Mon Mar 08 19:33:00 2021

Number of Points = 14582

Depth (nm)	Load (N)	Time (s)
-1.055792	91.673467	0.000000
-1.227272	77.624406	0.005005
-1.634495	43.746268	0.010010
-3.624020	5.229217	0.015014
-7.710538	-11.978163	0.020019
-13.290991	-2.796937	0.025024
-18.361239	-2.538418	0.030029
-22.481181	-4.013037	0.035034
-26.781451	3.951698	0.040038
-30.203049	-16.505913	0.045043
-34.191447	-1.865697	0.050048
-38.110795	-4.494995	0.055053
-41.629903	-1.982981	0.060058
-45.462572	-6.702791	0.065062
-48.352612	-6.845592	0.070067
-52.248381	-1.591277	0.075072
-56.006390	0.112103	0.080077
-59.881158	-7.694726	0.085082
-64.301947	4.297621	0.090086
-67.775022	-6.633920	0.095091
-71.634782	1.399380	0.100096
-75.255128	7.702547	0.105101
-78.868622	-6.041736	0.110106
-83.032074	1.163305	0.115110
-86.357304	-3.520703	0.120115
-90.568675	-9.255428	0.125120
-94.156197	-0.347806	0.130125
-97.415873	-11.887311	0.135130
-101.538082	-1.238699	0.140134
-105.341707	-9.257059	0.145139
-108.952038	-1.987267	0.150144
-112.646869	-2.733249	0.155149
-116.380501	-9.562784	0.160154
-120.733940	-2.243799	0.165158
-124.113389	-14.111058	0.170163
-127.768060	1.012179	0.175168
-131.832873	-5.146373	0.180173
-135.335099	-12.116867	0.185178
-139.524109	-6.394616	0.190182
-142.963992	-10.598235	0.195187
-146.598303	-16.937399	0.200192
-150.264304	-0.866223	0.205197
-153.978802	-14.196895	0.210202
-158.052472	-4.467352	0.215206
-161.636280	-22.905733	0.220211
-165.776148	-11.861576	0.225216
-169.698345	-6.631247	0.230221
-173.076173	-12.889880	0.235226
-177.682231	-3.810161	0.240230
-181.240572	-12.182900	0.245235
-184.416972	-1.877452	0.250240
-188.414894	-9.823672	0.255245
-191.838184	-12.680094	0.260250
-196.010108	-3.112994	0.265254
-199.199315	-18.227239	0.270259
-202.837228	-5.687861	0.275264
-206.911999	-11.590819	0.280269
-210.681913	-12.062913	0.285274
-214.936720	-4.734278	0.290278
-218.273463	-13.834552	0.295283
-222.161355	-4.237049	0.300288
-225.641314	-6.925120	0.305293
-229.315567	-4.403848	0.310298
-233.061676	-3.181454	0.315302
-236.965671	-22.451637	0.320307
-240.866428	-2.321949	0.325312
-244.821904	-10.651708	0.330317
-248.026840	-16.043757	0.335322
-252.305084	-4.442826	0.340326
-255.919397	-18.054220	0.345331
-259.875092	-2.067542	0.350336
-263.352446	-13.294535	0.355341
-267.041034	-9.493683	0.360346
-271.059566	-10.533084	0.365350
-274.736549	-16.630286	0.370355
-278.324644	-12.643624	0.375360
-282.485034	-1.635420	0.380365
-285.716504	-13.199645	0.385370
-289.709085	-4.892527	0.390374
-293.664588	-6.014484	0.395379
-297.330085	-10.159789	0.400384
-300.901285	-18.569704	0.405389
-304.416567	-8.637347	0.410394
-308.509809	-6.209915	0.415398
-312.304075	-19.210638	0.420403
-316.102417	-6.262327	0.425408
-319.865104	-9.192111	0.430413
-323.386435	-16.264913	0.435418
-327.406933	-10.446256	0.440422
-331.099270	-5.547233	0.445427
-334.798220	-8.841955	0.450432
-338.514345	-6.775849	0.455437
-342.159373	-19.182224	0.460442
-346.881576	2.275565	0.465446
-350.150837	-9.597903	0.470451
-353.708738	-1.647057	0.475456
-357.795730	-6.324178	0.480461
-360.968822	-5.503700	0.485466
-364.766975	-5.373424	0.490470
-368.544697	-15.210412	0.495475
-372.590707	-1.670585	0.500480
-375.807806	-4.644808	0.505485
-379.894316	-17.559339	0.510490
-384.155922	-7.420996	0.515494
-387.575223	1.324570	0.520499
-391.364152	-5.210284	0.525504
-395.437721	-0.253452	0.530509
-398.900874	-5.416425	0.535514
-402.620818	6.459873	0.540518
-406.512192	-3.333684	0.545523
-409.955472	4.691975	0.550528
-413.797422	3.593083	0.555533
-417.401228	-8.053418	0.560538
-421.437733	6.871010	0.565542
-425.171036	-1.643714	0.570547
-429.007374	-6.884239	0.575552
-433.020328	5.955027	0.580557
-436.389155	-7.179651	0.585562
-440.264906	4.967563	0.590566
-443.843239	-4.984715	0.595571
-447.542210	-5.784708	0.600576
-451.724193	-8.874392	0.605581
-455.270719	-5.343505	0.610586
-459.370928	-4.682335	0.615590
-462.972466	-0.693255	0.620595
-466.275548	-8.235897	0.625600
-469.999811	-5.222190	0.630605
-473.957949	-11.095997	0.635610
-478.006673	-8.006813	0.640614
-481.829598	-0.587433	0.645619
-485.400527	-5.315204	0.650624
-489.245129	-7.539406	0.655629
-492.570975	-8.927153	0.660634
-496.710792	2.171146	0.665638
-500.633931	-8.993745	0.670643
-504.083674	-6.930506	0.675648
-507.794319	-6.984276	0.680653
-511.345930	-5.633253	0.685658
-515.700819	1.984669	0.690662
-519.158429	3.128318	0.695667
-523.093619	-2.187721	0.700672
-527.392792	-1.329091	0.705677
-530.471329	-6.562754	0.710682
-534.276226	-3.297969	0.715686
-538.097164	-1.240045	0.720691
-541.634428	1.658756	0.725696
-545.498710	3.684194	0.730701
-549.122865	-5.752855	0.735706
-553.126036	-2.052704	0.740710
-556.898405	-4.253643	0.745715
-560.407770	-0.041040	0.750720
-564.422713	-3.646022	0.755725
-568.011416	-4.849763	0.760730
-571.786710	6.606719	0.765734
-575.735098	-1.933318	0.770739
-579.329560	-1.264425	0.775744
-583.225051	-2.794424	0.780749
-586.906322	-9.644169	0.785754
-591.091057	13.003861	0.790758
-594.373744	-8.200360	0.795763
-598.237381	-1.067589	0.800768
-602.121514	-6.708590	0.805773
-605.692785	-5.827336	0.810778
-609.483020	-0.606353	0.815782
-613.308800	-3.694308	0.820787
-617.119084	-1.975403	0.825792
-620.955860	-6.389279	0.830797
-624.219986	0.452233	0.835802
-628.563302	-3.642609	0.840806
-632.299348	2.381820	0.845811
-635.742543	-4.980507	0.850816
-639.463052	-2.626255	0.855821
-643.051784	-6.696552	0.860826
-647.141325	-0.860036	0.865830
-651.027574	-4.701454	0.870835
-654.847450	-6.290719	0.875840
-658.435090	4.527252	0.880845
-662.288875	2.114002	0.885850
-666.034339	-5.416011	0.890854
-669.310602	-10.201610	0.895859
-673.145976	-10.689320	0.900864
-677.190439	-5.720906	0.905869
-680.895601	-11.346214	0.910874
-684.745843	-2.212880	0.915878
-688.407392	-8.843277	0.920883
-691.906135	-6.693099	0.925888
-696.203683	3.986062	0.930893
-699.533500	-10.086340	0.935898
-703.552247	-9.831975	0.940902
-707.665280	-8.204889	0.945907
-711.103858	0.072718	0.950912
-715.044746	-5.950075	0.955917
-718.416373	-10.879625	0.960922
-722.366276	-0.456231	0.965926
-726.429001	-2.080686	0.970931
-729.871740	-12.372682	0.975936
-733.623999	-6.583614	0.980941
-736.897070	-13.562991	0.985946
-741.377014	-0.174005	0.990950
-744.860387	-0.787230	0.995955
-748.599981	-12.294797	1.000960
-752.613841	-2.439833	1.005965
-756.422830	-6.127852	1.010970
-759.787468	-6.550311	1.015974
-763.742991	-3.973821	1.020979
-767.454261	-6.278793	1.025984
-771.506317	0.094368	1.030989
-774.842542	-12.251841	1.035994
-778.856395	-3.590493	1.040998
-782.119714	-5.263768	1.046003
-786.123233	-2.146603	1.051008
-790.285265	-3.999483	1.056013
-793.978924	-11.058203	1.061018
-797.552944	3.376599	1.066022
-801.334942	-1.323254	1.071027
-805.280068	-6.433807	1.076032
-808.897213	-1.839375	1.081037
-812.722579	-13.536533	1.086042
-816.546885	-7.138206	1.091046
-820.394422	-1.973966	1.096051
-823.787649	-10.192320	1.101056
-827.592376	-1.226878	1.106061
-831.237477	-13.096308	1.111066
-835.048685	-9.833197	1.116070
-839.022251	-6.857916	1.121075
-842.725796	-7.759051	1.126080
-846.824828	-7.080058	1.131085
-850.211941	-2.743090	1.136090
-853.604029	-11.470894	1.141094
-857.616545	-7.152209	1.146099
-861.573255	-14.001624	1.151104
-865.518977	-3.156089	1.156109
-869.335816	-5.650586	1.161114
-873.021360	-8.082494	1.166118
-876.376738	-6.853755	1.171123
-880.187716	-10.413527	1.176128
-884.110479	-7.859420	1.181133
-887.482916	-13.267943	1.186138
-891.514260	-8.058441	1.191142
-895.833221	-4.685678	1.196147
-899.185872	-7.888217	1.201152
-903.177527	-14.687821	1.206157
-906.270006	-14.257944	1.211162
-910.065223	3.572584	1.216166
-914.308576	-11.539201	1.221171
-917.937726	-2.313134	1.226176
-921.949245	-3.718372	1.231181
-925.562104	-2.993978	1.236186
-929.477878	-13.765071	1.241190
-932.882912	-8.173128	1.246195
-936.712484	-13.883773	1.251200
-940.598256	1.121417	1.256205
-944.429756	-20.815991	1.261210
-948.351630	-5.606345	1.266214
-951.711306	-7.013260	1.271219
-955.627128	-12.820460	1.276224
-959.382306	-11.961304	1.281229
-962.654899	-18.101554	1.286234
-967.043259	-7.044750	1.291238
-970.690064	-2.893153	1.296243
-974.127760	-20.468909	1.301248
-978.337549	-14.901175	1.306253
-981.775196	-10.294193	1.311258
-985.972662	-10.822832	1.316262
-989.150789	-15.242069	1.321267
-992.885437	-8.630743	1.326272
-996.853959	-9.410420	1.331277
-1000.384717	-10.400431	1.336282
-1004.671257	-17.587900	1.341286
-1008.701022	-5.426249	1.346291
-1012.041674	-16.151979	1.351296
-1016.407873	-0.727680	1.356301
-1019.460398	-11.531016	1.361306
-1023.118845	-5.707625	1.366310
-1026.789709	-5.273396	1.371315
-1030.228646	-6.448343	1.376320
-1034.812771	0.250021	1.381325
-1038.664149	-16.430064	1.386330
-1042.215331	-6.615521	1.391334
-1045.727722	-9.134764	1.396339
-1049.361427	-9.185795	1.401344
-1053.423972	-9.737468	1.406349
-1057.172156	-7.731348	1.411354
-1061.109782	-8.391288	1.416358
-1064.885316	-2.350427	1.421363
-1068.173766	-16.823063	1.426368
-1072.206388	-3.330017	1.431373
-1075.687068	-13.651664	1.436378
-1079.934182	-3.598033	1.441382
-1083.644849	-0.000552	1.446387
-1087.246524	-11.598976	1.451392
-1090.938931	-4.896493	1.456397
-1094.416631	-7.980981	1.461402
-1098.454997	-2.770009	1.466406
-1102.261233	-4.510520	1.471411
-1106.023507	-5.721936	1.476416
-1109.819764	-6.405984	1.481421
-1113.349679	-19.669920	1.486426
-1117.226983	-14.085749	1.491430
-1121.265739	-7.165406	1.496435
-1124.641725	-10.917344	1.501440
-1128.964843	-6.132241	1.506445
-1132.351853	-9.906058	1.511450
-1135.984002	-13.364709	1.516454
-1140.106475	-7.700282	1.521459
-1143.447673	-19.570490	1.526464
-1147.648127	-3.701017	1.531469
-1151.152187	-14.349934	1.536474
-1154.631403	-6.506730	1.541478
-1158.590079	-16.858996	1.546483
-1162.301593	-13.302258	1.551488
-1166.364324	-5.569095	1.556493
-1170.095119	-18.688847	1.561498
-1174.235622	0.184382	1.566502
-1177.556749	-20.020897	1.571507
-1181.017227	-9.033327	1.576512
-1184.838239	-0.383252	1.581517
-1188.348425	1.056764	1.586522
-1192.328623	-6.691829	1.591526
-1196.525233	-9.970196	1.596531
-1199.913320	-10.541220	1.601536
-1204.088608	-14.106810	1.606541
-1207.203032	-12.961880	1.611546
-1211.294019	-10.072839	1.616550
-1215.308218	0.751090	1.621555
-1219.116219	-13.582992	1.626560
-1222.427419	-14.163131	1.631565
-1226.040854	-16.448327	1.636570
-1230.276036	-9.423840	1.641574
-1233.986814	-12.256372	1.646579
-1237.908828	-15.944421	1.651584
-1241.766865	-10.572848	1.656589
-1244.826978	-16.100188	1.661594
-1248.640529	-17.001993	1.666598
-1252.573178	-14.817826	1.671603
-1256.273494	-4.521837	1.676608
-1260.633971	-5.517438	1.681613
-1264.090819	-9.907455	1.686618
-1267.600883	-14.985901	1.691622
-1271.644958	-13.286875	1.696627
-1275.201951	-15.024408	1.701632
-1279.204782	-1.277202	1.706637
-1282.865813	-14.043679	1.711642
-1286.603972	-9.476473	1.716646
-1290.325934	-4.963887	1.721651
-1293.664239	-16.298206	1.726656
-1298.173997	0.581298	1.731661
-1301.619902	-11.506856	1.736666
-1305.488928	-7.147314	1.741670
-1309.346413	-11.581941	1.746675
-1312.726832	-3.301779	1.751680
-1316.979147	-7.160738	1.756685
-1320.166419	-10.453774	1.761690
-1324.365973	-10.006993	1.766694
-1328.055627	-4.113497	1.771699
-1331.341861	-15.019314	1.776704
-1335.546974	-4.358586	1.781709
-1338.993229	-10.689666	1.786714
-1343.043300	-23.106782	1.791718
-1346.686370	-11.611987	1.796723
-1350.499394	-10.987351	1.801728
-1354.314468	-9.507747	1.806733
-1357.913651	-15.404344	1.811738
-1361.810655	-15.800638	1.816742
-1365.610194	-9.386494	1.821747
-1369.106568	-17.475534	1.826752
-1373.310852	-12.199701	1.831757
-1376.503861	-14.315433	1.836762
-1380.193434	-17.119583	1.841766
-1384.368244	-15.842519	1.846771
-1388.309784	-19.162936	1.851776
-1392.296113	-6.662304	1.856781
-1395.845176	-13.938693	1.861786
-1399.447639	-3.311257	1.866790
-1402.882600	-13.114614	1.871795
-1406.720023	-16.614078	1.876800
-1410.590936	-10.483302	1.881805
-1414.345876	-13.502416	1.886810
-1418.352436	-11.580504	1.891814
-1422.087641	-4.066491	1.896819
-1425.352202	-17.290394	1.901824
-1429.791975	-4.463240	1.906829
-1433.064115	-16.823400	1.911834
-1436.794010	-19.106960	1.916838
-1441.090105	-7.218919	1.921843
-1444.666510	-15.859525	1.926848
-1448.356653	-23.204692	1.931853
-1451.786065	-13.847421	1.936858
-1455.843347	-21.854399	1.941862
-1459.619064	-4.653787	1.946867
-1463.176367	-15.924393	1.951872
-1467.270449	-5.235491	1.956877
-1470.980617	-10.344652	1.961882
-1474.856342	-8.429399	1.966886
-1478.575800	-1.542237	1.971891
-1481.828951	-20.065971	1.976896
-1486.182251	-7.728762	1.981901
-1489.548559	-6.211992	1.986906
-1493.319175	-14.594360	1.991910
-1497.085624	2.440842	1.996915
-1501.208538	-12.432757	2.006912
-1501.933111	-10.669754	2.016909
-1499.731937	-8.907907	2.026906
-1496.755523	-6.583401	2.036902
-1494.762570	-10.015721	2.046899
-1492.572579	-11.774451	2.056896
-1490.596604	-19.763713	2.066893
-1489.041890	-9.228979	2.076890
-1487.229247	-5.428210	2.086886
-1485.389621	-7.227141	2.096883
-1483.083488	-6.048885	2.106880
-1481.037544	-12.868379	2.116877
-1479.590048	-9.852234	2.126874
-1477.452035	-5.370975	2.136870
-1475.909482	-11.405705	2.146867
-1473.731508	-10.249548	2.156864
-1471.722211	-12.356667	2.166861
-1469.826765	-10.864764	2.176858
-1468.218482	-9.382140	2.186854
-1466.105846	-7.478199	2.196851
-1464.198201	-8.538059	2.206848
-1462.393145	-10.920342	2.216845
-1460.448223	-8.807977	2.226842
-1458.954529	-12.210853	2.236838
-1456.795741	-10.705844	2.246835
-1454.898838	-17.150952	2.256832
-1452.725032	-15.195218	2.266829
-1451.229225	-13.148299	2.276826
-1449.142151	-13.406408	2.286822
-1447.327983	-4.946714	2.296819
-1445.295490	-8.723194	2.306816
-1443.665440	-9.340727	2.316813
-1441.460810	-8.802972	2.326810
-1439.778849	-12.619636	2.336806
-1437.878467	-6.919327	2.346803
-1436.287646	-6.310137	2.356800
-1434.150967	-5.962008	2.366797
-1432.299119	-3.192131	2.376794
-1430.623201	-6.174198	2.386790
-1428.435709	-2.419181	2.396787
-1426.552075	-0.259081	2.406784
-1424.541899	-7.396467	2.416781
-1422.949920	-8.281029	2.426778
-1420.728925	-7.659039	2.436774
-1419.270732	-10.047333	2.446771
-1417.153390	-11.570168	2.456768
-1415.232424	-6.128905	2.466765
-1413.546541	-6.832719	2.476762
-1411.942069	-8.191345	2.486758
-1409.687887	-1.611400	2.496755
-1407.820227	-10.082175	2.506752
-1406.165851	-13.971762	2.516749
-1403.638049	-9.540201	2.526746
-1401.992368	-7.468296	2.536742
-1400.439894	-3.999989	2.546739
-1398.402204	-3.534935	2.556736
-1396.583524	-6.858756	2.566733
-1394.477049	-3.488602	2.576730
-1392.732901	-14.205220	2.586726
-1391.226123	-7.001965	2.596723
-1389.090697	-2.357585	2.606720
-1387.176666	-11.287315	2.616717
-1385.132158	-11.090163	2.626714
-1383.486528	-4.918004	2.636710
-1381.447669	-5.801447	2.646707
-1379.636866	-12.624269	2.656704
-1377.596429	-8.503056	2.666701
-1375.784180	-10.134900	2.676698
-1373.998948	-9.716249	2.686694
-1372.220186	-10.403323	2.696691
-1370.456333	-3.059636	2.706688
-1368.454603	-8.185768	2.716685
-1366.453762	-8.264222	2.726682
-1364.903589	-3.065118	2.736678
-1362.755956	-2.843404	2.746675
-1360.573327	-5.710754	2.756672
-1358.880753	-8.123898	2.766669
-1357.168088	-2.012970	2.776666
-1355.129746	-6.320800	2.786662
-1353.368031	-3.883775	2.796659
-1351.467425	-6.237061	2.806656
-1349.652680	-3.770629	2.816653
-1347.723992	-6.000521	2.826650
-1345.623603	-5.531247	2.836646
-1343.867281	-5.668431	2.846643
-1342.428861	-1.059274	2.856640
-1340.278344	-8.266421	2.866637
-1338.231051	-7.464980	2.876634
-1336.393839	-4.673735	2.886630
-1334.613895	-5.116251	2.896627
-1332.566922	-7.338223	2.906624
-1330.769164	-6.700506	2.916621
-1328.983244	-0.255514	2.926618
-1327.392618	-8.176665	2.936614
-1325.470721	-4.461137	2.946611
-1323.153711	-10.363957	2.956608
-1321.109452	-13.054398	2.966605
-1319.649002	-12.217434	2.976602
-1317.733344	-6.167383	2.986598
-1315.876183	-5.150768	2.996595
-1313.913995	-9.878976	3.006592
-1311.966550	-8.043182	3.016589
-1310.026366	-13.416766	3.026586
-1308.452979	-16.758099	3.036582
-1306.404467	-14.572187	3.046579
-1304.472067	-9.236860	3.056576
-1302.499017	-7.024657	3.066573
-1300.824829	-14.458671	3.076570
-1299.049217	-5.129053	3.086566
-1296.855687	-13.075625	3.096563
-1295.131796	-9.281018	3.106560
-1293.632528	-1.064454	3.116557
-1291.359699	-4.857165	3.126554
-1289.328069	-11.964720	3.136550
-1287.624956	-10.613978	3.146547
-1285.962956	-4.147541	3.156544
-1283.917053	-14.486094	3.166541
-1281.936880	-7.963213	3.176538
-1280.143416	-0.924166	3.186534
-1277.995658	-5.967813	3.196531
-1276.367683	-9.840458	3.206528
-1274.588608	-10.094907	3.216525
-1272.712634	-8.602881	3.226522
-1270.731008	-12.530536	3.236518
-1269.055458	-7.989278	3.246515
-1267.094675	-5.816130	3.256512
-1265.180564	-3.494995	3.266509
-1263.151113	-11.522642	3.276506
-1261.250100	-8.744704	3.286502
-1259.459319	-3.274574	3.296499
-1257.450292	-9.437501	3.306496
-1255.821653	-10.255190	3.316493
-1253.877815	-6.442066	3.326490
-1251.791288	-14.218329	3.336486
-1250.184928	-15.261380	3.346483
-1248.395417	-10.059442	3.356480
-1246.114445	-13.978140	3.366477
-1244.677148	-14.469961	3.376474
-1242.786499	-13.826515	3.386470
-1240.688497	-5.828870	3.396467
-1238.877918	-9.203378	3.406464
-1236.966923	-12.462908	3.416461
-1234.761433	-10.081012	3.426458
-1233.394953	-16.332141	3.436454
-1231.473297	-17.349846	3.446451
-1229.475671	-7.989383	3.456448
-1227.279257	-9.922567	3.466445
-1225.672095	-15.354895	3.476442
-1224.042175	-11.393629	3.486438
-1221.848298	-6.902114	3.496435
-1220.247943	-8.004180	3.506432
-1218.313226	-10.233353	3.516429
-1216.290832	-6.412241	3.526426
-1214.523406	-5.984301	3.536422
-1212.528731	-7.572583	3.546419
-1210.461074	-11.288181	3.556416
-1208.899206	-1.359060	3.566413
-1206.944508	-3.144611	3.576410
-1205.140422	-5.682850	3.586406
-1203.303236	0.136720	3.596403
-1201.186699	-7.974284	3.606400
-1199.547578	-10.157726	3.616397
-1197.335238	-12.276575	3.626394
-1195.463575	-4.921571	3.636390
-1194.161218	-14.474823	3.646387
-1191.838853	-5.294164	3.656384
-1190.117674	-15.890144	3.666381
-1188.010302	-17.085937	3.676378
-1186.281199	-16.460806	3.686374
-1184.385122	-11.732150	3.696371
-1182.660232	-11.958914	3.706368
-1180.559891	-10.837421	3.716365
-1179.008440	-10.139654	3.726362
-1177.144085	-3.478153	3.736358
-1174.867512	-2.408532	3.746355
-1172.901118	-5.267958	3.756352
-1171.150771	-8.489105	3.766349
-1169.467830	-11.892085	3.776346
-1167.835358	-4.588784	3.786342
-1165.712162	-1.164250	3.796339
-1163.535271	-7.150288	3.806336
-1161.885068	-9.534412	3.816333
-1159.964493	-6.023778	3.826330
-1158.080166	-6.037626	3.836326
-1156.263648	-5.626969	3.846323
-1154.369665	0.530902	3.856320
-1152.516645	-6.756380	3.866317
-1150.811744	-2.837050	3.876314
-1148.692655	-8.592791	3.886310
-1146.669776	-2.573948	3.896307
-1145.077432	-3.482064	3.906304
-1143.325495	-7.303405	3.916301
-1141.244130	-9.331781	3.926298
-1139.280301	-1.408878	3.936294
-1137.635446	-9.829610	3.946291
-1135.663367	-13.100411	3.956288
-1133.774785	-8.037376	3.966285
-1131.913565	-5.347692	3.976282
-1130.125850	-3.377250	3.986278
-1127.873724	-4.188806	3.996275
-1126.069421	-11.419330	4.006272
-1124.445599	-9.650020	4.016269
-1122.841259	-8.801213	4.026266
-1120.725865	-3.365527	4.036262
-1118.903340	-3.918893	4.046259
-1116.646446	-7.991504	4.056256
-1114.811848	-8.461541	4.066253
-1113.149357	-6.548418	4.076250
-1111.232784	-8.027813	4.086246
-1109.411191	-4.520248	4.096243
-1107.537352	-4.552902	4.106240
-1105.698997	-10.514736	4.116237
-1103.538991	-8.839071	4.126234
-1101.874728	-6.945170	4.136230
-1099.971587	-13.411537	4.146227
-1097.995348	-9.895545	4.156224
-1096.151369	-10.755463	4.166221
-1094.134692	-11.115669	4.176218
-1092.550527	-9.589450	4.186214
-1090.797462	-12.787291	4.196211
-1088.316274	-9.672562	4.206208
-1086.910655	-14.278410	4.216205
-1085.128997	-8.250927	4.226202
-1083.040864	-6.874779	4.236198
-1081.173805	-8.229395	4.246195
-1079.285205	-5.600885	4.256192
-1077.437986	-10.951526	4.266189
-1075.446924	-11.064479	4.276186
-1074.032216	-12.152541	4.286182
-1071.880953	-9.815494	4.296179
-1069.797301	-13.508270	4.306176
-1068.213704	-9.435275	4.316173
-1066.391020	-12.727912	4.326170
-1064.097729	-8.323189	4.336166
-1062.592121	-11.580900	4.346163
-1060.539749	-12.767783	4.356160
-1058.633357	-17.112679	4.366157
-1056.533131	-12.658125	4.376154
-1055.206476	-15.377244	4.386150
-1053.010727	-15.316087	4.396147
-1051.186206	-17.399615	4.406144
-1049.216663	-25.742747	4.416141
-1047.475743	-16.937860	4.426138
-1045.613847	-18.204786	4.436134
-1043.492375	-17.557043	4.446131
-1041.985628	-19.728680	4.456128
-1039.984240	-26.095455	4.466125
-1038.058586	-17.681659	4.476122
-1036.373638	-17.755095	4.486118
-1034.296961	-17.305429	4.496115
-1032.215282	-24.382886	4.506112
-1030.282059	-18.717473	4.516109
-1028.908318	-11.852657	4.526106
-1026.794856	-8.399596	4.536102
-1024.831886	-11.083102	4.546099
-1023.223130	-11.332226	4.556096
-1021.211368	-14.666119	4.566093
-1018.996116	-13.974933	4.576090
-1017.308523	-11.568421	4.586086
-1015.852054	-12.719966	4.596083
-1013.585182	-7.141045	4.606080
-1011.931407	-10.723978	4.616077
-1009.771748	-4.853189	4.626074
-1007.998826	-10.763439	4.636070
-1006.062637	-7.806185	4.646067
-1004.259230	-13.467113	4.656064
-1002.440194	-14.706626	4.666061
-1000.691926	-16.048498	4.676058
-998.492742	-18.526614	4.686054
-996.740701	-9.641358	4.696051
-994.793418	-11.027681	4.706048
-993.119473	-14.293321	4.716045
-991.224351	-13.434084	4.726042
-989.461005	-6.880996	4.736038
-987.303558	-10.493931	4.746035
-985.302738	-17.122664	4.756032
-983.842236	-16.501796	4.766029
-981.680121	-19.719181	4.776026
-979.999408	-12.230832	4.786022
-977.987373	-13.709595	4.796019
-976.099053	-11.961949	4.806016
-974.214279	-8.458062	4.816013
-972.342081	-9.044519	4.826010
-970.554197	-9.979048	4.836006
-968.710583	-17.211010	4.846003
-966.364535	-9.483268	4.856000
-964.910963	-9.012849	4.865997
-963.170794	-5.837911	4.875994
-961.336505	-9.760706	4.885990
-959.200276	-13.447586	4.895987
-957.107478	-9.858534	4.905984
-955.530368	-9.666791	4.915981
-953.508534	-7.091056	4.925978
-951.860258	-6.029696	4.935974
-949.969490	-15.939007	4.945971
-948.148409	-11.764959	4.955968
-945.929885	-17.741674	4.965965
-944.418313	-16.907909	4.975962
-942.262677	-11.724788	4.985958
-940.622065	-8.592333	4.995955
-938.616821	-11.034650	5.005952
-936.749966	-18.592389	5.015949
-934.856831	-17.098093	5.025946
-933.084670	-11.714713	5.035942
-930.975647	-16.181903	5.045939
-929.189294	-15.128394	5.055936
-927.569791	-11.493641	5.065933
-925.576967	-4.571427	5.075930
-923.352028	-5.016886	5.085926
-921.795481	-5.990177	5.095923
-919.604680	-9.548389	5.105920
-917.977840	-13.182212	5.115917
-915.970604	-8.330577	5.125914
-914.227164	-10.306310	5.135910
-912.732945	-5.800519	5.145907
-910.388206	-6.716668	5.155904
-908.502129	-4.916504	5.165901
-906.630987	-14.633187	5.175898
-905.011149	-4.962556	5.185894
-903.038965	-2.855648	5.195891
-900.844189	-3.395731	5.205888
-899.069439	-14.641107	5.215885
-897.207576	-6.423805	5.225882
-895.572739	-8.304799	5.235878
-893.624691	-6.039299	5.245875
-891.637392	-5.804148	5.255872
-889.734629	-1.995190	5.265869
-887.950617	-14.827198	5.275866
-886.282758	-4.278498	5.285862
-884.289679	-6.521470	5.295859
-882.048559	-9.618776	5.305856
-880.463945	-12.045905	5.315853
-878.509468	-8.175736	5.325850
-876.756634	-12.608044	5.335846
-874.916019	-19.327914	5.345843
-872.964632	-10.646516	5.355840
-870.953512	-13.036035	5.365837
-869.025712	-13.711820	5.375834
-867.158429	-14.254780	5.385830
-865.388577	-11.258186	5.395827
-863.728119	-15.914122	5.405824
-861.686414	-11.899999	5.415821
-859.935368	-15.714681	5.425818
-858.152794	-18.403949	5.435814
-856.288574	-16.505520	5.445811
-854.049385	-13.482895	5.455808
-851.876628	-17.238674	5.465805
-850.479334	-15.005093	5.475802
-848.615648	-17.012629	5.485798
-846.673225	-3.904272	5.495795
-844.934466	-7.110705	5.505792
-842.662553	-6.943111	5.515789
-840.677023	-15.029720	5.525786
-839.231930	-8.068820	5.535782
-837.569374	-8.054856	5.545779
-835.553452	-9.537279	5.555776
-833.586247	-12.903368	5.565773
-831.460718	-21.538098	5.575770
-829.961465	-8.513619	5.585766
-828.189700	-8.845504	5.595763
-826.011246	-15.674601	5.605760
-823.832521	-11.860754	5.615757
-822.031646	-23.179720	5.625754
-820.570994	-11.367933	5.635750
-818.704348	-2.530838	5.645747
-816.489108	-19.639345	5.655744
-814.887341	-11.378823	5.665741
-812.785244	-12.139259	5.675738
-810.827896	-4.922340	5.685734
-809.240397	-15.256735	5.695731
-807.707205	-3.153388	5.705728
-805.200510	-11.885338	5.715725
-803.608125	-8.743496	5.725722
-801.687099	1.175907	5.735718
-799.778780	-0.156666	5.745715
-797.673309	-10.537531	5.755712
-795.976713	-6.280307	5.765709
-794.188069	-3.359286	5.775706
-792.215843	-4.804691	5.785702
-790.194713	-11.862810	5.795699
-788.701556	-7.189407	5.805696
-786.481925	-13.049327	5.815693
-784.620120	-13.225054	5.825690
-782.899363	-6.199231	5.835686
-781.039340	-12.150085	5.845683
-779.251323	-12.849244	5.855680
-777.099828	-15.447424	5.865677
-775.578387	-10.614334	5.875674
-773.448076	-4.244443	5.885670
-771.403913	-10.302083	5.895667
-769.680117	-16.164845	5.905664
-768.003231	-19.367649	5.915661
-765.976235	-18.838756	5.925658
-764.059289	-11.650076	5.935654
-762.142135	-4.731406	5.945651
-760.424397	-6.115591	5.955648
-758.379309	-20.591766	5.965645
-756.785809	-9.690049	5.975642
-754.952287	-6.692490	5.985638
-752.790720	0.521846	5.995635
-750.894070	-8.911460	6.005632
-748.910518	-2.049174	6.015629
-747.047514	-14.208502	6.025626
-745.391956	-11.539316	6.035622
-743.605721	-9.999360	6.045619
-741.472181	-15.041850	6.055616
-739.438897	-9.951077	6.065613
-737.771342	-10.637270	6.075610
-736.172845	-4.468130	6.085606
-734.110052	-7.277874	6.095603
-732.320316	-4.690115	6.105600
-730.421589	-18.031377	6.115597
-728.587776	-5.117116	6.125594
-726.559451	-8.093439	6.135590
-724.673244	-10.895482	6.145587
-722.735206	-9.038737	6.155584
-720.766319	-9.858327	6.165581
-719.140777	-11.325638	6.175578
-717.401395	-6.715214	6.185574
-715.384112	-6.143676	6.195571
-713.296468	-13.079739	6.205568
-711.367401	-9.596919	6.215565
-709.905541	-9.902879	6.225562
-707.768388	-9.781513	6.235558
-705.988876	-15.597876	6.245555
-704.108451	-7.954913	6.255552
-702.201955	-11.642755	6.265549
-700.275846	-9.537785	6.275546
-698.455212	-12.681412	6.285542
-696.253124	-6.698682	6.295539
-694.758263	-7.823012	6.305536
-692.692451	-4.406232	6.315533
-691.108309	-6.203204	6.325530
-689.247542	-1.463739	6.335526
-687.204770	-5.811200	6.345523
-685.116273	-8.448179	6.355520
-683.193510	-10.665542	6.365517
-681.734230	-10.243224	6.375514
-679.466296	-15.518700	6.385510
-677.745467	-7.660752	6.395507
-676.375389	-7.765722	6.405504
-673.868724	-14.978689	6.415501
-671.978222	-12.097530	6.425498
-670.226438	-4.503451	6.435494
-668.420114	-11.006136	6.445491
-666.400115	-6.033164	6.455488
-664.746735	-21.714504	6.465485
-662.819058	-16.232603	6.475482
-660.948340	-12.487804	6.485478
-658.924321	-7.308639	6.495475
-656.965299	-8.813399	6.505472
-655.253266	-11.636505	6.515469
-653.534113	-8.083785	6.525466
-651.675794	-6.143196	6.535462
-649.877619	-7.241751	6.545459
-647.671144	-11.525337	6.555456
-645.997174	-12.768245	6.565453
-644.000809	-17.941885	6.575450
-642.130711	-15.284796	6.585446
-640.387472	-8.803995	6.595443
-638.379325	-9.670840	6.605440
-636.467966	-13.121003	6.615437
-634.510051	-12.426234	6.625434
-632.784987	-3.945279	6.635430
-630.925476	-10.694842	6.645427
-628.971235	-14.093432	6.655424
-626.990976	-17.710899	6.665421
-625.415335	-10.286003	6.675418
-623.493441	-13.496275	6.685414
-621.372928	-16.559865	6.695411
-619.523852	-15.812962	6.705408
-617.930709	-12.739001	6.715405
-615.994941	-17.219297	6.725402
-613.997545	-8.557639	6.735398
-611.910961	-10.152210	6.745395
-610.305049	-14.043001	6.755392
-608.272242	-11.168733	6.765389
-606.288290	-16.223526	6.775386
-604.799245	-15.505935	6.785382
-602.826456	-12.134211	6.795379
-600.784465	-10.754994	6.805376
-598.962922	-16.799036	6.815373
-597.127909	-6.494682	6.825370
-595.442144	-7.469456	6.835366
-593.519777	-14.385337	6.845363
-591.145335	-14.644381	6.855360
-589.512693	-18.245762	6.865357
-587.644355	-16.608283	6.875354
-585.880691	-20.360056	6.885350
-584.091271	-12.910861	6.895347
-581.942533	-11.232909	6.905344
-580.487008	-15.608048	6.915341
-578.234772	-12.737227	6.925338
-576.386663	-18.150800	6.935334
-574.486841	-13.733252	6.945331
-572.892672	-17.483204	6.955328
-570.971875	-17.835545	6.965325
-569.023683	-15.579267	6.975322
-566.961102	-11.524004	6.985318
-565.266406	-13.186983	6.995315
-563.506194	-7.567725	7.005312
-561.290079	-14.404194	7.015309
-559.541164	-14.849064	7.025306
-557.766793	-13.423906	7.035302
-556.008898	-10.259381	7.045299
-553.905866	-13.302755	7.055296
-551.859812	-13.223536	7.065293
-550.273361	-17.096970	7.075290
-548.231624	-4.267855	7.085286
-546.452878	-11.681784	7.095283
-544.912459	-15.503655	7.105280
-542.653307	-13.592266	7.115277
-540.849479	-12.361262	7.125274
-538.875681	-11.470015	7.135270
-537.142489	-10.894000	7.145267
-535.141598	-13.005312	7.155264
-533.277747	-14.387410	7.165261
-531.411595	-9.419744	7.175258
-529.499315	-10.620112	7.185254
-527.829600	-4.297991	7.195251
-525.699933	-12.707368	7.205248
-523.935051	-7.215131	7.215245
-522.071497	-12.800071	7.225242
-520.255236	-9.147502	7.235238
-518.297644	-10.165637	7.245235
-516.560584	-6.456208	7.255232
-514.392024	-12.273000	7.265229
-512.606596	-16.853937	7.275226
-510.797338	-14.635417	7.285222
-509.100249	-11.450094	7.295219
-507.003487	-12.403608	7.305216
-505.032762	-21.989084	7.315213
-503.335071	-18.375986	7.325210
-501.447389	-13.520675	7.335206
-499.573943	-13.999599	7.345203
-497.459765	-11.706615	7.355200
-495.704334	-15.804358	7.365197
-493.958108	-13.269462	7.375194
-492.181040	-10.878429	7.385190
-490.330386	-7.245538	7.395187
-488.310151	-13.059146	7.405184
-486.391193	-13.605324	7.415181
-484.520592	-10.667151	7.425178
-482.590362	-17.180020	7.435174
-480.712501	-15.356093	7.445171
-478.797558	-9.646221	7.455168
-477.161101	-11.962956	7.465165
-475.045357	-12.707909	7.475162
-473.184697	-4.257950	7.485158
-471.727367	-19.301606	7.495155
-469.329010	-10.718053	7.505152
-467.618143	-9.199006	7.515149
-465.537340	-14.351257	7.525146
-464.035430	-4.915639	7.535142
-462.280995	-3.138298	7.545139
-460.122740	-9.108128	7.555136
-458.228592	-11.860712	7.565133
-456.089561	-2.080010	7.575130
-454.412551	-10.262323	7.585126
-452.743103	-14.305257	7.595123
-450.724176	-9.892412	7.605120
-448.960368	-12.237358	7.615117
-447.037692	-12.624635	7.625114
-445.049005	-11.274663	7.635110
-443.285735	-7.785666	7.645107
-441.113797	-13.173488	7.655104
-439.510173	-11.583616	7.665101
-437.805162	-10.395171	7.675098
-436.001766	-13.629007	7.685094
-433.883816	-11.788118	7.695091
-431.985035	-7.495010	7.705088
-430.037485	-12.095462	7.715085
-428.071399	-12.870158	7.725082
-426.500374	-11.892402	7.735078
-424.436304	-9.070329	7.745075
-422.712337	-6.883908	7.755072
-420.692577	-7.921363	7.765069
-418.477832	-13.855968	7.775066
-416.916304	-10.568410	7.785062
-415.196729	-7.703955	7.795059
-413.182465	-16.169020	7.805056
-411.322051	-10.890883	7.815053
-410.034181	-8.371155	7.825050
-407.623223	-4.875022	7.835046
-405.389983	-11.526211	7.845043
-404.057427	-10.428266	7.855040
-401.917397	-11.825940	7.865037
-400.003068	-10.760882	7.875034
-398.201091	-8.591634	7.885030
-396.371780	-11.024365	7.895027
-394.616179	-18.196089	7.905024
-392.220859	-13.862233	7.915021
-390.480154	-16.768678	7.925018
-388.903115	-14.400889	7.935014
-387.098954	-10.402093	7.945011
-385.056186	-12.352611	7.955008
-383.276457	-9.260908	7.965005
-381.455364	-0.147748	7.975002
-379.321331	-4.151131	7.984998
-377.521980	-7.373228	7.994995
-376.094037	-14.271592	8.004992
-373.872732	-11.820345	8.014989
-371.635742	-12.234059	8.024986
-370.036159	-11.794477	8.034982
-368.288579	-12.403196	8.044979
-366.179613	-9.976636	8.054976
-364.505267	-16.034909	8.064973
-362.597766	-12.365204	8.074970
-360.647535	-10.859031	8.084966
-358.945336	-3.828325	8.094963
-357.142327	-9.711358	8.104960
-355.108260	1.012990	8.114957
-352.920658	-7.465498	8.124954
-351.479918	-11.266605	8.134950
-349.525722	-11.834088	8.144947
-347.504365	-4.969580	8.154944
-345.432339	-12.284940	8.164941
-343.728095	-4.368813	8.174938
-342.075900	-8.309455	8.184934
-339.866303	-0.723453	8.194931
-338.205826	-1.195095	8.204928
-336.376949	-5.361295	8.214925
-334.284318	-9.283824	8.224922
-332.595291	-7.524364	8.234918
-330.720186	-12.929442	8.244915
-329.005130	-11.287812	8.254912
-326.845595	-15.822556	8.264909
-325.169167	-13.224289	8.274906
-323.046790	-14.105948	8.284902
-321.165359	-8.033769	8.294899
-319.199201	-7.630564	8.304896
-317.626231	-10.044423	8.314893
-315.902746	-9.870883	8.324890
-313.742507	-13.914705	8.334886
-311.797552	-4.524435	8.344883
-309.854426	-8.263615	8.354880
-308.201566	-13.784772	8.364877
-306.226502	-14.311343	8.374874
-304.251786	-8.130890	8.384870
-302.926611	-5.309179	8.394867
-300.952106	-13.453625	8.404864
-298.655642	-5.147283	8.414861
-296.862626	-9.340886	8.424858
-294.982157	-11.047541	8.434854
-293.281141	-8.273185	8.444851
-291.372622	-4.553058	8.454848
-289.275905	-2.522343	8.464845
-287.442645	-9.829548	8.474842
-285.490160	-1.430394	8.484838
-283.596481	-2.045004	8.494835
-282.144278	-9.777671	8.504832
-280.056834	-6.967094	8.514829
-277.886652	-4.311817	8.524826
-276.329070	-3.510226	8.534822
-274.734761	-12.926523	8.544819
-272.516639	-3.013007	8.554816
-270.379000	-4.850685	8.564813
-268.641667	-14.889770	8.574810
-267.232531	-4.975018	8.584807
-265.030184	-5.324687	8.594803
-263.012914	-7.443129	8.604800
-261.041030	-8.243877	8.614797
-259.314211	-8.299763	8.624794
-257.550898	-8.389891	8.634791
-255.673983	-8.757081	8.644787
-253.840487	-12.022432	8.654784
-251.711532	-16.190674	8.664781
-249.538251	-21.193306	8.674778
-247.833417	-20.843067	8.684775
-246.375107	-18.814634	8.694771
-244.321536	-16.584375	8.704768
-242.633615	-19.962265	8.714765
-240.881393	-17.633386	8.724762
-238.476002	-14.418806	8.734759
-236.678305	-17.081623	8.744755
-235.149374	-16.307011	8.754752
-233.159856	-14.952257	8.764749
-231.196276	-13.530207	8.774746
-229.417109	-6.377482	8.784743
-227.307649	-13.543996	8.794739
-225.544722	-7.479664	8.804736
-223.697463	-12.542347	8.814733
-221.885188	-12.431855	8.824730
-220.105819	-13.983379	8.834727
-218.333101	-11.558286	8.844723
-216.207919	-10.356212	8.854720
-214.336988	-17.937780	8.864717
-212.352784	-19.097275	8.874714
-210.627484	-15.870446	8.884711
-208.642299	-19.658887	8.894707
-206.916461	-19.627742	8.904704
-205.180508	-14.016960	8.914701
-203.045331	-20.267084	8.924698
-201.026511	-18.365959	8.934695
-199.430079	-14.870677	8.944691
-197.570457	-14.774037	8.954688
-195.581890	-14.789546	8.964685
-193.674951	-13.862082	8.974682
-191.990735	-10.630260	8.984679
-189.937800	-17.184601	8.994675
-187.992215	-18.203711	9.004672
-186.212866	-17.794271	9.014669
-184.420463	-13.798176	9.024666
-182.367498	-9.164747	9.034663
-180.605353	-12.042892	9.044659
-178.771954	-12.330452	9.054656
-176.640758	-14.347009	9.064653
-174.715913	-11.886161	9.074650
-173.200037	-19.698396	9.084647
-171.290057	-9.372475	9.094643
-169.509352	-19.268426	9.104640
-167.470456	-15.066926	9.114637
-165.845105	-11.781486	9.124634
-163.753884	-16.770953	9.134631
-161.825230	-14.879091	9.144627
-159.836630	-11.661079	9.154624
-157.804357	-14.389689	9.164621
-155.959090	-14.977528	9.174618
-154.716897	-8.176407	9.184615
-152.409525	-17.381164	9.194611
-150.431473	-12.702600	9.204608
-148.761389	-13.001971	9.214605
-146.677461	-16.354567	9.224602
-144.867191	-10.352986	9.234599
-143.120643	-14.624324	9.244595
-141.104843	-14.108901	9.254592
-139.278882	-15.795689	9.264589
-137.537016	-7.946978	9.274586
-135.678200	-10.204236	9.284583
-133.719401	-10.363357	9.294579
-131.712965	-13.864621	9.304576
-129.960115	-11.450500	9.314573
-127.917746	-15.257476	9.324570
-126.020189	-8.439327	9.334567
-124.295399	-12.531929	9.344563
-122.517309	-13.811616	9.354560
-120.331684	-8.452499	9.364557
-118.694281	-10.249707	9.374554
-116.924115	-15.377378	9.384551
-114.927706	-18.038655	9.394547
-113.199028	-8.143202	9.404544
-111.199823	-13.725808	9.414541
-109.466978	-7.612377	9.424538
-107.383417	-14.372055	9.434535
-105.623867	-4.412049	9.444531
-103.716279	-1.242638	9.454528
-101.569998	-7.057112	9.464525
-99.750941	-7.274433	9.474522
-97.964856	-5.416611	9.484519
-96.348197	0.066460	9.494515
-94.390567	-4.799018	9.504512
-92.159384	-12.456923	9.514509
-90.594461	-5.890396	9.524506
-88.743954	-9.290965	9.534503
-86.732617	-16.714856	9.544499
-84.933401	-4.989683	9.554496
-82.798153	-4.681151	9.564493
-81.110624	-6.753158	9.574490
-79.291831	-11.054926	9.584487
-77.523636	-11.159912	9.594483
-75.472682	-9.527474	9.604480
-73.583595	0.219277	9.614477
-71.858716	-4.189078	9.624474
-70.012321	-14.477533	9.634471
-67.918789	-4.668663	9.644467
-66.205667	-9.585108	9.654464
-64.192552	-13.033703	9.664461
-62.241502	-7.201344	9.674458
-60.408872	-17.321815	9.684455
-58.768178	-2.074162	9.694451
-56.674890	-6.370758	9.704448
-55.000761	-8.525869	9.714445
-52.879620	-6.996181	9.724442
-51.290619	-9.156656	9.734439
-49.427986	-3.046512	9.744435
-47.163093	-6.535257	9.754432
-45.532630	-14.867781	9.764429
-43.496413	-6.126526	9.774426
-41.600481	-10.966332	9.784423
-39.771493	-10.215774	9.794419
-37.926018	-11.049859	9.804416
-36.104144	-12.964854	9.814413
-34.102112	-13.672339	9.824410
-32.542044	-19.593761	9.834407
-30.437643	-13.046933	9.844403
-28.731370	-14.221946	9.854400
-26.646697	-15.803083	9.864397
-24.979333	-10.814342	9.874394
-23.004878	-13.738872	9.884391
-21.017027	-12.326836	9.894387
-19.075401	-14.598795	9.904384
-17.472235	-13.010141	9.914381
-15.205715	-14.440284	9.924378
-13.511822	-13.770784	9.934375
-12.023617	-11.259104	9.944371
-9.804525	-11.998033	9.954368
-7.927020	-17.690614	9.964365
-6.061343	-15.256505	9.974362
-4.226025	-9.819299	9.984359
-3.378598	7.094321	9.994355
-2.415021	58.294998	10.004352
-0.887080	126.214520	10.014349
0.000000	194.872790	10.019354
0.622877	245.846644	10.024359
1.232389	288.828066	10.029363
1.687091	324.443487	10.034368
1.797511	357.310215	10.039373
2.189591	389.564416	10.044378
2.630688	410.184490	10.049383
2.947396	442.430331	10.054387
3.122374	458.537288	10.059392
3.332499	482.795924	10.064397
3.210634	493.043222	10.069402
3.406579	505.628836	10.074407
3.595093	529.474697	10.079411
3.989035	529.441955	10.084416
3.922283	549.517199	10.089421
3.990892	547.489529	10.094426
4.000262	557.845248	10.099431
4.274329	582.246811	10.104435
4.624394	589.747633	10.109440
4.361354	590.377900	10.114445
4.743044	590.490611	10.119450
4.653496	598.438433	10.124455
4.579071	601.892818	10.129459
4.903269	599.464841	10.134464
4.684168	609.661500	10.139469
4.681950	601.961947	10.144474
4.869952	605.707205	10.149479
4.828743	614.099898	10.154483
5.032158	610.459619	10.159488
4.723350	619.029032	10.164493
4.712625	615.620019	10.169498
4.930666	627.889988	10.174503
4.955124	637.492749	10.179507
5.042459	651.303725	10.184512
5.328801	657.110105	10.189517
5.323152	671.801656	10.194522
5.524604	663.766819	10.199527
5.080806	668.084357	10.204531
5.279289	669.461012	10.209536
5.386714	674.939552	10.214541
5.457772	675.343076	10.219546
5.723910	674.917567	10.224551
5.284652	679.724805	10.229555
5.527953	674.600579	10.234560
5.577826	683.767243	10.239565
5.444676	684.091376	10.244570
5.399728	679.725888	10.249575
5.542721	691.492229	10.254579
6.055722	712.489189	10.259584
5.950161	715.221607	10.264589
5.942826	726.327570	10.269594
6.127086	727.149847	10.274599
5.884935	724.370641	10.279603
6.213019	716.058540	10.284608
6.038384	735.025327	10.289613
5.826362	725.897365	10.294618
5.997892	721.443723	10.299623
6.435088	729.574104	10.304627
6.254036	748.436278	10.309632
6.017600	736.998858	10.314637
6.090303	733.682165	10.319642
6.067882	741.854320	10.324647
5.860020	744.845906	10.329651
6.232603	759.991298	10.334656
5.941859	775.573656	10.339661
6.036107	781.368146	10.344666
6.161276	772.244721	10.349671
6.426100	804.516990	10.354675
6.690063	801.250201	10.359680
6.766732	818.942282	10.364685
6.716804	815.982591	10.369690
6.845874	825.512023	10.374695
6.963117	827.169729	10.379699
6.959258	815.814999	10.384704
6.916455	822.937062	10.389709
7.060079	823.925096	10.394714
7.402255	815.143920	10.399719
7.198910	829.709469	10.404723
6.998083	829.407318	10.409728
7.071443	830.007596	10.414733
7.178825	829.413441	10.419738
7.333970	828.911015	10.424743
7.089125	831.440168	10.429747
7.426148	829.238764	10.434752
7.378497	833.881093	10.439757
7.003376	832.383042	10.444762
7.566939	828.361998	10.449767
7.472826	844.450801	10.454771
7.631955	861.246700	10.459776
7.820747	872.400341	10.464781
7.910705	868.730786	10.469786
7.690267	858.840845	10.474791
7.366379	864.457632	10.479795
7.626517	869.445117	10.484800
7.776691	885.072385	10.489805
7.619795	895.579441	10.494810
7.808809	881.833222	10.499815
7.787756	897.757470	10.504819
7.930483	886.596923	10.509824
7.790024	901.674480	10.514829
8.161323	890.527937	10.519834
7.850897	888.026091	10.524839
7.952008	911.672057	10.529843
8.261081	912.523324	10.534848
8.375823	919.200841	10.539853
8.317799	933.418466	10.544858
8.362381	930.953031	10.549863
8.166699	928.994269	10.554867
8.438555	926.055774	10.559872
8.176405	933.920921	10.564877
7.983507	935.112445	10.569882
8.247629	926.698463	10.574887
8.250425	955.612974	10.579891
8.717349	954.329116	10.584896
8.716168	967.164190	10.589901
8.770427	969.686663	10.594906
8.945328	967.501634	10.599911
8.890437	967.147820	10.604915
8.688259	965.204281	10.609920
8.420224	975.845814	10.614925
8.608434	982.968958	10.619930
8.821780	981.484267	10.624935
8.579465	987.545407	10.629939
9.136771	1000.382900	10.634944
9.071679	1010.572622	10.639949
8.892648	1014.084789	10.644954
8.893412	1015.376319	10.649959
8.901520	1012.908802	10.654963
9.437148	1011.924641	10.659968
9.180723	1020.938520	10.664973
8.992416	1016.400253	10.669978
9.599088	1029.360785	10.674983
9.161534	1051.216317	10.679987
9.354337	1052.611263	10.684992
9.459904	1051.085408	10.689997
9.450421	1053.163899	10.695002
9.685082	1055.001601	10.700007
9.643219	1058.242742	10.705011
9.786929	1051.735509	10.710016
9.426319	1065.085312	10.715021
9.299692	1056.746192	10.720026
9.791856	1067.580362	10.725031
9.913674	1088.102516	10.730035
10.144361	1087.367259	10.735040
10.179800	1093.843038	10.740045
10.081510	1096.607484	10.745050
10.452259	1094.902136	10.750055
10.196432	1106.691421	10.755059
10.412138	1095.493843	10.760064
10.024898	1100.064262	10.765069
10.014514	1102.278522	10.770074
10.248149	1101.989074	10.775079
9.979004	1110.623412	10.780083
10.189788	1108.110939	10.785088
9.994183	1103.573809	10.790093
10.345518	1115.316728	10.795098
10.367535	1132.305121	10.800103
10.025733	1146.631293	10.805107
10.294556	1133.554933	10.810112
10.659438	1148.109022	10.815117
10.341298	1145.004383	10.820122
10.715348	1150.580929	10.825127
11.024490	1148.879092	10.830131
10.698106	1153.353088	10.835136
10.930146	1160.393634	10.840141
11.213551	1173.126731	10.845146
11.085074	1183.555345	10.850151
11.342074	1177.342227	10.855155
10.810054	1169.146547	10.860160
11.075236	1168.959300	10.865165
11.042564	1186.522610	10.870170
11.375629	1180.508674	10.875175
11.413747	1180.469606	10.880179
11.498579	1188.255896	10.885184
11.448789	1187.540136	10.890189
11.431740	1185.116028	10.895194
11.638803	1196.842599	10.900199
11.355872	1189.513938	10.905203
11.696804	1193.689125	10.910208
11.460936	1198.569749	10.915213
11.524551	1189.375455	10.920218
11.892054	1190.138572	10.925223
11.411719	1185.916489	10.930227
11.650204	1188.106840	10.935232
11.554246	1191.020744	10.940237
11.646469	1186.380911	10.945242
11.496581	1194.860659	10.950247
11.317715	1201.802755	10.955251
11.713714	1218.340513	10.960256
11.513936	1232.404419	10.965261
11.753290	1238.193296	10.970266
12.132264	1227.717063	10.975271
11.690760	1250.630096	10.980275
12.077297	1233.608202	10.985280
12.121817	1245.977334	10.990285
12.164310	1252.819494	10.995290
12.473673	1253.246529	11.000295
12.227212	1265.576929	11.005299
12.665374	1262.450992	11.010304
12.625836	1257.254977	11.015309
12.420904	1258.246592	11.020314
12.527781	1262.109040	11.025319
12.327776	1272.829828	11.030323
12.480992	1265.434721	11.035328
12.247157	1269.688984	11.040333
12.624859	1270.967728	11.045338
13.285289	1265.142824	11.050343
12.637940	1275.695259	11.055347
12.569788	1270.866508	11.060352
13.012019	1267.717843	11.065357
12.626310	1276.096475	11.070362
12.997348	1264.139122	11.075367
13.101067	1283.839680	11.080371
13.041415	1287.011168	11.085376
12.824166	1293.153593	11.090381
13.170485	1301.454913	11.095386
13.723465	1293.858837	11.100391
13.249993	1314.845268	11.105395
13.475832	1303.040353	11.110400
13.188796	1305.611009	11.115405
12.862786	1299.683216	11.120410
13.220038	1307.386697	11.125415
13.071483	1300.333021	11.130419
13.381260	1313.645519	11.135424
12.989701	1306.321507	11.140429
13.323407	1315.310835	11.145434
14.083988	1321.098619	11.150439
13.542577	1338.167651	11.155443
13.772737	1330.870628	11.160448
14.044862	1333.683277	11.165453
13.786686	1341.652091	11.170458
14.101452	1331.441497	11.175463
13.801998	1340.542861	11.180467
13.859635	1334.266854	11.185472
14.086001	1337.632438	11.190477
13.922990	1343.882931	11.195482
14.161194	1331.768508	11.200487
13.918475	1348.250585	11.205491
14.002097	1345.591192	11.210496
14.359549	1332.115735	11.215501
14.326238	1343.276776	11.220506
14.576387	1338.857717	11.225511
14.142354	1338.157499	11.230515
14.240201	1340.964828	11.235520
14.406344	1343.463214	11.240525
14.062146	1340.523540	11.245530
14.384505	1331.092344	11.250535
14.606792	1343.095732	11.255539
14.230809	1350.241229	11.260544
14.935987	1357.688969	11.265549
14.661780	1366.609701	11.270554
14.735097	1368.509447	11.275559
14.475054	1376.849171	11.280563
14.874647	1373.218417	11.285568
15.078543	1370.101434	11.290573
15.031947	1381.739297	11.295578
15.191390	1368.596592	11.300583
15.063523	1380.551775	11.305587
14.899903	1377.897115	11.310592
15.119005	1373.848859	11.315597
14.981613	1376.898721	11.320602
15.447093	1374.154766	11.325607
15.469389	1377.210700	11.330611
15.282651	1366.595929	11.335616
14.926449	1384.297811	11.340621
14.973090	1370.119665	11.345626
15.456391	1366.166472	11.350631
15.184054	1379.620758	11.355635
15.582309	1375.564430	11.360640
15.675071	1366.426878	11.365645
15.528416	1384.738752	11.370650
15.708691	1376.881946	11.375655
15.681212	1376.749259	11.380659
15.895377	1369.128332	11.385664
16.068023	1372.830506	11.390669
15.688174	1376.001041	11.395674
16.076414	1366.240762	11.400679
15.823766	1381.795614	11.405683
15.632910	1365.136895	11.410688
16.005433	1374.277769	11.415693
15.929191	1379.246537	11.420698
16.073318	1368.433913	11.425703
15.514520	1373.760346	11.430707
15.820006	1389.897989	11.435712
16.147810	1400.471611	11.440717
15.965160	1414.367376	11.445722
16.120156	1405.508464	11.450727
16.007670	1417.492764	11.455731
15.887515	1405.479591	11.460736
16.362376	1413.091830	11.465741
16.044343	1431.912080	11.470746
16.527848	1430.113015	11.475751
16.666000	1432.037123	11.480755
16.796422	1427.252346	11.485760
17.045370	1444.310570	11.490765
16.969548	1436.362108	11.495770
17.378758	1418.170982	11.500775
16.968246	1401.469981	11.505779
17.061629	1398.763289	11.510784
17.329579	1395.629777	11.515789
16.844055	1394.325895	11.520794
17.048355	1397.969410	11.525799
16.834180	1396.988113	11.530803
17.119566	1394.457386	11.535808
17.165071	1396.740050	11.540813
16.979188	1395.878824	11.545818
16.835353	1403.775818	11.550823
17.120953	1403.377150	11.555827
16.853084	1410.055990	11.560832
17.344607	1421.906114	11.565837
17.514300	1432.541248	11.570842
17.470953	1428.200511	11.575847
17.329509	1441.070990	11.580851
17.689906	1440.343416	11.585856
17.962750	1434.709575	11.590861
17.404817	1419.060267	11.595866
17.532668	1434.138163	11.600871
17.683072	1443.294005	11.605875
17.835573	1440.675650	11.610880
17.878711	1439.175482	11.615885
17.645131	1440.572236	11.620890
17.821233	1442.726842	11.625895
17.767713	1451.342762	11.630899
18.172934	1434.287691	11.635904
18.285622	1437.948980	11.640909
17.927364	1437.875356	11.645914
18.142912	1431.848519	11.650919
18.230985	1442.100852	11.655923
18.213542	1434.130465	11.660928
17.989331	1437.298267	11.665933
17.889528	1443.574993	11.670938
18.306432	1435.838115	11.675943
18.243693	1441.227387	11.680947
18.045064	1440.025983	11.685952
18.122865	1435.134474	11.690957
17.721714	1436.182627	11.695962
18.294794	1432.550999	11.700967
18.466608	1458.397530	11.705971
18.457007	1464.338958	11.710976
18.503605	1462.509432	11.715981
18.563116	1474.276319	11.720986
18.515934	1468.376528	11.725991
18.355956	1474.937262	11.730995
19.074044	1462.858951	11.736000
19.123045	1457.388538	11.741005
18.852895	1472.431387	11.746010
18.939240	1463.193870	11.751015
19.037120	1472.097901	11.756019
19.103423	1473.574567	11.761024
19.136328	1465.471550	11.766029
19.146674	1471.894728	11.771034
19.283200	1472.603234	11.776039
19.531432	1473.558860	11.781043
19.175139	1474.186687	11.786048
19.514892	1465.440202	11.791053
19.432132	1475.369710	11.796058
19.686278	1474.734776	11.801063
19.445626	1461.049439	11.806067
19.421183	1468.598623	11.811072
18.965963	1470.497519	11.816077
18.947555	1472.586955	11.821082
19.431363	1461.746108	11.826087
19.168723	1476.462901	11.831091
19.213005	1469.545550	11.836096
19.652684	1487.492797	11.841101
19.638950	1497.239418	11.846106
19.740861	1500.036667	11.851111
20.275619	1501.667289	11.856115
20.192953	1496.714617	11.861120
19.977937	1499.456753	11.866125
19.789282	1497.876848	11.871130
20.292736	1496.579236	11.876135
19.988278	1500.958373	11.881139
19.868333	1509.501340	11.886144
20.124648	1499.440304	11.891149
19.955347	1505.382776	11.896154
20.298400	1495.325257	11.901159
20.390059	1498.917374	11.906163
20.495431	1492.786655	11.911168
20.379269	1495.596605	11.916173
20.386745	1500.228778	11.921178
20.526363	1490.112241	11.926183
20.488833	1497.837786	11.931187
20.482347	1503.971917	11.936192
20.654158	1491.752829	11.941197
20.149735	1500.640970	11.946202
20.451786	1502.349708	11.951207
20.426731	1499.770700	11.956211
20.749631	1504.281603	11.961216
20.779836	1518.692317	11.966221
20.434876	1526.708190	11.971226
21.193002	1505.570654	11.976231
21.301956	1513.667096	11.981235
21.621658	1515.656882	11.986240
21.355573	1498.738762	11.991245
21.135648	1495.403909	11.996250
21.155338	1474.160254	12.001255
21.428236	1490.564990	12.006259
21.379602	1483.178310	12.011264
21.284074	1481.745986	12.016269
21.500098	1490.973397	12.021274
21.316578	1484.067137	12.026279
21.426227	1477.599840	12.031283
21.194184	1490.169412	12.036288
21.319629	1481.876580	12.041293
21.263845	1491.464317	12.046298
21.206485	1482.560376	12.051303
20.889070	1491.830284	12.056307
21.366071	1491.312777	12.061312
21.392210	1484.863527	12.066317
21.205030	1495.785866	12.071322
21.442456	1482.412994	12.076327
21.471966	1489.279415	12.081331
21.324618	1495.122185	12.086336
21.546905	1485.035046	12.091341
21.452392	1491.889708	12.096346
21.591797	1480.871166	12.101351
21.567469	1494.385354	12.106355
21.361084	1497.558212	12.111360
21.370047	1488.881817	12.116365
21.135326	1496.911632	12.121370
21.304121	1489.263184	12.126375
21.350055	1498.266982	12.131379
21.316267	1490.496296	12.136384
21.531727	1495.666172	12.141389
21.420256	1488.910851	12.146394
21.552862	1494.333645	12.151399
21.427899	1488.367400	12.156403
21.526804	1473.613095	12.161408
21.117072	1467.993483	12.166413
20.880200	1464.544641	12.171418
20.896043	1477.379029	12.176423
21.285382	1481.943986	12.181427
21.099603	1488.286483	12.186432
21.014290	1495.942375	12.191437
21.147769	1500.041926	12.196442
21.328409	1490.414025	12.201447
21.343953	1504.931147	12.206451
21.567194	1503.224047	12.211456
21.832010	1497.482649	12.216461
21.502594	1501.596099	12.221466
21.433379	1497.142769	12.226471
21.532680	1497.756284	12.231475
21.485763	1485.311880	12.236480
21.220015	1472.796728	12.241485
21.395761	1469.356198	12.246490
21.448474	1464.404023	12.251495
21.381867	1464.597707	12.256499
21.308296	1472.885667	12.261504
21.489423	1453.922659	12.266509
21.196558	1473.895678	12.271514
21.268239	1461.084651	12.276519
21.218954	1460.826127	12.281523
21.003849	1473.526239	12.286528
21.384372	1464.427890	12.291533
21.298781	1468.819421	12.296538
21.463972	1464.175748	12.301543
21.577364	1464.318646	12.306547
21.283432	1463.801086	12.311552
21.331447	1470.879019	12.316557
21.114050	1467.400262	12.321562
21.405616	1461.660131	12.326567
21.399985	1476.324897	12.331571
21.596354	1466.202479	12.336576
21.629234	1469.192088	12.341581
21.573296	1471.643911	12.346586
21.614081	1461.427247	12.351591
21.381082	1476.673917	12.356595
21.342329	1471.512394	12.361600
21.789858	1464.065517	12.366605
21.082564	1465.891070	12.371610
21.135487	1465.534241	12.376615
21.285807	1463.769388	12.381619
21.431957	1465.867273	12.386624
21.603210	1466.776827	12.391629
21.371847	1466.033239	12.396634
21.363496	1440.601651	12.401639
21.197550	1446.373248	12.406643
21.100698	1440.806251	12.411648
21.568712	1452.679076	12.416653
21.418155	1458.470301	12.421658
21.402919	1445.926258	12.426663
21.582086	1447.129447	12.431667
21.223250	1446.688474	12.436672
21.405042	1445.140960	12.441677
21.020730	1448.909903	12.446682
21.380039	1438.789904	12.451687
21.353763	1450.344155	12.456691
21.249534	1449.812111	12.461696
21.581629	1442.850447	12.466701
21.469232	1449.780483	12.471706
21.170958	1438.645691	12.476711
21.421590	1449.480824	12.481715
21.428518	1442.659331	12.486720
21.682383	1443.685022	12.491725
21.055206	1451.862561	12.496730
21.409307	1445.949243	12.501735
21.260252	1448.236136	12.506739
21.114285	1448.302123	12.511744
21.491846	1455.974061	12.516749
21.344763	1450.361453	12.521754
21.369304	1452.474000	12.526759
21.187098	1459.544488	12.531763
21.172539	1452.116119	12.536768
21.450093	1459.009200	12.541773
21.291452	1465.994718	12.546778
21.415808	1451.983086	12.551783
21.384006	1454.713341	12.556787
20.964670	1462.417755	12.561792
21.453223	1449.312377	12.566797
21.224749	1457.702306	12.571802
21.212860	1463.424897	12.576807
21.291107	1456.632236	12.581811
21.526081	1464.171584	12.586816
21.569801	1461.790567	12.591821
20.891263	1466.723744	12.596826
21.254109	1462.298502	12.601831
21.081718	1458.183346	12.606835
21.228074	1462.424340	12.611840
21.446391	1466.949545	12.616845
21.464073	1462.259221	12.621850
21.591356	1465.920556	12.626855
21.369859	1468.652681	12.631859
21.569210	1463.837974	12.636864
21.355711	1451.996559	12.641869
20.996953	1458.808191	12.646874
21.311064	1455.755617	12.651879
21.328390	1467.573383	12.656883
21.104395	1466.721385	12.661888
21.389814	1465.381276	12.666893
21.504020	1464.290830	12.671898
21.344559	1468.834496	12.676903
21.147570	1456.542576	12.681907
21.288102	1462.238491	12.686912
21.418595	1456.122705	12.691917
20.928254	1478.063780	12.696922
21.252898	1455.367197	12.701927
21.350580	1460.890168	12.706931
21.450035	1463.724862	12.711936
21.487070	1456.733764	12.716941
21.214109	1468.659331	12.721946
21.447241	1461.793079	12.726951
21.559881	1465.532446	12.731955
21.471063	1458.845279	12.736960
21.494952	1461.945132	12.741965
21.209011	1468.973032	12.746970
21.414270	1465.032618	12.751975
21.515405	1461.637895	12.756979
21.350822	1455.518705	12.761984
21.339972	1444.927865	12.766989
21.091401	1432.181344	12.771994
21.038048	1440.543334	12.776999
21.324879	1460.401015	12.782003
21.188274	1462.249096	12.787008
21.737958	1464.608273	12.792013
21.436724	1457.958138	12.797018
21.145019	1443.010687	12.802023
20.984950	1443.563061	12.807027
21.113062	1454.565976	12.812032
21.439601	1460.935567	12.817037
20.956354	1477.039034	12.822042
21.124979	1468.420769	12.827047
21.328140	1473.800762	12.832051
21.036186	1462.915686	12.837056
21.128227	1469.614425	12.842061
21.145371	1479.250450	12.847066
21.516548	1468.344768	12.852071
21.699068	1474.294197	12.857075
21.358117	1468.862316	12.862080
21.606425	1478.306927	12.867085
21.677892	1471.962421	12.872090
21.382072	1468.161847	12.877095
21.441724	1444.099283	12.882099
21.113808	1448.396988	12.887104
21.327544	1437.754565	12.892109
21.147966	1439.615804	12.897114
21.212551	1443.697941	12.902119
21.395162	1445.821547	12.907123
21.076508	1458.196741	12.912128
21.313464	1465.186978	12.917133
21.433460	1471.291461	12.922138
21.081422	1476.520298	12.927143
21.631606	1469.523839	12.932147
21.417506	1456.135479	12.937152
21.664264	1443.361991	12.942157
21.177141	1457.968696	12.947162
21.042702	1441.796068	12.952167
21.438316	1438.082353	12.957171
21.150141	1449.722529	12.962176
21.333868	1435.416796	12.967181
21.408364	1440.449857	12.972186
21.674176	1433.199139	12.977191
21.537731	1436.032814	12.982195
21.051781	1442.721217	12.987200
21.250846	1438.338661	12.992205
21.212900	1441.781119	12.997210
21.403005	1447.290922	13.002215
21.207693	1454.566931	13.007219
21.466572	1443.079918	13.012224
21.043852	1457.141748	13.017229
21.094760	1447.553491	13.022234
21.099199	1455.559333	13.027239
21.067704	1457.824324	13.032243
21.116717	1462.162846	13.037248
21.822841	1474.373828	13.042253
21.573228	1465.662990	13.047258
21.401495	1458.093311	13.052263
21.676803	1446.280390	13.057267
21.303986	1459.653001	13.062272
21.306232	1456.241722	13.067277
21.493436	1463.690914	13.072282
21.629183	1443.473557	13.077287
21.495131	1456.193057	13.082291
21.240257	1461.594055	13.087296
21.652944	1449.208849	13.092301
21.308661	1440.229265	13.097306
21.364958	1454.411821	13.102311
21.242756	1449.176880	13.107315
21.125700	1457.025476	13.112320
21.615425	1442.142639	13.117325
21.374926	1460.155753	13.122330
21.252489	1454.048767	13.127335
21.357988	1456.323449	13.132339
20.956303	1456.938013	13.137344
21.483053	1453.510894	13.142349
21.179513	1456.497382	13.147354
21.491915	1452.350644	13.152359
21.537489	1454.529224	13.157363
21.210360	1458.864655	13.162368
21.311893	1468.377612	13.167373
21.221339	1461.865768	13.172378
21.482410	1459.340485	13.177383
21.158157	1467.915223	13.182387
21.261417	1461.301503	13.187392
21.484793	1459.389377	13.192397
21.548009	1450.806857	13.197402
21.033626	1446.531776	13.202407
21.257312	1441.694271	13.207411
21.292254	1448.927247	13.212416
21.354076	1451.054349	13.217421
21.581867	1453.508229	13.222426
21.069356	1443.940443	13.227431
21.210955	1429.595701	13.232435
21.295144	1450.647933	13.237440
21.338773	1450.861883	13.242445
21.304954	1460.334131	13.247450
21.417690	1451.644361	13.252455
21.359056	1449.583242	13.257459
21.170483	1431.910072	13.262464
21.543259	1430.863548	13.267469
21.148817	1436.471305	13.272474
21.174593	1428.113972	13.277479
21.521404	1424.647746	13.282483
21.171301	1435.542407	13.287488
21.197125	1423.428663	13.292493
21.100009	1432.999299	13.297498
21.288126	1441.521481	13.302503
21.118284	1459.337239	13.307507
21.202058	1467.507848	13.312512
21.634216	1462.467560	13.317517
21.481549	1466.544139	13.322522
21.226315	1454.065962	13.327527
21.376689	1444.849784	13.332531
20.941827	1452.742756	13.337536
21.091560	1451.867425	13.342541
21.365602	1459.166355	13.347546
21.379732	1469.685185	13.352551
21.330914	1467.490030	13.357555
21.286455	1475.886893	13.362560
21.403261	1469.629777	13.367565
21.346205	1465.177671	13.372570
21.547111	1466.604483	13.377575
22.052650	1444.960888	13.382579
21.642003	1451.780793	13.387584
21.559796	1437.533240	13.392589
21.410245	1439.345535	13.397594
21.406161	1435.698720	13.402599
21.333202	1436.918464	13.407603
21.378809	1440.276631	13.412608
21.591815	1431.968285	13.417613
21.269822	1440.803640	13.422618
21.623453	1439.287069	13.427623
21.598963	1435.851673	13.432627
21.085475	1436.362639	13.437632
21.619443	1426.913402	13.442637
21.147958	1423.968778	13.447642
21.096140	1409.123457	13.452647
21.463712	1434.386778	13.457651
21.208624	1440.112663	13.462656
21.657994	1420.047965	13.467661
21.091337	1429.879570	13.472666
21.068797	1414.890797	13.477671
21.534205	1427.027374	13.482675
21.112463	1440.833559	13.487680
21.354632	1438.697659	13.492685
21.181545	1445.462326	13.497690
21.704117	1437.314346	13.502695
21.097696	1421.414141	13.507699
21.343888	1423.008772	13.512704
21.651293	1423.977036	13.517709
21.295320	1419.198869	13.522714
21.096632	1411.938662	13.527719
21.378880	1408.033294	13.532723
21.083888	1410.349764	13.537728
21.247501	1401.954693	13.542733
21.126220	1418.661916	13.547738
21.369583	1439.281881	13.552743
21.225330	1446.576552	13.557747
21.040556	1447.713202	13.562752
21.612403	1441.055510	13.567757
21.522371	1447.262868	13.572762
20.948082	1430.581645	13.577767
21.455163	1429.934759	13.582771
21.281521	1438.768531	13.587776
21.235093	1437.866136	13.592781
21.557082	1443.760193	13.597786
21.328483	1433.915314	13.602791
20.957483	1416.287028	13.607795
21.021889	1432.923651	13.612800
21.475338	1433.699885	13.617805
21.439123	1448.029657	13.622810
21.400899	1451.893220	13.627815
21.268331	1450.080441	13.632819
21.306505	1454.874866	13.637824
21.573902	1437.851233	13.642829
21.384900	1420.827868	13.647834
21.363288	1420.402500	13.652839
21.518863	1403.305276	13.657843
21.185002	1414.156328	13.662848
21.323669	1401.795941	13.667853
21.220600	1413.018626	13.672858
21.112820	1416.637799	13.677863
21.548041	1415.554508	13.682867
21.286262	1419.135163	13.687872
21.511452	1408.334813	13.692877
21.235553	1416.114100	13.697882
21.421098	1417.477123	13.702887
21.436590	1407.508177	13.707891
21.316776	1410.936875	13.712896
21.512322	1410.658228	13.717901
21.218831	1415.614348	13.722906
21.134080	1407.679942	13.727911
21.423722	1410.994451	13.732915
20.988581	1419.311660	13.737920
21.570009	1407.962472	13.742925
21.190671	1422.619762	13.747930
20.858507	1414.932975	13.752935
21.285055	1401.195692	13.757939
20.928499	1425.552593	13.762944
21.267375	1419.368895	13.767949
21.312180	1415.343694	13.772954
21.507004	1414.931118	13.777959
21.441083	1417.770889	13.782963
21.308219	1415.179127	13.787968
21.288542	1414.277198	13.792973
21.101013	1422.043972	13.797978
21.315087	1413.345949	13.802983
21.580753	1408.771426	13.807987
21.299474	1424.701483	13.812992
21.343897	1412.657324	13.817997
21.344447	1413.045305	13.823002
21.504197	1433.839451	13.828007
21.119129	1421.559422	13.833011
21.233395	1420.377504	13.838016
21.312116	1426.378161	13.843021
21.273281	1423.796633	13.848026
21.150717	1419.110555	13.853031
21.582693	1415.573977	13.858035
21.324454	1418.704624	13.863040
21.379135	1407.086199	13.868045
21.356954	1418.576692	13.873050
21.260929	1421.582118	13.878055
21.412019	1417.421691	13.883059
21.262964	1422.165538	13.888064
21.583052	1414.972407	13.893069
21.421327	1424.173286	13.898074
21.430119	1418.214124	13.903079
21.517729	1416.888220	13.908083
21.400192	1423.008488	13.913088
21.611211	1420.167910	13.918093
21.106454	1423.416724	13.923098
21.419629	1418.098164	13.928103
21.346946	1416.444578	13.933107
21.059640	1424.310847	13.938112
21.479362	1414.775757	13.943117
21.376081	1415.263878	13.948122
21.211453	1420.267259	13.953127
21.518058	1413.849006	13.958131
21.156124	1423.017158	13.963136
21.266096	1420.971731	13.968141
21.343832	1412.497307	13.973146
21.258488	1427.569774	13.978151
21.286896	1421.366202	13.983155
21.212967	1428.969778	13.988160
21.369450	1414.181119	13.993165
21.502498	1432.445292	13.998170
21.160546	1428.532234	14.003175
21.439423	1422.365988	14.008179
21.222071	1431.101067	14.013184
21.293251	1426.418781	14.018189
21.205667	1426.911593	14.023207
21.218870	1422.830898	14.028224
21.383765	1424.140182	14.033242
21.261638	1432.760805	14.038259
21.472118	1422.583262	14.043277
21.619082	1422.882411	14.048295
21.489802	1431.313845	14.053312
21.637049	1427.509062	14.058330
21.083764	1429.052432	14.063347
21.539254	1433.563562	14.068365
21.502033	1432.375740	14.073383
21.439185	1430.811345	14.078400
21.470326	1432.631157	14.083418
21.183068	1437.847464	14.088435
21.294136	1441.079644	14.093453
21.474711	1432.107043	14.098471
21.191166	1431.697804	14.103488
21.542632	1429.653641	14.108506
21.266474	1441.328382	14.113523
21.526940	1433.823208	14.118541
21.485270	1436.925595	14.123559
21.207258	1433.032909	14.128576
21.535408	1446.714342	14.133594
21.549444	1471.999402	14.138611
21.700944	1464.201714	14.143629
21.626536	1476.478217	14.148647
21.563876	1469.729253	14.153664
21.879786	1479.904929	14.158682
21.662513	1480.767097	14.163699
22.001857	1476.264722	14.168717
21.827289	1482.255854	14.173735
21.899621	1479.246349	14.178752
21.991762	1474.402739	14.183770
21.937729	1476.634103	14.188787
21.756640	1471.678346	14.193805
22.003161	1480.402220	14.198823
21.511246	1480.842587	14.203840
21.625433	1469.547824	14.208858
21.930276	1474.440058	14.213875
21.960042	1480.793418	14.218893
21.899500	1470.835239	14.223911
21.739020	1483.658715	14.228928
21.801101	1470.453227	14.233946
21.607209	1491.021090	14.238963
22.034644	1497.613834	14.243981
22.205302	1506.120168	14.248999
22.231977	1517.156804	14.254016
22.391017	1504.061660	14.259034
22.227017	1507.515471	14.264051
22.169997	1502.022405	14.269069
22.500229	1501.526286	14.274087
22.273780	1490.561891	14.279104
22.266996	1480.011556	14.284122
22.156597	1485.563032	14.289139
22.211442	1472.294204	14.294157
22.019724	1489.567903	14.299175
22.075779	1506.321561	14.304192
22.419802	1506.982529	14.309210
22.289167	1511.338630	14.314227
22.188859	1512.627300	14.319245
22.497569	1519.011692	14.324263
22.470729	1518.021976	14.329280
22.375212	1508.374508	14.334298
22.269392	1524.138643	14.339315
22.267082	1521.510685	14.344333
22.451523	1516.484031	14.349351
22.239382	1521.822092	14.354368
22.298485	1508.228518	14.359386
22.332099	1518.553061	14.364403
22.354435	1516.561377	14.369421
22.422119	1510.795168	14.374439
22.173305	1516.565354	14.379456
22.596409	1513.795620	14.384474
22.425807	1528.478441	14.389491
22.817593	1536.406847	14.394509
22.840278	1543.687852	14.399527
22.460896	1535.339308	14.404544
22.677183	1548.219153	14.409562
22.827084	1541.620294	14.414579
22.721010	1556.544530	14.419597
22.583721	1546.478992	14.424615
22.518170	1550.236428	14.429632
22.732732	1546.128303	14.434650
22.775557	1542.497443	14.439667
22.819937	1548.760415	14.444685
23.197975	1540.767686	14.449703
22.920809	1549.063902	14.454720
23.268990	1534.851632	14.459738
23.039637	1547.889063	14.464755
22.944547	1540.044148	14.469773
22.800299	1545.423298	14.474791
23.120212	1539.737971	14.479808
22.953711	1538.404022	14.484826
23.057967	1536.032765	14.489843
22.811000	1542.678819	14.494861
22.935284	1543.039789	14.499879
22.908297	1552.073161	14.504896
23.110594	1551.847549	14.509914
23.421052	1542.110144	14.514931
23.167884	1548.349786	14.519949
23.555301	1534.722702	14.524967
23.343783	1548.915006	14.529984
23.378055	1526.389243	14.535002
23.492200	1523.736420	14.540019
23.260830	1516.550310	14.545037
23.354888	1506.351952	14.550055
23.022948	1516.780410	14.555072
23.194924	1504.913275	14.560090
23.338717	1505.120127	14.565107
23.101402	1517.968470	14.570125
23.129514	1517.026618	14.575143
23.554875	1532.894805	14.580160
23.296356	1533.765126	14.585178
23.545554	1544.563379	14.590195
23.283300	1543.741764	14.595213
23.709222	1531.807366	14.600231
23.115656	1539.236988	14.605248
23.381549	1527.189693	14.610266
23.681064	1524.232033	14.615283
23.566157	1523.135243	14.620301
23.551877	1531.291997	14.625319
23.321995	1535.328888	14.630336
23.522106	1534.740266	14.635354
23.750952	1524.919936	14.640371
23.397138	1542.759083	14.645389
23.940592	1535.295239	14.650407
23.744257	1538.732192	14.655424
23.632123	1535.884226	14.660442
23.931252	1533.513350	14.665459
23.616402	1537.645588	14.670477
23.667741	1533.366875	14.675495
23.747446	1536.339817	14.680512
23.778120	1531.517002	14.685530
23.618743	1537.766850	14.690547
23.500641	1535.383866	14.695565
23.949755	1527.515084	14.700583
23.835006	1537.204222	14.705600
23.655299	1533.825926	14.710618
23.677559	1540.526567	14.715635
23.806086	1535.686571	14.720653
23.651304	1530.072236	14.725671
23.684293	1535.218628	14.730688
23.726656	1533.513177	14.735706
24.187064	1539.162396	14.740723
23.904028	1544.098076	14.745741
24.112956	1543.629167	14.750759
23.819517	1547.174416	14.755776
24.177294	1542.930196	14.760794
24.115086	1550.196430	14.765811
23.887998	1546.322333	14.770829
24.188309	1553.187841	14.775847
24.005472	1576.604314	14.780864
24.158860	1572.074939	14.785882
24.139302	1574.752268	14.790899
23.908931	1579.528555	14.795917
24.541637	1564.253154	14.800935
24.552165	1571.578584	14.805952
24.399365	1564.184869	14.810970
24.309778	1576.179166	14.815987
24.375454	1571.004698	14.821005
24.529112	1563.617163	14.826023
24.418654	1580.280274	14.831040
24.518701	1569.585424	14.836058
24.662618	1558.579999	14.841075
24.144941	1546.582152	14.846093
24.698085	1550.168559	14.851111
24.423437	1548.519957	14.856128
24.560819	1542.514537	14.861146
24.588030	1529.462417	14.866163
24.335789	1547.771423	14.871181
24.312976	1545.579302	14.876199
24.429499	1555.252016	14.881216
24.434445	1562.457210	14.886234
24.633309	1573.562380	14.891251
24.258625	1580.139160	14.896269
24.686640	1569.939405	14.901287
24.475878	1575.631187	14.906304
24.353300	1576.353991	14.911322
24.811644	1570.432649	14.916339
24.903797	1570.473135	14.921357
24.776821	1563.157098	14.926375
24.813761	1568.444440	14.931392
24.654538	1573.232972	14.936410
25.037596	1562.540181	14.941427
24.898022	1564.511501	14.946445
24.851135	1560.814722	14.951463
24.963096	1571.274668	14.956480
24.728184	1567.000700	14.961498
24.790473	1579.211445	14.966515
24.648174	1568.157281	14.971533
25.068591	1564.570012	14.976551
25.113819	1560.974943	14.981568
25.222936	1561.041037	14.986586
25.419126	1568.849649	14.991603
24.807336	1565.898897	14.996621
25.023320	1566.992412	15.001639
25.105766	1565.815381	15.006656
25.005960	1570.014003	15.011674
25.169612	1570.763515	15.016691
24.949400	1566.268558	15.021709
25.008926	1561.837524	15.026727
24.961507	1571.199776	15.031744
24.653984	1580.155214	15.036762
25.344750	1578.604318	15.041779
24.983179	1600.839707	15.046797
25.326330	1606.509227	15.051815
25.442805	1601.553157	15.056832
25.050764	1607.472060	15.061850
25.667415	1604.278194	15.066867
25.266830	1609.665216	15.071885
25.705437	1600.572710	15.076903
25.476508	1593.357859	15.081920
25.621642	1603.788943	15.086938
25.719977	1585.886906	15.091955
25.439307	1608.060641	15.096973
25.636531	1605.726454	15.101991
25.736326	1596.639223	15.107008
25.399694	1597.013930	15.112026
25.660753	1600.875016	15.117043
26.061008	1594.760012	15.122061
25.704720	1578.358765	15.127079
25.627751	1572.459877	15.132096
25.112975	1574.439129	15.137114
25.845344	1584.592505	15.142131
25.367266	1594.676246	15.147149
25.408369	1597.329747	15.152167
25.902863	1590.548497	15.157184
25.729303	1604.807160	15.162202
25.782201	1600.616266	15.167219
25.469776	1598.618187	15.172237
25.901954	1589.466939	15.177255
25.909288	1583.254160	15.182272
25.594757	1597.923827	15.187290
26.197685	1592.248399	15.192307
25.701099	1591.166858	15.197325
25.790936	1589.817190	15.202343
25.963493	1589.327339	15.207360
25.739785	1596.254419	15.212378
25.920111	1588.894078	15.217395
26.115505	1600.358464	15.222413
25.807728	1580.290700	15.227431
26.009972	1591.178272	15.232448
25.847800	1600.433005	15.237466
26.281352	1591.651190	15.242483
26.352196	1601.927384	15.247501
25.991146	1596.416704	15.252519
26.130775	1589.459247	15.257536
26.037273	1590.230896	15.262554
26.382039	1610.610777	15.267571
26.287669	1622.498911	15.272589
26.439946	1614.756074	15.277607
26.399544	1598.782615	15.282624
26.266442	1606.871848	15.287642
26.326045	1597.424519	15.292659
26.131369	1606.918815	15.297677
25.999579	1617.922600	15.302695
26.335750	1610.892890	15.307712
26.355284	1624.173834	15.312730
26.929025	1617.395663	15.317747
26.689079	1619.518276	15.322765
26.810948	1614.968747	15.327783
26.827777	1616.421211	15.332800
26.750599	1603.486344	15.337818
26.840540	1586.052824	15.342835
26.856650	1582.470258	15.347853
26.456974	1582.798391	15.352871
26.625647	1585.742997	15.357888
26.627489	1587.850639	15.362906
26.552752	1585.920044	15.367923
26.231789	1593.180378	15.372941
26.436382	1611.536154	15.377959
26.894737	1608.059226	15.382976
26.797979	1618.665749	15.387994
26.776462	1616.959465	15.393011
26.687703	1616.670162	15.398029
26.632867	1611.540067	15.403047
26.835936	1610.153463	15.408064
26.904602	1616.377985	15.413082
27.218466	1614.970564	15.418099
27.000003	1616.399207	15.423117
26.995588	1616.960025	15.428135
27.337837	1609.301722	15.433152
27.330197	1617.199495	15.438170
27.350499	1610.940592	15.443187
27.089953	1605.069394	15.448205
26.785137	1607.465040	15.453223
26.972185	1608.298911	15.458240
26.859488	1612.425670	15.463258
27.024819	1610.634533	15.468275
27.261876	1612.883987	15.473293
27.189857	1615.410818	15.478311
27.277261	1610.398035	15.483328
27.014261	1616.820169	15.488346
27.277813	1612.007376	15.493363
27.183897	1619.531954	15.498381
27.212525	1614.133722	15.503399
27.281883	1607.058478	15.508416
27.053054	1618.066728	15.513434
27.198601	1610.721361	15.518451
27.260281	1612.828901	15.523469
27.199838	1618.644589	15.528487
27.255792	1625.752019	15.533504
26.977665	1640.392328	15.538522
27.065670	1657.747455	15.543539
27.751935	1643.432398	15.548557
27.242219	1646.309033	15.553575
27.522638	1641.668144	15.558592
27.405221	1648.045051	15.563610
27.554863	1639.395001	15.568627
27.559675	1640.679501	15.573645
27.805024	1654.871403	15.578663
27.710627	1645.970839	15.583680
27.892459	1647.359238	15.588698
27.759628	1641.558891	15.593715
28.010482	1646.184520	15.598733
27.673352	1646.081116	15.603751
27.907150	1642.243598	15.608768
27.550771	1648.026271	15.613786
27.977795	1645.468243	15.618803
27.853318	1649.063646	15.623821
28.002222	1646.435144	15.628839
27.876272	1640.010793	15.633856
27.627783	1652.625088	15.638874
27.483440	1639.763820	15.643891
27.883333	1653.808381	15.648909
28.208483	1665.934806	15.653927
28.383512	1672.730692	15.658944
28.182447	1675.974953	15.663962
28.543130	1668.570078	15.668979
28.380025	1642.476590	15.673997
28.301328	1645.319091	15.679015
28.484975	1645.184540	15.684032
28.070094	1633.011354	15.689050
28.105942	1639.953687	15.694067
28.403734	1640.848548	15.699085
28.349403	1633.726951	15.704103
28.261191	1637.508473	15.709120
27.931229	1646.146639	15.714138
27.923679	1637.980975	15.719155
28.128088	1654.169246	15.724173
28.073440	1676.933092	15.729191
28.610013	1663.994668	15.734208
28.462625	1674.123250	15.739226
28.586510	1670.196290	15.744243
29.014669	1665.923508	15.749261
29.098102	1660.802804	15.754279
28.999945	1645.346584	15.759296
28.901626	1638.711764	15.764314
28.696481	1619.956758	15.769331
28.990409	1636.509825	15.774349
28.543434	1632.530775	15.779367
28.990567	1624.014185	15.784384
28.673954	1628.349645	15.789402
28.783188	1631.918781	15.794419
28.669736	1616.358067	15.799437
28.806020	1632.851330	15.804455
28.680836	1622.815268	15.809472
28.485440	1627.269819	15.814490
28.715804	1627.412530	15.819507
28.738993	1630.257654	15.824525
28.809526	1631.204488	15.829543
29.295726	1621.080360	15.834560
28.966394	1625.084373	15.839578
28.989611	1627.887022	15.844595
29.239302	1619.576525	15.849613
28.874812	1632.742547	15.854631
29.047130	1622.817911	15.859648
28.758339	1631.558039	15.864666
28.979219	1624.018183	15.869683
29.323469	1648.865505	15.874701
28.944930	1657.588502	15.879719
29.272457	1651.414289	15.884736
29.248710	1659.212409	15.889754
29.240152	1664.826361	15.894771
29.205114	1659.101644	15.899789
29.399273	1661.419294	15.904807
29.378405	1652.602951	15.909824
29.661199	1661.524068	15.914842
29.469521	1640.740865	15.919859
29.541571	1622.237372	15.924877
29.144191	1635.002809	15.929895
29.206448	1635.011885	15.934912
29.518429	1645.042017	15.939930
29.383470	1654.715581	15.944947
29.754290	1649.108608	15.949965
29.626561	1647.828239	15.954983
29.625434	1660.560390	15.960000
29.552844	1657.824068	15.965018
29.473800	1648.938356	15.970035
29.755912	1647.866325	15.975053
29.621932	1649.929572	15.980071
29.791910	1653.353748	15.985088
29.585775	1639.772464	15.990106
29.611577	1648.459284	15.995123
29.687050	1645.598679	16.000141
29.459791	1655.445835	16.005159
29.697111	1642.602346	16.010176
29.970440	1647.487083	16.015194
29.802220	1651.194853	16.020211
29.794659	1651.622470	16.025229
29.658124	1656.331906	16.030247
29.628838	1654.143947	16.035264
29.806964	1647.674243	16.040282
29.463655	1665.502427	16.045299
30.116446	1667.616376	16.050317
29.845170	1685.346581	16.055335
30.004226	1690.617639	16.060352
30.194982	1683.389292	16.065370
29.742567	1685.196593	16.070387
30.189831	1686.289411	16.075405
30.246143	1690.406542	16.080423
30.199717	1677.432099	16.085440
30.482800	1682.242933	16.090458
30.215433	1678.120397	16.095475
30.732356	1683.939984	16.100493
30.628293	1677.430329	16.105511
30.450437	1682.259620	16.110528
30.471123	1680.320086	16.115546
30.266509	1685.260610	16.120563
30.523642	1675.479711	16.125581
30.466959	1685.397210	16.130599
30.429361	1670.074448	16.135616
30.618187	1675.573556	16.140634
30.500386	1682.527831	16.145651
30.737841	1682.958844	16.150669
30.891834	1691.002336	16.155687
30.662808	1687.597264	16.160704
30.628639	1685.455695	16.165722
30.683869	1688.762902	16.170739
30.814450	1679.593632	16.175757
30.698585	1681.163218	16.180775
30.613721	1688.447291	16.185792
30.691405	1682.235834	16.190810
30.471835	1689.008144	16.195827
30.462099	1686.604706	16.200845
30.338739	1689.729613	16.205863
30.476348	1691.965053	16.210880
30.861433	1691.705569	16.215898
30.675098	1705.705250	16.220915
31.096941	1720.814446	16.225933
31.107336	1711.189276	16.230951
31.255582	1725.489542	16.235968
31.427881	1711.923341	16.240986
31.181749	1697.678282	16.246003
31.046952	1689.949728	16.251021
31.025477	1684.504405	16.256039
30.987288	1703.156989	16.261056
30.981829	1704.075050	16.266074
31.166954	1716.407890	16.271091
31.476601	1712.828815	16.276109
31.450815	1724.942046	16.281127
31.243989	1713.627504	16.286144
31.271787	1718.065363	16.291162
30.982750	1707.567742	16.296179
31.270262	1726.498744	16.301197
31.351791	1714.461821	16.306215
31.216811	1715.587726	16.311232
31.468521	1701.774492	16.316250
31.085277	1721.292226	16.321267
31.230725	1703.075795	16.326285
31.572791	1716.539764	16.331303
31.278818	1707.392568	16.336320
31.521659	1715.593363	16.341338
31.428133	1721.297965	16.346355
31.494493	1728.570525	16.351373
31.560148	1745.487307	16.356391
31.693432	1744.476758	16.361408
31.765081	1752.311623	16.366426
31.665015	1756.897300	16.371443
31.539515	1755.910718	16.376461
31.964722	1738.972526	16.381479
31.548326	1751.133917	16.386496
31.859885	1747.109367	16.391514
31.735252	1743.583813	16.396531
32.015482	1739.244941	16.401549
32.086575	1743.021533	16.406567
32.127348	1753.530716	16.411584
32.196919	1736.334643	16.416602
32.514474	1748.957847	16.421619
32.402900	1748.923860	16.426637
32.241800	1743.065060	16.431655
32.218924	1742.192672	16.436672
32.631087	1733.993051	16.441690
32.476823	1747.182277	16.446707
32.404159	1732.302338	16.451725
32.658187	1729.683797	16.456743
32.475107	1714.244193	16.461760
32.341177	1710.101939	16.466778
32.143561	1710.559868	16.471795
32.263929	1702.166131	16.476813
32.309562	1707.762019	16.481831
32.452478	1733.816630	16.486848
32.580708	1731.888252	16.491866
32.562146	1733.055366	16.496883
32.545606	1739.735545	16.501901
32.658229	1736.949221	16.506919
32.440821	1726.962400	16.511936
32.595268	1730.645472	16.516954
32.218213	1727.303322	16.521971
32.771910	1735.004673	16.526989
32.647664	1738.242988	16.532007
32.434767	1738.574368	16.537024
32.700651	1732.694666	16.542042
32.595992	1740.562362	16.547059
32.148345	1741.258366	16.552077
32.563382	1742.183298	16.557095
32.798927	1738.163008	16.562112
32.734663	1739.961895	16.567130
32.513805	1753.580168	16.572147
32.768679	1763.157025	16.577165
33.305296	1753.855314	16.582183
32.980511	1769.333742	16.587200
33.252552	1768.829594	16.592218
33.460098	1770.475024	16.597235
33.230431	1752.105999	16.602253
33.185474	1738.129261	16.607271
32.810109	1740.802018	16.612288
33.313863	1750.661642	16.617306
33.098892	1754.134651	16.622323
32.881865	1760.724119	16.627341
33.456565	1761.110789	16.632359
33.130813	1764.574727	16.637376
33.964024	1761.682915	16.642394
33.630993	1756.570394	16.647411
33.555363	1741.283510	16.652429
33.498392	1734.481605	16.657447
33.334479	1726.757674	16.662464
33.503702	1733.784174	16.667482
33.438846	1741.379684	16.672499
33.653804	1758.752438	16.677517
33.923856	1755.137196	16.682535
33.639426	1747.451350	16.687552
33.442158	1738.803085	16.692570
33.676274	1734.499883	16.697587
33.884880	1752.921266	16.702605
33.719592	1733.801109	16.707623
33.482611	1748.567098	16.712640
33.987254	1750.957941	16.717658
34.367334	1753.395391	16.722675
34.143791	1756.375843	16.727693
34.281260	1729.424163	16.732711
33.683138	1731.434029	16.737728
33.755067	1721.693647	16.742746
33.654771	1736.426814	16.747763
33.725127	1738.871185	16.752781
33.786363	1746.558273	16.757799
33.872430	1759.504692	16.762816
34.304237	1758.308108	16.767834
34.047630	1755.023820	16.772851
33.989142	1766.448604	16.777869
34.318724	1757.179909	16.782887
33.834843	1762.533080	16.787904
34.063295	1769.262290	16.792922
33.992940	1766.811879	16.797939
33.944693	1768.847312	16.802957
33.947792	1758.023068	16.807975
33.982541	1769.083777	16.812992
34.476144	1782.078478	16.818010
34.515442	1794.824750	16.823027
34.450989	1787.105374	16.828045
34.703087	1787.416080	16.833063
34.167316	1795.423345	16.838080
34.498926	1801.461296	16.843098
34.715313	1794.615768	16.848115
34.668680	1791.754158	16.853133
34.735026	1790.474285	16.858151
34.474626	1792.935236	16.863168
34.579668	1789.385626	16.868186
34.915808	1787.335995	16.873203
34.486866	1791.536835	16.878221
34.676077	1790.334893	16.883239
34.881955	1796.963898	16.888256
34.774386	1783.508331	16.893274
34.611988	1791.863458	16.898291
34.458787	1796.086390	16.903309
34.726044	1788.131643	16.908327
34.532241	1798.736472	16.913344
34.825920	1797.308659	16.918362
35.131960	1805.334259	16.923379
35.160166	1804.253948	16.928397
35.328963	1803.352561	16.933415
35.152598	1813.265639	16.938432
35.151450	1810.102618	16.943450
35.256249	1814.273399	16.948467
35.011453	1809.019373	16.953485
35.638602	1801.016661	16.958503
35.410509	1817.014544	16.963520
35.568012	1812.396350	16.968538
35.563907	1807.586855	16.973555
35.353357	1811.707254	16.978573
35.624486	1791.762374	16.983591
35.526884	1792.610192	16.988608
35.279649	1783.699311	16.993626
35.731667	1791.094440	16.998643
35.533156	1800.254422	17.003661
36.046708	1792.834543	17.008679
35.347028	1798.000347	17.013696
35.380582	1793.719676	17.018714
35.772228	1792.115792	17.023731
35.463450	1807.837098	17.028749
35.619447	1796.923947	17.033767
35.565073	1811.917279	17.038784
35.702337	1807.332201	17.043802
35.819340	1802.814850	17.048819
35.760892	1809.278377	17.053837
35.718753	1804.507982	17.058855
35.399063	1802.454402	17.063872
35.860794	1791.457891	17.068890
36.085077	1797.159029	17.073907
35.732710	1799.280720	17.078925
35.804336	1804.704188	17.083943
36.054807	1816.059289	17.088960
36.351048	1829.134272	17.093978
36.062300	1831.657952	17.098995
36.128769	1835.093961	17.104013
36.483603	1829.231495	17.109031
36.357213	1838.162922	17.114048
36.534547	1824.329974	17.119066
36.678723	1816.626074	17.124083
36.235994	1812.300232	17.129101
36.369886	1789.545815	17.134119
36.373608	1798.607477	17.139136
36.162841	1809.181985	17.144154
36.457421	1805.167992	17.149171
36.542600	1828.040336	17.154189
36.845872	1821.887223	17.159207
36.471395	1820.746862	17.164224
36.250093	1827.678387	17.169242
36.447169	1823.140395	17.174259
36.350016	1830.659305	17.179277
36.601968	1825.069651	17.184295
36.748846	1823.075366	17.189312
36.598540	1822.907558	17.194330
36.707540	1826.841720	17.199347
36.753945	1830.044975	17.204365
37.035451	1818.886850	17.209383
36.959934	1834.058181	17.214400
36.803598	1824.648288	17.219418
36.906685	1816.711842	17.224435
36.687648	1828.786767	17.229453
36.955294	1838.627478	17.234471
37.087813	1846.136510	17.239488
37.261302	1852.833627	17.244506
37.031924	1848.719140	17.249523
37.090140	1853.631961	17.254541
37.123261	1847.556527	17.259559
36.842645	1856.135037	17.264576
36.941753	1860.353929	17.269594
37.175944	1848.594569	17.274611
36.982404	1857.571324	17.279629
36.910184	1857.943191	17.284647
37.267384	1859.527014	17.289664
37.390785	1879.624828	17.294682
37.652298	1886.509269	17.299699
37.919659	1882.082745	17.304717
37.907721	1874.436745	17.309735
37.868896	1854.841657	17.314752
37.703421	1851.925057	17.319770
37.722638	1842.411650	17.324787
37.705006	1844.618389	17.329805
37.733367	1846.979815	17.334823
37.870978	1852.900863	17.339840
37.747321	1844.212481	17.344858
37.980650	1842.338113	17.349875
37.720756	1847.699637	17.354893
37.843321	1851.911640	17.359911
37.741163	1841.281872	17.364928
37.539541	1846.572755	17.369946
38.036761	1866.360825	17.374963
37.802685	1874.263390	17.379981
38.129093	1877.170317	17.384999
38.344390	1883.012921	17.390016
38.424775	1871.490429	17.395034
38.295222	1876.636123	17.400051
38.209084	1880.941193	17.405069
38.441326	1873.363217	17.410087
38.380018	1875.580072	17.415104
38.244628	1861.387976	17.420122
38.575148	1860.515850	17.425139
38.249967	1850.843432	17.430157
38.344534	1848.465805	17.435175
38.512003	1863.062015	17.440192
38.514304	1875.501227	17.445210
38.494982	1874.142201	17.450227
38.340113	1878.436209	17.455245
38.337673	1872.328684	17.460263
38.530235	1875.860997	17.465280
37.951760	1876.253827	17.470298
38.678115	1876.023287	17.475315
38.788164	1883.271654	17.480333
38.644752	1866.529390	17.485351
38.627661	1865.465736	17.490368
38.723852	1883.909933	17.495386
38.774241	1873.726146	17.500403
38.716793	1872.544659	17.505421
38.756125	1891.367593	17.510439
39.088526	1894.998732	17.515456
38.902909	1907.895803	17.520474
39.054494	1902.447967	17.525491
39.106250	1903.671520	17.530509
39.141412	1899.404718	17.535527
39.434489	1907.481207	17.540544
39.410348	1897.494906	17.545562
39.455352	1896.696627	17.550579
39.366784	1901.006809	17.555597
39.093585	1893.440217	17.560615
39.088444	1893.875321	17.565632
39.210969	1903.051808	17.570650
39.537441	1894.837449	17.575667
39.579257	1901.319634	17.580685
39.404031	1893.570676	17.585703
39.317311	1893.855195	17.590720
39.488827	1898.644570	17.595738
39.585353	1895.750671	17.600755
39.294237	1901.851796	17.605773
39.458848	1896.272898	17.610791
39.733093	1888.773159	17.615808
39.544626	1902.310900	17.620826
39.878210	1893.124851	17.625843
39.652953	1906.040826	17.630861
39.870514	1892.528587	17.635879
39.803335	1891.386403	17.640896
39.617027	1896.751940	17.645914
39.845504	1889.979945	17.650931
40.003106	1899.923191	17.655949
40.057352	1910.853484	17.660967
39.915736	1910.992601	17.665984
39.905493	1919.158368	17.671002
40.078335	1920.714970	17.676019
40.354483	1934.839316	17.681037
40.251332	1928.161090	17.686055
40.507161	1927.736600	17.691072
40.534264	1930.779361	17.696090
40.573460	1904.473813	17.701107
40.388926	1898.571496	17.706125
40.119460	1893.922268	17.711143
40.534209	1880.616119	17.716160
40.260072	1880.593900	17.721178
40.353666	1896.847307	17.726195
40.498341	1910.448331	17.731213
40.490979	1915.473878	17.736231
40.711986	1915.122582	17.741248
40.542872	1920.164489	17.746266
40.862511	1914.957262	17.751283
40.788409	1926.755897	17.756301
40.682166	1925.986455	17.761319
41.061413	1903.983963	17.766336
40.437116	1921.100646	17.771354
40.758784	1918.944766	17.776371
40.826858	1916.275624	17.781389
40.851649	1905.668034	17.786407
41.061724	1909.626998	17.791424
40.480508	1915.382711	17.796442
40.636751	1917.583754	17.801459
40.780551	1908.006392	17.806477
40.548514	1918.938302	17.811495
41.182844	1922.151636	17.816512
41.096474	1930.480560	17.821530
41.232904	1940.647435	17.826547
41.445973	1936.396295	17.831565
41.164433	1931.657745	17.836583
41.386977	1925.303531	17.841600
41.403112	1943.740122	17.846618
41.509852	1932.724613	17.851635
41.299771	1928.767474	17.856653
41.402588	1948.203276	17.861671
41.785093	1928.617974	17.866688
41.547545	1942.997284	17.871706
41.718055	1939.512703	17.876723
41.690449	1931.099961	17.881741
41.770590	1935.878752	17.886759
42.103086	1930.801604	17.891776
41.906488	1933.371952	17.896794
42.180053	1930.586666	17.901811
42.404840	1929.412074	17.906829
42.028924	1923.077798	17.911847
41.807852	1902.689016	17.916864
41.675445	1896.224682	17.921882
42.025361	1923.567964	17.926899
42.063646	1925.599057	17.931917
42.007672	1927.083612	17.936935
42.235124	1924.321411	17.941952
41.723064	1930.665423	17.946970
41.983755	1919.202228	17.951987
42.113050	1926.702379	17.957005
41.931697	1923.328972	17.962023
42.095968	1920.721566	17.967040
41.818236	1929.817185	17.972058
42.132834	1922.449420	17.977075
42.622953	1930.967979	17.982093
42.236075	1943.691112	17.987111
42.410869	1939.844051	17.992128
42.298651	1951.801368	17.997146
42.711005	1960.514819	18.002163
42.952457	1956.149034	18.007181
42.526609	1955.622470	18.012199
42.586056	1951.321892	18.017216
42.590506	1955.604672	18.022234
42.592236	1962.783838	18.027251
42.891137	1955.920356	18.032269
43.003019	1967.749139	18.037287
43.211072	1950.271177	18.042304
42.914031	1957.985626	18.047322
43.018056	1955.987147	18.052339
42.932616	1953.103380	18.057357
42.927724	1955.611699	18.062375
43.317854	1948.986929	18.067392
43.509453	1947.863247	18.072410
43.136736	1946.478774	18.077427
43.399534	1942.855205	18.082445
43.220160	1949.959426	18.087463
43.046099	1946.562828	18.092480
43.329052	1947.936705	18.097498
43.398742	1941.595850	18.102515
43.428843	1946.223749	18.107533
43.547930	1945.912303	18.112551
43.592802	1940.413831	18.117568
43.612569	1944.771244	18.122586
43.390595	1951.476418	18.127603
43.491601	1946.700451	18.132621
43.665593	1944.071041	18.137639
43.516729	1945.383221	18.142656
43.463742	1949.694036	18.147674
43.560681	1952.305665	18.152691
43.797858	1948.291350	18.157709
43.320824	1960.372922	18.162727
43.480952	1968.945703	18.167744
43.470679	1973.480949	18.172762
43.719768	1980.826742	18.177779
44.089485	1974.500947	18.182797
43.877884	1976.518415	18.187815
43.777383	1981.749175	18.192832
43.905204	1978.007124	18.197850
43.667413	1985.395959	18.202867
43.656706	1978.334876	18.207885
43.670159	2004.511295	18.212903
44.080139	2000.898846	18.217920
44.232732	2011.088362	18.222938
44.213411	2004.824596	18.227955
44.433978	2003.924380	18.232973
44.130550	2009.058523	18.237991
44.588914	2003.209366	18.243008
44.721146	2008.712909	18.248026
44.671666	2005.258676	18.253043
44.726362	2003.257046	18.258061
44.792497	2010.880571	18.263079
44.729093	2002.789677	18.268096
44.552656	2001.765582	18.273114
45.109028	1993.237650	18.278131
45.133502	1989.238369	18.283149
45.010679	1989.077186	18.288167
45.269154	1988.334521	18.293184
45.071244	2005.139482	18.298202
44.906212	1995.411538	18.303219
45.348437	1988.286084	18.308237
45.282295	1995.372269	18.313255
45.336974	1992.170418	18.318272
45.667140	1994.312276	18.323290
45.411885	1975.467271	18.328307
45.121874	1966.396355	18.333325
44.851337	1979.285010	18.338343
45.157668	1982.003251	18.343360
45.010614	1986.697168	18.348378
45.135667	1993.277805	18.353395
45.635711	1987.999310	18.358413
45.568682	1991.529006	18.363431
45.596270	1984.035521	18.368448
45.772595	1980.326632	18.373466
45.499574	1990.849851	18.378483
45.632986	1982.313872	18.383501
45.650221	1978.254400	18.388519
45.231855	1976.181924	18.393536
45.573124	1990.907850	18.398554
45.287257	1982.910646	18.403571
45.734775	1997.176039	18.408589
45.763662	2012.222367	18.413607
45.853437	2028.141474	18.418624
45.789440	2022.174265	18.423642
45.682124	2010.771260	18.428659
45.879277	2013.491188	18.433677
45.934538	2024.111517	18.438695
45.971934	2020.140054	18.443712
45.943089	2017.278709	18.448730
45.710965	2018.527094	18.453747
46.680246	2028.927730	18.458765
46.549464	2044.501353	18.463783
46.039174	2042.010941	18.468800
46.315380	2034.010588	18.473818
46.261051	2048.930224	18.478835
46.557875	2059.930484	18.483853
46.752877	2058.559284	18.488871
46.885356	2051.439150	18.493888
46.824114	2053.550628	18.498906
46.409859	2048.918148	18.503923
46.790849	2045.129413	18.508941
47.025264	2052.661629	18.513959
46.548098	2047.770191	18.518976
46.798274	2035.097341	18.523994
46.770650	2046.316075	18.529011
46.992527	2032.408185	18.534029
46.907778	2038.276680	18.539047
47.016095	2040.807859	18.544064
47.227578	2042.649325	18.549082
47.034370	2040.072166	18.554099
46.992752	2030.829462	18.559117
47.087081	2036.173890	18.564135
46.455686	2041.947092	18.569152
46.983630	2048.320356	18.574170
46.823864	2044.087743	18.579187
47.204002	2056.296966	18.584205
47.189543	2073.300841	18.589223
47.377009	2074.770184	18.594240
47.580230	2069.524839	18.599258
47.377825	2069.852978	18.604275
47.554376	2068.255055	18.609293
47.870702	2068.093052	18.614311
47.392318	2066.267662	18.619328
47.433380	2061.642791	18.624346
47.813854	2070.893081	18.629363
47.801190	2066.797454	18.634381
47.937896	2064.302959	18.639399
48.006955	2057.696310	18.644416
48.293133	2056.648773	18.649434
47.750195	2065.629465	18.654451
47.972825	2065.287347	18.659469
48.254343	2057.822542	18.664487
47.771240	2071.722036	18.669504
48.072100	2057.007139	18.674522
48.115463	2055.023040	18.679539
48.200149	2049.246042	18.684557
47.912116	2070.254458	18.689575
48.235038	2079.705843	18.694592
48.387697	2077.548579	18.699610
48.169773	2094.035934	18.704627
48.389481	2094.446196	18.709645
48.710480	2083.530113	18.714663
48.168629	2090.860524	18.719680
48.227040	2086.907714	18.724698
48.621944	2093.904692	18.729715
48.619561	2092.612157	18.734733
48.301828	2094.898254	18.739751
48.773628	2088.320174	18.744768
49.105973	2079.820054	18.749786
48.775237	2087.102638	18.754803
48.968873	2084.128721	18.759821
49.040525	2088.298575	18.764839
48.777910	2086.721921	18.769856
48.950967	2086.744789	18.774874
48.896929	2109.798657	18.779891
49.009296	2107.421296	18.784909
49.009063	2102.870638	18.789927
49.297504	2113.103056	18.794944
49.482821	2100.678023	18.799962
49.160576	2108.572751	18.804979
49.096230	2111.710359	18.809997
49.585885	2111.166779	18.815015
49.718092	2105.688924	18.820032
49.623007	2113.736195	18.825050
49.494570	2111.046445	18.830067
49.621903	2105.600829	18.835085
49.633408	2110.223880	18.840103
49.576950	2105.084430	18.845120
49.901770	2099.412264	18.850138
49.577188	2120.649954	18.855155
49.746656	2104.054149	18.860173
49.739233	2100.594760	18.865191
49.694975	2112.506764	18.870208
49.756639	2102.401245	18.875226
49.888030	2122.666439	18.880243
49.944042	2127.252511	18.885261
50.241855	2139.218526	18.890279
49.943010	2144.740528	18.895296
50.137484	2130.696913	18.900314
50.099309	2140.745481	18.905331
50.000145	2136.591267	18.910349
50.366057	2132.380191	18.915367
50.519594	2141.150757	18.920384
50.512635	2139.438944	18.925402
50.729490	2130.697659	18.930419
50.937898	2131.079837	18.935437
50.570780	2138.336788	18.940455
50.495458	2137.269816	18.945472
50.795049	2135.515408	18.950490
50.649112	2132.381699	18.955507
50.570108	2133.217132	18.960525
50.763043	2132.535250	18.965543
50.685237	2127.880550	18.970560
50.432155	2133.912784	18.975578
50.517188	2133.738901	18.980595
50.679517	2145.117757	18.985613
51.187836	2155.519637	18.990631
50.904242	2164.890047	18.995648
51.329197	2148.424911	19.000666
51.340112	2147.814528	19.005683
51.004499	2162.477112	19.010701
51.214117	2145.097769	19.015719
51.286613	2146.764782	19.020736
51.380070	2143.632220	19.025754
51.461254	2155.418861	19.030771
51.512387	2150.241787	19.035789
51.842374	2139.198385	19.040807
51.647957	2148.246245	19.045824
51.764527	2134.602020	19.050842
51.785130	2148.723284	19.055859
51.638913	2144.785788	19.060877
51.937108	2137.798064	19.065895
51.508909	2146.916239	19.070912
51.942425	2141.991226	19.075930
51.748093	2141.106830	19.080947
51.558143	2136.034276	19.085965
51.870292	2127.509034	19.090983
51.670852	2140.491887	19.096000
51.977147	2142.063411	19.101018
51.784795	2141.855112	19.106035
51.792085	2151.638456	19.111053
52.210158	2159.084809	19.116071
51.980758	2170.894251	19.121088
52.217943	2160.763845	19.126106
51.988459	2166.573675	19.131123
52.318202	2174.282665	19.136141
52.399573	2174.759037	19.141159
51.957276	2179.501672	19.146176
52.689477	2176.657358	19.151194
52.800352	2190.024931	19.156211
53.016034	2192.870929	19.161229
53.123795	2182.772160	19.166247
53.127617	2174.527300	19.171264
53.082173	2163.727798	19.176282
53.043216	2157.803731	19.181299
52.766374	2169.192866	19.186317
53.026597	2154.794244	19.191335
53.020624	2158.940318	19.196352
53.159283	2162.072305	19.201370
52.964724	2154.175276	19.206387
53.052790	2165.341045	19.211405
53.227122	2169.566909	19.216423
53.220348	2174.925939	19.221440
53.372520	2186.995446	19.226458
53.284767	2193.732810	19.231475
53.399185	2196.830917	19.236493
53.465357	2184.799200	19.241511
53.326001	2191.296249	19.246528
53.406970	2188.705227	19.251546
53.635518	2174.509841	19.256563
53.859865	2183.835441	19.261581
53.706513	2183.351928	19.266599
53.785976	2192.846933	19.271616
53.791466	2182.075475	19.276634
53.501097	2182.096741	19.281651
53.585040	2183.577885	19.286669
53.739740	2186.914962	19.291687
53.665052	2189.786817	19.296704
53.721018	2206.699391	19.301722
53.901437	2206.606253	19.306739
53.807309	2219.325411	19.311757
54.169347	2205.070954	19.316775
53.941713	2212.972674	19.321792
54.510745	2208.606486	19.326810
54.181762	2208.309859	19.331827
54.066452	2217.585825	19.336845
54.427978	2209.008616	19.341863
54.556255	2219.296540	19.346880
54.770755	2228.839248	19.351898
54.756213	2211.656025	19.356915
54.381901	2211.413819	19.361933
54.411965	2217.328573	19.366951
54.526864	2236.855646	19.371968
54.775078	2225.952637	19.376986
54.441691	2234.778889	19.382003
54.485669	2241.669877	19.387021
54.915993	2233.017187	19.392039
54.976168	2241.102691	19.397056
54.909664	2240.152285	19.402074
55.219742	2234.778154	19.407091
55.458867	2254.804551	19.412109
55.575060	2240.510612	19.417127
55.308509	2239.975935	19.422144
55.285420	2233.291091	19.427162
55.201602	2237.740617	19.432179
55.288614	2256.631929	19.437197
55.720443	2250.606005	19.442215
55.471182	2263.087239	19.447232
55.337906	2254.241264	19.452250
55.622903	2258.685466	19.457267
55.432524	2262.831088	19.462285
55.808520	2251.943863	19.467303
55.826440	2255.425468	19.472320
55.830857	2268.338171	19.477338
55.958599	2268.409166	19.482355
55.718912	2268.834492	19.487373
55.700542	2261.127964	19.492391
56.177757	2267.216828	19.497408
55.782906	2267.451388	19.502426
56.457096	2265.527113	19.507443
56.407836	2285.015935	19.512461
56.599771	2284.636235	19.517479
56.403139	2272.520510	19.522496
56.587063	2259.769939	19.527514
56.508581	2254.907661	19.532531
56.343576	2258.596194	19.537549
56.628702	2250.592728	19.542567
56.682815	2270.313589	19.547584
56.622735	2280.461703	19.552602
56.748956	2282.837482	19.557619
56.499167	2288.763859	19.562637
56.765205	2279.045633	19.567655
56.769096	2287.854311	19.572672
56.942297	2283.997976	19.577690
57.228615	2283.994918	19.582707
56.879917	2291.500696	19.587725
57.138806	2288.939487	19.592743
57.165253	2283.177976	19.597760
57.016928	2291.004167	19.602778
57.364862	2277.297743	19.607795
56.961026	2273.984902	19.612813
57.364597	2280.145291	19.617831
57.104274	2281.198416	19.622848
57.200843	2279.482660	19.627866
57.205566	2276.000842	19.632883
57.036540	2289.457189	19.637901
57.404777	2302.585617	19.642919
57.266987	2312.831092	19.647936
57.388244	2300.670942	19.652954
57.712479	2311.844780	19.657971
57.727602	2308.535906	19.662989
57.942760	2302.385634	19.668007
57.907940	2301.219380	19.673024
57.853294	2308.034889	19.678042
58.189432	2308.528842	19.683059
57.880355	2309.920087	19.688077
58.085295	2322.926707	19.693095
58.470408	2332.549244	19.698112
58.347469	2336.221650	19.703130
58.230942	2324.052207	19.708147
58.701288	2334.435105	19.713165
58.636021	2324.255289	19.718183
58.931635	2328.554670	19.723200
58.744399	2313.225202	19.728218
58.704937	2301.936991	19.733235
58.510460	2298.804694	19.738253
58.712976	2305.683015	19.743271
58.961696	2297.701060	19.748288
58.893633	2311.364702	19.753306
58.880756	2305.137533	19.758323
58.885865	2321.904191	19.763341
58.943706	2318.821317	19.768359
59.031729	2317.802217	19.773376
58.728610	2319.968037	19.778394
58.998273	2323.145236	19.783411
58.856542	2329.556207	19.788429
58.690500	2329.908440	19.793447
58.902090	2326.714527	19.798464
58.661924	2346.240167	19.803482
59.091433	2342.520700	19.808499
59.081347	2354.123064	19.813517
59.065961	2344.345064	19.818535
59.169648	2363.710497	19.823552
59.691439	2383.161082	19.828570
60.083610	2371.066999	19.833587
59.991596	2376.901395	19.838605
60.190100	2359.224685	19.843623
60.355858	2342.143121	19.848640
60.103520	2348.243752	19.853658
60.157421	2347.456614	19.858675
60.137821	2341.611185	19.863693
60.227346	2348.122142	19.868711
60.150231	2336.283042	19.873728
59.981705	2344.073943	19.878746
60.500758	2335.815256	19.883763
60.305310	2339.054046	19.888781
60.146399	2344.530998	19.893799
60.571034	2337.173007	19.898816
60.376191	2335.818332	19.903834
60.209130	2336.486915	19.908851
60.314650	2346.949237	19.913869
60.534328	2358.463839	19.918887
60.847207	2367.249246	19.923904
60.639456	2362.165292	19.928922
60.807534	2353.824135	19.933939
60.588178	2377.353903	19.938957
60.698080	2367.696699	19.943975
60.930575	2362.245228	19.948992
60.920629	2363.832602	19.954010
60.984094	2370.612002	19.959027
61.263411	2378.778257	19.964045
61.188796	2393.789575	19.969063
61.286183	2395.741307	19.974080
61.071928	2399.287500	19.979098
61.270953	2407.782765	19.984115
61.236163	2399.217521	19.989133
61.031411	2394.492526	19.994151
61.401100	2394.408532	19.999168
61.200665	2399.073339	20.004186
61.740389	2408.521829	20.009203
61.960455	2430.484037	20.014221
61.714137	2420.107289	20.019239
62.233667	2420.940101	20.024256
61.849287	2417.537603	20.029274
62.290091	2407.749736	20.034291
62.267925	2427.850289	20.039309
62.144593	2414.956665	20.044327
62.586995	2415.004225	20.049344
62.083638	2422.747099	20.054362
62.280811	2414.444528	20.059379
62.591104	2414.897773	20.064397
62.654541	2407.015308	20.069415
62.771283	2409.056768	20.074432
62.442477	2404.784149	20.079450
62.640158	2394.486844	20.084467
62.839027	2397.094884	20.089485
62.580016	2404.721702	20.094503
62.637033	2394.311543	20.099520
62.584038	2392.495353	20.104538
62.800801	2403.532240	20.109555
62.722459	2411.933308	20.114573
62.764797	2396.801530	20.119591
62.836684	2406.755649	20.124608
62.768038	2413.945473	20.129626
62.703517	2401.406651	20.134643
62.838108	2400.914179	20.139661
62.464636	2443.483231	20.144679
63.176688	2432.038896	20.149696
62.977252	2451.116931	20.154714
63.078308	2432.805988	20.159731
63.371030	2458.660256	20.164749
63.490558	2460.157778	20.169767
63.792731	2469.241481	20.174784
63.502683	2466.291921	20.179802
64.136485	2474.149221	20.184819
64.350754	2470.585175	20.189837
64.014222	2463.306031	20.194855
64.226476	2459.118580	20.199872
64.331122	2470.911174	20.204890
64.483915	2447.743712	20.209907
64.104966	2432.426599	20.214925
64.155630	2432.868550	20.219943
64.297767	2428.298233	20.224960
64.130382	2442.930337	20.229978
64.167929	2446.089522	20.234995
64.421119	2458.313040	20.240013
63.918633	2462.275673	20.245031
64.399568	2459.096197	20.250048
64.556023	2459.794209	20.255066
64.177441	2459.852350	20.260083
64.373508	2461.808019	20.265101
64.814550	2485.986944	20.270119
65.196003	2490.154704	20.275136
64.844354	2500.875665	20.280154
64.885558	2491.140455	20.285171
64.966947	2494.051976	20.290189
64.867383	2496.614027	20.295207
65.353026	2492.435668	20.300224
65.030703	2496.713300	20.305242
65.298794	2490.037749	20.310259
65.225418	2487.236111	20.315277
65.303295	2489.340410	20.320295
65.470914	2475.575250	20.325312
65.332851	2482.545721	20.330330
65.381912	2482.965119	20.335347
65.712793	2490.228128	20.340365
65.484889	2504.638702	20.345383
65.609024	2502.835151	20.350400
65.771914	2514.620066	20.355418
65.583143	2504.051601	20.360435
65.553703	2504.536217	20.365453
65.530668	2516.149427	20.370471
65.888372	2520.763808	20.375488
65.955424	2541.721784	20.380506
65.908008	2542.479839	20.385523
66.377156	2527.758871	20.390541
66.187578	2534.344308	20.395559
66.357244	2526.059431	20.400576
66.430909	2530.870127	20.405594
66.167420	2530.563834	20.410611
66.468237	2520.878443	20.415629
66.380078	2528.219307	20.420647
66.965081	2519.343574	20.425664
66.528431	2539.967362	20.430682
66.610352	2542.074170	20.435699
67.150364	2537.640154	20.440717
66.971147	2555.488875	20.445735
66.951571	2554.507368	20.450752
67.448976	2558.255518	20.455770
66.981511	2554.484760	20.460787
67.453547	2563.579976	20.465805
67.169823	2540.006116	20.470823
67.637567	2544.576214	20.475840
67.433413	2548.732766	20.480858
67.336132	2552.736203	20.485875
67.514819	2543.040385	20.490893
67.516655	2539.030405	20.495911
67.672612	2551.517268	20.500928
68.075257	2551.777246	20.505946
68.037156	2539.646241	20.510963
67.854609	2539.253105	20.515981
67.668223	2538.549108	20.520999
68.156374	2535.488021	20.526016
67.938502	2550.623022	20.531034
67.759252	2547.685666	20.536051
68.158633	2551.665746	20.541069
68.149079	2575.944207	20.546087
68.296256	2562.518080	20.551104
68.506032	2582.930301	20.556122
68.512961	2574.880570	20.561139
68.310517	2583.797839	20.566157
68.594491	2576.353617	20.571175
68.590246	2566.850556	20.576192
68.612347	2573.804968	20.581210
68.543156	2583.042349	20.586227
68.725900	2575.780232	20.591245
68.376800	2576.497518	20.596263
68.397426	2593.040208	20.601280
68.537458	2599.019382	20.606298
68.960015	2604.655402	20.611315
69.229038	2606.383942	20.616333
69.151046	2603.220418	20.621351
69.251663	2596.610852	20.626368
69.406448	2604.749901	20.631386
69.265145	2614.171056	20.636403
69.393545	2623.068626	20.641421
69.353968	2632.782685	20.646439
69.410642	2629.025071	20.651456
69.729413	2624.011226	20.656474
69.830973	2635.584212	20.661491
69.968762	2620.452712	20.666509
69.646849	2619.189061	20.671527
69.922751	2625.204784	20.676544
70.251867	2624.129913	20.681562
70.013644	2622.297611	20.686579
70.413246	2614.923811	20.691597
70.187500	2628.502778	20.696615
70.206585	2620.418835	20.701632
70.142290	2622.236711	20.706650
70.288471	2620.127595	20.711667
70.346610	2622.729802	20.716685
70.189533	2631.537614	20.721703
70.716619	2641.807862	20.726720
70.681031	2647.929112	20.731738
70.742117	2644.840146	20.736755
70.907146	2653.393675	20.741773
70.856411	2654.274968	20.746791
70.830643	2646.742457	20.751808
70.887628	2660.898531	20.756826
70.893958	2647.626928	20.761843
70.811101	2650.607147	20.766861
70.919774	2655.080377	20.771879
71.288055	2673.105430	20.776896
71.437053	2669.180491	20.781914
71.503160	2684.223152	20.786931
71.859156	2673.065871	20.791949
71.773017	2677.339713	20.796967
71.633064	2674.907324	20.801984
71.974338	2686.057499	20.807002
71.498611	2680.072300	20.812019
71.741646	2667.258462	20.817037
71.917945	2679.573083	20.822055
71.729989	2671.434033	20.827072
71.967088	2674.968881	20.832090
71.933089	2677.455223	20.837107
72.196870	2667.527091	20.842125
72.275901	2671.566156	20.847143
72.047180	2673.716228	20.852160
72.004527	2686.863337	20.857178
72.361695	2705.798674	20.862195
72.561485	2704.583176	20.867213
72.470805	2703.480856	20.872231
72.584266	2717.860801	20.877248
72.594801	2700.669855	20.882266
72.478701	2706.217197	20.887283
73.061929	2700.071776	20.892301
73.250745	2684.846337	20.897319
73.160943	2702.022633	20.902336
73.102205	2688.064480	20.907354
72.988305	2700.082458	20.912371
73.245394	2702.747341	20.917389
73.235552	2713.980272	20.922407
73.394093	2712.758766	20.927424
73.746281	2717.185318	20.932442
73.604591	2718.606539	20.937459
73.908422	2712.957936	20.942477
73.697611	2689.192084	20.947495
73.685123	2689.727488	20.952512
73.631505	2687.621907	20.957530
73.800264	2711.364831	20.962547
74.133185	2711.892349	20.967565
74.187587	2714.031101	20.972583
74.685582	2709.573059	20.977600
74.672814	2687.244129	20.982618
74.303764	2680.169845	20.987635
74.354314	2678.339466	20.992653
74.261065	2673.773573	20.997671
74.090499	2673.597183	21.002688
74.274924	2687.087987	21.007706
74.165763	2702.953824	21.012723
74.374833	2698.713328	21.017741
74.431689	2708.163509	21.022759
74.216375	2709.604335	21.027776
74.488487	2712.796963	21.032794
74.476313	2726.337244	21.037811
74.772734	2734.371193	21.042829
75.026259	2731.410406	21.047847
75.131419	2727.730769	21.052864
75.121251	2728.425476	21.057882
75.117603	2735.176420	21.062899
75.413431	2730.629481	21.067917
75.483118	2729.219212	21.072935
74.966895	2722.063763	21.077952
75.218400	2740.550354	21.082970
75.698540	2759.474018	21.087987
75.615382	2762.905005	21.093005
75.807406	2762.432467	21.098023
75.633262	2760.321712	21.103040
75.955395	2760.043156	21.108058
75.515741	2764.337215	21.113075
75.633524	2766.045059	21.118093
75.610212	2771.947312	21.123111
75.777341	2785.908969	21.128128
76.068483	2779.884028	21.133146
76.143176	2785.596830	21.138163
76.540352	2777.024619	21.143181
76.638775	2788.455859	21.148199
76.392383	2779.373542	21.153216
77.219383	2786.306676	21.158234
76.558954	2794.178616	21.163251
77.087347	2791.477599	21.168269
77.099228	2794.309024	21.173287
77.037633	2782.226397	21.178304
77.278485	2762.929998	21.183322
77.241494	2765.045577	21.188339
77.044176	2772.304076	21.193357
77.196879	2797.094252	21.198375
77.431150	2801.252538	21.203392
77.827487	2790.279083	21.208410
77.488453	2795.317709	21.213427
77.675326	2767.110317	21.218445
77.542373	2760.189478	21.223463
77.310010	2778.874407	21.228480
78.158114	2783.257294	21.233498
77.955075	2793.053372	21.238515
77.806459	2797.607789	21.243533
78.154619	2794.672014	21.248551
78.068602	2792.627430	21.253568
78.397326	2793.402602	21.258586
78.036399	2793.614451	21.263603
78.174576	2784.035051	21.268621
77.980922	2785.739860	21.273639
78.042659	2798.828736	21.278656
78.492583	2782.657013	21.283674
78.311552	2797.104448	21.288691
78.278999	2801.074034	21.293709
78.571215	2805.687940	21.298727
78.387038	2829.802749	21.303744
78.756904	2816.043558	21.308762
78.681739	2823.293616	21.313779
78.651819	2815.921351	21.318797
79.110348	2823.485092	21.323815
78.950360	2821.980083	21.328832
79.038263	2849.353525	21.333850
79.385605	2855.016584	21.338867
79.245167	2861.885361	21.343885
79.426984	2842.569168	21.348903
79.435599	2850.348608	21.353920
79.478086	2844.804555	21.358938
79.482198	2844.699415	21.363955
79.460566	2856.635950	21.368973
79.857590	2848.309130	21.373991
79.985411	2860.551406	21.379008
79.994968	2874.259044	21.384026
80.131673	2863.237268	21.389043
80.011588	2869.909308	21.394061
80.279810	2877.789734	21.399079
80.216162	2872.490698	21.404096
80.088643	2864.687990	21.409114
80.366709	2867.458892	21.414131
80.252448	2868.982725	21.419149
80.528210	2874.020089	21.424167
80.301058	2895.832505	21.429184
80.518932	2890.522394	21.434202
80.809746	2904.621754	21.439219
80.784709	2898.430092	21.444237
81.283891	2895.888669	21.449255
81.026002	2893.180086	21.454272
81.233533	2897.416602	21.459290
81.021773	2889.777547	21.464307
81.213216	2892.648790	21.469325
81.702488	2910.028739	21.474343
81.373250	2917.368912	21.479360
81.751163	2907.362639	21.484378
81.810478	2909.416474	21.489395
81.797642	2911.702053	21.494413
81.777512	2896.849510	21.499431
81.279011	2914.284722	21.504448
81.574445	2910.354459	21.509466
81.664305	2912.703106	21.514483
81.303239	2918.014292	21.519501
82.101114	2920.096659	21.524519
81.972814	2949.018907	21.529536
82.009300	2947.665038	21.534554
82.327236	2953.769371	21.539571
82.516625	2948.724135	21.544589
82.969614	2938.963077	21.549607
82.823192	2940.184498	21.554624
82.992925	2939.183789	21.559642
83.087591	2939.154664	21.564659
82.721933	2942.838395	21.569677
83.367745	2932.640724	21.574695
82.994783	2943.711496	21.579712
82.954505	2939.774193	21.584730
83.055331	2941.443860	21.589747
83.036196	2945.919470	21.594765
83.068098	2946.609052	21.599783
83.125932	2963.162747	21.604800
83.285656	2973.649914	21.609818
83.546237	2967.378068	21.614835
83.520913	2971.425205	21.619853
84.064059	2969.702658	21.624871
83.996685	2960.240870	21.629888
83.816064	2960.572630	21.634906
83.875250	2956.694185	21.639923
83.972430	2967.566515	21.644941
84.256180	2956.834275	21.649959
84.158447	2976.212193	21.654976
83.950077	2989.168905	21.659994
84.298525	2991.949846	21.665011
84.113923	2993.410185	21.670029
84.837179	2983.551727	21.675047
84.592276	2983.220433	21.680064
84.923745	2995.796892	21.685082
84.758436	2987.633601	21.690099
84.666090	2987.817568	21.695117
84.855388	2997.623585	21.700135
84.739286	3001.932976	21.705152
84.970713	3015.322202	21.710170
85.393690	3010.597587	21.715187
85.008452	3016.972177	21.720205
85.566399	3012.443920	21.725223
85.444193	3012.517023	21.730240
85.127551	3010.563457	21.735258
85.447392	3015.018070	21.740275
85.698905	3031.072948	21.745293
85.956470	3034.280554	21.750311
85.809881	3045.555210	21.755328
85.776149	3041.503569	21.760346
85.940542	3036.341157	21.765363
85.578903	3038.826319	21.770381
86.054931	3032.171639	21.775399
86.024031	3039.763197	21.780416
85.734461	3049.495374	21.785434
86.286175	3051.965467	21.790451
86.361205	3064.531749	21.795469
86.562652	3058.386494	21.800487
86.507322	3062.544629	21.805504
86.601360	3065.922261	21.810522
86.778111	3055.521641	21.815539
86.567064	3063.948964	21.820557
86.938504	3077.256927	21.825575
86.719007	3086.228348	21.830592
86.938120	3102.347464	21.835610
87.321201	3095.568353	21.840627
87.341848	3086.344938	21.845645
87.548441	3087.113645	21.850663
87.467919	3095.120592	21.855680
87.424681	3083.406839	21.860698
87.689328	3090.598124	21.865715
87.674483	3102.056325	21.870733
88.174379	3107.053311	21.875751
88.104453	3113.713531	21.880768
87.938738	3108.610811	21.885786
88.139615	3114.364974	21.890803
88.128590	3113.906713	21.895821
88.568413	3116.768284	21.900839
88.279591	3110.650844	21.905856
88.200063	3112.247035	21.910874
88.433485	3106.689741	21.915891
88.294769	3120.740605	21.920909
88.625454	3124.712137	21.925927
88.677450	3135.408525	21.930944
88.908404	3140.945525	21.935962
89.138914	3141.028458	21.940979
88.778727	3146.202720	21.945997
89.097596	3137.434344	21.951015
89.279155	3143.042148	21.956032
89.307478	3147.931072	21.961050
89.499977	3130.834096	21.966067
89.328255	3140.960495	21.971085
89.478854	3140.770642	21.976103
89.724646	3149.568798	21.981120
89.716807	3161.443603	21.986138
89.935961	3154.217869	21.991155
89.685682	3159.566537	21.996173
90.003540	3154.785487	22.001191
89.916944	3169.540728	22.006208
90.258564	3155.723584	22.011226
90.397903	3145.628553	22.016243
90.521074	3155.128230	22.021261
90.730199	3145.939223	22.026279
90.775978	3143.992347	22.031296
90.657103	3146.365664	22.036314
90.969037	3138.305528	22.041331
90.813478	3132.520003	22.046349
90.918527	3137.605918	22.051367
91.135282	3137.695763	22.056384
91.063958	3137.890538	22.061402
90.993522	3140.417379	22.066419
90.820065	3139.686118	22.071437
91.102937	3157.273111	22.076455
91.204631	3168.669520	22.081472
91.255399	3177.550706	22.086490
91.545288	3163.669438	22.091507
91.782367	3172.192908	22.096525
91.811547	3161.073212	22.101543
91.664102	3168.734549	22.106560
91.509429	3172.636399	22.111578
91.946965	3182.657811	22.116595
91.840569	3191.862967	22.121613
91.720678	3195.774222	22.126631
92.137664	3189.128100	22.131648
92.003985	3199.218583	22.136666
92.208631	3199.272604	22.141683
92.301770	3216.276388	22.146701
92.594224	3221.803614	22.151719
92.594566	3235.992091	22.156736
92.366082	3238.954747	22.161754
92.909370	3224.814345	22.166771
92.782562	3240.428727	22.171789
92.577820	3234.385925	22.176807
92.850016	3230.154875	22.181824
93.283851	3250.695131	22.186842
93.365975	3245.164270	22.191859
93.035509	3249.417458	22.196877
93.326832	3246.853274	22.201895
93.763479	3250.876379	22.206912
93.517744	3271.393666	22.211930
93.940759	3271.556025	22.216947
94.118622	3269.290741	22.221965
93.687386	3274.223097	22.226983
94.184907	3270.595602	22.232000
94.131879	3274.937490	22.237018
94.429493	3276.329616	22.242035
94.216032	3272.459954	22.247053
94.418786	3256.998868	22.252071
94.578710	3263.526542	22.257088
94.409209	3272.728439	22.262106
94.603560	3279.805174	22.267123
94.415844	3289.638470	22.272141
94.774790	3303.524416	22.277159
94.966858	3298.124669	22.282176
94.860843	3296.942156	22.287194
95.178910	3293.089989	22.292211
95.067642	3299.867008	22.297229
95.237764	3310.558060	22.302247
95.216495	3314.587340	22.307264
95.374025	3327.195756	22.312282
96.118852	3315.395484	22.317299
96.032276	3319.082001	22.322317
95.949869	3323.806152	22.327335
96.237393	3319.653652	22.332352
96.085864	3320.009096	22.337370
96.359698	3304.726981	22.342387
96.285765	3317.452528	22.347405
96.638193	3314.252465	22.352423
96.647003	3304.579298	22.357440
96.675482	3317.815530	22.362458
96.851669	3296.028960	22.367475
97.001423	3310.616870	22.372493
96.549888	3291.128130	22.377511
96.706219	3299.426214	22.382528
96.472470	3311.581006	22.387546
96.738214	3312.235678	22.392563
96.624065	3318.471992	22.397581
96.646016	3307.274679	22.402599
97.116965	3332.892854	22.407616
96.884160	3341.164914	22.412634
96.838103	3337.395182	22.417651
97.063397	3353.981613	22.422669
97.045414	3372.645701	22.427687
97.223472	3368.864608	22.432704
97.628716	3371.454866	22.437722
97.973652	3388.192949	22.442739
98.278884	3401.347370	22.447757
98.096810	3403.848794	22.452775
98.423600	3388.016972	22.457792
98.197149	3401.368655	22.462810
98.270798	3395.198802	22.467827
98.621360	3393.609963	22.472845
98.419370	3394.415521	22.477863
98.566601	3400.569288	22.482880
98.247609	3395.999834	22.487898
98.784086	3409.376965	22.492915
98.848911	3430.062053	22.497933
98.910518	3426.202764	22.502951
99.507911	3414.709883	22.507968
99.302483	3430.529720	22.512986
99.436638	3425.851029	22.518003
99.476627	3413.066557	22.523021
99.255186	3420.049981	22.528039
99.717417	3422.116729	22.533056
99.724611	3436.957182	22.538074
100.223261	3441.460504	22.543091
100.183035	3442.337808	22.548109
100.136256	3448.241717	22.553127
100.373042	3442.522509	22.558144
100.118405	3444.635919	22.563162
100.427130	3445.150810	22.568179
100.404712	3443.564017	22.573197
100.141809	3441.040192	22.578215
100.558560	3438.466988	22.583232
100.565704	3447.253824	22.588250
100.507117	3458.790074	22.593267
100.868327	3470.496161	22.598285
100.865124	3465.540453	22.603303
100.915393	3461.698694	22.608320
100.757993	3478.296733	22.613338
100.880251	3469.581535	22.618355
101.229306	3472.736895	22.623373
101.281382	3486.998386	22.628391
101.278278	3497.827321	22.633408
101.418430	3493.872897	22.638426
101.559449	3484.925798	22.643443
101.749425	3493.744863	22.648461
101.786771	3519.290918	22.653479
101.822752	3515.032165	22.658496
102.219547	3529.219853	22.663514
102.184472	3525.969837	22.668531
102.389256	3518.483492	22.673549
102.119234	3525.513256	22.678567
102.411535	3515.368409	22.683584
102.679440	3533.607189	22.688602
102.800835	3533.556497	22.693619
103.042192	3536.854114	22.698637
102.934871	3544.996155	22.703655
103.452855	3531.257515	22.708672
103.422807	3538.779190	22.713690
103.405057	3548.508470	22.718707
103.454577	3542.126088	22.723725
103.233672	3540.931197	22.728743
103.437846	3529.466317	22.733760
103.353474	3539.613673	22.738778
103.444396	3562.443782	22.743795
103.375046	3558.411048	22.748813
103.539383	3574.206690	22.753831
103.954458	3568.060983	22.758848
104.100637	3583.173613	22.763866
103.912738	3590.812516	22.768883
104.474847	3594.811781	22.773901
104.466936	3604.343666	22.778919
104.790971	3590.256753	22.783936
105.052163	3589.252432	22.788954
104.974574	3592.799142	22.793971
104.949859	3592.240003	22.798989
104.817827	3590.009925	22.804007
105.436695	3581.571807	22.809024
104.996038	3588.461262	22.814042
105.012396	3602.903975	22.819059
105.451464	3609.447076	22.824077
105.792034	3623.027123	22.829095
105.767044	3617.980445	22.834112
105.932872	3616.811195	22.839130
106.137202	3606.342859	22.844147
106.173218	3608.162167	22.849165
106.234860	3614.063015	22.854183
106.352751	3611.970069	22.859200
106.347546	3606.368043	22.864218
106.605532	3605.321755	22.869235
106.560335	3602.696326	22.874253
106.051400	3606.377107	22.879271
106.303461	3605.725852	22.884288
106.692147	3604.023935	22.889306
106.927713	3595.267783	22.894323
107.026465	3600.107085	22.899341
106.776924	3617.773237	22.904359
106.799178	3620.830498	22.909376
107.223801	3627.202858	22.914394
106.886914	3627.647647	22.919411
107.340538	3628.082805	22.924429
107.273902	3635.873877	22.929447
107.297264	3655.640848	22.934464
107.124728	3653.479360	22.939482
107.269617	3657.068486	22.944499
107.387716	3657.113499	22.949517
107.699541	3682.379305	22.954535
107.890994	3687.747401	22.959552
108.265560	3679.250642	22.964570
108.136795	3694.131914	22.969587
108.536885	3708.260256	22.974605
108.517711	3710.337732	22.979623
108.585895	3718.587969	22.984640
108.898804	3714.017555	22.989658
108.815079	3719.502695	22.994675
109.160412	3708.715251	22.999693
108.984187	3714.592711	23.004711
109.714241	3709.353242	23.009728
109.884384	3701.654437	23.014746
109.553561	3708.837145	23.019763
109.455527	3705.352492	23.024781
109.689538	3703.862440	23.029799
109.664417	3718.628884	23.034816
109.859019	3726.585228	23.039834
109.869982	3728.361349	23.044851
110.279204	3721.304831	23.049869
109.634469	3733.343009	23.054887
110.104121	3726.672519	23.059904
110.298806	3736.958010	23.064922
110.111467	3749.863271	23.069939
110.221576	3746.081118	23.074957
110.477984	3757.246440	23.079975
110.546335	3757.887771	23.084992
111.025594	3770.994328	23.090010
111.029164	3791.327853	23.095027
111.180257	3785.522276	23.100045
111.312219	3782.959027	23.105063
111.387366	3783.112363	23.110080
111.533519	3777.436581	23.115098
111.699553	3785.773514	23.120115
111.492744	3785.268574	23.125133
111.552101	3793.407775	23.130151
111.982091	3797.803380	23.135168
112.000542	3815.204427	23.140186
112.315163	3817.862707	23.145203
112.624190	3800.798286	23.150221
112.467943	3807.047813	23.155239
112.577430	3811.568468	23.160256
112.919926	3802.641754	23.165274
112.673368	3812.093833	23.170291
113.151169	3793.092608	23.175309
112.778891	3799.323088	23.180327
113.149191	3789.953803	23.185344
113.409896	3789.711776	23.190362
113.260950	3800.837145	23.195379
113.374993	3792.323652	23.200397
113.333530	3795.070170	23.205415
113.469396	3789.045981	23.210432
113.765689	3798.637254	23.215450
113.308025	3803.054830	23.220467
113.582228	3810.560383	23.225485
113.692392	3810.378544	23.230503
113.593321	3819.494038	23.235520
113.629077	3833.970070	23.240538
113.919126	3850.569555	23.245555
114.086133	3851.307647	23.250573
113.977911	3853.444966	23.255591
114.148726	3869.254840	23.260608
114.631576	3878.166672	23.265626
114.504116	3875.124817	23.270643
114.835065	3878.796817	23.275661
115.018803	3887.289096	23.280679
115.307689	3901.977339	23.285696
115.500755	3917.178807	23.290714
115.580674	3911.332612	23.295731
115.940109	3900.047209	23.300749
115.575232	3910.989197	23.305767
115.671418	3908.693576	23.310784
115.849662	3899.765461	23.315802
115.686453	3903.071819	23.320819
115.809871	3913.460046	23.325837
116.095947	3923.827065	23.330855
116.127401	3922.754733	23.335872
116.421741	3923.053257	23.340890
116.365607	3925.957890	23.345907
116.918934	3929.859538	23.350925
117.154072	3941.394172	23.355943
116.857861	3941.470635	23.360960
117.488324	3943.747412	23.365978
117.379207	3954.593588	23.370995
117.015665	3943.891469	23.376013
117.511037	3939.975468	23.381031
117.684352	3945.875950	23.386048
117.453372	3946.423425	23.391066
117.285012	3947.722367	23.396083
117.697866	3933.973372	23.401101
117.839514	3953.524444	23.406119
117.829771	3970.735875	23.411136
118.204645	3953.232069	23.416154
118.127745	3963.078823	23.421171
118.484090	3963.841796	23.426189
118.759997	3951.618644	23.431207
118.879733	3956.554620	23.436224
118.751429	3943.751680	23.441242
118.503116	3963.201325	23.446259
118.886950	3950.514950	23.451277
119.254193	3959.291088	23.456295
119.228391	3986.120785	23.461312
119.713863	3975.150331	23.466330
119.356933	3991.201023	23.471347
119.495012	3983.059594	23.476365
119.865282	3986.024470	23.481383
119.643313	3981.495208	23.486400
119.955863	3978.735580	23.491418
119.878275	3987.172043	23.496435
119.696914	3975.061899	23.501453
120.105334	3998.693194	23.506471
120.040120	3990.831962	23.511488
120.324461	4000.164114	23.516506
120.563756	3993.148721	23.521523
120.431564	3999.720157	23.526541
120.073610	4018.544684	23.531559
120.211915	4033.357758	23.536576
120.739241	4027.635263	23.541594
120.548917	4052.398886	23.546611
121.026186	4062.446040	23.551629
121.185838	4058.403400	23.556647
121.151333	4081.255105	23.561664
121.678228	4074.965501	23.566682
121.690080	4087.656800	23.571699
121.865591	4090.237410	23.576717
122.025730	4092.814966	23.581735
122.079325	4090.075368	23.586752
122.731316	4081.843291	23.591770
122.189518	4091.083035	23.596787
122.441490	4085.709635	23.601805
122.733622	4101.635719	23.606823
122.636127	4115.710069	23.611840
122.895636	4109.953155	23.616858
122.900109	4116.659392	23.621875
122.923717	4109.086000	23.626893
122.858013	4110.547940	23.631911
123.034064	4127.027470	23.636928
123.417326	4132.391894	23.641946
123.790172	4149.862693	23.646963
123.504689	4147.148830	23.651981
124.007659	4148.924432	23.656999
123.950114	4140.475068	23.662016
124.019972	4142.522677	23.667034
124.128409	4143.744463	23.672051
124.254919	4161.721028	23.677069
124.529093	4158.270529	23.682087
124.423552	4167.368391	23.687104
125.034108	4160.628830	23.692122
124.648229	4166.571363	23.697139
124.610728	4157.179552	23.702157
125.030651	4158.501136	23.707175
124.992794	4164.360646	23.712192
124.984654	4150.942883	23.717210
125.202728	4174.868335	23.722227
125.394431	4181.123112	23.727245
125.142467	4187.695636	23.732263
125.552985	4197.140738	23.737280
125.815918	4184.977672	23.742298
125.742681	4190.495141	23.747315
125.713291	4200.690826	23.752333
126.223666	4197.389877	23.757351
126.427218	4205.312017	23.762368
126.532772	4207.225722	23.767386
126.579842	4195.984392	23.772403
126.497163	4205.997425	23.777421
127.030128	4216.293823	23.782439
126.869278	4234.395744	23.787456
127.361071	4229.829691	23.792474
127.107062	4229.685459	23.797491
127.000393	4240.489765	23.802509
127.487946	4231.313112	23.807527
127.325726	4234.325971	23.812544
127.642633	4250.740703	23.817562
127.837762	4259.167665	23.822579
128.184533	4256.084729	23.827597
128.223216	4263.683134	23.832615
128.323873	4264.434974	23.837632
128.408260	4254.282651	23.842650
128.411151	4253.576704	23.847667
127.937820	4259.585922	23.852685
128.543364	4278.857365	23.857703
128.539407	4284.849180	23.862720
128.734889	4278.030218	23.867738
128.958010	4300.448655	23.872755
128.911689	4303.191323	23.877773
129.267967	4306.554178	23.882791
129.061565	4321.328895	23.887808
129.458447	4314.667385	23.892826
130.005686	4330.330425	23.897843
129.812030	4334.373312	23.902861
129.968330	4348.913231	23.907879
130.039012	4337.455634	23.912896
130.140682	4344.033201	23.917914
130.250856	4336.499382	23.922931
130.532491	4338.929387	23.927949
130.876268	4331.810644	23.932967
130.429441	4361.408704	23.937984
130.591295	4355.271583	23.943002
130.810192	4354.668853	23.948019
130.966487	4360.634362	23.953037
131.255677	4360.202926	23.958055
131.107682	4369.856761	23.963072
131.398336	4384.374508	23.968090
131.222009	4395.265551	23.973107
131.550846	4394.847459	23.978125
132.145758	4381.207471	23.983143
131.698288	4399.511050	23.988160
131.714517	4403.119301	23.993178
132.172105	4408.717413	23.998195
132.051092	4413.046091	24.003213
132.370055	4403.067874	24.008231
132.663057	4407.900859	24.013248
132.537661	4407.834450	24.018266
132.922529	4421.845558	24.023283
132.812046	4433.515926	24.028301
133.295549	4423.151962	24.033319
133.071438	4442.677833	24.038336
133.218986	4442.281565	24.043354
133.393582	4434.011348	24.048371
133.146870	4470.615082	24.053389
133.478019	4467.926346	24.058407
133.815837	4472.300670	24.063424
133.904332	4471.868191	24.068442
134.038505	4485.607817	24.073459
134.192652	4499.738384	24.078477
134.676714	4495.892484	24.083495
134.969883	4495.576048	24.088512
135.030398	4492.169765	24.093530
135.171021	4494.912554	24.098547
134.943459	4490.233773	24.103565
135.441788	4485.620188	24.108583
135.455223	4478.748348	24.113600
135.353805	4481.586365	24.118618
135.253017	4492.054017	24.123635
135.347615	4514.256491	24.128653
135.595281	4509.314711	24.133671
135.694678	4520.569372	24.138688
135.791082	4538.810009	24.143706
136.224035	4541.290655	24.148723
135.890375	4553.898208	24.153741
136.046924	4547.226142	24.158759
136.328280	4557.455128	24.163776
136.349667	4569.191111	24.168794
136.282394	4569.341203	24.173811
136.602706	4581.857885	24.178829
137.030211	4597.501757	24.183847
137.349649	4605.215267	24.188864
137.128758	4610.042149	24.193882
137.278697	4606.030802	24.198899
137.475756	4607.877264	24.203917
137.398181	4628.540339	24.208935
137.665344	4638.206824	24.213952
137.960037	4634.365907	24.218970
138.028621	4633.450443	24.223987
138.206800	4655.320420	24.229005
138.411068	4658.508570	24.234023
138.700519	4657.707355	24.239040
138.625315	4672.325413	24.244058
139.334042	4644.470948	24.249075
138.950383	4664.153136	24.254093
139.066454	4658.731971	24.259111
139.509197	4657.431172	24.264128
139.505456	4647.155751	24.269146
139.596981	4645.816551	24.274163
139.465635	4682.959376	24.279181
139.955459	4667.959221	24.284199
139.940913	4683.864037	24.289216
139.720889	4677.561897	24.294234
140.063202	4675.150609	24.299251
139.909252	4682.776011	24.304269
140.276565	4697.667312	24.309287
140.539157	4700.780092	24.314304
140.931740	4714.175868	24.319322
140.759690	4709.982977	24.324339
141.081545	4717.726842	24.329357
141.464464	4713.883639	24.334375
141.724077	4721.514710	24.339392
141.688345	4720.468766	24.344410
141.903406	4730.610111	24.349427
141.908540	4727.733375	24.354445
141.773487	4733.702221	24.359463
142.156606	4723.428000	24.364480
142.170030	4720.251798	24.369498
142.293081	4715.295991	24.374515
141.879021	4734.428522	24.379533
142.276160	4742.152530	24.384551
142.353890	4758.040355	24.389568
142.338027	4761.225078	24.394586
142.476165	4773.875596	24.399603
142.938257	4787.422410	24.404621
142.640865	4786.746220	24.409639
143.030938	4796.595387	24.414656
143.385209	4814.093545	24.419674
143.942608	4816.905254	24.424691
143.640219	4820.116792	24.429709
143.739659	4825.184526	24.434727
144.064745	4823.139403	24.439744
144.178121	4840.201637	24.444762
144.795412	4830.755344	24.449779
144.671435	4834.651950	24.454797
144.905462	4835.686998	24.459815
144.865610	4828.619743	24.464832
144.893152	4833.484968	24.469850
145.157910	4844.367379	24.474867
145.145665	4866.596074	24.479885
145.257225	4869.243661	24.484903
145.597876	4853.430083	24.489920
145.526384	4871.002485	24.494938
145.785128	4862.794131	24.499955
145.763126	4877.731953	24.504973
146.109242	4879.394205	24.509991
146.054301	4887.829934	24.515008
146.262385	4893.839325	24.520026
146.062597	4875.253117	24.525043
146.115140	4907.233366	24.530061
146.414647	4914.521482	24.535079
146.528813	4923.032537	24.540096
146.516077	4934.967774	24.545114
146.970977	4934.907963	24.550131
147.082095	4956.621520	24.555149
147.239488	4953.596170	24.560167
147.126438	4967.912965	24.565184
147.504323	4977.855452	24.570202
147.788480	4965.484612	24.575219
147.791055	4987.332735	24.580237
148.092459	4984.394553	24.585255
148.446537	5000.981205	24.590272
148.105313	5001.702054	24.595290
148.581696	5002.209947	24.600307
148.680295	5006.104939	24.605325
148.670825	5024.129415	24.610343
148.923587	5042.163239	24.615360
148.970666	5034.597429	24.620378
149.235466	5038.071017	24.625395
148.957062	5065.012973	24.630413
149.565421	5072.813618	24.635431
149.769996	5063.300030	24.640448
149.852870	5065.269386	24.645466
150.208367	5094.428685	24.650483
150.277716	5086.232311	24.655501
150.471647	5087.943238	24.660519
150.428062	5091.433752	24.665536
150.477173	5094.278567	24.670554
151.459904	5098.981366	24.675571
151.193243	5121.615243	24.680589
150.843314	5117.118613	24.685607
151.161708	5114.202871	24.690624
151.039717	5121.212936	24.695642
151.266858	5130.244979	24.700659
151.346052	5145.150418	24.705677
151.569726	5142.267079	24.710695
151.722263	5166.228987	24.715712
151.897900	5178.491545	24.720730
152.135219	5172.106048	24.725747
152.376403	5179.485410	24.730765
152.528531	5191.805223	24.735783
152.856148	5194.541933	24.740800
152.969988	5196.198774	24.745818
153.544325	5207.746413	24.750835
153.473290	5185.376546	24.755853
153.776093	5198.735160	24.760871
153.970642	5183.574661	24.765888
153.761592	5190.040090	24.770906
154.163299	5194.578307	24.775923
154.508988	5205.505512	24.780941
154.466109	5216.508836	24.785959
154.565486	5205.741422	24.790976
154.414652	5209.846948	24.795994
154.885633	5216.122153	24.801011
154.598839	5211.610707	24.806029
154.944672	5203.925591	24.811047
155.181445	5205.731972	24.816064
155.147516	5210.534747	24.821082
155.244883	5196.680688	24.826099
155.757741	5209.415018	24.831117
155.455806	5233.972643	24.836135
155.895252	5230.394853	24.841152
155.679263	5248.595708	24.846170
155.685309	5250.469561	24.851187
156.062128	5241.216327	24.856205
155.926232	5264.384193	24.861223
155.981329	5269.200328	24.866240
155.933403	5270.681575	24.871258
156.379898	5290.764049	24.876275
156.319303	5294.269910	24.881293
156.519410	5324.655724	24.886311
156.762773	5327.519177	24.891328
156.965688	5341.387105	24.896346
157.070964	5363.382258	24.901363
157.894414	5351.948610	24.906381
157.932354	5363.139767	24.911399
158.365158	5368.411004	24.916416
158.482069	5376.459306	24.921434
158.463586	5379.931725	24.926451
158.661173	5377.347513	24.931469
158.785666	5381.266798	24.936487
159.182261	5371.498189	24.941504
159.059634	5383.141351	24.946522
159.058142	5385.397185	24.951539
159.621022	5393.497121	24.956557
159.255890	5404.643219	24.961575
159.632891	5388.997922	24.966592
160.029643	5397.392610	24.971610
160.036982	5402.212469	24.976627
160.253758	5418.388800	24.981645
160.260126	5432.038764	24.986663
160.587133	5422.240308	24.991680
160.714291	5429.482209	24.996698
160.754198	5422.977818	25.001715
160.753592	5443.514907	25.006733
160.690667	5451.776009	25.011751
160.871508	5441.454871	25.016768
160.737537	5465.377981	25.021786
161.379790	5479.551254	25.026803
161.554021	5479.247472	25.031821
161.449907	5493.497268	25.036839
162.191913	5501.257171	25.041856
162.079802	5501.867563	25.046874
161.884718	5498.191836	25.051891
162.306776	5511.179278	25.056909
162.273876	5519.325492	25.061927
162.828849	5524.709477	25.066944
163.130352	5532.712701	25.071962
163.461877	5518.530713	25.076979
163.705432	5512.539003	25.081997
163.730907	5525.448864	25.087015
163.800414	5521.929198	25.092032
163.929831	5533.112193	25.097050
163.829811	5542.383886	25.102067
164.022854	5552.829047	25.107085
164.214214	5547.428595	25.112103
164.381128	5553.310295	25.117120
164.418705	5560.149587	25.122138
164.597056	5567.100179	25.127155
165.020106	5566.334264	25.132173
164.902633	5579.971854	25.137191
164.867374	5572.067236	25.142208
165.303940	5581.485486	25.147226
165.158045	5598.938450	25.152243
165.747793	5616.655708	25.157261
165.568166	5609.176096	25.162279
165.733270	5611.671314	25.167296
165.621687	5640.912458	25.172314
165.965940	5644.251585	25.177331
166.698260	5650.780334	25.182349
166.359369	5674.876487	25.187367
166.810794	5674.054121	25.192384
166.846088	5673.314617	25.197402
166.691336	5669.844043	25.202419
167.214944	5698.248456	25.207437
167.193212	5687.018530	25.212455
167.947473	5693.431300	25.217472
168.064952	5704.311869	25.222490
168.253253	5717.045676	25.227507
168.504833	5716.078943	25.232525
168.625479	5712.350466	25.237543
168.725329	5710.693584	25.242560
169.026833	5703.997887	25.247578
168.680686	5715.774498	25.252595
169.120870	5705.012965	25.257613
169.222102	5735.605777	25.262631
169.294961	5728.236901	25.267648
169.351796	5730.429993	25.272666
169.424127	5738.580007	25.277683
170.235485	5745.584751	25.282701
170.051129	5759.977406	25.287719
170.009447	5771.615049	25.292736
170.230554	5767.763548	25.297754
170.652950	5754.524286	25.302771
171.082367	5772.350687	25.307789
171.104288	5786.968527	25.312807
171.128864	5792.657453	25.317824
171.076634	5798.198135	25.322842
171.008709	5787.043941	25.327859
171.285314	5789.870718	25.332877
171.412945	5816.038116	25.337895
171.921861	5813.992664	25.342912
171.948085	5817.185067	25.347930
171.740691	5819.872662	25.352947
171.985228	5827.134596	25.357965
171.977993	5841.772086	25.362983
172.315158	5849.742264	25.368000
172.514565	5853.018779	25.373018
172.725710	5880.213027	25.378035
173.106687	5869.639401	25.383053
172.834421	5879.850580	25.388071
172.871854	5900.403483	25.393088
173.574860	5903.571402	25.398106
173.756723	5897.861580	25.403123
173.996188	5914.040346	25.408141
174.116690	5931.388294	25.413159
174.348995	5924.073361	25.418176
174.686180	5920.984536	25.423194
174.276972	5932.613240	25.428211
174.655344	5945.620621	25.433229
174.988659	5959.435301	25.438247
175.135788	5960.972060	25.443264
175.305351	5961.635906	25.448282
175.841661	5978.209562	25.453299
176.097190	5976.189538	25.458317
176.053575	5991.979244	25.463335
176.430677	5975.026552	25.468352
176.388093	5990.480158	25.473370
176.191471	5986.647206	25.478387
177.027885	5992.551373	25.483405
176.707550	6001.985927	25.488423
176.689282	6003.902302	25.493440
176.876139	6011.484283	25.498458
177.148507	6017.070854	25.503475
177.344201	6027.209891	25.508493
177.235039	6044.185483	25.513511
177.412399	6053.892398	25.518528
177.704744	6063.557385	25.523546
177.902541	6081.550898	25.528563
178.238692	6078.815451	25.533581
178.263859	6092.197899	25.538599
178.361399	6097.732125	25.543616
178.628211	6097.021778	25.548634
179.019369	6121.340569	25.553651
179.376688	6118.429445	25.558669
179.372040	6116.882012	25.563687
179.516244	6120.404197	25.568704
179.964871	6136.157281	25.573722
179.415978	6154.560228	25.578739
180.346802	6136.433375	25.583757
180.679102	6140.768964	25.588775
180.419853	6159.444371	25.593792
180.892273	6158.778344	25.598810
180.864467	6171.465963	25.603827
181.150630	6158.616256	25.608845
181.096572	6165.693872	25.613863
181.170776	6174.697443	25.618880
181.680794	6193.118871	25.623898
181.490822	6200.052955	25.628915
181.718816	6191.929019	25.633933
181.802920	6194.518285	25.638951
181.912076	6216.802829	25.643968
182.523697	6216.216885	25.648986
182.261042	6215.515413	25.654003
182.807200	6217.212809	25.659021
182.691768	6244.909024	25.664039
183.011478	6259.742631	25.669056
183.070096	6258.016735	25.674074
183.152354	6269.537454	25.679092
183.568116	6281.132470	25.684109
183.540926	6287.978491	25.689127
183.445264	6288.172461	25.694144
183.987781	6302.754237	25.699162
184.124564	6316.302407	25.704180
184.276029	6323.552676	25.709197
184.595452	6336.373114	25.714215
184.643711	6331.944012	25.719232
184.923077	6340.446075	25.724250
184.999963	6363.788658	25.729268
185.279335	6382.095248	25.734285
185.547503	6380.579825	25.739303
185.948625	6395.967840	25.744320
186.009570	6395.623883	25.749338
186.254546	6394.902056	25.754356
186.411153	6398.044688	25.759373
186.682689	6412.283477	25.764391
186.966145	6430.541485	25.769408
187.607724	6425.082317	25.774426
187.034870	6439.260627	25.779444
187.132791	6439.320674	25.784461
187.605318	6427.489771	25.789479
187.615152	6448.160342	25.794496
187.778666	6448.199704	25.799514
187.992482	6456.668226	25.804532
188.585802	6461.773446	25.809549
188.600307	6471.687552	25.814567
188.253188	6489.766859	25.819584
188.635121	6476.586907	25.824602
188.626072	6490.293807	25.829620
188.740261	6507.415279	25.834637
189.295020	6512.069557	25.839655
189.421620	6530.015960	25.844672
189.685554	6536.154807	25.849690
189.679592	6551.317566	25.854708
189.921534	6547.842550	25.859725
190.252083	6558.548953	25.864743
190.323102	6571.159006	25.869760
190.875300	6567.437048	25.874778
190.692367	6580.859407	25.879796
190.836695	6594.027409	25.884813
191.325678	6586.724733	25.889831
191.149908	6597.878512	25.894848
191.391444	6602.384488	25.899866
191.756048	6611.793634	25.904884
192.151072	6616.822734	25.909901
191.880368	6620.926513	25.914919
191.959377	6627.566938	25.919936
192.312656	6643.097376	25.924954
192.620406	6641.740052	25.929972
192.888967	6655.598754	25.934989
193.174066	6659.122211	25.940007
193.178928	6676.286483	25.945024
193.424481	6683.299275	25.950042
193.252500	6681.348097	25.955060
193.698562	6686.339187	25.960077
193.644536	6708.081652	25.965095
193.866118	6720.745721	25.970112
194.560211	6726.551719	25.975130
194.602172	6740.256226	25.980148
194.342915	6741.730396	25.985165
195.102885	6743.413442	25.990183
195.013143	6767.747022	25.995200
195.340805	6774.259754	26.000218
195.517328	6777.913058	26.005236
195.753240	6786.044654	26.010253
196.046644	6791.716287	26.015271
195.816546	6802.982735	26.020288
196.273162	6807.943861	26.025306
196.408778	6823.281810	26.030324
196.521767	6818.924856	26.035341
196.778200	6816.822753	26.040359
197.142166	6837.036944	26.045376
197.152280	6848.697861	26.050394
197.317456	6857.279795	26.055412
197.610282	6867.511716	26.060429
197.816584	6875.120940	26.065447
197.417846	6886.726687	26.070464
198.150385	6891.969583	26.075482
198.450627	6898.328600	26.080500
198.656944	6910.824533	26.085517
199.022217	6916.798684	26.090535
199.293984	6935.635104	26.095552
199.343882	6927.503754	26.100570
199.472032	6949.250576	26.105588
199.505276	6949.176956	26.110605
200.269816	6947.661814	26.115623
200.013235	6974.507777	26.120640
200.107718	6963.843721	26.125658
200.664054	6973.544330	26.130676
200.742924	6987.764034	26.135693
201.033394	6991.763507	26.140711
200.907093	6988.059916	26.145728
201.691392	6987.290641	26.150746
201.556805	7005.955894	26.155764
201.802403	6996.975051	26.160781
201.976255	7005.914463	26.165799
202.318280	7017.683107	26.170816
202.474635	7000.381273	26.175834
202.174370	7012.437983	26.180852
202.315137	7023.661213	26.185869
202.906793	7020.346707	26.190887
203.057934	7031.801178	26.195904
203.035243	7044.095335	26.200922
203.167524	7052.229437	26.205940
203.432780	7067.448625	26.210957
203.878074	7056.481528	26.215975
203.609403	7082.004659	26.220992
203.970164	7093.610659	26.226010
204.173398	7091.162156	26.231028
204.264930	7115.645224	26.236045
204.447196	7111.841271	26.241063
204.333267	7129.873953	26.246080
204.914342	7143.832787	26.251098
204.949287	7165.719886	26.256116
205.050165	7182.177845	26.261133
205.818983	7180.364593	26.266151
205.796173	7205.107582	26.271168
206.362893	7205.246328	26.276186
206.421833	7220.223183	26.281204
206.570148	7221.245322	26.286221
206.948927	7231.326105	26.291239
207.045062	7231.661821	26.296256
207.445286	7236.245767	26.301274
207.465223	7239.159378	26.306292
207.696363	7263.144422	26.311309
208.200925	7255.642239	26.316327
208.357178	7259.361838	26.321344
208.085653	7265.885332	26.326362
208.452344	7277.113654	26.331380
208.863845	7292.834557	26.336397
208.930033	7290.698198	26.341415
209.160286	7302.535243	26.346432
209.479885	7312.730947	26.351450
209.733296	7323.834165	26.356468
209.431559	7336.868580	26.361485
210.110645	7329.958541	26.366503
210.161385	7346.320818	26.371520
210.263250	7345.340087	26.376538
210.650045	7349.427375	26.381556
210.641881	7371.608833	26.386573
210.797538	7375.009900	26.391591
211.151427	7384.788689	26.396608
211.431888	7401.534561	26.401626
211.739936	7409.610943	26.406644
211.549466	7418.458400	26.411661
212.194477	7420.251916	26.416679
211.975314	7439.446554	26.421696
212.266441	7451.077312	26.426714
212.387156	7453.439084	26.431732
212.593790	7464.263465	26.436749
212.928761	7453.634683	26.441767
212.978578	7483.667297	26.446784
213.417580	7487.190813	26.451802
213.840459	7495.512519	26.456820
213.513997	7496.918005	26.461837
213.898456	7508.241236	26.466855
213.952916	7525.104316	26.471872
213.950470	7522.672007	26.476890
214.748733	7537.672956	26.481908
214.604008	7561.863959	26.486925
214.811439	7557.989789	26.491943
215.103670	7566.731277	26.496960
215.471493	7586.090610	26.501978
215.821067	7588.929714	26.506996
215.657458	7614.737574	26.512013
216.291450	7607.491546	26.517031
216.371037	7621.868321	26.522048
216.289629	7637.236200	26.527066
216.786128	7645.682375	26.532084
217.005563	7645.711257	26.537101
217.007539	7664.799334	26.542119
217.218578	7673.868556	26.547136
217.430479	7684.085619	26.552154
217.857700	7693.212450	26.557172
217.891683	7704.294281	26.562189
218.286988	7727.424595	26.567207
218.407087	7740.543976	26.572224
218.673102	7743.620675	26.577242
218.898106	7741.350354	26.582260
219.034835	7751.359922	26.587277
219.339301	7763.663896	26.592295
219.356954	7792.127034	26.597312
219.731904	7798.253435	26.602330
220.291058	7798.905624	26.607348
220.059283	7822.465727	26.612365
220.635303	7808.607677	26.617383
220.995351	7818.912162	26.622400
220.964635	7832.319252	26.627418
221.277541	7836.749712	26.632436
221.218067	7854.463793	26.637453
221.406931	7861.559359	26.642471
221.556275	7870.863570	26.647488
221.974304	7882.895394	26.652506
222.216592	7904.754464	26.657524
222.154555	7927.578739	26.662541
222.318854	7924.041822	26.667559
222.655960	7932.302698	26.672576
223.010981	7941.643410	26.677594
223.405558	7957.312640	26.682612
223.358158	7966.548344	26.687629
223.439739	7969.320871	26.692647
223.843177	7997.334209	26.697664
223.916891	7997.302917	26.702682
224.777660	8018.311349	26.707700
224.753837	8033.542990	26.712717
225.166270	8023.392446	26.717735
225.425136	8028.732510	26.722752
225.345463	8035.329618	26.727770
225.751376	8042.422146	26.732788
225.659572	8052.674499	26.737805
225.841107	8058.614671	26.742823
225.779149	8067.819318	26.747840
226.103001	8082.678491	26.752858
226.312744	8086.371675	26.757876
226.654212	8116.263082	26.762893
226.778927	8113.811981	26.767911
227.070634	8123.388724	26.772928
227.300104	8149.958680	26.777946
227.496609	8147.944633	26.782964
228.092938	8164.720490	26.787981
228.207669	8182.305689	26.792999
228.068973	8180.161733	26.798016
228.320891	8203.401413	26.803034
228.657714	8201.071497	26.808052
228.721491	8229.598148	26.813069
229.086006	8245.440862	26.818087
229.478157	8247.635959	26.823104
229.865444	8273.152564	26.828122
229.921877	8267.405966	26.833140
230.223270	8285.632719	26.838157
230.647695	8295.379624	26.843175
230.626664	8301.471784	26.848192
230.658863	8318.945191	26.853210
231.138486	8317.458823	26.858228
231.382803	8332.590587	26.863245
231.290367	8352.383880	26.868263
231.619551	8353.051511	26.873280
231.943841	8378.313168	26.878298
232.532643	8388.118127	26.883316
232.649030	8394.612538	26.888333
232.776115	8398.395302	26.893351
232.847912	8413.547566	26.898368
233.298886	8421.121735	26.903386
233.729202	8420.730659	26.908404
233.923929	8448.422455	26.913421
233.873261	8433.152163	26.918439
234.504230	8444.118927	26.923456
234.183430	8467.543947	26.928474
234.671138	8467.327848	26.933492
234.934317	8479.661031	26.938509
235.105754	8493.557397	26.943527
235.382819	8497.122711	26.948544
235.243351	8515.772534	26.953562
235.694058	8521.309602	26.958580
235.904897	8529.502811	26.963597
236.224659	8561.642717	26.968615
236.534040	8565.335877	26.973632
236.432511	8575.586990	26.978650
236.600740	8588.210802	26.983668
237.000237	8603.853179	26.988685
237.230402	8634.308669	26.993703
237.364896	8629.326132	26.998720
237.545070	8647.169772	27.003738
238.102494	8662.833464	27.008756
238.000773	8659.873064	27.013773
238.310025	8683.402580	27.018791
238.710311	8686.812170	27.023808
238.826362	8684.006690	27.028826
239.298438	8712.409381	27.033844
239.315984	8718.954312	27.038861
239.548356	8717.847249	27.043879
239.926832	8738.356016	27.048896
240.307034	8745.205903	27.053914
240.302011	8747.902676	27.058932
240.915952	8762.628162	27.063949
240.928645	8777.754808	27.068967
241.057978	8779.371031	27.073984
241.375747	8799.825035	27.079002
241.421934	8808.382215	27.084020
241.541765	8819.486601	27.089037
242.053799	8833.997058	27.094055
242.145866	8841.763209	27.099072
242.412157	8871.495002	27.104090
242.980307	8863.575071	27.109108
243.099279	8871.074916	27.114125
243.518327	8884.125622	27.119143
243.848781	8876.778654	27.124160
243.823013	8893.726892	27.129178
243.962601	8910.490234	27.134196
244.257897	8923.280962	27.139213
244.264858	8928.682750	27.144231
244.944580	8935.812329	27.149248
244.725305	8960.006463	27.154266
244.950502	8968.558022	27.159284
245.404980	8981.934054	27.164301
245.372821	8999.973274	27.169319
245.876952	9010.527494	27.174336
245.844900	9028.406205	27.179354
246.474015	9037.362803	27.184372
246.709643	9054.659464	27.189389
246.763458	9068.843446	27.194407
247.555718	9076.071616	27.199424
247.500637	9099.387989	27.204442
248.006899	9105.497940	27.209460
247.986869	9097.797149	27.214477
247.983171	9111.986405	27.219495
248.619447	9122.381542	27.224512
248.554867	9130.634721	27.229530
249.041776	9155.029795	27.234548
248.844938	9168.535384	27.239565
249.167063	9178.738663	27.244583
249.794169	9183.400766	27.249600
249.490159	9208.331182	27.254618
249.711624	9222.550360	27.259636
250.462427	9234.937072	27.264653
250.389529	9255.791160	27.269671
250.840179	9249.223561	27.274688
251.260355	9256.921106	27.279706
251.472314	9273.274753	27.284724
251.468880	9282.156056	27.289741
251.619643	9295.501303	27.294759
251.852711	9299.509378	27.299776
252.085936	9310.644451	27.304794
252.462488	9335.351713	27.309812
252.977589	9346.510739	27.314829
252.909452	9345.422416	27.319847
253.245107	9375.642664	27.324864
253.282285	9376.991141	27.329882
253.637933	9379.375188	27.334900
254.288668	9415.772521	27.339917
253.997361	9420.213205	27.344935
254.612346	9416.275174	27.349952
254.453211	9449.965641	27.354970
255.277061	9458.494852	27.359988
255.499626	9468.608752	27.365005
255.246979	9466.016916	27.370023
255.779555	9491.217752	27.375040
255.588515	9509.424161	27.380058
255.944590	9539.401083	27.385076
256.345787	9535.376698	27.390093
256.536533	9563.020441	27.395111
257.121845	9580.740030	27.400128
257.069066	9596.880085	27.405146
257.398203	9609.991795	27.410164
257.937208	9621.783840	27.415181
257.829561	9643.733895	27.420199
258.416255	9650.776351	27.425216
258.711392	9656.495243	27.430234
259.094642	9672.312097	27.435252
259.157557	9687.445429	27.440269
259.741242	9692.920432	27.445287
260.098529	9706.349987	27.450304
260.125816	9720.233487	27.455322
260.100062	9712.610411	27.460340
260.576153	9732.597026	27.465357
260.634154	9751.495092	27.470375
260.709875	9763.184425	27.475392
261.011750	9777.111167	27.480410
261.129526	9803.634589	27.485428
261.489693	9815.160191	27.490445
261.489523	9837.507327	27.495463
262.137507	9852.358708	27.500480
262.493492	9870.225759	27.505498
262.552201	9875.778209	27.510516
263.049301	9892.179945	27.515533
262.954335	9919.459102	27.520551
263.163678	9922.623594	27.525568
263.715857	9946.404009	27.530586
264.201740	9967.532017	27.535604
264.609520	9974.439854	27.540621
264.374053	9988.750689	27.545639
264.936991	9991.328832	27.550656
265.520348	9996.112671	27.555674
265.742053	9998.964366	27.560692
265.907379	9998.863385	27.565709
265.931265	10004.401759	27.570727
266.304765	10027.660316	27.575744
266.921548	10032.132718	27.580762
266.790175	10029.876759	27.585780
267.055553	10051.255654	27.590797
266.973092	10053.446406	27.595815
267.582981	10062.233172	27.600832
267.529934	10089.822310	27.605850
267.856872	10090.349918	27.610868
268.277778	10112.983297	27.615885
268.667350	10122.948652	27.620903
268.601258	10133.478483	27.625920
268.930674	10149.895031	27.630938
268.891834	10168.233795	27.635956
269.334890	10183.088660	27.640973
269.141770	10208.100640	27.645991
269.854950	10217.517911	27.651008
270.170443	10246.444263	27.656026
270.196870	10255.497662	27.661044
270.769986	10281.971784	27.666061
271.155407	10301.920887	27.671079
271.339179	10310.706464	27.676096
271.452649	10330.267301	27.681114
271.613545	10350.391940	27.686132
272.294188	10357.574399	27.691149
272.372889	10378.261081	27.696167
273.123461	10376.470465	27.701184
273.304352	10398.218241	27.706202
273.148373	10420.958984	27.711220
273.749181	10409.178096	27.716237
274.060139	10437.625491	27.721255
274.149652	10446.841295	27.726272
274.437976	10466.620763	27.731290
274.573684	10480.724563	27.736308
275.306271	10497.610406	27.741325
275.394056	10509.445954	27.746343
275.470162	10515.655743	27.751360
275.982723	10520.982638	27.756378
276.031913	10545.878649	27.761396
276.480515	10553.596734	27.766413
276.747279	10561.858485	27.771431
277.144359	10576.446022	27.776448
277.507769	10590.492386	27.781466
277.589630	10602.714963	27.786484
278.080293	10613.000179	27.791501
278.116104	10629.933873	27.796519
277.991275	10645.979115	27.801536
278.532043	10656.459022	27.806554
278.533095	10670.819375	27.811572
279.078346	10691.695769	27.816589
279.181554	10705.947404	27.821607
279.382472	10718.234126	27.826624
279.618132	10734.350678	27.831642
279.955440	10748.674827	27.836660
280.327122	10747.745707	27.841677
280.178984	10777.007467	27.846695
280.750660	10792.230028	27.851712
281.314168	10811.238524	27.856730
281.460805	10825.981513	27.861748
281.672232	10829.717220	27.866765
281.771521	10854.820211	27.871783
282.046823	10872.258637	27.876800
282.625524	10882.987643	27.881818
282.554164	10896.578664	27.886836
282.963454	10898.832823	27.891853
283.252991	10932.763208	27.896871
283.580258	10938.991774	27.901888
284.002668	10959.427335	27.906906
284.114415	10991.437591	27.911924
284.443837	10999.314201	27.916941
284.599611	11012.494516	27.921959
284.865490	11033.173123	27.926976
285.456630	11055.765056	27.931994
285.594171	11070.793448	27.937012
285.911875	11079.243330	27.942029
286.310492	11103.822895	27.947047
286.213892	11133.556416	27.952064
286.849785	11144.822282	27.957082
286.738253	11175.081621	27.962100
287.048357	11187.686196	27.967117
287.704506	11205.096972	27.972135
287.865476	11225.142888	27.977152
288.012731	11242.643863	27.982170
288.412157	11261.097481	27.987188
289.153541	11266.002936	27.992205
289.282827	11293.544756	27.997223
289.497450	11299.822906	28.002240
290.015265	11312.008453	28.007258
289.903652	11332.565834	28.012276
290.538466	11339.356275	28.017293
290.443925	11362.282839	28.022311
290.460718	11368.753491	28.027328
291.150203	11386.016715	28.032346
291.481626	11403.167422	28.037364
291.880442	11412.739838	28.042381
292.071403	11442.598526	28.047399
292.059263	11451.166509	28.052416
292.818463	11462.258708	28.057434
292.977909	11491.990691	28.062452
293.146686	11511.268398	28.067469
293.626825	11525.312775	28.072487
294.221676	11542.345316	28.077504
294.235618	11545.769927	28.082522
294.422109	11565.219993	28.087540
294.969270	11568.575370	28.092557
295.568768	11571.210147	28.097575
295.696040	11580.943215	28.102592
295.939671	11592.395499	28.107610
296.313964	11596.175488	28.112628
296.539419	11605.703643	28.117645
296.722597	11608.079342	28.122663
296.568751	11630.004630	28.127680
297.176602	11629.816195	28.132698
296.938554	11660.228890	28.137716
297.624965	11657.647561	28.142733
297.896634	11676.961813	28.147751
297.622422	11699.551750	28.152768
298.456217	11705.712503	28.157786
298.572703	11726.881796	28.162804
298.871384	11750.699183	28.167821
299.399637	11763.086489	28.172839
299.392642	11779.818552	28.177856
299.978187	11793.803096	28.182874
300.070011	11810.596967	28.187892
300.272827	11832.337025	28.192909
300.628366	11859.639584	28.197927
300.454702	11880.891145	28.202944
301.308453	11888.766121	28.207962
301.528696	11919.710747	28.212980
301.706614	11932.522363	28.217997
302.121156	11952.694508	28.223015
302.104509	11976.685284	28.228032
302.968599	11986.100489	28.233050
302.996112	12015.621563	28.238068
303.406395	12023.836457	28.243085
303.767577	12038.919110	28.248103
304.036941	12056.833660	28.253120
304.571135	12076.215198	28.258138
304.800459	12103.232150	28.263156
305.266968	12099.933767	28.268173
305.311077	12131.321673	28.273191
305.633308	12136.672008	28.278208
306.085212	12157.962390	28.283226
306.147098	12185.745612	28.288244
306.662243	12193.482672	28.293261
307.100518	12210.872672	28.298279
307.083397	12238.036573	28.303296
307.630728	12244.898828	28.308314
307.794720	12266.546136	28.313332
307.926039	12277.534175	28.318349
308.504803	12304.309066	28.323367
308.507601	12322.165669	28.328384
308.800664	12344.708662	28.333402
309.270150	12359.022727	28.338420
309.501879	12378.726757	28.343437
310.323743	12399.397734	28.348455
310.117994	12416.447093	28.353472
310.487489	12423.875144	28.358490
310.804218	12438.809245	28.363508
311.543177	12463.546349	28.368525
311.628942	12474.801131	28.373543
311.947584	12484.384255	28.378560
312.598171	12493.227565	28.383578
312.286756	12519.341690	28.388596
312.832512	12507.751154	28.393613
313.179903	12533.946653	28.398631
313.066071	12529.598816	28.403648
313.642127	12559.283427	28.408666
313.739546	12567.616562	28.413684
314.147211	12595.813743	28.418701
314.197094	12601.269039	28.423719
314.503294	12635.853875	28.428736
314.967746	12649.232195	28.433754
314.875922	12663.107280	28.438772
315.141270	12704.335858	28.443789
316.045203	12708.773947	28.448807
316.174873	12733.325046	28.453824
316.756877	12749.108160	28.458842
317.373270	12756.996634	28.463860
317.718609	12775.269269	28.468877
317.973961	12786.219415	28.473895
318.304388	12798.846503	28.478912
319.321802	12810.657904	28.483930
318.743164	12820.445628	28.488948
319.049830	12833.466141	28.493965
319.863157	12837.695766	28.498983
320.237547	12853.713572	28.504000
320.509369	12860.591486	28.509018
320.647321	12881.197973	28.514036
321.079410	12878.562333	28.519053
320.828275	12885.762087	28.524071
321.344757	12909.983823	28.529088
321.343652	12917.793692	28.534106
321.795916	12944.763631	28.539124
321.646243	12971.376175	28.544141
322.301976	12986.004922	28.549159
322.375675	13015.553050	28.554176
322.669806	13027.932274	28.559194
323.131444	13061.582634	28.564212
323.116851	13072.635629	28.569229
323.773130	13106.096666	28.574247
323.698778	13127.875475	28.579264
324.207207	13149.580924	28.584282
324.771631	13173.635856	28.589300
324.900837	13216.097898	28.594317
325.715220	13228.607095	28.599335
325.953358	13252.155103	28.604352
326.146189	13278.038848	28.609370
326.634518	13294.600767	28.614388
326.880803	13310.719561	28.619405
327.359007	13331.575673	28.624423
327.392557	13359.331124	28.629440
327.829647	13363.888480	28.634458
328.143248	13390.996230	28.639476
328.972429	13414.273986	28.644493
329.506840	13411.381683	28.649511
329.347398	13429.450809	28.654528
329.734977	13437.808827	28.659546
330.217242	13446.387505	28.664564
330.287641	13474.803397	28.669581
330.728169	13479.079828	28.674599
330.676356	13498.631751	28.679616
331.183889	13508.228716	28.684634
331.468673	13523.748109	28.689652
331.777047	13536.685520	28.694669
331.994687	13555.694751	28.699687
332.090599	13576.157948	28.704704
332.491363	13586.656319	28.709722
332.866207	13626.606215	28.714740
333.329036	13635.175700	28.719757
333.894913	13660.776908	28.724775
333.881146	13676.718709	28.729792
334.233192	13698.408935	28.734810
334.657788	13717.019369	28.739828
334.800048	13734.808180	28.744845
335.271330	13753.916169	28.749863
335.517815	13783.266461	28.754880
335.766129	13813.531373	28.759898
336.609652	13837.261284	28.764916
336.878747	13849.552484	28.769933
337.061626	13870.891691	28.774951
336.964541	13895.172831	28.779968
337.599001	13912.678166	28.784986
337.971009	13933.614805	28.790004
338.536119	13946.898734	28.795021
339.384941	13965.084309	28.800039
339.561312	13987.692225	28.805056
339.884700	13985.279761	28.810074
340.156017	13999.127909	28.815092
340.501976	14012.872078	28.820109
340.849685	14038.704888	28.825127
340.896332	14041.712383	28.830144
341.184323	14061.003266	28.835162
341.582243	14083.223571	28.840180
341.594320	14107.906520	28.845197
342.084531	14122.935467	28.850215
342.391802	14153.548834	28.855232
342.694483	14178.837652	28.860250
342.939416	14206.878778	28.865268
343.237146	14237.213431	28.870285
343.548983	14248.631573	28.875303
343.777025	14270.335390	28.880320
344.098059	14298.525238	28.885338
344.948151	14333.265189	28.890356
344.868216	14357.346259	28.895373
345.547479	14378.264560	28.900391
345.887079	14396.754667	28.905408
346.230119	14418.630866	28.910426
346.670934	14437.293520	28.915444
346.540558	14466.563097	28.920461
347.247357	14471.567634	28.925479
347.682246	14505.356224	28.930496
347.903539	14518.874232	28.935514
348.399343	14541.433052	28.940532
348.193550	14560.916902	28.945549
348.709400	14569.073760	28.950567
349.331515	14598.004448	28.955584
349.349250	14617.800883	28.960602
349.751393	14639.803769	28.965620
350.209708	14656.534711	28.970637
350.527450	14681.141146	28.975655
350.881944	14710.248318	28.980672
351.281164	14719.492058	28.985690
352.195035	14744.877381	28.990708
352.368494	14763.327891	28.995725
352.670587	14772.349212	29.000743
353.190225	14793.216573	29.005760
353.224798	14810.839104	29.010778
353.593441	14834.488417	29.015796
353.787831	14856.848654	29.020813
354.351458	14872.488038	29.025831
354.432528	14900.728258	29.030848
354.450764	14922.224371	29.035866
355.307547	14930.965222	29.040884
355.844962	14965.449041	29.045901
355.896336	14990.781316	29.050919
356.453780	14999.835785	29.055936
356.554234	15017.133370	29.060954
357.133881	15033.085938	29.065972
357.212222	15066.691775	29.070989
357.715031	15077.465793	29.076007
357.903425	15110.149516	29.081024
358.373267	15127.887161	29.086042
358.940304	15143.303993	29.091060
359.126773	15177.679292	29.096077
359.268680	15200.960676	29.101095
359.576251	15229.956659	29.106112
360.235477	15251.875183	29.111130
360.337943	15274.727436	29.116148
360.904428	15292.223450	29.121165
361.297909	15322.493710	29.126183
362.143569	15345.699976	29.131200
362.094436	15355.035325	29.136218
362.840589	15385.299207	29.141236
362.923600	15403.239627	29.146253
363.212088	15423.085375	29.151271
363.720076	15445.701847	29.156288
364.160470	15461.410676	29.161306
364.523976	15484.294170	29.166324
364.842834	15506.035556	29.171341
365.359428	15519.309408	29.176359
365.369613	15533.353480	29.181376
365.205346	15562.354525	29.186394
366.021059	15568.327693	29.191412
366.288232	15603.282004	29.196429
366.458198	15634.426704	29.201447
367.072402	15643.539922	29.206464
367.404526	15678.359375	29.211482
368.187010	15695.390127	29.216500
368.210666	15720.963311	29.221517
368.271465	15734.482974	29.226535
368.672256	15762.311902	29.231552
368.905109	15785.397533	29.236570
369.633460	15802.157165	29.241588
370.061703	15825.252758	29.246605
370.358433	15844.919823	29.251623
370.480312	15873.997981	29.256640
371.121646	15894.857103	29.261658
371.308397	15923.921083	29.266676
371.513499	15947.293807	29.271693
372.174702	15960.168695	29.276711
372.465675	15987.338788	29.281728
372.619552	16025.675361	29.286746
373.327168	16041.944164	29.291764
373.448561	16072.992001	29.296781
373.800381	16098.881272	29.301799
374.279262	16117.753856	29.306816
374.814032	16142.857099	29.311834
375.268492	16156.969509	29.316852
375.536740	16198.926527	29.321869
375.752561	16201.153881	29.326887
376.216561	16227.843956	29.331904
376.587710	16269.912407	29.336922
376.626182	16286.555369	29.341940
377.032001	16312.949992	29.346957
377.297359	16349.462823	29.351975
377.929341	16369.803598	29.356992
378.511268	16393.506559	29.362010
378.889850	16421.867008	29.367028
379.225844	16442.272361	29.372045
379.530719	16477.889184	29.377063
380.301658	16485.498539	29.382080
380.495047	16519.269140	29.387098
381.127903	16530.938879	29.392116
381.346018	16553.047552	29.397133
381.614482	16583.641259	29.402151
382.198833	16600.011192	29.407168
382.855132	16630.229659	29.412186
383.492989	16629.425107	29.417204
383.429176	16660.990676	29.422221
383.750557	16674.070982	29.427239
384.414835	16681.154989	29.432256
384.432981	16708.941795	29.437274
384.913701	16725.090809	29.442292
385.368982	16763.814011	29.447309
385.613990	16780.816277	29.452327
386.316892	16805.566007	29.457344
386.267262	16823.014425	29.462362
386.687779	16841.931449	29.467380
387.069246	16870.872308	29.472397
387.343077	16894.582621	29.477415
387.921773	16896.217290	29.482432
387.940727	16936.295518	29.487450
388.572496	16949.666324	29.492468
389.153722	16967.135240	29.497485
388.805917	16989.144575	29.502503
389.211776	17011.854034	29.507520
389.293150	17045.818420	29.512538
390.103594	17062.464794	29.517556
390.349547	17101.394224	29.522573
390.514611	17131.419735	29.527591
390.930767	17159.423235	29.532608
391.254382	17191.262961	29.537626
391.664811	17216.890376	29.542644
392.213118	17246.169294	29.547661
392.626950	17286.302036	29.552679
393.113358	17312.311164	29.557696
393.628517	17350.048444	29.562714
394.075373	17357.355975	29.567732
394.573202	17393.098091	29.572749
394.724816	17425.081836	29.577767
395.649758	17451.372475	29.582784
395.747327	17481.694040	29.587802
396.091357	17509.652980	29.592820
396.619922	17519.725669	29.597837
396.912846	17551.400572	29.602855
397.527999	17575.270916	29.607872
398.193481	17596.612622	29.612890
398.577144	17602.622377	29.617908
399.291429	17637.267865	29.622925
399.347905	17652.446951	29.627943
400.202309	17673.850585	29.632960
400.342698	17695.821128	29.637978
400.644636	17699.107145	29.642996
401.107424	17717.943518	29.648013
401.362008	17738.916867	29.653031
402.104447	17748.131087	29.658048
402.049467	17777.363249	29.663066
402.555248	17799.877451	29.668084
402.871709	17810.656324	29.673101
402.978062	17843.651817	29.678119
403.308652	17863.744584	29.683136
404.024436	17897.387137	29.688154
404.686664	17917.567284	29.693172
404.890019	17943.673754	29.698189
405.146768	17951.547850	29.703207
405.885831	17975.739408	29.708224
405.824505	18015.815507	29.713242
406.568042	18032.005317	29.718260
407.083432	18047.361463	29.723277
407.174289	18075.580257	29.728295
407.674344	18101.885969	29.733312
407.780360	18128.026958	29.738330
407.950771	18165.963871	29.743348
408.541851	18189.526616	29.748365
409.167269	18221.278060	29.753383
409.405090	18248.013974	29.758400
409.276305	18263.730044	29.763418
410.217490	18284.004213	29.768436
410.269926	18316.372319	29.773453
409.958080	18344.027832	29.778471
410.943118	18370.366964	29.783488
411.252153	18402.259735	29.788506
411.619937	18443.446486	29.793524
411.909539	18471.607958	29.798541
412.573502	18506.426992	29.803559
413.082305	18529.341570	29.808576
413.361911	18575.111511	29.813594
413.898807	18598.477218	29.818612
414.677830	18639.621017	29.823629
414.869707	18668.397619	29.828647
415.614127	18690.705614	29.833664
415.816681	18719.282186	29.838682
416.093283	18756.096154	29.843700
416.575264	18780.348043	29.848717
416.884077	18808.913756	29.853735
417.530528	18837.125337	29.858752
418.030399	18860.087497	29.863770
418.316484	18893.600680	29.868788
419.134833	18924.357868	29.873805
419.212474	18957.870541	29.878823
419.751834	18973.854108	29.883840
420.468486	19001.409525	29.888858
420.304275	19036.377050	29.893876
421.047902	19067.307452	29.898893
421.322341	19082.838452	29.903911
421.717591	19108.266498	29.908928
422.331969	19144.556305	29.913946
422.980430	19172.223679	29.918964
423.574723	19194.712622	29.923981
423.372263	19236.012011	29.928999
423.837061	19249.473434	29.934016
424.458746	19282.082393	29.939034
424.648536	19315.273235	29.944052
425.213919	19338.565046	29.949069
425.733981	19375.222791	29.954087
425.707119	19391.338733	29.959104
426.314890	19420.463867	29.964122
426.518293	19446.553367	29.969140
427.164106	19481.952308	29.974157
427.583963	19526.658178	29.979175
428.147423	19552.882233	29.984192
428.719559	19584.400067	29.989210
428.761882	19614.901929	29.994228
429.325618	19646.861800	29.999245
429.733354	19684.133866	30.004263
430.265227	19713.987820	30.009280
430.477327	19746.574813	30.014298
430.731682	19790.110101	30.019316
431.526363	19806.462537	30.024333
431.336298	19848.627369	30.029351
431.883644	19877.171610	30.034368
432.739650	19908.772837	30.039386
433.233550	19938.416328	30.044404
433.480565	19950.065295	30.049421
434.184855	19985.409606	30.054439
434.380523	20007.260822	30.059456
435.060759	20028.668308	30.064474
434.961448	20068.517925	30.069492
436.085839	20080.663480	30.074509
436.138988	20118.120249	30.079527
436.487749	20152.603004	30.084544
436.721718	20179.111335	30.089562
437.075874	20214.026867	30.094580
437.866552	20253.711544	30.099597
437.845917	20281.284322	30.104615
438.846078	20314.537967	30.109632
439.185816	20352.872167	30.114650
439.303466	20378.639847	30.119668
439.990381	20405.944990	30.124685
440.202758	20451.659099	30.129703
440.636698	20480.013042	30.134720
441.461475	20498.795128	30.139738
441.565719	20543.648296	30.144756
442.140862	20570.704576	30.149773
442.696883	20604.613913	30.154791
443.430895	20644.170014	30.159808
443.972678	20671.390070	30.164826
444.160153	20706.909306	30.169844
444.728590	20731.852123	30.174861
444.899764	20757.656000	30.179879
445.614268	20802.205969	30.184896
446.038038	20822.643471	30.189914
446.206624	20874.495684	30.194932
446.720551	20894.772836	30.199949
447.321417	20920.995992	30.204967
447.714332	20951.317030	30.209984
448.118191	20979.807792	30.215002
448.472191	21019.927418	30.220020
449.473452	21043.040516	30.225037
449.718287	21074.020509	30.230055
449.867203	21113.891118	30.235072
450.756728	21137.915592	30.240090
451.292899	21163.852963	30.245108
451.797619	21189.506369	30.250125
451.815486	21209.139621	30.255143
452.349505	21243.262541	30.260160
452.665022	21281.475688	30.265178
453.004449	21317.880902	30.270196
453.654696	21350.460500	30.275213
453.800453	21382.833087	30.280231
454.001433	21417.583155	30.285248
454.699076	21452.113210	30.290266
455.487003	21487.531471	30.295284
455.990546	21518.682580	30.300301
456.311496	21554.825101	30.305319
456.513845	21572.755117	30.310336
457.110484	21607.912735	30.315354
457.017339	21645.776049	30.320372
458.117472	21659.324603	30.325389
458.308378	21697.055373	30.330407
458.902440	21731.213499	30.335424
459.266071	21753.101429	30.340442
459.764200	21781.414821	30.345460
460.500924	21810.870003	30.350477
460.619644	21846.112952	30.355495
461.092495	21873.397271	30.360512
461.842377	21902.596938	30.365530
462.215003	21932.995561	30.370548
462.529863	21957.492050	30.375565
463.073501	21995.550098	30.380583
462.952215	22017.039172	30.385600
463.868654	22054.515822	30.390618
464.168633	22095.419793	30.395636
464.839071	22130.686536	30.400653
465.114924	22177.414665	30.405671
465.596094	22198.268530	30.410688
466.090094	22232.876062	30.415706
466.310218	22271.845552	30.420724
466.761545	22310.875967	30.425741
467.230023	22342.363502	30.430759
467.756256	22388.382932	30.435776
468.289274	22426.586265	30.440794
468.655686	22462.742531	30.445812
469.342643	22502.523466	30.450829
469.748469	22546.583343	30.455847
470.358792	22572.170207	30.460864
471.129251	22608.387669	30.465882
471.490217	22654.038832	30.470900
472.026046	22679.400673	30.475917
472.383378	22714.579199	30.480935
472.987752	22759.033341	30.485952
473.572624	22778.946033	30.490970
474.151175	22819.504281	30.495988
473.814163	22844.495853	30.501005
474.504476	22880.463650	30.506023
475.275877	22925.129509	30.511040
476.097279	22949.368852	30.516058
475.798067	22989.616853	30.521076
476.411017	23030.938081	30.526093
477.135901	23058.809670	30.531111
477.545950	23098.970169	30.536128
478.095756	23136.390449	30.541146
478.422861	23166.986156	30.546164
479.300456	23215.540135	30.551181
479.639722	23249.846111	30.556199
479.770984	23280.871771	30.561216
480.498703	23319.232130	30.566234
480.651924	23353.873566	30.571252
481.196719	23397.678180	30.576269
481.964632	23431.707548	30.581287
482.004478	23459.853584	30.586304
482.913319	23493.071430	30.591322
483.304636	23530.905405	30.596340
483.781493	23554.710657	30.601357
484.158793	23580.589898	30.606375
484.479834	23619.168569	30.611392
485.128360	23642.310195	30.616410
485.448195	23686.409001	30.621428
485.957418	23718.976588	30.626445
486.529205	23756.347576	30.631463
487.094000	23790.791294	30.636480
487.559628	23824.256083	30.641498
487.974513	23868.208717	30.646516
488.323879	23899.544261	30.651533
488.910820	23937.333080	30.656551
489.229099	23976.428186	30.661568
489.836723	24006.248311	30.666586
489.857045	24047.995839	30.671604
490.174110	24084.015592	30.676621
491.257094	24138.737799	30.681639
491.532316	24180.370244	30.686656
491.941761	24226.438044	30.691674
492.439444	24259.317346	30.696692
493.090311	24297.418999	30.701709
493.737868	24349.148035	30.706727
494.260346	24386.277094	30.711744
495.032074	24412.190962	30.716762
495.605473	24464.398492	30.721780
496.008883	24492.579028	30.726797
496.622000	24523.964376	30.731815
496.908497	24555.910657	30.736832
497.783924	24584.584879	30.741850
498.352615	24614.432830	30.746868
498.696178	24644.768831	30.751885
498.939288	24685.894928	30.756903
499.339774	24723.442779	30.761920
500.037737	24752.956110	30.766938
500.345555	24800.567527	30.771956
500.715989	24839.386268	30.776973
501.367655	24878.802283	30.781991
501.955125	24920.802834	30.787008
502.743686	24952.025598	30.792026
503.070967	24997.213100	30.797044
503.566304	25021.417767	30.802061
503.988345	25077.977512	30.807079
504.208374	25112.280512	30.812096
505.456501	25144.474172	30.817114
505.585600	25178.823307	30.822132
506.106091	25207.972682	30.827149
506.544600	25249.431459	30.832167
506.837042	25279.784690	30.837184
507.334072	25333.420406	30.842202
507.843693	25361.833698	30.847220
508.563800	25420.585894	30.852237
509.258757	25437.515458	30.857255
509.216390	25484.483617	30.862272
509.911031	25506.815563	30.867290
510.210049	25554.273086	30.872308
510.643096	25590.504641	30.877325
511.261261	25618.039317	30.882343
511.517077	25659.631453	30.887360
512.013860	25708.752361	30.892378
512.021369	25742.870786	30.897396
512.755547	25795.098030	30.902413
513.168183	25841.362202	30.907431
513.626489	25888.530660	30.912448
514.124692	25936.742977	30.917466
514.991995	25986.517850	30.922484
515.032088	26038.907649	30.927501
515.915900	26089.506571	30.932519
516.732204	26129.251583	30.937536
517.313569	26176.925941	30.942554
517.367719	26215.399008	30.947572
518.241887	26269.566256	30.952589
518.983942	26313.605080	30.957607
519.636862	26361.107884	30.962624
519.829693	26381.320733	30.967642
520.582147	26440.366153	30.972660
520.942182	26485.196567	30.977677
521.343793	26529.759729	30.982695
521.662632	26573.057624	30.987712
522.417676	26615.897779	30.992730
523.067752	26668.966084	30.997748
523.637686	26713.098021	31.002765
524.159114	26747.091821	31.007783
524.740202	26800.159731	31.012800
525.580954	26837.389544	31.017818
526.217592	26871.487366	31.022836
526.411427	26913.565307	31.027853
527.017530	26941.046676	31.032871
527.695351	26984.093916	31.037888
528.292518	27025.123940	31.042906
528.833401	27066.569543	31.047924
529.354655	27102.092472	31.052941
529.978368	27136.122801	31.057959
530.048528	27183.559359	31.062976
530.903324	27214.324587	31.067994
531.460071	27256.351137	31.073012
531.727781	27308.280247	31.078029
532.403568	27339.689515	31.083047
532.856361	27379.331663	31.088064
533.255254	27419.463855	31.093082
534.012586	27462.633645	31.098100
534.315586	27507.841548	31.103117
535.137820	27542.477686	31.108135
535.314313	27585.023389	31.113152
535.891377	27629.508083	31.118170
536.452264	27664.066357	31.123188
536.896685	27720.107948	31.128205
537.560891	27750.656391	31.133223
538.131134	27790.730704	31.138240
538.474180	27833.092178	31.143258
538.983325	27877.182633	31.148276
539.140081	27922.580439	31.153293
540.204699	27960.267246	31.158311
540.251473	28001.327546	31.163328
540.904850	28054.460564	31.168346
541.617764	28088.737120	31.173364
541.928140	28125.260233	31.178381
542.729144	28171.225810	31.183399
543.100229	28219.098867	31.188416
543.518366	28263.337234	31.193434
544.022139	28304.528788	31.198452
544.330146	28361.871468	31.203469
545.225784	28402.250806	31.208487
545.892543	28462.210747	31.213504
546.121517	28500.304516	31.218522
547.102564	28544.151453	31.223540
547.321853	28595.691384	31.228557
547.925053	28638.798268	31.233575
548.405914	28696.280059	31.238592
549.226073	28741.580809	31.243610
549.722244	28777.103547	31.248628
549.859313	28832.672424	31.253645
550.757609	28880.156192	31.258663
551.593055	28931.844884	31.263680
551.997254	28975.102543	31.268698
552.772795	29019.153687	31.273716
553.192307	29067.511617	31.278733
553.494876	29108.527681	31.283751
554.261725	29157.150450	31.288768
554.862150	29200.821841	31.293786
555.484510	29242.018957	31.298804
555.860173	29295.318470	31.303821
556.728123	29344.559186	31.308839
557.312603	29386.574260	31.313856
557.433774	29423.187164	31.318874
558.191387	29469.847264	31.323892
558.690479	29512.071667	31.328909
559.186416	29568.922233	31.333927
559.926602	29618.628523	31.338944
560.681949	29667.516250	31.343962
561.320922	29705.731929	31.348980
561.856076	29762.231810	31.353997
562.471986	29793.571085	31.359015
563.267615	29831.891335	31.364032
563.353132	29889.317397	31.369050
564.292068	29927.047729	31.374068
564.836670	29970.482667	31.379085
565.068061	30007.432334	31.384103
565.412441	30049.120176	31.389120
566.191256	30096.949601	31.394138
566.673381	30137.865599	31.399156
566.926057	30184.400148	31.404173
568.124967	30221.981024	31.409191
568.537371	30261.504289	31.414208
569.015143	30306.567669	31.419226
569.805809	30338.937616	31.424244
570.032315	30368.537147	31.429261
570.883349	30416.491542	31.434279
571.343043	30459.430703	31.439296
571.836365	30492.024815	31.444314
572.496870	30541.997195	31.449332
572.674581	30580.327790	31.454349
573.317849	30613.360020	31.459367
573.725439	30661.434613	31.464384
574.133305	30709.094823	31.469402
574.582376	30752.153068	31.474420
575.334910	30812.821947	31.479437
575.861682	30862.430492	31.484455
576.001878	30917.005232	31.489472
576.829291	30973.741721	31.494490
577.247494	31026.672918	31.499508
577.937935	31087.932675	31.504525
578.666024	31145.066971	31.509543
579.210788	31199.428503	31.514560
579.328603	31257.159976	31.519578
580.401589	31312.219469	31.524596
580.945457	31353.185419	31.529613
581.628652	31415.613823	31.534631
581.939169	31479.151460	31.539648
582.977390	31527.856303	31.544666
583.466515	31584.106623	31.549684
583.857213	31647.985181	31.554701
584.529355	31696.422581	31.559719
585.272703	31748.954446	31.564736
585.858408	31797.933894	31.569754
586.574515	31857.298003	31.574772
587.199521	31916.880150	31.579789
587.798694	31965.156595	31.584807
588.374629	32015.421187	31.589824
588.784112	32073.012939	31.594842
589.227796	32118.165546	31.599860
590.098569	32178.251684	31.604877
590.718500	32223.401731	31.609895
591.401918	32279.423327	31.614912
592.049149	32337.364295	31.619930
592.823944	32379.235408	31.624948
593.148477	32427.736629	31.629965
593.899715	32469.624333	31.634983
594.538381	32527.026718	31.640000
595.049241	32583.644244	31.645018
595.516281	32618.054622	31.650036
595.947927	32677.791684	31.655053
596.628696	32730.487969	31.660071
597.643595	32783.949246	31.665088
597.652591	32840.456858	31.670106
598.660308	32882.662564	31.675124
599.195288	32944.603398	31.680141
599.855427	32986.741780	31.685159
600.516406	33031.305896	31.690176
601.297366	33066.378085	31.695194
602.009188	33104.066817	31.700212
602.308087	33145.911639	31.705229
602.922146	33176.669776	31.710247
603.711405	33210.265622	31.715264
604.042984	33256.752188	31.720282
604.750981	33302.721841	31.725300
605.071230	33344.226455	31.730317
605.658867	33386.732056	31.735335
606.418702	33435.400206	31.740352
606.861899	33487.540929	31.745370
607.524477	33527.278122	31.750388
607.826892	33597.046645	31.755405
607.976929	33638.008501	31.760423
608.963440	33694.008714	31.765440
609.473462	33751.989118	31.770458
609.644219	33810.791391	31.775476
610.346380	33868.112675	31.780493
610.747286	33936.355298	31.785511
611.720620	33991.433342	31.790528
612.118981	34059.845542	31.795546
612.904424	34120.236086	31.800564
613.509471	34178.267479	31.805581
614.218695	34254.462051	31.810599
615.055783	34299.394049	31.815616
615.364315	34368.540626	31.820634
615.959951	34422.387666	31.825652
617.017125	34485.887349	31.830669
617.692896	34547.565862	31.835687
618.600146	34594.539880	31.840704
618.995440	34657.790940	31.845722
619.844062	34704.988990	31.850740
620.474576	34765.103896	31.855757
620.985582	34821.669163	31.860775
621.813174	34871.211935	31.865792
622.391567	34925.384934	31.870810
623.153448	34974.802911	31.875828
623.477998	35025.868632	31.880845
623.853274	35077.624772	31.885863
624.857093	35127.288428	31.890880
624.967678	35194.827361	31.895898
626.048589	35254.482948	31.900916
626.468801	35304.635742	31.905933
627.134338	35358.512522	31.910951
628.209413	35415.961063	31.915968
628.309700	35469.567209	31.920986
629.217517	35529.341201	31.926004
629.806090	35584.145296	31.931021
630.534862	35634.560508	31.936039
631.028821	35683.785212	31.941056
631.536428	35751.723503	31.946074
632.254351	35793.973335	31.951092
632.715636	35849.629363	31.956109
633.303210	35909.666959	31.961127
634.166013	35952.762757	31.966144
634.541585	36009.044635	31.971162
635.144414	36066.909562	31.976180
635.608839	36117.825507	31.981197
636.161900	36177.242119	31.986215
637.105750	36220.670957	31.991232
637.549536	36279.481041	31.996250
638.251661	36329.718148	32.001268
638.770310	36378.510583	32.006285
639.310071	36444.561066	32.011303
640.214396	36492.515201	32.016320
640.405388	36558.895984	32.021338
640.964841	36619.743061	32.026356
641.616176	36676.793614	32.031373
642.221067	36746.360056	32.036391
643.093755	36795.500930	32.041408
643.493020	36871.328002	32.046426
644.210243	36920.899174	32.051444
644.878653	36986.576583	32.056461
645.396846	37058.264418	32.061479
646.385975	37119.372821	32.066496
646.990008	37186.582663	32.071514
647.669867	37248.477046	32.076532
648.244569	37323.204567	32.081549
649.393850	37386.688028	32.086567
650.321418	37438.934270	32.091584
650.717448	37498.771572	32.096602
651.205695	37549.388517	32.101620
652.019055	37603.567474	32.106637
652.419310	37668.092011	32.111655
653.567234	37727.534498	32.116672
653.981128	37787.407821	32.121690
654.694181	37845.854158	32.126708
655.431171	37907.436002	32.131725
656.384423	37960.234760	32.136743
657.130341	38010.766345	32.141760
657.108904	38082.637491	32.146778
657.987165	38134.576838	32.151796
658.872036	38190.051786	32.156813
659.134299	38248.227578	32.161831
659.868859	38296.295893	32.166848
660.582704	38372.062298	32.171866
661.327786	38437.444632	32.176884
661.744846	38499.949922	32.181901
662.111118	38558.146486	32.186919
663.069267	38614.684907	32.191936
663.523175	38687.857841	32.196954
664.258159	38757.485993	32.201972
665.363486	38802.833618	32.206989
665.506872	38867.537664	32.212007
666.558661	38931.225381	32.217024
667.008122	38992.686680	32.222042
667.506687	39056.092413	32.227060
668.096758	39121.224564	32.232077
668.960200	39185.884559	32.237095
669.565194	39249.349756	32.242112
670.716284	39301.774327	32.247130
671.220615	39357.698437	32.252148
671.816178	39407.149660	32.257165
672.393156	39461.367493	32.262183
672.883753	39514.716244	32.267200
673.525874	39561.361680	32.272218
674.166337	39627.763393	32.277236
675.136887	39682.895320	32.282253
675.423541	39744.807856	32.287271
676.036415	39800.077529	32.292288
676.328956	39870.313669	32.297306
677.157515	39939.890786	32.302324
677.955833	40001.115707	32.307341
678.509979	40081.352439	32.312359
679.459278	40144.107041	32.317376
680.386395	40205.999706	32.322394
680.829100	40279.010987	32.327412
681.721703	40326.716152	32.332429
682.291188	40399.748766	32.337447
682.903495	40467.012913	32.342464
683.509459	40526.652462	32.347482
684.364970	40598.569677	32.352500
685.350527	40666.798599	32.357517
685.941690	40737.799728	32.362535
686.303962	40800.941944	32.367552
686.948957	40849.496958	32.372570
687.596580	40929.790612	32.377588
688.311597	40991.718327	32.382605
688.834458	41073.866502	32.387623
689.726623	41139.565417	32.392640
690.223677	41212.795970	32.397658
690.577450	41291.297793	32.402676
691.729012	41356.852166	32.407693
692.297776	41422.430190	32.412711
693.264292	41506.058403	32.417728
694.018327	41571.730508	32.422746
694.811549	41633.454129	32.427764
695.695715	41708.877130	32.432781
696.334441	41785.481295	32.437799
697.139907	41837.296912	32.442816
697.852386	41905.619996	32.447834
698.375550	41972.595168	32.452852
699.629639	42034.404567	32.457869
699.795291	42099.932662	32.462887
700.409213	42166.118236	32.467904
701.186920	42228.013638	32.472922
702.045159	42300.913780	32.477940
702.870287	42361.177742	32.482957
703.242628	42436.240696	32.487975
704.109043	42501.702918	32.492992
705.394832	42546.359978	32.498010
705.704951	42609.788422	32.503028
706.746287	42671.359578	32.508045
707.591208	42736.170046	32.513063
707.815512	42779.362827	32.518080
708.574819	42833.488222	32.523098
709.046803	42891.860961	32.528116
710.015065	42936.096454	32.533133
710.101257	43005.031450	32.538151
710.525482	43061.873095	32.543168
711.698022	43126.718044	32.548186
712.120959	43190.446093	32.553204
713.383926	43253.794613	32.558221
713.827467	43308.485922	32.563239
714.205479	43371.316507	32.568256
715.111041	43439.170193	32.573274
716.113158	43501.160628	32.578292
716.800822	43567.835088	32.583309
716.862467	43644.410077	32.588327
718.058125	43708.808773	32.593344
718.600847	43769.690416	32.598362
718.826823	43847.337869	32.603380
719.662168	43924.320867	32.608397
720.534662	44001.689443	32.613415
721.078270	44072.331821	32.618432
721.700988	44149.993179	32.623450
722.434205	44225.302985	32.628468
723.326290	44298.887561	32.633485
724.087460	44390.988123	32.638503
724.349783	44460.392981	32.643520
725.676296	44543.445537	32.648538
725.906523	44623.297650	32.653556
727.471686	44688.480285	32.658573
728.428649	44756.214240	32.663591
729.038905	44825.713435	32.668608
729.935756	44897.078969	32.673626
730.851115	44969.978144	32.678644
731.620365	45020.342212	32.683661
731.970815	45106.543423	32.688679
732.798547	45170.561331	32.693696
733.847463	45227.156066	32.698714
734.359936	45308.108378	32.703732
734.862162	45361.471868	32.708749
735.553181	45441.705504	32.713767
736.474985	45506.135557	32.718784
737.406062	45581.164219	32.723802
738.116423	45638.274776	32.728820
738.798847	45699.528984	32.733837
739.641673	45774.010982	32.738855
739.935954	45835.706026	32.743872
741.070365	45889.752881	32.748890
742.054718	45953.108319	32.753908
743.105908	46019.929934	32.758925
744.422066	46072.159655	32.763943
744.336777	46136.077225	32.768960
745.282995	46196.881064	32.773978
745.875268	46261.726020	32.778996
746.852925	46314.338456	32.784013
747.555862	46371.692367	32.789031
748.149151	46448.567340	32.794048
748.984435	46488.987299	32.799066
749.162424	46544.570271	32.804084
749.513239	46598.267671	32.809101
750.740834	46646.790432	32.814119
751.326507	46716.745925	32.819136
751.760850	46769.572416	32.824154
752.529813	46840.284805	32.829172
753.359724	46907.372197	32.834189
754.263423	46972.327962	32.839207
754.207973	47040.317143	32.844224
755.178828	47114.424809	32.849242
756.058766	47194.456591	32.854260
756.783012	47271.355343	32.859277
757.251091	47342.098720	32.864295
757.831769	47425.832722	32.869312
758.622786	47498.923163	32.874330
759.024524	47585.172597	32.879348
759.814005	47676.620274	32.884365
760.494814	47763.917823	32.889383
761.198764	47855.591437	32.894400
762.578449	47933.849581	32.899418
763.159412	48028.282332	32.904436
763.779813	48112.256224	32.909453
764.703553	48197.488479	32.914471
765.532320	48287.383877	32.919488
766.375099	48373.311394	32.924506
766.967060	48457.272524	32.929524
767.921964	48534.755351	32.934541
768.892321	48619.644615	32.939559
769.797815	48706.702822	32.944576
770.356358	48790.800223	32.949594
770.958330	48873.177779	32.954612
771.796380	48966.328279	32.959629
772.918488	49038.227021	32.964647
773.798828	49130.172625	32.969664
774.549742	49208.728991	32.974682
775.144477	49284.852521	32.979700
776.356781	49354.463164	32.984717
777.505250	49428.385061	32.989735
777.873891	49513.125113	32.994752
778.782939	49586.274834	32.999770
779.379867	49667.735501	33.004788
780.529668	49738.449389	33.009805
781.329272	49820.938735	33.014823
781.894654	49894.756592	33.019840
782.644091	49974.395762	33.024858
783.264503	50058.508262	33.029876
783.942805	50131.324606	33.034893
784.766206	50207.371520	33.039911
785.380374	50289.870469	33.044928
786.206408	50365.639951	33.049946
786.989811	50454.247160	33.054964
787.541427	50546.498557	33.059981
788.568577	50619.526445	33.064999
789.369382	50700.277777	33.070016
789.922472	50766.896900	33.075034
790.627613	50842.242706	33.080052
791.680201	50908.811259	33.085069
792.746069	50978.691411	33.090087
793.220324	51064.946231	33.095104
794.613860	51138.785750	33.100122
795.183222	51201.740129	33.105140
795.846804	51271.079558	33.110157
796.806436	51350.372695	33.115175
797.705909	51413.594010	33.120192
798.227320	51481.432653	33.125210
799.170325	51553.900255	33.130228
799.774119	51611.555195	33.135245
800.594539	51700.910623	33.140263
801.264527	51775.379177	33.145280
802.304464	51852.626255	33.150298
802.966092	51927.450225	33.155316
803.970476	52016.676961	33.160333
804.607191	52082.422970	33.165351
805.035879	52158.288546	33.170368
806.206437	52237.362689	33.175386
806.752841	52315.463508	33.180404
807.871714	52396.446440	33.185421
808.491249	52483.322461	33.190439
808.852718	52585.865145	33.195456
809.569296	52658.843490	33.200474
810.427961	52751.372973	33.205492
811.263808	52840.886263	33.210509
812.153072	52937.612481	33.215527
813.101982	53023.485567	33.220544
813.905840	53113.418744	33.225562
814.579176	53206.967909	33.230580
815.291839	53308.120630	33.235597
816.324574	53394.613362	33.240615
817.069446	53490.125174	33.245632
817.936526	53567.520754	33.250650
818.832236	53665.035724	33.255668
819.502911	53760.810111	33.260685
820.533774	53848.343694	33.265703
821.750462	53937.880719	33.270720
822.895938	54018.216531	33.275738
823.665571	54107.711923	33.280756
824.283618	54187.725275	33.285773
825.381710	54256.057028	33.290791
825.941347	54334.587416	33.295808
826.808888	54415.695168	33.300826
827.514109	54508.510575	33.305844
828.202098	54590.455696	33.310861
829.340514	54674.182267	33.315879
830.104487	54761.223006	33.320896
831.072359	54843.853844	33.325914
831.640458	54925.014685	33.330932
832.228677	55006.516731	33.335949
833.155859	55077.467016	33.340967
833.927667	55168.700155	33.345984
834.559086	55247.027365	33.351002
835.701967	55324.695886	33.356020
836.643868	55406.058210	33.361037
837.370486	55474.557835	33.366055
838.282198	55567.775064	33.371072
839.196470	55634.929174	33.376090
839.693766	55706.294383	33.381108
839.956493	55794.003784	33.386125
841.414136	55869.534920	33.391143
841.979574	55961.584533	33.396160
843.045973	56047.352235	33.401178
843.552856	56139.973933	33.406196
844.780180	56217.443426	33.411213
845.522565	56307.133897	33.416231
846.141040	56406.399632	33.421248
847.322473	56481.923598	33.426266
847.788539	56568.600539	33.431284
848.901097	56669.588366	33.436301
849.554480	56745.585725	33.441319
850.332956	56845.990038	33.446336
850.848632	56937.051798	33.451354
851.794551	57035.318656	33.456372
852.840780	57127.733244	33.461389
853.735901	57230.236119	33.466407
854.493867	57332.164760	33.471424
855.490570	57428.749388	33.476442
856.276136	57525.870058	33.481460
856.829597	57623.230213	33.486477
858.029193	57725.649513	33.491495
858.780337	57819.459356	33.496512
859.799796	57924.781181	33.501530
860.683778	58013.412519	33.506548
861.751491	58109.771592	33.511565
862.471305	58204.226075	33.516583
863.219805	58307.017143	33.521600
864.076722	58407.714243	33.526618
865.117920	58503.596575	33.531636
865.713108	58610.558850	33.536653
866.643520	58709.686340	33.541671
867.604952	58795.736134	33.546688
868.620623	58900.745265	33.551706
869.376716	59003.191716	33.556724
870.348964	59097.553761	33.561741
871.447346	59187.040592	33.566759
872.194807	59273.609692	33.571776
872.957451	59384.047868	33.576794
874.296157	59480.667730	33.581812
874.929754	59577.605514	33.586829
876.268407	59663.855042	33.591847
877.119565	59754.921501	33.596864
877.641101	59849.621138	33.601882
878.800988	59943.452471	33.606900
879.268171	60040.349687	33.611917
880.316671	60129.069155	33.616935
880.843404	60214.067554	33.621952
881.887515	60305.140730	33.626970
882.800302	60387.994678	33.631988
883.327067	60469.262300	33.637005
884.148979	60557.230532	33.642023
884.834334	60646.133382	33.647040
885.811345	60739.019042	33.652058
886.874663	60833.741656	33.657076
887.457517	60924.411329	33.662093
888.358237	61028.696143	33.667111
889.152660	61131.849148	33.672128
890.244563	61221.542548	33.677146
891.299810	61323.003758	33.682164
891.517413	61433.022965	33.687181
892.559202	61531.456262	33.692199
893.853903	61633.402038	33.697216
894.559987	61742.173889	33.702234
895.551858	61836.717178	33.707252
896.261119	61933.907746	33.712269
897.116070	62045.347911	33.717287
898.292713	62146.146950	33.722304
899.375976	62250.908411	33.727322
900.197550	62361.762129	33.732340
900.786006	62469.950638	33.737357
901.703512	62558.206706	33.742375
902.737313	62662.709927	33.747392
903.381442	62782.167474	33.752410
904.895575	62878.104385	33.757428
905.629726	62997.498447	33.762445
906.819034	63094.037589	33.767463
907.629607	63213.619794	33.772480
908.169011	63296.880716	33.777498
909.596372	63392.379327	33.782516
909.819779	63518.340925	33.787533
911.251459	63616.577820	33.792551
911.974715	63717.381605	33.797568
912.817978	63829.434151	33.802586
913.990508	63939.164437	33.807604
914.699880	64054.861730	33.812621
916.148838	64142.427995	33.817639
916.915585	64256.339469	33.822656
917.601268	64361.074827	33.827674
919.073254	64458.217013	33.832692
919.542339	64569.142896	33.837709
920.504721	64667.968345	33.842727
921.882068	64775.308672	33.847744
922.796863	64873.470097	33.852762
923.778657	64960.195469	33.857780
924.558569	65075.827739	33.862797
925.257811	65173.658667	33.867815
926.370049	65278.072231	33.872832
927.152467	65385.614871	33.877850
928.872151	65468.526969	33.882868
929.281423	65560.329727	33.887885
930.688055	65652.444808	33.892903
931.718940	65736.449858	33.897920
932.565726	65825.487176	33.902938
933.468377	65889.733429	33.907956
933.940623	65986.707697	33.912973
934.869479	66077.277507	33.917991
935.489773	66159.707449	33.923008
935.967173	66247.652731	33.928026
937.244180	66343.177440	33.933044
937.746214	66446.251120	33.938061
938.628906	66546.965525	33.943079
939.821877	66647.700574	33.948096
940.562419	66751.578065	33.953114
941.668619	66845.610117	33.958132
942.631903	66962.462678	33.963149
943.288701	67060.600556	33.968167
944.438985	67175.488549	33.973184
944.667257	67281.250703	33.978202
946.046753	67387.600944	33.983220
946.791846	67511.790768	33.988237
947.912082	67614.876572	33.993255
948.890150	67724.833222	33.998272
949.313465	67851.619034	34.003290
950.354706	67968.920113	34.008308
951.465267	68086.716248	34.013325
952.470593	68211.567207	34.018343
953.499513	68326.598218	34.023360
954.146269	68446.832980	34.028378
955.230748	68573.347754	34.033396
956.235255	68680.361749	34.038413
957.345786	68808.775437	34.043431
958.397241	68932.922465	34.048448
959.359065	69042.939714	34.053466
960.447899	69164.163597	34.058484
961.438425	69276.382411	34.063501
962.739335	69399.658814	34.068519
963.685330	69514.583696	34.073536
964.394092	69633.520808	34.078554
965.926640	69748.366387	34.083572
966.500290	69867.162157	34.088589
967.424067	69978.770174	34.093607
968.932450	70081.535653	34.098624
969.627833	70196.725541	34.103642
970.503363	70304.950411	34.108660
971.305033	70426.354174	34.113677
972.376889	70537.057307	34.118695
973.362953	70638.291409	34.123712
974.160288	70768.145132	34.128730
975.335367	70882.327665	34.133748
976.520796	71004.299441	34.138765
977.525407	71115.130260	34.143783
978.675181	71226.355610	34.148800
979.444696	71347.808093	34.153818
980.679414	71456.260169	34.158836
981.315915	71566.962545	34.163853
982.443066	71671.787269	34.168871
983.508861	71767.138462	34.173888
984.295871	71881.881364	34.178906
985.442324	71971.698444	34.183924
986.347199	72078.841641	34.188941
987.116073	72176.655697	34.193959
987.942394	72272.609773	34.198976
988.972313	72377.952878	34.203994
989.897852	72484.071379	34.209012
990.952820	72595.926118	34.214029
991.852426	72705.563082	34.219047
993.182907	72810.456282	34.224064
993.904054	72936.210288	34.229082
994.512801	73027.969090	34.234100
995.938518	73141.069590	34.239117
996.616532	73255.047937	34.244135
997.930308	73376.072436	34.249152
998.634761	73498.155074	34.254170
999.551653	73606.378827	34.259188
1000.330212	73731.623215	34.264205
1001.305226	73853.652353	34.269223
1002.671941	73976.643616	34.274240
1003.218612	74103.886135	34.279258
1004.225351	74227.884073	34.284276
1005.374991	74347.108032	34.289293
1006.196105	74488.799209	34.294311
1007.646329	74599.547026	34.299328
1008.595787	74733.844957	34.304346
1009.923900	74841.371741	34.309364
1010.969391	74965.387045	34.314381
1011.850449	75079.899611	34.319399
1013.415989	75203.075332	34.324416
1014.072855	75335.054043	34.329434
1015.299031	75455.751185	34.334452
1016.386203	75561.133602	34.339469
1017.508278	75686.493563	34.344487
1018.376874	75797.119330	34.349504
1019.280000	75918.407806	34.354522
1020.294516	76038.238400	34.359540
1021.335299	76155.942095	34.364557
1022.465747	76283.503708	34.369575
1023.564952	76410.881503	34.374592
1024.372418	76529.616702	34.379610
1025.291369	76632.554097	34.384628
1026.477745	76766.189596	34.389645
1027.089102	76891.297003	34.394663
1028.231023	77015.758306	34.399680
1029.152332	77144.186536	34.404698
1030.644308	77263.708286	34.409716
1031.574372	77390.013131	34.414733
1032.440397	77522.598552	34.419751
1033.709797	77637.980282	34.424768
1034.552294	77776.600574	34.429786
1035.540226	77885.044608	34.434804
1036.443290	78014.037423	34.439821
1037.602548	78143.856192	34.444839
1038.639879	78263.317091	34.449856
1039.727203	78373.113121	34.454874
1040.520074	78468.438478	34.459892
1041.573498	78616.656993	34.464909
1042.671869	78725.808471	34.469927
1043.931706	78834.233267	34.474944
1044.539997	78951.162357	34.479962
1045.472317	79068.659998	34.484980
1046.677562	79200.563982	34.489997
1047.223390	79329.413338	34.495015
1048.595186	79447.348907	34.500032
1049.496893	79560.644611	34.505050
1050.533120	79696.137274	34.510068
1051.667500	79842.246938	34.515085
1052.792618	79954.858231	34.520103
1053.893544	80072.644527	34.525120
1054.835205	80212.536053	34.530138
1055.821908	80355.208942	34.535156
1057.374412	80480.473067	34.540173
1058.196337	80606.062751	34.545191
1059.360356	80738.254964	34.550208
1060.062736	80889.371263	34.555226
1061.299654	81009.947896	34.560244
1062.308367	81129.853545	34.565261
1063.162728	81277.990152	34.570279
1064.588582	81401.990460	34.575296
1065.787768	81548.310495	34.580314
1066.731288	81685.531415	34.585332
1068.059442	81817.432591	34.590349
1068.642521	81945.584333	34.595367
1069.927873	82090.491106	34.600384
1070.709752	82224.397181	34.605402
1072.094040	82368.278695	34.610420
1073.283897	82508.468648	34.615437
1074.302236	82639.267438	34.620455
1075.332740	82769.559371	34.625472
1076.531759	82907.651721	34.630490
1077.501841	83054.170500	34.635508
1078.655137	83189.926577	34.640525
1079.714880	83321.064431	34.645543
1080.685993	83459.266211	34.650560
1081.339806	83611.908293	34.655578
1082.454776	83741.554318	34.660596
1083.987581	83910.774327	34.665613
1084.857134	84047.257547	34.670631
1085.907401	84193.455423	34.675648
1087.141799	84332.461927	34.680666
1088.039359	84471.636721	34.685684
1089.552768	84621.557282	34.690701
1090.398960	84770.642990	34.695719
1091.405562	84907.716935	34.700736
1092.160006	85061.175428	34.705754
1093.725454	85203.365800	34.710772
1095.097452	85339.714250	34.715789
1096.037739	85492.077802	34.720807
1097.199291	85611.276678	34.725824
1098.116622	85737.292957	34.730842
1099.160059	85868.076215	34.735860
1100.486271	85996.671898	34.740877
1101.259666	86137.571887	34.745895
1102.533347	86263.016146	34.750912
1103.710079	86398.846050	34.755930
1104.146269	86535.477465	34.760948
1105.406533	86663.999150	34.765965
1106.147642	86818.654849	34.770983
1107.392839	86953.358230	34.776000
1108.770619	87090.450464	34.781018
1109.508824	87250.775218	34.786036
1110.801507	87384.013125	34.791053
1111.954949	87536.104471	34.796071
1113.014319	87670.734430	34.801088
1114.369281	87829.523735	34.806106
1115.308087	87982.518671	34.811124
1116.475268	88116.950907	34.816141
1117.526180	88279.902083	34.821159
1118.536798	88431.017060	34.826176
1119.883690	88580.505068	34.831194
1120.718296	88732.042204	34.836212
1122.000001	88888.277292	34.841229
1123.229108	89038.343682	34.846247
1124.682675	89185.694180	34.851264
1125.471958	89340.461544	34.856282
1126.671227	89509.222561	34.861300
1128.048336	89639.020871	34.866317
1128.862457	89801.913681	34.871335
1130.057063	89954.932507	34.876352
1131.508008	90104.528337	34.881370
1132.785583	90269.052093	34.886388
1133.871732	90416.532627	34.891405
1135.025051	90571.010561	34.896423
1136.021566	90721.479732	34.901440
1137.100639	90877.255440	34.906458
1138.244725	91030.941255	34.911476
1139.529691	91175.726491	34.916493
1140.533307	91335.887531	34.921511
1141.739839	91492.026812	34.926528
1143.064668	91639.502952	34.931546
1143.892277	91805.608721	34.936564
1145.003857	91956.118684	34.941581
1146.126284	92114.312255	34.946599
1147.613034	92258.775309	34.951616
1148.990830	92416.943100	34.956634
1149.951304	92581.414503	34.961652
1151.365924	92720.908230	34.966669
1152.783135	92867.625285	34.971687
1153.766144	93013.450992	34.976704
1155.009910	93165.295383	34.981722
1156.268224	93310.566964	34.986740
1157.380746	93453.029122	34.991757
1158.420568	93599.975498	34.996775
1159.324134	93742.017344	35.001792
1160.791277	93873.173656	35.006810
1161.391778	94022.020618	35.011828
1162.566804	94158.854384	35.016845
1163.333440	94301.984204	35.021863
1164.073786	94447.870584	35.026880
1165.622479	94587.202948	35.031898
1166.545095	94747.439568	35.036916
1167.422984	94902.522986	35.041933
1168.474183	95061.419422	35.046951
1169.944810	95222.698231	35.051968
1171.072106	95381.913767	35.056986
1171.736454	95560.819440	35.062004
1173.059402	95717.836606	35.067021
1174.309971	95887.498601	35.072039
1175.482190	96047.325304	35.077056
1176.763981	96226.587229	35.082074
1177.896498	96402.717770	35.087092
1178.803095	96568.833926	35.092109
1180.201962	96741.369671	35.097127
1180.969683	96907.763437	35.102144
1182.318880	97084.510093	35.107162
1183.364958	97278.569948	35.112180
1184.826255	97442.523082	35.117197
1186.260427	97624.112514	35.122215
1187.142868	97805.911322	35.127232
1188.773958	97977.255563	35.132250
1190.140882	98147.061542	35.137268
1191.250630	98311.526016	35.142285
1192.542871	98483.256915	35.147303
1193.719522	98655.810937	35.152320
1195.589616	98834.854470	35.157338
1196.207655	99013.060936	35.162356
1197.173403	99171.999869	35.167373
1198.687117	99348.908793	35.172391
1200.078211	99531.108651	35.177408
1201.498509	99696.906604	35.182426
1202.718222	99870.506844	35.187444
1203.994687	100035.419065	35.192461
1204.976461	100201.087924	35.197479
1206.116101	100376.121917	35.202496
1207.297135	100547.810058	35.207514
1208.579724	100730.106269	35.212532
1209.923113	100885.839873	35.217549
1211.233612	101062.370386	35.222567
1212.441372	101240.633221	35.227584
1213.691716	101406.331304	35.232602
1214.875976	101579.431219	35.237620
1215.913020	101741.261740	35.242637
1216.949638	101919.829078	35.247655
1218.188897	102093.740301	35.252672
1219.489011	102266.978777	35.257690
1220.358245	102452.492623	35.262708
1221.648397	102626.640177	35.267725
1223.055305	102786.533580	35.272743
1223.876962	102973.065199	35.277760
1225.302341	103126.035645	35.282778
1226.338872	103290.642163	35.287796
1227.868039	103456.456038	35.292813
1228.926758	103623.345660	35.297831
1230.087179	103783.949476	35.302848
1231.308722	103948.429952	35.307866
1232.320710	104118.766527	35.312884
1233.441223	104291.036076	35.317901
1234.782744	104473.529368	35.322919
1235.789965	104649.280939	35.327936
1237.628097	104821.478247	35.332954
1238.543349	105004.271218	35.337972
1239.876040	105164.983616	35.342989
1241.154220	105354.505364	35.348007
1242.161370	105540.964545	35.353024
1243.887210	105703.478598	35.358042
1245.067338	105888.254996	35.363060
1246.298421	106076.245876	35.368077
1247.870281	106245.793639	35.373095
1248.961543	106419.317352	35.378112
1250.344129	106596.143803	35.383130
1251.532398	106775.489582	35.388148
1252.509927	106947.592298	35.393165
1253.842977	107137.068873	35.398183
1254.933756	107316.358256	35.403200
1256.514150	107496.653364	35.408218
1257.452722	107693.829531	35.413236
1258.584724	107883.698372	35.418253
1260.484563	108050.143605	35.423271
1261.659259	108248.356362	35.428288
1262.660036	108431.756869	35.433306
1264.356068	108607.719204	35.438324
1265.469667	108789.699443	35.443341
1266.768693	108967.240158	35.448359
1267.998309	109150.381885	35.453376
1269.502138	109332.513031	35.458394
1270.574942	109526.891614	35.463412
1271.656967	109702.984821	35.468429
1273.299489	109884.749944	35.473447
1274.443964	110065.855050	35.478464
1275.755000	110260.613031	35.483482
1277.077374	110441.306544	35.488500
1278.384518	110623.446957	35.493517
1279.917122	110801.774103	35.498535
1281.040486	110992.694014	35.503552
1282.678200	111173.279506	35.508570
1283.733332	111348.224167	35.513588
1285.121798	111529.136734	35.518605
1286.695696	111706.894207	35.523623
1287.249662	111894.512495	35.528640
1288.660827	112075.741962	35.533658
1289.758565	112256.744058	35.538676
1291.259516	112436.233808	35.543693
1292.691956	112623.040672	35.548711
1293.423049	112803.421394	35.553728
1295.074881	112962.875099	35.558746
1296.025758	113150.560081	35.563764
1297.070635	113318.955871	35.568781
1298.796119	113492.492443	35.573799
1299.647149	113676.209162	35.578816
1300.979480	113854.602827	35.583834
1302.816318	114037.083011	35.588852
1303.638908	114213.819390	35.593869
1305.051887	114388.886871	35.598887
1306.051732	114577.992837	35.603904
1307.387227	114771.503643	35.608922
1308.734047	114962.728763	35.613940
1309.810095	115144.090785	35.618957
1311.510306	115337.636607	35.623975
1312.874146	115535.941183	35.628992
1313.961467	115721.939734	35.634010
1315.229466	115922.560683	35.639028
1316.298527	116111.508879	35.644045
1317.874460	116316.515684	35.649063
1318.772398	116520.346700	35.654080
1320.587349	116703.609411	35.659098
1321.601341	116907.380766	35.664116
1322.868506	117114.962892	35.669133
1324.319441	117312.704032	35.674151
1325.326316	117519.267163	35.679168
1326.936363	117724.754732	35.684186
1328.412532	117933.848814	35.689204
1329.643342	118142.166838	35.694221
1331.308081	118325.528380	35.699239
1332.777584	118565.228904	35.704256
1334.285447	118748.073878	35.709274
1335.878384	118947.489266	35.714292
1337.168335	119150.493782	35.719309
1338.624668	119340.942882	35.724327
1339.620988	119555.647698	35.729344
1341.061284	119751.256466	35.734362
1342.542835	119950.608645	35.739380
1344.076074	120144.711276	35.744397
1345.204122	120347.440631	35.749415
1346.423818	120553.683956	35.754432
1347.823006	120741.144679	35.759450
1349.564018	120951.069565	35.764468
1350.678889	121158.372800	35.769485
1352.344847	121358.903230	35.774503
1353.765162	121547.265555	35.779520
1354.576471	121746.617657	35.784538
1356.094867	121942.401408	35.789556
1357.357479	122145.078971	35.794573
1359.046773	122346.917718	35.799591
1359.971521	122541.584428	35.804608
1361.704056	122752.246966	35.809626
1363.249753	122955.088402	35.814644
1363.916976	123171.053013	35.819661
1365.501343	123359.921490	35.824679
1367.184239	123543.772757	35.829696
1368.316386	123723.925793	35.834714
1369.664388	123918.763327	35.839732
1370.960463	124096.347018	35.844749
1372.596947	124281.300015	35.849767
1373.465192	124484.982734	35.854784
1374.979569	124673.605659	35.859802
1376.301363	124844.502536	35.864820
1377.295811	125050.791397	35.869837
1378.915374	125245.418108	35.874855
1380.352685	125446.902411	35.879872
1381.584037	125639.149037	35.884890
1383.018416	125847.603404	35.889908
1383.871241	126054.961124	35.894925
1385.282958	126249.501445	35.899943
1386.810581	126469.675280	35.904960
1388.887375	126687.470898	35.909978
1390.195704	126874.672588	35.914996
1391.242269	127080.816651	35.920013
1392.616250	127297.373448	35.925031
1394.071236	127509.485495	35.930048
1395.353021	127696.747719	35.935066
1396.786459	127925.460857	35.940084
1398.015901	128141.920638	35.945101
1399.955240	128345.360821	35.950119
1400.796610	128560.986159	35.955136
1402.188344	128791.068600	35.960154
1404.008409	129003.184857	35.965172
1405.127423	129229.792562	35.970189
1406.821792	129444.795201	35.975207
1408.456143	129662.216046	35.980224
1409.657275	129888.322024	35.985242
1410.863698	130103.952059	35.990260
1412.228121	130326.057707	35.995277
1413.622067	130548.046416	36.000295
1414.833609	130779.516885	36.005312
1416.173110	130995.487398	36.010330
1417.836187	131226.560425	36.015348
1419.604761	131452.652259	36.020365
1421.038069	131673.351380	36.025383
1422.909909	131896.643130	36.030400
1424.629658	132122.507394	36.035418
1425.476655	132333.612671	36.040436
1427.052326	132551.153982	36.045453
1428.855963	132762.110453	36.050471
1430.478062	132992.989095	36.055488
1431.673778	133181.201440	36.060506
1433.835791	133408.564106	36.065524
1434.804706	133627.679815	36.070541
1436.323819	133827.666343	36.075559
1437.695333	134017.807509	36.080576
1439.085550	134241.574364	36.085594
1440.383661	134452.547665	36.090612
1441.757542	134657.758004	36.095629
1444.039317	134853.221136	36.100647
1445.134621	135065.561593	36.105664
1446.592728	135246.067315	36.110682
1448.285394	135422.431500	36.115700
1449.205609	135613.934709	36.120717
1450.654031	135812.286382	36.125735
1451.955588	135982.925413	36.130752
1453.317621	136210.627454	36.135770
1454.787012	136381.001405	36.140788
1455.893062	136582.175107	36.145805
1457.355177	136799.551266	36.150823
1458.585445	136992.826341	36.155840
1459.708930	137214.719823	36.160858
1461.353655	137419.399820	36.165876
1462.729121	137630.016482	36.170893
1463.807129	137879.369668	36.175911
1465.307317	138086.915826	36.180928
1467.008564	138299.006180	36.185946
1468.580297	138523.360105	36.190964
1469.678022	138771.425127	36.195981
1471.155202	138976.155244	36.200999
1472.806535	139188.411983	36.206016
1474.064175	139460.041103	36.211034
1475.973219	139662.312195	36.216052
1477.181143	139897.176716	36.221069
1478.586856	140137.220271	36.226087
1479.983461	140361.970751	36.231104
1481.615898	140609.243767	36.236122
1482.876666	140847.161594	36.241140
1484.783740	141073.699286	36.246157
1486.131115	141323.583499	36.251175
1488.061846	141554.011817	36.256192
1489.388923	141781.420064	36.261210
1491.099070	142041.898502	36.266228
1492.829521	142240.666670	36.271245
1494.153731	142500.386555	36.276263
1495.807509	142712.528399	36.281280
1497.169911	142959.052396	36.286298
1498.897115	143176.508968	36.291316
1500.241782	143431.987647	36.296333
1502.198353	143657.079207	36.301351
1503.818268	143887.853415	36.306368
1504.873625	144109.542578	36.311386
1506.784268	144341.123204	36.316404
1508.353941	144580.567453	36.321421
1509.730902	144808.357857	36.326439
1511.193733	145025.058301	36.331456
1512.838760	145252.061553	36.336474
1514.449070	145472.823091	36.341492
1515.674377	145705.524134	36.346509
1517.447094	145925.705368	36.351527
1519.411264	146158.305090	36.356544
1520.515507	146391.676927	36.361562
1522.212998	146613.142512	36.366580
1523.468878	146849.852727	36.371597
1525.284977	147062.125367	36.376615
1526.634567	147282.725595	36.381632
1527.645975	147482.072652	36.386650
1529.299774	147694.273919	36.391668
1530.440742	147918.638505	36.396685
1531.983322	148126.474364	36.401703
1533.574505	148350.580341	36.406720
1534.589844	148569.480602	36.411738
1536.453622	148784.774212	36.416756
1538.173617	149014.023752	36.421773
1539.456320	149235.155224	36.426791
1540.984179	149476.633622	36.431808
1542.609035	149697.016701	36.436826
1544.562861	149919.884437	36.441844
1546.007244	150152.798837	36.446861
1547.627170	150375.177643	36.451879
1549.229595	150605.509410	36.456896
1550.773598	150836.359190	36.461914
1552.724251	151041.296692	36.466932
1554.066840	151271.750526	36.471949
1555.745893	151498.323902	36.476967
1557.478468	151738.696382	36.481984
1558.716191	151960.107165	36.487002
1560.736610	152180.431601	36.492020
1562.002184	152415.495123	36.497037
1563.245003	152638.557809	36.502055
1564.954072	152872.552584	36.507072
1566.341049	153131.449545	36.512090
1568.016729	153350.999806	36.517108
1569.249194	153593.569871	36.522125
1570.787327	153829.994787	36.527143
1572.753400	154083.989363	36.532160
1574.130339	154319.175494	36.537178
1576.239908	154546.195880	36.542196
1577.667193	154790.113016	36.547213
1579.145079	155034.898737	36.552231
1580.866222	155261.491183	36.557248
1582.501574	155510.832499	36.562266
1584.112777	155743.468248	36.567284
1585.791355	155988.774229	36.572301
1587.195421	156219.062432	36.577319
1589.175230	156464.438126	36.582336
1590.498231	156712.810860	36.587354
1592.581627	156940.853203	36.592372
1593.917091	157179.704911	36.597389
1595.669603	157418.010214	36.602407
1597.555457	157640.991296	36.607424
1599.076903	157875.976293	36.612442
1600.220054	158114.218367	36.617460
1601.763411	158358.852751	36.622477
1603.802437	158589.918306	36.627495
1605.488857	158825.010365	36.632512
1606.712226	159068.952443	36.637530
1608.759504	159293.224642	36.642548
1610.170673	159525.575433	36.647565
1611.836454	159764.785645	36.652583
1613.576403	159975.390500	36.657600
1614.675122	160201.163342	36.662618
1616.225026	160410.735800	36.667636
1617.738772	160626.744533	36.672653
1619.341686	160853.443288	36.677671
1621.220520	161077.702933	36.682688
1622.610181	161296.969178	36.687706
1623.934287	161510.756164	36.692724
1625.597110	161744.818977	36.697741
1626.969636	161989.505819	36.702759
1628.543724	162223.471735	36.707776
1629.953508	162470.692277	36.712794
1631.410330	162709.321491	36.717812
1633.005838	162954.968699	36.722829
1634.542334	163216.859853	36.727847
1636.050974	163454.610725	36.732864
1637.538631	163715.498689	36.737882
1639.551211	163967.706625	36.742900
1641.282847	164225.021171	36.747917
1642.537889	164486.699871	36.752935
1644.805904	164732.937188	36.757952
1646.471317	165003.229240	36.762970
1647.838289	165261.674336	36.767988
1649.819753	165515.381779	36.773005
1651.273839	165775.287849	36.778023
1653.258382	166030.000290	36.783040
1654.567997	166309.705752	36.788058
1656.465169	166556.660997	36.793076
1658.383676	166810.425372	36.798093
1659.961105	167071.614625	36.803111
1662.209311	167332.851388	36.808128
1663.603964	167586.869110	36.813146
1665.508487	167842.760851	36.818164
1667.149089	168089.044001	36.823181
1668.912708	168356.224670	36.828199
1670.814190	168600.719380	36.833216
1672.040417	168861.875362	36.838234
1673.915864	169116.106071	36.843252
1675.412856	169373.518851	36.848269
1676.984844	169644.544229	36.853287
1678.891755	169884.112189	36.858304
1680.336343	170150.899480	36.863322
1681.990703	170413.888044	36.868340
1683.640146	170675.674158	36.873357
1685.228440	170948.228272	36.878375
1687.292736	171207.706944	36.883392
1688.846094	171476.794723	36.888410
1690.077223	171733.922991	36.893428
1692.458047	172001.132494	36.898445
1693.937959	172268.651779	36.903463
1695.704406	172519.129373	36.908480
1697.657512	172786.602421	36.913498
1699.357415	173047.990508	36.918516
1701.457961	173295.121820	36.923533
1703.030948	173545.928412	36.928551
1704.877885	173794.447757	36.933568
1706.285401	174022.931799	36.938586
1708.032368	174246.098713	36.943604
1709.811166	174477.558271	36.948621
1711.240964	174733.202943	36.953639
1713.004869	174952.539993	36.958656
1714.275401	175211.815777	36.963674
1715.737889	175439.119357	36.968692
1717.441659	175696.287012	36.973709
1719.014718	175965.313249	36.978727
1720.764389	176208.255656	36.983744
1722.396273	176472.645422	36.988762
1723.887662	176732.669704	36.993780
1725.563383	176996.510375	36.998797
1727.074326	177269.805028	37.003815
1728.801845	177546.492505	37.008832
1730.507291	177825.621192	37.013850
1731.981532	178080.746923	37.018868
1733.991089	178365.413160	37.023885
1735.613090	178649.407026	37.028903
1737.530993	178927.139169	37.033920
1739.474714	179209.880484	37.038938
1741.180872	179496.239222	37.043956
1743.081620	179779.612859	37.048973
1744.592739	180072.857632	37.053991
1746.306084	180343.475867	37.059008
1748.628573	180636.811403	37.064026
1750.324610	180928.154944	37.069044
1752.285844	181205.171940	37.074061
1754.243534	181488.230701	37.079079
1756.263642	181754.381093	37.084096
1757.887837	182040.490772	37.089114
1759.641900	182314.908678	37.094132
1761.647220	182576.283058	37.099149
1763.325341	182862.148509	37.104167
1765.138858	183135.407511	37.109184
1767.266725	183417.411378	37.114202
1768.562605	183692.608531	37.119220
1770.446981	183964.199241	37.124237
1771.761151	184236.580015	37.129255
1773.565102	184515.216377	37.134272
1775.586890	184793.604193	37.139290
1777.516454	185081.360090	37.144308
1779.569027	185347.983878	37.149325
1781.123179	185640.726275	37.154343
1783.058792	185921.317285	37.159360
1784.952834	186196.625240	37.164378
1786.595531	186477.050476	37.169396
1788.456822	186763.559007	37.174413
1789.814890	187045.517577	37.179431
1792.140620	187321.563235	37.184448
1793.684327	187599.955371	37.189466
1795.191300	187885.588126	37.194484
1797.007729	188165.120516	37.199501
1798.808870	188437.423823	37.204519
1800.404098	188712.426286	37.209536
1802.355793	188975.965509	37.214554
1803.835141	189242.753704	37.219572
1805.601161	189505.690877	37.224589
1807.311901	189772.914881	37.229607
1808.856231	190046.943404	37.234624
1810.593011	190321.996259	37.239642
1812.332285	190610.083345	37.244660
1814.487234	190884.641597	37.249677
1816.050975	191175.996028	37.254695
1817.798441	191456.764463	37.259712
1819.859378	191747.802312	37.264730
1821.602422	192027.280316	37.269748
1823.472573	192315.496436	37.274765
1825.067258	192601.778204	37.279783
1826.685386	192891.712933	37.284800
1828.507507	193184.485178	37.289818
1830.094495	193493.096967	37.294836
1831.905802	193789.910310	37.299853
1834.291963	194101.140345	37.304871
1835.881147	194405.924692	37.309888
1837.731674	194707.445785	37.314906
1839.439536	195017.025078	37.319924
1841.443963	195325.290041	37.324941
1843.276506	195638.660845	37.329959
1845.233498	195942.469620	37.334976
1847.381939	196255.134114	37.339994
1849.013667	196577.134946	37.345012
1851.041042	196876.356316	37.350029
1852.921126	197190.008307	37.355047
1854.550244	197509.248504	37.360064
1856.428101	197814.553190	37.365082
1858.514061	198135.818939	37.370100
1860.512147	198445.487077	37.375117
1861.977808	198767.083604	37.380135
1863.929952	199089.277583	37.385152
1865.711208	199405.700118	37.390170
1867.455044	199738.465963	37.395188
1869.880600	200035.217849	37.400205
1871.320250	200369.685951	37.405223
1873.460356	200693.217899	37.410240
1875.605858	201016.712845	37.415258
1877.256207	201339.082460	37.420276
1879.513748	201647.065136	37.425293
1881.249215	201973.562941	37.430311
1883.024573	202291.247208	37.435328
1885.322638	202616.314039	37.440346
1886.721707	202934.874086	37.445364
1888.672619	203256.458280	37.450381
1890.519829	203573.605331	37.455399
1892.400237	203905.143498	37.460416
1894.377699	204231.400309	37.465434
1896.115333	204557.443178	37.470452
1898.270758	204877.100060	37.475469
1900.179946	205200.656758	37.480487
1902.079116	205497.787941	37.485504
1904.560037	205781.969238	37.490522
1906.083885	206077.817386	37.495540
1908.156080	206368.438866	37.500557
1909.934991	206668.311667	37.505575
1911.857051	206942.812723	37.510592
1914.020570	207233.855595	37.515610
1915.581395	207530.441454	37.520628
1917.720769	207840.761298	37.525645
1919.376693	208131.977971	37.530663
1920.916565	208433.687543	37.535680
1923.023316	208730.167312	37.540698
1924.662597	209042.984701	37.545716
1926.554170	209365.906826	37.550733
1928.399637	209693.446218	37.555751
1930.160643	210005.995311	37.560768
1932.025391	210323.683702	37.565786
1933.617859	210661.614814	37.570804
1935.997042	210975.327503	37.575821
1937.404713	211324.717160	37.580839
1939.080024	211650.414946	37.585856
1941.515227	211995.697022	37.590874
1943.408498	212351.286784	37.595892
1945.245411	212693.442926	37.600909
1947.023245	213032.499845	37.605927
1948.872090	213381.538731	37.610944
1951.045420	213724.040496	37.615962
1952.799595	214087.888669	37.620980
1955.068036	214439.380371	37.625997
1957.084331	214787.397181	37.631015
1958.977031	215137.403295	37.636032
1961.428720	215481.964812	37.641050
1963.432628	215843.942015	37.646068
1965.325053	216182.704850	37.651085
1967.387701	216532.907053	37.656103
1969.408040	216886.317223	37.661120
1971.698747	217230.684584	37.666138
1973.520746	217574.353540	37.671156
1975.908681	217922.670180	37.676173
1977.627205	218276.427309	37.681191
1979.245242	218618.267337	37.686208
1981.999744	218968.067257	37.691226
1983.780315	219315.039683	37.696244
1985.574846	219668.271085	37.701261
1987.989223	220009.864421	37.706279
1989.859453	220363.582367	37.711296
1991.879059	220700.035827	37.716314
1993.608341	221060.254940	37.721332
1996.143887	221393.937923	37.726349
1998.305667	221743.451557	37.731367
1999.637122	222084.477146	37.736384
2002.331528	222427.129134	37.741402
2004.336492	222783.605156	37.746420
2006.064751	223126.997641	37.751437
2007.981353	223462.540151	37.756455
2009.608498	223833.543341	37.761472
2011.893816	224158.643796	37.766490
2013.743554	224482.405266	37.771508
2015.924091	224799.017590	37.776525
2017.574823	225120.768910	37.781543
2019.144713	225461.136555	37.786560
2021.427832	225781.139478	37.791578
2023.216212	226109.120216	37.796596
2025.026304	226459.624914	37.801613
2027.288763	226794.923365	37.806631
2029.399210	227134.107482	37.811648
2031.295953	227480.412400	37.816666
2033.203723	227823.745633	37.821684
2035.581673	228169.113563	37.826701
2037.586425	228518.072201	37.831719
2039.254555	228864.342828	37.836736
2041.124111	229218.481242	37.841754
2043.384368	229580.609880	37.846772
2045.295294	229940.001773	37.851789
2047.478242	230299.275778	37.856807
2049.132340	230670.139990	37.861824
2051.479184	231032.006826	37.866842
2053.299035	231398.276238	37.871860
2055.643472	231769.517973	37.876877
2057.719840	232136.841720	37.881895
2059.324426	232522.578799	37.886912
2061.822683	232889.990964	37.891930
2063.855838	233267.561248	37.896948
2066.144994	233643.212971	37.901965
2068.118665	234010.814251	37.906983
2070.384919	234385.812139	37.912000
2072.854855	234758.518716	37.917018
2074.751520	235131.546214	37.922036
2076.882821	235503.928324	37.927053
2079.272483	235879.572624	37.932071
2081.228548	236261.738317	37.937088
2083.317784	236632.048544	37.942106
2085.562473	237006.551621	37.947124
2087.577275	237373.345866	37.952141
2089.922543	237744.990951	37.957159
2092.247268	238114.837260	37.962176
2094.353132	238475.194902	37.967194
2096.300707	238848.202222	37.972212
2098.617946	239209.036736	37.977229
2101.042712	239580.726276	37.982247
2103.194577	239947.583649	37.987264
2105.013172	240306.418033	37.992282
2107.444827	240677.830685	37.997300
2109.663704	241039.220020	38.002317
2111.663785	241388.478710	38.007335
2113.820781	241752.216827	38.012352
2116.261198	242110.627927	38.017370
2118.199452	242478.390719	38.022388
2120.296142	242829.695678	38.027405
2122.821287	243173.262855	38.032423
2124.598748	243514.561952	38.037440
2126.736665	243834.087612	38.042458
2128.990261	244162.104826	38.047476
2130.818721	244491.663525	38.052493
2132.949283	244815.028248	38.057511
2135.037257	245154.402825	38.062528
2136.811455	245481.000761	38.067546
2139.173165	245821.121039	38.072564
2140.957550	246162.273559	38.077581
2142.931193	246511.296541	38.082599
2144.479354	246862.927960	38.087616
2146.685527	247222.203165	38.092634
2148.820076	247571.101659	38.097652
2150.703256	247938.431180	38.102669
2152.608259	248310.736772	38.107687
2154.833262	248688.428392	38.112704
2157.097033	249059.764521	38.117722
2159.127224	249441.248296	38.122740
2160.717909	249820.973822	38.127757
2163.051348	250210.260399	38.132775
2165.203300	250598.027226	38.137792
2167.198349	250995.599443	38.142810
2169.736048	251393.289781	38.147828
2171.770973	251787.250562	38.152845
2174.278048	252184.769824	38.157863
2176.120382	252585.342023	38.162880
2178.608202	252977.912822	38.167898
2180.701866	253384.035372	38.172916
2183.069595	253786.762321	38.177933
2185.219477	254181.345267	38.182951
2187.525122	254603.516325	38.187968
2189.502572	254993.454337	38.192986
2192.002112	255410.439793	38.198004
2194.589411	255816.032038	38.203021
2196.572977	256222.432093	38.208039
2199.017735	256630.436362	38.213056
2201.218512	257035.584243	38.218074
2203.515977	257435.738690	38.223092
2205.367939	257839.266819	38.228109
2207.925905	258240.524510	38.233127
2210.042493	258648.863977	38.238144
2212.558788	259057.953650	38.243162
2215.038558	259452.671948	38.248180
2217.289787	259861.601775	38.253197
2219.552635	260259.226236	38.258215
2221.685344	260670.259160	38.263232
2223.918186	261064.866672	38.268250
2226.216519	261469.371447	38.273268
2228.699452	261870.951612	38.278285
2231.188001	262252.259976	38.283303
2233.466330	262651.765214	38.288320
2235.437855	263035.671429	38.293338
2238.290012	263442.783776	38.298356
2240.350217	263832.062303	38.303373
2242.512437	264205.194203	38.308391
2244.914272	264576.840539	38.313408
2247.115825	264928.526820	38.318426
2249.414584	265282.585911	38.323444
2251.363998	265647.420823	38.328461
2253.725824	265994.560921	38.333479
2255.872611	266359.034943	38.338496
2257.602667	266721.035033	38.343514
2259.913727	267081.698546	38.348532
2261.946214	267454.955687	38.353549
2264.136328	267832.557479	38.358567
2266.102478	268217.917647	38.363584
2268.231697	268606.859502	38.368602
2270.468474	268988.747871	38.373620
2272.264560	269393.797944	38.378637
2274.710953	269789.244343	38.383655
2276.895477	270196.875280	38.388672
2279.151695	270595.070448	38.393690
2281.569337	270996.263230	38.398708
2284.048251	271408.192111	38.403725
2286.414019	271815.185463	38.408743
2288.543248	272232.733480	38.413760
2290.740718	272650.448660	38.418778
2293.065970	273051.072642	38.423796
2295.220262	273476.974819	38.428813
2297.551666	273896.472772	38.433831
2300.109478	274320.939392	38.438848
2302.110544	274746.612095	38.443866
2304.722413	275173.508998	38.448884
2306.696430	275607.238958	38.453901
2309.320660	276023.667742	38.458919
2311.724983	276461.571867	38.463936
2314.080332	276894.555469	38.468954
2316.496744	277321.153091	38.473972
2318.766443	277754.963072	38.478989
2321.426123	278188.558728	38.484007
2323.884151	278617.816863	38.489024
2326.078470	279036.955326	38.494042
2328.611525	279468.690841	38.499060
2331.039944	279903.745219	38.504077
2333.262054	280325.266725	38.509095
2335.414643	280756.757170	38.514112
2337.885810	281190.254565	38.519130
2340.536257	281609.802283	38.524148
2342.599586	282051.365871	38.529165
2345.253684	282476.145565	38.534183
2347.816055	282905.258065	38.539200
2349.779302	283335.227316	38.544218
2352.564864	283756.936854	38.549236
2354.534728	284195.719284	38.554253
2357.341264	284615.138497	38.559271
2359.838594	285038.391419	38.564288
2362.216068	285479.876984	38.569306
2364.799767	285897.196456	38.574324
2367.164086	286310.104738	38.579341
2369.536701	286720.496369	38.584359
2372.236966	287109.928933	38.589376
2374.325833	287496.816078	38.594394
2376.458921	287883.517969	38.599412
2378.414078	288275.328212	38.604429
2380.877277	288677.345645	38.609447
2383.120421	289072.183035	38.614464
2385.086602	289464.929982	38.619482
2387.685540	289864.282470	38.624500
2389.684061	290282.400616	38.629517
2391.843681	290687.359399	38.634535
2394.281850	291107.134020	38.639552
2396.632961	291528.471345	38.644570
2398.906204	291954.291194	38.649588
2401.208985	292387.218369	38.654605
2403.894166	292818.687043	38.659623
2406.106112	293260.213125	38.664640
2408.369965	293699.291518	38.669658
2410.935694	294124.146700	38.674676
2413.038410	294574.730814	38.679693
2415.344339	295006.433303	38.684711
2418.122370	295471.210006	38.689728
2420.243178	295930.780780	38.694746
2422.398276	296370.912471	38.699764
2424.995199	296836.349822	38.704781
2427.705972	297284.164440	38.709799
2430.090494	297747.651901	38.714816
2432.374315	298204.625893	38.719834
2435.313013	298666.270502	38.724852
2437.582420	299133.379757	38.729869
2440.007842	299606.991275	38.734887
2442.656980	300061.946668	38.739904
2444.876302	300530.253951	38.744922
2447.647072	300992.731794	38.749940
2450.016801	301457.405593	38.754957
2452.763382	301924.253637	38.759975
2455.328534	302397.022131	38.764992
2457.807634	302857.915071	38.770010
2460.279172	303312.863956	38.775028
2462.987846	303795.054546	38.780045
2465.528397	304259.235543	38.785063
2467.891695	304720.471234	38.790080
2470.249605	305199.308996	38.795098
2472.962517	305657.946138	38.800116
2475.564579	306125.413312	38.805133
2478.076211	306585.120650	38.810151
2480.510323	307053.093813	38.815168
2482.819139	307521.161362	38.820186
2485.689564	307970.748469	38.825204
2488.465825	308448.212845	38.830221
2490.915608	308911.503123	38.835239
2493.478384	309370.404974	38.840256
2496.219343	309834.814030	38.845274
2498.470242	310293.685604	38.850292
2501.026816	310751.617983	38.855309
2503.480088	311196.280982	38.860327
2506.621017	311624.603071	38.865344
2508.514465	312052.664026	38.870362
2511.132623	312470.702823	38.875380
2513.205392	312900.738674	38.880397
2515.617449	313319.543506	38.885415
2518.442801	313739.932180	38.890432
2520.717017	314170.997865	38.895450
2523.148699	314602.773423	38.900468
2525.633478	315045.993593	38.905485
2528.028915	315468.500824	38.910503
2530.588796	315914.270639	38.915520
2532.448098	316360.936851	38.920538
2535.065367	316816.725946	38.925556
2537.593373	317276.666990	38.930573
2539.726432	317731.639665	38.935591
2542.538311	318190.794910	38.940608
2544.769585	318663.272173	38.945626
2547.177002	319143.186085	38.950644
2549.776795	319612.831901	38.955661
2552.270004	320084.117670	38.960679
2555.230387	320568.000231	38.965696
2557.578428	321055.736008	38.970714
2560.643275	321529.615851	38.975732
2563.008425	322012.213550	38.980749
2565.620692	322504.724959	38.985767
2568.337180	322981.877591	38.990784
2570.382371	323469.622650	38.995802
2573.314938	323963.217868	39.000820
2576.049828	324453.997172	39.005837
2578.709835	324953.978802	39.010855
2581.464867	325440.050883	39.015872
2583.905857	325928.988761	39.020890
2587.171824	326419.748472	39.025908
2589.804683	326918.122510	39.030925
2592.332987	327399.393667	39.035943
2595.019121	327885.969851	39.040960
2597.529521	328377.040351	39.045978
2600.086883	328846.413245	39.050996
2602.786107	329358.423623	39.056013
2605.407762	329845.556384	39.061031
2608.502744	330321.259823	39.066048
2610.908032	330821.396982	39.071066
2613.372663	331312.328796	39.076084
2616.126786	331809.128212	39.081101
2618.539175	332297.496942	39.086119
2621.311355	332798.375092	39.091136
2623.914527	333301.638078	39.096154
2626.572201	333792.420912	39.101172
2629.211959	334275.432967	39.106189
2631.645717	334787.472699	39.111207
2634.507205	335264.780210	39.116224
2636.816264	335786.506804	39.121242
2639.431514	336270.118193	39.126260
2642.107040	336771.897167	39.131277
2644.572329	337269.084396	39.136295
2646.860226	337744.408520	39.141312
2649.682206	338215.861318	39.146330
2652.384768	338692.661777	39.151348
2654.758671	339169.206100	39.156365
2656.884240	339642.561605	39.161383
2660.075067	340109.498806	39.166400
2662.505490	340615.070236	39.171418
2664.926831	341089.459900	39.176436
2667.616214	341586.756071	39.181453
2670.085699	342079.030519	39.186471
2672.925291	342567.154695	39.191488
2675.629409	343078.045317	39.196506
2678.518414	343579.051363	39.201524
2680.663386	344082.456087	39.206541
2683.563359	344582.664965	39.211559
2686.489123	345093.934940	39.216576
2688.623547	345611.672881	39.221594
2691.257242	346122.243898	39.226612
2694.413745	346641.943419	39.231629
2697.034093	347163.551073	39.236647
2699.747243	347678.487781	39.241664
2702.183141	348220.805688	39.246682
2705.079863	348738.623201	39.251700
2707.982060	349285.782043	39.256717
2710.357301	349810.805836	39.261735
2713.597704	350344.268151	39.266752
2715.959583	350875.325802	39.271770
2718.904712	351418.521798	39.276788
2721.825322	351953.313640	39.281805
2724.700123	352481.304176	39.286823
2727.791207	353012.631420	39.291840
2730.499809	353563.686998	39.296858
2733.343607	354085.167955	39.301876
2736.024089	354619.590084	39.306893
2739.024516	355156.088280	39.311911
2741.833968	355688.625895	39.316928
2744.931449	356225.325984	39.321946
2747.391868	356749.455121	39.326964
2750.796155	357285.156209	39.331981
2753.183346	357824.693087	39.336999
2755.600771	358344.776515	39.342016
2758.249577	358882.915196	39.347034
2761.156297	359420.829471	39.352052
2764.262055	359961.396731	39.357069
2766.572214	360505.434251	39.362087
2769.620533	361032.495856	39.367104
2772.329224	361574.250029	39.372122
2775.030390	362120.618435	39.377140
2778.327100	362659.043813	39.382157
2780.814569	363200.839750	39.387175
2783.582265	363736.823905	39.392192
2786.364500	364275.286718	39.397210
2789.259117	364823.826216	39.402228
2791.958479	365357.873556	39.407245
2794.790732	365885.320635	39.412263
2797.205730	366392.246134	39.417280
2800.361089	366895.394325	39.422298
2802.761805	367395.966341	39.427316
2805.875994	367909.133683	39.432333
2808.318444	368413.621064	39.437351
2810.921630	368914.397626	39.442368
2813.580185	369433.405181	39.447386
2816.191581	369946.958201	39.452404
2819.261508	370475.759391	39.457421
2822.049802	370986.912110	39.462439
2825.268476	371505.298585	39.467456
2828.196679	372025.678587	39.472474
2830.715372	372548.705213	39.477492
2834.026023	373073.959754	39.482509
2836.522511	373601.391874	39.487527
2839.186482	374140.614803	39.492544
2841.724293	374675.105931	39.497562
2844.722762	375228.013914	39.502580
2847.213798	375760.925222	39.507597
2849.750147	376320.437663	39.512615
2852.765482	376877.532363	39.517632
2855.927284	377438.249652	39.522650
2858.788741	378001.416887	39.527668
2862.174749	378550.184104	39.532685
2865.086976	379103.661487	39.537703
2867.888981	379662.679192	39.542720
2870.296401	380225.962738	39.547738
2873.334735	380784.698677	39.552756
2876.374479	381360.829349	39.557773
2879.036230	381936.732204	39.562791
2882.069679	382501.329540	39.567808
2885.222755	383080.206954	39.572826
2887.778137	383652.853702	39.577844
2890.392292	384245.522305	39.582861
2893.213687	384819.301458	39.587879
2896.512572	385416.358390	39.592896
2898.913057	385996.070979	39.597914
2901.836080	386595.958627	39.602932
2905.029189	387185.140494	39.607949
2907.772550	387786.229254	39.612967
2910.666779	388384.976074	39.617984
2913.802260	388979.768802	39.623002
2916.174180	389587.024426	39.628020
2919.628079	390191.384680	39.633037
2922.450189	390790.838292	39.638055
2925.217915	391407.637897	39.643072
2928.271228	392005.969090	39.648090
2931.255060	392611.326064	39.653108
2934.461515	393220.339932	39.658125
2937.167155	393830.766454	39.663143
2940.321980	394438.676552	39.668160
2943.343438	395048.270696	39.673178
2945.812042	395654.720889	39.678196
2948.946444	396275.128744	39.683213
2951.760638	396882.643383	39.688231
2954.704093	397459.849849	39.693248
2957.654830	398034.281293	39.698266
2960.330083	398598.198103	39.703284
2963.507693	399175.033497	39.708301
2966.289500	399766.348810	39.713319
2969.151640	400341.337365	39.718336
2972.162385	400921.287171	39.723354
2974.674197	401513.982739	39.728372
2978.175907	402093.605699	39.733389
2980.452361	402688.345265	39.738407
2983.233115	403296.912729	39.743424
2985.990981	403904.534171	39.748442
2988.936789	404523.978938	39.753460
2991.903518	405138.794295	39.758477
2994.745683	405765.684378	39.763495
2997.684562	406400.354519	39.768512
3000.865667	407030.461118	39.773530
3003.733557	407665.725039	39.778548
3006.516098	408308.796819	39.783565
3009.334015	408966.703624	39.788583
3012.846867	409604.968527	39.793600
3016.049501	410263.268057	39.798618
3019.026165	410916.114136	39.803636
3022.329518	411562.507140	39.808653
3025.075976	412220.177044	39.813671
3028.446058	412872.943554	39.818688
3031.763363	413533.712884	39.823706
3034.767852	414187.648730	39.828724
3038.143373	414842.626414	39.833741
3041.037408	415519.941854	39.838759
3044.314811	416163.323777	39.843776
3047.513711	416822.314233	39.848794
3050.469473	417492.376757	39.853812
3053.752657	418136.803361	39.858829
3056.960824	418800.333514	39.863847
3059.476461	419468.442786	39.868864
3062.882866	420117.213996	39.873882
3066.285771	420785.861170	39.878900
3069.310653	421465.447289	39.883917
3071.999017	422133.187127	39.888935
3075.337976	422797.514264	39.893952
3078.531828	423454.779754	39.898970
3081.191669	424141.603940	39.903988
3084.795386	424804.751299	39.909005
3087.979976	425461.387392	39.914023
3091.094512	426135.219862	39.919040
3094.528609	426792.974834	39.924058
3097.359564	427466.388231	39.929076
3100.346036	428128.867660	39.934093
3103.665572	428809.414630	39.939111
3107.071833	429462.219466	39.944128
3110.294388	430130.006858	39.949146
3113.181825	430801.249680	39.954164
3116.649992	431463.569274	39.959181
3119.614142	432104.778076	39.964199
3122.267033	432742.727802	39.969216
3125.550093	433361.516826	39.974234
3128.346245	433985.914303	39.979252
3131.829140	434609.022996	39.984269
3134.412441	435231.726985	39.989287
3137.429299	435855.258807	39.994304
3140.237128	436484.987183	39.999322
3142.876989	437127.083768	40.004340
3146.062480	437764.038612	40.009357
3149.491090	438422.487073	40.014375
3152.599008	439075.575621	40.019392
3155.875956	439725.607203	40.024410
3158.577467	440407.893309	40.029428
3161.547562	441074.977636	40.034445
3164.703488	441743.685399	40.039463
3167.836347	442426.758568	40.044480
3171.024748	443104.892414	40.049498
3173.970856	443791.855428	40.054516
3177.570225	444484.062304	40.059533
3180.526517	445177.819174	40.064551
3183.559212	445879.593500	40.069568
3186.942998	446587.518532	40.074586
3189.888223	447286.480784	40.079604
3193.523295	447992.501609	40.084621
3196.484779	448710.402409	40.089639
3199.558468	449419.759454	40.094656
3203.180736	450135.588458	40.099674
3206.409748	450853.482248	40.104692
3209.871523	451578.605432	40.109709
3212.850852	452307.780513	40.114727
3215.811847	453022.156844	40.119744
3219.617787	453736.731477	40.124762
3222.607184	454471.757249	40.129780
3225.950930	455202.502812	40.134797
3228.905403	455945.482021	40.139815
3232.157694	456682.570219	40.144832
3235.633825	457399.661782	40.149850
3238.763931	458169.560540	40.154868
3242.202298	458905.230210	40.159885
3245.764993	459641.715870	40.164903
3248.821538	460385.947316	40.169920
3252.529916	461136.273340	40.174938
3255.554584	461870.037209	40.179956
3259.052407	462614.982942	40.184973
3262.314084	463351.694596	40.189991
3265.401398	464085.778189	40.195008
3268.961778	464822.442857	40.200026
3272.234721	465568.890038	40.205044
3275.098312	466315.072325	40.210061
3278.771691	467059.380646	40.215079
3282.076142	467810.650170	40.220096
3285.735050	468541.404398	40.225114
3288.608301	469276.606731	40.230132
3292.188786	470032.254087	40.235149
3295.425756	470760.064272	40.240167
3298.621440	471439.360453	40.245184
3302.418872	472134.417076	40.250202
3305.622298	472836.825497	40.255220
3308.505256	473507.810215	40.260237
3311.838655	474199.533046	40.265255
3314.633243	474899.710504	40.270272
3318.094487	475589.646781	40.275290
3321.168530	476305.252790	40.280308
3324.295693	477022.189953	40.285325
3327.797685	477716.799054	40.290343
3330.632463	478444.650937	40.295360
3333.991498	479166.984600	40.300378
3337.237664	479888.905452	40.305396
3339.796771	480643.257602	40.310413
3343.086892	481394.988683	40.315431
3346.122564	482143.344941	40.320448
3349.546206	482886.001348	40.325466
3352.527815	483686.362635	40.330484
3356.235938	484442.660806	40.335501
3359.243209	485237.091878	40.340519
3362.791072	486001.439650	40.345536
3366.120702	486822.535868	40.350554
3369.612452	487602.442144	40.355572
3372.568156	488405.137498	40.360589
3377.100113	489168.950189	40.365607
3380.217121	490012.323906	40.370624
3383.690678	490779.573062	40.375642
3387.185481	491607.205211	40.380660
3390.911615	492383.138564	40.385677
3394.357403	493178.480567	40.390695
3397.542102	493999.236241	40.395712
3401.663603	494782.128596	40.400730
3404.843974	495588.368991	40.405748
3408.410100	496384.361784	40.410765
3411.961700	497198.755101	40.415783
3415.923296	497978.808911	40.420800
3419.294627	498792.502784	40.425818
3422.785335	499590.235394	40.430836
3425.922620	500387.180639	40.435853
3429.526124	501184.117752	40.440871
3432.623800	501997.962160	40.445888
3436.385199	502793.085834	40.450906
3439.888866	503588.315565	40.455924
3443.275126	504413.160307	40.460941
3447.151568	505211.236314	40.465959
3450.563955	506008.137934	40.470976
3453.469503	506804.477653	40.475994
3456.823498	507627.863775	40.481012
3460.682952	508439.775394	40.486029
3464.221886	509234.894113	40.491047
3467.504597	510087.495580	40.496064
3470.733687	510871.132234	40.501082
3474.605580	511671.182167	40.506100
3477.520465	512491.427788	40.511117
3481.353022	513286.983739	40.516122
3484.657403	514040.397530	40.521127
3488.390666	514750.312744	40.526132
3491.612788	515385.171233	40.531136
3495.076484	515958.821416	40.536141
3498.199196	516485.926991	40.541146
3500.726650	516914.543590	40.546151
3504.013670	517257.259364	40.551156
3505.935923	517619.501825	40.556160
3507.843189	517853.088906	40.561165
3510.175885	518088.779945	40.566170
3511.825963	518242.755205	40.571175
3513.592675	518401.110054	40.576180
3515.126925	518449.261628	40.581184
3516.498502	518505.428535	40.586189
3517.769458	518483.786908	40.591194
3518.288834	518447.599234	40.596199
3519.817051	518348.496545	40.601204
3520.698088	518267.194648	40.606208
3521.243109	518178.916354	40.611213
3521.955257	517989.472119	40.616218
3522.331810	517826.476417	40.621223
3522.170488	517660.125316	40.626228
3522.806515	517430.179573	40.631232
3523.239593	517241.478927	40.636237
3523.961808	516991.992732	40.641242
3523.946966	516774.682840	40.646247
3523.751690	516513.399171	40.651252
3523.909050	516233.292368	40.656256
3524.045676	516013.622193	40.661261
3524.091337	515715.367702	40.666266
3524.042053	515439.832182	40.671271
3523.765120	515151.481241	40.676276
3523.702043	514868.452943	40.681280
3523.286700	514596.754888	40.686285
3523.681007	514283.195321	40.691290
3522.853514	514036.590889	40.696295
3523.328624	513719.214457	40.701300
3522.882089	513464.498840	40.706304
3522.869494	513145.367725	40.711309
3522.446754	512891.196154	40.716314
3522.157094	512584.289261	40.721319
3522.093416	512291.454842	40.726324
3521.508877	512059.099302	40.731328
3521.223073	511778.533340	40.736333
3520.888522	511494.226867	40.741338
3521.086678	511205.936038	40.746343
3520.804046	510972.303823	40.751348
3520.326489	510695.848235	40.756352
3520.281493	510403.737368	40.761357
3520.194585	510188.377977	40.766362
3519.845964	509915.936886	40.771367
3520.002105	509620.644098	40.776372
3519.399251	509378.844457	40.781376
3519.046661	509157.847467	40.786381
3518.916455	508923.556154	40.791386
3518.495449	508669.321617	40.796391
3517.743540	508413.010510	40.801396
3518.533536	508168.646278	40.806400
3517.961519	507968.464926	40.811405
3518.082274	507710.386323	40.816410
3517.332372	507516.654108	40.821415
3517.076991	507263.840205	40.826420
3517.161272	507016.231589	40.831424
3516.609719	506831.113386	40.836429
3516.517641	506622.339398	40.841434
3516.054891	506419.390359	40.846439
3515.883709	506204.298365	40.851444
3516.211898	505989.630856	40.856448
3515.047673	505824.992737	40.861453
3515.732287	505609.049693	40.866458
3514.762118	505436.179009	40.871463
3514.855560	505217.591803	40.876468
3514.609652	505067.781257	40.881472
3514.066656	504856.476472	40.886477
3514.156327	504708.583562	40.891482
3513.820255	504517.485588	40.896487
3513.560099	504384.220784	40.901492
3513.167574	504198.543533	40.906496
3513.410704	504014.332806	40.911501
3513.268588	503876.338687	40.916506
3512.802163	503753.426438	40.921511
3512.493004	503562.566924	40.926516
3512.503983	503448.737925	40.931520
3511.940956	503291.775415	40.936525
3512.034458	503122.307439	40.941530
3511.703172	503026.801300	40.946535
3511.816257	502868.665296	40.951540
3512.071445	502732.421582	40.956544
3511.488263	502632.499042	40.961549
3511.658617	502481.588474	40.966554
3511.033833	502363.955610	40.971559
3511.132102	502212.497379	40.976564
3510.553979	502126.996788	40.981568
3510.499072	501998.186448	40.986573
3510.667037	501860.988128	40.991578
3510.266347	501786.745477	40.996583
3510.191917	501651.557932	41.001588
3510.186935	501561.914627	41.006592
3510.133929	501458.611534	41.011597
3510.257792	501313.165193	41.016602
3509.745014	501246.632048	41.021607
3509.890125	501120.719658	41.026612
3509.925881	501050.100169	41.031616
3509.280935	500928.968281	41.036621
3509.573104	500826.265038	41.041626
3509.331004	500767.229717	41.046631
3509.267515	500644.485401	41.051636
3509.006910	500578.163017	41.056640
3508.505640	500491.680653	41.061645
3509.098758	500372.677898	41.066650
3508.480309	500331.266219	41.071655
3508.660027	500233.032040	41.076660
3508.832899	500160.311884	41.081664
3508.205440	500061.900609	41.086669
3508.368640	500019.605340	41.091674
3507.961933	499922.322726	41.096679
3508.056781	499837.869147	41.101684
3508.027461	499795.198795	41.106688
3508.135439	499692.113194	41.111693
3508.101800	499659.770346	41.116698
3507.654535	499557.075466	41.121703
3507.698774	499510.191051	41.126708
3507.798093	499422.748016	41.131712
3507.413515	499387.827695	41.136717
3507.616367	499298.697100	41.141722
3507.205457	499263.932573	41.146727
3507.404317	499204.822427	41.151732
3507.293712	499133.914791	41.156736
3507.412132	499096.383167	41.161741
3507.564435	499015.713525	41.166746
3507.188182	498958.718474	41.171751
3507.524867	498914.722560	41.176756
3507.506863	498829.674591	41.181760
3507.098110	498807.413382	41.186765
3507.611319	498710.434468	41.191770
3507.052564	498682.678576	41.196775
3507.056833	498611.193846	41.201780
3507.002139	498573.536618	41.206784
3506.830155	498513.622174	41.211789
3507.101497	498455.713161	41.216794
3506.604463	498398.786060	41.221799
3506.382540	498374.165952	41.226804
3506.409897	498301.765066	41.231808
3506.195241	498274.966707	41.236813
3506.372871	498244.866160	41.241818
3506.475442	498188.451159	41.246823
3506.525235	498138.828425	41.251828
3506.419567	498098.292491	41.256832
3506.161385	498058.590616	41.261837
3506.499077	498025.679877	41.266842
3506.215257	497988.867693	41.271847
3506.497068	497926.449441	41.276852
3506.503241	497916.424206	41.281856
3506.017623	497842.836857	41.286861
3505.807170	497844.996640	41.291866
3506.097271	497792.094759	41.296871
3505.839742	497767.175681	41.301876
3505.535583	497756.136203	41.306880
3505.615539	497698.660052	41.311885
3505.469225	497669.875471	41.316890
3505.390315	497625.385196	41.321895
3505.215018	497652.499546	41.326900
3505.437094	497601.734278	41.331904
3505.483623	497560.211135	41.336909
3505.942373	497538.165661	41.341914
3505.337092	497526.667342	41.346919
3505.739559	497483.923295	41.351924
3505.791215	497451.664278	41.356928
3505.431124	497435.165454	41.361933
3505.460483	497400.732799	41.366938
3505.503162	497383.967753	41.371943
3505.624497	497346.432047	41.376948
3505.592202	497334.134228	41.381952
3505.646330	497306.329989	41.386957
3505.612687	497262.641751	41.391962
3505.375548	497267.387952	41.396967
3505.513351	497208.685990	41.401972
3505.251551	497211.056483	41.406976
3505.001263	497181.477479	41.411981
3505.284672	497172.775035	41.416986
3505.226213	497137.039373	41.421991
3505.322686	497105.633377	41.426996
3505.652255	497108.366093	41.432000
3505.690394	497042.337926	41.437005
3505.664714	497051.556890	41.442010
3505.383410	496993.274888	41.447015
3505.235120	496985.146891	41.452020
3505.635024	496941.237469	41.457024
3505.237572	496927.731314	41.462029
3505.512749	496913.207484	41.467034
3505.400742	496893.631097	41.472039
3505.022372	496859.413753	41.477044
3505.433270	496837.324366	41.482048
3505.088692	496826.341340	41.487053
3505.208638	496799.741077	41.492058
3505.103076	496772.923260	41.497063
3504.808681	496769.172559	41.502068
3505.350355	496723.670633	41.507072
3505.070972	496731.866594	41.512077
3505.296350	496695.021944	41.517082
3504.948380	496681.609049	41.522087
3505.016256	496658.206604	41.527092
3504.836687	496635.653346	41.532096
3505.399820	496616.931962	41.537101
3505.010532	496617.550566	41.542106
3505.068555	496621.693333	41.547111
3504.911030	496572.048463	41.552116
3505.026913	496575.574512	41.557120
3504.597246	496557.263137	41.562125
3505.012664	496531.476529	41.567130
3504.810656	496527.154224	41.572135
3504.645098	496518.066738	41.577140
3505.115104	496488.423400	41.582144
3505.048107	496473.193817	41.587149
3505.091895	496459.161887	41.592154
3504.997481	496453.303591	41.597159
3504.897627	496436.762731	41.602164
3505.169996	496396.213891	41.607168
3504.740482	496414.256415	41.612173
3505.015282	496358.669276	41.617178
3505.119803	496371.209755	41.622183
3504.908183	496329.724610	41.627188
3504.974533	496349.005277	41.632192
3505.124226	496306.349057	41.637197
3504.959066	496306.122124	41.642202
3505.283773	496261.969792	41.647207
3504.698387	496264.492814	41.652212
3504.793043	496233.946365	41.657216
3504.605708	496229.469771	41.662221
3504.981197	496221.916879	41.667226
3505.268053	496175.188040	41.672231
3504.709840	496204.035952	41.677236
3504.943620	496148.150859	41.682240
3504.935120	496168.557475	41.687245
3504.610937	496139.292259	41.692250
3504.798795	496100.629548	41.697255
3504.774721	496084.076392	41.702260
3505.047631	496107.679131	41.707264
3504.408332	496081.501621	41.712269
3505.251003	496045.469501	41.717274
3505.000670	496037.407843	41.722279
3504.623739	496039.492881	41.727284
3505.011939	496022.773244	41.732288
3504.582279	496001.929635	41.737293
3504.825363	496016.473799	41.742298
3504.773442	495970.203048	41.747303
3504.736694	495983.576258	41.752308
3505.265828	495944.454211	41.757312
3504.831988	495953.282535	41.762317
3504.813400	495918.955932	41.767322
3504.723831	495920.894299	41.772327
3504.926211	495867.798171	41.777332
3504.914268	495893.420931	41.782336
3505.131282	495857.892398	41.787341
3504.992819	495858.218213	41.792346
3504.805032	495839.918523	41.797351
3504.508940	495836.218531	41.802356
3504.981467	495795.181020	41.807360
3504.816624	495779.966325	41.812365
3504.989786	495781.863182	41.817370
3505.033270	495747.475813	41.822375
3505.178116	495735.503361	41.827380
3504.742490	495709.191858	41.832384
3504.871436	495702.386600	41.837389
3505.120278	495696.220638	41.842394
3505.240946	495659.694261	41.847399
3504.643864	495642.724925	41.852404
3504.956386	495632.801921	41.857408
3505.035329	495613.447157	41.862413
3505.303228	495591.024427	41.867418
3505.309805	495579.124361	41.872423
3504.714016	495550.103668	41.877428
3504.840676	495544.868392	41.882432
3504.850443	495536.967944	41.887437
3504.565738	495490.783410	41.892442
3504.525963	495487.296011	41.897447
3504.438542	495497.335676	41.902452
3504.918382	495462.878808	41.907456
3504.627424	495457.709512	41.912461
3504.663687	495457.602637	41.917466
3504.829513	495432.765365	41.922471
3504.614959	495423.482538	41.927476
3504.714980	495407.516780	41.932480
3504.335716	495410.614960	41.937485
3504.893901	495413.261167	41.942490
3504.609812	495381.912360	41.947495
3504.226135	495399.898000	41.952500
3504.785742	495347.402166	41.957504
3504.774990	495391.406062	41.962509
3504.563722	495380.299826	41.967514
3504.687633	495330.657744	41.972519
3504.315552	495354.414030	41.977524
3504.660120	495320.535264	41.982528
3504.720513	495307.208724	41.987533
3504.812801	495308.004433	41.992538
3504.442051	495279.909818	41.997543
3504.565973	495292.701147	42.002548
3504.760402	495235.249794	42.007552
3504.649741	495270.408527	42.012557
3504.715304	495246.093204	42.017562
3504.512338	495231.238528	42.022567
3504.638871	495208.533861	42.027572
3504.994229	495206.249852	42.032576
3504.541801	495201.612360	42.037581
3504.764944	495158.688686	42.042586
3504.710336	495182.091202	42.047591
3504.414625	495157.630318	42.052596
3504.613590	495149.446622	42.057600
3504.322442	495154.657625	42.062605
3504.719499	495131.454384	42.067610
3504.525790	495132.852298	42.072615
3504.509293	495094.726127	42.077620
3504.906915	495124.285475	42.082624
3504.825831	495078.675354	42.087629
3504.952575	495080.883438	42.092634
3504.866807	495051.831983	42.097639
3504.484030	495054.576325	42.102644
3505.135548	494997.811530	42.107648
3504.887690	495023.219608	42.112653
3504.700716	494984.765699	42.117658
3504.754317	494999.391254	42.122663
3504.769977	494970.576823	42.127668
3505.295850	494937.023152	42.132672
3504.693263	494961.829104	42.137677
3504.596910	494914.752534	42.142682
3505.091412	494885.204013	42.147687
3504.690480	494911.041532	42.152692
3504.845891	494866.659421	42.157696
3504.391125	494887.644359	42.162701
3504.916346	494832.367478	42.167706
3504.675554	494855.901109	42.172711
3504.537188	494828.326079	42.177716
3504.752626	494826.722416	42.182720
3504.289448	494804.313002	42.187725
3504.648710	494827.650557	42.192730
3504.159743	494793.851925	42.197735
3504.388671	494762.977987	42.202740
3504.486179	494797.497079	42.207744
3504.597869	494761.324795	42.212749
3504.571334	494780.672427	42.217754
3504.583432	494735.806283	42.222759
3504.405265	494750.873763	42.227764
3504.636497	494724.708636	42.232768
3504.316040	494728.911650	42.237773
3504.316331	494720.860438	42.242778
3504.767337	494687.824517	42.247783
3504.248456	494699.350649	42.252788
3504.365382	494697.509359	42.257792
3504.222013	494665.529445	42.262797
3504.656532	494676.398535	42.267802
3504.437565	494652.988232	42.272807
3504.549988	494683.201012	42.277812
3504.934249	494632.705706	42.282816
3504.742902	494613.493884	42.287821
3504.687706	494646.619547	42.292826
3504.455401	494592.322507	42.297831
3504.435991	494598.351555	42.302836
3504.484517	494596.065329	42.307840
3504.777446	494559.053805	42.312845
3504.465481	494586.346205	42.317850
3504.298158	494585.613216	42.322855
3504.287984	494550.523165	42.327860
3505.097529	494534.393874	42.332864
3504.940787	494516.999435	42.337869
3504.563801	494529.262811	42.342874
3504.614685	494493.757902	42.347879
3504.553398	494487.539277	42.352884
3504.667875	494486.255368	42.357888
3504.100822	494464.165782	42.362893
3504.465327	494473.881389	42.367898
3504.408897	494463.459055	42.372903
3504.665103	494425.946690	42.377908
3504.321283	494465.549305	42.382912
3504.051218	494435.665165	42.387917
3504.100677	494433.226858	42.392922
3504.287760	494420.335394	42.397927
3504.580372	494398.312411	42.402932
3504.519568	494407.133152	42.407936
3504.718783	494384.061517	42.412941
3504.758681	494382.232370	42.417946
3504.322736	494410.658660	42.422951
3504.443521	494403.601024	42.427956
3504.763254	494378.332902	42.432960
3504.092078	494341.169489	42.437965
3504.536330	494326.566257	42.442970
3504.560248	494328.132387	42.447975
3504.278812	494333.139533	42.452980
3504.717923	494279.646943	42.457984
3504.299002	494321.388544	42.462989
3504.832290	494277.856781	42.467994
3504.742594	494299.544262	42.472999
3504.196407	494264.133277	42.478004
3504.306373	494261.482831	42.483008
3504.527589	494245.446274	42.488013
3504.711566	494273.217774	42.493018
3504.522887	494245.548548	42.498023
3504.974608	494213.321881	42.503028
3504.510176	494237.600584	42.508032
3504.696163	494179.691530	42.513037
3504.580310	494154.593224	42.518042
3504.604750	494175.553869	42.523047
3504.310654	494195.957174	42.528052
3504.378550	494149.814823	42.533056
3504.352803	494188.152433	42.538061
3504.392381	494158.421459	42.543066
3504.817823	494132.579269	42.548071
3504.433828	494144.742730	42.553076
3504.132261	494126.003568	42.558080
3504.060331	494113.203465	42.563085
3504.560981	494125.429676	42.568090
3504.411814	494116.743519	42.573095
3504.515566	494078.089853	42.578100
3504.500969	494076.826316	42.583104
3504.262650	494111.754240	42.588109
3504.528668	494058.744117	42.593114
3504.568386	494077.373070	42.598119
3504.376798	494033.296993	42.603124
3504.454067	494075.770950	42.608128
3503.979460	494041.664834	42.613133
3504.412268	493991.413298	42.618138
3504.147800	494048.930489	42.623143
3504.018930	494049.862485	42.628148
3504.360560	494026.109589	42.633152
3504.543856	494001.925935	42.638157
3504.514239	494006.386979	42.643162
3504.267794	494018.933895	42.648167
3504.525138	493964.557619	42.653172
3504.610889	493997.966004	42.658176
3504.474147	493967.300447	42.663181
3504.438666	493980.016603	42.668186
3504.201210	493958.127512	42.673191
3504.486902	493939.649819	42.678196
3504.352341	493952.989324	42.683200
3504.398400	493907.761325	42.688205
3504.271152	493927.682801	42.693210
3503.991746	493897.444790	42.698215
3504.492620	493913.114581	42.703220
3504.295503	493912.740749	42.708224
3504.063300	493902.447156	42.713229
3504.271260	493922.265019	42.718234
3503.944521	493884.894331	42.723239
3504.674847	493878.398469	42.728244
3504.469717	493900.256580	42.733248
3504.606819	493859.014580	42.738253
3504.346813	493873.184199	42.743258
3504.488941	493833.156692	42.748263
3504.331522	493864.730088	42.753268
3504.482107	493840.905871	42.758272
3504.824437	493824.292772	42.763277
3504.478115	493836.146643	42.768282
3504.370972	493804.159511	42.773287
3504.669892	493776.361877	42.778292
3504.664206	493803.860222	42.783296
3504.313283	493781.685018	42.788301
3504.742839	493762.222257	42.793306
3504.280817	493774.651491	42.798311
3504.621344	493723.552939	42.803316
3504.469232	493764.747228	42.808321
3504.432749	493734.825035	42.813325
3504.902906	493709.987985	42.818330
3504.578591	493726.345394	42.823335
3504.505761	493699.771116	42.828340
3504.805394	493680.987123	42.833345
3504.592934	493681.780428	42.838349
3504.585350	493643.396651	42.843354
3504.579976	493694.392068	42.848359
3504.211524	493647.051430	42.853364
3504.879131	493610.687753	42.858369
3504.655268	493638.220826	42.863373
3504.622605	493627.743623	42.868378
3504.924955	493578.980150	42.873383
3504.435758	493617.442831	42.878388
3504.698192	493573.648381	42.883393
3504.745242	493554.043296	42.888397
3504.534507	493558.533074	42.893402
3504.390654	493527.918553	42.898407
3504.462438	493557.886395	42.903412
3504.504961	493515.493852	42.908417
3504.475888	493515.346653	42.913421
3504.696630	493531.567448	42.918426
3505.007405	493476.978735	42.923431
3504.535835	493476.749551	42.928436
3504.758314	493476.461313	42.933441
3504.372958	493464.824389	42.938445
3504.738019	493420.709516	42.943450
3504.425233	493442.939665	42.948455
3504.337050	493436.471734	42.953460
3504.505391	493390.159693	42.958465
3504.461708	493406.473030	42.963469
3504.697771	493372.354640	42.968474
3504.781499	493394.319615	42.973479
3504.531640	493356.530583	42.978484
3504.625130	493384.520283	42.983489
3504.533424	493331.665899	42.988493
3504.298261	493348.566600	42.993498
3504.938180	493301.166987	42.998503
3504.650865	493291.742662	43.003508
3504.858819	493314.093226	43.008513
3504.236494	493291.859048	43.013517
3504.484092	493268.018762	43.018522
3504.628905	493269.971003	43.023527
3504.208764	493263.099707	43.028532
3504.611631	493218.471967	43.033537
3504.493050	493264.371699	43.038541
3504.186850	493240.669546	43.043546
3504.461016	493221.990396	43.048551
3504.273414	493205.308576	43.053556
3504.169555	493222.593768	43.058561
3504.407096	493204.528084	43.063565
3504.322764	493218.721078	43.068570
3504.534533	493189.872876	43.073575
3504.515578	493164.302140	43.078580
3504.657778	493172.736895	43.083585
3504.434961	493165.885018	43.088589
3504.547538	493135.938300	43.093594
3504.291203	493133.193662	43.098599
3504.392447	493142.495808	43.103604
3504.610694	493128.433769	43.108609
3504.703335	493105.985084	43.113613
3504.561077	493098.816601	43.118618
3504.552185	493107.832322	43.123623
3504.483751	493096.043793	43.128628
3504.710020	493076.764369	43.133633
3504.444239	493068.146791	43.138637
3504.980958	493074.291007	43.143642
3504.883483	493032.071411	43.148647
3504.247531	493047.516478	43.153652
3504.556298	493024.982896	43.158657
3504.471947	492996.940821	43.163661
3504.247077	493006.446502	43.168666
3504.487886	492987.215329	43.173671
3504.503099	492979.262284	43.178676
3504.387502	492987.839151	43.183681
3504.136432	492948.732792	43.188685
3504.244419	492951.602441	43.193690
3504.382279	492977.965201	43.198695
3504.009583	492952.196873	43.203700
3504.227070	492949.377321	43.208705
3504.258201	492957.677802	43.213709
3504.005459	492957.059530	43.218714
3504.249490	492905.822053	43.223719
3504.133901	492939.618661	43.228724
3504.329783	492895.731848	43.233729
3503.980088	492933.515548	43.238733
3504.119577	492904.425117	43.243738
3504.236887	492930.386056	43.248743
3503.984006	492903.484599	43.253748
3504.060098	492921.248051	43.258753
3504.260243	492899.288546	43.263757
3504.118261	492880.978679	43.268762
3503.985887	492913.714502	43.273767
3504.038206	492877.294711	43.278772
3504.345249	492887.020237	43.283777
3503.873693	492910.744737	43.288781
3504.186911	492878.942780	43.293786
3504.095419	492899.568698	43.298791
3503.990788	492876.391284	43.303796
3504.125081	492904.375259	43.308801
3503.719293	492892.791847	43.313805
3503.942334	492865.156769	43.318810
3504.226370	492870.631998	43.323815
3503.795316	492880.929963	43.328820
3504.145575	492848.514394	43.333825
3504.195092	492856.710730	43.338829
3504.290444	492885.663090	43.343834
3504.206492	492858.279090	43.348839
3503.900935	492894.789839	43.353844
3504.200319	492860.609860	43.358849
3504.236659	492884.355405	43.363853
3504.393985	492862.301339	43.368858
3504.008623	492840.586230	43.373863
3504.392708	492814.951314	43.378868
3504.464893	492844.312538	43.383873
3504.063744	492857.239184	43.388877
3504.277678	492799.878467	43.393882
3504.474559	492827.650097	43.398887
3504.326054	492792.730506	43.403892
3504.556955	492765.803031	43.408897
3504.467144	492800.912520	43.413901
3504.366943	492806.347213	43.418906
3503.944660	492769.293228	43.423911
3504.296275	492741.131221	43.428916
3504.460868	492766.730418	43.433921
3503.841016	492777.969842	43.438925
3504.261845	492764.787073	43.443930
3504.342015	492762.495620	43.448935
3504.397230	492712.857369	43.453940
3504.301731	492730.091056	43.458945
3504.510915	492724.082303	43.463949
3504.462524	492751.943453	43.468954
3504.372454	492719.951753	43.473959
3504.315801	492713.022803	43.478964
3504.518869	492694.202433	43.483969
3504.840802	492668.121355	43.488973
3504.436830	492698.570919	43.493978
3504.507451	492655.868117	43.498983
3504.097397	492652.641276	43.503988
3504.834777	492612.111916	43.508993
3504.405264	492632.690268	43.513997
3504.471165	492642.555320	43.519002
3504.279753	492595.690445	43.524007
3504.319694	492610.826477	43.529012
3504.427753	492597.186594	43.534017
3504.339024	492575.778793	43.539021
3504.357837	492595.172184	43.544026
3504.337367	492563.067927	43.549031
3504.349871	492545.341028	43.554036
3504.693492	492581.648502	43.559041
3504.480097	492527.089202	43.564045
3504.461854	492546.488500	43.569050
3504.555761	492502.566234	43.574055
3504.325681	492525.645340	43.579060
3504.385354	492520.976872	43.584065
3504.472406	492502.579790	43.589069
3504.750412	492501.421830	43.594074
3504.544834	492487.375649	43.599079
3504.233901	492472.738390	43.604084
3504.212608	492471.526445	43.609089
3503.858985	492452.186097	43.614093
3504.107310	492458.781245	43.619098
3504.157630	492486.576548	43.624103
3503.898466	492455.320122	43.629108
3504.296292	492457.435034	43.634113
3504.119521	492481.113488	43.639117
3503.516221	492445.201618	43.644122
3504.148564	492444.595370	43.649127
3504.455817	492428.138500	43.654132
3504.156062	492462.167656	43.659137
3503.627102	492442.297934	43.664141
3504.179077	492403.873800	43.669146
3504.355814	492441.980442	43.674151
3503.503093	492442.723061	43.679156
3504.136779	492423.682430	43.684161
3504.208895	492439.269306	43.689165
3503.971915	492450.093910	43.694170
3504.435905	492411.886272	43.699175
3504.440222	492441.258859	43.704180
3504.391064	492398.371825	43.709185
3504.383769	492379.736315	43.714189
3503.901422	492403.412522	43.719194
3504.036661	492417.976571	43.724199
3504.114504	492392.085615	43.729204
3504.418859	492397.051339	43.734209
3504.294282	492357.417309	43.739213
3504.019014	492389.670203	43.744218
3504.036752	492384.198034	43.749223
3504.129423	492356.025728	43.754228
3504.258488	492383.099730	43.759233
3503.851042	492368.984078	43.764237
3504.446257	492371.017159	43.769242
3504.366169	492371.840240	43.774247
3503.798217	492353.647821	43.779252
3504.483934	492327.052978	43.784257
3504.169073	492353.690749	43.789261
3504.434701	492311.361485	43.794266
3504.220279	492347.301822	43.799271
3503.945314	492314.123201	43.804276
3504.123906	492307.156920	43.809281
3503.983330	492300.595587	43.814285
3504.537549	492271.387975	43.819290
3504.247398	492314.835620	43.824295
3504.002269	492299.529457	43.829300
3503.906500	492304.558446	43.834305
3504.250855	492303.795136	43.839309
3503.814378	492319.158634	43.844314
3504.082322	492290.350804	43.849319
3503.745032	492294.202518	43.854324
3503.833363	492256.205865	43.859329
3503.729712	492312.284988	43.864333
3504.027683	492297.905860	43.869338
3504.480666	492273.221541	43.874343
3504.150096	492287.707382	43.879348
3504.317940	492261.700732	43.884353
3504.533249	492278.581850	43.889357
3504.444903	492264.162466	43.894362
3504.440083	492276.469792	43.899367
3504.273674	492249.756298	43.904372
3504.410844	492229.223984	43.909377
3504.114690	492261.581688	43.914381
3504.000925	492228.276148	43.919386
3504.364898	492248.881444	43.924391
3504.147935	492211.084882	43.929396
3504.211800	492215.835445	43.934401
3503.892778	492199.578644	43.939405
3504.117890	492225.574172	43.944410
3504.389761	492198.386183	43.949415
3504.360576	492196.517096	43.954420
3504.485428	492209.158480	43.959425
3504.483982	492167.782692	43.964429
3504.172073	492193.103480	43.969434
3504.142811	492174.319306	43.974439
3504.159568	492154.565601	43.979444
3504.428822	492191.898472	43.984449
3504.287049	492127.856255	43.989453
3504.367370	492124.703749	43.994458
3503.984926	492151.555067	43.999463
3503.981943	492126.385533	44.004468
3504.384015	492129.006254	44.009473
3504.174485	492152.487727	44.014477
3504.330671	492126.482731	44.019482
3504.316312	492137.474908	44.024487
3503.776269	492114.213429	44.029492
3503.852067	492100.882148	44.034497
3504.391251	492083.729943	44.039501
3504.231732	492080.007606	44.044506
3504.517585	492084.621828	44.049511
3504.415399	492077.294684	44.054516
3504.199976	492085.735810	44.059521
3503.996290	492102.885886	44.064525
3504.010689	492080.397688	44.069530
3503.954677	492056.097394	44.074535
3504.484330	492040.769852	44.079540
3504.306872	492052.243657	44.084545
3504.032105	492090.675599	44.089549
3504.258857	492064.355499	44.094554
3503.936550	492042.984003	44.099559
3504.297482	492004.487953	44.104564
3504.432687	492005.226379	44.109569
3504.279366	492049.513972	44.114573
3504.062724	492031.417645	44.119578
3504.451155	492006.135443	44.124583
3504.365121	492035.522948	44.129588
3504.231527	491984.950356	44.134593
3504.242046	492004.295028	44.139597
3504.176653	492016.915965	44.144602
3503.962764	491975.725261	44.149607
3504.109792	492019.104499	44.154612
3504.111751	491995.909142	44.159617
3504.413188	491995.203248	44.164621
3503.732680	491993.639660	44.169626
3504.040704	491967.813024	44.174631
3504.399415	491945.928625	44.179636
3504.107908	491992.061402	44.184641
3503.988993	491995.574796	44.189645
3503.906398	491965.505109	44.194650
3504.499183	491945.356274	44.199655
3504.146049	492000.969317	44.204660
3504.404374	491976.011504	44.209665
3504.316897	491918.645070	44.214669
3504.142734	491945.311831	44.219674
3504.430755	491940.961640	44.224679
3504.049651	491936.767848	44.229684
3503.789674	491946.482196	44.234689
3504.225646	491910.354391	44.239693
3504.062189	491937.829787	44.244698
3503.925078	491917.188546	44.249703
3503.839681	491902.717771	44.254708
3504.169521	491898.715475	44.259713
3503.967324	491906.040406	44.264717
3503.939291	491896.118588	44.269722
3504.227075	491914.204057	44.274727
3504.366479	491878.933380	44.279732
3504.369409	491902.837390	44.284737
3504.178182	491926.974636	44.289741
3504.398535	491859.886228	44.294746
3504.912597	491888.368802	44.299751
3504.041802	491883.695300	44.304756
3504.283053	491853.067800	44.309761
3504.627245	491872.106648	44.314765
3503.910403	491846.745693	44.319770
3504.572045	491802.377534	44.324775
3504.097923	491834.409590	44.329780
3504.267245	491831.394904	44.334785
3504.601239	491803.436848	44.339789
3504.293256	491830.378148	44.344794
3504.451746	491802.143958	44.349799
3504.125728	491786.394353	44.354804
3504.366203	491795.421941	44.359809
3504.095771	491789.438047	44.364813
3504.047889	491764.173831	44.369818
3504.190401	491801.780740	44.374823
3504.432290	491755.047848	44.379828
3504.502709	491727.789724	44.384833
3504.148303	491729.821029	44.389837
3504.549348	491771.843918	44.394842
3504.740534	491763.457381	44.399847
3504.084572	491720.917920	44.404852
3504.451005	491687.332938	44.409857
3504.319244	491741.848211	44.414861
3504.367132	491741.790125	44.419866
3504.229370	491707.626480	44.424871
3504.209284	491682.509697	44.429876
3504.850589	491660.124491	44.434881
3504.828810	491653.341572	44.439885
3504.346760	491629.259994	44.444890
3504.620061	491666.137467	44.449895
3504.009174	491655.598606	44.454900
3504.724743	491625.402222	44.459905
3504.721408	491594.458438	44.464909
3504.632772	491625.265076	44.469914
3504.703604	491613.149725	44.474919
3504.119336	491579.309643	44.479924
3504.721524	491541.129030	44.484929
3504.474506	491550.132494	44.489933
3504.483843	491569.376511	44.494938
3504.707337	491561.238006	44.499943
3503.981286	491550.464058	44.504948
3504.396223	491514.034939	44.509953
3504.499933	491522.122005	44.514957
3504.047246	491546.908813	44.519962
3504.153314	491523.038021	44.524967
3504.017419	491495.508291	44.529972
3504.277631	491468.321084	44.534977
3504.366197	491457.722208	44.539981
3504.197082	491448.987308	44.544986
3504.236134	491459.161106	44.549991
3503.983890	491522.761687	44.554996
3504.075805	491518.442393	44.560001
3504.251181	491504.993658	44.565005
3504.249913	491480.380088	44.570010
3503.937910	491468.629025	44.575015
3503.950431	491465.385833	44.580020
3504.082912	491476.557774	44.585025
3504.187802	491486.012109	44.590029
3503.671135	491487.258751	44.595034
3504.117573	491454.825563	44.600039
3504.496168	491433.089360	44.605044
3504.290544	491432.362296	44.610049
3504.234757	491446.197605	44.615053
3504.117951	491410.561371	44.620058
3503.976155	491427.297116	44.625063
3504.002807	491392.549803	44.630068
3504.087197	491400.893205	44.635073
3504.061167	491444.706297	44.640077
3504.043048	491419.133035	44.645082
3504.212336	491402.291900	44.650087
3503.843666	491436.029939	44.655092
3503.525060	491427.977055	44.660097
3504.134953	491405.241987	44.665101
3504.207965	491408.117404	44.670106
3504.056224	491439.288845	44.675111
3504.041025	491390.367250	44.680116
3504.255943	491409.730878	44.685121
3503.997039	491416.558502	44.690125
3503.907616	491379.803667	44.695130
3503.940812	491401.373811	44.700135
3504.076320	491421.205793	44.705140
3503.940125	491401.070297	44.710145
3504.329609	491387.435699	44.715149
3504.369990	491378.566363	44.720154
3504.232722	491402.948987	44.725159
3504.158260	491398.402731	44.730164
3504.317233	491370.066521	44.735169
3504.278973	491339.684943	44.740173
3504.226572	491344.606042	44.745178
3504.410944	491385.651119	44.750183
3503.934315	491372.913092	44.755188
3503.977397	491348.596216	44.760193
3504.038991	491355.525146	44.765197
3503.845690	491361.987897	44.770202
3504.199975	491344.914887	44.775207
3504.267091	491354.831075	44.780212
3504.171003	491333.220426	44.785217
3504.439470	491301.726736	44.790221
3504.169149	491326.485013	44.795226
3504.272305	491336.040991	44.800231
3503.742869	491308.066722	44.805236
3504.588465	491267.567994	44.810241
3504.238722	491283.982207	44.815245
3504.272778	491321.911101	44.820250
3504.291359	491298.762898	44.825255
3503.755185	491302.443662	44.830260
3504.364535	491305.133033	44.835265
3504.312666	491282.755642	44.840269
3504.160317	491282.678555	44.845274
3504.216930	491283.277492	44.850279
3504.262143	491273.394413	44.855284
3504.176934	491263.683882	44.860289
3504.338892	491254.795272	44.865293
3504.653080	491214.583006	44.870298
3504.594753	491190.636479	44.875303
3504.175040	491188.170607	44.880308
3504.307871	491192.505356	44.885313
3504.690396	491205.815747	44.890317
3504.295987	491207.904077	44.895322
3504.112114	491207.021626	44.900327
3504.183798	491187.308865	44.905332
3504.542365	491148.608843	44.910337
3504.188216	491155.299675	44.915341
3504.325766	491177.714578	44.920346
3504.426492	491166.353914	44.925351
3503.708099	491150.919021	44.930356
3503.964229	491145.054283	44.935361
3503.987876	491141.353455	44.940365
3504.412842	491117.482391	44.945370
3504.430420	491109.730763	44.950375
3504.053806	491136.582614	44.955380
3504.114190	491127.051588	44.960385
3504.378673	491117.994769	44.965389
3504.121657	491101.777858	44.970394
3504.871710	491074.208779	44.975399
3504.425125	491109.934951	44.980404
3504.117754	491097.473866	44.985409
3504.731700	491073.015761	44.990413
3504.271208	491039.610962	44.995418
3504.408172	491014.974932	45.000423
3504.379695	491016.448328	45.005428
3504.235714	490999.909581	45.010433
3504.322137	490986.879710	45.015437
3504.511821	490986.444680	45.020442
3504.438088	491018.009671	45.025447
3504.256336	491021.482530	45.030452
3504.134808	491017.602034	45.035457
3504.228066	490974.030809	45.040461
3504.396005	490950.402745	45.045466
3504.473213	490960.165605	45.050471
3504.367925	490996.648408	45.055476
3504.384747	490984.997012	45.060481
3504.388600	490970.916589	45.065485
3504.306006	490968.599994	45.070490
3504.744874	490947.005645	45.075495
3504.344709	490890.951664	45.080500
3504.638052	490876.015056	45.085505
3504.710307	490861.113379	45.090509
3504.409029	490863.389616	45.095514
3503.993709	490863.100852	45.100519
3504.652782	490847.853180	45.105524
3504.691804	490829.056862	45.110529
3504.305167	490806.124039	45.115533
3504.245478	490808.210157	45.120538
3504.383852	490834.423920	45.125543
3504.164208	490846.107720	45.130548
3503.929980	490848.981134	45.135553
3504.020701	490849.625342	45.140557
3503.728839	490856.559673	45.145562
3504.140636	490858.318029	45.150567
3504.208365	490848.380521	45.155572
3504.224308	490841.844584	45.160577
3504.232475	490828.168553	45.165581
3504.254529	490814.895498	45.170586
3504.085941	490788.332203	45.175591
3504.431835	490777.033851	45.180596
3504.228125	490804.314678	45.185601
3504.110602	490810.765642	45.190605
3503.863833	490772.717645	45.195610
3504.141134	490737.929504	45.200615
3503.913455	490773.773661	45.205620
3504.014690	490778.670626	45.210625
3504.199557	490752.102064	45.215629
3503.566859	490768.308208	45.220634
3504.293337	490736.082759	45.225639
3504.285508	490739.072351	45.230644
3504.363373	490780.642065	45.235649
3504.002387	490763.630928	45.240653
3504.370691	490741.085186	45.245658
3504.137700	490742.084448	45.250663
3503.946057	490731.529448	45.255668
3503.813600	490722.129992	45.260673
3504.136673	490705.669110	45.265677
3504.205901	490695.984524	45.270682
3504.559657	490684.127745	45.275687
3504.088310	490732.773800	45.280692
3503.728304	490717.433848	45.285697
3504.356218	490680.007139	45.290701
3503.825305	490712.303325	45.295706
3503.881024	490703.532542	45.300711
3503.875933	490717.512320	45.305716
3503.820017	490716.407030	45.310721
3504.130063	490714.636123	45.315725
3503.698510	490720.022494	45.320730
3503.955150	490695.721667	45.325735
3503.661281	490679.206326	45.330740
3503.984551	490663.707690	45.335745
3503.747202	490655.540333	45.340749
3503.939365	490655.763330	45.345754
3504.478704	490656.032752	45.350759
3504.199135	490662.002896	45.355764
3504.081394	490655.538671	45.360769
3504.285206	490673.436020	45.365773
3503.977652	490716.130402	45.370778
3504.491351	490713.618236	45.375783
3504.158762	490702.781609	45.380788
3503.762138	490657.767636	45.385793
3504.228252	490635.256956	45.390797
3504.147751	490683.385532	45.395802
3503.897742	490662.862047	45.400807
3503.882029	490661.395862	45.405812
3503.871210	490668.285843	45.410817
3504.098398	490653.916643	45.415821
3503.890012	490700.900479	45.420826
3503.864936	490666.311940	45.425831
3504.049246	490677.172278	45.430836
3504.054166	490683.553285	45.435841
3503.983531	490646.084970	45.440845
3504.307121	490601.716755	45.445850
3504.692293	490580.738251	45.450855
3504.363202	490597.403041	45.455860
3504.340263	490588.593988	45.460865
3504.498391	490586.138003	45.465869
3504.047701	490618.624264	45.470874
3504.206416	490600.771117	45.475879
3503.584481	490588.055520	45.480884
3504.141103	490555.198178	45.485889
3504.100564	490551.608675	45.490893
3504.145105	490557.882166	45.495898
3504.073193	490552.626224	45.500903
3503.443713	490561.437367	45.505908
3503.890025	490586.589839	45.510913
3503.978715	490614.280564	45.515917
3503.611067	490625.025576	45.520922
3504.009731	490602.525517	45.525927
3504.231584	490563.440713	45.530932
3503.921427	490581.064843	45.535937
3503.596221	490610.137848	45.540941
3503.701276	490612.400542	45.545946
3504.201183	490575.905526	45.550951
3503.668335	490609.873590	45.555956
3503.787747	490625.707745	45.560961
3504.242586	490603.249457	45.565965
3503.968963	490609.674513	45.570970
3503.819189	490605.697099	45.575975
3503.846331	490603.008577	45.580980
3503.388865	490587.734571	45.585985
3503.427856	490595.477728	45.590989
3503.613827	490607.604051	45.595994
3504.383153	490611.382503	45.600999
3504.069859	490631.235606	45.606004
3503.899860	490644.025945	45.611009
3504.285961	490638.039212	45.616013
3504.112312	490617.250367	45.621018
3504.163360	490584.017148	45.626023
3503.483525	490575.767747	45.631028
3504.262928	490544.090736	45.636033
3504.102043	490568.934011	45.641037
3503.994895	490589.311709	45.646042
3504.163401	490599.516162	45.651047
3504.248318	490569.215165	45.656052
3504.064050	490566.408106	45.661057
3503.981674	490597.823224	45.666061
3503.697725	490577.001119	45.671066
3503.874798	490563.500793	45.676071
3504.492148	490555.958033	45.681076
3504.470635	490522.280338	45.686081
3504.275323	490513.498493	45.691085
3504.054242	490541.238284	45.696090
3504.323620	490532.332356	45.701095
3504.248939	490528.748244	45.706100
3503.557668	490518.272091	45.711105
3503.342779	490527.169669	45.716109
3503.012778	490555.939624	45.721114
3503.721106	490541.747536	45.726119
3504.033320	490518.400017	45.731124
3504.142505	490534.590404	45.736129
3504.287030	490523.728914	45.741133
3503.920240	490531.282989	45.746138
3504.289595	490528.591018	45.751143
3504.106697	490565.340168	45.756148
3503.793685	490531.151427	45.761153
3503.817548	490513.876644	45.766157
3504.390776	490487.398273	45.771162
3504.561962	490525.712292	45.776167
3504.326734	490535.777995	45.781172
3503.726432	490516.778520	45.786177
3504.270906	490507.373263	45.791181
3504.273647	490491.823849	45.796186
3504.455897	490473.004538	45.801191
3504.209362	490448.479027	45.806196
3504.071015	490457.465837	45.811201
3504.167698	490464.845389	45.816205
3504.406915	490462.528518	45.821210
3504.538959	490440.931434	45.826215
3503.712084	490459.295779	45.831220
3504.104356	490449.002873	45.836225
3504.321573	490460.465920	45.841229
3504.001633	490473.989155	45.846234
3504.334935	490469.783415	45.851239
3504.152831	490467.482487	45.856244
3504.151701	490469.154198	45.861249
3503.860537	490442.863030	45.866253
3503.693027	490438.635140	45.871258
3503.840487	490439.726233	45.876263
3503.642593	490452.521111	45.881268
3503.667082	490445.021361	45.886273
3504.383345	490415.025520	45.891277
3503.937443	490423.858361	45.896282
3504.188884	490408.066975	45.901287
3503.751068	490386.357299	45.906292
3503.715428	490381.652714	45.911297
3503.996195	490393.966788	45.916301
3504.094776	490435.685938	45.921306
3503.842357	490427.014376	45.926311
3504.302798	490388.499284	45.931316
3504.068604	490412.138780	45.936321
3504.179603	490428.734162	45.941325
3503.954275	490401.723449	45.946330
3503.990035	490437.070772	45.951335
3504.050486	490413.560319	45.956340
3504.267031	490427.302688	45.961345
3504.116985	490405.446255	45.966349
3503.943440	490390.177862	45.971354
3503.774016	490385.697018	45.976359
3503.957448	490360.039809	45.981364
3503.985014	490395.185909	45.986369
3504.025312	490406.626302	45.991373
3503.337589	490396.453413	45.996378
3503.413278	490380.132644	46.001383
3504.237770	490379.799864	46.006388
3504.243031	490376.203089	46.011393
3503.973371	490375.992592	46.016397
3503.529391	490382.545947	46.021402
3504.414297	490351.864917	46.026407
3504.224994	490351.641719	46.031412
3504.282043	490357.254863	46.036417
3504.580675	490358.271419	46.041421
3504.099548	490347.306116	46.046426
3504.014456	490324.173098	46.051431
3504.477802	490324.150642	46.056436
3503.790127	490334.085367	46.061441
3504.137117	490337.525433	46.066445
3503.823900	490353.478843	46.071450
3503.711658	490386.621098	46.076455
3503.686060	490375.533166	46.081460
3503.414113	490357.342663	46.086465
3504.235042	490336.548261	46.091469
3504.089572	490329.835062	46.096474
3504.046740	490365.042994	46.101479
3503.920596	490362.479963	46.106484
3504.089729	490340.826253	46.111489
3503.991312	490387.084406	46.116493
3503.507153	490363.052179	46.121498
3504.546817	490330.016803	46.126503
3503.878637	490363.398912	46.131508
3503.826225	490359.507355	46.136513
3504.284967	490307.165200	46.141517
3503.987518	490358.519787	46.146522
3504.015105	490337.496232	46.151527
3503.773925	490330.089073	46.156532
3504.256547	490305.903973	46.161537
3504.130359	490348.823770	46.166541
3504.152834	490320.406252	46.171546
3504.385176	490330.398166	46.176551
3503.872159	490331.796250	46.181556
3504.097855	490335.458084	46.186561
3504.402562	490344.932062	46.191565
3503.823896	490304.504421	46.196570
3503.501549	490281.307550	46.201575
3503.512872	490291.233118	46.206580
3503.696742	490304.018409	46.211585
3503.664281	490327.930021	46.216589
3503.829580	490320.914456	46.221594
3504.462769	490298.832810	46.226599
3504.108467	490279.895512	46.231604
3503.956920	490272.930007	46.236609
3503.855246	490288.799388	46.241613
3503.633901	490322.617438	46.246618
3503.683879	490318.760339	46.251623
3503.981218	490309.748588	46.256628
3503.876643	490299.736724	46.261633
3503.952125	490293.191186	46.266637
3503.301810	490288.786324	46.271642
3503.769369	490274.176247	46.276647
3504.126506	490261.609580	46.281652
3503.612678	490295.777801	46.286657
3503.844146	490322.230811	46.291661
3503.659421	490316.334195	46.296666
3503.668912	490312.635441	46.301671
3503.559893	490321.972225	46.306676
3504.383830	490317.435661	46.311681
3504.172582	490294.322545	46.316685
3503.942814	490285.394092	46.321690
3504.127770	490283.288372	46.326695
3504.040273	490318.047609	46.331700
3503.671760	490342.721403	46.336705
3503.967027	490329.911314	46.341709
3503.890113	490341.066379	46.346714
3504.058032	490338.912709	46.351719
3503.846079	490332.007422	46.356724
3503.843858	490323.346917	46.361729
3504.187367	490326.382343	46.366733
3503.925751	490339.845807	46.371738
3503.999504	490346.013453	46.376743
3503.760204	490352.787715	46.381748
3503.877076	490358.594000	46.386753
3504.058270	490348.942188	46.391757
3504.205165	490349.628184	46.396762
3504.261635	490333.411710	46.401767
3503.677411	490291.313501	46.406772
3503.560598	490287.229511	46.411777
3504.095817	490275.445094	46.416781
3504.227416	490265.243937	46.421786
3504.647412	490264.671191	46.426791
3504.236960	490296.746454	46.431796
3503.812698	490310.640838	46.436801
3504.137311	490290.583266	46.441805
3504.147960	490269.359715	46.446810
3504.295026	490247.709385	46.451815
3504.280434	490271.668894	46.456820
3504.122443	490277.619945	46.461825
3504.397176	490244.198824	46.466829
3503.600485	490247.110577	46.471834
3504.368584	490233.820499	46.476839
3503.815840	490272.705294	46.481844
3503.769803	490262.937404	46.486849
3503.855372	490251.831829	46.491853
3504.270569	490224.466380	46.496858
3504.236014	490239.565455	46.501863
3504.322095	490264.268801	46.506868
3503.815615	490228.641261	46.511873
3503.770695	490212.136811	46.516877
3504.353115	490185.605915	46.521882
3504.284923	490191.745397	46.526887
3504.525357	490236.785428	46.531892
3504.200376	490234.608350	46.536897
3504.180252	490212.072717	46.541901
3504.284024	490160.140802	46.546906
3504.506321	490177.782454	46.551911
3504.316106	490196.603573	46.556916
3503.904661	490165.215439	46.561921
3504.206680	490169.928881	46.566925
3503.995482	490201.618268	46.571930
3504.421852	490154.801586	46.576935
3504.205249	490156.203484	46.581940
3503.908128	490155.338880	46.586945
3504.066441	490131.154164	46.591949
3503.704314	490132.275166	46.596954
3503.608148	490129.707365	46.601959
3503.834454	490135.597722	46.606964
3503.728204	490136.323736	46.611969
3504.387108	490140.879480	46.616973
3504.052365	490153.493592	46.621978
3504.468905	490128.508318	46.626983
3504.521378	490125.917024	46.631988
3504.455093	490108.352219	46.636993
3504.237494	490080.985277	46.641997
3504.209973	490127.688709	46.647002
3504.058098	490097.880223	46.652007
3504.270184	490095.668896	46.657012
3504.248353	490124.289503	46.662017
3504.416570	490061.761368	46.667021
3504.345401	490038.980347	46.672026
3504.233511	490070.958156	46.677031
3504.381478	490089.573983	46.682036
3504.431401	490094.631186	46.687041
3504.440826	490077.155685	46.692045
3504.098918	490064.040925	46.697050
3504.321599	490053.977207	46.702055
3504.112506	490055.985722	46.707060
3504.210387	490036.318264	46.712065
3504.148013	490026.704783	46.717069
3504.188415	490008.971075	46.722074
3504.402287	489978.192896	46.727079
3504.401498	490010.254548	46.732084
3504.196722	489976.706141	46.737089
3504.254932	489977.406167	46.742093
3504.036353	490003.880105	46.747098
3504.082855	489977.534919	46.752103
3504.374638	489986.403322	46.757108
3503.748977	489959.151346	46.762113
3504.847435	489924.079968	46.767117
3504.394911	489930.330929	46.772122
3504.149730	489965.571589	46.777127
3504.104734	489932.149799	46.782132
3503.846969	489944.194733	46.787137
3504.116310	489915.788238	46.792141
3504.161153	489893.849758	46.797146
3504.115580	489933.212246	46.802151
3503.840673	489913.198378	46.807156
3504.073079	489903.538244	46.812161
3503.956578	489907.811398	46.817165
3504.295729	489894.740828	46.822170
3504.238529	489921.442626	46.827175
3504.276032	489911.256150	46.832180
3503.917911	489894.952874	46.837185
3504.174560	489880.730380	46.842189
3503.982802	489890.536306	46.847194
3504.601452	489847.588537	46.852199
3504.442422	489896.744541	46.857204
3504.293237	489856.551958	46.862209
3504.534383	489868.973940	46.867213
3504.310573	489834.617884	46.872218
3504.290144	489834.621240	46.877223
3504.142334	489838.392854	46.882228
3503.731671	489828.530418	46.887233
3504.586153	489809.249645	46.892237
3504.708377	489798.745815	46.897242
3504.529552	489763.724064	46.902247
3504.563045	489786.106424	46.907252
3504.208447	489806.726679	46.912257
3504.420435	489763.032584	46.917261
3504.636244	489723.643090	46.922266
3504.419510	489730.920514	46.927271
3504.256222	489777.696921	46.932276
3504.386473	489760.708536	46.937281
3504.058355	489727.331130	46.942285
3503.543354	489724.171012	46.947290
3504.118403	489687.358498	46.952295
3504.450579	489693.688118	46.957300
3504.296246	489722.482229	46.962305
3504.216560	489736.575827	46.967309
3503.889636	489712.112711	46.972314
3504.267500	489688.956393	46.977319
3504.326873	489725.111731	46.982324
3504.375198	489716.189705	46.987329
3504.409747	489694.708476	46.992333
3503.992061	489675.932540	46.997338
3504.501379	489638.421208	47.002343
3504.271715	489668.442929	47.007348
3503.836847	489681.377085	47.012353
3503.794886	489640.204730	47.017357
3504.202247	489608.939510	47.022362
3503.756906	489641.527910	47.027367
3503.685423	489652.024062	47.032372
3503.907141	489627.018265	47.037377
3504.212583	489600.682278	47.042381
3504.160510	489614.568998	47.047386
3503.603954	489632.739467	47.052391
3503.748119	489639.453376	47.057396
3503.504207	489646.279270	47.062401
3503.728592	489647.510204	47.067405
3503.807020	489668.669981	47.072410
3503.877733	489664.302963	47.077415
3503.673561	489670.210852	47.082420
3503.991790	489672.439969	47.087425
3504.307919	489668.388719	47.092429
3503.771455	489669.993159	47.097434
3503.535997	489645.718104	47.102439
3503.758371	489631.703443	47.107444
3503.392525	489642.246125	47.112449
3503.997874	489643.416848	47.117453
3504.042243	489617.780608	47.122458
3504.045979	489658.756705	47.127463
3503.620569	489679.438942	47.132468
3503.648678	489655.730053	47.137473
3504.367674	489624.111699	47.142477
3504.170844	489623.940332	47.147482
3504.273997	489613.945923	47.152487
3504.528692	489608.992653	47.157492
3504.043779	489621.428250	47.162497
3504.274314	489648.034308	47.167501
3503.973285	489651.830176	47.172506
3504.308188	489625.641519	47.177511
3503.866752	489614.466910	47.182516
3504.193616	489592.888714	47.187521
3503.947674	489592.066645	47.192525
3504.126424	489641.625786	47.197530
3503.688581	489625.638783	47.202535
3503.902524	489606.104485	47.207540
3504.114834	489573.907667	47.212545
3504.393409	489576.295016	47.217549
3504.002638	489583.600002	47.222554
3503.858668	489617.508389	47.227559
3503.620272	489596.424744	47.232564
3503.420537	489592.455011	47.237569
3504.147521	489576.486468	47.242573
3503.932653	489637.706916	47.247578
3503.795168	489621.419183	47.252583
3503.568204	489610.767834	47.257588
3503.764611	489611.496684	47.262593
3504.271100	489599.716387	47.267597
3503.986182	489601.179773	47.272602
3504.430628	489585.002638	47.277607
3504.373765	489569.563185	47.282612
3503.962551	489566.842496	47.287617
3504.307571	489551.187557	47.292621
3504.272484	489558.892197	47.297626
3504.225761	489557.734734	47.302631
3504.268998	489545.166552	47.307636
3503.651694	489567.702680	47.312641
3503.928521	489562.644599	47.317645
3503.667609	489575.044823	47.322650
3503.883675	489572.478248	47.327655
3503.907101	489557.127397	47.332660
3503.449620	489542.511006	47.337665
3503.708940	489518.562797	47.342669
3504.081630	489546.767368	47.347674
3503.887784	489559.106352	47.352679
3503.506765	489563.623995	47.357684
3503.631133	489601.592736	47.362689
3503.758208	489615.907000	47.367693
3503.665489	489613.794442	47.372698
3504.368113	489582.381210	47.377703
3504.542462	489593.193098	47.382708
3504.001628	489583.756314	47.387713
3504.279437	489538.734371	47.392717
3504.154729	489568.689011	47.397722
3504.160964	489588.847266	47.402727
3504.478324	489585.454267	47.407732
3504.146407	489566.664665	47.412737
3504.203228	489536.670355	47.417741
3503.903404	489517.824981	47.422746
3504.674041	489501.950779	47.427751
3504.346617	489504.737822	47.432756
3504.401834	489503.665547	47.437761
3504.063612	489475.506369	47.442765
3503.752966	489469.274830	47.447770
3503.906308	489482.268109	47.452775
3503.899856	489480.648415	47.457780
3503.998865	489456.117648	47.462785
3504.322272	489451.761294	47.467789
3504.008780	489458.041087	47.472794
3504.054039	489449.980493	47.477799
3504.361206	489446.892989	47.482804
3504.300231	489471.114103	47.487809
3503.957707	489472.181393	47.492813
3503.727469	489472.167258	47.497818
3504.017585	489481.036163	47.502823
3503.930369	489475.630385	47.507828
3503.965586	489480.892682	47.512833
3504.122868	489476.562590	47.517837
3503.639886	489449.489930	47.522842
3504.008779	489443.708147	47.527847
3504.406473	489422.675727	47.532852
3504.016581	489431.804085	47.537857
3504.205976	489439.371992	47.542861
3504.013928	489418.078216	47.547866
3503.921877	489414.952501	47.552871
3504.034575	489417.619344	47.557876
3504.239884	489414.953146	47.562881
3504.411414	489400.389183	47.567885
3504.327636	489392.298307	47.572890
3504.119255	489375.565703	47.577895
3504.068772	489393.352506	47.582900
3504.021473	489402.528035	47.587905
3503.776420	489392.791149	47.592909
3504.031761	489388.749447	47.597914
3504.079805	489399.176197	47.602919
3504.008403	489424.057489	47.607924
3503.657231	489460.936689	47.612929
3504.144547	489430.266353	47.617933
3503.674500	489405.673507	47.622938
3504.104145	489387.320527	47.627943
3503.992710	489397.164665	47.632948
3503.535829	489402.454109	47.637953
3503.348514	489380.298467	47.642957
3504.401775	489375.218923	47.647962
3503.830879	489380.425090	47.652967
3503.708671	489389.561812	47.657972
3503.988992	489432.824656	47.662977
3503.876226	489401.793254	47.667981
3503.718940	489378.923744	47.672986
3503.309334	489400.262258	47.677991
3504.248438	489392.161670	47.682996
3503.790661	489389.347011	47.688001
3503.899442	489426.964006	47.693005
3504.158781	489435.787145	47.698010
3503.937400	489416.676015	47.703015
3503.774908	489390.970859	47.708020
3503.373203	489382.676970	47.713025
3503.388397	489403.137916	47.718029
3503.545675	489440.443311	47.723034
3503.982269	489454.455520	47.728039
3504.150784	489440.044019	47.733044
3503.523874	489461.366158	47.738049
3503.837145	489454.073628	47.743053
3503.523121	489440.346209	47.748058
3503.222493	489430.922035	47.753063
3504.028723	489405.266397	47.758068
3503.593705	489459.431006	47.763073
3503.861591	489453.411933	47.768077
3503.276730	489442.563798	47.773082
3503.816642	489417.355479	47.778087
3504.095092	489463.455030	47.783092
3503.933517	489477.359158	47.788097
3503.730191	489471.262612	47.793101
3503.883979	489452.041571	47.798106
3503.789223	489444.813526	47.803111
3503.851705	489469.319038	47.808116
3504.079842	489481.895285	47.813121
3503.968075	489450.610549	47.818125
3503.988725	489460.281824	47.823130
3504.135562	489457.270314	47.828135
3504.371741	489463.969743	47.833140
3503.708843	489457.186057	47.838145
3504.101206	489429.721764	47.843149
3504.661426	489422.947357	47.848154
3504.163560	489407.070957	47.853159
3503.969028	489407.203134	47.858164
3503.467728	489453.932463	47.863169
3504.020531	489441.992795	47.868173
3504.033979	489448.068964	47.873178
3503.676734	489448.733371	47.878183
3503.946899	489410.246357	47.883188
3504.125912	489379.928576	47.888193
3503.962903	489394.744720	47.893197
3503.613853	489429.040418	47.898202
3503.864893	489426.468297	47.903207
3503.968124	489439.064314	47.908212
3503.531281	489429.762971	47.913217
3503.993341	489402.034364	47.918221
3503.729893	489389.261293	47.923226
3503.650287	489438.557892	47.928231
3504.256101	489433.346476	47.933236
3503.589563	489430.818076	47.938241
3504.491237	489399.322429	47.943245
3504.009797	489442.452390	47.948250
3503.565216	489430.366443	47.953255
3504.278433	489404.978762	47.958260
3503.982602	489401.530692	47.963265
3504.351636	489393.013689	47.968269
3503.998988	489399.958160	47.973274
3503.884155	489423.782634	47.978279
3504.174893	489410.263519	47.983284
3504.202300	489401.496605	47.988289
3503.888416	489404.585432	47.993293
3503.466798	489407.539332	47.998298
3503.403546	489409.980728	48.003303
3503.755121	489409.621379	48.008308
3503.866470	489405.501137	48.013313
3503.775048	489403.945517	48.018317
3504.061560	489408.813556	48.023322
3503.201450	489400.592126	48.028327
3503.313317	489408.932071	48.033332
3503.868692	489427.788069	48.038337
3504.143435	489410.118063	48.043341
3503.990469	489458.919688	48.048346
3503.867621	489436.855227	48.053351
3504.560032	489386.854205	48.058356
3504.133359	489379.172079	48.063361
3504.106312	489415.696230	48.068365
3504.053980	489385.820235	48.073370
3503.894879	489409.854330	48.078375
3504.284375	489396.826111	48.083380
3504.173304	489414.318561	48.088385
3503.826174	489405.965405	48.093389
3503.906610	489403.268290	48.098394
3504.078444	489380.042853	48.103399
3504.091790	489400.149534	48.108404
3503.285903	489386.094602	48.113409
3504.335099	489361.312232	48.118413
3503.920869	489393.440277	48.123418
3503.789673	489373.301819	48.128423
3504.003062	489376.054057	48.133428
3503.659955	489384.313967	48.138433
3504.065282	489353.605814	48.143437
3504.108944	489398.425689	48.148442
3503.844713	489372.331376	48.153447
3504.583911	489353.625529	48.158452
3504.214120	489403.575902	48.163457
3504.260136	489378.597547	48.168461
3504.606473	489348.962393	48.173466
3504.096610	489362.617743	48.178471
3503.604076	489339.294654	48.183476
3504.072609	489327.621491	48.188481
3504.181449	489307.748935	48.193485
3504.261411	489301.354301	48.198490
3504.222995	489321.671853	48.203495
3504.203193	489351.002437	48.208500
3504.263974	489315.638075	48.213505
3504.017062	489330.163619	48.218509
3504.165825	489329.279155	48.223514
3504.059063	489308.073080	48.228519
3504.149690	489325.888295	48.233524
3504.067252	489328.383386	48.238529
3504.050285	489322.510596	48.243533
3504.286403	489326.778801	48.248538
3503.834997	489306.741532	48.253543
3503.869665	489291.388689	48.258548
3504.354761	489276.065946	48.263553
3504.308319	489262.498713	48.268557
3504.307401	489299.170915	48.273562
3503.911405	489298.625808	48.278567
3504.019497	489284.932863	48.283572
3503.914837	489275.680246	48.288577
3504.191246	489258.009834	48.293581
3503.222914	489264.899708	48.298586
3504.261544	489242.246232	48.303591
3504.258337	489255.264410	48.308596
3504.286032	489291.476237	48.313601
3504.200927	489267.734102	48.318605
3504.386679	489226.575507	48.323610
3504.385878	489209.455384	48.328615
3504.408627	489258.837577	48.333620
3503.867787	489239.320891	48.338625
3504.487096	489218.709087	48.343629
3504.123081	489209.446776	48.348634
3504.078052	489230.322644	48.353639
3504.277096	489194.885551	48.358644
3504.141828	489171.455136	48.363649
3504.137570	489211.926944	48.368653
3503.949175	489195.191021	48.373658
3504.343872	489173.652279	48.378663
3504.359588	489157.998410	48.383668
3503.842592	489147.139378	48.388673
3504.351522	489158.151895	48.393677
3504.032013	489159.671434	48.398682
3504.276266	489133.952294	48.403687
3504.503881	489142.274063	48.408692
3504.150903	489181.889310	48.413697
3503.954991	489147.527594	48.418701
3503.755127	489128.615380	48.423706
3504.032377	489114.085141	48.428711
3503.954650	489144.134332	48.433716
3503.965837	489108.220246	48.438721
3504.148244	489119.436351	48.443725
3504.415072	489090.421186	48.448730
3503.883400	489121.352598	48.453735
3504.042201	489122.290019	48.458740
3503.643434	489091.252659	48.463745
3503.902215	489116.689997	48.468749
3504.250545	489115.571373	48.473754
3504.409578	489103.541771	48.478759
3504.403715	489106.075440	48.483764
3503.783916	489100.855034	48.488769
3503.838897	489080.585534	48.493773
3504.190258	489072.982923	48.498778
3503.823234	489068.279733	48.503783
3504.047158	489087.239112	48.508788
3504.133291	489056.986146	48.513793
3504.131246	489091.582178	48.518797
3503.957405	489082.441705	48.523802
3504.174379	489049.483472	48.528807
3503.865899	489096.740384	48.533812
3503.883515	489080.731584	48.538817
3504.345272	489088.155280	48.543821
3504.420776	489072.745153	48.548826
3503.968290	489038.575747	48.553831
3504.107444	489023.864655	48.558836
3504.017968	489050.268870	48.563841
3504.153049	489019.653542	48.568845
3504.164928	489019.905054	48.573850
3504.076675	489063.378954	48.578855
3503.931811	489034.935297	48.583860
3503.992207	489027.277351	48.588865
3504.043458	489060.598703	48.593869
3504.010311	489018.055984	48.598874
3503.772808	489046.712312	48.603879
3503.728036	489004.120746	48.608884
3503.976219	489045.616715	48.613889
3503.962632	488999.930411	48.618893
3503.816506	489036.474114	48.623898
3503.942801	489002.770344	48.628903
3504.337944	488982.446976	48.633908
3503.933913	489018.676907	48.638913
3504.327402	489000.227963	48.643917
3504.114754	488998.792774	48.648922
3503.990961	488988.884557	48.653927
3504.223761	489021.518800	48.658932
3504.208288	488990.673957	48.663937
3503.957322	489008.188892	48.668941
3503.539563	488993.312534	48.673946
3503.861141	488974.064488	48.678951
3504.345485	489006.557695	48.683956
3503.564232	488985.457861	48.688961
3503.676964	488967.255869	48.693965
3503.699435	488967.860277	48.698970
3504.115990	488956.093797	48.703975
3504.177601	488981.917048	48.708980
3503.556334	488965.046726	48.713985
3503.894868	488964.892043	48.718989
3503.711962	488991.564370	48.723994
3503.303870	488980.333461	48.728999
3503.987009	488967.714411	48.734004
3503.898034	489026.789527	48.739009
3503.835435	489001.118705	48.744013
3504.094526	489022.301304	48.749018
3503.877837	488985.359298	48.754023
3504.028976	488986.551200	48.759028
3503.568641	488981.305557	48.764033
3504.066302	488975.959154	48.769037
3503.664913	489008.187128	48.774042
3503.699100	488972.117190	48.779047
3503.900497	488987.990416	48.784052
3503.835144	488964.599348	48.789057
3503.979728	488996.538439	48.794061
3503.842702	488963.787965	48.799066
3504.046360	488988.221134	48.804071
3504.263768	488968.483021	48.809076
3503.938432	488996.494822	48.814081
3504.190292	488972.496449	48.819085
3504.020602	489001.851264	48.824090
3503.388673	488992.935106	48.829095
3504.202817	488978.623822	48.834100
3503.994535	489003.375343	48.839105
3503.878700	488974.471134	48.844109
3503.785854	488989.580421	48.849114
3503.947539	488996.241138	48.854119
3504.153680	488979.695930	48.859124
3503.823257	489004.061533	48.864129
3504.066561	488958.334527	48.869133
3504.629598	489003.427820	48.874138
3504.009647	488965.637764	48.879143
3504.536703	488927.109167	48.884148
3504.054597	488969.987044	48.889153
3504.164061	488940.338037	48.894157
3504.358298	488969.584730	48.899162
3503.870758	488947.526684	48.904167
3504.723504	488901.855177	48.909172
3503.950629	488933.027629	48.914177
3504.537774	488894.286857	48.919181
3504.440262	488917.096174	48.924186
3504.031752	488919.744160	48.929191
3503.950799	488894.126746	48.934196
3504.412643	488873.032926	48.939201
3503.675250	488881.355371	48.944205
3504.192983	488854.427611	48.949210
3504.061430	488890.969292	48.954215
3503.899711	488862.831957	48.959220
3504.082753	488873.085701	48.964225
3503.912270	488873.366038	48.969229
3504.000594	488846.100912	48.974234
3504.274301	488889.923226	48.979239
3504.141077	488855.196501	48.984244
3504.159312	488844.556618	48.989249
3503.618239	488872.704005	48.994253
3503.763249	488860.473854	48.999258
3503.734157	488841.433056	49.004263
3504.360609	488827.657854	49.009268
3503.908252	488822.309600	49.014273
3503.937469	488862.523599	49.019277
3503.723933	488836.572492	49.024282
3504.097634	488819.088907	49.029287
3503.988856	488825.539165	49.034292
3503.897093	488874.332624	49.039297
3504.002368	488847.875268	49.044301
3504.142673	488812.497397	49.049306
3503.626084	488826.255500	49.054311
3503.865271	488861.826886	49.059316
3503.934288	488829.752756	49.064321
3503.964785	488857.303299	49.069325
3503.809832	488854.238085	49.074330
3503.945432	488822.204072	49.079335
3504.154105	488805.607659	49.084340
3503.840508	488821.511767	49.089345
3503.836738	488866.289746	49.094349
3503.767269	488850.395822	49.099354
3504.217473	488835.584769	49.104359
3504.336164	488865.755317	49.109364
3504.179034	488800.387212	49.114369
3504.173125	488814.976367	49.119373
3504.387278	488824.769342	49.124378
3504.172621	488801.148404	49.129383
3504.188266	488800.740834	49.134388
3503.834303	488821.665979	49.139393
3504.030967	488792.357530	49.144397
3503.816374	488803.332649	49.149402
3504.146523	488839.852109	49.154407
3503.867135	488801.400063	49.159412
3503.673150	488776.104273	49.164417
3504.237532	488788.881104	49.169421
3504.185222	488804.389357	49.174426
3503.623513	488799.463604	49.179431
3503.778282	488780.646952	49.184436
3503.832996	488794.213477	49.189441
3503.531498	488780.432945	49.194445
3504.027355	488776.555713	49.199450
3504.181962	488776.278139	49.204455
3504.195213	488767.513169	49.209460
3503.800461	488769.500508	49.214465
3504.593155	488742.275867	49.219469
3504.345799	488727.828246	49.224474
3504.052434	488757.861479	49.229479
3504.099142	488749.496438	49.234484
3503.878909	488724.863221	49.239489
3503.965079	488753.215569	49.244493
3503.965577	488756.204159	49.249498
3503.313355	488744.606468	49.254503
3504.259282	488723.638585	49.259508
3503.991624	488756.352383	49.264513
3503.782112	488740.075274	49.269517
3504.254884	488717.561262	49.274522
3503.975732	488758.229447	49.279527
3504.070439	488715.615188	49.284532
3504.035568	488757.055220	49.289537
3503.850145	488757.895105	49.294541
3503.728330	488749.404740	49.299546
3503.763624	488736.887930	49.304551
3504.555960	488732.913177	49.309556
3504.018906	488758.122207	49.314561
3504.164864	488726.795541	49.319565
3504.287016	488731.537773	49.324570
3504.185164	488731.908572	49.329575
3503.888347	488697.156759	49.334580
3503.860524	488697.009324	49.339585
3504.030399	488724.689990	49.344589
3503.764585	488712.980555	49.349594
3503.584817	488723.544989	49.354599
3503.986178	488713.351013	49.359604
3504.066174	488699.966007	49.364609
3504.426333	488676.507330	49.369613
3504.388687	488688.720886	49.374618
3504.099788	488730.910272	49.379623
3504.115111	488699.452247	49.384628
3504.102544	488672.405431	49.389633
3503.723876	488696.069906	49.394637
3503.852406	488674.116784	49.399642
3503.705797	488717.702007	49.404647
3503.849310	488698.279212	49.409652
3503.729000	488687.509179	49.414657
3504.020767	488668.012267	49.419661
3504.086471	488709.081934	49.424666
3503.578055	488691.535037	49.429671
3504.436895	488671.948504	49.434676
3503.797507	488702.087168	49.439681
3504.234674	488679.274817	49.444685
3503.898519	488678.264352	49.449690
3503.635698	488701.758550	49.454695
3503.709938	488678.800946	49.459700
3504.051951	488685.990459	49.464705
3503.745822	488712.024160	49.469709
3503.683427	488684.782624	49.474714
3503.992499	488664.928400	49.479719
3503.729932	488693.082689	49.484724
3503.960707	488689.044722	49.489729
3504.274257	488690.160321	49.494733
3503.896114	488690.321521	49.499738
3504.091682	488679.704172	49.504743
3504.010979	488687.770950	49.509748
3503.763801	488695.762729	49.514753
3503.630272	488710.068215	49.519757
3503.602881	488677.097303	49.524762
3503.936741	488707.993897	49.529767
3503.553390	488699.646152	49.534772
3504.098123	488691.101066	49.539777
3503.815485	488700.466090	49.544781
3504.150218	488688.408456	49.549786
3503.827798	488709.480699	49.554791
3503.810073	488687.094828	49.559796
3503.881347	488731.709304	49.564801
3503.821276	488707.253364	49.569805
3504.270529	488679.373766	49.574810
3503.633981	488732.964462	49.579815
3504.243787	488715.392812	49.584820
3504.091896	488666.688362	49.589825
3503.980610	488676.938078	49.594829
3503.981973	488660.323650	49.599834
3503.946492	488685.656116	49.604839
3504.290160	488650.600376	49.609844
3504.300323	488671.113562	49.614849
3503.965661	488659.009746	49.619853
3504.549316	488683.585865	49.624858
3504.225530	488651.218942	49.629863
3504.041325	488650.842954	49.634868
3504.351460	488612.348003	49.639873
3504.279459	488636.875848	49.644877
3504.406855	488622.318264	49.649882
3503.841470	488642.517218	49.654887
3504.365774	488605.001473	49.659892
3504.261689	488632.725574	49.664897
3503.529737	488583.606054	49.669901
3504.138903	488575.202693	49.674906
3503.868027	488583.147611	49.679911
3504.132848	488583.663074	49.684916
3503.710356	488590.466918	49.689921
3504.153985	488554.078204	49.694925
3504.456054	488544.203753	49.699930
3503.812696	488557.019665	49.704935
3503.979525	488597.516398	49.709940
3503.751781	488586.155443	49.714945
3504.105813	488561.887134	49.719949
3504.044575	488597.861075	49.724954
3503.373180	488588.191157	49.729959
3504.347848	488555.213619	49.734964
3504.157676	488603.618097	49.739969
3503.717159	488586.009718	49.744973
3504.463615	488587.208863	49.749978
3503.811570	488584.171517	49.754983
3504.069600	488543.253284	49.759988
3504.033756	488553.997680	49.764993
3504.067166	488568.935386	49.769997
3504.093043	488539.147001	49.775002
3504.152997	488548.559261	49.780007
3504.128711	488552.514222	49.785012
3504.127445	488541.775944	49.790017
3503.844852	488559.904138	49.795021
3504.400983	488528.411009	49.800026
3503.877768	488554.732505	49.805031
3503.606008	488503.463239	49.810036
3503.754757	488534.136103	49.815041
3503.832557	488506.416268	49.820045
3503.682363	488538.402721	49.825050
3503.581676	488566.025074	49.830055
3503.419544	488543.560550	49.835060
3503.877439	488542.323269	49.840065
3503.721051	488580.541048	49.845069
3504.011271	488540.681449	49.850074
3503.976415	488575.790146	49.855079
3503.357824	488561.806303	49.860084
3504.546998	488534.974584	49.865089
3504.077584	488584.486976	49.870093
3504.221136	488562.480697	49.875098
3504.210480	488517.400612	49.880103
3504.117193	488475.777951	49.885108
3504.220210	488520.235946	49.890113
3504.159888	488542.837219	49.895117
3503.929077	488512.785440	49.900122
3503.826088	488488.386654	49.905127
3503.832139	488488.639095	49.910132
3504.117477	488509.159618	49.915137
3504.163564	488542.735967	49.920141
3504.099803	488528.917676	49.925146
3503.734780	488504.155095	49.930151
3504.580058	488500.070620	49.935156
3504.023273	488517.330419	49.940161
3503.956804	488507.615505	49.945165
3504.400516	488491.285594	49.950170
3503.690496	488482.736113	49.955175
3503.850268	488480.938099	49.960180
3504.432671	488466.409789	49.965185
3504.084820	488480.597359	49.970189
3504.131243	488492.848407	49.975194
3503.830498	488457.742199	49.980199
3504.213325	488466.799544	49.985204
3503.768972	488458.157410	49.990209
3503.935026	488455.041396	49.995213
3504.379165	488421.033087	50.000218
3503.768654	488438.959953	50.005223
3503.740529	488453.147664	50.010228
3504.144023	488449.183657	50.015233
3504.099167	488433.842687	50.020237
3504.347135	488454.217214	50.025242
3503.895170	488432.507523	50.030247
3504.529977	488460.317709	50.035252
3504.107714	488441.541267	50.040257
3503.789412	488407.805401	50.045261
3504.168316	488413.976104	50.050266
3504.161169	488403.947836	50.055271
3503.353674	488415.675392	50.060276
3503.672084	488423.932473	50.065281
3503.509465	488409.775142	50.070285
3504.215223	488415.235681	50.075290
3503.913052	488437.166146	50.080295
3503.805524	488403.244997	50.085300
3504.603850	488380.729787	50.090305
3503.690772	488430.059431	50.095309
3503.789908	488407.857377	50.100314
3504.316405	488405.494853	50.105319
3504.032080	488423.724758	50.110324
3504.257959	488393.043414	50.115329
3504.211395	488414.984160	50.120333
3504.071784	488403.811782	50.125338
3503.843668	488408.153568	50.130343
3504.288401	488363.153105	50.135348
3503.945789	488387.065537	50.140353
3503.857392	488408.050473	50.145357
3503.591430	488395.935631	50.150362
3503.486872	488386.530600	50.155367
3503.493874	488352.540604	50.160372
3503.626168	488423.283771	50.165377
3503.458977	488399.654831	50.170381
3503.698950	488426.463733	50.175386
3503.893109	488406.627402	50.180391
3504.008422	488441.915229	50.185396
3503.773417	488410.648253	50.190401
3504.057069	488399.662246	50.195405
3504.156312	488434.699356	50.200410
3503.762248	488408.522925	50.205415
3503.918083	488429.722507	50.210420
3503.758027	488429.342698	50.215425
3503.789573	488397.273759	50.220429
3504.125062	488415.608327	50.225434
3503.620334	488448.613395	50.230439
3504.027943	488410.659824	50.235444
3503.913180	488392.746508	50.240449
3503.713883	488434.162579	50.245453
3503.901812	488434.487582	50.250458
3504.154927	488407.955593	50.255463
3504.152017	488421.784763	50.260468
3503.843868	488390.326697	50.265473
3504.125705	488359.383183	50.270477
3503.836161	488379.842744	50.275482
3503.845743	488360.238154	50.280487
3503.844740	488383.792673	50.285492
3504.251156	488363.416208	50.290497
3504.029388	488399.770475	50.295501
3504.200140	488383.230341	50.300506
3503.973650	488383.215611	50.305511
3503.829732	488382.985214	50.310516
3503.500934	488397.321797	50.315521
3504.118942	488376.152090	50.320525
3504.443818	488402.998260	50.325530
3503.899125	488387.432327	50.330535
3504.038747	488372.011497	50.335540
3503.874126	488352.687704	50.340545
3503.831505	488356.037752	50.345549
3504.428105	488318.104780	50.350554
3503.712007	488369.227008	50.355559
3503.652881	488353.432341	50.360564
3504.019075	488334.075287	50.365569
3503.611978	488378.107695	50.370573
3503.872196	488341.443638	50.375578
3504.105609	488354.222419	50.380583
3503.732235	488366.084010	50.385588
3503.544145	488354.564685	50.390593
3503.993129	488334.029497	50.395597
3504.135266	488358.321240	50.400602
3503.948839	488341.128362	50.405607
3504.106551	488370.837641	50.410612
3504.137716	488351.330940	50.415617
3503.903051	488350.456378	50.420621
3504.179458	488366.216961	50.425626
3504.319518	488355.810821	50.430631
3504.194162	488351.423836	50.435636
3504.199657	488347.472057	50.440641
3504.607221	488321.574043	50.445645
3504.446610	488310.050348	50.450650
3504.206059	488331.971196	50.455655
3504.086340	488311.475213	50.460660
3504.030802	488299.073780	50.465665
3503.789563	488283.561110	50.470669
3503.813598	488291.256921	50.475674
3503.672169	488287.885550	50.480679
3503.683826	488270.813265	50.485684
3503.820757	488318.761534	50.490689
3504.065251	488302.766874	50.495693
3503.714264	488299.631244	50.500698
3503.783232	488300.430942	50.505703
3504.158670	488287.252223	50.510708
3504.083450	488313.503247	50.515713
3503.350459	488288.038724	50.520717
3504.038907	488249.078009	50.525722
3503.651764	488305.771074	50.530727
3503.468387	488281.435383	50.535732
3503.999851	488257.037333	50.540737
3503.389252	488264.377568	50.545741
3503.466563	488198.919682	50.550746
3503.473929	488159.965121	50.555751
3503.762752	488125.372974	50.560756
3503.891876	488019.888852	50.565761
3503.157726	487972.844960	50.570765
3503.485309	487843.571130	50.575770
3503.429396	487782.539912	50.580775
3502.792986	487646.072005	50.585780
3503.176820	487505.997221	50.590785
3502.675314	487419.960249	50.595789
3502.616540	487273.064385	50.600794
3502.485544	487098.722379	50.605799
3502.052966	486950.515358	50.610804
3501.915410	486815.127797	50.615809
3501.423037	486639.572260	50.620813
3501.451191	486470.721191	50.625818
3501.246418	486299.676420	50.630823
3500.484792	486100.652355	50.635828
3500.514883	485918.776423	50.640833
3500.355434	485714.384459	50.645837
3499.663074	485486.111483	50.650842
3499.149207	485290.788854	50.655847
3498.973404	485077.121484	50.660852
3498.952374	484833.941080	50.665857
3498.335960	484647.038300	50.670861
3498.349669	484392.852741	50.675866
3498.202914	484118.777679	50.680871
3497.657468	483852.108357	50.685876
3497.128075	483618.518282	50.690881
3496.683139	483395.096195	50.695885
3496.270281	483104.784646	50.700890
3495.654650	482837.251139	50.705895
3495.746662	482565.345875	50.710900
3495.205042	482299.212043	50.715905
3494.505820	481993.728158	50.720909
3494.224088	481722.985022	50.725914
3494.044639	481422.781287	50.730919
3493.227984	481147.655584	50.735924
3493.195153	480823.349737	50.740929
3492.253192	480529.333773	50.745933
3492.277454	480192.947933	50.750938
3491.271113	479911.348473	50.755943
3490.598827	479570.146527	50.760948
3490.478414	479239.797952	50.765953
3489.606500	478945.646033	50.770957
3489.518252	478603.777704	50.775962
3488.846297	478301.830667	50.780967
3488.272187	477934.890133	50.785972
3487.648293	477631.404922	50.790977
3487.437131	477277.116180	50.795981
3486.745287	476932.172322	50.800986
3485.706807	476609.173159	50.805991
3485.433725	476242.762306	50.810996
3485.001972	475923.153555	50.816001
3484.441580	475548.716362	50.821005
3484.149114	475221.775518	50.826010
3483.457453	474860.829424	50.831015
3482.978567	474489.046300	50.836020
3482.202296	474147.211053	50.841025
3481.628164	473776.595868	50.846029
3481.298991	473383.579719	50.851034
3480.069959	473051.733485	50.856039
3479.610021	472667.038009	50.861044
3478.995284	472301.218527	50.866049
3478.326612	471929.469588	50.871053
3477.698843	471583.411003	50.876058
3477.292380	471205.371811	50.881063
3476.634184	470831.015840	50.886068
3475.836938	470466.815088	50.891073
3475.193232	470097.006585	50.896077
3475.152250	469706.916922	50.901082
3474.188314	469334.863928	50.906087
3473.560197	468951.545720	50.911092
3473.137569	468565.247148	50.916097
3472.104333	468200.486413	50.921101
3471.697192	467808.391049	50.926106
3471.297081	467427.087945	50.931111
3470.212591	467041.018141	50.936116
3469.666654	466649.886659	50.941121
3468.718491	466264.744627	50.946125
3468.096101	465870.923236	50.951130
3467.380886	465511.187671	50.956135
3466.546058	465119.566586	50.961140
3466.353086	464746.043106	50.966145
3465.316735	464359.004189	50.971149
3464.562530	463982.716105	50.976154
3463.950736	463598.740744	50.981159
3463.458945	463211.392228	50.986164
3462.772973	462835.783375	50.991169
3461.832015	462461.273409	50.996173
3461.416489	462066.842395	51.001178
3460.841966	461687.594916	51.006183
3460.136365	461295.731821	51.011188
3459.655893	460913.970647	51.016193
3458.657272	460544.914888	51.021197
3458.234708	460142.892403	51.026202
3457.529728	459760.842286	51.031207
3456.571745	459369.339718	51.036212
3455.889844	458995.845426	51.041217
3454.883133	458611.996926	51.046221
3454.495449	458229.667245	51.051226
3453.614787	457842.741768	51.056231
3452.837541	457474.411356	51.061236
3452.345225	457092.383053	51.066241
3451.544006	456712.477073	51.071245
3451.042054	456329.929945	51.076250
3450.367298	455954.506381	51.081255
3449.958025	455573.403006	51.086260
3449.060952	455193.131333	51.091265
3448.072391	454820.985576	51.096269
3447.445099	454428.532340	51.101274
3446.417952	454067.593285	51.106279
3445.756766	453685.533910	51.111284
3445.386976	453308.952720	51.116289
3444.742834	452935.757582	51.121293
3443.997914	452575.308433	51.126298
3443.507483	452182.947133	51.131303
3442.330855	451804.591278	51.136308
3441.941393	451445.235301	51.141313
3440.861706	451072.586185	51.146317
3440.348616	450686.850579	51.151322
3439.870657	450320.386703	51.156327
3438.780308	449946.909221	51.161332
3438.105385	449571.888373	51.166337
3437.472990	449222.584508	51.171341
3437.067273	448850.706705	51.176346
3436.049147	448479.427316	51.181351
3435.530387	448106.743575	51.186356
3434.893193	447743.309548	51.191361
3433.988310	447388.337221	51.196365
3433.455610	447004.015832	51.201370
3432.795701	446642.243333	51.206375
3432.269523	446278.312455	51.211380
3431.350064	445916.468423	51.216385
3431.039423	445538.635756	51.221389
3430.334231	445184.360278	51.226394
3429.280615	444810.237347	51.231399
3428.640764	444433.251414	51.236404
3427.831348	444076.184290	51.241409
3427.055372	443708.802161	51.246413
3426.745872	443342.508214	51.251418
3426.054006	442990.787178	51.256423
3424.936410	442619.127724	51.261428
3424.248681	442247.293103	51.266433
3423.576630	441892.050335	51.271437
3423.096147	441538.396604	51.276442
3422.166460	441183.996522	51.281447
3421.560331	440819.031450	51.286452
3420.730975	440455.086216	51.291457
3419.840956	440116.884687	51.296461
3419.388871	439747.970242	51.301466
3418.488413	439396.611342	51.306471
3417.890988	439048.753484	51.311476
3417.250691	438681.401425	51.316481
3416.510507	438346.909129	51.321485
3415.921897	437983.194183	51.326490
3415.030781	437637.901700	51.331495
3414.306238	437284.149648	51.336500
3413.929824	436927.316485	51.341505
3413.197748	436586.884172	51.346509
3412.434728	436225.278531	51.351514
3411.590410	435886.022370	51.356519
3410.836852	435537.201154	51.361524
3409.866445	435193.004855	51.366529
3409.536373	434845.402043	51.371533
3409.261766	434494.434277	51.376538
3408.092677	434160.132079	51.381543
3407.466592	433811.063991	51.386548
3406.971326	433464.204868	51.391553
3406.320357	433127.014321	51.396557
3405.756443	432760.656188	51.401562
3405.069250	432419.754977	51.406567
3404.289009	432070.484580	51.411572
3403.569118	431719.904927	51.416577
3402.643072	431388.016885	51.421581
3402.125347	431026.705561	51.426586
3401.553461	430698.307809	51.431591
3400.602310	430347.771696	51.436596
3400.196268	429993.716508	51.441601
3399.269407	429668.155361	51.446605
3398.369179	429325.571457	51.451610
3397.635177	428983.210786	51.456615
3396.872803	428646.665743	51.461620
3396.230660	428311.341822	51.466625
3395.387752	427976.477153	51.471629
3395.209517	427628.931957	51.476634
3394.446337	427297.423899	51.481639
3393.433839	426961.176509	51.486644
3392.834812	426625.469075	51.491649
3392.154353	426292.792659	51.496653
3391.553657	425957.737514	51.501658
3390.652644	425633.469196	51.506663
3389.780693	425298.575773	51.511668
3389.542179	424966.778340	51.516673
3388.754346	424631.736413	51.521677
3388.182778	424294.802011	51.526682
3387.318748	423973.149627	51.531687
3386.524832	423648.612165	51.536692
3386.284268	423319.309692	51.541697
3385.025828	422987.852745	51.546701
3384.620750	422653.259564	51.551706
3384.183263	422329.971081	51.556711
3383.312132	421998.339434	51.561716
3382.564700	421670.215147	51.566721
3381.780536	421330.966598	51.571725
3381.394815	421000.465632	51.576730
3380.420568	420687.124558	51.581735
3379.521971	420345.494282	51.586740
3379.151700	420038.858533	51.591745
3378.433165	419716.778222	51.596749
3377.536558	419381.613900	51.601754
3377.032748	419063.734676	51.606759
3376.455496	418733.643873	51.611764
3375.633194	418413.826170	51.616769
3374.665160	418094.307377	51.621773
3374.242827	417775.232241	51.626778
3373.647403	417458.213380	51.631783
3372.753958	417128.408076	51.636788
3372.340406	416813.055545	51.641793
3371.254369	416495.341451	51.646797
3370.813447	416167.918049	51.651802
3370.243744	415847.244214	51.656807
3369.765711	415521.877367	51.661812
3368.990957	415203.820417	51.666817
3368.034844	414895.951883	51.671821
3367.666414	414570.861992	51.676826
3366.788953	414252.836339	51.681831
3366.074647	413931.427476	51.686836
3365.555719	413605.690065	51.691841
3364.937913	413285.503946	51.696845
3364.048111	412970.464714	51.701850
3363.472579	412645.462557	51.706855
3362.554218	412324.576692	51.711860
3362.150493	412007.646265	51.716865
3361.393684	411693.995473	51.721869
3361.079630	411366.574830	51.726874
3360.371908	411042.821270	51.731879
3359.175225	410742.393141	51.736884
3358.627259	410419.141254	51.741889
3358.042472	410105.065505	51.746893
3357.390323	409783.449674	51.751898
3356.591068	409470.544820	51.756903
3355.952854	409146.099236	51.761908
3355.171187	408819.792307	51.766913
3354.463314	408525.313274	51.771917
3353.908600	408203.512893	51.776922
3353.455318	407886.775895	51.781927
3352.394592	407570.716217	51.786932
3351.730107	407252.735390	51.791937
3351.066636	406938.893737	51.796941
3350.480630	406627.374840	51.801946
3349.684719	406319.571224	51.806951
3349.066126	406017.124613	51.811956
3348.593736	405695.996800	51.816961
3347.589882	405383.921582	51.821965
3347.145755	405066.595254	51.826970
3346.811140	404756.568367	51.831975
3345.602281	404448.379597	51.836980
3345.363907	404131.748418	51.841985
3344.402247	403826.971223	51.846989
3343.852770	403508.044629	51.851994
3343.307045	403205.483286	51.856999
3342.430210	402874.884539	51.862004
3341.535140	402573.185830	51.867009
3340.835428	402278.468898	51.872013
3340.462334	401958.761843	51.877018
3339.673146	401647.200654	51.882023
3338.715430	401337.162846	51.887028
3338.361221	401018.460277	51.892033
3337.431841	400722.824961	51.897037
3337.146358	400415.264867	51.902042
3336.416258	400106.806218	51.907047
3335.613693	399787.221971	51.912052
3335.037692	399468.259724	51.917057
3333.883484	399165.655208	51.922061
3333.410135	398863.118199	51.927066
3332.698871	398556.396095	51.932071
3331.998801	398256.024787	51.937076
3331.317427	397953.156468	51.942081
3330.437450	397649.528716	51.947085
3329.833228	397350.074702	51.952090
3329.247283	397059.462159	51.957095
3328.557235	396748.982970	51.962100
3328.063528	396452.147436	51.967105
3327.187720	396158.623885	51.972109
3326.611759	395845.982795	51.977114
3326.116024	395551.605753	51.982119
3325.094968	395245.792214	51.987124
3324.463431	394937.397346	51.992129
3323.867911	394646.231702	51.997133
3323.476038	394327.394882	52.002138
3322.377024	394039.608904	52.007143
3321.891050	393739.926374	52.012148
3321.412634	393439.502717	52.017153
3320.493105	393143.671938	52.022157
3319.721835	392844.891239	52.027162
3319.120599	392546.691306	52.032167
3318.425076	392256.589232	52.037172
3317.694935	391951.564983	52.042177
3317.050408	391663.560314	52.047181
3316.399289	391361.620476	52.052186
3315.501235	391065.438166	52.057191
3314.956194	390779.114140	52.062196
3314.663339	390470.270123	52.067201
3314.030718	390178.742487	52.072205
3313.066680	389883.704983	52.077210
3312.165488	389579.729870	52.082215
3311.442603	389286.454687	52.087220
3311.130804	388993.112099	52.092225
3309.997967	388708.288408	52.097229
3309.771770	388401.119713	52.102234
3308.911150	388102.465758	52.107239
3307.637591	387817.428442	52.112244
3307.489009	387532.465278	52.117249
3306.645306	387241.582988	52.122253
3306.042456	386949.109071	52.127258
3305.574553	386654.933094	52.132263
3304.754594	386353.918835	52.137268
3304.233373	386069.384681	52.142273
3303.157466	385795.388058	52.147277
3303.040015	385491.610885	52.152282
3302.181637	385210.429464	52.157287
3301.613762	384919.790413	52.162292
3301.350453	384605.932873	52.167297
3300.205771	384324.739196	52.172301
3299.389817	384022.764460	52.177306
3298.957233	383745.650091	52.182311
3298.134741	383454.226133	52.187316
3297.776872	383157.105882	52.192321
3296.992998	382867.629604	52.197325
3296.392599	382572.170824	52.202330
3295.886021	382273.083427	52.207335
3295.180204	381990.658534	52.212340
3294.691020	381689.783508	52.217345
3293.577961	381396.049908	52.222349
3292.995755	381086.283114	52.227354
3292.175990	380804.655996	52.232359
3291.471604	380511.919279	52.237364
3290.817006	380212.381503	52.242369
3289.836376	379917.013393	52.247373
3289.603589	379629.384127	52.252378
3288.457174	379352.274705	52.257383
3287.653986	379072.031399	52.262388
3287.667588	378782.551083	52.267393
3287.388455	378492.122961	52.272397
3286.159949	378203.445309	52.277402
3285.432799	377898.051206	52.282407
3284.947869	377614.109939	52.287412
3284.468673	377318.337896	52.292417
3283.436936	377033.766782	52.297421
3282.970402	376732.672213	52.302426
3282.265115	376451.479303	52.307431
3281.718747	376151.741184	52.312436
3280.886892	375856.472072	52.317441
3280.150510	375570.165106	52.322445
3279.598076	375282.784102	52.327450
3278.991964	374992.382485	52.332455
3278.065110	374702.589175	52.337460
3277.580883	374413.868537	52.342465
3276.685197	374125.974104	52.347469
3276.381139	373841.901617	52.352474
3275.628034	373552.657860	52.357479
3274.767458	373264.472083	52.362484
3274.234536	372971.500856	52.367489
3273.742806	372673.407803	52.372493
3272.941302	372383.247817	52.377498
3272.050872	372089.970844	52.382503
3271.251095	371809.804361	52.387508
3271.122342	371509.432442	52.392513
3270.215878	371231.034368	52.397517
3269.831530	370940.238863	52.402522
3269.380500	370640.318848	52.407527
3268.460208	370355.201019	52.412532
3267.726760	370051.378290	52.417537
3266.936240	369767.940585	52.422541
3266.245623	369465.964158	52.427546
3265.547806	369184.975768	52.432551
3264.909974	368894.308364	52.437556
3264.347394	368599.785456	52.442561
3263.598379	368313.304199	52.447565
3262.849185	368010.105796	52.452570
3262.409145	367724.436873	52.457575
3261.347692	367440.543580	52.462580
3260.991008	367156.994968	52.467585
3260.216002	366855.802717	52.472589
3259.460691	366577.020345	52.477594
3258.973990	366279.620471	52.482599
3258.135531	366003.468311	52.487604
3257.831129	365701.150732	52.492609
3256.640325	365429.528801	52.497613
3256.167561	365131.177777	52.502618
3255.771849	364848.893014	52.507623
3254.964085	364555.858060	52.512628
3254.342070	364257.703058	52.517633
3253.556261	363971.072793	52.522637
3253.110062	363677.186296	52.527642
3252.546370	363401.458427	52.532647
3251.732716	363111.723033	52.537652
3250.865666	362795.277263	52.542657
3250.297564	362518.069079	52.547661
3249.681497	362223.538737	52.552666
3249.152652	361930.290470	52.557671
3248.235080	361649.519233	52.562676
3247.560454	361357.511862	52.567681
3246.950234	361066.739355	52.572685
3246.366110	360768.530757	52.577690
3245.700680	360482.750831	52.582695
3244.571289	360198.849273	52.587700
3244.332894	359907.374788	52.592705
3243.202782	359631.511058	52.597709
3242.751245	359343.909323	52.602714
3242.302585	359039.994052	52.607719
3241.145623	358765.198438	52.612724
3240.527130	358483.878006	52.617729
3239.855128	358201.826465	52.622733
3239.426568	357910.904575	52.627738
3238.645365	357635.101687	52.632743
3238.071648	357352.673513	52.637748
3237.448425	357053.379683	52.642753
3236.768386	356772.211997	52.647757
3235.757110	356504.582621	52.652762
3235.322132	356215.865888	52.657767
3234.589542	355927.499968	52.662772
3234.046263	355661.293571	52.667777
3233.332673	355354.852966	52.672781
3232.826552	355082.071924	52.677786
3231.644149	354787.459430	52.682791
3230.892020	354519.931358	52.687796
3230.536961	354242.312112	52.692801
3229.754454	353961.043394	52.697805
3229.379868	353689.735729	52.702810
3228.610011	353393.090469	52.707815
3228.082512	353124.425381	52.712820
3227.321979	352838.209917	52.717825
3226.333471	352550.069315	52.722829
3225.806150	352270.456354	52.727834
3225.496512	351995.159495	52.732839
3224.764743	351713.845343	52.737844
3224.052354	351423.313551	52.742849
3223.453580	351152.562861	52.747853
3222.917871	350859.887687	52.752858
3222.182759	350582.411249	52.757863
3221.559240	350305.755634	52.762868
3220.611144	350014.362808	52.767873
3219.870162	349731.334621	52.772877
3219.333842	349455.348119	52.777882
3218.894719	349164.862904	52.782887
3218.041355	348883.502517	52.787892
3217.585216	348606.226532	52.792897
3216.932445	348318.570415	52.797901
3216.232935	348032.523704	52.802906
3215.577838	347750.922663	52.807911
3214.960246	347464.096555	52.812916
3214.409700	347173.847760	52.817921
3213.657695	346888.719886	52.822925
3212.844608	346615.613960	52.827930
3212.200746	346317.027090	52.832935
3211.526815	346043.870994	52.837940
3210.783149	345746.773249	52.842945
3210.082216	345467.357248	52.847949
3209.474408	345177.718377	52.852954
3208.888847	344901.564919	52.857959
3208.163834	344619.017916	52.862964
3207.530217	344330.753471	52.867969
3206.818818	344050.874256	52.872973
3206.281979	343766.358947	52.877978
3205.865149	343478.692451	52.882983
3204.674411	343197.816014	52.887988
3204.230939	342904.601977	52.892993
3203.644368	342631.289104	52.897997
3202.687773	342336.677147	52.903002
3202.063534	342061.942233	52.908007
3201.471434	341783.815520	52.913012
3201.063128	341480.127181	52.918017
3200.350407	341213.649897	52.923021
3199.250642	340920.224775	52.928026
3198.727019	340637.143804	52.933031
3197.838943	340373.414402	52.938036
3197.556678	340070.030213	52.943041
3196.827872	339799.654794	52.948045
3196.153151	339507.734124	52.953050
3195.722755	339232.523422	52.958055
3194.650104	338938.983031	52.963060
3194.138205	338671.521440	52.968065
3193.498728	338387.252398	52.973069
3192.661731	338092.754479	52.978074
3192.400878	337816.721811	52.983079
3191.574827	337534.591466	52.988084
3190.905489	337248.412980	52.993089
3189.966456	336958.202850	52.998093
3189.393603	336677.454386	53.003098
3188.625897	336414.529972	53.008103
3188.025185	336125.051879	53.013108
3187.692647	335834.995523	53.018113
3186.759060	335551.677359	53.023117
3186.048355	335276.647318	53.028122
3185.612878	334996.633886	53.033127
3184.563361	334725.448403	53.038132
3184.508917	334430.479723	53.043137
3183.637643	334160.358515	53.048141
3183.161458	333869.705632	53.053146
3182.559943	333580.242442	53.058151
3181.697874	333294.943495	53.063156
3181.120480	333010.463944	53.068161
3180.172899	332722.655871	53.073165
3179.778579	332436.312078	53.078170
3179.267862	332153.982544	53.083175
3178.204456	331869.346240	53.088180
3177.616415	331588.452422	53.093185
3176.745606	331305.769227	53.098189
3176.409119	331021.141917	53.103194
3175.599531	330726.226552	53.108199
3174.728193	330450.032210	53.113204
3174.426256	330150.808048	53.118209
3173.649077	329878.517416	53.123213
3172.858246	329592.327148	53.128218
3172.443555	329306.712781	53.133223
3171.606703	329020.451265	53.138228
3171.121629	328730.161322	53.143233
3170.203429	328459.619193	53.148237
3169.703832	328173.733994	53.153242
3169.056841	327873.435283	53.158247
3168.066062	327602.825284	53.163252
3167.601312	327322.023470	53.168257
3166.781196	327029.336046	53.173261
3166.314287	326758.105619	53.178266
3165.805333	326468.193004	53.183271
3164.937361	326188.291192	53.188276
3164.293780	325906.774357	53.193281
3163.755295	325623.890509	53.198285
3163.146005	325341.373336	53.203290
3162.436552	325053.396964	53.208295
3161.384108	324776.320205	53.213300
3161.364872	324485.941187	53.218305
3160.585621	324198.711275	53.223309
3159.452416	323917.621604	53.228314
3158.741180	323627.985644	53.233319
3158.188616	323360.194889	53.238324
3157.683002	323066.552529	53.243329
3156.511037	322800.844021	53.248333
3156.258200	322526.077731	53.253338
3155.528573	322232.900843	53.258343
3155.003842	321956.928164	53.263348
3154.325187	321663.257544	53.268353
3153.429035	321385.330366	53.273357
3152.937638	321116.097213	53.278362
3152.370776	320826.632852	53.283367
3151.652050	320542.767806	53.288372
3150.702551	320263.954446	53.293377
3150.297715	319985.588774	53.298381
3149.709910	319695.182045	53.303386
3149.045399	319413.469244	53.308391
3148.121050	319146.895987	53.313396
3147.789749	318855.860433	53.318401
3147.116921	318576.081602	53.323405
3146.080158	318296.868787	53.328410
3145.757134	318010.285328	53.333415
3145.052778	317726.103941	53.338420
3144.485213	317446.585270	53.343425
3143.276249	317171.139520	53.348429
3142.644850	316892.775213	53.353434
3142.473556	316610.237755	53.358439
3141.725120	316340.064108	53.363444
3141.387568	316044.081294	53.368449
3140.577523	315766.658810	53.373453
3139.612418	315479.583985	53.378458
3139.027971	315194.256044	53.383463
3138.347883	314915.512063	53.388468
3137.692774	314634.140626	53.393473
3136.795719	314352.781253	53.398477
3136.477500	314069.037805	53.403482
3135.763908	313787.011312	53.408487
3134.931769	313505.410259	53.413492
3134.199329	313225.549716	53.418497
3133.772174	312951.573285	53.423501
3132.445345	312671.932694	53.428506
3131.953395	312389.256379	53.433511
3131.286960	312114.424489	53.438516
3130.832800	311839.889377	53.443521
3129.975211	311567.989336	53.448525
3129.384783	311291.819276	53.453530
3128.926975	311002.080444	53.458535
3127.895404	310739.806099	53.463540
3127.474234	310454.923843	53.468545
3126.922359	310180.094672	53.473549
3126.014478	309905.855954	53.478554
3125.760515	309631.080240	53.483559
3125.154776	309357.403621	53.488564
3124.529449	309070.029349	53.493569
3123.519393	308797.230327	53.498573
3123.017887	308512.763638	53.503578
3122.689928	308226.893726	53.508583
3121.656582	307946.660718	53.513588
3121.059890	307664.346248	53.518593
3120.588627	307379.974087	53.523597
3119.769046	307102.175541	53.528602
3119.163872	306817.645080	53.533607
3118.603306	306532.801361	53.538612
3117.871273	306252.517021	53.543617
3117.280113	305975.061947	53.548621
3116.545352	305690.753312	53.553626
3116.131834	305400.026843	53.558631
3115.312860	305132.053861	53.563636
3114.329505	304827.741271	53.568641
3113.558963	304551.788732	53.573645
3113.123920	304276.724807	53.578650
3112.688344	303996.185268	53.583655
3111.777345	303720.584411	53.588660
3111.606003	303427.574578	53.593665
3110.772026	303148.446151	53.598669
3109.831337	302858.765655	53.603674
3109.257069	302572.770147	53.608679
3108.641532	302290.218571	53.613684
3108.009313	302010.317605	53.618689
3107.529521	301719.492445	53.623693
3106.640807	301434.716042	53.628698
3106.107922	301152.684129	53.633703
3105.450632	300864.279333	53.638708
3104.721683	300577.591619	53.643713
3104.133388	300288.385432	53.648717
3103.525490	300003.740359	53.653722
3102.935032	299712.165129	53.658727
3101.999827	299431.263546	53.663732
3100.947756	299142.638124	53.668737
3100.544045	298858.544577	53.673741
3099.680301	298580.660861	53.678746
3099.334221	298302.287331	53.683751
3098.483238	298023.942335	53.688756
3097.847534	297731.199526	53.693761
3097.089454	297458.569028	53.698765
3096.191859	297177.963586	53.703770
3095.746606	296895.248793	53.708775
3095.164113	296616.197090	53.713780
3094.386055	296339.926381	53.718785
3093.893203	296058.949675	53.723789
3093.378658	295782.560097	53.728794
3092.641653	295500.678968	53.733799
3091.741271	295221.217228	53.738804
3091.113964	294942.221249	53.743809
3090.653372	294669.590811	53.748813
3089.607868	294384.395333	53.753818
3089.300232	294094.982480	53.758823
3088.647666	293820.343979	53.763828
3088.160068	293536.485305	53.768833
3087.503887	293254.766756	53.773837
3086.860804	292963.266286	53.778842
3086.278867	292670.889888	53.783847
3085.490755	292393.622541	53.788852
3085.017766	292099.598296	53.793857
3084.213094	291809.726474	53.798861
3083.277137	291525.834521	53.803866
3082.682241	291232.388854	53.808871
3082.054592	290956.520739	53.813876
3081.281454	290672.958652	53.818881
3080.495624	290389.780296	53.823885
3079.884571	290103.874414	53.828890
3079.039735	289825.900251	53.833895
3078.382737	289546.775515	53.838900
3078.068976	289263.572284	53.843905
3077.093179	288986.713176	53.848909
3076.555290	288710.650431	53.853914
3076.040263	288425.720999	53.858919
3075.445027	288141.033221	53.863924
3074.503585	287862.435885	53.868929
3074.272878	287578.479447	53.873933
3073.022836	287298.657090	53.878938
3072.261768	287011.371412	53.883943
3071.520531	286743.692743	53.888948
3071.533104	286460.664707	53.893953
3070.357084	286186.254482	53.898957
3069.915040	285906.430554	53.903962
3069.496972	285624.845339	53.908967
3068.628790	285350.334894	53.913972
3068.042343	285064.344500	53.918977
3067.221840	284782.338522	53.923981
3066.570094	284490.984318	53.928986
3066.165189	284210.847801	53.933991
3065.208739	283941.928001	53.938996
3064.867160	283645.659780	53.944001
3064.198518	283368.620713	53.949005
3063.153266	283087.235100	53.954010
3062.539111	282801.808078	53.959015
3061.887610	282522.702952	53.964020
3061.318215	282238.592925	53.969025
3060.814781	281972.682146	53.974029
3060.238504	281685.185683	53.979034
3059.624387	281405.386514	53.984039
3058.471100	281133.185714	53.989044
3057.740518	280839.473602	53.994049
3057.332179	280566.492536	53.999053
3056.246797	280293.236504	54.004058
3056.132658	280006.812365	54.009063
3055.015214	279736.286356	54.014068
3054.713288	279454.781698	54.019073
3053.702083	279174.739040	54.024077
3053.305012	278892.256037	54.029082
3052.945931	278617.560280	54.034087
3051.782005	278345.258529	54.039092
3051.008221	278061.790777	54.044097
3050.565363	277788.381554	54.049101
3049.712578	277510.274581	54.054106
3049.274032	277232.229361	54.059111
3048.241250	276957.945604	54.064116
3047.835351	276680.710156	54.069121
3047.092156	276412.518413	54.074125
3046.446907	276134.785979	54.079130
3046.103713	275851.148004	54.084135
3045.152204	275591.368311	54.089140
3044.740537	275309.702241	54.094145
3044.381513	275031.211397	54.099149
3043.476665	274758.562807	54.104154
3042.850064	274468.322481	54.109159
3042.224493	274178.413107	54.114164
3041.481952	273889.821166	54.119169
3040.638321	273621.212470	54.124173
3039.978161	273352.320091	54.129178
3039.659036	273054.874676	54.134183
3038.625082	272783.774868	54.139188
3038.057328	272505.572062	54.144193
3037.769314	272219.429856	54.149197
3036.837969	271939.272727	54.154202
3036.429242	271650.704811	54.159207
3035.402511	271378.763736	54.164212
3034.826260	271097.761126	54.169217
3034.044949	270801.408198	54.174221
3033.260265	270525.252277	54.179226
3032.639982	270229.943744	54.184231
3032.094765	269958.487234	54.189236
3031.359734	269683.138755	54.194241
3031.201565	269391.908765	54.199245
3030.397113	269110.561003	54.204250
3029.580783	268837.798047	54.209255
3029.101056	268550.694267	54.214260
3028.682763	268256.577150	54.219265
3027.728329	267980.754811	54.224269
3026.923155	267694.263292	54.229274
3026.364777	267408.878941	54.234279
3025.713566	267133.492969	54.239284
3025.025026	266844.946035	54.244289
3024.463522	266548.611397	54.249293
3023.668210	266262.297461	54.254298
3023.000292	265980.216725	54.259303
3022.121363	265711.311105	54.264308
3021.577130	265418.361778	54.269313
3021.072788	265129.048284	54.274317
3020.233933	264850.331712	54.279322
3019.788873	264562.919369	54.284327
3018.830343	264289.035615	54.289332
3018.338439	264007.285021	54.294337
3017.787756	263726.027849	54.299341
3017.231339	263442.785320	54.304346
3016.569217	263151.995798	54.309351
3015.609985	262863.520203	54.314356
3014.871199	262577.098343	54.319361
3014.230718	262303.165893	54.324365
3013.765032	262013.135839	54.329370
3013.253216	261728.308796	54.334375
3012.374980	261441.528076	54.339380
3011.559506	261158.277724	54.344385
3011.126508	260884.695784	54.349389
3010.399757	260595.166910	54.354394
3009.854524	260305.100264	54.359399
3008.914813	260029.230903	54.364404
3008.249638	259741.272211	54.369409
3007.770358	259465.610722	54.374413
3007.035905	259192.816821	54.379418
3006.289162	258896.569592	54.384423
3005.643093	258618.006688	54.389428
3004.778728	258332.296840	54.394433
3004.316306	258053.731000	54.399437
3003.648003	257778.101365	54.404442
3003.010618	257494.572292	54.409447
3002.256774	257207.878595	54.414452
3001.589237	256926.086798	54.419457
3001.343137	256647.004592	54.424461
3000.272028	256368.740949	54.429466
2999.905871	256079.389735	54.434471
2999.424259	255804.191468	54.439476
2998.429181	255509.363295	54.444481
2997.947730	255228.282878	54.449485
2997.165746	254947.861637	54.454490
2996.564174	254660.383347	54.459495
2995.981987	254380.593439	54.464500
2995.152797	254086.938094	54.469505
2994.512255	253795.723635	54.474509
2993.536604	253518.009171	54.479514
2993.118094	253225.130588	54.484519
2992.290128	252952.894440	54.489524
2991.488432	252667.870247	54.494529
2991.230086	252389.814782	54.499533
2990.505790	252111.247780	54.504538
2990.107394	251816.178213	54.509543
2989.019091	251543.425203	54.514548
2988.365403	251256.495387	54.519553
2987.840044	250972.321598	54.524557
2987.042225	250695.296560	54.529562
2986.379612	250401.188111	54.534567
2985.897982	250124.877992	54.539572
2985.387204	249823.030267	54.544577
2984.625831	249542.308842	54.549581
2983.863000	249271.341711	54.554586
2983.221312	248981.358124	54.559591
2982.325502	248701.525360	54.564596
2981.752908	248417.389120	54.569601
2980.935415	248137.595941	54.574605
2980.314304	247866.074113	54.579610
2979.902158	247569.308450	54.584615
2979.394304	247292.600181	54.589620
2978.537786	247011.058200	54.594625
2978.178823	246724.777782	54.599629
2977.582837	246439.706887	54.604634
2976.949200	246147.639479	54.609639
2976.034990	245866.261726	54.614644
2975.352747	245575.018130	54.619649
2974.805888	245287.751813	54.624653
2973.428735	245010.854652	54.629658
2973.072161	244726.640741	54.634663
2972.716458	244441.739741	54.639668
2972.002154	244158.296718	54.644673
2971.335392	243866.876176	54.649677
2970.504059	243588.724235	54.654682
2970.090541	243294.743861	54.659687
2968.957570	243032.862166	54.664692
2968.424473	242743.638514	54.669697
2968.057488	242454.516568	54.674701
2967.555394	242172.954293	54.679706
2966.905836	241886.908741	54.684711
2966.332325	241606.199428	54.689716
2965.660045	241315.040417	54.694721
2965.134861	241016.372235	54.699725
2964.301201	240729.900241	54.704730
2963.732665	240437.912114	54.709735
2962.822727	240157.157657	54.714740
2962.061881	239860.847015	54.719745
2961.642626	239571.231114	54.724749
2960.464969	239294.951955	54.729754
2960.019798	239006.945857	54.734759
2959.508284	238715.869849	54.739764
2958.712071	238436.145716	54.744769
2958.101946	238145.697965	54.749773
2957.434255	237862.746496	54.754778
2957.021711	237561.115841	54.759783
2956.400942	237283.047530	54.764788
2955.611917	236995.610473	54.769793
2954.887944	236700.652128	54.774797
2954.256501	236413.038938	54.779802
2953.805828	236118.981127	54.784807
2952.777917	235830.031828	54.789812
2952.225319	235551.677248	54.794817
2951.612363	235256.170732	54.799821
2950.493586	234978.747645	54.804826
2950.361014	234676.724592	54.809831
2949.569248	234400.422649	54.814836
2948.734364	234112.873663	54.819841
2948.386285	233818.475321	54.824845
2947.462067	233538.861133	54.829850
2946.890709	233248.803084	54.834855
2946.308721	232959.791564	54.839860
2945.855592	232672.033651	54.844865
2945.526501	232377.764028	54.849869
2944.298642	232088.068074	54.854874
2943.889354	231786.632589	54.859879
2943.158070	231497.241795	54.864884
2942.294507	231210.546382	54.869889
2942.000410	230909.732080	54.874893
2941.083954	230624.727379	54.879898
2940.559187	230329.425857	54.884903
2939.929155	230038.572336	54.889908
2939.142786	229737.279714	54.894913
2938.748224	229448.096785	54.899917
2937.598177	229150.479299	54.904922
2936.980424	228851.098094	54.909927
2936.277701	228571.871380	54.914932
2935.504731	228279.824156	54.919937
2935.180595	227995.065179	54.924941
2934.279788	227701.512486	54.929946
2933.971765	227416.829272	54.934951
2933.330570	227126.012734	54.939956
2932.506244	226835.238925	54.944961
2932.221714	226535.685793	54.949965
2930.886371	226256.566862	54.954970
2930.580301	225942.583037	54.959975
2929.946476	225660.096107	54.964980
2928.946923	225376.891510	54.969985
2928.440706	225080.586809	54.974989
2927.690822	224791.947133	54.979994
2927.123120	224494.037599	54.984999
2926.459201	224213.877381	54.990004
2925.919419	223925.143932	54.995009
2925.419170	223618.570603	55.000013
2924.492535	223338.556930	55.005018
2923.718710	223043.562474	55.010023
2923.181280	222755.685876	55.015028
2922.299488	222460.481603	55.020033
2921.856535	222170.059016	55.025037
2921.329781	221879.205265	55.030042
2920.413433	221589.941864	55.035047
2919.398893	221300.720579	55.040052
2919.076908	221011.556248	55.045057
2918.741575	220712.491617	55.050061
2917.960059	220436.755496	55.055066
2917.260842	220146.788656	55.060071
2916.364802	219849.407466	55.065076
2915.879826	219565.595462	55.070081
2915.166110	219270.008058	55.075085
2914.638465	218980.566053	55.080090
2914.209200	218682.021044	55.085095
2913.492051	218404.207598	55.090100
2912.638060	218100.907944	55.095105
2912.226155	217805.571574	55.100109
2911.261126	217511.125935	55.105114
2910.835733	217217.410742	55.110119
2909.846516	216925.746290	55.115124
2909.177051	216621.545534	55.120129
2908.941958	216327.562132	55.125133
2908.289927	216047.163816	55.130138
2907.740825	215736.329028	55.135143
2906.754608	215452.091122	55.140148
2906.020887	215153.036672	55.145153
2905.732495	214853.225707	55.150157
2904.552063	214554.537400	55.155162
2903.903073	214260.793970	55.160167
2903.426423	213973.261396	55.165172
2902.977807	213679.654285	55.170177
2902.154963	213386.413211	55.175181
2901.408485	213096.076090	55.180186
2900.999153	212796.930003	55.185191
2900.233706	212506.483967	55.190196
2899.252581	212217.155257	55.195201
2898.525721	211915.327030	55.200205
2897.926941	211625.265881	55.205210
2897.663510	211327.847240	55.210215
2897.004609	211046.058552	55.215220
2896.237681	210744.102230	55.220225
2895.752634	210441.122708	55.225229
2894.638866	210153.300822	55.230234
2894.304566	209849.078468	55.235239
2893.451793	209559.257989	55.240244
2892.699368	209265.490245	55.245249
2892.779509	208961.435742	55.250253
2891.553262	208672.162219	55.255258
2891.003456	208370.717657	55.260263
2890.397502	208075.290656	55.265268
2889.802622	207781.288773	55.270273
2889.180183	207476.971148	55.275277
2888.225236	207182.660132	55.280282
2887.964929	206874.292007	55.285287
2887.022342	206580.096561	55.290292
2886.025074	206280.922383	55.295297
2885.473643	205988.895128	55.300301
2884.519969	205690.200674	55.305306
2883.951836	205395.888251	55.310311
2883.384980	205103.409722	55.315316
2882.677902	204818.857944	55.320321
2882.276636	204510.779143	55.325325
2881.251248	204227.935112	55.330330
2881.157881	203928.299091	55.335335
2880.046695	203637.441372	55.340340
2879.320994	203340.364715	55.345345
2879.107168	203042.559551	55.350349
2878.221074	202747.598479	55.355354
2877.318537	202449.956418	55.360359
2876.563860	202153.526935	55.365364
2875.909210	201869.923420	55.370369
2875.605409	201576.085308	55.375373
2874.873079	201296.009318	55.380378
2874.181360	200990.795484	55.385383
2873.503497	200708.512368	55.390388
2873.079717	200421.443929	55.395393
2872.466091	200114.619253	55.400397
2871.374042	199822.518794	55.405402
2870.791242	199527.348880	55.410407
2870.388524	199238.501891	55.415412
2869.574202	198943.448213	55.420417
2869.200687	198648.631773	55.425421
2868.150783	198351.073707	55.430426
2867.588401	198043.820186	55.435431
2867.309315	197760.267924	55.440436
2866.467148	197467.924554	55.445441
2865.988862	197159.988500	55.450445
2865.185832	196866.077193	55.455450
2864.174461	196565.405702	55.460455
2863.659579	196270.281514	55.465460
2863.089716	195969.390905	55.470465
2862.461556	195680.930122	55.475469
2861.601207	195384.835086	55.480474
2861.594978	195078.707213	55.485479
2861.036367	194780.862903	55.490484
2860.045422	194478.164661	55.495489
2859.411754	194183.656712	55.500493
2858.759098	193877.778468	55.505498
2857.816436	193570.332118	55.510503
2857.300534	193281.205692	55.515508
2856.771612	192971.038313	55.520513
2855.986009	192670.290706	55.525517
2855.381401	192381.349010	55.530522
2854.708927	192069.161597	55.535527
2854.012470	191780.148939	55.540532
2853.113634	191479.133965	55.545537
2852.604927	191167.231771	55.550541
2851.825724	190879.420838	55.555546
2851.139608	190579.790043	55.560551
2850.796435	190278.656416	55.565556
2849.916871	189973.576521	55.570561
2849.628108	189674.690019	55.575565
2848.621909	189378.349020	55.580570
2848.042644	189070.530201	55.585575
2847.490634	188757.174834	55.590580
2846.689775	188460.845265	55.595585
2846.166653	188167.081655	55.600589
2845.497762	187862.745421	55.605594
2844.628540	187553.990180	55.610599
2844.114535	187266.502810	55.615604
2843.021093	186956.298600	55.620609
2842.865814	186655.909111	55.625613
2841.917113	186356.601367	55.630618
2841.333534	186060.405461	55.635623
2840.648479	185763.680525	55.640628
2840.066476	185475.146579	55.645633
2839.170699	185164.681563	55.650637
2838.567099	184867.491646	55.655642
2838.148411	184563.583043	55.660647
2837.550740	184266.828693	55.665652
2836.847097	183960.056178	55.670657
2836.582903	183645.977955	55.675661
2835.627498	183350.024197	55.680666
2834.723939	183049.535607	55.685671
2834.254662	182746.423434	55.690676
2833.293899	182441.063312	55.695681
2832.687250	182134.758810	55.700685
2831.873725	181840.255640	55.705690
2831.199579	181537.146150	55.710695
2830.674618	181254.469364	55.715700
2829.861142	180949.885065	55.720705
2829.808016	180646.543563	55.725709
2828.501093	180350.246127	55.730714
2827.981171	180049.297822	55.735719
2827.489806	179740.206428	55.740724
2826.681096	179445.375489	55.745729
2825.898341	179150.110025	55.750733
2825.201755	178842.189737	55.755738
2824.920101	178541.468808	55.760743
2824.137341	178252.505783	55.765748
2823.198433	177952.440104	55.770753
2822.979764	177644.720040	55.775757
2822.067036	177351.408442	55.780762
2821.375004	177052.938208	55.785767
2820.761557	176757.688292	55.790772
2820.402685	176454.221968	55.795777
2819.504105	176151.428421	55.800781
2818.579053	175851.757374	55.805786
2818.003007	175538.119167	55.810791
2817.426847	175251.624571	55.815796
2816.765315	174954.652869	55.820801
2816.369529	174646.322004	55.825805
2815.535547	174354.189534	55.830810
2814.752837	174056.493266	55.835815
2814.154682	173750.058164	55.840820
2813.310008	173446.564131	55.845825
2812.568225	173148.333998	55.850829
2812.100370	172860.821893	55.855834
2811.825665	172557.180800	55.860839
2810.866766	172246.833817	55.865844
2809.908611	171949.168413	55.870849
2809.637474	171651.421896	55.875853
2808.830962	171350.990080	55.880858
2807.861371	171055.635098	55.885863
2807.504280	170749.566647	55.890868
2806.657577	170473.691810	55.895873
2806.231991	170163.569420	55.900877
2805.736144	169841.405202	55.905882
2805.237983	169498.299801	55.910887
2804.520985	169187.697330	55.915892
2803.755623	168887.685083	55.920897
2803.528541	168579.654979	55.925901
2802.597216	168279.699240	55.930906
2801.777530	167970.483596	55.935911
2801.384262	167662.220227	55.940916
2800.574449	167359.378735	55.945921
2800.272039	167035.719889	55.950925
2799.170746	166752.588049	55.955930
2798.746084	166437.994582	55.960935
2797.889605	166131.915228	55.965940
2797.221775	165827.156347	55.970945
2796.871519	165507.676270	55.975949
2796.004646	165207.340779	55.980954
2794.978340	164902.824307	55.985959
2794.564561	164592.466198	55.990964
2793.983336	164287.553753	55.995969
2793.188553	163972.696617	56.000973
2792.370004	163672.544060	56.005978
2791.795665	163372.266303	56.010983
2791.332120	163070.257041	56.015988
2790.372562	162764.362000	56.020993
2789.935294	162448.253627	56.025997
2788.831546	162153.346246	56.031002
2788.213386	161843.018617	56.036007
2787.825843	161548.129928	56.041012
2786.906769	161241.758341	56.046017
2786.130612	160948.296540	56.051021
2785.825973	160648.799834	56.056026
2785.246913	160345.713084	56.061031
2784.481730	160040.662422	56.066036
2783.500079	159750.167185	56.071041
2783.259000	159439.012670	56.076045
2782.336258	159136.384888	56.081050
2781.427916	158834.520221	56.086055
2781.214855	158524.805970	56.091060
2780.552078	158235.150015	56.096065
2780.082945	157922.901022	56.101069
2779.060744	157633.739256	56.106074
2778.558758	157331.162281	56.111079
2777.681506	157024.871874	56.116084
2776.881986	156720.542269	56.121089
2776.274782	156416.312032	56.126093
2775.564762	156118.685548	56.131098
2775.203345	155824.425920	56.136103
2774.478078	155517.947006	56.141108
2773.863893	155219.931874	56.146113
2773.238806	154910.862150	56.151117
2772.353627	154610.391173	56.156122
2771.833986	154306.420251	56.161127
2771.480247	154010.586326	56.166132
2770.384444	153708.974661	56.171137
2769.783797	153399.266743	56.176141
2768.704831	153098.496857	56.181146
2768.101655	152803.920678	56.186151
2767.548041	152508.843559	56.191156
2766.988312	152206.741192	56.196161
2766.686577	151911.121108	56.201165
2765.667270	151614.028568	56.206170
2764.964677	151314.677006	56.211175
2764.449243	151008.791052	56.216180
2763.401303	150718.765198	56.221185
2762.952541	150415.289121	56.226189
2762.580123	150120.242953	56.231194
2761.726995	149827.143906	56.236199
2761.523162	149527.373936	56.241204
2760.748460	149227.023584	56.246209
2760.427411	148911.823480	56.251213
2759.363796	148604.877844	56.256218
2758.948327	148303.640443	56.261223
2758.438917	147996.206185	56.266228
2757.483740	147687.943189	56.271233
2756.700961	147384.840947	56.276237
2756.009037	147081.968673	56.281242
2755.119589	146782.574525	56.286247
2754.760196	146473.491907	56.291252
2753.772682	146167.904856	56.296257
2753.548677	145868.032764	56.301261
2752.503738	145568.001298	56.306266
2751.740789	145259.985767	56.311271
2751.570061	144963.379781	56.316276
2750.618644	144663.939456	56.321281
2749.858126	144355.398788	56.326285
2749.367738	144053.070325	56.331290
2748.776041	143755.093964	56.336295
2747.855849	143446.613081	56.341300
2747.328669	143156.180199	56.346305
2746.760378	142841.563105	56.351309
2745.854732	142549.925254	56.356314
2744.966601	142246.800824	56.361319
2744.677223	141950.776321	56.366324
2743.645929	141654.656217	56.371329
2743.087107	141353.928111	56.376333
2742.432485	141047.335335	56.381338
2741.711618	140762.165400	56.386343
2741.060796	140456.098970	56.391348
2740.101169	140163.615958	56.396353
2739.826098	139855.971462	56.401357
2738.983379	139568.723069	56.406362
2738.101529	139264.954239	56.411367
2737.535941	138975.787297	56.416372
2736.610089	138677.926561	56.421377
2735.981378	138391.049489	56.426381
2735.544848	138109.379070	56.431386
2734.942949	137814.474006	56.436391
2734.264345	137520.498759	56.441396
2733.860823	137230.815033	56.446401
2733.269083	136933.693942	56.451405
2732.230617	136641.105739	56.456410
2731.686955	136342.585594	56.461415
2731.130627	136048.224640	56.466420
2730.492770	135758.973735	56.471425
2729.833229	135466.870856	56.476429
2729.318869	135167.837289	56.481434
2728.621115	134865.977636	56.486439
2728.190876	134572.958237	56.491444
2727.195826	134271.062988	56.496449
2726.654564	133977.101821	56.501453
2726.081258	133665.911161	56.506458
2724.871137	133374.132680	56.511463
2724.400295	133086.901873	56.516468
2723.917864	132791.546311	56.521473
2723.417274	132491.128521	56.526477
2722.677246	132204.520869	56.531482
2721.948803	131900.995318	56.536487
2721.598948	131591.494025	56.541492
2720.498616	131298.855784	56.546497
2720.122428	130994.179152	56.551501
2719.388277	130702.467132	56.556506
2718.626658	130401.007944	56.561511
2718.334672	130107.225287	56.566516
2717.607295	129805.271762	56.571521
2717.111217	129499.957252	56.576525
2716.328272	129209.538656	56.581530
2715.540226	128888.642566	56.586535
2715.021082	128595.115090	56.591540
2714.006351	128309.467219	56.596545
2713.450921	127992.621485	56.601549
2713.149299	127694.052594	56.606554
2712.075583	127396.942749	56.611559
2711.504021	127090.777873	56.616564
2711.037791	126798.556584	56.621569
2710.558160	126487.177083	56.626573
2709.478749	126187.465223	56.631578
2708.774438	125878.236374	56.636583
2708.797640	125571.791177	56.641588
2707.912317	125271.842813	56.646593
2707.164313	124971.202997	56.651597
2706.537040	124661.798083	56.656602
2705.697467	124361.471654	56.661607
2704.897245	124052.901157	56.666612
2704.183235	123744.015803	56.671617
2703.429958	123456.422106	56.676621
2702.715539	123158.197233	56.681626
2702.158101	122863.303035	56.686631
2701.676903	122553.124835	56.691636
2700.871465	122260.028896	56.696641
2700.289657	121956.349322	56.701645
2699.618589	121651.989037	56.706650
2698.834067	121344.768023	56.711655
2698.592576	121050.402666	56.716660
2697.640318	120739.266583	56.721665
2696.884588	120436.679589	56.726669
2696.265309	120137.826272	56.731674
2695.260779	119849.549927	56.736679
2695.086226	119537.092467	56.741684
2694.042142	119251.139716	56.746689
2693.396883	118939.690822	56.751693
2692.750929	118639.951204	56.756698
2691.926058	118354.494155	56.761703
2691.479230	118060.607755	56.766708
2690.968467	117768.391570	56.771713
2690.449772	117459.384338	56.776717
2689.541502	117153.755931	56.781722
2688.750944	116858.319147	56.786727
2688.573301	116554.334037	56.791732
2687.461965	116252.633150	56.796737
2686.758908	115959.934928	56.801741
2686.556753	115659.277619	56.806746
2685.599342	115359.892341	56.811751
2685.317112	115063.443828	56.816756
2684.343888	114765.489814	56.821761
2683.794661	114452.703141	56.826765
2683.198719	114151.827863	56.831770
2682.120349	113864.157493	56.836775
2681.605622	113556.739435	56.841780
2681.095733	113268.300417	56.846785
2680.353445	112953.075217	56.851789
2679.920012	112651.519516	56.856794
2678.799778	112362.825935	56.861799
2678.387765	112041.981583	56.866804
2677.426430	111759.939690	56.871809
2677.062879	111466.510351	56.876813
2676.345837	111170.075401	56.881818
2675.652386	110869.845439	56.886823
2675.234088	110557.296410	56.891828
2674.144911	110261.083673	56.896833
2673.800759	109960.206647	56.901837
2673.315638	109659.990212	56.906842
2672.344824	109356.694362	56.911847
2672.177568	109058.973158	56.916852
2671.309869	108756.023796	56.921857
2670.547045	108452.623775	56.926861
2669.843146	108152.638268	56.931866
2668.846677	107850.691437	56.936871
2668.493866	107554.204642	56.941876
2667.732957	107254.201257	56.946881
2666.755588	106950.276712	56.951885
2666.835540	106646.873730	56.956890
2665.706578	106349.090845	56.961895
2665.014645	106051.071119	56.966900
2664.271799	105746.287203	56.971905
2663.681093	105442.694870	56.976909
2663.158076	105154.277797	56.981914
2662.411359	104860.392807	56.986919
2661.982873	104548.989034	56.991924
2660.931040	104248.397033	56.996929
2660.332539	103954.772598	57.001933
2659.760429	103657.487155	57.006938
2659.030945	103365.711533	57.011943
2658.818420	103060.878155	57.016948
2657.788691	102760.035209	57.021953
2657.091995	102465.569492	57.026957
2656.197922	102162.092806	57.031962
2655.537694	101873.128663	57.036967
2654.934774	101563.714174	57.041972
2654.270886	101278.430830	57.046977
2653.573404	100977.057117	57.051981
2652.969618	100689.640153	57.056986
2652.492104	100388.734008	57.061991
2651.875067	100085.088332	57.066996
2650.818238	99795.990909	57.072001
2650.386611	99495.704406	57.077005
2649.680233	99198.465488	57.082010
2648.999522	98914.939247	57.087015
2648.756121	98604.346737	57.092020
2647.914824	98323.713779	57.097025
2647.068716	98010.935179	57.102029
2646.415011	97727.844331	57.107034
2645.706774	97428.459642	57.112039
2644.930675	97129.222838	57.117044
2644.163041	96837.205965	57.122049
2643.945022	96537.647546	57.127053
2643.343644	96244.806539	57.132058
2642.626349	95947.288378	57.137063
2641.801425	95650.070239	57.142068
2640.698195	95352.557675	57.147073
2640.435387	95053.888548	57.152077
2639.611516	94762.617742	57.157082
2638.947046	94471.503030	57.162087
2638.764329	94171.076413	57.167092
2637.510563	93884.457296	57.172097
2637.296684	93586.801949	57.177101
2636.732480	93294.678473	57.182106
2635.593432	93002.066553	57.187111
2635.239890	92697.539881	57.192116
2634.275766	92401.604553	57.197121
2633.961009	92107.187195	57.202125
2633.079830	91823.953381	57.207130
2632.544682	91537.929240	57.212135
2632.044910	91223.979565	57.217140
2631.005126	90943.191633	57.222145
2630.677312	90634.149674	57.227149
2630.114955	90346.179885	57.232154
2629.347206	90051.399048	57.237159
2628.899246	89751.626255	57.242164
2628.261833	89455.323892	57.247169
2627.302416	89156.122192	57.252173
2626.705683	88852.663846	57.257178
2626.034523	88556.810212	57.262183
2625.233760	88253.259468	57.267188
2624.618576	87959.624022	57.272193
2623.977932	87660.126254	57.277197
2623.411767	87367.353286	57.282202
2622.450876	87061.695661	57.287207
2622.226072	86761.269708	57.292212
2621.092913	86471.261287	57.297217
2620.680759	86167.386842	57.302221
2620.053631	85879.379137	57.307226
2619.469369	85590.278249	57.312231
2618.668724	85283.505039	57.317236
2617.640902	84996.079890	57.322241
2617.309964	84689.361273	57.327245
2616.918659	84396.493620	57.332250
2615.952578	84098.174987	57.337255
2615.264503	83803.663883	57.342260
2614.669316	83504.249055	57.347265
2614.204589	83210.604545	57.352269
2613.342373	82920.202496	57.357274
2612.447572	82622.850536	57.362279
2611.936884	82316.866777	57.367284
2611.257543	82042.343333	57.372289
2610.829366	81725.897790	57.377293
2610.325570	81438.279804	57.382298
2609.361493	81132.645102	57.387303
2608.723835	80847.572495	57.392308
2607.797499	80554.253965	57.397313
2607.275724	80250.716865	57.402317
2606.051285	79966.585885	57.407322
2605.535242	79675.660944	57.412327
2605.194649	79382.405642	57.417332
2604.441286	79098.066232	57.422337
2603.528903	78816.841981	57.427341
2603.091737	78523.468486	57.432346
2602.309494	78234.095256	57.437351
2601.491771	77943.413741	57.442356
2600.864856	77671.563406	57.447361
2600.413415	77375.433272	57.452365
2599.689152	77086.491653	57.457370
2598.641787	76801.445068	57.462375
2598.501335	76496.014949	57.467380
2597.738843	76228.095745	57.472385
2597.277569	75929.992392	57.477389
2596.729997	75650.623127	57.482394
2595.739290	75358.637472	57.487399
2595.287449	75069.415354	57.492404
2594.510458	74775.940742	57.497409
2594.149480	74490.494868	57.502413
2593.397210	74207.142379	57.507418
2592.562771	73908.114432	57.512423
2592.246473	73611.935694	57.517428
2591.399411	73325.791547	57.522433
2590.434134	73039.790602	57.527437
2589.927897	72747.297420	57.532442
2589.081948	72456.370057	57.537447
2588.615250	72167.185914	57.542452
2587.692887	71886.921342	57.547457
2587.217389	71589.182600	57.552461
2586.439261	71298.160132	57.557466
2585.471816	71012.391460	57.562471
2585.121758	70722.981901	57.567476
2584.452121	70444.699367	57.572481
2583.909889	70152.357924	57.577485
2583.322772	69869.832953	57.582490
2582.416580	69578.286148	57.587495
2582.063217	69295.783076	57.592500
2581.153811	69010.376360	57.597505
2580.728561	68720.412888	57.602509
2580.024291	68432.081324	57.607514
2579.041565	68145.159846	57.612519
2578.491296	67850.656400	57.617524
2578.080435	67569.574456	57.622529
2577.359715	67281.794556	57.627533
2576.782246	66996.608615	57.632538
2576.137663	66694.227708	57.637543
2575.516352	66416.663150	57.642548
2574.456766	66124.878988	57.647553
2574.008152	65842.213291	57.652557
2573.406702	65559.607633	57.657562
2572.550808	65263.327132	57.662567
2571.976296	64974.960090	57.667572
2571.333513	64682.419400	57.672577
2570.614175	64413.276956	57.677581
2570.143069	64112.162987	57.682586
2569.399672	63835.063563	57.687591
2568.728362	63529.463144	57.692596
2567.963143	63259.790221	57.697601
2567.172082	62960.457938	57.702605
2566.882899	62674.673321	57.707610
2565.939246	62390.073098	57.712615
2565.700008	62096.194443	57.717620
2564.630892	61804.623530	57.722625
2563.664165	61514.975091	57.727629
2563.082474	61230.692705	57.732634
2562.486584	60946.033838	57.737639
2561.904471	60668.660856	57.742644
2560.937099	60390.666137	57.747649
2560.214570	60113.342621	57.752653
2559.724554	59825.331857	57.757658
2558.826119	59544.898314	57.762663
2558.161312	59267.103421	57.767668
2557.535840	58999.162839	57.772673
2556.910225	58718.932715	57.777677
2556.509682	58439.278844	57.782682
2555.294869	58169.668010	57.787687
2555.070050	57880.904685	57.792692
2554.455787	57613.529876	57.797697
2553.236705	57337.912095	57.802701
2553.135320	57057.953164	57.807706
2552.210240	56784.202305	57.812711
2551.670324	56504.305463	57.817716
2551.172678	56213.544877	57.822721
2550.438969	55947.646790	57.827725
2549.676531	55682.121042	57.832730
2548.684077	55399.151320	57.837735
2548.160038	55122.130663	57.842740
2547.496212	54847.348331	57.847745
2546.516968	54583.806396	57.852749
2546.107546	54307.052087	57.857754
2545.428092	54044.710877	57.862759
2544.700839	53774.729769	57.867764
2544.059030	53499.780762	57.872769
2543.521450	53227.056491	57.877773
2543.181744	52951.662899	57.882778
2542.309081	52690.593264	57.887783
2541.677509	52403.914134	57.892788
2541.071618	52128.372780	57.897793
2540.279408	51867.413047	57.902797
2539.800992	51588.278152	57.907802
2538.558883	51322.174026	57.912807
2538.186095	51046.897041	57.917812
2537.678925	50777.568151	57.922817
2536.802183	50499.611154	57.927821
2536.074108	50227.225116	57.932826
2535.607124	49954.574069	57.937831
2535.002343	49691.800396	57.942836
2534.291964	49423.900276	57.947841
2533.300454	49164.131440	57.952845
2533.178086	48876.007666	57.957850
2532.397981	48611.193047	57.962855
2531.647393	48337.317916	57.967860
2530.712713	48074.047899	57.972865
2530.045190	47808.813044	57.977869
2529.490922	47531.483996	57.982874
2528.954364	47277.364469	57.987879
2528.347692	46996.259534	57.992884
2527.562793	46739.394120	57.997889
2526.430890	46466.029159	58.002893
2526.140799	46197.513507	58.007898
2525.215427	45938.983564	58.012903
2524.864587	45688.090067	58.017908
2524.104155	45414.211366	58.022913
2523.349558	45147.135965	58.027917
2522.887869	44877.203409	58.032922
2521.782580	44614.255836	58.037927
2521.253049	44359.567118	58.042932
2520.558592	44097.719748	58.047937
2519.727624	43836.328066	58.052941
2519.492037	43565.949912	58.057946
2518.720265	43334.960438	58.062951
2517.608681	43060.355386	58.067956
2516.880501	42794.608533	58.072961
2516.425854	42545.955667	58.077965
2515.578859	42283.258664	58.082970
2514.460487	42051.509625	58.087975
2514.207257	41786.629543	58.092980
2513.142921	41531.191326	58.097985
2512.427212	41291.628914	58.102989
2511.929884	41040.136586	58.107994
2511.040555	40809.746634	58.112999
2510.133084	40559.951619	58.118004
2509.395261	40333.292525	58.123009
2508.791521	40088.591145	58.128013
2508.590949	39853.393775	58.133018
2507.622589	39622.098059	58.138023
2506.938959	39384.647198	58.143028
2505.832346	39145.851856	58.148033
2505.165000	38919.390096	58.153037
2504.427093	38706.045690	58.158042
2503.620362	38471.293897	58.163047
2502.733798	38254.956307	58.168052
2501.331455	38035.328391	58.173057
2500.416433	37828.369733	58.178061
2499.575149	37631.635291	58.183066
2497.887163	37452.162343	58.188071
2497.130910	37250.431853	58.193076
2496.362388	37089.810142	58.198081
2495.527819	36914.211401	58.203085
2494.542626	36739.234257	58.208090
2493.552794	36580.052911	58.213095
2492.868169	36411.154743	58.218100
2492.148616	36274.549889	58.223105
2491.114738	36117.105889	58.228109
2490.659648	35964.984938	58.233114
2489.308087	35826.200058	58.238119
2488.664294	35693.640381	58.243124
2488.063020	35542.308247	58.248129
2487.162181	35417.191371	58.253133
2486.621470	35273.525300	58.258138
2485.926066	35160.414616	58.263143
2485.519430	35014.317746	58.268148
2484.306614	34906.119057	58.273153
2483.895459	34774.383229	58.278157
2483.380391	34636.904334	58.283162
2482.260775	34516.323573	58.288167
2481.941484	34387.338773	58.293172
2481.000495	34270.606574	58.298177
2480.279911	34152.557004	58.303181
2480.078813	34028.316295	58.308186
2479.088130	33920.626125	58.313191
2478.773779	33792.925225	58.318196
2477.785801	33674.900896	58.323201
2477.352364	33560.081270	58.328205
2476.929259	33435.862803	58.333210
2475.723206	33323.798480	58.338215
2475.470722	33194.278219	58.343220
2475.102454	33086.392085	58.348225
2474.144283	32978.268318	58.353229
2473.654862	32841.388079	58.358234
2473.074983	32729.658341	58.363239
2472.505069	32602.836747	58.368244
2472.027814	32485.044924	58.373249
2471.023545	32358.028594	58.378253
2470.757508	32229.056887	58.383258
2469.964206	32112.502959	58.388263
2469.805072	31990.982448	58.393268
2469.119621	31876.072258	58.398273
2468.096493	31743.909229	58.403277
2467.408097	31612.844523	58.408282
2466.914284	31498.919442	58.413287
2466.232335	31361.224016	58.418292
2465.190604	31247.281675	58.423297
2464.548767	31130.094468	58.428301
2464.356529	30996.859267	58.433306
2463.244969	30891.845158	58.438311
2462.920313	30781.707735	58.443316
2462.469095	30645.157287	58.448321
2461.608750	30531.496114	58.453325
2461.138638	30405.453013	58.458330
2460.464736	30291.876128	58.463335
2459.659623	30151.437509	58.468340
2459.168394	30036.773273	58.473345
2458.537438	29912.529032	58.478349
2458.099982	29758.906093	58.483354
2457.266812	29662.254709	58.488359
2456.582885	29540.145127	58.493364
2455.955440	29405.601552	58.498369
2455.151404	29291.709420	58.503373
2454.510442	29157.029431	58.508378
2453.989963	29038.585139	58.513383
2453.307674	28905.272473	58.518388
2452.279018	28784.191667	58.523393
2451.976507	28669.930529	58.528397
2451.722329	28539.946471	58.533402
2450.600982	28426.184962	58.538407
2449.748792	28304.048147	58.543412
2449.365785	28173.619826	58.548417
2448.737006	28051.158817	58.553421
2448.011141	27940.788244	58.558426
2447.369875	27809.130513	58.563431
2446.684379	27682.611850	58.568436
2445.980834	27559.694072	58.573441
2444.988313	27444.588124	58.578445
2444.629553	27323.701121	58.583450
2444.117116	27206.268105	58.588455
2443.299762	27072.672837	58.593460
2442.635975	26953.926086	58.598465
2442.117611	26832.361167	58.603469
2441.552097	26705.359614	58.608474
2440.911948	26587.691499	58.613479
2440.134342	26452.659187	58.618484
2439.417466	26345.623982	58.623489
2438.839335	26228.385424	58.628493
2438.377513	26103.055243	58.633498
2437.541879	25987.842430	58.638503
2436.838606	25860.222557	58.643508
2436.754714	25739.795896	58.648513
2435.663775	25603.921633	58.653517
2435.126847	25484.281875	58.658522
2434.346756	25352.449844	58.663527
2433.726904	25233.462437	58.668532
2432.827839	25110.032866	58.673537
2432.251030	24983.966770	58.678541
2431.724014	24866.833518	58.683546
2430.999765	24743.548853	58.688551
2430.367656	24620.036517	58.693556
2429.822259	24489.517701	58.698561
2428.767194	24370.007122	58.703565
2428.379162	24241.059015	58.708570
2427.909957	24130.731576	58.713575
2427.337722	24003.397142	58.718580
2426.524189	23878.565788	58.723585
2425.664168	23758.557435	58.728589
2425.305322	23617.278971	58.733594
2424.566991	23504.767725	58.738599
2423.717952	23382.515458	58.743604
2423.089061	23259.187679	58.748609
2422.248729	23136.259197	58.753613
2422.074646	23006.276429	58.758618
2420.974256	22896.798306	58.763623
2420.397456	22766.434421	58.768628
2419.961215	22642.459456	58.773633
2418.904950	22521.148431	58.778637
2418.747733	22394.992890	58.783642
2417.951665	22270.660973	58.788647
2417.146747	22148.498878	58.793652
2416.624465	22036.173837	58.798657
2416.032832	21910.196053	58.803661
2415.661158	21784.654988	58.808666
2414.667619	21668.345697	58.813671
2413.888270	21533.097170	58.818676
2413.289003	21405.585763	58.823681
2412.239862	21287.315786	58.828685
2411.629804	21173.666986	58.833690
2410.967495	21041.708373	58.838695
2409.874953	20927.990993	58.843700
2409.849279	20818.763499	58.848705
2408.919046	20687.218657	58.853709
2408.599881	20574.012044	58.858714
2407.900108	20459.477450	58.863719
2407.114972	20335.565278	58.868724
2407.075865	20204.203334	58.873729
2405.804680	20079.395616	58.878733
2405.266444	19961.329362	58.883738
2404.449801	19845.190656	58.888743
2403.767518	19727.312823	58.893748
2403.491563	19608.022647	58.898753
2402.336010	19489.901119	58.903757
2402.112247	19360.271686	58.908762
2401.264452	19247.002559	58.913767
2400.631474	19117.556862	58.918772
2399.947276	18988.867955	58.923777
2399.030612	18882.495494	58.928781
2398.483781	18760.005046	58.933786
2397.920298	18657.126195	58.938791
2397.365012	18529.958820	58.943796
2396.457022	18412.348135	58.948801
2395.592989	18293.751722	58.953805
2395.275496	18160.578233	58.958810
2394.705017	18048.329271	58.963815
2393.975917	17928.370710	58.968820
2393.463194	17799.849156	58.973825
2392.566828	17699.035624	58.978829
2391.726487	17578.323625	58.983834
2391.104812	17473.692864	58.988839
2390.434097	17347.153777	58.993844
2389.707089	17242.183901	58.998849
2388.758299	17127.749376	59.003853
2388.337403	17004.455956	59.008858
2387.679934	16893.483399	59.013863
2387.156490	16783.749163	59.018868
2386.261585	16664.547328	59.023873
2385.513470	16540.366650	59.028877
2385.169782	16431.311663	59.033882
2384.593901	16330.446562	59.038887
2383.705459	16210.852752	59.043892
2383.310215	16096.829623	59.048897
2382.396717	15993.348713	59.053901
2381.878476	15862.023620	59.058906
2381.273064	15762.819267	59.063911
2380.194713	15650.495775	59.068916
2379.641056	15522.242043	59.073921
2378.923054	15430.590190	59.078925
2378.036958	15320.625331	59.083930
2377.372701	15213.152356	59.088935
2376.931957	15110.627847	59.093940
2375.994695	14989.499133	59.098945
2375.147869	14898.155699	59.103949
2374.759036	14795.705563	59.108954
2374.035576	14675.509191	59.113959
2373.451455	14579.090700	59.118964
2372.878124	14472.575278	59.123969
2372.202927	14377.349008	59.128973
2371.275199	14266.193398	59.133978
2370.707497	14169.280453	59.138983
2369.778104	14058.790029	59.143988
2369.203406	13967.492156	59.148993
2368.235142	13875.309906	59.153997
2367.931369	13763.331886	59.159002
2366.931582	13684.568941	59.164007
2366.236115	13576.378476	59.169012
2365.456738	13486.636844	59.174017
2364.873685	13386.163924	59.179021
2364.432493	13289.389200	59.184026
2363.599461	13217.244762	59.189031
2362.879035	13113.168333	59.194036
2362.388442	13027.538809	59.199041
2361.437155	12929.702819	59.204045
2361.142994	12850.665296	59.209050
2360.320608	12753.053446	59.214055
2359.590117	12649.264290	59.219060
2359.159120	12553.938869	59.224065
2358.057594	12471.397505	59.229069
2357.341836	12384.034786	59.234074
2356.609884	12296.853078	59.239079
2356.253890	12200.335525	59.244084
2355.457057	12125.894675	59.249089
2354.643132	12038.007809	59.254093
2354.129124	11949.806198	59.259098
2353.743324	11864.731586	59.264103
2352.384038	11785.548737	59.269108
2351.925097	11692.003433	59.274113
2351.129081	11606.996108	59.279117
2350.719274	11522.709180	59.284122
2349.761768	11433.806447	59.289127
2349.014529	11364.232477	59.294132
2348.865195	11276.295733	59.299137
2347.816179	11203.022417	59.304141
2347.421919	11122.052762	59.309146
2346.640626	11032.896020	59.314151
2345.933701	10966.601621	59.319156
2345.655777	10881.759631	59.324161
2344.818468	10799.419240	59.329165
2344.102224	10708.535622	59.334170
2343.473637	10635.990951	59.339175
2342.740867	10553.296843	59.344180
2342.215294	10463.957339	59.349185
2340.881645	10390.458541	59.354189
2340.727926	10312.307300	59.359194
2339.991401	10225.332948	59.364199
2339.202396	10146.683288	59.369204
2338.731289	10067.276307	59.374209
2337.885571	9998.372009	59.379213
2337.473230	9910.499131	59.384218
2336.517977	9859.554411	59.389223
2335.731779	9766.690697	59.394228
2335.042305	9692.781913	59.399233
2334.277015	9617.591632	59.404237
2333.983901	9547.066072	59.409242
2333.308782	9472.031449	59.414247
2332.103424	9405.385307	59.419252
2332.011927	9320.411307	59.424257
2331.162576	9258.952645	59.429261
2330.509490	9175.538706	59.434266
2329.682131	9113.871241	59.439271
2329.126226	9041.850138	59.444276
2328.772169	8963.135730	59.449281
2327.808281	8895.395625	59.454285
2327.270640	8814.447713	59.459290
2326.549893	8736.161468	59.464295
2325.736829	8687.846157	59.469300
2324.932994	8605.570473	59.474305
2324.108733	8545.509880	59.479309
2323.785526	8462.540266	59.484314
2323.005446	8409.237977	59.489319
2322.475370	8342.463845	59.494324
2321.807418	8263.533887	59.499329
2321.294617	8199.317581	59.504333
2320.826305	8133.891459	59.509338
2320.136842	8056.344174	59.514343
2319.284582	7988.795193	59.519348
2318.925792	7914.175762	59.524353
2317.712010	7839.887935	59.529357
2317.403133	7770.829084	59.534362
2316.484415	7705.963389	59.539367
2315.670033	7628.518604	59.544372
2315.295432	7560.386216	59.549377
2314.459549	7509.285833	59.554381
2314.047273	7442.669015	59.559386
2313.320005	7366.884117	59.564391
2312.607078	7298.726121	59.569396
2311.892395	7236.978736	59.574401
2311.209215	7173.714433	59.579405
2310.707056	7089.694621	59.584410
2310.018207	7018.168983	59.589415
2309.092829	6951.610497	59.594420
2308.760250	6884.155287	59.599425
2307.908147	6824.599849	59.604429
2307.444271	6745.661348	59.609434
2306.933641	6676.372167	59.614439
2306.009082	6617.348872	59.619444
2305.380517	6548.806260	59.624449
2304.784580	6492.021998	59.629453
2304.130140	6411.493747	59.634458
2303.079886	6345.017738	59.639463
2302.140078	6295.403576	59.644468
2302.313680	6225.274421	59.649473
2301.138301	6155.472336	59.654477
2300.348190	6090.103088	59.659482
2300.115341	6029.543186	59.664487
2299.514475	5971.523342	59.669492
2298.947845	5899.097941	59.674497
2297.731807	5829.758957	59.679501
2297.342529	5773.335899	59.684506
2296.871019	5699.781094	59.689511
2295.942112	5648.701095	59.694516
2295.378236	5567.756868	59.699521
2294.679284	5515.412003	59.704525
2294.017073	5442.991376	59.709530
2293.426485	5393.167903	59.714535
2292.738454	5319.922230	59.719540
2292.350229	5258.181799	59.724545
2291.441052	5197.236465	59.729549
2290.633692	5134.990414	59.734554
2290.051545	5063.036916	59.739559
2289.200592	5006.919523	59.744564
2288.836889	4934.887048	59.749569
2287.699585	4886.243569	59.754573
2287.411835	4813.385699	59.759578
2286.705239	4757.705385	59.764583
2285.912940	4694.536033	59.769588
2285.370365	4631.330499	59.774593
2284.492181	4568.448197	59.779597
2283.944822	4501.887329	59.784602
2283.378620	4447.648139	59.789607
2282.526590	4395.726663	59.794612
2282.313814	4336.646135	59.799617
2281.568370	4268.075076	59.804621
2281.059565	4209.293597	59.809626
2280.362315	4150.740196	59.814631
2279.774629	4083.505423	59.819636
2279.122311	4018.064362	59.824641
2278.068685	3948.887510	59.829645
2277.864410	3878.187460	59.834650
2276.886907	3823.533946	59.839655
2275.989086	3757.407432	59.844660
2275.246608	3695.009714	59.849665
2274.604194	3637.071114	59.854669
2274.046026	3574.467233	59.859674
2273.803414	3523.785765	59.864679
2272.813275	3462.730347	59.869684
2272.188551	3399.230849	59.874689
2271.214898	3348.171471	59.879693
2270.936249	3275.320568	59.884698
2270.234491	3220.560116	59.889703
2269.477203	3159.429601	59.894708
2268.748392	3100.727680	59.899713
2268.060331	3040.838201	59.904718
2267.620686	2977.848216	59.909722
2266.687949	2912.287812	59.914727
2266.174220	2864.177507	59.919732
2265.619803	2798.443262	59.924737
2264.838369	2743.351833	59.929742
2264.282402	2675.606696	59.934746
2263.566933	2618.580339	59.939751
2262.821432	2557.127156	59.944756
2261.911327	2499.147992	59.949761
2261.237127	2443.905051	59.954766
2260.503975	2395.595311	59.959770
2260.104597	2339.048253	59.964775
2259.603421	2286.938249	59.969780
2258.895410	2220.523626	59.974785
2258.249090	2164.879885	59.979790
2257.438723	2105.632662	59.984794
2257.074258	2056.747486	59.989799
2256.207718	1990.869248	59.994804
2255.604862	1933.681039	59.999809
2254.666458	1878.709249	60.004814
2254.157141	1826.483114	60.009818
2253.672502	1766.829973	60.014823
2252.888174	1708.741749	60.019828
2252.401636	1650.100286	60.024833
2251.480396	1594.123840	60.029838
2250.552309	1538.542958	60.034842
2250.150350	1485.955644	60.039847
2249.172418	1424.150640	60.044852
2248.879491	1388.616217	60.049857
2248.294137	1333.672495	60.054862
2247.702243	1277.406900	60.059866
2246.857606	1217.757918	60.064871
2246.139456	1164.315139	60.069876
2245.522012	1114.322831	60.074881
2244.791720	1063.060979	60.079886
2243.659245	1005.177454	60.084890
2243.405329	947.375582	60.089895
2242.385214	907.122655	60.094900
2241.792035	859.710468	60.099905
2241.371391	822.992880	60.104910
2240.618588	759.691572	60.109914
2239.912541	701.068261	60.114919
2238.977223	668.427135	60.119924
2238.753540	607.895268	60.124929
2238.042064	571.867843	60.129934
2237.399995	510.566969	60.134938
2236.667125	469.520654	60.139943
2235.828637	426.248820	60.144948
2235.338359	374.620968	60.149953
2234.815565	336.066360	60.154958
2234.040839	280.451789	60.159962
2233.352411	241.991513	60.164967
2232.545759	196.695300	60.169972
2231.766902	148.608445	60.174977
2230.867488	125.928841	60.179982
2229.790962	83.299746	60.184986
2229.394162	43.588997	60.189991
2228.208585	9.573020	60.194996
2227.287812	-16.278808	60.200001
2226.466162	-23.819855	60.205006
2223.580307	12.302330	60.210010
2220.449815	82.831665	60.215015
2220.453720	74.391667	60.220020
2221.591019	87.799436	60.225025
2221.901152	86.506202	60.230030
2221.466267	70.213520	60.235034
2221.041000	76.167630	60.240039
2220.773794	76.016187	60.245044
2220.073158	73.626512	60.250049
2219.180271	79.235350	60.255054
2218.070575	85.127730	60.260058
2217.118260	84.078912	60.265063
2216.054960	91.457250	60.270068
2215.599481	77.067982	60.275073
2215.182235	90.238245	60.280078
2215.133439	89.889736	60.285082
2214.636640	90.687733	60.290087
2213.488085	90.617756	60.295092
2212.685651	85.281254	60.300097
2212.593578	87.483133	60.305102
2211.852622	86.968468	60.310106
2211.336088	83.991370	60.315111
2210.220559	83.838888	60.320116
2209.959421	91.370665	60.325121
2208.447341	99.935062	60.330126
2208.109568	86.313983	60.335130
2208.181264	88.095661	60.340135
2207.222806	88.342446	60.345140
2206.606679	83.422652	60.350145
2205.673204	88.883400	60.355150
2205.049916	96.072099	60.360154
2205.163126	78.626489	60.365159
2204.563164	95.400548	60.370164
2203.169754	72.118194	60.375169
2202.576650	86.623591	60.380174
2202.103768	86.813848	60.385178
2201.619102	75.537265	60.390183
2200.752859	85.870970	60.395188
2199.867525	84.584460	60.400193
2199.086053	83.166361	60.405198
2198.348593	84.322648	60.410202
2198.311362	83.929729	60.415207
2197.880891	96.622721	60.420212
2196.732942	82.111504	60.425217
2196.290519	84.845182	60.430222
2195.547065	89.490498	60.435226
2195.129285	80.472446	60.440231
2194.198213	81.780868	60.445236
2193.497873	82.883960	60.450241
2192.866991	86.683551	60.455246
2191.915729	83.045324	60.460250
2191.805445	84.784909	60.465255
2190.768856	91.279114	60.470260
2190.240561	80.034683	60.475265
2189.268397	86.879773	60.480270
2188.418095	85.026337	60.485274
2188.511584	79.976629	60.490279
2188.042216	76.783906	60.495284
2186.995953	85.499903	60.500289
2186.027168	82.268141	60.505294
2185.945608	81.044927	60.510298
2185.644553	81.121199	60.515303
2183.919769	89.821844	60.520308
2183.852480	71.968082	60.525313
2183.368906	84.086040	60.530318
2182.211382	84.883211	60.535322
2181.556155	76.361709	60.540327
2181.200673	84.056677	60.545332
2180.470375	81.364225	60.550337
2180.005177	77.508549	60.555342
2179.212179	86.231675	60.560346
2178.951949	85.609217	60.565351
2177.268318	85.102193	60.570356
2176.905356	81.066301	60.575361
2176.645811	79.412450	60.580366
2175.810697	87.098360	60.585370
2175.316315	88.182974	60.590375
2174.303819	83.305573	60.595380
2173.774616	79.144674	60.600385
2173.221889	85.675655	60.605390
2172.523402	80.382600	60.610394
2172.051490	71.768947	60.615399
2171.092638	89.196000	60.620404
2170.423604	75.472961	60.625409
2169.917155	82.393974	60.630414
2169.416520	78.014088	60.635418
2168.840677	74.059280	60.640423
2167.995159	88.221542	60.645428
2167.259199	82.980163	60.650433
2166.943487	78.503134	60.655438
2166.005476	74.383443	60.660442
2165.396126	78.178044	60.665447
2164.798435	71.796720	60.670452
2164.276140	73.440828	60.675457
2163.039036	76.532388	60.680462
2162.529760	74.678473	60.685466
2162.234141	69.712578	60.690471
2161.452827	70.235614	60.695476
2160.544617	61.563461	60.700481
2159.809304	74.736866	60.705486
2159.516431	73.726944	60.710490
2159.231680	79.748651	60.715495
2157.367062	83.739253	60.720500
2157.186400	82.375652	60.725505
2157.346351	70.154758	60.730510
2156.017650	84.258065	60.735514
2155.217584	81.434769	60.740519
2154.665773	84.192114	60.745524
2154.297427	92.143008	60.750529
2153.471041	82.434463	60.755534
2152.899184	87.508284	60.760538
2152.194286	80.852245	60.765543
2151.170672	81.841063	60.770548
2151.259486	75.730854	60.775553
2150.345832	83.511226	60.780558
2149.398936	84.289186	60.785562
2148.763941	74.655934	60.790567
2148.224911	93.011404	60.795572
2147.602516	73.027038	60.800577
2146.920008	82.382316	60.805582
2146.105404	80.458579	60.810586
2145.873379	77.108365	60.815591
2145.056744	82.012873	60.820596
2144.410987	79.985080	60.825601
2144.115259	80.853686	60.830606
2143.258926	77.943132	60.835610
2142.138260	72.653996	60.840615
2141.093183	80.076768	60.845620
2141.317631	81.744323	60.850625
2140.311287	74.770280	60.855630
2139.224282	84.621805	60.860634
2139.135466	76.972352	60.865639
2138.475685	78.769160	60.870644
2137.734032	85.503579	60.875649
2137.164117	72.761423	60.880654
2136.294512	80.667267	60.885658
2136.233447	85.229557	60.890663
2135.604657	76.885218	60.895668
2134.754480	80.938800	60.900673
2133.695418	74.707954	60.905678
2132.542845	84.825340	60.910682
2132.689530	73.957942	60.915687
2131.552780	75.702701	60.920692
2130.647022	82.936223	60.925697
2130.680269	65.585325	60.930702
2130.045068	75.724692	60.935706
2129.346768	79.199114	60.940711
2128.667066	80.691592	60.945716
2128.154278	78.106565	60.950721
2127.497818	73.078084	60.955726
2126.690355	71.104338	60.960730
2125.722810	79.084068	60.965735
2124.623441	76.656765	60.970740
2124.845984	77.428948	60.975745
2123.925783	79.170890	60.980750
2122.727687	80.433397	60.985754
2122.295254	67.128566	60.990759
2121.798327	80.456537	60.995764
2121.667373	81.171273	61.000769
2120.806903	71.012437	61.005774
2120.037167	76.160232	61.010778
2119.768625	76.447386	61.015783
2118.804378	74.512711	61.020788
2118.551330	71.905398	61.025793
2117.458692	69.964288	61.030798
2116.387440	83.646729	61.035802
2115.935212	79.162985	61.040807
2115.308673	75.651455	61.045812
2114.684346	80.016122	61.050817
2114.477905	79.134411	61.055822
2113.661152	73.888527	61.060826
2112.779011	67.331590	61.065831
2111.576700	74.498631	61.070836
2110.699717	80.098667	61.075841
2110.583267	60.100287	61.080846
2110.292526	75.342990	61.085850
2109.653387	70.382727	61.090855
2108.784725	62.771873	61.095860
2108.228802	71.405350	61.100865
2107.906446	65.970643	61.105870
2107.042427	66.303399	61.110874
2106.091531	72.328306	61.115879
2105.307504	76.179019	61.120884
2104.680120	77.759391	61.125889
2104.326290	72.014299	61.130894
2103.254497	76.688077	61.135898
2103.301863	71.609425	61.140903
2102.452042	76.035103	61.145908
2101.762641	77.453436	61.150913
2100.921807	59.547415	61.155918
2099.898781	78.905296	61.160922
2099.112487	69.408031	61.165927
2098.700848	75.210185	61.170932
2097.947859	81.973216	61.175937
2097.590169	77.114945	61.180942
2097.012641	68.671031	61.185946
2096.526020	72.126062	61.190951
2095.930772	71.209857	61.195956
2094.910962	64.550200	61.200961
2093.909689	68.470077	61.205966
2092.984547	78.622343	61.210970
2093.546104	74.401923	61.215975
2092.325404	73.514005	61.220980
2091.574457	72.870078	61.225985
2091.069983	73.476935	61.230990
2090.465783	74.314072	61.235994
2090.097841	78.158687	61.240999
2088.598687	75.280772	61.246004
2088.086202	67.468332	61.251009
2087.358580	70.792879	61.256014
2086.658306	69.469161	61.261018
2086.609540	71.635783	61.266023
2085.767245	79.147814	61.271028
2085.400584	67.978698	61.276033
2085.147397	73.153340	61.281038
2083.731115	80.694954	61.286042
2083.168373	66.765866	61.291047
2082.314745	75.894425	61.296052
2081.728081	75.777920	61.301057
2081.308725	70.281340	61.306062
2080.680297	71.732578	61.311066
2080.076229	66.825105	61.316071
2078.757908	68.149284	61.321076
2077.957774	63.591455	61.326081
2077.600550	69.325053	61.331086
2076.807713	63.072493	61.336090
2076.635464	65.324937	61.341095
2075.647081	73.596555	61.346100
2075.299303	68.765102	61.351105
2075.027310	70.669115	61.356110
2074.189708	79.900787	61.361114
2073.235991	73.697405	61.366119
2072.226181	78.936923	61.371124
2071.698437	68.154479	61.376129
2071.406237	79.489897	61.381134
2070.665467	69.826154	61.386138
2070.309919	71.177325	61.391143
2069.002592	77.173653	61.396148
2067.895301	66.216684	61.401153
2067.792942	60.456929	61.406158
2067.013206	69.345113	61.411162
2066.540776	58.932353	61.416167
2066.124174	72.394222	61.421172
2065.306995	73.200510	61.426177
2064.853205	71.329926	61.431182
2064.058940	79.192293	61.436186
2063.133230	74.913003	61.441191
2062.468870	76.699517	61.446196
2061.997600	75.148661	61.451201
2061.726193	74.332455	61.456206
2060.923727	76.569798	61.461210
2060.225260	73.328307	61.466215
2059.051603	73.274996	61.471220
2058.405786	81.274651	61.476225
2057.794678	75.335437	61.481230
2057.414769	78.740427	61.486234
2057.113818	72.837148	61.491239
2056.328626	84.469989	61.496244
2055.567278	74.315950	61.501249
2054.845536	67.735159	61.506254
2053.740930	84.666561	61.511258
2053.246921	67.749415	61.516263
2052.903416	70.864788	61.521268
2052.175074	71.187069	61.526273
2052.107339	72.196114	61.531278
2050.597815	71.298859	61.536282
2049.900547	69.433802	61.541287
2049.157193	58.870084	61.546292
2048.559202	59.915970	61.551297
2048.288545	69.844535	61.556302
2047.580918	61.254136	61.561306
2046.969063	77.708383	61.566311
2045.805161	66.154887	61.571316
2045.186332	70.750494	61.576321
2044.817792	67.574917	61.581326
2044.233076	74.711780	61.586330
2043.962038	67.778783	61.591335
2043.542024	71.551244	61.596340
2042.075264	74.553150	61.601345
2041.452127	72.611678	61.606350
2040.520340	73.401470	61.611354
2040.064404	71.163817	61.616359
2039.585291	77.246333	61.621364
2039.200370	77.723845	61.626369
2038.149484	77.632136	61.631374
2036.942816	84.246414	61.636378
2036.343998	69.173517	61.641383
2035.839137	71.909238	61.646388
2035.380969	79.308284	61.651393
2035.174188	69.767960	61.656398
2034.706972	74.052516	61.661402
2034.147513	71.649952	61.666407
2033.446846	63.839010	61.671412
2032.257789	74.988763	61.676417
2031.979111	58.478990	61.681422
2031.189452	70.855246	61.686426
2030.163278	68.932011	61.691431
2028.581174	78.026388	61.696436
2028.661889	78.469426	61.701441
2029.019210	68.614086	61.706446
2027.586581	86.807025	61.711450
2026.924127	70.999938	61.716455
2026.056218	79.839055	61.721460
2025.421382	70.803463	61.726465
2025.145051	71.322087	61.731470
2024.574198	65.676107	61.736474
2023.473071	78.309950	61.741479
2022.653115	86.810315	61.746484
2021.933477	77.917483	61.751489
2021.586361	72.907746	61.756494
2021.075478	81.108333	61.761498
2020.789123	72.525193	61.766503
2020.290299	72.427876	61.771508
2019.089527	79.683015	61.776513
2018.360943	75.027119	61.781518
2017.693660	82.803117	61.786522
2017.065684	80.878187	61.791527
2016.749937	71.353583	61.796532
2015.946963	77.859645	61.801537
2014.889983	71.060847	61.806542
2013.993868	82.867410	61.811546
2013.406693	73.357498	61.816551
2012.993443	83.217243	61.821556
2012.797201	75.206403	61.826561
2012.240217	73.547740	61.831566
2011.405041	82.149865	61.836570
2010.659203	75.033616	61.841575
2009.911879	76.404396	61.846580
2009.364982	80.663758	61.851585
2008.934112	74.244966	61.856590
2007.801780	84.494791	61.861594
2007.267704	75.570938	61.866599
2006.262162	80.033973	61.871604
2005.592661	77.547959	61.876609
2005.317239	69.270582	61.881614
2004.585357	70.965328	61.886618
2004.318811	74.787550	61.891623
2003.423586	68.522880	61.896628
2002.567314	72.407161	61.901633
2002.078108	74.656300	61.906638
2001.339388	76.766853	61.911642
2000.891290	72.813891	61.916647
1999.515002	77.715798	61.921652
1998.993862	76.030950	61.926657
1998.552297	64.058500	61.931662
1997.985113	69.215173	61.936666
1997.590128	69.536599	61.941671
1997.116330	69.649770	61.946676
1996.390773	81.137542	61.951681
1995.409327	76.619553	61.956686
1994.578981	88.644334	61.961690
1994.285150	74.026069	61.966695
1993.262842	66.649371	61.971700
1992.300701	67.803526	61.976705
1991.782469	61.753408	61.981710
1990.948325	78.317053	61.986714
1990.799350	59.169078	61.991719
1990.245974	66.502811	61.996724
1989.837382	72.520524	62.001729
1989.097776	66.724726	62.006734
1987.765612	71.605442	62.011738
1986.969664	58.990686	62.016743
1986.539653	70.064129	62.021748
1985.857706	78.479518	62.026753
1985.774321	58.392350	62.031758
1985.145162	67.818020	62.036762
1983.760183	71.790952	62.041767
1983.136919	69.184071	62.046772
1982.588773	72.376083	62.051777
1982.511570	56.630676	62.056782
1981.544215	72.024912	62.061786
1981.084856	72.145256	62.066791
1980.496359	62.977755	62.071796
1979.394456	78.546312	62.076801
1978.847718	70.282042	62.081806
1978.487539	69.028948	62.086810
1977.669315	69.064331	62.091815
1976.583405	71.646293	62.096820
1975.658998	78.715664	62.101825
1975.056184	61.997165	62.106830
1974.153553	74.708318	62.111834
1974.263100	73.779619	62.116839
1973.850541	67.189205	62.121844
1973.474047	71.987625	62.126849
1972.850616	77.799754	62.131854
1971.988288	82.415104	62.136858
1971.403643	72.452240	62.141863
1970.331384	63.766785	62.146868
1969.327976	74.734134	62.151873
1969.038630	67.107074	62.156878
1968.252938	76.486638	62.161882
1967.929186	69.292374	62.166887
1967.017792	74.793835	62.171892
1965.883006	82.410666	62.176897
1965.330324	71.397257	62.181902
1964.690159	68.359421	62.186906
1964.534103	73.066085	62.191911
1964.285792	75.534026	62.196916
1963.183550	72.495420	62.201921
1962.435111	61.607704	62.206926
1961.398791	66.466702	62.211930
1961.154801	69.247756	62.216935
1960.571553	58.482050	62.221940
1959.177733	69.359986	62.226945
1958.620418	65.407025	62.231950
1958.197962	72.634833	62.236954
1957.623299	70.058089	62.241959
1957.117716	76.800799	62.246964
1956.740989	71.429938	62.251969
1956.486034	65.921484	62.256974
1954.878870	81.833590	62.261978
1954.442616	71.990673	62.266983
1954.462244	62.780269	62.271988
1952.961963	73.115315	62.276993
1952.095842	61.861523	62.281998
1951.391266	74.292095	62.287002
1950.910669	63.141104	62.292007
1950.800859	60.706610	62.297012
1950.146631	73.469797	62.302017
1949.349137	65.387260	62.307022
1948.167029	67.065180	62.312026
1947.632146	71.541829	62.317031
1947.187780	64.682093	62.322036
1946.817065	72.040454	62.327041
1946.400744	63.798072	62.332046
1944.969063	62.497456	62.337050
1944.189373	70.456874	62.342055
1943.743957	64.582858	62.347060
1943.302816	69.670649	62.352065
1943.013975	55.132046	62.357070
1941.659817	69.078611	62.362074
1940.902560	74.837874	62.367079
1940.308461	61.957718	62.372084
1939.811106	59.439669	62.377089
1939.737161	60.596351	62.382094
1938.788450	73.712198	62.387098
1937.957225	64.521742	62.392103
1937.282114	51.719107	62.397108
1936.710071	64.606430	62.402113
1936.263936	53.629745	62.407118
1934.994597	63.712101	62.412122
1934.233562	57.812500	62.417127
1933.474565	70.628584	62.422132
1933.250696	71.019047	62.427137
1932.584722	58.730598	62.432142
1932.163958	75.966610	62.437146
1931.550408	58.984921	62.442151
1930.824257	69.383162	62.447156
1929.647008	63.309944	62.452161
1929.348259	60.090196	62.457166
1928.496950	70.828414	62.462170
1928.628226	54.360828	62.467175
1927.550647	62.323379	62.472180
1926.449177	68.511005	62.477185
1926.147790	60.579953	62.482190
1925.501592	60.100789	62.487194
1924.710779	59.543662	62.492199
1923.768653	67.814284	62.497204
1922.998353	65.459408	62.502209
1922.951270	66.405255	62.507214
1922.391947	73.806173	62.512218
1921.854665	62.758803	62.517223
1920.826241	61.081964	62.522228
1919.638974	73.428321	62.527233
1919.277262	68.498189	62.532238
1918.804039	63.155272	62.537242
1918.358169	66.807277	62.542247
1917.800278	57.743747	62.547252
1916.421127	66.954183	62.552257
1916.077415	57.804617	62.557262
1915.726166	67.547285	62.562266
1915.125579	67.772057	62.567271
1914.614464	56.971264	62.572276
1913.428684	65.897126	62.577281
1913.295978	60.839186	62.582286
1911.930112	64.930536	62.587290
1911.031490	69.058096	62.592295
1910.631436	63.725642	62.597300
1909.969974	65.311466	62.602305
1909.361239	70.446365	62.607310
1909.110307	65.823488	62.612314
1909.025435	71.731473	62.617319
1907.886047	60.246706	62.622324
1906.653504	74.110907	62.627329
1906.058184	63.299825	62.632334
1905.979505	74.147198	62.637338
1904.482670	61.976463	62.642343
1903.652923	65.173769	62.647348
1903.074882	64.314801	62.652353
1902.820789	64.498762	62.657358
1902.521750	59.314270	62.662362
1902.055270	63.762719	62.667367
1901.736779	67.506464	62.672372
1900.038135	69.794659	62.677377
1899.826690	61.404654	62.682382
1899.009978	69.797293	62.687386
1898.326667	64.099819	62.692391
1897.575356	71.783519	62.697396
1896.785832	69.508970	62.702401
1896.230334	60.684751	62.707406
1895.767869	74.023023	62.712410
1895.277164	67.892867	62.717415
1894.259989	65.030015	62.722420
1893.221536	72.003975	62.727425
1892.763860	57.556838	62.732430
1892.388382	63.006352	62.737434
1891.917791	58.169204	62.742439
1891.527073	62.433747	62.747444
1890.213098	65.417783	62.752449
1889.801372	65.410738	62.757454
1888.940838	54.996571	62.762458
1888.662745	61.700013	62.767463
1887.633442	62.342919	62.772468
1886.780970	62.145659	62.777473
1886.599739	57.186885	62.782478
1885.899234	59.578390	62.787482
1885.406640	58.854088	62.792487
1884.742353	61.162577	62.797492
1883.443256	61.621246	62.802497
1882.955669	55.189419	62.807502
1882.923929	62.167550	62.812506
1882.096288	63.611037	62.817511
1881.021600	59.633006	62.822516
1880.014935	64.034758	62.827521
1879.698503	60.376298	62.832526
1879.015876	68.101133	62.837530
1878.589993	70.296086	62.842535
1878.052231	48.403030	62.847540
1877.134341	70.219947	62.852545
1876.885320	67.148422	62.857550
1876.227211	69.493779	62.862554
1875.212713	73.363793	62.867559
1874.378638	63.457912	62.872564
1873.343333	68.994839	62.877569
1872.980355	66.165324	62.882574
1872.527779	67.123510	62.887578
1872.118310	69.375779	62.892583
1871.659493	62.986691	62.897588
1870.443517	64.050306	62.902593
1870.022634	67.420819	62.907598
1869.693490	61.271331	62.912602
1868.544210	67.747251	62.917607
1867.791440	69.164664	62.922612
1866.486741	69.632114	62.927617
1866.448264	51.964676	62.932622
1866.252191	64.555782	62.937626
1865.758903	57.516188	62.942631
1865.037272	69.664060	62.947636
1863.937522	62.151494	62.952641
1862.903235	76.220767	62.957646
1862.711183	58.451554	62.962650
1862.171242	66.096970	62.967655
1861.434557	58.755413	62.972660
1860.361666	69.099911	62.977665
1860.079373	55.485920	62.982670
1859.681158	68.128044	62.987674
1858.930157	68.804044	62.992679
1858.105700	60.654868	62.997684
1857.310856	62.417991	63.002689
1857.026297	70.297241	63.007694
1856.246358	52.597720	63.012698
1855.012908	66.022125	63.017703
1854.755793	65.314056	63.022708
1853.771704	71.889907	63.027713
1853.607390	63.773110	63.032718
1853.039801	62.947185	63.037722
1851.735026	63.734761	63.042727
1851.317574	57.012699	63.047732
1850.072230	56.780060	63.052737
1849.960837	61.222599	63.057742
1849.842962	56.190695	63.062746
1849.206115	65.100386	63.067751
1848.496076	55.453937	63.072756
1847.720336	59.472121	63.077761
1847.424295	51.790966	63.082766
1845.949563	63.709915	63.087770
1845.379063	64.852400	63.092775
1844.594855	54.342561	63.097780
1843.732317	72.900749	63.102785
1843.588686	52.134094	63.107790
1843.145812	64.051634	63.112794
1842.292710	61.481284	63.117799
1841.691596	69.822360	63.122804
1841.159266	64.812106	63.127809
1840.080287	70.918924	63.132814
1838.964127	64.916473	63.137818
1838.350480	70.487384	63.142823
1837.884945	50.795239	63.147828
1837.447589	64.958956	63.152833
1837.163185	60.216832	63.157838
1836.812140	59.361260	63.162842
1835.761602	56.655112	63.167847
1835.072610	61.274509	63.172852
1834.292085	62.697914	63.177857
1834.060374	58.406297	63.182862
1833.025801	53.321259	63.187866
1831.988157	69.704347	63.192871
1831.694320	62.469096	63.197876
1831.022249	64.506034	63.202881
1830.159317	61.382187	63.207886
1829.463243	60.594014	63.212890
1828.671647	65.147708	63.217895
1828.332220	54.811670	63.222900
1827.783467	56.715492	63.227905
1827.362287	54.505480	63.232910
1826.200269	60.887246	63.237914
1825.280749	69.496488	63.242919
1825.212430	54.129733	63.247924
1824.516101	53.142916	63.252929
1824.241535	61.536214	63.257934
1822.999732	55.055430	63.262938
1822.205822	53.213670	63.267943
1822.079930	45.431394	63.272948
1820.989414	64.260727	63.277953
1820.223293	54.555387	63.282958
1819.672620	48.836885	63.287962
1819.179318	56.378706	63.292967
1818.657969	51.038728	63.297972
1818.004128	65.995298	63.302977
1816.913381	59.086850	63.307982
1815.969148	65.408811	63.312986
1815.259703	57.607228	63.317991
1815.444060	47.060304	63.322996
1814.742607	53.286944	63.328001
1814.016248	56.810040	63.333006
1813.040438	58.116231	63.338010
1812.312458	67.220163	63.343015
1812.194875	43.751353	63.348020
1811.335680	46.962818	63.353025
1810.412599	48.046181	63.358030
1809.595661	51.336090	63.363034
1809.078568	49.557608	63.368039
1809.067998	55.592550	63.373044
1807.769351	68.243615	63.378049
1807.125827	48.354254	63.383054
1806.650260	47.135278	63.388058
1805.973393	57.241868	63.393063
1805.455350	54.432258	63.398068
1804.429287	55.438940	63.403073
1803.627513	45.759774	63.408078
1803.151250	46.857343	63.413082
1802.863946	68.391219	63.418087
1801.882873	53.521047	63.423092
1801.136907	58.233072	63.428097
1800.993455	55.310369	63.433102
1800.170931	59.058463	63.438106
1799.103566	61.106138	63.443111
1798.435533	53.526635	63.448116
1797.408225	55.875442	63.453121
1797.407176	44.996855	63.458126
1796.841851	55.393225	63.463130
1796.040390	56.504588	63.468135
1795.226136	49.631095	63.473140
1794.299392	58.291946	63.478145
1794.163623	63.025347	63.483150
1793.810303	58.935964	63.488154
1792.550202	60.678371	63.493159
1791.801859	53.512150	63.498164
1790.791328	45.444594	63.503169
1790.692060	52.113331	63.508174
1790.379243	47.016203	63.513178
1789.798693	56.260717	63.518183
1789.017473	49.782508	63.523188
1787.876073	44.064783	63.528193
1787.303202	54.131206	63.533198
1786.954805	48.208713	63.538202
1785.897102	45.722912	63.543207
1785.336901	45.936570	63.548212
1784.730509	60.150777	63.553217
1784.358672	51.182322	63.558222
1783.722122	51.996279	63.563226
1782.400876	50.094774	63.568231
1782.083288	46.655704	63.573236
1781.375894	62.134839	63.578241
1780.835764	45.649326	63.583246
1780.269887	46.406331	63.588250
1778.965410	60.824429	63.593255
1778.501322	47.955237	63.598260
1778.314944	42.923186	63.603265
1777.842735	47.960731	63.608270
1777.010363	48.793170	63.613274
1775.896248	54.757357	63.618279
1775.529669	44.701604	63.623284
1774.837513	57.048215	63.628289
1774.448163	46.661779	63.633294
1773.755031	44.321508	63.638298
1772.643977	55.640285	63.643303
1772.293169	49.692947	63.648308
1771.656025	45.891482	63.653313
1771.260510	42.994619	63.658318
1770.214609	52.041807	63.663322
1769.356970	44.574426	63.668327
1768.996123	47.631076	63.673332
1768.220638	52.543327	63.678337
1767.667497	48.386340	63.683342
1766.689894	53.515183	63.688346
1766.132479	45.891322	63.693351
1765.814744	51.438900	63.698356
1764.857839	53.216746	63.703361
1763.974721	46.459854	63.708366
1763.293206	53.342472	63.713370
1762.610304	43.669677	63.718375
1762.406555	50.684572	63.723380
1762.086519	49.158645	63.728385
1761.272416	42.977394	63.733390
1760.501897	48.516454	63.738394
1759.603785	58.921524	63.743399
1759.672652	47.852073	63.748404
1758.184353	50.608398	63.753409
1757.717490	41.426399	63.758414
1757.176302	55.297529	63.763418
1756.300004	43.878307	63.768423
1755.361891	51.489193	63.773428
1754.360100	53.589547	63.778433
1754.193303	51.280807	63.783438
1753.683543	58.602910	63.788442
1753.448683	54.931518	63.793447
1753.317241	47.571158	63.798452
1751.921210	49.324131	63.803457
1751.428534	49.432460	63.808462
1750.333743	48.813279	63.813466
1749.205641	45.190707	63.818471
1748.909774	41.297207	63.823476
1748.347434	56.791149	63.828481
1748.177270	45.289752	63.833486
1747.229026	47.187648	63.838490
1746.017107	51.809685	63.843495
1745.771108	43.890383	63.848500
1745.253798	39.685138	63.853505
1744.949094	44.839581	63.858510
1743.600844	45.845415	63.863514
1742.687664	55.609514	63.868519
1742.586057	45.972138	63.873524
1742.061786	59.794856	63.878529
1741.240861	61.639422	63.883534
1740.434750	51.617207	63.888538
1739.466180	59.513623	63.893543
1738.869243	50.989339	63.898548
1738.518309	69.617668	63.903553
1738.204640	51.063604	63.908558
1737.655616	57.638196	63.913562
1736.515584	50.480588	63.918567
1736.187865	56.330939	63.923572
1735.293369	59.002435	63.928577
1734.222660	58.153943	63.933582
1733.731654	57.069890	63.938586
1733.023304	54.459246	63.943591
1732.758962	49.491617	63.948596
1732.428944	50.753620	63.953601
1731.186614	55.006775	63.958606
1730.535439	46.628299	63.963610
1729.721704	60.068079	63.968615
1729.614218	45.671045	63.973620
1728.087697	58.937033	63.978625
1727.115415	63.880553	63.983630
1727.138195	57.325136	63.988634
1726.304541	58.066336	63.993639
1726.193790	54.840416	63.998644
1725.355977	66.866414	64.003649
1724.999811	57.403495	64.008654
1723.957222	47.647495	64.013658
1723.009028	55.312029	64.018663
1722.832114	52.844058	64.023668
1722.230906	56.495526	64.028673
1721.737560	58.398453	64.033678
1720.968001	59.700305	64.038682
1719.783932	64.749999	64.043687
1719.828410	62.625316	64.048692
1718.463360	53.384129	64.053697
1717.678733	56.402440	64.058702
1717.369207	50.920042	64.063706
1716.544931	58.681589	64.068711
1716.348823	57.326788	64.073716
1715.210343	55.541363	64.078721
1714.427726	64.866867	64.083726
1714.052047	60.140836	64.088730
1713.453466	56.137727	64.093735
1713.343928	58.552106	64.098740
1712.420093	54.909722	64.103745
1711.480644	49.442220	64.108750
1710.977141	55.598021	64.113754
1710.158070	49.311925	64.118759
1709.457218	58.526673	64.123764
1708.822652	57.468579	64.128769
1708.549297	55.036425	64.133774
1707.651854	58.708139	64.138778
1706.617039	52.913601	64.143783
1706.075098	66.974089	64.148788
1705.453520	59.317854	64.153793
1704.996426	48.659934	64.158798
1704.368804	58.873830	64.163802
1702.600694	66.794749	64.168807
1702.494782	64.348616	64.173812
1702.144514	53.500269	64.178817
1701.734048	49.927736	64.183822
1701.450031	54.345651	64.188826
1700.379315	58.249881	64.193831
1699.579861	45.960658	64.198836
1699.028661	51.707739	64.203841
1698.443792	56.868841	64.208846
1697.476596	53.171853	64.213850
1696.735139	66.806735	64.218855
1696.331936	56.607008	64.223860
1695.634591	54.393577	64.228865
1694.952621	56.246047	64.233870
1694.304078	60.923702	64.238874
1693.193049	57.604356	64.243879
1693.181028	50.305455	64.248884
1692.827484	55.647426	64.253889
1691.407682	57.024179	64.258894
1691.271469	55.740288	64.263898
1690.441635	54.123462	64.268903
1689.813731	51.805968	64.273908
1688.635340	55.487618	64.278913
1687.846992	50.718336	64.283918
1687.510962	57.519290	64.288922
1686.988268	51.230280	64.293927
1686.904359	50.278687	64.298932
1685.843779	63.860181	64.303937
1684.989204	58.749773	64.308942
1684.607432	58.402127	64.313946
1683.648728	57.524827	64.318951
1682.674208	54.511796	64.323956
1682.167074	58.242942	64.328961
1681.299514	57.299130	64.333966
1681.205919	51.757212	64.338970
1680.714576	58.302151	64.343975
1680.054939	52.534764	64.348980
1679.190926	56.182253	64.353985
1678.565294	50.499348	64.358990
1678.113124	56.137668	64.363994
1676.906111	58.578138	64.368999
1676.098152	60.001214	64.374004
1675.654499	53.989797	64.379009
1675.248920	57.428860	64.384014
1674.702018	49.347637	64.389018
1673.428992	57.989409	64.394023
1672.668952	57.700270	64.399028
1672.358008	58.870947	64.404033
1671.701937	57.705897	64.409038
1671.713170	43.149678	64.414042
1670.670749	56.740901	64.419047
1669.741198	46.645291	64.424052
1669.216037	52.897571	64.429057
1668.822961	49.852112	64.434062
1667.957789	54.117923	64.439066
1666.761180	53.978552	64.444071
1666.502078	53.073710	64.449076
1666.068549	47.309836	64.454081
1665.188396	61.868721	64.459086
1664.631535	46.560684	64.464090
1663.837285	65.234187	64.469095
1662.942492	60.350937	64.474100
1662.545964	50.131241	64.479105
1662.411482	57.455243	64.484110
1661.590570	59.361327	64.489114
1660.849601	54.515145	64.494119
1660.450127	53.739828	64.499124
1659.269038	46.344368	64.504129
1658.347077	55.319867	64.509134
1658.023568	48.849425	64.514138
1657.256914	64.924586	64.519143
1656.529144	56.895747	64.524148
1655.560472	54.009524	64.529153
1655.216459	60.590987	64.534158
1654.941009	41.601981	64.539162
1654.435646	53.989893	64.544167
1653.677419	51.732532	64.549172
1652.653183	54.752652	64.554177
1651.839702	63.509087	64.559182
1651.593056	51.231414	64.564186
1650.123337	66.721277	64.569191
1649.684118	52.253950	64.574196
1649.175727	58.069931	64.579201
1648.902491	59.985213	64.584206
1648.753482	52.048941	64.589210
1647.402123	58.539693	64.594215
1646.600212	56.648800	64.599220
1646.207548	49.968581	64.604225
1645.146290	61.311028	64.609230
1644.526162	44.410944	64.614234
1643.603809	59.720819	64.619239
1643.209411	57.544432	64.624244
1642.943201	51.938478	64.629249
1642.367601	65.781976	64.634254
1641.838540	43.916035	64.639258
1640.521068	58.823495	64.644263
1640.359161	55.528441	64.649268
1639.664162	58.262891	64.654273
1638.975818	54.647781	64.659278
1638.291366	51.355314	64.664282
1637.165895	57.540541	64.669287
1637.097876	54.309418	64.674292
1635.891946	56.264055	64.679297
1634.817853	55.476063	64.684302
1634.719075	52.864807	64.689306
1633.937805	62.067115	64.694311
1633.770380	57.823658	64.699316
1633.462721	52.282634	64.704321
1632.466578	63.296214	64.709326
1631.829149	49.704011	64.714330
1631.175036	53.318170	64.719335
1630.423853	54.249716	64.724340
1629.383604	70.603302	64.729345
1628.716077	56.030327	64.734350
1628.376777	50.598405	64.739354
1627.394449	61.240801	64.744359
1626.474104	52.548742	64.749364
1625.621032	50.681753	64.754369
1625.363207	61.007219	64.759374
1625.010312	42.631314	64.764378
1624.590195	56.511603	64.769383
1624.338107	52.554397	64.774388
1623.131079	62.552857	64.779393
1622.418112	62.814470	64.784398
1621.872528	51.186659	64.789402
1620.422097	64.640876	64.794407
1619.904058	56.029981	64.799412
1619.550371	55.652654	64.804417
1618.878844	54.668261	64.809422
1619.062300	60.647141	64.814426
1617.857928	58.612044	64.819431
1617.176324	60.481820	64.824436
1616.477377	51.352492	64.829441
1615.604215	51.434561	64.834446
1615.086833	48.069831	64.839450
1614.240975	58.988579	64.844455
1613.764490	45.238363	64.849460
1613.336984	59.801038	64.854465
1612.197907	52.108781	64.859470
1611.660295	50.833471	64.864474
1610.885854	62.310128	64.869479
1610.516235	56.903523	64.874484
1609.879034	56.788845	64.879489
1608.573730	61.790036	64.884494
1608.095447	52.657193	64.889498
1607.450432	55.700661	64.894503
1607.492759	58.026263	64.899508
1607.138867	56.764343	64.904513
1605.754057	56.762125	64.909518
1605.247288	50.420148	64.914522
1604.586912	61.224282	64.919527
1603.685105	52.631785	64.924532
1602.755365	63.382524	64.929537
1602.042260	61.524844	64.934542
1601.752896	47.631367	64.939546
1601.400973	62.046426	64.944551
1600.977234	49.833167	64.949556
1599.819374	52.735769	64.954561
1599.145652	53.358566	64.959566
1598.680875	56.739237	64.964570
1597.688391	66.930696	64.969575
1596.963512	50.644902	64.974580
1595.998536	58.936583	64.979585
1595.810549	53.611508	64.984590
1595.151252	56.013882	64.989594
1594.848274	63.391460	64.994599
1594.238698	48.864490	64.999604
1593.425354	47.363344	65.004609
1592.722003	53.785862	65.009614
1592.334463	55.725615	65.014618
1591.086714	54.530013	65.019623
1590.591548	46.219835	65.024628
1590.066751	56.715438	65.029633
1588.859696	59.122838	65.034638
1588.284448	47.293184	65.039642
1587.505364	63.513822	65.044647
1586.913041	47.744691	65.049652
1586.211325	52.359853	65.054657
1586.035434	58.545620	65.059662
1586.447251	44.600676	65.064666
1584.968884	66.145556	65.069671
1583.974233	54.295800	65.074676
1583.853935	52.042764	65.079681
1582.205372	58.170774	65.084686
1582.023635	57.070732	65.089690
1581.472028	51.084374	65.094695
1580.901276	51.124718	65.099700
1579.762893	58.934622	65.104705
1578.866360	58.124752	65.109710
1578.923362	48.142094	65.114714
1578.326124	62.238175	65.119719
1577.674018	57.598665	65.124724
1576.744161	52.014584	65.129729
1575.629595	62.922419	65.134734
1575.353924	53.834662	65.139738
1574.991779	61.473939	65.144743
1574.228661	65.416076	65.149748
1573.454996	54.286539	65.154753
1572.774335	59.402961	65.159758
1572.319104	53.421792	65.164762
1571.298861	53.774813	65.169767
1570.343263	57.441615	65.174772
1569.983748	48.070731	65.179777
1569.177846	59.112444	65.184782
1569.087561	52.399969	65.189786
1568.330876	58.446211	65.194791
1567.665438	56.062176	65.199796
1567.021463	57.191162	65.204801
1566.573247	55.516901	65.209806
1565.585618	56.210078	65.214810
1564.504950	54.401346	65.219815
1563.970898	41.177511	65.224820
1563.904774	46.311405	65.229825
1562.967869	62.104556	65.234830
1562.226754	56.410071	65.239834
1561.460346	57.988997	65.244839
1561.018116	54.725874	65.249844
1560.246420	56.873315	65.254849
1559.055763	57.185610	65.259854
1558.686025	57.137255	65.264858
1558.165249	54.266638	65.269863
1557.761771	55.655445	65.274868
1557.443132	51.480176	65.279873
1555.917720	54.086397	65.284878
1555.676820	63.179213	65.289882
1554.912374	60.598034	65.294887
1554.672679	52.963175	65.299892
1553.558228	49.677554	65.304897
1552.246802	57.915487	65.309902
1552.222966	51.775900	65.314906
1551.786275	56.932406	65.319911
1551.242894	47.360517	65.324916
1550.581111	55.711263	65.329921
1549.361226	57.579851	65.334926
1549.147404	51.747981	65.339930
1548.351170	45.836770	65.344935
1547.532149	63.277949	65.349940
1547.052669	49.447806	65.354945
1546.210282	53.862989	65.359950
1545.954552	54.398887	65.364954
1544.931885	54.991988	65.369959
1543.885015	66.183955	65.374964
1543.586504	58.263565	65.379969
1543.079834	53.977831	65.384974
1542.850200	57.835210	65.389978
1541.861177	60.272641	65.394983
1540.937323	48.440047	65.399988
1540.915652	48.959255	65.404993
1539.399073	52.117564	65.409998
1538.723129	47.232711	65.415002
1538.022522	51.775171	65.420007
1537.761464	61.027298	65.425012
1537.585908	54.377258	65.430017
1536.832228	50.537608	65.435022
1535.951565	49.696848	65.440026
1535.159051	54.410023	65.445031
1534.636435	47.629059	65.450036
1533.556214	52.337487	65.455041
1532.879357	58.194443	65.460046
1532.502183	62.065805	65.465050
1531.944537	51.245724	65.470055
1531.471999	63.618974	65.475060
1530.766335	60.974849	65.480065
1529.344374	54.447162	65.485070
1529.018227	64.230003	65.490074
1528.597594	57.585789	65.495079
1528.062964	58.489263	65.500084
1527.342701	52.532871	65.505089
1526.273907	60.503617	65.510094
1526.091664	49.724810	65.515098
1525.088462	61.408132	65.520103
1523.994728	51.928426	65.525108
1523.948063	53.686298	65.530113
1523.355005	61.179351	65.535118
1522.907035	51.273779	65.540122
1521.753515	52.925264	65.545127
1521.079631	53.120773	65.550132
1520.989989	52.315171	65.555137
1520.255698	54.005693	65.560142
1519.375950	48.213412	65.565146
1518.091615	53.145081	65.570151
1517.740791	53.166262	65.575156
1517.690673	50.845312	65.580161
1516.777250	50.772971	65.585166
1516.022547	47.412860	65.590170
1515.417397	55.270513	65.595175
1514.735334	52.382960	65.600180
1513.638602	43.223846	65.605185
1512.516769	50.378315	65.610190
1512.058475	43.751134	65.615194
1511.696789	58.390077	65.620199
1511.434241	51.966742	65.625204
1511.295443	50.520856	65.630209
1510.539125	52.757326	65.635214
1509.418164	48.074074	65.640218
1508.751056	50.510823	65.645223
1508.184450	50.928974	65.650228
1507.531622	52.847817	65.655233
1506.276847	52.271507	65.660238
1505.989347	49.523100	65.665242
1505.677248	54.864807	65.670247
1504.536281	60.063847	65.675252
1503.967192	46.886594	65.680257
1503.190717	49.301300	65.685262
1503.074883	46.601306	65.690266
1502.567365	52.516508	65.695271
1501.103737	56.166294	65.700276
1500.693322	45.966196	65.705281
1499.789267	59.805122	65.710286
1499.703618	52.349211	65.715290
1499.137256	49.969953	65.720295
1497.946171	53.582739	65.725300
1497.485830	51.992416	65.730305
1496.851251	49.928335	65.735310
1496.327998	54.887301	65.740314
1495.209660	48.264086	65.745319
1494.429294	51.682304	65.750324
1494.116111	51.877271	65.755329
1493.749314	53.843701	65.760334
1493.329791	52.508653	65.765338
1491.822904	49.214463	65.770343
1491.142123	57.596622	65.775348
1490.970413	48.935467	65.780353
1490.554773	57.250264	65.785358
1489.772671	44.094253	65.790362
1488.585874	50.642497	65.795367
1488.030702	59.933476	65.800372
1487.953986	45.161037	65.805377
1487.003659	61.569737	65.810382
1485.690652	48.316748	65.815386
1485.438239	55.788787	65.820391
1485.056300	58.383644	65.825396
1484.544599	52.734729	65.830401
1483.477789	55.091505	65.835406
1482.506485	52.424957	65.840410
1481.877203	64.786850	65.845415
1481.420139	53.345282	65.850420
1481.111376	48.750586	65.855425
1480.544186	65.741771	65.860430
1479.927383	55.484588	65.865434
1479.371395	59.857433	65.870439
1478.457961	61.423478	65.875444
1477.676176	49.752832	65.880449
1476.610557	57.212181	65.885454
1476.216208	50.713609	65.890458
1475.699864	57.114319	65.895463
1475.071540	58.138342	65.900468
1474.525336	53.300695	65.905473
1474.028093	64.290227	65.910478
1473.441986	51.639207	65.915482
1472.340196	51.259365	65.920487
1471.512901	58.318163	65.925492
1471.243600	47.967920	65.930497
1470.506250	63.380888	65.935502
1469.667428	51.919571	65.940506
1468.792806	58.088650	65.945511
1468.144311	54.342687	65.950516
1468.220874	46.938271	65.955521
1467.135655	48.824917	65.960526
1466.218410	37.666219	65.965530
1465.918912	47.015905	65.970535
1465.287618	52.607024	65.975540
1464.927047	40.287587	65.980545
1463.421397	57.309635	65.985550
1462.872165	47.199413	65.990554
1462.620933	47.359308	65.995559
1461.888222	47.743945	66.000564
1460.901302	50.967927	66.005569
1460.011517	49.780155	66.010574
1459.649389	54.738751	66.015578
1459.186114	50.958626	66.020583
1458.924361	46.586687	66.025588
1458.201584	46.223886	66.030593
1457.058635	49.428513	66.035598
1456.734773	40.484058	66.040602
1456.221042	41.794211	66.045607
1454.982694	44.335944	66.050612
1454.621588	44.661527	66.055617
1453.866494	45.508593	66.060622
1453.301799	45.232628	66.065626
1452.406346	42.776379	66.070631
1451.595808	54.414904	66.075636
1451.345716	39.223776	66.080641
1451.002284	61.193847	66.085646
1450.116486	42.890076	66.090650
1449.378837	42.166961	66.095655
1448.067694	50.214086	66.100660
1448.043069	42.199737	66.105665
1447.212560	43.795188	66.110670
1446.112934	51.622630	66.115674
1445.533470	52.049145	66.120679
1444.800437	49.954995	66.125684
1444.610672	45.776612	66.130689
1444.302848	51.675854	66.135694
1443.866256	51.606602	66.140698
1442.843329	39.453935	66.145703
1442.340591	53.973370	66.150708
1441.613058	45.432097	66.155713
1440.348157	50.548358	66.160718
1439.898623	40.941094	66.165722
1439.476186	56.059595	66.170727
1438.833918	55.497933	66.175732
1437.718486	41.451953	66.180737
1436.655878	54.119240	66.185742
1436.357146	56.197856	66.190746
1436.323823	48.333113	66.195751
1435.542092	56.800708	66.200756
1435.335509	45.855487	66.205761
1434.120224	58.414586	66.210766
1433.622299	52.036557	66.215770
1432.953676	51.732962	66.220775
1431.859560	52.001589	66.225780
1431.405901	46.824412	66.230785
1430.917865	55.883963	66.235790
1430.180956	55.435111	66.240794
1429.292523	46.913105	66.245799
1428.653944	44.556381	66.250804
1428.314622	49.831458	66.255809
1427.621975	54.940351	66.260814
1426.872308	53.992082	66.265818
1426.083632	43.278143	66.270823
1425.406483	51.604543	66.275828
1425.134576	50.305968	66.280833
1423.863161	53.728136	66.285838
1423.119798	53.187276	66.290842
1422.868585	52.806305	66.295847
1422.394537	44.439207	66.300852
1421.987577	47.976284	66.305857
1420.683182	48.670977	66.310862
1420.141593	51.439439	66.315866
1419.442045	50.312905	66.320871
1418.929798	45.859366	66.325876
1418.308688	43.788435	66.330881
1417.258845	54.089970	66.335886
1416.684526	54.350102	66.340890
1416.767521	44.606168	66.345895
1415.387998	54.346698	66.350900
1414.613490	48.324856	66.355905
1413.652418	45.156843	66.360910
1413.250998	41.579777	66.365914
1413.183653	42.462618	66.370919
1412.656036	55.126880	66.375924
1412.055759	37.044249	66.380929
1410.762150	48.217112	66.385934
1410.535628	42.723158	66.390938
1409.804312	39.548592	66.395943
1408.584229	51.648009	66.400948
1408.393993	40.813735	66.405953
1407.631851	45.895830	66.410958
1407.451715	55.127208	66.415962
1406.182949	44.853838	66.420967
1405.262221	56.957719	66.425972
1405.241026	43.759652	66.430977
1404.274671	54.899431	66.435982
1403.797643	44.940171	66.440986
1402.720355	46.738854	66.445991
1402.086310	53.208739	66.450996
1401.801176	43.480742	66.456001
1401.123587	47.068719	66.461006
1400.519794	51.140106	66.466010
1399.575208	46.717443	66.471015
1398.806351	58.943837	66.476020
1399.031736	40.654285	66.481025
1398.121450	53.759395	66.486030
1397.280143	46.731095	66.491034
1396.745469	34.196516	66.496039
1395.596096	50.999538	66.501044
1394.801030	53.961251	66.506049
1393.725069	51.372872	66.511054
1393.219680	55.283548	66.516058
1393.137000	54.601417	66.521063
1392.743229	48.831287	66.526068
1392.271476	51.413622	66.531073
1391.337728	49.884374	66.536078
1390.632322	49.790053	66.541082
1390.320741	53.494891	66.546087
1388.759705	50.811736	66.551092
1388.252084	43.864437	66.556097
1387.806999	63.133714	66.561102
1387.215889	53.039630	66.566106
1386.883635	50.240009	66.571111
1385.904354	46.417347	66.576116
1385.499271	50.993288	66.581121
1384.591609	47.228624	66.586126
1383.689846	48.803883	66.591130
1383.386558	42.448549	66.596135
1382.705113	54.495477	66.601140
1382.002411	44.788126	66.606145
1380.981170	44.422327	66.611150
1380.497692	41.878546	66.616154
1380.102674	51.079424	66.621159
1379.697098	42.160588	66.626164
1378.681630	50.443005	66.631169
1377.611906	44.797669	66.636174
1377.022834	50.911920	66.641178
1376.848682	47.412271	66.646183
1375.945278	52.168341	66.651188
1375.049236	42.679373	66.656193
1374.348365	55.688128	66.661198
1374.004984	52.425100	66.666202
1373.743284	53.182725	66.671207
1372.263121	49.199999	66.676212
1371.733847	52.822754	66.681217
1371.328122	44.788567	66.686222
1370.884349	59.049492	66.691226
1370.349329	50.296302	66.696231
1369.109879	61.249281	66.701236
1368.765021	59.005147	66.706241
1368.168809	48.702160	66.711246
1367.149612	57.179132	66.716250
1366.315366	49.042757	66.721255
1365.662346	56.602130	66.726260
1365.270518	60.412763	66.731265
1364.983523	51.762068	66.736270
1364.525460	51.109647	66.741274
1363.699963	43.386603	66.746279
1362.960722	58.798302	66.751284
1362.257452	46.381983	66.756289
1360.755497	50.175122	66.761294
1360.120160	48.967438	66.766298
1359.949888	49.544960	66.771303
1359.406449	44.930822	66.776308
1358.954993	53.524118	66.781313
1358.451182	52.134688	66.786318
1357.416467	43.298518	66.791322
1357.051479	52.991339	66.796327
1355.996533	54.357581	66.801332
1355.769958	47.220543	66.806337
1354.686961	50.790977	66.811342
1353.706574	63.254423	66.816346
1353.653297	41.005496	66.821351
1352.917092	56.858236	66.826356
1352.502393	45.760044	66.831361
1351.229536	59.195600	66.836366
1350.787959	44.798138	66.841370
1350.580964	45.838789	66.846375
1349.361522	50.928941	66.851380
1348.878374	54.254224	66.856385
1348.164116	53.636223	66.861390
1347.801252	48.364212	66.866394
1347.036060	43.066276	66.871399
1345.570812	45.445442	66.876404
1345.128078	50.812653	66.881409
1345.021598	48.406059	66.886414
1344.455981	46.477706	66.891418
1344.096747	51.224549	66.896423
1342.971127	41.374720	66.901428
1342.508363	35.554076	66.906433
1341.705492	42.120186	66.911438
1340.803024	51.385964	66.916442
1340.185297	40.999684	66.921447
1339.519919	48.244070	66.926452
1339.344666	46.485464	66.931457
1338.304610	54.021214	66.936462
1337.267490	49.058227	66.941466
1337.079545	49.791516	66.946471
1336.429891	47.496498	66.951476
1335.980277	36.047496	66.956481
1335.096174	49.790238	66.961486
1334.083066	45.687562	66.966490
1333.994829	34.256804	66.971495
1333.049321	47.421134	66.976500
1332.007517	42.175061	66.981505
1331.475408	47.845047	66.986510
1330.782077	45.418210	66.991514
1330.877825	37.364240	66.996519
1329.512730	36.455492	67.001524
1328.862775	39.010972	67.006529
1328.289538	44.387891	67.011534
1327.886571	46.011602	67.016538
1327.516698	39.039271	67.021543
1326.184651	46.392792	67.026548
1325.636778	39.398298	67.031553
1325.104058	46.030272	67.036558
1324.332230	53.458734	67.041562
1323.297925	35.708479	67.046567
1322.622342	40.557648	67.051572
1322.448698	40.733606	67.056577
1322.048943	37.515821	67.061582
1321.453992	47.313002	67.066586
1320.784284	45.133135	67.071591
1319.777872	51.506119	67.076596
1319.329379	41.542351	67.081601
1318.630898	45.772299	67.086606
1317.522692	47.055564	67.091610
1317.230500	45.812264	67.096615
1316.587402	41.786385	67.101620
1316.229052	40.963589	67.106625
1315.148727	49.633207	67.111630
1314.208959	51.813742	67.116634
1314.125494	44.333857	67.121639
1313.507670	48.536793	67.126644
1312.240812	48.462368	67.131649
1311.778513	45.814314	67.136654
1311.052336	57.344845	67.141658
1310.670190	45.478284	67.146663
1309.791929	57.431941	67.151668
1309.107081	50.377225	67.156673
1308.400020	50.945474	67.161678
1307.616347	57.860189	67.166682
1307.552640	46.490178	67.171687
1306.697762	53.422519	67.176692
1305.780814	40.953470	67.181697
1305.406751	43.520286	67.186702
1304.817129	38.530328	67.191706
1304.344407	41.172750	67.196711
1303.307016	46.308091	67.201716
1302.584856	46.240110	67.206721
1302.083933	48.226309	67.211726
1300.871937	43.920313	67.216730
1300.281373	40.387532	67.221735
1299.799567	48.137300	67.226740
1299.413322	43.148123	67.231745
1298.960732	40.733483	67.236750
1298.061237	44.675289	67.241754
1297.662412	43.876275	67.246759
1296.771342	49.324230	67.251764
1295.995501	48.192515	67.256769
1295.213294	55.471255	67.261774
1294.175420	43.464535	67.266778
1293.952720	41.152112	67.271783
1293.487904	51.089451	67.276788
1293.248957	36.820641	67.281793
1292.420850	49.198382	67.286798
1291.625101	47.891647	67.291802
1291.056135	47.647935	67.296807
1289.652276	53.995814	67.301812
1289.207284	46.936087	67.306817
1288.733974	51.790953	67.311822
1288.267900	49.402111	67.316826
1287.887003	50.617063	67.321831
1286.973336	50.104896	67.326836
1286.226273	55.663995	67.331841
1285.642732	48.403957	67.336846
1284.214650	47.525746	67.341850
1283.544055	38.284816	67.346855
1282.970469	48.192140	67.351860
1283.072922	45.429074	67.356865
1282.611425	39.234524	67.361870
1281.750932	54.288635	67.366874
1281.037944	47.312517	67.371879
1280.075270	50.458595	67.376884
1279.541190	50.737590	67.381889
1278.772742	49.707201	67.386894
1277.965641	50.843268	67.391898
1277.634078	41.196794	67.396903
1277.064298	41.035212	67.401908
1276.498532	33.556328	67.406913
1275.564409	42.458162	67.411918
1274.917528	50.038647	67.416922
1274.564584	46.146411	67.421927
1273.583774	50.186305	67.426932
1272.471725	41.723578	67.431937
1272.057667	44.903851	67.436942
1271.706088	45.771964	67.441946
1271.665901	34.123854	67.446951
1270.327292	51.612973	67.451956
1269.537455	42.780490	67.456961
1268.912261	44.814836	67.461966
1267.979892	46.178969	67.466970
1267.376009	41.345821	67.471975
1266.289755	50.278158	67.476980
1266.046478	45.744048	67.481985
1265.746112	44.655010	67.486990
1265.013176	53.154302	67.491994
1264.879923	43.684446	67.496999
1263.217310	57.601448	67.502004
1263.140059	43.854104	67.507009
1262.726927	48.152231	67.512014
1261.686486	45.364310	67.517018
1261.070188	44.511575	67.522023
1260.369312	49.095137	67.527028
1260.013768	57.876610	67.532033
1258.769957	55.234558	67.537038
1257.900838	48.253311	67.542042
1257.576176	35.043604	67.547047
1257.052020	50.786943	67.552052
1256.685944	47.029255	67.557057
1255.876230	49.222246	67.562062
1254.790563	54.921916	67.567066
1254.477468	47.748191	67.572071
1253.481305	50.477003	67.577076
1253.492969	56.333343	67.582081
1252.375720	42.983159	67.587086
1251.403151	51.507940	67.592090
1251.169613	44.651133	67.597095
1250.485473	53.081172	67.602100
1250.271056	47.003451	67.607105
1249.284151	35.130577	67.612110
1248.516229	45.953425	67.617114
1248.029097	43.454405	67.622119
1246.970941	54.662434	67.627124
1245.998954	54.925913	67.632129
1245.864029	46.159608	67.637134
1245.459014	51.251189	67.642138
1244.831411	46.565312	67.647143
1243.676747	54.068856	67.652148
1243.406520	55.725087	67.657153
1242.869865	39.051594	67.662158
1241.661587	50.972582	67.667162
1241.277424	47.416458	67.672167
1240.280015	56.514443	67.677172
1240.231201	42.461401	67.682177
1239.195819	47.758862	67.687182
1238.064059	58.429850	67.692186
1237.967392	42.522135	67.697191
1237.575558	46.886260	67.702196
1236.680484	52.169299	67.707201
1235.710403	52.754159	67.712206
1234.973531	55.064878	67.717210
1234.641218	45.475298	67.722215
1234.143534	52.221558	67.727220
1233.203246	51.067127	67.732225
1232.388382	40.822613	67.737230
1231.670700	58.077410	67.742234
1231.558623	39.500935	67.747239
1230.897867	52.304641	67.752244
1229.970018	45.348515	67.757249
1229.160018	44.493474	67.762254
1228.740487	61.119003	67.767258
1228.458104	38.483942	67.772263
1227.281786	47.402227	67.777268
1226.821539	48.275011	67.782273
1226.096987	44.381952	67.787278
1224.775780	64.050718	67.792282
1224.302958	40.616504	67.797287
1223.650793	49.128188	67.802292
1223.167346	52.332118	67.807297
1222.709462	50.263668	67.812302
1222.072806	55.735843	67.817306
1222.338054	54.085388	67.822311
1221.035821	45.679734	67.827316
1220.321146	51.653143	67.832321
1219.175902	43.954195	67.837326
1218.400418	47.280251	67.842330
1218.076580	43.498509	67.847335
1217.412265	48.159841	67.852340
1216.984518	58.699966	67.857345
1216.217664	45.249932	67.862350
1215.254462	50.499657	67.867354
1215.044878	41.521316	67.872359
1214.216000	56.390650	67.877364
1213.859117	54.987348	67.882369
1212.908669	48.991979	67.887374
1211.951292	54.124092	67.892378
1211.470651	42.605944	67.897383
1210.452678	60.883001	67.902388
1209.609611	46.491082	67.907393
1209.452056	46.667643	67.912398
1208.735669	47.890225	67.917402
1208.459999	43.648265	67.922407
1207.721851	53.688996	67.927412
1206.516546	39.884515	67.932417
1206.274304	56.246893	67.937422
1205.739259	52.845647	67.942426
1205.421013	48.072744	67.947431
1204.146070	49.362072	67.952436
1203.559650	46.375829	67.957441
1203.002356	50.061411	67.962446
1202.047562	52.004690	67.967450
1201.660217	42.286684	67.972455
1201.018351	43.409113	67.977460
1200.569823	44.004085	67.982465
1199.544106	40.684024	67.987470
1198.231469	48.370389	67.992474
1198.060635	38.950675	67.997479
1197.806163	49.084792	68.002484
1197.166303	45.957248	68.007489
1196.656019	44.121051	68.012494
1195.517958	43.184156	68.017498
1195.189977	35.850399	68.022503
1194.344506	50.641949	68.027508
1193.469290	55.997533	68.032513
1192.622925	43.663963	68.037518
1192.058582	48.186406	68.042522
1191.880137	42.259086	68.047527
1191.363562	35.116161	68.052532
1190.398922	51.479876	68.057537
1189.469501	43.606281	68.062542
1188.790674	45.685442	68.067546
1188.688131	48.030909	68.072551
1187.370472	49.235579	68.077556
1186.513750	42.121514	68.082561
1186.247617	45.797064	68.087566
1185.818741	51.997829	68.092570
1185.429335	52.286951	68.097575
1184.504475	48.703288	68.102580
1183.558626	45.338994	68.107585
1183.233913	41.771851	68.112590
1182.653354	46.145495	68.117594
1182.065873	51.098952	68.122599
1180.801963	50.866436	68.127604
1180.241453	37.885055	68.132609
1179.974917	39.712582	68.137614
1179.187263	48.804030	68.142618
1178.355309	45.122021	68.147623
1177.618506	50.887658	68.152628
1177.064346	36.358363	68.157633
1176.923808	36.823940	68.162638
1175.539644	52.249911	68.167642
1175.226041	42.406650	68.172647
1174.789733	53.725530	68.177652
1174.023875	47.798590	68.182657
1173.622982	51.918174	68.187662
1172.414705	51.124912	68.192666
1172.027403	36.515470	68.197671
1170.846862	47.605791	68.202676
1170.008011	48.874666	68.207681
1169.764330	43.355093	68.212686
1169.369552	51.852662	68.217690
1169.152293	45.940977	68.222695
1168.029933	51.288564	68.227700
1166.837575	56.178956	68.232705
1166.669872	52.607343	68.237710
1166.080368	53.297277	68.242714
1164.993682	49.223721	68.247719
1163.989081	53.330511	68.252724
1163.537546	47.516005	68.257729
1163.539729	37.996247	68.262734
1162.695651	43.537684	68.267738
1162.716829	39.920268	68.272743
1161.441594	44.109518	68.277748
1160.774032	53.483055	68.282753
1159.907887	30.552962	68.287758
1158.842505	50.012319	68.292762
1158.285208	39.115052	68.297767
1157.810635	37.270032	68.302772
1157.336813	42.960732	68.307777
1156.924742	36.838774	68.312782
1155.787140	50.568254	68.317786
1155.623848	44.048779	68.322791
1154.972385	43.316775	68.327796
1154.243647	43.246729	68.332801
1153.571078	39.203510	68.337806
1152.378727	46.750922	68.342810
1152.089020	48.468603	68.347815
1151.688511	45.290390	68.352820
1150.291800	44.191235	68.357825
1150.097391	39.622565	68.362830
1149.478171	40.856516	68.367834
1149.028603	40.805148	68.372839
1148.098085	46.166382	68.377844
1147.243700	43.315808	68.382849
1146.804858	49.317899	68.387854
1146.358262	47.252400	68.392858
1145.423346	48.777821	68.397863
1144.658946	49.561804	68.402868
1143.860433	47.544390	68.407873
1143.741052	41.394806	68.412878
1142.305114	45.978610	68.417882
1141.570689	42.861391	68.422887
1141.007829	43.595976	68.427892
1140.614341	52.120148	68.432897
1140.484163	36.326595	68.437902
1140.046180	47.869653	68.442906
1139.421871	43.880260	68.447911
1138.324189	46.880710	68.452916
1137.612267	35.706863	68.457921
1136.873551	44.702230	68.462926
1135.970004	42.759869	68.467930
1135.423098	45.362079	68.472935
1134.942256	42.609786	68.477940
1134.383743	38.657237	68.482945
1133.472368	36.216257	68.487950
1132.605598	51.649835	68.492954
1132.392484	39.546723	68.497959
1131.640334	53.459322	68.502964
1130.519631	41.897927	68.507969
1130.070459	50.629641	68.512974
1129.251920	46.267464	68.517978
1129.100352	46.801026	68.522983
1128.590036	47.874167	68.527988
1127.561306	40.647144	68.532993
1127.002816	44.753951	68.537998
1126.436381	49.756105	68.543002
1125.939718	43.780063	68.548007
1124.826588	44.343564	68.553012
1123.926853	49.129086	68.558017
1123.803621	40.793005	68.563022
1123.452441	49.061302	68.568026
1122.361141	48.156425	68.573031
1121.376842	43.024298	68.578036
1120.983595	47.552655	68.583041
1120.643358	34.917866	68.588046
1119.465107	54.347882	68.593050
1118.633705	38.613825	68.598055
1118.166666	42.280334	68.603060
1117.641733	45.129775	68.608065
1117.688673	37.141924	68.613070
1116.248680	50.758670	68.618074
1115.686725	37.277677	68.623079
1115.284984	49.128769	68.628084
1114.381453	42.425857	68.633089
1113.750843	45.065038	68.638094
1112.775704	58.341366	68.643098
1112.187156	43.076432	68.648103
1112.006832	47.585115	68.653108
1111.328050	40.270902	68.658113
1110.843965	36.989304	68.663118
1109.814890	44.725215	68.668122
1109.258966	41.958063	68.673127
1108.115414	38.057576	68.678132
1107.390129	39.940730	68.683137
1106.965104	35.104412	68.688142
1106.773987	41.738847	68.693146
1106.423153	31.595619	68.698151
1105.510145	36.244490	68.703156
1104.505231	43.339506	68.708161
1103.471685	33.159797	68.713166
1102.376299	47.355633	68.718170
1101.919496	39.309142	68.723175
1101.596653	45.584506	68.728180
1101.070636	35.316185	68.733185
1101.056427	25.873161	68.738190
1100.509412	44.329184	68.743194
1099.380363	37.135478	68.748199
1098.849048	45.430850	68.753204
1097.809321	44.062067	68.758209
1097.230811	31.020511	68.763214
1096.416678	44.422600	68.768218
1096.336508	40.829190	68.773223
1095.242982	43.007449	68.778228
1094.125279	39.115472	68.783233
1093.998512	39.892659	68.788238
1093.240809	41.486099	68.793242
1092.796496	49.228348	68.798247
1091.975983	37.053136	68.803252
1090.718788	45.235323	68.808257
1090.376129	42.576171	68.813262
1089.823510	37.397473	68.818266
1089.710259	49.268907	68.823271
1088.826712	47.206693	68.828276
1087.880183	40.923771	68.833281
1087.687934	49.931570	68.838286
1086.960483	44.738104	68.843290
1085.534475	46.937716	68.848295
1085.020402	35.998910	68.853300
1084.474513	43.557052	68.858305
1084.265400	30.463051	68.863310
1083.530693	41.242797	68.868314
1082.525422	42.933964	68.873319
1081.904605	33.432895	68.878324
1081.263936	43.492827	68.883329
1081.380134	40.727574	68.888334
1080.248016	40.280192	68.893338
1079.342007	40.777653	68.898343
1078.875478	40.159746	68.903348
1078.186544	36.097079	68.908353
1077.519933	25.452191	68.913358
1076.409926	37.354439	68.918362
1076.397194	33.726652	68.923367
1075.182637	31.368612	68.928372
1074.083088	45.402700	68.933377
1073.649451	27.777819	68.938382
1073.015105	39.456182	68.943386
1072.786972	27.355482	68.948391
1072.479741	31.740854	68.953396
1071.622685	42.937435	68.958401
1070.997587	35.666736	68.963406
1069.961741	48.544314	68.968410
1069.614899	31.258842	68.973415
1069.328479	34.450373	68.978420
1068.258503	35.931076	68.983425
1067.707745	30.543945	68.988430
1067.008703	41.264408	68.993434
1065.942638	36.845443	68.998439
1065.753540	34.936109	69.003444
1065.187926	41.552849	69.008449
1063.928782	33.253977	69.013454
1063.149004	40.697947	69.018458
1062.763375	28.984980	69.023463
1062.232156	47.250848	69.028468
1061.770810	35.772258	69.033473
1061.599602	39.566748	69.038478
1060.201217	38.062656	69.043482
1059.595192	47.150466	69.048487
1058.700308	35.330858	69.053492
1057.579887	42.819556	69.058497
1057.139728	40.727822	69.063502
1056.683277	39.187429	69.068506
1056.337466	45.147922	69.073511
1056.036989	38.117307	69.078516
1055.093104	39.931175	69.083521
1054.369774	34.946792	69.088526
1053.614179	39.867089	69.093530
1052.996200	28.124859	69.098535
1052.597757	37.108683	69.103540
1051.413673	39.643544	69.108545
1050.811655	35.910816	69.113550
1050.294994	38.995481	69.118554
1049.912701	37.755511	69.123559
1049.067765	30.180767	69.128564
1048.280758	40.661350	69.133569
1048.083587	33.075018	69.138574
1046.778435	27.893052	69.143578
1046.114379	33.413764	69.148583
1045.657348	37.758318	69.153588
1044.716469	36.982502	69.158593
1044.349014	31.228769	69.163598
1044.029407	37.754339	69.168602
1043.015913	39.967193	69.173607
1042.616597	36.085533	69.178612
1042.133633	38.899925	69.183617
1041.111077	39.395441	69.188622
1040.137467	38.757290	69.193626
1039.676476	40.469115	69.198631
1039.384958	32.915138	69.203636
1038.380504	32.620921	69.208641
1037.804395	34.272215	69.213646
1037.167244	33.123251	69.218650
1036.447227	38.115158	69.223655
1035.885173	37.044128	69.228660
1034.343657	39.954385	69.233665
1034.399857	32.748770	69.238670
1033.801073	37.842810	69.243674
1033.406939	41.001022	69.248679
1032.857187	28.735464	69.253684
1031.639333	47.427515	69.258689
1031.073728	31.350044	69.263694
1030.603341	41.775532	69.268698
1030.133682	33.776837	69.273703
1029.001529	27.838850	69.278708
1028.285427	36.862172	69.283713
1028.029134	30.422168	69.288718
1027.315564	36.854303	69.293722
1026.479393	44.674664	69.298727
1026.069350	32.371111	69.303732
1025.426100	39.310849	69.308737
1025.006363	32.419057	69.313742
1023.543663	33.031907	69.318746
1022.936691	35.755650	69.323751
1022.791623	38.374373	69.328756
1022.033863	36.940265	69.333761
1021.290201	38.898900	69.338766
1020.816522	41.990925	69.343770
1020.132889	35.910625	69.348775
1019.273725	34.088974	69.353780
1018.237204	37.442418	69.358785
1017.940351	28.143710	69.363790
1017.436587	36.002643	69.368794
1016.859777	32.661707	69.373799
1016.010157	28.165759	69.378804
1014.993535	35.432963	69.383809
1014.783388	29.641595	69.388814
1014.331321	26.622995	69.393818
1013.436315	27.814124	69.398823
1012.837260	29.746601	69.403828
1011.905474	24.196192	69.408833
1011.465491	30.723566	69.413838
1010.483326	32.231321	69.418842
1009.888312	38.576794	69.423847
1009.680562	21.742284	69.428852
1008.911540	38.718257	69.433857
1008.091326	22.531510	69.438862
1006.920035	29.156309	69.443866
1006.593559	34.465635	69.448871
1006.510569	29.661653	69.453876
1005.331357	42.740238	69.458881
1004.331109	35.215450	69.463886
1003.910081	35.329868	69.468890
1003.034125	30.030760	69.473895
1003.173157	34.017152	69.478900
1002.543722	33.176034	69.483905
1001.732308	32.169915	69.488910
1000.958171	30.982833	69.493914
999.858331	30.889877	69.498919
999.041813	32.074831	69.503924
998.061703	26.893217	69.508929
997.844629	31.636389	69.513934
997.381688	31.571407	69.518938
996.879879	30.396190	69.523943
996.993109	26.453496	69.528948
995.594956	36.736446	69.533953
994.849659	33.967916	69.538958
994.424087	34.824183	69.543962
993.652618	33.368613	69.548967
992.405658	25.551947	69.553972
991.934088	37.969198	69.558977
991.702649	34.183834	69.563982
991.430061	37.694851	69.568986
990.023305	33.882029	69.573991
989.349133	26.073575	69.578996
988.970378	43.235030	69.584001
988.514223	36.025783	69.589006
987.409267	33.322362	69.594010
986.810282	38.413289	69.599015
986.254233	34.121363	69.604020
985.811171	37.396168	69.609025
985.243935	25.939188	69.614030
984.253458	23.627541	69.619034
983.659990	28.421137	69.624039
983.198648	34.664925	69.629044
981.812247	48.383579	69.634049
981.402143	36.999357	69.639054
980.804160	41.848867	69.644058
980.423887	37.224641	69.649063
979.959647	28.083453	69.654068
978.980343	24.981599	69.659073
978.378256	26.788417	69.664078
977.960138	33.129401	69.669082
976.959557	36.929702	69.674087
976.340126	34.103307	69.679092
975.597211	32.834000	69.684097
975.497914	28.646015	69.689102
974.838454	28.962367	69.694106
973.473226	33.612270	69.699111
973.238926	28.643143	69.704116
972.644194	20.580798	69.709121
971.624149	31.666138	69.714126
971.082369	29.970615	69.719130
970.014678	38.430184	69.724135
969.570458	37.972742	69.729140
969.529921	26.397274	69.734145
968.681670	21.513221	69.739150
967.744246	29.912637	69.744154
967.195697	34.166112	69.749159
966.356531	28.525295	69.754164
965.397047	37.596815	69.759169
965.164041	30.687942	69.764174
964.593244	35.271369	69.769178
963.808471	34.440785	69.774183
962.975835	29.450174	69.779188
962.105555	40.070172	69.784193
961.972919	29.516971	69.789198
961.417313	32.130058	69.794202
960.573380	30.055284	69.799207
959.970842	32.667954	69.804212
958.706539	41.702829	69.809217
958.732158	28.224600	69.814222
958.002446	31.832006	69.819226
956.621097	36.426139	69.824231
956.345779	34.902674	69.829236
955.982106	35.533069	69.834241
955.570413	31.005307	69.839246
954.682864	28.284655	69.844250
953.537664	32.555803	69.849255
953.409359	27.820534	69.854260
952.518044	41.340575	69.859265
952.147142	25.112322	69.864270
950.611573	30.956216	69.869274
950.149979	30.947795	69.874279
950.285390	29.206022	69.879284
949.551649	33.421162	69.884289
948.701513	28.490108	69.889294
947.870690	36.971914	69.894298
947.652443	32.482754	69.899303
946.998175	29.464804	69.904308
945.341952	33.318980	69.909313
944.919318	33.668616	69.914318
944.538214	30.457398	69.919322
944.132730	27.704197	69.924327
943.664182	27.135521	69.929332
942.559787	31.554713	69.934337
941.884225	29.301776	69.939342
941.248128	27.856220	69.944346
940.883976	35.456417	69.949351
940.238602	19.629795	69.954356
939.296492	34.807311	69.959361
938.522539	26.459697	69.964366
938.165575	31.835376	69.969370
937.322459	37.398795	69.974375
936.698195	29.186624	69.979380
936.188652	32.648620	69.984385
935.597290	24.675631	69.989390
934.968096	40.637520	69.994394
933.849728	31.091104	69.999399
933.249325	26.320580	70.004404
932.728523	33.259769	70.009409
932.603096	26.049951	70.014414
931.640045	24.189674	70.019418
930.771710	34.017782	70.024423
930.630150	25.905413	70.029428
929.425099	32.751645	70.034433
928.757681	26.296661	70.039438
928.148304	25.264725	70.044442
927.377029	29.031706	70.049447
926.875501	23.494866	70.054452
925.757728	32.932184	70.059457
925.571544	29.995864	70.064462
924.847358	27.973008	70.069466
924.032679	30.141653	70.074471
923.719554	27.269687	70.079476
923.165652	27.536141	70.084481
922.472279	20.886607	70.089486
921.771455	24.295469	70.094490
920.537901	28.697376	70.099495
920.315139	24.314591	70.104500
919.650149	32.796819	70.109505
918.864631	24.214525	70.114510
917.888590	26.109246	70.119514
917.086493	28.443039	70.124519
917.123164	22.940399	70.129524
916.571328	26.300324	70.134529
915.715103	24.725811	70.139534
914.653664	34.877948	70.144538
914.232468	21.447181	70.149543
913.857151	18.253974	70.154548
913.018747	19.995915	70.159553
911.917156	23.632547	70.164558
911.598686	30.137441	70.169562
911.007632	25.568851	70.174567
910.665354	29.202918	70.179572
909.351905	35.500316	70.184577
908.715351	27.559755	70.189582
908.173442	25.203563	70.194586
907.857478	24.214822	70.199591
906.946419	21.116331	70.204596
906.144385	28.396724	70.209601
905.466714	27.760416	70.214606
905.200162	23.622707	70.219610
904.220987	21.760277	70.224615
903.160273	20.440647	70.229620
902.750777	29.517692	70.234625
902.473063	29.935730	70.239630
902.150632	18.985422	70.244634
901.692775	27.163467	70.249639
900.546394	23.389686	70.254644
899.791934	24.169004	70.259649
898.835906	33.036575	70.264654
898.111987	20.935975	70.269658
897.485166	23.670786	70.274663
897.251561	22.178536	70.279668
896.940145	27.936453	70.284673
895.785551	24.922450	70.289678
894.785672	29.189417	70.294682
893.993654	27.584194	70.299687
893.922959	30.839173	70.304692
893.390563	26.519857	70.309697
892.845146	25.862505	70.314702
891.890400	23.590939	70.319706
890.971190	32.386425	70.324711
890.677867	26.204637	70.329716
889.701894	32.631253	70.334721
888.985562	28.886803	70.339726
888.593023	27.788832	70.344730
888.053376	39.433224	70.349735
887.296797	31.782989	70.354740
886.600850	26.841614	70.359745
886.037421	30.028359	70.364750
885.278620	33.181546	70.369754
884.117927	36.468074	70.374759
884.142481	29.533995	70.379764
883.196216	33.046580	70.384769
882.658292	23.570240	70.389774
881.478130	23.015484	70.394778
880.789983	29.167651	70.399783
880.613370	24.186204	70.404788
879.947615	26.701724	70.409793
879.503612	32.543819	70.414798
878.717921	22.105607	70.419802
877.902656	23.727189	70.424807
877.676991	21.997149	70.429812
876.325871	27.758115	70.434817
875.578976	32.730682	70.439822
875.442665	21.082170	70.444826
874.769028	33.107406	70.449831
874.400216	35.055307	70.454836
873.248391	30.609085	70.459841
872.381543	35.657511	70.464846
872.033267	32.458428	70.469850
871.426180	35.757775	70.474855
870.821286	35.740637	70.479860
869.742178	37.347447	70.484865
869.266773	35.814838	70.489870
868.963069	23.186929	70.494874
867.902596	34.896863	70.499879
867.330671	23.265642	70.504884
866.365588	31.365155	70.509889
866.081663	25.240221	70.514894
865.847279	26.245843	70.519898
864.791843	30.978951	70.524903
864.426467	29.616479	70.529908
863.723413	31.295897	70.534913
862.866176	21.871961	70.539918
861.729094	27.989930	70.544922
861.074945	24.801686	70.549927
860.774600	21.943465	70.554932
860.434601	28.495939	70.559937
859.348110	25.348121	70.564942
858.796060	26.913626	70.569946
858.016282	35.508746	70.574951
857.763264	23.364754	70.579956
856.676411	35.011084	70.584961
855.876402	33.492296	70.589966
855.317527	30.590070	70.594970
854.851812	28.666438	70.599975
854.536013	21.436472	70.604980
853.504302	36.082674	70.609985
852.579134	30.198561	70.614990
852.255922	34.827752	70.619994
851.337714	36.948247	70.624999
850.693134	29.225011	70.630004
849.841561	25.558867	70.635009
849.415072	28.492026	70.640014
849.308015	28.791450	70.645018
848.460579	38.643061	70.650023
847.645116	27.864264	70.655028
846.816334	26.151375	70.660033
846.246958	29.331190	70.665038
845.984395	26.741330	70.670042
844.430011	36.954601	70.675047
844.122929	25.823674	70.680052
843.462262	27.080060	70.685057
843.002909	28.553548	70.690062
842.324330	33.478983	70.695066
841.500451	34.890649	70.700071
841.358571	27.409088	70.705076
840.468611	37.507150	70.710081
839.150955	32.051342	70.715086
838.853700	29.528502	70.720090
837.874460	32.817705	70.725095
838.023954	26.869782	70.730100
837.662439	30.271966	70.735105
836.365832	38.067888	70.740110
835.971930	26.909782	70.745114
834.992884	34.877496	70.750119
834.219787	27.994689	70.755124
833.303054	28.065038	70.760129
832.739299	32.699402	70.765134
832.688072	25.039420	70.770138
831.735473	31.895970	70.775143
830.905117	25.301383	70.780148
830.136781	34.716230	70.785153
829.722019	37.275388	70.790158
829.775832	37.894541	70.795162
828.203632	45.109899	70.800167
827.521035	35.229267	70.805172
827.115885	38.062846	70.810177
826.578978	36.037017	70.815182
825.541215	36.694301	70.820186
824.870829	40.459447	70.825191
824.438444	39.470323	70.830196
824.016562	43.575939	70.835201
823.121617	32.980101	70.840206
822.445499	33.090998	70.845210
821.801342	42.853496	70.850215
821.673866	37.056879	70.855220
820.483988	48.320684	70.860225
819.550469	39.370918	70.865230
819.254158	29.922365	70.870234
818.648580	43.031124	70.875239
817.914594	30.777620	70.880244
816.803516	40.071997	70.885249
816.004125	42.914716	70.890254
815.699348	45.071617	70.895258
815.130406	45.938119	70.900263
814.887869	35.337781	70.905268
813.779856	38.789409	70.910273
813.316387	44.180478	70.915278
812.927479	31.736440	70.920282
811.858136	40.866489	70.925287
811.172062	30.202722	70.930292
810.337582	46.727127	70.935297
809.813191	36.958506	70.940302
809.600455	36.814310	70.945306
808.410423	38.588603	70.950311
808.074973	37.826889	70.955316
807.346216	35.033712	70.960321
806.829349	48.473688	70.965326
805.890829	39.832211	70.970330
805.010251	36.065048	70.975335
805.037729	32.714709	70.980340
804.192903	37.792764	70.985345
802.974511	41.839096	70.990350
802.430114	29.069750	70.995354
801.949574	33.206779	71.000359
801.610884	33.672378	71.005364
800.795755	34.554417	71.010369
799.796606	30.128082	71.015374
799.554092	31.888742	71.020378
798.864760	41.081302	71.025383
798.184726	25.072607	71.030388
797.388605	29.305597	71.035393
796.498904	43.151824	71.040398
796.455290	32.628632	71.045402
794.824191	39.490702	71.050407
794.521155	30.432710	71.055412
794.035490	39.906645	71.060417
793.686857	35.703173	71.065422
792.868565	36.508451	71.070426
791.552082	42.331755	71.075431
791.207917	32.603836	71.080436
790.995213	31.221803	71.085441
789.967221	36.018377	71.090446
789.650253	38.205604	71.095450
788.508593	38.598762	71.100455
788.165889	36.549912	71.105460
787.536248	41.857055	71.110465
786.960474	43.372740	71.115470
785.869974	40.399045	71.120474
785.210061	36.003865	71.125479
784.968853	34.590103	71.130484
784.424525	36.651106	71.135489
782.995000	54.531731	71.140494
782.898201	35.662800	71.145498
782.177193	36.157724	71.150503
781.849924	30.511183	71.155508
780.687730	34.941215	71.160513
779.771943	39.070267	71.165518
779.698012	31.257793	71.170522
778.712257	46.300384	71.175527
778.583084	29.551184	71.180532
777.617200	44.141205	71.185537
776.466557	36.066490	71.190542
776.325338	33.867305	71.195546
775.676372	46.304929	71.200551
775.159295	36.776414	71.205556
774.294235	39.445105	71.210561
773.845930	43.061376	71.215566
773.066376	33.525765	71.220570
771.627719	41.956149	71.225575
771.170396	32.077525	71.230580
770.785285	40.004327	71.235585
770.301703	40.275389	71.240590
770.232944	30.811123	71.245594
768.895778	37.427733	71.250599
768.583672	32.322796	71.255604
767.847938	37.954317	71.260609
766.584324	34.440522	71.265614
766.389285	24.878098	71.270618
765.296866	36.181589	71.275623
764.743507	35.989125	71.280628
764.529754	36.259810	71.285633
764.033639	40.732042	71.290638
763.346644	30.599841	71.295642
762.553126	28.729989	71.300647
761.500554	32.809861	71.305652
760.647768	41.714654	71.310657
760.030819	27.983952	71.315662
759.857524	28.716523	71.320666
759.154513	34.238763	71.325671
758.599603	30.260513	71.330676
757.778151	38.646261	71.335681
756.969280	42.796146	71.340686
756.971695	32.948410	71.345690
755.245542	45.000886	71.350695
754.965814	27.935060	71.355700
754.344222	38.569127	71.360705
753.438891	38.238745	71.365710
753.621668	34.212441	71.370714
752.577501	49.127153	71.375719
752.192190	33.973514	71.380724
751.375868	34.644459	71.385729
750.400720	42.569007	71.390734
749.574116	39.077107	71.395738
748.817632	40.492266	71.400743
748.829451	37.388832	71.405748
748.049020	44.221158	71.410753
746.828589	41.007984	71.415758
746.648949	31.621293	71.420762
746.107739	35.365890	71.425767
745.401823	33.050038	71.430772
744.657893	37.706795	71.435777
743.646355	39.097908	71.440782
743.519853	29.470961	71.445786
742.183752	33.640130	71.450791
741.741069	32.603779	71.455796
741.094140	32.325299	71.460801
740.561215	42.073253	71.465806
740.244624	32.750940	71.470810
738.577172	47.559889	71.475815
738.061510	33.636458	71.480820
737.662291	40.854346	71.485825
736.786588	43.959958	71.490830
736.975131	33.633188	71.495834
736.060073	44.512666	71.500839
735.512816	38.961074	71.505844
734.531595	42.677960	71.510849
734.068011	37.540377	71.515854
733.603033	32.046647	71.520858
732.531716	41.410412	71.525863
731.869684	34.448462	71.530868
731.779600	36.336238	71.535873
730.578517	43.544601	71.540878
729.762973	29.653151	71.545882
728.941957	33.939007	71.550887
728.812908	39.305227	71.555892
728.393648	34.949018	71.560897
727.491112	36.822647	71.565902
726.748229	38.806469	71.570906
725.812694	42.541314	71.575911
725.392478	29.771148	71.580916
724.610479	35.479426	71.585921
723.627202	46.134818	71.590926
723.480524	32.537401	71.595930
722.871487	36.712245	71.600935
722.239564	32.355205	71.605940
721.493648	38.978625	71.610945
720.587720	32.479684	71.615950
720.128357	35.835963	71.620954
719.252245	42.202586	71.625959
718.696703	39.430742	71.630964
718.145867	36.940406	71.635969
717.579092	40.085143	71.640974
717.141942	24.614945	71.645978
715.567104	41.509527	71.650983
715.143775	22.394592	71.655988
714.864832	24.023871	71.660993
714.496716	34.836768	71.665998
713.601872	28.900582	71.671002
712.587655	27.296106	71.676007
712.412286	33.732500	71.681012
711.681864	37.950325	71.686017
710.677359	47.579413	71.691022
710.079322	27.766933	71.696026
709.249731	34.115111	71.701031
709.015374	33.640073	71.706036
708.587418	31.442394	71.711041
707.474240	32.928546	71.716046
706.988056	28.843180	71.721050
706.593727	30.024082	71.726055
705.395002	27.826127	71.731060
705.040477	25.492187	71.736065
704.267244	27.972824	71.741070
703.992683	29.169349	71.746074
702.384161	26.967259	71.751079
702.179448	40.849513	71.756084
701.967444	34.916568	71.761089
700.792724	44.553836	71.766094
699.967656	33.024470	71.771098
699.363994	39.092268	71.776103
698.409730	36.926351	71.781108
698.414229	37.502892	71.786113
697.972101	40.780742	71.791118
697.237979	30.973018	71.796122
696.352572	39.302736	71.801127
695.936037	32.207100	71.806132
695.086106	27.534719	71.811137
693.937127	40.228566	71.816142
693.626984	29.946509	71.821146
693.343260	37.653758	71.826151
692.524712	42.238836	71.831156
691.604401	39.312201	71.836161
690.889195	41.630650	71.841166
690.728988	33.776733	71.846170
689.453621	33.120538	71.851175
688.439572	43.881757	71.856180
687.927864	32.903285	71.861185
687.266621	37.422318	71.866190
686.915827	38.150042	71.871194
686.594888	26.969323	71.876199
686.250180	33.289185	71.881204
685.327675	34.987823	71.886209
684.316849	38.442951	71.891214
684.289083	33.595512	71.896218
682.793475	34.702623	71.901223
682.267923	31.156508	71.906228
681.826691	31.923862	71.911233
681.354116	27.107828	71.916238
680.370105	31.946319	71.921242
679.499061	38.430409	71.926247
679.038038	30.935033	71.931252
678.657931	37.845548	71.936257
677.943058	37.294068	71.941262
676.869213	31.406897	71.946266
676.124872	26.148466	71.951271
675.811037	33.866814	71.956276
675.736949	28.854876	71.961281
674.520540	36.587638	71.966286
673.971738	28.822406	71.971290
673.449881	45.647114	71.976295
672.706339	29.334789	71.981300
671.598470	31.865566	71.986305
670.992418	34.340093	71.991310
670.832762	25.688206	71.996314
669.931817	31.905838	72.001319
669.013045	40.458482	72.006324
667.719739	31.504583	72.011329
667.587762	32.755674	72.016334
667.592481	32.996310	72.021338
666.582034	32.376787	72.026343
666.561580	32.500013	72.031348
665.545187	24.858124	72.036353
664.884115	32.988132	72.041358
664.290791	34.735281	72.046362
663.129185	37.339270	72.051367
662.743214	34.690241	72.056372
662.126731	33.284212	72.061377
660.851914	34.674704	72.066382
660.275777	33.856725	72.071386
659.964268	35.636267	72.076391
659.498756	30.109528	72.081396
659.056627	20.009342	72.086401
658.070882	31.422025	72.091406
657.523737	20.015580	72.096410
656.784827	35.075648	72.101415
655.616298	32.223244	72.106420
655.098032	35.074857	72.111425
654.401832	37.272024	72.116430
654.385554	26.134260	72.121434
653.550939	27.038370	72.126439
652.634297	27.597595	72.131444
651.767815	34.844163	72.136449
651.332005	34.951532	72.141454
651.079060	31.942299	72.146458
650.116925	33.585763	72.151463
648.944237	30.953207	72.156468
648.806267	31.440478	72.161473
648.318561	43.559141	72.166478
647.545687	33.648803	72.171482
646.544192	40.670884	72.176487
646.024024	37.820890	72.181492
645.783061	26.543873	72.186497
644.606031	40.420113	72.191502
643.912266	30.372610	72.196506
643.295409	32.132972	72.201511
642.663540	29.496297	72.206516
642.765211	29.675765	72.211521
641.136480	40.694139	72.216526
640.765634	32.500057	72.221530
640.470180	28.532559	72.226535
639.789400	18.585494	72.231540
638.923793	25.865035	72.236545
637.739509	29.846086	72.241550
637.494079	31.531534	72.246554
637.008857	36.244885	72.251559
636.203311	25.347917	72.256564
635.349087	22.819190	72.261569
634.372931	24.901680	72.266574
634.463173	21.413627	72.271578
634.164548	30.908246	72.276583
632.999328	34.446321	72.281588
632.321691	29.666107	72.286593
631.712160	27.809576	72.291598
630.713996	25.027821	72.296602
630.025507	34.240771	72.301607
629.466408	38.653671	72.306612
629.131646	26.421829	72.311617
628.215794	33.438159	72.316622
627.104568	28.039485	72.321626
626.279904	35.096485	72.326631
626.012654	35.326817	72.331636
625.680772	29.849765	72.336641
625.399375	37.946128	72.341646
624.619225	38.027917	72.346650
623.783707	36.877538	72.351655
623.018622	42.524807	72.356660
622.995226	33.543737	72.361665
621.719070	33.824356	72.366670
620.847338	22.184201	72.371674
620.529275	31.565228	72.376679
619.512743	41.935800	72.381684
619.182064	26.024506	72.386689
618.542417	29.176134	72.391694
617.997348	34.610179	72.396698
617.201735	31.045590	72.401703
615.953462	32.340419	72.406708
615.762926	26.167544	72.411713
615.080049	35.627170	72.416718
614.570272	27.087814	72.421722
613.241267	32.309255	72.426727
612.785282	36.033996	72.431732
612.589024	34.837008	72.436737
612.046889	38.329480	72.441742
611.177646	26.714159	72.446746
610.449735	35.359416	72.451751
609.690451	28.630604	72.456756
609.351576	25.174622	72.461761
608.345086	32.795135	72.466766
607.388298	25.566378	72.471770
607.227870	29.305547	72.476775
606.453942	34.922688	72.481780
606.228185	21.689539	72.486785
604.850953	37.195025	72.491790
604.257257	32.507101	72.496794
603.684631	21.803278	72.501799
603.393786	35.648778	72.506804
602.615372	24.659201	72.511809
601.686803	40.115315	72.516814
601.601346	26.489258	72.521818
600.927008	26.820692	72.526823
599.744195	24.145623	72.531828
599.246830	28.960253	72.536833
598.503645	32.475283	72.541838
597.963929	29.920133	72.546842
597.061318	27.064832	72.551847
596.272010	33.870219	72.556852
595.950139	33.073260	72.561857
595.784151	34.156316	72.566862
594.351780	26.054039	72.571866
593.625599	34.681678	72.576871
593.268356	35.683236	72.581876
592.731914	31.900773	72.586881
591.746610	38.444083	72.591886
590.739819	30.684010	72.596890
590.218087	30.532278	72.601895
589.704083	27.307604	72.606900
589.683005	28.394387	72.611905
589.035285	31.656111	72.616910
588.212305	27.881440	72.621914
587.730046	20.972911	72.626919
586.847432	22.458662	72.631924
585.894970	26.177323	72.636929
585.111405	28.080935	72.641934
584.475116	27.624194	72.646938
583.962678	31.928750	72.651943
583.451860	31.313262	72.656948
582.498147	28.330496	72.661953
581.741878	32.074681	72.666958
581.604086	28.697057	72.671962
580.943804	28.851226	72.676967
580.049072	38.898077	72.681972
579.493736	29.290571	72.686977
578.781415	33.073487	72.691982
578.387945	27.355534	72.696986
577.450139	31.158593	72.701991
576.738083	33.323614	72.706996
576.397311	24.235416	72.712001
575.316576	33.722145	72.717006
574.584807	23.839989	72.722010
574.176328	29.782108	72.727015
573.434935	34.492115	72.732020
573.018790	34.788742	72.737025
571.784174	39.446426	72.742030
571.286701	29.782402	72.747034
570.821122	30.993594	72.752039
570.512458	31.244720	72.757044
569.732716	22.559155	72.762049
568.723267	36.344074	72.767054
568.039586	31.350391	72.772058
567.948394	31.382388	72.777063
566.558592	28.295630	72.782068
565.892387	30.136403	72.787073
565.216601	35.400477	72.792078
565.052237	39.014128	72.797082
564.392459	32.362518	72.802087
563.221301	38.415076	72.807092
562.953519	28.544172	72.812097
562.226476	37.501518	72.817102
561.962576	29.150083	72.822106
560.912495	33.062488	72.827111
560.265311	39.422653	72.832116
559.904634	33.428259	72.837121
558.682626	37.662921	72.842126
558.149011	24.876181	72.847130
557.439499	25.807702	72.852135
556.943795	32.042819	72.857140
556.680904	28.344522	72.862145
555.642039	38.754935	72.867150
554.452264	34.903086	72.872154
554.256174	31.115306	72.877159
553.670908	36.191511	72.882164
553.637586	28.710044	72.887169
552.295333	31.489501	72.892174
551.565221	30.387010	72.897178
551.037798	27.990753	72.902183
549.742020	40.542459	72.907188
549.334420	32.937689	72.912193
548.854752	29.717016	72.917198
548.426054	34.351994	72.922202
548.100985	33.643855	72.927207
546.969388	31.758542	72.932212
546.259264	27.541737	72.937217
545.674132	33.701220	72.942222
545.196566	23.616171	72.947226
544.657918	27.169594	72.952231
543.678365	23.066664	72.957236
543.246803	20.970512	72.962241
542.474744	31.712142	72.967246
541.827078	25.373984	72.972250
540.935399	28.721881	72.977255
540.132073	31.374506	72.982260
539.910861	18.828159	72.987265
538.946156	31.737109	72.992270
537.695271	35.627894	72.997274
537.429426	31.532702	73.002279
536.800154	35.583081	73.007284
537.061306	28.267587	73.012289
536.346515	34.900280	73.017294
535.436855	28.559702	73.022298
534.901044	35.271114	73.027303
534.058915	27.726103	73.032308
533.064993	29.485052	73.037313
532.216736	28.776676	73.042318
532.138687	24.960638	73.047322
531.156348	28.917452	73.052327
529.727668	33.535106	73.057332
529.742183	28.789747	73.062337
529.036214	30.745667	73.067342
528.639772	34.688002	73.072346
528.297732	28.942945	73.077351
527.181893	42.888321	73.082356
526.405115	37.494765	73.087361
525.559311	36.831730	73.092366
525.303633	32.164099	73.097370
525.049816	19.744367	73.102375
523.599090	29.507650	73.107380
523.404697	25.683337	73.112385
522.984301	33.890145	73.117390
521.856802	31.050195	73.122394
521.059992	32.632681	73.127399
520.055373	31.020450	73.132404
520.063661	19.683265	73.137409
519.406756	26.275201	73.142414
518.664769	36.040707	73.147418
517.849069	30.522478	73.152423
517.238051	31.711118	73.157428
517.032519	28.752695	73.162433
515.876055	32.891783	73.167438
515.158391	26.790274	73.172442
514.555105	21.212985	73.177447
514.057355	27.087332	73.182452
513.506761	23.042235	73.187457
512.364687	37.475883	73.192462
511.705632	35.054873	73.197466
511.450876	33.961824	73.202471
510.741556	39.907723	73.207476
510.190297	30.726918	73.212481
509.333534	28.334250	73.217486
508.898430	31.773422	73.222490
508.435616	29.124048	73.227495
507.520322	40.236991	73.232500
506.801686	24.583063	73.237505
506.360760	23.295758	73.242510
504.986152	35.137834	73.247514
504.074687	25.694312	73.252519
503.152872	25.778206	73.257524
503.536900	26.947106	73.262529
502.512367	34.753443	73.267534
502.478462	29.410287	73.272538
502.143732	34.880226	73.277543
501.283186	33.366470	73.282548
500.398670	36.131382	73.287553
499.277498	37.552669	73.292558
498.379221	29.141463	73.297562
497.957844	29.092028	73.302567
497.515770	41.914590	73.307572
497.195079	29.828763	73.312577
496.378198	41.090026	73.317582
495.567763	31.499531	73.322586
495.022311	30.872234	73.327591
494.021667	26.000027	73.332596
493.041325	26.123209	73.337601
492.574893	27.806029	73.342606
492.090422	26.010032	73.347610
491.877875	27.578297	73.352615
491.081905	33.088597	73.357620
490.219350	24.867236	73.362625
489.326272	32.088122	73.367630
488.926024	34.578787	73.372634
488.621758	25.987810	73.377639
487.362039	37.813171	73.382644
486.928124	24.767739	73.387649
486.070162	36.743551	73.392654
485.960464	31.623768	73.397658
485.298985	25.680465	73.402663
484.454456	35.806067	73.407668
483.806541	27.809118	73.412673
482.605824	37.810125	73.417678
481.706515	36.062869	73.422682
481.417099	25.947865	73.427687
480.788535	35.487165	73.432692
480.606057	23.565399	73.437697
480.193036	30.659352	73.442702
479.115176	40.658136	73.447706
478.639952	17.532166	73.452711
477.530505	39.669855	73.457716
476.426109	29.520688	73.462721
475.724081	33.325642	73.467726
475.205926	25.970303	73.472730
474.878737	37.369585	73.477735
474.420536	32.839874	73.482740
474.434869	22.203429	73.487745
473.604121	37.431108	73.492750
472.900990	44.162880	73.497754
472.059672	26.125385	73.502759
470.371716	36.352241	73.507764
470.198685	19.998019	73.512769
469.584861	38.090970	73.517774
468.893232	29.892845	73.522778
469.072914	26.283317	73.527783
467.525244	29.808278	73.532788
467.711740	29.427058	73.537793
466.560250	26.676108	73.542798
465.170225	27.990440	73.547802
464.857094	25.522221	73.552807
464.313448	35.904225	73.557812
463.792215	35.744556	73.562817
463.669635	34.151093	73.567822
462.338157	34.295536	73.572826
461.934883	18.080494	73.577831
461.063510	37.062821	73.582836
460.982442	25.563266	73.587841
459.854564	32.719072	73.592846
458.755106	28.865501	73.597850
458.969533	28.041466	73.602855
458.194284	36.954476	73.607860
457.044139	21.200596	73.612865
456.219076	29.210117	73.617870
455.651029	35.953483	73.622874
455.643114	22.056500	73.627879
454.090903	38.859287	73.632884
453.647166	28.543383	73.637889
453.201579	18.566804	73.642894
452.726450	32.405387	73.647898
452.325444	33.746652	73.652903
451.060551	31.748589	73.657908
450.552723	32.304255	73.662913
450.229001	22.522711	73.667918
449.544209	28.761159	73.672922
448.768011	28.105984	73.677927
447.616428	40.529106	73.682932
447.452214	28.114032	73.687937
446.286381	31.343222	73.692942
445.475023	37.168204	73.697946
444.906288	31.470318	73.702951
444.690187	24.983017	73.707956
444.222482	25.155425	73.712961
443.879461	21.228654	73.717966
442.806977	32.150622	73.722970
441.994394	31.239488	73.727975
441.731995	29.606805	73.732980
440.738871	26.269278	73.737985
440.095872	33.325765	73.742990
439.498888	32.269903	73.747994
438.249422	31.724823	73.752999
437.374241	33.297745	73.758004
437.153167	30.668215	73.763009
436.475048	35.521130	73.768014
436.254198	35.018738	73.773018
436.235631	27.410361	73.778023
434.969907	34.294845	73.783028
434.321903	34.193224	73.788033
433.745267	30.682117	73.793038
432.665117	27.468838	73.798042
431.918614	25.090170	73.803047
431.469842	27.443502	73.808052
430.653227	25.355107	73.813057
429.628362	27.115871	73.818062
429.039562	30.980062	73.823066
429.032795	21.509124	73.828071
428.122721	36.620146	73.833076
428.065539	32.083321	73.838081
426.902055	30.777120	73.843086
426.222492	25.577839	73.848090
425.700835	31.214751	73.853095
424.705444	31.493312	73.858100
424.025823	27.631210	73.863105
423.312909	23.709764	73.868110
422.771848	35.355995	73.873114
422.541281	26.204545	73.878119
421.068604	43.806758	73.883124
420.388529	30.805293	73.888129
420.179172	33.872641	73.893134
419.566934	36.354516	73.898138
419.366236	26.302656	73.903143
418.468297	40.372606	73.908148
417.797730	25.303955	73.913153
417.023055	37.403699	73.918158
415.846900	35.733692	73.923162
415.259397	31.565197	73.928167
414.785265	35.472619	73.933172
414.310520	29.225214	73.938177
414.032323	26.975350	73.943182
413.039393	34.745144	73.948186
412.141902	33.418645	73.953191
411.533666	38.515881	73.958196
411.446371	31.576003	73.963201
410.422796	31.606764	73.968206
409.498215	29.472504	73.973210
408.804940	26.706918	73.978215
408.490884	33.231636	73.983220
407.762173	31.200201	73.988225
406.832316	33.392086	73.993230
406.357828	34.190014	73.998234
405.933537	27.910921	74.003239
404.633441	38.041325	74.008244
404.088876	25.549679	74.013249
403.738111	22.429920	74.018254
402.871924	34.121648	74.023258
402.551732	17.940695	74.028263
401.700168	33.354612	74.033268
400.864149	30.151331	74.038273
400.558375	32.778332	74.043278
400.208343	29.794064	74.048282
399.022098	23.929675	74.053287
398.358104	28.613199	74.058292
397.841784	23.864127	74.063297
397.453532	28.301878	74.068302
396.276981	31.189044	74.073306
395.914784	28.178333	74.078311
395.513862	27.187430	74.083316
394.306480	28.780184	74.088321
393.555783	21.998054	74.093326
393.012324	27.606906	74.098330
392.754101	24.721545	74.103335
391.737331	28.207686	74.108340
391.128831	21.529047	74.113345
390.137433	33.393683	74.118350
389.732567	24.856603	74.123354
389.723325	26.532819	74.128359
388.147208	27.755427	74.133364
387.191962	27.981878	74.138369
386.937348	22.107812	74.143374
386.632148	21.450142	74.148378
386.554219	21.282927	74.153383
385.179739	33.561820	74.158388
384.628021	25.872833	74.163393
384.106242	30.707154	74.168398
382.950806	32.569162	74.173402
382.322392	26.568589	74.178407
381.356866	27.656063	74.183412
380.905853	36.126366	74.188417
380.702191	29.425793	74.193422
380.136332	32.106853	74.198426
379.531099	35.338202	74.203431
378.298131	30.351689	74.208436
378.067048	41.806619	74.213441
377.707280	37.653881	74.218446
376.430637	42.220585	74.223450
376.179613	23.551378	74.228455
375.226785	37.485010	74.233460
374.684485	30.366920	74.238465
373.861823	31.813230	74.243470
373.112863	34.889299	74.248474
373.061075	25.912785	74.253479
372.034048	32.852294	74.258484
370.790645	37.626577	74.263489
370.535662	33.592754	74.268494
369.744116	37.188086	74.273498
369.414536	35.356395	74.278503
368.911141	29.667043	74.283508
367.993520	21.118643	74.288513
367.575828	35.813770	74.293518
366.600205	42.511720	74.298522
366.445987	22.499382	74.303527
365.720880	37.521022	74.308532
364.756245	32.515410	74.313537
364.350139	37.060084	74.318542
362.866202	38.214407	74.323546
362.132079	23.829226	74.328551
361.713523	42.324705	74.333556
361.194156	20.244963	74.338561
360.924308	33.836387	74.343566
360.778343	29.651162	74.348570
359.558059	20.487142	74.353575
358.827413	27.951820	74.358580
358.516851	24.434603	74.363585
357.103753	32.867419	74.368590
356.363092	23.511859	74.373594
356.181747	29.845131	74.378599
355.592398	23.950299	74.383604
354.921940	36.292049	74.388609
354.023685	24.407105	74.393614
353.206601	34.832694	74.398618
352.920490	23.838889	74.403623
352.308493	35.042297	74.408628
351.675518	15.243452	74.413633
350.629651	30.048138	74.418638
349.941032	19.463809	74.423642
349.980505	27.362393	74.428647
349.100490	29.752922	74.433652
348.018209	30.813286	74.438657
347.559349	25.487404	74.443662
346.895654	36.262265	74.448666
346.272898	14.561690	74.453671
345.257664	29.801436	74.458676
344.680582	20.167520	74.463681
344.467969	20.959995	74.468686
343.928875	31.338129	74.473690
343.365105	18.780191	74.478695
342.263362	29.700543	74.483700
341.664938	29.031264	74.488705
340.508811	22.651209	74.493710
339.787017	19.322525	74.498714
339.343947	24.587402	74.503719
338.993356	17.771493	74.508724
338.693166	23.232782	74.513729
338.202994	14.922190	74.518734
336.872483	31.508352	74.523738
336.314697	21.010404	74.528743
335.724028	32.022768	74.533748
334.988261	27.745469	74.538753
334.165405	24.934330	74.543758
333.474955	34.489820	74.548762
333.048858	34.997794	74.553767
332.537178	33.455310	74.558772
331.554950	22.233424	74.563777
331.268629	22.709661	74.568782
330.555684	33.134426	74.573786
329.689069	20.340921	74.578791
328.675824	31.527855	74.583796
328.205350	35.283329	74.588801
328.062866	28.341218	74.593806
327.406472	38.048970	74.598810
326.301013	21.561124	74.603815
325.523604	26.294275	74.608820
325.011915	24.808561	74.613825
324.644032	29.479602	74.618830
323.772959	28.423299	74.623834
322.989720	26.009523	74.628839
322.152745	33.625189	74.633844
322.056629	32.759176	74.638849
321.629584	16.294101	74.643854
320.054356	32.165536	74.648858
319.752481	13.163864	74.653863
319.171167	18.728299	74.658868
318.825924	22.356587	74.663873
317.924449	16.954607	74.668878
317.165182	27.508170	74.673882
316.866896	21.543312	74.678887
315.275354	17.905423	74.683892
314.936015	23.680438	74.688897
314.320146	21.320411	74.693902
313.489194	27.276272	74.698906
313.369086	15.997423	74.703911
313.048602	33.832328	74.708916
311.883843	18.754188	74.713921
311.324490	25.560837	74.718926
310.417370	27.558332	74.723930
310.157420	23.843836	74.728935
309.012528	26.705495	74.733940
308.477701	19.756539	74.738945
307.865522	22.929087	74.743950
307.181600	35.108995	74.748954
307.064832	32.317787	74.753959
306.298921	19.799962	74.758964
305.609593	29.106133	74.763969
304.744307	23.163837	74.768974
303.644917	40.850094	74.773978
303.501728	22.709314	74.778983
303.085142	37.260773	74.783988
301.606768	26.102205	74.788993
301.003273	34.625199	74.793998
300.124170	29.971813	74.799002
299.840649	27.539899	74.804007
299.629520	32.346798	74.809012
298.769319	23.683629	74.814017
297.790725	23.338286	74.819022
297.304254	20.728998	74.824026
296.974399	29.433866	74.829031
295.906773	29.856446	74.834036
294.942877	31.888227	74.839041
294.931059	30.091054	74.844046
294.136083	42.028489	74.849050
293.748587	31.008276	74.854055
292.846330	27.050822	74.859060
291.899545	29.034147	74.864065
291.539759	25.267760	74.869070
291.097342	29.785114	74.874074
290.141599	21.977638	74.879079
289.401152	28.869921	74.884084
288.943609	26.781114	74.889089
288.097397	27.794417	74.894094
286.938265	25.446871	74.899098
286.496927	24.661113	74.904103
286.283499	28.060252	74.909108
285.581288	36.121197	74.914113
285.017655	20.046883	74.919118
284.107494	30.616621	74.924122
283.672578	18.883358	74.929127
283.130930	28.579129	74.934132
281.715417	22.194719	74.939137
281.420717	18.301275	74.944142
280.643340	17.231632	74.949146
280.387498	20.918210	74.954151
279.166356	31.409790	74.959156
278.205623	20.219198	74.964161
278.337565	30.723759	74.969166
277.555265	17.450096	74.974170
277.326384	20.903734	74.979175
276.512247	21.423106	74.984180
275.633094	29.398718	74.989185
275.217848	19.899871	74.994190
274.052174	35.020124	74.999194
273.127246	15.165356	75.004199
272.898121	19.000629	75.009204
272.458867	29.894254	75.014209
272.071364	22.674261	75.019214
271.005858	18.958866	75.024218
270.322511	23.170870	75.029223
269.985516	18.185106	75.034228
268.545496	18.383222	75.039233
268.178509	17.010067	75.044238
267.530962	22.372194	75.049242
267.250425	26.600415	75.054247
266.730759	15.394721	75.059252
265.315452	24.960103	75.064257
265.057128	13.995012	75.069262
264.010880	27.943550	75.074266
263.811726	22.073280	75.079271
263.094985	25.260927	75.084276
262.442461	20.975119	75.089281
261.862595	18.573101	75.094286
260.852497	25.773279	75.099290
260.209227	23.477554	75.104295
259.565675	15.462651	75.109300
259.065379	21.711149	75.114305
258.787272	12.441171	75.119310
257.463832	23.204508	75.124314
257.036534	17.290186	75.129319
256.458517	18.274943	75.134324
255.776547	19.282576	75.139329
255.716589	14.150164	75.144334
254.143952	18.664757	75.149338
253.749429	23.395239	75.154343
253.178163	17.863387	75.159348
252.272897	17.656174	75.164353
251.417275	18.519612	75.169358
250.892064	20.732201	75.174362
250.675647	26.285792	75.179367
250.233507	21.979068	75.184372
249.106482	26.851539	75.189377
248.639283	23.610027	75.194382
247.744954	30.254054	75.199386
247.078062	18.327559	75.204391
246.245757	24.510719	75.209396
245.447986	26.358352	75.214401
245.340450	17.045416	75.219406
244.546400	23.105791	75.224410
244.103576	16.173728	75.229415
242.991215	17.361925	75.234420
242.211814	18.470242	75.239425
242.374755	17.624437	75.244430
241.359894	24.883724	75.249434
240.517102	26.098335	75.254439
239.887467	22.978905	75.259444
239.730584	20.779110	75.264449
238.610251	14.418638	75.269454
237.302495	26.325853	75.274458
236.975264	21.436303	75.279463
236.647570	18.480043	75.284468
236.098323	21.525887	75.289473
235.465432	13.529793	75.294478
234.637185	25.977121	75.299482
234.111889	17.348903	75.304487
233.551350	20.298783	75.309492
232.389415	27.844852	75.314497
232.054618	8.605630	75.319502
231.273012	18.073163	75.324506
230.743162	26.205979	75.329511
229.655527	22.082574	75.334516
228.775839	22.729097	75.339521
228.485528	28.357543	75.344526
228.200957	24.061972	75.349530
227.903239	22.463330	75.354535
226.613447	15.923309	75.359540
225.656545	25.344680	75.364545
225.567099	18.170222	75.369550
224.868885	34.192041	75.374554
223.963627	28.115809	75.379559
223.379779	18.473554	75.384564
222.596797	20.263646	75.389569
222.544637	18.100771	75.394574
221.300588	21.055540	75.399578
220.508366	17.183072	75.404583
219.987688	17.635184	75.409588
219.229070	23.130136	75.414593
218.939150	15.899334	75.419598
218.325684	32.716564	75.424602
217.988265	16.276660	75.429607
217.085546	22.415862	75.434612
215.502227	26.591584	75.439617
215.339037	20.463293	75.444622
214.502118	26.560471	75.449626
214.537548	23.297185	75.454631
213.613123	26.689829	75.459636
212.513989	30.364197	75.464641
212.051893	22.050740	75.469646
211.590307	25.263953	75.474650
211.073698	28.213143	75.479655
210.181347	18.714683	75.484660
209.436469	23.155691	75.489665
209.122743	20.048985	75.494670
208.162788	17.067373	75.499674
207.375983	26.016963	75.504679
206.613029	23.432848	75.509684
205.853337	23.292326	75.514689
205.902353	19.120189	75.519694
204.655558	19.092010	75.524698
203.817116	18.990849	75.529703
203.206128	12.481394	75.534708
202.825983	22.711204	75.539713
202.432240	19.111087	75.544718
202.172621	17.679829	75.549722
201.156770	28.135556	75.554727
200.669711	19.578517	75.559732
199.416594	23.056678	75.564737
198.696932	18.899857	75.569742
197.984761	12.007592	75.574746
197.408168	19.835646	75.579751
197.051122	12.309642	75.584756
196.528341	19.777481	75.589761
195.832518	22.567599	75.594766
194.947820	22.536889	75.599770
194.585955	19.863608	75.604775
193.556231	7.154528	75.609780
192.543705	20.050678	75.614785
192.345717	15.041193	75.619790
191.657405	23.700712	75.624794
191.666496	17.295819	75.629799
190.615953	12.800693	75.634804
189.587302	24.338601	75.639809
189.208945	20.851143	75.644814
187.895329	23.928975	75.649818
187.116877	20.404383	75.654823
186.949442	10.925980	75.659828
186.300381	27.789879	75.664833
186.227961	20.685245	75.669838
184.991428	20.147695	75.674842
184.024218	29.655873	75.679847
183.686391	15.201297	75.684852
183.267654	10.208086	75.689857
182.967695	20.768864	75.694862
181.782563	24.784938	75.699866
181.237032	20.086309	75.704871
180.740295	23.847566	75.709876
178.985988	18.464921	75.714881
178.733615	14.733470	75.719886
178.092381	27.176225	75.724890
177.614635	15.706852	75.729895
177.321183	17.657017	75.734900
176.719017	16.412828	75.739905
176.435209	8.673319	75.744910
175.306968	24.948182	75.749914
174.572505	17.595885	75.754919
173.899575	22.761818	75.759924
172.808486	25.813642	75.764929
172.918901	18.355030	75.769934
172.191742	22.088373	75.774938
171.388004	20.128896	75.779943
170.324524	26.874023	75.784948
169.401473	27.424986	75.789953
169.289012	21.985579	75.794958
168.262019	21.425669	75.799962
167.585260	16.457827	75.804967
166.706959	21.777922	75.809972
166.551054	20.689653	75.814977
166.347833	15.062883	75.819982
165.649961	22.427764	75.824986
164.524356	15.175676	75.829991
164.060553	19.541923	75.834996
163.381674	25.197630	75.840001
162.685888	25.736015	75.845006
161.584835	20.665521	75.850010
161.232934	21.478640	75.855015
161.155831	20.261121	75.860020
159.865997	31.990485	75.865025
159.279049	21.334832	75.870030
158.676596	13.273991	75.875034
157.929586	18.926368	75.880039
157.555254	23.002404	75.885044
155.992656	25.142304	75.890049
155.385284	28.246314	75.895054
155.115426	28.945436	75.900058
154.841131	26.534147	75.905063
154.939257	24.148631	75.910068
153.611417	32.085435	75.915073
153.230961	23.330075	75.920078
152.181982	34.142739	75.925082
151.104676	19.042875	75.930087
150.206906	22.062308	75.935092
149.577859	28.542649	75.940097
149.442886	31.421543	75.945102
148.888807	26.356879	75.950106
148.174699	24.039367	75.955111
147.568705	30.027211	75.960116
146.891532	23.391137	75.965121
146.569285	26.046016	75.970126
145.511404	27.069463	75.975130
144.773530	25.138915	75.980135
144.401186	17.654782	75.985140
142.959473	37.248448	75.990145
142.352887	7.289038	75.995150
141.882132	22.306404	76.000154
141.462798	28.255027	76.005159
141.120526	17.017937	76.010164
140.045656	27.867842	76.015169
139.278133	15.590034	76.020174
138.604632	29.269455	76.025178
138.122733	30.459673	76.030183
138.037728	17.882242	76.035188
136.533818	26.102573	76.040193
136.216039	13.421921	76.045198
135.559432	29.801362	76.050202
134.867113	16.705796	76.055207
134.534075	23.463770	76.060212
133.466721	19.319834	76.065217
133.030982	29.268376	76.070222
132.446430	27.456878	76.075226
131.498671	21.597187	76.080231
130.804243	26.479573	76.085236
130.192179	29.492881	76.090241
130.100342	18.671570	76.095246
128.907906	22.182663	76.100250
128.366291	22.947194	76.105255
128.053630	28.355297	76.110260
126.806490	31.197072	76.115265
126.056937	24.998293	76.120270
125.283557	26.635507	76.125274
125.166014	31.413298	76.130279
124.841701	13.925888	76.135284
123.519334	23.861268	76.140289
123.187839	29.553053	76.145294
122.382270	30.823265	76.150298
121.358927	21.601180	76.155303
120.722377	11.388666	76.160308
120.078509	36.850286	76.165313
119.815554	19.826140	76.170318
119.516904	33.534102	76.175322
118.310012	20.992064	76.180327
117.593035	31.877947	76.185332
117.008927	24.582113	76.190337
116.677174	27.003562	76.195342
115.502823	34.023416	76.200346
114.926865	37.745283	76.205351
114.489144	26.208043	76.210356
113.712948	34.673453	76.215361
113.193539	24.010198	76.220366
111.745526	33.998738	76.225370
111.507532	19.737981	76.230375
111.285869	37.270133	76.235380
110.939041	26.912074	76.240385
109.911861	28.555071	76.245390
109.093179	28.923846	76.250394
108.486002	24.686043	76.255399
108.208971	14.279020	76.260404
106.970715	26.066402	76.265409
106.595102	23.699660	76.270414
105.881025	31.516542	76.275418
105.113655	18.082894	76.280423
104.184398	25.044745	76.285428
103.138063	29.983253	76.290433
102.930314	28.911139	76.295438
102.440714	22.305091	76.300442
102.078146	34.602508	76.305447
101.793927	21.588524	76.310452
100.848329	27.537494	76.315457
100.235160	27.520288	76.320462
98.956346	24.682599	76.325466
98.314330	26.604782	76.330471
97.991503	25.402796	76.335476
97.581197	22.798753	76.340481
96.485194	35.484342	76.345486
95.396330	22.619165	76.350490
94.931182	26.933602	76.355495
94.828713	16.285871	76.360500
94.384072	30.083335	76.365505
93.439701	26.880104	76.370510
92.963127	21.481422	76.375514
91.903030	28.975039	76.380519
90.804407	12.522532	76.385524
89.784042	27.425711	76.390529
89.638482	28.005677	76.395534
89.206951	29.339248	76.400538
88.655901	26.215215	76.405543
88.546608	25.914249	76.410548
87.577030	25.332602	76.415553
86.832666	15.298129	76.420558
86.150889	30.861630	76.425562
85.147538	20.039033	76.430567
84.651279	22.395260	76.435572
84.069616	26.365604	76.440577
83.925274	25.109929	76.445582
82.738649	25.365510	76.450586
81.676662	29.702590	76.455591
81.560911	13.392954	76.460596
80.641085	33.348084	76.465601
80.162015	25.660222	76.470606
79.343851	30.439360	76.475610
78.378336	28.720164	76.480615
78.207415	25.970724	76.485620
77.455205	19.304067	76.490625
76.509951	24.995964	76.495630
75.958372	30.126802	76.500634
75.228385	22.983546	76.505639
74.889754	22.470012	76.510644
74.208980	29.232987	76.515649
72.948874	21.778483	76.520654
72.389530	31.325724	76.525658
72.437535	28.615485	76.530663
72.100552	20.699979	76.535668
70.463261	28.202076	76.540673
70.330073	35.871144	76.545678
70.214688	31.308937	76.550682
68.722508	26.616230	76.555687
68.071994	33.036938	76.560692
67.503914	26.366147	76.565697
67.034742	34.468814	76.570702
65.807487	24.030413	76.575706
64.637785	39.436786	76.580711
64.683985	24.714427	76.585716
63.747185	38.621924	76.590721
63.815766	26.844696	76.595726
63.813961	24.656452	76.600730
62.580009	39.153772	76.605735
61.847500	31.031698	76.610740
61.041891	32.932674	76.615745
59.788416	20.536866	76.620750
59.207241	34.990001	76.625754
58.319605	33.433423	76.630759
58.353092	21.999241	76.635764
57.620139	28.098805	76.640769
57.214915	31.501737	76.645774
55.867849	39.347045	76.650778
55.558157	31.916008	76.655783
55.472675	23.835825	76.660788
54.248224	36.341652	76.665793
53.659799	29.874368	76.670798
53.248441	27.847626	76.675802
52.463870	39.720373	76.680807
51.235970	20.640974	76.685812
50.246839	34.134221	76.690817
50.033633	30.401268	76.695822
49.787579	28.531078	76.700826
49.122403	26.598428	76.705831
49.215360	20.872403	76.710836
47.705461	31.105791	76.715841
47.298544	23.606692	76.720846
46.348396	29.671516	76.725850
45.335960	37.994858	76.730855
44.878081	32.790308	76.735860
44.327209	30.910388	76.740865
44.001727	22.877944	76.745870
43.072089	28.613091	76.750874
42.201822	23.017029	76.755879
42.045624	26.284060	76.760884
41.204977	37.236988	76.765889
40.623846	18.581118	76.770894
39.865790	27.242329	76.775898
38.954950	29.106481	76.780903
38.949274	29.099630	76.785908
37.833984	26.295816	76.790913
37.193387	24.064381	76.795918
36.521387	19.057979	76.800922
35.288373	30.064018	76.805927
35.094027	24.815868	76.810932
34.126785	26.208079	76.815937
34.044991	16.247718	76.820942
33.652688	25.976463	76.825946
32.491384	32.775088	76.830951
31.640427	17.680197	76.835956
30.899339	33.874443	76.840961
30.567610	25.533935	76.845966
29.962960	26.617601	76.850970
29.003253	31.389367	76.855975
28.535597	23.892076	76.860980
27.821795	30.702903	76.865985
27.732506	29.648172	76.870990
26.754958	13.576912	76.875994
25.486608	25.447967	76.880999
25.430490	24.493594	76.886004
24.334235	24.957125	76.891009
23.653394	24.849813	76.896014
23.333618	27.901676	76.901018
22.681797	30.503485	76.906023
22.341195	24.584851	76.911028
20.777651	25.681114	76.916033
20.280431	29.863493	76.921038
20.108246	23.003429	76.926042
19.424445	22.500803	76.931047
18.788545	21.886465	76.936052
17.724371	26.637051	76.941057
17.115444	20.783291	76.946062
16.900444	16.167600	76.951066
16.211792	32.864380	76.956071
15.488153	21.524154	76.961076
14.406061	17.847795	76.966081
14.037868	30.433092	76.971086
13.271593	16.166741	76.976090
12.349747	30.073433	76.981095
12.086271	19.093448	76.986100
11.384429	30.024239	76.991105
10.894111	22.574719	76.996110
10.259670	23.495996	77.001114
8.825163	34.384386	77.006119
8.707853	24.227851	77.011124
7.780331	29.592115	77.016129
7.778687	29.619312	77.021134
6.918569	23.739390	77.026139
5.884517	28.431564	77.031143
5.748348	30.889635	77.036148
4.732040	32.043696	77.041153
3.945555	26.377520	77.046158