002	891.647239	15.428173
26.164155	893.180347	15.433191
26.276106	895.276647	15.438208
26.540841	885.112866	15.443226
26.347733	890.136255	15.448243
26.459766	894.557311	15.453261
26.574923	885.672574	15.458279
26.430693	903.595521	15.463296
26.254297	885.746042	15.468314
26.106284	906.950698	15.473331
26.839392	908.516953	15.478349
27.019031	919.509898	15.483367
26.889299	915.464749	15.488384
26.853130	915.404611	15.493402
26.707390	909.894484	15.498419
26.681945	926.655003	15.503437
26.965223	919.017496	15.508455
26.836972	924.975877	15.513472
27.102226	906.680006	15.518490
26.818387	916.897493	15.523507
26.945477	904.630639	15.528525
27.079297	921.359459	15.533543
26.866512	924.349067	15.538560
27.152573	918.619069	15.543578
26.837979	930.120254	15.548595
26.978153	931.096857	15.553613
27.098829	922.423561	15.558631
26.909133	918.600319	15.563648
27.443047	926.812471	15.568666
27.236596	933.678319	15.573683
27.224180	917.224569	15.578701
27.352044	925.830221	15.583719
27.358381	909.132832	15.588736
27.112526	894.868090	15.593754
27.053233	897.999941	15.598771
26.983866	912.721085	15.603789
27.171480	909.182138	15.608807
27.115445	918.400668	15.613824
27.064508	918.671625	15.618842
26.979874	911.207623	15.623859
27.011369	926.203684	15.628877
27.315933	916.934812	15.633895
27.341833	924.487141	15.638912
27.291657	916.254775	15.643930
27.393539	928.710360	15.648947
27.357491	937.040160	15.653965
27.458824	944.202967	15.658983
27.678998	943.994986	15.664000
27.789310	947.353039	15.669018
27.889848	945.921530	15.674035
27.645006	933.794189	15.679053
27.689332	937.922483	15.684071
27.525356	940.445017	15.689088
27.774304	935.834560	15.694106
27.751430	940.126146	15.699123
27.737369	935.963449	15.704141
27.687462	943.244752	15.709159
27.677901	954.310368	15.714176
27.363829	941.747352	15.719194
27.514660	947.398553	15.724211
27.771148	948.510754	15.729229
27.874489	936.708526	15.734247
27.697253	950.748535	15.739264
27.991876	934.499037	15.744282
27.766354	954.336673	15.749299
27.630025	941.913611	15.754317
27.785529	947.834610	15.759335
27.897255	952.722891	15.764352
28.283116	963.579167	15.769370
28.244969	964.065148	15.774387
28.008603	962.364921	15.779405
28.237766	962.012370	15.784423
28.391955	973.600834	15.789440
28.423948	957.223320	15.794458
28.325676	943.479224	15.799475
27.966571	941.579938	15.804493
28.282443	943.351159	15.809511
28.404635	969.126192	15.814528
28.471602	956.098150	15.819546
28.300742	945.778871	15.824563
28.297462	955.899733	15.829581
28.621774	949.782975	15.834599
28.355707	958.789652	15.839616
28.294222	964.017001	15.844634
28.657320	964.047331	15.849651
28.302923	983.183588	15.854669
28.880375	968.304577	15.859687
28.770655	975.578134	15.864704
28.526809	948.465371	15.869722
28.395095	955.995666	15.874739
28.299150	973.017578	15.879757
28.678652	966.564842	15.884775
28.466283	978.719827	15.889792
28.905049	964.534578	15.894810
28.950086	974.935592	15.899827
28.626099	982.288940	15.904845
28.855645	976.457827	15.909863
28.967848	978.176598	15.914880
29.093297	962.274926	15.919898
29.044089	977.069993	15.924915
28.662864	976.839958	15.929933
28.895015	974.410669	15.934951
28.691137	970.026568	15.939968
28.798658	977.613095	15.944986
29.043775	969.012727	15.950003
28.976966	974.958183	15.955021
28.965160	971.051503	15.960039
28.635714	969.529703	15.965056
28.512886	974.618985	15.970074
29.351123	966.340848	15.975091
28.909322	980.729801	15.980109
29.295277	955.929447	15.985127
29.038282	965.884728	15.990144
29.007172	966.732932	15.995162
29.100975	986.530694	16.000179
29.017635	997.927414	16.005197
29.334757	990.459068	16.010215
29.391530	1000.225912	16.015232
29.386124	991.522350	16.020250
29.378654	996.969170	16.025267
29.525505	998.857012	16.030285
29.858625	996.545315	16.035303
29.485079	1004.273070	16.040320
29.514894	1004.669567	16.045338
29.606959	994.033058	16.050355
29.523674	1011.468248	16.055373
29.621817	991.622848	16.060391
29.549995	1005.163209	16.065408
29.460856	991.051118	16.070426
29.880032	994.303296	16.075443
29.773934	999.762703	16.080461
29.783531	986.699741	16.085479
29.763334	994.283052	16.090496
29.847445	995.698011	16.095514
29.779701	999.384902	16.100531
29.614749	996.034290	16.105549
29.785456	993.621089	16.110567
29.780494	1000.166988	16.115584
29.596914	999.318728	16.120602
29.940151	1001.277489	16.125619
29.522683	989.817814	16.130637
29.769893	992.745083	16.135655
29.763784	997.354890	16.140672
29.475902	1006.341482	16.145690
30.025418	1003.177349	16.150707
29.932760	1013.992011	16.155725
30.069832	1020.899060	16.160743
30.484526	1019.922351	16.165760
30.472393	1015.287444	16.170778
30.453749	998.471248	16.175795
30.152373	993.607217	16.180813
30.429797	991.175424	16.185831
30.040843	989.177079	16.190848
30.076308	1001.833643	16.195866
30.465243	982.320953	16.200883
30.122796	1001.716435	16.205901
30.567738	1003.901207	16.210919
30.247103	1008.620951	16.215936
30.142605	1012.879963	16.220954
30.943882	1020.198573	16.225971
30.562314	1027.828525	16.230989
30.680415	1009.589026	16.236007
30.540315	999.201886	16.241024
30.367311	993.351604	16.246042
30.634548	1003.905952	16.251059
30.500833	1013.239172	16.256077
30.438986	1023.913655	16.261095
30.771471	1018.893470	16.266112
31.070377	1026.784533	16.271130
30.847526	1026.644063	16.276147
30.678504	1015.984688	16.281165
31.055486	1014.584583	16.286183
30.747660	996.219560	16.291200
30.449951	1009.069259	16.296218
30.765377	1013.973834	16.301235
30.759165	1026.089687	16.306253
31.038424	1024.554167	16.311271
30.838193	1028.111194	16.316288
30.989505	1020.791966	16.321306
30.954244	1013.230380	16.326323
31.007625	1037.935908	16.331341
31.104495	1022.469712	16.336359
31.412471	1017.843522	16.341376
30.883643	1024.454106	16.346394
31.219008	1019.971404	16.351411
31.223667	1033.987203	16.356429
31.043440	1015.807858	16.361447
30.991988	1032.778702	16.366464
30.826318	1026.837579	16.371482
31.079511	1030.501606	16.376499
30.925963	1025.791728	16.381517
30.849855	1037.251816	16.386535
31.400961	1046.384607	16.391552
31.237670	1051.536994	16.396570
31.767179	1050.526242	16.401587
31.351374	1053.685100	16.406605
31.258266	1063.957209	16.411623
31.412304	1063.531699	16.416640
31.093564	1054.352712	16.421658
31.668358	1045.968691	16.426675
31.563781	1054.020068	16.431693
31.481601	1055.082477	16.436711
31.724524	1047.363256	16.441728
31.170450	1056.703774	16.446746
31.459348	1055.264235	16.451763
31.670783	1057.284921	16.456781
31.679214	1072.932861	16.461799
32.260771	1080.027011	16.466816
31.845178	1058.366492	16.471834
32.037535	1056.225092	16.476851
31.999244	1047.130361	16.481869
32.009523	1046.505996	16.486887
32.258232	1043.495216	16.491904
31.830975	1046.855661	16.496922
31.898424	1045.347627	16.501939
32.064117	1044.412202	16.506957
32.327808	1044.422209	16.511975
32.150298	1058.868183	16.516992
31.937889	1049.028910	16.522010
32.111308	1040.060858	16.527027
31.853499	1052.466956	16.532045
31.902506	1053.181273	16.537063
32.016307	1064.729064	16.542080
32.376666	1076.273719	16.547098
32.502687	1071.756752	16.552115
32.590269	1078.939122	16.557133
32.348836	1078.779593	16.562151
32.556515	1071.795822	16.567168
32.383414	1083.235237	16.572186
32.794629	1063.045669	16.577203
32.498569	1058.691972	16.582221
32.445590	1052.253121	16.587239
32.146094	1051.882642	16.592256
32.523752	1069.061927	16.597274
33.027375	1077.884578	16.602291
32.664244	1064.920314	16.607309
32.193354	1068.249973	16.612327
32.709909	1077.073707	16.617344
32.507066	1087.034590	16.622362
32.576483	1084.994586	16.627379
32.444660	1084.109754	16.632397
32.346435	1081.310018	16.637415
33.053214	1082.400748	16.642432
32.902546	1078.223620	16.647450
32.457763	1081.190488	16.652467
32.710021	1078.926280	16.657485
32.805022	1076.092582	16.662503
33.044005	1085.369553	16.667520
32.707594	1074.788738	16.672538
33.277713	1093.095038	16.677555
33.279761	1097.593470	16.682573
33.227112	1088.205291	16.687591
33.098392	1075.269696	16.692608
33.148175	1082.156092	16.697626
32.873375	1076.210333	16.702643
32.762341	1087.919836	16.707661
33.125888	1098.311037	16.712679
33.091670	1102.640658	16.717696
33.319791	1103.880085	16.722714
33.614852	1105.357361	16.727731
33.520271	1106.833861	16.732749
33.312543	1108.271782	16.737767
33.610346	1099.469462	16.742784
33.540036	1100.916924	16.747802
33.937254	1098.264672	16.752819
33.856192	1100.081917	16.757837
33.795157	1096.049354	16.762855
33.724711	1083.006936	16.767872
33.710631	1077.645624	16.772890
33.603486	1082.236967	16.777907
33.425236	1065.957351	16.782925
33.319552	1080.583790	16.787943
33.964847	1085.426343	16.792960
34.140154	1104.223463	16.797978
33.947130	1079.705563	16.802995
33.864877	1080.876518	16.808013
33.767452	1070.740482	16.813031
33.887252	1069.527673	16.818048
33.772444	1080.830382	16.823066
33.902154	1084.199529	16.828083
33.919514	1077.746303	16.833101
33.630632	1096.807770	16.838119
33.822138	1095.959455	16.843136
33.863441	1100.997438	16.848154
33.630006	1108.314386	16.853171
33.626284	1095.833864	16.858189
33.706582	1098.130287	16.863207
33.976141	1105.176687	16.868224
34.216345	1123.631592	16.873242
34.275911	1123.044978	16.878259
34.579124	1124.421860	16.883277
34.169797	1133.674851	16.888295
34.243650	1121.241708	16.893312
34.333886	1128.077632	16.898330
34.606167	1121.203078	16.903347
34.589895	1124.063863	16.908365
34.683683	1129.194152	16.913383
35.075724	1107.444076	16.918400
34.561405	1106.747653	16.923418
34.723369	1100.442805	16.928435
34.842584	1090.319392	16.933453
34.525300	1098.519543	16.938471
34.870168	1089.450188	16.943488
34.748406	1097.814200	16.948506
34.622364	1086.941862	16.953523
34.538672	1093.967522	16.958541
34.511090	1098.041267	16.963559
34.809738	1095.311933	16.968576
34.772009	1123.333735	16.973594
34.956734	1124.188423	16.978611
35.256216	1120.195879	16.983629
34.905896	1115.981371	16.988647
34.847442	1105.588998	16.993664
34.640926	1114.985801	16.998682
34.671076	1135.698360	17.003699
34.677901	1126.835471	17.008717
34.637737	1127.925789	17.013735
34.617285	1123.646087	17.018752
34.874819	1130.541842	17.023770
35.044515	1143.144090	17.028787
35.399507	1154.258678	17.033805
35.566319	1152.859049	17.038823
35.733930	1151.473449	17.043840
35.627334	1139.308156	17.048858
35.246255	1133.928280	17.053875
35.408927	1127.777455	17.058893
35.255071	1129.650355	17.063911
35.489732	1122.210823	17.068928
35.603629	1120.146417	17.073946
35.269027	1123.960839	17.078963
35.619605	1131.966409	17.083981
35.370476	1131.210388	17.088999
35.532424	1150.653033	17.094016
35.434445	1147.478884	17.099034
35.224909	1163.899396	17.104051
35.582187	1148.278282	17.109069
35.355763	1163.340890	17.114087
35.892502	1144.051364	17.119104
35.816015	1153.631936	17.124122
35.808793	1157.477521	17.129139
36.258171	1139.498040	17.134157
35.878672	1153.768694	17.139175
35.890470	1150.844437	17.144192
35.962648	1148.297495	17.149210
35.686520	1152.928395	17.154227
36.052357	1152.513146	17.159245
35.812666	1155.829546	17.164263
36.096736	1145.796200	17.169280
35.853289	1149.902815	17.174298
35.787409	1171.583945	17.179315
36.268717	1172.591099	17.184333
36.361024	1177.517159	17.189351
36.250990	1181.583630	17.194368
36.564194	1172.728476	17.199386
36.443202	1177.473060	17.204403
36.445951	1177.235262	17.209421
36.655916	1176.596347	17.214439
36.638180	1171.875772	17.219456
36.785008	1165.236699	17.224474
36.157848	1156.673095	17.229491
36.523121	1162.013342	17.234509
36.442743	1162.790768	17.239527
36.840201	1165.912750	17.244544
37.030399	1167.052844	17.249562
36.640296	1169.215098	17.254579
36.940513	1162.889746	17.259597
36.532487	1159.137438	17.264615
36.772405	1159.660871	17.269632
36.958847	1162.816507	17.274650
36.930081	1166.234542	17.279667
37.114615	1158.807704	17.284685
36.792366	1153.699995	17.289703
37.047803	1156.430941	17.294720
37.144752	1165.348391	17.299738
36.789711	1158.481064	17.304755
37.074084	1157.789386	17.309773
37.053251	1166.335531	17.314791
37.162814	1165.939133	17.319808
36.999990	1166.698249	17.324826
36.699961	1174.469422	17.329843
37.111848	1166.753076	17.334861
36.870918	1169.493978	17.339879
36.992946	1172.258787	17.344896
36.709540	1169.540475	17.349914
36.864435	1177.624467	17.354931
37.529702	1179.181128	17.359949
37.692663	1197.093196	17.364967
37.585490	1198.047922	17.369984
37.604162	1188.382474	17.375002
37.202504	1183.553247	17.380019
37.632419	1177.921322	17.385037
37.569128	1196.902900	17.390055
37.740055	1185.597754	17.395072
37.945904	1191.197808	17.400090
37.700522	1190.883184	17.405107
38.139148	1178.179468	17.410125
37.715884	1182.810248	17.415143
37.541304	1169.534261	17.420160
37.707941	1167.179880	17.425178
37.470865	1192.251303	17.430195
37.536217	1187.799030	17.435213
37.827929	1196.814419	17.440231
37.545124	1191.958369	17.445248
37.968499	1183.988511	17.450266
37.934881	1183.732918	17.455283
38.236647	1190.988145	17.460301
38.212480	1187.437292	17.465319
38.007008	1190.345567	17.470336
38.238927	1165.020463	17.475354
38.188799	1182.430123	17.480371
38.245131	1184.297821	17.485389
38.152797	1176.241909	17.490407
37.893241	1187.602391	17.495424
38.350210	1199.776647	17.500442
38.502428	1200.896061	17.505459
38.754120	1209.307536	17.510477
38.818095	1199.593960	17.515495
38.435358	1194.263086	17.520512
38.629943	1175.286050	17.525530
38.392503	1178.858486	17.530547
38.957332	1201.543282	17.535565
38.752387	1192.626041	17.540583
38.678801	1180.661506	17.545600
38.870587	1179.399456	17.550618
38.612213	1175.494294	17.555635
38.986038	1183.810775	17.560653
38.899282	1179.551068	17.565671
38.678232	1179.113021	17.570688
38.971910	1185.152074	17.575706
38.863730	1199.879699	17.580723
39.055736	1216.657782	17.585741
39.212629	1208.245941	17.590759
39.130220	1194.948939	17.595776
39.335098	1194.674185	17.600794
38.943509	1180.706094	17.605811
39.015868	1185.237383	17.610829
39.284258	1209.993854	17.615847
39.179630	1210.765712	17.620864
39.353023	1200.625717	17.625882
39.077197	1207.238502	17.630899
39.069947	1202.552423	17.635917
39.333096	1207.080030	17.640935
39.004248	1209.510933	17.645952
39.253746	1210.223168	17.650970
39.091360	1205.415545	17.655987
39.158331	1208.311832	17.661005
39.441380	1201.061161	17.666023
38.957370	1214.434658	17.671040
39.537202	1231.539425	17.676058
39.610955	1237.634023	17.681075
39.499196	1234.510814	17.686093
39.479970	1232.046072	17.691111
39.618272	1242.004562	17.696128
39.874858	1229.529599	17.701146
39.511457	1241.441488	17.706163
39.739850	1233.711902	17.711181
39.862904	1236.150959	17.716199
39.440690	1240.408799	17.721216
39.988301	1230.393138	17.726234
39.960276	1237.586159	17.731251
40.143901	1247.468214	17.736269
40.856125	1250.170371	17.741287
40.476832	1245.735512	17.746304
40.668886	1226.923973	17.751322
40.213113	1234.252849	17.756339
40.566887	1222.737623	17.761357
40.636789	1228.543408	17.766375
40.090553	1232.077019	17.771392
40.577611	1219.496098	17.776410
40.779831	1226.926088	17.781427
40.397964	1228.843229	17.786445
40.669466	1217.042267	17.791463
40.651708	1223.377959	17.796480
40.941345	1222.073561	17.801498
40.779080	1230.552641	17.806515
40.707028	1215.036105	17.811533
40.748696	1215.850696	17.816551
40.538108	1216.703944	17.821568
40.753903	1215.815571	17.826586
40.799861	1228.503693	17.831603
40.495284	1222.328251	17.836621
40.845380	1221.284758	17.841639
40.387059	1231.250307	17.846656
40.630086	1217.272200	17.851674
40.902951	1232.805786	17.856691
40.684212	1220.287093	17.861709
41.035468	1221.160843	17.866727
40.352661	1224.612418	17.871744
40.878010	1231.183952	17.876762
41.000911	1244.880663	17.881779
41.063539	1254.358895	17.886797
41.575634	1257.744175	17.891815
41.278435	1253.862485	17.896832
41.356666	1250.723129	17.901850
41.463687	1249.284265	17.906867
41.301469	1251.567482	17.911885
41.605863	1246.279579	17.916903
41.150647	1262.560068	17.921920
41.237226	1252.896331	17.926938
41.470367	1249.000846	17.931955
41.309559	1252.822188	17.936973
41.210120	1242.054025	17.941991
41.517840	1241.525353	17.947008
41.502474	1247.911008	17.952026
41.694171	1245.565202	17.957043
42.044169	1248.350295	17.962061
42.275604	1239.692178	17.967079
41.824690	1256.800921	17.972096
42.229252	1251.632315	17.977114
42.023341	1249.071507	17.982131
41.817451	1251.378991	17.987149
41.818044	1244.607481	17.992167
41.838040	1247.635531	17.997184
41.668945	1243.189172	18.002202
41.668788	1251.028959	18.007219
41.828292	1257.039107	18.012237
42.183362	1259.489926	18.017255
42.309671	1274.148771	18.022272
42.155279	1262.123126	18.027290
42.343906	1257.080188	18.032307
42.351141	1269.643966	18.037325
42.368265	1265.999995	18.042343
42.386238	1262.294544	18.047360
42.307586	1255.551397	18.052378
42.524537	1261.489467	18.057395
42.259907	1254.802721	18.062413
42.591588	1258.396090	18.067431
42.368000	1263.018645	18.072448
42.083010	1267.581783	18.077466
42.475750	1272.977465	18.082483
42.655360	1286.498438	18.087501
42.793816	1281.529557	18.092519
42.822570	1293.336477	18.097536
43.155057	1281.009807	18.102554
43.486574	1283.629548	18.107571
43.099262	1286.434713	18.112589
43.607383	1270.130342	18.117607
42.949985	1260.785017	18.122624
43.145765	1248.580846	18.127642
43.024756	1242.319493	18.132659
42.942716	1257.857799	18.137677
43.415619	1260.615428	18.142695
43.150671	1285.030815	18.147712
43.290949	1273.626673	18.152730
43.061719	1283.121584	18.157747
43.271818	1278.621031	18.162765
43.443681	1283.056260	18.167783
43.233537	1283.231496	18.172800
43.459787	1275.082250	18.177818
43.428455	1282.385929	18.182835
43.271919	1288.304926	18.187853
43.517434	1271.790761	18.192871
43.333500	1282.475468	18.197888
43.743044	1272.215968	18.202906
43.522249	1279.952538	18.207923
43.553436	1286.848289	18.212941
43.798187	1280.067711	18.217959
43.517886	1272.622143	18.222976
43.975934	1285.640980	18.227994
43.900191	1275.713691	18.233011
43.702133	1278.399013	18.238029
43.635067	1290.848823	18.243047
43.832885	1286.583024	18.248064
43.971510	1308.307246	18.253082
44.232428	1313.779020	18.258099
43.935357	1314.592586	18.263117
44.485129	1305.005948	18.268135
44.136029	1312.380768	18.273152
44.083687	1306.194949	18.278170
44.331021	1301.625532	18.283187
44.266058	1303.537757	18.288205
44.215514	1304.428405	18.293223
44.344471	1302.828741	18.298240
44.406588	1297.159478	18.303258
44.593658	1292.031837	18.308275
44.329721	1303.887017	18.313293
44.223239	1303.786182	18.318311
44.655038	1325.956012	18.323328
44.468184	1337.388383	18.328346
45.082438	1319.523952	18.333363
44.984216	1332.631546	18.338381
45.266540	1314.247500	18.343399
45.257778	1306.952084	18.348416
45.267115	1294.282126	18.353434
45.472145	1291.342753	18.358451
45.147631	1289.634521	18.363469
45.212295	1288.680588	18.368487
45.330862	1279.552830	18.373504
45.126592	1294.096111	18.378522
45.267720	1283.857388	18.383539
45.171217	1288.234750	18.388557
45.145940	1283.913299	18.393575
45.025139	1304.282102	18.398592
44.843911	1298.613897	18.403610
45.368294	1289.528373	18.408627
45.105363	1294.957848	18.413645
44.958569	1294.688844	18.418663
45.239056	1312.160760	18.423680
45.535869	1317.147058	18.428698
45.695218	1317.274377	18.433715
45.589644	1324.371275	18.438733
45.706654	1321.276054	18.443751
45.629495	1315.943589	18.448768
45.581520	1328.863848	18.453786
45.736177	1310.375903	18.458803
45.468072	1326.093388	18.463821
45.366644	1325.683446	18.468839
45.862558	1313.187546	18.473856
45.254602	1329.358766	18.478874
45.708788	1327.414660	18.483891
45.815893	1345.452221	18.488909
45.735184	1336.924048	18.493927
45.767814	1342.858515	18.498944
46.083238	1338.023407	18.503962
46.124555	1343.045742	18.508979
46.041286	1335.944658	18.513997
46.144776	1343.536739	18.519015
46.024467	1348.459015	18.524032
46.321402	1365.513109	18.529050
46.839022	1358.108551	18.534067
46.798304	1368.608466	18.539085
46.791562	1343.552339	18.544103
46.881817	1339.349295	18.549120
46.926831	1327.746380	18.554138
46.688236	1335.496829	18.559155
46.369748	1333.229228	18.564173
46.732527	1319.117100	18.569191
46.932573	1328.631665	18.574208
46.801774	1333.522576	18.579226
46.669161	1331.363753	18.584243
46.854004	1330.838946	18.589261
46.997482	1342.766031	18.594279
46.979454	1353.185241	18.599296
46.913084	1368.250849	18.604314
47.306289	1344.790417	18.609331
47.244949	1362.035347	18.614349
47.440480	1367.368138	18.619367
47.287321	1346.113626	18.624384
46.784920	1349.336691	18.629402
46.967080	1360.227328	18.634419
47.119196	1360.291310	18.639437
47.176349	1353.570502	18.644455
47.283037	1348.968447	18.649472
47.411875	1361.030011	18.654490
47.701768	1350.784819	18.659507
47.688293	1350.629827	18.664525
47.578836	1359.931087	18.669543
47.696621	1350.765658	18.674560
47.461184	1357.405101	18.679578
47.421831	1346.235608	18.684595
47.474737	1361.873623	18.689613
47.741091	1372.595119	18.694631
47.844993	1388.138515	18.699648
47.734320	1385.809450	18.704666
48.266181	1373.984142	18.709683
48.055065	1386.645764	18.714701
48.154764	1376.709301	18.719719
48.335477	1372.645972	18.724736
48.013657	1382.770745	18.729754
48.258187	1376.336210	18.734771
48.094677	1385.463642	18.739789
48.047957	1375.657494	18.744807
48.424013	1378.183636	18.749824
48.363796	1374.127271	18.754842
48.791709	1361.783741	18.759859
48.435357	1372.779146	18.764877
48.284468	1371.359381	18.769895
48.623848	1370.658922	18.774912
48.488988	1380.475461	18.779930
48.829453	1374.456621	18.784947
48.619140	1378.550150	18.789965
48.499686	1378.498572	18.794983
49.012422	1373.606818	18.800000
48.706350	1388.042163	18.805018
48.612002	1370.776727	18.810035
48.442914	1379.780781	18.815053
48.353610	1387.946307	18.820071
48.962664	1403.712742	18.825088
48.733359	1402.281885	18.830106
49.152669	1410.323839	18.835123
49.255204	1398.541813	18.840141
49.395979	1405.994279	18.845159
49.396808	1406.216091	18.850176
49.173730	1405.147597	18.855194
49.546056	1392.507750	18.860211
49.704206	1392.009220	18.865229
49.490019	1399.519865	18.870247
49.540907	1392.491735	18.875264
49.469347	1392.146239	18.880282
49.796255	1388.298682	18.885299
49.569695	1396.180946	18.890317
49.560205	1393.662716	18.895335
50.018309	1383.354496	18.900352
49.419450	1402.863761	18.905370
49.906252	1390.721594	18.910387
50.081201	1385.594279	18.915405
49.792494	1398.216377	18.920423
50.168493	1387.362844	18.925440
49.797898	1394.207896	18.930458
49.670076	1390.909469	18.935475
49.893605	1399.149376	18.940493
49.905464	1398.584516	18.945511
50.315979	1404.032468	18.950528
50.115282	1425.402009	18.955546
50.212840	1416.261786	18.960563
50.168145	1420.534974	18.965581
50.162917	1414.009697	18.970599
50.374548	1409.653573	18.975616
50.588140	1412.126983	18.980634
50.565822	1419.245255	18.985651
50.632965	1409.639567	18.990669
50.641468	1422.733368	18.995687
50.724252	1406.580046	19.000704
50.426294	1420.965367	19.005722
50.590341	1401.733365	19.010739
50.424846	1400.389856	19.015757
50.207338	1416.605865	19.020775
50.811667	1418.719670	19.025792
50.839840	1433.859929	19.030810
50.996202	1440.971737	19.035827
51.299226	1441.467816	19.040845
51.176631	1437.597554	19.045863
51.364616	1433.547206	19.050880
51.250307	1442.846147	19.055898
51.476262	1433.940258	19.060915
51.295601	1423.724442	19.065933
51.144030	1419.657465	19.070951
51.270548	1410.739135	19.075968
51.379744	1429.290829	19.080986
51.155314	1443.743096	19.086003
51.415559	1435.555307	19.091021
51.636083	1443.454383	19.096039
51.872058	1441.416079	19.101056
51.767210	1438.831254	19.106074
51.698807	1437.374732	19.111091
51.949121	1429.537731	19.116109
51.626320	1438.684308	19.121127
51.728863	1425.667473	19.126144
51.839531	1439.540921	19.131162
51.923398	1441.347635	19.136179
51.911712	1423.781097	19.141197
51.596248	1442.636478	19.146215
52.200141	1428.270294	19.151232
52.158665	1446.040676	19.156250
51.956224	1430.848286	19.161267
52.075533	1437.753650	19.166285
52.175495	1461.724187	19.171303
51.947556	1461.889679	19.176320
52.521913	1457.977473	19.181338
52.614739	1459.685235	19.186355
52.794606	1445.886864	19.191373
52.893582	1461.552245	19.196391
52.990825	1446.766636	19.201408
52.838154	1463.963334	19.206426
52.709506	1458.237917	19.211443
53.231956	1450.901755	19.216461
52.654941	1440.966207	19.221479
52.946223	1448.234249	19.226496
53.043254	1447.245258	19.231514
53.178775	1443.064851	19.236531
53.174491	1428.982842	19.241549
53.076040	1426.502388	19.246567
53.074724	1411.598829	19.251584
53.106604	1428.473480	19.256602
53.189572	1429.193410	19.261619
53.441730	1425.916171	19.266637
52.821961	1430.532749	19.271655
53.022060	1437.530618	19.276672
53.111665	1446.568961	19.281690
53.027243	1460.808586	19.286707
53.252522	1454.155297	19.291725
53.268902	1449.190098	19.296743
53.437693	1457.075410	19.301760
53.010364	1454.318648	19.306778
53.487046	1478.354972	19.311795
53.643089	1472.480331	19.316813
53.750185	1490.542456	19.321831
53.686011	1481.452365	19.326848
53.920271	1489.368938	19.331866
53.665255	1485.231926	19.336883
53.791975	1479.685206	19.341901
53.796232	1483.288381	19.346919
53.648064	1488.760184	19.351936
54.288375	1490.281541	19.356954
54.246173	1504.250215	19.361971
54.743481	1511.743401	19.366989
54.259636	1502.732023	19.372007
54.081958	1512.490988	19.377024
54.245547	1493.958914	19.382042
54.468196	1507.219982	19.387059
54.490212	1505.966105	19.392077
54.611901	1503.143798	19.397095
54.452552	1504.729765	19.402112
54.339952	1500.411165	19.407130
54.352135	1499.355480	19.412147
54.520169	1497.364183	19.417165
54.804896	1498.644955	19.422183
54.449346	1490.025246	19.427200
54.977050	1510.265748	19.432218
55.096233	1525.942133	19.437235
55.285083	1531.614243	19.442253
55.164995	1536.188917	19.447271
55.273530	1532.473674	19.452288
55.937210	1516.973184	19.457306
55.051506	1501.870808	19.462323
55.347634	1489.554480	19.467341
54.966375	1500.284973	19.472359
55.204417	1512.275767	19.477376
55.642424	1523.871321	19.482394
55.523596	1514.287357	19.487411
55.885365	1522.568209	19.492429
55.290500	1516.385451	19.497447
55.945100	1521.992719	19.502464
55.793219	1514.712157	19.507482
55.556473	1528.213243	19.512499
56.099888	1505.054206	19.517517
55.604501	1517.199721	19.522535
55.704052	1514.846546	19.527552
55.859709	1513.236310	19.532570
55.571216	1513.263598	19.537587
55.744910	1511.274543	19.542605
55.747083	1515.584327	19.547623
56.077394	1527.429861	19.552640
56.184390	1532.171234	19.557658
56.293016	1541.793326	19.562675
56.570703	1543.946660	19.567693
56.442633	1545.913025	19.572711
56.740989	1533.899890	19.577728
56.776158	1540.894226	19.582746
56.459432	1539.593697	19.587763
57.150214	1521.015265	19.592781
56.690291	1524.747530	19.597799
56.493752	1511.627308	19.602816
56.835237	1522.470638	19.607834
56.628919	1537.640537	19.612851
56.718398	1527.273030	19.617869
56.715299	1529.771580	19.622887
56.508489	1548.137875	19.627904
56.670805	1538.889722	19.632922
56.725706	1533.136577	19.637939
57.111558	1535.560516	19.642957
56.959936	1541.359284	19.647975
57.045721	1553.740900	19.652992
57.291010	1560.881057	19.658010
57.374950	1566.256887	19.663027
58.122102	1565.181512	19.668045
57.868295	1557.973811	19.673063
57.713524	1544.043101	19.678080
58.047841	1530.224737	19.683098
57.705695	1519.658662	19.688115
57.749479	1514.824347	19.693133
57.585611	1525.702656	19.698151
57.713125	1523.859386	19.703168
57.849929	1522.640683	19.708186
58.035154	1542.386877	19.713203
58.021385	1557.376655	19.718221
58.169271	1554.068827	19.723239
57.937703	1563.392837	19.728256
58.307232	1551.351035	19.733274
58.296241	1557.231200	19.738291
58.530226	1547.202421	19.743309
58.280624	1553.222882	19.748327
58.576289	1555.093358	19.753344
59.021355	1533.958666	19.758362
58.445939	1535.038422	19.763379
58.263886	1515.891349	19.768397
58.348727	1516.227177	19.773415
58.428734	1536.138003	19.778432
58.510518	1536.205338	19.783450
58.348126	1542.395926	19.788467
58.531805	1544.885141	19.793485
58.442644	1547.924371	19.798503
58.602584	1539.829596	19.803520
58.869034	1560.239245	19.808538
58.799912	1570.893271	19.813555
58.827410	1569.909068	19.818573
59.393326	1576.381489	19.823591
59.098535	1571.237788	19.828608
59.255986	1573.040649	19.833626
59.079073	1569.380356	19.838643
59.056766	1566.678527	19.843661
59.323634	1564.407197	19.848679
59.078370	1578.553041	19.853696
59.437623	1575.960244	19.858714
59.636611	1569.957595	19.863731
59.306856	1578.587855	19.868749
59.676398	1592.258147	19.873767
59.423151	1590.323011	19.878784
59.670666	1596.548923	19.883802
59.811406	1602.845347	19.888819
59.964226	1592.065007	19.893837
60.031749	1596.590904	19.898855
59.829666	1591.861839	19.903872
59.904687	1593.603917	19.908890
60.103492	1605.028476	19.913907
59.989939	1600.920779	19.918925
60.071136	1593.304138	19.923943
60.070212	1602.308252	19.928960
60.126727	1608.811589	19.933978
60.295825	1621.145370	19.938995
60.529239	1625.462354	19.944013
60.755804	1620.556384	19.949031
60.174899	1626.264774	19.954048
60.663081	1618.216708	19.959066
60.891645	1611.506196	19.964083
60.821881	1617.005656	19.969101
61.279559	1598.824516	19.974119
60.956543	1616.839776	19.979136
61.103032	1600.952925	19.984154
60.965275	1617.590586	19.989171
61.296370	1601.315652	19.994189
61.225402	1606.189248	19.999207
61.325340	1604.480925	20.004224
61.449531	1592.976853	20.009242
61.492725	1601.288106	20.014259
61.049364	1606.856579	20.019277
61.575569	1602.456523	20.024295
61.170513	1603.888207	20.029312
61.715030	1607.271550	20.034330
61.590697	1591.317788	20.039347
61.230815	1602.710322	20.044365
61.545284	1590.801535	20.049383
61.636838	1616.497670	20.054400
61.986804	1621.860983	20.059418
62.087978	1624.405841	20.064435
62.121576	1633.781988	20.069453
61.990861	1625.047692	20.074471
62.269647	1631.677611	20.079488
62.361020	1620.896037	20.084506
62.572173	1620.969483	20.089523
62.241369	1611.576559	20.094541
62.093201	1602.333836	20.099559
61.911535	1610.769042	20.104576
62.347212	1625.929457	20.109594
62.520910	1625.172042	20.114611
62.127949	1632.775809	20.119629
62.549750	1628.533966	20.124647
62.255649	1629.685266	20.129664
62.609268	1624.617463	20.134682
62.430061	1630.549652	20.139699
62.135917	1619.516533	20.144717
62.892275	1642.511253	20.149735
62.880820	1641.742466	20.154752
63.223229	1643.860326	20.159770
63.046939	1642.922775	20.164787
63.246246	1647.470143	20.169805
63.398581	1641.105251	20.174823
63.330533	1645.228074	20.179840
63.482478	1635.778597	20.184858
63.272535	1651.526482	20.189875
63.357600	1641.727450	20.194893
63.260447	1649.520002	20.199911
63.145030	1651.907499	20.204928
63.410409	1643.328672	20.209946
63.505922	1639.750756	20.214963
63.396904	1669.195963	20.219981
63.668412	1663.581253	20.224999
63.729187	1682.010435	20.230016
64.154636	1678.373601	20.235034
63.974974	1680.091812	20.240051
64.001580	1674.335258	20.245069
64.099749	1664.284014	20.250087
64.029913	1678.466472	20.255104
64.069081	1673.277341	20.260122
64.262030	1675.209832	20.265139
63.921600	1676.719303	20.270157
64.182599	1677.228387	20.275175
64.255182	1697.368704	20.280192
64.469943	1705.456031	20.285210
64.330329	1701.626164	20.290227
64.389064	1707.218421	20.295245
64.662832	1696.958256	20.300263
64.602036	1709.693712	20.305280
64.665576	1699.430891	20.310298
64.596856	1691.095649	20.315315
64.831314	1726.919782	20.320333
65.339144	1722.206448	20.325351
65.456526	1723.474603	20.330368
65.862461	1710.209358	20.335386
65.702669	1698.970711	20.340403
65.189290	1692.991954	20.345421
65.635495	1678.741907	20.350439
65.387823	1686.718929	20.355456
65.281859	1688.257076	20.360474
65.752740	1673.372325	20.365491
65.575198	1691.477734	20.370509
65.629814	1677.585861	20.375527
65.624334	1697.167628	20.380544
65.757383	1690.624894	20.385562
65.678429	1679.415841	20.390579
65.767335	1706.679268	20.395597
66.078019	1706.647181	20.400615
65.926051	1719.081011	20.405632
65.791764	1721.878938	20.410650
66.099967	1703.553194	20.415667
65.991183	1727.739930	20.420685
66.139016	1715.950422	20.425703
65.999865	1721.215598	20.430720
66.247598	1719.779417	20.435738
66.433864	1708.564226	20.440755
65.984226	1730.968055	20.445773
66.547114	1728.597584	20.450791
66.862559	1751.982114	20.455808
66.850622	1739.692681	20.460826
67.103343	1736.827412	20.465843
67.109037	1745.604046	20.470861
67.083749	1737.617351	20.475879
67.164253	1735.956156	20.480896
67.149726	1734.942465	20.485914
67.421061	1732.052207	20.490931
67.155681	1717.847961	20.495949
67.353272	1712.753101	20.500967
67.266849	1714.085217	20.505984
67.471398	1725.401992	20.511002
67.729804	1724.950384	20.516019
67.706619	1733.377691	20.521037
67.590287	1721.219751	20.526055
67.229115	1717.389032	20.531072
67.442025	1724.613085	20.536090
67.955347	1739.772250	20.541107
67.509331	1741.978105	20.546125
67.821239	1733.970672	20.551143
67.787434	1731.536484	20.556160
67.480935	1740.428968	20.561178
68.132757	1729.512320	20.566195
67.819351	1743.968063	20.571213
68.443661	1747.783877	20.576231
68.355717	1753.869875	20.581248
67.903087	1762.419165	20.586266
68.242803	1766.187562	20.591283
67.920523	1764.684977	20.596301
68.075435	1762.999329	20.601319
68.153365	1766.464984	20.606336
68.115304	1771.704618	20.611354
69.078306	1780.592877	20.616371
68.833146	1785.978800	20.621389
69.090446	1781.080458	20.626407
69.202818	1791.170878	20.631424
69.214666	1790.623308	20.636442
69.422318	1777.641305	20.641459
69.360169	1778.945960	20.646477
69.476964	1772.533196	20.651495
69.508257	1744.975510	20.656512
69.394151	1747.818987	20.661530
69.384719	1739.084156	20.666547
69.173654	1738.141132	20.671565
69.320610	1757.088343	20.676583
69.228754	1772.776630	20.681600
69.137177	1768.438866	20.686618
69.379732	1772.405229	20.691635
69.220028	1772.053330	20.696653
69.476006	1787.536726	20.701671
69.714488	1796.450873	20.706688
69.341617	1796.861273	20.711706
70.161674	1805.492347	20.716723
69.796055	1798.588643	20.721741
69.986859	1801.331596	20.726759
70.182855	1798.660977	20.731776
70.218273	1804.057218	20.736794
70.619673	1807.485456	20.741811
70.618489	1823.009900	20.746829
70.847342	1815.887119	20.751847
70.778405	1805.423554	20.756864
70.577138	1789.631279	20.761882
70.910106	1801.184036	20.766899
70.870974	1810.494818	20.771917
70.809941	1821.135153	20.776935
71.040580	1823.558727	20.781952
71.030307	1813.647369	20.786970
71.512856	1817.871199	20.791987
71.094688	1809.719030	20.797005
71.359621	1809.189301	20.802023
71.601813	1808.812636	20.807040
71.598478	1814.117533	20.812058
71.745131	1797.999207	20.817075
71.432573	1782.978160	20.822093
71.381010	1798.872406	20.827111
71.483212	1785.169468	20.832128
71.320747	1800.022763	20.837146
71.927569	1804.631036	20.842163
71.427842	1802.434731	20.847181
71.381593	1799.252187	20.852199
71.516681	1798.205195	20.857216
71.533270	1816.202723	20.862234
71.746403	1830.450315	20.867251
71.721199	1832.136047	20.872269
72.009939	1833.518457	20.877287
71.960011	1842.033461	20.882304
72.146020	1854.498453	20.887322
72.717034	1845.982451	20.892339
72.601187	1860.037144	20.897357
72.563323	1864.976334	20.902375
72.837482	1865.175015	20.907392
72.858458	1861.824435	20.912410
73.342779	1859.696135	20.917427
73.229421	1856.500686	20.922445
73.214494	1845.064217	20.927463
73.051964	1829.383698	20.932480
72.759890	1822.528028	20.937498
72.877729	1828.014954	20.942515
73.093924	1858.454741	20.947533
72.838186	1855.352783	20.952551
73.240167	1841.985803	20.957568
73.189357	1854.288787	20.962586
73.373219	1845.504191	20.967603
73.701553	1844.486153	20.972621
73.611714	1849.762387	20.977639
73.474835	1847.898319	20.982656
73.354764	1857.324286	20.987674
73.676187	1864.325039	20.992691
73.825798	1880.484594	20.997709
73.975782	1885.050915	21.002727
74.101122	1874.273175	21.007744
74.320743	1884.823183	21.012762
74.119516	1883.664649	21.017779
74.266527	1881.709687	21.022797
74.168154	1886.438310	21.027815
74.280314	1882.152965	21.032832
73.941849	1881.872042	21.037850
74.438391	1886.963544	21.042867
74.552352	1889.751802	21.047885
74.415430	1907.555273	21.052903
74.848899	1894.269741	21.057920
74.970360	1890.596390	21.062938
74.929033	1897.106022	21.067955
74.868189	1896.430041	21.072973
74.744495	1892.965671	21.077991
75.257606	1896.234544	21.083008
75.194715	1897.435509	21.088026
75.219460	1900.628107	21.093043
75.353810	1889.677459	21.098061
74.937671	1898.036964	21.103079
75.252600	1914.884348	21.108096
75.412774	1929.742953	21.113114
75.492846	1921.393288	21.118131
75.986669	1920.811325	21.123149
76.045647	1918.694218	21.128167
76.127704	1917.139721	21.133184
76.133835	1910.552634	21.138202
76.266920	1917.449740	21.143219
76.692601	1914.747192	21.148237
76.289230	1923.357933	21.153255
76.400402	1920.573403	21.158272
76.594339	1916.135008	21.163290
76.219517	1920.696941	21.168307
76.478814	1917.695309	21.173325
76.105216	1928.980171	21.178343
76.180419	1913.305694	21.183360
76.396031	1918.909197	21.188378
76.341274	1922.487285	21.193395
76.610683	1923.768968	21.198413
76.374260	1942.849919	21.203431
76.795563	1949.233889	21.208448
77.195590	1942.521052	21.213466
76.802896	1947.203820	21.218483
76.803453	1946.612427	21.223501
76.583634	1947.887186	21.228519
77.106174	1958.936356	21.233536
76.871007	1974.889962	21.238554
76.926141	1978.596831	21.243571
77.495666	1962.566618	21.248589
77.235389	1981.031648	21.253607
77.620893	1975.497742	21.258624
77.811667	1993.006814	21.263642
77.677779	1993.956411	21.268659
78.122664	1995.246298	21.273677
78.175700	1994.781816	21.278695
78.466230	1984.896304	21.283712
78.309568	1990.944594	21.288730
78.487105	1979.502496	21.293747
78.882166	1977.871337	21.298765
78.985735	1963.329586	21.303783
78.560594	1957.130577	21.308800
78.528794	1944.301442	21.313818
78.468275	1950.482248	21.318835
78.710970	1953.039203	21.323853
78.393838	1957.175095	21.328871
79.106376	1962.166113	21.333888
78.641723	1974.173395	21.338906
78.686673	1979.835598	21.343923
78.991695	1977.399246	21.348941
78.748259	1983.821595	21.353959
78.875667	1980.944803	21.358976
79.156543	1983.239270	21.363994
79.022155	1986.169398	21.369011
79.252171	1998.135136	21.374029
79.310607	2009.093186	21.379047
79.298236	2003.584965	21.384064
79.441900	2012.835267	21.389082
79.248236	2010.008096	21.394099
79.814341	2013.877312	21.399117
79.821749	2031.086906	21.404135
80.030127	2035.406434	21.409152
79.991515	2031.673631	21.414170
80.360981	2033.298021	21.419187
80.130067	2036.671419	21.424205
80.263184	2027.597501	21.429223
80.406149	2029.331943	21.434240
80.455210	2031.215069	21.439258
80.231432	2023.777399	21.444275
80.712711	2027.524865	21.449293
80.570062	2027.041250	21.454311
80.562821	2033.363034	21.459328
80.507690	2047.307551	21.464346
80.959911	2050.974713	21.469363
81.001824	2058.787779	21.474381
80.698902	2057.313535	21.479399
81.082391	2063.423585	21.484416
81.144937	2062.029488	21.489434
81.108880	2061.777414	21.494451
81.407419	2052.019570	21.499469
81.409737	2064.688643	21.504487
81.517924	2062.757153	21.509504
81.275509	2062.723605	21.514522
81.262645	2073.889705	21.519539
81.466349	2075.493343	21.524557
81.806528	2084.739095	21.529575
81.836068	2085.569827	21.534592
81.628507	2086.638146	21.539610
81.817118	2080.478066	21.544627
82.135367	2077.618012	21.549645
82.027047	2074.129125	21.554663
82.348119	2098.848834	21.559680
82.611524	2101.894878	21.564698
82.620504	2108.144894	21.569715
83.120431	2089.778653	21.574733
82.895196	2089.441914	21.579751
83.259673	2074.131699	21.584768
82.864985	2067.105083	21.589786
82.774665	2066.973349	21.594803
82.773600	2066.388502	21.599821
82.805479	2075.928807	21.604839
82.301315	2092.644318	21.609856
82.924127	2087.807140	21.614874
83.182534	2098.428199	21.619891
83.586464	2087.056882	21.624909
83.487427	2089.105206	21.629927
83.768820	2094.306599	21.634944
83.762678	2092.836935	21.639962
83.548698	2088.922867	21.644979
83.748707	2092.454078	21.649997
84.215531	2107.095649	21.655015
83.875453	2109.220168	21.660032
84.041850	2113.441020	21.665050
83.661394	2114.255335	21.670067
83.968998	2126.304763	21.675085
83.991648	2116.745030	21.680103
84.105811	2113.113686	21.685120
84.564083	2113.758073	21.690138
84.386572	2124.428216	21.695155
84.418938	2107.498774	21.700173
84.540181	2132.351083	21.705191
84.741364	2139.006197	21.710208
85.019339	2138.362693	21.715226
84.777773	2151.737707	21.720243
84.751183	2144.490330	21.725261
84.977868	2140.690024	21.730279
84.999454	2147.446142	21.735296
84.952934	2143.439287	21.740314
84.875999	2159.784720	21.745331
85.264792	2151.750642	21.750349
85.304177	2163.397698	21.755367
85.283000	2162.652457	21.760384
85.280502	2169.140288	21.765402
85.799414	2164.909550	21.770419
85.720799	2169.095555	21.775437
85.364464	2171.339080	21.780455
85.501302	2168.887045	21.785472
86.063719	2178.386860	21.790490
86.124121	2197.398788	21.795507
86.601339	2187.727194	21.800525
86.501527	2178.693472	21.805543
86.631874	2197.107497	21.810560
86.581957	2179.867042	21.815578
86.609014	2183.235515	21.820595
86.530217	2180.344374	21.825613
86.740873	2189.807481	21.830631
86.826600	2187.602697	21.835648
86.856882	2181.184672	21.840666
86.826477	2189.519011	21.845683
86.975682	2180.585581	21.850701
86.955054	2182.684337	21.855719
86.722997	2171.843817	21.860736
87.241119	2198.226455	21.865754
87.405466	2200.659093	21.870771
87.847869	2203.308519	21.875789
87.439432	2210.966962	21.880807
87.240468	2210.023548	21.885824
87.738219	2209.684775	21.890842
87.381115	2215.535455	21.895859
87.730579	2208.286282	21.900877
88.062608	2212.751317	21.905895
87.976237	2227.462349	21.910912
88.073947	2236.510905	21.915930
87.989625	2240.765483	21.920947
88.081690	2231.410115	21.925965
88.287553	2229.758762	21.930983
88.333592	2241.126388	21.936000
88.712252	2221.503566	21.941018
88.628126	2232.813289	21.946035
88.665746	2227.529824	21.951053
89.315847	2240.207441	21.956071
89.403276	2241.554354	21.961088
89.057845	2238.288858	21.966106
88.939484	2225.498446	21.971123
89.266153	2234.412960	21.976141
89.027896	2243.987014	21.981159
89.138073	2251.303222	21.986176
89.365738	2248.479604	21.991194
89.255663	2242.738328	21.996211
89.370608	2248.957350	22.001229
89.473953	2242.118651	22.006247
89.541633	2263.585056	22.011264
89.857535	2260.632532	22.016282
89.621059	2277.310286	22.021299
89.712109	2268.269669	22.026317
90.245414	2267.989722	22.031335
89.865147	2267.263983	22.036352
90.441226	2262.217120	22.041370
90.366773	2264.996169	22.046387
90.318780	2266.894803	22.051405
90.595220	2261.242899	22.056423
90.739159	2286.025783	22.061440
90.568756	2284.689262	22.066458
90.809718	2293.581299	22.071475
91.335538	2282.593100	22.076493
91.315973	2283.080880	22.081511
91.144251	2295.994992	22.086528
91.057967	2277.486034	22.091546
91.069151	2277.948461	22.096563
91.041939	2287.570689	22.101581
91.464785	2275.758897	22.106599
91.600399	2282.522065	22.111616
91.754613	2278.261359	22.116634
91.547847	2276.875580	22.121651
91.795656	2283.974798	22.126669
91.873121	2279.589474	22.131687
91.688615	2293.491935	22.136704
92.038468	2299.149687	22.141722
92.035199	2308.030341	22.146739
91.811175	2310.737293	22.151757
92.084624	2312.071853	22.156775
91.911418	2317.430765	22.161792
92.129457	2323.071793	22.166810
91.789432	2341.014364	22.171827
92.445362	2338.757173	22.176845
92.817102	2336.988119	22.181863
92.424921	2350.626440	22.186880
92.897880	2349.893631	22.191898
93.066952	2361.109594	22.196915
93.113866	2369.929585	22.201933
93.212006	2364.853504	22.206951
93.264189	2365.690080	22.211968
93.643587	2358.450218	22.216986
93.392097	2364.779634	22.222003
93.753113	2370.686540	22.227021
93.780070	2352.152352	22.232039
93.844257	2350.731224	22.237056
94.119076	2351.222401	22.242074
94.081592	2358.028151	22.247091
93.907739	2360.686212	22.252109
94.185658	2367.509313	22.257127
94.352636	2376.999171	22.262144
94.328408	2385.776245	22.267162
94.360592	2392.407301	22.272179
94.636552	2388.721774	22.277197
94.933462	2380.252323	22.282215
94.453993	2391.342844	22.287232
94.733925	2382.862727	22.292250
95.057209	2377.323650	22.297267
94.792339	2381.864257	22.302285
95.249848	2376.369846	22.307303
94.912699	2383.814869	22.312320
95.302918	2383.468860	22.317338
95.062454	2380.439858	22.322355
95.028711	2393.831506	22.327373
95.149099	2399.163294	22.332391
95.228163	2408.288865	22.337408
95.152645	2411.451158	22.342426
95.447294	2412.535373	22.347443
95.590779	2435.566173	22.352461
95.822446	2430.370459	22.357479
95.950408	2438.933741	22.362496
96.469235	2436.120290	22.367514
96.355260	2431.376896	22.372531
96.314673	2425.728290	22.377549
96.943592	2425.218370	22.382567
96.584282	2435.598393	22.387584
96.659048	2429.179458	22.392602
96.703091	2437.450156	22.397619
96.689439	2426.526637	22.402637
96.831563	2432.014640	22.407655
96.647766	2436.254462	22.412672
96.910746	2454.693283	22.417690
96.867636	2457.766258	22.422707
96.986880	2457.483120	22.427725
97.390064	2465.686340	22.432743
97.113866	2464.101607	22.437760
97.351427	2483.066782	22.442778
97.485952	2478.011603	22.447795
97.694701	2486.714620	22.452813
98.059875	2477.761514	22.457831
98.175902	2482.353104	22.462848
98.111851	2473.038992	22.467866
98.042305	2481.856385	22.472883
97.990909	2482.779488	22.477901
98.417333	2468.029228	22.482919
98.289431	2495.413658	22.487936
98.144366	2507.138381	22.492954
98.599132	2503.366896	22.497971
98.754481	2510.876601	22.502989
98.730557	2504.488314	22.508007
98.871631	2511.570056	22.513024
98.865066	2514.415408	22.518042
98.825277	2505.104486	22.523059
98.956626	2522.020394	22.528077
99.404069	2524.445699	22.533095
99.584405	2522.283197	22.538112
99.828806	2525.990703	22.543130
99.942012	2518.927709	22.548147
99.682491	2519.027452	22.553165
99.667313	2531.246671	22.558183
99.829016	2527.906533	22.563200
99.840182	2524.720966	22.568218
99.938411	2517.067305	22.573235
99.939740	2525.109687	22.578253
100.353155	2517.824996	22.583271
100.142435	2527.311469	22.588288
100.182711	2543.743254	22.593306
100.496679	2541.308532	22.598323
100.687968	2544.611574	22.603341
100.662112	2546.050516	22.608359
100.455838	2547.574858	22.613376
100.368025	2543.627961	22.618394
100.630674	2550.324591	22.623411
100.764856	2573.978466	22.628429
100.651918	2571.335735	22.633447
100.678247	2578.262765	22.638464
101.110955	2583.415825	22.643482
101.347074	2591.097532	22.648499
101.527987	2603.996585	22.653517
101.552363	2595.501252	22.658535
101.766524	2603.365800	22.663552
102.033997	2589.279445	22.668570
102.076684	2598.381047	22.673587
101.849731	2601.823944	22.678605
102.222357	2608.556549	22.683623
102.603467	2611.015257	22.688640
102.436374	2618.120235	22.693658
102.636846	2606.287792	22.698675
102.926786	2616.984433	22.703693
102.680108	2614.771240	22.708711
102.811709	2612.929544	22.713728
102.684036	2616.677526	22.718746
102.814254	2598.548936	22.723763
102.466597	2620.660212	22.728781
102.808648	2635.732799	22.733799
103.252796	2628.465176	22.738816
103.049381	2640.357408	22.743834
103.603499	2625.781694	22.748851
103.627319	2637.736795	22.753869
104.100574	2632.939810	22.758887
103.680784	2647.919162	22.763904
103.872988	2653.518819	22.768922
104.389363	2654.468593	22.773939
104.191796	2663.625065	22.778957
104.267863	2661.368265	22.783975
104.694270	2647.900698	22.788992
104.207899	2659.590301	22.794010
104.794049	2639.381672	22.799027
104.546538	2655.581820	22.804045
104.848358	2637.255923	22.809063
104.470135	2652.975877	22.814080
104.662586	2661.880597	22.819098
105.240475	2659.093083	22.824115
105.083485	2679.070013	22.829133
105.360804	2673.359607	22.834151
105.506114	2676.484384	22.839168
105.572268	2676.994690	22.844186
105.818284	2674.595952	22.849203
105.918828	2667.116459	22.854221
105.833778	2670.005819	22.859239
106.022980	2666.680142	22.864256
105.857089	2673.181667	22.869274
106.338691	2668.005794	22.874291
105.921017	2674.865237	22.879309
106.128645	2669.356291	22.884327
106.328037	2671.423966	22.889344
106.071217	2669.862075	22.894362
106.281253	2680.311942	22.899379
106.357688	2694.656120	22.904397
106.643377	2682.394726	22.909415
106.743444	2703.827516	22.914432
106.646763	2701.053172	22.919450
106.919061	2707.857669	22.924467
106.948243	2716.591031	22.929485
107.069059	2723.742177	22.934503
107.312821	2727.213870	22.939520
107.028103	2740.957333	22.944538
107.638873	2731.258582	22.949555
107.613165	2738.599851	22.954573
107.622042	2753.588826	22.959591
107.663407	2756.118252	22.964608
107.629938	2766.639258	22.969626
108.006920	2755.768042	22.974643
108.016764	2768.066059	22.979661
108.261032	2773.224853	22.984679
108.626721	2785.595139	22.989696
108.569504	2783.076412	22.994714
108.923995	2784.226626	22.999731
108.823848	2784.252189	23.004749
109.011899	2777.772562	23.009767
109.006318	2779.128065	23.014784
108.949379	2788.443099	23.019802
109.464061	2771.154388	23.024819
109.452577	2785.129620	23.029837
109.165732	2770.224575	23.034855
109.444984	2776.305147	23.039872
109.343977	2800.916383	23.044890
109.732498	2801.981729	23.049907
109.654942	2805.768962	23.054925
109.266473	2802.676948	23.059943
109.479293	2810.143036	23.064960
109.805803	2836.536156	23.069978
110.060427	2832.136576	23.074995
110.116758	2837.728868	23.080013
110.083973	2850.888747	23.085031
110.674542	2852.210549	23.090048
110.659487	2865.469081	23.095066
110.884521	2858.108861	23.100083
110.915008	2857.513445	23.105101
110.881800	2849.254463	23.110119
111.415910	2845.435632	23.115136
110.997764	2867.692238	23.120154
111.152968	2869.317859	23.125171
111.392534	2879.159079	23.130189
111.268141	2896.307337	23.135207
111.697160	2889.945764	23.140224
111.802616	2889.739542	23.145242
112.218256	2876.688789	23.150259
112.266232	2886.362348	23.155277
112.201919	2881.112205	23.160295
112.176083	2875.163750	23.165312
112.172992	2882.550252	23.170330
112.225828	2875.055449	23.175347
112.235941	2882.044989	23.180365
112.469082	2897.946164	23.185383
112.748620	2901.151841	23.190400
112.630467	2902.717227	23.195418
112.929666	2894.518482	23.200435
113.048503	2902.226135	23.205453
112.761232	2906.337076	23.210471
113.171178	2912.949035	23.215488
113.019951	2937.662898	23.220506
113.166692	2933.731194	23.225523
113.946220	2920.850484	23.230541
113.405946	2932.047853	23.235559
113.929144	2931.295213	23.240576
113.969954	2955.504184	23.245594
114.193270	2956.883770	23.250611
114.558689	2950.080036	23.255629
114.243596	2948.543136	23.260647
114.604857	2957.844295	23.265664
114.327661	2954.038391	23.270682
114.745149	2956.584962	23.275699
115.011949	2947.232735	23.280717
114.569989	2956.531399	23.285735
115.135988	2949.764113	23.290752
115.017878	2956.163756	23.295770
114.868537	2973.113934	23.300787
115.311605	2974.898962	23.305805
115.377182	2976.289544	23.310823
115.645888	2975.081942	23.315840
115.819363	2973.545007	23.320858
115.646829	2980.287631	23.325875
115.925671	2984.559242	23.330893
115.680529	2997.138801	23.335911
115.477427	2993.822118	23.340928
115.995679	3001.802002	23.345946
116.254126	3001.432947	23.350963
116.408845	3013.606602	23.355981
116.489666	3024.993679	23.360999
116.639425	3022.623606	23.366016
116.964849	3034.756688	23.371034
116.940946	3022.200643	23.376051
117.041940	3022.633042	23.381069
116.887810	3034.579874	23.386087
117.178206	3026.251101	23.391104
117.205689	3048.594239	23.396122
117.392161	3053.104773	23.401139
117.756416	3052.979988	23.406157
117.536205	3059.647661	23.411175
118.085966	3050.538923	23.416192
117.625762	3053.147591	23.421210
117.846842	3055.473007	23.426227
118.116618	3047.749240	23.431245
117.815943	3048.867867	23.436263
117.959755	3070.217137	23.441280
118.106634	3074.663985	23.446298
118.351745	3074.897213	23.451315
118.651144	3083.572763	23.456333
118.639067	3095.995685	23.461351
118.799536	3099.461872	23.466368
118.865684	3095.087547	23.471386
119.051334	3110.653581	23.476403
119.327470	3099.424566	23.481421
119.228449	3105.084994	23.486439
119.214721	3126.136968	23.491456
119.480275	3139.522479	23.496474
119.741675	3133.463620	23.501491
119.860939	3124.601247	23.506509
119.547845	3134.724261	23.511527
119.918008	3126.882977	23.516544
120.117210	3150.105815	23.521562
120.249823	3160.238009	23.526579
120.499173	3152.828930	23.531597
120.395979	3158.682756	23.536615
120.592973	3152.160636	23.541632
120.736098	3178.233591	23.546650
120.901643	3182.592545	23.551667
121.322958	3183.048599	23.556685
121.023544	3185.921113	23.561703
121.556247	3179.394220	23.566720
121.572452	3178.381034	23.571738
121.486384	3179.119355	23.576755
121.864492	3181.309633	23.581773
121.773138	3175.351051	23.586791
122.014758	3196.817843	23.591808
122.569071	3207.805492	23.596826
122.609998	3201.202047	23.601843
122.441270	3202.165140	23.606861
122.036877	3212.112412	23.611879
122.432208	3201.692586	23.616896
122.583988	3196.268648	23.621914
122.569676	3198.595438	23.626931
122.818339	3206.942495	23.631949
122.568115	3201.464667	23.636967
122.570479	3223.873432	23.641984
122.881794	3225.541062	23.647002
122.828263	3238.262537	23.652019
123.544042	3246.067904	23.657037
123.644461	3269.440404	23.662055
123.946868	3255.192094	23.667072
124.081465	3261.098503	23.672090
123.978077	3257.435492	23.677107
123.971029	3254.885086	23.682125
123.760023	3257.393486	23.687143
124.004138	3255.475564	23.692160
124.144814	3277.911126	23.697178
124.202965	3283.206756	23.702195
124.343237	3286.643958	23.707213
124.400767	3287.977645	23.712231
124.925603	3293.390007	23.717248
124.690051	3299.994947	23.722266
124.935226	3306.279396	23.727283
125.524905	3294.344224	23.732301
125.356288	3292.683247	23.737319
125.659656	3299.046512	23.742336
125.654395	3301.141405	23.747354
125.679322	3294.266736	23.752371
126.107553	3308.781964	23.757389
126.366141	3321.711746	23.762407
126.726500	3312.819470	23.767424
126.522634	3305.730355	23.772442
126.319655	3318.134350	23.777459
126.846083	3316.243771	23.782477
126.512820	3323.806636	23.787495
126.694202	3325.019896	23.792512
126.693480	3316.559608	23.797530
126.513315	3316.457917	23.802547
126.996281	3327.715822	23.807565
126.895929	3340.286747	23.812583
126.962813	3337.254944	23.817600
127.437081	3348.211415	23.822618
127.108233	3362.565811	23.827635
127.520637	3374.103231	23.832653
127.411309	3384.338659	23.837671
127.442571	3386.252331	23.842688
127.783083	3391.501404	23.847706
127.714406	3411.236355	23.852723
128.021760	3416.471846	23.857741
128.217719	3425.017002	23.862759
128.511762	3427.134983	23.867776
128.636265	3434.860107	23.872794
128.455915	3433.809023	23.877811
128.822260	3440.370757	23.882829
128.854270	3449.731811	23.887847
129.082977	3455.237860	23.892864
129.047426	3456.649333	23.897882
129.376285	3456.272975	23.902899
129.925367	3464.203366	23.907917
130.201247	3473.008756	23.912935
130.342521	3472.486896	23.917952
131.008055	3458.424336	23.922970
130.205800	3453.382893	23.927987
130.350272	3432.081012	23.933005
130.584600	3447.461875	23.938023
131.049912	3458.524475	23.943040
131.104474	3463.134043	23.948058
131.081138	3455.843017	23.953075
131.243982	3445.928901	23.958093
131.116263	3442.349956	23.963111
131.003405	3457.930134	23.968128
131.579497	3459.268467	23.973146
131.100397	3459.791014	23.978163
131.558850	3449.379828	23.983181
131.561822	3459.837315	23.988199
131.299909	3457.336164	23.993216
131.854407	3468.103736	23.998234
131.631199	3478.050614	24.003251
131.767312	3479.221550	24.008269
131.673177	3479.915549	24.013287
131.834501	3491.918647	24.018304
132.487174	3509.609973	24.023322
132.348556	3524.995320	24.028339
132.265147	3533.953213	24.033357
132.540144	3540.426513	24.038375
132.452544	3547.153495	24.043392
132.927048	3556.556548	24.048410
133.145932	3584.313277	24.053427
133.540752	3588.200805	24.058445
133.602319	3583.424324	24.063463
133.506930	3583.564759	24.068480
133.982857	3582.238330	24.073498
133.949003	3582.301305	24.078515
134.093129	3598.301607	24.083533
134.566808	3610.190498	24.088551
134.496855	3604.887503	24.093568
134.762762	3607.979095	24.098586
134.870811	3591.614018	24.103603
134.710183	3597.441779	24.108621
134.625125	3600.314804	24.113639
134.607451	3621.216306	24.118656
135.260236	3626.502989	24.123674
135.427662	3624.363625	24.128691
135.382853	3626.315416	24.133709
135.860788	3617.054170	24.138727
135.476681	3630.523268	24.143744
135.837598	3634.306877	24.148762
135.864033	3661.923745	24.153779
136.039299	3660.164631	24.158797
136.150239	3651.677693	24.163815
136.215029	3662.858586	24.168832
136.267778	3675.120636	24.173850
136.520848	3684.185439	24.178867
136.694401	3680.120258	24.183885
136.638616	3693.799006	24.188903
136.735720	3697.696276	24.193920
137.153991	3710.197413	24.198938
137.104180	3712.372622	24.203955
137.256558	3709.746374	24.208973
137.249129	3720.028718	24.213991
137.342373	3753.065083	24.219008
138.117512	3737.244796	24.224026
138.054022	3740.532887	24.229043
138.363757	3733.618107	24.234061
138.396453	3732.137366	24.239079
138.485788	3730.645234	24.244096
138.634155	3727.970852	24.249114
138.496130	3736.317727	24.254131
138.561924	3759.462908	24.259149
139.047850	3751.594971	24.264167
138.995422	3768.767387	24.269184
139.180891	3766.264858	24.274202
139.073182	3767.904971	24.279219
139.035961	3779.197399	24.284237
139.489377	3777.685756	24.289255
139.761635	3803.043084	24.294272
139.915992	3791.293341	24.299290
139.789791	3797.660029	24.304307
139.918036	3803.410348	24.309325
140.515280	3810.760596	24.314343
140.203357	3821.485655	24.319360
140.340191	3810.545759	24.324378
140.434277	3819.020075	24.329395
140.431892	3831.465675	24.334413
140.665397	3835.864335	24.339431
140.816736	3853.206522	24.344448
140.979592	3844.516900	24.349466
141.149689	3867.761255	24.354483
141.212690	3873.076777	24.359501
141.340919	3867.819963	24.364519
141.336063	3903.623117	24.369536
142.097952	3891.980162	24.374554
142.272239	3903.975240	24.379571
142.496747	3897.492455	24.384589
142.913175	3894.426830	24.389607
142.514327	3894.651836	24.394624
142.828855	3886.619220	24.399642
142.731716	3895.530752	24.404659
142.921359	3905.100591	24.409677
143.176982	3911.541749	24.414695
142.905190	3923.972172	24.419712
143.112486	3914.150554	24.424730
143.405112	3935.628394	24.429747
143.572759	3950.332124	24.434765
143.746761	3941.923066	24.439783
143.968717	3951.568805	24.444800
144.303965	3942.795789	24.449818
144.335983	3950.924524	24.454835
144.374571	3965.036067	24.459853
145.058222	3971.439684	24.464871
144.930773	3977.237133	24.469888
145.025785	3962.247954	24.474906
145.253063	3968.738495	24.479923
145.389015	3971.400150	24.484941
145.484548	3953.170005	24.489959
145.414938	3962.047297	24.494976
145.826976	3953.388678	24.499994
145.583404	3952.474280	24.505011
145.730408	3950.650416	24.510029
145.738094	3952.742552	24.515047
145.657016	3980.220624	24.520064
146.139581	3984.839992	24.525082
146.281973	3991.230803	24.530099
146.181706	3990.166908	24.535117
146.186880	3993.612446	24.540135
146.228083	4008.665991	24.545152
146.532121	4025.122680	24.550170
146.682273	4034.466845	24.555187
146.577811	4047.113761	24.560205
147.229521	4040.635957	24.565223
147.041565	4048.618895	24.570240
147.490548	4055.093004	24.575258
147.780709	4077.869385	24.580275
147.692097	4075.080119	24.585293
148.194987	4080.789693	24.590311
147.935787	4080.255362	24.595328
148.243973	4080.625654	24.600346
148.384775	4102.913791	24.605363
148.391075	4103.428186	24.610381
148.936922	4096.769006	24.615399
148.620595	4108.007858	24.620416
148.844422	4125.866642	24.625434
149.090011	4125.463430	24.630451
149.026404	4131.372688	24.635469
149.621729	4138.016227	24.640487
149.885649	4157.651169	24.645504
150.471234	4154.540430	24.650522
150.431834	4142.159739	24.655539
150.429868	4152.746730	24.660557
150.578247	4148.847481	24.665575
150.712646	4155.096470	24.670592
150.638716	4142.319315	24.675610
151.004006	4149.348802	24.680627
150.838459	4160.148311	24.685645
150.841588	4144.626099	24.690663
150.714115	4168.841098	24.695680
150.999531	4169.395950	24.700698
151.318968	4176.022923	24.705715
151.183935	4199.432091	24.710733
151.624099	4202.127883	24.715751
151.620624	4200.287862	24.720768
151.851493	4216.066552	24.725786
152.470846	4215.746914	24.730803
152.462308	4215.449508	24.735821
152.795514	4225.740041	24.740839
152.560515	4227.752913	24.745856
153.090205	4217.403776	24.750874
153.182120	4207.115003	24.755891
152.884346	4229.458313	24.760909
152.918401	4241.859906	24.765927
153.324694	4243.167182	24.770944
153.227064	4256.489699	24.775962
153.356305	4263.202101	24.780979
153.663229	4265.505376	24.785997
153.680479	4278.850502	24.791015
153.688924	4285.922790	24.796032
153.982489	4297.432695	24.801050
154.262806	4306.949796	24.806067
153.942013	4312.676725	24.811085
154.574401	4312.237798	24.816103
154.964743	4330.365275	24.821120
155.212596	4333.905143	24.826138
155.217389	4330.573884	24.831155
155.128679	4332.829332	24.836173
155.513670	4317.384503	24.841191
155.322183	4339.281526	24.846208
155.650061	4352.750256	24.851226
156.111204	4354.331990	24.856243
155.933331	4362.954606	24.861261
155.960735	4365.820862	24.866279
156.333449	4383.692409	24.871296
156.480798	4387.493749	24.876314
156.372227	4392.870641	24.881331
156.484814	4396.624820	24.886349
157.120911	4410.199431	24.891367
157.417240	4417.534249	24.896384
157.254241	4425.687261	24.901402
157.760572	4427.464755	24.906419
158.124323	4423.372193	24.911437
157.613540	4421.484803	24.916455
157.781985	4421.522608	24.921472
157.763292	4445.192878	24.926490
158.141231	4446.573133	24.931507
158.265776	4453.054309	24.936525
158.459501	4466.282578	24.941543
158.746048	4476.183469	24.946560
158.612634	4467.705126	24.951578
158.753626	4486.046401	24.956595
158.892353	4504.142624	24.961613
159.374188	4497.682268	24.966631
159.461890	4503.591152	24.971648
159.938170	4521.490408	24.976666
159.856701	4533.611738	24.981683
159.685833	4543.874304	24.986701
160.268020	4528.814742	24.991719
160.181804	4533.417987	24.996736
160.530020	4544.290837	25.001754
160.833307	4549.677641	25.006771
160.704537	4550.097161	25.011789
161.050603	4559.326255	25.016807
160.785059	4552.425722	25.021824
161.011469	4578.664107	25.026842
161.702551	4580.072329	25.031859
161.548883	4585.114285	25.036877
161.936340	4585.577368	25.041895
161.784649	4592.526656	25.046912
161.733590	4606.385645	25.051930
162.515008	4607.017982	25.056947
162.215491	4611.128983	25.061965
162.367506	4605.418933	25.066983
162.526714	4618.235126	25.072000
162.739039	4641.299339	25.077018
162.887610	4640.807744	25.082035
162.941335	4646.706369	25.087053
162.965936	4652.595480	25.092071
163.433444	4660.510432	25.097088
163.120073	4672.122119	25.102106
163.567729	4667.205852	25.107123
163.608514	4684.127693	25.112141
163.512061	4695.655254	25.117159
163.850605	4696.675231	25.122176
163.852067	4725.364013	25.127194
164.040892	4727.638205	25.132211
164.282106	4736.360209	25.137229
164.838496	4751.834272	25.142247
165.114209	4751.198897	25.147264
165.141074	4767.146013	25.152282
165.489644	4772.598054	25.157299
165.615722	4785.349662	25.162317
165.789534	4789.531569	25.167335
166.050696	4776.616263	25.172352
166.417843	4774.768214	25.177370
166.367765	4782.235539	25.182387
166.448638	4788.690000	25.187405
166.577400	4802.280571	25.192423
167.168364	4805.846093	25.197440
166.821927	4808.693371	25.202458
167.065290	4804.358726	25.207475
167.369817	4804.211209	25.212493
167.364085	4831.538835	25.217511
167.667066	4826.378900	25.222528
167.690001	4837.245615	25.227546
167.828753	4829.571702	25.232563
168.023727	4849.511994	25.237581
168.310536	4855.371182	25.242599
168.439155	4866.729260	25.247616
168.343226	4865.195751	25.252634
168.772343	4872.456922	25.257651
168.965110	4885.935098	25.262669
168.994239	4904.581866	25.267687
169.344943	4898.235073	25.272704
169.172325	4906.226255	25.277722
169.329970	4918.971374	25.282739
169.541938	4934.012017	25.287757
169.444874	4936.649639	25.292775
170.005894	4926.752074	25.297792
170.077940	4964.976384	25.302810
170.307241	4961.112008	25.307827
170.121641	4960.571413	25.312845
170.471171	4973.171917	25.317863
171.167485	4978.991828	25.322880
170.855178	4977.928625	25.327898
170.968094	4984.881538	25.332915
171.306769	5005.350593	25.337933
171.415611	5011.121789	25.342951
171.490467	5008.304708	25.347968
171.523357	5015.124859	25.352986
171.737205	5031.000757	25.358003
172.345922	5037.131236	25.363021
172.024818	5048.166239	25.368039
172.311706	5046.561452	25.373056
172.532470	5062.995613	25.378074
172.723476	5068.116518	25.383091
173.113519	5069.616843	25.388109
173.030457	5071.880155	25.393127
173.462747	5079.261287	25.398144
173.629603	5098.902740	25.403162
173.570319	5101.923777	25.408179
173.620631	5093.381953	25.413197
173.703388	5116.607600	25.418215
174.334718	5110.561332	25.423232
174.242171	5122.289209	25.428250
174.442823	5132.417432	25.433267
174.599485	5145.435884	25.438285
174.421320	5152.012832	25.443303
174.804337	5165.391705	25.448320
174.927125	5188.047027	25.453338
175.423036	5176.291289	25.458355
175.487921	5187.359260	25.463373
175.508454	5207.999683	25.468391
175.978525	5212.101438	25.473408
176.163228	5209.612950	25.478426
176.297090	5233.884014	25.483443
176.316052	5234.833044	25.488461
176.398256	5238.054186	25.493479
176.904822	5248.173052	25.498496
176.964658	5265.667598	25.503514
176.856631	5268.967063	25.508531
177.211563	5274.637767	25.513549
177.125981	5291.751166	25.518567
177.590716	5294.137226	25.523584
177.665498	5298.796071	25.528602
177.966517	5323.620428	25.533619
178.331354	5326.550294	25.538637
178.189935	5330.168989	25.543655
178.797702	5336.559358	25.548672
178.440077	5355.084269	25.553690
178.660002	5358.092313	25.558707
179.453222	5360.617183	25.563725
179.288639	5374.806527	25.568743
179.618971	5390.784608	25.573760
179.927071	5387.721795	25.578778
179.999775	5373.458501	25.583795
179.906812	5391.942837	25.588813
179.934505	5409.092595	25.593831
180.382422	5405.094127	25.598848
180.227172	5410.046932	25.603866
180.672024	5422.955962	25.608883
181.052774	5437.347145	25.613901
181.067070	5438.008999	25.618919
181.315772	5440.339055	25.623936
181.405262	5449.693795	25.628954
181.302202	5450.367279	25.633971
181.762605	5458.113872	25.638989
181.927664	5473.138159	25.644007
182.223617	5457.832996	25.649024
182.146720	5480.175239	25.654042
182.253602	5497.513873	25.659059
182.524316	5491.019879	25.664077
182.592028	5490.453825	25.669095
182.839414	5505.818251	25.674112
183.112591	5515.216126	25.679130
183.306763	5519.240802	25.684148
183.738666	5530.940463	25.689165
183.552604	5544.558310	25.694183
184.104796	5561.617548	25.699200
184.228736	5556.791148	25.704218
184.366950	5558.540939	25.709236
184.940188	5570.694059	25.714253
184.506223	5579.784608	25.719271
184.912080	5579.451005	25.724288
185.058440	5578.668651	25.729306
184.863641	5592.033040	25.734324
185.154320	5598.216036	25.739341
185.210179	5605.801416	25.744359
185.274892	5619.591764	25.749376
185.705491	5639.409025	25.754394
185.530433	5644.933860	25.759412
186.092365	5661.962553	25.764429
186.376178	5671.195982	25.769447
186.351904	5693.512065	25.774464
186.712637	5692.885915	25.779482
186.989446	5701.697226	25.784500
186.970174	5720.112008	25.789517
187.165384	5726.252061	25.794535
187.512700	5727.564950	25.799552
188.018383	5741.541582	25.804570
188.038565	5756.586894	25.809588
188.546413	5757.476113	25.814605
188.811101	5746.643422	25.819623
188.707303	5752.104225	25.824640
188.631468	5759.344068	25.829658
188.992260	5772.127559	25.834676
189.783676	5761.540520	25.839693
189.733992	5773.302990	25.844711
189.921716	5760.136557	25.849728
190.126627	5756.490639	25.854746
189.994777	5771.343069	25.859764
190.691161	5766.180672	25.864781
190.731689	5783.508979	25.869799
190.709189	5783.515868	25.874816
191.084996	5776.009794	25.879834
191.000364	5780.634415	25.884852
191.311018	5772.515647	25.889869
191.131935	5787.807534	25.894887
191.391007	5776.907270	25.899904
191.642143	5787.842154	25.904922
191.588595	5801.780549	25.909940
192.051491	5797.220231	25.914957
191.957493	5817.261402	25.919975
191.763312	5805.147083	25.924992
192.003288	5836.671544	25.930010
192.168489	5835.562044	25.935028
192.361934	5867.688752	25.940045
192.562173	5873.581033	25.945063
193.008363	5875.943402	25.950080
193.446197	5897.101227	25.955098
193.098957	5905.962584	25.960116
193.501457	5914.434575	25.965133
193.504905	5931.536095	25.970151
193.505687	5940.412797	25.975168
193.694100	5954.415037	25.980186
194.318044	5964.611671	25.985204
195.078381	5979.089205	25.990221
194.830075	5999.920712	25.995239
195.105465	5991.288203	26.000256
195.638046	5987.855907	26.005274
195.708061	6000.980978	26.010292
196.064395	6004.606239	26.015309
196.009909	6012.604360	26.020327
196.012813	6012.135159	26.025344
196.379286	6026.153925	26.030362
196.481174	6042.493270	26.035380
196.624413	6040.327523	26.040397
196.778018	6043.306160	26.045415
197.087419	6061.633568	26.050432
197.631090	6064.712092	26.055450
197.375362	6063.671253	26.060468
197.602779	6088.488967	26.065485
197.671808	6078.581746	26.070503
197.869188	6092.496147	26.075520
198.332812	6110.168852	26.080538
198.122521	6123.675443	26.085556
198.830697	6122.786190	26.090573
198.746729	6133.755872	26.095591
198.781905	6162.877144	26.100608
199.380832	6155.830171	26.105626
199.367491	6161.578027	26.110644
199.668584	6175.334359	26.115661
199.582073	6190.155592	26.120679
199.863239	6199.766627	26.125696
200.294152	6209.371105	26.130714
200.554354	6222.540794	26.135732
200.929420	6222.332463	26.140749
200.748626	6220.574743	26.145767
201.019620	6240.695194	26.150784
201.637095	6242.352143	26.155802
201.194230	6255.031296	26.160820
201.326168	6244.243007	26.165837
201.924479	6272.484829	26.170855
201.889097	6285.873208	26.175872
202.025990	6279.842358	26.180890
201.984669	6292.418979	26.185908
202.640425	6296.174385	26.190925
202.381492	6313.465297	26.195943
202.627407	6317.627494	26.200960
203.313643	6336.529291	26.205978
203.549288	6345.216952	26.210996
203.394974	6348.709708	26.216013
203.629396	6360.476919	26.221031
203.785732	6365.462192	26.226048
204.370163	6360.789494	26.231066
204.130595	6381.847516	26.236084
204.382878	6398.441790	26.241101
204.541727	6404.525770	26.246119
204.376620	6421.917505	26.251136
204.605041	6439.100974	26.256154
204.899249	6451.042828	26.261172
205.129445	6467.992381	26.266189
205.971442	6472.899069	26.271207
206.262200	6486.394562	26.276224
206.234704	6497.645037	26.281242
206.132118	6501.250744	26.286260
206.479502	6508.668954	26.291277
207.115429	6504.484449	26.296295
206.882208	6520.823457	26.301312
207.390629	6514.824550	26.306330
207.371426	6538.038792	26.311348
207.548703	6549.321964	26.316365
207.534588	6556.243159	26.321383
208.015278	6567.735248	26.326400
208.417151	6572.322685	26.331418
207.982436	6597.147675	26.336436
208.527443	6609.311669	26.341453
208.686826	6615.820505	26.346471
208.900475	6639.453323	26.351488
209.555970	6624.035357	26.356506
209.691539	6629.834399	26.361524
210.007775	6647.668144	26.366541
210.173768	6657.656605	26.371559
210.297471	6661.811633	26.376576
210.469710	6653.751429	26.381594
210.799324	6680.752864	26.386612
211.100854	6692.661489	26.391629
211.428372	6683.593840	26.396647
211.319833	6699.891927	26.401664
211.893342	6675.023708	26.406682
211.910289	6692.525208	26.411700
211.870743	6701.181419	26.416717
212.247186	6714.881398	26.421735
211.968590	6712.876427	26.426752
212.184864	6720.277093	26.431770
212.341925	6740.123709	26.436788
212.430674	6748.181218	26.441805
213.036624	6748.984845	26.446823
213.096500	6766.448906	26.451840
213.212076	6763.296917	26.456858
213.156156	6788.175923	26.461876
213.432520	6800.201943	26.466893
213.744153	6816.437898	26.471911
213.821338	6832.206920	26.476928
214.319776	6831.561926	26.481946
214.424613	6859.401245	26.486964
214.736656	6867.660830	26.491981
215.195017	6875.004100	26.496999
214.987471	6889.217476	26.502016
215.487997	6896.455688	26.507034
215.341022	6915.790032	26.512052
215.760043	6915.282793	26.517069
215.925136	6936.458839	26.522087
216.029892	6944.797932	26.527104
216.496739	6944.197309	26.532122
216.475344	6973.185212	26.537140
216.737708	6984.356018	26.542157
217.163351	6994.673892	26.547175
217.038948	7011.697119	26.552192
217.762983	7020.053979	26.557210
217.896502	7046.143982	26.562228
218.040072	7033.701011	26.567245
218.515317	7046.144783	26.572263
218.888550	7070.872452	26.577280
219.519380	7067.141799	26.582298
219.461414	7069.359714	26.587316
219.198506	7064.413532	26.592333
219.729238	7059.026909	26.597351
219.696949	7081.216541	26.602368
220.070651	7075.799869	26.607386
220.574850	7097.127442	26.612404
220.710600	7090.404070	26.617421
220.519104	7102.364869	26.622439
220.677799	7108.714314	26.627456
221.293449	7108.372424	26.632474
221.278218	7132.927658	26.637492
221.052804	7149.667377	26.642509
221.758288	7151.821826	26.647527
221.470901	7176.596758	26.652544
221.617900	7179.815866	26.657562
221.939686	7201.551903	26.662580
222.056165	7217.895728	26.667597
222.426398	7232.465017	26.672615
222.816950	7250.595282	26.677632
223.222248	7256.197361	26.682650
223.624004	7278.207944	26.687668
223.606010	7277.509929	26.692685
224.236721	7282.582761	26.697703
224.300191	7297.063324	26.702720
224.246666	7303.588307	26.707738
224.623208	7293.888539	26.712756
224.944077	7297.400185	26.717773
224.934849	7306.725418	26.722791
225.159519	7332.103501	26.727808
225.539949	7336.143836	26.732826
225.500615	7343.247235	26.737844
225.495154	7354.224974	26.742861
225.991434	7370.412434	26.747879
225.797219	7379.121233	26.752896
225.927064	7392.393002	26.757914
226.314124	7410.923719	26.762932
226.585056	7426.316293	26.767949
226.884112	7418.726430	26.772967
226.751374	7443.457483	26.777984
227.089573	7461.198226	26.783002
227.426679	7480.596190	26.788020
227.615212	7494.495226	26.793037
228.087803	7511.014718	26.798055
228.207515	7521.243250	26.803072
228.360993	7540.416423	26.808090
228.668037	7555.075571	26.813108
229.014206	7559.521131	26.818125
229.454921	7580.185220	26.823143
229.633142	7598.672354	26.828160
229.855174	7602.301328	26.833178
230.310153	7611.170361	26.838196
230.131509	7623.264074	26.843213
230.507710	7622.695189	26.848231
230.784394	7647.787774	26.853248
231.133931	7647.139736	26.858266
231.536981	7656.187814	26.863284
231.457616	7665.058654	26.868301
231.705268	7671.582211	26.873319
232.235517	7689.085680	26.878336
232.425197	7702.485096	26.883354
232.667465	7709.806581	26.888372
232.714026	7713.113417	26.893389
232.838088	7711.849827	26.898407
233.092399	7730.368272	26.903424
233.552597	7741.161126	26.908442
233.808687	7739.811969	26.913460
233.882310	7756.090830	26.918477
234.381074	7768.564512	26.923495
234.825587	7762.648475	26.928512
234.880184	7764.820224	26.933530
235.117522	7772.259764	26.938548
234.962821	7784.867523	26.943565
235.418652	7776.527034	26.948583
235.647114	7793.735677	26.953600
235.729519	7815.111851	26.958618
235.933613	7821.400075	26.963636
235.859349	7838.486283	26.968653
236.210149	7838.399047	26.973671
235.998263	7867.725923	26.978688
236.534814	7879.387960	26.983706
236.693570	7883.221437	26.988724
236.783660	7902.768700	26.993741
237.261641	7909.946488	26.998759
237.705998	7917.775632	27.003776
237.630022	7931.320676	27.008794
238.209958	7938.597105	27.013812
238.371582	7961.396837	27.018829
238.654705	7955.904590	27.023847
238.599876	7970.532134	27.028864
239.000661	7987.955092	27.033882
239.495751	7986.397073	27.038900
239.441785	8000.942678	27.043917
239.780237	8014.671166	27.048935
239.769234	8029.139921	27.053952
239.950079	8044.900790	27.058970
240.517522	8052.720614	27.063988
240.615036	8073.292566	27.069005
240.842621	8086.936503	27.074023
241.092138	8096.796170	27.079040
241.160128	8115.482492	27.084058
241.603643	8116.020182	27.089076
241.944162	8133.987187	27.094093
242.196776	8136.703399	27.099111
242.658709	8143.690296	27.104128
242.827258	8167.047901	27.109146
242.996315	8177.367376	27.114164
243.034387	8194.768923	27.119181
243.338146	8197.283428	27.124199
243.596963	8207.779821	27.129216
243.867782	8225.855617	27.134234
244.227050	8231.373346	27.139252
244.222877	8247.761142	27.144269
244.651659	8259.596455	27.149287
244.857301	8274.602171	27.154304
244.398367	8294.231167	27.159322
245.203336	8312.693251	27.164340
245.670877	8327.148177	27.169357
245.929697	8347.462279	27.174375
246.006310	8354.316343	27.179392
245.923075	8372.719432	27.184410
246.473232	8378.553007	27.189428
246.797569	8402.655697	27.194445
247.215801	8407.179732	27.199463
247.567248	8422.107275	27.204480
247.416144	8436.605052	27.209498
248.047576	8437.082115	27.214516
247.998791	8457.269142	27.219533
248.278844	8462.594213	27.224551
248.641384	8482.803839	27.229568
248.395737	8493.323404	27.234586
248.970534	8491.285234	27.239604
249.527481	8522.429681	27.244621
249.628674	8523.941802	27.249639
249.803859	8527.445492	27.254656
250.111597	8555.855240	27.259674
250.255376	8554.187135	27.264692
250.503811	8558.352716	27.269709
251.079368	8573.579109	27.274727
251.397101	8594.211495	27.279744
251.248104	8585.880412	27.284762
251.679048	8582.207225	27.289780
251.458376	8614.996049	27.294797
251.330583	8619.932162	27.299815
251.845367	8632.774638	27.304832
251.725274	8655.489717	27.309850
252.408894	8682.437584	27.314868
252.344397	8701.890143	27.319885
252.674805	8713.137966	27.324903
253.117027	8742.686490	27.329920
253.516612	8752.182741	27.334938
253.983352	8759.310803	27.339956
254.184176	8775.506767	27.344973
254.230816	8786.066504	27.349991
254.523719	8808.751396	27.355008
254.400599	8817.644057	27.360026
254.901071	8826.426311	27.365044
255.308149	8850.342637	27.370061
255.681274	8869.268480	27.375079
255.892859	8871.616811	27.380096
256.307769	8891.034119	27.385114
256.817519	8888.223316	27.390132
256.872662	8912.894201	27.395149
256.849974	8920.528027	27.400167
257.629557	8924.815214	27.405184
257.557861	8942.901230	27.410202
258.023698	8944.058222	27.415220
258.387922	8967.893830	27.420237
258.525206	8972.401050	27.425255
259.116715	8975.783011	27.430272
258.903655	8994.565987	27.435290
259.600182	8994.657352	27.440308
259.559369	9003.986321	27.445325
259.703024	9006.204254	27.450343
260.144926	9031.368053	27.455360
260.207236	9043.956054	27.460378
260.197007	9057.251242	27.465396
260.402314	9066.668497	27.470413
260.689729	9092.783199	27.475431
260.949685	9101.607494	27.480448
261.059066	9121.402726	27.485466
261.364172	9139.120062	27.490484
261.701988	9158.810472	27.495501
261.734945	9171.702281	27.500519
262.578388	9200.748279	27.505536
262.522870	9210.270937	27.510554
262.889135	9210.174154	27.515572
263.179838	9233.770491	27.520589
263.257897	9249.491574	27.525607
263.899603	9248.018265	27.530624
263.964594	9273.724135	27.535642
264.525594	9290.240571	27.540660
264.514830	9296.984270	27.545677
264.510738	9302.208177	27.550695
265.075999	9307.364156	27.555712
265.180350	9323.742917	27.560730
265.708993	9326.715953	27.565748
265.652912	9346.906523	27.570765
265.771610	9346.455745	27.575783
266.699762	9346.585742	27.580800
267.332467	9362.455005	27.585818
267.696099	9359.007583	27.590836
268.016260	9351.484206	27.595853
268.170446	9347.575990	27.600871
268.170719	9360.909907	27.605888
268.340628	9360.174761	27.610906
268.576830	9379.247410	27.615924
268.885700	9390.060869	27.620941
268.614727	9379.999476	27.625959
269.071029	9395.663967	27.630976
269.210265	9418.090598	27.635994
269.491821	9422.436463	27.641012
270.004260	9438.944279	27.646029
270.198437	9450.525600	27.651047
270.680961	9463.279117	27.656064
270.538796	9474.011079	27.661082
271.075912	9477.676463	27.666100
271.210753	9499.404348	27.671117
271.046531	9515.331547	27.676135
271.915298	9526.963183	27.681152
271.702175	9543.358949	27.686170
272.048960	9561.773258	27.691188
272.530014	9568.175464	27.696205
272.675501	9578.683415	27.701223
272.916899	9588.666946	27.706240
273.596074	9609.028300	27.711258
273.999217	9621.820181	27.716276
274.159222	9632.421466	27.721293
274.484976	9647.125341	27.726311
274.833001	9640.357549	27.731328
274.949585	9660.303043	27.736346
275.252459	9664.273366	27.741364
275.759944	9684.639761	27.746381
275.765076	9683.250958	27.751399
275.949753	9690.832452	27.756416
276.329069	9705.379118	27.761434
276.657598	9720.795187	27.766452
277.075803	9732.868657	27.771469
277.020345	9749.655410	27.776487
277.315669	9738.075235	27.781504
277.504053	9773.175958	27.786522
277.695483	9777.892773	27.791540
278.183869	9792.853772	27.796557
277.989146	9808.350970	27.801575
278.221641	9819.569595	27.806592
278.452264	9836.077915	27.811610
278.498857	9850.406654	27.816628
278.931386	9870.238722	27.821645
278.897164	9896.570565	27.826663
279.489380	9896.568402	27.831680
279.784375	9922.310339	27.836698
280.042595	9941.188182	27.841716
280.803701	9951.595520	27.846733
280.483046	9976.273361	27.851751
280.826062	9989.391493	27.856768
281.272316	10015.438423	27.861786
281.597273	10014.196925	27.866804
281.962131	10034.721492	27.871821
282.227182	10057.981684	27.876839
282.464811	10065.114239	27.881856
282.814939	10082.190453	27.886874
283.328965	10097.602528	27.891892
283.775235	10113.821813	27.896909
283.881685	10124.591341	27.901927
284.295425	10136.103573	27.906944
284.371607	10147.327684	27.911962
284.761000	10147.871730	27.916980
285.136756	10171.533901	27.921997
285.443551	10183.098627	27.927015
286.052003	10187.995423	27.932032
285.934317	10199.657328	27.937050
285.954089	10205.539576	27.942068
286.134258	10226.109974	27.947085
286.687423	10237.465493	27.952103
286.874415	10252.609168	27.957120
287.083782	10271.895776	27.962138
287.181444	10291.075873	27.967156
287.788522	10295.612497	27.972173
288.030936	10328.647615	27.977191
288.021149	10333.908596	27.982208
288.423687	10356.278139	27.987226
288.389220	10376.843212	27.992244
288.896750	10391.086804	27.997261
289.040045	10415.989680	28.002279
289.531170	10428.093013	28.007296
289.991791	10448.373484	28.012314
290.385888	10471.271027	28.017332
290.992240	10485.521781	28.022349
290.725669	10507.988751	28.027367
291.370083	10514.891423	28.032384
292.050707	10519.706788	28.037402
291.538200	10544.166665	28.042420
292.747608	10557.797251	28.047437
292.474638	10559.273597	28.052455
292.708482	10573.397294	28.057472
293.011233	10589.891408	28.062490
293.632858	10608.020421	28.067508
294.192349	10608.613714	28.072525
294.011375	10615.517739	28.077543
294.519334	10629.144501	28.082560
294.492340	10638.384928	28.087578
294.683040	10660.201996	28.092596
294.874206	10671.494348	28.097613
295.028241	10685.045356	28.102631
295.199424	10705.751631	28.107648
295.653325	10720.291334	28.112666
295.803964	10732.852116	28.117684
296.001373	10745.733627	28.122701
296.661658	10764.220255	28.127719
297.208816	10776.156365	28.132736
297.592963	10788.388400	28.137754
297.625833	10792.837656	28.142772
297.799554	10806.023623	28.147789
297.884243	10826.462502	28.152807
298.649092	10831.360166	28.157824
299.058649	10849.284027	28.162842
299.092315	10859.891759	28.167860
299.523937	10871.386756	28.172877
299.559932	10894.422685	28.177895
300.005142	10911.106149	28.182912
300.229463	10927.406943	28.187930
300.303012	10934.044288	28.192948
300.806064	10947.781909	28.197965
301.071404	10969.438789	28.202983
301.111671	10995.820889	28.208000
301.528090	11009.496822	28.213018
301.936773	11034.896340	28.218036
302.165827	11050.167512	28.223053
302.286204	11077.907547	28.228071
302.299496	11098.521870	28.233088
303.132563	11111.789147	28.238106
303.244053	11128.450094	28.243124
303.854922	11150.678228	28.248141
304.216344	11172.826918	28.253159
304.452593	11178.431073	28.258176
304.851712	11196.241717	28.263194
305.096340	11225.973812	28.268212
305.674306	11233.016875	28.273229
305.983413	11249.747592	28.278247
306.338477	11264.354338	28.283264
306.414487	11267.269272	28.288282
306.448776	11294.119937	28.293300
306.925148	11304.130521	28.298317
307.284496	11324.524728	28.303335
307.719157	11346.188023	28.308352
308.226107	11350.380875	28.313370
308.152864	11362.184553	28.318388
308.631525	11373.645289	28.323405
308.947839	11399.106971	28.328423
308.682708	11414.429727	28.333440
309.247552	11416.830381	28.338458
309.452450	11444.173555	28.343476
309.976088	11462.370379	28.348493
310.162429	11481.009768	28.353511
310.277583	11498.265135	28.358528
310.786677	11516.409250	28.363546
311.137466	11541.196708	28.368564
311.576788	11549.680237	28.373581
311.455640	11561.643601	28.378599
312.161439	11578.803354	28.383616
312.347918	11605.830224	28.388634
312.654237	11616.990422	28.393652
312.950836	11636.741032	28.398669
313.419716	11643.410522	28.403687
313.593799	11656.080098	28.408704
313.992375	11674.759097	28.413722
314.292615	11687.770628	28.418740
314.961715	11686.908992	28.423757
315.058813	11710.662466	28.428775
315.222070	11733.601478	28.433792
315.483146	11737.215803	28.438810
315.486497	11766.759571	28.443828
316.132388	11790.025108	28.448845
316.254175	11813.196336	28.453863
316.757474	11818.062429	28.458880
317.137805	11834.940247	28.463898
316.898373	11851.807851	28.468916
317.578857	11858.269385	28.473933
318.109818	11891.199377	28.478951
318.495125	11906.681056	28.483968
318.974518	11917.094143	28.488986
319.195043	11929.377585	28.494004
319.550186	11950.059402	28.499021
319.852207	11966.530353	28.504039
320.104463	11979.841779	28.509056
320.393011	11993.404797	28.514074
320.532173	12013.580419	28.519092
320.585846	12020.891189	28.524109
321.033467	12047.538407	28.529127
321.002078	12084.300477	28.534144
321.787138	12112.796735	28.539162
321.832575	12131.358247	28.544180
322.125905	12162.233134	28.549197
322.220197	12175.517567	28.554215
322.664650	12195.926152	28.559232
323.235936	12218.120854	28.564250
323.733673	12254.779926	28.569268
323.860555	12261.651181	28.574285
324.755803	12277.899247	28.579303
324.971920	12298.104305	28.584320
325.183205	12318.267264	28.589338
325.469622	12337.533222	28.594356
325.674116	12345.889146	28.599373
326.290594	12370.834163	28.604391
326.448250	12383.868823	28.609408
327.034794	12396.475847	28.614426
327.079815	12420.582291	28.619444
327.386723	12441.951907	28.624461
327.773741	12448.747553	28.629479
327.916008	12474.053037	28.634496
328.421752	12485.104965	28.639514
328.696031	12506.814379	28.644532
329.268588	12516.075909	28.649549
329.448660	12534.437203	28.654567
329.470043	12555.076818	28.659584
330.070975	12554.499121	28.664602
329.913627	12585.684785	28.669620
330.313189	12602.948233	28.674637
330.746414	12613.405171	28.679655
330.697993	12645.280987	28.684672
331.302753	12656.098256	28.689690
331.922031	12687.889990	28.694708
332.061897	12705.792929	28.699725
332.627029	12721.418766	28.704743
332.838735	12733.596831	28.709760
333.443348	12744.652872	28.714778
333.519325	12773.423357	28.719796
333.670214	12786.904541	28.724813
334.317502	12813.105117	28.729831
334.188802	12825.431364	28.734848
335.174803	12836.874156	28.739866
335.230320	12848.766303	28.744884
335.610832	12869.137976	28.749901
335.796550	12885.097766	28.754919
336.332818	12913.788868	28.759936
336.925328	12926.020138	28.764954
336.759820	12946.232371	28.769972
337.032909	12969.771855	28.774989
337.874868	12979.732778	28.780007
337.635488	13009.970549	28.785024
338.160794	13031.957718	28.790042
338.444607	13050.302712	28.795060
338.578709	13068.356350	28.800077
339.078855	13086.726142	28.805095
339.162227	13112.893332	28.810112
339.632044	13119.516502	28.815130
340.020302	13153.955488	28.820148
340.234236	13184.877384	28.825165
340.786699	13208.703698	28.830183
341.169312	13225.917625	28.835200
341.604626	13236.948272	28.840218
341.960520	13275.005736	28.845236
342.595811	13287.528012	28.850253
342.948104	13299.122916	28.855271
343.027392	13316.748932	28.860288
343.427735	13346.397413	28.865306
343.713968	13352.500533	28.870324
343.862202	13383.529725	28.875341
344.495568	13390.388473	28.880359
344.602871	13438.006780	28.885376
345.180852	13440.387972	28.890394
345.589123	13453.124847	28.895412
345.826852	13472.563337	28.900429
346.428220	13503.363729	28.905447
346.563460	13516.023146	28.910464
347.217346	13521.277668	28.915482
347.319629	13544.584330	28.920500
347.543402	13558.163406	28.925517
348.079132	13557.051182	28.930535
348.331269	13590.274696	28.935552
348.336987	13594.138361	28.940570
348.766030	13620.846412	28.945588
348.855403	13635.475756	28.950605
348.954848	13656.946464	28.955623
349.268164	13676.056347	28.960640
349.992178	13702.772242	28.965658
350.635339	13730.443274	28.970676
350.321516	13758.025204	28.975693
351.068862	13772.726149	28.980711
351.395405	13803.728178	28.985728
351.834158	13814.512520	28.990746
352.275343	13836.350144	28.995764
352.164191	13850.302729	29.000781
352.664463	13874.704069	29.005799
353.109367	13894.593490	29.010816
353.334004	13910.562915	29.015834
353.732102	13935.068402	29.020852
353.796385	13971.756818	29.025869
354.315995	14001.247951	29.030887
354.939830	14028.766258	29.035904
355.022338	14050.120177	29.040922
355.607899	14064.417696	29.045940
356.294739	14082.435919	29.050957
356.850682	14104.780380	29.055975
357.204246	14130.473720	29.060992
357.755019	14144.695388	29.066010
358.433169	14150.111275	29.071028
358.460738	14173.667643	29.076045
358.642367	14181.140799	29.081063
358.840969	14203.418273	29.086080
359.210134	14212.850426	29.091098
359.427939	14236.731120	29.096116
359.689633	14264.106540	29.101133
360.203586	14287.471044	29.106151
360.453570	14310.488295	29.111168
361.009850	14327.439354	29.116186
361.320120	14341.387616	29.121204
361.348847	14373.015453	29.126221
361.723337	14381.758482	29.131239
362.070725	14410.691016	29.136256
362.433929	14451.270689	29.141274
362.620700	14460.785196	29.146292
362.902486	14476.148346	29.151309
364.090878	14505.454776	29.156327
363.998659	14542.281477	29.161344
364.142229	14557.085401	29.166362
364.990987	14576.663990	29.171380
364.820054	14611.185935	29.176397
365.061035	14631.894722	29.181415
365.444596	14650.241496	29.186432
365.820591	14678.824997	29.191450
366.254966	14708.598432	29.196468
366.351191	14734.970043	29.201485
367.238951	14751.965383	29.206503
367.514271	14772.229340	29.211520
367.819732	14800.856288	29.216538
368.231458	14812.154275	29.221556
368.390186	14835.925936	29.226573
368.870877	14849.570021	29.231591
369.165961	14886.558611	29.236608
369.612307	14912.948341	29.241626
369.821012	14942.050007	29.246644
370.729360	14957.361132	29.251661
370.961026	14975.008670	29.256679
371.289549	15003.092498	29.261696
371.464278	15022.275552	29.266714
372.275212	15039.065205	29.271732
372.294912	15068.411914	29.276749
372.746645	15080.516419	29.281767
373.191759	15101.424851	29.286784
373.183137	15127.018666	29.291802
373.738425	15152.925325	29.296820
374.232464	15173.393192	29.301837
374.605700	15200.058982	29.306855
374.879538	15232.417268	29.311872
375.214166	15258.634793	29.316890
375.964901	15275.793173	29.321908
376.193555	15306.615968	29.326925
376.307408	15323.484735	29.331943
376.810081	15337.027353	29.336960
377.081700	15377.666884	29.341978
377.279604	15402.277382	29.346996
377.414081	15421.057500	29.352013
378.312321	15457.906392	29.357031
378.663181	15493.931179	29.362048
378.790226	15506.780226	29.367066
379.790656	15523.903331	29.372084
379.605128	15562.089577	29.377101
380.034107	15576.780029	29.382119
380.458117	15602.684851	29.387136
381.043409	15633.534135	29.392154
381.334605	15655.579627	29.397172
381.616261	15681.028722	29.402189
381.883465	15713.638243	29.407207
382.184094	15738.588744	29.412224
382.695104	15761.640884	29.417242
383.291475	15796.599025	29.422260
383.551798	15832.270800	29.427277
383.820949	15849.654567	29.432295
384.587494	15876.096199	29.437312
385.007686	15905.354050	29.442330
385.306717	15917.998807	29.447348
385.632446	15949.146336	29.452365
386.012314	15970.729419	29.457383
386.757499	15997.621333	29.462400
386.726026	16023.451242	29.467418
387.465591	16035.530522	29.472436
387.512971	16052.421508	29.477453
387.770302	16066.847905	29.482471
388.256792	16077.958573	29.487488
388.604661	16105.049197	29.492506
389.110198	16130.293513	29.497524
389.461582	16154.517933	29.502541
389.636797	16175.461787	29.507559
390.111251	16204.820403	29.512576
390.137443	16226.794788	29.517594
390.676316	16258.037208	29.522612
391.051933	16284.855367	29.527629
391.097075	16323.562953	29.532647
391.779399	16340.119362	29.537664
392.118739	16374.006572	29.542682
392.455305	16396.130629	29.547700
392.821852	16430.559604	29.552717
393.488691	16459.536140	29.557735
393.778956	16491.635646	29.562752
394.034259	16523.895491	29.567770
395.041483	16539.504619	29.572788
395.502670	16564.430880	29.577805
395.380823	16594.535156	29.582823
396.089294	16626.782648	29.587840
396.202933	16652.601905	29.592858
396.761386	16661.588155	29.597876
397.031482	16702.148767	29.602893
397.482869	16730.881050	29.607911
398.389382	16746.816828	29.612928
398.565665	16775.987463	29.617946
399.247147	16797.566264	29.622964
399.360789	16817.244497	29.627981
399.740832	16848.452213	29.632999
400.111141	16867.385967	29.638016
400.527980	16896.890698	29.643034
400.840361	16910.246852	29.648052
401.013444	16944.273014	29.653069
401.248275	16980.550947	29.658087
401.787125	16999.618226	29.663104
402.030034	17034.714040	29.668122
402.657719	17070.271793	29.673140
403.101680	17095.546108	29.678157
403.307315	17120.791320	29.683175
404.098282	17150.946689	29.688192
404.384199	17173.705849	29.693210
404.910451	17205.739325	29.698228
404.905560	17231.824278	29.703245
405.576247	17267.353393	29.708263
405.944244	17293.502842	29.713280
406.237232	17330.120523	29.718298
406.794866	17351.470254	29.723316
407.051511	17382.966010	29.728333
407.058623	17415.433193	29.733351
407.705708	17441.291008	29.738368
408.065670	17478.395764	29.743386
408.643246	17505.164680	29.748404
408.930203	17533.733732	29.753421
409.361850	17558.046088	29.758439
410.249689	17585.207010	29.763456
410.149692	17617.811949	29.768474
410.820937	17640.254716	29.773492
411.600359	17667.091155	29.778509
411.676972	17691.299474	29.783527
412.223013	17713.051720	29.788544
412.475610	17734.731075	29.793562
412.973660	17753.039508	29.798580
413.426660	17772.045248	29.803597
413.657413	17799.797822	29.808615
414.561672	17819.324594	29.813632
414.318680	17859.748752	29.818650
414.516420	17877.330625	29.823668
415.172744	17911.360263	29.828685
415.451273	17940.437284	29.833703
416.271835	17970.093904	29.838720
416.574786	18006.396853	29.843738
416.568570	18034.490539	29.848756
417.250563	18064.042653	29.853773
417.733650	18089.080288	29.858791
418.005198	18115.231931	29.863808
418.525765	18159.652136	29.868826
418.947500	18191.663172	29.873844
419.437498	18211.154481	29.878861
419.731386	18247.688171	29.883879
420.357417	18274.833167	29.888896
420.792197	18312.885841	29.893914
421.091099	18328.314982	29.898932
421.458588	18366.360399	29.903949
421.963807	18403.345808	29.908967
422.529886	18424.290968	29.913984
422.865322	18459.310707	29.919002
423.168699	18486.394493	29.924020
423.935668	18522.388901	29.929037
423.719206	18556.990897	29.934055
424.297780	18577.443340	29.939072
424.677820	18616.146018	29.944090
425.231823	18636.977645	29.949108
425.703574	18685.382664	29.954125
426.087161	18716.259930	29.959143
426.848328	18726.671384	29.964160
427.003448	18778.145220	29.969178
427.730001	18796.783837	29.974196
428.388692	18819.961617	29.979213
428.661484	18856.548920	29.984231
429.385792	18881.060036	29.989248
429.567812	18900.381992	29.994266
429.646071	18925.802803	29.999284
430.285715	18952.053904	30.004301
430.726404	18987.351767	30.009319
431.258727	19006.672375	30.014336
431.705858	19038.357095	30.019354
431.961587	19054.122581	30.024372
432.865329	19079.545199	30.029389
433.047472	19104.831640	30.034407
433.632910	19119.864732	30.039424
433.838383	19130.692559	30.044442
434.055361	19157.260564	30.049460
434.479391	19168.674473	30.054477
434.719415	19210.700609	30.059495
435.328773	19237.419627	30.064512
435.526696	19275.663977	30.069530
435.590859	19304.017253	30.074548
436.181879	19331.498431	30.079565
436.771764	19355.788008	30.084583
436.898945	19382.039984	30.089600
437.269099	19427.179537	30.094618
438.104546	19451.700624	30.099636
438.596203	19484.765432	30.104653
438.291904	19523.410493	30.109671
438.855531	19556.782898	30.114688
439.698178	19602.356365	30.119706
440.095414	19633.508096	30.124724
440.828963	19672.376780	30.129741
440.976828	19711.530219	30.134759
441.776464	19739.970668	30.139776
441.896960	19765.301469	30.144794
442.543605	19806.844721	30.149812
443.095718	19838.032426	30.154829
443.026126	19878.601329	30.159847
443.919460	19911.315235	30.164864
444.440092	19934.918279	30.169882
444.561655	19981.981847	30.174900
444.927975	20004.707550	30.179917
445.206617	20046.006504	30.184935
445.643465	20078.603709	30.189952
446.373883	20116.122714	30.194970
446.879974	20166.689245	30.199988
447.710490	20200.007516	30.205005
447.807491	20244.972462	30.210023
448.455848	20272.909595	30.215040
449.027869	20299.778920	30.220058
449.257971	20344.598132	30.225076
449.542204	20362.696449	30.230093
450.182743	20393.891259	30.235111
450.682612	20435.476894	30.240128
451.320044	20472.616651	30.245146
451.459719	20506.996917	30.250164
452.410543	20538.713117	30.255181
452.251444	20576.037897	30.260199
453.133488	20603.838383	30.265216
453.475327	20624.372978	30.270234
453.940235	20658.736806	30.275252
454.437034	20679.192055	30.280269
455.117412	20706.590552	30.285287
455.473649	20740.952580	30.290304
456.116149	20769.223466	30.295322
456.153544	20796.374512	30.300340
456.750671	20815.979209	30.305357
457.205483	20847.227352	30.310375
457.529147	20870.738375	30.315392
458.113775	20900.689403	30.320410
458.041290	20933.345122	30.325428
458.380831	20956.152864	30.330445
459.183470	20992.501688	30.335463
459.445185	21022.632364	30.340480
459.970182	21053.237761	30.345498
460.595193	21085.921674	30.350516
461.367408	21109.402155	30.355533
461.164376	21150.604354	30.360551
461.922003	21177.759842	30.365568
462.373809	21198.844291	30.370586
462.618643	21234.900990	30.375604
463.616180	21268.473325	30.380621
464.106479	21301.292553	30.385639
464.475121	21330.418838	30.390656
465.234595	21357.262877	30.395674
465.186870	21399.098571	30.400692
465.947810	21423.729537	30.405709
466.225602	21461.475875	30.410727
466.536727	21483.130060	30.415744
467.257656	21519.236391	30.420762
467.391631	21556.138792	30.425780
468.025408	21578.055934	30.430797
468.443833	21619.027264	30.435815
468.793257	21653.940901	30.440832
469.017897	21692.347558	30.445850
469.563575	21729.778587	30.450868
470.423643	21755.420456	30.455885
470.672654	21802.378615	30.460903
471.022958	21837.198012	30.465920
471.827367	21870.988270	30.470938
472.041102	21909.950057	30.475956
472.699947	21943.081638	30.480973
473.454472	21984.874566	30.485991
473.667440	22018.857806	30.491008
474.137648	22058.828921	30.496026
474.383109	22089.055982	30.501044
474.893749	22116.930932	30.506061
475.400270	22175.631146	30.511079
475.807049	22201.103384	30.516096
476.588231	22240.636363	30.521114
476.755906	22270.740702	30.526132
477.048740	22304.170773	30.531149
478.168220	22348.575617	30.536167
478.621605	22387.022348	30.541184
478.945220	22414.381828	30.546202
479.104655	22452.059612	30.551220
479.694352	22486.775366	30.556237
480.124759	22535.464697	30.561255
480.826158	22568.098576	30.566272
481.524838	22609.772898	30.571290
481.587627	22630.421517	30.576308
482.045291	22656.258916	30.581325
482.726583	22687.416363	30.586343
483.372891	22715.047084	30.591360
483.956196	22744.729339	30.596378
483.957679	22785.750433	30.601396
484.677813	22803.549000	30.606413
485.331359	22850.956991	30.611431
485.455760	22885.190911	30.616448
485.787131	22905.741973	30.621466
485.945992	22947.993071	30.626484
486.839901	22972.924272	30.631501
487.056102	23016.797553	30.636519
487.700533	23064.514017	30.641536
488.247225	23098.076242	30.646554
488.511128	23142.197459	30.651572
488.893945	23177.000459	30.656589
489.710500	23225.750124	30.661607
489.874277	23266.707231	30.666624
490.720559	23297.468632	30.671642
491.230145	23344.252034	30.676660
491.682737	23376.598783	30.681677
492.294869	23424.123784	30.686695
492.682806	23461.020113	30.691712
493.385241	23486.044064	30.696730
493.917299	23534.443034	30.701748
494.577189	23557.563862	30.706765
495.279178	23590.655806	30.711783
495.270214	23635.216469	30.716800
495.940334	23662.515038	30.721818
496.406150	23710.499772	30.726836
496.771699	23744.460055	30.731853
497.300231	23787.160960	30.736871
497.560988	23822.559018	30.741888
498.611899	23859.272690	30.746906
498.582668	23903.810555	30.751924
499.329781	23936.177695	30.756941
500.089833	23980.906686	30.761959
500.421481	24019.537463	30.766976
501.061833	24039.120795	30.771994
501.831333	24080.615220	30.777012
502.146564	24108.478345	30.782029
502.496744	24141.165124	30.787047
502.841979	24172.742148	30.792064
503.616135	24210.886228	30.797082
503.874314	24258.815113	30.802100
504.381693	24296.734087	30.807117
505.059832	24321.791589	30.812135
505.293673	24368.492761	30.817152
505.677939	24406.097632	30.822170
506.527282	24445.905691	30.827188
506.335485	24488.430996	30.832205
507.233779	24526.609624	30.837223
507.958821	24567.908396	30.842240
508.927790	24601.057599	30.847258
509.282330	24628.397864	30.852276
509.532709	24658.660558	30.857293
510.465248	24679.408822	30.862311
510.385838	24712.689808	30.867328
510.763003	24740.178686	30.872346
511.039977	24776.868107	30.877364
511.396704	24813.197533	30.882381
511.853583	24850.227108	30.887399
512.241217	24903.660667	30.892416
513.033287	24930.733258	30.897434
513.853970	24986.996080	30.902452
513.895844	25035.673058	30.907469
514.751967	25061.606095	30.912487
515.129491	25103.324748	30.917504
515.858642	25148.303779	30.922522
516.634596	25181.388840	30.927540
517.220603	25215.820503	30.932557
517.512891	25240.393454	30.937575
517.871963	25291.642217	30.942592
519.144418	25310.140212	30.947610
519.702866	25349.462797	30.952628
520.299243	25369.433677	30.957645
521.144536	25400.775156	30.962663
521.014097	25438.828381	30.967680
521.452959	25468.784522	30.972698
522.175729	25509.964793	30.977716
522.461713	25541.646924	30.982733
522.936192	25582.811003	30.987751
523.067211	25621.836833	30.992768
524.008811	25652.368640	30.997786
524.254799	25701.626420	31.002804
524.645389	25745.723652	31.007821
525.328931	25776.285772	31.012839
525.910690	25819.676086	31.017856
526.362587	25850.811702	31.022874
526.522211	25912.896633	31.027892
526.863588	25956.571385	31.032909
527.445345	25982.760746	31.037927
527.990125	26041.621202	31.042944
528.880409	26088.483596	31.047962
529.361393	26135.813080	31.052980
529.865867	26183.211437	31.057997
530.424710	26220.780176	31.063015
531.047511	26265.958910	31.068032
531.423036	26313.243482	31.073050
531.879954	26352.787955	31.078068
532.175767	26412.649725	31.083085
532.970788	26450.197928	31.088103
533.523651	26501.766323	31.093120
534.207491	26539.329293	31.098138
534.763861	26588.053511	31.103156
534.814921	26627.749962	31.108173
535.740522	26681.427556	31.113191
536.333812	26727.095206	31.118208
537.180447	26776.244075	31.123226
537.865838	26801.650173	31.128244
538.071912	26843.799298	31.133261
538.611231	26869.198833	31.138279
539.144231	26909.095735	31.143296
539.736735	26944.911894	31.148314
540.085408	26984.967543	31.153332
540.566746	27024.449909	31.158349
541.400397	27053.966417	31.163367
541.732561	27100.597668	31.168384
542.085182	27148.205048	31.173402
542.654319	27187.477666	31.178420
543.227087	27212.643163	31.183437
544.242651	27265.375611	31.188455
544.667340	27310.785798	31.193472
544.822353	27343.009948	31.198490
545.538842	27379.157909	31.203508
545.598074	27438.455344	31.208525
546.219336	27481.164757	31.213543
546.855223	27522.626393	31.218560
547.145252	27576.553961	31.223578
547.754662	27606.490088	31.228596
548.645286	27660.432576	31.233613
549.509552	27711.279291	31.238631
549.371282	27768.538951	31.243648
549.820396	27807.712447	31.248666
550.843577	27853.906501	31.253684
551.176443	27906.893176	31.258701
552.204197	27951.093521	31.263719
552.713340	27994.021479	31.268736
553.246165	28041.655584	31.273754
554.113443	28080.609511	31.278772
554.583866	28129.336330	31.283789
555.160254	28161.398884	31.288807
555.661417	28204.139585	31.293824
556.186824	28249.504860	31.298842
556.937809	28283.908176	31.303860
557.297347	28330.943591	31.308877
557.835766	28377.511020	31.313895
558.553025	28419.984665	31.318912
559.152563	28461.274872	31.323930
559.648077	28499.070964	31.328948
560.078598	28545.566243	31.333965
560.790199	28586.794801	31.338983
560.892511	28637.409670	31.344000
561.629343	28672.392801	31.349018
562.410513	28718.914673	31.354036
562.650134	28765.647416	31.359053
563.321580	28805.015623	31.364071
563.708243	28845.418880	31.369088
564.041688	28895.124753	31.374106
564.877531	28946.154802	31.379124
565.039590	28998.493086	31.384141
565.902991	29054.514393	31.389159
566.310632	29103.733193	31.394176
567.151209	29151.304220	31.399194
567.389069	29178.581789	31.404212
567.670032	29240.175637	31.409229
568.540494	29281.839233	31.414247
569.330270	29317.849076	31.419264
569.799901	29369.096367	31.424282
570.739979	29414.767614	31.429300
571.000071	29453.879865	31.434317
571.873864	29489.299949	31.439335
572.274599	29536.713660	31.444352
572.577668	29582.051894	31.449370
573.183663	29624.732375	31.454388
573.560439	29675.243731	31.459405
574.370436	29718.794944	31.464423
574.915614	29772.455173	31.469440
575.168031	29824.439760	31.474458
575.837795	29873.839773	31.479476
575.947702	29927.732152	31.484493
576.886432	29974.287692	31.489511
577.686790	30030.015109	31.494528
578.147162	30086.731378	31.499546
578.741229	30132.767056	31.504564
579.418700	30176.669970	31.509581
579.834531	30222.159076	31.514599
580.367839	30299.994476	31.519616
581.043368	30339.472923	31.524634
581.831320	30393.128052	31.529652
582.173315	30459.479288	31.534669
583.098291	30497.424394	31.539687
583.828909	30555.553858	31.544704
584.248883	30612.012052	31.549722
585.126370	30630.906939	31.554740
585.557298	30702.756146	31.559757
585.946487	30739.441265	31.564775
586.525703	30806.805732	31.569792
587.091857	30848.450893	31.574810
587.873410	30899.560343	31.579828
588.481948	30952.033949	31.584845
589.140250	31006.611639	31.589863
589.932554	31057.442495	31.594880
590.220645	31105.862137	31.599898
591.047619	31153.378151	31.604916
591.321457	31202.485915	31.609933
591.794619	31253.435974	31.614951
592.393184	31293.986502	31.619968
592.942584	31349.986922	31.624986
593.796266	31400.121919	31.630004
594.055112	31464.572437	31.635021
594.612030	31520.264913	31.640039
595.458115	31562.243990	31.645056
595.614119	31625.058236	31.650074
596.629948	31678.044572	31.655092
597.319649	31731.861594	31.660109
597.914698	31798.694911	31.665127
598.634650	31839.905174	31.670144
598.946952	31891.042017	31.675162
599.741775	31932.002600	31.680180
599.980960	31975.824117	31.685197
600.748994	32022.935956	31.690215
601.309656	32065.622163	31.695232
601.608178	32124.116018	31.700250
602.344714	32174.678679	31.705268
602.668569	32230.470575	31.710285
603.476012	32280.642426	31.715303
604.351727	32334.412890	31.720320
604.685057	32391.850878	31.725338
605.648047	32427.816374	31.730356
605.786263	32489.309649	31.735373
606.250346	32550.410811	31.740391
607.590175	32585.058876	31.745408
607.902559	32649.641065	31.750426
608.448145	32693.073674	31.755444
609.088059	32751.069338	31.760461
609.658346	32798.914713	31.765479
610.589189	32860.270540	31.770496
610.866866	32908.553723	31.775514
611.185377	32965.096069	31.780532
611.743798	33034.627643	31.785549
612.557829	33079.829570	31.790567
613.662925	33126.961830	31.795584
613.486439	33208.826745	31.800602
614.423457	33252.258391	31.805620
615.429838	33309.951775	31.810637
615.967645	33361.530142	31.815655
616.912616	33417.547121	31.820672
617.600849	33465.151824	31.825690
618.296867	33521.883431	31.830708
618.878812	33571.817712	31.835725
619.318091	33618.902936	31.840743
620.232893	33665.299407	31.845760
620.170545	33716.949234	31.850778
621.037682	33762.979997	31.855796
621.850697	33817.195610	31.860813
622.360625	33874.145636	31.865831
623.032272	33922.318605	31.870848
623.271337	33982.392184	31.875866
624.559503	34030.377445	31.880884
624.861762	34093.144699	31.885901
625.197452	34143.406806	31.890919
626.298789	34200.096690	31.895936
626.626944	34250.707109	31.900954
627.224542	34315.132165	31.905972
628.005867	34363.284223	31.910989
628.431679	34411.135208	31.916007
629.096149	34477.615232	31.921024
629.415111	34532.323283	31.926042
630.138160	34585.116544	31.931060
630.884755	34637.928292	31.936077
631.489504	34708.777351	31.941095
632.173209	34765.827300	31.946112
632.382883	34826.163983	31.951130
633.252518	34863.618840	31.956148
633.908010	34935.129163	31.961165
634.245132	34985.721478	31.966183
634.907620	35031.873484	31.971200
635.314836	35095.633545	31.976218
636.138499	35147.397378	31.981236
636.930831	35197.416557	31.986253
637.277216	35268.444712	31.991271
638.044200	35324.885862	31.996288
638.501207	35389.520334	32.001306
639.036131	35457.930796	32.006324
639.991004	35505.368061	32.011341
640.618895	35579.373152	32.016359
641.341912	35631.086730	32.021376
641.944085	35683.770307	32.026394
642.497915	35750.632468	32.031412
642.893587	35813.463853	32.036429
644.076263	35877.604741	32.041447
644.870313	35931.253297	32.046464
645.396065	36000.066290	32.051482
646.116735	36052.918189	32.056500
646.802270	36122.089327	32.061517
647.315060	36181.020561	32.066535
648.327590	36234.728317	32.071552
648.694105	36291.309026	32.076570
649.200816	36348.384698	32.081588
649.644767	36403.329652	32.086605
650.512806	36474.153750	32.091623
651.444488	36532.248604	32.096640
651.916626	36597.419783	32.101658
652.552438	36664.444387	32.106676
653.760194	36717.800998	32.111693
654.133941	36783.143068	32.116711
655.020604	36828.258514	32.121728
655.353052	36894.641813	32.126746
655.981439	36942.174566	32.131764
656.920997	37005.630128	32.136781
657.208129	37060.681037	32.141799
658.106190	37111.945654	32.146816
658.836491	37176.166714	32.151834
659.163895	37244.054684	32.156852
659.764077	37296.196581	32.161869
660.088700	37363.379160	32.166887
661.195318	37413.772740	32.171904
661.683394	37490.548689	32.176922
662.487940	37546.931453	32.181940
663.122418	37609.908133	32.186957
663.774574	37681.798092	32.191975
664.596563	37729.004265	32.196992
665.153047	37793.238017	32.202010
665.742600	37855.376112	32.207028
666.682261	37915.096861	32.212045
667.416080	37987.604209	32.217063
667.510115	38041.085607	32.222080
668.478447	38111.545899	32.227098
669.104215	38163.148766	32.232116
670.183203	38207.523067	32.237133
670.400089	38264.430662	32.242151
671.289118	38319.679965	32.247168
671.741672	38369.100519	32.252186
672.154795	38424.107445	32.257204
673.344636	38474.125163	32.262221
673.605042	38534.035095	32.267239
674.112779	38598.334862	32.272256
674.932688	38668.493157	32.277274
675.325555	38716.047928	32.282292
676.345242	38793.729048	32.287309
677.009783	38851.888653	32.292327
677.613541	38898.746551	32.297344
678.529667	38963.490397	32.302362
678.873887	39034.299887	32.307380
679.688156	39082.277389	32.312397
680.360971	39147.625161	32.317415
681.040669	39222.245110	32.322432
681.695604	39281.457854	32.327450
682.508380	39357.577230	32.332468
683.185271	39409.387055	32.337485
683.847672	39467.153340	32.342503
684.714022	39526.136180	32.347520
685.449767	39592.200978	32.352538
686.245949	39661.492040	32.357556
687.068910	39722.226432	32.362573
687.729352	39776.837285	32.367591
688.617638	39835.865016	32.372608
689.167456	39891.903542	32.377626
689.514247	39947.786933	32.382644
690.362651	40009.399757	32.387661
691.021822	40077.044447	32.392679
691.796095	40122.956124	32.397696
692.743265	40183.913652	32.402714
692.988741	40257.896123	32.407732
693.892406	40304.760622	32.412749
694.558269	40372.143659	32.417767
695.327306	40442.027252	32.422784
695.870789	40510.173034	32.427802
696.279233	40568.704141	32.432820
697.522081	40637.253156	32.437837
697.809229	40712.134532	32.442855
698.712263	40766.164329	32.447872
699.527238	40824.352476	32.452890
699.816634	40878.598595	32.457908
701.057848	40947.213774	32.462925
701.620606	41002.200502	32.467943
702.216719	41058.364808	32.472960
702.870248	41128.501417	32.477978
703.437934	41203.121085	32.482996
704.512380	41256.059122	32.488013
704.856045	41332.755614	32.493031
705.495010	41392.967016	32.498048
706.229840	41456.916587	32.503066
706.624594	41510.389409	32.508084
707.415990	41564.981996	32.513101
708.068375	41636.893414	32.518119
708.578876	41697.230421	32.523136
709.078854	41773.516058	32.528154
709.740195	41844.184235	32.533172
710.871412	41896.150083	32.538189
711.188198	41970.507099	32.543207
711.933640	42045.518476	32.548224
713.168968	42099.843387	32.553242
713.607437	42169.614779	32.558260
714.216658	42238.025082	32.563277
714.978287	42302.083937	32.568295
715.793070	42368.115366	32.573312
716.097954	42445.750325	32.578330
716.879866	42530.813445	32.583348
718.168815	42584.008475	32.588365
718.648493	42672.643625	32.593383
719.640498	42731.248509	32.598400
720.524019	42797.847866	32.603418
720.829818	42865.495185	32.608436
721.440755	42930.129208	32.613453
722.509662	42999.087589	32.618471
723.380914	43067.068349	32.623488
724.144842	43141.277231	32.628506
724.832276	43214.407227	32.633524
725.768130	43273.196385	32.638541
726.772872	43334.756879	32.643559
726.873590	43399.136376	32.648576
727.707905	43465.250921	32.653594
728.511597	43534.670042	32.658612
729.369558	43598.223157	32.663629
729.831111	43672.520315	32.668647
730.535349	43733.786247	32.673664
731.386702	43817.226467	32.678682
732.166619	43886.991464	32.683700
733.144496	43949.927447	32.688717
733.671278	44017.780683	32.693735
733.936092	44093.394824	32.698752
735.275841	44154.863906	32.703770
735.646261	44226.881506	32.708788
736.415424	44295.741377	32.713805
737.388401	44369.846552	32.718823
737.861813	44443.466914	32.723840
739.255725	44509.146221	32.728858
739.427989	44585.840317	32.733876
739.991208	44647.791234	32.738893
740.760048	44718.413075	32.743911
741.418325	44793.992870	32.748928
742.185410	44857.435742	32.753946
742.837160	44941.682874	32.758964
743.243494	45028.294436	32.763981
744.140722	45100.250724	32.768999
744.631417	45174.820979	32.774016
746.172472	45259.076349	32.779034
746.337217	45331.169125	32.784052
747.242637	45394.443667	32.789069
747.932928	45454.825128	32.794087
748.518479	45529.804533	32.799104
749.650259	45593.772505	32.804122
750.255724	45665.689246	32.809140
750.864614	45727.494777	32.814157
751.933647	45801.578154	32.819175
752.627036	45874.551224	32.824192
753.085500	45953.669661	32.829210
754.033515	46035.007221	32.834228
754.816909	46093.568374	32.839245
755.752999	46169.592604	32.844263
755.700404	46239.673092	32.849280
756.722053	46325.259315	32.854298
757.126855	46406.877524	32.859316
757.990038	46486.230504	32.864333
758.692104	46574.440048	32.869351
759.335158	46658.453931	32.874368
760.581703	46730.992329	32.879386
761.331827	46811.696161	32.884404
761.950163	46891.301334	32.889421
763.071719	46972.180247	32.894439
763.616468	47057.360101	32.899456
764.619464	47126.963759	32.904474
765.456581	47208.936502	32.909492
766.217208	47282.396923	32.914509
766.928293	47363.175764	32.919527
767.554765	47439.122282	32.924544
768.678403	47524.316370	32.929562
769.447621	47608.194826	32.934580
769.857945	47687.675812	32.939597
770.691607	47765.083119	32.944615
771.418614	47855.039908	32.949632
772.212843	47934.312607	32.954650
772.869938	48011.947880	32.959668
773.851395	48099.521134	32.964685
774.829560	48185.934238	32.969703
775.212666	48262.333221	32.974720
776.625413	48343.235203	32.979738
777.410924	48428.377058	32.984756
778.124285	48489.793915	32.989773
778.955245	48565.223678	32.994791
779.435858	48654.062629	32.999808
780.371285	48725.219988	33.004826
781.241605	48798.940632	33.009844
782.177481	48882.991100	33.014861
782.946427	48964.951316	33.019879
783.875575	49044.431557	33.024896
784.737083	49109.364123	33.029914
785.214012	49196.429922	33.034932
785.764084	49266.309766	33.039949
786.636655	49341.606849	33.044967
787.516786	49415.315879	33.049984
788.570866	49485.438216	33.055002
789.371985	49550.748043	33.060020
789.850119	49611.376359	33.065037
790.807368	49684.089736	33.070055
791.396283	49765.384956	33.075072
792.312103	49809.712563	33.080090
792.682143	49885.054076	33.085108
793.346099	49974.643559	33.090125
794.091487	50040.658272	33.095143
794.299111	50115.670040	33.100160
795.359727	50201.852670	33.105178
796.065840	50285.501428	33.110196
796.801303	50380.133624	33.115213
797.450829	50469.443892	33.120231
797.930569	50559.725159	33.125248
799.172727	50649.361698	33.130266
799.860691	50732.204447	33.135284
800.334283	50826.887006	33.140301
801.705317	50904.891508	33.145319
802.567515	51012.098012	33.150336
802.963016	51103.130710	33.155354
804.399308	51180.879889	33.160372
805.264692	51270.967676	33.165389
806.365625	51351.661629	33.170407
807.463712	51434.218301	33.175424
808.310820	51506.435951	33.180442
809.374001	51588.919999	33.185460
809.854883	51675.082102	33.190477
810.795793	51741.984021	33.195495
811.184032	51836.669731	33.200512
811.960172	51901.853297	33.205530
813.249162	51993.455222	33.210548
813.996338	52069.269795	33.215565
814.937213	52136.274182	33.220583
815.432564	52230.124388	33.225600
816.382807	52298.970939	33.230618
817.111720	52390.165399	33.235636
817.845427	52476.565675	33.240653
818.876798	52549.452510	33.245671
819.472828	52633.738870	33.250688
819.803118	52722.612543	33.255706
820.664224	52814.422468	33.260724
821.472498	52892.629355	33.265741
822.452899	52986.100170	33.270759
823.084173	53086.027510	33.275776
823.797329	53175.278014	33.280794
824.770891	53271.746508	33.285812
825.350557	53364.850682	33.290829
826.028460	53460.704461	33.295847
826.870195	53554.818891	33.300864
827.849933	53646.898225	33.305882
828.769321	53746.622401	33.310900
829.791123	53844.007875	33.315917
830.999994	53935.275790	33.320935
831.607831	54038.740760	33.325952
832.603284	54110.765352	33.330970
833.404544	54186.163600	33.335988
833.823460	54267.768247	33.341005
835.028883	54345.833000	33.346023
835.398805	54438.821422	33.351040
836.236542	54507.050426	33.356058
837.262999	54604.874821	33.361076
837.853360	54686.801261	33.366093
839.089152	54774.376212	33.371111
839.699783	54857.651113	33.376128
840.820263	54933.853883	33.381146
841.683170	55025.630554	33.386164
842.238190	55115.531281	33.391181
843.123223	55191.056096	33.396199
844.146745	55286.021754	33.401216
844.704181	55379.676401	33.406234
845.319560	55470.591964	33.411252
845.676873	55564.247843	33.416269
846.821212	55657.387543	33.421287
847.742081	55759.404686	33.426304
848.588287	55860.537825	33.431322
849.519321	55953.952883	33.436340
849.989324	56058.088891	33.441357
851.035685	56153.055428	33.446375
852.094598	56262.297773	33.451392
853.052944	56356.285042	33.456410
854.150283	56447.397076	33.461428
855.156949	56550.787587	33.466445
856.279353	56629.838130	33.471463
857.214009	56726.485827	33.476480
858.370572	56804.351088	33.481498
859.707351	56885.928702	33.486516
860.398985	56960.664556	33.491533
861.550599	57043.607635	33.496551
862.173701	57126.038570	33.501568
862.712821	57200.114654	33.506586
863.698361	57286.311472	33.511604
863.994195	57373.353988	33.516621
865.139712	57461.887453	33.521639
865.683469	57547.451832	33.526656
866.753459	57642.573852	33.531674
867.696782	57721.281933	33.536692
868.132439	57818.396764	33.541709
869.119334	57918.634937	33.546727
869.955473	58004.432715	33.551744
870.765012	58108.349523	33.556762
871.495265	58196.791602	33.561780
872.201770	58299.030606	33.566797
873.110179	58391.868159	33.571815
873.818221	58501.656352	33.576832
874.523313	58593.112941	33.581850
875.652942	58690.459717	33.586868
876.252047	58821.078222	33.591885
877.106042	58921.816543	33.596903
878.317119	59021.554622	33.601920
879.062521	59116.088684	33.606938
879.651090	59207.832045	33.611956
880.530572	59325.474820	33.616973
881.817094	59400.959370	33.621991
882.312064	59509.395137	33.627008
883.307468	59592.605005	33.632026
884.164393	59701.928291	33.637044
885.192489	59778.165868	33.642061
886.002962	59884.526690	33.647079
886.872647	59982.562529	33.652096
887.382875	60075.926517	33.657114
888.466940	60188.241164	33.662132
889.353341	60297.351717	33.667149
890.419361	60384.629954	33.672167
891.220790	60492.419630	33.677184
891.808366	60604.256940	33.682202
892.909517	60695.060950	33.687220
893.575952	60815.051904	33.692237
894.871809	60916.062232	33.697255
896.059052	61029.369573	33.702272
896.737278	61129.674194	33.707290
898.091127	61219.938513	33.712308
899.086327	61317.219386	33.717325
899.891206	61410.006380	33.722343
900.710590	61515.352045	33.727360
901.240411	61621.053813	33.732378
902.526059	61727.172687	33.737396
903.306714	61826.485901	33.742413
904.017767	61931.993230	33.747431
905.195998	62030.113849	33.752448
905.599968	62138.468818	33.757466
906.753102	62238.258572	33.762484
907.343579	62363.705774	33.767501
908.624529	62467.792900	33.772519
909.006492	62590.395005	33.777536
910.115252	62687.175460	33.782554
911.172542	62801.524631	33.787572
912.340796	62907.469907	33.792589
913.108226	63019.520328	33.797607
914.712131	63123.989143	33.802624
915.103817	63239.908924	33.807642
916.302471	63338.083627	33.812660
917.085037	63444.506955	33.817677
917.864245	63535.675909	33.822695
919.117870	63652.351574	33.827712
919.834098	63772.366077	33.832730
920.691525	63872.700991	33.837748
921.451531	63981.284603	33.842765
922.175204	64088.191442	33.847783
923.380411	64201.211835	33.852800
924.340671	64313.517122	33.857818
925.401891	64427.038621	33.862836
925.941271	64538.167956	33.867853
926.886058	64640.030967	33.872871
928.145759	64748.261545	33.877888
928.449642	64868.399099	33.882906
929.625576	64961.112902	33.887924
930.402040	65068.901107	33.892941
931.501942	65175.700500	33.897959
932.581948	65274.425177	33.902976
933.429481	65380.640563	33.907994
934.623042	65473.240358	33.913012
935.065996	65584.984861	33.918029
935.897265	65687.500001	33.923047
936.904873	65796.064025	33.928064
937.781264	65912.876725	33.933082
938.971030	66013.141600	33.938100
939.633658	66128.827393	33.943117
940.369568	66247.587866	33.948135
941.613011	66344.892941	33.953152
942.472866	66460.293528	33.958170
943.614708	66572.178930	33.963188
944.201725	66690.830023	33.968205
945.329693	66811.426613	33.973223
946.373625	66901.467247	33.978240
947.114807	67024.640791	33.983258
948.382324	67143.555936	33.988276
949.244620	67257.182715	33.993293
950.148715	67377.805836	33.998311
951.648614	67483.309996	34.003328
952.506346	67605.123187	34.008346
953.563233	67701.536203	34.013364
954.358919	67818.686001	34.018381
955.679867	67920.294957	34.023399
956.673760	68014.116904	34.028416
957.577627	68132.704334	34.033434
958.164750	68247.603090	34.038452
959.501744	68353.956002	34.043469
960.512913	68475.933460	34.048487
961.268521	68582.323268	34.053504
962.045698	68696.752230	34.058522
963.167771	68803.097578	34.063540
964.098468	68924.907453	34.068557
965.013947	69029.688596	34.073575
966.270841	69135.376247	34.078592
966.755844	69257.631846	34.083610
967.958883	69364.131636	34.088628
968.992487	69489.858209	34.093645
969.496782	69597.708695	34.098663
970.885334	69713.120365	34.103680
971.503770	69837.436887	34.108698
972.652004	69951.163455	34.113716
973.379390	70074.522803	34.118733
974.020681	70205.566498	34.123751
975.417589	70315.799759	34.128768
976.302925	70454.046592	34.133786
977.272102	70571.387519	34.138804
978.090444	70706.898475	34.143821
978.823242	70828.897016	34.148839
980.181940	70951.453822	34.153856
980.975908	71076.419991	34.158874
982.393875	71179.546859	34.163892
983.030092	71307.869269	34.168909
983.689747	71422.895195	34.173927
985.170418	71530.398790	34.178944
985.772941	71655.500182	34.183962
986.657135	71774.005420	34.188980
987.704584	71888.877595	34.193997
988.503241	72012.989654	34.199015
989.410092	72136.068006	34.204032
990.427871	72250.890140	34.209050
991.814351	72359.936003	34.214068
992.430292	72496.230725	34.219085
992.981676	72631.620452	34.224103
994.906124	72756.133072	34.229120
995.647582	72887.387172	34.234138
996.581511	73005.310550	34.239156
997.593826	73129.123906	34.244173
998.470781	73256.264314	34.249191
999.514014	73389.407285	34.254208
1000.685376	73523.421730	34.259226
1001.570108	73635.113585	34.264244
1002.562983	73771.167517	34.269261
1003.314464	73905.207093	34.274279
1004.682446	74030.163771	34.279296
1005.811767	74158.223969	34.284314
1007.111005	74293.581859	34.289332
1008.267563	74416.817867	34.294349
1009.088913	74544.405038	34.299367
1010.237248	74669.021500	34.304384
1011.141328	74795.320616	34.309402
1012.177500	74917.119093	34.314420
1013.291726	75050.261844	34.319437
1014.201127	75169.769123	34.324455
1015.811611	75289.127672	34.329472
1016.532328	75413.134281	34.334490
1017.619836	75525.107767	34.339508
1018.728835	75656.991463	34.344525
1019.685209	75775.129839	34.349543
1020.942905	75895.281186	34.354560
1021.707534	76020.074506	34.359578
1022.558130	76134.970854	34.364596
1024.184322	76261.556137	34.369613
1024.637178	76394.029333	34.374631
1026.237953	76511.026745	34.379648
1027.130236	76628.232335	34.384666
1027.729404	76756.292307	34.389684
1029.098554	76879.901428	34.394701
1029.803737	76999.180278	34.399719
1030.748137	77126.340791	34.404736
1031.926724	77254.197980	34.409754
1032.852232	77387.171292	34.414772
1033.876674	77506.661466	34.419789
1034.479505	77648.978460	34.424807
1035.980424	77776.124041	34.429824
1036.799754	77896.578209	34.434842
1037.672569	78032.294483	34.439860
1038.645699	78148.118157	34.444877
1039.464287	78249.973716	34.449895
1040.444110	78380.985559	34.454912
1040.946411	78509.015090	34.459930
1042.089471	78641.475309	34.464948
1043.388259	78764.538234	34.469965
1044.282279	78908.941403	34.474983
1045.510675	79030.670841	34.480000
1046.273038	79176.430491	34.485018
1047.153879	79314.909821	34.490036
1048.045232	79459.077101	34.495053
1049.218184	79603.143716	34.500071
1050.573562	79735.646767	34.505088
1051.612685	79883.130929	34.510106
1052.583416	80024.988747	34.515124
1053.790840	80147.758460	34.520141
1054.829125	80307.666520	34.525159
1056.486893	80432.136185	34.530176
1057.115428	80585.082548	34.535194
1058.193128	80733.470577	34.540212
1059.494117	80865.812558	34.545229
1060.463676	80990.407697	34.550247
1061.563909	81131.247445	34.555264
1062.377326	81288.101432	34.560282
1063.700708	81422.390380	34.565300
1065.261013	81555.188591	34.570317
1065.919295	81692.157886	34.575335
1066.980648	81841.359275	34.580352
1068.137219	81974.104273	34.585370
1069.199076	82107.756526	34.590388
1070.364432	82248.833718	34.595405
1071.347414	82407.559347	34.600423
1072.670043	82543.758483	34.605440
1073.440199	82684.781370	34.610458
1074.299105	82825.323281	34.615476
1075.738357	82957.751426	34.620493
1076.663641	83115.676098	34.625511
1077.930461	83243.290918	34.630528
1079.001878	83392.229956	34.635546
1079.935024	83537.664364	34.640564
1081.306237	83673.256218	34.645581
1082.123551	83838.006028	34.650599
1082.980413	83984.214313	34.655616
1084.041540	84126.585172	34.660634
1085.085278	84275.560166	34.665652
1086.350636	84411.085106	34.670669
1087.226631	84563.547096	34.675687
1088.601938	84721.469164	34.680704
1089.553714	84869.053090	34.685722
1090.653851	85025.276210	34.690740
1091.864304	85171.215203	34.695757
1093.166868	85312.227941	34.700775
1094.506992	85466.133713	34.705792
1095.624053	85606.046168	34.710810
1096.389601	85734.527168	34.715828
1097.757277	85849.831516	34.720845
1098.713242	85981.919281	34.725863
1099.610043	86117.823588	34.730880
1100.762559	86255.964310	34.735898
1101.782865	86386.324548	34.740916
1102.840536	86509.490510	34.745933
1103.757580	86644.414911	34.750951
1104.711707	86782.451495	34.755968
1105.880239	86920.486488	34.760986
1106.874749	87076.412692	34.766004
1108.220227	87232.941819	34.771021
1109.425779	87377.315954	34.776039
1110.334467	87505.835450	34.781056
1111.557924	87658.934638	34.786074
1112.246177	87802.786878	34.791092
1113.304756	87937.070918	34.796109
1114.211554	88112.968682	34.801127
1116.083623	88259.228293	34.806144
1117.279301	88409.422158	34.811162
1117.831090	88561.831518	34.816180
1119.401610	88722.838054	34.821197
1120.274226	88872.776672	34.826215
1121.068150	89027.692897	34.831232
1122.548741	89172.459031	34.836250
1123.395494	89340.003804	34.841268
1124.931435	89496.689857	34.846285
1125.997180	89656.733881	34.851303
1127.011513	89820.568934	34.856320
1128.439630	89968.978639	34.861338
1129.087845	90132.267171	34.866356
1130.785136	90281.173741	34.871373
1131.919865	90443.641010	34.876391
1133.032108	90594.483061	34.881408
1134.025245	90747.906371	34.886426
1135.043433	90917.744354	34.891444
1136.192680	91078.044847	34.896461
1137.528802	91236.286705	34.901479
1138.517231	91387.634570	34.906496
1139.870649	91541.948487	34.911514
1140.879983	91709.220008	34.916532
1142.116447	91864.718488	34.921549
1143.230959	92023.393391	34.926567
1144.502008	92187.686046	34.931584
1145.816578	92332.392063	34.936602
1146.997954	92499.775062	34.941620
1148.318242	92656.246133	34.946637
1149.471064	92803.915624	34.951655
1150.607127	92955.990810	34.956672
1152.004981	93113.616550	34.961690
1152.686420	93265.083077	34.966708
1154.333763	93410.476937	34.971725
1155.524490	93560.732345	34.976743
1156.422078	93723.299539	34.981760
1157.621161	93859.691272	34.986778
1158.969708	94003.182104	34.991796
1159.888743	94125.262099	34.996813
1161.044296	94281.941642	35.001831
1161.942347	94416.069657	35.006848
1163.481059	94552.013150	35.011866
1164.512366	94692.484819	35.016884
1165.872685	94824.435474	35.021901
1166.601339	94968.752190	35.026919
1167.352577	95117.165096	35.031936
1168.769496	95257.325988	35.036954
1169.745173	95409.247383	35.041972
1170.503833	95563.747172	35.046989
1171.753990	95720.598886	35.052007
1173.152208	95881.141282	35.057024
1174.537749	96033.729182	35.062042
1175.372204	96197.020251	35.067060
1176.531058	96348.931533	35.072077
1177.752378	96523.619362	35.077095
1178.460338	96691.374827	35.082112
1179.694695	96850.666057	35.087130
1181.028593	97016.116679	35.092148
1182.021326	97195.495607	35.097165
1183.585604	97366.630842	35.102183
1184.595638	97530.953763	35.107200
1186.227765	97705.629694	35.112218
1186.936890	97884.679607	35.117236
1188.230831	98050.232706	35.122253
1189.782470	98223.957517	35.127271
1190.552993	98397.769894	35.132288
1192.208466	98558.208166	35.137306
1193.293416	98734.592227	35.142324
1194.330159	98902.457270	35.147341
1195.510047	99074.697696	35.152359
1196.951853	99245.025121	35.157376
1198.254339	99411.396544	35.162394
1199.459287	99583.428039	35.167412
1200.535561	99750.812196	35.172429
1201.892732	99933.893805	35.177447
1202.881183	100099.643192	35.182464
1204.613560	100263.105393	35.187482
1205.608906	100435.132306	35.192500
1206.814186	100601.831498	35.197517
1208.280578	100773.438062	35.202535
1209.385338	100940.434069	35.207552
1210.868869	101104.663085	35.212570
1211.937417	101281.442606	35.217588
1212.778427	101451.913527	35.222605
1214.247192	101621.273543	35.227623
1215.264539	101795.325450	35.232640
1216.562215	101962.494298	35.237658
1217.548533	102137.850797	35.242676
1219.001133	102311.394455	35.247693
1220.080706	102491.984190	35.252711
1221.188105	102666.281390	35.257728
1222.569423	102820.560368	35.262746
1223.769185	102993.415307	35.267764
1225.157522	103153.175034	35.272781
1226.720462	103303.093913	35.277799
1227.710612	103464.741436	35.282816
1229.154047	103615.889905	35.287834
1229.833019	103778.614155	35.292852
1231.229193	103926.608252	35.297869
1232.389898	104092.010682	35.302887
1233.398276	104257.640984	35.307904
1234.831995	104409.397253	35.312922
1235.613038	104598.656677	35.317940
1236.592675	104770.167525	35.322957
1238.069867	104932.772839	35.327975
1239.248451	105115.702070	35.332992
1240.290065	105289.181205	35.338010
1241.511920	105467.170291	35.343028
1242.629863	105651.771294	35.348045
1243.899249	105836.299027	35.353063
1245.286301	106024.334390	35.358080
1246.777578	106197.913211	35.363098
1247.840349	106380.864266	35.368116
1248.771235	106575.083465	35.373133
1250.377978	106754.938532	35.378151
1251.602384	106945.918156	35.383168
1252.812939	107133.173919	35.388186
1253.965914	107328.547386	35.393204
1255.205747	107515.997673	35.398221
1256.553461	107698.299603	35.403239
1257.730775	107902.610157	35.408256
1259.311540	108085.529845	35.413274
1260.717942	108276.060743	35.418292
1262.035222	108468.088303	35.423309
1263.352176	108647.649181	35.428327
1264.632419	108840.805833	35.433344
1265.933800	109024.220083	35.438362
1267.460416	109209.580957	35.443380
1269.052758	109388.761773	35.448397
1270.131824	109579.494208	35.453415
1270.951618	109771.642822	35.458432
1272.751532	109948.060480	35.463450
1273.776809	110126.349485	35.468468
1274.521700	110344.218421	35.473485
1276.279442	110519.064535	35.478503
1277.503377	110711.795587	35.483520
1278.799702	110897.522384	35.488538
1280.133620	111087.536147	35.493556
1281.155789	111265.688357	35.498573
1282.965602	111456.407882	35.503591
1284.224568	111659.869806	35.508608
1285.712495	111847.314030	35.513626
1287.021913	112025.710922	35.518644
1287.832003	112213.582174	35.523661
1289.602197	112400.783171	35.528679
1290.703560	112599.467062	35.533696
1291.900130	112772.044607	35.538714
1293.312527	112945.430958	35.543732
1294.405727	113126.231302	35.548749
1295.554802	113294.135663	35.553767
1296.524160	113473.964368	35.558784
1297.911421	113637.275361	35.563802
1299.080198	113818.676430	35.568820
1299.834048	114009.013720	35.573837
1301.454963	114186.389063	35.578855
1303.009579	114384.458059	35.583872
1303.894010	114577.393423	35.588890
1305.606625	114761.272435	35.593908
1306.487334	114954.312576	35.598925
1308.261154	115131.493040	35.603943
1309.397254	115335.966789	35.608960
1310.644453	115518.108378	35.613978
1312.060572	115716.507429	35.618996
1313.321605	115918.560306	35.624013
1315.040336	116109.462846	35.629031
1315.994906	116304.527477	35.634048
1317.436524	116500.269589	35.639066
1318.813987	116699.214289	35.644084
1319.875022	116895.095906	35.649101
1321.387315	117080.334180	35.654119
1322.658302	117290.968851	35.659136
1324.043408	117500.080269	35.664154
1325.226062	117688.078818	35.669172
1326.517705	117901.507367	35.674189
1328.068102	118095.338672	35.679207
1329.446981	118297.898199	35.684224
1330.695529	118497.504204	35.689242
1332.244878	118700.432364	35.694260
1333.435986	118893.073131	35.699277
1334.945317	119092.344708	35.704295
1336.008911	119295.715664	35.709312
1337.357038	119512.840006	35.714330
1339.335623	119710.864051	35.719348
1340.531361	119917.638091	35.724365
1341.675259	120099.030875	35.729383
1342.981456	120319.150977	35.734400
1344.281161	120528.712099	35.739418
1345.658550	120727.016737	35.744436
1347.452041	120939.010188	35.749453
1348.965569	121138.385444	35.754471
1350.323494	121338.420175	35.759488
1351.382570	121537.718724	35.764506
1353.184289	121731.809548	35.769524
1354.447229	121934.751472	35.774541
1356.047721	122127.496738	35.779559
1357.419239	122316.961582	35.784576
1358.805559	122515.582280	35.789594
1359.959911	122707.402150	35.794612
1361.179917	122909.294520	35.799629
1362.879078	123106.768061	35.804647
1364.209225	123300.248778	35.809664
1365.078495	123495.235357	35.814682
1367.124770	123675.559494	35.819700
1368.244749	123847.178738	35.824717
1369.349562	124030.036054	35.829735
1370.713838	124212.144098	35.834752
1371.920689	124390.820594	35.839770
1373.047209	124574.260819	35.844788
1374.331594	124759.893786	35.849805
1375.587948	124958.312718	35.854823
1376.905853	125155.710028	35.859840
1378.043131	125361.915321	35.864858
1379.498190	125556.405831	35.869876
1380.307706	125756.700307	35.874893
1381.642898	125970.073431	35.879911
1383.425357	126181.046469	35.884928
1384.746925	126390.359030	35.889946
1386.014515	126598.541755	35.894964
1387.208563	126811.095246	35.899981
1389.002024	127026.569933	35.904999
1390.549916	127237.208443	35.910016
1391.817272	127451.414699	35.915034
1393.161879	127668.675891	35.920052
1394.541003	127881.943032	35.925069
1396.251359	128089.800763	35.930087
1397.838223	128319.531636	35.935104
1398.879786	128526.232173	35.940122
1400.591604	128742.493426	35.945140
1401.767554	128965.986338	35.950157
1403.057251	129178.720355	35.955175
1404.636532	129394.083002	35.960192
1405.810019	129626.943517	35.965210
1407.755318	129834.409689	35.970228
1409.181347	130066.017583	35.975245
1410.695048	130283.057142	35.980263
1412.005844	130501.118801	35.985280
1413.149264	130719.601498	35.990298
1415.046093	130922.066602	35.995316
1416.088214	131141.164133	36.000333
1417.579128	131360.673491	36.005351
1419.352225	131573.653055	36.010368
1420.887467	131796.022031	36.015386
1422.440443	132018.174565	36.020404
1423.881018	132237.306013	36.025421
1425.217401	132441.594194	36.030439
1426.921256	132664.931464	36.035456
1428.215834	132875.032173	36.040474
1429.732244	133088.342698	36.045492
1430.997517	133308.219809	36.050509
1432.168019	133518.775777	36.055527
1433.590775	133729.179186	36.060544
1435.034802	133956.913791	36.065562
1436.936309	134174.491848	36.070580
1438.139701	134392.892039	36.075597
1439.214728	134601.469210	36.080615
1440.886213	134824.004954	36.085632
1442.250940	135047.566816	36.090650
1443.748462	135256.955897	36.095668
1445.106636	135458.918089	36.100685
1446.616219	135659.375117	36.105703
1448.447921	135859.769683	36.110720
1449.109939	136052.102495	36.115738
1450.465804	136262.611095	36.120756
1452.332255	136469.276674	36.125773
1453.515501	136683.769243	36.130791
1454.788404	136893.725372	36.135808
1456.029879	137117.259422	36.140826
1457.717035	137324.466422	36.145844
1459.086311	137553.825209	36.150861
1460.413246	137769.329337	36.155879
1461.644518	137982.404530	36.160896
1463.074346	138222.276760	36.165914
1464.707081	138447.064007	36.170932
1466.187633	138684.460839	36.175949
1467.328537	138905.109807	36.180967
1468.888928	139149.176086	36.185984
1470.051688	139381.965483	36.191002
1471.924079	139609.828291	36.196020
1473.124161	139838.762801	36.201037
1474.486313	140095.300450	36.206055
1476.477342	140343.578902	36.211072
1477.396429	140582.106601	36.216090
1479.494240	140824.757847	36.221108
1480.965694	141066.319268	36.226125
1482.168536	141309.179981	36.231143
1483.727652	141550.528581	36.236160
1485.475805	141798.477429	36.241178
1486.833155	142035.882411	36.246196
1488.664602	142295.215857	36.251213
1490.018057	142537.340081	36.256231
1491.700419	142780.427907	36.261248
1492.915220	143022.071046	36.266266
1494.652008	143268.246623	36.271284
1496.406003	143509.453070	36.276301
1498.220558	143754.961135	36.281319
1499.369370	143983.326761	36.286336
1500.877267	144227.670555	36.291354
1502.589594	144467.104002	36.296372
1504.063604	144703.383087	36.301389
1505.316085	144953.806466	36.306407
1507.424219	145175.374114	36.311424
1508.971853	145417.908456	36.316442
1510.449246	145658.478499	36.321460
1512.179271	145879.363390	36.326477
1513.972332	146115.678580	36.331495
1515.364367	146343.173677	36.336512
1517.090487	146584.953547	36.341530
1518.717109	146800.943206	36.346548
1519.800083	147035.819017	36.351565
1521.366931	147276.754874	36.356583
1523.020879	147497.282961	36.361600
1524.196889	147722.616713	36.366618
1525.694318	147940.561470	36.371636
1527.090033	148163.315529	36.376653
1528.595609	148381.984572	36.381671
1530.087540	148600.289666	36.386688
1531.281136	148822.636769	36.391706
1532.703314	149037.000838	36.396724
1534.376146	149273.155893	36.401741
1535.639237	149489.424421	36.406759
1537.518811	149720.998945	36.411776
1538.821474	149944.908443	36.416794
1540.394903	150189.896553	36.421812
1541.916567	150410.478442	36.426829
1543.371977	150650.912324	36.431847
1544.915904	150895.454079	36.436864
1546.074451	151127.761732	36.441882
1547.927086	151364.461326	36.446900
1549.179885	151610.804207	36.451917
1550.590441	151873.478206	36.456935
1552.497117	152116.412128	36.461952
1553.940642	152365.760401	36.466970
1555.362113	152608.267917	36.471988
1556.886616	152862.031727	36.477005
1558.389328	153101.740774	36.482023
1559.682810	153370.911223	36.487040
1561.281912	153628.257034	36.492058
1563.658458	153877.886899	36.497076
1564.919702	154135.873518	36.502093
1566.662715	154400.277119	36.507111
1568.487542	154656.669469	36.512128
1570.162966	154903.312058	36.517146
1571.591729	155158.630054	36.522164
1573.291268	155405.995206	36.527181
1574.916908	155664.328753	36.532199
1576.422958	155908.013309	36.537216
1578.176632	156172.023405	36.542234
1579.767047	156419.362585	36.547252
1581.394194	156682.369707	36.552269
1583.028943	156940.711524	36.557287
1584.557930	157191.958734	36.562304
1586.045544	157458.189298	36.567322
1587.816101	157709.858412	36.572340
1589.371465	157947.273116	36.577357
1590.772785	158215.399899	36.582375
1592.900355	158463.746336	36.587392
1594.345462	158724.490208	36.592410
1595.972064	158979.336168	36.597428
1597.597143	159227.222628	36.602445
1599.249130	159491.413860	36.607463
1600.887490	159722.347738	36.612480
1602.475789	159991.967534	36.617498
1603.683869	160249.323954	36.622516
1605.293213	160499.517172	36.627533
1606.968523	160752.098414	36.632551
1608.409572	161006.861789	36.637568
1610.009464	161280.775846	36.642586
1611.262460	161524.146986	36.647604
1613.128010	161762.058255	36.652621
1614.122051	162015.263956	36.657639
1616.311126	162239.266117	36.662656
1617.788364	162492.081415	36.667674
1619.390599	162737.840252	36.672692
1621.070805	162990.753646	36.677709
1622.281190	163245.544273	36.682727
1623.772674	163494.255397	36.687744
1625.285779	163759.844730	36.692762
1627.228439	164013.966458	36.697780
1628.966155	164275.414849	36.702797
1630.397151	164540.870744	36.707815
1631.985259	164803.957352	36.712832
1633.492466	165071.827358	36.717850
1634.947654	165346.606967	36.722868
1636.572106	165614.259385	36.727885
1638.458085	165893.768757	36.732903
1640.357830	166152.465293	36.737920
1641.937067	166424.861513	36.742938
1643.372270	166707.137420	36.747956
1645.138689	166980.662152	36.752973
1646.592343	167251.790673	36.757991
1648.148348	167526.025029	36.763008
1650.118674	167811.991279	36.768026
1651.838072	168094.892062	36.773044
1653.614432	168362.235678	36.778061
1655.148906	168653.731527	36.783079
1656.968730	168926.627738	36.788096
1658.543881	169204.321264	36.793114
1659.906602	169495.635215	36.798132
1662.344521	169770.633665	36.803149
1663.584794	170062.694374	36.808167
1665.381079	170336.099077	36.813184
1667.357751	170614.132275	36.818202
1668.780742	170907.337341	36.823220
1670.643931	171179.367457	36.828237
1672.182899	171466.266744	36.833255
1673.999598	171734.375855	36.838272
1675.987304	172014.523012	36.843290
1677.097347	172305.619177	36.848308
1678.869172	172590.345966	36.853325
1680.439871	172874.624714	36.858343
1682.109784	173163.088586	36.863360
1684.071790	173456.950209	36.868378
1685.882729	173741.514168	36.873396
1687.541618	174023.846275	36.878413
1689.169728	174321.826682	36.883431
1690.917232	174594.050959	36.888448
1692.487952	174873.586822	36.893466
1694.087334	175166.808187	36.898484
1695.877958	175442.063288	36.903501
1697.435036	175760.984862	36.908519
1699.385526	176043.525862	36.913536
1701.178432	176306.759944	36.918554
1703.251504	176579.263031	36.923572
1704.759662	176844.639041	36.928589
1706.153449	177110.212536	36.933607
1707.916274	177370.781369	36.938624
1709.188591	177638.026810	36.943642
1711.043628	177911.600958	36.948660
1712.870841	178184.559672	36.953677
1714.318463	178457.453578	36.958695
1715.916840	178715.430765	36.963712
1717.551024	179001.721470	36.968730
1718.770998	179295.692211	36.973748
1720.748825	179569.625641	36.978765
1722.505024	179858.567126	36.983783
1724.013442	180149.998601	36.988800
1725.728070	180448.009540	36.993818
1727.281448	180739.031907	36.998836
1729.403043	181040.496840	37.003853
1731.295179	181345.235714	37.008871
1732.674204	181645.465196	37.013888
1734.676699	181951.891015	37.018906
1736.115123	182252.178717	37.023924
1737.829376	182561.585551	37.028941
1739.260213	182869.085587	37.033959
1741.262512	183164.811094	37.038976
1743.137071	183496.479811	37.043994
1744.398513	183813.707319	37.049012
1746.803482	184122.025783	37.054029
1748.489559	184438.365588	37.059047
1749.841910	184753.885099	37.064064
1751.987638	185062.860305	37.069082
1753.951347	185382.626784	37.074100
1755.759921	185697.268410	37.079117
1757.572938	186011.429338	37.084135
1759.514042	186315.928293	37.089152
1761.190938	186627.843728	37.094170
1762.776660	186952.541313	37.099188
1764.599624	187259.869686	37.104205
1766.415894	187581.730747	37.109223
1767.895889	187897.251849	37.114240
1770.085175	188212.751325	37.119258
1771.633651	188535.714786	37.124276
1773.597864	188856.469887	37.129293
1775.114559	189184.823412	37.134311
1777.109998	189497.469023	37.139328
1779.149213	189825.173013	37.144346
1780.630065	190137.790345	37.149364
1782.733809	190455.361612	37.154381
1784.691398	190772.158702	37.159399
1786.058024	191094.660917	37.164416
1788.368026	191405.974707	37.169434
1790.109958	191734.246620	37.174452
1792.110924	192045.118655	37.179469
1793.867117	192361.184026	37.184487
1795.465099	192680.423914	37.189504
1797.918504	192970.340746	37.194522
1799.206276	193278.440298	37.199540
1801.235786	193560.584805	37.204557
1803.243263	193851.948262	37.209575
1804.734880	194137.557313	37.214592
1806.218373	194418.739997	37.219610
1808.302865	194705.324262	37.224628
1809.947123	195001.333708	37.229645
1811.882991	195302.679847	37.234663
1813.139303	195599.693565	37.239680
1814.972886	195879.724660	37.244698
1816.463053	196201.923297	37.249716
1818.352950	196515.950381	37.254733
1820.224379	196812.048542	37.259751
1821.755831	197137.013350	37.264768
1823.330475	197459.295301	37.269786
1825.207036	197773.205230	37.274804
1826.971878	198111.097844	37.279821
1828.864059	198433.106949	37.284839
1830.258145	198761.416393	37.289856
1832.735311	199087.233226	37.294874
1833.973343	199428.454503	37.299892
1835.892556	199757.511779	37.304909
1837.865107	200086.549920	37.309927
1839.372489	200442.141205	37.314944
1841.535831	200767.929241	37.319962
1843.666147	201118.970879	37.324980
1845.291104	201453.695514	37.329997
1847.072875	201797.472924	37.335015
1848.792016	202148.599123	37.340032
1851.008757	202485.685909	37.345050
1852.706089	202845.718016	37.350068
1854.456176	203195.436957	37.355085
1856.475804	203548.682192	37.360103
1858.483201	203906.844028	37.365120
1860.574943	204250.955478	37.370138
1862.480421	204604.606235	37.375156
1864.172071	204951.768462	37.380173
1866.520688	205306.317953	37.385191
1868.380808	205648.697409	37.390208
1870.485433	205985.365811	37.395226
1871.836807	206343.151893	37.400244
1874.160176	206680.893981	37.405261
1876.494504	207031.305215	37.410279
1878.417892	207380.590472	37.415296
1880.254421	207707.435026	37.420314
1882.142287	208058.443647	37.425332
1883.997241	208380.452323	37.430349
1885.997966	208721.494316	37.435367
1887.756575	209069.025593	37.440384
1889.935724	209402.058079	37.445402
1891.640845	209746.212174	37.450420
1893.196915	210074.510432	37.455437
1895.596081	210407.424574	37.460455
1897.287905	210766.261919	37.465472
1899.530544	211080.428424	37.470490
1901.331235	211405.533765	37.475508
1903.183712	211721.199947	37.480525
1904.817433	212034.007871	37.485543
1906.561905	212343.118077	37.490560
1908.564810	212654.727859	37.495578
1909.916778	212978.769834	37.500596
1911.733099	213302.193826	37.505613
1913.843900	213628.835483	37.510631
1915.517016	213973.550798	37.515648
1917.616157	214294.344879	37.520666
1919.179708	214631.742842	37.525684
1920.773247	214980.297488	37.530701
1922.831381	215312.402375	37.535719
1924.234095	215667.973677	37.540736
1926.455426	216022.667867	37.545754
1928.394999	216371.708024	37.550772
1929.955855	216725.228359	37.555789
1932.293480	217086.638629	37.560807
1934.216972	217449.005251	37.565824
1936.333375	217798.862520	37.570842
1938.125722	218176.032403	37.575860
1940.057022	218536.041845	37.580877
1941.954314	218895.410978	37.585895
1943.511845	219262.961733	37.590912
1945.715246	219635.439805	37.595930
1948.017575	220006.050354	37.600948
1949.734666	220393.706041	37.605965
1951.568449	220751.316886	37.610983
1953.675396	221138.990812	37.616000
1955.963851	221510.969719	37.621018
1957.926661	221884.627384	37.626036
1959.892100	222257.461160	37.631053
1962.011230	222628.151930	37.636071
1963.944294	223013.463288	37.641088
1966.258246	223373.854580	37.646106
1968.056037	223769.615752	37.651124
1970.087386	224192.082912	37.656141
1971.995227	224561.724447	37.661159
1974.198714	224933.034979	37.666176
1976.518632	225305.839791	37.671194
1978.311614	225684.888365	37.676212
1980.432134	226044.662197	37.681229
1982.478740	226409.528501	37.686247
1984.312248	226789.502711	37.691264
1986.161610	227170.377704	37.696282
1988.366802	227543.248977	37.701300
1990.511978	227911.966435	37.706317
1992.602614	228279.424329	37.711335
1994.649203	228648.998697	37.716352
1996.777369	229015.056976	37.721370
1998.592567	229379.591857	37.726388
2000.933422	229749.403578	37.731405
2003.113485	230120.969349	37.736423
2004.626869	230489.544009	37.741440
2006.765028	230848.827302	37.746458
2009.014171	231189.910012	37.751476
2010.679794	231540.661360	37.756493
2013.080554	231867.347670	37.761511
2014.644851	232211.234950	37.766528
2016.671521	232541.919593	37.771546
2018.597630	232886.310696	37.776564
2020.682774	233241.090902	37.781581
2022.641286	233579.409308	37.786599
2024.532068	233940.775582	37.791616
2026.444505	234280.576831	37.796634
2028.737550	234630.986088	37.801652
2030.015703	235000.047501	37.806669
2031.893851	235357.103283	37.811687
2033.955763	235727.541536	37.816704
2036.115979	236097.152794	37.821722
2038.243358	236469.920020	37.826740
2039.854931	236845.361084	37.831757
2041.889887	237223.885778	37.836775
2043.606866	237614.526735	37.841792
2045.686458	237995.206007	37.846810
2047.999751	238378.973635	37.851828
2049.990494	238774.934573	37.856845
2052.098846	239160.743991	37.861863
2054.055797	239555.747919	37.866880
2056.461411	239942.376460	37.871898
2058.553810	240353.160122	37.876916
2060.441099	240745.613896	37.881933
2062.679126	241135.600391	37.886951
2064.947245	241536.683099	37.891968
2066.797865	241935.699806	37.896986
2068.994528	242329.430562	37.902004
2071.082961	242736.616364	37.907021
2073.315071	243133.392088	37.912039
2075.547115	243535.934926	37.917056
2077.360610	243932.347784	37.922074
2079.543454	244329.897100	37.927092
2081.641551	244735.182804	37.932109
2084.096469	245128.881347	37.937127
2085.941195	245539.797823	37.942144
2087.812258	245936.995039	37.947162
2090.515528	246347.320574	37.952180
2092.249461	246762.576434	37.957197
2094.462768	247160.459507	37.962215
2096.818928	247570.386475	37.967232
2098.831823	247971.427909	37.972250
2101.195029	248370.814612	37.977268
2102.984783	248781.419048	37.982285
2105.593850	249175.663281	37.987303
2107.209509	249588.101002	37.992320
2109.097580	249988.075359	37.997338
2111.750823	250391.536366	38.002356
2113.514758	250802.302658	38.007373
2115.851912	251201.776997	38.012391
2117.866022	251607.095103	38.017408
2119.963696	252004.755039	38.022426
2122.223565	252385.193225	38.027444
2124.009075	252770.991048	38.032461
2126.404249	253145.135195	38.037479
2128.021442	253525.830187	38.042496
2129.918606	253902.595076	38.047514
2132.584582	254289.348778	38.052532
2134.656385	254670.583665	38.057549
2136.507442	255063.209045	38.062567
2138.725260	255453.059017	38.067584
2140.620818	255844.357982	38.072602
2142.572441	256228.586991	38.077620
2144.437369	256634.015951	38.082637
2146.661064	257037.610625	38.087655
2148.922682	257448.566724	38.092672
2150.520322	257863.744081	38.097690
2153.152701	258280.942707	38.102708
2155.135711	258702.004642	38.107725
2157.238580	259112.760286	38.112743
2159.489605	259535.102110	38.117760
2161.709481	259966.721550	38.122778
2164.017780	260391.468975	38.127796
2166.034260	260817.533501	38.132813
2168.642916	261226.993000	38.137831
2171.094004	261656.063640	38.142848
2173.192891	262082.015425	38.147866
2175.535895	262495.634129	38.152884
2177.698684	262922.669300	38.157901
2179.799756	263347.987440	38.162919
2182.066872	263779.630546	38.167936
2184.118908	264202.137834	38.172954
2186.384054	264616.965529	38.177972
2188.197596	265068.344100	38.182989
2190.560049	265494.690339	38.188007
2192.920629	265923.323619	38.193024
2194.959115	266372.889804	38.198042
2197.564170	266800.621512	38.203060
2199.892663	267228.880146	38.208077
2202.175943	267659.686661	38.213095
2204.506148	268087.361515	38.218112
2206.553192	268523.032838	38.223130
2208.988962	268953.486001	38.228148
2211.097004	269392.171307	38.233165
2213.980172	269812.723068	38.238183
2216.200124	270253.931545	38.243200
2217.852786	270679.429373	38.248218
2220.641254	271092.325096	38.253236
2222.426199	271519.351994	38.258253
2224.643806	271948.164928	38.263271
2226.946109	272379.555756	38.268288
2229.034090	272817.992065	38.273306
2231.766833	273242.201998	38.278324
2233.490799	273676.530137	38.283341
2235.707901	274106.436204	38.288359
2238.163671	274532.443192	38.293376
2240.204680	274962.605957	38.298394
2242.729056	275367.060077	38.303412
2245.135337	275777.299520	38.308429
2247.033881	276168.643123	38.313447
2249.504179	276564.900535	38.318464
2251.251470	276975.523874	38.323482
2253.352071	277374.329372	38.328500
2255.388795	277785.846644	38.333517
2257.357801	278205.300437	38.338535
2259.923494	278623.745004	38.343552
2261.815185	279054.515348	38.348570
2264.065407	279471.841125	38.353588
2266.112844	279902.942123	38.358605
2268.110958	280348.378253	38.363623
2270.435718	280786.954283	38.368640
2272.847355	281226.100587	38.373658
2274.948875	281661.510715	38.378676
2277.136816	282124.977517	38.383693
2279.297790	282572.647430	38.388711
2281.860359	283025.232386	38.393728
2283.885144	283486.158299	38.398746
2286.218041	283938.448684	38.403764
2288.607096	284410.442640	38.408781
2290.989240	284874.282813	38.413799
2293.600700	285335.469637	38.418816
2295.688641	285801.387737	38.423834
2298.163446	286246.616677	38.428852
2300.235393	286728.794215	38.433869
2302.674178	287181.369271	38.438887
2305.613197	287650.376402	38.443904
2307.806844	288124.175208	38.448922
2310.139682	288587.891724	38.453940
2312.939977	289040.432410	38.458957
2315.117398	289513.469662	38.463975
2317.601863	289967.761035	38.468992
2319.892220	290439.407151	38.474010
2322.554527	290891.255602	38.479028
2324.795233	291360.342347	38.484045
2326.707232	291820.614850	38.489063
2329.561189	292279.746507	38.494080
2331.754787	292748.711171	38.499098
2333.701959	293214.487876	38.504116
2336.530501	293684.950411	38.509133
2338.506274	294156.156820	38.514151
2341.264637	294610.904488	38.519168
2343.312097	295086.492153	38.524186
2345.663393	295555.146594	38.529204
2348.216734	296018.331891	38.534221
2350.546796	296500.603097	38.539239
2353.295252	296958.319250	38.544256
2355.134395	297429.311280	38.549274
2357.681586	297901.510809	38.554292
2360.165148	298367.292556	38.559309
2362.560784	298839.767716	38.564327
2365.049651	299303.285443	38.569344
2367.487210	299754.185456	38.574362
2369.925554	300195.863384	38.579380
2372.125680	300632.421404	38.584397
2374.484022	301062.602832	38.589415
2377.273862	301470.945745	38.594432
2379.442601	301906.616269	38.599450
2381.426658	302329.614235	38.604468
2383.657641	302774.645525	38.609485
2386.025809	303204.641721	38.614503
2388.774659	303647.429262	38.619520
2390.740961	304098.823418	38.624538
2393.134398	304541.283567	38.629556
2395.409140	304993.972271	38.634573
2397.750686	305449.697013	38.639591
2400.443774	305901.275036	38.644608
2402.431098	306360.431176	38.649626
2404.384718	306821.419917	38.654644
2406.812377	307281.087302	38.659661
2409.282527	307761.930146	38.664679
2412.008923	308235.821732	38.669696
2414.072820	308715.912553	38.674714
2416.537742	309192.432770	38.679732
2418.990318	309662.780925	38.684749
2421.214580	310161.534976	38.689767
2423.704971	310639.010648	38.694784
2426.034743	311127.177650	38.699802
2428.178790	311622.255280	38.704820
2430.844387	312114.682780	38.709837
2433.418320	312626.273669	38.714855
2435.965216	313114.016731	38.719872
2438.362782	313618.417630	38.724890
2440.824087	314138.654973	38.729908
2443.494601	314636.556529	38.734925
2445.586474	315145.037065	38.739943
2448.180573	315643.428519	38.744960
2450.545181	316156.965957	38.749978
2453.021510	316662.330253	38.754996
2455.755841	317179.435842	38.760013
2458.514789	317679.314993	38.765031
2461.523243	318190.733471	38.770048
2463.757977	318679.261515	38.775066
2466.494416	319187.314494	38.780084
2469.478278	319672.010669	38.785101
2471.947908	320178.779891	38.790119
2474.479264	320662.018759	38.795136
2477.214549	321162.213375	38.800154
2479.557192	321640.651494	38.805172
2482.504125	322129.988096	38.810189
2485.055075	322612.603833	38.815207
2487.614155	323086.733190	38.820224
2489.975533	323579.557591	38.825242
2492.497338	324062.880953	38.830260
2494.709873	324543.507790	38.835277
2497.116468	325029.231099	38.840295
2499.684746	325521.046327	38.845312
2502.333146	325992.072314	38.850330
2504.707625	326452.396699	38.855348
2507.231897	326906.244313	38.860365
2509.594315	327348.153870	38.865383
2512.173379	327788.452146	38.870400
2514.436176	328255.945210	38.875418
2516.881455	328704.284318	38.880436
2519.309905	329152.598099	38.885453
2521.352610	329621.565267	38.890471
2523.988295	330086.372504	38.895488
2526.431393	330551.435933	38.900506
2528.707113	331020.382868	38.905524
2531.172965	331504.202870	38.910541
2533.072815	331998.216022	38.915559
2535.656970	332476.551213	38.920576
2538.089520	332986.699644	38.925594
2540.857832	333475.968896	38.930612
2543.304403	333979.404211	38.935629
2545.666435	334493.590441	38.940647
2547.755542	335003.524774	38.945664
2550.236857	335518.877954	38.950682
2552.835468	336040.226614	38.955700
2555.489582	336565.015782	38.960717
2557.784397	337100.852413	38.965735
2560.619605	337633.145874	38.970752
2563.242966	338164.199042	38.975770
2565.922869	338700.875784	38.980788
2568.776836	339228.786034	38.985805
2570.901147	339778.491233	38.990823
2573.424432	340319.724238	38.995840
2576.484376	340861.933993	39.000858
2579.275806	341403.775363	39.005876
2581.744327	341941.423069	39.010893
2584.150707	342500.834845	39.015911
2587.231375	343032.688765	39.020928
2589.865731	343576.744755	39.025946
2592.296691	344126.667510	39.030964
2595.111726	344656.441900	39.035981
2597.721805	345216.938693	39.040999
2600.681286	345754.246120	39.046016
2603.340373	346288.168808	39.051034
2605.851267	346835.514791	39.056052
2608.669129	347384.000151	39.061069
2611.068433	347921.883885	39.066087
2613.985187	348464.453307	39.071104
2616.735063	349013.136753	39.076122
2619.461535	349558.010529	39.081140
2622.375564	350098.152771	39.086157
2624.932112	350635.706181	39.091175
2627.159170	351171.351780	39.096192
2630.228789	351710.412600	39.101210
2632.548685	352245.550510	39.106228
2635.527230	352779.690257	39.111245
2638.185514	353328.547747	39.116263
2641.172916	353850.109813	39.121280
2643.828120	354375.704623	39.126298
2646.308322	354894.645843	39.131316
2648.790609	355380.506483	39.136333
2651.198687	355884.498105	39.141351
2653.767454	356395.135091	39.146368
2656.349201	356889.316686	39.151386
2658.525302	357395.589103	39.156404
2661.116629	357902.298282	39.161421
2663.434209	358427.523917	39.166439
2666.175015	358944.224744	39.171456
2668.797846	359468.477179	39.176474
2671.156930	360001.700009	39.181492
2673.782287	360536.676861	39.186509
2676.536225	361068.860893	39.191527
2678.979655	361612.077968	39.196544
2681.764047	362163.331142	39.201562
2684.103140	362719.749782	39.206580
2686.693702	363271.629801	39.211597
2689.218033	363828.285099	39.216615
2691.893606	364395.975027	39.221632
2694.531233	364968.105245	39.226650
2697.033994	365553.954009	39.231668
2700.023354	366123.603077	39.236685
2702.612824	366720.208715	39.241703
2705.218349	367295.080807	39.246720
2707.780927	367894.466557	39.251738
2710.420766	368484.442566	39.256756
2713.388471	369069.917874	39.261773
2716.195676	369685.430635	39.266791
2718.997204	370284.009987	39.271808
2722.172455	370877.446787	39.276826
2724.941980	371480.328373	39.281844
2728.070849	372072.360308	39.286861
2730.879835	372658.826907	39.291879
2733.493225	373264.042265	39.296896
2736.231382	373862.327504	39.301914
2738.954450	374451.675162	39.306932
2741.980244	375052.206641	39.311949
2744.401491	375655.565295	39.316967
2747.181979	376247.034760	39.321984
2750.076801	376851.163354	39.327002
2752.772374	377457.648613	39.332020
2755.759500	378056.010574	39.337037
2758.571235	378677.503899	39.342055
2761.200299	379276.208632	39.347072
2764.276867	379870.139999	39.352090
2767.206013	380480.474324	39.357108
2770.044260	381075.363760	39.362125
2772.792223	381677.640613	39.367143
2775.546956	382282.900416	39.372160
2778.838455	382873.986530	39.377178
2781.546998	383483.750069	39.382196
2784.483180	384084.716128	39.387213
2787.421697	384671.619128	39.392231
2790.047454	385265.081555	39.397248
2792.910844	385841.501814	39.402266
2795.791330	386417.783564	39.407284
2798.571541	386951.484305	39.412301
2800.927102	387514.160211	39.417319
2803.538255	388066.387625	39.422336
2806.009026	388624.259638	39.427354
2808.187911	389186.379580	39.432372
2811.475940	389750.318808	39.437389
2814.162657	390333.619962	39.442407
2816.947179	390915.906935	39.447424
2819.944487	391484.455249	39.452442
2822.654371	392064.249631	39.457460
2825.744066	392637.000010	39.462477
2828.250899	393219.825319	39.467495
2830.918416	393806.520857	39.472512
2834.243611	394387.092048	39.477530
2836.773341	394991.845306	39.482548
2839.344100	395591.484239	39.487565
2842.501840	396186.379084	39.492583
2844.672239	396788.722851	39.497600
2847.665837	397408.422168	39.502618
2850.562070	398017.374061	39.507636
2853.684516	398641.163288	39.512653
2856.505451	399256.747786	39.517671
2858.935419	399879.431530	39.522688
2862.070381	400505.262657	39.527706
2864.929329	401121.794983	39.532724
2867.860488	401758.004316	39.537741
2870.745387	402388.656004	39.542759
2873.720127	403020.421986	39.547776
2876.983127	403656.363743	39.552794
2879.601325	404291.330070	39.557812
2882.515956	404923.093143	39.562829
2885.923711	405563.638368	39.567847
2887.980810	406201.798543	39.572864
2891.627391	406832.672105	39.577882
2894.449683	407468.910670	39.582900
2897.425454	408121.335193	39.587917
2900.543354	408758.311510	39.592935
2903.494611	409406.783549	39.597952
2906.303980	410032.983876	39.602970
2909.147351	410690.443902	39.607988
2912.168580	411310.272862	39.613005
2915.165385	411960.964052	39.618023
2918.368202	412605.297494	39.623040
2921.450665	413247.963265	39.628058
2924.441379	413888.830160	39.633076
2927.402673	414521.146974	39.638093
2930.287595	415159.671274	39.643111
2933.317207	415806.471024	39.648128
2936.445298	416436.363066	39.653146
2939.627126	417074.544838	39.658164
2942.450894	417712.845143	39.663181
2945.476453	418347.475632	39.668199
2948.238947	418993.004338	39.673216
2951.553311	419593.758194	39.678234
2954.222862	420199.263622	39.683252
2956.808792	420796.230339	39.688269
2959.944231	421378.350947	39.693287
2962.771950	421966.310276	39.698304
2965.713145	422569.162363	39.703322
2968.034350	423170.984658	39.708340
2971.032886	423776.765607	39.713357
2974.073348	424384.933351	39.718375
2976.485069	425003.396738	39.723392
2979.359577	425621.342165	39.728410
2982.361712	426251.565151	39.733428
2984.951666	426875.986860	39.738445
2987.854063	427517.798247	39.743463
2990.775343	428173.726062	39.748480
2994.036987	428819.198333	39.753498
2996.626305	429475.070585	39.758516
2999.922929	430133.600851	39.763533
3002.677035	430778.168384	39.768551
3005.352279	431460.218055	39.773568
3008.977398	432116.569574	39.778586
3011.584068	432791.174280	39.783604
3014.800501	433468.425438	39.788621
3017.467671	434143.086521	39.793639
3020.813126	434824.434868	39.798656
3023.873860	435514.192335	39.803674
3026.657004	436207.165740	39.808692
3029.802376	436895.555409	39.813709
3033.163328	437587.817054	39.818727
3035.965275	438294.024087	39.823744
3039.197920	438980.342325	39.828762
3042.278435	439686.643042	39.833780
3045.401089	440401.322877	39.838797
3048.548373	441095.115739	39.843815
3051.891797	441790.933995	39.848832
3055.150442	442491.201626	39.853850
3058.372722	443202.188921	39.858868
3061.413230	443893.387407	39.863885
3065.059539	444597.380754	39.868903
3067.806060	445296.584907	39.873920
3071.183569	445988.631699	39.878938
3074.448276	446684.928731	39.883956
3077.425231	447381.503963	39.888973
3080.967440	448080.297837	39.893991
3083.764000	448763.850884	39.899008
3087.293569	449461.390745	39.904026
3090.360392	450144.607567	39.909044
3093.174846	450839.030384	39.914061
3096.691397	451524.109439	39.919079
3099.640018	452222.467988	39.924096
3102.692834	452908.591437	39.929114
3105.830756	453608.902243	39.934132
3108.452744	454290.041932	39.939149
3111.574112	454986.820925	39.944167
3114.939674	455701.403481	39.949184
3118.108356	456363.771423	39.954202
3121.228662	457028.050338	39.959220
3124.016780	457686.998363	39.964237
3127.290288	458338.968586	39.969255
3129.914948	459003.013966	39.974272
3132.934180	459661.563167	39.979290
3136.040777	460324.632376	39.984308
3139.034359	461010.365176	39.989325
3141.997907	461678.981238	39.994343
3144.779942	462374.266435	39.999360
3147.607945	463057.734972	40.004378
3150.307918	463761.487447	40.009396
3153.306185	464457.632546	40.014413
3156.568666	465157.051760	40.019431
3159.427223	465877.503412	40.024448
3162.588888	466597.528667	40.029466
3165.779800	467321.065322	40.034484
3168.819188	468072.873449	40.039501
3172.230500	468806.641840	40.044519
3175.101127	469552.708710	40.049536
3178.202992	470293.705788	40.054554
3181.443625	471044.869508	40.059572
3184.317184	471806.936042	40.064589
3187.868751	472559.866500	40.069607
3190.942662	473326.800500	40.074624
3194.138796	474093.838105	40.079642
3197.559221	474863.895520	40.084660
3200.670691	475649.645556	40.089677
3204.049553	476415.808143	40.094695
3207.407835	477188.820190	40.099712
3210.758515	477960.944261	40.104730
3213.781431	478752.097192	40.109748
3216.627534	479545.723494	40.114765
3220.558211	480310.234106	40.119783
3223.847223	481123.642235	40.124800
3227.214634	481899.401044	40.129818
3230.245241	482682.712867	40.134836
3233.765482	483497.805282	40.139853
3237.135978	484266.192035	40.144871
3240.083822	485071.707006	40.149888
3243.607609	485863.049426	40.154906
3246.909996	486650.301353	40.159924
3250.265430	487452.771836	40.164941
3254.163108	488247.645018	40.169959
3257.040968	489051.235161	40.174976
3260.257952	489800.174601	40.179994
3263.758373	490624.717220	40.185012
3266.936683	491402.394839	40.190029
3270.154446	492214.636560	40.195047
3273.534426	492991.003751	40.200064
3276.740215	493775.195153	40.205082
3280.213677	494586.080420	40.210100
3282.845798	495398.729739	40.215117
3286.623293	496160.658023	40.220135
3289.487995	496992.997415	40.225152
3292.939570	497757.233663	40.230170
3296.393705	498532.193285	40.235188
3299.420605	499275.577194	40.240205
3303.145020	500037.704628	40.245223
3305.651574	500792.671083	40.250240
3309.243114	501530.267892	40.255258
3312.317117	502305.831669	40.260276
3315.785799	503062.771347	40.265293
3318.868476	503834.884459	40.270311
3322.166409	504566.848410	40.275328
3325.356153	505379.311655	40.280346
3328.829376	506118.653962	40.285364
3331.814515	506934.156416	40.290381
3334.817416	507704.647999	40.295399
3338.040064	508486.022408	40.300416
3341.107910	509316.086322	40.305434
3344.487250	510106.648439	40.310452
3347.241244	510944.353960	40.315469
3351.194424	511726.676719	40.320487
3354.224968	512598.721163	40.325504
3356.688358	513404.513385	40.330522
3360.794057	514232.761492	40.335540
3363.799216	515119.159802	40.340557
3367.496813	515943.907196	40.345575
3370.700153	516799.311824	40.350592
3374.091924	517676.080515	40.355610
3377.831219	518528.032862	40.360628
3380.789703	519402.256837	40.365645
3384.698519	520248.495224	40.370663
3387.856014	521146.450297	40.375680
3391.212651	521998.031397	40.380698
3394.594209	522880.525516	40.385716
3398.381767	523745.864562	40.390733
3401.618223	524644.219339	40.395751
3405.086121	525526.505182	40.400768
3408.655978	526387.753955	40.405786
3412.639215	527258.469352	40.410804
3415.792927	528193.540035	40.415821
3419.272995	529075.023194	40.420839
3422.539402	529927.660277	40.425856
3426.560816	530798.477845	40.430874
3430.309882	531706.131107	40.435892
3433.334085	532591.067857	40.440909
3437.661936	533457.204082	40.445927
3441.218867	534333.290256	40.450944
3444.443274	535236.688948	40.455962
3447.529132	536087.909749	40.460980
3451.463158	536954.718628	40.465997
3454.721816	537863.902694	40.471015
3458.571346	538713.194672	40.476032
3461.769027	539590.549246	40.481050
3465.746191	540492.108594	40.486068
3468.970220	541339.287405	40.491085
3472.565419	542234.356247	40.496103
3476.338552	543101.544754	40.501120
3480.104799	543952.600775	40.506125
3483.306906	544751.776431	40.511130
3486.764455	545488.221890	40.516135
3489.834822	546220.502260	40.521140
3493.244690	546813.781850	40.526144
3495.831127	547388.340707	40.531149
3498.505873	547908.655479	40.536154
3501.167669	548311.810131	40.541159
3503.698778	548738.341971	40.546164
3506.011758	549038.774532	40.551168
3507.818383	549314.854460	40.556173
3509.711493	549542.568008	40.561178
3511.695535	549695.623618	40.566183
3513.005007	549848.279567	40.571188
3514.522414	549909.204749	40.576192
3516.079726	549929.246080	40.581197
3517.608390	549980.732064	40.586202
3518.290347	549912.192820	40.591207
3519.589455	549864.902891	40.596212
3519.965126	549753.262746	40.601216
3520.876389	549645.776321	40.606221
3521.427514	549487.828261	40.611226
3521.906740	549306.977405	40.616231
3522.621711	549151.220414	40.621236
3523.155923	548930.586960	40.626240
3523.242832	548703.863527	40.631245
3523.490254	548490.687881	40.636250
3523.660448	548223.567163	40.641255
3523.758274	547985.979498	40.646260
3524.193055	547681.962127	40.651264
3523.843762	547457.559722	40.656269
3523.787337	547174.859206	40.661274
3523.568311	546859.066486	40.666279
3523.975217	546602.327589	40.671284
3524.082230	546302.876570	40.676288
3523.916529	546002.806364	40.681293
3523.839188	545715.841003	40.686298
3523.837810	545380.648390	40.691303
3523.340972	545114.233147	40.696308
3523.051496	544787.856623	40.701312
3523.265566	544476.336788	40.706317
3523.243207	544200.692517	40.711322
3522.689864	543920.229892	40.716327
3522.485902	543594.873964	40.721332
3522.673062	543265.460551	40.726336
3522.347188	542957.023698	40.731341
3522.127565	542695.772416	40.736346
3521.829705	542419.331035	40.741351
3521.680463	542099.387086	40.746356
3521.485466	541800.196417	40.751360
3521.153105	541499.708658	40.756365
3521.232646	541232.426336	40.761370
3521.007974	540918.276210	40.766375
3520.800459	540612.196447	40.771380
3520.573262	540381.356204	40.776384
3519.714132	540089.255864	40.781389
3519.978937	539796.113766	40.786394
3519.389372	539545.976482	40.791399
3519.554128	539276.373637	40.796404
3519.052178	538988.740855	40.801408
3518.393133	538763.146064	40.806413
3518.932053	538473.520928	40.811418
3518.127808	538242.739411	40.816423
3517.644156	537974.074605	40.821428
3517.719394	537738.550411	40.826432
3517.743083	537482.726591	40.831437
3517.374186	537278.630872	40.836442
3516.708032	537020.938535	40.841447
3516.603816	536808.157618	40.846452
3516.640052	536561.711334	40.851456
3515.953110	536357.603125	40.856461
3515.963921	536135.803665	40.861466
3515.664854	535936.932369	40.866471
3515.452653	535696.017405	40.871476
3515.193621	535531.736429	40.876480
3514.879878	535304.015616	40.881485
3515.081129	535117.885507	40.886490
3514.906213	534896.804819	40.891495
3514.367574	534729.781111	40.896500
3514.359857	534500.737190	40.901504
3513.623963	534353.796094	40.906509
3514.205012	534140.971156	40.911514
3514.076260	533978.623347	40.916519
3513.367164	533815.052042	40.921524
3513.405967	533611.399127	40.926528
3513.264515	533468.296307	40.931533
3513.530997	533258.388708	40.936538
3513.019973	533115.138966	40.941543
3512.561322	532956.874408	40.946548
3512.742686	532773.750722	40.951552
3512.201067	532622.619663	40.956557
3512.354261	532473.347776	40.961562
3511.798090	532303.269333	40.966567
3511.905731	532182.649388	40.971572
3511.761117	532012.805896	40.976576
3511.089756	531889.224737	40.981581
3511.382350	531729.313239	40.986586
3510.616752	531606.603697	40.991591
3510.858019	531469.586385	40.996596
3511.102784	531332.314685	41.001600
3510.744413	531206.303867	41.006605
3510.729165	531060.582130	41.011610
3510.517473	530956.425069	41.016615
3510.421011	530809.501142	41.021620
3510.328276	530703.605602	41.026624
3510.246076	530586.793145	41.031629
3510.136429	530456.694589	41.036634
3509.759119	530326.586730	41.041639
3509.257908	530254.911735	41.046644
3509.677144	530106.838595	41.051648
3509.723967	529981.865640	41.056653
3509.462371	529897.821283	41.061658
3509.358067	529826.485872	41.066663
3509.043785	529690.450478	41.071668
3509.386594	529568.611065	41.076672
3508.973156	529505.863232	41.081677
3509.014401	529399.432430	41.086682
3508.313195	529297.767419	41.091687
3508.581477	529182.253612	41.096692
3508.785352	529127.744954	41.101696
3508.318231	529014.519154	41.106701
3508.340969	528932.345074	41.111706
3508.496023	528825.033323	41.116711
3507.777750	528759.955522	41.121716
3508.143865	528679.747310	41.126720
3508.107377	528592.072361	41.131725
3508.119767	528501.609672	41.136730
3508.170247	528438.582144	41.141735
3507.461078	528334.486430	41.146740
3507.769063	528282.434754	41.151744
3507.877022	528194.128329	41.156749
3507.650228	528108.451769	41.161754
3507.485302	528034.995275	41.166759
3507.371384	527961.833613	41.171764
3507.590537	527885.435024	41.176768
3507.000556	527813.308157	41.181773
3507.410241	527742.134838	41.186778
3507.137524	527685.674985	41.191783
3506.973400	527628.035356	41.196788
3507.183358	527554.214159	41.201792
3506.841675	527491.244861	41.206797
3506.801498	527416.097973	41.211802
3506.526337	527373.434923	41.216807
3506.304473	527308.677049	41.221812
3506.507330	527256.335395	41.226816
3506.415018	527209.094325	41.231821
3506.752494	527141.366532	41.236826
3506.727540	527094.872598	41.241831
3506.332578	527042.624726	41.246836
3506.595708	526968.337544	41.251840
3506.299795	526930.629687	41.256845
3506.087078	526877.240549	41.261850
3506.055109	526821.194468	41.266855
3505.995908	526769.195890	41.271860
3506.242492	526734.484920	41.276864
3505.924933	526681.010612	41.281869
3505.769171	526640.348442	41.286874
3505.777633	526584.851114	41.291879
3505.669211	526546.253487	41.296884
3506.025885	526509.351275	41.301888
3505.498241	526472.083307	41.306893
3505.649707	526407.414410	41.311898
3505.731314	526403.813071	41.316903
3505.440177	526328.599649	41.321908
3505.788535	526310.601676	41.326912
3505.464485	526271.380395	41.331917
3505.833140	526212.539491	41.336922
3505.534493	526180.238525	41.341927
3505.473785	526152.600519	41.346932
3505.596193	526102.946662	41.351936
3505.468489	526079.059413	41.356941
3505.360238	526023.174230	41.361946
3505.445173	525993.086780	41.366951
3505.138149	525962.757951	41.371956
3505.464912	525913.778842	41.376960
3505.048664	525914.602959	41.381965
3505.487816	525847.965625	41.386970
3505.480615	525816.830954	41.391975
3505.127494	525805.261461	41.396980
3505.480319	525768.509792	41.401984
3505.094360	525728.488239	41.406989
3505.175763	525685.461061	41.411994
3504.963144	525667.247754	41.416999
3505.241496	525620.347785	41.422004
3505.381415	525591.463999	41.427008
3504.948762	525567.320907	41.432013
3505.044107	525521.460498	41.437018
3504.857823	525524.522875	41.442023
3504.889063	525473.617824	41.447028
3504.818691	525451.792988	41.452032
3504.653531	525433.571915	41.457037
3504.913012	525418.417604	41.462042
3505.099575	525374.362040	41.467047
3504.740629	525347.022517	41.472052
3504.814830	525325.629582	41.477056
3504.854830	525301.815766	41.482061
3504.866143	525274.164865	41.487066
3505.082233	525242.134490	41.492071
3505.027770	525214.493883	41.497076
3504.978851	525189.177533	41.502080
3504.724691	525166.420956	41.507085
3504.716408	525136.296088	41.512090
3504.515154	525126.724007	41.517095
3504.874880	525083.297398	41.522100
3504.628359	525079.242146	41.527104
3504.445450	525060.164143	41.532109
3504.707369	525024.284457	41.537114
3504.551298	525023.197223	41.542119
3504.699252	524987.183823	41.547124
3504.530004	524962.543259	41.552128
3504.639057	524941.953077	41.557133
3504.919924	524922.144487	41.562138
3504.648573	524892.010192	41.567143
3504.589026	524883.426535	41.572148
3504.901110	524840.916676	41.577152
3504.563144	524817.111331	41.582157
3504.376146	524819.365177	41.587162
3504.574339	524783.545576	41.592167
3504.439284	524754.400457	41.597172
3504.504797	524756.260561	41.602176
3504.580461	524723.189825	41.607181
3504.359453	524703.814129	41.612186
3504.489610	524678.367577	41.617191
3504.145431	524683.527577	41.622196
3504.772593	524649.257449	41.627200
3504.505572	524633.376829	41.632205
3504.605549	524613.293154	41.637210
3504.676257	524588.361348	41.642215
3504.506656	524567.410334	41.647220
3504.606948	524548.741911	41.652224
3504.381738	524534.472166	41.657229
3504.682958	524497.068614	41.662234
3504.678896	524474.423181	41.667239
3504.370313	524471.691874	41.672244
3504.545156	524451.697265	41.677248
3504.470189	524443.772959	41.682253
3504.257240	524426.063796	41.687258
3504.279550	524394.365665	41.692263
3504.336368	524384.802904	41.697268
3504.200032	524368.951918	41.702272
3504.177406	524358.036847	41.707277
3504.382610	524321.052464	41.712282
3504.626011	524340.981439	41.717287
3504.348482	524298.765541	41.722292
3504.612436	524274.308211	41.727296
3504.531705	524268.811142	41.732301
3504.287515	524251.763880	41.737306
3504.449085	524233.590912	41.742311
3504.474829	524212.456913	41.747316
3504.736591	524196.997795	41.752320
3504.174772	524174.945599	41.757325
3504.665845	524147.570798	41.762330
3504.279878	524146.671490	41.767335
3503.965939	524112.953372	41.772340
3504.262839	524107.952624	41.777344
3504.095834	524089.376468	41.782349
3504.303417	524067.708032	41.787354
3504.375469	524047.678619	41.792359
3504.141769	524058.887473	41.797364
3504.432084	524019.715258	41.802368
3504.026673	524015.482644	41.807373
3504.127751	524006.974238	41.812378
3504.339292	523976.155300	41.817383
3504.007732	523984.902661	41.822388
3504.351361	523963.970853	41.827392
3504.302370	523943.808789	41.832397
3504.131768	523925.637423	41.837402
3504.403605	523921.398850	41.842407
3504.257562	523905.751149	41.847412
3504.180056	523877.707484	41.852416
3504.034174	523878.842827	41.857421
3504.079036	523843.247585	41.862426
3504.215263	523837.614977	41.867431
3504.062284	523841.936198	41.872436
3504.232043	523813.246722	41.877440
3504.440209	523804.569630	41.882445
3504.414528	523800.175840	41.887450
3504.547078	523778.670532	41.892455
3504.307033	523763.543069	41.897460
3504.351856	523733.053329	41.902464
3504.211621	523732.570127	41.907469
3504.078146	523706.708746	41.912474
3504.319853	523695.144827	41.917479
3503.795673	523658.324760	41.922484
3504.025493	523671.078293	41.927488
3503.898337	523652.040367	41.932493
3503.763631	523652.011258	41.937498
3503.949698	523657.896614	41.942503
3503.951727	523638.636046	41.947508
3504.310666	523611.533986	41.952512
3503.799188	523617.276840	41.957517
3504.114933	523615.255550	41.962522
3504.084342	523582.350933	41.967527
3503.904763	523579.043008	41.972532
3504.085091	523580.379577	41.977536
3504.215666	523540.422613	41.982541
3503.922485	523540.216340	41.987546
3504.141825	523543.619402	41.992551
3504.130114	523526.888501	41.997556
3504.167090	523498.826086	42.002560
3504.087893	523505.511712	42.007565
3503.925289	523484.052662	42.012570
3504.209094	523470.510373	42.017575
3504.078734	523469.570626	42.022580
3504.049892	523423.926104	42.027584
3504.083318	523424.578163	42.032589
3504.146788	523422.596721	42.037594
3504.247347	523403.522513	42.042599
3504.115641	523388.225918	42.047604
3504.417564	523373.720176	42.052608
3503.797893	523358.601780	42.057613
3503.920230	523340.585672	42.062618
3504.081926	523340.509717	42.067623
3503.837827	523333.420448	42.072628
3504.075418	523297.186909	42.077632
3504.049467	523295.725118	42.082637
3504.256254	523297.967489	42.087642
3504.054510	523282.833523	42.092647
3503.844238	523269.268047	42.097652
3504.013366	523265.500517	42.102656
3503.910194	523242.919580	42.107661
3504.043450	523241.786496	42.112666
3504.395094	523228.890479	42.117671
3503.971094	523230.120376	42.122676
3504.351686	523211.203898	42.127680
3504.085637	523205.836865	42.132685
3503.892777	523184.179985	42.137690
3503.964023	523169.154429	42.142695
3503.967395	523168.041868	42.147700
3504.072075	523155.336486	42.152704
3503.992095	523136.088283	42.157709
3503.725278	523133.147930	42.162714
3504.278180	523128.763623	42.167719
3503.745530	523115.501738	42.172724
3504.319114	523098.071244	42.177728
3504.189526	523093.440915	42.182733
3504.248863	523080.692087	42.187738
3504.015156	523046.504082	42.192743
3503.659961	523074.668433	42.197748
3504.102239	523049.321656	42.202752
3503.957066	523031.094714	42.207757
3503.956502	523021.439111	42.212762
3504.109154	523023.083426	42.217767
3503.886615	523006.031430	42.222772
3504.125249	522988.400985	42.227776
3504.131720	522973.132714	42.232781
3504.248430	522941.568486	42.237786
3504.314419	522961.628308	42.242791
3504.484249	522917.063158	42.247796
3504.579637	522931.051830	42.252800
3504.309899	522906.676789	42.257805
3503.953160	522879.787731	42.262810
3504.246660	522862.906799	42.267815
3504.052078	522872.239764	42.272820
3504.140790	522845.886903	42.277824
3504.089985	522826.583168	42.282829
3504.061901	522825.829438	42.287834
3504.421127	522795.136583	42.292839
3504.121719	522794.274070	42.297844
3504.371636	522769.007814	42.302848
3504.310235	522753.143404	42.307853
3503.926414	522743.952648	42.312858
3504.053416	522737.158352	42.317863
3503.986128	522716.340438	42.322868
3504.106481	522700.700027	42.327872
3503.898623	522701.137473	42.332877
3504.088123	522679.116159	42.337882
3504.131442	522665.408988	42.342887
3503.804960	522663.944082	42.347892
3504.032271	522645.809504	42.352896
3503.735149	522616.888374	42.357901
3503.247222	522621.010078	42.362906
3503.458396	522627.953504	42.367911
3503.525781	522624.454684	42.372916
3503.649145	522623.171455	42.377920
3503.824222	522628.047814	42.382925
3504.153049	522616.924359	42.387930
3504.100383	522607.377855	42.392935
3503.827609	522600.848907	42.397940
3504.119672	522587.405690	42.402944
3504.196427	522574.754825	42.407949
3504.272811	522553.206218	42.412954
3504.079479	522549.293587	42.417959
3504.108394	522536.599697	42.422964
3504.267233	522530.760841	42.427968
3504.082687	522519.212900	42.432973
3503.979453	522494.204256	42.437978
3504.212399	522483.298088	42.442983
3504.120329	522477.953871	42.447988
3504.073795	522452.177864	42.452992
3504.308238	522442.788110	42.457997
3503.853894	522436.388905	42.463002
3504.056855	522409.107273	42.468007
3504.052169	522394.345783	42.473012
3504.215111	522383.551724	42.478016
3503.882308	522389.772328	42.483021
3503.556689	522365.556976	42.488026
3503.884943	522347.102775	42.493031
3503.767551	522349.851521	42.498036
3503.936927	522359.582263	42.503040
3503.953474	522343.553465	42.508045
3503.814603	522332.807073	42.513050
3504.243686	522324.296503	42.518055
3503.892012	522309.286439	42.523060
3503.593947	522276.118114	42.528064
3503.525713	522290.790431	42.533069
3503.884675	522295.182819	42.538074
3504.310004	522279.746585	42.543079
3504.146851	522259.752143	42.548084
3503.894022	522243.816378	42.553088
3503.966071	522251.540303	42.558093
3503.951614	522234.555723	42.563098
3503.884566	522208.327562	42.568103
3503.936520	522213.071835	42.573108
3504.158578	522212.986336	42.578112
3503.714992	522193.440588	42.583117
3504.012106	522175.496682	42.588122
3504.285679	522167.364507	42.593127
3503.986595	522161.597893	42.598132
3503.978188	522153.105821	42.603136
3503.905592	522141.590476	42.608141
3503.824288	522142.007935	42.613146
3504.165985	522132.196597	42.618151
3503.740142	522106.581105	42.623156
3503.903318	522082.186965	42.628160
3504.039239	522092.782625	42.633165
3503.787693	522076.795936	42.638170
3504.283906	522063.067237	42.643175
3503.725815	522050.516301	42.648180
3503.894946	522042.956700	42.653184
3504.006475	522026.811465	42.658189
3503.796180	522020.221851	42.663194
3503.775689	522019.315212	42.668199
3503.672538	522020.039471	42.673204
3504.115218	522016.784550	42.678208
3503.888338	522010.096439	42.683213
3503.757130	521997.831896	42.688218
3503.895594	521974.300975	42.693223
3503.633357	521996.587831	42.698228
3503.948590	521976.416319	42.703232
3503.745516	521962.039695	42.708237
3503.788748	521951.618173	42.713242
3503.994016	521942.283301	42.718247
3503.836503	521938.971552	42.723252
3504.098176	521913.550442	42.728256
3503.715269	521919.374681	42.733261
3503.620536	521901.037386	42.738266
3503.784305	521906.016864	42.743271
3503.594251	521893.357082	42.748276
3504.011453	521877.618408	42.753280
3504.140045	521865.262146	42.758285
3503.546223	521875.316030	42.763290
3503.857363	521889.726516	42.768295
3503.912745	521846.389914	42.773300
3503.949610	521840.570090	42.778304
3503.865967	521847.054866	42.783309
3503.788838	521838.624050	42.788314
3504.310232	521810.077702	42.793319
3504.208819	521805.644784	42.798324
3503.848552	521804.286255	42.803329
3503.994492	521781.411129	42.808333
3503.873833	521762.622754	42.813338
3504.186350	521756.658217	42.818343
3503.978381	521754.112776	42.823348
3503.962053	521717.258603	42.828353
3504.133191	521728.101724	42.833357
3503.781998	521727.500127	42.838362
3504.391034	521695.451211	42.843367
3504.141255	521691.294503	42.848372
3504.019793	521686.965838	42.853377
3504.149803	521659.846160	42.858381
3503.969863	521654.566119	42.863386
3504.091637	521634.879788	42.868391
3503.742735	521627.654661	42.873396
3503.980405	521607.697188	42.878401
3504.093968	521613.695862	42.883405
3503.968684	521603.806338	42.888410
3503.975962	521583.531338	42.893415
3504.063625	521570.119590	42.898420
3504.078420	521569.359026	42.903425
3503.830311	521561.410118	42.908429
3503.580796	521535.411950	42.913434
3503.991266	521535.549465	42.918439
3503.866450	521536.934433	42.923444
3503.922975	521522.769186	42.928449
3503.927852	521504.870733	42.933453
3503.814448	521490.226726	42.938458
3504.094150	521492.356708	42.943463
3503.805354	521477.942646	42.948468
3503.638647	521475.946788	42.953473
3503.770514	521454.842994	42.958477
3503.663750	521443.383115	42.963482
3503.898629	521454.772494	42.968487
3503.923971	521448.752116	42.973492
3503.818503	521427.129646	42.978497
3503.850931	521414.788243	42.983501
3503.652376	521408.702118	42.988506
3504.073111	521415.360146	42.993511
3503.793020	521415.505686	42.998516
3503.970919	521388.984700	43.003521
3503.515051	521379.855118	43.008525
3503.368782	521409.961129	43.013530
3503.431711	521376.632803	43.018535
3503.537573	521387.992060	43.023540
3503.514273	521384.406190	43.028545
3503.713700	521383.919791	43.033549
3503.719891	521355.201281	43.038554
3504.106121	521339.719784	43.043559
3503.992752	521335.743662	43.048564
3503.752434	521329.866346	43.053569
3504.000278	521310.260818	43.058573
3504.075740	521305.243655	43.063578
3504.040222	521310.709848	43.068583
3503.499914	521288.245850	43.073588
3504.109827	521271.262708	43.078593
3504.240467	521270.938857	43.083597
3503.891465	521275.847891	43.088602
3504.097537	521262.771095	43.093607
3503.952892	521238.070430	43.098612
3504.217865	521222.152948	43.103617
3504.072720	521210.193375	43.108621
3503.704302	521203.527302	43.113626
3504.282115	521171.482298	43.118631
3503.922576	521186.049965	43.123636
3503.909553	521156.171266	43.128641
3503.826691	521139.398600	43.133645
3503.907794	521149.801295	43.138650
3504.277866	521138.619760	43.143655
3503.963014	521121.428700	43.148660
3504.109223	521108.866844	43.153665
3503.839703	521111.285919	43.158669
3503.767110	521086.523078	43.163674
3504.030144	521076.066259	43.168679
3503.554838	521082.512119	43.173684
3503.648457	521072.688797	43.178689
3503.816420	521078.881310	43.183693
3503.436175	521052.296313	43.188698
3503.659930	521052.159982	43.193703
3503.952406	521027.996638	43.198708
3503.624597	521024.762177	43.203713
3503.626833	521038.615513	43.208717
3503.621909	521027.998773	43.213722
3503.808726	521018.868533	43.218727
3504.010663	520997.550835	43.223732
3503.526690	520998.840930	43.228737
3503.757179	520993.546368	43.233741
3503.632421	520989.167478	43.238746
3504.003882	520996.692994	43.243751
3503.634723	520972.229653	43.248756
3503.419591	520949.005947	43.253761
3503.378987	520971.006366	43.258765
3503.552629	520964.810689	43.263770
3503.752664	520958.358037	43.268775
3503.683373	520965.801544	43.273780
3503.613988	520957.621853	43.278785
3503.967920	520924.853343	43.283789
3503.730952	520917.054042	43.288794
3503.626372	520916.160632	43.293799
3503.659922	520934.913494	43.298804
3503.903084	520928.706816	43.303809
3503.627994	520902.357759	43.308813
3503.497647	520893.833746	43.313818
3503.607751	520884.260509	43.318823
3503.426168	520899.760960	43.323828
3503.375203	520888.898602	43.328833
3503.528005	520900.402462	43.333837
3503.536297	520893.727284	43.338842
3503.834113	520873.456047	43.343847
3503.505087	520895.401030	43.348852
3503.881578	520865.662483	43.353857
3504.014611	520844.052110	43.358861
3503.974097	520873.485099	43.363866
3504.259444	520827.328608	43.368871
3503.839802	520835.838766	43.373876
3503.995278	520816.803419	43.378881
3503.815432	520816.427509	43.383885
3503.701217	520798.597667	43.388890
3503.721583	520790.656513	43.393895
3503.713266	520789.596198	43.398900
3503.910894	520777.329328	43.403905
3503.717307	520779.483645	43.408909
3503.376276	520789.346553	43.413914
3503.745031	520754.300111	43.418919
3503.730635	520742.268970	43.423924
3503.553042	520737.847802	43.428929
3503.695511	520756.179164	43.433933
3503.996613	520731.558969	43.438938
3504.033311	520737.974603	43.443943
3503.828886	520726.276851	43.448948
3504.032420	520706.323677	43.453953
3503.939921	520711.091216	43.458957
3503.969953	520709.316976	43.463962
3504.132918	520670.106288	43.468967
3503.966410	520681.054030	43.473972
3503.817529	520661.510430	43.478977
3503.703603	520652.073588	43.483981
3503.707729	520623.960862	43.488986
3503.729633	520647.114752	43.493991
3503.702116	520634.782237	43.498996
3503.616861	520627.312751	43.504001
3504.010487	520632.155166	43.509005
3503.230624	520592.992183	43.514010
3503.245640	520600.725901	43.519015
3503.794891	520593.661734	43.524020
3503.668780	520581.243637	43.529025
3503.565759	520596.276902	43.534029
3503.462500	520603.473134	43.539034
3503.672088	520588.221094	43.544039
3503.370335	520589.027365	43.549044
3503.511038	520583.544615	43.554049
3503.551237	520551.229439	43.559053
3503.168453	520578.947387	43.564058
3503.493657	520560.693906	43.569063
3503.268332	520563.004953	43.574068
3503.411337	520555.297111	43.579073
3503.250688	520556.738385	43.584077
3503.593644	520572.762984	43.589082
3503.794866	520562.618979	43.594087
3503.460834	520580.166297	43.599092
3503.316827	520565.222929	43.604097
3503.537842	520558.513995	43.609101
3503.676269	520561.525979	43.614106
3503.591311	520544.146293	43.619111
3503.686641	520525.423485	43.624116
3503.968987	520517.238546	43.629121
3503.652767	520527.350499	43.634125
3503.444169	520535.220714	43.639130
3503.936537	520517.850879	43.644135
3503.686972	520492.558929	43.649140
3503.506383	520511.598929	43.654145
3503.845169	520486.011734	43.659149
3503.501213	520491.476385	43.664154
3503.423655	520493.157343	43.669159
3503.554823	520495.816552	43.674164
3503.599551	520486.910722	43.679169
3503.859175	520473.420339	43.684173
3503.576120	520463.555061	43.689178
3503.961027	520451.966218	43.694183
3503.940045	520457.480960	43.699188
3503.665528	520450.445803	43.704193
3504.147654	520422.105498	43.709197
3503.813263	520423.169746	43.714202
3504.020622	520418.232591	43.719207
3503.760218	520416.301974	43.724212
3503.664302	520388.406905	43.729217
3503.801362	520380.244860	43.734221
3503.761648	520373.779308	43.739226
3503.744079	520367.815877	43.744231
3503.252261	520383.517533	43.749236
3503.307987	520381.284136	43.754241
3503.702021	520368.480297	43.759245
3503.676346	520360.293399	43.764250
3504.047604	520345.420082	43.769255
3503.748516	520344.709069	43.774260
3503.956638	520342.401018	43.779265
3503.817204	520331.248900	43.784269
3503.362053	520310.944287	43.789274
3503.880882	520303.935368	43.794279
3503.703328	520307.654652	43.799284
3503.673761	520308.519043	43.804289
3504.046792	520299.156724	43.809293
3503.884087	520282.901426	43.814298
3503.590148	520280.065965	43.819303
3503.780696	520270.327969	43.824308
3503.796961	520266.078286	43.829313
3504.060723	520258.300657	43.834317
3503.459639	520261.075635	43.839322
3503.976808	520238.291374	43.844327
3503.837161	520236.291087	43.849332
3503.719905	520226.854527	43.854337
3503.954776	520219.334260	43.859341
3503.605429	520198.911661	43.864346
3503.929354	520190.163796	43.869351
3503.967842	520190.714059	43.874356
3503.691001	520190.353464	43.879361
3504.029303	520176.850403	43.884365
3503.594289	520165.138131	43.889370
3504.148378	520152.005449	43.894375
3503.876657	520157.762172	43.899380
3504.014645	520141.256959	43.904385
3503.925879	520120.186321	43.909389
3504.034325	520117.540051	43.914394
3504.008025	520115.976903	43.919399
3503.818115	520084.809569	43.924404
3503.515112	520086.880142	43.929409
3503.972235	520076.240324	43.934413
3503.416868	520073.446145	43.939418
3503.641898	520089.034785	43.944423
3503.974382	520067.948065	43.949428
3503.625993	520053.643294	43.954433
3503.856761	520039.095285	43.959437
3503.583762	520042.374643	43.964442
3503.495549	520042.540429	43.969447
3503.490435	520048.608997	43.974452
3503.624654	520036.553850	43.979457
3503.701272	520014.647924	43.984461
3503.307661	520010.210137	43.989466
3503.622524	519991.856533	43.994471
3503.401225	520008.881006	43.999476
3503.490567	520009.322111	44.004481
3503.768810	520004.828701	44.009485
3503.411227	520003.823536	44.014490
3503.677224	520004.641229	44.019495
3503.527992	520010.226953	44.024500
3503.197910	519968.817161	44.029505
3503.557715	519973.816810	44.034509
3503.393101	519988.203037	44.039514
3503.494658	519970.135940	44.044519
3503.487340	519968.822596	44.049524
3503.723127	519972.527191	44.054529
3503.914233	519968.249798	44.059533
3503.526930	519988.941108	44.064538
3503.886512	519964.007142	44.069543
3503.522183	519941.058408	44.074548
3503.436741	519937.026969	44.079553
3503.785770	519943.848623	44.084557
3503.420972	519946.839127	44.089562
3504.104835	519914.926608	44.094567
3503.647690	519939.269611	44.099572
3503.902849	519915.515041	44.104577
3504.086845	519899.305697	44.109581
3503.800502	519895.053180	44.114586
3503.782183	519901.578964	44.119591
3503.630798	519864.388027	44.124596
3503.578563	519856.710716	44.129601
3503.619065	519869.345454	44.134605
3503.855805	519847.009486	44.139610
3503.467621	519855.161228	44.144615
3503.547961	519873.655086	44.149620
3503.254536	519850.492764	44.154625
3503.752969	519863.661899	44.159629
3503.998315	519844.055020	44.164634
3503.708791	519828.223828	44.169639
3503.706371	519825.797290	44.174644
3503.759989	519818.558308	44.179649
3503.899987	519805.945874	44.184653
3503.771957	519797.066976	44.189658
3503.919566	519794.363900	44.194663
3503.891474	519777.227237	44.199668
3503.700873	519775.487768	44.204673
3503.536449	519774.452060	44.209677
3503.277404	519766.048929	44.214682
3503.394369	519744.186831	44.219687
3503.157234	519739.168032	44.224692
3503.141867	519753.834261	44.229697
3503.769329	519734.217423	44.234701
3503.614956	519736.871320	44.239706
3503.312197	519754.970780	44.244711
3503.548370	519756.197714	44.249716
3503.429345	519749.441066	44.254721
3503.750522	519740.440576	44.259725
3503.663248	519759.365568	44.264730
3503.651341	519718.966710	44.269735
3503.625785	519720.690092	44.274740
3503.754040	519722.085777	44.279745
3503.656662	519715.325694	44.284749
3503.735140	519720.875527	44.289754
3503.661308	519713.757771	44.294759
3503.787577	519694.826871	44.299764
3503.394020	519676.433188	44.304769
3503.773581	519675.463192	44.309773
3503.638370	519681.249069	44.314778
3503.646148	519673.461059	44.319783
3503.274494	519684.947530	44.324788
3503.529207	519681.418477	44.329793
3504.063494	519669.906607	44.334797
3503.654345	519654.953752	44.339802
3503.823088	519627.167258	44.344807
3503.597765	519652.181950	44.349812
3503.804854	519626.209719	44.354817
3503.933497	519623.863566	44.359821
3503.575627	519614.464683	44.364826
3503.536703	519614.369859	44.369831
3503.801611	519608.007555	44.374836
3503.365002	519606.913726	44.379841
3503.491509	519618.523768	44.384845
3503.497106	519633.591309	44.389850
3503.656278	519615.261894	44.394855
3503.684160	519602.869284	44.399860
3503.602216	519586.600535	44.404865
3503.951957	519572.791784	44.409869
3503.699641	519575.006103	44.414874
3503.988976	519568.842183	44.419879
3503.887092	519558.189253	44.424884
3503.999875	519538.249008	44.429889
3504.121292	519535.499465	44.434893
3503.856799	519540.395656	44.439898
3503.843605	519503.839409	44.444903
3503.565619	519490.079235	44.449908
3503.768083	519495.710678	44.454913
3503.885990	519502.063394	44.459917
3503.593220	519509.441750	44.464922
3503.710965	519489.551227	44.469927
3503.702944	519467.860212	44.474932
3503.448347	519470.378296	44.479937
3503.840539	519452.163567	44.484941
3503.220094	519465.358163	44.489946
3503.531054	519450.392441	44.494951
3503.846205	519463.135778	44.499956
3503.633315	519445.977412	44.504961
3503.686327	519420.737123	44.509965
3503.677501	519425.491809	44.514970
3504.056065	519412.790805	44.519975
3503.926258	519423.632451	44.524980
3503.420223	519403.486454	44.529985
3503.755893	519378.201426	44.534989
3503.654367	519396.016647	44.539994
3503.694052	519386.554801	44.544999
3503.748640	519376.584940	44.550004
3504.030348	519382.608421	44.555009
3503.787105	519374.859943	44.560013
3503.586666	519360.278357	44.565018
3503.731266	519343.215080	44.570023
3503.833010	519345.676865	44.575028
3503.517895	519340.872530	44.580033
3503.886521	519336.920876	44.585037
3503.579344	519323.873094	44.590042
3503.766526	519315.449774	44.595047
3503.414920	519316.112285	44.600052
3503.623183	519307.281103	44.605057
3503.595795	519309.257646	44.610061
3503.483928	519316.253537	44.615066
3503.498187	519305.582088	44.620071
3503.565956	519278.164925	44.625076
3503.560882	519279.126630	44.630081
3503.894993	519261.881620	44.635085
3503.304936	519287.055641	44.640090
3503.705449	519271.367683	44.645095
3503.484000	519254.564431	44.650100
3503.190424	519278.933120	44.655105
3504.033507	519269.394797	44.660109
3503.294449	519251.662034	44.665114
3503.614039	519233.711368	44.670119
3503.820381	519240.404169	44.675124
3503.675022	519228.139790	44.680129
3503.815530	519231.151690	44.685133
3503.695443	519222.220660	44.690138
3503.710321	519232.685602	44.695143
3503.708593	519200.829497	44.700148
3503.330104	519196.186835	44.705153
3503.551994	519193.825883	44.710157
3503.270677	519204.034260	44.715162
3503.775931	519186.054199	44.720167
3503.886336	519186.744828	44.725172
3503.441497	519200.013012	44.730177
3503.670617	519184.807155	44.735181
3503.852512	519170.518936	44.740186
3503.660234	519154.924558	44.745191
3503.389233	519170.946426	44.750196
3503.512036	519153.481870	44.755201
3503.938567	519155.133859	44.760205
3503.874949	519155.245200	44.765210
3503.596341	519112.156438	44.770215
3503.900992	519118.732619	44.775220
3503.543653	519123.036811	44.780225
3503.903351	519109.276667	44.785229
3503.557925	519108.775186	44.790234
3503.546922	519088.449432	44.795239
3503.496727	519087.142795	44.800244
3503.332120	519085.753107	44.805249
3503.691266	519062.739371	44.810253
3503.525867	519078.946905	44.815258
3503.367587	519078.061880	44.820263
3503.684179	519083.574294	44.825268
3503.160810	519087.803604	44.830273
3503.408259	519074.465702	44.835277
3503.205703	519085.167368	44.840282
3503.565919	519080.711319	44.845287
3503.566101	519086.324306	44.850292
3503.094052	519079.016382	44.855297
3503.869269	519087.793688	44.860301
3503.700728	519055.154606	44.865306
3503.568973	519055.074451	44.870311
3503.856042	519037.836643	44.875316
3503.538104	519073.890334	44.880321
3503.530279	519043.703579	44.885325
3503.473493	519051.752772	44.890330
3503.219706	519036.016303	44.895335
3503.600826	519038.990210	44.900340
3503.176194	519035.517823	44.905345
3503.478605	519025.306316	44.910349
3503.061204	519042.413344	44.915354
3503.340740	519029.019768	44.920359
3503.560748	519015.635589	44.925364
3503.431012	519023.848024	44.930369
3503.299114	519030.290970	44.935373
3503.368479	519026.942772	44.940378
3503.096900	519028.705109	44.945383
3503.328280	519027.101132	44.950388
3503.153165	519037.849058	44.955393
3503.711906	519029.012902	44.960397
3503.583110	519042.736927	44.965402
3503.239705	519027.823678	44.970407
3503.364143	519053.289661	44.975412
3503.338302	519045.354969	44.980417
3503.637982	519035.497865	44.985421
3503.335306	519054.103743	44.990426
3503.447050	519038.258938	44.995431
3503.822838	519032.283421	45.000436
3503.373614	519027.601324	45.005441
3503.694607	518995.542118	45.010445
3503.383213	518986.995163	45.015450
3503.444698	519019.550474	45.020455
3503.317459	518983.617898	45.025460
3503.294639	519015.883142	45.030465
3503.454950	518981.320977	45.035469
3503.186037	519014.990416	45.040474
3503.726714	518993.161489	45.045479
3503.634051	519007.638332	45.050484
3503.412769	519013.286346	45.055489
3503.580868	518982.060344	45.060493
3503.585686	518993.892326	45.065498
3503.464390	518981.118294	45.070503
3503.467885	518964.683728	45.075508
3503.426696	518976.219594	45.080513
3503.885748	518977.158529	45.085517
3503.593352	518968.204028	45.090522
3503.590870	518984.790438	45.095527
3503.862874	518953.800793	45.100532
3503.382106	518952.764464	45.105537
3504.156149	518922.959583	45.110541
3503.431278	518939.862478	45.115546
3503.649794	518910.448776	45.120551
3503.669994	518948.168572	45.125556
3503.213896	518929.935639	45.130561
3503.643646	518904.635019	45.135565
3503.253247	518936.958511	45.140570
3503.412509	518891.372763	45.145575
3503.815280	518879.830565	45.150580
3503.656652	518922.989345	45.155585
3503.521949	518900.255703	45.160589
3503.271266	518891.800237	45.165594
3503.970331	518869.642714	45.170599
3503.687952	518888.397271	45.175604
3503.565529	518905.710653	45.180609
3503.864174	518886.701018	45.185613
3503.572090	518858.986066	45.190618
3503.799780	518819.457345	45.195623
3503.789094	518832.707773	45.200628
3503.178418	518873.359206	45.205633
3503.793235	518834.426707	45.210637
3503.596305	518857.415430	45.215642
3503.489115	518820.114020	45.220647
3503.633386	518845.172652	45.225652
3503.262124	518818.228652	45.230657
3503.709951	518819.776175	45.235661
3503.544097	518817.122484	45.240666
3503.684722	518842.029996	45.245671
3503.843357	518792.348141	45.250676
3503.422450	518814.765515	45.255681
3503.840872	518782.033125	45.260685
3503.947139	518777.010325	45.265690
3503.882618	518790.471563	45.270695
3503.619414	518770.084144	45.275700
3503.788042	518785.986335	45.280705
3504.017113	518747.519137	45.285709
3503.884803	518739.449423	45.290714
3503.967640	518757.944136	45.295719
3504.154558	518703.251378	45.300724
3503.598416	518719.925558	45.305729
3503.772280	518686.270850	45.310733
3503.823729	518705.023421	45.315738
3503.730112	518700.133323	45.320743
3503.545586	518657.028505	45.325748
3503.615132	518688.723544	45.330753
3503.814346	518650.715947	45.335757
3503.715556	518676.369495	45.340762
3503.779131	518658.458670	45.345767
3503.786423	518630.594884	45.350772
3503.399208	518649.265145	45.355777
3503.821383	518611.475058	45.360781
3503.443637	518634.088126	45.365786
3503.359400	518625.707352	45.370791
3503.617536	518615.098049	45.375796
3503.191755	518646.163506	45.380801
3503.898160	518603.423415	45.385805
3503.553012	518640.342002	45.390810
3503.493873	518607.179068	45.395815
3503.737862	518591.515206	45.400820
3503.690101	518577.060501	45.405825
3503.594448	518597.960294	45.410829
3503.764272	518582.409280	45.415834
3503.739632	518584.638314	45.420839
3503.316368	518580.356528	45.425844
3503.442968	518551.462395	45.430849
3503.625897	518535.605859	45.435853
3503.460011	518533.002694	45.440858
3503.329611	518562.403447	45.445863
3503.710027	518544.998670	45.450868
3503.356079	518554.258134	45.455873
3503.480348	518547.816516	45.460877
3503.372298	518552.182592	45.465882
3503.040420	518568.366368	45.470887
3503.477311	518554.947539	45.475892
3503.104250	518540.190240	45.480897
3503.095652	518560.368369	45.485901
3503.261906	518548.964458	45.490906
3503.608604	518519.580371	45.495911
3503.402722	518571.900350	45.500916
3503.391051	518564.570002	45.505921
3503.685894	518548.796927	45.510925
3503.417338	518544.086136	45.515930
3503.613834	518497.583195	45.520935
3503.604198	518532.577975	45.525940
3503.477431	518514.848781	45.530945
3503.657199	518530.901161	45.535949
3503.500269	518507.159131	45.540954
3503.461127	518508.025129	45.545959
3503.483019	518526.782573	45.550964
3503.431678	518534.780588	45.555969
3503.751066	518518.396789	45.560973
3503.154543	518504.180456	45.565978
3503.517754	518489.509017	45.570983
3503.710237	518487.557159	45.575988
3503.450145	518490.834781	45.580993
3503.692594	518481.289803	45.585997
3503.706464	518497.065026	45.591002
3503.744272	518495.491593	45.596007
3503.738543	518489.879589	45.601012
3503.484796	518470.299395	45.606017
3503.610390	518457.435370	45.611021
3503.395019	518463.588319	45.616026
3503.910947	518455.921696	45.621031
3503.779763	518463.173841	45.626036
3503.469718	518477.179822	45.631041
3503.748462	518447.958053	45.636045
3503.458954	518424.540268	45.641050
3503.215498	518427.208453	45.646055
3503.388336	518422.225592	45.651060
3503.281193	518410.713092	45.656065
3503.394529	518421.466395	45.661069
3503.517832	518425.947644	45.666074
3503.586670	518407.631169	45.671079
3503.737855	518407.708565	45.676084
3503.539413	518428.574248	45.681089
3503.590575	518426.948129	45.686093
3503.693441	518413.834821	45.691098
3503.115522	518397.289309	45.696103
3503.389393	518386.171689	45.701108
3503.269341	518387.910144	45.706113
3503.711024	518377.322248	45.711117
3503.670371	518386.785132	45.716122
3503.427669	518397.139607	45.721127
3504.160895	518379.982306	45.726132
3503.656498	518390.782693	45.731137
3503.637257	518368.434620	45.736141
3503.461307	518359.006267	45.741146
3503.514715	518347.670622	45.746151
3503.347656	518349.365942	45.751156
3503.716907	518349.510011	45.756161
3503.238289	518337.651622	45.761165
3502.951084	518366.875230	45.766170
3503.589571	518343.158956	45.771175
3503.698576	518355.430045	45.776180
3503.488921	518369.319112	45.781185
3503.682157	518342.891941	45.786189
3503.608438	518338.757121	45.791194
3503.558505	518318.133162	45.796199
3503.789779	518309.752931	45.801204
3503.745040	518323.514835	45.806209
3503.830001	518312.932709	45.811213
3503.937882	518308.617473	45.816218
3503.718326	518296.515836	45.821223
3503.503112	518287.295923	45.826228
3503.560317	518275.251665	45.831233
3503.893119	518274.491257	45.836237
3503.638065	518271.396456	45.841242
3503.541903	518276.670963	45.846247
3503.751324	518228.243611	45.851252
3503.422081	518263.137766	45.856257
3503.540521	518224.535133	45.861261
3503.353784	518245.955454	45.866266
3503.422467	518241.747535	45.871271
3503.680751	518220.821897	45.876276
3503.353366	518249.748648	45.881281
3503.324046	518241.409569	45.886285
3503.552529	518239.148579	45.891290
3503.576471	518256.692351	45.896295
3503.554140	518218.213090	45.901300
3503.532477	518222.869013	45.906305
3503.766909	518195.828269	45.911309
3503.849866	518200.265386	45.916314
3503.376185	518194.170982	45.921319
3503.600622	518203.086383	45.926324
3503.140214	518207.154255	45.931329
3503.799863	518174.079127	45.936333
3503.334566	518206.365311	45.941338
3503.191917	518176.754544	45.946343
3503.350733	518183.556424	45.951348
3503.623363	518167.381945	45.956353
3503.781512	518153.754002	45.961357
3503.591027	518176.439235	45.966362
3503.292324	518155.601546	45.971367
3503.817528	518179.286182	45.976372
3503.523416	518161.583059	45.981377
3503.540088	518174.374567	45.986381
3503.719125	518155.585275	45.991386
3503.762859	518144.402728	45.996391
3503.550052	518139.733579	46.001396
3503.252974	518124.003084	46.006401
3503.691797	518110.179038	46.011405
3503.258692	518129.008844	46.016410
3503.401607	518124.586885	46.021415
3503.579524	518141.550182	46.026420
3503.371962	518115.691686	46.031425
3503.302876	518141.745920	46.036429
3503.917375	518125.365661	46.041434
3503.531321	518136.602632	46.046439
3503.518609	518079.764892	46.051444
3502.900338	518112.378852	46.056449
3503.479075	518069.455288	46.061453
3503.525618	518105.099493	46.066458
3503.571089	518090.022797	46.071463
3504.171815	518076.223703	46.076468
3503.561729	518111.567118	46.081473
3503.753251	518051.157150	46.086477
3503.359043	518081.055576	46.091482
3503.566617	518064.436154	46.096487
3503.395535	518040.695693	46.101492
3503.511415	518031.827864	46.106497
3503.454968	518079.726226	46.111501
3503.446768	518067.135891	46.116506
3503.482657	518035.676155	46.121511
3504.013926	518056.477545	46.126516
3503.435077	518049.540028	46.131521
3503.855051	518003.101521	46.136525
3503.258735	518028.935843	46.141530
3503.637510	517995.095638	46.146535
3503.873908	518033.187904	46.151540
3503.514583	517998.250692	46.156545
3503.826350	518033.145158	46.161549
3503.725217	517988.558904	46.166554
3503.737870	517994.827696	46.171559
3503.893746	517953.740605	46.176564
3503.612321	518002.585002	46.181569
3503.669801	517974.358193	46.186573
3503.471722	517954.313464	46.191578
3503.789156	517973.682231	46.196583
3503.099190	517947.798577	46.201588
3503.269492	517923.953423	46.206593
3503.449126	517950.929475	46.211597
3503.583402	517933.107832	46.216602
3503.269867	517965.016509	46.221607
3503.848381	517970.993597	46.226612
3503.717201	517943.555100	46.231617
3503.865297	517915.516149	46.236621
3503.824397	517944.903850	46.241626
3503.904468	517898.215353	46.246631
3503.825272	517915.624076	46.251636
3503.481753	517910.975522	46.256641
3503.986427	517889.454257	46.261645
3503.876034	517879.711850	46.266650
3503.474212	517879.522662	46.271655
3503.353589	517895.370283	46.276660
3503.243124	517868.080097	46.281665
3503.517517	517874.459277	46.286669
3503.296879	517895.531418	46.291674
3503.390131	517875.541688	46.296679
3503.834452	517881.135459	46.301684
3503.562801	517876.070976	46.306689
3503.258743	517873.438974	46.311693
3502.971298	517885.368510	46.316698
3503.203512	517859.794099	46.321703
3503.197845	517890.036020	46.326708
3503.700642	517887.124788	46.331713
3503.502367	517852.869796	46.336717
3503.595211	517859.985657	46.341722
3503.434709	517832.197619	46.346727
3503.757908	517849.138253	46.351732
3503.734570	517849.394946	46.356737
3503.431279	517834.878840	46.361741
3503.437670	517852.526954	46.366746
3503.201159	517821.969557	46.371751
3503.560225	517849.524256	46.376756
3503.385863	517814.355143	46.381761
3503.701964	517834.482836	46.386765
3503.630386	517835.303425	46.391770
3503.192353	517799.164550	46.396775
3503.872901	517786.768569	46.401780
3503.361536	517793.625961	46.406785
3503.093324	517815.514845	46.411789
3503.304344	517788.628850	46.416794
3503.644938	517808.853844	46.421799
3503.227021	517804.672150	46.426804
3503.599017	517794.347750	46.431809
3503.253856	517807.955281	46.436813
3503.713017	517789.171872	46.441818
3503.329372	517837.122646	46.446823
3503.866607	517799.059676	46.451828
3503.593293	517782.010274	46.456833
3502.950539	517774.779319	46.461837
3504.014734	517738.605168	46.466842
3503.379153	517787.354461	46.471847
3503.504095	517776.108260	46.476852
3503.148085	517752.548325	46.481857
3503.807772	517758.512662	46.486861
3503.576590	517782.317412	46.491866
3503.530703	517751.780328	46.496871
3503.804240	517762.609881	46.501876
3503.184179	517756.943013	46.506881
3503.417321	517724.288393	46.511885
3503.339408	517740.382264	46.516890
3503.496103	517708.144259	46.521895
3503.422054	517746.134538	46.526900
3503.475341	517748.857072	46.531905
3503.531660	517717.342933	46.536909
3503.337138	517744.884159	46.541914
3503.414811	517731.470872	46.546919
3503.738351	517732.127877	46.551924
3503.668463	517716.512799	46.556929
3503.474386	517725.090039	46.561933
3503.498961	517688.068680	46.566938
3503.259250	517702.721613	46.571943
3503.571310	517664.643354	46.576948
3503.244364	517722.547914	46.581953
3503.005751	517695.176556	46.586957
3503.734105	517670.888846	46.591962
3503.215181	517688.569589	46.596967
3503.308746	517724.864596	46.601972
3503.545390	517688.163713	46.606977
3503.374366	517670.642894	46.611981
3503.497172	517716.238293	46.616986
3503.434776	517701.886280	46.621991
3503.380212	517693.955480	46.626996
3503.829775	517668.902701	46.632001
3503.855500	517707.079582	46.637005
3503.695793	517681.870264	46.642010
3503.260950	517650.989904	46.647015
3503.666368	517660.028706	46.652020
3503.459357	517666.130057	46.657025
3503.478188	517639.071913	46.662029
3503.520273	517671.380084	46.667034
3503.308982	517678.291237	46.672039
3503.985978	517635.957874	46.677044
3503.366740	517668.775138	46.682049
3503.226349	517632.588858	46.687053
3503.612590	517616.446459	46.692058
3503.087092	517644.090733	46.697063
3503.314216	517625.596666	46.702068
3503.610884	517602.641354	46.707073
3503.621699	517634.398260	46.712077
3503.484594	517627.289606	46.717082
3503.710749	517600.805481	46.722087
3503.356850	517633.328024	46.727092
3503.112098	517656.882244	46.732097
3503.528675	517620.001061	46.737101
3504.136707	517596.389680	46.742106
3503.488036	517592.446686	46.747111
3503.557780	517602.398276	46.752116
3503.455453	517566.559833	46.757121
3503.259096	517607.604016	46.762125
3503.342388	517610.271260	46.767130
3503.538630	517578.026752	46.772135
3504.177064	517556.281633	46.777140
3503.219393	517586.623998	46.782145
3503.628787	517587.115727	46.787149
3503.823126	517547.032969	46.792154
3503.556102	517575.951351	46.797159
3503.737520	517524.542689	46.802164
3503.446745	517568.636156	46.807169
3503.089101	517557.010941	46.812173
3503.678440	517528.294748	46.817178
3503.288521	517563.048248	46.822183
3503.736572	517525.150461	46.827188
3503.502385	517564.228458	46.832193
3503.141953	517536.016384	46.837197
3503.761034	517494.399809	46.842202
3503.091484	517544.166605	46.847207
3503.135868	517511.187403	46.852212
3503.611404	517487.141669	46.857217
3503.538700	517527.509080	46.862221
3503.437554	517546.641075	46.867226
3503.208877	517522.504408	46.872231
3503.798781	517483.471542	46.877236
3503.363450	517510.090363	46.882241
3503.210653	517540.002176	46.887245
3503.443343	517519.383129	46.892250
3503.535528	517489.026025	46.897255
3503.634757	517501.602718	46.902260
3503.372453	517525.261040	46.907265
3503.253119	517515.823260	46.912269
3503.059121	517484.550528	46.917274
3503.418651	517480.498732	46.922279
3503.576946	517479.260158	46.927284
3503.221838	517518.660801	46.932289
3503.492325	517509.515403	46.937293
3503.642623	517490.123049	46.942298
3503.556273	517460.350393	46.947303
3503.524002	517454.590520	46.952308
3503.701005	517501.947937	46.957313
3503.493680	517485.191227	46.962317
3503.155234	517474.119203	46.967322
3503.788638	517452.425315	46.972327
3503.552326	517454.991383	46.977332
3503.261944	517482.093052	46.982337
3503.379436	517464.475845	46.987341
3503.212359	517435.929615	46.992346
3503.541828	517424.448566	46.997351
3503.472869	517421.931049	47.002356
3503.270209	517468.741709	47.007361
3503.358443	517473.380472	47.012365
3503.048235	517454.212572	47.017370
3503.419200	517441.662979	47.022375
3503.778232	517447.826662	47.027380
3503.548182	517449.734313	47.032385
3503.643894	517443.043925	47.037389
3503.816652	517468.454135	47.042394
3503.605680	517430.104006	47.047399
3503.980574	517397.729771	47.052404
3503.674955	517413.859947	47.057409
3503.533408	517404.021042	47.062413
3503.769454	517409.850176	47.067418
3503.846644	517396.537838	47.072423
3504.113016	517357.050096	47.077428
3503.536288	517390.417476	47.082433
3503.435872	517357.359712	47.087437
3503.691217	517374.311555	47.092442
3503.854745	517348.747216	47.097447
3504.048557	517370.007375	47.102452
3503.855124	517328.417660	47.107457
3503.770050	517345.271621	47.112461
3503.786313	517320.843090	47.117466
3503.207140	517332.060552	47.122471
3504.029423	517307.352895	47.127476
3503.739067	517295.312288	47.132481
3503.523513	517313.097196	47.137485
3503.817589	517275.779467	47.142490
3503.887089	517292.406763	47.147495
3503.623248	517298.213800	47.152500
3504.151791	517260.707265	47.157505
3503.515692	517257.267921	47.162509
3503.785027	517250.499443	47.167514
3503.529346	517255.293766	47.172519
3503.658720	517263.820122	47.177524
3503.196921	517232.791529	47.182529
3503.282687	517229.187518	47.187533
3503.337913	517215.726790	47.192538
3503.838661	517202.043922	47.197543
3503.256797	517240.671907	47.202548
3503.189064	517210.440714	47.207553
3503.372191	517216.986288	47.212557
3503.675046	517209.251628	47.217562
3503.089935	517226.943319	47.222567
3503.379576	517203.280560	47.227572
3503.606199	517229.694062	47.232577
3503.254774	517213.060997	47.237581
3503.389171	517236.050167	47.242586
3503.410060	517213.441338	47.247591
3503.646699	517244.859863	47.252596
3503.649242	517219.775917	47.257601
3503.698115	517223.510675	47.262605
3503.584263	517179.278265	47.267610
3503.436141	517211.566819	47.272615
3503.871257	517181.913536	47.277620
3504.087987	517166.556075	47.282625
3503.539404	517197.643644	47.287629
3504.016324	517162.673652	47.292634
3503.755750	517144.610137	47.297639
3503.947097	517144.377760	47.302644
3503.445406	517163.067779	47.307649
3503.785803	517127.461851	47.312653
3503.474479	517118.812773	47.317658
3503.725444	517114.019464	47.322663
3503.670831	517105.532095	47.327668
3503.720802	517110.126435	47.332673
3503.301119	517096.639526	47.337677
3503.200889	517126.998924	47.342682
3503.125885	517093.279179	47.347687
3503.239919	517114.956853	47.352692
3503.503947	517093.523168	47.357697
3503.175134	517120.833788	47.362701
3503.497382	517083.713466	47.367706
3503.208096	517123.660935	47.372711
3503.820370	517111.275246	47.377716
3503.600603	517086.883676	47.382721
3503.416503	517093.588484	47.387725
3503.977431	517056.834958	47.392730
3503.322125	517080.606597	47.397735
3503.928030	517063.366925	47.402740
3503.319435	517085.108276	47.407745
3503.638701	517070.796542	47.412749
3503.676526	517068.565529	47.417754
3503.689803	517048.031149	47.422759
3503.383918	517032.402156	47.427764
3503.597294	517042.938251	47.432769
3503.489137	517031.070947	47.437773
3503.689765	517026.234995	47.442778
3503.454997	517042.860057	47.447783
3503.757703	517023.999371	47.452788
3503.522160	517025.402212	47.457793
3503.594377	517029.082751	47.462797
3504.041244	516981.625696	47.467802
3503.373760	516987.901217	47.472807
3503.608327	516991.556105	47.477812
3503.825966	516980.497008	47.482817
3503.343094	516987.704234	47.487821
3503.674809	516966.512552	47.492826
3503.734646	516997.150324	47.497831
3503.891339	516976.896627	47.502836
3503.355843	516966.715144	47.507841
3503.180936	516941.203670	47.512845
3503.926404	516928.189920	47.517850
3503.436648	516960.330663	47.522855
3503.264850	516938.308215	47.527860
3503.885407	516910.850349	47.532865
3503.395349	516912.546290	47.537869
3503.681004	516925.195100	47.542874
3503.352251	516893.133388	47.547879
3503.471312	516873.138377	47.552884
3503.481412	516924.266221	47.557889
3503.287592	516897.139335	47.562893
3503.890964	516881.214774	47.567898
3503.265185	516923.946846	47.572903
3503.611358	516889.047518	47.577908
3503.574229	516923.443154	47.582913
3503.577396	516862.097756	47.587917
3503.429230	516868.594682	47.592922
3503.521111	516894.827719	47.597927
3503.834012	516851.690171	47.602932
3503.666448	516857.937302	47.607937
3502.990271	516876.756364	47.612941
3504.041061	516849.533837	47.617946
3503.385150	516887.466317	47.622951
3503.398598	516842.707165	47.627956
3503.486244	516851.392046	47.632961
3503.410823	516849.836353	47.637965
3503.451133	516813.569161	47.642970
3503.451283	516828.690684	47.647975
3503.139987	516823.783863	47.652980
3503.285529	516800.244455	47.657985
3503.082979	516819.140445	47.662989
3503.213302	516837.579218	47.667994
3502.832313	516837.993599	47.672999
3503.242530	516811.377984	47.678004
3503.489142	516852.910319	47.683009
3503.233604	516831.002111	47.688013
3503.869249	516812.847163	47.693018
3503.067836	516854.292269	47.698023
3503.454736	516810.030309	47.703028
3503.359620	516859.758929	47.708033
3503.007891	516847.373686	47.713037
3503.880705	516814.211599	47.718042
3503.506538	516849.065242	47.723047
3503.148874	516840.625636	47.728052
3503.563384	516816.335715	47.733057
3503.317857	516866.290381	47.738061
3503.273419	516836.712279	47.743066
3503.674766	516827.950412	47.748071
3503.450669	516835.976548	47.753076
3503.603419	516792.054987	47.758081
3503.187867	516810.782358	47.763085
3503.692138	516789.866620	47.768090
3503.499444	516787.520283	47.773095
3503.410125	516803.869728	47.778100
3503.462316	516793.746976	47.783105
3503.080059	516806.804878	47.788109
3503.603675	516766.668203	47.793114
3503.550594	516769.104269	47.798119
3503.624619	516798.425255	47.803124
3503.764128	516820.605018	47.808129
3503.581634	516823.617835	47.813133
3503.701035	516777.880872	47.818138
3503.587321	516752.359437	47.823143
3503.579954	516771.932660	47.828148
3503.743143	516739.944622	47.833153
3503.614540	516779.867518	47.838157
3503.301026	516756.248880	47.843162
3503.851757	516733.049924	47.848167
3503.769576	516742.368586	47.853172
3503.899482	516729.907133	47.858177
3503.760839	516695.488613	47.863181
3503.798125	516728.760269	47.868186
3503.494301	516716.316783	47.873191
3503.629941	516689.491503	47.878196
3503.469100	516719.608353	47.883201
3503.359952	516692.214884	47.888205
3503.891943	516652.632921	47.893210
3503.438385	516697.411876	47.898215
3503.586908	516715.392745	47.903220
3503.510774	516691.584778	47.908225
3503.227053	516686.521838	47.913229
3503.395676	516692.968764	47.918234
3503.556141	516677.720894	47.923239
3503.334110	516685.139891	47.928244
3503.504842	516673.885711	47.933249
3503.618125	516622.282743	47.938253
3503.302304	516667.748041	47.943258
3503.234840	516678.733343	47.948263
3503.576705	516651.622541	47.953268
3503.402787	516664.344184	47.958273
3503.470070	516660.995840	47.963277
3503.280014	516665.375370	47.968282
3503.601452	516635.789659	47.973287
3503.650734	516632.595875	47.978292
3503.540391	516677.017197	47.983297
3503.343027	516648.322683	47.988301
3503.920823	516589.161281	47.993306
3503.208793	516631.401994	47.998311
3503.261251	516620.874504	48.003316
3503.621380	516615.912078	48.008321
3503.120536	516637.738127	48.013325
3503.410878	516602.290713	48.018330
3503.591123	516651.672988	48.023335
3503.584863	516613.440346	48.028340
3503.741561	516610.836467	48.033345
3503.404198	516653.624794	48.038349
3503.887975	516619.613483	48.043354
3503.367649	516588.340070	48.048359
3503.541963	516586.795456	48.053364
3503.438797	516588.177411	48.058369
3503.638077	516562.049903	48.063373
3503.742649	516596.170947	48.068378
3503.656705	516563.261043	48.073383
3503.704578	516556.527287	48.078388
3503.753536	516568.960907	48.083393
3503.127388	516540.991439	48.088397
3503.803234	516518.682746	48.093402
3503.842621	516539.310909	48.098407
3503.323972	516543.337812	48.103412
3503.541093	516532.430223	48.108417
3503.650242	516515.470796	48.113421
3503.619380	516493.071466	48.118426
3503.483507	516508.063055	48.123431
3503.454318	516522.228583	48.128436
3503.306289	516505.815534	48.133441
3503.463920	516472.158915	48.138445
3503.556382	516498.139612	48.143450
3503.518109	516519.134094	48.148455
3503.487488	516480.601553	48.153460
3503.630040	516505.107670	48.158465
3503.083132	516489.516260	48.163469
3503.537887	516528.487795	48.168474
3503.332633	516519.315899	48.173479
3503.655993	516474.203333	48.178484
3503.156671	516491.831666	48.183489
3503.114178	516454.261851	48.188493
3503.564797	516475.533139	48.193498
3503.059165	516471.820137	48.198503
3503.129948	516434.788692	48.203508
3503.245702	516494.852817	48.208513
3503.453823	516479.293788	48.213517
3503.036926	516495.644734	48.218522
3503.121812	516490.220031	48.223527
3503.015880	516493.271380	48.228532
3503.217846	516505.326845	48.233537
3503.122133	516501.093895	48.238541
3503.547173	516513.822137	48.243546
3503.364908	516519.009659	48.248551
3503.403445	516498.672908	48.253556
3503.499862	516530.013795	48.258561
3503.570233	516501.175565	48.263565
3503.500859	516477.214501	48.268570
3503.501750	516465.987024	48.273575
3503.425600	516483.194464	48.278580
3503.800064	516458.404612	48.283585
3503.270890	516473.964135	48.288589
3503.913781	516453.026068	48.293594
3503.592852	516464.607888	48.298599
3503.390076	516468.079143	48.303604
3503.468104	516429.529312	48.308609
3503.347014	516425.907247	48.313613
3503.387012	516439.303293	48.318618
3503.311572	516428.947620	48.323623
3503.483947	516442.322743	48.328628
3503.611226	516427.535059	48.333633
3503.557523	516434.067798	48.338637
3503.384283	516418.012668	48.343642
3503.696494	516452.859804	48.348647
3503.756823	516424.731069	48.353652
3503.739872	516429.184451	48.358657
3503.421098	516404.706382	48.363661
3503.451807	516406.320065	48.368666
3503.118072	516388.115570	48.373671
3503.229234	516392.700436	48.378676
3503.205579	516403.527272	48.383681
3503.165557	516393.115404	48.388685
3503.412490	516409.563814	48.393690
3503.788871	516383.762058	48.398695
3503.704136	516407.039878	48.403700
3503.651512	516384.188672	48.408705
3503.672079	516408.107316	48.413709
3503.754763	516384.577257	48.418714
3503.295711	516355.063831	48.423719
3503.235579	516373.229771	48.428724
3503.436508	516346.494771	48.433729
3503.262127	516346.674210	48.438733
3503.202350	516361.148156	48.443738
3503.619914	516353.040949	48.448743
3503.529350	516356.140469	48.453748
3503.641646	516360.269993	48.458753
3503.601391	516359.669614	48.463757
3503.590312	516347.027860	48.468762
3503.368021	516371.237814	48.473767
3503.187649	516348.963070	48.478772
3503.906739	516326.090965	48.483777
3503.208600	516355.484195	48.488781
3503.251605	516310.718945	48.493786
3503.356662	516332.753077	48.498791
3503.256501	516329.582855	48.503796
3503.231467	516307.182355	48.508801
3503.504498	516289.134727	48.513805
3503.503440	516330.050035	48.518810
3503.427075	516305.331209	48.523815
3503.164650	516332.329175	48.528820
3503.385385	516310.901330	48.533825
3503.692264	516295.174798	48.538829
3503.352663	516331.895323	48.543834
3503.558178	516332.267593	48.548839
3503.329769	516298.267040	48.553844
3503.481298	516321.153614	48.558849
3503.451307	516327.075750	48.563853
3503.921755	516298.123363	48.568858
3503.254096	516301.516402	48.573863
3503.489399	516270.628715	48.578868
3503.129075	516292.078980	48.583873
3503.465447	516263.198298	48.588877
3503.363005	516291.233118	48.593882
3503.536232	516261.063272	48.598887
3503.505592	516287.518927	48.603892
3503.357506	516286.328690	48.608897
3503.035960	516278.034813	48.613901
3504.062932	516252.838079	48.618906
3503.736015	516270.338246	48.623911
3503.096496	516295.423451	48.628916
3503.706855	516250.618946	48.633921
3503.148229	516274.224723	48.638925
3503.605011	516252.102023	48.643930
3503.262648	516266.519564	48.648935
3503.787059	516239.682693	48.653940
3503.472150	516266.739634	48.658945
3503.445715	516255.920935	48.663949
3503.599690	516248.613961	48.668954
3503.501599	516242.307748	48.673959
3503.179598	516268.758908	48.678964
3503.899302	516236.125626	48.683969
3503.426306	516242.876434	48.688973
3503.430684	516226.995348	48.693978
3503.476456	516191.282268	48.698983
3503.272565	516225.452820	48.703988
3503.370940	516198.329193	48.708993
3503.055849	516235.754106	48.713997
3503.416006	516191.646462	48.719002
3503.313946	516230.453822	48.724007
3503.080523	516209.097626	48.729012
3503.193676	516218.233982	48.734017
3503.363385	516200.961214	48.739021
3503.301377	516225.752947	48.744026
3503.444979	516207.675112	48.749031
3503.203992	516209.129456	48.754036
3503.356463	516225.542402	48.759041
3503.247085	516197.237807	48.764045
3503.510451	516225.366646	48.769050
3503.314831	516210.427505	48.774055
3503.652127	516197.174251	48.779060
3503.323290	516239.658838	48.784065
3503.227888	516217.926815	48.789069
3503.607124	516207.347419	48.794074
3502.920543	516226.168854	48.799079
3503.002749	516189.489085	48.804084
3503.269962	516237.645036	48.809089
3503.407585	516209.706024	48.814093
3503.457660	516231.799554	48.819098
3503.462846	516200.189482	48.824103
3503.279733	516246.393577	48.829108
3503.602950	516207.804484	48.834113
3503.407700	516221.945937	48.839117
3503.260331	516220.300406	48.844122
3503.175756	516196.037891	48.849127
3503.263912	516217.821970	48.854132
3503.324413	516207.090649	48.859137
3503.165126	516223.502295	48.864141
3503.171441	516204.687530	48.869146
3503.329861	516228.483493	48.874151
3503.068237	516244.810143	48.879156
3503.393032	516208.243799	48.884161
3503.218952	516249.591250	48.889165
3503.476730	516231.950571	48.894170
3503.104679	516214.409417	48.899175
3503.068219	516246.530463	48.904180
3503.086262	516223.819593	48.909185
3503.157506	516242.217786	48.914189
3503.335372	516237.182906	48.919194
3503.699091	516215.428891	48.924199
3503.322615	516226.665629	48.929204
3503.707699	516203.441546	48.934209
3503.241012	516180.453203	48.939213
3503.310128	516197.031077	48.944218
3503.261195	516188.137743	48.949223
3503.114259	516207.278510	48.954228
3503.413165	516199.847459	48.959233
3503.322943	516197.383692	48.964237
3503.312119	516191.923444	48.969242
3502.962060	516209.174458	48.974247
3503.262487	516197.545434	48.979252
3503.411384	516200.455411	48.984257
3503.227074	516193.606480	48.989261
3503.060045	516220.488398	48.994266
3503.443864	516185.935679	48.999271
3503.138597	516223.611943	49.004276
3503.490587	516184.310197	49.009281
3502.787111	516231.254055	49.014285
3503.206272	516201.803857	49.019290
3503.547000	516197.855876	49.024295
3503.099997	516215.678531	49.029300
3503.469310	516214.457089	49.034305
3503.473451	516212.180710	49.039309
3503.276275	516212.212028	49.044314
3503.232125	516221.929568	49.049319
3502.962311	516226.068943	49.054324
3503.274025	516216.258849	49.059329
3502.906797	516224.206749	49.064333
3503.489445	516211.926230	49.069338
3503.236180	516217.479093	49.074343
3503.173538	516221.788025	49.079348
3503.159140	516223.004255	49.084353
3503.320517	516220.247852	49.089357
3503.589804	516200.936345	49.094362
3503.212018	516219.203232	49.099367
3503.282568	516213.426679	49.104372
3503.610643	516208.469200	49.109377
3503.264359	516217.475869	49.114381
3503.416743	516215.732387	49.119386
3503.550396	516223.449398	49.124391
3503.294475	516224.198050	49.129396
3503.183454	516212.886941	49.134401
3502.842882	516242.881331	49.139405
3502.996778	516221.817961	49.144410
3503.169736	516224.218380	49.149415
3503.005232	516244.120507	49.154420
3503.275413	516216.514580	49.159425
3503.410861	516226.557758	49.164429
3503.428467	516237.934504	49.169434
3503.351436	516212.962772	49.174439
3503.602333	516228.449807	49.179444
3503.529945	516226.084376	49.184449
3503.318426	516220.099532	49.189453
3503.498421	516237.064442	49.194458
3503.387693	516208.911805	49.199463
3503.368314	516242.901435	49.204468
3503.206871	516222.848830	49.209473
3503.405979	516199.502410	49.214477
3503.471253	516244.605176	49.219482
3503.483984	516263.366618	49.224487
3503.139313	516232.722250	49.229492
3503.429549	516201.218853	49.234497
3503.259919	516240.239170	49.239501
3503.072622	516206.383656	49.244506
3503.729644	516208.808722	49.249511
3503.446768	516217.603069	49.254516
3503.832479	516187.753534	49.259521
3503.564181	516211.667538	49.264525
3503.853411	516174.752718	49.269530
3503.452945	516204.048590	49.274535
3503.766461	516171.327655	49.279540
3503.535709	516207.727798	49.284545
3503.354335	516186.970249	49.289549
3503.752058	516142.704814	49.294554
3503.491206	516186.240872	49.299559
3503.574626	516160.333350	49.304564
3503.619195	516158.606902	49.309569
3503.369051	516180.242197	49.314573
3503.570101	516150.168904	49.319578
3503.417183	516192.878682	49.324583
3503.379044	516170.783522	49.329588
3503.526208	516153.615419	49.334593
3503.326218	516122.593956	49.339597
3503.783393	516135.823160	49.344602
3503.455071	516127.075102	49.349607
3503.458101	516100.623864	49.354612
3503.720650	516129.359900	49.359617
3503.714981	516107.259523	49.364621
3503.510382	516126.106044	49.369626
3503.649837	516108.635662	49.374631
3503.424003	516078.933162	49.379636
3503.730750	516103.767945	49.384641
3503.261417	516069.653278	49.389645
3503.598177	516100.097201	49.394650
3503.853234	516065.766887	49.399655
3503.426739	516108.014365	49.404660
3503.574620	516068.946910	49.409665
3503.608788	516083.608551	49.414669
3503.567004	516050.640082	49.419674
3503.558920	516059.947412	49.424679
3503.618685	516040.871138	49.429684
3503.756005	516025.373454	49.434689
3503.538925	516060.608515	49.439693
3503.560222	516033.597954	49.444698
3503.983979	516015.475634	49.449703
3503.292638	516032.679616	49.454708
3503.514125	516020.203161	49.459713
3503.695591	515992.054554	49.464717
3503.578234	516006.740210	49.469722
3503.344097	515994.032292	49.474727
3503.374766	515999.489776	49.479732
3503.638933	515995.503273	49.484737
3503.149781	516016.013313	49.489741
3503.847016	515997.240843	49.494746
3503.846502	516000.123893	49.499751
3503.519404	515975.646511	49.504756
3503.792780	515970.950486	49.509761
3503.669205	515969.200018	49.514765
3503.606816	515961.775388	49.519770
3503.746062	515960.387987	49.524775
3503.377961	515961.457835	49.529780
3503.608288	515950.092599	49.534785
3503.499545	515930.284193	49.539789
3503.339904	515918.221930	49.544794
3503.508931	515921.533382	49.549799
3503.341798	515929.652099	49.554804
3503.714362	515915.937867	49.559809
3503.707233	515921.907109	49.564813
3503.299761	515948.574586	49.569818
3503.770592	515908.949958	49.574823
3503.492310	515929.072745	49.579828
3503.740865	515899.547829	49.584833
3503.554453	515885.163277	49.589837
3503.812501	515886.033015	49.594842
3503.799818	515897.263052	49.599847
3503.592792	515893.300421	49.604852
3503.410628	515887.614274	49.609857
3503.672137	515889.545562	49.614861
3503.371200	515874.622765	49.619866
3503.474830	515852.150745	49.624871
3503.312876	515849.900569	49.629876
3503.619877	515840.293305	49.634881
3503.481131	515850.177740	49.639885
3503.358548	515853.231837	49.644890
3503.648875	515848.077914	49.649895
3503.589101	515850.565746	49.654900
3503.571718	515854.412435	49.659905
3503.529628	515845.871870	49.664909
3503.852245	515828.372248	49.669914
3503.597761	515794.779402	49.674919
3503.424098	515814.683486	49.679924
3503.839248	515795.095577	49.684929
3503.289539	515803.932313	49.689933
3503.344571	515808.425059	49.694938
3503.514428	515782.098680	49.699943
3503.193836	515822.812847	49.704948
3503.627426	515798.619590	49.709953
3503.539168	515796.964674	49.714957
3503.679752	515801.747358	49.719962
3503.484623	515772.191190	49.724967
3503.206974	515772.437531	49.729972
3503.453264	515753.280873	49.734977
3503.134618	515775.281552	49.739981
3503.155545	515760.813547	49.744986
3503.544639	515759.892406	49.749991
3503.725001	515765.579189	49.754996
3503.701612	515755.821789	49.760001
3503.368212	515768.012978	49.765005
3503.327725	515757.044447	49.770010
3503.737795	515758.395930	49.775015
3503.590967	515741.425600	49.780020
3503.731926	515720.414222	49.785025
3503.249543	515715.534113	49.790029
3503.370963	515719.712931	49.795034
3503.616708	515718.409831	49.800039
3503.221254	515717.410378	49.805044
3503.618188	515717.853562	49.810049
3503.957956	515710.314684	49.815053
3503.827663	515723.788795	49.820058
3504.080484	515692.846698	49.825063
3503.599655	515694.440146	49.830068
3503.609010	515669.757410	49.835073
3503.661467	515680.673836	49.840077
3503.596820	515689.282238	49.845082
3503.579734	515664.300214	49.850087
3503.290335	515650.184621	49.855092
3503.471853	515641.507458	49.860097
3503.167911	515641.859110	49.865101
3503.203431	515633.660209	49.870106
3503.359734	515638.592185	49.875111
3503.306026	515647.654071	49.880116
3503.778561	515635.087075	49.885121
3503.612568	515628.235017	49.890125
3503.332137	515639.001776	49.895130
3503.587781	515632.791156	49.900135
3503.379792	515647.946642	49.905140
3503.487059	515641.405438	49.910145
3503.454761	515642.624539	49.915149
3503.463271	515625.528387	49.920154
3503.447126	515615.516877	49.925159
3503.026554	515619.781381	49.930164
3503.509457	515609.792147	49.935169
3503.161459	515608.785187	49.940173
3502.944059	515606.037972	49.945178
3503.233771	515640.283434	49.950183
3503.451370	515642.525152	49.955188
3503.408219	515621.087556	49.960193
3503.246828	515620.506296	49.965197
3503.178250	515620.567865	49.970202
3503.853627	515597.701679	49.975207
3503.297289	515607.753411	49.980212
3503.676389	515598.640383	49.985217
3503.602717	515617.770243	49.990221
3503.450018	515607.173388	49.995226
3503.499549	515594.774371	50.000231
3503.314160	515606.588245	50.005236
3503.658507	515599.048594	50.010241
3503.530153	515597.602303	50.015245
3503.711667	515580.731647	50.020250
3503.561210	515573.674803	50.025255
3503.395491	515562.624785	50.030260
3503.416842	515553.821160	50.035265
3503.696896	515557.924369	50.040269
3503.541236	515565.687409	50.045274
3503.384050	515559.997203	50.050279
3503.523462	515569.079185	50.055284
3503.347275	515554.338694	50.060289
3503.452982	515585.477573	50.065293
3503.391044	515556.557474	50.070298
3503.833385	515536.762658	50.075303
3503.455942	515549.466737	50.080308
3503.691012	515539.112014	50.085313
3503.515941	515534.031551	50.090317
3503.461590	515539.654353	50.095322
3503.550058	515533.217232	50.100327
3503.339871	515538.460048	50.105332
3503.662617	515532.744556	50.110337
3503.551589	515515.768339	50.115341
3503.543130	515499.787439	50.120346
3503.747129	515489.842214	50.125351
3503.243489	515491.945058	50.130356
3503.598133	515489.613184	50.135361
3503.699939	515493.238809	50.140365
3503.533641	515489.370798	50.145370
3503.536028	515490.382120	50.150375
3503.360827	515493.697484	50.155380
3503.719655	515478.720636	50.160385
3503.592565	515468.423109	50.165389
3503.304329	515456.330260	50.170394
3503.690563	515452.172605	50.175399
3503.654849	515455.415354	50.180404
3503.741276	515454.592610	50.185409
3503.721961	515458.844313	50.190413
3503.258557	515446.020482	50.195418
3503.650829	515425.778254	50.200423
3503.636004	515413.136387	50.205428
3503.608635	515403.733454	50.210433
3503.489173	515422.870773	50.215437
3503.437827	515413.218747	50.220442
3503.819116	515398.895785	50.225447
3503.413112	515404.422479	50.230452
3503.602899	515409.703273	50.235457
3503.631139	515393.615316	50.240461
3503.349478	515372.822031	50.245466
3503.057290	515364.826525	50.250471
3502.918362	515374.357226	50.255476
3503.377240	515382.478422	50.260481
3503.134479	515390.407042	50.265485
3502.559182	515409.009491	50.270490
3503.079200	515397.648673	50.275495
3503.001246	515418.853115	50.280500
3503.192493	515406.785603	50.285505
3503.110318	515412.311691	50.290509
3503.280926	515425.839638	50.295514
3503.278075	515401.360746	50.300519
3503.075534	515415.200565	50.305524
3503.287572	515406.316147	50.310529
3503.131552	515390.661930	50.315533
3502.999172	515428.110344	50.320538
3503.486456	515406.436908	50.325543
3502.936266	515426.097497	50.330548
3502.894514	515414.522013	50.335553
3503.125808	515401.689507	50.340557
3503.070459	515426.481368	50.345562
3503.100915	515430.371171	50.350567
3503.047165	515475.444241	50.355572
3503.338156	515450.362629	50.360577
3503.252005	515453.714504	50.365581
3503.161735	515481.597022	50.370586
3503.125736	515454.999202	50.375591
3503.546243	515468.285309	50.380596
3503.321172	515472.114333	50.385601
3503.588612	515471.364136	50.390605
3503.398940	515444.891742	50.395610
3503.416602	515431.587249	50.400615
3503.562608	515430.047004	50.405620
3503.553157	515419.983742	50.410625
3503.402776	515427.948321	50.415629
3503.501145	515424.797127	50.420634
3503.489346	515415.138852	50.425639
3503.455636	515424.804627	50.430644
3503.401695	515423.498293	50.435649
3503.509220	515432.332502	50.440653
3503.371379	515428.864600	50.445658
3503.617714	515412.792769	50.450663
3503.231900	515412.955055	50.455668
3503.149388	515390.612992	50.460673
3503.463400	515390.563516	50.465677
3503.462600	515385.050844	50.470682
3503.370543	515385.369012	50.475687
3503.501274	515387.422184	50.480692
3503.736576	515387.435726	50.485697
3503.285463	515373.648923	50.490701
3503.277380	515392.414630	50.495706
3503.505046	515398.953880	50.500711
3503.802627	515396.681590	50.505716
3503.689289	515397.711207	50.510721
3503.575997	515391.103611	50.515725
3503.744030	515359.971992	50.520730
3503.496257	515357.836468	50.525735
3503.450663	515333.161921	50.530740
3503.444291	515283.748584	50.535745
3503.393156	515267.470740	50.540749
3503.462329	515177.380459	50.545754
3503.507008	515118.095818	50.550759
3502.921617	515057.393193	50.555764
3502.949173	514951.527767	50.560769
3503.034372	514847.878048	50.565773
3502.805020	514773.057108	50.570778
3503.095927	514647.826809	50.575783
3502.454847	514515.105275	50.580788
3502.488090	514375.397160	50.585793
3501.877507	514260.169673	50.590797
3501.843134	514099.934089	50.595802
3501.776453	513944.507371	50.600807
3501.315999	513789.748448	50.605812
3501.448829	513614.560036	50.610817
3501.201768	513424.052495	50.615821
3500.516558	513257.942951	50.620826
3500.779632	513053.794118	50.625831
3500.229043	512861.557766	50.630836
3500.194909	512638.532068	50.635841
3499.820721	512427.495587	50.640845
3499.365573	512212.371731	50.645850
3499.569364	511970.025986	50.650855
3498.888569	511731.661332	50.655860
3498.792195	511488.799717	50.660865
3498.258657	511236.695197	50.665869
3497.717377	510986.864761	50.670874
3497.615774	510731.750269	50.675879
3497.305929	510451.621741	50.680884
3496.858931	510168.677102	50.685889
3496.651539	509890.344571	50.690893
3495.953809	509614.614772	50.695898
3495.790376	509339.049086	50.700903
3495.114112	509032.696253	50.705908
3494.835616	508726.528099	50.710913
3494.500878	508422.336742	50.715917
3494.006383	508123.731190	50.720922
3493.449468	507803.675961	50.725927
3492.816047	507480.995671	50.730932
3492.729291	507168.090353	50.735937
3492.469288	506838.963293	50.740941
3491.865769	506510.086728	50.745946
3491.718940	506173.439861	50.750951
3490.636058	505838.148999	50.755956
3490.191731	505459.785645	50.760961
3489.863451	505106.750332	50.765965
3489.041149	504766.994914	50.770970
3488.650013	504408.945248	50.775975
3488.048078	504059.424250	50.780980
3487.439051	503684.085386	50.785985
3487.172043	503330.296230	50.790989
3486.625805	502973.962830	50.795994
3486.170787	502596.703856	50.800999
3485.556864	502230.698759	50.806004
3485.133207	501855.747445	50.811009
3484.459110	501479.410519	50.816013
3484.057159	501106.262278	50.821018
3483.500346	500709.237925	50.826023
3482.794454	500330.654556	50.831028
3482.190466	499940.808890	50.836033
3481.644420	499551.451851	50.841037
3481.118453	499158.792613	50.846042
3481.208360	498754.181034	50.851047
3479.806838	498357.744580	50.856052
3479.269233	497957.517669	50.861057
3478.637549	497557.347430	50.866061
3478.104144	497156.444023	50.871066
3477.747016	496745.073846	50.876071
3477.002744	496352.844080	50.881076
3476.508563	495929.730446	50.886081
3475.944333	495523.226354	50.891085
3475.280718	495116.627695	50.896090
3474.923923	494691.539633	50.901095
3474.131303	494278.663847	50.906100
3473.507598	493856.383831	50.911105
3472.675130	493439.596356	50.916109
3471.937965	493026.582571	50.921114
3471.331369	492600.473105	50.926119
3470.701538	492171.116336	50.931124
3469.874937	491746.744011	50.936129
3469.552195	491335.045273	50.941133
3468.318161	490913.959812	50.946138
3467.948135	490489.436165	50.951143
3467.210172	490071.393603	50.956148
3466.381563	489662.726491	50.961153
3465.896263	489245.182826	50.966157
3465.250809	488823.805625	50.971162
3464.563353	488386.013730	50.976167
3463.747129	487976.903023	50.981172
3463.442271	487552.657727	50.986177
3463.107850	487125.925443	50.991181
3461.984128	486703.006478	50.996186
3461.514332	486279.670840	51.001191
3460.706273	485860.128238	51.006196
3459.929176	485427.095478	51.011201
3459.192911	485008.485534	51.016205
3458.450731	484574.262846	51.021210
3457.792279	484151.872882	51.026215
3457.051283	483725.332107	51.031220
3456.476230	483300.782436	51.036225
3455.971695	482885.383396	51.041229
3455.146630	482455.129255	51.046234
3454.853204	482023.717512	51.051239
3453.762928	481607.015776	51.056244
3452.897792	481182.668637	51.061249
3452.428316	480760.834180	51.066253
3451.659113	480338.024570	51.071258
3451.092594	479906.913621	51.076263
3450.331801	479485.250002	51.081268
3449.204815	479049.242596	51.086273
3448.584443	478633.569442	51.091277
3447.787614	478215.482836	51.096282
3447.872239	477792.484049	51.101287
3446.954832	477372.422278	51.106292
3446.312799	476952.409541	51.111297
3445.277229	476532.399548	51.116301
3444.716321	476111.139980	51.121306
3444.178916	475686.421181	51.126311
3443.415891	475267.608951	51.131316
3442.823253	474863.562362	51.136321
3442.094583	474430.534458	51.141325
3441.371936	474015.491787	51.146330
3440.791626	473593.422635	51.151335
3439.748195	473169.035391	51.156340
3439.169474	472737.012425	51.161345
3438.286838	472327.435801	51.166349
3437.806205	471913.833150	51.171354
3437.120375	471498.530929	51.176359
3436.126136	471084.130989	51.181364
3435.291628	470674.159058	51.186369
3435.073481	470253.637289	51.191373
3434.283713	469837.659119	51.196378
3433.545299	469424.554572	51.201383
3432.754405	469014.086735	51.206388
3432.010422	468610.702063	51.211393
3431.417523	468193.950209	51.216397
3430.480308	467790.935277	51.221402
3430.066250	467376.116511	51.226407
3429.221256	466965.110148	51.231412
3428.557516	466553.002251	51.236417
3427.684571	466152.227840	51.241421
3426.736094	465748.060152	51.246426
3425.772552	465340.895149	51.251431
3425.621578	464935.876019	51.256436
3424.718838	464538.068063	51.261441
3424.219174	464147.136980	51.266445
3423.578131	463741.665619	51.271450
3422.895919	463327.368362	51.276455
3421.783150	462942.192642	51.281460
3421.044705	462541.278743	51.286465
3421.012316	462144.404835	51.291469
3420.075585	461742.087362	51.296474
3419.482473	461336.512661	51.301479
3418.532611	460954.116346	51.306484
3417.844013	460537.585818	51.311489
3417.189782	460142.092616	51.316493
3416.453801	459751.373404	51.321498
3415.837795	459354.693311	51.326503
3414.859308	458960.904116	51.331508
3414.339381	458573.680791	51.336513
3413.707362	458186.164047	51.341517
3412.186175	457785.439151	51.346522
3411.976999	457396.218428	51.351527
3411.418045	457013.336939	51.356532
3410.609759	456627.647288	51.361537
3410.087291	456244.949812	51.366541
3409.215773	455863.721555	51.371546
3409.031827	455460.866433	51.376551
3408.068631	455083.089445	51.381556
3407.164665	454688.046236	51.386561
3406.753716	454302.761318	51.391565
3405.685396	453906.614243	51.396570
3405.246332	453529.286621	51.401575
3404.455928	453151.247195	51.406580
3403.745235	452754.516153	51.411585
3403.048767	452379.087655	51.416589
3402.144797	451992.319414	51.421594
3401.714495	451606.789119	51.426599
3400.676342	451240.631414	51.431604
3400.086094	450851.104961	51.436609
3399.862773	450469.531849	51.441613
3398.706127	450100.228571	51.446618
3398.087899	449724.135583	51.451623
3397.688552	449342.774805	51.456628
3396.871630	448950.207425	51.461633
3396.156550	448588.575080	51.466637
3395.094404	448219.176359	51.471642
3394.782868	447827.017790	51.476647
3394.322723	447454.009996	51.481652
3393.317854	447079.762841	51.486657
3392.863896	446696.134613	51.491661
3391.944180	446322.674107	51.496666
3391.269947	445948.356825	51.501671
3390.285968	445577.787882	51.506676
3389.698576	445208.622453	51.511681
3388.960561	444824.501428	51.516685
3388.419518	444464.504473	51.521690
3387.808775	444092.939888	51.526695
3386.783771	443718.440189	51.531700
3386.534439	443349.903421	51.536705
3386.248588	442984.412553	51.541709
3385.217934	442611.571774	51.546714
3384.437803	442231.477205	51.551719
3383.743855	441869.486040	51.556724
3383.108595	441500.474615	51.561729
3382.040758	441132.998239	51.566733
3381.188449	440770.965101	51.571738
3380.810119	440395.702879	51.576743
3380.534864	440031.206930	51.581748
3379.277481	439670.643187	51.586753
3378.640140	439306.726884	51.591757
3377.781739	438945.784891	51.596762
3377.246715	438579.303224	51.601767
3376.333721	438227.396743	51.606772
3375.609876	437857.888011	51.611777
3374.950320	437495.548119	51.616781
3374.223579	437150.603800	51.621786
3373.434721	436787.030163	51.626791
3372.910078	436440.140095	51.631796
3372.403592	436085.270502	51.636801
3371.876000	435725.220008	51.641805
3371.084010	435360.128428	51.646810
3370.408044	435011.998686	51.651815
3369.577607	434669.905950	51.656820
3369.006995	434305.779849	51.661825
3368.529217	433942.725676	51.666829
3367.410787	433590.431751	51.671834
3367.122583	433239.347451	51.676839
3366.476411	432873.207106	51.681844
3365.739932	432526.119650	51.686849
3364.785404	432173.704295	51.691853
3364.388364	431806.773112	51.696858
3363.643687	431451.978686	51.701863
3362.873395	431106.401183	51.706868
3362.206272	430750.010582	51.711873
3361.936168	430391.063767	51.716877
3360.598897	430030.985685	51.721882
3360.014509	429679.011444	51.726887
3359.429616	429342.294873	51.731892
3358.780493	428983.236446	51.736897
3358.100042	428622.527402	51.741901
3357.479838	428291.466262	51.746906
3357.154792	427931.402733	51.751911
3356.323705	427567.808060	51.756916
3355.389555	427224.973959	51.761921
3355.065303	426859.943506	51.766925
3354.139543	426515.752973	51.771930
3353.775911	426163.164069	51.776935
3353.044216	425804.584000	51.781940
3352.181010	425447.518488	51.786945
3351.692904	425097.754628	51.791949
3350.567925	424738.054309	51.796954
3349.729095	424383.764888	51.801959
3349.051621	424040.697480	51.806964
3348.194609	423700.752982	51.811969
3348.113329	423342.977501	51.816973
3347.090887	422997.386165	51.821978
3346.581645	422642.539554	51.826983
3345.658055	422306.525559	51.831988
3344.943002	421960.618650	51.836993
3344.175576	421612.835966	51.841997
3343.466133	421286.784183	51.847002
3342.786881	420935.778420	51.852007
3342.603509	420591.650259	51.857012
3341.768508	420268.197570	51.862017
3341.126020	419911.889309	51.867021
3340.256517	419571.464475	51.872026
3339.560068	419222.624789	51.877031
3339.157013	418876.986193	51.882036
3338.177410	418544.721278	51.887041
3337.905200	418201.721289	51.892045
3336.558356	417862.316843	51.897050
3336.260279	417515.069998	51.902055
3335.843168	417176.272574	51.907060
3334.722798	416843.247975	51.912065
3334.482640	416493.896321	51.917069
3333.776590	416153.379507	51.922074
3332.819013	415811.755138	51.927079
3332.256074	415474.180362	51.932084
3331.501518	415139.807947	51.937089
3330.961841	414789.670103	51.942093
3330.281174	414459.851681	51.947098
3329.654178	414118.612559	51.952103
3329.081603	413771.745484	51.957108
3328.079913	413437.214869	51.962113
3327.568709	413091.194002	51.967117
3326.870106	412741.997083	51.972122
3326.326380	412404.968448	51.977127
3325.637560	412076.852599	51.982132
3325.089563	411736.234204	51.987137
3324.279799	411388.639881	51.992141
3322.971138	411053.368680	51.997146
3322.871236	410711.320984	52.002151
3322.339043	410382.043712	52.007156
3321.175045	410040.436217	52.012161
3320.851113	409702.249766	52.017165
3320.133969	409359.191661	52.022170
3319.701869	409019.947394	52.027175
3318.737182	408683.019951	52.032180
3317.959359	408347.558649	52.037185
3317.747110	407998.839860	52.042189
3316.746818	407671.818350	52.047194
3316.392614	407326.646966	52.052199
3315.617157	406978.818974	52.057204
3314.782073	406652.090944	52.062209
3314.281681	406297.375191	52.067213
3313.355059	405984.073880	52.072218
3312.543967	405627.950968	52.077223
3311.793864	405305.973577	52.082228
3311.334577	404958.886385	52.087233
3310.983448	404624.206994	52.092237
3309.819664	404290.669248	52.097242
3309.844189	403952.797068	52.102247
3308.899146	403614.591693	52.107252
3308.186081	403285.648914	52.112257
3307.486832	402935.781580	52.117261
3306.774874	402607.695859	52.122266
3306.318033	402265.764197	52.127271
3305.328285	401926.099191	52.132276
3304.911254	401588.704007	52.137281
3304.408585	401250.124140	52.142285
3303.312829	400917.506452	52.147290
3302.505403	400569.816648	52.152295
3301.786986	400247.173269	52.157300
3301.188246	399916.322432	52.162305
3301.009152	399572.234022	52.167309
3299.761495	399245.724293	52.172314
3299.156088	398918.703021	52.177319
3298.521125	398572.261265	52.182324
3298.096209	398245.611542	52.187329
3297.270602	397916.098463	52.192333
3296.317897	397580.882247	52.197338
3295.923449	397240.820395	52.202343
3295.494884	396916.573370	52.207348
3294.449634	396570.531642	52.212353
3293.778680	396241.536943	52.217357
3293.039723	395910.465079	52.222362
3292.652403	395580.402161	52.227367
3291.666276	395249.947687	52.232372
3290.843517	394923.760849	52.237377
3290.364066	394595.457228	52.242381
3289.562441	394269.998123	52.247386
3289.201490	393932.109760	52.252391
3288.601947	393604.502138	52.257396
3287.672082	393283.910195	52.262401
3287.682009	392938.630968	52.267405
3286.630079	392620.467632	52.272410
3285.573211	392276.443865	52.277415
3284.777653	391959.479834	52.282420
3284.211644	391625.796823	52.287425
3283.709719	391300.135373	52.292429
3282.601302	390980.135351	52.297434
3282.203106	390651.527406	52.302439
3281.445598	390326.049969	52.307444
3280.916757	390003.432147	52.312449
3280.414761	389675.391008	52.317453
3279.510557	389350.029575	52.322458
3279.138657	389029.437827	52.327463
3278.143644	388703.220331	52.332468
3277.384432	388373.453406	52.337473
3277.041487	388054.323288	52.342477
3276.117716	387729.077472	52.347482
3275.389759	387397.923555	52.352487
3275.229116	387083.918291	52.357492
3274.179811	386753.801123	52.362497
3273.328447	386430.286966	52.367501
3272.934553	386100.899471	52.372506
3272.312396	385775.003712	52.377511
3271.561857	385452.940025	52.382516
3271.032081	385127.430860	52.387521
3270.355382	384803.010205	52.392525
3269.376140	384486.391208	52.397530
3268.978319	384150.400295	52.402535
3268.044067	383837.380019	52.407540
3267.350697	383515.595801	52.412545
3267.075169	383189.419246	52.417549
3266.057435	382868.240344	52.422554
3265.509761	382533.403238	52.427559
3264.763662	382204.698518	52.432564
3263.817905	381897.844319	52.437569
3263.640554	381568.306624	52.442573
3263.026980	381252.162372	52.447578
3262.188136	380927.454497	52.452583
3261.689349	380594.729232	52.457588
3260.876077	380274.717169	52.462593
3259.948989	379954.110052	52.467597
3259.224129	379628.533976	52.472602
3258.788094	379304.588225	52.477607
3258.015546	379003.457522	52.482612
3257.130881	378679.653901	52.487617
3257.150071	378339.934603	52.492621
3256.162256	378043.434492	52.497626
3255.473005	377711.147387	52.502631
3255.168843	377393.193505	52.507636
3254.248487	377070.654268	52.512641
3253.546625	376736.733156	52.517645
3252.875374	376419.363812	52.522650
3252.505951	376087.674072	52.527655
3251.839756	375766.432393	52.532660
3250.902130	375446.197737	52.537665
3250.456760	375120.108372	52.542669
3249.552391	374785.999786	52.547674
3248.805688	374466.592174	52.552679
3248.434254	374144.273652	52.557684
3247.594340	373818.872360	52.562689
3247.126599	373493.358777	52.567693
3246.054737	373163.282905	52.572698
3245.746560	372842.038172	52.577703
3245.029499	372523.068870	52.582708
3244.309894	372198.526325	52.587713
3243.692070	371870.785239	52.592717
3242.829895	371553.383391	52.597722
3242.444516	371219.520404	52.602727
3241.876094	370901.889164	52.607732
3241.036171	370565.269110	52.612737
3240.380871	370255.965839	52.617741
3239.619076	369933.117274	52.622746
3238.943931	369599.160342	52.627751
3238.742634	369263.879276	52.632756
3237.641255	368942.807067	52.637761
3236.821422	368609.781334	52.642765
3236.228702	368286.868398	52.647770
3235.269277	367964.036543	52.652775
3234.954379	367642.983097	52.657780
3233.990659	367332.970133	52.662785
3233.669902	367003.186298	52.667789
3232.796900	366685.343652	52.672794
3232.353915	366364.606582	52.677799
3231.853219	366031.282072	52.682804
3230.718390	365715.712981	52.687809
3230.394130	365391.260962	52.692813
3229.852090	365069.639869	52.697818
3229.034140	364745.821107	52.702823
3228.158796	364424.044649	52.707828
3227.616251	364101.322755	52.712833
3227.038568	363775.856185	52.717837
3226.187175	363461.855175	52.722842
3225.461542	363125.288232	52.727847
3224.870256	362809.129778	52.732852
3224.151337	362494.490632	52.737857
3223.670929	362165.104371	52.742861
3223.034435	361846.376639	52.747866
3222.418712	361518.203208	52.752871
3221.636399	361206.542645	52.757876
3220.747967	360873.878591	52.762881
3220.216218	360553.115423	52.767885
3219.659406	360237.621438	52.772890
3219.067373	359910.705562	52.777895
3218.702788	359585.787224	52.782900
3217.543045	359259.134894	52.787905
3216.978508	358924.548598	52.792909
3216.272420	358603.774695	52.797914
3215.531106	358281.655574	52.802919
3214.995568	357962.911748	52.807924
3213.857221	357637.873909	52.812929
3213.586737	357324.529830	52.817933
3212.848696	357008.178565	52.822938
3211.993558	356689.986127	52.827943
3211.921315	356365.636625	52.832948
3210.888175	356049.198784	52.837953
3210.675533	355723.086003	52.842957
3209.919222	355406.778519	52.847962
3209.152811	355076.219359	52.852967
3208.626642	354749.004782	52.857972
3207.742171	354418.078343	52.862977
3207.277555	354091.333407	52.867981
3206.528486	353768.499734	52.872986
3205.639100	353440.647247	52.877991
3205.332331	353116.288963	52.882996
3204.366528	352796.054025	52.888001
3203.566561	352463.574889	52.893005
3203.144738	352143.733515	52.898010
3202.596928	351819.176389	52.903015
3202.095105	351490.359787	52.908020
3200.961911	351170.956008	52.913025
3200.711647	350829.573856	52.918029
3199.966366	350502.342269	52.923034
3199.067855	350187.782177	52.928039
3198.703599	349860.002902	52.933044
3197.603491	349528.265856	52.938049
3197.171558	349203.038532	52.943053
3196.494709	348880.342320	52.948058
3196.158859	348553.568901	52.953063
3195.190853	348229.896924	52.958068
3194.184195	347906.941861	52.963073
3193.527851	347579.628095	52.968077
3192.781541	347265.994651	52.973082
3192.204153	346931.639790	52.978087
3191.953566	346619.731518	52.983092
3190.767504	346296.337578	52.988097
3190.078054	345972.685096	52.993101
3189.587967	345655.133488	52.998106
3189.160300	345329.170687	53.003111
3188.171852	345016.454226	53.008116
3187.552514	344699.172428	53.013121
3187.534707	344368.532377	53.018125
3186.381240	344046.775376	53.023130
3185.368391	343728.939766	53.028135
3185.038623	343393.660142	53.033140
3184.404329	343079.579340	53.038145
3183.833173	342754.108801	53.043149
3183.021062	342440.307372	53.048154
3182.433516	342108.243260	53.053159
3181.878690	341783.834079	53.058164
3180.902739	341466.133561	53.063169
3180.417991	341148.124613	53.068173
3179.670084	340821.984558	53.073178
3178.860537	340504.354643	53.078183
3178.146311	340178.765943	53.083188
3177.117605	339861.192925	53.088193
3176.843277	339545.102687	53.093197
3176.384668	339225.883519	53.098202
3175.736837	338892.793741	53.103207
3175.029883	338583.894900	53.108212
3174.627245	338272.324456	53.113217
3173.888567	337928.501585	53.118221
3173.282521	337611.359781	53.123226
3172.393473	337291.028238	53.128231
3171.695084	336961.016888	53.133236
3170.900867	336638.503381	53.138241
3170.349504	336316.509954	53.143245
3169.665243	336001.587631	53.148250
3169.164646	335670.596745	53.153255
3168.537338	335358.055408	53.158260
3167.877830	335038.975177	53.163265
3167.308381	334708.576061	53.168269
3166.727516	334388.563912	53.173274
3165.844224	334057.091213	53.178279
3165.399314	333722.874507	53.183284
3164.564128	333416.619977	53.188289
3163.679692	333083.768146	53.193293
3163.059558	332770.475813	53.198298
3162.587286	332433.100546	53.203303
3162.097005	332104.153313	53.208308
3160.715579	331789.984283	53.213313
3160.186776	331467.863175	53.218317
3159.819015	331141.921806	53.223322
3158.888678	330830.274097	53.228327
3158.430649	330509.079586	53.233332
3157.649614	330188.774948	53.238337
3157.015949	329861.469786	53.243341
3156.352912	329558.557940	53.248346
3155.578339	329227.860777	53.253351
3155.189789	328900.130800	53.258356
3154.378733	328593.292310	53.263361
3153.851834	328267.720148	53.268365
3153.335912	327946.269394	53.273370
3152.672771	327623.440312	53.278375
3151.843142	327305.168149	53.283380
3150.911477	326971.762020	53.288385
3150.462570	326654.419964	53.293389
3149.535914	326339.851048	53.298394
3149.022950	326015.845980	53.303399
3148.644728	325688.864869	53.308404
3147.657018	325379.444943	53.313409
3146.944576	325050.910146	53.318413
3146.237495	324723.060644	53.323418
3145.763128	324411.646315	53.328423
3144.873580	324101.900571	53.333428
3144.049283	323788.858873	53.338433
3143.808291	323463.960611	53.343437
3142.827326	323146.281926	53.348442
3142.137821	322833.342716	53.353447
3141.979631	322508.096752	53.358452
3140.952173	322195.514261	53.363457
3140.359123	321879.781052	53.368461
3139.665842	321552.477432	53.373466
3138.824117	321233.853162	53.378471
3138.270083	320920.631120	53.383476
3137.377931	320604.253264	53.388481
3136.850239	320281.934871	53.393485
3136.123723	319973.600148	53.398490
3135.369500	319650.678832	53.403495
3134.753685	319335.551476	53.408500
3134.132736	319033.868107	53.413505
3133.732359	318714.172248	53.418509
3133.095573	318400.038133	53.423514
3132.546427	318073.183178	53.428519
3132.004825	317753.761090	53.433524
3130.957504	317445.036035	53.438529
3130.719418	317123.985158	53.443533
3129.810432	316794.254608	53.448538
3129.090976	316482.851966	53.453543
3128.811005	316158.647165	53.458548
3127.883945	315837.472002	53.463553
3127.172740	315507.935119	53.468557
3126.518052	315195.856233	53.473562
3125.747405	314873.431059	53.478567
3125.096929	314549.330736	53.483572
3124.039166	314240.826767	53.488577
3123.660000	313908.558605	53.493581
3122.874330	313605.790042	53.498586
3122.233508	313292.863038	53.503591
3122.022436	312967.389736	53.508596
3121.016267	312661.215787	53.513601
3120.560619	312332.978256	53.518605
3119.635867	312020.372675	53.523610
3118.902446	311705.113123	53.528615
3118.548615	311392.950224	53.533620
3117.538396	311064.058297	53.538625
3117.213801	310745.319174	53.543629
3116.468544	310425.397977	53.548634
3115.662714	310104.874342	53.553639
3115.143277	309789.117373	53.558644
3114.569892	309474.030195	53.563649
3113.878330	309153.231292	53.568653
3113.392028	308827.509792	53.573658
3112.555781	308516.663468	53.578663
3112.015855	308183.589365	53.583668
3111.274512	307857.803831	53.588673
3110.599584	307539.493736	53.593677
3109.695125	307225.828396	53.598682
3109.008373	306916.024050	53.603687
3108.606346	306586.463676	53.608692
3107.614764	306280.398560	53.613697
3107.257802	305946.041959	53.618701
3106.510572	305638.663442	53.623706
3105.901162	305317.918415	53.628711
3105.265814	304994.375518	53.633716
3104.434631	304684.767181	53.638721
3103.952649	304362.013466	53.643725
3103.029496	304042.206479	53.648730
3102.080781	303722.810285	53.653735
3102.004124	303409.336310	53.658740
3101.207022	303085.840179	53.663745
3100.513316	302763.422031	53.668749
3099.804860	302449.536698	53.673754
3099.229198	302136.801156	53.678759
3098.641241	301815.051865	53.683764
3097.521568	301505.278831	53.688769
3097.063298	301181.852417	53.693773
3096.550672	300859.096081	53.698778
3095.811686	300543.760205	53.703783
3095.302584	300221.333120	53.708788
3094.738453	299912.538739	53.713793
3093.859335	299592.129927	53.718797
3093.584550	299268.467018	53.723802
3092.451491	298944.506389	53.728807
3091.977101	298626.069088	53.733812
3090.960688	298313.905427	53.738817
3090.682650	297993.933396	53.743821
3090.170794	297675.729557	53.748826
3089.392585	297350.156445	53.753831
3088.712460	297024.898324	53.758836
3088.262089	296707.803676	53.763841
3087.596019	296379.486203	53.768845
3086.740451	296058.685504	53.773850
3085.982035	295732.699090	53.778855
3085.481409	295412.605216	53.783860
3084.819953	295099.947264	53.788865
3083.976949	294773.972733	53.793869
3083.506111	294442.692548	53.798874
3082.457977	294126.579885	53.803879
3081.916882	293804.376233	53.808884
3081.354680	293490.910786	53.813889
3080.899916	293167.342802	53.818893
3080.149343	292840.230269	53.823898
3079.539276	292519.512868	53.828903
3079.220349	292196.227685	53.833908
3078.114985	291880.197459	53.838913
3077.763554	291541.457755	53.843917
3077.007456	291219.615762	53.848922
3076.340005	290900.433456	53.853927
3075.317048	290577.079392	53.858932
3074.633649	290243.127570	53.863937
3073.864308	289930.709217	53.868941
3073.223220	289608.057644	53.873946
3072.400183	289284.033782	53.878951
3072.069669	288969.558477	53.883956
3071.374715	288660.692522	53.888961
3070.877738	288328.924763	53.893965
3070.148969	287999.689204	53.898970
3069.120976	287692.861534	53.903975
3068.877095	287361.485714	53.908980
3067.876558	287050.145301	53.913985
3067.470271	286721.723409	53.918989
3066.982802	286409.511748	53.923994
3066.002655	286081.129181	53.928999
3065.370953	285760.051474	53.934004
3064.686459	285439.185614	53.939009
3064.147163	285120.716003	53.944013
3063.707053	284797.085899	53.949018
3062.779149	284473.150738	53.954023
3062.018341	284152.983668	53.959028
3061.251051	283836.994196	53.964033
3060.967398	283503.736949	53.969037
3059.967389	283192.979427	53.974042
3059.219353	282877.368357	53.979047
3058.949129	282545.763839	53.984052
3058.124669	282236.658923	53.989057
3057.358310	281911.143092	53.994061
3056.928376	281587.229298	53.999066
3056.228783	281269.241208	54.004071
3055.712395	280941.902586	54.009076
3054.917840	280630.245399	54.014081
3054.381010	280297.459533	54.019085
3053.647366	279983.984224	54.024090
3052.730204	279657.116039	54.029095
3052.410703	279329.236305	54.034100
3051.563410	279015.243858	54.039105
3050.338006	278685.597192	54.044109
3050.041134	278367.417073	54.049114
3049.495712	278047.697186	54.054119
3048.812794	277707.675236	54.059124
3047.719311	277393.645023	54.064129
3047.545896	277066.811369	54.069133
3046.814141	276748.674361	54.074138
3045.805488	276433.026118	54.079143
3045.489477	276104.304826	54.084148
3044.835630	275793.770488	54.089153
3044.235759	275474.950380	54.094157
3043.416438	275149.466823	54.099162
3043.002444	274832.298233	54.104167
3042.310623	274505.215496	54.109172
3041.622806	274189.032628	54.114177
3041.185327	273866.010120	54.119181
3040.273842	273535.753256	54.124186
3039.584758	273222.143036	54.129191
3039.129493	272890.285989	54.134196
3038.550163	272563.644201	54.139201
3038.000192	272240.257798	54.144205
3037.149476	271917.835945	54.149210
3036.332535	271581.936094	54.154215
3035.815609	271256.863850	54.159220
3034.700114	270938.100730	54.164225
3034.466579	270606.336644	54.169229
3033.998990	270283.778328	54.174234
3032.848813	269962.958157	54.179239
3032.466994	269638.578304	54.184244
3031.884364	269317.006433	54.189249
3031.308137	268990.136316	54.194253
3030.289311	268664.406093	54.199258
3029.779057	268331.795546	54.204263
3029.382857	268007.877274	54.209268
3028.492932	267680.930226	54.214273
3027.534234	267343.272174	54.219277
3027.093751	267027.434949	54.224282
3025.953109	266713.644334	54.229287
3025.861092	266381.656536	54.234292
3025.109912	266056.802516	54.239297
3024.783677	265734.300956	54.244301
3024.381437	265410.156256	54.249306
3023.645615	265071.471436	54.254311
3022.715035	264739.643169	54.259316
3021.872219	264417.402740	54.264321
3021.367221	264085.074752	54.269325
3020.964293	263760.116626	54.274330
3019.811670	263424.402670	54.279335
3019.307256	263093.094274	54.284340
3018.446048	262769.253840	54.289345
3017.839256	262440.483645	54.294349
3017.093250	262115.428670	54.299354
3016.305947	261790.788068	54.304359
3015.753576	261455.566991	54.309364
3014.883885	261136.466668	54.314369
3014.316065	260818.388572	54.319373
3013.887350	260498.022206	54.324378
3012.947940	260175.954322	54.329383
3012.647538	259840.771744	54.334388
3011.997803	259520.619828	54.339393
3011.000780	259191.686054	54.344397
3010.321232	258869.629628	54.349402
3009.881562	258545.803874	54.354407
3009.070347	258208.514164	54.359412
3008.431639	257898.065742	54.364417
3007.712156	257572.502912	54.369421
3007.177457	257245.128593	54.374426
3006.476867	256926.745503	54.379431
3005.813530	256597.762607	54.384436
3005.203832	256277.303243	54.389441
3004.585062	255946.735338	54.394445
3003.908889	255625.294281	54.399450
3003.283682	255296.332875	54.404455
3002.835439	254962.326991	54.409460
3002.332746	254646.157195	54.414465
3001.345132	254312.543403	54.419469
3000.959422	253979.242392	54.424474
2999.498242	253661.239529	54.429479
2999.263122	253326.438770	54.434484
2998.471416	253001.174903	54.439489
2997.874654	252680.031845	54.444493
2997.360129	252357.348350	54.449498
2996.668110	252021.705561	54.454503
2996.028281	251691.123017	54.459508
2995.183834	251377.381421	54.464513
2994.744196	251044.221802	54.469517
2994.356180	250718.236218	54.474522
2993.469388	250392.712232	54.479527
2992.531859	250062.460197	54.484532
2991.935622	249742.468669	54.489537
2991.491358	249398.770142	54.494541
2990.722182	249076.515393	54.499546
2989.899468	248765.704087	54.504551
2989.594939	248426.263930	54.509556
2988.865879	248103.521049	54.514561
2988.324527	247769.467741	54.519565
2987.649810	247435.971092	54.524570
2986.931723	247114.833010	54.529575
2986.085740	246778.436429	54.534580
2985.417918	246450.212409	54.539585
2984.745574	246115.037753	54.544589
2983.833254	245795.690568	54.549594
2983.145517	245471.928509	54.554599
2982.874450	245132.058020	54.559604
2982.032791	244810.511952	54.564609
2981.281328	244475.353894	54.569613
2981.156198	244150.410988	54.574618
2979.937233	243823.044597	54.579623
2979.443017	243494.876759	54.584628
2978.782280	243165.411947	54.589633
2978.044678	242832.522390	54.594637
2977.557663	242513.548851	54.599642
2976.860098	242184.041542	54.604647
2976.379876	241849.764265	54.609652
2975.463373	241528.722250	54.614657
2974.780920	241193.918590	54.619661
2974.018060	240867.964822	54.624666
2973.406028	240537.582721	54.629671
2973.018916	240210.399943	54.634676
2972.073896	239886.795033	54.639681
2971.757638	239548.933351	54.644685
2971.062097	239218.313636	54.649690
2970.303657	238888.850742	54.654695
2969.615779	238547.893357	54.659700
2968.967452	238227.989500	54.664705
2968.159167	237908.799431	54.669709
2967.201418	237566.894746	54.674714
2966.801011	237246.725376	54.679719
2966.203470	236917.064757	54.684724
2965.687658	236593.503500	54.689729
2964.928962	236265.754749	54.694733
2964.265760	235928.901467	54.699738
2963.504147	235598.685345	54.704743
2963.102933	235269.100750	54.709748
2962.376390	234944.763227	54.714753
2961.572176	234605.059325	54.719757
2961.161038	234276.090685	54.724762
2960.447384	233942.918721	54.729767
2959.734231	233604.604316	54.734772
2958.741767	233278.404662	54.739777
2958.124969	232945.373570	54.744781
2957.522351	232620.362113	54.749786
2957.018195	232301.192562	54.754791
2956.296383	231964.744103	54.759796
2955.645577	231650.004985	54.764801
2954.836445	231312.197745	54.769805
2954.747923	230978.351610	54.774810
2953.561997	230645.367902	54.779815
2953.170776	230311.393902	54.784820
2952.110833	229990.894488	54.789825
2952.082588	229657.985783	54.794829
2951.187015	229315.642043	54.799834
2950.395516	228993.856116	54.804839
2950.071349	228658.095419	54.809844
2949.369602	228314.553690	54.814849
2948.478592	227976.008244	54.819853
2947.837972	227644.044406	54.824858
2947.197260	227315.366361	54.829863
2946.574383	226968.456708	54.834868
2945.844041	226651.342005	54.839873
2945.174228	226305.906538	54.844877
2944.729496	225971.499543	54.849882
2943.740313	225649.986774	54.854887
2943.204757	225313.890988	54.859892
2942.664832	224973.125312	54.864897
2941.775448	224642.256793	54.869901
2941.140573	224313.589844	54.874906
2940.334213	223978.688233	54.879911
2939.826527	223642.442302	54.884916
2939.097545	223319.586528	54.889921
2938.400846	222989.241822	54.894925
2937.890595	222644.980791	54.899930
2937.065032	222319.140247	54.904935
2936.764283	221987.527830	54.909940
2935.900199	221659.201186	54.914945
2935.059790	221320.115724	54.919949
2934.767773	220978.424528	54.924954
2933.628725	220646.326991	54.929959
2933.418905	220321.288675	54.934964
2932.390538	219997.208792	54.939969
2931.623149	219659.226821	54.944973
2931.338285	219317.389441	54.949978
2930.274594	218998.551313	54.954983
2930.008068	218669.723320	54.959988
2929.556551	218329.419053	54.964993
2928.746262	217993.730198	54.969997
2927.940871	217661.924488	54.975002
2927.230097	217329.201614	54.980007
2926.535723	216981.050399	54.985012
2925.527870	216661.768462	54.990017
2925.316136	216324.618151	54.995021
2924.619919	215986.184235	55.000026
2923.866476	215659.802284	55.005031
2923.302868	215331.278913	55.010036
2922.573232	215002.096088	55.015041
2922.062964	214663.664792	55.020045
2921.245893	214333.964499	55.025050
2920.700816	214001.231637	55.030055
2919.961049	213672.375188	55.035060
2919.309775	213328.652646	55.040065
2918.723646	212996.656868	55.045069
2918.339007	212659.272395	55.050074
2917.271149	212331.289243	55.055079
2916.672665	211990.429215	55.060084
2916.160171	211652.293862	55.065089
2915.372265	211319.893204	55.070093
2914.589365	210984.311582	55.075098
2913.904447	210660.260163	55.080103
2913.731423	210317.852637	55.085108
2912.932698	209986.822584	55.090113
2912.022663	209651.930066	55.095117
2911.473184	209300.869489	55.100122
2910.802099	208977.855574	55.105127
2910.082395	208636.294831	55.110132
2909.391595	208300.509537	55.115137
2908.745630	207953.888298	55.120141
2908.037787	207620.731253	55.125146
2907.423068	207294.535654	55.130151
2906.827265	206950.979455	55.135156
2905.845804	206622.147525	55.140161
2905.094747	206291.142863	55.145165
2904.958007	205946.501687	55.150170
2904.003689	205624.250699	55.155175
2903.162083	205295.594964	55.160180
2902.370573	204951.266975	55.165185
2902.197710	204616.833245	55.170189
2901.442902	204288.424034	55.175194
2900.751193	203959.141341	55.180199
2899.889048	203618.994005	55.185204
2899.146135	203294.546466	55.190209
2897.974344	202960.649696	55.195213
2897.917480	202626.120251	55.200218
2897.181596	202302.339085	55.205223
2896.418467	201965.902030	55.210228
2896.163666	201637.721829	55.215233
2895.228839	201314.932365	55.220237
2895.092805	200976.798638	55.225242
2894.018086	200653.971597	55.230247
2893.632564	200312.483811	55.235252
2893.077886	199980.785232	55.240257
2892.083183	199642.134073	55.245261
2891.860002	199305.589781	55.250266
2890.980092	198970.538623	55.255271
2890.242256	198632.871195	55.260276
2889.580171	198297.102655	55.265281
2888.769393	197963.968376	55.270285
2888.514691	197633.178579	55.275290
2887.367921	197286.664541	55.280295
2886.820893	196956.612453	55.285300
2886.319803	196617.177279	55.290305
2885.475359	196285.547841	55.295309
2885.109894	195945.103125	55.300314
2884.334926	195615.477458	55.305319
2883.643092	195266.525565	55.310324
2883.016625	194942.097636	55.315329
2882.416608	194600.808382	55.320333
2881.735471	194257.625712	55.325338
2880.737671	193922.600573	55.330343
2880.421268	193583.118292	55.335348
2879.687853	193252.687220	55.340353
2878.948979	192918.620296	55.345357
2878.444086	192576.871812	55.350362
2877.849342	192251.476696	55.355367
2876.935768	191911.197138	55.360372
2876.419327	191571.913097	55.365377
2875.685331	191231.126389	55.370381
2875.321043	190888.349652	55.375386
2874.211025	190554.128718	55.380391
2873.928966	190215.338754	55.385396
2873.315451	189871.400093	55.390401
2872.512798	189532.455693	55.395405
2871.921865	189199.472504	55.400410
2871.179254	188858.627776	55.405415
2870.537346	188505.059958	55.410420
2869.750535	188176.644194	55.415425
2869.062574	187837.057761	55.420429
2868.795259	187494.150355	55.425434
2867.810054	187162.834387	55.430439
2867.506914	186808.996852	55.435444
2866.566441	186466.992446	55.440449
2865.671504	186136.903609	55.445453
2865.368263	185788.251719	55.450458
2864.394034	185450.394816	55.455463
2864.124605	185102.569750	55.460468
2863.351016	184766.123721	55.465473
2862.579721	184421.194811	55.470477
2862.193777	184076.220265	55.475482
2861.039324	183739.333439	55.480487
2860.766753	183390.021127	55.485492
2859.782304	183055.809418	55.490497
2859.095248	182710.587902	55.495501
2858.313211	182376.349313	55.500506
2857.912871	182046.950236	55.505511
2857.342578	181695.396157	55.510516
2856.436931	181362.864021	55.515521
2855.500064	181032.501826	55.520525
2855.254820	180676.935852	55.525530
2854.447601	180346.418480	55.530535
2853.834426	180008.457224	55.535540
2853.153032	179674.796031	55.540545
2852.502983	179331.897986	55.545549
2851.835944	178989.043570	55.550554
2851.320504	178650.378092	55.555559
2850.514793	178308.225319	55.560564
2849.740773	177973.244010	55.565569
2848.961357	177633.280321	55.570573
2848.759851	177286.728440	55.575578
2848.114292	176958.399773	55.580583
2847.128318	176624.200625	55.585588
2846.506913	176278.728494	55.590593
2845.826309	175938.317964	55.595597
2845.335751	175602.140895	55.600602
2844.333931	175264.406884	55.605607
2843.924756	174922.181282	55.610612
2843.129194	174588.579147	55.615617
2842.299291	174251.220641	55.620621
2841.931345	173909.238756	55.625626
2840.936097	173572.891432	55.630631
2840.486733	173242.056338	55.635636
2839.840939	172907.910344	55.640641
2839.071218	172573.456135	55.645645
2838.814672	172221.958346	55.650650
2837.804229	171891.757531	55.655655
2837.204984	171557.958972	55.660660
2836.597845	171188.480144	55.665665
2835.968842	170816.401288	55.670669
2835.736159	170480.175819	55.675674
2834.439019	170141.184260	55.680679
2833.858866	169807.334133	55.685684
2833.416351	169466.814326	55.690689
2832.552565	169132.035810	55.695693
2831.735572	168779.030260	55.700698
2831.079405	168460.705166	55.705703
2830.389071	168106.388742	55.710708
2830.171789	167771.939442	55.715713
2829.494951	167435.429611	55.720717
2829.258639	167089.697650	55.725722
2828.311771	166755.487371	55.730727
2827.528416	166402.981917	55.735732
2826.709300	166072.699347	55.740737
2826.073371	165722.516635	55.745741
2825.314243	165397.901611	55.750746
2824.407273	165066.611996	55.755751
2823.959668	164706.936340	55.760756
2823.443272	164383.792187	55.765761
2822.614187	164047.985656	55.770765
2822.004121	163698.784452	55.775770
2821.271050	163366.084088	55.780775
2820.473871	163027.726311	55.785780
2820.071151	162691.597799	55.790785
2819.407525	162342.087596	55.795789
2818.622404	162009.306273	55.800794
2817.661119	161675.793107	55.805799
2817.243602	161338.916779	55.810804
2816.650500	160996.668134	55.815809
2815.691973	160669.037681	55.820813
2815.319832	160324.853495	55.825818
2814.651105	159996.293442	55.830823
2814.037604	159659.909098	55.835828
2813.341144	159322.613063	55.840833
2812.635689	158987.673600	55.845837
2812.045360	158658.198349	55.850842
2811.463990	158320.169148	55.855847
2811.002995	157972.755008	55.860852
2810.141337	157640.726318	55.865857
2809.198015	157307.086581	55.870861
2809.142587	156955.677631	55.875866
2807.992899	156628.865487	55.880871
2807.232692	156281.681080	55.885876
2806.641877	155937.333541	55.890881
2806.218249	155598.530734	55.895885
2805.370751	155261.412815	55.900890
2804.774620	154934.542006	55.905895
2804.330487	154597.366835	55.910900
2803.471628	154258.061696	55.915905
2802.937886	153926.932557	55.920909
2802.057163	153573.770053	55.925914
2801.349029	153244.912426	55.930919
2800.764199	152899.082485	55.935924
2800.110210	152571.557576	55.940929
2799.141299	152236.739170	55.945933
2798.953076	151880.383690	55.950938
2798.185964	151556.318564	55.955943
2797.480341	151215.558640	55.960948
2796.970678	150875.584665	55.965953
2796.057602	150537.063494	55.970957
2795.478075	150198.925146	55.975962
2794.737177	149862.137671	55.980967
2794.110373	149520.442531	55.985972
2793.234685	149201.145962	55.990977
2792.856842	148865.785662	55.995981
2792.358487	148519.378446	56.000986
2791.183320	148180.097452	56.005991
2790.797392	147848.231317	56.010996
2790.490290	147509.734997	56.016001
2789.866039	147174.876295	56.021005
2788.892651	146833.849374	56.026010
2788.376396	146493.922883	56.031015
2787.542216	146150.047394	56.036020
2786.765745	145811.491131	56.041025
2786.563849	145479.684284	56.046029
2785.601309	145137.314346	56.051034
2784.528569	144797.748560	56.056039
2784.083667	144468.189367	56.061044
2783.723029	144121.249604	56.066049
2782.662764	143779.736094	56.071053
2782.165121	143443.003998	56.076058
2781.599992	143118.294174	56.081063
2780.710199	142777.946520	56.086068
2779.877549	142443.768957	56.091073
2779.175077	142102.852775	56.096077
2779.220158	141769.712558	56.101082
2777.935104	141435.516074	56.106087
2777.402877	141099.221911	56.111092
2777.000167	140762.822037	56.116097
2776.184468	140426.199102	56.121101
2775.048488	140088.004366	56.126106
2774.201834	139769.486340	56.131111
2774.032973	139424.666173	56.136116
2773.500122	139099.384527	56.141121
2772.677734	138771.064997	56.146125
2772.356691	138428.135398	56.151130
2771.518653	138097.856559	56.156135
2770.629290	137754.503900	56.161140
2770.095757	137427.157190	56.166145
2769.452974	137093.669883	56.171149
2768.973602	136765.724870	56.176154
2768.106487	136430.679932	56.181159
2767.570906	136092.677160	56.186164
2766.536392	135761.299716	56.191169
2765.983087	135427.614016	56.196173
2765.640067	135085.451124	56.201178
2764.864473	134755.263696	56.206183
2763.807277	134433.864357	56.211188
2763.459659	134094.927820	56.216193
2762.492056	133774.385465	56.221197
2762.353555	133435.004413	56.226202
2761.216232	133104.740845	56.231207
2760.824837	132766.995604	56.236212
2760.340135	132442.822368	56.241217
2759.487953	132110.340414	56.246221
2759.153652	131776.319617	56.251226
2758.131436	131448.381549	56.256231
2757.339004	131104.965790	56.261236
2756.867175	130779.488651	56.266241
2756.163021	130455.195206	56.271245
2755.743446	130109.446350	56.276250
2754.919017	129789.485364	56.281255
2754.439990	129441.734752	56.286260
2753.852513	129120.486550	56.291265
2753.002018	128769.882048	56.296269
2752.733720	128436.767052	56.301274
2751.589211	128093.139411	56.306279
2750.754463	127760.681127	56.311284
2749.967633	127427.673185	56.316289
2749.328657	127105.567641	56.321293
2748.962123	126775.358499	56.326298
2748.120031	126446.549428	56.331303
2747.826614	126103.916802	56.336308
2747.050598	125770.851184	56.341313
2746.193531	125430.932365	56.346317
2745.582167	125103.995169	56.351322
2745.030723	124768.963408	56.356327
2743.746375	124441.290056	56.361332
2743.708481	124104.915371	56.366337
2742.859704	123780.673135	56.371341
2742.543193	123439.868489	56.376346
2741.572699	123105.254068	56.381351
2741.110857	122771.058489	56.386356
2740.438888	122437.662255	56.391361
2739.613503	122104.332612	56.396365
2739.322891	121771.290677	56.401370
2738.397231	121438.328153	56.406375
2737.245229	121111.957296	56.411380
2736.937174	120774.042439	56.416385
2736.342249	120445.477622	56.421389
2735.788001	120098.507043	56.426394
2734.847937	119775.521918	56.431399
2734.604023	119439.404335	56.436404
2733.968833	119107.987095	56.441409
2732.861123	118777.226605	56.446413
2732.432759	118439.989538	56.451418
2731.995785	118108.287100	56.456423
2731.386583	117768.840367	56.461428
2730.650242	117425.368524	56.466433
2729.524664	117096.060661	56.471437
2729.217221	116764.164646	56.476442
2728.269620	116430.781185	56.481447
2727.600004	116096.482133	56.486452
2727.320368	115755.035951	56.491457
2726.178210	115437.132570	56.496461
2725.887239	115092.828237	56.501466
2725.366794	114760.516122	56.506471
2724.561847	114425.873410	56.511476
2723.759989	114094.077988	56.516481
2723.109165	113750.775628	56.521485
2722.871607	113411.366397	56.526490
2722.082544	113078.370212	56.531495
2721.397980	112749.886881	56.536500
2720.665674	112405.441845	56.541505
2719.547834	112071.483119	56.546509
2718.697572	111739.821875	56.551514
2718.476189	111421.024042	56.556519
2717.912594	111079.013950	56.561524
2717.134419	110756.518040	56.566529
2716.602154	110423.415339	56.571533
2715.936071	110082.653731	56.576538
2715.046463	109756.178150	56.581543
2714.475511	109410.321664	56.586548
2713.829962	109079.806101	56.591553
2713.071481	108746.311572	56.596557
2712.569782	108410.775842	56.601562
2712.225495	108073.455863	56.606567
2711.273771	107740.957556	56.611572
2710.784850	107393.594001	56.616577
2709.992570	107081.294660	56.621581
2709.556892	106719.650025	56.626586
2708.496999	106394.534748	56.631591
2707.862027	106062.466295	56.636596
2707.142181	105721.863459	56.641601
2706.652004	105392.097148	56.646605
2705.980914	105058.417872	56.651610
2705.264375	104719.091390	56.656615
2704.521827	104391.003094	56.661620
2703.795825	104056.014348	56.666625
2703.075070	103731.243376	56.671629
2702.458118	103379.448030	56.676634
2701.954225	103054.855036	56.681639
2701.199942	102718.919190	56.686644
2701.054709	102373.135143	56.691649
2699.988400	102056.638074	56.696653
2699.045055	101716.648645	56.701658
2698.820861	101382.817495	56.706663
2697.985240	101053.071589	56.711668
2697.017773	100715.225631	56.716673
2696.357200	100389.521076	56.721677
2695.893581	100053.431770	56.726682
2695.153069	99724.260609	56.731687
2694.261880	99399.868807	56.736692
2693.700767	99059.369478	56.741697
2692.798534	98736.079757	56.746701
2692.630001	98414.371821	56.751706
2691.695498	98081.138660	56.756711
2691.179753	97757.078518	56.761716
2690.473756	97420.127561	56.766721
2689.672946	97096.610350	56.771725
2689.421290	96765.000679	56.776730
2688.688932	96427.941799	56.781735
2687.725560	96104.077670	56.786740
2687.488261	95761.369426	56.791745
2686.736930	95433.676251	56.796749
2686.137328	95109.001458	56.801754
2685.533400	94784.002291	56.806759
2684.676584	94430.841172	56.811764
2683.948265	94114.020202	56.816769
2683.040734	93783.883783	56.821773
2682.136528	93456.858904	56.826778
2681.597039	93132.558442	56.831783
2681.127520	92799.285497	56.836788
2680.371573	92474.287071	56.841793
2679.624032	92150.959722	56.846797
2679.056978	91829.009810	56.851802
2678.306956	91507.581822	56.856807
2677.954659	91163.257014	56.861812
2676.984783	90845.037472	56.866817
2676.483118	90519.197052	56.871821
2675.835935	90190.353919	56.876826
2674.735583	89867.655046	56.881831
2674.203774	89542.436301	56.886836
2674.168810	89213.764511	56.891841
2673.319561	88889.372971	56.896845
2672.410786	88571.925066	56.901850
2671.774830	88233.631856	56.906855
2671.275208	87911.006398	56.911860
2670.618798	87570.539682	56.916865
2669.562628	87267.379096	56.921869
2669.374813	86930.563139	56.926874
2668.806691	86599.074240	56.931879
2667.842230	86271.545465	56.936884
2667.462188	85941.799219	56.941889
2666.337080	85612.943130	56.946893
2665.937818	85279.780845	56.951898
2665.234168	84965.884550	56.956903
2664.472032	84634.824602	56.961908
2663.916152	84306.120420	56.966913
2662.963573	83991.339923	56.971917
2662.247072	83659.394312	56.976922
2661.555172	83342.135627	56.981927
2660.826693	83021.471290	56.986932
2660.441922	82710.213691	56.991937
2659.463512	82380.167814	56.996941
2658.782464	82063.402097	57.001946
2658.125083	81742.080621	57.006951
2657.792766	81431.486534	57.011956
2657.361336	81098.313196	57.016961
2656.396440	80779.140354	57.021965
2656.234896	80453.292343	57.026970
2655.678740	80131.979724	57.031975
2654.369613	79797.996768	57.036980
2653.855482	79481.877703	57.041985
2653.019224	79162.506657	57.046989
2652.515750	78829.628432	57.051994
2651.966389	78513.079923	57.056999
2650.939599	78194.514532	57.062004
2650.724580	77873.360563	57.067009
2649.685525	77548.990246	57.072013
2649.142118	77229.083358	57.077018
2648.744064	76901.745082	57.082023
2647.932890	76580.116684	57.087028
2647.559428	76260.590943	57.092033
2646.771522	75930.010038	57.097037
2646.097344	75611.752347	57.102042
2645.399016	75279.400196	57.107047
2644.411151	74958.921654	57.112052
2644.357955	74631.692170	57.117057
2643.167216	74311.952992	57.122061
2642.320277	73987.641025	57.127066
2641.864944	73660.155336	57.132071
2641.006590	73335.006837	57.137076
2640.233173	73008.222082	57.142081
2639.431695	72706.438297	57.147085
2638.980308	72386.144004	57.152090
2638.348061	72060.144299	57.157095
2637.405684	71750.960427	57.162100
2637.074986	71422.421262	57.167105
2636.332672	71107.388014	57.172109
2635.802937	70798.191660	57.177114
2635.098738	70477.366561	57.182119
2634.540377	70165.872691	57.187124
2634.053450	69831.259739	57.192129
2633.077431	69527.436625	57.197133
2632.503175	69199.372196	57.202138
2631.767531	68878.046201	57.207143
2631.062368	68569.368798	57.212148
2630.719392	68253.222399	57.217153
2629.555330	67939.630593	57.222157
2628.999990	67623.616748	57.227162
2628.769312	67294.402635	57.232167
2627.526075	66993.805805	57.237172
2626.980139	66667.945493	57.242177
2626.269290	66361.685305	57.247181
2626.054062	66039.114283	57.252186
2625.053683	65728.524617	57.257191
2624.085011	65418.717016	57.262196
2623.782222	65092.417391	57.267201
2623.143916	64782.656366	57.272205
2622.551127	64470.265270	57.277210
2621.818153	64153.782452	57.282215
2621.320997	63832.287385	57.287220
2620.431929	63521.440470	57.292225
2619.535684	63198.952419	57.297229
2619.011398	62889.802442	57.302234
2618.012336	62580.460485	57.307239
2617.215794	62270.876220	57.312244
2616.772101	61960.395869	57.317249
2615.958381	61665.592216	57.322253
2615.442282	61350.954719	57.327258
2614.579985	61042.176614	57.332263
2614.404521	60730.126085	57.337268
2613.810718	60419.365730	57.342273
2612.864197	60119.346430	57.347277
2612.495262	59796.367725	57.352282
2611.589267	59495.028915	57.357287
2610.907751	59187.686618	57.362292
2610.309736	58870.831144	57.367297
2609.605711	58566.326008	57.372301
2608.948764	58258.067798	57.377306
2608.358593	57953.124231	57.382311
2607.358679	57640.866761	57.387316
2606.935169	57333.052204	57.392321
2605.921984	57035.296037	57.397325
2605.258458	56724.535713	57.402330
2604.393419	56420.683247	57.407335
2603.693809	56125.199211	57.412340
2603.596516	55818.010210	57.417345
2602.696399	55527.292402	57.422349
2602.138140	55225.363673	57.427354
2601.368879	54911.568545	57.432359
2600.621462	54607.854087	57.437364
2600.240130	54298.124968	57.442369
2599.422882	54018.901611	57.447373
2598.707259	53698.945248	57.452378
2598.664298	53384.526572	57.457383
2597.331930	53104.455980	57.462388
2596.665773	52789.649617	57.467393
2595.791283	52497.112508	57.472397
2595.462640	52186.411265	57.477402
2594.622677	51881.614939	57.482407
2594.095254	51599.358249	57.487412
2593.663674	51281.987756	57.492417
2592.572287	50985.330135	57.497421
2592.046730	50684.626731	57.502426
2590.809844	50395.762623	57.507431
2590.459416	50101.840055	57.512436
2590.018743	49800.154178	57.517441
2589.202150	49501.310572	57.522445
2588.429276	49217.554908	57.527450
2587.898134	48924.727509	57.532455
2587.287281	48611.311269	57.537460
2586.568137	48321.860984	57.542465
2585.771862	48032.310612	57.547469
2584.982338	47746.929885	57.552474
2584.323755	47437.056351	57.557479
2583.733118	47165.606272	57.562484
2583.107962	46865.774084	57.567489
2582.252833	46579.748915	57.572493
2581.545356	46281.439010	57.577498
2581.146238	46000.683765	57.582503
2580.400205	45722.651132	57.587508
2580.038020	45414.717769	57.592513
2579.386720	45133.273141	57.597517
2578.803470	44835.670318	57.602522
2578.010146	44543.004817	57.607527
2577.145435	44257.809800	57.612532
2576.467639	43949.617094	57.617537
2575.678417	43665.776561	57.622541
2574.934815	43377.872869	57.627546
2573.988841	43101.387477	57.632551
2573.481746	42804.787722	57.637556
2573.426134	42510.872685	57.642561
2572.093587	42244.091434	57.647565
2571.487020	41960.003303	57.652570
2571.099473	41663.669844	57.657575
2570.175063	41391.470998	57.662580
2569.658396	41110.035644	57.667585
2568.840740	40816.203929	57.672589
2568.431145	40528.906758	57.677594
2567.551489	40251.479630	57.682599
2566.440918	39974.953621	57.687604
2565.951205	39690.237997	57.692609
2565.127966	39417.422179	57.697613
2564.386428	39145.908293	57.702618
2563.965026	38879.662672	57.707623
2563.120541	38601.540741	57.712628
2562.509702	38329.021729	57.717633
2561.429309	38058.762929	57.722637
2560.768300	37780.350354	57.727642
2560.053817	37526.056188	57.732647
2558.962706	37268.324396	57.737652
2558.538105	36989.455874	57.742657
2557.402099	36750.366850	57.747661
2556.668279	36488.512397	57.752666
2556.271483	36225.691883	57.757671
2555.195917	35983.865082	57.762676
2554.508018	35736.881592	57.767681
2553.756231	35499.782023	57.772685
2552.798046	35255.864046	57.777690
2552.058617	35015.067940	57.782695
2550.897767	34777.457112	57.787700
2550.236819	34554.092011	57.792705
2549.051901	34339.844822	57.797709
2547.997377	34131.902741	57.802714
2547.462451	33909.596217	57.807719
2546.001989	33713.310765	57.812724
2545.140357	33518.925479	57.817729
2544.139407	33333.041194	57.822733
2543.102450	33141.072778	57.827738
2542.085389	32962.742553	57.832743
2541.020126	32799.931869	57.837748
2540.673973	32623.061815	57.842753
2539.645749	32459.801411	57.847757
2538.669094	32310.961541	57.852762
2538.058584	32147.600092	57.857767
2537.420612	31994.591470	57.862772
2536.379098	31850.885742	57.867777
2535.586974	31708.236768	57.872781
2535.028308	31552.012030	57.877786
2534.354396	31420.970126	57.882791
2533.509411	31295.910158	57.887796
2533.059302	31150.288650	57.892801
2532.439630	31011.486412	57.897805
2531.580007	30872.363132	57.902810
2531.038290	30744.884482	57.907815
2530.308806	30629.302566	57.912820
2529.404795	30481.178768	57.917825
2528.838737	30355.582478	57.922829
2528.472249	30210.839279	57.927834
2527.804630	30090.953805	57.932839
2526.734839	29970.839086	57.937844
2526.597042	29845.355787	57.942849
2525.730081	29711.163511	57.947853
2524.908086	29583.250145	57.952858
2524.629551	29474.071548	57.957863
2523.714831	29334.737846	57.962868
2523.495279	29206.218476	57.967873
2522.648465	29090.925153	57.972877
2522.217113	28942.587151	57.977882
2521.553360	28816.899705	57.982887
2520.695781	28695.432105	57.987892
2520.101302	28571.078442	57.992897
2519.601405	28445.965067	57.997901
2519.061747	28316.704084	58.002906
2518.480743	28193.202693	58.007911
2517.668736	28060.236508	58.012916
2517.090052	27928.855266	58.017921
2516.457470	27808.497654	58.022925
2515.615325	27673.703751	58.027930
2515.176518	27544.832614	58.032935
2514.232039	27424.445156	58.037940
2514.011771	27292.043116	58.042945
2513.253078	27173.992886	58.047949
2512.616120	27035.917620	58.052954
2511.922205	26907.878682	58.057959
2511.325089	26781.339512	58.062964
2510.917303	26651.128678	58.067969
2509.984087	26533.731600	58.072973
2509.428589	26391.034068	58.077978
2508.694281	26266.089250	58.082983
2508.226865	26137.473993	58.087988
2507.554057	26005.625762	58.092993
2506.737928	25877.770773	58.097997
2506.173108	25751.722667	58.103002
2505.300867	25632.637921	58.108007
2505.022672	25503.645506	58.113012
2504.444186	25375.813709	58.118017
2503.406813	25241.904315	58.123021
2502.825573	25102.630086	58.128026
2502.498138	24981.994891	58.133031
2501.657706	24862.262459	58.138036
2501.093906	24716.581740	58.143041
2500.461207	24592.785277	58.148045
2499.716239	24467.200712	58.153050
2499.293795	24343.639772	58.158055
2498.491993	24198.540878	58.163060
2498.131960	24061.058548	58.168065
2497.354329	23943.107760	58.173069
2496.692243	23810.112721	58.178074
2495.928884	23667.425040	58.183079
2495.320210	23542.275482	58.188084
2494.809077	23426.230436	58.193089
2493.747720	23286.284578	58.198093
2493.378977	23141.398312	58.203098
2492.813008	23018.444484	58.208103
2492.302378	22886.028557	58.213108
2491.630704	22743.230413	58.218113
2490.585877	22620.784348	58.223117
2489.894258	22491.970277	58.228122
2489.295236	22362.869370	58.233127
2488.492665	22229.042074	58.238132
2487.994227	22090.684385	58.243137
2487.302644	21966.837970	58.248141
2486.785299	21832.135013	58.253146
2486.125420	21705.890821	58.258151
2485.317752	21574.819174	58.263156
2484.764991	21444.414862	58.268161
2483.853137	21316.838315	58.273165
2483.133883	21198.706852	58.278170
2482.822772	21059.682653	58.283175
2482.036805	20935.765344	58.288180
2481.170467	20808.631789	58.293185
2480.190618	20687.870944	58.298189
2479.976333	20552.777175	58.303194
2479.499715	20425.168075	58.308199
2478.642933	20306.707469	58.313204
2478.172100	20167.841219	58.318209
2477.493654	20047.930438	58.323213
2476.504839	19913.301679	58.328218
2476.173899	19784.354679	58.333223
2475.123454	19670.626189	58.338228
2474.646615	19541.507741	58.343233
2474.053951	19418.521108	58.348237
2473.737944	19274.459776	58.353242
2472.650852	19161.294998	58.358247
2471.997487	19042.177791	58.363252
2471.698784	18898.780309	58.368257
2470.855652	18779.723216	58.373261
2470.237326	18644.403666	58.378266
2470.176344	18522.669577	58.383271
2468.946750	18386.114675	58.388276
2468.416329	18244.483222	58.393281
2467.462674	18124.814770	58.398285
2466.866712	17994.384068	58.403290
2466.382185	17860.721646	58.408295
2465.540162	17743.791395	58.413300
2464.807033	17600.609131	58.418305
2464.083589	17479.005995	58.423309
2463.538577	17345.144078	58.428314
2462.849999	17221.343030	58.433319
2462.308983	17102.057502	58.438324
2461.552764	16974.520960	58.443329
2460.918282	16854.384679	58.448333
2460.119532	16721.939244	58.453338
2459.810351	16591.972539	58.458343
2458.685089	16469.967838	58.463348
2458.550511	16324.788597	58.468353
2457.718594	16209.502979	58.473357
2456.718168	16083.344645	58.478362
2456.358162	15960.416783	58.483367
2455.306983	15835.565513	58.488372
2454.997032	15697.417020	58.493377
2454.373968	15589.402891	58.498381
2453.502187	15454.580058	58.503386
2452.992565	15325.913084	58.508391
2452.024567	15201.294496	58.513396
2451.491477	15086.950939	58.518401
2450.843080	14952.364843	58.523405
2450.091656	14840.795088	58.528410
2449.753400	14704.317992	58.533415
2448.894466	14585.072552	58.538420
2448.252470	14465.179740	58.543425
2447.390035	14339.382305	58.548429
2446.840848	14210.096243	58.553434
2446.150502	14096.622928	58.558439
2445.512215	13987.379517	58.563444
2445.100751	13846.254003	58.568449
2444.458647	13717.184426	58.573453
2443.468687	13605.954368	58.578458
2442.839461	13481.754466	58.583463
2442.201164	13363.805600	58.588468
2441.670161	13243.245338	58.593473
2440.826131	13111.503471	58.598477
2440.177106	12994.832236	58.603482
2439.697674	12868.000276	58.608487
2438.828842	12747.616260	58.613492
2438.206343	12630.132202	58.618497
2437.429840	12512.949460	58.623501
2436.358391	12389.071526	58.628506
2436.224847	12272.374208	58.633511
2435.426414	12160.948376	58.638516
2434.843217	12035.799061	58.643521
2434.212047	11912.741740	58.648525
2433.580601	11804.478927	58.653530
2432.840562	11675.201427	58.658535
2431.839449	11571.016603	58.663540
2431.290174	11448.226436	58.668545
2430.853755	11340.623080	58.673549
2430.030899	11216.900934	58.678554
2429.666510	11103.875430	58.683559
2428.716114	10994.108275	58.688564
2428.259041	10870.333729	58.693569
2427.471775	10747.691133	58.698573
2426.707791	10634.760505	58.703578
2426.304875	10517.029202	58.708583
2425.535087	10411.655469	58.713588
2425.014870	10287.991178	58.718593
2424.148048	10177.220024	58.723597
2423.512998	10062.005307	58.728602
2422.848115	9938.271357	58.733607
2422.049295	9826.942086	58.738612
2421.254574	9707.537193	58.743617
2420.496789	9607.765250	58.748621
2419.708417	9485.001750	58.753626
2419.294365	9366.690677	58.758631
2418.544976	9268.583141	58.763636
2417.807843	9157.536222	58.768641
2417.307139	9052.461094	58.773645
2416.531449	8940.500431	58.778650
2415.887410	8837.719256	58.783655
2415.126789	8726.678070	58.788660
2414.712248	8616.005290	58.793665
2413.769868	8499.267179	58.798669
2412.807690	8407.539778	58.803674
2412.577434	8288.763527	58.808679
2411.796184	8192.770075	58.813684
2410.987934	8085.220560	58.818689
2410.525464	7982.851137	58.823693
2410.009830	7875.459474	58.828698
2409.114200	7764.776190	58.833703
2408.138497	7662.362945	58.838708
2407.775377	7563.767135	58.843713
2406.871741	7455.244127	58.848717
2406.260260	7360.676635	58.853722
2405.997305	7250.867906	58.858727
2404.894669	7160.298476	58.863732
2404.163335	7064.952786	58.868737
2403.290825	6965.524308	58.873741
2402.603773	6871.806472	58.878746
2401.865484	6774.528007	58.883751
2401.018739	6688.553533	58.888756
2400.560132	6591.010268	58.893761
2399.502394	6494.945396	58.898765
2398.719119	6415.262512	58.903770
2398.181148	6326.179109	58.908775
2397.491751	6244.802151	58.913780
2396.506120	6160.067481	58.918785
2396.413007	6078.395748	58.923789
2395.272698	5993.192791	58.928794
2394.818518	5917.082406	58.933799
2393.971913	5849.079950	58.938804
2393.440811	5762.737406	58.943809
2392.415446	5679.545122	58.948813
2391.615484	5605.225627	58.953818
2391.218756	5525.154180	58.958823
2390.544446	5459.074383	58.963828
2389.557880	5381.460296	58.968833
2389.147221	5307.518313	58.973837
2388.501575	5245.490563	58.978842
2387.980821	5155.371150	58.983847
2386.795547	5095.317795	58.988852
2386.454040	5010.294345	58.993857
2385.833981	4938.247986	58.998861
2385.105978	4874.248892	59.003866
2384.256867	4796.402350	59.008871
2383.762832	4737.647885	59.013876
2382.937053	4665.680437	59.018881
2382.389406	4610.099218	59.023885
2381.480938	4539.778087	59.028890
2381.045673	4463.190310	59.033895
2380.349144	4404.003964	59.038900
2379.788220	4331.709860	59.043905
2379.165055	4260.048243	59.048909
2378.077646	4189.224812	59.053914
2377.671706	4130.673318	59.058919
2376.906796	4056.468069	59.063924
2376.213538	3990.486197	59.068929
2375.596682	3935.520249	59.073933
2374.978753	3869.071924	59.078938
2374.671950	3795.217278	59.083943
2373.560998	3746.383254	59.088948
2372.911126	3669.646733	59.093953
2372.691178	3610.329653	59.098957
2371.537750	3552.816183	59.103962
2371.035063	3482.891598	59.108967
2370.644612	3420.890225	59.113972
2369.591461	3356.343641	59.118977
2368.904094	3305.850111	59.123981
2368.109184	3243.458593	59.128986
2367.480969	3175.164950	59.133991
2366.834537	3111.372744	59.138996
2366.423566	3056.752033	59.144001
2365.519613	2992.874216	59.149005
2364.805537	2933.550698	59.154010
2364.449300	2865.947977	59.159015
2363.586192	2817.008362	59.164020
2362.955783	2752.073298	59.169025
2362.383150	2692.642372	59.174029
2361.556153	2640.212857	59.179034
2361.310476	2578.076174	59.184039
2360.308104	2525.373645	59.189044
2359.760764	2458.859807	59.194049
2359.138089	2404.713553	59.199053
2358.249438	2343.951007	59.204058
2357.928171	2288.955412	59.209063
2357.031551	2230.289822	59.214068
2356.377697	2165.335853	59.219073
2355.563691	2107.017241	59.224077
2354.831124	2056.437421	59.229082
2354.547387	2002.037044	59.234087
2353.538142	1949.835265	59.239092
2352.893323	1890.574398	59.244097
2352.128267	1840.539845	59.249101
2351.321006	1788.900384	59.254106
2350.825256	1729.193879	59.259111
2350.066105	1684.593511	59.264116
2349.389887	1627.352610	59.269121
2348.863861	1577.941841	59.274125
2348.095415	1536.825537	59.279130
2347.468355	1472.551696	59.284135
2346.912954	1437.689556	59.289140
2346.299550	1380.204688	59.294145
2345.555215	1322.559453	59.299149
2344.961978	1286.349012	59.304154
2344.317723	1220.054118	59.309159
2343.517699	1175.627384	59.314164
2343.084823	1121.847693	59.319169
2342.134384	1076.826141	59.324173
2341.486073	1034.804358	59.329178
2341.032131	979.863135	59.334183
2340.226804	941.004734	59.339188
2339.535237	885.871312	59.344193
2338.773646	833.202974	59.349197
2338.180417	788.285734	59.354202
2337.450778	749.023180	59.359207
2336.700001	704.960667	59.364212
2336.061028	645.085790	59.369217
2335.325484	617.910300	59.374221
2334.874433	564.239638	59.379226
2334.521025	508.714980	59.384231
2333.515552	475.377317	59.389236
2332.883669	424.135948	59.394241
2331.992622	384.753328	59.399245
2330.841354	337.612640	59.404250
2330.469370	300.262580	59.409255
2329.423860	267.076827	59.414260
2329.322883	222.400235	59.419265
2328.369397	198.998946	59.424269
2327.699215	151.511343	59.429274
2327.169100	115.296977	59.434279
2326.075442	95.794096	59.439284
2325.303003	70.292268	59.444289
2324.274308	20.427237	59.449293
2322.554946	31.971652	59.454298
2320.898808	38.266055	59.459303
2319.497863	71.803318	59.464308
2318.930094	71.463028	59.469313
2319.613253	72.207932	59.474317
2318.612037	78.776938	59.479322
2318.752817	71.072154	59.484327
2317.702358	88.589441	59.489332
2316.797379	77.955071	59.494337
2316.654731	84.573985	59.499341
2315.507111	94.521844	59.504346
2315.141056	94.444441	59.509351
2314.612884	94.060026	59.514356
2313.807490	96.111725	59.519361
2313.348478	93.317888	59.524365
2312.877948	101.109982	59.529370
2312.396422	89.361388	59.534375
2311.512709	100.863211	59.539380
2310.246325	92.946371	59.544385
2309.662254	84.903974	59.549389
2309.125357	98.392865	59.554394
2308.614511	83.025228	59.559399
2308.330083	105.358292	59.564404
2307.862153	93.631193	59.569409
2307.470555	101.076468	59.574413
2306.632756	107.346768	59.579418
2305.787480	101.859360	59.584423
2305.008597	97.523594	59.589428
2304.009911	96.043752	59.594433
2303.290526	99.568822	59.599437
2302.867639	107.627744	59.604442
2302.706088	93.598673	59.609447
2301.829978	101.783089	59.614452
2301.120081	95.943065	59.619457
2300.103046	96.090334	59.624461
2299.347779	90.971841	59.629466
2299.491826	86.404547	59.634471
2298.518538	105.794005	59.639476
2297.996141	97.375984	59.644481
2297.039063	91.595667	59.649485
2296.163614	94.462697	59.654490
2295.438582	92.247199	59.659495
2294.923912	93.358694	59.664500
2294.852746	110.913072	59.669505
2294.638077	93.748101	59.674509
2293.613386	98.075351	59.679514
2292.986592	96.199073	59.684519
2291.600306	95.447738	59.689524
2291.030248	99.367003	59.694529
2290.369031	87.254272	59.699533
2289.354874	104.374758	59.704538
2288.748158	95.823463	59.709543
2289.097877	97.907991	59.714548
2288.359636	94.541882	59.719553
2287.912905	101.972250	59.724557
2287.074423	95.094531	59.729562
2285.839317	88.793791	59.734567
2284.823774	93.084900	59.739572
2284.532171	92.032212	59.744577
2283.943331	95.743153	59.749581
2283.171958	103.923578	59.754586
2282.898349	102.448581	59.759591
2282.010266	97.127240	59.764596
2281.477169	92.531734	59.769601
2281.330226	96.973647	59.774605
2280.096711	105.186374	59.779610
2279.971727	95.081125	59.784615
2278.717667	95.124077	59.789620
2278.149664	92.262382	59.794625
2277.890135	89.436912	59.799629
2276.913714	94.447189	59.804634
2276.507807	90.623111	59.809639
2275.484791	85.744209	59.814644
2275.216709	87.149318	59.819649
2274.469872	87.554926	59.824653
2273.169161	87.214211	59.829658
2272.946479	87.856789	59.834663
2272.383329	94.526636	59.839668
2271.446165	93.778187	59.844673
2271.143477	93.337516	59.849677
2270.217051	93.804726	59.854682
2269.736504	86.409791	59.859687
2268.857225	89.089785	59.864692
2267.895457	94.455695	59.869697
2267.385738	86.343172	59.874701
2266.734134	91.032282	59.879706
2266.141812	91.392883	59.884711
2265.862913	94.236258	59.889716
2265.562272	99.448421	59.894721
2264.693683	87.218788	59.899725
2263.374207	92.980470	59.904730
2262.772064	84.530962	59.909735
2262.509054	93.261505	59.914740
2262.273190	92.062789	59.919745
2261.288365	92.495111	59.924750
2260.161208	84.583027	59.929754
2259.597793	90.480239	59.934759
2259.727532	85.692873	59.939764
2258.488996	95.554251	59.944769
2257.617637	86.962950	59.949774
2256.936825	89.799117	59.954778
2257.054559	96.958606	59.959783
2255.725624	100.935176	59.964788
2255.149147	89.211123	59.969793
2254.532484	96.575409	59.974798
2253.702298	103.631383	59.979802
2253.612113	100.112027	59.984807
2252.666932	92.353996	59.989812
2251.849098	83.207029	59.994817
2251.264623	87.994298	59.999822
2250.032462	83.938604	60.004826
2250.482141	88.539756	60.009831
2249.426474	87.865304	60.014836
2248.233969	91.132710	60.019841
2248.033575	90.508665	60.024846
2247.240955	93.736293	60.029850
2247.235619	91.441340	60.034855
2246.243519	89.324989	60.039860
2245.356037	90.301673	60.044865
2245.059885	86.280426	60.049870
2244.093137	79.467231	60.054874
2243.713907	84.654010	60.059879
2243.113089	83.681915	60.064884
2242.428516	86.081883	60.069889
2241.565825	84.470111	60.074894
2240.253498	84.088679	60.079898
2240.080677	79.138006	60.084903
2239.931396	90.305724	60.089908
2238.676156	102.024186	60.094913
2238.042361	85.540713	60.099918
2237.045300	91.038381	60.104922
2236.822915	93.188423	60.109927
2235.936275	87.362269	60.114932
2235.394514	96.778826	60.119937
2235.191676	78.673762	60.124942
2233.977550	90.548115	60.129946
2233.647291	80.221567	60.134951
2233.200531	92.317956	60.139956
2232.591830	89.629879	60.144961
2231.983689	93.585155	60.149966
2231.158583	98.131492	60.154970
2230.656136	96.669150	60.159975
2229.570330	95.092774	60.164980
2228.191907	95.831964	60.169985
2228.315082	82.232398	60.174990
2227.424665	96.557931	60.179994
2227.172008	84.708409	60.184999
2226.236550	81.200150	60.190004
2225.054173	88.751945	60.195009
2224.960095	76.188173	60.200014
2224.092673	95.004192	60.205018
2224.219384	75.419772	60.210023
2223.504649	89.969732	60.215028
2222.671905	88.070953	60.220033
2222.300622	88.789146	60.225038
2221.064628	87.799549	60.230042
2220.149715	75.055346	60.235047
2219.512376	80.910673	60.240052
2219.015188	79.650919	60.245057
2218.224005	74.082437	60.250062
2217.398837	86.951605	60.255066
2217.465760	83.090378	60.260071
2216.451642	92.190798	60.265076
2215.944349	80.682863	60.270081
2215.405541	81.995311	60.275086
2214.501676	87.498700	60.280090
2214.326758	83.902910	60.285095
2213.683656	95.410732	60.290100
2212.103568	79.443233	60.295105
2211.318417	89.120740	60.300110
2210.825202	82.508394	60.305114
2210.364217	93.807558	60.310119
2209.624758	102.257312	60.315124
2208.892201	87.158260	60.320129
2208.955097	73.800069	60.325134
2207.956531	100.595460	60.330138
2206.900794	81.165503	60.335143
2206.715251	84.325217	60.340148
2205.803677	83.503350	60.345153
2205.884124	93.450380	60.350158
2205.245451	85.205374	60.355162
2204.060798	90.229784	60.360167
2203.161511	85.162558	60.365172
2202.266733	91.982790	60.370177
2201.627865	79.693096	60.375182
2200.929367	87.273787	60.380186
2200.555502	82.632544	60.385191
2199.906372	85.902072	60.390196
2199.593169	89.148269	60.395201
2198.974809	87.590787	60.400206
2198.314914	88.469882	60.405210
2197.829300	84.754656	60.410215
2196.302175	92.342232	60.415220
2195.540494	80.933005	60.420225
2195.045210	85.647787	60.425230
2194.537295	80.811779	60.430234
2194.177845	88.658792	60.435239
2193.710210	87.660849	60.440244
2192.871579	86.836875	60.445249
2192.669779	77.235829	60.450254
2191.782604	91.969263	60.455258
2190.407391	82.781442	60.460263
2189.491985	83.557578	60.465268
2189.301922	88.611855	60.470273
2188.596705	80.268609	60.475278
2187.750181	89.578981	60.480282
2187.334160	92.109815	60.485287
2187.150252	82.228394	60.490292
2186.189536	78.719428	60.495297
2185.835697	77.473208	60.500302
2185.233299	87.993745	60.505306
2184.563154	80.176348	60.510311
2183.594949	74.320585	60.515316
2182.430346	82.911895	60.520321
2182.099458	75.592590	60.525326
2181.388358	86.821049	60.530330
2181.017579	78.205561	60.535335
2180.557934	82.629274	60.540340
2180.036754	87.368667	60.545345
2178.840705	77.545330	60.550350
2177.820875	85.735222	60.555354
2177.167252	85.366007	60.560359
2176.788041	80.812346	60.565364
2176.025355	93.536002	60.570369
2175.782048	78.263163	60.575374
2175.198734	85.500744	60.580378
2174.948757	90.313802	60.585383
2174.050310	87.993395	60.590388
2172.597580	88.632443	60.595393
2171.778194	84.404073	60.600398
2171.416211	85.573364	60.605402
2170.883458	85.448315	60.610407
2170.494642	71.154165	60.615412
2169.630800	80.049406	60.620417
2169.726550	78.001761	60.625422
2168.817301	84.614568	60.630426
2167.974882	82.269506	60.635431
2166.936654	83.530318	60.640436
2165.971849	92.034749	60.645441
2165.707031	81.943828	60.650446
2165.056542	89.382874	60.655450
2164.742299	81.848048	60.660455
2163.999486	87.627085	60.665460
2162.645617	86.414954	60.670465
2161.888348	76.701778	60.675470
2161.246460	80.485806	60.680474
2160.766728	89.250730	60.685479
2160.450339	76.252329	60.690484
2159.411788	84.322198	60.695489
2159.396877	81.576201	60.700494
2158.537283	85.383734	60.705498
2158.181987	84.577700	60.710503
2157.923376	91.293857	60.715508
2156.767945	89.421066	60.720513
2156.142634	79.347922	60.725518
2155.222172	84.376163	60.730522
2154.755935	83.322815	60.735527
2153.419722	88.536863	60.740532
2152.752627	90.667585	60.745537
2152.383429	77.901481	60.750542
2151.532086	78.623312	60.755546
2151.176110	80.745669	60.760551
2150.702326	76.183366	60.765556
2149.864998	80.626007	60.770561
2149.726453	81.897038	60.775566
2148.872242	91.978161	60.780570
2148.213419	82.230444	60.785575
2147.385441	85.621395	60.790580
2146.247701	89.495140	60.795585
2146.107670	89.905427	60.800590
2145.224282	86.865157	60.805594
2144.888592	84.460203	60.810599
2143.883757	76.528775	60.815604
2142.991110	93.149045	60.820609
2142.505082	84.736344	60.825614
2141.745524	84.888551	60.830618
2141.195632	75.986115	60.835623
2140.908862	76.159497	60.840628
2140.361755	76.757369	60.845633
2139.787841	78.698273	60.850638
2138.219890	86.732304	60.855642
2137.283637	74.712165	60.860647
2136.880077	75.418143	60.865652
2136.163658	84.442963	60.870657
2136.329629	79.459047	60.875662
2135.462586	85.410758	60.880666
2135.022196	71.478025	60.885671
2134.512044	82.825985	60.890676
2133.533262	86.652436	60.895681
2132.623939	77.515307	60.900686
2131.440358	88.681553	60.905690
2130.836373	82.000074	60.910695
2130.893305	84.492140	60.915700
2129.949384	89.150389	60.920705
2129.879782	82.620654	60.925710
2129.194431	85.148499	60.930714
2128.562858	69.785905	60.935719
2127.433952	81.697224	60.940724
2126.794215	81.210706	60.945729
2126.303259	71.620864	60.950734
2125.403233	85.247791	60.955738
2124.834653	79.197760	60.960743
2123.929247	77.301083	60.965748
2122.981679	81.944142	60.970753
2122.762403	75.911226	60.975758
2121.969999	79.859487	60.980762
2121.572224	87.449244	60.985767
2120.922300	74.385510	60.990772
2120.567682	92.642374	60.995777
2120.295914	74.512016	61.000782
2118.839577	84.559376	61.005786
2118.180031	81.729594	61.010791
2117.827191	88.575815	61.015796
2117.031687	88.535044	61.020801
2116.474168	91.334334	61.025806
2115.374127	88.951323	61.030810
2114.442626	83.050339	61.035815
2114.186249	85.253087	61.040820
2113.041221	79.999396	61.045825
2112.632686	83.982941	61.050830
2112.166669	80.315086	61.055834
2111.805720	87.003328	61.060839
2111.675788	76.526758	61.065844
2110.596658	93.006319	61.070849
2109.731361	71.616105	61.075854
2108.925523	94.158009	61.080858
2108.610502	90.485115	61.085863
2108.026439	89.295937	61.090868
2106.687152	85.492271	61.095873
2106.158921	81.375415	61.100878
2105.156359	74.777692	61.105882
2104.551661	88.045540	61.110887
2104.606434	83.820404	61.115892
2103.605699	90.677974	61.120897
2103.528326	86.593650	61.125902
2103.055481	88.330875	61.130906
2102.007817	80.294301	61.135911
2101.480872	80.486876	61.140916
2100.406165	84.148794	61.145921
2099.946240	81.907058	61.150926
2098.737469	78.669290	61.155930
2098.051632	90.261170	61.160935
2097.262752	75.987944	61.165940
2096.524177	78.992576	61.170945
2096.383937	80.416836	61.175950
2096.127002	77.281911	61.180954
2095.450199	70.219359	61.185959
2095.409468	77.312504	61.190964
2094.151049	71.449218	61.195969
2093.363386	72.194076	61.200974
2092.800423	74.655200	61.205978
2091.263356	70.331021	61.210983
2090.557666	80.271891	61.215988
2089.883559	82.252357	61.220993
2090.311150	74.057385	61.225998
2089.408657	76.805767	61.231002
2088.866006	75.313567	61.236007
2088.452979	74.989771	61.241012
2086.947666	74.974917	61.246017
2086.114004	78.790968	61.251022
2085.324011	68.174733	61.256026
2084.900738	77.159346	61.261031
2084.843606	79.816160	61.266036
2084.242325	83.672605	61.271041
2083.766285	85.985903	61.276046
2082.634649	83.246814	61.281050
2081.517494	72.914296	61.286055
2081.003503	76.652813	61.291060
2080.373328	85.052124	61.296065
2080.194312	84.803154	61.301070
2079.756513	75.933410	61.306074
2078.713996	78.432791	61.311079
2077.972467	80.449188	61.316084
2077.163579	84.198237	61.321089
2076.809363	80.194117	61.326094
2076.164759	84.932611	61.331098
2075.548729	75.671699	61.336103
2074.802218	87.754158	61.341108
2073.718331	83.194075	61.346113
2073.625812	79.027007	61.351118
2072.921000	87.146441	61.356122
2071.867250	81.813632	61.361127
2071.346088	80.267565	61.366132
2070.174192	83.842419	61.371137
2070.070820	82.412972	61.376142
2069.673077	92.041645	61.381146
2069.231184	86.931847	61.386151
2068.665119	78.659600	61.391156
2067.204981	92.768074	61.396161
2066.876095	83.448978	61.401166
2066.629703	84.984698	61.406170
2065.490084	85.823264	61.411175
2064.336309	85.069843	61.416180
2063.355528	89.536851	61.421185
2063.213274	85.339830	61.426190
2062.803591	86.292786	61.431194
2062.193111	81.796348	61.436199
2062.283518	72.782865	61.441204
2061.305425	84.414816	61.446209
2060.097402	74.309609	61.451214
2059.985579	77.594817	61.456218
2058.809651	86.173777	61.461223
2058.281114	80.297175	61.466228
2056.639397	81.193348	61.471233
2056.167009	83.718951	61.476238
2056.252552	82.693168	61.481242
2055.453696	85.136545	61.486247
2055.238439	81.274373	61.491252
2054.669558	81.092005	61.496257
2054.032967	76.333221	61.501262
2052.971179	82.145555	61.506266
2051.871603	77.933311	61.511271
2051.442474	80.985037	61.516276
2050.881229	89.816521	61.521281
2050.441987	80.156990	61.526286
2049.441767	83.069122	61.531290
2048.616079	89.463707	61.536295
2047.949005	77.973301	61.541300
2047.434136	86.340127	61.546305
2047.075012	80.540717	61.551310
2046.651924	78.198533	61.556314
2046.178534	89.146448	61.561319
2045.421023	78.875136	61.566324
2044.377071	81.436257	61.571329
2043.701541	82.164911	61.576334
2043.115557	94.881044	61.581338
2042.330801	76.696507	61.586343
2041.575452	76.885919	61.591348
2040.712685	77.852439	61.596353
2040.223440	79.209092	61.601358
2039.723753	77.076177	61.606362
2039.185551	70.999276	61.611367
2038.084141	74.088312	61.616372
2036.934607	86.557998	61.621377
2036.725648	75.065854	61.626382
2036.326679	84.822445	61.631386
2035.930919	76.010693	61.636391
2035.355956	80.799639	61.641396
2035.055186	76.965234	61.646401
2034.381576	84.819535	61.651406
2033.193149	79.012977	61.656410
2032.336690	77.972699	61.661415
2031.972588	71.674212	61.666420
2030.639267	77.982212	61.671425
2029.956148	77.847941	61.676430
2029.389401	86.421690	61.681434
2028.787075	81.003065	61.686439
2028.466620	80.227790	61.691444
2028.159571	75.962315	61.696449
2027.862753	76.753867	61.701454
2026.834802	79.561602	61.706458
2026.047232	80.729071	61.711463
2025.550997	91.507158	61.716468
2024.427194	81.339715	61.721473
2023.278048	79.059153	61.726478
2023.004395	85.260479	61.731482
2022.352268	79.338850	61.736487
2021.951356	75.901946	61.741492
2021.582172	86.065379	61.746497
2021.150341	76.529256	61.751502
2019.660907	75.335564	61.756506
2019.028366	87.105065	61.761511
2018.715769	75.703486	61.766516
2018.339302	79.472224	61.771521
2017.173688	82.908913	61.776526
2016.238957	77.271826	61.781530
2015.527501	82.180206	61.786535
2015.396922	80.299360	61.791540
2014.676605	83.690606	61.796545
2014.307875	71.391231	61.801550
2013.539782	81.774084	61.806554
2012.760040	79.289825	61.811559
2012.205384	80.235836	61.816564
2011.387509	75.742369	61.821569
2010.712398	76.073591	61.826574
2009.730251	74.447745	61.831578
2009.104314	73.785609	61.836583
2009.041992	77.499758	61.841588
2008.480791	76.549815	61.846593
2007.547107	72.527298	61.851598
2006.471891	73.048173	61.856602
2005.882079	72.485956	61.861607
2005.257499	74.152664	61.866612
2004.896702	81.640367	61.871617
2004.335949	76.921597	61.876622
2003.320263	79.465631	61.881626
2002.451270	72.775796	61.886631
2002.006823	68.118992	61.891636
2001.575246	75.728308	61.896641
2001.297624	74.302868	61.901646
1999.700249	83.128503	61.906650
1999.224864	86.744218	61.911655
1998.917904	71.852104	61.916660
1998.452343	83.631370	61.921665
1997.643970	72.335294	61.926670
1996.542113	82.193986	61.931674
1995.647436	78.980530	61.936679
1995.626792	78.723775	61.941684
1994.580465	82.944174	61.946689
1994.368921	71.107114	61.951694
1993.844997	83.520090	61.956698
1992.771850	83.554962	61.961703
1992.212993	85.378393	61.966708
1991.506149	76.630218	61.971713
1991.160047	82.456707	61.976718
1990.129684	76.863193	61.981722
1989.007277	78.086972	61.986727
1988.851710	75.491036	61.991732
1988.414464	84.900482	61.996737
1988.008312	77.716160	62.001742
1987.254085	81.626859	62.006746
1986.170268	69.254921	62.011751
1985.913611	72.230394	62.016756
1985.013303	73.292772	62.021761
1983.778853	75.567196	62.026766
1982.948686	74.998981	62.031770
1982.561072	70.266931	62.036775
1982.313786	73.378106	62.041780
1981.541087	79.166653	62.046785
1981.393345	73.445667	62.051790
1980.992577	78.063476	62.056794
1979.437404	81.207213	62.061799
1979.074384	85.309699	62.066804
1978.316271	79.611478	62.071809
1977.768819	71.091891	62.076814
1976.867130	79.305663	62.081818
1975.522574	67.919672	62.086823
1975.311550	72.777010	62.091828
1974.762353	72.522153	62.096833
1974.687742	71.837167	62.101838
1974.055299	75.039439	62.106842
1973.469480	84.199668	62.111847
1972.596376	77.166734	62.116852
1971.779839	82.823478	62.121857
1971.375173	65.988394	62.126862
1970.250556	77.012866	62.131866
1969.333145	71.133365	62.136871
1968.547468	79.256187	62.141876
1968.241050	82.327868	62.146881
1967.850936	69.614027	62.151886
1967.328427	81.897474	62.156890
1966.661713	77.917747	62.161895
1965.988477	76.353267	62.166900
1964.959623	82.450549	62.171905
1964.670437	66.898067	62.176910
1964.122268	70.753985	62.181914
1963.077318	71.993863	62.186919
1962.199496	72.207469	62.191924
1961.552400	81.505152	62.196929
1961.309157	77.300520	62.201934
1960.867396	73.128977	62.206938
1959.911501	82.064110	62.211943
1959.347403	77.703836	62.216948
1958.462877	77.524287	62.221953
1958.046092	79.733585	62.226958
1956.826363	73.134134	62.231962
1956.157478	73.763988	62.236967
1955.887169	71.356572	62.241972
1955.204962	80.347605	62.246977
1954.993102	76.554291	62.251982
1954.308305	70.797137	62.256986
1952.952888	73.079739	62.261991
1952.540585	73.503293	62.266996
1951.893986	78.379314	62.272001
1951.412315	70.592006	62.277006
1950.431429	81.376062	62.282010
1949.528558	71.096330	62.287015
1949.016526	71.341759	62.292020
1948.267260	78.011226	62.297025
1947.937236	67.106002	62.302030
1947.730991	73.500043	62.307034
1946.757414	72.625035	62.312039
1946.147767	71.983982	62.317044
1945.409003	71.480114	62.322049
1944.985970	77.610539	62.327054
1944.122190	76.640836	62.332058
1943.034044	66.349522	62.337063
1942.431108	73.620205	62.342068
1941.470298	70.267466	62.347073
1941.739311	70.075113	62.352078
1941.207313	66.372043	62.357082
1939.867508	81.923227	62.362087
1939.274606	67.784545	62.367092
1938.599211	72.800750	62.372097
1938.187261	76.488400	62.377102
1937.926470	72.784854	62.382106
1936.486374	70.999930	62.387111
1935.645387	71.682340	62.392116
1934.733833	72.211956	62.397121
1934.804637	73.487608	62.402126
1934.521944	65.624568	62.407130
1933.597028	61.509232	62.412135
1933.078867	69.260022	62.417140
1931.808328	82.076936	62.422145
1931.658265	70.614890	62.427150
1931.074854	70.786501	62.432154
1929.729825	77.588390	62.437159
1929.157983	70.203316	62.442164
1928.532944	74.322168	62.447169
1928.220639	69.634941	62.452174
1928.062186	77.740201	62.457178
1926.627539	78.434856	62.462183
1926.284170	73.509719	62.467188
1925.519443	79.506740	62.472193
1925.230947	65.524737	62.477198
1924.049843	75.534792	62.482202
1922.752861	72.511381	62.487207
1922.308908	75.579667	62.492212
1921.830150	69.135410	62.497217
1921.674039	76.191669	62.502222
1921.434548	76.989900	62.507226
1920.615625	74.258013	62.512231
1919.737373	79.255967	62.517236
1919.104166	82.740635	62.522241
1918.590645	66.734944	62.527246
1917.490712	74.601747	62.532250
1916.573903	78.913570	62.537255
1916.465511	69.078565	62.542260
1915.589215	64.304264	62.547265
1915.232310	71.215786	62.552270
1914.423696	79.682868	62.557274
1913.496969	73.530490	62.562279
1913.096529	72.960307	62.567284
1912.565739	78.797196	62.572289
1911.675849	66.645240	62.577294
1910.768236	75.131190	62.582298
1909.979506	75.295978	62.587303
1909.902977	71.345574	62.592308
1909.344619	68.550250	62.597313
1908.366567	72.367195	62.602318
1907.803172	67.877522	62.607322
1906.914604	74.308924	62.612327
1906.641844	72.023324	62.617332
1905.720495	76.473059	62.622337
1904.877034	71.843352	62.627342
1904.430433	72.161976	62.632346
1903.733531	82.006868	62.637351
1903.483095	73.291923	62.642356
1902.108220	67.825682	62.647361
1901.581791	82.676922	62.652366
1901.111909	79.695671	62.657370
1900.541772	77.373706	62.662375
1900.034373	72.111932	62.667380
1898.670393	73.840857	62.672385
1898.127630	64.912141	62.677390
1897.608792	73.262259	62.682394
1897.062349	71.158874	62.687399
1896.671262	65.825025	62.692404
1895.220493	55.952418	62.697409
1894.553444	74.780792	62.702414
1894.150210	79.769570	62.707418
1893.567184	77.102738	62.712423
1893.589404	69.804704	62.717428
1893.016266	72.697970	62.722433
1892.248063	69.918618	62.727438
1891.557763	60.515035	62.732442
1890.707659	79.148559	62.737447
1889.712507	63.637220	62.742452
1888.554569	71.978420	62.747457
1887.674713	70.993943	62.752462
1887.397994	63.560454	62.757466
1886.964639	66.920360	62.762471
1886.987942	74.161013	62.767476
1886.291194	72.076763	62.772481
1885.499959	71.888735	62.777486
1884.605778	70.233204	62.782490
1883.824524	76.095668	62.787495
1883.793815	63.731632	62.792500
1882.796833	69.737148	62.797505
1881.966560	65.248854	62.802510
1881.419898	62.948399	62.807514
1881.095324	73.899492	62.812519
1880.068367	69.341503	62.817524
1879.100044	73.658361	62.822529
1878.558479	72.986016	62.827534
1878.417336	66.147564	62.832538
1876.901253	85.200630	62.837543
1876.519229	68.086027	62.842548
1875.681098	89.250138	62.847553
1875.172809	71.162141	62.852558
1875.217776	71.088927	62.857562
1874.126546	67.525120	62.862567
1873.565208	58.880049	62.867572
1872.647387	72.623373	62.872577
1872.290243	76.324405	62.877582
1871.019223	68.910012	62.882586
1869.897410	73.773190	62.887591
1869.674043	73.920767	62.892596
1869.488522	78.330956	62.897601
1868.883179	69.806402	62.902606
1868.533891	75.308564	62.907610
1867.486705	69.181640	62.912615
1866.789669	71.413368	62.917620
1866.085557	72.548709	62.922625
1865.262862	78.507640	62.927630
1865.075296	59.268077	62.932634
1863.301191	72.485064	62.937639
1862.873019	66.857501	62.942644
1862.411721	70.978751	62.947649
1862.187874	77.471779	62.952654
1861.849865	73.998113	62.957658
1861.340783	81.455752	62.962663
1860.575080	64.572379	62.967668
1859.637019	72.396153	62.972673
1859.003754	74.508954	62.977678
1858.153544	75.552381	62.982682
1856.985050	75.387991	62.987687
1856.963716	76.831227	62.992692
1856.301410	81.274541	62.997697
1856.380727	68.347435	63.002702
1855.177936	79.105248	63.007706
1853.919235	76.282365	63.012711
1853.612837	74.719593	63.017716
1852.302920	70.498266	63.022721
1851.643292	78.385066	63.027726
1851.016150	71.273711	63.032730
1850.432685	77.008589	63.037735
1850.359246	62.205600	63.042740
1850.159329	71.667247	63.047745
1849.433467	69.795779	63.052750
1848.329147	68.944721	63.057754
1847.557046	70.574965	63.062759
1847.394292	66.042196	63.067764
1846.254803	75.572606	63.072769
1845.358915	70.657945	63.077774
1844.896855	71.042109	63.082778
1844.168777	72.570752	63.087783
1844.083066	63.922705	63.092788
1842.510920	72.660833	63.097793
1841.889552	73.661623	63.102798
1841.306396	69.652900	63.107802
1840.469217	76.000471	63.112807
1840.405181	63.133979	63.117812
1840.107622	78.710510	63.122817
1839.206700	69.040774	63.127822
1838.526940	71.436915	63.132826
1837.696531	75.638853	63.137831
1837.329428	67.188442	63.142836
1836.084089	74.223690	63.147841
1835.352522	69.908964	63.152846
1834.755638	62.477439	63.157850
1834.379396	74.108488	63.162855
1834.257361	62.028609	63.167860
1833.087835	59.994214	63.172865
1832.087264	65.757474	63.177870
1832.034504	60.697911	63.182874
1831.233720	66.106188	63.187879
1830.916897	61.752420	63.192884
1829.495641	63.556702	63.197889
1829.052329	58.008822	63.202894
1828.575013	64.792815	63.207898
1827.429882	74.391932	63.212903
1826.937127	63.518887	63.217908
1826.013143	65.901771	63.222913
1825.405124	61.095948	63.227918
1825.188492	68.563916	63.232922
1824.338833	61.615634	63.237927
1824.391923	63.520114	63.242932
1823.304225	59.553667	63.247937
1822.609022	65.560165	63.252942
1822.301042	49.080367	63.257946
1820.808038	64.550247	63.262951
1820.290634	53.115026	63.267956
1819.359898	72.015230	63.272961
1818.895501	67.361635	63.277966
1818.986420	55.489213	63.282970
1818.430986	66.850680	63.287975
1817.664219	61.888723	63.292980
1817.058494	58.016052	63.297985
1815.805845	58.358607	63.302990
1815.081959	50.650806	63.307994
1814.000494	67.208043	63.312999
1813.612247	56.056652	63.318004
1813.122662	61.603166	63.323009
1813.140636	65.700355	63.328014
1812.269053	55.382615	63.333018
1810.875688	56.266310	63.338023
1810.741187	52.531695	63.343028
1810.018688	58.936747	63.348033
1809.440467	68.799068	63.353038
1808.792621	58.513606	63.358042
1807.583226	76.776854	63.363047
1807.243197	60.393596	63.368052
1806.863691	75.212040	63.373057
1806.041225	60.818145	63.378062
1805.226356	68.508835	63.383066
1804.738101	64.620666	63.388071
1803.981898	71.135150	63.393076
1803.516110	65.556151	63.398081
1802.164645	78.966249	63.403086
1802.289105	61.664025	63.408090
1801.043977	76.309278	63.413095
1800.733087	60.582108	63.418100
1800.340494	61.669576	63.423105
1799.177295	72.244504	63.428110
1798.789845	61.192330	63.433114
1797.808995	72.894157	63.438119
1797.711534	60.949149	63.443124
1796.876716	67.840376	63.448129
1795.914781	77.646947	63.453134
1795.465743	69.119673	63.458138
1794.646214	78.365915	63.463143
1794.051563	69.059132	63.468148
1792.987146	70.600198	63.473153
1792.221541	61.602828	63.478158
1791.716252	69.909805	63.483162
1791.198123	58.492050	63.488167
1791.148867	59.964948	63.493172
1790.719993	55.737786	63.498177
1789.750750	70.460648	63.503182
1788.967684	56.227659	63.508186
1788.256879	60.629800	63.513191
1787.540164	63.418155	63.518196
1786.400929	60.232580	63.523201
1786.037255	62.963296	63.528206
1785.729800	52.655331	63.533210
1784.928585	65.333101	63.538215
1784.421755	46.163200	63.543220
1783.771264	63.071451	63.548225
1782.920288	61.609361	63.553230
1782.721458	57.747774	63.558234
1780.818212	68.571107	63.563239
1780.399918	58.310700	63.568244
1779.893340	60.550048	63.573249
1779.198178	59.976229	63.578254
1779.477971	56.043368	63.583258
1778.863162	61.209245	63.588263
1778.033315	52.652577	63.593268
1777.043671	63.592588	63.598273
1776.322458	58.979788	63.603278
1775.617069	55.894049	63.608282
1774.598144	57.123559	63.613287
1774.169678	56.707653	63.618292
1773.354017	64.010562	63.623297
1773.384994	60.213402	63.628302
1772.798882	54.275071	63.633306
1771.517360	72.843077	63.638311
1771.112450	49.807826	63.643316
1770.682280	62.562284	63.648321
1769.134944	63.549296	63.653326
1768.620203	56.454816	63.658330
1767.721735	65.527520	63.663335
1767.390614	68.754518	63.668340
1767.166271	62.542702	63.673345
1766.752848	67.351764	63.678350
1766.410590	61.338438	63.683354
1765.091328	66.288200	63.688359
1764.306079	64.900830	63.693364
1763.720662	67.915911	63.698369
1762.451972	65.920949	63.703374
1761.879503	61.144189	63.708378
1761.290105	72.693977	63.713383
1761.153923	65.984057	63.718388
1761.264423	56.726151	63.723393
1760.179897	66.727225	63.728398
1759.525536	67.903577	63.733402
1758.698650	67.470525	63.738407
1757.607907	63.914579	63.743412
1756.704431	64.515509	63.748417
1756.010824	71.086292	63.753422
1756.001478	63.714441	63.758426
1755.445243	63.604244	63.763431
1755.028267	64.520557	63.768436
1753.922788	60.329895	63.773441
1752.946864	60.064010	63.778446
1752.679518	54.380976	63.783450
1751.702195	61.843596	63.788455
1750.887099	57.296175	63.793460
1750.306376	58.878706	63.798465
1749.878138	64.447024	63.803470
1749.919730	52.642366	63.808474
1748.176662	60.810043	63.813479
1747.486857	51.734430	63.818484
1747.367220	62.878463	63.823489
1746.276688	65.975343	63.828494
1746.253876	57.247941	63.833498
1744.825459	65.600606	63.838503
1744.257377	58.016310	63.843508
1743.749329	66.410456	63.848513
1743.268945	60.247192	63.853518
1742.954402	56.471793	63.858522
1742.107753	66.236408	63.863527
1741.206728	62.030626	63.868532
1740.720871	59.200178	63.873537
1740.141954	71.166175	63.878542
1739.461082	63.538292	63.883546
1738.310293	67.258151	63.888551
1737.703390	67.554956	63.893556
1737.367924	62.551336	63.898561
1736.961022	72.531532	63.903566
1736.021347	59.173375	63.908570
1735.028211	74.606488	63.913575
1734.487709	57.621189	63.918580
1734.255326	71.134259	63.923585
1733.231692	65.032043	63.928590
1732.345359	63.518818	63.933594
1731.714462	61.045705	63.938599
1731.269826	67.299419	63.943604
1731.177826	62.698660	63.948609
1730.297785	66.591554	63.953614
1729.195220	68.228585	63.958618
1728.496613	75.118699	63.963623
1728.307337	68.712091	63.968628
1727.829248	65.990792	63.973633
1726.336696	71.715536	63.978638
1726.297195	62.172384	63.983642
1725.641201	67.926682	63.988647
1724.924291	60.925819	63.993652
1723.769494	62.818718	63.998657
1723.077905	71.549511	64.003662
1722.581726	64.560897	64.008666
1722.353709	70.244070	64.013671
1721.946364	66.663175	64.018676
1720.762646	59.575613	64.023681
1720.042212	74.735194	64.028686
1719.533642	61.672833	64.033690
1718.875136	70.037266	64.038695
1718.057177	59.550207	64.043700
1717.026280	74.577756	64.048705
1716.461069	79.598584	64.053710
1716.470836	62.544812	64.058714
1715.745248	68.762730	64.063719
1715.082315	63.971966	64.068724
1714.280289	56.104730	64.073729
1713.350054	79.024341	64.078734
1713.219131	62.555862	64.083738
1711.892153	79.951608	64.088743
1711.269750	58.530946	64.093748
1710.765499	68.187573	64.098753
1710.131737	75.174619	64.103758
1709.969662	71.102205	64.108762
1708.895008	67.985252	64.113767
1708.026544	65.116235	64.118772
1707.877674	62.795216	64.123777
1707.019404	66.866000	64.128782
1706.322405	61.541358	64.133786
1704.900236	66.012351	64.138791
1704.207158	69.680026	64.143796
1704.142303	77.429806	64.148801
1703.484833	69.416611	64.153806
1703.481641	64.538409	64.158810
1702.435016	71.237809	64.163815
1701.399919	66.696962	64.168820
1700.755025	63.888628	64.173825
1700.432358	72.568713	64.178830
1700.236352	77.038916	64.183834
1699.226543	69.012302	64.188839
1698.725167	63.191411	64.193844
1698.114753	68.446489	64.198849
1696.680590	68.841584	64.203854
1696.036399	62.513546	64.208858
1695.313480	72.928697	64.213863
1695.069775	66.399859	64.218868
1694.670770	61.489914	64.223873
1693.248029	66.385185	64.228878
1692.647047	66.706289	64.233882
1692.201819	58.506435	64.238887
1692.051117	68.310325	64.243892
1691.584776	62.892283	64.248897
1690.505521	66.339038	64.253902
1689.928323	72.281092	64.258906
1688.977926	66.949395	64.263911
1688.701535	73.917526	64.268916
1687.710917	62.420316	64.273921
1686.690908	61.907581	64.278926
1686.839737	64.717746	64.283930
1686.091098	62.591338	64.288935
1685.097773	70.140098	64.293940
1684.003878	62.284539	64.298945
1683.556967	57.298633	64.303950
1683.752617	60.008324	64.308954
1682.442032	63.550169	64.313959
1681.429793	60.022789	64.318964
1681.278334	59.181295	64.323969
1680.484815	65.441546	64.328974
1680.315722	60.870383	64.333978
1679.002230	62.030029	64.338983
1678.279062	66.117207	64.343988
1677.758669	68.716719	64.348993
1677.093759	60.357806	64.353998
1677.048320	69.157851	64.359002
1675.468108	67.456831	64.364007
1675.147505	65.016443	64.369012
1674.056112	57.838552	64.374017
1673.911434	67.242533	64.379022
1673.644746	63.902645	64.384026
1672.811678	63.040116	64.389031
1672.087409	54.551872	64.394036
1671.307185	58.145088	64.399041
1670.665171	64.854339	64.404046
1669.567943	63.464518	64.409050
1668.564538	64.092389	64.414055
1668.193128	69.061939	64.419060
1667.986071	63.003503	64.424065
1667.213505	64.350032	64.429070
1667.451143	53.118187	64.434074
1666.302494	71.266165	64.439079
1665.589184	61.759091	64.444084
1665.235213	68.280672	64.449089
1664.053056	62.041252	64.454094
1663.651774	66.930394	64.459098
1662.621533	73.486863	64.464103
1661.486773	64.437801	64.469108
1661.097154	59.122693	64.474113
1660.297212	62.860965	64.479118
1659.730216	56.640522	64.484122
1659.146432	63.431983	64.489127
1658.900729	66.863031	64.494132
1658.531184	64.696912	64.499137
1657.350264	69.716207	64.504142
1656.856733	57.829410	64.509146
1656.421553	62.541019	64.514151
1655.394810	63.256177	64.519156
1654.699570	57.521286	64.524161
1653.951711	66.899661	64.529166
1653.739634	67.859132	64.534170
1652.815762	63.097222	64.539175
1652.031074	64.918744	64.544180
1651.316845	65.614222	64.549185
1650.442414	76.055026	64.554190
1650.464461	63.384616	64.559194
1649.497245	72.140283	64.564199
1648.782312	68.329155	64.569204
1648.433710	63.051685	64.574209
1647.599566	65.910766	64.579214
1646.622141	70.902471	64.584218
1645.472089	65.960460	64.589223
1645.168968	67.580913	64.594228
1644.640228	66.860852	64.599233
1644.195658	72.808652	64.604238
1644.171825	63.176292	64.609242
1643.009365	77.065754	64.614247
1642.588249	64.259171	64.619252
1641.952216	68.316748	64.624257
1640.517982	71.554997	64.629262
1640.176049	69.871749	64.634266
1639.499399	65.904740	64.639271
1638.981882	71.819976	64.644276
1638.335969	64.158191	64.649281
1637.225519	81.322456	64.654286
1637.047817	59.433812	64.659290
1636.152470	78.093474	64.664295
1635.725286	65.194820	64.669300
1635.225128	61.601880	64.674305
1633.927079	65.472901	64.679310
1633.857352	60.151134	64.684314
1633.149854	65.697598	64.689319
1632.141566	64.180129	64.694324
1631.250765	57.361459	64.699329
1630.631204	70.705805	64.704334
1630.338571	58.970019	64.709338
1629.740448	63.444178	64.714343
1629.224782	68.472915	64.719348
1628.520613	61.556791	64.724353
1627.418107	64.315013	64.729358
1627.218652	67.953171	64.734362
1626.768274	61.042460	64.739367
1625.541196	65.588152	64.744372
1624.964788	57.071704	64.749377
1624.103053	62.811397	64.754382
1623.916347	57.077727	64.759386
1622.800091	68.922524	64.764391
1622.178125	67.953939	64.769396
1621.467660	73.735835	64.774401
1620.888689	64.158552	64.779406
1620.764683	67.789455	64.784410
1619.898724	74.999475	64.789415
1619.144742	66.602692	64.794420
1618.790174	64.888341	64.799425
1617.748756	74.590894	64.804430
1616.894853	61.698541	64.809434
1616.055518	73.948761	64.814439
1615.943391	63.936210	64.819444
1615.629558	64.490822	64.824449
1614.366747	66.180164	64.829454
1613.204854	60.948330	64.834458
1612.602101	66.337816	64.839463
1612.207249	61.706337	64.844468
1611.976650	62.873746	64.849473
1611.304762	71.156749	64.854478
1611.327682	56.537190	64.859482
1610.134850	67.164191	64.864487
1609.376251	53.422541	64.869492
1608.287036	59.874855	64.874497
1607.241525	65.337835	64.879502
1606.977938	62.462643	64.884506
1606.431249	58.722570	64.889511
1606.227829	55.990777	64.894516
1605.738069	64.134461	64.899521
1604.262139	68.377515	64.904526
1604.012282	63.962686	64.909530
1603.396129	56.176347	64.914535
1602.671393	68.818346	64.919540
1601.677910	62.593137	64.924545
1600.969376	60.017281	64.929550
1600.663064	72.209629	64.934554
1600.110463	65.663652	64.939559
1599.189047	62.066687	64.944564
1598.546947	60.087375	64.949569
1597.493647	72.494587	64.954574
1597.248996	69.526504	64.959578
1596.820458	57.619940	64.964583
1595.975651	62.194793	64.969588
1595.292783	55.555983	64.974593
1594.628633	65.897156	64.979598
1594.417866	52.585693	64.984602
1593.584661	70.035476	64.989607
1592.454217	57.784710	64.994612
1592.140037	60.808767	64.999617
1591.392780	67.295068	65.004622
1590.866243	57.955462	65.009626
1589.717912	62.282086	65.014631
1589.220662	54.535206	65.019636
1588.843782	63.763194	65.024641
1588.154814	66.419463	65.029646
1587.434494	57.585285	65.034650
1586.186421	66.518045	65.039655
1585.874424	61.288386	65.044660
1585.740270	64.193961	65.049665
1585.127533	62.533247	65.054670
1584.416292	64.187009	65.059674
1583.503649	58.012041	65.064679
1582.532153	66.498757	65.069684
1581.429060	64.485463	65.074689
1580.963595	63.892550	65.079694
1580.709096	49.187776	65.084698
1580.122697	65.406226	65.089703
1579.751930	63.546228	65.094708
1579.358830	56.402515	65.099713
1578.298719	59.474125	65.104718
1577.638768	72.269834	65.109722
1577.037870	60.797492	65.114727
1575.913498	68.736094	65.119732
1575.115320	56.255938	65.124737
1574.691972	68.260305	65.129742
1574.219476	60.968364	65.134746
1574.047656	57.003168	65.139751
1572.808237	66.664651	65.144756
1572.324314	55.583718	65.149761
1571.576962	59.267927	65.154766
1571.048714	58.845833	65.159770
1569.922612	64.512433	65.164775
1569.085083	66.377065	65.169780
1568.858625	57.032365	65.174785
1568.079974	68.427743	65.179790
1567.975103	61.143623	65.184794
1567.067061	63.063611	65.189799
1565.984598	69.718289	65.194804
1565.789551	57.495529	65.199809
1565.210437	68.357758	65.204814
1563.814396	61.488508	65.209818
1563.257113	58.533836	65.214823
1562.801015	65.573095	65.219828
1562.625189	67.698431	65.224833
1561.853060	72.990267	65.229838
1561.177586	57.264330	65.234842
1560.409820	64.651137	65.239847
1559.705504	72.146133	65.244852
1559.191911	59.521422	65.249857
1557.735898	64.756343	65.254862
1557.274738	60.245791	65.259866
1556.762211	56.574416	65.264871
1556.171952	70.100183	65.269876
1555.748253	57.886949	65.274881
1555.398708	67.432279	65.279886
1554.495545	50.287074	65.284890
1553.611459	66.956505	65.289895
1553.202928	55.988172	65.294900
1552.514669	50.384666	65.299905
1551.497732	58.508040	65.304910
1550.944109	56.913634	65.309914
1550.515240	64.355400	65.314919
1549.817311	60.385494	65.319924
1549.206741	58.785944	65.324929
1548.451840	56.711034	65.329934
1547.887482	61.466833	65.334938
1547.271436	61.966974	65.339943
1546.168639	57.446418	65.344948
1545.487312	68.089935	65.349953
1545.159405	54.822324	65.354958
1544.687588	54.104278	65.359962
1543.585262	58.212308	65.364967
1543.021375	59.180379	65.369972
1542.624593	52.808353	65.374977
1541.729673	63.033242	65.379982
1541.769840	62.626488	65.384986
1540.577796	67.988202	65.389991
1539.801619	61.594458	65.394996
1539.163012	58.463489	65.400001
1537.702755	67.341677	65.405006
1537.782955	57.803184	65.410010
1537.218865	62.216760	65.415015
1536.308446	57.489031	65.420020
1536.245993	57.984786	65.425025
1535.299389	58.428650	65.430030
1534.172089	48.963763	65.435034
1534.102590	60.137655	65.440039
1533.425761	59.709217	65.445044
1533.325852	54.881087	65.450049
1531.693991	59.405984	65.455054
1531.010590	60.260590	65.460058
1530.550983	54.773714	65.465063
1529.766051	59.867324	65.470068
1528.786186	51.180064	65.475073
1528.155667	67.530102	65.480078
1527.808933	56.779026	65.485082
1527.418194	63.044694	65.490087
1526.852820	57.672390	65.495092
1526.666730	52.449546	65.500097
1525.802889	51.123624	65.505102
1524.988005	64.394936	65.510106
1523.836092	60.069842	65.515111
1522.672600	63.372357	65.520116
1522.438178	51.934844	65.525121
1522.239338	61.074622	65.530126
1521.594522	49.472099	65.535130
1520.552685	69.593152	65.540135
1519.801623	63.179656	65.545140
1519.684755	56.750539	65.550145
1519.081172	66.489194	65.555150
1518.051819	53.446588	65.560154
1517.323090	52.941250	65.565159
1516.666063	58.634250	65.570164
1516.601021	55.618718	65.575169
1514.990173	60.258551	65.580174
1514.530777	66.946696	65.585178
1513.699911	60.462309	65.590183
1513.271697	57.772555	65.595188
1513.270062	59.241039	65.600193
1512.107307	59.077470	65.605198
1511.246556	58.791799	65.610202
1510.405769	63.645144	65.615207
1510.058526	60.562496	65.620212
1509.968154	56.827204	65.625217
1508.504314	61.666020	65.630222
1507.929385	65.923638	65.635226
1507.614921	64.079935	65.640231
1506.887216	65.209657	65.645236
1506.015912	54.273876	65.650241
1505.089172	56.586344	65.655246
1504.536103	58.776358	65.660250
1504.590182	60.239143	65.665255
1504.026987	61.017887	65.670260
1502.791017	56.461747	65.675265
1501.903090	60.822715	65.680270
1501.751912	65.438753	65.685274
1501.077726	61.865615	65.690279
1499.720494	63.577898	65.695284
1499.396776	62.129887	65.700289
1498.910269	64.665699	65.705294
1498.688789	66.575954	65.710298
1497.759103	62.874692	65.715303
1496.485685	57.425686	65.720308
1496.039938	61.522435	65.725313
1495.219193	65.316094	65.730318
1495.092564	61.297995	65.735322
1494.737314	56.130418	65.740327
1493.511139	56.719643	65.745332
1493.195310	51.408616	65.750337
1492.308344	68.058016	65.755342
1491.425154	52.308357	65.760346
1490.568001	65.384553	65.765351
1490.023448	62.826825	65.770356
1489.739053	60.789122	65.775361
1489.184422	64.818024	65.780366
1488.341868	59.516584	65.785370
1487.861914	66.457145	65.790375
1486.925219	57.349899	65.795380
1486.531605	52.008659	65.800385
1485.629819	66.353448	65.805390
1485.041786	48.409188	65.810394
1484.307493	61.562047	65.815399
1483.711030	63.225978	65.820404
1483.092804	60.634230	65.825409
1481.979589	62.120097	65.830414
1481.663729	56.276091	65.835418
1481.280195	58.024450	65.840423
1480.694949	57.605125	65.845428
1479.805119	52.030522	65.850433
1478.935534	59.848242	65.855438
1478.391419	51.112258	65.860442
1478.118047	62.815260	65.865447
1477.067716	57.198356	65.870452
1476.695556	54.764616	65.875457
1476.013993	55.106460	65.880462
1475.023411	55.166270	65.885466
1474.284489	58.037074	65.890471
1473.217493	60.961592	65.895476
1472.984020	57.524997	65.900481
1472.673863	53.619643	65.905486
1471.979392	53.692317	65.910490
1470.953074	59.541779	65.915495
1469.930606	57.088390	65.920500
1469.946687	52.191375	65.925505
1469.412598	59.963665	65.930510
1468.720149	56.377672	65.935514
1467.577685	56.439545	65.940519
1467.188218	57.928665	65.945524
1467.055640	53.654485	65.950529
1465.710979	59.161899	65.955534
1464.898132	61.188212	65.960538
1464.387686	55.502861	65.965543
1463.767355	61.196348	65.970548
1463.968234	56.755639	65.975553
1462.376534	60.605600	65.980558
1461.575047	47.930495	65.985562
1461.178027	64.612414	65.990567
1460.750789	61.931975	65.995572
1460.112841	49.047963	66.000577
1459.069088	62.212162	66.005582
1458.735304	58.788356	66.010586
1458.216216	55.064434	66.015591
1456.617353	62.420926	66.020596
1456.119834	47.743770	66.025601
1455.694477	63.332687	66.030606
1455.258424	56.041296	66.035610
1454.928682	57.052594	66.040615
1454.235302	59.950857	66.045620
1453.549355	56.554636	66.050625
1452.744087	58.371600	66.055630
1452.232553	55.024929	66.060634
1451.105714	53.953708	66.065639
1449.894767	64.313996	66.070644
1449.821898	54.594845	66.075649
1449.284658	49.265401	66.080654
1449.154621	52.957182	66.085658
1448.493633	46.524672	66.090663
1447.212337	60.522945	66.095668
1447.079488	51.106628	66.100673
1446.186893	55.012637	66.105678
1445.022097	50.727477	66.110682
1444.213866	51.526255	66.115687
1443.967757	60.484317	66.120692
1443.697715	57.316876	66.125697
1442.850138	56.324271	66.130702
1442.157771	68.945381	66.135706
1441.432165	60.589889	66.140711
1440.604189	59.076956	66.145716
1440.469292	58.977131	66.150721
1439.293264	50.070368	66.155726
1438.280682	58.428039	66.160730
1438.156353	55.967532	66.165735
1437.597067	59.915183	66.170740
1436.911490	50.501563	66.175745
1435.590224	61.945353	66.180750
1435.115808	53.944164	66.185754
1434.714029	50.031303	66.190759
1434.454501	62.597807	66.195764
1434.169758	43.271337	66.200769
1433.081371	53.638951	66.205774
1432.368093	53.971655	66.210778
1431.718417	51.613568	66.215783
1430.566000	55.431573	66.220788
1430.157919	50.543630	66.225793
1429.409138	53.204710	66.230798
1429.269714	55.018352	66.235802
1428.168202	49.351264	66.240807
1427.218387	55.775177	66.245812
1426.819358	52.074757	66.250817
1426.321393	62.430537	66.255822
1425.909099	54.018951	66.260826
1425.031650	49.450024	66.265831
1423.822638	64.045492	66.270836
1424.158068	54.769204	66.275841
1422.760242	55.857229	66.280846
1422.111217	60.645428	66.285850
1421.450443	51.604744	66.290855
1420.947985	52.670303	66.295860
1420.880008	52.312274	66.300865
1419.691634	55.541518	66.305870
1418.961867	56.770933	66.310874
1418.309727	58.241887	66.315879
1417.674693	64.191597	66.320884
1416.845131	58.474980	66.325889
1415.861877	66.681351	66.330894
1415.320381	53.115006	66.335898
1415.068775	51.871577	66.340903
1414.332235	58.438206	66.345908
1414.017444	55.552257	66.350913
1412.976892	60.047892	66.355918
1412.330835	53.584634	66.360922
1412.217010	58.194733	66.365927
1410.944903	55.052533	66.370932
1410.241148	49.812640	66.375937
1409.450338	55.534808	66.380942
1409.084934	55.545735	66.385946
1408.745103	55.264030	66.390951
1407.590862	60.272874	66.395956
1407.294023	46.956218	66.400961
1406.780614	62.831929	66.405966
1405.238190	59.376322	66.410970
1404.703691	49.536599	66.415975
1403.918504	52.988755	66.420980
1403.442698	52.222487	66.425985
1403.334579	56.878985	66.430990
1402.765258	54.538094	66.435994
1402.098042	56.639043	66.440999
1401.164933	58.487380	66.446004
1400.576819	56.725035	66.451009
1400.142486	53.914857	66.456014
1399.094362	60.737586	66.461018
1398.431932	51.894282	66.466023
1397.992236	47.296785	66.471028
1397.209360	44.204559	66.476033
1396.016674	58.616095	66.481038
1395.813370	53.698763	66.486042
1395.523998	50.815085	66.491047
1394.655810	55.452053	66.496052
1394.010864	53.017534	66.501057
1393.105009	63.266272	66.506062
1392.486511	52.399166	66.511066
1392.187585	51.596901	66.516071
1391.170828	44.473524	66.521076
1390.364888	47.236735	66.526081
1389.726930	49.749330	66.531086
1389.416360	53.577034	66.536090
1388.724500	37.923182	66.541095
1387.768615	47.129666	66.546100
1387.104615	53.769920	66.551105
1386.549809	43.800978	66.556110
1386.483792	46.079166	66.561114
1385.660772	51.199362	66.566119
1384.383212	52.969999	66.571124
1384.306716	51.284022	66.576129
1383.273398	45.776420	66.581134
1382.020934	59.164613	66.586138
1381.893868	37.985509	66.591143
1381.053213	53.123215	66.596148
1380.801762	48.018008	66.601153
1380.278975	47.243444	66.606158
1379.296244	55.668922	66.611162
1378.658871	48.690237	66.616167
1378.227222	49.979503	66.621172
1377.325300	49.463891	66.626177
1376.505618	54.569368	66.631182
1375.791019	53.005321	66.636186
1375.460007	45.066510	66.641191
1374.420964	55.774788	66.646196
1374.327136	46.254517	66.651201
1373.278611	47.157740	66.656206
1372.507202	61.007183	66.661210
1372.284749	42.993829	66.666215
1371.492100	59.890008	66.671220
1370.900019	46.968781	66.676225
1369.846184	64.018440	66.681230
1369.219610	49.424903	66.686234
1369.122579	44.142195	66.691239
1367.816112	53.979976	66.696244
1367.179405	47.933121	66.701249
1366.461028	57.746804	66.706254
1365.958318	49.575101	66.711258
1365.931755	49.754511	66.716263
1364.885476	54.791938	66.721268
1363.977493	44.371391	66.726273
1363.503866	49.811347	66.731278
1363.010101	52.904969	66.736282
1362.399850	40.287822	66.741287
1361.356578	43.290607	66.746292
1360.866974	45.670820	66.751297
1360.243605	57.284380	66.756302
1359.684143	52.675968	66.761306
1358.727689	47.547222	66.766311
1357.762970	58.672602	66.771316
1357.493836	43.845645	66.776321
1357.090559	56.807133	66.781326
1356.359405	58.777916	66.786330
1355.616111	48.771137	66.791335
1354.567423	57.576096	66.796340
1354.239926	48.730027	66.801345
1354.044142	53.594414	66.806350
1352.603972	56.054778	66.811354
1351.851041	51.379358	66.816359
1351.368390	60.635206	66.821364
1351.235240	55.541155	66.826369
1350.574730	59.637370	66.831374
1349.570888	52.010511	66.836378
1349.443085	44.397352	66.841383
1348.348082	62.071691	66.846388
1347.332654	54.044571	66.851393
1346.577631	50.722440	66.856398
1345.916901	56.425522	66.861402
1345.799237	45.235984	66.866407
1345.370535	56.474841	66.871412
1344.557402	55.662866	66.876417
1343.813423	54.228072	66.881422
1343.258494	52.771109	66.886426
1342.640625	49.971197	66.891431
1341.190660	60.632855	66.896436
1340.983286	46.510405	66.901441
1340.519199	58.691550	66.906446
1339.469097	58.033936	66.911450
1338.835197	48.553794	66.916455
1338.137235	58.031517	66.921460
1337.667330	67.264845	66.926465
1337.212710	52.721249	66.931470
1336.389129	57.893586	66.936474
1335.831512	52.494875	66.941479
1334.917289	61.119202	66.946484
1334.440924	53.499953	66.951489
1334.110083	57.233120	66.956494
1333.307383	58.072051	66.961498
1332.500972	47.802517	66.966503
1331.888787	65.598795	66.971508
1331.177526	48.169329	66.976513
1330.194363	60.253232	66.981518
1329.656899	57.211894	66.986522
1329.055539	52.425657	66.991527
1328.220709	60.460229	66.996532
1327.955351	56.118867	67.001537
1327.074430	55.275099	67.006542
1326.259397	58.744636	67.011546
1326.103333	61.753042	67.016551
1325.554889	53.057214	67.021556
1324.612868	59.891483	67.026561
1323.865790	57.118424	67.031566
1323.090486	61.166666	67.036570
1322.850778	59.506639	67.041575
1321.446087	58.290424	67.046580
1320.689926	63.106714	67.051585
1320.346888	56.857072	67.056590
1319.852467	53.119802	67.061594
1319.605995	59.857688	67.066599
1318.565837	52.432149	67.071604
1318.073417	53.109798	67.076609
1317.454453	61.438045	67.081614
1316.877182	54.325250	67.086618
1316.077469	58.225994	67.091623
1314.797684	53.804646	67.096628
1314.634680	56.811001	67.101633
1314.223163	59.511530	67.106638
1313.448392	60.973622	67.111642
1312.627230	46.581348	67.116647
1311.625337	58.732884	67.121652
1311.498381	45.553241	67.126657
1310.779253	53.220931	67.131662
1309.272550	57.387032	67.136666
1308.915245	49.247419	67.141671
1308.439358	55.296416	67.146676
1308.272201	45.393595	67.151681
1307.874988	50.619571	67.156686
1307.062467	53.554155	67.161690
1306.120977	49.239871	67.166695
1305.511369	67.642838	67.171700
1304.494163	50.394480	67.176705
1303.676376	64.437380	67.181710
1303.110145	59.896286	67.186714
1302.955007	57.202580	67.191719
1302.462384	51.456095	67.196724
1301.714917	52.552745	67.201729
1300.409823	61.890471	67.206734
1299.685147	58.219772	67.211738
1299.558084	56.995977	67.216743
1298.562504	60.344424	67.221748
1298.093105	51.659692	67.226753
1297.609271	47.496567	67.231758
1296.538850	53.950731	67.236762
1296.481620	51.038044	67.241767
1295.308732	54.110345	67.246772
1294.867100	35.597310	67.251777
1294.176408	51.127479	67.256782
1293.554460	48.645180	67.261786
1292.818501	46.631993	67.266791
1292.010736	54.887760	67.271796
1291.566114	55.174636	67.276801
1291.251743	41.543852	67.281806
1290.193719	57.176582	67.286810
1289.821042	51.333763	67.291815
1288.890095	51.053020	67.296820
1288.072515	53.146365	67.301825
1287.204875	59.831632	67.306830
1286.386498	53.233396	67.311834
1286.199777	60.620914	67.316839
1285.818897	65.363355	67.321844
1285.511546	54.131444	67.326849
1284.530451	52.417416	67.331854
1283.535596	60.409636	67.336858
1282.993577	51.533038	67.341863
1281.624438	58.411574	67.346868
1281.160534	53.882603	67.351873
1280.504394	49.385773	67.356878
1280.284755	62.046848	67.361882
1279.937192	47.317530	67.366887
1279.227815	62.145822	67.371892
1278.431422	52.672612	67.376897
1277.683576	55.160128	67.381902
1277.408705	49.891512	67.386906
1276.197459	54.321297	67.391911
1275.226574	62.644006	67.396916
1275.056411	49.923798	67.401921
1274.656142	50.630957	67.406926
1273.240284	54.066733	67.411930
1272.682750	55.748173	67.416935
1272.329041	57.176443	67.421940
1271.890727	49.860230	67.426945
1271.411109	52.461210	67.431950
1270.422606	57.167804	67.436954
1269.778312	53.388146	67.441959
1269.162715	53.222841	67.446964
1268.225795	55.388781	67.451969
1267.382850	55.206011	67.456974
1266.562991	54.130217	67.461978
1266.547515	48.692633	67.466983
1265.935712	72.540886	67.471988
1265.197077	60.555998	67.476993
1264.412187	54.223667	67.481998
1263.509964	47.236671	67.487002
1263.305860	53.127348	67.492007
1262.542836	55.812813	67.497012
1261.423886	48.229531	67.502017
1261.012026	43.633947	67.507022
1260.382453	52.933659	67.512026
1260.309263	52.540195	67.517031
1259.066499	62.823611	67.522036
1258.381374	53.458867	67.527041
1258.039540	53.677368	67.532046
1257.534179	51.367343	67.537050
1256.203578	43.604840	67.542055
1255.509360	57.333220	67.547060
1254.970254	54.744723	67.552065
1254.638544	44.593701	67.557070
1253.754452	49.882906	67.562074
1252.925475	49.735765	67.567079
1252.055924	58.411354	67.572084
1251.598384	41.294810	67.577089
1251.466451	54.331418	67.582094
1250.988063	52.078602	67.587098
1250.475044	36.631330	67.592103
1249.274733	48.393399	67.597108
1249.045002	47.920753	67.602113
1248.270475	44.612796	67.607118
1247.390451	67.341537	67.612122
1246.803351	42.736538	67.617127
1245.471697	48.497434	67.622132
1244.925344	51.993654	67.627137
1244.605648	52.173946	67.632142
1243.505556	48.452580	67.637146
1243.542985	49.588436	67.642151
1242.634297	43.933357	67.647156
1241.703975	47.526898	67.652161
1241.247736	52.651886	67.657166
1240.654814	58.590199	67.662170
1240.828242	45.083701	67.667175
1239.161655	52.920981	67.672180
1238.664366	46.539778	67.677185
1238.038084	56.580100	67.682190
1236.957884	49.436921	67.687194
1236.173446	58.770726	67.692199
1235.696736	55.295573	67.697204
1235.308540	59.564542	67.702209
1234.946309	46.794466	67.707214
1234.400260	50.511400	67.712218
1233.257784	49.808598	67.717223
1232.679209	48.308116	67.722228
1232.256046	54.776069	67.727233
1231.555885	55.389002	67.732238
1230.385178	51.038662	67.737242
1230.076075	50.086657	67.742247
1229.571782	58.702593	67.747252
1228.723651	50.013453	67.752257
1227.816622	52.523140	67.757262
1227.003146	50.186426	67.762266
1226.742136	48.848325	67.767271
1226.423484	48.749348	67.772276
1225.986327	46.098919	67.777281
1224.455171	54.031361	67.782286
1224.091757	51.768153	67.787290
1223.880571	54.231845	67.792295
1222.589034	48.476810	67.797300
1221.652176	52.886639	67.802305
1221.503425	50.567221	67.807310
1220.583669	50.754631	67.812314
1220.612289	52.841162	67.817319
1219.674851	56.292349	67.822324
1218.523963	53.036364	67.827329
1218.355122	46.476788	67.832334
1217.615975	51.143745	67.837338
1217.157947	49.188881	67.842343
1216.040215	50.232476	67.847348
1215.252978	46.026160	67.852353
1215.037626	38.717087	67.857358
1214.310573	46.764501	67.862362
1213.316507	54.326128	67.867367
1212.728342	50.759901	67.872372
1212.281546	54.729124	67.877377
1211.963183	46.192280	67.882382
1210.982987	47.628722	67.887386
1210.324242	54.400631	67.892391
1209.493433	43.800737	67.897396
1208.869174	56.549799	67.902401
1208.362481	49.720690	67.907406
1207.336068	53.096148	67.912410
1206.892967	49.014871	67.917415
1206.319586	49.103052	67.922420
1205.843862	53.581474	67.927425
1205.183733	42.669028	67.932430
1204.178769	51.979559	67.937434
1204.006929	50.611512	67.942439
1202.749453	50.508876	67.947444
1202.159811	53.586232	67.952449
1201.677788	52.765802	67.957454
1201.180553	57.657632	67.962458
1201.026031	48.634289	67.967463
1199.225777	57.219787	67.972468
1198.777211	50.312055	67.977473
1198.641546	48.020518	67.982478
1197.940424	55.303766	67.987482
1196.882664	47.461641	67.992487
1196.334101	57.074893	67.997492
1195.792778	54.482032	68.002497
1195.192616	48.153468	68.007502
1193.950331	55.500699	68.012506
1193.418097	59.587587	68.017511
1192.935146	54.028815	68.022516
1192.521745	45.890268	68.027521
1191.776006	55.799790	68.032526
1190.927502	61.654184	68.037530
1190.473731	56.483412	68.042535
1189.943421	52.720342	68.047540
1189.490830	58.150671	68.052545
1188.570806	57.212250	68.057550
1187.564726	59.726666	68.062554
1187.229841	41.015350	68.067559
1186.643243	47.011005	68.072564
1186.010843	47.480717	68.077569
1184.970138	49.852413	68.082574
1184.153308	61.651296	68.087578
1184.042147	50.120144	68.092583
1182.806003	60.080853	68.097588
1182.273011	42.470158	68.102593
1181.781062	47.507796	68.107598
1180.894677	55.742977	68.112602
1181.056802	51.824061	68.117607
1180.067298	49.740850	68.122612
1178.760476	50.434508	68.127617
1178.623518	42.701409	68.132622
1177.817298	57.057857	68.137626
1177.760712	50.770576	68.142631
1176.549420	62.170171	68.147636
1175.651626	61.735971	68.152641
1175.489349	44.693914	68.157646
1174.516398	60.314722	68.162650
1173.700467	51.650444	68.167655
1172.685646	51.476118	68.172660
1172.278922	53.128863	68.177665
1172.077831	54.655869	68.182670
1171.394425	54.495065	68.187674
1171.452743	53.052572	68.192679
1170.206623	53.533164	68.197684
1169.364182	53.498573	68.202689
1168.372128	52.931142	68.207694
1167.490506	50.982157	68.212698
1167.565270	43.813021	68.217703
1166.799291	50.540492	68.222708
1166.199867	55.670917	68.227713
1165.414135	45.904343	68.232718
1164.621975	52.074614	68.237722
1164.142303	43.560282	68.242727
1163.332324	56.308925	68.247732
1162.271402	48.092026	68.252737
1161.810801	42.269529	68.257742
1161.204415	56.740846	68.262746
1160.852370	40.604140	68.267751
1160.570486	48.798373	68.272756
1159.304478	49.843498	68.277761
1158.602856	48.282183	68.282766
1157.672327	48.096035	68.287770
1157.534506	52.848711	68.292775
1156.733368	57.214900	68.297780
1155.976368	60.334653	68.302785
1155.521735	52.311473	68.307790
1155.029392	58.710018	68.312794
1154.572291	46.383961	68.317799
1153.632738	50.007383	68.322804
1152.813523	55.795629	68.327809
1152.604026	35.433908	68.332814
1151.007957	53.809259	68.337818
1150.771681	44.931385	68.342823
1150.214402	49.455898	68.347828
1149.415817	47.541021	68.352833
1148.433762	44.422214	68.357838
1147.261060	57.171782	68.362842
1147.267131	58.113938	68.367847
1146.775927	51.689215	68.372852
1146.604319	56.888789	68.377857
1146.100408	45.577799	68.382862
1145.253943	47.530708	68.387866
1144.329161	55.489746	68.392871
1143.642530	44.948947	68.397876
1142.503159	54.304527	68.402881
1142.229984	39.454624	68.407886
1141.234086	53.674094	68.412890
1140.964605	54.276897	68.417895
1140.562744	42.512888	68.422900
1139.154220	56.736491	68.427905
1138.798944	48.058884	68.432910
1138.149239	50.322681	68.437914
1138.170899	48.692064	68.442919
1137.319882	49.568700	68.447924
1136.176694	54.883381	68.452929
1135.845022	43.880874	68.457934
1134.697208	56.842519	68.462938
1134.120152	53.671916	68.467943
1133.434794	57.374758	68.472948
1132.662252	49.574028	68.477953
1132.734317	43.373520	68.482958
1131.457670	67.737490	68.487962
1130.782778	45.079751	68.492967
1130.195881	59.940613	68.497972
1129.519653	53.553206	68.502977
1129.408603	51.828585	68.507982
1128.237018	57.560926	68.512986
1127.732530	47.227691	68.517991
1126.946107	54.319527	68.522996
1126.423631	48.965746	68.528001
1126.144334	52.105713	68.533006
1124.947562	45.906755	68.538010
1124.637562	55.340151	68.543015
1123.900484	51.444414	68.548020
1122.886660	59.603694	68.553025
1122.147024	44.744409	68.558030
1121.272898	58.504574	68.563034
1121.276229	43.790455	68.568039
1121.147358	51.747476	68.573044
1119.715195	52.573057	68.578049
1119.394828	43.071511	68.583054
1118.352285	53.326281	68.588058
1117.391410	57.448244	68.593063
1116.440355	54.127409	68.598068
1116.166017	48.548093	68.603073
1115.603176	52.428559	68.608078
1115.106114	48.863637	68.613082
1114.977410	46.055365	68.618087
1114.398806	53.401137	68.623092
1113.199061	54.339556	68.628097
1112.598916	55.345022	68.633102
1111.620095	57.011506	68.638106
1111.286289	42.526046	68.643111
1110.662101	52.742658	68.648116
1110.074325	48.020554	68.653121
1109.293385	53.764877	68.658126
1108.260954	51.909285	68.663130
1107.953335	54.695810	68.668135
1107.333076	62.076597	68.673140
1106.369226	53.494218	68.678145
1105.680154	51.276523	68.683150
1104.920685	51.757005	68.688154
1104.890205	46.809071	68.693159
1104.185089	59.009643	68.698164
1103.076834	55.133531	68.703169
1102.448238	50.424229	68.708174
1101.828920	61.367008	68.713178
1101.448031	43.997065	68.718183
1101.015541	52.828658	68.723188
1099.762404	59.341917	68.728193
1099.320103	48.391704	68.733198
1098.704528	62.347281	68.738202
1098.236889	44.618996	68.743207
1097.308575	60.264257	68.748212
1096.419896	59.801829	68.753217
1096.356630	43.888850	68.758222
1094.926793	56.434922	68.763226
1094.035087	42.637420	68.768231
1093.776715	54.396364	68.773236
1093.260806	54.756111	68.778241
1093.018403	51.604823	68.783246
1092.404898	40.189869	68.788250
1091.721729	50.174603	68.793255
1091.223241	48.282969	68.798260
1090.050421	44.003997	68.803265
1089.190580	53.755077	68.808270
1088.207305	54.379969	68.813274
1087.878806	49.269717	68.818279
1087.552135	53.147313	68.823284
1086.741365	43.643362	68.828289
1085.946002	59.685345	68.833294
1085.223801	57.698417	68.838298
1084.425680	50.087844	68.843303
1084.465771	49.600678	68.848308
1083.577521	55.421999	68.853313
1083.063683	45.896045	68.858318
1082.318194	49.517004	68.863322
1081.874715	48.482320	68.868327
1080.640122	36.445543	68.873332
1079.884289	51.427885	68.878337
1079.375842	46.748361	68.883342
1078.910476	51.666675	68.888346
1078.268287	47.923008	68.893351
1077.494333	50.782140	68.898356
1076.600514	57.684503	68.903361
1076.706818	45.968978	68.908366
1075.064242	54.469547	68.913370
1074.406700	56.072323	68.918375
1074.368672	48.960553	68.923380
1073.418636	52.595131	68.928385
1073.272682	41.336030	68.933390
1072.127140	55.356985	68.938394
1071.507486	50.928528	68.943399
1071.022538	56.475975	68.948404
1070.211045	54.403913	68.953409
1069.626186	48.621702	68.958414
1068.595386	43.511217	68.963418
1068.176182	36.080066	68.968423
1067.844990	48.117079	68.973428
1066.932029	53.183863	68.978433
1066.182487	47.610767	68.983438
1065.283549	50.007263	68.988442
1065.254065	40.473651	68.993447
1064.837502	47.617041	68.998452
1063.726001	52.855750	69.003457
1062.966777	35.377290	69.008462
1062.129692	49.882154	69.013466
1061.428213	51.334235	69.018471
1060.564420	41.359364	69.023476
1059.943330	49.085618	69.028481
1059.881096	39.681789	69.033486
1059.136450	50.259748	69.038490
1058.893156	48.549862	69.043495
1057.780100	42.607268	69.048500
1056.872716	52.935166	69.053505
1056.584172	44.937632	69.058510
1055.246306	56.097217	69.063514
1054.678011	54.391727	69.068519
1054.284533	42.691061	69.073524
1053.461463	47.794007	69.078529
1053.245060	53.609377	69.083534
1052.677322	51.690921	69.088538
1051.959960	55.010964	69.093543
1051.244995	47.283105	69.098548
1050.311144	48.907766	69.103553
1049.500257	41.155748	69.108558
1048.842561	45.033969	69.113562
1048.094674	49.478442	69.118567
1048.079422	40.037179	69.123572
1047.207073	57.384442	69.128577
1046.501566	47.734457	69.133582
1045.361973	51.224167	69.138586
1045.301340	41.261874	69.143591
1045.313318	45.620154	69.148596
1043.733493	57.967771	69.153601
1043.350624	35.809231	69.158606
1042.815944	58.095128	69.163610
1041.823963	44.580093	69.168615
1041.046919	52.433658	69.173620
1040.176659	46.887661	69.178625
1039.985367	48.089858	69.183630
1039.219991	55.599390	69.188634
1038.219750	50.310600	69.193639
1037.592010	44.141006	69.198644
1037.080005	54.371319	69.203649
1036.577901	47.748098	69.208654
1036.140108	42.655246	69.213658
1035.056460	51.199373	69.218663
1034.218593	51.063179	69.223668
1034.032091	49.968700	69.228673
1033.760216	44.622383	69.233678
1032.637803	51.933263	69.238682
1031.757478	45.018575	69.243687
1031.352727	49.263391	69.248692
1030.836959	41.108059	69.253697
1030.085006	42.583946	69.258702
1028.704706	49.775013	69.263706
1028.120528	50.035254	69.268711
1028.021898	50.650309	69.273716
1027.346556	39.363482	69.278721
1026.876939	42.948449	69.283726
1025.773200	44.316310	69.288730
1025.600532	47.636428	69.293735
1025.122384	42.509000	69.298740
1023.862402	53.025459	69.303745
1023.379428	40.375578	69.308750
1023.117617	43.935369	69.313754
1022.101433	40.716396	69.318759
1021.392150	51.213047	69.323764
1020.956273	47.619490	69.328769
1020.336976	49.189387	69.333774
1018.573295	44.914573	69.338778
1017.807038	52.703353	69.343783
1018.118921	43.003477	69.348788
1017.244478	54.532446	69.353793
1017.258816	46.652303	69.358798
1016.483346	44.290694	69.363802
1015.397217	46.934594	69.368807
1014.702903	44.698839	69.373812
1014.094311	48.644945	69.378817
1012.990737	51.775721	69.383822
1012.097260	50.757453	69.388826
1011.598281	52.527394	69.393831
1011.647491	46.849314	69.398836
1010.766774	48.776177	69.403841
1010.539752	50.373547	69.408846
1009.364056	43.464864	69.413850
1008.986803	52.528936	69.418855
1008.531166	58.529019	69.423860
1007.574647	44.230967	69.428865
1006.724985	51.709761	69.433870
1005.855921	53.343052	69.438874
1005.616154	46.433688	69.443879
1005.338791	43.306898	69.448884
1003.859385	52.002306	69.453889
1003.350531	43.424858	69.458894
1002.981170	45.503742	69.463898
1002.443323	48.703776	69.468903
1001.435270	41.438862	69.473908
1000.854573	54.535807	69.478913
1000.154233	43.609337	69.483918
999.560863	53.653913	69.488922
999.103939	44.336538	69.493927
998.109019	47.509953	69.498932
997.533789	55.437069	69.503937
997.149186	44.767853	69.508942
996.047838	54.008631	69.513946
995.091848	47.082343	69.518951
994.981458	56.275837	69.523956
994.110777	43.777530	69.528961
994.202683	41.419843	69.533966
993.011865	48.364748	69.538970
992.492597	53.154462	69.543975
991.948933	39.260641	69.548980
990.915217	51.828878	69.553985
990.013247	51.532598	69.558990
989.120294	46.857507	69.563994
988.597951	43.345521	69.568999
988.534010	39.673873	69.574004
988.334701	46.949851	69.579009
987.341941	49.443298	69.584014
986.564936	49.049869	69.589018
985.485605	41.135597	69.594023
984.767299	45.804023	69.599028
984.040666	48.255127	69.604033
983.543236	42.886364	69.609038
983.390459	47.065863	69.614042
982.565750	49.116280	69.619047
981.823233	53.392768	69.624052
980.872894	48.567548	69.629057
980.573328	54.427689	69.634062
979.879499	47.398198	69.639066
978.775917	46.630981	69.644071
978.317816	47.241735	69.649076
977.730813	52.728165	69.654081
977.406062	46.057820	69.659086
976.327287	47.923172	69.664090
975.580752	50.301756	69.669095
975.069430	51.190624	69.674100
974.489586	50.798942	69.679105
973.883552	46.813024	69.684110
972.593637	61.971828	69.689114
971.928224	42.245638	69.694119
971.742924	48.734109	69.699124
971.049961	50.971714	69.704129
970.738758	48.528364	69.709134
970.127868	53.780489	69.714138
968.947889	48.329530	69.719143
968.990038	45.292247	69.724148
968.156298	50.647635	69.729153
967.249668	44.039919	69.734158
966.508465	50.161131	69.739162
966.119681	37.305484	69.744167
964.940791	46.331537	69.749172
963.718666	44.220779	69.754177
963.514499	51.492801	69.759182
962.940425	45.522837	69.764186
962.667586	51.129580	69.769191
962.872980	41.855057	69.774196
961.459039	57.771567	69.779201
960.633005	42.248055	69.784206
960.307909	50.999494	69.789210
959.038413	49.014540	69.794215
958.452973	41.750205	69.799220
957.706427	43.674658	69.804225
957.398630	50.335578	69.809230
956.762998	43.711552	69.814234
955.593256	43.325435	69.819239
954.901884	41.423525	69.824244
954.454399	43.997365	69.829249
954.252719	44.431712	69.834254
953.825512	38.539303	69.839258
952.641136	47.383318	69.844263
952.228919	44.751053	69.849268
951.496563	45.626213	69.854273
950.396426	47.408248	69.859278
949.596925	38.766687	69.864282
948.950137	52.191100	69.869287
948.727214	42.169493	69.874292
948.312797	47.215325	69.879297
947.853623	40.334580	69.884302
946.596315	53.439851	69.889306
945.833388	32.068766	69.894311
945.890794	48.556922	69.899316
944.718361	46.209621	69.904321
943.924714	39.257528	69.909326
943.178640	43.678083	69.914330
942.852592	52.699319	69.919335
942.563223	40.143230	69.924340
941.321602	57.987637	69.929345
940.715660	49.141818	69.934350
940.037711	46.178123	69.939354
939.629010	57.437468	69.944359
938.811245	48.131799	69.949364
937.796984	57.172670	69.954369
937.704126	41.724879	69.959374
936.827158	45.494522	69.964378
935.786270	42.981222	69.969383
935.279016	46.586383	69.974388
934.759442	52.174047	69.979393
934.530029	43.987367	69.984398
933.601028	45.657025	69.989402
932.658880	54.894567	69.994407
932.088396	44.920385	69.999412
931.678325	50.873801	70.004417
931.267344	42.138883	70.009422
930.626742	48.794419	70.014426
929.988926	47.524199	70.019431
928.860709	43.905225	70.024436
927.688960	55.577714	70.029441
927.416986	43.293232	70.034446
926.760601	51.638525	70.039450
926.400330	42.113414	70.044455
925.319567	51.313093	70.049460
924.492366	55.199395	70.054465
924.278912	50.055098	70.059470
923.635523	47.385512	70.064474
923.024638	52.948287	70.069479
922.530852	49.199972	70.074484
921.465457	53.701311	70.079489
921.053269	51.168388	70.084494
920.570090	39.392157	70.089498
919.484720	52.552073	70.094503
918.872411	44.233950	70.099508
918.015777	51.368543	70.104513
917.811185	48.261721	70.109518
917.373080	45.461704	70.114522
916.067655	49.083507	70.119527
915.700865	47.006959	70.124532
914.833981	63.522372	70.129537
914.492968	42.170875	70.134542
913.446563	53.839189	70.139546
912.680918	55.413478	70.144551
912.309839	53.668753	70.149556
911.773317	48.605831	70.154561
911.653247	53.407719	70.159566
910.499553	47.835921	70.164570
909.621465	52.331109	70.169575
909.443319	53.668410	70.174580
908.082273	53.929313	70.179585
907.644106	47.562442	70.184590
907.215769	46.697260	70.189594
906.399171	46.426845	70.194599
905.939335	37.677635	70.199604
904.615844	43.503616	70.204609
904.272940	52.864984	70.209614
903.521358	46.186891	70.214618
903.377815	48.250350	70.219623
902.456385	42.479178	70.224628
901.292971	47.428181	70.229633
900.911468	53.493743	70.234638
900.462232	51.575389	70.239642
900.170671	54.222191	70.244647
900.033251	45.778039	70.249652
898.834102	51.142716	70.254657
897.804199	50.966171	70.259662
896.869756	43.342681	70.264666
895.964494	53.306026	70.269671
895.552376	47.695061	70.274676
894.983495	56.542070	70.279681
894.813506	43.077641	70.284686
894.415334	53.415998	70.289690
893.303815	52.752578	70.294695
892.953801	31.531840	70.299700
891.734693	46.223674	70.304705
890.679015	49.961853	70.309710
890.096509	52.913563	70.314714
889.457713	46.621203	70.319719
889.210862	44.585492	70.324724
888.895897	47.510393	70.329729
888.506170	38.901408	70.334734
887.470943	45.674944	70.339738
886.820374	39.937940	70.344743
886.403775	38.689293	70.349748
885.182310	44.065409	70.354753
884.826077	49.600277	70.359758
884.576558	55.944440	70.364762
883.100818	45.005809	70.369767
882.410958	50.641080	70.374772
881.813825	49.859533	70.379777
881.284078	39.658127	70.384782
880.918534	48.193667	70.389786
879.787693	49.789818	70.394791
879.213437	38.458579	70.399796
878.459442	51.712415	70.404801
878.228222	50.737023	70.409806
877.156652	40.408974	70.414810
876.633028	45.670878	70.419815
876.002536	38.632925	70.424820
875.243645	51.299371	70.429825
874.763172	41.853325	70.434830
873.860660	47.872504	70.439834
872.620494	49.011422	70.444839
872.897546	40.933372	70.449844
872.080785	60.376928	70.454849
871.927438	38.423183	70.459854
871.062574	52.915157	70.464858
870.186975	50.320388	70.469863
869.774760	52.390340	70.474868
868.611978	53.717206	70.479873
867.849850	54.671241	70.484878
867.008072	45.342619	70.489882
866.691490	64.388048	70.494887
866.642044	54.289956	70.499892
865.287351	48.665021	70.504897
864.822280	54.239290	70.509902
864.216207	51.059186	70.514906
863.762297	53.318691	70.519911
862.578899	50.129554	70.524916
861.864518	52.920920	70.529921
861.529295	45.864357	70.534926
860.866696	46.808860	70.539930
860.358968	55.262962	70.544935
859.582103	42.786058	70.549940
858.427060	49.816781	70.554945
858.120368	37.843758	70.559950
858.064823	55.526219	70.564954
857.042576	49.160864	70.569959
856.530322	50.902985	70.574964
855.671385	51.620133	70.579969
855.034850	45.239120	70.584974
854.065242	46.869541	70.589978
853.319710	47.510296	70.594983
853.086221	43.244359	70.599988
852.415827	49.884152	70.604993
851.197155	45.932703	70.609998
850.629564	48.781128	70.615002
849.868254	49.883262	70.620007
849.890019	55.441546	70.625012
849.503640	56.758381	70.630017
848.501174	39.050671	70.635022
847.867531	50.576039	70.640026
846.899020	49.386859	70.645031
845.978987	47.642793	70.650036
844.915898	46.471821	70.655041
844.208478	58.623914	70.660046
844.132835	53.643762	70.665050
843.416538	44.662588	70.670055
843.334483	37.043797	70.675060
842.824243	46.931662	70.680065
842.275184	50.166624	70.685070
841.525938	40.474802	70.690074
840.407127	44.724488	70.695079
840.008794	38.251957	70.700084
839.095189	52.781655	70.705089
838.531619	40.966208	70.710094
837.702255	51.401582	70.715098
836.418072	50.559101	70.720103
836.602522	34.442763	70.725108
835.924329	46.847223	70.730113
835.521497	41.034535	70.735118
834.481262	43.655435	70.740122
833.501487	49.795728	70.745127
833.282562	43.278870	70.750132
832.424701	42.590872	70.755137
831.435384	47.152669	70.760142
831.132128	42.421627	70.765146
830.397252	50.579167	70.770151
830.254475	43.570824	70.775156
828.999608	47.824826	70.780161
828.213258	40.114723	70.785166
827.804715	51.637379	70.790170
827.149486	46.605990	70.795175
826.913772	45.779544	70.800180
825.704786	53.441728	70.805185
825.155824	44.282547	70.810190
824.482530	43.172535	70.815194
823.977790	55.949918	70.820199
823.192172	33.589087	70.825204
822.497596	51.152492	70.830209
822.050160	46.285138	70.835214
821.542468	41.316996	70.840218
820.162967	56.674599	70.845223
819.750371	47.201993	70.850228
819.167333	46.481293	70.855233
818.853291	48.253367	70.860238
817.631556	45.697946	70.865242
817.357284	48.974323	70.870247
816.860289	47.587107	70.875252
816.165324	47.262669	70.880257
814.995098	50.684815	70.885262
814.233831	56.966944	70.890266
813.642467	55.312491	70.895271
813.421093	51.320579	70.900276
812.898841	47.466442	70.905281
812.301049	56.794275	70.910286
811.397896	52.064112	70.915290
810.300216	55.548826	70.920295
810.226396	54.012253	70.925300
809.147779	48.390712	70.930305
808.107702	49.843144	70.935310
807.889898	42.927166	70.940314
807.272922	43.069683	70.945319
807.265669	48.123254	70.950324
806.202015	48.270645	70.955329
805.425728	47.744702	70.960334
805.177419	50.006180	70.965338
803.847350	45.056990	70.970343
803.146859	43.328454	70.975348
802.215443	39.523684	70.980353
801.615895	44.173248	70.985358
801.873071	46.235997	70.990362
801.084731	49.190530	70.995367
799.964738	47.093557	71.000372
799.463147	55.236047	71.005377
799.009440	47.636995	71.010382
797.945299	47.387098	71.015386
797.072229	50.323582	71.020391
797.170559	44.828493	71.025396
796.400940	44.157998	71.030401
795.144132	43.185033	71.035406
794.483855	53.453160	71.040410
793.721395	56.778870	71.045415
793.503573	47.455028	71.050420
793.610865	59.250371	71.055425
792.313486	45.695782	71.060430
791.475903	51.723573	71.065434
790.823322	49.123293	71.070439
790.391073	46.103186	71.075444
788.937093	48.830965	71.080449
788.356620	50.601303	71.085454
788.370108	53.864990	71.090458
787.744007	51.916470	71.095463
787.223010	45.075566	71.100468
786.414007	44.893862	71.105473
785.551954	48.538183	71.110478
785.184187	46.628960	71.115482
783.681403	59.178895	71.120487
783.278331	49.029884	71.125492
782.266351	51.430278	71.130497
781.967304	46.665459	71.135502
781.740144	42.877890	71.140506
781.555271	56.515782	71.145511
780.619372	44.912579	71.150516
779.775915	46.368413	71.155521
779.478822	43.590129	71.160526
778.339025	43.371206	71.165530
777.667095	60.306585	71.170535
777.265271	50.762891	71.175540
775.814885	43.322510	71.180545
774.828302	54.248101	71.185550
774.516937	47.181451	71.190554
774.131627	53.378508	71.195559
773.896489	43.177541	71.200564
773.383380	46.693780	71.205569
772.696036	57.385668	71.210574
771.867331	43.972515	71.215578
771.070793	52.206112	71.220583
770.504412	47.556389	71.225588
769.210990	53.038624	71.230593
768.807392	51.161914	71.235598
768.335117	48.395750	71.240602
767.722644	58.041299	71.245607
767.310094	43.806582	71.250612
766.411468	45.020482	71.255617
765.769678	49.713047	71.260622
765.509252	48.218798	71.265626
764.064376	54.844718	71.270631
763.551642	44.268500	71.275636
762.957970	42.743731	71.280641
762.380652	43.605301	71.285646
762.166218	45.277950	71.290650
761.002112	50.014246	71.295655
760.423307	46.968593	71.300660
759.561852	53.662475	71.305665
759.317988	51.783991	71.310670
758.931824	45.758942	71.315674
757.581620	51.024731	71.320679
757.209693	49.360588	71.325684
756.717196	52.607060	71.330689
755.391568	58.938052	71.335694
754.847090	54.535564	71.340698
753.916009	54.434804	71.345703
754.037430	47.239337	71.350708
753.516986	52.106541	71.355713
752.907145	49.223517	71.360718
752.277009	49.934235	71.365722
751.217267	47.280523	71.370727
750.728219	50.270995	71.375732
749.761960	57.837802	71.380737
748.766656	52.635085	71.385742
748.736599	50.271581	71.390746
748.205749	48.714738	71.395751
746.996968	47.254785	71.400756
746.341361	49.566919	71.405761
745.780690	52.471030	71.410766
745.331524	37.035858	71.415770
744.750059	51.701919	71.420775
743.855189	51.157030	71.425780
743.020476	49.587066	71.430785
742.772331	46.834108	71.435790
742.587296	57.091237	71.440794
741.139416	58.764730	71.445799
740.815798	39.523526	71.450804
739.980728	57.039931	71.455809
739.432428	51.116387	71.460814
738.445116	54.905237	71.465818
737.420805	60.453449	71.470823
736.790901	49.813893	71.475828
736.950321	57.849576	71.480833
736.599624	48.794466	71.485838
735.967550	53.792980	71.490842
734.851051	59.565591	71.495847
733.863882	49.610506	71.500852
732.959045	58.105771	71.505857
731.983344	54.249733	71.510862
732.039103	44.065535	71.515866
731.344347	57.664761	71.520871
731.076176	45.791281	71.525876
730.752816	53.351923	71.530881
729.537467	57.143969	71.535886
728.928023	41.480442	71.540890
727.743382	55.547145	71.545895
727.033428	47.772879	71.550900
726.639366	48.919076	71.555905
725.841699	48.158457	71.560910
725.577228	40.568721	71.565914
725.060950	55.334788	71.570919
724.502698	48.537677	71.575924
723.660290	47.700608	71.580929
722.426408	45.110902	71.585934
721.906298	55.826630	71.590938
720.788074	38.471723	71.595943
720.480776	46.417713	71.600948
720.456817	47.165960	71.605953
719.734146	52.549462	71.610958
719.532724	46.952297	71.615962
718.262052	49.559472	71.620967
717.781522	50.932313	71.625972
716.723910	51.635411	71.630977
715.824375	55.973234	71.635982
715.344259	41.921170	71.640986
714.655317	51.777582	71.645991
714.532766	43.936606	71.650996
713.823366	53.942924	71.656001
712.684652	50.456606	71.661006
712.373851	48.929386	71.666010
711.842631	53.088726	71.671015
711.355755	53.003983	71.676020
710.418263	47.028881	71.681025
709.481838	55.491335	71.686030
709.052737	45.631904	71.691034
707.703444	53.974025	71.696039
707.412743	39.286294	71.701044
706.725722	48.762377	71.706049
706.074437	52.226516	71.711054
706.021197	38.108070	71.716058
705.117822	52.074804	71.721063
704.469618	53.351350	71.726068
703.999688	49.845279	71.731073
703.218181	63.057804	71.736078
702.110582	48.351908	71.741082
701.061684	57.016766	71.746087
700.840325	60.693136	71.751092
700.669976	57.420046	71.756097
699.777524	65.996926	71.761102
698.976428	52.161536	71.766106
698.430256	53.141156	71.771111
697.793449	43.368414	71.776116
697.071263	48.199942	71.781121
695.949739	50.967872	71.786126
695.458292	45.557231	71.791130
694.944198	47.313866	71.796135
694.720608	45.747534	71.801140
694.008155	50.664241	71.806145
692.807678	49.699703	71.811150
692.534502	54.166445	71.816154
691.833962	52.157267	71.821159
691.409559	45.137017	71.826164
690.126297	52.415289	71.831169
689.235238	57.753077	71.836174
689.374130	46.213736	71.841178
688.749668	46.182443	71.846183
687.990778	45.004102	71.851188
686.934479	55.177618	71.856193
686.288053	50.190600	71.861198
685.908227	42.288098	71.866202
685.253834	51.847295	71.871207
684.539739	43.288431	71.876212
683.955460	51.505596	71.881217
682.977392	53.009701	71.886222
683.074829	43.812293	71.891226
681.674757	55.454992	71.896231
681.330626	47.778603	71.901236
680.971824	33.953233	71.906241
679.605610	38.746970	71.911246
678.835637	45.801595	71.916250
678.276545	45.506021	71.921255
678.152428	43.792973	71.926260
677.427255	50.842044	71.931265
676.388539	46.836804	71.936270
675.791950	40.446337	71.941274
675.227310	44.874337	71.946279
674.761136	48.171820	71.951284
673.756161	48.596912	71.956289
672.887244	51.394011	71.961294
672.627387	41.909742	71.966298
672.111423	47.867429	71.971303
671.362721	41.264656	71.976308
670.393505	51.703413	71.981313
670.184138	49.622338	71.986318
669.997209	44.388705	71.991322
668.555182	49.481511	71.996327
667.888574	48.067722	72.001332
667.751118	45.604636	72.006337
666.483501	48.026857	72.011342
665.567643	49.229344	72.016346
665.003014	62.341111	72.021351
664.753310	41.199084	72.026356
664.234808	46.111719	72.031361
663.358423	52.915230	72.036366
663.018708	42.320956	72.041370
662.000463	45.714235	72.046375
661.439498	40.961186	72.051380
661.158660	47.263033	72.056385
660.186062	48.133956	72.061390
659.867545	38.742607	72.066394
658.611810	49.181261	72.071399
657.735988	39.150147	72.076404
657.230006	44.872871	72.081409
656.822267	43.613393	72.086414
656.598752	48.196799	72.091418
655.149380	42.430960	72.096423
654.431938	41.654436	72.101428
654.100953	38.840571	72.106433
653.530135	52.766975	72.111438
653.186386	40.921320	72.116442
651.925937	40.092503	72.121447
651.667710	46.706121	72.126452
651.143190	39.842166	72.131457
649.703535	45.349317	72.136462
649.305317	50.668553	72.141466
648.200567	59.465318	72.146471
648.174321	55.063908	72.151476
648.044953	53.947749	72.156481
646.802469	58.043756	72.161486
645.928332	43.109923	72.166490
645.524285	58.512520	72.171495
645.109210	52.386449	72.176500
644.721226	47.154875	72.181505
643.502501	56.006057	72.186510
642.784991	41.857791	72.191514
642.332796	50.047619	72.196519
641.181658	57.673860	72.201524
640.438775	40.049509	72.206529
639.820870	46.464954	72.211534
639.255725	46.952474	72.216538
639.027844	52.028556	72.221543
638.708800	41.047821	72.226548
637.992490	39.922636	72.231553
636.920894	38.095562	72.236558
636.371293	40.953777	72.241562
635.498648	39.897641	72.246567
634.336690	36.870778	72.251572
633.916059	35.515593	72.256577
633.561952	33.276236	72.261582
633.522237	35.718959	72.266586
632.633211	36.076719	72.271591
631.650468	41.531614	72.276596
631.183389	46.428181	72.281601
630.536722	42.217035	72.286606
629.969090	31.731608	72.291610
628.695415	47.572286	72.296615
628.176632	48.188035	72.301620
628.093609	37.316366	72.306625
627.170593	44.829011	72.311630
626.093040	38.592421	72.316634
625.502583	50.385312	72.321639
625.258307	42.104868	72.326644
624.676449	43.340906	72.331649
623.353319	46.623491	72.336654
622.930720	35.969896	72.341658
622.406488	41.175166	72.346663
621.884471	43.027688	72.351668
620.925887	48.995950	72.356673
619.732011	42.721119	72.361678
619.711282	33.671842	72.366682
619.212839	49.154114	72.371687
618.963503	48.556926	72.376692
618.097363	41.517164	72.381697
617.272857	49.100853	72.386702
616.832083	45.047721	72.391706
615.520947	50.007753	72.396711
614.717451	55.378922	72.401716
614.418923	43.000982	72.406721
613.765259	50.746687	72.411726
613.749755	47.348030	72.416730
612.225326	52.417722	72.421735
611.619487	54.311979	72.426740
611.208569	42.048127	72.431745
610.541245	56.950213	72.436750
609.938874	46.202249	72.441754
608.667989	51.936419	72.446759
608.309103	53.338790	72.451764
608.024376	47.203008	72.456769
607.351276	56.080843	72.461774
606.910953	56.327731	72.466778
605.689698	51.033340	72.471783
605.177453	40.644744	72.476788
605.038512	54.097120	72.481793
603.699551	49.597291	72.486798
602.909854	45.267015	72.491802
602.321146	47.164852	72.496807
601.768086	56.711081	72.501812
601.628991	39.572450	72.506817
600.493060	56.745729	72.511822
599.943387	47.607232	72.516826
599.114997	48.912500	72.521831
598.624645	57.182525	72.526836
598.248598	48.867879	72.531841
597.059917	49.826853	72.536846
596.777046	48.314124	72.541850
596.121792	43.801600	72.546855
595.536377	44.454774	72.551860
594.509022	48.863449	72.556865
593.737992	49.625028	72.561870
593.311442	41.402004	72.566874
592.675156	48.867418	72.571879
591.834419	46.754452	72.576884
591.487720	55.654417	72.581889
590.740614	47.320028	72.586894
590.390144	49.608830	72.591898
589.285980	44.685286	72.596903
588.593486	52.265303	72.601908
588.180232	53.515496	72.606913
587.446835	49.097415	72.611918
586.530683	51.564617	72.616922
585.534365	48.506664	72.621927
584.912902	39.732826	72.626932
585.257858	52.423774	72.631937
584.438373	50.239620	72.636942
583.990051	39.293682	72.641946
583.102513	39.129283	72.646951
582.350002	47.687049	72.651956
581.395280	39.600187	72.656961
580.250965	57.405549	72.661966
580.313216	44.698935	72.666970
579.813960	49.302609	72.671975
578.669546	53.715743	72.676980
578.309163	41.480121	72.681985
577.431108	51.663124	72.686990
576.768483	49.832436	72.691994
576.365701	51.298568	72.696999
575.434264	38.819608	72.702004
574.799076	48.446719	72.707009
574.149309	54.279086	72.712014
573.977318	46.346660	72.717018
572.636088	53.153275	72.722023
571.963085	54.755482	72.727028
571.641182	40.957375	72.732033
571.188436	52.808760	72.737038
570.095323	48.643508	72.742042
569.669116	47.413794	72.747047
568.847739	50.706371	72.752052
568.673874	41.924321	72.757057
567.164335	53.565581	72.762062
566.804043	33.844614	72.767066
566.087418	51.040991	72.772071
565.729813	43.280049	72.777076
565.549174	48.466873	72.782081
564.271292	51.879468	72.787086
563.400592	47.357116	72.792090
563.047481	45.125495	72.797095
562.151865	47.548435	72.802100
561.537359	43.193425	72.807105
560.612700	56.353079	72.812110
560.176744	45.285332	72.817114
560.017953	45.733376	72.822119
558.992935	59.341077	72.827124
558.186003	45.776333	72.832129
557.646810	54.309591	72.837134
557.391571	45.573616	72.842138
556.476374	38.275207	72.847143
555.494181	46.205704	72.852148
555.129884	48.627592	72.857153
554.487220	47.539584	72.862158
553.773279	44.742579	72.867162
552.888221	54.683870	72.872167
552.222298	50.639807	72.877172
551.835283	43.120081	72.882177
551.030234	51.422888	72.887182
550.005124	48.016322	72.892186
549.440204	41.343323	72.897191
549.475651	45.811372	72.902196
548.756815	35.679617	72.907201
547.725066	46.055829	72.912206
547.010082	48.591919	72.917210
546.662844	41.225123	72.922215
546.057831	47.249047	72.927220
545.116379	47.801259	72.932225
544.259527	47.140007	72.937230
543.633061	38.844769	72.942234
543.508628	47.663599	72.947239
542.556569	40.894582	72.952244
541.820886	37.858210	72.957249
540.722736	42.921536	72.962254
540.400618	44.357479	72.967258
539.984984	42.044364	72.972263
538.737360	54.213163	72.977268
538.382052	40.619071	72.982273
537.674342	45.766855	72.987278
537.378335	48.326091	72.992282
536.898629	49.432344	72.997287
535.966601	53.059505	73.002292
535.370523	41.919509	73.007297
534.593581	50.924274	73.012302
534.039212	51.780662	73.017306
533.380099	44.957101	73.022311
532.200809	52.281954	73.027316
532.087348	43.258490	73.032321
531.285961	42.495374	73.037326
530.257952	47.407192	73.042330
529.784324	46.738516	73.047335
529.616201	41.662747	73.052340
529.159252	39.141762	73.057345
527.827890	44.002560	73.062350
527.347944	49.222870	73.067354
526.742401	47.553404	73.072359
525.748326	47.937397	73.077364
525.191301	46.711183	73.082369
524.203247	54.010309	73.087374
524.128456	49.260272	73.092378
523.727654	54.128953	73.097383
522.528173	42.878510	73.102388
521.850498	43.316176	73.107393
521.072410	52.942409	73.112398
520.992656	40.925436	73.117402
520.394082	53.388220	73.122407
519.284078	52.032487	73.127412
518.901439	41.725769	73.132417
518.197737	55.745888	73.137422
517.507078	56.171433	73.142426
516.271485	51.659919	73.147431
515.682013	46.667037	73.152436
515.601736	36.681142	73.157441
514.945865	47.265553	73.162446
514.060231	43.679100	73.167450
513.179529	42.487105	73.172455
512.645937	44.040312	73.177460
512.538096	41.315495	73.182465
511.353640	41.958465	73.187470
510.542894	50.634326	73.192474
509.821454	47.234594	73.197479
509.278166	47.477402	73.202484
509.371401	40.772108	73.207489
508.085699	44.523421	73.212494
507.269846	46.181513	73.217498
506.733068	48.898948	73.222503
506.585446	44.843294	73.227508
505.768220	42.433320	73.232513
504.511209	52.057005	73.237518
504.332392	41.052388	73.242522
503.664706	49.907299	73.247527
502.427692	53.904734	73.252532
501.941436	41.714415	73.257537
501.209462	45.719698	73.262542
500.991957	48.982325	73.267546
500.657764	41.750647	73.272551
499.615357	49.119934	73.277556
498.752955	47.453549	73.282561
498.410575	47.706930	73.287566
497.801613	41.559748	73.292570
496.799209	48.730287	73.297575
495.903003	49.023012	73.302580
496.175149	31.211816	73.307585
494.904545	44.316205	73.312590
493.769004	52.403610	73.317594
493.237605	32.268411	73.322599
492.569061	43.737880	73.327604
492.377448	43.522570	73.332609
491.839595	40.566655	73.337614
491.369538	40.856145	73.342618
490.491920	52.467731	73.347623
489.632821	42.191194	73.352628
489.162697	38.896505	73.357633
487.795384	47.085482	73.362638
487.271233	45.574938	73.367642
487.140929	46.114636	73.372647
486.387125	48.822497	73.377652
485.992243	42.426762	73.382657
484.908191	45.307075	73.387662
484.142950	43.183698	73.392666
483.960124	50.617890	73.397671
483.270953	51.520994	73.402676
482.325814	47.243909	73.407681
481.407483	52.871511	73.412686
481.233705	39.209097	73.417690
480.788895	44.422237	73.422695
479.885037	47.849397	73.427700
479.474264	43.384688	73.432705
478.445463	48.870627	73.437710
477.479052	43.611399	73.442714
476.898342	50.244862	73.447719
475.857531	50.549594	73.452724
475.820445	50.311244	73.457729
475.327358	46.157675	73.462734
474.814762	44.460801	73.467738
474.134335	49.435530	73.472743
473.275940	54.268314	73.477748
472.271333	49.038824	73.482753
471.363999	56.586866	73.487758
471.046475	52.548820	73.492762
470.540274	46.115632	73.497767
469.879073	50.327256	73.502772
469.169967	50.747868	73.507777
467.854712	44.429384	73.512782
467.621124	54.894495	73.517786
467.232988	49.451684	73.522791
466.551271	53.975642	73.527796
466.529933	50.822332	73.532801
465.079629	59.455030	73.537806
464.579113	49.372092	73.542810
464.301365	33.133901	73.547815
462.971498	45.331592	73.552820
462.334541	36.271704	73.557825
461.743705	41.099704	73.562830
461.116725	52.655597	73.567834
460.816597	40.773086	73.572839
460.011326	49.008143	73.577844
459.475247	31.246874	73.582849
458.750939	42.466627	73.587854
457.789090	40.368275	73.592858
457.200943	42.385895	73.597863
456.579653	53.973997	73.602868
456.455243	45.630334	73.607873
455.143400	47.881519	73.612878
454.343858	47.488695	73.617882
453.777183	44.092708	73.622887
453.016208	41.938702	73.627892
452.998811	41.440189	73.632897
451.957903	54.493815	73.637902
451.141942	48.212478	73.642906
450.670911	37.877288	73.647911
450.207435	45.660524	73.652916
449.550186	41.572538	73.657921
448.506998	44.570926	73.662926
448.320527	47.746615	73.667930
447.790234	50.852511	73.672935
446.553262	53.109117	73.677940
445.771260	42.228996	73.682945
445.133827	45.101242	73.687950
444.779923	47.012163	73.692954
444.474434	43.311231	73.697959
443.178606	48.573238	73.702964
442.637400	31.295309	73.707969
441.903554	47.251878	73.712974
441.716639	38.796762	73.717978
440.536445	46.252672	73.722983
439.738997	51.441584	73.727988
439.720105	33.506461	73.732993
439.012511	47.891456	73.737998
437.990202	46.476061	73.743002
437.244674	39.527540	73.748007
436.656340	51.818399	73.753012
436.300464	51.824796	73.758017
435.526883	46.754045	73.763022
434.704354	41.957584	73.768026
434.242290	42.756711	73.773031
433.749735	52.810525	73.778036
433.166078	51.880294	73.783041
431.942054	51.966669	73.788046
431.175985	46.634542	73.793050
430.934137	42.615986	73.798055
430.293411	48.122106	73.803060
429.809627	37.519313	73.808065
428.674383	41.068505	73.813070
427.903971	46.041813	73.818074
427.788749	45.986214	73.823079
426.715548	50.383333	73.828084
426.034623	36.779662	73.833089
425.421975	47.808180	73.838094
425.038758	40.026123	73.843098
424.753264	38.118046	73.848103
423.536456	42.165907	73.853108
422.639539	46.747814	73.858113
422.094043	57.033979	73.863118
421.872067	47.561070	73.868122
421.336487	46.522264	73.873127
420.372841	43.862853	73.878132
420.138130	36.449774	73.883137
419.011808	46.309694	73.888142
418.146238	52.698414	73.893146
417.560360	42.923968	73.898151
416.638371	47.380570	73.903156
416.462012	43.920824	73.908161
415.813180	49.500775	73.913166
414.668254	48.197962	73.918170
414.353886	44.511064	73.923175
413.809321	62.056921	73.928180
413.225625	51.466888	73.933185
412.324599	47.603824	73.938190
411.595657	48.991071	73.943194
411.225637	47.134307	73.948199
410.162798	48.347690	73.953204
409.506991	47.302814	73.958209
408.800666	47.693040	73.963214
408.450939	50.809594	73.968218
408.232900	36.638619	73.973223
407.109475	45.954066	73.978228
406.390646	44.376796	73.983233
405.673683	43.671228	73.988238
405.183689	45.078746	73.993242
404.246036	42.615461	73.998247
403.279672	44.262877	74.003252
403.137656	50.361278	74.008257
402.547145	47.707070	74.013262
402.107341	59.275725	74.018266
401.306449	42.942717	74.023271
400.516808	50.202380	74.028276
400.146594	37.604125	74.033281
399.080052	48.257145	74.038286
397.991628	44.058118	74.043290
397.558218	39.805180	74.048295
396.914828	40.970654	74.053300
396.867939	42.077347	74.058305
396.119414	48.641374	74.063310
395.060093	48.400344	74.068314
394.702878	44.449058	74.073319
393.993836	52.769718	74.078324
393.520840	42.029604	74.083329
392.463026	37.075123	74.088334
392.014175	46.396619	74.093338
391.650469	42.443215	74.098343
390.353967	50.737643	74.103348
389.704947	45.713289	74.108353
389.491876	49.918174	74.113358
388.652311	47.975394	74.118362
387.742579	37.858354	74.123367
386.843876	54.129770	74.128372
386.672916	45.014570	74.133377
386.183769	51.400083	74.138382
384.776620	53.833637	74.143386
384.450014	38.017963	74.148391
383.466670	54.531511	74.153396
383.107204	56.500094	74.158401
383.049073	43.869453	74.163406
382.508137	40.105132	74.168410
381.720787	41.599459	74.173415
380.651976	49.756690	74.178420
380.270469	40.813807	74.183425
379.214523	43.038444	74.188430
378.449513	57.495679	74.193434
378.241867	44.890441	74.198439
377.810612	52.242803	74.203444
376.342343	50.165261	74.208449
375.614522	43.999213	74.213454
374.962551	43.556093	74.218458
374.644961	54.742596	74.223463
374.451456	49.035416	74.228468
373.708279	42.763013	74.233473
372.915192	51.797192	74.238478
372.018321	58.058460	74.243482
371.561765	50.843150	74.248487
370.308511	38.221627	74.253492
370.142555	32.637789	74.258497
369.678625	43.991096	74.263502
368.667170	45.406029	74.268506
368.067101	34.079091	74.273511
366.962595	46.016996	74.278516
366.818597	41.634372	74.283521
366.270221	38.164535	74.288526
365.890269	44.162087	74.293530
364.641649	40.605155	74.298535
363.791590	52.340102	74.303540
363.432354	40.501726	74.308545
363.425530	40.004683	74.313550
362.182412	45.378168	74.318554
361.415708	44.086067	74.323559
360.679797	44.148305	74.328564
360.333273	35.217202	74.333569
359.427178	42.042872	74.338574
358.173513	44.989687	74.343578
358.168606	32.973436	74.348583
357.553609	39.415270	74.353588
357.731635	44.404599	74.358593
356.390468	44.561715	74.363598
355.225067	39.365792	74.368602
355.006623	34.562978	74.373607
354.321720	36.168712	74.378612
353.230573	34.191927	74.383617
352.809072	39.196376	74.388622
352.192056	47.502376	74.393626
351.949582	37.269557	74.398631
350.976297	45.058357	74.403636
350.184041	37.038750	74.408641
349.737614	30.592923	74.413646
348.822416	39.011089	74.418650
348.001694	37.218277	74.423655
347.178499	35.488935	74.428660
346.643706	42.331127	74.433665
346.282838	33.036484	74.438670
346.014267	43.899796	74.443674
345.386553	48.771542	74.448679
344.319744	49.414764	74.453684
344.171501	35.503902	74.458689
343.171977	37.596567	74.463694
341.990920	43.991430	74.468698
341.653295	43.807287	74.473703
341.006994	52.256721	74.478708
340.660248	44.973463	74.483713
339.674940	48.951357	74.488718
338.832610	46.755164	74.493722
338.708496	49.214489	74.498727
337.657546	51.755295	74.503732
337.234946	37.577516	74.508737
336.277234	42.855068	74.513742
335.477267	51.576558	74.518746
335.363206	37.578252	74.523751
334.389692	54.512840	74.528756
333.669063	46.415592	74.533761
333.095616	49.143634	74.538766
332.412217	53.563817	74.543770
332.190511	45.147376	74.548775
330.937642	50.971833	74.553780
330.679515	47.287023	74.558785
330.086692	49.857315	74.563790
329.042562	58.166744	74.568794
328.730548	32.764654	74.573799
327.905051	45.779246	74.578804
327.205099	40.863950	74.583809
326.221770	49.378136	74.588814
325.477955	45.715543	74.593818
325.141309	33.036275	74.598823
324.582743	61.265955	74.603828
323.967906	44.318320	74.608833
322.935804	45.550493	74.613838
322.275692	46.761226	74.618842
322.256607	42.696144	74.623847
321.617968	47.063466	74.628852
320.692128	49.749909	74.633857
319.859338	43.127555	74.638862
319.219997	47.343612	74.643866
318.514091	49.059929	74.648871
317.395028	39.378381	74.653876
317.059551	42.186763	74.658881
316.386025	50.230558	74.663886
315.825113	46.384286	74.668890
315.715593	43.990889	74.673895
314.452657	48.077690	74.678900
313.999994	38.960098	74.683905
313.402624	33.768279	74.688910
312.496403	46.190229	74.693914
312.032879	36.312751	74.698919
310.697405	47.002352	74.703924
310.662678	42.031498	74.708929
310.352913	34.209382	74.713934
309.353957	41.980210	74.718938
308.519285	37.087970	74.723943
307.796007	41.833035	74.728948
307.401663	39.130244	74.733953
307.184503	36.194222	74.738958
306.102172	53.441029	74.743962
305.350207	38.921541	74.748967
304.979704	45.631906	74.753972
304.273877	46.111963	74.758977
303.361244	47.427599	74.763982
302.552205	48.047101	74.768986
302.292890	41.325469	74.773991
301.311329	44.979524	74.778996
300.552276	48.623346	74.784001
300.432555	40.791438	74.789006
299.745954	44.166685	74.794010
298.535364	33.148378	74.799015
297.719406	45.525984	74.804020
297.095472	37.634103	74.809025
296.918445	53.886699	74.814030
296.516820	46.271597	74.819034
295.586224	41.667445	74.824039
294.494459	45.053657	74.829044
294.178402	40.670081	74.834049
293.880483	44.484817	74.839054
292.639286	52.857201	74.844058
292.170317	46.414974	74.849063
291.401980	45.752319	74.854068
290.787936	46.295017	74.859073
290.064728	44.929778	74.864078
289.116140	41.820198	74.869082
289.094864	46.005553	74.874087
288.310762	34.808895	74.879092
287.967247	44.987184	74.884097
287.214882	45.995025	74.889102
286.212114	38.892033	74.894106
285.554067	44.634316	74.899111
284.332124	42.404038	74.904116
283.706145	48.778259	74.909121
283.161252	46.706554	74.914126
282.828288	47.068843	74.919130
282.996899	37.875888	74.924135
281.894641	43.786739	74.929140
280.622019	45.815731	74.934145
280.426652	33.301602	74.939150
279.734117	45.825109	74.944154
278.884256	32.246855	74.949159
277.665005	34.644208	74.954164
277.201553	40.836413	74.959169
277.061948	36.101462	74.964174
276.836656	49.255350	74.969178
276.235278	43.012418	74.974183
275.254842	46.483388	74.979188
274.383459	43.418274	74.984193
273.561089	38.673887	74.989198
272.253690	48.002939	74.994202
272.141258	35.317906	74.999207
271.621018	43.938053	75.004212
271.311258	42.398116	75.009217
270.788153	39.373679	75.014222
269.285290	41.081431	75.019226
269.052974	40.295500	75.024231
268.179234	40.862252	75.029236
267.777719	46.744986	75.034241
266.942124	39.960687	75.039246
266.079036	31.789993	75.044250
266.007838	42.738529	75.049255
265.380977	35.820043	75.054260
264.390917	42.925613	75.059265
263.650308	43.545258	75.064270
263.256761	39.836317	75.069274
262.386829	33.461170	75.074279
261.177928	36.396164	75.079284
260.413282	35.333988	75.084289
260.147440	37.399617	75.089294
259.846217	48.796380	75.094298
259.994685	49.171813	75.099303
258.945644	52.227977	75.104308
257.768396	37.998637	75.109313
257.446971	40.654984	75.114318
256.062965	45.763987	75.119322
255.639371	47.026916	75.124327
254.989051	62.199129	75.129332
254.524465	48.092711	75.134337
254.650992	32.506032	75.139342
253.280189	50.863205	75.144346
252.796329	46.290354	75.149351
252.037732	39.826503	75.154356
250.726309	40.816243	75.159361
249.990064	38.629980	75.164366
249.285331	45.278517	75.169370
249.455130	45.292603	75.174375
248.895597	53.318242	75.179380
248.235947	40.860776	75.184385
247.114011	45.049703	75.189390
246.433103	40.219703	75.194394
246.132466	54.464169	75.199399
245.427717	40.258859	75.204404
244.535155	47.445084	75.209409
243.863392	48.455857	75.214414
242.987486	47.638488	75.219418
243.010317	44.035054	75.224423
241.708091	38.605552	75.229428
240.850932	47.528554	75.234433
240.727323	40.753765	75.239438
240.101733	48.080349	75.244442
239.489556	46.158144	75.249447
238.597125	43.367617	75.254452
237.932539	44.616929	75.259457
237.329041	38.167782	75.264462
236.654853	44.138137	75.269466
235.992319	34.915262	75.274471
235.356666	42.765385	75.279476
234.704272	44.012754	75.284481
234.581520	34.719602	75.289486
233.271471	43.728991	75.294490
232.766533	42.921871	75.299495
232.180197	44.936098	75.304500
231.005131	40.063459	75.309505
230.058848	41.485403	75.314510
229.386741	46.818381	75.319514
229.704304	38.101545	75.324519
229.123640	49.989104	75.329524
228.372416	43.628158	75.334529
227.592802	45.859265	75.339534
226.873569	46.374594	75.344538
226.726948	41.287551	75.349543
225.331289	28.881207	75.354548
224.466436	31.177937	75.359553
223.934449	34.515937	75.364558
223.375253	42.194613	75.369562
223.297829	40.475729	75.374567
222.332270	31.838874	75.379572
221.369856	43.041435	75.384577
221.055219	42.923025	75.389582
219.822384	42.118413	75.394586
218.993927	43.426967	75.399591
218.374902	34.813711	75.404596
218.022146	48.199212	75.409601
217.800926	40.574295	75.414606
217.035153	40.373273	75.419610
216.522786	32.473097	75.424615
215.613747	45.247156	75.429620
214.909800	43.602921	75.434625
214.447009	36.831749	75.439630
213.179371	48.278504	75.444634
213.033045	36.619106	75.449639
212.199765	44.070260	75.454644
211.731027	43.864461	75.459649
211.178562	46.341618	75.464654
210.249208	56.755228	75.469658
209.967702	47.052169	75.474663
208.868429	48.132682	75.479668
208.077206	53.374277	75.484673
207.857305	41.319778	75.489678
206.956520	50.282859	75.494682
206.260389	43.014333	75.499687
204.790212	47.949455	75.504692
204.365968	51.677114	75.509697
204.335338	40.546437	75.514702
203.712158	46.940725	75.519706
203.458842	41.266761	75.524711
202.473812	52.518669	75.529716
201.682944	49.902763	75.534721
201.503053	44.862024	75.539726
200.445607	44.146147	75.544730
199.563182	32.744446	75.549735
199.050457	45.160456	75.554740
198.414479	42.707504	75.559745
197.644773	44.948078	75.564750
196.561135	50.770846	75.569754
196.324403	50.725169	75.574759
195.709625	48.134805	75.579764
195.153294	46.735107	75.584769
194.804947	42.467076	75.589774
193.616160	44.138993	75.594778
193.182134	43.073011	75.599783
192.617178	37.548075	75.604788
191.624853	45.223274	75.609793
190.814255	33.262959	75.614798
190.239268	44.181428	75.619802
189.998354	36.966485	75.624807
189.552474	47.731918	75.629812
188.348467	49.180775	75.634817
187.844590	29.817137	75.639822
187.130858	51.830362	75.644826
186.122611	38.209596	75.649831
185.411210	45.641326	75.654836
184.784559	43.907512	75.659841
184.851858	40.525634	75.664846
183.794364	45.002337	75.669850
183.599021	49.888756	75.674855
182.095676	53.832611	75.679860
181.662785	46.187832	75.684865
181.481161	43.813825	75.689870
180.636703	42.688711	75.694874
179.614989	40.943772	75.699879
178.899284	46.345209	75.704884
178.570577	36.969790	75.709889
178.461554	43.834005	75.714894
177.279591	41.537489	75.719898
176.412838	42.275035	75.724903
176.157768	44.255382	75.729908
175.415682	42.948378	75.734913
174.763331	44.582084	75.739918
173.345133	46.270087	75.744922
173.040076	39.186790	75.749927
172.750421	37.038153	75.754932
172.220147	36.868980	75.759937
171.262321	36.753782	75.764942
170.249798	42.089009	75.769946
170.027301	35.295307	75.774951
169.551580	44.669986	75.779956
168.780346	39.647845	75.784961
168.063450	45.714905	75.789966
167.360888	42.359583	75.794970
166.734249	27.219410	75.799975
165.676742	44.227333	75.804980
164.931497	34.276553	75.809985
164.947168	36.587446	75.814990
164.403085	41.409625	75.819994
163.290575	39.772203	75.824999
162.433910	32.739015	75.830004
161.900331	40.098244	75.835009
161.532256	42.503436	75.840014
161.009058	36.598139	75.845018
160.067178	37.025992	75.850023
159.509549	47.656289	75.855028
158.906792	39.403133	75.860033
157.670516	27.490209	75.865038
157.108336	35.197749	75.870042
156.397164	33.917361	75.875047
155.826285	29.003624	75.880052
155.465751	38.445084	75.885057
155.389250	31.702220	75.890062
154.209281	40.217846	75.895066
153.681883	41.948320	75.900071
152.762381	38.047313	75.905076
151.731546	38.161369	75.910081
151.292475	38.803927	75.915086
150.481554	38.775693	75.920090
150.439324	42.786199	75.925095
149.922558	43.179389	75.930100
148.660151	37.806668	75.935105
148.486377	37.126526	75.940110
147.591343	40.448315	75.945114
146.697081	36.464444	75.950119
145.754263	32.325902	75.955124
145.545516	37.944535	75.960129
145.233098	38.426560	75.965134
144.417066	40.054834	75.970138
143.355754	38.519639	75.975143
142.879492	29.196144	75.980148
142.273502	41.934511	75.985153
141.801612	29.680535	75.990158
140.392506	30.420997	75.995162
139.927571	40.817330	76.000167
139.938412	29.552334	76.005172
139.298890	42.734412	76.010177
138.638902	26.718111	76.015182
137.615826	36.135910	76.020186
137.019095	37.339738	76.025191
136.086012	30.843837	76.030196
135.092427	34.928769	76.035201
134.684882	30.897257	76.040206
133.832514	32.383104	76.045210
133.616103	39.811604	76.050215
133.218776	31.364867	76.055220
132.734957	33.548836	76.060225
131.957869	30.353635	76.065230
131.405408	35.787393	76.070234
130.545751	29.918410	76.075239
129.522068	35.435190	76.080244
128.303832	42.074173	76.085249
128.137415	30.290276	76.090254
127.624238	31.520203	76.095258
127.225207	39.198581	76.100263
126.555360	32.070969	76.105268
125.621040	39.850470	76.110273
125.332641	31.044190	76.115278
123.977355	34.059355	76.120282
123.341380	37.068625	76.125287
122.831344	31.112360	76.130292
122.322150	43.540425	76.135297
122.302302	17.339705	76.140302
121.371770	45.228129	76.145306
120.855809	39.659133	76.150311
120.566190	43.775315	76.155316
118.891005	38.873681	76.160321
118.292191	33.533928	76.165326
117.365731	36.865468	76.170330
117.246348	41.071190	76.175335
116.814111	40.135816	76.180340
115.308123	34.497625	76.185345
114.888078	27.385377	76.190350
114.566364	49.435432	76.195354
114.032333	46.713953	76.200359
113.281319	34.895549	76.205364
112.387778	48.603809	76.210369
112.148244	29.690029	76.215374
111.070819	39.452374	76.220378
110.120604	40.767764	76.225383
109.567160	30.630317	76.230388
109.055323	48.369629	76.235393
108.876094	27.779507	76.240398
108.046132	36.113189	76.245402
107.363059	36.889274	76.250407
106.729198	25.761780	76.255412
106.092896	40.450811	76.260417
105.236433	38.594404	76.265422
104.464002	38.418132	76.270426
104.015160	40.593375	76.275431
103.506107	30.803642	76.280436
101.917102	40.619186	76.285441
101.264579	33.238101	76.290446
100.899457	38.798099	76.295450
100.799231	32.428006	76.300455
100.854071	28.204506	76.305460
99.495750	44.799975	76.310465
98.966276	29.125553	76.315470
98.023250	38.109583	76.320474
96.790214	36.902970	76.325479
96.426208	26.050971	76.330484
95.593182	42.830737	76.335489
95.594472	33.751200	76.340494
94.953973	42.595534	76.345498
94.040230	35.508402	76.350503
93.169410	34.641396	76.355508
92.547895	41.765516	76.360513
92.218982	39.178480	76.365518
91.421104	37.139283	76.370522
90.261548	31.564129	76.375527
89.717650	32.887266	76.380532
89.046213	40.746274	76.385537
88.974638	21.689040	76.390542
88.272170	38.488980	76.395546
87.310052	34.752483	76.400551
87.086142	26.632896	76.405556
86.328890	33.102192	76.410561
85.567226	33.979119	76.415566
84.686145	34.004671	76.420570
84.228326	31.458693	76.425575
83.800158	28.207867	76.430580
82.648968	34.624877	76.435585
81.841723	29.670012	76.440590
81.385571	30.755246	76.445594
80.964547	27.749270	76.450599
80.510555	23.108633	76.455604
79.494710	44.362685	76.460609
79.067166	30.363971	76.465614
78.039330	40.323409	76.470618
77.250405	37.131691	76.475623
76.694612	27.082936	76.480628
76.032816	36.402143	76.485633
75.940220	24.642755	76.490638
74.564775	40.550301	76.495642
73.816323	22.741076	76.500647
73.402905	38.954064	76.505652
72.822938	29.938844	76.510657
72.640604	31.328895	76.515662
71.640090	40.498709	76.520666
70.632660	38.051420	76.525671
70.257980	37.343404	76.530676
69.618865	39.364505	76.535681
68.613453	31.426317	76.540686
67.660951	34.218015	76.545690
67.465010	19.390804	76.550695
67.211366	35.497888	76.555700
66.435607	30.880183	76.560705
65.935417	29.995078	76.565710
65.130399	34.103576	76.570714
64.327761	33.386545	76.575719
63.916037	31.110745	76.580724
62.334602	30.182049	76.585729
62.130067	30.845561	76.590734
61.547311	32.272666	76.595738
60.985308	34.191591	76.600743
60.745314	29.635091	76.605748
59.454132	24.956098	76.610753
59.118935	29.562063	76.615758
58.169218	38.063080	76.620762
58.184048	30.577158	76.625767
57.029950	31.915622	76.630772
55.879723	34.773548	76.635777
55.870341	25.900712	76.640782
55.384592	32.668892	76.645786
54.052517	26.172012	76.650791
53.686818	32.804359	76.655796
52.978887	25.009537	76.660801
52.850225	31.082144	76.665806
51.471666	27.514575	76.670810
50.805165	36.784077	76.675815
50.236761	21.456489	76.680820
49.831586	33.885307	76.685825
49.500797	24.481876	76.690830
48.339968	34.907200	76.695834
47.346954	31.765389	76.700839
47.167431	24.039250	76.705844
46.646252	34.190684	76.710849
45.831021	28.166429	76.715854
45.024559	27.282869	76.720858
44.649975	36.365476	76.725863
43.969095	28.180015	76.730868
42.845548	33.764788	76.735873
42.259593	31.575123	76.740878
42.063627	35.264814	76.745882
41.099767	28.545224	76.750887
40.514180	27.036699	76.755892
39.391786	38.286896	76.760897
38.868846	26.596149	76.765902
38.726719	34.671921	76.770906
38.155371	28.796417	76.775911
37.234239	27.369791	76.780916
36.338166	33.414993	76.785921
36.280230	34.264847	76.790926
35.523855	25.113787	76.795930
34.312588	31.109918	76.800935
33.831642	35.631908	76.805940
33.611156	32.291202	76.810945
32.875234	21.642034	76.815950
31.916808	33.804301	76.820954
31.157081	35.909298	76.825959
30.695589	23.251611	76.830964
29.515778	31.995898	76.835969
28.584319	24.206777	76.840974
28.618681	33.779208	76.845978
27.817484	31.218628	76.850983
27.534134	23.691967	76.855988
26.865959	31.998285	76.860993
26.257209	32.533895	76.865998
25.260220	30.758275	76.871002
24.726892	37.349558	76.876007
24.341404	33.573155	76.881012
23.168314	35.901768	76.886017
22.884036	29.795991	76.891022
22.300616	33.724087	76.896026
21.021028	28.015162	76.901031
20.407779	26.815386	76.906036
19.841864	34.928790	76.911041
19.749003	27.319710	76.916046
18.562239	36.926070	76.921050
17.312476	40.102645	76.926055
17.339964	29.393212	76.931060
16.492654	29.282524	76.936065
16.453399	31.305725	76.941070
15.936243	35.546507	76.946074
14.861051	32.069334	76.951079
14.142562	28.314510	76.956084
13.479476	33.925193	76.961089
12.686659	22.491954	76.966094
11.981890	33.569897	76.971098
11.203043	31.675917	76.976103
11.047226	28.619770	76.981108
10.331688	36.386484	76.986113
9.146674	34.875810	76.991118
8.763721	28.557133	76.996122
8.243768	30.942414	77.001127
7.575171	32.671785	77.006132
6.293012	34.762355	77.011137
6.016787	27.559390	77.016142
5.511244	30.224629	77.021147
5.278787	30.364356	77.026151
4.436217	31.784032	77.031156
3.160122	30.871323	77.036161