Mon Mar 08 19:29:17 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-0.737684	90.473524	0.000000
-0.788496	80.602830	0.005005
-1.770103	40.595695	0.010010
-3.559494	14.962692	0.015014
-8.579144	0.198487	0.020019
-13.814885	2.487602	0.025024
-18.338563	0.557060	0.030029
-22.836812	10.674261	0.035034
-26.946317	6.605703	0.040038
-30.320387	17.932804	0.045043
-34.257725	20.994077	0.050048
-37.665914	11.871847	0.055053
-41.590383	9.273373	0.060058
-44.934993	19.501467	0.065062
-48.721786	18.546187	0.070067
-52.688866	12.272604	0.075072
-56.376114	6.900496	0.080077
-60.315330	17.680743	0.085082
-63.746388	14.782838	0.090086
-68.073579	20.922852	0.095091
-71.921660	20.567123	0.100096
-75.285226	21.417656	0.105101
-78.936078	20.776603	0.110106
-83.035662	6.807155	0.115110
-86.594615	16.970153	0.120115
-90.428542	21.768465	0.125120
-93.974584	17.583323	0.130125
-97.701622	14.142948	0.135130
-101.465101	12.086551	0.140134
-105.572745	15.085226	0.145139
-109.268433	18.633153	0.150144
-112.766178	5.849715	0.155149
-116.429674	12.462620	0.160154
-120.261049	7.361172	0.165158
-124.105638	16.319359	0.170163
-127.952330	13.912030	0.175168
-131.580773	14.677177	0.180173
-135.499571	20.039416	0.185178
-139.234221	2.946474	0.190182
-143.058423	7.621894	0.195187
-146.729980	10.565249	0.200192
-150.396475	2.316981	0.205197
-154.590938	1.825856	0.210202
-158.023210	0.852026	0.215206
-161.877974	13.422850	0.220211
-166.232103	16.255968	0.225216
-169.785910	19.609470	0.230221
-173.345629	17.351951	0.235226
-176.597521	16.071840	0.240230
-180.479515	25.360914	0.245235
-184.810385	28.232930	0.250240
-188.571095	15.989845	0.255245
-192.062236	17.286644	0.260250
-195.506118	14.558121	0.265254
-199.336401	21.147306	0.270259
-202.993663	17.099917	0.275264
-206.411004	0.345937	0.280269
-211.189146	16.489078	0.285274
-214.744854	13.552942	0.290278
-218.508630	21.985904	0.295283
-222.311358	11.143512	0.300288
-225.912931	4.611641	0.305293
-229.468922	17.426600	0.310298
-233.294138	9.274750	0.315302
-236.924389	19.690589	0.320307
-241.029163	13.794091	0.325312
-244.232541	10.219916	0.330317
-248.386877	19.710238	0.335322
-252.146136	11.748149	0.340326
-255.990253	13.640652	0.345331
-259.868405	14.576722	0.350336
-263.398324	12.584222	0.355341
-267.291195	15.324978	0.360346
-270.733046	13.775715	0.365350
-274.744595	17.755897	0.370355
-278.517142	15.158795	0.375360
-282.045673	11.833675	0.380365
-286.264789	11.036077	0.385370
-289.619579	10.672918	0.390374
-293.150254	18.408088	0.395379
-297.563805	7.683823	0.400384
-301.040926	4.440407	0.405389
-305.253808	12.289215	0.410394
-308.477305	10.982676	0.415398
-312.267606	14.727344	0.420403
-316.426739	16.417932	0.425408
-319.788839	11.167791	0.430413
-323.671660	22.076621	0.435418
-327.398011	17.796045	0.440422
-331.150212	17.324508	0.445427
-334.947205	18.742870	0.450432
-338.554570	17.171245	0.455437
-342.774953	11.293385	0.460442
-346.061731	10.534700	0.465446
-349.591853	17.317450	0.470451
-353.711426	18.451472	0.475456
-357.475693	17.827373	0.480461
-361.635782	21.951250	0.485466
-365.133910	7.843731	0.490470
-368.923906	16.096608	0.495475
-372.586675	12.972813	0.500480
-376.143409	10.975302	0.505485
-380.187262	17.436443	0.510490
-383.898174	10.606907	0.515494
-387.579399	14.055176	0.520499
-391.289995	11.967143	0.525504
-395.305315	11.419454	0.530509
-399.098029	15.341246	0.535514
-402.491370	11.728237	0.540518
-406.246476	10.402638	0.545523
-409.950448	13.783615	0.550528
-413.610063	3.979915	0.555533
-417.588528	12.299222	0.560538
-421.496590	5.934857	0.565542
-425.236812	12.275054	0.570547
-429.043717	14.556097	0.575552
-432.429556	8.117825	0.580557
-436.696029	24.115031	0.585562
-440.692135	22.306035	0.590566
-444.408609	2.075978	0.595571
-447.661165	18.259773	0.600576
-451.120699	-3.042543	0.605581
-455.151078	2.481501	0.610586
-459.038876	16.094015	0.615590
-462.988391	23.059006	0.620595
-466.762877	23.187284	0.625600
-470.395999	8.735667	0.630605
-474.096819	5.249131	0.635610
-477.938060	20.151975	0.640614
-481.619029	17.504307	0.645619
-485.795910	20.120469	0.650624
-488.924994	6.178128	0.655629
-493.323635	8.739837	0.660634
-496.903394	17.336193	0.665638
-500.165423	19.301690	0.670643
-503.957180	20.345772	0.675648
-507.744628	0.354229	0.680653
-511.865392	34.212725	0.685658
-515.595867	8.980148	0.690662
-519.261779	20.628853	0.695667
-523.133969	24.539879	0.700672
-526.470964	7.794075	0.705677
-530.400619	7.381154	0.710682
-534.299172	18.728016	0.715686
-538.096558	31.056870	0.720691
-542.094934	8.129889	0.725696
-545.566467	21.116274	0.730701
-549.841050	23.300332	0.735706
-553.266053	23.574761	0.740710
-556.687371	2.509343	0.745715
-560.556901	20.002827	0.750720
-564.089380	18.495273	0.755725
-568.188253	18.252935	0.760730
-571.775733	8.707607	0.765734
-575.692865	17.105671	0.770739
-579.609160	19.525841	0.775744
-583.367740	25.216403	0.780749
-586.981241	14.180416	0.785754
-590.812355	16.416699	0.790758
-594.636732	25.731888	0.795763
-598.313355	17.922738	0.800768
-601.869567	16.068975	0.805773
-605.679037	10.632119	0.810778
-609.642301	28.169039	0.815782
-613.178808	10.379842	0.820787
-617.376989	12.671652	0.825792
-621.125827	28.506048	0.830797
-624.727596	0.097887	0.835802
-628.256333	42.052032	0.840806
-631.909875	5.632371	0.845811
-635.854454	27.862143	0.850816
-639.157948	21.045194	0.855821
-643.525574	25.991123	0.860826
-647.306464	8.466516	0.865830
-650.851061	25.297990	0.870835
-654.732282	29.388850	0.875840
-658.396486	22.500259	0.880845
-662.259791	13.232514	0.885850
-666.216743	20.200590	0.890854
-669.577550	23.232268	0.895859
-673.806691	22.720789	0.900864
-677.182168	0.642234	0.905869
-681.061164	31.896826	0.910874
-684.343631	16.989019	0.915878
-688.478568	13.736177	0.920883
-692.516862	24.263584	0.925888
-695.890434	14.712657	0.930893
-699.725079	19.933039	0.935898
-703.480297	13.683493	0.940902
-707.539154	34.105668	0.945907
-711.313811	11.252065	0.950912
-714.829451	19.877905	0.955917
-718.541819	27.535481	0.960922
-722.056777	0.017151	0.965926
-726.338149	21.458835	0.970931
-730.440366	21.988381	0.975936
-733.937926	5.243340	0.980941
-737.462390	12.314289	0.985946
-740.939124	15.590076	0.990950
-744.541286	6.378510	0.995955
-748.603372	30.014832	1.000960
-752.435312	16.457983	1.005965
-756.509962	28.993877	1.010970
-760.315429	17.194129	1.015974
-763.620594	12.938405	1.020979
-767.713905	23.774321	1.025984
-770.842763	6.577784	1.030989
-774.983646	25.154078	1.035994
-778.742436	17.932322	1.040998
-782.499542	18.093014	1.046003
-786.255218	23.578434	1.051008
-789.964054	19.287921	1.056013
-793.754234	32.232538	1.061018
-797.859569	5.401580	1.066022
-801.588821	21.578418	1.071027
-805.602804	31.230137	1.076032
-809.396746	-4.330991	1.081037
-812.991012	33.584505	1.086042
-816.315865	13.656751	1.091046
-819.864106	8.976375	1.096051
-823.726903	27.148781	1.101056
-827.526378	3.241322	1.106061
-831.430438	39.143882	1.111066
-835.356149	7.987424	1.116070
-839.225341	26.805797	1.121075
-842.638641	21.160938	1.126080
-846.356003	1.800577	1.131085
-850.327433	28.424829	1.136090
-853.755589	21.349025	1.141094
-857.800165	5.453239	1.146099
-861.957294	34.652200	1.151104
-865.500023	7.709365	1.156109
-869.201905	34.222761	1.161114
-872.785037	17.579919	1.166118
-876.260967	10.636362	1.171123
-880.534470	24.378973	1.176128
-883.792236	12.834060	1.181133
-887.908539	29.030327	1.186138
-891.575116	16.458037	1.191142
-895.378382	18.477482	1.196147
-899.723752	15.269697	1.201152
-902.846033	27.226247	1.206157
-906.642802	5.284804	1.211162
-910.500031	30.011310	1.216166
-914.160251	17.341854	1.221171
-918.126350	22.042744	1.226176
-921.513511	11.735887	1.231181
-925.112936	17.166576	1.236186
-929.327575	18.595888	1.241190
-933.158617	25.418117	1.246195
-936.945360	17.717010	1.251200
-940.641037	7.521009	1.256205
-944.171619	14.307825	1.261210
-947.894294	9.991402	1.266214
-951.556802	8.536763	1.271219
-955.664647	18.925908	1.276224
-959.368442	12.116678	1.281229
-963.376971	19.888197	1.286234
-967.220280	17.617312	1.291238
-970.637079	5.476697	1.296243
-974.163806	18.666423	1.301248
-977.991962	8.561048	1.306253
-981.663082	14.175158	1.311258
-985.624717	9.247357	1.316262
-989.535105	12.160796	1.321267
-993.258853	17.603583	1.326272
-996.763767	1.140838	1.331277
-1000.914860	7.408845	1.336282
-1004.694602	8.040252	1.341286
-1008.322913	14.549499	1.346291
-1012.127427	21.377068	1.351296
-1015.813430	14.505166	1.356301
-1019.557056	14.700348	1.361306
-1023.516188	17.541221	1.366310
-1026.885676	15.230929	1.371315
-1031.111241	14.030451	1.376320
-1034.530367	10.496610	1.381325
-1038.398143	14.499208	1.386330
-1042.579553	4.232844	1.391334
-1045.889909	5.675422	1.396339
-1050.049926	20.620623	1.401344
-1053.187787	9.463614	1.406349
-1057.068581	8.487140	1.411354
-1060.769746	8.328697	1.416358
-1064.649146	23.864503	1.421363
-1068.680795	21.835205	1.426368
-1072.261684	6.791259	1.431373
-1076.225392	5.698780	1.436378
-1079.968466	21.192302	1.441382
-1083.022400	6.995991	1.446387
-1087.122549	17.114484	1.451392
-1090.717708	11.103313	1.456397
-1094.714906	11.722344	1.461402
-1098.611551	5.062457	1.466406
-1102.305514	-2.925986	1.471411
-1106.349929	25.969876	1.476416
-1109.863211	11.176928	1.481421
-1114.091751	8.996295	1.486426
-1117.546095	16.009266	1.491430
-1120.726572	9.916041	1.496435
-1124.446509	8.194919	1.501440
-1128.428181	8.836753	1.506445
-1132.352751	22.959168	1.511450
-1136.534275	18.856791	1.516454
-1139.898218	6.679608	1.521459
-1144.123902	5.368980	1.526464
-1147.075941	-3.830813	1.531469
-1151.003115	15.126569	1.536474
-1155.345061	17.734038	1.541478
-1158.626072	19.402296	1.546483
-1162.723405	19.280588	1.551488
-1166.078289	4.186457	1.556493
-1170.156385	15.444752	1.561498
-1173.797838	4.119355	1.566502
-1177.460627	5.815605	1.571507
-1181.070616	26.226585	1.576512
-1184.933690	15.381319	1.581517
-1188.605659	5.934091	1.586522
-1192.513605	8.686638	1.591526
-1196.238921	1.334094	1.596531
-1200.367032	16.879928	1.601536
-1203.814800	13.901235	1.606541
-1207.380146	5.536023	1.611546
-1211.048045	1.878266	1.616550
-1215.131647	13.977958	1.621555
-1219.324318	22.470006	1.626560
-1222.921648	4.860310	1.631565
-1226.698972	2.286017	1.636570
-1229.958786	11.175967	1.641574
-1233.639926	-1.814402	1.646579
-1237.873645	10.228927	1.651584
-1241.343798	2.614874	1.656589
-1245.567399	14.317584	1.661594
-1249.273458	2.091254	1.666598
-1252.913918	11.023223	1.671603
-1256.471759	6.803924	1.676608
-1259.836111	-2.255625	1.681613
-1263.979925	14.745071	1.686618
-1267.931237	16.279495	1.691622
-1271.278373	2.277031	1.696627
-1275.407289	3.362113	1.701632
-1279.090121	2.280223	1.706637
-1282.737567	6.102886	1.711642
-1286.665575	16.998337	1.716646
-1290.338693	-0.725251	1.721651
-1294.315222	3.823396	1.726656
-1297.681633	15.247097	1.731661
-1301.561673	12.525376	1.736666
-1305.535009	-9.096903	1.741670
-1309.020923	18.555618	1.746675
-1312.954997	18.026457	1.751680
-1316.536066	-0.643716	1.756685
-1320.482465	30.016996	1.761690
-1324.056046	-4.528194	1.766694
-1328.064839	12.875155	1.771699
-1331.864133	-3.806382	1.776704
-1335.526944	4.995254	1.781709
-1339.142230	10.001777	1.786714
-1342.984810	10.818817	1.791718
-1346.790595	2.240029	1.796723
-1351.056022	8.642045	1.801728
-1354.307106	5.611603	1.806733
-1358.192296	9.742073	1.811738
-1362.124017	14.096022	1.816742
-1365.645715	15.760522	1.821747
-1369.419692	15.931167	1.826752
-1372.541861	-12.833019	1.831757
-1376.673961	13.992691	1.836762
-1380.727162	17.445257	1.841766
-1383.992058	2.516833	1.846771
-1388.454267	13.859046	1.851776
-1391.792930	2.909714	1.856781
-1395.889900	-9.159164	1.861786
-1399.573643	18.444717	1.866790
-1402.929823	15.060614	1.871795
-1407.323863	9.166810	1.876800
-1411.087278	24.414931	1.881805
-1414.202926	-4.120032	1.886810
-1417.870428	5.773633	1.891814
-1421.585708	8.077859	1.896819
-1426.041176	24.624139	1.901824
-1429.346121	13.917020	1.906829
-1433.470069	19.123385	1.911834
-1436.983606	12.727579	1.916838
-1440.446670	6.498726	1.921843
-1444.952075	13.540100	1.926848
-1448.526722	6.750433	1.931853
-1452.294585	13.645353	1.936858
-1456.157788	4.924573	1.941862
-1459.402955	29.911777	1.946867
-1463.203162	8.626307	1.951872
-1466.855357	12.103116	1.956877
-1470.716727	14.651566	1.961882
-1474.934159	22.802696	1.966886
-1478.484603	2.511664	1.971891
-1482.333730	21.048654	1.976896
-1485.402012	9.671428	1.981901
-1489.370920	1.275114	1.986906
-1493.928259	20.543633	1.991910
-1497.060628	-6.153096	1.996915
-1501.385458	16.031314	2.006912
-1502.129820	3.569114	2.016909
-1499.609769	22.032972	2.026906
-1496.764675	15.912864	2.036902
-1494.499964	15.561604	2.046899
-1492.988447	10.567610	2.056896
-1490.951466	12.682643	2.066893
-1488.829123	10.680621	2.076890
-1486.925032	12.520117	2.086886
-1485.264833	14.504449	2.096883
-1483.523484	10.231499	2.106880
-1481.320704	17.800128	2.116877
-1479.422710	5.963167	2.126874
-1477.473226	9.735788	2.136870
-1475.462166	18.700812	2.146867
-1473.662430	8.818396	2.156864
-1472.279573	16.843556	2.166861
-1470.169402	16.755468	2.176858
-1468.006999	1.999546	2.186854
-1466.272774	16.184319	2.196851
-1464.276850	15.542991	2.206848
-1462.292292	15.156098	2.216845
-1460.593864	16.848558	2.226842
-1458.747195	9.113747	2.236838
-1456.755655	9.221494	2.246835
-1454.983676	16.281271	2.256832
-1453.265111	7.065503	2.266829
-1451.190460	4.155428	2.276826
-1448.957629	9.616268	2.286822
-1447.362063	3.329991	2.296819
-1445.400814	10.713129	2.306816
-1443.610704	13.646097	2.316813
-1441.446411	7.671369	2.326810
-1439.694570	9.105836	2.336806
-1437.990922	8.223977	2.346803
-1436.296277	5.215292	2.356800
-1434.169621	7.829141	2.366797
-1432.286743	7.834315	2.376794
-1430.639404	12.182682	2.386790
-1428.479167	-1.892381	2.396787
-1426.678192	5.620634	2.406784
-1425.214209	17.977793	2.416781
-1422.917806	10.510455	2.426778
-1420.607976	-1.430284	2.436774
-1419.171112	2.274465	2.446771
-1417.309887	8.683712	2.456768
-1415.270747	3.346369	2.466765
-1413.455561	2.996106	2.476762
-1411.378739	5.107990	2.486758
-1409.700259	2.823440	2.496755
-1408.118852	6.596630	2.506752
-1406.364997	14.210362	2.516749
-1403.888312	1.649281	2.526746
-1402.317085	12.448342	2.536742
-1400.100330	7.126784	2.546739
-1398.607178	7.386993	2.556736
-1396.511172	13.646579	2.566733
-1394.646992	8.799858	2.576730
-1392.750402	14.483520	2.586726
-1390.852655	9.944038	2.596723
-1389.308096	7.887766	2.606720
-1386.905535	8.422374	2.616717
-1385.315272	6.518252	2.626714
-1383.569699	12.578176	2.636710
-1381.513265	-3.524825	2.646707
-1379.834262	8.608481	2.656704
-1377.772597	4.134343	2.666701
-1375.839155	6.676551	2.676698
-1374.141163	4.752034	2.686694
-1372.212557	9.841682	2.696691
-1370.250164	12.439257	2.706688
-1368.435124	-1.283682	2.716685
-1366.661903	10.686145	2.726682
-1364.424910	6.079750	2.736678
-1362.490964	-1.558440	2.746675
-1361.043458	12.593378	2.756672
-1359.572102	6.450186	2.766669
-1357.099649	10.232355	2.776666
-1355.194588	7.605279	2.786662
-1353.371624	13.839143	2.796659
-1351.469380	16.782657	2.806656
-1349.843986	37.767662	2.816653
-1347.834778	16.203125	2.826650
-1345.490158	20.585204	2.836646
-1344.139563	17.628492	2.846643
-1341.838368	5.179234	2.856640
-1340.383386	21.756552	2.866637
-1338.582343	6.783846	2.876634
-1336.539787	25.003844	2.886630
-1334.644233	14.141510	2.896627
-1332.599606	11.070564	2.906624
-1330.956239	2.770007	2.916621
-1329.107381	17.767027	2.926618
-1326.759839	3.657321	2.936614
-1325.324932	19.282666	2.946611
-1323.216437	15.806795	2.956608
-1321.611567	11.263719	2.966605
-1319.610449	23.332903	2.976602
-1317.752696	14.158094	2.986598
-1315.531602	15.508082	2.996595
-1314.022373	20.945939	3.006592
-1312.174797	15.148318	3.016589
-1310.495022	16.591263	3.026586
-1308.268953	25.204696	3.036582
-1306.459699	8.231884	3.046579
-1304.673189	17.239327	3.056576
-1302.785007	23.150191	3.066573
-1300.666456	22.056776	3.076570
-1298.844212	8.692693	3.086566
-1297.110183	7.318213	3.096563
-1295.239064	18.566703	3.106560
-1293.274908	14.258229	3.116557
-1291.494348	10.661197	3.126554
-1289.373428	8.703790	3.136550
-1287.855807	21.385608	3.146547
-1285.890654	18.177429	3.156544
-1283.891286	15.516370	3.166541
-1281.874272	16.599072	3.176538
-1280.130531	11.823812	3.186534
-1278.367865	10.061106	3.196531
-1276.353672	13.119389	3.206528
-1274.617447	25.935174	3.216525
-1272.736491	20.361169	3.226522
-1270.258990	11.819797	3.236518
-1269.113062	7.339147	3.246515
-1267.175323	14.464129	3.256512
-1265.176840	18.470661	3.266509
-1263.387454	0.893210	3.276506
-1261.518947	19.306913	3.286502
-1259.491282	20.629492	3.296499
-1257.530066	11.891296	3.306496
-1255.649969	15.313665	3.316493
-1253.948859	17.247415	3.326490
-1252.105079	16.119071	3.336486
-1250.156087	4.162010	3.346483
-1248.136467	22.824689	3.356480
-1246.177971	13.608547	3.366477
-1244.481471	21.504737	3.376474
-1242.722906	2.369177	3.386470
-1240.783927	15.545669	3.396467
-1238.944025	14.500055	3.406464
-1237.163680	12.407731	3.416461
-1234.949287	15.137195	3.426458
-1233.436152	0.314832	3.436454
-1231.379363	13.003565	3.446451
-1229.205538	9.160507	3.456448
-1227.708608	20.213164	3.466445
-1225.942978	12.650946	3.476442
-1223.818508	9.445746	3.486438
-1221.915623	8.342703	3.496435
-1220.059870	17.803319	3.506432
-1218.182679	10.655858	3.516429
-1216.421245	13.307827	3.526426
-1214.745633	19.368035	3.536422
-1212.486483	14.568770	3.546419
-1210.696178	7.700463	3.556416
-1208.791594	23.814401	3.566413
-1207.090099	13.957350	3.576410
-1205.086975	17.268505	3.586406
-1203.205484	6.383257	3.596403
-1201.378470	19.615598	3.606400
-1199.266819	19.415422	3.616397
-1197.573666	12.647923	3.626394
-1195.947218	9.536640	3.636390
-1193.850693	10.467759	3.646387
-1191.802825	12.087145	3.656384
-1189.991053	8.469405	3.666381
-1188.390709	3.641370	3.676378
-1186.359722	2.956778	3.686374
-1184.547277	14.274751	3.696371
-1182.683897	8.152615	3.706368
-1180.482931	8.332876	3.716365
-1178.785030	17.904042	3.726362
-1177.047266	7.314945	3.736358
-1175.106191	9.126682	3.746355
-1173.247843	9.623852	3.756352
-1171.353079	19.558239	3.766349
-1169.485081	14.047962	3.776346
-1167.303010	4.221418	3.786342
-1165.812421	10.175481	3.796339
-1164.065751	16.824318	3.806336
-1162.100899	13.377884	3.816333
-1159.797689	12.716074	3.826330
-1158.094121	14.130064	3.836326
-1156.419382	17.830091	3.846323
-1154.424137	5.069962	3.856320
-1152.488224	10.363885	3.866317
-1150.705683	21.437222	3.876314
-1148.781140	11.143501	3.886310
-1146.834918	10.698277	3.896307
-1144.945573	13.612452	3.906304
-1143.224710	15.937834	3.916301
-1141.152987	9.483998	3.926298
-1139.555617	8.889338	3.936294
-1137.677159	6.530357	3.946291
-1135.648570	20.478883	3.956288
-1133.985758	12.238485	3.966285
-1131.913858	9.404908	3.976282
-1129.747297	5.788875	3.986278
-1128.188776	3.340565	3.996275
-1126.171252	11.131811	4.006272
-1124.611817	9.802754	4.016269
-1122.679932	9.713504	4.026266
-1120.627427	10.953290	4.036262
-1118.817323	1.675729	4.046259
-1116.924604	15.964931	4.056256
-1114.863840	9.711802	4.066253
-1113.275079	5.605618	4.076250
-1111.222872	14.845445	4.086246
-1109.511845	4.742215	4.096243
-1107.521042	2.281609	4.106240
-1105.559781	12.936418	4.116237
-1103.943474	13.593931	4.126234
-1101.839181	9.975251	4.136230
-1099.880322	0.023428	4.146227
-1098.048724	12.271509	4.156224
-1096.399611	14.572090	4.166221
-1094.182955	4.255370	4.176218
-1092.545719	19.752227	4.186214
-1090.740809	15.302028	4.196211
-1088.624774	7.638070	4.206208
-1086.799315	13.589150	4.216205
-1085.101332	12.781079	4.226202
-1083.081896	-0.775441	4.236198
-1081.350442	8.738331	4.246195
-1079.429614	8.125131	4.256192
-1077.311750	8.953476	4.266189
-1075.613103	12.210821	4.276186
-1073.919775	12.589212	4.286182
-1071.665448	9.200755	4.296179
-1069.986336	14.128485	4.306176
-1068.378129	13.124799	4.316173
-1066.256562	6.186242	4.326170
-1064.338379	6.272904	4.336166
-1062.550523	7.545597	4.346163
-1060.776428	-0.777280	4.356160
-1058.713980	8.887243	4.366157
-1056.802301	12.906266	4.376154
-1054.830306	-0.031636	4.386150
-1052.981922	12.175909	4.396147
-1051.300218	3.799922	4.406144
-1049.520104	9.769337	4.416141
-1047.460157	12.528423	4.426138
-1045.525819	9.306422	4.436134
-1043.478570	10.671846	4.446131
-1042.065791	16.021116	4.456128
-1039.859210	10.226274	4.466125
-1037.961314	7.513759	4.476122
-1036.346290	1.680908	4.486118
-1034.591958	10.445850	4.496115
-1032.528787	24.548418	4.506112
-1030.727358	7.163364	4.516109
-1028.795924	6.292737	4.526106
-1026.438290	13.492881	4.536102
-1024.743926	4.769118	4.546099
-1023.123725	15.745377	4.556096
-1021.387273	16.508463	4.566093
-1019.429603	12.697000	4.576090
-1017.094395	9.009888	4.586086
-1015.628376	8.554731	4.596083
-1013.869106	9.058401	4.606080
-1011.781465	18.319501	4.616077
-1010.109476	10.859239	4.626074
-1008.357575	15.325408	4.636070
-1006.140416	6.598573	4.646067
-1004.111974	19.134194	4.656064
-1002.487784	8.612311	4.666061
-1000.498955	19.037042	4.676058
-998.761560	5.424632	4.686054
-996.929784	14.772447	4.696051
-994.846354	13.760707	4.706048
-992.864915	11.165910	4.716045
-991.292945	9.219187	4.726042
-989.408147	16.480774	4.736038
-987.251715	14.862143	4.746035
-985.304635	10.820311	4.756032
-983.962666	6.096874	4.766029
-982.084615	15.208371	4.776026
-979.918015	4.473462	4.786022
-977.910813	16.889353	4.796019
-975.985620	5.960959	4.806016
-974.268946	12.051100	4.816013
-972.510511	18.358763	4.826010
-970.508699	12.273061	4.836006
-968.683263	18.429497	4.846003
-966.694978	15.847836	4.856000
-965.200906	21.372043	4.865997
-963.064882	17.132657	4.875994
-960.904419	3.987851	4.885990
-959.596027	29.785686	4.895987
-957.441450	19.546886	4.905984
-955.401724	12.518879	4.915981
-953.823486	12.768927	4.925978
-951.707144	19.114111	4.935974
-949.934270	6.463887	4.945971
-948.081277	15.257337	4.955968
-945.987208	-0.646130	4.965965
-944.130478	11.116526	4.975962
-942.323466	17.694323	4.985958
-940.500354	13.345526	4.995955
-938.696237	6.080488	5.005952
-936.978875	14.343038	5.015949
-934.777046	12.436162	5.025946
-933.055706	13.531708	5.035942
-931.287585	9.698520	5.045939
-929.196295	21.619473	5.055936
-927.465451	8.429700	5.065933
-925.481321	19.232599	5.075930
-923.640394	15.116214	5.085926
-921.710521	9.335718	5.095923
-919.638416	13.941802	5.105920
-918.058476	18.396066	5.115917
-916.363210	19.056875	5.125914
-914.341666	10.061410	5.135910
-912.401064	19.983971	5.145907
-910.373279	11.396432	5.155904
-908.686566	14.185317	5.165901
-906.929966	8.790933	5.175898
-904.697735	12.894620	5.185894
-903.072785	22.690825	5.195891
-901.050949	12.354883	5.205888
-899.123658	15.893157	5.215885
-897.270545	20.756892	5.225882
-895.723870	18.648494	5.235878
-893.479573	20.645666	5.245875
-891.720504	28.925276	5.255872
-890.104613	16.069666	5.265869
-888.039184	20.590013	5.275866
-885.967157	-0.711117	5.285862
-884.008431	9.278035	5.295859
-882.354119	11.626885	5.305856
-880.559894	12.058755	5.315853
-878.677532	14.538509	5.325850
-876.716111	12.068578	5.335846
-874.804269	12.710584	5.345843
-872.902214	20.899457	5.355840
-870.903596	9.834666	5.365837
-869.244392	16.022495	5.375834
-867.543818	1.085085	5.385830
-865.406675	22.080286	5.395827
-863.523994	15.871614	5.405824
-861.861449	13.479470	5.415821
-859.687814	15.972674	5.425818
-857.781395	10.565426	5.435814
-855.931516	9.035388	5.445811
-854.411855	13.202508	5.455808
-852.669591	19.678634	5.465805
-850.676943	16.921118	5.475802
-848.341174	18.341641	5.485798
-846.497563	17.966748	5.495795
-844.660320	19.953249	5.505792
-843.076580	16.408526	5.515789
-841.022494	25.844101	5.525786
-839.152045	20.393668	5.535782
-837.424909	18.348034	5.545779
-835.407164	20.684614	5.555776
-833.566897	19.553998	5.565773
-831.667567	13.268483	5.575770
-829.872220	27.748790	5.585766
-828.178846	15.967075	5.595763
-826.035072	12.048655	5.605760
-824.138284	19.557931	5.615757
-822.519047	12.709338	5.625754
-820.353867	15.598642	5.635750
-818.549954	14.901716	5.645747
-816.345286	5.712858	5.655744
-814.751283	14.033118	5.665741
-812.802145	20.678303	5.675738
-811.461149	17.758150	5.685734
-809.124153	9.864903	5.695731
-807.357085	-3.188482	5.705728
-805.424003	26.734621	5.715725
-803.394374	-10.157094	5.725722
-801.939591	6.510668	5.735718
-799.827659	9.964256	5.745715
-797.868951	12.232939	5.755712
-796.112397	11.680959	5.765709
-793.792325	7.860697	5.775706
-792.298032	11.270911	5.785702
-790.551805	10.595857	5.795699
-788.431460	15.031732	5.805696
-786.765988	14.587468	5.815693
-784.530126	13.965207	5.825690
-782.994629	13.770651	5.835686
-781.200159	13.522076	5.845683
-779.100276	14.978790	5.855680
-777.254617	13.027934	5.865677
-775.524626	6.712689	5.875674
-773.397339	23.012505	5.885670
-771.493306	17.075206	5.895667
-770.027392	17.436482	5.905664
-768.007598	20.740627	5.915661
-765.824876	13.129424	5.925658
-764.228646	20.263657	5.935654
-762.456128	23.121040	5.945651
-760.467427	16.268697	5.955648
-758.411107	15.798304	5.965645
-756.518840	17.027708	5.975642
-754.678952	10.871743	5.985638
-752.970671	9.801753	5.995635
-751.106349	5.819117	6.005632
-749.102390	12.790310	6.015629
-747.398086	11.746221	6.025626
-745.321610	15.287627	6.035622
-743.281530	11.677936	6.045619
-741.770050	5.841288	6.055616
-739.837945	16.767933	6.065613
-737.973471	16.516098	6.075610
-735.717399	17.137943	6.085606
-734.012009	6.162741	6.095603
-732.394906	16.511350	6.105600
-730.516281	18.211873	6.115597
-728.249681	16.533240	6.125594
-726.368630	15.874580	6.135590
-724.850442	1.400577	6.145587
-723.098366	14.054842	6.155584
-721.262698	17.470551	6.165581
-719.125418	12.676999	6.175578
-717.181339	5.984973	6.185574
-715.468213	22.791530	6.195571
-713.390432	26.369073	6.205568
-711.587909	14.186325	6.215565
-709.871881	25.488564	6.225562
-707.617993	8.164016	6.235558
-705.762352	4.890125	6.245555
-703.869610	17.594561	6.255552
-702.293694	16.334192	6.265549
-700.574371	21.611025	6.275546
-698.641617	17.832214	6.285542
-696.666264	21.707172	6.295539
-694.669854	16.961411	6.305536
-692.833892	24.223173	6.315533
-690.909752	12.883059	6.325530
-689.092648	12.108338	6.335526
-686.993634	8.628216	6.345523
-685.624728	24.136729	6.355520
-683.291636	15.876344	6.365517
-681.566065	12.075392	6.375514
-679.853553	13.420416	6.385510
-677.599052	8.200829	6.395507
-675.730499	8.041542	6.405504
-674.047437	14.985135	6.415501
-672.263975	10.505508	6.425498
-670.585708	10.105067	6.435494
-668.368118	10.908377	6.445491
-666.649171	5.217035	6.455488
-664.745793	8.806694	6.465485
-662.792667	17.797544	6.475482
-660.829524	0.647379	6.485478
-658.931060	20.376819	6.495475
-657.312498	4.276381	6.505472
-655.497095	17.815799	6.515469
-653.505349	14.995433	6.525466
-651.628538	11.422954	6.535462
-649.709579	14.989613	6.545459
-647.579432	6.914837	6.555456
-645.789635	17.865886	6.565453
-644.475565	10.695126	6.575450
-641.854496	5.243334	6.585446
-640.422595	12.912299	6.595443
-638.473252	6.178440	6.605440
-636.583853	16.903597	6.615437
-634.751459	14.936022	6.625434
-632.732523	11.786086	6.635430
-630.889076	17.625738	6.645427
-628.998294	15.415169	6.655424
-627.182275	12.727103	6.665421
-625.569349	16.784751	6.675418
-623.249333	12.866769	6.685414
-621.365090	8.495807	6.695411
-619.748799	1.448877	6.705408
-618.196350	20.188437	6.715405
-615.880446	5.571256	6.725402
-613.829675	6.033394	6.735398
-612.217841	0.987583	6.745395
-610.222588	14.679876	6.755392
-608.426328	6.844773	6.765389
-606.346052	10.512005	6.775386
-604.853424	8.770825	6.785382
-602.784394	9.984746	6.795379
-600.914456	16.731187	6.805376
-599.079512	19.018232	6.815373
-597.272494	8.582630	6.825370
-595.268976	10.107005	6.835366
-593.422611	20.914864	6.845363
-591.442231	12.301983	6.855360
-589.754473	18.715979	6.865357
-587.744625	13.275041	6.875354
-585.668633	21.496384	6.885350
-584.217951	21.250771	6.895347
-582.283064	15.684451	6.905344
-580.319528	14.493288	6.915341
-578.203394	7.366536	6.925338
-576.295380	16.948846	6.935334
-574.788498	11.278805	6.945331
-572.939361	17.112860	6.955328
-570.696488	15.229756	6.965325
-568.924852	10.041607	6.975322
-566.968116	12.118182	6.985318
-565.405740	18.018573	6.995315
-563.348385	15.854075	7.005312
-561.501742	6.130546	7.015309
-559.786051	7.547777	7.025306
-557.774327	18.340305	7.035302
-555.836805	10.610559	7.045299
-553.701003	2.456014	7.055296
-552.340108	13.917727	7.065293
-550.392314	14.011129	7.075290
-548.540660	7.995528	7.085286
-546.387074	8.586557	7.095283
-544.450958	16.715022	7.105280
-542.734854	15.403945	7.115277
-540.861953	16.545044	7.125274
-539.173046	11.210665	7.135270
-537.124297	5.580409	7.145267
-535.294836	16.337336	7.155264
-533.247496	11.711455	7.165261
-531.414563	3.821604	7.175258
-529.522743	14.508578	7.185254
-527.581429	11.475330	7.195251
-526.134579	9.460473	7.205248
-523.847096	8.580752	7.215245
-522.275890	9.249029	7.225242
-520.074195	7.419914	7.235238
-518.182947	15.553990	7.245235
-516.434047	3.048378	7.255232
-514.553472	20.087303	7.265229
-512.718347	10.506160	7.275226
-511.129590	9.283335	7.285222
-508.947975	18.572552	7.295219
-506.910777	14.027254	7.305216
-505.319626	20.308334	7.315213
-503.458151	10.195653	7.325210
-501.544904	14.765920	7.335206
-499.731183	18.297411	7.345203
-497.734072	12.244404	7.355200
-495.612366	4.862636	7.365197
-493.902753	13.152047	7.375194
-491.931352	5.769023	7.385190
-490.220531	6.176618	7.395187
-488.258998	18.731332	7.405184
-486.180701	11.209667	7.415181
-485.000642	11.116274	7.425178
-482.820853	10.370625	7.435174
-480.352250	15.539023	7.445171
-479.039220	6.382313	7.455168
-477.487477	16.545785	7.465165
-474.936571	9.872286	7.475162
-473.039224	3.650507	7.485158
-471.392505	17.032305	7.495155
-469.615723	11.022399	7.505152
-467.778009	16.864681	7.515149
-466.036243	13.754405	7.525146
-464.012901	17.756105	7.535142
-461.778145	15.129178	7.545139
-460.067129	24.427286	7.555136
-458.453669	12.491191	7.565133
-456.484330	24.983120	7.575130
-454.573574	23.361564	7.585126
-452.746816	10.597250	7.595123
-450.559212	23.346417	7.605120
-448.875882	14.779494	7.615117
-446.899370	15.400469	7.625114
-445.197226	15.158994	7.635110
-443.383833	21.620935	7.645107
-441.601185	19.561979	7.655104
-439.239293	16.057455	7.665101
-437.656559	19.207484	7.675098
-435.872900	20.639215	7.685094
-433.660320	20.491497	7.695091
-431.912367	17.283947	7.705088
-430.589915	17.881485	7.715085
-428.487566	9.640805	7.725082
-426.561279	8.402033	7.735078
-424.360644	4.534876	7.745075
-422.382304	16.438060	7.755072
-420.752666	10.115386	7.765069
-418.831677	13.402459	7.775066
-417.165565	19.292709	7.785062
-415.190001	18.412371	7.795059
-413.164704	12.084945	7.805056
-411.379402	10.316097	7.815053
-409.754281	15.950807	7.825050
-407.664634	10.309385	7.835046
-405.651516	10.357740	7.845043
-403.925703	9.400453	7.855040
-402.179006	20.963300	7.865037
-400.074348	17.280422	7.875034
-398.044564	21.675867	7.885030
-396.312079	7.087277	7.895027
-394.509010	14.299279	7.905024
-392.769952	15.566069	7.915021
-390.727393	14.262974	7.925018
-388.711014	17.127499	7.935014
-387.070320	16.763253	7.945011
-385.234304	23.287942	7.955008
-383.021575	14.424971	7.965005
-381.295038	21.412379	7.975002
-379.624352	14.978971	7.984998
-377.698663	13.299832	7.994995
-375.887125	12.979366	8.004992
-373.816687	21.334423	8.014989
-372.110992	7.367455	8.024986
-370.069362	15.324504	8.034982
-368.053621	15.966121	8.044979
-366.406858	22.743659	8.054976
-364.297730	13.170971	8.064973
-362.813331	19.574980	8.074970
-360.631440	11.422701	8.084966
-358.682211	7.613103	8.094963
-357.195447	11.757397	8.104960
-355.107829	9.251946	8.114957
-353.082166	16.058997	8.124954
-351.194796	14.179166	8.134950
-349.693227	8.285905	8.144947
-347.740359	17.605487	8.154944
-345.785808	12.157776	8.164941
-343.950671	12.323012	8.174938
-342.003406	15.547537	8.184934
-340.005592	19.488689	8.194931
-337.960672	18.325780	8.204928
-336.408136	24.968392	8.214925
-334.375020	24.607849	8.224922
-332.683950	16.415528	8.234918
-330.733690	19.039620	8.244915
-328.676235	18.730457	8.254912
-326.898119	22.258297	8.264909
-324.962675	21.708103	8.274906
-323.531450	21.056830	8.284902
-321.358146	12.198625	8.294899
-319.735510	15.961277	8.304896
-317.483260	13.920601	8.314893
-315.698607	13.910770	8.324890
-313.669704	13.066209	8.334886
-311.759712	9.673413	8.344883
-309.997375	16.609374	8.354880
-308.504225	13.155230	8.364877
-306.343273	9.900789	8.374874
-304.261196	3.540704	8.384870
-302.355155	11.251051	8.394867
-300.760940	8.140760	8.404864
-298.524095	9.086597	8.414861
-297.224204	14.042293	8.424858
-295.551999	13.084166	8.434854
-293.037126	12.473087	8.444851
-291.186253	8.331892	8.454848
-289.688816	17.111626	8.464845
-287.479093	14.048352	8.474842
-285.702019	16.333830	8.484838
-283.835297	1.832822	8.494835
-281.797065	17.054807	8.504832
-280.159795	12.892453	8.514829
-278.032199	11.815866	8.524826
-276.240393	17.742999	8.534822
-274.538898	14.531921	8.544819
-272.322089	4.804761	8.554816
-270.786660	16.475642	8.564813
-269.014425	15.395784	8.574810
-266.831757	19.501696	8.584807
-264.976260	12.601519	8.594803
-263.111558	2.837414	8.604800
-261.091190	11.265297	8.614797
-259.641755	8.634428	8.624794
-257.461567	8.146272	8.634791
-255.743374	15.596135	8.644787
-253.980290	11.513185	8.654784
-251.821510	10.471115	8.664781
-249.807702	18.061687	8.674778
-248.220556	5.776246	8.684775
-246.279934	13.886890	8.694771
-244.140066	-0.032458	8.704768
-242.251665	6.294521	8.714765
-240.700604	0.958654	8.724762
-239.039011	-3.681207	8.734759
-236.716181	8.512938	8.744755
-234.805702	-6.175005	8.754752
-233.281083	1.686265	8.764749
-231.196114	1.309639	8.774746
-229.261669	1.983293	8.784743
-227.542381	-0.251700	8.794739
-225.730234	-3.219890	8.804736
-223.754653	10.123835	8.814733
-221.939262	6.002563	8.824730
-219.990409	1.010570	8.834727
-217.968635	9.555103	8.844723
-216.458572	-3.191670	8.854720
-214.681609	6.874478	8.864717
-212.275452	7.640227	8.874714
-210.438107	4.870118	8.884711
-208.788103	4.870802	8.894707
-207.052838	11.984838	8.904704
-204.991432	3.752448	8.914701
-203.282160	6.132487	8.924698
-201.078873	5.225456	8.934695
-199.258423	4.968434	8.944691
-197.486987	4.122427	8.954688
-195.666174	5.845234	8.964685
-193.596249	5.849967	8.974682
-192.042907	5.304014	8.984679
-189.916126	2.738773	8.994675
-188.145942	3.983378	9.004672
-186.216765	12.380095	9.014669
-184.343417	5.958680	9.024666
-182.775893	6.192004	9.034663
-180.709781	4.916904	9.044659
-178.554867	1.755112	9.054656
-176.788898	2.252020	9.064653
-174.940315	6.543948	9.074650
-173.107231	4.887641	9.084647
-171.261024	-0.648429	9.094643
-169.268301	8.855992	9.104640
-167.546861	-0.349956	9.114637
-165.684674	6.860694	9.124634
-163.669726	-1.214258	9.134631
-161.737106	9.886512	9.144627
-160.141838	10.249627	9.154624
-158.192173	5.428066	9.164621
-156.429881	8.230708	9.174618
-154.171039	-4.417628	9.184615
-152.282730	-3.337100	9.194611
-150.644733	6.148151	9.204608
-148.903823	10.799895	9.214605
-146.860506	8.031703	9.224602
-144.967604	17.053160	9.234599
-142.894246	6.936910	9.244595
-141.103347	8.468755	9.254592
-139.330512	12.843849	9.264589
-137.758660	12.253927	9.274586
-135.462158	14.273495	9.284583
-133.729180	11.597457	9.294579
-131.835585	6.345940	9.304576
-129.921277	5.374560	9.314573
-128.217871	8.309769	9.324570
-126.442927	9.754176	9.334567
-124.087568	11.342809	9.344563
-122.292892	12.457247	9.354560
-120.699307	9.959766	9.364557
-118.787566	20.495526	9.374554
-116.703010	16.154549	9.384551
-114.919284	10.672690	9.394547
-112.976412	4.882829	9.404544
-111.485268	14.034724	9.414541
-109.367293	8.374813	9.424538
-107.433571	1.830144	9.434535
-105.733443	6.491583	9.444531
-103.604632	7.896918	9.454528
-101.896356	6.431092	9.464525
-99.955372	9.937858	9.474522
-97.930327	8.985150	9.484519
-96.061190	17.004709	9.494515
-94.313542	13.780073	9.504512
-92.424931	19.402980	9.514509
-90.787321	15.873813	9.524506
-88.475184	6.515255	9.534503
-86.922636	6.612091	9.544499
-84.833879	11.418378	9.554496
-82.852542	3.320427	9.564493
-81.330726	7.072489	9.574490
-79.304081	7.819972	9.584487
-77.332140	7.939904	9.594483
-75.590059	13.529359	9.604480
-73.976319	8.390419	9.614477
-71.595206	10.488124	9.624474
-69.854349	9.444993	9.634471
-68.015976	9.385724	9.644467
-66.219172	12.130827	9.654464
-64.510216	18.976034	9.664461
-62.282262	19.890355	9.674458
-60.445595	9.057227	9.684455
-58.778728	7.277527	9.694451
-56.754785	11.420007	9.704448
-54.708199	7.111981	9.714445
-53.059542	14.598358	9.724442
-51.299176	8.951331	9.734439
-49.448337	14.981328	9.744435
-47.324838	12.304630	9.754432
-45.666397	11.254137	9.764429
-43.493785	12.922524	9.774426
-41.742759	16.705944	9.784423
-39.868794	8.797245	9.794419
-37.939414	15.302590	9.804416
-36.136474	14.293788	9.814413
-34.193752	16.647766	9.824410
-32.513270	8.266277	9.834407
-30.362013	11.891132	9.844403
-28.642754	9.983102	9.854400
-26.966368	1.769633	9.864397
-25.112477	3.697284	9.874394
-23.149303	4.814918	9.884391
-20.820819	-2.918381	9.894387
-19.150176	6.326516	9.904384
-17.320564	10.784222	9.914381
-15.829802	13.568706	9.924378
-13.531624	11.380462	9.934375
-11.675405	2.691500	9.944371
-10.013467	13.008264	9.954368
-8.214144	9.454936	9.964365
-5.808001	12.325515	9.974362
-4.658663	17.452232	9.984359
-3.335916	51.250287	9.994355
-2.070350	97.933219	10.004352
-0.925325	155.138210	10.014349
0.000000	224.603204	10.019354
0.684920	261.662447	10.024359
1.058814	297.200827	10.029363
1.471997	341.979834	10.034368
2.186271	368.960005	10.039373
2.314902	406.486797	10.044378
2.823791	426.608852	10.049383
3.331211	435.451688	10.054387
3.597783	466.600203	10.059392
3.977056	466.986134	10.064397
4.010952	473.674795	10.069402
3.962090	489.090569	10.074407
4.130736	488.095622	10.079411
4.011557	498.303105	10.084416
3.716888	498.101118	10.089421
4.021930	501.663718	10.094426
4.066322	532.973964	10.099431
4.055776	537.000054	10.104435
4.347710	538.322404	10.109440
4.618093	531.771583	10.114445
4.501082	542.377707	10.119450
4.339762	541.525268	10.124455
4.793224	542.485975	10.129459
4.295047	552.214645	10.134464
4.776860	566.708527	10.139469
4.999608	569.703969	10.144474
4.860621	573.081949	10.149479
5.080564	581.556001	10.154483
4.946182	589.007969	10.159488
4.980850	585.930794	10.164493
4.921596	586.391404	10.169498
5.028496	590.534390	10.174503
5.399640	587.278974	10.179507
5.175433	592.061380	10.184512
5.243945	600.335675	10.189517
5.307166	592.064350	10.194522
5.496275	605.505854	10.199527
5.632527	594.649369	10.204531
5.209715	587.198289	10.209536
5.152668	578.175048	10.214541
5.552680	599.951536	10.219546
5.051488	595.822877	10.224551
5.590667	604.454178	10.229555
5.447677	611.439189	10.234560
5.338835	607.210103	10.239565
5.295788	611.359666	10.244570
5.199270	611.791527	10.249575
5.686449	620.617207	10.254579
5.542449	630.360400	10.259584
5.768995	639.883654	10.264589
6.042457	638.498252	10.269594
5.600116	647.126858	10.274599
6.133483	655.970423	10.279603
6.185061	644.463526	10.284608
5.797811	651.899089	10.289613
6.132671	660.641857	10.294618
6.098965	664.146564	10.299623
6.012838	659.885456	10.304627
5.869419	674.887588	10.309632
6.009059	657.670825	10.314637
6.191837	663.512681	10.319642
5.979732	681.886176	10.324647
6.398110	685.662551	10.329651
6.414748	697.624118	10.334656
6.805591	700.141780	10.339661
6.553327	701.992478	10.344666
6.819486	714.130299	10.349671
6.924093	707.012920	10.354675
6.619420	714.589881	10.359680
6.965624	711.059301	10.364685
6.641574	708.696888	10.369690
6.423556	720.063556	10.374695
6.889313	725.738881	10.379699
6.923786	711.905549	10.384704
7.012050	711.129985	10.389709
7.076249	721.027685	10.394714
6.918599	728.117590	10.399719
7.430012	717.426677	10.404723
6.773926	734.295710	10.409728
7.014713	725.929757	10.414733
7.140820	723.079238	10.419738
6.905363	724.025261	10.424743
7.202988	722.874113	10.429747
7.147824	725.732567	10.434752
7.223077	720.110052	10.439757
7.330666	731.807988	10.444762
6.986558	750.010238	10.449767
7.664311	742.725736	10.454771
7.541505	757.194820	10.459776
7.604915	748.639530	10.464781
7.629734	753.117347	10.469786
7.279466	767.143336	10.474791
7.646602	757.691213	10.479795
7.286284	758.698153	10.484800
7.428513	758.437516	10.489805
7.764449	779.065456	10.494810
7.683332	791.772808	10.499815
8.203884	799.169310	10.504819
7.933909	799.606765	10.509824
8.014446	803.170555	10.514829
8.211016	801.628671	10.519834
8.139052	801.695505	10.524839
8.303637	800.721685	10.529843
8.297089	801.147087	10.534848
8.507537	804.368464	10.539853
8.284112	803.044951	10.544858
8.148229	812.766471	10.549863
8.600790	810.199754	10.554867
8.031728	814.327616	10.559872
8.017892	815.969993	10.564877
8.605857	802.280106	10.569882
8.467873	812.728925	10.574887
8.365623	813.245283	10.579891
8.383089	821.494731	10.584896
8.752245	812.669868	10.589901
8.755865	832.075150	10.594906
8.690578	840.446616	10.599911
9.121355	840.187265	10.604915
8.834938	848.340117	10.609920
8.970520	845.872835	10.614925
8.933583	840.763323	10.619930
8.918441	846.840244	10.624935
9.244458	848.116187	10.629939
9.297577	847.786185	10.634944
9.469727	845.177454	10.639949
9.147697	837.287551	10.644954
8.990912	845.520651	10.649959
9.237877	847.449437	10.654963
9.385632	854.784003	10.659968
8.882091	857.876420	10.664973
9.216589	856.126454	10.669978
9.154027	857.912223	10.674983
9.883164	855.071153	10.679987
9.421755	859.413668	10.684992
9.411707	855.316984	10.689997
9.791311	852.771357	10.695002
9.555205	859.605761	10.700007
9.499145	858.908399	10.705011
9.479770	860.346663	10.710016
9.343675	858.107210	10.715021
9.432203	875.355956	10.720026
9.772598	889.234059	10.725031
9.755447	892.215793	10.730035
9.922071	901.663623	10.735040
10.041512	899.093251	10.740045
10.178632	901.665608	10.745050
9.615282	911.863800	10.750055
10.175540	900.866921	10.755059
10.058988	899.717163	10.760064
9.946655	913.052491	10.765069
10.139574	912.135646	10.770074
10.062983	924.123307	10.775079
10.367232	920.315520	10.780083
10.250386	917.155209	10.785088
10.212810	931.432678	10.790093
10.667820	928.851358	10.795098
10.494640	939.816811	10.800103
10.782752	930.985880	10.805107
10.772673	933.075522	10.810112
10.799220	928.796363	10.815117
10.773102	930.626791	10.820122
10.531771	931.867075	10.825127
10.846652	937.740011	10.830131
11.003470	938.714945	10.835136
10.861997	942.164368	10.840141
10.919449	936.498877	10.845146
11.028975	939.126104	10.850151
11.158228	932.742692	10.855155
11.121440	938.458830	10.860160
11.164938	936.742651	10.865165
11.247820	940.441718	10.870170
10.964233	939.386406	10.875175
11.476314	935.077115	10.880179
11.121559	941.148317	10.885184
11.420784	944.956382	10.890189
11.376795	946.844855	10.895194
11.042904	949.552267	10.900199
11.351359	940.601392	10.905203
11.167447	948.176560	10.910208
11.348787	973.402570	10.915213
11.517470	973.593448	10.920218
11.564590	978.670172	10.925223
11.606328	973.478679	10.930227
11.512138	980.200619	10.935232
11.730120	978.155409	10.940237
11.834855	973.305528	10.945242
11.878809	975.810757	10.950247
12.392737	969.935254	10.955251
12.174874	974.912314	10.960256
11.791005	984.566268	10.965261
11.966793	985.046173	10.970266
11.956077	983.190402	10.975271
11.962933	979.270759	10.980275
11.856654	988.344281	10.985280
11.992765	980.166765	10.990285
12.573133	975.557990	10.995290
12.047672	994.650484	11.000295
12.205287	995.648949	11.005299
12.454586	1006.331028	11.010304
12.442954	1004.634672	11.015309
12.489508	1014.253114	11.020314
12.658832	1017.159400	11.025319
12.986139	1006.669527	11.030323
12.791367	997.537104	11.035328
12.790810	995.025278	11.040333
12.526447	986.944747	11.045338
12.306188	986.954809	11.050343
12.953408	1006.323907	11.055347
12.625582	1019.483967	11.060352
12.882437	1007.666500	11.065357
13.000887	1016.426654	11.070362
12.761362	1019.834964	11.075367
13.143208	1010.222637	11.080371
12.691110	1017.634034	11.085376
12.643569	1018.762992	11.090381
13.164560	1013.244313	11.095386
13.074613	1018.448568	11.100391
13.022323	1019.404819	11.105395
12.905664	1027.010302	11.110400
13.052312	1038.484637	11.115405
13.347918	1056.378661	11.120410
13.435121	1053.532705	11.125415
13.548024	1055.960719	11.130419
13.435078	1055.483733	11.135424
13.605800	1066.099541	11.140429
13.838858	1049.812011	11.145434
13.595309	1071.597235	11.150439
13.932756	1058.029066	11.155443
13.668455	1059.676725	11.160448
13.718083	1063.409512	11.165453
13.804051	1057.523382	11.170458
13.904719	1063.752234	11.175463
13.895835	1057.890694	11.180467
13.946451	1068.724357	11.185472
13.697383	1065.712834	11.190477
14.189043	1053.059941	11.195482
14.008446	1060.517943	11.200487
13.814375	1062.600679	11.205491
14.155241	1059.818345	11.210496
13.960357	1064.362838	11.215501
14.065567	1074.762019	11.220506
13.806060	1067.915425	11.225511
14.147746	1065.120344	11.230515
14.071286	1076.906260	11.235520
14.176684	1078.423994	11.240525
14.503159	1094.991652	11.245530
14.364250	1101.919476	11.250535
14.518169	1083.958760	11.255539
14.555231	1087.083275	11.260544
14.570345	1096.441856	11.265549
14.735319	1094.890788	11.270554
14.531698	1108.986757	11.275559
14.626809	1090.475590	11.280563
14.824578	1100.640831	11.285568
14.263449	1106.216734	11.290573
14.653234	1104.232416	11.295578
14.698169	1126.129407	11.300583
14.661003	1134.873451	11.305587
15.056750	1133.682968	11.310592
14.835090	1145.634025	11.315597
15.053105	1121.440338	11.320602
14.685464	1135.967772	11.325607
15.122329	1133.884477	11.330611
15.092759	1136.030874	11.335616
14.920619	1120.848686	11.340621
15.514733	1131.048506	11.345626
15.011939	1146.482182	11.350631
15.169244	1159.008326	11.355635
15.137336	1168.382338	11.360640
15.075701	1165.074393	11.365645
15.605709	1154.504777	11.370650
15.391325	1170.166871	11.375655
15.799102	1153.209534	11.380659
15.654711	1157.388031	11.385664
15.570469	1161.314084	11.390669
15.808548	1164.444403	11.395674
15.502105	1170.985815	11.400679
15.758191	1156.657817	11.405683
15.554861	1171.539129	11.410688
16.214867	1194.894593	11.415693
16.372138	1180.454598	11.420698
16.298234	1177.314189	11.425703
16.181992	1172.001163	11.430707
15.974602	1174.611169	11.435712
16.195006	1165.221610	11.440717
15.898842	1172.154048	11.445722
16.132274	1190.922333	11.450727
16.427513	1182.364506	11.455731
16.432642	1208.082658	11.460736
16.488649	1204.607706	11.465741
16.619384	1191.073960	11.470746
16.494777	1208.260899	11.475751
16.657840	1204.696333	11.480755
16.468643	1192.021020	11.485760
16.600339	1204.049811	11.490765
16.748505	1202.178134	11.495770
16.633655	1200.897191	11.500775
16.664925	1193.147867	11.505779
17.036150	1197.187369	11.510784
16.801888	1213.491354	11.515789
17.027455	1202.421472	11.520794
16.564935	1193.670677	11.525799
16.569937	1209.755145	11.530803
16.817667	1206.861480	11.535808
16.592594	1209.242498	11.540813
16.788742	1213.272080	11.545818
16.763467	1212.595023	11.550823
16.942282	1231.834125	11.555827
17.382715	1240.320708	11.560832
17.300488	1231.367309	11.565837
17.283659	1217.893343	11.570842
17.257269	1236.099145	11.575847
17.185194	1238.783776	11.580851
17.730830	1229.110489	11.585856
17.649129	1221.815989	11.590861
17.846872	1220.974051	11.595866
17.415311	1236.544696	11.600871
17.672812	1231.131040	11.605875
17.483025	1234.083606	11.610880
17.823018	1238.779392	11.615885
18.251610	1235.735448	11.620890
17.847934	1244.670479	11.625895
17.868537	1240.800613	11.630899
17.743421	1229.282010	11.635904
17.874425	1239.905857	11.640909
17.819098	1240.548789	11.645914
17.745168	1243.585382	11.650919
18.313811	1242.042459	11.655923
18.198767	1245.965563	11.660928
17.575104	1246.787449	11.665933
18.279581	1233.483860	11.670938
17.794377	1240.673565	11.675943
18.210713	1241.460471	11.680947
17.878879	1243.480047	11.685952
17.773630	1254.669872	11.690957
18.079484	1269.336031	11.695962
18.368201	1275.579138	11.700967
18.621225	1269.582699	11.705971
18.328931	1274.327300	11.710976
18.103972	1276.531688	11.715981
18.716798	1278.052093	11.720986
18.495444	1273.564785	11.725991
18.696006	1280.735025	11.730995
18.519746	1265.647960	11.736000
18.717368	1277.273630	11.741005
18.826637	1298.723799	11.746010
18.891191	1309.320447	11.751015
19.237638	1293.189606	11.756019
19.302927	1298.988955	11.761024
18.999257	1281.667111	11.766029
19.409536	1270.760110	11.771034
19.106710	1263.212268	11.776039
19.206430	1267.197320	11.781043
19.169568	1269.338591	11.786048
19.080111	1272.565327	11.791053
19.407359	1283.068020	11.796058
19.082669	1302.507370	11.801063
19.282878	1302.844616	11.806067
19.297392	1295.921094	11.811072
18.988207	1325.028052	11.816077
19.495703	1295.779404	11.821082
19.578803	1300.383716	11.826087
19.534055	1299.734992	11.831091
19.588320	1306.272553	11.836096
19.925464	1305.466726	11.841101
20.203305	1299.947296	11.846106
19.997477	1314.917464	11.851111
20.189494	1306.790774	11.856115
19.933624	1299.330043	11.861120
19.779584	1310.751624	11.866125
19.883232	1312.473093	11.871130
19.726797	1298.048319	11.876135
19.724665	1312.659562	11.881139
19.632686	1308.654667	11.886144
19.830271	1316.654892	11.891149
19.784686	1307.448015	11.896154
19.764326	1331.255994	11.901159
20.363748	1340.814862	11.906163
20.624127	1339.647530	11.911168
20.517684	1350.186324	11.916173
20.758262	1337.262564	11.921178
20.253019	1325.673619	11.926183
20.362080	1313.051559	11.931187
20.615535	1334.655407	11.936192
20.679042	1338.244123	11.941197
20.810864	1343.947722	11.946202
20.472950	1341.659954	11.951207
20.590300	1338.586781	11.956211
20.871240	1336.969883	11.961216
20.852937	1344.151406	11.966221
21.070329	1338.110159	11.971226
20.957990	1347.757317	11.976231
21.117034	1333.094532	11.981235
20.815773	1320.712952	11.986240
20.548922	1339.712610	11.991245
21.085028	1328.533180	11.996250
20.813279	1346.355620	12.001255
21.341011	1333.129017	12.006259
21.375450	1339.001113	12.011264
21.080185	1347.010571	12.016269
21.158035	1338.692333	12.021274
21.129962	1339.797710	12.026279
21.110350	1341.592458	12.031283
21.086968	1336.818084	12.036288
21.111132	1341.064370	12.041293
21.348307	1334.524796	12.046298
21.232272	1339.946218	12.051303
21.126825	1331.781799	12.056307
21.436966	1339.962786	12.061312
21.396447	1336.589932	12.066317
21.534118	1334.661564	12.071322
21.449375	1335.656128	12.076327
21.497884	1331.264536	12.081331
21.469847	1329.859347	12.086336
21.275950	1340.259114	12.091341
21.692876	1331.572981	12.096346
21.481087	1326.095361	12.101351
21.419140	1308.517308	12.106355
21.610904	1295.864726	12.111360
21.118365	1311.692762	12.116365
21.312095	1303.430181	12.121370
21.298828	1302.981444	12.126375
21.202565	1303.007999	12.131379
21.323407	1308.155084	12.136384
21.111191	1309.466449	12.141389
21.654224	1303.761218	12.146394
21.139323	1304.343406	12.151399
21.194885	1295.405838	12.156403
21.527523	1300.206899	12.161408
21.557439	1300.650154	12.166413
21.590406	1297.700836	12.171418
21.132382	1302.992281	12.176423
21.476782	1303.481576	12.181427
21.410438	1315.901597	12.186432
21.525285	1304.339931	12.191437
21.967104	1298.467915	12.196442
21.439096	1288.202564	12.201447
21.131372	1283.156584	12.206451
21.059417	1280.742829	12.211456
21.136159	1275.331177	12.216461
21.332037	1268.727254	12.221466
21.012917	1277.262458	12.226471
21.286368	1282.082414	12.231475
21.224543	1287.654447	12.236480
21.307362	1301.285441	12.241485
21.520762	1301.292572	12.246490
21.215063	1290.722100	12.251495
21.113550	1279.053033	12.256499
21.206694	1269.669510	12.261504
21.209049	1278.711695	12.266509
21.410043	1279.092971	12.271514
21.158336	1283.742790	12.276519
21.387589	1278.153846	12.281523
20.866783	1287.684758	12.286528
21.356407	1296.578276	12.291533
21.273159	1303.907334	12.296538
21.441426	1310.888771	12.301543
21.199687	1296.750422	12.306547
21.734170	1285.577591	12.311552
21.323164	1287.179284	12.316557
21.120331	1275.502724	12.321562
20.988602	1278.911249	12.326567
21.213999	1279.162474	12.331571
21.316996	1283.099699	12.336576
21.130953	1286.513733	12.341581
21.260771	1281.744907	12.346586
21.227949	1290.045220	12.351591
21.054280	1291.903956	12.356595
21.138838	1301.671072	12.361600
21.391153	1320.092731	12.366605
21.440849	1308.989316	12.371610
21.295327	1303.819686	12.376615
21.208441	1288.410832	12.381619
21.696680	1285.895116	12.386624
21.312389	1298.603955	12.391629
21.513310	1284.357171	12.396634
21.385849	1277.613998	12.401639
21.247459	1283.745452	12.406643
21.478514	1287.707987	12.411648
21.288058	1286.754490	12.416653
21.255615	1296.936085	12.421658
21.071983	1300.381277	12.426663
21.352638	1289.373508	12.431667
21.496202	1292.025334	12.436672
21.229228	1298.927945	12.441677
21.462458	1281.171959	12.446682
21.352088	1286.606651	12.451687
21.269351	1289.475921	12.456691
21.346166	1288.867736	12.461696
21.376172	1291.630715	12.466701
21.219448	1285.010479	12.471706
21.060963	1298.254171	12.476711
21.311194	1284.215569	12.481715
21.730422	1281.865405	12.486720
21.481208	1293.791015	12.491725
21.282239	1284.856202	12.496730
21.426607	1287.518938	12.501735
21.395992	1297.387999	12.506739
21.485787	1269.743579	12.511744
21.182949	1263.435243	12.516749
21.245207	1259.090367	12.521754
21.025127	1253.894799	12.526759
20.822862	1279.431686	12.531763
21.317236	1274.986348	12.536768
21.215216	1296.019195	12.541773
21.363710	1294.885481	12.546778
21.469172	1306.141090	12.551783
21.171738	1299.013423	12.556787
21.230151	1290.669926	12.561792
21.159530	1298.515795	12.566797
21.307104	1300.004747	12.571802
21.349310	1303.935904	12.576807
21.140313	1302.826088	12.581811
21.268754	1298.915353	12.586816
21.508165	1306.183491	12.591821
21.748032	1286.969307	12.596826
21.275019	1285.494740	12.601831
21.179341	1273.581891	12.606835
21.308029	1274.209669	12.611840
21.449798	1269.755913	12.616845
21.373969	1267.071538	12.621850
21.357249	1274.309545	12.626855
21.102792	1275.756957	12.631859
21.477272	1266.287566	12.636864
21.017344	1279.377464	12.641869
21.322411	1269.455509	12.646874
21.505347	1278.774827	12.651879
21.258713	1269.596885	12.656883
21.564701	1258.279165	12.661888
21.382854	1265.160298	12.666893
21.485786	1271.652234	12.671898
21.098463	1272.989947	12.676903
21.530296	1268.734361	12.681907
21.497763	1265.543179	12.686912
20.999108	1274.673151	12.691917
21.289528	1268.520936	12.696922
21.031269	1279.413480	12.701927
21.072349	1267.854146	12.706931
21.092665	1273.018828	12.711936
21.062934	1275.406548	12.716941
21.032739	1268.673098	12.721946
21.109093	1277.359699	12.726951
21.448904	1276.204935	12.731955
21.370916	1265.736939	12.736960
21.176324	1273.506370	12.741965
21.187646	1264.049167	12.746970
21.067761	1265.478269	12.751975
21.288680	1263.918262	12.756979
21.481387	1268.259074	12.761984
21.058087	1274.980021	12.766989
20.947038	1269.163075	12.771994
20.924582	1276.495040	12.776999
21.011275	1273.201262	12.782003
21.136989	1291.844930	12.787008
21.107565	1297.452800	12.792013
21.189141	1308.053041	12.797018
21.495087	1305.396082	12.802023
21.526675	1297.165671	12.807027
21.342326	1284.502120	12.812032
21.041187	1292.815266	12.817037
21.668243	1288.760354	12.822042
21.328452	1279.488452	12.827047
21.148386	1287.356500	12.832051
21.225740	1276.105194	12.837056
21.088624	1274.165464	12.842061
21.139717	1274.455528	12.847066
21.137373	1300.443123	12.852071
21.207960	1308.042544	12.857075
21.536635	1311.476997	12.862080
21.278541	1303.696491	12.867085
21.255895	1285.525561	12.872090
21.291545	1288.334948	12.877095
21.082690	1280.869883	12.882099
21.698893	1279.749887	12.887104
21.250669	1289.844821	12.892109
21.112773	1282.945612	12.897114
21.308461	1281.541017	12.902119
21.575396	1288.864681	12.907123
21.507937	1290.692286	12.912128
21.242553	1296.413483	12.917133
21.426685	1286.725273	12.922138
21.206081	1287.236869	12.927143
20.972172	1291.940624	12.932147
21.143262	1289.730960	12.937152
20.931330	1289.384872	12.942157
20.934336	1293.755947	12.947162
20.935949	1296.553418	12.952167
21.200432	1311.275105	12.957171
21.693557	1311.180851	12.962176
21.311215	1325.849593	12.967181
21.641277	1313.674842	12.972186
21.420625	1303.202763	12.977191
21.446050	1294.484472	12.982195
21.350368	1286.263327	12.987200
21.448143	1283.373062	12.992205
21.456884	1287.651756	12.997210
21.711294	1286.933243	13.002215
21.550857	1296.991746	13.007219
21.566968	1281.506546	13.012224
21.210377	1295.232848	13.017229
21.466056	1295.047151	13.022234
21.361299	1296.890167	13.027239
20.945975	1305.037024	13.032243
21.807986	1291.339245	13.037248
21.553520	1284.201579	13.042253
21.226938	1265.970336	13.047258
21.026982	1257.303783	13.052263
20.657751	1260.707603	13.057267
21.209908	1269.422394	13.062272
21.043610	1282.221033	13.067277
21.162422	1280.617383	13.072282
21.306715	1293.218260	13.077287
21.226432	1299.739429	13.082291
21.409966	1293.413436	13.087296
20.835321	1297.319966	13.092301
21.380217	1285.104667	13.097306
21.576162	1304.189744	13.102311
21.744021	1298.280995	13.107315
21.814070	1282.131168	13.112320
21.229473	1279.005953	13.117325
21.459660	1264.633093	13.122330
21.330808	1262.453923	13.127335
21.548437	1270.791554	13.132339
21.701664	1258.802750	13.137344
21.612053	1258.577505	13.142349
21.441873	1263.747334	13.147354
21.501561	1266.981821	13.152359
21.072576	1266.350225	13.157363
22.027160	1252.402748	13.162368
21.191601	1247.557660	13.167373
21.292231	1236.655914	13.172378
21.298663	1228.467401	13.177383
21.439144	1225.964580	13.182387
21.055868	1229.769608	13.187392
20.872961	1244.398576	13.192397
21.070372	1248.979909	13.197402
21.133052	1262.418534	13.202407
21.109666	1260.105848	13.207411
21.059409	1256.750335	13.212416
20.889567	1266.321454	13.217421
21.219211	1265.830643	13.222426
21.594318	1275.062538	13.227431
21.340979	1282.183744	13.232435
21.783129	1267.210940	13.237440
21.424275	1267.172141	13.242445
21.476319	1253.739197	13.247450
21.260743	1242.946225	13.252455
21.121248	1239.699568	13.257459
21.262455	1232.412088	13.262464
20.941992	1245.440289	13.267469
21.399993	1249.436005	13.272474
21.536730	1262.430727	13.277479
21.274962	1255.305279	13.282483
21.217462	1248.185103	13.287488
21.051813	1248.946557	13.292493
21.456702	1240.073161	13.297498
21.265990	1238.279181	13.302503
21.332836	1239.265331	13.307507
21.587741	1237.796102	13.312512
21.120402	1241.236065	13.317517
21.014889	1238.084914	13.322522
21.018649	1236.400270	13.327527
21.371552	1251.024214	13.332531
21.380488	1235.357279	13.337536
21.299132	1241.045951	13.342541
21.323560	1237.522410	13.347546
21.310143	1249.582268	13.352551
21.259329	1244.613601	13.357555
21.801284	1242.997663	13.362560
21.377776	1237.750965	13.367565
21.094129	1241.667841	13.372570
21.271175	1242.716842	13.377575
21.639879	1239.542099	13.382579
21.726590	1238.676867	13.387584
21.316796	1248.268897	13.392589
21.390492	1240.104344	13.397594
21.654522	1240.775191	13.402599
21.380252	1240.309734	13.407603
21.450205	1234.131193	13.412608
21.246484	1227.485363	13.417613
21.378467	1219.436106	13.422618
21.265033	1213.547022	13.427623
21.187511	1217.112469	13.432627
21.228492	1206.931473	13.437632
21.186934	1212.501821	13.442637
21.319308	1218.597949	13.447642
21.514284	1209.674470	13.452647
21.079545	1220.218220	13.457651
21.541325	1207.434339	13.462656
21.215557	1208.848963	13.467661
21.424892	1206.417166	13.472666
21.188414	1206.415621	13.477671
21.160236	1210.137201	13.482675
21.105519	1203.712048	13.487680
21.200016	1204.559744	13.492685
21.192058	1203.436797	13.497690
21.141580	1209.011720	13.502695
21.380257	1221.075504	13.507699
21.076110	1209.382039	13.512704
21.240429	1228.486253	13.517709
21.194961	1224.015063	13.522714
20.821421	1222.893649	13.527719
20.861654	1244.550293	13.532723
21.243649	1238.430795	13.537728
21.173003	1249.999879	13.542733
21.428663	1235.104161	13.547738
21.521089	1240.318832	13.552743
21.299380	1256.013727	13.557747
21.551489	1239.128426	13.562752
21.298365	1249.610115	13.567757
21.407878	1249.815167	13.572762
21.117983	1248.461211	13.577767
20.991109	1255.566964	13.582771
21.301348	1242.718911	13.587776
21.175234	1252.358741	13.592781
20.917725	1251.062699	13.597786
20.988843	1252.943892	13.602791
20.614924	1265.908096	13.607795
21.054547	1258.445274	13.612800
20.900579	1256.246457	13.617805
21.157464	1257.916670	13.622810
20.767280	1268.503812	13.627815
21.119386	1281.878948	13.632819
21.184023	1283.754871	13.637824
21.489208	1282.249232	13.642829
21.576130	1279.836947	13.647834
21.509807	1268.890840	13.652839
21.263470	1255.578024	13.657843
21.183961	1257.241963	13.662848
21.342647	1251.719478	13.667853
21.331748	1245.225816	13.672858
21.070379	1253.461633	13.677863
20.878551	1260.729138	13.682867
21.496992	1250.074385	13.687872
21.219075	1271.102133	13.692877
21.144850	1262.301983	13.697882
21.421629	1265.763625	13.702887
21.284116	1270.565541	13.707891
21.454335	1253.710630	13.712896
21.360532	1253.695792	13.717901
21.186462	1257.391766	13.722906
21.331838	1259.753133	13.727911
21.396547	1248.010271	13.732915
21.347148	1239.669805	13.737920
21.094806	1263.705487	13.742925
21.109691	1253.762013	13.747930
21.331305	1256.062334	13.752935
21.136538	1266.553652	13.757939
21.337879	1249.214382	13.762944
21.276303	1266.692541	13.767949
21.318460	1254.729339	13.772954
21.506248	1266.522152	13.777959
21.128203	1259.945111	13.782963
21.249607	1258.098196	13.787968
21.006107	1252.770743	13.792973
21.229696	1254.533000	13.797978
21.561627	1246.893392	13.802983
21.353231	1255.928174	13.807987
21.757383	1254.312135	13.812992
21.185887	1262.043899	13.817997
21.452310	1262.772714	13.823002
21.520598	1257.889127	13.828007
21.326455	1271.119558	13.833011
21.301015	1263.320892	13.838016
21.387135	1257.210726	13.843021
21.129414	1262.377169	13.848026
21.587514	1262.537664	13.853031
21.160508	1267.505601	13.858035
21.109224	1264.476684	13.863040
21.054575	1267.775140	13.868045
21.467859	1256.005063	13.873050
21.523234	1254.720621	13.878055
21.233212	1258.471359	13.883059
21.652356	1252.563552	13.888064
21.365049	1263.252556	13.893069
21.176014	1255.233977	13.898074
21.556013	1253.367898	13.903079
21.327708	1252.037235	13.908083
21.128102	1239.155380	13.913088
21.096758	1236.620036	13.918093
21.178519	1233.429556	13.923098
21.310584	1241.222567	13.928103
21.081267	1253.706375	13.933107
21.470442	1248.990813	13.938112
21.099618	1254.806083	13.943117
21.294051	1260.215807	13.948122
21.370964	1254.545511	13.953127
21.238816	1251.220407	13.958131
21.638438	1238.044284	13.963136
21.119393	1241.224408	13.968141
21.165826	1230.151536	13.973146
21.564718	1229.135589	13.978151
20.928114	1244.631711	13.983155
21.374486	1226.942723	13.988160
20.977236	1247.008591	13.993165
21.187357	1245.841398	13.998170
21.320251	1242.552873	14.003175
21.159828	1257.504702	14.008179
21.649806	1257.264291	14.013184
21.192180	1257.040969	14.018189
21.186591	1246.918127	14.023207
21.137553	1239.475036	14.028224
21.101940	1254.568644	14.033242
21.354925	1262.383794	14.038259
21.431002	1262.604622	14.043277
21.608923	1261.649939	14.048295
21.513259	1255.024349	14.053312
21.090238	1235.999479	14.058330
21.332912	1238.611364	14.063347
21.079866	1252.385336	14.068365
21.248975	1264.780149	14.073383
21.167044	1258.172814	14.078400
21.182865	1278.639322	14.083418
21.602604	1271.456490	14.088435
21.479329	1269.914370	14.093453
21.231042	1272.802756	14.098471
21.190748	1274.162089	14.103488
20.854552	1269.364877	14.108506
21.251761	1276.716604	14.113523
21.263041	1285.687114	14.118541
21.576437	1299.974806	14.123559
21.566861	1297.668968	14.128576
21.587951	1312.602589	14.133594
21.427531	1307.313308	14.138611
21.514764	1301.657355	14.143629
21.521110	1314.427365	14.148647
21.861673	1308.380236	14.153664
21.617383	1323.587419	14.158682
21.825050	1319.213091	14.163699
21.775236	1315.395760	14.168717
21.859028	1307.604273	14.173735
21.947696	1310.800707	14.178752
21.649474	1308.492140	14.183770
21.649982	1308.058087	14.188787
21.864942	1317.136125	14.193805
21.813063	1312.771733	14.198823
21.908322	1312.107073	14.203840
21.900748	1312.893352	14.208858
22.073188	1301.866309	14.213875
21.776250	1312.314239	14.218893
21.994832	1308.553200	14.223911
21.871667	1310.518759	14.228928
21.851257	1313.602034	14.233946
22.209546	1310.100273	14.238963
22.060914	1321.251264	14.243981
21.638284	1321.232320	14.248999
21.959607	1317.385682	14.254016
21.977781	1337.960432	14.259034
22.403278	1340.434643	14.264051
21.947180	1335.994719	14.269069
22.157683	1344.475759	14.274087
22.491951	1336.943172	14.279104
22.370783	1350.582951	14.284122
22.167339	1338.201735	14.289139
22.435778	1331.181425	14.294157
22.278824	1323.088567	14.299175
22.310750	1316.703711	14.304192
21.867525	1324.611055	14.309210
22.249220	1321.171623	14.314227
22.075679	1340.661724	14.319245
22.083057	1351.869650	14.324263
22.637994	1337.080392	14.329280
22.171623	1346.979665	14.334298
22.574845	1347.676835	14.339315
22.506165	1350.393451	14.344333
22.287717	1350.944387	14.349351
22.425145	1343.965414	14.354368
22.256557	1351.050355	14.359386
22.407196	1348.555367	14.364403
22.348588	1353.161080	14.369421
22.575672	1348.772636	14.374439
22.499960	1346.216225	14.379456
22.477355	1352.625104	14.384474
22.638063	1342.225941	14.389491
22.869489	1342.283573	14.394509
22.375649	1352.149480	14.399527
22.606667	1351.600013	14.404544
22.594385	1343.592604	14.409562
22.424882	1354.514151	14.414579
22.739254	1351.401615	14.419597
22.288351	1346.438635	14.424615
22.594835	1343.026923	14.429632
22.315650	1359.650657	14.434650
22.593203	1369.447027	14.439667
22.950483	1365.025229	14.444685
22.794731	1389.413920	14.449703
23.274075	1377.681944	14.454720
22.994123	1361.163424	14.459738
22.804552	1347.362745	14.464755
22.803724	1357.527537	14.469773
22.487475	1366.605387	14.474791
22.916788	1375.548605	14.479808
22.870411	1378.774457	14.484826
22.798346	1369.467860	14.489843
22.821395	1378.982370	14.494861
22.800365	1386.680845	14.499879
23.077763	1373.436426	14.504896
22.833503	1380.019090	14.509914
23.151387	1371.587788	14.514931
23.225265	1369.016953	14.519949
22.963267	1386.548724	14.524967
23.269252	1374.094094	14.529984
23.135058	1379.293868	14.535002
23.340952	1380.060262	14.540019
23.527606	1375.676684	14.545037
23.346633	1367.222704	14.550055
23.307558	1372.860319	14.555072
23.332248	1376.213256	14.560090
23.260670	1385.769603	14.565107
23.417470	1382.517030	14.570125
23.086787	1384.061107	14.575143
23.594581	1372.102810	14.580160
23.391208	1379.212187	14.585178
23.249587	1379.738288	14.590195
23.648659	1368.351018	14.595213
23.338768	1376.367681	14.600231
23.750434	1372.852674	14.605248
23.769952	1384.041387	14.610266
23.637661	1364.306188	14.615283
23.874205	1354.160753	14.620301
23.461339	1349.139798	14.625319
23.752575	1344.333725	14.630336
23.565754	1330.038714	14.635354
23.332270	1355.819233	14.640371
23.722128	1333.893027	14.645389
23.401380	1342.433627	14.650407
23.640427	1334.620511	14.655424
23.619219	1336.462851	14.660442
23.242317	1343.105976	14.665459
23.504726	1337.873512	14.670477
23.423121	1357.721765	14.675495
23.853726	1365.938062	14.680512
23.941241	1367.207808	14.685530
23.758837	1367.046735	14.690547
23.920719	1368.345518	14.695565
23.785199	1374.327266	14.700583
24.056722	1365.088565	14.705600
23.600456	1359.670276	14.710618
23.896716	1374.203011	14.715635
24.037920	1373.755954	14.720653
23.641213	1376.101763	14.725671
23.861227	1366.501629	14.730688
23.988694	1374.616846	14.735706
24.081485	1372.793300	14.740723
23.957295	1368.959503	14.745741
24.085946	1381.406484	14.750759
23.987126	1377.109333	14.755776
24.013622	1380.177276	14.760794
24.159059	1381.890801	14.765811
24.411798	1366.811522	14.770829
24.014501	1370.050868	14.775847
24.385620	1367.943842	14.780864
24.312997	1338.654407	14.785882
24.203512	1338.266208	14.790899
23.957538	1336.416474	14.795917
23.768786	1345.873510	14.800935
24.143947	1347.441858	14.805952
24.180364	1372.230864	14.810970
24.093079	1372.507635	14.815987
24.333325	1367.780470	14.821005
24.134680	1382.425177	14.826023
23.989507	1383.431600	14.831040
24.414309	1377.166522	14.836058
24.053058	1377.243177	14.841075
24.698264	1380.055147	14.846093
24.263722	1373.570062	14.851111
24.076043	1374.051600	14.856128
24.393662	1372.149726	14.861146
24.279498	1371.499587	14.866163
24.519277	1369.931014	14.871181
24.370487	1371.516864	14.876199
24.227263	1372.019625	14.881216
24.448156	1368.439094	14.886234
24.185092	1388.808668	14.891251
24.455913	1397.785043	14.896269
24.314523	1407.759937	14.901287
24.634693	1397.094638	14.906304
24.792488	1403.361514	14.911322
24.469834	1414.785714	14.916339
24.913802	1413.787019	14.921357
24.660815	1407.859680	14.926375
24.710630	1414.798138	14.931392
24.961712	1403.454892	14.936410
24.820533	1404.534609	14.941427
24.881782	1406.399985	14.946445
25.064524	1411.621580	14.951463
24.865173	1397.932520	14.956480
25.157072	1393.351261	14.961498
24.911381	1404.546108	14.966515
25.076400	1398.644913	14.971533
24.931576	1404.020990	14.976551
24.884845	1405.331026	14.981568
25.071778	1404.203444	14.986586
24.926460	1415.228141	14.991603
24.745890	1409.836646	14.996621
24.756599	1417.221774	15.001639
24.821672	1407.168141	15.006656
25.074672	1400.269807	15.011674
24.879913	1413.926101	15.016691
25.132915	1404.575502	15.021709
25.120660	1411.228140	15.026727
24.986329	1404.380566	15.031744
24.910348	1403.455358	15.036762
25.061811	1403.392042	15.041779
25.055060	1398.031030	15.046797
25.055283	1415.179680	15.051815
25.493319	1432.971081	15.056832
25.366959	1420.171674	15.061850
25.201174	1426.678923	15.066867
25.309165	1425.103049	15.071885
25.382545	1429.414038	15.076903
25.266690	1431.324966	15.081920
25.957404	1448.500380	15.086938
25.644275	1420.987273	15.091955
25.511403	1410.704095	15.096973
25.464809	1404.455987	15.101991
25.535807	1402.576140	15.107008
25.545808	1402.458309	15.112026
25.566286	1403.619205	15.117043
25.623991	1398.603404	15.122061
26.015777	1397.042044	15.127079
25.403122	1399.475778	15.132096
25.708409	1394.212860	15.137114
25.200319	1408.502693	15.142131
25.192013	1401.822205	15.147149
25.544159	1414.990169	15.152167
25.700465	1427.192114	15.157184
25.924966	1426.723906	15.162202
25.861892	1438.094141	15.167219
26.140460	1429.212914	15.172237
26.112788	1406.544681	15.177255
25.823486	1411.534831	15.182272
26.206855	1397.000957	15.187290
25.768871	1400.624311	15.192307
26.156437	1388.306090	15.197325
25.797794	1394.224334	15.202343
25.995311	1400.338588	15.207360
26.157598	1398.577884	15.212378
25.978767	1397.898733	15.217395
25.737182	1402.870260	15.222413
25.844462	1393.796157	15.227431
25.770405	1399.757101	15.232448
25.975007	1396.361626	15.237466
25.788667	1409.510077	15.242483
26.147910	1415.604836	15.247501
25.966496	1423.739457	15.252519
26.267980	1435.265471	15.257536
26.459913	1424.115681	15.262554
26.240390	1439.761040	15.267571
26.142715	1414.126320	15.272589
26.212247	1421.818236	15.277607
26.439895	1428.835302	15.282624
26.464304	1427.714762	15.287642
26.434937	1408.840806	15.292659
26.293742	1395.239998	15.297677
26.184473	1390.846985	15.302695
26.406487	1416.199475	15.307712
26.426496	1413.170052	15.312730
26.384544	1425.615967	15.317747
26.437019	1429.749398	15.322765
26.945402	1421.817778	15.327783
26.295931	1408.971252	15.332800
26.216340	1417.190299	15.337818
26.621590	1414.834013	15.342835
26.632317	1418.517938	15.347853
26.779531	1422.444355	15.352871
26.412136	1430.596057	15.357888
26.725135	1436.927855	15.362906
26.311561	1429.291129	15.367923
26.611419	1417.554715	15.372941
26.701138	1416.713187	15.377959
26.390289	1433.521374	15.382976
26.841703	1424.924032	15.387994
26.659279	1434.587748	15.393011
26.958363	1422.801118	15.398029
26.765580	1424.883184	15.403047
26.522920	1436.382729	15.408064
26.796820	1421.098678	15.413082
26.570163	1427.952252	15.418099
26.686060	1435.226235	15.423117
27.077219	1421.142538	15.428135
26.874101	1426.633310	15.433152
26.953292	1417.241213	15.438170
27.135522	1429.368242	15.443187
27.051935	1420.365460	15.448205
27.388569	1425.191295	15.453223
27.058680	1427.966887	15.458240
27.021218	1420.133333	15.463258
26.884582	1431.475971	15.468275
27.018846	1429.298176	15.473293
26.920878	1424.931663	15.478311
26.954924	1425.137176	15.483328
26.976480	1446.715098	15.488346
26.904355	1446.072407	15.493363
27.238331	1447.574979	15.498381
27.285161	1444.336785	15.503399
27.348630	1446.514834	15.508416
27.588445	1449.800447	15.513434
27.327623	1449.612554	15.518451
27.219181	1457.439836	15.523469
27.295961	1438.224880	15.528487
27.595755	1440.066373	15.533504
27.575199	1440.919221	15.538522
27.499198	1447.372836	15.543539
27.460246	1454.047054	15.548557
27.624054	1443.859676	15.553575
27.619184	1447.898442	15.558592
27.472965	1445.582913	15.563610
27.374573	1449.210319	15.568627
27.366939	1447.635580	15.573645
27.593871	1443.487797	15.578663
27.462144	1453.519381	15.583680
27.206451	1448.009296	15.588698
27.211880	1440.118555	15.593715
27.456197	1456.185443	15.598733
27.809627	1469.867616	15.603751
27.775751	1471.301446	15.608768
27.766726	1469.384017	15.613786
27.776101	1477.566888	15.618803
27.765886	1475.003155	15.623821
27.997046	1470.576272	15.628839
27.994374	1474.959178	15.633856
27.917887	1468.673340	15.638874
27.987687	1478.411686	15.643891
27.928689	1468.904746	15.648909
28.210710	1471.949259	15.653927
27.745089	1473.332400	15.658944
27.972604	1467.078301	15.663962
28.069445	1472.598327	15.668979
27.855855	1474.350247	15.673997
28.333656	1464.984206	15.679015
28.006840	1466.776205	15.684032
28.118843	1464.024673	15.689050
28.030195	1468.812960	15.694067
28.316703	1465.059924	15.699085
28.438478	1467.104412	15.704103
28.144543	1480.331433	15.709120
28.129193	1470.845844	15.714138
28.237711	1468.475528	15.719155
28.286532	1472.021261	15.724173
28.410809	1472.725174	15.729191
28.000510	1476.045266	15.734208
28.114560	1476.316669	15.739226
28.503207	1479.523498	15.744243
28.390571	1482.678145	15.749261
28.738890	1488.181664	15.754279
28.725802	1480.169589	15.759296
28.571110	1467.413982	15.764314
28.527303	1474.093702	15.769331
28.476730	1487.347982	15.774349
28.574916	1483.480262	15.779367
28.435490	1474.546126	15.784384
28.808163	1492.156122	15.789402
28.754052	1497.294403	15.794419
28.786870	1492.010414	15.799437
28.946376	1482.216940	15.804455
28.601305	1494.513061	15.809472
28.629636	1494.801281	15.814490
28.989037	1489.641381	15.819507
28.474643	1499.988849	15.824525
29.204265	1496.217044	15.829543
29.014308	1491.561597	15.834560
29.007856	1489.421965	15.839578
29.222261	1488.332466	15.844595
29.191803	1482.136806	15.849613
29.311845	1473.331170	15.854631
29.150466	1463.356084	15.859648
28.959821	1464.643462	15.864666
29.164414	1458.819298	15.869683
28.946759	1465.503146	15.874701
28.688897	1460.827079	15.879719
29.012476	1470.738871	15.884736
28.813314	1484.930747	15.889754
28.978724	1484.569486	15.894771
28.934268	1486.105676	15.899789
29.411863	1489.309332	15.904807
29.300794	1491.313883	15.909824
28.890922	1501.333233	15.914842
29.236792	1484.821723	15.919859
29.089949	1505.502465	15.924877
29.060301	1485.827019	15.929895
29.318033	1496.273133	15.934912
29.493813	1490.002107	15.939930
29.452719	1493.794986	15.944947
29.343889	1516.909373	15.949965
29.850103	1511.055960	15.954983
29.023206	1524.441951	15.960000
29.151634	1522.532480	15.965018
29.767870	1526.396709	15.970035
29.690357	1529.014095	15.975053
29.623261	1534.225245	15.980071
29.839706	1536.171276	15.985088
29.681148	1540.297499	15.990106
30.040255	1535.585930	15.995123
29.820583	1537.974313	16.000141
30.008593	1519.298347	16.005159
29.623940	1515.605148	16.010176
29.625975	1526.334303	16.015194
30.126176	1514.891466	16.020211
30.013652	1532.575748	16.025229
29.778634	1504.309149	16.030247
29.646341	1512.744289	16.035264
29.831254	1530.613933	16.040282
29.886403	1530.698108	16.045299
29.773637	1535.274764	16.050317
29.985127	1523.901560	16.055335
29.793891	1528.534772	16.060352
29.753234	1534.116075	16.065370
29.995796	1525.894894	16.070387
30.041242	1524.753689	16.075405
30.214243	1525.144676	16.080423
29.851916	1534.178070	16.085440
29.921538	1525.811442	16.090458
30.266211	1535.620817	16.095475
29.946078	1533.403794	16.100493
30.241406	1538.344791	16.105511
30.634948	1550.070142	16.110528
30.587701	1558.285684	16.115546
30.676282	1523.642460	16.120563
30.659122	1531.601511	16.125581
30.109750	1526.328564	16.130599
30.247056	1530.571188	16.135616
30.575359	1533.331488	16.140634
30.716787	1533.780992	16.145651
30.532897	1540.756783	16.150669
30.715019	1531.003713	16.155687
30.829879	1525.152936	16.160704
30.287335	1526.685200	16.165722
30.636423	1522.456566	16.170739
30.428247	1524.575706	16.175757
30.740809	1532.809353	16.180775
31.116197	1551.214918	16.185792
30.875178	1539.388493	16.190810
31.018158	1525.234167	16.195827
30.469126	1531.695623	16.200845
30.757396	1533.856709	16.205863
31.085615	1535.520653	16.210880
30.767163	1545.456241	16.215898
30.762779	1531.606976	16.220915
31.039470	1540.285210	16.225933
30.894354	1548.544668	16.230951
31.015605	1539.136347	16.235968
31.460490	1536.780013	16.240986
31.469584	1534.362623	16.246003
31.372690	1516.112760	16.251021
31.362556	1509.750256	16.256039
31.647549	1503.402033	16.261056
31.303123	1512.261104	16.266074
31.737021	1509.400026	16.271091
31.543316	1510.418915	16.276109
31.296699	1509.522487	16.281127
31.380104	1512.126791	16.286144
31.126428	1519.477060	16.291162
31.393198	1507.659337	16.296179
31.209954	1518.556457	16.301197
31.165661	1511.269768	16.306215
31.551732	1500.014240	16.311232
31.241244	1508.908007	16.316250
31.340940	1505.205204	16.321267
31.367042	1496.621383	16.326285
31.535750	1514.544714	16.331303
31.458965	1506.256501	16.336320
31.487485	1506.258408	16.341338
31.229848	1508.583630	16.346355
31.494181	1511.486259	16.351373
31.274167	1518.063544	16.356391
31.780706	1497.026881	16.361408
31.512224	1521.908027	16.366426
31.410086	1518.954690	16.371443
31.850259	1524.964232	16.376461
31.308388	1538.948128	16.381479
31.967602	1541.414988	16.386496
31.451626	1549.241249	16.391514
31.697142	1535.325384	16.396531
31.733367	1531.005076	16.401549
32.028588	1538.563536	16.406567
32.268877	1533.793841	16.411584
31.774914	1548.695021	16.416602
31.850967	1537.934848	16.421619
31.897432	1543.827868	16.426637
31.870369	1537.387830	16.431655
32.039726	1540.851437	16.436672
31.871261	1539.156051	16.441690
32.153563	1558.940250	16.446707
32.139072	1565.303886	16.451725
32.360635	1568.079643	16.456743
32.606802	1565.429388	16.461760
32.403710	1563.516157	16.466778
32.542865	1547.809880	16.471795
32.382747	1543.267631	16.476813
32.257879	1540.448472	16.481831
32.282373	1534.300653	16.486848
32.020840	1542.526766	16.491866
32.472846	1553.888875	16.496883
32.671327	1567.133395	16.501901
32.289256	1568.092669	16.506919
32.760489	1560.126002	16.511936
32.853416	1570.356213	16.516954
32.465581	1554.320280	16.521971
32.724446	1563.061145	16.526989
32.578929	1560.898065	16.532007
33.043356	1559.568917	16.537024
32.773425	1544.988079	16.542042
32.662635	1528.189137	16.547059
32.629051	1535.302971	16.552077
32.577721	1555.829342	16.557095
32.866814	1553.074719	16.562112
32.413436	1564.062144	16.567130
32.917572	1551.572615	16.572147
33.153205	1556.309213	16.577165
32.431834	1567.820716	16.582183
32.738136	1563.493504	16.587200
32.820424	1562.890675	16.592218
33.056791	1562.838985	16.597235
33.025248	1566.861590	16.602253
32.555979	1578.647493	16.607271
33.093134	1557.785967	16.612288
32.718387	1574.599788	16.617306
32.946009	1574.321410	16.622323
33.229397	1578.987479	16.627341
33.361656	1583.531365	16.632359
33.420261	1589.408311	16.637376
33.119833	1596.530126	16.642394
33.620141	1597.196097	16.647411
33.563746	1589.865682	16.652429
33.536113	1594.089013	16.657447
33.758676	1574.525017	16.662464
33.488879	1554.836655	16.667482
33.758453	1559.605593	16.672499
33.522137	1559.023689	16.677517
33.292082	1553.855531	16.682535
33.535385	1559.223247	16.687552
33.263979	1562.802771	16.692570
33.536044	1577.273506	16.697587
33.801083	1586.463274	16.702605
33.647947	1589.717210	16.707623
33.877290	1591.735123	16.712640
33.637070	1594.615992	16.717658
33.529283	1595.319170	16.722675
33.818764	1591.979325	16.727693
33.681965	1591.307618	16.732711
34.117810	1587.960161	16.737728
33.560711	1600.499394	16.742746
34.157702	1588.221535	16.747763
34.381362	1593.949466	16.752781
33.688597	1586.612006	16.757799
34.036904	1584.804311	16.762816
34.052336	1588.710893	16.767834
33.987188	1586.066241	16.772851
33.997709	1587.612549	16.777869
33.957030	1588.325473	16.782887
34.252522	1588.130651	16.787904
34.081358	1588.070025	16.792922
34.051021	1589.039270	16.797939
34.070883	1588.683917	16.802957
33.819581	1592.430125	16.807975
34.330334	1589.525315	16.812992
34.158358	1610.297515	16.818010
34.180939	1611.948866	16.823027
34.197831	1617.319680	16.828045
34.167831	1621.453736	16.833063
34.337180	1613.907985	16.838080
34.609086	1615.146774	16.843098
34.645699	1606.565144	16.848115
34.719695	1598.924498	16.853133
34.522422	1612.693062	16.858151
34.403880	1608.863020	16.863168
34.448334	1606.776599	16.868186
34.363546	1614.287167	16.873203
34.730941	1609.289541	16.878221
34.686317	1601.276137	16.883239
34.656001	1600.988560	16.888256
34.876690	1607.544363	16.893274
34.917540	1599.893273	16.898291
34.918412	1603.806901	16.903309
34.675461	1605.923734	16.908327
34.818793	1603.494362	16.913344
35.276959	1614.114657	16.918362
35.066807	1611.865925	16.923379
35.028487	1596.751031	16.928397
34.879430	1602.398411	16.933415
35.295253	1617.140408	16.938432
35.128294	1630.309563	16.943450
34.778519	1622.756938	16.948467
35.190845	1635.445181	16.953485
35.444618	1632.306073	16.958503
35.719953	1629.577225	16.963520
35.490445	1622.349905	16.968538
35.551081	1616.575378	16.973555
35.347921	1601.282280	16.978573
35.407448	1593.511813	16.983591
35.474654	1598.610333	16.988608
35.653257	1597.874167	16.993626
35.683834	1599.662665	16.998643
35.776444	1593.223965	17.003661
35.263206	1593.203737	17.008679
35.403194	1603.193664	17.013696
35.647874	1595.453441	17.018714
35.484343	1591.177557	17.023731
35.174005	1602.280621	17.028749
35.433240	1616.592997	17.033767
35.712321	1619.216449	17.038784
35.466123	1631.150858	17.043802
35.785281	1635.534394	17.048819
35.892357	1623.104983	17.053837
35.919894	1627.048970	17.058855
35.762459	1631.912774	17.063872
36.027057	1630.750767	17.068890
35.984858	1628.865349	17.073907
35.895034	1617.049352	17.078925
35.705039	1627.140685	17.083943
35.872944	1623.011703	17.088960
35.932286	1619.197332	17.093978
35.799413	1627.275561	17.098995
35.862171	1639.113514	17.104013
36.197168	1650.130998	17.109031
36.366504	1656.086264	17.114048
36.461826	1657.790512	17.119066
36.316864	1658.457151	17.124083
36.605128	1647.169133	17.129101
36.373214	1630.107823	17.134119
36.249992	1622.338172	17.139136
36.408063	1630.659434	17.144154
36.492835	1653.250028	17.149171
37.143647	1641.532967	17.154189
36.781440	1630.754533	17.159207
36.512084	1614.064148	17.164224
36.632045	1615.193465	17.169242
36.482324	1613.268569	17.174259
36.572732	1613.842614	17.179277
36.514660	1626.204758	17.184295
36.575813	1622.097520	17.189312
36.871844	1637.022234	17.194330
36.778891	1643.423585	17.199347
37.333570	1645.043561	17.204365
36.960046	1631.808339	17.209383
36.841686	1621.571457	17.214400
36.941407	1612.937288	17.219418
36.695727	1619.182091	17.224435
36.942024	1618.798490	17.229453
36.676298	1630.913762	17.234471
36.746515	1641.251463	17.239488
37.058015	1638.866050	17.244506
36.636008	1653.759007	17.249523
36.967910	1642.512796	17.254541
36.995221	1640.674491	17.259559
36.786185	1656.334140	17.264576
37.010602	1653.570937	17.269594
37.246374	1670.359859	17.274611
37.539315	1677.715839	17.279629
37.225160	1686.019637	17.284647
37.288361	1681.259261	17.289664
37.420597	1678.493451	17.294682
37.076486	1690.528466	17.299699
37.408840	1683.500941	17.304717
37.438215	1680.985912	17.309735
37.456795	1688.700253	17.314752
37.650162	1674.174383	17.319770
37.725380	1683.062584	17.324787
37.753751	1675.941972	17.329805
37.685994	1677.247521	17.334823
37.762493	1679.294542	17.339840
37.735334	1681.573596	17.344858
37.186433	1690.245164	17.349875
37.655747	1677.860180	17.354893
37.344017	1681.263695	17.359911
37.789528	1684.115443	17.364928
38.060237	1674.927013	17.369946
38.181355	1674.305402	17.374963
38.094309	1681.556820	17.379981
37.922635	1684.713061	17.384999
37.865679	1669.652972	17.390016
37.850578	1672.040211	17.395034
37.848894	1706.781943	17.400051
38.104368	1702.297631	17.405069
38.239319	1703.995565	17.410087
38.213755	1711.208879	17.415104
38.426391	1704.246054	17.420122
38.036263	1710.037313	17.425139
38.616345	1707.481642	17.430157
38.565714	1698.766009	17.435175
38.642440	1702.919247	17.440192
38.989560	1698.028643	17.445210
38.196058	1693.812299	17.450227
38.634398	1696.506320	17.455245
38.696116	1695.220937	17.460263
38.493947	1701.696359	17.465280
38.761076	1702.835246	17.470298
38.361798	1697.983456	17.475315
38.122073	1702.553671	17.480333
38.205242	1696.945403	17.485351
38.540129	1708.137553	17.490368
38.790856	1696.146059	17.495386
38.435507	1703.149272	17.500403
38.703982	1710.823772	17.505421
38.840930	1724.199370	17.510439
38.767207	1734.544363	17.515456
39.119664	1720.342283	17.520474
39.246506	1733.102884	17.525491
39.420039	1730.254974	17.530509
38.933655	1714.030089	17.535527
38.853338	1723.337943	17.540544
39.379923	1725.881045	17.545562
39.171191	1728.821411	17.550579
39.450121	1721.882611	17.555597
39.721360	1725.372487	17.560615
39.388938	1709.885959	17.565632
39.415840	1696.415359	17.570650
39.241110	1702.972921	17.575667
39.345139	1696.390784	17.580685
39.673732	1699.970605	17.585703
39.558275	1706.160071	17.590720
39.723538	1699.914227	17.595738
39.617642	1694.068702	17.600755
39.457587	1695.544700	17.605773
39.348019	1696.488836	17.610791
39.422787	1698.709166	17.615808
39.878662	1710.372799	17.620826
39.923180	1716.769561	17.625843
39.910275	1723.180203	17.630861
39.526371	1706.058100	17.635879
39.242404	1701.694426	17.640896
39.807203	1711.275337	17.645914
39.501141	1725.687413	17.650931
39.730608	1720.180071	17.655949
40.197865	1714.600203	17.660967
39.927187	1730.532454	17.665984
40.158603	1723.299214	17.671002
39.875192	1722.993797	17.676019
40.159731	1725.937292	17.681037
40.173167	1727.967636	17.686055
39.900886	1731.627563	17.691072
40.136639	1723.948470	17.696090
40.221844	1720.158262	17.701107
40.287704	1712.595931	17.706125
40.293314	1719.134178	17.711143
40.213150	1722.083926	17.716160
40.356204	1728.660031	17.721178
40.216267	1730.283832	17.726195
40.498039	1743.546690	17.731213
40.477609	1751.556720	17.736231
40.376939	1756.170841	17.741248
40.747469	1748.898099	17.746266
40.866265	1756.698740	17.751283
40.844318	1762.107262	17.756301
40.959243	1753.719120	17.761319
40.761366	1752.462548	17.766336
40.918639	1760.776147	17.771354
40.771887	1760.470957	17.776371
40.821368	1756.897219	17.781389
40.733955	1746.324983	17.786407
40.624768	1758.942353	17.791424
40.936324	1747.908516	17.796442
41.081722	1746.034062	17.801459
40.807386	1745.451921	17.806477
40.811766	1740.376867	17.811495
40.867720	1749.049533	17.816512
41.136800	1747.238724	17.821530
40.825527	1742.586812	17.826547
40.871046	1748.692423	17.831565
41.209156	1757.461666	17.836583
41.077713	1771.943466	17.841600
41.515419	1768.262194	17.846618
41.426881	1782.672669	17.851635
41.439759	1786.774765	17.856653
41.637171	1774.706767	17.861671
41.508214	1776.843196	17.866688
41.616293	1767.801766	17.871706
41.507781	1775.718892	17.876723
41.667081	1765.034937	17.881741
41.869302	1770.184344	17.886759
41.843061	1766.171227	17.891776
41.948313	1763.862731	17.896794
41.952791	1761.088966	17.901811
41.563065	1745.427497	17.906829
41.907346	1752.201181	17.911847
41.881799	1756.937027	17.916864
41.931103	1767.109842	17.921882
41.914360	1776.885787	17.926899
41.881335	1768.447300	17.931917
42.149708	1771.385518	17.936935
42.058575	1765.223008	17.941952
41.825318	1764.884422	17.946970
42.112146	1760.690819	17.951987
41.621962	1766.136264	17.957005
42.080082	1771.960581	17.962023
42.345291	1763.765541	17.967040
42.179990	1757.256216	17.972058
42.200460	1755.982125	17.977075
42.137961	1762.795519	17.982093
42.379912	1759.209962	17.987111
42.288802	1770.164935	17.992128
42.383662	1772.577126	17.997146
42.598552	1774.460518	18.002163
42.556385	1781.099220	18.007181
42.532435	1795.667719	18.012199
42.562315	1807.091058	18.017216
42.857838	1800.752039	18.022234
42.800040	1799.216722	18.027251
42.815949	1797.501338	18.032269
42.985993	1792.594899	18.037287
42.988108	1795.852435	18.042304
43.019496	1791.513945	18.047322
43.065504	1787.077170	18.052339
42.570693	1777.474364	18.057357
42.777769	1788.748308	18.062375
42.898886	1780.782303	18.067392
42.916698	1787.211670	18.072410
43.091418	1781.346525	18.077427
43.010352	1794.236291	18.082445
43.367664	1778.822160	18.087463
43.112421	1795.864139	18.092480
42.955140	1794.354126	18.097498
43.272311	1788.299522	18.102515
43.265568	1793.949447	18.107533
43.098954	1779.625599	18.112551
43.272729	1797.247241	18.117568
43.281461	1805.181864	18.122586
43.678166	1807.272217	18.127603
43.758929	1804.089879	18.132621
43.974732	1800.917466	18.137639
43.588357	1800.998125	18.142656
43.670978	1785.196789	18.147674
43.784204	1786.737751	18.152691
43.709815	1801.764181	18.157709
43.824302	1800.169928	18.162727
43.845102	1794.719432	18.167744
43.749950	1798.321240	18.172762
43.740535	1801.893645	18.177779
43.588674	1800.747706	18.182797
44.258058	1795.250403	18.187815
44.443988	1790.781875	18.192832
44.170182	1794.287905	18.197850
44.240640	1792.014841	18.202867
44.197129	1790.887803	18.207885
44.479648	1778.526233	18.212903
44.484225	1789.080572	18.217920
44.351152	1779.070866	18.222938
44.059369	1773.056754	18.227955
44.282138	1776.485160	18.232973
44.256756	1780.970880	18.237991
44.392242	1789.218758	18.243008
44.446982	1794.833710	18.248026
44.757729	1788.714063	18.253043
44.274671	1794.375458	18.258061
44.190411	1787.599940	18.263079
44.466384	1791.282558	18.268096
44.362641	1793.196319	18.273114
44.618589	1785.562737	18.278131
44.445731	1797.850525	18.283149
44.838849	1796.803289	18.288167
44.624740	1794.401003	18.293184
44.462221	1806.952988	18.298202
44.678973	1818.272603	18.303219
44.742036	1824.754544	18.308237
44.677207	1821.619016	18.313255
44.783921	1826.901651	18.318272
45.198906	1827.033834	18.323290
45.381053	1824.623404	18.328307
45.016101	1822.869656	18.333325
45.242133	1820.131333	18.338343
45.146027	1817.823481	18.343360
45.101181	1827.294058	18.348378
45.257632	1822.158544	18.353395
45.256636	1841.156186	18.358413
45.558807	1839.456492	18.363431
45.240185	1841.022285	18.368448
45.633555	1843.273624	18.373466
45.869271	1839.341406	18.378483
45.877118	1847.391023	18.383501
45.950089	1844.988563	18.388519
45.976851	1828.055651	18.393536
45.557017	1818.783776	18.398554
45.716499	1801.705461	18.403571
45.480152	1828.092885	18.408589
46.082794	1829.387487	18.413607
45.853815	1834.808603	18.418624
45.807291	1848.046837	18.423642
45.827369	1838.791310	18.428659
46.187486	1846.092619	18.433677
46.480995	1839.142001	18.438695
46.396868	1839.512656	18.443712
45.788886	1853.104702	18.448730
46.304838	1839.941365	18.453747
46.380498	1835.915124	18.458765
46.315169	1837.210861	18.463783
46.361980	1848.714903	18.468800
46.336795	1851.674786	18.473818
46.569112	1839.417124	18.478835
46.107420	1845.778270	18.483853
46.240597	1846.501233	18.488871
46.342113	1841.283238	18.493888
46.413534	1840.002586	18.498906
46.464536	1848.831831	18.503923
46.326230	1845.523973	18.508941
46.230487	1842.665503	18.513959
46.308377	1846.286916	18.518976
46.359389	1872.255788	18.523994
46.557643	1869.948174	18.529011
46.684169	1880.748972	18.534029
46.765812	1883.586432	18.539047
46.859811	1876.279077	18.544064
46.765975	1887.686030	18.549082
46.999242	1880.115791	18.554099
47.375947	1880.669357	18.559117
47.217912	1876.619026	18.564135
47.197885	1870.539512	18.569152
47.022142	1878.616852	18.574170
47.269582	1870.402565	18.579187
46.870629	1880.948966	18.584205
46.980486	1899.851929	18.589223
47.300140	1899.851452	18.594240
47.136442	1908.057449	18.599258
47.216314	1909.902617	18.604275
47.469158	1910.655263	18.609293
47.526617	1906.026290	18.614311
47.396200	1901.790650	18.619328
47.348469	1905.828514	18.624346
47.925925	1906.087371	18.629363
48.151437	1902.919680	18.634381
47.904250	1896.714360	18.639399
48.055190	1888.903989	18.644416
47.795781	1906.118221	18.649434
48.026973	1893.118227	18.654451
48.000345	1892.139498	18.659469
47.538012	1900.688844	18.664487
47.777243	1907.366097	18.669504
47.775328	1928.981514	18.674522
48.154175	1925.067345	18.679539
48.137161	1929.125485	18.684557
48.107117	1927.195618	18.689575
48.526558	1924.267556	18.694592
48.458232	1928.878146	18.699610
48.684550	1908.559623	18.704627
48.448927	1915.463618	18.709645
48.611366	1917.190228	18.714663
49.015539	1920.242099	18.719680
48.965992	1912.328408	18.724698
49.069728	1906.200828	18.729715
48.796533	1894.061491	18.734733
48.712054	1887.613150	18.739751
48.892260	1882.023942	18.744768
48.337867	1880.567811	18.749786
48.737030	1877.732654	18.754803
48.585854	1895.145117	18.759821
48.832123	1902.187759	18.764839
49.210112	1915.507792	18.769856
49.024361	1916.689034	18.774874
49.251403	1908.754831	18.779891
49.036237	1912.842994	18.784909
48.867616	1912.577467	18.789927
49.524001	1905.984225	18.794944
49.177603	1904.284137	18.799962
49.376967	1905.202614	18.804979
49.269604	1910.145040	18.809997
49.307534	1899.571578	18.815015
49.448612	1906.706503	18.820032
49.285712	1916.150348	18.825050
49.197015	1906.289206	18.830067
49.167130	1910.244001	18.835085
49.254312	1913.269346	18.840103
49.361340	1914.407043	18.845120
49.339615	1918.250427	18.850138
49.323629	1926.878044	18.855155
49.438838	1938.901360	18.860173
49.736896	1944.672622	18.865191
49.748937	1941.468180	18.870208
49.970720	1937.827595	18.875226
49.930147	1932.243689	18.880243
50.051604	1944.604214	18.885261
49.896521	1938.525761	18.890279
50.152076	1931.504073	18.895296
50.084553	1936.120830	18.900314
49.911529	1944.974849	18.905331
50.098276	1949.082298	18.910349
50.050230	1965.850759	18.915367
50.464614	1968.142813	18.920384
50.042901	1969.048656	18.925402
50.249672	1974.675613	18.930419
50.400627	1972.973278	18.935437
50.167407	1982.359166	18.940455
50.346699	1972.032096	18.945472
50.513549	1973.204301	18.950490
50.560619	1963.486637	18.955507
50.681612	1966.747275	18.960525
50.537829	1987.660237	18.965543
50.814166	1988.360377	18.970560
50.964556	2007.121734	18.975578
50.850643	2002.381634	18.980595
51.011697	1998.857684	18.985613
50.827526	1990.289015	18.990631
50.959774	1996.102472	18.995648
51.214382	1992.967874	19.000666
51.073987	1981.788858	19.005683
51.115951	1992.062102	19.010701
50.878591	1995.464839	19.015719
51.249273	1980.653982	19.020736
51.053747	1986.839032	19.025754
51.257400	1997.193461	19.030771
51.426315	1975.633436	19.035789
51.677479	1986.296459	19.040807
51.390023	1976.152361	19.045824
51.513550	1992.728323	19.050842
51.522681	2000.058944	19.055859
51.533689	2000.870612	19.060877
51.687219	2014.874622	19.065895
51.936167	2011.740923	19.070912
51.616962	2020.292681	19.075930
51.818269	2024.399403	19.080947
52.272032	2017.273705	19.085965
51.791177	2020.781347	19.090983
52.145034	2021.664183	19.096000
52.357624	2014.803465	19.101018
52.231761	2018.364606	19.106035
52.407745	2008.151297	19.111053
52.236342	2007.192502	19.116071
52.316258	1999.173174	19.121088
52.218847	1998.834940	19.126106
52.268222	1999.105657	19.131123
52.464345	2007.392754	19.136141
52.413200	2016.601762	19.141159
52.452155	2014.278631	19.146176
52.107578	2013.482734	19.151194
52.255255	2020.427899	19.156211
52.577030	2019.683039	19.161229
52.239294	2007.295921	19.166247
52.536127	2002.680654	19.171264
52.595901	2016.602090	19.176282
52.546833	2036.142486	19.181299
52.821779	2042.634780	19.186317
52.415459	2054.514845	19.191335
52.645281	2047.278553	19.196352
52.815520	2038.418953	19.201370
52.713291	2036.802606	19.206387
53.000820	2043.835592	19.211405
53.171317	2055.416028	19.216423
53.277576	2067.525822	19.221440
53.521334	2062.458099	19.226458
53.380443	2061.829493	19.231475
53.773133	2044.317295	19.236493
53.531261	2043.520748	19.241511
53.533658	2043.901206	19.246528
53.595824	2030.917033	19.251546
53.508854	2038.039627	19.256563
53.707147	2036.914906	19.261581
53.770572	2037.954173	19.266599
53.987017	2025.256863	19.271616
53.644052	2024.463854	19.276634
53.588305	2032.067535	19.281651
54.299519	2031.886638	19.286669
54.031860	2030.949484	19.291687
53.764026	2030.278202	19.296704
54.128904	2034.075694	19.301722
54.121395	2042.112138	19.306739
54.310437	2028.047505	19.311757
53.934940	2034.881054	19.316775
54.038325	2039.093059	19.321792
54.166145	2050.395577	19.326810
54.307058	2062.690179	19.331827
54.520472	2057.037406	19.336845
54.392551	2056.361113	19.341863
54.432619	2065.832461	19.346880
54.295686	2061.656015	19.351898
54.233500	2058.183383	19.356915
54.436229	2058.917288	19.361933
54.480282	2068.476093	19.366951
54.495721	2052.771697	19.371968
54.515936	2058.013155	19.376986
54.331865	2072.568142	19.382003
54.737211	2068.967464	19.387021
54.568692	2083.239980	19.392039
54.401384	2083.424130	19.397056
54.470678	2080.471652	19.402074
54.714786	2098.159524	19.407091
55.331275	2101.819379	19.412109
55.245770	2115.298456	19.417127
55.513987	2107.486569	19.422144
55.475244	2095.451247	19.427162
55.409398	2119.581431	19.432179
56.193795	2109.013045	19.437197
55.971362	2088.559766	19.442215
56.052194	2070.578166	19.447232
55.847591	2069.674999	19.452250
56.009139	2061.735427	19.457267
55.983274	2068.175029	19.462285
55.782106	2062.067693	19.467303
56.120120	2061.238443	19.472320
55.964491	2057.201834	19.477338
55.761358	2070.001198	19.482355
55.839147	2059.081486	19.487373
55.617897	2057.668163	19.492391
55.582876	2065.726311	19.497408
55.933634	2070.095506	19.502426
55.809563	2063.582613	19.507443
55.952111	2085.658149	19.512461
55.873338	2098.738158	19.517479
55.975383	2097.630355	19.522496
56.206813	2094.093587	19.527514
56.003184	2091.714747	19.532531
56.300931	2083.275238	19.537549
56.294206	2102.377957	19.542567
56.318730	2108.443022	19.547584
56.407803	2115.962303	19.552602
56.435987	2122.608817	19.557619
56.715710	2120.649974	19.562637
56.607980	2123.687570	19.567655
56.804591	2117.766889	19.572672
56.826418	2121.792148	19.577690
56.522354	2133.117987	19.582707
56.852510	2129.493106	19.587725
56.715854	2123.666469	19.592743
56.794941	2124.259644	19.597760
57.161593	2133.960531	19.602778
57.115680	2159.747170	19.607795
57.443970	2149.149244	19.612813
57.326929	2162.617664	19.617831
57.502843	2156.196891	19.622848
57.826707	2152.305589	19.627866
57.419428	2144.785453	19.632883
57.561570	2142.969672	19.637901
57.881075	2143.233494	19.642919
57.574599	2136.153471	19.647936
57.521115	2137.875216	19.652954
57.569586	2144.417830	19.657971
57.734144	2151.528683	19.662989
57.727044	2160.170751	19.668007
57.726302	2159.178438	19.673024
57.998672	2153.659374	19.678042
57.879465	2153.253825	19.683059
58.046187	2142.381217	19.688077
58.239663	2142.438617	19.693095
58.136739	2143.095427	19.698112
58.179646	2150.716471	19.703130
57.855211	2151.240289	19.708147
58.316671	2143.512398	19.713165
58.133828	2145.169828	19.718183
58.097712	2174.492722	19.723200
58.374480	2156.184035	19.728218
58.276758	2166.113158	19.733235
58.418267	2159.131572	19.738253
58.164048	2164.777063	19.743271
58.271860	2165.961846	19.748288
58.544576	2174.625368	19.753306
58.674476	2193.811814	19.758323
58.873869	2188.581232	19.763341
58.846365	2182.798514	19.768359
59.072633	2190.766298	19.773376
59.260949	2190.066309	19.778394
59.280680	2189.915460	19.783411
59.232561	2188.408445	19.788429
59.577735	2187.773106	19.793447
59.671685	2179.328289	19.798464
59.616410	2182.536860	19.803482
59.671066	2178.485559	19.808499
60.071978	2174.276792	19.813517
59.746592	2165.205139	19.818535
59.413673	2160.196312	19.823552
59.709675	2143.383693	19.828570
59.775618	2143.063450	19.833587
59.585651	2144.482912	19.838605
59.520521	2138.114745	19.843623
60.002295	2160.886644	19.848640
59.998211	2164.958519	19.853658
59.893143	2173.762513	19.858675
60.091154	2170.629038	19.863693
60.165586	2167.249426	19.868711
59.864663	2175.030709	19.873728
60.159491	2171.027627	19.878746
59.922014	2178.259237	19.883763
60.126866	2181.917118	19.888781
60.160790	2167.612815	19.893799
59.971443	2169.318476	19.898816
60.273370	2176.616650	19.903834
60.054849	2174.734110	19.908851
60.349467	2183.304481	19.913869
60.664083	2204.463983	19.918887
60.155284	2213.502275	19.923904
60.511284	2208.721775	19.928922
60.672511	2203.728514	19.933939
60.796644	2209.598408	19.938957
60.716941	2216.732515	19.943975
60.874509	2209.930819	19.948992
60.958798	2201.419888	19.954010
60.584389	2216.381332	19.959027
60.801939	2233.886411	19.964045
60.930613	2236.551269	19.969063
61.011420	2241.894818	19.974080
61.200033	2243.200432	19.979098
61.002042	2248.196752	19.984115
61.048533	2240.586898	19.989133
61.784476	2249.565140	19.994151
61.623223	2247.912562	19.999168
61.657081	2249.640841	20.004186
61.604330	2257.601247	20.009203
61.774991	2249.345507	20.014221
62.119976	2252.682177	20.019239
61.975539	2263.539058	20.024256
62.256430	2253.700539	20.029274
62.265343	2246.658258	20.034291
61.954795	2227.351438	20.039309
62.127802	2227.794357	20.044327
62.031229	2229.851753	20.049344
62.251436	2242.110267	20.054362
62.257081	2244.920591	20.059379
62.264150	2256.602758	20.064397
62.401666	2253.227224	20.069415
61.990285	2262.928000	20.074432
62.411938	2249.362474	20.079450
62.439096	2241.634576	20.084467
62.556674	2246.410680	20.089485
62.714325	2249.289575	20.094503
62.448233	2253.304155	20.099520
62.880762	2229.389314	20.104538
62.579392	2248.866410	20.109555
62.951654	2246.414582	20.114573
63.170722	2239.568457	20.119591
62.950030	2248.320147	20.124608
63.161920	2242.546420	20.129626
63.055406	2247.410172	20.134643
62.855436	2248.049428	20.139661
63.099981	2247.941379	20.144679
63.084934	2257.594679	20.149696
63.389263	2279.647857	20.154714
63.374639	2286.208463	20.159731
63.673053	2284.136503	20.164749
63.625217	2273.620492	20.169767
63.291583	2270.905268	20.174784
63.454936	2272.499638	20.179802
63.642075	2272.367710	20.184819
63.460803	2275.310097	20.189837
63.923992	2263.765614	20.194855
63.893474	2264.997635	20.199872
64.132138	2272.579660	20.204890
63.720832	2269.905138	20.209907
63.924457	2285.232234	20.214925
64.254035	2286.188175	20.219943
63.985515	2307.357448	20.224960
63.907834	2308.972956	20.229978
64.617342	2304.109310	20.234995
64.484889	2302.931919	20.240013
64.683755	2303.414763	20.245031
64.411726	2288.234168	20.250048
64.683225	2299.985889	20.255066
64.726062	2307.718715	20.260083
64.769836	2295.648045	20.265101
64.740661	2292.395041	20.270119
64.732553	2289.085194	20.275136
64.725175	2285.893211	20.280154
64.710430	2301.215821	20.285171
64.419020	2295.792902	20.290189
64.922700	2305.009572	20.295207
64.707043	2326.960123	20.300224
64.777647	2323.257033	20.305242
65.154390	2329.956599	20.310259
65.141937	2333.229163	20.315277
65.581489	2319.517569	20.320295
65.660390	2306.920602	20.325312
65.433090	2312.198477	20.330330
65.466005	2322.709359	20.335347
65.413504	2316.809447	20.340365
65.622051	2332.036704	20.345383
65.826376	2342.633527	20.350400
66.144791	2345.803778	20.355418
66.148122	2349.670023	20.360435
65.856081	2341.521840	20.365453
66.020589	2348.724037	20.370471
65.848696	2348.479471	20.375488
65.700089	2354.618654	20.380506
66.022722	2356.300108	20.385523
66.011276	2349.467882	20.390541
66.150542	2348.348620	20.395559
66.151365	2353.563389	20.400576
66.199751	2345.535526	20.405594
66.016469	2356.419907	20.410611
66.249078	2370.730198	20.415629
66.405312	2365.960269	20.420647
66.635347	2374.367228	20.425664
66.652815	2370.293488	20.430682
66.941151	2368.797297	20.435699
66.790944	2367.556663	20.440717
67.031738	2363.340342	20.445735
66.879969	2373.043050	20.450752
66.970317	2368.838135	20.455770
67.265782	2363.894201	20.460787
67.097244	2362.239626	20.465805
67.431503	2357.340633	20.470823
67.104334	2366.873887	20.475840
67.140791	2396.528586	20.480858
67.651668	2388.727404	20.485875
67.409028	2379.252297	20.490893
67.693453	2388.586571	20.495911
67.867635	2399.516229	20.500928
68.133796	2389.956044	20.505946
68.012880	2379.871621	20.510963
67.798787	2395.768831	20.515981
68.287320	2393.640583	20.520999
68.144484	2382.455354	20.526016
67.631160	2389.727910	20.531034
67.876268	2386.329682	20.536051
67.833706	2388.652989	20.541069
67.922550	2390.403977	20.546087
68.104486	2403.066719	20.551104
68.056186	2406.731207	20.556122
68.463386	2391.807141	20.561139
67.934737	2392.885793	20.566157
68.480803	2404.077845	20.571175
68.412954	2421.431242	20.576192
68.384982	2426.156682	20.581210
68.822391	2425.512918	20.586227
68.364908	2425.379963	20.591245
68.490014	2422.433461	20.596263
68.795401	2429.422102	20.601280
69.029731	2438.681811	20.606298
69.288583	2440.198047	20.611315
68.924267	2450.860460	20.616333
69.091538	2446.529208	20.621351
69.158631	2446.923742	20.626368
69.106062	2449.703275	20.631386
69.340784	2431.408028	20.636403
69.485867	2438.636963	20.641421
69.388466	2435.814033	20.646439
69.224326	2442.197984	20.651456
69.120815	2442.504889	20.656474
69.739092	2460.715577	20.661491
69.609078	2464.413560	20.666509
70.054904	2463.277651	20.671527
70.076671	2462.495667	20.676544
70.254684	2463.949289	20.681562
70.520994	2459.071323	20.686579
70.394642	2454.768801	20.691597
69.915962	2459.783211	20.696615
70.177657	2459.445903	20.701632
70.474513	2449.953933	20.706650
70.668812	2453.693794	20.711667
70.196081	2459.496156	20.716685
70.522280	2453.339949	20.721703
70.835242	2458.662288	20.726720
70.773667	2465.281587	20.731738
70.676774	2454.334377	20.736755
70.975053	2459.844681	20.741773
70.701845	2456.233352	20.746791
70.925708	2447.044044	20.751808
70.979900	2454.731878	20.756826
71.237163	2452.534319	20.761843
71.101915	2461.709828	20.766861
71.107976	2446.733267	20.771879
71.225166	2445.980900	20.776896
70.929000	2452.643895	20.781914
71.314163	2450.289869	20.786931
71.248928	2462.453297	20.791949
71.465199	2468.444675	20.796967
71.451645	2486.864697	20.801984
71.730105	2483.190557	20.807002
71.926784	2478.425152	20.812019
71.672534	2485.302497	20.817037
71.605315	2477.189174	20.822055
71.918619	2485.674158	20.827072
71.662395	2475.933729	20.832090
72.128882	2486.397612	20.837107
71.885121	2483.510706	20.842125
72.348185	2482.003157	20.847143
72.521294	2492.117411	20.852160
72.100252	2493.125425	20.857178
72.389570	2487.707357	20.862195
72.568142	2515.280464	20.867213
72.341331	2517.348444	20.872231
72.322426	2512.012554	20.877248
72.358493	2517.750320	20.882266
72.678513	2507.483017	20.887283
72.550535	2515.445335	20.892301
72.598432	2517.965818	20.897319
72.795642	2533.231276	20.902336
72.718476	2535.284833	20.907354
73.255511	2533.229059	20.912371
72.908159	2534.103409	20.917389
72.972560	2536.129672	20.922407
73.343034	2530.303015	20.927424
73.089923	2535.451373	20.932442
73.080788	2536.147514	20.937459
73.323545	2553.483786	20.942477
73.359267	2551.166591	20.947495
73.137774	2568.459718	20.952512
73.288193	2563.932908	20.957530
73.590864	2554.220496	20.962547
73.715653	2566.468544	20.967565
73.809753	2587.223304	20.972583
74.203810	2589.788490	20.977600
74.453006	2598.599170	20.982618
74.480147	2585.998418	20.987635
74.137091	2565.652580	20.992653
74.397496	2567.283419	20.997671
74.543820	2571.414797	21.002688
74.670802	2584.017244	21.007706
74.937860	2565.764651	21.012723
74.503812	2565.632675	21.017741
74.322081	2561.894256	21.022759
74.496880	2581.707226	21.027776
74.572225	2574.504747	21.032794
74.679951	2581.968597	21.037811
74.631593	2584.491856	21.042829
74.775198	2585.390955	21.047847
74.758586	2581.481474	21.052864
74.809377	2606.580985	21.057882
75.216690	2614.802505	21.062899
75.356302	2596.015680	21.067917
75.230471	2608.073270	21.072935
75.659033	2615.965770	21.077952
75.155869	2611.477100	21.082970
75.419391	2608.388145	21.087987
75.637725	2601.458595	21.093005
75.726560	2595.878180	21.098023
75.769352	2592.655320	21.103040
75.649529	2611.541565	21.108058
76.019444	2624.957141	21.113075
76.294051	2627.135522	21.118093
76.013426	2627.392806	21.123111
76.329937	2628.582102	21.128128
75.943145	2643.857431	21.133146
76.314659	2629.115789	21.138163
76.399715	2634.163062	21.143181
76.282701	2636.536822	21.148199
76.758839	2623.824323	21.153216
76.645717	2627.654940	21.158234
76.757969	2620.910619	21.163251
76.800411	2625.570622	21.168269
76.817516	2619.597350	21.173287
76.715200	2616.858542	21.178304
76.811112	2621.392036	21.183322
76.991406	2643.914669	21.188339
76.866415	2666.952447	21.193357
76.672423	2660.951469	21.198375
76.838850	2654.237821	21.203392
76.763344	2659.900622	21.208410
77.243714	2660.386569	21.213427
77.383098	2676.263112	21.218445
77.160051	2689.772519	21.223463
77.259663	2683.797862	21.228480
77.288572	2683.225524	21.233498
77.731915	2668.732738	21.238515
77.827635	2676.008205	21.243533
78.124136	2673.208935	21.248551
78.476621	2659.118418	21.253568
78.277067	2666.444112	21.258586
78.322063	2668.461690	21.263603
78.657024	2668.668789	21.268621
78.409923	2672.049637	21.273639
78.274187	2670.922291	21.278656
78.215978	2667.533826	21.283674
78.507173	2669.096843	21.288691
78.816421	2656.790048	21.293709
78.489182	2661.483845	21.298727
78.839257	2652.273495	21.303744
78.766488	2690.555033	21.308762
79.027836	2691.996963	21.313779
79.138558	2688.798644	21.318797
78.983495	2698.571310	21.323815
79.386218	2692.932152	21.328832
79.722202	2691.593508	21.333850
79.539631	2674.410618	21.338867
79.472057	2676.630988	21.343885
79.345202	2679.204536	21.348903
80.080174	2678.780742	21.353920
79.601474	2681.319943	21.358938
79.425720	2683.223279	21.363955
79.701608	2684.696712	21.368973
79.582361	2679.419236	21.373991
79.764426	2685.783480	21.379008
79.470690	2702.215996	21.384026
79.604735	2691.870464	21.389043
79.837022	2695.675120	21.394061
79.939705	2710.787517	21.399079
80.169018	2715.423256	21.404096
80.003694	2716.228474	21.409114
79.843792	2713.719853	21.414131
80.220909	2717.469172	21.419149
80.124081	2735.824918	21.424167
80.342453	2741.105814	21.429184
80.601652	2738.455634	21.434202
80.855683	2742.408642	21.439219
80.546633	2739.145895	21.444237
80.845271	2747.824507	21.449255
81.093353	2737.505591	21.454272
81.107917	2757.445032	21.459290
81.293316	2759.986104	21.464307
81.741724	2756.224232	21.469325
81.741361	2752.205928	21.474343
81.677990	2728.448006	21.479360
81.507132	2729.055895	21.484378
81.387230	2723.543327	21.489395
81.736874	2733.380260	21.494413
81.737314	2753.884337	21.499431
82.204251	2752.689983	21.504448
81.976474	2752.518818	21.509466
81.840605	2762.618820	21.514483
82.078389	2758.102402	21.519501
82.122045	2754.797566	21.524519
82.239169	2759.061863	21.529536
82.300672	2758.131160	21.534554
82.245615	2753.642564	21.539571
82.507246	2749.762604	21.544589
82.422283	2761.170400	21.549607
82.587655	2757.290057	21.554624
82.633628	2752.926144	21.559642
82.456836	2747.815130	21.564659
82.576474	2740.917770	21.569677
82.651961	2756.794366	21.574695
82.924724	2766.689989	21.579712
82.830078	2776.835340	21.584730
82.742463	2787.357913	21.589747
82.854811	2776.799476	21.594765
82.827674	2782.707883	21.599783
83.202411	2801.105712	21.604800
83.347906	2813.861145	21.609818
83.299759	2798.900732	21.614835
83.454609	2812.190320	21.619853
83.407046	2824.534501	21.624871
83.800929	2797.993845	21.629888
83.733436	2812.345350	21.634906
83.879714	2828.818748	21.639923
83.815952	2835.066519	21.644941
83.934452	2847.053095	21.649959
84.344337	2824.457600	21.654976
84.194388	2835.051499	21.659994
83.614828	2839.634568	21.665011
84.096365	2844.518010	21.670029
84.175363	2856.302454	21.675047
84.232485	2862.010255	21.680064
84.411098	2860.132725	21.685082
84.923072	2851.998410	21.690099
85.091892	2844.123326	21.695117
85.095191	2849.264728	21.700135
85.449667	2854.247878	21.705152
85.420532	2844.798198	21.710170
85.195270	2846.937552	21.715187
85.465451	2841.143284	21.720205
85.611895	2847.562834	21.725223
85.628021	2843.074657	21.730240
85.991671	2840.287460	21.735258
85.593380	2844.752743	21.740275
85.531391	2848.312551	21.745293
85.117010	2846.517785	21.750311
85.860675	2856.258935	21.755328
86.376505	2868.028003	21.760346
86.312316	2865.114744	21.765363
86.180403	2844.701021	21.770381
86.353638	2842.397248	21.775399
85.993322	2842.025406	21.780416
86.253699	2852.313984	21.785434
86.268590	2881.564098	21.790451
86.825304	2858.354426	21.795469
86.695285	2862.033632	21.800487
86.673770	2865.550809	21.805504
87.061985	2868.448123	21.810522
86.913288	2868.560093	21.815539
86.982494	2857.187305	21.820557
86.904088	2862.332301	21.825575
87.044382	2858.462223	21.830592
87.199283	2858.199357	21.835610
87.013395	2864.409197	21.840627
87.116455	2853.220574	21.845645
87.126732	2861.271153	21.850663
87.010808	2857.076966	21.855680
87.531004	2874.495233	21.860698
87.272679	2877.696220	21.865715
87.561001	2883.643247	21.870733
87.361697	2890.568651	21.875751
87.457214	2890.809218	21.880768
87.471515	2907.472075	21.885786
87.695180	2920.684717	21.890803
87.614446	2918.327043	21.895821
88.079797	2918.341097	21.900839
88.271880	2937.734916	21.905856
88.356153	2937.853786	21.910874
88.389198	2946.951636	21.915891
88.609590	2936.936678	21.920909
88.791548	2941.031803	21.925927
88.847356	2940.154697	21.930944
89.199761	2938.485415	21.935962
89.162719	2939.788537	21.940979
89.126861	2938.072621	21.945997
88.948662	2938.757199	21.951015
89.012318	2935.795223	21.956032
89.117828	2929.475795	21.961050
89.025924	2934.235191	21.966067
89.476205	2958.316713	21.971085
89.629210	2958.479682	21.976103
89.720962	2954.621252	21.981120
89.920129	2963.284393	21.986138
89.750176	2968.632801	21.991155
89.662769	2960.450063	21.996173
90.135216	2953.401169	22.001191
89.691607	2952.970240	22.006208
89.977546	2952.729739	22.011226
89.959423	2951.107742	22.016243
90.197373	2964.746041	22.021261
90.383251	2986.192288	22.026279
90.117865	2980.473142	22.031296
90.768740	2977.636186	22.036314
90.828214	2988.365913	22.041331
90.745091	2977.367345	22.046349
90.695873	2979.958455	22.051367
90.481558	2987.558816	22.056384
91.066528	2969.365932	22.061402
90.954791	2979.658879	22.066419
90.935365	2986.138762	22.071437
91.343881	3001.194827	22.076455
91.473501	2998.795730	22.081472
91.530028	3009.089396	22.086490
91.253427	3020.358052	22.091507
91.520661	3012.919464	22.096525
91.454413	3006.993933	22.101543
91.610862	3004.393128	22.106560
91.672776	2999.170023	22.111578
91.668880	3005.406748	22.116595
91.940541	3029.258088	22.121613
92.028179	3025.507270	22.126631
92.039716	3040.229458	22.131648
92.082662	3036.780729	22.136666
92.180300	3032.586259	22.141683
92.279479	3029.735013	22.146701
92.265475	3039.029987	22.151719
92.448218	3056.650945	22.156736
92.957241	3061.615030	22.161754
93.003086	3064.804524	22.166771
92.889258	3066.005061	22.171789
93.353641	3062.612616	22.176807
93.326427	3053.927044	22.181824
93.401580	3055.610292	22.186842
93.183026	3073.303913	22.191859
93.301331	3067.214425	22.196877
93.711378	3062.802591	22.201895
93.278750	3071.455635	22.206912
93.513185	3068.366504	22.211930
93.742285	3085.619068	22.216947
93.709275	3086.939651	22.221965
93.925377	3077.308344	22.226983
93.697937	3086.401409	22.232000
94.020678	3084.345914	22.237018
93.971679	3081.701558	22.242035
94.050721	3088.525250	22.247053
94.580740	3103.360683	22.252071
94.326780	3120.764254	22.257088
94.441606	3121.173220	22.262106
94.394569	3126.587036	22.267123
94.165457	3121.051615	22.272141
94.346973	3127.053529	22.277159
94.595403	3139.535624	22.282176
94.998840	3146.370542	22.287194
95.111694	3149.767252	22.292211
95.124080	3142.366877	22.297229
95.448286	3136.872217	22.302247
95.419817	3148.471884	22.307264
95.533479	3139.615133	22.312282
95.399520	3143.122777	22.317299
95.786619	3131.814711	22.322317
95.673168	3142.247269	22.327335
95.717098	3159.372131	22.332352
95.968970	3161.739067	22.337370
95.708972	3172.353904	22.342387
95.992309	3163.817752	22.347405
96.248740	3167.859378	22.352423
95.946806	3170.918718	22.357440
96.259007	3165.230104	22.362458
96.585518	3169.730145	22.367475
96.514727	3186.618480	22.372493
96.840784	3190.581364	22.377511
96.615218	3189.473020	22.382528
96.939103	3183.243728	22.387546
96.873723	3183.353426	22.392563
96.766520	3181.865955	22.397581
97.127820	3179.009851	22.402599
96.635967	3198.931540	22.407616
97.108264	3203.181022	22.412634
97.495481	3205.185007	22.417651
97.626124	3206.147567	22.422669
97.626459	3218.231950	22.427687
97.600461	3222.411444	22.432704
97.906046	3224.300236	22.437722
97.906837	3209.952998	22.442739
97.857280	3217.958253	22.447757
97.962808	3204.266848	22.452775
98.151516	3218.992429	22.457792
98.471616	3227.083476	22.462810
98.797547	3225.115551	22.467827
98.973331	3228.779909	22.472845
98.735019	3213.883215	22.477863
98.535759	3215.813964	22.482880
98.789034	3212.385929	22.487898
99.122272	3225.088976	22.492915
98.884594	3230.069145	22.497933
99.215006	3220.088365	22.502951
98.918250	3228.775683	22.507968
99.070095	3235.615366	22.512986
98.998053	3223.752748	22.518003
99.001424	3231.237505	22.523021
99.179662	3237.313927	22.528039
99.474523	3255.457632	22.533056
99.797308	3255.807484	22.538074
99.704161	3261.212971	22.543091
99.694827	3268.335584	22.548109
100.262982	3251.165236	22.553127
99.988690	3261.360807	22.558144
100.147585	3282.037007	22.563162
100.364482	3279.796997	22.568179
100.547036	3270.755346	22.573197
100.316495	3262.466261	22.578215
100.431100	3290.185544	22.583232
100.897270	3271.867285	22.588250
100.970833	3268.613412	22.593267
100.825704	3279.229674	22.598285
101.079121	3254.755714	22.603303
101.048794	3283.879340	22.608320
101.208025	3253.790799	22.613338
101.153434	3274.323262	22.618355
101.222829	3256.544962	22.623373
101.619324	3260.446293	22.628391
101.362992	3302.262158	22.633408
101.653033	3281.136325	22.638426
101.872888	3278.097458	22.643443
101.665853	3288.123433	22.648461
101.722324	3285.024092	22.653479
101.694761	3292.799345	22.658496
101.770752	3283.413635	22.663514
102.276656	3299.286690	22.668531
102.221878	3321.328710	22.673549
102.336120	3321.407408	22.678567
102.098602	3323.684078	22.683584
102.056613	3318.992643	22.688602
102.437336	3325.956337	22.693619
102.469768	3348.247998	22.698637
102.374953	3351.274349	22.703655
102.611380	3357.450092	22.708672
102.766444	3363.096850	22.713690
102.720001	3368.830803	22.718707
102.669494	3375.820807	22.723725
103.311419	3380.511317	22.728743
103.765120	3394.585213	22.733760
103.947541	3394.332897	22.738778
104.058893	3398.791805	22.743795
104.174084	3399.887417	22.748813
104.298829	3385.280331	22.753831
104.270711	3393.894232	22.758848
104.316780	3397.977333	22.763866
104.510619	3389.006177	22.768883
104.538796	3383.423336	22.773901
104.858559	3382.243753	22.778919
104.528376	3387.621795	22.783936
104.767957	3387.798497	22.788954
104.831057	3373.431723	22.793971
104.843613	3381.711124	22.798989
105.417191	3377.196036	22.804007
105.244743	3371.584622	22.809024
105.458849	3374.812642	22.814042
105.423086	3371.719338	22.819059
105.314240	3376.388760	22.824077
105.432738	3367.572004	22.829095
105.316358	3371.397828	22.834112
105.290968	3366.072098	22.839130
105.820601	3382.787047	22.844147
105.324250	3405.799466	22.849165
106.058167	3408.420736	22.854183
105.982131	3396.474449	22.859200
106.012676	3402.012863	22.864218
105.934583	3400.539605	22.869235
106.013261	3416.506870	22.874253
106.275344	3430.401335	22.879271
106.355260	3434.686710	22.884288
106.372390	3432.356608	22.889306
106.966976	3431.571333	22.894323
106.701973	3441.155937	22.899341
106.712033	3438.507604	22.904359
106.803320	3448.855033	22.909376
106.986184	3456.518946	22.914394
107.301122	3468.786991	22.919411
107.119124	3477.641007	22.924429
107.033156	3469.710250	22.929447
107.044894	3480.455031	22.934464
107.365230	3495.576800	22.939482
107.413427	3491.534031	22.944499
107.519522	3503.962049	22.949517
107.632932	3513.889885	22.954535
107.959180	3516.380317	22.959552
107.908440	3528.622555	22.964570
108.153676	3512.886236	22.969587
108.245964	3527.847752	22.974605
108.540116	3536.065033	22.979623
108.783143	3550.645420	22.984640
108.716956	3554.420025	22.989658
109.339214	3538.694355	22.994675
109.335522	3551.976863	22.999693
109.530006	3540.814041	23.004711
109.232272	3547.270902	23.009728
109.220233	3542.555741	23.014746
109.618316	3545.312394	23.019763
109.430965	3548.788530	23.024781
109.391273	3538.162541	23.029799
109.636807	3535.462486	23.034816
109.769801	3546.365752	23.039834
110.146405	3548.571277	23.044851
109.891395	3557.716226	23.049869
110.108145	3553.272141	23.054887
110.200411	3557.237010	23.059904
110.172199	3559.862629	23.064922
110.393631	3561.810508	23.069939
110.400898	3560.941105	23.074957
110.497677	3574.004669	23.079975
110.748883	3572.520576	23.084992
110.579072	3598.453013	23.090010
111.054802	3587.769974	23.095027
110.808491	3593.539032	23.100045
111.144738	3600.504444	23.105063
111.011153	3614.454309	23.110080
111.384213	3612.227893	23.115098
111.505565	3613.805514	23.120115
111.384778	3619.396459	23.125133
111.481291	3613.250437	23.130151
112.027629	3629.212587	23.135168
112.081461	3649.733007	23.140186
112.133991	3645.255299	23.145203
112.154711	3648.521295	23.150221
112.134931	3650.630358	23.155239
112.389707	3641.290639	23.160256
112.321930	3649.923601	23.165274
112.684891	3647.067145	23.170291
112.423318	3648.985074	23.175309
112.745704	3648.763140	23.180327
112.650014	3660.458884	23.185344
112.567755	3670.193844	23.190362
113.004542	3659.682938	23.195379
113.077178	3672.553788	23.200397
112.951957	3665.246670	23.205415
113.404628	3689.513878	23.210432
113.424598	3696.368513	23.215450
113.863727	3685.990151	23.220467
113.553612	3697.706743	23.225485
113.745529	3700.249304	23.230503
113.945621	3691.632514	23.235520
113.870237	3709.339471	23.240538
114.317058	3714.279881	23.245555
114.009065	3716.648081	23.250573
114.049157	3718.758620	23.255591
114.390081	3716.200644	23.260608
114.513072	3744.719435	23.265626
114.549285	3752.707374	23.270643
114.966635	3758.171661	23.275661
115.068808	3747.131954	23.280679
115.193183	3745.359716	23.285696
115.124812	3759.794099	23.290714
115.581553	3764.420658	23.295731
115.686827	3760.942155	23.300749
115.590397	3767.627383	23.305767
115.897879	3767.932495	23.310784
115.913838	3766.153943	23.315802
115.919853	3763.504624	23.320819
115.991887	3771.159630	23.325837
115.964885	3770.724383	23.330855
116.484076	3766.550589	23.335872
116.443288	3791.907447	23.340890
116.411581	3793.697494	23.345907
116.680123	3800.289931	23.350925
116.233499	3803.063330	23.355943
116.821522	3798.804611	23.360960
116.806307	3809.933866	23.365978
116.991847	3814.790900	23.370995
117.345154	3827.806708	23.376013
117.477960	3826.749723	23.381031
117.502764	3820.150159	23.386048
117.428854	3820.909393	23.391066
117.202456	3828.361870	23.396083
118.113985	3825.555570	23.401101
117.559115	3830.506282	23.406119
117.964839	3837.662105	23.411136
117.967914	3855.404712	23.416154
118.138777	3854.304686	23.421171
118.356007	3857.735263	23.426189
118.004561	3856.049894	23.431207
118.477447	3848.489993	23.436224
118.496699	3850.303387	23.441242
118.722656	3858.903009	23.446259
119.007270	3880.382027	23.451277
118.991301	3876.715161	23.456295
119.295719	3871.866053	23.461312
119.427651	3878.266348	23.466330
119.426266	3875.795178	23.471347
119.268331	3862.876721	23.476365
119.518850	3871.040581	23.481383
119.558880	3862.214014	23.486400
119.557482	3889.185979	23.491418
119.652620	3892.488147	23.496435
119.896153	3889.171638	23.501453
119.905385	3902.488587	23.506471
120.153372	3907.135106	23.511488
120.523655	3918.964427	23.516506
120.597006	3914.819989	23.521523
120.732740	3920.364640	23.526541
120.667663	3927.351724	23.531559
120.804115	3920.775217	23.536576
120.888550	3937.842616	23.541594
120.867464	3922.312728	23.546611
120.901470	3929.969948	23.551629
120.874589	3939.157420	23.556647
121.285978	3959.813987	23.561664
121.872128	3947.394312	23.566682
121.621182	3946.668319	23.571699
121.983560	3960.673158	23.576717
122.377749	3973.067439	23.581735
122.349658	3968.150178	23.586752
122.062843	3975.182866	23.591770
122.277216	3971.918972	23.596787
122.445284	3960.350212	23.601805
122.108906	3966.467304	23.606823
122.652922	3970.078643	23.611840
122.638666	3989.560255	23.616858
122.869650	3999.136146	23.621875
122.977069	4003.450342	23.626893
122.585073	4008.014867	23.631911
123.121954	4000.370743	23.636928
123.167868	4016.958242	23.641946
123.164278	4027.636646	23.646963
123.504455	4023.792603	23.651981
123.250291	4029.164262	23.656999
123.611158	4035.656343	23.662016
123.543244	4064.104722	23.667034
123.998743	4063.303841	23.672051
124.289230	4061.190428	23.677069
124.355484	4066.577087	23.682087
124.909024	4045.964287	23.687104
124.546154	4059.108654	23.692122
124.787727	4051.419554	23.697139
124.761915	4063.889533	23.702157
124.809880	4067.563472	23.707175
125.316283	4073.009748	23.712192
125.467030	4080.335355	23.717210
125.676393	4068.732394	23.722227
125.774924	4068.126876	23.727245
125.743605	4074.229196	23.732263
125.974506	4063.096356	23.737280
126.273437	4060.456129	23.742298
125.841743	4068.756408	23.747315
125.981069	4048.025578	23.752333
126.191605	4060.391793	23.757351
126.179379	4058.408457	23.762368
126.414242	4064.567446	23.767386
126.572882	4066.066803	23.772403
126.687686	4081.263644	23.777421
126.623238	4102.006509	23.782439
126.704010	4093.980390	23.787456
126.909301	4092.227461	23.792474
126.616811	4094.358045	23.797491
126.795108	4097.949854	23.802509
126.949114	4115.052778	23.807527
127.055323	4121.203986	23.812544
127.130634	4142.295128	23.817562
127.528958	4153.352415	23.822579
128.013741	4159.697360	23.827597
127.366122	4170.248071	23.832615
127.963175	4163.418663	23.837632
128.553563	4181.403914	23.842650
128.248672	4183.926659	23.847667
128.666331	4179.180538	23.852685
128.487713	4184.094972	23.857703
128.497273	4180.979323	23.862720
128.505617	4193.192243	23.867738
128.719214	4211.962101	23.872755
129.291695	4201.912956	23.877773
128.784132	4216.032363	23.882791
129.146679	4223.682191	23.887808
129.710201	4229.660626	23.892826
130.026127	4235.614037	23.897843
130.027772	4228.550719	23.902861
130.222390	4242.978257	23.907879
130.274664	4232.768178	23.912896
130.153099	4229.704892	23.917914
130.273875	4238.311283	23.922931
130.525210	4223.202542	23.927949
130.582986	4236.534868	23.932967
130.603866	4253.049536	23.937984
130.749789	4260.338244	23.943002
131.156425	4257.592706	23.948019
131.137985	4261.344146	23.953037
131.056417	4260.207249	23.958055
131.092191	4262.738621	23.963072
131.240961	4262.034622	23.968090
131.517239	4286.379721	23.973107
131.622850	4286.086936	23.978125
131.502778	4291.794444	23.983143
131.750480	4300.584374	23.988160
131.858995	4276.275770	23.993178
131.823830	4299.237290	23.998195
132.477090	4306.589085	24.003213
132.400885	4309.585918	24.008231
132.696095	4305.250243	24.013248
132.394866	4312.017930	24.018266
132.350792	4310.470717	24.023283
132.891618	4316.527538	24.028301
133.003985	4336.652562	24.033319
132.957116	4349.148953	24.038336
133.394090	4328.647169	24.043354
133.187130	4344.617725	24.048371
133.300537	4344.775229	24.053389
133.383508	4365.302233	24.058407
133.656381	4362.934354	24.063424
133.739928	4370.325886	24.068442
134.028803	4387.854441	24.073459
134.291818	4388.163513	24.078477
134.248328	4401.670251	24.083495
134.340524	4405.767519	24.088512
134.439971	4396.426916	24.093530
134.395284	4421.554997	24.098547
134.923564	4420.886452	24.103565
134.728280	4428.970669	24.108583
134.964455	4431.938960	24.113600
135.366513	4442.280808	24.118618
135.454985	4454.474877	24.123635
135.948283	4446.735997	24.128653
135.693605	4457.754461	24.133671
135.811116	4456.602327	24.138688
136.425831	4456.174874	24.143706
136.392636	4447.951190	24.148723
136.276462	4446.519296	24.153741
136.477193	4456.602981	24.158759
136.496814	4462.765779	24.163776
137.030767	4479.264189	24.168794
136.832915	4477.745410	24.173811
137.219212	4476.419835	24.178829
137.346672	4477.361750	24.183847
137.159171	4479.777722	24.188864
137.472007	4467.143957	24.193882
137.280484	4468.296421	24.198899
137.300503	4476.310150	24.203917
137.482193	4489.497085	24.208935
137.832379	4484.032400	24.213952
137.842383	4486.375190	24.218970
137.485746	4501.056859	24.223987
137.949058	4522.822992	24.229005
137.790191	4522.315135	24.234023
137.901787	4525.224644	24.239040
138.365451	4536.650185	24.244058
138.389888	4557.587985	24.249075
138.644517	4546.093856	24.254093
138.795567	4557.889427	24.259111
138.863028	4576.172512	24.264128
139.424810	4579.946374	24.269146
139.239386	4585.343460	24.274163
139.278133	4585.824387	24.279181
139.692004	4589.324479	24.284199
139.656142	4596.175064	24.289216
140.010769	4602.382839	24.294234
139.856839	4614.009176	24.299251
140.255030	4605.711117	24.304269
140.237078	4620.983178	24.309287
140.527412	4630.192092	24.314304
140.896604	4635.180598	24.319322
140.696201	4642.424022	24.324339
140.794446	4638.588503	24.329357
140.792303	4637.265848	24.334375
141.104073	4652.008655	24.339392
141.543374	4648.866869	24.344410
141.536710	4665.429660	24.349427
141.636037	4661.183325	24.354445
142.070312	4664.433171	24.359463
141.605648	4662.527395	24.364480
142.196182	4674.256135	24.369498
141.944615	4692.803417	24.374515
142.087767	4695.726021	24.379533
142.402923	4690.630285	24.384551
141.882232	4701.268119	24.389568
142.464578	4718.047789	24.394586
142.453954	4719.765361	24.399603
142.517156	4734.694989	24.404621
142.844947	4753.372600	24.409639
142.878701	4755.290780	24.414656
143.650933	4761.490255	24.419674
143.584919	4783.370277	24.424691
143.764588	4771.430872	24.429709
144.260462	4769.646481	24.434727
144.039472	4774.967493	24.439744
144.120720	4782.174733	24.444762
144.336978	4777.336242	24.449779
144.403564	4806.759749	24.454797
144.667645	4800.580222	24.459815
144.708718	4809.802245	24.464832
145.052496	4800.588417	24.469850
144.875897	4785.242890	24.474867
144.735414	4815.726030	24.479885
145.482515	4830.591557	24.484903
145.238822	4828.617487	24.489920
145.745284	4821.833691	24.494938
145.759217	4820.676804	24.499955
146.073780	4839.790877	24.504973
146.446263	4852.078448	24.509991
146.623887	4838.339411	24.515008
146.697425	4836.386349	24.520026
146.671964	4833.605761	24.525043
146.932266	4834.386493	24.530061
147.215248	4838.816906	24.535079
146.822323	4841.000580	24.540096
147.202655	4842.625153	24.545114
147.082577	4844.640245	24.550131
147.166462	4835.593700	24.555149
147.296868	4844.349166	24.560167
147.125141	4848.594051	24.565184
147.381396	4856.733950	24.570202
147.499347	4870.872250	24.575219
147.485405	4873.937152	24.580237
147.945234	4886.322533	24.585255
147.671225	4903.295592	24.590272
148.137642	4904.473777	24.595290
148.414097	4915.119977	24.600307
148.669858	4925.238479	24.605325
148.957389	4930.139413	24.610343
148.528429	4930.505332	24.615360
148.912425	4936.396259	24.620378
148.773326	4947.609849	24.625395
148.655795	4969.061756	24.630413
149.218630	4974.986332	24.635431
149.245284	4991.342788	24.640448
149.439688	4991.424452	24.645466
149.767772	5015.815999	24.650483
150.083754	5022.985145	24.655501
150.291050	5019.476707	24.660519
150.311376	5027.028906	24.665536
150.952884	5041.291580	24.670554
150.975660	5057.393842	24.675571
151.012441	5052.275497	24.680589
151.595672	5042.027405	24.685607
151.343416	5043.198248	24.690624
151.557325	5040.709076	24.695642
151.574132	5040.103963	24.700659
151.645658	5053.466306	24.705677
151.791158	5077.373362	24.710695
151.840278	5089.121103	24.715712
152.019340	5067.082902	24.720730
152.159541	5080.624697	24.725747
152.366536	5095.971523	24.730765
152.699066	5097.698150	24.735783
152.543765	5108.927819	24.740800
152.814293	5106.494904	24.745818
152.760114	5106.757806	24.750835
152.711385	5122.063614	24.755853
153.377455	5119.977497	24.760871
153.510799	5134.101009	24.765888
153.509830	5134.676395	24.770906
153.603797	5148.375095	24.775923
153.373007	5158.709789	24.780941
153.750411	5158.669449	24.785959
153.740921	5185.645086	24.790976
153.914138	5184.727888	24.795994
154.510016	5184.768360	24.801011
154.594801	5198.890236	24.806029
154.721340	5208.611017	24.811047
154.288837	5225.353254	24.816064
154.814663	5216.263549	24.821082
155.257641	5218.657002	24.826099
155.224904	5234.256174	24.831117
155.849774	5243.109263	24.836135
155.906822	5242.847804	24.841152
156.370288	5243.637077	24.846170
156.458058	5248.333173	24.851187
156.509924	5232.623488	24.856205
156.597831	5235.886207	24.861223
156.754346	5238.208118	24.866240
156.530807	5230.191349	24.871258
157.154223	5224.088095	24.876275
156.897043	5237.609215	24.881293
157.242576	5251.535379	24.886311
157.315057	5258.549937	24.891328
157.023123	5260.959870	24.896346
157.347345	5267.934298	24.901363
157.343926	5278.353975	24.906381
157.406422	5289.460948	24.911399
157.641317	5299.338374	24.916416
158.208197	5305.323018	24.921434
158.492992	5313.176198	24.926451
158.327791	5327.133513	24.931469
158.405804	5319.635039	24.936487
158.962845	5335.628826	24.941504
158.628544	5350.718432	24.946522
158.815737	5356.841514	24.951539
158.796415	5353.340020	24.956557
159.551872	5361.801042	24.961575
159.285717	5372.972276	24.966592
159.519543	5373.436288	24.971610
159.758818	5380.361377	24.976627
159.510060	5390.924879	24.981645
160.108016	5392.761058	24.986663
160.346498	5411.927343	24.991680
160.384913	5422.732229	24.996698
160.437451	5429.307923	25.001715
160.869348	5433.804460	25.006733
160.855461	5428.198441	25.011751
160.767904	5464.312776	25.016768
161.041850	5461.632235	25.021786
161.449984	5454.309205	25.026803
160.810614	5490.126882	25.031821
161.267528	5492.285295	25.036839
161.637226	5505.181984	25.041856
161.583286	5513.660425	25.046874
162.313760	5523.208819	25.051891
162.240611	5539.943680	25.056909
163.075200	5541.366107	25.061927
162.580096	5556.033135	25.066944
162.684134	5549.578291	25.071962
163.418596	5543.280981	25.076979
163.466124	5546.412533	25.081997
163.748645	5539.332913	25.087015
163.763043	5544.832229	25.092032
163.759224	5543.594724	25.097050
164.064879	5550.520325	25.102067
164.132417	5568.710228	25.107085
164.442163	5566.985319	25.112103
164.578732	5584.825164	25.117120
164.396939	5585.891982	25.122138
164.744960	5566.647241	25.127155
164.713927	5579.662953	25.132173
164.648538	5579.733333	25.137191
165.091085	5590.189909	25.142208
165.259504	5595.338204	25.147226
165.238028	5602.457591	25.152243
165.353122	5628.310420	25.157261
165.740462	5627.984496	25.162279
165.618505	5636.499813	25.167296
165.870464	5635.262431	25.172314
166.008590	5655.651850	25.177331
166.045279	5664.169425	25.182349
166.107889	5666.525258	25.187367
166.551792	5694.558477	25.192384
166.688961	5696.775766	25.197402
166.920062	5690.351740	25.202419
166.830789	5711.891480	25.207437
167.380609	5725.392167	25.212455
167.575695	5723.254399	25.217472
167.503112	5741.581716	25.222490
167.971067	5749.122711	25.227507
168.008188	5758.213003	25.232525
168.291394	5752.563428	25.237543
168.561196	5759.864602	25.242560
168.751314	5766.483810	25.247578
169.136484	5781.726635	25.252595
169.064281	5778.626831	25.257613
169.362688	5773.250964	25.262631
169.440084	5783.868169	25.267648
169.175132	5787.051949	25.272666
169.605390	5803.888586	25.277683
169.676298	5813.297655	25.282701
169.940534	5814.320128	25.287719
169.918919	5809.383909	25.292736
169.560514	5841.330238	25.297754
169.862051	5842.251573	25.302771
169.995282	5859.027059	25.307789
170.334400	5874.143578	25.312807
170.534980	5880.858723	25.317824
170.555086	5889.976198	25.322842
170.985653	5895.312529	25.327859
171.116419	5917.051932	25.332877
171.797961	5929.686075	25.337895
171.931907	5929.438307	25.342912
171.807479	5933.104009	25.347930
172.193513	5926.201238	25.352947
172.083800	5927.194437	25.357965
172.672206	5948.492738	25.362983
172.737802	5942.650420	25.368000
172.797209	5952.318672	25.373018
173.092979	5953.403000	25.378035
173.058548	5951.941403	25.383053
173.067507	5946.060122	25.388071
173.484735	5959.354013	25.393088
173.623130	5968.311852	25.398106
173.870742	5968.777622	25.403123
173.753426	5978.836748	25.408141
174.156474	5979.277737	25.413159
174.156127	5997.308271	25.418176
174.513714	6008.987900	25.423194
174.925896	5998.047350	25.428211
174.507821	6007.545513	25.433229
174.618049	6018.708365	25.438247
174.821682	6030.620253	25.443264
174.857987	6036.044667	25.448282
175.287603	6058.788500	25.453299
175.258763	6058.665810	25.458317
175.549700	6080.574244	25.463335
176.102815	6083.005358	25.468352
176.122491	6096.454014	25.473370
176.371681	6087.178158	25.478387
176.570799	6099.802818	25.483405
176.664737	6103.760245	25.488423
176.821688	6116.497852	25.493440
177.018283	6121.907758	25.498458
177.321373	6114.369852	25.503475
177.384164	6126.272014	25.508493
177.380220	6139.940829	25.513511
177.717326	6153.230361	25.518528
177.866700	6156.597562	25.523546
178.205412	6163.776235	25.528563
178.061231	6169.150798	25.533581
178.158968	6182.072558	25.538599
178.471256	6179.001061	25.543616
178.845692	6204.417823	25.548634
179.021440	6207.075910	25.553651
178.918441	6216.286379	25.558669
179.378180	6224.072821	25.563687
179.601549	6224.492900	25.568704
180.160418	6236.630763	25.573722
180.205054	6225.754149	25.578739
180.434445	6226.864030	25.583757
180.314119	6227.981672	25.588775
180.731924	6234.305954	25.593792
180.778725	6265.531666	25.598810
180.916395	6257.202631	25.603827
181.017085	6261.972518	25.608845
180.955684	6259.668651	25.613863
181.453308	6249.313796	25.618880
180.921103	6271.028815	25.623898
181.268956	6285.219938	25.628915
181.577005	6278.770017	25.633933
181.502164	6282.109266	25.638951
181.971235	6290.489825	25.643968
182.087268	6318.624496	25.648986
182.614549	6298.912795	25.654003
182.526989	6300.671138	25.659021
182.597919	6322.323122	25.664039
183.043811	6329.032409	25.669056
183.076066	6328.331944	25.674074
183.498441	6353.503724	25.679092
183.443067	6367.822150	25.684109
183.762270	6366.558255	25.689127
183.639807	6359.870099	25.694144
183.713266	6383.824591	25.699162
184.110893	6388.847721	25.704180
184.230021	6390.217513	25.709197
184.243540	6415.451431	25.714215
184.663809	6415.609607	25.719232
184.568245	6447.892196	25.724250
184.889680	6453.062030	25.729268
184.950395	6459.529881	25.734285
185.337237	6469.860647	25.739303
185.438858	6475.679203	25.744320
185.939346	6489.223865	25.749338
186.153389	6507.470244	25.754356
186.330728	6511.412124	25.759373
186.413881	6517.003121	25.764391
186.758419	6520.293661	25.769408
186.595104	6536.247036	25.774426
186.815643	6544.652413	25.779444
187.290448	6546.828595	25.784461
187.705984	6555.398008	25.789479
188.128714	6554.296189	25.794496
187.899800	6567.831323	25.799514
188.376816	6559.303255	25.804532
188.794514	6560.922861	25.809549
188.519252	6568.629972	25.814567
189.014439	6563.238188	25.819584
188.996854	6565.683265	25.824602
189.135807	6582.408309	25.829620
189.197459	6592.365364	25.834637
189.407720	6596.724511	25.839655
189.587026	6592.787448	25.844672
189.536480	6601.014993	25.849690
189.801075	6592.968439	25.854708
189.974744	6613.517950	25.859725
189.982508	6622.941536	25.864743
190.360287	6631.081145	25.869760
190.489967	6645.910060	25.874778
190.289345	6648.464581	25.879796
190.770207	6659.881966	25.884813
191.175484	6672.973063	25.889831
191.513520	6675.095539	25.894848
191.261165	6673.845633	25.899866
191.701557	6691.386617	25.904884
191.855734	6700.994618	25.909901
191.746609	6707.205629	25.914919
192.012720	6709.135016	25.919936
192.201944	6714.708390	25.924954
192.402536	6732.499293	25.929972
192.942972	6724.809947	25.934989
192.775487	6738.484143	25.940007
192.922160	6745.970661	25.945024
192.928286	6771.370013	25.950042
193.169081	6771.180730	25.955060
194.015165	6784.928633	25.960077
193.519732	6803.596897	25.965095
193.790086	6802.783709	25.970112
193.912613	6812.510911	25.975130
194.155397	6824.031680	25.980148
194.465334	6844.205739	25.985165
194.699395	6841.957746	25.990183
194.849167	6849.658612	25.995200
195.099462	6895.189090	26.000218
195.450096	6886.826539	26.005236
195.559356	6885.990248	26.010253
195.486954	6911.382689	26.015271
195.968000	6918.871064	26.020288
196.537056	6920.588534	26.025306
196.280772	6938.770378	26.030324
196.679114	6943.995790	26.035341
196.721281	6950.361384	26.040359
197.099132	6969.461844	26.045376
196.990715	6981.953753	26.050394
197.178370	6980.101809	26.055412
197.641251	6985.681229	26.060429
197.535920	7006.990164	26.065447
197.951764	7018.823388	26.070464
198.350295	7022.544463	26.075482
198.406888	7030.360199	26.080500
198.340943	7031.247357	26.085517
198.540625	7046.750806	26.090535
198.647143	7063.568111	26.095552
198.652370	7081.743059	26.100570
199.358869	7088.681020	26.105588
199.548678	7098.292254	26.110605
199.404766	7110.584577	26.115623
199.639631	7124.305924	26.120640
200.010154	7144.709133	26.125658
200.015493	7150.447315	26.130676
200.695576	7152.033030	26.135693
200.827983	7160.294663	26.140711
201.058313	7174.757153	26.145728
201.347996	7181.483080	26.150746
201.423607	7191.155853	26.155764
201.806406	7186.832923	26.160781
201.871236	7198.120350	26.165799
202.106547	7191.543943	26.170816
202.702400	7190.731563	26.175834
202.800951	7190.182569	26.180852
202.635354	7193.617530	26.185869
202.570322	7189.436801	26.190887
203.036500	7193.730939	26.195904
203.146031	7199.853797	26.200922
203.225306	7221.150920	26.205940
203.748146	7216.882763	26.210957
203.786899	7230.879380	26.215975
203.778397	7226.919374	26.220992
204.169951	7244.918064	26.226010
204.267867	7258.827382	26.231028
204.396158	7256.157156	26.236045
204.507466	7270.630846	26.241063
204.949340	7281.089527	26.246080
205.257171	7294.682168	26.251098
204.859035	7298.359577	26.256116
205.225254	7310.584906	26.261133
205.319523	7325.114868	26.266151
205.387427	7346.468273	26.271168
205.900119	7361.269107	26.276186
205.907903	7381.704504	26.281204
206.219967	7383.980719	26.286221
206.100178	7402.650433	26.291239
206.606775	7415.648932	26.296256
207.025499	7426.844711	26.301274
206.997365	7444.043485	26.306292
207.330232	7443.018877	26.311309
207.521151	7452.193485	26.316327
207.830892	7473.942054	26.321344
208.135327	7481.649280	26.326362
208.780692	7495.417261	26.331380
209.056814	7493.273408	26.336397
209.295815	7510.570513	26.341415
209.304445	7500.281733	26.346432
209.536885	7510.345151	26.351450
209.253661	7530.048985	26.356468
209.883589	7519.370029	26.361485
209.931449	7539.199703	26.366503
210.266730	7544.344113	26.371520
209.915781	7552.564208	26.376538
210.244476	7565.233199	26.381556
210.587526	7574.555945	26.386573
210.737258	7589.709138	26.391591
211.083807	7587.597320	26.396608
211.462570	7589.433333	26.401626
211.219693	7611.795791	26.406644
211.687147	7621.563744	26.411661
211.421801	7637.484209	26.416679
211.838288	7647.185556	26.421696
212.543898	7660.488519	26.426714
212.459001	7674.129951	26.431732
212.829628	7683.391719	26.436749
213.018200	7688.773582	26.441767
213.153100	7690.823944	26.446784
213.548786	7695.246705	26.451802
213.431423	7720.045776	26.456820
213.697948	7710.373524	26.461837
213.983952	7711.676711	26.466855
214.064776	7734.319004	26.471872
214.722683	7732.810597	26.476890
214.641417	7748.309997	26.481908
214.664310	7740.948127	26.486925
214.658854	7771.631417	26.491943
214.918880	7766.903794	26.496960
215.203243	7790.325731	26.501978
215.182507	7801.221253	26.506996
215.728714	7810.696668	26.512013
215.815769	7831.260889	26.517031
215.960722	7838.941795	26.522048
216.574562	7851.459355	26.527066
216.276561	7866.538638	26.532084
216.618569	7877.465304	26.537101
217.075091	7902.602020	26.542119
217.182534	7895.957563	26.547136
217.411835	7905.891137	26.552154
217.398171	7926.927908	26.557172
217.742294	7948.149234	26.562189
218.254742	7957.262673	26.567207
218.067523	7966.434931	26.572224
218.407739	7980.084413	26.577242
218.680589	7996.425403	26.582260
218.890148	8014.189663	26.587277
219.386743	8020.337712	26.592295
219.602403	8019.044556	26.597312
220.010994	8038.297291	26.602330
219.941541	8045.708761	26.607348
220.163603	8043.307498	26.612365
220.632910	8058.905936	26.617383
220.689622	8078.828159	26.622400
221.195553	8075.748232	26.627418
221.203208	8081.660297	26.632436
221.441436	8090.346999	26.637453
221.388246	8102.564303	26.642471
221.465031	8100.660655	26.647488
221.966175	8118.335283	26.652506
222.048406	8130.265070	26.657524
222.368320	8141.563697	26.662541
222.749432	8154.614326	26.667559
222.409519	8154.652151	26.672576
222.656282	8178.630699	26.677594
222.472416	8194.983337	26.682612
223.250363	8210.427299	26.687629
223.285455	8225.073799	26.692647
223.508167	8253.595641	26.697664
224.246742	8256.311526	26.702682
224.363134	8256.976124	26.707700
224.739224	8277.644390	26.712717
225.025442	8284.794701	26.717735
225.135640	8283.801601	26.722752
225.139184	8283.673730	26.727770
225.350645	8313.296714	26.732788
225.786804	8314.121220	26.737805
226.137613	8315.432231	26.742823
226.256066	8325.246055	26.747840
227.045250	8323.697786	26.752858
227.085497	8331.762312	26.757876
226.938116	8334.543112	26.762893
227.416273	8323.274822	26.767911
227.365107	8332.421683	26.772928
227.550421	8336.638182	26.777946
227.653875	8347.093339	26.782964
228.009354	8360.968928	26.787981
228.354055	8366.635387	26.792999
228.328894	8373.189366	26.798016
228.792995	8375.864046	26.803034
228.990146	8387.914995	26.808052
229.013365	8394.787032	26.813069
229.112653	8415.236802	26.818087
229.016295	8420.461341	26.823104
229.359470	8441.941615	26.828122
229.295717	8452.981385	26.833140
229.757626	8472.479555	26.838157
230.010268	8491.253358	26.843175
230.230558	8512.422052	26.848192
230.752495	8517.048408	26.853210
231.158587	8545.051361	26.858228
230.878214	8550.549994	26.863245
231.191485	8564.585153	26.868263
231.534328	8577.988478	26.873280
231.557401	8591.217743	26.878298
231.858988	8615.596642	26.883316
232.539971	8624.661598	26.888333
232.634525	8627.749324	26.893351
232.566073	8648.359133	26.898368
233.044753	8664.550805	26.903386
233.167087	8673.402681	26.908404
233.305855	8692.939273	26.913421
233.671876	8703.135649	26.918439
233.951387	8721.705594	26.923456
234.168130	8731.079893	26.928474
234.516808	8746.698285	26.933492
234.949788	8752.385443	26.938509
234.999136	8776.114720	26.943527
235.466514	8782.449517	26.948544
235.888378	8782.897842	26.953562
236.074390	8797.117964	26.958580
236.049898	8810.019006	26.963597
236.478248	8798.187025	26.968615
236.544312	8821.132338	26.973632
236.580444	8828.072548	26.978650
236.921316	8840.804427	26.983668
237.062918	8853.598769	26.988685
237.247240	8859.338982	26.993703
237.010929	8880.272522	26.998720
237.739419	8882.434597	27.003738
237.788450	8887.012124	27.008756
238.029748	8911.956659	27.013773
238.006326	8935.506576	27.018791
238.021445	8937.474697	27.023808
238.779065	8961.772029	27.028826
238.898448	8966.514629	27.033844
239.319928	8982.286125	27.038861
239.450265	8976.567250	27.043879
239.520750	9029.628052	27.048896
240.031921	9024.855677	27.053914
240.103928	9028.981844	27.058932
239.976636	9070.019126	27.063949
240.573431	9071.726545	27.068967
240.722032	9089.875581	27.073984
241.109465	9097.114022	27.079002
241.607271	9115.055162	27.084020
241.759617	9120.168300	27.089037
242.295261	9134.777612	27.094055
242.148988	9151.805968	27.099072
242.463554	9147.968254	27.104090
243.120508	9172.666771	27.109108
243.685526	9168.547158	27.114125
244.050328	9161.002611	27.119143
244.014758	9164.916975	27.124160
244.065036	9161.473128	27.129178
244.269608	9174.589387	27.134196
244.098908	9180.765993	27.139213
244.622052	9178.740306	27.144231
244.578914	9203.938803	27.149248
245.098874	9211.649564	27.154266
245.381781	9221.431864	27.159284
245.221412	9240.178410	27.164301
245.432413	9253.372797	27.169319
245.961840	9266.380305	27.174336
246.138383	9281.472323	27.179354
246.191513	9300.705844	27.184372
246.267814	9319.192069	27.189389
246.903447	9317.320374	27.194407
246.926459	9349.054071	27.199424
247.150002	9361.657553	27.204442
247.456695	9366.087137	27.209460
247.639992	9386.901777	27.214477
248.105698	9401.976941	27.219495
248.310914	9423.944900	27.224512
248.157287	9423.880237	27.229530
248.694606	9437.219502	27.234548
248.485211	9463.973517	27.239565
249.297868	9478.609442	27.244583
249.150338	9497.531318	27.249600
249.505010	9502.903891	27.254618
250.129114	9525.886456	27.259636
250.539993	9544.279103	27.264653
250.762786	9544.529408	27.269671
250.981428	9543.706228	27.274688
251.350594	9559.034589	27.279706
251.494545	9565.840705	27.284724
251.422759	9574.308957	27.289741
251.979168	9579.606910	27.294759
252.175587	9600.186040	27.299776
252.397798	9603.777712	27.304794
252.760890	9602.542372	27.309812
252.682582	9609.845464	27.314829
253.079689	9618.435734	27.319847
253.203805	9628.298697	27.324864
253.313009	9649.711378	27.329882
253.699451	9656.053551	27.334900
253.741208	9677.798088	27.339917
254.170213	9688.379747	27.344935
254.356357	9706.123788	27.349952
254.540880	9726.325689	27.354970
255.086219	9731.235538	27.359988
255.197972	9758.605418	27.365005
255.192955	9755.496039	27.370023
255.269601	9777.151351	27.375040
255.893000	9797.564329	27.380058
256.113685	9812.067123	27.385076
255.998905	9836.583633	27.390093
256.514698	9851.907417	27.395111
256.661330	9876.750612	27.400128
256.659527	9895.770163	27.405146
257.272609	9906.053110	27.410164
257.353576	9922.390994	27.415181
257.649990	9955.930524	27.420199
258.111997	9969.302338	27.425216
258.385202	9999.965066	27.430234
258.911352	9993.474861	27.435252
258.792409	10012.022572	27.440269
259.289846	10010.990853	27.445287
259.564844	10043.851320	27.450304
259.975643	10056.273268	27.455322
260.548641	10064.720867	27.460340
260.279736	10094.476281	27.465357
260.686008	10073.262072	27.470375
261.274769	10098.331842	27.475392
261.449668	10118.403598	27.480410
261.845137	10119.697430	27.485428
261.696257	10129.598727	27.490445
262.357058	10141.256117	27.495463
262.166333	10142.146425	27.500480
262.233933	10161.560530	27.505498
263.192944	10148.497898	27.510516
263.589437	10159.295584	27.515533
264.005021	10165.715174	27.520551
264.182547	10189.175616	27.525568
264.076628	10194.119778	27.530586
264.706122	10188.181594	27.535604
264.444433	10197.173492	27.540621
264.928041	10204.855154	27.545639
265.266866	10212.212457	27.550656
265.187311	10222.621369	27.555674
265.442490	10222.934204	27.560692
265.399499	10234.403227	27.565709
266.360654	10231.628452	27.570727
266.741385	10233.183552	27.575744
267.028899	10229.920422	27.580762
267.725838	10220.003253	27.585780
267.577011	10238.406878	27.590797
267.638258	10239.222011	27.595815
267.787150	10247.161654	27.600832
267.846478	10250.884110	27.605850
268.175676	10269.156101	27.610868
268.553685	10276.071610	27.615885
268.712533	10287.338127	27.620903
268.503082	10298.176226	27.625920
268.539859	10316.429565	27.630938
268.737206	10333.188078	27.635956
268.746827	10358.220745	27.640973
268.926267	10371.427446	27.645991
269.345212	10401.010482	27.651008
269.442867	10439.945153	27.656026
269.955031	10454.711784	27.661044
270.055496	10473.433639	27.666061
270.123158	10501.351368	27.671079
271.219056	10517.862204	27.676096
271.555520	10538.641835	27.681114
272.274715	10552.729068	27.686132
272.271572	10567.643262	27.691149
272.203255	10588.022770	27.696167
272.971700	10583.955747	27.701184
273.058419	10605.096361	27.706202
273.605475	10607.524506	27.711220
273.929741	10623.472991	27.716237
274.103157	10631.090991	27.721255
274.130946	10645.780765	27.726272
274.230196	10671.258082	27.731290
274.525892	10671.580209	27.736308
274.548717	10695.020061	27.741325
274.683511	10704.694337	27.746343
275.267549	10711.243530	27.751360
275.727494	10745.020040	27.756378
276.051674	10764.791850	27.761396
276.203823	10781.312528	27.766413
276.437641	10793.157714	27.771431
276.819182	10798.441090	27.776448
277.102983	10829.069197	27.781466
277.840596	10828.801484	27.786484
277.642652	10861.460528	27.791501
277.922151	10869.152244	27.796519
278.636688	10875.621294	27.801536
278.640413	10893.632307	27.806554
278.907037	10915.924776	27.811572
279.103841	10931.077400	27.816589
279.477280	10922.871103	27.821607
279.652962	10939.339804	27.826624
279.785903	10956.740446	27.831642
280.309031	10952.503088	27.836660
280.288055	10972.342776	27.841677
280.307589	10988.497223	27.846695
280.792086	10996.149249	27.851712
280.983066	11022.586447	27.856730
281.277963	11022.916189	27.861748
281.496718	11045.321937	27.866765
281.826069	11063.418978	27.871783
282.317717	11086.023295	27.876800
282.176776	11097.364565	27.881818
282.516680	11103.155218	27.886836
282.746353	11128.663283	27.891853
282.657825	11153.880547	27.896871
283.227388	11175.052825	27.901888
283.681151	11196.147181	27.906906
283.853327	11209.345546	27.911924
284.072057	11229.342151	27.916941
284.614386	11243.913512	27.921959
285.102160	11261.355935	27.926976
285.375062	11286.432786	27.931994
286.244309	11295.474500	27.937012
286.174984	11297.731057	27.942029
286.568177	11322.230018	27.947047
287.119248	11332.163781	27.952064
287.018526	11336.571926	27.957082
287.772525	11344.704936	27.962100
287.689187	11360.827580	27.967117
288.185440	11359.304284	27.972135
288.272851	11373.275968	27.977152
287.938392	11395.476064	27.982170
288.728270	11399.586849	27.987188
288.879717	11428.244545	27.992205
288.808155	11436.344696	27.997223
289.435249	11466.140632	28.002240
289.636928	11473.932422	28.007258
289.721960	11480.463504	28.012276
290.081595	11514.086159	28.017293
290.505890	11522.169109	28.022311
291.191450	11537.050052	28.027328
290.836617	11549.598416	28.032346
291.549119	11569.081945	28.037364
292.066244	11588.743026	28.042381
291.844745	11615.324919	28.047399
292.212508	11605.952392	28.052416
292.632247	11625.859248	28.057434
292.990470	11637.083590	28.062452
293.169556	11660.700730	28.067469
293.371435	11674.337474	28.072487
293.925870	11687.811791	28.077504
294.030190	11711.772662	28.082522
294.433000	11731.559579	28.087540
294.735245	11752.719791	28.092557
294.518955	11771.402446	28.097575
295.191499	11777.801064	28.102592
295.628582	11787.404248	28.107610
295.823549	11806.609319	28.112628
295.976812	11819.025769	28.117645
296.259218	11830.966739	28.122663
296.973355	11838.198132	28.127680
296.667381	11857.718037	28.132698
296.915340	11871.521157	28.137716
297.420456	11892.223444	28.142733
297.444089	11907.082749	28.147751
297.986877	11930.867048	28.152768
297.978071	11943.314940	28.157786
298.407555	11968.129102	28.162804
298.623978	11970.789621	28.167821
298.772402	12007.730595	28.172839
299.384414	12021.170064	28.177856
299.637970	12053.508655	28.182874
300.172939	12075.649494	28.187892
300.456655	12081.937455	28.192909
300.409334	12107.317383	28.197927
300.853145	12122.713605	28.202944
301.170832	12143.826649	28.207962
301.145187	12157.235246	28.212980
301.806827	12178.979836	28.217997
302.056603	12194.956028	28.223015
302.712581	12209.326635	28.228032
302.559982	12241.982415	28.233050
302.932333	12251.485631	28.238068
303.556391	12267.575010	28.243085
303.431415	12293.978213	28.248103
304.004585	12311.055446	28.253120
304.387225	12327.074946	28.258138
304.790144	12343.065061	28.263156
305.079809	12362.453694	28.268173
305.233175	12380.870794	28.273191
305.657594	12396.208601	28.278208
305.624333	12412.560701	28.283226
306.016264	12423.104952	28.288244
306.990832	12453.260284	28.293261
306.842409	12474.670029	28.298279
307.246818	12466.313542	28.303296
307.549878	12485.059914	28.308314
307.667989	12513.926471	28.313332
308.176359	12522.399939	28.318349
308.056623	12550.681109	28.323367
308.781632	12562.412021	28.328384
308.773053	12588.019554	28.333402
308.987058	12606.649221	28.338420
309.643595	12619.000486	28.343437
309.655852	12640.050151	28.348455
309.966993	12666.205831	28.353472
310.387485	12678.924355	28.358490
310.565759	12691.534110	28.363508
310.936656	12709.416554	28.368525
311.140758	12734.460731	28.373543
311.630620	12752.580660	28.378560
312.052170	12773.526714	28.383578
312.220960	12783.321857	28.388596
312.793974	12788.417615	28.393613
312.724435	12816.759757	28.398631
313.157147	12831.850327	28.403648
313.546581	12844.984803	28.408666
313.602030	12868.122942	28.413684
314.161234	12894.153296	28.418701
314.077259	12907.532890	28.423719
314.560966	12921.490468	28.428736
314.919301	12949.828227	28.433754
314.866008	12958.465833	28.438772
315.690254	12969.691282	28.443789
315.601817	12999.653672	28.448807
316.042750	13025.632262	28.453824
316.333429	13057.030823	28.458842
316.699831	13059.647761	28.463860
317.144337	13092.495928	28.468877
317.400371	13119.910505	28.473895
317.894184	13132.081314	28.478912
318.178095	13141.816035	28.483930
318.112646	13177.466095	28.488948
318.745084	13193.250715	28.493965
319.054984	13215.182729	28.498983
319.464458	13226.222005	28.504000
319.745546	13248.835575	28.509018
320.053856	13275.636222	28.514036
320.627082	13275.552906	28.519053
320.443470	13297.459788	28.524071
320.895752	13316.090333	28.529088
321.232104	13358.118346	28.534106
321.811498	13349.925156	28.539124
322.308144	13370.108568	28.544141
322.664196	13388.433393	28.549159
323.171283	13405.079249	28.554176
323.571860	13419.797317	28.559194
323.685041	13427.917496	28.564212
324.326487	13441.147321	28.569229
324.528100	13460.173573	28.574247
324.857326	13462.669780	28.579264
325.163742	13472.712633	28.584282
325.321653	13496.561523	28.589300
325.988523	13486.016165	28.594317
326.090103	13510.490569	28.599335
326.170323	13519.436825	28.604352
326.473752	13540.150689	28.609370
326.876140	13559.507542	28.614388
327.301577	13573.414007	28.619405
326.995560	13587.982533	28.624423
327.223462	13608.934432	28.629440
327.835916	13625.596800	28.634458
327.986360	13660.763937	28.639476
328.159156	13691.536163	28.644493
328.544199	13696.659238	28.649511
328.597300	13708.632923	28.654528
329.080929	13744.894409	28.659546
329.388992	13768.420486	28.664564
329.912351	13769.049806	28.669581
330.254381	13814.793279	28.674599
330.726526	13829.169741	28.679616
331.110107	13838.975614	28.684634
331.032339	13867.496752	28.689652
331.537449	13876.138577	28.694669
332.049775	13893.497093	28.699687
332.145729	13921.591466	28.704704
332.101631	13964.178965	28.709722
332.484257	13965.614329	28.714740
332.822507	13987.624510	28.719757
333.045177	14018.976467	28.724775
333.276200	14042.585794	28.729792
333.845179	14062.534362	28.734810
334.010396	14103.575195	28.739828
334.864535	14142.149893	28.744845
335.296339	14145.222502	28.749863
335.709556	14178.916723	28.754880
335.950980	14194.142649	28.759898
336.463694	14219.536626	28.764916
336.766947	14223.363470	28.769933
337.124111	14252.346589	28.774951
337.559648	14273.107800	28.779968
337.765635	14265.892648	28.784986
337.861489	14315.022896	28.790004
338.497202	14325.993272	28.795021
338.953187	14339.113324	28.800039
339.166815	14358.394320	28.805056
339.429792	14396.237440	28.810074
339.670617	14412.381324	28.815092
340.491696	14423.736777	28.820109
340.577308	14451.547637	28.825127
340.863990	14469.442036	28.830144
341.339644	14473.650409	28.835162
341.257936	14511.817859	28.840180
341.789097	14538.770896	28.845197
342.196287	14531.277563	28.850215
342.247578	14554.598600	28.855232
342.451398	14599.802439	28.860250
342.609290	14620.030182	28.865268
343.382241	14626.965846	28.870285
343.538383	14658.444451	28.875303
344.007417	14689.892843	28.880320
344.413733	14718.121064	28.885338
344.846656	14730.600914	28.890356
344.911910	14764.698932	28.895373
345.496871	14785.075414	28.900391
345.748873	14795.355411	28.905408
346.545970	14813.631353	28.910426
346.846556	14832.587756	28.915444
347.355046	14849.713591	28.920461
347.673041	14871.770983	28.925479
347.889262	14872.408465	28.930496
348.610688	14875.174413	28.935514
348.658744	14894.805124	28.940532
348.808160	14884.904219	28.945549
349.423501	14916.999767	28.950567
349.308793	14926.560143	28.955584
350.127659	14932.764314	28.960602
350.274182	14945.671870	28.965620
350.583894	14981.518558	28.970637
350.689952	14991.871047	28.975655
350.701080	14999.906089	28.980672
351.425824	15029.601381	28.985690
351.770076	15057.332767	28.990708
352.006603	15073.885195	28.995725
352.100807	15091.147085	29.000743
352.478430	15128.502410	29.005760
353.237173	15127.578418	29.010778
353.534885	15149.685004	29.015796
353.748466	15196.096730	29.020813
354.013551	15195.176221	29.025831
353.738499	15248.708871	29.030848
354.828113	15253.724141	29.035866
355.132972	15255.183933	29.040884
355.392339	15303.461770	29.045901
355.173620	15313.395867	29.050919
355.538610	15364.992711	29.055936
356.180074	15356.330411	29.060954
356.117824	15436.242182	29.065972
356.843518	15449.807410	29.070989
357.087414	15472.404327	29.076007
357.456696	15513.823128	29.081024
358.011489	15535.780865	29.086042
358.398152	15549.639525	29.091060
358.690879	15592.830397	29.096077
359.597843	15615.491909	29.101095
359.727340	15646.842667	29.106112
360.814082	15664.886709	29.111130
361.068628	15670.130445	29.116148
361.448407	15688.292875	29.121165
362.011872	15695.909431	29.126183
361.950331	15747.724417	29.131200
362.436156	15730.498994	29.136218
362.471686	15766.662512	29.141236
362.892149	15767.406930	29.146253
363.243242	15797.106476	29.151271
363.848232	15795.862731	29.156288
364.316293	15819.074901	29.161306
364.051402	15864.551117	29.166324
364.814658	15865.490574	29.171341
365.228917	15880.560942	29.176359
365.446404	15927.228933	29.181376
366.150894	15920.183821	29.186394
366.302288	15960.131849	29.191412
366.562496	15964.184459	29.196429
366.641531	15986.023711	29.201447
367.203491	16014.378710	29.206464
367.370713	16030.347978	29.211482
367.595417	16043.976642	29.216500
367.970177	16055.033943	29.221517
368.472832	16104.468917	29.226535
368.519949	16115.709942	29.231552
369.078434	16139.517726	29.236570
369.678163	16152.427299	29.241588
369.772506	16165.815374	29.246605
370.044451	16208.600045	29.251623
370.535054	16235.771658	29.256640
370.774902	16242.432749	29.261658
371.211238	16273.216887	29.266676
371.662856	16290.675593	29.271693
372.392124	16330.898092	29.276711
372.669411	16347.171063	29.281728
372.804846	16353.579888	29.286746
373.144875	16390.257875	29.291764
373.317913	16409.710791	29.296781
373.828664	16424.801158	29.301799
374.194731	16458.885219	29.306816
374.687044	16484.720006	29.311834
375.001100	16506.710806	29.316852
375.298877	16541.083250	29.321869
376.077754	16551.623830	29.326887
375.903628	16593.440550	29.331904
376.454502	16595.663027	29.336922
377.004941	16634.171374	29.341940
377.464016	16671.073743	29.346957
377.893211	16684.460285	29.351975
378.039235	16706.771608	29.356992
378.512948	16737.470712	29.362010
379.024916	16758.120480	29.367028
379.073908	16782.496500	29.372045
379.869593	16802.001663	29.377063
379.927321	16835.254705	29.382080
380.476982	16852.853330	29.387098
380.812494	16879.210748	29.392116
381.096695	16901.007682	29.397133
381.528727	16918.713107	29.402151
381.936605	16945.991863	29.407168
382.089344	16971.650110	29.412186
382.374370	16994.657329	29.417204
382.795222	17023.167271	29.422221
383.673516	17050.218125	29.427239
384.325674	17082.074580	29.432256
384.280886	17108.498694	29.437274
384.766475	17120.012673	29.442292
385.069652	17151.154295	29.447309
385.436737	17175.147808	29.452327
385.707214	17196.869011	29.457344
386.162270	17219.026531	29.462362
386.637367	17253.818917	29.467380
386.840158	17274.903444	29.472397
387.379632	17289.555881	29.477415
387.501418	17312.983442	29.482432
387.978114	17340.446203	29.487450
388.813951	17365.540599	29.492468
388.909364	17372.417402	29.497485
389.497952	17397.436100	29.502503
389.509596	17413.295483	29.507520
389.703114	17436.153194	29.512538
390.025397	17454.337112	29.517556
390.281321	17488.296132	29.522573
390.718328	17510.797075	29.527591
391.048232	17540.779423	29.532608
391.175786	17562.845145	29.537626
391.991835	17600.753991	29.542644
392.389196	17632.962001	29.547661
392.948276	17646.200745	29.552679
393.060272	17680.784647	29.557696
393.531208	17710.865317	29.562714
394.096362	17730.879816	29.567732
394.289183	17774.461792	29.572749
394.821312	17796.605107	29.577767
395.285638	17826.882318	29.582784
395.632933	17844.048608	29.587802
396.258394	17867.306802	29.592820
396.673883	17901.555654	29.597837
397.204389	17924.944215	29.602855
397.098073	17956.128298	29.607872
398.059627	17980.042714	29.612890
398.501263	17996.800268	29.617908
398.295536	18026.255551	29.622925
398.879782	18044.405709	29.627943
399.340546	18072.731714	29.632960
399.830214	18095.353065	29.637978
400.484040	18126.038836	29.642996
400.784267	18140.823113	29.648013
401.207817	18159.196639	29.653031
401.697292	18188.265884	29.658048
402.156279	18214.383478	29.663066
402.604426	18224.983822	29.668084
402.846883	18258.501422	29.673101
403.140529	18270.979093	29.678119
403.510849	18303.667396	29.683136
403.704212	18335.394628	29.688154
404.371639	18354.105106	29.693172
404.491694	18383.868989	29.698189
405.048468	18395.767453	29.703207
405.170592	18438.370861	29.708224
405.705094	18468.047219	29.713242
406.267251	18490.228083	29.718260
406.442486	18532.227239	29.723277
406.918921	18542.994943	29.728295
407.325479	18576.087093	29.733312
407.499559	18605.093989	29.738330
408.187459	18627.219190	29.743348
408.506372	18661.639636	29.748365
408.945214	18683.915622	29.753383
409.280233	18707.453048	29.758400
409.340235	18745.888508	29.763418
410.137703	18759.295346	29.768436
410.304700	18789.210399	29.773453
410.998688	18813.194333	29.778471
411.644987	18839.400066	29.783488
411.680239	18872.331929	29.788506
412.207770	18888.037790	29.793524
412.401305	18924.440606	29.798541
412.829012	18951.321515	29.803559
413.102151	18977.703079	29.808576
413.500556	19002.289914	29.813594
414.078104	19023.323020	29.818612
414.395596	19066.064345	29.823629
415.056004	19084.437847	29.828647
415.693218	19104.779660	29.833664
415.976611	19132.837829	29.838682
416.312206	19161.675147	29.843700
416.739815	19182.580388	29.848717
417.236241	19204.895587	29.853735
417.515562	19244.044199	29.858752
417.953490	19266.524715	29.863770
418.608780	19281.619663	29.868788
418.542293	19328.622203	29.873805
418.894662	19355.402426	29.878823
419.650212	19401.691128	29.883840
419.859386	19418.105358	29.888858
420.458525	19435.960676	29.893876
420.507593	19472.541732	29.898893
421.486118	19505.419533	29.903911
421.888125	19539.337327	29.908928
422.262452	19564.811997	29.913946
422.780666	19575.039886	29.918964
423.236084	19617.744608	29.923981
423.370943	19634.939840	29.928999
424.073536	19674.258329	29.934016
424.070118	19687.141574	29.939034
424.497399	19722.101856	29.944052
424.991708	19759.961934	29.949069
425.444043	19790.145278	29.954087
425.818670	19813.953677	29.959104
426.330008	19860.428331	29.964122
426.789369	19872.601346	29.969140
426.992870	19916.063208	29.974157
427.464468	19951.481540	29.979175
428.045563	19983.213355	29.984192
428.311213	20012.391761	29.989210
428.668011	20052.167506	29.994228
428.835492	20081.389242	29.999245
429.686273	20111.290027	30.004263
430.163640	20151.501969	30.009280
430.498080	20188.293194	30.014298
431.117726	20202.191076	30.019316
431.539554	20245.451734	30.024333
431.604173	20270.768614	30.029351
432.525736	20294.227201	30.034368
433.102391	20322.890455	30.039386
433.566904	20338.355443	30.044404
434.034830	20359.711791	30.049421
434.637832	20371.817822	30.054439
434.837722	20399.878583	30.059456
435.046089	20423.699439	30.064474
435.914260	20434.689153	30.069492
436.003749	20460.427223	30.074509
435.880611	20485.106186	30.079527
436.651437	20532.986530	30.084544
436.849217	20542.129377	30.089562
437.354403	20567.269843	30.094580
437.272648	20622.648892	30.099597
437.826894	20637.369092	30.104615
438.325483	20670.054530	30.109632
438.699622	20716.783144	30.114650
439.429411	20762.959902	30.119668
440.051089	20793.509595	30.124685
440.264240	20815.011500	30.129703
440.861601	20848.000118	30.134720
441.006642	20884.210085	30.139738
441.631055	20902.026051	30.144756
442.453802	20956.097461	30.149773
442.963351	20980.808314	30.154791
443.477534	21010.791621	30.159808
443.415818	21030.889779	30.164826
443.993008	21071.109053	30.169844
444.717389	21100.945644	30.174861
444.938527	21126.337804	30.179879
445.540471	21165.935574	30.184896
445.912585	21197.331444	30.189914
446.747457	21228.158304	30.194932
446.921966	21249.230282	30.199949
447.223337	21287.033840	30.204967
447.850156	21317.228565	30.209984
448.288381	21349.253676	30.215002
448.927844	21372.589515	30.220020
449.037783	21407.919528	30.225037
449.302109	21435.488336	30.230055
450.029199	21452.663670	30.235072
450.277446	21507.054527	30.240090
450.761930	21539.063993	30.245108
450.751526	21564.991472	30.250125
451.142559	21607.079099	30.255143
451.816764	21635.566595	30.260160
452.261986	21685.282570	30.265178
452.914943	21720.162145	30.270196
453.204925	21749.431660	30.275213
453.842275	21788.298852	30.280231
454.289810	21814.854704	30.285248
454.601738	21860.044376	30.290266
455.250172	21884.588440	30.295284
455.784309	21926.208371	30.300301
456.459146	21953.777269	30.305319
456.883880	21978.018468	30.310336
456.890421	21994.251499	30.315354
457.731350	22009.867275	30.320372
457.800241	22045.945564	30.325389
458.438075	22089.032381	30.330407
459.046648	22107.623665	30.335424
459.354126	22126.386585	30.340442
459.718230	22158.921320	30.345460
460.212132	22192.695553	30.350477
460.457775	22233.858214	30.355495
461.000704	22264.650142	30.360512
461.218557	22303.668132	30.365530
461.658512	22328.227201	30.370548
462.429673	22381.992777	30.375565
462.713064	22391.781479	30.380583
462.842613	22457.656142	30.385600
463.661088	22470.474533	30.390618
464.207575	22532.774416	30.395636
464.774198	22543.671905	30.400653
464.873242	22609.057455	30.405671
465.890718	22608.029185	30.410688
465.948115	22660.303524	30.415706
466.110151	22706.463035	30.420724
466.872810	22737.502842	30.425741
467.121864	22773.518652	30.430759
467.705130	22816.996564	30.435776
468.175334	22873.203694	30.440794
468.716541	22898.052324	30.445812
469.294654	22937.055444	30.450829
469.793329	22978.408930	30.455847
470.703861	23004.251136	30.460864
470.708615	23045.323543	30.465882
471.102773	23075.398040	30.470900
472.201262	23099.219379	30.475917
472.479159	23141.953707	30.480935
473.295829	23167.436228	30.485952
473.635698	23199.873007	30.490970
474.008901	23217.456357	30.495988
474.526039	23259.140801	30.501005
475.018594	23283.982037	30.506023
475.405526	23317.651277	30.511040
475.700230	23359.519492	30.516058
476.064304	23397.090499	30.521076
476.669195	23411.555174	30.526093
477.032795	23467.059931	30.531111
477.733037	23496.879325	30.536128
477.588190	23529.809076	30.541146
478.496490	23566.496706	30.546164
478.793650	23602.196411	30.551181
479.292896	23639.055702	30.556199
480.388172	23671.540093	30.561216
480.471937	23713.383772	30.566234
480.743749	23737.090448	30.571252
481.597353	23779.231482	30.576269
482.261677	23814.335214	30.581287
482.620280	23831.948355	30.586304
482.764979	23869.990212	30.591322
483.294049	23894.880941	30.596340
483.708341	23921.559061	30.601357
483.601215	23960.029562	30.606375
484.665878	23995.922956	30.611392
484.926767	24031.275747	30.616410
485.020651	24067.630343	30.621428
485.738757	24099.958304	30.626445
486.303558	24146.958937	30.631463
487.013636	24185.315559	30.636480
486.725705	24230.932081	30.641498
487.692498	24257.781112	30.646516
488.353679	24295.237606	30.651533
488.810425	24333.846038	30.656551
489.692496	24361.218366	30.661568
489.950782	24399.302472	30.666586
490.224780	24430.795236	30.671604
490.966115	24468.548142	30.676621
491.017274	24510.627540	30.681639
491.736494	24548.698444	30.686656
492.159092	24600.950934	30.691674
492.925380	24631.652033	30.696692
493.069871	24676.176952	30.701709
493.728960	24714.388589	30.706727
494.244979	24749.288010	30.711744
494.856581	24783.226260	30.716762
495.296299	24821.851193	30.721780
495.687180	24857.012608	30.726797
496.324126	24899.284869	30.731815
496.842319	24939.513951	30.736832
497.265144	24971.776508	30.741850
497.881517	25003.426973	30.746868
498.397984	25043.822800	30.751885
498.541709	25099.356466	30.756903
499.126460	25124.825526	30.761920
499.857590	25173.204040	30.766938
500.169088	25215.540010	30.771956
500.852769	25249.748201	30.776973
501.164282	25295.755151	30.781991
501.837933	25329.182116	30.787008
502.342519	25386.375748	30.792026
502.751496	25421.204680	30.797044
503.260383	25449.753755	30.802061
503.871894	25496.193223	30.807079
504.587470	25532.521452	30.812096
505.173548	25568.318978	30.817114
505.261515	25607.517810	30.822132
505.841135	25650.647226	30.827149
506.217908	25688.791162	30.832167
506.766683	25736.853039	30.837184
507.277288	25780.039487	30.842202
507.579478	25821.753076	30.847220
508.293026	25857.497861	30.852237
508.834340	25897.203398	30.857255
509.430440	25921.537565	30.862272
509.969382	25957.467937	30.867290
510.387649	26000.393974	30.872308
510.822962	26029.793978	30.877325
511.329828	26062.684227	30.882343
512.150236	26096.415558	30.887360
512.559090	26125.331542	30.892378
512.905705	26161.241802	30.897396
513.396577	26186.406894	30.902413
513.811127	26230.064398	30.907431
514.197759	26280.361847	30.912448
514.594293	26311.968788	30.917466
515.129764	26361.800059	30.922484
515.524867	26402.959950	30.927501
515.767091	26449.479916	30.932519
516.025029	26488.180375	30.937536
517.062136	26541.649047	30.942554
517.617038	26598.950076	30.947572
517.907827	26643.220832	30.952589
518.527593	26682.183967	30.957607
519.102177	26721.972121	30.962624
520.076304	26768.831777	30.967642
520.379138	26825.607342	30.972660
520.684284	26864.123145	30.977677
521.396632	26905.489830	30.982695
521.678281	26958.703656	30.987712
522.619934	27006.835180	30.992730
522.931737	27050.031507	30.997748
523.843186	27091.056561	31.002765
524.362218	27140.031791	31.007783
524.757581	27186.992734	31.012800
525.147497	27228.679465	31.017818
525.666751	27274.866990	31.022836
526.061399	27306.929975	31.027853
526.490892	27350.150904	31.032871
527.025753	27399.757025	31.037888
527.920971	27445.743351	31.042906
528.231916	27496.411185	31.047924
528.746711	27529.697095	31.052941
529.371084	27578.981470	31.057959
529.741271	27638.283632	31.062976
530.413195	27690.552975	31.067994
530.556092	27736.340097	31.073012
531.543041	27777.439179	31.078029
531.979186	27816.761269	31.083047
532.334671	27863.916467	31.088064
532.954543	27920.048205	31.093082
533.021170	27968.249498	31.098100
533.802263	28011.338990	31.103117
534.827958	28063.877006	31.108135
535.183218	28110.156075	31.113152
535.957558	28152.427648	31.118170
536.598647	28199.811726	31.123188
537.408686	28237.205690	31.128205
538.006897	28268.388848	31.133223
538.392190	28312.226054	31.138240
538.825095	28335.585349	31.143258
538.853481	28370.395422	31.148276
539.932115	28411.665885	31.153293
540.090708	28448.450283	31.158311
540.720343	28481.240841	31.163328
541.660096	28527.549346	31.168346
541.584065	28563.128101	31.173364
542.084399	28598.730166	31.178381
542.550802	28640.234241	31.183399
542.845058	28685.497273	31.188416
543.522895	28743.677451	31.193434
543.696491	28789.719518	31.198452
544.423893	28829.389266	31.203469
544.938594	28888.751001	31.208487
545.676736	28945.370143	31.213504
546.217164	28978.060885	31.218522
547.255882	29027.015014	31.223540
547.805250	29059.699769	31.228557
548.617982	29115.267592	31.233575
548.710356	29146.616529	31.238592
549.560771	29180.769519	31.243610
549.665823	29235.963537	31.248628
550.324182	29278.201376	31.253645
550.775442	29327.937043	31.258663
550.992825	29374.076223	31.263680
551.420105	29431.857543	31.268698
552.267045	29481.144578	31.273716
552.794627	29525.961496	31.278733
553.197050	29583.280861	31.283751
553.598787	29634.260828	31.288768
554.635666	29670.102847	31.293786
555.079675	29741.922031	31.298804
555.547765	29788.326600	31.303821
556.256040	29827.560595	31.308839
556.681027	29888.843945	31.313856
557.128450	29941.970267	31.318874
557.618869	29997.611355	31.323892
558.415642	30045.474024	31.328909
558.700999	30109.202608	31.333927
559.459218	30160.133751	31.338944
560.083414	30203.775701	31.343962
560.526681	30270.598514	31.348980
560.885892	30313.468206	31.353997
561.869404	30368.753091	31.359015
562.541196	30420.261423	31.364032
563.277662	30466.049964	31.369050
563.524673	30516.545153	31.374068
564.343304	30563.334218	31.379085
564.939839	30605.865875	31.384103
565.362558	30660.791917	31.389120
566.298559	30703.230365	31.394138
566.757627	30746.148330	31.399156
567.209390	30795.217036	31.404173
568.045242	30844.245206	31.409191
568.039592	30886.353425	31.414208
568.744902	30926.496735	31.419226
569.286901	30969.264969	31.424244
570.116167	31013.530466	31.429261
570.492028	31058.282782	31.434279
570.832857	31089.682566	31.439296
571.852316	31125.068805	31.444314
572.495739	31174.122310	31.449332
572.758940	31211.191007	31.454349
573.430398	31247.302741	31.459367
573.921375	31299.739403	31.464384
574.735030	31345.559098	31.469402
575.118538	31382.438812	31.474420
575.524992	31432.537917	31.479437
575.912452	31488.039728	31.484455
576.465490	31532.583880	31.489472
577.354190	31564.384322	31.494490
577.664041	31624.292987	31.499508
577.952913	31674.156236	31.504525
578.906566	31725.672656	31.509543
579.282013	31787.090798	31.514560
579.959763	31839.560910	31.519578
580.310509	31885.503121	31.524596
581.162321	31928.941642	31.529613
581.615041	31987.716164	31.534631
582.184386	32046.964065	31.539648
583.001488	32092.566226	31.544666
583.383002	32154.654620	31.549684
583.804730	32197.650111	31.554701
584.326377	32252.898298	31.559719
584.742411	32319.289347	31.564736
585.193258	32366.157907	31.569754
586.322740	32433.121412	31.574772
586.621420	32490.306724	31.579789
587.473796	32558.796443	31.584807
587.456714	32620.691585	31.589824
588.953943	32659.590812	31.594842
589.608896	32720.844990	31.599860
590.136702	32776.644036	31.604877
590.774570	32817.035996	31.609895
591.444327	32866.947809	31.614912
591.893682	32914.885242	31.619930
592.819722	32973.948857	31.624948
593.324537	33025.228752	31.629965
593.953641	33070.310324	31.634983
594.200627	33118.483905	31.640000
595.011902	33174.265952	31.645018
595.852080	33226.872248	31.650036
596.408426	33264.081733	31.655053
597.026932	33312.939115	31.660071
597.503852	33363.442699	31.665088
597.760559	33415.355978	31.670106
598.442211	33466.993686	31.675124
598.950792	33518.755266	31.680141
599.650530	33566.380454	31.685159
599.827375	33626.093755	31.690176
600.635638	33660.653750	31.695194
601.186256	33718.881356	31.700212
601.579705	33764.208842	31.705229
602.401256	33814.340519	31.710247
602.758765	33869.826755	31.715264
603.604005	33929.611254	31.720282
603.978612	33981.348330	31.725300
604.149563	34031.543287	31.730317
605.521654	34065.910309	31.735335
606.087313	34133.378774	31.740352
606.743213	34185.954421	31.745370
607.334983	34233.559317	31.750388
607.691246	34288.495447	31.755405
608.438717	34336.480957	31.760423
609.144867	34396.625049	31.765440
609.632618	34444.327508	31.770458
610.200619	34498.432995	31.775476
610.726801	34560.523159	31.780493
611.410083	34609.799669	31.785511
611.726858	34665.512590	31.790528
612.344436	34717.126571	31.795546
613.312439	34784.224647	31.800564
613.922711	34840.766298	31.805581
614.724591	34886.369156	31.810599
615.333694	34942.230348	31.815616
615.789515	34995.275501	31.820634
616.409957	35057.349360	31.825652
616.855619	35107.331997	31.830669
617.743675	35163.928249	31.835687
618.251136	35233.511786	31.840704
618.683699	35284.890581	31.845722
619.522747	35341.916144	31.850740
620.222374	35393.580641	31.855757
621.092542	35446.547065	31.860775
621.789091	35501.656870	31.865792
622.443112	35547.362333	31.870810
623.252830	35597.173390	31.875828
623.532873	35651.973247	31.880845
624.264508	35688.406728	31.885863
624.699501	35752.138023	31.890880
625.783281	35811.355326	31.895898
626.249732	35856.971697	31.900916
626.454032	35912.077690	31.905933
627.239226	35965.853837	31.910951
627.749914	36023.225668	31.915968
628.258374	36072.898518	31.920986
629.078777	36139.811166	31.926004
629.386643	36201.710470	31.931021
630.092609	36259.857607	31.936039
630.751571	36312.914018	31.941056
631.756833	36366.862937	31.946074
632.439786	36427.894603	31.951092
632.526424	36493.896045	31.956109
633.333663	36550.024308	31.961127
633.814888	36592.994926	31.966144
634.559332	36637.192851	31.971162
635.336610	36696.886191	31.976180
635.706899	36747.934142	31.981197
636.366966	36782.130105	31.986215
636.962621	36846.224664	31.991232
637.460489	36899.696421	31.996250
638.279713	36959.872753	32.001268
638.547409	37018.666182	32.006285
639.163289	37071.829608	32.011303
640.069029	37125.263939	32.016320
640.501830	37183.788864	32.021338
641.511907	37245.334263	32.026356
641.601347	37299.717381	32.031373
642.383005	37356.536663	32.036391
642.803787	37419.743676	32.041408
643.465270	37483.858568	32.046426
644.337941	37545.592492	32.051444
645.225427	37611.972174	32.056461
645.842788	37672.790206	32.061479
646.633907	37726.394485	32.066496
647.165697	37801.160919	32.071514
647.921398	37855.509117	32.076532
648.141337	37921.450793	32.081549
648.916560	37974.542827	32.086567
649.702663	38038.239519	32.091584
650.381568	38104.329563	32.096602
651.314873	38167.829872	32.101620
651.780979	38228.891579	32.106637
652.550096	38283.882312	32.111655
653.119468	38344.834972	32.116672
653.692641	38414.805968	32.121690
654.511493	38470.787442	32.126708
655.003250	38528.705354	32.131725
655.831855	38587.159521	32.136743
656.208179	38652.552528	32.141760
656.987581	38722.780504	32.146778
657.880720	38778.273423	32.151796
658.197715	38844.926971	32.156813
658.754050	38915.825116	32.161831
659.622645	38975.283378	32.166848
660.254136	39039.427883	32.171866
661.231369	39095.581731	32.176884
661.663613	39155.069106	32.181901
662.430304	39222.448807	32.186919
663.190907	39283.055895	32.191936
663.474712	39347.080326	32.196954
664.547399	39406.387773	32.201972
664.826849	39472.091076	32.206989
665.627651	39534.605320	32.212007
666.449788	39604.199429	32.217024
667.168977	39667.263272	32.222042
667.827514	39721.270280	32.227060
668.907100	39787.419794	32.232077
669.229385	39825.176282	32.237095
669.739487	39880.014767	32.242112
669.923968	39936.956745	32.247130
670.782647	39996.784424	32.252148
671.694530	40059.735473	32.257165
672.387509	40114.539291	32.262183
672.663253	40176.038850	32.267200
673.198047	40223.039078	32.272218
674.428868	40282.978817	32.277236
674.863454	40354.998289	32.282253
675.414139	40403.792553	32.287271
676.330100	40463.079768	32.292288
676.366272	40530.502128	32.297306
677.539078	40589.736276	32.302324
677.940700	40658.772474	32.307341
678.586336	40726.259418	32.312359
679.434343	40793.730177	32.317376
679.818329	40863.638895	32.322394
680.383413	40927.592951	32.327412
680.952768	41010.936619	32.332429
681.846239	41080.966958	32.337447
682.803433	41143.116867	32.342464
683.201512	41215.085857	32.347482
683.960830	41272.912181	32.352500
684.873121	41350.171015	32.357517
685.273361	41431.192392	32.362535
686.096915	41496.380048	32.367552
686.771439	41563.263292	32.372570
687.871355	41637.036785	32.377588
688.211394	41708.310596	32.382605
689.112325	41773.275670	32.387623
689.934702	41835.361250	32.392640
690.799124	41900.247460	32.397658
691.690248	41970.248701	32.402676
692.696425	42029.722551	32.407693
693.038701	42091.472312	32.412711
693.686374	42153.533241	32.417728
694.307348	42220.339262	32.422746
695.058293	42273.716709	32.427764
695.792956	42344.381519	32.432781
696.380321	42400.551573	32.437799
697.059026	42471.039719	32.442816
697.698161	42530.059615	32.447834
698.600562	42599.061759	32.452852
699.098921	42666.958304	32.457869
699.726936	42730.528995	32.462887
700.370294	42790.561610	32.467904
700.948328	42853.516179	32.472922
701.906484	42919.359668	32.477940
702.622208	43002.773303	32.482957
703.303775	43059.126075	32.487975
704.081059	43125.636309	32.492992
704.371362	43195.984234	32.498010
705.324496	43264.551990	32.503028
706.154315	43336.464292	32.508045
706.747408	43403.739878	32.513063
707.392921	43463.026920	32.518080
707.810281	43516.997572	32.523098
708.885042	43571.286416	32.528116
709.381458	43642.193209	32.533133
710.248366	43702.291198	32.538151
711.275273	43757.682816	32.543168
711.595696	43825.530237	32.548186
712.254640	43886.677692	32.553204
712.664445	43943.499310	32.558221
713.541187	44019.523505	32.563239
714.263236	44078.680610	32.568256
714.787635	44158.953766	32.573274
715.679094	44225.021056	32.578292
716.383228	44299.023553	32.583309
717.019400	44361.457032	32.588327
717.630337	44419.021042	32.593344
718.022927	44498.259995	32.598362
718.937711	44574.596025	32.603380
719.707278	44655.416039	32.608397
720.079914	44732.873766	32.613415
721.064397	44810.789638	32.618432
721.568251	44887.750825	32.623450
722.773858	44958.294583	32.628468
723.489869	45039.001880	32.633485
724.155861	45116.666985	32.638503
725.153588	45181.957585	32.643520
725.698859	45252.853725	32.648538
726.343925	45331.450590	32.653556
727.582345	45401.621831	32.658573
728.155513	45475.842630	32.663591
728.704706	45550.673266	32.668608
729.463691	45630.376423	32.673626
730.334690	45695.578711	32.678644
730.898481	45764.319300	32.683661
731.514839	45849.500725	32.688679
732.540170	45917.404992	32.693696
733.053924	46002.846418	32.698714
733.699701	46079.194020	32.703732
734.601175	46147.544799	32.708749
735.341611	46228.307350	32.713767
736.576206	46293.324645	32.718784
737.074423	46360.450121	32.723802
737.818976	46428.839602	32.728820
738.605138	46500.715180	32.733837
739.059993	46573.189591	32.738855
740.255281	46637.454096	32.743872
740.606288	46725.612941	32.748890
741.261961	46798.116258	32.753908
742.092612	46874.071930	32.758925
742.986590	46946.481137	32.763943
743.897330	47025.535509	32.768960
744.282144	47093.287602	32.773978
745.276988	47163.195518	32.778996
745.927963	47235.464767	32.784013
746.350087	47314.456247	32.789031
747.179413	47376.456468	32.794048
747.671555	47446.694786	32.799066
748.523417	47518.914293	32.804084
749.215172	47588.559800	32.809101
750.096402	47665.580419	32.814119
750.878038	47718.562728	32.819136
751.124992	47807.961437	32.824154
751.857300	47870.395321	32.829172
752.694206	47949.304694	32.834189
753.117631	48036.218614	32.839207
753.897766	48108.754857	32.844224
754.901742	48193.283329	32.849242
755.360899	48281.514792	32.854260
756.364406	48365.539333	32.859277
756.636175	48439.536689	32.864295
757.497769	48525.446167	32.869312
758.302247	48622.746180	32.874330
759.162632	48705.577192	32.879348
760.238612	48800.591566	32.884365
761.186519	48871.583388	32.889383
761.940796	48942.716755	32.894400
763.160491	49028.249834	32.899418
763.811080	49102.486265	32.904436
764.654989	49168.447280	32.909453
765.512184	49247.554861	32.914471
766.234052	49318.546595	32.919488
766.976527	49402.680728	32.924506
768.142257	49478.871973	32.929524
768.732792	49546.796377	32.934541
768.931756	49631.343117	32.939559
770.085972	49702.829240	32.944576
770.801518	49773.583989	32.949594
771.420372	49860.232788	32.954612
772.253739	49936.084467	32.959629
772.652132	50021.607922	32.964647
773.743714	50096.860661	32.969664
774.105279	50186.436153	32.974682
774.800627	50274.277054	32.979700
775.595935	50363.468840	32.984717
776.032740	50451.190833	32.989735
777.036991	50540.511182	32.994752
777.589775	50643.520338	32.999770
778.330563	50726.622807	33.004788
779.244703	50818.183614	33.009805
780.050568	50921.002617	33.014823
780.840202	51016.380529	33.019840
781.390496	51107.170787	33.024858
782.330100	51203.317909	33.029876
783.522430	51289.958115	33.034893
783.933410	51394.673023	33.039911
784.982532	51475.262098	33.044928
785.981800	51564.853452	33.049946
786.422240	51655.755496	33.054964
787.434930	51743.515245	33.059981
788.125027	51834.501535	33.064999
789.113346	51904.981479	33.070016
789.822536	51994.166710	33.075034
790.720949	52075.183269	33.080052
791.310965	52150.227850	33.085069
792.023912	52234.973349	33.090087
792.849151	52296.246627	33.095104
793.678210	52371.459219	33.100122
794.487674	52468.975115	33.105140
795.474691	52551.365180	33.110157
796.159227	52622.502240	33.115175
797.359575	52708.292764	33.120192
797.718757	52786.807298	33.125210
797.753377	52871.487026	33.130228
799.193065	52960.715429	33.135245
799.812726	53066.091721	33.140263
800.760353	53145.372602	33.145280
801.614802	53229.033513	33.150298
802.047424	53326.945422	33.155316
802.938943	53406.220599	33.160333
803.436206	53520.825388	33.165351
804.777584	53605.041767	33.170368
805.527653	53690.362622	33.175386
806.460333	53783.731457	33.180404
807.505938	53866.247611	33.185421
807.917379	53959.308945	33.190439
808.763874	54040.307889	33.195456
809.824956	54142.546045	33.200474
810.343007	54230.630206	33.205492
811.333569	54317.708491	33.210509
811.943105	54420.035862	33.215527
812.771781	54510.821066	33.220544
813.476155	54614.299110	33.225562
814.285418	54708.629780	33.230580
815.440338	54790.179533	33.235597
816.556249	54896.952042	33.240615
816.858054	54993.467094	33.245632
818.057414	55060.109716	33.250650
818.587774	55172.128268	33.255668
819.823370	55262.170677	33.260685
820.565759	55353.109547	33.265703
821.390952	55435.087133	33.270720
822.483010	55527.543139	33.275738
823.114361	55641.284561	33.280756
824.125367	55712.340765	33.285773
824.805929	55804.541703	33.290791
825.671885	55881.508565	33.295808
826.543616	55983.635697	33.300826
827.073503	56083.488255	33.305844
827.879632	56159.285252	33.310861
828.431903	56251.120600	33.315879
829.198520	56346.732330	33.320896
830.435518	56439.128849	33.325914
831.045069	56542.819167	33.330932
832.249958	56627.800469	33.335949
833.026966	56729.280781	33.340967
833.747110	56810.902455	33.345984
834.601163	56888.124825	33.351002
834.927911	56967.268653	33.356020
836.294735	57057.838831	33.361037
836.797149	57147.606314	33.366055
837.289338	57238.692234	33.371072
838.506850	57316.354175	33.376090
838.874646	57408.527725	33.381108
839.956486	57503.760696	33.386125
841.190184	57588.994413	33.391143
842.147747	57671.592311	33.396160
842.724938	57764.611921	33.401178
843.705796	57856.317636	33.406196
844.680787	57940.280893	33.411213
845.321633	58028.111249	33.416231
846.210540	58104.433464	33.421248
847.420666	58195.886556	33.426266
847.885546	58291.430142	33.431284
848.945092	58379.258674	33.436301
849.723515	58463.350303	33.441319
850.066848	58567.369046	33.446336
851.222598	58670.987580	33.451354
852.022657	58760.541908	33.456372
853.055903	58839.571863	33.461389
853.886079	58942.081937	33.466407
854.759106	59030.230536	33.471424
855.541022	59128.199976	33.476442
856.082856	59228.651741	33.481460
857.010057	59323.524068	33.486477
858.291388	59431.177461	33.491495
859.001627	59526.189537	33.496512
860.162145	59610.383424	33.501530
860.616996	59715.038072	33.506548
861.640834	59817.680020	33.511565
862.403090	59905.430494	33.516583
863.318717	59998.183298	33.521600
864.526566	60089.646102	33.526618
865.290422	60200.278344	33.531636
866.288042	60277.349953	33.536653
866.890675	60384.412795	33.541671
867.507860	60468.817008	33.546688
868.720196	60572.658160	33.551706
869.621110	60681.610685	33.556724
870.550031	60764.170091	33.561741
871.526127	60854.805254	33.566759
872.154767	60961.968302	33.571776
873.320325	61053.515184	33.576794
874.286170	61147.999133	33.581812
874.919030	61218.577846	33.586829
875.850883	61339.303392	33.591847
876.841153	61428.259306	33.596864
877.495175	61502.558389	33.601882
878.171345	61621.618236	33.606900
879.141145	61711.402862	33.611917
880.455572	61787.151486	33.616935
880.942968	61892.567790	33.621952
881.677715	61977.171649	33.626970
882.325279	62082.263559	33.631988
882.977246	62168.356044	33.637005
884.133187	62249.348115	33.642023
884.724428	62357.781812	33.647040
886.352539	62438.727984	33.652058
886.907923	62534.907259	33.657076
887.939099	62615.674464	33.662093
888.560054	62716.116569	33.667111
889.613070	62807.598341	33.672128
890.761554	62893.817227	33.677146
891.712279	62984.289873	33.682164
892.372276	63082.962540	33.687181
893.503604	63173.012633	33.692199
894.240062	63266.242724	33.697216
895.058339	63355.153013	33.702234
895.624112	63465.873899	33.707252
896.781992	63553.360586	33.712269
897.154631	63645.892557	33.717287
898.074769	63765.517630	33.722304
899.256099	63846.496729	33.727322
900.256413	63955.063966	33.732340
900.936120	64057.250157	33.737357
902.050549	64161.309856	33.742375
902.963534	64259.758918	33.747392
903.828518	64363.104663	33.752410
904.759582	64479.205041	33.757428
906.160848	64577.369625	33.762445
906.825897	64674.063378	33.767463
907.262992	64778.155278	33.772480
908.640570	64875.248278	33.777498
909.330718	64987.594108	33.782516
910.075328	65100.696191	33.787533
911.012676	65197.481909	33.792551
911.412148	65314.196202	33.797568
913.110293	65420.326903	33.802586
913.746715	65531.465436	33.807604
914.612078	65644.226230	33.812621
915.691372	65746.199983	33.817639
916.859814	65842.030001	33.822656
918.330004	65943.920505	33.827674
919.251209	66049.843552	33.832692
919.834913	66148.383172	33.837709
921.173055	66244.993564	33.842727
922.043626	66333.290407	33.847744
922.599023	66429.094573	33.852762
923.512514	66537.503971	33.857780
924.550789	66627.108296	33.862797
925.443509	66731.848944	33.867815
926.102428	66829.978979	33.872832
926.885133	66923.769140	33.877850
927.951558	67052.193949	33.882868
928.648360	67152.783162	33.887885
929.761392	67247.011895	33.892903
930.535423	67360.151038	33.897920
931.244253	67445.007566	33.902938
932.159683	67539.474469	33.907956
933.354149	67642.384348	33.912973
934.338597	67736.560126	33.917991
934.763051	67827.275264	33.923008
935.718138	67943.130625	33.928026
937.128612	68042.072702	33.933044
937.348753	68137.610199	33.938061
938.704576	68232.398924	33.943079
939.525845	68343.767486	33.948096
940.358440	68454.642137	33.953114
940.961978	68565.863413	33.958132
941.966460	68676.667763	33.963149
943.227956	68796.617340	33.968167
943.631286	68908.902167	33.973184
944.611309	69032.738981	33.978202
945.783171	69144.789179	33.983220
946.376377	69266.155701	33.988237
947.429107	69366.241749	33.993255
948.236044	69495.099927	33.998272
949.444801	69630.275863	34.003290
950.272711	69731.081861	34.008308
951.687767	69873.315114	34.013325
952.528772	69982.068042	34.018343
953.141258	70113.147183	34.023360
954.241659	70237.964390	34.028378
955.352366	70337.926156	34.033396
956.015011	70486.816276	34.038413
957.263844	70589.158165	34.043431
958.304590	70719.269754	34.048448
959.238809	70849.140114	34.053466
960.140993	70962.153435	34.058484
961.112573	71096.524285	34.063501
962.258489	71209.260162	34.068519
963.206830	71343.080394	34.073536
964.408532	71438.578950	34.078554
965.690132	71568.537795	34.083572
966.476134	71682.414068	34.088589
967.820078	71793.845488	34.093607
968.732688	71909.674259	34.098624
969.618485	72034.050497	34.103642
970.895434	72135.966311	34.108660
972.151569	72250.927350	34.113677
972.860764	72348.568500	34.118695
973.290754	72468.761295	34.123712
974.734690	72576.908205	34.128730
975.725283	72683.889376	34.133748
976.432123	72801.177798	34.138765
977.732827	72894.980562	34.143783
978.497041	73022.244726	34.148800
979.383352	73134.230409	34.153818
980.295692	73254.306993	34.158836
981.154595	73352.915007	34.163853
982.737558	73446.188923	34.168871
983.151550	73579.572179	34.173888
983.857873	73677.346700	34.178906
985.030250	73775.622587	34.183924
985.699873	73891.375206	34.188941
986.561576	74005.549771	34.193959
987.574849	74093.129091	34.198976
988.533788	74239.592731	34.203994
989.308782	74327.798667	34.209012
989.994847	74472.986722	34.214029
991.477656	74581.169948	34.219047
991.786286	74697.730335	34.224064
993.066232	74830.023647	34.229082
994.530633	74937.763059	34.234100
995.179580	75086.778357	34.239117
995.975108	75193.930416	34.244135
996.990884	75326.597640	34.249152
998.463333	75453.075799	34.254170
999.446183	75570.854778	34.259188
1000.227275	75691.282853	34.264205
1001.779311	75792.288870	34.269223
1002.615378	75938.695987	34.274240
1003.956594	76054.253141	34.279258
1005.006899	76172.359853	34.284276
1005.730955	76291.612477	34.289293
1006.770163	76407.421930	34.294311
1007.900121	76519.691135	34.299328
1008.750620	76643.065222	34.304346
1010.042245	76769.049539	34.309364
1010.918101	76900.940429	34.314381
1011.929229	77015.538079	34.319399
1012.699091	77143.231964	34.324416
1013.913563	77257.166629	34.329434
1014.754734	77377.456152	34.334452
1015.615308	77510.333055	34.339469
1016.789419	77642.870221	34.344487
1017.675788	77767.553724	34.349504
1019.054333	77894.093705	34.354522
1020.163207	78035.397394	34.359540
1020.883888	78162.378667	34.364557
1022.211534	78277.198539	34.369575
1023.107082	78395.443942	34.374592
1023.756594	78526.572364	34.379610
1025.109697	78662.134159	34.384628
1026.130369	78775.419216	34.389645
1027.096057	78913.376586	34.394663
1028.108430	79049.140521	34.399680
1029.243660	79158.667662	34.404698
1030.188151	79314.581813	34.409716
1031.316110	79411.078147	34.414733
1032.372675	79566.989030	34.419751
1033.226351	79675.944282	34.424768
1033.881002	79833.330661	34.429786
1035.257158	79947.722372	34.434804
1036.015513	80083.211183	34.439821
1037.274702	80233.475563	34.444839
1038.418040	80333.937051	34.449856
1039.405692	80480.137752	34.454874
1040.796911	80572.419434	34.459892
1041.349357	80713.703664	34.464909
1043.374622	80786.928348	34.469927
1043.737799	80929.129120	34.474944
1044.844750	81027.393672	34.479962
1046.165464	81133.975091	34.484980
1046.705023	81286.182123	34.489997
1047.726075	81384.354570	34.495015
1048.533606	81534.991038	34.500032
1049.376213	81640.519580	34.505050
1051.021826	81759.379329	34.510068
1051.914559	81886.545855	34.515085
1053.017205	82004.412392	34.520103
1054.239938	82129.296412	34.525120
1054.957139	82264.964084	34.530138
1056.121769	82388.992842	34.535156
1057.186020	82525.574224	34.540173
1058.305459	82642.771605	34.545191
1059.130098	82778.716331	34.550208
1060.418251	82933.635852	34.555226
1061.268719	83021.823078	34.560244
1061.834402	83197.550878	34.565261
1063.780687	83313.754412	34.570279
1064.491426	83463.010411	34.575296
1065.482159	83592.529841	34.580314
1066.575116	83728.355870	34.585332
1067.543458	83885.033929	34.590349
1068.627289	83998.280604	34.595367
1069.607233	84146.670443	34.600384
1070.415310	84305.362288	34.605402
1071.901376	84419.982407	34.610420
1072.836782	84592.046725	34.615437
1074.334763	84717.066782	34.620455
1075.426438	84843.227010	34.625472
1076.249538	85001.453846	34.630490
1077.488254	85119.158202	34.635508
1078.185981	85274.056105	34.640525
1079.443719	85414.848944	34.645543
1080.670355	85555.230374	34.650560
1081.916988	85691.272218	34.655578
1083.114273	85830.458837	34.660596
1084.139958	85977.052286	34.665613
1085.267994	86118.667091	34.670631
1086.491745	86232.010973	34.675648
1087.220890	86385.097340	34.680666
1088.276009	86531.620379	34.685684
1089.322450	86680.188115	34.690701
1090.632710	86821.260131	34.695719
1091.629864	86953.739305	34.700736
1092.527536	87102.308348	34.705754
1094.025392	87236.537011	34.710772
1095.079185	87375.895656	34.715789
1095.977057	87518.643942	34.720807
1097.595245	87639.248500	34.725824
1098.278167	87766.736752	34.730842
1099.348115	87883.528425	34.735860
1100.148499	88026.403091	34.740877
1101.228012	88149.733022	34.745895
1102.545935	88289.276914	34.750912
1103.320099	88421.876508	34.755930
1104.489877	88556.121345	34.760948
1105.360836	88688.485863	34.765965
1106.570061	88828.474214	34.770983
1107.625200	88970.290208	34.776000
1108.746725	89112.229373	34.781018
1109.632304	89253.378589	34.786036
1110.617760	89395.796561	34.791053
1111.843544	89544.753982	34.796071
1113.227820	89685.257565	34.801088
1113.996663	89837.767771	34.806106
1115.376491	89989.372422	34.811124
1116.761821	90149.963599	34.816141
1117.582017	90294.513307	34.821159
1118.918064	90434.055513	34.826176
1119.847077	90596.626092	34.831194
1121.132367	90724.763259	34.836212
1122.010114	90890.898342	34.841229
1123.255582	91055.312942	34.846247
1124.413612	91192.213167	34.851264
1124.923275	91339.652452	34.856282
1126.446625	91507.536250	34.861300
1127.815317	91661.405771	34.866317
1128.749362	91811.519207	34.871335
1130.442121	91958.818788	34.876352
1131.528633	92132.513147	34.881370
1132.602966	92271.539494	34.886388
1133.392761	92433.285707	34.891405
1134.992901	92575.196604	34.896423
1136.144530	92728.146768	34.901440
1136.937055	92890.737090	34.906458
1138.385803	93035.951249	34.911476
1139.227985	93188.207486	34.916493
1140.231445	93359.957701	34.921511
1141.547697	93516.903450	34.926528
1142.603750	93678.205319	34.931546
1143.801963	93825.570719	34.936564
1144.843215	93982.759573	34.941581
1146.102636	94142.470189	34.946599
1147.503732	94298.876672	34.951616
1148.720082	94462.094242	34.956634
1150.020608	94618.911130	34.961652
1151.309932	94770.474593	34.966669
1152.149190	94918.037144	34.971687
1153.731087	95073.136275	34.976704
1154.927818	95222.301241	34.981722
1155.848242	95379.791157	34.986740
1157.080796	95529.711531	34.991757
1157.971768	95671.906813	34.996775
1159.246128	95814.756823	35.001792
1159.958919	95946.994096	35.006810
1161.313012	96100.087069	35.011828
1162.463307	96233.205309	35.016845
1163.178172	96390.140388	35.021863
1164.504709	96537.452670	35.026880
1165.608085	96687.939010	35.031898
1166.793597	96821.529566	35.036916
1167.930410	96997.404671	35.041933
1169.038920	97139.543008	35.046951
1170.273480	97290.961401	35.051968
1171.075117	97453.090037	35.056986
1172.281573	97606.330582	35.062004
1173.623111	97759.500075	35.067021
1174.659637	97942.180071	35.072039
1175.790678	98092.924404	35.077056
1177.062695	98253.832598	35.082074
1177.941090	98407.902520	35.087092
1179.317931	98597.922794	35.092109
1180.503536	98756.305084	35.097127
1181.567673	98911.462322	35.102144
1182.646094	99090.114920	35.107162
1183.962488	99256.217182	35.112180
1185.397108	99437.922191	35.117197
1186.459708	99614.639137	35.122215
1187.774762	99761.202306	35.127232
1188.859222	99943.156796	35.132250
1190.103885	100121.000157	35.137268
1191.524903	100291.901636	35.142285
1192.740373	100450.967863	35.147303
1193.852043	100603.509668	35.152320
1194.712154	100805.879299	35.157338
1196.247528	100965.562543	35.162356
1197.483454	101133.272915	35.167373
1198.527227	101327.557247	35.172391
1199.818547	101475.666255	35.177408
1201.292406	101668.689236	35.182426
1202.213729	101826.002113	35.187444
1203.616015	102003.252794	35.192461
1205.039799	102176.394968	35.197479
1206.159305	102332.699027	35.202496
1207.123589	102518.951209	35.207514
1208.369406	102681.742125	35.212532
1210.094402	102875.874138	35.217549
1211.279664	103030.305797	35.222567
1212.431221	103205.530042	35.227584
1213.545382	103386.114746	35.232602
1214.644725	103553.927549	35.237620
1215.907626	103713.831168	35.242637
1217.312810	103899.922997	35.247655
1218.406336	104058.672593	35.252672
1219.353065	104243.859215	35.257690
1220.789807	104410.023530	35.262708
1221.886817	104583.330371	35.267725
1222.742308	104759.024583	35.272743
1224.132426	104911.803403	35.277760
1225.542488	105093.746336	35.282778
1226.619202	105249.026144	35.287796
1227.938406	105398.636316	35.292813
1228.900184	105567.326964	35.297831
1230.014505	105727.508318	35.302848
1231.022957	105911.457830	35.307866
1232.137989	106073.065275	35.312884
1234.003342	106238.098449	35.317901
1235.050035	106420.432063	35.322919
1236.412638	106592.857011	35.327936
1237.473056	106765.559072	35.332954
1238.142696	106934.242552	35.337972
1239.884286	107115.641947	35.342989
1240.959409	107290.231396	35.348007
1242.341574	107468.988250	35.353024
1243.419377	107653.775536	35.358042
1244.353715	107847.542372	35.363060
1245.947275	108004.764178	35.368077
1246.612777	108207.006728	35.373095
1248.175135	108406.602111	35.378112
1249.601750	108575.037517	35.383130
1250.950618	108755.543368	35.388148
1252.283736	108958.698727	35.393165
1253.724797	109138.718092	35.398183
1255.521358	109320.669661	35.403200
1256.343756	109504.220533	35.408218
1257.501260	109694.618490	35.413236
1258.912982	109877.749369	35.418253
1259.912207	110059.371171	35.423271
1261.598351	110231.871957	35.428288
1262.881711	110423.394902	35.433306
1264.042417	110616.464272	35.438324
1265.703582	110791.644059	35.443341
1266.482068	110984.321356	35.448359
1267.549845	111169.181286	35.453376
1269.228216	111365.377096	35.458394
1270.026663	111540.218306	35.463412
1272.230194	111733.130686	35.468429
1273.062493	111929.085693	35.473447
1274.493549	112107.951139	35.478464
1275.859260	112295.538350	35.483482
1277.047840	112477.502407	35.488500
1278.506237	112666.356366	35.493517
1279.577148	112853.443947	35.498535
1280.857513	113039.910934	35.503552
1282.030592	113228.118201	35.508570
1283.090323	113421.060973	35.513588
1284.646439	113597.448469	35.518605
1285.886993	113786.788691	35.523623
1287.067230	113980.932072	35.528640
1288.318793	114178.376464	35.533658
1289.537252	114375.890980	35.538676
1290.973941	114553.950150	35.543693
1292.149068	114748.492789	35.548711
1293.363951	114937.257040	35.553728
1294.852355	115101.371735	35.558746
1295.822149	115285.378876	35.563764
1297.207470	115456.007628	35.568781
1298.556296	115641.742407	35.573799
1299.713439	115809.206407	35.578816
1300.739616	115985.802548	35.583834
1302.180927	116186.144758	35.588852
1303.288227	116355.557576	35.593869
1304.629299	116569.853344	35.598887
1306.340290	116748.979677	35.603904
1307.927850	116914.692154	35.608922
1308.871308	117115.260110	35.613940
1310.428950	117289.229355	35.618957
1311.897238	117489.096366	35.623975
1313.043408	117651.730799	35.628992
1314.260033	117869.127972	35.634010
1315.531646	118021.791855	35.639028
1316.772242	118241.891903	35.644045
1317.930664	118413.880843	35.649063
1318.911489	118629.118554	35.654080
1320.757305	118796.100143	35.659098
1321.874855	119042.452221	35.664116
1323.217122	119208.237513	35.669133
1324.700644	119439.104779	35.674151
1325.963158	119628.003811	35.679168
1327.212360	119814.816815	35.684186
1328.593557	120034.954123	35.689204
1329.790110	120216.801489	35.694221
1331.009452	120445.205898	35.699239
1332.584242	120634.480528	35.704256
1334.134110	120853.502500	35.709274
1335.351200	121051.353724	35.714292
1336.745139	121252.952344	35.719309
1338.183532	121457.774913	35.724327
1339.656351	121659.972026	35.729344
1340.622591	121875.321235	35.734362
1341.951661	122077.519078	35.739380
1343.618045	122270.584095	35.744397
1344.432808	122484.645204	35.749415
1345.861005	122706.298299	35.754432
1347.212307	122904.610744	35.759450
1348.623131	123129.119823	35.764468
1350.329453	123339.183212	35.769485
1351.629455	123563.928896	35.774503
1352.976536	123756.979507	35.779520
1354.291612	123960.789826	35.784538
1355.672628	124174.888561	35.789556
1357.411429	124381.079259	35.794573
1359.131633	124593.822851	35.799591
1360.330387	124795.099479	35.804608
1362.067578	124982.169190	35.809626
1363.091526	125185.895781	35.814644
1364.489574	125386.727182	35.819661
1365.876333	125576.833336	35.824679
1367.229606	125765.084161	35.829696
1368.328960	125941.292633	35.834714
1369.542215	126126.933562	35.839732
1371.091873	126301.831477	35.844749
1372.482237	126518.164082	35.849767
1373.835839	126688.700219	35.854784
1375.343454	126877.858949	35.859802
1376.552980	127070.499183	35.864820
1377.897563	127268.388914	35.869837
1378.995809	127465.622522	35.874855
1380.292550	127649.373142	35.879872
1381.473389	127854.602280	35.884890
1382.928141	128058.383316	35.889908
1384.605056	128251.844340	35.894925
1385.755514	128461.693916	35.899943
1387.056490	128668.240173	35.904960
1388.622299	128865.447552	35.909978
1389.628637	129079.505191	35.914996
1391.057072	129283.071456	35.920013
1392.641378	129496.293052	35.925031
1393.916151	129705.511583	35.930048
1395.220442	129920.795223	35.935066
1396.740581	130138.453270	35.940084
1398.005931	130365.731064	35.945101
1399.483254	130590.113872	35.950119
1400.854886	130793.244156	35.955136
1402.420154	131009.508253	35.960154
1403.327900	131222.673221	35.965172
1404.922847	131446.651468	35.970189
1406.684622	131675.482681	35.975207
1407.974670	131895.230728	35.980224
1409.349435	132117.298218	35.985242
1410.880557	132350.175134	35.990260
1412.733818	132552.608129	35.995277
1413.867662	132769.486441	36.000295
1415.231441	133005.208039	36.005312
1416.937846	133225.280363	36.010330
1418.430164	133427.929006	36.015348
1419.768111	133652.713114	36.020365
1421.301304	133866.558843	36.025383
1422.567978	134103.394611	36.030400
1423.994392	134321.784047	36.035418
1424.824208	134554.207603	36.040436
1426.438440	134756.846300	36.045453
1428.199390	135014.048878	36.050471
1429.155606	135229.035456	36.055488
1431.005732	135444.084333	36.060506
1432.402764	135696.003663	36.065524
1434.015154	135916.453708	36.070541
1435.287936	136141.153591	36.075559
1436.478831	136393.327148	36.080576
1437.932969	136599.083354	36.085594
1439.217021	136834.646278	36.090612
1441.311767	137067.028413	36.095629
1442.998625	137265.884288	36.100647
1444.044378	137516.354579	36.105664
1445.561836	137690.111901	36.110682
1446.833104	137919.159526	36.115700
1448.676470	138117.616150	36.120717
1450.128674	138307.950002	36.125735
1451.641901	138527.877929	36.130752
1453.094477	138715.844629	36.135770
1454.357619	138930.074684	36.140788
1455.418075	139142.944508	36.145805
1457.138291	139364.657947	36.150823
1458.555440	139569.236910	36.155840
1460.025021	139772.452953	36.160858
1461.569418	139988.711632	36.165876
1462.609492	140206.547424	36.170893
1464.296644	140428.958381	36.175911
1465.601153	140652.559702	36.180928
1467.286974	140855.989546	36.185946
1468.384752	141106.659290	36.190964
1470.160452	141313.360366	36.195981
1471.620579	141550.326865	36.200999
1473.149335	141764.497003	36.206016
1474.258775	142009.976178	36.211034
1476.235778	142225.916065	36.216052
1477.475820	142447.652519	36.221069
1478.684009	142708.381130	36.226087
1480.106473	142917.696767	36.231104
1481.409791	143167.539745	36.236122
1482.831060	143398.544569	36.241140
1483.992542	143640.289666	36.246157
1485.814650	143904.048853	36.251175
1486.878250	144144.824851	36.256192
1488.694671	144378.854217	36.261210
1489.778742	144659.290391	36.266228
1491.571268	144893.657001	36.271245
1492.983242	145166.199853	36.276263
1494.553200	145416.893287	36.281280
1496.341113	145655.880161	36.286298
1497.892725	145922.665544	36.291316
1499.028691	146170.467941	36.296333
1500.768314	146430.674552	36.301351
1502.163371	146694.943590	36.306368
1503.951506	146937.489421	36.311386
1505.232771	147195.759731	36.316404
1506.458484	147461.380400	36.321421
1507.983172	147715.876863	36.326439
1509.805055	147966.918250	36.331456
1511.345375	148251.712738	36.336474
1512.768665	148486.418367	36.341492
1514.387431	148770.165562	36.346509
1516.640286	148989.353777	36.351527
1517.953844	149291.877488	36.356544
1519.378425	149518.553427	36.361562
1521.274710	149777.368141	36.366580
1522.397856	150019.548700	36.371597
1524.200640	150271.359154	36.376615
1525.476940	150486.681387	36.381632
1527.160086	150743.813607	36.386650
1528.811067	150939.391444	36.391668
1530.247380	151205.516779	36.396685
1531.647704	151411.532832	36.401703
1533.004039	151676.166081	36.406720
1534.852666	151878.602148	36.411738
1536.047981	152153.584540	36.416756
1537.242125	152363.417346	36.421773
1539.157814	152629.845775	36.426791
1540.445667	152845.891698	36.431808
1541.891598	153103.866192	36.436826
1543.468901	153351.882013	36.441844
1544.750434	153610.431736	36.446861
1546.398592	153848.474768	36.451879
1547.454802	154129.847634	36.456896
1549.140475	154349.542314	36.461914
1550.829616	154647.707054	36.466932
1551.984534	154884.973665	36.471949
1553.764002	155167.229319	36.476967
1555.277736	155430.599618	36.481984
1556.937441	155687.951517	36.487002
1558.429084	155968.116806	36.492020
1559.956526	156240.569634	36.497037
1561.528869	156494.619530	36.502055
1563.127180	156789.952044	36.507072
1564.694577	157044.120940	36.512090
1566.841894	157329.797731	36.517108
1568.295922	157613.215878	36.522125
1569.754923	157840.767372	36.527143
1571.355040	158127.957882	36.532160
1573.115394	158418.548993	36.537178
1574.932253	158659.528134	36.542196
1576.519448	158937.267904	36.547213
1577.928122	159220.148498	36.552231
1580.037975	159475.529881	36.557248
1581.327796	159765.560284	36.562266
1583.148180	160022.475288	36.567284
1584.362667	160287.185719	36.572301
1585.847821	160576.494351	36.577319
1587.614442	160823.202853	36.582336
1589.175993	161130.143305	36.587354
1590.918913	161370.670962	36.592372
1592.148459	161670.985785	36.597389
1594.080958	161934.402452	36.602407
1595.464031	162206.176727	36.607424
1596.924083	162496.532202	36.612442
1598.964700	162758.111604	36.617460
1600.138441	163039.550923	36.622477
1602.002036	163328.809117	36.627495
1603.187059	163617.391112	36.632512
1604.842775	163878.113979	36.637530
1606.789374	164175.063838	36.642548
1607.755780	164466.261804	36.647565
1609.837974	164735.217362	36.652583
1611.220166	165008.002068	36.657600
1612.645484	165275.011340	36.662618
1614.381065	165538.358691	36.667636
1615.603408	165826.419533	36.672653
1617.368430	166060.113431	36.677671
1618.831618	166354.215260	36.682688
1620.264117	166622.894614	36.687706
1622.282127	166899.498715	36.692724
1623.482633	167182.322692	36.697741
1625.558611	167438.171677	36.702759
1627.033214	167736.848619	36.707776
1628.556111	168019.450140	36.712794
1630.226858	168290.209097	36.717812
1631.646862	168589.205872	36.722829
1633.562648	168864.673764	36.727847
1634.748061	169160.630113	36.732864
1636.587895	169449.521272	36.737882
1638.514868	169728.633967	36.742900
1639.664457	170029.942773	36.747917
1641.226324	170337.505284	36.752935
1643.937067	170594.872964	36.757952
1646.045502	170880.878237	36.762970
1648.354498	171150.300320	36.767988
1649.997361	171421.555182	36.773005
1651.424960	171693.911643	36.778023
1653.319440	171979.197890	36.783040
1654.926915	172245.859481	36.788058
1657.041732	172497.055322	36.793076
1658.173794	172789.229677	36.798093
1660.221240	173035.872996	36.803111
1661.805661	173311.551990	36.808128
1663.365693	173603.740513	36.813146
1664.865397	173863.275560	36.818164
1666.105277	174115.686196	36.823181
1667.875104	174420.812068	36.828199
1669.164074	174699.414541	36.833216
1670.580622	174988.261549	36.838234
1672.709058	175261.444605	36.843252
1674.189272	175567.449743	36.848269
1675.704481	175878.792500	36.853287
1677.365803	176143.771626	36.858304
1679.063662	176458.299425	36.863322
1680.481076	176758.437028	36.868340
1682.469769	177027.670593	36.873357
1683.986679	177339.709268	36.878375
1685.547459	177676.533137	36.883392
1686.850699	177990.297979	36.888410
1688.947369	178269.240571	36.893428
1690.137172	178566.902750	36.898445
1692.735954	178858.431152	36.903463
1694.305053	179177.871881	36.908480
1695.748157	179454.274533	36.913498
1697.680754	179758.005895	36.918516
1699.573785	180093.806841	36.923533
1701.090499	180356.222151	36.928551
1702.843131	180669.605742	36.933568
1704.260140	180949.092669	36.938586
1706.362851	181191.424281	36.943604
1707.631410	181516.525601	36.948621
1709.104459	181782.572616	36.953639
1711.402235	182058.450408	36.958656
1712.501421	182385.158461	36.963674
1713.914025	182683.917859	36.968692
1715.448226	182987.786059	36.973709
1716.555576	183260.599586	36.978727
1718.898658	183549.992720	36.983744
1720.212690	183891.459928	36.988762
1721.944950	184195.190819	36.993780
1723.796329	184505.325365	36.998797
1725.134519	184844.423277	37.003815
1727.088077	185137.631814	37.008832
1728.881024	185448.277049	37.013850
1730.577984	185809.416814	37.018868
1731.998080	186115.798868	37.023885
1734.083323	186431.289787	37.028903
1735.758939	186778.330207	37.033920
1737.356812	187083.028241	37.038938
1739.423835	187446.139861	37.043956
1741.145837	187747.853248	37.048973
1742.959212	188104.246754	37.053991
1744.606005	188403.895245	37.059008
1746.559970	188764.662170	37.064026
1748.556688	189059.462539	37.069044
1750.068000	189422.944330	37.074061
1751.983286	189718.282056	37.079079
1753.782695	190079.337417	37.084096
1755.811451	190407.744930	37.089114
1757.796147	190724.105800	37.094132
1759.482656	191076.912493	37.099149
1761.488141	191374.911187	37.104167
1763.343688	191726.896307	37.109184
1765.268506	192035.445159	37.114202
1766.928162	192352.109450	37.119220
1768.511586	192694.893158	37.124237
1770.496912	193018.083973	37.129255
1772.515992	193331.791301	37.134272
1773.955816	193682.371651	37.139290
1776.232699	193993.694385	37.144308
1777.760635	194325.114159	37.149325
1779.537175	194642.574157	37.154343
1781.501355	194969.525020	37.159360
1783.426987	195264.260155	37.164378
1785.118074	195621.274230	37.169396
1786.751161	195936.404495	37.174413
1788.547355	196280.816289	37.179431
1790.533265	196573.836053	37.184448
1791.787837	196938.391484	37.189466
1793.960784	197236.297141	37.194484
1795.767853	197583.038575	37.199501
1797.892854	197869.849837	37.204519
1799.956232	198188.593623	37.209536
1801.206554	198495.778721	37.214554
1803.236946	198765.208641	37.219572
1804.470005	199104.816566	37.224589
1806.230755	199367.946091	37.229607
1808.182453	199705.184496	37.234624
1809.722844	199995.412896	37.239642
1811.559235	200316.744060	37.244660
1813.605672	200630.466139	37.249677
1815.281242	200924.714429	37.254695
1816.752359	201249.231583	37.259712
1818.456465	201567.405204	37.264730
1820.195210	201883.455413	37.269748
1821.978924	202202.851320	37.274765
1823.543200	202550.983542	37.279783
1825.626250	202880.998253	37.284800
1827.114062	203213.356146	37.289818
1829.089691	203563.955399	37.294836
1830.926098	203883.251016	37.299853
1832.494653	204254.292471	37.304871
1834.465782	204576.439388	37.309888
1835.858381	204927.114223	37.314906
1838.173805	205287.495233	37.319924
1839.736593	205632.638177	37.324941
1841.389638	206010.684673	37.329959
1843.434218	206334.860811	37.334976
1845.047344	206718.795630	37.339994
1847.151844	207064.127627	37.345012
1849.293105	207414.711293	37.350029
1850.948618	207786.129617	37.355047
1853.050137	208161.617887	37.360064
1855.150935	208494.759273	37.365082
1857.266772	208862.962916	37.370100
1859.495374	209213.860583	37.375117
1861.223385	209555.826363	37.380135
1863.244430	209927.999573	37.385152
1864.972836	210275.047260	37.390170
1867.233189	210617.835779	37.395188
1869.310704	210961.785068	37.400205
1870.975159	211315.754854	37.405223
1873.228197	211662.346114	37.410240
1874.746339	212016.838160	37.415258
1876.468055	212368.075227	37.420276
1878.100155	212719.023747	37.425293
1879.941882	213066.881275	37.430311
1882.366227	213420.818285	37.435328
1883.881195	213782.176180	37.440346
1885.871642	214136.058966	37.445364
1888.028916	214466.582218	37.450381
1889.498735	214841.144055	37.455399
1891.470497	215193.651594	37.460416
1893.129586	215541.335324	37.465434
1895.204677	215895.264792	37.470452
1897.123314	216273.089747	37.475469
1899.058994	216612.711082	37.480487
1901.277620	216938.297867	37.485504
1902.741171	217279.114686	37.490522
1904.458629	217608.237563	37.495540
1906.846962	217941.051774	37.500557
1908.444666	218274.538981	37.505575
1910.090222	218602.078157	37.510592
1911.891568	218942.278084	37.515610
1913.813099	219286.929803	37.520628
1915.836086	219633.954068	37.525645
1917.370014	219985.933195	37.530663
1919.415199	220328.640328	37.535680
1921.382104	220687.423150	37.540698
1923.195539	221033.204917	37.545716
1925.414850	221389.538653	37.550733
1926.625525	221748.395814	37.555751
1928.794156	222117.577868	37.560768
1930.665249	222478.149398	37.565786
1932.549304	222837.158803	37.570804
1934.427011	223207.077952	37.575821
1936.065984	223588.693014	37.580839
1938.114244	223942.792974	37.585856
1940.112698	224343.807267	37.590874
1942.068938	224717.428791	37.595892
1943.748248	225156.247907	37.600909
1945.748568	225534.069191	37.605927
1947.903058	225928.336854	37.610944
1949.577740	226315.228899	37.615962
1951.481014	226708.410068	37.620980
1953.591710	227111.363051	37.625997
1955.539831	227493.290380	37.631015
1957.814183	227887.205498	37.636032
1959.788714	228290.795241	37.641050
1961.620436	228673.863790	37.646068
1963.875662	229066.466755	37.651085
1966.052077	229459.134789	37.656103
1968.225702	229844.897088	37.661120
1970.417669	230244.601075	37.666138
1972.521524	230627.355606	37.671156
1974.973273	231003.656484	37.676173
1976.616072	231400.913026	37.681191
1978.660852	231772.583157	37.686208
1980.683963	232157.236327	37.691226
1982.804443	232537.481857	37.696244
1984.891643	232922.178798	37.701261
1986.681981	233307.610140	37.706279
1989.135929	233666.727141	37.711296
1991.083649	234066.359364	37.716314
1993.051093	234435.537806	37.721332
1995.082802	234807.552033	37.726349
1996.701287	235202.288467	37.731367
1999.042012	235573.392984	37.736384
2001.145645	235944.841263	37.741402
2002.804779	236329.136884	37.746420
2005.008425	236707.175681	37.751437
2007.072876	237078.431076	37.756455
2009.263555	237434.555461	37.761472
2010.746080	237792.342727	37.766490
2012.625998	238144.708956	37.771508
2014.671233	238498.624851	37.776525
2016.215681	238870.959531	37.781543
2018.522078	239223.744173	37.786560
2020.099863	239584.849507	37.791578
2021.957391	239967.018522	37.796596
2024.277747	240324.960491	37.801613
2025.899506	240716.008441	37.806631
2027.962004	241081.461141	37.811648
2030.163415	241464.240960	37.816666
2032.128416	241851.834685	37.821684
2034.289241	242228.400447	37.826701
2035.924228	242623.897579	37.831719
2038.337261	243000.527319	37.836736
2040.450870	243385.333747	37.841754
2042.182670	243786.127857	37.846772
2044.176084	244178.906039	37.851789
2046.141533	244574.280695	37.856807
2048.247321	244979.870669	37.861824
2050.110686	245385.017737	37.866842
2052.105547	245798.222564	37.871860
2054.568092	246189.967096	37.876877
2056.316407	246614.618410	37.881895
2058.604761	247024.579879	37.886912
2060.557017	247427.254995	37.891930
2062.315344	247842.484683	37.896948
2064.715733	248253.422537	37.901965
2066.606636	248678.260560	37.906983
2068.934645	249101.277770	37.912000
2070.989359	249518.294011	37.917018
2072.678286	249935.598012	37.922036
2075.167321	250358.212103	37.927053
2077.263563	250786.554144	37.932071
2079.174599	251203.623018	37.937088
2081.821742	251628.425273	37.942106
2083.508997	252056.606870	37.947124
2085.721722	252484.248960	37.952141
2087.706228	252907.254374	37.957159
2090.120687	253326.941165	37.962176
2092.483982	253758.855358	37.967194
2094.203755	254191.558490	37.972212
2096.862364	254602.623608	37.977229
2099.145786	255032.495842	37.982247
2101.387550	255453.332477	37.987264
2103.885503	255852.791546	37.992282
2105.915948	256268.938602	37.997300
2108.178579	256665.210496	38.002317
2110.509661	257090.456316	38.007335
2112.738964	257486.303178	38.012352
2114.690160	257906.327146	38.017370
2116.547804	258296.290225	38.022388
2119.288127	258700.136142	38.027405
2121.076671	259100.882181	38.032423
2122.879789	259476.478017	38.037440
2124.676084	259858.095924	38.042458
2126.624034	260245.990211	38.047476
2128.625267	260630.421859	38.052493
2130.703525	261029.600831	38.057511
2132.480028	261409.014087	38.062528
2134.849201	261814.041491	38.067546
2136.779170	262202.043013	38.072564
2138.536820	262610.166038	38.077581
2140.956630	263015.263257	38.082599
2142.692392	263409.317597	38.087616
2145.086705	263825.774995	38.092634
2147.003471	264244.010645	38.097652
2149.525959	264650.135103	38.102669
2151.129436	265072.917749	38.107687
2153.240861	265494.096130	38.112704
2155.371491	265919.869881	38.117722
2157.494070	266356.035236	38.122740
2159.909039	266775.922050	38.127757
2161.969180	267224.596530	38.132775
2163.973681	267651.738346	38.137792
2166.724205	268084.173110	38.142810
2168.435813	268523.530256	38.147828
2170.505038	268956.810465	38.152845
2172.867069	269405.616775	38.157863
2175.034337	269846.833304	38.162880
2177.373840	270286.930467	38.167898
2179.344065	270742.125232	38.172916
2181.958117	271173.186597	38.177933
2184.037738	271623.487062	38.182951
2186.059793	272073.847677	38.187968
2188.362305	272522.360370	38.192986
2190.505875	272976.258551	38.198004
2193.059181	273421.861208	38.203021
2195.754839	273878.034635	38.208039
2198.100874	274328.192193	38.213056
2200.356092	274759.006833	38.218074
2202.368183	275220.547404	38.223092
2204.930317	275650.678381	38.228109
2207.094007	276090.144800	38.233127
2209.223416	276540.489309	38.238144
2211.640070	276968.814290	38.243162
2214.144197	277412.367400	38.248180
2216.452524	277854.173249	38.253197
2218.629837	278279.563781	38.258215
2220.667836	278721.666329	38.263232
2223.431823	279147.573289	38.268250
2225.399984	279587.806780	38.273268
2227.797929	280026.295329	38.278285
2230.085882	280452.023241	38.283303
2232.128264	280897.147235	38.288320
2234.823577	281322.810128	38.293338
2236.603057	281761.903925	38.298356
2238.892827	282190.755221	38.303373
2240.794802	282608.896733	38.308391
2242.936242	283034.493953	38.313408
2245.326989	283429.592846	38.318426
2247.119898	283851.713655	38.323444
2249.545514	284243.351576	38.328461
2251.799323	284666.617981	38.333479
2253.680088	285084.811711	38.338496
2256.180243	285487.766581	38.343514
2257.993824	285917.477785	38.348532
2260.026488	286348.169925	38.353549
2262.176440	286784.482474	38.358567
2264.366469	287201.278645	38.363584
2266.570001	287648.174738	38.368602
2268.558819	288088.804367	38.373620
2270.655625	288547.909625	38.378637
2273.227185	288985.371915	38.383655
2275.149676	289448.745790	38.388672
2277.531564	289899.420928	38.393690
2279.609500	290359.313959	38.398708
2281.859754	290829.390819	38.403725
2284.223436	291297.264261	38.408743
2286.744265	291759.675802	38.413760
2289.154882	292226.422429	38.418778
2291.318762	292702.326814	38.423796
2293.717180	293168.997387	38.428813
2296.122781	293636.707402	38.433831
2298.165300	294116.489358	38.438848
2300.801961	294583.449532	38.443866
2303.303640	295068.567335	38.448884
2305.757500	295546.401179	38.453901
2308.350804	296013.212688	38.458919
2310.361958	296482.858838	38.463936
2313.160116	296959.364680	38.468954
2315.226473	297432.810113	38.473972
2317.607955	297920.912119	38.478989
2320.277572	298377.900712	38.484007
2322.430067	298856.993475	38.489024
2325.062328	299332.706676	38.494042
2327.387643	299803.310704	38.499060
2330.048990	300281.277429	38.504077
2332.412020	300754.768614	38.509095
2334.079610	301216.074386	38.514112
2336.807366	301692.832619	38.519130
2338.784438	302171.232488	38.524148
2341.043124	302643.413757	38.529165
2343.988837	303118.913818	38.534183
2346.129029	303596.749947	38.539200
2348.502761	304075.741355	38.544218
2351.119875	304564.700545	38.549236
2353.447870	305031.427405	38.554253
2355.799223	305507.750472	38.559271
2358.144026	305982.218691	38.564288
2361.077419	306451.461055	38.569306
2363.137320	306932.905427	38.574324
2365.343520	307399.872062	38.579341
2368.077394	307865.356367	38.584359
2369.967011	308313.014886	38.589376
2372.262296	308751.895297	38.594394
2374.704563	309192.757462	38.599412
2376.828274	309641.542496	38.604429
2379.081615	310085.530163	38.609447
2381.020419	310538.811520	38.614464
2383.720607	310987.881126	38.619482
2385.971808	311464.019820	38.624500
2388.087694	311910.003519	38.629517
2390.682054	312374.273315	38.634535
2392.549309	312839.545397	38.639552
2395.246363	313314.361052	38.644570
2397.768465	313782.268457	38.649588
2400.033717	314264.996666	38.654605
2402.119968	314735.686661	38.659623
2404.203291	315219.607692	38.664640
2406.907028	315719.657778	38.669658
2409.439527	316219.630973	38.674676
2411.096105	316714.381491	38.679693
2414.201526	317200.848746	38.684711
2416.321578	317705.603934	38.689728
2418.863474	318205.387876	38.694746
2421.085679	318725.893638	38.699764
2423.802283	319228.895470	38.704781
2426.191775	319732.022650	38.709799
2428.317174	320251.494036	38.714816
2430.783124	320767.505304	38.719834
2433.421730	321289.784746	38.724852
2435.942817	321803.571830	38.729869
2438.805797	322310.673224	38.734887
2440.994718	322827.275246	38.739904
2443.632842	323340.653861	38.744922
2446.038004	323862.497892	38.749940
2448.856778	324380.768519	38.754957
2451.553424	324896.896654	38.759975
2453.727016	325422.119987	38.764992
2456.135453	325936.204868	38.770010
2458.410238	326453.710684	38.775028
2461.168163	326981.599492	38.780045
2463.734345	327495.420896	38.785063
2466.520436	328016.416291	38.790080
2469.138086	328535.479512	38.795098
2471.657651	329065.880808	38.800116
2474.109090	329567.212582	38.805133
2476.498176	330087.545863	38.810151
2478.842733	330607.984183	38.815168
2481.660879	331134.666922	38.820186
2484.019693	331656.771634	38.825204
2486.364285	332169.276106	38.830221
2489.401347	332685.527032	38.835239
2491.750483	333209.425036	38.840256
2494.200847	333722.409541	38.845274
2496.681435	334232.770068	38.850292
2499.028201	334751.121370	38.855309
2501.864796	335258.091541	38.860327
2503.779812	335765.000856	38.865344
2506.497285	336249.027947	38.870362
2509.064352	336724.949992	38.875380
2511.184480	337205.459204	38.880397
2514.334538	337699.513201	38.885415
2516.411401	338176.391242	38.890432
2518.748998	338655.535100	38.895450
2521.183049	339151.011939	38.900468
2523.332405	339644.422644	38.905485
2526.037505	340141.016883	38.910503
2528.143287	340668.729238	38.915520
2530.553408	341173.283906	38.920538
2533.382726	341676.828659	38.925556
2535.867807	342202.284441	38.930573
2538.160958	342716.264686	38.935591
2540.603153	343241.261346	38.940608
2543.041183	343764.527660	38.945626
2545.714526	344290.570305	38.950644
2548.181283	344827.329661	38.955661
2551.046751	345356.099799	38.960679
2553.050265	345898.279752	38.965696
2555.857320	346445.760384	38.970714
2558.632515	346991.006763	38.975732
2560.895775	347534.729652	38.980749
2563.650661	348087.813512	38.985767
2566.303316	348639.054906	38.990784
2568.821359	349179.395919	38.995802
2571.552508	349746.861447	39.000820
2573.874614	350302.429044	39.005837
2576.901699	350854.122212	39.010855
2579.301505	351420.861326	39.015872
2581.887325	351982.056392	39.020890
2584.500740	352539.027277	39.025908
2587.143289	353091.316898	39.030925
2589.873155	353658.893841	39.035943
2592.532284	354218.124398	39.040960
2595.052130	354788.489235	39.045978
2598.072088	355350.569597	39.050996
2600.814155	355918.805248	39.056013
2603.395045	356478.835930	39.061031
2605.915007	357036.890196	39.066048
2608.844772	357597.919272	39.071066
2611.641445	358157.567093	39.076084
2614.007657	358716.946813	39.081101
2616.460872	359270.849310	39.086119
2619.397886	359831.928014	39.091136
2621.948645	360395.117298	39.096154
2624.603320	360964.730301	39.101172
2627.294224	361527.681075	39.106189
2630.387414	362073.226717	39.111207
2632.876943	362638.911901	39.116224
2635.623533	363203.432854	39.121242
2638.482483	363744.732402	39.126260
2641.313509	364296.562394	39.131277
2643.899490	364829.009798	39.136295
2646.545272	365351.594677	39.141312
2648.826974	365871.312729	39.146330
2651.736867	366374.683434	39.151348
2654.510173	366886.901577	39.156365
2657.464154	367387.462405	39.161383
2659.450148	367899.083069	39.166400
2662.135226	368426.447602	39.171418
2664.824281	368934.747445	39.176436
2667.293826	369455.561245	39.181453
2669.706671	369986.071385	39.186471
2672.188104	370517.173180	39.191488
2674.964142	371048.500894	39.196506
2677.585362	371578.730038	39.201524
2680.065306	372119.226302	39.206541
2682.555643	372652.812212	39.211559
2685.344729	373201.644555	39.216576
2687.707864	373763.020987	39.221594
2690.555606	374313.859309	39.226612
2693.025952	374880.582787	39.231629
2695.589583	375438.022692	39.236647
2698.522921	376011.457088	39.241664
2700.985513	376590.818856	39.246682
2703.569815	377162.871428	39.251700
2706.022214	377754.091972	39.256717
2709.073618	378321.690208	39.261735
2711.443024	378919.985059	39.266752
2714.176177	379523.972248	39.271770
2717.321343	380101.221428	39.276788
2720.016677	380697.661735	39.281805
2722.411055	381291.629028	39.286823
2725.281240	381879.829308	39.291840
2728.278676	382479.289230	39.296858
2731.255505	383096.322808	39.301876
2733.632026	383707.074238	39.306893
2736.779667	384300.139825	39.311911
2739.828576	384902.774834	39.316928
2742.253150	385508.568270	39.321946
2745.616579	386089.141918	39.326964
2748.374274	386686.594143	39.331981
2751.415464	387289.495929	39.336999
2754.345303	387884.770716	39.342016
2756.998390	388473.332754	39.347034
2760.274339	389055.673967	39.352052
2762.943228	389649.287026	39.357069
2765.601353	390224.884392	39.362087
2768.613157	390824.180957	39.367104
2770.999270	391418.468706	39.372122
2774.252984	392001.297845	39.377140
2776.713355	392597.785702	39.382157
2779.550360	393185.733280	39.387175
2782.574246	393771.029205	39.392192
2785.226506	394360.583763	39.397210
2788.096602	394937.515490	39.402228
2790.521349	395537.736729	39.407245
2793.170285	396122.595385	39.412263
2796.299814	396678.561140	39.417280
2799.128551	397242.831916	39.422298
2801.714151	397786.237373	39.427316
2803.844356	398339.899501	39.432333
2806.639905	398892.762445	39.437351
2809.596383	399455.428762	39.442368
2811.965362	400023.782032	39.447386
2814.706610	400592.852513	39.452404
2817.416748	401179.108396	39.457421
2820.364610	401760.879086	39.462439
2823.169280	402347.479164	39.467456
2825.653856	402932.699438	39.472474
2828.448833	403525.414985	39.477492
2831.174208	404124.139008	39.482509
2833.598481	404725.231755	39.487527
2836.354080	405334.702580	39.492544
2839.255751	405943.986349	39.497562
2842.162497	406565.729779	39.502580
2844.692939	407197.305364	39.507597
2847.899958	407812.030456	39.512615
2850.568479	408442.494052	39.517632
2853.238849	409084.655269	39.522650
2856.288438	409710.317647	39.527668
2859.452442	410352.500718	39.532685
2862.078070	410986.365637	39.537703
2865.012129	411640.876120	39.542720
2867.863292	412265.781846	39.547738
2870.853091	412936.273489	39.552756
2873.842944	413578.617677	39.557773
2876.896936	414233.508282	39.562791
2880.148605	414886.528276	39.567808
2882.566076	415530.846458	39.572826
2885.301882	416182.119761	39.577844
2888.759112	416850.395132	39.582861
2891.531971	417510.274100	39.587879
2894.474760	418166.487312	39.592896
2897.712169	418829.962015	39.597914
2901.058599	419472.473761	39.602932
2903.427105	420143.428972	39.607949
2906.448941	420801.874485	39.612967
2909.763376	421458.788642	39.617984
2912.532745	422114.709450	39.623002
2915.717745	422756.233993	39.628020
2919.001428	423412.524062	39.633037
2921.956855	424055.042820	39.638055
2925.276960	424704.658449	39.643072
2927.946215	425356.819002	39.648090
2930.847635	426004.443164	39.653108
2934.017028	426658.469229	39.658125
2936.861026	427294.950468	39.663143
2940.079370	427933.333201	39.668160
2942.783526	428594.554452	39.673178
2945.951431	429234.408497	39.678196
2949.123724	429858.972627	39.683213
2951.872779	430489.465264	39.688231
2954.707681	431101.540752	39.693248
2957.930560	431689.301780	39.698266
2961.005133	432272.514102	39.703284
2963.842171	432872.289228	39.708301
2966.576926	433471.078902	39.713319
2969.766217	434059.449907	39.718336
2972.392077	434654.835603	39.723354
2974.972542	435255.785960	39.728372
2977.912435	435877.000193	39.733389
2980.825923	436481.920629	39.738407
2983.717569	437096.224673	39.743424
2986.422642	437720.013613	39.748442
2989.497419	438339.778409	39.753460
2991.898390	438965.027726	39.758477
2994.524869	439619.799327	39.763495
2997.691662	440252.187158	39.768512
3000.256470	440910.327107	39.773530
3003.447281	441571.135338	39.778548
3006.497884	442221.314662	39.783565
3009.541987	442890.870150	39.788583
3012.688918	443560.238998	39.793600
3014.601610	444241.378940	39.798618
3018.291228	444912.598964	39.803636
3021.467282	445597.145837	39.808653
3024.234066	446289.939243	39.813671
3027.894858	446968.294904	39.818688
3030.984053	447670.716877	39.823706
3033.757105	448351.856299	39.828724
3037.063305	449045.546620	39.833741
3039.873141	449746.432114	39.838759
3043.387427	450437.415983	39.843776
3046.083550	451137.113353	39.848794
3049.325460	451839.689405	39.853812
3052.407008	452535.133032	39.858829
3055.069352	453244.944752	39.863847
3058.544803	453956.579519	39.868864
3061.457036	454663.068527	39.873882
3064.918684	455373.952509	39.878900
3068.289272	456077.440231	39.883917
3071.344195	456774.478687	39.888935
3074.424989	457488.898191	39.893952
3077.420706	458196.224293	39.898970
3080.285139	458907.495277	39.903988
3083.429567	459619.963994	39.909005
3086.499682	460347.296283	39.914023
3089.863816	461056.496196	39.919040
3093.024557	461771.624466	39.924058
3096.222617	462487.431587	39.929076
3099.335105	463213.194467	39.934093
3102.481593	463937.764083	39.939111
3106.032037	464630.781673	39.944128
3109.018374	465352.951367	39.949146
3112.117269	466040.228235	39.954164
3115.567048	466768.245241	39.959181
3118.623227	467457.759040	39.964199
3122.041961	468119.527646	39.969216
3125.142327	468778.746465	39.974234
3127.868402	469428.495971	39.979252
3131.029311	470094.743998	39.984269
3134.015659	470719.985934	39.989287
3137.024978	471415.343982	39.994304
3139.824328	472058.678571	39.999322
3142.993065	472741.173285	40.004340
3146.129084	473396.801219	40.009357
3148.689258	474101.594848	40.014375
3151.760816	474771.649511	40.019392
3154.624721	475453.292812	40.024410
3157.599800	476174.987065	40.029428
3160.992550	476868.430335	40.034445
3163.908699	477589.274320	40.039463
3167.210751	478284.199573	40.044480
3169.881645	479002.756553	40.049498
3172.854438	479747.979536	40.054516
3176.299480	480475.863672	40.059533
3179.490272	481201.789952	40.064551
3182.475853	481943.086664	40.069568
3185.492559	482708.912876	40.074586
3188.432184	483427.164851	40.079604
3191.473282	484227.849332	40.084621
3194.576804	484961.078358	40.089639
3197.733846	485751.473491	40.094656
3200.568585	486510.457397	40.099674
3204.080544	487296.437693	40.104692
3207.947885	488097.941913	40.109709
3210.735207	488888.973138	40.114727
3214.145401	489651.277509	40.119744
3217.725692	490467.479155	40.124762
3220.772027	491240.082721	40.129780
3224.367689	492020.751020	40.134797
3227.186589	492839.293370	40.139815
3230.697756	493593.793733	40.144832
3233.920371	494425.789698	40.149850
3237.220045	495204.602962	40.154868
3240.307220	496020.386117	40.159885
3243.799285	496800.666805	40.164903
3246.996421	497616.563305	40.169920
3250.653191	498429.623599	40.174938
3253.645696	499216.040266	40.179956
3256.704461	500044.776054	40.184973
3260.255221	500830.478478	40.189991
3263.687922	501638.178193	40.195008
3266.914611	502453.497359	40.200026
3270.218097	503251.854778	40.205044
3273.711964	504075.387021	40.210061
3277.161412	504852.042827	40.215079
3280.433551	505697.089049	40.220096
3283.385777	506476.628751	40.225114
3287.024725	507285.147744	40.230132
3290.258570	508113.881270	40.235149
3293.639296	508869.121186	40.240167
3297.094980	509662.367347	40.245184
3300.411123	510401.401305	40.250202
3303.223675	511192.912244	40.255220
3306.273120	511932.881012	40.260237
3309.718646	512690.566233	40.265255
3312.747413	513439.504451	40.270272
3316.185372	514220.886490	40.275290
3319.219511	514979.543290	40.280308
3322.779711	515757.000512	40.285325
3325.999307	516536.594198	40.290343
3329.083888	517327.320691	40.295360
3332.622336	518092.314111	40.300378
3335.378636	518882.917582	40.305396
3339.291843	519673.098593	40.310413
3342.278689	520454.058002	40.315431
3345.624746	521259.735443	40.320448
3348.627949	522099.769053	40.325466
3351.925405	522866.847733	40.330484
3355.123347	523728.903412	40.335501
3358.047635	524551.225109	40.340519
3361.680489	525348.032619	40.345536
3365.220838	526190.239654	40.350554
3368.146371	527044.397051	40.355572
3371.704601	527859.189690	40.360589
3374.741734	528757.648980	40.365607
3378.053770	529606.264641	40.370624
3381.758371	530440.559337	40.375642
3384.769178	531330.913034	40.380660
3388.447100	532216.020752	40.385677
3391.660580	533108.307660	40.390695
3394.859447	533983.261843	40.395712
3398.459216	534852.711872	40.400730
3401.243886	535741.791223	40.405748
3405.670440	536616.553600	40.410765
3408.328697	537515.072705	40.415783
3412.162665	538405.141948	40.420800
3415.592207	539286.810872	40.425818
3419.170924	540208.650864	40.430836
3422.634153	541149.038443	40.435853
3425.985721	542060.022937	40.440871
3429.280729	542949.305999	40.445888
3433.004729	543834.087344	40.450906
3436.435703	544743.486160	40.455924
3440.040884	545697.312825	40.460941
3443.123620	546619.491515	40.465959
3446.571925	547532.039595	40.470976
3450.115413	548438.928078	40.475994
3453.558797	549324.029776	40.481012
3457.083489	550256.582377	40.486029
3459.984095	551200.649821	40.491047
3463.676560	552131.596044	40.496064
3467.576228	553058.322857	40.501082
3470.917945	553995.092575	40.506100
3474.653844	554923.687750	40.511117
3478.139567	555826.937288	40.516122
3480.900282	556687.728147	40.521127
3484.585346	557516.392768	40.526132
3487.804768	558281.734303	40.531136
3491.276756	558972.402590	40.536141
3493.792382	559606.956758	40.541146
3496.617573	560173.807132	40.546151
3499.370266	560679.628297	40.551156
3501.422099	561117.466424	40.556160
3504.208371	561493.706731	40.561165
3506.103195	561882.482009	40.566170
3507.867094	562164.926151	40.571175
3509.636403	562403.244704	40.576180
3511.482519	562570.655018	40.581184
3513.229914	562685.137200	40.586189
3514.260157	562806.639358	40.591194
3515.386033	562881.688537	40.596199
3517.168454	562875.659132	40.601204
3517.904482	562830.921131	40.606208
3518.998204	562763.538099	40.611213
3519.463993	562692.875785	40.616218
3520.209974	562599.630629	40.621223
3520.963627	562470.786069	40.626228
3521.469809	562338.298620	40.631232
3522.172422	562187.727602	40.636237
3522.500760	562012.355490	40.641242
3522.729884	561788.539462	40.646247
3522.679025	561600.868220	40.651252
3522.729655	561402.034410	40.656256
3523.228185	561156.835734	40.661261
3523.825460	560879.394163	40.666266
3523.867536	560636.729460	40.671271
3523.692313	560394.548762	40.676276
3523.862423	560140.256561	40.681280
3523.838334	559823.052602	40.686285
3523.953714	559557.663676	40.691290
3523.620190	559301.670791	40.696295
3523.683976	559003.397261	40.701300
3524.191572	558689.563717	40.706304
3523.339860	558406.603226	40.711309
3523.599214	558131.934929	40.716314
3523.195294	557855.146846	40.721319
3523.198501	557512.364970	40.726324
3522.292348	557247.548070	40.731328
3522.543960	556954.951899	40.736333
3522.479807	556675.111075	40.741338
3522.172256	556358.328236	40.746343
3521.941189	556096.662045	40.751348
3521.457859	555826.001214	40.756352
3521.802472	555503.547348	40.761357
3521.521195	555218.264045	40.766362
3520.790704	554959.279216	40.771367
3520.933683	554690.566302	40.776372
3520.556629	554450.081748	40.781376
3520.701675	554120.817531	40.786381
3520.251214	553892.494000	40.791386
3520.173392	553593.625069	40.796391
3519.432660	553349.546948	40.801396
3519.595103	553083.525442	40.806400
3519.468721	552807.756234	40.811405
3519.093493	552559.469597	40.816410
3518.645506	552325.520155	40.821415
3518.624000	552088.976611	40.826420
3518.353974	551851.661130	40.831424
3518.015478	551591.897838	40.836429
3518.095781	551336.756586	40.841434
3517.672995	551148.552243	40.846439
3517.786693	550919.789828	40.851444
3517.183205	550691.793180	40.856448
3517.123552	550441.755132	40.861453
3516.933466	550220.246105	40.866458
3516.778645	549962.342349	40.871463
3516.950814	549741.525794	40.876468
3516.445471	549555.383044	40.881472
3516.104304	549353.314600	40.886477
3515.828274	549140.887006	40.891482
3515.456295	548942.602906	40.896487
3515.368865	548734.025743	40.901492
3514.876102	548554.076085	40.906496
3514.955680	548365.655536	40.911501
3514.689162	548195.608571	40.916506
3514.647953	548010.382284	40.921511
3514.781360	547824.318499	40.926516
3514.392390	547643.584190	40.931520
3514.291799	547455.584249	40.936525
3514.340102	547281.741864	40.941530
3513.851673	547102.177558	40.946535
3513.739210	546870.964844	40.951540
3513.904127	546707.192544	40.956544
3513.236328	546555.866543	40.961549
3512.867547	546425.944874	40.966554
3512.901499	546273.848872	40.971559
3512.926642	546077.684492	40.976564
3512.605427	545928.064066	40.981568
3512.479929	545789.163466	40.986573
3512.624710	545660.314962	40.991578
3512.044450	545505.077386	40.996583
3511.763006	545339.997528	41.001588
3512.045505	545182.298075	41.006592
3511.648883	545078.165361	41.011597
3511.638699	544946.255724	41.016602
3511.376780	544808.377172	41.021607
3511.677302	544678.889751	41.026612
3511.379388	544538.136806	41.031616
3511.099505	544368.805242	41.036621
3511.489981	544241.824056	41.041626
3510.481023	544146.868963	41.046631
3510.121728	544031.616180	41.051636
3509.840342	543925.134836	41.056640
3510.133848	543822.045466	41.061645
3510.145918	543737.175215	41.066650
3510.065575	543637.122389	41.071655
3510.204402	543513.506953	41.076660
3509.922561	543364.813819	41.081664
3509.528273	543264.101277	41.086669
3509.443369	543158.340752	41.091674
3509.376907	543049.244268	41.096679
3509.683972	542958.415725	41.101684
3509.047245	542890.658225	41.106688
3509.144223	542803.951631	41.111693
3509.087304	542710.048715	41.116698
3508.972356	542594.291835	41.121703
3509.025169	542536.017029	41.126708
3509.033580	542454.169558	41.131712
3508.834915	542331.506563	41.136717
3508.969598	542279.781756	41.141722
3508.524085	542165.841036	41.146727
3508.520429	542114.894911	41.151732
3508.817692	541994.119997	41.156736
3508.335204	541930.524699	41.161741
3508.331323	541849.635251	41.166746
3508.188645	541741.197730	41.171751
3507.979539	541684.829291	41.176756
3508.037733	541632.912375	41.181760
3508.209882	541516.849363	41.186765
3507.993063	541466.490172	41.191770
3507.851253	541414.149660	41.196775
3507.911196	541361.474111	41.201780
3507.893122	541240.894485	41.206784
3507.576728	541186.207486	41.211789
3507.530747	541136.931101	41.216794
3507.698960	541045.759495	41.221799
3507.728810	540976.221652	41.226804
3507.515402	540942.776437	41.231808
3507.641145	540835.198921	41.236813
3507.294021	540779.757856	41.241818
3506.912128	540743.561492	41.246823
3507.139906	540702.824932	41.251828
3507.407498	540608.706146	41.256832
3507.036236	540563.973583	41.261837
3507.163186	540531.534119	41.266842
3506.980804	540473.793494	41.271847
3506.963271	540392.140929	41.276852
3507.075966	540306.225463	41.281856
3506.632369	540290.338176	41.286861
3506.692598	540240.385603	41.291866
3506.394719	540178.470705	41.296871
3506.604453	540150.562252	41.301876
3506.189952	540108.259130	41.306880
3506.421307	540036.867155	41.311885
3506.574639	540011.138836	41.316890
3506.515177	539986.706595	41.321895
3506.593708	539903.975726	41.326900
3506.394787	539850.477332	41.331904
3506.273074	539836.457700	41.336909
3506.443946	539811.281772	41.341914
3506.352913	539761.503029	41.346919
3506.504733	539685.071931	41.351924
3505.790740	539644.834873	41.356928
3506.329929	539625.610019	41.361933
3506.021265	539553.543605	41.366938
3505.535488	539562.458225	41.371943
3506.029021	539500.112477	41.376948
3506.284118	539455.833166	41.381952
3505.284100	539442.052981	41.386957
3505.936423	539420.486922	41.391962
3505.815445	539402.830664	41.396967
3506.245820	539369.936753	41.401972
3505.905740	539301.308221	41.406976
3506.059691	539231.742767	41.411981
3505.398044	539216.292830	41.416986
3505.298264	539216.359264	41.421991
3506.076744	539199.217147	41.426996
3505.986605	539126.003121	41.432000
3505.841801	539085.775631	41.437005
3505.657234	539053.432746	41.442010
3506.017225	538998.479449	41.447015
3505.935148	538965.413139	41.452020
3505.621966	538949.402827	41.457024
3505.844504	538931.742236	41.462029
3505.891989	538889.110189	41.467034
3505.409324	538870.601416	41.472039
3505.430113	538857.063393	41.477044
3505.299351	538856.124656	41.482048
3505.416408	538822.269014	41.487053
3505.562543	538799.873016	41.492058
3505.503749	538776.953831	41.497063
3505.920030	538746.484979	41.502068
3505.323349	538690.015139	41.507072
3505.763388	538646.259792	41.512077
3505.392642	538627.884547	41.517082
3505.196842	538574.078145	41.522087
3505.928994	538527.448050	41.527092
3505.023152	538532.490305	41.532096
3505.220922	538513.873560	41.537101
3505.303037	538472.396480	41.542106
3505.224110	538438.974998	41.547111
3505.244320	538451.547648	41.552116
3505.025262	538447.491547	41.557120
3504.982173	538395.731076	41.562125
3505.368881	538339.407551	41.567130
3505.050421	538359.155017	41.572135
3505.157558	538347.269561	41.577140
3505.141456	538323.383352	41.582144
3505.032555	538309.511803	41.587149
3505.081806	538303.948610	41.592154
3504.913262	538280.136930	41.597159
3505.193852	538254.638060	41.602164
3505.087504	538229.957882	41.607168
3505.469061	538184.594281	41.612173
3505.426219	538138.135986	41.617178
3505.301745	538120.731323	41.622183
3504.764393	538117.584037	41.627188
3504.350200	538119.619386	41.632192
3504.762928	538093.897341	41.637197
3504.808023	538105.355213	41.642202
3504.691708	538097.040288	41.647207
3504.797053	538032.982191	41.652212
3505.085827	538030.411410	41.657216
3504.907286	538047.611859	41.662221
3504.861704	538021.709595	41.667226
3504.752739	537966.927713	41.672231
3504.877264	537957.716042	41.677236
3504.792524	537960.860990	41.682240
3504.547883	537923.020010	41.687245
3504.986551	537885.121452	41.692250
3504.440354	537885.915028	41.697255
3504.922689	537897.303954	41.702260
3504.814600	537892.927128	41.707264
3504.008739	537866.993237	41.712269
3504.498083	537846.309334	41.717274
3504.597502	537846.748344	41.722279
3504.770493	537847.377754	41.727284
3504.895567	537839.226566	41.732288
3504.750889	537821.521715	41.737293
3504.585456	537807.507124	41.742298
3504.262184	537792.911383	41.747303
3504.858399	537773.069108	41.752308
3504.623966	537775.278120	41.757312
3504.769925	537770.810602	41.762317
3504.768625	537761.719712	41.767322
3504.448734	537748.941646	41.772327
3504.814876	537681.507397	41.777332
3504.742904	537666.568775	41.782336
3504.936689	537653.355896	41.787341
3504.609537	537637.699965	41.792346
3504.460417	537679.089209	41.797351
3505.180461	537653.317858	41.802356
3504.808561	537652.467663	41.807360
3504.382779	537614.654548	41.812365
3505.053573	537579.597475	41.817370
3504.790281	537568.123511	41.822375
3504.788631	537591.104893	41.827380
3504.269355	537554.266048	41.832384
3505.094893	537514.386141	41.837389
3504.675016	537524.402698	41.842394
3504.824045	537478.063598	41.847399
3505.518002	537460.276299	41.852404
3505.341709	537445.050900	41.857408
3505.092395	537424.382152	41.862413
3505.090050	537407.411949	41.867418
3504.271226	537424.461747	41.872423
3505.120982	537384.476659	41.877428
3504.962930	537366.217804	41.882432
3504.938288	537334.452103	41.887437
3504.896801	537314.962563	41.892442
3505.028935	537311.254724	41.897447
3505.365719	537265.592429	41.902452
3504.796459	537286.189051	41.907456
3504.641776	537292.476721	41.912461
3504.871046	537268.398561	41.917466
3504.803873	537249.973679	41.922471
3504.430954	537225.435027	41.927476
3504.345602	537222.569678	41.932480
3504.607517	537199.496426	41.937485
3505.096408	537156.789791	41.942490
3505.000712	537151.299596	41.947495
3504.883074	537126.063822	41.952500
3504.663984	537156.757601	41.957504
3504.479946	537142.543305	41.962509
3504.042387	537110.589854	41.967514
3504.446089	537078.351854	41.972519
3504.381586	537084.271792	41.977524
3504.079501	537106.341706	41.982528
3504.148675	537097.087757	41.987533
3504.566647	537072.878449	41.992538
3503.754581	537075.279869	41.997543
3504.548659	537081.165135	42.002548
3504.561208	537090.204467	42.007552
3504.697177	537079.424674	42.012557
3504.742070	537062.800189	42.017562
3504.726958	537029.214015	42.022567
3505.259005	536988.621487	42.027572
3504.509165	536988.841175	42.032576
3504.920993	536961.955658	42.037581
3504.671098	536942.801640	42.042586
3504.359319	536963.155962	42.047591
3504.656570	536959.725001	42.052596
3505.144899	536909.037240	42.057600
3504.165159	536920.708475	42.062605
3504.393531	536923.854660	42.067610
3504.575206	536910.693566	42.072615
3504.513597	536893.934201	42.077620
3504.245210	536912.261338	42.082624
3504.629800	536893.209023	42.087629
3504.552042	536860.541558	42.092634
3504.439827	536879.450173	42.097639
3504.608011	536865.280974	42.102644
3504.715118	536814.956212	42.107648
3504.643150	536794.965728	42.112653
3504.978536	536776.022064	42.117658
3504.278256	536800.832391	42.122663
3504.513652	536781.348925	42.127668
3504.402224	536793.388128	42.132672
3504.682351	536791.929733	42.137677
3504.749992	536783.736551	42.142682
3504.581260	536774.722048	42.147687
3504.362724	536765.462859	42.152692
3504.637896	536747.538882	42.157696
3504.668823	536714.853931	42.162701
3504.238468	536700.375092	42.167706
3504.508500	536699.069815	42.172711
3504.830589	536659.267259	42.177716
3504.139646	536667.407807	42.182720
3504.281866	536677.437100	42.187725
3504.681285	536678.182306	42.192730
3504.635981	536634.194860	42.197735
3505.114424	536597.852673	42.202740
3505.262887	536584.545018	42.207744
3504.899711	536563.539527	42.212749
3505.050293	536542.604346	42.217754
3504.426266	536567.958616	42.222759
3504.650293	536565.700892	42.227764
3504.296559	536552.472577	42.232768
3504.456214	536539.870267	42.237773
3504.800305	536531.077639	42.242778
3504.504645	536531.427594	42.247783
3504.627054	536491.353095	42.252788
3504.732691	536479.213874	42.257792
3504.619277	536467.765909	42.262797
3504.474180	536460.161800	42.267802
3504.415346	536456.231380	42.272807
3504.918323	536450.848364	42.277812
3504.481422	536438.087696	42.282816
3504.517066	536429.798360	42.287821
3504.602381	536419.430201	42.292826
3504.432997	536415.820311	42.297831
3504.396709	536393.500140	42.302836
3504.484489	536384.444867	42.307840
3504.688620	536335.365991	42.312845
3505.113808	536307.163917	42.317850
3504.785652	536303.124486	42.322855
3505.116387	536293.121551	42.327860
3504.891616	536263.658298	42.332864
3504.376671	536265.053153	42.337869
3504.832502	536243.412668	42.342874
3504.582984	536207.285633	42.347879
3504.414980	536208.524638	42.352884
3504.906649	536198.193134	42.357888
3505.060647	536176.499233	42.362893
3505.139999	536166.333896	42.367898
3504.296049	536174.145297	42.372903
3504.533471	536166.733151	42.377908
3504.237200	536157.283831	42.382912
3503.899674	536144.103114	42.387917
3504.186987	536127.338281	42.392922
3504.363080	536118.218383	42.397927
3504.645155	536145.349617	42.402932
3504.552295	536104.651473	42.407936
3504.628727	536074.938206	42.412941
3504.032111	536085.892853	42.417946
3503.938808	536093.181561	42.422951
3504.204641	536093.190223	42.427956
3504.213332	536089.148012	42.432960
3504.216819	536099.300633	42.437965
3504.554607	536071.667578	42.442970
3504.219527	536062.982022	42.447975
3503.791486	536055.725506	42.452980
3503.961795	536053.476197	42.457984
3503.935602	536059.390474	42.462989
3504.486729	536057.384057	42.467994
3503.708093	536065.286215	42.472999
3504.743741	536036.987169	42.478004
3504.244561	536025.852405	42.483008
3504.727009	536032.646048	42.488013
3504.966146	536055.440134	42.493018
3504.911199	536011.553458	42.498023
3504.736877	535992.083234	42.503028
3503.928665	535958.367502	42.508032
3504.560207	535932.304186	42.513037
3504.820314	535925.848086	42.518042
3503.870289	535950.547708	42.523047
3504.410406	535946.926602	42.528052
3504.414779	535921.669569	42.533056
3504.154807	535907.062026	42.538061
3504.619529	535889.612227	42.543066
3504.634584	535884.760747	42.548071
3504.411401	535879.391271	42.553076
3504.267000	535849.914524	42.558080
3504.370325	535861.465895	42.563085
3504.494729	535858.112521	42.568090
3504.242123	535865.780106	42.573095
3504.432942	535853.273338	42.578100
3504.379973	535817.114324	42.583104
3504.359075	535854.750221	42.588109
3504.481474	535863.267780	42.593114
3504.604204	535845.417361	42.598119
3504.304472	535831.119110	42.603124
3504.200610	535836.742667	42.608128
3504.197224	535836.490798	42.613133
3504.425294	535810.440529	42.618138
3504.293366	535786.669705	42.623143
3504.082231	535773.771776	42.628148
3503.846507	535765.322916	42.633152
3504.137409	535763.307075	42.638157
3504.771195	535744.567554	42.643162
3504.861873	535737.430962	42.648167
3504.640346	535717.563743	42.653172
3504.312480	535735.800650	42.658176
3504.168684	535726.225940	42.663181
3504.644245	535716.957449	42.668186
3504.573662	535694.237575	42.673191
3504.665036	535662.702657	42.678196
3504.394013	535688.810801	42.683200
3504.430802	535689.512343	42.688205
3504.516717	535679.497189	42.693210
3504.597144	535682.212388	42.698215
3504.635468	535648.412702	42.703220
3504.081081	535625.668160	42.708224
3503.894959	535620.292737	42.713229
3504.763055	535596.666658	42.718234
3504.305670	535582.140521	42.723239
3504.150178	535607.321290	42.728244
3504.267096	535614.678028	42.733248
3504.311102	535607.599266	42.738253
3503.995501	535586.433379	42.743258
3503.852882	535588.325105	42.748263
3504.656715	535567.436901	42.753268
3504.257100	535573.258839	42.758272
3504.219355	535593.521143	42.763277
3504.237902	535571.393172	42.768282
3504.015439	535559.254567	42.773287
3504.794977	535527.863185	42.778292
3504.732012	535496.756434	42.783296
3504.138562	535535.089771	42.788301
3504.247098	535549.469353	42.793306
3504.179504	535543.671056	42.798311
3504.421847	535494.735011	42.803316
3504.348610	535510.103132	42.808321
3504.192837	535502.904352	42.813325
3504.660156	535487.827869	42.818330
3504.454662	535482.152371	42.823335
3504.373454	535457.867880	42.828340
3504.453735	535455.127568	42.833345
3504.459877	535424.666439	42.838349
3504.387512	535459.533126	42.843354
3504.279548	535415.855193	42.848359
3504.440417	535378.701578	42.853364
3504.306389	535413.628628	42.858369
3504.244676	535432.985667	42.863373
3504.360542	535390.838242	42.868378
3504.388161	535404.169938	42.873383
3504.093122	535372.038803	42.878388
3504.521017	535381.367099	42.883393
3504.210714	535386.871902	42.888397
3504.505908	535365.104032	42.893402
3504.324665	535361.798856	42.898407
3504.679803	535317.340247	42.903412
3504.733087	535336.578202	42.908417
3504.316579	535347.807993	42.913421
3504.560249	535334.080093	42.918426
3504.567662	535325.036902	42.923431
3504.372056	535302.487756	42.928436
3504.456777	535282.925182	42.933441
3504.062839	535267.529962	42.938445
3503.953987	535261.788595	42.943450
3504.099945	535284.447002	42.948455
3504.347228	535273.446295	42.953460
3504.512712	535233.715329	42.958465
3504.194257	535223.814303	42.963469
3503.964578	535220.718814	42.968474
3504.000360	535233.039060	42.973479
3503.914086	535239.771391	42.978484
3504.524285	535249.828684	42.983489
3504.427531	535234.588525	42.988493
3504.395778	535179.531934	42.993498
3504.378932	535180.747130	42.998503
3504.743298	535163.312374	43.003508
3504.236655	535185.568909	43.008513
3504.226185	535165.768654	43.013517
3504.490425	535154.310543	43.018522
3504.484736	535188.460086	43.023527
3504.207429	535167.944273	43.028532
3504.700752	535146.902517	43.033537
3504.631210	535111.249626	43.038541
3504.562555	535096.964689	43.043546
3504.439537	535132.244245	43.048551
3504.485924	535125.973136	43.053556
3504.328486	535090.384605	43.058561
3504.353448	535064.213632	43.063565
3504.476376	535105.364733	43.068570
3504.280760	535072.105915	43.073575
3503.832128	535048.737618	43.078580
3504.367764	535016.575495	43.083585
3504.328572	535060.480201	43.088589
3504.476218	535073.641665	43.093594
3504.159255	535076.621838	43.098599
3504.569452	535043.368247	43.103604
3504.710296	535039.709003	43.108609
3503.819527	535028.887983	43.113613
3504.138346	534995.295119	43.118618
3504.167570	535027.014727	43.123623
3504.226540	534980.227706	43.128628
3504.363850	534980.660813	43.133633
3503.992128	534973.243334	43.138637
3504.651204	534968.542364	43.143642
3504.136426	534977.262146	43.148647
3504.280871	534966.883668	43.153652
3504.004389	534934.395077	43.158657
3504.614725	534909.545785	43.163661
3504.716388	534913.520672	43.168666
3504.624746	534955.514344	43.173671
3504.354687	534932.218681	43.178676
3504.346671	534875.894350	43.183681
3504.663491	534872.459838	43.188685
3504.518923	534900.014305	43.193690
3504.336593	534905.296987	43.198695
3504.071225	534892.558441	43.203700
3504.505319	534893.752908	43.208705
3504.177958	534877.791097	43.213709
3504.111539	534884.722511	43.218714
3504.654683	534859.479626	43.223719
3504.662791	534829.825280	43.228724
3504.352724	534805.323350	43.233729
3504.522828	534782.564098	43.238733
3504.960073	534755.014009	43.243738
3504.589007	534760.478118	43.248743
3504.564661	534743.407425	43.253748
3505.280515	534723.340264	43.258753
3503.895668	534758.971643	43.263757
3504.307794	534756.229279	43.268762
3504.401827	534735.805756	43.273767
3504.258518	534722.340542	43.278772
3504.016846	534719.752016	43.283777
3504.314802	534702.630341	43.288781
3504.247568	534707.642315	43.293786
3503.693315	534716.873650	43.298791
3504.052220	534718.433633	43.303796
3504.522209	534691.737045	43.308801
3504.096969	534686.550638	43.313805
3504.441461	534670.836051	43.318810
3504.340569	534668.174750	43.323815
3504.639798	534640.292650	43.328820
3503.794459	534646.437961	43.333825
3503.969420	534659.848046	43.338829
3504.161234	534627.537387	43.343834
3504.093148	534609.867252	43.348839
3504.415689	534643.814569	43.353844
3504.442446	534652.145842	43.358849
3504.154050	534626.983481	43.363853
3504.211621	534608.182105	43.368858
3503.911936	534604.541864	43.373863
3504.021386	534594.825394	43.378868
3504.120316	534600.417350	43.383873
3504.480036	534631.024673	43.388877
3504.784767	534621.934081	43.393882
3504.210610	534602.020123	43.398887
3504.225212	534602.270564	43.403892
3504.507396	534581.918137	43.408897
3504.260113	534575.844771	43.413901
3504.435349	534550.356425	43.418906
3504.633258	534546.031318	43.423911
3504.454032	534541.563744	43.428916
3504.438802	534543.485980	43.433921
3504.291382	534525.525183	43.438925
3504.559702	534514.823720	43.443930
3504.335623	534531.631145	43.448935
3504.361037	534477.017679	43.453940
3504.676772	534449.991431	43.458945
3504.468866	534466.897406	43.463949
3504.515766	534491.391270	43.468954
3504.165481	534483.667061	43.473959
3504.028369	534417.914647	43.478964
3504.259588	534392.770821	43.483969
3504.267327	534393.325458	43.488973
3504.735914	534397.141453	43.493978
3503.962545	534433.030563	43.498983
3504.220125	534442.386345	43.503988
3504.091157	534403.407037	43.508993
3504.402371	534360.518684	43.513997
3504.250466	534375.849845	43.519002
3503.699560	534388.212967	43.524007
3503.889520	534387.728445	43.529012
3504.460491	534396.024365	43.534017
3504.484590	534416.581544	43.539021
3504.463545	534368.643410	43.544026
3504.609138	534388.070027	43.549031
3504.415843	534375.269146	43.554036
3504.493026	534345.047257	43.559041
3504.033237	534320.921850	43.564045
3504.769203	534282.361243	43.569050
3504.755136	534287.567023	43.574055
3504.206306	534281.642234	43.579060
3504.484507	534264.169570	43.584065
3504.350881	534267.575587	43.589069
3504.392902	534264.133854	43.594074
3504.216450	534272.497447	43.599079
3504.000262	534245.807501	43.604084
3504.130381	534239.472283	43.609089
3504.209494	534238.500090	43.614093
3504.558170	534218.338753	43.619098
3504.759044	534213.305825	43.624103
3504.502116	534234.463365	43.629108
3504.607095	534184.837633	43.634113
3504.391820	534188.307090	43.639117
3504.525171	534179.596957	43.644122
3504.789982	534135.098717	43.649127
3504.634596	534174.629151	43.654132
3504.695134	534153.856525	43.659137
3504.171840	534119.333960	43.664141
3504.663248	534094.249568	43.669146
3504.951673	534083.999303	43.674151
3505.095019	534049.421744	43.679156
3504.977750	534052.016916	43.684161
3504.224664	534043.295244	43.689165
3504.174095	534035.675001	43.694170
3504.094710	534028.817096	43.699175
3504.233293	534017.226449	43.704180
3504.011535	534027.365508	43.709185
3504.335129	534026.910375	43.714189
3504.465536	534013.199210	43.719194
3504.471092	534016.431727	43.724199
3504.645408	534022.618209	43.729204
3504.817384	533991.976498	43.734209
3504.408477	533946.270690	43.739213
3504.721478	533947.989568	43.744218
3504.543995	533928.264647	43.749223
3504.324894	533899.048588	43.754228
3504.491170	533897.860520	43.759233
3504.327830	533900.867156	43.764237
3504.479311	533881.090185	43.769242
3504.039872	533914.452248	43.774247
3504.061635	533890.603702	43.779252
3504.371074	533886.361827	43.784257
3504.030127	533890.356408	43.789261
3504.146857	533879.072230	43.794266
3503.968560	533882.030714	43.799271
3504.481486	533858.407613	43.804276
3504.825024	533826.475468	43.809281
3504.551359	533869.208124	43.814285
3504.532898	533843.850271	43.819290
3504.563515	533807.218677	43.824295
3504.408458	533778.750069	43.829300
3504.492155	533821.931577	43.834305
3503.904485	533815.558068	43.839309
3503.941977	533784.280443	43.844314
3504.547897	533757.914411	43.849319
3504.165827	533734.634650	43.854324
3504.229079	533764.633775	43.859329
3503.796582	533804.512066	43.864333
3504.354102	533773.253273	43.869338
3503.950128	533750.987399	43.874343
3504.200912	533759.283746	43.879348
3504.449263	533768.742435	43.884353
3504.052764	533752.184148	43.889357
3504.061734	533731.318067	43.894362
3504.205491	533728.921061	43.899367
3503.804449	533731.864256	43.904372
3504.302119	533706.121487	43.909377
3503.966492	533724.766143	43.914381
3504.588189	533743.259478	43.919386
3504.208417	533721.545459	43.924391
3503.914525	533700.929283	43.929396
3503.707806	533688.281517	43.934401
3503.622624	533683.899873	43.939405
3504.406913	533661.698677	43.944410
3504.454280	533682.960435	43.949415
3504.406003	533709.087226	43.954420
3504.258457	533659.146084	43.959425
3504.421216	533660.130932	43.964429
3504.369325	533638.112375	43.969434
3504.218871	533673.955306	43.974439
3503.996871	533673.737952	43.979444
3504.014447	533660.650553	43.984449
3504.582944	533603.927371	43.989453
3504.129320	533627.238687	43.994458
3504.011906	533624.377735	43.999463
3504.107454	533606.074351	44.004468
3504.092126	533628.962750	44.009473
3503.459954	533619.362879	44.014477
3504.535899	533591.810830	44.019482
3504.209830	533589.033369	44.024487
3503.944900	533597.714431	44.029492
3504.257293	533609.183921	44.034497
3504.134041	533594.350502	44.039501
3503.845204	533586.262488	44.044506
3503.973108	533577.603400	44.049511
3504.309373	533583.814983	44.054516
3504.482791	533587.576788	44.059521
3504.271691	533551.285916	44.064525
3504.450515	533515.943753	44.069530
3504.402060	533560.005729	44.074535
3503.901118	533556.599130	44.079540
3504.385015	533527.119705	44.084545
3504.011646	533544.911686	44.089549
3504.402735	533514.739615	44.094554
3504.188873	533499.667822	44.099559
3503.973890	533515.312924	44.104564
3503.999072	533511.520039	44.109569
3503.686402	533501.061265	44.114573
3504.227558	533479.453966	44.119578
3504.224535	533482.435345	44.124583
3504.202431	533476.477522	44.129588
3504.174749	533491.587837	44.134593
3503.909185	533502.491975	44.139597
3504.105762	533470.531805	44.144602
3503.875744	533454.704706	44.149607
3503.664019	533433.873105	44.154612
3503.557347	533434.294296	44.159617
3503.589843	533450.961295	44.164621
3503.632421	533483.894453	44.169626
3503.963225	533485.762132	44.174631
3503.815704	533471.740767	44.179636
3504.196634	533462.637458	44.184641
3504.073735	533492.060276	44.189645
3504.326558	533465.092782	44.194650
3504.042254	533501.866641	44.199655
3504.218101	533483.651464	44.204660
3504.456464	533485.533753	44.209665
3504.652424	533430.536010	44.214669
3504.373438	533459.882514	44.219674
3504.361252	533418.709873	44.224679
3504.288981	533433.877812	44.229684
3504.161556	533431.675182	44.234689
3504.380569	533401.681651	44.239693
3504.581494	533418.018939	44.244698
3504.106193	533405.413391	44.249703
3504.595586	533377.701060	44.254708
3504.939463	533361.025345	44.259713
3504.331453	533405.024628	44.264717
3503.771331	533378.993805	44.269722
3504.072343	533372.378619	44.274727
3504.683965	533337.371822	44.279732
3504.709654	533346.057615	44.284737
3503.962213	533347.085291	44.289741
3504.683199	533314.183058	44.294746
3504.417235	533299.826607	44.299751
3504.224812	533328.603940	44.304756
3504.074458	533294.273207	44.309761
3504.215307	533280.509225	44.314765
3504.171690	533312.193326	44.319770
3503.991400	533284.738233	44.324775
3504.190084	533289.961245	44.329780
3503.641504	533242.658750	44.334785
3503.501118	533268.295620	44.339789
3503.877272	533251.917818	44.344794
3504.072594	533253.402763	44.349799
3503.885797	533264.193575	44.354804
3504.162515	533270.414695	44.359809
3503.540082	533294.005796	44.364813
3504.302470	533241.898643	44.369818
3503.847185	533261.421633	44.374823
3503.974399	533286.612007	44.379828
3504.177319	533259.551000	44.384833
3504.311251	533254.376779	44.389837
3504.010054	533296.559618	44.394842
3503.780254	533278.509354	44.399847
3503.714041	533254.219042	44.404852
3504.294030	533221.086288	44.409857
3503.875598	533274.351995	44.414861
3504.207324	533266.620434	44.419866
3503.974911	533246.852809	44.424871
3503.762339	533246.229784	44.429876
3504.001996	533252.456768	44.434881
3504.052475	533253.863561	44.439885
3504.388286	533217.232867	44.444890
3504.302063	533271.203910	44.449895
3503.969642	533232.001210	44.454900
3504.385427	533185.859699	44.459905
3504.037271	533209.609667	44.464909
3503.702561	533205.418889	44.469914
3504.441066	533176.252217	44.474919
3503.931143	533202.856993	44.479924
3504.207012	533230.550058	44.484929
3503.658343	533216.187687	44.489933
3504.223716	533194.475124	44.494938
3504.148863	533210.401517	44.499943
3503.719700	533176.468242	44.504948
3504.258009	533198.916121	44.509953
3503.638481	533188.455110	44.514957
3504.143947	533158.466362	44.519962
3504.219326	533161.890110	44.524967
3503.715140	533179.804225	44.529972
3504.356887	533151.511673	44.534977
3504.126122	533155.741637	44.539981
3504.749125	533137.556431	44.544986
3504.160000	533118.249195	44.549991
3503.930993	533133.694807	44.554996
3504.103440	533167.315419	44.560001
3503.947511	533149.000720	44.565005
3503.990652	533116.104154	44.570010
3504.180018	533106.424648	44.575015
3503.951318	533160.519636	44.580020
3503.715768	533148.027553	44.585025
3503.403813	533142.165932	44.590029
3503.450296	533140.794652	44.595034
3504.008710	533136.563747	44.600039
3503.479338	533157.311107	44.605044
3504.346195	533151.313709	44.610049
3503.952135	533175.222551	44.615053
3503.755729	533186.065457	44.620058
3504.286913	533179.565379	44.625063
3504.009387	533170.111267	44.630068
3504.109508	533138.569838	44.635073
3503.821003	533133.765473	44.640077
3503.966276	533106.359657	44.645082
3504.649110	533109.182190	44.650087
3503.861586	533145.076499	44.655092
3504.353857	533097.861676	44.660097
3504.067590	533131.302251	44.665101
3504.396357	533140.041303	44.670106
3503.785291	533104.772523	44.675111
3504.462669	533072.331373	44.680116
3504.222927	533075.653376	44.685121
3504.046182	533098.972243	44.690125
3504.087235	533098.258606	44.695130
3504.091036	533108.564702	44.700135
3503.970142	533105.300027	44.705140
3504.266066	533084.943474	44.710145
3503.986689	533055.583790	44.715149
3504.291060	533033.154416	44.720154
3503.936289	533061.250586	44.725159
3503.948136	533024.670640	44.730164
3504.193336	533059.088347	44.735169
3504.019937	533085.539092	44.740173
3504.104463	533061.224657	44.745178
3504.520635	533032.159181	44.750183
3504.255624	533037.809218	44.755188
3504.211862	533014.828569	44.760193
3504.454975	532986.800810	44.765197
3504.400361	533023.792108	44.770202
3503.839172	533000.640601	44.775207
3504.593391	532960.911826	44.780212
3504.333864	532936.803140	44.785217
3504.133485	532982.052783	44.790221
3503.994433	533005.668968	44.795226
3504.142851	533006.302467	44.800231
3503.931955	533013.863817	44.805236
3504.482447	533003.975607	44.810241
3504.073140	532966.451634	44.815245
3504.123864	532927.743364	44.820250
3504.307438	532935.040318	44.825255
3503.882963	532960.874159	44.830260
3504.273123	532924.537325	44.835265
3504.042850	532940.640125	44.840269
3504.085823	532933.863445	44.845274
3504.710714	532882.534667	44.850279
3504.262434	532934.341086	44.855284
3504.421339	532920.978116	44.860289
3504.183644	532904.798010	44.865293
3504.502929	532871.756242	44.870298
3504.831981	532831.488057	44.875303
3504.466393	532869.034099	44.880308
3504.458433	532858.678304	44.885313
3503.964943	532826.320645	44.890317
3504.599240	532804.899788	44.895322
3504.711212	532832.366848	44.900327
3504.216016	532830.980102	44.905332
3504.397735	532801.344974	44.910337
3504.114329	532793.861967	44.915341
3504.271273	532796.717149	44.920346
3504.390894	532818.271807	44.925351
3503.956034	532786.662648	44.930356
3504.253520	532793.588002	44.935361
3504.436000	532748.290443	44.940365
3504.019346	532761.644098	44.945370
3504.544846	532737.259465	44.950375
3504.538624	532765.907361	44.955380
3504.301142	532730.477643	44.960385
3504.324587	532686.417602	44.965389
3504.429482	532733.438567	44.970394
3504.311919	532708.094529	44.975399
3504.320930	532700.413692	44.980404
3504.453195	532673.160743	44.985409
3504.068284	532713.489012	44.990413
3504.109301	532693.273282	44.995418
3504.648196	532664.996106	45.000423
3504.426109	532645.983941	45.005428
3504.345518	532649.786118	45.010433
3503.929599	532660.765128	45.015437
3503.821078	532637.491016	45.020442
3503.523830	532632.687877	45.025447
3503.361208	532636.503021	45.030452
3504.165351	532630.262721	45.035457
3503.801655	532633.402312	45.040461
3504.300953	532611.497288	45.045466
3504.467918	532599.800056	45.050471
3503.762461	532614.816242	45.055476
3504.063536	532610.625869	45.060481
3503.918512	532623.734616	45.065485
3503.990502	532658.786866	45.070490
3503.724643	532641.752036	45.075495
3503.794313	532638.052955	45.080500
3504.451404	532603.542567	45.085505
3504.064502	532634.271822	45.090509
3503.617098	532629.239794	45.095514
3504.177076	532603.081172	45.100519
3504.240455	532570.432877	45.105524
3504.379907	532600.422200	45.110529
3503.918250	532633.386320	45.115533
3504.152297	532589.444292	45.120538
3504.330752	532603.866077	45.125543
3504.132000	532610.061559	45.130548
3504.305242	532580.023161	45.135553
3504.356417	532562.079232	45.140557
3504.130453	532562.822442	45.145562
3503.986687	532586.642102	45.150567
3503.996270	532548.444633	45.155572
3504.446413	532529.730278	45.160577
3503.903410	532536.434912	45.165581
3504.325305	532515.097751	45.170586
3504.083481	532497.604248	45.175591
3503.987433	532546.274309	45.180596
3504.054484	532548.436407	45.185601
3503.526537	532535.484804	45.190605
3503.644593	532532.283292	45.195610
3504.236047	532512.687673	45.200615
3504.198767	532555.588664	45.205620
3504.171644	532534.524590	45.210625
3503.960114	532520.967202	45.215629
3504.002815	532520.910092	45.220634
3504.164771	532526.897027	45.225639
3503.843053	532523.209251	45.230644
3503.940022	532498.336208	45.235649
3504.021930	532477.355874	45.240653
3504.101594	532473.655175	45.245658
3504.018028	532492.059366	45.250663
3503.679379	532478.067314	45.255668
3504.182978	532495.065074	45.260673
3503.877301	532535.835996	45.265677
3503.903414	532533.154256	45.270682
3504.307790	532508.081073	45.275687
3504.027502	532474.425885	45.280692
3504.037114	532464.572293	45.285697
3503.896255	532454.338282	45.290701
3503.958848	532448.114058	45.295706
3503.865145	532457.273934	45.300711
3503.945511	532472.065014	45.305716
3503.778553	532460.369928	45.310721
3504.024584	532449.367427	45.315725
3503.982351	532432.903319	45.320730
3504.092241	532481.187364	45.325735
3503.776248	532485.228882	45.330740
3504.258698	532450.998380	45.335745
3504.284836	532414.212649	45.340749
3503.839823	532419.436637	45.345754
3503.588456	532423.973200	45.350759
3503.811533	532438.287038	45.355764
3504.309473	532449.980680	45.360769
3503.981852	532456.499736	45.365773
3504.005563	532458.719220	45.370778
3504.357816	532441.333862	45.375783
3504.116117	532457.085295	45.380788
3504.036723	532464.120884	45.385793
3504.314918	532452.961730	45.390797
3504.211078	532429.534995	45.395802
3504.188484	532433.782778	45.400807
3503.900672	532415.942781	45.405812
3504.213870	532392.753228	45.410817
3504.510430	532368.909451	45.415821
3504.217489	532395.430781	45.420826
3504.503091	532390.080730	45.425831
3504.081701	532388.530705	45.430836
3504.158517	532384.729386	45.435841
3504.303274	532380.816280	45.440845
3504.160176	532379.020173	45.445850
3504.234333	532344.550819	45.450855
3504.023512	532319.827186	45.455860
3504.106599	532303.999958	45.460865
3503.702937	532297.040966	45.465869
3503.988852	532295.631771	45.470874
3504.189498	532302.926323	45.475879
3503.672537	532323.167576	45.480884
3503.912815	532342.329159	45.485889
3504.050810	532360.647964	45.490893
3503.848783	532358.558020	45.495898
3503.916770	532311.357355	45.500903
3503.897103	532321.263481	45.505908
3503.392959	532330.286200	45.510913
3503.936279	532349.551453	45.515917
3503.916393	532340.864514	45.520922
3503.925023	532330.606795	45.525927
3503.510860	532333.249174	45.530932
3503.820491	532335.019291	45.535937
3503.788488	532336.489728	45.540941
3503.703120	532336.806531	45.545946
3503.845096	532331.428635	45.550951
3504.074933	532326.036851	45.555956
3503.833853	532338.958919	45.560961
3503.541442	532347.645016	45.565965
3503.975098	532367.786498	45.570970
3504.416521	532360.390827	45.575975
3504.333443	532325.693659	45.580980
3503.870590	532289.187014	45.585985
3504.616629	532270.678210	45.590989
3504.563545	532264.977445	45.595994
3504.331822	532281.384301	45.600999
3503.668480	532288.108059	45.606004
3503.966088	532285.383368	45.611009
3504.202059	532296.562755	45.616013
3504.183295	532302.578337	45.621018
3504.555188	532281.299286	45.626023
3504.325758	532261.428890	45.631028
3504.343193	532237.831127	45.636033
3503.947364	532244.866300	45.641037
3503.676877	532248.092286	45.646042
3504.151262	532240.590299	45.651047
3504.243046	532221.679587	45.656052
3504.098033	532241.710586	45.661057
3504.194602	532261.602330	45.666061
3504.430263	532242.972055	45.671066
3504.736130	532201.240687	45.676071
3504.142991	532209.469137	45.681076
3504.388779	532189.371969	45.686081
3504.435200	532205.128645	45.691085
3504.755889	532188.253246	45.696090
3504.388964	532165.372946	45.701095
3504.268058	532178.528780	45.706100
3504.354800	532176.090022	45.711105
3504.350024	532184.882326	45.716109
3504.195199	532141.556277	45.721114
3504.504411	532102.956690	45.726119
3503.685489	532124.610110	45.731124
3503.939680	532137.201442	45.736129
3504.196374	532099.317501	45.741133
3504.393229	532098.478144	45.746138
3504.407340	532086.855212	45.751143
3503.399219	532089.844130	45.756148
3503.980370	532079.546290	45.761153
3503.945635	532082.634000	45.766157
3504.075228	532086.554671	45.771162
3504.104708	532103.375162	45.776167
3503.992585	532088.083823	45.781172
3504.221528	532053.134635	45.786177
3503.662929	532091.673032	45.791181
3503.501163	532109.332150	45.796186
3503.716743	532080.751341	45.801191
3503.624888	532046.105465	45.806196
3503.977191	532048.828858	45.811201
3503.622258	532073.390030	45.816205
3503.718169	532081.661224	45.821210
3504.220340	532068.647480	45.826215
3504.314300	532058.426624	45.831220
3503.908513	532064.149785	45.836225
3503.864769	532062.590567	45.841229
3504.060134	532048.867412	45.846234
3504.473582	532052.945333	45.851239
3504.096826	532080.288852	45.856244
3503.940087	532079.606429	45.861249
3504.251056	532074.302788	45.866253
3503.621149	532051.817563	45.871258
3504.418000	532038.959325	45.876263
3504.145703	532034.202583	45.881268
3504.416716	532026.985265	45.886273
3504.059026	532018.503111	45.891277
3503.897865	532005.594150	45.896282
3504.081785	532016.781963	45.901287
3503.801182	532049.213439	45.906292
3504.077903	532047.856201	45.911297
3504.388636	532024.615968	45.916301
3504.188304	532028.790900	45.921306
3504.148936	532011.770113	45.926311
3503.900001	532016.407461	45.931316
3504.105205	532008.594226	45.936321
3504.711638	531982.073547	45.941325
3504.395410	531965.652251	45.946330
3504.290052	532012.658086	45.951335
3503.964076	532004.069860	45.956340
3503.893039	531973.209966	45.961345
3504.598532	531938.538889	45.966349
3504.960546	531920.241944	45.971354
3504.649646	531907.103937	45.976359
3504.347022	531895.935129	45.981364
3504.254259	531916.918282	45.986369
3504.085397	531913.155677	45.991373
3504.262178	531871.443833	45.996378
3504.443427	531891.726873	46.001383
3504.085761	531894.562500	46.006388
3504.264843	531893.523837	46.011393
3504.093426	531875.967985	46.016397
3504.121198	531861.311154	46.021402
3504.091200	531854.697119	46.026407
3503.687210	531862.744276	46.031412
3504.243549	531825.064947	46.036417
3504.105317	531820.943794	46.041421
3504.035127	531858.192942	46.046426
3503.871059	531858.522192	46.051431
3503.728379	531855.462802	46.056436
3503.694968	531825.000879	46.061441
3504.169414	531801.633390	46.066445
3504.406724	531782.395990	46.071450
3504.314620	531834.553966	46.076455
3504.149912	531842.159107	46.081460
3504.299886	531811.415544	46.086465
3504.288426	531847.998591	46.091469
3504.151937	531786.984453	46.096474
3504.683576	531792.407979	46.101479
3503.683170	531790.646243	46.106484
3504.299545	531763.567833	46.111489
3504.279895	531752.000516	46.116493
3504.444632	531755.663083	46.121498
3504.489687	531770.965672	46.126503
3504.024168	531758.054082	46.131508
3504.519849	531716.392479	46.136513
3504.179484	531769.347809	46.141517
3503.886666	531744.585699	46.146522
3503.830665	531741.411535	46.151527
3504.113177	531703.522557	46.156532
3503.573303	531718.109214	46.161537
3504.072475	531703.327208	46.166541
3504.086375	531707.165206	46.171546
3504.118262	531712.768796	46.176551
3503.639129	531709.762552	46.181556
3504.399113	531683.368682	46.186561
3503.983148	531734.163425	46.191565
3503.886964	531720.587113	46.196570
3503.910490	531702.899204	46.201575
3504.184990	531687.243209	46.206580
3504.007137	531700.256863	46.211585
3504.106897	531727.929900	46.216589
3503.917754	531693.702834	46.221594
3503.716268	531683.225265	46.226599
3503.377266	531677.973688	46.231604
3503.524672	531692.754909	46.236609
3504.441161	531682.201705	46.241613
3504.091379	531678.770797	46.246618
3504.400364	531675.842097	46.251623
3504.114624	531716.056205	46.256628
3504.156066	531707.813962	46.261633
3504.441628	531689.276196	46.266637
3504.240308	531678.545965	46.271642
3504.175904	531663.499303	46.276647
3503.995721	531674.997539	46.281652
3504.001154	531642.457523	46.286657
3504.250631	531611.091518	46.291661
3504.302341	531614.418293	46.296666
3504.190661	531672.895779	46.301671
3503.721343	531642.401340	46.306676
3503.988871	531616.489403	46.311681
3504.275102	531594.414528	46.316685
3503.990868	531605.221880	46.321690
3503.913673	531633.529375	46.326695
3503.475257	531619.299685	46.331700
3503.944403	531597.650649	46.336705
3504.095408	531612.027161	46.341709
3503.645855	531610.885723	46.346714
3503.841277	531609.692878	46.351719
3503.988085	531600.777074	46.356724
3503.806662	531621.724107	46.361729
3504.001876	531629.676683	46.366733
3503.962717	531602.246856	46.371738
3504.338538	531604.663449	46.376743
3504.005822	531611.335239	46.381748
3504.123328	531608.335734	46.386753
3504.126534	531569.075818	46.391757
3504.014085	531588.344597	46.396762
3504.120568	531558.516900	46.401767
3504.180837	531586.095374	46.406772
3503.984253	531568.189464	46.411777
3504.526345	531537.585502	46.416781
3504.119010	531542.500660	46.421786
3504.011789	531563.941315	46.426791
3503.959420	531538.231388	46.431796
3504.399461	531527.248108	46.436801
3504.282789	531558.593616	46.441805
3504.173873	531575.032328	46.446810
3504.076631	531572.521501	46.451815
3503.944061	531549.097989	46.456820
3504.247862	531507.971432	46.461825
3504.046416	531531.498646	46.466829
3503.956132	531512.767436	46.471834
3503.923878	531494.431251	46.476839
3504.472220	531479.590737	46.481844
3503.758082	531482.533302	46.486849
3504.033510	531514.675896	46.491853
3504.116466	531496.523615	46.496858
3504.369308	531465.106260	46.501863
3504.162067	531487.320740	46.506868
3503.893664	531488.020179	46.511873
3503.893238	531450.478472	46.516877
3504.015083	531437.120095	46.521882
3503.917816	531488.269486	46.526887
3503.672095	531494.978104	46.531892
3503.664979	531470.726210	46.536897
3503.576109	531455.531632	46.541901
3503.858719	531440.834134	46.546906
3503.754820	531432.008385	46.551911
3503.689407	531451.926757	46.556916
3504.020691	531430.349807	46.561921
3504.296744	531430.003175	46.566925
3503.959202	531431.370402	46.571930
3504.415984	531439.180681	46.576935
3503.852907	531476.306522	46.581940
3503.918111	531474.325807	46.586945
3504.004064	531480.021990	46.591949
3504.246015	531487.815670	46.596954
3504.220026	531466.295233	46.601959
3504.161759	531465.294054	46.606964
3504.001854	531444.805303	46.611969
3504.164039	531432.147932	46.616973
3503.496957	531432.556688	46.621978
3504.587946	531407.423761	46.626983
3504.244324	531408.539312	46.631988
3504.188078	531441.694500	46.636993
3504.278189	531412.071223	46.641997
3504.043717	531430.753148	46.647002
3504.397397	531418.772889	46.652007
3503.867724	531422.949503	46.657012
3504.147108	531401.784937	46.662017
3503.684799	531398.523335	46.667021
3503.778410	531407.755275	46.672026
3504.486272	531408.603591	46.677031
3504.112343	531400.123666	46.682036
3504.207702	531389.043181	46.687041
3504.212438	531375.854844	46.692045
3504.245438	531384.186876	46.697050
3504.156556	531384.150558	46.702055
3503.912301	531347.000834	46.707060
3504.124967	531318.419098	46.712065
3504.439982	531313.923011	46.717069
3503.786149	531325.799527	46.722074
3503.754256	531314.486462	46.727079
3503.592919	531315.724794	46.732084
3503.934019	531286.213197	46.737089
3504.112877	531336.612049	46.742093
3504.084605	531338.738852	46.747098
3504.156855	531315.990013	46.752103
3503.945571	531310.263375	46.757108
3504.036806	531291.553741	46.762113
3504.089894	531341.366117	46.767117
3503.805811	531330.497144	46.772122
3504.016933	531294.791165	46.777127
3503.885702	531305.928238	46.782132
3503.873711	531318.713882	46.787137
3503.706485	531290.394246	46.792141
3503.829641	531261.169687	46.797146
3504.120109	531249.704571	46.802151
3504.058879	531245.621625	46.807156
3504.243728	531239.630242	46.812161
3504.392878	531240.415284	46.817165
3504.180845	531297.646821	46.822170
3504.051402	531301.659157	46.827175
3504.081056	531308.122221	46.832180
3504.217630	531287.586408	46.837185
3504.208458	531252.572015	46.842189
3503.544096	531246.967488	46.847194
3503.821361	531250.460805	46.852199
3503.894033	531263.031001	46.857204
3503.932241	531277.981455	46.862209
3503.938875	531286.519819	46.867213
3503.622320	531266.813514	46.872218
3503.910588	531215.785126	46.877223
3503.287037	531250.546226	46.882228
3503.669112	531261.147452	46.887233
3503.706867	531279.938117	46.892237
3503.979761	531271.760122	46.897242
3504.298304	531229.114661	46.902247
3503.765585	531253.048344	46.907252
3503.541238	531254.498753	46.912257
3503.784449	531248.397093	46.917261
3503.356743	531257.054645	46.922266
3503.831701	531258.141892	46.927271
3503.702166	531252.200200	46.932276
3504.036208	531239.060759	46.937281
3504.212969	531223.874504	46.942285
3503.917805	531260.705870	46.947290
3503.975573	531268.730881	46.952295
3503.899192	531236.506122	46.957300
3504.302756	531225.275756	46.962305
3504.013710	531255.992242	46.967309
3504.224670	531255.858007	46.972314
3504.214048	531222.410150	46.977319
3504.337831	531201.067793	46.982324
3504.566541	531188.551297	46.987329
3504.056991	531189.996258	46.992333
3504.038499	531208.846425	46.997338
3504.129443	531241.675603	47.002343
3504.219518	531257.527388	47.007348
3504.177761	531228.985699	47.012353
3504.205561	531220.593771	47.017357
3503.612304	531195.575106	47.022362
3504.184726	531163.803472	47.027367
3504.140490	531152.896468	47.032372
3503.879546	531200.333553	47.037377
3503.984249	531211.686047	47.042381
3504.005935	531204.356172	47.047386
3504.202516	531190.682604	47.052391
3503.637371	531189.306760	47.057396
3503.938810	531165.005629	47.062401
3504.188256	531172.798281	47.067405
3503.842517	531198.572049	47.072410
3504.180262	531178.560112	47.077415
3504.051189	531178.226974	47.082420
3504.254817	531182.894099	47.087425
3503.975745	531176.420199	47.092429
3503.887835	531168.602343	47.097434
3504.142297	531131.575405	47.102439
3503.967183	531156.210647	47.107444
3503.637271	531157.374577	47.112449
3504.122529	531128.345186	47.117453
3503.928255	531160.562738	47.122458
3504.048235	531165.798901	47.127463
3503.914062	531149.853261	47.132468
3503.642686	531120.993965	47.137473
3504.111371	531113.290231	47.142477
3503.861743	531111.409757	47.147482
3504.486539	531091.756572	47.152487
3504.173662	531095.494779	47.157492
3504.246747	531091.036864	47.162497
3504.594966	531098.056012	47.167501
3504.415901	531085.149122	47.172506
3504.325699	531047.367998	47.177511
3504.315841	531058.182890	47.182516
3503.825758	531086.910326	47.187521
3503.910314	531088.412986	47.192525
3503.648110	531088.555646	47.197530
3504.443401	531064.176309	47.202535
3503.653264	531065.564567	47.207540
3503.814556	531064.983422	47.212545
3503.605970	531061.479533	47.217549
3504.748905	531039.015838	47.222554
3504.155596	531014.704298	47.227559
3504.174227	531016.419500	47.232564
3504.681572	531010.073888	47.237569
3504.735080	530992.380441	47.242573
3504.536728	530978.415401	47.247578
3504.175449	530982.312871	47.252583
3503.808619	531013.547414	47.257588
3503.699949	531035.292193	47.262593
3504.193185	531026.978190	47.267597
3504.076835	531009.261077	47.272602
3503.795200	530979.544151	47.277607
3503.722130	530993.400823	47.282612
3503.788929	531017.391701	47.287617
3503.905274	531007.318210	47.292621
3503.852564	530992.218528	47.297626
3503.633216	530992.404944	47.302631
3503.797027	531027.749504	47.307636
3504.035122	530983.347579	47.312641
3503.677154	530992.954306	47.317645
3503.716531	531004.873093	47.322650
3504.014757	530977.237266	47.327655
3504.036358	530952.373684	47.332660
3503.771074	530969.797797	47.337665
3503.943516	530981.341868	47.342669
3503.757683	530998.248101	47.347674
3504.114027	531005.569181	47.352679
3504.094366	531007.896784	47.357684
3503.851085	531004.600482	47.362689
3504.210475	530994.690687	47.367693
3504.070260	530972.126517	47.372698
3503.778581	531005.572479	47.377703
3503.862313	531016.524196	47.382708
3503.936811	530994.785116	47.387713
3504.173119	530977.062761	47.392717
3503.330360	530988.160924	47.397722
3503.449202	530979.350247	47.402727
3503.327404	530985.028915	47.407732
3503.484740	530974.039401	47.412737
3503.874456	530947.197527	47.417741
3503.627609	530946.781939	47.422746
3504.271815	530960.171575	47.427751
3503.855509	530979.943885	47.432756
3503.475761	530983.440041	47.437761
3503.354508	530993.969409	47.442765
3503.308861	530999.080217	47.447770
3503.768291	531003.504851	47.452775
3503.569516	531020.463635	47.457780
3503.468103	531028.059166	47.462785
3503.980692	531020.702150	47.467789
3503.644574	531033.791896	47.472794
3503.650554	531026.919181	47.477799
3503.531920	531032.849976	47.482804
3504.261195	531017.020383	47.487809
3504.117945	530999.054866	47.492813
3503.957052	530987.004016	47.497818
3503.807097	530980.459100	47.502823
3503.979092	531029.899967	47.507828
3503.832046	531032.197170	47.512833
3503.966690	531029.093789	47.517837
3503.881580	531040.375348	47.522842
3504.049674	531032.011676	47.527847
3503.995633	531015.143714	47.532852
3504.032475	531010.085156	47.537857
3504.118433	531029.020090	47.542861
3503.790162	531018.865288	47.547866
3504.599366	530987.914870	47.552871
3504.157861	530963.225554	47.557876
3503.990010	530945.314392	47.562881
3504.092094	530940.447618	47.567885
3503.825925	530940.287730	47.572890
3504.302906	530931.369895	47.577895
3504.163425	530949.329969	47.582900
3504.244423	530942.344303	47.587905
3504.249658	530971.296842	47.592909
3503.943925	530978.722571	47.597914
3503.919013	530965.033283	47.602919
3504.081508	530960.106438	47.607924
3503.918388	530941.335529	47.612929
3503.717059	530923.682279	47.617933
3503.769351	530905.938398	47.622938
3503.901538	530955.133145	47.627943
3503.669926	530940.465921	47.632948
3503.906627	530910.161651	47.637953
3503.872679	530907.640713	47.642957
3504.087415	530954.144364	47.647962
3503.969451	530955.274811	47.652967
3503.948600	530966.344150	47.657972
3503.837935	530962.723705	47.662977
3504.173312	530967.117427	47.667981
3503.970145	530976.851286	47.672986
3504.205670	530959.684855	47.677991
3504.025498	530936.470070	47.682996
3503.556066	530908.045918	47.688001
3504.006853	530890.239039	47.693005
3504.012442	530871.340324	47.698010
3504.052759	530915.901006	47.703015
3503.880672	530904.407684	47.708020
3503.874115	530891.928136	47.713025
3503.909703	530891.922674	47.718029
3503.486759	530903.459841	47.723034
3503.911843	530889.901486	47.728039
3504.615502	530873.772622	47.733044
3504.103998	530924.231374	47.738049
3504.038110	530892.509544	47.743053
3504.235487	530882.675814	47.748058
3504.101608	530914.227443	47.753063
3503.893377	530904.508359	47.758068
3503.834969	530870.915718	47.763073
3503.845375	530849.136038	47.768077
3503.627591	530850.737034	47.773082
3503.913136	530891.519845	47.778087
3503.922034	530880.856902	47.783092
3503.451470	530872.442493	47.788097
3503.932995	530845.282759	47.793101
3503.790305	530856.118784	47.798106
3503.812863	530903.613017	47.803111
3503.913152	530893.895696	47.808116
3503.740837	530876.439926	47.813121
3503.638276	530882.620884	47.818125
3503.675822	530892.266223	47.823130
3503.377955	530874.527117	47.828135
3503.969957	530870.492422	47.833140
3503.788167	530871.178198	47.838145
3504.435796	530854.148639	47.843149
3504.113134	530848.742611	47.848154
3503.817427	530857.379521	47.853159
3504.043442	530880.486444	47.858164
3503.830974	530857.630352	47.863169
3504.093423	530850.767556	47.868173
3504.103778	530871.331572	47.873178
3504.192550	530869.599703	47.878183
3503.840738	530847.169854	47.883188
3504.154021	530840.248490	47.888193
3504.487584	530823.420123	47.893197
3503.651154	530854.577610	47.898202
3503.961912	530818.046331	47.903207
3503.663465	530857.961463	47.908212
3503.868615	530833.826628	47.913217
3503.822940	530852.226753	47.918221
3503.760771	530836.319944	47.923226
3503.937389	530853.522756	47.928231
3503.923233	530844.985671	47.933236
3503.738714	530863.054020	47.938241
3504.071197	530840.920249	47.943245
3504.142265	530858.442915	47.948250
3504.123092	530833.535060	47.953255
3504.165112	530872.992109	47.958260
3503.976216	530824.513806	47.963265
3504.257398	530844.782406	47.968269
3504.076409	530844.255348	47.973274
3504.270040	530790.259296	47.978279
3503.750520	530806.814234	47.983284
3503.655828	530803.595465	47.988289
3504.456538	530789.927130	47.993293
3504.430038	530784.322684	47.998298
3503.948902	530810.219545	48.003303
3504.067197	530797.821249	48.008308
3503.878790	530784.561881	48.013313
3504.203546	530740.701403	48.018317
3503.970771	530742.304779	48.023322
3504.327281	530750.636548	48.028327
3504.532992	530754.040226	48.033332
3504.190546	530744.544375	48.038337
3504.197413	530731.910988	48.043341
3504.156623	530744.802710	48.048346
3504.204722	530763.693416	48.053351
3503.679036	530742.907850	48.058356
3503.992629	530743.717459	48.063361
3504.008819	530737.146182	48.068365
3503.583394	530748.026966	48.073370
3503.464553	530742.285510	48.078375
3504.131064	530750.265107	48.083380
3503.813725	530754.458867	48.088385
3504.168874	530735.201564	48.093389
3504.631120	530720.222354	48.098394
3504.435557	530697.616008	48.103399
3504.111966	530688.571912	48.108404
3504.426919	530676.597210	48.113409
3504.344222	530670.344715	48.118413
3504.001238	530687.528768	48.123418
3503.841283	530689.828061	48.128423
3503.723021	530688.886844	48.133428
3503.262615	530704.826186	48.138433
3503.635690	530700.674459	48.143437
3503.731603	530705.156630	48.148442
3503.834905	530696.550371	48.153447
3504.790849	530684.878611	48.158452
3504.248753	530666.874689	48.163457
3503.721264	530673.426067	48.168461
3503.732447	530678.224817	48.173466
3503.818852	530678.817684	48.178471
3503.961841	530695.874393	48.183476
3503.799684	530702.772261	48.188481
3503.883879	530697.251349	48.193485
3504.266413	530696.433105	48.198490
3504.447740	530637.739185	48.203495
3503.785899	530669.324215	48.208500
3503.388530	530671.762092	48.213505
3504.327822	530652.513428	48.218509
3503.853000	530677.045197	48.223514
3503.940569	530679.659081	48.228519
3504.159668	530686.749351	48.233524
3504.259871	530680.316363	48.238529
3504.233596	530622.008905	48.243533
3503.992271	530611.334795	48.248538
3504.215404	530634.392005	48.253543
3504.221079	530653.845381	48.258548
3504.061873	530655.639259	48.263553
3504.108130	530605.405092	48.268557
3503.934210	530616.246218	48.273562
3503.767336	530627.136752	48.278567
3503.710999	530628.257483	48.283572
3503.459046	530640.626831	48.288577
3503.555767	530633.790133	48.293581
3503.431111	530631.182426	48.298586
3504.158121	530612.472566	48.303591
3504.354194	530607.136062	48.308596
3504.126606	530621.068012	48.313601
3503.685194	530608.859087	48.318605
3503.421427	530606.323892	48.323610
3504.095818	530610.563074	48.328615
3504.127970	530597.470812	48.333620
3503.956903	530602.096267	48.338625
3503.861976	530621.312931	48.343629
3503.917533	530644.042899	48.348634
3504.133010	530640.219245	48.353639
3504.367446	530630.379500	48.358644
3503.931537	530629.387421	48.363649
3504.422307	530641.841505	48.368653
3504.175755	530647.287360	48.373658
3504.047755	530618.202362	48.378663
3504.298373	530597.091792	48.383668
3504.124606	530584.992139	48.388673
3504.245138	530587.499769	48.393677
3503.928893	530597.605445	48.398682
3504.091214	530580.955475	48.403687
3503.986448	530574.706429	48.408692
3503.455083	530595.962785	48.413697
3503.638317	530565.918955	48.418701
3504.107453	530555.637828	48.423706
3503.759384	530539.523252	48.428711
3503.866702	530568.359337	48.433716
3503.741914	530605.064248	48.438721
3503.929556	530603.670437	48.443725
3504.010125	530611.843770	48.448730
3504.085499	530598.239375	48.453735
3504.108043	530561.854114	48.458740
3504.076802	530507.286267	48.463745
3504.526508	530508.781804	48.468749
3504.538687	530518.380851	48.473754
3504.172473	530508.939143	48.478759
3504.192709	530483.620262	48.483764
3504.471037	530469.731027	48.488769
3504.392219	530465.802250	48.493773
3503.196899	530505.152589	48.498778
3503.736066	530501.681989	48.503783
3503.954341	530516.958423	48.508788
3503.929489	530512.010517	48.513793
3504.145744	530472.309947	48.518797
3503.690956	530481.629102	48.523802
3503.626644	530499.880992	48.528807
3503.816391	530509.805695	48.533812
3503.793948	530513.194953	48.538817
3504.826252	530489.282578	48.543821
3503.894419	530456.180807	48.548826
3504.110755	530440.330643	48.553831
3503.739838	530460.096430	48.558836
3503.509118	530476.252356	48.563841
3503.805056	530474.790888	48.568845
3503.941078	530497.356759	48.573850
3503.619061	530500.439651	48.578855
3503.920399	530455.470407	48.583860
3503.761128	530436.546694	48.588865
3504.380202	530444.483414	48.593869
3503.804358	530454.276495	48.598874
3504.001861	530451.819966	48.603879
3503.778295	530456.504292	48.608884
3504.012234	530484.006721	48.613889
3504.033153	530498.657464	48.618893
3503.974800	530480.122100	48.623898
3504.305532	530440.453888	48.628903
3504.336121	530444.239026	48.633908
3503.495900	530450.233551	48.638913
3504.252598	530462.241504	48.643917
3504.096521	530468.127898	48.648922
3504.011991	530423.017423	48.653927
3504.359977	530384.963332	48.658932
3503.995704	530406.648313	48.663937
3504.148252	530445.179408	48.668941
3504.101655	530410.724896	48.673946
3504.134615	530407.132155	48.678951
3503.500611	530414.205782	48.683956
3503.863864	530443.860672	48.688961
3503.814222	530446.193096	48.693965
3504.056834	530458.029647	48.698970
3504.084500	530410.728582	48.703975
3504.535945	530383.724401	48.708980
3504.077182	530364.999529	48.713985
3504.166973	530359.831332	48.718989
3504.377398	530382.587733	48.723994
3504.294211	530364.460405	48.728999
3504.192472	530322.081037	48.734004
3503.572058	530350.830410	48.739009
3504.288009	530352.031229	48.744013
3503.748868	530369.297161	48.749018
3503.663348	530372.999604	48.754023
3504.164338	530332.748373	48.759028
3504.159931	530337.195972	48.764033
3503.815295	530360.040129	48.769037
3503.979024	530351.979974	48.774042
3504.194925	530338.049958	48.779047
3503.911865	530361.591817	48.784052
3503.528522	530383.785154	48.789057
3504.207336	530356.088089	48.794061
3503.975564	530354.912136	48.799066
3503.946980	530310.196744	48.804071
3504.167228	530296.619723	48.809076
3503.084899	530323.117710	48.814081
3503.630960	530338.847824	48.819085
3503.636518	530378.665591	48.824090
3503.753196	530328.975256	48.829095
3503.240769	530351.189039	48.834100
3503.402450	530382.189710	48.839105
3503.768773	530364.294526	48.844109
3503.719518	530342.068794	48.849114
3503.418396	530375.315460	48.854119
3503.655542	530350.012614	48.859124
3503.817880	530332.705475	48.864129
3503.401066	530364.606107	48.869133
3503.968799	530379.675851	48.874138
3504.193587	530334.617299	48.879143
3503.893465	530366.347891	48.884148
3503.470822	530398.249377	48.889153
3503.815930	530355.092043	48.894157
3503.780449	530352.369134	48.899162
3503.649920	530382.001117	48.904167
3503.757786	530393.606357	48.909172
3503.894211	530350.583053	48.914177
3504.155181	530339.020877	48.919181
3503.855314	530345.132166	48.924186
3504.004494	530366.685522	48.929191
3504.254971	530375.438498	48.934196
3503.905556	530415.615459	48.939201
3504.025530	530388.057302	48.944205
3504.215789	530404.146769	48.949210
3504.121820	530392.893382	48.954215
3504.291880	530363.255496	48.959220
3504.106634	530355.301027	48.964225
3504.348903	530359.456980	48.969229
3503.958581	530359.417768	48.974234
3503.571289	530342.803878	48.979239
3503.923504	530346.285553	48.984244
3503.171165	530349.082766	48.989249
3503.878010	530340.734644	48.994253
3504.387448	530316.702521	48.999258
3503.911798	530316.626263	49.004263
3503.809245	530351.812312	49.009268
3503.847609	530359.588198	49.014273
3504.064334	530336.208738	49.019277
3504.296620	530327.733486	49.024282
3504.269949	530306.615820	49.029287
3504.198204	530309.002289	49.034292
3503.870399	530321.484937	49.039297
3503.957681	530328.949919	49.044301
3504.372284	530319.283632	49.049306
3504.015757	530320.401296	49.054311
3504.019733	530319.087019	49.059316
3504.183783	530286.569661	49.064321
3504.406613	530293.053143	49.069325
3503.947306	530308.588460	49.074330
3504.100274	530301.692198	49.079335
3503.903387	530272.263729	49.084340
3503.649329	530272.051387	49.089345
3503.549689	530270.652419	49.094349
3503.822892	530268.941869	49.099354
3503.818223	530268.740643	49.104359
3503.430891	530261.020190	49.109364
3503.309758	530268.214952	49.114369
3503.775844	530276.428593	49.119373
3503.773445	530291.083214	49.124378
3504.198824	530280.859356	49.129383
3503.886403	530300.312910	49.134388
3503.254981	530270.043549	49.139393
3504.065951	530252.179027	49.144397
3503.906885	530286.565651	49.149402
3504.096510	530284.059811	49.154407
3503.698513	530281.141527	49.159412
3503.688615	530260.475930	49.164417
3504.273117	530240.676463	49.169421
3504.262096	530287.318825	49.174426
3504.185517	530314.062125	49.179431
3504.027236	530307.518244	49.184436
3504.050871	530300.389765	49.189441
3504.013158	530278.970620	49.194445
3503.598285	530280.804947	49.199450
3503.593366	530280.351104	49.204455
3504.456748	530249.946524	49.209460
3504.382766	530238.689868	49.214465
3504.326195	530241.427670	49.219469
3504.274406	530241.334954	49.224474
3504.135446	530254.090998	49.229479
3504.076972	530260.972671	49.234484
3503.771605	530250.813752	49.239489
3504.207473	530205.772004	49.244493
3503.746891	530233.334103	49.249498
3503.795217	530199.521037	49.254503
3504.060626	530176.184177	49.259508
3503.994710	530239.763451	49.264513
3503.991560	530215.812185	49.269517
3503.359354	530206.917649	49.274522
3503.251602	530205.823147	49.279527
3503.782318	530208.215479	49.284532
3503.762375	530228.633527	49.289537
3504.213721	530238.365462	49.294541
3504.088523	530225.853605	49.299546
3504.015014	530227.128673	49.304551
3504.337179	530214.950356	49.309556
3503.858903	530208.760196	49.314561
3503.742361	530202.058079	49.319565
3504.107057	530179.059253	49.324570
3503.875652	530177.327380	49.329575
3504.106750	530175.067626	49.334580
3503.855887	530177.583487	49.339585
3504.091552	530190.482501	49.344589
3504.207007	530169.140063	49.349594
3504.054073	530161.433047	49.354599
3503.979226	530189.338514	49.359604
3503.926469	530191.974657	49.364609
3504.117109	530170.266617	49.369613
3504.148502	530167.785766	49.374618
3503.906410	530159.536991	49.379623
3504.550307	530140.587052	49.384628
3504.563855	530126.031917	49.389633
3504.254751	530121.533067	49.394637
3504.068939	530152.285918	49.399642
3503.921244	530154.937073	49.404647
3504.121659	530155.006624	49.409652
3503.945930	530159.127628	49.414657
3504.272152	530135.124185	49.419661
3503.643802	530134.263550	49.424666
3503.868516	530116.440998	49.429671
3504.499292	530092.136697	49.434676
3504.386508	530093.620110	49.439681
3504.268500	530107.434131	49.444685
3504.116734	530097.958283	49.449690
3503.762188	530080.934686	49.454695
3504.626582	530054.673192	49.459700
3504.029206	530059.871501	49.464705
3504.307353	530082.213376	49.469709
3504.380982	530083.869456	49.474714
3503.787221	530050.157548	49.479719
3504.232402	530042.103285	49.484724
3504.024368	530076.245446	49.489729
3504.663508	530029.806707	49.494733
3504.280044	530055.335643	49.499738
3503.662883	530019.858747	49.504743
3504.547184	529989.298764	49.509748
3504.083269	529998.569112	49.514753
3504.330556	529977.458241	49.519757
3503.924092	529981.059903	49.524762
3504.039749	529976.443348	49.529767
3504.372560	529940.563475	49.534772
3504.011674	529956.487841	49.539777
3503.456245	529974.464230	49.544781
3503.831422	529984.157829	49.549786
3503.899783	529991.272236	49.554791
3504.250997	529996.270115	49.559796
3503.878254	530009.972883	49.564801
3503.370011	530009.446984	49.569805
3503.659882	530012.130072	49.574810
3503.788040	530016.961068	49.579815
3503.894922	530009.869834	49.584820
3503.928442	530012.997694	49.589825
3504.142900	529991.790966	49.594829
3504.116497	530008.117208	49.599834
3504.089133	530000.036542	49.604839
3503.952185	529977.571495	49.609844
3503.701641	529977.712319	49.614849
3504.164299	530003.107615	49.619853
3504.038142	530002.773990	49.624858
3503.948000	529976.258966	49.629863
3504.435618	529972.038415	49.634868
3504.136465	529960.665551	49.639873
3504.535735	529922.501178	49.644877
3504.436036	529912.360068	49.649882
3503.223288	529923.871173	49.654887
3504.182224	529908.913763	49.659892
3504.323320	529899.189381	49.664897
3504.178187	529884.709635	49.669901
3504.394645	529881.289904	49.674906
3504.141098	529906.798547	49.679911
3504.370169	529936.627195	49.684916
3504.146795	529931.558885	49.689921
3504.207337	529908.254008	49.694925
3504.041251	529893.979712	49.699930
3503.993648	529868.620033	49.704935
3503.837755	529855.304211	49.709940
3503.813268	529871.882954	49.714945
3503.612001	529861.707331	49.719949
3503.583916	529859.134766	49.724954
3503.558770	529887.437173	49.729959
3503.706859	529878.469661	49.734964
3503.807110	529873.855512	49.739969
3503.788258	529845.307696	49.744973
3503.606225	529839.424299	49.749978
3503.594478	529857.517026	49.754983
3503.967368	529873.830833	49.759988
3503.889228	529895.370228	49.764993
3504.060820	529885.489420	49.769997
3504.258527	529858.120184	49.775002
3504.005786	529836.987086	49.780007
3504.035678	529875.892686	49.785012
3503.718639	529862.602339	49.790017
3504.350675	529863.513265	49.795021
3503.693535	529873.471149	49.800026
3504.006985	529863.770038	49.805031
3504.140278	529882.900999	49.810036
3503.823718	529853.743326	49.815041
3503.943499	529876.312652	49.820045
3504.496621	529875.669538	49.825050
3503.964960	529854.479481	49.830055
3503.662992	529844.218696	49.835060
3504.240456	529814.262730	49.840065
3504.163603	529830.698194	49.845069
3504.358683	529855.883352	49.850074
3504.048141	529840.317988	49.855079
3504.327400	529827.539762	49.860084
3503.882080	529810.530219	49.865089
3503.851319	529801.287734	49.870093
3503.832117	529811.751228	49.875098
3503.695591	529802.525459	49.880103
3504.040389	529792.010824	49.885108
3503.955483	529797.936752	49.890113
3504.107799	529793.920745	49.895117
3503.883385	529817.555211	49.900122
3504.002494	529808.339576	49.905127
3504.088938	529783.009107	49.910132
3504.139952	529779.817633	49.915137
3503.960666	529814.562211	49.920141
3503.847786	529792.851089	49.925146
3504.379080	529781.751112	49.930151
3504.380820	529786.349494	49.935156
3504.206389	529753.177073	49.940161
3504.320691	529735.472608	49.945165
3504.272136	529772.116873	49.950170
3504.104039	529733.132119	49.955175
3504.303983	529738.962516	49.960180
3503.621015	529705.415568	49.965185
3503.847777	529707.199086	49.970189
3503.925526	529721.538370	49.975194
3503.915610	529702.792305	49.980199
3504.414522	529675.779415	49.985204
3503.936994	529731.542597	49.990209
3504.162559	529731.355511	49.995213
3503.912598	529732.506906	50.000218
3503.679590	529717.434497	50.005223
3503.986586	529716.880810	50.010228
3503.678892	529741.791879	50.015233
3504.046657	529711.616195	50.020237
3504.523334	529684.859500	50.025242
3504.177549	529707.553181	50.030247
3504.311919	529655.028073	50.035252
3504.276931	529679.946673	50.040257
3504.262359	529651.852631	50.045261
3504.285218	529676.812627	50.050266
3503.537663	529657.222955	50.055271
3504.160072	529636.759811	50.060276
3504.423081	529674.466796	50.065281
3504.030060	529639.408419	50.070285
3504.105740	529619.031658	50.075290
3504.044328	529634.151017	50.080295
3504.211506	529643.574498	50.085300
3503.807988	529632.622158	50.090305
3503.949454	529636.844767	50.095309
3504.330314	529661.899807	50.100314
3504.278605	529646.546011	50.105319
3504.315461	529625.063661	50.110324
3503.958333	529590.504837	50.115329
3504.420270	529562.739595	50.120333
3504.365453	529597.515511	50.125338
3504.000308	529588.982684	50.130343
3504.433938	529532.821993	50.135348
3504.242771	529514.912891	50.140353
3504.477732	529532.663795	50.145357
3504.342545	529573.769178	50.150362
3503.931489	529553.418725	50.155367
3504.253611	529531.840630	50.160372
3503.905444	529517.139967	50.165377
3503.550939	529513.305056	50.170381
3503.798045	529506.343036	50.175386
3504.034059	529499.787037	50.180391
3504.372881	529465.522219	50.185396
3503.803742	529487.240837	50.190401
3503.999574	529527.687617	50.195405
3503.887700	529537.256332	50.200410
3504.191987	529530.083151	50.205415
3504.013084	529507.472465	50.210420
3503.991616	529518.846119	50.215425
3503.565460	529511.283034	50.220429
3503.385651	529515.910187	50.225434
3504.237722	529501.373555	50.230439
3504.502663	529500.826507	50.235444
3503.901221	529510.927416	50.240449
3503.704064	529468.661906	50.245453
3504.330930	529455.323104	50.250458
3503.809034	529488.101186	50.255463
3504.338947	529436.826722	50.260468
3504.013736	529455.474789	50.265473
3503.971318	529501.113754	50.270477
3503.663771	529471.549681	50.275482
3503.362587	529461.995998	50.280487
3504.461855	529439.435877	50.285492
3504.138401	529448.482211	50.290497
3503.921389	529482.980808	50.295501
3504.535669	529426.892259	50.300506
3504.282748	529460.284832	50.305511
3503.980579	529432.033717	50.310516
3504.072409	529456.578887	50.315521
3504.339633	529416.614941	50.320525
3504.584060	529427.592900	50.325530
3503.890874	529422.143870	50.330535
3504.490182	529382.430558	50.335540
3504.160447	529412.348512	50.340545
3504.196735	529374.694993	50.345549
3504.536148	529407.033913	50.350554
3504.013276	529393.977837	50.355559
3503.690426	529360.474310	50.360564
3504.349028	529340.055597	50.365569
3504.241524	529323.446948	50.370573
3504.147922	529369.043849	50.375578
3503.752901	529356.573947	50.380583
3504.382743	529311.600067	50.385588
3503.975741	529361.440877	50.390593
3503.961060	529363.161524	50.395597
3504.425533	529330.291515	50.400602
3504.208314	529334.823564	50.405607
3504.346600	529299.074050	50.410612
3503.999975	529330.611930	50.415617
3504.560866	529281.606114	50.420621
3504.436824	529320.335270	50.425626
3504.067631	529293.964274	50.430631
3503.828794	529259.335496	50.435636
3504.253511	529242.541578	50.440641
3503.701231	529280.984768	50.445645
3503.918139	529256.694064	50.450650
3503.879204	529262.360253	50.455655
3503.378271	529284.826385	50.460660
3503.563399	529262.006212	50.465665
3503.873489	529283.889357	50.470669
3504.100591	529241.000308	50.475674
3503.751661	529279.815641	50.480679
3503.853535	529284.095136	50.485684
3503.900436	529242.346329	50.490689
3504.181843	529267.316643	50.495693
3504.158571	529283.946345	50.500698
3504.026405	529261.176317	50.505703
3504.076136	529239.741944	50.510708
3503.909159	529274.132018	50.515713
3503.951985	529263.159414	50.520717
3503.822707	529214.565675	50.525722
3503.939520	529220.813680	50.530727
3503.852864	529247.055030	50.535732
3503.385216	529207.105629	50.540737
3503.743477	529169.249131	50.545741
3503.713890	529151.920499	50.550746
3503.597721	529083.464047	50.555751
3503.888388	529032.579833	50.560756
3503.434134	528953.412228	50.565761
3503.508257	528867.894278	50.570765
3503.581443	528805.875286	50.575770
3503.278470	528694.945823	50.580775
3503.175126	528556.593100	50.585780
3503.339754	528420.369922	50.590785
3503.049930	528322.322773	50.595789
3503.043650	528156.761995	50.600794
3502.696512	527992.264138	50.605799
3502.863473	527858.815408	50.610804
3502.148440	527670.113610	50.615809
3502.272962	527486.785774	50.620813
3502.246297	527343.912314	50.625818
3501.432548	527147.082878	50.630823
3501.398918	526925.817041	50.635828
3501.256718	526700.622972	50.640833
3500.209555	526492.854600	50.645837
3500.918834	526262.516005	50.650842
3500.707820	526023.625845	50.655847
3500.126640	525806.879040	50.660852
3499.503203	525583.514436	50.665857
3499.187513	525322.187850	50.670861
3499.108556	525052.277016	50.675866
3498.861840	524778.546473	50.680871
3498.521952	524557.043669	50.685876
3497.716815	524262.060745	50.690881
3497.846247	523957.117779	50.695885
3497.285791	523711.525257	50.700890
3496.950047	523393.552208	50.705895
3496.629480	523077.188261	50.710900
3496.263721	522785.142255	50.715905
3495.314421	522500.463278	50.720909
3495.464694	522209.993738	50.725914
3494.698693	521882.251139	50.730919
3494.329677	521551.001220	50.735924
3493.954886	521209.582979	50.740929
3493.267059	520928.677820	50.745933
3492.826402	520596.863755	50.750938
3492.173477	520243.536785	50.755943
3492.548492	519863.594811	50.760948
3491.694929	519564.489479	50.765953
3491.054024	519232.072765	50.770957
3490.638194	518846.265575	50.775962
3490.173005	518476.588463	50.780967
3489.708624	518153.628999	50.785972
3488.874352	517779.291735	50.790977
3488.201628	517406.184790	50.795981
3487.529709	517036.912872	50.800986
3487.736200	516648.023039	50.805991
3487.210461	516301.368781	50.810996
3486.598776	515895.091842	50.816001
3485.874889	515556.646797	50.821005
3485.358228	515130.661814	50.826010
3484.593958	514773.948572	50.831015
3484.575417	514348.219101	50.836020
3483.841441	513981.570470	50.841025
3483.467879	513548.188497	50.846029
3482.828575	513192.636075	50.851034
3481.981870	512771.651548	50.856039
3482.035315	512341.560461	50.861044
3480.942785	511966.982807	50.866049
3480.028231	511535.304367	50.871053
3479.670155	511101.199896	50.876058
3478.761479	510723.075145	50.881063
3478.313560	510295.187191	50.886068
3478.105028	509862.191330	50.891073
3477.300171	509487.615127	50.896077
3476.765854	509027.935518	50.901082
3475.879859	508655.226126	50.906087
3475.385196	508205.486086	50.911092
3475.257864	507775.612784	50.916097
3474.030764	507382.436844	50.921101
3473.944482	506908.664225	50.926106
3472.797527	506528.410602	50.931111
3472.197938	506062.995161	50.936116
3471.333073	505677.263672	50.941121
3470.714182	505234.804480	50.946125
3470.221529	504777.030322	50.951130
3469.340898	504384.946821	50.956135
3469.201212	503924.007488	50.961140
3468.472695	503536.689161	50.966145
3467.539219	503060.112308	50.971149
3467.065001	502659.575020	50.976154
3465.959593	502215.244308	50.981159
3465.731581	501769.599614	50.986164
3464.726840	501368.256622	50.991169
3464.401122	500897.245675	50.996173
3463.510167	500506.394290	51.001178
3462.734643	500041.557090	51.006183
3462.066280	499630.655630	51.011188
3461.736468	499178.482790	51.016193
3460.647946	498764.793019	51.021197
3460.222609	498333.775746	51.026202
3459.335249	497886.468298	51.031207
3458.781326	497468.057229	51.036212
3457.799734	497033.654203	51.041217
3457.246298	496582.363333	51.046221
3456.515243	496188.963077	51.051226
3455.659237	495742.762612	51.056231
3455.754783	495298.780746	51.061236
3454.529312	494892.822580	51.066241
3453.732095	494428.199783	51.071245
3453.377094	494021.831642	51.076250
3452.853465	493574.614581	51.081255
3452.187443	493140.120238	51.086260
3451.328511	492728.688598	51.091265
3450.915547	492272.712152	51.096269
3450.032612	491839.032001	51.101274
3449.055983	491412.396403	51.106279
3448.111469	490972.425757	51.111284
3447.923353	490523.208486	51.116289
3447.070283	490135.118439	51.121293
3446.286885	489683.088178	51.126298
3445.526527	489260.472241	51.131303
3444.758106	488832.428252	51.136308
3444.377515	488409.429361	51.141313
3443.753460	487957.484660	51.146317
3442.918082	487550.849586	51.151322
3442.132048	487123.681710	51.156327
3441.251566	486700.926522	51.161332
3441.004625	486255.771496	51.166337
3439.726741	485835.593032	51.171341
3439.368483	485416.627885	51.176346
3438.753427	484985.788358	51.181351
3437.995197	484555.012513	51.186356
3437.182451	484140.651313	51.191361
3436.278025	483718.949094	51.196365
3435.753718	483304.473774	51.201370
3434.970178	482883.088989	51.206375
3434.469604	482444.017254	51.211380
3433.426007	482035.272079	51.216385
3433.157994	481608.863246	51.221389
3432.063119	481207.861748	51.226394
3431.527807	480788.672946	51.231399
3431.256138	480353.318818	51.236404
3430.272285	479937.324702	51.241409
3429.424446	479516.992758	51.246413
3428.829383	479105.784753	51.251418
3427.843706	478675.574479	51.256423
3427.292795	478288.263339	51.261428
3427.025041	477838.814943	51.266433
3425.751151	477444.404933	51.271437
3425.465692	477035.031262	51.276442
3424.537596	476607.149525	51.281447
3424.123909	476195.396845	51.286452
3423.176726	475794.567087	51.291457
3422.531982	475363.522274	51.296461
3422.204354	474956.292664	51.301466
3420.820282	474554.949859	51.306471
3420.296437	474109.057827	51.311476
3419.716637	473734.083098	51.316481
3419.154353	473306.732871	51.321485
3418.284477	472888.445897	51.326490
3417.496664	472498.374579	51.331495
3417.213924	472070.447457	51.336500
3416.074655	471663.888949	51.341505
3415.285098	471250.017320	51.346509
3415.078269	470860.887844	51.351514
3414.075546	470434.054647	51.356519
3413.474934	470027.023951	51.361524
3412.729938	469627.613436	51.366529
3411.684147	469230.777981	51.371533
3411.016478	468830.832976	51.376538
3410.539717	468425.272612	51.381543
3409.845086	468008.837077	51.386548
3409.012879	467628.163445	51.391553
3408.309569	467229.309160	51.396557
3408.078564	466820.129498	51.401562
3406.906657	466428.534852	51.406567
3406.030623	466023.549284	51.411572
3405.946277	465624.110555	51.416577
3404.781097	465216.061929	51.421581
3404.230271	464837.068697	51.426586
3403.323299	464445.598586	51.431591
3402.769181	464036.315148	51.436596
3402.156706	463646.761821	51.441601
3401.215577	463245.943454	51.446605
3400.773717	462856.298161	51.451610
3399.665386	462463.048723	51.456615
3399.364334	462085.692058	51.461620
3398.908997	461693.796330	51.466625
3397.838190	461305.490661	51.471629
3397.373203	460913.734602	51.476634
3396.436982	460521.944581	51.481639
3396.097881	460119.705339	51.486644
3395.298801	459733.154908	51.491649
3394.265971	459342.830167	51.496653
3393.887443	458949.300710	51.501658
3392.959960	458559.452741	51.506663
3392.337916	458168.129208	51.511668
3391.572066	457778.546334	51.516673
3390.860502	457397.470837	51.521677
3390.156332	457008.980832	51.526682
3389.352261	456636.379164	51.531687
3388.742773	456246.237504	51.536692
3388.102038	455866.900412	51.541697
3387.137514	455492.935304	51.546701
3386.980062	455101.636890	51.551706
3386.056335	454732.675599	51.556711
3385.566313	454332.334562	51.561716
3384.771766	453951.670452	51.566721
3384.296335	453579.017084	51.571725
3383.696969	453185.573710	51.576730
3382.407584	452807.353515	51.581735
3382.172103	452419.623918	51.586740
3381.442891	452035.162631	51.591745
3380.669012	451664.199793	51.596749
3379.780011	451283.049544	51.601754
3379.234492	450912.038506	51.606759
3378.645920	450531.285071	51.611764
3377.822308	450148.126692	51.616769
3377.091141	449764.795139	51.621773
3376.633960	449387.250053	51.626778
3375.829185	449021.578441	51.631783
3374.823411	448647.305354	51.636788
3374.529169	448262.966587	51.641793
3373.469691	447902.037637	51.646797
3372.716443	447518.825078	51.651802
3372.370481	447146.707669	51.656807
3372.020780	446763.875848	51.661812
3370.961481	446402.720953	51.666817
3370.102764	446028.129311	51.671821
3369.533338	445651.861825	51.676826
3368.983478	445273.047442	51.681831
3368.401845	444903.317814	51.686836
3367.606662	444536.458757	51.691841
3366.623201	444169.471588	51.696845
3366.237153	443785.684135	51.701850
3365.621938	443418.982645	51.706855
3365.019113	443051.156872	51.711860
3364.225946	442683.812481	51.716865
3363.339209	442308.304379	51.721869
3362.697416	441930.873472	51.726874
3361.765836	441566.630752	51.731879
3361.228292	441196.329918	51.736884
3360.977227	440832.984011	51.741889
3359.771852	440464.656106	51.746893
3359.411880	440098.118216	51.751898
3358.228302	439733.964333	51.756903
3357.499415	439366.966244	51.761908
3356.994951	439004.547357	51.766913
3356.098464	438652.110950	51.771917
3355.559550	438286.463081	51.776922
3354.662620	437930.310190	51.781927
3354.302913	437560.891580	51.786932
3353.729338	437203.052474	51.791937
3352.772017	436852.123562	51.796941
3352.255790	436488.045301	51.801946
3351.789481	436131.494184	51.806951
3351.067652	435771.525609	51.811956
3350.421377	435404.811926	51.816961
3349.798745	435045.122038	51.821965
3349.253250	434687.623774	51.826970
3348.409188	434335.245708	51.831975
3347.804681	433961.344708	51.836980
3347.295084	433597.351013	51.841985
3346.450625	433230.485148	51.846989
3345.752296	432862.067472	51.851994
3344.958408	432513.719144	51.856999
3343.944360	432149.353137	51.862004
3343.242074	431783.180640	51.867009
3342.767155	431422.121782	51.872013
3342.182191	431081.034350	51.877018
3341.238696	430727.607140	51.882023
3340.669746	430361.012719	51.887028
3340.085441	430003.202002	51.892033
3339.646340	429653.413529	51.897037
3338.943049	429300.157705	51.902042
3338.290244	428933.404324	51.907047
3337.418096	428578.387909	51.912052
3337.108063	428215.100388	51.917057
3336.035266	427861.147364	51.922061
3335.393042	427500.442264	51.927066
3334.710673	427153.960925	51.932071
3334.052577	426794.645667	51.937076
3333.503369	426434.749644	51.942081
3332.548082	426087.358012	51.947085
3331.908788	425718.475822	51.952090
3331.006803	425377.898785	51.957095
3330.268972	425029.214667	51.962100
3330.212752	424663.096019	51.967105
3329.564188	424317.106396	51.972109
3329.183736	423963.577032	51.977114
3328.095092	423611.729911	51.982119
3327.592441	423250.006409	51.987124
3326.741990	422878.020394	51.992129
3326.028194	422535.803399	51.997133
3325.400320	422173.628383	52.002138
3324.926048	421815.539456	52.007143
3324.096665	421468.983867	52.012148
3323.306789	421118.632752	52.017153
3322.388732	420753.411458	52.022157
3322.108572	420384.020026	52.027162
3321.340674	420051.408909	52.032167
3320.207819	419691.110645	52.037172
3319.567585	419345.210229	52.042177
3319.260715	419008.119010	52.047181
3318.744606	418653.019527	52.052186
3317.825638	418302.476010	52.057191
3317.494522	417939.157952	52.062196
3316.795308	417588.189838	52.067201
3316.064951	417244.742521	52.072205
3315.118704	416882.041867	52.077210
3314.144639	416539.463078	52.082215
3313.921943	416180.043662	52.087220
3313.403701	415830.118011	52.092225
3312.400611	415485.574989	52.097229
3311.643050	415131.130822	52.102234
3310.794349	414780.025228	52.107239
3310.489638	414442.245048	52.112244
3309.670198	414091.533109	52.117249
3308.890815	413738.701701	52.122253
3308.482105	413380.928858	52.127258
3307.675955	413039.705396	52.132263
3306.846848	412693.602927	52.137268
3306.468122	412340.793131	52.142273
3305.591632	412000.381981	52.147277
3305.056000	411651.070080	52.152282
3304.356192	411308.082024	52.157287
3303.798391	410959.629549	52.162292
3303.012175	410617.231735	52.167297
3302.052809	410264.540148	52.172301
3301.690978	409915.765095	52.177306
3300.937555	409582.270088	52.182311
3300.302127	409240.646065	52.187316
3299.483876	408880.088922	52.192321
3298.742646	408535.703707	52.197325
3298.288324	408196.123270	52.202330
3297.438009	407847.655976	52.207335
3296.802716	407498.312063	52.212340
3296.146432	407163.148851	52.217345
3295.216139	406830.109362	52.222349
3294.929921	406479.529670	52.227354
3294.365374	406130.692881	52.232359
3293.698579	405784.409933	52.237364
3292.945795	405449.421443	52.242369
3292.129994	405112.329796	52.247373
3291.399942	404756.768585	52.252378
3290.777393	404425.332325	52.257383
3290.248135	404075.958810	52.262388
3289.296499	403736.942270	52.267393
3288.576585	403395.648720	52.272397
3288.081255	403055.332715	52.277402
3287.171277	402707.376963	52.282407
3286.925210	402364.014848	52.287412
3286.299026	402034.359024	52.292417
3285.325136	401681.903172	52.297421
3284.702911	401338.081243	52.302426
3283.984999	401001.998330	52.307431
3283.341675	400658.680932	52.312436
3282.940753	400311.991556	52.317441
3281.998566	399982.695334	52.322445
3281.566832	399631.707596	52.327450
3280.987639	399281.908791	52.332455
3280.393304	398943.726114	52.337460
3279.577616	398606.007147	52.342465
3278.774307	398254.580527	52.347469
3278.233255	397913.124941	52.352474
3277.748508	397579.537817	52.357479
3277.048548	397222.008074	52.362484
3276.400994	396882.033300	52.367489
3275.321761	396538.259076	52.372493
3274.733779	396193.030800	52.377498
3274.261869	395840.026489	52.382503
3273.510077	395503.155980	52.387508
3272.827506	395163.398279	52.392513
3272.119085	394828.192217	52.397517
3271.480075	394486.031014	52.402522
3270.757292	394143.015207	52.407527
3270.233916	393800.040718	52.412532
3269.715145	393455.129774	52.417537
3268.442284	393124.089840	52.422541
3267.882208	392776.941240	52.427546
3267.308901	392433.478036	52.432551
3266.850050	392087.196467	52.437556
3266.241932	391759.979507	52.442561
3265.437411	391413.720533	52.447565
3264.982479	391060.257888	52.452570
3264.046684	390733.515477	52.457575
3263.463999	390379.125427	52.462580
3263.124688	390041.857051	52.467585
3262.241970	389707.112512	52.472589
3261.679563	389355.379012	52.477594
3260.841152	389020.875332	52.482599
3259.964323	388671.575137	52.487604
3259.587777	388334.728887	52.492609
3258.957906	387993.342323	52.497613
3258.454317	387633.725135	52.502618
3257.475160	387300.397569	52.507623
3256.494126	386956.081557	52.512628
3256.320751	386609.778169	52.517633
3255.253716	386275.565126	52.522637
3254.890353	385928.853069	52.527642
3254.137153	385583.038638	52.532647
3253.543326	385245.638885	52.537652
3253.101876	384903.329168	52.542657
3252.459747	384566.744712	52.547661
3251.828984	384211.056198	52.552666
3251.170083	383862.133675	52.557671
3250.229419	383530.393800	52.562676
3249.572355	383182.481995	52.567681
3249.060006	382836.858484	52.572685
3248.034655	382482.411460	52.577690
3247.390941	382147.026501	52.582695
3246.716369	381817.493157	52.587700
3246.125731	381479.118265	52.592705
3245.358148	381132.553274	52.597709
3244.771191	380792.391417	52.602714
3243.816079	380449.283569	52.607719
3243.208146	380122.039760	52.612724
3242.733886	379772.262375	52.617729
3242.186450	379432.667407	52.622733
3241.566169	379100.864177	52.627738
3241.057803	378754.949277	52.632743
3240.348965	378401.890233	52.637748
3239.613558	378062.033430	52.642753
3238.704624	377726.448988	52.647757
3238.282722	377377.939404	52.652762
3237.568171	377041.122973	52.657767
3236.474540	376696.554631	52.662772
3236.120485	376354.766172	52.667777
3235.579352	376030.861251	52.672781
3234.634647	375675.907787	52.677786
3234.060346	375339.970779	52.682791
3233.565908	375008.266479	52.687796
3232.964147	374666.121495	52.692801
3231.924001	374314.223895	52.697805
3231.385884	373982.645446	52.702810
3230.916204	373637.367586	52.707815
3230.119080	373309.335258	52.712820
3229.556088	372951.906764	52.717825
3228.808762	372620.808491	52.722829
3228.076695	372275.408274	52.727834
3227.469952	371938.355032	52.732839
3226.909691	371595.695008	52.737844
3226.169563	371256.240674	52.742849
3225.162790	370916.189816	52.747853
3224.845582	370563.968439	52.752858
3224.015171	370232.966493	52.757863
3223.304541	369899.195459	52.762868
3222.728618	369561.431751	52.767873
3222.061679	369220.626876	52.772877
3221.597422	368886.096742	52.777882
3220.748312	368540.685052	52.782887
3219.917433	368207.301725	52.787892
3219.694580	367861.912860	52.792897
3218.619060	367529.860662	52.797901
3218.094766	367185.023055	52.802906
3217.557913	366854.814235	52.807911
3216.687945	366512.748475	52.812916
3216.231594	366173.209863	52.817921
3215.822949	365830.607976	52.822925
3214.635232	365486.778239	52.827930
3213.695451	365166.849017	52.832935
3213.256297	364816.382274	52.837940
3212.780280	364475.841796	52.842945
3211.938045	364152.226140	52.847949
3211.356850	363818.796335	52.852954
3210.896091	363477.177419	52.857959
3210.092360	363138.663602	52.862964
3209.268718	362795.723086	52.867969
3208.786172	362460.079704	52.872973
3208.471800	362109.343789	52.877978
3207.462399	361777.341214	52.882983
3207.123393	361432.482058	52.887988
3206.505469	361105.680091	52.892993
3205.436367	360759.099471	52.897997
3204.872574	360414.472100	52.903002
3204.418814	360077.407844	52.908007
3203.443336	359736.225109	52.913012
3202.732138	359389.730726	52.918017
3201.790075	359058.971070	52.923021
3201.287325	358721.294455	52.928026
3200.394102	358387.647044	52.933031
3199.966220	358051.048222	52.938036
3199.764731	357713.673326	52.943041
3198.654064	357384.888587	52.948045
3198.138874	357028.345710	52.953050
3197.633973	356693.963882	52.958055
3196.867243	356354.302590	52.963060
3196.237809	356018.001930	52.968065
3195.855870	355681.659894	52.973069
3195.234777	355335.250355	52.978074
3194.461579	354993.468779	52.983079
3193.638502	354650.522171	52.988084
3193.056909	354297.762604	52.993089
3191.873795	353974.438900	52.998093
3191.515972	353631.157472	53.003098
3190.891792	353294.507399	53.008103
3190.108657	352948.336631	53.013108
3189.813876	352612.088193	53.018113
3189.117662	352271.371004	53.023117
3188.388043	351916.481091	53.028122
3187.236567	351582.423168	53.033127
3186.672599	351232.592630	53.038132
3186.548927	350898.164272	53.043137
3185.538668	350552.726588	53.048141
3184.847546	350225.102923	53.053146
3184.233855	349871.377487	53.058151
3183.532631	349539.577323	53.063156
3183.200590	349188.119035	53.068161
3181.889410	348862.137924	53.073165
3181.700512	348507.674846	53.078170
3181.254988	348180.356580	53.083175
3179.976017	347828.886854	53.088180
3179.750620	347477.528247	53.093185
3179.056493	347153.272210	53.098189
3178.430849	346806.401530	53.103194
3177.798711	346451.766671	53.108199
3177.039437	346123.086337	53.113204
3176.551882	345772.064218	53.118209
3175.273871	345441.247675	53.123213
3175.020151	345096.980534	53.128218
3174.477347	344747.920937	53.133223
3173.505666	344418.450134	53.138228
3172.987078	344083.662330	53.143233
3172.039126	343737.129922	53.148237
3171.363762	343394.599600	53.153242
3170.547113	343072.427664	53.158247
3169.978812	342731.225728	53.163252
3169.443921	342390.983872	53.168257
3168.789008	342052.719128	53.173261
3168.206060	341707.313784	53.178266
3167.733309	341375.456590	53.183271
3166.606661	341035.606348	53.188276
3166.123012	340690.714212	53.193281
3165.512497	340370.124708	53.198285
3164.851274	340017.569455	53.203290
3164.088778	339693.309521	53.208295
3163.385683	339354.528739	53.213300
3162.903385	339010.136388	53.218305
3161.875509	338677.945605	53.223309
3161.711671	338354.806111	53.228314
3160.939578	338004.879370	53.233319
3160.227281	337676.935686	53.238324
3159.690641	337326.866263	53.243329
3158.861054	336993.642777	53.248333
3158.264627	336661.220815	53.253338
3157.373622	336319.195618	53.258343
3156.937800	335983.053635	53.263348
3156.064819	335637.636346	53.268353
3155.189972	335313.296294	53.273357
3154.588259	334975.088088	53.278362
3154.211003	334628.212585	53.283367
3153.493695	334299.769628	53.288372
3152.719403	333959.572617	53.293377
3151.816333	333622.703867	53.298381
3151.418980	333298.126131	53.303386
3150.606918	332968.648174	53.308391
3149.983822	332633.334303	53.313396
3149.349819	332307.007421	53.318401
3148.410973	331970.314748	53.323405
3147.829813	331635.626077	53.328410
3147.280721	331302.661999	53.333415
3146.278342	330976.743870	53.338420
3146.120431	330635.899009	53.343425
3145.126264	330312.649862	53.348429
3144.820168	329980.023293	53.353434
3143.991844	329658.298105	53.358439
3143.448616	329316.489850	53.363444
3143.165289	328975.784624	53.368449
3142.045298	328652.701067	53.373453
3141.513062	328310.606539	53.378458
3140.892442	327968.499031	53.383463
3140.299994	327637.791657	53.388468
3139.908355	327297.732719	53.393473
3139.001399	326965.060943	53.398477
3137.850702	326625.068306	53.403482
3137.483173	326290.627998	53.408487
3136.570001	325959.862576	53.413492
3136.168015	325623.566351	53.418497
3135.463390	325298.137450	53.423501
3134.732301	324951.197030	53.428506
3134.284285	324618.010215	53.433511
3133.650694	324288.721517	53.438516
3132.870106	323939.467776	53.443521
3132.185739	323617.339084	53.448525
3131.685806	323264.753666	53.453530
3130.591499	322935.023400	53.458535
3129.989677	322606.054188	53.463540
3129.935445	322249.040191	53.468545
3128.973051	321937.643143	53.473549
3128.323900	321592.382102	53.478554
3127.827027	321257.204024	53.483559
3126.788341	320928.144929	53.488564
3126.238218	320581.871316	53.493569
3125.212774	320253.520622	53.498573
3124.752322	319914.741655	53.503578
3124.211205	319577.476495	53.508583
3123.615143	319251.167687	53.513588
3123.188521	318907.669147	53.518593
3122.364484	318574.722872	53.523597
3121.948232	318226.840651	53.528602
3121.197004	317896.757794	53.533607
3120.224669	317562.838432	53.538612
3119.862042	317217.337624	53.543617
3119.002721	316892.004606	53.548621
3118.199143	316538.804949	53.553626
3117.553110	316219.750869	53.558631
3116.903845	315878.568616	53.563636
3116.394683	315536.344514	53.568641
3115.621340	315203.378880	53.573645
3114.921329	314864.925892	53.578650
3113.984044	314528.291813	53.583655
3113.469337	314198.897903	53.588660
3113.227585	313853.239295	53.593665
3112.210978	313529.321079	53.598669
3111.827203	313188.266323	53.603674
3111.159822	312848.197550	53.608679
3110.603991	312506.964189	53.613684
3110.262675	312156.910666	53.618689
3109.081874	311829.117404	53.623693
3108.574949	311466.610416	53.628698
3107.881548	311139.603837	53.633703
3107.325980	310789.834661	53.638708
3106.663641	310449.095818	53.643713
3105.695499	310110.314233	53.648717
3104.926576	309773.308160	53.653722
3104.399549	309426.840867	53.658727
3103.562961	309093.688800	53.663732
3103.378274	308753.404334	53.668737
3102.576143	308415.202912	53.673741
3101.751491	308077.819024	53.678746
3101.302904	307727.565729	53.683751
3100.653353	307390.152310	53.688756
3099.825736	307048.488010	53.693761
3098.906279	306703.934293	53.698765
3098.796479	306365.235946	53.703770
3097.934161	306024.007401	53.708775
3097.112685	305697.592515	53.713780
3096.506847	305354.335386	53.718785
3095.441072	305017.822207	53.723789
3094.433980	304682.292098	53.728794
3094.168423	304343.282359	53.733799
3093.618617	304015.725525	53.738804
3093.015118	303675.876384	53.743809
3092.535758	303347.186396	53.748813
3091.715734	303012.361329	53.753818
3091.342117	302668.653590	53.758823
3090.324096	302342.211263	53.763828
3090.004045	301985.862282	53.768833
3089.258233	301651.761015	53.773837
3088.480917	301323.292092	53.778842
3087.768862	300976.399952	53.783847
3087.032712	300624.544922	53.788852
3086.807093	300290.434915	53.793857
3085.707281	299958.525368	53.798861
3084.961476	299614.411571	53.803866
3084.703302	299279.362454	53.808871
3083.681622	298945.375781	53.813876
3083.347787	298598.648111	53.818881
3082.557278	298278.935928	53.823885
3081.888263	297932.896690	53.828890
3081.572350	297587.310263	53.833895
3080.455298	297255.220129	53.838900
3080.043735	296901.854697	53.843905
3079.360609	296576.596278	53.848909
3079.004632	296218.203803	53.853914
3077.964538	295883.934453	53.858919
3077.226048	295540.779716	53.863924
3076.807337	295193.244379	53.868929
3076.076881	294853.015970	53.873933
3075.510166	294508.533537	53.878938
3074.613325	294173.449316	53.883943
3073.741817	293830.160086	53.888948
3073.143455	293490.290678	53.893953
3072.581432	293152.554285	53.898957
3072.235951	292809.103890	53.903962
3071.693200	292461.660353	53.908967
3070.684022	292134.715118	53.913972
3070.113864	291778.539587	53.918977
3069.825890	291434.696170	53.923981
3068.822033	291091.551347	53.928986
3068.350635	290735.944520	53.933991
3067.080794	290388.638728	53.938996
3066.972646	290052.609153	53.944001
3066.083270	289714.512586	53.949005
3065.263244	289358.067828	53.954010
3064.754330	289013.466897	53.959015
3063.951814	288677.010829	53.964020
3063.643713	288325.373695	53.969025
3063.022402	287991.485958	53.974029
3062.124210	287641.673300	53.979034
3061.308384	287300.913853	53.984039
3060.649533	286964.866284	53.989044
3060.370130	286621.296225	53.994049
3059.471894	286283.528630	53.999053
3058.585413	285938.016589	54.004058
3058.165377	285586.369026	54.009063
3057.276210	285253.743687	54.014068
3056.947268	284912.370266	54.019073
3055.918407	284552.031707	54.024077
3055.254344	284228.971475	54.029082
3054.661739	283878.699695	54.034087
3054.161989	283539.797264	54.039092
3053.952230	283201.332617	54.044097
3052.979937	282854.609391	54.049101
3052.381500	282509.431290	54.054106
3051.860592	282161.770302	54.059111
3050.679412	281818.059330	54.064116
3050.277235	281468.952962	54.069121
3049.658547	281108.623699	54.074125
3049.009323	280763.783835	54.079130
3048.483344	280410.647116	54.084135
3047.667783	280062.140385	54.089140
3047.015570	279702.376136	54.094145
3046.190917	279376.461024	54.099149
3045.591348	279016.739152	54.104154
3044.972082	278669.907289	54.109159
3044.202455	278326.613772	54.114164
3043.438339	277978.123762	54.119169
3042.767835	277644.237720	54.124173
3042.434849	277286.485271	54.129178
3041.570268	276943.232016	54.134183
3040.727672	276603.744569	54.139188
3040.145224	276248.298181	54.144193
3039.362472	275918.046252	54.149197
3038.528090	275582.479596	54.154202
3038.476365	275230.820396	54.159207
3037.508066	274890.232214	54.164212
3037.010816	274545.825654	54.169217
3036.387098	274201.439144	54.174221
3035.733327	273847.939757	54.179226
3034.958841	273514.019247	54.184231
3034.278651	273169.157943	54.189236
3033.773403	272818.054746	54.194241
3033.020485	272475.981167	54.199245
3032.099884	272129.171641	54.204250
3031.647125	271780.225240	54.209255
3031.038200	271440.497744	54.214260
3030.332043	271081.633579	54.219265
3029.443003	270741.695995	54.224269
3028.895914	270395.617509	54.229274
3028.433884	270058.235873	54.234279
3028.056206	269713.658991	54.239284
3027.509913	269351.943362	54.244289
3026.462539	269007.600187	54.249293
3025.589613	268652.099980	54.254298
3025.374514	268301.793266	54.259303
3024.431865	267955.218413	54.264308
3023.754040	267607.532211	54.269313
3023.218313	267258.117394	54.274317
3022.262548	266904.439726	54.279322
3021.749455	266558.434578	54.284327
3021.086099	266223.404768	54.289332
3020.695400	265872.236234	54.294337
3019.949162	265526.498034	54.299341
3018.998371	265178.525854	54.304346
3018.325938	264835.297918	54.309351
3017.454659	264484.334031	54.314356
3017.281268	264137.462240	54.319361
3016.530340	263796.361554	54.324365
3015.945388	263439.954187	54.329370
3015.317459	263083.350262	54.334375
3013.903087	262750.097901	54.339380
3014.007117	262387.393955	54.344385
3013.410241	262057.247363	54.349389
3012.633964	261706.245954	54.354394
3012.094872	261348.229266	54.359399
3011.531373	261001.448154	54.364404
3010.755638	260654.675601	54.369409
3009.742668	260303.713414	54.374413
3009.330360	259946.442522	54.379418
3008.605534	259597.931502	54.384423
3007.596025	259253.693634	54.389428
3007.116100	258902.801806	54.394433
3006.626429	258555.375603	54.399437
3005.680957	258204.583951	54.404442
3005.224055	257855.880224	54.409447
3004.357862	257517.505158	54.414452
3004.004666	257159.897983	54.419457
3003.305108	256807.083126	54.424461
3002.397026	256465.634771	54.429466
3002.081589	256110.493681	54.434471
3001.389068	255771.533587	54.439476
3000.733751	255413.264103	54.444481
3000.040326	255056.223708	54.449485
2999.502792	254707.283261	54.454490
2998.844359	254348.736065	54.459495
2998.220779	254008.978610	54.464500
2997.635573	253652.534896	54.469505
2996.638695	253306.929496	54.474509
2996.041833	252944.300567	54.479514
2995.364271	252593.425302	54.484519
2994.545789	252245.705443	54.489524
2994.009051	251896.872084	54.494529
2993.462828	251550.485728	54.499533
2992.643338	251194.898993	54.504538
2992.056055	250848.571520	54.509543
2991.254264	250502.609796	54.514548
2990.978124	250141.387664	54.519553
2990.337455	249799.985892	54.524557
2989.554507	249445.594135	54.529562
2989.097658	249088.172027	54.534567
2988.061635	248736.088450	54.539572
2987.256995	248382.568434	54.544577
2986.554042	248034.482884	54.549581
2985.526480	247682.807910	54.554586
2985.223213	247324.423474	54.559591
2984.559987	246992.148435	54.564596
2984.034186	246628.733273	54.569601
2982.958915	246294.131322	54.574605
2982.657981	245944.790338	54.579610
2982.192287	245585.137309	54.584615
2981.383309	245242.041211	54.589620
2980.571580	244886.799422	54.594625
2980.255338	244535.554609	54.599629
2979.289576	244193.326406	54.604634
2979.119259	243836.356157	54.609639
2978.022196	243495.933157	54.614644
2977.483640	243141.238615	54.619649
2976.798282	242780.431250	54.624653
2975.696439	242439.757229	54.629658
2975.654912	242091.098598	54.634663
2974.702970	241734.283564	54.639668
2974.069285	241391.908631	54.644673
2973.435700	241046.249731	54.649677
2972.633446	240695.602027	54.654682
2971.797247	240350.562938	54.659687
2971.258314	239993.993377	54.664692
2970.710164	239643.232254	54.669697
2970.220971	239293.557848	54.674701
2969.565074	238943.452567	54.679706
2968.981616	238590.332162	54.684711
2967.950933	238237.411007	54.689716
2967.510767	237882.538650	54.694721
2966.814717	237526.129210	54.699725
2965.972496	237187.161305	54.704730
2965.374755	236841.280592	54.709735
2964.757463	236494.894842	54.714740
2964.449649	236125.976982	54.719745
2963.517040	235783.997783	54.724749
2962.794479	235433.278020	54.729754
2962.154281	235079.567233	54.734759
2961.132636	234733.786190	54.739764
2960.612874	234384.693089	54.744769
2959.817183	234041.857868	54.749773
2959.689105	233698.841772	54.754778
2958.828751	233344.764645	54.759783
2958.155336	233001.251707	54.764788
2957.652931	232640.958541	54.769793
2957.040617	232292.142270	54.774797
2956.077309	231943.433784	54.779802
2955.525483	231583.967290	54.784807
2954.313070	231243.601582	54.789812
2953.806811	230895.461248	54.794817
2953.342534	230545.864264	54.799821
2952.769466	230192.873957	54.804826
2952.437184	229851.075586	54.809831
2951.159061	229510.523117	54.814836
2950.847262	229147.743753	54.819841
2950.007818	228807.939329	54.824845
2949.126282	228464.756526	54.829850
2949.099040	228112.757534	54.834855
2948.203269	227766.677179	54.839860
2947.834081	227413.665828	54.844865
2946.995478	227056.312782	54.849869
2946.307972	226706.677450	54.854874
2945.984958	226347.119827	54.859879
2944.683982	226002.409402	54.864884
2944.321303	225651.492265	54.869889
2943.285428	225301.841665	54.874893
2942.679835	224961.837580	54.879898
2942.275629	224600.416448	54.884903
2941.410757	224259.094270	54.889908
2940.763943	223910.011924	54.894913
2940.129043	223567.994362	54.899917
2939.505838	223207.008899	54.904922
2939.041861	222853.956052	54.909927
2937.955010	222513.847776	54.914932
2937.683477	222157.317886	54.919937
2937.153475	221810.174156	54.924941
2936.272799	221468.395780	54.929946
2935.638393	221104.341453	54.934951
2934.898563	220756.930294	54.939956
2934.090273	220414.088732	54.944961
2933.655210	220064.977746	54.949965
2932.890927	219707.570119	54.954970
2932.360055	219356.771956	54.959975
2931.544484	219010.564882	54.964980
2931.237204	218657.405279	54.969985
2930.755367	218306.388077	54.974989
2929.698810	217954.419820	54.979994
2928.933191	217594.069809	54.984999
2928.436468	217246.802533	54.990004
2927.666223	216894.106904	54.995009
2927.030487	216532.799879	55.000013
2926.653213	216185.939049	55.005018
2926.168278	215826.482974	55.010023
2925.075226	215482.195658	55.015028
2924.403124	215117.656094	55.020033
2923.564049	214764.498672	55.025037
2923.041007	214412.604096	55.030042
2922.255533	214059.836494	55.035047
2921.634112	213715.814529	55.040052
2921.137702	213356.220792	55.045057
2920.415000	213013.173155	55.050061
2919.747622	212659.732523	55.055066
2919.139066	212303.777107	55.060071
2918.332601	211960.277380	55.065076
2917.993240	211603.112267	55.070081
2917.223275	211240.722605	55.075085
2916.554809	210888.971983	55.080090
2915.848915	210531.183657	55.085095
2915.575763	210172.870671	55.090100
2914.627742	209821.132128	55.095105
2913.851064	209462.686597	55.100109
2912.990283	209106.178286	55.105114
2912.616252	208756.404037	55.110119
2911.861027	208402.504924	55.115124
2911.262003	208053.533971	55.120129
2910.542998	207699.365971	55.125133
2909.813496	207348.561628	55.130138
2909.497690	206980.245364	55.135143
2908.493774	206636.742955	55.140148
2908.010898	206273.090080	55.145153
2907.483616	205915.860690	55.150157
2906.386425	205559.360043	55.155162
2905.954090	205204.487111	55.160167
2905.270653	204852.341376	55.165172
2904.456714	204493.384442	55.170177
2904.158422	204138.102344	55.175181
2903.133797	203799.086918	55.180186
2902.559640	203440.773133	55.185191
2901.876980	203083.102373	55.190196
2901.678037	202718.485324	55.195201
2900.835827	202380.454904	55.200205
2899.896806	202015.946902	55.205210
2899.485465	201650.657841	55.210215
2898.238330	201306.284374	55.215220
2897.486398	200952.608691	55.220225
2897.245436	200598.981650	55.225229
2896.514259	200253.400576	55.230234
2896.082485	199892.122270	55.235239
2895.152403	199539.871067	55.240244
2895.029218	199184.109554	55.245249
2894.056059	198838.168705	55.250253
2893.239560	198476.350089	55.255258
2893.066596	198118.224048	55.260263
2892.189967	197765.339925	55.265268
2891.675992	197403.798908	55.270273
2890.782784	197042.803981	55.275277
2889.987287	196675.561113	55.280282
2889.455302	196330.037800	55.285287
2888.726608	195975.780927	55.290292
2888.002031	195612.784337	55.295297
2887.443675	195253.912072	55.300301
2886.459598	194902.680542	55.305306
2886.107917	194547.495975	55.310311
2885.432318	194189.998575	55.315316
2884.905169	193837.824195	55.320321
2884.153405	193462.747133	55.325325
2883.588723	193114.757175	55.330330
2883.331096	192753.221455	55.335335
2882.120730	192404.282707	55.340340
2881.736304	192038.522725	55.345345
2880.873457	191685.004605	55.350349
2879.796719	191319.957640	55.355354
2879.308048	190958.471816	55.360359
2879.007878	190622.531889	55.365364
2877.983270	190253.184423	55.370369
2877.710826	189894.064277	55.375373
2876.726295	189543.685533	55.380378
2876.306329	189178.500033	55.385383
2875.486424	188825.237986	55.390388
2875.077049	188467.855172	55.395393
2874.387462	188104.718125	55.400397
2873.630618	187751.912207	55.405402
2873.234091	187381.978956	55.410407
2872.154365	187020.973146	55.415412
2871.706899	186667.388657	55.420417
2870.980384	186311.319460	55.425421
2870.358322	185943.150955	55.430426
2869.809477	185584.489542	55.435431
2868.947215	185230.892845	55.440436
2868.158966	184858.001674	55.445441
2867.483309	184498.936459	55.450445
2866.593691	184152.323823	55.455450
2866.296016	183791.995938	55.460455
2865.705170	183445.583203	55.465460
2865.111302	183084.939068	55.470465
2864.505524	182720.394517	55.475469
2863.697402	182363.250269	55.480474
2862.938327	181998.290788	55.485479
2862.316474	181650.599657	55.490484
2861.931134	181293.295481	55.495489
2860.999944	180930.102212	55.500493
2860.182614	180565.634694	55.505498
2859.635797	180212.791653	55.510503
2858.909336	179852.411656	55.515508
2858.504651	179487.442806	55.520513
2857.491003	179124.430600	55.525517
2856.727378	178759.550314	55.530522
2856.104916	178408.464138	55.535527
2855.212314	178059.649565	55.540532
2854.731800	177711.764750	55.545537
2854.401780	177347.222421	55.550541
2853.310000	176994.161990	55.555546
2853.078993	176628.249385	55.560551
2852.102998	176286.674555	55.565556
2851.594404	175924.297126	55.570561
2851.021861	175562.861493	55.575565
2850.255427	175218.006468	55.580570
2849.617565	174847.684633	55.585575
2848.518439	174501.451228	55.590580
2848.275986	174140.370291	55.595585
2847.883612	173783.182612	55.600589
2846.785325	173431.947419	55.605594
2845.952507	173076.730777	55.610599
2845.412838	172724.497692	55.615604
2844.871865	172374.875045	55.620609
2843.685350	172023.170329	55.625613
2843.372554	171665.226090	55.630618
2842.683500	171309.214135	55.635623
2841.974501	170910.059561	55.640628
2841.467218	170555.831529	55.645633
2840.946718	170197.806497	55.650637
2840.239679	169850.890583	55.655642
2839.765286	169490.118011	55.660647
2838.919040	169139.046811	55.665652
2838.269464	168788.494495	55.670657
2837.587881	168439.412841	55.675661
2836.726982	168083.610530	55.680666
2836.461124	167716.056752	55.685671
2835.010528	167378.996132	55.690676
2834.840821	167010.620195	55.695681
2834.510716	166660.787257	55.700685
2833.447787	166315.168050	55.705690
2833.126174	165957.494884	55.710695
2832.123223	165616.335786	55.715700
2831.546466	165252.097885	55.720705
2831.081446	164892.258005	55.725709
2830.072160	164551.325923	55.730714
2829.977853	164187.874063	55.735719
2829.269264	163838.432952	55.740724
2828.537501	163467.053557	55.745729
2828.108608	163109.564998	55.750733
2827.474925	162764.534271	55.755738
2826.932861	162389.169041	55.760743
2825.842761	162034.694686	55.765748
2825.198064	161671.266277	55.770753
2824.537733	161315.230751	55.775757
2823.950712	160963.497106	55.780762
2823.528326	160594.310627	55.785767
2822.385801	160242.837389	55.790772
2821.745787	159888.656425	55.795777
2821.409072	159522.607776	55.800781
2820.652531	159160.036525	55.805786
2819.533259	158789.059710	55.810791
2819.364983	158444.938098	55.815796
2818.810169	158081.456236	55.820801
2818.102340	157720.977145	55.825805
2817.094297	157370.236177	55.830810
2816.975421	156995.166618	55.835815
2816.166516	156644.287116	55.840820
2815.046249	156280.545188	55.845825
2814.719854	155927.753403	55.850829
2813.905756	155572.233238	55.855834
2813.413060	155204.971280	55.860839
2812.616640	154842.121430	55.865844
2811.953508	154473.559733	55.870849
2811.439045	154121.744518	55.875853
2810.449242	153762.915545	55.880858
2809.990314	153400.320204	55.885863
2809.222598	153036.659176	55.890868
2808.270966	152673.946425	55.895873
2808.013408	152321.601131	55.900877
2807.116180	151969.259227	55.905882
2806.358591	151612.234351	55.910887
2805.957638	151259.008019	55.915892
2805.151422	150902.329046	55.920897
2804.681293	150545.473649	55.925901
2803.409938	150190.833445	55.930906
2803.032317	149834.250826	55.935911
2802.535542	149471.399892	55.940916
2801.708007	149126.385591	55.945921
2801.317209	148772.231554	55.950925
2800.346036	148412.301832	55.955930
2799.973689	148059.665118	55.960935
2799.288183	147704.476635	55.965940
2798.623116	147345.908425	55.970945
2797.974260	146985.981913	55.975949
2797.200807	146632.433335	55.980954
2796.727416	146268.687460	55.985959
2795.963307	145911.028097	55.990964
2795.100097	145561.241913	55.995969
2794.716183	145189.818898	56.000973
2794.096139	144840.192896	56.005978
2793.125836	144478.439975	56.010983
2792.194522	144140.993944	56.015988
2791.707533	143773.454481	56.020993
2791.054408	143423.214374	56.025997
2790.207089	143070.734508	56.031002
2789.716204	142716.639328	56.036007
2789.270570	142364.815536	56.041012
2788.494728	142012.501732	56.046017
2788.014319	141655.088165	56.051021
2787.157753	141304.129511	56.056026
2786.434912	140940.486006	56.061031
2785.486010	140594.696092	56.066036
2784.952519	140237.510994	56.071041
2784.584425	139892.348679	56.076045
2783.841270	139539.461420	56.081050
2783.274686	139178.533441	56.086055
2782.356327	138832.898800	56.091060
2781.765426	138479.999982	56.096065
2781.230659	138120.401122	56.101069
2780.581592	137775.422218	56.106074
2779.921612	137415.648506	56.111079
2779.285590	137065.962538	56.116084
2778.699509	136708.929889	56.121089
2778.374354	136350.780440	56.126093
2777.367371	135994.102684	56.131098
2776.548179	135629.294675	56.136103
2776.183302	135276.195362	56.141108
2775.400727	134931.131466	56.146113
2774.747341	134565.192720	56.151117
2774.044104	134210.241869	56.156122
2773.827312	133849.006688	56.161127
2772.667437	133495.940803	56.166132
2772.026230	133129.129264	56.171137
2771.432777	132783.349913	56.176141
2770.649530	132420.571233	56.181146
2770.082622	132063.415315	56.186151
2769.281397	131716.614914	56.191156
2768.565207	131376.346673	56.196161
2767.583363	131019.345906	56.201165
2767.029971	130669.318369	56.206170
2766.708947	130300.613031	56.211175
2765.895417	129961.850712	56.216180
2765.357645	129604.467433	56.221185
2764.901337	129247.113945	56.226189
2763.721823	128904.548762	56.231194
2763.261785	128554.113910	56.236199
2762.877967	128194.730466	56.241204
2762.142424	127840.004851	56.246209
2761.387795	127482.873857	56.251213
2760.915467	127131.658980	56.256218
2760.443631	126762.783427	56.261223
2759.664012	126419.728711	56.266228
2758.767162	126055.666938	56.271233
2758.312000	125695.387905	56.276237
2757.143303	125349.093898	56.281242
2756.559196	124971.777602	56.286247
2756.137369	124631.190526	56.291252
2755.450267	124278.979949	56.296257
2755.080429	123920.412718	56.301261
2754.254903	123568.665149	56.306266
2753.819624	123202.740336	56.311271
2753.338398	122846.909822	56.316276
2751.893617	122499.210772	56.321281
2751.632348	122134.073062	56.326285
2751.071453	121775.539617	56.331290
2750.164881	121425.090332	56.336295
2749.466571	121062.995089	56.341300
2748.684566	120698.645392	56.346305
2747.959798	120350.340095	56.351309
2747.416796	120002.328058	56.356314
2747.077951	119645.115335	56.361319
2745.931081	119286.645303	56.366324
2745.185211	118932.757029	56.371329
2744.891476	118579.265361	56.376333
2744.317749	118226.464005	56.381338
2743.569317	117858.936860	56.386343
2742.986965	117517.337499	56.391348
2742.325336	117153.640628	56.396353
2741.648159	116805.991237	56.401357
2740.719156	116450.833182	56.406362
2740.396770	116083.771821	56.411367
2739.674069	115731.193484	56.416372
2738.765284	115381.772267	56.421377
2738.449819	115025.540470	56.426381
2737.302802	114669.965869	56.431386
2737.090967	114310.224293	56.436391
2736.345074	113962.129761	56.441396
2735.147796	113592.533174	56.446401
2734.852708	113238.659010	56.451405
2733.551867	112894.443409	56.456410
2733.279410	112550.145810	56.461415
2732.608257	112199.119324	56.466420
2731.958773	111849.725331	56.471425
2731.660301	111497.869165	56.476429
2730.671881	111153.964568	56.481434
2730.190025	110790.547125	56.486439
2729.386045	110449.117083	56.491444
2728.857707	110088.484147	56.496449
2728.020368	109744.994159	56.501453
2727.102829	109394.611448	56.506458
2726.848409	109029.293150	56.511463
2725.826311	108688.886763	56.516468
2725.007514	108344.284126	56.521473
2724.564923	107999.734660	56.526477
2724.066624	107650.643183	56.531482
2723.267852	107306.420181	56.536487
2722.539146	106950.636999	56.541492
2722.005805	106608.304433	56.546497
2721.520847	106258.444297	56.551501
2720.718387	105913.582009	56.556506
2720.007113	105558.356039	56.561511
2719.596287	105212.077786	56.566516
2718.497758	104859.816640	56.571521
2718.135166	104516.890676	56.576525
2717.450616	104178.835874	56.581530
2716.831584	103816.059177	56.586535
2715.984130	103470.535343	56.591540
2715.301603	103126.309973	56.596545
2714.863088	102775.675524	56.601549
2713.800680	102427.022882	56.606554
2713.412479	102087.860092	56.611559
2712.911974	101734.707300	56.616564
2711.944861	101387.019305	56.621569
2711.550422	101032.896168	56.626573
2710.598351	100692.504615	56.631578
2710.291434	100343.579553	56.636583
2709.277722	99999.522634	56.641588
2708.471191	99646.596031	56.646593
2708.232395	99299.071417	56.651597
2706.987546	98952.631138	56.656602
2706.754441	98620.293994	56.661607
2706.250567	98264.797311	56.666612
2705.608271	97921.746541	56.671617
2705.029545	97571.321089	56.676621
2704.017225	97227.749566	56.681626
2703.409537	96878.633202	56.686631
2702.800590	96532.059229	56.691636
2702.281329	96187.391625	56.696641
2701.705184	95830.587345	56.701645
2700.634044	95482.250912	56.706650
2700.378051	95132.649241	56.711655
2699.890685	94784.148711	56.716660
2699.041248	94431.233917	56.721665
2698.135911	94087.877267	56.726669
2697.608936	93737.408162	56.731674
2697.034604	93389.184161	56.736679
2696.193001	93041.978143	56.741684
2695.522842	92694.293855	56.746689
2695.241843	92340.656393	56.751693
2694.129799	91998.049650	56.756698
2693.245473	91649.236374	56.761703
2692.895081	91296.171962	56.766708
2692.291630	90955.796154	56.771713
2691.521738	90603.963308	56.776717
2690.585353	90263.302300	56.781722
2690.002174	89910.398563	56.786727
2689.423037	89580.184556	56.791732
2688.613892	89234.009991	56.796737
2688.516913	88885.908582	56.801741
2687.331904	88545.015917	56.806746
2686.904120	88185.896318	56.811751
2686.728466	87841.158836	56.816756
2685.561156	87494.777248	56.821761
2685.162172	87146.517178	56.826765
2684.002279	86807.087073	56.831770
2683.328500	86446.254183	56.836775
2682.508017	86118.597347	56.841780
2681.902805	85780.382484	56.846785
2681.464301	85421.900394	56.851789
2680.584207	85097.552218	56.856794
2679.982699	84751.867104	56.861799
2679.248011	84410.734430	56.866804
2678.648361	84064.755996	56.871809
2678.052847	83726.293471	56.876813
2677.256822	83398.598735	56.881818
2676.753997	83049.953239	56.886823
2676.305767	82706.882320	56.891828
2675.555192	82374.842159	56.896833
2675.120125	82022.482673	56.901837
2674.195266	81679.649889	56.906842
2673.350221	81342.380838	56.911847
2672.700196	80991.397397	56.916852
2672.063397	80656.698506	56.921857
2671.486230	80309.295677	56.926861
2670.733766	79975.798511	56.931866
2670.193591	79632.469656	56.936871
2669.342310	79288.429039	56.941876
2668.642977	78953.349418	56.946881
2668.431253	78610.771331	56.951885
2667.815899	78268.674800	56.956890
2667.324948	77921.545738	56.961895
2666.368223	77570.770553	56.966900
2665.733282	77223.315000	56.971905
2664.845092	76885.802663	56.976909
2664.055778	76550.003687	56.981914
2663.606344	76196.979517	56.986919
2663.252763	75847.735171	56.991924
2662.236653	75528.151928	56.996929
2661.508728	75173.878237	57.001933
2660.820219	74821.872662	57.006938
2660.024380	74491.633547	57.011943
2659.302058	74148.305706	57.016948
2658.778956	73806.776730	57.021953
2657.797057	73464.857479	57.026957
2657.247506	73136.495892	57.031962
2656.885539	72789.992100	57.036967
2656.313060	72455.063390	57.041972
2655.524873	72127.066669	57.046977
2655.419619	71777.879262	57.051981
2654.310196	71443.933211	57.056986
2653.603333	71097.291919	57.061991
2652.894452	70753.716486	57.066996
2652.333445	70411.466455	57.072001
2651.464510	70066.268831	57.077005
2650.482203	69727.593863	57.082010
2649.969151	69402.854498	57.087015
2649.593692	69057.444431	57.092020
2648.637892	68728.720165	57.097025
2648.125848	68386.820760	57.102029
2647.395611	68060.649759	57.107034
2646.896739	67708.823075	57.112039
2646.456424	67379.077269	57.117044
2645.663948	67028.921236	57.122049
2645.184219	66678.778980	57.127053
2644.139042	66360.352540	57.132058
2643.308605	66012.659094	57.137063
2643.150470	65673.544249	57.142068
2642.096056	65342.230245	57.147073
2641.827194	64997.499451	57.152077
2640.739886	64664.720591	57.157082
2640.137906	64322.087411	57.162087
2639.554611	63988.705393	57.167092
2638.783237	63660.503719	57.172097
2638.481905	63312.414563	57.177101
2637.312926	62988.893901	57.182106
2636.631225	62648.788684	57.187111
2636.092292	62315.204228	57.192116
2635.129010	61977.378057	57.197121
2634.531281	61639.006168	57.202125
2633.939688	61313.877848	57.207130
2633.227088	60979.945663	57.212135
2632.701559	60658.635832	57.217140
2631.696810	60321.102376	57.222145
2631.288524	59988.655850	57.227149
2630.243957	59660.779142	57.232154
2629.806223	59347.299382	57.237159
2629.146861	59014.748557	57.242164
2628.232885	58698.712243	57.247169
2627.896616	58356.693032	57.252173
2626.959557	58043.732162	57.257178
2626.214583	57714.503491	57.262183
2625.522040	57391.586382	57.267188
2625.154891	57063.205110	57.272193
2624.670307	56732.509503	57.277197
2624.216722	56413.682731	57.282202
2623.173987	56085.656977	57.287207
2622.899209	55757.528047	57.292212
2621.876374	55438.802087	57.297217
2621.474735	55092.613266	57.302221
2620.611520	54764.873860	57.307226
2619.722386	54441.995490	57.312231
2619.292641	54125.267999	57.317236
2618.643185	53795.983770	57.322241
2618.037063	53459.250025	57.327245
2616.883997	53150.178725	57.332250
2616.460146	52817.661697	57.337255
2616.032481	52494.055076	57.342260
2615.366208	52166.508577	57.347265
2614.581068	51834.459248	57.352269
2613.775935	51520.823604	57.357274
2613.186349	51201.018256	57.362279
2612.571060	50868.849117	57.367284
2611.729690	50549.443308	57.372289
2611.276658	50213.625488	57.377293
2610.456665	49890.634135	57.382298
2609.441450	49583.725119	57.387303
2609.164441	49260.320638	57.392308
2608.154435	48953.674742	57.397313
2607.786807	48623.652971	57.402317
2606.881160	48308.466874	57.407322
2606.390724	47985.562305	57.412327
2605.584534	47671.137310	57.417332
2604.712207	47356.184333	57.422337
2604.299743	47029.672556	57.427341
2603.349601	46723.761216	57.432346
2602.771121	46420.405767	57.437351
2602.757671	46100.063290	57.442356
2601.681057	45772.427604	57.447361
2601.282204	45465.365972	57.452365
2600.480652	45142.107468	57.457370
2599.806557	44817.212286	57.462375
2599.349966	44495.030698	57.467380
2598.141604	44195.001624	57.472385
2597.736768	43867.001140	57.477389
2596.817251	43561.719058	57.482394
2596.129425	43242.655452	57.487399
2595.842451	42921.298411	57.492404
2594.500584	42605.876231	57.497409
2594.149859	42294.777308	57.502413
2593.103504	41996.525201	57.507418
2592.869044	41691.977110	57.512423
2592.289796	41382.388629	57.517428
2591.259871	41079.922129	57.522433
2590.723733	40755.710636	57.527437
2589.769746	40450.206159	57.532442
2589.116554	40150.077292	57.537447
2588.976361	39841.620125	57.542452
2588.027628	39540.069107	57.547457
2587.525837	39228.918561	57.552461
2586.671791	38927.824990	57.557466
2586.000481	38612.014437	57.562471
2585.507152	38300.574463	57.567476
2584.236124	38000.658898	57.572481
2583.979269	37703.817279	57.577485
2583.157370	37407.870244	57.582490
2582.708557	37105.959258	57.587495
2581.824734	36795.620519	57.592500
2581.236559	36495.294726	57.597505
2580.771376	36190.677827	57.602509
2580.061396	35890.361606	57.607514
2579.390544	35582.693675	57.612519
2578.968719	35273.084305	57.617524
2577.541144	34986.526403	57.622529
2576.980828	34677.816093	57.627533
2576.296909	34388.106737	57.632538
2575.328327	34093.052204	57.637543
2575.169961	33799.056577	57.642548
2574.274947	33503.906021	57.647553
2573.742002	33201.928710	57.652557
2573.048463	32909.941039	57.657562
2572.460834	32620.141392	57.662567
2571.621612	32322.446263	57.667572
2570.366332	32028.968780	57.672577
2570.233897	31738.870691	57.677581
2569.677790	31451.382504	57.682586
2568.835568	31158.897929	57.687591
2568.152292	30863.928497	57.692596
2567.281765	30581.822218	57.697601
2566.728150	30296.843961	57.702605
2565.910897	30009.728940	57.707610
2565.381588	29727.343151	57.712615
2564.810027	29440.799562	57.717620
2563.382827	29164.610558	57.722625
2562.925509	28885.139664	57.727629
2562.087116	28618.844966	57.732634
2561.477215	28344.135982	57.737639
2560.802419	28065.176537	57.742644
2559.906131	27794.054637	57.747649
2559.321753	27508.844111	57.752653
2558.226202	27255.683180	57.757658
2557.806016	26992.551755	57.762663
2556.858630	26723.208557	57.767668
2555.887143	26464.125403	57.772673
2554.995998	26200.289375	57.777677
2554.339603	25968.577328	57.782682
2553.177181	25722.995110	57.787687
2552.238787	25478.870631	57.792692
2551.193540	25258.430074	57.797697
2550.091301	25023.659135	57.802701
2548.819334	24828.413633	57.807706
2547.483313	24622.038523	57.812711
2546.953637	24419.177249	57.817716
2545.767793	24232.964387	57.822721
2545.145340	24029.343341	57.827725
2544.128578	23865.285630	57.832730
2543.254162	23683.198559	57.837735
2542.121312	23508.059354	57.842740
2541.266410	23350.214907	57.847745
2540.693694	23180.718689	57.852749
2539.314474	23035.560097	57.857754
2538.463043	22879.365392	57.862759
2538.150227	22728.864536	57.867764
2537.393773	22583.252095	57.872769
2536.487347	22450.994974	57.877773
2535.832751	22303.034874	57.882778
2535.407242	22169.450776	57.887783
2534.670103	22034.623852	57.892788
2533.771699	21901.500717	57.897793
2533.252578	21763.427156	57.902797
2532.444799	21643.723327	57.907802
2531.622542	21510.317441	57.912807
2531.101439	21384.017551	57.917812
2530.254822	21258.143728	57.922817
2529.712258	21145.611039	57.927821
2528.966428	21012.125410	57.932826
2528.143338	20884.395036	57.937831
2527.690628	20772.059212	57.942836
2527.081763	20663.073619	57.947841
2526.428050	20532.619486	57.952845
2525.572432	20422.308817	57.957850
2524.924340	20303.987697	57.962855
2524.685214	20171.968812	57.967860
2524.001644	20056.759088	57.972865
2523.475567	19946.178079	57.977869
2522.614920	19836.016809	57.982874
2522.056466	19710.095903	57.987879
2521.453541	19600.907540	57.992884
2520.465738	19483.330147	57.997889
2519.907617	19356.919013	58.002893
2519.217161	19260.938714	58.007898
2518.329848	19153.082207	58.012903
2517.854010	19025.825870	58.017908
2517.252083	18910.780982	58.022913
2516.656173	18797.880864	58.027917
2516.211650	18695.720942	58.032922
2515.437613	18581.344016	58.037927
2514.793200	18471.290327	58.042932
2513.791021	18361.193478	58.047937
2513.659433	18246.361940	58.052941
2512.965585	18136.815774	58.057946
2512.017660	18025.825027	58.062951
2511.608240	17913.651283	58.067956
2510.651709	17806.336863	58.072961
2510.114483	17699.611501	58.077965
2509.410606	17587.785763	58.082970
2508.956027	17487.774947	58.087975
2508.475066	17370.842410	58.092980
2507.571077	17260.861138	58.097985
2506.820189	17162.764822	58.102989
2506.243371	17052.905438	58.107994
2505.535359	16946.754805	58.112999
2504.952756	16838.166519	58.118004
2503.845346	16741.955104	58.123009
2503.707884	16629.794108	58.128013
2503.195188	16525.965398	58.133018
2502.576222	16414.344633	58.138023
2502.021017	16308.657807	58.143028
2501.086911	16212.497204	58.148033
2500.575681	16097.087044	58.153037
2499.816103	15994.090931	58.158042
2498.678304	15896.477479	58.163047
2498.051386	15785.687520	58.168052
2497.215419	15703.426592	58.173057
2496.317047	15598.191602	58.178061
2495.667018	15510.557033	58.183066
2495.050755	15408.654680	58.188071
2494.672289	15311.567317	58.193076
2493.811793	15233.997286	58.198081
2493.228558	15133.956704	58.203085
2492.527402	15035.663598	58.208090
2491.841072	14949.298198	58.213095
2491.518332	14844.064134	58.218100
2490.600486	14756.519436	58.223105
2489.890149	14655.279940	58.228109
2489.199143	14579.147291	58.233114
2488.334165	14492.794632	58.238119
2487.888673	14398.522006	58.243124
2487.155872	14324.465750	58.248129
2486.446032	14225.005188	58.253133
2486.086251	14134.033936	58.258138
2485.317721	14050.364948	58.263143
2484.824694	13956.239801	58.268148
2483.865442	13872.742471	58.273153
2483.528415	13777.939464	58.278157
2482.955241	13688.361672	58.283162
2482.299065	13599.523691	58.288167
2481.840399	13497.114363	58.293172
2480.916222	13416.143638	58.298177
2480.142741	13322.521903	58.303181
2479.354387	13228.937033	58.308186
2478.308017	13134.973625	58.313191
2478.167683	13054.731643	58.318196
2477.423597	12983.483039	58.323201
2476.967826	12881.718159	58.328205
2475.955506	12799.955440	58.333210
2475.046819	12710.580896	58.338215
2474.703444	12623.560938	58.343220
2473.687390	12546.856998	58.348225
2472.939308	12461.701094	58.353229
2472.716015	12375.272313	58.358234
2471.631613	12305.262124	58.363239
2471.188753	12212.722619	58.368244
2470.490946	12142.050805	58.373249
2469.921226	12063.585170	58.378253
2469.466417	11984.784514	58.383258
2468.338327	11905.377881	58.388263
2468.082867	11827.696709	58.393268
2467.138522	11752.432577	58.398273
2466.531287	11663.324544	58.403277
2466.047266	11580.049937	58.408282
2465.429096	11503.144200	58.413287
2464.581933	11415.674284	58.418292
2463.771126	11343.757492	58.423297
2463.610627	11260.972268	58.428301
2462.764221	11177.374645	58.433306
2461.875199	11107.102318	58.438311
2461.706543	11019.803285	58.443316
2460.822305	10944.168921	58.448321
2459.855947	10862.337776	58.453325
2458.982327	10790.011061	58.458330
2458.288447	10712.240022	58.463335
2457.861490	10636.307272	58.468340
2456.930832	10566.045252	58.473345
2456.827218	10488.339193	58.478349
2455.837948	10423.142652	58.483354
2455.004720	10348.406397	58.488359
2455.001769	10265.684888	58.493364
2453.694764	10192.553975	58.498369
2453.295235	10121.962475	58.503373
2452.512154	10040.645219	58.508378
2451.975972	9972.739277	58.513383
2451.619207	9897.360478	58.518388
2450.807435	9819.531478	58.523393
2450.114611	9729.606215	58.528397
2449.128785	9671.769055	58.533402
2448.160572	9607.256744	58.538407
2447.989268	9534.004603	58.543412
2447.265784	9461.183556	58.548417
2446.876009	9385.221245	58.553421
2446.009483	9315.402237	58.558426
2445.335337	9239.714934	58.563431
2444.738987	9167.400588	58.568436
2443.965871	9100.437510	58.573441
2443.195576	9020.458226	58.578445
2442.538913	8951.424573	58.583450
2441.835511	8878.845371	58.588455
2441.616396	8799.933666	58.593460
2440.899532	8732.761747	58.598465
2440.023146	8664.820995	58.603469
2438.980219	8592.377877	58.608474
2438.327470	8531.819915	58.613479
2437.986585	8457.440239	58.618484
2437.255166	8399.228047	58.623489
2436.586348	8320.537692	58.628493
2436.098144	8246.906619	58.633498
2435.194796	8192.995079	58.638503
2434.552054	8108.557086	58.643508
2433.688906	8043.120562	58.648513
2432.984586	7975.130031	58.653517
2432.603913	7913.565864	58.658522
2431.980459	7849.915252	58.663527
2430.988466	7776.635378	58.668532
2430.784030	7714.257600	58.673537
2430.207571	7644.403569	58.678541
2429.538474	7573.690905	58.683546
2428.952979	7507.539824	58.688551
2428.585005	7433.627074	58.693556
2427.733066	7375.013595	58.698561
2427.130919	7287.239407	58.703565
2426.474789	7228.147405	58.708570
2425.568052	7158.851686	58.713575
2424.939727	7073.264801	58.718580
2424.105992	7012.099612	58.723585
2423.277167	6946.002232	58.728589
2422.604431	6870.236405	58.733594
2422.094041	6812.183111	58.738599
2421.390376	6753.920893	58.743604
2420.988679	6684.275965	58.748609
2420.371111	6613.667763	58.753613
2419.585097	6539.602510	58.758618
2419.029679	6479.186549	58.763623
2418.381977	6398.639888	58.768628
2417.546473	6338.344634	58.773633
2417.049877	6266.295944	58.778637
2416.533823	6203.113355	58.783642
2415.286871	6136.423313	58.788647
2414.913004	6068.379646	58.793652
2414.185401	6002.083489	58.798657
2413.494843	5939.649047	58.803661
2412.666410	5876.184528	58.808666
2412.029438	5811.295408	58.813671
2411.605216	5736.464563	58.818676
2410.578721	5678.832762	58.823681
2410.120680	5616.511890	58.828685
2409.393378	5552.300774	58.833690
2408.662852	5486.108354	58.838695
2408.355693	5414.489663	58.843700
2407.516159	5366.646005	58.848705
2406.815520	5293.298299	58.853709
2406.086806	5235.004233	58.858714
2405.518871	5176.148575	58.863719
2404.772683	5111.852456	58.868724
2403.997586	5050.755489	58.873729
2403.460226	4992.444661	58.878733
2402.879389	4928.164926	58.883738
2402.044271	4869.934922	58.888743
2401.681518	4792.609965	58.893748
2400.961277	4742.138828	58.898753
2400.513726	4682.096417	58.903757
2399.656411	4610.664295	58.908762
2398.860808	4543.823138	58.913767
2398.370749	4475.727153	58.918772
2397.545352	4421.554365	58.923777
2396.696005	4353.697311	58.928781
2396.237158	4293.924848	58.933786
2395.527070	4241.860701	58.938791
2394.921458	4172.066722	58.943796
2394.036721	4117.876072	58.948801
2393.108044	4069.047594	58.953805
2392.707599	4004.517735	58.958810
2392.146464	3938.572769	58.963815
2391.595349	3874.318165	58.968820
2390.650872	3834.461505	58.973825
2390.360548	3761.144702	58.978829
2389.716289	3698.095704	58.983834
2388.628579	3629.772699	58.988839
2388.214840	3576.662353	58.993844
2387.285996	3528.148793	58.998849
2386.879977	3471.469835	59.003853
2386.298955	3401.338090	59.008858
2385.469902	3349.071220	59.013863
2385.337725	3286.030331	59.018868
2384.402200	3229.555354	59.023873
2383.879344	3168.759806	59.028877
2383.272444	3101.001805	59.033882
2382.404156	3055.114955	59.038887
2381.755734	2992.810943	59.043892
2380.916456	2936.090778	59.048897
2380.187172	2877.006529	59.053901
2379.498690	2811.701934	59.058906
2378.739321	2760.734396	59.063911
2378.559463	2696.241559	59.068916
2377.653388	2645.188862	59.073921
2377.075054	2576.671721	59.078925
2376.727111	2520.747428	59.083930
2375.832483	2454.243787	59.088935
2375.172454	2399.583850	59.093940
2374.467092	2329.288495	59.098945
2373.836637	2268.554761	59.103949
2373.305928	2212.853827	59.108954
2372.201219	2161.749158	59.113959
2371.890854	2092.632710	59.118964
2370.873999	2043.351069	59.123969
2370.065278	1994.780192	59.128973
2369.837041	1941.773326	59.133978
2368.979889	1884.143799	59.138983
2368.310218	1817.911769	59.143988
2367.484338	1767.880842	59.148993
2367.039832	1709.650366	59.153997
2366.337635	1654.615108	59.159002
2365.575769	1593.180370	59.164007
2365.218753	1530.440555	59.169012
2364.183001	1483.635834	59.174017
2363.429088	1431.405719	59.179021
2362.891100	1374.306374	59.184026
2362.136393	1325.790673	59.189031
2361.453516	1257.760749	59.194036
2360.898875	1220.284345	59.199041
2360.305424	1166.667197	59.204045
2359.823737	1114.844500	59.209050
2358.497419	1069.288083	59.214055
2357.999061	1009.009395	59.219060
2357.673220	967.770932	59.224065
2356.956296	917.012863	59.229069
2356.111185	879.364204	59.234074
2355.593850	819.748488	59.239079
2355.033660	765.734883	59.244084
2354.337450	725.457866	59.249089
2353.564424	661.679172	59.254093
2352.765362	608.624974	59.259098
2351.789272	577.739325	59.264103
2351.565575	519.156910	59.269108
2350.448132	473.254652	59.274113
2349.556833	433.829391	59.279117
2349.080601	390.665759	59.284122
2348.080322	351.504006	59.289127
2347.825671	312.353422	59.294132
2347.024987	269.304682	59.299137
2346.319763	230.258890	59.304141
2346.001280	181.039201	59.309146
2344.899795	159.113792	59.314151
2344.558794	119.037593	59.319156
2343.575090	83.540221	59.324161
2342.400970	43.676775	59.329165
2341.741726	25.551116	59.334170
2340.671725	-5.307348	59.339175
2339.014625	-0.890885	59.344180
2334.552176	87.688945	59.349185
2334.458383	100.844219	59.354189
2335.562173	93.541781	59.359194
2335.738623	99.389460	59.364199
2336.315219	89.694911	59.369204
2335.705628	77.559810	59.374209
2334.805341	84.994289	59.379213
2333.679678	84.848132	59.384218
2332.197264	101.962436	59.389223
2332.170623	100.172321	59.394228
2331.561589	92.215885	59.399233
2330.732993	97.844500	59.404237
2330.698354	93.811737	59.409242
2329.596282	103.553682	59.414247
2329.008905	90.274957	59.419252
2328.541286	97.237142	59.424257
2328.234790	92.364434	59.429261
2327.303361	98.972839	59.434266
2326.507989	101.130179	59.439271
2325.757790	101.664041	59.444276
2325.080805	106.789241	59.449281
2324.635645	105.967482	59.454285
2324.238918	97.952145	59.459290
2323.211970	101.341496	59.464295
2322.499525	104.015521	59.469300
2321.652986	101.319419	59.474305
2321.415149	105.454068	59.479309
2321.250203	98.428529	59.484314
2320.335699	100.691493	59.489319
2319.751700	109.824600	59.494324
2318.933080	109.806364	59.499329
2317.741643	102.735471	59.504333
2317.137199	102.902457	59.509338
2316.594259	112.282933	59.514343
2316.171306	108.448942	59.519348
2315.723132	105.992425	59.524353
2314.991152	103.357000	59.529357
2314.348219	104.416304	59.534362
2313.275161	104.725418	59.539367
2312.503683	100.140913	59.544372
2311.879096	111.505453	59.549377
2311.635030	107.622592	59.554381
2311.367134	108.002698	59.559386
2310.496048	107.633255	59.564391
2310.162817	110.860553	59.569396
2308.915501	111.771294	59.574401
2308.232138	107.324195	59.579405
2307.717976	110.611727	59.584410
2307.045810	109.811782	59.589415
2306.110862	99.483357	59.594420
2305.460974	108.642683	59.599425
2305.468586	100.537990	59.604429
2305.009009	104.796114	59.609434
2303.432210	109.281891	59.614439
2303.438044	101.999041	59.619444
2302.933631	105.524713	59.624449
2301.616139	121.083309	59.629453
2301.298391	113.367668	59.634458
2300.617512	106.461802	59.639463
2300.037291	98.753105	59.644468
2299.256841	105.998293	59.649473
2298.336333	106.954974	59.654477
2297.933773	101.022064	59.659482
2296.721063	108.968145	59.664487
2296.195973	104.527486	59.669492
2295.578410	103.482350	59.674497
2294.601680	113.497735	59.679501
2295.370102	105.701287	59.684506
2294.140022	104.414268	59.689511
2293.036259	100.907451	59.694516
2292.805195	104.216312	59.699521
2292.551684	114.068108	59.704525
2291.174328	104.983062	59.709530
2290.448412	112.076108	59.714535
2290.084955	101.865196	59.719540
2289.990849	96.182977	59.724545
2288.594660	97.566753	59.729549
2287.862339	104.395894	59.734554
2287.735226	108.776325	59.739559
2286.786604	108.119577	59.744564
2285.629596	102.348907	59.749569
2285.437721	102.480424	59.754573
2285.250048	103.111149	59.759578
2284.366771	109.592089	59.764583
2282.961984	98.492982	59.769588
2283.075744	102.469367	59.774593
2282.250239	109.453634	59.779597
2281.883848	94.980856	59.784602
2280.282870	110.890328	59.789607
2279.936285	101.996602	59.794612
2279.699966	99.566413	59.799617
2279.224449	111.869216	59.804621
2278.474808	103.190800	59.809626
2277.080013	108.874546	59.814631
2277.189046	103.152220	59.819636
2276.052524	98.294481	59.824641
2275.347209	104.250474	59.829645
2275.419543	102.947690	59.834650
2274.328926	112.199005	59.839655
2273.433515	105.956355	59.844660
2272.539924	103.206234	59.849665
2272.352921	95.357911	59.854669
2272.410424	102.167429	59.859674
2270.739034	108.823838	59.864679
2269.863176	104.197558	59.869684
2269.262312	100.492718	59.874689
2269.151964	111.952310	59.879693
2269.053901	104.797899	59.884698
2267.590278	100.682725	59.889703
2267.108695	97.894064	59.894708
2266.072114	109.003846	59.899713
2265.472092	94.061949	59.904718
2265.101265	85.127929	59.909722
2263.978210	106.196870	59.914727
2264.204950	98.751257	59.919732
2263.299342	114.921013	59.924737
2262.550794	106.584613	59.929742
2262.145754	94.576345	59.934746
2260.996095	110.426854	59.939751
2260.478803	105.604935	59.944756
2260.064433	97.131960	59.949761
2259.438076	100.908783	59.954766
2258.810390	102.334674	59.959770
2257.829047	109.103978	59.964775
2256.582427	97.162970	59.969780
2256.639533	102.069244	59.974785
2256.061773	106.505385	59.979790
2254.967426	92.920762	59.984794
2253.940895	104.538286	59.989799
2254.421914	100.616112	59.994804
2253.139713	105.810518	59.999809
2252.118371	102.095111	60.004814
2252.388196	104.857764	60.009818
2251.364811	102.375810	60.014823
2250.591835	102.438662	60.019828
2249.860266	102.179567	60.024833
2249.213312	100.409004	60.029838
2248.412692	98.689624	60.034842
2247.712142	102.623293	60.039847
2247.349012	90.833880	60.044852
2246.634091	105.316070	60.049857
2246.044158	116.400745	60.054862
2245.813731	100.135556	60.059866
2244.984587	99.850941	60.064871
2244.354611	102.344753	60.069876
2243.039938	98.213851	60.074881
2242.309336	109.651982	60.079886
2242.506953	99.478235	60.084890
2241.070824	110.277680	60.089895
2240.308560	101.058832	60.094900
2239.940441	103.099539	60.099905
2239.714204	106.087529	60.104910
2238.982618	92.208838	60.109914
2237.835768	106.576626	60.114919
2237.576895	104.104289	60.119924
2236.865415	104.707724	60.124929
2236.477533	112.992904	60.129934
2235.979921	114.057559	60.134938
2235.239289	103.928566	60.139943
2234.045457	111.524760	60.144948
2233.086514	106.449643	60.149953
2232.280899	112.434174	60.154958
2231.889733	98.257062	60.159962
2231.268916	105.057488	60.164967
2231.372105	115.628531	60.169972
2230.484037	107.404158	60.174977
2229.891410	112.684724	60.179982
2229.367587	102.953410	60.184986
2228.382443	105.801598	60.189991
2227.549776	107.886038	60.194996
2226.307326	97.516547	60.200001
2225.943290	108.399811	60.205006
2225.981120	99.437234	60.210010
2224.816340	104.313416	60.215015
2223.961715	100.388656	60.220020
2223.321387	99.364495	60.225025
2222.836318	101.460024	60.230030
2222.269367	95.964779	60.235034
2221.620218	102.701895	60.240039
2221.247266	107.769424	60.245044
2220.739775	100.795083	60.250049
2219.885441	107.074337	60.255054
2219.636117	102.036463	60.260058
2218.151503	104.282670	60.265063
2217.187573	106.925655	60.270068
2216.724003	107.051393	60.275073
2216.158770	104.605581	60.280078
2215.654527	101.472031	60.285082
2215.137686	104.950805	60.290087
2214.477865	101.077144	60.295092
2214.227769	99.719856	60.300097
2213.401141	106.505628	60.305102
2212.717507	94.424880	60.310106
2211.465478	104.379877	60.315111
2210.757163	102.256373	60.320116
2210.297557	100.774633	60.325121
2209.576329	97.011636	60.330126
2209.421846	106.778333	60.335130
2208.593247	100.369001	60.340135
2208.131050	105.944256	60.345140
2207.750730	104.134560	60.350145
2206.693136	105.302245	60.355150
2205.736990	98.763344	60.360154
2205.053239	107.503873	60.365159
2204.264074	100.656219	60.370164
2204.055393	95.845282	60.375169
2203.585627	97.312361	60.380174
2203.002560	87.653540	60.385178
2201.609082	105.548539	60.390183
2200.670039	103.092649	60.395188
2200.181926	90.577207	60.400193
2199.332494	107.080238	60.405198
2199.257415	94.500847	60.410202
2198.311619	97.934135	60.415207
2198.048083	97.018933	60.420212
2197.511049	98.748987	60.425217
2196.654758	93.853140	60.430222
2196.539919	84.121619	60.435226
2195.786791	96.358072	60.440231
2194.789201	94.081777	60.445236
2193.790017	91.736353	60.450241
2192.739834	98.674282	60.455246
2192.770536	99.875895	60.460250
2192.314169	95.446438	60.465255
2191.609482	95.455897	60.470260
2191.106007	95.657353	60.475265
2189.448252	105.541112	60.480270
2188.660647	102.696940	60.485274
2188.563044	103.043734	60.490279
2188.309278	97.334816	60.495284
2187.665721	93.958459	60.500289
2186.789371	107.067566	60.505294
2186.540633	99.359931	60.510298
2185.681027	92.723728	60.515303
2184.575453	103.205833	60.520308
2183.690561	99.344235	60.525313
2182.963949	104.565641	60.530318
2182.617492	102.701693	60.535322
2182.068789	101.614123	60.540327
2181.819773	98.706585	60.545332
2181.271078	108.215713	60.550337
2180.371885	99.229916	60.555342
2179.375407	96.679072	60.560346
2178.457771	100.685041	60.565351
2177.710454	99.892322	60.570356
2177.469068	97.910785	60.575361
2176.724781	98.148872	60.580366
2176.475339	100.891397	60.585370
2175.869491	93.481685	60.590375
2175.091760	103.859745	60.595380
2173.840496	95.060690	60.600385
2172.865754	99.566133	60.605390
2172.837422	96.644085	60.610394
2171.917058	99.857313	60.615399
2171.364464	102.231635	60.620404
2170.957979	100.918086	60.625409
2170.387819	106.212441	60.630414
2170.451882	94.284311	60.635418
2169.497325	109.408481	60.640423
2168.137079	109.250726	60.645428
2167.348269	95.313336	60.650433
2166.393845	100.909918	60.655438
2166.523921	90.004182	60.660442
2165.862116	96.336474	60.665447
2165.280678	100.036805	60.670452
2164.352028	91.552413	60.675457
2162.648311	99.814549	60.680462
2162.809709	95.708117	60.685466
2162.321152	105.893651	60.690471
2161.144368	106.037940	60.695476
2160.837943	92.872389	60.700481
2160.240389	101.685974	60.705486
2160.034122	97.682027	60.710490
2159.341795	99.163924	60.715495
2158.740293	100.248228	60.720500
2157.698030	86.841475	60.725505
2156.930678	105.966467	60.730510
2156.334016	86.635604	60.735514
2155.430284	104.099693	60.740519
2155.127764	101.251107	60.745524
2154.855953	88.048532	60.750529
2153.909771	101.865705	60.755534
2152.993055	100.357155	60.760538
2152.040057	102.690934	60.765543
2151.360661	90.874457	60.770548
2151.185772	99.218877	60.775553
2150.567314	103.595263	60.780558
2150.150033	85.675644	60.785562
2149.552226	103.671490	60.790567
2148.262622	92.185208	60.795572
2147.686301	95.723887	60.800577
2147.247300	97.007906	60.805582
2146.842100	89.485950	60.810586
2146.038984	95.533172	60.815591
2144.987366	97.065771	60.820596
2144.296805	96.604665	60.825601
2143.244580	99.700057	60.830606
2143.182055	92.469070	60.835610
2142.397300	103.155742	60.840615
2141.834275	110.905764	60.845620
2141.511382	101.552590	60.850625
2140.752188	100.339160	60.855630
2140.598026	82.910789	60.860634
2139.203996	105.672170	60.865639
2138.602908	101.268839	60.870644
2137.925685	95.611348	60.875649
2137.409115	100.972894	60.880654
2136.991137	101.007838	60.885658
2135.486701	103.402307	60.890663
2134.685079	104.786439	60.895668
2134.372169	92.804591	60.900673
2133.766091	110.334999	60.905678
2133.530993	98.940019	60.910682
2133.073480	104.640689	60.915687
2132.344752	99.738815	60.920692
2131.346181	96.500800	60.925697
2130.164257	101.701422	60.930702
2129.916825	98.402571	60.935706
2129.827668	94.742731	60.940711
2128.904667	99.251016	60.945716
2128.371445	88.113073	60.950721
2126.935053	95.422947	60.955726
2126.410386	89.417994	60.960730
2125.799888	95.612848	60.965735
2124.986801	87.015526	60.970740
2125.125229	88.966411	60.975745
2124.363371	98.157715	60.980750
2123.903943	95.580026	60.985754
2122.563461	90.451963	60.990759
2121.564640	100.168125	60.995764
2121.532536	89.259742	61.000769
2120.807041	103.242171	61.005774
2120.664713	92.860610	61.010778
2119.458339	97.204133	61.015783
2118.425344	97.003941	61.020788
2117.852033	98.033320	61.025793
2117.229547	98.753547	61.030798
2116.512906	96.235594	61.035802
2116.311710	84.646023	61.040807
2116.152064	97.392267	61.045812
2115.288207	94.099768	61.050817
2113.807507	95.791921	61.055822
2113.402502	91.862091	61.060826
2112.806560	100.402625	61.065831
2112.536798	98.561210	61.070836
2111.920339	90.184995	61.075841
2110.402540	100.754606	61.080846
2110.024901	100.265933	61.085850
2109.402082	91.567465	61.090855
2108.767944	92.540268	61.095860
2108.724148	94.988402	61.100865
2107.944055	87.672592	61.105870
2107.051542	86.101876	61.110874
2105.874211	97.738630	61.115879
2105.273750	98.833818	61.120884
2105.129871	92.073041	61.125889
2104.575520	95.628741	61.130894
2103.697327	94.213441	61.135898
2102.435368	96.334496	61.140903
2102.172343	103.642695	61.145908
2101.717276	97.685047	61.150913
2100.909711	97.761314	61.155918
2100.413404	87.587309	61.160922
2100.121260	88.521616	61.165927
2098.831322	101.912396	61.170932
2098.472026	92.380518	61.175937
2097.570681	98.045965	61.180942
2096.972169	94.370761	61.185946
2096.836594	90.626830	61.190951
2095.587743	97.291974	61.195956
2094.890412	86.877068	61.200961
2094.055865	101.712553	61.205966
2093.915819	86.667781	61.210970
2093.017674	97.503333	61.215975
2092.791510	99.483686	61.220980
2091.822517	91.125571	61.225985
2090.698036	86.461549	61.230990
2089.919567	94.289909	61.235994
2089.603051	96.652014	61.240999
2089.192035	95.700305	61.246004
2088.955371	87.416791	61.251009
2087.901849	89.351818	61.256014
2087.034902	90.377337	61.261018
2086.680226	86.359107	61.266023
2085.618258	95.508156	61.271028
2085.309851	89.338016	61.276033
2084.626708	86.800567	61.281038
2083.762765	80.188752	61.286042
2082.722325	91.035842	61.291047
2082.436431	90.660343	61.296052
2082.212041	90.601500	61.301057
2081.306632	87.618371	61.306062
2080.532718	86.752635	61.311066
2079.550613	91.530497	61.316071
2078.536337	97.065642	61.321076
2078.629717	93.649642	61.326081
2077.966817	91.657738	61.331086
2077.836885	86.249299	61.336090
2077.074887	93.537330	61.341095
2075.638604	88.992176	61.346100
2075.213420	88.375441	61.351105
2074.440759	94.387887	61.356110
2074.377599	97.520309	61.361114
2073.187062	79.081638	61.366119
2072.306690	88.741164	61.371124
2071.649665	92.228011	61.376129
2071.403948	88.356488	61.381134
2070.827922	84.436462	61.386138
2070.473777	86.531737	61.391143
2069.078107	95.973432	61.396148
2068.601423	89.893074	61.401153
2067.670283	83.645150	61.406158
2067.489470	89.275105	61.411162
2066.915862	94.180528	61.416167
2065.922281	89.686548	61.421172
2065.059225	81.902972	61.426177
2063.981791	88.548807	61.431182
2063.952562	92.631436	61.436186
2063.537122	89.146378	61.441191
2062.721947	93.601301	61.446196
2062.657468	80.041017	61.451201
2060.976204	91.639484	61.456206
2060.825714	80.007189	61.461210
2060.028458	83.513136	61.466215
2059.469971	83.628733	61.471220
2059.171898	89.311988	61.476225
2057.998719	93.382198	61.481230
2057.269022	83.674159	61.486234
2057.123975	93.095581	61.491239
2056.220505	87.417255	61.496244
2055.459853	82.867394	61.501249
2054.083461	91.990657	61.506254
2053.547724	89.456631	61.511258
2053.155222	81.177357	61.516263
2052.543978	87.727137	61.521268
2052.568352	88.500837	61.526273
2051.875690	89.407250	61.531278
2051.387040	87.835537	61.536282
2050.412658	94.925475	61.541287
2049.425808	88.509786	61.546292
2049.338696	84.324527	61.551297
2047.561353	91.540316	61.556302
2046.784135	86.609902	61.561306
2047.079813	85.760507	61.566311
2046.113087	93.759095	61.571316
2045.608598	84.433195	61.576321
2045.148450	97.665496	61.581326
2044.703708	95.661057	61.586330
2043.707964	79.722394	61.591335
2042.612391	99.762031	61.596340
2042.195360	95.666973	61.601345
2041.421965	91.220057	61.606350
2041.320827	86.481960	61.611354
2040.025124	89.464646	61.616359
2039.056785	93.123902	61.621364
2038.803496	83.986788	61.626369
2038.353538	89.290465	61.631374
2038.002140	93.577181	61.636378
2037.557982	85.112150	61.641383
2036.128186	105.617981	61.646388
2035.934254	89.432220	61.651393
2035.049666	90.868969	61.656398
2034.261700	83.633283	61.661402
2033.216879	81.098058	61.666407
2032.245694	89.139930	61.671412
2032.111798	97.903599	61.676417
2031.298117	97.250760	61.681422
2030.953255	97.892256	61.686426
2030.955293	88.883346	61.691431
2030.018073	95.336639	61.696436
2029.481063	75.551698	61.701441
2028.223764	88.429553	61.706446
2027.409279	85.291672	61.711450
2027.125330	84.628878	61.716455
2026.607354	89.610629	61.721460
2025.772108	76.816048	61.726465
2024.676922	88.375131	61.731470
2024.461024	77.456517	61.736474
2024.087420	81.169614	61.741479
2023.369544	88.710837	61.746484
2022.251036	87.032520	61.751489
2021.513512	90.710341	61.756494
2020.816410	85.488113	61.761498
2020.569925	79.798573	61.766503
2019.897319	68.622880	61.771508
2019.499479	84.775131	61.776513
2018.183799	83.434025	61.781518
2017.567712	82.593720	61.786522
2017.276008	87.481216	61.791527
2016.460535	77.211248	61.796532
2016.293497	75.150127	61.801537
2015.099900	88.260716	61.806542
2014.469061	83.001168	61.811546
2013.967603	77.353673	61.816551
2013.144916	83.650023	61.821556
2012.661525	78.674567	61.826561
2011.690081	91.057650	61.831566
2011.207684	81.468070	61.836570
2010.734678	85.066065	61.841575
2010.277667	87.483588	61.846580
2009.247042	75.543159	61.851585
2008.091249	86.290308	61.856590
2007.631746	85.019894	61.861594
2007.126336	84.152564	61.866599
2006.398971	85.640059	61.871604
2006.194850	88.072637	61.876609
2005.449918	88.769747	61.881614
2004.214731	92.761514	61.886618
2003.746066	86.701977	61.891623
2003.179858	82.652683	61.896628
2002.963965	86.730244	61.901633
2002.462826	96.859435	61.906638
2001.244066	84.723367	61.911642
2000.544432	80.996436	61.916647
1999.847428	96.341510	61.921652
1999.797542	99.345674	61.926657
1998.597020	76.431861	61.931662
1997.548464	93.035891	61.936666
1997.156030	91.743795	61.941671
1996.583284	88.294755	61.946676
1996.075198	80.950011	61.951681
1995.544360	91.883393	61.956686
1995.116023	91.423284	61.961690
1994.318474	85.961552	61.966695
1993.323665	90.949606	61.971700
1993.206540	86.193552	61.976705
1991.862413	92.189489	61.981710
1991.041203	89.588828	61.986714
1990.502288	89.116310	61.991719
1989.818597	94.329365	61.996724
1989.298809	94.785750	62.001729
1989.314594	92.982605	62.006734
1988.490935	78.541509	62.011738
1987.312433	97.785375	62.016743
1986.682615	94.903612	62.021748
1986.506877	69.326226	62.026753
1985.321096	100.246495	62.031758
1984.227743	85.203254	62.036762
1983.827762	82.944152	62.041767
1983.232015	85.771613	62.046772
1983.135552	84.606001	62.051777
1982.715482	89.740945	62.056782
1981.934276	83.294225	62.061786
1981.190337	83.302086	62.066791
1980.634697	88.294552	62.071796
1979.729668	87.585269	62.076801
1978.442273	90.662855	62.081806
1977.810939	92.630257	62.086810
1977.431953	80.389299	62.091815
1976.923313	82.709371	62.096820
1976.687040	93.432005	62.101825
1975.447466	90.744796	62.106830
1974.747177	84.466577	62.111834
1974.220211	87.782995	62.116839
1973.239126	90.253747	62.121844
1973.281772	81.386629	62.126849
1971.997587	89.654811	62.131854
1971.063999	83.093516	62.136858
1970.769332	80.156986	62.141863
1970.041014	85.238360	62.146868
1969.840498	84.778362	62.151873
1969.323441	86.812778	62.156878
1968.293923	86.728783	62.161882
1967.416729	81.959341	62.166887
1966.737933	85.530085	62.171892
1966.919405	90.544319	62.176897
1966.048299	97.118018	62.181902
1965.049785	82.482343	62.186906
1964.326111	83.685424	62.191911
1963.500736	88.260257	62.196916
1963.385492	76.953534	62.201921
1962.208897	94.867787	62.206926
1961.333672	77.205431	62.211930
1960.704959	74.071203	62.216935
1960.358024	86.832961	62.221940
1960.163014	83.656696	62.226945
1959.319894	79.652946	62.231950
1957.966720	88.007773	62.236954
1957.713924	93.917226	62.241959
1956.748278	86.247744	62.246964
1956.413306	81.519967	62.251969
1955.847478	87.146383	62.256974
1955.271055	93.258588	62.261978
1954.357250	78.067029	62.266983
1953.459963	89.547414	62.271988
1953.656414	78.068219	62.276993
1952.942868	82.697838	62.281998
1951.639571	79.098282	62.287002
1951.053348	74.550732	62.292007
1950.303389	90.153357	62.297012
1949.949169	77.869056	62.302017
1948.974938	85.156106	62.307022
1947.996327	85.387299	62.312026
1947.684799	80.045548	62.317031
1946.976389	81.298247	62.322036
1946.746704	82.735141	62.327041
1946.673175	86.715992	62.332046
1945.288284	79.786397	62.337050
1944.496655	85.710421	62.342055
1943.843935	85.434165	62.347060
1943.161763	79.966754	62.352065
1942.300163	80.452176	62.357070
1941.537919	81.109476	62.362074
1940.979965	74.272538	62.367079
1940.420775	84.879275	62.372084
1940.194047	71.888799	62.377089
1939.761830	83.166054	62.382094
1938.445534	80.762268	62.387098
1937.792670	66.424978	62.392103
1937.050582	85.774598	62.397108
1936.990862	77.557642	62.402113
1936.067911	78.270414	62.407118
1935.078592	74.934827	62.412122
1934.415584	78.480993	62.417127
1933.823803	82.463689	62.422132
1933.527270	78.734289	62.427137
1933.219275	75.561772	62.432142
1932.214251	84.219295	62.437146
1931.649531	79.594222	62.442151
1930.649314	85.967657	62.447156
1929.662002	79.648289	62.452161
1928.857893	87.176410	62.457166
1928.232295	86.389673	62.462170
1928.232657	79.303266	62.467175
1927.455881	85.281703	62.472180
1927.343677	81.247088	62.477185
1926.048233	76.690708	62.482190
1925.466534	75.412902	62.487194
1924.886546	70.924292	62.492199
1924.219397	82.683521	62.497204
1922.965739	85.219636	62.502209
1922.274919	88.650379	62.507214
1921.258878	94.815030	62.512218
1921.446801	86.852059	62.517223
1921.125659	91.186018	62.522228
1921.032180	81.205157	62.527233
1919.659307	90.692177	62.532238
1918.833455	89.533550	62.537242
1918.330259	85.166782	62.542247
1917.149279	84.756782	62.547252
1916.282751	86.099243	62.552257
1915.446490	88.911284	62.557262
1915.061101	89.742146	62.562266
1914.986369	85.606969	62.567271
1914.406898	93.474735	62.572276
1914.099517	81.340693	62.577281
1913.215960	84.854072	62.582286
1912.314640	90.383951	62.587290
1911.839126	84.580980	62.592295
1910.537090	86.492450	62.597300
1909.761328	84.854387	62.602305
1908.952983	94.611324	62.607310
1908.498764	86.445955	62.612314
1908.609678	83.071327	62.617319
1908.012744	100.004217	62.622324
1907.377492	89.081230	62.627329
1906.267554	90.121728	62.632334
1905.421811	91.202284	62.637338
1904.965946	83.678970	62.642343
1904.042701	94.493315	62.647348
1903.476371	93.101113	62.652353
1902.747990	88.837902	62.657358
1902.168097	91.817398	62.662362
1901.693531	82.138301	62.667367
1901.160015	92.677896	62.672372
1900.480830	87.355095	62.677377
1899.512979	82.997446	62.682382
1898.915539	88.302475	62.687386
1898.803080	79.087844	62.692391
1897.387865	88.310370	62.697396
1896.401613	91.942555	62.702401
1896.025379	87.074687	62.707406
1895.929715	86.035103	62.712410
1895.349241	83.710057	62.717415
1894.474777	86.074028	62.722420
1893.591888	80.666881	62.727425
1893.140172	92.439227	62.732430
1892.538555	84.194766	62.737434
1892.036236	80.509080	62.742439
1890.672676	90.628540	62.747444
1890.615393	83.109759	62.752449
1889.781423	80.189476	62.757454
1889.111060	91.463547	62.762458
1888.358356	83.703524	62.767463
1887.319169	85.464471	62.772468
1887.058994	80.332188	62.777473
1886.613921	82.694220	62.782478
1886.149452	85.188636	62.787482
1885.307442	75.813876	62.792487
1883.981070	85.709822	62.797492
1883.793917	81.373310	62.802497
1883.301616	83.099472	62.807502
1882.522571	84.795468	62.812506
1881.943887	82.955822	62.817511
1881.319445	91.313256	62.822516
1880.479997	81.837167	62.827521
1880.187009	75.398131	62.832526
1878.966197	84.779025	62.837530
1878.302764	88.120278	62.842535
1877.726706	79.838652	62.847540
1877.603538	78.161645	62.852545
1876.502847	81.107137	62.857550
1875.422120	81.827633	62.862554
1875.025979	87.288357	62.867559
1874.068479	92.409293	62.872564
1873.982169	92.156666	62.877569
1873.700074	85.417865	62.882574
1872.514166	91.171126	62.887578
1871.568120	81.451779	62.892583
1870.805821	90.860805	62.897588
1870.676526	89.140617	62.902593
1870.331051	85.701258	62.907598
1869.497948	81.025775	62.912602
1868.667370	88.714224	62.917607
1868.018247	89.743075	62.922612
1867.346069	74.046446	62.927617
1866.174063	84.957055	62.932622
1865.654098	89.478695	62.937626
1865.127077	86.022430	62.942631
1864.632447	78.305020	62.947636
1864.243432	86.085782	62.952641
1863.772275	85.131045	62.957646
1862.397171	90.122753	62.962650
1861.790218	88.295483	62.967655
1861.287498	93.475101	62.972660
1860.662052	92.289405	62.977665
1860.176191	82.512769	62.982670
1859.236482	72.032372	62.987674
1858.816229	80.486689	62.992679
1857.917434	92.670625	62.997684
1857.424933	92.969746	63.002689
1856.293443	78.713199	63.007694
1855.546179	91.604749	63.012698
1855.193545	88.488212	63.017703
1854.966444	82.502320	63.022708
1854.437791	80.334630	63.027713
1854.107044	82.022532	63.032718
1852.806387	96.962014	63.037722
1852.732861	79.850486	63.042727
1851.440299	82.542613	63.047732
1850.528954	79.584169	63.052737
1849.968500	85.173479	63.057742
1849.285584	88.368029	63.062746
1849.266990	77.023904	63.067751
1847.680335	84.127534	63.072756
1847.069484	84.566867	63.077761
1846.570443	89.853129	63.082766
1846.314459	87.199044	63.087770
1846.003653	80.483732	63.092775
1844.828608	74.484357	63.097780
1843.940959	86.718559	63.102785
1843.669950	80.077350	63.107790
1843.080836	76.858022	63.112794
1842.559151	83.491380	63.117799
1841.734175	87.910071	63.122804
1840.819665	78.018584	63.127809
1840.276996	76.632103	63.132814
1838.940389	83.380660	63.137818
1838.313970	72.617151	63.142823
1837.554490	91.715669	63.147828
1837.408688	78.337064	63.152833
1837.208304	83.564868	63.157838
1836.685698	89.137134	63.162842
1836.014018	92.206906	63.167847
1835.230764	86.982648	63.172852
1834.290100	78.825157	63.177857
1833.611209	73.546488	63.182862
1832.763313	81.035851	63.187866
1831.986801	74.336144	63.192871
1831.306457	83.721122	63.197876
1830.759068	86.430553	63.202881
1830.353176	77.607861	63.207886
1830.031770	85.141358	63.212890
1829.086330	79.916049	63.217895
1828.214932	78.876643	63.222900
1827.733640	72.303521	63.227905
1827.246330	73.607872	63.232910
1826.149768	83.957760	63.237914
1825.546515	84.848457	63.242919
1824.712913	92.531091	63.247924
1824.330517	79.246823	63.252929
1824.348846	72.942861	63.257934
1822.638533	79.298196	63.262938
1822.102034	81.113384	63.267943
1821.351439	74.434796	63.272948
1820.921689	91.224444	63.277953
1821.025897	79.865553	63.282958
1819.647226	85.912778	63.287962
1819.280935	70.648553	63.292967
1818.485440	83.490992	63.297972
1817.880462	80.824521	63.302977
1816.854081	83.876503	63.307982
1815.627281	87.598947	63.312986
1815.161763	80.214380	63.317991
1814.427261	89.650539	63.322996
1814.451188	83.574333	63.328001
1814.105506	80.035673	63.333006
1813.562952	84.852629	63.338010
1813.358690	81.073905	63.343015
1812.104736	91.142879	63.348020
1811.475560	85.984046	63.353025
1810.392766	81.878064	63.358030
1809.263039	87.302320	63.363034
1809.104555	83.853779	63.368039
1808.697364	80.829490	63.373044
1808.179485	84.376293	63.378049
1807.007708	73.904385	63.383054
1806.104598	78.190416	63.388058
1805.769609	77.767553	63.393063
1805.020125	81.980308	63.398068
1804.804170	72.296450	63.403073
1803.963783	74.889990	63.408078
1802.832409	84.753427	63.413082
1802.647168	73.331699	63.418087
1802.024010	72.806369	63.423092
1801.544648	89.575508	63.428097
1800.351885	74.901393	63.433102
1799.389819	75.883762	63.438106
1799.227649	67.462333	63.443111
1798.745880	79.182677	63.448116
1798.068336	78.967168	63.453121
1797.245924	75.538905	63.458126
1796.254949	82.406053	63.463130
1796.190319	69.908666	63.468135
1795.096778	75.421790	63.473140
1794.648556	64.328822	63.478145
1793.857538	77.440195	63.483150
1792.817324	79.944051	63.488154
1792.593093	79.716482	63.493159
1792.101377	79.171859	63.498164
1791.586732	72.933610	63.503169
1791.309171	72.643549	63.508174
1789.797125	81.526696	63.513178
1789.512306	71.708703	63.518183
1788.924303	85.811242	63.523188
1787.836632	74.428743	63.528193
1787.214032	73.157464	63.533198
1786.410750	79.408210	63.538202
1786.541376	76.506670	63.543207
1785.388995	76.109535	63.548212
1784.428624	74.679015	63.553217
1784.043689	78.474356	63.558222
1783.350105	77.165466	63.563226
1783.162823	75.719410	63.568231
1782.131998	79.666200	63.573236
1781.023216	76.713906	63.578241
1780.524646	65.464941	63.583246
1780.043029	77.672516	63.588250
1779.842578	75.659298	63.593255
1778.950534	84.590646	63.598260
1778.272163	80.795755	63.603265
1777.849949	78.275305	63.608270
1776.973478	82.913491	63.613274
1776.084090	84.116129	63.618279
1775.203233	75.512373	63.623284
1774.571111	85.020584	63.628289
1774.456843	81.192881	63.633294
1773.541118	88.114318	63.638298
1772.770476	74.262548	63.643303
1771.654969	85.963695	63.648308
1771.514272	76.157507	63.653313
1771.166303	69.402387	63.658318
1770.197259	85.613803	63.663322
1769.168291	78.183114	63.668327
1768.458789	82.443142	63.673332
1768.128014	77.637466	63.678337
1767.878440	69.843326	63.683342
1767.343560	85.071205	63.688346
1766.273711	80.524815	63.693351
1765.604936	88.406780	63.698356
1765.158592	89.540642	63.703361
1763.881179	81.067668	63.708366
1763.219437	84.530097	63.713370
1762.553332	78.437325	63.718375
1762.117391	87.457090	63.723380
1761.782280	82.402955	63.728385
1761.535537	71.580757	63.733390
1760.399759	83.654113	63.738394
1759.635241	75.560143	63.743399
1759.231593	80.444929	63.748404
1758.819693	81.043490	63.753409
1758.150640	76.338844	63.758414
1756.930171	88.033011	63.763418
1756.470366	80.996042	63.768423
1755.052083	78.982271	63.773428
1754.627294	77.980769	63.778433
1754.301576	82.354887	63.783438
1753.589217	89.813287	63.788442
1753.646727	85.083137	63.793447
1752.698136	86.033423	63.798452
1751.721345	84.942974	63.803457
1751.126899	68.619074	63.808462
1750.335615	78.767543	63.813466
1749.291092	78.335950	63.818471
1748.103885	83.280523	63.823476
1747.800498	74.987175	63.828481
1747.432658	79.151948	63.833486
1746.960480	93.395367	63.838490
1747.027625	84.013466	63.843495
1746.352359	80.722693	63.848500
1745.434146	87.958332	63.853505
1744.903579	63.817162	63.858510
1743.715937	90.000790	63.863514
1742.813178	82.553222	63.868519
1742.051926	82.715281	63.873524
1741.788028	76.795173	63.878529
1741.299899	76.680478	63.883534
1740.733464	81.414509	63.888538
1739.922485	71.120296	63.893543
1738.848857	82.568806	63.898548
1737.989768	88.598205	63.903553
1737.931935	80.149169	63.908558
1737.641790	79.187786	63.913562
1736.886416	76.704486	63.918567
1735.775299	80.317131	63.923572
1735.066361	87.707185	63.928577
1734.807120	74.751879	63.933582
1733.589836	87.522557	63.938586
1733.173880	77.589787	63.943591
1732.366079	75.606802	63.948596
1732.022694	87.549594	63.953601
1731.678787	81.631155	63.958606
1730.140912	88.954173	63.963610
1729.852086	89.126357	63.968615
1729.280155	79.871187	63.973620
1728.664984	82.659207	63.978625
1727.999928	80.200987	63.983630
1727.498830	90.481569	63.988634
1726.856001	85.443197	63.993639
1725.820562	87.678250	63.998644
1724.933387	81.664753	64.003649
1723.951084	77.404087	64.008654
1723.668093	76.216075	64.013658
1723.583565	74.649631	64.018663
1723.244981	86.812423	64.023668
1722.098727	83.512885	64.028673
1721.170371	78.996081	64.033678
1720.694466	85.339924	64.038682
1720.360686	83.393615	64.043687
1719.489423	84.412052	64.048692
1718.351264	83.194288	64.053697
1717.873751	78.311006	64.058702
1717.295876	91.193018	64.063706
1717.116293	86.298684	64.068711
1716.020463	91.854781	64.073716
1715.245412	86.410077	64.078721
1714.423163	85.955810	64.083726
1713.922551	85.625494	64.088730
1713.875808	74.691118	64.093735
1712.818055	81.035911	64.098740
1712.040429	76.410022	64.103745
1711.552510	82.352091	64.108750
1710.585918	81.785139	64.113754
1709.636707	87.223338	64.118759
1708.961991	71.560298	64.123764
1708.372694	84.395236	64.128769
1707.982013	78.558345	64.133774
1707.476585	76.855334	64.138778
1707.290244	77.246198	64.143783
1706.735388	82.672222	64.148788
1705.523624	83.091916	64.153793
1704.918513	83.229186	64.158798
1704.296531	85.929988	64.163802
1703.714438	77.931637	64.168807
1702.880539	88.394382	64.173812
1702.333444	78.977588	64.178817
1701.175624	78.541933	64.183822
1700.047607	78.345961	64.188826
1699.960891	75.143065	64.193831
1699.283624	82.066067	64.198836
1698.684343	85.222136	64.203841
1698.597937	78.442829	64.208846
1697.770115	91.553768	64.213850
1697.145264	80.621328	64.218855
1696.659933	80.853111	64.223860
1695.628376	89.976944	64.228865
1694.529962	82.295557	64.233870
1693.808489	81.639219	64.238874
1693.472493	75.687996	64.243879
1692.839856	87.150053	64.248884
1692.436328	81.573813	64.253889
1692.587293	84.404149	64.258894
1691.238713	85.299722	64.263898
1690.339431	81.178840	64.268903
1689.559494	83.352825	64.273908
1688.506868	85.935959	64.278913
1688.258634	78.195230	64.283918
1687.713707	96.662051	64.288922
1687.213595	90.746352	64.293927
1686.172729	86.105512	64.298932
1685.017447	88.241350	64.303937
1684.909217	79.730943	64.308942
1684.277545	88.543693	64.313946
1683.690931	76.334224	64.318951
1683.416860	77.295662	64.323956
1682.291064	81.410530	64.328961
1681.996745	83.838529	64.333966
1681.531480	84.205892	64.338970
1680.664428	84.181356	64.343975
1679.817136	81.575485	64.348980
1678.845783	84.823771	64.353985
1678.384181	77.793417	64.358990
1677.440984	82.527380	64.363994
1676.655493	80.171879	64.368999
1676.260493	85.365947	64.374004
1675.569141	78.373662	64.379009
1675.352278	75.347551	64.384014
1674.977190	81.456197	64.389018
1673.615860	78.307535	64.394023
1672.702813	88.376023	64.399028
1672.291944	80.959158	64.404033
1672.007160	70.836849	64.409038
1671.400057	89.129042	64.414042
1670.597085	85.341359	64.419047
1669.589382	85.957304	64.424052
1669.530791	81.813276	64.429057
1668.663224	88.897395	64.434062
1667.390923	83.957450	64.439066
1667.012027	75.977296	64.444071
1666.690258	86.483273	64.449076
1665.596706	87.317850	64.454081
1665.660879	74.304882	64.459086
1664.467512	80.329051	64.464090
1663.916948	81.993545	64.469095
1663.426149	88.199419	64.474100
1662.315241	77.456159	64.479105
1661.696210	79.700783	64.484110
1660.928342	89.309418	64.489114
1660.737383	80.632390	64.494119
1660.122000	82.330835	64.499124
1659.054383	93.046749	64.504129
1658.710408	80.667862	64.509134
1657.798721	89.444675	64.514138
1657.585857	71.700928	64.519143
1656.661530	88.452441	64.524148
1655.476885	86.970866	64.529153
1655.265664	78.552513	64.534158
1654.361105	84.641193	64.539162
1654.549130	75.383599	64.544167
1653.820843	77.905764	64.549172
1652.675807	81.700440	64.554177
1652.431308	72.128372	64.559182
1650.913383	85.957610	64.564186
1650.133797	73.636889	64.569191
1649.447514	79.668819	64.574196
1648.815435	74.423772	64.579201
1649.106798	76.995269	64.584206
1648.439136	82.166421	64.589210
1647.811817	75.309049	64.594215
1646.941941	81.122573	64.599220
1646.240427	95.340928	64.604225
1645.486834	77.854951	64.609230
1644.278636	81.752700	64.614234
1643.546439	80.336448	64.619239
1643.042877	84.237377	64.624244
1642.626304	78.760988	64.629249
1642.532500	77.032025	64.634254
1641.476204	80.738496	64.639258
1640.853403	70.190517	64.644263
1640.284936	72.398728	64.649268
1639.510957	82.744735	64.654273
1639.025356	78.717425	64.659278
1637.920420	82.835304	64.664282
1637.473230	74.679935	64.669287
1637.142285	84.897223	64.674292
1635.686415	72.685516	64.679297
1635.637508	73.775186	64.684302
1634.711837	87.809957	64.689306
1634.120432	84.420743	64.694311
1633.805008	77.967969	64.699316
1632.247388	74.571405	64.704321
1631.933413	72.765460	64.709326
1631.230686	82.720123	64.714330
1630.848503	77.386501	64.719335
1630.586999	61.948010	64.724340
1629.711469	65.926949	64.729345
1628.877886	85.269047	64.734350
1628.068632	75.214291	64.739354
1627.747189	76.659476	64.744359
1626.660546	70.592559	64.749364
1625.743423	68.658514	64.754369
1625.819183	67.270030	64.759374
1625.185223	79.949648	64.764378
1624.570249	71.945511	64.769383
1623.593442	82.793651	64.774388
1622.665067	87.996765	64.779393
1622.692670	78.796193	64.784398
1621.478700	79.930601	64.789402
1620.502790	76.405366	64.794407
1619.895529	80.977176	64.799412
1619.174709	84.262949	64.804417
1619.285362	77.843412	64.809422
1618.511016	89.540870	64.814426
1617.942185	76.283129	64.819431
1617.094948	79.141152	64.824436
1616.250802	83.536139	64.829441
1616.074184	65.651042	64.834446
1614.723227	78.718939	64.839450
1614.414775	75.437740	64.844455
1613.886454	76.627224	64.849460
1613.346409	78.807272	64.854465
1612.397139	70.416298	64.859470
1611.310681	73.570932	64.864474
1610.724450	74.296553	64.869479
1610.643786	84.997604	64.874484
1609.961348	77.418905	64.879489
1608.811477	69.201721	64.884494
1608.032703	75.268850	64.889498
1607.206003	79.405613	64.894503
1607.040340	86.565888	64.899508
1606.424173	84.839491	64.904513
1606.134437	78.701170	64.909518
1604.781984	87.346178	64.914522
1604.393206	81.554735	64.919527
1604.330637	87.208483	64.924532
1602.474675	94.637293	64.929537
1602.192216	80.591349	64.934542
1601.332806	81.535405	64.939546
1601.044064	77.013227	64.944551
1600.658508	72.567930	64.949556
1600.109884	94.036131	64.954561
1599.561761	78.095989	64.959566
1598.546583	87.084790	64.964570
1598.098562	80.383441	64.969575
1597.226716	85.919764	64.974580
1595.968074	96.678662	64.979585
1595.782598	68.029627	64.984590
1594.948946	71.628205	64.989594
1594.583064	70.322498	64.994599
1594.267670	69.552792	64.999604
1593.048861	85.846497	65.004609
1592.604178	85.296018	65.009614
1591.778821	72.004932	65.014618
1591.418910	86.514349	65.019623
1590.556316	100.458700	65.024628
1589.534266	86.413564	65.029633
1589.297783	79.155088	65.034638
1588.978672	75.337871	65.039642
1588.119138	72.245147	65.044647
1587.437822	77.421633	65.049652
1586.758508	83.917648	65.054657
1586.217068	82.158885	65.059662
1585.127920	76.650598	65.064666
1584.427473	76.050872	65.069671
1584.180691	73.228212	65.074676
1583.330585	73.909034	65.079681
1582.628115	67.069934	65.084686
1581.579149	80.851498	65.089690
1581.420418	71.964375	65.094695
1580.931449	70.862720	65.099700
1579.687959	69.445722	65.104705
1579.034596	78.916332	65.109710
1578.137047	83.203126	65.114714
1577.961086	68.127926	65.119719
1577.976195	74.120969	65.124724
1576.945225	81.186916	65.129729
1576.207992	78.618788	65.134734
1575.418372	69.095500	65.139738
1574.792418	80.547043	65.144743
1573.746114	87.277979	65.149748
1572.817992	86.384861	65.154753
1572.722263	77.706912	65.159758
1572.249694	83.480988	65.164762
1571.509234	79.008506	65.169767
1570.771430	74.243882	65.174772
1569.838831	83.891319	65.179777
1569.181606	80.028480	65.184782
1568.915828	81.187298	65.189786
1568.557949	79.661137	65.194791
1567.606511	78.744919	65.199796
1566.388368	78.853470	65.204801
1565.966267	70.299916	65.209806
1565.732339	80.970120	65.214810
1564.807914	80.147378	65.219815
1564.310620	74.978708	65.224820
1563.612377	85.481424	65.229825
1563.188800	72.347279	65.234830
1561.447959	74.483166	65.239834
1561.070955	70.910108	65.244839
1560.867539	70.141537	65.249844
1560.039170	77.850201	65.254849
1560.023821	74.093531	65.259854
1559.097493	78.074257	65.264858
1558.292063	75.263093	65.269863
1557.708752	70.038711	65.274868
1556.954053	70.489928	65.279873
1555.995184	67.291581	65.284878
1555.179646	76.097288	65.289882
1554.511723	76.127884	65.294887
1554.613736	69.682918	65.299892
1553.810772	83.048532	65.304897
1552.307579	74.925357	65.309902
1551.747078	81.755721	65.314906
1551.311745	72.825822	65.319911
1550.999598	73.495293	65.324916
1550.743283	68.439721	65.329921
1550.303625	76.004628	65.334926
1549.138531	86.630406	65.339930
1548.430789	79.968760	65.344935
1547.345901	80.253256	65.349940
1546.685617	78.704188	65.354945
1545.976727	70.694499	65.359950
1545.535314	75.351928	65.364954
1545.197579	76.929015	65.369959
1544.892208	87.224240	65.374964
1543.453839	68.588780	65.379969
1543.174306	73.893813	65.384974
1542.812342	70.584860	65.389978
1542.065680	70.158061	65.394983
1540.844787	50.552985	65.399988
1540.360585	86.533942	65.404993
1540.103915	69.006916	65.409998
1538.926104	75.432340	65.415002
1538.057480	73.539504	65.420007
1537.691464	56.520277	65.425012
1537.050896	74.221714	65.430017
1536.399334	71.949054	65.435022
1535.209524	51.895940	65.440026
1534.736044	77.247050	65.445031
1534.571355	73.124623	65.450036
1533.710306	70.971978	65.455041
1533.614221	56.046527	65.460046
1532.455329	62.453173	65.465050
1531.568722	64.273584	65.470055
1531.331477	64.532206	65.475060
1530.434209	71.960100	65.480065
1529.690863	68.472064	65.485070
1528.828665	89.840279	65.490074
1528.262144	64.952753	65.495079
1528.142422	73.428718	65.500084
1527.306499	73.626357	65.505089
1526.214667	60.465959	65.510094
1525.439010	81.132893	65.515098
1525.041875	75.301799	65.520103
1524.753698	57.748261	65.525108
1523.948301	76.299020	65.530113
1522.931364	78.226871	65.535118
1522.371162	72.984635	65.540122
1521.995145	65.593814	65.545127
1521.827021	67.940274	65.550132
1520.457114	74.460880	65.555137
1520.145138	71.870927	65.560142
1519.787888	70.824045	65.565146
1518.173093	78.375420	65.570151
1517.565474	74.848474	65.575156
1517.296298	63.919518	65.580161
1516.728312	90.372132	65.585166
1516.442219	72.171728	65.590170
1514.937018	75.774541	65.595175
1514.349036	79.146459	65.600180
1513.430662	81.467063	65.605185
1513.481361	67.670977	65.610190
1512.916194	76.839012	65.615194
1511.913111	64.106042	65.620199
1511.497361	59.843751	65.625204
1510.804895	73.786286	65.630209
1510.114015	75.397416	65.635214
1508.899591	72.493572	65.640218
1508.196883	57.273455	65.645223
1508.012842	71.344922	65.650228
1507.311843	65.338205	65.655233
1507.049606	70.621568	65.660238
1505.928159	69.672468	65.665242
1505.443196	70.353636	65.670247
1504.919214	69.937193	65.675252
1504.229528	74.750767	65.680257
1503.182972	70.867819	65.685262
1502.201177	76.271832	65.690266
1502.028475	73.795362	65.695271
1501.456032	74.812115	65.700276
1500.749958	80.270083	65.705281
1499.744205	77.303123	65.710286
1499.377926	73.255308	65.715290
1498.709956	75.004720	65.720295
1498.660923	65.805306	65.725300
1497.494669	76.357166	65.730305
1496.615539	73.392163	65.735310
1495.985241	80.780801	65.740314
1495.479038	85.141043	65.745319
1495.128306	70.590349	65.750324
1493.661125	75.287790	65.755329
1493.685907	72.816207	65.760334
1493.250740	71.363838	65.765338
1492.055934	79.307359	65.770343
1491.412132	63.734122	65.775348
1490.476281	78.488009	65.780353
1490.337533	73.626639	65.785358
1489.940025	68.514670	65.790362
1488.808177	77.946216	65.795367
1488.304889	69.859725	65.800372
1487.338236	76.688409	65.805377
1487.097436	66.928142	65.810382
1486.157175	82.819660	65.815386
1485.093791	68.637673	65.820391
1484.741986	61.960493	65.825396
1484.080743	66.659167	65.830401
1484.350464	72.947617	65.835406
1482.917259	71.649120	65.840410
1481.826447	79.200822	65.845415
1481.603837	73.550152	65.850420
1480.987734	63.879490	65.855425
1480.490348	67.375779	65.860430
1479.357665	73.223225	65.865434
1478.843780	70.692172	65.870439
1478.566021	68.539890	65.875444
1477.917811	77.741626	65.880449
1476.841840	73.417108	65.885454
1476.066458	77.938394	65.890458
1475.487388	66.814276	65.895463
1475.304781	69.464222	65.900468
1474.008744	82.679558	65.905473
1473.532153	75.809327	65.910478
1472.962825	75.387481	65.915482
1472.469805	69.210535	65.920487
1472.254334	67.663336	65.925492
1470.834132	76.024285	65.930497
1470.380412	69.894707	65.935502
1469.982270	72.038039	65.940506
1468.760414	70.994531	65.945511
1468.333202	69.398984	65.950516
1467.325514	72.823416	65.955521
1467.161850	63.547613	65.960526
1466.507591	70.202081	65.965530
1465.378708	69.842355	65.970535
1464.863638	69.807684	65.975540
1464.249052	63.536526	65.980545
1463.775252	66.142867	65.985550
1463.478039	66.824166	65.990554
1462.458744	71.751627	65.995559
1461.739568	71.293677	66.000564
1460.963135	71.328927	66.005569
1460.661196	66.767874	66.010574
1459.822581	68.555451	66.015578
1458.757981	75.142677	66.020583
1458.417554	69.945953	66.025588
1457.718288	77.209944	66.030593
1457.642411	57.820320	66.035598
1456.023535	60.853054	66.040602
1455.377282	69.731219	66.045607
1455.142610	79.319801	66.050612
1454.628740	73.179286	66.055617
1454.240459	49.898714	66.060622
1453.584752	82.422014	66.065626
1452.553828	64.740537	66.070631
1452.021106	67.319975	66.075636
1450.739975	56.414676	66.080641
1450.193520	69.883025	66.085646
1449.853764	58.118524	66.090650
1449.119101	65.090108	66.095655
1449.140200	54.536066	66.100660
1448.157327	74.561028	66.105665
1447.592656	67.860916	66.110670
1447.199846	50.853867	66.115674
1445.592730	79.691838	66.120679
1445.233450	60.913350	66.125684
1444.213169	70.018108	66.130689
1444.221112	66.986260	66.135694
1443.296055	62.759196	66.140698
1441.939434	70.793099	66.145703
1441.691363	66.587746	66.150708
1441.261976	76.481648	66.155713
1440.731343	48.658659	66.160718
1440.420382	70.864870	66.165722
1439.353082	63.151872	66.170727
1438.807069	59.883229	66.175732
1438.123956	66.401945	66.180737
1437.480549	59.922500	66.185742
1436.738418	68.379111	66.190746
1435.753720	68.341818	66.195751
1435.376681	65.342771	66.200756
1434.892927	67.045574	66.205761
1433.649211	62.982693	66.210766
1432.959433	65.366334	66.215770
1432.348916	56.869576	66.220775
1432.090673	69.962553	66.225780
1431.483140	73.082138	66.230785
1430.684744	73.144541	66.235790
1430.057503	71.388414	66.240794
1428.983666	63.151361	66.245799
1428.966395	77.226282	66.250804
1428.441868	75.591018	66.255809
1427.531129	63.478897	66.260814
1427.009580	74.713596	66.265818
1426.105547	70.448504	66.270823
1425.522025	65.148505	66.275828
1424.434902	79.577959	66.280833
1424.098283	56.331754	66.285838
1423.415399	57.028625	66.290842
1422.881851	79.640789	66.295847
1422.193051	64.492605	66.300852
1421.102267	68.376513	66.305857
1420.713761	72.263918	66.310862
1420.333830	74.328672	66.315866
1419.648802	76.438763	66.320871
1418.844775	74.589317	66.325876
1417.985166	82.511129	66.330881
1417.448018	76.486280	66.335886
1417.063576	69.268700	66.340890
1416.156941	75.248969	66.345895
1415.579083	63.911804	66.350900
1414.879916	68.868820	66.355905
1414.298315	61.969571	66.360910
1413.623603	70.210479	66.365914
1412.599958	70.494759	66.370919
1412.340148	72.988254	66.375924
1411.652399	66.873812	66.380929
1411.011817	70.571058	66.385934
1410.040038	61.161948	66.390938
1409.089601	69.058769	66.395943
1409.031179	59.871901	66.400948
1408.314968	66.507841	66.405953
1408.164967	72.000439	66.410958
1406.956904	73.217582	66.415962
1406.321683	80.611747	66.420967
1405.851895	66.892095	66.425972
1404.484988	76.174959	66.430977
1403.702699	65.717070	66.435982
1403.254592	60.725122	66.440986
1402.957804	78.329354	66.445991
1403.151380	75.055122	66.450996
1402.236219	74.238852	66.456001
1401.323100	63.514769	66.461006
1400.697419	69.521343	66.466010
1399.337223	73.055442	66.471015
1399.007640	67.160028	66.476020
1398.144298	66.034341	66.481025
1397.873022	67.332813	66.486030
1397.338726	72.613694	66.491034
1396.187314	72.503571	66.496039
1395.759102	71.523177	66.501044
1395.147507	69.871799	66.506049
1394.615604	75.264260	66.511054
1393.640842	70.549976	66.516058
1392.455046	68.616148	66.521063
1392.463046	64.874700	66.526068
1391.810879	68.890743	66.531073
1391.562306	71.786132	66.536078
1390.409640	81.091718	66.541082
1389.562463	78.506433	66.546087
1389.515353	71.422888	66.551092
1388.333866	83.483123	66.556097
1387.753873	79.901361	66.561102
1386.797858	82.212222	66.566106
1386.190940	79.736974	66.571111
1386.009683	77.419561	66.576116
1385.392801	73.919355	66.581121
1384.197210	67.083015	66.586126
1384.012996	69.868832	66.591130
1383.361472	76.071898	66.596135
1382.945170	66.410508	66.601140
1381.495251	77.136800	66.606145
1380.759316	63.011633	66.611150
1380.611638	64.408725	66.616154
1380.056974	68.398234	66.621159
1379.435405	72.660139	66.626164
1378.441655	73.308669	66.631169
1377.714827	74.561289	66.636174
1377.247040	67.262354	66.641178
1376.204230	80.864805	66.646183
1375.731115	64.900228	66.651188
1375.096033	75.400810	66.656193
1374.673802	73.520652	66.661198
1374.550396	76.605871	66.666202
1373.073818	70.176881	66.671207
1372.612218	67.172365	66.676212
1371.981618	78.966849	66.681217
1371.500061	68.372864	66.686222
1370.297135	75.314829	66.691226
1369.350090	74.140958	66.696231
1368.963336	71.250694	66.701236
1368.538476	70.280810	66.706241
1368.170948	75.476843	66.711246
1368.014757	67.466095	66.716250
1366.629778	74.302965	66.721255
1366.018573	74.116447	66.726260
1365.242912	76.275650	66.731265
1364.752241	67.122801	66.736270
1363.920789	67.617811	66.741274
1362.912517	66.251836	66.746279
1362.799919	65.380543	66.751284
1362.313370	74.184455	66.756289
1361.828699	79.523684	66.761294
1360.673440	67.704337	66.766298
1359.976564	70.227889	66.771303
1359.631438	60.739690	66.776308
1358.537071	72.658351	66.781313
1357.729673	73.352956	66.786318
1357.518422	68.785388	66.791322
1356.477639	77.059271	66.796327
1356.740209	62.794314	66.801332
1355.459617	74.739427	66.806337
1354.898271	75.361806	66.811342
1354.472982	62.084512	66.816346
1353.014356	71.569622	66.821351
1352.714994	64.704369	66.826356
1352.107154	77.496549	66.831361
1351.564317	69.939906	66.836366
1351.002279	64.191835	66.841370
1349.832991	72.527144	66.846375
1349.385696	70.911158	66.851380
1348.639219	79.841546	66.856385
1348.527451	73.391147	66.861390
1347.594422	64.228204	66.866394
1346.339075	72.156169	66.871399
1346.239080	73.294961	66.876404
1345.683032	76.488377	66.881409
1345.104890	71.613299	66.886414
1344.298789	67.982344	66.891418
1343.227292	77.055856	66.896423
1343.217587	73.473332	66.901428
1341.983032	73.521523	66.906433
1341.229579	73.237781	66.911438
1340.631277	75.994815	66.916442
1339.874778	80.338100	66.921447
1339.807221	68.919837	66.926452
1339.282099	73.040268	66.931457
1338.241717	70.372181	66.936462
1337.942955	70.088695	66.941466
1337.011564	75.295525	66.946471
1336.792122	74.505868	66.951476
1335.784949	71.774159	66.956481
1334.653251	76.052517	66.961486
1334.454468	77.449852	66.966490
1332.828590	85.206510	66.971495
1332.510120	74.498301	66.976500
1331.721564	82.218038	66.981505
1331.160393	77.140001	66.986510
1330.905084	71.805196	66.991514
1330.384728	78.676513	66.996519
1330.814639	69.967077	67.001524
1329.532927	75.289520	67.006529
1328.465374	68.639427	67.011534
1328.227323	68.164950	67.016538
1326.483257	75.300186	67.021543
1325.908780	69.336490	67.026548
1325.709203	69.475608	67.031553
1325.293011	78.514333	67.036558
1324.822096	71.266368	67.041562
1323.450171	78.198950	67.046567
1323.126475	68.002486	67.051572
1322.701675	62.816050	67.056577
1321.508929	69.854178	67.061582
1321.074723	62.805376	67.066586
1320.362213	71.959010	67.071591
1319.645882	70.168192	67.076596
1319.310190	70.101880	67.081601
1318.168057	74.895964	67.086606
1317.653741	61.527184	67.091610
1316.879124	68.093585	67.096615
1316.912840	61.342538	67.101620
1315.872830	76.966103	67.106625
1314.754531	71.727497	67.111630
1314.318369	57.136838	67.116634
1313.755903	71.489212	67.121639
1313.304921	69.437026	67.126644
1313.040129	75.422513	67.131649
1311.783779	62.405079	67.136654
1311.521767	53.641658	67.141658
1310.428315	64.746517	67.146663
1309.569566	71.138649	67.151668
1308.940715	73.894238	67.156673
1308.625280	75.411039	67.161678
1308.485352	73.241597	67.166682
1307.367879	75.522963	67.171687
1306.498657	68.054490	67.176692
1305.846553	71.968045	67.181697
1305.101886	74.789354	67.186702
1304.359845	69.298558	67.191706
1303.342041	73.115720	67.196711
1303.047526	66.511466	67.201716
1302.609323	77.386015	67.206721
1302.120375	63.484954	67.211726
1301.721030	68.801161	67.216730
1300.518066	71.138696	67.221735
1299.995913	72.844472	67.226740
1299.425493	77.019419	67.231745
1298.322535	76.635146	67.236750
1297.714883	65.944544	67.241754
1296.948610	76.773484	67.246759
1297.060036	71.911785	67.251764
1296.380183	78.262867	67.256769
1295.452741	71.090644	67.261774
1294.453484	56.822893	67.266778
1293.779479	83.465790	67.271783
1293.778987	68.411643	67.276788
1292.705078	70.572553	67.281793
1291.653315	71.422717	67.286798
1291.402303	63.409712	67.291802
1290.595962	73.015063	67.296807
1290.642849	62.415935	67.301812
1289.184208	67.362845	67.306817
1288.479704	67.732045	67.311822
1287.947618	68.442821	67.316826
1287.592789	71.454453	67.321831
1286.682314	74.615925	67.326836
1286.064478	68.897242	67.331841
1285.500209	68.796317	67.336846
1285.303633	67.577275	67.341850
1283.796682	69.565777	67.346855
1282.821301	68.836392	67.351860
1282.784435	68.607463	67.356865
1281.942518	71.450546	67.361870
1281.948387	59.774632	67.366874
1280.834533	76.111651	67.371879
1280.340455	67.623232	67.376884
1279.483984	71.466788	67.381889
1278.825540	72.781098	67.386894
1277.759206	67.359218	67.391898
1277.066721	65.722309	67.396903
1276.546800	61.082412	67.401908
1276.602812	65.164069	67.406913
1275.903616	73.084060	67.411918
1275.338869	73.770071	67.416922
1274.296780	75.039729	67.421927
1273.559681	70.990994	67.426932
1272.374869	66.647611	67.431937
1271.494291	74.243223	67.436942
1271.336849	67.680256	67.441946
1270.803678	75.092906	67.446951
1270.258061	85.871006	67.451956
1270.208416	71.542152	67.456961
1268.817344	64.921451	67.461966
1268.430021	67.041012	67.466970
1267.876199	74.152609	67.471975
1266.839555	69.117077	67.476980
1265.656580	67.036214	67.481985
1265.146982	60.455129	67.486990
1264.815085	64.756148	67.491994
1264.626693	67.914775	67.496999
1264.233465	65.364587	67.502004
1263.330826	64.942172	67.507009
1262.418923	63.072087	67.512014
1262.112196	60.233772	67.517018
1260.457658	76.757685	67.522023
1260.257715	61.482964	67.527028
1259.622011	68.763690	67.532033
1259.034538	68.042019	67.537038
1258.581168	61.824136	67.542042
1257.654991	70.475618	67.547047
1257.140772	72.180141	67.552052
1256.336829	71.018252	67.557057
1255.646747	72.099491	67.562062
1254.667780	66.570695	67.567066
1253.841136	70.699660	67.572071
1253.987324	62.692890	67.577076
1253.254169	63.989124	67.582081
1252.409528	73.709377	67.587086
1251.502255	76.088224	67.592090
1250.522237	72.816097	67.597095
1250.518482	73.865476	67.602100
1250.615124	69.660529	67.607105
1249.161933	66.988737	67.612110
1248.364828	58.633665	67.617114
1247.721312	76.594196	67.622119
1247.307291	74.020509	67.627124
1245.952185	64.068485	67.632129
1245.159922	71.333110	67.637134
1244.997196	78.399872	67.642138
1244.460775	73.540264	67.647143
1244.437555	67.522055	67.652148
1243.244027	70.569282	67.657153
1242.287877	77.695975	67.662158
1241.735838	61.195249	67.667162
1241.217330	78.164554	67.672167
1240.839551	72.757778	67.677172
1240.110031	69.890502	67.682177
1239.569150	70.577456	67.687182
1238.591485	62.629545	67.692186
1237.706933	77.192407	67.697191
1237.294674	72.612663	67.702196
1236.804454	64.714971	67.707201
1235.866549	65.952308	67.712206
1234.960078	61.083742	67.717210
1234.329601	68.056151	67.722215
1233.966544	58.960321	67.727220
1233.407939	65.471894	67.732225
1232.197192	68.110301	67.737230
1231.620151	66.010372	67.742234
1231.354284	66.423375	67.747239
1230.800047	61.375806	67.752244
1230.203391	64.220903	67.757249
1229.021472	70.930934	67.762254
1228.855088	64.981220	67.767258
1228.079942	74.340364	67.772263
1227.399792	61.827419	67.777268
1226.416126	74.256769	67.782273
1225.843538	67.305682	67.787278
1225.498018	62.030971	67.792282
1224.828054	67.560518	67.797287
1223.998175	65.710519	67.802292
1223.028484	71.869593	67.807297
1222.510822	67.836443	67.812302
1222.523491	63.827769	67.817306
1221.080156	67.736277	67.822311
1220.350186	66.329261	67.827316
1219.913292	60.126114	67.832321
1219.379516	71.851600	67.837326
1219.189039	64.013476	67.842330
1218.087904	72.992396	67.847335
1217.566509	72.783748	67.852340
1217.097107	64.427036	67.857345
1215.993379	68.067090	67.862350
1215.161681	70.911721	67.867354
1214.189125	75.931179	67.872359
1213.913546	66.949165	67.877364
1213.730199	59.471014	67.882369
1213.104837	67.513306	67.887374
1211.970034	61.290260	67.892378
1211.299915	72.110230	67.897383
1210.808505	68.635851	67.902388
1210.341083	61.650702	67.907393
1209.023369	60.644642	67.912398
1208.651811	55.240043	67.917402
1208.127516	61.957462	67.922407
1207.519609	61.556004	67.927412
1207.179881	66.161032	67.932417
1206.048287	74.353212	67.937422
1205.505198	71.774829	67.942426
1204.533598	73.591517	67.947431
1204.340267	66.392480	67.952436
1203.257119	73.075778	67.957441
1202.195936	70.649165	67.962446
1202.174100	66.884085	67.967450
1201.520856	78.224897	67.972455
1201.317701	71.051074	67.977460
1200.868659	73.434335	67.982465
1199.884780	77.799621	67.987470
1199.153005	68.767158	67.992474
1197.785332	71.145123	67.997479
1197.110475	69.426591	68.002484
1196.500929	66.625402	68.007489
1196.042552	75.743378	68.012494
1196.119318	63.193651	68.017498
1195.133934	75.465595	68.022503
1194.196585	76.289720	68.027508
1193.931541	68.132314	68.032513
1193.210121	68.855872	68.037518
1192.469176	71.913147	68.042522
1191.244929	70.775543	68.047527
1190.638924	68.844224	68.052532
1190.141039	62.904658	68.057537
1189.870258	67.167582	68.062542
1188.984400	69.312820	68.067546
1187.997981	78.893219	68.072551
1187.781027	56.113754	68.077556
1187.366315	90.166123	68.082561
1186.361722	72.794406	68.087566
1185.688163	62.380819	68.092570
1184.885651	68.973763	68.097575
1184.461348	61.207523	68.102580
1183.558646	67.868436	68.107585
1182.660265	65.512132	68.112590
1182.313862	56.787386	68.117594
1181.668832	69.449879	68.122599
1181.482898	74.009955	68.127604
1180.637261	67.941199	68.132609
1179.477374	63.590747	68.137614
1179.203812	60.332454	68.142618
1178.701645	72.092339	68.147623
1177.862878	72.981212	68.152628
1177.299261	65.134630	68.157633
1176.273276	72.236177	68.162638
1176.121364	58.702589	68.167642
1174.379162	65.303057	68.172647
1174.007725	77.199843	68.177652
1173.510809	62.451739	68.182657
1173.001675	57.548394	68.187662
1172.941296	66.978366	68.192666
1172.030326	75.132318	68.197671
1171.416451	63.577052	68.202676
1171.132479	71.161383	68.207681
1170.007761	79.292564	68.212686
1169.464342	65.663547	68.217690
1168.552444	72.161935	68.222695
1167.737183	77.165854	68.227700
1166.611567	73.696156	68.232705
1165.486502	70.022955	68.237710
1165.315468	73.096829	68.242714
1165.197380	75.837448	68.247719
1164.623415	67.027471	68.252724
1164.517226	67.842417	68.257729
1163.583396	68.604495	68.262734
1162.936910	71.219424	68.267738
1162.261241	67.894202	68.272743
1161.440441	67.723721	68.277748
1160.372833	64.375683	68.282753
1159.538719	71.389953	68.287758
1159.462846	64.672111	68.292762
1158.704146	70.136942	68.297767
1157.470871	75.084348	68.302772
1156.964282	73.846817	68.307777
1156.494727	76.566066	68.312782
1156.394565	77.547203	68.317786
1155.563294	72.860661	68.322791
1154.470960	77.941764	68.327796
1154.021089	67.569876	68.332801
1153.497860	74.843773	68.337806
1152.982491	63.400574	68.342810
1151.543444	66.251935	68.347815
1151.028339	66.803928	68.352820
1150.888403	64.274975	68.357825
1150.062939	73.750940	68.362830
1149.368133	67.937314	68.367834
1148.418792	62.635656	68.372839
1147.859398	66.531344	68.377844
1147.949798	64.867727	68.382849
1146.620324	69.584444	68.387854
1145.953570	56.588461	68.392858
1145.348981	68.914962	68.397863
1144.744685	59.748717	68.402868
1144.541837	68.958509	68.407873
1143.207755	68.942204	68.412878
1142.611911	58.748076	68.417882
1142.248371	81.096661	68.422887
1141.514458	64.629628	68.427892
1140.672810	65.894265	68.432897
1139.557054	71.349661	68.437902
1139.188602	64.003455	68.442906
1138.700030	69.004304	68.447911
1138.425764	73.129022	68.452916
1137.856585	76.433369	68.457921
1136.610220	70.538745	68.462926
1135.985323	68.496910	68.467930
1135.859766	68.971181	68.472935
1135.195825	65.415456	68.477940
1134.193456	65.691733	68.482945
1133.308440	72.056552	68.487950
1133.029981	62.737566	68.492954
1132.004799	62.930743	68.497959
1131.110739	68.161656	68.502964
1130.717760	61.483216	68.507969
1130.213220	75.246105	68.512974
1130.010286	57.996081	68.517978
1128.791920	77.891405	68.522983
1127.788787	62.678235	68.527988
1127.604587	54.195772	68.532993
1127.067581	68.257115	68.537998
1126.512903	70.710801	68.543002
1125.732258	77.506855	68.548007
1125.260360	74.032545	68.553012
1124.359518	84.652703	68.558017
1123.247216	53.502157	68.563022
1122.919985	61.772993	68.568026
1122.343522	68.780982	68.573031
1121.740811	72.226275	68.578036
1120.549005	85.420432	68.583041
1119.596672	55.239446	68.588046
1119.560366	88.898892	68.593050
1119.337568	68.340593	68.598055
1118.720896	58.290127	68.603060
1117.734044	76.097126	68.608065
1116.968853	83.696506	68.613070
1116.469374	54.580418	68.618074
1116.159381	82.568819	68.623079
1114.549034	76.257460	68.628084
1114.372006	50.745273	68.633089
1113.595528	90.951331	68.638094
1113.412145	63.308206	68.643098
1112.173289	66.804223	68.648103
1111.775095	66.252743	68.653108
1111.052184	69.889035	68.658113
1110.493173	64.768145	68.663118
1109.325811	63.359774	68.668122
1108.823858	37.415196	68.673127
1108.008224	79.425074	68.678132
1107.888057	58.153493	68.683137
1107.214984	65.544259	68.688142
1106.730507	74.417248	68.693146
1105.505367	71.460123	68.698151
1104.871618	58.285450	68.703156
1104.971049	51.563390	68.708161
1103.570059	76.130058	68.713166
1102.779193	59.612187	68.718170
1102.403411	69.093899	68.723175
1102.207120	52.986061	68.728180
1101.608978	57.690543	68.733185
1100.125292	73.282229	68.738190
1099.938134	55.102509	68.743194
1099.071277	56.573008	68.748199
1098.492450	63.600297	68.753204
1097.632894	58.975048	68.758209
1096.952335	55.500824	68.763214
1096.580848	65.927970	68.768218
1095.903306	73.365183	68.773223
1095.565588	65.436965	68.778228
1094.653165	55.521857	68.783233
1093.860054	66.623162	68.788238
1093.450249	65.796004	68.793242
1092.300570	77.428672	68.798247
1091.260148	60.941040	68.803252
1090.807741	71.444137	68.808257
1090.689967	50.905434	68.813262
1090.160463	66.193961	68.818266
1089.704394	77.298431	68.823271
1088.648868	54.016913	68.828276
1088.317609	57.374878	68.833281
1087.290791	53.126304	68.838286
1086.138499	76.221625	68.843290
1085.596277	43.961792	68.848295
1085.011763	71.451392	68.853300
1084.982625	67.023618	68.858305
1084.303535	62.038525	68.863310
1083.554962	75.069146	68.868314
1082.690835	65.132163	68.873319
1081.688660	68.172675	68.878324
1081.605745	74.050395	68.883329
1080.458676	67.023587	68.888334
1079.890683	59.611373	68.893338
1079.460527	48.834284	68.898343
1079.008441	74.382203	68.903348
1077.856405	69.343038	68.908353
1077.012193	49.711481	68.913358
1076.501456	80.585929	68.918362
1076.231988	52.253249	68.923367
1075.505052	73.412321	68.928372
1074.662330	76.299747	68.933377
1074.080378	65.318148	68.938382
1073.414155	65.676588	68.943386
1073.491071	47.856978	68.948391
1071.542053	77.679795	68.953396
1071.767111	56.957250	68.958401
1070.957103	74.674628	68.963406
1070.299173	73.011782	68.968410
1069.194106	55.091620	68.973415
1068.344460	73.480739	68.978420
1068.400260	65.373240	68.983425
1067.579533	70.895265	68.988430
1066.628707	65.611223	68.993434
1065.659320	68.039432	68.998439
1065.246569	65.615382	69.003444
1064.629393	58.559484	69.008449
1064.468332	69.607560	69.013454
1063.867255	59.824276	69.018458
1062.605929	59.056891	69.023463
1062.195418	81.099143	69.028468
1062.038344	49.601168	69.033473
1060.628720	82.338967	69.038478
1060.524360	61.940041	69.043482
1059.675081	69.333619	69.048487
1058.788511	73.830120	69.053492
1058.223182	51.380500	69.058497
1057.087097	58.332447	69.063502
1056.784095	70.350798	69.068506
1056.471865	71.600626	69.073511
1055.565636	70.024590	69.078516
1054.604583	52.518322	69.083521
1053.655311	82.763982	69.088526
1053.759031	60.827626	69.093530
1053.258717	59.327360	69.098535
1052.211954	59.711650	69.103540
1051.535921	57.149725	69.108545
1050.502591	57.000475	69.113550
1050.400401	59.934095	69.118554
1050.065672	69.306783	69.123559
1048.742300	62.501995	69.128564
1048.360261	59.410780	69.133569
1047.684256	60.548176	69.138574
1047.372616	59.079395	69.143578
1046.088575	63.260681	69.148583
1045.571924	73.562702	69.153588
1044.951632	65.794559	69.158593
1044.411240	77.424927	69.163598
1043.985128	63.786758	69.168602
1042.810792	66.380036	69.173607
1042.154420	76.792591	69.178612
1041.982420	56.811269	69.183617
1040.971927	70.430731	69.188622
1040.384721	63.918820	69.193626
1039.548658	65.087989	69.198631
1039.370684	70.870449	69.203636
1038.782839	65.336296	69.208641
1037.543482	68.756736	69.213646
1036.806851	70.264883	69.218650
1036.562973	65.775086	69.223655
1035.868653	70.622611	69.228660
1035.029719	54.528719	69.233665
1034.143410	78.669776	69.238670
1034.114780	75.347305	69.243674
1033.492672	62.986045	69.248679
1032.256812	58.706100	69.253684
1031.736256	67.578523	69.258689
1031.134557	78.755048	69.263694
1030.913296	59.193125	69.268698
1029.809013	65.321633	69.273703
1028.984278	63.655376	69.278708
1028.631643	58.167384	69.283713
1027.807199	71.538068	69.288718
1026.902372	67.508217	69.293722
1026.183546	65.634311	69.298727
1025.882766	63.870508	69.303732
1025.628505	72.669033	69.308737
1024.436361	69.694086	69.313742
1023.472051	61.789881	69.318746
1023.084554	64.601745	69.323751
1022.395537	83.786874	69.328756
1022.473853	58.861676	69.333761
1021.092607	65.914140	69.338766
1020.701942	79.103863	69.343770
1019.950376	73.064356	69.348775
1019.202429	75.157749	69.353780
1018.185230	62.692203	69.358785
1017.423215	74.979115	69.363790
1017.036119	58.032796	69.368794
1017.273114	55.595268	69.373799
1016.087813	68.343732	69.378804
1015.258969	65.605866	69.383809
1014.262103	69.392992	69.388814
1013.820086	63.914490	69.393818
1013.583311	59.861937	69.398823
1012.785085	62.100516	69.403828
1012.189784	58.759402	69.408833
1011.284222	68.992417	69.413838
1011.071033	63.851227	69.418842
1009.882132	56.774350	69.423847
1008.873330	67.569385	69.428852
1008.761076	56.107834	69.433857
1007.916136	61.742528	69.438862
1007.285035	63.189740	69.443866
1006.588323	66.937000	69.448871
1005.726821	67.993539	69.453876
1005.477653	71.606521	69.458881
1004.965350	71.839571	69.463886
1003.875519	58.862072	69.468890
1003.319473	65.382733	69.473895
1002.792533	77.908200	69.478900
1002.074049	74.471572	69.483905
1001.595963	71.127578	69.488910
1000.616981	64.050418	69.493914
1000.032397	66.201397	69.498919
999.718532	71.362117	69.503924
999.091531	65.417913	69.508929
998.072613	79.291033	69.513934
997.444837	63.400085	69.518938
996.831056	65.893159	69.523943
995.845472	70.108982	69.528948
995.045143	57.134313	69.533953
994.298805	68.748562	69.538958
993.975585	65.217514	69.543962
993.705547	66.465366	69.548967
993.259109	65.932620	69.553972
992.570979	57.402628	69.558977
991.340581	76.954568	69.563982
991.124824	65.856391	69.568986
990.599194	64.098406	69.573991
989.295283	68.268689	69.578996
988.650440	64.072917	69.584001
988.364878	70.921110	69.589006
987.487730	59.368382	69.594010
986.371632	67.848314	69.599015
985.763537	80.974868	69.604020
985.376939	75.165871	69.609025
984.904316	69.200261	69.614030
984.802843	69.885160	69.619034
983.891528	68.697869	69.624039
982.855555	77.040487	69.629044
982.894102	65.340486	69.634049
981.455889	70.254345	69.639054
980.640065	74.083638	69.644058
980.235251	71.158475	69.649063
979.747357	69.804473	69.654068
979.089663	65.976581	69.659073
977.719526	75.414675	69.664078
977.365190	73.943234	69.669082
977.134360	73.349379	69.674087
976.375220	66.782845	69.679092
975.760268	61.918462	69.684097
974.778350	74.415401	69.689102
974.248056	58.174663	69.694106
973.691599	64.261755	69.699111
973.092437	71.360107	69.704116
972.467596	64.803745	69.709121
971.381840	76.352168	69.714126
971.245452	83.572424	69.719130
970.718841	55.588187	69.724135
969.297758	57.623124	69.729140
968.825905	71.603154	69.734145
968.471035	64.792537	69.739150
967.419509	61.009968	69.744154
967.739639	71.002243	69.749159
966.481351	73.780791	69.754164
966.042815	44.715025	69.759169
965.033911	84.600079	69.764174
964.091397	47.402182	69.769178
963.416782	80.459836	69.774183
962.888154	64.854306	69.779188
962.988007	46.832383	69.784193
962.016743	53.836980	69.789198
960.985242	63.076120	69.794202
960.568245	61.384431	69.799207
959.944902	70.579131	69.804212
958.935167	62.321082	69.809217
957.913134	60.340911	69.814222
957.730244	57.033533	69.819226
957.379958	68.674651	69.824231
957.025916	67.457042	69.829236
955.795840	61.649812	69.834241
954.861806	66.737335	69.839246
954.487060	66.601596	69.844250
954.317999	59.662077	69.849255
953.172154	68.485779	69.854260
952.494154	57.902690	69.859265
951.885681	67.500277	69.864270
951.274899	67.616550	69.869274
950.677045	69.790151	69.874279
949.567458	69.478044	69.879284
949.090399	63.621956	69.884289
948.751761	59.503623	69.889294
948.155171	59.778479	69.894298
947.259942	50.048355	69.899303
946.110353	88.747929	69.904308
946.215090	68.255831	69.909313
945.502133	58.135598	69.914318
944.603662	67.564877	69.919322
944.059047	62.075911	69.924327
943.402623	70.807549	69.929332
942.954834	63.917112	69.934337
941.415215	67.926239	69.939342
940.928859	66.308664	69.944346
940.551439	60.389418	69.949351
940.204111	83.689408	69.954356
939.877239	70.432845	69.959361
938.598740	70.838287	69.964366
938.118529	73.526152	69.969370
937.672087	62.147747	69.974375
936.352195	70.276948	69.979380
935.751759	67.807099	69.984385
935.052053	56.858485	69.989390
934.764731	72.725041	69.994394
934.194220	66.964245	69.999399
932.914796	76.271237	70.004404
932.558716	57.219628	70.009409
932.058763	55.848634	70.014414
931.414813	68.023732	70.019418
931.285708	64.887559	70.024423
930.061710	68.152648	70.029428
929.634084	65.399850	70.034433
929.131679	65.907290	70.039438
927.552171	65.059725	70.044442
926.867636	63.338080	70.049447
926.139858	69.646398	70.054452
925.916313	64.948390	70.059457
925.604375	67.445484	70.064462
925.151567	60.830226	70.069466
924.646814	67.393196	70.074471
923.691891	64.888302	70.079476
923.116398	68.602099	70.084481
921.867873	67.104237	70.089486
921.236824	62.896830	70.094490
921.044004	59.874870	70.099495
920.357536	73.494839	70.104500
919.781732	62.863959	70.109505
918.630437	63.693845	70.114510
917.802155	68.423949	70.119514
917.454164	58.813319	70.124519
916.909317	63.733270	70.129524
916.315661	67.191353	70.134529
915.213230	68.208996	70.139534
914.523924	63.919403	70.144538
914.426894	56.096423	70.149543
913.794516	64.463134	70.154548
913.132031	55.399266	70.159553
912.101521	61.222779	70.164558
911.125141	72.818463	70.169562
910.921796	59.804019	70.174567
909.936871	59.632932	70.179572
909.160054	54.460036	70.184577
908.819827	62.173162	70.189582
908.458276	68.817419	70.194586
908.459164	60.374917	70.199591
907.177659	70.109575	70.204596
906.423316	59.343121	70.209601
906.043681	58.162708	70.214606
904.906477	55.125468	70.219610
903.893191	78.214475	70.224615
903.317640	66.071345	70.229620
903.229758	65.416904	70.234625
902.599664	64.839289	70.239630
901.510938	55.147860	70.244634
901.063508	54.105963	70.249639
900.146944	67.286334	70.254644
899.595356	70.162172	70.259649
899.122499	55.117050	70.264654
897.954461	69.218908	70.269658
897.825162	68.279339	70.274663
897.205698	63.992828	70.279668
896.583072	55.849818	70.284673
895.568307	67.055818	70.289678
895.046836	75.627225	70.294682
894.905179	73.019724	70.299687
893.553881	62.611609	70.304692
893.105574	67.263904	70.309697
892.505203	63.748596	70.314702
891.853510	78.665528	70.319706
891.392162	51.169243	70.324711
890.290255	74.567223	70.329716
889.463232	66.526119	70.334721
889.327520	69.133936	70.339726
888.571814	79.125533	70.344730
887.770318	58.380313	70.349735
886.861523	63.632564	70.354740
886.552570	58.035152	70.359745
886.188544	70.990408	70.364750
885.031777	70.034594	70.369754
883.997851	67.141766	70.374759
883.207528	76.478166	70.379764
883.178467	57.793976	70.384769
882.756083	59.064506	70.389774
882.210139	70.799839	70.394778
881.193123	63.329842	70.399783
880.604645	62.889104	70.404788
880.079511	61.028570	70.409793
879.141967	61.095945	70.414798
878.141075	62.602040	70.419802
877.838807	50.614124	70.424807
877.229660	55.555350	70.429812
877.018217	54.274062	70.434817
876.049716	54.929804	70.439822
875.416930	54.912411	70.444826
875.018695	53.621430	70.449831
873.524148	62.806564	70.454836
872.734045	57.071278	70.459841
872.246274	74.656975	70.464846
872.113911	55.531940	70.469850
871.834532	57.085624	70.474855
870.760406	55.930596	70.479860
869.826442	71.682454	70.484865
869.573742	53.830180	70.489870
868.586711	41.858221	70.494874
867.847835	56.183493	70.499879
866.838710	65.964696	70.504884
866.634872	41.445574	70.509889
865.952178	72.621715	70.514894
865.583363	68.197555	70.519898
864.772591	60.480290	70.524903
863.784716	52.311850	70.529908
863.609193	72.642047	70.534913
863.019139	51.222993	70.539918
861.965430	51.988490	70.544922
861.361437	58.497877	70.549927
860.634655	66.299337	70.554932
860.161942	62.987635	70.559937
859.050433	75.360158	70.564942
858.034500	63.424324	70.569946
858.073372	39.450018	70.574951
857.555346	65.262266	70.579956
857.251795	58.380434	70.584961
855.961430	48.902466	70.589966
855.198105	69.482320	70.594970
855.063864	46.434367	70.599975
854.489358	57.124048	70.604980
853.798574	70.372570	70.609985
852.908637	52.957596	70.614990
852.548422	55.946475	70.619994
851.584661	54.628819	70.624999
850.666452	61.535129	70.630004
850.246875	51.910683	70.635009
849.603829	55.882810	70.640014
848.374269	63.130395	70.645018
847.881922	61.211037	70.650023
847.281395	63.798223	70.655028
847.042483	63.429582	70.660033
846.756411	62.846109	70.665038
845.555021	65.139444	70.670042
844.912641	53.308164	70.675047
844.019952	67.954381	70.680052
843.661573	52.134168	70.685057
842.662971	66.013541	70.690062
841.912975	69.597443	70.695066
841.661009	58.131350	70.700071
841.004491	60.952939	70.705076
840.449835	56.484255	70.710081
839.237475	73.012094	70.715086
838.298063	57.186591	70.720090
837.998773	57.505611	70.725095
837.704695	75.877295	70.730100
837.501699	63.744275	70.735105
836.594188	45.319772	70.740110
835.484584	67.452756	70.745114
835.432498	72.556052	70.750119
834.320108	69.270480	70.755124
833.485905	58.420580	70.760129
833.096253	59.755290	70.765134
832.608558	66.317133	70.770138
831.753815	47.065839	70.775143
830.707550	63.485237	70.780148
830.097856	72.047039	70.785153
829.872864	74.725836	70.790158
828.908887	62.860591	70.795162
828.180183	67.658444	70.800167
827.678211	78.581012	70.805172
827.236031	49.567923	70.810177
826.351962	82.215807	70.815182
824.860944	69.568750	70.820186
824.863325	57.633270	70.825191
824.208819	71.120435	70.830196
823.970160	45.104114	70.835201
823.474090	63.168907	70.840206
822.850977	55.046499	70.845210
821.941237	59.915741	70.850215
821.345015	65.421017	70.855220
820.288184	58.435179	70.860225
819.255851	61.291363	70.865230
818.756193	65.051452	70.870234
818.815554	52.028335	70.875239
818.309276	59.643323	70.880244
817.054314	55.156813	70.885249
816.348693	72.021867	70.890254
815.816347	49.966060	70.895258
815.380914	50.324099	70.900263
814.164965	73.245108	70.905268
813.666748	64.967207	70.910273
813.258084	54.426454	70.915278
812.541803	68.943680	70.920282
811.953009	60.785849	70.925287
810.705008	58.193620	70.930292
810.209281	59.751786	70.935297
809.880553	51.647177	70.940302
809.271942	62.414831	70.945306
808.694864	61.234325	70.950311
807.630169	58.903062	70.955316
807.196889	74.568930	70.960321
806.998872	54.965538	70.965326
806.040211	57.529317	70.970330
805.020855	65.594966	70.975335
804.370028	60.063026	70.980340
804.000680	57.938030	70.985345
803.900362	58.313686	70.990350
802.535604	47.445764	70.995354
801.999837	50.421594	71.000359
801.427586	66.680399	71.005364
800.758145	58.495989	71.010369
799.963347	53.728094	71.015374
798.960232	58.252682	71.020378
798.777508	57.496655	71.025383
798.071963	65.742575	71.030388
796.795696	66.644446	71.035393
796.505606	58.106356	71.040398
795.797225	58.315469	71.045402
795.615123	55.386430	71.050407
794.954661	62.053043	71.055412
794.059610	57.302685	71.060417
793.258538	62.099448	71.065422
792.634108	68.537992	71.070426
792.178931	54.458288	71.075431
791.173263	60.468688	71.080436
790.436235	65.833966	71.085441
790.138546	61.419001	71.090446
789.743854	50.816112	71.095450
788.656152	63.807716	71.100455
787.687713	69.033226	71.105460
787.383963	62.693878	71.110465
787.400943	68.166199	71.115470
785.906279	66.638207	71.120474
785.408589	61.427227	71.125479
784.781408	60.972174	71.130484
784.053854	64.386947	71.135489
783.332469	68.341601	71.140494
781.952657	64.541994	71.145498
781.349344	56.354950	71.150503
780.943632	68.665596	71.155508
780.796570	59.609606	71.160513
780.477154	53.564477	71.165518
780.136952	61.722280	71.170522
779.490974	56.437144	71.175527
778.333354	61.863070	71.180532
777.933399	70.404106	71.185537
777.004554	65.156112	71.190542
775.992001	70.653561	71.195546
775.624237	61.307871	71.200551
774.831690	73.114009	71.205556
773.527847	65.494192	71.210561
773.184129	62.950406	71.215566
772.889859	68.232592	71.220570
772.857615	63.068939	71.225575
771.671582	67.170100	71.230580
770.868371	56.882965	71.235585
770.325256	66.241526	71.240590
769.528797	71.671463	71.245594
768.837051	64.181278	71.250599
767.972999	64.594942	71.255604
767.463663	58.605276	71.260609
767.062957	65.862866	71.265614
766.500526	73.636609	71.270618
765.720222	65.737922	71.275623
764.711468	68.077894	71.280628
764.612407	56.713628	71.285633
763.862437	65.852822	71.290638
762.840420	71.020641	71.295642
762.384715	60.365968	71.300647
761.970520	60.916165	71.305652
760.713665	61.326136	71.310657
760.076911	61.965378	71.315662
759.668381	69.995300	71.320666
759.229439	69.772045	71.325671
758.743258	64.560816	71.330676
757.739502	63.110800	71.335681
757.144214	62.688521	71.340686
756.254991	54.428738	71.345690
755.844964	62.275979	71.350695
754.672487	68.290874	71.355700
754.229705	66.500832	71.360705
753.790051	68.617753	71.365710
753.254566	55.405504	71.370714
752.544656	53.336311	71.375719
751.324200	69.113299	71.380724
750.988242	61.072923	71.385729
750.528483	59.093209	71.390734
749.456828	56.889229	71.395738
748.925394	56.087802	71.400743
748.140944	66.974919	71.405748
747.368229	62.556741	71.410753
747.554697	56.943559	71.415758
746.590023	61.848378	71.420762
745.854048	63.515762	71.425767
744.964644	66.757628	71.430772
744.325053	56.990050	71.435777
744.254997	51.094452	71.440782
743.227636	59.643911	71.445786
742.136900	60.509964	71.450791
741.775830	58.449888	71.455796
741.133278	69.245036	71.460801
740.559240	65.134255	71.465806
739.779713	63.695854	71.470810
739.181730	48.956128	71.475815
738.916218	70.043329	71.480820
738.225400	62.620812	71.485825
737.142447	66.571543	71.490830
736.506085	72.959962	71.495834
735.955640	59.061010	71.500839
734.723278	69.645725	71.505844
734.038437	60.607555	71.510849
733.745334	53.137495	71.515854
733.157845	63.283668	71.520858
733.088627	64.769215	71.525863
732.500942	55.461706	71.530868
731.617988	58.940653	71.535873
730.756331	57.321377	71.540878
729.561091	62.352790	71.545882
728.620035	65.000523	71.550887
728.241682	62.020738	71.555892
727.635176	67.682201	71.560897
727.602285	53.639361	71.565902
726.943238	68.538545	71.570906
726.332700	63.033329	71.575911
725.320843	58.173869	71.580916
724.590747	58.517339	71.585921
724.253764	49.663479	71.590926
723.022867	61.892623	71.595930
722.323897	49.661997	71.600935
721.689654	64.055787	71.605940
721.374027	57.423473	71.610945
721.194527	58.114495	71.615950
720.270326	62.473593	71.620954
719.624699	63.267213	71.625959
718.764887	72.548480	71.630964
718.012881	72.811866	71.635969
717.544364	54.643935	71.640974
716.697377	61.797549	71.645978
716.358875	61.447931	71.650983
715.003911	66.716081	71.655988
714.266561	57.150148	71.660993
713.921864	58.788358	71.665998
713.533772	57.047961	71.671002
713.312831	52.649176	71.676007
712.319319	67.052865	71.681012
711.262130	60.675806	71.686017
711.215205	53.090866	71.691022
710.114173	57.604268	71.696026
709.327679	57.114679	71.701031
708.600328	63.306287	71.706036
708.420246	62.436312	71.711041
707.798398	60.614870	71.716046
706.253729	62.125611	71.721050
705.863738	63.296400	71.726055
705.405775	63.766848	71.731060
704.866123	64.571982	71.736065
704.809715	60.249494	71.741070
703.392720	69.570594	71.746074
702.891563	60.202009	71.751079
702.205516	64.348164	71.756084
701.486141	63.450522	71.761089
700.414926	57.469917	71.766094
700.044630	63.387069	71.771098
699.881239	54.526072	71.776103
699.320098	66.938733	71.781108
698.364435	73.524645	71.786113
697.872159	53.198632	71.791118
696.991609	68.189854	71.796122
695.988355	58.037098	71.801127
695.316710	61.398838	71.806132
694.592177	59.730936	71.811137
694.265850	62.003275	71.816142
693.791542	66.314402	71.821146
693.113362	63.549510	71.826151
692.354593	61.932788	71.831156
691.294653	72.303999	71.836161
691.190514	56.380274	71.841166
690.284747	63.978468	71.846170
689.612764	54.316989	71.851175
688.764189	61.674277	71.856180
688.081685	50.686761	71.861185
688.172527	50.369703	71.866190
686.830164	76.472475	71.871194
686.263497	57.843968	71.876199
685.379689	47.030426	71.881204
684.860181	60.633288	71.886209
684.852743	51.242869	71.891214
683.397652	69.234879	71.896218
682.942294	62.172259	71.901223
682.216856	59.509507	71.906228
681.926132	62.186162	71.911233
681.555404	61.428542	71.916238
680.230242	62.800276	71.921242
679.654853	50.026472	71.926247
679.059743	57.262983	71.931252
678.393080	64.310629	71.936257
677.569273	60.162371	71.941262
676.330621	57.634953	71.946266
676.287494	55.423344	71.951271
676.120550	59.396966	71.956276
675.541679	65.500288	71.961281
675.059979	62.600043	71.966286
673.839880	61.614993	71.971290
673.153120	55.957938	71.976295
671.931837	70.369526	71.981300
671.407506	67.908128	71.986305
671.039340	69.483853	71.991310
670.496998	77.041536	71.996314
670.667707	60.594682	72.001319
669.738785	61.524881	72.006324
669.058081	66.469660	72.011329
668.055345	59.552550	72.016334
666.434055	65.547487	72.021338
666.105655	55.020801	72.026343
665.471996	59.052971	72.031348
665.374745	64.811538	72.036353
665.103095	64.558508	72.041358
663.793943	77.705265	72.046362
663.305258	55.836521	72.051367
662.840090	60.038969	72.056372
661.825830	60.780922	72.061377
660.737169	60.736832	72.066382
660.026604	67.804089	72.071386
659.712598	67.575150	72.076391
659.213728	54.992580	72.081396
658.713471	69.193168	72.086401
658.885442	56.981563	72.091406
657.287381	68.669996	72.096410
656.952068	62.482347	72.101415
656.106125	68.628201	72.106420
655.111429	58.314841	72.111425
654.652439	56.901116	72.116430
653.758095	69.773671	72.121434
653.865588	55.298504	72.126439
653.059725	51.338200	72.131444
651.947169	61.694142	72.136449
651.490437	60.578084	72.141454
650.069127	71.115654	72.146458
649.863210	57.685390	72.151463
649.157200	59.172999	72.156468
648.503462	53.029754	72.161473
648.694304	51.692314	72.166478
647.054850	65.822009	72.171482
646.560506	55.089954	72.176487
645.895556	65.954907	72.181492
645.294652	59.986162	72.186497
645.231396	54.974107	72.191502
643.978488	59.693060	72.196506
643.501131	57.788706	72.201511
642.890594	56.559955	72.206516
642.024890	57.000732	72.211521
641.383030	44.018350	72.216526
640.344937	52.739847	72.221530
639.918019	57.097046	72.226535
639.645702	50.528812	72.231540
638.935649	55.755795	72.236545
638.072029	43.207673	72.241550
637.268518	60.503032	72.246554
636.866062	56.188351	72.251559
636.542517	59.390599	72.256564
635.128980	55.922861	72.261569
634.660805	51.257548	72.266574
634.287059	55.271986	72.271578
633.959452	58.470150	72.276583
632.786186	61.115473	72.281588
631.773169	62.786009	72.286593
631.573718	54.408553	72.291598
630.898339	65.149020	72.296602
630.279170	59.813932	72.301607
629.232383	55.929848	72.306612
628.507578	62.617777	72.311617
628.630656	40.539693	72.316622
627.940320	52.991844	72.321626
626.645730	55.722717	72.326631
626.017418	61.805536	72.331636
625.381833	71.508406	72.336641
625.337864	53.328094	72.341646
624.360856	54.805252	72.346650
623.779122	63.115060	72.351655
623.072582	54.510873	72.356660
622.239108	58.123891	72.361665
621.305222	55.981604	72.366670
620.546565	58.512022	72.371674
620.118466	63.519078	72.376679
619.921797	58.356393	72.381684
619.126155	57.723219	72.386689
618.506031	52.684739	72.391694
617.648537	63.129376	72.396698
617.336628	51.239250	72.401703
616.726223	48.758462	72.406708
615.290731	51.734116	72.411713
614.564299	53.600277	72.416718
614.122180	61.375373	72.421722
613.949636	57.911853	72.426727
613.236478	52.013036	72.431732
612.209537	62.667574	72.436737
611.691363	54.935355	72.441742
611.023914	55.043390	72.446746
610.655300	60.015744	72.451751
609.722227	62.930312	72.456756
608.926483	61.310044	72.461761
608.771998	53.933044	72.466766
607.586589	58.042058	72.471770
606.840177	55.705926	72.476775
606.478849	58.291335	72.481780
605.999752	54.291624	72.486785
605.596947	46.947867	72.491790
604.649162	61.106188	72.496794
603.896441	54.786345	72.501799
603.049797	58.798834	72.506804
602.023209	55.468176	72.511809
601.510248	54.698531	72.516814
600.747616	58.487919	72.521818
600.049502	53.337294	72.526823
599.722438	65.706375	72.531828
599.341665	60.779581	72.536833
598.904390	50.189834	72.541838
597.655447	60.655818	72.546842
597.338482	46.631442	72.551847
596.794198	53.878792	72.556852
595.509837	63.768559	72.561857
594.887449	59.859474	72.566862
594.568317	54.061902	72.571866
594.246410	50.004046	72.576871
593.658224	53.486549	72.581876
592.117380	59.821931	72.586881
591.873549	62.044874	72.591886
591.361092	61.803398	72.596890
590.779991	52.103830	72.601895
589.767218	56.350926	72.606900
588.859518	66.675842	72.611905
588.785912	52.723085	72.616910
587.943870	61.008127	72.621914
587.286979	62.565195	72.626919
586.288925	54.417433	72.631924
585.653862	53.746080	72.636929
585.623078	45.214050	72.641934
584.905326	46.504861	72.646938
583.845859	62.369788	72.651943
583.241494	49.736245	72.656948
582.678152	64.979721	72.661953
582.513535	60.668168	72.666958
581.153482	62.124353	72.671962
580.708314	66.050833	72.676967
580.409010	63.561503	72.681972
579.185555	62.799371	72.686977
578.771916	52.264208	72.691982
577.940626	61.618226	72.696986
577.676881	58.289076	72.701991
576.889442	44.374331	72.706996
576.049940	61.255987	72.712001
575.509082	60.976462	72.717006
574.794533	59.962979	72.722010
574.019449	54.485596	72.727015
572.899725	60.657729	72.732020
572.442499	61.932280	72.737025
572.154121	58.947656	72.742030
571.581105	58.088240	72.747034
570.939073	58.217467	72.752039
570.021979	63.236184	72.757044
569.105697	71.966697	72.762049
568.800473	53.823277	72.767054
568.068616	61.824287	72.772058
567.504271	57.719897	72.777063
566.959862	55.473023	72.782068
566.172506	64.960388	72.787073
565.536888	62.808460	72.792078
564.212112	62.865093	72.797082
563.691995	68.224262	72.802087
563.521019	55.088059	72.807092
562.942487	62.643628	72.812097
562.656747	64.324503	72.817102
561.643017	61.712438	72.822106
560.814539	64.499984	72.827111
560.265066	58.869983	72.832116
559.516318	67.871838	72.837121
558.511104	51.159746	72.842126
557.836461	66.269574	72.847130
557.242456	56.614645	72.852135
557.165035	65.735063	72.857140
556.582345	67.300820	72.862145
555.922510	57.522343	72.867150
555.038833	63.852418	72.872154
554.448860	61.671147	72.877159
553.225613	56.022318	72.882164
552.555253	62.215920	72.887169
552.339022	56.020366	72.892174
551.712181	65.330790	72.897178
551.224134	54.230356	72.902183
550.529495	62.701651	72.907188
549.472292	61.984013	72.912193
549.394912	48.854986	72.917198
548.248561	53.761999	72.922202
547.380041	61.862046	72.927207
546.716945	68.190105	72.932212
546.365007	61.724446	72.937217
545.902526	43.975079	72.942222
544.847294	69.915451	72.947226
544.275750	52.208676	72.952231
543.561810	65.320581	72.957236
543.407232	71.764751	72.962241
542.269004	33.619170	72.967246
541.260538	82.444889	72.972250
540.813644	55.900466	72.977255
540.571528	61.830328	72.982260
540.023797	68.483767	72.987265
539.092118	49.071435	72.992270
538.134129	63.370163	72.997274
537.898754	64.024369	73.002279
537.361763	56.886489	73.007284
536.283388	63.747445	73.012289
535.855333	46.904017	73.017294
535.280428	59.006660	73.022298
534.489786	57.724630	73.027303
533.257579	58.532887	73.032308
532.706427	61.784014	73.037313
532.083348	55.670614	73.042318
531.613064	68.311654	73.047322
531.733699	57.215188	73.052327
530.882560	55.168559	73.057332
529.862097	61.890989	73.062337
529.703333	57.441325	73.067342
528.153746	62.111400	73.072346
527.194802	52.085710	73.077351
526.889078	57.041746	73.082356
526.186428	66.745848	73.087361
526.065522	62.883051	73.092366
525.795944	64.849920	73.097370
524.978235	65.216864	73.102375
524.134045	62.568348	73.107380
523.161723	70.391645	73.112385
522.300617	58.874431	73.117390
521.615715	63.914522	73.122394
520.903814	61.790526	73.127399
520.709940	50.152844	73.132404
520.089363	76.080761	73.137409
519.567573	73.139629	73.142414
518.474742	65.141024	73.147418
518.073443	70.711494	73.152423
517.489951	65.123190	73.157428
516.210705	59.781326	73.162433
515.570431	58.882178	73.167438
515.419400	55.069911	73.172442
515.022728	59.808638	73.177447
514.017975	55.236710	73.182452
512.781424	64.145976	73.187457
512.738622	55.363565	73.192462
512.549034	56.970784	73.197466
511.422097	57.593559	73.202471
510.626369	51.906615	73.207476
509.796049	56.731765	73.212481
509.238185	66.600452	73.217486
508.213743	63.578556	73.222490
507.341109	64.745838	73.227495
507.226025	52.086418	73.232500
506.730306	52.860941	73.237505
506.626650	53.702311	73.242510
505.952270	58.944142	73.247514
504.874517	59.082875	73.252519
504.423378	50.255135	73.257524
502.969931	57.607906	73.262529
502.532828	58.336825	73.267534
501.773634	57.770419	73.272538
501.137225	46.190624	73.277543
501.130019	63.594104	73.282548
499.944606	56.827595	73.287553
499.060099	57.577326	73.292558
498.613899	54.854383	73.297562
498.015324	61.156401	73.302567
497.831123	57.098700	73.307572
497.001092	66.534535	73.312577
496.142527	64.984233	73.317582
495.602008	67.145644	73.322586
495.007950	62.926165	73.327591
494.319021	61.954354	73.332596
493.483730	60.906516	73.337601
492.828701	67.739470	73.342606
492.357916	66.556300	73.347610
491.393568	58.950382	73.352615
491.059428	61.482591	73.357620
490.078856	63.682568	73.362625
489.328151	72.544411	73.367630
488.245344	60.826001	73.372634
487.750001	63.601498	73.377639
487.455272	45.871156	73.382644
487.030053	68.108059	73.387649
486.950253	58.707108	73.392654
486.037896	45.096140	73.397658
484.942052	79.051847	73.402663
484.691839	40.712798	73.407668
483.248882	64.537302	73.412673
482.802940	56.574431	73.417678
481.731602	62.063997	73.422682
481.484919	57.822298	73.427687
481.367017	54.398971	73.432692
479.867423	65.504139	73.437697
479.636652	50.713901	73.442702
478.632026	57.446438	73.447706
478.316705	73.412038	73.452711
478.304142	47.175337	73.457716
476.577311	64.982067	73.462721
476.274783	44.320022	73.467726
475.692977	62.333820	73.472730
474.919058	59.663090	73.477735
474.395528	53.467622	73.482740
473.483511	62.884985	73.487745
473.195120	60.247285	73.492750
472.677378	52.683763	73.497754
471.404208	62.202813	73.502759
471.123950	52.177832	73.507764
470.341237	57.943099	73.512769
470.049689	51.474148	73.517774
468.924667	63.292304	73.522778
468.364260	60.021469	73.527783
467.908423	44.946995	73.532788
466.944956	58.453449	73.537793
466.067359	55.228418	73.542798
465.708888	55.291999	73.547802
465.148132	52.568391	73.552807
464.927475	55.763724	73.557812
463.523608	61.342541	73.562817
462.793023	58.428383	73.567822
462.183259	54.816930	73.572826
461.530573	62.027959	73.577831
461.436700	48.100534	73.582836
460.602180	62.215615	73.587841
459.884258	58.619816	73.592846
459.018569	59.601515	73.597850
458.695637	57.595332	73.602855
457.969938	57.174981	73.607860
456.800186	71.617851	73.612865
456.421665	55.279029	73.617870
455.780566	65.922604	73.622874
454.985977	66.408882	73.627879
454.688806	58.652537	73.632884
453.775658	61.363723	73.637889
453.259222	56.865403	73.642894
452.726097	50.551631	73.647898
451.380646	52.830252	73.652903
450.931061	45.621711	73.657908
450.519787	70.308400	73.662913
450.231087	64.518618	73.667918
449.693996	50.680729	73.672922
448.339261	58.446705	73.677927
447.836387	54.376707	73.682932
447.298732	68.512304	73.687937
446.598772	61.220653	73.692942
445.746590	54.186632	73.697946
445.122000	65.765805	73.702951
445.163859	50.716112	73.707956
444.089955	55.624240	73.712961
443.178689	59.289127	73.717966
442.685703	63.675801	73.722970
441.729226	65.633852	73.727975
441.672640	54.368523	73.732980
440.145000	54.435468	73.737985
439.548525	55.487814	73.742990
439.023787	63.652959	73.747994
438.637016	73.443941	73.752999
438.616023	40.281482	73.758004
437.224437	59.704700	73.763009
436.636724	64.746670	73.768014
435.972870	52.110045	73.773018
435.422525	58.442233	73.778023
434.681264	54.690900	73.783028
434.154088	56.724048	73.788033
433.830181	59.983139	73.793038
432.792509	64.335180	73.798042
431.453382	56.104649	73.803047
431.146245	56.137979	73.808052
430.461974	59.697322	73.813057
430.148130	58.810839	73.818062
429.701915	63.852341	73.823066
428.506994	65.066268	73.828071
428.206848	58.213940	73.833076
427.534380	67.317200	73.838081
427.323987	58.749145	73.843086
426.203992	65.958950	73.848090
425.222589	55.358182	73.853095
425.244075	51.460095	73.858100
423.756212	59.296177	73.863105
422.843955	65.903639	73.868110
422.480657	57.445098	73.873114
421.722724	58.122654	73.878119
421.595644	56.370682	73.883124
421.493421	64.996755	73.888129
420.656652	50.867601	73.893134
419.541605	56.824594	73.898138
418.925948	53.821181	73.903143
418.193196	44.708778	73.908148
417.114037	56.675746	73.913153
416.625625	46.887361	73.918158
416.661892	47.690672	73.923162
415.819219	58.566624	73.928167
414.757343	55.462433	73.933172
413.907231	59.152276	73.938177
413.492801	50.604123	73.943182
413.043180	53.501648	73.948186
411.813417	63.392251	73.953191
411.426723	55.940321	73.958196
410.622574	63.922923	73.963201
410.102888	59.679004	73.968206
410.270816	53.135276	73.973210
408.874594	57.856670	73.978215
408.292793	47.971211	73.983220
407.670723	62.154945	73.988225
407.275591	61.347645	73.993230
406.315227	58.496924	73.998234
405.562085	60.676462	74.003239
405.278455	55.975490	74.008244
404.163305	57.356478	74.013249
403.483407	55.730437	74.018254
402.865477	52.590205	74.023258
402.148229	59.532428	74.028263
402.211094	61.905201	74.033268
401.097458	68.420187	74.038273
400.585131	49.387368	74.043278
400.057652	53.315947	74.048282
398.573629	56.990114	74.053287
397.962557	59.503386	74.058292
397.334563	49.483373	74.063297
397.017112	59.105616	74.068302
396.807901	53.749432	74.073306
395.549487	61.709808	74.078311
395.124813	56.457337	74.083316
394.481164	55.397920	74.088321
394.079996	45.322846	74.093326
393.382585	55.532300	74.098330
392.137269	65.863756	74.103335
392.146973	55.180768	74.108340
391.108253	61.612860	74.113345
389.834919	57.779177	74.118350
389.450331	49.697755	74.123354
388.614525	59.049381	74.128359
388.547735	42.348706	74.133364
388.114277	59.060038	74.138369
387.855429	58.738772	74.143374
386.427200	54.433065	74.148378
385.814844	62.670520	74.153383
385.284712	53.467494	74.158388
383.886256	58.275984	74.163393
383.262100	57.319113	74.168398
383.051914	59.629745	74.173402
382.254092	65.673394	74.178407
382.315204	62.067016	74.183412
381.785130	61.416832	74.188417
380.722461	64.851993	74.193422
380.065560	49.498944	74.198426
379.030008	63.587731	74.203431
378.480083	53.629394	74.208436
377.971648	67.009756	74.213441
377.091541	66.016406	74.218446
376.911712	55.593842	74.223450
375.384340	66.233585	74.228455
375.151946	43.106818	74.233460
374.227100	61.905364	74.238465
374.205783	62.514436	74.243470
373.782248	50.714697	74.248474
372.545556	63.033195	74.253479
372.190985	57.569298	74.258484
371.429887	61.016326	74.263489
370.551337	54.035421	74.268494
369.470894	56.216666	74.273498
368.577940	59.998500	74.278503
368.331437	58.268716	74.283508
367.895553	62.745643	74.288513
367.769835	60.241298	74.293518
366.782450	55.669824	74.298522
365.837190	64.854408	74.303527
365.392638	62.776162	74.308532
365.223312	57.397857	74.313537
364.070924	60.301729	74.318542
363.599392	51.094104	74.323546
362.660875	56.251907	74.328551
361.979796	55.507527	74.333556
360.958346	61.985760	74.338561
360.418421	50.534134	74.343566
359.915505	51.961072	74.348570
359.418371	49.555339	74.353575
359.347647	49.923142	74.358580
358.359692	51.236575	74.363585
357.379613	64.018779	74.368590
357.183811	56.910155	74.373594
355.745666	49.662066	74.378599
355.458651	45.329052	74.383604
354.734629	55.534868	74.388609
354.231706	61.928894	74.393614
353.516769	52.223930	74.398618
352.361554	55.872531	74.403623
352.392226	56.508009	74.408628
351.531928	58.999510	74.413633
351.019955	48.346053	74.418638
350.017182	57.431000	74.423642
349.010390	67.692926	74.428647
348.942545	60.013590	74.433652
348.520223	55.118701	74.438657
347.357889	54.846808	74.443662
346.981607	52.836530	74.448666
346.122233	60.135707	74.453671
345.938107	55.059366	74.458676
344.399306	58.933093	74.463681
343.892434	56.596719	74.468686
343.451048	52.296189	74.473690
342.978063	54.021116	74.478695
342.886202	53.189150	74.483700
341.606469	63.447266	74.488705
340.862051	52.964885	74.493710
340.343406	52.484766	74.498714
339.195688	59.719517	74.503719
338.681461	55.017461	74.508724
338.180955	59.072632	74.513729
338.043917	61.452029	74.518734
337.463506	61.018022	74.523738
335.971423	59.497781	74.528743
335.376536	51.465655	74.533748
335.004421	57.964984	74.538753
334.087852	53.563577	74.543758
333.286586	54.189721	74.548762
332.641362	64.589557	74.553767
332.312135	65.205126	74.558772
331.948329	56.666269	74.563777
331.485363	50.656721	74.568782
330.143201	70.735968	74.573786
329.638567	74.940027	74.578791
329.324060	55.725902	74.583796
328.315268	49.558931	74.588801
327.320382	60.492276	74.593806
326.781508	48.892272	74.598810
326.140942	67.052632	74.603815
326.045916	58.724813	74.608820
325.102148	55.007367	74.613825
324.113967	60.742343	74.618830
323.654849	66.176975	74.623834
322.807492	61.652584	74.628839
322.779930	58.195950	74.633844
321.833749	61.863288	74.638849
320.940915	57.331955	74.643854
320.846684	52.730115	74.648858
320.062410	64.658007	74.653863
319.103023	58.823762	74.658868
318.138722	54.291206	74.663873
317.712287	54.548554	74.668878
317.433180	62.975745	74.673882
316.412798	62.200303	74.678887
315.652216	62.886197	74.683892
314.848363	58.987194	74.688897
314.347387	67.582203	74.693902
314.086609	58.096587	74.698906
313.184919	68.294468	74.703911
312.571553	57.647715	74.708916
311.994530	63.325052	74.713921
311.476099	60.230484	74.718926
310.528045	53.319026	74.723930
309.618641	65.396165	74.728935
309.598583	59.189882	74.733940
308.706101	49.328742	74.738945
307.402725	55.293717	74.743950
307.173719	53.070752	74.748954
306.597033	70.580734	74.753959
306.240554	63.357384	74.758964
304.997278	65.678142	74.763969
304.367696	64.890879	74.768974
304.356125	65.518898	74.773978
302.952044	66.603804	74.778983
302.262326	57.262244	74.783988
301.647778	60.791583	74.788993
301.205938	74.623359	74.793998
300.889133	38.076873	74.799002
300.303100	71.019401	74.804007
299.477225	64.939971	74.809012
298.501063	62.597983	74.814017
298.114222	60.799116	74.819022
297.461986	55.005810	74.824026
296.279534	62.512602	74.829031
296.017906	61.753424	74.834036
295.638761	61.842400	74.839041
294.568729	63.943175	74.844046
293.720687	57.047320	74.849050
292.822459	63.438132	74.854055
292.703347	47.341863	74.859060
291.917348	54.750774	74.864065
291.500912	53.522717	74.869070
290.888623	48.781115	74.874074
289.828654	54.152251	74.879079
289.566017	48.787255	74.884084
289.301697	57.049670	74.889089
288.134113	59.367832	74.894094
287.646124	41.054967	74.899098
286.739726	56.197021	74.904103
285.871146	53.423180	74.909108
285.100275	58.891735	74.914113
284.579944	60.066014	74.919118
284.689671	43.031317	74.924122
283.341755	55.313956	74.929127
282.694060	58.749241	74.934132
282.120456	50.828851	74.939137
281.456848	56.234581	74.944142
281.131474	46.283066	74.949146
279.880571	56.826748	74.954151
279.197329	48.930142	74.959156
278.647003	57.443135	74.964161
278.074931	50.921169	74.969166
277.595385	59.247850	74.974170
276.347551	55.347093	74.979175
275.949680	53.133701	74.984180
275.772289	55.229390	74.989185
275.205576	56.601862	74.994190
274.290398	56.874045	74.999194
273.181687	73.546374	75.004199
272.818285	58.493489	75.009204
272.701117	65.321173	75.014209
271.559091	66.048957	75.019214
271.031805	55.695987	75.024218
269.981156	66.871616	75.029223
269.733244	54.022113	75.034228
269.189496	57.549634	75.039233
268.080283	66.432395	75.044238
267.721948	57.258787	75.049242
267.124540	68.281755	75.054247
266.259975	57.159429	75.059252
265.591204	61.895825	75.064257
264.816132	61.603243	75.069262
264.674765	63.275326	75.074266
263.310598	62.348137	75.079271
262.863882	56.692382	75.084276
262.241278	55.479847	75.089281
261.847216	48.789173	75.094286
260.758278	50.423072	75.099290
259.746926	60.002970	75.104295
259.185415	56.059052	75.109300
259.024451	65.285799	75.114305
258.689465	62.603521	75.119310
258.250866	60.666265	75.124314
256.886103	59.512108	75.129319
256.088511	54.051048	75.134324
255.708280	54.728369	75.139329
255.344741	58.413236	75.144334
254.105517	59.009874	75.149338
253.537313	64.012500	75.154343
253.321241	58.329444	75.159348
252.709594	60.267288	75.164353
251.471465	64.162525	75.169358
250.786645	44.121281	75.174362
250.169707	59.013791	75.179367
250.384640	58.456180	75.184372
248.778759	59.850808	75.189377
247.863956	59.832800	75.194382
247.602884	48.537027	75.199386
246.943986	64.289306	75.204391
246.850043	60.564154	75.209396
246.194718	63.527609	75.214401
245.222723	72.691264	75.219406
245.007474	55.941735	75.224410
243.861483	59.349232	75.229415
242.838483	57.251262	75.234420
242.258725	53.999342	75.239425
241.580777	61.752144	75.244430
241.313462	56.244405	75.249434
240.253113	72.631507	75.254439
239.461978	55.079704	75.259444
238.983704	53.079396	75.264449
238.120761	72.995559	75.269454
238.411239	51.431712	75.274458
237.870236	53.454486	75.279463
236.387918	65.905225	75.284468
236.169356	61.578659	75.289473
235.275932	48.980292	75.294478
234.359417	70.149125	75.299482
233.353847	39.292945	75.304487
232.928738	74.855773	75.309492
232.812619	53.085520	75.314497
232.158698	57.717060	75.319502
231.398604	58.399748	75.324506
230.478058	62.345287	75.329511
230.218225	50.454846	75.334516
229.942215	48.316649	75.339521
228.438943	64.359639	75.344526
228.037317	60.675652	75.349530
227.220489	64.946836	75.354535
226.761249	51.393067	75.359540
225.864974	62.892581	75.364545
225.188579	67.188685	75.369550
224.630015	56.544269	75.374554
224.067807	58.802223	75.379559
222.786555	65.716133	75.384564
222.417194	50.069750	75.389569
221.788124	56.483901	75.394574
221.457729	54.368565	75.399578
220.993135	57.568107	75.404583
220.470103	61.989564	75.409588
219.817050	50.639595	75.414593
218.980945	55.907267	75.419598
218.140380	55.640908	75.424602
217.245076	65.757374	75.429607
216.805712	55.349408	75.434612
216.249853	55.419262	75.439617
215.107935	65.332207	75.444622
214.616863	57.029695	75.449626
214.019135	62.746617	75.454631
213.632426	54.976214	75.459636
212.428992	56.052836	75.464641
211.739037	61.320866	75.469646
211.504880	54.860160	75.474650
210.793880	51.438373	75.479655
210.651983	51.539999	75.484660
209.513526	62.431616	75.489665
208.605956	60.476098	75.494670
208.534410	49.914891	75.499674
207.416604	68.897189	75.504679
206.409266	60.714825	75.509684
206.166591	49.956986	75.514689
205.054662	61.295354	75.519694
205.077947	52.166576	75.524698
204.618233	59.127706	75.529703
203.627870	52.312924	75.534708
202.911956	52.712628	75.539713
202.532706	59.514284	75.544718
201.336030	51.735825	75.549722
200.819506	57.480799	75.554727
199.937853	52.009510	75.559732
199.701504	50.131481	75.564737
199.106512	57.954637	75.569742
198.385201	45.663145	75.574746
197.221528	59.258349	75.579751
197.039038	58.172773	75.584756
196.370740	57.803269	75.589761
195.202176	59.161328	75.594766
194.875412	49.186401	75.599770
193.817388	55.233732	75.604775
193.761957	62.078376	75.609780
193.428638	55.892084	75.614785
191.969079	69.042493	75.619790
191.793150	56.798079	75.624794
190.885937	61.864223	75.629799
190.469616	56.028611	75.634804
189.533099	57.553091	75.639809
188.642551	64.444148	75.644814
188.169877	66.536460	75.649818
187.667663	66.662418	75.654823
187.298476	55.823831	75.659828
186.512040	63.611286	75.664833
185.694042	63.896392	75.669838
185.650828	55.923009	75.674842
184.311242	69.404354	75.679847
183.504804	62.030433	75.684852
183.077893	50.142987	75.689857
182.473173	54.374058	75.694862
181.784336	56.956541	75.699866
180.797384	59.988650	75.704871
180.086228	48.449279	75.709876
180.081998	60.103031	75.714881
178.974674	67.255719	75.719886
178.283406	56.334450	75.724890
177.630108	56.743101	75.729895
177.219942	53.940369	75.734900
176.816029	60.107335	75.739905
175.409258	52.568953	75.744910
174.958764	43.257116	75.749914
174.245442	62.096084	75.754919
173.875037	66.685592	75.759924
173.480161	55.486852	75.764929
172.175315	55.862196	75.769934
171.714850	57.985677	75.774938
170.973932	67.025783	75.779943
170.852411	49.845049	75.784948
169.723838	52.426685	75.789953
168.662837	55.913698	75.794958
168.533073	49.996138	75.799962
168.155717	50.389180	75.804967
167.640822	48.945047	75.809972
166.223823	63.200354	75.814977
165.751105	59.333762	75.819982
165.563341	52.782094	75.824986
164.389150	67.998417	75.829991
163.666353	52.102492	75.834996
163.389445	52.766507	75.840001
162.700776	66.309648	75.845006
162.269117	56.802427	75.850010
161.258172	64.447499	75.855015
160.513572	64.402387	75.860020
160.213755	64.134983	75.865025
158.916874	67.393123	75.870030
158.391403	56.212054	75.875034
157.736659	60.189350	75.880039
157.220476	60.759060	75.885044
157.041663	54.187044	75.890049
155.990373	60.324774	75.895054
155.346329	64.090644	75.900058
154.591697	58.398860	75.905063
154.224016	55.256643	75.910068
153.247962	54.382747	75.915073
152.573888	60.643249	75.920078
152.036071	48.538547	75.925082
151.404112	56.149999	75.930087
150.792708	48.601508	75.935092
149.975570	50.378187	75.940097
149.091888	55.875800	75.945102
149.088064	49.704789	75.950106
148.063419	59.819815	75.955111
146.791159	61.602834	75.960116
146.381162	51.314781	75.965121
145.680057	60.477841	75.970126
145.546354	51.960688	75.975130
145.210233	56.353931	75.980135
144.149342	53.826836	75.985140
143.642130	54.406156	75.990145
142.983484	60.719390	75.995150
141.618055	53.781525	76.000154
140.748431	54.043340	76.005159
140.237202	52.123996	76.010164
140.304476	46.395784	76.015169
139.877967	66.073640	76.020174
139.454283	49.515066	76.025178
138.242001	53.962859	76.030183
137.406039	52.421702	76.035188
137.064326	59.173225	76.040193
135.835850	45.171327	76.045198
135.915223	51.836784	76.050202
134.542321	52.645595	76.055207
134.239068	46.613787	76.060212
133.411905	51.443269	76.065217
132.686333	57.223163	76.070222
132.122500	55.163984	76.075226
131.509641	56.102328	76.080231
131.249311	52.646552	76.085236
130.322599	52.244159	76.090241
129.642669	56.493541	76.095246
129.419065	49.017255	76.100250
128.295517	60.500992	76.105255
127.455273	53.253906	76.110260
127.413888	49.916175	76.115265
125.860556	64.912281	76.120270
125.174743	57.216398	76.125274
124.240553	59.607798	76.130279
124.057013	51.664684	76.135284
123.750521	51.805175	76.140289
123.258233	56.929749	76.145294
122.620678	49.877414	76.150298
121.417313	53.339840	76.155303
121.013462	55.982545	76.160308
120.371476	49.515928	76.165313
119.405527	61.978992	76.170318
118.541420	45.501695	76.175322
118.241710	55.050155	76.180327
117.733132	55.393170	76.185332
117.382257	41.692868	76.190337
116.033837	52.400384	76.195342
115.895059	45.475088	76.200346
115.598766	63.373991	76.205351
114.253913	51.500482	76.210356
113.624686	47.871736	76.215361
112.728004	55.001892	76.220366
112.472957	46.056272	76.225370
111.862552	60.621346	76.230375
110.835434	55.258438	76.235380
110.212384	50.898627	76.240385
109.737807	58.757787	76.245390
109.622955	53.686199	76.250394
108.320617	63.509651	76.255399
107.474034	56.230470	76.260404
107.343136	42.294832	76.265409
106.575190	51.052265	76.270414
105.784940	53.058044	76.275418
104.945956	52.722091	76.280423
104.608483	51.948223	76.285428
103.738737	42.935058	76.290433
102.547828	53.592234	76.295438
102.242737	52.915698	76.300442
101.361218	55.621961	76.305447
101.136898	71.423227	76.310452
100.708452	57.359994	76.315457
100.049393	53.565708	76.320462
99.649193	58.148934	76.325466
98.612226	60.482621	76.330471
97.967544	45.979250	76.335476
97.063041	47.918100	76.340481
95.961081	54.142771	76.345486
95.861359	50.741809	76.350490
95.393393	58.492690	76.355495
94.695253	53.742760	76.360500
93.958665	51.961859	76.365505
92.965358	65.621392	76.370510
92.646284	55.448154	76.375514
92.170185	62.022429	76.380519
90.940595	58.951440	76.385524
90.267558	48.148724	76.390529
89.652028	54.660081	76.395534
89.433417	56.926345	76.400538
89.218231	60.147633	76.405543
87.843998	50.197852	76.410548
87.269389	57.387036	76.415553
86.571400	62.304739	76.420558
85.970124	61.989229	76.425562
85.079828	63.414921	76.430567
84.606379	58.643354	76.435572
84.371592	49.801732	76.440577
83.197136	52.994654	76.445582
82.432639	50.595353	76.450586
81.589645	51.647673	76.455591
81.280478	49.850652	76.460596
81.141415	52.014350	76.465601
80.133067	57.894540	76.470606
79.471517	56.803374	76.475610
79.042854	59.150442	76.480615
77.790991	58.069840	76.485620
77.253117	48.980106	76.490625
76.354960	56.263463	76.495630
76.193947	45.006966	76.500634
75.521881	56.193230	76.505639
74.741419	60.852869	76.510644
74.285002	54.903838	76.515649
73.136765	59.049732	76.520654
72.903965	50.914222	76.525658
71.704211	64.338618	76.530663
70.946828	52.491292	76.535668
70.551447	49.906983	76.540673
69.661894	55.279408	76.545678
69.745749	52.634442	76.550682
69.324875	55.511665	76.555687
68.199731	60.361883	76.560692
67.704026	52.550556	76.565697
67.094601	58.570546	76.570702
66.028848	52.084799	76.575706
65.235880	49.978607	76.580711
64.381286	66.317165	76.585716
64.333496	39.550092	76.590721
63.574103	54.153116	76.595726
62.823297	64.352225	76.600730
61.993288	50.835566	76.605735
61.445038	44.054422	76.610740
61.505657	54.494679	76.615745
60.135774	56.823130	76.620750
59.462678	45.124788	76.625754
58.920856	44.590084	76.630759
57.978838	48.499680	76.635764
57.322661	62.777191	76.640769
56.291402	59.425449	76.645774
55.752753	35.677489	76.650778
55.482617	58.364242	76.655783
55.357192	53.418918	76.660788
55.088976	49.858762	76.665793
53.488354	57.952699	76.670798
53.187494	53.497370	76.675802
52.306982	46.576841	76.680807
51.314228	38.991443	76.685812
50.959956	41.771318	76.690817
50.198623	49.603676	76.695822
49.754623	54.452495	76.700826
48.740379	64.717273	76.705831
47.944796	45.851200	76.710836
47.506633	46.780624	76.715841
47.103042	51.831141	76.720846
46.622701	52.798830	76.725850
45.399806	56.201332	76.730855
44.770048	52.651532	76.735860
44.486813	59.598726	76.740865
44.126201	63.412452	76.745870
42.947129	52.037641	76.750874
42.175577	41.033056	76.755879
41.717409	73.530993	76.760884
41.323992	55.822828	76.765889
40.409268	59.102072	76.770894
39.954769	56.571348	76.775898
39.297733	44.036303	76.780903
38.904931	54.886316	76.785908
37.958060	40.574665	76.790913
36.757333	57.182871	76.795918
36.685528	48.398839	76.800922
35.273421	45.090506	76.805927
34.320487	57.199875	76.810932
34.470513	58.656770	76.815937
33.769093	58.144371	76.820942
33.529468	49.404449	76.825946
32.339340	53.698956	76.830951
31.434817	53.898571	76.835956
31.119571	36.928545	76.840961
30.678749	49.340982	76.845966
30.229143	48.045729	76.850970
29.461361	49.865032	76.855975
28.403041	62.059020	76.860980
28.094944	52.691394	76.865985
26.938887	53.333225	76.870990
25.988011	52.590974	76.875994
25.921509	59.117273	76.880999
25.236799	66.514831	76.886004
24.885719	41.229494	76.891009
23.571464	65.467253	76.896014
23.166557	52.973989	76.901018
22.505891	43.612145	76.906023
22.065033	65.946114	76.911028
21.324987	57.744866	76.916033
20.111518	57.046076	76.921038
19.841893	44.679468	76.926042
19.424871	54.245062	76.931047
18.324162	57.104576	76.936052
17.569646	48.754265	76.941057
17.103938	52.275692	76.946062
16.754334	56.718402	76.951066
16.187798	61.968368	76.956071
15.277290	54.213754	76.961076
14.615456	44.226090	76.966081
13.463407	72.132539	76.971086
13.488485	50.428138	76.976090
12.991314	47.610934	76.981095
11.922786	63.192042	76.986100
11.639859	55.042461	76.991105
10.834236	54.193476	76.996110
9.827231	50.260764	77.001114
9.159793	52.491395	77.006119
7.995067	66.522043	77.011124
8.296654	37.220464	77.016129
7.599602	57.316742	77.021134
6.813458	46.637750	77.026139
6.138546	49.164442	77.031143
5.272056	64.459457	77.036148
5.074876	50.430333	77.041153
3.747661	49.170992	77.046158