Mon Mar 08 19:25:49 2021

Number of Points = 14581

Depth (nm)	Load (N)	Time (s)
-0.400284	110.810806	0.000000
-0.439831	92.724490	0.005005
-1.311350	69.900025	0.010010
-2.632137	17.220318	0.015014
-5.945441	1.383004	0.020019
-11.551677	-0.800465	0.025024
-16.889169	-8.542582	0.030029
-21.466079	-8.777267	0.035034
-25.375842	-10.985354	0.040038
-29.488082	1.746320	0.045043
-32.762395	-5.873933	0.050048
-36.193005	-8.443853	0.055053
-40.084286	-7.311964	0.060058
-43.698215	-9.103627	0.065062
-47.883190	-1.839841	0.070067
-51.235742	-7.985853	0.075072
-54.930754	-5.448752	0.080077
-58.759730	-10.772895	0.085082
-62.373780	-10.367972	0.090086
-66.552032	-3.795885	0.095091
-70.226952	-8.963253	0.100096
-74.185886	4.223392	0.105101
-77.971938	-1.497051	0.110106
-81.327545	-12.876062	0.115110
-84.912782	-11.023434	0.120115
-88.745758	-18.759451	0.125120
-92.540294	-19.565080	0.130125
-96.777766	-12.548290	0.135130
-100.353996	-18.790989	0.140134
-104.393120	-13.928259	0.145139
-108.514241	-8.487930	0.150144
-112.219754	-4.742785	0.155149
-116.078635	-1.432021	0.160154
-119.206560	-11.741941	0.165158
-123.211834	-7.009151	0.170163
-126.784613	-6.342656	0.175168
-130.353829	-7.245679	0.180173
-134.380779	-4.704371	0.185178
-137.685618	-17.231448	0.190182
-141.734780	-0.302663	0.195187
-145.264838	-4.748763	0.200192
-148.964779	3.177326	0.205197
-153.125844	7.539243	0.210202
-156.855223	-7.009377	0.215206
-160.825896	2.218252	0.220211
-164.088096	-4.024012	0.225216
-167.931805	-12.784708	0.230221
-171.987275	-4.480175	0.235226
-175.700785	-20.187104	0.240230
-179.810179	6.458368	0.245235
-183.069347	1.250051	0.250240
-186.944334	-4.607396	0.255245
-190.736909	3.322501	0.260250
-194.157941	-9.884493	0.265254
-198.438436	-4.951549	0.270259
-201.940835	-9.747303	0.275264
-205.458328	-5.008660	0.280269
-209.398974	-2.261823	0.285274
-213.328801	-9.600582	0.290278
-217.178021	-2.889965	0.295283
-220.860410	-6.193657	0.300288
-224.471860	-12.684416	0.305293
-228.189709	-6.049941	0.310298
-231.818071	-4.983363	0.315302
-235.937215	-0.074530	0.320307
-239.553208	-8.843072	0.325312
-243.410207	-7.538146	0.330317
-247.386027	-8.540082	0.335322
-250.633219	-15.833209	0.340326
-254.726507	-14.895795	0.345331
-258.242340	-4.371931	0.350336
-261.932590	-11.135459	0.355341
-266.160725	-7.424921	0.360346
-269.624335	-11.870399	0.365350
-273.644966	-4.985687	0.370355
-277.194824	-9.483614	0.375360
-280.794431	-9.484340	0.380365
-285.159570	-2.982973	0.385370
-288.268547	-11.300981	0.390374
-292.445277	-0.903357	0.395379
-295.993917	-10.135112	0.400384
-299.877622	-12.335868	0.405389
-303.811068	-7.559065	0.410394
-307.117286	-10.191025	0.415398
-310.813350	-4.799298	0.420403
-314.729558	-6.045587	0.425408
-318.661174	-15.597753	0.430413
-322.770412	-10.479065	0.435418
-326.083989	-18.360680	0.440422
-329.859037	-7.539889	0.445427
-333.435480	-4.906190	0.450432
-337.238783	-13.376604	0.455437
-341.225602	-5.565273	0.460442
-344.783825	-14.145762	0.465446
-348.981906	-5.340396	0.470451
-352.819239	-11.731813	0.475456
-356.228808	-10.072402	0.480461
-360.166652	-3.364761	0.485466
-363.562158	-9.255893	0.490470
-367.675492	-1.875293	0.495475
-371.200495	-15.623601	0.500480
-374.941302	-13.070821	0.505485
-378.724568	-16.995196	0.510490
-382.368759	-14.885155	0.515494
-386.211197	-4.687406	0.520499
-390.054095	-10.746737	0.525504
-393.920751	-24.683274	0.530509
-397.841377	-1.937199	0.535514
-401.385313	-13.878537	0.540518
-405.072749	-15.006678	0.545523
-409.165139	9.143434	0.550528
-412.621733	-18.439839	0.555533
-416.353968	-23.375165	0.560538
-419.946454	-2.570507	0.565542
-424.305502	-9.151282	0.570547
-427.905776	-10.458875	0.575552
-431.185317	-16.863549	0.580557
-435.536593	0.831384	0.585562
-438.817422	-6.995382	0.590566
-442.821871	-3.162578	0.595571
-446.584294	-9.945819	0.600576
-450.470171	-23.964336	0.605581
-454.533717	-10.754118	0.610586
-457.812448	-11.236301	0.615590
-461.692843	-2.470446	0.620595
-465.262944	-16.105749	0.625600
-468.691810	-23.475189	0.630605
-472.689020	-1.069988	0.635610
-476.405128	-15.555518	0.640614
-480.489025	-9.390445	0.645619
-484.096627	-16.761277	0.650624
-487.964935	-11.652413	0.655629
-491.931108	-8.465837	0.660634
-495.512480	-9.852035	0.665638
-499.216414	-2.654874	0.670643
-502.754064	-13.742408	0.675648
-506.415918	-21.085614	0.680653
-510.488745	-9.458541	0.685658
-514.274457	-12.157107	0.690662
-518.156578	-14.072349	0.695667
-522.036667	-17.664080	0.700672
-525.529212	-20.351114	0.705677
-529.331188	-16.064850	0.710682
-533.236225	-16.784322	0.715686
-536.941625	-9.372425	0.720691
-540.628667	-21.058876	0.725696
-543.847699	-25.539854	0.730701
-547.976194	-7.192839	0.735706
-551.944274	-6.844156	0.740710
-555.579614	-8.224795	0.745715
-559.480977	-14.514177	0.750720
-563.344181	-16.120154	0.755725
-567.107780	-16.953622	0.760730
-570.532839	-21.048440	0.765734
-574.716899	-3.952389	0.770739
-578.193212	-15.604644	0.775744
-581.509758	-21.170619	0.780749
-585.780117	1.393496	0.785754
-589.499943	-9.783058	0.790758
-593.201686	-4.211821	0.795763
-596.672848	-14.349535	0.800768
-600.674372	-19.662553	0.805773
-604.794244	-5.487538	0.810778
-608.257183	-17.830954	0.815782
-612.355373	-5.598892	0.820787
-615.949405	-8.323189	0.825792
-619.734458	-8.487723	0.830797
-623.295001	-7.896556	0.835802
-627.048996	-25.477386	0.840806
-630.760815	-12.753569	0.845811
-634.488571	-11.134380	0.850816
-637.903451	-14.465964	0.855821
-642.134466	-9.576423	0.860826
-645.897338	-17.743713	0.865830
-649.825484	-14.657565	0.870835
-653.497029	-19.212728	0.875840
-657.129771	-17.682798	0.880845
-660.738705	-5.672331	0.885850
-664.341380	-11.537792	0.890854
-668.387744	-15.266698	0.895859
-672.619691	-22.073867	0.900864
-675.896644	-19.183196	0.905869
-679.895235	-14.163589	0.910874
-683.238517	-20.357451	0.915878
-687.168913	-20.654756	0.920883
-691.267890	-14.360780	0.925888
-694.805263	-10.431909	0.930893
-698.548486	-15.481708	0.935898
-702.384039	-14.732940	0.940902
-706.047958	-2.899685	0.945907
-709.631743	-8.578875	0.950912
-713.501224	-3.513617	0.955917
-717.612719	-9.912638	0.960922
-721.110754	-20.537826	0.965926
-724.934124	-9.142653	0.970931
-729.059830	-14.192769	0.975936
-732.172699	-17.304421	0.980941
-736.392746	-5.959360	0.985946
-739.912710	-15.516658	0.990950
-743.841206	-7.482216	0.995955
-747.782607	-10.213861	1.000960
-751.264221	-11.508387	1.005965
-755.077828	-17.187035	1.010970
-758.306427	-23.321850	1.015974
-762.404019	-9.534896	1.020979
-766.107935	-18.646465	1.025984
-769.865123	-20.071942	1.030989
-774.199315	-8.317522	1.035994
-777.449324	-16.646987	1.040998
-781.395481	-17.900326	1.046003
-785.042669	-20.633206	1.051008
-788.622448	-18.003032	1.056013
-792.704352	-10.640950	1.061018
-796.223285	-9.617816	1.066022
-800.260881	-6.815100	1.071027
-803.761435	-7.707584	1.076032
-807.883096	-17.416148	1.081037
-811.680456	-14.625011	1.086042
-814.902609	-8.816321	1.091046
-818.840977	-3.022428	1.096051
-822.824710	-8.787299	1.101056
-826.304245	-17.406401	1.106061
-830.548359	-9.948943	1.111066
-833.887254	-20.395982	1.116070
-837.338477	-15.362708	1.121075
-841.502941	-7.318770	1.126080
-845.244226	-16.022143	1.131085
-849.590817	-12.036206	1.136090
-852.944680	-17.324604	1.141094
-856.508399	-16.598547	1.146099
-860.194333	-9.745902	1.151104
-863.602837	-18.365263	1.156109
-867.808758	-8.359391	1.161114
-871.384625	-11.748461	1.166118
-875.319938	-10.341694	1.171123
-879.313394	-14.506008	1.176128
-883.138520	-11.475371	1.181133
-886.926560	-13.269435	1.186138
-890.496319	-14.119186	1.191142
-894.331565	-6.206640	1.196147
-897.803133	-3.177322	1.201152
-901.457608	-12.906804	1.206157
-905.583891	-5.878030	1.211162
-909.262813	-12.342716	1.216166
-912.943948	-11.635643	1.221171
-916.581417	-16.000305	1.226176
-920.119604	-14.668004	1.231181
-923.789538	-10.954125	1.236186
-928.064535	-17.511102	1.241190
-931.847259	-7.027213	1.246195
-935.970660	-12.597675	1.251200
-939.423301	-19.442240	1.256205
-943.102485	-8.164406	1.261210
-946.847743	-11.124179	1.266214
-950.440366	-11.290571	1.271219
-954.575137	-12.105056	1.276224
-958.081475	-17.204924	1.281229
-962.103904	-8.797176	1.286234
-965.641642	-15.940304	1.291238
-969.562510	-3.925245	1.296243
-973.221118	-10.304773	1.301248
-977.035458	-18.058027	1.306253
-980.631548	-23.835727	1.311258
-984.174631	-15.996579	1.316262
-988.181667	-11.374049	1.321267
-992.099520	-5.293022	1.326272
-995.669953	-12.755701	1.331277
-999.497045	-9.888553	1.336282
-1002.956974	-15.207068	1.341286
-1006.947141	-6.008111	1.346291
-1011.185935	-7.099147	1.351296
-1014.643964	-6.282531	1.356301
-1018.350439	-13.619343	1.361306
-1021.699166	-23.490553	1.366310
-1025.800090	-12.359592	1.371315
-1029.516382	-10.407331	1.376320
-1033.428771	-9.423401	1.381325
-1036.961372	-1.809756	1.386330
-1040.376251	-17.813662	1.391334
-1044.614903	-18.616099	1.396339
-1048.669066	-10.248863	1.401344
-1052.194366	-20.347228	1.406349
-1055.988531	-12.406315	1.411354
-1059.635462	-14.380350	1.416358
-1063.454727	-11.881751	1.421363
-1067.254993	-16.086099	1.426368
-1070.907471	-22.542128	1.431373
-1074.787209	-16.731975	1.436378
-1078.503673	-24.473902	1.441382
-1082.352736	-19.758228	1.446387
-1086.387051	-17.702966	1.451392
-1089.896053	-19.235432	1.456397
-1093.456686	-11.744948	1.461402
-1096.932690	-14.302886	1.466406
-1100.817530	-15.352621	1.471411
-1104.755075	-4.493647	1.476416
-1108.588470	-14.988874	1.481421
-1112.849926	-2.051850	1.486426
-1116.408632	-5.003349	1.491430
-1119.293429	-8.214037	1.496435
-1123.446909	-17.210503	1.501440
-1127.200151	-30.279264	1.506445
-1131.227812	-12.988184	1.511450
-1135.251887	-14.313602	1.516454
-1138.754802	-8.382300	1.521459
-1142.228501	-18.594423	1.526464
-1145.812494	-24.525168	1.531469
-1150.083277	-23.497891	1.536474
-1153.763563	-7.236826	1.541478
-1157.667536	-3.357416	1.546483
-1161.733093	-15.931493	1.551488
-1164.563249	-17.641847	1.556493
-1168.536807	-17.259711	1.561498
-1172.469703	-22.357212	1.566502
-1176.465580	-12.094296	1.571507
-1180.129838	-12.855945	1.576512
-1183.469460	-16.536194	1.581517
-1187.763424	-11.250880	1.586522
-1191.314141	-24.265218	1.591526
-1194.946381	-24.241980	1.596531
-1199.006984	-12.071758	1.601536
-1202.383920	-9.503381	1.606541
-1206.494332	3.132115	1.611546
-1209.829329	-12.557898	1.616550
-1214.104040	-25.333343	1.621555
-1217.953595	-17.154680	1.626560
-1221.248976	-13.388331	1.631565
-1225.439200	-1.641977	1.636570
-1228.950228	-14.807678	1.641574
-1232.837583	-4.565188	1.646579
-1236.448148	-12.445218	1.651584
-1239.913019	-40.380431	1.656589
-1244.197608	-12.305209	1.661594
-1247.665815	-17.842774	1.666598
-1251.573367	-14.995455	1.671603
-1255.327470	-16.004357	1.676608
-1258.778301	-20.661666	1.681613
-1262.702806	-9.821879	1.686618
-1266.238664	-15.351741	1.691622
-1270.444098	-14.702102	1.696627
-1274.260404	-3.215770	1.701632
-1277.686939	-18.367511	1.706637
-1281.877102	-13.538576	1.711642
-1285.207242	-27.419041	1.716646
-1289.236646	-9.443096	1.721651
-1292.880094	-8.730418	1.726656
-1296.841046	-7.840768	1.731661
-1300.351271	-15.497075	1.736666
-1304.114213	-19.085731	1.741670
-1307.557130	3.990413	1.746675
-1311.507230	-24.209200	1.751680
-1315.255632	2.916235	1.756685
-1319.125953	-32.831731	1.761690
-1322.916335	-4.904865	1.766694
-1327.201078	-9.898471	1.771699
-1330.319592	-6.161860	1.776704
-1334.041635	-21.755012	1.781709
-1338.047064	-19.476880	1.786714
-1341.693101	-4.152928	1.791718
-1345.626598	-27.913226	1.796723
-1349.580034	-0.628783	1.801728
-1352.790002	-10.461782	1.806733
-1356.893874	-6.233102	1.811738
-1360.806245	-21.196546	1.816742
-1364.289117	-8.036849	1.821747
-1368.058440	-18.418878	1.826752
-1371.431020	-22.732179	1.831757
-1375.581307	-15.219416	1.836762
-1379.139035	-8.192564	1.841766
-1382.946555	-12.209154	1.846771
-1387.387489	-29.866262	1.851776
-1390.785043	-5.244130	1.856781
-1394.432299	-14.844637	1.861786
-1398.331463	-3.090982	1.866790
-1401.645845	-3.291763	1.871795
-1406.236576	-16.277984	1.876800
-1409.439639	3.298772	1.881805
-1413.680350	-6.796415	1.886810
-1417.110811	-8.889687	1.891814
-1420.325054	-13.206195	1.896819
-1424.220146	6.970205	1.901824
-1427.810523	-12.065565	1.906829
-1432.219302	-10.451173	1.911834
-1435.857221	-15.338426	1.916838
-1439.459914	-1.847225	1.921843
-1443.758980	2.822837	1.926848
-1446.969857	-26.160286	1.931853
-1450.413091	-11.127260	1.936858
-1454.442069	-3.816693	1.941862
-1458.755568	-10.451636	1.946867
-1462.396991	-20.967510	1.951872
-1465.689537	-7.954837	1.956877
-1470.016965	-6.227255	1.961882
-1473.505082	-4.697149	1.966886
-1477.128836	-6.141265	1.971891
-1480.937985	-4.288523	1.976896
-1484.478519	-7.770584	1.981901
-1488.485373	-22.581473	1.986906
-1492.066773	-6.264809	1.991910
-1495.783860	-8.573809	1.996915
-1500.005699	-8.011004	2.006912
-1501.029279	-7.928797	2.016909
-1498.402170	-10.376393	2.026906
-1495.414390	3.042367	2.036902
-1493.268669	-15.484331	2.046899
-1491.338990	-6.577353	2.056896
-1489.695809	-6.802247	2.066893
-1487.946493	-12.356912	2.076890
-1485.951488	-6.357549	2.086886
-1483.783976	-6.644307	2.096883
-1481.742299	-9.318631	2.106880
-1480.093617	-15.253460	2.116877
-1478.514023	-13.641453	2.126874
-1476.392427	-3.671063	2.136870
-1474.347534	-11.031875	2.146867
-1472.362181	-9.506947	2.156864
-1470.652490	-12.950668	2.166861
-1468.747779	-17.901827	2.176858
-1467.084708	-7.722221	2.186854
-1464.930956	-3.658648	2.196851
-1462.852005	-8.888743	2.206848
-1461.252459	-10.445480	2.216845
-1459.121304	-4.786818	2.226842
-1457.392127	-8.322066	2.236838
-1455.606470	-12.362110	2.246835
-1453.519164	-16.649390	2.256832
-1451.558245	-10.391925	2.266829
-1449.938038	-13.874982	2.276826
-1448.114550	-5.825632	2.286822
-1446.076492	-10.622879	2.296819
-1444.114822	-10.183529	2.306816
-1442.529302	-11.987463	2.316813
-1440.321903	-14.445148	2.326810
-1438.657932	-18.407276	2.336806
-1436.589019	-13.828024	2.346803
-1434.694814	-12.997364	2.356800
-1432.972670	-12.645957	2.366797
-1431.043218	-17.749459	2.376794
-1428.893468	-13.955193	2.386790
-1427.440789	-11.025026	2.396787
-1425.594189	-10.755116	2.406784
-1423.343079	-12.150914	2.416781
-1421.572331	-17.154792	2.426778
-1419.870216	-15.341325	2.436774
-1417.778413	-13.372375	2.446771
-1415.815834	-11.194850	2.456768
-1414.023158	-10.373177	2.466765
-1412.347367	-18.339525	2.476762
-1410.376814	-11.099952	2.486758
-1408.465690	-18.278247	2.496755
-1406.358649	-13.581922	2.506752
-1404.492030	-20.074189	2.516749
-1403.242682	-20.957490	2.526746
-1401.327152	-12.769693	2.536742
-1399.048489	-13.918845	2.546739
-1397.152072	-10.701310	2.556736
-1395.341638	-14.498978	2.566733
-1393.105518	-19.083171	2.576730
-1391.682784	-17.540718	2.586726
-1389.773716	-16.303483	2.596723
-1387.698864	-3.676233	2.606720
-1385.868847	-15.055439	2.616717
-1384.109989	-9.738122	2.626714
-1382.039479	-12.265409	2.636710
-1380.228103	-15.936910	2.646707
-1378.648669	-9.705136	2.656704
-1376.656099	-13.126191	2.666701
-1374.671436	-16.672284	2.676698
-1372.759063	-16.397074	2.686694
-1370.992064	-19.483609	2.696691
-1368.896004	-10.547897	2.706688
-1367.042262	-14.906650	2.716685
-1365.268866	1.614934	2.726682
-1363.135595	-16.505494	2.736678
-1361.694798	-15.062223	2.746675
-1359.799619	-6.665877	2.756672
-1357.593236	-8.984386	2.766669
-1356.118254	-9.392242	2.776666
-1353.909590	-1.693398	2.786662
-1352.090172	0.096607	2.796659
-1350.242957	-6.147800	2.806656
-1348.372372	-12.500148	2.816653
-1346.445081	-0.166574	2.826650
-1344.480813	-10.983079	2.836646
-1342.773390	-4.653352	2.846643
-1340.894929	-8.177682	2.856640
-1338.947962	2.488659	2.866637
-1337.050529	-13.885697	2.876634
-1335.504622	17.233958	2.886630
-1333.191950	-1.984059	2.896627
-1331.514969	-0.365433	2.906624
-1329.660579	-6.071012	2.916621
-1327.814799	-7.201320	2.926618
-1325.699544	-12.858658	2.936614
-1323.775441	-0.019325	2.946611
-1321.972529	-1.733251	2.956608
-1320.308079	-5.218570	2.966605
-1318.487533	-0.738381	2.976602
-1316.393260	2.529653	2.986598
-1314.442664	-8.740927	2.996595
-1312.742308	-5.667184	3.006592
-1310.573516	-6.915496	3.016589
-1308.977712	1.408832	3.026586
-1307.406553	-2.760971	3.036582
-1305.258191	-0.887804	3.046579
-1303.191182	-3.403411	3.056576
-1301.437536	-0.562384	3.066573
-1299.311565	6.202455	3.076570
-1297.674593	-0.191407	3.086566
-1295.849890	-6.369017	3.096563
-1293.943784	1.604095	3.106560
-1291.845467	6.674539	3.116557
-1290.133671	-5.896656	3.126554
-1288.543586	-5.536633	3.136550
-1286.418343	-9.495131	3.146547
-1284.295011	-4.422372	3.156544
-1282.808918	1.556018	3.166541
-1280.735497	-1.590553	3.176538
-1278.943722	-1.295962	3.186534
-1276.934658	-11.456475	3.196531
-1275.177264	-1.563361	3.206528
-1273.316040	-5.395911	3.216525
-1271.374347	-4.585347	3.226522
-1269.368464	-2.441464	3.236518
-1267.652271	-5.390329	3.246515
-1265.644692	-4.508206	3.256512
-1263.891114	-0.756149	3.266509
-1262.072870	-2.478799	3.276506
-1260.173944	-2.302388	3.286502
-1258.468256	-8.609333	3.296499
-1256.623802	3.612861	3.306496
-1254.412598	-4.435929	3.316493
-1252.455338	-1.210639	3.326490
-1250.768195	0.057498	3.336486
-1248.726259	-3.246627	3.346483
-1246.871193	0.418153	3.356480
-1245.190015	-1.329912	3.366477
-1243.380534	-1.527567	3.376474
-1241.205451	-9.250058	3.386470
-1239.397589	-8.124384	3.396467
-1237.528049	-4.272453	3.406464
-1235.746685	-10.376771	3.416461
-1234.118080	6.911749	3.426458
-1232.273685	-5.781680	3.436454
-1229.988701	4.039672	3.446451
-1228.263271	-1.125756	3.456448
-1226.267980	-4.998673	3.466445
-1224.601133	2.002337	3.476442
-1222.370242	-13.105403	3.486438
-1220.482505	-3.574131	3.496435
-1219.094457	-2.450724	3.506432
-1216.973575	-2.868708	3.516429
-1215.122445	-10.776158	3.526426
-1213.153222	-2.825706	3.536422
-1211.143376	0.828544	3.546419
-1209.381002	-3.925969	3.556416
-1207.987164	-0.432066	3.566413
-1205.873327	-8.144726	3.576410
-1203.854207	-4.973501	3.586406
-1201.980954	-7.153298	3.596403
-1199.981276	-3.642665	3.606400
-1197.817471	2.003138	3.616397
-1196.229841	-1.859778	3.626394
-1194.649984	-1.218598	3.636390
-1192.588380	-6.142554	3.646387
-1190.700266	-0.146333	3.656384
-1188.844773	-0.681285	3.666381
-1186.920284	-4.669147	3.676378
-1185.128924	4.397617	3.686374
-1183.314773	-1.549294	3.696371
-1181.412792	0.694973	3.706368
-1179.344393	-0.799241	3.716365
-1177.572776	-3.048013	3.726362
-1175.745423	-0.828114	3.736358
-1173.593422	-4.659752	3.746355
-1171.923476	1.155095	3.756352
-1169.996554	-6.121866	3.766349
-1168.488031	5.699461	3.776346
-1166.105756	1.395220	3.786342
-1164.465476	-3.699700	3.796339
-1162.527230	-9.694869	3.806336
-1160.579409	1.508310	3.816333
-1159.155374	2.698623	3.826330
-1156.902120	-0.681867	3.836326
-1154.870235	0.186992	3.846323
-1152.955953	1.500956	3.856320
-1151.318535	-0.213201	3.866317
-1149.743929	0.724093	3.876314
-1147.140097	2.256130	3.886310
-1145.336854	-4.593684	3.896307
-1144.111689	3.464837	3.906304
-1142.245420	-1.383617	3.916301
-1139.901894	-1.020893	3.926298
-1137.829277	0.665618	3.936294
-1136.284523	-5.277626	3.946291
-1134.498952	-13.125584	3.956288
-1132.723067	-6.258786	3.966285
-1130.824137	-1.874660	3.976282
-1128.687867	-6.272124	3.986278
-1126.927747	-5.842885	3.996275
-1124.731798	-0.685279	4.006272
-1123.258115	-3.451569	4.016269
-1121.346484	0.179006	4.026266
-1119.231872	-2.827185	4.036262
-1117.372569	-2.647475	4.046259
-1115.571868	-2.557856	4.056256
-1113.828778	-6.497691	4.066253
-1111.958879	-0.324815	4.076250
-1110.043431	0.223261	4.086246
-1108.024970	-5.429462	4.096243
-1106.132735	-4.947138	4.106240
-1104.611566	3.509283	4.116237
-1102.567704	5.797229	4.126234
-1100.624563	-4.938360	4.136230
-1098.608022	-2.578150	4.146227
-1096.967994	-1.073431	4.156224
-1094.870866	2.325399	4.166221
-1093.097889	-0.163513	4.176218
-1091.415671	-0.339111	4.186214
-1089.217974	1.902132	4.196211
-1087.231034	-6.652178	4.206208
-1085.644748	-7.563953	4.216205
-1083.816489	-3.452673	4.226202
-1082.038290	-7.524410	4.236198
-1080.005955	-3.051064	4.246195
-1078.040459	-14.229125	4.256192
-1076.112486	2.247481	4.266189
-1074.224621	-9.412339	4.276186
-1072.533165	-0.045305	4.286182
-1070.712507	-7.278352	4.296179
-1068.794576	-4.659200	4.306176
-1066.645145	-1.799203	4.316173
-1064.739829	-5.562864	4.326170
-1063.198872	-5.603746	4.336166
-1061.248545	-3.149233	4.346163
-1059.247118	-6.171999	4.356160
-1057.571777	-7.421663	4.366157
-1055.935171	0.084810	4.376154
-1053.701109	-11.608270	4.386150
-1051.501221	-4.368731	4.396147
-1049.933910	-1.436125	4.406144
-1048.352123	-3.344983	4.416141
-1046.237319	-9.644603	4.426138
-1044.420280	-7.159282	4.436134
-1042.331758	-1.570753	4.446131
-1040.411956	1.311792	4.456128
-1038.648641	-2.432293	4.466125
-1036.834667	-2.447360	4.476122
-1034.863564	-0.375069	4.486118
-1032.885956	-4.454986	4.496115
-1031.234793	-14.856466	4.506112
-1029.340180	-5.244020	4.516109
-1027.603567	-2.425315	4.526106
-1025.406996	-1.650575	4.536102
-1023.824998	-4.628327	4.546099
-1021.699028	-0.401994	4.556096
-1019.874910	-2.005407	4.566093
-1018.176126	-6.280698	4.576090
-1016.118056	-1.432486	4.586086
-1014.362415	-6.439978	4.596083
-1012.350116	-10.170187	4.606080
-1010.464826	-9.159341	4.616077
-1008.725255	-5.548517	4.626074
-1006.804472	-4.589131	4.636070
-1005.273409	-4.407355	4.646067
-1003.115273	-5.765778	4.656064
-1001.082210	-10.201883	4.666061
-999.266710	-9.266702	4.676058
-997.358959	-9.069385	4.686054
-995.659967	-8.320816	4.696051
-993.355711	-10.128888	4.706048
-991.861279	-9.066566	4.716045
-990.049407	-2.431176	4.726042
-987.875258	0.390209	4.736038
-986.154240	-5.213266	4.746035
-984.203201	-5.673344	4.756032
-982.414875	-8.313040	4.766029
-980.614738	-5.640239	4.776026
-979.043703	-7.004210	4.786022
-976.811080	-7.127237	4.796019
-974.841745	-4.601483	4.806016
-973.146086	-4.438116	4.816013
-971.221865	-1.763048	4.826010
-969.171726	-3.238370	4.836006
-967.151870	-11.221574	4.846003
-965.201467	-0.514378	4.856000
-963.467191	-6.221003	4.865997
-961.898308	-2.780199	4.875994
-959.858448	-11.623908	4.885990
-958.033226	-3.779654	4.895987
-955.930052	-6.007082	4.905984
-954.373145	-7.450877	4.915981
-952.978857	-5.193119	4.925978
-950.406466	-13.229936	4.935974
-948.508981	-7.328156	4.945971
-946.663865	-12.299385	4.955968
-944.651977	-13.762253	4.965965
-943.170787	-1.514835	4.975962
-941.192796	0.895887	4.985958
-939.162174	1.676722	4.995955
-937.319954	2.522422	5.005952
-935.333739	-2.509258	5.015949
-933.620917	-5.583658	5.025946
-931.656207	-8.442563	5.035942
-930.217770	-5.598205	5.045939
-928.267595	-2.212034	5.055936
-925.934970	-2.428367	5.065933
-924.128557	-1.936908	5.075930
-922.162149	-7.142239	5.085926
-920.593342	0.856729	5.095923
-918.563087	-5.839765	5.105920
-916.711902	-3.481372	5.115917
-914.970147	-3.645839	5.125914
-912.906550	-4.600667	5.135910
-911.062774	-1.870056	5.145907
-909.007206	2.116608	5.155904
-907.245366	-2.696026	5.165901
-905.752831	-13.065753	5.175898
-903.810159	-0.176879	5.185894
-901.997347	4.524354	5.195891
-899.631380	-5.205087	5.205888
-897.942710	-3.895885	5.215885
-896.063939	-3.824895	5.225882
-894.283127	-5.381817	5.235878
-892.291552	0.798636	5.245875
-890.355196	-3.271414	5.255872
-888.649908	-3.766324	5.265869
-886.827774	5.447349	5.275866
-884.751537	5.565717	5.285862
-882.877476	-5.234456	5.295859
-881.080926	-2.284704	5.305856
-879.159574	-7.768569	5.315853
-877.218032	-4.747267	5.325850
-875.574207	-5.821249	5.335846
-873.612130	-5.757245	5.345843
-871.766095	1.747465	5.355840
-869.762308	0.949069	5.365837
-867.926812	-1.123386	5.375834
-866.138174	4.372743	5.385830
-864.262432	1.207609	5.395827
-862.356270	-5.284276	5.405824
-860.232737	-2.978854	5.415821
-858.621649	-6.602162	5.425818
-856.819436	-0.722959	5.435814
-854.727014	-1.183431	5.445811
-852.674612	-0.769137	5.455808
-851.020868	-1.738906	5.465805
-849.541618	-0.740375	5.475802
-847.281015	-11.693893	5.485798
-845.280551	4.119296	5.495795
-843.606976	1.327530	5.505792
-841.440618	1.485210	5.515789
-839.839591	3.703672	5.525786
-837.817898	-7.584252	5.535782
-836.345326	-1.117104	5.545779
-834.073729	-8.837314	5.555776
-832.224143	-2.171506	5.565773
-830.352671	-4.207056	5.575770
-828.549030	0.121516	5.585766
-826.478307	-5.820372	5.595763
-824.710247	-4.882206	5.605760
-823.160391	-0.509901	5.615757
-821.278818	-4.215898	5.625754
-819.074171	4.444083	5.635750
-816.970806	-4.322836	5.645747
-815.530299	-3.848582	5.655744
-813.458033	-8.143969	5.665741
-811.474100	-10.424835	5.675738
-809.810228	-1.499989	5.685734
-807.897687	-5.424071	5.695731
-805.985079	-0.858706	5.705728
-804.057635	-7.736031	5.715725
-802.330102	-3.532632	5.725722
-800.555410	-2.360260	5.735718
-798.528046	-2.972903	5.745715
-796.666934	-1.988016	5.755712
-794.861430	-2.194162	5.765709
-792.938549	-1.902786	5.775706
-791.011546	-4.147695	5.785702
-789.026883	-7.001781	5.795699
-787.220730	-1.918890	5.805696
-785.473010	-7.188625	5.815693
-783.261582	-4.189858	5.825690
-781.725525	-5.008144	5.835686
-779.848851	-5.243022	5.845683
-777.701863	-10.720247	5.855680
-775.953240	-1.281587	5.865677
-774.114311	4.503403	5.875674
-772.415536	-4.506684	5.885670
-770.591305	-4.469505	5.895667
-768.671011	-3.363011	5.905664
-766.478239	-4.632026	5.915661
-764.902451	-5.485071	5.925658
-763.053178	-6.579185	5.935654
-760.805446	-4.242999	5.945651
-758.889286	-5.199390	5.955648
-757.372201	2.408522	5.965645
-755.393514	-0.364061	5.975642
-753.387716	-3.853036	5.985638
-751.538493	2.713434	5.995635
-749.714362	-8.857039	6.005632
-747.944612	-8.850605	6.015629
-746.016942	1.148375	6.025626
-744.377149	-4.667731	6.035622
-742.158794	-2.522609	6.045619
-740.237286	-2.602000	6.055616
-738.605755	-1.896142	6.065613
-736.656869	-3.056680	6.075610
-734.465952	-0.675074	6.085606
-732.819415	-4.264496	6.095603
-730.966055	-5.954464	6.105600
-729.191621	-1.651142	6.115597
-727.227010	-6.867087	6.125594
-725.285903	-3.307197	6.135590
-723.504862	-0.340631	6.145587
-721.575183	1.069119	6.155584
-719.448989	-3.176392	6.165581
-718.042008	-6.435432	6.175578
-716.315036	0.401643	6.185574
-714.037635	-0.631392	6.195571
-711.876314	-6.584508	6.205568
-710.346764	-8.451642	6.215565
-708.320711	-8.555610	6.225562
-706.475762	-7.958043	6.235558
-704.656285	-5.387582	6.245555
-703.142293	-5.550227	6.255552
-700.820140	-1.923326	6.265549
-698.992205	-3.490793	6.275546
-697.120793	-3.672662	6.285542
-695.439650	2.147082	6.295539
-693.490247	7.319259	6.305536
-691.750681	0.470460	6.315533
-689.624554	-0.473644	6.325530
-687.832556	-1.125942	6.335526
-686.068068	-1.615958	6.345523
-683.988805	-5.970774	6.355520
-681.999926	-4.115743	6.365517
-680.356067	1.048433	6.375514
-678.555599	1.206316	6.385510
-676.635311	-2.897314	6.395507
-674.634648	-12.612380	6.405504
-672.675490	-7.065983	6.415501
-670.825363	-9.860582	6.425498
-669.150659	-3.536138	6.435494
-667.089974	-9.883634	6.445491
-665.331842	-5.197155	6.455488
-663.539534	1.534791	6.465485
-661.491951	1.727404	6.475482
-659.644219	-2.082005	6.485478
-658.027102	-8.529129	6.495475
-655.986489	-7.422823	6.505472
-653.770163	-5.971985	6.515469
-652.030681	0.354753	6.525466
-650.389629	-5.532543	6.535462
-648.593618	-1.646263	6.545459
-646.551855	-0.829062	6.555456
-644.527974	-0.989466	6.565453
-642.616982	-1.236035	6.575450
-640.817060	-3.108436	6.585446
-639.279789	4.183725	6.595443
-637.345883	-4.983842	6.605440
-635.238996	-2.298207	6.615437
-633.424657	4.712860	6.625434
-631.461961	-1.475279	6.635430
-629.523753	-2.307202	6.645427
-627.543071	4.699394	6.655424
-625.935574	-4.899139	6.665421
-624.088056	3.402869	6.675418
-621.919665	6.175001	6.685414
-620.559240	9.052551	6.695411
-618.489380	5.891321	6.705408
-616.264030	0.774316	6.715405
-614.402967	-2.672476	6.725402
-613.020643	-2.277217	6.735398
-610.986314	-0.339392	6.745395
-609.196001	-1.651322	6.755392
-607.034590	4.740664	6.765389
-605.131803	1.880860	6.775386
-603.471389	-3.076401	6.785382
-601.481215	1.172029	6.795379
-599.593814	-2.714722	6.805376
-597.650007	0.936421	6.815373
-595.980625	8.224875	6.825370
-593.974778	1.136240	6.835366
-592.177591	-0.445180	6.845363
-589.985861	-7.748232	6.855360
-588.372595	5.207790	6.865357
-586.543915	6.183817	6.875354
-584.730491	-0.267789	6.885350
-582.693983	-4.615690	6.895347
-580.813321	3.354238	6.905344
-578.989254	1.695906	6.915341
-577.274402	2.852747	6.925338
-575.173364	2.451141	6.935334
-573.331789	-3.591294	6.945331
-571.506259	1.259747	6.955328
-569.560781	1.805047	6.965325
-567.713708	5.905854	6.975322
-565.966322	0.819466	6.985318
-564.004295	-0.336717	6.995315
-562.231886	2.007709	7.005312
-560.275190	-10.559549	7.015309
-558.318171	2.123697	7.025306
-556.482650	1.950830	7.035302
-554.554065	-4.596514	7.045299
-552.989009	-2.338949	7.055296
-550.797137	-2.721889	7.065293
-548.752160	0.496316	7.075290
-546.984345	-3.338135	7.085286
-545.358351	-1.496064	7.095283
-543.319091	0.726805	7.105280
-541.453397	-0.783422	7.115277
-539.555751	-6.612171	7.125274
-537.767881	4.637682	7.135270
-535.914913	-0.718169	7.145267
-534.122468	-1.218854	7.155264
-532.303004	-4.681042	7.165261
-530.129979	5.673659	7.175258
-528.209843	0.289716	7.185254
-526.663559	-2.786219	7.195251
-524.479006	-3.633726	7.205248
-522.597850	-6.125295	7.215245
-520.687397	-2.786109	7.225242
-519.009514	-0.728112	7.235238
-517.015965	-2.042440	7.245235
-515.143446	9.942291	7.255232
-513.547186	-1.299549	7.265229
-511.002644	3.537736	7.275226
-509.578370	4.491584	7.285222
-507.709902	-0.476745	7.295219
-506.023742	2.762500	7.305216
-504.019270	-1.330763	7.315213
-502.215322	-0.221254	7.325210
-499.931290	4.294520	7.335206
-498.422667	0.042057	7.345203
-496.359849	3.203779	7.355200
-494.468909	1.204848	7.365197
-492.705967	0.993099	7.375194
-490.829382	3.685656	7.385190
-488.978077	-1.794625	7.395187
-486.952539	-4.350279	7.405184
-484.987589	-1.976551	7.415181
-483.354245	-0.282443	7.425178
-481.491962	-1.421049	7.435174
-479.999209	-0.888623	7.445171
-477.672519	-7.760006	7.455168
-475.777002	-6.481956	7.465165
-473.545309	-1.529929	7.475162
-472.012947	-8.223914	7.485158
-470.352276	-3.606971	7.495155
-468.299986	-0.948776	7.505152
-466.353110	1.083665	7.515149
-464.429119	-1.346811	7.525146
-462.823780	-2.127015	7.535142
-460.798728	-5.768820	7.545139
-458.616679	-7.241093	7.555136
-456.865819	-1.869643	7.565133
-455.011683	2.572739	7.575130
-453.698008	-5.512015	7.585126
-451.811024	-1.788519	7.595123
-449.227459	-4.008553	7.605120
-447.157370	-3.314117	7.615117
-445.826395	-11.771078	7.625114
-444.136345	-7.067235	7.635110
-441.967764	-4.849143	7.645107
-440.387796	-1.052923	7.655104
-438.455738	-5.319294	7.665101
-435.999896	-13.235939	7.675098
-434.162149	-6.774732	7.685094
-432.708660	-4.702939	7.695091
-430.727201	-11.384942	7.705088
-428.801278	-6.134582	7.715085
-427.293544	-4.101447	7.725082
-425.434835	-1.041269	7.735078
-423.065706	-3.351759	7.745075
-421.212357	-8.000260	7.755072
-419.454655	-2.421465	7.765069
-417.691147	-3.152692	7.775066
-415.472436	-5.167591	7.785062
-413.641809	0.277993	7.795059
-412.271697	-4.484374	7.805056
-410.342940	-8.008134	7.815053
-408.096321	-1.893233	7.825050
-406.159057	-3.512673	7.835046
-404.628583	-0.005348	7.845043
-402.587395	2.694151	7.855040
-400.640234	-2.769797	7.865037
-399.049950	2.092111	7.875034
-396.958442	-0.262438	7.885030
-395.203667	4.129549	7.895027
-393.076610	1.911423	7.905024
-391.426862	8.702677	7.915021
-389.494798	4.316346	7.925018
-387.487723	-0.964539	7.935014
-385.706402	3.832139	7.945011
-384.021374	3.869740	7.955008
-381.945900	6.574835	7.965005
-379.918224	-5.237895	7.975002
-378.418336	3.427712	7.984998
-376.470861	6.619012	7.994995
-374.410619	-0.495509	8.004992
-372.767480	-6.607162	8.014989
-370.714238	-1.798634	8.024986
-368.569501	-6.912021	8.034982
-367.145962	2.452586	8.044979
-365.113811	-3.534875	8.054976
-363.165525	-2.492515	8.064973
-361.288509	-8.608349	8.074970
-359.583376	-4.236830	8.084966
-357.680882	-1.085699	8.094963
-355.815815	-7.357507	8.104960
-353.762556	-8.292837	8.114957
-351.801566	-10.307578	8.124954
-349.976487	-2.431201	8.134950
-347.957472	-4.038388	8.144947
-346.286743	-11.000694	8.154944
-344.660096	-8.740192	8.164941
-342.632603	0.218544	8.174938
-340.859909	-5.481169	8.184934
-338.767961	1.507923	8.194931
-336.723312	-3.128433	8.204928
-334.984772	-2.306757	8.214925
-333.216534	0.128506	8.224922
-331.460059	-2.864034	8.234918
-329.393309	-10.169017	8.244915
-327.457037	2.539868	8.254912
-325.695200	-10.910278	8.264909
-323.917496	4.342202	8.274906
-321.766153	-9.599579	8.284902
-319.978407	-2.124561	8.294899
-318.300967	4.583383	8.304896
-316.297322	-4.855603	8.314893
-314.507217	-0.840227	8.324890
-312.639179	1.590170	8.334886
-310.781667	1.620810	8.344883
-308.840833	1.713934	8.354880
-306.693550	0.432073	8.364877
-305.029390	-4.350342	8.374874
-303.276456	-0.171137	8.384870
-301.223256	5.153750	8.394867
-299.362629	8.070050	8.404864
-297.616274	2.718758	8.414861
-295.505136	4.991946	8.424858
-293.415117	2.535096	8.434854
-291.951833	0.757742	8.444851
-290.384363	-4.366049	8.454848
-288.390338	5.103319	8.464845
-286.262994	0.216972	8.474842
-284.426303	1.716135	8.484838
-282.322157	3.875193	8.494835
-280.530047	-7.918805	8.504832
-278.881150	8.481585	8.514829
-276.864489	1.089902	8.524826
-275.031672	4.984816	8.534822
-273.031803	1.055092	8.544819
-271.245019	-3.702669	8.554816
-269.410058	-4.162579	8.564813
-267.514590	-3.062764	8.574810
-265.778711	-2.927415	8.584807
-263.990984	-2.830339	8.594803
-261.705945	2.904390	8.604800
-260.007685	-4.840638	8.614797
-257.786062	-1.023566	8.624794
-256.542593	0.965028	8.634791
-254.456934	-8.649625	8.644787
-252.354328	-4.644613	8.654784
-250.585051	1.612958	8.664781
-248.964530	-0.959952	8.674778
-246.794127	-0.197674	8.684775
-245.100159	-4.823765	8.694771
-243.096620	-1.347636	8.704768
-240.839257	-9.538716	8.714765
-239.354877	0.552014	8.724762
-237.683731	2.440774	8.734759
-235.734054	-1.842466	8.744755
-233.773480	0.715320	8.754752
-231.759604	2.287288	8.764749
-230.323662	2.516326	8.774746
-228.216809	-1.771472	8.784743
-226.151266	-5.978467	8.794739
-224.296403	2.403236	8.804736
-222.319969	0.820316	8.814733
-220.646086	8.709890	8.824730
-218.815967	-2.954359	8.834727
-216.850024	4.124431	8.844723
-214.756724	-7.513928	8.854720
-212.968887	8.205959	8.864717
-211.565475	7.737609	8.874714
-209.469788	-2.480159	8.884711
-207.348660	-5.799220	8.894707
-205.304363	-1.848012	8.904704
-203.910629	-3.476852	8.914701
-201.959442	4.218483	8.924698
-199.983559	-8.283706	8.934695
-198.092992	1.783275	8.944691
-196.177290	0.800563	8.954688
-194.429211	-2.602624	8.964685
-192.465619	0.011555	8.974682
-190.477779	1.513507	8.984679
-188.609594	1.529907	8.994675
-187.029375	2.294859	9.004672
-184.983437	-5.570344	9.014669
-182.800103	-9.276659	9.024666
-181.092508	-11.197142	9.034663
-179.346040	-9.397727	9.044659
-177.532393	-5.043389	9.054656
-175.578288	-13.437052	9.064653
-173.605383	-17.139771	9.074650
-171.710932	-13.600386	9.084647
-170.215646	-11.467210	9.094643
-167.958044	-11.964496	9.104640
-166.004799	-13.930488	9.114637
-164.516768	-16.659028	9.124634
-162.407289	-12.261897	9.134631
-160.675348	-15.071990	9.144627
-158.563019	-22.262537	9.154624
-156.801112	-16.395279	9.164621
-155.354282	-11.769240	9.174618
-153.135401	-18.258409	9.184615
-151.169580	-16.847643	9.194611
-149.438785	-15.239905	9.204608
-147.300799	-16.840649	9.214605
-145.505516	-13.441724	9.224602
-143.818959	-22.021597	9.234599
-141.786941	-24.952190	9.244595
-139.889099	-20.938086	9.254592
-137.721975	-13.665562	9.264589
-136.070252	-22.099354	9.274586
-134.401005	-15.315764	9.284583
-132.593027	-14.921840	9.294579
-130.535851	-27.470094	9.304576
-128.964130	-17.669535	9.314573
-126.767914	-13.688821	9.324570
-124.915955	-17.162215	9.334567
-122.970852	-24.226579	9.344563
-121.159583	-17.530377	9.354560
-119.341259	-20.256336	9.364557
-117.347405	-16.347528	9.374554
-115.536574	-15.006732	9.384551
-113.725292	-13.083408	9.394547
-112.031015	-14.321231	9.404544
-109.855337	-13.166536	9.414541
-108.037895	-10.634752	9.424538
-105.926499	-13.890597	9.434535
-104.110138	-12.092806	9.444531
-102.422973	-17.099799	9.454528
-101.014646	-17.066793	9.464525
-98.752222	-20.594611	9.474522
-96.703901	-17.690735	9.484519
-94.802971	-13.673927	9.494515
-92.972054	-20.187976	9.504512
-91.207091	-16.373668	9.514509
-89.263458	-11.853697	9.524506
-87.131418	-13.999726	9.534503
-85.627964	-17.854828	9.544499
-83.703703	-8.416776	9.554496
-81.805174	-20.121840	9.564493
-79.621659	-14.110224	9.574490
-77.968804	-5.951944	9.584487
-76.320999	-12.217308	9.594483
-74.489377	-8.353624	9.604480
-72.597829	-3.138522	9.614477
-70.413537	-4.211356	9.624474
-68.451712	-12.045680	9.634471
-66.567245	-3.337008	9.644467
-64.982379	-6.136202	9.654464
-63.197764	-8.187309	9.664461
-61.156240	-10.104149	9.674458
-59.163706	0.840321	9.684455
-57.328427	-5.383896	9.694451
-55.632532	0.634499	9.704448
-53.518780	-7.362996	9.714445
-51.520416	-3.844824	9.724442
-49.833850	-0.774246	9.734439
-48.451810	-1.815377	9.744435
-46.135604	-0.690937	9.754432
-44.217488	-8.080928	9.764429
-42.650961	-2.337131	9.774426
-40.573945	-9.635635	9.784423
-38.627635	-12.939293	9.794419
-36.449086	-6.906314	9.804416
-34.855664	-8.601652	9.814413
-33.138812	-8.095226	9.824410
-31.139891	-7.404864	9.834407
-29.409666	-2.514496	9.844403
-27.192845	-8.779035	9.854400
-25.280709	-7.916937	9.864397
-23.465351	-10.268166	9.874394
-21.982543	-9.989643	9.884391
-19.941552	-8.893900	9.894387
-17.890286	-8.576595	9.904384
-16.181230	-9.433047	9.914381
-14.097250	-5.759565	9.924378
-12.337633	-11.884841	9.934375
-10.574012	-12.983665	9.944371
-8.593684	-8.174232	9.954368
-6.510023	-11.204530	9.964365
-5.045295	-4.129278	9.974362
-4.138374	24.850104	9.984359
-2.695955	69.452273	9.994355
-1.071632	126.009217	10.004352
0.000000	163.601633	10.009357
1.041642	194.821502	10.014362
1.592642	223.275041	10.019367
2.379849	244.842614	10.024371
2.637038	270.518945	10.029376
2.911383	278.793365	10.034381
2.840344	293.695296	10.039386
3.173535	292.584248	10.044391
3.290304	285.564489	10.049395
3.168619	304.793566	10.054400
3.560209	308.473210	10.059405
3.847961	314.846955	10.064410
3.907428	324.694711	10.069415
3.950445	325.104331	10.074419
3.658203	322.930893	10.079424
3.932108	325.739956	10.084429
3.603733	318.177786	10.089434
3.614064	328.837590	10.094439
4.101927	331.470605	10.099443
4.041080	343.201436	10.104448
4.442322	339.624329	10.109453
4.036473	329.171478	10.114458
4.187255	317.256381	10.119463
4.255854	326.768384	10.124467
4.162401	325.312252	10.129472
4.049982	323.136935	10.134477
4.701841	344.841362	10.139482
4.540723	329.314496	10.144487
4.680734	327.583012	10.149491
3.995451	326.919845	10.154496
4.346101	323.904296	10.159501
4.439738	329.843835	10.164506
4.558486	351.738966	10.169511
4.705270	348.336483	10.174515
4.255797	352.432567	10.179520
4.530221	354.456267	10.184525
4.824000	372.565802	10.189530
4.714672	373.070685	10.194535
4.924491	366.207924	10.199539
4.750339	372.882449	10.204544
4.718916	364.577480	10.209549
5.148216	368.810917	10.214554
5.011453	370.381418	10.219559
5.125774	374.439609	10.224563
4.902847	375.241721	10.229568
5.075067	373.801548	10.234573
5.087607	374.977665	10.239578
5.315915	376.921996	10.244583
5.461114	373.467723	10.249587
5.229382	377.790842	10.254592
5.431980	373.280363	10.259597
5.128861	380.218304	10.264602
5.204048	379.750777	10.269607
5.487877	376.118277	10.274611
5.025912	381.955664	10.279616
5.626953	388.618496	10.284621
5.418081	381.625407	10.289626
5.239477	383.998910	10.294631
5.625059	386.971513	10.299635
5.573336	389.788380	10.304640
5.846950	405.316661	10.309645
5.822588	399.812671	10.314650
5.765304	400.008068	10.319655
6.001139	406.503671	10.324659
5.862425	409.802755	10.329664
6.073312	408.689133	10.334669
6.075320	417.232572	10.339674
6.216375	418.831297	10.344679
5.898683	420.846963	10.349683
5.911107	432.017421	10.354688
6.210770	417.897655	10.359693
6.120159	428.087953	10.364698
5.997602	427.770236	10.369703
6.274132	420.472624	10.374707
6.316753	426.391957	10.379712
6.432457	416.081339	10.384717
6.813908	425.318006	10.389722
6.544829	424.859665	10.394727
6.670364	427.883220	10.399731
6.296324	428.135454	10.404736
6.598178	432.788193	10.409741
6.557817	439.252180	10.414746
6.397455	433.621645	10.419751
6.464256	423.768236	10.424755
6.512150	435.199532	10.429760
6.686378	442.991722	10.434765
7.256680	460.648842	10.439770
6.937775	462.043412	10.444775
7.432218	446.134312	10.449779
6.798894	451.406151	10.454784
7.063367	437.832853	10.459789
6.996783	441.073131	10.464794
7.273871	451.341979	10.469799
7.432587	454.412285	10.474803
6.995560	450.683455	10.479808
7.469040	459.172208	10.484813
7.457034	461.948063	10.489818
7.105181	476.443986	10.494823
7.573058	470.104538	10.499827
7.321466	476.285282	10.504832
7.514811	493.162090	10.509837
7.496883	476.681855	10.514842
7.497774	482.008648	10.519847
7.876493	478.208028	10.524851
7.637567	483.607768	10.529856
7.669182	466.928837	10.534861
7.487632	499.536625	10.539866
7.801655	474.708967	10.544871
7.844975	482.025339	10.549875
7.642379	491.290563	10.554880
7.810122	477.000979	10.559885
7.988634	483.215613	10.564890
8.082876	478.425929	10.569895
8.071009	478.535237	10.574899
8.086907	485.671488	10.579904
8.010528	492.705773	10.584909
7.978260	489.361780	10.589914
8.105719	491.926166	10.594919
8.228206	499.568950	10.599923
8.196503	515.007286	10.604928
8.335661	519.482587	10.609933
8.498886	519.404698	10.614938
8.366128	524.721287	10.619943
8.483938	518.587467	10.624947
8.385642	522.007857	10.629952
8.396570	539.128277	10.634957
8.552009	526.300817	10.639962
8.819555	525.260147	10.644967
9.060056	516.102764	10.649971
8.607539	529.698620	10.654976
8.588653	529.397477	10.659981
8.875459	531.084925	10.664986
8.767733	524.247514	10.669991
8.781452	538.366649	10.674995
8.568589	531.274779	10.680000
9.002906	535.288277	10.685005
8.969602	533.515032	10.690010
8.646907	549.237936	10.695015
9.055442	544.450132	10.700019
9.194935	569.284782	10.705024
9.630524	568.920602	10.710029
9.402554	568.760040	10.715034
9.488417	565.621107	10.720039
9.588278	558.454107	10.725043
9.019386	571.636495	10.730048
9.243295	576.574520	10.735053
9.226237	577.186112	10.740058
9.357712	573.667751	10.745063
9.602752	572.362594	10.750067
9.547391	579.461375	10.755072
9.365712	580.348379	10.760077
9.688133	573.488058	10.765082
9.142145	580.195185	10.770087
9.417746	589.043578	10.775091
9.551103	605.993164	10.780096
9.873305	609.283421	10.785101
9.753340	614.851885	10.790106
9.571500	606.163929	10.795111
10.128819	615.282780	10.800115
9.850397	621.605055	10.805120
10.003311	616.288741	10.810125
10.069768	620.460289	10.815130
10.235499	639.907306	10.820135
10.271694	643.292079	10.825139
10.308922	651.248157	10.830144
10.264733	651.236469	10.835149
10.205510	647.004208	10.840154
10.105428	645.765136	10.845159
10.410888	651.104906	10.850163
10.214046	652.872673	10.855168
10.392650	663.862264	10.860173
10.301539	655.169266	10.865178
10.267089	657.584471	10.870183
10.444538	660.505180	10.875187
10.750245	669.154859	10.880192
11.021030	677.939421	10.885197
11.014538	678.497294	10.890202
10.741214	686.912929	10.895207
11.022897	689.004904	10.900211
11.133381	685.382634	10.905216
11.316868	682.838368	10.910221
10.943323	679.865732	10.915226
10.863713	678.292240	10.920231
11.120731	682.162179	10.925235
10.955291	687.898770	10.930240
11.444391	681.335079	10.935245
11.264417	693.137234	10.940250
10.955589	691.523036	10.945255
11.210256	686.682463	10.950259
11.351952	689.772880	10.955264
11.428583	690.803184	10.960269
11.068378	695.847042	10.965274
11.024109	695.956790	10.970279
11.311175	689.893667	10.975283
11.836991	713.616712	10.980288
11.783421	705.726655	10.985293
11.413069	708.958680	10.990298
11.536116	718.213102	10.995303
11.623717	729.625682	11.000307
11.962731	733.225516	11.005312
11.926891	729.155077	11.010317
11.735676	739.577680	11.015322
11.932769	732.374585	11.020327
12.218882	741.260818	11.025331
11.810894	740.148124	11.030336
11.816497	729.742886	11.035341
11.831388	737.177459	11.040346
11.266570	746.628358	11.045351
11.782554	755.790161	11.050355
11.867224	756.915380	11.055360
12.304900	749.719630	11.060365
12.282532	762.058085	11.065370
12.409301	766.902863	11.070375
12.629697	758.760921	11.075379
12.267633	771.524149	11.080384
12.159324	770.475611	11.085389
12.328840	773.146876	11.090394
12.206750	775.793697	11.095399
12.590056	784.702299	11.100403
12.677483	801.288862	11.105408
12.798725	803.460063	11.110413
12.624012	809.743799	11.115418
12.927708	806.718296	11.120423
12.945428	806.184230	11.125427
12.730533	820.571917	11.130432
13.117046	813.576683	11.135437
13.161570	801.887870	11.140442
13.093340	807.616886	11.145447
13.205066	810.707379	11.150451
13.105308	810.201515	11.155456
13.045578	807.960949	11.160461
12.888477	818.242552	11.165466
12.929894	816.170351	11.170471
13.234957	811.075697	11.175475
13.320159	808.941321	11.180480
13.402134	810.469091	11.185485
13.141311	817.118222	11.190490
13.269181	839.933564	11.195495
13.541352	835.580576	11.200499
13.758374	838.690548	11.205504
13.595640	832.957734	11.210509
13.585382	844.130551	11.215514
13.579071	832.140744	11.220519
13.780987	831.135754	11.225523
13.531206	840.692574	11.230528
13.699343	849.137228	11.235533
13.888332	838.262694	11.240538
14.104514	840.191677	11.245543
14.063810	847.173134	11.250547
13.940390	845.696498	11.255552
13.820879	848.117419	11.260557
13.980566	850.954268	11.265562
13.965436	844.961363	11.270567
13.951158	849.951670	11.275571
13.723437	875.178154	11.280576
14.020159	881.497104	11.285581
14.108319	878.562739	11.290586
14.175587	880.282095	11.295591
14.462749	871.629550	11.300595
14.586114	876.724064	11.305600
14.438645	879.773917	11.310605
14.309806	887.734539	11.315610
14.700154	877.390822	11.320615
14.532909	874.809432	11.325619
14.527963	880.388035	11.330624
14.650112	886.097752	11.335629
14.814899	895.940136	11.340634
14.704135	920.700191	11.345639
14.792804	915.767752	11.350643
14.848738	908.885128	11.355648
15.033051	913.689238	11.360653
14.994936	919.202184	11.365658
14.882018	922.677040	11.370663
15.212555	913.359966	11.375667
15.273885	919.166130	11.380672
15.269641	916.317459	11.385677
15.274930	911.298974	11.390682
15.121711	913.239585	11.395687
15.306910	905.655105	11.400691
15.160409	915.827853	11.405696
15.201876	918.590534	11.410701
15.007192	923.215408	11.415706
14.841832	926.369049	11.420711
15.292475	936.364556	11.425715
15.200249	961.265225	11.430720
15.480662	957.932748	11.435725
15.758005	956.797446	11.440730
15.818063	959.621824	11.445735
15.904758	957.682730	11.450739
15.825568	961.604798	11.455744
15.797120	958.607016	11.460749
15.776707	963.073217	11.465754
15.903758	968.722261	11.470759
15.776515	957.079646	11.475763
15.771443	965.304417	11.480768
16.089144	955.800131	11.485773
16.340679	954.492328	11.490778
15.667622	959.758069	11.495783
16.112520	953.914087	11.500787
16.149503	968.381589	11.505792
16.149019	958.607936	11.510797
16.388925	968.783738	11.515802
15.748733	968.439769	11.520807
16.396599	968.055913	11.525811
16.410104	996.002208	11.530816
16.497333	990.798737	11.535821
16.687428	990.528904	11.540826
16.487411	999.548035	11.545831
16.725400	984.398347	11.550835
16.713729	990.348648	11.555840
16.649191	989.253688	11.560845
16.550159	998.690371	11.565850
16.430305	999.171722	11.570855
16.897562	991.367163	11.575859
16.842129	987.523704	11.580864
16.672578	997.023674	11.585869
16.579127	1002.912908	11.590874
16.442754	1005.103156	11.595879
16.679793	1013.486453	11.600883
16.990641	1029.097775	11.605888
17.325484	1030.446460	11.610893
17.278037	1031.685816	11.615898
16.815635	1035.667455	11.620903
17.472349	1020.659095	11.625907
17.031904	1025.737942	11.630912
17.086864	1037.515517	11.635917
17.336622	1022.947385	11.640922
17.615976	1029.817951	11.645927
17.453196	1026.601886	11.650931
17.168042	1028.372746	11.655936
17.513919	1035.098663	11.660941
17.727397	1036.223857	11.665946
17.239804	1045.230542	11.670951
17.724416	1050.412573	11.675955
17.471308	1060.088340	11.680960
17.773868	1060.029224	11.685965
17.904914	1060.855332	11.690970
17.722290	1075.432089	11.695975
17.453728	1065.563931	11.700979
17.365966	1065.289534	11.705984
17.587744	1068.567531	11.710989
17.990144	1074.344582	11.715994
18.079373	1096.799062	11.720999
18.377325	1096.359057	11.726003
18.204584	1105.779182	11.731008
18.014841	1099.228973	11.736013
18.416246	1105.288471	11.741018
18.329173	1107.650644	11.746023
18.458100	1100.642745	11.751027
18.190027	1112.124978	11.756032
18.292601	1105.766258	11.761037
18.315655	1108.199174	11.766042
18.203863	1107.509136	11.771047
18.605686	1103.118041	11.776051
18.658985	1110.048359	11.781056
18.439828	1107.558787	11.786061
18.718850	1095.296165	11.791066
18.212478	1120.477637	11.796071
18.910461	1117.822842	11.801075
18.765072	1139.807031	11.806080
18.644302	1142.899988	11.811085
18.893844	1133.573617	11.816090
18.751472	1141.165949	11.821095
19.064629	1139.785222	11.826099
18.897239	1148.460193	11.831104
19.007239	1149.264433	11.836109
18.840918	1141.590822	11.841114
19.184307	1145.956469	11.846119
19.495013	1143.379215	11.851123
19.387877	1135.634665	11.856128
19.281180	1153.000079	11.861133
19.388907	1143.745209	11.866138
19.373871	1146.201553	11.871143
19.387025	1148.904139	11.876147
19.247207	1145.261757	11.881152
19.527638	1145.597259	11.886157
19.670111	1165.936526	11.891162
19.647711	1186.913985	11.896167
19.975853	1168.967948	11.901171
19.787858	1164.674073	11.906176
19.951722	1152.603239	11.911181
19.738567	1141.015181	11.916186
19.703769	1164.822087	11.921191
19.978749	1164.825719	11.926195
20.030654	1173.869428	11.931200
20.028461	1177.731963	11.936205
20.122848	1178.871435	11.941210
20.228568	1175.114185	11.946215
20.009506	1173.703233	11.951219
20.020960	1183.891973	11.956224
20.245878	1172.599869	11.961229
20.254525	1174.768586	11.966234
20.454466	1179.226512	11.971239
20.239128	1172.172568	11.976243
20.362172	1174.080184	11.981248
20.382572	1173.170358	11.986253
20.226078	1181.291671	11.991258
19.892128	1184.566878	11.996263
20.206635	1175.007765	12.001267
20.218535	1177.155463	12.006272
20.792628	1202.661472	12.011277
20.743713	1199.987031	12.016282
20.502963	1186.020534	12.021287
20.819194	1203.309083	12.026291
20.798662	1185.860196	12.031296
20.906425	1177.780142	12.036301
20.817356	1181.937237	12.041306
20.692388	1176.658737	12.046311
20.828307	1167.651670	12.051315
20.458288	1175.250370	12.056320
20.466487	1175.641914	12.061325
20.840709	1168.892902	12.066330
20.285788	1178.017642	12.071335
20.620240	1172.607511	12.076339
20.584298	1180.961910	12.081344
20.646762	1176.462498	12.086349
20.832885	1176.082907	12.091354
20.298371	1186.201042	12.096359
20.871451	1183.783781	12.101363
20.627020	1187.667613	12.106368
20.489991	1181.025378	12.111373
20.889516	1186.263610	12.116378
20.829035	1180.246262	12.121383
20.752928	1175.809955	12.126387
20.607860	1183.803290	12.131392
20.711652	1181.740012	12.136397
20.773985	1183.575310	12.141402
20.496216	1186.420505	12.146407
20.806465	1180.859689	12.151411
20.552987	1187.405313	12.156416
20.671136	1183.228180	12.161421
20.708299	1182.695730	12.166426
20.677025	1183.976674	12.171431
20.914767	1180.259864	12.176435
20.653695	1190.946249	12.181440
20.693597	1183.809007	12.186445
20.861717	1183.701950	12.191450
20.604769	1185.685951	12.196455
20.740879	1176.388685	12.201459
20.686800	1181.538421	12.206464
20.535876	1187.356472	12.211469
20.878814	1180.136200	12.216474
20.554039	1189.148540	12.221479
20.768017	1188.296146	12.226483
20.766337	1187.698928	12.231488
20.692567	1185.859517	12.236493
20.764181	1185.908205	12.241498
20.369504	1190.363212	12.246503
20.751588	1181.520299	12.251507
20.922805	1186.541057	12.256512
20.702228	1193.560835	12.261517
21.017608	1191.272990	12.266522
20.993129	1183.486844	12.271527
20.936068	1180.879938	12.276531
20.432935	1176.590596	12.281536
20.173294	1181.429342	12.286541
20.903537	1176.553748	12.291546
20.859708	1189.493662	12.296551
20.783450	1190.196725	12.301555
20.474678	1192.144839	12.306560
20.570040	1186.897422	12.311565
20.803487	1188.460996	12.316570
20.792999	1202.436404	12.321575
21.055722	1179.282587	12.326579
20.657364	1163.535622	12.331584
20.912296	1163.231789	12.336589
21.043589	1151.415312	12.341594
20.621243	1167.104315	12.346599
20.646075	1154.569950	12.351603
21.055167	1161.268495	12.356608
20.860181	1156.518417	12.361613
20.786750	1161.529305	12.366618
20.916601	1160.490057	12.371623
20.748565	1157.866164	12.376627
20.585631	1163.470077	12.381632
20.937846	1159.378618	12.386637
21.018599	1166.446511	12.391642
20.625697	1154.708917	12.396647
20.676832	1150.190820	12.401651
21.053306	1141.257362	12.406656
21.161594	1138.520008	12.411661
20.890423	1144.868161	12.416666
20.669262	1142.954495	12.421671
20.689658	1140.822523	12.426675
20.745578	1140.101000	12.431680
20.687845	1137.284473	12.436685
20.842865	1132.476995	12.441690
20.720411	1145.484605	12.446695
20.692965	1139.739550	12.451699
20.718968	1137.702879	12.456704
20.539748	1137.297988	12.461709
21.012426	1136.029012	12.466714
20.717341	1152.836268	12.471719
20.824607	1139.370972	12.476723
20.679515	1143.718344	12.481728
20.610416	1139.711442	12.486733
20.870472	1139.007820	12.491738
20.517051	1144.780884	12.496743
20.818865	1137.269146	12.501747
20.629826	1146.830671	12.506752
20.633425	1132.098267	12.511757
20.920758	1140.391613	12.516762
20.855686	1145.011651	12.521767
20.680209	1126.660295	12.526771
20.410625	1122.013592	12.531776
20.541548	1124.257415	12.536781
20.717045	1117.883904	12.541786
20.689597	1137.917496	12.546791
20.474107	1134.776048	12.551795
20.842559	1145.360404	12.556800
20.431177	1148.121247	12.561805
20.703390	1132.680515	12.566810
20.559884	1137.079672	12.571815
20.918515	1151.497626	12.576819
20.798447	1131.429570	12.581824
20.497585	1133.669729	12.586829
20.658222	1122.805813	12.591834
20.938922	1136.239542	12.596839
21.030560	1119.450937	12.601843
20.942445	1127.070877	12.606848
20.682364	1115.390977	12.611853
21.056045	1118.051817	12.616858
20.736005	1110.070004	12.621863
20.701876	1109.541044	12.626867
20.916979	1109.439108	12.631872
20.871530	1105.195053	12.636877
21.015686	1109.483660	12.641882
20.689624	1105.714877	12.646887
20.677694	1115.738565	12.651891
20.576237	1123.936223	12.656896
20.721148	1124.626082	12.661901
20.780761	1114.626693	12.666906
20.565343	1128.560602	12.671911
20.710552	1111.613649	12.676915
21.025125	1109.321215	12.681920
20.549902	1098.341125	12.686925
20.602238	1093.229917	12.691930
20.788858	1084.732056	12.696935
20.801874	1075.370912	12.701939
20.666677	1094.183719	12.706944
20.672624	1080.802448	12.711949
20.726825	1076.548814	12.716954
20.460564	1079.141416	12.721959
20.476801	1078.402572	12.726963
20.381607	1091.839450	12.731968
20.324939	1105.820554	12.736973
20.736118	1101.990943	12.741978
20.703030	1109.704598	12.746983
20.835165	1110.112641	12.751987
20.837363	1115.914123	12.756992
20.621764	1111.711401	12.761997
20.944947	1106.191128	12.767002
20.704550	1095.372279	12.772007
20.676300	1084.707256	12.777011
20.931925	1088.263713	12.782016
20.629453	1091.713651	12.787021
20.550313	1079.599638	12.792026
20.614953	1079.166888	12.797031
20.666085	1085.700147	12.802035
20.730398	1090.674846	12.807040
20.479525	1095.728209	12.812045
20.527621	1085.995607	12.817050
20.466317	1095.954616	12.822055
20.458850	1104.126232	12.827059
20.727452	1119.932050	12.832064
20.714759	1117.609816	12.837069
21.035309	1120.988766	12.842074
20.331106	1099.764976	12.847079
20.604165	1096.542451	12.852083
20.839486	1114.905096	12.857088
20.510768	1107.798306	12.862093
20.434024	1104.327224	12.867098
20.361385	1122.868314	12.872103
20.423717	1129.615850	12.877107
20.435444	1122.207163	12.882112
20.312468	1126.186723	12.887117
20.667516	1121.482960	12.892122
20.543458	1132.011827	12.897127
20.911779	1125.609131	12.902131
20.742327	1131.269265	12.907136
20.399775	1140.213448	12.912141
20.881782	1124.808645	12.917146
20.826918	1133.602854	12.922151
20.737835	1129.189133	12.927155
20.676993	1133.537255	12.932160
20.777894	1138.309013	12.937165
20.735245	1131.050922	12.942170
21.012906	1126.995019	12.947175
20.924901	1131.994029	12.952179
20.729384	1124.366085	12.957184
20.768513	1109.807811	12.962189
20.689643	1103.421264	12.967194
19.954439	1105.850553	12.972199
20.644727	1119.775599	12.977203
20.934887	1127.467663	12.982208
20.631938	1121.821756	12.987213
20.804454	1135.920874	12.992218
20.615560	1137.897167	12.997223
20.857678	1125.094776	13.002227
20.593799	1110.576950	13.007232
20.474315	1110.492116	13.012237
20.942508	1120.928079	13.017242
20.665357	1108.107609	13.022247
20.426443	1110.998631	13.027251
20.662296	1106.460544	13.032256
20.713072	1115.988525	13.037261
20.773664	1120.462353	13.042266
20.541015	1111.406879	13.047271
20.433494	1109.153390	13.052275
20.545055	1130.913651	13.057280
20.769317	1130.436514	13.062285
20.927619	1131.702983	13.067290
20.546518	1129.089427	13.072295
20.575968	1115.694914	13.077299
20.547149	1119.394523	13.082304
20.761747	1134.786345	13.087309
20.395967	1144.555834	13.092314
20.851530	1139.758761	13.097319
21.014065	1135.839491	13.102323
20.658206	1114.620039	13.107328
20.529238	1116.630925	13.112333
20.741763	1109.387335	13.117338
20.382816	1113.713617	13.122343
20.650650	1133.138703	13.127347
20.862733	1136.385146	13.132352
20.388194	1129.279529	13.137357
20.738727	1135.099572	13.142362
20.705121	1137.459528	13.147367
21.051377	1128.895177	13.152371
20.617768	1118.690608	13.157376
20.575047	1117.677313	13.162381
20.919253	1102.398595	13.167386
20.668667	1107.016674	13.172391
20.459152	1115.690461	13.177395
20.841960	1110.658996	13.182400
20.530234	1114.629237	13.187405
20.737423	1106.878717	13.192410
20.522755	1117.221753	13.197415
20.617962	1112.209355	13.202419
20.747676	1107.692929	13.207424
20.382409	1120.368663	13.212429
20.617815	1107.914290	13.217434
20.775836	1124.335421	13.222439
20.712615	1113.877807	13.227443
20.697286	1115.550442	13.232448
20.532182	1108.485362	13.237453
20.782616	1103.949681	13.242458
20.692972	1106.521999	13.247463
20.714990	1116.661698	13.252467
20.959279	1107.933851	13.257472
20.481807	1118.774551	13.262477
21.058897	1107.825292	13.267482
21.055131	1109.161766	13.272487
20.810326	1114.841798	13.277491
20.675746	1110.626152	13.282496
20.445839	1113.372234	13.287501
20.667375	1113.341813	13.292506
20.706897	1112.917799	13.297511
20.627911	1110.390098	13.302515
20.627019	1113.508082	13.307520
20.489176	1117.918945	13.312525
20.679331	1117.565521	13.317530
20.590952	1125.587628	13.322535
20.683026	1115.502635	13.327539
21.023855	1124.979624	13.332544
21.078506	1110.223329	13.337549
21.063305	1110.473523	13.342554
20.918466	1124.257397	13.347559
20.719097	1102.826917	13.352563
20.789006	1083.365716	13.357568
20.252196	1095.737630	13.362573
20.767564	1093.611866	13.367578
20.821977	1109.902850	13.372583
20.309165	1095.733832	13.377587
20.626366	1099.275738	13.382592
20.646844	1112.976460	13.387597
20.629599	1116.324136	13.392602
20.218011	1120.627278	13.397607
20.532051	1122.821390	13.402611
20.703885	1113.403347	13.407616
20.677951	1128.688451	13.412621
20.732220	1120.650078	13.417626
20.721560	1129.976555	13.422631
20.235019	1122.645772	13.427635
20.543204	1121.436152	13.432640
20.463933	1129.160339	13.437645
20.445767	1119.173354	13.442650
20.567458	1121.904354	13.447655
20.199757	1125.993915	13.452659
20.639038	1124.998351	13.457664
20.368347	1133.077929	13.462669
20.852936	1127.262240	13.467674
20.786770	1133.541416	13.472679
20.804640	1124.188928	13.477683
20.811717	1122.598405	13.482688
20.597935	1135.281527	13.487693
21.092965	1128.376066	13.492698
20.582728	1128.716265	13.497703
20.813831	1125.237073	13.502707
20.889406	1121.740113	13.507712
20.656906	1129.641708	13.512717
20.739362	1134.129400	13.517722
20.693185	1123.623327	13.522727
20.669940	1129.925618	13.527731
20.569438	1126.855715	13.532736
20.551715	1132.155754	13.537741
20.730725	1124.140059	13.542746
20.949779	1135.235520	13.547751
20.809999	1131.533211	13.552755
21.006083	1132.017787	13.557760
20.476608	1130.820360	13.562765
20.764383	1131.077418	13.567770
20.645971	1137.961023	13.572775
20.623413	1135.856405	13.577779
20.869921	1129.903649	13.582784
20.745739	1127.116647	13.587789
20.993159	1117.328574	13.592794
20.501455	1111.681241	13.597799
20.353389	1105.805629	13.602803
20.746164	1106.539527	13.607808
20.429876	1122.332990	13.612813
20.874741	1130.061880	13.617818
20.729627	1133.215489	13.622823
20.877805	1121.590310	13.627827
20.888921	1108.969862	13.632832
20.134497	1107.379386	13.637837
20.638750	1103.681585	13.642842
20.688260	1120.036441	13.647847
20.742859	1126.226964	13.652851
20.868054	1106.463597	13.657856
20.419853	1104.868429	13.662861
20.433005	1111.256369	13.667866
20.648335	1131.677007	13.672871
20.569779	1132.178583	13.677875
20.655010	1132.461642	13.682880
20.538706	1138.606892	13.687885
21.016696	1136.652665	13.692890
20.890780	1141.403834	13.697895
20.479876	1116.438404	13.702899
21.011735	1106.511925	13.707904
20.624584	1110.610892	13.712909
20.719424	1107.382099	13.717914
20.455552	1108.810527	13.722919
20.579308	1107.184047	13.727923
20.745944	1108.097522	13.732928
20.418351	1110.334057	13.737933
20.853664	1098.167928	13.742938
20.554410	1110.244917	13.747943
20.628403	1104.234535	13.752947
20.768153	1099.241845	13.757952
20.584622	1106.594718	13.762957
21.012208	1106.137188	13.767962
20.619565	1109.965793	13.772967
20.748694	1102.653508	13.777971
20.409057	1105.954836	13.782976
20.528125	1111.430166	13.787981
20.679690	1103.265895	13.792986
21.098618	1102.424968	13.797991
20.563131	1122.610543	13.802995
20.515475	1105.754286	13.808000
20.521124	1111.236670	13.813005
20.678840	1101.115985	13.818010
20.660720	1115.608194	13.823015
20.697526	1113.161370	13.828019
21.072208	1095.893977	13.833024
20.743607	1118.068209	13.838029
20.795737	1102.222643	13.843034
20.479490	1111.817051	13.848039
20.711651	1109.189254	13.853043
20.920558	1108.654643	13.858048
20.723393	1119.482169	13.863053
20.758581	1115.803994	13.868058
20.748269	1117.239285	13.873063
20.567873	1106.341471	13.878067
20.879483	1113.445053	13.883072
20.529083	1108.503738	13.888077
20.879777	1112.852441	13.893082
20.542727	1104.868613	13.898087
20.554448	1099.923153	13.903091
20.730963	1112.872006	13.908096
20.501206	1108.026565	13.913101
20.872991	1103.739610	13.918106
20.387861	1106.546903	13.923111
20.470339	1108.544560	13.928115
20.771632	1107.958941	13.933120
20.323614	1120.816610	13.938125
20.624996	1113.959393	13.943130
20.789804	1112.731644	13.948135
20.675616	1113.215248	13.953139
20.689770	1099.674955	13.958144
20.722244	1118.520972	13.963149
20.806985	1108.498656	13.968154
20.651896	1119.401473	13.973159
20.572723	1115.929199	13.978163
20.764109	1110.027823	13.983168
20.364216	1116.251415	13.988173
20.723318	1104.176286	13.993178
20.647383	1115.437060	13.998183
20.474237	1109.511830	14.003187
20.688502	1108.222575	14.008192
20.878978	1119.703691	14.013210
20.884832	1108.933021	14.018227
20.579413	1124.140355	14.023245
20.149322	1115.216644	14.028263
20.839410	1113.283713	14.033280
20.708543	1112.552910	14.038298
20.719088	1110.589958	14.043315
20.884273	1119.186654	14.048333
20.910247	1112.211425	14.053351
21.156445	1114.371310	14.058368
20.666906	1118.386655	14.063386
20.933657	1107.767841	14.068403
20.812740	1112.775108	14.073421
20.808562	1112.307225	14.078439
20.950783	1117.742829	14.083456
20.249041	1118.839614	14.088474
20.582583	1123.330823	14.093491
20.686669	1129.005309	14.098509
20.892304	1148.547969	14.103527
21.255485	1154.657738	14.108544
20.505488	1161.528640	14.113562
20.940448	1154.376473	14.118579
20.985734	1174.459098	14.123597
20.864578	1163.911558	14.128615
21.261066	1151.387628	14.133632
21.160006	1164.261188	14.138650
21.164630	1152.905546	14.143667
21.102017	1152.824490	14.148685
20.932575	1157.894566	14.153703
21.269045	1164.074663	14.158720
21.039909	1172.663509	14.163738
21.036181	1149.475929	14.168755
21.323108	1164.607692	14.173773
21.173163	1167.071436	14.178791
21.212678	1165.291037	14.183808
20.893321	1164.886011	14.188826
21.084418	1164.828975	14.193843
20.974167	1162.245096	14.198861
20.985873	1176.889118	14.203879
21.210484	1178.698543	14.208896
21.536546	1192.078121	14.213914
21.640168	1193.559226	14.218931
21.501839	1189.441477	14.223949
21.252883	1198.676835	14.228967
21.968411	1190.039074	14.233984
21.550069	1189.019085	14.239002
21.478404	1176.942599	14.244019
21.391476	1167.179216	14.249037
21.156803	1168.242397	14.254055
21.689786	1179.080108	14.259072
21.578945	1187.182926	14.264090
21.724433	1197.465866	14.269107
21.748800	1188.029192	14.274125
21.159783	1181.156749	14.279143
21.505175	1183.612264	14.284160
21.385665	1186.486415	14.289178
21.346025	1201.794573	14.294195
21.462320	1191.419911	14.299213
21.221100	1197.504991	14.304231
21.644448	1199.380240	14.309248
21.400236	1195.306120	14.314266
21.709203	1184.391093	14.319283
21.682450	1191.192257	14.324301
21.549568	1199.635209	14.329319
21.834538	1210.388242	14.334336
22.041309	1218.416820	14.339354
21.773297	1213.673268	14.344371
21.731593	1212.519269	14.349389
21.515544	1228.214226	14.354407
21.824916	1216.685660	14.359424
21.634626	1225.183400	14.364442
21.672312	1227.398584	14.369459
21.727689	1232.192162	14.374477
21.768883	1235.213713	14.379495
22.023728	1227.945529	14.384512
21.783553	1236.119340	14.389530
21.744301	1231.249633	14.394547
22.114586	1235.170325	14.399565
22.162803	1232.447903	14.404583
21.894353	1238.161408	14.409600
21.560099	1233.390665	14.414618
21.534042	1245.259799	14.419635
22.039343	1260.089426	14.424653
21.881809	1261.807242	14.429671
21.924256	1265.377561	14.434688
22.037830	1253.005634	14.439706
22.133755	1267.373630	14.444723
22.331674	1264.330034	14.449741
22.119126	1263.698764	14.454759
22.215928	1255.924117	14.459776
21.974794	1265.549936	14.464794
22.486020	1266.508299	14.469811
22.759149	1267.045339	14.474829
22.289682	1262.676809	14.479847
22.419661	1257.281471	14.484864
22.432585	1267.631222	14.489882
22.451632	1266.253606	14.494899
22.574095	1263.676631	14.499917
22.579676	1264.338142	14.504935
22.720676	1263.057472	14.509952
22.320194	1259.458125	14.514970
22.306632	1271.984357	14.519987
22.800841	1263.221415	14.525005
22.394232	1270.130396	14.530023
22.581484	1258.762843	14.535040
22.737833	1257.487589	14.540058
22.595127	1266.120902	14.545075
22.556542	1261.466573	14.550093
22.571299	1262.917818	14.555111
22.696260	1257.778099	14.560128
22.658196	1262.128862	14.565146
22.663145	1263.748404	14.570163
23.020504	1245.629339	14.575181
22.551479	1256.507397	14.580199
22.607392	1265.385867	14.585216
22.809432	1264.669590	14.590234
22.962239	1281.005732	14.595251
23.060672	1271.985033	14.600269
22.663428	1268.377304	14.605287
22.947632	1254.582945	14.610304
22.862797	1266.132724	14.615322
22.930099	1266.326660	14.620339
23.174810	1259.725437	14.625357
22.786335	1267.315761	14.630375
22.806947	1263.569022	14.635392
23.006568	1266.518119	14.640410
23.156614	1287.037202	14.645427
23.328550	1284.184928	14.650445
23.130371	1270.351103	14.655463
23.322481	1257.744857	14.660480
23.325468	1253.766562	14.665498
23.080411	1270.557824	14.670515
23.338968	1252.772247	14.675533
23.177022	1261.172683	14.680551
22.969768	1263.538624	14.685568
23.473136	1265.388534	14.690586
23.151848	1265.452554	14.695603
23.187371	1258.702237	14.700621
23.158951	1270.477391	14.705639
23.160674	1261.069449	14.710656
23.119390	1260.503665	14.715674
23.263531	1265.482860	14.720691
23.584304	1250.153759	14.725709
23.382541	1257.665532	14.730727
23.243531	1260.698531	14.735744
23.168854	1258.082220	14.740762
23.161757	1263.261710	14.745779
23.639833	1291.190581	14.750797
23.372350	1292.985712	14.755815
23.410173	1291.320393	14.760832
23.553623	1290.001578	14.765850
23.408028	1298.114722	14.770867
23.646255	1296.441029	14.775885
23.465605	1295.225820	14.780903
23.449375	1294.654466	14.785920
23.964143	1289.029430	14.790938
23.575043	1297.563644	14.795955
23.874160	1297.906212	14.800973
23.634807	1298.707464	14.805991
23.612943	1294.427968	14.811008
24.104106	1292.735951	14.816026
23.809516	1295.197622	14.821043
24.034746	1265.469147	14.826061
23.617388	1262.948394	14.831079
23.383572	1268.827839	14.836096
23.395809	1283.891864	14.841114
23.483591	1306.926630	14.846131
23.603235	1300.049623	14.851149
23.360791	1307.983173	14.856167
23.620937	1307.381889	14.861184
23.959326	1295.971322	14.866202
23.913902	1305.350453	14.871219
23.717986	1296.656678	14.876237
23.778487	1301.034200	14.881255
23.837460	1306.502030	14.886272
24.015851	1313.460856	14.891290
23.873922	1323.363459	14.896307
24.359835	1322.281012	14.901325
24.227082	1328.075150	14.906343
24.242970	1311.896454	14.911360
23.958177	1304.412303	14.916378
23.818651	1303.328955	14.921395
24.289308	1314.341870	14.926413
24.453903	1328.736724	14.931431
23.940670	1315.988120	14.936448
24.333549	1306.497305	14.941466
24.326575	1327.406419	14.946483
24.220996	1320.187817	14.951501
24.382440	1332.009810	14.956519
24.282500	1324.817046	14.961536
24.475479	1319.468263	14.966554
24.368389	1325.557168	14.971571
24.407407	1331.877591	14.976589
24.224141	1319.932041	14.981607
24.265268	1335.299812	14.986624
24.047871	1332.217062	14.991642
24.214057	1336.853005	14.996659
24.618129	1333.667976	15.001677
24.522962	1327.814615	15.006695
24.871875	1343.314189	15.011712
24.645266	1334.596974	15.016730
24.435673	1336.829598	15.021747
24.528848	1334.554572	15.026765
24.673920	1338.125841	15.031783
24.483512	1328.430764	15.036800
24.673799	1334.506843	15.041818
24.937002	1334.174046	15.046835
24.971037	1334.574629	15.051853
24.593952	1331.021867	15.056871
24.489647	1331.667877	15.061888
24.926193	1329.478074	15.066906
24.674174	1338.448178	15.071923
24.714666	1331.516144	15.076941
24.608693	1323.668417	15.081959
24.561547	1335.657389	15.086976
24.564744	1337.483277	15.091994
24.245182	1344.722887	15.097011
24.602539	1340.080878	15.102029
24.644522	1366.394811	15.107047
24.337756	1366.489547	15.112064
24.874341	1365.768662	15.117082
24.523758	1373.483552	15.122099
24.908653	1372.420362	15.127117
25.070912	1379.336177	15.132135
24.855671	1377.881096	15.137152
25.017515	1369.509295	15.142170
24.995937	1378.264920	15.147187
25.192475	1373.645407	15.152205
24.925699	1371.916985	15.157223
24.936151	1395.807339	15.162240
25.600198	1388.066403	15.167258
25.306261	1377.289874	15.172275
25.223999	1375.145069	15.177293
25.314341	1379.610660	15.182311
25.119114	1378.440240	15.187328
25.365896	1371.155968	15.192346
25.214076	1394.818956	15.197363
25.314949	1401.694239	15.202381
25.976021	1387.444823	15.207399
25.547657	1394.244079	15.212416
25.876100	1379.544380	15.217434
25.794952	1380.608254	15.222451
25.585482	1377.755455	15.227469
25.705780	1362.544727	15.232487
25.465241	1371.259773	15.237504
25.686279	1360.128988	15.242522
25.327301	1371.989985	15.247539
25.392944	1360.007844	15.252557
25.713184	1362.634138	15.257575
25.494320	1366.667720	15.262592
25.794973	1353.671284	15.267610
25.532879	1369.334414	15.272627
25.216308	1367.142046	15.277645
25.433212	1365.946783	15.282663
25.589061	1372.781823	15.287680
25.807945	1362.466177	15.292698
25.995446	1376.439016	15.297715
25.845465	1377.726221	15.302733
25.831102	1353.509717	15.307751
25.622448	1369.010172	15.312768
26.091803	1370.986640	15.317786
25.844560	1372.717206	15.322803
25.923041	1375.564531	15.327821
26.052313	1384.712934	15.332839
25.764408	1383.160908	15.337856
25.654736	1389.489343	15.342874
25.724576	1389.512995	15.347891
26.017279	1395.907806	15.352909
25.982156	1383.557914	15.357927
25.748040	1397.231524	15.362944
25.747588	1388.668531	15.367962
25.880465	1393.578784	15.372979
25.440171	1396.416059	15.377997
25.802533	1400.113126	15.383015
26.291203	1419.351464	15.388032
26.408208	1416.476467	15.393050
26.228033	1428.005405	15.398067
26.495265	1422.795744	15.403085
26.416834	1411.171587	15.408103
26.345868	1420.070390	15.413120
26.320102	1410.684038	15.418138
26.372455	1404.144894	15.423155
26.145696	1406.671266	15.428173
26.688308	1417.642896	15.433191
26.630218	1405.807866	15.438208
26.710251	1405.081157	15.443226
26.796754	1394.550659	15.448243
26.887192	1386.629098	15.453261
26.786942	1383.576412	15.458279
26.704601	1387.671589	15.463296
26.782759	1389.785964	15.468314
26.713227	1386.717367	15.473331
26.509877	1394.177555	15.478349
26.727840	1386.485755	15.483367
26.642464	1390.280980	15.488384
26.712636	1386.129916	15.493402
26.517545	1382.301155	15.498419
26.465518	1390.665256	15.503437
26.822880	1382.351920	15.508455
26.357087	1390.761574	15.513472
26.360069	1378.219998	15.518490
26.725696	1391.665807	15.523507
26.496675	1385.374467	15.528525
26.968787	1402.768758	15.533543
26.805045	1404.089619	15.538560
26.792040	1419.444092	15.543578
26.795322	1421.140993	15.548595
26.977947	1414.343545	15.553613
27.125758	1414.993387	15.558631
27.144172	1418.249836	15.563648
26.950728	1413.149841	15.568666
27.287800	1428.234558	15.573683
27.062053	1425.552655	15.578701
27.232899	1418.236429	15.583719
27.117310	1418.835481	15.588736
27.214218	1409.681237	15.593754
27.325015	1416.213608	15.598771
27.171259	1423.217604	15.603789
27.565068	1408.660027	15.608807
27.276121	1423.374278	15.613824
27.381006	1414.377629	15.618842
27.378077	1408.344360	15.623859
27.102019	1404.755016	15.628877
27.344856	1401.004254	15.633895
27.325476	1414.999119	15.638912
27.628349	1405.991343	15.643930
27.388784	1419.346530	15.648947
27.402379	1415.212347	15.653965
27.687761	1406.993846	15.658983
27.138281	1416.088523	15.664000
27.041026	1415.844682	15.669018
27.915146	1408.163032	15.674035
27.408238	1411.522151	15.679053
27.461827	1411.682098	15.684071
27.358171	1411.340181	15.689088
27.531443	1418.715139	15.694106
27.961067	1414.785146	15.699123
27.545669	1409.275406	15.704141
27.531150	1407.333715	15.709159
27.454373	1416.466243	15.714176
27.710781	1411.744362	15.719194
27.577289	1408.858990	15.724211
27.512298	1417.273936	15.729229
27.672077	1420.605361	15.734247
27.493898	1421.760218	15.739264
27.826425	1436.387934	15.744282
28.035834	1435.536770	15.749299
27.656737	1449.711740	15.754317
27.761709	1440.584504	15.759335
27.869252	1442.253766	15.764352
27.829627	1445.292971	15.769370
28.270544	1438.946652	15.774387
28.011767	1443.453795	15.779405
28.116661	1428.322531	15.784423
28.072077	1440.100401	15.789440
27.998253	1441.084463	15.794458
28.345721	1447.767854	15.799475
28.081381	1441.114046	15.804493
28.347941	1440.601394	15.809511
28.135518	1436.094284	15.814528
28.226535	1437.091375	15.819546
28.546191	1445.511048	15.824563
28.424599	1449.080837	15.829581
28.544295	1455.600796	15.834599
28.465015	1442.812745	15.839616
28.414803	1453.322132	15.844634
28.648348	1452.635426	15.849651
28.473370	1458.732070	15.854669
28.679217	1437.568055	15.859687
28.520653	1443.282987	15.864704
28.484847	1446.658200	15.869722
28.659037	1435.503371	15.874739
28.648160	1443.961610	15.879757
28.562972	1436.451842	15.884775
28.390053	1436.981390	15.889792
28.477397	1442.318907	15.894810
28.793661	1428.942400	15.899827
28.375164	1447.713593	15.904845
28.395968	1447.350250	15.909863
28.764189	1443.404877	15.914880
28.574189	1435.532741	15.919898
28.744731	1442.148400	15.924915
28.617265	1442.374978	15.929933
28.916440	1446.319656	15.934951
29.065017	1451.935265	15.939968
28.840194	1438.053620	15.944986
29.150588	1436.020773	15.950003
28.652998	1449.741178	15.955021
28.815918	1445.867877	15.960039
29.174695	1448.887576	15.965056
29.287705	1459.416548	15.970074
29.083287	1455.022983	15.975091
28.823071	1458.034458	15.980109
28.856066	1464.911161	15.985127
29.143180	1472.439442	15.990144
29.169441	1472.377239	15.995162
29.462411	1466.136303	16.000179
29.011509	1464.213877	16.005197
29.342972	1465.767202	16.010215
29.463565	1469.704194	16.015232
29.275943	1479.040054	16.020250
29.665554	1464.730049	16.025267
29.377762	1454.424375	16.030285
29.264742	1456.025005	16.035303
29.323335	1447.380202	16.040320
29.312435	1464.442639	16.045338
29.663131	1465.016077	16.050355
29.421497	1465.584901	16.055373
29.776579	1475.430350	16.060391
29.624479	1454.208580	16.065408
29.507663	1462.784399	16.070426
29.479625	1450.716455	16.075443
29.485508	1466.838725	16.080461
29.516642	1467.964917	16.085479
29.629756	1477.111237	16.090496
29.651284	1470.753153	16.095514
29.983518	1466.242523	16.100531
29.630555	1475.095109	16.105549
29.568394	1475.548792	16.110567
29.780232	1472.244964	16.115584
29.686125	1473.350236	16.120602
29.840724	1478.412778	16.125619
29.609240	1473.395905	16.130637
29.559516	1481.942158	16.135655
29.771005	1485.289730	16.140672
29.573963	1479.513118	16.145690
30.275063	1471.988019	16.150707
29.847093	1475.721513	16.155725
30.068012	1478.250417	16.160743
30.103817	1478.421066	16.165760
29.791814	1488.880218	16.170778
29.596513	1489.037396	16.175795
30.283240	1500.840232	16.180813
30.151370	1500.391131	16.185831
30.323158	1501.449274	16.190848
30.253693	1504.397299	16.195866
30.415291	1491.509435	16.200883
30.400037	1493.130653	16.205901
30.031234	1492.922261	16.210919
30.251243	1491.934127	16.215936
30.271215	1491.605520	16.220954
30.397127	1500.954302	16.225971
30.507451	1499.637607	16.230989
30.547239	1492.548310	16.236007
30.706293	1490.863631	16.241024
30.403212	1486.578600	16.246042
30.589593	1471.649004	16.251059
30.847976	1478.636048	16.256077
30.743704	1486.570464	16.261095
31.240696	1478.534454	16.266112
30.865660	1473.074877	16.271130
30.861425	1466.569899	16.276147
30.960818	1456.103365	16.281165
30.787363	1461.114413	16.286183
31.150780	1453.438701	16.291200
30.848665	1459.933139	16.296218
30.810517	1460.733765	16.301235
30.631368	1462.127873	16.306253
30.605348	1469.040731	16.311271
30.806496	1464.794822	16.316288
30.535522	1477.980472	16.321306
30.795993	1467.110722	16.326323
31.010901	1473.853022	16.331341
30.807923	1480.740631	16.336359
31.169374	1477.268223	16.341376
30.982004	1478.872850	16.346394
31.099317	1470.641798	16.351411
31.115225	1474.022925	16.356429
30.930817	1472.364720	16.361447
31.124792	1471.641855	16.366464
31.072946	1466.259713	16.371482
31.120086	1474.969830	16.376499
31.133760	1479.287237	16.381517
31.257047	1471.797679	16.386535
31.215929	1474.649943	16.391552
30.750840	1477.072775	16.396570
31.059261	1458.445314	16.401587
31.172356	1473.746698	16.406605
30.776572	1485.030869	16.411623
31.553024	1488.234057	16.416640
31.467630	1506.744559	16.421658
31.505996	1509.157874	16.426675
31.711664	1504.189234	16.431693
31.504622	1501.315574	16.436711
31.907657	1510.753862	16.441728
31.561700	1512.655915	16.446746
31.499283	1509.823676	16.451763
31.841904	1509.171478	16.456781
31.590248	1512.673942	16.461799
31.858570	1509.502665	16.466816
31.496281	1512.889073	16.471834
31.484521	1503.093024	16.476851
31.650020	1510.009958	16.481869
31.566577	1510.871293	16.486887
31.588009	1509.556193	16.491904
31.540037	1519.119907	16.496922
31.950189	1510.428427	16.501939
31.993241	1510.638818	16.506957
31.518705	1507.781085	16.511975
31.968133	1530.185954	16.516992
32.027080	1536.923274	16.522010
32.002229	1549.412221	16.527027
32.355891	1539.380112	16.532045
32.273069	1545.422768	16.537063
32.459130	1524.859517	16.542080
32.329483	1539.405333	16.547098
32.347407	1527.487293	16.552115
32.312712	1520.606486	16.557133
32.098802	1517.118882	16.562151
32.521152	1527.905293	16.567168
32.380670	1518.460093	16.572186
32.239014	1510.795704	16.577203
32.484364	1522.841990	16.582221
32.652414	1528.342840	16.587239
32.676284	1514.764363	16.592256
32.319035	1514.182903	16.597274
32.432403	1503.358612	16.602291
32.697407	1519.909930	16.607309
32.563781	1514.770471	16.612327
32.483139	1511.389022	16.617344
32.572332	1528.622755	16.622362
32.866314	1525.755686	16.627379
33.024849	1530.982782	16.632397
32.536679	1524.287562	16.637415
32.771407	1515.696419	16.642432
32.523459	1528.271269	16.647450
32.874448	1538.208648	16.652467
33.009588	1518.886749	16.657485
32.596463	1535.621757	16.662503
32.822643	1524.063747	16.667520
32.784837	1526.794374	16.672538
32.886010	1527.102458	16.677555
32.748568	1528.968106	16.682573
32.516600	1523.454230	16.687591
32.953835	1523.932072	16.692608
32.820314	1524.755778	16.697626
32.893945	1541.081250	16.702643
33.196897	1531.971140	16.707661
33.300792	1564.886818	16.712679
33.074165	1550.053695	16.717696
33.138335	1559.898416	16.722714
33.149284	1553.652093	16.727731
33.388086	1560.928584	16.732749
33.583353	1570.499150	16.737767
33.639506	1559.432266	16.742784
33.512039	1542.510134	16.747802
33.219045	1548.644516	16.752819
33.927518	1547.119152	16.757837
33.426739	1531.362390	16.762855
33.168850	1536.957925	16.767872
33.373352	1533.759071	16.772890
33.509945	1546.519558	16.777907
33.645811	1544.462627	16.782925
33.700806	1554.741380	16.787943
33.817975	1557.750880	16.792960
33.981304	1547.143524	16.797978
33.695457	1560.814528	16.802995
33.848204	1539.304913	16.808013
33.835562	1545.537716	16.813031
33.739561	1537.263576	16.818048
33.896614	1549.635421	16.823066
33.871029	1550.990885	16.828083
34.306761	1551.303804	16.833101
33.603197	1541.586619	16.838119
33.924204	1533.285289	16.843136
33.757011	1555.739793	16.848154
33.778968	1547.508178	16.853171
34.255212	1550.109624	16.858189
33.878074	1549.046854	16.863207
33.969424	1556.891117	16.868224
34.111093	1552.165472	16.873242
33.913614	1555.612115	16.878259
33.936905	1556.379351	16.883277
33.540813	1558.322439	16.888295
33.946688	1549.998124	16.893312
34.094687	1579.760827	16.898330
33.558198	1582.600896	16.903347
34.282509	1580.344707	16.908365
34.201645	1587.093341	16.913383
34.340349	1584.411474	16.918400
34.100140	1581.582414	16.923418
34.492905	1582.105103	16.928435
34.540006	1581.080052	16.933453
34.620347	1576.219466	16.938471
34.658872	1582.066606	16.943488
34.486260	1575.997413	16.948506
34.467788	1575.146413	16.953523
34.711321	1594.848795	16.958541
34.597447	1596.512496	16.963559
34.786503	1606.924055	16.968576
35.074254	1606.159484	16.973594
35.377927	1604.536666	16.978611
35.240633	1586.584166	16.983629
34.763572	1576.514656	16.988647
35.030081	1569.977456	16.993664
35.347776	1552.005906	16.998682
35.262812	1567.414485	17.003699
35.374698	1566.185623	17.008717
35.313683	1558.775753	17.013735
35.495359	1563.228405	17.018752
35.378069	1561.496564	17.023770
35.226401	1571.444933	17.028787
35.287864	1556.005866	17.033805
35.006378	1575.309060	17.038823
35.253967	1565.605304	17.043840
34.979446	1563.335412	17.048858
34.940312	1566.852753	17.053875
35.117773	1570.344984	17.058893
35.365769	1579.614570	17.063911
35.546460	1570.866849	17.068928
35.470936	1567.074020	17.073946
35.341373	1555.774072	17.078963
35.649481	1553.554389	17.083981
35.312484	1565.132044	17.088999
35.529490	1568.706054	17.094016
35.595789	1563.081667	17.099034
35.348296	1573.735865	17.104051
35.768015	1561.585396	17.109069
35.501268	1572.025592	17.114087
35.609399	1566.690252	17.119104
35.382818	1565.251117	17.124122
35.319060	1576.690818	17.129139
35.993315	1589.068285	17.134157
35.872185	1602.949004	17.139175
35.528770	1600.984245	17.144192
35.726606	1598.094747	17.149210
35.676756	1606.828278	17.154227
35.663728	1600.178354	17.159245
36.014596	1599.292034	17.164263
35.797470	1595.768744	17.169280
36.011330	1590.641469	17.174298
36.181478	1591.747070	17.179315
35.861329	1602.283892	17.184333
35.922246	1612.162201	17.189351
36.216065	1615.676781	17.194368
36.490410	1619.310869	17.199386
36.337440	1631.230449	17.204403
36.575333	1620.302840	17.209421
36.447392	1608.991581	17.214439
36.040415	1605.375878	17.219456
36.423809	1612.758318	17.224474
36.484146	1628.414340	17.229491
36.807510	1621.449631	17.234509
36.321856	1613.369732	17.239527
36.516477	1633.721751	17.244544
36.517592	1635.027347	17.249562
36.355823	1630.892761	17.254579
36.730979	1620.146174	17.259597
36.579128	1630.369886	17.264615
36.747644	1631.500919	17.269632
36.893452	1638.875652	17.274650
36.416423	1638.542949	17.279667
36.584169	1629.819280	17.284685
36.607692	1629.011913	17.289703
36.342255	1631.341576	17.294720
36.757136	1632.648811	17.299738
36.571576	1636.397161	17.304755
36.456000	1656.554877	17.309773
36.741060	1656.199713	17.314791
37.024369	1662.171432	17.319808
37.233556	1661.678935	17.324826
37.252337	1666.830847	17.329843
37.471917	1664.060562	17.334861
37.334418	1659.884344	17.339879
37.234785	1655.884556	17.344896
37.808353	1651.857610	17.349914
37.824202	1663.901298	17.354931
37.545937	1639.133389	17.359949
37.419757	1628.826979	17.364967
37.167472	1618.573724	17.369984
37.334418	1626.983256	17.375002
37.285722	1631.518293	17.380019
37.290789	1630.510954	17.385037
37.464355	1647.254752	17.390055
37.197934	1664.542224	17.395072
37.286418	1648.571793	17.400090
37.688571	1644.679156	17.405107
37.565141	1653.470069	17.410125
37.605036	1651.120124	17.415143
37.860680	1654.931807	17.420160
37.853732	1645.189949	17.425178
37.889628	1650.123625	17.430195
37.535345	1653.598448	17.435213
37.743766	1654.268521	17.440231
37.785335	1654.279379	17.445248
37.980919	1653.582990	17.450266
37.831298	1664.098949	17.455283
37.592665	1656.424782	17.460301
38.203567	1650.933712	17.465319
38.133454	1675.674213	17.470336
37.923039	1660.753448	17.475354
38.162688	1675.331728	17.480371
38.530968	1673.786685	17.485389
38.513446	1664.148746	17.490407
38.024786	1665.513592	17.495424
38.467909	1649.750856	17.500442
38.490602	1662.444672	17.505459
38.149733	1650.490954	17.510477
38.289183	1657.706265	17.515495
38.361524	1673.541316	17.520512
38.758563	1660.260251	17.525530
38.659189	1682.804805	17.530547
38.707602	1673.670715	17.535565
38.963245	1671.365003	17.540583
38.447928	1658.013966	17.545600
38.584703	1661.935846	17.550618
38.676501	1661.760944	17.555635
38.637709	1672.105076	17.560653
38.751276	1672.006925	17.565671
38.776111	1671.660236	17.570688
38.586014	1673.707332	17.575706
38.756483	1674.331549	17.580723
38.872290	1674.513035	17.585741
38.897291	1673.914639	17.590759
38.609313	1674.880966	17.595776
38.878029	1674.806830	17.600794
39.046228	1666.625752	17.605811
38.940107	1683.475551	17.610829
38.826123	1681.626766	17.615847
38.755825	1672.360603	17.620864
38.841958	1684.441860	17.625882
39.113079	1697.868424	17.630899
39.090064	1708.796796	17.635917
39.398997	1701.667613	17.640935
39.285018	1698.585589	17.645952
39.257684	1703.814082	17.650970
39.437589	1699.938004	17.655987
39.290894	1704.793859	17.661005
39.573089	1691.645912	17.666023
39.327739	1705.164303	17.671040
39.359813	1698.747809	17.676058
39.093210	1702.834713	17.681075
39.414363	1702.904795	17.686093
39.655087	1695.040890	17.691111
39.194252	1709.340833	17.696128
39.423092	1720.708808	17.701146
39.616674	1723.048637	17.706163
39.417860	1726.056664	17.711181
39.662354	1721.053444	17.716199
39.663434	1738.331368	17.721216
40.112952	1727.582278	17.726234
40.134481	1727.346226	17.731251
40.054250	1728.232229	17.736269
40.242965	1715.907697	17.741287
39.992858	1731.734470	17.746304
40.331734	1720.870901	17.751322
40.296230	1722.559867	17.756339
40.504837	1726.627608	17.761357
40.408688	1716.119719	17.766375
40.034806	1723.566379	17.771392
40.204178	1717.283704	17.776410
40.053673	1711.992712	17.781427
39.965618	1719.835793	17.786445
40.268100	1717.585523	17.791463
40.188035	1718.218245	17.796480
40.470642	1724.042240	17.801498
40.617932	1730.402194	17.806515
40.546949	1742.988328	17.811533
40.778904	1743.517799	17.816551
40.679790	1747.299578	17.821568
40.979402	1729.807315	17.826586
40.684178	1720.929352	17.831603
40.583341	1710.178399	17.836621
40.822717	1714.157859	17.841639
40.875023	1744.433235	17.846656
40.918454	1734.277445	17.851674
41.015540	1748.132933	17.856691
40.799889	1750.934441	17.861709
41.105284	1736.927036	17.866727
40.491426	1749.193931	17.871744
40.666377	1752.828178	17.876762
40.886709	1752.599740	17.881779
40.883552	1744.461681	17.886797
41.390979	1748.834117	17.891815
41.221983	1742.169680	17.896832
41.255812	1741.665827	17.901850
41.521486	1746.208957	17.906867
41.350935	1735.778988	17.911885
41.477035	1742.409740	17.916903
41.177744	1738.466943	17.921920
41.563197	1737.853521	17.926938
41.440441	1739.496633	17.931955
41.139589	1752.613365	17.936973
41.124417	1750.434207	17.941991
41.137939	1740.289476	17.947008
40.950874	1746.309518	17.952026
41.487065	1759.755207	17.957043
41.168192	1765.890661	17.962061
41.646208	1771.969794	17.967079
41.687832	1759.656103	17.972096
41.921949	1766.706933	17.977114
41.961171	1766.603337	17.982131
41.788258	1762.199932	17.987149
42.234127	1766.786685	17.992167
42.401595	1759.719363	17.997184
42.297735	1768.241386	18.002202
42.536309	1772.214698	18.007219
42.192542	1767.085072	18.012237
42.075334	1757.870381	18.017255
42.177476	1768.966023	18.022272
42.656260	1765.315959	18.027290
42.300371	1767.531084	18.032307
42.109572	1764.511635	18.037325
42.374141	1754.814484	18.042343
42.492065	1761.588119	18.047360
42.390496	1760.515983	18.052378
42.737843	1762.543432	18.057395
42.626815	1763.557044	18.062413
42.592468	1751.246039	18.067431
42.489954	1756.503846	18.072448
42.461655	1752.173331	18.077466
42.587099	1759.798337	18.082483
42.416806	1761.219374	18.087501
42.873004	1763.629005	18.092519
42.727092	1756.271900	18.097536
42.646623	1755.067413	18.102554
42.917979	1757.129004	18.107571
42.978893	1758.443948	18.112589
42.599895	1754.038812	18.117607
42.719428	1752.253443	18.122624
42.647477	1757.734461	18.127642
42.591792	1756.938149	18.132659
42.459771	1786.086850	18.137677
42.606658	1794.285749	18.142695
42.980342	1788.244159	18.147712
42.742386	1792.999770	18.152730
43.075527	1789.612029	18.157747
42.898106	1799.383765	18.162765
43.072747	1804.715357	18.167783
43.479568	1812.144500	18.172800
43.539628	1818.428745	18.177818
43.663649	1812.293261	18.182835
43.587154	1818.536367	18.187853
43.763556	1801.609508	18.192871
43.791264	1783.440110	18.197888
43.366171	1790.095881	18.202906
43.464925	1785.507566	18.207923
43.709778	1792.216925	18.212941
43.952492	1796.044866	18.217959
43.808635	1799.042569	18.222976
43.556869	1781.861559	18.227994
43.856147	1790.599288	18.233011
43.804029	1808.887792	18.238029
43.813624	1813.265724	18.243047
44.008675	1807.266777	18.248064
43.907737	1810.134941	18.253082
44.148611	1799.607841	18.258099
44.074394	1806.072373	18.263117
44.362585	1812.018209	18.268135
44.197478	1814.149426	18.273152
43.931902	1815.442522	18.278170
44.261715	1810.979364	18.283187
44.020651	1815.541996	18.288205
44.114413	1814.846111	18.293223
44.134286	1804.874926	18.298240
44.174157	1809.911841	18.303258
44.428543	1811.974574	18.308275
43.992727	1806.710179	18.313293
44.607084	1821.743216	18.318311
44.576366	1830.873377	18.323328
44.494801	1832.552400	18.328346
44.682642	1839.928397	18.333363
44.445816	1838.067724	18.338381
44.606154	1838.135144	18.343399
44.924582	1826.434767	18.348416
44.975725	1835.208956	18.353434
44.918382	1823.453688	18.358451
44.955134	1829.541882	18.363469
45.183917	1831.215447	18.368487
45.394869	1835.413405	18.373504
45.451353	1837.322092	18.378522
45.654304	1827.928875	18.383539
45.364129	1808.935551	18.388557
45.252332	1797.642019	18.393575
45.376928	1788.188966	18.398592
45.150181	1799.220689	18.403610
44.942524	1793.572270	18.408627
45.144739	1809.784727	18.413645
45.534886	1821.669743	18.418663
45.354027	1835.420212	18.423680
45.202364	1837.997599	18.428698
45.975403	1835.478775	18.433715
45.651536	1834.470405	18.438733
45.530803	1835.491862	18.443751
45.721833	1823.344621	18.448768
45.687119	1823.833261	18.453786
45.534551	1832.679267	18.458803
45.586985	1828.477424	18.463821
45.508278	1831.947658	18.468839
45.950030	1824.422852	18.473856
45.682175	1831.611982	18.478874
46.020247	1828.111762	18.483891
45.694368	1838.723600	18.488909
45.649783	1834.576556	18.493927
45.708012	1819.145589	18.498944
45.946658	1829.141988	18.503962
46.033882	1829.782638	18.508979
45.927205	1838.895033	18.513997
46.326306	1854.360412	18.519015
46.182989	1861.433739	18.524032
46.093839	1856.235153	18.529050
46.401530	1852.234834	18.534067
46.273781	1850.414963	18.539085
46.246005	1853.861348	18.544103
46.407231	1852.586840	18.549120
46.416077	1858.099054	18.554138
46.224831	1858.197385	18.559155
46.103397	1861.502982	18.564173
46.678793	1873.133550	18.569191
46.773746	1868.185593	18.574208
46.680958	1879.520052	18.579226
46.786274	1877.238286	18.584243
46.718166	1886.690624	18.589261
46.716848	1884.336204	18.594279
47.122672	1884.721545	18.599296
47.149767	1883.400788	18.604314
47.116618	1876.620239	18.609331
47.137077	1884.129922	18.614349
47.212537	1878.104404	18.619367
47.086744	1875.768266	18.624384
47.046389	1886.029430	18.629402
47.348031	1878.953234	18.634419
47.429317	1871.446573	18.639437
47.138786	1875.029256	18.644455
47.457704	1866.267176	18.649472
47.404215	1856.018221	18.654490
47.631151	1866.618982	18.659507
47.251438	1871.847112	18.664525
47.265982	1874.849452	18.669543
47.892070	1861.111673	18.674560
47.559889	1872.693522	18.679578
47.531489	1873.412391	18.684595
47.721731	1872.259095	18.689613
47.824367	1876.490072	18.694631
47.632710	1860.063871	18.699648
47.819727	1869.920670	18.704666
47.603008	1866.976120	18.709683
47.933085	1881.719510	18.714701
47.969993	1881.449542	18.719719
48.044917	1878.686560	18.724736
48.099322	1897.216160	18.729754
48.346366	1896.944134	18.734771
48.497760	1895.874111	18.739789
48.251877	1873.439724	18.744807
48.207228	1868.163249	18.749824
47.991146	1871.600349	18.754842
48.683567	1877.370051	18.759859
48.167462	1892.095838	18.764877
48.310354	1889.213474	18.769895
48.476184	1885.863410	18.774912
48.177147	1899.881328	18.779930
48.288224	1886.423873	18.784947
48.582014	1883.901259	18.789965
48.255818	1888.861310	18.794983
48.648388	1886.068110	18.800000
48.499172	1886.156591	18.805018
48.756668	1879.845633	18.810035
48.661530	1900.860873	18.815053
48.707069	1919.354162	18.820071
49.325694	1920.608480	18.825088
48.935687	1930.406346	18.830106
49.243062	1923.220675	18.835123
49.365989	1919.976547	18.840141
49.206109	1926.424909	18.845159
49.223082	1929.420581	18.850176
49.018795	1921.106864	18.855194
49.336328	1920.573483	18.860211
48.893324	1929.848119	18.865229
48.899544	1923.419919	18.870247
49.063700	1907.913760	18.875264
49.194816	1922.876118	18.880282
49.188046	1914.087306	18.885299
49.559100	1919.406489	18.890317
49.466440	1941.564983	18.895335
49.764709	1929.811110	18.900352
50.028001	1944.112184	18.905370
49.849858	1937.818777	18.910387
50.300231	1928.275919	18.915405
49.801773	1930.947963	18.920423
49.986322	1913.934730	18.925440
49.489527	1914.089662	18.930458
49.760030	1927.261709	18.935475
50.186288	1924.864251	18.940493
50.118984	1941.667259	18.945511
50.212158	1939.418882	18.950528
49.908950	1934.034187	18.955546
50.158668	1929.715904	18.960563
50.400642	1937.132080	18.965581
50.100092	1936.291443	18.970599
50.284538	1934.129182	18.975616
50.161570	1931.182250	18.980634
50.626903	1936.934715	18.985651
50.529953	1930.079373	18.990669
50.342978	1931.043762	18.995687
50.268034	1930.033434	19.000704
50.393107	1924.762901	19.005722
50.460315	1931.242684	19.010739
50.788377	1941.703100	19.015757
50.445670	1958.200843	19.020775
50.279800	1965.150401	19.025792
50.991507	1953.962923	19.030810
50.572947	1967.830082	19.035827
51.381256	1964.575725	19.040845
50.947974	1959.111094	19.045863
51.351107	1958.694620	19.050880
51.484930	1964.658849	19.055898
51.550396	1956.635568	19.060915
51.574209	1955.390834	19.065933
51.223065	1954.054896	19.070951
51.143409	1958.956771	19.075968
51.241238	1955.779559	19.080986
51.129960	1960.835916	19.086003
51.649888	1954.899921	19.091021
51.561371	1963.430622	19.096039
51.760680	1950.998809	19.101056
51.447023	1951.643630	19.106074
51.392164	1953.263351	19.111091
51.687992	1946.438161	19.116109
51.551140	1959.626448	19.121127
51.699643	1953.147226	19.126144
51.888827	1949.931849	19.131162
51.639183	1946.655906	19.136179
51.781163	1939.037283	19.141197
51.512192	1950.349561	19.146215
51.654086	1961.229798	19.151232
51.659085	1977.470754	19.156250
52.160233	1971.827186	19.161267
52.286359	1973.536019	19.166285
51.878716	1986.775387	19.171303
52.123554	1978.835169	19.176320
52.146318	1977.955545	19.181338
52.199399	1986.248168	19.186355
52.276002	1967.472987	19.191373
52.189702	2005.708543	19.196391
52.619143	2007.073269	19.201408
52.549355	2005.596494	19.206426
52.615094	2006.956310	19.211443
52.812403	1998.779841	19.216461
52.545103	2008.781559	19.221479
52.744703	2003.258437	19.226496
53.134800	2004.231460	19.231514
52.598228	2014.428716	19.236531
52.846478	1997.647472	19.241549
52.562051	2010.332377	19.246567
52.900727	2002.268639	19.251584
52.929430	2007.085605	19.256602
52.679842	2008.619987	19.261619
52.975360	2016.965194	19.266637
52.967381	2029.601302	19.271655
52.973126	2027.566632	19.276672
53.109917	2038.834709	19.281690
53.022308	2034.966605	19.286707
53.461843	2022.266751	19.291725
53.685710	2026.511470	19.296743
53.704395	2010.995371	19.301760
54.058596	2012.477492	19.306778
53.940869	2023.627276	19.311795
54.040494	2017.731554	19.316813
54.130910	2024.564756	19.321831
53.904919	2009.937126	19.326848
54.191473	2011.047789	19.331866
54.129233	2015.276790	19.336883
54.175704	1985.827040	19.341901
53.981986	1994.550719	19.346919
54.082433	1986.185212	19.351936
54.387813	1989.389727	19.356954
53.949198	1983.416272	19.361971
54.166877	1974.995893	19.366989
54.266717	1994.492079	19.372007
54.276252	1994.062879	19.377024
54.554882	1997.384921	19.382042
54.259899	2001.566097	19.387059
54.415278	2007.939042	19.392077
54.415696	2005.403426	19.397095
54.752849	2007.003098	19.402112
54.679557	2001.035862	19.407130
54.380554	2012.530731	19.412147
54.638836	2006.271504	19.417165
54.404983	2015.800700	19.422183
54.579327	2017.931287	19.427200
54.714001	2003.018046	19.432218
54.429571	2013.252162	19.437235
54.511543	2023.081775	19.442253
54.948337	2035.360654	19.447271
54.836534	2041.208361	19.452288
54.732424	2040.297059	19.457306
54.831078	2041.996125	19.462323
54.942791	2034.931271	19.467341
54.767899	2040.847244	19.472359
54.978856	2062.207154	19.477376
55.244428	2066.947034	19.482394
55.444565	2072.861404	19.487411
55.520782	2073.044492	19.492429
55.642317	2069.467068	19.497447
55.865656	2070.844225	19.502464
55.537558	2066.411995	19.507482
55.439691	2069.512531	19.512499
55.840469	2064.113029	19.517517
55.683818	2059.533904	19.522535
55.758412	2071.971259	19.527552
56.064771	2047.980868	19.532570
55.822738	2072.348341	19.537587
55.934785	2052.532334	19.542605
55.949539	2058.891551	19.547623
56.164329	2062.200195	19.552640
56.055099	2056.798671	19.557658
55.786128	2074.220744	19.562675
56.193950	2080.193228	19.567693
56.180814	2100.643538	19.572711
56.137635	2105.382339	19.577728
56.376511	2080.770292	19.582746
56.328999	2095.747162	19.587763
56.305465	2085.416189	19.592781
56.578084	2094.178805	19.597799
56.736969	2081.773777	19.602816
56.720542	2093.739598	19.607834
56.615737	2091.429965	19.612851
56.834349	2095.073066	19.617869
56.971912	2077.010049	19.622887
57.034952	2087.361831	19.627904
57.267136	2070.441492	19.632922
56.832759	2078.852817	19.637939
56.801768	2082.268308	19.642957
57.084576	2082.942269	19.647975
56.931176	2106.501274	19.652992
57.301326	2109.549192	19.658010
57.109801	2112.496359	19.663027
57.468308	2103.793890	19.668045
57.774066	2101.538323	19.673063
57.610219	2106.634576	19.678080
57.981916	2091.422313	19.683098
57.815103	2097.337020	19.688115
57.807967	2078.081116	19.693133
57.583718	2074.274122	19.698151
57.860726	2073.940686	19.703168
57.933266	2076.021451	19.708186
57.511454	2070.289102	19.713203
57.713013	2092.424494	19.718221
58.010904	2089.842990	19.723239
58.225044	2101.490467	19.728256
58.574247	2095.867941	19.733274
58.242738	2094.145034	19.738291
58.478970	2094.363948	19.743309
58.167612	2107.421325	19.748327
58.154682	2103.066231	19.753344
58.573189	2091.635974	19.758362
58.463535	2104.019374	19.763379
58.774894	2094.504873	19.768397
59.325937	2075.760847	19.773415
58.631596	2080.032484	19.778432
58.358577	2052.145254	19.783450
58.524897	2065.217640	19.788467
58.482029	2076.832157	19.793485
58.528854	2090.933521	19.798503
58.732599	2088.939622	19.803520
58.671527	2092.621039	19.808538
58.627172	2099.139141	19.813555
58.616796	2084.791653	19.818573
58.800389	2094.962188	19.823591
58.535992	2104.221030	19.828608
58.801317	2119.143308	19.833626
58.743446	2130.220705	19.838643
58.910554	2138.426014	19.843661
59.227869	2133.360701	19.848679
58.888694	2128.554260	19.853696
59.174564	2135.617466	19.858714
59.237997	2156.396994	19.863731
59.501921	2153.849211	19.868749
59.823000	2149.206444	19.873767
59.778148	2168.724370	19.878784
59.957922	2172.436607	19.883802
59.850689	2166.454266	19.888819
60.115291	2164.106151	19.893837
59.959609	2159.276724	19.898855
60.004597	2160.241882	19.903872
60.425419	2156.333551	19.908890
60.533592	2153.414201	19.913907
60.459959	2154.082095	19.918925
60.422819	2137.421717	19.923943
60.387667	2120.197889	19.928960
60.367378	2112.296740	19.933978
60.211052	2108.441149	19.938995
60.323646	2123.317006	19.944013
60.406713	2130.269409	19.949031
60.428417	2139.570731	19.954048
60.393442	2140.449540	19.959066
60.192394	2145.570617	19.964083
60.467518	2151.775086	19.969101
60.829720	2144.836970	19.974119
60.394924	2148.966554	19.979136
60.456777	2151.321173	19.984154
60.883416	2163.095258	19.989171
60.700756	2169.747138	19.994189
60.765302	2176.593977	19.999207
60.542514	2180.364133	20.004224
60.705776	2177.253517	20.009242
60.776000	2179.172642	20.014259
60.787153	2187.314762	20.019277
61.005159	2196.786162	20.024295
61.058435	2201.114772	20.029312
61.326564	2197.100221	20.034330
61.543245	2198.782053	20.039347
61.275864	2202.755959	20.044365
61.319987	2213.606361	20.049383
61.448560	2233.664587	20.054400
61.780413	2223.726727	20.059418
61.890828	2219.861596	20.064435
61.759853	2232.703120	20.069453
62.196851	2223.890532	20.074471
61.869628	2223.006939	20.079488
62.161827	2215.592306	20.084506
62.128362	2225.204510	20.089523
62.289174	2219.687493	20.094541
62.633652	2218.791148	20.099559
62.428163	2214.715277	20.104576
62.698252	2219.983036	20.109594
62.833836	2217.174135	20.114611
62.438258	2219.431834	20.119629
62.634744	2208.851743	20.124647
62.371324	2220.292335	20.129664
62.414615	2215.256544	20.134682
62.916297	2213.764106	20.139699
62.470510	2213.715842	20.144717
62.368516	2214.488938	20.149735
62.501687	2220.234722	20.154752
62.495108	2214.829350	20.159770
62.743395	2232.310685	20.164787
62.609778	2239.355905	20.169805
63.275274	2241.949322	20.174823
63.140136	2246.400808	20.179840
63.294309	2241.147543	20.184858
63.183118	2249.729220	20.189875
63.221468	2244.832636	20.194893
63.639017	2236.101796	20.199911
63.148153	2245.563592	20.204928
63.371823	2237.884592	20.209946
63.688966	2241.669322	20.214963
63.978070	2267.118045	20.219981
63.778753	2254.911579	20.224999
63.694551	2251.994577	20.230016
64.145845	2258.271670	20.235034
64.104209	2264.342662	20.240051
63.946484	2265.049143	20.245069
64.084262	2255.244465	20.250087
64.410881	2265.494557	20.255104
64.318055	2247.474368	20.260122
64.196557	2252.077840	20.265139
63.929551	2261.599899	20.270157
64.420572	2259.122845	20.275175
64.682328	2264.775777	20.280192
64.527934	2260.433760	20.285210
64.518593	2265.337107	20.290227
64.507441	2260.736284	20.295245
64.567009	2253.085024	20.300263
64.498256	2267.173531	20.305280
64.436771	2266.577895	20.310298
64.776261	2258.551640	20.315315
64.525030	2268.664233	20.320333
64.614509	2267.130567	20.325351
64.716193	2285.071087	20.330368
64.915197	2290.274702	20.335386
65.272186	2292.478449	20.340403
64.919127	2291.539195	20.345421
65.139183	2285.666629	20.350439
64.979887	2294.875793	20.355456
65.160423	2291.320366	20.360474
65.523845	2292.351151	20.365491
65.388531	2305.638609	20.370509
65.481665	2320.613728	20.375527
65.677163	2317.659968	20.380544
65.691191	2321.445872	20.385562
65.747184	2321.662077	20.390579
65.830057	2322.789522	20.395597
66.098508	2315.853694	20.400615
66.112015	2324.104058	20.405632
66.204299	2318.322646	20.410650
66.220616	2312.517173	20.415667
66.060757	2320.128203	20.420685
66.108131	2313.806527	20.425703
65.941996	2315.005149	20.430720
66.241992	2312.936092	20.435738
66.264051	2310.678551	20.440755
66.118947	2310.629519	20.445773
66.058529	2305.967325	20.450791
66.496917	2318.339003	20.455808
66.428284	2328.570382	20.460826
66.947064	2336.713421	20.465843
66.850279	2338.160540	20.470861
66.733044	2341.199726	20.475879
66.601127	2330.967664	20.480896
66.814064	2339.560619	20.485914
67.079041	2329.317166	20.490931
67.070259	2339.495747	20.495949
67.257016	2331.419093	20.500967
67.035910	2332.622551	20.505984
67.208397	2326.571147	20.511002
67.405745	2335.515021	20.516019
67.322883	2329.339170	20.521037
67.474435	2353.781983	20.526055
67.690083	2353.371023	20.531072
67.614088	2352.710841	20.536090
67.990786	2358.131539	20.541107
68.061769	2358.906942	20.546125
67.713622	2345.614332	20.551143
67.789535	2347.490885	20.556160
67.982058	2358.848640	20.561178
68.154767	2359.810744	20.566195
67.838015	2368.758769	20.571213
68.000292	2361.031293	20.576231
68.175371	2354.728558	20.581248
68.087498	2357.369009	20.586266
68.265981	2347.132260	20.591283
68.290225	2356.261851	20.596301
68.374471	2346.740151	20.601319
68.400362	2346.024392	20.606336
68.475887	2364.413577	20.611354
68.429171	2368.381434	20.616371
68.855603	2379.284245	20.621389
68.744537	2371.749016	20.626407
69.014257	2377.594997	20.631424
68.714771	2381.201252	20.636442
69.015169	2380.982848	20.641459
68.899004	2384.846951	20.646477
69.213587	2379.058375	20.651495
69.052873	2365.913609	20.656512
69.238451	2386.570949	20.661530
69.443822	2367.441221	20.666547
69.233254	2380.842214	20.671565
69.351611	2385.773999	20.676583
69.269486	2363.782296	20.681600
69.416379	2373.243131	20.686618
69.334629	2376.402511	20.691635
69.510061	2394.063194	20.696653
69.984543	2403.204377	20.701671
69.776628	2392.989111	20.706688
69.620152	2407.713899	20.711706
69.791056	2400.391668	20.716723
69.957225	2400.242651	20.721741
69.904030	2401.779569	20.726759
70.038119	2397.572404	20.731776
69.763371	2397.986085	20.736794
70.134622	2406.770128	20.741811
70.079332	2427.402233	20.746829
70.464212	2427.785429	20.751847
70.660049	2413.307196	20.756864
70.150963	2430.741248	20.761882
70.717142	2414.855027	20.766899
70.730681	2420.608173	20.771917
70.853472	2411.475128	20.776935
71.093893	2413.954685	20.781952
71.031251	2417.555421	20.786970
70.927943	2411.735166	20.791987
70.862515	2419.558497	20.797005
70.992000	2424.778755	20.802023
71.471871	2429.437383	20.807040
71.066956	2448.252526	20.812058
71.523958	2443.470794	20.817075
71.778952	2449.591297	20.822093
71.898844	2436.279012	20.827111
71.887629	2431.772530	20.832128
71.855888	2409.374731	20.837146
72.195110	2387.085333	20.842163
71.863887	2394.675755	20.847181
71.817726	2395.351076	20.852199
71.965184	2390.487380	20.857216
71.807255	2400.062133	20.862234
71.982242	2401.255120	20.867251
72.362206	2410.320144	20.872269
72.275676	2418.269541	20.877287
72.660556	2419.887606	20.882304
72.154269	2412.247858	20.887322
72.314347	2415.209795	20.892339
72.506026	2431.530027	20.897357
72.463495	2427.929918	20.902375
72.932013	2415.503537	20.907392
72.585464	2427.939153	20.912410
72.663272	2413.477384	20.917427
72.774627	2422.899874	20.922445
72.551191	2430.069627	20.927463
72.569508	2423.684109	20.932480
72.504891	2430.277953	20.937498
72.680855	2420.192571	20.942515
72.879523	2436.947439	20.947533
72.852846	2442.395538	20.952551
73.264708	2439.876810	20.957568
72.871773	2457.679348	20.962586
73.083297	2454.956607	20.967603
73.462531	2454.108192	20.972621
73.113021	2460.006565	20.977639
73.463337	2473.579318	20.982656
73.514151	2480.420625	20.987674
73.785550	2480.063694	20.992691
73.865663	2481.707565	20.997709
73.896366	2482.276246	21.002727
74.306615	2480.982418	21.007744
73.991460	2480.141715	21.012762
74.142825	2484.059920	21.017779
74.354660	2482.092208	21.022797
74.444227	2479.211155	21.027815
74.599448	2474.836996	21.032832
74.493563	2474.141462	21.037850
74.402278	2474.597459	21.042867
74.569110	2480.801253	21.047885
74.398460	2470.453355	21.052903
74.483222	2469.952365	21.057920
74.319403	2477.424891	21.062938
74.716863	2493.060327	21.067955
74.891789	2496.800165	21.072973
74.752730	2508.398906	21.077991
75.275230	2498.706531	21.083008
75.014228	2505.222401	21.088026
74.997658	2496.581884	21.093043
75.142096	2501.198077	21.098061
74.898336	2503.635319	21.103079
75.249999	2502.926585	21.108096
75.374509	2526.715664	21.113114
75.580807	2528.241096	21.118131
75.892458	2529.368251	21.123149
75.669673	2528.194261	21.128167
75.861377	2527.337211	21.133184
76.023740	2531.742121	21.138202
75.752990	2530.979279	21.143219
76.087468	2524.466210	21.148237
76.177475	2530.718460	21.153255
76.454139	2522.391396	21.158272
76.280793	2521.023897	21.163290
76.237894	2520.429218	21.168307
76.669897	2520.480844	21.173325
76.381268	2523.531673	21.178343
76.414712	2512.600611	21.183360
76.799704	2517.741610	21.188378
76.690371	2514.919803	21.193395
76.517550	2511.529224	21.198413
76.521853	2521.480106	21.203431
76.909753	2511.190966	21.208448
76.858388	2534.447301	21.213466
77.126007	2533.703991	21.218483
77.197305	2537.682960	21.223501
77.326148	2536.536261	21.228519
77.437439	2533.812975	21.233536
77.581353	2533.103553	21.238554
77.249473	2529.419000	21.243571
77.712142	2528.331536	21.248589
77.434077	2545.993945	21.253607
77.713831	2524.416997	21.258624
77.624450	2537.906562	21.263642
77.568586	2536.132556	21.268659
77.756243	2534.062509	21.273677
77.688607	2537.877225	21.278695
77.631735	2527.831264	21.283712
77.417088	2543.720118	21.288730
77.728162	2551.850789	21.293747
77.873012	2563.197431	21.298765
77.816550	2564.779720	21.303783
78.075686	2565.868847	21.308800
78.419015	2574.124953	21.313818
77.973600	2589.356139	21.318835
78.612748	2585.444339	21.323853
78.797242	2594.292892	21.328871
78.813979	2598.878358	21.333888
78.584585	2599.136939	21.338906
78.497657	2591.761348	21.343923
78.934456	2588.231048	21.348941
78.629746	2599.718635	21.353959
79.394380	2602.881505	21.358976
79.265874	2621.756611	21.363994
79.272965	2626.258676	21.369011
79.277753	2619.551171	21.374029
79.474158	2621.377081	21.379047
79.463844	2617.955053	21.384064
79.424657	2603.159381	21.389082
79.666495	2620.663451	21.394099
79.646440	2616.076521	21.399117
79.578113	2623.386805	21.404135
79.776291	2613.952945	21.409152
79.726740	2623.435836	21.414170
80.165358	2629.406001	21.419187
80.309184	2627.609574	21.424205
80.269817	2637.583232	21.429223
80.621732	2627.940789	21.434240
80.418159	2639.291148	21.439258
80.482221	2627.289338	21.444275
80.776907	2623.517414	21.449293
80.291475	2633.226355	21.454311
80.383068	2630.954527	21.459328
80.599263	2628.522035	21.464346
80.327316	2644.254961	21.469363
80.304016	2634.786407	21.474381
80.761386	2652.765827	21.479399
80.605702	2660.149841	21.484416
80.672860	2665.505189	21.489434
80.663003	2663.839452	21.494451
80.919584	2666.357378	21.499469
80.896873	2697.640911	21.504487
81.459965	2684.051636	21.509504
81.413080	2688.268158	21.514522
81.460630	2690.262544	21.519539
81.698939	2687.397056	21.524557
81.596878	2687.022602	21.529575
81.869870	2689.176885	21.534592
81.921193	2700.153138	21.539610
81.909686	2709.560801	21.544627
82.304531	2712.046457	21.549645
82.528453	2711.383258	21.554663
82.530982	2710.548505	21.559680
82.598798	2695.310932	21.564698
82.305557	2699.205720	21.569715
82.711690	2705.413918	21.574733
82.749752	2710.758978	21.579751
82.965130	2697.321108	21.584768
82.506600	2698.103899	21.589786
82.956604	2705.208853	21.594803
83.018842	2704.547845	21.599821
82.858401	2710.559315	21.604839
82.859590	2717.879010	21.609856
83.027381	2712.848360	21.614874
82.899858	2713.080469	21.619891
82.995184	2713.730093	21.624909
83.118719	2708.386374	21.629927
83.379307	2729.338210	21.634944
83.543407	2727.451229	21.639962
83.253926	2734.221080	21.644979
83.424945	2734.100391	21.649997
83.602568	2736.221911	21.655015
83.632232	2733.468347	21.660032
83.949739	2722.077306	21.665050
83.758593	2724.391355	21.670067
83.842237	2743.966641	21.675085
84.029041	2759.125486	21.680103
84.220086	2751.935942	21.685120
84.470377	2759.095585	21.690138
84.421606	2764.943754	21.695155
84.619250	2750.207694	21.700173
84.590093	2755.734175	21.705191
84.112915	2756.589946	21.710208
84.474710	2758.940875	21.715226
84.386339	2775.793827	21.720243
84.637060	2776.177982	21.725261
84.896082	2784.810260	21.730279
85.050374	2780.637518	21.735296
85.367094	2777.793328	21.740314
85.136736	2785.618777	21.745331
85.310347	2781.573522	21.750349
85.336307	2780.760198	21.755367
85.176204	2786.256448	21.760384
85.419177	2772.659155	21.765402
85.568048	2806.099047	21.770419
85.789053	2804.965159	21.775437
86.094928	2812.431375	21.780455
86.024090	2819.864862	21.785472
86.462848	2798.707344	21.790490
86.140308	2812.685049	21.795507
86.178590	2814.024152	21.800525
86.289240	2809.833192	21.805543
85.993968	2815.568102	21.810560
86.315752	2796.481385	21.815578
86.376857	2804.887248	21.820595
86.428506	2793.323822	21.825613
86.330716	2808.521030	21.830631
86.656844	2803.675895	21.835648
86.990732	2802.999087	21.840666
86.720396	2810.148189	21.845683
86.727077	2811.596157	21.850701
86.901505	2827.140104	21.855719
86.939497	2832.593766	21.860736
87.008922	2830.845362	21.865754
86.837977	2829.492394	21.870771
86.897440	2830.587431	21.875789
86.808029	2850.237654	21.880807
87.349756	2859.258285	21.885824
87.543306	2859.305472	21.890842
87.590845	2868.667639	21.895859
87.715405	2860.551846	21.900877
87.798989	2866.749419	21.905895
87.895306	2894.075273	21.910912
88.108567	2883.856986	21.915930
88.193930	2883.684672	21.920947
88.206581	2878.537127	21.925965
88.461827	2881.876478	21.930983
88.380699	2882.851574	21.936000
88.823627	2886.009973	21.941018
88.724035	2878.211510	21.946035
88.502171	2881.734714	21.951053
89.150077	2876.879924	21.956071
88.783732	2883.723455	21.961088
88.879247	2887.767089	21.966106
88.802039	2876.678784	21.971123
88.944823	2904.648524	21.976141
88.900870	2916.668179	21.981159
89.424861	2909.702329	21.986176
89.222159	2914.812924	21.991194
89.365529	2901.472873	21.996211
89.331968	2913.670992	22.001229
89.890093	2896.636361	22.006247
89.558850	2906.639449	22.011264
89.487086	2899.549167	22.016282
89.956446	2912.888615	22.021299
89.897559	2916.911261	22.026317
89.873469	2927.010105	22.031335
90.112214	2921.056435	22.036352
90.116829	2917.061694	22.041370
90.206892	2918.342994	22.046387
90.076322	2929.305955	22.051405
90.312381	2911.499921	22.056423
90.161191	2918.181730	22.061440
90.289243	2926.826328	22.066458
90.662362	2938.995004	22.071475
90.776189	2944.695395	22.076493
91.151286	2941.619265	22.081511
90.720711	2944.099744	22.086528
91.336566	2940.051560	22.091546
90.782578	2943.328064	22.096563
90.844208	2943.592935	22.101581
91.358816	2950.853674	22.106599
90.912427	2965.044772	22.111616
91.390318	2970.365402	22.116634
91.504689	2966.667771	22.121651
91.884837	2965.740528	22.126669
92.180755	2971.165692	22.131687
91.870294	2968.045513	22.136704
91.977895	2964.805959	22.141722
92.145526	2964.935938	22.146739
92.225383	2960.859180	22.151757
92.281382	2967.206711	22.156775
92.182005	2987.252779	22.161792
92.480809	2985.856340	22.166810
92.824183	2992.877763	22.171827
92.943955	2993.248987	22.176845
92.978701	2986.474396	22.181863
92.909443	2998.859191	22.186880
92.770438	2987.074315	22.191898
92.802610	2990.324204	22.196915
92.597526	2992.911098	22.201933
93.155395	2988.535496	22.206951
93.035068	2988.875007	22.211968
93.156033	2999.687785	22.216986
93.379216	3006.298128	22.222003
93.559370	3014.405106	22.227021
93.473147	3012.068763	22.232039
93.275794	3024.990788	22.237056
93.599527	3012.775774	22.242074
93.667390	3013.399115	22.247091
93.600079	3033.857804	22.252109
94.172196	3036.074555	22.257127
94.308920	3045.063147	22.262144
94.108075	3044.897935	22.267162
94.292296	3032.145114	22.272179
94.345382	3040.457216	22.277197
94.418451	3041.767981	22.282215
94.208170	3043.650941	22.287232
95.028187	3040.214375	22.292250
95.244946	3059.012170	22.297267
94.904701	3049.559285	22.302285
95.303099	3024.670074	22.307303
94.972680	3032.178891	22.312320
95.180467	3031.495442	22.317338
95.493438	3040.493679	22.322355
95.298522	3047.267469	22.327373
95.524460	3047.259152	22.332391
95.293979	3047.895467	22.337408
95.768624	3043.458398	22.342426
95.935622	3049.453968	22.347443
95.709076	3052.701871	22.352461
95.969112	3053.705158	22.357479
95.779380	3050.174778	22.362496
95.638389	3051.193254	22.367514
95.927568	3061.941495	22.372531
96.048140	3067.228692	22.377549
96.188905	3067.646912	22.382567
96.180264	3067.810511	22.387584
96.447805	3074.594723	22.392602
96.376333	3073.182606	22.397619
96.293966	3084.602075	22.402637
96.866179	3091.592556	22.407655
96.800486	3091.222516	22.412672
96.954384	3103.593048	22.417690
96.984036	3100.863800	22.422707
97.186778	3099.254564	22.427725
97.300249	3101.828427	22.432743
96.882112	3098.907091	22.437760
97.435338	3108.944665	22.442778
97.681810	3119.480304	22.447795
97.745193	3131.794503	22.452813
97.763118	3129.681438	22.457831
97.908335	3118.456794	22.462848
97.895277	3128.988996	22.467866
98.058049	3126.691582	22.472883
97.889063	3116.222610	22.477901
98.295264	3113.825023	22.482919
98.435063	3130.410741	22.487936
98.308718	3139.860594	22.492954
98.770195	3137.016062	22.497971
98.281584	3155.115512	22.502989
98.805785	3157.687594	22.508007
98.625677	3154.268135	22.513024
98.609550	3149.849524	22.518042
99.016365	3145.300536	22.523059
99.021213	3149.526245	22.528077
99.597169	3155.763404	22.533095
99.566190	3173.848100	22.538112
99.554304	3172.803242	22.543130
99.869607	3175.833397	22.548147
99.748983	3181.513852	22.553165
99.778399	3168.116219	22.558183
99.845678	3170.853992	22.563200
99.978971	3172.798588	22.568218
100.063244	3174.289278	22.573235
99.969052	3171.770907	22.578253
100.153354	3171.157271	22.583271
100.028604	3179.412077	22.588288
99.950594	3176.876966	22.593306
100.112586	3168.414443	22.598323
99.938188	3191.868429	22.603341
100.371484	3181.503149	22.608359
100.332870	3198.904768	22.613376
100.250745	3197.703567	22.618394
100.637461	3216.266017	22.623411
100.520510	3229.854221	22.628429
100.827713	3229.236714	22.633447
100.998658	3221.910133	22.638464
100.844686	3242.589807	22.643482
101.564111	3239.721423	22.648499
101.288330	3251.399192	22.653517
101.532529	3249.465548	22.658535
101.701778	3252.061219	22.663552
101.684810	3258.716270	22.668570
102.046716	3251.172800	22.673587
101.693816	3254.739801	22.678605
102.340064	3262.297486	22.683623
102.245658	3285.827749	22.688640
102.319876	3286.629431	22.693658
102.622908	3271.509489	22.698675
102.611864	3278.989521	22.703693
102.493429	3271.547817	22.708711
103.218776	3275.647644	22.713728
103.115177	3270.227463	22.718746
103.267356	3275.414519	22.723763
103.404841	3278.363719	22.728781
103.112367	3268.774858	22.733799
103.345261	3272.949289	22.738816
102.991411	3276.724892	22.743834
103.525598	3272.770663	22.748851
103.028037	3271.327369	22.753869
103.521071	3279.498652	22.758887
103.608012	3289.200117	22.763904
103.317427	3291.450666	22.768922
103.439639	3291.813644	22.773939
103.875660	3315.316783	22.778957
104.198336	3309.641396	22.783975
104.051767	3325.223697	22.788992
104.073357	3323.685017	22.794010
104.600791	3315.268744	22.799027
104.539315	3319.529464	22.804045
104.721632	3317.033830	22.809063
105.070992	3339.536129	22.814080
104.784140	3339.800735	22.819098
104.833866	3337.285341	22.824115
104.785086	3350.487582	22.829133
105.527665	3345.647435	22.834151
105.303395	3355.221593	22.839168
104.926643	3356.938426	22.844186
105.195956	3339.014087	22.849203
105.191439	3352.529414	22.854221
105.319493	3368.546997	22.859239
105.585173	3374.503366	22.864256
105.597304	3378.722474	22.869274
105.748188	3366.274371	22.874291
105.771723	3385.065646	22.879309
106.032708	3385.887890	22.884327
106.055665	3392.079624	22.889344
106.216728	3398.511271	22.894362
106.600852	3389.175473	22.899379
106.564969	3401.212332	22.904397
106.874058	3401.432240	22.909415
106.772410	3396.728288	22.914432
106.767977	3400.316049	22.919450
107.198845	3401.014450	22.924467
107.166665	3428.267407	22.929485
107.226050	3420.919190	22.934503
107.750122	3406.589783	22.939520
107.667561	3428.093693	22.944538
107.965589	3408.324844	22.949555
107.977406	3419.144328	22.954573
107.948990	3403.940241	22.959591
108.464755	3403.426334	22.964608
108.328071	3395.447872	22.969626
108.200904	3369.375478	22.974643
108.318143	3385.856536	22.979661
108.440132	3390.239830	22.984679
108.384485	3401.593145	22.989696
108.315444	3406.287723	22.994714
108.107847	3399.169304	22.999731
108.543367	3402.627908	23.004749
108.560020	3397.544042	23.009767
108.685675	3408.624605	23.014784
108.899886	3430.094561	23.019802
109.344840	3429.064141	23.024819
109.013778	3428.918116	23.029837
109.267951	3427.819010	23.034855
109.713596	3417.167635	23.039872
109.265856	3434.537243	23.044890
109.567492	3432.584190	23.049907
109.779845	3442.169006	23.054925
109.540871	3455.634506	23.059943
109.628654	3456.716422	23.064960
109.994976	3463.341904	23.069978
110.116629	3453.535063	23.074995
110.007207	3464.280310	23.080013
109.793690	3480.828382	23.085031
110.503838	3470.039608	23.090048
110.336516	3482.751158	23.095066
110.617949	3477.108243	23.100083
110.708097	3499.109375	23.105101
110.454098	3518.185782	23.110119
110.913844	3505.777976	23.115136
111.167046	3514.731765	23.120154
111.339666	3512.240005	23.125171
111.421342	3504.199129	23.130189
111.242521	3506.154216	23.135207
111.702208	3514.667616	23.140224
111.629198	3535.174325	23.145242
111.785504	3537.798070	23.150259
111.992624	3538.166393	23.155277
111.963484	3542.433819	23.160295
112.170047	3531.395726	23.165312
111.833967	3535.164626	23.170330
111.966854	3541.418339	23.175347
111.985121	3553.493883	23.180365
112.063539	3565.091029	23.185383
112.385464	3570.387203	23.190400
112.502131	3571.813773	23.195418
112.630463	3576.394336	23.200435
112.851926	3589.337379	23.205453
112.747517	3598.608616	23.210471
113.225157	3597.081345	23.215488
113.044824	3600.098601	23.220506
113.636636	3599.558402	23.225523
113.372834	3618.776519	23.230541
113.548003	3623.452672	23.235559
113.939022	3622.080015	23.240576
113.945979	3629.238780	23.245594
113.945014	3621.445428	23.250611
113.868111	3623.346520	23.255629
114.047938	3624.641099	23.260647
114.732985	3627.414948	23.265664
114.506937	3644.560663	23.270682
114.663159	3653.443477	23.275699
115.031608	3643.390273	23.280717
115.106179	3651.018882	23.285735
115.500389	3638.691424	23.290752
115.655816	3634.077761	23.295770
115.463997	3631.214613	23.300787
115.407582	3613.097251	23.305805
114.921959	3632.703161	23.310823
115.190445	3620.962911	23.315840
115.202159	3625.814588	23.320858
115.718425	3622.133720	23.325875
115.661850	3633.663563	23.330893
115.700480	3658.992631	23.335911
115.999594	3649.856652	23.340928
116.151330	3664.313302	23.345946
116.029158	3666.190941	23.350963
116.285662	3661.580028	23.355981
116.073293	3670.248680	23.360999
116.662096	3675.514131	23.366016
116.377753	3680.514513	23.371034
116.790930	3684.786956	23.376051
117.068713	3671.217891	23.381069
116.879562	3680.236820	23.386087
117.075663	3692.411550	23.391104
117.189237	3700.980257	23.396122
117.338301	3701.110847	23.401139
117.343952	3712.698477	23.406157
117.160234	3709.809637	23.411175
117.427378	3709.909597	23.416192
117.334062	3714.621517	23.421210
117.642269	3732.145448	23.426227
117.774668	3731.795717	23.431245
117.898077	3734.041664	23.436263
118.378829	3722.925876	23.441280
118.310593	3742.320632	23.446298
118.226844	3760.716529	23.451315
118.720721	3757.896607	23.456333
118.847209	3760.379626	23.461351
118.818178	3759.578950	23.466368
119.024879	3761.823418	23.471386
118.992464	3753.899714	23.476403
119.319597	3761.130981	23.481421
119.208547	3765.756073	23.486439
119.517487	3779.724451	23.491456
119.679662	3778.371757	23.496474
119.623581	3786.700121	23.501491
119.847689	3778.501083	23.506509
119.585715	3781.455094	23.511527
120.060053	3782.517867	23.516544
120.028372	3790.632317	23.521562
120.187917	3799.391978	23.526579
120.320346	3799.002123	23.531597
120.140056	3815.415481	23.536615
120.711946	3808.351901	23.541632
120.732483	3808.414102	23.546650
120.715562	3812.544361	23.551667
120.942464	3803.789512	23.556685
120.699482	3825.748295	23.561703
121.330243	3831.184888	23.566720
121.199806	3832.099473	23.571738
121.446361	3836.452811	23.576755
121.823502	3851.242623	23.581773
121.874832	3861.009145	23.586791
121.666649	3859.645496	23.591808
122.097646	3861.448316	23.596826
122.230109	3858.559366	23.601843
122.252689	3848.174164	23.606861
122.398953	3855.005616	23.611879
122.404424	3860.740952	23.616896
122.579918	3851.465666	23.621914
122.867038	3848.272019	23.626931
123.051613	3859.545689	23.631949
122.904115	3874.055773	23.636967
123.103479	3876.399757	23.641984
123.354343	3881.581519	23.647002
123.128242	3879.180814	23.652019
123.303466	3870.316961	23.657037
123.446179	3871.503423	23.662055
123.551648	3871.533200	23.667072
123.858758	3879.714024	23.672090
123.705587	3899.141412	23.677107
124.166503	3893.607374	23.682125
124.049771	3906.833539	23.687143
124.112728	3906.336768	23.692160
124.332106	3900.414898	23.697178
124.328712	3897.526368	23.702195
124.234834	3898.181835	23.707213
124.265228	3912.714718	23.712231
124.815259	3915.518024	23.717248
124.890053	3920.366819	23.722266
124.984027	3929.238489	23.727283
125.015392	3914.118733	23.732301
124.938271	3922.466262	23.737319
125.029286	3940.721242	23.742336
125.472684	3944.582260	23.747354
125.349142	3955.872890	23.752371
125.351255	3975.274041	23.757389
126.006833	3955.397093	23.762407
126.299963	3974.965797	23.767424
126.086713	3971.465686	23.772442
126.092864	3979.847952	23.777459
126.464537	3972.309638	23.782477
126.534145	3967.862948	23.787495
126.489451	3973.638580	23.792512
127.139447	3985.507544	23.797530
127.206075	3999.055387	23.802547
127.245801	4000.675981	23.807565
127.175767	3995.832280	23.812583
127.460775	3994.629102	23.817600
127.671118	3997.503115	23.822618
127.292695	4006.554787	23.827635
127.851328	3997.569145	23.832653
127.479087	3992.352006	23.837671
127.560085	4022.110731	23.842688
127.960412	4031.204209	23.847706
128.081311	4027.465153	23.852723
128.425159	4029.012079	23.857741
128.380602	4019.874040	23.862759
128.425604	4023.304612	23.867776
128.709141	4031.685938	23.872794
129.020191	4044.943124	23.877811
129.542533	4043.168761	23.882829
129.519560	4051.565939	23.887847
129.370513	4045.129312	23.892864
129.773237	4043.247377	23.897882
129.685539	4048.011213	23.902899
129.775290	4047.356771	23.907917
129.532878	4056.175967	23.912935
129.916581	4047.579254	23.917952
129.812517	4040.379505	23.922970
129.756871	4046.818467	23.927987
130.012377	4043.760400	23.933005
130.296077	4059.252053	23.938023
130.002854	4067.859890	23.943040
130.503113	4054.212515	23.948058
130.487138	4071.612348	23.953075
130.696998	4085.028088	23.958093
130.986256	4090.875585	23.963111
130.969778	4096.783640	23.968128
131.200955	4088.930993	23.973146
130.812170	4097.735798	23.978163
131.021526	4102.114815	23.983181
131.445723	4125.296272	23.988199
131.414735	4116.428970	23.993216
131.725471	4117.919830	23.998234
131.612692	4121.470768	24.003251
131.813517	4141.227474	24.008269
132.067260	4138.397007	24.013287
132.210536	4153.449399	24.018304
132.365337	4138.785641	24.023322
132.524476	4153.085841	24.028339
133.280346	4154.079364	24.033357
133.161500	4155.792914	24.038375
132.975927	4165.482569	24.043392
133.248477	4158.666366	24.048410
133.385167	4165.319351	24.053427
133.253273	4170.873763	24.058445
133.500126	4166.233554	24.063463
133.332038	4167.809430	24.068480
133.659270	4176.172072	24.073498
133.476542	4197.479121	24.078515
133.638491	4196.495358	24.083533
133.945538	4199.906995	24.088551
134.262830	4227.008954	24.093568
134.283022	4228.821482	24.098586
133.963658	4220.655374	24.103603
134.658381	4238.336177	24.108621
134.678827	4244.664761	24.113639
135.027673	4254.594920	24.118656
135.686458	4250.762166	24.123674
135.335151	4246.877311	24.128691
135.323529	4256.455902	24.133709
135.923952	4244.247664	24.138727
135.601919	4247.472507	24.143744
135.960770	4255.726317	24.148762
136.044110	4263.566241	24.153779
136.021112	4280.577269	24.158797
136.079485	4267.428097	24.163815
136.310980	4271.360756	24.168832
136.450003	4267.131032	24.173850
136.322235	4273.782188	24.178867
136.413428	4296.682699	24.183885
136.916795	4288.165880	24.188903
136.929849	4303.245486	24.193920
136.910421	4296.465555	24.198938
137.156004	4310.914960	24.203955
137.415431	4311.742230	24.208973
137.738864	4324.651573	24.213991
137.915700	4321.951332	24.219008
137.909481	4320.892115	24.224026
137.915748	4334.000720	24.229043
138.147237	4317.114872	24.234061
138.623141	4311.004829	24.239079
138.228465	4313.999771	24.244096
138.306387	4325.150000	24.249114
138.458610	4331.558299	24.254131
138.864332	4341.105792	24.259149
139.246941	4328.082643	24.264167
138.940133	4338.861580	24.269184
139.378317	4328.637102	24.274202
139.583566	4334.357286	24.279219
139.848018	4327.577696	24.284237
139.836370	4318.814171	24.289255
139.829607	4329.608186	24.294272
139.901274	4334.306582	24.299290
139.521442	4338.086592	24.304307
139.786609	4342.477235	24.309325
140.212452	4347.279631	24.314343
140.267765	4355.925666	24.319360
140.539669	4352.562064	24.324378
140.617326	4348.184773	24.329395
140.532431	4358.494110	24.334413
140.753148	4371.416728	24.339431
140.559695	4388.127818	24.344448
140.706023	4383.865430	24.349466
141.141975	4394.186917	24.354483
141.173462	4400.945678	24.359501
141.474051	4406.815883	24.364519
141.483115	4410.786410	24.369536
141.946272	4420.332664	24.374554
142.340856	4449.223349	24.379571
142.114551	4444.630974	24.384589
142.206515	4438.185633	24.389607
142.448814	4442.921359	24.394624
142.879034	4441.105004	24.399642
142.797120	4453.023417	24.404659
142.794325	4448.000500	24.409677
142.958404	4447.483652	24.414695
142.946420	4467.413185	24.419712
142.993321	4450.816214	24.424730
143.339826	4470.454950	24.429747
143.276456	4480.010473	24.434765
143.753947	4478.876470	24.439783
143.635331	4498.609867	24.444800
144.055872	4491.858017	24.449818
144.073900	4512.881780	24.454835
143.808914	4506.844964	24.459853
144.672949	4504.588124	24.464871
144.135258	4519.591366	24.469888
144.388973	4530.319605	24.474906
144.726237	4537.005282	24.479923
144.671714	4541.732520	24.484941
144.869866	4547.189603	24.489959
144.968690	4557.313237	24.494976
145.445919	4576.194173	24.499994
145.514766	4560.660285	24.505011
145.808763	4564.280981	24.510029
146.110206	4552.942223	24.515047
146.075797	4563.957936	24.520064
146.389550	4558.479375	24.525082
146.460021	4573.573703	24.530099
146.299748	4577.989780	24.535117
146.731748	4588.201118	24.540135
146.408294	4586.185547	24.545152
146.723330	4592.245468	24.550170
146.909768	4593.396698	24.555187
146.720563	4595.079824	24.560205
147.166478	4607.494746	24.565223
147.114630	4617.972059	24.570240
146.957169	4619.351196	24.575258
147.353042	4637.734643	24.580275
147.336022	4651.814051	24.585293
147.862961	4646.861565	24.590311
148.107262	4664.512448	24.595328
148.200594	4669.480468	24.600346
148.505706	4677.101171	24.605363
148.438989	4679.468838	24.610381
148.845532	4670.665163	24.615399
148.400914	4692.907552	24.620416
148.781198	4700.605174	24.625434
149.234985	4704.780983	24.630451
149.221770	4713.094384	24.635469
149.401557	4698.592856	24.640487
149.471143	4727.287331	24.645504
149.486721	4725.063491	24.650522
149.887060	4741.596120	24.655539
150.106301	4734.720501	24.660557
149.895616	4741.980595	24.665575
150.112982	4763.681716	24.670592
150.333828	4754.374244	24.675610
150.583436	4771.344730	24.680627
150.679467	4784.481116	24.685645
151.153030	4789.341345	24.690663
151.192033	4789.616939	24.695680
151.563346	4786.408095	24.700698
151.588847	4786.309028	24.705715
151.345091	4793.426528	24.710733
151.831048	4789.315186	24.715751
151.625477	4813.332909	24.720768
151.663130	4810.752321	24.725786
152.127777	4811.969339	24.730803
151.936661	4814.084676	24.735821
152.465431	4837.024815	24.740839
152.495387	4836.301994	24.745856
152.788107	4840.655354	24.750874
153.463112	4823.414214	24.755891
153.294804	4833.862265	24.760909
153.698061	4823.932511	24.765927
153.677717	4824.664399	24.770944
153.706460	4827.005853	24.775962
154.104137	4824.305707	24.780979
153.856872	4824.477483	24.785997
153.631291	4831.012326	24.791015
153.986815	4850.511681	24.796032
154.205784	4844.057710	24.801050
154.420634	4858.552679	24.806067
154.343505	4852.180534	24.811085
154.629018	4853.978365	24.816103
154.541749	4869.096576	24.821120
154.721008	4865.210336	24.826138
154.917586	4874.301434	24.831155
154.909332	4876.323113	24.836173
154.973900	4896.694146	24.841191
155.499480	4907.328177	24.846208
155.934129	4900.092448	24.851226
156.012526	4900.736220	24.856243
155.888361	4901.898457	24.861261
156.278218	4911.057093	24.866279
155.946219	4920.725751	24.871296
155.831134	4928.966624	24.876314
156.590412	4944.612305	24.881331
156.569587	4960.778883	24.886349
156.722249	4954.299250	24.891367
157.299675	4961.150576	24.896384
157.263416	4973.740247	24.901402
157.878959	4969.413884	24.906419
157.291415	4983.884309	24.911437
157.837195	4971.280623	24.916455
157.881627	4967.010716	24.921472
157.918702	4991.045890	24.926490
158.166792	4989.503172	24.931507
158.666165	5004.321868	24.936525
158.384977	5011.757753	24.941543
158.563437	5002.961932	24.946560
158.676906	5010.522115	24.951578
158.874535	5021.707280	24.956595
159.051172	5043.862933	24.961613
159.319776	5048.010157	24.966631
159.161008	5048.896291	24.971648
159.419272	5066.259080	24.976666
159.904056	5063.971384	24.981683
159.937580	5066.424610	24.986701
159.897867	5081.794275	24.991719
160.238259	5086.253391	24.996736
160.603078	5086.795645	25.001754
160.691638	5083.075640	25.006771
160.814354	5097.464387	25.011789
161.065321	5076.862984	25.016807
161.321535	5101.014438	25.021824
161.159119	5117.229726	25.026842
161.376940	5124.789061	25.031859
161.328573	5125.082528	25.036877
161.413702	5124.109382	25.041895
161.905723	5130.478009	25.046912
162.072054	5135.163927	25.051930
162.466176	5140.339818	25.056947
162.335248	5148.064125	25.061965
162.399527	5141.913966	25.066983
162.702959	5148.455850	25.072000
162.617742	5151.878343	25.077018
162.937107	5153.889513	25.082035
163.494625	5170.111211	25.087053
163.307583	5164.802753	25.092071
163.214737	5163.850904	25.097088
163.299299	5166.189806	25.102106
163.475219	5174.735276	25.107123
163.543987	5193.650676	25.112141
163.538767	5203.332707	25.117159
163.878548	5207.507176	25.122176
164.026139	5223.431634	25.127194
163.926481	5226.670788	25.132211
164.281294	5238.712150	25.137229
164.471780	5255.830296	25.142247
164.950376	5248.238887	25.147264
165.096995	5258.284582	25.152282
165.417567	5278.086663	25.157299
165.519217	5279.050863	25.162317
166.005250	5288.387927	25.167335
166.324683	5279.278386	25.172352
166.027307	5279.348018	25.177370
166.171188	5281.288065	25.182387
166.337969	5288.976776	25.187405
166.308845	5300.557831	25.192423
166.310417	5296.270275	25.197440
166.701558	5309.659806	25.202458
167.070011	5318.206128	25.207475
167.105653	5330.936471	25.212493
167.205962	5325.353992	25.217511
167.656862	5321.744504	25.222528
167.603008	5349.958751	25.227546
167.487479	5339.245223	25.232563
168.088953	5346.504342	25.237581
168.007107	5354.619000	25.242599
168.319143	5365.303939	25.247616
168.365848	5379.657094	25.252634
168.669598	5373.481241	25.257651
168.615523	5376.289128	25.262669
168.822577	5383.023493	25.267687
169.221598	5402.870663	25.272704
169.047522	5403.643613	25.277722
169.470138	5408.579833	25.282739
169.521176	5440.883325	25.287757
169.649309	5437.271780	25.292775
169.954787	5440.739033	25.297792
170.256921	5451.726135	25.302810
170.683632	5457.818174	25.307827
170.529360	5467.804999	25.312845
170.666472	5466.524595	25.317863
171.092804	5459.709236	25.322880
171.135080	5458.713008	25.327898
171.226110	5459.839400	25.332915
171.673306	5466.766804	25.337933
171.730562	5478.619012	25.342951
171.820453	5487.601630	25.347968
171.739846	5488.933189	25.352986
171.971091	5489.665114	25.358003
171.860403	5485.094095	25.363021
171.892506	5510.542261	25.368039
172.425917	5515.545816	25.373056
172.442490	5524.075989	25.378074
172.641669	5520.687535	25.383091
173.013444	5541.385735	25.388109
172.813584	5546.897217	25.393127
173.287905	5543.378347	25.398144
173.190674	5562.540968	25.403162
173.330969	5569.926446	25.408179
173.830699	5574.488540	25.413197
173.508990	5583.209576	25.418215
174.179529	5597.409188	25.423232
174.345368	5595.510558	25.428250
174.441553	5607.216628	25.433267
174.825703	5604.271474	25.438285
174.948526	5620.970504	25.443303
175.264230	5626.124458	25.448320
175.397585	5614.608718	25.453338
175.504331	5618.895989	25.458355
175.796334	5620.736939	25.463373
175.405707	5634.584989	25.468391
175.843099	5645.357925	25.473408
175.827379	5652.560628	25.478426
176.090677	5659.897430	25.483443
176.414704	5680.636482	25.488461
176.388948	5678.530803	25.493479
176.591621	5687.018810	25.498496
176.466709	5708.896273	25.503514
177.018429	5709.476411	25.508531
177.369778	5709.660523	25.513549
177.452213	5737.301504	25.518567
177.889740	5736.847221	25.523584
178.189367	5725.920884	25.528602
178.133514	5728.964350	25.533619
178.137908	5736.336965	25.538637
178.382041	5755.557120	25.543655
178.841837	5743.431445	25.548672
178.692508	5763.076239	25.553690
179.211642	5760.334534	25.558707
179.392166	5755.808256	25.563725
179.161447	5774.964903	25.568743
179.560045	5780.792502	25.573760
179.659935	5780.764174	25.578778
179.553287	5790.899393	25.583795
180.018989	5807.831116	25.588813
180.130903	5817.777307	25.593831
180.146553	5804.417227	25.598848
180.257597	5821.811465	25.603866
180.382385	5834.316400	25.608883
180.784431	5833.700200	25.613901
180.607357	5859.830582	25.618919
181.001867	5853.474061	25.623936
181.324717	5867.435140	25.628954
181.448645	5873.889537	25.633971
181.390028	5877.442486	25.638989
181.710447	5886.508960	25.644007
181.798427	5893.493844	25.649024
181.686648	5906.497582	25.654042
182.211878	5921.507409	25.659059
182.502041	5922.481717	25.664077
182.708023	5944.358692	25.669095
183.020682	5928.412365	25.674112
183.395914	5942.693230	25.679130
183.204997	5959.146858	25.684148
183.778092	5943.321841	25.689165
184.093597	5952.485907	25.694183
184.719440	5931.521436	25.699200
184.423108	5947.106788	25.704218
184.471036	5946.134014	25.709236
184.728652	5937.590146	25.714253
184.461613	5959.050860	25.719271
184.729571	5966.709632	25.724288
185.236678	5962.614272	25.729306
185.136791	5974.757065	25.734324
185.474556	5978.393955	25.739341
185.430163	5997.169510	25.744359
185.591376	5999.848780	25.749376
185.629821	6003.437420	25.754394
185.557303	6021.920893	25.759412
186.180966	6021.430631	25.764429
185.964708	6044.402556	25.769447
186.298378	6055.473984	25.774464
186.577855	6060.394701	25.779482
186.634462	6083.047820	25.784500
187.070996	6089.048870	25.789517
187.153514	6092.058547	25.794535
187.446043	6112.756814	25.799552
187.629383	6112.562553	25.804570
187.706895	6118.252666	25.809588
188.074813	6133.830644	25.814605
188.317625	6145.276167	25.819623
188.482530	6150.948426	25.824640
188.985929	6150.041482	25.829658
188.823263	6164.132970	25.834676
188.981973	6170.611847	25.839693
188.671088	6177.585723	25.844711
189.390019	6189.687036	25.849728
189.722231	6194.400344	25.854746
189.491337	6211.344473	25.859764
189.950933	6199.579575	25.864781
189.910605	6219.548255	25.869799
190.405318	6225.681700	25.874816
190.279959	6232.280639	25.879834
190.582528	6254.941222	25.884852
191.043242	6256.199125	25.889869
191.126364	6265.652199	25.894887
191.353545	6266.464276	25.899904
191.518821	6250.740149	25.904922
191.244479	6282.021094	25.909940
191.846269	6284.066856	25.914957
191.654754	6291.601586	25.919975
192.127213	6299.588257	25.924992
192.320175	6316.698589	25.930010
192.529273	6317.942331	25.935028
192.628986	6335.358650	25.940045
192.612930	6336.938833	25.945063
192.916821	6346.571541	25.950080
193.483768	6360.966221	25.955098
193.420501	6376.459003	25.960116
193.744443	6385.137355	25.965133
193.863959	6384.809291	25.970151
193.854432	6386.305041	25.975168
194.242770	6394.264266	25.980186
194.416428	6400.172038	25.985204
194.993060	6407.256273	25.990221
195.190161	6421.780004	25.995239
195.248729	6415.724637	26.000256
195.619188	6422.582124	26.005274
195.319841	6429.213611	26.010292
195.850310	6424.110503	26.015309
196.489377	6429.779649	26.020327
196.208579	6443.857194	26.025344
196.661197	6439.022189	26.030362
196.606776	6441.111236	26.035380
196.906555	6445.955679	26.040397
196.878353	6450.001146	26.045415
196.863357	6458.557349	26.050432
197.630801	6462.199021	26.055450
197.291534	6472.913872	26.060468
197.526512	6471.737367	26.065485
197.842375	6487.767753	26.070503
198.083696	6503.952444	26.075520
198.367617	6497.274189	26.080538
198.274585	6508.824683	26.085556
198.431621	6514.181272	26.090573
198.715988	6536.251973	26.095591
198.626420	6536.423793	26.100608
199.016472	6546.710856	26.105626
198.818781	6562.362161	26.110644
199.383404	6582.769089	26.115661
199.775990	6599.028112	26.120679
199.557831	6597.875854	26.125696
200.131066	6611.368932	26.130714
200.366908	6617.472223	26.135732
200.815502	6613.852571	26.140749
201.041090	6637.946130	26.145767
200.712725	6637.033308	26.150784
201.316495	6641.050447	26.155802
201.137437	6650.532195	26.160820
201.294941	6652.731461	26.165837
201.873069	6678.439185	26.170855
201.805755	6674.313272	26.175872
202.081746	6688.244838	26.180890
202.191132	6702.051922	26.185908
202.201132	6704.611452	26.190925
202.488252	6713.942595	26.195943
202.582754	6725.782000	26.200960
203.096651	6715.181903	26.205978
203.119726	6738.388965	26.210996
203.292502	6754.232385	26.216013
203.501558	6758.019025	26.221031
203.714404	6772.001651	26.226048
203.826566	6768.117746	26.231066
204.324282	6785.720546	26.236084
204.280385	6793.927502	26.241101
204.834799	6806.544147	26.246119
204.725794	6823.899907	26.251136
205.178378	6815.483380	26.256154
204.968334	6841.254898	26.261172
205.460919	6847.023094	26.266189
205.767381	6858.935812	26.271207
205.916015	6870.905175	26.276224
205.794825	6879.748418	26.281242
205.942799	6892.718687	26.286260
206.726080	6893.290289	26.291277
206.678536	6908.248469	26.296295
206.825553	6915.312544	26.301312
207.427441	6919.772234	26.306330
207.462961	6946.193216	26.311348
207.846292	6937.280187	26.316365
208.211206	6940.333133	26.321383
207.930153	6965.793607	26.326400
208.552030	6963.269773	26.331418
208.603785	6967.544962	26.336436
208.650607	6959.679281	26.341453
209.029349	6978.566430	26.346471
209.126967	6985.691917	26.351488
209.276184	6991.879986	26.356506
209.080963	7001.313392	26.361524
209.375459	7016.656960	26.366541
209.719436	7020.788799	26.371559
209.673291	7050.791069	26.376576
209.688233	7050.766056	26.381594
210.357606	7065.794987	26.386612
210.446788	7079.573386	26.391629
210.619736	7091.494991	26.396647
210.834332	7102.844261	26.401664
211.657819	7111.204999	26.406682
211.555239	7120.043844	26.411700
211.632066	7131.699922	26.416717
212.010790	7131.011078	26.421735
212.153158	7137.772298	26.426752
212.314363	7162.585091	26.431770
212.607378	7166.698345	26.436788
213.088725	7153.979569	26.441805
213.260265	7164.361700	26.446823
213.088902	7175.647462	26.451840
213.380825	7175.287174	26.456858
213.415103	7190.106706	26.461876
213.330663	7195.979628	26.466893
213.760762	7211.868274	26.471911
214.038021	7230.050431	26.476928
214.302228	7239.808072	26.481946
214.491999	7254.449451	26.486964
214.911577	7258.083848	26.491981
214.875571	7261.687025	26.496999
214.963809	7292.840691	26.502016
215.152473	7291.994098	26.507034
215.472124	7297.449360	26.512052
215.124539	7326.827532	26.517069
216.155108	7328.004910	26.522087
216.038384	7349.686001	26.527104
216.454343	7356.358854	26.532122
216.678665	7370.154531	26.537140
216.828020	7384.730095	26.542157
217.068663	7393.414457	26.547175
217.402335	7404.606496	26.552192
217.760022	7405.164939	26.557210
218.093066	7402.597389	26.562228
218.488627	7430.377298	26.567245
219.042234	7421.015105	26.572263
218.997558	7436.526486	26.577280
218.636308	7425.288049	26.582298
218.981349	7437.653007	26.587316
219.523248	7460.747009	26.592333
219.574569	7453.424822	26.597351
219.571228	7457.806502	26.602368
220.065858	7469.143667	26.607386
220.301231	7485.822926	26.612404
219.999074	7492.947089	26.617421
220.559151	7495.862031	26.622439
220.994933	7510.535254	26.627456
221.053676	7516.492481	26.632474
221.132290	7522.998100	26.637492
221.398488	7530.988432	26.642509
221.943894	7542.652742	26.647527
221.598469	7551.566753	26.652544
221.868154	7546.917926	26.657562
221.849921	7571.409878	26.662580
222.071755	7579.179919	26.667597
222.718030	7597.422505	26.672615
222.726928	7606.559379	26.677632
222.720302	7624.500880	26.682650
223.073187	7631.129624	26.687668
223.342369	7641.962320	26.692685
223.447066	7659.224399	26.697703
223.695935	7666.500773	26.702720
223.842741	7694.760670	26.707738
224.450281	7693.230404	26.712756
224.135272	7700.193054	26.717773
224.972857	7716.752958	26.722791
225.069273	7718.360991	26.727808
225.191258	7732.730393	26.732826
225.622942	7752.409505	26.737844
225.754109	7750.415420	26.742861
226.326370	7749.622521	26.747879
226.289001	7760.191021	26.752896
226.507681	7777.655376	26.757914
226.863966	7776.696269	26.762932
226.856650	7774.838349	26.767949
226.974607	7779.372313	26.772967
227.504411	7804.901653	26.777984
227.366612	7803.319465	26.783002
227.843430	7820.843430	26.788020
227.866988	7834.745509	26.793037
228.479369	7835.718154	26.798055
228.463715	7847.718433	26.803072
229.047672	7863.558072	26.808090
229.161912	7861.463596	26.813108
228.976098	7879.898203	26.818125
229.438024	7873.397109	26.823143
229.556236	7893.489902	26.828160
229.642154	7898.747390	26.833178
230.162404	7909.338826	26.838196
230.514025	7924.046336	26.843213
230.718436	7927.579871	26.848231
230.630369	7943.837537	26.853248
230.626816	7950.991420	26.858266
231.164761	7960.532005	26.863284
231.488009	7975.312545	26.868301
231.615430	7975.323103	26.873319
231.811004	7987.344111	26.878336
232.343287	7988.301211	26.883354
232.561378	7999.316993	26.888372
232.551981	8011.647666	26.893389
232.876492	8019.614804	26.898407
232.896563	8027.765032	26.903424
232.925825	8047.742386	26.908442
233.435578	8044.828674	26.913460
233.633316	8069.516378	26.918477
233.612960	8082.510592	26.923495
233.990193	8105.025197	26.928512
234.458682	8109.453807	26.933530
234.645747	8127.016461	26.938548
234.507422	8129.896525	26.943565
235.118807	8144.689523	26.948583
234.969117	8154.979569	26.953600
235.695156	8167.743916	26.958618
235.983723	8182.356298	26.963636
235.997715	8188.681307	26.968653
236.569086	8197.889388	26.973671
236.967126	8212.192425	26.978688
237.156544	8212.705340	26.983706
237.561476	8198.173944	26.988724
237.381786	8209.766326	26.993741
237.285519	8221.272239	26.998759
237.623001	8230.452321	27.003776
237.883565	8239.672997	27.008794
238.147333	8239.134629	27.013812
238.213799	8270.193097	27.018829
238.261313	8280.913673	27.023847
238.677510	8284.883282	27.028864
238.907927	8301.767258	27.033882
238.923381	8307.104581	27.038900
239.288403	8330.976441	27.043917
239.272236	8326.583824	27.048935
239.836289	8351.808854	27.053952
239.833977	8370.573619	27.058970
240.511534	8386.933176	27.063988
240.481268	8397.771676	27.069005
240.629785	8407.528861	27.074023
240.710400	8428.190975	27.079040
241.265895	8439.411385	27.084058
241.880400	8450.753015	27.089076
241.850379	8469.804806	27.094093
242.248568	8466.737265	27.099111
242.295605	8484.314796	27.104128
242.351284	8493.704422	27.109146
243.044615	8495.996375	27.114164
243.161174	8516.161091	27.119181
243.464712	8530.192295	27.124199
243.625794	8539.313348	27.129216
243.739939	8553.325982	27.134234
244.119484	8562.572743	27.139252
244.168830	8579.106630	27.144269
244.879619	8594.206062	27.149287
245.038566	8596.753188	27.154304
244.871472	8613.774070	27.159322
245.137146	8620.180316	27.164340
245.077582	8643.521557	27.169357
245.393648	8649.615263	27.174375
245.866590	8674.341538	27.179392
245.991941	8687.322492	27.184410
246.657713	8697.059568	27.189428
246.925765	8707.227528	27.194445
246.940766	8726.742234	27.199463
247.301489	8725.276403	27.204480
247.656701	8749.332267	27.209498
247.864515	8760.015829	27.214516
248.038759	8757.788910	27.219533
248.106534	8772.156942	27.224551
248.807006	8784.526166	27.229568
248.909712	8787.669305	27.234586
249.102868	8805.847131	27.239604
249.324912	8818.276918	27.244621
249.253184	8820.798694	27.249639
250.092145	8837.977345	27.254656
249.949835	8849.325049	27.259674
250.166194	8851.973232	27.264692
250.351071	8875.339603	27.269709
250.607517	8887.158848	27.274727
251.140892	8882.901148	27.279744
251.057030	8907.486806	27.284762
251.180985	8898.060787	27.289780
251.183982	8924.726532	27.294797
251.511388	8940.644423	27.299815
252.010124	8947.175362	27.304832
251.776891	8967.499928	27.309850
252.350285	8979.884067	27.314868
252.825694	8996.007408	27.319885
252.764541	9010.712554	27.324903
253.165532	9023.075820	27.329920
253.173195	9047.579051	27.334938
253.641364	9055.052496	27.339956
253.753641	9079.268017	27.344973
254.061693	9096.310094	27.349991
254.543918	9097.210337	27.355008
254.918084	9123.242043	27.360026
255.372828	9124.082931	27.365044
255.630357	9146.543835	27.370061
255.984656	9146.261699	27.375079
256.199684	9148.489156	27.380096
256.430257	9177.451443	27.385114
256.725345	9174.898307	27.390132
256.840955	9185.483166	27.395149
256.958241	9203.341105	27.400167
257.263622	9208.496397	27.405184
257.363175	9220.107208	27.410202
257.556158	9242.247653	27.415220
257.705226	9251.201480	27.420237
257.770545	9280.339429	27.425255
258.432743	9274.734360	27.430272
258.451779	9311.443888	27.435290
258.990049	9308.404211	27.440308
259.221608	9335.881359	27.445325
259.413088	9345.583915	27.450343
259.938162	9355.184902	27.455360
259.948627	9371.765997	27.460378
260.390815	9383.072075	27.465396
260.860633	9389.312729	27.470413
261.152759	9409.661556	27.475431
261.448751	9413.112387	27.480448
261.406737	9433.158828	27.485466
261.842764	9424.369706	27.490484
262.000261	9442.638192	27.495501
262.226998	9455.351445	27.500519
262.937480	9450.218241	27.505536
262.469518	9480.267854	27.510554
262.834827	9475.599651	27.515572
263.301209	9493.192965	27.520589
263.493235	9506.985545	27.525607
263.859614	9505.606876	27.530624
263.884179	9527.808824	27.535642
264.343205	9529.568964	27.540660
264.411719	9548.965650	27.545677
264.729030	9565.512209	27.550695
264.995868	9565.310899	27.555712
265.161282	9583.856472	27.560730
265.192984	9594.019829	27.565748
265.661603	9604.557367	27.570765
265.897275	9617.236677	27.575783
266.199536	9635.738072	27.580800
266.464893	9642.692512	27.585818
266.748066	9656.998728	27.590836
266.835970	9674.005344	27.595853
267.258868	9691.269413	27.600871
267.746683	9691.134390	27.605888
267.703481	9714.204381	27.610906
268.051613	9729.450529	27.615924
268.323550	9738.707703	27.620941
268.488187	9752.303422	27.625959
268.767376	9765.293447	27.630976
268.828555	9792.128521	27.635994
269.504977	9796.950624	27.641012
269.817998	9811.429684	27.646029
269.562551	9832.245678	27.651047
270.374878	9840.917068	27.656064
270.451763	9856.222324	27.661082
270.898557	9867.965181	27.666100
271.416939	9881.643914	27.671117
271.670817	9901.100431	27.676135
271.831006	9904.269269	27.681152
272.207841	9920.204330	27.686170
272.369324	9930.000185	27.691188
272.495230	9931.140645	27.696205
272.445554	9944.392577	27.701223
272.998716	9953.224569	27.706240
273.509681	9959.753616	27.711258
273.514352	9993.701790	27.716276
273.685413	9993.895838	27.721293
274.052796	10009.440210	27.726311
273.980080	10020.798165	27.731328
274.660040	10047.288348	27.736346
275.015030	10055.852558	27.741364
275.290458	10079.470398	27.746381
275.168647	10102.652673	27.751399
275.703049	10108.032251	27.756416
275.793003	10121.942399	27.761434
275.916599	10141.308643	27.766452
276.426505	10155.594146	27.771469
276.732764	10180.345557	27.776487
277.010982	10181.340959	27.781504
277.261237	10205.077117	27.786522
277.781514	10218.377727	27.791540
278.175464	10225.581866	27.796557
278.248122	10248.526003	27.801575
279.114064	10245.970224	27.806592
279.237268	10247.534522	27.811610
279.491647	10255.216181	27.816628
280.017713	10265.892980	27.821645
279.838087	10279.752994	27.826663
280.372805	10268.736690	27.831680
280.233893	10273.659412	27.836698
280.495759	10290.855017	27.841716
280.841339	10296.526428	27.846733
280.736271	10312.734287	27.851751
281.008262	10324.404246	27.856768
280.977936	10335.322852	27.861786
281.079257	10362.685321	27.866804
281.551470	10382.587708	27.871821
282.094875	10401.356166	27.876839
282.248420	10410.931284	27.881856
282.596430	10436.238356	27.886874
282.600511	10449.001327	27.891892
282.856316	10466.800917	27.896909
282.823739	10501.982667	27.901927
283.252922	10515.940625	27.906944
284.045137	10545.400748	27.911962
283.826078	10569.928442	27.916980
284.610815	10596.004294	27.921997
285.191469	10611.107248	27.927015
285.323980	10628.022054	27.932032
285.550069	10643.007637	27.937050
286.099579	10656.232756	27.942068
286.629346	10658.890723	27.947085
286.459541	10682.393578	27.952103
286.685466	10692.725431	27.957120
287.229452	10708.192404	27.962138
287.250855	10718.021729	27.967156
287.505861	10739.499338	27.972173
288.017316	10767.457445	27.977191
288.551108	10771.389313	27.982208
288.834001	10789.876335	27.987226
289.059038	10795.425495	27.992244
289.312386	10814.513005	27.997261
289.436075	10816.584107	28.002279
289.704789	10840.609907	28.007296
290.241774	10840.940813	28.012314
290.226076	10862.817075	28.017332
290.762331	10872.845781	28.022349
290.962368	10894.194256	28.027367
291.511013	10903.858992	28.032384
291.834549	10915.985128	28.037402
291.746119	10926.602169	28.042420
292.580385	10932.915631	28.047437
292.491208	10942.209473	28.052455
292.687780	10960.225283	28.057472
292.753725	10972.499557	28.062490
292.971862	10987.284888	28.067508
293.225765	11007.999277	28.072525
293.778205	11027.877141	28.077543
293.992214	11041.558632	28.082560
294.284701	11056.570640	28.087578
294.245032	11073.052604	28.092596
295.053255	11082.044905	28.097613
295.198273	11098.430169	28.102631
295.294422	11106.656515	28.107648
295.679671	11124.671959	28.112666
295.658236	11152.787739	28.117684
295.910726	11165.835179	28.122701
296.226194	11176.705964	28.127719
296.737875	11200.695185	28.132736
297.137908	11215.948742	28.137754
297.221616	11224.624156	28.142772
297.851574	11241.181758	28.147789
298.018970	11251.885350	28.152807
298.397662	11287.209180	28.157824
298.650402	11282.709085	28.162842
298.897410	11302.846132	28.167860
299.499561	11312.469157	28.172877
299.682613	11330.127900	28.177895
299.849093	11354.493297	28.182912
300.562832	11357.008739	28.187930
300.115649	11376.232238	28.192948
301.021417	11405.577578	28.197965
300.963578	11412.778362	28.202983
301.440195	11427.350567	28.208000
301.800508	11432.870925	28.213018
302.013475	11464.103115	28.218036
302.260167	11478.593180	28.223053
302.930445	11490.538980	28.228071
302.999226	11513.247588	28.233088
303.336332	11519.582311	28.238106
303.174912	11548.755291	28.243124
303.915285	11552.661525	28.248141
304.067638	11561.630770	28.253159
304.410400	11593.753915	28.258176
304.992008	11608.777844	28.263194
305.417805	11610.801294	28.268212
305.659827	11633.602884	28.273229
305.483294	11645.180482	28.278247
305.638195	11672.377810	28.283264
306.002366	11674.524425	28.288282
306.394034	11707.404224	28.293300
306.470583	11726.936628	28.298317
306.903247	11759.055240	28.303335
307.194542	11771.011303	28.308352
307.768419	11774.452631	28.313370
308.007782	11811.107560	28.318388
308.200209	11830.534266	28.323405
308.469571	11838.915208	28.328423
308.786924	11870.292156	28.333440
309.363858	11870.340081	28.338458
309.467759	11907.331259	28.343476
309.842753	11922.546238	28.348493
310.386019	11926.986125	28.353511
310.503454	11947.152951	28.358528
310.950581	11956.151790	28.363546
311.683411	11970.327152	28.368564
311.718202	11980.738762	28.373581
311.900267	11981.515078	28.378599
312.178513	12000.990501	28.383616
312.584977	12011.481409	28.388634
312.643544	12023.908828	28.393652
312.874544	12031.529800	28.398669
313.489704	12046.083672	28.403687
313.261980	12067.719220	28.408704
313.267261	12074.986995	28.413722
313.788887	12106.100873	28.418740
314.031485	12123.147776	28.423757
314.668136	12148.098081	28.428775
314.465172	12181.298005	28.433792
315.194000	12186.842545	28.438810
315.485423	12221.949111	28.443828
315.736917	12242.701787	28.448845
316.303720	12245.876360	28.453863
316.429359	12278.165042	28.458880
317.031977	12287.207770	28.463898
317.507546	12305.912098	28.468916
317.985020	12315.598343	28.473933
318.340242	12331.358781	28.478951
318.347496	12340.545630	28.483968
319.074810	12344.738291	28.488986
319.168306	12368.056581	28.494004
319.616989	12385.787952	28.499021
320.048093	12390.888501	28.504039
320.150927	12413.559188	28.509056
320.783011	12424.614565	28.514074
320.861201	12433.084948	28.519092
321.066197	12448.223662	28.524109
321.218164	12463.943832	28.529127
321.534336	12472.617543	28.534144
321.955252	12495.618598	28.539162
321.994154	12510.851143	28.544180
322.530784	12525.422720	28.549197
322.806321	12541.675409	28.554215
322.740840	12556.759352	28.559232
323.182640	12584.939138	28.564250
323.806817	12610.451220	28.569268
324.359753	12617.510361	28.574285
324.400507	12640.981710	28.579303
324.283895	12664.814853	28.584320
325.258529	12673.529535	28.589338
325.588760	12692.824013	28.594356
326.139747	12699.166469	28.599373
326.712994	12719.645574	28.604391
326.987573	12727.544682	28.609408
327.191829	12732.774184	28.614426
327.572028	12737.728303	28.619444
327.634848	12759.676060	28.624461
328.427893	12766.213336	28.629479
328.359451	12789.461667	28.634496
328.796639	12796.433478	28.639514
328.938108	12793.714152	28.644532
328.905381	12814.391703	28.649549
329.531997	12821.524203	28.654567
329.520129	12841.278749	28.659584
329.859497	12852.881493	28.664602
330.018824	12880.785326	28.669620
330.299404	12895.557855	28.674637
330.901982	12899.851826	28.679655
330.847251	12941.595552	28.684672
331.458269	12946.604451	28.689690
331.634005	12969.284816	28.694708
331.740926	12993.142861	28.699725
332.426732	13006.341252	28.704743
332.558758	13032.660362	28.709760
333.023104	13041.460728	28.714778
332.952342	13075.583697	28.719796
333.336470	13089.337532	28.724813
333.550740	13117.456779	28.729831
333.598590	13143.681664	28.734848
334.302535	13168.685114	28.739866
334.918131	13193.782776	28.744884
335.178511	13214.633167	28.749901
335.831774	13234.211568	28.754919
335.995087	13258.542756	28.759936
336.479340	13275.245862	28.764954
336.996293	13295.178231	28.769972
337.446161	13319.802304	28.774989
337.971385	13323.529017	28.780007
337.937250	13346.336864	28.785024
338.356952	13362.671358	28.790042
338.788303	13373.629359	28.795060
339.126723	13394.071834	28.800077
339.290314	13403.260974	28.805095
339.521031	13427.338861	28.810112
340.058381	13433.570656	28.815130
340.382315	13464.920738	28.820148
340.848540	13478.279300	28.825165
341.275555	13486.002398	28.830183
341.433987	13506.693518	28.835200
341.599865	13523.468304	28.840218
341.835989	13535.680341	28.845236
342.282905	13567.256814	28.850253
342.786285	13574.654115	28.855271
343.041295	13591.390959	28.860288
343.337355	13615.893032	28.865306
343.758311	13631.581380	28.870324
343.709613	13665.406585	28.875341
344.331219	13669.195754	28.880359
344.547094	13709.639827	28.885376
344.805052	13707.188685	28.890394
345.340775	13736.782333	28.895412
345.316260	13763.424409	28.900429
346.017562	13788.850821	28.905447
346.052370	13813.979894	28.910464
346.647273	13825.106186	28.915482
347.075007	13851.406248	28.920500
347.239632	13870.090738	28.925517
347.708437	13889.399682	28.930535
348.010691	13914.352775	28.935552
348.330763	13923.355630	28.940570
348.689542	13939.994456	28.945588
348.859935	13962.216967	28.950605
349.026685	13971.547732	28.955623
349.537748	13993.120021	28.960640
349.822180	14016.852298	28.965658
350.196761	14041.467502	28.970676
350.551538	14060.494636	28.975693
351.157264	14066.300475	28.980711
351.291242	14114.244726	28.985728
351.383971	14130.174821	28.990746
351.837598	14149.181687	28.995764
351.870977	14180.162356	29.000781
352.319898	14198.938806	29.005799
352.738069	14220.119357	29.010816
353.033640	14258.899265	29.015834
353.607360	14286.213904	29.020852
353.575828	14317.349346	29.025869
354.584579	14331.175084	29.030887
354.638909	14353.735761	29.035904
355.014040	14379.995333	29.040922
355.570117	14405.821602	29.045940
355.868143	14427.390676	29.050957
356.227079	14458.553715	29.055975
356.351449	14487.923720	29.060992
356.623105	14501.576916	29.066010
357.714325	14526.739034	29.071028
358.021585	14541.688883	29.076045
358.276609	14565.819013	29.081063
358.428894	14587.266600	29.086080
358.819056	14614.091441	29.091098
359.478927	14625.072182	29.096116
359.648989	14656.412832	29.101133
360.154100	14671.110766	29.106151
360.455931	14691.842336	29.111168
360.912396	14717.646734	29.116186
361.222588	14740.442032	29.121204
361.341973	14756.505995	29.126221
361.928492	14785.353529	29.131239
362.356780	14796.164369	29.136256
362.734007	14818.055438	29.141274
363.241242	14839.375471	29.146292
363.519242	14858.170431	29.151309
363.543830	14881.610219	29.156327
363.827236	14888.533515	29.161344
364.132847	14913.370613	29.166362
364.667778	14952.885075	29.171380
364.754170	14968.612775	29.176397
365.568168	14987.946133	29.181415
365.918097	15021.750759	29.186432
366.198459	15035.750008	29.191450
366.471308	15050.084119	29.196468
366.948917	15068.439064	29.201485
367.128257	15091.876159	29.206503
367.269442	15114.201139	29.211520
367.759063	15125.407852	29.216538
368.080905	15155.129857	29.221556
368.214190	15169.784307	29.226573
368.684848	15194.998416	29.231591
369.043636	15221.531366	29.236608
369.542846	15250.138931	29.241626
370.453344	15262.028297	29.246644
370.471017	15286.127034	29.251661
370.872147	15317.262076	29.256679
371.203939	15329.465817	29.261696
371.559018	15354.265243	29.266714
371.932074	15373.924229	29.271732
371.985713	15396.318678	29.276749
372.375019	15420.823846	29.281767
373.177987	15440.983567	29.286784
372.909153	15474.421571	29.291802
373.651080	15494.999565	29.296820
373.977177	15523.209930	29.301837
374.551245	15558.735546	29.306855
374.859010	15586.488812	29.311872
375.241655	15597.773933	29.316890
375.830957	15617.593413	29.321908
376.207025	15642.531270	29.326925
376.851337	15651.441261	29.331943
377.212885	15667.692147	29.336960
377.013751	15697.408782	29.341978
378.036261	15716.450049	29.346996
378.493050	15734.497564	29.352013
378.788739	15748.641648	29.357031
379.425893	15753.685316	29.362048
379.680501	15779.741548	29.367066
379.999744	15781.529072	29.372084
379.968016	15808.047633	29.377101
380.523314	15820.490307	29.382119
381.072103	15844.027616	29.387136
381.234717	15873.196781	29.392154
381.445794	15886.640639	29.397172
381.883485	15918.908850	29.402189
382.496741	15940.540630	29.407207
382.421627	15955.447506	29.412224
382.825702	15977.267959	29.417242
383.342642	15997.512085	29.422260
383.410391	16035.368095	29.427277
383.862860	16055.078970	29.432295
384.260256	16084.570799	29.437312
384.565548	16114.880368	29.442330
385.198964	16125.632205	29.447348
385.406314	16158.237476	29.452365
385.500845	16180.073204	29.457383
385.952870	16217.657633	29.462400
386.241379	16235.341384	29.467418
386.745622	16263.793574	29.472436
387.222970	16297.393437	29.477453
387.361302	16320.395121	29.482471
387.973157	16346.646818	29.487488
387.772183	16379.128487	29.492506
388.470143	16392.787669	29.497524
388.976815	16426.170085	29.502541
389.247677	16460.778747	29.507559
389.758294	16477.137917	29.512576
390.158554	16502.319440	29.517594
390.664816	16532.648685	29.522612
391.165112	16573.249062	29.527629
391.407463	16603.180214	29.532647
392.042735	16627.132342	29.537664
392.079700	16649.022686	29.542682
392.899606	16663.354507	29.547700
393.233708	16696.703210	29.552717
393.027592	16718.546968	29.557735
394.039811	16738.645242	29.562752
393.908835	16770.650108	29.567770
394.417651	16793.450367	29.572788
395.148717	16836.816256	29.577805
395.451015	16856.968968	29.582823
395.905798	16886.746361	29.587840
396.316350	16908.643278	29.592858
396.539856	16942.586639	29.597876
397.011761	16959.935048	29.602893
397.504958	16995.368232	29.607911
398.039145	17017.813052	29.612928
398.407103	17051.458666	29.617946
398.959923	17082.514363	29.622964
399.275307	17098.817327	29.627981
399.712271	17127.372772	29.632999
400.164837	17145.799156	29.638016
400.329023	17178.766970	29.643034
400.866706	17189.794235	29.648052
401.262629	17220.373103	29.653069
401.399718	17245.282657	29.658087
401.995878	17267.177078	29.663104
402.350285	17300.497673	29.668122
403.046592	17322.924584	29.673140
403.216538	17347.170078	29.678157
403.215774	17383.253680	29.683175
403.970992	17397.474072	29.688192
404.250144	17437.994855	29.693210
404.491928	17471.281408	29.698228
405.010603	17489.031783	29.703245
405.179071	17533.941521	29.708263
405.808815	17559.009274	29.713280
406.305933	17587.327068	29.718298
406.986490	17616.459314	29.723316
407.491995	17625.937227	29.728333
407.444628	17670.005448	29.733351
408.522239	17683.298421	29.738368
408.854702	17708.144520	29.743386
409.057782	17721.495594	29.748404
409.344949	17743.751524	29.753421
409.994696	17756.961574	29.758439
410.081443	17778.343652	29.763456
410.334638	17805.410650	29.768474
410.713413	17812.898186	29.773492
411.110094	17847.290119	29.778509
411.408604	17870.787453	29.783527
411.689736	17894.826336	29.788544
412.189777	17933.486759	29.793562
412.699839	17956.969212	29.798580
413.050730	17984.611472	29.803597
413.231958	18017.574618	29.808615
413.574296	18044.670741	29.813632
413.738206	18079.313065	29.818650
414.777342	18109.228824	29.823668
415.574951	18135.463620	29.828685
415.558390	18170.923847	29.833703
416.132816	18181.641065	29.838720
416.465117	18219.044934	29.843738
416.632185	18239.084983	29.848756
417.384237	18282.782881	29.853773
417.636343	18305.383382	29.858791
418.242148	18321.378181	29.863808
418.493551	18354.871000	29.868826
418.762754	18382.272271	29.873844
419.590626	18413.044700	29.878861
419.935456	18454.813546	29.883879
420.254121	18466.226032	29.888896
421.067900	18501.170850	29.893914
421.146052	18528.218975	29.898932
421.886664	18549.993582	29.903949
422.320499	18584.641267	29.908967
422.781416	18588.081326	29.913984
423.117473	18638.244824	29.919002
423.252816	18663.382919	29.924020
423.770453	18685.280648	29.929037
424.170830	18714.136388	29.934055
424.810304	18736.887602	29.939072
424.936113	18756.823478	29.944090
425.590088	18788.313335	29.949108
426.180518	18814.151988	29.954125
426.376833	18847.623152	29.959143
426.782461	18870.992533	29.964160
426.966245	18892.746116	29.969178
427.516309	18929.400462	29.974196
428.391486	18946.310077	29.979213
428.256921	18984.935859	29.984231
428.726133	19007.774838	29.989248
428.943733	19037.250074	29.994266
429.537286	19076.803379	29.999284
429.952706	19116.057606	30.004301
430.283663	19149.414657	30.009319
431.022786	19168.613164	30.014336
431.182960	19215.097032	30.019354
431.690500	19238.833806	30.024372
432.250035	19248.887592	30.029389
432.207070	19292.422098	30.034407
432.729757	19314.093134	30.039424
433.544672	19341.300871	30.044442
433.884299	19361.536533	30.049460
434.305402	19397.116041	30.054477
434.575827	19422.719287	30.059495
434.663086	19451.951500	30.064512
435.367180	19476.362857	30.069530
436.037054	19509.640298	30.074548
436.106499	19536.386824	30.079565
436.164819	19582.445872	30.084583
436.980850	19607.996344	30.089600
437.942606	19637.532102	30.094618
437.840912	19675.471645	30.099636
438.367840	19704.265750	30.104653
438.814353	19735.760271	30.109671
439.557130	19772.836318	30.114688
439.903576	19798.733598	30.119706
440.213260	19845.939661	30.124724
440.692832	19861.747890	30.129741
440.927408	19892.558343	30.134759
441.830790	19923.375682	30.139776
442.428034	19959.887136	30.144794
442.770079	19988.780129	30.149812
443.488600	20007.369925	30.154829
443.636032	20033.881239	30.159847
444.213872	20067.870654	30.164864
444.382714	20088.965640	30.169882
444.813854	20116.763882	30.174900
445.647011	20154.529249	30.179917
445.640755	20186.660651	30.184935
445.920827	20214.883566	30.189952
446.294416	20240.218546	30.194970
446.853422	20280.651358	30.199988
447.641239	20314.661796	30.205005
447.963201	20362.951029	30.210023
448.232761	20382.540852	30.215040
448.734707	20427.142198	30.220058
449.030111	20451.799359	30.225076
449.720247	20486.426190	30.230093
450.061778	20523.499052	30.235111
450.731666	20555.647111	30.240128
451.196018	20581.064256	30.245146
451.722878	20613.731735	30.250164
452.073765	20640.322695	30.255181
452.455935	20672.338079	30.260199
453.192084	20698.698442	30.265216
453.575804	20740.655431	30.270234
454.074682	20762.913451	30.275252
454.420372	20791.246258	30.280269
454.699645	20824.396595	30.285287
455.218273	20862.188198	30.290304
455.731607	20888.350102	30.295322
455.680514	20911.027895	30.300340
456.618081	20930.750976	30.305357
456.863127	20978.913795	30.310375
456.987737	20997.033188	30.315392
457.909572	21020.951191	30.320410
458.090777	21072.484379	30.325428
458.862534	21085.482342	30.330445
459.199354	21112.533892	30.335463
459.435044	21147.854371	30.340480
459.870010	21177.305705	30.345498
460.154574	21204.915033	30.350516
460.869035	21240.862299	30.355533
461.457521	21272.357774	30.360551
461.748189	21296.865817	30.365568
462.458550	21332.897819	30.370586
462.710224	21372.265711	30.375604
463.267391	21398.400222	30.380621
463.500208	21434.400653	30.385639
463.907705	21474.781152	30.390656
464.764469	21507.685777	30.395674
465.023810	21542.815944	30.400692
465.786423	21585.704364	30.405709
465.713317	21615.930113	30.410727
466.452703	21639.961615	30.415744
467.105350	21679.938163	30.420762
467.654060	21704.174192	30.425780
468.317983	21733.218764	30.430797
468.291072	21763.479964	30.435815
468.905353	21801.401137	30.440832
469.236603	21833.248232	30.445850
469.729445	21878.261929	30.450868
470.391676	21895.143329	30.455885
470.574666	21937.860445	30.460903
471.071766	21964.144079	30.465920
472.136217	22000.653588	30.470938
472.316741	22045.882126	30.475956
472.768478	22064.734647	30.480973
473.247068	22095.735008	30.485991
473.482973	22151.658014	30.491008
474.533011	22168.262916	30.496026
474.558354	22207.811509	30.501044
475.262867	22236.842672	30.506061
475.834095	22261.416205	30.511079
476.037166	22305.665307	30.516096
476.806996	22316.835075	30.521114
477.050260	22361.620570	30.526132
477.803290	22390.882136	30.531149
478.409430	22405.580408	30.536167
478.748935	22453.218403	30.541184
479.274434	22477.068684	30.546202
479.553577	22512.961816	30.551220
480.138580	22533.894942	30.556237
480.568857	22582.848310	30.561255
481.035010	22605.707218	30.566272
481.777610	22638.520570	30.571290
481.884400	22665.249544	30.576308
482.294621	22690.539331	30.581325
482.863663	22706.186545	30.586343
483.089630	22750.167827	30.591360
483.742602	22771.355073	30.596378
484.152793	22816.357843	30.601396
484.387156	22830.418721	30.606413
484.611024	22868.984344	30.611431
485.067438	22901.706798	30.616448
485.693985	22929.771097	30.621466
486.068527	22969.819649	30.626484
486.586166	23015.456430	30.631501
487.312144	23048.929365	30.636519
487.385594	23085.634729	30.641536
488.177693	23123.376387	30.646554
488.362309	23174.731996	30.651572
488.857276	23214.187021	30.656589
489.698041	23254.389636	30.661607
489.847391	23296.515619	30.666624
490.527714	23327.924971	30.671642
490.937127	23372.912908	30.676660
491.246862	23423.933554	30.681677
492.309632	23446.047258	30.686695
492.592657	23504.366665	30.691712
493.253799	23527.996081	30.696730
493.548715	23575.675280	30.701748
494.425580	23600.552708	30.706765
494.918318	23637.277614	30.711783
495.539530	23678.416562	30.716800
496.360059	23707.568217	30.721818
496.595053	23728.082958	30.726836
497.305945	23766.069871	30.731853
497.880571	23781.962225	30.736871
498.171162	23820.236770	30.741888
498.650362	23851.690233	30.746906
498.986676	23890.736651	30.751924
499.319918	23924.606401	30.756941
499.876651	23967.623113	30.761959
500.187888	24001.658791	30.766976
500.958183	24038.152946	30.771994
501.662571	24071.285705	30.777012
501.514954	24102.556758	30.782029
502.306430	24135.235474	30.787047
502.686978	24179.779756	30.792064
503.544447	24199.731215	30.797082
504.239675	24252.910398	30.802100
504.807252	24281.988413	30.807117
505.040584	24318.563246	30.812135
505.352052	24355.956713	30.817152
506.434702	24387.454521	30.822170
506.851796	24415.971512	30.827188
506.837222	24448.427196	30.832205
507.208288	24475.407773	30.837223
507.625123	24525.212895	30.842240
508.138369	24559.212071	30.847258
508.782383	24605.230293	30.852276
509.298170	24630.470918	30.857293
509.994204	24665.272214	30.862311
510.067432	24704.798137	30.867328
510.672372	24722.777934	30.872346
511.431987	24765.719590	30.877364
511.912001	24796.019247	30.882381
512.538158	24824.879398	30.887399
512.750336	24857.888990	30.892416
513.263669	24905.306587	30.897434
513.399422	24933.673190	30.902452
514.047523	24975.999077	30.907469
515.018298	25009.972804	30.912487
514.848988	25060.571676	30.917504
515.505698	25099.698417	30.922522
516.074978	25148.396522	30.927540
516.238436	25175.347556	30.932557
517.082301	25219.739017	30.937575
517.616922	25268.113743	30.942592
518.110202	25302.931406	30.947610
518.611690	25359.727716	30.952628
519.105442	25391.376478	30.957645
519.919218	25440.828192	30.962663
519.916352	25487.501064	30.967680
520.786043	25530.901463	30.972698
521.444028	25575.518886	30.977716
521.708314	25619.323188	30.982733
522.480296	25666.983068	30.987751
522.861645	25717.786970	30.992768
523.382032	25760.727669	30.997786
524.119005	25795.076688	31.002804
524.538968	25847.608681	31.007821
525.427665	25881.926627	31.012839
525.748844	25932.956642	31.017856
526.494750	25968.541384	31.022874
527.030999	26008.367802	31.027892
527.192551	26054.208682	31.032909
527.862599	26094.121923	31.037927
528.268324	26133.829225	31.042944
529.010470	26181.281121	31.047962
529.251077	26214.281897	31.052980
529.794499	26272.758228	31.057997
530.566073	26301.448213	31.063015
531.125672	26351.401722	31.068032
531.487364	26385.321799	31.073050
532.283309	26434.873177	31.078068
532.691847	26476.488091	31.083085
533.322699	26505.769638	31.088103
533.896606	26551.273678	31.093120
534.166466	26595.280645	31.098138
534.992917	26630.595638	31.103156
535.155566	26679.709812	31.108173
536.079398	26714.993722	31.113191
536.874826	26756.767526	31.118208
536.839502	26798.539853	31.123226
537.905483	26822.517762	31.128244
537.957624	26860.836009	31.133261
538.358429	26900.675194	31.138279
538.953281	26940.293706	31.143296
539.547502	26975.956062	31.148314
539.811998	27012.130313	31.153332
539.892379	27051.915350	31.158349
540.904598	27089.779472	31.163367
541.264275	27145.237065	31.168384
541.626754	27191.533688	31.173402
542.548939	27234.302463	31.178420
543.068928	27276.745450	31.183437
543.720995	27324.364767	31.188455
544.073566	27367.245117	31.193472
544.841309	27404.332742	31.198490
545.528505	27456.517818	31.203508
545.614519	27496.380262	31.208525
546.469853	27528.615371	31.213543
546.772076	27570.346170	31.218560
547.316513	27622.489923	31.223578
548.208371	27671.934516	31.228596
548.447478	27713.414177	31.233613
549.032709	27765.226515	31.238631
549.871706	27806.268932	31.243648
550.360015	27851.274250	31.248666
550.646741	27882.079313	31.253684
551.268214	27945.380386	31.258701
552.064467	27979.906643	31.263719
552.526812	28027.383358	31.268736
553.099177	28074.132039	31.273754
553.721193	28120.647619	31.278772
554.229932	28165.455958	31.283789
554.869379	28213.847294	31.288807
555.197254	28248.708733	31.293824
556.045274	28299.501610	31.298842
556.634298	28348.082591	31.303860
557.128859	28386.114957	31.308877
557.738318	28435.704575	31.313895
558.118755	28484.375919	31.318912
558.475455	28530.900276	31.323930
559.344609	28575.526281	31.328948
560.033514	28625.245645	31.333965
560.630949	28668.487543	31.338983
561.021272	28709.570639	31.344000
561.905439	28748.688965	31.349018
562.373630	28789.824469	31.354036
562.658403	28832.237320	31.359053
563.282805	28873.983198	31.364071
564.226502	28897.926971	31.369088
564.728505	28950.549783	31.374106
565.393482	28982.473816	31.379124
565.963725	29031.299364	31.384141
566.313568	29073.496050	31.389159
566.881440	29116.083588	31.394176
567.590884	29158.109756	31.399194
568.068542	29194.771025	31.404212
568.157692	29223.764823	31.409229
568.822384	29258.606304	31.414247
569.425862	29303.821878	31.419264
569.790703	29352.818210	31.424282
570.520355	29380.235278	31.429300
570.829520	29425.067865	31.434317
571.135554	29468.496991	31.439335
571.679167	29514.677654	31.444352
572.162659	29572.033001	31.449370
573.002611	29610.637270	31.454388
572.914378	29669.863181	31.459405
573.768355	29724.112317	31.464423
574.588362	29770.821727	31.469440
575.078374	29840.448370	31.474458
575.636117	29884.921149	31.479476
576.050001	29950.630116	31.484493
576.678624	29989.773236	31.489511
577.548588	30039.513800	31.494528
577.824854	30098.561865	31.499546
578.770619	30139.213408	31.504564
579.051453	30202.410509	31.509581
580.129701	30250.153368	31.514599
580.987960	30307.828261	31.519616
580.889541	30372.645028	31.524634
581.728998	30405.941931	31.529652
582.445965	30461.293295	31.534669
583.032827	30505.964855	31.539687
583.613079	30553.278892	31.544704
584.020917	30618.354827	31.549722
585.108483	30647.125941	31.554740
585.378663	30716.652657	31.559757
585.688996	30769.611321	31.564775
586.621464	30819.434145	31.569792
586.913887	30872.481097	31.574810
587.475142	30912.945237	31.579828
588.192388	30976.532861	31.584845
588.507525	31024.684795	31.589863
589.598676	31075.137167	31.594880
589.753659	31133.533760	31.599898
590.406934	31184.620427	31.604916
591.004849	31250.727687	31.609933
591.783274	31299.126571	31.614951
592.674122	31343.211426	31.619968
593.028559	31406.852207	31.624986
594.020383	31443.071003	31.630004
594.614280	31502.995536	31.635021
595.106984	31545.305104	31.640039
595.546780	31585.386786	31.645056
596.232307	31652.835548	31.650074
596.696601	31686.549438	31.655092
597.277536	31746.456436	31.660109
597.850666	31793.595527	31.665127
598.608499	31844.974937	31.670144
598.851820	31894.988035	31.675162
599.835461	31942.445159	31.680180
600.176481	31987.093728	31.685197
600.779689	32023.117228	31.690215
601.708662	32072.258828	31.695232
602.042447	32118.038971	31.700250
602.880212	32147.966835	31.705268
603.231226	32213.151147	31.710285
603.768326	32253.431740	31.715303
604.392478	32292.185488	31.720320
604.697304	32346.187212	31.725338
605.481963	32392.651274	31.730356
605.797291	32438.126325	31.735373
606.123768	32487.615736	31.740391
606.941751	32541.408702	31.745408
607.278554	32618.306085	31.750426
608.067554	32654.528347	31.755444
608.527466	32733.078961	31.760461
608.862178	32784.862850	31.765479
610.060700	32840.175508	31.770496
610.584743	32906.435178	31.775514
611.298868	32968.811059	31.780532
612.174229	33027.966551	31.785549
612.756643	33077.136408	31.790567
613.361141	33137.128260	31.795584
614.003312	33179.404046	31.800602
614.826642	33249.775466	31.805620
615.216938	33301.008330	31.810637
615.573597	33355.238384	31.815655
616.844596	33402.925076	31.820672
617.193598	33462.613609	31.825690
617.787717	33523.606277	31.830708
618.823274	33560.283054	31.835725
619.231809	33614.650712	31.840743
619.870385	33672.260522	31.845760
620.438437	33717.416701	31.850778
621.453190	33762.278030	31.855796
621.965274	33807.372437	31.860813
622.381828	33865.596772	31.865831
623.201522	33910.812707	31.870848
623.772298	33958.015118	31.875866
624.138524	34003.938771	31.880884
624.697840	34075.892639	31.885901
625.124443	34118.906615	31.890919
626.090253	34170.327942	31.895936
626.322335	34238.688645	31.900954
627.331981	34281.520338	31.905972
627.779083	34341.462813	31.910989
628.362654	34390.224975	31.916007
629.171147	34451.242092	31.921024
630.003062	34507.531428	31.926042
630.399987	34553.716540	31.931060
631.095320	34612.759781	31.936077
631.680383	34667.895683	31.941095
632.386127	34711.175705	31.946112
632.822897	34781.881610	31.951130
633.477137	34820.787839	31.956148
634.162882	34863.631638	31.961165
634.186907	34928.645430	31.966183
635.002917	34967.259831	31.971200
635.664597	35024.435583	31.976218
635.961831	35075.304116	31.981236
636.659968	35142.449855	31.986253
637.301878	35197.608414	31.991271
637.962274	35250.598231	31.996288
638.244852	35319.992611	32.001306
638.943521	35372.819081	32.006324
639.621245	35436.474342	32.011341
640.161378	35501.928394	32.016359
641.214533	35556.513462	32.021376
641.840820	35631.688784	32.026394
642.101451	35688.832948	32.031412
642.897522	35752.817389	32.036429
643.800898	35817.849096	32.041447
644.430476	35878.218915	32.046464
644.761994	35946.072629	32.051482
645.807741	36007.019837	32.056500
646.696809	36061.776153	32.061517
646.997646	36135.526833	32.066535
648.039502	36191.326525	32.071552
648.394750	36246.617761	32.076570
649.027411	36307.272410	32.081588
649.704922	36376.258300	32.086605
650.344586	36437.385259	32.091623
651.141333	36497.967173	32.096640
651.982155	36553.294027	32.101658
652.939842	36601.347251	32.106676
653.599727	36658.930909	32.111693
653.990969	36733.533770	32.116711
654.680393	36774.668194	32.121728
655.336971	36824.974028	32.126746
655.765161	36890.356752	32.131764
656.756025	36950.936195	32.136781
657.188714	37013.201813	32.141799
658.057784	37071.314835	32.146816
658.243249	37132.899772	32.151834
658.824990	37208.034091	32.156852
659.469234	37259.836224	32.161869
660.353680	37345.125093	32.166887
660.636800	37403.942724	32.171904
661.640670	37454.720152	32.176922
662.361180	37527.568210	32.181940
663.256079	37576.134021	32.186957
663.736107	37645.459294	32.191975
664.369356	37701.655456	32.196992
665.450064	37767.716541	32.202010
665.930776	37831.096956	32.207028
666.617886	37890.607169	32.212045
667.100707	37948.338544	32.217063
667.579401	38014.786572	32.222080
668.316931	38079.128206	32.227098
668.394345	38137.106103	32.232116
669.526063	38198.534791	32.237133
670.148552	38245.239707	32.242151
670.840361	38313.662098	32.247168
671.412345	38380.295374	32.252186
671.906672	38442.772472	32.257204
672.822824	38493.697876	32.262221
673.302456	38567.375568	32.267239
673.825383	38627.139996	32.272256
674.806619	38680.379688	32.277274
675.170940	38749.120883	32.282292
675.903232	38801.780944	32.287309
676.600840	38872.542979	32.292327
677.172482	38942.197991	32.297344
678.276992	38996.980035	32.302362
678.558481	39069.412717	32.307380
679.188358	39139.450306	32.312397
680.279140	39223.675155	32.317415
680.798664	39276.335887	32.322432
681.652515	39338.074719	32.327450
682.049675	39406.318241	32.332468
683.019911	39476.325100	32.337485
683.300483	39544.012209	32.342503
684.389749	39601.055050	32.347520
685.263802	39681.448768	32.352538
685.720594	39750.428437	32.357556
686.834527	39805.818681	32.362573
687.203789	39874.516348	32.367591
687.640528	39949.277551	32.372608
688.291765	40006.716338	32.377626
688.988657	40082.365465	32.382644
689.826506	40151.207240	32.387661
690.293108	40229.965423	32.392679
691.085723	40294.746657	32.397696
691.732272	40361.777955	32.402714
692.701220	40436.314632	32.407732
693.322791	40500.590898	32.412749
693.747541	40576.323401	32.417767
694.492899	40649.970975	32.422784
695.665506	40705.197120	32.427802
696.357773	40784.226277	32.432820
697.038711	40845.966587	32.437837
697.882517	40920.637274	32.442855
698.203602	40986.076533	32.447872
699.265881	41050.976976	32.452890
699.644994	41119.580323	32.457908
700.660432	41189.006719	32.462925
701.443218	41255.243974	32.467943
701.893301	41330.794438	32.472960
702.994667	41377.136834	32.477978
703.378675	41450.651435	32.482996
704.560939	41513.527034	32.488013
704.804869	41586.351723	32.493031
705.470532	41649.152379	32.498048
706.173584	41705.774909	32.503066
706.574703	41770.611471	32.508084
707.252355	41836.186447	32.513101
708.018811	41898.921507	32.518119
708.458833	41957.750429	32.523136
709.241990	42017.348128	32.528154
709.991837	42092.958308	32.533172
710.507721	42166.101721	32.538189
711.110497	42229.453869	32.543207
711.728227	42303.389102	32.548224
712.673340	42376.124419	32.553242
712.619496	42455.784757	32.558260
713.471188	42530.983226	32.563277
714.654532	42609.605122	32.568295
715.131622	42684.936457	32.573312
716.113391	42762.490336	32.578330
716.784969	42839.813228	32.583348
717.451717	42915.844001	32.588365
718.188635	42996.349279	32.593383
718.846521	43062.430456	32.598400
719.847351	43143.156204	32.603418
720.264612	43215.613224	32.608436
721.425175	43290.690132	32.613453
721.696432	43377.564170	32.618471
722.773158	43455.355243	32.623488
723.648813	43530.055877	32.628506
724.512552	43605.585175	32.633524
725.142124	43675.225020	32.638541
726.145816	43757.848969	32.643559
726.832484	43812.395997	32.648576
727.482393	43886.941701	32.653594
727.923725	43974.674896	32.658612
728.918040	44037.072339	32.663629
729.762350	44116.244032	32.668647
730.121044	44172.850651	32.673664
731.493815	44245.399592	32.678682
732.329354	44316.958695	32.683700
732.856739	44387.601879	32.688717
733.619789	44465.592552	32.693735
733.968812	44531.946189	32.698752
735.294749	44588.109946	32.703770
735.791471	44671.989314	32.708788
736.485354	44740.310910	32.713805
737.306864	44808.555672	32.718823
737.594806	44887.447232	32.723840
738.598209	44954.660448	32.728858
739.082966	45029.606451	32.733876
739.682644	45100.335664	32.738893
740.570116	45189.328914	32.743911
741.199146	45271.000781	32.748928
742.214047	45334.380721	32.753946
742.594825	45410.527922	32.758964
743.646274	45481.344491	32.763981
744.216131	45568.973790	32.768999
744.760807	45647.973037	32.774016
745.615045	45713.503072	32.779034
746.418527	45794.383016	32.784052
747.442348	45855.397367	32.789069
748.371818	45919.013874	32.794087
748.672641	45978.433874	32.799104
750.056638	46028.132042	32.804122
750.641326	46106.880923	32.809140
751.234986	46178.199111	32.814157
752.054086	46234.240673	32.819175
752.396844	46307.709922	32.824192
753.505995	46370.031218	32.829210
754.067610	46450.520494	32.834228
754.479977	46523.194001	32.839245
755.062983	46599.601286	32.844263
755.721875	46675.548824	32.849280
756.580288	46742.258843	32.854298
757.248707	46832.106165	32.859316
758.162986	46917.620903	32.864333
759.006510	46999.528567	32.869351
759.691525	47072.870815	32.874368
760.502401	47155.005252	32.879386
761.127389	47238.037298	32.884404
761.987646	47315.558300	32.889421
762.970326	47399.698371	32.894439
763.181164	47479.765494	32.899456
764.252746	47560.983218	32.904474
765.099713	47648.821752	32.909492
765.908997	47727.267663	32.914509
766.884334	47795.490145	32.919527
767.822411	47880.772308	32.924544
768.734624	47963.383438	32.929562
769.391799	48037.122226	32.934580
770.205733	48102.408899	32.939597
771.083669	48177.870563	32.944615
771.678071	48259.303154	32.949632
772.728911	48335.116589	32.954650
773.535089	48419.576763	32.959668
774.113368	48484.817178	32.964685
775.161894	48551.854037	32.969703
776.048983	48625.817416	32.974720
776.433336	48705.341861	32.979738
777.002695	48790.276939	32.984756
778.104798	48852.529295	32.989773
778.748154	48931.275181	32.994791
779.577869	49020.776685	32.999808
780.159370	49094.727570	33.004826
781.384715	49175.969281	33.009844
781.971743	49251.412427	33.014861
782.774084	49334.391401	33.019879
783.378395	49407.058869	33.024896
784.444094	49478.987391	33.029914
785.108659	49555.208342	33.034932
785.687202	49634.914303	33.039949
786.711260	49703.455107	33.044967
787.468774	49791.589909	33.049984
788.146024	49853.544234	33.055002
789.144254	49930.458373	33.060020
789.483379	50000.983729	33.065037
790.575742	50074.469245	33.070055
791.129957	50138.113421	33.075072
792.135867	50197.271310	33.080090
792.391700	50283.156466	33.085108
793.214116	50355.534338	33.090125
794.278747	50424.282891	33.095143
794.688716	50511.895962	33.100160
795.513274	50585.978455	33.105178
796.331255	50672.498633	33.110196
796.886362	50743.453269	33.115213
798.244589	50818.231217	33.120231
798.485002	50918.880891	33.125248
799.665085	50996.307154	33.130266
800.220415	51079.267323	33.135284
800.936899	51154.559082	33.140301
802.035134	51243.940675	33.145319
802.863256	51338.566384	33.150336
803.779686	51410.264554	33.155354
804.326747	51492.233891	33.160372
805.016811	51570.640046	33.165389
806.114507	51655.965443	33.170407
806.766637	51746.285251	33.175424
807.631416	51822.376728	33.180442
808.182939	51923.481144	33.185460
808.994845	52011.946464	33.190477
810.036356	52090.065412	33.195495
810.751170	52180.298530	33.200512
811.383917	52276.620294	33.205530
812.557934	52360.961723	33.210548
812.684398	52461.849642	33.215565
814.090019	52552.549046	33.220583
814.569977	52651.260952	33.225600
815.681086	52734.875652	33.230618
816.555666	52828.245738	33.235636
817.503948	52915.901641	33.240653
818.434151	53002.626661	33.245671
818.966437	53094.768108	33.250688
819.946266	53185.166068	33.255706
820.783137	53267.958978	33.260724
821.863835	53368.169849	33.265741
822.807118	53448.680570	33.270759
823.664879	53522.028223	33.275776
824.386269	53611.046041	33.280794
825.393645	53695.502310	33.285812
826.026528	53789.275646	33.290829
826.985779	53869.050309	33.295847
827.830202	53949.099256	33.300864
828.314687	54034.880730	33.305882
829.221405	54120.355527	33.310900
829.689395	54201.570191	33.315917
830.746821	54285.415248	33.320935
831.316465	54380.180149	33.325952
832.105211	54462.086648	33.330970
833.204628	54558.731370	33.335988
833.500441	54644.567852	33.341005
834.480518	54718.753094	33.346023
835.319128	54812.618916	33.351040
836.198290	54899.266464	33.356058
837.218367	54981.877076	33.361076
837.697363	55088.357657	33.366093
838.558131	55161.007590	33.371111
839.754517	55254.982881	33.376128
840.226421	55329.099993	33.381146
841.419597	55420.570434	33.386164
841.737740	55513.269600	33.391181
843.030858	55598.734040	33.396199
843.507127	55690.900743	33.401216
844.126162	55794.718007	33.406234
845.203909	55886.164966	33.411252
846.212811	55985.824073	33.416269
846.657449	56077.880970	33.421287
847.419764	56186.434607	33.426304
848.528340	56276.808531	33.431322
849.073237	56374.700154	33.436340
849.774199	56477.655964	33.441357
851.272316	56581.662905	33.446375
852.280129	56695.373188	33.451392
852.546006	56794.608859	33.456410
853.779158	56886.077119	33.461428
854.841385	56975.293884	33.466445
855.676391	57073.607101	33.471463
856.601708	57169.418942	33.476480
857.790454	57270.312803	33.481498
858.573234	57366.454566	33.486516
859.080754	57459.433325	33.491533
860.446792	57559.160945	33.496551
861.008586	57652.488761	33.501568
861.967471	57748.029942	33.506586
863.103482	57841.406223	33.511604
863.924827	57929.696800	33.516621
864.474308	58024.452216	33.521639
865.151420	58130.410666	33.526656
865.899279	58225.312326	33.531674
866.908739	58313.300143	33.536692
867.444763	58414.910297	33.541709
868.649140	58520.629216	33.546727
869.757556	58626.332443	33.551744
870.235159	58728.976491	33.556762
871.038988	58830.325310	33.561780
871.771115	58935.562966	33.566797
872.831715	59044.739488	33.571815
873.681056	59148.643196	33.576832
874.355548	59246.330541	33.581850
875.739312	59347.810885	33.586868
876.368627	59467.129787	33.591885
877.383639	59560.398248	33.596903
878.491304	59658.735497	33.601920
879.039910	59761.086645	33.606938
880.164679	59863.113022	33.611956
880.567561	59954.548666	33.616973
881.656702	60039.090609	33.621991
882.422673	60132.594169	33.627008
883.328247	60237.682143	33.632026
884.332715	60335.922576	33.637044
884.962403	60430.096563	33.642061
885.942302	60517.512276	33.647079
886.815658	60613.523861	33.652096
887.378803	60730.884885	33.657114
888.570385	60831.027294	33.662132
889.468894	60930.866411	33.667149
890.147047	61025.610332	33.672167
890.920394	61136.373022	33.677184
891.914995	61246.580175	33.682202
892.982500	61335.706583	33.687220
893.688635	61445.405101	33.692237
894.657520	61557.629494	33.697255
895.603791	61670.846462	33.702272
896.665061	61781.797640	33.707290
897.433652	61877.027202	33.712308
898.584358	61983.162692	33.717325
899.625041	62089.597317	33.722343
900.064012	62205.973740	33.727360
900.732277	62312.096293	33.732378
902.113595	62409.728725	33.737396
903.070976	62525.310988	33.742413
903.764241	62625.633854	33.747431
904.683796	62743.689626	33.752448
905.135275	62849.158164	33.757466
906.215774	62959.459574	33.762484
907.151970	63079.453648	33.767501
908.106298	63197.876182	33.772519
909.233787	63307.294281	33.777536
910.180042	63417.632359	33.782554
911.367558	63525.510627	33.787572
912.404878	63637.828090	33.792589
913.341922	63741.200141	33.797607
914.388454	63849.450056	33.802624
915.239062	63962.370732	33.807642
916.408807	64054.714792	33.812660
917.445840	64156.437391	33.817677
918.278436	64249.215004	33.822695
918.827972	64362.779668	33.827712
919.935458	64481.697436	33.832730
920.989570	64573.001333	33.837748
921.486509	64682.436125	33.842765
922.284615	64792.992095	33.847783
923.677725	64900.873882	33.852800
924.295447	65009.189164	33.857818
925.151182	65113.835373	33.862836
926.323647	65223.165765	33.867853
927.236550	65329.992635	33.872871
928.134491	65441.003874	33.877888
929.022987	65542.909103	33.882906
929.967033	65616.145535	33.887924
930.814846	65736.555736	33.892941
931.633861	65830.941252	33.897959
932.866388	65927.664843	33.902976
933.667229	66020.013966	33.907994
934.340325	66129.593235	33.913012
935.221297	66235.571191	33.918029
935.890972	66324.452751	33.923047
937.069253	66431.297224	33.928064
937.585330	66550.072464	33.933082
938.462733	66653.479252	33.938100
939.328457	66771.508540	33.943117
939.759237	66884.510126	33.948135
941.141886	67004.849485	33.953152
941.858432	67136.833331	33.958170
942.625413	67251.599664	33.963188
943.642684	67381.146382	33.968205
944.701387	67497.257481	33.973223
945.578036	67637.033369	33.978240
946.524277	67763.868161	33.983258
947.565682	67880.947670	33.988276
948.454810	67997.534113	33.993293
949.069017	68136.660484	33.998311
950.659397	68252.580962	34.003328
951.851147	68376.853814	34.008346
952.667797	68497.245153	34.013364
954.053242	68620.357946	34.018381
954.867919	68736.360530	34.023399
956.137414	68848.349366	34.028416
957.090041	68982.904680	34.033434
958.245093	69088.879940	34.038452
959.256032	69191.227179	34.043469
960.100910	69305.926943	34.048487
960.961278	69420.599646	34.053504
962.177697	69536.018708	34.058522
963.049969	69646.862359	34.063540
963.773265	69762.664476	34.068557
965.013442	69880.981627	34.073575
965.798186	69993.736499	34.078592
966.799187	70115.555275	34.083610
967.951829	70229.023737	34.088628
969.071796	70353.781827	34.093645
969.626613	70473.291975	34.098663
970.954120	70577.794752	34.103680
971.659929	70701.047775	34.108698
972.345419	70817.474991	34.113716
973.444297	70921.826437	34.118733
974.732582	71046.966511	34.123751
975.893555	71163.964572	34.128768
976.451772	71291.326312	34.133786
977.633821	71399.236845	34.138804
978.835883	71513.848474	34.143821
979.400401	71635.385988	34.148839
980.849471	71740.279979	34.153856
981.623614	71865.557609	34.158874
982.340036	71966.664615	34.163892
983.190768	72085.701496	34.168909
984.010085	72176.481484	34.173927
985.177512	72279.521291	34.178944
985.868924	72408.069560	34.183962
986.783152	72518.524658	34.188980
987.912919	72631.789463	34.193997
988.593257	72752.468715	34.199015
989.951198	72864.839208	34.204032
990.578656	72992.257754	34.209050
991.667522	73112.033799	34.214068
992.520482	73244.454154	34.219085
993.603065	73355.272573	34.224103
994.696576	73485.324599	34.229120
995.367466	73611.128878	34.234138
996.362111	73725.072268	34.239156
997.571313	73853.825540	34.244173
998.234164	73983.816641	34.249191
999.467848	74114.368633	34.254208
1000.365346	74245.398350	34.259226
1001.475420	74376.976469	34.264244
1002.613245	74504.152858	34.269261
1003.409723	74641.463594	34.274279
1004.299396	74769.591126	34.279296
1005.313084	74907.848622	34.284314
1006.702044	75040.132412	34.289332
1007.752172	75168.243282	34.294349
1008.404736	75306.510424	34.299367
1009.574848	75433.605420	34.304384
1010.838423	75570.867158	34.309402
1011.743021	75705.463198	34.314420
1012.757758	75840.996880	34.319437
1013.481478	75972.672208	34.324455
1014.818246	76099.043407	34.329472
1015.763686	76240.284871	34.334490
1016.754346	76375.952375	34.339508
1017.901226	76505.674232	34.344525
1018.761623	76640.694333	34.349543
1020.035225	76767.850795	34.354560
1020.911093	76915.238379	34.359578
1022.215669	77044.856446	34.364596
1023.336363	77178.549436	34.369613
1024.314929	77317.214561	34.374631
1025.591907	77436.259669	34.379648
1026.005848	77583.934164	34.384666
1027.171037	77719.987390	34.389684
1028.542895	77831.062550	34.394701
1029.338453	77969.426265	34.399719
1030.888636	78103.429910	34.404736
1031.770077	78232.010488	34.409754
1032.601934	78353.666256	34.414772
1033.803513	78493.915626	34.419789
1034.620392	78627.179791	34.424807
1035.655296	78745.417797	34.429824
1036.930862	78875.425053	34.434842
1037.754843	79010.921755	34.439860
1039.118295	79117.637707	34.444877
1039.814642	79243.529887	34.449895
1040.772712	79357.308596	34.454912
1041.756856	79477.872296	34.459930
1043.049038	79598.229679	34.464948
1044.195755	79707.606320	34.469965
1044.987332	79831.186167	34.474983
1045.931061	79951.329255	34.480000
1047.133126	80073.770702	34.485018
1047.936496	80191.238472	34.490036
1049.273475	80320.960672	34.495053
1049.814839	80462.080731	34.500071
1051.022421	80588.563525	34.505088
1051.885825	80713.850260	34.510106
1053.091098	80851.270626	34.515124
1054.419781	80981.308036	34.520141
1055.089526	81124.814262	34.525159
1056.291593	81246.775929	34.530176
1057.472933	81372.389032	34.535194
1058.167313	81521.798231	34.540212
1059.419757	81655.113841	34.545229
1060.408646	81800.818085	34.550247
1061.225359	81937.706926	34.555264
1062.315322	82083.966013	34.560282
1063.361218	82229.120533	34.565300
1064.368132	82377.190228	34.570317
1065.201098	82518.505461	34.575335
1066.272275	82665.511256	34.580352
1067.288465	82815.611867	34.585370
1068.086397	82972.392524	34.590388
1069.554450	83125.438995	34.595405
1070.565337	83275.594325	34.600423
1071.428630	83442.009044	34.605440
1072.566135	83587.360729	34.610458
1074.144969	83735.589301	34.615476
1075.528045	83896.525897	34.620493
1076.262322	84055.404753	34.625511
1077.395036	84194.508784	34.630528
1078.698965	84347.653502	34.635546
1079.584341	84483.789399	34.640564
1081.108179	84622.897267	34.645581
1082.202236	84782.988845	34.650599
1083.127644	84924.558465	34.655616
1084.536223	85070.471581	34.660634
1085.338259	85210.109096	34.665652
1086.553501	85363.193098	34.670669
1087.526007	85509.380927	34.675687
1088.650806	85647.680176	34.680704
1089.722772	85795.055456	34.685722
1090.534142	85950.237520	34.690740
1091.622493	86087.628637	34.695757
1092.978920	86243.573393	34.700775
1093.664986	86397.893459	34.705792
1094.938161	86541.732721	34.710810
1096.182329	86670.895691	34.715828
1097.031380	86804.244876	34.720845
1097.840344	86961.299966	34.725863
1099.208363	87084.356664	34.730880
1100.229988	87234.690136	34.735898
1101.158621	87374.062464	34.740916
1102.309804	87508.392333	34.745933
1103.773271	87657.918684	34.750951
1104.305015	87805.387455	34.755968
1105.408784	87963.446343	34.760986
1106.296026	88106.946501	34.766004
1107.356755	88256.161677	34.771021
1108.328252	88419.581914	34.776039
1109.547265	88583.368727	34.781056
1110.717036	88739.051499	34.786074
1111.874250	88895.255927	34.791092
1113.157633	89043.068916	34.796109
1114.242952	89210.688587	34.801127
1115.455699	89379.124022	34.806144
1116.665676	89535.723082	34.811162
1117.412005	89688.488892	34.816180
1118.726285	89850.088430	34.821197
1119.830491	90015.105883	34.826215
1120.902725	90178.567654	34.831232
1122.350142	90336.709397	34.836250
1123.262430	90495.563486	34.841268
1124.347477	90663.124851	34.846285
1125.224892	90826.059623	34.851303
1126.428018	90988.254467	34.856320
1128.011824	91158.440744	34.861338
1129.299056	91330.945942	34.866356
1130.879217	91484.483451	34.871373
1132.009678	91629.656824	34.876391
1132.840798	91799.841316	34.881408
1134.237218	91945.315999	34.886426
1135.091349	92099.801799	34.891444
1136.425825	92260.745570	34.896461
1137.420647	92426.253993	34.901479
1138.500208	92586.892839	34.906496
1139.806993	92742.917627	34.911514
1140.856509	92893.532498	34.916532
1142.181021	93052.997325	34.921549
1143.308858	93218.370366	34.926567
1144.236159	93389.317145	34.931584
1145.608850	93527.102326	34.936602
1146.759716	93697.775582	34.941620
1147.898394	93856.055032	34.946637
1149.326581	94009.868342	34.951655
1150.739566	94164.507401	34.956672
1152.046021	94321.239132	34.961690
1152.613846	94477.399991	34.966708
1154.252564	94624.827245	34.971725
1155.185380	94764.701493	34.976743
1156.288615	94929.249926	34.981760
1157.368449	95079.242275	34.986778
1157.998002	95230.856969	34.991796
1159.123807	95365.574375	34.996813
1160.272364	95521.422459	35.001831
1161.900767	95680.313807	35.006848
1162.905455	95814.534482	35.011866
1163.635324	95969.237754	35.016884
1164.791370	96116.277186	35.021901
1165.872625	96272.267702	35.026919
1166.975528	96427.591654	35.031936
1168.600036	96576.463646	35.036954
1169.540273	96729.361140	35.041972
1170.523707	96892.178110	35.046989
1171.734256	97039.512220	35.052007
1172.927019	97213.197788	35.057024
1173.950803	97372.987990	35.062042
1175.197963	97547.679638	35.067060
1176.171360	97702.305454	35.072077
1177.313043	97877.471897	35.077095
1178.469855	98048.265875	35.082112
1180.178180	98221.111706	35.087130
1180.909475	98389.888256	35.092148
1182.071014	98553.574515	35.097165
1183.532241	98717.878563	35.102183
1184.597628	98894.469426	35.107200
1185.769188	99063.415023	35.112218
1187.201657	99234.294258	35.117236
1188.536234	99392.277785	35.122253
1189.499614	99576.463052	35.127271
1190.433050	99747.956915	35.132288
1191.744019	99914.583712	35.137306
1192.973534	100090.354201	35.142324
1194.047526	100266.397511	35.147341
1195.620058	100439.598047	35.152359
1196.707901	100626.201449	35.157376
1197.836474	100784.474058	35.162394
1199.162499	100961.159580	35.167412
1200.445242	101142.282277	35.172429
1201.730964	101318.293616	35.177447
1202.898837	101494.325032	35.182464
1203.984647	101661.873401	35.187482
1205.136181	101842.307462	35.192500
1206.390313	102015.595744	35.197517
1207.684994	102183.076695	35.202535
1208.845558	102373.365115	35.207552
1210.342025	102548.422137	35.212570
1211.352770	102725.386355	35.217588
1212.964134	102898.801571	35.222605
1214.074816	103068.355606	35.227623
1215.275077	103251.735153	35.232640
1216.726337	103416.934767	35.237658
1218.044022	103582.485828	35.242676
1219.120411	103761.434344	35.247693
1220.325818	103933.390453	35.252711
1221.641321	104108.487916	35.257728
1222.872801	104263.224183	35.262746
1224.000750	104423.445274	35.267764
1225.049039	104580.788229	35.272781
1226.392715	104734.908592	35.277799
1227.205696	104890.386289	35.282816
1228.586219	105046.806246	35.287834
1229.667772	105210.666062	35.292852
1230.782683	105383.944401	35.297869
1231.612721	105546.378386	35.302887
1232.885472	105724.646087	35.307904
1234.110026	105904.270725	35.312922
1235.312091	106077.818713	35.317940
1236.309914	106256.159424	35.322957
1238.013206	106432.952731	35.327975
1238.664072	106620.964302	35.332992
1240.144122	106789.334498	35.338010
1241.398780	106982.796742	35.343028
1241.980235	107179.595215	35.348045
1243.582361	107355.898808	35.353063
1244.931982	107539.654839	35.358080
1246.262400	107749.439461	35.363098
1247.839143	107930.295407	35.368116
1248.720130	108097.314391	35.373133
1250.319961	108301.339641	35.378151
1251.405587	108487.771405	35.383168
1252.575066	108672.026733	35.388186
1254.096486	108871.316131	35.393204
1255.172654	109066.570328	35.398221
1256.781440	109261.488243	35.403239
1257.648883	109455.316702	35.408256
1259.290298	109647.827406	35.413274
1260.241713	109836.227646	35.418292
1261.749204	110037.611191	35.423309
1263.231768	110228.575713	35.428327
1264.184374	110423.259136	35.433344
1265.588961	110616.821537	35.438362
1267.018256	110795.228420	35.443380
1268.333448	110994.473030	35.448397
1269.980311	111165.973997	35.453415
1271.361655	111365.185780	35.458432
1273.092825	111542.543668	35.463450
1274.195837	111725.218510	35.468468
1275.315498	111906.176654	35.473485
1276.604486	112071.081765	35.478503
1277.783718	112264.439767	35.483520
1279.597332	112440.670598	35.488538
1281.305331	112610.038670	35.493556
1282.444324	112792.722011	35.498573
1283.680209	112963.395603	35.503591
1285.096967	113139.491934	35.508608
1286.368728	113304.692855	35.513626
1287.696699	113484.907758	35.518644
1288.693132	113658.017041	35.523661
1290.206962	113827.474925	35.528679
1291.350035	114006.583520	35.533696
1292.520145	114171.331559	35.538714
1294.406158	114320.438096	35.543732
1295.175086	114482.194319	35.548749
1296.337275	114636.741815	35.553767
1297.583875	114809.952237	35.558784
1298.874995	114953.446875	35.563802
1299.667982	115115.279317	35.568820
1300.590961	115287.303653	35.573837
1302.054408	115457.274360	35.578855
1303.225995	115644.063038	35.583872
1304.095974	115819.758662	35.588890
1305.543097	115996.598289	35.593908
1306.621391	116191.844989	35.598925
1308.013731	116382.478588	35.603943
1309.539144	116568.154219	35.608960
1310.614705	116747.812173	35.613978
1311.841727	116936.697165	35.618996
1312.763782	117147.993926	35.624013
1314.836357	117321.641046	35.629031
1315.945314	117522.508919	35.634048
1316.809431	117725.171081	35.639066
1318.484041	117932.334271	35.644084
1319.748412	118125.362861	35.649101
1321.253548	118314.783654	35.654119
1322.463139	118524.684786	35.659136
1323.918918	118717.820362	35.664154
1325.646215	118910.863570	35.669172
1326.676647	119118.309675	35.674189
1328.014530	119309.562577	35.679207
1329.365714	119507.279555	35.684224
1330.456444	119712.479378	35.689242
1332.021816	119917.839653	35.694260
1333.671382	120113.797877	35.699277
1335.086080	120314.341293	35.704295
1336.196932	120515.732393	35.709312
1337.589297	120710.577229	35.714330
1338.949033	120916.535298	35.719348
1340.320054	121124.595486	35.724365
1341.983983	121312.575532	35.729383
1343.288442	121514.532450	35.734400
1344.292653	121715.563468	35.739418
1345.822353	121914.017530	35.744436
1347.279138	122119.678333	35.749453
1348.198462	122321.955969	35.754471
1349.740316	122528.670298	35.759488
1351.463247	122726.428514	35.764506
1352.869181	122930.064621	35.769524
1353.592145	123141.663383	35.774541
1355.029163	123340.307545	35.779559
1356.803045	123540.786817	35.784576
1358.051896	123749.925706	35.789594
1359.490027	123947.586308	35.794612
1360.915417	124163.957863	35.799629
1362.499792	124354.138042	35.804647
1363.681057	124567.410514	35.809664
1365.267475	124757.643902	35.814682
1366.620885	124951.411556	35.819700
1367.351090	125143.519048	35.824717
1368.912889	125321.018029	35.829735
1370.205129	125509.162879	35.834752
1371.404357	125697.197160	35.839770
1372.619553	125887.041547	35.844788
1374.138136	126085.579110	35.849805
1375.389445	126276.433833	35.854823
1376.737235	126476.420097	35.859840
1377.704880	126675.150885	35.864858
1379.114676	126881.463796	35.869876
1380.518259	127092.884153	35.874893
1382.169952	127284.176341	35.879911
1383.718085	127497.527630	35.884928
1384.520233	127702.081224	35.889946
1386.370917	127915.565034	35.894964
1387.462562	128131.970715	35.899981
1388.665478	128343.153947	35.904999
1390.156399	128554.837746	35.910016
1391.762700	128771.179330	35.915034
1393.347116	128987.298066	35.920052
1394.298581	129217.568135	35.925069
1395.908627	129422.753543	35.930087
1397.810909	129646.820619	35.935104
1398.803702	129862.799527	35.940122
1399.744711	130082.994321	35.945140
1401.690897	130312.418612	35.950157
1403.138176	130508.795161	35.955175
1404.358770	130739.858549	35.960192
1405.794191	130969.724156	35.965210
1407.504777	131181.861846	35.970228
1408.741437	131409.076800	35.975245
1410.273520	131628.100277	35.980263
1411.761314	131849.894431	35.985280
1413.071778	132087.276669	35.990298
1414.518260	132298.691925	35.995316
1415.945181	132531.726388	36.000333
1417.445115	132746.379944	36.005351
1419.087653	132947.379654	36.010368
1420.940454	133169.620284	36.015386
1422.561966	133401.313293	36.020404
1424.010482	133609.823884	36.025421
1425.201868	133821.734491	36.030439
1426.944884	134032.203273	36.035456
1427.947344	134249.405282	36.040474
1429.655651	134461.770642	36.045492
1430.752255	134686.157882	36.050509
1432.000636	134907.760527	36.055527
1433.663147	135124.610847	36.060544
1434.904728	135350.374020	36.065562
1436.555306	135562.465251	36.070580
1437.874828	135790.272187	36.075597
1439.281917	136019.131383	36.080615
1440.850431	136224.423375	36.085632
1441.924523	136460.181492	36.090650
1443.454689	136656.156448	36.095668
1444.680421	136863.382809	36.100685
1446.169855	137070.365989	36.105703
1447.414733	137283.294556	36.110720
1448.287561	137505.901763	36.115738
1450.110147	137710.859715	36.120756
1451.335287	137935.188269	36.125773
1452.709951	138153.995047	36.130791
1454.491735	138377.541546	36.135808
1455.554259	138599.455251	36.140826
1456.834162	138836.859845	36.145844
1458.569759	139078.477257	36.150861
1459.796235	139302.777967	36.155879
1461.156688	139532.128184	36.160896
1462.355598	139770.997814	36.165914
1464.082538	140009.760103	36.170932
1465.340131	140258.826051	36.175949
1466.614856	140501.149220	36.180967
1468.047636	140744.868638	36.185984
1469.735327	140994.315916	36.191002
1471.440586	141241.329162	36.196020
1472.640014	141497.537123	36.201037
1474.249203	141735.381327	36.206055
1476.319056	141980.543023	36.211072
1477.647195	142223.239088	36.216090
1479.655932	142476.259647	36.221108
1481.001143	142717.917682	36.226125
1482.347453	142968.462075	36.231143
1484.220197	143196.681468	36.236160
1485.356358	143443.067950	36.241178
1487.286604	143689.507677	36.246196
1488.548189	143926.727124	36.251213
1490.330183	144172.459155	36.256231
1492.064922	144416.755728	36.261248
1493.042651	144657.460774	36.266266
1494.875538	144895.547511	36.271284
1496.693925	145134.589015	36.276301
1497.632913	145377.080317	36.281319
1499.635884	145617.680609	36.286336
1500.964241	145853.649355	36.291354
1502.716271	146100.478836	36.296372
1504.028835	146345.567483	36.301389
1505.423760	146580.466386	36.306407
1507.209411	146812.997972	36.311424
1508.091712	147061.621059	36.316442
1509.806814	147309.441956	36.321460
1511.267188	147551.195404	36.326477
1512.682807	147803.187480	36.331495
1514.597161	148050.234629	36.336512
1516.032961	148292.149749	36.341530
1517.581104	148537.927856	36.346548
1518.941713	148787.908243	36.351565
1520.487071	149029.912965	36.356583
1522.387004	149267.413641	36.361600
1523.757110	149509.906197	36.366618
1525.363836	149728.403571	36.371636
1526.793375	149963.905117	36.376653
1527.928726	150184.305967	36.381671
1529.749255	150409.733727	36.386688
1531.075866	150648.882300	36.391706
1532.616140	150870.960282	36.396724
1534.174975	151097.778208	36.401741
1535.001944	151344.465637	36.406759
1536.832282	151571.307113	36.411776
1538.118159	151817.164543	36.416794
1539.724662	152059.841452	36.421812
1541.408459	152305.005431	36.426829
1542.620896	152550.081311	36.431847
1544.312097	152798.341231	36.436864
1546.083225	153058.736062	36.441882
1547.552562	153301.241060	36.446900
1548.919469	153554.616831	36.451917
1550.226084	153817.589071	36.456935
1552.180311	154053.480415	36.461952
1553.439860	154323.386645	36.466970
1555.158391	154587.478636	36.471988
1557.013123	154838.555191	36.477005
1558.245260	155100.509687	36.482023
1559.831983	155359.950145	36.487040
1561.292752	155613.846442	36.492058
1562.745607	155888.438514	36.497076
1564.494957	156158.712752	36.502093
1566.041400	156425.407721	36.507111
1567.992302	156678.511398	36.512128
1569.065527	156951.536704	36.517146
1570.383792	157217.044184	36.522164
1572.232086	157496.835841	36.527181
1573.814205	157772.842705	36.532199
1575.267597	158026.415783	36.537216
1576.930799	158314.726479	36.542234
1578.563800	158591.200977	36.547252
1580.123159	158868.982781	36.552269
1581.654594	159153.162216	36.557287
1583.224273	159424.048621	36.562304
1584.657420	159705.382355	36.567322
1586.740112	159983.622498	36.572340
1588.771262	160256.965529	36.577357
1590.154676	160533.190721	36.582375
1591.973307	160803.249334	36.587392
1593.638267	161081.209447	36.592410
1595.550465	161346.552623	36.597428
1597.380421	161612.595644	36.602445
1598.855513	161885.189946	36.607463
1600.528291	162142.777984	36.612480
1601.879519	162409.727303	36.617498
1603.584876	162672.564193	36.622516
1605.300985	162936.504622	36.627533
1606.612491	163217.238753	36.632551
1608.165650	163469.668394	36.637568
1609.933128	163731.501262	36.642586
1611.465415	163982.149611	36.647604
1612.660309	164240.703634	36.652621
1614.430668	164486.498365	36.657639
1616.482110	164729.827751	36.662656
1617.976968	164982.150329	36.667674
1619.246589	165234.827488	36.672692
1620.963346	165482.641284	36.677709
1622.282407	165737.330598	36.682727
1624.024807	165997.192471	36.687744
1625.334515	166246.889712	36.692762
1626.846429	166512.600628	36.697780
1628.452492	166780.137552	36.702797
1629.630287	167058.677407	36.707815
1631.114280	167328.343074	36.712832
1632.772095	167616.754605	36.717850
1634.274482	167892.712409	36.722868
1636.145189	168180.396852	36.727885
1637.653752	168469.384017	36.732903
1639.250197	168757.306668	36.737920
1640.952587	169052.140113	36.742938
1642.868688	169325.772226	36.747956
1644.401933	169614.700758	36.752973
1645.873701	169918.684739	36.757991
1647.988711	170200.460166	36.763008
1649.726556	170489.515000	36.768026
1651.379334	170797.130285	36.773044
1652.949299	171074.622505	36.778061
1654.676132	171363.736358	36.783079
1656.454781	171650.028103	36.788096
1657.888909	171948.655650	36.793114
1659.826232	172234.583985	36.798132
1661.687285	172522.644928	36.803149
1663.208516	172832.643892	36.808167
1665.230306	173116.611705	36.813184
1667.097772	173400.047910	36.818202
1668.640759	173698.899767	36.823220
1670.279689	173983.886002	36.828237
1672.163483	174271.854567	36.833255
1673.533542	174558.092734	36.838272
1675.611167	174842.698269	36.843290
1677.134622	175136.591118	36.848308
1679.193094	175409.380424	36.853325
1680.616569	175706.604341	36.858343
1682.483077	176001.172091	36.863360
1684.296002	176278.979224	36.868378
1685.627397	176573.166696	36.873396
1687.639200	176856.731153	36.878413
1689.116104	177138.910877	36.883431
1690.700935	177436.844874	36.888448
1692.223043	177720.683346	36.893466
1694.155506	178019.809630	36.898484
1696.024102	178303.482881	36.903501
1697.491767	178603.549883	36.908519
1699.183320	178895.654059	36.913536
1701.012915	179178.375223	36.918554
1702.542956	179452.264787	36.923572
1704.466816	179718.785690	36.928589
1705.937150	179995.745904	36.933607
1707.325715	180258.295240	36.938624
1709.447064	180529.052869	36.943642
1710.900454	180805.729232	36.948660
1712.217053	181072.570742	36.953677
1713.646996	181360.013598	36.958695
1715.337283	181638.890766	36.963712
1717.520338	181932.384160	36.968730
1718.712576	182227.711709	36.973748
1720.577300	182515.994057	36.978765
1722.509259	182824.048593	36.983783
1723.973244	183125.873515	36.988800
1725.530198	183417.154370	36.993818
1727.066422	183730.569179	36.998836
1729.077954	184030.524277	37.003853
1730.887455	184340.068058	37.008871
1732.381051	184639.386263	37.013888
1734.585901	184951.218934	37.018906
1735.824478	185262.242857	37.023924
1737.665692	185559.266073	37.028941
1739.422846	185877.596912	37.033959
1740.780329	186184.763518	37.038976
1742.633788	186495.000389	37.043994
1744.643093	186828.524997	37.049012
1746.765135	187142.695400	37.054029
1748.358485	187461.215592	37.059047
1749.856111	187767.812242	37.064064
1751.973716	188080.784239	37.069082
1753.584005	188406.021115	37.074100
1755.402433	188724.349293	37.079117
1757.385542	189040.191636	37.084135
1759.167845	189359.976532	37.089152
1761.035186	189679.420156	37.094170
1762.759577	189998.292197	37.099188
1765.176443	190314.962530	37.104205
1766.810506	190631.771956	37.109223
1768.487447	190941.368478	37.114240
1770.368534	191242.076571	37.119258
1772.099470	191569.245005	37.124276
1773.972827	191879.273241	37.129293
1775.533095	192194.505642	37.134311
1777.320249	192509.234498	37.139328
1779.207558	192826.183094	37.144346
1780.889781	193143.572415	37.149364
1783.136300	193456.978008	37.154381
1784.814741	193767.150685	37.159399
1786.397472	194080.234116	37.164416
1788.707238	194387.975236	37.169434
1790.240973	194699.027018	37.174452
1792.269726	195001.866862	37.179469
1794.360035	195308.328557	37.184487
1796.133796	195610.273361	37.189504
1798.137974	195903.324532	37.194522
1799.518211	196189.521327	37.199540
1801.705829	196472.278956	37.204557
1803.356000	196744.995280	37.209575
1805.060101	197030.396525	37.214592
1806.968441	197306.235151	37.219610
1808.412832	197600.311405	37.224628
1810.209371	197874.279665	37.229645
1811.501336	198165.311783	37.234663
1813.021207	198469.280954	37.239680
1815.216191	198761.746873	37.244698
1816.853512	199061.055371	37.249716
1818.824380	199366.620830	37.254733
1820.139568	199670.426315	37.259751
1821.681101	199983.971008	37.264768
1823.920142	200285.678632	37.269786
1825.077198	200613.097821	37.274804
1826.879504	200934.603172	37.279821
1828.886685	201258.058016	37.284839
1830.434034	201589.051334	37.289856
1832.360303	201915.975444	37.294874
1833.961279	202248.995135	37.299892
1836.002963	202575.625580	37.304909
1837.605583	202911.822328	37.309927
1839.457560	203263.937253	37.314944
1841.477800	203588.431826	37.319962
1843.194692	203936.662786	37.324980
1845.266918	204278.746487	37.329997
1847.335728	204616.745381	37.335015
1848.868154	204955.834238	37.340032
1851.043668	205314.841390	37.345050
1852.923055	205663.640996	37.350068
1854.964667	205993.375777	37.355085
1856.838173	206337.521621	37.360103
1858.550265	206690.276432	37.365120
1860.469667	207035.155346	37.370138
1862.567122	207379.233648	37.375156
1864.446128	207723.932563	37.380173
1866.476133	208068.457163	37.385191
1868.571478	208410.929532	37.390208
1870.669998	208744.301241	37.395226
1872.442596	209103.217618	37.400244
1874.385410	209437.201800	37.405261
1876.559183	209766.657142	37.410279
1877.920552	210104.647277	37.415296
1880.198189	210443.928357	37.420314
1881.942550	210790.570236	37.425332
1883.957016	211122.457438	37.430349
1885.770100	211461.970119	37.435367
1887.642353	211806.299454	37.440384
1889.729192	212147.333877	37.445402
1891.307053	212488.044653	37.450420
1893.218007	212831.027646	37.455437
1895.338367	213164.292484	37.460455
1896.730649	213507.361383	37.465472
1898.823935	213846.956451	37.470490
1900.941603	214166.439277	37.475508
1902.714524	214496.388964	37.480525
1904.517453	214814.464853	37.485543
1906.243407	215136.756841	37.490560
1908.297537	215449.577836	37.495578
1909.857181	215776.038191	37.500596
1911.620986	216108.206374	37.505613
1913.623290	216431.349403	37.510631
1915.294668	216768.194973	37.515648
1916.883184	217111.949451	37.520666
1918.711238	217461.266728	37.525684
1920.638467	217800.171610	37.530701
1922.121677	218140.177019	37.535719
1923.917672	218508.371632	37.540736
1926.130116	218857.698315	37.545754
1928.110352	219240.760646	37.550772
1929.786256	219600.282691	37.555789
1932.172472	219943.137103	37.560807
1933.926263	220312.134852	37.565824
1936.156574	220682.531679	37.570842
1938.472319	221038.518371	37.575860
1940.019029	221411.934957	37.580877
1941.846148	221770.694477	37.585895
1943.673332	222137.480336	37.590912
1945.628808	222519.992235	37.595930
1947.560109	222896.923055	37.600948
1949.388743	223280.919076	37.605965
1951.235679	223671.415199	37.610983
1952.791012	224104.762947	37.616000
1954.664706	224490.230675	37.621018
1956.743259	224878.613623	37.626036
1958.838860	225269.814649	37.631053
1960.812777	225666.433445	37.636071
1962.559200	226072.766044	37.641088
1964.983282	226471.780703	37.646106
1967.082161	226865.084022	37.651124
1968.904907	227265.950258	37.656141
1970.931890	227653.300624	37.661159
1972.744067	228059.708683	37.666176
1975.024515	228467.187208	37.671194
1977.269639	228855.524279	37.676212
1979.167547	229253.416538	37.681229
1980.996091	229660.718420	37.686247
1983.220790	230057.800562	37.691264
1985.508477	230451.522079	37.696282
1987.452372	230848.957063	37.701300
1989.069844	231256.096535	37.706317
1991.711479	231635.950951	37.711335
1993.736209	232045.365854	37.716352
1995.930547	232426.031020	37.721370
1998.138235	232804.562210	37.726388
2000.094558	233194.690778	37.731405
2002.566458	233578.415063	37.736423
2004.194910	233964.281152	37.741440
2006.343188	234333.582953	37.746458
2008.503379	234692.978979	37.751476
2010.127046	235052.029674	37.756493
2012.081134	235404.197082	37.761511
2013.930669	235769.945063	37.766528
2015.738755	236130.138666	37.771546
2017.628250	236489.533260	37.776564
2019.228469	236859.439258	37.781581
2021.282333	237241.008818	37.786599
2022.958668	237628.125816	37.791616
2025.127569	238005.895446	37.796634
2027.144274	238389.202143	37.801652
2028.740512	238784.006518	37.806669
2031.183178	239173.775960	37.811687
2032.921141	239565.385736	37.816704
2034.889007	239968.796524	37.821722
2036.749526	240368.847644	37.826740
2039.064781	240772.180753	37.831757
2041.080524	241174.115005	37.836775
2042.849772	241593.818773	37.841792
2045.054552	241995.548027	37.846810
2046.937953	242417.166960	37.851828
2048.707772	242830.550367	37.856845
2050.987978	243246.927594	37.861863
2052.934387	243670.268020	37.866880
2055.035531	244107.403062	37.871898
2056.972468	244523.432546	37.876916
2059.334239	244955.195034	37.881933
2061.213167	245381.472827	37.886951
2063.538472	245813.878907	37.891968
2065.886284	246235.893917	37.896986
2067.835411	246664.222062	37.902004
2069.898717	247100.636275	37.907021
2072.298104	247527.447769	37.912039
2074.685806	247959.596593	37.917056
2076.531416	248389.470400	37.922074
2078.798179	248822.707792	37.927092
2080.656143	249252.632923	37.932109
2082.836882	249678.215239	37.937127
2084.967391	250116.507363	37.942144
2086.660489	250540.670701	37.947162
2089.358594	250977.706682	37.952180
2091.234308	251413.985242	37.957197
2093.390656	251846.969018	37.962215
2095.718630	252283.178089	37.967232
2097.605876	252710.237344	37.972250
2099.581140	253140.255684	37.977268
2101.891353	253573.701977	37.982285
2104.491174	254010.227795	37.987303
2106.527197	254447.936360	37.992320
2108.402595	254871.446268	37.997338
2110.850103	255303.122027	38.002356
2112.570604	255743.626995	38.007373
2114.853329	256170.580563	38.012391
2116.983415	256604.214620	38.017408
2119.202641	257024.829443	38.022426
2121.364641	257435.750462	38.027444
2123.036160	257837.452771	38.032461
2125.232590	258244.864287	38.037479
2127.348826	258656.836289	38.042496
2129.408400	259053.271646	38.047514
2131.445525	259451.413186	38.052532
2133.666027	259857.451894	38.057549
2135.768200	260278.522993	38.062567
2137.929439	260693.564962	38.067584
2140.256485	261098.953637	38.072602
2142.480772	261520.058123	38.077620
2144.710306	261922.694560	38.082637
2146.843599	262353.569380	38.087655
2148.725017	262767.744271	38.092672
2150.704889	263194.021287	38.097690
2152.965244	263612.455677	38.102708
2154.829769	264044.289943	38.107725
2156.888569	264478.761253	38.112743
2158.952271	264912.089178	38.117760
2161.002468	265352.862852	38.122778
2163.045548	265790.157932	38.127796
2165.282445	266236.415452	38.132813
2167.718383	266682.489457	38.137831
2170.318571	267141.264854	38.142848
2172.052168	267583.894699	38.147866
2174.103258	268021.190716	38.152884
2176.366949	268486.955826	38.157901
2178.531980	268944.125271	38.162919
2180.863694	269394.130314	38.167936
2182.536410	269851.429334	38.172954
2184.960745	270318.135701	38.177972
2187.123162	270786.992386	38.182989
2189.897903	271241.627970	38.188007
2191.783918	271696.023693	38.193024
2193.916213	272175.225068	38.198042
2196.657343	272623.744421	38.203060
2198.457344	273094.056887	38.208077
2200.823056	273562.298322	38.213095
2203.069578	274010.058238	38.218112
2205.056606	274487.987847	38.223130
2207.429598	274962.223637	38.228148
2209.401863	275437.107310	38.233165
2212.061998	275897.427376	38.238183
2214.349269	276370.355865	38.243200
2216.177396	276846.456360	38.248218
2218.510353	277305.100811	38.253236
2220.777049	277778.261044	38.258253
2223.119156	278256.820141	38.263271
2225.847861	278723.352801	38.268288
2227.980306	279199.582348	38.273306
2230.129801	279661.252878	38.278324
2232.188657	280135.740879	38.283341
2234.932633	280604.378845	38.288359
2237.479143	281069.567618	38.293376
2239.542419	281522.613754	38.298394
2242.149809	281954.895037	38.303412
2244.353979	282389.577088	38.308429
2246.459269	282807.813204	38.313447
2248.813365	283233.503529	38.318464
2250.917293	283650.189650	38.323482
2253.061323	284077.817867	38.328500
2254.730097	284522.846054	38.333517
2256.973452	284953.353715	38.338535
2259.012618	285395.502579	38.343552
2260.933887	285839.397095	38.348570
2263.449573	286281.139227	38.353588
2265.601394	286739.069499	38.358605
2267.528270	287197.695363	38.363623
2270.006560	287651.457450	38.368640
2271.922703	288122.099433	38.373658
2274.337672	288592.814076	38.378676
2276.871816	289062.493020	38.383693
2278.882621	289532.584473	38.388711
2281.366943	289996.274812	38.393728
2283.167050	290474.781094	38.398746
2285.984322	290949.492692	38.403764
2288.433835	291431.882572	38.408781
2290.403264	291910.765920	38.413799
2293.135685	292387.800019	38.418816
2295.065472	292873.902149	38.423834
2297.763046	293349.060110	38.428852
2299.833632	293838.211641	38.433869
2302.400848	294325.327399	38.438887
2305.200641	294797.316243	38.443904
2307.458315	295276.197814	38.448922
2309.778718	295752.350319	38.453940
2312.358326	296232.245544	38.458957
2314.381500	296715.733329	38.463975
2317.103403	297190.243844	38.468992
2319.313659	297692.090588	38.474010
2321.936696	298156.377381	38.479028
2323.987826	298640.160655	38.484045
2326.403454	299127.136260	38.489063
2328.686395	299600.795679	38.494080
2330.922498	300095.620753	38.499098
2333.311108	300571.394459	38.504116
2335.838605	301067.465938	38.509133
2337.891896	301558.962630	38.514151
2340.128781	302044.154581	38.519168
2342.470867	302538.345776	38.524186
2345.299361	303030.045161	38.529204
2347.477588	303520.169561	38.534221
2349.536208	304005.789928	38.539239
2352.146832	304498.662015	38.544256
2354.102757	305005.962233	38.549274
2357.009052	305486.210624	38.554292
2359.508149	305979.349203	38.559309
2361.505456	306465.300994	38.564327
2364.519903	306955.306243	38.569344
2366.776304	307432.932879	38.574362
2369.068188	307903.008261	38.579380
2371.506601	308361.908025	38.584397
2373.876074	308800.624006	38.589415
2376.313801	309246.998406	38.594432
2377.895671	309719.922705	38.599450
2380.481559	310168.937220	38.604468
2382.959500	310632.546563	38.609485
2385.256190	311097.706784	38.614503
2387.473366	311559.931408	38.619520
2389.472485	312029.554545	38.624538
2392.007496	312504.907212	38.629556
2394.362867	312982.470656	38.634573
2396.809147	313467.688126	38.639591
2399.474010	313935.521324	38.644608
2401.506584	314429.003903	38.649626
2403.857689	314918.319108	38.654644
2406.626418	315406.168908	38.659661
2408.846952	315902.611777	38.664679
2410.914451	316397.704980	38.669696
2413.328037	316906.176536	38.674714
2415.774079	317405.471653	38.679732
2418.121097	317915.777235	38.684749
2420.189675	318425.717907	38.689767
2423.268052	318937.197458	38.694784
2425.142312	319450.998497	38.699802
2427.845181	319968.297212	38.704820
2430.145416	320493.098244	38.709837
2432.113548	321012.082180	38.714855
2435.267654	321537.199005	38.719872
2437.766574	322061.908656	38.724890
2439.867780	322588.481391	38.729908
2442.637817	323119.338542	38.734925
2444.998751	323649.343006	38.739943
2447.850018	324162.758961	38.744960
2450.106296	324702.373201	38.749978
2452.627876	325223.199779	38.754996
2455.731495	325754.520835	38.760013
2457.919690	326278.974362	38.765031
2460.472401	326800.319283	38.770048
2462.886558	327330.748855	38.775066
2465.637967	327862.594346	38.780084
2468.064765	328376.533524	38.785101
2470.487905	328912.944176	38.790119
2473.353072	329424.978502	38.795136
2475.588404	329957.170727	38.800154
2478.304876	330486.870507	38.805172
2481.073544	331002.490003	38.810189
2483.436147	331526.194701	38.815207
2485.852478	332046.585978	38.820224
2488.469584	332573.670969	38.825242
2490.870473	333098.272437	38.830260
2493.590886	333611.316359	38.835277
2495.755872	334142.727444	38.840295
2498.536685	334663.676697	38.845312
2500.650482	335180.411022	38.850330
2502.835023	335674.911997	38.855348
2505.745749	336166.577358	38.860365
2507.997446	336657.480256	38.865383
2510.448007	337148.652755	38.870400
2512.612788	337641.542761	38.875418
2515.106157	338151.033759	38.880436
2517.565024	338644.834522	38.885453
2519.649280	339171.292904	38.890471
2522.344368	339662.560161	38.895488
2524.571862	340180.024636	38.900506
2526.782929	340708.710033	38.905524
2529.734193	341227.269985	38.910541
2531.870516	341763.219915	38.915559
2534.362203	342294.005568	38.920576
2536.713727	342843.063882	38.925594
2539.428677	343376.648389	38.930612
2542.087174	343907.825174	38.935629
2544.303541	344467.096544	38.940647
2546.845565	345016.942681	38.945664
2549.274957	345562.688634	38.950682
2552.231928	346119.059678	38.955700
2555.097465	346669.829168	38.960717
2557.976076	347224.627951	38.965735
2560.513195	347773.001686	38.970752
2563.038447	348343.814196	38.975770
2565.619912	348888.869758	38.980788
2568.223131	349444.147354	38.985805
2570.734360	350006.491367	38.990823
2573.296269	350567.704617	38.995840
2575.988613	351134.984029	39.000858
2578.433835	351695.797959	39.005876
2581.141020	352264.510131	39.010893
2583.492763	352839.085727	39.015911
2586.325081	353403.272756	39.020928
2589.163722	353972.351933	39.025946
2591.733128	354545.325959	39.030964
2594.574118	355103.553351	39.035981
2596.952567	355688.069247	39.040999
2599.598314	356259.336782	39.046016
2602.342484	356825.251853	39.051034
2604.921906	357403.497304	39.056052
2607.722121	357973.401027	39.061069
2610.045715	358551.496014	39.066087
2612.951227	359115.735063	39.071104
2615.764372	359686.962181	39.076122
2618.498811	360259.464125	39.081140
2620.986705	360828.876483	39.086157
2623.353933	361408.758039	39.091175
2626.345619	361982.899176	39.096192
2629.164906	362564.065557	39.101210
2631.436664	363131.403396	39.106228
2634.206986	363698.223917	39.111245
2636.724231	364278.680816	39.116263
2639.546789	364854.031664	39.121280
2642.240693	365410.082639	39.126298
2644.836791	365958.198946	39.131316
2647.406272	366497.988887	39.136333
2649.849598	367039.035835	39.141351
2652.120929	367577.667263	39.146368
2655.257960	368109.582401	39.151386
2657.410627	368662.557422	39.156404
2659.927735	369201.510773	39.161421
2662.485236	369768.719950	39.166439
2665.352703	370326.991131	39.171456
2667.975473	370888.618019	39.176474
2670.209721	371444.615091	39.181492
2673.171882	371998.459639	39.186509
2675.724671	372579.512342	39.191527
2678.083556	373152.544191	39.196544
2680.777033	373724.373391	39.201562
2683.368782	374320.416965	39.206580
2686.171971	374884.981417	39.211597
2688.771487	375483.823352	39.216615
2691.293206	376074.981069	39.221632
2694.367842	376664.900884	39.226650
2696.567488	377263.500854	39.231668
2699.495250	377847.362846	39.236685
2702.504104	378459.136596	39.241703
2705.167172	379062.913303	39.246720
2708.235052	379671.132504	39.251738
2710.448604	380285.972183	39.256756
2713.281319	380876.831770	39.261773
2716.523020	381497.121411	39.266791
2719.183765	382096.792538	39.271808
2722.104668	382698.797667	39.276826
2724.832664	383309.321960	39.281844
2727.848290	383914.971115	39.286861
2730.385685	384530.604656	39.291879
2733.136308	385137.163918	39.296896
2736.021489	385739.430532	39.301914
2738.486178	386360.448289	39.306932
2741.627671	386969.173186	39.311949
2744.369649	387582.364682	39.316967
2747.074476	388196.287305	39.321984
2750.236270	388814.007814	39.327002
2752.970199	389427.828818	39.332020
2755.910762	390025.120719	39.337037
2758.437088	390647.856023	39.342055
2761.370093	391263.693614	39.347072
2764.512025	391865.817488	39.352090
2767.151970	392483.075027	39.357108
2770.221172	393089.297865	39.362125
2772.896534	393696.257209	39.367143
2775.777329	394291.051378	39.372160
2778.517493	394898.232881	39.377178
2781.027179	395518.804231	39.382196
2783.989797	396120.679451	39.387213
2786.350721	396735.368946	39.392231
2789.313174	397345.210113	39.397248
2792.375791	397937.908303	39.402266
2794.488071	398529.833596	39.407284
2796.937633	399110.664990	39.412301
2799.672481	399691.643836	39.417319
2802.638161	400275.846686	39.422336
2805.465149	400859.452542	39.427354
2807.736733	401449.398399	39.432372
2810.530628	402038.287361	39.437389
2813.466959	402632.340463	39.442407
2815.898051	403246.161800	39.447424
2818.807562	403831.627594	39.452442
2821.654624	404446.120518	39.457460
2824.612594	405046.615269	39.462477
2827.505549	405665.006667	39.467495
2830.026457	406288.388110	39.472512
2832.950349	406890.779541	39.477530
2835.621749	407529.144834	39.482548
2838.318352	408147.568657	39.487565
2841.303724	408777.290422	39.492583
2843.809450	409419.140772	39.497600
2846.937241	410041.082789	39.502618
2849.988566	410693.262950	39.507636
2852.752537	411333.435000	39.512653
2855.420824	411993.504961	39.517671
2858.519506	412633.114650	39.522688
2861.501986	413272.399486	39.527706
2863.899397	413939.464231	39.532724
2867.500166	414589.875402	39.537741
2870.619574	415248.027251	39.542759
2873.157093	415904.051573	39.547776
2876.152798	416557.682421	39.552794
2878.908775	417217.823782	39.557812
2881.798332	417874.127734	39.562829
2885.026568	418544.528109	39.567847
2887.700029	419206.689177	39.572864
2890.700229	419867.237376	39.577882
2893.359138	420546.017013	39.582900
2896.379406	421209.571113	39.587917
2899.862778	421874.708389	39.592935
2902.850735	422558.049076	39.597952
2905.831307	423208.868199	39.602970
2908.543139	423885.024386	39.607988
2911.430144	424555.106544	39.613005
2914.222938	425228.404585	39.618023
2917.285584	425898.096563	39.623040
2920.347161	426575.169286	39.628058
2922.982162	427252.419174	39.633076
2926.007826	427930.907351	39.638093
2929.249775	428603.087339	39.643111
2932.143639	429277.357161	39.648128
2935.061747	429949.452953	39.653146
2938.570924	430629.239319	39.658164
2941.418471	431299.513398	39.663181
2944.255495	431961.413841	39.668199
2947.066705	432625.580936	39.673216
2950.450994	433275.913444	39.678234
2952.894897	433926.834245	39.683252
2955.864677	434553.393955	39.688269
2959.201123	435175.752394	39.693287
2961.638263	435810.899840	39.698304
2964.453007	436435.285252	39.703322
2966.966679	437073.047838	39.708340
2969.678270	437713.598978	39.713357
2972.658140	438364.371686	39.718375
2975.046176	439022.994493	39.723392
2978.420810	439682.304571	39.728410
2981.121062	440351.730207	39.733428
2983.702327	441027.992481	39.738445
2986.851004	441711.134024	39.743463
2989.579193	442389.917854	39.748480
2992.591686	443076.637725	39.753498
2995.741357	443757.392573	39.758516
2998.515535	444452.667774	39.763533
3001.829504	445155.431686	39.768551
3004.250470	445862.872704	39.773568
3007.553552	446559.825560	39.778586
3010.562764	447282.318861	39.783604
3013.508719	447991.739545	39.788621
3016.801805	448703.614948	39.793639
3019.588467	449435.290346	39.798656
3022.901065	450155.470622	39.803674
3026.327065	450874.446462	39.808692
3029.074414	451600.239078	39.813709
3032.014707	452332.760423	39.818727
3035.072207	453073.337626	39.823744
3038.503817	453791.259760	39.828762
3041.767304	454530.896662	39.833780
3044.573813	455262.282302	39.838797
3047.739549	455998.597253	39.843815
3050.768217	456740.880919	39.848832
3054.129867	457467.097257	39.853850
3057.003296	458211.026465	39.858868
3059.829252	458951.143404	39.863885
3063.221038	459689.779927	39.868903
3066.288863	460447.972413	39.873920
3069.541917	461185.821660	39.878938
3072.484944	461928.349403	39.883956
3075.583491	462667.336515	39.888973
3078.679415	463431.744383	39.893991
3081.929208	464168.177444	39.899008
3084.854823	464951.376204	39.904026
3088.140293	465692.961375	39.909044
3091.173778	466450.291117	39.914061
3094.671562	467210.959709	39.919079
3097.322497	467982.558334	39.924096
3100.578598	468689.549813	39.929114
3103.509289	469494.023562	39.934132
3106.238915	470211.313248	39.939149
3109.832992	471013.044249	39.944167
3112.887736	471752.226921	39.949184
3115.651785	472518.684050	39.954202
3119.134359	473226.395325	39.959220
3122.382967	473933.765211	39.964237
3125.519237	474671.616286	39.969255
3127.995342	475374.305655	39.974272
3131.674167	476068.741808	39.979290
3134.468167	476821.887407	39.984308
3137.150391	477536.248174	39.989325
3140.204194	478257.905179	39.994343
3143.009259	479012.179885	39.999360
3145.953831	479736.479709	40.004378
3148.948295	480508.258145	40.009396
3152.079073	481256.178726	40.014413
3155.194243	481999.019127	40.019431
3157.926942	482783.839947	40.024448
3161.681960	483543.703935	40.029466
3164.400400	484328.414207	40.034484
3167.686852	485102.744461	40.039501
3170.565774	485906.163819	40.044519
3173.802306	486683.621855	40.049536
3176.504962	487468.863471	40.054554
3179.846134	488287.571141	40.059572
3182.858722	489081.589628	40.064589
3186.502045	489900.230349	40.069607
3189.301213	490709.774590	40.074624
3192.825809	491544.831636	40.079642
3196.326134	492342.777620	40.084660
3199.273390	493193.158089	40.089677
3202.789409	494010.931743	40.094695
3206.530344	494830.754943	40.099712
3209.917258	495646.153136	40.104730
3213.000464	496457.421839	40.109748
3215.983593	497311.242608	40.114765
3219.466193	498103.235060	40.119783
3222.373384	498961.282645	40.124800
3225.899601	499779.755800	40.129818
3229.291257	500599.525774	40.134836
3231.866323	501443.319334	40.139853
3235.240734	502284.472728	40.144871
3238.729161	503128.799306	40.149888
3241.713535	503967.359917	40.154906
3245.067397	504840.097928	40.159924
3248.098781	505666.707487	40.164941
3251.484953	506538.497790	40.169959
3254.652147	507374.948593	40.174976
3258.172295	508259.401019	40.179994
3261.574850	509085.486753	40.185012
3264.971322	509952.965496	40.190029
3268.356068	510794.414239	40.195047
3271.488767	511663.765727	40.200064
3274.576528	512508.406445	40.205082
3278.114032	513390.119126	40.210100
3281.523021	514217.418895	40.215117
3284.803891	515098.326225	40.220135
3288.017964	515926.733141	40.225152
3291.681297	516782.974240	40.230170
3294.699682	517590.395180	40.235188
3297.849268	518373.746926	40.240205
3301.279954	519223.089769	40.245223
3304.320213	520005.927544	40.250240
3307.599295	520822.731998	40.255258
3310.452783	521632.553345	40.260276
3313.926879	522455.650019	40.265293
3317.508984	523266.636539	40.270311
3320.230740	524107.467532	40.275328
3323.219910	524911.961006	40.280346
3326.543755	525777.365724	40.285364
3329.173847	526599.124524	40.290381
3332.632174	527460.182345	40.295399
3335.794081	528347.100173	40.300416
3339.177572	529162.911558	40.305434
3342.210288	530071.831189	40.310452
3345.321491	530942.381854	40.315469
3348.797978	531848.306377	40.320487
3351.729369	532733.350964	40.325504
3355.032354	533649.882178	40.330522
3358.883232	534545.714171	40.335540
3362.115151	535448.343920	40.340557
3365.616972	536389.572165	40.345575
3368.976878	537269.503546	40.350592
3372.833924	538191.269699	40.355610
3376.230809	539139.297640	40.360628
3379.286339	540031.560253	40.365645
3383.358245	540925.574000	40.370663
3386.258338	541897.785186	40.375680
3389.502255	542796.653874	40.380698
3393.445576	543713.839634	40.385716
3396.669552	544692.264325	40.390733
3400.083279	545619.034452	40.395751
3404.163718	546532.047098	40.400768
3407.145687	547485.403150	40.405786
3411.081037	548376.625625	40.410804
3414.636380	549354.135593	40.415821
3418.339037	550243.771070	40.420839
3421.786333	551213.723844	40.425856
3424.714483	552133.062472	40.430874
3429.307153	553026.966694	40.435892
3432.600832	553971.796942	40.440909
3436.044091	554938.480834	40.445927
3439.638111	555846.658253	40.450944
3442.963769	556767.398607	40.455962
3446.979900	557666.990899	40.460980
3450.453139	558639.858539	40.465997
3453.439801	559540.249025	40.471015
3457.873118	560436.480117	40.476032
3460.817857	561380.570700	40.481050
3464.451316	562313.826454	40.486068
3467.671996	563216.156493	40.491085
3471.785436	564106.720779	40.496103
3475.521109	565006.388810	40.501120
3478.934734	565913.092306	40.506125
3482.737621	566748.851781	40.511130
3485.867308	567554.928990	40.516135
3489.335123	568262.473713	40.521140
3492.403455	568950.540916	40.526144
3495.196565	569599.812412	40.531149
3498.418124	570126.580040	40.536154
3501.103504	570601.911740	40.541159
3503.462062	571023.864996	40.546164
3505.693611	571361.474511	40.551168
3507.276764	571637.201210	40.556173
3509.991893	571863.414623	40.561178
3511.217951	572100.692585	40.566183
3512.931139	572236.262107	40.571188
3514.338967	572346.383670	40.576192
3515.840548	572407.817785	40.581197
3516.456108	572394.570214	40.586202
3518.342256	572364.041286	40.591207
3519.043655	572320.397850	40.596212
3519.960272	572276.115632	40.601216
3520.608036	572155.440656	40.606221
3520.937367	572007.001666	40.611226
3522.281433	571820.912717	40.616231
3522.472475	571678.286480	40.621236
3522.829196	571500.965451	40.626240
3522.834083	571267.010011	40.631245
3523.721879	571036.841396	40.636250
3523.918880	570826.531255	40.641255
3523.584854	570546.005326	40.646260
3524.027092	570303.447866	40.651264
3523.808784	570052.574722	40.656269
3523.833369	569755.345814	40.661274
3524.387096	569460.546563	40.666279
3524.513810	569150.487719	40.671284
3524.427629	568866.561690	40.676288
3524.099827	568607.514677	40.681293
3524.089342	568302.246111	40.686298
3523.935688	568003.243102	40.691303
3524.041427	567695.321729	40.696308
3523.792792	567387.600643	40.701312
3523.369302	567088.116233	40.706317
3523.409705	566743.589959	40.711322
3522.911443	566444.506554	40.716327
3522.868977	566147.965816	40.721332
3522.765898	565847.395527	40.726336
3522.435881	565559.557932	40.731341
3522.241722	565251.931605	40.736346
3522.014797	564943.496996	40.741351
3521.815079	564651.233962	40.746356
3521.479531	564348.449554	40.751360
3521.151533	564046.211901	40.756365
3521.721181	563724.112767	40.761370
3521.279440	563449.155613	40.766375
3520.948331	563190.107903	40.771380
3521.069720	562894.429425	40.776384
3520.155679	562600.975579	40.781389
3520.438603	562276.871391	40.786394
3520.000903	562000.221027	40.791399
3519.643871	561772.262110	40.796404
3519.506894	561504.781989	40.801408
3519.030716	561241.031456	40.806413
3518.928982	560973.132192	40.811418
3518.139985	560702.159474	40.816423
3517.985260	560439.502882	40.821428
3517.960770	560179.443138	40.826432
3517.271993	559946.463964	40.831437
3516.945164	559703.034843	40.836442
3517.742118	559452.111203	40.841447
3517.427403	559219.968661	40.846452
3517.244198	558973.982584	40.851456
3516.741598	558733.893154	40.856461
3516.691689	558552.082166	40.861466
3516.073592	558318.610990	40.866471
3516.026803	558060.180082	40.871476
3516.060666	557846.672115	40.876480
3515.366467	557688.153361	40.881485
3515.188771	557478.607502	40.886490
3514.975660	557264.070572	40.891495
3515.063827	557030.718749	40.896500
3515.410116	556809.882304	40.901504
3514.464054	556608.566180	40.906509
3514.500417	556428.479826	40.911514
3514.167560	556288.804501	40.916519
3513.955516	556092.207646	40.921524
3514.217546	555884.889251	40.926528
3513.622877	555658.836523	40.931533
3513.927670	555473.752000	40.936538
3513.424187	555293.686208	40.941543
3513.337666	555123.843585	40.946548
3513.136909	554943.574197	40.951552
3512.448218	554779.271085	40.956557
3512.634783	554606.200878	40.961562
3512.074471	554478.197652	40.966567
3511.830931	554356.449519	40.971572
3512.023610	554173.484841	40.976576
3511.509593	554011.920139	40.981581
3511.674000	553894.492904	40.986586
3511.213666	553753.753495	40.991591
3511.129059	553587.323159	40.996596
3511.046517	553453.080001	41.001600
3510.918173	553299.317096	41.006605
3511.102264	553176.028211	41.011610
3510.248716	553055.324120	41.016615
3510.166711	552925.314181	41.021620
3510.371499	552800.303330	41.026624
3510.682483	552661.954140	41.031629
3510.215302	552536.643567	41.036634
3510.394319	552410.321540	41.041639
3510.237377	552280.973593	41.046644
3510.245833	552163.355089	41.051648
3509.782133	552069.979863	41.056653
3510.174204	551936.152176	41.061658
3509.762021	551830.303910	41.066663
3508.768517	551735.647868	41.071668
3509.100845	551628.015282	41.076672
3508.582742	551527.530301	41.081677
3509.210272	551395.123755	41.086682
3508.847161	551301.323991	41.091687
3508.807570	551201.013422	41.096692
3508.982841	551106.218995	41.101696
3508.665865	551028.911172	41.106701
3508.588663	550933.247207	41.111706
3508.437538	550837.341983	41.116711
3508.328633	550763.229472	41.121716
3508.625875	550691.726938	41.126720
3508.401309	550606.832780	41.131725
3508.436322	550456.546327	41.136730
3507.897644	550391.028269	41.141735
3507.940583	550317.646454	41.146740
3507.794570	550241.114854	41.151744
3507.288619	550143.040691	41.156749
3507.474310	550072.814382	41.161754
3507.916349	550012.085213	41.166759
3507.165250	549936.101842	41.171764
3507.694370	549854.414919	41.176768
3507.598318	549732.453184	41.181773
3507.371953	549674.250652	41.186778
3506.849194	549632.546948	41.191783
3507.201756	549583.790787	41.196788
3507.357780	549510.588910	41.201792
3506.785349	549439.470040	41.206797
3506.762287	549389.157641	41.211802
3506.741630	549316.285524	41.216807
3506.783622	549250.014477	41.221812
3506.793976	549202.673778	41.226816
3506.751667	549098.917332	41.231821
3506.606440	549033.179583	41.236826
3506.415483	549002.676206	41.241831
3506.824134	548962.892602	41.246836
3506.971609	548864.807518	41.251840
3506.803842	548789.079267	41.256845
3506.721332	548724.793845	41.261850
3506.386513	548690.931068	41.266855
3506.061766	548657.571322	41.271860
3506.180672	548561.154240	41.276864
3505.523028	548532.136825	41.281869
3505.817608	548508.167330	41.286874
3506.020056	548473.714422	41.291879
3505.892844	548414.734148	41.296884
3506.188821	548346.400029	41.301888
3505.847332	548296.790339	41.306893
3506.168797	548234.609191	41.311898
3505.470862	548209.887598	41.316903
3505.765431	548168.908554	41.321908
3505.926422	548137.994446	41.326912
3505.774400	548091.382436	41.331917
3505.890432	548030.848007	41.336922
3505.367901	547990.704232	41.341927
3506.143284	547931.882190	41.346932
3506.499463	547870.703473	41.351936
3505.777790	547836.546559	41.356941
3505.596134	547788.171714	41.361946
3505.750381	547759.276806	41.366951
3505.793255	547709.957695	41.371956
3505.709429	547660.910813	41.376960
3505.376789	547647.083312	41.381965
3505.749450	547628.399783	41.386970
3505.361083	547577.937021	41.391975
3505.379484	547524.078500	41.396980
3505.624120	547490.020415	41.401984
3505.535509	547463.989872	41.406989
3505.389595	547427.671554	41.411994
3505.221469	547399.785910	41.416999
3505.362084	547363.169772	41.422004
3505.569592	547333.659915	41.427008
3505.214622	547288.086934	41.432013
3505.621173	547243.907698	41.437018
3505.058373	547204.878594	41.442023
3505.118953	547177.915410	41.447028
3505.301981	547119.284709	41.452032
3505.479301	547056.061388	41.457037
3505.290502	547060.129472	41.462042
3504.885568	547020.267315	41.467047
3505.480059	546956.170013	41.472052
3505.342160	546949.327247	41.477056
3504.888580	546947.228652	41.482061
3505.067807	546903.185281	41.487066
3505.101604	546864.464787	41.492071
3504.544522	546814.884178	41.497076
3505.606558	546760.605529	41.502080
3505.527191	546726.243559	41.507085
3505.036921	546715.418231	41.512090
3504.953759	546720.226864	41.517095
3504.942458	546673.537649	41.522100
3504.782716	546628.537497	41.527104
3504.047402	546601.194289	41.532109
3505.124211	546566.144427	41.537114
3504.972435	546541.232743	41.542119
3504.558088	546563.558975	41.547124
3504.561866	546530.596775	41.552128
3504.375236	546485.348049	41.557133
3503.972400	546457.447246	41.562138
3504.653398	546424.327289	41.567143
3504.661948	546445.930642	41.572148
3504.406494	546397.764813	41.577152
3504.819945	546372.763504	41.582157
3504.931705	546382.387330	41.587162
3504.494841	546346.768556	41.592167
3504.098149	546316.494041	41.597172
3504.270488	546298.648151	41.602176
3504.114148	546283.176195	41.607181
3504.488875	546253.789188	41.612186
3504.419224	546237.495827	41.617191
3504.198852	546225.718864	41.622196
3504.831904	546187.053313	41.627200
3504.712225	546208.727759	41.632205
3504.809559	546159.495820	41.637210
3504.675729	546141.445740	41.642215
3504.308822	546109.550771	41.647220
3504.809340	546097.659761	41.652224
3504.871207	546060.548054	41.657229
3504.761944	546056.981490	41.662234
3504.916442	545989.870326	41.667239
3504.436487	546002.515731	41.672244
3504.651450	545942.159021	41.677248
3504.153523	545939.158657	41.682253
3504.680715	545918.378886	41.687258
3504.606270	545903.045028	41.692263
3504.151520	545884.439604	41.697268
3504.165525	545878.228566	41.702272
3504.068239	545862.191560	41.707277
3503.780611	545840.076557	41.712282
3504.404283	545813.728602	41.717287
3504.340250	545820.452742	41.722292
3504.496546	545828.807891	41.727296
3504.172123	545808.213054	41.732301
3504.128307	545767.280838	41.737306
3504.016955	545745.440712	41.742311
3504.681771	545710.352994	41.747316
3504.390964	545722.060094	41.752320
3504.079500	545725.340246	41.757325
3503.766922	545689.952646	41.762330
3503.608514	545686.444241	41.767335
3503.702607	545662.299902	41.772340
3504.389982	545623.927183	41.777344
3504.161569	545648.295106	41.782349
3504.067755	545646.543300	41.787354
3504.283703	545617.483014	41.792359
3504.112364	545600.144932	41.797364
3504.048212	545576.782677	41.802368
3504.399652	545536.645523	41.807373
3504.036489	545514.844860	41.812378
3504.114361	545539.871283	41.817383
3504.041871	545545.536785	41.822388
3504.420927	545513.371180	41.827392
3504.114384	545498.477437	41.832397
3503.936637	545477.606551	41.837402
3504.423266	545431.894824	41.842407
3504.222285	545467.667469	41.847412
3504.280862	545455.088584	41.852416
3504.219749	545411.987432	41.857421
3504.686054	545395.810357	41.862426
3504.274647	545402.337185	41.867431
3504.095212	545360.062286	41.872436
3504.167181	545333.497797	41.877440
3504.079332	545358.651683	41.882445
3503.808630	545315.936750	41.887450
3504.640596	545284.860142	41.892455
3504.430473	545250.616381	41.897460
3504.288736	545268.509544	41.902464
3504.394202	545277.579783	41.907469
3504.471660	545228.196451	41.912474
3504.161372	545209.516862	41.917479
3504.376324	545174.398025	41.922484
3504.255146	545127.721309	41.927488
3504.172943	545147.473053	41.932493
3504.150013	545159.390663	41.937498
3504.222249	545133.683972	41.942503
3503.941199	545111.062020	41.947508
3504.395073	545080.297160	41.952512
3504.070772	545121.946093	41.957517
3503.826447	545102.953049	41.962522
3503.851216	545079.172097	41.967527
3503.927568	545080.018415	41.972532
3504.356938	545043.502351	41.977536
3503.920850	545033.828322	41.982541
3504.436139	545005.224352	41.987546
3504.304593	544984.345471	41.992551
3504.023423	545004.785129	41.997556
3504.424612	544957.369037	42.002560
3504.017028	544944.863403	42.007565
3504.054600	544955.913404	42.012570
3503.883116	544930.598266	42.017575
3503.524120	544906.271900	42.022580
3504.245571	544871.122772	42.027584
3503.956496	544918.673235	42.032589
3503.889096	544867.443731	42.037594
3504.113053	544867.862865	42.042599
3503.805968	544840.549679	42.047604
3504.144018	544876.188062	42.052608
3503.780373	544858.273712	42.057613
3504.099842	544827.479091	42.062618
3504.184999	544797.327244	42.067623
3503.870014	544820.448121	42.072628
3504.302874	544762.879250	42.077632
3504.062909	544782.050611	42.082637
3504.216056	544758.602240	42.087642
3504.227831	544718.567053	42.092647
3504.372434	544702.389593	42.097652
3504.353382	544683.208955	42.102656
3503.893833	544680.707102	42.107661
3504.107971	544674.564897	42.112666
3504.415514	544690.216935	42.117671
3504.055327	544682.196644	42.122676
3504.081130	544655.587758	42.127680
3504.067428	544658.568658	42.132685
3504.217313	544631.233342	42.137690
3504.347735	544607.535905	42.142695
3504.247355	544587.358317	42.147700
3504.608836	544513.089507	42.152704
3503.867367	544529.765758	42.157709
3504.119695	544527.555233	42.162714
3504.240601	544521.427701	42.167719
3503.858751	544520.377586	42.172724
3503.937379	544497.596879	42.177728
3503.968081	544494.462175	42.182733
3503.879583	544486.550288	42.187738
3503.982074	544483.101328	42.192743
3503.729901	544448.256552	42.197748
3503.827263	544415.375834	42.202752
3503.973400	544394.351265	42.207757
3503.957196	544374.008628	42.212762
3504.158284	544362.415992	42.217767
3503.956728	544412.932842	42.222772
3504.223167	544360.336225	42.227776
3504.034104	544366.071085	42.232781
3503.829436	544351.311543	42.237786
3504.087216	544332.642031	42.242791
3503.838487	544334.196080	42.247796
3503.989956	544302.568686	42.252800
3503.837289	544306.126958	42.257805
3503.902349	544311.468277	42.262810
3504.017447	544270.001972	42.267815
3503.926854	544256.435950	42.272820
3503.901696	544293.799150	42.277824
3503.800075	544261.000029	42.282829
3503.606686	544232.304654	42.287834
3504.070462	544206.080108	42.292839
3503.638223	544227.150534	42.297844
3503.966469	544220.889135	42.302848
3503.663229	544230.630438	42.307853
3503.805671	544206.375126	42.312858
3503.828444	544181.835776	42.317863
3504.262999	544161.421602	42.322868
3504.217075	544146.384337	42.327872
3504.192980	544188.442795	42.332877
3504.024734	544150.655899	42.337882
3504.121908	544128.780440	42.342887
3503.878228	544123.316200	42.347892
3503.709262	544093.556498	42.352896
3503.401806	544080.680909	42.357901
3503.813974	544049.415660	42.362906
3504.187390	544039.663515	42.367911
3503.815016	544067.136422	42.372916
3503.749722	544034.785436	42.377920
3503.986009	544046.158104	42.382925
3503.919061	544056.669946	42.387930
3503.658796	544026.520654	42.392935
3503.845159	543997.512373	42.397940
3503.762483	543998.434376	42.402944
3503.972671	543998.906198	42.407949
3503.695001	544014.045615	42.412954
3503.974134	543945.996787	42.417959
3503.899831	543980.894709	42.422964
3503.822732	543951.927982	42.427968
3503.730533	543952.144685	42.432973
3503.584538	543931.720988	42.437978
3503.651951	543927.823068	42.442983
3503.249156	543934.551118	42.447988
3503.524589	543933.901930	42.452992
3503.414450	543923.468847	42.457997
3503.512150	543944.304448	42.463002
3504.048671	543901.811270	42.468007
3503.721146	543903.579764	42.473012
3503.840428	543882.255799	42.478016
3503.924261	543899.509111	42.483021
3503.950480	543876.685255	42.488026
3503.688798	543880.210372	42.493031
3503.618346	543873.961362	42.498036
3504.141271	543853.330854	42.503040
3503.823262	543867.164143	42.508045
3503.607520	543827.566420	42.513050
3503.858128	543832.373715	42.518055
3503.838002	543831.215887	42.523060
3503.960511	543815.091445	42.528064
3503.503431	543811.377371	42.533069
3504.161301	543803.195687	42.538074
3503.626403	543802.624091	42.543079
3504.018203	543785.194882	42.548084
3503.991300	543753.947930	42.553088
3504.062600	543766.861498	42.558093
3504.117008	543737.267727	42.563098
3504.304604	543738.550921	42.568103
3503.902812	543705.293156	42.573108
3504.115413	543706.521914	42.578112
3503.715299	543681.442740	42.583117
3504.022079	543654.737171	42.588122
3504.107901	543689.156079	42.593127
3503.691010	543685.082210	42.598132
3503.888965	543648.599315	42.603136
3503.952409	543626.122604	42.608141
3503.871378	543603.113333	42.613146
3503.756271	543634.888289	42.618151
3503.865940	543626.237799	42.623156
3503.699265	543611.925906	42.628160
3503.842333	543600.594288	42.633165
3504.503219	543558.837793	42.638170
3504.194107	543588.825957	42.643175
3503.921890	543557.869808	42.648180
3504.208549	543491.029424	42.653184
3504.007468	543493.535296	42.658189
3503.896655	543526.370048	42.663194
3503.713119	543475.810464	42.668199
3503.988755	543469.809509	42.673204
3503.560348	543487.598653	42.678208
3503.810841	543459.790902	42.683213
3503.885144	543459.324950	42.688218
3503.789188	543451.363204	42.693223
3503.805544	543411.323790	42.698228
3503.914263	543406.005538	42.703232
3504.104208	543403.097875	42.708237
3503.685748	543436.082429	42.713242
3504.258247	543423.572064	42.718247
3504.046938	543378.519740	42.723252
3504.229367	543330.880626	42.728256
3503.779826	543361.143885	42.733261
3503.787859	543348.217795	42.738266
3503.860581	543345.732557	42.743271
3503.814544	543354.827914	42.748276
3503.968094	543325.722542	42.753280
3504.001487	543305.269634	42.758285
3503.719113	543306.728129	42.763290
3503.065064	543281.133047	42.768295
3503.584972	543260.653667	42.773300
3503.741896	543298.949856	42.778304
3503.300637	543288.922087	42.783309
3504.036749	543257.402028	42.788314
3504.043657	543233.570471	42.793319
3503.867059	543278.432471	42.798324
3504.344918	543225.192583	42.803329
3504.285454	543247.063772	42.808333
3503.985246	543197.985862	42.813338
3504.216721	543207.188911	42.818343
3503.782189	543194.534598	42.823348
3504.049035	543158.342553	42.828353
3503.755016	543174.293225	42.833357
3503.578221	543128.022957	42.838362
3503.991175	543147.901034	42.843367
3503.651732	543117.913891	42.848372
3503.615750	543156.543870	42.853377
3503.765082	543108.606347	42.858381
3503.904795	543111.815752	42.863386
3504.174432	543086.528738	42.868391
3503.665710	543111.248042	42.873396
3504.049603	543060.395409	42.878401
3503.544250	543074.965890	42.883405
3503.766384	543057.966569	42.888410
3503.990459	543052.528980	42.893415
3503.835255	543037.861299	42.898420
3503.757977	543034.389932	42.903425
3503.507224	543026.401938	42.908429
3503.727891	543041.261609	42.913434
3503.747355	543011.015565	42.918439
3503.706776	543025.714587	42.923444
3503.471792	542985.006909	42.928449
3504.222768	542959.340662	42.933453
3503.604227	542965.699327	42.938458
3503.914960	542984.079091	42.943463
3504.064154	542943.916452	42.948468
3503.920060	542950.250621	42.953473
3503.946505	542938.432041	42.958477
3503.856873	542936.022887	42.963482
3503.822485	542897.201872	42.968487
3503.734121	542917.462435	42.973492
3503.757792	542896.606589	42.978497
3503.699710	542889.900803	42.983501
3503.548412	542887.602368	42.988506
3503.795550	542847.222030	42.993511
3503.461443	542887.969913	42.998516
3503.693323	542859.356153	43.003521
3503.495924	542889.075609	43.008525
3503.671511	542839.820340	43.013530
3503.786340	542861.816012	43.018535
3503.523600	542827.221576	43.023540
3503.505196	542842.371683	43.028545
3504.288369	542818.366278	43.033549
3503.888266	542833.627217	43.038554
3503.857180	542784.757866	43.043559
3503.676414	542811.344452	43.048564
3503.957354	542787.216421	43.053569
3503.590226	542758.192247	43.058573
3503.795411	542771.287473	43.063578
3503.878736	542745.170999	43.068583
3503.120371	542774.221995	43.073588
3503.880112	542758.601577	43.078593
3503.526294	542743.460098	43.083597
3503.626707	542733.699769	43.088602
3503.834110	542711.905798	43.093607
3503.584022	542735.070125	43.098612
3503.888926	542700.486654	43.103617
3503.629098	542725.167251	43.108621
3503.951522	542679.170123	43.113626
3504.006809	542684.816512	43.118631
3503.395524	542699.101156	43.123636
3503.750271	542665.923461	43.128641
3504.199212	542668.478196	43.133645
3503.744655	542679.860121	43.138650
3504.310961	542635.742953	43.143655
3503.995570	542643.720030	43.148660
3503.848177	542598.301822	43.153665
3503.753266	542625.329585	43.158669
3503.844379	542605.068562	43.163674
3503.764319	542603.920113	43.168679
3503.405134	542573.581564	43.173684
3503.746315	542564.742397	43.178689
3503.454572	542590.488569	43.183693
3503.605218	542572.086255	43.188698
3503.790094	542580.640673	43.193703
3503.801682	542554.131279	43.198708
3503.999696	542531.429693	43.203713
3503.925186	542547.093877	43.208717
3503.912609	542533.867398	43.213722
3503.817667	542501.669259	43.218727
3503.639277	542536.637487	43.223732
3504.105576	542492.081286	43.228737
3503.816204	542504.144110	43.233741
3503.609925	542461.562301	43.238746
3503.966278	542471.351960	43.243751
3503.879954	542450.058458	43.248756
3503.759367	542456.086171	43.253761
3503.610757	542415.666244	43.258765
3503.532572	542450.770307	43.263770
3504.111606	542419.525780	43.268775
3503.540825	542436.126876	43.273780
3503.722654	542416.507649	43.278785
3503.804877	542397.106107	43.283789
3503.930460	542390.825491	43.288794
3503.878393	542378.160524	43.293799
3503.753960	542358.488647	43.298804
3503.795441	542371.812064	43.303809
3503.853744	542345.143442	43.308813
3503.470849	542347.577258	43.313818
3503.840190	542352.820689	43.318823
3503.718516	542340.318167	43.323828
3503.625489	542308.371770	43.328833
3503.627797	542319.883719	43.333837
3503.591773	542291.109257	43.338842
3503.537734	542317.373734	43.343847
3503.918638	542281.767452	43.348852
3503.738322	542305.779774	43.353857
3503.958519	542299.282198	43.358861
3503.513943	542271.582112	43.363866
3503.954647	542263.282449	43.368871
3503.743449	542233.828678	43.373876
3503.681288	542256.004689	43.378881
3503.587354	542212.192608	43.383885
3503.598031	542231.832534	43.388890
3503.975384	542256.463676	43.393895
3503.554980	542232.496104	43.398900
3503.424532	542195.455682	43.403905
3504.214596	542169.832406	43.408909
3503.674139	542201.021230	43.413914
3503.534357	542206.496663	43.418919
3503.414063	542170.464417	43.423924
3503.782101	542129.760088	43.428929
3503.912383	542170.587989	43.433933
3503.398733	542171.881177	43.438938
3503.687529	542149.720081	43.443943
3504.087970	542127.389828	43.448948
3503.922437	542154.227630	43.453953
3504.090285	542129.308543	43.458957
3503.785137	542106.635355	43.463962
3503.982705	542104.786581	43.468967
3504.291906	542067.474382	43.473972
3504.223501	542090.913938	43.478977
3503.992913	542079.488757	43.483981
3503.506039	542044.624990	43.488986
3504.297400	542022.081313	43.493991
3503.663878	542054.295005	43.498996
3503.640745	542043.190455	43.504001
3503.393501	542018.538766	43.509005
3503.772752	541989.849566	43.514010
3503.956116	542019.611540	43.519015
3503.806785	541961.366542	43.524020
3503.558880	541956.003161	43.529025
3503.973556	541984.617796	43.534029
3503.283181	541964.883380	43.539034
3504.235474	541925.499953	43.544039
3503.858995	541942.171866	43.549044
3504.055946	541943.150781	43.554049
3503.603359	541921.914424	43.559053
3503.875102	541909.197879	43.564058
3503.864559	541867.037886	43.569063
3503.735588	541914.774546	43.574068
3503.145994	541884.218558	43.579073
3504.182631	541862.696233	43.584077
3503.589070	541888.592297	43.589082
3503.537479	541887.186826	43.594087
3503.609268	541860.262748	43.599092
3503.385816	541834.243677	43.604097
3503.358289	541822.230776	43.609101
3503.481327	541863.313123	43.614106
3503.841758	541820.892390	43.619111
3503.484555	541869.523657	43.624116
3503.736412	541817.576842	43.629121
3503.822507	541808.070644	43.634125
3503.316866	541810.473452	43.639130
3503.525930	541818.317573	43.644135
3503.351960	541813.800844	43.649140
3503.507757	541811.554689	43.654145
3503.713558	541821.823011	43.659149
3503.129187	541798.486585	43.664154
3503.461713	541757.988840	43.669159
3503.154246	541796.210784	43.674164
3503.365731	541768.860513	43.679169
3503.388407	541793.649463	43.684173
3503.355735	541757.905341	43.689178
3503.457985	541790.760702	43.694183
3503.309572	541782.200439	43.699188
3503.482519	541776.669485	43.704193
3503.391422	541775.219754	43.709197
3503.338012	541805.575007	43.714202
3503.850469	541771.158569	43.719207
3503.747543	541782.586576	43.724212
3503.383084	541750.782885	43.729217
3503.583076	541759.133408	43.734221
3503.114715	541753.602826	43.739226
3503.422419	541738.103300	43.744231
3503.278158	541771.805567	43.749236
3503.396446	541744.419489	43.754241
3503.402631	541758.253966	43.759245
3503.167076	541759.402243	43.764250
3503.952964	541724.336556	43.769255
3503.483540	541767.078118	43.774260
3503.224650	541732.329071	43.779265
3503.787668	541696.339165	43.784269
3503.573494	541714.904441	43.789274
3503.659295	541722.869083	43.794279
3503.800844	541716.989614	43.799284
3503.697933	541704.433103	43.804289
3503.818845	541688.205644	43.809293
3503.249715	541704.201356	43.814298
3503.576724	541673.954504	43.819303
3503.519609	541692.898933	43.824308
3503.672677	541662.629058	43.829313
3503.550919	541679.260999	43.834317
3503.218843	541696.128140	43.839322
3503.694140	541663.787581	43.844327
3503.301029	541659.002479	43.849332
3503.702014	541642.781195	43.854337
3503.943749	541640.218467	43.859341
3503.760683	541644.438594	43.864346
3504.019176	541629.098218	43.869351
3503.924992	541612.147264	43.874356
3503.841206	541606.555840	43.879361
3503.641902	541619.615017	43.884365
3503.986296	541584.467307	43.889370
3503.887520	541587.714736	43.894375
3503.686079	541559.873919	43.899380
3503.160780	541581.972643	43.904385
3503.983937	541557.908422	43.909389
3503.391904	541565.727816	43.914394
3503.858788	541541.719883	43.919399
3504.029359	541529.069505	43.924404
3503.869326	541520.460435	43.929409
3503.969477	541529.382305	43.934413
3503.636598	541500.804738	43.939418
3504.106383	541471.140847	43.944423
3503.901067	541487.634722	43.949428
3503.631955	541477.830999	43.954433
3504.007836	541460.553102	43.959437
3503.779848	541471.041714	43.964442
3503.837996	541455.328871	43.969447
3503.982964	541438.592394	43.974452
3503.912225	541440.977012	43.979457
3504.039317	541419.799804	43.984461
3503.531317	541414.426846	43.989466
3503.573213	541401.897689	43.994471
3503.511681	541378.982918	43.999476
3503.336385	541366.387073	44.004481
3503.515444	541380.598530	44.009485
3503.190733	541388.830215	44.014490
3503.607019	541370.232961	44.019495
3503.661055	541378.404785	44.024500
3503.596438	541387.908228	44.029505
3503.665092	541369.517405	44.034509
3503.591864	541359.278683	44.039514
3503.928865	541349.833528	44.044519
3504.028552	541331.084288	44.049524
3503.782417	541343.848135	44.054529
3503.515429	541320.107334	44.059533
3503.337622	541303.118755	44.064538
3503.582042	541294.597112	44.069543
3503.176476	541319.404036	44.074548
3503.509088	541300.213980	44.079553
3503.595291	541303.785697	44.084557
3503.261226	541308.534736	44.089562
3503.487220	541293.249651	44.094567
3503.181386	541328.998254	44.099572
3503.352499	541301.653518	44.104577
3503.466219	541309.563470	44.109581
3503.640182	541277.269714	44.114586
3503.560883	541259.205114	44.119591
3503.631233	541269.141756	44.124596
3503.741033	541264.075054	44.129601
3503.819263	541265.224266	44.134605
3503.355046	541264.136434	44.139610
3503.743939	541230.293744	44.144615
3503.390463	541234.187453	44.149620
3503.441257	541234.028122	44.154625
3503.558166	541228.909790	44.159629
3503.491457	541228.971014	44.164634
3503.585502	541232.642499	44.169639
3503.425361	541236.808620	44.174644
3503.478236	541237.911345	44.179649
3503.983750	541204.555119	44.184653
3503.629404	541188.957695	44.189658
3503.713962	541188.086089	44.194663
3503.559162	541196.139535	44.199668
3503.454964	541193.732404	44.204673
3503.423042	541182.073157	44.209677
3503.339222	541177.794464	44.214682
3503.542664	541153.171113	44.219687
3503.376789	541168.548197	44.224692
3503.818420	541163.883472	44.229697
3503.899141	541150.540040	44.234701
3503.316400	541182.747562	44.239706
3503.881890	541158.773931	44.244711
3503.588951	541130.845793	44.249716
3503.494477	541126.316291	44.254721
3503.499542	541121.670063	44.259725
3503.432639	541114.459922	44.264730
3503.664933	541114.221406	44.269735
3503.464947	541127.685082	44.274740
3503.524088	541119.293618	44.279745
3503.691951	541097.503564	44.284749
3503.399184	541087.602334	44.289754
3503.693988	541092.908486	44.294759
3503.883379	541092.727247	44.299764
3503.806813	541071.783725	44.304769
3503.581072	541084.544567	44.309773
3503.407883	541058.667700	44.314778
3503.484652	541053.202180	44.319783
3503.435442	541052.604191	44.324788
3503.437586	541059.320006	44.329793
3503.494264	541049.615996	44.334797
3503.128427	541065.933720	44.339802
3503.742250	541062.049682	44.344807
3503.838094	541038.402575	44.349812
3503.600047	541031.976888	44.354817
3503.579562	541044.604328	44.359821
3503.644673	541022.123462	44.364826
3503.901179	541012.943301	44.369831
3503.759533	541019.984838	44.374836
3503.617162	540989.659321	44.379841
3503.818825	540963.319070	44.384845
3503.481502	540983.722576	44.389850
3503.447640	540985.091511	44.394855
3503.614644	540977.844333	44.399860
3503.560519	540958.210010	44.404865
3503.590408	540951.893427	44.409869
3503.506994	540938.171780	44.414874
3503.411024	540955.456894	44.419879
3503.538056	540947.610064	44.424884
3503.767093	540937.171789	44.429889
3503.758621	540936.011895	44.434893
3503.197281	540933.273008	44.439898
3503.739323	540919.603972	44.444903
3503.869653	540909.282273	44.449908
3503.752672	540902.281932	44.454913
3503.894831	540904.935962	44.459917
3503.493606	540910.554181	44.464922
3503.593916	540881.402004	44.469927
3503.896301	540878.375093	44.474932
3503.546899	540864.745919	44.479937
3503.622271	540882.206020	44.484941
3503.747112	540865.068118	44.489946
3503.393874	540862.296324	44.494951
3503.613857	540847.920679	44.499956
3503.356828	540822.965600	44.504961
3503.877377	540834.295775	44.509965
3503.701101	540842.100320	44.514970
3504.111073	540829.916484	44.519975
3503.770296	540814.569011	44.524980
3503.352783	540806.404206	44.529985
3503.857956	540782.389017	44.534989
3503.636731	540790.200693	44.539994
3503.791812	540787.146551	44.544999
3503.796540	540764.725344	44.550004
3503.522273	540748.862322	44.555009
3503.425311	540755.038469	44.560013
3502.938735	540758.195882	44.565018
3503.619835	540772.177067	44.570023
3503.527709	540742.651063	44.575028
3503.697833	540774.184985	44.580033
3503.931749	540738.699294	44.585037
3503.380303	540728.535733	44.590042
3503.364440	540725.963072	44.595047
3503.674684	540721.116992	44.600052
3503.417373	540718.027026	44.605057
3503.799540	540730.944562	44.610061
3503.765172	540717.315957	44.615066
3503.515132	540696.904307	44.620071
3503.824734	540681.049920	44.625076
3503.549179	540674.074538	44.630081
3503.566455	540682.454539	44.635085
3503.395059	540688.541485	44.640090
3503.238033	540691.141848	44.645095
3503.052804	540696.120039	44.650100
3503.590416	540682.855468	44.655105
3503.289279	540668.612520	44.660109
3503.488573	540671.712036	44.665114
3503.453322	540635.460692	44.670119
3503.217414	540666.150065	44.675124
3503.554867	540650.341740	44.680129
3503.796923	540640.355680	44.685133
3503.883904	540650.946566	44.690138
3503.904665	540650.892971	44.695143
3503.655645	540599.930094	44.700148
3503.643339	540630.432703	44.705153
3503.872318	540632.063109	44.710157
3503.100538	540615.874606	44.715162
3503.872554	540583.535336	44.720167
3503.486229	540567.841329	44.725172
3503.061814	540598.510137	44.730177
3503.538163	540582.225309	44.735181
3503.436983	540573.353908	44.740186
3503.466160	540584.509451	44.745191
3503.833532	540566.878397	44.750196
3503.742982	540593.606124	44.755201
3503.490717	540565.216033	44.760205
3503.407791	540568.410676	44.765210
3503.558460	540541.774766	44.770215
3503.576373	540520.815548	44.775220
3503.841740	540505.775934	44.780225
3503.764942	540553.912629	44.785229
3503.344655	540537.971471	44.790234
3503.910020	540501.574373	44.795239
3503.815446	540520.526192	44.800244
3503.642580	540510.555133	44.805249
3502.991306	540487.075754	44.810253
3503.101685	540485.543554	44.815258
3503.797754	540473.061721	44.820263
3503.825397	540464.472881	44.825268
3503.432161	540452.314705	44.830273
3503.642869	540441.273010	44.835277
3503.536648	540473.457216	44.840282
3503.656370	540445.159595	44.845287
3503.524801	540468.460159	44.850292
3503.486361	540445.237334	44.855297
3503.846831	540417.255094	44.860301
3503.358614	540456.316964	44.865306
3503.523975	540442.101062	44.870311
3503.191651	540412.056902	44.875316
3503.450144	540392.927911	44.880321
3503.488158	540433.573103	44.885325
3503.465499	540412.923136	44.890330
3503.114054	540442.116280	44.895335
3503.537096	540424.627756	44.900340
3503.454027	540419.843749	44.905345
3503.265601	540424.620540	44.910349
3503.113023	540446.964994	44.915354
3503.222864	540429.222992	44.920359
3503.082669	540432.174226	44.925364
3503.248911	540419.776096	44.930369
3503.660537	540418.953745	44.935373
3503.293251	540436.837816	44.940378
3503.417756	540400.661654	44.945383
3503.266054	540409.068515	44.950388
3503.384653	540390.668608	44.955393
3503.560842	540389.681477	44.960397
3503.167738	540403.176322	44.965402
3503.157153	540399.542309	44.970407
3503.130942	540387.427063	44.975412
3503.416782	540376.676435	44.980417
3503.260688	540403.717847	44.985421
3503.373683	540376.784613	44.990426
3503.496034	540418.274985	44.995431
3503.390765	540401.728410	45.000436
3503.470086	540389.242998	45.005441
3503.755938	540410.003258	45.010445
3503.505706	540379.794563	45.015450
3503.694057	540366.685919	45.020455
3503.721853	540353.451147	45.025460
3503.376960	540369.564315	45.030465
3503.620441	540367.506081	45.035469
3503.627586	540365.384207	45.040474
3503.651320	540351.998581	45.045479
3503.316775	540355.586529	45.050484
3503.304025	540330.642524	45.055489
3503.668091	540324.323356	45.060493
3503.577088	540332.821663	45.065498
3503.503912	540320.612790	45.070503
3503.741142	540331.180151	45.075508
3503.342833	540336.798120	45.080513
3503.349561	540311.346020	45.085517
3503.180320	540331.824832	45.090522
3503.882710	540301.566403	45.095527
3503.440542	540318.149488	45.100532
3503.591119	540303.632803	45.105537
3503.567255	540314.443439	45.110541
3503.241837	540289.700283	45.115546
3503.087709	540313.762129	45.120551
3503.104050	540302.751056	45.125556
3503.344253	540298.723889	45.130561
3503.961534	540275.094167	45.135565
3503.593037	540309.946104	45.140570
3503.300637	540277.420939	45.145575
3503.593654	540288.585495	45.150580
3502.961750	540278.636341	45.155585
3503.587218	540257.732222	45.160589
3503.155528	540289.968262	45.165594
3503.280767	540274.748575	45.170599
3503.296708	540264.343521	45.175604
3503.459979	540284.820337	45.180609
3503.066866	540264.279222	45.185613
3503.241258	540284.299793	45.190618
3503.593138	540278.790510	45.195623
3503.576728	540272.632457	45.200628
3503.362566	540276.049900	45.205633
3503.400204	540281.952472	45.210637
3503.434848	540261.495236	45.215642
3503.585937	540229.808845	45.220647
3503.505805	540214.268067	45.225652
3503.307400	540275.150566	45.230657
3503.431706	540238.014574	45.235661
3503.371303	540222.218192	45.240666
3503.335613	540242.120529	45.245671
3503.707634	540216.812526	45.250676
3503.327023	540266.866611	45.255681
3503.822945	540235.428718	45.260685
3504.000203	540183.639579	45.265690
3503.572408	540213.754210	45.270695
3503.412931	540221.960409	45.275700
3502.716349	540191.468398	45.280705
3503.036870	540198.790757	45.285709
3503.688848	540170.509491	45.290714
3503.314651	540213.997870	45.295719
3503.766471	540206.503309	45.300724
3503.641103	540172.487050	45.305729
3503.718221	540191.715136	45.310733
3503.418476	540210.043288	45.315738
3503.225167	540176.189272	45.320743
3503.436552	540148.987587	45.325748
3503.314256	540149.411094	45.330753
3503.518535	540187.202720	45.335757
3503.526099	540181.293335	45.340762
3503.759475	540156.714132	45.345767
3503.249693	540180.529411	45.350772
3503.217963	540157.860573	45.355777
3503.866190	540137.154688	45.360781
3503.411670	540152.275432	45.365786
3503.212222	540113.220846	45.370791
3503.344702	540145.671012	45.375796
3503.094575	540132.328479	45.380801
3503.586756	540115.384161	45.385805
3503.287462	540155.729920	45.390810
3503.679292	540111.127975	45.395815
3503.857490	540139.884488	45.400820
3503.569124	540146.646627	45.405825
3503.541292	540120.593681	45.410829
3503.344412	540098.455850	45.415834
3503.621392	540068.971189	45.420839
3503.641155	540114.569052	45.425844
3503.355066	540081.941471	45.430849
3503.921070	540104.475842	45.435853
3503.513524	540082.472285	45.440858
3503.875809	540031.562367	45.445863
3503.688599	540080.526008	45.450868
3503.600356	540047.008592	45.455873
3504.033162	540066.433112	45.460877
3503.759115	540023.754136	45.465882
3503.901354	540052.768996	45.470887
3503.346985	540035.687015	45.475892
3503.615692	540005.496547	45.480897
3503.796092	540028.394978	45.485901
3503.688517	539977.508648	45.490906
3503.371217	540007.303225	45.495911
3503.744820	539981.489585	45.500916
3503.649591	539986.302283	45.505921
3503.661772	539971.504158	45.510925
3504.014587	539962.055642	45.515930
3503.615570	539956.765932	45.520935
3503.768927	539943.712954	45.525940
3503.456226	539944.469561	45.530945
3504.027989	539946.298359	45.535949
3503.672433	539926.861843	45.540954
3503.237948	539910.366769	45.545959
3503.299609	539893.742753	45.550964
3503.445271	539908.112375	45.555969
3503.558525	539890.874203	45.560973
3503.596023	539883.747973	45.565978
3503.633312	539910.355698	45.570983
3503.697386	539873.682833	45.575988
3503.383472	539893.932604	45.580993
3503.662696	539847.176187	45.585997
3503.465542	539882.204022	45.591002
3503.242812	539877.795418	45.596007
3503.547374	539852.547972	45.601012
3503.444528	539846.201408	45.606017
3503.719706	539890.699070	45.611021
3503.261487	539866.026713	45.616026
3503.342337	539880.861105	45.621031
3503.288951	539853.801741	45.626036
3502.866814	539890.481120	45.631041
3503.618222	539872.334060	45.636045
3503.286627	539850.015160	45.641050
3503.509530	539825.538077	45.646055
3503.494444	539853.315682	45.651060
3503.715736	539825.606852	45.656065
3503.661919	539840.816069	45.661069
3504.073344	539797.422107	45.666074
3503.726326	539782.074572	45.671079
3503.230248	539804.676266	45.676084
3503.286043	539819.009677	45.681089
3503.172361	539787.465213	45.686093
3502.909677	539781.800390	45.691098
3503.280162	539783.408523	45.696103
3503.618840	539821.230317	45.701108
3502.989896	539797.342335	45.706113
3503.686657	539766.780732	45.711117
3503.556679	539800.283128	45.716122
3503.557415	539819.220758	45.721127
3503.565640	539797.807571	45.726132
3503.423754	539768.641036	45.731137
3503.575639	539786.191307	45.736141
3503.227276	539790.539075	45.741146
3503.324083	539771.737861	45.746151
3504.245844	539743.918163	45.751156
3503.702416	539767.638405	45.756161
3503.774295	539756.971660	45.761165
3503.520612	539735.145279	45.766170
3503.677316	539742.241251	45.771175
3503.569456	539718.270780	45.776180
3503.060628	539737.491058	45.781185
3503.943692	539716.595981	45.786189
3503.033136	539749.262362	45.791194
3503.519117	539717.117964	45.796199
3503.548700	539742.161686	45.801204
3503.302131	539713.971100	45.806209
3503.377543	539721.281933	45.811213
3503.060421	539691.536943	45.816218
3503.457719	539702.331945	45.821223
3503.737009	539678.805222	45.826228
3503.383340	539700.021046	45.831233
3503.565272	539676.459208	45.836237
3503.429215	539690.166557	45.841242
3503.466403	539674.051175	45.846247
3503.639475	539699.223790	45.851252
3502.992811	539684.529525	45.856257
3503.276369	539696.150519	45.861261
3503.210651	539686.515484	45.866266
3503.422204	539701.935398	45.871271
3503.452820	539659.207240	45.876276
3503.200468	539683.285610	45.881281
3503.195333	539651.218700	45.886285
3503.173828	539668.544011	45.891290
3503.153845	539654.558672	45.896295
3503.394912	539651.743215	45.901300
3503.359158	539667.959764	45.906305
3503.817736	539638.243561	45.911309
3503.425609	539659.718023	45.916314
3503.596465	539664.286761	45.921319
3503.710029	539656.037387	45.926324
3503.260910	539664.239167	45.931329
3503.453245	539643.200666	45.936333
3503.399038	539645.128446	45.941338
3503.382424	539623.516936	45.946343
3503.312115	539608.226488	45.951348
3503.143886	539634.109669	45.956353
3503.771564	539594.721006	45.961357
3503.242425	539637.781017	45.966362
3503.517731	539619.658410	45.971367
3503.508242	539620.670111	45.976372
3503.053128	539631.650400	45.981377
3504.078185	539608.106691	45.986381
3503.767936	539624.063669	45.991386
3503.823978	539598.299574	45.996391
3503.746136	539593.160973	46.001396
3503.357912	539582.869837	46.006401
3503.444493	539592.805014	46.011405
3503.525133	539598.499051	46.016410
3503.406650	539575.489551	46.021415
3503.251347	539546.476212	46.026420
3502.981613	539552.124646	46.031425
3503.130997	539551.394204	46.036429
3503.263050	539552.333035	46.041434
3503.251848	539572.333381	46.046439
3503.470002	539554.421735	46.051444
3503.306973	539549.094580	46.056449
3503.477498	539551.643363	46.061453
3503.423117	539541.854941	46.066458
3503.285721	539565.157812	46.071463
3503.780673	539537.708207	46.076468
3503.394545	539574.685661	46.081473
3503.592431	539543.343948	46.086477
3503.791085	539554.978470	46.091482
3503.486024	539514.525009	46.096487
3503.438853	539525.339890	46.101492
3503.057477	539509.088489	46.106497
3503.374461	539525.552442	46.111501
3503.381000	539509.845739	46.116506
3503.076606	539535.851613	46.121511
3503.753227	539521.301533	46.126516
3503.558460	539524.968583	46.131521
3503.530981	539517.296940	46.136525
3503.295227	539542.079926	46.141530
3503.674508	539514.598062	46.146535
3503.845243	539482.149489	46.151540
3503.506508	539501.545183	46.156545
3504.084745	539460.143940	46.161549
3503.550222	539487.398303	46.166554
3503.591359	539467.191477	46.171559
3503.940990	539441.128204	46.176564
3503.293841	539449.866414	46.181569
3503.558626	539432.553270	46.186573
3503.916090	539437.496592	46.191578
3503.445628	539445.247351	46.196583
3503.634249	539426.683704	46.201588
3503.405101	539411.822177	46.206593
3503.370971	539394.051223	46.211597
3503.387280	539402.634090	46.216602
3503.545536	539404.225308	46.221607
3503.755284	539385.809777	46.226612
3503.485869	539408.628739	46.231617
3503.887860	539400.333636	46.236621
3503.442069	539365.659195	46.241626
3503.277034	539372.200176	46.246631
3503.303884	539355.985088	46.251636
3503.655916	539344.566748	46.256641
3503.774384	539367.980983	46.261645
3503.572279	539344.933849	46.266650
3503.258728	539370.941451	46.271655
3503.929775	539330.787727	46.276660
3503.259580	539347.963429	46.281665
3503.328164	539334.721322	46.286669
3503.375990	539319.512914	46.291674
3503.529010	539310.752099	46.296679
3503.605245	539329.425896	46.301684
3503.579676	539306.249796	46.306689
3503.435584	539311.322939	46.311693
3503.491789	539333.232014	46.316698
3503.424328	539316.779283	46.321703
3503.449691	539286.423844	46.326708
3503.211495	539304.187837	46.331713
3503.354086	539282.853689	46.336717
3503.397158	539280.523977	46.341722
3503.237340	539299.336127	46.346727
3503.811134	539296.821526	46.351732
3503.358679	539291.792537	46.356737
3503.495258	539294.700242	46.361741
3503.364855	539295.428065	46.366746
3503.334185	539279.979516	46.371751
3503.555007	539299.640534	46.376756
3503.222786	539270.705136	46.381761
3503.267837	539291.858504	46.386765
3503.497615	539248.138175	46.391770
3503.278919	539237.617999	46.396775
3503.031784	539255.686474	46.401780
3502.952417	539242.770684	46.406785
3503.121853	539253.905036	46.411789
3503.445075	539253.349110	46.416794
3503.515446	539255.055240	46.421799
3503.429046	539252.796490	46.426804
3503.103936	539243.353681	46.431809
3503.286799	539263.778277	46.436813
3503.227334	539241.516471	46.441818
3503.166412	539273.797063	46.446823
3503.304968	539239.029968	46.451828
3503.026130	539263.517205	46.456833
3503.070445	539245.430665	46.461837
3503.033097	539255.234145	46.466842
3503.249114	539266.411627	46.471847
3503.435097	539236.081201	46.476852
3503.443731	539266.381233	46.481857
3503.592094	539252.065903	46.486861
3503.211962	539264.196150	46.491866
3503.385868	539264.774869	46.496871
3503.576050	539250.149915	46.501876
3503.411634	539273.407001	46.506881
3503.496684	539259.808712	46.511885
3503.435434	539264.212251	46.516890
3502.821561	539238.300926	46.521895
3503.524649	539204.454561	46.526900
3503.188445	539245.869113	46.531905
3503.182553	539223.144294	46.536909
3503.264022	539232.625996	46.541914
3503.258360	539236.667241	46.546919
3503.538907	539223.846052	46.551924
3503.385921	539234.829373	46.556929
3503.474784	539240.673750	46.561933
3503.620100	539226.560886	46.566938
3503.647172	539247.212137	46.571943
3504.101136	539220.071451	46.576948
3503.773350	539202.700204	46.581953
3503.765352	539191.995187	46.586957
3503.836192	539190.469107	46.591962
3503.356372	539201.049593	46.596967
3503.760071	539158.008545	46.601972
3503.167439	539197.645676	46.606977
3503.496942	539169.918548	46.611981
3503.365166	539159.485584	46.616986
3503.356950	539171.809629	46.621991
3503.495701	539165.121579	46.626996
3503.557559	539174.050891	46.632001
3503.924976	539160.761398	46.637005
3503.494171	539145.628471	46.642010
3503.481253	539145.529693	46.647015
3504.009638	539112.821792	46.652020
3503.425578	539153.972755	46.657025
3503.504925	539130.729302	46.662029
3503.677523	539100.501728	46.667034
3503.474925	539112.250516	46.672039
3503.602256	539105.210727	46.677044
3503.180124	539091.439943	46.682049
3503.688984	539075.703896	46.687053
3503.356083	539108.330844	46.692058
3503.374850	539081.662721	46.697063
3503.371484	539108.076266	46.702068
3503.011146	539100.305518	46.707073
3503.606308	539062.890219	46.712077
3503.435204	539101.955944	46.717082
3503.300641	539079.352254	46.722087
3503.501006	539094.067517	46.727092
3503.013190	539092.175209	46.732097
3502.983307	539093.190168	46.737101
3503.581891	539086.530405	46.742106
3503.398577	539069.691698	46.747111
3503.571540	539062.240656	46.752116
3503.547595	539049.214936	46.757121
3503.624331	539043.799203	46.762125
3503.476021	539058.418105	46.767130
3503.176006	539040.587759	46.772135
3503.378872	539050.252397	46.777140
3503.419193	539051.458272	46.782145
3503.517117	539052.402529	46.787149
3503.321822	539050.564984	46.792154
3503.577304	539049.868251	46.797159
3503.606563	539018.653117	46.802164
3503.071369	539034.949284	46.807169
3503.501586	539014.781363	46.812173
3503.642127	539017.991512	46.817178
3503.569561	539015.579032	46.822183
3503.297689	539009.965875	46.827188
3503.334083	539030.363433	46.832193
3503.598979	539019.817170	46.837197
3503.619496	539011.935675	46.842202
3503.050539	539008.137074	46.847207
3503.378992	538981.369323	46.852212
3503.471607	538979.637769	46.857217
3503.415635	538982.979993	46.862221
3503.479780	538984.030599	46.867226
3503.288857	538969.263603	46.872231
3503.319363	538983.450289	46.877236
3503.345294	538971.780198	46.882241
3503.275919	538977.144660	46.887245
3503.603312	538987.294684	46.892250
3503.443201	538975.654002	46.897255
3503.880307	538982.251482	46.902260
3503.367771	538954.758065	46.907265
3503.211080	538956.853639	46.912269
3503.448636	538951.159938	46.917274
3503.292326	538933.761279	46.922279
3503.404970	538952.126766	46.927284
3502.580265	538952.459319	46.932289
3503.639267	538920.980213	46.937293
3503.371289	538937.840284	46.942298
3503.396573	538944.805892	46.947303
3503.477946	538948.126414	46.952308
3503.228087	538957.711162	46.957313
3503.346885	538940.269025	46.962317
3503.810903	538935.095056	46.967322
3503.526138	538959.735226	46.972327
3503.566501	538907.912878	46.977332
3503.411878	538904.351778	46.982337
3503.889569	538915.033628	46.987341
3503.910993	538896.950293	46.992346
3503.349122	538942.946624	46.997351
3503.567619	538911.903372	47.002356
3503.662367	538886.131954	47.007361
3503.306304	538882.602689	47.012365
3503.511799	538894.590159	47.017370
3503.259555	538866.802924	47.022375
3503.274647	538898.668269	47.027380
3503.170479	538860.908486	47.032385
3503.284494	538891.697640	47.037389
3503.663901	538850.780699	47.042394
3503.547697	538896.201694	47.047399
3503.560997	538857.009244	47.052404
3503.568134	538887.057751	47.057409
3503.570037	538839.281506	47.062413
3503.911701	538843.570976	47.067418
3503.180335	538829.848833	47.072423
3503.405398	538852.539964	47.077428
3503.709387	538836.987565	47.082433
3503.406050	538831.126798	47.087437
3503.786237	538836.319242	47.092442
3503.232733	538807.215925	47.097447
3503.613034	538814.125478	47.102452
3503.611135	538796.702255	47.107457
3503.431762	538807.942571	47.112461
3503.324917	538785.586581	47.117466
3503.311840	538818.517121	47.122471
3503.766470	538769.558022	47.127476
3503.367329	538820.579360	47.132481
3503.668335	538786.846129	47.137485
3503.402470	538784.110641	47.142490
3503.515544	538741.922414	47.147495
3503.698256	538743.661348	47.152500
3503.092841	538760.423440	47.157505
3503.383292	538747.095249	47.162509
3503.333420	538763.264489	47.167514
3503.471238	538735.920397	47.172519
3503.315506	538767.459491	47.177524
3503.414615	538742.646710	47.182529
3503.531714	538769.395326	47.187533
3503.545891	538716.263371	47.192538
3503.420832	538737.898931	47.197543
3503.729732	538701.033032	47.202548
3503.837566	538738.035444	47.207553
3503.733406	538710.982074	47.212557
3503.847387	538722.277092	47.217562
3503.702200	538681.089090	47.222567
3503.796614	538677.892604	47.227572
3503.618758	538687.466139	47.232577
3503.273908	538672.622177	47.237581
3503.509348	538689.049422	47.242586
3503.387149	538673.564222	47.247591
3503.156130	538648.298429	47.252596
3503.259643	538654.645757	47.257601
3503.567275	538620.961616	47.262605
3503.392343	538658.261438	47.267610
3503.319633	538629.586825	47.272615
3503.304768	538648.831401	47.277620
3503.438050	538632.144184	47.282625
3503.480294	538643.046566	47.287629
3503.609925	538632.521418	47.292634
3503.300972	538634.540095	47.297639
3503.431318	538645.630567	47.302644
3503.496772	538633.347922	47.307649
3503.500794	538622.085059	47.312653
3503.427220	538610.480924	47.317658
3503.440789	538590.428805	47.322663
3503.359083	538609.431476	47.327668
3503.451698	538586.892154	47.332673
3503.290736	538621.311118	47.337677
3503.747312	538594.623445	47.342682
3503.569049	538591.571050	47.347687
3503.426573	538618.158945	47.352692
3503.347304	538588.071174	47.357697
3503.741013	538587.908119	47.362701
3503.626373	538571.058006	47.367706
3503.305610	538581.512768	47.372711
3503.800092	538556.031139	47.377716
3503.597200	538581.467047	47.382721
3503.525093	538568.903068	47.387725
3503.794410	538545.982226	47.392730
3503.399599	538552.610381	47.397735
3503.461922	538521.742534	47.402740
3503.249329	538521.523800	47.407745
3503.584888	538540.107071	47.412749
3503.901545	538524.905882	47.417754
3503.293667	538540.355489	47.422759
3503.507657	538524.968511	47.427764
3503.648769	538500.199201	47.432769
3503.674302	538507.417493	47.437773
3503.675479	538473.983486	47.442778
3503.709286	538502.715414	47.447783
3503.917008	538476.016365	47.452788
3503.878698	538482.234669	47.457793
3503.718211	538462.967463	47.462797
3503.695655	538440.900672	47.467802
3503.372093	538454.335741	47.472807
3503.860058	538418.551959	47.477812
3503.592602	538448.493219	47.482817
3503.589985	538411.978889	47.487821
3503.349736	538417.724090	47.492826
3503.533575	538403.250842	47.497831
3503.371071	538408.478709	47.502836
3503.381922	538415.244821	47.507841
3503.169625	538398.813992	47.512845
3503.189927	538411.437173	47.517850
3503.312331	538422.579567	47.522855
3503.368416	538404.944713	47.527860
3503.599270	538410.665956	47.532865
3503.697792	538371.610304	47.537869
3503.597422	538393.040430	47.542874
3503.490121	538379.572771	47.547879
3503.868117	538354.664772	47.552884
3503.416833	538386.958438	47.557889
3503.808656	538351.189695	47.562893
3503.292314	538360.362392	47.567898
3503.525879	538327.295371	47.572903
3503.741476	538340.998853	47.577908
3503.560014	538321.987310	47.582913
3503.370658	538325.653792	47.587917
3503.440542	538353.319692	47.592922
3503.514152	538321.742587	47.597927
3503.544347	538349.010728	47.602932
3503.422452	538329.282708	47.607937
3503.302020	538311.120091	47.612941
3503.485501	538287.101316	47.617946
3503.121421	538317.159116	47.622951
3503.438826	538281.907025	47.627956
3503.219497	538274.871143	47.632961
3503.015523	538302.580423	47.637965
3503.219027	538282.901920	47.642970
3503.267926	538298.854018	47.647975
3503.584690	538274.662641	47.652980
3503.259918	538281.734389	47.657985
3503.030169	538314.447738	47.662989
3503.361396	538294.193505	47.667994
3503.292936	538300.063111	47.672999
3503.419609	538303.477624	47.678004
3503.394594	538295.855482	47.683009
3503.447029	538305.190834	47.688013
3503.342123	538315.207618	47.693018
3503.458391	538297.815653	47.698023
3503.666805	538280.156577	47.703028
3503.553504	538275.780714	47.708033
3503.315390	538254.959853	47.713037
3503.206269	538269.472305	47.718042
3503.110709	538231.911626	47.723047
3503.420525	538274.994387	47.728052
3503.086527	538266.410964	47.733057
3503.549598	538234.923635	47.738061
3503.094060	538259.793948	47.743066
3503.042259	538272.580157	47.748071
3503.597658	538242.441892	47.753076
3503.461963	538282.716245	47.758081
3503.528925	538258.059274	47.763085
3503.721292	538259.039158	47.768090
3503.467553	538250.544051	47.773095
3503.654743	538249.908583	47.778100
3503.319492	538225.567661	47.783105
3503.305732	538217.287130	47.788109
3503.142078	538226.151633	47.793114
3503.557659	538207.348608	47.798119
3503.271653	538223.151700	47.803124
3503.714830	538192.172483	47.808129
3503.325331	538239.305312	47.813133
3503.555945	538191.793922	47.818138
3503.484980	538227.310668	47.823143
3503.189666	538204.882607	47.828148
3503.483133	538188.876663	47.833153
3503.211166	538178.364174	47.838157
3503.091019	538178.686383	47.843162
3503.040091	538182.583546	47.848167
3503.481355	538169.635059	47.853172
3503.371294	538193.137727	47.858177
3503.494356	538173.017248	47.863181
3503.284041	538198.353956	47.868186
3503.400657	538161.517148	47.873191
3503.258178	538190.631068	47.878196
3503.220696	538181.091628	47.883201
3503.326505	538189.004459	47.888205
3503.511564	538189.076403	47.893210
3503.240611	538180.179933	47.898215
3503.544894	538191.293747	47.903220
3503.083027	538198.639731	47.908225
3503.381147	538171.168279	47.913229
3503.411024	538199.547860	47.918234
3503.326992	538153.348722	47.923239
3502.991823	538171.129359	47.928244
3503.487414	538152.162103	47.933249
3503.128781	538138.026878	47.938253
3503.522325	538153.874146	47.943258
3503.337748	538158.499520	47.948263
3503.500972	538129.231111	47.953268
3503.240855	538163.818295	47.958273
3503.356857	538145.567603	47.963277
3503.314259	538162.695937	47.968282
3503.399718	538137.126746	47.973287
3503.359829	538159.608260	47.978292
3503.122162	538163.332922	47.983297
3503.270677	538124.824298	47.988301
3503.551042	538169.023139	47.993306
3503.352091	538161.377917	47.998311
3503.709286	538123.846419	48.003316
3503.247866	538154.475488	48.008321
3503.091863	538110.762373	48.013325
3503.345282	538126.429796	48.018330
3503.164596	538094.892417	48.023335
3503.092218	538128.136854	48.028340
3503.460849	538112.371478	48.033345
3503.285953	538126.288394	48.038349
3503.661858	538112.744121	48.043354
3503.104127	538126.620537	48.048359
3503.383076	538111.172370	48.053364
3503.466048	538113.331188	48.058369
3502.947915	538137.201479	48.063373
3503.498256	538124.185207	48.068378
3503.308270	538125.023513	48.073383
3503.734179	538120.208835	48.078388
3503.063410	538132.587941	48.083393
3503.305012	538123.913455	48.088397
3503.456460	538122.576551	48.093402
3503.598784	538122.453228	48.098407
3503.431268	538108.792824	48.103412
3503.470317	538058.331456	48.108417
3503.139109	538098.485680	48.113421
3503.614709	538095.935902	48.118426
3503.688402	538066.125961	48.123431
3503.515856	538095.396332	48.128436
3503.299802	538094.117515	48.133441
3503.657923	538065.272730	48.138445
3503.527839	538084.435218	48.143450
3503.451515	538037.274899	48.148455
3503.531705	538062.565913	48.153460
3503.489089	538020.450808	48.158465
3503.186491	538069.590668	48.163469
3503.316171	538038.812211	48.168474
3503.359462	538052.543187	48.173479
3503.412665	538037.383158	48.178484
3503.358293	538039.563696	48.183489
3503.172657	538055.250085	48.188493
3503.649631	538022.244942	48.193498
3503.616216	538066.443172	48.198503
3503.646154	538021.589281	48.203508
3503.375078	538001.530876	48.208513
3502.996307	538041.238213	48.213517
3503.222318	538003.222094	48.218522
3503.237039	537979.532548	48.223527
3503.228167	538019.332992	48.228532
3502.931941	538013.420278	48.233537
3503.474033	538009.748842	48.238541
3503.535682	538008.274604	48.243546
3503.402170	537984.709509	48.248551
3503.402315	538032.286449	48.253556
3503.306677	538008.715404	48.258561
3503.643026	537995.833861	48.263565
3503.317977	538036.744865	48.268570
3503.236599	538001.656174	48.273575
3503.412833	538023.295628	48.278580
3503.341491	537991.286197	48.283585
3503.277594	538016.095001	48.288589
3503.523875	537966.913734	48.293594
3503.387086	538000.017112	48.298599
3503.324952	537986.845004	48.303604
3503.276688	537969.680697	48.308609
3503.211889	537998.378654	48.313613
3503.395596	537981.581744	48.318618
3503.295906	538006.396221	48.323623
3503.371526	537981.232374	48.328628
3503.441808	538009.555415	48.333633
3503.121779	537999.353437	48.338637
3503.506108	537984.393546	48.343642
3502.830991	538022.279044	48.348647
3503.164124	537972.023437	48.353652
3503.294706	538018.064616	48.358657
3502.812531	538003.847782	48.363661
3503.537032	537960.247591	48.368666
3503.265184	538008.827216	48.373671
3503.198011	537988.787070	48.378676
3503.476239	537998.389957	48.383681
3502.897935	538009.390879	48.388685
3503.365285	537977.094247	48.393690
3503.172780	537984.902818	48.398695
3503.198358	538018.536060	48.403700
3503.312772	538008.366429	48.408705
3503.214174	537999.998178	48.413709
3503.375464	537974.921791	48.418714
3503.097233	538011.734456	48.423719
3503.464010	538022.737503	48.428724
3503.257818	538014.083230	48.433729
3503.280532	538007.918076	48.438733
3504.118938	537947.481293	48.443738
3503.536337	537957.422298	48.448743
3503.069683	537997.244653	48.453748
3503.287521	537997.462936	48.458753
3503.188370	537973.538849	48.463757
3503.335696	537964.576137	48.468762
3503.579899	537950.698995	48.473767
3503.500130	537943.438875	48.478772
3503.155495	537993.848281	48.483777
3503.071279	537969.366259	48.488781
3503.480247	537974.453438	48.493786
3503.151027	537965.566052	48.498791
3503.333459	537960.789810	48.503796
3503.245605	537987.218649	48.508801
3502.909216	537972.170642	48.513805
3503.606089	537960.343220	48.518810
3503.355542	537937.554145	48.523815
3503.497092	537946.168542	48.528820
3503.519813	537932.427404	48.533825
3503.806620	537896.876225	48.538829
3503.854441	537887.979703	48.543834
3503.837930	537905.306228	48.548839
3503.643680	537889.276049	48.553844
3503.364150	537865.632838	48.558849
3503.355194	537906.191188	48.563853
3502.908603	537882.826942	48.568858
3503.407371	537865.980105	48.573863
3503.386348	537902.752377	48.578868
3503.354781	537887.403572	48.583873
3502.871537	537878.590988	48.588877
3503.886144	537855.096749	48.593882
3503.728651	537841.384015	48.598887
3503.583082	537862.569495	48.603892
3503.695298	537892.300310	48.608897
3503.086859	537846.183134	48.613901
3503.798862	537798.190377	48.618906
3503.388250	537831.286895	48.623911
3503.493511	537856.422767	48.628916
3503.428103	537855.776703	48.633921
3502.543480	537847.280078	48.638925
3503.393186	537825.832125	48.643930
3503.385143	537830.328680	48.648935
3502.875994	537862.026519	48.653940
3503.409833	537831.133254	48.658945
3503.411261	537877.397298	48.663949
3503.249171	537846.058493	48.668954
3503.093529	537830.173669	48.673959
3503.278590	537866.812439	48.678964
3503.426304	537850.324114	48.683969
3503.516976	537822.531280	48.688973
3503.344268	537867.812742	48.693978
3503.179100	537855.010353	48.698983
3503.404091	537842.499829	48.703988
3503.500684	537861.222713	48.708993
3503.152190	537808.397459	48.713997
3503.335206	537781.297049	48.719002
3503.270419	537835.198224	48.724007
3503.182084	537818.848190	48.729012
3503.519065	537785.460611	48.734017
3503.399176	537796.742774	48.739021
3503.267282	537829.997266	48.744026
3503.258597	537844.292219	48.749031
3503.313938	537801.302414	48.754036
3503.467937	537815.016105	48.759041
3503.237051	537833.689772	48.764045
3503.515838	537792.634386	48.769050
3503.263753	537837.120376	48.774055
3503.405313	537834.370823	48.779060
3503.910942	537796.411007	48.784065
3503.103555	537816.539504	48.789069
3503.377149	537794.071421	48.794074
3503.459006	537755.673419	48.799079
3503.398687	537762.451070	48.804084
3503.334636	537791.906900	48.809089
3503.023725	537768.521032	48.814093
3503.733013	537761.843201	48.819098
3503.220931	537816.269708	48.824103
3503.422115	537803.257847	48.829108
3503.205549	537777.533767	48.834113
3503.193664	537757.585593	48.839117
3503.064311	537797.708699	48.844122
3503.437568	537783.760500	48.849127
3503.236812	537785.156102	48.854132
3503.402935	537773.563951	48.859137
3503.263823	537797.576887	48.864141
3503.675375	537759.025766	48.869146
3503.235288	537741.569589	48.874151
3503.269266	537783.283140	48.879156
3503.198830	537764.404874	48.884161
3502.895009	537744.149279	48.889165
3503.539713	537724.349813	48.894170
3503.153133	537727.340512	48.899175
3503.240280	537772.985237	48.904180
3503.200817	537763.294329	48.909185
3502.886858	537742.636279	48.914189
3503.179013	537741.226594	48.919194
3502.995718	537745.801382	48.924199
3503.185516	537771.479608	48.929204
3503.262116	537768.790818	48.934209
3503.412848	537786.192056	48.939213
3503.147643	537754.717842	48.944218
3503.450181	537719.921370	48.949223
3503.623146	537767.320295	48.954228
3503.257364	537764.650923	48.959233
3503.153001	537742.949604	48.964237
3503.407966	537759.425271	48.969242
3502.968471	537752.423948	48.974247
3503.288546	537728.887777	48.979252
3503.458261	537781.842946	48.984257
3503.410145	537787.153958	48.989261
3503.208310	537764.963008	48.994266
3503.415269	537734.373752	48.999271
3503.335344	537755.094442	49.004276
3503.514113	537770.369973	49.009281
3503.330481	537759.691713	49.014285
3503.556530	537736.119907	49.019290
3503.461409	537771.035447	49.024295
3503.125086	537737.602669	49.029300
3503.648041	537703.023853	49.034305
3503.351179	537701.858790	49.039309
3503.319701	537738.077531	49.044314
3503.136788	537724.419217	49.049319
3503.276512	537707.426930	49.054324
3503.436297	537749.575252	49.059329
3502.964306	537741.366893	49.064333
3503.184841	537720.472807	49.069338
3503.650598	537701.307681	49.074343
3503.220450	537724.912170	49.079348
3503.358530	537742.567993	49.084353
3503.480216	537715.073104	49.089357
3503.626245	537723.838440	49.094362
3503.575094	537755.817653	49.099367
3503.385864	537730.291201	49.104372
3503.662184	537692.973459	49.109377
3503.084342	537688.771869	49.114381
3503.914128	537661.569016	49.119386
3503.485480	537681.637824	49.124391
3503.320959	537691.815960	49.129396
3503.688169	537663.069997	49.134401
3503.361589	537702.517425	49.139405
3503.527933	537686.177500	49.144410
3503.268727	537666.419821	49.149415
3503.362044	537641.555662	49.154420
3503.528136	537626.225860	49.159425
3503.072744	537676.098237	49.164429
3503.161151	537649.214576	49.169434
3503.762067	537616.946581	49.174439
3503.310923	537642.726333	49.179444
3503.419622	537677.155304	49.184449
3503.237691	537662.638157	49.189453
3503.806494	537629.213595	49.194458
3503.448712	537633.967519	49.199463
3503.405599	537649.985346	49.204468
3503.700616	537610.189588	49.209473
3503.220682	537624.104668	49.214477
3503.584781	537593.136739	49.219482
3503.368672	537637.971174	49.224487
3503.346217	537596.205266	49.229492
3503.611675	537587.324677	49.234497
3503.407894	537641.854593	49.239501
3503.386077	537613.624595	49.244506
3503.517092	537599.108429	49.249511
3503.429308	537600.839743	49.254516
3503.591163	537596.975775	49.259521
3503.228813	537570.819824	49.264525
3503.929564	537540.505683	49.269530
3503.770688	537547.804083	49.274535
3503.749568	537580.940591	49.279540
3503.199475	537542.894482	49.284545
3503.385411	537527.763476	49.289549
3503.572994	537554.907139	49.294554
3503.299810	537567.678422	49.299559
3503.107131	537566.294850	49.304564
3503.635896	537550.655108	49.309569
3503.257797	537545.209723	49.314573
3503.047613	537533.777886	49.319578
3503.375622	537517.765782	49.324583
3503.544913	537500.111991	49.329588
3503.637443	537539.493592	49.334593
3503.188168	537561.182064	49.339597
3503.648238	537534.239455	49.344602
3503.613054	537504.193091	49.349607
3503.728644	537480.890892	49.354612
3503.430111	537506.848781	49.359617
3503.102747	537490.738210	49.364621
3503.474051	537463.354937	49.369626
3503.384393	537495.037734	49.374631
3503.357355	537518.225267	49.379636
3503.384671	537484.279887	49.384641
3503.270193	537513.845238	49.389645
3503.539284	537500.721372	49.394650
3503.780452	537493.965896	49.399655
3503.235432	537460.211945	49.404660
3503.679914	537478.324721	49.409665
3503.226299	537455.516518	49.414669
3503.391713	537435.539899	49.419674
3503.507509	537482.544679	49.424679
3503.194535	537459.764760	49.429684
3503.580113	537423.994839	49.434689
3503.252649	537445.866251	49.439693
3503.583806	537449.046603	49.444698
3503.528740	537425.165198	49.449703
3503.246971	537451.575104	49.454708
3503.676905	537428.677711	49.459713
3503.355962	537417.970407	49.464717
3503.383941	537406.349306	49.469722
3503.463522	537441.389507	49.474727
3503.274534	537426.216647	49.479732
3503.554639	537420.364129	49.484737
3503.182664	537457.344467	49.489741
3503.443011	537408.916805	49.494746
3503.339090	537416.812679	49.499751
3503.203572	537444.209642	49.504756
3503.616793	537399.343853	49.509761
3503.317966	537418.180289	49.514765
3503.631136	537371.057369	49.519770
3503.064716	537406.300776	49.524775
3503.025155	537375.951803	49.529780
3503.614296	537347.018644	49.534785
3503.119731	537397.605234	49.539789
3503.638385	537369.541897	49.544794
3503.044682	537381.808407	49.549799
3502.975386	537392.729312	49.554804
3503.386414	537361.905024	49.559809
3503.410398	537408.672001	49.564813
3503.361463	537398.830835	49.569818
3503.093868	537379.175127	49.574823
3503.659362	537358.327039	49.579828
3503.664198	537389.338510	49.584833
3503.173169	537412.498528	49.589837
3503.173215	537379.516880	49.594842
3503.473940	537362.599780	49.599847
3503.120568	537371.393747	49.604852
3503.584828	537388.543847	49.609857
3503.175016	537363.051649	49.614861
3503.204932	537344.712594	49.619866
3503.781671	537334.570456	49.624871
3503.362982	537332.616486	49.629876
3503.598616	537370.814208	49.634881
3503.151463	537384.875847	49.639885
3503.422211	537379.327842	49.644890
3503.387714	537364.635583	49.649895
3503.485031	537334.972010	49.654900
3503.575670	537364.606243	49.659905
3502.782238	537345.942758	49.664909
3503.532238	537326.126136	49.669914
3503.278327	537346.268779	49.674919
3503.396374	537350.139444	49.679924
3503.534716	537313.802247	49.684929
3503.179652	537315.070757	49.689933
3503.339483	537321.207703	49.694938
3503.684527	537321.001823	49.699943
3503.356347	537305.497286	49.704948
3503.325064	537328.180693	49.709953
3503.548140	537315.417501	49.714957
3503.521056	537313.452138	49.719962
3503.632723	537322.576694	49.724967
3503.260662	537304.200112	49.729972
3503.406651	537299.782985	49.734977
3503.181369	537287.898775	49.739981
3503.618105	537291.264505	49.744986
3503.452891	537274.117904	49.749991
3503.298883	537275.304129	49.754996
3503.625078	537297.981584	49.760001
3502.964438	537286.822798	49.765005
3503.732927	537276.195737	49.770010
3503.077715	537302.210351	49.775015
3503.427978	537272.658200	49.780020
3503.355257	537296.964477	49.785025
3502.828708	537314.675340	49.790029
3503.383083	537270.948558	49.795034
3503.646455	537287.928490	49.800039
3502.924991	537288.850849	49.805044
3503.452265	537262.856804	49.810049
3503.545053	537292.389820	49.815053
3503.453327	537250.280360	49.820058
3503.120616	537239.120213	49.825063
3503.466769	537225.882914	49.830068
3503.569361	537256.323607	49.835073
3503.610304	537231.366044	49.840077
3503.717686	537247.613047	49.845082
3503.686296	537258.477547	49.850087
3503.667070	537219.387059	49.855092
3503.656504	537233.379827	49.860097
3503.904895	537208.742997	49.865101
3503.597324	537213.085043	49.870106
3503.604252	537192.375528	49.875111
3503.221356	537209.962787	49.880116
3503.732583	537164.777769	49.885121
3503.341458	537187.265719	49.890125
3503.539059	537141.221046	49.895130
3503.554567	537188.848685	49.900135
3503.371773	537173.118998	49.905140
3503.844516	537141.476371	49.910145
3503.284100	537182.123804	49.915149
3503.446153	537141.388180	49.920154
3503.689078	537142.057092	49.925159
3503.431417	537165.988737	49.930164
3503.510427	537148.298304	49.935169
3503.067604	537141.297226	49.940173
3503.563669	537110.256955	49.945178
3503.081115	537152.104379	49.950183
3502.803602	537148.107712	49.955188
3503.099526	537118.917417	49.960193
3503.498671	537121.228437	49.965197
3503.402973	537150.084393	49.970202
3503.491714	537160.525903	49.975207
3503.341502	537141.457443	49.980212
3503.512258	537124.106043	49.985217
3503.621469	537142.625774	49.990221
3503.476349	537107.646128	49.995226
3503.483217	537117.292463	50.000231
3503.481144	537071.127614	50.005236
3503.431246	537096.794350	50.010241
3503.232617	537084.249149	50.015245
3503.331580	537094.335524	50.020250
3502.841580	537085.675075	50.025255
3503.055829	537056.649100	50.030260
3503.133873	537096.539221	50.035265
3503.424020	537105.736713	50.040269
3502.843297	537088.251509	50.045274
3503.474734	537063.957975	50.050279
3503.377546	537121.553955	50.055284
3503.470399	537113.154957	50.060289
3503.161492	537103.758767	50.065293
3503.503868	537069.762670	50.070298
3503.659309	537069.940321	50.075303
3503.354002	537113.729693	50.080308
3503.656393	537076.002257	50.085313
3503.276869	537082.174044	50.090317
3503.276475	537039.140402	50.095322
3503.143791	537060.981574	50.100327
3503.148581	537048.555719	50.105332
3503.363600	537073.220944	50.110337
3503.226127	537050.614712	50.115341
3502.986223	537064.037773	50.120346
3503.433566	537063.310628	50.125351
3503.089148	537056.647521	50.130356
3503.228060	537053.494173	50.135361
3503.054277	537071.402102	50.140365
3503.177818	537036.682883	50.145370
3503.261796	537067.581477	50.150375
3503.113105	537043.057656	50.155380
3503.136706	537068.965367	50.160385
3502.898222	537057.537648	50.165389
3503.542232	537029.958970	50.170394
3503.275629	537056.720723	50.175399
3503.308717	537085.910008	50.180404
3503.148768	537046.285721	50.185409
3503.508283	537039.915414	50.190413
3503.254176	537074.857669	50.195418
3502.963420	537060.660207	50.200423
3503.597074	537033.638775	50.205428
3503.730953	537075.944572	50.210433
3503.220700	537076.530502	50.215437
3503.679044	537042.111939	50.220442
3503.739645	537078.166156	50.225447
3503.087481	537046.600124	50.230452
3503.743893	537001.492696	50.235457
3503.480120	537047.296070	50.240461
3503.451181	537015.985029	50.245466
3503.471267	537027.043594	50.250471
3503.265364	537013.539808	50.255476
3503.511361	536983.700526	50.260481
3503.336129	537039.743354	50.265485
3503.285694	537032.175110	50.270490
3503.407924	537012.053238	50.275495
3503.200952	537040.522914	50.280500
3503.552470	537003.393647	50.285505
3502.972255	537014.143032	50.290509
3503.473010	536987.344563	50.295514
3503.014258	537015.197459	50.300519
3503.577497	536964.346576	50.305524
3503.396012	536993.923520	50.310529
3503.085157	536985.588264	50.315533
3503.541700	536973.444509	50.320538
3503.840022	537000.521140	50.325543
3503.694249	536969.683058	50.330548
3503.666125	536996.407220	50.335553
3503.496041	536972.139215	50.340557
3503.426133	536978.312613	50.345562
3503.510281	536929.507214	50.350567
3503.556069	536923.691546	50.355572
3503.610212	536956.918524	50.360577
3503.265554	536939.900933	50.365581
3503.568268	536931.317135	50.370586
3503.462428	536963.559193	50.375591
3503.420721	536932.047961	50.380596
3503.378331	536957.057118	50.385601
3503.332117	536902.110065	50.390605
3503.320040	536911.456464	50.395610
3503.243610	536913.640649	50.400615
3503.238022	536889.194982	50.405620
3503.549732	536912.380397	50.410625
3503.653060	536880.543076	50.415629
3503.409232	536925.131424	50.420634
3503.505000	536895.921834	50.425639
3503.058189	536882.354992	50.430644
3503.399646	536926.042667	50.435649
3503.050980	536904.378777	50.440653
3503.495808	536886.024101	50.445658
3503.448332	536920.630986	50.450663
3503.510283	536897.891988	50.455668
3503.637692	536895.144504	50.460673
3503.531966	536853.440246	50.465677
3503.407605	536876.543113	50.470682
3503.563194	536860.102990	50.475687
3503.488288	536851.780876	50.480692
3503.642462	536872.162695	50.485697
3503.588710	536850.704662	50.490701
3503.648611	536868.272830	50.495706
3503.209126	536834.147248	50.500711
3503.456041	536820.571717	50.505716
3503.481289	536848.398921	50.510721
3503.461474	536835.421174	50.515725
3503.534366	536827.631294	50.520730
3503.511718	536817.684581	50.525735
3503.465331	536788.850827	50.530740
3503.467962	536751.321507	50.535745
3503.303955	536709.019947	50.540749
3503.198423	536638.019005	50.545754
3503.184973	536599.633175	50.550759
3503.045841	536498.835517	50.555764
3503.174063	536423.604215	50.560769
3503.131461	536296.978654	50.565773
3502.851116	536224.134499	50.570778
3503.110499	536084.477867	50.575783
3502.636295	535991.357229	50.580788
3502.464483	535823.428700	50.585793
3502.295067	535658.175198	50.590797
3502.123501	535498.072734	50.595802
3501.620587	535387.929634	50.600807
3501.518505	535233.521610	50.605812
3501.158858	535026.111125	50.610817
3501.288123	534825.086703	50.615821
3500.721720	534686.305712	50.620826
3500.665508	534481.315300	50.625831
3500.618609	534254.648312	50.630836
3500.080378	534053.012131	50.635841
3499.833524	533837.383817	50.640845
3499.432579	533599.244711	50.645850
3499.765362	533338.908140	50.650855
3499.058250	533133.396582	50.655860
3498.759108	532883.509314	50.660865
3498.841095	532607.841218	50.665869
3498.356496	532329.377912	50.670874
3497.743695	532105.194292	50.675879
3497.005780	531825.953661	50.680884
3496.737706	531532.789324	50.685889
3496.585390	531245.816180	50.690893
3496.427061	530980.566242	50.695898
3495.721537	530696.399081	50.700903
3495.056078	530367.298466	50.705908
3495.596506	530037.596110	50.710913
3494.975753	529749.204315	50.715917
3494.466723	529433.400203	50.720922
3493.848812	529135.041560	50.725927
3493.238361	528802.059002	50.730932
3493.294035	528435.761282	50.735937
3492.518274	528139.531432	50.740941
3492.119452	527779.708780	50.745946
3491.695814	527436.054841	50.750951
3491.071051	527081.912674	50.755956
3490.509659	526722.546755	50.760961
3490.223461	526398.257114	50.765965
3489.546713	526017.614737	50.770970
3489.393180	525621.565178	50.775975
3488.540337	525292.136516	50.780980
3487.737654	524920.131605	50.785985
3487.334657	524531.373611	50.790989
3486.829010	524192.869794	50.795994
3486.365267	523799.705906	50.800999
3486.016262	523409.850835	50.806004
3485.341578	523029.289295	50.811009
3485.076247	522640.009167	50.816013
3484.466917	522236.719374	50.821018
3483.658451	521872.279483	50.826023
3482.913107	521460.751096	50.831028
3482.940036	521062.387629	50.836033
3482.008435	520668.312043	50.841037
3481.162059	520250.398480	50.846042
3480.971932	519855.629997	50.851047
3480.078757	519468.295139	50.856052
3479.548979	519054.852053	50.861057
3479.069255	518634.918047	50.866061
3478.684778	518232.050641	50.871066
3478.076397	517824.252968	50.876071
3477.427018	517380.242592	50.881076
3476.946222	516969.521213	50.886081
3476.057038	516525.778834	50.891085
3475.328300	516104.960545	50.896090
3474.599646	515690.959509	50.901095
3474.045998	515246.927869	50.906100
3473.283243	514854.356630	50.911105
3472.993147	514408.136851	50.916109
3472.273577	514012.554914	50.921114
3471.327856	513570.716073	50.926119
3470.681181	513139.087033	50.931124
3470.536420	512723.555036	50.936129
3469.654071	512279.649101	50.941133
3468.970309	511868.936585	50.946138
3468.372008	511431.489497	50.951143
3468.216905	510967.350432	50.956148
3467.390851	510559.209042	50.961153
3466.342786	510108.645324	50.966157
3466.042641	509648.085600	50.971162
3465.294686	509251.486956	50.976167
3464.446775	508782.591786	50.981172
3463.949913	508373.030980	50.986177
3463.259394	507917.799632	50.991181
3462.463697	507492.731147	50.996186
3462.026314	507053.578811	51.001191
3461.030416	506601.599801	51.006196
3460.680431	506172.481548	51.011201
3459.673111	505722.708203	51.016205
3458.914544	505283.663347	51.021210
3458.389879	504842.546186	51.026215
3457.272954	504444.175661	51.031220
3457.189124	503953.419513	51.036225
3456.448870	503545.909749	51.041229
3455.657034	503096.187049	51.046234
3455.188706	502674.999185	51.051239
3454.747826	502202.775980	51.056244
3453.839546	501800.314297	51.061249
3452.398181	501345.942587	51.066253
3452.403164	500887.027970	51.071258
3451.688223	500487.239612	51.076263
3450.500418	500013.001148	51.081268
3450.031903	499599.081034	51.086273
3449.211634	499140.859745	51.091277
3448.602454	498734.636991	51.096282
3448.237406	498282.447697	51.101287
3446.976214	497860.867107	51.106292
3446.582317	497410.179479	51.111297
3446.033160	496964.720213	51.116301
3444.820053	496555.405059	51.121306
3444.438848	496100.632487	51.126311
3443.606439	495709.415538	51.131316
3443.264225	495242.210074	51.136321
3442.415235	494833.912869	51.141325
3441.804852	494396.198887	51.146330
3441.379953	493944.013029	51.151335
3440.279315	493526.966099	51.156340
3439.930386	493081.938096	51.161345
3438.804292	492670.091997	51.166349
3438.324835	492201.666616	51.171354
3437.335272	491804.162655	51.176359
3436.491484	491368.541268	51.181364
3436.238331	490942.895190	51.186369
3435.491895	490507.238385	51.191373
3434.490076	490099.367879	51.196378
3434.415385	489646.566653	51.201383
3433.318088	489230.892216	51.206388
3432.858739	488810.194427	51.211393
3431.911375	488371.531544	51.216397
3431.148535	487934.956878	51.221402
3430.376634	487521.574333	51.226407
3429.627848	487094.602919	51.231412
3428.884157	486649.839912	51.236417
3428.573561	486256.468606	51.241421
3427.552996	485819.785028	51.246426
3426.744654	485423.233043	51.251431
3426.309980	484991.048272	51.256436
3425.330636	484558.737283	51.261441
3424.441809	484164.452053	51.266445
3423.786495	483738.962015	51.271450
3423.265265	483315.721498	51.276455
3422.215516	482916.420277	51.281460
3422.326060	482487.336320	51.286465
3421.333154	482080.053852	51.291469
3420.661812	481668.810335	51.296474
3420.021104	481229.429864	51.301479
3419.282884	480840.779725	51.306484
3418.287908	480409.595475	51.311489
3417.561806	480016.467765	51.316493
3417.349912	479609.720148	51.321498
3416.658989	479176.535216	51.326503
3415.561656	478794.641862	51.331508
3415.124948	478359.979930	51.336513
3414.502547	477957.824663	51.341517
3413.117945	477556.998194	51.346522
3412.787320	477132.986785	51.351527
3412.208283	476753.354596	51.356532
3411.820084	476322.087311	51.361537
3411.155867	475912.142789	51.366541
3410.265568	475501.414692	51.371546
3409.540869	475107.531362	51.376551
3408.967265	474681.276559	51.381556
3408.031284	474265.461695	51.386561
3406.980068	473876.218974	51.391565
3406.351339	473464.850751	51.396570
3405.930460	473057.953124	51.401575
3404.933450	472670.402465	51.406580
3404.323546	472259.514019	51.411585
3403.588379	471857.002115	51.416589
3402.897460	471459.899998	51.421594
3402.472354	471065.739435	51.426599
3401.462436	470682.057233	51.431604
3400.867347	470256.322371	51.436609
3400.173441	469885.199903	51.441613
3399.725014	469480.416356	51.446618
3398.884241	469083.647428	51.451623
3398.019032	468682.970608	51.456628
3397.288985	468281.605592	51.461633
3396.629027	467906.335533	51.466637
3395.944925	467487.657287	51.471642
3395.374607	467117.683271	51.476647
3394.703892	466716.532615	51.481652
3393.716449	466336.722640	51.486657
3393.142393	465944.720605	51.491661
3392.045015	465548.838575	51.496666
3391.778401	465167.220255	51.501671
3391.180365	464785.748954	51.506676
3390.367182	464371.238968	51.511681
3389.462469	464010.392487	51.516685
3388.711923	463615.637041	51.521690
3388.209943	463224.080968	51.526695
3387.618746	462825.989250	51.531700
3386.735761	462461.867459	51.536705
3386.440359	462071.627287	51.541709
3385.858713	461667.274226	51.546714
3385.102801	461304.634580	51.551719
3384.342370	460909.172043	51.556724
3383.706121	460513.885613	51.561729
3382.767519	460155.364412	51.566733
3382.027724	459763.935902	51.571738
3381.401699	459361.373384	51.576743
3380.632353	458997.733929	51.581748
3380.237160	458612.622114	51.586753
3379.095692	458221.432685	51.591757
3378.069709	457863.750474	51.596762
3377.332772	457473.092657	51.601767
3376.717440	457091.540433	51.606772
3376.280124	456742.574422	51.611777
3375.657980	456374.505823	51.616781
3375.030115	455990.552360	51.621786
3374.411446	455608.417339	51.626791
3373.393109	455236.080287	51.631796
3372.969448	454876.530127	51.636801
3372.365296	454493.206993	51.641805
3371.575933	454125.381811	51.646810
3370.764479	453740.658077	51.651815
3370.165785	453376.799019	51.656820
3369.576551	453011.207481	51.661825
3368.675939	452637.540702	51.666829
3367.549641	452272.073024	51.671834
3367.149929	451893.291424	51.676839
3366.458988	451553.368733	51.681844
3366.072700	451176.298512	51.686849
3365.267029	450816.897148	51.691853
3364.510493	450462.404821	51.696858
3363.706712	450084.418662	51.701863
3363.070982	449723.857057	51.706868
3362.510563	449352.468498	51.711873
3362.054989	448992.882080	51.716877
3361.088845	448621.647570	51.721882
3360.593391	448260.787467	51.726887
3359.512169	447903.364075	51.731892
3359.106498	447545.016387	51.736897
3358.511003	447176.441098	51.741901
3357.841340	446810.054224	51.746906
3357.106880	446443.621180	51.751911
3356.190516	446090.864536	51.756916
3355.756799	445726.555379	51.761921
3355.068183	445367.508966	51.766925
3354.240109	445011.981517	51.771930
3353.760847	444634.212052	51.776935
3352.989526	444286.532487	51.781940
3352.737961	443923.943707	51.786945
3351.629832	443562.094067	51.791949
3351.323007	443185.645171	51.796954
3350.406853	442822.586592	51.801959
3349.427234	442473.847880	51.806964
3349.006422	442103.897945	51.811969
3348.421257	441756.304920	51.816973
3347.314949	441390.513766	51.821978
3347.039520	441030.119280	51.826983
3346.279419	440668.679277	51.831988
3345.409867	440309.383520	51.836993
3344.667618	439952.397749	51.841997
3344.006464	439599.100152	51.847002
3343.482570	439256.945205	51.852007
3342.719005	438899.541468	51.857012
3342.159498	438529.509009	51.862017
3341.533508	438184.664572	51.867021
3340.713889	437832.890116	51.872026
3340.375079	437468.468216	51.877031
3339.661528	437117.174679	51.882036
3338.618818	436751.508180	51.887041
3338.122483	436399.129386	51.892045
3337.276179	436032.431280	51.897050
3336.720404	435679.467932	51.902055
3335.839166	435331.095770	51.907060
3335.244459	434981.734118	51.912065
3334.902890	434636.643885	51.917069
3333.820257	434278.666517	51.922074
3333.534706	433914.185107	51.927079
3332.559591	433570.856472	51.932084
3332.113723	433215.099510	51.937089
3331.308445	432863.761800	51.942093
3330.503500	432511.302025	51.947098
3330.326616	432150.282560	51.952103
3329.076520	431806.897802	51.957108
3328.628034	431438.141319	51.962113
3327.845603	431090.635703	51.967117
3327.115397	430744.590030	51.972122
3326.341357	430395.093162	51.977127
3325.806444	430046.518802	51.982132
3325.021926	429698.436403	51.987137
3324.281472	429351.586787	51.992141
3323.511504	429008.546559	51.997146
3323.235887	428647.342135	52.002151
3322.163908	428316.860696	52.007156
3321.518521	427967.641541	52.012161
3321.003176	427618.422646	52.017165
3319.777012	427267.914789	52.022170
3319.768204	426928.003591	52.027175
3318.913483	426585.656740	52.032180
3318.005290	426237.472511	52.037185
3317.469154	425897.758703	52.042189
3316.485997	425554.911132	52.047194
3316.569894	425206.734523	52.052199
3315.381647	424871.250987	52.057204
3314.814968	424527.486420	52.062209
3314.307602	424181.980968	52.067213
3313.533265	423841.288580	52.072218
3312.928454	423485.451960	52.077223
3312.182665	423156.913322	52.082228
3311.485644	422805.476808	52.087233
3310.637046	422475.371459	52.092237
3309.725143	422139.226617	52.097242
3309.445837	421781.817887	52.102247
3308.653469	421445.848969	52.107252
3307.891881	421105.425699	52.112257
3307.420757	420769.905892	52.117261
3306.865116	420432.159963	52.122266
3306.148395	420084.832956	52.127271
3305.351996	419749.352409	52.132276
3304.963867	419397.620929	52.137281
3304.166471	419064.926861	52.142285
3303.341649	418726.593397	52.147290
3303.030531	418371.483601	52.152295
3302.123093	418026.803646	52.157300
3301.163780	417697.167835	52.162305
3300.842893	417353.098347	52.167309
3300.096359	417010.108307	52.172314
3299.387427	416671.833836	52.177319
3298.654581	416340.850923	52.182324
3298.217228	415989.491837	52.187329
3297.622504	415643.717599	52.192333
3296.457147	415294.675691	52.197338
3296.169576	414965.613878	52.202343
3295.355516	414631.854880	52.207348
3294.384657	414298.421781	52.212353
3294.021835	413952.489211	52.217357
3293.342459	413610.414015	52.222362
3292.697789	413273.030106	52.227367
3291.817836	412932.173023	52.232372
3291.357925	412598.690714	52.237377
3290.688023	412261.172233	52.242381
3289.725358	411938.053207	52.247386
3289.569321	411584.691240	52.252391
3288.590475	411247.718390	52.257396
3287.975776	410911.548149	52.262401
3287.418623	410572.518938	52.267405
3286.825985	410223.072606	52.272410
3286.293346	409877.119647	52.277415
3285.242460	409544.891274	52.282420
3284.786176	409210.379716	52.287425
3283.878805	408879.087066	52.292429
3283.159861	408533.529505	52.297434
3282.691823	408197.966775	52.302439
3282.049207	407851.932019	52.307444
3281.012887	407509.030775	52.312449
3280.559093	407194.065822	52.317453
3279.786390	406828.064342	52.322458
3278.899880	406526.275098	52.327463
3278.507138	406181.122501	52.332468
3277.781035	405842.703127	52.337473
3277.034471	405525.226030	52.342477
3275.945529	405176.563413	52.347482
3275.538702	404852.773399	52.352487
3275.208659	404527.798748	52.357492
3274.387591	404177.888128	52.362497
3273.668986	403853.959282	52.367501
3272.962146	403522.908371	52.372506
3272.428093	403188.674887	52.377511
3271.671129	402865.631680	52.382516
3270.927101	402534.322225	52.387521
3270.455647	402200.271869	52.392525
3269.674018	401872.469301	52.397530
3269.399250	401536.144097	52.402535
3268.156636	401209.043194	52.407540
3267.275002	400869.833007	52.412545
3266.992910	400550.911169	52.417549
3266.234054	400219.478680	52.422554
3265.892704	399877.096876	52.427559
3264.998551	399546.822899	52.432564
3264.528441	399218.969775	52.437569
3263.643476	398883.603517	52.442573
3262.873438	398563.493931	52.447578
3262.438919	398237.099881	52.452583
3261.643057	397900.768986	52.457588
3261.229238	397570.704378	52.462593
3260.269905	397236.706064	52.467597
3259.566926	396905.002754	52.472602
3259.243950	396568.176904	52.477607
3258.019875	396247.786464	52.482612
3257.597307	395921.571363	52.487617
3257.157954	395587.449027	52.492621
3255.938032	395276.531760	52.497626
3255.662643	394934.317709	52.502631
3255.100783	394610.934156	52.507636
3254.321850	394279.878234	52.512641
3253.904869	393950.261933	52.517645
3253.447579	393603.715740	52.522650
3252.886118	393269.056192	52.527655
3252.002139	392938.029440	52.532660
3250.934133	392602.121459	52.537665
3250.407042	392272.659178	52.542669
3249.536212	391941.875145	52.547674
3248.926335	391605.122324	52.552679
3248.321026	391276.552985	52.557684
3247.600125	390947.617464	52.562689
3246.935289	390616.152715	52.567693
3246.271552	390294.982835	52.572698
3245.681094	389960.296334	52.577703
3244.891356	389624.977089	52.582708
3244.052743	389307.106188	52.587713
3243.715442	388982.033205	52.592717
3243.037730	388661.944298	52.597722
3242.301006	388319.306455	52.602727
3241.559355	387996.094009	52.607732
3241.138395	387669.471280	52.612737
3240.364399	387339.926206	52.617741
3239.496284	387004.544189	52.622746
3239.064118	386677.304043	52.627751
3238.395160	386354.701320	52.632756
3237.649587	386019.240061	52.637761
3237.000461	385703.087852	52.642765
3236.015054	385372.490507	52.647770
3235.832354	385034.642508	52.652775
3234.901596	384716.873438	52.657780
3234.079119	384379.095288	52.662785
3233.777624	384048.276302	52.667789
3232.838206	383730.449383	52.672794
3232.684656	383394.998056	52.677799
3231.714902	383071.575293	52.682804
3231.193337	382740.220161	52.687809
3230.551084	382401.149625	52.692813
3229.464393	382078.194719	52.697818
3228.998135	381748.602563	52.702823
3228.164109	381412.681927	52.707828
3227.800800	381086.247017	52.712833
3227.086371	380759.712297	52.717837
3226.131625	380430.618555	52.722842
3225.606595	380110.228939	52.727847
3224.750973	379785.692275	52.732852
3224.302818	379454.500828	52.737857
3223.822633	379125.931473	52.742861
3222.693354	378805.982895	52.747866
3222.051617	378483.207564	52.752871
3221.383878	378156.440314	52.757876
3221.221332	377820.840500	52.762881
3220.362269	377492.775412	52.767885
3219.689543	377171.698590	52.772890
3219.251362	376840.534661	52.777895
3218.467057	376515.578468	52.782900
3217.718223	376189.087835	52.787905
3217.222791	375841.543382	52.792909
3216.417531	375521.949795	52.797914
3216.116238	375190.318316	52.802919
3215.145949	374856.017275	52.807924
3214.597303	374524.979189	52.812929
3214.163687	374193.233419	52.817933
3212.934347	373863.442446	52.822938
3212.204450	373537.258438	52.827943
3211.505967	373198.703650	52.832948
3210.883936	372882.672988	52.837953
3210.532273	372553.190717	52.842957
3209.746176	372221.001707	52.847962
3209.190453	371883.762038	52.852967
3208.229180	371570.497258	52.857972
3208.011514	371236.099103	52.862977
3207.418371	370898.348749	52.867981
3206.598678	370569.942758	52.872986
3205.618105	370237.540101	52.877991
3205.015741	369916.930447	52.882996
3204.007782	369581.397863	52.888001
3203.822862	369247.716888	52.893005
3203.024023	368931.150751	52.898010
3202.661848	368598.790374	52.903015
3201.940845	368266.178952	52.908020
3201.395464	367932.214257	52.913025
3200.594037	367612.687784	52.918029
3199.895691	367283.500076	52.923034
3199.441448	366937.860914	52.928039
3198.886670	366613.759494	52.933044
3197.974658	366284.496468	52.938049
3197.613077	365938.071665	52.943053
3196.595757	365611.186594	52.948058
3196.017839	365272.500231	52.953063
3194.895138	364943.082688	52.958068
3194.434993	364603.914748	52.963073
3193.925839	364274.242663	52.968077
3193.200511	363961.497344	52.973082
3192.326461	363615.670360	52.978087
3191.677550	363280.848107	52.983092
3190.786181	362957.511928	52.988097
3190.674055	362638.732083	52.993101
3189.696600	362311.919122	52.998106
3189.058976	361971.971279	53.003111
3188.288379	361652.423809	53.008116
3187.404248	361321.314413	53.013121
3187.023648	360988.698088	53.018125
3186.426193	360672.170146	53.023130
3186.053686	360352.449214	53.028135
3185.409845	360016.305355	53.033140
3184.386742	359691.466500	53.038145
3183.906455	359355.877458	53.043149
3183.132024	359026.490772	53.048154
3182.164633	358702.781628	53.053159
3181.492140	358379.914344	53.058164
3180.806716	358051.499486	53.063169
3180.413068	357727.387804	53.068173
3179.548101	357409.481463	53.073178
3178.992261	357080.276267	53.078183
3178.226195	356753.367043	53.083188
3177.996509	356426.040005	53.088193
3177.177203	356099.338554	53.093197
3176.392717	355780.874790	53.098202
3175.595360	355442.942890	53.103207
3175.076982	355120.513821	53.108212
3174.329680	354797.915360	53.113217
3174.021439	354460.128653	53.118221
3173.182536	354134.257616	53.123226
3172.430258	353805.393251	53.128231
3171.831345	353478.029528	53.133236
3171.066666	353149.112108	53.138241
3170.298825	352818.080797	53.143245
3169.862782	352502.341298	53.148250
3169.235188	352169.425898	53.153255
3168.439918	351848.547524	53.158260
3167.688898	351522.239271	53.163265
3167.163097	351189.759795	53.168269
3166.233788	350873.350688	53.173274
3165.731407	350544.375763	53.178279
3165.292527	350207.829824	53.183284
3164.577335	349886.367246	53.188289
3164.244354	349574.819273	53.193293
3163.568949	349231.432909	53.198298
3162.473660	348896.891709	53.203303
3161.844103	348573.320927	53.208308
3161.262559	348242.385045	53.213313
3161.058527	347909.605834	53.218317
3159.735805	347582.779354	53.223322
3159.467023	347239.367384	53.228327
3158.777555	346912.945912	53.233332
3157.954826	346588.554437	53.238337
3157.394041	346251.978651	53.243341
3156.721135	345919.974748	53.248346
3156.118414	345580.321884	53.253351
3155.262076	345257.862736	53.258356
3154.554284	344920.284394	53.263361
3154.171983	344583.594404	53.268365
3153.160853	344264.386935	53.273370
3152.507596	343929.059710	53.278375
3151.947190	343608.937441	53.283380
3151.263427	343271.447775	53.288385
3150.685633	342939.972137	53.293389
3149.680371	342628.900452	53.298394
3149.286309	342285.555854	53.303399
3148.618582	341960.885513	53.308404
3147.627521	341645.301106	53.313409
3147.067210	341306.228327	53.318413
3146.195661	340994.999968	53.323418
3145.755029	340665.679546	53.328423
3145.081122	340331.557787	53.333428
3144.621637	339997.502155	53.338433
3144.228453	339671.096434	53.343437
3143.044483	339354.360103	53.348442
3142.668639	339011.121993	53.353447
3141.751527	338687.288860	53.358452
3141.128342	338370.637157	53.363457
3140.692374	338031.781846	53.368461
3140.189800	337705.230786	53.373466
3139.076114	337383.891581	53.378471
3138.553713	337056.602215	53.383476
3137.597628	336727.776088	53.388481
3137.060742	336399.823919	53.393485
3136.163541	336081.728139	53.398490
3135.792530	335755.732246	53.403495
3135.297226	335439.580978	53.408500
3134.473466	335113.933694	53.413505
3134.075281	334790.788737	53.418509
3133.627290	334449.473383	53.423514
3132.747154	334119.400707	53.428519
3132.375714	333784.027107	53.433524
3131.357118	333463.290849	53.438529
3130.865578	333127.653098	53.443533
3129.822529	332800.629555	53.448538
3129.219088	332478.703003	53.453543
3128.298370	332156.137841	53.458548
3127.565279	331822.034263	53.463553
3127.048998	331488.098514	53.468557
3126.348070	331176.288729	53.473562
3125.811197	330849.685481	53.478567
3124.927386	330532.835594	53.483572
3124.521449	330202.033498	53.488577
3123.923083	329869.961973	53.493581
3123.197765	329559.956901	53.498586
3122.277143	329224.140092	53.503591
3122.097568	328904.167707	53.508596
3121.027913	328573.616308	53.513601
3120.415401	328256.102958	53.518605
3119.750869	327934.472039	53.523610
3119.390434	327600.749086	53.528615
3118.670364	327287.246052	53.533620
3118.070269	326961.629186	53.538625
3117.130884	326636.726653	53.543629
3116.322948	326314.373507	53.548634
3116.119191	325983.317803	53.553639
3115.218434	325658.354304	53.558644
3114.308691	325335.707863	53.563649
3113.622522	325011.115216	53.568653
3113.253246	324685.809166	53.573658
3113.085665	324353.366302	53.578663
3112.111463	324034.798786	53.583668
3111.080069	323710.535807	53.588673
3110.941836	323355.627572	53.593677
3109.914301	323045.645270	53.598682
3109.186711	322721.661475	53.603687
3108.821634	322376.205881	53.608692
3108.080531	322066.429378	53.613697
3107.611183	321732.572837	53.618701
3106.931354	321405.368446	53.623706
3106.248155	321069.455390	53.628711
3105.456580	320753.876982	53.633716
3104.370569	320424.518112	53.638721
3104.215413	320087.117438	53.643725
3103.057609	319767.290462	53.648730
3102.469914	319428.708184	53.653735
3102.093503	319106.132646	53.658740
3101.206980	318787.456127	53.663745
3100.423901	318452.160480	53.668749
3099.745263	318130.775282	53.673754
3099.166729	317814.160194	53.678759
3098.596605	317490.464038	53.683764
3097.584501	317171.751129	53.688769
3097.744355	316849.643362	53.693773
3096.360134	316524.315921	53.698778
3095.520864	316195.692803	53.703783
3095.204653	315873.682708	53.708788
3094.630700	315558.969470	53.713793
3093.982725	315227.002705	53.718797
3092.976616	314904.309385	53.723802
3092.591433	314586.303974	53.728807
3092.166438	314257.634581	53.733812
3091.169528	313932.339521	53.738817
3090.663516	313613.357229	53.743821
3089.532628	313289.431016	53.748826
3089.045303	312968.534069	53.753831
3088.896111	312641.649523	53.758836
3088.092602	312314.230961	53.763841
3087.363990	311992.070699	53.768845
3086.699364	311669.084529	53.773850
3086.346731	311343.272442	53.778855
3085.383958	311023.514691	53.783860
3084.536481	310690.521689	53.788865
3084.180772	310366.871835	53.793869
3083.564053	310038.551427	53.798874
3082.615817	309708.118076	53.803879
3082.173435	309383.893581	53.808884
3081.714414	309056.615062	53.813889
3081.175683	308732.022113	53.818893
3080.417131	308396.895098	53.823898
3079.769185	308066.307942	53.828903
3079.015880	307730.159717	53.833908
3078.066715	307394.296260	53.838913
3077.891638	307064.599354	53.843917
3077.110404	306743.783117	53.848922
3076.443021	306401.226038	53.853927
3075.666888	306080.865768	53.858932
3075.252292	305744.124074	53.863937
3074.553047	305402.129743	53.868941
3073.882358	305087.225566	53.873946
3073.207900	304730.302748	53.878951
3072.519889	304400.833346	53.883956
3071.502126	304070.396739	53.888961
3071.030539	303741.528218	53.893965
3070.422776	303395.389088	53.898970
3069.576394	303077.910777	53.903975
3068.925312	302748.431806	53.908980
3068.270460	302407.085474	53.913985
3067.831714	302076.221735	53.918989
3066.927089	301749.047241	53.923994
3066.280958	301428.426935	53.928999
3066.064917	301097.424024	53.934004
3065.119590	300758.462998	53.939009
3064.317678	300423.298545	53.944013
3063.034231	300101.757834	53.949018
3062.787957	299776.385157	53.954023
3062.090500	299445.022209	53.959028
3061.344614	299121.102564	53.964033
3060.592450	298785.977949	53.969037
3059.748535	298464.899422	53.974042
3059.406056	298138.978660	53.979047
3059.160035	297817.014882	53.984052
3057.934628	297495.562097	53.989057
3057.656477	297158.856923	53.994061
3057.054039	296833.688104	53.999066
3056.134430	296507.397458	54.004071
3055.822274	296175.127226	54.009076
3054.755405	295835.845100	54.014081
3054.170942	295511.104214	54.019085
3053.271857	295199.604634	54.024090
3052.831419	294872.064031	54.029095
3052.203222	294552.065496	54.034100
3051.343612	294224.743061	54.039105
3050.870612	293901.968542	54.044109
3050.526257	293572.679012	54.049114
3049.460733	293236.474143	54.054119
3049.020800	292914.482493	54.059124
3048.373814	292587.200472	54.064129
3047.877602	292255.666533	54.069133
3046.911806	291930.420566	54.074138
3046.184558	291602.946209	54.079143
3045.733569	291268.220366	54.084148
3044.919871	290938.619576	54.089153
3044.454886	290608.784914	54.094157
3043.850938	290280.398045	54.099162
3042.801514	289960.103652	54.104167
3042.274652	289621.058297	54.109172
3041.507183	289298.069896	54.114177
3041.071873	288963.491639	54.119181
3040.336164	288655.192480	54.124186
3039.817938	288320.040900	54.129191
3039.237655	287994.780352	54.134196
3037.995823	287663.435491	54.139201
3037.837523	287326.112103	54.144205
3037.117908	287006.653904	54.149210
3036.219740	286664.506214	54.154215
3035.805955	286340.058234	54.159220
3034.920034	286012.654016	54.164225
3034.548803	285682.137358	54.169229
3033.536821	285358.012480	54.174234
3033.012725	285015.498548	54.179239
3032.426209	284684.684108	54.184244
3031.606493	284356.223945	54.189249
3030.735464	284018.246580	54.194253
3030.052217	283698.398083	54.199258
3029.723417	283375.207883	54.204263
3029.039213	283044.891706	54.209268
3028.068377	282721.930091	54.214273
3027.856574	282382.217380	54.219277
3027.130764	282067.875835	54.224282
3026.469221	281745.323179	54.229287
3026.018527	281402.795323	54.234292
3025.335744	281071.000730	54.239297
3024.482557	280737.475654	54.244301
3023.955462	280405.248647	54.249306
3023.236393	280080.743339	54.254311
3022.693183	279747.830997	54.259316
3022.126295	279414.387461	54.264321
3021.236182	279072.819648	54.269325
3020.433457	278741.374316	54.274330
3019.888868	278416.229666	54.279335
3019.411263	278084.401630	54.284340
3018.443760	277763.449674	54.289345
3017.738133	277422.412596	54.294349
3016.917551	277096.725636	54.299354
3016.233963	276775.677671	54.304359
3015.776340	276438.090394	54.309364
3014.924361	276123.588950	54.314369
3014.625401	275781.035661	54.319373
3014.138175	275448.139226	54.324378
3013.398132	275113.474564	54.329383
3012.825539	274785.634409	54.334388
3011.983361	274446.911018	54.339393
3011.487346	274109.151601	54.344397
3010.578075	273782.332647	54.349402
3009.999024	273452.379798	54.354407
3009.297072	273124.713150	54.359412
3008.437577	272790.933635	54.364417
3007.971309	272457.728662	54.369421
3007.104545	272129.961000	54.374426
3006.589723	271795.006584	54.379431
3006.238597	271466.266105	54.384436
3005.438879	271139.888902	54.389441
3004.819705	270788.549759	54.394445
3004.368395	270462.219535	54.399450
3003.669279	270132.210307	54.404455
3003.284977	269781.573022	54.409460
3002.155992	269468.899649	54.414465
3001.420746	269107.035833	54.419469
3000.401102	268786.908760	54.424474
2999.919463	268452.587295	54.429479
2999.399844	268118.068297	54.434484
2998.551132	267793.203114	54.439489
2998.042522	267450.176423	54.444493
2997.111111	267125.095551	54.449498
2996.614029	266797.883226	54.454503
2996.029648	266461.720176	54.459508
2995.419851	266137.709693	54.464513
2994.576328	265789.974735	54.469517
2994.152747	265471.309055	54.474522
2993.260551	265132.063234	54.479527
2993.128857	264796.084565	54.484532
2992.225260	264459.693571	54.489537
2991.714586	264134.293784	54.494541
2991.038256	263795.651724	54.499546
2990.061865	263457.235778	54.504551
2989.647375	263115.420395	54.509556
2988.753536	262788.147009	54.514561
2988.075482	262448.386028	54.519565
2987.122897	262112.234377	54.524570
2986.468078	261789.381083	54.529575
2985.976685	261456.162364	54.534580
2985.496792	261126.864242	54.539585
2984.939941	260782.374479	54.544589
2984.364017	260452.353802	54.549594
2983.784837	260116.603831	54.554599
2983.182819	259772.784679	54.559604
2982.305536	259451.904907	54.564609
2981.608904	259098.322106	54.569613
2981.137655	258756.597451	54.574618
2980.030436	258433.310534	54.579623
2979.660525	258082.402520	54.584628
2978.722427	257749.539494	54.589633
2978.351274	257425.628107	54.594637
2977.627191	257074.777721	54.599642
2976.755811	256741.268956	54.604647
2976.448455	256409.199449	54.609652
2975.681712	256071.549477	54.614657
2975.158023	255738.420193	54.619661
2974.234472	255406.806383	54.624666
2973.721219	255067.920985	54.629671
2972.955374	254727.064264	54.634676
2972.468636	254391.944955	54.639681
2971.732187	254055.516021	54.644685
2971.289050	253720.238193	54.649690
2970.507698	253379.691950	54.654695
2969.992491	253041.294349	54.659700
2969.002259	252707.251003	54.664705
2968.703919	252357.182065	54.669709
2968.039959	252013.258240	54.674714
2967.232214	251673.839985	54.679719
2966.216625	251339.981554	54.684724
2965.176654	250997.901975	54.689729
2965.161446	250663.147993	54.694733
2964.186262	250332.111977	54.699738
2963.523073	249993.973075	54.704743
2963.288217	249651.921672	54.709748
2962.133379	249318.904380	54.714753
2961.847477	248975.767497	54.719757
2961.165468	248642.956939	54.724762
2960.603864	248307.810641	54.729767
2959.879134	247970.093394	54.734772
2958.972425	247632.023746	54.739777
2958.701042	247280.713908	54.744781
2957.787031	246955.609126	54.749786
2957.087649	246609.640126	54.754791
2956.592814	246273.138294	54.759796
2955.793071	245945.598522	54.764801
2955.319525	245590.657876	54.769805
2954.632576	245259.765906	54.774810
2953.836118	244924.766692	54.779815
2953.187947	244579.686027	54.784820
2952.786758	244238.743475	54.789825
2951.972635	243890.380421	54.794829
2951.261226	243550.787531	54.799834
2950.471989	243213.677987	54.804839
2950.131157	242869.775585	54.809844
2949.337780	242528.288562	54.814849
2948.773707	242180.068917	54.819853
2947.972307	241836.955342	54.824858
2947.196010	241497.225579	54.829863
2946.430309	241148.353292	54.834868
2945.722916	240827.840357	54.839873
2945.474370	240477.156588	54.844877
2944.977000	240143.981883	54.849882
2944.084158	239804.581063	54.854887
2943.284906	239460.786580	54.859892
2942.815732	239118.163167	54.864897
2942.075170	238770.159916	54.869901
2941.299904	238431.457635	54.874906
2940.644896	238081.202181	54.879911
2939.951795	237744.755318	54.884916
2939.069451	237412.108117	54.889921
2938.808333	237063.576078	54.894925
2937.802820	236726.850867	54.899930
2937.025588	236391.185528	54.904935
2936.800672	236049.297124	54.909940
2936.090266	235708.377944	54.914945
2935.029740	235357.813819	54.919949
2934.355244	235023.358933	54.924954
2933.894442	234688.209285	54.929959
2933.281057	234355.274748	54.934964
2931.964566	234011.172568	54.939969
2931.855653	233679.866460	54.944973
2931.059331	233343.093974	54.949978
2930.214830	233010.327938	54.954983
2929.899383	232672.030292	54.959988
2928.996778	232345.768745	54.964993
2928.336018	232008.139253	54.969997
2928.086961	231664.614916	54.975002
2927.201368	231334.560321	54.980007
2926.777888	230993.739634	54.985012
2925.708023	230658.114980	54.990017
2925.267039	230328.146396	54.995021
2924.919236	229991.238639	55.000026
2923.816412	229649.130195	55.005031
2923.401010	229301.745504	55.010036
2922.785469	228964.043811	55.015041
2922.070361	228633.564788	55.020045
2921.156039	228296.320380	55.025050
2920.365278	227955.034848	55.030055
2920.149120	227613.150470	55.035060
2919.226823	227278.610225	55.040065
2918.653230	226935.104755	55.045069
2917.938195	226598.293837	55.050074
2917.303167	226257.563389	55.055079
2916.909111	225919.291335	55.060084
2916.138444	225578.356032	55.065089
2915.526324	225237.435242	55.070093
2914.755096	224909.283983	55.075098
2914.118812	224559.204167	55.080103
2913.569326	224212.472877	55.085108
2912.525654	223876.909191	55.090113
2912.019682	223528.239054	55.095117
2911.656998	223195.791124	55.100122
2910.655499	222865.355247	55.105127
2910.042712	222515.471772	55.110132
2909.623910	222178.378008	55.115137
2909.048607	221835.060248	55.120141
2908.198285	221498.890716	55.125146
2907.294254	221151.287321	55.130151
2907.021124	220811.134228	55.135156
2905.930049	220476.636789	55.140161
2905.741573	220139.935778	55.145165
2905.157087	219793.013728	55.150170
2904.310687	219444.059932	55.155175
2903.554903	219102.069066	55.160180
2902.643044	218760.753723	55.165185
2902.061396	218415.836304	55.170189
2901.456694	218070.109549	55.175194
2900.859138	217741.783829	55.180199
2900.170326	217391.809515	55.185204
2899.649753	217060.368942	55.190209
2898.682286	216711.180440	55.195213
2898.400959	216365.945503	55.200218
2897.795947	216033.899513	55.205223
2896.989763	215681.190324	55.210228
2896.296779	215333.823742	55.215233
2895.716668	214990.412346	55.220237
2894.852671	214650.700706	55.225242
2894.245557	214308.709929	55.230247
2893.897884	213958.050074	55.235252
2893.069952	213628.940577	55.240257
2892.376880	213280.502815	55.245261
2891.783588	212935.156753	55.250266
2890.788359	212586.146876	55.255271
2890.419988	212238.656062	55.260276
2889.623294	211897.382502	55.265281
2888.912718	211554.187960	55.270285
2888.118927	211222.959767	55.275290
2887.355114	210878.300897	55.280295
2886.997993	210536.366850	55.285300
2886.384887	210202.289894	55.290305
2885.898004	209836.248886	55.295309
2885.310834	209494.242443	55.300314
2884.288118	209154.381419	55.305319
2883.671297	208804.645318	55.310324
2883.061210	208466.033679	55.315329
2882.506728	208119.677064	55.320333
2881.630319	207784.547723	55.325338
2880.952575	207431.214737	55.330343
2880.737828	207083.041255	55.335348
2879.707707	206748.209332	55.340353
2878.995901	206399.482239	55.345357
2878.341384	206062.405733	55.350362
2877.520416	205717.950670	55.355367
2877.516579	205371.268368	55.360372
2876.307555	205029.793200	55.365377
2875.752788	204681.433307	55.370381
2875.488162	204345.539485	55.375386
2874.251672	204000.575067	55.380391
2874.086867	203643.862274	55.385396
2873.139643	203310.195196	55.390401
2872.126196	202963.394682	55.395405
2871.840140	202614.852207	55.400410
2871.252100	202273.066221	55.405415
2870.305773	201928.679406	55.410420
2870.007982	201594.168922	55.415425
2869.165053	201246.117738	55.420429
2868.573957	200900.841212	55.425434
2867.715206	200560.483083	55.430439
2867.478959	200201.080521	55.435444
2866.749562	199865.999999	55.440449
2865.953634	199513.867682	55.445453
2865.322536	199169.677464	55.450458
2864.423768	198821.663468	55.455463
2863.827404	198476.899610	55.460468
2863.146232	198128.982955	55.465473
2862.703281	197776.857166	55.470477
2862.172805	197436.352478	55.475482
2860.865690	197090.832292	55.480487
2860.557433	196739.646520	55.485492
2859.650813	196400.467925	55.490497
2859.180345	196053.078939	55.495501
2858.392868	195711.442963	55.500506
2857.378138	195369.972510	55.505511
2856.839921	195034.981771	55.510516
2856.240835	194701.949657	55.515521
2855.904780	194362.198052	55.520525
2855.234890	194019.855072	55.525530
2854.230929	193675.913267	55.530535
2854.079518	193328.479784	55.535540
2853.260860	192987.770647	55.540545
2852.746558	192645.425233	55.545549
2851.838557	192301.566863	55.550554
2851.025040	191956.232773	55.555559
2850.639373	191602.677821	55.560564
2850.088670	191267.243797	55.565569
2849.204210	190926.623091	55.570573
2848.590039	190572.653841	55.575578
2847.790275	190234.111191	55.580583
2847.382267	189889.987240	55.585588
2846.612085	189549.892599	55.590593
2846.123537	189204.323278	55.595597
2845.434504	188862.897588	55.600602
2844.683684	188512.298637	55.605607
2844.311927	188165.929675	55.610612
2843.485484	187820.233243	55.615617
2843.075517	187467.832512	55.620621
2842.495020	187112.433651	55.625626
2841.408030	186767.269797	55.630631
2840.854000	186413.157063	55.635636
2840.334866	186067.603228	55.640641
2839.287100	185715.698632	55.645645
2838.956881	185380.399133	55.650650
2838.135274	185035.600757	55.655655
2837.440691	184671.346798	55.660660
2836.586404	184345.373666	55.665665
2836.261086	183990.760306	55.670669
2835.760533	183644.051814	55.675674
2834.593914	183304.333528	55.680679
2834.100453	182943.763648	55.685684
2833.178643	182605.449428	55.690689
2832.607538	182252.224642	55.695693
2832.108514	181910.757737	55.700698
2831.160336	181567.927253	55.705703
2830.837035	181216.566970	55.710708
2830.152881	180881.103316	55.715713
2829.319726	180533.874372	55.720717
2828.854151	180181.870917	55.725722
2828.121240	179840.711870	55.730727
2827.377315	179492.434240	55.735732
2826.816069	179150.032459	55.740737
2826.120357	178792.022426	55.745741
2825.618840	178452.516910	55.750746
2824.653715	178104.133158	55.755751
2824.277031	177757.249015	55.760756
2823.431471	177416.992380	55.765761
2822.638581	177067.763284	55.770765
2822.271412	176722.145476	55.775770
2821.453523	176368.194826	55.780775
2821.182313	176021.333987	55.785780
2820.197567	175676.433305	55.790785
2819.689505	175325.596819	55.795789
2819.067814	174973.967387	55.800794
2818.649765	174630.270388	55.805799
2817.861428	174276.091620	55.810804
2816.863031	173930.622952	55.815809
2816.156538	173567.140596	55.820813
2815.507291	173214.691545	55.825818
2814.723153	172881.140057	55.830823
2814.325292	172530.704812	55.835828
2813.707909	172186.399121	55.840833
2812.909152	171829.903779	55.845837
2812.362712	171425.122487	55.850842
2811.907196	171077.468977	55.855847
2811.364274	170719.379036	55.860852
2810.346625	170376.246356	55.865857
2809.921818	170013.413546	55.870861
2809.869076	169662.720490	55.875866
2808.868745	169310.921792	55.880871
2807.986099	168955.025714	55.885876
2807.293176	168598.047452	55.890881
2806.996692	168243.209644	55.895885
2806.236994	167878.390122	55.900890
2805.159626	167546.876640	55.905895
2804.943872	167168.740520	55.910900
2803.965602	166808.035055	55.915905
2802.756800	166483.341974	55.920909
2802.889851	166096.794579	55.925914
2802.078169	165760.041513	55.930919
2801.211430	165388.295227	55.935924
2800.396495	165054.613468	55.940929
2799.921943	164692.055959	55.945933
2799.094660	164342.641488	55.950938
2798.332751	163986.290472	55.955943
2797.880184	163614.877994	55.960948
2797.123878	163298.927125	55.965953
2796.435799	162927.228416	55.970957
2795.734336	162575.191854	55.975962
2794.922546	162256.245625	55.980967
2794.339542	161880.752269	55.985972
2793.653791	161536.262805	55.990977
2792.961752	161186.272616	55.995981
2792.580319	160840.584726	56.000986
2791.623878	160495.881237	56.005991
2790.944294	160138.322181	56.010996
2790.204924	159804.321143	56.016001
2789.397283	159439.695485	56.021005
2788.756979	159084.047906	56.026010
2788.273179	158759.423959	56.031015
2787.701127	158414.400355	56.036020
2787.353607	158071.251505	56.041025
2786.598313	157712.559722	56.046029
2785.814332	157359.126413	56.051034
2784.772158	157021.640626	56.056039
2784.256374	156667.205823	56.061044
2783.663747	156335.859084	56.066049
2782.833718	155983.324395	56.071053
2782.033622	155636.191096	56.076058
2781.332775	155291.549811	56.081063
2780.687692	154952.636071	56.086068
2779.967649	154607.026034	56.091073
2779.110833	154274.457480	56.096077
2778.896989	153939.324424	56.101082
2777.930691	153599.127863	56.106087
2777.792601	153246.321563	56.111092
2776.900490	152904.620475	56.116097
2776.135322	152564.161144	56.121101
2775.658242	152225.718771	56.126106
2774.807569	151888.292326	56.131111
2774.229783	151535.192636	56.136116
2773.729510	151198.709164	56.141121
2772.763840	150852.007879	56.146125
2772.248490	150508.314704	56.151130
2771.018472	150196.969966	56.156135
2770.826328	149831.512017	56.161140
2770.325043	149490.331175	56.166145
2769.219303	149150.457075	56.171149
2768.951870	148818.905303	56.176154
2768.307901	148479.079540	56.181159
2767.659075	148132.840209	56.186164
2766.919491	147792.579382	56.191169
2766.361403	147444.172689	56.196173
2765.829174	147092.296336	56.201178
2764.813268	146751.061078	56.206183
2764.343371	146413.746071	56.211188
2763.670175	146066.897778	56.216193
2762.986416	145734.808795	56.221197
2762.353327	145391.723143	56.226202
2761.744414	145055.232658	56.231207
2760.732576	144699.761212	56.236212
2760.323780	144380.769863	56.241217
2759.578745	144036.967166	56.246221
2759.146428	143683.474136	56.251226
2758.310216	143352.565708	56.256231
2758.010709	143007.052029	56.261236
2757.512764	142654.051386	56.266241
2756.328614	142311.709870	56.271245
2756.101036	141958.064534	56.276250
2755.393230	141614.905719	56.281255
2754.629602	141259.256930	56.286260
2754.023031	140923.065509	56.291265
2753.452126	140584.826564	56.296269
2752.867016	140223.647424	56.301274
2751.830133	139882.478990	56.306279
2751.299713	139531.146228	56.311284
2750.854609	139176.437227	56.316289
2749.941140	138832.440708	56.321293
2749.431519	138489.070253	56.326298
2748.772890	138134.115316	56.331303
2748.256259	137783.842816	56.336308
2747.171333	137432.254328	56.341313
2746.131390	137095.819050	56.346317
2745.780995	136741.073457	56.351322
2745.193674	136404.625228	56.356327
2744.507474	136063.940779	56.361332
2743.857163	135714.603466	56.366337
2743.014325	135370.788756	56.371341
2742.329717	135033.355533	56.376346
2741.822120	134688.873353	56.381351
2741.152254	134342.896637	56.386356
2740.381976	134002.529253	56.391361
2739.613464	133662.000494	56.396365
2739.044333	133323.108236	56.401370
2738.490802	132990.644951	56.406375
2737.832751	132646.846283	56.411380
2737.299234	132304.111725	56.416385
2736.375044	131964.047108	56.421389
2735.944726	131615.880800	56.426394
2735.187282	131274.299261	56.431399
2734.358260	130920.323858	56.436404
2733.956390	130603.589060	56.441409
2733.129728	130243.550588	56.446413
2732.916122	129894.558421	56.451418
2732.047702	129555.225417	56.456423
2731.429499	129207.487147	56.461428
2730.626676	128871.479693	56.466433
2730.017893	128515.747269	56.471437
2729.448005	128174.351824	56.476442
2728.297403	127844.342987	56.481447
2728.157921	127493.273846	56.486452
2727.586840	127137.426276	56.491457
2726.447910	126801.040182	56.496461
2725.941942	126449.242435	56.501466
2725.252522	126122.445070	56.506471
2724.553617	125771.207337	56.511476
2724.063195	125418.417253	56.516481
2723.193026	125092.511782	56.521485
2723.089805	124732.862755	56.526490
2721.930883	124391.163643	56.531495
2721.732270	124044.567568	56.536500
2720.771895	123696.966537	56.541505
2720.070889	123359.614294	56.546509
2719.522337	123008.541228	56.551514
2718.709398	122669.247308	56.556519
2718.308346	122326.362568	56.561524
2717.537378	121982.347330	56.566529
2716.709104	121630.003628	56.571533
2715.998270	121280.045759	56.576538
2715.129018	120938.472150	56.581543
2714.555728	120581.734395	56.586548
2713.724210	120260.643332	56.591553
2713.274993	119926.291467	56.596557
2713.332172	119560.942183	56.601562
2712.006530	119226.617557	56.606567
2711.415052	118879.942156	56.611572
2711.065490	118531.728634	56.616577
2710.093072	118185.021345	56.621581
2709.582007	117839.235855	56.626586
2708.793631	117499.180025	56.631591
2708.351152	117149.032184	56.636596
2707.571667	116812.424392	56.641601
2706.792141	116467.125230	56.646605
2706.597195	116107.552083	56.651610
2705.265323	115780.306045	56.656615
2704.629204	115431.856387	56.661620
2703.978323	115081.992145	56.666625
2703.400846	114738.607622	56.671629
2702.522213	114388.903321	56.676634
2701.778981	114059.422060	56.681639
2701.272067	113713.692069	56.686644
2700.692381	113374.312217	56.691649
2699.944422	113042.001845	56.696653
2699.480169	112700.512189	56.701658
2698.407544	112356.838957	56.706663
2697.976999	112011.241043	56.711668
2697.399398	111665.607789	56.716673
2696.956044	111339.427647	56.721677
2696.423806	110982.665859	56.726682
2695.289097	110659.250514	56.731687
2694.775169	110293.541847	56.736692
2694.117796	109947.374234	56.741697
2693.231509	109625.684561	56.746701
2692.713755	109277.061274	56.751706
2691.986586	108939.022193	56.756711
2691.719537	108592.386819	56.761716
2690.987470	108253.019201	56.766721
2690.431050	107911.052389	56.771725
2689.862749	107562.055660	56.776730
2688.993586	107222.622717	56.781735
2688.466772	106879.009818	56.786740
2687.687698	106532.041017	56.791745
2686.750686	106190.285859	56.796749
2686.250751	105834.762048	56.801754
2685.541660	105489.446875	56.806759
2684.929152	105144.267325	56.811764
2684.096473	104797.199009	56.816769
2683.199258	104471.564037	56.821773
2682.924050	104129.213392	56.826778
2682.096776	103795.265860	56.831783
2681.822051	103438.422716	56.836788
2680.955563	103097.563720	56.841793
2680.001786	102763.168752	56.846797
2679.540059	102421.798688	56.851802
2678.789756	102075.797784	56.856807
2678.259783	101732.069776	56.861812
2677.606389	101390.091794	56.866817
2676.800576	101054.372100	56.871821
2676.333994	100702.238079	56.876826
2675.267193	100362.675046	56.881831
2674.744426	100033.725096	56.886836
2674.302444	99684.393607	56.891841
2673.392630	99352.964861	56.896845
2672.926087	99015.825629	56.901850
2672.228867	98654.575188	56.906855
2671.487004	98309.028930	56.911860
2671.142606	97985.230206	56.916865
2670.105948	97655.786930	56.921869
2669.794300	97286.131502	56.926874
2668.754232	96967.512271	56.931879
2668.282168	96625.639964	56.936884
2667.610521	96273.264113	56.941889
2666.675257	95944.203832	56.946893
2666.284473	95589.967693	56.951898
2665.908559	95265.147444	56.956903
2665.001000	94911.035610	56.961908
2664.227966	94577.771517	56.966913
2663.354429	94247.229750	56.971917
2663.149620	93895.977716	56.976922
2662.208939	93557.048279	56.981927
2661.247519	93210.758949	56.986932
2660.825553	92875.029724	56.991937
2660.154707	92543.434909	56.996941
2659.509480	92198.062443	57.001946
2658.804864	91864.460460	57.006951
2658.093667	91525.196070	57.011956
2657.565417	91183.454148	57.016961
2656.432783	90856.992273	57.021965
2656.267406	90519.248385	57.026970
2655.456000	90183.545859	57.031975
2654.685904	89844.082260	57.036980
2654.305486	89505.532223	57.041985
2653.466543	89168.404186	57.046989
2652.781175	88839.505164	57.051994
2652.029202	88503.280285	57.056999
2651.342253	88170.537128	57.062004
2650.877806	87842.321965	57.067009
2649.680358	87509.067665	57.072013
2649.408766	87165.852173	57.077018
2648.645434	86835.620442	57.082023
2647.711364	86504.425615	57.087028
2647.303767	86171.447283	57.092033
2646.617902	85847.132867	57.097037
2645.922063	85516.663608	57.102042
2645.142166	85189.052564	57.107047
2644.465806	84860.999139	57.112052
2644.034039	84522.123815	57.117057
2643.094151	84202.945609	57.122061
2642.608861	83870.098072	57.127066
2642.057960	83537.183790	57.132071
2641.235814	83215.453897	57.137076
2641.011319	82876.641886	57.142081
2640.211780	82551.331251	57.147085
2639.683483	82222.984878	57.152090
2638.601529	81892.018847	57.157095
2638.426675	81555.590680	57.162100
2637.793398	81200.506803	57.167105
2636.810981	80875.796307	57.172109
2636.125124	80544.091824	57.177114
2635.955711	80199.433531	57.182119
2634.799537	79865.247882	57.187124
2634.481605	79535.415083	57.192129
2633.749820	79203.885145	57.197133
2633.562623	78870.544285	57.202138
2632.058953	78533.647122	57.207143
2631.497648	78183.451323	57.212148
2631.237617	77847.242807	57.217153
2630.097052	77515.773272	57.222157
2629.432066	77186.312064	57.227162
2628.993195	76847.075267	57.232167
2628.075739	76507.913644	57.237172
2627.510346	76182.723450	57.242177
2626.775653	75846.306426	57.247181
2626.293918	75526.999553	57.252186
2625.517880	75191.309597	57.257191
2624.930301	74854.721056	57.262196
2624.158537	74515.702837	57.267201
2623.592973	74194.567748	57.272205
2622.771151	73865.103191	57.277210
2622.657190	73521.575510	57.282215
2621.802607	73198.601658	57.287220
2621.162189	72860.167152	57.292225
2620.101950	72524.782310	57.297229
2619.783082	72184.591589	57.302234
2618.772947	71865.268499	57.307239
2618.141103	71522.636556	57.312244
2617.263577	71184.445569	57.317249
2616.463264	70870.647895	57.322253
2616.027536	70539.904095	57.327258
2615.416779	70221.025694	57.332263
2614.821749	69892.085250	57.337268
2614.102384	69564.512810	57.342273
2613.247412	69242.876765	57.347277
2612.849271	68897.745323	57.352282
2612.060739	68576.166724	57.357287
2611.418232	68247.267800	57.362292
2610.771611	67925.861117	57.367297
2609.653638	67612.457362	57.372301
2609.168573	67280.218560	57.377306
2608.785154	66960.353611	57.382311
2607.913086	66634.675433	57.387316
2607.407420	66304.271047	57.392321
2606.455574	65986.279186	57.397325
2606.084568	65658.888403	57.402330
2605.353089	65339.773597	57.407335
2604.708866	65017.306758	57.412340
2604.497575	64686.234458	57.417345
2603.459664	64365.471566	57.422349
2602.853579	64041.533401	57.427354
2601.996306	63708.538341	57.432359
2601.572353	63391.981263	57.437364
2601.014148	63051.807954	57.442369
2600.246771	62743.370112	57.447373
2599.479791	62402.443756	57.452378
2598.878298	62084.100506	57.457383
2598.081604	61763.197719	57.462388
2597.689182	61437.677842	57.467393
2596.949678	61107.691866	57.472397
2596.034896	60778.739762	57.477402
2595.474828	60456.457431	57.482407
2594.728923	60131.820232	57.487412
2594.301395	59818.242186	57.492417
2593.602499	59488.686610	57.497421
2592.930638	59153.200947	57.502426
2592.410878	58841.173250	57.507431
2591.380046	58510.516483	57.512436
2591.018243	58188.064668	57.517441
2589.876936	57874.103950	57.522445
2589.211772	57539.146459	57.527450
2588.627447	57215.541010	57.532455
2587.649157	56907.274012	57.537460
2587.137680	56587.750673	57.542465
2586.204526	56266.774322	57.547469
2585.883008	55945.858535	57.552474
2585.131164	55645.978998	57.557479
2584.439339	55316.455540	57.562484
2583.945505	54998.371643	57.567489
2582.988799	54694.995923	57.572493
2582.314618	54373.783879	57.577498
2581.565260	54068.933257	57.582503
2581.049586	53750.200600	57.587508
2580.496629	53447.316450	57.592513
2579.573652	53136.038146	57.597517
2578.912266	52817.990464	57.602522
2578.738428	52505.360762	57.607527
2577.738570	52196.790787	57.612532
2577.140141	51882.799545	57.617537
2576.197438	51575.822623	57.622541
2575.749914	51260.185750	57.627546
2575.086317	50950.536618	57.632551
2574.210200	50644.624942	57.637556
2573.716053	50316.483645	57.642561
2572.969272	50033.476526	57.647565
2572.526872	49710.105767	57.652570
2571.880200	49407.364637	57.657575
2570.978375	49090.430316	57.662580
2570.711349	48783.979482	57.667585
2569.675160	48460.557901	57.672589
2568.930062	48146.914969	57.677594
2568.452121	47851.794022	57.682599
2567.908236	47539.670466	57.687604
2567.072083	47232.087250	57.692609
2565.849533	46928.489715	57.697613
2565.394826	46617.576650	57.702618
2564.778980	46325.732565	57.707623
2564.061894	46012.850654	57.712628
2563.696463	45709.862627	57.717633
2562.549642	45406.630496	57.722637
2562.078747	45112.145870	57.727642
2561.445059	44809.858003	57.732647
2560.654140	44505.101811	57.737652
2560.069469	44204.211409	57.742657
2559.491822	43897.063279	57.747661
2558.888208	43598.004835	57.752666
2558.332654	43303.659109	57.757671
2557.334345	43008.702335	57.762676
2556.972018	42694.185712	57.767681
2555.953593	42398.470939	57.772685
2555.563125	42105.972525	57.777690
2554.560324	41802.862768	57.782695
2554.241755	41510.217619	57.787700
2553.631295	41199.081502	57.792705
2552.400551	40900.656192	57.797709
2551.790156	40606.320978	57.802714
2551.258114	40319.559009	57.807719
2550.556098	40018.395067	57.812724
2549.961496	39723.906550	57.817729
2549.129450	39436.606236	57.822733
2548.707544	39126.154571	57.827738
2547.945573	38844.596299	57.832743
2547.186725	38550.190492	57.837748
2546.575958	38262.101961	57.842753
2545.657508	37973.860031	57.847757
2545.065850	37678.089783	57.852762
2544.194133	37394.701471	57.857767
2543.395151	37103.640283	57.862772
2543.160553	36809.489907	57.867777
2542.494770	36531.664606	57.872781
2541.717474	36250.276864	57.877786
2540.943234	35966.143226	57.882791
2540.396439	35674.957738	57.887796
2540.037947	35382.890841	57.892801
2538.938161	35105.085275	57.897805
2538.116743	34817.457369	57.902810
2537.710775	34527.330007	57.907815
2536.749896	34240.998471	57.912820
2536.533503	33962.433429	57.917825
2535.522058	33680.226876	57.922829
2534.755486	33388.305447	57.927834
2534.191821	33111.491158	57.932839
2533.618482	32842.464112	57.937844
2532.917510	32545.556747	57.942849
2532.000077	32276.602939	57.947853
2531.455550	32000.196102	57.952858
2530.951644	31725.377070	57.957863
2529.781480	31448.726300	57.962868
2529.387847	31166.851851	57.967873
2528.462195	30897.277205	57.972877
2527.931826	30625.078364	57.977882
2527.207491	30348.010479	57.982887
2526.443056	30076.080646	57.987892
2525.904199	29801.762296	57.992897
2524.965251	29542.382178	57.997901
2524.128885	29273.215117	58.002906
2523.678615	29004.695913	58.007911
2523.022173	28737.935850	58.012916
2522.524342	28474.613234	58.017921
2521.313018	28218.600789	58.022925
2520.701057	27960.720128	58.027930
2520.179820	27687.881683	58.032935
2519.344456	27434.134769	58.037940
2518.356003	27179.859266	58.042945
2517.386188	26931.106533	58.047949
2516.657074	26683.900696	58.052954
2516.219346	26432.062087	58.057959
2515.001592	26190.278029	58.062964
2514.385903	25955.605784	58.067969
2513.314935	25725.807019	58.072973
2512.511783	25483.958384	58.077978
2511.651813	25266.964006	58.082983
2510.674336	25038.663954	58.087988
2509.777633	24814.854227	58.092993
2508.963107	24613.404955	58.097997
2507.968428	24416.203042	58.103002
2506.803009	24228.370414	58.108007
2505.797760	24034.089684	58.113012
2504.884625	23859.608238	58.118017
2503.528417	23680.937877	58.123021
2502.830978	23498.996949	58.128026
2501.757379	23324.592613	58.133031
2500.828215	23171.947335	58.138036
2500.047126	23019.292683	58.143041
2498.859858	22876.554563	58.148045
2498.253844	22731.726242	58.153050
2497.675974	22588.626415	58.158055
2496.915906	22450.393926	58.163060
2496.074436	22313.031484	58.168065
2495.279937	22193.240034	58.173069
2494.823760	22057.615059	58.178074
2494.248880	21919.384697	58.183079
2493.099527	21802.393124	58.188084
2492.636709	21674.343769	58.193089
2491.727447	21540.392378	58.198093
2491.161768	21426.361937	58.203098
2490.455999	21317.144762	58.208103
2489.839859	21190.852768	58.213108
2489.084153	21074.206859	58.218113
2488.266949	20961.396083	58.223117
2487.750178	20842.644237	58.228122
2487.217920	20732.364587	58.233127
2486.279400	20627.810195	58.238132
2486.075051	20511.818452	58.243137
2485.518767	20401.715468	58.248141
2484.725487	20284.559513	58.253146
2484.113985	20175.653493	58.258151
2483.515584	20069.397662	58.263156
2482.894638	19937.322029	58.268161
2481.941074	19843.117522	58.273165
2481.222569	19727.039417	58.278170
2480.915142	19615.418285	58.283175
2480.153794	19514.280584	58.288180
2479.647069	19405.354625	58.293185
2479.242216	19297.653898	58.298189
2478.251548	19193.482870	58.303194
2477.743816	19074.225506	58.308199
2476.946794	18965.317461	58.313204
2476.805447	18862.610612	58.318209
2475.965382	18755.202095	58.323213
2475.399086	18634.726661	58.328218
2475.148926	18510.085239	58.333223
2473.990385	18407.914483	58.338228
2473.342075	18288.640026	58.343233
2472.381777	18185.382290	58.348237
2471.598015	18077.053825	58.353242
2471.218298	17975.670223	58.358247
2470.453040	17872.428637	58.363252
2469.999384	17752.508949	58.368257
2469.201117	17660.558128	58.373261
2468.361712	17554.104063	58.378266
2468.089368	17441.860258	58.383271
2466.885606	17348.955531	58.388276
2466.392085	17234.482258	58.393281
2465.627484	17133.416198	58.398285
2465.102648	17046.407215	58.403290
2464.328459	16953.631914	58.408295
2463.465622	16847.747440	58.413300
2463.215774	16742.670270	58.418305
2462.234853	16652.664167	58.423309
2461.810385	16547.916147	58.428314
2461.498855	16447.595328	58.433319
2460.491120	16363.878257	58.438324
2459.841442	16259.909255	58.443329
2459.273037	16159.616238	58.448333
2458.214724	16062.604491	58.453338
2457.748473	15976.210655	58.458343
2456.946927	15867.485414	58.463348
2456.458308	15770.636755	58.468353
2455.447408	15686.779037	58.473357
2454.738621	15599.947768	58.478362
2454.527388	15501.986375	58.483367
2453.621694	15417.414949	58.488372
2453.224294	15313.556667	58.493377
2452.363203	15233.879637	58.498381
2451.766663	15132.544129	58.503386
2451.178484	15043.531202	58.508391
2450.199443	14957.689851	58.513396
2449.796217	14848.935191	58.518401
2448.745380	14761.331354	58.523405
2448.204365	14675.212713	58.528410
2447.667443	14589.765897	58.533415
2447.124113	14505.288145	58.538420
2446.411876	14418.135305	58.543425
2445.521942	14331.637074	58.548429
2445.108571	14241.401798	58.553434
2444.333596	14154.380860	58.558439
2443.767523	14074.403536	58.563444
2443.489692	13975.569184	58.568449
2442.508485	13895.599632	58.573453
2441.641093	13804.344708	58.578458
2441.298019	13696.938571	58.583463
2440.382645	13619.059314	58.588468
2439.617353	13535.526596	58.593473
2439.211145	13457.581235	58.598477
2438.402622	13357.113198	58.603482
2437.747659	13278.195522	58.608487
2436.600018	13211.250330	58.613492
2436.356839	13120.525344	58.618497
2435.884201	13045.188494	58.623501
2435.005950	12959.214160	58.628506
2434.563446	12872.577989	58.633511
2433.554474	12791.686778	58.638516
2432.956280	12712.986550	58.643521
2432.489423	12629.534975	58.648525
2431.810296	12534.813355	58.653530
2431.359406	12461.527428	58.658535
2430.245182	12378.386832	58.663540
2429.712938	12292.220353	58.668545
2428.983157	12208.068276	58.673549
2428.370628	12128.012762	58.678554
2427.914355	12046.037912	58.683559
2426.676626	11973.327513	58.688564
2426.649738	11889.676684	58.693569
2425.799720	11812.859006	58.698573
2425.246487	11737.290696	58.703578
2424.631736	11650.635943	58.708583
2423.412939	11577.392421	58.713588
2423.066864	11483.987055	58.718593
2422.468833	11408.863440	58.723597
2421.632357	11346.543185	58.728602
2420.912060	11257.461380	58.733607
2420.314941	11174.726118	58.738612
2419.575139	11093.350952	58.743617
2419.028104	11024.046196	58.748621
2418.339959	10952.469847	58.753626
2417.767942	10865.442370	58.758631
2416.929149	10797.312827	58.763636
2416.303739	10726.248157	58.768641
2415.797158	10661.241536	58.773645
2415.010639	10583.870494	58.778650
2414.625938	10502.816190	58.783655
2413.622044	10428.833673	58.788660
2413.349935	10351.422488	58.793665
2412.715737	10279.960902	58.798669
2411.865473	10199.286610	58.803674
2411.450072	10113.557032	58.808679
2410.154252	10051.668047	58.813684
2410.008630	9959.970155	58.818689
2409.402401	9886.122516	58.823693
2408.620422	9806.305003	58.828698
2407.890239	9734.190218	58.833703
2407.091928	9667.268062	58.838708
2406.477680	9589.980929	58.843713
2405.890046	9521.705698	58.848717
2404.828018	9444.115576	58.853722
2404.616478	9376.748610	58.858727
2403.484117	9307.079503	58.863732
2403.026741	9236.287134	58.868737
2402.227682	9164.299224	58.873741
2401.523711	9094.360809	58.878746
2401.100281	9012.734111	58.883751
2400.559594	8956.412121	58.888756
2399.927548	8876.793521	58.893761
2399.323804	8811.119617	58.898765
2398.397290	8736.840094	58.903770
2398.027551	8654.429758	58.908775
2396.791619	8589.419180	58.913780
2396.223137	8527.161212	58.918785
2395.991850	8464.137657	58.923789
2394.999600	8391.464632	58.928794
2394.724481	8323.053400	58.933799
2393.732568	8239.269591	58.938804
2393.401899	8179.478483	58.943809
2392.502912	8106.638224	58.948813
2391.661738	8037.997784	58.953818
2391.650119	7971.828577	58.958823
2390.679867	7898.344299	58.963828
2389.911367	7821.381066	58.968833
2389.290123	7749.204536	58.973837
2388.469733	7679.072697	58.978842
2388.116374	7599.987440	58.983847
2387.354604	7533.454003	58.988852
2386.787767	7471.266444	58.993857
2385.942962	7400.066572	58.998861
2385.154579	7323.927878	59.003866
2384.690451	7260.348395	59.008871
2383.729397	7194.235397	59.013876
2383.133981	7122.928673	59.018881
2382.588050	7057.188246	59.023885
2381.983852	6994.200855	59.028890
2381.195765	6922.645619	59.033895
2380.671517	6860.277167	59.038900
2380.399613	6788.293637	59.043905
2379.457538	6720.318947	59.048909
2378.689159	6644.523691	59.053914
2378.066911	6576.449243	59.058919
2377.298877	6509.508846	59.063924
2376.802089	6439.271195	59.068929
2375.942548	6370.521474	59.073933
2375.174908	6307.373612	59.078938
2374.734152	6231.537973	59.083943
2373.760173	6181.374300	59.088948
2373.472609	6106.298258	59.093953
2372.734058	6040.302619	59.098957
2371.952254	5973.672870	59.103962
2371.555198	5904.683957	59.108967
2370.588519	5836.004980	59.113972
2370.234835	5774.348378	59.118977
2369.497776	5718.606141	59.123981
2368.462704	5648.072705	59.128986
2367.803810	5574.420417	59.133991
2367.232747	5506.908297	59.138996
2366.430255	5444.207399	59.144001
2366.100417	5379.525442	59.149005
2365.356243	5320.865165	59.154010
2364.669368	5248.432004	59.159015
2364.017292	5184.455072	59.164020
2363.450086	5126.107441	59.169025
2362.380532	5067.941459	59.174029
2361.969983	4998.219891	59.179034
2361.739306	4939.370848	59.184039
2360.683337	4874.377214	59.189044
2360.396583	4805.614916	59.194049
2359.473889	4739.082493	59.199053
2358.661764	4672.324620	59.204058
2358.075408	4604.326124	59.209063
2357.647616	4534.533770	59.214068
2356.875986	4459.496337	59.219073
2356.168979	4407.649595	59.224077
2355.626440	4346.935890	59.229082
2354.931149	4267.983382	59.234087
2353.968209	4213.177812	59.239092
2353.266864	4142.788727	59.244097
2353.049427	4087.626419	59.249101
2352.278659	4028.801217	59.254106
2351.712889	3944.637374	59.259111
2350.826658	3897.231805	59.264116
2350.337165	3831.706561	59.269121
2349.564412	3764.054610	59.274125
2348.827995	3702.524949	59.279130
2348.019045	3641.044906	59.284135
2347.198881	3570.349340	59.289140
2346.657223	3507.109818	59.294145
2345.988970	3456.549703	59.299149
2345.211800	3395.629519	59.304154
2344.744219	3332.515434	59.309159
2344.251467	3276.958211	59.314164
2343.636317	3202.755671	59.319169
2343.373968	3151.379891	59.324173
2342.359210	3087.834742	59.329178
2341.954488	3005.018195	59.334183
2340.924715	2954.252974	59.339188
2340.073719	2878.535943	59.344193
2339.669837	2826.914050	59.349197
2338.545838	2767.901534	59.354202
2338.060695	2698.980263	59.359207
2337.226618	2638.226036	59.364212
2336.598939	2574.945044	59.369217
2336.148722	2523.018508	59.374221
2335.489075	2461.997620	59.379226
2335.191450	2397.941921	59.384231
2334.019670	2343.980038	59.389236
2333.643816	2279.252790	59.394241
2332.995411	2215.572898	59.399245
2331.845618	2161.403968	59.404250
2331.709630	2093.984420	59.409255
2330.682665	2037.837697	59.414260
2329.968639	1989.354352	59.419265
2329.535295	1929.995965	59.424269
2328.478810	1871.795673	59.429274
2328.217905	1820.780764	59.434279
2327.446932	1774.972431	59.439284
2326.873399	1707.735254	59.444289
2326.387974	1646.798964	59.449293
2325.642326	1584.478548	59.454298
2325.051411	1518.628078	59.459303
2324.354224	1468.391700	59.464308
2323.786634	1402.156414	59.469313
2322.704374	1341.268761	59.474317
2321.819210	1291.294636	59.479322
2321.271314	1237.673163	59.484327
2320.497727	1199.632294	59.489332
2320.187290	1134.451887	59.494337
2319.546283	1065.281570	59.499341
2318.495515	1026.624360	59.504346
2317.913447	970.508183	59.509351
2317.277139	932.925644	59.514356
2316.696179	863.906827	59.519361
2316.203077	815.909605	59.524365
2315.314548	757.373327	59.529370
2314.839388	705.287711	59.534375
2313.976810	662.982502	59.539380
2313.390172	603.213091	59.544385
2312.760738	536.529521	59.549389
2311.930328	497.922350	59.554394
2311.348122	462.653702	59.559399
2310.593709	407.505318	59.564404
2309.881784	338.531855	59.569409
2309.162453	316.353251	59.574413
2308.271358	247.424412	59.579418
2307.761992	206.646153	59.584423
2306.815805	173.780804	59.589428
2306.267970	117.044360	59.594433
2305.310866	78.895208	59.599437
2304.204095	59.118566	59.604442
2303.894673	23.038200	59.609447
2302.855999	-16.288308	59.614452
2301.704483	-38.749451	59.619457
2300.383575	-38.525542	59.624461
2295.209409	79.025865	59.629466
2294.939689	83.275981	59.634471
2295.909662	84.763845	59.639476
2296.640651	80.854074	59.644481
2297.011179	75.902390	59.649485
2296.155194	83.052370	59.654490
2295.701749	73.667870	59.659495
2295.401504	75.500722	59.664500
2294.525632	93.455566	59.669505
2293.857458	83.734552	59.674509
2292.585122	86.590476	59.679514
2291.479684	77.421360	59.684519
2291.083226	83.415122	59.689524
2290.178451	83.434257	59.694529
2290.112710	89.973202	59.699533
2289.871628	93.898670	59.704538
2289.239837	92.721794	59.709543
2288.347638	92.421979	59.714548
2287.224356	102.228860	59.719553
2286.678412	95.154978	59.724557
2285.960946	99.031442	59.729562
2285.559878	95.812159	59.734567
2284.935447	98.486465	59.739572
2284.664281	103.085310	59.744577
2284.169319	91.777270	59.749581
2283.288464	96.796093	59.754586
2282.749264	80.152569	59.759591
2281.877831	91.496383	59.764596
2280.974330	97.785044	59.769601
2280.102637	96.438076	59.774605
2279.561603	90.077753	59.779610
2279.439113	79.669387	59.784615
2278.873503	86.218243	59.789620
2277.882999	86.482786	59.794625
2277.263916	85.472625	59.799629
2275.837861	94.375091	59.804634
2275.946489	85.022845	59.809639
2275.609566	84.472529	59.814644
2274.882351	83.864284	59.819649
2274.364551	84.752402	59.824653
2273.367025	81.979391	59.829658
2272.814651	84.106123	59.834663
2271.865565	90.925543	59.839668
2270.934422	103.631814	59.844673
2270.344257	88.171156	59.849677
2270.036357	92.949284	59.854682
2269.722353	79.527900	59.859687
2268.988219	83.834346	59.864692
2268.234758	91.228259	59.869697
2267.592223	92.128282	59.874701
2266.643592	93.944155	59.879706
2266.125152	89.608135	59.884711
2265.225094	88.333480	59.889716
2264.217705	89.373383	59.894721
2264.542020	88.193064	59.899725
2264.053239	86.339097	59.904730
2262.830575	89.190309	59.909735
2262.358054	87.038885	59.914740
2261.936121	94.323438	59.919745
2260.965271	78.710306	59.924750
2259.848151	90.108869	59.929754
2259.971982	95.130732	59.934759
2259.427668	89.489997	59.939764
2258.547691	92.160695	59.944769
2257.820661	83.294246	59.949774
2257.164930	84.921734	59.954778
2255.639326	96.503373	59.959783
2255.542372	92.348060	59.964788
2254.864214	95.535501	59.969793
2254.074041	92.548258	59.974798
2253.355885	95.844542	59.979802
2252.378635	88.146842	59.984807
2252.675650	93.983289	59.989812
2252.248130	90.440217	59.994817
2251.173296	76.541901	59.999822
2250.094100	95.462528	60.004826
2249.893594	82.918815	60.009831
2249.608001	82.656815	60.014836
2248.571592	87.911625	60.019841
2247.659965	91.858321	60.024846
2246.986200	92.189316	60.029850
2246.988306	82.033989	60.034855
2245.808913	85.657326	60.039860
2244.674669	85.755458	60.044865
2244.799023	83.728533	60.049870
2243.958852	100.446176	60.054874
2243.642392	92.705144	60.059879
2242.450895	91.009973	60.064884
2241.507951	95.064138	60.069889
2241.705137	94.947888	60.074894
2240.723898	84.682072	60.079898
2239.691193	82.553297	60.084903
2239.310258	90.812172	60.089908
2238.726816	98.423539	60.094913
2238.453616	83.783057	60.099918
2237.003867	89.876124	60.104922
2236.099706	86.987394	60.109927
2236.186983	84.371863	60.114932
2235.261442	91.433553	60.119937
2234.864928	94.626774	60.124942
2234.291926	96.424064	60.129946
2233.447691	87.584100	60.134951
2232.254341	81.339900	60.139956
2231.857012	90.769852	60.144961
2231.516206	85.658213	60.149966
2231.068404	86.748115	60.154970
2230.141211	79.523440	60.159975
2229.199318	90.839020	60.164980
2228.469618	94.353176	60.169985
2228.488094	79.352623	60.174990
2227.490691	86.231756	60.179994
2226.361232	89.902371	60.184999
2225.971526	80.946148	60.190004
2225.832214	81.132433	60.195009
2225.434487	76.225363	60.200014
2223.747589	95.721785	60.205018
2223.433043	82.656874	60.210023
2222.571845	79.658836	60.215028
2221.731598	88.578764	60.220033
2221.910776	90.138450	60.225038
2221.152210	92.545478	60.230042
2220.046307	80.555413	60.235047
2219.687448	89.744305	60.240052
2218.763246	78.723586	60.245057
2218.546948	78.327597	60.250062
2217.685764	82.214259	60.255066
2217.273697	85.348450	60.260071
2216.424853	78.656955	60.265076
2216.056760	78.777040	60.270081
2215.629488	76.271532	60.275086
2213.852355	83.624448	60.280090
2213.226833	83.436884	60.285095
2213.260066	79.749759	60.290100
2212.392596	95.702210	60.295105
2211.667999	75.401363	60.300110
2210.355730	76.885457	60.305114
2210.105641	75.952380	60.310119
2210.183151	83.122999	60.315124
2209.132860	86.771597	60.320129
2208.223749	74.813396	60.325134
2207.217459	81.654520	60.330138
2206.944260	77.706945	60.335143
2206.238562	73.086854	60.340148
2205.683715	78.104427	60.345153
2205.332165	65.671432	60.350158
2204.691459	78.569724	60.355162
2203.845429	77.704395	60.360167
2203.642024	79.009403	60.365172
2202.690973	88.874126	60.370177
2202.600587	77.317435	60.375182
2200.711717	81.496463	60.380186
2200.074062	81.697166	60.385191
2199.609388	72.959422	60.390196
2199.080535	87.265482	60.395201
2198.347684	76.457255	60.400206
2197.773033	78.480306	60.405210
2197.244167	80.346289	60.410215
2196.758420	81.104761	60.415220
2195.627739	91.357520	60.420225
2195.283622	84.535487	60.425230
2194.728882	85.714898	60.430234
2194.234983	83.872797	60.435239
2193.812331	79.455369	60.440244
2192.555207	84.923406	60.445249
2191.831599	82.606840	60.450254
2190.841915	82.541715	60.455258
2190.681505	82.326088	60.460263
2189.756838	79.778085	60.465268
2188.863248	81.277756	60.470273
2189.113827	81.829515	60.475278
2187.865495	84.014653	60.480282
2187.208997	69.207944	60.485287
2186.746309	84.334523	60.490292
2186.366204	81.572387	60.495297
2186.179744	67.839075	60.500302
2184.913450	97.278865	60.505306
2183.916708	72.443504	60.510311
2182.943832	75.048541	60.515316
2182.229464	86.239721	60.520321
2181.823618	83.842777	60.525326
2181.496696	84.061986	60.530330
2180.590007	79.303489	60.535335
2180.199306	78.282344	60.540340
2179.364658	91.561492	60.545345
2179.126645	76.778260	60.550350
2178.335613	71.987222	60.555354
2177.982068	66.423478	60.560359
2177.258666	72.634695	60.565364
2175.662213	73.149958	60.570369
2175.262996	65.726425	60.575374
2174.540958	77.997409	60.580378
2173.803946	71.193576	60.585383
2172.997164	75.972020	60.590388
2172.551074	76.615399	60.595393
2172.305416	74.680299	60.600398
2171.572370	82.455749	60.605402
2171.064008	69.610844	60.610407
2170.907819	68.643951	60.615412
2170.297248	69.152586	60.620417
2169.281227	64.334179	60.625422
2168.263595	87.526292	60.630426
2167.683969	65.478937	60.635431
2167.069394	78.310011	60.640436
2166.286906	83.116141	60.645441
2165.418420	63.632918	60.650446
2164.454248	85.657534	60.655450
2164.267804	73.814909	60.660455
2163.504619	71.838934	60.665460
2162.687192	71.640834	60.670465
2162.186013	72.272457	60.675470
2161.243731	81.109239	60.680474
2161.101009	65.987640	60.685479
2160.547014	74.966225	60.690484
2159.906534	80.341155	60.695489
2159.541292	69.506154	60.700494
2158.936920	76.280361	60.705498
2157.569665	68.931595	60.710503
2157.142290	68.096040	60.715508
2156.333280	70.783887	60.720513
2155.926310	74.566952	60.725518
2155.181678	85.064377	60.730522
2154.377317	78.230235	60.735527
2153.335481	67.195107	60.740532
2152.224038	76.866099	60.745537
2152.844108	70.368879	60.750542
2151.633964	71.893563	60.755546
2150.948503	75.671937	60.760551
2150.416786	77.757567	60.765556
2149.686049	64.127980	60.770561
2149.098215	66.476393	60.775566
2148.590163	75.100774	60.780570
2148.323349	72.246555	60.785575
2147.001860	71.753148	60.790580
2145.747738	74.541592	60.795585
2145.672691	79.694341	60.800590
2145.428650	76.626783	60.805594
2144.647955	77.025231	60.810599
2144.062090	70.189540	60.815604
2143.585621	65.266602	60.820609
2143.118327	75.738935	60.825614
2141.684998	70.881107	60.830618
2140.282501	77.293134	60.835623
2140.019844	64.425023	60.840628
2139.888942	68.202125	60.845633
2139.673035	76.121008	60.850638
2138.692562	62.024877	60.855642
2138.275613	64.175871	60.860647
2137.807524	74.632560	60.865652
2136.562617	65.450973	60.870657
2135.425697	69.047111	60.875662
2135.047939	66.677259	60.880666
2134.401159	79.901362	60.885671
2134.182263	70.549071	60.890676
2133.501801	56.906789	60.895681
2133.072166	70.200499	60.900686
2132.611642	60.495491	60.905690
2131.010540	66.317740	60.910695
2130.744737	68.216102	60.915700
2129.708706	67.346258	60.920705
2129.398557	59.782454	60.925710
2128.909896	67.798230	60.930714
2128.120745	67.436389	60.935719
2126.881378	78.034400	60.940724
2125.988040	65.414603	60.945729
2126.190081	66.428202	60.950734
2124.984052	73.278968	60.955738
2124.621470	70.391067	60.960743
2124.408923	60.791783	60.965748
2123.687563	58.086971	60.970753
2123.162792	67.250144	60.975758
2122.633373	67.879947	60.980762
2121.442425	63.765805	60.985767
2120.636182	63.190645	60.990772
2119.634564	71.984812	60.995777
2119.627057	53.344242	61.000782
2119.234232	53.925562	61.005786
2118.655604	68.688918	61.010791
2117.462823	61.172149	61.015796
2116.498629	69.380083	61.020801
2116.461315	69.729951	61.025806
2115.577605	64.433273	61.030810
2114.961579	74.189650	61.035815
2113.846786	61.969267	61.040820
2112.834696	75.484720	61.045825
2113.223881	65.856171	61.050830
2112.237485	70.981664	61.055834
2111.233872	67.932156	61.060839
2111.335768	67.980823	61.065844
2110.100782	59.698082	61.070849
2109.998014	57.029140	61.075854
2108.626352	65.172433	61.080858
2107.743884	68.037525	61.085863
2107.333569	60.273588	61.090868
2106.160569	65.300967	61.095873
2106.068049	65.180223	61.100878
2105.709657	70.351127	61.105882
2104.972645	66.581251	61.110887
2104.873653	59.444392	61.115892
2104.197113	75.592032	61.120897
2103.122812	60.096344	61.125902
2102.185811	60.275193	61.130906
2101.684697	58.013231	61.135911
2101.001524	64.919790	61.140916
2100.720518	62.520399	61.145921
2099.567990	60.912150	61.150926
2098.410412	63.231149	61.155930
2098.367434	60.331955	61.160935
2098.021996	57.742525	61.165940
2097.170032	74.927211	61.170945
2096.812985	63.761361	61.175950
2095.580599	65.439403	61.180954
2094.323983	64.591966	61.185959
2094.384697	62.843210	61.190964
2093.297263	74.211868	61.195969
2093.117740	66.362420	61.200974
2092.734119	61.208727	61.205978
2092.347304	77.095932	61.210983
2091.455959	57.425582	61.215988
2090.190079	64.440391	61.220993
2089.972828	58.309433	61.225998
2089.386673	58.486219	61.231002
2088.289703	56.948004	61.236007
2087.430127	58.339810	61.241012
2086.708297	65.977874	61.246017
2086.368174	52.262679	61.251022
2085.669715	59.387698	61.256026
2084.974232	70.107548	61.261031
2084.937407	56.024106	61.266036
2083.889233	71.565279	61.271041
2083.553467	56.866989	61.276046
2082.564668	52.861129	61.281050
2081.661358	76.334700	61.286055
2081.438409	63.282114	61.291060
2080.751651	69.536418	61.296065
2080.512517	52.350239	61.301070
2078.998238	69.551732	61.306074
2078.315404	68.007713	61.311079
2077.894439	58.444671	61.316084
2077.139551	65.782068	61.321089
2076.684173	53.540632	61.326094
2076.117978	63.429441	61.331098
2075.015271	78.216065	61.336103
2074.550416	57.295371	61.341108
2073.797997	52.195487	61.346113
2073.151880	63.585559	61.351118
2073.183675	60.163588	61.356122
2072.191055	71.402089	61.361127
2071.236836	64.336315	61.366132
2070.359086	64.141511	61.371137
2069.729681	67.053177	61.376142
2069.151270	56.868604	61.381146
2069.012800	64.111322	61.386151
2068.306426	69.652836	61.391156
2067.115016	63.190812	61.396161
2066.130075	69.087185	61.401166
2065.702494	58.391415	61.406170
2065.043176	68.657692	61.411175
2065.059777	65.205017	61.416180
2064.320242	68.693959	61.421185
2064.105010	62.056503	61.426190
2062.534227	66.087367	61.431194
2061.707355	67.374647	61.436199
2061.510639	56.359976	61.441204
2060.823846	62.811396	61.446209
2060.587682	62.358654	61.451214
2059.508595	67.699138	61.456218
2057.931768	64.769016	61.461223
2057.881727	63.247565	61.466228
2057.246939	65.054692	61.471233
2056.903534	55.176586	61.476238
2056.410189	64.434119	61.481242
2055.845814	61.097310	61.486247
2054.897431	55.323667	61.491252
2053.876489	63.572159	61.496257
2053.500091	56.357918	61.501262
2053.333422	50.911192	61.506266
2052.320222	64.264406	61.511271
2051.335271	63.479523	61.516276
2050.620966	61.860087	61.521281
2050.154755	58.067748	61.526286
2049.573930	67.235095	61.531290
2049.132875	69.555500	61.536295
2048.465960	59.060141	61.541300
2047.273276	67.862576	61.546305
2046.734070	51.359522	61.551310
2046.127936	72.113102	61.556314
2045.715109	59.085936	61.561319
2045.339574	53.087339	61.566324
2044.083481	57.102954	61.571329
2043.503807	65.186797	61.576334
2042.946166	57.331149	61.581338
2042.278044	61.165136	61.586343
2041.982016	61.773678	61.591348
2040.546095	67.371072	61.596353
2039.807307	59.332873	61.601358
2039.169752	60.471844	61.606362
2038.733830	56.933310	61.611367
2038.456619	66.411996	61.616372
2037.792200	64.666378	61.621377
2037.533842	61.776143	61.626382
2036.638631	64.685854	61.631386
2035.327361	60.866809	61.636391
2035.024447	59.475379	61.641396
2034.416556	60.543413	61.646401
2033.852587	58.592627	61.651406
2033.440998	66.788559	61.656410
2032.025056	69.648468	61.661415
2031.457576	61.821190	61.666420
2030.625510	55.059311	61.671425
2030.234648	55.529950	61.676430
2029.823184	63.552403	61.681434
2029.195004	67.993462	61.686439
2028.436195	56.126617	61.691444
2027.397029	56.775852	61.696449
2026.916708	57.041504	61.701454
2026.446713	62.837227	61.706458
2026.182502	61.373426	61.711463
2025.698408	57.397860	61.716468
2024.284684	64.486622	61.721473
2023.528491	59.906147	61.726478
2022.884687	64.396992	61.731482
2022.304591	65.777572	61.736487
2022.618728	62.377014	61.741492
2021.143852	62.527734	61.746497
2020.263780	65.075517	61.751502
2019.934316	58.500355	61.756506
2019.118516	56.463396	61.761511
2018.886960	57.851726	61.766516
2017.634582	62.197909	61.771521
2016.727481	60.271633	61.776526
2016.359703	56.960396	61.781530
2015.495535	65.346434	61.786535
2015.536209	47.207580	61.791540
2015.085044	62.516804	61.796545
2014.055701	60.884310	61.801550
2013.287969	53.945077	61.806554
2012.189985	61.060992	61.811559
2012.094498	63.039555	61.816564
2011.386829	62.251671	61.821569
2010.443637	64.008420	61.826574
2009.443435	57.505039	61.831578
2008.617708	55.655731	61.836583
2008.181593	49.439689	61.841588
2007.666419	54.663866	61.846593
2007.548054	62.666602	61.851598
2007.258047	62.358023	61.856602
2006.400498	75.118872	61.861607
2005.578551	54.493003	61.866612
2004.663751	66.840329	61.871617
2004.171786	51.864100	61.876622
2003.561012	55.009353	61.881626
2001.918614	68.314234	61.886631
2001.785146	67.450973	61.891636
2001.061969	67.822987	61.896641
2000.778973	58.778936	61.901646
2000.490215	67.184020	61.906650
1999.600311	74.858247	61.911655
1998.607484	63.523699	61.916660
1997.839847	58.434139	61.921665
1997.118354	63.134432	61.926670
1996.710461	62.776762	61.931674
1996.205321	67.805396	61.936679
1995.832264	68.837738	61.941684
1995.041288	63.644654	61.946689
1993.903916	64.654828	61.951694
1993.715581	64.126693	61.956698
1992.678703	66.054432	61.961703
1991.908326	59.561881	61.966708
1991.350215	58.330811	61.971713
1990.989032	58.203836	61.976718
1990.538428	61.571238	61.981722
1989.571726	51.840978	61.986727
1988.807800	59.881538	61.991732
1987.684070	65.202327	61.996737
1987.508938	57.134593	62.001742
1986.915531	66.450594	62.006746
1986.156857	52.235769	62.011751
1985.542750	55.569204	62.016756
1984.275846	64.314058	62.021761
1983.532832	63.747826	62.026766
1983.426608	58.365625	62.031770
1983.091591	62.203513	62.036775
1982.755626	50.668519	62.041780
1981.960269	63.430528	62.046785
1980.818496	64.420907	62.051790
1980.040272	54.974529	62.056794
1979.658760	65.147831	62.061799
1979.285150	55.257192	62.066804
1978.013409	65.811502	62.071809
1977.221350	65.522705	62.076814
1976.894670	64.221784	62.081818
1976.295943	58.007906	62.086823
1975.849375	54.086317	62.091828
1974.715671	62.223428	62.096833
1973.788681	56.608842	62.101838
1973.282305	58.029764	62.106842
1972.559344	70.122727	62.111847
1972.828442	56.359730	62.116852
1972.408201	62.989616	62.121857
1971.163285	61.006603	62.126862
1970.313501	59.217894	62.131866
1969.579643	67.923865	62.136871
1969.328535	63.577023	62.141876
1968.319900	63.444031	62.146881
1967.314564	55.211644	62.151886
1966.778258	59.064142	62.156890
1966.043400	56.862970	62.161895
1965.809983	44.395537	62.166900
1965.526979	55.392094	62.171905
1964.533579	55.873246	62.176910
1963.741240	51.765288	62.181914
1963.173998	68.895323	62.186919
1962.659531	55.244106	62.191924
1961.583064	64.587913	62.196929
1960.494642	60.933795	62.201934
1960.086935	61.698842	62.206938
1959.571513	66.317546	62.211943
1959.027333	58.491323	62.216948
1958.707806	61.976686	62.221953
1958.123563	58.210990	62.226958
1956.964760	63.508974	62.231962
1956.115237	64.566503	62.236967
1955.948098	51.296949	62.241972
1955.316956	64.455497	62.246977
1954.503465	52.638366	62.251982
1953.650078	53.348018	62.256986
1952.948921	64.921877	62.261991
1952.935025	62.224645	62.266996
1952.161727	59.865583	62.272001
1951.317009	56.798803	62.277006
1950.207588	62.051103	62.282010
1949.545409	69.365926	62.287015
1949.131857	65.342907	62.292020
1948.731469	66.272367	62.297025
1948.396713	64.236327	62.302030
1947.215199	50.536486	62.307034
1946.305054	50.173410	62.312039
1946.000510	52.785954	62.317044
1945.172078	63.066477	62.322049
1944.900466	58.730780	62.327054
1943.818456	56.136895	62.332058
1942.879192	65.693881	62.337063
1942.707607	57.318099	62.342068
1941.998297	60.165210	62.347073
1941.383482	58.637238	62.352078
1940.404781	61.375738	62.357082
1939.303879	59.451875	62.362087
1938.871481	59.132795	62.367092
1938.524936	51.965879	62.372097
1937.995790	70.029689	62.377102
1937.843334	65.665612	62.382106
1936.823111	61.647455	62.387111
1936.200720	64.163815	62.392116
1935.599758	58.488021	62.397121
1934.794425	68.714423	62.402126
1933.826355	56.658500	62.407130
1932.634792	68.329147	62.412135
1932.729673	57.654541	62.417140
1932.236318	53.261017	62.422145
1931.323318	72.305094	62.427150
1931.008442	58.880806	62.432154
1930.011600	56.853697	62.437159
1929.349522	53.578164	62.442164
1928.699613	66.099481	62.447169
1928.247777	60.429973	62.452174
1927.854829	53.287772	62.457178
1926.415969	57.617871	62.462183
1926.029659	60.964035	62.467188
1925.239034	52.719657	62.472193
1924.788539	63.083676	62.477198
1924.721136	61.183381	62.482202
1923.204566	58.841417	62.487207
1922.623764	56.931175	62.492212
1921.980159	68.037031	62.497217
1921.612549	62.358882	62.502222
1921.323133	66.399262	62.507226
1919.927206	69.877342	62.512231
1919.271692	48.017213	62.517236
1918.803460	66.613794	62.522241
1918.106363	64.206376	62.527246
1917.713441	54.579006	62.532250
1916.482296	57.352863	62.537255
1915.755517	50.774578	62.542260
1915.468118	62.979730	62.547265
1915.082893	63.481028	62.552270
1915.056164	60.943523	62.557274
1913.537373	59.013484	62.562279
1913.140674	56.995170	62.567284
1912.454725	55.784415	62.572289
1910.811785	59.680168	62.577294
1910.517347	55.185683	62.582298
1909.901250	53.940185	62.587303
1909.454035	55.673410	62.592308
1908.946692	58.286620	62.597313
1908.436828	60.365668	62.602318
1908.216510	49.357933	62.607322
1907.040249	54.346482	62.612327
1906.098130	54.284951	62.617332
1905.526977	62.129349	62.622337
1904.949194	61.978432	62.627342
1904.484621	58.923846	62.632346
1903.015770	54.921747	62.637351
1902.795768	63.981358	62.642356
1902.577853	58.057106	62.647361
1901.501231	67.080850	62.652366
1901.652256	50.331072	62.657370
1900.119667	59.570705	62.662375
1899.229318	50.826532	62.667380
1899.157402	58.271554	62.672385
1898.591289	63.499107	62.677390
1897.974058	48.497079	62.682394
1896.614924	62.529700	62.687399
1896.029696	51.314991	62.692404
1895.458845	59.384834	62.697409
1894.993485	48.237824	62.702414
1895.045192	54.412748	62.707418
1893.633799	59.940087	62.712423
1893.005318	53.928070	62.717428
1892.580176	60.872540	62.722433
1891.888126	49.770984	62.727438
1891.492130	56.734477	62.732442
1890.070963	64.059438	62.737447
1889.621623	56.664436	62.742452
1889.261053	49.780443	62.747457
1888.454873	56.709722	62.752462
1888.078330	49.768345	62.757466
1886.468461	58.734840	62.762471
1886.513165	47.517881	62.767476
1885.971141	46.809383	62.772481
1885.391453	45.933408	62.777486
1884.790887	54.296538	62.782490
1884.188910	48.002787	62.787495
1883.439858	54.896189	62.792500
1882.264913	50.737054	62.797505
1881.277706	57.029636	62.802510
1880.861692	51.442760	62.807514
1880.156984	62.094716	62.812519
1879.934703	47.908307	62.817524
1879.644978	51.303790	62.822529
1878.741344	46.710511	62.827534
1877.903759	48.434765	62.832538
1877.233840	48.080876	62.837543
1876.900488	46.664340	62.842548
1876.253989	55.001651	62.847553
1874.991286	56.370806	62.852558
1874.521948	47.622869	62.857562
1873.963468	48.899125	62.862567
1873.275046	50.479852	62.867572
1872.496889	51.169700	62.872577
1871.261671	58.223878	62.877582
1871.138001	57.012157	62.882586
1870.339711	56.497311	62.887591
1870.115389	56.626152	62.892596
1869.932809	55.094217	62.897601
1868.988492	59.361586	62.902606
1868.151454	51.014220	62.907610
1867.150507	45.925488	62.912615
1866.820335	44.703983	62.917620
1865.541413	49.625274	62.922625
1864.761960	39.280326	62.927630
1864.390656	50.623621	62.932634
1863.879805	44.488865	62.937639
1863.410888	55.065532	62.942644
1863.298362	40.713479	62.947649
1862.320103	51.065107	62.952654
1861.521523	48.577634	62.957658
1860.797619	55.492278	62.962663
1860.289495	47.734478	62.967668
1859.467701	48.713519	62.972673
1858.461205	55.237818	62.977678
1857.930806	48.898018	62.982682
1857.351359	62.759537	62.987687
1857.043977	39.483322	62.992692
1855.985098	52.003349	62.997697
1854.984843	57.817063	63.002702
1854.624855	55.163754	63.007706
1853.773455	54.400316	63.012711
1853.609256	59.261291	63.017716
1853.208586	47.966832	63.022721
1852.221716	56.544268	63.027726
1851.175591	46.684771	63.032730
1850.826637	55.318596	63.037735
1850.555865	44.391426	63.042740
1849.939543	51.971775	63.047745
1848.429728	51.188319	63.052750
1847.942315	47.571275	63.057754
1847.296539	46.926567	63.062759
1847.072135	46.613897	63.067764
1846.257878	52.461151	63.072769
1845.038831	50.288022	63.077774
1844.601577	52.789192	63.082778
1844.106191	53.186573	63.087783
1843.780028	46.595159	63.092788
1843.319247	53.029649	63.097793
1842.226647	59.578666	63.102798
1841.769932	56.128626	63.107802
1840.915913	50.743773	63.112807
1840.422844	55.735816	63.117812
1839.434433	54.965756	63.122817
1838.682110	65.928043	63.127822
1838.314140	42.470649	63.132826
1837.860984	62.878240	63.137831
1837.127551	43.365893	63.142836
1836.225868	56.135343	63.147841
1835.320518	53.322649	63.152846
1835.025349	49.555236	63.157850
1834.597401	56.039705	63.162855
1833.833739	50.638928	63.167860
1832.678740	42.384650	63.172865
1832.087221	50.438857	63.177870
1831.942309	49.747728	63.182874
1831.145967	49.727726	63.187879
1830.067217	45.384616	63.192884
1829.672275	46.660140	63.197889
1828.801222	67.816890	63.202894
1828.620821	57.469848	63.207898
1828.055847	57.045691	63.212903
1826.578502	51.573758	63.217908
1826.066399	47.547497	63.222913
1825.260024	58.425329	63.227918
1825.423759	54.643384	63.232922
1824.757300	51.912600	63.237927
1823.791621	44.851919	63.242932
1823.497723	47.279865	63.247937
1822.747680	51.185249	63.252942
1821.491747	47.997749	63.257946
1820.524277	56.121126	63.262951
1819.938832	48.829757	63.267956
1819.438488	41.324614	63.272961
1818.862831	52.168957	63.277966
1818.975808	45.684419	63.282970
1818.080403	54.089650	63.287975
1817.274021	54.476504	63.292980
1816.350731	49.804373	63.297985
1815.686191	57.289890	63.302990
1815.469771	46.822428	63.307994
1814.395346	46.679444	63.312999
1813.812438	49.884960	63.318004
1813.024399	54.230024	63.323009
1812.481341	54.895168	63.328014
1812.324399	46.968075	63.333018
1811.209979	52.740010	63.338023
1810.512411	43.150018	63.343028
1810.071858	50.811263	63.348033
1809.443313	61.632475	63.353038
1808.597681	56.895974	63.358042
1807.796866	55.771297	63.363047
1806.839607	50.431236	63.368052
1807.102396	53.849360	63.373057
1805.598122	62.155762	63.378062
1804.766656	45.938909	63.383066
1803.975670	51.717825	63.388071
1803.639977	59.707759	63.393076
1803.330502	55.956813	63.398081
1802.647627	59.603967	63.403086
1802.690492	47.411221	63.408090
1801.322014	54.600124	63.413095
1800.654664	57.744942	63.418100
1800.224839	56.039400	63.423105
1799.321414	62.474815	63.428110
1798.426664	48.314804	63.433114
1797.577638	59.391794	63.438119
1796.935057	56.745531	63.443124
1797.096839	49.655603	63.448129
1796.266749	51.328232	63.453134
1795.190083	49.206628	63.458138
1794.375059	53.560713	63.463143
1794.021045	50.176372	63.468148
1793.606234	51.865045	63.473153
1792.886587	65.912834	63.478158
1791.812998	55.438008	63.483162
1791.103974	49.052482	63.488167
1790.381592	54.207101	63.493172
1790.348542	54.447490	63.498177
1789.657070	57.537797	63.503182
1788.980473	57.369485	63.508186
1787.705112	51.747232	63.513191
1787.112804	58.172658	63.518196
1787.250992	50.755333	63.523201
1785.769026	48.584568	63.528206
1785.304833	49.905789	63.533210
1784.339826	54.673186	63.538215
1784.295999	57.566021	63.543220
1783.980225	60.937267	63.548225
1782.918285	58.406494	63.553230
1782.446055	50.781779	63.558234
1781.790937	62.882910	63.563239
1780.960308	53.697237	63.568244
1780.424804	44.348008	63.573249
1779.440877	61.047501	63.578254
1779.200779	44.268406	63.583258
1777.912857	41.650533	63.588263
1776.861290	57.042495	63.593268
1776.547529	53.658071	63.598273
1775.910841	56.526801	63.603278
1775.684288	52.182399	63.608282
1775.015224	56.866528	63.613287
1774.511290	52.559874	63.618292
1773.706287	46.262134	63.623297
1772.527949	67.284776	63.628302
1772.337451	48.728540	63.633306
1771.883161	63.707118	63.638311
1770.829799	47.076112	63.643316
1770.290467	52.288390	63.648321
1769.242224	50.919185	63.653326
1768.719841	52.840980	63.658330
1768.386254	52.793228	63.663335
1767.515619	56.478095	63.668340
1766.760118	47.969596	63.673345
1766.186704	51.386492	63.678350
1765.970638	51.069351	63.683354
1765.089675	52.398425	63.688359
1764.566278	46.555833	63.693364
1764.014247	48.668408	63.698369
1762.948698	49.970033	63.703374
1762.204419	48.115758	63.708378
1761.445972	53.438529	63.713383
1760.786506	46.168398	63.718388
1760.739456	49.605767	63.723393
1759.860293	53.230492	63.728398
1758.987606	51.402919	63.733402
1758.146565	51.360078	63.738407
1757.678439	51.942372	63.743412
1757.250861	52.625453	63.748417
1756.464226	54.079890	63.753422
1755.308411	52.380863	63.758426
1754.763267	55.924154	63.763431
1754.342507	54.993005	63.768436
1754.114678	37.097124	63.773441
1753.422501	54.578135	63.778446
1752.451590	55.569856	63.783450
1751.738506	45.072491	63.788455
1750.671706	48.410068	63.793460
1750.700880	40.160127	63.798465
1749.669139	49.438541	63.803470
1748.655293	50.260473	63.808474
1747.874435	45.520018	63.813479
1747.850383	51.408932	63.818484
1747.590574	51.529228	63.823489
1746.752699	55.495890	63.828494
1745.681040	45.744577	63.833498
1745.045129	53.862616	63.838503
1744.225989	49.976602	63.843508
1744.305780	55.773333	63.848513
1743.208485	43.250789	63.853518
1742.275090	48.415280	63.858522
1741.778722	50.225719	63.863527
1741.387547	47.411813	63.868532
1740.796802	47.412796	63.873537
1739.607523	50.001893	63.878542
1739.077951	47.444924	63.883546
1738.626398	60.300586	63.888551
1738.312520	47.281461	63.893556
1737.188869	43.066946	63.898561
1736.009108	56.140770	63.903566
1735.729240	53.126266	63.908570
1735.158785	48.522697	63.913575
1734.592029	48.261262	63.918580
1734.669864	37.748660	63.923585
1733.416516	45.512207	63.928590
1732.836433	41.217662	63.933594
1732.069057	44.149733	63.938599
1730.976105	56.888088	63.943604
1730.029656	49.015454	63.948609
1729.700600	46.593786	63.953614
1729.590130	42.975240	63.958618
1729.043660	53.028094	63.963623
1728.285282	54.788696	63.968628
1727.672702	43.210984	63.973633
1726.781994	52.834417	63.978638
1726.069630	45.796617	63.983642
1724.786780	55.496534	63.988647
1724.065971	46.976233	63.993652
1724.028934	43.338138	63.998657
1723.400342	54.186169	64.003662
1723.386503	41.500998	64.008666
1722.073447	49.777059	64.013671
1721.106715	57.815196	64.018676
1720.919052	46.882736	64.023681
1720.254980	49.367915	64.028686
1719.308705	50.041936	64.033690
1718.245919	52.644064	64.038695
1717.553792	55.400193	64.043700
1717.157750	47.014378	64.048705
1716.861985	57.580897	64.053710
1716.547163	42.338533	64.058714
1715.714208	50.315995	64.063719
1714.718458	41.490885	64.068724
1714.526445	41.512110	64.073729
1713.294827	40.236711	64.078734
1712.610796	48.783422	64.083738
1712.049705	40.699783	64.088743
1711.407352	51.351313	64.093748
1711.217373	42.084409	64.098753
1710.000465	47.147296	64.103758
1709.232587	44.194549	64.108762
1708.634758	52.027437	64.113767
1708.190869	53.417981	64.118772
1707.763815	41.109096	64.123777
1706.856020	42.637983	64.128782
1706.257507	45.309860	64.133786
1705.745008	37.581188	64.138791
1704.985956	51.114863	64.143796
1704.177185	47.408558	64.148801
1702.844014	51.017115	64.153806
1702.501288	42.066200	64.158810
1702.436292	41.034395	64.163815
1701.845647	51.073768	64.168820
1701.318844	38.946305	64.173825
1700.103521	50.436293	64.178830
1699.707696	46.768466	64.183834
1699.364984	44.642272	64.188839
1698.152741	54.597474	64.193844
1697.485521	38.406629	64.198849
1696.410390	54.992892	64.203854
1696.118284	43.304361	64.208858
1695.994308	39.066675	64.213863
1694.767012	51.991949	64.218868
1694.034092	37.205503	64.223873
1693.706206	45.566336	64.228878
1693.090812	42.212498	64.233882
1692.103684	54.118805	64.238887
1691.443685	56.852491	64.243892
1691.175188	44.822758	64.248897
1690.149771	51.392689	64.253902
1689.915853	47.237118	64.258906
1689.554988	51.530122	64.263911
1688.076818	48.280228	64.268916
1687.792141	53.940897	64.273921
1686.992448	55.889414	64.278926
1686.744073	49.418130	64.283930
1685.756448	53.448019	64.288935
1684.749946	50.055393	64.293940
1684.655050	51.472497	64.298945
1684.350221	52.888260	64.303950
1682.911827	56.549811	64.308954
1682.346076	40.798568	64.313959
1681.908542	43.247767	64.318964
1681.553246	43.481005	64.323969
1680.013430	53.002573	64.328974
1679.125699	52.360077	64.333978
1679.179484	45.940137	64.338983
1678.449722	61.903871	64.343988
1678.202052	51.282133	64.348993
1676.830227	53.573843	64.353998
1676.242346	49.026672	64.359002
1675.809021	52.582172	64.364007
1675.268355	42.975189	64.369012
1674.805379	46.734084	64.374017
1673.689042	48.985208	64.379022
1673.106835	43.937269	64.384026
1672.321922	51.572812	64.389031
1671.752232	54.279540	64.394036
1671.893548	48.170530	64.399041
1670.562239	61.225879	64.404046
1669.689338	59.945548	64.409050
1669.448953	55.082987	64.414055
1668.155764	51.414230	64.419060
1667.689775	55.424330	64.424065
1666.767511	54.423066	64.429070
1666.784163	45.867627	64.434074
1666.488293	43.085901	64.439079
1665.426383	49.936013	64.444084
1664.672822	44.298740	64.449089
1663.789606	53.112060	64.454094
1663.323958	50.417227	64.459098
1662.050078	47.393502	64.464103
1661.216878	53.746835	64.469108
1660.930622	45.111793	64.474113
1660.247489	55.167444	64.479118
1659.938761	52.010886	64.484122
1659.767517	52.979673	64.489127
1659.305200	62.650182	64.494132
1658.436067	46.450424	64.499137
1657.399948	46.615218	64.504142
1656.836625	57.779303	64.509146
1655.943365	47.723740	64.514151
1654.820638	55.537531	64.519156
1654.262137	46.368604	64.524161
1653.707302	62.082210	64.529166
1653.543688	49.638445	64.534170
1653.492071	38.930383	64.539175
1652.061055	49.905903	64.544180
1651.576682	46.449262	64.549185
1650.678559	54.372443	64.554190
1649.621686	58.120048	64.559194
1648.773299	58.404823	64.564199
1648.419525	57.081447	64.569204
1647.994036	43.925546	64.574209
1647.723952	65.485125	64.579214
1647.025479	63.478532	64.584218
1646.300437	61.983917	64.589223
1645.169664	60.987403	64.594228
1645.050003	49.660971	64.599233
1644.302043	60.548480	64.604238
1643.299185	51.467497	64.609242
1642.828037	55.345962	64.614247
1642.138468	51.065680	64.619252
1641.785102	55.359074	64.624257
1640.745247	45.845601	64.629262
1639.856236	44.414885	64.634266
1639.592762	49.151290	64.639271
1639.178057	55.097534	64.644276
1638.227703	42.911232	64.649281
1637.408616	52.936448	64.654286
1636.671540	52.361490	64.659290
1636.304482	48.854676	64.664295
1635.582788	50.445480	64.669300
1634.710103	37.991389	64.674305
1633.976513	40.850312	64.679310
1633.615505	46.819560	64.684314
1632.997141	48.368717	64.689319
1632.205411	49.284707	64.694324
1631.263862	53.638438	64.699329
1630.644798	58.127005	64.704334
1630.237875	54.186576	64.709338
1630.233959	42.635191	64.714343
1628.929607	53.327261	64.719348
1628.048036	44.463550	64.724353
1627.308857	45.908907	64.729358
1627.054388	50.697496	64.734362
1626.622157	34.196551	64.739367
1625.507015	50.123741	64.744372
1624.629735	44.728478	64.749377
1624.556405	47.066206	64.754382
1623.931767	50.109663	64.759386
1622.931251	53.228610	64.764391
1621.797898	46.492690	64.769396
1621.730529	50.357463	64.774401
1621.061509	59.188802	64.779406
1620.600040	59.073082	64.784410
1619.551314	48.337372	64.789415
1618.713767	56.071174	64.794420
1618.350695	60.878599	64.799425
1617.973932	49.175149	64.804430
1616.847874	50.697747	64.809434
1616.351451	61.338726	64.814439
1615.479616	49.642977	64.819444
1615.505952	51.247391	64.824449
1614.612684	50.301460	64.829454
1613.501937	50.400863	64.834458
1613.216243	39.823033	64.839463
1612.618130	54.912759	64.844468
1611.771221	53.920042	64.849473
1611.022839	59.504590	64.854478
1610.262575	48.946967	64.859482
1609.848515	47.216881	64.864487
1609.105348	51.745668	64.869492
1608.776317	52.203390	64.874497
1607.763227	56.532228	64.879502
1607.149794	56.992563	64.884506
1606.757890	49.650009	64.889511
1605.421572	55.706424	64.894516
1604.689269	53.744643	64.899521
1604.298483	43.475233	64.904526
1603.583496	59.370395	64.909530
1603.331676	54.623196	64.914535
1602.407935	49.673694	64.919540
1601.966583	51.458070	64.924545
1601.402468	49.256689	64.929550
1600.737535	42.730191	64.934554
1600.278205	44.441733	64.939559
1598.920839	53.923313	64.944564
1598.619013	54.797740	64.949569
1597.782434	50.698517	64.954574
1597.059810	53.379100	64.959578
1596.348630	48.660741	64.964583
1595.268448	60.408407	64.969588
1595.083147	49.269023	64.974593
1594.554666	48.375519	64.979598
1594.335503	48.807901	64.984602
1593.874926	45.612407	64.989607
1592.820108	41.931047	64.994612
1592.229265	45.514738	64.999617
1590.976323	53.349241	65.004622
1590.321471	52.111559	65.009626
1589.693028	52.460748	65.014631
1589.099179	56.894856	65.019636
1588.804640	38.068226	65.024641
1588.350385	53.259666	65.029646
1587.602195	54.395822	65.034650
1586.681617	42.330964	65.039655
1586.018350	52.011326	65.044660
1585.609727	49.603900	65.049665
1584.537051	47.000809	65.054670
1583.467091	50.226993	65.059674
1583.357591	49.665865	65.064679
1582.591756	49.642668	65.069684
1582.253706	49.581458	65.074689
1581.219845	47.183502	65.079694
1580.184438	54.587647	65.084698
1579.870609	49.498663	65.089703
1579.279320	50.737616	65.094708
1579.208000	42.615614	65.099713
1577.900521	53.177320	65.104718
1576.960524	47.664313	65.109722
1576.722797	53.918316	65.114727
1576.473633	57.636944	65.119732
1575.924546	51.446839	65.124737
1574.826248	57.359796	65.129742
1573.884288	48.023180	65.134746
1573.293686	43.295131	65.139751
1572.706833	50.270050	65.144756
1571.712510	45.803263	65.149761
1570.966139	51.769101	65.154766
1570.478052	50.645267	65.159770
1570.387871	43.795647	65.164775
1569.708976	54.303201	65.169780
1569.268974	44.886825	65.174785
1568.268727	45.708242	65.179790
1567.742493	57.705340	65.184794
1567.221024	37.654854	65.189799
1565.865875	51.712182	65.194804
1565.265780	45.900754	65.199809
1565.020197	51.673480	65.204814
1564.115602	63.413755	65.209818
1563.758511	46.339511	65.214823
1562.458282	51.721614	65.219828
1562.172407	45.926483	65.224833
1561.534046	46.598937	65.229838
1561.057019	51.112251	65.234842
1560.297317	43.845502	65.239847
1559.244326	52.058230	65.244852
1558.851069	41.385547	65.249857
1558.582126	55.257659	65.254862
1557.424759	41.634647	65.259866
1556.906918	42.836702	65.264871
1556.003150	47.818355	65.269876
1555.933754	45.491063	65.274881
1555.429613	53.253894	65.279886
1554.305178	55.566276	65.284890
1553.517638	56.396473	65.289895
1552.766087	57.325025	65.294900
1552.570550	50.610411	65.299905
1551.717090	42.718354	65.304910
1550.715223	55.495897	65.309914
1550.328481	44.298656	65.314919
1549.788132	55.438600	65.319924
1549.068162	47.648325	65.324929
1548.207099	45.101504	65.329934
1547.320423	39.166899	65.334938
1547.031438	46.821424	65.339943
1546.460826	43.630812	65.344948
1546.160816	46.890765	65.349953
1545.335740	38.875937	65.354958
1544.322199	49.550206	65.359962
1543.962520	39.580208	65.364967
1542.771900	50.459229	65.369972
1542.304152	42.873292	65.374977
1541.844213	43.938422	65.379982
1541.009783	50.135869	65.384986
1540.516169	35.823948	65.389991
1539.238761	59.088918	65.394996
1538.834841	41.076005	65.400001
1538.580761	49.242198	65.405006
1537.783726	60.251059	65.410010
1537.894455	39.467790	65.415015
1536.604583	50.622769	65.420020
1536.092315	49.704624	65.425025
1534.664218	46.905738	65.430030
1533.418758	55.355633	65.435034
1533.761733	46.964379	65.440039
1532.860002	54.050843	65.445044
1532.344162	55.463888	65.450049
1532.330200	59.768007	65.455054
1531.544584	53.527197	65.460058
1530.944134	51.582330	65.465063
1530.274763	50.432123	65.470068
1528.819286	53.836283	65.475073
1527.992170	52.793143	65.480078
1527.125369	53.553946	65.485082
1527.085361	46.436172	65.490087
1526.349913	64.759831	65.495092
1526.123441	46.643026	65.500097
1525.726068	48.557612	65.505102
1524.926893	43.060095	65.510106
1524.183578	51.600492	65.515111
1523.310995	49.989020	65.520116
1522.732397	50.358687	65.525121
1521.568643	51.833703	65.530126
1520.779264	40.217938	65.535130
1520.812709	35.368655	65.540135
1520.310309	56.198763	65.545140
1519.537207	57.163863	65.550145
1518.519461	45.948646	65.555150
1517.805181	58.948564	65.560154
1517.811040	49.355691	65.565159
1516.530585	54.591178	65.570164
1515.872709	47.918511	65.575169
1515.093467	51.398125	65.580174
1514.238492	61.044319	65.585178
1514.295158	52.655987	65.590183
1513.282815	61.234416	65.595188
1512.372002	54.980396	65.600193
1511.953194	49.099172	65.605198
1511.560060	54.579976	65.610202
1511.098058	50.858050	65.615207
1509.849574	56.143650	65.620212
1509.189389	60.463743	65.625217
1508.790662	48.990884	65.630222
1508.144692	47.292943	65.635226
1507.464763	47.413803	65.640231
1506.313492	49.404055	65.645236
1506.182907	47.376636	65.650241
1505.569253	45.129538	65.655246
1504.732519	46.459551	65.660250
1503.891787	45.790725	65.665255
1503.102663	50.694253	65.670260
1503.014334	57.861178	65.675265
1502.380862	50.296856	65.680270
1501.541284	55.345592	65.685274
1501.208316	54.088314	65.690279
1500.008837	57.849177	65.695284
1499.513658	51.718331	65.700289
1498.422763	46.085846	65.705294
1497.763474	60.918817	65.710298
1497.479951	39.356163	65.715303
1496.797352	37.399133	65.720308
1496.565904	41.789848	65.725313
1495.857659	45.814818	65.730318
1495.032962	48.229388	65.735322
1494.668419	39.621018	65.740327
1493.352431	46.902632	65.745332
1492.495793	43.760648	65.750337
1492.196430	48.696719	65.755342
1491.540900	50.434731	65.760346
1491.006755	42.589716	65.765351
1489.735050	43.006474	65.770356
1489.279516	61.854896	65.775361
1489.006577	54.684261	65.780366
1488.129713	56.791750	65.785370
1488.311249	54.612226	65.790375
1486.938881	53.731449	65.795380
1485.959265	53.349617	65.800385
1485.630705	46.711349	65.805390
1485.041696	56.890833	65.810394
1484.367849	46.729517	65.815399
1483.272597	44.156867	65.820404
1482.710430	58.968093	65.825409
1482.157333	47.633313	65.830414
1481.891892	48.353743	65.835418
1481.303710	44.276584	65.840423
1480.183115	57.186551	65.845428
1479.662810	52.012136	65.850433
1479.216607	52.431730	65.855438
1478.039538	44.856051	65.860442
1477.661422	43.235388	65.865447
1476.927384	49.265515	65.870452
1476.478452	48.249011	65.875457
1475.892772	46.620339	65.880462
1474.663939	49.903354	65.885466
1474.492453	42.278232	65.890471
1473.730463	52.847889	65.895476
1473.277326	45.811552	65.900481
1472.702875	49.520389	65.905486
1471.399791	50.590238	65.910490
1471.255972	41.992519	65.915495
1470.609236	47.923620	65.920500
1469.499013	39.047443	65.925505
1468.859948	43.912934	65.930510
1468.342803	47.041834	65.935514
1467.914662	35.655670	65.940519
1467.329087	50.670872	65.945524
1466.245973	43.558060	65.950529
1466.075492	43.731991	65.955534
1465.037988	57.469229	65.960538
1464.671968	46.878967	65.965543
1463.359910	49.875608	65.970548
1462.917481	48.996838	65.975553
1462.387052	50.577786	65.980558
1461.999484	57.141023	65.985562
1461.551671	43.957191	65.990567
1460.322738	44.483854	65.995572
1459.443589	50.328903	66.000577
1459.457727	41.218825	66.005582
1458.533987	47.026808	66.010586
1457.468839	43.810751	66.015591
1456.973389	54.448427	66.020596
1456.336271	45.908618	66.025601
1456.151429	49.872481	66.030606
1455.543805	41.925621	66.035610
1454.850592	43.959775	66.040615
1454.005290	49.432034	66.045620
1453.148368	47.089583	66.050625
1452.973592	40.770638	66.055630
1451.725665	54.065108	66.060634
1451.006988	47.572429	66.065639
1450.642616	45.085460	66.070644
1450.042802	52.633286	66.075649
1448.900759	56.247853	66.080654
1448.077099	50.069891	66.085658
1447.692815	47.996073	66.090663
1447.259474	56.372106	66.095668
1446.736872	59.208581	66.100673
1446.577319	49.061719	66.105678
1445.298884	50.990213	66.110682
1444.660192	43.056178	66.115687
1444.166439	53.051798	66.120692
1443.385645	48.328786	66.125697
1442.801861	47.759480	66.130702
1441.676126	54.042679	66.135706
1441.527619	51.357403	66.140711
1440.876068	44.947095	66.145716
1439.762884	48.981255	66.150721
1439.197305	54.341251	66.155726
1438.332695	47.662049	66.160730
1438.402232	50.737121	66.165735
1437.529906	47.695416	66.170740
1436.379337	56.321067	66.175745
1436.111338	40.585668	66.180750
1435.120378	46.773330	66.185754
1435.221578	42.802634	66.190759
1434.165803	44.881811	66.195764
1433.373437	45.995070	66.200769
1432.922007	39.675952	66.205774
1432.374573	44.872221	66.210778
1431.353999	40.778657	66.215783
1430.605888	43.076997	66.220788
1430.156743	50.053701	66.225793
1429.803016	48.265174	66.230798
1428.676775	44.932691	66.235802
1427.824543	45.024194	66.240807
1427.165717	43.534888	66.245812
1426.553166	50.069236	66.250817
1426.666435	43.925268	66.255822
1425.348125	51.360240	66.260826
1424.744574	47.990401	66.265831
1423.974638	53.028087	66.270836
1423.869115	44.772775	66.275841
1423.231896	55.839823	66.280846
1421.847073	48.765530	66.285850
1421.527700	42.084817	66.290855
1420.877677	51.485568	66.295860
1420.305447	49.056875	66.300865
1419.341070	44.282635	66.305870
1418.551656	54.072957	66.310874
1418.184287	40.756513	66.315879
1417.662915	52.437470	66.320884
1417.179328	52.134501	66.325889
1416.336729	43.938014	66.330894
1415.394952	50.847958	66.335898
1415.209301	49.918917	66.340903
1414.368014	48.433389	66.345908
1413.169204	43.636498	66.350913
1412.905807	52.620995	66.355918
1412.088991	53.143667	66.360922
1412.036739	36.114062	66.365927
1411.125524	45.743979	66.370932
1409.885912	53.828734	66.375937
1409.641092	40.256281	66.380942
1408.652960	54.845077	66.385946
1408.422013	48.158192	66.390951
1407.786247	51.551952	66.395956
1406.683785	45.943426	66.400961
1406.439195	53.731243	66.405966
1405.830738	47.381900	66.410970
1405.579042	53.538784	66.415975
1404.109507	36.203077	66.420980
1403.349475	49.967173	66.425985
1403.435818	41.192535	66.430990
1402.774893	49.880698	66.435994
1401.919652	39.891749	66.440999
1401.540881	43.919555	66.446004
1400.462165	45.808437	66.451009
1399.674102	39.454537	66.456014
1398.799176	52.502079	66.461018
1398.042564	40.050148	66.466023
1397.739068	50.315129	66.471028
1397.206986	38.660094	66.476033
1396.187171	46.211618	66.481038
1395.282754	48.178444	66.486042
1395.038714	32.844511	66.491047
1394.784252	45.082243	66.496052
1394.167003	37.873335	66.501057
1393.259843	42.776729	66.506062
1392.489682	39.739300	66.511066
1392.200433	50.136051	66.516071
1391.032922	43.464026	66.521076
1389.682499	44.893084	66.526081
1389.608373	41.803348	66.531086
1389.209453	45.414911	66.536090
1388.944951	48.702347	66.541095
1388.008084	50.313230	66.546100
1386.970598	45.684661	66.551105
1386.651999	47.254022	66.556110
1385.910090	47.342193	66.561114
1385.725377	40.092906	66.566119
1384.775677	46.923696	66.571124
1384.202367	39.539079	66.576129
1383.355949	43.015214	66.581134
1382.160412	52.884299	66.586138
1381.703084	44.599770	66.591143
1381.301789	49.364405	66.596148
1380.775064	50.766593	66.601153
1379.738387	38.176278	66.606158
1378.729821	40.035092	66.611162
1378.348888	39.996495	66.616167
1377.824083	37.265400	66.621172
1377.217498	41.290003	66.626177
1377.279331	41.734497	66.631182
1375.919352	44.827103	66.636186
1375.258185	41.682470	66.641191
1374.772374	42.496288	66.646196
1374.168432	38.196173	66.651201
1373.074904	39.915541	66.656206
1372.303482	53.837567	66.661210
1371.837134	46.251451	66.666215
1371.726203	53.073472	66.671220
1370.737123	50.911325	66.676225
1369.957801	37.151061	66.681230
1369.112284	47.453330	66.686234
1368.860481	49.534019	66.691239
1368.062982	47.834975	66.696244
1367.103482	53.580867	66.701249
1366.541352	44.245463	66.706254
1365.646711	42.232299	66.711258
1365.567889	47.518071	66.716263
1365.252441	53.065381	66.721268
1363.872982	53.002618	66.726273
1363.257689	40.561348	66.731278
1362.667030	54.022574	66.736282
1362.325250	43.693401	66.741287
1361.638247	39.504261	66.746292
1360.631921	53.665474	66.751297
1360.314414	33.838108	66.756302
1359.730222	43.097517	66.761306
1358.392752	52.635956	66.766311
1358.114943	47.044572	66.771316
1357.452765	51.137941	66.776321
1357.143604	37.271397	66.781326
1356.230434	46.690338	66.786330
1355.477368	42.857037	66.791335
1355.169510	45.616808	66.796340
1354.052165	46.463231	66.801345
1353.067751	34.325071	66.806350
1352.301307	48.309377	66.811354
1351.981601	41.761189	66.816359
1351.639131	39.955117	66.821364
1351.265115	49.381377	66.826369
1350.631399	38.291267	66.831374
1349.277522	40.594481	66.836378
1348.813954	45.029992	66.841383
1348.579452	51.321330	66.846388
1347.069312	44.375813	66.851393
1346.607027	36.342809	66.856398
1345.926905	46.017998	66.861402
1345.229002	38.017725	66.866407
1345.035721	34.540106	66.871412
1344.684166	49.623757	66.876417
1343.841744	39.355267	66.881422
1342.920468	40.738194	66.886426
1342.453455	42.369001	66.891431
1342.099020	46.334601	66.896436
1340.760660	43.844820	66.901441
1340.362925	39.675924	66.906446
1339.165104	53.567982	66.911450
1339.193718	42.967048	66.916455
1338.122052	49.784130	66.921460
1337.253597	47.415171	66.926465
1336.958485	42.698552	66.931470
1336.398531	53.184075	66.936474
1335.695795	48.861831	66.941479
1335.117421	36.449396	66.946484
1334.384744	39.700890	66.951489
1334.022433	35.799162	66.956494
1333.045001	38.707969	66.961498
1332.476376	37.568606	66.966503
1332.136049	36.307793	66.971508
1331.084753	45.187336	66.976513
1330.227861	42.097489	66.981518
1329.282902	36.744646	66.986522
1328.370551	42.101446	66.991527
1328.335233	40.372691	66.996532
1327.808563	40.757798	67.001537
1327.738572	35.174379	67.006542
1326.570801	45.836960	67.011546
1325.396557	47.734753	67.016551
1325.096920	39.377864	67.021556
1324.801798	44.010511	67.026561
1324.042929	25.685143	67.031566
1323.059741	51.054218	67.036570
1322.589139	27.864098	67.041575
1321.906783	32.425855	67.046580
1320.830047	43.411411	67.051585
1320.151875	39.168843	67.056590
1319.584903	61.008953	67.061594
1319.301406	47.426896	67.066599
1319.043078	35.365682	67.071604
1317.890082	38.005958	67.076609
1317.117236	32.240999	67.081614
1316.564636	51.533744	67.086618
1315.834360	37.664786	67.091623
1314.989057	33.890320	67.096628
1313.919580	43.870258	67.101633
1313.668269	35.444192	67.106638
1313.213777	44.277729	67.111642
1312.875131	41.163830	67.116647
1312.384570	32.777384	67.121652
1311.306677	45.626987	67.126657
1310.842983	33.718273	67.131662
1309.791883	50.600405	67.136666
1309.300422	38.019625	67.141671
1308.679236	48.511730	67.146676
1308.037359	35.836604	67.151681
1307.267418	40.005461	67.156686
1306.477206	48.871883	67.161690
1305.589744	43.388487	67.166695
1305.486058	33.116089	67.171700
1304.572136	46.668136	67.176705
1303.942148	49.464941	67.181710
1303.050918	44.138254	67.186714
1302.674303	50.884253	67.191719
1302.436188	44.800892	67.196724
1301.498940	45.401092	67.201729
1300.761523	36.279657	67.206734
1299.885967	39.452959	67.211738
1299.287409	46.081290	67.216743
1299.278951	33.404794	67.221748
1297.967153	47.679240	67.226753
1297.644342	41.692922	67.231758
1296.496851	48.652955	67.236762
1295.590314	51.104250	67.241767
1294.697283	40.536339	67.246772
1294.020487	51.133479	67.251777
1293.656239	37.939573	67.256782
1293.506579	43.441599	67.261786
1293.411250	40.963913	67.266791
1292.949070	33.668883	67.271796
1291.493305	56.774622	67.276801
1291.260335	37.968259	67.281806
1289.676227	41.836098	67.286810
1289.248838	40.078230	67.291815
1288.380680	38.347875	67.296820
1287.719664	51.099663	67.301825
1287.698040	29.877055	67.306830
1287.252417	43.365674	67.311834
1286.009636	39.968218	67.316839
1285.645754	38.641775	67.321844
1284.949906	33.571021	67.326849
1284.206640	36.543529	67.331854
1283.154047	42.365744	67.336858
1282.423562	38.997208	67.341863
1282.256578	39.172172	67.346868
1281.499482	41.442020	67.351873
1281.225756	30.523344	67.356878
1279.774442	35.920132	67.361882
1279.047459	41.520268	67.366887
1279.254172	41.047637	67.371892
1278.551761	50.303782	67.376897
1277.672955	38.174095	67.381902
1276.617796	43.003293	67.386906
1276.463241	41.083777	67.391911
1275.855377	32.233473	67.396916
1274.432774	58.016197	67.401921
1274.171805	44.514147	67.406926
1273.403799	42.320040	67.411930
1272.971711	40.326391	67.416935
1272.440699	40.179218	67.421940
1271.108125	37.384221	67.426945
1270.788733	47.993910	67.431950
1270.444071	48.578732	67.436954
1269.855601	57.458816	67.441959
1269.293816	44.493433	67.446964
1267.875797	50.424226	67.451969
1267.928367	50.584777	67.456974
1267.219429	44.423336	67.461978
1266.277154	49.906336	67.466983
1265.264314	37.201912	67.471988
1264.693969	41.570840	67.476993
1264.753955	48.453980	67.481998
1264.375063	45.800626	67.487002
1263.214113	38.268234	67.492007
1262.650573	41.630038	67.497012
1261.484819	48.831096	67.502017
1260.548152	39.684592	67.507022
1259.773710	47.977690	67.512026
1259.279531	44.745037	67.517031
1258.979573	42.673612	67.522036
1258.836336	41.595921	67.527041
1258.665889	42.108888	67.532046
1257.394777	58.493046	67.537050
1256.592991	51.882771	67.542055
1255.790521	50.651308	67.547060
1254.386974	43.537524	67.552065
1254.232059	42.819639	67.557070
1253.747763	43.842962	67.562074
1252.929300	44.574093	67.567079
1252.894745	41.719334	67.572084
1251.711492	47.690067	67.577089
1250.958773	46.059631	67.582094
1250.780146	37.303489	67.587098
1249.795804	46.623395	67.592103
1249.042479	40.352333	67.597108
1248.061008	44.720416	67.602113
1247.632731	40.789772	67.607118
1247.281851	49.026552	67.612122
1246.760048	44.986208	67.617127
1246.136891	45.883389	67.622132
1245.033605	45.969149	67.627137
1245.043475	35.257676	67.632142
1244.079312	32.643791	67.637146
1242.699892	43.032568	67.642151
1242.393962	37.059347	67.647156
1241.930327	50.809445	67.652161
1241.746422	42.637583	67.657166
1240.537885	53.622055	67.662170
1239.621361	41.421114	67.667175
1239.361645	49.037880	67.672180
1238.784000	54.101798	67.677185
1237.904968	38.988728	67.682190
1237.015707	51.765783	67.687194
1236.509353	46.671212	67.692199
1236.401044	37.913351	67.697204
1234.982128	50.052433	67.702209
1234.388646	37.650321	67.707214
1233.894616	36.190052	67.712218
1233.206976	41.992089	67.717223
1232.971973	40.668811	67.722228
1231.782463	55.759580	67.727233
1230.915424	47.931313	67.732238
1230.734528	46.370784	67.737242
1230.061356	50.090634	67.742247
1229.665016	44.917071	67.747252
1228.833103	44.571770	67.752257
1228.121040	36.021888	67.757262
1227.636385	49.494646	67.762266
1226.290404	40.427446	67.767271
1225.942207	43.441213	67.772276
1225.019675	42.350274	67.777281
1224.699185	43.017985	67.782286
1224.449050	42.351515	67.787290
1223.376727	45.940891	67.792295
1222.743998	38.594158	67.797300
1221.853720	51.202653	67.802305
1221.462276	36.169736	67.807310
1220.382691	48.940793	67.812314
1219.362833	46.148125	67.817319
1219.343774	33.451250	67.822324
1219.032140	48.583738	67.827329
1218.546028	40.783202	67.832334
1218.051081	39.559612	67.837338
1217.020250	47.228056	67.842343
1216.701440	39.806169	67.847348
1215.338738	54.380467	67.852353
1214.778264	41.009643	67.857358
1214.397036	34.058131	67.862362
1213.293600	45.282920	67.867367
1212.452824	35.607132	67.872372
1211.554914	45.640237	67.877377
1211.335326	43.305314	67.882382
1210.803577	44.637374	67.887386
1210.382633	47.728941	67.892391
1209.971945	38.997098	67.897396
1208.858106	31.365789	67.902401
1208.229253	37.440738	67.907406
1207.806555	35.152312	67.912410
1206.859901	50.981854	67.917415
1206.036100	31.745975	67.922420
1205.337203	44.909046	67.927425
1204.861600	37.357567	67.932430
1204.578441	47.158867	67.937434
1203.590048	40.209310	67.942439
1202.932134	40.205331	67.947444
1202.090423	34.520749	67.952449
1201.808370	40.799150	67.957454
1200.499236	45.008063	67.962458
1199.606371	40.085358	67.967463
1199.723809	50.261316	67.972468
1199.063910	46.482631	67.977473
1198.999376	43.262078	67.982478
1197.936652	30.751702	67.987482
1196.961335	42.444945	67.992487
1196.463573	30.746681	67.997492
1195.095233	34.356340	68.002497
1194.663951	32.755219	68.007502
1194.528473	34.263938	68.012506
1193.372491	39.913403	68.017511
1193.494447	32.711563	68.022516
1192.369013	43.471527	68.027521
1191.663839	27.868818	68.032526
1191.018903	29.335571	68.037530
1190.337891	31.610686	68.042535
1190.036555	29.999937	68.047540
1188.847939	41.820142	68.052545
1188.382618	37.348231	68.057550
1187.991579	37.327038	68.062554
1187.031397	33.003219	68.067559
1186.309574	38.336064	68.072564
1185.400463	37.742874	68.077569
1184.910090	24.819794	68.082574
1184.816413	29.861927	68.087578
1184.112863	37.856770	68.092583
1183.378372	39.503340	68.097588
1182.540863	45.586256	68.102593
1181.887008	32.777477	68.107598
1180.637313	38.826608	68.112602
1179.912368	38.418580	68.117607
1179.398040	38.298734	68.122612
1179.061292	37.144601	68.127617
1178.863352	37.991511	68.132622
1178.057960	30.736911	68.137626
1177.058726	32.457129	68.142631
1176.754225	28.257671	68.147636
1176.269582	40.125171	68.152641
1174.906223	33.397689	68.157646
1174.237736	36.005113	68.162650
1173.474426	33.118048	68.167655
1173.505652	32.138764	68.172660
1172.398114	32.124312	68.177665
1171.557991	34.222902	68.182670
1170.999696	34.540535	68.187674
1170.656945	33.847804	68.192679
1170.491917	31.267679	68.197684
1169.256621	34.845151	68.202689
1168.364191	46.905246	68.207694
1167.857752	32.423622	68.212698
1167.261462	37.720736	68.217703
1166.890710	21.907164	68.222708
1165.749543	22.793724	68.227713
1165.449589	38.977687	68.232718
1165.158020	26.363594	68.237722
1163.411173	41.960890	68.242727
1162.753803	21.619997	68.247732
1162.146075	33.141238	68.252737
1161.911644	42.895363	68.257742
1161.672593	24.372285	68.262746
1160.926188	33.113496	68.267751
1159.981077	27.286116	68.272756
1159.347745	33.059027	68.277761
1158.937083	39.378386	68.282766
1157.767864	40.781893	68.287770
1156.802971	34.635978	68.292775
1156.459549	30.682398	68.297780
1156.098454	41.129991	68.302785
1155.869914	28.977356	68.307790
1155.198192	38.484086	68.312794
1153.898283	43.625058	68.317799
1153.386304	24.621875	68.322804
1153.033035	33.127098	68.327809
1151.678964	30.625732	68.332814
1151.257191	22.252050	68.337818
1150.626136	29.585694	68.342823
1150.378209	31.970116	68.347828
1149.385357	34.227040	68.352833
1148.644117	35.862078	68.357838
1148.236274	21.866232	68.362842
1147.564708	42.951862	68.367847
1147.024539	22.761057	68.372852
1145.806147	28.275392	68.377857
1145.371537	32.572287	68.382862
1144.776252	25.356817	68.387866
1144.188850	33.429378	68.392871
1143.193078	38.323290	68.397876
1142.295918	39.240428	68.402881
1141.858965	43.391050	68.407886
1141.541365	36.262285	68.412890
1140.951247	40.426232	68.417895
1140.497973	25.994512	68.422900
1139.272446	32.508142	68.427905
1138.871984	35.219587	68.432910
1138.475205	32.353073	68.437914
1137.578994	33.115529	68.442919
1136.745569	40.859821	68.447924
1135.916654	34.971390	68.452929
1135.536890	47.796719	68.457934
1135.330104	35.534972	68.462938
1134.019486	41.097102	68.467943
1133.408919	31.741103	68.472948
1132.967517	38.344458	68.477953
1132.316471	40.206414	68.482958
1132.031936	33.133890	68.487962
1130.943015	37.597947	68.492967
1130.495415	41.228321	68.497972
1129.876026	39.075271	68.502977
1128.997176	35.276250	68.507982
1128.277415	30.521572	68.512986
1127.543641	43.292831	68.517991
1127.000384	39.041477	68.522996
1125.939509	38.196498	68.528001
1125.400757	39.502881	68.533006
1125.096549	41.224514	68.538010
1124.671845	34.942222	68.543015
1124.001291	31.152644	68.548020
1122.225222	42.318890	68.553025
1121.976718	41.942314	68.558030
1122.057292	26.194144	68.563034
1121.303438	49.639248	68.568039
1120.630602	35.721820	68.573044
1119.532364	38.351892	68.578049
1119.086640	22.490342	68.583054
1118.731617	30.071801	68.588058
1117.189434	40.871277	68.593063
1117.066309	39.247955	68.598068
1116.539995	38.467744	68.603073
1115.870604	42.257976	68.608078
1115.114664	43.548452	68.613082
1114.223383	45.117488	68.618087
1114.016877	34.956087	68.623092
1113.136377	33.812776	68.628097
1111.990562	43.658273	68.633102
1111.402764	31.507607	68.638106
1110.768036	36.023989	68.643111
1110.481380	35.328650	68.648116
1110.321415	34.469662	68.653121
1109.297729	41.816898	68.658126
1108.489382	40.901793	68.663130
1107.914697	36.127195	68.668135
1107.457378	47.173542	68.673140
1106.094409	41.516729	68.678145
1105.292187	35.680831	68.683150
1104.862162	32.606735	68.688154
1104.583114	35.249986	68.693159
1104.306221	36.486332	68.698164
1103.212419	32.595368	68.703169
1102.542827	41.119383	68.708174
1102.384368	25.618966	68.713178
1101.040563	27.504408	68.718183
1100.091196	27.520016	68.723188
1099.516364	29.209013	68.728193
1099.065507	28.030471	68.733198
1098.889149	33.470512	68.738202
1097.895880	37.545647	68.743207
1096.957057	30.279193	68.748212
1096.489184	39.431823	68.753217
1096.174802	33.157218	68.758222
1095.687131	33.337483	68.763226
1094.655800	36.349560	68.768231
1094.106713	39.275456	68.773236
1093.304283	36.954429	68.778241
1092.352348	42.180410	68.783246
1091.816658	28.532903	68.788250
1091.005416	38.966960	68.793255
1090.649761	32.150173	68.798260
1090.208910	38.743984	68.803265
1089.215293	44.061749	68.808270
1088.370687	36.406590	68.813274
1087.726988	34.881858	68.818279
1087.165002	38.218216	68.823284
1086.882469	40.630225	68.828289
1086.453586	34.675018	68.833294
1085.519154	38.814910	68.838298
1084.638517	39.395145	68.843303
1084.447081	31.213475	68.848308
1083.306519	39.650003	68.853313
1082.477024	40.701469	68.858318
1082.078585	35.033140	68.863322
1081.628212	28.879517	68.868327
1080.985391	49.577407	68.873332
1080.170941	38.989211	68.878337
1079.356418	48.931818	68.883342
1078.784735	36.702906	68.888346
1077.595187	55.723275	68.893351
1077.107101	26.942903	68.898356
1076.530917	43.815750	68.903361
1075.861689	44.564192	68.908366
1075.897411	37.976858	68.913370
1075.023176	46.270103	68.918375
1074.105829	40.105620	68.923380
1073.470000	36.654288	68.928385
1072.922302	50.592797	68.933390
1072.188672	38.233542	68.938394
1071.407196	36.522589	68.943399
1070.741745	41.482237	68.948404
1070.364558	35.827874	68.953409
1069.256200	37.086127	68.958414
1068.838358	34.899452	68.963418
1067.844973	43.810862	68.968423
1067.908158	46.327133	68.973428
1067.119856	33.968698	68.978433
1065.815494	41.557711	68.983438
1065.414491	34.282969	68.988442
1064.601943	38.272596	68.993447
1064.422434	34.327643	68.998452
1063.653750	36.805963	69.003457
1062.628442	39.717752	69.008462
1062.410352	41.663796	69.013466
1061.720800	39.914567	69.018471
1061.208798	37.564688	69.023476
1060.342348	32.967405	69.028481
1059.608714	32.467760	69.033486
1059.243783	33.648734	69.038490
1057.837065	45.535225	69.043495
1057.128423	38.112321	69.048500
1056.493842	35.365654	69.053505
1056.194115	34.858471	69.058510
1056.327064	33.087185	69.063514
1055.285830	28.673823	69.068519
1054.430067	38.244542	69.073524
1053.490895	40.620688	69.078529
1052.955309	44.985700	69.083534
1052.183774	39.512348	69.088538
1051.535177	42.577081	69.093543
1050.684793	38.467649	69.098548
1050.394857	39.223554	69.103553
1050.105319	41.851134	69.108558
1049.116658	38.246224	69.113562
1048.253881	41.805480	69.118567
1047.681542	48.087502	69.123572
1047.362319	48.084865	69.128577
1046.377078	49.840752	69.133582
1045.615703	38.924023	69.138586
1045.048704	53.210941	69.143591
1044.549193	46.871183	69.148596
1043.810785	48.169929	69.153601
1042.492542	53.011114	69.158606
1042.251491	37.233696	69.163610
1041.889986	46.279530	69.168615
1041.372143	42.382102	69.173620
1040.447858	35.324658	69.178625
1039.645512	46.342332	69.183630
1039.449275	42.442617	69.188634
1038.326915	41.181705	69.193639
1037.278322	39.469112	69.198644
1036.965292	40.632371	69.203649
1036.139952	45.710503	69.208654
1035.913090	43.698437	69.213658
1035.671012	44.956057	69.218663
1034.802105	48.656635	69.223668
1034.226112	43.864918	69.228673
1033.044585	55.026506	69.233678
1032.026903	38.693033	69.238682
1031.375137	51.033395	69.243687
1030.727698	38.270958	69.248692
1030.160125	44.862865	69.253697
1030.195535	51.100225	69.258702
1030.029844	46.076075	69.263706
1028.806955	41.436174	69.268711
1027.994686	44.096472	69.273716
1027.342987	47.707300	69.278721
1026.346399	42.142040	69.283726
1026.023363	33.153465	69.288730
1025.109261	46.070122	69.293735
1024.856062	41.327966	69.298740
1024.185170	42.508746	69.303745
1023.230355	36.752349	69.308750
1022.777883	44.589011	69.313754
1021.726625	36.585160	69.318759
1020.604961	43.148546	69.323764
1020.125143	42.968050	69.328769
1019.630812	46.233737	69.333774
1019.573891	30.374998	69.338778
1018.755040	49.274891	69.343783
1018.363005	36.662621	69.348788
1017.759318	36.842439	69.353793
1016.546999	40.466784	69.358798
1016.138757	51.183650	69.363802
1015.222186	40.118174	69.368807
1014.182873	39.454305	69.373812
1014.164262	44.071357	69.378817
1013.271421	36.639934	69.383822
1013.248757	23.287698	69.388826
1012.267533	44.678058	69.393831
1011.623630	48.336533	69.398836
1011.127045	43.317733	69.403841
1009.522343	32.599869	69.408846
1008.791095	36.937676	69.413850
1008.190239	44.638686	69.418855
1007.885796	50.821320	69.423860
1007.313605	52.807946	69.428865
1007.086034	46.997329	69.433870
1006.274249	35.520970	69.438874
1005.538532	41.092597	69.443879
1004.848846	44.310528	69.448884
1004.406221	38.556211	69.453889
1002.918646	34.715338	69.458894
1002.361832	43.107891	69.463898
1002.073974	39.017769	69.468903
1001.729471	36.062541	69.473908
1001.152466	26.836861	69.478913
999.876232	39.125207	69.483918
999.200274	41.987737	69.488922
998.881671	47.399959	69.493927
998.228665	40.220520	69.498932
997.951845	41.054764	69.503937
996.774123	40.744069	69.508942
996.363708	48.041062	69.513946
995.647901	45.781972	69.518951
994.523103	46.290710	69.523956
993.894469	41.777025	69.528961
992.905926	46.031209	69.533966
992.978064	41.111138	69.538970
992.679099	45.845338	69.543975
991.743117	42.798162	69.548980
990.893245	32.299222	69.553985
989.796019	39.308134	69.558990
989.771753	48.789134	69.563994
989.201787	51.847678	69.568999
988.291826	52.678603	69.574004
987.728076	36.438495	69.579009
986.997864	45.565079	69.584014
986.236692	37.322707	69.589018
985.378116	38.211683	69.594023
984.830248	44.283250	69.599028
984.498184	41.091092	69.604033
983.741770	48.531451	69.609038
982.845672	30.887216	69.614042
982.309176	38.287843	69.619047
982.006607	41.716973	69.624052
981.303405	42.106589	69.629057
979.670992	42.390201	69.634062
979.689516	29.070832	69.639066
978.605805	42.932220	69.644071
978.421649	33.844289	69.649076
978.227143	29.930117	69.654081
976.946889	36.890893	69.659086
976.564598	34.425781	69.664090
975.866339	32.931838	69.669095
974.780137	30.835773	69.674100
973.871296	31.972435	69.679105
973.475169	41.211425	69.684110
973.281654	38.897610	69.689114
972.967857	38.356409	69.694119
971.933557	39.858370	69.699124
970.866036	39.172202	69.704129
970.203709	35.813422	69.709134
970.030703	32.099244	69.714138
968.819451	38.459297	69.719143
968.078376	46.892218	69.724148
967.805985	33.694831	69.729153
967.039765	45.626081	69.734158
966.848372	43.818101	69.739162
965.678773	35.934031	69.744167
964.776317	44.793157	69.749172
964.426794	40.318637	69.754177
964.046320	40.715244	69.759182
963.233497	28.732902	69.764186
962.083194	35.538970	69.769191
961.356276	36.175203	69.774196
961.466095	25.432096	69.779201
960.859584	38.927401	69.784206
960.270002	32.955224	69.789210
958.673103	33.578530	69.794215
958.596286	34.316297	69.799220
958.183678	28.424762	69.804225
957.075896	44.409291	69.809230
956.516111	28.542290	69.814234
955.721593	33.388467	69.819239
955.426512	42.247121	69.824244
954.931678	30.562663	69.829249
953.751076	41.361442	69.834254
953.296277	38.239283	69.839258
952.907855	45.163792	69.844263
951.543373	42.299938	69.849268
950.767390	37.027594	69.854273
950.016642	38.637393	69.859278
950.038985	35.595409	69.864282
949.540116	43.650760	69.869287
948.966859	47.006285	69.874292
948.033267	37.088355	69.879297
947.141635	38.375244	69.884302
946.980271	41.165350	69.889306
945.934626	37.293603	69.894311
945.174285	33.087885	69.899316
944.765209	30.557660	69.904321
944.015972	33.018726	69.909326
943.661427	28.819387	69.914330
943.102431	35.323210	69.919335
942.224418	38.268369	69.924340
941.509929	37.535490	69.929345
940.209980	35.315772	69.934350
939.978806	30.196411	69.939354
939.354217	40.947704	69.944359
938.905453	47.293649	69.949364
938.536395	38.534753	69.954369
937.093445	33.672898	69.959374
936.906631	26.228491	69.964378
936.258780	35.791376	69.969383
934.953069	44.850299	69.974388
934.323346	36.227502	69.979393
933.595375	41.774261	69.984398
933.671121	30.107803	69.989402
933.168805	34.823907	69.994407
932.039343	33.917393	69.999412
931.380134	28.594937	70.004417
930.567244	37.405121	70.009422
930.626852	32.267864	70.014426
929.839886	41.348299	70.019431
928.709006	35.835997	70.024436
928.109054	25.401387	70.029441
927.413403	37.017071	70.034446
926.575221	31.664755	70.039450
925.713181	42.699834	70.044455
924.831772	33.662963	70.049460
924.654620	30.758381	70.054465
924.134039	39.722307	70.059470
924.026869	36.436023	70.064474
923.721007	35.783185	70.069479
922.396123	40.094077	70.074484
921.790735	41.644481	70.079489
920.334370	40.081990	70.084494
919.917775	29.288633	70.089498
919.380745	28.606360	70.094503
918.584477	26.547750	70.099508
918.576378	28.230158	70.104513
917.938923	34.530442	70.109518
916.804620	46.092955	70.114522
916.099777	40.832952	70.119527
915.511373	39.551764	70.124532
915.066980	31.361501	70.129537
913.937167	32.451357	70.134542
913.492263	28.750502	70.139546
912.927986	32.940338	70.144551
912.427237	34.781578	70.149556
912.042876	23.372852	70.154561
910.795693	38.006128	70.159566
910.235346	30.080313	70.164570
909.880119	32.611132	70.169575
909.008437	26.907787	70.174580
908.346359	35.988845	70.179585
907.587813	38.033534	70.184590
907.338380	34.719436	70.189594
906.213019	25.454917	70.194599
905.513850	35.156854	70.199604
904.980607	36.851888	70.204609
904.618177	36.726844	70.209614
904.155051	35.971314	70.214618
902.760201	29.827722	70.219623
902.171248	33.173136	70.224628
902.183603	32.282005	70.229633
900.735772	36.022729	70.234638
899.986398	29.177194	70.239642
899.395778	26.418846	70.244647
898.846553	26.421299	70.249652
898.867891	36.628263	70.254657
898.164350	41.892037	70.259662
897.388050	36.331197	70.264666
896.954635	30.130768	70.269671
895.766685	34.292150	70.274676
894.882992	25.925828	70.279681
894.005455	39.123676	70.284686
893.884543	40.018265	70.289690
893.153524	36.304609	70.294695
892.542578	31.032826	70.299700
891.539925	23.811320	70.304705
890.687035	34.288312	70.309710
890.402486	38.520356	70.314714
890.186960	25.883193	70.319719
889.378180	41.190977	70.324724
888.628995	30.447413	70.329729
887.670719	30.152300	70.334734
887.491258	33.292197	70.339738
886.743470	31.566482	70.344743
885.371193	40.907238	70.349748
885.150797	22.073788	70.354753
884.728457	32.505902	70.359758
884.424717	32.480322	70.364762
883.578285	25.828429	70.369767
882.467659	36.538825	70.374772
882.291907	30.363615	70.379777
880.848761	33.504396	70.384782
880.064312	34.266498	70.389786
879.901501	34.428209	70.394791
878.995779	36.125770	70.399796
879.096395	32.440585	70.404801
877.969081	27.728789	70.409806
876.681639	28.484228	70.414810
876.431967	34.267082	70.419815
875.878396	27.409312	70.424820
875.660149	28.812952	70.429825
875.034596	37.147077	70.434830
874.110030	36.565922	70.439834
873.515878	33.155321	70.444839
872.644127	32.855902	70.449844
872.000103	34.611152	70.454849
871.210044	50.127267	70.459854
870.874002	39.800461	70.464858
870.541143	35.769560	70.469863
869.224291	25.609926	70.474868
868.683353	33.006541	70.479873
867.288796	40.562691	70.484878
867.343783	30.654592	70.489882
867.067678	33.283202	70.494887
865.663530	35.634084	70.499892
865.502250	32.268115	70.504897
864.664813	45.516359	70.509902
864.195854	37.751038	70.514906
863.595910	37.006256	70.519911
862.747734	46.782387	70.524916
862.033429	38.997776	70.529921
861.564306	43.844220	70.534926
860.857477	44.502514	70.539930
860.266731	43.431435	70.544935
859.178023	43.451968	70.549940
859.014431	36.191519	70.554945
857.851162	39.278302	70.559950
856.979048	44.622533	70.564954
856.778205	35.758038	70.569959
856.212663	29.871948	70.574964
855.968836	28.089674	70.579969
855.304730	43.103215	70.584974
854.501701	35.189239	70.589978
853.915049	26.720460	70.594983
852.613432	46.830980	70.599988
852.134150	41.185029	70.604993
851.831079	40.257382	70.609998
851.034905	39.278928	70.615002
849.545451	36.520178	70.620007
848.902786	33.913621	70.625012
848.665103	29.017647	70.630017
848.081198	37.420836	70.635022
847.834621	33.653733	70.640026
847.313204	37.535578	70.645031
846.238863	35.707326	70.650036
845.859802	28.910089	70.655041
845.095460	25.447747	70.660046
844.184836	32.456963	70.665050
843.446603	25.264346	70.670055
842.850168	37.867131	70.675060
842.601799	25.714572	70.680065
841.400069	41.598973	70.685070
840.716826	33.848851	70.690074
840.184735	21.837650	70.695079
839.591786	25.475430	70.700084
839.416590	25.954487	70.705089
838.308336	28.679301	70.710094
837.412586	31.744003	70.715098
837.126011	28.099957	70.720103
836.281812	35.806613	70.725108
835.963841	20.462538	70.730113
834.564207	31.282028	70.735118
834.204202	32.708238	70.740122
833.769800	29.548169	70.745127
833.225877	28.097505	70.750132
832.456274	16.663407	70.755137
831.419871	24.213010	70.760142
830.987125	34.610517	70.765146
830.655651	21.222321	70.770151
829.874218	33.909745	70.775156
829.157810	23.402253	70.780161
828.543202	31.529649	70.785166
828.001635	27.776396	70.790170
826.947581	25.077652	70.795175
826.360056	32.934248	70.800180
825.917672	23.384440	70.805185
825.454242	30.909062	70.810190
824.292348	27.412250	70.815194
823.341028	23.443549	70.820199
822.390642	27.948741	70.825204
822.414990	27.397881	70.830209
822.233253	36.585400	70.835214
821.518987	32.772913	70.840218
820.412453	34.349508	70.845223
819.858471	39.578451	70.850228
819.652905	29.314467	70.855233
818.239095	43.348293	70.860238
817.529799	36.975770	70.865242
816.911087	27.942860	70.870247
816.566658	39.176238	70.875252
816.246891	22.922603	70.880257
815.497101	27.299674	70.885262
814.537796	34.289843	70.890266
814.022897	26.020954	70.895271
812.868038	24.361646	70.900276
812.300397	21.937111	70.905281
811.306685	23.065265	70.910286
811.277880	35.140894	70.915290
810.537463	26.592536	70.920295
810.134376	37.833674	70.925300
809.590729	23.764943	70.930305
809.015776	27.500783	70.935310
807.823886	31.394763	70.940314
807.677370	27.988606	70.945319
806.405647	38.043472	70.950324
806.353839	29.417023	70.955329
805.167101	28.010360	70.960334
804.209870	31.967902	70.965338
803.774290	33.210617	70.970343
803.183662	27.401073	70.975348
803.135172	26.095455	70.980353
802.078844	30.841435	70.985358
800.669727	35.572624	70.990362
800.449407	27.955388	70.995367
799.731020	35.501683	71.000372
800.079057	25.974266	71.005377
799.070885	34.334626	71.010382
797.818070	28.207909	71.015386
797.454327	26.804257	71.020391
797.160234	33.447266	71.025396
796.024849	34.597982	71.030401
795.086298	39.979613	71.035406
794.550126	41.835975	71.040410
794.407808	28.389285	71.045415
792.907654	39.087616	71.050420
792.473388	30.987232	71.055425
792.072564	32.706934	71.060430
791.441527	33.886159	71.065434
791.281405	28.902156	71.070439
790.084741	40.268065	71.075444
789.308039	28.857183	71.080449
788.621198	29.430317	71.085454
788.314317	32.024412	71.090458
787.637748	30.621684	71.095463
786.788798	23.773125	71.100468
786.037444	25.829317	71.105473
785.477603	25.336775	71.110478
784.641671	30.880253	71.115482
783.765332	26.059165	71.120487
783.046420	37.002101	71.125492
782.863550	30.705043	71.130497
782.500328	21.167876	71.135502
781.872174	31.624878	71.140506
781.162877	28.015029	71.145511
780.307148	27.796665	71.150516
779.898846	32.262871	71.155521
778.510957	40.976994	71.160526
777.861708	38.988056	71.165530
777.567187	26.593717	71.170535
776.812105	39.314803	71.175540
776.607515	30.143436	71.180545
775.518747	22.640824	71.185550
774.674208	31.443464	71.190554
774.243018	29.880253	71.195559
773.744317	35.570304	71.200564
773.423509	38.333766	71.205569
772.448059	36.912400	71.210574
771.783446	36.028136	71.215578
770.901417	22.677155	71.220583
769.343586	50.807401	71.225588
769.189485	28.103269	71.230593
768.749628	27.356675	71.235598
768.286075	30.426698	71.240602
768.135607	29.372270	71.245607
767.129760	41.975601	71.250612
766.641279	33.453371	71.255617
765.791230	32.174459	71.260622
765.238824	37.824180	71.265626
764.544168	29.443584	71.270631
763.470036	30.769054	71.275636
762.956952	38.563350	71.280641
762.802085	28.138350	71.285646
761.539301	27.756160	71.290650
761.242780	29.557025	71.295655
760.435811	35.873291	71.300660
760.044298	29.801834	71.305665
758.870018	42.226994	71.310670
758.133522	42.987805	71.315674
758.067268	29.130065	71.320679
756.441661	26.888188	71.325684
756.010736	28.716760	71.330689
755.369669	30.539372	71.335694
755.091346	33.171498	71.340698
754.964985	22.765618	71.345703
754.313451	31.815058	71.350708
752.968542	31.341876	71.355713
752.634996	31.265868	71.360718
751.816076	34.789846	71.365722
750.964495	40.911382	71.370727
750.100818	43.154195	71.375732
749.578023	25.013868	71.380737
749.235029	29.393988	71.385742
748.593396	35.825849	71.390746
747.980257	34.876628	71.395751
746.626487	34.349670	71.400756
746.304805	28.662889	71.405761
745.958303	33.434631	71.410766
745.599251	35.010502	71.415770
744.979023	25.077474	71.420775
743.938513	32.462194	71.425780
743.103942	35.099319	71.430785
742.498596	26.081653	71.435790
741.605419	32.383265	71.440794
741.056711	22.706918	71.445799
740.663018	39.768323	71.450804
740.145200	27.718611	71.455809
739.270574	31.849091	71.460814
738.465242	45.757681	71.465818
737.984788	31.402957	71.470823
737.292571	35.584813	71.475828
736.505109	24.901026	71.480833
735.589638	36.660543	71.485838
734.864844	32.225325	71.490842
734.886683	23.114104	71.495847
734.035970	26.848139	71.500852
733.119878	34.638804	71.505857
732.409471	30.634933	71.510862
731.955444	31.798600	71.515866
731.654785	20.225221	71.520871
731.076317	16.217691	71.525876
729.877000	45.982820	71.530881
729.359264	31.403814	71.535886
728.582591	31.590747	71.540890
728.277422	33.031892	71.545895
727.101715	36.932792	71.550900
726.432382	25.033363	71.555905
726.090537	27.760756	71.560910
725.390244	39.336212	71.565914
725.067985	30.901062	71.570919
723.748140	33.610734	71.575924
723.189554	22.974082	71.580929
722.714312	36.588844	71.585934
722.364128	42.094416	71.590938
721.796354	25.646924	71.595943
720.460419	30.576222	71.600948
720.357395	31.748650	71.605953
719.600197	35.819439	71.610958
718.528862	38.385470	71.615962
718.166913	23.486797	71.620967
717.406393	36.311252	71.625972
717.010788	31.697472	71.630977
716.069047	32.875731	71.635982
715.102600	29.548112	71.640986
714.815016	34.001410	71.645991
714.180514	44.681778	71.650996
713.492519	42.651723	71.656001
712.367504	37.796147	71.661006
711.757656	38.279776	71.666010
711.549331	23.820237	71.671015
710.964200	37.443038	71.676020
710.599230	34.555771	71.681025
710.036524	29.011450	71.686030
708.793981	35.723500	71.691034
708.454262	37.766202	71.696039
706.921260	33.063904	71.701044
706.122696	29.605481	71.706049
705.902287	24.832928	71.711054
705.310241	35.397727	71.716058
705.153079	28.557302	71.721063
704.774407	40.286537	71.726068
704.004876	37.269741	71.731073
703.162386	41.177511	71.736078
702.387501	35.184460	71.741082
701.124655	24.655233	71.746087
700.591311	38.832727	71.751092
700.210534	29.098110	71.756097
699.723490	43.444843	71.761102
699.331405	29.875529	71.766106
698.438520	13.963929	71.771111
697.430837	36.301498	71.776116
696.862345	42.075211	71.781121
696.621915	34.353966	71.786126
695.559007	35.532606	71.791130
694.709626	31.457844	71.796135
694.310298	33.820680	71.801140
694.122086	29.635898	71.806145
693.397381	37.743007	71.811150
692.507395	34.767474	71.816154
691.976755	31.329463	71.821159
690.678916	41.897862	71.826164
690.037147	30.454497	71.831169
689.375719	29.065154	71.836174
688.701701	28.253370	71.841178
688.501196	26.672362	71.846183
688.083173	37.652547	71.851188
687.266309	28.788425	71.856193
686.540833	38.117721	71.861198
685.900751	36.483721	71.866202
684.798319	29.834832	71.871207
683.638088	34.297800	71.876212
683.217221	31.108800	71.881217
682.997623	33.799385	71.886222
682.567108	46.464074	71.891226
682.602006	28.659131	71.896231
681.276154	31.237325	71.901236
680.506579	33.425751	71.906241
680.244991	40.539803	71.911246
679.229452	35.515432	71.916250
678.447584	34.145272	71.921255
677.592210	40.549690	71.926260
677.436926	34.614083	71.931265
676.580219	34.414833	71.936270
675.181754	44.731200	71.941274
674.834693	30.891387	71.946279
674.480752	36.112147	71.951284
674.246389	36.528103	71.956289
673.511101	32.463562	71.961294
672.496875	37.860437	71.966298
671.990827	37.983789	71.971303
671.557677	32.492958	71.976308
670.663318	31.430858	71.981313
669.991236	24.130006	71.986318
669.368212	47.336682	71.991322
668.427728	32.317275	71.996327
667.285843	32.631772	72.001332
666.757152	32.560048	72.006337
666.453901	28.839841	72.011342
666.019119	38.182767	72.016346
665.937314	30.701179	72.021351
664.637509	40.927722	72.026356
663.595362	28.300838	72.031361
663.489227	33.018537	72.036366
662.719978	32.401688	72.041370
662.216110	28.044846	72.046375
661.013568	32.782628	72.051380
660.618010	18.486959	72.056385
660.437481	26.166800	72.061390
659.074342	35.009488	72.066394
658.642808	18.500911	72.071399
657.843148	29.474068	72.076404
657.505227	33.919618	72.081409
656.662434	23.930611	72.086414
655.452543	37.413236	72.091418
655.114931	32.768157	72.096423
654.510184	35.783419	72.101428
654.225344	28.876608	72.106433
653.951069	23.226449	72.111438
652.569762	35.031792	72.116442
652.168355	25.935948	72.121447
651.481017	35.725925	72.126452
650.718879	23.207412	72.131457
649.741651	30.766577	72.136462
648.979994	38.496403	72.141466
648.894955	32.231088	72.146471
648.412057	33.175455	72.151476
647.598291	36.017440	72.156481
647.023322	35.893170	72.161486
646.266571	41.146552	72.166490
645.783064	31.929749	72.171495
644.236162	34.577859	72.176500
643.673604	36.633983	72.181505
643.395151	44.747298	72.186510
642.735627	35.891244	72.191514
642.725153	28.866625	72.196519
641.597993	23.232465	72.201524
640.786257	41.557283	72.206529
640.462530	30.727139	72.211534
639.170518	39.385056	72.216538
638.509167	35.794422	72.221543
637.846100	34.810607	72.226548
637.425762	37.203604	72.231553
637.295218	34.547079	72.236558
636.355269	42.489800	72.241562
635.591228	42.849781	72.246567
635.009511	40.697173	72.251572
634.621452	33.653848	72.256577
633.305505	30.574305	72.261582
632.422334	36.376071	72.266586
631.973246	34.268568	72.271591
631.723952	31.528462	72.276596
631.257783	36.809676	72.281601
630.386296	32.326900	72.286606
629.592985	41.331144	72.291610
629.237057	33.713457	72.296615
628.218636	31.179427	72.301620
627.480025	32.533510	72.306625
626.981002	39.532425	72.311630
626.295494	39.346923	72.316634
625.857093	30.941331	72.321639
625.056107	40.519196	72.326644
624.126634	35.184694	72.331649
623.987677	34.199401	72.336654
622.930874	33.164769	72.341658
622.255862	26.971352	72.346663
621.256431	31.498615	72.351668
620.674336	36.178591	72.356673
620.632399	34.911356	72.361678
619.741693	34.995068	72.366682
619.045712	27.308555	72.371687
618.351499	28.045326	72.376692
617.874526	27.577468	72.381697
617.373588	31.366207	72.386702
616.306668	30.946587	72.391706
615.721906	29.838350	72.396711
615.166467	37.316154	72.401716
614.246494	30.021688	72.406721
613.468940	23.925028	72.411726
612.550010	36.025726	72.416730
612.289057	26.349313	72.421735
611.760217	31.763505	72.426740
611.703753	40.183637	72.431745
610.494236	26.588447	72.436750
609.856523	34.246501	72.441754
609.156514	36.439636	72.446759
608.750851	29.063254	72.451764
607.749018	18.889883	72.456769
607.004040	30.064062	72.461774
606.590778	44.072638	72.466778
605.975984	29.359338	72.471783
604.750909	41.882521	72.476788
603.962287	42.779405	72.481793
603.484648	31.070246	72.486798
603.229826	34.319923	72.491802
602.922621	24.486888	72.496807
601.813583	28.886545	72.501812
601.357555	34.986113	72.506817
600.801628	33.431766	72.511822
600.075752	41.608463	72.516826
599.408406	27.673044	72.521831
598.218590	23.844925	72.526836
597.734215	42.095529	72.531841
597.029082	39.823826	72.536846
596.656425	36.731235	72.541850
595.982366	31.761314	72.546855
595.092603	38.060851	72.551860
594.594532	32.706527	72.556865
594.281454	30.567907	72.561870
592.959197	33.954501	72.566874
592.488745	34.836974	72.571879
592.050570	32.423409	72.576884
591.752430	36.012703	72.581889
590.846912	31.713549	72.586894
589.607420	31.777140	72.591898
589.518652	34.921525	72.596903
589.180789	38.307426	72.601908
587.871826	43.814355	72.606913
587.385993	26.119187	72.611918
586.553714	35.388248	72.616922
586.113136	32.948259	72.621927
584.984385	25.521496	72.626932
584.160875	37.548658	72.631937
583.946818	28.391450	72.636942
583.174447	31.966405	72.641946
583.174713	24.703554	72.646951
582.152856	27.908268	72.651956
581.412503	34.753252	72.656961
581.006507	19.382277	72.661966
580.143550	30.822821	72.666970
579.556898	27.887318	72.671975
578.695032	37.687765	72.676980
578.065097	36.254015	72.681985
577.659126	20.860960	72.686990
576.567342	38.875601	72.691994
575.703142	28.825386	72.696999
575.597490	30.449217	72.702004
575.070654	28.117584	72.707009
573.926419	24.573934	72.712014
572.979014	38.323838	72.717018
572.890800	29.553414	72.722023
572.509598	38.279145	72.727028
571.600523	34.638113	72.732033
570.868313	35.396719	72.737038
570.081169	33.123897	72.742042
569.646457	30.506371	72.747047
568.773643	28.644565	72.752052
567.889664	32.618903	72.757057
567.414052	16.804891	72.762062
566.595028	33.289104	72.767066
566.461425	29.212326	72.772071
565.724624	24.645049	72.777076
564.522257	23.037581	72.782081
564.419869	23.427792	72.787086
563.784761	36.095107	72.792090
563.042710	23.485130	72.797095
562.097962	14.840125	72.802100
561.450342	29.229775	72.807105
561.220642	21.648768	72.812110
560.164998	31.937372	72.817114
559.655242	28.464532	72.822119
558.752965	26.981139	72.827124
558.227307	26.662966	72.832129
557.759919	9.532559	72.837134
556.744288	35.638517	72.842138
556.322620	20.716296	72.847143
555.711544	36.462534	72.852148
555.095180	26.954708	72.857153
554.272820	25.193674	72.862158
553.308609	28.881194	72.867162
553.061566	16.794728	72.872167
552.687419	24.773477	72.877172
551.688538	24.325701	72.882177
551.017012	15.862665	72.887182
550.272946	39.684660	72.892186
549.886684	24.135517	72.897191
548.737924	31.474473	72.902196
547.640227	35.391406	72.907201
547.623610	20.440929	72.912206
546.920133	22.223072	72.917210
546.561562	23.877733	72.922215
546.355465	29.863377	72.927220
545.162642	22.684949	72.932225
544.612998	21.825008	72.937230
543.985025	32.449161	72.942234
542.953666	25.861560	72.947239
542.165069	30.970236	72.952244
541.660216	27.567578	72.957249
541.280208	27.224628	72.962254
540.165156	32.886753	72.967258
539.259727	16.665016	72.972263
538.741471	26.194695	72.977268
538.224618	29.903986	72.982273
537.886886	24.662900	72.987278
537.260509	23.059872	72.992282
536.693538	18.930723	72.997287
535.839554	15.974750	73.002292
535.207291	18.374714	73.007297
535.223001	20.980512	73.012302
534.043184	27.515494	73.017306
533.533673	23.825017	73.022311
532.406259	24.906774	73.027316
531.354608	27.023494	73.032321
530.860292	17.575082	73.037326
530.446821	26.089920	73.042330
530.033939	28.787653	73.047335
529.626303	32.162598	73.052340
528.518978	32.424347	73.057345
528.103428	24.388860	73.062350
527.067618	35.820690	73.067354
526.382586	23.371945	73.072359
525.657458	18.705059	73.077364
524.967326	20.155519	73.082369
524.507726	27.133968	73.087374
523.957912	32.821157	73.092378
523.545006	19.569019	73.097383
522.508528	18.515426	73.102388
521.888347	29.808500	73.107393
521.671998	15.657782	73.112398
520.717697	28.095268	73.117402
519.404121	28.055587	73.122407
519.146661	26.923612	73.127412
518.484823	18.816989	73.132417
518.411552	20.725802	73.137422
517.173572	25.680588	73.142426
516.435317	28.658805	73.147431
515.884506	27.283426	73.152436
515.549999	29.561846	73.157441
515.117938	21.965782	73.162446
514.055785	30.347444	73.167450
513.390197	21.803053	73.172455
512.929643	26.592984	73.177460
511.930527	23.258043	73.182465
511.397562	8.421387	73.187470
510.619305	16.623779	73.192474
510.139751	18.187340	73.197479
509.553754	24.583570	73.202484
508.573543	17.281411	73.207489
507.941167	17.585762	73.212494
507.347124	23.869741	73.217498
506.923144	18.853702	73.222503
506.018248	24.343591	73.227508
504.928906	30.916207	73.232513
504.842381	20.891930	73.237518
504.383852	21.425611	73.242522
503.885379	17.197255	73.247527
502.758020	17.345520	73.252532
502.183863	31.720320	73.257537
501.424393	18.928657	73.262542
500.364076	34.547788	73.267546
499.756739	25.303457	73.272551
499.320336	32.989377	73.277556
498.553662	28.674447	73.282561
498.451553	17.634009	73.287566
497.922411	24.186751	73.292570
496.756955	19.315659	73.297575
496.150769	18.206135	73.302580
495.464997	32.989779	73.307585
495.123008	12.195305	73.312590
494.191318	22.684932	73.317594
493.473879	26.341039	73.322599
493.208857	18.265812	73.327604
492.131673	29.978612	73.332609
491.591220	14.293226	73.337614
490.814097	19.721762	73.342618
490.436622	16.992639	73.347623
489.725745	21.822454	73.352628
488.523944	30.251605	73.357633
487.952376	14.930700	73.362638
487.817173	22.023034	73.367642
487.581440	20.086560	73.372647
486.419537	24.748558	73.377652
485.515760	26.291413	73.382657
485.053873	22.161302	73.387662
483.592275	19.082978	73.392666
483.266222	28.381780	73.397671
482.572165	17.637498	73.402676
482.072072	32.000499	73.407681
481.631553	22.608178	73.412686
481.122999	17.772768	73.417690
480.871559	28.568729	73.422695
479.808019	22.222817	73.427700
479.197310	23.157618	73.432705
478.903526	30.380872	73.437710
477.518136	32.631210	73.442714
476.892149	23.479740	73.447719
476.568389	23.170413	73.452724
475.340380	35.772946	73.457729
474.599014	21.649121	73.462734
473.895195	22.072091	73.467738
473.673592	30.783431	73.472743
473.369875	28.443077	73.477748
472.808473	22.449217	73.482753
471.989113	34.157213	73.487758
471.203061	26.193389	73.492762
470.430909	19.343766	73.497767
470.075305	25.435228	73.502772
468.606655	18.515247	73.507777
468.356402	15.232881	73.512782
467.745981	33.052577	73.517786
467.249398	28.633125	73.522791
466.287859	21.837333	73.527796
465.677200	28.950238	73.532801
465.612671	20.120871	73.537806
464.342198	25.792018	73.542810
463.770114	24.959325	73.547815
463.075844	24.545044	73.552820
462.478265	27.869843	73.557825
462.317172	13.886944	73.562830
461.028713	38.238780	73.567834
460.028675	22.115729	73.572839
459.494863	16.273587	73.577844
459.215624	18.762388	73.582849
459.111761	25.204796	73.587854
457.864995	33.223259	73.592858
456.911971	23.482128	73.597863
456.742826	29.099209	73.602868
455.963039	37.639315	73.607873
455.184909	22.742390	73.612878
454.479817	25.248590	73.617882
453.618761	27.653494	73.622887
453.726488	22.577972	73.627892
452.657256	17.798797	73.632897
451.958967	26.026309	73.637902
451.471733	26.001638	73.642906
450.518985	22.068016	73.647911
449.968799	12.772029	73.652916
449.094345	15.820846	73.657921
448.836870	27.231163	73.662926
448.184489	17.643971	73.667930
447.111160	17.909800	73.672935
446.443864	22.316392	73.677940
445.669384	25.369781	73.682945
445.608580	19.531112	73.687950
444.986521	20.664837	73.692954
443.743271	21.093353	73.697959
443.354350	14.980563	73.702964
442.273977	21.053483	73.707969
442.345712	12.629737	73.712974
441.005502	14.721514	73.717978
440.229208	25.495458	73.722983
440.022593	17.737344	73.727988
439.693487	17.047276	73.732993
439.398468	23.808707	73.737998
438.157612	15.765999	73.743002
437.280385	19.439695	73.748007
436.780783	13.612609	73.753012
435.977157	26.439240	73.758017
435.348506	11.773966	73.763022
434.552224	17.180338	73.768026
433.859002	16.641328	73.773031
433.885376	15.383714	73.778036
432.695302	33.891832	73.783041
432.016923	17.034768	73.788046
431.589110	20.657351	73.793050
430.931621	16.478005	73.798055
429.740176	23.562047	73.803060
428.857747	25.352239	73.808065
428.587925	21.057504	73.813070
428.357276	20.195639	73.818074
427.576117	19.986014	73.823079
427.346773	20.844287	73.828084
426.377625	23.556565	73.833089
425.623070	29.836178	73.838094
425.049623	22.704187	73.843098
423.757490	29.774320	73.848103
423.415519	30.171179	73.853108
422.981564	36.986295	73.858113
422.693150	23.947720	73.863118
421.453741	23.796930	73.868122
420.459376	32.774911	73.873127
419.912701	15.890559	73.878132
419.595940	31.039577	73.883137
419.376060	27.427544	73.888142
417.876204	23.093875	73.893146
417.310572	25.100075	73.898151
417.270868	30.398503	73.903156
416.323232	26.479849	73.908161
415.290809	27.936003	73.913166
414.521307	22.490954	73.918170
414.264303	27.131773	73.923175
414.270314	19.792334	73.928180
412.956959	25.938663	73.933185
412.335995	24.415226	73.938190
411.518316	26.751734	73.943194
410.939486	25.406075	73.948199
410.822437	21.110648	73.953204
409.256254	30.025225	73.958209
409.004423	20.688007	73.963214
408.205075	35.901322	73.968218
407.743934	22.436145	73.973223
407.066019	14.920292	73.978228
405.910150	31.201180	73.983233
405.496074	26.445341	73.988238
405.213312	20.903805	73.993242
404.445957	22.142691	73.998247
403.845527	12.954067	74.003252
402.853696	24.445143	74.008257
402.804196	28.592453	74.013262
401.802920	21.173860	74.018266
400.940926	24.285360	74.023271
400.770741	24.200711	74.028276
399.738329	29.517003	74.033281
399.119480	23.652160	74.038286
398.329847	31.619871	74.043290
397.611357	36.422543	74.048295
397.516325	23.402039	74.053300
396.235178	26.539342	74.058305
395.636832	24.096154	74.063310
395.142176	25.785138	74.068314
394.595365	19.114085	74.073319
394.205650	23.041241	74.078324
392.988159	28.241960	74.083329
392.469879	27.585201	74.088334
392.209770	19.764660	74.093338
390.928968	22.457238	74.098343
390.429369	20.586481	74.103348
389.542652	23.116912	74.108353
389.202668	16.945875	74.113358
388.791146	24.399191	74.118362
387.679547	32.919656	74.123367
387.089397	23.040309	74.128372
386.353012	32.894913	74.133377
386.023030	32.504593	74.138382
385.140818	31.945257	74.143386
384.118825	33.967429	74.148391
383.584350	29.596612	74.153396
383.091655	36.998222	74.158401
383.054614	25.969502	74.163406
381.918982	22.979630	74.168410
381.118229	27.029064	74.173415
380.298380	20.638057	74.178420
379.914877	22.601045	74.183425
379.667956	24.371967	74.188430
378.688617	25.824406	74.193434
377.821127	27.646926	74.198439
377.501804	24.675180	74.203444
377.076342	31.154652	74.208449
375.982092	23.380328	74.213454
375.161574	24.205099	74.218458
374.634814	37.735053	74.223463
374.151815	13.266954	74.228468
372.811387	29.039558	74.233473
372.309251	18.810323	74.238478
371.906047	24.816343	74.243482
371.173373	24.253679	74.248487
371.326912	16.119652	74.253492
369.817318	39.674180	74.258497
369.224636	27.600262	74.263502
368.892946	31.092425	74.268506
368.124098	22.607119	74.273511
367.537603	15.937670	74.278516
366.620975	17.260278	74.283521
366.182581	22.466136	74.288526
365.299393	17.435016	74.293530
364.087006	27.608320	74.298535
364.201406	19.701289	74.303540
363.436504	31.118369	74.308545
363.135256	20.500748	74.313550
362.664758	18.994342	74.318554
361.539925	13.443534	74.323559
361.079885	26.863503	74.328564
359.662769	27.368655	74.333569
359.171900	27.215280	74.338574
358.510183	18.916319	74.343578
357.751372	23.615043	74.348583
357.764422	22.835762	74.353588
357.463241	26.903343	74.358593
356.488171	28.288884	74.363598
355.652388	19.204012	74.368602
354.765125	20.454140	74.373607
353.964235	20.039539	74.378612
353.226172	32.713824	74.383617
353.104386	15.988845	74.388622
352.318899	21.779848	74.393626
351.274898	16.928897	74.398631
350.639433	11.978142	74.403636
349.931090	15.331653	74.408641
349.585885	22.149969	74.413646
349.207726	17.380538	74.418650
347.999693	23.640988	74.423655
347.557724	24.514235	74.428660
346.479014	26.786719	74.433665
346.301537	31.703431	74.438670
345.896925	23.967426	74.443674
344.897842	26.186221	74.448679
344.088275	21.783575	74.453684
343.537389	24.069696	74.458689
343.112267	15.435007	74.463694
342.367429	22.471553	74.468698
341.357598	29.942975	74.473703
341.186524	26.400438	74.478708
340.479847	32.227769	74.483713
339.596997	26.945883	74.488718
339.045126	29.522303	74.493722
338.054756	35.841103	74.498727
337.586397	22.618359	74.503732
337.045245	26.191216	74.508737
335.793685	22.294234	74.513742
335.395438	24.647484	74.518746
334.703938	38.282541	74.523751
334.523636	29.050618	74.528756
334.120024	28.465475	74.533761
333.243574	23.393871	74.538766
332.554113	26.574080	74.543770
331.725081	23.484903	74.548775
331.546691	21.203438	74.553780
330.426616	30.989907	74.558785
329.658366	24.401473	74.563790
329.321728	9.705468	74.568794
327.695809	25.704929	74.573799
327.301137	18.987570	74.578804
326.466502	25.667874	74.583809
326.451536	23.048144	74.588814
326.195467	26.529833	74.593818
325.539672	18.121138	74.598823
324.398278	11.081291	74.603828
323.705150	24.808053	74.608833
323.212207	25.539629	74.613838
322.727820	17.001118	74.618842
321.747467	32.930802	74.623847
321.112245	17.987514	74.628852
320.803816	28.242236	74.633857
319.986489	14.909560	74.638862
318.866680	25.672056	74.643866
318.052260	27.635937	74.648871
318.031418	17.929205	74.653876
317.416064	22.113095	74.658881
316.681526	27.293631	74.663886
316.044929	18.161259	74.668890
315.036484	22.606492	74.673895
314.619219	15.738207	74.678900
313.150968	15.754829	74.683905
312.894704	15.881014	74.688910
312.527925	16.171462	74.693914
311.855168	13.886807	74.698919
311.665592	19.984927	74.703924
310.694392	17.249560	74.708929
309.746021	14.374946	74.713934
309.509316	20.546807	74.718938
308.787424	32.463210	74.723943
308.390161	14.998460	74.728948
307.535840	23.397518	74.733953
306.735410	22.719525	74.738958
305.886484	25.420568	74.743962
304.798785	17.228953	74.748967
304.862083	11.648043	74.753972
304.003543	21.553663	74.758977
303.049939	18.071221	74.763982
302.799430	10.737996	74.768986
301.999586	19.054257	74.773991
301.622144	22.017589	74.778996
300.152535	25.541349	74.784001
299.623555	20.742355	74.789006
299.280154	18.875102	74.794010
298.618832	27.654957	74.799015
298.385117	20.716416	74.804020
297.714544	18.923394	74.809025
296.276592	21.283125	74.814030
296.145879	14.481122	74.819034
295.246140	24.170978	74.824039
295.100262	19.441795	74.829044
293.720977	28.883268	74.834049
292.994905	17.746799	74.839054
293.214984	20.578614	74.844058
292.291074	20.188375	74.849063
291.434210	14.150214	74.854068
290.290186	17.693034	74.859073
289.689996	24.922562	74.864078
289.583988	20.054569	74.869082
288.936195	13.328689	74.874087
288.471828	9.083914	74.879092
287.909529	17.947320	74.884097
286.973546	24.837743	74.889102
286.120401	19.365079	74.894106
284.836411	23.526264	74.899111
284.725542	16.191277	74.904116
284.164759	19.090804	74.909121
283.823195	19.419811	74.914126
282.720005	23.910120	74.919130
281.835334	21.976202	74.924135
281.416067	14.613114	74.929140
281.147755	23.249898	74.934145
280.351582	26.202720	74.939150
279.260485	22.251806	74.944154
278.675646	14.907230	74.949159
278.290937	19.144239	74.954164
277.647880	31.150574	74.959169
276.743433	17.423401	74.964174
275.947152	21.809596	74.969178
275.561427	37.434780	74.974183
275.280827	14.290552	74.979188
274.659162	22.190512	74.984193
273.389952	21.342851	74.989198
272.977238	11.469956	74.994202
272.402566	18.274398	74.999207
271.635085	22.102528	75.004212
270.626771	26.863127	75.009217
269.877050	28.389383	75.014222
269.683847	24.088764	75.019226
269.154528	27.369607	75.024231
268.581748	19.036002	75.029236
267.507187	24.608202	75.034241
266.994033	14.475370	75.039246
266.685672	27.273536	75.044250
265.423807	22.791648	75.049255
264.809335	16.173997	75.054260
264.281592	19.553929	75.059265
263.531248	28.228142	75.064270
263.417190	20.833744	75.069274
262.380340	22.202362	75.074279
261.910055	24.609682	75.079284
261.424815	20.167977	75.084289
260.165609	17.880643	75.089294
259.776762	17.403538	75.094298
259.024295	21.954629	75.099303
258.440727	16.509959	75.104308
257.436110	17.051902	75.109313
256.707743	18.305115	75.114318
256.160129	6.350220	75.119322
255.518234	15.530650	75.124327
255.856811	18.231612	75.129332
254.693910	18.877633	75.134337
253.652915	22.941750	75.139342
253.351833	16.151145	75.144346
252.743921	23.041311	75.149351
251.674697	17.033868	75.154356
250.876530	23.277897	75.159361
250.414216	14.898306	75.164366
250.012673	20.177145	75.169370
248.640578	24.355547	75.174375
248.171150	4.637982	75.179380
247.287023	35.426745	75.184385
247.179287	14.788965	75.189390
247.052505	13.172596	75.194394
246.141393	18.471178	75.199399
245.307498	10.053067	75.204404
244.688443	25.275497	75.209409
243.880997	23.513772	75.214414
242.785971	17.370107	75.219418
241.994113	26.430962	75.224423
241.637242	13.237790	75.229428
241.426204	8.977867	75.234433
240.744487	25.739830	75.239438
240.171115	24.639332	75.244442
239.155748	13.405519	75.249447
239.006430	20.131114	75.254452
238.416400	24.612161	75.259457
236.976665	28.195845	75.264462
236.585054	1.277030	75.269466
235.571702	33.746811	75.274471
235.431108	13.737131	75.279476
234.527029	23.252663	75.284481
233.707980	35.477865	75.289486
233.401130	11.683450	75.294490
232.832099	20.035463	75.299495
232.256891	26.687046	75.304500
231.381086	29.045492	75.309505
230.649484	21.896203	75.314510
230.066740	16.624863	75.319514
228.667392	35.368241	75.324519
228.328512	31.849316	75.329524
227.923493	20.369969	75.334529
227.193588	25.429947	75.339534
227.263200	22.522364	75.344538
225.709801	21.500857	75.349543
224.978298	26.543746	75.354548
225.016388	30.830041	75.359553
224.210072	26.310234	75.364558
223.896257	30.313614	75.369562
222.959010	17.679724	75.374567
221.840308	13.257035	75.379572
221.618811	27.351710	75.384577
220.426731	32.103784	75.389582
220.004987	11.587040	75.394586
219.322623	19.660678	75.399591
219.186445	36.009265	75.404596
218.401329	17.860534	75.409601
217.362907	30.753028	75.414606
217.229251	16.243869	75.419610
216.522345	35.712578	75.424615
215.165204	27.595502	75.429620
214.585283	23.067986	75.434625
213.848046	20.913481	75.439630
213.707609	33.889868	75.444634
212.820647	31.216798	75.449639
211.827098	26.578625	75.454644
211.246563	21.773684	75.459649
210.676360	12.381626	75.464654
210.725911	27.565260	75.469658
209.599657	38.429748	75.474663
208.990305	25.682081	75.479668
208.396372	14.158754	75.484673
207.563599	36.361287	75.489678
206.791661	15.559780	75.494682
205.930979	24.757763	75.499687
205.394352	11.230590	75.504692
204.935921	25.481304	75.509697
204.331335	23.982119	75.514702
203.853684	25.572238	75.519706
202.766114	30.761788	75.524711
202.390542	31.321719	75.529716
201.510061	30.003710	75.534721
200.452903	24.784367	75.539726
199.613596	11.489948	75.544730
199.029814	39.955442	75.549735
199.175971	27.967195	75.554740
198.768892	29.580754	75.559745
198.088474	13.979300	75.564750
197.302504	25.585833	75.569754
196.950550	35.855385	75.574759
195.768308	24.810610	75.579764
194.863148	22.856340	75.584769
194.109410	24.980883	75.589774
193.974385	26.101661	75.594778
192.779465	30.620826	75.599783
192.147748	21.156581	75.604788
191.618084	6.997567	75.609793
190.772771	29.925863	75.614798
190.720215	24.073286	75.619802
189.242350	34.607515	75.624807
188.825870	32.077040	75.629812
188.437614	26.109268	75.634817
187.885091	28.176499	75.639822
187.596597	25.893682	75.644826
186.418191	23.912026	75.649831
185.766122	29.356970	75.654836
185.168289	33.735203	75.659841
184.315250	32.794422	75.664846
183.732690	5.439325	75.669850
183.014046	28.216543	75.674855
182.562287	27.558683	75.679860
181.882855	24.111417	75.684865
180.600427	24.987830	75.689870
180.246992	24.052536	75.694874
179.592911	25.219814	75.699879
179.659681	22.894541	75.704884
178.707521	22.281784	75.709889
177.685703	26.462713	75.714894
177.169455	26.471107	75.719898
176.743410	24.976573	75.724903
175.871515	25.656648	75.729908
175.325962	22.156499	75.734913
174.445681	28.185001	75.739918
174.011295	15.996044	75.744922
172.974092	23.883440	75.749927
172.434402	22.577328	75.754932
172.404776	20.082936	75.759937
171.224311	22.657128	75.764942
170.232714	17.998166	75.769946
169.575081	23.395117	75.774951
169.128633	25.819150	75.779956
168.999862	26.104780	75.784961
167.794364	26.107974	75.789966
167.062051	23.034973	75.794970
166.251445	23.101346	75.799975
165.708354	22.074880	75.804980
165.791739	25.281691	75.809985
164.537278	22.112194	75.814990
163.912275	14.969588	75.819994
163.297574	22.940991	75.824999
162.495547	30.929655	75.830004
161.947582	22.568473	75.835009
160.899880	36.679793	75.840014
160.467037	25.906596	75.845018
159.994143	31.589462	75.850023
159.526874	23.838267	75.855028
159.023682	27.517059	75.860033
157.719881	32.859372	75.865038
157.256973	24.656503	75.870042
156.770281	34.062930	75.875047
156.353366	17.607394	75.880052
155.237905	27.565062	75.885057
154.649216	25.669143	75.890062
154.308657	24.987249	75.895066
153.065289	23.604133	75.900071
152.321355	32.121241	75.905076
152.232803	29.235726	75.910081
151.198076	36.088329	75.915086
151.388742	27.841156	75.920090
150.063344	40.222813	75.925095
149.351062	20.465153	75.930100
148.700803	22.216839	75.935105
147.914780	35.576852	75.940110
147.693187	18.057336	75.945114
146.268587	17.414283	75.950119
145.642393	23.266663	75.955124
145.485182	24.911342	75.960129
144.918091	30.896217	75.965134
144.491559	25.385536	75.970138
143.408837	23.972077	75.975143
142.689545	14.892379	75.980148
142.204778	19.006597	75.985153
141.581642	28.854222	75.990158
140.700274	19.674220	75.995162
139.982302	25.814033	76.000167
139.427393	18.291274	76.005172
139.139830	19.676061	76.010177
138.546079	30.472993	76.015182
137.819802	18.504048	76.020186
136.869375	15.727599	76.025191
136.084673	22.278572	76.030196
135.010276	14.499639	76.035201
134.355154	27.413022	76.040206
134.162280	21.693207	76.045210
133.676500	32.304200	76.050215
133.207126	36.485351	76.055220
132.571270	14.079030	76.060225
131.193426	18.999526	76.065230
131.506698	20.249074	76.070234
130.238689	19.680399	76.075239
128.980681	21.172645	76.080244
128.984814	12.993073	76.085249
128.212876	15.014887	76.090254
128.102343	20.892260	76.095258
127.306469	26.024280	76.100263
126.408048	24.404830	76.105268
126.011212	31.721799	76.110273
124.950924	29.713451	76.115278
124.295080	13.089470	76.120282
123.751624	16.566543	76.125287
123.164910	19.263670	76.130292
121.866489	16.993703	76.135297
121.110881	31.184594	76.140302
121.034479	22.204208	76.145306
120.423590	21.016689	76.150311
119.865809	26.571180	76.155316
119.281360	24.633595	76.160321
118.192500	24.241346	76.165326
117.867503	21.004062	76.170330
117.212865	32.083503	76.175335
116.285364	26.731567	76.180340
115.633319	30.210194	76.185345
114.779880	45.301313	76.190350
114.685604	21.651210	76.195354
113.946884	20.141905	76.200359
112.754008	28.807883	76.205364
112.636499	20.710782	76.210369
111.326221	51.304211	76.215374
111.459219	13.673805	76.220378
110.172561	19.549529	76.225383
109.483278	18.089107	76.230388
109.076064	30.154037	76.235393
108.586714	31.575740	76.240398
108.140220	24.559210	76.245402
107.066652	30.612252	76.250407
106.305236	11.974139	76.255412
106.163130	27.645605	76.260417
105.642020	28.082114	76.265422
104.611082	18.697342	76.270426
103.915762	30.112832	76.275431
103.212851	26.018097	76.280436
102.252647	22.472143	76.285441
101.231318	35.410829	76.290446
101.259653	18.807035	76.295450
100.598868	19.677378	76.300455
100.244472	24.210752	76.305460
99.354420	28.613529	76.310465
98.184059	26.700016	76.315470
97.701275	26.830814	76.320474
97.520925	29.236071	76.325479
97.008112	22.064554	76.330484
95.640987	18.678114	76.335489
94.920581	21.511679	76.340494
94.713802	12.391259	76.345498
94.150563	21.469294	76.350503
92.853121	26.749124	76.355508
92.556433	23.694973	76.360513
91.961778	21.443655	76.365518
91.623018	21.967771	76.370522
90.329698	24.725568	76.375527
89.799129	21.169439	76.380532
89.388376	21.495317	76.385537
88.847875	10.890700	76.390542
88.174421	12.633486	76.395546
87.311625	22.524069	76.400551
86.643027	19.376283	76.405556
86.479305	21.170226	76.410561
85.428505	24.919025	76.415566
84.604335	14.378573	76.420570
83.667757	16.991171	76.425575
83.388174	17.521617	76.430580
83.075354	14.384893	76.435585
81.836241	21.088775	76.440590
81.555279	18.803196	76.445594
80.960739	27.504632	76.450599
79.839220	19.370567	76.455604
79.445458	7.506305	76.460609
78.417174	16.518174	76.465614
78.444145	13.027654	76.470618
77.391529	19.626103	76.475623
76.306804	18.408524	76.480628
76.194533	18.388772	76.485633
75.410742	19.198323	76.490638
74.893031	22.035832	76.495642
74.031873	17.299344	76.500647
73.314040	18.869451	76.505652
73.024782	25.499103	76.510657
72.430251	31.789545	76.515662
71.550672	20.609848	76.520666
70.453068	23.019493	76.525671
70.014177	26.782654	76.530676
69.665314	21.830423	76.535681
68.709422	23.175170	76.540686
67.931740	31.983088	76.545690
67.330476	25.183630	76.550695
66.863436	22.505138	76.555700
66.622958	20.315598	76.560705
65.389161	29.022813	76.565710
64.963358	20.347308	76.570714
64.324505	22.642785	76.575719
63.703828	24.410273	76.580724
62.412021	17.927531	76.585729
61.556229	24.828884	76.590734
61.328243	20.915438	76.595738
61.352861	22.212595	76.600743
60.602275	21.952483	76.605748
59.954124	17.495817	76.610753
58.792041	31.813050	76.615758
58.558797	28.505949	76.620762
57.709265	19.822345	76.625767
56.566825	22.821002	76.630772
55.822860	7.660235	76.635777
55.466971	22.003396	76.640782
55.055593	28.351352	76.645786
54.489963	20.439270	76.650791
53.627324	23.062161	76.655796
53.306209	12.961843	76.660801
52.629934	19.255860	76.665806
51.816002	9.478564	76.670810
50.656397	21.376516	76.675815
49.909247	27.051104	76.680820
50.056914	11.312903	76.685825
48.718857	29.691773	76.690830
48.241731	20.299110	76.695834
47.541114	18.096244	76.700839
47.229284	16.045813	76.705844
46.938471	21.434736	76.710849
45.687594	23.159260	76.715854
45.243577	29.905057	76.720858
44.482821	19.416002	76.725863
43.454463	21.590700	76.730868
42.904310	16.082421	76.735873
41.942019	15.144928	76.740878
41.883177	18.915274	76.745882
41.332751	11.376066	76.750887
40.649015	18.021334	76.755892
39.853259	12.731995	76.760897
38.737691	20.668202	76.765902
38.413991	18.223878	76.770906
38.243996	19.793335	76.775911
37.283571	25.900888	76.780916
36.794343	18.952693	76.785921
35.992181	22.179335	76.790926
35.078714	18.534499	76.795930
34.300547	25.924915	76.800935
33.383941	29.508837	76.805940
33.320116	18.741470	76.810945
32.680455	34.768251	76.815950
31.650197	16.641378	76.820954
31.135121	21.886316	76.825959
30.427165	29.714935	76.830964
30.247560	22.540744	76.835969
28.995721	34.555921	76.840974
28.183022	26.817289	76.845978
27.814205	15.448916	76.850983
27.263504	19.463291	76.855988
27.207647	10.129588	76.860993
25.629856	21.436714	76.865998
25.126261	14.232214	76.871002
24.973665	16.467477	76.876007
24.208258	26.708371	76.881012
23.330830	15.222451	76.886017
22.440780	29.005899	76.891022
22.027585	23.535696	76.896026
21.027688	22.128003	76.901031
19.938540	28.323901	76.906036
19.568359	21.512827	76.911041
18.856574	24.190507	76.916046
18.639986	30.122644	76.921050
18.430791	17.487832	76.926055
17.431627	21.148001	76.931060
16.605892	17.317302	76.936065
15.915949	27.426320	76.941070
15.912124	12.898074	76.946074
14.911783	17.143440	76.951079
14.122055	20.142616	76.956084
13.600109	19.948540	76.961089
12.294775	18.763029	76.966094
11.212587	20.659342	76.971098
11.116599	15.688860	76.976103
10.472736	21.064724	76.981108
10.406455	15.264815	76.986113
9.863730	25.714598	76.991118
8.942940	27.307640	76.996122
8.530909	18.912210	77.001127
7.464790	27.189026	77.006132
6.485205	25.853788	77.011137
5.798692	27.165047	77.016142
5.231985	18.758025	77.021147
5.148625	25.340642	77.026151
4.336445	19.497307	77.031156
3.328821	25.095196	77.036161